Tue Jun 08 17:30:13 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.144475	98.404721	0.000000
-0.384854	88.281097	0.005005
-1.139974	46.798021	0.010010
-2.943225	9.042828	0.015014
-6.841628	-2.036115	0.020019
-12.365520	-4.432945	0.025024
-17.713159	2.461494	0.030029
-22.516059	1.549100	0.035034
-25.953393	-4.650526	0.040038
-30.114450	0.327026	0.045043
-33.407359	-3.343187	0.050048
-36.750034	-0.202818	0.055053
-40.379429	4.029938	0.060058
-44.030964	-2.104131	0.065062
-48.020832	5.290893	0.070067
-51.562299	-5.984199	0.075072
-55.390939	-10.464442	0.080077
-59.433493	0.472280	0.085082
-62.786202	-10.037457	0.090086
-66.762035	4.767834	0.095091
-70.485579	1.810134	0.100096
-74.221462	-2.340629	0.105101
-78.039838	-1.275750	0.110106
-81.969558	-11.305233	0.115110
-85.989556	0.975971	0.120115
-89.492103	-5.013091	0.125120
-93.020484	-8.726950	0.130125
-97.278262	6.482741	0.135130
-100.755854	-2.395135	0.140134
-104.388520	-0.121901	0.145139
-108.082545	-4.794909	0.150144
-112.234278	-0.530548	0.155149
-115.750203	6.400782	0.160154
-119.136210	-10.881950	0.165158
-122.954636	-0.706329	0.170163
-126.916800	-8.826915	0.175168
-131.199802	-11.257989	0.180173
-134.935572	-6.052908	0.185178
-138.770995	-4.797173	0.190182
-142.836220	0.413893	0.195187
-145.893174	2.390283	0.200192
-149.659991	-0.884773	0.205197
-153.618931	2.248478	0.210202
-157.332792	-2.601863	0.215206
-161.039129	-0.489228	0.220211
-164.436799	-0.979748	0.225216
-168.237702	-2.387095	0.230221
-172.472845	4.230675	0.235226
-175.936991	-5.904618	0.240230
-179.891200	0.899435	0.245235
-183.675916	-4.675259	0.250240
-187.429680	-3.909508	0.255245
-190.996826	-3.420086	0.260250
-194.613579	-9.079229	0.265254
-198.105578	6.070647	0.270259
-201.794404	-1.013271	0.275264
-206.098424	1.009289	0.280269
-210.358568	9.498359	0.285274
-213.719787	3.571206	0.290278
-217.285982	4.890956	0.295283
-221.269364	-3.114989	0.300288
-224.892031	-0.920739	0.305293
-228.475428	3.145201	0.310298
-232.304802	-2.225224	0.315302
-236.914260	2.190379	0.320307
-240.483636	1.387154	0.325312
-243.408597	-3.832877	0.330317
-247.766502	-2.052861	0.335322
-251.157034	-2.268637	0.340326
-255.213507	-0.673727	0.345331
-258.884509	-5.547117	0.350336
-262.651857	-1.360791	0.355341
-266.448110	6.451564	0.360346
-269.686796	5.385603	0.365350
-273.662712	2.795816	0.370355
-277.543264	1.038301	0.375360
-281.457277	-4.727664	0.380365
-284.813090	0.067386	0.385370
-289.117226	-9.108649	0.390374
-293.061639	5.370122	0.395379
-296.565231	5.479278	0.400384
-300.155971	-4.704054	0.405389
-304.162005	-0.867515	0.410394
-307.792490	-10.057246	0.415398
-311.144605	-1.605438	0.420403
-315.301580	-1.268935	0.425408
-318.721638	-2.825948	0.430413
-323.177286	7.543598	0.435418
-326.323155	-10.874660	0.440422
-330.043120	3.380911	0.445427
-333.920747	-2.935946	0.450432
-337.664141	0.078387	0.455437
-341.721731	-0.223406	0.460442
-345.206347	-8.964080	0.465446
-349.348524	4.096520	0.470451
-353.077844	0.686139	0.475456
-356.270056	-4.207724	0.480461
-360.414491	-8.412878	0.485466
-363.990654	-7.311947	0.490470
-368.251663	-2.399450	0.495475
-371.714410	2.254543	0.500480
-375.460874	1.595087	0.505485
-379.442025	7.012970	0.510490
-382.629394	-3.506308	0.515494
-386.628729	-4.796142	0.520499
-390.508669	0.744507	0.525504
-393.767059	-0.917939	0.530509
-397.905927	5.407611	0.535514
-401.827464	1.188728	0.540518
-405.776751	-4.307010	0.545523
-409.293014	-0.166403	0.550528
-412.985496	-0.516558	0.555533
-416.722058	2.778885	0.560538
-420.329640	-6.783333	0.565542
-423.996265	0.063547	0.570547
-427.957041	1.578251	0.575552
-431.735113	6.604521	0.580557
-436.021440	10.604912	0.585562
-439.706711	-6.496320	0.590566
-443.149371	8.591168	0.595571
-446.853714	-0.780756	0.600576
-450.705432	7.215716	0.605581
-454.719093	0.361429	0.610586
-458.465098	-5.237023	0.615590
-462.233886	2.408147	0.620595
-465.642492	-2.423245	0.625600
-469.626980	-8.221542	0.630605
-473.292311	1.797030	0.635610
-476.627092	-8.828313	0.640614
-480.882001	-5.990559	0.645619
-484.511764	-2.541688	0.650624
-488.181301	-9.936524	0.655629
-492.339206	0.307089	0.660634
-495.648240	-7.876646	0.665638
-499.590957	-2.754186	0.670643
-503.060536	-1.562492	0.675648
-506.736103	-5.274833	0.680653
-510.853003	-4.733460	0.685658
-514.391402	-4.617370	0.690662
-518.419648	3.982953	0.695667
-522.487035	-1.728841	0.700672
-526.260042	4.255777	0.705677
-529.933318	1.031710	0.710682
-533.234067	-9.643629	0.715686
-537.325784	4.489173	0.720691
-541.078728	-1.861908	0.725696
-544.541421	-5.657317	0.730701
-548.669883	-2.480827	0.735706
-552.205779	-13.572871	0.740710
-556.077082	0.921172	0.745715
-559.832109	-3.873593	0.750720
-563.231945	-6.868646	0.755725
-567.374641	-6.650402	0.760730
-570.745061	-7.056476	0.765734
-575.006360	-7.215739	0.770739
-578.520413	4.979818	0.775744
-582.229824	-6.562790	0.780749
-586.269362	8.837191	0.785754
-590.069868	1.835153	0.790758
-593.845138	-4.012347	0.795763
-597.338730	0.120563	0.800768
-601.342583	-9.272836	0.805773
-604.781478	1.907677	0.810778
-608.630016	-10.195986	0.815782
-612.253934	6.121830	0.820787
-615.877152	1.388963	0.825792
-620.129185	-7.883678	0.830797
-623.918544	-2.848215	0.835802
-627.211746	-8.433825	0.840806
-631.460660	3.852347	0.845811
-634.943457	-2.717887	0.850816
-638.514027	-3.828454	0.855821
-642.748344	1.452712	0.860826
-645.979495	-13.350088	0.865830
-650.007245	-2.004159	0.870835
-653.844612	-3.292334	0.875840
-657.643782	-4.253138	0.880845
-661.757125	4.795297	0.885850
-665.190236	-3.357532	0.890854
-668.594554	-0.152058	0.895859
-672.461347	-11.085766	0.900864
-676.237255	-11.238237	0.905869
-680.652150	-4.630618	0.910874
-683.941332	-8.871709	0.915878
-687.729096	1.355911	0.920883
-691.502652	-4.389957	0.925888
-694.809955	-2.544698	0.930893
-699.062908	2.187128	0.935898
-702.614530	-3.231319	0.940902
-706.713419	-10.901190	0.945907
-710.454813	-5.401030	0.950912
-713.728646	-11.277634	0.955917
-717.945693	1.974909	0.960922
-721.292246	-11.824012	0.965926
-725.197430	6.963284	0.970931
-729.081866	-0.765478	0.975936
-732.664975	-10.449226	0.980941
-736.258850	0.761919	0.985946
-740.242050	-8.413847	0.990950
-744.510070	2.401467	0.995955
-748.134289	-0.934636	1.000960
-751.735592	-9.217585	1.005965
-755.243338	-2.246156	1.010970
-758.714769	-8.732578	1.015974
-762.949141	-3.542866	1.020979
-766.895275	3.193576	1.025984
-770.209501	-11.860887	1.030989
-774.026816	-2.680816	1.035994
-777.631272	-7.569508	1.040998
-781.824099	0.761276	1.046003
-785.791701	-6.483846	1.051008
-789.454708	-4.843891	1.056013
-793.340167	-1.417594	1.061018
-796.732267	-2.247633	1.066022
-800.544158	6.646949	1.071027
-804.355773	-7.698081	1.076032
-807.761435	-9.634910	1.081037
-811.871080	-3.781745	1.086042
-815.151005	-11.432612	1.091046
-819.511038	-7.157919	1.096051
-823.057232	-9.258888	1.101056
-827.009760	-17.771586	1.106061
-830.599324	-3.640683	1.111066
-833.992735	-7.707853	1.116070
-837.960815	-9.153017	1.121075
-841.982604	-7.799564	1.126080
-846.052198	-4.937622	1.131085
-849.809927	1.365527	1.136090
-853.018415	-7.900478	1.141094
-856.852074	-6.454973	1.146099
-860.435850	-4.262945	1.151104
-864.383332	-4.411456	1.156109
-868.581603	-0.136062	1.161114
-871.948525	-1.099038	1.166118
-875.657662	-3.165284	1.171123
-879.662291	-6.672397	1.176128
-882.960334	0.184188	1.181133
-887.507727	-4.332558	1.186138
-890.713283	-1.321683	1.191142
-894.039159	-7.718114	1.196147
-897.906455	-2.937448	1.201152
-901.731319	-10.380626	1.206157
-906.373789	-3.547425	1.211162
-909.832075	-6.049436	1.216166
-913.734130	0.346035	1.221171
-916.977472	-2.336148	1.226176
-920.727691	-4.659754	1.231181
-924.368346	-2.752755	1.236186
-928.285219	-10.339573	1.241190
-932.508591	0.653750	1.246195
-936.013529	-9.966840	1.251200
-939.614284	-10.989479	1.256205
-943.323188	-5.697588	1.261210
-946.896386	-10.646754	1.266214
-950.946645	4.721791	1.271219
-954.820559	1.796208	1.276224
-958.122151	-3.133663	1.281229
-962.393867	6.463230	1.286234
-965.868470	0.205276	1.291238
-969.825571	4.106228	1.296243
-973.505807	2.975298	1.301248
-977.377116	-2.460254	1.306253
-981.500761	-10.746462	1.311258
-984.426829	-11.290863	1.316262
-988.546075	-4.003110	1.321267
-992.485066	0.667193	1.326272
-995.969526	-5.297747	1.331277
-1000.036742	4.149603	1.336282
-1003.568342	-10.068042	1.341286
-1007.529771	-11.292757	1.346291
-1011.297213	-3.510033	1.351296
-1015.161514	-6.119074	1.356301
-1018.986875	-10.284413	1.361306
-1022.121908	-2.976547	1.366310
-1025.884454	-3.380460	1.371315
-1029.796591	-3.984457	1.376320
-1033.462007	-2.939890	1.381325
-1037.774374	3.074986	1.386330
-1041.551531	1.477241	1.391334
-1044.987794	5.231206	1.396339
-1048.732338	2.216793	1.401344
-1051.884627	-4.217204	1.406349
-1055.993220	-1.606904	1.411354
-1060.417772	-8.375426	1.416358
-1063.988271	0.753417	1.421363
-1067.745970	2.414206	1.426368
-1071.340246	-9.160711	1.431373
-1075.067099	-1.470555	1.436378
-1078.840442	-10.095867	1.441382
-1082.738519	-3.361886	1.446387
-1086.099838	-4.290524	1.451392
-1089.999905	-3.192198	1.456397
-1094.111484	3.156910	1.461402
-1097.426627	-5.331160	1.466406
-1101.461879	1.482047	1.471411
-1105.014061	-9.110538	1.476416
-1108.946098	-10.122722	1.481421
-1113.154645	6.090171	1.486426
-1116.661855	-7.666983	1.491430
-1120.308863	-3.581534	1.496435
-1123.824728	-10.037505	1.501440
-1127.717181	-4.483043	1.506445
-1131.477472	0.766910	1.511450
-1135.001720	-10.441447	1.516454
-1139.254917	-2.556655	1.521459
-1142.977602	-4.575733	1.526464
-1146.419500	-11.340019	1.531469
-1150.530246	0.339886	1.536474
-1153.902653	-1.407386	1.541478
-1157.893793	-5.569387	1.546483
-1161.357889	-6.218231	1.551488
-1165.323931	-4.554340	1.556493
-1169.181358	2.541785	1.561498
-1172.952042	-11.599899	1.566502
-1176.826191	3.929221	1.571507
-1180.363568	-1.489669	1.576512
-1183.963501	-0.429775	1.581517
-1188.129384	4.619900	1.586522
-1191.661138	-0.997298	1.591526
-1195.099649	2.651387	1.596531
-1199.301901	-1.324332	1.601536
-1203.065958	-6.961224	1.606541
-1206.845900	-0.165720	1.611546
-1210.169222	-2.657897	1.616550
-1214.615929	-3.257540	1.621555
-1218.441527	-10.194663	1.626560
-1221.646741	-4.308577	1.631565
-1225.499480	-4.214097	1.636570
-1228.952786	-4.096641	1.641574
-1232.988276	-3.784862	1.646579
-1236.852524	3.660227	1.651584
-1240.642561	-3.268776	1.656589
-1244.570912	0.792469	1.661594
-1247.897306	-10.824729	1.666598
-1251.869892	-9.418561	1.671603
-1255.775711	-4.752542	1.676608
-1259.447826	0.420404	1.681613
-1263.008877	-0.749291	1.686618
-1266.976743	-15.155799	1.691622
-1270.953268	-5.805897	1.696627
-1274.340166	-1.858936	1.701632
-1278.023588	-7.528156	1.706637
-1281.945595	6.084289	1.711642
-1285.632836	-0.531169	1.716646
-1289.565505	1.860467	1.721651
-1293.771851	-5.255511	1.726656
-1296.994575	-6.833784	1.731661
-1301.095107	-4.901952	1.736666
-1304.338261	-6.133318	1.741670
-1308.255031	-3.311405	1.746675
-1311.819299	-6.888994	1.751680
-1315.636611	-10.526528	1.756685
-1319.379239	-8.969548	1.761690
-1323.074351	-14.765784	1.766694
-1327.317994	-6.003454	1.771699
-1331.092492	-10.408134	1.776704
-1334.750060	-8.498281	1.781709
-1338.630560	0.215107	1.786714
-1341.745769	-5.316806	1.791718
-1345.669847	-5.626375	1.796723
-1349.370276	-1.190142	1.801728
-1353.317888	-3.054745	1.806733
-1357.352129	-7.275848	1.811738
-1361.109602	-3.057551	1.816742
-1364.547893	-1.956196	1.821747
-1368.546929	-6.039268	1.826752
-1372.493459	-5.978275	1.831757
-1376.066480	-0.194280	1.836762
-1379.692068	-6.449213	1.841766
-1383.687974	-7.086643	1.846771
-1387.638446	-3.671155	1.851776
-1390.974858	-2.337825	1.856781
-1394.894061	0.027516	1.861786
-1398.278575	-4.623684	1.866790
-1402.199615	3.016021	1.871795
-1405.682245	-1.388206	1.876800
-1409.586902	-3.055282	1.881805
-1413.729532	2.174937	1.886810
-1417.374692	-3.638083	1.891814
-1420.908103	-2.064853	1.896819
-1424.876795	0.161004	1.901824
-1428.568660	-7.549219	1.906829
-1432.627323	-6.542534	1.911834
-1436.121173	-13.279478	1.916838
-1439.847261	-1.771584	1.921843
-1443.691198	-3.372881	1.926848
-1447.142292	-4.986797	1.931853
-1451.486704	0.695324	1.936858
-1455.158860	-5.791124	1.941862
-1459.040501	-8.453207	1.946867
-1462.700128	-6.039643	1.951872
-1466.158961	-8.329920	1.956877
-1469.909172	5.213293	1.961882
-1473.550445	-13.459010	1.966886
-1477.227370	3.280559	1.971891
-1481.744927	2.360243	1.976896
-1485.334663	-2.563888	1.981901
-1489.284308	3.989450	1.986906
-1492.315501	-2.862852	1.991910
-1496.147891	-5.466657	1.996915
-1500.160056	-2.318599	2.006912
-1501.163096	-2.805086	2.016909
-1498.780112	-2.743016	2.026906
-1495.877583	-2.826325	2.036902
-1493.643095	-4.598595	2.046899
-1491.917422	-6.512668	2.056896
-1489.918427	-7.080586	2.066893
-1488.265121	-10.221996	2.076890
-1486.243494	-2.418128	2.086886
-1484.208159	-11.848532	2.096883
-1482.113173	-6.086667	2.106880
-1480.657342	-3.303552	2.116877
-1478.577178	-7.437551	2.126874
-1476.662293	-3.338211	2.136870
-1474.717729	-10.475821	2.146867
-1472.821169	-10.330168	2.156864
-1470.950465	-10.713210	2.166861
-1469.053659	-9.603287	2.176858
-1467.313176	-6.855238	2.186854
-1465.356619	-6.560620	2.196851
-1463.408625	-12.014036	2.206848
-1461.437177	-4.644169	2.216845
-1459.864510	1.657194	2.226842
-1457.562231	-7.333350	2.236838
-1455.756873	-6.679985	2.246835
-1454.070012	-3.858299	2.256832
-1452.040391	-10.696715	2.266829
-1450.302919	-6.923759	2.276826
-1448.227122	-7.029018	2.286822
-1446.783400	-6.420625	2.296819
-1444.660120	-6.228148	2.306816
-1442.629739	-7.362237	2.316813
-1440.778727	-3.451882	2.326810
-1438.790407	-3.420385	2.336806
-1437.019496	-8.761956	2.346803
-1435.110650	-0.806683	2.356800
-1433.453941	3.192386	2.366797
-1431.324752	5.507712	2.376794
-1429.520672	-2.268911	2.386790
-1427.576720	0.009472	2.396787
-1425.645547	-3.434956	2.406784
-1424.074614	0.615210	2.416781
-1422.196282	3.520607	2.426778
-1419.937064	1.118904	2.436774
-1417.939316	0.926684	2.446771
-1416.471288	-1.491651	2.456768
-1414.460431	-3.036948	2.466765
-1412.536003	0.793624	2.476762
-1410.840134	-2.035741	2.486758
-1408.702360	-6.234144	2.496755
-1406.931369	-2.295009	2.506752
-1405.070919	-0.933384	2.516749
-1403.222244	-0.462910	2.526746
-1401.338723	0.035567	2.536742
-1399.518075	-0.536845	2.546739
-1397.378664	2.552146	2.556736
-1395.735107	-0.287989	2.566733
-1393.946027	-1.913742	2.576730
-1391.849542	-4.280756	2.586726
-1390.309297	-4.124444	2.596723
-1388.369677	-0.612638	2.606720
-1386.123210	-3.655929	2.616717
-1384.371244	-2.640043	2.626714
-1382.366610	2.030420	2.636710
-1380.517092	-3.791378	2.646707
-1378.857148	-7.983171	2.656704
-1376.923747	-8.200282	2.666701
-1375.052191	-3.423568	2.676698
-1372.989210	-2.371390	2.686694
-1371.265889	-8.634691	2.696691
-1369.431489	-9.809775	2.706688
-1367.386939	-2.036256	2.716685
-1365.561209	-1.777608	2.726682
-1363.907556	-0.659461	2.736678
-1361.844442	-2.774117	2.746675
-1359.892742	-2.733920	2.756672
-1357.942057	-0.801678	2.766669
-1356.122903	-6.006465	2.776666
-1354.592077	-5.063240	2.786662
-1352.628706	-5.077212	2.796659
-1350.878468	-2.486498	2.806656
-1348.785084	-2.494741	2.816653
-1346.986471	0.036683	2.826650
-1344.848965	-8.527134	2.836646
-1342.755032	-7.659288	2.846643
-1341.353895	-4.415791	2.856640
-1339.264092	-8.039585	2.866637
-1337.534134	-9.499842	2.876634
-1335.631817	-2.600185	2.886630
-1333.643536	-2.782835	2.896627
-1331.804847	-3.448819	2.906624
-1329.862202	-5.051521	2.916621
-1327.941265	-5.545092	2.926618
-1326.430776	-5.520783	2.936614
-1324.388093	-8.097470	2.946611
-1322.125603	-9.895406	2.956608
-1320.801652	-9.392468	2.966605
-1318.632317	-8.068051	2.976602
-1316.583027	-8.096764	2.986598
-1314.816328	-4.719232	2.996595
-1313.174040	-10.099923	3.006592
-1311.078827	-10.553468	3.016589
-1309.365989	-9.805105	3.026586
-1307.147111	-11.715687	3.036582
-1305.426350	-7.316943	3.046579
-1303.841288	-9.541533	3.056576
-1302.190301	-13.933712	3.066573
-1299.830875	-14.476501	3.076570
-1297.905643	-12.029642	3.086566
-1296.371309	-10.796914	3.096563
-1294.087098	-10.225725	3.106560
-1292.302856	-11.737575	3.116557
-1290.546277	-6.630436	3.126554
-1288.691903	-11.864167	3.136550
-1286.732123	-10.642460	3.146547
-1284.932509	-11.771222	3.156544
-1283.169363	-9.490960	3.166541
-1281.093070	-8.063597	3.176538
-1279.157184	-8.375150	3.186534
-1277.401280	-12.214261	3.196531
-1275.266718	-15.254083	3.206528
-1273.663830	-8.396238	3.216525
-1271.981837	-12.834043	3.226522
-1269.839952	-10.628310	3.236518
-1267.740297	-5.190406	3.246515
-1266.167606	-11.033380	3.256512
-1264.602856	-10.233481	3.266509
-1262.357728	-7.385474	3.276506
-1260.251406	-7.764626	3.286502
-1258.765762	-12.116536	3.296499
-1256.481199	-17.647828	3.306496
-1254.895047	-11.890132	3.316493
-1253.057304	-11.367918	3.326490
-1251.384984	-16.107180	3.336486
-1249.272890	-17.695080	3.346483
-1247.447218	-18.205845	3.356480
-1245.209439	-19.782131	3.366477
-1243.564802	-13.336140	3.376474
-1241.452667	-11.011857	3.386470
-1239.882317	-10.378108	3.396467
-1237.884540	-8.535309	3.406464
-1236.230785	-14.517476	3.416461
-1233.999819	-11.587190	3.426458
-1232.608973	-5.659197	3.436454
-1230.557147	-10.755297	3.446451
-1228.337415	-7.240536	3.456448
-1226.936479	-12.387280	3.466445
-1224.867567	-6.970157	3.476442
-1222.851472	-9.360039	3.486438
-1220.901763	-4.096728	3.496435
-1219.057275	-10.666128	3.506432
-1217.632073	-6.928753	3.516429
-1215.363779	-6.361506	3.526426
-1213.480192	-2.346766	3.536422
-1211.569687	-4.696773	3.546419
-1209.383521	-7.565606	3.556416
-1207.935085	-10.564629	3.566413
-1206.074157	-4.886506	3.576410
-1204.451363	-3.274514	3.586406
-1202.680726	-8.479605	3.596403
-1200.601542	-1.282226	3.606400
-1198.358827	-1.085631	3.616397
-1196.778488	-5.087031	3.626394
-1194.749650	-5.243382	3.636390
-1192.920449	-10.176347	3.646387
-1190.991109	-2.486881	3.656384
-1189.183250	-4.637454	3.666381
-1187.356274	-3.877025	3.676378
-1185.330241	-4.063716	3.686374
-1183.428698	-6.349333	3.696371
-1181.483214	-0.022158	3.706368
-1179.830838	-1.778479	3.716365
-1178.106078	-7.132582	3.726362
-1176.125843	1.733390	3.736358
-1174.043116	-4.522404	3.746355
-1172.168064	-3.098366	3.756352
-1170.427909	-3.311047	3.766349
-1168.644229	-3.197248	3.776346
-1166.830472	1.061101	3.786342
-1164.739232	-2.628862	3.796339
-1162.757728	-2.126947	3.806336
-1160.662101	-1.873457	3.816333
-1159.058616	-0.899162	3.826330
-1157.587287	-0.326628	3.836326
-1155.191574	0.827001	3.846323
-1153.447141	-4.002076	3.856320
-1151.850107	-6.206538	3.866317
-1149.719619	-6.959307	3.876314
-1147.855538	-10.149436	3.886310
-1145.911373	-7.234268	3.896307
-1143.987407	-11.901701	3.906304
-1142.210047	-3.687750	3.916301
-1140.480318	-5.778252	3.926298
-1138.725687	-5.116037	3.936294
-1136.446693	-10.502064	3.946291
-1134.821458	-11.541933	3.956288
-1133.057693	-9.018656	3.966285
-1130.756047	-5.917860	3.976282
-1129.371406	-6.457573	3.986278
-1127.232453	-9.717816	3.996275
-1125.473123	-11.183033	4.006272
-1123.493251	-15.134845	4.016269
-1121.729912	-9.550978	4.026266
-1119.622684	-9.195124	4.036262
-1117.817583	-11.707206	4.046259
-1115.996375	-9.285475	4.056256
-1114.018951	-11.585672	4.066253
-1111.926372	-11.504341	4.076250
-1110.304367	-7.920469	4.086246
-1108.519654	-10.290723	4.096243
-1106.619098	-18.335149	4.106240
-1104.746736	-20.903828	4.116237
-1102.913832	-13.360588	4.126234
-1101.005842	-14.090145	4.136230
-1099.001743	-11.288791	4.146227
-1097.403942	-15.127561	4.156224
-1095.404904	-16.699531	4.166221
-1093.240483	-10.720148	4.176218
-1091.685517	-7.246086	4.186214
-1089.540800	-11.169280	4.196211
-1087.881085	-13.082935	4.206208
-1085.885368	-10.085296	4.216205
-1084.322857	-7.421129	4.226202
-1082.226551	-12.414143	4.236198
-1080.295128	-9.407832	4.246195
-1078.204541	-12.349507	4.256192
-1076.512780	-18.987083	4.266189
-1074.801676	-12.843302	4.276186
-1072.922775	-12.661238	4.286182
-1071.017665	-10.411582	4.296179
-1068.999930	-17.199978	4.306176
-1066.818867	-17.742443	4.316173
-1065.272096	-12.945379	4.326170
-1063.626675	-16.733428	4.336166
-1061.741455	-13.502996	4.346163
-1059.596861	-11.549365	4.356160
-1057.697592	-15.831539	4.366157
-1055.827323	-17.254913	4.376154
-1053.990852	-14.287222	4.386150
-1052.072788	-11.252126	4.396147
-1050.178436	-13.052317	4.406144
-1048.356710	-10.915196	4.416141
-1046.703573	-10.201528	4.426138
-1044.788778	-9.734344	4.436134
-1043.139723	-14.256521	4.446131
-1040.713801	-16.181571	4.456128
-1039.078134	-17.250069	4.466125
-1037.460004	-15.310371	4.476122
-1035.404644	-16.966284	4.486118
-1033.329746	-18.222829	4.496115
-1031.556717	-14.695287	4.506112
-1029.332470	-13.297152	4.516109
-1027.610667	-18.154701	4.526106
-1025.946734	-9.575410	4.536102
-1023.912259	-11.566033	4.546099
-1022.571182	-12.632952	4.556096
-1020.266848	-20.184682	4.566093
-1018.205107	-18.432590	4.576090
-1016.653244	-9.818245	4.586086
-1014.560899	-12.287520	4.596083
-1012.770010	-13.198885	4.606080
-1010.966324	-18.168105	4.616077
-1009.023096	-13.289301	4.626074
-1007.221322	-12.748156	4.636070
-1005.091899	-16.060849	4.646067
-1003.254244	-15.942020	4.656064
-1001.654094	-11.412167	4.666061
-999.640700	-13.846143	4.676058
-997.850388	-10.448019	4.686054
-996.039036	-7.656599	4.696051
-993.990171	-18.138028	4.706048
-991.884080	-19.317705	4.716045
-990.287723	-13.974643	4.726042
-988.518510	-11.934396	4.736038
-986.404231	-13.299250	4.746035
-984.445623	-18.211273	4.756032
-982.759129	-11.267662	4.766029
-980.972627	-6.604199	4.776026
-979.109112	-16.880699	4.786022
-977.229123	-13.186140	4.796019
-975.131956	-14.233068	4.806016
-973.421178	-15.241323	4.816013
-971.351316	-13.426183	4.826010
-969.523383	-10.125008	4.836006
-967.698861	-5.452257	4.846003
-965.923132	-10.683431	4.856000
-963.981867	-10.316791	4.865997
-962.381611	-4.093060	4.875994
-959.866401	-13.860561	4.885990
-958.341766	-14.817883	4.895987
-956.616221	-11.149362	4.905984
-954.720188	-10.647299	4.915981
-952.614096	-14.897357	4.925978
-950.902107	-5.906563	4.935974
-948.953966	-0.063856	4.945971
-946.938599	-6.745489	4.955968
-945.492663	-12.341728	4.965965
-943.387628	-10.985129	4.975962
-941.379533	-8.140513	4.985958
-939.806700	-10.745442	4.995955
-937.755305	-9.335367	5.005952
-935.593906	-6.477940	5.015949
-933.906735	-13.199260	5.025946
-932.311362	-4.557564	5.035942
-930.007811	-3.276534	5.045939
-928.353488	-4.476243	5.055936
-926.553396	-6.432513	5.065933
-924.333556	-0.676748	5.075930
-922.662300	-4.163292	5.085926
-920.980471	-9.289407	5.095923
-919.009188	-10.223404	5.105920
-917.036015	-6.011276	5.115917
-915.338844	-7.183162	5.125914
-913.088184	-4.833480	5.135910
-911.547737	-1.025269	5.145907
-909.772977	-6.748296	5.155904
-907.389521	3.770943	5.165901
-905.479828	5.485962	5.175898
-904.066128	-1.442134	5.185894
-902.249957	5.815587	5.195891
-900.062838	-0.882868	5.205888
-898.198203	-4.142155	5.215885
-896.168532	2.571860	5.225882
-894.142953	-3.296975	5.235878
-892.754070	2.958727	5.245875
-891.257926	1.122624	5.255872
-888.949783	-4.645719	5.265869
-887.184786	-6.695938	5.275866
-884.982997	-14.263994	5.285862
-883.217249	-15.792659	5.295859
-881.199576	-9.764251	5.305856
-879.718090	-12.204088	5.315853
-877.723651	-13.978704	5.325850
-875.857467	-7.718777	5.335846
-874.089557	-10.462297	5.345843
-871.964389	-11.114818	5.355840
-870.380590	-5.406740	5.365837
-868.076204	-10.466997	5.375834
-866.545168	-16.652064	5.385830
-864.851754	-6.243575	5.395827
-862.370405	-14.475746	5.405824
-860.684384	-14.498001	5.415821
-858.699424	-13.689853	5.425818
-857.271776	-7.962871	5.435814
-855.291823	-10.036933	5.445811
-853.341532	-14.676756	5.455808
-851.206700	-12.019050	5.465805
-849.355382	-10.226010	5.475802
-847.668762	-12.231538	5.485798
-845.754611	-13.357252	5.495795
-843.925905	-6.888922	5.505792
-841.861237	-18.683137	5.515789
-840.519625	-14.177209	5.525786
-838.368268	-15.562190	5.535782
-836.349287	-15.793350	5.545779
-834.125445	-14.906841	5.555776
-832.839599	-13.892916	5.565773
-830.755053	-15.386174	5.575770
-828.478084	-21.158222	5.585766
-826.953384	-13.680501	5.595763
-825.295995	-13.181286	5.605760
-823.494648	-20.132814	5.615757
-821.160044	-18.289532	5.625754
-819.370278	-21.348998	5.635750
-817.636268	-21.928028	5.645747
-815.610479	-19.644428	5.655744
-814.008990	-22.368843	5.665741
-812.067615	-18.831762	5.675738
-810.468743	-14.666390	5.685734
-808.245531	-15.173672	5.695731
-806.138273	-14.861931	5.705728
-804.475091	-16.123187	5.715725
-802.855602	-16.910592	5.725722
-800.806427	-12.122586	5.735718
-798.861599	-15.178625	5.745715
-796.832349	-21.623868	5.755712
-794.815524	-11.119096	5.765709
-793.282848	-12.385217	5.775706
-791.352619	-8.192135	5.785702
-789.300984	-7.554668	5.795699
-787.626290	-12.914665	5.805696
-786.207975	-15.421881	5.815693
-783.591123	-12.025622	5.825690
-782.071476	-13.185562	5.835686
-780.116355	-12.352890	5.845683
-777.939476	-13.552520	5.855680
-776.222443	-14.571653	5.865677
-774.414845	-12.632357	5.875674
-772.673264	-19.502077	5.885670
-770.677024	-12.162569	5.895667
-768.835511	-14.268162	5.905664
-766.898620	-19.100884	5.915661
-764.966836	-22.228178	5.925658
-763.194151	-14.457062	5.935654
-761.597466	-18.079348	5.945651
-759.412778	-10.950024	5.955648
-757.820275	-12.011801	5.965645
-755.612221	-12.113733	5.975642
-753.635329	-12.506387	5.985638
-751.752653	-16.348091	5.995635
-750.432247	-8.940793	6.005632
-748.232666	-15.533817	6.015629
-746.070780	-16.057021	6.025626
-744.518802	-15.235765	6.035622
-742.437323	-12.003296	6.045619
-740.565963	-13.195921	6.055616
-738.951102	-10.501872	6.065613
-737.051448	-3.094783	6.075610
-734.764205	-10.041546	6.085606
-733.178303	-14.156383	6.095603
-731.517609	-15.653127	6.105600
-729.293045	-8.309308	6.115597
-727.228117	-12.603185	6.125594
-725.325471	-8.888286	6.135590
-724.285466	-9.985253	6.145587
-722.197012	-19.492460	6.155584
-720.194519	-17.835574	6.165581
-718.161371	-11.812106	6.175578
-716.006006	-12.723065	6.185574
-714.369307	-10.180169	6.195571
-712.609170	-12.921107	6.205568
-710.630309	-7.539627	6.215565
-708.795237	-12.933841	6.225562
-707.039265	-10.871834	6.235558
-704.986233	-13.332639	6.245555
-703.313855	-12.306759	6.255552
-701.309026	-13.207290	6.265549
-699.207261	-9.232117	6.275546
-697.436277	-8.361877	6.285542
-695.476833	-6.826429	6.295539
-693.701689	-11.879560	6.305536
-692.040935	-12.233739	6.315533
-690.176306	-3.651971	6.325530
-688.123074	-7.698793	6.335526
-686.193742	-7.007880	6.345523
-684.153962	-6.890405	6.355520
-682.260945	-7.007396	6.365517
-680.618013	-8.296353	6.375514
-679.101977	-11.189833	6.385510
-677.046958	-10.712559	6.395507
-674.953255	-12.905658	6.405504
-673.013140	-5.962346	6.415501
-671.328411	-9.747128	6.425498
-669.581298	-10.595908	6.435494
-667.533002	-7.741457	6.445491
-665.259137	-11.826921	6.455488
-663.656311	-11.515491	6.465485
-662.178720	-8.638188	6.475482
-660.051002	-6.500445	6.485478
-658.188926	-4.370073	6.495475
-656.194840	-14.370889	6.505472
-654.037037	-14.890581	6.515469
-652.372976	-13.909098	6.525466
-650.654782	-16.327831	6.535462
-648.754303	-13.118397	6.545459
-646.785791	-16.471289	6.555456
-645.243884	-10.813629	6.565453
-643.390413	-12.648132	6.575450
-641.289138	-8.423861	6.585446
-639.393872	-15.687460	6.595443
-637.337175	-15.095844	6.605440
-635.519547	-11.057257	6.615437
-633.581392	-12.590512	6.625434
-632.040399	-14.310920	6.635430
-629.918157	-7.449428	6.645427
-628.058966	-5.552513	6.655424
-626.299639	-9.844493	6.665421
-624.567849	-12.646930	6.675418
-622.870317	-7.612341	6.685414
-620.696270	-6.211697	6.695411
-618.596571	-5.559079	6.705408
-616.671799	-13.362063	6.715405
-614.492638	-10.960034	6.725402
-613.066642	-9.139353	6.735398
-611.342008	-14.635120	6.745395
-609.430276	-9.264597	6.755392
-607.202464	-9.489198	6.765389
-605.531619	-13.606320	6.775386
-603.992314	-10.461356	6.785382
-601.772819	-4.367440	6.795379
-600.072084	-3.196598	6.805376
-598.164425	-5.841479	6.815373
-596.510032	-7.906990	6.825370
-594.104039	-10.662279	6.835366
-592.377637	-12.468238	6.845363
-590.642255	-9.316998	6.855360
-588.613608	-8.467213	6.865357
-586.623166	-5.624530	6.875354
-584.782190	-15.031521	6.885350
-583.184754	-5.388152	6.895347
-580.990861	-9.946758	6.905344
-579.236744	-9.113096	6.915341
-577.804617	-6.858720	6.925338
-575.519780	-18.056700	6.935334
-573.617484	-20.144189	6.945331
-572.201226	-19.024908	6.955328
-569.953055	-13.869392	6.965325
-567.697047	-16.385120	6.975322
-566.167250	-21.001682	6.985318
-564.325144	-16.121112	6.995315
-562.503036	-12.556330	7.005312
-560.576151	-18.751927	7.015309
-558.471645	-14.653451	7.025306
-557.007653	-14.060875	7.035302
-554.729379	-16.165048	7.045299
-552.952960	-15.142339	7.055296
-551.280456	-11.047590	7.065293
-549.202770	-12.490534	7.075290
-547.340034	-13.010527	7.085286
-545.965381	-11.494418	7.095283
-543.695299	-14.387608	7.105280
-541.494721	-9.112457	7.115277
-540.017554	-10.674863	7.125274
-538.185639	-10.059254	7.135270
-535.829244	-11.852352	7.145267
-534.454722	-16.390490	7.155264
-532.398839	-18.692041	7.165261
-530.454634	-12.883227	7.175258
-528.531645	-14.220577	7.185254
-526.910868	-13.552927	7.195251
-524.839781	-7.418486	7.205248
-522.985004	-8.898658	7.215245
-521.030967	-11.108430	7.225242
-519.188045	-8.950997	7.235238
-517.585887	-5.833777	7.245235
-515.710727	-9.939685	7.255232
-513.313530	-6.570380	7.265229
-511.797963	-12.540859	7.275226
-510.006384	-13.976985	7.285222
-507.952795	-7.234065	7.295219
-505.941874	-8.071924	7.305216
-504.415774	-11.995026	7.315213
-502.336518	-10.463842	7.325210
-500.498525	-6.923888	7.335206
-498.496100	-11.062691	7.345203
-496.744914	-13.758540	7.355200
-494.999096	-5.096609	7.365197
-492.730258	-5.384312	7.375194
-491.094671	-3.608639	7.385190
-489.675781	-1.586322	7.395187
-486.965360	-6.291604	7.405184
-485.138632	-7.497018	7.415181
-483.922550	-3.847192	7.425178
-481.883789	-6.456423	7.435174
-479.815238	-4.593386	7.445171
-478.024252	-12.290769	7.455168
-476.010564	-2.388760	7.465165
-474.274781	-5.061013	7.475162
-472.104395	-8.633826	7.485158
-470.757440	-3.241030	7.495155
-468.503211	-1.689260	7.505152
-466.776285	-9.695377	7.515149
-464.895005	-11.343691	7.525146
-463.010894	-11.814358	7.535142
-461.138458	-10.554751	7.545139
-459.026094	-7.841608	7.555136
-457.339183	-9.127754	7.565133
-455.524430	-15.691385	7.575130
-453.655451	-6.830035	7.585126
-451.737573	-13.169882	7.595123
-449.898367	-4.555173	7.605120
-447.880705	-9.439967	7.615117
-445.856412	-8.662878	7.625114
-444.225744	-14.418328	7.635110
-442.416397	-3.622049	7.645107
-440.634780	-10.920623	7.655104
-438.474641	-9.508806	7.665101
-436.604188	-6.431654	7.675098
-434.926841	-9.843193	7.685094
-432.909178	-2.943096	7.695091
-431.159176	-3.135828	7.705088
-429.016451	-2.987284	7.715085
-427.371668	-4.610818	7.725082
-425.062509	-7.990841	7.735078
-423.882346	-6.205382	7.745075
-421.525494	-2.753219	7.755072
-419.753258	-7.022443	7.765069
-417.792116	-9.868105	7.775066
-416.060489	-5.338033	7.785062
-414.075868	-4.021375	7.795059
-412.496701	-3.908143	7.805056
-410.565052	-5.132317	7.815053
-408.533501	-3.156980	7.825050
-406.552743	-5.772432	7.835046
-404.979122	-7.388493	7.845043
-403.056871	-4.482249	7.855040
-400.843083	-7.479535	7.865037
-399.069297	-5.449699	7.875034
-397.323226	-5.875316	7.885030
-395.362282	-5.786864	7.895027
-393.296115	-12.786053	7.905024
-391.582456	-7.530043	7.915021
-390.020130	-11.979822	7.925018
-388.144390	-11.622234	7.935014
-385.909763	-12.299623	7.945011
-383.998142	-18.558537	7.955008
-382.351022	-12.500682	7.965005
-380.626427	-9.246326	7.975002
-378.723431	-10.986463	7.984998
-376.588021	-10.430358	7.994995
-374.628100	-13.550466	8.004992
-372.785068	-3.698167	8.014989
-370.906490	-8.629420	8.024986
-369.074118	-9.125950	8.034982
-367.480960	-0.133451	8.044979
-365.365162	-3.409927	8.054976
-363.530983	-4.313441	8.064973
-361.735486	-9.624467	8.074970
-359.744131	-10.185811	8.084966
-357.863859	-6.264550	8.094963
-356.182335	-12.263060	8.104960
-354.266796	-9.869817	8.114957
-352.204570	-10.461100	8.124954
-350.205287	-9.740935	8.134950
-348.440956	-10.185869	8.144947
-346.886217	-8.940877	8.154944
-344.896011	-5.255834	8.164941
-342.649918	-5.798820	8.174938
-340.922697	-7.831680	8.184934
-339.207489	-8.118002	8.194931
-337.324221	-6.470913	8.204928
-335.200945	-12.987044	8.214925
-333.288783	-9.279520	8.224922
-331.838896	-15.724795	8.234918
-329.663757	-10.611154	8.244915
-328.026105	-12.452773	8.254912
-326.043176	-6.211018	8.264909
-324.330600	-14.926806	8.274906
-322.136433	-9.046941	8.284902
-319.975351	-6.453139	8.294899
-318.604954	-10.250674	8.304896
-316.552208	-8.785990	8.314893
-314.775225	-10.905233	8.324890
-312.827430	-7.695458	8.334886
-310.879938	-9.917062	8.344883
-309.072828	-4.290129	8.354880
-307.142216	-3.119081	8.364877
-305.326343	-11.829661	8.374874
-303.647071	-13.309281	8.384870
-301.525451	-13.797698	8.394867
-299.893901	-6.945519	8.404864
-297.971982	-7.973136	8.414861
-295.902645	-9.818443	8.424858
-293.904782	-10.266263	8.434854
-292.199214	-4.832159	8.444851
-290.430530	-4.556154	8.454848
-288.440002	-9.001495	8.464845
-286.563461	-9.436801	8.474842
-284.702027	-3.438978	8.484838
-282.584921	-10.019635	8.494835
-280.931478	-7.245075	8.504832
-279.053088	-9.395136	8.514829
-276.986322	-14.840398	8.524826
-275.196511	-15.436298	8.534822
-273.554684	-9.042344	8.544819
-271.815439	-10.297482	8.554816
-269.719178	-7.465288	8.564813
-267.780645	-11.855857	8.574810
-266.065896	-11.931818	8.584807
-264.003062	-10.700831	8.594803
-262.115460	-7.313137	8.604800
-260.191085	-8.533628	8.614797
-258.502375	-5.226035	8.624794
-256.672098	-5.034091	8.634791
-254.642782	-4.726105	8.644787
-253.047770	-13.722466	8.654784
-250.966659	-8.563012	8.664781
-248.778100	-7.319989	8.674778
-246.912433	-14.155891	8.684775
-245.456503	-7.508324	8.694771
-243.506205	-4.487067	8.704768
-242.091794	-7.747130	8.714765
-239.748601	-9.716055	8.724762
-237.483676	-12.347767	8.734759
-235.616367	-6.591615	8.744755
-234.262804	-0.349758	8.754752
-232.568053	1.560122	8.764749
-230.152429	-4.740527	8.774746
-228.036723	-5.771315	8.784743
-226.289071	0.956650	8.794739
-224.691070	-1.118821	8.804736
-223.147902	-0.966940	8.814733
-220.720967	2.860233	8.824730
-219.152727	-4.490995	8.834727
-217.064404	-11.872532	8.844723
-215.060158	-1.371982	8.854720
-213.376401	-5.256038	8.864717
-211.515963	-11.591086	8.874714
-209.613146	-9.073473	8.884711
-207.779154	-7.148735	8.894707
-205.915114	-3.955371	8.904704
-204.046357	-3.712304	8.914701
-202.195217	-1.411492	8.924698
-200.112460	-2.769388	8.934695
-198.222334	1.551798	8.944691
-196.506121	2.721726	8.954688
-194.828770	4.174575	8.964685
-192.817594	2.009282	8.974682
-190.884473	-0.066741	8.984679
-189.230921	-3.957465	8.994675
-187.260625	-1.428492	9.004672
-185.240790	-4.564334	9.014669
-183.388172	-8.039046	9.024666
-181.436979	-4.976416	9.034663
-179.494271	-3.122083	9.044659
-177.799375	-11.179136	9.054656
-176.054359	-11.369334	9.064653
-174.024882	-14.017151	9.074650
-171.999251	-9.519216	9.084647
-169.957955	-14.941492	9.094643
-168.418639	-12.689155	9.104640
-166.653972	-9.828497	9.114637
-164.626172	-4.960613	9.124634
-162.735585	-6.029040	9.134631
-161.114033	-10.365601	9.144627
-159.013999	-8.465917	9.154624
-157.007436	-9.091434	9.164621
-155.353990	-5.436284	9.174618
-153.109263	-4.128940	9.184615
-151.550545	0.358973	9.194611
-149.775920	-5.837241	9.204608
-148.027326	-1.883814	9.214605
-145.758741	-1.330280	9.224602
-144.053261	-3.289388	9.234599
-141.878472	-3.140276	9.244595
-140.193288	-9.537725	9.254592
-138.612493	-0.027641	9.264589
-136.510057	-2.629464	9.274586
-134.750245	-8.095937	9.284583
-132.818960	-3.672700	9.294579
-131.006971	-1.452486	9.304576
-129.105074	-11.885490	9.314573
-126.913203	-5.283064	9.324570
-125.087632	-6.241127	9.334567
-122.981877	-1.280671	9.344563
-121.410492	-2.269838	9.354560
-120.014512	1.170219	9.364557
-117.849736	-7.564965	9.374554
-115.736443	-6.520407	9.384551
-113.751721	1.714619	9.394547
-112.056600	2.313158	9.404544
-110.155108	-0.938313	9.414541
-108.262707	-6.569397	9.424538
-106.603385	-4.053455	9.434535
-104.678429	1.306752	9.444531
-102.611508	-0.540824	9.454528
-101.038533	-5.258720	9.464525
-98.930128	-0.019684	9.474522
-97.003585	0.981817	9.484519
-95.173835	-0.375329	9.494515
-93.205096	2.147237	9.504512
-91.579172	-0.286301	9.514509
-89.521751	-0.483402	9.524506
-87.647424	-4.831671	9.534503
-86.103621	-2.005033	9.544499
-83.896544	1.786411	9.554496
-82.176597	4.324771	9.564493
-80.431259	-2.411403	9.574490
-78.236668	-5.557802	9.584487
-76.317394	-4.249544	9.594483
-74.512897	-0.831308	9.604480
-72.853044	-0.708474	9.614477
-70.839441	-8.709885	9.624474
-68.713972	-9.207153	9.634471
-66.918705	-4.988206	9.644467
-65.260534	5.649240	9.654464
-63.396162	4.924047	9.664461
-61.443613	-1.774143	9.674458
-59.319397	-5.326604	9.684455
-57.710526	5.419288	9.694451
-55.886178	1.338466	9.704448
-54.014133	1.484994	9.714445
-52.119037	-3.927189	9.724442
-50.198495	-7.625334	9.734439
-48.698568	-6.422214	9.744435
-46.419645	-7.197932	9.754432
-44.473426	0.154101	9.764429
-42.621795	-1.445487	9.774426
-40.667348	-6.815277	9.784423
-38.876758	-8.852571	9.794419
-37.100142	-3.798088	9.804416
-35.193548	-1.979785	9.814413
-33.137475	-0.074081	9.824410
-31.407388	-7.480280	9.834407
-29.581325	-13.416922	9.844403
-27.831184	-8.023939	9.854400
-25.654652	-8.445367	9.864397
-24.101346	-7.147054	9.874394
-22.084645	-6.634054	9.884391
-19.994762	-7.295535	9.894387
-18.322300	-5.116165	9.904384
-16.293548	-3.358717	9.914381
-14.707669	-2.862346	9.924378
-12.511343	-8.329325	9.934375
-10.663784	-11.096459	9.944371
-8.897532	-7.053125	9.954368
-7.115825	-0.422194	9.964365
-5.705801	14.417088	9.974362
-4.255052	32.512313	9.984359
-2.833730	74.205912	9.994355
-1.028396	116.812737	10.004352
0.000000	159.644890	10.009357
0.897811	186.228943	10.014362
1.890070	217.379107	10.019367
1.715836	239.688356	10.024371
2.340907	259.285449	10.029376
2.733725	268.677495	10.034381
2.520411	274.605229	10.039386
2.842033	274.316803	10.044391
2.843151	298.396376	10.049395
3.469281	304.063745	10.054400
3.440396	310.182096	10.059405
3.225437	316.519845	10.064410
3.625805	315.435585	10.069415
3.689936	320.115819	10.074419
3.593398	313.586356	10.079424
3.443968	310.162926	10.084429
3.319256	307.085768	10.089434
3.691835	323.602040	10.094439
3.433425	330.591426	10.099443
3.838627	325.386260	10.104448
3.839828	331.242892	10.109453
3.826749	336.315696	10.114458
3.810402	333.846766	10.119463
3.475373	339.690398	10.124467
4.106841	337.595502	10.129472
3.870115	336.712448	10.134477
4.018667	342.406457	10.139482
4.054586	337.141058	10.144487
3.866545	353.940979	10.149491
4.237168	345.716209	10.154496
4.098623	350.624222	10.159501
4.435604	348.690734	10.164506
4.662890	342.716366	10.169511
4.573681	343.980553	10.174515
4.690587	331.159763	10.179520
4.123903	324.761037	10.184525
4.229315	327.912949	10.189530
4.440140	322.215346	10.194535
4.443210	337.733591	10.199539
4.655496	348.721308	10.204544
4.645569	351.900501	10.209549
5.051004	353.873657	10.214554
4.706677	330.080201	10.219559
4.493869	338.119619	10.224563
4.635392	337.168551	10.229568
4.965523	352.341008	10.234573
4.696274	349.002848	10.239578
5.157576	357.459956	10.244583
5.121540	357.595602	10.249587
5.073009	351.520109	10.254592
4.560095	346.770765	10.259597
5.000216	354.967832	10.264602
5.062605	364.849600	10.269607
5.274585	371.337974	10.274611
5.527532	376.773317	10.279616
5.230148	373.621547	10.284621
5.135451	372.310734	10.289626
5.461772	362.507961	10.294631
5.161531	379.220178	10.299635
5.355556	378.317340	10.304640
5.077582	379.230228	10.309645
5.040585	375.376996	10.314650
5.415877	377.219540	10.319655
5.463067	381.302328	10.324659
5.616361	383.818042	10.329664
5.229742	385.983454	10.334669
5.221201	387.544063	10.339674
5.800439	391.561285	10.344679
5.771122	405.700866	10.349683
5.698342	410.419997	10.354688
5.774802	417.241877	10.359693
5.627052	421.198633	10.364698
6.138474	414.419628	10.369703
5.533152	418.188403	10.374707
6.014217	419.927161	10.379712
5.999878	417.618920	10.384717
5.581648	424.916793	10.389722
5.732114	425.311766	10.394727
6.157061	450.737927	10.399731
6.307009	445.032166	10.404736
6.292783	449.759426	10.409741
6.232583	454.796138	10.414746
6.347655	455.486117	10.419751
6.289570	459.721182	10.424755
6.914228	450.341262	10.429760
6.719912	456.145022	10.434765
6.723958	458.012547	10.439770
6.869044	458.231213	10.444775
6.692684	457.488584	10.449779
6.728038	454.841040	10.454784
7.006407	460.361261	10.459789
7.004483	462.945048	10.464794
7.159923	457.247814	10.469799
6.282015	461.774232	10.474803
6.923174	456.382123	10.479808
6.984652	464.442862	10.484813
6.530014	465.720376	10.489818
6.968675	468.128755	10.494823
6.717127	471.919775	10.499827
6.989713	472.908788	10.504832
7.067193	468.415401	10.509837
6.823782	473.011050	10.514842
7.059847	479.845458	10.519847
7.301093	495.968394	10.524851
7.622104	495.657571	10.529856
7.372538	502.370000	10.534861
7.231713	509.607717	10.539866
7.609911	502.729942	10.544871
7.291328	509.749856	10.549875
7.478414	508.635445	10.554880
7.582108	510.389973	10.559885
7.640397	507.907429	10.564890
7.666128	504.946932	10.569895
7.374784	508.172435	10.574899
7.719189	503.648665	10.579904
7.666880	513.385989	10.584909
7.110381	515.563573	10.589914
7.643606	514.355076	10.594919
7.998994	536.112506	10.599923
8.093591	539.158556	10.604928
8.147939	545.211808	10.609933
8.350837	542.242636	10.614938
8.472675	535.405250	10.619943
8.079931	546.841836	10.624947
8.470977	548.208030	10.629952
8.711679	548.821605	10.634957
8.377403	558.314813	10.639962
8.361977	550.926631	10.644967
8.532612	562.085846	10.649971
8.294139	551.988228	10.654976
8.608601	552.956251	10.659981
8.325633	557.102010	10.664986
8.576387	553.536491	10.669991
8.267416	557.522109	10.674995
8.616063	554.741491	10.680000
8.362298	556.441660	10.685005
8.581856	562.345411	10.690010
8.719678	558.518605	10.695015
8.539672	559.292735	10.700019
8.742504	565.394349	10.705024
8.733124	578.634247	10.710029
8.921738	583.374925	10.715034
9.399475	587.608544	10.720039
9.212140	588.436036	10.725043
9.396648	588.347953	10.730048
8.971464	580.543318	10.735053
9.111871	590.096862	10.740058
9.352068	589.554769	10.745063
9.417894	586.705799	10.750067
9.277666	591.914562	10.755072
9.149215	598.017730	10.760077
9.531920	599.372728	10.765082
9.637357	595.606332	10.770087
9.270361	607.906154	10.775091
9.415035	599.783149	10.780096
9.354429	606.874923	10.785101
9.193806	606.789176	10.790106
9.545040	600.892929	10.795111
9.223723	598.756898	10.800115
9.436675	618.515106	10.805120
9.991914	624.323036	10.810125
9.744375	631.961991	10.815130
10.315813	622.037688	10.820135
10.042151	630.817144	10.825139
9.914576	627.424632	10.830144
10.195514	637.389492	10.835149
9.962420	636.275671	10.840154
10.133651	636.604328	10.845159
10.206345	637.603152	10.850163
10.162606	634.835722	10.855168
10.477158	635.671896	10.860173
9.868550	642.474367	10.865178
10.198468	642.450560	10.870183
9.920124	639.745458	10.875187
10.502242	633.018974	10.880192
10.530412	642.699554	10.885197
10.072580	647.681352	10.890202
10.089160	642.890470	10.895207
10.369519	667.344696	10.900211
10.633094	669.983650	10.905216
10.700671	674.731688	10.910221
10.598036	675.832812	10.915226
10.553037	674.653580	10.920231
11.013341	682.244217	10.925235
10.806335	678.278747	10.930240
11.044316	679.816063	10.935245
10.065182	680.728008	10.940250
10.561788	682.162166	10.945255
10.913749	695.189026	10.950259
10.978440	705.111273	10.955264
11.066573	709.946190	10.960269
10.839035	710.982287	10.965274
11.355829	708.741221	10.970279
10.885968	714.966919	10.975283
11.131310	711.598867	10.980288
11.279771	714.717819	10.985293
11.305962	720.511104	10.990298
11.320715	713.842393	10.995303
11.568098	716.192032	11.000307
11.420517	709.476158	11.005312
11.287974	717.292801	11.010317
11.376853	722.437851	11.015322
12.026235	729.761623	11.020327
11.552405	740.237270	11.025331
11.819568	740.645400	11.030336
11.984723	741.375751	11.035341
11.578980	741.744129	11.040346
11.831568	738.288383	11.045351
11.783926	751.523542	11.050355
11.744307	741.549992	11.055360
11.618524	735.600882	11.060365
11.464485	746.837608	11.065370
11.842655	739.055804	11.070375
11.911967	753.668648	11.075379
11.874287	759.336717	11.080384
12.411284	773.417819	11.085389
12.228357	777.171095	11.090394
12.419965	775.298402	11.095399
12.177757	785.907653	11.100403
12.172129	781.450136	11.105408
12.335413	786.457320	11.110413
12.152379	790.212985	11.115418
12.375892	783.885023	11.120423
12.391370	783.325403	11.125427
12.609635	781.907211	11.130432
12.913070	779.574036	11.135437
12.825234	786.278592	11.140442
13.372042	785.497609	11.145447
12.877624	786.320133	11.150451
13.354103	788.152482	11.155456
13.036198	781.316574	11.160461
12.819755	791.484838	11.165466
13.175696	784.234184	11.170471
12.708183	796.825332	11.175475
13.028878	796.689819	11.180480
13.089192	797.709724	11.185485
12.984034	798.306428	11.190490
12.936892	793.005381	11.195495
12.398543	805.134214	11.200499
12.913914	812.743104	11.205504
13.154547	824.042476	11.210509
13.166618	830.567291	11.215514
13.456083	830.664499	11.220519
13.176981	836.306885	11.225523
12.909406	825.126989	11.230528
13.054237	841.117211	11.235533
13.420962	861.892638	11.240538
13.455649	864.744158	11.245543
13.529214	872.754089	11.250547
13.769271	862.502774	11.255552
13.673038	869.437751	11.260557
13.593509	870.123221	11.265562
13.830771	861.385396	11.270567
13.836478	866.502124	11.275571
13.725224	860.638499	11.280576
13.758161	866.140948	11.285581
13.761639	869.669655	11.290586
13.912053	883.127542	11.295591
14.142701	896.903260	11.300595
14.519445	892.252256	11.305600
14.308031	892.717185	11.310605
14.152701	900.139540	11.315610
14.104393	900.928605	11.320615
14.007205	900.020407	11.325619
13.961558	900.942435	11.330624
14.494810	903.087957	11.335629
13.953462	909.024017	11.340634
14.286507	907.476792	11.345639
14.396861	903.152116	11.350643
14.136468	905.432532	11.355648
14.650813	925.815237	11.360653
14.673316	934.955000	11.365658
14.652123	934.061007	11.370663
14.693094	940.203153	11.375667
14.675288	932.736252	11.380672
14.763817	932.649230	11.385677
14.312124	943.527398	11.390682
14.830836	936.473370	11.395687
14.999313	946.589157	11.400691
15.186644	945.916382	11.405696
15.163149	946.589484	11.410701
14.722224	948.997571	11.415706
15.278209	948.576979	11.420711
15.373317	947.171600	11.425715
15.232101	948.584883	11.430720
14.715107	948.847603	11.435725
15.021633	962.178529	11.440730
15.132183	970.689799	11.445735
15.162027	979.117016	11.450739
15.188541	973.850647	11.455744
15.130466	975.822832	11.460749
14.961102	992.015501	11.465754
15.631760	989.868409	11.470759
15.466260	1005.492010	11.475763
15.757101	1010.715816	11.480768
16.120096	1011.686601	11.485773
15.713397	1017.011062	11.490778
15.886325	1014.618519	11.495783
15.673126	1022.589275	11.500787
15.951883	1018.575166	11.505792
15.577707	1010.980647	11.510797
15.757092	1018.344878	11.515802
15.847059	1019.283529	11.520807
15.548001	1019.120463	11.525811
15.819954	1021.410673	11.530816
16.016293	1036.401080	11.535821
16.385655	1044.223408	11.540826
16.728718	1041.920900	11.545831
16.283623	1047.438665	11.550835
16.148662	1044.978513	11.555840
16.441863	1040.543106	11.560845
16.307152	1045.232389	11.565850
16.468530	1045.444718	11.570855
16.337078	1058.169901	11.575859
16.299427	1050.017924	11.580864
16.569002	1051.908677	11.585869
16.228180	1058.483043	11.590874
16.679022	1053.365733	11.595879
16.246262	1056.531121	11.600883
16.706408	1059.100517	11.605888
17.252843	1070.117108	11.610893
16.618465	1069.479033	11.615898
16.682191	1065.009939	11.620903
16.610367	1087.333232	11.625907
16.745695	1084.732387	11.630912
16.814498	1079.938733	11.635917
16.822012	1084.880747	11.640922
17.291534	1078.851145	11.645927
16.968137	1088.973599	11.650931
17.039196	1087.809568	11.655936
16.982256	1087.741566	11.660941
17.113665	1097.164726	11.665946
17.644069	1109.087649	11.670951
17.524958	1117.848772	11.675955
17.704626	1115.496901	11.680960
17.602646	1105.188809	11.685965
17.317792	1102.078951	11.690970
17.768132	1107.177547	11.695975
17.849414	1120.476571	11.700979
17.677196	1111.838422	11.705984
17.909720	1108.365509	11.710989
17.286669	1104.655608	11.715994
17.871366	1107.835633	11.720999
18.082048	1119.036933	11.726003
17.874293	1118.755973	11.731008
17.997596	1122.843274	11.736013
17.606775	1119.319342	11.741018
18.084159	1110.511786	11.746023
17.971649	1122.244558	11.751027
17.737243	1117.815513	11.756032
18.059848	1124.410761	11.761037
17.695846	1127.982402	11.766042
17.608325	1124.276202	11.771047
17.971324	1140.943407	11.776051
18.169919	1145.632808	11.781056
18.258949	1152.637987	11.786061
18.186310	1158.737330	11.791066
18.469174	1156.514996	11.796071
18.160636	1166.063763	11.801075
18.285647	1161.797292	11.806080
18.658823	1155.519705	11.811085
18.575876	1167.305468	11.816090
18.384231	1162.154204	11.821095
18.314231	1168.258624	11.826099
18.672846	1185.804531	11.831104
18.930123	1180.708528	11.836109
18.692424	1190.236478	11.841114
19.030050	1186.409604	11.846119
18.952638	1190.770155	11.851123
18.957726	1196.344601	11.856128
18.928716	1189.033448	11.861133
18.982165	1192.449448	11.866138
19.055660	1183.751366	11.871143
19.093386	1196.254230	11.876147
19.074747	1189.247617	11.881152
19.011058	1192.517121	11.886157
19.201187	1189.854363	11.891162
19.014145	1183.333737	11.896167
19.202090	1202.881050	11.901171
19.219500	1214.292401	11.906176
19.694923	1219.673710	11.911181
19.519824	1221.645860	11.916186
19.422021	1221.183806	11.921191
19.344522	1226.636632	11.926195
19.539242	1222.465563	11.931200
19.485589	1227.025737	11.936205
19.706513	1226.237453	11.941210
20.082475	1211.898348	11.946215
20.303044	1222.058673	11.951219
19.918361	1218.195767	11.956224
20.120929	1218.632750	11.961229
19.436423	1225.055715	11.966234
19.861148	1221.883775	11.971239
19.368856	1233.708984	11.976243
19.813948	1226.907452	11.981248
19.724549	1231.969947	11.986253
19.753464	1253.979359	11.991258
20.105579	1250.785914	11.996263
20.454490	1258.534883	12.001267
20.486436	1250.325079	12.006272
20.391887	1258.706669	12.011277
20.435117	1259.827430	12.016282
20.506851	1256.840745	12.021287
20.699664	1266.131503	12.026291
20.734210	1259.587457	12.031296
20.303838	1240.860463	12.036301
19.924685	1240.792048	12.041306
20.411271	1241.756263	12.046311
20.879322	1253.348537	12.051315
20.821913	1247.102109	12.056320
20.579640	1241.612916	12.061325
20.517587	1241.281707	12.066330
20.556366	1227.682516	12.071335
20.406658	1236.509741	12.076339
20.691588	1236.929840	12.081344
20.517933	1226.940672	12.086349
20.378853	1231.676944	12.091354
20.388695	1240.780767	12.096359
20.423966	1239.064696	12.101363
20.253446	1234.417424	12.106368
20.405308	1241.686216	12.111373
20.477755	1242.265907	12.116378
20.259845	1235.101201	12.121383
20.472208	1244.882416	12.126387
20.231375	1242.177882	12.131392
20.445382	1235.693867	12.136397
19.900817	1241.509416	12.141402
20.490102	1244.637367	12.146407
20.110950	1246.007787	12.151411
20.321680	1243.847941	12.156416
20.139328	1248.319266	12.161421
19.863188	1244.812353	12.166426
19.989289	1237.776165	12.171431
19.980007	1249.107248	12.176435
19.741017	1246.013576	12.181440
20.547565	1254.873434	12.186445
20.500190	1273.946440	12.191450
20.597726	1253.970345	12.196455
20.239415	1251.953856	12.201459
20.142066	1246.960083	12.206464
20.529321	1259.238855	12.211469
20.005638	1256.958216	12.216474
20.727890	1258.195055	12.221479
20.248871	1263.681606	12.226483
20.079465	1259.108743	12.231488
20.602255	1268.808721	12.236493
20.521572	1276.362141	12.241498
20.496776	1247.290050	12.246503
20.476217	1248.317930	12.251507
20.550818	1236.983935	12.256512
20.373966	1259.389430	12.261517
20.247776	1253.245583	12.266522
20.522665	1252.220278	12.271527
20.607541	1251.905720	12.276531
20.460088	1248.987013	12.281536
20.770043	1248.650048	12.286541
20.496600	1252.908436	12.291546
20.687744	1259.923393	12.296551
20.755801	1259.785800	12.301555
20.735493	1252.744707	12.306560
20.307156	1231.413655	12.311565
20.250169	1228.531942	12.316570
20.680770	1225.269782	12.321575
20.294791	1224.649899	12.326579
19.858258	1229.194011	12.331584
20.437041	1224.849720	12.336589
20.619819	1243.098085	12.341594
20.653001	1230.772105	12.346599
20.361234	1232.362807	12.351603
20.546398	1224.251879	12.356608
20.556826	1223.337052	12.361613
19.985528	1221.443929	12.366618
20.701978	1214.494822	12.371623
20.842840	1228.659653	12.376627
20.750679	1222.211955	12.381632
20.259227	1228.596294	12.386637
20.108461	1235.023276	12.391642
20.485950	1219.172436	12.396647
19.974581	1230.750648	12.401651
20.304807	1224.363949	12.406656
20.369921	1222.118941	12.411661
20.310194	1228.353466	12.416666
20.446608	1232.760262	12.421671
20.432170	1228.518079	12.426675
20.374529	1229.189942	12.431680
20.463222	1219.089481	12.436685
20.706880	1230.947188	12.441690
20.567839	1231.619983	12.446695
20.474880	1233.267388	12.451699
20.382280	1229.886906	12.456704
20.635381	1231.761558	12.461709
20.306633	1240.532641	12.466714
20.989479	1223.313371	12.471719
20.731468	1222.449703	12.476723
20.791674	1215.468244	12.481728
19.998436	1206.280857	12.486733
20.197761	1207.946040	12.491738
20.240410	1201.939451	12.496743
20.085002	1205.148104	12.501747
20.369717	1203.649401	12.506752
20.583445	1200.630486	12.511757
20.115576	1210.206203	12.516762
20.112124	1203.414088	12.521767
19.928942	1218.753167	12.526771
20.257214	1226.058811	12.531776
20.373878	1241.008601	12.536781
20.228273	1236.732457	12.541786
20.562105	1236.735218	12.546791
20.529303	1241.737090	12.551795
20.438750	1239.098370	12.556800
20.539051	1242.483452	12.561805
20.256405	1231.535982	12.566810
20.464527	1212.184409	12.571815
20.237681	1213.275288	12.576819
20.181606	1214.616364	12.581824
20.449317	1225.748356	12.586829
20.446682	1239.020816	12.591834
20.862356	1231.947217	12.596839
20.592021	1216.119824	12.601843
20.874191	1213.513518	12.606848
20.888443	1207.765219	12.611853
20.612882	1219.078383	12.616858
20.977980	1210.310946	12.621863
20.361437	1200.406811	12.626867
20.068257	1195.810977	12.631872
20.500941	1198.520501	12.636877
20.244457	1200.949502	12.641882
20.633531	1200.542523	12.646887
20.459989	1189.901642	12.651891
20.283446	1185.891740	12.656896
20.261194	1180.514056	12.661901
19.936201	1184.877581	12.666906
20.551986	1195.266181	12.671911
20.471775	1207.550852	12.676915
20.097947	1199.252752	12.681920
20.357608	1206.404360	12.686925
20.065260	1218.646464	12.691930
20.887216	1207.525801	12.696935
20.306678	1212.102494	12.701939
19.956739	1203.328580	12.706944
20.395151	1211.134811	12.711949
20.383532	1213.671831	12.716954
20.432789	1224.881937	12.721959
20.409813	1220.441085	12.726963
20.779864	1216.181534	12.731968
20.585399	1202.005770	12.736973
20.296024	1194.846231	12.741978
20.486473	1192.502763	12.746983
20.513288	1189.183526	12.751987
20.397075	1189.544901	12.756992
20.574954	1179.818387	12.761997
20.144956	1187.432447	12.767002
20.277348	1189.925034	12.772007
20.488771	1194.082509	12.777011
20.422781	1192.189593	12.782016
20.272424	1186.463604	12.787021
19.962388	1189.466264	12.792026
19.999626	1190.535547	12.797031
20.262912	1194.757156	12.802035
20.160431	1197.698967	12.807040
20.389102	1213.203085	12.812045
20.274738	1232.546477	12.817050
20.386457	1229.522151	12.822055
20.611025	1222.253163	12.827059
20.349217	1209.043425	12.832064
20.229060	1200.806831	12.837069
20.298826	1210.412735	12.842074
20.614731	1216.116267	12.847079
20.203320	1213.347036	12.852083
20.063489	1200.161786	12.857088
20.514534	1207.567162	12.862093
20.674266	1221.331247	12.867098
20.416779	1210.224344	12.872103
20.051903	1192.368425	12.877107
20.230284	1198.378164	12.882112
20.578293	1210.857050	12.887117
20.151724	1209.271485	12.892122
20.398903	1214.032315	12.897127
20.482311	1227.635806	12.902131
20.492410	1224.015476	12.907136
20.148066	1203.240068	12.912141
20.011683	1213.981859	12.917146
20.319734	1220.692540	12.922151
20.234073	1231.785256	12.927155
20.401342	1232.688165	12.932160
20.711715	1229.793991	12.937165
20.220639	1235.610235	12.942170
20.792434	1230.483579	12.947175
20.274841	1218.014409	12.952179
20.335105	1206.139730	12.957184
20.933716	1196.261330	12.962189
20.458091	1197.885921	12.967194
20.460094	1194.680281	12.972199
20.453956	1202.048382	12.977203
20.451148	1200.365292	12.982208
20.557456	1200.735489	12.987213
19.957888	1200.190914	12.992218
20.516004	1193.525545	12.997223
20.162316	1203.404579	13.002227
20.312169	1206.669841	13.007232
20.351176	1194.008150	13.012237
20.115930	1202.698837	13.017242
20.007274	1194.174482	13.022247
20.121996	1206.141121	13.027251
20.389939	1212.435512	13.032256
20.393392	1197.102779	13.037261
20.361937	1201.666246	13.042266
20.532871	1207.747134	13.047271
20.333842	1201.127502	13.052275
20.318693	1202.606430	13.057280
20.411848	1199.200026	13.062285
20.410551	1197.789837	13.067290
20.382687	1203.959679	13.072295
20.275502	1206.179922	13.077299
20.170034	1198.911084	13.082304
20.415187	1193.608337	13.087309
19.858198	1204.792111	13.092314
20.398271	1218.736904	13.097319
20.543270	1230.477315	13.102323
20.221089	1230.579924	13.107328
20.396012	1229.816106	13.112333
20.111806	1234.366470	13.117338
20.236380	1229.483864	13.122343
20.584670	1243.298929	13.127347
20.476504	1243.641557	13.132352
20.564062	1223.407471	13.137357
20.052708	1229.516141	13.142362
20.310233	1222.765324	13.147367
20.305907	1240.040360	13.152371
20.646010	1237.109508	13.157376
20.436597	1222.517468	13.162381
20.066987	1217.759467	13.167386
20.639746	1230.872473	13.172391
20.410884	1219.320519	13.177395
19.978817	1216.295879	13.182400
20.760322	1224.978828	13.187405
20.295447	1225.694068	13.192410
20.036041	1214.771836	13.197415
20.122084	1219.737140	13.202419
20.670586	1238.689776	13.207424
20.468486	1227.593497	13.212429
20.375057	1229.792832	13.217434
20.451684	1211.225657	13.222439
20.308427	1217.805688	13.227443
20.551242	1215.084549	13.232448
20.660455	1216.657420	13.237453
20.624406	1226.739772	13.242458
20.762625	1213.836446	13.247463
20.273833	1224.039845	13.252467
20.865512	1212.652342	13.257472
20.855136	1223.557669	13.262477
20.538515	1215.234356	13.267482
20.511401	1210.656057	13.272487
19.874929	1209.488987	13.277491
20.230655	1210.113264	13.282496
20.569937	1211.949848	13.287501
20.356595	1217.566095	13.292506
20.549504	1220.784504	13.297511
20.285171	1217.487943	13.302515
20.420285	1216.816610	13.307520
20.440094	1210.338270	13.312525
20.026872	1221.846357	13.317530
20.403753	1213.484271	13.322535
20.084253	1220.895847	13.327539
20.213667	1220.211675	13.332544
20.401006	1213.610267	13.337549
20.137454	1229.471958	13.342554
20.206151	1218.915840	13.347559
20.189562	1217.771565	13.352563
20.211055	1215.788250	13.357568
20.518217	1215.357816	13.362573
20.392771	1226.344848	13.367578
20.621776	1222.763960	13.372583
20.594272	1222.942361	13.377587
20.404495	1225.208742	13.382592
21.118241	1220.916312	13.387597
20.416013	1204.371920	13.392602
20.561877	1196.543274	13.397607
20.157374	1184.269875	13.402611
20.239835	1181.528077	13.407616
20.416707	1180.534978	13.412621
20.130892	1186.241009	13.417626
20.268542	1187.814923	13.422631
20.402299	1201.853052	13.427635
20.463693	1196.275492	13.432640
20.600453	1193.591094	13.437645
20.146402	1195.845150	13.442650
20.397425	1191.576803	13.447655
20.259532	1194.676660	13.452659
20.185302	1191.973175	13.457664
20.374864	1200.583129	13.462669
20.643480	1212.905496	13.467674
20.237052	1197.782384	13.472679
20.168631	1192.683799	13.477683
20.218595	1200.098728	13.482688
20.458804	1209.813568	13.487693
20.258090	1228.971627	13.492698
20.680268	1224.215630	13.497703
20.338300	1208.809478	13.502707
20.147552	1194.927955	13.507712
20.327495	1198.410295	13.512717
20.257836	1222.578034	13.517722
20.381654	1216.917526	13.522727
20.870040	1218.040511	13.527731
20.476175	1210.789142	13.532736
20.334428	1199.706614	13.537741
19.975180	1205.677878	13.542746
20.529638	1202.150930	13.547751
20.197896	1191.752307	13.552755
19.847831	1196.784088	13.557760
20.538501	1204.547459	13.562765
20.222987	1221.137270	13.567770
20.737205	1218.037224	13.572775
20.749293	1211.884685	13.577779
20.298729	1207.092803	13.582784
20.394415	1187.516588	13.587789
20.217030	1190.547820	13.592794
20.622657	1188.764701	13.597799
20.325223	1194.616808	13.602803
20.118257	1190.893571	13.607808
20.358846	1190.261787	13.612813
20.227015	1200.833445	13.617818
20.425421	1195.723056	13.622823
20.101381	1189.672369	13.627827
20.228205	1196.756747	13.632832
20.711337	1199.112618	13.637837
20.231777	1200.614725	13.642842
20.137034	1199.358718	13.647847
19.967250	1206.091321	13.652851
20.912342	1220.466809	13.657856
20.758248	1209.350074	13.662861
20.315995	1207.983517	13.667866
20.211634	1203.362017	13.672871
20.186800	1202.537317	13.677875
20.155342	1207.424868	13.682880
20.320198	1204.455779	13.687885
19.904084	1212.658399	13.692890
20.389117	1220.460984	13.697895
20.614560	1232.848006	13.702899
20.229093	1233.376340	13.707904
20.811393	1227.709455	13.712909
20.260774	1220.430879	13.717914
20.384533	1198.843365	13.722919
20.473051	1199.098189	13.727923
20.266484	1198.293597	13.732928
20.095605	1193.549688	13.737933
20.234147	1209.308468	13.742938
20.587025	1225.461573	13.747943
20.699426	1210.192253	13.752947
20.121786	1203.493061	13.757952
20.395350	1202.392196	13.762957
20.359281	1204.015239	13.767962
20.473322	1196.832319	13.772967
20.531534	1201.841074	13.777971
20.255926	1201.853196	13.782976
20.523333	1193.583708	13.787981
20.492716	1202.643129	13.792986
20.795194	1196.656335	13.797991
20.641664	1200.541645	13.802995
20.247736	1201.395511	13.808000
20.696357	1195.817085	13.813005
20.250546	1196.637608	13.818010
20.667999	1193.274287	13.823015
20.865466	1202.880792	13.828019
20.362904	1197.428743	13.833024
20.566737	1199.953688	13.838029
20.349562	1196.160752	13.843034
20.433993	1183.066935	13.848039
20.441047	1168.684937	13.853043
20.138108	1164.618553	13.858048
20.257849	1168.019234	13.863053
20.336158	1198.318330	13.868058
20.289502	1197.562505	13.873063
20.178213	1204.239287	13.878067
20.278254	1203.851866	13.883072
20.326295	1200.245958	13.888077
20.476604	1200.578215	13.893082
20.758846	1196.421357	13.898087
20.194218	1190.507447	13.903091
20.094305	1195.484890	13.908096
20.647984	1198.585384	13.913101
20.660423	1200.069449	13.918106
20.027263	1180.587815	13.923111
20.395506	1183.231411	13.928115
20.335853	1191.276190	13.933120
20.724603	1188.637008	13.938125
20.157853	1180.332523	13.943130
20.413704	1167.789595	13.948135
20.274484	1171.297442	13.953139
20.230699	1176.602363	13.958144
20.518236	1169.067206	13.963149
20.071138	1179.206585	13.968154
20.164673	1185.954031	13.973159
20.702308	1193.822979	13.978163
20.378316	1183.694218	13.983168
20.504821	1174.604549	13.988173
20.005359	1171.184891	13.993178
20.203448	1180.488114	13.998183
20.502261	1191.907253	14.003187
20.396026	1208.383403	14.008192
20.851762	1193.652374	14.013210
20.668160	1186.170625	14.018227
20.722220	1176.303448	14.023245
20.513196	1180.021088	14.028263
20.382093	1180.547544	14.033280
20.664953	1171.816829	14.038298
20.529632	1188.957200	14.043315
20.586256	1186.228759	14.048333
20.285043	1183.604984	14.053351
20.201372	1184.635949	14.058368
20.389327	1186.777525	14.063386
19.991668	1190.492467	14.068403
20.145631	1184.546676	14.073421
20.213160	1198.844957	14.078439
20.421095	1207.939603	14.083456
20.724338	1208.426237	14.088474
21.055888	1222.261125	14.093491
20.549034	1216.640060	14.098509
20.592621	1216.090807	14.103527
20.474904	1220.458605	14.108544
20.621757	1225.445272	14.113562
20.589230	1221.836758	14.118579
20.801164	1210.972722	14.123597
20.804976	1217.008409	14.128615
20.530078	1215.891269	14.133632
21.056196	1210.995926	14.138650
20.079018	1229.092172	14.143667
20.459338	1216.959390	14.148685
20.943702	1217.652785	14.153703
20.554333	1219.348817	14.158720
20.536571	1224.043996	14.163738
20.621391	1231.156838	14.168755
20.829464	1244.036848	14.173773
20.773541	1250.794269	14.178791
20.469276	1258.543570	14.183808
20.965768	1247.892159	14.188826
20.698755	1258.631004	14.193843
20.883067	1254.151372	14.198861
21.141774	1252.301343	14.203879
20.949289	1255.882688	14.208896
21.080633	1253.533978	14.213914
21.021092	1255.868406	14.218931
21.148151	1255.539112	14.223949
20.780518	1256.732559	14.228967
20.870915	1252.359982	14.233984
21.200355	1259.966768	14.239002
21.154936	1264.548581	14.244019
21.094085	1275.575740	14.249037
21.341182	1278.697040	14.254055
21.103250	1295.220025	14.259072
21.581161	1283.805565	14.264090
21.338565	1284.387365	14.269107
21.087393	1270.326414	14.274125
21.408703	1273.635400	14.279143
21.346911	1280.178860	14.284160
21.463309	1278.269756	14.289178
21.210622	1273.371695	14.294195
21.208032	1273.132746	14.299213
21.650259	1283.831900	14.304231
21.184013	1288.734322	14.309248
21.432434	1287.771565	14.314266
21.395297	1293.385523	14.319283
21.832831	1295.219731	14.324301
21.722430	1286.423691	14.329319
21.231052	1276.523582	14.334336
21.546431	1282.428701	14.339354
21.842988	1293.048891	14.344371
21.480273	1286.788857	14.349389
21.650442	1263.320581	14.354407
21.385042	1268.577964	14.359424
21.626146	1284.294723	14.364442
21.764336	1289.947129	14.369459
21.949636	1283.653770	14.374477
21.756984	1273.905217	14.379495
21.223695	1275.423158	14.384512
21.542846	1274.496311	14.389530
21.663598	1289.154480	14.394547
21.761580	1295.976879	14.399565
22.307964	1291.854879	14.404583
22.219486	1300.327900	14.409600
22.130700	1272.681186	14.414618
21.671513	1264.648961	14.419635
21.691734	1260.840432	14.424653
21.770753	1264.761482	14.429671
21.903339	1265.964840	14.434688
21.661223	1262.943089	14.439706
21.454891	1279.195655	14.444723
21.816750	1284.495114	14.449741
22.301944	1282.179044	14.454759
21.997489	1304.433250	14.459776
22.432368	1293.517545	14.464794
22.249896	1292.469598	14.469811
21.944631	1278.085995	14.474829
21.711199	1275.168274	14.479847
21.667460	1292.062326	14.484864
21.759890	1294.195884	14.489882
21.813394	1300.828255	14.494899
21.664447	1302.027915	14.499917
21.875136	1304.235300	14.504935
21.992902	1304.407644	14.509952
21.917443	1294.592918	14.514970
21.815012	1313.023573	14.519987
22.147976	1322.961495	14.525005
22.168411	1319.308441	14.530023
22.288831	1322.649126	14.535040
22.281834	1324.293390	14.540058
22.310967	1327.272527	14.545075
22.341556	1320.376488	14.550093
22.331540	1313.015717	14.555111
22.438910	1316.478334	14.560128
22.409639	1313.686639	14.565146
22.339510	1319.920493	14.570163
22.228836	1318.087329	14.575181
22.632357	1321.294426	14.580199
22.498874	1329.897238	14.585216
22.516482	1311.515754	14.590234
22.690052	1315.326502	14.595251
22.813272	1321.774079	14.600269
22.703543	1311.799848	14.605287
22.563726	1317.696405	14.610304
22.744954	1312.460917	14.615322
22.804895	1310.940264	14.620339
22.846297	1312.104137	14.625357
22.786894	1314.707472	14.630375
22.574687	1315.415965	14.635392
22.436766	1310.292289	14.640410
22.718426	1315.526762	14.645427
22.648667	1321.360123	14.650445
23.045973	1314.014954	14.655463
22.529286	1324.241090	14.660480
22.532855	1320.101119	14.665498
22.701911	1320.048507	14.670515
22.778675	1321.314990	14.675533
22.916726	1316.954305	14.680551
22.648028	1319.857724	14.685568
23.209180	1321.004143	14.690586
22.966128	1313.486065	14.695603
23.379995	1325.144922	14.700621
23.336990	1321.594486	14.705639
23.380938	1314.908383	14.710656
23.179293	1294.020184	14.715674
23.125514	1290.818090	14.720691
23.175855	1289.941663	14.725709
22.689479	1286.515290	14.730727
22.387386	1284.738969	14.735744
22.666711	1306.932458	14.740762
23.179875	1311.129113	14.745779
22.732756	1310.370659	14.750797
23.244578	1314.843161	14.755815
23.105771	1315.375668	14.760832
23.188577	1313.719980	14.765850
22.994098	1321.436313	14.770867
22.893950	1323.305623	14.775885
23.028072	1320.744596	14.780903
22.970538	1324.030352	14.785920
23.084651	1328.939193	14.790938
23.161896	1345.614510	14.795955
23.069361	1363.587973	14.800973
23.571829	1356.353899	14.805991
23.115094	1352.908255	14.811008
23.364050	1355.933574	14.816026
23.330892	1356.475529	14.821043
23.300337	1363.617662	14.826061
23.790111	1362.196944	14.831079
23.417810	1360.230664	14.836096
23.326467	1355.309637	14.841114
23.444480	1356.546213	14.846131
23.135836	1351.753399	14.851149
23.527409	1353.735665	14.856167
23.826144	1355.308612	14.861184
23.480283	1356.737332	14.866202
23.628910	1355.365658	14.871219
23.246107	1358.448505	14.876237
23.891437	1356.192379	14.881255
23.489796	1356.821531	14.886272
23.384727	1359.435460	14.891290
23.717482	1353.718816	14.896307
23.539090	1353.517096	14.901325
23.829987	1358.658259	14.906343
23.953036	1369.520870	14.911360
23.725181	1356.710293	14.916378
23.536414	1364.399287	14.921395
23.719250	1383.888699	14.926413
24.071124	1383.395254	14.931431
24.075716	1389.208017	14.936448
24.001453	1378.219298	14.941466
24.028689	1372.249490	14.946483
23.895578	1368.463287	14.951501
24.284463	1366.373582	14.956519
24.203001	1353.988737	14.961536
24.019542	1350.919112	14.966554
23.999388	1344.058537	14.971571
23.639786	1354.165230	14.976589
24.093813	1358.658680	14.981607
24.194296	1377.671213	14.986624
24.183425	1380.072518	14.991642
24.655110	1375.228194	14.996659
24.386975	1355.545522	15.001677
24.032198	1345.238447	15.006695
24.041399	1348.063117	15.011712
24.136267	1349.380440	15.016730
24.391233	1354.964024	15.021747
24.225931	1359.371125	15.026765
24.403761	1363.600879	15.031783
24.173793	1370.127145	15.036800
24.317420	1377.290212	15.041818
24.177367	1368.525590	15.046835
24.089551	1377.271400	15.051853
24.304334	1370.565038	15.056871
24.343967	1373.772721	15.061888
24.235053	1376.301870	15.066906
24.614648	1368.157274	15.071923
24.634396	1380.084160	15.076941
24.716879	1365.178832	15.081959
24.508414	1366.124109	15.086976
24.729396	1364.884923	15.091994
24.725579	1366.503840	15.097011
24.221530	1381.059754	15.102029
24.508574	1374.946177	15.107047
24.662125	1367.553792	15.112064
24.521485	1375.014440	15.117082
24.872817	1369.114273	15.122099
24.588694	1369.501602	15.127117
24.787684	1381.931272	15.132135
24.680619	1378.302822	15.137152
24.620637	1379.864829	15.142170
24.908093	1378.560696	15.147187
24.405059	1373.525589	15.152205
24.458839	1371.912670	15.157223
24.562087	1381.143882	15.162240
24.602765	1400.980161	15.167258
25.230471	1405.944289	15.172275
24.904447	1415.816108	15.177293
24.802205	1410.152372	15.182311
24.794540	1405.938312	15.187328
24.853910	1416.147242	15.192346
25.199025	1406.085908	15.197363
25.096605	1402.608639	15.202381
24.973736	1404.073546	15.207399
25.277536	1404.207301	15.212416
25.233215	1404.727153	15.217434
25.728715	1402.628613	15.222451
25.192776	1400.792756	15.227469
25.096843	1385.250218	15.232487
25.496584	1396.112262	15.237504
24.951941	1379.186681	15.242522
25.465918	1386.637467	15.247539
25.377280	1393.272988	15.252557
25.344448	1378.781157	15.257575
25.329426	1376.287430	15.262592
24.887323	1385.335351	15.267610
25.059210	1388.505400	15.272627
25.283617	1402.527733	15.277645
25.460402	1394.441914	15.282663
25.636416	1399.827614	15.287680
25.698723	1405.745853	15.292698
25.687252	1399.470436	15.297715
25.622250	1402.566132	15.302733
25.430706	1407.110829	15.307751
25.434603	1406.467578	15.312768
25.376922	1404.702884	15.317786
25.827474	1403.764131	15.322803
25.639969	1411.454507	15.327821
25.329442	1405.354391	15.332839
25.761389	1405.605164	15.337856
25.250184	1406.555102	15.342874
25.447480	1411.168183	15.347891
25.599670	1403.761052	15.352909
25.517852	1403.099817	15.357927
25.734162	1404.945982	15.362944
25.403726	1404.725838	15.367962
25.768825	1394.583912	15.372979
25.780643	1406.704717	15.377997
25.623148	1406.789993	15.383015
25.421888	1416.149821	15.388032
25.789756	1425.936535	15.393050
25.830556	1434.246504	15.398067
25.380128	1422.832831	15.403085
25.996710	1431.554757	15.408103
25.966407	1432.722665	15.413120
26.014162	1427.938412	15.418138
26.027234	1430.649431	15.423155
25.850610	1431.278985	15.428173
26.049011	1428.947495	15.433191
26.665597	1420.889809	15.438208
26.261179	1428.431933	15.443226
25.936166	1426.224442	15.448243
26.329902	1432.608752	15.453261
26.467542	1429.035587	15.458279
26.559355	1431.787441	15.463296
26.392776	1429.659882	15.468314
26.240343	1421.755311	15.473331
26.403046	1436.126477	15.478349
26.292478	1429.175450	15.483367
26.209432	1423.344622	15.488384
25.948156	1430.331837	15.493402
26.184481	1419.428433	15.498419
26.473488	1428.878636	15.503437
26.038398	1424.899684	15.508455
25.999485	1427.289267	15.513472
26.371619	1444.994945	15.518490
26.990745	1448.430089	15.523507
26.354366	1447.629660	15.528525
26.457568	1451.339897	15.533543
26.672328	1461.927766	15.538560
26.901592	1460.605649	15.543578
26.499871	1443.930324	15.548595
26.729055	1458.066466	15.553613
26.574392	1457.055083	15.558631
26.528930	1463.137900	15.563648
26.508769	1460.442657	15.568666
26.955061	1451.585330	15.573683
26.549830	1465.949952	15.578701
26.597573	1461.823238	15.583719
26.642935	1451.397087	15.588736
26.669541	1463.797711	15.593754
26.861317	1458.405232	15.598771
26.498401	1459.462832	15.603789
26.466369	1458.457197	15.608807
26.786639	1464.316660	15.613824
26.686441	1475.206203	15.618842
27.142873	1476.387914	15.623859
27.211792	1481.396295	15.628877
27.219328	1486.903440	15.633895
27.494016	1474.754316	15.638912
27.261273	1462.632355	15.643930
27.377967	1457.565380	15.648947
27.316419	1460.540010	15.653965
27.198696	1449.251575	15.658983
27.405159	1453.240200	15.664000
27.394379	1460.616413	15.669018
27.727905	1452.465103	15.674035
27.058791	1455.405308	15.679053
26.880047	1449.659782	15.684071
27.241348	1453.585242	15.689088
27.415203	1452.977815	15.694106
27.385993	1454.886163	15.699123
27.293318	1446.546488	15.704141
27.502712	1444.976573	15.709159
27.663383	1444.054446	15.714176
26.871006	1447.307545	15.719194
27.253002	1447.836989	15.724211
27.393089	1450.462447	15.729229
27.430652	1458.084726	15.734247
27.519598	1455.276280	15.739264
27.565665	1474.779018	15.744282
27.857008	1481.012777	15.749299
27.801732	1476.241843	15.754317
27.300891	1471.385479	15.759335
27.848802	1465.135791	15.764352
27.872263	1472.875074	15.769370
27.960032	1469.295882	15.774387
27.581191	1459.967758	15.779405
27.424773	1472.479307	15.784423
27.751740	1473.946628	15.789440
27.902557	1490.031867	15.794458
27.961624	1480.410516	15.799475
27.855909	1478.408355	15.804493
27.856674	1482.511792	15.809511
27.890199	1478.678486	15.814528
27.904569	1487.570239	15.819546
27.650529	1485.187955	15.824563
27.945689	1484.201818	15.829581
27.893527	1483.498876	15.834599
27.822886	1475.966515	15.839616
27.880921	1476.536543	15.844634
27.846789	1478.871372	15.849651
27.763461	1489.122928	15.854669
27.942367	1507.386271	15.859687
28.197937	1504.075182	15.864704
28.297295	1510.255246	15.869722
28.102006	1509.126009	15.874739
28.414662	1516.140855	15.879757
28.120605	1514.476132	15.884775
28.286308	1510.244919	15.889792
28.128078	1523.104099	15.894810
28.634780	1514.429312	15.899827
28.448191	1507.467267	15.904845
28.509895	1515.100397	15.909863
28.784630	1513.747248	15.914880
28.573485	1518.107523	15.919898
28.565189	1515.329126	15.924915
28.735621	1515.117207	15.929933
28.331183	1515.332234	15.934951
28.461141	1516.849875	15.939968
28.398061	1515.914528	15.944986
28.772073	1513.527322	15.950003
29.018954	1512.838861	15.955021
28.686035	1519.565536	15.960039
28.742124	1507.426699	15.965056
28.297006	1509.365022	15.970074
28.384256	1514.880559	15.975091
28.905588	1508.325537	15.980109
28.753358	1515.129115	15.985127
28.708437	1511.283264	15.990144
28.904047	1519.256466	15.995162
28.850382	1518.594730	16.000179
28.591018	1514.530501	16.005197
28.608939	1517.084781	16.010215
28.724851	1514.001594	16.015232
28.859506	1517.189864	16.020250
28.678612	1521.090182	16.025267
29.038728	1522.822719	16.030285
29.245470	1537.256513	16.035303
29.257525	1522.974986	16.040320
29.019526	1530.795351	16.045338
29.089815	1537.083964	16.050355
29.210648	1535.972578	16.055373
29.230750	1545.287443	16.060391
28.994517	1539.567491	16.065408
29.080883	1551.375200	16.070426
29.024037	1549.780443	16.075443
29.057280	1544.137921	16.080461
29.034198	1545.867258	16.085479
29.394111	1547.269876	16.090496
29.401009	1550.228851	16.095514
29.096135	1550.090945	16.100531
29.188769	1550.963344	16.105549
28.989734	1550.076505	16.110567
29.466936	1548.715807	16.115584
29.658200	1562.156896	16.120602
29.513643	1574.268812	16.125619
29.726656	1570.575199	16.130637
30.073915	1575.334684	16.135655
30.238054	1558.138153	16.140672
29.861716	1549.483635	16.145690
29.565763	1539.023810	16.150707
29.778226	1530.891248	16.155725
29.883345	1544.960937	16.160743
29.959003	1530.813395	16.165760
29.860097	1535.268222	16.170778
30.061750	1546.230483	16.175795
30.185885	1538.998589	16.180813
30.225019	1532.417954	16.185831
29.979488	1538.068125	16.190848
30.097469	1534.407746	16.195866
29.952806	1547.637887	16.200883
29.721444	1529.743369	16.205901
29.400403	1544.834652	16.210919
29.731053	1535.934500	16.215936
29.648997	1538.824463	16.220954
29.490564	1549.912646	16.225971
29.857984	1557.996189	16.230989
29.669203	1572.885274	16.236007
29.884985	1569.149844	16.241024
30.053746	1573.549733	16.246042
30.000859	1572.027532	16.251059
30.235157	1572.830757	16.256077
30.031848	1580.654254	16.261095
30.370435	1571.872419	16.266112
30.493412	1581.093674	16.271130
29.910189	1590.324587	16.276147
30.094831	1572.577615	16.281165
30.247202	1583.916108	16.286183
30.234741	1587.926949	16.291200
30.827780	1594.640973	16.296218
30.410275	1601.706237	16.301235
30.493444	1597.427728	16.306253
30.292823	1611.722752	16.311271
30.256865	1602.124706	16.316288
30.633443	1601.129327	16.321306
30.465132	1603.375751	16.326323
30.636357	1602.125391	16.331341
30.377558	1605.668574	16.336359
30.510666	1603.055307	16.341376
30.474630	1600.766350	16.346394
30.505380	1600.657916	16.351411
30.784121	1605.703203	16.356429
30.792163	1615.717104	16.361447
30.957639	1624.295200	16.366464
31.040443	1629.997388	16.371482
30.795132	1624.128157	16.376499
30.985530	1624.344357	16.381517
30.897583	1632.326074	16.386535
31.080299	1631.398975	16.391552
31.058883	1633.481225	16.396570
30.970793	1637.045544	16.401587
31.505366	1630.572463	16.406605
31.687080	1631.804833	16.411623
31.670842	1609.583490	16.416640
31.561001	1608.076562	16.421658
31.015999	1601.411780	16.426675
31.025044	1599.999443	16.431693
30.914101	1604.957196	16.436711
30.973774	1599.531013	16.441728
31.118817	1599.126180	16.446746
31.133592	1622.903049	16.451763
31.590666	1626.006924	16.456781
31.590902	1640.658524	16.461799
31.273476	1637.964213	16.466816
31.378266	1632.882291	16.471834
31.422478	1638.580862	16.476851
31.262721	1635.854399	16.481869
31.580170	1643.444924	16.486887
31.553435	1634.892245	16.491904
31.650254	1628.786379	16.496922
31.272318	1639.484653	16.501939
31.289608	1635.165848	16.506957
31.444783	1644.335551	16.511975
31.538435	1632.323657	16.516992
31.805629	1632.338086	16.522010
31.464569	1640.686863	16.527027
31.617730	1636.132140	16.532045
31.508620	1649.335796	16.537063
31.659664	1659.171646	16.542080
31.871444	1664.858032	16.547098
32.009793	1672.519441	16.552115
32.201053	1661.526734	16.557133
32.063877	1672.836974	16.562151
31.916590	1667.192680	16.567168
32.340621	1663.485703	16.572186
32.152552	1667.065990	16.577203
32.158130	1659.563390	16.582221
32.374540	1665.745497	16.587239
32.512733	1654.471309	16.592256
31.944220	1647.954648	16.597274
31.896324	1643.982095	16.602291
32.176658	1650.930095	16.607309
32.169871	1659.605863	16.612327
32.428415	1669.692610	16.617344
32.383654	1672.474223	16.622362
32.008948	1673.962253	16.627379
32.036115	1663.625704	16.632397
32.319698	1669.167876	16.637415
32.062322	1664.799689	16.642432
32.244079	1663.890865	16.647450
31.767149	1665.284598	16.652467
32.230144	1680.190001	16.657485
32.353741	1692.149718	16.662503
32.294237	1691.544888	16.667520
32.947478	1698.764050	16.672538
32.541693	1695.734050	16.677555
32.494593	1692.951644	16.682573
32.831168	1689.623083	16.687591
32.819407	1691.454051	16.692608
32.896967	1690.244944	16.697626
33.002932	1689.134915	16.702643
33.121747	1686.452424	16.707661
33.106256	1690.099988	16.712679
32.748997	1686.561219	16.717696
32.811046	1686.165495	16.722714
32.428725	1700.628383	16.727731
32.937345	1685.232316	16.732749
32.909245	1691.848527	16.737767
33.079544	1686.891591	16.742784
33.150767	1689.531653	16.747802
32.578625	1698.095692	16.752819
33.127877	1690.160451	16.757837
33.699912	1700.433259	16.762855
33.466424	1695.338443	16.767872
33.499282	1689.002547	16.772890
33.307372	1690.732103	16.777907
33.382575	1694.052271	16.782925
33.353320	1691.393197	16.787943
32.952969	1698.182697	16.792960
33.356103	1697.222528	16.797978
32.972517	1695.226245	16.802995
32.979454	1698.285252	16.808013
33.295276	1721.448777	16.813031
33.063174	1724.479474	16.818048
33.793976	1725.550771	16.823066
33.178888	1730.797388	16.828083
33.419799	1718.074272	16.833101
33.054970	1724.245415	16.838119
32.933037	1724.122996	16.843136
33.338234	1731.701275	16.848154
33.562836	1747.202013	16.853171
34.174303	1748.221322	16.858189
33.710762	1753.925880	16.863207
33.788350	1760.502736	16.868224
34.072522	1741.829738	16.873242
34.198084	1754.008877	16.878259
33.920077	1751.178245	16.883277
34.263377	1754.120529	16.888295
34.289051	1743.171118	16.893312
34.300564	1723.319942	16.898330
34.051860	1734.088259	16.903347
34.138391	1718.168395	16.908365
34.221931	1720.839819	16.913383
34.287515	1725.473609	16.918400
34.448369	1719.011019	16.923418
34.107036	1712.428998	16.928435
34.371188	1708.590349	16.933453
34.200031	1726.647796	16.938471
34.570044	1723.948610	16.943488
34.447895	1712.647355	16.948506
33.850698	1720.023042	16.953523
33.966234	1711.442778	16.958541
34.151464	1719.015847	16.963559
34.450329	1740.074186	16.968576
34.468180	1743.534134	16.973594
34.356738	1754.676223	16.978611
34.418423	1751.317607	16.983629
34.402656	1749.472056	16.988647
34.249444	1756.797230	16.993664
34.586130	1746.433544	16.998682
34.316536	1746.033257	17.003699
34.737613	1750.326148	17.008717
34.694179	1741.988897	17.013735
34.652964	1755.373545	17.018752
34.740721	1750.059438	17.023770
34.619336	1744.790641	17.028787
34.764106	1753.431814	17.033805
34.961279	1761.444247	17.038823
34.809607	1768.352182	17.043840
34.880596	1767.194202	17.048858
35.000298	1777.707629	17.053875
34.874062	1780.747748	17.058893
34.989047	1777.957617	17.063911
34.746368	1778.956427	17.068928
35.178108	1769.650182	17.073946
35.016558	1778.902224	17.078963
35.165881	1770.899277	17.083981
35.267821	1776.689981	17.088999
35.080411	1778.948760	17.094016
35.167612	1773.838308	17.099034
35.304991	1785.050762	17.104051
35.432073	1781.188348	17.109069
35.489693	1770.566158	17.114087
35.657907	1776.282499	17.119104
35.533781	1772.929355	17.124122
35.466304	1770.822557	17.129139
35.714492	1770.883558	17.134157
35.686525	1762.757844	17.139175
35.800544	1765.426413	17.144192
35.351126	1768.420354	17.149210
35.893434	1781.564407	17.154227
35.647878	1774.778121	17.159245
35.879291	1764.466729	17.164263
35.591157	1778.093362	17.169280
35.453554	1778.223660	17.174298
35.679117	1773.100510	17.179315
35.677939	1774.554036	17.184333
35.863424	1774.713201	17.189351
35.418062	1776.194848	17.194368
35.818812	1779.973453	17.199386
36.219381	1793.455242	17.204403
36.189600	1780.728086	17.209421
36.401723	1773.282550	17.214439
35.923577	1772.186828	17.219456
36.009883	1775.302329	17.224474
36.131461	1778.181834	17.229491
36.036422	1770.382221	17.234509
36.169082	1783.792206	17.239527
36.137996	1806.275482	17.244544
36.433476	1798.595536	17.249562
36.269098	1808.296561	17.254579
36.162110	1805.019616	17.259597
36.523102	1802.731856	17.264615
36.207975	1808.044012	17.269632
36.578984	1801.285482	17.274650
36.673598	1797.885772	17.279667
36.332802	1808.696312	17.284685
36.695945	1800.595263	17.289703
36.537401	1805.450204	17.294720
36.544829	1805.369392	17.299738
36.728556	1799.086334	17.304755
36.591770	1799.734666	17.309773
36.925281	1797.704799	17.314791
36.658285	1795.440057	17.319808
36.572089	1799.645506	17.324826
36.612004	1802.908747	17.329843
36.234526	1806.025811	17.334861
36.548792	1790.493258	17.339879
36.671347	1805.633945	17.344896
37.180971	1809.988058	17.349914
36.988910	1802.193645	17.354931
37.273425	1809.530811	17.359949
37.292924	1792.598616	17.364967
37.036148	1800.731427	17.369984
36.975112	1795.096317	17.375002
37.202086	1790.554881	17.380019
36.850523	1798.663779	17.385037
37.281591	1807.641376	17.390055
36.826507	1822.408619	17.395072
37.210859	1830.426796	17.400090
37.491256	1824.991040	17.405107
37.260739	1817.941887	17.410125
37.370161	1822.944614	17.415143
37.388455	1831.005472	17.420160
37.430452	1823.604830	17.425178
37.353160	1816.876300	17.430195
37.045251	1824.670603	17.435213
37.689110	1816.575360	17.440231
37.402904	1824.559273	17.445248
37.663897	1825.675298	17.450266
37.863850	1818.455869	17.455283
37.609506	1823.542229	17.460301
37.482509	1816.227659	17.465319
37.345462	1826.538652	17.470336
37.156934	1837.037635	17.475354
37.323395	1855.478343	17.480371
37.437618	1860.396390	17.485389
37.934516	1857.191113	17.490407
37.879451	1858.487330	17.495424
38.060110	1864.044463	17.500442
37.855922	1862.159543	17.505459
37.795012	1863.523306	17.510477
38.148220	1868.401561	17.515495
37.915709	1877.795373	17.520512
38.067388	1884.600554	17.525530
38.444472	1880.307406	17.530547
38.259704	1892.617824	17.535565
38.381849	1887.451731	17.540583
37.960033	1884.562649	17.545600
38.137078	1882.014254	17.550618
38.559681	1877.298682	17.555635
38.331738	1889.996077	17.560653
38.527314	1876.628553	17.565671
38.493877	1879.984712	17.570688
38.772730	1879.288392	17.575706
38.844107	1878.662689	17.580723
38.634236	1877.398899	17.585741
39.135860	1872.311467	17.590759
39.036790	1875.887960	17.595776
38.588080	1868.688376	17.600794
38.910293	1863.171806	17.605811
38.664023	1876.633059	17.610829
38.913070	1861.978263	17.615847
38.640493	1867.525695	17.620864
38.924799	1863.520146	17.625882
38.807103	1870.073832	17.630899
38.864782	1868.951989	17.635917
39.082896	1871.926391	17.640935
38.902039	1873.515865	17.645952
38.703104	1868.305604	17.650970
38.792366	1871.897450	17.655987
38.539649	1879.949281	17.661005
38.745034	1874.727576	17.666023
38.950370	1890.030946	17.671040
39.334884	1897.332108	17.676058
39.155483	1892.562642	17.681075
38.892628	1905.747199	17.686093
39.148613	1900.713293	17.691111
39.302528	1914.039026	17.696128
39.143348	1908.030494	17.701146
39.099003	1903.307956	17.706163
39.141431	1898.770174	17.711181
39.038920	1897.975439	17.716199
39.015101	1915.678665	17.721216
39.244184	1921.207828	17.726234
39.818856	1920.008366	17.731251
40.088504	1920.158614	17.736269
40.005806	1930.087080	17.741287
39.723886	1932.371142	17.746304
39.501174	1925.635210	17.751322
40.394933	1924.628708	17.756339
40.021334	1922.815746	17.761357
40.296637	1925.742947	17.766375
40.405660	1921.606786	17.771392
40.080910	1908.573361	17.776410
40.275070	1902.625919	17.781427
40.265703	1895.716002	17.786445
40.209162	1892.376445	17.791463
40.124040	1901.023647	17.796480
40.002126	1899.586880	17.801498
40.310695	1894.293534	17.806515
40.602258	1901.506290	17.811533
40.254344	1888.257534	17.816551
40.603343	1900.640636	17.821568
40.299521	1894.565165	17.826586
40.437895	1894.050824	17.831603
40.295312	1899.801992	17.836621
40.079378	1896.696876	17.841639
40.314663	1906.891715	17.846656
39.992703	1927.500379	17.851674
40.471271	1917.407569	17.856691
40.059401	1926.603786	17.861709
39.830178	1916.152347	17.866727
40.139418	1937.802952	17.871744
40.631185	1957.884686	17.876762
41.074556	1953.668354	17.881779
40.682328	1967.615400	17.886797
40.576948	1959.979298	17.891815
40.513601	1960.560312	17.896832
40.571786	1962.666758	17.901850
40.933267	1960.292661	17.906867
40.594446	1970.654487	17.911885
40.822238	1959.928179	17.916903
40.982028	1966.910376	17.921920
40.837834	1985.010353	17.926938
41.237406	1988.515947	17.931955
41.107360	1993.327471	17.936973
41.616830	1993.779562	17.941991
41.486655	1985.684644	17.947008
41.475872	1992.424014	17.952026
41.826040	1977.954556	17.957043
41.391674	1968.503345	17.962061
41.560395	1959.557480	17.967079
41.554370	1961.166206	17.972096
41.210447	1954.490813	17.977114
41.347518	1954.034182	17.982131
41.663611	1968.344101	17.987149
41.810511	1977.281923	17.992167
41.623139	1978.993013	17.997184
41.692686	1984.816123	18.002202
41.976956	1978.157834	18.007219
41.909132	1975.453349	18.012237
41.878191	1968.796738	18.017255
41.917529	1963.188852	18.022272
41.821982	1967.977129	18.027290
42.009343	1975.690527	18.032307
41.841854	1987.859456	18.037325
41.839737	1985.943812	18.042343
41.831176	1988.358202	18.047360
41.825666	1995.737701	18.052378
41.945520	1989.252891	18.057395
41.700675	1983.610640	18.062413
41.707981	1982.277711	18.067431
41.529996	1996.129774	18.072448
41.742006	2006.920088	18.077466
41.995483	2014.161477	18.082483
42.313178	2020.292496	18.087501
42.564232	2025.614752	18.092519
42.637585	2012.250743	18.097536
42.489166	2020.930520	18.102554
42.566082	2011.595587	18.107571
42.546364	2013.178315	18.112589
42.523368	2017.331642	18.117607
42.654128	2014.615940	18.122624
42.662063	2007.695920	18.127642
42.827994	2006.335004	18.132659
42.670173	2016.158672	18.137677
42.702956	2014.411868	18.142695
42.791588	2008.735663	18.147712
42.869761	2013.315010	18.152730
42.989577	2020.310778	18.157747
43.101645	2018.113312	18.162765
43.008650	2018.713981	18.167783
42.893201	2017.863576	18.172800
43.101725	2031.701772	18.177818
43.154622	2027.121994	18.182835
43.076382	2033.807978	18.187853
43.166742	2040.534359	18.192871
43.266493	2036.546628	18.197888
43.288010	2045.000011	18.202906
43.398602	2042.961478	18.207923
43.136537	2042.316550	18.212941
43.351567	2050.611937	18.217959
43.360657	2032.994164	18.222976
43.256287	2055.942788	18.227994
43.471727	2033.097182	18.233011
43.263451	2042.670427	18.238029
43.621664	2045.255831	18.243047
43.522145	2037.366289	18.248064
43.183354	2045.438868	18.253082
43.425645	2043.746309	18.258099
43.204036	2061.696239	18.263117
43.529698	2071.578011	18.268135
43.770364	2078.900378	18.273152
43.847577	2082.058844	18.278170
44.026358	2067.143032	18.283187
43.769939	2079.832862	18.288205
43.832344	2073.311011	18.293223
44.003784	2073.512356	18.298240
44.057952	2074.357912	18.303258
44.124671	2070.407337	18.308275
44.050042	2067.626040	18.313293
43.965010	2087.958038	18.318311
44.160919	2093.589421	18.323328
44.026388	2103.595003	18.328346
44.383651	2096.117341	18.333363
44.331457	2092.420253	18.338381
44.191683	2095.669870	18.343399
44.532028	2092.415788	18.348416
44.301087	2093.824473	18.353434
44.613937	2096.597217	18.358451
44.775469	2095.194129	18.363469
44.521123	2101.226380	18.368487
44.923245	2092.574328	18.373504
44.266500	2103.833390	18.378522
44.711172	2088.712105	18.383539
44.841029	2101.107738	18.388557
44.602542	2101.326604	18.393575
44.997679	2105.813046	18.398592
45.081372	2121.204043	18.403610
44.997316	2119.444184	18.408627
44.945185	2130.991784	18.413645
45.030096	2131.433983	18.418663
45.297896	2124.650879	18.423680
45.283434	2130.255736	18.428698
45.176968	2128.255589	18.433715
45.371031	2125.021068	18.438733
45.139404	2128.266752	18.443751
45.314825	2121.797955	18.448768
45.473502	2125.520892	18.453786
45.531028	2120.160655	18.458803
45.575294	2111.402995	18.463821
45.744949	2125.497186	18.468839
45.720798	2104.235297	18.473856
45.575890	2114.623034	18.478874
45.813357	2104.746271	18.483891
45.703090	2088.530986	18.488909
45.272079	2096.352042	18.493927
45.666308	2109.887169	18.498944
45.420128	2118.084871	18.503962
45.603149	2121.514615	18.508979
45.988561	2127.317880	18.513997
45.806416	2122.059373	18.519015
46.276204	2116.507176	18.524032
45.736345	2129.139327	18.529050
45.563647	2120.753556	18.534067
45.748299	2121.232992	18.539085
45.717789	2130.219826	18.544103
46.003023	2136.970324	18.549120
45.977191	2151.810757	18.554138
46.314559	2145.563827	18.559155
46.470849	2151.306369	18.564173
46.572953	2152.545737	18.569191
46.711296	2146.812527	18.574208
46.522697	2152.451187	18.579226
46.306158	2144.658043	18.584243
46.739514	2151.643820	18.589261
46.564770	2151.628891	18.594279
46.656730	2142.670883	18.599296
46.567850	2148.219992	18.604314
46.419725	2138.393569	18.609331
46.475106	2153.220866	18.614349
46.502175	2152.942169	18.619367
46.599744	2148.428723	18.624384
46.470860	2160.261197	18.629402
46.644688	2162.282086	18.634419
47.159092	2176.056546	18.639437
46.733344	2189.158229	18.644455
47.144120	2189.132687	18.649472
47.165158	2185.049738	18.654490
47.045122	2179.481306	18.659507
47.430097	2176.684190	18.664525
47.060554	2176.371115	18.669543
47.260520	2175.061051	18.674560
47.541729	2178.966172	18.679578
47.202742	2175.018979	18.684595
47.310854	2172.587489	18.689613
47.202060	2177.469847	18.694631
47.355421	2171.672626	18.699648
47.485094	2171.566915	18.704666
47.519932	2171.023067	18.709683
47.494712	2168.957796	18.714701
47.397144	2194.220755	18.719719
47.754586	2196.550375	18.724736
47.766433	2201.918429	18.729754
47.840948	2203.735058	18.734771
47.871940	2201.667232	18.739789
47.840271	2208.094874	18.744807
47.803772	2201.707268	18.749824
47.860420	2212.698402	18.754842
47.865081	2202.910320	18.759859
47.803740	2199.647909	18.764877
47.756222	2208.997600	18.769895
48.201738	2204.435508	18.774912
48.121103	2207.076493	18.779930
48.348273	2199.544305	18.784947
48.272932	2203.112079	18.789965
47.910837	2213.722974	18.794983
48.431478	2219.171542	18.800000
48.411511	2234.393781	18.805018
48.734650	2229.739261	18.810035
48.460517	2225.476165	18.815053
48.455139	2235.691218	18.820071
48.701830	2230.220546	18.825088
48.277225	2230.559526	18.830106
48.677685	2234.025255	18.835123
48.636467	2229.034719	18.840141
48.733560	2229.718964	18.845159
48.560473	2223.835154	18.850176
48.710824	2241.456121	18.855194
48.848713	2238.971478	18.860211
48.978590	2243.512889	18.865229
48.986441	2255.095185	18.870247
49.393955	2268.807727	18.875264
49.270733	2263.750913	18.880282
49.218444	2264.988411	18.885299
49.306303	2258.730663	18.890317
49.025107	2258.776512	18.895335
49.181637	2267.354920	18.900352
49.329138	2262.290279	18.905370
49.370416	2265.891624	18.910387
49.769335	2265.783851	18.915405
49.420941	2261.381486	18.920423
49.471592	2259.729244	18.925440
49.536412	2264.091235	18.930458
49.124643	2267.509587	18.935475
49.622174	2255.248415	18.940493
49.477482	2265.942561	18.945511
49.503512	2272.832063	18.950528
49.978899	2288.851450	18.955546
50.426041	2294.298471	18.960563
50.054630	2282.583959	18.965581
50.031221	2280.970400	18.970599
50.263029	2289.583953	18.975616
50.106939	2270.887370	18.980634
49.821980	2261.612757	18.985651
50.375651	2273.271589	18.990669
50.055916	2285.846437	18.995687
49.992122	2289.973754	19.000704
49.996562	2295.859726	19.005722
50.195412	2290.493314	19.010739
50.246521	2279.838032	19.015757
50.043642	2293.204786	19.020775
49.994667	2288.782578	19.025792
50.492462	2291.306292	19.030810
50.486758	2307.288479	19.035827
50.566777	2306.518735	19.040845
50.697585	2319.238445	19.045863
50.710971	2317.802067	19.050880
50.695273	2319.685365	19.055898
50.362263	2323.609204	19.060915
50.931630	2306.535714	19.065933
50.660206	2310.945919	19.070951
50.773437	2315.783164	19.075968
50.980001	2315.987154	19.080986
50.816060	2316.855550	19.086003
51.063457	2311.598147	19.091021
51.144801	2330.393432	19.096039
51.391570	2330.244018	19.101056
51.423612	2340.648030	19.106074
51.593911	2340.033700	19.111091
51.392943	2339.637378	19.116109
51.437336	2334.043850	19.121127
51.733996	2341.873751	19.126144
51.719067	2336.359694	19.131162
51.396134	2317.503443	19.136179
51.702015	2327.339155	19.141197
51.526579	2336.995150	19.146215
51.739179	2340.359232	19.151232
51.585976	2339.497957	19.156250
51.255223	2343.675785	19.161267
51.589952	2333.932620	19.166285
51.590622	2346.328940	19.171303
51.590413	2345.196513	19.176320
52.113004	2347.389162	19.181338
51.647085	2360.457711	19.186355
52.150678	2366.188038	19.191373
52.248272	2364.997890	19.196391
52.294261	2368.811083	19.201408
52.418438	2375.601112	19.206426
52.269178	2368.284588	19.211443
52.282504	2363.902866	19.216461
52.088087	2362.528101	19.221479
52.474637	2362.635081	19.226496
52.630911	2359.463693	19.231514
52.341686	2364.633777	19.236531
52.588008	2362.606977	19.241549
52.234248	2364.889241	19.246567
52.475798	2374.724987	19.251584
52.447688	2388.223300	19.256602
52.406217	2399.755094	19.261619
53.149815	2400.899460	19.266637
53.017925	2400.341663	19.271655
52.864677	2396.511411	19.276672
53.108090	2399.372505	19.281690
53.067590	2394.410145	19.286707
53.367332	2389.425677	19.291725
53.388822	2391.369548	19.296743
53.626552	2395.652317	19.301760
53.558487	2386.434158	19.306778
53.522890	2393.699692	19.311795
53.777423	2378.914320	19.316813
53.575555	2355.429445	19.321831
53.445713	2352.248049	19.326848
53.330190	2346.704772	19.331866
53.257636	2356.273837	19.336883
53.569604	2374.790227	19.341901
53.641120	2382.113780	19.346919
53.805994	2383.010856	19.351936
53.558959	2388.651744	19.356954
53.585384	2395.582183	19.361971
53.554244	2386.346668	19.366989
53.649204	2383.714219	19.372007
53.530804	2387.484725	19.377024
53.611161	2389.241309	19.382042
53.692784	2405.859909	19.387059
54.078391	2402.766535	19.392077
53.877797	2411.066827	19.397095
54.059759	2416.594008	19.402112
54.041990	2407.872020	19.407130
54.162544	2419.035050	19.412147
54.400698	2409.093401	19.417165
54.276812	2417.021432	19.422183
54.621454	2430.617316	19.427200
54.745954	2436.919835	19.432218
54.774757	2441.366805	19.437235
55.030868	2420.358059	19.442253
54.807436	2417.079293	19.447271
54.829335	2402.903955	19.452288
54.982811	2399.979535	19.457306
54.814124	2405.796003	19.462323
54.676580	2397.823808	19.467341
54.808305	2419.385023	19.472359
54.800446	2426.808835	19.477376
55.078557	2418.966972	19.482394
55.272541	2430.889987	19.487411
55.176629	2430.787513	19.492429
55.216282	2433.496116	19.497447
55.030380	2438.869018	19.502464
55.070032	2433.909441	19.507482
54.922775	2431.224796	19.512499
55.103860	2430.731468	19.517517
55.374551	2440.045639	19.522535
55.477333	2460.080127	19.527552
55.598675	2459.184374	19.532570
55.556013	2463.250624	19.537587
55.733456	2471.633402	19.542605
55.556609	2467.919795	19.547623
55.825816	2465.900871	19.552640
55.848502	2461.240306	19.557658
55.725020	2464.878609	19.562675
56.095298	2460.568753	19.567693
55.974992	2466.266693	19.572711
56.006680	2466.181718	19.577728
55.850615	2466.614841	19.582746
55.758341	2467.870235	19.587763
55.873643	2458.229193	19.592781
55.741363	2480.630376	19.597799
55.871581	2493.931527	19.602816
55.898887	2492.336815	19.607834
55.936336	2507.173822	19.612851
56.156168	2509.177418	19.617869
56.886375	2510.662728	19.622887
56.874875	2522.483225	19.627904
57.040040	2521.986323	19.632922
56.849548	2509.701947	19.637939
56.757644	2496.813179	19.642957
57.215386	2496.932368	19.647975
56.921549	2485.910032	19.652992
57.054168	2478.315169	19.658010
56.999294	2489.219301	19.663027
57.043158	2484.908701	19.668045
57.030112	2487.566496	19.673063
57.051602	2501.816372	19.678080
57.670169	2503.713015	19.683098
57.243015	2507.241160	19.688115
57.376332	2496.192833	19.693133
57.481510	2497.737265	19.698151
56.916803	2506.099247	19.703168
57.594569	2510.342042	19.708186
57.383418	2520.889461	19.713203
57.368014	2518.171169	19.718221
57.651500	2506.826964	19.723239
57.985382	2508.132940	19.728256
57.896619	2504.706635	19.733274
57.771763	2507.067803	19.738291
57.604767	2506.003336	19.743309
57.686471	2503.644839	19.748327
58.138860	2506.925319	19.753344
58.396936	2497.009339	19.758362
58.192431	2500.361490	19.763379
58.089080	2503.856956	19.768397
58.036806	2501.073324	19.773415
57.951387	2499.291604	19.778432
58.294818	2505.945657	19.783450
58.334545	2515.254583	19.788467
58.503126	2524.763508	19.793485
58.540661	2534.998175	19.798503
58.472693	2545.605328	19.803520
58.708329	2533.095879	19.808538
58.391306	2538.822848	19.813555
58.764140	2532.407453	19.818573
58.705286	2536.077218	19.823591
58.315088	2537.938909	19.828608
58.524549	2530.093011	19.833626
58.854008	2529.793175	19.838643
58.931770	2528.136257	19.843661
58.886706	2531.526444	19.848679
58.479511	2536.288390	19.853696
59.040775	2544.157293	19.858714
59.235947	2556.363712	19.863731
59.253614	2563.783213	19.868749
59.305748	2562.763076	19.873767
59.063517	2561.112977	19.878784
59.223871	2566.788823	19.883802
59.203422	2571.714433	19.888819
59.320633	2564.937270	19.893837
59.565978	2569.999231	19.898855
59.427211	2571.064145	19.903872
59.988428	2577.090236	19.908890
59.333171	2586.007248	19.913907
59.757659	2591.459833	19.918925
60.020466	2583.967817	19.923943
59.997290	2587.751182	19.928960
60.026104	2589.465436	19.933978
60.020186	2595.545455	19.938995
60.020786	2596.862902	19.944013
60.077950	2592.857920	19.949031
59.800385	2594.883803	19.954048
60.335875	2593.072008	19.959066
60.116617	2592.886726	19.964083
60.039270	2592.775555	19.969101
60.327088	2600.761460	19.974119
60.378456	2610.010956	19.979136
60.448085	2612.048193	19.984154
60.518501	2612.252692	19.989171
60.519274	2615.865788	19.994189
60.930174	2620.336289	19.999207
60.953040	2617.481475	20.004224
61.036857	2610.645440	20.009242
61.240548	2620.494920	20.014259
60.949705	2610.517048	20.019277
61.092511	2617.216571	20.024295
61.004389	2612.815947	20.029312
60.992975	2603.731280	20.034330
60.782213	2610.328399	20.039347
60.897712	2616.373434	20.044365
61.001692	2626.448711	20.049383
61.096913	2643.722040	20.054400
60.989085	2648.724871	20.059418
61.151964	2650.897334	20.064435
61.091333	2649.747680	20.069453
61.501463	2658.104052	20.074471
61.260467	2679.027828	20.079488
61.355371	2682.400350	20.084506
61.756756	2682.594571	20.089523
61.767072	2683.093678	20.094541
61.828716	2675.975538	20.099559
61.320687	2683.134769	20.104576
61.911305	2686.491606	20.109594
62.322557	2703.218603	20.114611
62.246578	2704.708273	20.119629
62.569111	2706.605294	20.124647
62.286319	2689.058486	20.129664
62.329764	2677.875807	20.134682
62.363411	2679.139555	20.139699
62.349133	2694.849542	20.144717
62.592560	2691.318990	20.149735
62.477299	2709.179758	20.154752
62.674426	2713.317580	20.159770
62.809454	2712.147764	20.164787
62.651050	2708.124583	20.169805
63.162796	2707.943913	20.174823
62.889334	2707.741145	20.179840
62.767667	2696.636377	20.184858
63.208390	2701.953123	20.189875
62.854886	2711.164201	20.194893
63.014481	2695.784463	20.199911
63.178645	2707.678149	20.204928
63.138951	2704.848221	20.209946
63.595067	2693.075000	20.214963
62.910364	2701.203281	20.219981
62.985897	2696.853328	20.224999
63.328934	2705.876465	20.230016
63.300701	2711.249990	20.235034
63.218022	2719.215210	20.240051
63.325678	2727.398241	20.245069
63.253060	2716.603217	20.250087
62.912042	2725.594012	20.255104
63.606048	2742.500961	20.260122
63.556301	2749.309159	20.265139
63.315585	2754.943580	20.270157
63.707305	2754.926034	20.275175
63.451231	2770.086104	20.280192
63.759668	2774.965629	20.285210
64.220419	2773.910073	20.290227
64.182770	2772.296543	20.295245
64.647926	2765.528156	20.300263
64.654294	2779.041370	20.305280
64.621170	2768.812085	20.310298
64.818399	2768.643599	20.315315
65.135642	2770.731334	20.320333
65.138660	2773.180874	20.325351
65.025013	2774.050908	20.330368
65.020394	2774.487213	20.335386
64.898896	2760.887421	20.340403
64.865835	2764.145655	20.345421
65.145615	2751.723758	20.350439
65.180964	2768.308149	20.355456
65.082903	2765.380323	20.360474
65.289633	2756.091208	20.365491
65.046467	2772.144507	20.370509
65.455790	2762.720635	20.375527
65.223319	2764.167836	20.380544
65.267429	2760.606863	20.385562
65.186167	2758.752734	20.390579
65.323216	2773.381542	20.395597
65.818379	2763.660222	20.400615
65.567247	2760.620821	20.405632
65.611251	2760.257304	20.410650
65.727935	2756.361782	20.415667
65.218385	2763.410265	20.420685
65.544668	2778.648485	20.425703
65.483517	2788.511976	20.430720
65.196559	2787.019943	20.435738
65.990981	2787.630334	20.440755
65.679462	2803.693809	20.445773
65.951523	2812.556703	20.450791
66.078021	2820.800343	20.455808
65.886990	2816.028256	20.460826
66.485342	2812.485653	20.465843
66.473055	2821.824155	20.470861
66.875790	2823.506616	20.475879
66.381462	2820.749888	20.480896
66.805752	2819.816351	20.485914
66.411517	2817.539407	20.490931
66.489960	2821.566085	20.495949
66.740132	2829.717646	20.500967
66.856466	2845.531399	20.505984
66.918776	2846.515391	20.511002
67.266460	2842.917315	20.516019
66.927855	2850.157830	20.521037
67.068334	2846.807129	20.526055
67.041231	2850.306137	20.531072
67.214480	2850.519786	20.536090
67.471059	2843.051554	20.541107
66.929470	2843.983149	20.546125
67.198528	2847.970065	20.551143
67.563073	2866.607968	20.556160
67.279474	2879.677188	20.561178
67.616769	2869.768656	20.566195
67.569355	2873.199485	20.571213
67.472400	2869.553202	20.576231
67.931786	2871.700061	20.581248
67.722022	2879.647773	20.586266
67.739412	2887.966071	20.591283
67.948872	2906.826712	20.596301
68.300653	2898.942054	20.601319
68.696992	2902.651995	20.606336
68.793281	2906.329899	20.611354
68.955961	2900.985232	20.616371
68.592042	2887.126048	20.621389
68.400011	2868.523120	20.626407
68.383122	2869.012722	20.631424
68.146255	2868.324058	20.636442
68.509243	2886.927600	20.641459
68.365397	2909.261284	20.646477
68.423651	2897.056028	20.651495
68.898568	2900.285477	20.656512
68.824713	2916.610741	20.661530
68.820403	2898.520581	20.666547
68.776343	2905.658643	20.671565
69.236222	2930.078248	20.676583
69.161913	2927.434565	20.681600
69.152013	2935.871762	20.686618
69.521127	2932.252666	20.691635
69.232514	2938.371047	20.696653
69.593794	2929.042732	20.701671
69.992292	2927.727709	20.706688
69.819264	2927.154107	20.711706
70.070234	2927.551320	20.716723
69.716452	2926.615717	20.721741
69.896889	2924.411917	20.726759
69.758604	2924.574234	20.731776
69.557329	2917.898777	20.736794
69.966209	2912.518196	20.741811
69.797955	2923.889400	20.746829
70.083775	2923.581290	20.751847
69.963366	2929.579473	20.756864
69.828487	2941.041048	20.761882
69.760676	2941.657516	20.766899
69.408825	2955.055096	20.771917
69.816589	2965.430546	20.776935
69.851353	2967.242265	20.781952
70.194070	2988.597977	20.786970
70.656889	2981.240806	20.791987
70.214001	2991.139157	20.797005
70.552385	2992.214436	20.802023
70.916066	3006.579365	20.807040
71.028596	3018.732583	20.812058
71.321879	3015.110718	20.817075
71.002900	3014.496767	20.822093
71.349592	3003.784805	20.827111
71.562266	3005.956656	20.832128
71.503672	3019.134688	20.837146
71.749050	3008.032137	20.842163
71.708371	3011.804429	20.847181
71.532335	3004.439432	20.852199
71.864756	3000.170575	20.857216
71.793001	3004.523111	20.862234
72.184654	2994.409867	20.867251
71.961449	2984.039769	20.872269
71.811048	2968.357724	20.877287
72.134920	2960.740864	20.882304
71.524305	2968.749470	20.887322
72.295033	2985.489957	20.892339
72.435830	2995.247286	20.897357
72.494123	2991.773610	20.902375
72.661296	2994.329713	20.907392
72.580650	2980.829047	20.912410
72.765077	2967.151423	20.917427
72.107531	2958.367130	20.922445
71.903438	2970.660440	20.927463
72.548001	2976.240030	20.932480
72.409525	2988.993851	20.937498
72.665819	2982.609281	20.942515
72.764582	2983.340527	20.947533
73.071804	2992.323504	20.952551
72.645207	2987.438177	20.957568
72.369931	2985.166802	20.962586
72.467873	2998.649541	20.967603
72.824110	3018.865741	20.972621
72.641480	3015.577489	20.977639
72.782065	3013.351370	20.982656
73.014621	3040.057815	20.987674
73.372344	3041.404641	20.992691
73.473299	3046.645873	20.997709
73.160468	3051.253183	21.002727
73.677148	3050.355773	21.007744
73.306896	3053.107984	21.012762
73.369857	3047.036907	21.017779
73.989885	3066.466849	21.022797
73.765514	3071.285028	21.027815
73.829496	3074.855102	21.032832
73.816636	3086.818017	21.037850
74.738765	3067.872621	21.042867
74.363269	3073.931919	21.047885
74.153013	3061.997026	21.052903
74.140549	3060.574463	21.057920
74.223379	3068.509121	21.062938
74.402567	3071.560128	21.067955
74.782854	3085.709641	21.072973
74.675159	3100.885543	21.077991
74.925577	3096.696875	21.083008
74.588950	3097.401177	21.088026
74.797551	3095.201975	21.093043
74.800368	3103.548875	21.098061
74.703943	3099.092045	21.103079
75.103194	3096.974354	21.108096
74.827092	3102.500768	21.113114
75.103471	3103.246459	21.118131
75.200138	3110.351036	21.123149
75.246982	3124.705814	21.128167
75.788583	3125.694283	21.133184
75.685662	3127.403617	21.138202
75.812484	3114.390996	21.143219
75.807532	3118.208381	21.148237
75.667481	3124.873922	21.153255
75.762340	3117.939691	21.158272
75.865678	3128.042965	21.163290
75.731971	3113.589665	21.168307
75.886546	3117.499409	21.173325
76.076325	3123.845355	21.178343
75.816948	3111.698328	21.183360
75.832080	3142.459588	21.188378
76.391650	3142.593619	21.193395
76.405883	3144.990890	21.198413
76.323837	3155.822961	21.203431
76.318123	3144.014389	21.208448
76.529440	3153.685695	21.213466
76.561818	3145.530411	21.218483
76.602406	3147.949153	21.223501
76.748667	3152.469119	21.228519
76.934811	3157.931266	21.233536
76.793900	3176.126952	21.238554
77.271045	3175.378864	21.243571
77.185888	3173.185124	21.248589
77.469990	3179.334569	21.253607
77.534650	3174.368109	21.258624
77.008621	3172.609874	21.263642
77.316996	3175.383581	21.268659
77.478331	3174.805410	21.273677
77.209484	3173.168471	21.278695
77.761548	3167.903443	21.283712
77.215010	3177.560571	21.288730
77.420640	3191.855109	21.293747
77.877771	3196.022514	21.298765
77.833418	3199.605677	21.303783
77.729248	3199.529815	21.308800
77.987685	3196.621907	21.313818
78.114153	3196.294647	21.318835
78.042600	3198.898800	21.323853
78.303222	3216.973712	21.328871
78.694701	3215.616555	21.333888
78.429248	3216.347250	21.338906
79.014310	3221.181064	21.343923
78.994995	3220.870135	21.348941
78.649534	3227.593776	21.353959
79.240879	3222.110927	21.358976
78.757934	3230.660100	21.363994
79.293991	3228.878069	21.369011
79.253677	3226.820758	21.374029
79.095105	3227.503990	21.379047
79.419350	3216.307439	21.384064
79.431222	3224.040122	21.389082
79.405596	3222.741874	21.394099
79.461313	3218.540876	21.399117
79.305150	3217.810794	21.404135
79.232128	3218.484871	21.409152
79.218790	3225.738309	21.414170
79.200624	3227.680419	21.419187
79.519340	3239.564551	21.424205
79.341209	3257.255578	21.429223
79.440976	3248.161716	21.434240
79.357951	3261.755251	21.439258
79.344085	3283.072477	21.444275
80.114055	3294.943078	21.449293
79.526161	3292.454328	21.454311
80.201153	3298.161919	21.459328
80.733576	3301.413097	21.464346
80.803855	3304.077222	21.469363
81.031883	3299.784442	21.474381
81.234068	3290.058689	21.479399
81.179668	3273.384078	21.484416
81.327570	3269.510643	21.489434
81.239056	3263.451276	21.494451
81.320120	3248.654665	21.499469
80.996040	3254.620946	21.504487
81.585912	3264.166776	21.509504
81.268011	3259.332821	21.514522
81.410277	3257.927029	21.519539
81.017869	3249.633449	21.524557
81.063281	3254.014008	21.529575
81.390973	3251.822720	21.534592
81.369302	3263.710886	21.539610
81.358370	3282.821621	21.544627
81.750237	3285.842508	21.549645
81.610303	3291.684299	21.554663
82.229417	3288.412110	21.559680
82.122813	3296.814889	21.564698
82.402738	3294.283678	21.569715
82.253796	3288.841880	21.574733
82.389802	3301.077138	21.579751
82.450941	3285.464831	21.584768
82.351145	3291.703765	21.589786
82.073520	3293.446219	21.594803
82.329426	3290.388302	21.599821
82.322289	3307.104982	21.604839
82.187296	3314.729001	21.609856
82.386075	3316.719773	21.614874
82.371452	3320.166342	21.619891
82.570978	3326.138177	21.624909
82.621193	3349.931668	21.629927
82.717063	3348.184139	21.634944
83.019344	3350.937658	21.639962
82.837735	3352.797545	21.644979
83.155729	3366.104259	21.649997
83.348756	3377.290198	21.655015
83.346870	3385.092263	21.660032
83.638815	3379.853649	21.665050
83.507466	3377.481931	21.670067
84.066001	3382.578670	21.675085
83.834240	3374.920622	21.680103
83.953119	3366.280210	21.685120
84.261257	3367.033858	21.690138
84.178472	3375.945308	21.695155
84.625476	3371.349552	21.700173
83.973412	3371.450318	21.705191
84.168739	3375.477577	21.710208
84.393521	3394.648845	21.715226
84.320598	3407.157067	21.720243
84.474418	3392.084008	21.725261
84.449613	3399.930176	21.730279
84.506975	3397.713546	21.735296
84.601528	3395.084937	21.740314
84.764438	3394.048906	21.745331
85.086634	3406.269651	21.750349
85.260451	3419.554662	21.755367
85.307548	3410.995838	21.760384
85.194702	3420.542530	21.765402
85.104490	3423.124717	21.770419
85.656894	3410.350770	21.775437
85.414842	3427.550472	21.780455
85.287069	3418.478983	21.785472
85.520162	3417.068631	21.790490
85.388156	3416.169794	21.795507
85.942030	3408.041528	21.800525
85.883606	3413.443309	21.805543
86.020301	3408.336050	21.810560
86.063531	3411.231653	21.815578
86.298390	3435.916661	21.820595
86.405679	3440.522937	21.825613
86.106621	3449.158050	21.830631
86.379282	3455.245771	21.835648
86.601300	3449.361492	21.840666
86.206530	3449.422871	21.845683
86.436872	3449.147893	21.850701
86.511416	3451.104851	21.855719
86.239995	3443.438605	21.860736
86.706883	3465.621903	21.865754
86.502267	3471.169267	21.870771
86.864653	3470.128960	21.875789
86.788858	3479.955228	21.880807
87.281708	3474.311974	21.885824
87.236804	3491.034537	21.890842
87.603082	3494.487510	21.895859
87.823127	3498.468821	21.900877
88.220400	3498.275483	21.905895
88.293444	3481.729231	21.910912
87.954890	3473.965005	21.915930
87.831031	3466.952344	21.920947
88.319368	3451.370593	21.925965
87.956211	3460.425456	21.930983
87.813812	3465.360440	21.936000
88.098060	3477.549943	21.941018
87.926334	3496.392373	21.946035
88.240893	3495.739879	21.951053
88.107358	3492.038291	21.956071
88.359261	3494.900497	21.961088
88.522553	3494.889039	21.966106
88.552236	3512.555750	21.971123
88.780627	3503.574366	21.976141
88.716889	3513.030786	21.981159
88.838260	3515.642870	21.986176
88.641936	3512.137912	21.991194
88.401605	3519.372908	21.996211
88.930347	3524.245615	22.001229
89.146483	3545.178801	22.006247
89.321224	3546.522391	22.011264
89.639273	3549.696965	22.016282
89.081765	3546.669767	22.021299
89.566622	3550.749819	22.026317
89.481975	3551.770077	22.031335
89.544269	3562.861212	22.036352
89.542970	3569.453535	22.041370
89.903979	3575.944365	22.046387
89.559225	3567.978746	22.051405
89.799594	3566.103245	22.056423
89.540259	3588.063897	22.061440
89.946542	3591.966047	22.066458
89.810710	3592.543008	22.071475
90.307745	3601.670213	22.076493
90.519486	3619.356237	22.081511
90.180933	3626.127691	22.086528
90.563996	3626.535358	22.091546
90.755622	3630.427852	22.096563
90.705252	3625.543190	22.101581
90.640519	3635.226679	22.106599
90.708315	3658.600200	22.111616
91.021798	3663.422433	22.116634
91.076852	3659.112743	22.121651
91.517025	3657.382548	22.126669
91.729544	3661.906266	22.131687
91.375862	3662.826951	22.136704
91.558426	3657.755065	22.141722
91.268084	3674.269446	22.146739
91.883872	3681.523922	22.151757
91.806832	3691.634068	22.156775
91.753726	3691.213146	22.161792
92.076993	3688.087686	22.166810
91.900465	3695.499270	22.171827
92.399185	3701.923226	22.176845
92.413853	3712.294895	22.181863
92.372734	3720.562232	22.186880
92.804535	3717.617420	22.191898
92.956389	3725.513797	22.196915
93.565952	3721.113750	22.201933
93.509559	3714.164234	22.206951
93.413913	3702.755794	22.211968
93.382911	3683.548563	22.216986
93.096870	3689.065070	22.222003
93.114724	3677.826212	22.227021
93.309445	3701.966416	22.232039
93.656734	3712.474808	22.237056
93.645730	3710.917258	22.242074
93.724399	3712.543540	22.247091
94.017421	3702.343581	22.252109
93.854985	3712.695995	22.257127
93.400711	3717.059963	22.262144
93.813920	3708.405921	22.267162
93.569370	3717.066488	22.272179
93.588042	3714.497303	22.277197
93.843047	3728.014385	22.282215
94.088041	3748.389215	22.287232
94.097933	3737.387170	22.292250
94.045106	3750.128497	22.297267
93.640032	3751.710914	22.302285
94.185311	3762.719386	22.307303
94.110966	3775.138356	22.312320
94.496288	3769.579593	22.317338
94.362393	3797.583526	22.322355
94.552778	3802.882926	22.327373
94.639895	3811.210235	22.332391
94.968644	3808.256296	22.337408
95.605109	3805.782018	22.342426
95.347645	3809.391617	22.347443
95.719285	3817.533896	22.352461
95.360596	3819.795941	22.357479
95.376275	3838.545217	22.362496
95.627244	3840.439686	22.367514
95.571753	3832.282572	22.372531
95.710106	3835.065070	22.377549
96.003626	3833.707331	22.382567
96.142831	3850.703511	22.387584
96.367197	3849.912097	22.392602
96.161396	3856.917649	22.397619
96.579068	3859.891695	22.402637
96.785469	3852.915966	22.407655
96.869052	3863.562606	22.412672
97.290454	3854.653472	22.417690
97.173815	3858.586270	22.422707
96.855101	3851.743100	22.427725
97.103542	3853.155204	22.432743
96.814615	3851.527147	22.437760
96.843049	3846.316230	22.442778
96.744807	3848.588760	22.447795
96.878889	3852.729030	22.452813
97.075672	3868.158270	22.457831
97.101803	3881.461902	22.462848
97.255099	3882.383105	22.467866
97.300806	3897.991858	22.472883
97.819869	3912.457783	22.477901
98.035434	3911.897856	22.482919
98.086522	3915.518376	22.487936
98.319224	3915.047660	22.492954
97.786232	3911.913798	22.497971
98.361970	3919.629699	22.502989
98.438098	3909.765294	22.508007
98.498811	3923.096899	22.513024
98.344396	3940.950810	22.518042
98.273592	3948.801199	22.523059
98.545946	3948.189791	22.528077
99.078797	3948.003925	22.533095
99.477996	3937.899814	22.538112
99.824901	3928.390654	22.543130
99.144746	3939.796003	22.548147
99.076137	3933.291907	22.553165
99.506259	3934.675234	22.558183
99.322585	3938.677828	22.563200
99.775543	3954.532647	22.568218
99.622435	3970.084981	22.573235
99.679051	3953.981323	22.578253
100.044210	3954.696086	22.583271
99.835893	3960.393113	22.588288
100.099828	3952.082723	22.593306
100.082606	3954.989577	22.598323
100.321449	3954.169686	22.603341
99.996775	3957.945212	22.608359
100.132505	3953.838203	22.613376
100.379227	3965.535176	22.618394
100.165601	3985.188730	22.623411
100.356807	3991.492253	22.628429
100.725590	3991.673973	22.633447
100.752321	3995.117537	22.638464
101.081297	3992.637666	22.643482
100.937382	3999.692528	22.648499
100.538100	4013.092833	22.653517
101.049652	4020.413383	22.658535
100.910603	4029.046581	22.663552
101.438790	4032.262413	22.668570
101.132394	4049.899131	22.673587
101.296093	4049.449693	22.678605
101.763545	4041.113816	22.683623
101.514679	4054.379678	22.688640
102.103841	4065.430459	22.693658
102.227510	4080.240778	22.698675
102.514633	4086.353832	22.703693
102.782202	4082.294285	22.708711
102.358479	4085.567785	22.713728
102.836382	4081.221717	22.718746
102.545360	4080.354828	22.723763
102.553309	4086.362160	22.728781
103.081203	4079.799844	22.733799
102.944607	4077.842416	22.738816
103.000278	4078.355845	22.743834
103.031227	4073.650857	22.748851
102.985551	4071.239142	22.753869
103.246811	4080.415713	22.758887
102.990302	4099.983824	22.763904
103.516975	4099.748608	22.768922
103.422663	4108.687650	22.773939
103.686042	4105.065941	22.778957
103.748563	4106.709998	22.783975
103.744051	4117.052929	22.788992
104.140273	4122.345502	22.794010
104.120215	4129.387852	22.799027
104.054261	4131.804533	22.804045
104.368015	4124.905582	22.809063
104.176726	4134.843420	22.814080
104.624648	4130.697020	22.819098
104.679710	4132.774759	22.824115
104.816620	4156.296265	22.829133
104.626050	4153.795175	22.834151
104.738308	4157.285545	22.839168
104.917881	4159.644386	22.844186
105.078879	4165.690881	22.849203
104.591101	4165.468122	22.854221
105.086208	4171.028876	22.859239
104.970338	4188.814236	22.864256
105.129844	4189.609162	22.869274
105.233459	4190.052154	22.874291
105.286378	4206.884721	22.879309
105.476488	4217.895333	22.884327
105.685542	4225.617542	22.889344
105.954916	4221.068539	22.894362
106.179396	4216.287797	22.899379
106.284893	4224.909894	22.904397
106.583424	4226.534767	22.909415
106.466843	4241.080828	22.914432
106.756924	4235.210582	22.919450
107.142382	4229.169613	22.924467
106.663303	4239.893280	22.929485
107.247672	4230.900864	22.934503
107.150751	4241.872487	22.939520
107.367707	4240.342750	22.944538
106.817210	4230.120879	22.949555
106.893400	4245.423878	22.954573
107.285926	4241.461799	22.959591
107.002378	4259.630414	22.964608
107.577079	4269.124329	22.969626
107.646909	4268.649235	22.974643
107.972487	4260.947974	22.979661
108.090805	4259.735230	22.984679
108.156671	4259.191504	22.989696
108.329891	4254.397486	22.994714
108.498681	4256.955095	22.999731
108.210848	4256.516903	23.004749
108.573730	4267.742879	23.009767
108.560322	4287.249065	23.014784
108.352218	4280.617517	23.019802
108.648125	4285.426416	23.024819
108.579846	4289.763744	23.029837
109.148120	4291.901592	23.034855
109.032136	4314.330938	23.039872
109.101019	4311.454539	23.044890
109.293450	4313.040115	23.049907
109.390310	4316.847423	23.054925
109.440328	4311.065563	23.059943
109.348810	4322.960199	23.064960
109.765678	4330.718506	23.069978
109.981189	4356.318767	23.074995
109.476463	4350.902153	23.080013
109.960026	4348.881691	23.085031
110.025256	4345.785377	23.090048
109.935465	4348.989078	23.095066
110.362698	4364.062671	23.100083
110.274785	4370.974988	23.105101
110.733004	4370.910607	23.110119
110.783604	4380.391262	23.115136
110.606607	4382.411939	23.120154
111.241137	4375.284609	23.125171
111.153428	4375.492613	23.130189
111.325669	4375.224432	23.135207
111.340979	4363.845325	23.140224
111.590624	4385.525278	23.145242
111.583442	4388.085511	23.150259
111.374707	4386.561004	23.155277
111.656305	4381.088336	23.160295
111.702536	4390.954896	23.165312
111.661996	4391.784916	23.170330
111.970487	4383.290234	23.175347
111.798694	4388.454229	23.180365
112.102396	4401.761909	23.185383
112.296893	4419.402954	23.190400
112.446434	4420.760392	23.195418
112.337130	4417.562452	23.200435
112.092773	4423.653337	23.205453
112.960091	4426.364526	23.210471
113.010240	4437.967955	23.215488
112.913128	4453.061427	23.220506
113.224046	4443.450224	23.225523
112.806282	4445.967436	23.230541
113.203419	4443.190689	23.235559
113.268850	4448.105312	23.240576
113.435956	4462.653350	23.245594
114.030871	4468.089195	23.250611
112.975524	4477.375933	23.255629
113.143616	4472.207028	23.260647
113.503713	4480.156298	23.265664
113.637404	4498.497034	23.270682
114.211396	4499.509979	23.275699
114.105503	4499.452519	23.280717
114.496244	4517.721642	23.285735
114.618934	4534.668618	23.290752
114.613657	4532.104195	23.295770
115.074572	4526.215582	23.300787
115.301038	4530.432346	23.305805
115.441978	4529.160569	23.310823
115.267525	4526.999276	23.315840
115.608199	4530.335576	23.320858
115.907312	4522.952205	23.325875
115.180582	4527.300877	23.330893
115.394049	4524.838365	23.335911
115.800890	4519.998702	23.340928
115.827703	4527.797198	23.345946
116.012338	4536.570514	23.350963
115.665847	4549.858251	23.355981
116.022595	4550.741465	23.360999
116.206015	4551.125103	23.366016
116.167474	4552.922793	23.371034
116.594678	4564.868093	23.376051
116.644019	4578.817346	23.381069
116.654011	4579.172431	23.386087
116.607494	4582.824015	23.391104
116.762687	4586.493002	23.396122
116.854688	4581.684455	23.401139
116.767150	4588.982745	23.406157
117.004600	4600.858999	23.411175
117.240796	4613.516814	23.416192
117.238977	4610.507557	23.421210
117.502135	4613.166404	23.426227
117.369946	4616.341984	23.431245
117.494668	4632.292353	23.436263
117.695945	4648.782538	23.441280
117.873345	4654.934316	23.446298
117.959904	4645.423679	23.451315
117.880328	4655.043386	23.456333
118.048405	4664.451300	23.461351
118.137279	4665.179596	23.466368
118.337333	4672.016684	23.471386
118.719634	4686.464236	23.476403
118.805922	4710.774225	23.481421
118.942490	4694.548987	23.486439
119.005861	4698.113234	23.491456
118.669357	4698.177223	23.496474
119.387825	4716.899997	23.501491
119.315460	4727.262836	23.506509
119.536764	4725.083289	23.511527
119.593049	4725.954225	23.516544
119.594760	4731.343783	23.521562
119.879183	4742.872615	23.526579
120.002703	4757.609555	23.531597
120.068011	4762.713332	23.536615
120.236689	4762.262235	23.541632
120.242553	4758.641994	23.546650
120.243643	4764.332550	23.551667
120.231950	4781.559602	23.556685
120.651386	4794.739864	23.561703
120.872944	4794.415964	23.566720
120.686045	4799.913493	23.571738
121.029745	4818.825086	23.576755
121.072626	4823.700371	23.581773
121.278735	4838.631955	23.586791
121.473653	4831.515202	23.591808
121.367222	4831.787858	23.596826
121.740791	4836.137015	23.601843
122.117057	4841.356853	23.606861
122.128816	4845.909817	23.611879
122.346914	4843.956860	23.616896
122.244702	4851.104195	23.621914
122.329583	4846.696127	23.626931
122.148905	4846.761757	23.631949
122.112128	4846.204891	23.636967
122.630854	4864.175221	23.641984
122.504004	4880.037430	23.647002
122.732004	4880.348059	23.652019
122.905408	4888.565050	23.657037
123.032177	4904.297950	23.662055
123.115160	4899.568831	23.667072
123.242427	4907.833912	23.672090
123.439140	4905.512841	23.677107
123.414434	4899.454508	23.682125
123.539278	4912.189939	23.687143
123.523315	4925.014894	23.692160
123.995953	4935.451418	23.697178
124.617325	4930.591395	23.702195
124.394044	4934.775887	23.707213
124.282675	4939.330295	23.712231
124.626835	4932.297396	23.717248
124.187155	4934.886966	23.722266
124.537011	4941.283395	23.727283
124.596613	4957.913975	23.732301
124.286833	4965.429336	23.737319
124.501260	4967.764208	23.742336
124.635832	4993.417971	23.747354
125.027806	4989.555049	23.752371
124.997193	4997.241534	23.757389
125.137870	5015.722662	23.762407
125.682206	5029.275538	23.767424
125.719374	5026.823482	23.772442
125.765368	5027.625310	23.777459
125.952112	5045.689780	23.782477
126.310101	5050.799397	23.787495
126.269075	5055.879752	23.792512
125.947492	5065.765680	23.797530
126.177411	5058.860220	23.802547
126.223179	5072.312717	23.807565
126.382478	5085.761515	23.812583
127.199310	5076.673638	23.817600
127.332646	5088.537389	23.822618
127.639112	5095.940863	23.827635
127.974104	5098.972646	23.832653
127.381311	5083.831424	23.837671
127.763878	5092.472658	23.842688
127.520801	5101.386563	23.847706
128.109206	5098.058633	23.852723
128.152923	5100.711863	23.857741
128.307883	5098.195494	23.862759
128.220447	5101.973936	23.867776
128.222375	5101.119777	23.872794
128.294261	5099.779453	23.877811
128.176916	5125.213536	23.882829
128.159198	5125.352051	23.887847
128.821842	5125.924505	23.892864
128.803565	5162.399688	23.897882
128.927205	5160.818911	23.902899
129.383831	5167.402709	23.907917
129.041028	5171.543952	23.912935
129.431970	5160.626826	23.917952
129.534587	5178.910664	23.922970
129.700711	5185.860126	23.927987
129.825665	5186.605891	23.933005
129.809682	5190.188579	23.938023
129.878309	5187.713776	23.943040
129.864971	5205.354307	23.948058
130.171873	5215.463404	23.953075
129.990422	5217.325839	23.958093
130.257927	5224.620266	23.963111
131.161904	5231.400721	23.968128
130.781330	5247.363506	23.973146
130.999297	5248.344595	23.978163
130.935615	5246.183904	23.983181
131.098608	5248.126711	23.988199
131.254775	5236.593653	23.993216
131.056996	5256.320891	23.998234
131.493216	5267.133296	24.003251
131.662526	5278.530233	24.008269
131.475533	5280.476332	24.013287
131.843807	5275.936069	24.018304
131.696481	5287.002911	24.023322
131.730424	5303.346813	24.028339
131.928687	5300.611892	24.033357
132.309127	5318.566275	24.038375
132.663780	5330.352093	24.043392
132.601010	5333.682114	24.048410
132.623312	5330.095945	24.053427
133.099836	5336.121880	24.058445
133.362606	5353.475788	24.063463
134.291121	5331.895784	24.068480
134.399643	5324.289512	24.073498
134.688566	5302.659297	24.078515
134.718082	5290.062499	24.083533
134.811882	5290.055869	24.088551
135.075978	5278.066332	24.093568
135.122350	5281.015302	24.098586
134.962751	5258.234846	24.103603
135.438776	5235.610113	24.108621
134.998246	5251.596571	24.113639
135.511519	5244.956735	24.118656
135.310566	5238.791433	24.123674
135.435387	5243.581909	24.128691
135.739140	5240.570558	24.133709
135.599355	5247.561464	24.138727
135.644433	5239.361965	24.143744
135.616523	5244.389721	24.148762
135.540481	5240.810192	24.153779
135.967058	5237.953436	24.158797
135.769630	5243.552169	24.163815
135.585081	5239.869154	24.168832
136.110094	5252.214886	24.173850
135.809726	5275.974494	24.178867
135.993025	5280.410744	24.183885
135.740917	5284.126090	24.188903
136.301754	5297.189587	24.193920
135.799667	5314.994371	24.198938
136.310960	5327.345665	24.203955
136.355979	5345.774262	24.208973
136.290897	5373.230410	24.213991
136.238724	5383.524838	24.219008
136.494628	5402.816087	24.224026
136.725461	5418.046448	24.229043
136.933393	5425.610327	24.234061
136.998763	5439.425258	24.239079
137.478550	5455.394354	24.244096
137.677979	5479.199336	24.249114
137.764605	5485.748239	24.254131
138.140935	5483.092248	24.259149
138.194491	5502.177277	24.264167
138.455708	5512.303848	24.269184
138.974228	5514.357454	24.274202
138.657701	5512.231408	24.279219
139.270126	5523.407624	24.284237
139.175141	5537.814900	24.289255
139.564571	5540.735038	24.294272
139.575762	5534.640377	24.299290
139.381893	5547.630241	24.304307
139.570826	5540.339332	24.309325
139.194353	5565.728747	24.314343
139.570013	5565.851815	24.319360
139.916087	5569.555262	24.324378
139.729487	5580.803120	24.329395
140.222347	5596.641724	24.334413
140.368331	5605.345065	24.339431
140.793869	5602.482122	24.344448
140.525752	5611.257245	24.349466
140.927403	5625.083217	24.354483
141.184076	5623.874221	24.359501
141.246792	5624.285670	24.364519
141.208157	5629.573747	24.369536
141.468551	5640.475628	24.374554
141.633049	5657.101561	24.379571
141.757521	5648.358125	24.384589
141.760281	5661.592427	24.389607
142.229628	5675.814862	24.394624
142.381212	5679.233450	24.399642
142.582057	5689.550865	24.404659
142.871689	5684.453681	24.409677
142.753797	5684.003638	24.414695
142.419762	5676.898419	24.419712
142.857511	5698.710188	24.424730
143.154275	5706.789090	24.429747
143.527324	5715.356680	24.434765
143.148433	5718.657478	24.439783
143.588014	5716.431715	24.444800
143.433113	5716.736325	24.449818
143.347638	5734.957736	24.454835
143.989766	5738.886952	24.459853
143.869785	5755.830361	24.464871
144.041704	5751.303934	24.469888
144.178219	5765.085683	24.474906
144.266105	5763.815028	24.479923
144.863190	5764.850889	24.484941
144.365523	5780.715337	24.489959
144.639422	5790.987211	24.494976
145.140352	5794.939071	24.499994
144.795290	5795.421218	24.505011
145.020334	5804.893300	24.510029
145.355839	5828.622702	24.515047
145.461452	5828.314722	24.520064
145.748237	5834.252859	24.525082
145.830123	5834.080493	24.530099
146.129913	5835.663574	24.535117
145.567342	5850.896456	24.540135
145.915885	5847.839504	24.545152
146.422172	5861.748570	24.550170
146.600125	5888.532206	24.555187
146.747841	5891.741974	24.560205
146.835251	5891.834116	24.565223
146.958858	5891.442705	24.570240
146.713242	5895.529661	24.575258
147.090017	5911.734283	24.580275
147.540211	5914.228956	24.585293
147.457000	5921.663387	24.590311
147.823902	5915.577706	24.595328
148.064376	5928.696646	24.600346
148.066895	5932.863956	24.605363
148.536019	5938.975677	24.610381
148.655897	5944.395801	24.615399
148.812421	5936.022449	24.620416
149.056539	5936.266535	24.625434
148.967994	5941.549093	24.630451
149.057164	5940.255361	24.635469
148.883005	5952.304805	24.640487
149.059609	5959.073214	24.645504
149.544821	5956.964054	24.650522
149.678972	5956.267567	24.655539
149.833314	5960.794045	24.660557
149.833604	5968.018044	24.665575
150.052936	5980.079612	24.670592
150.252215	5984.310092	24.675610
150.401831	5988.483708	24.680627
150.384458	5977.063362	24.685645
150.636823	5995.354764	24.690663
150.743640	5999.941389	24.695680
151.008728	6011.906126	24.700698
150.670147	6017.739645	24.705715
150.826373	6016.054736	24.710733
151.108714	6041.052328	24.715751
151.565371	6050.718013	24.720768
150.888151	6043.774651	24.725786
151.380530	6066.147074	24.730803
151.637115	6070.052669	24.735821
151.898622	6080.891645	24.740839
151.773232	6106.661876	24.745856
152.141638	6113.501449	24.750874
151.919461	6114.199639	24.755891
152.584973	6138.069071	24.760909
152.580842	6144.958342	24.765927
152.963973	6153.952170	24.770944
152.647001	6157.416527	24.775962
152.243937	6186.598821	24.780979
152.849008	6184.530527	24.785997
153.340442	6208.024232	24.791015
153.118936	6217.617224	24.796032
153.431738	6220.930308	24.801050
153.316344	6235.551245	24.806067
153.634179	6241.952118	24.811085
153.951755	6259.138501	24.816103
154.011099	6266.905491	24.821120
154.330718	6277.001271	24.826138
154.050011	6296.665237	24.831155
154.447499	6303.577103	24.836173
154.552416	6312.966101	24.841191
154.621529	6329.115185	24.846208
155.038775	6332.315073	24.851226
155.269398	6347.105235	24.856243
155.645026	6368.595365	24.861261
155.665012	6366.123993	24.866279
155.997600	6358.492996	24.871296
156.343793	6365.745315	24.876314
156.407463	6391.581273	24.881331
156.573085	6384.142734	24.886349
156.410722	6385.183583	24.891367
156.637750	6389.754439	24.896384
156.841364	6402.300322	24.901402
156.843819	6430.547830	24.906419
157.168565	6425.848498	24.911437
156.984141	6420.181685	24.916455
157.400719	6441.351377	24.921472
157.872037	6444.018967	24.926490
157.549655	6452.949581	24.931507
158.011955	6451.853369	24.936525
158.149873	6465.607914	24.941543
158.073543	6482.754934	24.946560
158.316209	6488.258175	24.951578
158.462611	6499.230602	24.956595
158.894853	6509.944498	24.961613
159.054392	6514.284338	24.966631
159.098623	6516.970801	24.971648
159.092254	6505.504078	24.976666
159.149532	6541.507065	24.981683
159.347526	6543.065921	24.986701
159.995343	6546.142827	24.991719
160.332606	6534.640019	24.996736
160.725342	6532.944445	25.001754
160.653545	6537.466529	25.006771
161.064565	6550.442525	25.011789
160.993537	6544.044116	25.016807
161.049256	6554.748542	25.021824
161.351545	6560.262856	25.026842
161.021260	6570.284329	25.031859
161.192774	6565.916865	25.036877
161.268134	6559.014412	25.041895
161.541968	6568.307647	25.046912
161.655509	6574.389195	25.051930
161.568566	6587.788525	25.056947
161.673055	6596.871334	25.061965
161.783978	6603.722961	25.066983
161.923162	6606.928823	25.072000
161.982120	6617.203419	25.077018
162.200233	6634.973643	25.082035
162.569254	6640.596282	25.087053
163.043219	6661.661114	25.092071
162.994436	6660.891976	25.097088
162.953036	6662.688817	25.102106
162.693145	6660.546602	25.107123
163.193138	6669.998849	25.112141
163.734717	6674.166108	25.117159
164.072529	6673.354328	25.122176
164.496913	6690.399192	25.127194
164.107428	6695.928949	25.132211
164.584853	6703.604000	25.137229
165.022230	6701.283955	25.142247
165.171891	6699.492968	25.147264
165.206441	6692.224851	25.152282
165.180260	6694.146702	25.157299
165.718843	6697.107661	25.162317
165.870724	6695.950425	25.167335
165.482318	6693.764066	25.172352
166.324386	6700.132762	25.177370
165.578961	6710.252271	25.182387
165.916731	6712.068407	25.187405
165.539103	6711.938569	25.192423
165.707865	6738.611773	25.197440
165.948573	6751.576955	25.202458
165.989921	6763.271028	25.207475
166.537016	6782.599898	25.212493
166.329832	6791.574760	25.217511
166.351540	6816.236978	25.222528
167.174287	6824.383832	25.227546
167.162189	6837.107256	25.232563
167.391472	6862.427968	25.237581
167.603321	6853.402637	25.242599
168.093217	6880.254200	25.247616
167.815679	6889.647657	25.252634
167.930203	6892.327648	25.257651
168.385891	6899.054916	25.262669
168.927369	6913.954593	25.267687
168.571799	6921.010790	25.272704
169.074719	6909.903127	25.277722
169.174630	6920.175624	25.282739
169.320483	6933.752756	25.287757
169.989799	6936.614937	25.292775
170.062078	6933.907640	25.297792
170.580912	6934.514284	25.302810
170.322938	6925.611203	25.307827
170.784118	6923.707707	25.312845
170.747895	6923.253868	25.317863
170.884217	6927.129088	25.322880
171.122742	6920.226080	25.327898
170.860373	6926.937022	25.332915
170.614163	6928.033242	25.337933
171.116493	6941.655618	25.342951
170.966278	6959.928911	25.347968
171.415634	6952.595870	25.352986
171.405320	6966.774074	25.358003
171.756145	6982.086195	25.363021
171.642785	6985.292888	25.368039
171.743330	7002.601569	25.373056
171.978387	7012.787937	25.378074
171.863823	7020.217224	25.383091
171.995060	7030.040914	25.388109
172.294111	7046.407327	25.393127
172.609418	7060.530582	25.398144
172.648569	7074.117459	25.403162
172.969842	7083.999985	25.408179
173.161144	7101.638254	25.413197
173.296894	7115.339375	25.418215
173.577746	7126.342753	25.423232
173.821546	7130.642321	25.428250
174.152819	7147.123842	25.433267
173.845245	7151.960659	25.438285
174.364507	7161.851045	25.443303
174.431066	7180.125241	25.448320
174.864925	7180.455777	25.453338
174.986241	7190.442758	25.458355
175.071068	7206.304076	25.463373
175.317789	7216.574441	25.468391
175.156762	7220.201354	25.473408
175.361153	7232.884830	25.478426
175.963591	7244.045859	25.483443
176.005072	7253.304486	25.488461
176.210082	7253.058219	25.493479
176.093702	7275.227105	25.498496
176.473392	7274.646026	25.503514
176.738249	7295.340265	25.508531
176.908842	7304.546067	25.513549
177.254665	7302.188853	25.518567
176.905934	7321.883067	25.523584
177.272686	7330.833105	25.528602
177.602225	7340.677348	25.533619
178.320071	7343.779436	25.538637
178.775901	7352.252581	25.543655
178.868638	7358.691705	25.548672
178.640398	7359.247610	25.553690
178.837358	7360.169415	25.558707
178.808856	7357.768437	25.563725
179.264875	7348.846710	25.568743
179.054629	7359.240406	25.573760
179.401521	7370.302743	25.578778
179.227974	7379.140608	25.583795
179.541133	7390.461618	25.588813
179.873814	7386.918678	25.593831
180.179417	7407.930642	25.598848
180.103077	7414.046637	25.603866
180.227559	7420.522096	25.608883
180.325363	7419.123567	25.613901
180.615701	7419.450353	25.618919
180.843585	7445.641935	25.623936
181.170942	7448.729054	25.628954
181.136783	7453.619139	25.633971
181.001279	7446.232517	25.638989
181.372388	7463.626087	25.644007
181.313943	7478.607075	25.649024
181.536995	7485.096387	25.654042
182.003693	7499.504464	25.659059
181.611708	7515.957520	25.664077
181.956018	7519.586105	25.669095
182.071667	7541.524940	25.674112
182.675199	7547.867125	25.679130
182.731751	7568.516284	25.684148
183.131751	7574.765749	25.689165
183.506147	7567.995154	25.694183
183.742492	7585.371781	25.699200
183.777539	7606.461896	25.704218
184.118258	7602.105325	25.709236
184.312164	7601.905861	25.714253
184.964903	7589.836160	25.719271
184.808245	7588.267747	25.724288
185.643337	7576.726911	25.729306
185.808984	7569.933017	25.734324
185.815307	7574.735057	25.739341
185.956459	7568.592133	25.744359
185.926203	7569.967276	25.749376
185.810744	7572.181048	25.754394
186.291576	7567.591705	25.759412
185.972221	7568.496468	25.764429
186.361767	7581.161085	25.769447
186.351668	7595.172009	25.774464
186.303206	7591.347737	25.779482
186.542876	7605.770407	25.784500
186.765926	7628.425167	25.789517
186.610612	7625.778039	25.794535
186.619103	7646.165326	25.799552
186.899259	7657.938073	25.804570
187.327809	7660.284697	25.809588
187.246284	7686.884218	25.814605
187.918862	7692.587545	25.819623
187.699642	7698.650149	25.824640
188.150926	7707.974290	25.829658
188.600140	7717.876243	25.834676
188.735590	7735.409768	25.839693
188.681279	7741.246383	25.844711
189.092671	7747.846895	25.849728
189.083967	7764.703239	25.854746
189.336497	7772.121151	25.859764
189.351444	7792.322385	25.864781
189.871253	7802.736174	25.869799
189.889822	7815.051765	25.874816
190.151828	7826.345614	25.879834
190.428680	7830.180421	25.884852
190.117586	7848.461032	25.889869
190.831001	7849.081630	25.894887
191.159092	7854.764501	25.899904
191.033768	7851.449655	25.904922
191.528846	7854.724749	25.909940
191.555493	7885.664947	25.914957
191.615795	7883.206126	25.919975
191.424410	7885.150136	25.924992
191.602877	7902.278629	25.930010
192.189793	7911.458319	25.935028
192.134077	7921.501313	25.940045
192.061832	7932.438939	25.945063
192.306147	7941.596231	25.950080
192.606859	7956.621664	25.955098
192.962011	7971.045350	25.960116
193.175924	7981.009073	25.965133
193.682670	7988.364601	25.970151
193.910594	7992.613554	25.975168
194.053650	7998.310075	25.980186
194.285322	8001.839121	25.985204
194.357664	8011.525402	25.990221
194.828292	8019.554408	25.995239
194.643407	8018.200348	26.000256
194.921471	8025.327239	26.005274
195.240488	8037.253528	26.010292
195.154786	8051.945871	26.015309
195.382592	8057.177259	26.020327
195.759419	8070.274588	26.025344
195.782155	8069.241023	26.030362
196.092806	8071.295948	26.035380
196.179847	8085.740487	26.040397
196.426678	8096.373005	26.045415
196.671017	8100.705044	26.050432
196.936712	8113.622931	26.055450
197.003000	8129.604936	26.060468
197.008790	8139.693458	26.065485
196.903510	8149.823872	26.070503
197.523588	8162.044496	26.075520
197.436336	8178.923404	26.080538
197.764317	8200.786564	26.085556
197.632762	8213.942796	26.090573
198.466031	8226.530286	26.095591
198.882803	8242.927377	26.100608
198.974584	8246.353620	26.105626
199.392254	8247.640220	26.110644
199.284773	8271.657963	26.115661
199.496741	8269.069092	26.120679
199.997825	8269.677264	26.125696
199.713034	8285.185464	26.130714
199.938273	8289.835957	26.135732
199.977528	8305.996880	26.140749
199.838513	8310.942226	26.145767
200.002826	8328.579382	26.150784
200.070553	8347.660649	26.155802
200.839283	8354.737454	26.160820
200.327139	8376.297383	26.165837
201.014307	8388.123797	26.170855
201.180876	8398.187283	26.175872
201.242357	8419.695421	26.180890
202.265758	8428.115178	26.185908
202.234196	8439.300643	26.190925
202.487967	8436.873963	26.195943
202.857041	8460.622793	26.200960
202.863304	8461.678984	26.205978
203.284722	8458.739049	26.210996
203.362420	8466.394452	26.216013
203.380034	8476.640299	26.221031
203.517733	8481.190043	26.226048
203.577167	8490.128811	26.231066
203.945223	8497.671430	26.236084
203.734111	8512.369934	26.241101
203.886940	8523.422218	26.246119
204.573946	8542.553551	26.251136
204.246084	8561.732821	26.256154
204.902526	8561.120019	26.261172
204.671688	8588.110602	26.266189
204.807074	8595.047127	26.271207
205.172405	8609.441280	26.276224
205.145013	8623.585269	26.281242
205.814311	8630.689485	26.286260
205.924677	8652.984481	26.291277
206.429859	8666.926130	26.296295
206.563775	8680.729746	26.301312
206.566037	8682.249886	26.306330
207.418618	8687.716306	26.311348
207.935812	8678.506044	26.316365
209.119546	8660.618515	26.321383
209.717038	8651.148699	26.326400
209.425350	8638.695717	26.331418
209.787669	8617.524312	26.336436
209.883080	8613.701132	26.341453
210.010718	8592.556594	26.346471
210.499691	8577.335321	26.351488
210.416505	8578.448608	26.356506
210.482796	8559.728554	26.361524
210.403563	8539.498769	26.366541
210.341893	8533.603749	26.371559
210.229940	8533.199872	26.376576
209.833100	8535.480129	26.381594
210.290353	8550.725090	26.386612
210.604339	8554.324448	26.391629
210.540475	8567.908188	26.396647
210.715368	8580.567851	26.401664
210.697875	8598.585479	26.406682
211.157718	8592.315845	26.411700
210.856562	8618.836380	26.416717
211.516526	8625.081089	26.421735
211.582067	8632.447944	26.426752
211.531494	8649.564500	26.431770
211.707378	8667.441911	26.436788
211.764150	8687.935691	26.441805
212.060973	8695.312563	26.446823
212.189135	8713.842659	26.451840
212.097002	8740.347259	26.456858
212.949199	8752.835019	26.461876
213.068456	8765.185287	26.466893
213.295628	8782.609690	26.471911
213.478974	8803.900491	26.476928
213.495025	8819.875248	26.481946
213.800727	8817.163077	26.486964
213.879209	8845.869783	26.491981
214.240119	8863.474614	26.496999
214.760397	8880.013761	26.502016
214.873997	8897.897377	26.507034
215.113726	8901.099073	26.512052
215.110075	8917.496440	26.517069
215.282043	8933.316951	26.522087
215.865263	8945.023725	26.527104
215.917356	8967.971246	26.532122
215.976580	8979.794653	26.537140
216.578930	8999.148250	26.542157
216.236392	9012.858919	26.547175
216.693544	9018.207304	26.552192
216.964757	9035.449527	26.557210
217.257466	9044.595216	26.562228
217.246890	9070.366275	26.567245
217.676828	9074.565919	26.572263
217.911798	9095.221120	26.577280
218.293176	9104.060135	26.582298
218.773252	9104.753095	26.587316
219.267385	9122.218770	26.592333
219.512960	9126.489424	26.597351
219.485467	9121.429766	26.602368
219.836766	9126.583610	26.607386
219.891535	9140.680090	26.612404
220.300616	9157.775906	26.617421
220.135394	9160.497140	26.622439
220.743957	9163.422942	26.627456
220.416436	9177.881222	26.632474
221.021460	9184.731195	26.637492
221.179202	9193.643260	26.642509
221.123548	9207.897391	26.647527
221.469848	9215.513412	26.652544
221.638910	9230.947083	26.657562
221.994377	9241.150472	26.662580
222.042721	9248.987762	26.667597
221.911714	9263.525884	26.672615
222.305766	9282.447535	26.677632
222.465703	9303.711493	26.682650
222.222858	9317.351755	26.687668
222.299298	9343.880446	26.692685
222.368181	9365.866027	26.697703
223.066682	9387.050383	26.702720
223.302849	9406.222998	26.707738
223.740568	9418.651541	26.712756
224.043357	9424.858519	26.717773
224.382548	9446.933390	26.722791
224.546007	9450.707662	26.727808
224.953586	9465.618492	26.732826
225.461231	9470.477769	26.737844
225.769039	9479.803905	26.742861
225.830157	9471.007012	26.747879
226.224136	9473.418141	26.752896
226.536912	9475.378342	26.757914
227.097282	9485.775248	26.762932
227.040157	9479.861770	26.767949
227.363727	9488.983512	26.772967
227.658489	9488.647773	26.777984
227.215891	9487.255033	26.783002
227.815039	9485.609664	26.788020
227.924655	9498.189055	26.793037
227.555272	9507.431165	26.798055
228.082978	9519.177815	26.803072
227.976343	9532.292241	26.808090
228.224978	9554.660116	26.813108
228.349161	9568.042280	26.818125
228.315325	9588.906494	26.823143
228.547732	9604.190996	26.828160
228.960577	9630.972921	26.833178
229.085498	9652.835831	26.838196
229.708092	9661.265075	26.843213
229.538825	9689.615500	26.848231
229.742437	9706.942516	26.853248
230.068129	9726.612293	26.858266
230.272984	9747.015062	26.863284
230.631887	9758.437846	26.868301
230.800795	9782.119724	26.873319
231.013794	9799.621717	26.878336
231.455897	9823.193794	26.883354
231.610037	9834.700581	26.888372
232.224668	9855.688775	26.893389
232.095704	9871.599607	26.898407
232.421890	9882.851599	26.903424
232.646551	9901.563491	26.908442
233.141910	9923.314418	26.913460
234.019571	9915.458317	26.918477
234.245103	9921.177627	26.923495
234.623625	9910.405190	26.928512
234.387553	9912.317703	26.933530
234.700472	9924.641965	26.938548
234.865298	9934.517614	26.943565
234.992670	9942.277086	26.948583
235.337979	9940.878463	26.953600
235.410964	9960.817183	26.958618
235.363765	9983.371880	26.963636
235.592567	9978.698216	26.968653
235.554530	10002.726323	26.973671
235.941969	9999.245136	26.978688
236.160413	10030.263723	26.983706
236.574723	10038.698929	26.988724
236.837570	10044.991785	26.993741
236.506116	10068.083825	26.998759
236.865284	10069.366427	27.003776
237.345136	10102.634729	27.008794
237.267068	10103.812639	27.013812
237.824707	10119.522504	27.018829
237.795583	10131.164920	27.023847
238.059877	10151.427217	27.028864
238.341257	10166.596701	27.033882
238.529270	10184.379162	27.038900
238.925483	10200.726622	27.043917
239.111083	10213.047715	27.048935
239.124689	10226.496652	27.053952
239.845853	10255.042116	27.058970
239.882058	10261.923871	27.063988
240.072767	10271.944994	27.069005
240.387618	10297.035040	27.074023
240.849192	10302.502863	27.079040
240.635615	10319.590029	27.084058
241.215778	10333.983570	27.089076
241.849076	10347.539124	27.094093
242.214995	10355.569920	27.099111
242.139374	10357.514863	27.104128
242.767544	10365.568473	27.109146
243.005396	10367.514839	27.114164
243.375954	10371.879439	27.119181
243.641158	10375.898079	27.124199
244.012391	10371.882230	27.129216
243.853947	10385.895001	27.134234
244.437333	10397.982587	27.139252
244.457033	10394.039596	27.144269
244.958795	10404.861592	27.149287
245.291669	10401.859276	27.154304
245.289685	10403.575712	27.159322
245.112092	10397.967775	27.164340
245.374097	10412.756305	27.169357
245.649373	10429.034903	27.174375
245.654306	10434.027921	27.179392
246.263992	10452.029930	27.184410
246.134980	10458.880206	27.189428
246.292535	10471.631783	27.194445
246.019051	10485.251485	27.199463
246.453316	10506.362843	27.204480
246.808357	10521.609858	27.209498
247.218809	10554.489141	27.214516
247.318618	10564.510268	27.219533
247.206782	10588.049189	27.224551
247.697830	10591.280636	27.229568
248.252346	10617.694797	27.234586
248.077783	10635.007259	27.239604
248.544082	10658.784422	27.244621
248.510392	10683.742553	27.249639
249.465429	10699.074420	27.254656
249.304993	10713.218611	27.259674
249.836958	10739.732965	27.264692
249.607049	10741.393951	27.269709
249.972146	10761.573545	27.274727
250.129285	10774.481444	27.279744
250.367050	10801.533275	27.284762
251.003191	10819.472850	27.289780
251.550929	10820.978487	27.294797
251.476058	10827.701446	27.299815
251.815598	10838.936057	27.304832
252.250994	10855.157694	27.309850
252.141077	10861.546282	27.314868
252.646432	10872.558659	27.319885
252.876142	10888.464162	27.324903
252.921460	10890.501902	27.329920
253.587082	10903.943648	27.334938
253.338616	10913.715812	27.339956
253.744486	10940.444367	27.344973
253.784142	10967.859795	27.349991
253.914211	10981.793682	27.355008
254.292865	10982.406414	27.360026
254.301306	11011.682103	27.365044
254.648714	11022.523092	27.370061
254.757423	11050.743142	27.375079
255.236530	11065.381589	27.380096
255.282311	11082.078397	27.385114
255.353699	11104.291258	27.390132
256.007307	11117.713178	27.395149
256.318774	11144.299082	27.400167
257.231420	11148.574129	27.405184
257.716379	11153.076925	27.410202
258.208506	11148.480715	27.415220
258.690582	11148.076596	27.420237
259.291178	11150.326495	27.425255
259.591286	11145.495293	27.430272
259.866418	11148.269026	27.435290
259.791516	11139.195121	27.440308
260.279145	11128.464643	27.445325
260.164926	11134.163823	27.450343
260.129432	11134.335377	27.455360
260.670376	11127.620654	27.460378
260.188113	11135.638056	27.465396
260.494073	11142.261197	27.470413
260.734493	11157.794788	27.475431
260.605966	11160.533702	27.480448
260.745927	11178.046552	27.485466
260.957174	11203.062779	27.490484
260.861990	11218.798937	27.495501
261.259630	11244.585425	27.500519
261.191136	11276.678353	27.505536
261.257698	11296.608781	27.510554
261.350900	11332.013503	27.515572
261.898449	11350.974301	27.520589
262.309498	11379.647398	27.525607
262.653643	11404.576541	27.530624
263.427186	11419.353954	27.535642
264.890074	11406.594940	27.540660
265.942972	11391.228685	27.545677
266.127377	11386.207645	27.550695
266.329314	11374.143876	27.555712
266.822135	11352.374481	27.560730
266.827130	11354.554722	27.565748
267.007233	11341.334829	27.570765
267.006538	11323.498502	27.575783
267.153046	11305.819772	27.580800
267.475429	11293.979686	27.585818
267.203424	11301.627031	27.590836
267.178676	11296.714362	27.595853
267.223132	11310.945298	27.600871
267.021138	11333.473242	27.605888
267.438897	11347.038216	27.610906
267.529307	11365.399736	27.615924
267.779825	11370.607825	27.620941
268.129127	11395.421029	27.625959
268.447651	11407.509070	27.630976
268.961639	11417.675635	27.635994
268.715866	11434.854588	27.641012
268.955715	11451.271088	27.646029
269.402059	11472.731495	27.651047
269.450591	11492.307513	27.656064
269.833912	11515.981960	27.661082
269.892217	11538.029030	27.666100
270.034858	11562.373604	27.671117
270.335438	11586.295577	27.676135
270.731569	11610.724427	27.681152
271.211181	11628.666516	27.686170
271.624678	11657.506737	27.691188
271.859866	11676.351252	27.696205
272.309435	11695.658627	27.701223
272.197113	11702.791813	27.706240
272.654909	11726.436465	27.711258
273.010852	11742.962589	27.716276
273.189298	11759.462419	27.721293
273.276448	11778.449049	27.726311
274.249348	11795.249289	27.731328
274.621629	11805.106279	27.736346
274.620669	11826.230915	27.741364
274.895182	11831.580030	27.746381
275.502767	11855.487600	27.751399
275.454336	11868.537194	27.756416
275.893120	11874.278956	27.761434
276.095633	11888.880454	27.766452
276.506254	11891.374207	27.771469
276.769947	11902.081991	27.776487
276.726772	11915.486895	27.781504
277.542086	11914.913749	27.786522
277.565918	11931.117176	27.791540
278.266327	11936.161655	27.796557
278.261863	11936.354691	27.801575
278.297047	11954.237780	27.806592
279.054390	11970.468392	27.811610
278.970823	11974.348637	27.816628
279.298540	11965.660726	27.821645
279.404261	11979.714689	27.826663
279.427361	11996.706305	27.831680
280.070174	12000.225653	27.836698
279.896327	12026.007318	27.841716
279.751804	12033.600056	27.846733
279.995888	12055.625437	27.851751
279.831708	12079.720779	27.856768
280.433872	12099.229423	27.861786
280.871625	12130.395666	27.866804
281.037804	12147.414923	27.871821
281.365978	12165.880006	27.876839
281.387327	12198.487310	27.881856
281.983904	12214.788274	27.886874
282.214476	12241.129791	27.891892
282.671722	12269.330034	27.896909
283.010268	12278.327856	27.901927
283.726558	12290.707710	27.906944
284.162173	12306.245189	27.911962
284.210052	12327.937352	27.916980
285.015907	12314.869465	27.921997
285.366944	12333.430110	27.927015
285.561171	12344.121723	27.932032
286.163875	12350.042019	27.937050
285.571948	12355.774646	27.942068
286.113992	12367.357007	27.947085
286.475678	12379.867055	27.952103
286.458217	12409.033062	27.957120
286.952770	12414.808011	27.962138
286.701514	12431.295489	27.967156
287.524522	12449.381359	27.972173
287.784925	12462.539248	27.977191
287.709997	12476.526886	27.982208
288.309081	12481.064083	27.987226
288.579398	12507.046182	27.992244
289.024114	12522.254489	27.997261
289.435779	12532.496031	28.002279
289.837452	12546.997788	28.007296
289.937854	12556.800967	28.012314
290.205134	12568.666975	28.017332
290.332858	12584.118799	28.022349
290.819857	12584.394667	28.027367
291.362674	12596.752480	28.032384
291.915170	12598.927305	28.037402
292.055373	12607.954577	28.042420
292.377118	12604.671661	28.047437
292.972465	12600.653112	28.052455
292.691767	12607.169367	28.057472
293.402712	12616.349413	28.062490
293.464214	12629.888262	28.067508
293.469975	12635.870002	28.072525
293.954525	12649.312716	28.077543
294.212590	12651.946214	28.082560
294.628953	12646.128523	28.087578
295.101318	12654.673352	28.092596
295.278329	12654.182801	28.097613
295.625110	12661.781456	28.102631
295.627658	12674.392689	28.107648
295.902081	12676.890998	28.112666
296.031279	12687.715339	28.117684
296.035405	12695.855017	28.122701
296.266929	12712.784860	28.127719
295.902558	12726.053199	28.132736
296.626687	12748.722229	28.137754
296.701500	12768.337823	28.142772
296.880175	12796.853081	28.147789
297.241113	12817.092678	28.152807
297.369370	12849.188064	28.157824
297.645207	12882.032076	28.162842
297.996393	12891.447309	28.167860
298.252499	12917.382061	28.172877
298.598193	12935.600719	28.177895
298.653810	12975.820942	28.182912
299.244316	12994.054444	28.187930
299.390619	13022.654448	28.192948
299.566665	13056.597116	28.197965
299.964869	13075.111116	28.202983
299.549022	13108.431909	28.208000
300.378901	13145.648174	28.213018
301.020113	13178.119659	28.218036
301.206099	13192.684175	28.223053
302.144845	13219.071379	28.228071
302.104982	13246.334033	28.233088
302.742357	13261.904039	28.238106
303.939054	13262.821126	28.243124
304.493821	13270.419092	28.248141
305.020262	13260.605764	28.253159
305.114054	13268.117245	28.258176
305.461147	13284.556610	28.263194
305.899353	13286.973354	28.268212
305.986175	13293.042312	28.273229
306.134870	13290.501330	28.278247
305.978256	13292.696920	28.283264
306.525693	13306.610115	28.288282
306.900961	13315.892225	28.293300
306.948090	13333.614007	28.298317
306.694238	13337.507997	28.303335
306.951845	13367.110855	28.308352
307.351378	13380.918645	28.313370
307.815544	13400.022215	28.318388
307.557812	13421.314277	28.323405
308.030407	13442.530051	28.328423
308.263417	13468.436533	28.333440
308.305935	13483.382105	28.338458
308.337394	13517.804437	28.343476
308.543273	13551.211852	28.348493
309.360879	13576.846508	28.353511
309.113952	13617.772681	28.358528
309.864995	13633.838962	28.363546
310.184543	13660.022503	28.368564
310.970454	13681.838992	28.373581
312.283471	13673.681126	28.378599
312.791002	13666.950619	28.383616
313.608742	13663.765319	28.388634
313.983573	13650.209149	28.393652
314.658957	13647.948238	28.398669
314.740358	13631.510720	28.403687
314.576738	13615.982099	28.408704
314.950712	13613.167610	28.413722
315.361461	13606.170007	28.418740
315.286367	13609.188604	28.423757
315.322506	13602.114931	28.428775
315.556484	13619.689938	28.433792
315.615568	13641.225876	28.438810
315.937732	13644.097584	28.443828
315.739428	13656.632087	28.448845
316.173049	13671.316931	28.453863
316.028570	13695.442787	28.458880
316.481470	13709.564822	28.463898
316.970459	13737.989124	28.468916
316.809592	13758.615638	28.473933
317.512100	13770.169921	28.478951
317.589100	13808.095187	28.483968
317.213250	13835.487331	28.488986
317.903211	13859.653246	28.494004
318.049362	13892.992784	28.499021
318.779252	13921.163329	28.504039
318.850173	13946.053335	28.509056
319.393143	13964.879257	28.514074
319.792781	13977.612573	28.519092
320.226633	14010.368710	28.524109
320.873480	14036.980646	28.529127
321.005807	14055.418381	28.534144
321.150661	14082.885614	28.539162
321.935141	14096.224524	28.544180
321.639754	14123.165169	28.549197
322.140507	14140.029849	28.554215
321.954680	14163.898673	28.559232
322.634210	14183.092340	28.564250
323.096816	14203.984536	28.569268
323.488696	14233.447723	28.574285
324.155752	14247.063804	28.579303
324.426947	14277.890691	28.584320
324.934628	14296.434595	28.589338
325.363264	14303.665336	28.594356
325.737707	14340.190024	28.599373
325.874749	14346.208205	28.604391
326.034539	14367.377909	28.609408
326.162753	14377.809476	28.614426
326.238936	14396.012898	28.619444
326.482741	14425.612144	28.624461
327.131046	14442.048330	28.629479
327.399191	14473.181894	28.634496
327.374207	14496.460913	28.639514
328.170425	14497.823451	28.644532
328.478602	14524.963941	28.649549
328.624654	14535.901677	28.654567
329.116280	14561.825452	28.659584
329.131885	14571.143121	28.664602
330.206837	14576.420579	28.669620
330.160987	14594.342496	28.674637
330.962932	14612.015095	28.679655
331.554674	14624.388127	28.684672
331.849929	14617.018987	28.689690
332.378231	14629.642486	28.694708
332.976465	14643.710468	28.699725
333.241904	14632.382153	28.704743
333.871840	14638.115780	28.709760
333.725780	14637.726258	28.714778
334.121212	14629.515562	28.719796
334.313846	14646.069457	28.724813
334.385902	14660.609089	28.729831
334.742338	14666.507821	28.734848
334.652469	14677.016361	28.739866
335.234437	14674.925804	28.744884
335.334202	14701.263737	28.749901
335.802448	14705.179301	28.754919
337.373118	14700.041038	28.759936
337.863021	14683.477292	28.764954
338.021458	14676.780992	28.769972
338.392838	14685.659448	28.774989
338.861935	14680.136232	28.780007
339.050915	14675.023565	28.785024
338.850662	14671.585392	28.790042
339.476413	14692.814365	28.795060
339.206155	14707.087998	28.800077
339.633353	14711.428308	28.805095
339.677720	14713.023760	28.810112
339.717121	14735.907475	28.815130
340.102168	14744.411622	28.820148
339.980582	14778.962121	28.825165
340.296847	14798.363786	28.830183
340.210699	14818.595782	28.835200
340.145382	14848.562445	28.840218
340.784644	14873.979071	28.845236
340.945277	14916.142187	28.850253
340.884974	14948.756322	28.855271
341.148492	14988.055221	28.860288
341.524116	15035.653086	28.865306
342.357992	15073.697438	28.870324
342.452931	15122.079786	28.875341
342.961082	15147.678510	28.880359
343.300298	15185.938732	28.885376
343.748260	15222.224205	28.890394
344.390242	15239.538702	28.895412
345.009720	15282.150596	28.900429
345.608711	15297.700745	28.905447
346.191718	15320.826278	28.910464
346.288763	15335.929695	28.915482
347.169382	15358.892356	28.920500
347.124357	15370.596383	28.925517
347.265619	15383.214285	28.930535
347.791187	15401.015496	28.935552
347.960373	15413.262927	28.940570
348.206605	15425.788784	28.945588
348.842215	15454.225597	28.950605
348.955007	15463.880210	28.955623
349.915980	15477.487926	28.960640
350.053852	15490.763822	28.965658
351.208437	15487.799475	28.970676
351.441902	15499.827878	28.975693
351.944035	15502.090558	28.980711
352.619753	15496.991953	28.985728
352.438012	15502.136730	28.990746
352.465056	15514.616675	28.995764
352.930166	15531.520419	29.000781
352.982668	15531.840874	29.005799
353.276162	15547.363225	29.010816
353.208949	15568.032687	29.015834
353.914666	15587.601830	29.020852
353.915397	15605.852618	29.025869
354.016202	15634.155982	29.030887
354.779734	15647.452459	29.035904
354.554528	15665.945385	29.040922
354.826267	15696.185268	29.045940
355.191375	15734.473847	29.050957
355.250369	15757.614136	29.055975
355.721303	15787.957191	29.060992
355.538671	15829.825201	29.066010
356.404508	15861.971857	29.071028
357.074183	15904.956656	29.076045
357.508799	15929.342774	29.081063
357.963204	15956.886174	29.086080
357.843544	15982.899605	29.091098
358.245097	16020.405441	29.096116
358.504138	16045.564297	29.101133
359.233122	16070.097220	29.106151
359.893020	16096.056042	29.111168
360.080108	16132.426051	29.116186
360.480982	16153.200454	29.121204
360.935611	16188.101246	29.126221
361.538494	16213.530895	29.131239
361.852086	16231.284204	29.136256
362.338889	16248.977894	29.141274
362.351292	16274.999098	29.146292
363.000364	16300.570723	29.151309
363.382403	16320.438975	29.156327
363.641973	16344.327604	29.161344
363.757221	16379.573870	29.166362
364.170754	16392.547863	29.171380
364.394575	16417.454785	29.176397
364.517372	16450.388872	29.181415
365.004615	16467.750094	29.186432
365.633122	16502.885010	29.191450
366.070846	16513.312170	29.196468
366.297725	16537.752125	29.201485
366.822563	16556.111185	29.206503
367.217201	16583.798288	29.211520
367.721761	16613.673615	29.216538
367.969601	16632.293051	29.221556
368.197105	16654.029471	29.226573
368.478423	16680.039901	29.231591
368.974446	16687.635340	29.236608
369.159054	16729.862005	29.241626
369.471954	16745.325397	29.246644
369.804761	16774.011849	29.251661
369.747211	16797.800984	29.256679
370.228526	16821.925022	29.261696
370.638135	16865.683623	29.266714
371.011556	16898.476324	29.271732
371.204123	16923.524935	29.276749
371.743669	16961.088063	29.281767
371.978470	16985.224632	29.286784
372.386520	17026.709067	29.291802
373.127806	17049.185601	29.296820
373.600820	17078.698271	29.301837
373.434077	17107.994304	29.306855
373.885252	17133.293711	29.311872
373.771355	17183.061004	29.316890
374.580733	17206.921278	29.321908
375.242386	17246.805219	29.326925
375.780597	17274.724257	29.331943
376.640929	17288.798449	29.336960
377.051401	17323.110113	29.341978
377.717087	17335.765741	29.346996
378.162813	17346.445872	29.352013
378.883619	17362.048029	29.357031
379.341321	17365.794203	29.362048
379.569932	17389.880393	29.367066
380.178508	17405.027294	29.372084
380.389075	17412.906890	29.377101
380.145197	17430.340816	29.382119
380.597474	17445.993802	29.387136
381.029896	17466.917361	29.392154
381.422156	17482.730436	29.397172
381.412581	17509.555049	29.402189
381.524479	17539.171412	29.407207
382.301017	17551.366779	29.412224
381.993503	17595.409420	29.417242
382.776324	17611.377975	29.422260
383.064703	17648.662506	29.427277
383.027071	17680.053124	29.432295
383.450780	17711.785674	29.437312
383.684125	17758.808736	29.442330
384.100466	17794.342187	29.447348
384.630000	17833.050414	29.452365
384.968413	17871.864008	29.457383
385.671783	17891.833566	29.462400
386.169038	17919.737052	29.467418
386.124095	17946.674054	29.472436
387.027877	17966.084359	29.477453
387.652109	17997.899752	29.482471
388.415204	18001.045087	29.487488
388.890548	18013.965608	29.492506
389.431272	18019.091394	29.497524
390.150585	18021.178474	29.502541
390.205482	18045.587044	29.507559
390.547302	18043.070582	29.512576
390.624169	18059.649291	29.517594
390.825471	18086.709858	29.522612
391.316270	18098.319236	29.527629
392.137510	18105.777611	29.532647
392.634256	18104.380764	29.537664
393.408937	18120.746926	29.542682
393.497315	18121.007681	29.547700
394.133373	18121.171423	29.552717
393.665586	18134.384525	29.557735
394.568418	18149.530550	29.562752
394.799194	18176.294543	29.567770
395.214244	18181.965345	29.572788
395.928345	18188.942341	29.577805
396.162952	18210.225510	29.582823
396.452379	18220.020143	29.587840
396.597150	18236.034006	29.592858
396.709131	18257.056039	29.597876
397.152396	18277.146313	29.602893
397.072170	18311.745905	29.607911
397.542846	18320.727542	29.612928
397.790983	18359.781615	29.617946
397.942529	18394.835134	29.622964
398.718491	18422.428403	29.627981
398.905379	18448.927598	29.632999
399.153208	18474.842503	29.638016
399.486409	18513.433019	29.643034
400.091295	18543.247306	29.648052
400.111582	18583.592784	29.653069
400.068718	18624.349645	29.658087
400.382625	18659.513057	29.663104
400.981194	18709.151737	29.668122
401.189366	18765.214489	29.673140
401.601453	18808.383346	29.678157
401.961941	18851.594266	29.683175
402.641336	18895.669834	29.688192
402.852145	18941.976384	29.693210
403.289844	18979.012816	29.698228
403.809822	19023.969014	29.703245
404.324821	19065.903708	29.708263
404.945013	19108.742833	29.713280
405.431855	19155.715322	29.718298
405.801598	19193.244758	29.723316
406.498427	19212.851226	29.728333
407.129738	19263.197011	29.733351
406.954038	19285.523097	29.738368
407.968121	19313.004494	29.743386
408.565540	19340.409133	29.748404
408.940679	19360.485574	29.753421
409.604612	19391.204154	29.758439
409.821443	19405.502366	29.763456
410.375138	19433.352973	29.768474
410.550888	19453.690741	29.773492
410.879786	19475.459167	29.778509
411.081973	19509.706933	29.783527
411.752344	19528.600901	29.788544
412.123442	19557.052198	29.793562
412.515520	19586.545313	29.798580
412.847194	19605.555749	29.803597
412.770954	19642.915070	29.808615
413.132028	19667.661392	29.813632
413.234877	19709.745578	29.818650
413.792561	19751.747192	29.823668
414.555284	19779.337076	29.828685
414.746194	19822.992650	29.833703
415.238077	19859.969698	29.838720
415.656403	19893.582039	29.843738
416.334316	19929.422059	29.848756
416.720742	19955.965109	29.853773
416.969194	19998.113357	29.858791
417.309797	20026.668431	29.863808
417.889517	20067.651620	29.868826
418.120456	20104.629772	29.873844
418.750689	20140.664470	29.878861
419.438708	20176.426020	29.883879
420.153843	20202.173619	29.888896
420.587421	20229.191511	29.893914
420.955896	20260.047453	29.898932
421.727672	20275.731899	29.903949
421.838709	20306.222079	29.908967
422.748085	20328.661599	29.913984
423.103393	20351.129875	29.919002
423.286388	20380.209244	29.924020
423.683151	20402.806088	29.929037
423.865296	20430.291548	29.934055
425.278631	20428.087807	29.939072
426.834742	20429.134608	29.944090
426.816047	20440.634247	29.949108
427.438312	20436.263945	29.954125
427.269058	20441.427005	29.959143
427.437726	20441.935788	29.964160
427.896924	20462.033825	29.969178
428.110008	20476.762476	29.974196
428.324348	20502.719346	29.979213
428.568218	20522.371854	29.984231
428.590714	20542.246807	29.989248
428.772851	20582.564585	29.994266
428.589199	20610.981849	29.999284
429.413843	20649.114592	30.004301
429.646276	20694.584944	30.009319
429.480790	20730.389861	30.014336
429.874323	20775.999966	30.019354
430.513222	20819.152436	30.024372
430.928212	20846.188691	30.029389
431.640307	20887.507545	30.034407
432.116990	20927.255308	30.039424
432.457771	20957.030820	30.044442
433.152819	20994.081179	30.049460
433.460398	21030.283443	30.054477
433.860518	21077.138942	30.059495
434.289622	21099.940897	30.064512
435.069581	21129.266157	30.069530
435.277595	21157.776476	30.074548
436.146284	21179.834617	30.079565
437.158988	21216.723799	30.084583
437.385978	21234.905650	30.089600
438.114776	21257.046209	30.094618
438.328486	21277.412775	30.099636
439.105895	21296.216269	30.104653
439.218366	21314.143453	30.109671
439.588905	21340.655128	30.114688
440.345385	21359.626275	30.119706
440.283050	21391.121049	30.124724
441.009100	21408.955801	30.129741
441.401805	21440.648643	30.134759
441.674858	21455.673785	30.139776
442.254304	21475.582114	30.144794
442.237570	21505.090281	30.149812
442.751589	21532.361385	30.154829
442.890624	21572.505976	30.159847
443.499946	21607.375738	30.164864
444.233244	21637.794787	30.169882
444.440935	21673.700156	30.174900
444.840560	21710.777474	30.179917
444.994333	21763.511670	30.184935
445.280863	21787.917479	30.189952
445.653286	21828.413754	30.194970
445.729927	21874.849072	30.199988
446.466125	21909.377593	30.205005
447.203292	21945.807806	30.210023
447.374174	21996.168073	30.215040
447.965060	22041.858136	30.220058
447.936494	22088.654262	30.225076
448.413014	22126.000002	30.230093
448.986705	22170.201556	30.235111
449.462680	22215.265222	30.240128
449.964039	22246.535664	30.245146
450.968395	22312.060069	30.250164
451.438235	22333.432691	30.255181
451.958933	22376.256124	30.260199
452.691645	22415.309040	30.265216
453.404708	22427.275988	30.270234
455.039875	22431.310403	30.275252
456.553715	22422.661439	30.280269
457.188925	22421.748325	30.285287
457.765859	22414.471039	30.290304
458.238121	22399.847194	30.295322
458.434358	22386.822410	30.300340
458.541657	22378.168488	30.305357
458.631404	22386.337625	30.310375
458.619648	22387.159667	30.315392
459.211845	22385.916453	30.320410
459.323918	22380.601753	30.325428
459.526424	22391.236888	30.330445
459.344247	22404.719743	30.335463
459.894370	22423.981339	30.340480
460.209904	22443.724713	30.345498
460.227216	22482.676448	30.350516
460.733823	22506.686020	30.355533
460.840697	22537.601964	30.360551
461.281504	22572.251838	30.365568
461.271133	22608.297468	30.370586
461.628090	22653.382687	30.375604
462.500842	22695.121541	30.380621
462.617752	22735.340466	30.385639
462.730187	22782.820828	30.390656
463.021894	22830.986568	30.395674
463.113667	22897.439189	30.400692
463.545625	22946.467507	30.405709
463.876959	23006.356902	30.410727
464.148774	23078.257993	30.415744
464.822525	23132.563195	30.420762
465.465530	23202.221718	30.425780
465.910029	23261.893903	30.430797
466.431514	23315.768430	30.435815
466.997285	23375.271984	30.440832
468.002394	23433.407256	30.445850
468.106972	23495.683900	30.450868
468.685518	23534.718478	30.455885
469.396326	23585.287383	30.460903
469.997432	23638.524751	30.465920
470.575810	23689.678101	30.470938
471.110075	23740.712994	30.475956
471.984231	23775.117557	30.480973
472.145902	23829.547409	30.485991
472.426488	23863.514491	30.491008
473.412849	23903.492531	30.496026
473.844889	23958.687100	30.501044
474.834149	24000.052737	30.506061
475.634286	24013.195036	30.511079
476.355817	24034.268005	30.516096
477.443257	24061.463810	30.521114
477.795203	24089.848681	30.526132
478.232899	24099.006226	30.531149
478.691506	24123.259706	30.536167
478.867625	24145.397790	30.541184
479.021845	24172.040818	30.546202
479.051971	24212.410546	30.551220
479.082466	24244.692683	30.556237
480.062530	24283.057687	30.561255
479.945446	24324.919655	30.566272
480.504721	24369.507867	30.571290
480.292185	24413.897246	30.576308
480.792819	24454.101746	30.581325
481.604531	24484.673295	30.586343
482.541404	24531.471503	30.591360
483.215121	24568.003335	30.596378
483.368903	24608.614611	30.601396
483.684972	24648.444277	30.606413
484.320258	24683.137632	30.611431
484.341715	24737.446117	30.616448
484.835906	24765.643697	30.621466
485.412490	24812.709441	30.626484
485.865169	24853.345778	30.631501
486.585688	24898.929757	30.636519
486.958404	24944.737483	30.641536
487.765452	24986.108325	30.646554
487.897890	25033.913209	30.651572
488.421852	25070.689424	30.656589
489.102872	25116.861164	30.661607
489.364901	25167.454832	30.666624
490.169048	25204.908848	30.671642
491.042615	25246.928200	30.676660
492.171196	25257.273933	30.681677
492.941272	25288.213655	30.686695
493.455035	25315.635930	30.691712
493.939663	25329.527295	30.696730
494.676481	25353.993501	30.701748
495.197478	25373.506299	30.706765
496.207875	25387.847039	30.711783
496.544376	25405.410457	30.716800
496.929857	25423.422905	30.721818
497.011953	25442.736546	30.726836
497.358699	25451.348896	30.731853
498.403424	25453.510529	30.736871
498.907919	25468.083133	30.741888
499.237322	25486.155728	30.746906
499.837224	25504.216691	30.751924
499.588077	25530.186462	30.756941
500.576828	25550.445797	30.761959
500.525662	25583.580375	30.766976
500.840136	25608.895331	30.771994
501.125586	25635.249991	30.777012
501.607770	25676.110334	30.782029
502.156087	25713.382163	30.787047
501.951692	25764.467592	30.792064
502.519465	25800.300943	30.797082
503.218906	25853.900535	30.802100
503.040542	25906.720099	30.807117
503.786708	25948.327653	30.812135
504.008756	26006.665721	30.817152
504.338921	26062.051652	30.822170
504.649867	26111.791097	30.827188
505.743957	26170.049687	30.832205
506.247484	26219.128664	30.837223
506.299711	26277.458882	30.842240
507.055113	26313.907849	30.847258
507.225859	26368.751077	30.852276
507.353655	26429.867059	30.857293
508.257453	26481.177961	30.862311
508.788904	26529.300307	30.867328
509.227403	26583.189771	30.872346
509.632246	26641.290428	30.877364
509.818886	26696.248687	30.882381
510.443084	26762.158007	30.887399
511.058895	26823.633412	30.892416
511.396780	26875.518815	30.897434
512.631211	26930.790417	30.902452
512.916457	26982.161462	30.907469
513.673495	27037.489965	30.912487
514.453376	27087.536726	30.917504
515.438937	27129.752822	30.922522
516.043048	27176.457453	30.927540
517.135601	27208.320188	30.932557
517.670858	27234.536663	30.937575
518.184326	27274.701332	30.942592
519.173105	27300.537331	30.947610
519.154273	27338.032860	30.952628
519.104336	27367.056677	30.957645
519.533901	27404.402953	30.962663
519.998041	27452.176568	30.967680
520.549352	27488.694514	30.972698
520.589659	27547.150896	30.977716
521.037330	27599.051183	30.982733
521.944881	27634.858483	30.987751
522.157858	27693.844186	30.992768
522.496733	27747.151721	30.997786
523.442550	27794.856355	31.002804
523.525944	27852.126422	31.007821
524.099927	27902.384320	31.012839
524.801632	27964.233923	31.017856
525.445512	28005.860760	31.022874
526.099881	28062.364822	31.027892
526.649357	28114.034651	31.032909
527.458426	28150.718042	31.037927
527.878978	28197.589361	31.042944
528.199617	28244.253918	31.047962
528.911182	28297.281568	31.052980
529.738226	28340.720355	31.057997
530.535859	28386.902870	31.063015
530.739276	28419.049526	31.068032
531.185572	28462.181558	31.073050
532.015862	28509.052912	31.078068
532.235538	28556.789393	31.083085
532.849409	28595.053149	31.088103
533.063611	28649.321844	31.093120
533.520944	28693.850260	31.098138
533.805812	28750.662791	31.103156
534.678353	28800.521886	31.108173
535.293154	28846.525545	31.113191
535.710406	28903.555676	31.118208
536.255319	28948.729154	31.123226
536.857510	28982.919305	31.128244
537.111176	29029.966575	31.133261
537.821080	29074.193953	31.138279
537.998634	29114.612857	31.143296
538.582263	29166.519721	31.148314
539.118133	29219.479290	31.153332
539.477488	29272.421935	31.158349
540.255392	29321.326918	31.163367
540.219237	29380.584982	31.168384
540.656114	29425.528930	31.173402
541.674381	29489.585648	31.178420
542.131397	29548.895449	31.183437
542.982230	29595.977581	31.188455
543.034672	29660.260357	31.193472
543.276964	29708.532474	31.198490
543.725592	29763.890863	31.203508
544.084803	29824.120759	31.208525
545.225195	29889.076194	31.213543
545.669488	29948.768153	31.218560
546.404956	30006.084940	31.223578
547.681647	30058.307953	31.228596
547.859218	30107.854387	31.233613
548.837354	30157.942190	31.238631
549.268873	30204.630798	31.243648
549.854080	30262.545284	31.248666
550.355818	30314.229741	31.253684
550.822227	30357.583836	31.258701
551.424844	30398.264158	31.263719
552.103915	30452.922582	31.268736
552.652362	30507.411074	31.273754
553.575693	30553.874340	31.278772
553.689502	30606.765230	31.283789
554.774892	30644.252131	31.288807
555.301548	30679.042267	31.293824
555.789317	30724.031281	31.298842
556.293596	30776.704310	31.303860
556.702342	30823.310096	31.308877
557.226033	30867.248852	31.313895
557.346100	30919.637878	31.318912
557.950476	30970.189612	31.323930
558.416636	31018.603645	31.328948
559.000322	31091.535048	31.333965
559.564328	31139.475092	31.338983
559.763346	31192.290011	31.344000
560.121707	31266.046468	31.349018
560.782478	31327.012371	31.354036
561.128043	31390.670557	31.359053
561.891270	31453.638911	31.364071
562.375723	31523.237845	31.369088
563.035980	31590.768398	31.374106
563.717016	31646.373685	31.379124
564.374363	31711.109308	31.384141
565.179887	31749.444875	31.389159
565.987411	31803.347020	31.394176
567.149350	31848.071891	31.399194
568.548020	31871.761650	31.404212
568.935281	31896.874381	31.409229
569.961026	31926.791137	31.414247
570.202296	31948.227346	31.419264
570.512740	31978.658053	31.424282
571.022064	32000.436545	31.429300
571.582145	32043.488377	31.434317
572.237004	32065.317750	31.439335
572.589723	32104.151373	31.444352
572.463227	32141.684985	31.449370
573.336864	32178.340434	31.454388
573.607174	32218.457025	31.459405
574.114580	32270.165125	31.464423
574.351282	32322.494103	31.469440
574.700232	32363.758860	31.474458
575.653622	32414.239114	31.479476
575.356023	32479.879591	31.484493
575.996038	32541.295008	31.489511
576.719529	32592.045526	31.494528
576.936747	32664.285598	31.499546
577.855657	32728.317372	31.504564
578.104779	32798.785261	31.509581
579.163405	32841.084558	31.514599
579.832160	32905.623735	31.519616
580.437256	32962.107674	31.524634
580.826665	33020.396033	31.529652
581.257722	33089.079226	31.534669
581.582402	33156.559577	31.539687
581.691309	33232.143645	31.544704
582.153531	33301.377748	31.549722
582.969309	33366.388869	31.554740
583.607476	33451.249977	31.559757
584.573163	33520.928863	31.564775
585.774587	33581.850845	31.569792
585.960240	33643.029127	31.574810
586.731419	33700.784039	31.579828
587.373541	33769.095974	31.584845
587.885557	33826.150876	31.589863
588.679817	33891.669389	31.594880
589.300733	33961.746747	31.599898
589.910471	34015.421174	31.604916
590.438515	34080.985987	31.609933
591.322158	34143.106809	31.614951
591.939811	34195.862002	31.619968
592.749788	34265.810311	31.624986
593.159054	34316.423860	31.630004
593.209799	34379.234203	31.635021
593.529739	34451.533276	31.640039
594.095992	34515.893796	31.645056
594.314550	34598.329382	31.650074
594.835071	34667.060067	31.655092
595.010503	34752.719868	31.660109
595.540703	34828.591926	31.665127
596.208135	34910.472285	31.670144
596.405406	34997.193138	31.675162
597.311798	35063.211150	31.680180
597.965300	35157.072890	31.685197
599.199081	35214.330448	31.690215
600.225484	35278.810528	31.695232
601.352449	35343.472454	31.700250
602.071698	35393.773933	31.705268
602.318324	35452.618547	31.710285
603.123637	35502.302730	31.715303
603.711221	35565.097796	31.720320
604.015775	35622.989299	31.725338
604.595816	35679.583880	31.730356
604.924354	35751.880349	31.735373
605.335388	35816.698186	31.740391
605.838418	35886.575932	31.745408
606.553748	35962.806089	31.750426
607.289602	36024.295846	31.755444
607.860048	36089.033682	31.760461
609.463729	36132.412037	31.765479
610.347660	36196.260098	31.770496
610.388635	36245.591178	31.775514
611.264396	36298.819612	31.780532
611.518087	36364.300800	31.785549
612.376613	36420.966763	31.790567
612.919050	36484.640763	31.795584
613.245334	36552.524891	31.800602
614.362944	36602.000750	31.805620
614.463124	36674.179020	31.810637
615.017876	36730.108862	31.815655
615.482462	36798.642546	31.820672
615.643955	36873.481518	31.825690
616.935653	36942.113930	31.830708
617.503837	37008.809323	31.835725
617.976979	37080.745372	31.840743
618.494105	37136.304115	31.845760
619.070901	37216.575264	31.850778
619.983132	37286.448237	31.855796
620.103391	37346.330723	31.860813
621.302460	37415.713120	31.865831
622.146829	37475.310979	31.870848
622.740802	37535.990470	31.875866
623.974384	37585.098739	31.880884
625.156427	37629.174769	31.885901
626.251150	37676.813971	31.890919
627.112163	37718.126304	31.895936
627.565558	37766.873129	31.900954
627.928072	37798.270648	31.905972
628.211125	37846.245066	31.910989
628.648601	37900.437136	31.916007
629.216338	37944.464493	31.921024
629.756130	38016.004518	31.926042
630.036140	38054.484543	31.931060
630.501642	38113.442277	31.936077
630.635632	38174.982407	31.941095
631.275959	38243.324074	31.946112
631.847842	38305.856609	31.951130
632.695474	38362.918739	31.956148
633.104828	38426.868521	31.961165
633.557429	38494.002657	31.966183
633.774192	38546.065708	31.971200
634.782743	38622.455586	31.976218
635.758364	38677.154389	31.981236
636.360643	38730.859770	31.986253
637.225129	38794.331931	31.991271
637.367291	38852.400366	31.996288
638.207863	38917.076660	32.001306
638.843213	38973.283652	32.006324
639.631454	39038.449186	32.011341
640.275921	39089.670210	32.016359
641.432028	39145.400208	32.021376
641.827135	39204.433474	32.026394
642.321348	39263.639367	32.031412
643.457642	39320.948608	32.036429
644.046522	39380.006063	32.041447
644.384723	39439.640183	32.046464
644.659367	39505.694073	32.051482
645.215661	39572.037744	32.056500
645.584713	39642.580989	32.061517
645.924490	39713.382080	32.066535
646.620288	39780.517110	32.071552
646.952408	39870.461237	32.076570
647.540227	39946.862377	32.081588
648.261932	40024.386914	32.086605
648.777882	40116.438081	32.091623
649.325466	40200.572569	32.096640
649.712377	40289.293849	32.101658
650.354590	40382.720151	32.106676
651.116819	40474.156297	32.111693
651.548864	40563.297368	32.116711
652.345821	40652.799411	32.121728
652.773535	40742.974483	32.126746
653.882290	40830.977968	32.131764
654.708886	40915.923495	32.136781
655.528311	41006.367401	32.141799
656.341807	41092.651492	32.146816
656.728685	41183.697624	32.151834
657.401932	41261.740781	32.156852
658.228825	41348.989893	32.161869
658.816141	41437.044528	32.166887
659.526907	41512.461732	32.171904
660.200464	41607.855820	32.176922
661.323988	41678.132283	32.181940
662.350565	41756.186437	32.186957
663.038994	41838.286625	32.191975
663.784216	41903.223302	32.196992
664.463290	41987.400156	32.202010
664.787779	42050.401310	32.207028
665.334663	42126.783664	32.212045
665.793686	42209.433126	32.217063
666.581960	42280.849136	32.222080
667.085336	42368.313141	32.227098
667.585735	42451.951187	32.232116
668.504993	42517.775850	32.237133
669.067442	42595.695149	32.242151
669.754820	42679.835796	32.247168
670.214970	42752.699126	32.252186
670.780848	42823.106996	32.257204
671.505005	42897.163417	32.262221
672.213980	42983.240466	32.267239
673.456700	43046.823370	32.272256
673.529231	43124.967724	32.277274
673.897143	43213.065124	32.282292
674.963725	43283.477351	32.287309
675.225532	43384.388440	32.292327
675.651185	43460.307543	32.297344
676.532653	43551.785652	32.302362
677.794638	43629.614649	32.307380
678.316977	43704.444558	32.312397
679.006872	43799.831185	32.317415
680.120318	43877.639286	32.322432
680.664875	43957.070356	32.327450
681.121404	44041.727133	32.332468
682.124126	44116.744788	32.337485
682.833558	44191.377211	32.342503
683.697803	44273.325274	32.347520
685.111578	44323.996237	32.352538
686.578363	44380.099163	32.357556
687.030489	44438.491819	32.362573
687.463370	44506.156186	32.367591
688.287294	44559.170890	32.372608
688.694238	44626.199087	32.377626
689.548486	44692.064587	32.382644
690.317320	44756.062856	32.387661
690.290000	44820.384047	32.392679
691.446350	44882.067942	32.397696
691.657435	44956.741384	32.402714
692.159714	45021.373582	32.407732
692.871472	45103.458726	32.412749
692.927868	45191.555537	32.417767
694.221951	45262.251957	32.422784
695.159709	45350.729054	32.427802
695.294905	45423.538334	32.432820
696.364005	45491.795133	32.437837
696.518219	45570.279792	32.442855
697.436763	45641.932516	32.447872
698.271579	45728.891050	32.452890
699.160935	45804.601145	32.457908
699.902663	45876.695589	32.462925
700.187376	45967.438061	32.467943
701.144287	46045.638735	32.472960
701.500671	46118.103279	32.477978
701.987081	46204.823647	32.482996
702.861863	46294.307558	32.488013
703.504191	46382.287378	32.493031
703.870424	46463.259579	32.498048
704.326290	46555.927261	32.503066
704.972804	46646.639396	32.508084
705.984086	46723.914498	32.513101
706.618990	46812.977672	32.518119
707.666385	46879.667205	32.523136
708.131585	46969.278125	32.528154
708.533422	47051.427891	32.533172
709.774401	47132.673116	32.538189
710.770273	47206.071294	32.543207
711.468070	47273.987493	32.548224
712.163874	47344.285632	32.553242
712.643603	47431.716992	32.558260
713.813168	47503.302105	32.563277
713.969239	47591.197059	32.568295
714.613839	47673.560564	32.573312
715.459507	47758.574589	32.578330
715.449957	47854.931962	32.583348
716.389005	47951.995874	32.588365
716.791604	48044.414550	32.593383
717.766563	48140.102505	32.598400
718.164770	48232.042749	32.603418
718.168973	48335.156076	32.608436
719.102176	48438.695127	32.613453
719.918610	48562.507025	32.618471
720.874578	48657.079527	32.623488
722.291698	48748.016989	32.628506
723.090358	48832.124662	32.633524
724.581525	48921.117227	32.638541
726.061576	48984.376075	32.643559
727.059891	49048.614690	32.648576
727.664439	49125.485844	32.653594
728.142622	49200.976529	32.658612
728.649511	49273.487175	32.663629
729.479457	49359.335334	32.668647
730.020251	49446.421056	32.673664
730.554989	49514.448875	32.678682
730.828207	49607.702628	32.683700
731.453860	49698.186303	32.688717
731.946958	49785.913452	32.693735
732.175121	49884.703972	32.698752
733.035489	49982.407488	32.703770
733.360598	50092.269599	32.708788
734.005228	50195.330471	32.713805
734.547767	50305.630351	32.718823
735.286011	50416.794429	32.723840
736.398477	50527.414894	32.728858
736.791869	50641.330637	32.733876
737.639018	50750.759552	32.738893
738.073940	50872.674065	32.743911
738.799452	50978.688237	32.748928
739.472735	51090.758080	32.753946
740.042343	51216.473941	32.758964
741.227249	51341.257561	32.763981
741.719791	51460.765058	32.768999
742.685525	51575.643283	32.774016
743.482799	51678.780586	32.779034
744.330123	51795.784279	32.784052
745.918426	51875.416678	32.789069
746.716109	51960.308810	32.794087
747.705060	52053.615880	32.799104
748.312078	52142.515562	32.804122
748.900259	52235.569920	32.809140
749.763090	52320.218673	32.814157
750.241030	52416.805697	32.819175
750.725655	52513.215137	32.824192
751.560282	52609.723051	32.829210
751.847451	52712.713054	32.834228
752.811476	52814.633576	32.839245
753.551809	52921.887765	32.844263
754.681542	53021.790673	32.849280
755.857323	53100.317147	32.854298
756.688405	53194.857167	32.859316
757.835923	53279.000016	32.864333
758.426592	53380.216550	32.869351
759.105917	53464.490935	32.874368
760.171208	53555.542615	32.879386
760.987826	53630.872319	32.884404
763.094194	53676.492239	32.889421
764.358346	53748.150421	32.894439
765.275000	53812.355465	32.899456
765.784203	53871.840930	32.904474
765.633489	53947.413361	32.909492
766.266520	54019.875694	32.914509
766.792034	54100.387877	32.919527
767.247742	54182.359349	32.924544
767.827353	54264.278340	32.929562
768.335221	54369.368588	32.934580
768.938015	54450.431327	32.939597
769.622885	54557.267855	32.944615
770.194087	54645.843685	32.949632
770.927193	54744.597333	32.954650
771.571636	54855.328557	32.959668
771.864585	54972.174259	32.964685
772.443428	55081.603609	32.969703
772.598376	55208.306836	32.974720
773.177657	55318.040722	32.979738
774.011089	55450.487128	32.984756
774.919747	55575.843966	32.989773
775.725173	55699.222377	32.994791
777.081624	55819.277987	32.999808
777.808959	55927.549044	33.004826
778.389746	56064.320985	33.009844
779.493027	56173.603270	33.014861
780.316299	56297.102368	33.019879
780.585009	56422.055910	33.024896
781.738346	56543.307111	33.029914
782.474959	56665.161268	33.034932
783.141336	56780.291472	33.039949
783.786515	56907.483880	33.044967
784.859513	57030.287451	33.049984
786.249198	57137.825911	33.055002
786.963630	57235.944079	33.060020
788.509376	57324.687105	33.065037
789.551049	57415.956317	33.070055
790.704996	57492.247625	33.075072
791.748091	57556.025909	33.080090
792.231667	57649.015975	33.085108
792.998824	57733.015202	33.090125
794.236620	57815.916650	33.095143
795.338746	57890.442433	33.100160
795.962859	57964.886049	33.105178
796.557535	58048.865570	33.110196
797.170645	58124.259659	33.115213
797.735312	58216.315711	33.120231
797.982499	58306.764373	33.125248
798.675452	58399.709376	33.130266
799.243373	58502.655754	33.135284
799.896424	58599.166754	33.140301
800.915649	58699.603552	33.145319
801.149609	58812.430327	33.150336
802.107400	58906.766980	33.155354
802.409393	59027.028588	33.160372
803.261304	59141.754880	33.165389
804.127045	59255.278573	33.170407
805.273744	59368.874861	33.175424
806.132035	59477.009737	33.180442
806.865825	59588.073938	33.185460
808.125020	59688.316489	33.190477
808.587643	59812.094696	33.195495
809.416966	59919.844999	33.200512
810.217705	60026.368242	33.205530
811.245940	60133.402969	33.210548
812.653017	60229.950537	33.215565
813.836116	60309.679557	33.220583
814.619069	60426.169380	33.225600
815.958181	60520.675714	33.230618
816.547503	60619.387835	33.235636
817.155645	60722.496515	33.240653
817.674607	60826.208828	33.245671
818.199469	60923.233131	33.250688
819.680355	61006.605263	33.255706
820.353355	61103.124649	33.260724
821.338215	61186.083113	33.265741
822.242174	61292.020025	33.270759
823.128538	61387.701428	33.275776
823.845917	61475.517192	33.280794
824.843559	61564.024895	33.285812
825.424477	61653.609414	33.290829
826.422217	61746.719667	33.295847
826.921931	61844.087627	33.300864
827.960136	61952.798900	33.305882
828.053787	62047.038826	33.310900
828.825601	62150.499557	33.315917
829.454819	62256.425255	33.320935
830.250744	62369.921202	33.325952
830.897118	62480.364870	33.330970
831.150221	62589.074881	33.335988
831.598058	62692.505303	33.341005
832.076235	62821.248582	33.346023
832.251604	62946.118854	33.351040
833.955664	63082.947624	33.356058
834.350886	63212.491402	33.361076
834.367757	63348.744838	33.366093
835.471918	63481.298072	33.371111
835.871272	63630.276607	33.376128
837.015797	63761.573004	33.381146
837.655463	63925.412900	33.386164
838.192498	64068.080758	33.391181
839.169011	64217.242775	33.396199
839.959527	64379.391398	33.401216
840.772601	64524.145577	33.406234
841.878400	64680.780318	33.411252
842.727331	64832.472090	33.416269
843.604938	64975.081454	33.421287
844.780919	65133.142668	33.426304
845.722632	65281.793460	33.431322
846.627772	65426.784646	33.436340
847.408860	65575.907581	33.441357
848.332387	65731.266310	33.446375
848.716478	65876.134863	33.451392
850.230808	66024.553714	33.456410
850.932318	66177.310961	33.461428
851.863307	66327.741244	33.466445
853.182344	66467.522126	33.471463
854.396265	66619.031437	33.476480
856.002563	66749.091357	33.481498
856.283297	66885.777689	33.486516
857.468695	67004.593621	33.491533
858.333500	67133.815517	33.496551
859.098071	67283.010188	33.501568
860.184646	67409.167138	33.506586
860.652548	67550.017730	33.511604
861.488882	67688.928234	33.516621
862.833238	67822.024006	33.521639
863.004233	67958.413531	33.526656
864.685132	68069.752598	33.531674
865.889622	68206.225939	33.536692
866.974279	68317.377554	33.541709
868.779052	68411.302262	33.546727
869.612620	68526.449941	33.551744
870.767873	68631.198349	33.556762
872.390080	68737.327964	33.561780
873.158254	68826.335492	33.566797
874.196702	68916.688227	33.571815
874.710759	69010.880891	33.576832
875.082555	69103.517493	33.581850
876.030108	69198.325979	33.586868
877.074715	69282.747859	33.591885
878.142070	69373.742553	33.596903
878.963453	69482.940765	33.601920
880.192332	69565.283389	33.606938
880.691097	69652.968280	33.611956
881.042495	69735.904488	33.616973
882.237512	69827.182763	33.621991
882.712934	69913.551083	33.627008
883.681338	69999.158688	33.632026
884.385999	70096.801445	33.637044
884.651467	70194.083528	33.642061
886.051702	70286.334062	33.647079
886.191114	70400.213104	33.652096
887.063655	70500.617699	33.657114
887.915618	70606.755647	33.662132
888.722115	70718.353044	33.667149
889.795922	70821.854954	33.672167
890.291318	70946.571912	33.677184
891.321040	71057.785009	33.682202
892.229043	71177.335535	33.687220
892.948528	71298.588542	33.692237
893.930838	71413.732459	33.697255
894.246521	71539.830613	33.702272
895.024685	71659.317484	33.707290
895.678785	71795.585237	33.712308
896.274998	71935.089089	33.717325
897.606992	72065.930112	33.722343
898.249636	72206.243566	33.727360
899.432724	72335.789935	33.732378
900.403707	72481.247494	33.737396
900.906911	72613.865417	33.742413
902.048183	72753.319076	33.747431
902.650680	72901.169914	33.752448
903.508540	73051.185265	33.757466
904.441239	73186.351430	33.762484
905.212063	73340.007621	33.767501
906.451750	73484.344295	33.772519
907.430814	73630.155926	33.777536
908.990087	73755.275888	33.782554
910.609742	73886.103791	33.787572
911.412468	74016.528448	33.792589
912.558915	74136.294610	33.797607
913.550438	74273.487629	33.802624
914.134757	74386.634419	33.807642
914.717473	74517.953570	33.812660
915.691842	74645.582218	33.817677
916.451904	74777.005354	33.822695
917.389173	74904.003017	33.827712
918.700225	75021.152505	33.832730
919.772410	75153.207519	33.837748
920.942929	75281.166758	33.842765
922.010290	75396.139833	33.847783
923.144496	75516.820044	33.852800
924.370379	75626.390731	33.857818
925.456401	75733.202789	33.862836
926.576904	75836.132044	33.867853
927.630163	75924.499733	33.872871
928.616105	76023.392038	33.877888
929.908352	76118.974751	33.882906
931.390936	76198.623206	33.887924
931.845970	76292.186753	33.892941
932.731786	76364.277905	33.897959
933.188932	76456.576687	33.902976
934.025398	76551.081742	33.907994
935.228847	76636.055031	33.913012
935.591194	76743.969986	33.918029
935.989080	76832.257407	33.923047
936.449010	76940.352685	33.928064
937.448875	77055.181386	33.933082
938.136639	77177.680240	33.938100
938.283338	77296.603507	33.943117
939.102856	77429.600829	33.948135
939.478896	77565.059706	33.953152
940.187876	77710.609004	33.958170
941.088062	77867.747120	33.963188
941.495817	78020.061750	33.968205
942.127534	78179.556967	33.973223
942.854439	78339.093940	33.978240
943.672373	78503.689938	33.983258
945.518106	78659.925147	33.988276
946.715107	78822.598670	33.993293
947.878846	78969.495231	33.998311
949.298293	79126.667018	34.003328
950.011260	79281.430372	34.008346
951.451715	79428.731675	34.013364
952.164049	79576.436982	34.018381
953.400372	79715.038408	34.023399
954.594543	79866.269116	34.028416
954.871045	80014.361887	34.033434
956.131910	80166.418251	34.038452
957.237885	80314.510097	34.043469
958.519284	80455.727486	34.048487
959.411150	80595.437123	34.053504
960.092781	80739.194721	34.058522
961.416191	80881.944920	34.063540
962.164429	81024.408573	34.068557
963.022502	81182.658617	34.073575
963.748723	81335.839226	34.078592
964.531142	81484.133209	34.083610
965.916573	81639.012427	34.088628
966.444150	81799.727528	34.093645
967.616130	81952.203193	34.098663
968.494009	82106.520782	34.103680
969.699459	82252.172140	34.108698
971.336037	82408.361172	34.113716
971.610050	82561.488140	34.118733
973.038598	82700.384658	34.123751
974.080258	82856.292625	34.128768
974.808021	83011.078515	34.133786
975.896739	83161.342853	34.138804
976.784750	83318.058485	34.143821
977.807366	83459.597965	34.148839
978.716828	83607.168759	34.153856
979.372865	83765.097695	34.158874
981.078982	83893.450158	34.163892
981.717187	84036.957223	34.168909
982.998509	84166.390013	34.173927
983.671751	84304.628152	34.178944
984.529285	84449.745371	34.183962
986.322820	84581.794659	34.188980
986.957399	84725.768481	34.193997
987.820290	84855.245088	34.199015
988.795198	84999.080041	34.204032
989.656016	85133.722040	34.209050
990.622214	85272.694030	34.214068
991.247350	85422.406803	34.219085
992.566826	85562.205912	34.224103
993.256828	85712.599165	34.229120
993.879649	85866.561246	34.234138
994.923919	86006.119016	34.239156
995.985628	86171.854122	34.244173
996.895815	86329.706105	34.249191
998.001156	86485.639908	34.254208
998.869950	86648.854776	34.259226
999.766959	86794.479566	34.264244
1001.009117	86966.966933	34.269261
1001.802868	87119.205533	34.274279
1002.900572	87286.764820	34.279296
1003.786848	87450.937780	34.284314
1004.993654	87610.627015	34.289332
1005.333490	87777.680340	34.294349
1006.860752	87954.309197	34.299367
1007.850669	88118.260141	34.304384
1009.138021	88283.686489	34.309402
1010.411298	88437.749968	34.314420
1011.537034	88603.554274	34.319437
1012.819359	88744.941624	34.324455
1014.053654	88900.337465	34.329472
1015.228676	89048.118132	34.334490
1016.321257	89189.034268	34.339508
1017.312798	89348.651665	34.344525
1018.260654	89500.657457	34.349543
1019.555291	89652.687100	34.354560
1020.432939	89809.833393	34.359578
1021.405214	89952.635332	34.364596
1022.325782	90099.776121	34.369613
1023.262625	90240.870618	34.374631
1024.699161	90400.975715	34.379648
1025.799362	90540.012284	34.384666
1027.256924	90671.469218	34.389684
1028.381623	90825.813862	34.394701
1029.399141	90966.886094	34.399719
1030.298984	91109.257837	34.404736
1030.844032	91254.083704	34.409754
1032.034509	91388.691681	34.414772
1032.753324	91538.350537	34.419789
1033.863812	91689.456010	34.424807
1034.584369	91836.489610	34.429824
1035.423679	91996.283346	34.434842
1036.335168	92138.424876	34.439860
1037.173286	92294.093786	34.444877
1038.013450	92437.629141	34.449895
1038.969187	92595.052150	34.454912
1039.288803	92758.402231	34.459930
1040.414908	92917.988258	34.464948
1041.196259	93083.673116	34.469965
1042.919325	93239.367363	34.474983
1044.869173	93389.371048	34.480000
1045.394522	93547.291598	34.485018
1046.818067	93684.353596	34.490036
1048.302295	93832.933134	34.495053
1049.667103	93976.241986	34.500071
1050.654644	94120.793684	34.505088
1051.635477	94273.551368	34.510106
1052.591576	94416.249072	34.515124
1053.705403	94561.028581	34.520141
1054.469025	94708.147824	34.525159
1055.315778	94855.190394	34.530176
1055.700541	95021.937280	34.535194
1056.762395	95177.940465	34.540212
1057.513914	95347.241200	34.545229
1057.992258	95527.263181	34.550247
1059.230042	95703.528973	34.555264
1059.994679	95889.265376	34.560282
1061.490410	96076.796166	34.565300
1062.843273	96245.335254	34.570317
1063.800983	96414.481246	34.575335
1064.873703	96589.717929	34.580352
1065.745792	96775.391806	34.585370
1067.333928	96950.169209	34.590388
1068.498954	97131.325908	34.595405
1069.625067	97309.477002	34.600423
1071.005561	97487.990976	34.605440
1071.586187	97660.261416	34.610458
1072.971795	97843.031502	34.615476
1073.676545	98019.936509	34.620493
1074.346530	98192.809370	34.625511
1075.591307	98374.923607	34.630528
1076.399133	98577.032295	34.635546
1077.889288	98750.990437	34.640564
1079.291159	98943.091710	34.645581
1079.913998	99121.316289	34.650599
1081.447288	99309.035422	34.655616
1082.321343	99498.154108	34.660634
1083.246768	99678.464467	34.665652
1084.215017	99854.513892	34.670669
1085.319382	100055.469051	34.675687
1086.395594	100246.154185	34.680704
1087.492659	100428.890771	34.685722
1088.784259	100617.205331	34.690740
1089.368585	100811.803270	34.695757
1090.152904	101003.702683	34.700775
1091.240879	101204.998811	34.705792
1092.108684	101405.327402	34.710810
1093.101698	101597.651360	34.715828
1094.352516	101794.086455	34.720845
1095.725251	101985.385768	34.725863
1097.229959	102167.773473	34.730880
1097.795811	102361.151339	34.735898
1098.807075	102534.887585	34.740916
1100.322716	102725.319300	34.745933
1101.023618	102914.296135	34.750951
1102.635320	103120.380573	34.755968
1103.378826	103304.160315	34.760986
1104.034594	103502.850442	34.766004
1104.957384	103705.979799	34.771021
1106.024354	103914.988027	34.776039
1107.317939	104119.196934	34.781056
1108.230619	104325.131801	34.786074
1109.938426	104532.059354	34.791092
1111.331250	104725.984185	34.796109
1112.349357	104923.647644	34.801127
1114.330581	105104.061489	34.806144
1116.174863	105286.475880	34.811162
1117.368073	105461.897379	34.816180
1118.974212	105630.840304	34.821197
1120.292720	105807.825871	34.826215
1121.626376	105976.513640	34.831232
1122.654031	106147.091473	34.836250
1123.441642	106310.200326	34.841268
1124.565633	106483.917725	34.846285
1125.312836	106667.618652	34.851303
1126.450173	106831.228103	34.856320
1127.621694	107015.150075	34.861338
1128.448230	107191.012952	34.866356
1129.687376	107373.456430	34.871373
1130.571223	107563.866148	34.876391
1131.391835	107745.915109	34.881408
1132.056683	107938.290333	34.886426
1132.965276	108134.172003	34.891444
1134.324195	108326.633806	34.896461
1135.231711	108543.267658	34.901479
1136.120105	108747.429002	34.906496
1136.940877	108964.790420	34.911514
1137.852510	109177.906987	34.916532
1138.942619	109399.672095	34.921549
1139.956625	109618.741087	34.926567
1141.318866	109821.587823	34.931584
1142.744480	110042.996632	34.936602
1144.125179	110243.208340	34.941620
1146.076351	110450.633427	34.946637
1146.796196	110662.730156	34.951655
1148.392054	110862.478776	34.956672
1150.029014	111063.108595	34.961690
1152.302369	111221.697676	34.966708
1153.808074	111400.448332	34.971725
1155.086344	111580.353928	34.976743
1156.113123	111733.509063	34.981760
1157.122413	111918.201043	34.986778
1157.812598	112077.522126	34.991796
1159.030095	112242.024179	34.996813
1159.902956	112413.883647	35.001831
1160.795859	112578.025158	35.006848
1161.747569	112749.873180	35.011866
1162.511489	112933.879024	35.016884
1163.389681	113111.367055	35.021901
1164.237606	113296.716517	35.026919
1165.463012	113485.309347	35.031936
1166.756866	113676.742407	35.036954
1168.238164	113860.073988	35.041972
1169.169808	114033.440952	35.046989
1170.015284	114239.727684	35.052007
1171.572099	114437.265798	35.057024
1172.644343	114637.092851	35.062042
1173.634968	114840.064832	35.067060
1174.958783	115035.074910	35.072077
1175.870244	115238.202641	35.077095
1176.701706	115433.768532	35.082112
1177.431763	115649.055920	35.087130
1178.714727	115880.836226	35.092148
1179.439866	116094.822704	35.097165
1180.171240	116330.198200	35.102183
1181.507153	116557.083898	35.107200
1182.571436	116796.055441	35.112218
1183.607726	117028.444708	35.117236
1185.212563	117263.906328	35.122253
1186.071950	117506.035934	35.127271
1187.822985	117731.009703	35.132288
1188.924281	117972.316128	35.137306
1189.947828	118208.074962	35.142324
1191.819346	118442.752803	35.147341
1192.621854	118674.650304	35.152359
1193.900315	118909.294014	35.157376
1195.139999	119154.742894	35.162394
1196.519134	119389.233795	35.167412
1197.520263	119628.733486	35.172429
1198.546216	119871.158198	35.177447
1199.768059	120110.433907	35.182464
1201.116363	120357.394867	35.187482
1201.653044	120611.188041	35.192500
1203.189201	120855.472360	35.197517
1204.258168	121093.147332	35.202535
1205.624712	121330.114246	35.207552
1207.034726	121578.050557	35.212570
1208.582047	121829.399866	35.217588
1210.098780	122057.906409	35.222605
1211.587291	122297.217315	35.227623
1213.119003	122520.211836	35.232640
1214.345168	122761.231567	35.237658
1215.635532	122985.234030	35.242676
1216.895299	123209.750339	35.247693
1218.020872	123445.672487	35.252711
1219.496017	123661.182097	35.257728
1220.598375	123882.625172	35.262746
1221.882915	124101.655909	35.267764
1223.237215	124292.488605	35.272781
1225.144243	124496.561320	35.277799
1226.296428	124695.960992	35.282816
1227.929547	124883.555666	35.287834
1228.797074	125080.687121	35.292852
1230.226541	125270.676497	35.297869
1230.707600	125478.219212	35.302887
1231.696258	125688.984564	35.307904
1232.813417	125892.086349	35.312922
1234.101433	126105.908652	35.317940
1235.043265	126323.505504	35.322957
1235.953982	126552.085949	35.327975
1237.030567	126774.707623	35.332992
1238.083955	127001.669844	35.338010
1238.905680	127244.492400	35.343028
1240.642070	127470.542536	35.348045
1242.066142	127714.406415	35.353063
1243.237101	127945.031280	35.358080
1244.583473	128174.284160	35.363098
1245.249344	128410.766420	35.368116
1246.464964	128647.435208	35.373133
1247.581755	128885.770582	35.378151
1249.349802	129133.034433	35.383168
1250.601990	129368.751614	35.388186
1251.639074	129616.182375	35.393204
1252.965705	129871.399597	35.398221
1254.162639	130116.803969	35.403239
1255.528237	130356.312009	35.408256
1256.588512	130613.165321	35.413274
1258.016763	130865.520755	35.418292
1259.320400	131115.085189	35.423309
1260.503270	131367.030172	35.428327
1261.365819	131622.087163	35.433344
1262.761860	131873.695333	35.438362
1263.932870	132137.679125	35.443380
1265.101533	132394.971709	35.448397
1266.475124	132660.192801	35.453415
1268.086498	132919.366082	35.458432
1269.558035	133173.975967	35.463450
1270.392940	133440.499973	35.468468
1272.181727	133696.593624	35.473485
1273.076487	133962.718582	35.478503
1273.919652	134223.402861	35.483520
1275.463161	134485.782306	35.488538
1276.340762	134761.400011	35.493556
1277.351764	135028.819488	35.498573
1278.642019	135319.674186	35.503591
1280.055383	135587.916763	35.508608
1282.303136	135852.455892	35.513626
1283.370567	136118.074002	35.518644
1284.908403	136384.412462	35.523661
1286.026088	136655.135861	35.528679
1286.865364	136921.090960	35.533696
1288.807101	137178.655874	35.538714
1289.909021	137421.354021	35.543732
1291.546042	137660.412027	35.548749
1293.096558	137904.507651	35.553767
1294.960787	138133.044017	35.558784
1296.682936	138355.215609	35.563802
1298.132045	138585.842142	35.568820
1299.326204	138794.678961	35.573837
1300.694209	139020.174222	35.578855
1301.889086	139251.850454	35.583872
1303.239673	139476.070978	35.588890
1304.112716	139704.064662	35.593908
1305.286859	139937.727152	35.598925
1306.387504	140192.821105	35.603943
1307.219354	140420.357352	35.608960
1308.580987	140673.622182	35.613978
1309.643228	140917.569027	35.618996
1311.477317	141156.871074	35.624013
1312.314184	141408.620569	35.629031
1313.697316	141675.875991	35.634048
1314.724361	141920.609348	35.639066
1316.097447	142189.645724	35.644084
1317.595920	142433.553735	35.649101
1318.788500	142702.295176	35.654119
1320.541765	142961.938826	35.659136
1322.156752	143226.718701	35.664154
1323.120447	143491.104750	35.669172
1323.683148	143745.593531	35.674189
1324.313965	144024.966897	35.679207
1325.399474	144302.387666	35.684224
1326.829468	144582.275321	35.689242
1328.018896	144875.915705	35.694260
1329.457526	145161.196253	35.699277
1330.963724	145449.828288	35.704295
1331.967859	145736.050100	35.709312
1333.827038	146031.652375	35.714330
1334.432876	146332.569984	35.719348
1336.354038	146625.021122	35.724365
1338.096205	146909.755998	35.729383
1339.392880	147199.287371	35.734400
1340.947183	147486.849082	35.739418
1342.405810	147773.249858	35.744436
1344.363297	148050.283319	35.749453
1346.049035	148319.704619	35.754471
1347.718641	148589.828204	35.759488
1349.786228	148835.533292	35.764506
1351.426045	149089.367275	35.769524
1353.398757	149335.751408	35.774541
1355.048296	149576.218419	35.779559
1356.273199	149820.957981	35.784576
1357.285859	150053.685738	35.789594
1358.411903	150295.629445	35.794612
1360.128623	150534.936768	35.799629
1361.410192	150776.971055	35.804647
1362.679798	151017.562914	35.809664
1364.571076	151245.264099	35.814682
1365.539237	151466.427285	35.819700
1367.092196	151676.418127	35.824717
1368.655972	151900.906649	35.829735
1369.709379	152118.291669	35.834752
1371.083497	152331.056535	35.839770
1372.377307	152549.569803	35.844788
1373.955174	152762.264095	35.849805
1375.435900	152970.434991	35.854823
1376.322363	153188.476100	35.859840
1378.042252	153404.003675	35.864858
1379.190766	153636.755071	35.869876
1380.412957	153869.203471	35.874893
1381.617163	154095.453242	35.879911
1382.522178	154340.745399	35.884928
1383.727185	154570.790645	35.889946
1384.470516	154821.631575	35.894964
1385.476605	155071.629918	35.899981
1386.751157	155334.624679	35.904999
1387.724854	155605.106475	35.910016
1388.559655	155880.015828	35.915034
1390.028232	156175.762954	35.920052
1391.216641	156463.212827	35.925069
1392.357068	156746.740270	35.930087
1393.403832	157063.257018	35.935104
1394.650529	157355.397087	35.940122
1395.331545	157669.456560	35.945140
1396.650138	157987.012255	35.950157
1397.494358	158313.557535	35.955175
1398.441767	158648.093000	35.960192
1400.118806	158970.352382	35.965210
1401.914568	159311.624198	35.970228
1403.317454	159650.428655	35.975245
1405.072001	159974.966169	35.980263
1406.678972	160321.835445	35.985280
1408.175038	160652.613745	35.990298
1409.737668	160989.790345	35.995316
1411.159619	161319.343165	36.000333
1413.122486	161644.428748	36.005351
1414.615964	161977.450786	36.010368
1416.582039	162295.790935	36.015386
1417.889480	162625.183070	36.020404
1419.361556	162946.099376	36.025421
1421.147829	163266.888151	36.030439
1422.603538	163587.215651	36.035456
1424.574326	163886.534500	36.040474
1426.027834	164203.199996	36.045492
1427.578523	164500.437919	36.050509
1429.218496	164812.431934	36.055527
1429.988718	165115.022522	36.060544
1431.530206	165421.936879	36.065562
1433.650027	165740.669084	36.070580
1434.398309	166038.917458	36.075597
1436.232274	166349.582077	36.080615
1437.381940	166665.606506	36.085632
1439.290156	166968.966513	36.090650
1440.738671	167258.258816	36.095668
1442.427215	167538.642103	36.100685
1443.169900	167821.942573	36.105703
1444.235502	168115.099941	36.110720
1445.778293	168403.190548	36.115738
1447.247478	168702.335462	36.120756
1448.872878	168994.387449	36.125773
1450.269392	169292.254266	36.130791
1451.528453	169594.651390	36.135808
1452.745465	169903.123428	36.140826
1453.841764	170208.039583	36.145844
1454.753206	170528.077814	36.150861
1456.109503	170844.666502	36.155879
1457.055543	171181.606487	36.160896
1458.830060	171504.638081	36.165914
1460.437242	171839.845205	36.170932
1461.632714	172176.863728	36.175949
1463.222809	172511.215503	36.180967
1464.938432	172854.114305	36.185984
1466.213621	173193.258295	36.191002
1467.478430	173536.645161	36.196020
1468.829967	173893.129323	36.201037
1470.043722	174234.613476	36.206055
1471.112876	174600.555127	36.211072
1473.108905	174952.494745	36.216090
1474.641801	175304.808010	36.221108
1475.890151	175673.595104	36.226125
1477.734119	176025.568293	36.231143
1479.335140	176393.284981	36.236160
1481.036758	176747.102445	36.241178
1482.555981	177102.413132	36.246196
1484.464052	177452.709924	36.251213
1486.261872	177795.387440	36.256231
1487.978733	178151.559990	36.261248
1489.689697	178496.490806	36.266266
1491.271091	178834.731923	36.271284
1492.748079	179180.456138	36.276301
1494.474097	179506.834970	36.281319
1495.796352	179857.755891	36.286336
1497.228369	180189.037749	36.291354
1498.825364	180531.374053	36.296372
1500.591104	180869.774332	36.301389
1501.828989	181215.870025	36.306407
1503.600794	181567.321785	36.311424
1504.959563	181911.433853	36.316442
1506.095501	182252.603378	36.321460
1507.416779	182603.060016	36.326477
1508.905986	182950.964214	36.331495
1510.633184	183302.269739	36.336512
1512.046087	183648.274699	36.341530
1513.495601	183991.305290	36.346548
1515.035735	184349.402300	36.351565
1517.234387	184680.567454	36.356583
1518.999131	185015.642272	36.361600
1520.399375	185352.863205	36.366618
1521.796504	185681.886496	36.371636
1523.279951	186009.487888	36.376653
1524.772130	186344.718681	36.381671
1525.806876	186678.823766	36.386688
1527.303344	187000.424284	36.391706
1528.874997	187334.009645	36.396724
1530.109010	187665.725162	36.401741
1531.868086	187994.674203	36.406759
1532.893977	188331.557547	36.411776
1534.302906	188732.902925	36.416794
1536.188869	189074.847988	36.421812
1537.396755	189423.436031	36.426829
1539.021852	189773.846185	36.431847
1540.454375	190118.819891	36.436864
1541.738421	190482.393410	36.441882
1543.415772	190840.938084	36.446900
1544.611213	191208.923464	36.451917
1546.094967	191564.725259	36.456935
1547.018715	191943.184057	36.461952
1548.516238	192321.661199	36.466970
1549.719373	192709.141118	36.471988
1551.193177	193092.438404	36.477005
1553.029732	193486.124210	36.482023
1554.658793	193876.521716	36.487040
1556.705975	194262.647799	36.492058
1558.648581	194647.016676	36.497076
1560.245775	195040.803631	36.502093
1561.653654	195411.074690	36.507111
1563.311385	195797.733461	36.512128
1565.235053	196177.188469	36.517146
1566.871626	196555.894897	36.522164
1568.672555	196927.909893	36.527181
1570.783745	197296.941026	36.532199
1572.523952	197679.470186	36.537216
1574.410313	198046.207712	36.542234
1576.021209	198405.719321	36.547252
1577.841872	198761.311792	36.552269
1579.810777	199125.095294	36.557287
1580.795003	199484.262574	36.562304
1582.298124	199853.881030	36.567322
1583.927915	200216.471172	36.572340
1584.984385	200594.003684	36.577357
1586.602196	200963.341565	36.582375
1588.286541	201339.919818	36.587392
1590.126260	201705.668350	36.592410
1591.368766	202076.967874	36.597428
1592.574096	202461.505905	36.602445
1594.195197	202839.461151	36.607463
1595.723145	203228.582326	36.612480
1597.148128	203614.942413	36.617498
1598.769206	203998.134661	36.622516
1600.545428	204382.229167	36.627533
1601.917690	204768.540550	36.632551
1603.133891	205169.419139	36.637568
1604.559492	205557.540999	36.642586
1606.594647	205921.879438	36.647604
1607.882189	206305.546301	36.652621
1609.647823	206687.952290	36.657639
1611.049243	207066.803528	36.662656
1612.516056	207446.648453	36.667674
1614.321101	207825.688071	36.672692
1615.492159	208217.345366	36.677709
1617.053020	208613.661444	36.682727
1618.682543	209007.681974	36.687744
1620.410560	209401.839845	36.692762
1621.836583	209797.422595	36.697780
1622.925733	210189.026746	36.702797
1625.132515	210600.276149	36.707815
1626.981639	211001.302995	36.712832
1628.452464	211400.212246	36.717850
1630.280041	211794.668555	36.722868
1631.792945	212191.948696	36.727885
1633.220261	212601.080277	36.732903
1634.981091	213018.918659	36.737920
1636.615021	213431.751944	36.742938
1638.253599	213840.192476	36.747956
1640.103484	214262.795865	36.752973
1642.629227	214670.554800	36.757991
1644.142369	215073.205964	36.763008
1645.365893	215477.736986	36.768026
1646.981129	215888.907717	36.773044
1648.524608	216313.070861	36.778061
1650.172219	216733.814605	36.783079
1651.638026	217146.920894	36.788096
1652.686763	217569.599214	36.793114
1654.768308	217993.245470	36.798132
1656.258411	218437.948508	36.803149
1658.299950	218855.204597	36.808167
1659.766959	219290.060409	36.813184
1661.445706	219722.773615	36.818202
1663.023996	220150.476696	36.823220
1664.965555	220606.693302	36.828237
1666.575939	221035.613423	36.833255
1668.332228	221469.488459	36.838272
1669.963771	221903.564262	36.843290
1672.086680	222333.950870	36.848308
1673.639855	222769.313245	36.853325
1675.417607	223192.751708	36.858343
1677.666796	223608.110050	36.863360
1679.400525	224042.328498	36.868378
1681.651789	224454.717535	36.873396
1683.042437	224880.666390	36.878413
1684.536560	225306.802158	36.883431
1686.194551	225735.552911	36.888448
1687.909691	226156.421189	36.893466
1690.587556	226555.535759	36.898484
1692.298133	226964.392972	36.903501
1694.562119	227370.235662	36.908519
1696.393698	227752.302356	36.913536
1698.082081	228141.913183	36.918554
1699.974899	228521.685414	36.923572
1701.449380	228895.586428	36.928589
1702.786043	229261.485302	36.933607
1704.274211	229645.038201	36.938624
1705.343306	230025.463249	36.943642
1706.742814	230421.047945	36.948660
1707.695435	230819.478828	36.953677
1709.430469	231225.092399	36.958695
1711.056713	231642.715001	36.963712
1712.441016	232055.376009	36.968730
1714.185419	232464.801266	36.973748
1715.822575	232882.602942	36.978765
1717.743095	233302.643293	36.983783
1719.645589	233722.027302	36.988800
1721.121488	234147.048240	36.993818
1723.367351	234554.081070	36.998836
1725.348799	234983.818386	37.003853
1726.755288	235408.930318	37.008871
1728.781821	235828.704335	37.013888
1730.084632	236257.036502	37.018906
1731.757534	236683.274117	37.023924
1733.376549	237120.241493	37.028941
1735.049160	237560.299668	37.033959
1736.872874	237989.384590	37.038976
1738.332781	238445.458895	37.043994
1739.783938	238886.726135	37.049012
1741.081139	239345.598933	37.054029
1742.169843	239815.837730	37.059047
1743.916876	240278.674338	37.064064
1745.422067	240763.043625	37.069082
1747.319699	241237.109500	37.074100
1749.125086	241722.546931	37.079117
1750.182125	242205.674607	37.084135
1752.518721	242699.786756	37.089152
1754.147155	243203.267455	37.094170
1755.663891	243700.112601	37.099188
1756.919447	244215.064550	37.104205
1758.734451	244722.376985	37.109223
1760.374202	245223.039223	37.114240
1761.950922	245754.729808	37.119258
1763.972343	246272.322694	37.124276
1766.149795	246781.862259	37.129293
1768.138772	247290.494791	37.134311
1769.857040	247800.495188	37.139328
1771.540720	248318.529415	37.144346
1773.893948	248834.087174	37.149364
1776.085722	249356.557292	37.154381
1777.123229	249866.244402	37.159399
1778.851344	250381.605709	37.164416
1780.572080	250914.319010	37.169434
1782.635758	251439.276903	37.174452
1784.444720	251962.246478	37.179469
1786.242719	252476.835209	37.184487
1788.572131	252993.086127	37.189504
1790.366386	253500.994984	37.194522
1792.596238	253981.190867	37.199540
1794.704885	254470.908433	37.204557
1796.389243	254943.094300	37.209575
1798.297812	255410.466108	37.214592
1800.480415	255877.892723	37.219610
1802.716006	256346.402659	37.224628
1804.696232	256799.409538	37.229645
1806.709063	257261.683007	37.234663
1808.640906	257723.640062	37.239680
1809.809099	258183.441411	37.244698
1811.773565	258651.514929	37.249716
1813.465902	259109.346606	37.254733
1815.043697	259580.534425	37.259751
1817.565998	260038.401678	37.264768
1819.043731	260514.128049	37.269786
1821.270371	260982.105157	37.274804
1822.795874	261449.719316	37.279821
1824.990388	261925.271571	37.284839
1826.462051	262393.681903	37.289856
1827.648806	262866.230565	37.294874
1829.996139	263342.314616	37.299892
1831.618319	263816.490102	37.304909
1832.874906	264312.371116	37.309927
1834.790479	264793.557626	37.314944
1836.603966	265294.575466	37.319962
1837.971715	265802.705645	37.324980
1839.842182	266302.671129	37.329997
1841.277368	266811.982541	37.335015
1843.199842	267310.921803	37.340032
1844.916965	267826.864635	37.345050
1847.158613	268340.659395	37.350068
1848.720508	268851.648366	37.355085
1850.324344	269374.644871	37.360103
1852.771257	269898.410814	37.365120
1854.095444	270418.201891	37.370138
1856.164541	270941.471810	37.375156
1858.250609	271475.508548	37.380173
1860.311814	272003.883758	37.385191
1862.146889	272525.869789	37.390208
1863.904398	273060.238995	37.395226
1865.913409	273587.527596	37.400244
1867.612760	274120.177093	37.405261
1869.419586	274653.772284	37.410279
1871.490825	275184.247339	37.415296
1873.672854	275709.774167	37.420314
1875.820924	276222.172675	37.425332
1878.018957	276753.282632	37.430349
1879.650936	277278.289967	37.435367
1881.736260	277794.200724	37.440384
1883.411310	278319.299517	37.445402
1885.858324	278837.888989	37.450420
1887.561017	279363.437354	37.455437
1889.186998	279894.560249	37.460455
1891.026832	280404.841167	37.465472
1892.675162	280922.367327	37.470490
1894.160475	281436.770023	37.475508
1896.116224	281956.475715	37.480525
1897.802930	282471.704353	37.485543
1899.475079	282997.145038	37.490560
1900.891337	283521.840286	37.495578
1902.361882	284044.543176	37.500596
1904.046736	284571.347913	37.505613
1905.933268	285110.334004	37.510631
1907.914076	285655.118692	37.515648
1909.801224	286204.972000	37.520666
1911.590832	286754.128599	37.525684
1913.766778	287294.123595	37.530701
1915.348204	287850.423423	37.535719
1917.220804	288408.982501	37.540736
1919.154503	288977.637901	37.545754
1920.797948	289536.155049	37.550772
1922.805345	290100.627183	37.555789
1925.236765	290682.041941	37.560807
1927.185104	291252.208337	37.565824
1929.347627	291828.837594	37.570842
1931.155530	292393.993386	37.575860
1933.195342	292965.024722	37.580877
1935.102984	293538.920460	37.585895
1937.506015	294099.749681	37.590912
1939.894738	294669.468029	37.595930
1941.624113	295239.702511	37.600948
1943.993494	295803.678038	37.605965
1946.192806	296365.622345	37.610983
1948.351257	296928.103939	37.616000
1950.449569	297486.300435	37.621018
1952.531483	298032.534214	37.626036
1954.914857	298576.072049	37.631053
1956.776191	299152.052710	37.636071
1958.807614	299697.092118	37.641088
1960.412787	300256.474598	37.646106
1962.181851	300819.686084	37.651124
1963.995507	301380.600788	37.656141
1966.021826	301954.072521	37.661159
1967.827561	302523.997405	37.666176
1969.663154	303087.361237	37.671194
1971.410029	303657.542866	37.676212
1973.646545	304228.297319	37.681229
1975.920489	304808.361923	37.686247
1977.959056	305367.993764	37.691264
1979.609736	305946.176271	37.696282
1981.973496	306523.293161	37.701300
1984.189414	307087.276496	37.706317
1985.888941	307654.061505	37.711335
1987.955134	308227.280912	37.716352
1989.660837	308801.599013	37.721370
1991.669955	309381.346250	37.726388
1993.486037	309965.312243	37.731405
1994.846766	310553.160797	37.736423
1997.018458	311135.965061	37.741440
1998.757998	311728.082053	37.746458
2000.340874	312305.670579	37.751476
2002.394754	312884.951552	37.756493
2004.308316	313465.369208	37.761511
2006.722404	314041.024271	37.766528
2007.951203	314626.526651	37.771546
2009.736336	315204.285860	37.776564
2011.911991	315790.911616	37.781581
2013.780452	316386.345220	37.786599
2015.324766	316983.022499	37.791616
2017.095573	317582.804362	37.796634
2019.436810	318205.868849	37.801652
2021.636497	318809.933669	37.806669
2023.162158	319439.143726	37.811687
2025.126162	320050.092967	37.816704
2027.325664	320690.322170	37.821722
2029.076687	321331.002502	37.826740
2031.252674	321969.115444	37.831757
2032.640325	322615.227508	37.836775
2034.509427	323265.135086	37.841792
2036.715678	323917.618597	37.846810
2038.637218	324581.086405	37.851828
2040.745195	325231.262153	37.856845
2042.416795	325906.030568	37.861863
2044.717825	326580.582074	37.866880
2046.873414	327249.590747	37.871898
2048.964411	327923.350185	37.876916
2050.561540	328596.678418	37.881933
2052.783202	329290.683695	37.886951
2055.192661	329970.101810	37.891968
2057.249381	330655.639268	37.896986
2059.439195	331336.195199	37.902004
2062.507819	332012.251442	37.907021
2065.310550	332687.253151	37.912039
2067.094951	333354.348102	37.917056
2069.610571	334021.487345	37.922074
2071.495802	334688.700571	37.927092
2074.330681	335340.588650	37.932109
2076.532401	336001.181878	37.937127
2079.108797	336643.477307	37.942144
2081.434022	337289.767358	37.947162
2083.504923	337944.164349	37.952180
2085.820301	338570.057360	37.957197
2087.890573	339216.290073	37.962215
2089.830768	339847.383692	37.967232
2092.044790	340486.569800	37.972250
2094.019094	341125.940795	37.977268
2096.047476	341757.527581	37.982285
2097.864383	342413.964234	37.987303
2099.695101	343060.516639	37.992320
2101.894356	343702.911045	37.997338
2103.831848	344359.452323	38.002356
2106.212452	344995.300832	38.007373
2108.562525	345642.033244	38.012391
2110.576438	346292.646136	38.017408
2112.908877	346928.831365	38.022426
2114.565054	347555.682825	38.027444
2116.812378	348157.656289	38.032461
2119.170453	348774.904942	38.037479
2121.666491	349383.036607	38.042496
2123.807140	349980.613395	38.047514
2125.691842	350595.608215	38.052532
2128.249434	351195.939129	38.057549
2130.478019	351800.910840	38.062567
2132.414300	352399.072813	38.067584
2134.788399	352995.197696	38.072602
2136.586631	353611.483511	38.077620
2138.753217	354222.394219	38.082637
2140.671987	354843.386191	38.087655
2142.684884	355450.473808	38.092672
2145.320127	356067.798072	38.097690
2146.931128	356690.895422	38.102708
2148.609372	357322.039967	38.107725
2150.689841	357962.239588	38.112743
2152.843806	358602.492572	38.117760
2155.106602	359231.020880	38.122778
2157.406157	359880.311099	38.127796
2159.277241	360529.131143	38.132813
2161.600811	361176.619998	38.137831
2163.380295	361827.539824	38.142848
2165.499338	362485.240136	38.147866
2167.088275	363148.955969	38.152884
2169.153809	363813.847182	38.157901
2171.406169	364488.714833	38.162919
2173.766681	365170.882901	38.167936
2175.664600	365850.631788	38.172954
2177.869155	366535.287546	38.177972
2180.308467	367222.401684	38.182989
2182.270223	367919.705205	38.188007
2184.283309	368599.992606	38.193024
2186.500012	369301.106889	38.198042
2188.511930	370009.166778	38.203060
2190.567671	370713.045728	38.208077
2192.839804	371416.468012	38.213095
2195.172649	372136.275055	38.218112
2197.301208	372845.907108	38.223130
2199.737390	373566.149079	38.228148
2201.804621	374271.831749	38.233165
2204.047841	374990.859878	38.238183
2206.746356	375709.693703	38.243200
2209.261486	376403.032972	38.248218
2211.636940	377123.160172	38.253236
2214.111074	377827.584170	38.258253
2216.046641	378531.020485	38.263271
2218.811008	379247.916739	38.268288
2221.534347	379947.714603	38.273306
2223.110818	380652.612673	38.278324
2225.214708	381346.223930	38.283341
2227.365322	382054.594051	38.288359
2229.433740	382762.379631	38.293376
2231.414400	383465.372933	38.298394
2233.777864	384162.327509	38.303412
2236.112492	384841.981637	38.308429
2238.273314	385518.152407	38.313447
2240.391070	386204.405785	38.318464
2242.515085	386882.683042	38.323482
2244.877398	387570.664564	38.328500
2247.159505	388253.422596	38.333517
2249.571625	388948.336104	38.338535
2251.200557	389632.113186	38.343552
2253.819649	390321.434280	38.348570
2255.963443	391022.708808	38.353588
2258.160984	391718.888601	38.358605
2260.930915	392418.122682	38.363623
2263.162204	393119.333427	38.368640
2265.339404	393812.173159	38.373658
2267.345560	394511.868862	38.378676
2270.287732	395222.209633	38.383693
2272.545611	395931.154961	38.388711
2274.025912	396638.264652	38.393728
2276.440174	397345.729638	38.398746
2278.641213	398068.063611	38.403764
2280.418076	398787.943252	38.408781
2283.118735	399519.759251	38.413799
2285.300763	400265.074812	38.418816
2287.663564	401001.572746	38.423834
2289.539739	401737.222449	38.428852
2292.129701	402482.004186	38.433869
2294.121174	403230.010047	38.438887
2295.951998	403979.923373	38.443904
2298.269773	404734.876077	38.448922
2300.901115	405496.442666	38.453940
2302.645414	406254.314273	38.458957
2304.944057	407023.368443	38.463975
2307.237023	407799.950679	38.468992
2309.540500	408574.279513	38.474010
2311.895479	409359.747955	38.479028
2314.193125	410137.528028	38.484045
2316.784812	410917.691904	38.489063
2318.919950	411705.103985	38.494080
2321.991373	412468.878890	38.499098
2324.635182	413264.439165	38.504116
2327.215689	414033.165438	38.509133
2329.979560	414786.971429	38.514151
2332.674840	415575.917652	38.519168
2335.186340	416334.380961	38.524186
2337.460298	417091.140269	38.529204
2340.129777	417847.454813	38.534221
2343.073419	418599.091229	38.539239
2344.739116	419360.596124	38.544256
2347.601079	420107.466143	38.549274
2349.885597	420858.919237	38.554292
2352.323469	421610.475173	38.559309
2354.524619	422352.073398	38.564327
2356.903470	423109.720405	38.569344
2359.239543	423840.515958	38.574362
2361.397432	424574.256551	38.579380
2363.533702	425279.221020	38.584397
2366.013851	426001.623321	38.589415
2367.963543	426726.018307	38.594432
2369.959697	427446.029602	38.599450
2372.385596	428177.386476	38.604468
2374.685780	428916.942932	38.609485
2376.915113	429642.668951	38.614503
2378.966512	430395.078902	38.619520
2380.878830	431146.577259	38.624538
2382.842750	431908.114923	38.629556
2385.036322	432682.241648	38.634573
2387.733530	433451.144454	38.639591
2390.007525	434232.088410	38.644608
2392.306867	435010.673317	38.649626
2394.399716	435798.730280	38.654644
2396.392550	436605.450073	38.659661
2398.406235	437402.674628	38.664679
2400.598043	438227.215632	38.669696
2403.420731	439037.652906	38.674714
2405.996273	439864.850603	38.679732
2408.314945	440690.290403	38.684749
2411.132058	441509.745170	38.689767
2413.302656	442350.376541	38.694784
2415.867744	443168.092072	38.699802
2418.457762	444004.692402	38.704820
2420.741897	444833.674144	38.709837
2423.674391	445668.077347	38.714855
2425.724741	446511.905893	38.719872
2428.590778	447352.476233	38.724890
2430.829636	448189.529433	38.729908
2433.085006	449038.431989	38.734925
2435.517299	449882.819532	38.739943
2438.129337	450727.344580	38.744960
2440.163221	451571.023968	38.749978
2443.010267	452436.628153	38.754996
2445.903105	453277.208828	38.760013
2448.801105	454131.305282	38.765031
2451.128316	454976.918783	38.770048
2453.831515	455819.197142	38.775066
2456.083532	456677.038724	38.780084
2458.762468	457524.609354	38.785101
2461.012077	458377.475162	38.790119
2463.312299	459240.153407	38.795136
2465.469885	460090.990357	38.800154
2468.088758	460948.283048	38.805172
2470.440811	461815.339202	38.810189
2473.211286	462678.899346	38.815207
2475.390320	463552.478859	38.820224
2477.714978	464413.562177	38.825242
2479.973179	465283.765580	38.830260
2482.847545	466163.122600	38.835277
2485.781747	467029.442895	38.840295
2488.452864	467900.973454	38.845312
2490.771595	468757.770885	38.850330
2493.388553	469584.669716	38.855348
2495.281091	470424.892946	38.860365
2498.074274	471255.326169	38.865383
2500.346782	472090.610824	38.870400
2502.862385	472919.047679	38.875418
2505.267754	473765.499585	38.880436
2507.733129	474611.296545	38.885453
2510.526333	475452.150045	38.890471
2512.762866	476309.020110	38.895488
2515.172233	477156.831054	38.900506
2517.685988	478011.048967	38.905524
2520.072631	478866.662495	38.910541
2522.399668	479731.537149	38.915559
2524.359797	480602.088408	38.920576
2526.554174	481482.807251	38.925594
2529.203074	482376.936121	38.930612
2531.356127	483280.646830	38.935629
2533.886632	484174.705691	38.940647
2536.092554	485099.517818	38.945664
2538.660798	486006.955919	38.950682
2541.238391	486930.649190	38.955700
2543.586196	487859.733552	38.960717
2546.103807	488782.783828	38.965735
2548.244590	489725.329880	38.970752
2550.255099	490670.117681	38.975770
2552.885851	491626.404321	38.980788
2555.417655	492597.035340	38.985805
2558.188658	493562.322781	38.990823
2560.573363	494537.409329	38.995840
2562.986638	495514.553692	39.000858
2565.902345	496484.139697	39.005876
2568.964127	497467.970941	39.010893
2571.737339	498442.360937	39.015911
2574.084243	499429.023283	39.020928
2576.640283	500412.918010	39.025946
2579.253983	501402.846523	39.030964
2581.365204	502392.044782	39.035981
2584.228558	503382.668320	39.040999
2587.412841	504382.152112	39.046016
2589.880389	505379.780803	39.051034
2592.713304	506382.075055	39.056052
2595.196989	507391.121992	39.061069
2597.510942	508373.366188	39.066087
2600.483395	509382.002251	39.071104
2602.755655	510392.508474	39.076122
2605.331713	511405.720704	39.081140
2607.732966	512429.834002	39.086157
2610.270824	513435.664609	39.091175
2612.732741	514473.038876	39.096192
2615.368432	515498.321926	39.101210
2617.906493	516520.480344	39.106228
2619.826962	517569.378710	39.111245
2622.460785	518611.685602	39.116263
2624.791297	519658.758904	39.121280
2627.188410	520696.228773	39.126298
2629.844914	521729.251791	39.131316
2632.410655	522750.031599	39.136333
2635.215725	523774.377630	39.141351
2637.600604	524803.257640	39.146368
2640.766033	525814.964154	39.151386
2643.505141	526846.009251	39.156404
2646.296093	527872.794954	39.161421
2648.631413	528901.751841	39.166439
2651.375358	529936.607664	39.171456
2653.782875	530972.907586	39.176474
2656.732686	532017.195099	39.181492
2659.161745	533068.592909	39.186509
2662.096893	534105.082524	39.191527
2664.518571	535160.355328	39.196544
2666.781410	536222.370633	39.201562
2669.845816	537282.509731	39.206580
2672.032201	538353.989477	39.211597
2674.353351	539437.489163	39.216615
2676.860368	540522.986723	39.221632
2679.503079	541608.075577	39.226650
2682.712842	542691.726162	39.231668
2685.388731	543796.405466	39.236685
2688.504411	544882.667696	39.241703
2691.267601	545980.319191	39.246720
2693.841132	547090.133540	39.251738
2696.781840	548184.713034	39.256756
2699.453876	549292.120228	39.261773
2702.217017	550391.027335	39.266791
2704.817486	551501.634764	39.271808
2707.577126	552619.511796	39.276826
2710.728462	553734.113356	39.281844
2713.207431	554853.008458	39.286861
2715.940432	555972.871892	39.291879
2718.612641	557088.933613	39.296896
2721.178258	558207.883617	39.301914
2723.840216	559326.169801	39.306932
2726.038368	560476.536426	39.311949
2728.740257	561609.539252	39.316967
2731.574467	562770.393682	39.321984
2734.260926	563915.753532	39.327002
2736.912880	565070.106177	39.332020
2739.719012	566229.600857	39.337037
2742.930714	567371.752491	39.342055
2746.139824	568522.336203	39.347072
2749.317393	569658.767383	39.352090
2752.559120	570790.067023	39.357108
2755.524509	571932.202634	39.362125
2758.427832	573063.356366	39.367143
2761.474677	574194.233123	39.372160
2763.831169	575327.232722	39.377178
2766.782473	576456.666557	39.382196
2769.131077	577595.280112	39.387213
2771.998227	578730.540371	39.392231
2774.871617	579869.606804	39.397248
2777.114299	581001.253465	39.402266
2779.784931	582109.706745	39.407284
2781.849982	583218.613890	39.412301
2784.459256	584337.804719	39.417319
2787.131016	585448.208995	39.422336
2789.663613	586575.677287	39.427354
2792.579899	587703.525490	39.432372
2795.548466	588838.074067	39.437389
2797.689918	589962.483621	39.442407
2800.712744	591110.085479	39.447424
2803.031527	592250.381672	39.452442
2806.116590	593404.162887	39.457460
2808.813165	594570.169361	39.462477
2811.630866	595732.833525	39.467495
2814.289262	596894.457472	39.472512
2816.958802	598077.646110	39.477530
2820.272526	599244.881676	39.482548
2822.806474	600424.348280	39.487565
2825.641671	601616.908323	39.492583
2828.534822	602814.089477	39.497600
2831.006733	604013.369099	39.502618
2834.149499	605210.005458	39.507636
2836.805592	606428.215341	39.512653
2839.350368	607633.103856	39.517671
2842.804030	608850.615226	39.522688
2845.482318	610070.927948	39.527706
2848.428521	611286.309804	39.532724
2851.359233	612512.914086	39.537741
2854.282546	613746.934711	39.542759
2857.046129	614968.144475	39.547776
2859.942847	616202.344525	39.552794
2862.787541	617447.512017	39.557812
2865.425612	618696.921298	39.562829
2868.510422	619939.763509	39.567847
2871.352764	621188.151375	39.572864
2873.632737	622461.723831	39.577882
2876.496810	623723.554814	39.582900
2879.265174	624998.141724	39.587917
2882.282655	626273.283075	39.592935
2884.637274	627554.427744	39.597952
2887.455022	628847.822419	39.602970
2890.388275	630151.374356	39.607988
2893.168940	631459.533482	39.613005
2895.652811	632765.383543	39.618023
2898.492569	634077.547767	39.623040
2901.077464	635408.753373	39.628058
2904.200869	636739.246776	39.633076
2906.618979	638077.771547	39.638093
2909.611027	639424.704012	39.643111
2912.413449	640773.786069	39.648128
2915.220536	642123.387076	39.653146
2918.192973	643484.100031	39.658164
2921.243646	644850.001414	39.663181
2923.744739	646205.841203	39.668199
2926.819469	647570.322291	39.673216
2929.945655	648927.880298	39.678234
2933.406967	650242.689605	39.683252
2936.989758	651564.229773	39.688269
2940.353577	652872.179768	39.693287
2943.840820	654153.983012	39.698304
2946.989690	655436.174834	39.703322
2950.311202	656711.994114	39.708340
2953.970534	657988.883417	39.713357
2957.062332	659243.397702	39.718375
2960.445952	660498.396589	39.723392
2963.382070	661759.629960	39.728410
2966.444367	663016.894177	39.733428
2969.682963	664270.729007	39.738445
2972.609044	665520.820676	39.743463
2975.514866	666775.029980	39.748480
2978.182406	668037.619896	39.753498
2981.438895	669294.420252	39.758516
2984.287179	670570.715307	39.763533
2986.846280	671844.947309	39.768551
2989.374440	673112.449027	39.773568
2991.778688	674400.825790	39.778586
2994.980504	675691.869883	39.783604
2997.607483	676992.174611	39.788621
3000.488983	678297.171760	39.793639
3003.626198	679617.440034	39.798656
3005.807933	680949.503341	39.803674
3009.131236	682272.834028	39.808692
3011.847215	683618.123955	39.813709
3014.725746	684964.924542	39.818727
3018.246021	686312.755389	39.823744
3021.037346	687665.621614	39.828762
3023.797484	689020.919721	39.833780
3026.575347	690395.361332	39.838797
3028.885580	691776.269486	39.843815
3031.505815	693173.577241	39.848832
3034.113498	694580.883598	39.853850
3036.942362	696003.448964	39.858868
3039.821790	697431.873986	39.863885
3042.420994	698884.553045	39.868903
3045.718086	700331.171433	39.873920
3048.954109	701779.294136	39.878938
3051.892663	703219.843185	39.883956
3054.854398	704684.966967	39.888973
3057.826037	706159.943793	39.893991
3060.993797	707624.085250	39.899008
3063.800659	709120.716096	39.904026
3067.066722	710604.827266	39.909044
3070.230487	712090.378999	39.914061
3072.899990	713593.915654	39.919079
3076.405564	715088.035954	39.924096
3079.390999	716589.844484	39.929114
3082.542671	718090.316027	39.934132
3085.897745	719595.031913	39.939149
3088.659232	721101.751646	39.944167
3092.004765	722610.766340	39.949184
3094.749271	724115.109489	39.954202
3097.923662	725592.863843	39.959220
3101.016220	727053.715021	39.964237
3103.779359	728532.439993	39.969255
3106.651635	730004.851532	39.974272
3109.613488	731499.941210	39.979290
3112.404264	732979.132350	39.984308
3115.826579	734475.762590	39.989325
3118.552679	735972.725307	39.994343
3121.858345	737471.775154	39.999360
3124.978420	738978.220507	40.004378
3128.177133	740493.983922	40.009396
3131.133597	742005.897505	40.014413
3134.061544	743527.583339	40.019431
3137.944086	745046.148585	40.024448
3141.308021	746561.648305	40.029466
3144.391514	748073.155592	40.034484
3147.930550	749583.600538	40.039501
3151.260604	751111.764391	40.044519
3154.982901	752635.125538	40.049536
3157.867826	754158.720886	40.054554
3161.041905	755676.991099	40.059572
3164.823243	757204.206151	40.064589
3167.288610	758732.421034	40.069607
3170.914948	760258.554478	40.074624
3174.630316	761789.085536	40.079642
3177.666207	763317.994420	40.084660
3180.755703	764855.087656	40.089677
3183.506879	766391.036926	40.094695
3186.551464	767929.616532	40.099712
3189.929449	769475.435649	40.104730
3193.465525	771016.826356	40.109748
3196.591611	772570.488469	40.114765
3199.602772	774124.380874	40.119783
3203.211453	775677.104078	40.124800
3206.479902	777236.425788	40.129818
3209.324978	778788.466796	40.134836
3212.926794	780347.797204	40.139853
3215.633086	781924.258380	40.144871
3219.053782	783487.451225	40.149888
3221.999221	785069.456540	40.154906
3225.045786	786646.338330	40.159924
3228.401019	788230.903702	40.164941
3231.554982	789828.182047	40.169959
3234.679660	791411.289105	40.174976
3237.523054	793009.661833	40.179994
3240.175662	794618.180681	40.185012
3243.619017	796235.494792	40.190029
3246.644591	797860.383576	40.195047
3249.690747	799485.181256	40.200064
3253.157766	801125.423216	40.205082
3256.102765	802759.005171	40.210100
3259.375328	804391.946229	40.215117
3262.236031	806050.475482	40.220135
3265.392502	807710.260516	40.225152
3268.276976	809362.356723	40.230170
3271.326813	810990.622604	40.235188
3274.007766	812631.792241	40.240205
3277.141907	814266.575341	40.245223
3280.040073	815912.420999	40.250240
3283.230566	817556.638947	40.255258
3286.066609	819211.097132	40.260276
3289.406014	820870.274598	40.265293
3292.567193	822551.154576	40.270311
3296.019180	824226.240942	40.275328
3299.537087	825905.956090	40.280346
3302.819697	827601.553082	40.285364
3306.312242	829281.522155	40.290381
3309.728071	830979.720594	40.295399
3313.234727	832672.539170	40.300416
3316.352952	834379.385949	40.305434
3319.430315	836091.527016	40.310452
3323.064677	837807.540787	40.315469
3325.754214	839541.685543	40.320487
3329.222499	841273.812900	40.325504
3332.632362	843011.113683	40.330522
3335.903211	844757.288720	40.335540
3339.305178	846509.464922	40.340557
3342.554277	848263.118471	40.345575
3346.001839	850014.690373	40.350592
3349.627400	851780.202092	40.355610
3352.878261	853545.661569	40.360628
3356.299753	855307.189883	40.365645
3359.219958	857092.740987	40.370663
3363.043193	858852.016954	40.375680
3366.852530	860635.797505	40.380698
3370.466112	862410.655881	40.385716
3373.976072	864192.277153	40.390733
3377.045154	865978.095820	40.395751
3380.675241	867752.249467	40.400768
3384.292413	869531.783644	40.405786
3387.471135	871317.344727	40.410804
3391.372551	873089.089226	40.415821
3395.025746	874872.627622	40.420839
3398.383835	876651.519658	40.425856
3401.546241	878430.099800	40.430874
3405.054901	880222.960123	40.435892
3408.154196	882019.782482	40.440909
3411.068862	883808.645735	40.445927
3414.851631	885606.654504	40.450944
3418.399695	887402.116600	40.455962
3421.425315	889219.102591	40.460980
3425.006346	891020.083659	40.465997
3428.120834	892830.313610	40.471015
3431.279741	894650.079750	40.476032
3434.695254	896467.965390	40.481050
3437.601829	898310.972975	40.486068
3440.883803	900144.454786	40.491085
3444.074029	901992.079496	40.496103
3447.882970	903836.293425	40.501120
3450.907958	905657.636758	40.506125
3454.472356	907455.935340	40.511130
3457.861733	909173.977780	40.516135
3461.553997	910845.958056	40.521140
3464.164782	912436.130164	40.526144
3467.530556	913961.582603	40.531149
3470.310798	915412.392852	40.536154
3473.275434	916780.307527	40.541159
3476.106701	918090.843772	40.546164
3478.452047	919320.727126	40.551168
3481.302185	920486.000124	40.556173
3483.741838	921555.802117	40.561178
3486.334172	922573.066869	40.566183
3488.895020	923527.474280	40.571188
3490.754361	924385.054929	40.576192
3493.002991	925197.557770	40.581197
3494.890876	925947.164883	40.586202
3497.175523	926622.053491	40.591207
3499.261146	927240.411553	40.596212
3500.951933	927792.495725	40.601216
3502.642104	928292.184276	40.606221
3503.973459	928746.947090	40.611226
3505.770699	929133.898498	40.616231
3506.895473	929483.971721	40.621236
3508.104521	929786.580147	40.626240
3509.796136	930057.984293	40.631245
3511.091347	930289.987175	40.636250
3512.442882	930456.310173	40.641255
3513.175648	930600.271411	40.646260
3514.154920	930697.151517	40.651264
3515.569572	930776.389558	40.656269
3516.172432	930813.050323	40.661274
3517.137676	930807.126251	40.666279
3517.763288	930785.422008	40.671284
3518.447211	930732.991071	40.676288
3519.114739	930662.516120	40.681293
3519.814675	930568.804496	40.686298
3520.391373	930440.170139	40.691303
3520.691826	930306.107955	40.696308
3521.782069	930146.179499	40.701312
3522.345744	929964.927313	40.706317
3522.800009	929771.014659	40.711322
3523.278373	929552.704002	40.716327
3523.789267	929324.393215	40.721332
3524.163238	929073.051244	40.726336
3525.038977	928808.264298	40.731341
3525.024910	928532.284545	40.736346
3525.491971	928229.606640	40.741351
3525.744323	927930.405604	40.746356
3526.048778	927614.466805	40.751360
3526.784916	927293.056636	40.756365
3526.852210	926947.822768	40.761370
3527.096711	926598.309423	40.766375
3527.220455	926237.937739	40.771380
3527.372869	925877.344647	40.776384
3527.728898	925504.874070	40.781389
3527.703566	925130.712971	40.786394
3528.388560	924745.353159	40.791399
3528.531795	924343.335786	40.796404
3528.415881	923942.389680	40.801408
3529.147501	923538.769767	40.806413
3529.065502	923123.434735	40.811418
3529.196340	922692.072850	40.816423
3529.315151	922275.003571	40.821428
3529.073133	921837.579723	40.826432
3529.713682	921392.853935	40.831437
3529.826810	920957.221032	40.836442
3529.804588	920507.630806	40.841447
3529.469693	920059.018270	40.846452
3529.895100	919610.238637	40.851456
3529.833399	919150.730693	40.856461
3530.083234	918701.135935	40.861466
3530.383254	918224.940111	40.866471
3530.811806	917761.574330	40.871476
3530.889922	917284.371483	40.876480
3530.852359	916806.953919	40.881485
3530.561025	916335.890059	40.886490
3530.892387	915841.673744	40.891495
3530.334430	915359.116184	40.896500
3530.376304	914871.022107	40.901504
3530.631418	914389.202557	40.906509
3530.677901	913905.257664	40.911514
3530.804170	913417.307974	40.916519
3530.738030	912933.103579	40.921524
3530.793437	912437.277565	40.926528
3530.937832	911942.162065	40.931533
3530.763627	911453.414278	40.936538
3531.298325	910939.549118	40.941543
3531.009528	910451.887824	40.946548
3530.819183	909952.892290	40.951552
3531.058276	909442.310245	40.956557
3530.750701	908940.544604	40.961562
3531.104676	908442.186671	40.966567
3531.010554	907929.015294	40.971572
3531.092321	907416.826665	40.976576
3531.140233	906916.648066	40.981581
3530.482646	906407.963112	40.986586
3530.724055	905895.510018	40.991591
3530.868028	905400.385407	40.996596
3530.924719	904888.545931	41.001600
3531.436763	904369.057881	41.006605
3531.039365	903863.278364	41.011610
3531.241757	903336.608284	41.016615
3531.385697	902827.458613	41.021620
3531.136431	902298.258972	41.026624
3531.153127	901779.579067	41.031629
3531.101481	901259.028988	41.036634
3531.277725	900731.056023	41.041639
3531.136991	900214.864023	41.046644
3530.835772	899687.453434	41.051648
3531.221745	899172.040970	41.056653
3531.001598	898655.043250	41.061658
3531.041649	898119.316477	41.066663
3530.939201	897595.538309	41.071668
3531.074068	897074.278710	41.076672
3531.196772	896548.529788	41.081677
3531.113634	896022.670469	41.086682
3531.121367	895490.080610	41.091687
3531.179965	894958.011671	41.096692
3531.083893	894433.746087	41.101696
3531.066126	893895.599507	41.106701
3531.207954	893375.254311	41.111706
3530.863630	892839.189625	41.116711
3530.819664	892310.949655	41.121716
3530.868096	891781.194818	41.126720
3531.188479	891252.214483	41.131725
3530.843985	890730.163721	41.136730
3531.010893	890192.119098	41.141735
3530.919125	889661.998203	41.146740
3530.957707	889131.128945	41.151744
3531.366614	888587.185827	41.156749
3531.372476	888057.770449	41.161754
3531.384379	887513.309690	41.166759
3531.014038	886973.797123	41.171764
3531.102532	886440.638825	41.176768
3531.283182	885894.544699	41.181773
3530.847130	885357.698437	41.186778
3531.032081	884822.438486	41.191783
3530.879984	884286.508919	41.196788
3530.698474	883748.985799	41.201792
3531.219408	883211.099260	41.206797
3530.898672	882668.465189	41.211802
3531.017541	882128.900934	41.216807
3531.460358	881582.355315	41.221812
3531.027612	881043.462437	41.226816
3531.204329	880490.564257	41.231821
3531.028111	879957.145191	41.236826
3531.186137	879394.265383	41.241831
3531.292562	878851.299595	41.246836
3531.053379	878304.272649	41.251840
3531.289116	877751.977391	41.256845
3531.191041	877204.920646	41.261850
3531.149207	876658.094094	41.266855
3531.394560	876118.728595	41.271860
3531.250271	875562.802675	41.276864
3531.269416	875003.790812	41.281869
3530.861943	874462.639918	41.286874
3531.109468	873905.909100	41.291879
3531.080548	873353.925087	41.296884
3530.870853	872794.646184	41.301888
3530.747009	872236.560790	41.306893
3530.805722	871694.204016	41.311898
3530.642822	871136.700872	41.316903
3530.935216	870590.225695	41.321908
3530.813933	870045.614603	41.326912
3530.880645	869486.559120	41.331917
3530.825185	868953.191078	41.336922
3531.088860	868391.961291	41.341927
3531.092258	867838.488893	41.346932
3530.987586	867287.701964	41.351936
3530.774313	866720.766180	41.356941
3530.512856	866171.845214	41.361946
3530.527742	865616.029397	41.366951
3530.792668	865069.928165	41.371956
3530.559422	864517.549316	41.376960
3530.839060	863961.923974	41.381965
3530.647195	863415.265014	41.386970
3530.755194	862860.441809	41.391975
3530.453597	862302.625619	41.396980
3530.585467	861758.773489	41.401984
3530.513337	861206.161360	41.406989
3530.380656	860663.130658	41.411994
3530.450061	860095.426462	41.416999
3530.302427	859551.812965	41.422004
3530.343523	858995.578197	41.427008
3530.365883	858446.781912	41.432013
3530.080954	857903.336365	41.437018
3530.258034	857346.636261	41.442023
3530.442744	856798.344732	41.447028
3530.432018	856244.688305	41.452032
3530.511694	855688.923817	41.457037
3530.382106	855134.020151	41.462042
3530.320169	854580.708586	41.467047
3530.506183	854038.298861	41.472052
3530.227346	853475.487558	41.477056
3530.669807	852918.340265	41.482061
3530.122769	852365.496244	41.487066
3530.077393	851796.263442	41.492071
3530.447810	851250.073198	41.497076
3530.067944	850702.210631	41.502080
3530.261730	850137.554287	41.507085
3530.188858	849591.001389	41.512090
3530.504879	849030.994230	41.517095
3530.324214	848476.572039	41.522100
3530.043798	847920.754045	41.527104
3530.517668	847357.258148	41.532109
3529.948779	846802.850672	41.537114
3529.790080	846245.596341	41.542119
3529.975580	845697.099049	41.547124
3529.781954	845145.305752	41.552128
3529.944533	844584.730902	41.557133
3529.760201	844037.515638	41.562138
3530.143417	843471.931331	41.567143
3529.967106	842916.820530	41.572148
3529.908870	842363.492631	41.577152
3530.105291	841801.396690	41.582157
3529.798081	841254.447858	41.587162
3529.905834	840696.753319	41.592167
3530.106910	840133.825709	41.597172
3530.186591	839576.768582	41.602176
3530.157174	839012.512968	41.607181
3530.082399	838458.065928	41.612186
3529.983444	837892.796112	41.617191
3530.143802	837338.211271	41.622196
3530.258327	836776.805527	41.627200
3530.154154	836210.606809	41.632205
3529.931420	835645.988139	41.637210
3529.946135	835087.866115	41.642215
3530.046176	834531.388750	41.647220
3529.795926	833965.260132	41.652224
3529.471466	833396.361071	41.657229
3529.540995	832846.185076	41.662234
3529.519699	832291.242515	41.667239
3529.246124	831748.353338	41.672244
3528.987592	831189.548495	41.677248
3529.309920	830621.953716	41.682253
3529.271218	830078.004982	41.687258
3529.317963	829527.989173	41.692263
3529.522033	828971.990211	41.697268
3529.175258	828428.736918	41.702272
3529.453289	827865.743555	41.707277
3529.431424	827318.873738	41.712282
3529.230817	826760.360721	41.717287
3529.578988	826201.070929	41.722292
3529.248011	825650.253778	41.727296
3529.549808	825088.237826	41.732301
3529.212445	824543.827957	41.737306
3529.126114	823984.666893	41.742311
3529.312804	823419.985693	41.747316
3529.253510	822871.576629	41.752320
3529.294047	822307.411261	41.757325
3529.189212	821756.325736	41.762330
3529.238412	821204.238712	41.767335
3529.295165	820649.218944	41.772340
3529.025239	820093.963716	41.777344
3529.329718	819531.814178	41.782349
3529.242066	818976.629588	41.787354
3529.188021	818408.820733	41.792359
3529.096954	817853.249060	41.797364
3529.274987	817298.416680	41.802368
3529.258026	816736.280613	41.807373
3529.105647	816181.313545	41.812378
3528.943421	815613.773594	41.817383
3529.212771	815054.774548	41.822388
3529.025522	814511.078080	41.827392
3529.138138	813943.104433	41.832397
3529.057641	813387.892829	41.837402
3529.148140	812823.646495	41.842407
3528.860214	812268.524466	41.847412
3528.968519	811707.412825	41.852416
3528.827215	811145.170627	41.857421
3528.853240	810603.667459	41.862426
3528.926919	810034.145418	41.867431
3529.100426	809485.523226	41.872436
3528.626934	808922.907524	41.877440
3528.781262	808365.379938	41.882445
3528.686854	807819.803836	41.887450
3528.928094	807257.907690	41.892455
3528.687059	806703.103889	41.897460
3528.434639	806147.227576	41.902464
3528.478155	805589.049804	41.907469
3528.411031	805042.069757	41.912474
3528.337683	804484.556732	41.917479
3528.368879	803936.539930	41.922484
3528.198991	803399.299550	41.927488
3528.900988	802843.922730	41.932493
3528.521248	802286.233822	41.937498
3528.540231	801728.578629	41.942503
3528.772619	801176.825014	41.947508
3528.437996	800623.113007	41.952512
3528.287290	800056.817033	41.957517
3528.077421	799506.525679	41.962522
3528.019438	798954.545578	41.967527
3528.297126	798408.449766	41.972532
3528.090415	797858.615415	41.977536
3528.193275	797301.520253	41.982541
3528.029616	796765.331626	41.987546
3527.927807	796201.214505	41.992551
3528.366058	795658.604763	41.997556
3528.156018	795111.203878	42.002560
3528.496726	794545.551729	42.007565
3528.358616	794002.076903	42.012570
3527.775066	793450.829286	42.017575
3528.245517	792897.394215	42.022580
3527.770708	792347.317761	42.027584
3527.966256	791788.882424	42.032589
3527.879855	791251.176635	42.037594
3528.008556	790698.461402	42.042599
3527.695234	790148.185150	42.047604
3527.762217	789610.769929	42.052608
3527.701439	789055.845832	42.057613
3527.675258	788511.337429	42.062618
3527.739044	787968.294961	42.067623
3527.779995	787421.234412	42.072628
3527.456046	786874.636231	42.077632
3527.523014	786320.557087	42.082637
3527.267790	785779.465693	42.087642
3527.552125	785240.649627	42.092647
3527.810736	784691.719659	42.097652
3527.123829	784148.218414	42.102656
3527.621149	783598.573666	42.107661
3527.376141	783060.666698	42.112666
3527.315725	782519.934061	42.117671
3527.544388	781977.439240	42.122676
3527.184480	781438.544926	42.127680
3527.556675	780893.583017	42.132685
3527.557788	780348.643176	42.137690
3527.231041	779798.454488	42.142695
3527.214513	779257.665688	42.147700
3527.053820	778720.304964	42.152704
3527.458881	778172.671807	42.157709
3527.098735	777642.005871	42.162714
3527.236521	777090.596776	42.167719
3527.577507	776555.942418	42.172724
3526.960372	776018.360755	42.177728
3526.907043	775471.487848	42.182733
3526.835567	774935.751119	42.187738
3526.861572	774392.377107	42.192743
3527.005757	773862.038343	42.197748
3526.442838	773325.774987	42.202752
3526.972432	772784.164859	42.207757
3526.896863	772254.633402	42.212762
3526.810469	771713.689498	42.217767
3527.223544	771185.327130	42.222772
3527.301123	770646.936223	42.227776
3526.888774	770100.166486	42.232781
3526.900621	769562.544906	42.237786
3526.710517	769017.085485	42.242791
3527.183364	768481.277073	42.247796
3526.803589	767939.810559	42.252800
3526.975546	767393.578326	42.257805
3526.919951	766859.319608	42.262810
3527.132279	766320.639798	42.267815
3527.007265	765772.121221	42.272820
3526.690624	765226.305888	42.277824
3526.897232	764687.459547	42.282829
3526.601577	764160.244904	42.287834
3526.764083	763611.321061	42.292839
3526.814663	763080.470775	42.297844
3526.163991	762551.231111	42.302848
3526.556554	762014.675134	42.307853
3526.174500	761474.070592	42.312858
3526.517443	760941.687527	42.317863
3526.710850	760413.681979	42.322868
3526.374521	759874.483671	42.327872
3526.433169	759338.287105	42.332877
3526.293186	758800.359743	42.337882
3526.341108	758260.783279	42.342887
3526.484492	757724.803184	42.347892
3525.997011	757198.662789	42.352896
3526.206483	756657.118903	42.357901
3526.132175	756127.675592	42.362906
3525.883490	755609.823215	42.367911
3526.007725	755076.028493	42.372916
3525.886777	754548.210839	42.377920
3526.027724	754020.509442	42.382925
3525.795910	753499.351685	42.387930
3525.853564	752968.926160	42.392935
3525.917042	752435.895499	42.397940
3525.957842	751911.373919	42.402944
3526.139725	751390.693497	42.407949
3526.126558	750856.973811	42.412954
3525.856278	750321.137378	42.417959
3525.977540	749797.742087	42.422964
3525.712796	749269.882362	42.427968
3526.057328	748746.871703	42.432973
3525.688893	748219.056755	42.437978
3525.886194	747692.690196	42.442983
3525.926267	747164.042032	42.447988
3525.322215	746642.780644	42.452992
3525.813887	746117.047641	42.457997
3525.546882	745601.786319	42.463002
3525.599827	745075.563780	42.468007
3525.705916	744547.023191	42.473012
3525.339976	744024.607006	42.478016
3525.727653	743499.704044	42.483021
3525.323562	742982.415046	42.488026
3525.368154	742461.653604	42.493031
3525.712117	741941.795336	42.498036
3525.221251	741419.869704	42.503040
3525.290418	740896.231552	42.508045
3524.824535	740383.578467	42.513050
3524.693294	739864.851077	42.518055
3525.007608	739351.305437	42.523060
3525.045355	738844.846445	42.528064
3525.065482	738322.876149	42.533069
3524.878795	737814.213244	42.538074
3524.513392	737302.134870	42.543079
3525.244748	736787.560530	42.548084
3524.827631	736283.489451	42.553088
3524.943168	735774.347656	42.558093
3524.737580	735264.881824	42.563098
3524.906410	734745.669948	42.568103
3525.293090	734235.691021	42.573108
3524.826408	733722.311405	42.578112
3524.749107	733211.851619	42.583117
3524.285270	732694.495650	42.588122
3524.403130	732189.035839	42.593127
3524.695457	731677.722508	42.598132
3524.496590	731179.679049	42.603136
3524.840309	730669.679230	42.608141
3524.678685	730164.288731	42.613146
3524.301942	729660.586934	42.618151
3524.462069	729152.602488	42.623156
3524.004208	728645.186943	42.628160
3524.322464	728136.468075	42.633165
3524.340318	727642.825451	42.638170
3524.197419	727139.174871	42.643175
3524.526479	726634.372340	42.648180
3524.384620	726137.000140	42.653184
3524.179609	725629.303875	42.658189
3523.982481	725137.478407	42.663194
3524.083725	724626.447251	42.668199
3524.315330	724127.303587	42.673204
3523.805394	723631.080694	42.678208
3524.278099	723130.794678	42.683213
3524.293056	722632.390081	42.688218
3524.218691	722119.795762	42.693223
3524.085567	721616.398764	42.698228
3523.772531	721126.137386	42.703232
3524.111979	720625.226428	42.708237
3523.913963	720128.541150	42.713242
3524.097301	719626.951999	42.718247
3523.922165	719139.771981	42.723252
3523.911408	718640.089962	42.728256
3523.962910	718134.416953	42.733261
3524.024770	717644.133681	42.738266
3523.829908	717144.641288	42.743271
3523.712790	716637.616876	42.748276
3523.685742	716156.734057	42.753280
3523.961373	715665.157357	42.758285
3523.985375	715168.435983	42.763290
3523.674380	714670.849462	42.768295
3523.961623	714173.131319	42.773300
3523.794395	713676.602392	42.778304
3523.578195	713183.277541	42.783309
3523.907355	712693.700937	42.788314
3523.348493	712194.769879	42.793319
3523.507186	711696.828201	42.798324
3523.391676	711214.536555	42.803329
3523.259043	710718.274365	42.808333
3523.299235	710224.187101	42.813338
3523.448112	709739.483309	42.818343
3523.395767	709254.736594	42.823348
3523.403488	708771.242687	42.828353
3523.246618	708278.664565	42.833357
3523.227833	707789.857245	42.838362
3523.537382	707307.420377	42.843367
3523.551040	706807.082200	42.848372
3523.704019	706322.382162	42.853377
3523.554225	705826.284987	42.858381
3523.478050	705338.390334	42.863386
3523.238232	704844.883879	42.868391
3523.468490	704357.278557	42.873396
3523.170383	703868.990799	42.878401
3522.864050	703381.719919	42.883405
3523.142877	702896.755731	42.888410
3523.110878	702417.182642	42.893415
3522.934002	701934.974636	42.898420
3522.764387	701454.527168	42.903425
3522.992984	700963.550981	42.908429
3522.927700	700481.740031	42.913434
3522.991431	699990.935826	42.918439
3523.164619	699513.900401	42.923444
3522.842959	699034.488193	42.928449
3523.019239	698549.497633	42.933453
3522.456933	698064.357746	42.938458
3522.757845	697590.426174	42.943463
3522.766874	697110.205854	42.948468
3522.662236	696638.628368	42.953473
3522.538600	696149.380446	42.958477
3522.742401	695683.217266	42.963482
3522.405360	695203.896479	42.968487
3522.317729	694725.203151	42.973492
3522.444352	694254.602093	42.978497
3522.490699	693780.657968	42.983501
3522.618595	693315.327508	42.988506
3522.619055	692836.317966	42.993511
3522.332999	692354.347363	42.998516
3522.327661	691876.928286	43.003521
3522.396426	691403.698859	43.008525
3522.215693	690939.142157	43.013530
3522.260312	690466.513722	43.018535
3522.125160	689986.876435	43.023540
3522.122399	689524.205616	43.028545
3522.103928	689051.314082	43.033549
3522.004987	688588.462051	43.038554
3522.058168	688129.690123	43.043559
3522.185931	687659.984315	43.048564
3522.047280	687186.965269	43.053569
3522.255309	686719.635078	43.058573
3522.071473	686257.175145	43.063578
3521.833701	685796.940426	43.068583
3521.932919	685319.452652	43.073588
3521.713067	684865.438971	43.078593
3521.663227	684404.752865	43.083597
3521.908621	683943.295996	43.088602
3521.705641	683479.751491	43.093607
3522.023073	683011.215381	43.098612
3521.854890	682565.939872	43.103617
3521.761244	682095.733987	43.108621
3521.649544	681635.216837	43.113626
3521.345764	681180.137103	43.118631
3521.621719	680716.868243	43.123636
3521.180098	680270.431853	43.128641
3521.287121	679811.877217	43.133645
3521.195630	679365.237356	43.138650
3521.264594	678906.444759	43.143655
3521.183997	678445.263844	43.148660
3521.035220	678002.004546	43.153665
3521.057805	677552.965778	43.158669
3521.396119	677111.672822	43.163674
3521.040873	676651.495285	43.168679
3521.266076	676201.658748	43.173684
3521.018108	675760.501073	43.178689
3521.427448	675308.098419	43.183693
3521.358311	674853.114366	43.188698
3521.252525	674407.532812	43.193703
3521.312059	673956.818442	43.198708
3520.895303	673502.176521	43.203713
3521.092297	673046.012111	43.208717
3520.769575	672594.798772	43.213722
3520.420253	672160.665181	43.218727
3520.564329	671713.367104	43.223732
3520.519118	671277.096874	43.228737
3520.818532	670838.803275	43.233741
3521.041495	670398.906930	43.238746
3520.684302	669959.039201	43.243751
3520.881647	669505.943205	43.248756
3521.004283	669077.719236	43.253761
3520.551750	668625.290227	43.258765
3520.595421	668192.402224	43.263770
3521.047670	667750.548024	43.268775
3520.703250	667304.420572	43.273780
3520.668214	666857.321582	43.278785
3520.422484	666419.015643	43.283789
3520.716242	665979.150919	43.288794
3520.561418	665539.192810	43.293799
3520.721842	665098.861266	43.298804
3520.406319	664665.225350	43.303809
3520.796084	664216.632819	43.308813
3520.886043	663779.694704	43.313818
3520.559012	663347.797019	43.318823
3520.823662	662898.715068	43.323828
3520.449704	662461.047623	43.328833
3520.567979	662022.427917	43.333837
3520.312463	661591.436970	43.338842
3520.259270	661158.445963	43.343847
3520.352951	660722.416108	43.348852
3520.086790	660299.054625	43.353857
3520.138441	659850.815129	43.358861
3520.050593	659418.650409	43.363866
3519.831395	658989.234122	43.368871
3520.135452	658566.148720	43.373876
3520.042971	658145.259088	43.378881
3520.169115	657715.328145	43.383885
3520.314485	657284.725927	43.388890
3519.863354	656858.350317	43.393895
3520.143620	656422.245113	43.398900
3519.778034	655998.413557	43.403905
3519.610277	655571.533935	43.408909
3520.070389	655144.578435	43.413914
3520.097786	654715.431085	43.418919
3520.031373	654280.238430	43.423924
3519.628170	653863.362260	43.428929
3519.872068	653437.218420	43.433933
3519.736536	653018.762484	43.438938
3519.364958	652601.078286	43.443943
3519.545423	652173.242386	43.448948
3519.578125	651761.247739	43.453953
3519.469047	651341.966953	43.458957
3519.791051	650920.147001	43.463962
3519.708771	650500.826050	43.468967
3519.839936	650076.704773	43.473972
3519.715030	649650.660605	43.478977
3519.604998	649220.398676	43.483981
3519.400492	648811.269956	43.488986
3519.066250	648398.199117	43.493991
3519.403519	647973.203568	43.498996
3518.981342	647567.109206	43.504001
3519.068527	647156.963428	43.509005
3519.129470	646736.860039	43.514010
3519.067114	646329.554597	43.519015
3519.248878	645921.341289	43.524020
3519.146668	645513.909629	43.529025
3518.989931	645103.721634	43.534029
3519.223130	644695.099925	43.539034
3518.850801	644287.414854	43.544039
3518.852538	643872.300837	43.549044
3518.844482	643478.568299	43.554049
3518.633555	643063.157435	43.559053
3518.751597	642666.122135	43.564058
3518.814285	642259.081036	43.569063
3518.988174	641863.454773	43.574068
3518.803206	641460.724029	43.579073
3518.679337	641046.865917	43.584077
3518.754521	640654.909879	43.589082
3518.893747	640256.526777	43.594087
3519.086704	639852.617825	43.599092
3518.819914	639450.221773	43.604097
3518.616986	639045.598370	43.609101
3519.080847	638640.094909	43.614106
3518.640322	638234.029578	43.619111
3518.713190	637825.959772	43.624116
3518.882434	637431.813527	43.629121
3519.268159	637029.561354	43.634125
3518.931324	636617.511680	43.639130
3518.771295	636218.872929	43.644135
3518.802573	635808.729257	43.649140
3518.268544	635411.223876	43.654145
3518.506108	635012.670889	43.659149
3518.327204	634622.029313	43.664154
3518.073963	634223.980146	43.669159
3518.347703	633822.623224	43.674164
3518.424408	633436.547131	43.679169
3518.620944	633040.627768	43.684173
3518.539089	632642.939276	43.689178
3518.208033	632255.838135	43.694183
3518.445345	631857.014239	43.699188
3518.238335	631464.807679	43.704193
3518.243633	631054.130733	43.709197
3518.158618	630659.270451	43.714202
3518.125690	630272.495603	43.719207
3518.296271	629873.057036	43.724212
3518.158092	629487.773057	43.729217
3517.982223	629087.312567	43.734221
3517.888577	628703.243866	43.739226
3517.955663	628322.588301	43.744231
3518.205755	627926.316722	43.749236
3517.869113	627544.750806	43.754241
3517.980160	627160.941643	43.759245
3517.792142	626774.315480	43.764250
3517.438386	626385.650459	43.769255
3517.609972	625999.735914	43.774260
3517.580421	625629.766724	43.779265
3517.574452	625251.867966	43.784269
3517.749415	624874.575997	43.789274
3517.734760	624490.541744	43.794279
3517.826988	624102.869273	43.799284
3517.455980	623724.978833	43.804289
3517.568610	623344.988918	43.809293
3517.426604	622973.694769	43.814298
3517.443379	622604.514660	43.819303
3517.946185	622223.717159	43.824308
3517.445416	621849.139180	43.829313
3517.623028	621464.563041	43.834317
3517.567139	621091.986913	43.839322
3517.234793	620716.689545	43.844327
3517.541432	620330.898669	43.849332
3517.576102	619960.773257	43.854337
3517.620464	619585.773193	43.859341
3517.630337	619208.410953	43.864346
3517.904639	618820.918290	43.869351
3517.886749	618444.736915	43.874356
3517.479532	618079.533799	43.879361
3517.144946	617695.212060	43.884365
3517.549395	617318.869590	43.889370
3517.380958	616951.984197	43.894375
3517.518397	616566.790368	43.899380
3517.334353	616200.985102	43.904385
3517.229993	615826.632936	43.909389
3517.265021	615452.043691	43.914394
3517.038636	615084.002866	43.919399
3517.080189	614708.685379	43.924404
3516.793531	614350.856647	43.929409
3516.803511	613986.749228	43.934413
3516.899905	613623.517449	43.939418
3516.576863	613262.601439	43.944423
3516.840162	612896.359250	43.949428
3516.635933	612538.908951	43.954433
3516.510090	612179.779092	43.959437
3516.501660	611826.233484	43.964442
3516.287165	611463.736055	43.969447
3516.733478	611107.031145	43.974452
3516.467450	610758.510094	43.979457
3516.470682	610400.052888	43.984461
3516.791708	610044.789666	43.989466
3515.991324	609694.471021	43.994471
3516.503884	609338.450505	43.999476
3516.449822	608987.982297	44.004481
3516.458827	608632.225913	44.009485
3516.374225	608274.066629	44.014490
3516.033114	607931.388904	44.019495
3516.248167	607579.376099	44.024500
3516.443116	607234.930296	44.029505
3516.073572	606871.558034	44.034509
3516.197392	606525.647918	44.039514
3515.905239	606182.055754	44.044519
3515.988266	605824.692932	44.049524
3515.789823	605500.027921	44.054529
3516.015449	605145.077639	44.059533
3516.371102	604804.393522	44.064538
3515.786710	604464.361422	44.069543
3516.198937	604115.468423	44.074548
3515.890090	603776.572926	44.079553
3516.061842	603427.047551	44.084557
3516.537621	603085.538718	44.089562
3516.364527	602743.728983	44.094567
3516.534080	602388.049851	44.099572
3516.389112	602044.508121	44.104577
3516.142004	601688.928563	44.109581
3516.579913	601342.004056	44.114586
3516.349793	600987.503982	44.119591
3516.323001	600641.189716	44.124596
3515.765589	600302.484611	44.129601
3515.408007	599956.005400	44.134605
3515.676139	599620.703112	44.139610
3515.521700	599277.782951	44.144615
3515.658637	598949.611643	44.149620
3515.889218	598619.858801	44.154625
3515.924358	598268.994810	44.159629
3515.715140	597932.218941	44.164634
3515.449694	597601.166266	44.169639
3515.679117	597256.815320	44.174644
3515.311837	596932.890299	44.179649
3515.266056	596603.579159	44.184653
3515.541929	596272.245558	44.189658
3515.341807	595950.473919	44.194663
3515.502344	595614.672424	44.199668
3514.961334	595288.421487	44.204673
3515.302379	594960.052396	44.209677
3515.275585	594631.736890	44.214682
3515.082267	594307.508372	44.219687
3515.313993	593974.711013	44.224692
3515.095305	593655.892643	44.229697
3515.250392	593336.198225	44.234701
3515.307988	593010.183429	44.239706
3515.069326	592678.132807	44.244711
3514.973994	592347.052905	44.249716
3514.889172	592040.272764	44.254721
3514.994680	591712.305184	44.259725
3515.187188	591383.660636	44.264730
3514.961402	591057.941664	44.269735
3515.200070	590747.003846	44.274740
3514.892871	590427.560748	44.279745
3514.750723	590112.803160	44.284749
3514.717553	589790.884755	44.289754
3514.733744	589473.973192	44.294759
3514.846649	589156.383543	44.299764
3514.492846	588845.748335	44.304769
3514.633535	588538.386941	44.309773
3514.898031	588223.962181	44.314778
3514.370152	587924.286141	44.319783
3514.647395	587591.854362	44.324788
3514.398980	587280.155494	44.329793
3514.434722	586975.485307	44.334797
3514.781312	586668.794496	44.339802
3514.455908	586366.482085	44.344807
3514.368495	586045.979664	44.349812
3514.472020	585738.351785	44.354817
3514.292169	585427.749023	44.359821
3514.204487	585125.314592	44.364826
3514.064736	584820.016688	44.369831
3514.254496	584513.850639	44.374836
3514.384127	584220.302837	44.379841
3514.029929	583924.015791	44.384845
3514.172842	583611.652561	44.389850
3514.270609	583323.215431	44.394855
3514.364629	583008.080405	44.399860
3514.334541	582706.028117	44.404865
3514.684989	582402.646623	44.409869
3514.453278	582097.044517	44.414874
3514.083110	581796.837479	44.419879
3514.352639	581489.827505	44.424884
3514.045034	581195.879142	44.429889
3514.119985	580891.652450	44.434893
3514.350745	580596.290591	44.439898
3514.247057	580292.280611	44.444903
3514.215721	579991.468614	44.449908
3513.854924	579693.420642	44.454913
3514.156503	579392.788540	44.459917
3514.020160	579096.397344	44.464922
3513.759123	578799.919731	44.469927
3514.129542	578498.650629	44.474932
3514.132512	578207.997094	44.479937
3513.791255	577904.873826	44.484941
3513.500204	577614.306803	44.489946
3513.856463	577322.063438	44.494951
3513.689887	577029.952735	44.499956
3513.659757	576743.997832	44.504961
3513.554859	576451.963564	44.509965
3513.764570	576159.717826	44.514970
3513.580613	575870.399307	44.519975
3513.900302	575575.354776	44.524980
3513.753930	575285.664166	44.529985
3513.576183	575008.194976	44.534989
3513.595463	574707.547644	44.539994
3513.361072	574430.880102	44.544999
3513.693784	574136.050823	44.550004
3513.455151	573861.232614	44.555009
3513.279667	573572.815160	44.560013
3513.430660	573292.686201	44.565018
3513.645749	573012.238201	44.570023
3513.607994	572725.085741	44.575028
3513.642588	572432.631833	44.580033
3513.299160	572152.763117	44.585037
3513.457979	571859.469707	44.590042
3513.184630	571580.029113	44.595047
3513.343473	571297.489673	44.600052
3513.143838	571030.955138	44.605057
3513.102893	570748.638800	44.610061
3513.465447	570460.913592	44.615066
3512.974608	570187.920026	44.620071
3512.939536	569917.308438	44.625076
3513.013906	569638.168146	44.630081
3512.923718	569360.811089	44.635085
3513.053154	569082.605312	44.640090
3512.945404	568824.664308	44.645095
3513.177314	568532.136919	44.650100
3513.007955	568270.420810	44.655105
3512.536298	567997.477592	44.660109
3512.782542	567729.992436	44.665114
3512.384929	567463.567878	44.670119
3512.698525	567198.677251	44.675124
3513.024529	566931.010788	44.680129
3513.344160	566663.843153	44.685133
3513.194474	566393.579058	44.690138
3512.740679	566117.774026	44.695143
3512.831560	565836.182113	44.700148
3512.723840	565578.528039	44.705153
3512.420900	565313.200425	44.710157
3512.735323	565045.748378	44.715162
3512.379954	564786.610583	44.720167
3512.743992	564527.042709	44.725172
3512.534525	564272.803121	44.730177
3512.515229	564003.473479	44.735181
3512.666076	563731.088535	44.740186
3512.251202	563475.458721	44.745191
3512.607289	563211.586499	44.750196
3512.778161	562957.910676	44.755201
3512.419337	562698.127513	44.760205
3512.782644	562426.585196	44.765210
3512.388679	562166.092520	44.770215
3512.564968	561898.649498	44.775220
3512.574838	561643.666423	44.780225
3512.539655	561377.809752	44.785229
3512.595893	561114.701551	44.790234
3512.368656	560864.829542	44.795239
3512.769782	560584.379924	44.800244
3512.531346	560333.492561	44.805249
3512.369863	560068.033709	44.810253
3512.536544	559809.916279	44.815258
3512.383144	559560.661480	44.820263
3512.172878	559290.310292	44.825268
3512.558445	559041.608332	44.830273
3512.459123	558781.048381	44.835277
3512.324359	558518.273304	44.840282
3512.055482	558271.985322	44.845287
3512.347285	558002.176743	44.850292
3512.156800	557753.196295	44.855297
3511.968378	557504.361913	44.860301
3512.394757	557258.893350	44.865306
3512.010524	557009.176456	44.870311
3512.338883	556743.818931	44.875316
3512.466613	556497.631712	44.880321
3513.113061	556234.929801	44.885325
3512.646036	555972.009827	44.890330
3512.465439	555725.054971	44.895335
3512.480244	555463.251681	44.900340
3512.436921	555206.138223	44.905345
3512.134730	554944.933031	44.910349
3512.563039	554691.305962	44.915354
3512.322927	554437.737830	44.920359
3512.047186	554186.488488	44.925364
3511.760295	553932.515729	44.930369
3511.714598	553680.310751	44.935373
3511.625504	553427.806141	44.940378
3511.711679	553186.704129	44.945383
3512.081700	552946.506651	44.950388
3511.940845	552696.566798	44.955393
3511.867884	552460.819895	44.960397
3511.858955	552202.282532	44.965402
3512.145048	551957.798775	44.970407
3511.923288	551703.571265	44.975412
3511.726663	551469.138294	44.980417
3511.973263	551227.268392	44.985421
3512.224287	550980.656507	44.990426
3512.055979	550731.440872	44.995431
3511.702512	550489.408288	45.000436
3511.489965	550239.536041	45.005441
3511.232415	550001.610808	45.010445
3511.313320	549759.339863	45.015450
3511.199462	549530.302151	45.020455
3511.180980	549294.742846	45.025460
3510.937740	549068.491402	45.030465
3510.977155	548835.131862	45.035469
3511.430068	548596.859193	45.040474
3511.360809	548375.455504	45.045479
3511.088321	548139.566825	45.050484
3511.294930	547910.548035	45.055489
3511.063313	547683.364410	45.060493
3511.512677	547451.120992	45.065498
3511.379503	547222.904819	45.070503
3511.321233	546989.429697	45.075508
3510.822479	546759.907251	45.080513
3510.677174	546534.050898	45.085517
3511.070305	546310.821041	45.090522
3510.796274	546093.952406	45.095527
3510.759440	545868.873201	45.100532
3510.941975	545645.265239	45.105537
3510.875662	545419.074665	45.110541
3511.018342	545193.399260	45.115546
3511.324440	544981.707575	45.120551
3510.767083	544744.196074	45.125556
3510.750314	544534.821388	45.130561
3510.582988	544308.982841	45.135565
3510.939888	544091.924677	45.140570
3510.869470	543880.129215	45.145575
3510.734305	543657.551803	45.150580
3510.816073	543432.614454	45.155585
3510.660272	543212.856994	45.160589
3510.840943	542988.803175	45.165594
3510.914325	542779.840476	45.170599
3511.123828	542552.648524	45.175604
3510.882846	542335.412964	45.180609
3510.750802	542113.667593	45.185613
3511.338522	541879.744016	45.190618
3510.670308	541671.244351	45.195623
3510.501290	541444.048602	45.200628
3510.274382	541228.709714	45.205633
3510.211009	541012.129301	45.210637
3510.315435	540806.813183	45.215642
3510.268076	540597.687261	45.220647
3510.433848	540383.781296	45.225652
3510.401517	540185.237257	45.230657
3510.304991	539964.611818	45.235661
3510.544946	539752.095721	45.240666
3510.167924	539546.439969	45.245671
3510.407640	539339.515913	45.250676
3510.348596	539128.151053	45.255681
3510.496672	538921.438272	45.260685
3510.763224	538714.399621	45.265690
3510.455773	538509.927415	45.270695
3510.629427	538291.600330	45.275700
3510.247247	538082.645669	45.280705
3510.190973	537879.836440	45.285709
3510.166905	537669.755316	45.290714
3510.090930	537465.732959	45.295719
3510.088343	537259.072141	45.300724
3510.066016	537053.874548	45.305729
3510.111370	536852.395294	45.310733
3510.476278	536652.624197	45.315738
3510.332579	536456.720543	45.320743
3510.076050	536246.052785	45.325748
3510.067758	536042.805661	45.330753
3509.662614	535840.531463	45.335757
3510.213536	535641.420748	45.340762
3509.652869	535440.025067	45.345767
3509.892479	535239.145761	45.350772
3510.012444	535045.599363	45.355777
3509.772606	534848.882931	45.360781
3510.033718	534649.101625	45.365786
3509.784293	534466.911673	45.370791
3509.729828	534265.614905	45.375796
3510.061199	534068.588465	45.380801
3509.647259	533884.552449	45.385805
3509.967422	533673.445760	45.390810
3509.733957	533475.902207	45.395815
3509.875619	533291.006924	45.400820
3509.829198	533099.430601	45.405825
3509.774883	532896.601008	45.410829
3509.805634	532695.015512	45.415834
3509.533386	532511.442405	45.420839
3509.850351	532311.720158	45.425844
3509.713076	532120.802388	45.430849
3509.219490	531934.837674	45.435853
3509.558561	531740.200368	45.440858
3509.691614	531558.867260	45.445863
3509.933564	531366.865592	45.450868
3509.209025	531172.149977	45.455873
3509.418662	530992.159261	45.460877
3509.543042	530801.078573	45.465882
3509.636533	530615.602352	45.470887
3509.396189	530428.162122	45.475892
3509.465396	530241.877842	45.480897
3509.335532	530057.391547	45.485901
3509.796197	529868.159018	45.490906
3509.665434	529686.343020	45.495911
3509.518115	529492.011146	45.500916
3509.435005	529309.273884	45.505921
3509.291282	529119.630190	45.510925
3509.420879	528933.722744	45.515930
3509.278901	528760.073566	45.520935
3509.424541	528580.266034	45.525940
3509.612680	528394.594144	45.530945
3509.330292	528212.987696	45.535949
3509.601145	528033.101634	45.540954
3509.214505	527843.684876	45.545959
3509.269222	527651.565583	45.550964
3509.135192	527484.512360	45.555969
3509.202514	527298.796836	45.560973
3509.310469	527116.908351	45.565978
3509.066744	526948.656340	45.570983
3508.884234	526764.491118	45.575988
3508.909140	526595.633964	45.580993
3509.125281	526418.211104	45.585997
3509.070121	526235.632935	45.591002
3509.255227	526069.266477	45.596007
3509.269490	525889.398189	45.601012
3509.648253	525709.162596	45.606017
3509.397649	525520.601601	45.611021
3509.218152	525331.218337	45.616026
3508.810080	525174.282651	45.621031
3509.020660	524994.168096	45.626036
3509.530673	524816.474034	45.631041
3508.815832	524652.214348	45.636045
3508.992308	524469.171095	45.641050
3508.705621	524296.049704	45.646055
3508.853038	524117.147061	45.651060
3508.814344	523956.702342	45.656065
3508.887727	523789.269291	45.661069
3509.019922	523611.524459	45.666074
3509.247196	523445.676966	45.671079
3509.229528	523270.377210	45.676084
3509.200646	523092.451775	45.681089
3509.270348	522919.152659	45.686093
3509.113005	522736.094767	45.691098
3508.946084	522560.357787	45.696103
3508.838292	522393.445056	45.701108
3508.833016	522212.122112	45.706113
3508.610463	522045.477595	45.711117
3508.966465	521875.854217	45.716122
3508.539343	521708.230999	45.721127
3508.578859	521547.646253	45.726132
3509.020590	521378.911602	45.731137
3508.363756	521221.270124	45.736141
3508.701408	521043.156950	45.741146
3508.614561	520889.303055	45.746151
3508.722858	520717.032560	45.751156
3508.917166	520557.319878	45.756161
3508.609257	520393.802741	45.761165
3508.985328	520222.541425	45.766170
3508.416955	520064.266806	45.771175
3508.781947	519896.387307	45.776180
3508.599639	519729.255938	45.781185
3508.570646	519572.752707	45.786189
3509.012072	519404.804240	45.791194
3508.750678	519244.701063	45.796199
3508.914055	519071.695487	45.801204
3509.190055	518904.274810	45.806209
3509.088918	518736.108599	45.811213
3508.987291	518559.859600	45.816218
3508.793455	518386.654734	45.821223
3508.353302	518230.612016	45.826228
3508.455271	518072.505333	45.831233
3508.260208	517912.932480	45.836237
3508.288494	517741.248160	45.841242
3508.071321	517599.808585	45.846247
3508.177984	517439.169099	45.851252
3508.377578	517284.522831	45.856257
3507.950261	517124.728893	45.861261
3508.255312	516967.889460	45.866266
3508.292436	516820.085339	45.871271
3507.943799	516676.437188	45.876276
3508.128382	516513.148084	45.881281
3508.117962	516366.105427	45.886285
3508.424069	516207.338565	45.891290
3508.238444	516061.585779	45.896295
3507.996115	515903.010461	45.901300
3508.296284	515755.201751	45.906305
3507.923252	515605.687995	45.911309
3508.154511	515452.432421	45.916314
3508.146103	515312.805348	45.921319
3508.088097	515148.280334	45.926324
3508.255080	514995.637434	45.931329
3508.224187	514853.787273	45.936333
3508.347991	514702.159233	45.941338
3507.939513	514545.215006	45.946343
3507.860619	514395.993008	45.951348
3508.134122	514252.620309	45.956353
3507.731485	514097.943995	45.961357
3507.937578	513936.392326	45.966362
3507.951772	513791.291405	45.971367
3508.151924	513652.472692	45.976372
3508.007037	513507.446817	45.981377
3507.636476	513370.541867	45.986381
3507.879157	513221.556865	45.991386
3507.832481	513076.813369	45.996391
3507.815751	512932.467618	46.001396
3508.151701	512787.656117	46.006401
3507.882160	512644.816112	46.011405
3507.838922	512489.304621	46.016410
3507.555882	512348.283162	46.021415
3507.821755	512206.661441	46.026420
3507.525420	512071.399854	46.031425
3507.573870	511932.591800	46.036429
3507.979222	511779.725200	46.041434
3507.933860	511642.800161	46.046439
3507.750165	511500.996201	46.051444
3507.907890	511359.435847	46.056449
3507.367956	511227.745685	46.061453
3507.492840	511077.749855	46.066458
3507.309439	510944.328934	46.071463
3507.357770	510814.202404	46.076468
3507.324522	510680.500958	46.081473
3507.270090	510553.068018	46.086477
3507.447987	510412.657975	46.091482
3507.338144	510285.485005	46.096487
3507.271303	510151.026819	46.101492
3507.420734	510004.705575	46.106497
3507.309651	509876.468313	46.111501
3507.351618	509744.868573	46.116506
3507.294947	509618.540264	46.121511
3507.104386	509484.855583	46.126516
3507.091243	509353.059860	46.131521
3507.025592	509232.491143	46.136525
3507.325532	509094.828109	46.141530
3506.991008	508974.606567	46.146535
3507.257543	508844.729838	46.151540
3507.725669	508715.424088	46.156545
3507.536306	508593.001733	46.161549
3507.267962	508453.914030	46.166554
3507.502417	508327.525761	46.171559
3507.401508	508192.703048	46.176564
3507.505420	508055.519368	46.181569
3507.245269	507930.829701	46.186573
3507.250830	507792.599200	46.191578
3507.113999	507669.048881	46.196583
3507.125627	507539.609390	46.201588
3507.436700	507406.327043	46.206593
3507.115877	507282.350273	46.211597
3507.124671	507157.204312	46.216602
3506.827359	507037.163998	46.221607
3507.008670	506909.560556	46.226612
3507.392696	506784.094897	46.231617
3507.222888	506670.297568	46.236621
3507.405094	506533.491843	46.241626
3507.499444	506404.585066	46.246631
3507.361016	506274.301713	46.251636
3507.634144	506142.279004	46.256641
3507.555074	506013.600890	46.261645
3507.609393	505888.133993	46.266650
3506.937317	505760.515505	46.271655
3507.018327	505630.897145	46.276660
3506.827550	505505.064731	46.281665
3507.094796	505390.779346	46.286669
3507.134543	505250.448641	46.291674
3506.943106	505139.019997	46.296679
3506.790469	505021.113574	46.301684
3507.363925	504890.444744	46.306689
3506.813628	504775.131941	46.311693
3507.200586	504654.047121	46.316698
3506.752348	504543.315385	46.321703
3506.517787	504422.688815	46.326708
3506.939520	504302.202051	46.331713
3506.648025	504190.682860	46.336717
3506.930804	504059.399783	46.341722
3506.904055	503944.952184	46.346727
3507.023790	503828.911606	46.351732
3507.003463	503705.715449	46.356737
3506.578763	503592.344394	46.361741
3506.652485	503476.056383	46.366746
3506.917815	503366.306984	46.371751
3506.888378	503247.759979	46.376756
3506.876926	503127.136254	46.381761
3506.563924	503020.415508	46.386765
3506.757865	502894.598267	46.391770
3506.768668	502785.697324	46.396775
3506.907063	502670.808119	46.401780
3507.121259	502554.186207	46.406785
3506.848730	502427.990001	46.411789
3506.731973	502312.282356	46.416794
3506.555545	502209.830449	46.421799
3506.333693	502094.796472	46.426804
3506.527443	501991.824964	46.431809
3506.357175	501889.521678	46.436813
3507.060106	501767.653631	46.441818
3506.963016	501658.763609	46.446823
3506.755144	501534.319086	46.451828
3507.054384	501417.977929	46.456833
3507.064118	501303.505591	46.461837
3506.954153	501179.142782	46.466842
3506.920472	501071.603208	46.471847
3506.483782	500954.828244	46.476852
3506.524075	500841.459846	46.481857
3506.623112	500747.951962	46.486861
3506.848182	500623.679437	46.491866
3506.855168	500508.140200	46.496871
3506.376277	500388.941361	46.501876
3506.629614	500280.032941	46.506881
3506.563710	500174.566159	46.511885
3506.602810	500056.793422	46.516890
3506.433194	499955.792692	46.521895
3506.281175	499845.130256	46.526900
3506.445618	499742.099111	46.531905
3506.186718	499635.144852	46.536909
3506.700166	499519.208822	46.541914
3506.281027	499408.538506	46.546919
3506.083947	499306.324886	46.551924
3506.461067	499207.653478	46.556929
3506.207645	499101.554489	46.561933
3506.415291	498996.488603	46.566938
3506.333650	498902.444876	46.571943
3506.371786	498795.940168	46.576948
3506.347696	498687.928320	46.581953
3506.209322	498597.786399	46.586957
3506.234217	498485.517014	46.591962
3506.484520	498386.761244	46.596967
3505.991193	498288.789277	46.601972
3506.214230	498178.709099	46.606977
3505.905055	498082.221601	46.611981
3506.118522	497974.872558	46.616986
3506.013147	497885.732577	46.621991
3505.998368	497783.883037	46.626996
3506.522588	497683.660309	46.632001
3505.933802	497594.651883	46.637005
3505.952110	497482.882594	46.642010
3506.056411	497387.281363	46.647015
3506.026417	497298.024224	46.652020
3506.008662	497198.396861	46.657025
3505.852360	497109.918893	46.662029
3506.336480	497004.085198	46.667034
3506.129636	496901.302155	46.672039
3506.023017	496813.067008	46.677044
3506.199858	496713.808134	46.682049
3505.836426	496621.721520	46.687053
3505.637499	496515.445033	46.692058
3505.554614	496419.364475	46.697063
3505.678309	496341.455659	46.702068
3505.558933	496251.955322	46.707073
3505.562678	496161.270213	46.712077
3505.438225	496066.712046	46.717082
3505.549812	495995.378749	46.722087
3505.509888	495908.745939	46.727092
3505.333356	495820.517507	46.732097
3505.352557	495747.934482	46.737101
3505.880192	495649.722146	46.742106
3506.021770	495562.044987	46.747111
3505.637286	495463.936728	46.752116
3505.583145	495379.883161	46.757121
3506.017324	495291.193624	46.762125
3506.252065	495193.129797	46.767130
3506.069151	495103.128397	46.772135
3506.190878	495011.203021	46.777140
3506.000452	494914.929911	46.782145
3505.809556	494824.928389	46.787149
3505.691038	494733.801239	46.792154
3505.788087	494653.764749	46.797159
3506.075769	494559.178333	46.802164
3506.212846	494468.511930	46.807169
3506.048760	494383.005290	46.812173
3506.039402	494273.596757	46.817178
3506.039051	494188.465839	46.822183
3505.647928	494087.669814	46.827188
3505.741831	494001.611363	46.832193
3505.573492	493913.068061	46.837197
3505.709630	493825.787495	46.842202
3505.755441	493736.751450	46.847207
3505.635520	493653.307543	46.852212
3505.810062	493567.991894	46.857217
3506.003244	493482.874973	46.862221
3505.559727	493393.465413	46.867226
3505.503721	493312.892286	46.872231
3505.723289	493229.641260	46.877236
3505.663860	493132.678037	46.882241
3505.300212	493050.082161	46.887245
3505.465650	492958.289947	46.892250
3505.666663	492892.037550	46.897255
3505.504215	492805.359182	46.902260
3505.484773	492717.441859	46.907265
3505.774797	492641.207572	46.912269
3505.610445	492548.913000	46.917274
3505.380601	492476.409068	46.922279
3505.190546	492394.943900	46.927284
3505.193441	492309.145369	46.932289
3505.266635	492240.079303	46.937293
3505.384516	492157.902771	46.942298
3505.173259	492073.910240	46.947303
3505.075322	491990.505021	46.952308
3505.412471	491918.711342	46.957313
3505.506390	491851.916707	46.962317
3505.291424	491761.447760	46.967322
3505.142992	491691.456106	46.972327
3505.006406	491614.632407	46.977332
3505.329855	491535.807361	46.982337
3505.258403	491463.272086	46.987341
3505.222621	491382.787576	46.992346
3505.461308	491306.201967	46.997351
3505.176005	491235.017620	47.002356
3505.187559	491156.041717	47.007361
3505.028982	491083.114974	47.012365
3505.155068	491004.523556	47.017370
3505.222743	490934.340134	47.022375
3505.196804	490875.555799	47.027380
3505.457479	490792.134110	47.032385
3504.933956	490719.015168	47.037389
3505.291856	490642.912180	47.042394
3505.232132	490573.204378	47.047399
3505.388639	490500.828489	47.052404
3505.452508	490419.411761	47.057409
3504.838991	490345.345306	47.062413
3505.203930	490264.787139	47.067418
3505.160006	490195.985815	47.072423
3505.044651	490128.511884	47.077428
3505.376668	490049.779754	47.082433
3505.031508	489980.371266	47.087437
3505.230014	489907.125591	47.092442
3504.957236	489839.525621	47.097447
3504.859680	489771.237719	47.102452
3505.103222	489688.926730	47.107457
3504.756522	489623.160001	47.112461
3504.982234	489554.461870	47.117466
3505.218596	489487.279555	47.122471
3504.787871	489417.731623	47.127476
3504.983008	489353.186875	47.132481
3504.865840	489287.480871	47.137485
3504.997517	489223.300657	47.142490
3505.098490	489150.068428	47.147495
3505.037491	489084.908642	47.152500
3505.044524	489013.108620	47.157505
3504.646899	488943.755523	47.162509
3504.961547	488875.646695	47.167514
3505.264570	488817.305168	47.172519
3505.015858	488755.414520	47.177524
3504.916179	488670.728541	47.182529
3504.988124	488609.440413	47.187533
3504.965570	488544.221430	47.192538
3504.940465	488477.636443	47.197543
3504.764946	488401.614672	47.202548
3504.893668	488337.988287	47.207553
3504.721449	488275.273262	47.212557
3504.709699	488206.762139	47.217562
3504.815221	488154.422982	47.222567
3504.647056	488099.296747	47.227572
3504.887426	488030.944287	47.232577
3505.046143	487967.311425	47.237581
3505.001363	487902.751649	47.242586
3504.875133	487837.699523	47.247591
3505.088713	487765.150652	47.252596
3505.155005	487685.947145	47.257601
3505.179630	487628.357596	47.262605
3504.840876	487557.420239	47.267610
3505.188905	487497.902746	47.272615
3505.018649	487434.830139	47.277620
3504.990022	487353.313596	47.282625
3505.439813	487291.298471	47.287629
3505.391551	487221.878851	47.292634
3505.047549	487155.950502	47.297639
3504.775964	487079.028494	47.302644
3505.111829	487006.556798	47.307649
3504.642330	486955.880956	47.312653
3505.147023	486891.426034	47.317658
3504.974405	486825.720197	47.322663
3504.373357	486763.832024	47.327668
3504.679532	486706.596201	47.332673
3504.434919	486650.921786	47.337677
3504.387380	486587.926377	47.342682
3504.602330	486526.049850	47.347687
3504.605203	486474.937719	47.352692
3504.730244	486411.659181	47.357697
3504.818481	486357.394569	47.362701
3504.690176	486289.604308	47.367706
3504.607912	486226.917168	47.372711
3504.453344	486184.535366	47.377716
3504.723845	486115.967849	47.382721
3504.428740	486060.300178	47.387725
3504.433814	486007.162033	47.392730
3504.515337	485938.879126	47.397735
3504.245696	485895.301701	47.402740
3504.498322	485834.529665	47.407745
3504.396249	485781.915208	47.412749
3504.530876	485724.705476	47.417754
3504.544663	485663.923023	47.422759
3504.321481	485616.642589	47.427764
3504.679288	485561.266719	47.432769
3504.299558	485511.229276	47.437773
3504.497496	485465.647827	47.442778
3504.423394	485408.573923	47.447783
3504.336748	485358.739047	47.452788
3504.857504	485295.439533	47.457793
3504.389257	485236.661054	47.462797
3504.913832	485181.306124	47.467802
3505.071579	485128.949009	47.472807
3504.830809	485068.106745	47.477812
3504.705053	485007.244633	47.482817
3504.777155	484953.889423	47.487821
3504.761365	484884.961115	47.492826
3504.901056	484824.002437	47.497831
3504.362589	484771.257032	47.502836
3504.608607	484711.342631	47.507841
3504.658798	484666.341063	47.512845
3504.526179	484595.609582	47.517850
3504.726747	484544.407477	47.522855
3504.807236	484486.190746	47.527860
3505.043177	484414.737664	47.532865
3504.336923	484360.248273	47.537869
3504.878573	484306.152983	47.542874
3504.723866	484242.408300	47.547879
3504.251309	484195.065410	47.552884
3504.479148	484136.215022	47.557889
3504.244792	484078.404995	47.562893
3504.253809	484032.042305	47.567898
3504.573676	483975.959369	47.572903
3504.449949	483934.579146	47.577908
3504.706966	483872.382446	47.582913
3504.290979	483824.978293	47.587917
3504.079500	483770.756897	47.592922
3504.434921	483718.665537	47.597927
3504.260074	483672.687596	47.602932
3504.141672	483616.374674	47.607937
3504.242294	483570.804959	47.612941
3504.216647	483518.120094	47.617946
3504.245748	483472.056196	47.622951
3504.249203	483430.197552	47.627956
3504.438778	483376.362002	47.632961
3504.182021	483341.380542	47.637965
3504.480388	483274.720599	47.642970
3504.352790	483230.707424	47.647975
3504.042728	483185.611764	47.652980
3504.449867	483130.675405	47.657985
3504.439819	483082.795034	47.662989
3504.302749	483033.518989	47.667994
3503.952089	482992.074086	47.672999
3503.951271	482940.344967	47.678004
3504.205708	482884.016679	47.683009
3504.057982	482846.636678	47.688013
3504.191513	482806.779000	47.693018
3504.408416	482763.515706	47.698023
3504.105288	482719.683087	47.703028
3504.090545	482667.803705	47.708033
3503.908714	482625.215556	47.713037
3503.858395	482590.298603	47.718042
3504.204381	482540.078227	47.723047
3503.981886	482501.242377	47.728052
3504.341894	482448.083560	47.733057
3503.845633	482418.354747	47.738061
3503.962742	482375.917429	47.743066
3504.110092	482326.236542	47.748071
3504.195190	482285.879795	47.753076
3504.003218	482224.007087	47.758081
3504.065672	482192.461493	47.763085
3503.934468	482146.067213	47.768090
3503.910000	482109.575745	47.773095
3503.638351	482072.316517	47.778100
3503.956403	482025.845216	47.783105
3503.893661	481992.751476	47.788109
3503.789788	481944.175410	47.793114
3503.799529	481907.829546	47.798119
3503.863635	481870.512568	47.803124
3503.876061	481827.484397	47.808129
3503.533700	481790.793463	47.813133
3503.705325	481758.924750	47.818138
3504.006224	481713.923523	47.823143
3503.608959	481688.175511	47.828148
3504.045498	481640.012539	47.833153
3503.692083	481607.322055	47.838157
3503.556922	481566.596336	47.843162
3503.996731	481526.227930	47.848167
3503.622902	481500.931224	47.853172
3503.801015	481461.518513	47.858177
3503.770521	481421.736374	47.863181
3503.604370	481381.218006	47.868186
3503.844930	481360.625116	47.873191
3503.628854	481315.660541	47.878196
3503.950461	481284.069098	47.883201
3503.869670	481248.901626	47.888205
3503.685370	481206.462380	47.893210
3503.702817	481173.150951	47.898215
3504.043045	481149.959142	47.903220
3503.933137	481107.911927	47.908225
3504.065557	481075.947454	47.913229
3504.238690	481029.042725	47.918234
3504.173969	480989.467956	47.923239
3504.097886	480944.225440	47.928244
3504.534747	480890.998262	47.933249
3504.072869	480860.501662	47.938253
3504.025271	480818.848105	47.943258
3504.120503	480776.866332	47.948263
3503.973237	480737.811323	47.953268
3503.736082	480681.306934	47.958273
3503.802079	480652.238512	47.963277
3503.725040	480609.425185	47.968282
3503.996040	480569.842792	47.973287
3503.786520	480548.617108	47.978292
3503.875002	480493.980186	47.983297
3503.715448	480471.581558	47.988301
3503.661916	480443.495040	47.993306
3504.055181	480395.842355	47.998311
3503.645185	480370.752721	48.003316
3503.967015	480329.996792	48.008321
3503.904053	480294.621916	48.013325
3503.666410	480247.684043	48.018330
3503.836912	480218.495831	48.023335
3503.925115	480174.742033	48.028340
3504.207141	480134.144329	48.033345
3504.057417	480106.984939	48.038349
3503.686990	480063.461052	48.043354
3503.798282	480023.297242	48.048359
3503.521215	479992.615740	48.053364
3503.764560	479957.339774	48.058369
3503.536886	479927.662213	48.063373
3503.713654	479888.651282	48.068378
3503.612662	479865.786281	48.073383
3503.663196	479843.148501	48.078388
3503.768370	479797.872156	48.083393
3503.633779	479771.975293	48.088397
3503.526071	479747.845672	48.093402
3504.099584	479698.742876	48.098407
3503.784762	479678.192270	48.103412
3503.749111	479641.647075	48.108417
3503.626976	479606.685955	48.113421
3503.805137	479579.621661	48.118426
3503.900462	479547.306434	48.123431
3503.503329	479507.633293	48.128436
3503.650955	479479.105923	48.133441
3503.697805	479452.570116	48.138445
3503.729075	479413.026121	48.143450
3503.965855	479383.774619	48.148455
3503.669074	479355.829194	48.153460
3503.710280	479306.461844	48.158465
3503.641174	479287.590123	48.163469
3503.785568	479254.152220	48.168474
3504.170111	479212.522420	48.173479
3503.907741	479188.013448	48.178484
3504.262120	479135.858336	48.183489
3504.431512	479102.466512	48.188493
3504.171349	479055.326879	48.193498
3504.056993	479025.577861	48.198503
3503.957693	478984.131405	48.203508
3504.086275	478949.480594	48.208513
3504.106953	478914.544379	48.213517
3504.309863	478868.287106	48.218522
3504.294437	478822.674524	48.223527
3504.011481	478791.435087	48.228532
3503.730962	478738.526573	48.233537
3503.506352	478706.821379	48.238541
3503.479241	478687.739352	48.243546
3503.364715	478643.864586	48.248551
3503.376550	478611.865714	48.253556
3503.787487	478580.912458	48.258561
3503.503630	478562.481675	48.263565
3503.557068	478521.058709	48.268570
3503.222067	478492.510939	48.273575
3502.838314	478479.970011	48.278580
3503.324392	478463.635309	48.283585
3503.480593	478448.268231	48.288589
3503.201267	478426.241916	48.293594
3503.633054	478390.829469	48.298599
3503.321138	478362.935726	48.303604
3503.315498	478330.281169	48.308609
3503.235702	478315.511191	48.313613
3503.518174	478298.097273	48.318618
3503.639731	478264.610819	48.323623
3503.673886	478233.771937	48.328628
3503.642171	478204.665639	48.333633
3503.314992	478194.342533	48.338637
3503.201761	478146.871676	48.343642
3503.477593	478118.269649	48.348647
3503.065851	478110.543031	48.353652
3503.505174	478086.267163	48.358657
3503.681264	478077.376942	48.363661
3503.308974	478036.025564	48.368666
3503.977054	478008.065203	48.373671
3503.063529	477989.133795	48.378676
3503.559403	477960.898987	48.383681
3503.575343	477935.429466	48.388685
3503.471968	477911.600439	48.393690
3503.721318	477873.433493	48.398695
3503.418742	477854.600146	48.403700
3503.360001	477811.523928	48.408705
3503.577935	477795.133154	48.413709
3503.453252	477770.244345	48.418714
3503.671588	477741.803436	48.423719
3503.843784	477712.661535	48.428724
3503.551459	477680.257286	48.433729
3503.346325	477655.331427	48.438733
3503.322279	477629.969567	48.443738
3503.603966	477591.188941	48.448743
3503.417039	477577.904949	48.453748
3503.319086	477555.340302	48.458753
3503.234048	477540.013649	48.463757
3503.443818	477507.877779	48.468762
3503.458395	477471.724690	48.473767
3503.162801	477454.408671	48.478772
3503.254696	477436.115111	48.483777
3503.197540	477425.289780	48.488781
3503.228230	477404.930757	48.493786
3503.246527	477371.966609	48.498791
3503.227302	477345.185851	48.503796
3503.626215	477311.852816	48.508801
3503.379886	477301.616661	48.513805
3503.148610	477291.782982	48.518810
3503.279528	477273.533228	48.523815
3503.277066	477243.255871	48.528820
3503.566374	477200.118781	48.533825
3503.257251	477190.551499	48.538829
3503.438307	477165.964086	48.543834
3503.570316	477148.676028	48.548839
3503.254618	477113.439369	48.553844
3503.455719	477086.266186	48.558849
3503.351540	477082.942247	48.563853
3503.205956	477059.321843	48.568858
3503.526853	477034.355950	48.573863
3503.141074	477000.042420	48.578868
3503.333383	476971.807287	48.583873
3503.351696	476957.778944	48.588877
3503.287109	476945.790050	48.593882
3503.614144	476932.772259	48.598887
3503.496000	476908.438117	48.603892
3503.207068	476856.183796	48.608897
3503.103688	476845.112850	48.613901
3503.071650	476833.168957	48.618906
3503.633285	476816.111026	48.623911
3503.298317	476799.611235	48.628916
3503.121151	476763.692018	48.633921
3503.248038	476741.087974	48.638925
3503.326437	476719.707380	48.643930
3503.320942	476707.100640	48.648935
3502.939481	476698.608750	48.653940
3502.939450	476678.051630	48.658945
3503.295839	476666.648905	48.663949
3503.110492	476645.414524	48.668954
3503.287415	476620.877719	48.673959
3503.128413	476591.436149	48.678964
3503.177176	476567.883193	48.683969
3503.431545	476562.320691	48.688973
3503.045140	476542.031926	48.693978
3503.303408	476525.329327	48.698983
3503.258950	476514.551923	48.703988
3503.372596	476491.089058	48.708993
3503.229628	476461.543274	48.713997
3503.387286	476439.389310	48.719002
3503.243466	476418.653915	48.724007
3503.183894	476406.258738	48.729012
3503.201290	476396.888458	48.734017
3503.548012	476383.461844	48.739021
3503.147367	476344.541914	48.744026
3503.678421	476317.918867	48.749031
3503.525285	476312.932214	48.754036
3503.582716	476285.073495	48.759041
3503.669995	476248.601771	48.764045
3503.236536	476224.421829	48.769050
3503.090236	476205.155020	48.774055
3503.244364	476185.735623	48.779060
3503.185800	476170.504572	48.784065
3503.052266	476158.375030	48.789069
3503.243816	476132.923649	48.794074
3503.495429	476101.132613	48.799079
3502.966604	476097.881001	48.804084
3503.283767	476080.205878	48.809089
3503.190228	476058.144981	48.814093
3503.229693	476054.239342	48.819098
3502.944946	476046.642065	48.824103
3503.180340	476034.196273	48.829108
3503.112359	476005.447112	48.834113
3502.991382	475969.061027	48.839117
3503.132909	475950.099251	48.844122
3503.319038	475930.572851	48.849127
3503.102535	475924.837380	48.854132
3502.990189	475910.678640	48.859137
3503.344581	475900.339128	48.864141
3503.046323	475889.351515	48.869146
3503.059850	475876.690321	48.874151
3503.149469	475855.306804	48.879156
3503.476598	475821.223788	48.884161
3503.119805	475804.777463	48.889165
3502.954968	475788.754068	48.894170
3503.142928	475782.797585	48.899175
3503.018952	475771.223149	48.904180
3503.238071	475753.361911	48.909185
3503.218965	475744.706433	48.914189
3503.255683	475727.635853	48.919194
3503.601548	475687.067986	48.924199
3503.249697	475671.633418	48.929204
3503.212809	475656.904601	48.934209
3503.114552	475643.300247	48.939213
3503.402594	475623.654848	48.944218
3503.457608	475605.669578	48.949223
3503.307091	475586.909203	48.954228
3503.206791	475566.266687	48.959233
3503.599849	475546.704548	48.964237
3503.035709	475534.850665	48.969242
3503.250619	475519.116650	48.974247
3503.054066	475506.035344	48.979252
3503.262885	475464.224472	48.984257
3503.146583	475451.483881	48.989261
3502.984363	475436.725651	48.994266
3503.431663	475417.356660	48.999271
3503.017434	475417.326114	49.004276
3502.902995	475407.319562	49.009281
3503.055630	475391.140340	49.014285
3503.184564	475378.509735	49.019290
3503.022579	475366.992172	49.024295
3502.600482	475359.924432	49.029300
3503.207443	475346.756451	49.034305
3503.056824	475313.766811	49.039309
3502.890287	475281.033016	49.044314
3503.309742	475263.643469	49.049319
3503.281301	475260.306266	49.054324
3503.108192	475245.701654	49.059329
3503.375444	475235.326012	49.064333
3503.345030	475224.190992	49.069338
3503.605751	475204.752362	49.074343
3503.341160	475173.807428	49.079348
3503.266040	475149.666160	49.084353
3503.334113	475136.083668	49.089357
3503.105775	475123.108792	49.094362
3503.546760	475112.652779	49.099367
3503.237748	475082.981218	49.104372
3503.430471	475058.692822	49.109377
3503.446421	475046.283834	49.114381
3503.213017	475034.119965	49.119386
3503.500151	475017.157883	49.124391
3503.005321	474995.417421	49.129396
3503.085879	474955.399626	49.134401
3502.967915	474939.620680	49.139405
3502.923825	474931.880573	49.144410
3503.312996	474920.167345	49.149415
3502.941348	474915.116346	49.154420
3502.588239	474903.226021	49.159425
3503.030559	474890.744126	49.164429
3503.275217	474885.182780	49.169434
3503.700203	474866.931065	49.174439
3503.519675	474848.529531	49.179444
3503.587908	474814.438224	49.184449
3503.788936	474800.123846	49.189453
3503.473305	474780.479349	49.194458
3503.539593	474750.641895	49.199463
3503.586289	474722.377539	49.204468
3503.164279	474703.409428	49.209473
3503.363255	474698.412852	49.214477
3502.995473	474686.524892	49.219482
3503.121403	474662.753769	49.224487
3502.916663	474636.253935	49.229492
3502.942508	474616.044568	49.234497
3503.212334	474605.364300	49.239501
3502.818282	474588.821971	49.244506
3503.104993	474577.075383	49.249511
3503.125083	474574.084243	49.254516
3503.389989	474564.974605	49.259521
3503.112714	474553.577497	49.264525
3502.991113	474545.597267	49.269530
3502.770218	474527.556780	49.274535
3502.758355	474517.734787	49.279540
3502.960726	474514.459318	49.284545
3503.137045	474502.275778	49.289549
3502.756758	474495.605679	49.294554
3502.955187	474486.861829	49.299559
3502.755536	474472.919448	49.304564
3503.026131	474464.669659	49.309569
3503.144475	474459.585509	49.314573
3503.048990	474435.244227	49.319578
3503.016250	474406.385277	49.324583
3502.802790	474396.040607	49.329588
3502.454568	474375.439091	49.334593
3502.709794	474381.320351	49.339597
3502.550259	474397.147154	49.344602
3502.911703	474386.906873	49.349607
3502.833495	474385.097199	49.354612
3502.809275	474373.403573	49.359617
3502.855139	474363.723561	49.364621
3502.411418	474360.001346	49.369626
3502.867796	474343.870625	49.374631
3502.745536	474338.523685	49.379636
3502.856631	474328.731237	49.384641
3502.870160	474319.664401	49.389645
3502.686981	474315.087453	49.394650
3502.764379	474306.009704	49.399655
3502.489008	474306.765680	49.404660
3503.067621	474292.740917	49.409665
3502.843795	474280.777476	49.414669
3502.494571	474276.076950	49.419674
3502.876734	474250.134669	49.424679
3502.861277	474249.681547	49.429684
3502.765910	474250.659990	49.434689
3503.068983	474239.619355	49.439693
3502.907521	474226.328589	49.444698
3502.761653	474214.908834	49.449703
3502.415424	474212.537225	49.454708
3502.865887	474193.926019	49.459713
3502.665800	474188.491044	49.464717
3502.323184	474187.182259	49.469722
3502.917722	474189.562110	49.474727
3502.898542	474197.363969	49.479732
3502.562727	474196.864266	49.484737
3502.585732	474188.150228	49.489741
3502.528004	474193.882423	49.494746
3502.792009	474171.099897	49.499751
3502.788498	474171.505617	49.504756
3502.882577	474165.919127	49.509761
3503.004782	474143.869743	49.514765
3502.758516	474142.696424	49.519770
3502.791792	474134.436370	49.524775
3502.536732	474132.859429	49.529780
3502.382169	474120.884057	49.534785
3502.622844	474114.816758	49.539789
3502.328585	474111.828577	49.544794
3502.679177	474115.414821	49.549799
3502.594062	474128.646486	49.554804
3502.553383	474119.335606	49.559809
3502.682637	474127.466632	49.564813
3502.434004	474117.786136	49.569818
3502.731110	474101.074716	49.574823
3502.374994	474093.742018	49.579828
3502.757992	474095.955441	49.584833
3502.819060	474075.334346	49.589837
3502.494866	474074.224969	49.594842
3502.675422	474061.179528	49.599847
3502.395663	474074.140624	49.604852
3502.828803	474080.143523	49.609857
3502.620383	474085.698920	49.614861
3502.444356	474081.728378	49.619866
3502.860084	474073.251073	49.624871
3502.641464	474066.148090	49.629876
3502.945483	474058.905225	49.634881
3502.989399	474046.946556	49.639885
3502.705466	474043.348915	49.644890
3502.732583	474035.596274	49.649895
3502.714928	474036.510818	49.654900
3502.662946	474019.808290	49.659905
3502.849516	474012.686742	49.664909
3502.841750	474010.713081	49.669914
3502.741196	474006.476433	49.674919
3502.431987	473995.084433	49.679924
3502.377274	473991.346361	49.684929
3502.787648	474003.075573	49.689933
3502.356994	474013.226598	49.694938
3502.339212	474013.027070	49.699943
3502.269820	474010.608166	49.704948
3502.300276	474002.044690	49.709953
3502.657247	474004.465131	49.714957
3502.279217	474012.682825	49.719962
3502.666597	474007.603254	49.724967
3502.424951	474016.101503	49.729972
3502.628893	474014.041053	49.734977
3502.727700	474001.617217	49.739981
3502.477104	473996.545294	49.744986
3502.594881	473984.472692	49.749991
3502.502754	473988.387758	49.754996
3502.617256	473977.683010	49.760001
3502.432797	473995.641322	49.765005
3502.586893	474012.225153	49.770010
3502.926945	473994.189647	49.775015
3502.573412	473995.364106	49.780020
3502.478346	473992.291254	49.785025
3502.595312	473983.409154	49.790029
3502.328576	473979.909845	49.795034
3502.392945	473970.631595	49.800039
3502.471608	473982.518739	49.805044
3502.651438	473986.589932	49.810049
3502.472366	473991.482016	49.815053
3502.630081	473986.239091	49.820058
3502.917523	473977.631725	49.825063
3502.707693	473972.248990	49.830068
3502.737942	473961.710542	49.835073
3502.775398	473968.692574	49.840077
3502.657229	473958.128824	49.845082
3502.854326	473946.498421	49.850087
3502.637643	473944.307221	49.855092
3502.862168	473938.191981	49.860097
3503.120648	473914.954317	49.865101
3502.575457	473927.353145	49.870106
3502.641008	473910.073400	49.875111
3502.553446	473917.532566	49.880116
3502.926265	473902.479190	49.885121
3502.499807	473902.349442	49.890125
3502.276062	473916.415184	49.895130
3502.408747	473925.558532	49.900135
3502.209022	473931.669539	49.905140
3502.233692	473914.548701	49.910145
3502.476245	473915.114976	49.915149
3502.508079	473935.517820	49.920154
3503.089836	473945.496015	49.925159
3502.677935	473945.211859	49.930164
3503.004175	473945.814484	49.935169
3502.547909	473937.891135	49.940173
3502.691030	473929.916079	49.945178
3502.542208	473918.395364	49.950183
3502.359247	473921.009290	49.955188
3502.296875	473915.145592	49.960193
3502.519898	473910.651109	49.965197
3502.421894	473907.781308	49.970202
3502.701004	473917.355426	49.975207
3502.714725	473924.341527	49.980212
3502.801064	473923.617811	49.985217
3502.820295	473927.159389	49.990221
3502.805518	473919.464494	49.995226
3502.480342	473904.479659	50.000231
3502.685454	473904.242072	50.005236
3502.509485	473902.145197	50.010241
3502.762288	473889.796273	50.015245
3503.050646	473891.570111	50.020250
3503.121665	473883.657988	50.025255
3502.774833	473882.197978	50.030260
3502.739108	473867.670100	50.035265
3503.209585	473860.905146	50.040269
3502.894670	473863.389687	50.045274
3502.877351	473848.757370	50.050279
3503.061922	473850.548933	50.055284
3502.635831	473835.479991	50.060289
3502.710792	473836.631937	50.065293
3502.456844	473835.004139	50.070298
3502.475785	473825.581649	50.075303
3502.568631	473824.806177	50.080308
3502.302793	473813.406660	50.085313
3502.546492	473824.658032	50.090317
3502.616922	473829.406274	50.095322
3502.777873	473831.353796	50.100327
3502.448824	473832.372161	50.105332
3502.416025	473823.870045	50.110337
3502.661383	473820.840320	50.115341
3502.746500	473822.294380	50.120346
3502.746727	473811.153278	50.125351
3502.330557	473811.781390	50.130356
3502.610985	473801.706545	50.135361
3502.499281	473811.094243	50.140365
3502.561794	473830.124651	50.145370
3502.606045	473824.850414	50.150375
3502.721970	473833.237051	50.155380
3502.706761	473829.137713	50.160385
3502.899826	473817.406636	50.165389
3502.527965	473823.141941	50.170394
3502.847114	473806.375851	50.175399
3502.655172	473805.598364	50.180404
3502.698900	473798.501124	50.185409
3503.244235	473784.228456	50.190413
3502.700630	473783.764220	50.195418
3502.914311	473775.118713	50.200423
3503.108713	473772.148322	50.205428
3502.862298	473752.896046	50.210433
3502.648231	473755.565947	50.215437
3502.573063	473760.592274	50.220442
3502.855612	473751.226019	50.225447
3502.791885	473744.147106	50.230452
3502.602687	473749.344831	50.235457
3502.695566	473734.136552	50.240461
3502.391318	473737.784041	50.245466
3502.645320	473746.501631	50.250471
3502.946280	473739.968143	50.255476
3502.839299	473751.026231	50.260481
3503.024742	473743.651566	50.265485
3502.755783	473739.595535	50.270490
3502.807759	473732.750069	50.275495
3502.474820	473731.490239	50.280500
3502.748015	473731.392949	50.285505
3503.206682	473715.717067	50.290509
3503.105338	473717.253614	50.295514
3503.159204	473714.408493	50.300519
3503.467498	473690.554346	50.305524
3503.143285	473679.012788	50.310529
3503.451272	473664.122214	50.315533
3503.103854	473663.877684	50.320538
3503.240799	473648.915020	50.325543
3502.618482	473649.375769	50.330548
3502.666665	473637.162900	50.335553
3502.677726	473634.122509	50.340557
3502.536892	473636.324147	50.345562
3502.544543	473624.067548	50.350567
3502.389432	473619.789486	50.355572
3502.363030	473613.362492	50.360577
3502.719739	473611.275914	50.365581
3502.782809	473628.483331	50.370586
3502.750904	473627.779793	50.375591
3502.695805	473628.548826	50.380596
3502.625769	473625.471639	50.385601
3502.785993	473615.771710	50.390605
3502.603819	473620.461854	50.395610
3502.487099	473612.277821	50.400615
3502.666786	473611.335588	50.405620
3502.688448	473605.963861	50.410625
3502.773066	473600.328175	50.415629
3502.655274	473598.018764	50.420634
3502.717795	473586.309831	50.425639
3502.612576	473582.276450	50.430644
3502.488463	473579.411057	50.435649
3502.810928	473592.269659	50.440653
3502.236749	473603.154399	50.445658
3502.681357	473601.913721	50.450663
3502.631679	473600.352307	50.455668
3502.529991	473600.774803	50.460673
3502.719038	473596.437971	50.465677
3502.500854	473592.271955	50.470682
3502.722693	473596.437345	50.475687
3502.492905	473588.930951	50.480692
3502.431956	473591.372163	50.485697
3502.837704	473598.342091	50.490701
3502.552709	473609.430658	50.495706
3502.590809	473602.688797	50.500711
3502.573656	473606.439215	50.505716
3502.424124	473601.552495	50.510721
3502.669564	473598.725287	50.515725
3502.677817	473599.939280	50.520730
3502.579487	473588.409738	50.525735
3502.777677	473555.509331	50.530740
3502.730429	473527.056626	50.535745
3503.019323	473480.619185	50.540749
3502.582087	473431.115153	50.545754
3502.444080	473356.137405	50.550759
3502.749809	473279.614952	50.555764
3502.295441	473187.421389	50.560769
3502.545607	473084.269435	50.565773
3502.440391	472981.835955	50.570778
3502.636781	472853.268869	50.575783
3502.521968	472722.880201	50.580788
3502.549281	472578.842973	50.585793
3502.714342	472416.346346	50.590797
3502.367301	472248.820557	50.595802
3502.387098	472057.984146	50.600807
3502.568595	471870.258263	50.605812
3502.735421	471664.553320	50.610817
3502.768887	471436.989123	50.615821
3502.493898	471209.981321	50.620826
3502.715810	470962.980918	50.625831
3502.679042	470710.095442	50.630836
3502.558307	470439.949158	50.635841
3502.880097	470157.010029	50.640845
3502.855873	469864.197984	50.645850
3502.973453	469552.666360	50.650855
3502.150029	469226.955335	50.655860
3502.290231	468899.453239	50.660865
3503.032144	468549.402444	50.665869
3502.606979	468195.593305	50.670874
3502.779397	467815.029833	50.675879
3503.086594	467434.233138	50.680884
3502.622184	467033.651494	50.685889
3502.874778	466606.139662	50.690893
3502.870824	466190.111660	50.695898
3502.861154	465732.076221	50.700903
3502.683003	465282.519576	50.705908
3502.554299	464806.750132	50.710913
3502.435665	464313.436689	50.715917
3502.301588	463816.718625	50.720922
3502.113950	463291.977011	50.725927
3502.404470	462768.102401	50.730932
3502.655958	462228.512162	50.735937
3502.603329	461662.000809	50.740941
3502.330689	461074.176613	50.745946
3502.549111	460479.105707	50.750951
3502.184546	459868.761058	50.755956
3502.243366	459236.685204	50.760961
3502.175472	458593.613133	50.765965
3501.926377	457926.324918	50.770970
3501.593445	457240.934432	50.775975
3501.591083	456554.146336	50.780980
3501.510062	455849.252690	50.785985
3501.710402	455123.706411	50.790989
3501.245092	454385.575010	50.795994
3501.072820	453628.711667	50.800999
3501.037982	452847.970044	50.806004
3501.175415	452059.209922	50.811009
3501.181177	451248.337257	50.816013
3501.012404	450424.077566	50.821018
3501.019711	449563.147306	50.826023
3501.183445	448699.568996	50.831028
3500.965889	447816.852856	50.836033
3501.119960	446896.663215	50.841037
3500.993335	445981.755754	50.846042
3500.598136	445023.697053	50.851047
3500.667340	444058.213119	50.856052
3500.273180	443077.346570	50.861057
3500.380017	442074.134225	50.866061
3500.248298	441065.641251	50.871066
3500.435380	440020.930573	50.876071
3500.194262	438957.575497	50.881076
3500.013731	437881.527158	50.886081
3499.937556	436780.397599	50.891085
3499.427978	435670.155646	50.896090
3499.527901	434531.341592	50.901095
3499.514948	433384.117594	50.906100
3499.283112	432208.355649	50.911105
3499.559309	431021.130645	50.916109
3499.018704	429826.219893	50.921114
3498.862578	428590.023030	50.926119
3499.107804	427348.414372	50.931124
3498.768746	426082.172742	50.936129
3498.712464	424795.055149	50.941133
3498.319643	423493.611347	50.946138
3498.265816	422172.393890	50.951143
3498.153210	420846.114593	50.956148
3498.093669	419489.445006	50.961153
3497.884682	418106.578769	50.966157
3497.573383	416728.401463	50.971162
3497.703678	415307.673386	50.976167
3497.610129	413885.558895	50.981172
3497.583120	412434.534415	50.986177
3497.633149	410973.334654	50.991181
3497.291220	409494.217070	50.996186
3497.185028	407981.808920	51.001191
3497.535984	406463.395907	51.006196
3496.739959	404916.417704	51.011201
3496.496665	403363.720339	51.016205
3496.166030	401802.517227	51.021210
3495.678920	400204.875558	51.026215
3495.986603	398604.670693	51.031220
3495.424689	396978.889577	51.036225
3495.410538	395350.636913	51.041229
3494.973295	393710.830116	51.046234
3494.804333	392047.229300	51.051239
3494.687960	390368.991487	51.056244
3493.901467	388678.017785	51.061249
3493.968086	386965.024804	51.066253
3493.953310	385248.571289	51.071258
3493.695650	383510.282967	51.076263
3493.761744	381760.533537	51.081268
3493.040261	379992.394473	51.086273
3493.425771	378202.795056	51.091277
3492.611922	376407.660775	51.096282
3492.604064	374601.717330	51.101287
3492.139132	372768.449845	51.106292
3491.946689	370933.412575	51.111297
3492.052393	369070.792305	51.116301
3491.625049	367202.191195	51.121306
3491.531332	365318.255817	51.126311
3491.276165	363426.369182	51.131316
3490.958070	361507.312423	51.136321
3490.936496	359573.256111	51.141325
3490.441027	357637.074963	51.146330
3490.374945	355676.053133	51.151335
3489.757968	353706.077439	51.156340
3489.489296	351723.993020	51.161345
3488.957780	349733.059167	51.166349
3488.855132	347710.209579	51.171354
3488.385789	345684.583253	51.176359
3488.374849	343644.361935	51.181364
3487.770907	341606.748449	51.186369
3488.058252	339543.932990	51.191373
3487.224273	337463.816190	51.196378
3487.101202	335373.999766	51.201383
3486.999666	333275.747751	51.206388
3486.318078	331163.463154	51.211393
3486.255143	329037.476425	51.216397
3485.827515	326913.889690	51.221402
3485.494227	324764.348175	51.226407
3484.959784	322599.440129	51.231412
3484.659796	320425.303140	51.236417
3484.490150	318255.601128	51.241421
3483.883269	316060.700060	51.246426
3483.758930	313851.797227	51.251431
3483.430523	311648.283441	51.256436
3482.785060	309428.616959	51.261441
3482.909345	307176.293475	51.266445
3482.156879	304937.500124	51.271450
3481.991388	302678.025113	51.276455
3481.527697	300403.240556	51.281460
3481.116497	298128.009482	51.286465
3480.847387	295834.826120	51.291469
3480.286253	293541.820240	51.296474
3479.863507	291232.878719	51.301479
3479.593752	288919.842286	51.306484
3478.612317	286584.628204	51.311489
3478.729852	284246.690632	51.316493
3478.132694	281912.708831	51.321498
3477.597574	279554.667605	51.326503
3477.224176	277193.995209	51.331508
3476.713077	274819.871430	51.336513
3476.547589	272441.155597	51.341517
3475.406238	270048.322442	51.346522
3475.365790	267651.691294	51.351527
3475.281293	265246.367375	51.356532
3474.553327	262846.922155	51.361537
3474.043897	260414.933275	51.366541
3473.440800	257989.678256	51.371546
3472.823026	255552.402548	51.376551
3472.921008	253105.888311	51.381556
3472.086643	250664.682735	51.386561
3471.954994	248198.381496	51.391565
3471.266272	245736.135167	51.396570
3471.145278	243248.518387	51.401575
3470.332422	240768.017793	51.406580
3469.810870	238274.349976	51.411585
3469.236231	235771.015974	51.416589
3468.621418	233273.068467	51.421594
3468.083927	230754.999389	51.426599
3467.337923	228251.139204	51.431604
3466.720873	225723.388339	51.436609
3466.078532	223199.051123	51.441613
3465.269160	220684.215977	51.446618
3464.614146	218149.446285	51.451623
3464.340770	215615.791943	51.456628
3463.552294	213085.421516	51.461633
3463.010372	210542.040513	51.466637
3461.905944	208005.549853	51.471642
3461.846557	205464.552339	51.476647
3460.999518	202919.569055	51.481652
3460.430061	200376.265223	51.486657
3459.983299	197817.220045	51.491661
3458.900342	195270.965684	51.496666
3458.390973	192707.922466	51.501671
3457.763873	190137.505440	51.506676
3456.852348	187575.236553	51.511681
3456.391995	185001.713163	51.516685
3455.530033	182453.252635	51.521690
3454.984752	179876.249912	51.526695
3454.379171	177312.615265	51.531700
3453.627219	174745.837493	51.536705
3453.234386	172164.231499	51.541709
3452.291381	169595.782905	51.546714
3451.291253	167027.090007	51.551719
3450.771443	164452.875103	51.556724
3449.665383	161884.811800	51.561729
3449.207072	159310.545431	51.566733
3448.637694	156742.993109	51.571738
3447.589408	154181.241325	51.576743
3447.082885	151607.009849	51.581748
3446.155567	149036.403022	51.586753
3445.712180	146460.610728	51.591757
3444.891282	143831.686999	51.596762
3443.911666	141270.603918	51.601767
3443.172564	138695.757596	51.606772
3442.055206	136141.086379	51.611777
3441.257397	133585.104242	51.616781
3440.445414	131026.487271	51.621786
3439.235536	128478.001649	51.626791
3438.637528	125934.431740	51.631796
3437.756498	123397.991720	51.636801
3436.957761	120857.034150	51.641805
3435.917537	118328.186036	51.646810
3435.134983	115814.704040	51.651815
3434.696197	113285.021286	51.656820
3433.419498	110771.900600	51.661825
3432.484358	108251.480259	51.666829
3431.042880	105745.968681	51.671834
3430.095087	103241.240352	51.676839
3428.987563	100751.420932	51.681844
3427.853502	98281.305107	51.686849
3426.940177	95811.979359	51.691853
3426.023364	93357.123744	51.696858
3424.626712	90909.394649	51.701863
3424.015271	88472.359249	51.706868
3422.704045	86048.048010	51.711873
3421.911781	83625.950282	51.716877
3420.663989	81214.316493	51.721882
3419.524574	78811.820216	51.726887
3418.338718	76428.185092	51.731892
3417.054464	74053.373181	51.736897
3416.213989	71685.314256	51.741901
3414.963252	69334.558858	51.746906
3413.669710	66994.550764	51.751911
3412.216241	64670.456470	51.756916
3411.199164	62371.127203	51.761921
3409.947568	60074.119268	51.766925
3408.570117	57802.423340	51.771930
3407.441001	55535.962441	51.776935
3405.976927	53295.463600	51.781940
3404.338499	51083.623571	51.786945
3403.164476	48868.083023	51.791949
3401.317452	46689.550449	51.796954
3400.001196	44527.149180	51.801959
3398.767703	42386.878903	51.806964
3396.956740	40270.072378	51.811969
3395.273872	38171.653691	51.816973
3393.585180	36094.853887	51.821978
3391.739042	34062.561573	51.826983
3390.153613	32052.270352	51.831988
3387.521108	30087.709525	51.836993
3385.026799	28165.399205	51.841997
3381.480391	26287.732132	51.847002
3377.366021	24482.654949	51.852007
3372.048450	22777.819958	51.857012
3366.037616	21170.240775	51.862017
3360.646497	19648.931675	51.867021
3355.509577	18229.755425	51.872026
3350.519343	16900.089528	51.877031
3345.978829	15660.312056	51.882036
3341.506009	14534.418585	51.887041
3337.569310	13483.842113	51.892045
3333.732223	12532.964571	51.897050
3330.323250	11655.942232	51.902055
3327.290385	10863.693101	51.907060
3324.127826	10139.558659	51.912065
3321.399664	9480.648337	51.917069
3318.113040	8906.525197	51.922074
3315.475668	8381.527945	51.927079
3313.178806	7919.157181	51.932084
3310.642959	7523.501480	51.937089
3308.882298	7168.362511	51.942093
3307.131515	6867.740234	51.947098
3305.234461	6606.168336	51.952103
3303.953199	6375.808180	51.957108
3302.828909	6194.569543	51.962113
3301.619110	6027.799200	51.967117
3299.829582	5887.081369	51.972122
3298.795859	5772.777941	51.977127
3298.760988	5668.438543	51.982132
3297.498572	5599.694890	51.987137
3297.434178	5542.697801	51.992141
3296.265451	5489.175609	51.997146
3295.919576	5445.223445	52.002151
3295.801901	5408.308305	52.007156
3295.717619	5387.641532	52.012161
3294.860956	5351.049408	52.017165
3294.914174	5327.140337	52.022170
3294.821486	5310.080153	52.027175
3294.724572	5277.577857	52.032180
3294.166823	5259.568967	52.037185
3293.752766	5232.850305	52.042189
3293.580856	5211.271608	52.047194
3293.374701	5190.063637	52.052199
3293.265680	5149.821363	52.057204
3293.040436	5133.408671	52.062209
3292.719673	5086.956942	52.067213
3292.540866	5047.788999	52.072218
3292.058142	5015.888562	52.077223
3291.920916	4973.714416	52.082228
3291.009719	4935.328894	52.087233
3291.463115	4885.784928	52.092237
3290.785938	4848.874270	52.097242
3290.247169	4811.256971	52.102247
3289.652837	4746.645089	52.107252
3288.961903	4698.635713	52.112257
3288.960430	4641.517378	52.117261
3288.138772	4592.365084	52.122266
3287.688366	4532.383068	52.127271
3287.563810	4477.864641	52.132276
3286.811775	4435.392636	52.137281
3286.580405	4373.497540	52.142285
3286.020693	4313.182042	52.147290
3285.437161	4250.813770	52.152295
3285.420886	4184.170750	52.157300
3284.253948	4126.751929	52.162305
3283.560951	4046.036556	52.167309
3283.400312	4004.461217	52.172314
3283.134883	3941.687633	52.177319
3282.319000	3860.677547	52.182324
3281.646412	3808.064112	52.187329
3281.256751	3722.255132	52.192333
3280.775893	3654.645063	52.197338
3280.328243	3584.974203	52.202343
3280.191932	3506.870954	52.207348
3279.003302	3449.115600	52.212353
3278.618807	3357.443976	52.217357
3278.044169	3276.747043	52.222362
3277.715593	3207.943447	52.227367
3276.730073	3129.046708	52.232372
3276.196583	3050.893538	52.237377
3275.487377	2970.008756	52.242381
3274.882916	2901.260731	52.247386
3274.136746	2824.552862	52.252391
3273.486895	2745.361450	52.257396
3272.787323	2685.432938	52.262401
3272.570548	2597.869750	52.267405
3272.079697	2526.529127	52.272410
3270.835641	2443.619980	52.277415
3270.634986	2356.739934	52.282420
3270.095742	2289.289380	52.287425
3269.399753	2210.261712	52.292429
3268.447679	2133.572642	52.297434
3267.857062	2051.710629	52.302439
3267.536880	1986.520758	52.307444
3266.396989	1905.250759	52.312449
3266.205741	1834.771642	52.317453
3265.315345	1754.635428	52.322458
3264.522992	1686.677231	52.327463
3264.011182	1610.941102	52.332468
3263.252971	1549.940538	52.337473
3262.899521	1470.948468	52.342477
3262.153204	1397.801617	52.347482
3261.601111	1318.564759	52.352487
3260.931542	1245.849214	52.357492
3260.033497	1169.193124	52.362497
3259.636801	1101.945559	52.367501
3259.125516	1037.499272	52.372506
3258.438534	963.798370	52.377511
3257.526552	891.001538	52.382516
3256.509749	811.427016	52.387521
3256.104956	747.660060	52.392525
3255.004498	689.553995	52.397530
3254.180570	616.697213	52.402535
3254.067749	555.851581	52.407540
3252.869639	500.333443	52.412545
3252.177613	427.141194	52.417549
3251.420695	380.231114	52.422554
3250.733963	332.600638	52.427559
3249.977580	284.889444	52.432564
3249.257436	235.408943	52.437569
3248.161251	176.108028	52.442573
3247.303811	139.078951	52.447578
3245.728007	122.274589	52.452583
3243.616228	148.940846	52.457588
3241.959452	163.597148	52.462593
3241.400264	155.508765	52.467597
3241.116471	151.956138	52.472602
3240.777464	160.022705	52.477607
3240.287037	141.959234	52.482612
3239.899193	155.898623	52.487617
3239.657359	149.077185	52.492621
3239.074223	160.659466	52.497626
3238.107843	163.584507	52.502631
3237.522882	151.537058	52.507636
3236.636043	156.840959	52.512641
3236.334898	151.882904	52.517645
3235.775748	159.080783	52.522650
3234.794597	162.571231	52.527655
3234.591257	154.476529	52.532660
3233.707760	166.145654	52.537665
3233.491689	161.044775	52.542669
3232.873773	154.947177	52.547674
3231.774750	163.646868	52.552679
3231.164431	161.039742	52.557684
3230.741619	158.886494	52.562689
3230.208098	164.434373	52.567693
3229.323289	158.889203	52.572698
3228.528267	167.243676	52.577703
3228.234251	154.761660	52.582708
3227.573447	163.802133	52.587713
3227.126009	162.466234	52.592717
3226.357932	158.690428	52.597722
3225.530016	159.535672	52.602727
3224.720471	148.523287	52.607732
3224.046552	161.806569	52.612737
3223.779202	164.341403	52.617741
3223.182144	152.108922	52.622746
3222.501927	159.948787	52.627751
3221.649789	151.889144	52.632756
3220.885083	157.705065	52.637761
3220.181983	159.488177	52.642765
3220.000128	162.212084	52.647770
3219.324363	160.389415	52.652775
3218.833217	150.995099	52.657780
3217.468052	162.821511	52.662785
3216.879981	158.512858	52.667789
3216.436249	158.768662	52.672794
3215.937847	158.422372	52.677799
3215.558722	156.288109	52.682804
3215.136182	160.942308	52.687809
3214.232310	156.027623	52.692813
3213.547519	151.615105	52.697818
3212.951259	158.427358	52.702823
3212.047879	156.041222	52.707828
3211.418082	163.809319	52.712833
3210.931013	158.370277	52.717837
3210.017733	153.725221	52.722842
3209.215262	167.941899	52.727847
3208.721736	156.651316	52.732852
3207.966830	162.032153	52.737857
3207.261276	155.543751	52.742861
3207.334423	151.276473	52.747866
3206.659440	159.742669	52.752871
3205.934191	153.443945	52.757876
3205.271710	156.662061	52.762881
3204.384355	158.401655	52.767885
3203.506464	155.912089	52.772890
3202.748400	151.116968	52.777895
3202.597310	147.337993	52.782900
3201.714395	154.101326	52.787905
3201.507251	153.126605	52.792909
3200.931055	152.406773	52.797914
3199.968526	156.782971	52.802919
3199.014785	148.503462	52.807924
3198.442303	161.883094	52.812929
3197.582627	155.299055	52.817933
3197.215127	149.779985	52.822938
3196.710747	158.563999	52.827943
3196.074428	148.912260	52.832948
3194.817562	160.155313	52.837953
3194.468990	160.345125	52.842957
3193.957720	155.627442	52.847962
3193.053328	150.507199	52.852967
3192.770258	152.480650	52.857972
3191.819448	152.032844	52.862977
3191.078378	150.235943	52.867981
3190.775438	147.939854	52.872986
3190.355711	152.973299	52.877991
3189.569969	147.176353	52.882996
3188.630946	151.215384	52.888001
3188.463438	154.567220	52.893005
3187.925614	146.927561	52.898010
3186.916000	157.891533	52.903015
3186.314852	148.440231	52.908020
3185.074411	151.835643	52.913025
3184.583228	148.166089	52.918029
3184.401556	155.386710	52.923034
3183.376565	152.201111	52.928039
3182.462228	142.180045	52.933044
3182.469482	147.634738	52.938049
3181.968966	152.577778	52.943053
3181.280509	145.090564	52.948058
3180.190451	156.278274	52.953063
3179.506483	145.095241	52.958068
3178.666989	147.323229	52.963073
3178.555730	149.209696	52.968077
3177.800327	148.348778	52.973082
3176.638676	150.405233	52.978087
3176.448271	145.288137	52.983092
3176.091225	152.175964	52.988097
3175.653025	154.289602	52.993101
3174.784841	146.897437	52.998106
3173.438536	158.464448	53.003111
3172.624232	153.031586	53.008116
3172.185924	146.686215	53.013121
3171.764571	154.079624	53.018125
3171.457590	148.989550	53.023130
3170.172879	149.217729	53.028135
3169.591642	143.402822	53.033140
3169.159791	153.349941	53.038145
3168.673148	153.778866	53.043149
3168.439701	149.208718	53.048154
3167.579189	150.769260	53.053159
3166.633812	145.693131	53.058164
3165.521040	147.918864	53.063169
3164.608011	146.956592	53.068173
3164.726710	148.429567	53.073178
3163.880733	151.288256	53.078183
3163.364318	144.872944	53.083188
3162.709671	150.284413	53.088193
3161.616927	149.078905	53.093197
3161.272156	139.363157	53.098202
3161.111986	146.456549	53.103207
3160.661600	140.203244	53.108212
3159.624539	144.412182	53.113217
3158.949140	148.211968	53.118221
3158.381957	155.854104	53.123226
3157.243890	145.482856	53.128231
3156.652594	147.471471	53.133236
3156.004585	156.217261	53.138241
3154.670419	142.904058	53.143245
3154.411962	141.555220	53.148250
3154.051662	135.837171	53.153255
3153.643644	138.397615	53.158260
3152.889975	142.710500	53.163265
3152.278881	143.436999	53.168269
3151.501709	148.180996	53.173274
3150.353754	149.430264	53.178279
3150.371504	145.657971	53.183284
3150.140080	148.808757	53.188289
3149.017372	148.471247	53.193293
3148.332023	135.798761	53.198298
3148.043519	147.894361	53.203303
3146.901951	147.642967	53.208308
3146.225635	149.151120	53.213313
3145.743938	148.035025	53.218317
3145.290240	137.728826	53.223322
3144.343146	147.309248	53.228327
3143.463991	147.136569	53.233332
3142.791852	146.569712	53.238337
3141.764128	151.597304	53.243341
3141.288013	142.364646	53.248346
3140.740382	147.500468	53.253351
3140.776963	139.792678	53.258356
3139.873004	144.973592	53.263361
3138.857675	147.207943	53.268365
3138.325594	142.149625	53.273370
3137.170481	142.306327	53.278375
3136.618661	138.166758	53.283380
3136.043279	146.434750	53.288385
3136.087920	141.500916	53.293389
3136.042859	136.462018	53.298394
3134.943081	140.436153	53.303399
3133.712776	138.731930	53.308404
3132.417930	141.979544	53.313409
3132.706363	144.923089	53.318413
3132.447081	139.328305	53.323418
3131.226884	146.604390	53.328423
3130.551816	135.877344	53.333428
3129.799796	145.968370	53.338433
3129.320116	140.065067	53.343437
3128.777559	139.190289	53.348442
3127.391478	150.247791	53.353447
3127.031103	138.855937	53.358452
3125.902440	142.853167	53.363457
3125.300931	144.658006	53.368461
3125.246203	138.795779	53.373466
3124.907614	142.614201	53.378471
3124.328344	135.813727	53.383476
3122.923530	144.679741	53.388481
3122.539365	142.305565	53.393485
3122.042843	140.772016	53.398490
3121.655021	139.055687	53.403495
3121.151658	136.652932	53.408500
3119.802363	137.987922	53.413505
3119.257400	138.191557	53.418509
3119.025221	137.490717	53.423514
3117.891903	139.815097	53.428519
3117.503138	133.513378	53.433524
3116.807253	142.508520	53.438529
3115.827987	136.865051	53.443533
3115.181165	136.845701	53.448538
3114.310355	138.559189	53.453543
3113.624260	134.367173	53.458548
3112.923309	133.304729	53.463553
3112.305524	139.470933	53.468557
3112.664980	129.389353	53.473562
3111.440094	138.416460	53.478567
3110.630127	136.571740	53.483572
3110.533257	136.259087	53.488577
3109.440930	137.300704	53.493581
3108.607534	133.018598	53.498586
3108.042170	140.237268	53.503591
3107.814695	136.990420	53.508596
3107.224353	129.776195	53.513601
3105.721178	136.223544	53.518605
3105.799414	139.338392	53.523610
3105.100066	138.333305	53.528615
3103.827939	135.292188	53.533620
3103.500183	136.434479	53.538625
3103.027418	140.508716	53.543629
3102.584413	134.349290	53.548634
3101.388541	139.736000	53.553639
3100.823150	134.813247	53.558644
3100.625577	136.109343	53.563649
3099.415503	133.228936	53.568653
3098.818375	130.797207	53.573658
3098.172406	136.085221	53.578663
3098.024841	133.927195	53.583668
3096.954686	142.520904	53.588673
3095.804213	137.153396	53.593677
3095.757684	141.029677	53.598682
3095.267018	143.592009	53.603687
3094.539351	137.831740	53.608692
3093.293403	139.690248	53.613697
3092.827505	139.586305	53.618701
3092.576515	141.376649	53.623706
3091.960486	145.303266	53.628711
3091.293036	133.009439	53.633716
3089.724109	136.990322	53.638721
3089.744110	132.732924	53.643725
3089.560771	134.302898	53.648730
3088.002519	133.041554	53.653735
3087.713733	131.525802	53.658740
3087.492391	136.446006	53.663745
3086.287579	130.438067	53.668749
3085.529643	132.645417	53.673754
3085.341557	135.387753	53.678759
3084.491775	132.636836	53.683764
3083.315015	132.031476	53.688769
3083.199492	134.431816	53.693773
3082.845481	124.595698	53.698778
3081.267158	143.402180	53.703783
3081.530991	132.043810	53.708788
3080.546024	130.254655	53.713793
3079.176689	135.177992	53.718797
3079.655893	128.242062	53.723802
3078.636222	135.893613	53.728807
3077.550682	131.641175	53.733812
3077.432913	131.261832	53.738817
3076.196458	136.325093	53.743821
3076.106285	130.938654	53.748826
3074.809124	136.147679	53.753831
3074.906745	133.320537	53.758836
3073.808115	134.765070	53.763841
3072.818565	135.908340	53.768845
3072.925366	130.570743	53.773850
3071.738675	145.441587	53.778855
3071.365977	130.080105	53.783860
3070.514579	119.771626	53.788865
3069.849488	131.373015	53.793869
3069.906796	128.883939	53.798874
3068.508093	138.844677	53.803879
3068.049372	133.817257	53.808884
3067.456690	130.980966	53.813889
3066.497846	130.590211	53.818893
3066.215271	120.852021	53.823898
3065.441942	128.260165	53.828903
3064.952702	130.241610	53.833908
3064.179822	126.229035	53.838913
3063.555821	128.527578	53.843917
3063.135444	127.786268	53.848922
3061.607090	132.507837	53.853927
3061.403444	130.201111	53.858932
3061.221922	134.430052	53.863937
3059.839946	132.980310	53.868941
3058.997503	122.695959	53.873946
3058.436783	127.651256	53.878951
3058.531166	134.277598	53.883956
3057.176340	141.384068	53.888961
3056.498025	136.451801	53.893965
3056.694787	128.644023	53.898970
3055.650293	132.237283	53.903975
3054.621490	130.464307	53.908980
3054.063706	120.243421	53.913985
3053.291698	128.815785	53.918989
3052.952503	122.504426	53.923994
3051.970291	131.899006	53.928999
3051.091115	126.682520	53.934004
3050.802726	127.415859	53.939009
3050.039370	127.131042	53.944013
3049.918171	120.250342	53.949018
3049.161203	131.786117	53.954023
3048.444277	121.407692	53.959028
3048.127780	115.887833	53.964033
3046.823209	124.296991	53.969037
3046.551296	126.290642	53.974042
3045.020919	125.479274	53.979047
3045.199980	123.632142	53.984052
3044.053048	129.638505	53.989057
3043.136744	127.813546	53.994061
3043.205754	124.679461	53.999066
3042.256784	135.395042	54.004071
3041.806958	123.821925	54.009076
3040.939903	125.707670	54.014081
3040.085581	115.145103	54.019085
3039.484085	127.746124	54.024090
3038.797254	118.389246	54.029095
3038.816354	118.257695	54.034100
3038.024700	117.936269	54.039105
3037.251495	127.927881	54.044109
3037.133121	124.107017	54.049114
3035.827386	132.924924	54.054119
3034.311206	117.730041	54.059124
3034.045656	131.273107	54.064129
3033.900954	129.571690	54.069133
3033.529578	120.621950	54.074138
3032.324747	126.376504	54.079143
3031.594512	126.976928	54.084148
3031.183485	122.591878	54.089153
3030.362739	133.183313	54.094157
3030.291672	119.558424	54.099162
3029.194779	125.421240	54.104167
3028.688147	125.724121	54.109172
3028.182654	123.487923	54.114177
3026.672650	131.422995	54.119181
3026.145794	125.746452	54.124186
3026.092152	128.214372	54.129191
3024.826243	124.827223	54.134196
3024.375827	129.511837	54.139201
3023.793970	129.034566	54.144205
3022.778581	122.329558	54.149210
3022.051126	130.818919	54.154215
3022.223725	118.055926	54.159220
3021.365706	129.336605	54.164225
3020.312229	130.707117	54.169229
3020.230497	121.361710	54.174234
3019.408743	128.013545	54.179239
3019.087359	122.642938	54.184244
3018.440092	127.033566	54.189249
3017.090086	127.740688	54.194253
3016.237709	125.622975	54.199258
3015.409647	128.019153	54.204263
3015.033469	130.468769	54.209268
3014.898514	125.741683	54.214273
3013.836538	127.831656	54.219277
3013.186939	114.945091	54.224282
3012.334066	125.324517	54.229287
3011.780106	109.655762	54.234292
3011.500441	118.257277	54.239297
3010.935566	127.432126	54.244301
3010.325186	129.207701	54.249306
3009.643537	124.199834	54.254311
3009.104331	121.513095	54.259316
3007.920909	121.101911	54.264321
3006.873090	124.100891	54.269325
3006.298361	121.855211	54.274330
3005.952449	123.564278	54.279335
3005.831637	120.372239	54.284340
3005.033726	118.988493	54.289345
3004.273748	125.087022	54.294349
3003.850424	116.305242	54.299354
3003.081852	133.805350	54.304359
3001.723072	123.709111	54.309364
3001.077137	127.795967	54.314369
3000.023947	121.245054	54.319373
3000.731366	118.715545	54.324378
2999.471728	120.562198	54.329383
2998.427327	125.611991	54.334388
2997.923660	121.377771	54.339393
2996.905600	127.551982	54.344397
2996.765483	119.270871	54.349402
2996.216993	129.078036	54.354407
2995.568616	114.590254	54.359412
2995.116923	113.173004	54.364417
2994.441699	122.112898	54.369421
2994.309303	122.485249	54.374426
2992.633552	123.615530	54.379431
2991.700398	123.755648	54.384436
2991.309595	126.294603	54.389441
2990.536831	122.220839	54.394445
2990.348869	120.027093	54.399450
2989.393976	120.567232	54.404455
2988.784189	130.821835	54.409460
2988.203737	113.887377	54.414465
2987.637441	122.385115	54.419469
2987.283782	120.093372	54.424474
2986.523468	128.432036	54.429479
2986.232447	125.320792	54.434484
2985.247722	123.560430	54.439489
2983.863247	127.843359	54.444493
2983.872534	124.179494	54.449498
2982.982161	133.297077	54.454503
2982.054800	123.101071	54.459508
2981.582072	130.325224	54.464513
2981.192577	128.469856	54.469517
2980.651850	124.626436	54.474522
2979.197448	128.133835	54.479527
2978.620657	127.505312	54.484532
2978.359397	122.125620	54.489537
2977.743464	116.842064	54.494541
2977.053038	113.424086	54.499546
2976.229742	123.985558	54.504551
2975.685713	116.375038	54.509556
2975.503593	117.559549	54.514561
2974.848325	119.477794	54.519565
2974.140277	119.500106	54.524570
2972.824829	126.086708	54.529575
2971.857422	126.184131	54.534580
2971.734556	118.160595	54.539585
2971.078670	118.592009	54.544589
2970.653635	118.698193	54.549594
2970.093931	126.398248	54.554599
2969.092213	125.118412	54.559604
2968.863957	118.253646	54.564609
2967.763699	122.245251	54.569613
2967.239239	116.596338	54.574618
2966.631104	123.475347	54.579623
2965.594415	124.103281	54.584628
2965.185479	121.805196	54.589633
2964.578703	128.912918	54.594637
2964.222917	115.584981	54.599642
2963.572235	120.377236	54.604647
2961.900089	114.488277	54.609652
2961.006596	112.046032	54.614657
2961.071768	127.052662	54.619661
2960.780776	114.514555	54.624666
2959.994178	124.910682	54.629671
2959.431168	120.740292	54.634676
2958.958136	128.669084	54.639681
2957.549260	123.656820	54.644685
2957.727309	116.714729	54.649690
2956.190183	120.989802	54.654695
2955.516289	122.095726	54.659700
2955.182625	112.868776	54.664705
2954.251173	120.789458	54.669709
2953.549870	113.145031	54.674714
2953.310343	114.596715	54.679719
2952.782184	117.215983	54.684724
2952.195896	113.192465	54.689729
2951.525577	119.969209	54.694733
2950.810574	113.730377	54.699738
2950.129090	118.389347	54.704743
2949.568052	117.619586	54.709748
2948.605321	120.082599	54.714753
2947.844290	119.804504	54.719757
2947.429753	112.705136	54.724762
2946.720271	115.375917	54.729767
2946.239550	126.212393	54.734772
2945.733473	119.161823	54.739777
2944.226073	123.943385	54.744781
2943.484565	120.638348	54.749786
2943.330807	121.206187	54.754791
2942.834759	118.011173	54.759796
2942.181710	119.825228	54.764801
2941.071543	119.202204	54.769805
2940.525506	112.505826	54.774810
2939.876072	122.034587	54.779815
2939.442143	123.837643	54.784820
2939.180249	114.616193	54.789825
2938.497869	122.158794	54.794829
2938.037234	115.121777	54.799834
2936.836253	123.900475	54.804839
2936.206732	114.829478	54.809844
2935.585010	117.541314	54.814849
2934.878169	123.923259	54.819853
2934.366896	116.327674	54.824858
2933.092428	119.644468	54.829863
2931.999128	117.138875	54.834868
2932.025899	114.481343	54.839873
2931.065124	124.525141	54.844877
2931.323448	120.729513	54.849882
2930.437269	118.968899	54.854887
2929.205278	126.961077	54.859892
2929.259259	116.108713	54.864897
2928.315889	121.769257	54.869901
2928.038142	115.109924	54.874906
2926.782317	119.044437	54.879911
2926.406608	115.993856	54.884916
2925.351192	106.914336	54.889921
2925.191075	123.811119	54.894925
2924.331078	107.480629	54.899930
2923.853639	113.589689	54.904935
2922.217340	116.386888	54.909940
2922.040521	112.543260	54.914945
2921.451032	117.740706	54.919949
2920.592455	107.909146	54.924954
2920.272261	114.813549	54.929959
2919.552772	114.731642	54.934964
2919.255285	119.941159	54.939969
2918.508719	118.096689	54.944973
2918.007446	119.171538	54.949978
2917.102814	116.009644	54.954983
2916.025121	119.444782	54.959988
2915.315828	113.375109	54.964993
2914.409386	114.926556	54.969997
2914.205388	106.389544	54.975002
2913.527520	107.063136	54.980007
2913.135708	110.225536	54.985012
2912.704439	107.763122	54.990017
2912.187858	118.549274	54.995021
2911.667428	106.044472	55.000026
2910.301542	116.301573	55.005031
2909.341336	114.415066	55.010036
2908.788144	109.907885	55.015041
2908.464067	118.006210	55.020045
2907.981990	109.397512	55.025050
2907.432365	116.251127	55.030055
2906.558197	115.003978	55.035060
2905.608787	114.522825	55.040065
2904.483227	123.706651	55.045069
2903.790056	120.771113	55.050074
2903.787944	108.992052	55.055079
2903.091315	118.621637	55.060084
2902.652241	115.978193	55.065089
2901.872122	123.415924	55.070093
2901.791667	112.704564	55.075098
2900.824209	117.639377	55.080103
2899.497819	123.323147	55.085108
2898.962999	119.820167	55.090113
2898.620482	128.059802	55.095117
2898.104074	115.698384	55.100122
2898.203560	118.866032	55.105127
2896.744527	114.369190	55.110132
2896.111603	117.809239	55.115137
2894.889630	123.474375	55.120141
2894.745136	114.619305	55.125146
2894.075478	117.923926	55.130151
2893.345767	118.832953	55.135156
2892.468043	110.703573	55.140161
2891.195377	124.718333	55.145165
2891.022429	116.191011	55.150170
2890.339413	122.344287	55.155175
2889.793506	123.475712	55.160180
2889.549321	114.044406	55.165185
2888.979350	117.800531	55.170189
2888.226194	114.727620	55.175194
2886.983074	118.831280	55.180199
2885.700650	121.490645	55.185204
2886.040189	114.454251	55.190209
2885.354560	113.855391	55.195213
2884.651322	114.399905	55.200218
2884.025614	112.171244	55.205223
2883.415297	117.701058	55.210228
2882.881696	108.838283	55.215233
2882.688916	114.102138	55.220237
2881.737402	121.539951	55.225242
2880.830892	115.296362	55.230247
2880.289771	113.445603	55.235252
2879.885339	114.355487	55.240257
2878.333158	115.846777	55.245261
2877.564549	118.679244	55.250266
2876.942904	117.814063	55.255271
2876.042215	116.612107	55.260276
2875.665843	114.550829	55.265281
2875.226828	118.093131	55.270285
2875.079423	108.465690	55.275290
2874.488008	114.679491	55.280295
2873.944567	116.860073	55.285300
2873.746153	105.621395	55.290305
2871.828848	118.850294	55.295309
2871.374236	112.200671	55.300314
2870.401831	109.891925	55.305319
2870.039437	107.490768	55.310324
2869.715199	100.312041	55.315329
2868.875133	113.695901	55.320333
2867.651773	109.032480	55.325338
2866.946968	116.926668	55.330343
2866.904698	112.638481	55.335348
2866.122835	116.751338	55.340353
2865.626175	118.197234	55.345357
2864.749467	117.339330	55.350362
2864.028541	114.051711	55.355367
2863.598455	116.304496	55.360372
2863.239176	109.691475	55.365377
2862.146642	118.654138	55.370381
2861.807630	106.713589	55.375386
2860.851232	112.107950	55.380391
2860.149872	118.723033	55.385396
2859.869325	121.661953	55.390401
2859.026934	119.599402	55.395405
2858.301224	118.549514	55.400410
2857.713078	119.885918	55.405415
2857.033694	124.778610	55.410420
2856.345440	116.925924	55.415425
2855.544384	120.088799	55.420429
2854.965445	114.971832	55.425434
2853.993786	111.005112	55.430439
2852.994560	112.703475	55.435444
2852.844350	104.749367	55.440449
2851.914800	119.303494	55.445453
2851.610784	113.412850	55.450458
2851.461540	122.215091	55.455463
2850.692074	117.723170	55.460468
2850.502634	106.261520	55.465473
2849.382979	118.688197	55.470477
2848.505239	110.883690	55.475482
2847.643972	117.001511	55.480487
2847.048963	119.840627	55.485492
2846.362957	109.447501	55.490497
2845.060619	124.300995	55.495501
2844.690057	113.202657	55.500506
2843.784724	117.473982	55.505511
2843.380401	110.687482	55.510516
2843.483033	110.345476	55.515521
2842.754154	111.906849	55.520525
2842.400111	104.737558	55.525530
2841.355518	111.504061	55.530535
2840.056875	114.303570	55.535540
2839.606920	110.958986	55.540545
2838.845409	118.068679	55.545549
2838.545388	107.619455	55.550554
2837.911390	110.531153	55.555559
2837.703118	120.304638	55.560564
2836.586714	110.673474	55.565569
2835.542015	115.533472	55.570573
2835.276686	110.267781	55.575578
2834.509667	110.622286	55.580583
2833.865049	109.964715	55.585588
2833.519033	114.080449	55.590593
2832.429884	122.231377	55.595597
2831.968264	121.297404	55.600602
2831.175036	117.630972	55.605607
2830.363086	120.054417	55.610612
2829.961414	109.781641	55.615617
2829.317480	115.104050	55.620621
2827.926387	109.285523	55.625626
2827.447505	110.289448	55.630631
2826.971897	110.237711	55.635636
2826.646072	109.638152	55.640641
2825.909570	110.808077	55.645645
2825.470483	115.605227	55.650650
2825.489213	108.358806	55.655655
2824.120229	116.572558	55.660660
2823.559267	114.120476	55.665665
2822.377086	117.427043	55.670669
2821.903035	110.156294	55.675674
2821.616235	109.478620	55.680679
2820.358844	110.636917	55.685684
2819.452666	107.737011	55.690689
2818.750662	110.999008	55.695693
2818.723342	105.544620	55.700698
2818.054848	116.747115	55.705703
2817.260669	116.396152	55.710708
2817.017824	105.888610	55.715713
2816.647077	112.879016	55.720717
2815.638908	105.647454	55.725722
2814.134140	108.280887	55.730727
2813.125132	113.561880	55.735732
2812.902297	108.358795	55.740737
2812.205518	106.178212	55.745741
2812.245199	104.427926	55.750746
2811.790009	102.282628	55.755751
2811.006193	110.499389	55.760756
2810.797591	103.576028	55.765761
2809.063408	109.423845	55.770765
2808.703655	107.584727	55.775770
2808.144394	106.202064	55.780775
2807.352046	113.220714	55.785780
2807.277390	103.544536	55.790785
2805.943679	109.732053	55.795789
2805.265234	110.059187	55.800794
2804.590553	96.717122	55.805799
2803.526933	105.621553	55.810804
2803.563216	102.838456	55.815809
2803.371291	114.241725	55.820813
2802.435116	107.150225	55.825818
2801.428231	105.565788	55.830823
2800.539657	108.976512	55.835828
2800.271099	105.099629	55.840833
2799.305709	108.959260	55.845837
2798.947885	107.641246	55.850842
2798.668468	110.300506	55.855847
2797.210967	116.316559	55.860852
2796.513606	102.419436	55.865857
2795.688672	105.869414	55.870861
2795.286032	104.004865	55.875866
2795.289699	107.056255	55.880871
2794.660609	116.079050	55.885876
2794.181621	103.707322	55.890881
2792.311992	105.556040	55.895885
2791.805190	100.211237	55.900890
2791.542887	108.340047	55.905895
2790.698050	103.926942	55.910900
2790.762777	99.996254	55.915905
2790.152906	113.256694	55.920909
2788.871470	109.850157	55.925914
2788.095805	106.995448	55.930919
2787.166320	115.245794	55.935924
2786.767359	105.068879	55.940929
2786.714349	106.837230	55.945933
2786.254007	100.879768	55.950938
2785.000690	99.461793	55.955943
2784.084050	105.671972	55.960948
2783.783540	105.849251	55.965953
2783.124623	105.810296	55.970957
2782.683016	100.911444	55.975962
2781.809440	101.888888	55.980967
2780.556148	106.493235	55.985972
2780.198678	103.064170	55.990977
2779.674405	109.605566	55.995981
2779.056662	106.552161	56.000986
2779.361398	102.540188	56.005991
2778.011175	108.344491	56.010996
2777.073221	102.996411	56.016001
2776.340126	112.620780	56.021005
2775.314007	106.074777	56.026010
2775.271938	103.790190	56.031015
2773.919581	110.106817	56.036020
2773.257795	102.107137	56.041025
2772.736738	102.178827	56.046029
2772.911094	99.606599	56.051034
2772.048539	103.464839	56.056039
2771.299276	106.558080	56.061044
2770.912501	95.364253	56.066049
2769.452819	96.382667	56.071053
2768.886003	95.398789	56.076058
2768.295429	97.732691	56.081063
2767.564957	98.229374	56.086068
2767.218836	95.038760	56.091073
2766.777373	100.544055	56.096077
2766.374096	93.717922	56.101082
2765.314712	101.070361	56.106087
2764.043208	100.424029	56.111092
2764.042536	93.465138	56.116097
2763.037528	99.580687	56.121101
2762.947418	99.038735	56.126106
2761.851037	98.255107	56.131111
2760.694830	95.127563	56.136116
2760.265012	97.805819	56.141121
2759.820526	94.583862	56.146125
2759.214727	97.590609	56.151130
2758.905251	98.405719	56.156135
2758.163276	96.712066	56.161140
2757.276876	93.387622	56.166145
2756.239209	99.126660	56.171149
2755.652679	104.169661	56.176154
2755.463466	91.535270	56.181159
2754.682480	102.634223	56.186164
2754.630898	102.901978	56.191169
2753.029654	96.347711	56.196173
2752.178701	95.602264	56.201178
2751.762634	100.560077	56.206183
2751.180706	109.382577	56.211188
2750.924273	92.765054	56.216193
2750.304788	106.145941	56.221197
2749.671802	99.829189	56.226202
2749.004503	96.895968	56.231207
2748.391823	101.274773	56.236212
2747.811625	93.184186	56.241217
2746.278971	105.208175	56.246221
2745.927249	93.004181	56.251226
2745.385545	93.255056	56.256231
2744.434469	99.248102	56.261236
2744.584624	90.875579	56.266241
2743.503560	103.945372	56.271245
2742.575427	98.436943	56.276250
2741.873850	89.277664	56.281255
2741.082566	100.128910	56.286260
2740.451555	94.604433	56.291265
2739.936863	101.259053	56.296269
2739.889772	97.491555	56.301274
2739.008321	100.612524	56.306279
2737.495063	99.772264	56.311284
2737.053045	92.889208	56.316289
2736.373789	102.123065	56.321293
2735.888287	95.127444	56.326298
2735.773041	100.828420	56.331303
2735.520332	101.196472	56.336308
2734.838452	100.433575	56.341313
2733.376659	99.531627	56.346317
2732.513235	100.744572	56.351322
2732.139302	96.709266	56.356327
2731.713050	102.695106	56.361332
2730.459107	93.655504	56.366337
2729.600065	100.276223	56.371341
2729.091536	96.497207	56.376346
2728.573679	101.164928	56.381351
2727.957107	103.410516	56.386356
2728.100136	93.137426	56.391361
2727.218781	102.695950	56.396365
2727.108061	94.881950	56.401370
2726.313490	91.459319	56.406375
2724.833752	103.376767	56.411380
2724.232746	99.124099	56.416385
2723.121388	105.758344	56.421389
2722.184982	94.240066	56.426394
2722.240862	95.716258	56.431399
2721.447038	108.585383	56.436404
2721.216139	92.679929	56.441409
2720.293585	93.835090	56.446413
2720.210731	101.186795	56.451418
2719.237193	97.186088	56.456423
2718.120523	99.720442	56.461428
2717.958657	97.723169	56.466433
2717.086673	97.704459	56.471437
2716.317803	92.627485	56.476442
2715.205558	93.521001	56.481447
2714.581890	105.606720	56.486452
2714.064847	93.332309	56.491457
2713.621545	94.653044	56.496461
2713.396615	95.399627	56.501466
2713.195368	99.113652	56.506471
2711.318567	100.976251	56.511476
2710.808569	89.580877	56.516481
2710.187819	101.493599	56.521485
2709.494986	96.655463	56.526490
2709.204497	95.803169	56.531495
2708.869551	107.371788	56.536500
2708.016524	96.571475	56.541505
2706.718919	105.155527	56.546509
2706.016012	101.134220	56.551514
2705.903895	94.479373	56.556519
2705.304565	95.578103	56.561524
2704.826716	90.922294	56.566529
2703.817845	100.426828	56.571533
2703.134804	100.127146	56.576538
2702.184336	89.258236	56.581543
2701.663214	108.895277	56.586548
2701.120315	98.465099	56.591553
2700.608806	98.501217	56.596557
2699.581791	95.708831	56.601562
2699.186980	96.422876	56.606567
2698.734708	97.733699	56.611572
2698.235436	92.241578	56.616577
2697.124582	97.035924	56.621581
2696.403560	99.709883	56.626586
2696.020265	91.274211	56.631591
2695.152440	104.444526	56.636596
2694.563140	93.970575	56.641601
2694.257090	98.852742	56.646605
2693.050883	96.841359	56.651610
2692.131154	92.619100	56.656615
2691.263258	102.833332	56.661620
2691.094701	96.056690	56.666625
2690.671325	97.332970	56.671629
2689.831051	92.036109	56.676634
2689.760660	95.312514	56.681639
2688.554296	96.019629	56.686644
2687.848864	95.110375	56.691649
2687.088999	96.230231	56.696653
2686.775899	90.845232	56.701658
2686.496406	87.037336	56.706663
2685.118207	95.733843	56.711668
2684.432436	90.570043	56.716673
2683.558370	94.584596	56.721677
2683.134342	100.123621	56.726682
2682.681907	91.173207	56.731687
2682.110091	105.623936	56.736692
2681.483423	92.023444	56.741697
2680.253340	99.167840	56.746701
2679.567253	93.696603	56.751706
2679.196431	98.105120	56.756711
2678.411694	105.432726	56.761716
2678.237911	96.353759	56.766721
2677.619492	100.826705	56.771725
2676.869714	98.425472	56.776730
2676.130366	90.950639	56.781735
2675.211499	96.432148	56.786740
2674.955353	96.440802	56.791745
2674.533378	91.909258	56.796749
2673.456254	96.181937	56.801754
2672.573124	91.088979	56.806759
2671.803112	106.373694	56.811764
2671.280241	101.153626	56.816769
2670.832523	101.025295	56.821773
2670.317127	92.933513	56.826778
2669.398237	90.204754	56.831783
2668.602056	92.830380	56.836788
2667.876272	94.590972	56.841793
2667.373450	100.124520	56.846797
2666.706249	101.046177	56.851802
2666.767567	95.396261	56.856807
2665.788158	94.684627	56.861812
2664.783243	89.075269	56.866817
2663.879538	98.641168	56.871821
2663.652086	95.334360	56.876826
2663.089524	89.509259	56.881831
2661.650348	97.245961	56.886836
2661.143497	96.720383	56.891841
2660.665398	88.871301	56.896845
2660.215480	92.275737	56.901850
2659.923060	86.660635	56.906855
2659.323978	97.673625	56.911860
2658.519475	85.995854	56.916865
2657.766582	96.227135	56.921869
2657.585215	95.903674	56.926874
2656.542348	88.713222	56.931879
2655.020566	94.123723	56.936884
2654.683317	96.969707	56.941889
2654.162400	95.848132	56.946893
2653.591977	97.100209	56.951898
2653.560829	87.735165	56.956903
2651.782609	97.751335	56.961908
2651.079589	91.441051	56.966913
2650.456797	103.645429	56.971917
2649.925015	100.314857	56.976922
2649.844321	94.036738	56.981927
2649.074064	95.690465	56.986932
2648.797289	88.984828	56.991937
2647.641852	94.159423	56.996941
2646.661453	93.795320	57.001946
2646.315184	88.881771	57.006951
2645.778856	99.118268	57.011956
2645.272331	95.887588	57.016961
2644.056797	102.457153	57.021965
2643.486939	99.487554	57.026970
2642.836194	98.674348	57.031975
2641.850360	103.980606	57.036980
2641.820271	97.239113	57.041985
2641.324533	97.503061	57.046989
2640.643577	98.603119	57.051994
2639.684928	95.722087	57.056999
2638.705731	107.895028	57.062004
2638.230274	90.928143	57.067009
2637.930506	99.422150	57.072013
2637.366618	100.433120	57.077018
2637.130255	101.414153	57.082023
2635.463839	102.623462	57.087028
2635.281872	101.291977	57.092033
2634.470527	95.097709	57.097037
2633.739823	101.581633	57.102042
2632.960712	101.312987	57.107047
2632.098343	101.763947	57.112052
2631.586906	96.768504	57.117057
2631.058120	101.326786	57.122061
2630.370633	99.866988	57.127066
2630.457278	92.544244	57.132071
2629.525428	97.877193	57.137076
2627.930505	94.360482	57.142081
2627.655409	91.492467	57.147085
2627.056451	109.128131	57.152090
2626.973042	94.468497	57.157095
2626.580175	98.310012	57.162100
2625.186268	94.568286	57.167105
2624.182096	94.488900	57.172109
2623.631344	101.977030	57.177114
2623.592891	97.841362	57.182119
2622.288359	92.590327	57.187124
2621.561341	95.508863	57.192129
2620.645464	94.087714	57.197133
2620.371227	100.170327	57.202138
2619.981784	91.858082	57.207143
2619.420762	103.226531	57.212148
2619.220106	96.117500	57.217153
2617.893180	99.334373	57.222157
2617.156963	95.095757	57.227162
2616.495660	94.816053	57.232167
2615.813769	94.865517	57.237172
2615.978075	91.227278	57.242177
2614.829207	91.132368	57.247181
2613.699853	89.099183	57.252186
2613.384652	92.277703	57.257191
2612.856490	105.873887	57.262196
2612.003185	95.490873	57.267201
2610.879230	96.837186	57.272205
2610.024439	102.526428	57.277210
2609.830397	86.547995	57.282215
2608.817932	99.154499	57.287220
2608.877706	88.344619	57.292225
2608.431726	86.287768	57.297229
2608.299830	90.846486	57.302234
2607.274775	88.261410	57.307239
2605.763747	91.610016	57.312244
2605.204700	94.037222	57.317249
2604.674012	94.437406	57.322253
2603.089562	95.344168	57.327258
2603.468596	89.625734	57.332263
2602.669450	90.168518	57.337268
2602.301131	84.182333	57.342273
2601.823588	91.307822	57.347277
2601.079342	87.793324	57.352282
2600.352008	94.072993	57.357287
2599.067279	99.017469	57.362292
2599.253624	90.718504	57.367297
2598.729620	85.889423	57.372301
2596.967480	94.556450	57.377306
2596.488011	96.822425	57.382311
2595.816970	99.708500	57.387316
2595.110882	97.382309	57.392321
2594.661133	93.611420	57.397325
2594.225634	95.868694	57.402330
2594.249667	88.359691	57.407335
2592.800176	95.603183	57.412340
2592.015820	90.534407	57.417345
2591.534708	95.146905	57.422349
2590.814249	100.647794	57.427354
2590.407840	97.177381	57.432359
2589.431829	102.462230	57.437364
2588.816502	97.317190	57.442369
2588.384455	95.987408	57.447373
2587.527116	89.767858	57.452378
2587.560503	86.603961	57.457383
2585.951860	100.175252	57.462388
2585.237640	95.929724	57.467393
2584.906224	96.132033	57.472397
2584.070109	95.302763	57.477402
2584.298813	95.248664	57.482407
2582.708124	101.800664	57.487412
2581.941459	92.568865	57.492417
2581.055300	91.724862	57.497421
2580.544577	98.522880	57.502426
2580.190644	95.332040	57.507431
2580.030953	100.612331	57.512436
2579.448779	98.883887	57.517441
2578.551425	97.964827	57.522445
2577.599766	102.825922	57.527450
2577.236884	95.498321	57.532455
2576.360704	99.221153	57.537460
2575.273357	90.245093	57.542465
2574.556784	97.259086	57.547469
2573.871943	97.616154	57.552474
2573.772119	88.701003	57.557479
2573.054127	91.700892	57.562484
2572.750221	80.788199	57.567489
2572.594796	90.171308	57.572493
2571.313341	93.683169	57.577498
2570.372254	82.581784	57.582503
2569.626192	93.859100	57.587508
2568.820284	90.241073	57.592513
2567.678601	99.987000	57.597517
2567.241674	104.336560	57.602522
2567.405564	91.845514	57.607527
2566.684000	95.419548	57.612532
2565.983152	94.898330	57.617537
2565.739173	93.582187	57.622541
2564.147280	88.869755	57.627546
2563.604154	88.633800	57.632551
2562.824391	94.166143	57.637556
2562.385809	88.370783	57.642561
2562.168514	89.184747	57.647565
2560.998085	93.494314	57.652570
2560.357530	94.228274	57.657575
2559.485424	90.432493	57.662580
2559.222711	94.450699	57.667585
2558.676762	94.776920	57.672589
2558.523737	92.581572	57.677594
2557.628346	88.185450	57.682599
2556.630033	97.139916	57.687604
2556.073677	93.592514	57.692609
2555.003672	93.434398	57.697613
2553.627421	93.283245	57.702618
2553.772457	92.127169	57.707623
2553.311386	94.939457	57.712628
2552.814427	85.702612	57.717633
2552.221421	86.542914	57.722637
2551.533278	97.222191	57.727642
2550.796376	87.907948	57.732647
2549.990031	92.218033	57.737652
2549.382733	90.202582	57.742657
2547.774198	90.286530	57.747661
2547.519377	94.063789	57.752666
2547.281941	88.228912	57.757671
2546.128925	88.865753	57.762676
2545.407226	91.790096	57.767681
2545.250412	87.881111	57.772685
2544.619949	86.557625	57.777690
2544.903118	88.524279	57.782695
2543.586705	98.995188	57.787700
2542.677468	92.947146	57.792705
2542.354615	89.218910	57.797709
2541.457191	89.803767	57.802714
2540.721817	84.404535	57.807719
2539.876601	95.381051	57.812724
2539.157469	98.023518	57.817729
2538.785528	92.189531	57.822733
2538.385077	91.877478	57.827738
2537.224881	80.575150	57.832743
2536.488327	100.861997	57.837748
2535.643273	82.225498	57.842753
2534.982763	83.765346	57.847757
2534.662537	91.503788	57.852762
2534.229435	77.016073	57.857767
2533.734087	87.987241	57.862772
2532.941822	81.788159	57.867777
2531.915013	85.067418	57.872781
2531.331243	96.532904	57.877786
2530.994420	88.991259	57.882791
2529.946126	101.617314	57.887796
2529.179675	92.380754	57.892801
2528.641845	96.286527	57.897805
2527.881940	96.789851	57.902810
2527.818236	100.574699	57.907815
2527.018923	96.324387	57.912820
2526.335676	90.137454	57.917825
2525.483515	89.483036	57.922829
2524.415864	97.706884	57.927834
2524.444678	90.413377	57.932839
2523.684636	98.618976	57.937844
2522.617208	83.946425	57.942849
2521.798210	80.649978	57.947853
2520.767073	86.192141	57.952858
2520.567990	90.336042	57.957863
2520.207114	88.413066	57.962868
2519.996893	92.708077	57.967873
2519.688828	88.714823	57.972877
2518.658196	83.278446	57.977882
2518.109193	75.253629	57.982887
2516.855392	82.554459	57.987892
2515.776063	81.912435	57.992897
2514.863849	76.515814	57.997901
2514.640916	86.114925	58.002906
2514.295162	80.620667	58.007911
2514.001296	92.799587	58.012916
2513.306557	97.276117	58.017921
2512.015435	85.828025	58.022925
2510.717250	88.667779	58.027930
2510.873122	88.419689	58.032935
2509.958872	98.969077	58.037940
2509.970790	87.396099	58.042945
2509.750437	93.744617	58.047949
2508.302830	93.732776	58.052954
2507.517280	89.211310	58.057959
2507.129052	91.909702	58.062964
2506.691990	90.337636	58.067969
2505.731026	91.485581	58.072973
2504.497696	94.845153	58.077978
2504.189618	86.200083	58.082983
2503.687877	84.403031	58.087988
2503.039888	83.212806	58.092993
2502.794748	85.237413	58.097997
2501.550419	92.788859	58.103002
2500.832876	93.239946	58.108007
2500.303546	91.855755	58.113012
2499.758070	85.708824	58.118017
2499.306069	91.372628	58.123021
2498.593973	91.703182	58.128026
2497.685359	83.410647	58.133031
2497.022807	86.455930	58.138036
2496.691356	86.777457	58.143041
2496.463052	90.421501	58.148045
2494.995134	90.973644	58.153050
2494.392166	86.233471	58.158055
2493.595150	88.941361	58.163060
2493.284002	84.812064	58.168065
2492.285000	93.687312	58.173069
2491.050398	91.798066	58.178074
2490.590281	85.273792	58.183079
2490.242458	94.508218	58.188084
2489.883628	91.032841	58.193089
2489.287003	94.078301	58.198093
2488.320566	94.559312	58.203098
2488.249879	88.812770	58.208103
2487.513570	93.907440	58.213108
2486.713353	93.714658	58.218113
2486.426013	88.274755	58.223117
2485.229868	91.329561	58.228122
2484.489305	89.411111	58.233127
2483.847698	88.552154	58.238132
2482.670792	85.697420	58.243137
2482.734209	90.420893	58.248141
2482.071274	91.201318	58.253146
2481.241660	87.204874	58.258151
2480.406869	98.037116	58.263156
2479.677216	94.716715	58.268161
2479.230818	91.149735	58.273165
2478.762585	96.152390	58.278170
2478.261237	88.504282	58.283175
2476.719419	101.068275	58.288180
2476.211210	93.757643	58.293185
2476.005872	99.491773	58.298189
2475.192263	93.363056	58.303194
2475.020017	96.039918	58.308199
2473.891654	100.889790	58.313204
2472.859132	99.177174	58.318209
2472.763455	94.776176	58.323213
2471.780974	95.014414	58.328218
2471.742091	89.954386	58.333223
2471.149410	90.356498	58.338228
2470.053218	96.984626	58.343233
2469.261686	86.340840	58.348237
2468.654004	93.248984	58.353242
2468.175358	83.710219	58.358247
2466.723715	88.989165	58.363252
2465.966474	86.475958	58.368257
2466.034213	83.342506	58.373261
2465.026756	89.819676	58.378266
2465.195801	82.218000	58.383271
2464.297099	90.966367	58.388276
2463.487070	88.417582	58.393281
2463.051334	87.421590	58.398285
2462.128157	101.124772	58.403290
2461.316443	91.077705	58.408295
2460.964646	94.399061	58.413300
2460.003148	88.422736	58.418305
2459.285773	87.070306	58.423309
2458.537486	89.864998	58.428314
2458.435149	86.313008	58.433319
2457.814983	93.519330	58.438324
2456.809923	90.748111	58.443329
2455.625197	85.384278	58.448333
2455.001400	87.553757	58.453338
2454.643507	85.520149	58.458343
2454.043807	89.493737	58.463348
2453.737443	86.493325	58.468353
2453.219728	87.672068	58.473357
2452.227915	92.624906	58.478362
2451.247987	85.583218	58.483367
2450.749432	90.855127	58.488372
2450.296138	81.932142	58.493377
2450.189119	80.123264	58.498381
2448.444514	91.218425	58.503386
2447.883320	78.757432	58.508391
2447.218350	89.621815	58.513396
2447.057104	89.628858	58.518401
2446.743927	87.392217	58.523405
2445.649324	88.899720	58.528410
2444.840834	88.034566	58.533415
2444.377433	88.765091	58.538420
2443.764459	84.006112	58.543425
2443.055749	86.983899	58.548429
2441.678187	100.582804	58.553434
2441.288278	91.096365	58.558439
2440.792007	90.837807	58.563444
2440.072560	80.883130	58.568449
2440.140337	82.712136	58.573453
2438.840300	88.441992	58.578458
2438.245596	79.564109	58.583463
2437.262063	93.188397	58.588468
2436.744229	85.200891	58.593473
2436.454676	83.551903	58.598477
2436.429888	87.825074	58.603482
2435.669280	83.451722	58.608487
2434.354181	91.760910	58.613492
2434.038544	93.930201	58.618497
2432.962592	89.525900	58.623501
2432.193620	93.301861	58.628506
2431.618679	84.052321	58.633511
2431.089233	81.508856	58.638516
2430.512904	94.655377	58.643521
2429.800607	90.158110	58.648525
2428.358460	90.738231	58.653530
2427.981546	83.838964	58.658535
2427.703193	85.206116	58.663540
2427.314325	87.980802	58.668545
2427.176514	82.046409	58.673549
2425.693079	83.538296	58.678554
2424.670107	82.518772	58.683559
2424.320915	83.616994	58.688564
2423.632021	87.029143	58.693569
2423.620430	73.419486	58.698573
2422.576184	84.686204	58.703578
2421.715654	79.557072	58.708583
2421.041177	82.887811	58.713588
2420.318917	84.611907	58.718593
2420.171762	78.398860	58.723597
2418.935017	89.709943	58.728602
2418.090662	87.037171	58.733607
2417.445019	94.739282	58.738612
2417.139722	93.944405	58.743617
2416.507449	85.289651	58.748621
2416.410809	87.747143	58.753626
2415.659748	85.096709	58.758631
2414.314671	89.371031	58.763636
2413.702214	88.519730	58.768641
2413.525374	86.230571	58.773645
2412.154930	94.068848	58.778650
2411.728092	77.658181	58.783655
2411.041691	93.105021	58.788660
2410.504607	93.781834	58.793665
2410.130548	92.673067	58.798669
2409.546295	90.329231	58.803674
2408.429476	84.111855	58.808679
2407.727913	88.792840	58.813684
2407.102387	84.729937	58.818689
2407.032902	88.732470	58.823693
2405.898486	79.661887	58.828698
2405.309009	82.658368	58.833703
2404.429805	83.544463	58.838708
2403.776529	94.279354	58.843713
2403.453533	81.710537	58.848717
2403.141628	95.343142	58.853722
2402.068742	87.205030	58.858727
2400.870685	87.459616	58.863732
2399.981441	85.575680	58.868737
2399.968077	87.801046	58.873741
2399.323532	89.875003	58.878746
2399.318387	89.382477	58.883751
2398.423136	83.791144	58.888756
2397.163559	80.412559	58.893761
2397.185003	85.397799	58.898765
2395.693921	87.468876	58.903770
2395.090332	83.656821	58.908775
2394.485058	90.027731	58.913780
2393.618661	93.492735	58.918785
2393.650375	78.210335	58.923789
2392.618941	85.076860	58.928794
2392.699539	87.900349	58.933799
2391.326402	81.384186	58.938804
2390.555475	83.017926	58.943809
2390.190847	77.740063	58.948813
2389.687700	86.152780	58.953818
2388.995535	81.078153	58.958823
2387.961448	86.486236	58.963828
2386.852627	92.194853	58.968833
2386.907298	84.319852	58.973837
2386.494469	92.692656	58.978842
2385.969370	79.858017	58.983847
2384.563182	83.248350	58.988852
2383.633582	86.803895	58.993857
2383.382661	87.108105	58.998861
2382.897017	82.010008	59.003866
2382.520800	87.172581	59.008871
2381.404571	85.980728	59.013876
2380.144058	83.215708	59.018881
2380.192930	78.930920	59.023885
2379.348258	91.764122	59.028890
2379.192241	81.988241	59.033895
2378.643658	93.082980	59.038900
2377.728345	95.157056	59.043905
2376.983143	78.504003	59.048909
2376.462147	91.621322	59.053914
2376.117443	86.700827	59.058919
2374.615086	83.872954	59.063924
2373.872757	91.282529	59.068929
2373.688710	83.743207	59.073933
2373.084633	91.322951	59.078938
2372.049716	83.190198	59.083943
2370.775620	86.821624	59.088948
2370.122494	86.143066	59.093953
2370.849317	82.227468	59.098957
2369.965212	77.960901	59.103962
2369.370249	77.590546	59.108967
2368.031839	81.503748	59.113972
2367.399177	83.906847	59.118977
2366.894855	75.043921	59.123981
2366.059523	83.224501	59.128986
2366.264270	81.272714	59.133991
2365.453030	85.566679	59.138996
2363.813527	85.253753	59.144001
2363.532987	81.799345	59.149005
2362.915175	87.847937	59.154010
2362.482910	82.426515	59.159015
2362.136110	82.344109	59.164020
2360.961265	84.151917	59.169025
2360.385337	79.644767	59.174029
2359.586955	82.991172	59.179034
2359.068117	94.205953	59.184039
2358.313366	78.829889	59.189044
2357.564250	86.882048	59.194049
2356.822046	80.248538	59.199053
2356.126123	83.807547	59.204058
2355.882174	82.200897	59.209063
2355.448889	85.001337	59.214068
2354.385493	85.281853	59.219073
2353.387518	78.114994	59.224077
2353.240862	81.608896	59.229082
2352.752911	76.064767	59.234087
2352.331773	76.696496	59.239092
2351.036503	85.999372	59.244097
2350.657764	81.612842	59.249101
2349.502777	87.995650	59.254106
2349.431845	86.433622	59.259111
2348.353722	86.203122	59.264116
2347.415563	81.739362	59.269121
2346.874107	78.278257	59.274125
2346.605870	80.557071	59.279130
2345.907285	77.334406	59.284135
2345.731004	72.834710	59.289140
2344.696347	85.461587	59.294145
2343.588402	80.974363	59.299149
2342.735785	79.644288	59.304154
2342.194274	73.690519	59.309159
2342.059256	82.113703	59.314164
2341.398388	80.011919	59.319169
2340.631729	76.295256	59.324173
2339.540328	83.441241	59.329178
2339.472743	78.435474	59.334183
2338.856385	76.071482	59.339188
2338.320978	84.083939	59.344193
2337.250707	77.081022	59.349197
2336.512769	86.166234	59.354202
2336.116979	76.996211	59.359207
2335.642225	76.507412	59.364212
2334.104329	85.507187	59.369217
2333.886481	74.569957	59.374221
2333.202434	77.133419	59.379226
2332.615340	78.314956	59.384231
2332.378601	80.918373	59.389236
2330.913915	80.746478	59.394241
2330.589830	73.587152	59.399245
2329.914018	79.587636	59.404250
2329.178404	82.112156	59.409255
2329.350829	81.541110	59.414260
2328.298958	83.072115	59.419265
2327.147746	72.584615	59.424269
2326.648554	79.308817	59.429274
2326.062390	80.248231	59.434279
2325.459021	85.684113	59.439284
2324.585600	92.152195	59.444289
2324.420420	84.975164	59.449293
2323.180783	85.378188	59.454298
2322.912992	75.349863	59.459303
2322.072016	75.664584	59.464308
2321.019739	80.303707	59.469313
2320.801993	77.672220	59.474317
2319.677489	78.531592	59.479322
2319.513286	76.207122	59.484327
2319.351219	75.026193	59.489332
2317.960123	79.001307	59.494337
2317.107795	66.538430	59.499341
2316.658304	81.373184	59.504346
2316.627352	80.570873	59.509351
2315.645945	69.849874	59.514356
2314.180292	77.338927	59.519361
2313.857192	76.354872	59.524365
2313.425250	77.426198	59.529370
2312.916888	76.849599	59.534375
2312.777860	74.345963	59.539380
2311.250616	88.082962	59.544385
2310.961995	75.093042	59.549389
2310.256130	83.099518	59.554394
2309.524913	74.047648	59.559399
2308.858209	77.391671	59.564404
2307.563226	77.295759	59.569409
2307.244249	73.163876	59.574413
2306.259347	84.844386	59.579418
2306.263022	82.023461	59.584423
2305.945985	76.900096	59.589428
2305.531953	77.626531	59.594433
2304.119838	72.725166	59.599437
2303.259534	80.876862	59.604442
2302.867218	75.470328	59.609447
2302.676240	72.862686	59.614452
2301.844259	76.388125	59.619457
2300.923248	73.377577	59.624461
2300.208417	79.940505	59.629466
2299.790926	69.463330	59.634471
2299.272875	68.699713	59.639476
2298.311840	80.610604	59.644481
2297.304974	79.738346	59.649485
2296.505629	78.049050	59.654490
2295.992536	80.977215	59.659495
2295.965872	76.844290	59.664500
2295.462327	88.016188	59.669505
2294.523902	73.484293	59.674509
2293.510897	78.860755	59.679514
2293.060367	70.212850	59.684519
2292.301054	79.260663	59.689524
2290.559489	79.728212	59.694529
2290.853772	68.662759	59.699533
2290.210145	68.603486	59.704538
2289.856382	69.213435	59.709543
2289.039644	69.434414	59.714548
2288.743722	77.695641	59.719553
2288.410418	73.828700	59.724557
2286.976788	78.120951	59.729562
2286.338653	81.031817	59.734567
2286.198852	64.971570	59.739572
2284.907687	77.326531	59.744577
2284.091096	68.923984	59.749581
2283.280054	75.553889	59.754586
2282.918541	71.870582	59.759591
2282.422674	75.432489	59.764596
2281.712421	73.137456	59.769601
2281.590327	71.609443	59.774605
2280.438569	79.325472	59.779610
2279.693044	82.154049	59.784615
2279.364714	79.370560	59.789620
2278.475000	81.002129	59.794625
2277.636618	68.032817	59.799629
2276.434036	71.946490	59.804634
2276.160248	74.431905	59.809639
2275.813042	76.255294	59.814644
2275.910997	80.274580	59.819649
2275.162471	70.160719	59.824653
2273.618776	83.086220	59.829658
2273.241531	77.561459	59.834663
2273.324107	69.039488	59.839668
2272.020948	73.346928	59.844673
2271.539146	67.480064	59.849677
2270.813343	71.616141	59.854682
2269.836269	72.690301	59.859687
2268.665217	70.989580	59.864692
2267.777622	80.107488	59.869697
2267.292330	69.653361	59.874701
2267.006100	77.712016	59.879706
2266.726776	81.956473	59.884711
2266.292861	84.638214	59.889716
2265.662047	84.508466	59.894721
2265.024887	72.508918	59.899725
2263.643768	81.101774	59.904730
2263.102741	68.350421	59.909735
2262.915718	72.622510	59.914740
2261.882193	82.100890	59.919745
2260.884679	72.700639	59.924750
2259.988643	72.447307	59.929754
2259.631315	77.813483	59.934759
2259.210789	73.044521	59.939764
2258.836325	77.782467	59.944769
2258.454260	67.768567	59.949774
2257.504146	73.091253	59.954778
2256.774366	70.441945	59.959783
2256.490798	66.787942	59.964788
2255.452678	79.713427	59.969793
2254.602154	71.431553	59.974798
2253.820343	76.527307	59.979802
2253.152027	75.957938	59.984807
2252.829832	76.516702	59.989812
2252.504199	76.770539	59.994817
2251.346449	72.103181	59.999822
2250.351708	71.558058	60.004826
2249.996445	79.823512	60.009831
2249.297475	68.560830	60.014836
2248.804505	76.621683	60.019841
2248.386243	70.323181	60.024846
2246.971779	71.002031	60.029850
2246.372147	74.476689	60.034855
2246.312693	73.419921	60.039860
2245.565762	74.931948	60.044865
2245.374988	66.426334	60.049870
2243.995875	73.248123	60.054874
2243.366121	75.839412	60.059879
2242.650817	67.796909	60.064884
2241.958020	74.869604	60.069889
2241.769217	69.463802	60.074894
2240.502176	78.150041	60.079898
2239.704844	81.069980	60.084903
2239.115590	58.800658	60.089908
2238.794867	72.893798	60.094913
2238.776469	64.033456	60.099918
2237.912419	73.196676	60.104922
2236.827166	74.913399	60.109927
2236.386869	68.234999	60.114932
2235.939366	78.636674	60.119937
2234.913896	68.753731	60.124942
2234.081706	78.312939	60.129946
2233.589161	69.899589	60.134951
2233.084087	73.905556	60.139956
2232.274321	72.606066	60.144961
2231.427771	74.593403	60.149966
2230.217951	75.241208	60.154970
2229.969826	77.693815	60.159975
2229.494731	72.124219	60.164980
2229.177304	78.488929	60.169985
2229.205751	77.532387	60.174990
2227.631941	79.658310	60.179994
2226.481324	72.761136	60.184999
2226.471255	74.388323	60.190004
2225.896786	79.799924	60.195009
2224.873293	71.057393	60.200014
2224.073392	78.453528	60.205018
2223.308957	75.813309	60.210023
2222.939093	70.932271	60.215028
2222.687685	80.887137	60.220033
2222.330038	70.710388	60.225038
2220.674363	69.282024	60.230042
2220.228450	75.061624	60.235047
2219.813230	71.383562	60.240052
2219.239139	78.604505	60.245057
2218.826626	67.909792	60.250062
2218.333272	72.860694	60.255066
2217.099837	71.559454	60.260071
2216.019384	68.209496	60.265076
2214.993726	73.447609	60.270081
2214.413470	73.006864	60.275086
2213.989654	71.268359	60.280090
2213.844992	74.980593	60.285095
2213.647930	75.159946	60.290100
2212.471744	78.681501	60.295105
2212.343469	67.293993	60.300110
2210.746064	80.089743	60.305114
2210.088347	72.200811	60.310119
2209.825021	74.542338	60.315124
2209.434608	75.058694	60.320129
2209.002117	68.809604	60.325134
2207.448450	75.036408	60.330138
2206.907393	71.900112	60.335143
2206.802437	69.687091	60.340148
2205.751595	74.978854	60.345153
2205.032792	67.428781	60.350158
2204.296489	77.238422	60.355162
2203.825278	78.687116	60.360167
2203.300924	71.009054	60.365172
2202.689914	80.014535	60.370177
2202.093975	66.757082	60.375182
2200.742894	76.647786	60.380186
2200.250928	68.380392	60.385191
2199.878764	70.538434	60.390196
2199.679527	74.521702	60.395201
2198.614039	73.288451	60.400206
2197.841612	75.942433	60.405210
2197.053696	72.241669	60.410215
2196.917931	71.165980	60.415220
2196.336783	73.619492	60.420225
2195.454356	71.038930	60.425230
2194.636422	74.577768	60.430234
2193.911097	72.920434	60.435239
2193.440321	73.343960	60.440244
2192.440463	77.121931	60.445249
2191.745343	63.024899	60.450254
2191.318572	68.918455	60.455258
2190.713776	73.754212	60.460263
2190.457178	72.183682	60.465268
2188.625990	76.039491	60.470273
2187.892595	72.785703	60.475278
2187.583031	86.388276	60.480282
2186.776227	71.492079	60.485287
2186.819914	67.941976	60.490292
2186.342164	78.228827	60.495297
2186.271425	62.770190	60.500302
2184.891953	75.728003	60.505306
2183.951668	71.818441	60.510311
2183.534405	74.194191	60.515316
2182.442896	81.483497	60.520321
2181.557156	67.324332	60.525326
2180.712634	72.739489	60.530330
2180.450701	75.868249	60.535335
2180.686840	68.116178	60.540340
2179.698865	79.681562	60.545345
2179.248306	69.302431	60.550350
2177.967602	68.927804	60.555354
2177.372335	74.140864	60.560359
2177.078193	68.292444	60.565364
2176.356428	80.145051	60.570369
2175.764233	74.307737	60.575374
2175.094204	72.131363	60.580378
2173.889170	75.958241	60.585383
2173.375594	70.311160	60.590388
2172.287901	71.338338	60.595393
2171.863193	73.362874	60.600398
2171.010728	71.185730	60.605402
2170.913124	73.424706	60.610407
2170.645674	69.615987	60.615412
2169.709955	68.376731	60.620417
2168.930965	69.887934	60.625422
2167.999364	66.393718	60.630426
2167.564396	72.632876	60.635431
2167.098357	73.353215	60.640436
2165.705425	76.037539	60.645441
2165.471595	65.304779	60.650446
2164.885204	69.689379	60.655450
2164.367234	83.623632	60.660455
2164.028171	71.957980	60.665460
2162.903389	84.204373	60.670465
2162.213598	72.248983	60.675470
2161.499333	73.713986	60.680474
2161.182258	78.419224	60.685479
2160.417270	72.138985	60.690484
2159.127590	79.964273	60.695489
2158.276422	76.476431	60.700494
2158.157050	77.671934	60.705498
2157.584585	80.519476	60.710503
2157.792981	78.374438	60.715508
2156.331984	83.398872	60.720513
2155.392612	75.241949	60.725518
2155.355946	78.598619	60.730522
2154.500566	78.680970	60.735527
2153.930481	73.645901	60.740532
2152.828227	77.375866	60.745537
2152.408703	74.122479	60.750542
2151.943676	71.178048	60.755546
2150.541063	70.872038	60.760551
2149.755790	66.382179	60.765556
2149.048294	77.677759	60.770561
2148.778907	70.610942	60.775566
2148.210129	78.693446	60.780570
2147.939849	76.385549	60.785575
2147.721760	76.033653	60.790580
2146.612477	80.825440	60.795585
2145.658988	74.845458	60.800590
2145.228134	78.329150	60.805594
2144.337867	73.160168	60.810599
2143.968609	72.780444	60.815604
2142.907970	71.482431	60.820609
2142.649180	71.467878	60.825614
2141.882677	68.406465	60.830618
2140.747980	69.295246	60.835623
2140.474011	73.078934	60.840628
2139.237618	78.727694	60.845633
2138.901803	71.206073	60.850638
2138.446649	69.153605	60.855642
2137.869925	69.307900	60.860647
2138.016024	68.983317	60.865652
2136.404487	68.966456	60.870657
2135.733266	67.430136	60.875662
2135.071239	67.117855	60.880666
2134.388784	74.586665	60.885671
2134.112512	63.723808	60.890676
2133.070199	72.825158	60.895681
2132.462926	66.865307	60.900686
2131.891849	71.617934	60.905690
2131.272186	65.477841	60.910695
2130.346336	68.136755	60.915700
2129.503523	68.632208	60.920705
2129.091278	68.203787	60.925710
2128.428497	61.696480	60.930714
2127.872804	70.059362	60.935719
2127.893459	66.787138	60.940724
2126.706284	74.798178	60.945729
2126.451089	73.096759	60.950734
2125.565394	71.585282	60.955738
2124.559009	78.338213	60.960743
2123.705890	60.945851	60.965748
2122.707612	66.288235	60.970753
2122.607523	63.741241	60.975758
2122.278360	67.656338	60.980762
2120.989047	68.511570	60.985767
2120.369039	64.407118	60.990772
2119.449413	74.973614	60.995777
2119.270006	73.425016	61.000782
2119.261381	73.925024	61.005786
2118.239341	66.206581	61.010791
2117.591121	64.350553	61.015796
2116.682126	68.875198	61.020801
2116.150909	63.861911	61.025806
2115.530105	68.684225	61.030810
2114.369216	73.767857	61.035815
2113.929144	70.261420	61.040820
2113.062904	61.155728	61.045825
2112.655924	69.495147	61.050830
2112.285477	67.041367	61.055834
2111.583115	64.772643	61.060839
2110.672829	65.789619	61.065844
2109.950350	70.919840	61.070849
2109.716936	70.440308	61.075854
2108.291198	69.917221	61.080858
2107.127264	69.554611	61.085863
2107.618963	74.675309	61.090868
2106.582843	71.776460	61.095873
2105.948910	73.206021	61.100878
2105.697599	64.689860	61.105882
2105.065116	67.167948	61.110887
2104.449161	66.074531	61.115892
2102.768073	74.816607	61.120897
2102.245474	78.841369	61.125902
2102.175519	70.999159	61.130906
2101.329945	75.544144	61.135911
2101.623029	67.808388	61.140916
2099.770056	69.514347	61.145921
2099.407514	74.160653	61.150926
2098.727060	73.768637	61.155930
2097.949297	69.082114	61.160935
2098.213643	60.160402	61.165940
2096.649713	71.481680	61.170945
2096.212307	64.404534	61.175950
2095.733272	68.879324	61.180954
2094.972933	73.050533	61.185959
2094.031498	69.132110	61.190964
2093.179566	71.781545	61.195969
2092.823891	71.955270	61.200974
2092.110765	66.907181	61.205978
2091.447700	73.259562	61.210983
2091.374316	67.945344	61.215988
2090.140673	68.615016	61.220993
2089.445021	74.937052	61.225998
2088.734957	63.972748	61.231002
2088.222553	71.401816	61.236007
2088.164928	70.566177	61.241012
2086.893677	70.328502	61.246017
2086.522434	62.514938	61.251022
2085.883757	61.756187	61.256026
2084.927859	68.317332	61.261031
2083.564308	61.665038	61.266036
2083.156396	67.540370	61.271041
2082.450108	64.742606	61.276046
2082.464424	63.454154	61.281050
2081.920189	71.021687	61.286055
2081.450425	66.040128	61.291060
2080.501390	62.884427	61.296065
2079.550094	65.590330	61.301070
2079.196348	60.855366	61.306074
2078.738832	67.623359	61.311079
2078.122353	57.571045	61.316084
2077.020632	68.774583	61.321089
2076.505757	65.496859	61.326094
2075.942688	67.524541	61.331098
2074.748444	72.480468	61.336103
2074.281959	68.957239	61.341108
2073.442056	72.633658	61.346113
2072.879446	68.146778	61.351118
2072.776018	70.374514	61.356122
2071.424118	63.455767	61.361127
2070.729780	59.385748	61.366132
2069.796485	71.342817	61.371137
2069.473245	65.369130	61.376142
2069.386435	63.157749	61.381146
2068.807061	61.166404	61.386151
2068.270468	55.999315	61.391156
2067.362416	65.447557	61.396161
2066.314701	60.446443	61.401166
2065.934559	54.434337	61.406170
2064.951218	55.423949	61.411175
2064.403765	64.135537	61.416180
2063.821277	69.720218	61.421185
2063.293323	67.116943	61.426190
2063.062426	60.644325	61.431194
2061.713105	79.082045	61.436199
2061.150009	69.472157	61.441204
2060.452131	70.499387	61.446209
2059.556678	63.992813	61.451214
2059.515365	66.559252	61.456218
2058.494383	72.632606	61.461223
2057.910716	65.290363	61.466228
2056.872173	67.205962	61.471233
2056.618174	64.079006	61.476238
2056.414182	59.942878	61.481242
2054.947704	68.137879	61.486247
2054.246461	64.011018	61.491252
2053.722223	64.889736	61.496257
2053.291140	64.664668	61.501262
2052.935977	62.799178	61.506266
2052.052910	67.061248	61.511271
2051.449411	65.339284	61.516276
2050.218797	66.673157	61.521281
2050.112707	61.938859	61.526286
2049.792392	67.298702	61.531290
2048.279129	78.101346	61.536295
2047.780490	70.589828	61.541300
2047.090630	80.438503	61.546305
2046.744833	67.639993	61.551310
2046.653109	70.218213	61.556314
2044.681983	72.126367	61.561319
2044.267262	65.849002	61.566324
2043.775725	75.129692	61.571329
2043.362976	70.160095	61.576334
2043.150507	69.412915	61.581338
2041.922108	70.309060	61.586343
2041.190689	64.680712	61.591348
2040.429503	69.738220	61.596353
2040.276861	71.728068	61.601358
2039.897552	73.523802	61.606362
2038.724006	63.742432	61.611367
2037.844449	60.762743	61.616372
2037.339938	63.810238	61.621377
2036.757943	64.401217	61.626382
2036.779232	66.148952	61.631386
2035.475586	64.336367	61.636391
2034.749114	56.028994	61.641396
2034.064295	62.766001	61.646401
2033.489790	62.146274	61.651406
2032.231633	68.298882	61.656410
2031.221783	66.475120	61.661415
2031.754072	60.328256	61.666420
2031.239441	61.808466	61.671425
2030.660034	63.931705	61.676430
2029.937504	59.802966	61.681434
2028.641826	62.996057	61.686439
2027.802512	53.777237	61.691444
2027.151131	52.969748	61.696449
2027.342757	66.137624	61.701454
2026.426017	61.269241	61.706458
2025.481562	71.191065	61.711463
2024.959278	65.018940	61.716468
2024.107226	70.913802	61.721473
2023.456660	68.648467	61.726478
2022.520424	65.005476	61.731482
2021.564704	78.015162	61.736487
2021.567853	71.856574	61.741492
2020.866150	75.986183	61.746497
2020.133523	72.716898	61.751502
2019.890647	71.923213	61.756506
2018.604081	80.282443	61.761511
2018.220040	72.389761	61.766516
2017.370628	76.759366	61.771521
2016.904567	82.365189	61.776526
2016.267937	71.897922	61.781530
2016.246674	76.490983	61.786535
2015.179877	70.223324	61.791540
2014.614092	73.807862	61.796545
2013.845055	69.302225	61.801550
2012.787210	66.740653	61.806554
2011.717138	71.296024	61.811559
2011.424423	69.672870	61.816564
2010.945850	76.119614	61.821569
2010.191551	73.437042	61.826574
2010.092533	56.646754	61.831578
2009.019578	68.670343	61.836583
2008.495911	69.925531	61.841588
2007.884839	72.763504	61.846593
2007.478343	71.638216	61.851598
2006.165831	68.748382	61.856602
2005.331501	75.854773	61.861607
2004.859316	61.230206	61.866612
2004.621327	71.198151	61.871617
2003.813299	67.451920	61.876622
2003.086332	69.878287	61.881626
2001.869916	64.268571	61.886631
2001.560401	65.126352	61.891636
2001.381391	67.035450	61.896641
2001.037553	68.239746	61.901646
1999.952396	69.679402	61.906650
1998.548808	68.431005	61.911655
1998.190801	65.768670	61.916660
1997.482579	70.189120	61.921665
1997.265343	68.322539	61.926670
1996.562847	66.907242	61.931674
1995.417854	76.459576	61.936679
1995.509554	59.690346	61.941684
1994.570355	66.496922	61.946689
1993.722859	70.068074	61.951694
1993.172293	64.130916	61.956698
1992.288316	70.276363	61.961703
1991.581162	63.072885	61.966708
1991.078055	74.139693	61.971713
1990.617550	72.963648	61.976718
1990.356170	73.463078	61.981722
1989.029835	77.530601	61.986727
1988.669290	63.439154	61.991732
1987.922408	74.267016	61.996737
1987.756028	72.522783	62.001742
1986.279207	70.962851	62.006746
1985.566808	73.117134	62.011751
1984.918392	63.424366	62.016756
1984.537530	73.893969	62.021761
1984.325247	73.857258	62.026766
1983.276688	68.568555	62.031770
1982.564909	78.706364	62.036775
1982.307566	61.125298	62.041780
1981.487038	71.687478	62.046785
1980.585497	68.904183	62.051790
1979.685057	69.721346	62.056794
1979.021457	77.560346	62.061799
1978.375840	69.895175	62.066804
1977.821870	72.908506	62.071809
1977.214806	66.585898	62.076814
1976.843937	66.470926	62.081818
1975.575866	71.377527	62.086823
1975.473814	73.545425	62.091828
1974.845519	71.550618	62.096833
1974.419845	70.932673	62.101838
1973.460253	71.554306	62.106842
1972.681064	68.275628	62.111847
1972.265807	68.396003	62.116852
1971.309804	71.532186	62.121857
1970.136576	70.016242	62.126862
1970.119320	68.220843	62.131866
1969.095770	70.091263	62.136871
1968.602859	65.799311	62.141876
1968.460556	75.769440	62.146881
1967.238060	75.825809	62.151886
1966.565868	73.757595	62.156890
1965.626437	76.113343	62.161895
1965.108197	68.358098	62.166900
1964.711204	78.961906	62.171905
1964.400610	79.686063	62.176910
1963.558537	79.049749	62.181914
1962.517794	75.776342	62.186919
1962.506566	74.078593	62.191924
1961.652038	80.669387	62.196929
1960.588424	77.983685	62.201934
1960.159469	63.765400	62.206938
1959.229130	69.070527	62.211943
1958.964658	59.831539	62.216948
1958.716054	66.217624	62.221953
1957.536922	68.099662	62.226958
1956.957311	77.513836	62.231962
1955.858235	78.571028	62.236967
1955.494524	68.646803	62.241972
1954.943855	78.093131	62.246977
1954.179333	71.732332	62.251982
1953.483102	71.511185	62.256986
1952.559065	75.492921	62.261991
1952.268861	70.286459	62.266996
1951.838754	69.418626	62.272001
1950.764079	69.572076	62.277006
1950.272885	65.422721	62.282010
1949.041259	70.182572	62.287015
1949.143163	63.016743	62.292020
1948.814568	72.274294	62.297025
1947.532929	77.139804	62.302030
1946.873016	68.068326	62.307034
1946.148850	73.788562	62.312039
1945.723586	74.265505	62.317044
1945.011447	75.854114	62.322049
1944.131805	81.032946	62.327054
1943.297231	72.815523	62.332058
1943.101524	80.355413	62.337063
1942.892207	75.975474	62.342068
1941.207030	68.319209	62.347073
1940.573970	78.736435	62.352078
1940.029361	76.073263	62.357082
1939.314988	80.188075	62.362087
1939.151235	74.285008	62.367092
1938.908535	75.407667	62.372097
1937.928715	78.785552	62.377102
1937.152395	74.621029	62.382106
1936.537849	81.857586	62.387111
1935.545857	74.394960	62.392116
1934.710333	73.583064	62.397121
1933.810524	74.506701	62.402126
1933.429495	69.842337	62.407130
1932.789983	82.387031	62.412135
1932.286968	78.655339	62.417140
1931.774977	79.379216	62.422145
1931.443538	76.559977	62.427150
1930.384742	73.471239	62.432154
1929.682478	74.511866	62.437159
1929.370373	69.600458	62.442164
1928.813591	67.136732	62.447169
1927.418379	74.479207	62.452174
1927.216399	68.397559	62.457178
1926.014918	80.807872	62.462183
1925.854568	67.824905	62.467188
1925.302574	74.796163	62.472193
1924.387897	69.662590	62.477198
1923.767069	63.737858	62.482202
1923.334434	68.579702	62.487207
1922.949059	70.775542	62.492212
1921.629113	74.299638	62.497217
1920.915855	72.784355	62.502222
1920.421980	75.081650	62.507226
1919.723231	73.524018	62.512231
1919.406168	66.113298	62.517236
1918.278665	71.401636	62.522241
1917.397735	75.079961	62.527246
1916.743147	70.728045	62.532250
1916.186015	77.755445	62.537255
1915.971670	73.351502	62.542260
1915.806007	74.339803	62.547265
1915.221644	75.203558	62.552270
1913.911748	75.477778	62.557274
1912.951516	82.556378	62.562279
1912.587970	72.429638	62.567284
1912.131855	78.167177	62.572289
1910.884516	75.144644	62.577294
1910.585252	73.566432	62.582298
1909.538939	77.801583	62.587303
1909.249831	78.805477	62.592308
1909.156976	74.456537	62.597313
1908.451235	77.567284	62.602318
1907.609090	70.217578	62.607322
1906.798673	70.967249	62.612327
1906.012074	73.832496	62.617332
1905.098851	77.808442	62.622337
1904.251006	74.019305	62.627342
1904.354691	64.929699	62.632346
1903.624057	69.609375	62.637351
1902.590319	62.862824	62.642356
1901.776170	64.524543	62.647361
1901.437813	68.464111	62.652366
1901.343106	63.852212	62.657370
1899.692297	72.102462	62.662375
1898.992140	66.966931	62.667380
1898.371170	63.812378	62.672385
1897.895305	65.780552	62.677390
1897.502535	66.069184	62.682394
1896.928713	71.520554	62.687399
1896.200148	60.808535	62.692404
1895.112536	75.787155	62.697409
1894.234625	64.210589	62.702414
1894.144230	67.717751	62.707418
1893.772782	77.875097	62.712423
1893.128704	77.227026	62.717428
1891.589482	75.691613	62.722433
1891.041988	77.937295	62.727438
1890.880849	71.458284	62.732442
1889.987508	75.361359	62.737447
1889.803719	75.850282	62.742452
1888.576441	72.032514	62.747457
1887.699790	74.455293	62.752462
1887.581999	64.610979	62.757466
1886.704826	72.606514	62.762471
1886.653924	74.867498	62.767476
1885.387532	73.619344	62.772481
1884.302545	74.194159	62.777486
1884.077354	72.927342	62.782490
1883.561729	64.549982	62.787495
1883.209492	68.853094	62.792500
1882.419610	70.449878	62.797505
1881.025217	78.448249	62.802510
1880.934032	65.117551	62.807514
1880.289387	73.487367	62.812519
1879.984950	69.301334	62.817524
1878.855922	63.340402	62.822529
1878.356338	68.469215	62.827534
1877.487564	59.838078	62.832538
1877.025873	68.163960	62.837543
1876.420535	59.480650	62.842548
1875.318768	62.011019	62.847553
1874.760568	64.691146	62.852558
1874.365524	71.250305	62.857562
1873.945949	72.740318	62.862567
1873.174428	63.651244	62.867572
1872.182661	70.760895	62.872577
1871.322885	74.513762	62.877582
1870.989896	64.901654	62.882586
1870.096646	65.735367	62.887591
1869.886464	64.651897	62.892596
1868.998144	65.954879	62.897601
1867.751077	72.908481	62.902606
1867.788299	63.106332	62.907610
1867.486865	67.428382	62.912615
1866.348380	67.659474	62.917620
1865.448625	67.783803	62.922625
1864.654426	70.612856	62.927630
1864.499876	62.357271	62.932634
1863.947054	66.485893	62.937639
1862.872778	59.434460	62.942644
1862.218414	70.002556	62.947649
1861.409993	70.048500	62.952654
1861.335457	68.078570	62.957658
1860.258997	68.242605	62.962663
1859.711017	68.371092	62.967668
1858.916628	63.273401	62.972673
1857.921871	66.126504	62.977678
1857.709528	66.720967	62.982682
1857.404886	74.228568	62.987687
1857.024892	66.293383	62.992692
1856.097450	69.518244	62.997697
1854.838266	63.163946	63.002702
1854.855801	57.378687	63.007706
1853.570692	67.339461	63.012711
1853.035097	71.790387	63.017716
1852.235237	59.733529	63.022721
1852.073596	66.202624	63.027726
1851.935226	68.157664	63.032730
1850.282797	71.873258	63.037735
1849.393217	68.349027	63.042740
1849.082625	66.566714	63.047745
1848.358085	73.422632	63.052750
1848.067383	65.495855	63.057754
1847.239229	67.458781	63.062759
1846.302885	60.984913	63.067764
1845.799929	73.010861	63.072769
1845.058784	69.042436	63.077774
1844.899199	61.322561	63.082778
1844.315900	64.062640	63.087783
1843.284353	69.705215	63.092788
1842.860120	66.991464	63.097793
1841.410790	69.558411	63.102798
1840.880499	58.016334	63.107802
1839.908682	79.894990	63.112807
1839.511917	70.321426	63.117812
1838.872284	71.676203	63.122817
1838.888120	77.362600	63.127822
1838.517695	62.914077	63.132826
1837.805695	69.234976	63.137831
1836.875595	66.601064	63.142836
1836.504154	66.438438	63.147841
1835.008320	74.013663	63.152846
1834.594472	67.364351	63.157850
1833.277219	70.579728	63.162855
1832.968782	68.892176	63.167860
1832.610069	68.104504	63.172865
1832.033565	71.488396	63.177870
1831.786362	71.552793	63.182874
1830.792810	76.519820	63.187879
1830.264786	81.489696	63.192884
1829.529011	76.758542	63.197889
1828.491649	76.733535	63.202894
1827.983309	70.980222	63.207898
1827.104478	71.513461	63.212903
1826.320723	61.676919	63.217908
1825.907658	69.564236	63.222913
1825.466155	69.295182	63.227918
1825.098078	62.938030	63.232922
1823.842471	67.255183	63.237927
1823.207243	64.241628	63.242932
1823.009570	69.241818	63.247937
1822.271011	71.482697	63.252942
1821.830561	60.004196	63.257946
1820.286722	73.188717	63.262951
1819.607064	68.509542	63.267956
1819.361637	68.214441	63.272961
1818.819854	69.569452	63.277966
1818.450159	62.609445	63.282970
1817.284063	62.011622	63.287975
1816.622712	65.042941	63.292980
1816.021305	65.625817	63.297985
1815.219590	70.090699	63.302990
1815.449168	58.171918	63.307994
1814.551140	66.809681	63.312999
1813.496347	72.612152	63.318004
1812.989708	68.146129	63.323009
1812.582084	74.142597	63.328014
1811.732544	59.849081	63.333018
1810.415231	68.374643	63.338023
1810.292841	63.028176	63.343028
1809.936846	68.380309	63.348033
1808.641401	68.340254	63.353038
1807.666687	57.367625	63.358042
1806.907948	61.886334	63.363047
1806.626363	67.462962	63.368052
1806.446519	61.491616	63.373057
1805.621254	73.309430	63.378062
1805.551935	62.417537	63.383066
1803.963293	71.133203	63.388071
1803.455689	62.345161	63.393076
1802.725652	56.724522	63.398081
1802.389270	67.646746	63.403086
1801.989054	60.311850	63.408090
1801.011182	62.710513	63.413095
1800.463775	67.733438	63.418100
1800.075508	70.083325	63.423105
1798.973490	69.671112	63.428110
1798.249032	60.235337	63.433114
1797.346118	62.245007	63.438119
1796.896940	67.883861	63.443124
1796.733645	60.468562	63.448129
1795.481314	60.717568	63.453134
1794.980367	60.643417	63.458138
1794.113252	66.469038	63.463143
1793.795635	73.408881	63.468148
1793.467631	73.521051	63.473153
1792.033498	76.654204	63.478158
1791.487349	68.325106	63.483162
1790.953086	69.488971	63.488167
1790.327289	62.789489	63.493172
1790.291250	67.481772	63.498177
1788.811963	74.847736	63.503182
1788.491607	62.091903	63.508186
1787.700628	69.111553	63.513191
1787.450022	66.089428	63.518196
1786.343632	67.198823	63.523201
1785.116964	68.421952	63.528206
1784.929097	62.465402	63.533210
1784.287517	67.538781	63.538215
1783.843620	62.957033	63.543220
1783.823867	55.874004	63.548225
1782.546894	68.762613	63.553230
1781.854463	60.717092	63.558234
1780.957798	71.617951	63.563239
1780.772386	61.503393	63.568244
1780.107246	57.206992	63.573249
1778.389053	73.293728	63.578254
1778.189409	66.348049	63.583258
1777.879968	73.436092	63.588263
1777.491791	70.665260	63.593268
1776.916976	76.519027	63.598273
1775.740301	65.452674	63.603278
1775.255168	65.395160	63.608282
1774.722712	74.768899	63.613287
1773.735994	60.216245	63.618292
1772.880553	65.001362	63.623297
1772.109914	68.152039	63.628302
1772.092644	66.124553	63.633306
1771.555775	72.210237	63.638311
1770.690188	58.052896	63.643316
1769.706931	64.330215	63.648321
1768.674707	65.555208	63.653326
1768.744853	66.738416	63.658330
1767.615711	68.725619	63.663335
1767.644284	64.037375	63.668340
1767.073022	63.866709	63.673345
1765.746348	71.484052	63.678350
1765.489345	56.283939	63.683354
1764.920108	71.451352	63.688359
1763.892680	65.934889	63.693364
1762.960899	71.056347	63.698369
1762.321834	74.656598	63.703374
1761.858964	65.261724	63.708378
1761.781306	71.236073	63.713383
1761.021567	66.311282	63.718388
1759.968725	68.238853	63.723393
1759.386434	62.899243	63.728398
1758.704961	60.460034	63.733402
1758.130122	67.568618	63.738407
1756.758767	67.006719	63.743412
1756.428210	68.095866	63.748417
1755.673311	76.368505	63.753422
1755.637444	67.466201	63.758426
1754.882208	60.848872	63.763431
1754.412473	64.067269	63.768436
1753.210420	65.873142	63.773441
1752.405859	69.519473	63.778446
1752.369597	63.924204	63.783450
1751.914675	73.778470	63.788455
1750.826754	71.078426	63.793460
1750.320099	66.612022	63.798465
1749.706698	68.792021	63.803470
1748.870169	71.085986	63.808474
1748.167470	73.331790	63.813479
1747.413522	67.275531	63.818484
1747.150316	63.617304	63.823489
1745.839835	60.903242	63.828494
1744.415830	59.796169	63.833498
1744.706134	63.002538	63.838503
1744.190079	63.222675	63.843508
1744.031134	66.958264	63.848513
1742.996872	64.491005	63.853518
1742.635594	69.995616	63.858522
1741.120288	67.213579	63.863527
1740.577358	69.154557	63.868532
1740.584693	59.082023	63.873537
1739.311399	66.073287	63.878542
1738.389443	66.358930	63.883546
1737.589763	67.516508	63.888551
1736.904526	60.672478	63.893556
1737.146075	71.793825	63.898561
1736.579019	65.552834	63.903566
1736.554277	64.217781	63.908570
1735.247035	63.662680	63.913575
1734.459821	66.813434	63.918580
1734.103442	71.671445	63.923585
1732.240401	74.435916	63.928590
1732.059906	63.214517	63.933594
1731.077963	64.453411	63.938599
1730.461456	64.318912	63.943604
1730.309135	59.733463	63.948609
1729.282135	72.858374	63.953614
1728.996225	64.466209	63.958618
1728.651782	71.386958	63.963623
1727.792161	65.717059	63.968628
1727.156785	63.626794	63.973633
1726.347788	67.372962	63.978638
1725.844552	68.378373	63.983642
1725.093466	70.980602	63.988647
1724.181137	70.854486	63.993652
1723.827108	69.431706	63.998657
1723.259974	67.171086	64.003662
1721.912169	59.896904	64.008666
1721.045613	68.461792	64.013671
1720.792092	71.085851	64.018676
1720.321616	63.994688	64.023681
1719.691166	65.677497	64.028686
1719.567074	69.349100	64.033690
1718.241473	73.102355	64.038695
1717.363281	67.306957	64.043700
1716.932241	67.257955	64.048705
1716.434648	77.822915	64.053710
1716.224212	63.764657	64.058714
1714.732791	64.209719	64.063719
1714.341931	59.520226	64.068724
1714.089899	61.236568	64.073729
1713.623444	69.947723	64.078734
1712.493302	61.102021	64.083738
1711.434164	64.617846	64.088743
1710.911628	67.642395	64.093748
1710.659442	61.716200	64.098753
1709.510340	65.940942	64.103758
1709.674077	59.123744	64.108762
1708.633859	73.046278	64.113767
1708.228043	72.159707	64.118772
1707.738304	68.474327	64.123777
1706.084367	63.796896	64.128782
1705.509111	66.525743	64.133786
1704.916455	67.165947	64.138791
1704.586432	64.715158	64.143796
1704.249948	62.109166	64.148801
1702.479981	64.202879	64.153806
1702.319427	63.395519	64.158810
1701.833583	62.684083	64.163815
1701.684140	64.727855	64.168820
1701.064724	57.144708	64.173825
1699.770987	68.841378	64.178830
1699.346897	65.478305	64.183834
1698.583801	74.797171	64.188839
1697.995790	67.342061	64.193844
1697.466422	62.990468	64.198849
1696.223114	75.357037	64.203854
1695.358684	73.765424	64.208858
1694.908927	62.987195	64.213863
1694.071101	73.601293	64.218868
1694.317983	64.873631	64.223873
1693.535751	60.091250	64.228878
1692.777576	53.420364	64.233882
1691.638926	67.197113	64.238887
1690.827523	61.685151	64.243892
1691.028420	62.160356	64.248897
1690.429155	67.386362	64.253902
1689.110628	61.342653	64.258906
1688.384125	70.371452	64.263911
1687.828954	63.162557	64.268916
1687.525704	62.024763	64.273921
1686.834809	71.956115	64.278926
1685.891487	62.529397	64.283930
1685.012254	70.305440	64.288935
1684.308843	66.234277	64.293940
1684.468133	65.961503	64.298945
1683.648782	68.902640	64.303950
1683.072440	64.250022	64.308954
1682.034073	60.271703	64.313959
1681.410223	61.244470	64.318964
1681.219851	61.833600	64.323969
1680.165523	67.464700	64.328974
1679.334307	67.799955	64.333978
1678.634886	61.273350	64.338983
1678.121787	73.580489	64.343988
1677.787258	63.680138	64.348993
1676.029559	62.075605	64.353998
1675.591850	56.272343	64.359002
1675.295947	57.086759	64.364007
1674.712704	62.564222	64.369012
1674.987691	64.199459	64.374017
1674.191791	67.843528	64.379022
1673.108179	55.950143	64.384026
1672.661143	69.057911	64.389031
1671.226150	69.526881	64.394036
1670.568486	61.166764	64.399041
1669.714524	70.084355	64.404046
1669.623135	51.858819	64.409050
1669.434893	58.977822	64.414055
1667.846370	63.689459	64.419060
1667.411856	54.288178	64.424065
1666.760455	63.455695	64.429070
1666.345363	67.750620	64.434074
1665.426570	68.882409	64.439079
1664.869985	71.561093	64.444084
1664.161062	55.832047	64.449089
1662.816455	62.794080	64.454094
1662.786273	59.978973	64.459098
1662.001753	58.663023	64.464103
1662.111401	63.098273	64.469108
1661.336325	59.439231	64.474113
1659.817853	65.936830	64.479118
1659.217572	63.277699	64.484122
1659.230236	73.943224	64.489127
1658.744055	70.801165	64.494132
1657.572978	67.061867	64.499137
1656.657193	64.471332	64.504142
1656.057544	54.242560	64.509146
1655.871416	66.625181	64.514151
1654.964839	59.712865	64.519156
1654.779540	54.069693	64.524161
1653.490554	61.358116	64.529166
1652.920747	58.260765	64.534170
1652.659561	62.130685	64.539175
1651.322478	61.737810	64.544180
1650.543556	65.227798	64.549185
1649.812181	66.185812	64.554190
1649.476690	60.611365	64.559194
1649.129744	59.097779	64.564199
1648.688271	62.247795	64.569204
1648.516990	58.246230	64.574209
1647.212779	64.746243	64.579214
1646.719587	57.404784	64.584218
1646.404394	62.745592	64.589223
1644.782902	62.511516	64.594228
1644.348842	56.827233	64.599233
1644.121526	59.545487	64.604238
1643.477893	54.358496	64.609242
1642.478651	60.211478	64.614247
1641.750063	54.853112	64.619252
1641.534916	58.936591	64.624257
1640.283956	64.146233	64.629262
1639.486550	61.406765	64.634266
1638.742749	65.944645	64.639271
1637.856575	58.994896	64.644276
1637.802413	51.628440	64.649281
1636.994089	63.305990	64.654286
1637.158886	58.426292	64.659290
1636.000362	60.037643	64.664295
1634.975320	68.151259	64.669300
1634.747212	64.005083	64.674305
1633.873661	66.931029	64.679310
1632.837504	61.317021	64.684314
1631.963514	62.415886	64.689319
1631.394340	63.753496	64.694324
1631.656709	51.276123	64.699329
1630.602610	58.319492	64.704334
1630.561169	62.996902	64.709338
1629.366140	59.616171	64.714343
1628.610313	61.262816	64.719348
1628.217904	53.299405	64.724353
1627.143246	58.450852	64.729358
1626.420683	55.651213	64.734362
1625.553995	62.905660	64.739367
1625.015817	61.793469	64.744372
1624.857118	61.307097	64.749377
1624.479635	62.052191	64.754382
1623.305926	65.922754	64.759386
1622.680028	64.540982	64.764391
1621.567016	66.743338	64.769396
1621.505217	68.854609	64.774401
1620.141943	65.457673	64.779406
1619.530492	63.695683	64.784410
1618.997777	63.060168	64.789415
1618.065883	64.217100	64.794420
1618.137980	64.884468	64.799425
1617.439711	67.690818	64.804430
1617.123403	59.200458	64.809434
1616.236958	60.455002	64.814439
1615.181849	66.818844	64.819444
1614.758422	55.029202	64.824449
1614.243307	65.361502	64.829454
1613.479997	66.197493	64.834458
1612.676079	56.976275	64.839463
1611.722374	65.674894	64.844468
1611.938662	58.698713	64.849473
1610.613752	67.881631	64.854478
1609.682291	68.002746	64.859482
1609.010183	64.407798	64.864487
1608.660632	60.412666	64.869492
1608.167907	62.642287	64.874497
1607.514656	65.330807	64.879502
1606.925258	59.609168	64.884506
1605.984354	53.845454	64.889511
1604.866436	58.867340	64.894516
1604.800697	50.998418	64.899521
1604.378665	66.259435	64.904526
1603.663629	64.572803	64.909530
1602.690606	56.112337	64.914535
1602.019847	61.400711	64.919540
1601.761487	49.280867	64.924545
1601.080655	55.818274	64.929550
1600.577921	59.305604	64.934554
1599.346141	55.929592	64.939559
1598.544059	60.765198	64.944564
1598.577715	50.784886	64.949569
1597.701771	59.533745	64.954574
1596.562160	48.193505	64.959578
1596.027606	58.019150	64.964583
1595.698060	60.674772	64.969588
1595.330424	59.275253	64.974593
1593.926737	60.118211	64.979598
1593.367636	61.317922	64.984602
1593.187957	59.374680	64.989607
1592.196760	57.164154	64.994612
1591.757134	57.516087	64.999617
1590.795255	64.786434	65.004622
1590.019141	52.125620	65.009626
1589.222772	59.999980	65.014631
1588.843037	67.458452	65.019636
1588.846317	55.428823	65.024641
1587.308792	54.851594	65.029646
1586.435528	58.448913	65.034650
1585.913744	56.382254	65.039655
1585.435396	57.964838	65.044660
1585.468059	55.303972	65.049665
1584.763381	62.392940	65.054670
1583.791398	60.949618	65.059674
1582.946366	65.361150	65.064679
1582.019502	64.202593	65.069684
1582.047747	59.912687	65.074689
1580.896260	61.038525	65.079694
1580.190665	65.018054	65.084698
1579.484038	63.456297	65.089703
1579.213898	66.366610	65.094708
1578.956224	61.860779	65.099713
1577.602646	60.304352	65.104718
1576.939869	58.908373	65.109722
1576.139366	58.447371	65.114727
1575.567044	72.811654	65.119732
1575.554110	65.517480	65.124737
1574.459632	58.385907	65.129742
1573.412565	57.447652	65.134746
1573.132932	57.143813	65.139751
1572.368295	58.955387	65.144756
1572.174995	53.566607	65.149761
1570.888019	69.946267	65.154766
1570.172464	61.507267	65.159770
1569.965328	58.142211	65.164775
1569.102867	64.035344	65.169780
1568.486463	61.188337	65.174785
1567.492613	62.633763	65.179790
1566.903810	65.031401	65.184794
1566.818013	62.088848	65.189799
1566.060370	62.714674	65.194804
1565.770695	58.375367	65.199809
1564.478539	69.019068	65.204814
1563.700957	63.800147	65.209818
1563.178669	59.322632	65.214823
1561.874882	64.917892	65.219828
1561.322073	57.436263	65.224833
1560.903274	61.544333	65.229838
1560.448524	62.488962	65.234842
1560.011990	53.040682	65.239847
1559.482669	55.237490	65.244852
1559.253935	51.070512	65.249857
1558.016064	63.259716	65.254862
1557.122673	59.555814	65.259866
1556.802360	55.877381	65.264871
1555.753736	64.599354	65.269876
1555.062370	54.596687	65.274881
1554.280685	58.705682	65.279886
1553.805389	54.050793	65.284890
1553.024889	56.614655	65.289895
1552.896679	58.271127	65.294900
1552.558965	52.496953	65.299905
1550.900659	61.530102	65.304910
1550.485771	59.342920	65.309914
1549.883549	63.496198	65.314919
1549.504114	58.221772	65.319924
1548.350504	54.895551	65.324929
1547.959908	60.902523	65.329934
1547.284252	61.975352	65.334938
1547.007605	60.175413	65.339943
1546.151479	58.811740	65.344948
1545.373599	56.201969	65.349953
1544.949613	61.822700	65.354958
1544.620207	61.595668	65.359962
1543.324134	54.084548	65.364967
1542.375622	61.996792	65.369972
1541.802914	56.323623	65.374977
1540.934481	55.753074	65.379982
1540.704635	48.764049	65.384986
1540.721400	57.840105	65.389991
1539.417660	60.393261	65.394996
1538.630584	55.989094	65.400001
1538.021531	59.929209	65.405006
1537.620047	57.730261	65.410010
1536.745634	49.389909	65.415015
1535.729674	57.152650	65.420020
1535.337573	56.554655	65.425025
1534.869873	58.598426	65.430030
1534.345535	58.302130	65.435034
1533.781150	55.643979	65.440039
1532.305014	57.224451	65.445044
1532.252551	60.479597	65.450049
1531.294560	60.609610	65.455054
1530.746769	54.650349	65.460058
1529.926614	52.508059	65.465063
1528.973943	56.952227	65.470068
1528.178987	51.977859	65.475073
1527.766099	63.274721	65.480078
1527.387069	54.004096	65.485082
1527.366158	62.556888	65.490087
1527.113741	61.424615	65.495092
1526.284021	64.551091	65.500097
1525.337398	70.157464	65.505102
1524.397663	61.458831	65.510106
1522.669373	52.333086	65.515111
1522.005486	62.467041	65.520116
1521.974441	55.888443	65.525121
1521.972180	60.495197	65.530126
1521.270313	62.881403	65.535130
1520.513653	58.000738	65.540135
1519.569836	62.710618	65.545140
1518.958795	60.671479	65.550145
1518.141922	57.391444	65.555150
1517.704077	69.728718	65.560154
1516.753052	59.014217	65.565159
1515.814568	68.191799	65.570164
1515.382577	60.089526	65.575169
1515.055943	60.678694	65.580174
1514.377438	62.020818	65.585178
1514.050880	57.006545	65.590183
1512.606157	59.969082	65.595188
1512.195951	49.528326	65.600193
1511.688618	61.852225	65.605198
1511.322401	52.813084	65.610202
1510.582360	53.359329	65.615207
1509.703267	56.363998	65.620212
1509.125793	58.349984	65.625217
1508.269817	52.775039	65.630222
1507.576824	61.743240	65.635226
1506.790824	57.460073	65.640231
1506.116057	58.192112	65.645236
1505.880491	51.395902	65.650241
1505.296450	54.426253	65.655246
1504.748597	53.181133	65.660250
1503.837548	57.101889	65.665255
1503.151438	67.676999	65.670260
1502.580215	63.381939	65.675265
1501.098847	52.524545	65.680270
1500.322676	51.542309	65.685274
1500.714348	57.761955	65.690279
1499.826972	51.926741	65.695284
1498.980410	51.727439	65.700289
1498.605388	48.982018	65.705294
1498.175285	58.127449	65.710298
1497.172901	49.769143	65.715303
1496.409663	52.936344	65.720308
1495.779555	48.530978	65.725313
1495.185903	62.548389	65.730318
1494.688201	57.523939	65.735322
1493.784264	59.866973	65.740327
1492.590933	63.382514	65.745332
1492.967973	57.692449	65.750337
1491.706606	61.485675	65.755342
1490.555700	61.173077	65.760346
1489.903913	55.499243	65.765351
1489.590996	58.306357	65.770356
1489.389312	52.319838	65.775361
1488.948857	58.882424	65.780366
1488.578599	59.839833	65.785370
1488.018874	65.687080	65.790375
1486.857105	59.358856	65.795380
1486.182000	55.283677	65.800385
1484.956135	60.768512	65.805390
1484.189944	55.345565	65.810394
1483.605227	46.503691	65.815399
1483.116729	57.487452	65.820404
1482.436764	53.468761	65.825409
1482.071824	59.317797	65.830414
1481.176018	59.892680	65.835418
1480.420037	51.710483	65.840423
1479.742476	64.290483	65.845428
1479.764216	52.555723	65.850433
1478.938635	60.230626	65.855438
1477.827393	62.184428	65.860442
1476.970072	58.101755	65.865447
1476.237831	58.556280	65.870452
1476.600673	57.633688	65.875457
1475.645994	56.110852	65.880462
1474.673741	60.723767	65.885466
1474.127631	57.308979	65.890471
1473.378543	71.658514	65.895476
1472.618627	53.399426	65.900481
1472.223990	63.034949	65.905486
1471.716991	60.090682	65.910490
1471.401223	55.457050	65.915495
1469.658514	59.034260	65.920500
1469.415025	52.456506	65.925505
1468.574254	66.412800	65.930510
1468.179798	61.022539	65.935514
1467.023018	58.194226	65.940519
1465.856926	61.585510	65.945524
1465.780149	56.302712	65.950529
1464.634220	61.398491	65.955534
1464.540802	60.964106	65.960538
1464.632859	61.392407	65.965543
1463.869239	71.688695	65.970548
1463.291985	60.389205	65.975553
1462.036225	59.981277	65.980558
1461.466036	64.951673	65.985562
1461.219031	57.117340	65.990567
1459.834726	57.599796	65.995572
1459.321005	54.936932	66.000577
1458.590561	59.844365	66.005582
1458.020021	59.791237	66.010586
1457.710832	54.750316	66.015591
1457.211323	66.464221	66.020596
1456.342648	55.612494	66.025601
1455.340778	62.536032	66.030606
1454.614001	61.316017	66.035610
1454.485007	58.949258	66.040615
1453.761201	72.184912	66.045620
1452.432867	57.942678	66.050625
1452.036702	63.969158	66.055630
1451.617774	57.132498	66.060634
1451.360180	61.064565	66.065639
1450.441176	65.054188	66.070644
1449.169410	54.387901	66.075649
1448.784211	64.669147	66.080654
1447.978257	62.509046	66.085658
1447.442917	55.566398	66.090663
1446.889711	60.231927	66.095668
1446.247471	58.094723	66.100673
1445.528025	57.965246	66.105678
1444.838976	57.941088	66.110682
1444.539437	50.055361	66.115687
1443.804668	56.739373	66.120692
1443.027538	51.404752	66.125697
1442.648202	56.615228	66.130702
1441.530586	54.118099	66.135706
1441.545607	48.512896	66.140711
1440.354634	57.828032	66.145716
1439.626966	53.951719	66.150721
1439.130329	55.796774	66.155726
1438.003237	56.650058	66.160730
1437.032978	56.962969	66.165735
1436.417318	59.331270	66.170740
1436.007621	55.243037	66.175745
1435.613336	58.378276	66.180750
1435.182891	59.416646	66.185754
1435.055563	56.560152	66.190759
1433.917822	59.606342	66.195764
1433.525784	49.620759	66.200769
1432.538919	61.442947	66.205774
1431.801027	67.593840	66.210778
1430.657976	50.963041	66.215783
1429.959352	59.315263	66.220788
1429.695656	58.372023	66.225793
1429.262312	66.971722	66.230798
1428.679697	63.738048	66.235802
1428.014783	51.998862	66.240807
1427.116549	64.319410	66.245812
1426.244174	55.068909	66.250817
1425.856306	58.107923	66.255822
1425.383627	62.476262	66.260826
1424.432466	57.074725	66.265831
1423.237224	63.132988	66.270836
1422.928730	59.808186	66.275841
1422.289267	55.996905	66.280846
1421.788798	53.235466	66.285850
1421.772865	55.552031	66.290855
1420.324042	58.881197	66.295860
1419.731495	52.266096	66.300865
1419.172898	56.669271	66.305870
1418.722162	63.119151	66.310874
1418.252311	57.307219	66.315879
1416.966368	65.071982	66.320884
1416.268683	53.556686	66.325889
1415.929206	57.434877	66.330894
1415.714241	66.389940	66.335898
1414.220542	60.016717	66.340903
1413.839786	61.671816	66.345908
1412.983458	64.016582	66.350913
1412.824304	67.837068	66.355918
1412.265532	58.884977	66.360922
1411.286275	58.433284	66.365927
1409.971099	67.987576	66.370932
1409.726914	58.823354	66.375937
1409.354235	62.823277	66.380942
1408.939365	66.653590	66.385946
1408.238505	60.529506	66.390951
1406.948296	63.552460	66.395956
1406.886552	55.578665	66.400961
1406.320126	59.029937	66.405966
1405.276340	57.908403	66.410970
1404.501840	53.676182	66.415975
1403.437937	59.726175	66.420980
1403.420969	56.692115	66.425985
1403.007171	57.990520	66.430990
1401.772025	57.624076	66.435994
1401.323181	59.698575	66.440999
1400.477362	61.089482	66.446004
1400.300899	47.184557	66.451009
1399.969688	60.728770	66.456014
1398.517977	51.877037	66.461018
1397.820807	56.667074	66.466023
1396.823839	53.064619	66.471028
1396.840565	51.379071	66.476033
1396.446015	51.823563	66.481038
1395.310383	54.885976	66.486042
1394.619724	54.420411	66.491047
1393.967962	66.276424	66.496052
1393.403341	55.763044	66.501057
1393.200528	59.559425	66.506062
1392.178997	59.879936	66.511066
1391.524522	54.624193	66.516071
1390.970387	56.289630	66.521076
1390.655566	59.531658	66.526081
1389.444312	50.701529	66.531086
1388.612071	62.178715	66.536090
1388.248179	57.166901	66.541095
1387.625974	62.678679	66.546100
1386.365301	52.947183	66.551105
1385.482555	53.869568	66.556110
1384.845292	58.101877	66.561114
1384.683129	50.971817	66.566119
1384.121901	63.698078	66.571124
1383.980400	58.008751	66.576129
1383.567020	53.162508	66.581134
1382.470301	61.997727	66.586138
1381.723880	54.475859	66.591143
1380.871054	59.186364	66.596148
1380.089770	57.287303	66.601153
1378.965010	60.523904	66.606158
1378.302685	60.716617	66.611162
1378.206946	69.888102	66.616167
1377.640597	62.743939	66.621172
1377.383056	56.592921	66.626177
1376.515715	56.392855	66.631182
1375.600330	61.205250	66.636186
1375.138363	47.146711	66.641191
1374.545301	62.072657	66.646196
1373.640108	52.667139	66.651201
1372.562793	62.776740	66.656206
1371.867406	54.110534	66.661210
1371.660334	51.212435	66.666215
1371.089192	60.117152	66.671220
1370.728780	55.049879	66.676225
1369.403068	57.432764	66.681230
1368.792078	57.607613	66.686234
1368.587631	57.879440	66.691239
1368.027123	55.507610	66.696244
1367.026767	51.039335	66.701249
1366.184686	53.511924	66.706254
1365.697746	64.396740	66.711258
1365.618585	55.479791	66.716263
1364.387781	60.112113	66.721268
1363.318993	54.782436	66.726273
1362.646385	59.223289	66.731278
1362.147249	54.126083	66.736282
1361.710298	51.418118	66.741287
1360.961395	55.373107	66.746292
1360.398019	44.853608	66.751297
1359.484419	50.492630	66.756302
1358.776349	64.447523	66.761306
1358.394508	53.921415	66.766311
1358.210740	60.499666	66.771316
1357.507912	55.907832	66.776321
1356.228382	49.989001	66.781326
1355.354772	51.853992	66.786330
1355.277131	48.871373	66.791335
1354.786035	51.975820	66.796340
1353.961657	54.681422	66.801345
1353.220835	50.957764	66.806350
1352.112150	56.129682	66.811354
1352.255459	53.088714	66.816359
1351.024074	53.998157	66.821364
1350.265885	59.560845	66.826369
1349.841866	54.388416	66.831374
1349.415754	58.320517	66.836378
1348.928022	52.358113	66.841383
1347.417607	55.200496	66.846388
1346.781846	45.353754	66.851393
1346.079530	55.605597	66.856398
1345.640876	61.104902	66.861402
1345.567195	47.468957	66.866407
1344.903360	52.552882	66.871412
1344.102862	46.435216	66.876417
1343.299327	51.238728	66.881422
1342.683245	48.268156	66.886426
1342.071494	42.126865	66.891431
1340.970036	58.355961	66.896436
1340.216251	53.133411	66.901441
1339.900245	52.018747	66.906446
1339.320051	55.323571	66.911450
1339.510524	52.595040	66.916455
1338.253510	62.815535	66.921460
1337.431966	53.916734	66.926465
1336.563193	44.392108	66.931470
1335.533465	55.907046	66.936474
1335.192881	52.430255	66.941479
1333.992217	51.583081	66.946484
1333.787003	56.442451	66.951489
1333.277687	56.320438	66.956494
1333.051283	57.849255	66.961498
1332.349613	49.875287	66.966503
1331.084187	53.129660	66.971508
1330.811232	51.616461	66.976513
1330.666618	53.530335	66.981518
1329.425806	63.014277	66.986522
1328.121409	51.706285	66.991527
1327.267168	56.234283	66.996532
1327.088154	50.815453	67.001537
1326.824211	45.055917	67.006542
1326.268745	57.889338	67.011546
1325.898367	47.908752	67.016551
1324.713199	55.682326	67.021556
1323.731272	48.721818	67.026561
1323.331128	48.271264	67.031566
1322.470785	61.372395	67.036570
1322.541539	43.788235	67.041575
1321.380950	52.513211	67.046580
1321.097774	40.169133	67.051585
1320.581562	53.633298	67.056590
1319.125998	51.789683	67.061594
1318.627274	50.223165	67.066599
1317.502124	53.914557	67.071604
1317.464763	41.093418	67.076609
1316.855673	46.013242	67.081614
1316.607838	50.699915	67.086618
1315.224602	49.413892	67.091623
1314.667386	48.837077	67.096628
1314.277510	43.225017	67.101633
1313.815842	46.054836	67.106638
1313.012607	51.068290	67.111642
1311.881226	48.322510	67.116647
1310.985648	61.103241	67.121652
1310.898445	56.523652	67.126657
1310.546214	55.458215	67.131662
1309.704551	56.843293	67.136666
1308.982463	49.691471	67.141671
1308.074144	52.779325	67.146676
1307.475022	56.962876	67.151681
1307.009980	57.974021	67.156686
1306.370655	60.638477	67.161690
1305.247957	48.669814	67.166695
1304.675106	49.081682	67.171700
1303.905850	54.681397	67.176705
1303.725035	44.142207	67.181710
1303.339708	50.508653	67.186714
1302.529272	49.863879	67.191719
1301.407952	56.635786	67.196724
1301.060051	50.972331	67.201729
1300.734043	53.116986	67.206734
1299.381178	54.253676	67.211738
1299.079906	45.543704	67.216743
1298.057656	52.115105	67.221748
1297.384008	49.197419	67.226753
1297.348355	57.592062	67.231758
1296.307096	53.796695	67.236762
1295.770366	44.329704	67.241767
1295.189997	51.538317	67.246772
1294.478404	51.278840	67.251777
1293.706944	49.656785	67.256782
1292.668659	51.993639	67.261786
1292.220911	44.039367	67.266791
1291.522682	44.542171	67.271796
1291.082588	49.234523	67.276801
1290.851072	48.665897	67.281806
1289.785109	51.545490	67.286810
1289.180142	48.282116	67.291815
1288.809408	53.293763	67.296820
1287.874266	54.263026	67.301825
1286.607958	56.637735	67.306830
1285.801053	46.904381	67.311834
1285.572332	44.471026	67.316839
1284.955205	58.341267	67.321844
1284.831728	57.967293	67.326849
1284.010840	45.679353	67.331854
1283.082500	58.359118	67.336858
1282.501442	55.178489	67.341863
1281.736441	57.517505	67.346868
1281.442818	51.155189	67.351873
1280.167740	54.141238	67.356878
1279.447698	58.444173	67.361882
1279.036926	57.831239	67.366887
1278.868364	56.026632	67.371892
1277.956535	51.915442	67.376897
1277.260760	45.878938	67.381902
1276.048058	63.665695	67.386906
1276.019455	56.382521	67.391911
1275.133364	56.203840	67.396916
1274.826379	49.094639	67.401921
1273.926493	60.228163	67.406926
1273.324792	59.898957	67.411930
1272.458953	51.355110	67.416935
1272.015463	53.397912	67.421940
1271.313139	56.169072	67.426945
1270.596025	60.061395	67.431950
1269.992163	69.435119	67.436954
1269.289321	58.686494	67.441959
1269.054340	55.204656	67.446964
1267.907450	53.506359	67.451969
1267.164765	52.147394	67.456974
1266.316867	55.580946	67.461978
1266.477792	52.585513	67.466983
1264.928528	63.277610	67.471988
1264.418960	48.445706	67.476993
1263.567857	45.100535	67.481998
1263.064181	58.928064	67.487002
1263.076371	44.842850	67.492007
1262.251462	49.320835	67.497012
1261.296537	41.901009	67.502017
1260.579021	45.030410	67.507022
1259.684782	58.318913	67.512026
1259.567401	51.395136	67.517031
1258.968328	53.889686	67.522036
1258.068357	54.585710	67.527041
1257.755827	52.856670	67.532046
1256.694630	54.008959	67.537050
1256.167316	55.050505	67.542055
1254.810469	60.503336	67.547060
1254.646395	53.041264	67.552065
1254.056643	55.228707	67.557070
1253.431249	56.341121	67.562074
1253.190592	44.232524	67.567079
1252.244714	55.253137	67.572084
1250.981264	57.260672	67.577089
1250.447947	56.293344	67.582094
1249.781255	56.370775	67.587098
1249.790154	48.279911	67.592103
1248.758886	54.073296	67.597108
1247.762988	58.822126	67.602113
1247.468073	54.745449	67.607118
1246.646265	65.114859	67.612122
1246.470792	51.994488	67.617127
1245.256085	61.938159	67.622132
1244.542269	52.883184	67.627137
1244.154371	54.180717	67.632142
1243.300861	56.804483	67.637146
1243.450902	51.984161	67.642151
1242.338594	52.887058	67.647156
1241.398305	51.693370	67.652161
1240.921586	53.838963	67.657166
1239.908514	49.878926	67.662170
1239.820906	51.490161	67.667175
1238.880931	56.090082	67.672180
1238.177835	57.321190	67.677185
1238.178477	45.775201	67.682190
1237.100438	54.677495	67.687194
1236.297288	53.054953	67.692199
1235.341497	54.834564	67.697204
1234.869769	61.053578	67.702209
1234.536119	53.849477	67.707214
1233.551560	63.630596	67.712218
1232.569697	51.352465	67.717223
1232.095290	50.392027	67.722228
1231.535792	48.740008	67.727233
1230.931628	50.217850	67.732238
1230.613331	63.667477	67.737242
1229.718452	59.318932	67.742247
1228.404108	61.749640	67.747252
1228.205030	59.828686	67.752257
1227.913942	53.347132	67.757262
1226.831144	59.029351	67.762266
1226.313957	52.880966	67.767271
1225.412101	62.119004	67.772276
1224.546293	62.826158	67.777281
1224.407428	49.948592	67.782286
1224.261199	63.024564	67.787290
1223.543790	51.314945	67.792295
1222.214755	60.430339	67.797300
1221.762970	62.487197	67.802305
1221.271158	57.059563	67.807310
1219.817221	58.226999	67.812314
1219.430719	52.569768	67.817319
1218.875404	63.626937	67.822324
1218.367717	53.519488	67.827329
1217.940627	51.071155	67.832334
1217.113409	59.436325	67.837338
1216.365771	55.233488	67.842343
1215.594884	62.274606	67.847348
1215.003779	54.004246	67.852353
1214.654317	59.322897	67.857358
1213.747595	66.466611	67.862362
1213.137614	56.126425	67.867367
1212.322194	60.236102	67.872372
1211.665996	60.225298	67.877377
1211.314838	59.093372	67.882382
1210.353707	51.465418	67.887386
1209.657130	47.420808	67.892391
1208.873411	53.589821	67.897396
1208.610273	52.334673	67.902401
1208.204540	54.890068	67.907406
1207.118535	63.511117	67.912410
1206.507203	49.165181	67.917415
1205.433262	55.365727	67.922420
1204.913142	59.760355	67.927425
1204.718032	54.446523	67.932430
1203.945943	64.996491	67.937434
1203.187252	53.113558	67.942439
1202.456548	65.787915	67.947444
1201.885742	58.146812	67.952449
1201.611975	46.488739	67.957454
1200.655966	62.136390	67.962458
1199.815663	54.610112	67.967463
1198.995008	61.098464	67.972468
1198.726897	55.145847	67.977473
1198.612773	49.558427	67.982478
1196.840043	53.446370	67.987482
1196.454022	50.642868	67.992487
1196.190328	55.861969	67.997492
1195.432145	52.408931	68.002497
1194.752337	46.141168	68.007502
1193.424208	61.174802	68.012506
1192.822474	47.433119	68.017511
1192.559963	55.300175	68.022516
1192.120857	52.768248	68.027521
1191.855325	46.994790	68.032526
1190.540528	56.856529	68.037530
1189.939749	44.785524	68.042535
1189.501192	50.258367	68.047540
1188.794512	51.606142	68.052545
1188.158990	44.098492	68.057550
1187.261413	51.732059	68.062554
1186.901115	43.963745	68.067559
1186.440317	44.291706	68.072564
1185.195655	58.951855	68.077569
1184.645295	51.330547	68.082574
1183.970018	52.365856	68.087578
1183.548151	45.189897	68.092583
1183.328783	52.320916	68.097588
1182.276408	48.219998	68.102593
1181.501341	48.753735	68.107598
1180.620277	49.857040	68.112602
1179.995120	49.017545	68.117607
1179.321403	47.192073	68.122612
1177.998910	51.962095	68.127617
1177.601851	48.934312	68.132622
1177.141347	55.583225	68.137626
1176.784216	47.722398	68.142631
1176.557772	54.140192	68.147636
1175.649171	49.907295	68.152641
1174.909365	47.356992	68.157646
1173.764228	51.843240	68.162650
1173.340325	51.131911	68.167655
1173.145860	59.524133	68.172660
1172.311194	58.040808	68.177665
1171.458797	48.967345	68.182670
1170.621189	57.474815	68.187674
1170.043322	53.753684	68.192679
1169.765630	59.320560	68.197684
1168.390422	58.423184	68.202689
1167.940109	50.067943	68.207694
1167.052479	58.661738	68.212698
1166.939543	52.634796	68.217703
1166.476883	52.674935	68.222708
1165.768601	53.320391	68.227713
1164.958038	54.582540	68.232718
1164.027038	55.559800	68.237722
1163.530032	48.407365	68.242727
1162.950635	51.915740	68.247732
1162.560645	51.003221	68.252737
1161.671473	47.503543	68.257742
1160.709262	48.482200	68.262746
1160.682796	56.289103	68.267751
1159.956205	51.260478	68.272756
1158.580284	58.003372	68.277761
1158.170521	53.332979	68.282766
1157.339508	51.254588	68.287770
1157.276077	52.402627	68.292775
1156.551335	48.261012	68.297780
1155.490101	53.507727	68.302785
1154.998123	51.386680	68.307790
1154.104204	56.747241	68.312794
1154.036477	45.706760	68.317799
1152.895412	51.355150	68.322804
1151.947673	48.812429	68.327809
1151.665590	50.917992	68.332814
1151.120650	48.218281	68.337818
1150.762603	53.107764	68.342823
1149.756029	45.345907	68.347828
1148.471412	55.194984	68.352833
1148.295357	47.095932	68.357838
1147.604558	55.452745	68.362842
1147.319966	55.003340	68.367847
1146.976925	56.188993	68.372852
1145.303074	55.735898	68.377857
1144.958813	51.482164	68.382862
1144.337574	61.495540	68.387866
1143.993458	49.812416	68.392871
1142.847228	52.379744	68.397876
1142.415496	51.551343	68.402881
1142.261274	43.143439	68.407886
1141.136877	53.509002	68.412890
1141.033751	45.296811	68.417895
1139.622990	51.168216	68.422900
1138.882711	42.829083	68.427905
1138.630402	50.304801	68.432910
1137.901628	61.572843	68.437914
1137.097393	51.823280	68.442919
1136.225720	46.177300	68.447924
1135.672708	48.565689	68.452929
1135.292342	48.150841	68.457934
1134.928935	57.018016	68.462938
1133.996162	53.823031	68.467943
1132.946949	51.450839	68.472948
1132.322887	49.806730	68.477953
1132.031991	44.841662	68.482958
1131.706510	57.382682	68.487962
1130.382381	43.599328	68.492967
1129.725416	53.823279	68.497972
1129.156871	52.616089	68.502977
1129.032816	49.893258	68.507982
1127.619681	53.660443	68.512986
1126.951341	52.605334	68.517991
1126.464267	46.315241	68.522996
1125.769793	53.595502	68.528001
1125.521347	50.853709	68.533006
1124.652491	56.376553	68.538010
1123.735753	44.197043	68.543015
1123.142693	57.114653	68.548020
1122.391934	58.350386	68.553025
1122.745745	40.029412	68.558030
1121.067231	54.071123	68.563034
1120.499487	51.451500	68.568039
1119.962944	50.151599	68.573044
1119.148576	56.119433	68.578049
1118.947256	50.122234	68.583054
1117.603632	56.791715	68.588058
1117.059606	48.912770	68.593063
1116.541831	55.696616	68.598068
1116.321166	61.084789	68.603073
1116.061194	51.288614	68.608078
1114.658293	56.222412	68.613082
1114.059968	51.939558	68.618087
1113.623039	53.973352	68.623092
1112.670454	48.004143	68.628097
1111.657414	44.358723	68.633102
1111.093539	52.198039	68.638106
1110.669066	49.793083	68.643111
1110.352598	50.508422	68.648116
1109.406939	53.693485	68.653121
1109.077999	44.380812	68.658126
1107.603806	48.550014	68.663130
1107.117935	47.164074	68.668135
1106.600172	48.331492	68.673140
1106.134771	52.033893	68.678145
1105.785758	40.227682	68.683150
1105.013267	50.608380	68.688154
1104.301976	50.012581	68.693159
1103.544639	45.015680	68.698164
1102.993734	49.033891	68.703169
1102.200072	48.199183	68.708174
1101.047503	48.806257	68.713178
1100.688495	43.296305	68.718183
1100.264599	45.453387	68.723188
1099.536980	48.836365	68.728193
1098.790756	44.034133	68.733198
1097.852728	51.259393	68.738202
1097.626416	45.497388	68.743207
1097.268869	51.520412	68.748212
1096.062266	58.102885	68.753217
1095.265758	45.431109	68.758222
1094.312886	51.044127	68.763226
1093.907152	48.225854	68.768231
1093.570918	47.629777	68.773236
1093.058359	53.259367	68.778241
1092.804699	43.579746	68.783246
1091.629874	50.281505	68.788250
1090.975569	37.067124	68.793255
1090.528319	45.959701	68.798260
1089.491442	47.276009	68.803265
1088.747218	47.724745	68.808270
1087.925660	54.242468	68.813274
1087.568222	45.506227	68.818279
1087.175484	44.492349	68.823284
1086.579893	51.474641	68.828289
1085.747168	51.603023	68.833294
1085.158757	51.901533	68.838298
1084.856239	46.655052	68.843303
1083.848985	47.449209	68.848308
1082.487888	53.593556	68.853313
1082.274723	45.022471	68.858318
1081.660018	49.002663	68.863322
1081.165562	42.400043	68.868327
1080.066333	47.149222	68.873332
1078.819940	50.746162	68.878337
1078.656909	44.088368	68.883342
1078.546204	49.672433	68.888346
1078.016188	55.066999	68.893351
1077.521758	49.569580	68.898356
1076.524575	48.017397	68.903361
1075.726121	45.153487	68.908366
1074.855342	54.192011	68.913370
1074.663525	47.246266	68.918375
1073.739110	52.966908	68.923380
1073.075514	50.947886	68.928385
1072.840752	51.471219	68.933390
1071.529600	58.519997	68.938394
1071.225186	47.439534	68.943399
1070.189745	55.650905	68.948404
1069.417300	53.218308	68.953409
1069.129006	53.409378	68.958414
1068.254944	55.264622	68.963418
1068.086922	52.921146	68.968423
1067.295333	49.137950	68.973428
1066.344791	57.362414	68.978433
1065.661406	53.867778	68.983438
1064.777457	58.444315	68.988442
1064.876675	53.798086	68.993447
1064.118273	46.477679	68.998452
1063.114835	52.138041	69.003457
1062.725244	48.249300	69.008462
1061.959189	49.113862	69.013466
1061.309285	46.273462	69.018471
1060.226417	45.909448	69.023476
1059.363131	58.409540	69.028481
1059.316189	45.945321	69.033486
1058.767406	52.873417	69.038490
1058.152391	46.205397	69.043495
1057.114637	49.655303	69.048500
1056.227710	58.324773	69.053505
1056.096574	50.336453	69.058510
1055.318260	50.322898	69.063514
1055.072112	42.435195	69.068519
1053.885563	49.467766	69.073524
1052.950078	58.065029	69.078529
1053.138098	46.458950	69.083534
1052.016050	58.369834	69.088538
1050.826799	50.797172	69.093543
1050.257504	52.231564	69.098548
1049.653410	50.006578	69.103553
1049.527535	48.110994	69.108558
1048.988087	49.479094	69.113562
1048.141190	44.074406	69.118567
1046.933632	51.955665	69.123572
1046.264701	48.703678	69.128577
1046.172389	49.930475	69.133582
1045.648994	59.008589	69.138586
1044.860578	50.204848	69.143591
1044.183632	57.578820	69.148596
1043.033257	54.656764	69.153601
1043.144060	53.584290	69.158606
1041.485539	55.967012	69.163610
1040.954181	50.790905	69.168615
1040.536782	54.674555	69.173620
1039.614004	54.433123	69.178625
1039.633522	47.039897	69.183630
1038.942409	49.247875	69.188634
1038.591846	44.138306	69.193639
1037.358500	44.671599	69.198644
1036.410668	44.114344	69.203649
1036.588446	41.196154	69.208654
1035.554800	44.933108	69.213658
1034.846995	41.161230	69.218663
1034.119886	39.176776	69.223668
1033.468356	44.025732	69.228673
1033.485433	44.237137	69.233678
1031.932156	44.198410	69.238682
1030.991607	42.355501	69.243687
1031.008653	36.573936	69.248692
1030.408151	39.072302	69.253697
1029.434046	43.502445	69.258702
1028.392269	46.733188	69.263706
1027.870214	41.696802	69.268711
1027.604645	38.363903	69.273716
1026.930831	34.203333	69.278721
1026.586820	33.418735	69.283726
1025.313916	34.571800	69.288730
1024.702183	30.193768	69.293735
1024.115540	43.942722	69.298740
1023.896903	48.601106	69.303745
1023.203192	34.417361	69.308750
1021.910043	45.341145	69.313754
1021.458109	43.544820	69.318759
1021.080578	41.616154	69.323764
1020.284304	46.492267	69.328769
1019.485683	42.204656	69.333774
1018.593651	49.060093	69.338778
1018.279391	39.788343	69.343783
1018.052067	42.397663	69.348788
1016.983462	48.925330	69.353793
1016.163149	47.808242	69.358798
1015.145609	48.741535	69.363802
1014.513120	50.414110	69.368807
1014.185140	46.638369	69.373812
1013.700211	42.596629	69.378817
1013.685994	45.845208	69.383822
1012.356978	47.026438	69.388826
1011.665957	44.620565	69.393831
1011.589498	45.692681	69.398836
1010.158421	45.536723	69.403841
1009.893661	44.157927	69.408846
1009.215435	36.877093	69.413850
1008.557729	38.213346	69.418855
1007.338864	39.987917	69.423860
1006.281132	42.942726	69.428865
1005.976346	38.758038	69.433870
1005.520494	50.851658	69.438874
1005.071127	40.476922	69.443879
1004.616710	43.071451	69.448884
1004.270597	43.522676	69.453889
1003.532180	43.235074	69.458894
1002.219381	40.333743	69.463898
1001.622866	41.445976	69.468903
1001.179555	46.150335	69.473908
1000.009798	47.361923	69.478913
999.375409	38.626159	69.483918
998.759147	46.721934	69.488922
998.215376	44.198877	69.493927
997.829685	39.808583	69.498932
997.386168	44.115498	69.503937
996.940370	37.221946	69.508942
995.789267	45.726666	69.513946
995.269135	43.316003	69.518951
994.800097	38.948271	69.523956
993.556624	42.636302	69.528961
993.005751	40.268007	69.533966
992.174488	43.988861	69.538970
991.555921	42.729470	69.543975
991.457777	42.123020	69.548980
990.622208	42.152831	69.553985
989.613447	44.497710	69.558990
989.270272	52.137794	69.563994
988.816596	42.959393	69.568999
988.376464	34.600871	69.574004
987.031433	47.767638	69.579009
986.803055	40.115311	69.584014
985.957315	40.530924	69.589018
985.287403	43.175780	69.594023
984.767231	46.991771	69.599028
983.491957	57.739228	69.604033
983.495142	47.508029	69.609038
983.096778	45.779898	69.614042
982.003430	37.286941	69.619047
981.114978	40.448409	69.624052
980.378677	45.391225	69.629057
979.920153	38.761551	69.634062
979.565038	41.249475	69.639066
978.399791	39.060606	69.644071
977.684712	36.425583	69.649076
976.933250	41.333497	69.654081
976.757930	38.983778	69.659086
976.587446	44.447029	69.664090
975.722671	48.893587	69.669095
974.853791	41.449236	69.674100
973.566084	45.535221	69.679105
973.537646	49.078326	69.684110
972.099033	48.156736	69.689114
971.510881	45.767198	69.694119
971.696663	50.674068	69.699124
970.676517	52.233442	69.704129
970.740795	37.523207	69.709134
969.692628	45.071272	69.714138
968.684393	48.488508	69.719143
968.269858	41.439218	69.724148
967.471950	51.881509	69.729153
966.118035	43.961704	69.734158
965.289803	42.795063	69.739162
965.381958	42.287858	69.744167
964.779241	36.073257	69.749172
963.738031	47.223494	69.754177
963.840665	38.567162	69.759182
963.106522	39.300359	69.764186
962.040767	41.117005	69.769191
961.440406	42.057410	69.774196
960.560990	44.805645	69.779201
960.398973	37.139984	69.784206
959.434490	46.483097	69.789210
958.637546	39.099454	69.794215
958.138347	29.772950	69.799220
957.648533	42.137233	69.804225
957.109440	42.618749	69.809230
956.027876	50.326083	69.814234
955.125725	41.749469	69.819239
954.690115	43.573453	69.824244
954.068467	43.795964	69.829249
953.550058	40.327173	69.834254
953.353479	46.795498	69.839258
952.008173	51.433693	69.844263
951.343212	41.133389	69.849268
950.480543	53.281289	69.854273
950.555860	44.218338	69.859278
950.157470	42.881378	69.864282
948.696676	36.482966	69.869287
948.378414	40.708829	69.874292
947.836385	40.044198	69.879297
946.908462	37.893241	69.884302
946.047442	42.098776	69.889306
945.575984	49.162834	69.894311
945.052475	45.970823	69.899316
944.600357	44.827002	69.904321
943.706758	36.261561	69.909326
942.598922	40.665280	69.914330
942.075419	39.733018	69.919335
941.868197	44.714296	69.924340
941.354196	45.326903	69.929345
940.409364	46.143159	69.934350
939.207843	47.537823	69.939354
938.707579	45.220469	69.944359
938.443772	29.516492	69.949364
937.716447	43.987000	69.954369
937.095068	38.818044	69.959374
936.169292	43.319261	69.964378
935.510203	38.380173	69.969383
935.023817	32.681678	69.974388
934.262048	41.237350	69.979393
934.133756	38.782085	69.984398
933.015851	44.926254	69.989402
932.513333	48.223332	69.994407
932.100705	41.311082	69.999412
931.105517	56.995837	70.004417
930.164227	54.056948	70.009422
929.426515	52.115771	70.014426
929.232973	45.567818	70.019431
928.902474	44.075951	70.024436
927.827242	50.898436	70.029441
927.178807	38.154386	70.034446
926.464599	54.875694	70.039450
926.121865	53.574596	70.044455
925.333704	48.564459	70.049460
924.210064	48.910448	70.054465
923.812410	47.593100	70.059470
923.235147	48.908481	70.064474
922.732990	45.181134	70.069479
921.777540	45.248857	70.074484
920.906784	45.229841	70.079489
920.333144	38.735545	70.084494
919.923299	49.141371	70.089498
919.443628	42.589929	70.094503
918.490578	43.717053	70.099508
917.150294	45.488759	70.104513
916.839169	42.847714	70.109518
916.791060	42.318350	70.114522
916.242409	49.497861	70.119527
915.588819	50.345157	70.124532
914.312742	43.488824	70.129537
914.026072	38.254257	70.134542
913.548151	37.767719	70.139546
912.691900	47.547803	70.144551
911.950461	47.015219	70.149556
910.929772	48.380891	70.154561
910.668286	49.265631	70.159566
910.109222	48.344594	70.164570
908.872575	52.798408	70.169575
908.058308	44.154257	70.174580
907.489692	54.257297	70.179585
907.306964	52.290145	70.184590
906.865677	46.791942	70.189594
905.966841	49.827707	70.194599
905.642716	38.661846	70.199604
904.241336	52.097608	70.204609
903.844135	49.195399	70.209614
903.584099	46.129969	70.214618
902.909787	48.500472	70.219623
902.017737	46.597576	70.224628
901.277562	50.495068	70.229633
900.727382	41.871211	70.234638
900.293192	43.192482	70.239642
899.660168	46.610199	70.244647
898.463797	46.810764	70.249652
897.798707	57.451355	70.254657
897.419218	50.996037	70.259662
896.840346	43.609398	70.264666
896.299409	41.124552	70.269671
895.165913	35.351381	70.274676
894.177218	47.219301	70.279681
894.022386	43.167616	70.284686
893.609218	43.968605	70.289690
892.998059	48.739610	70.294695
891.884071	49.416304	70.299700
891.316647	50.788026	70.304705
890.483496	35.223409	70.309710
890.391853	42.960530	70.314714
889.713467	56.247203	70.319719
888.896663	42.404294	70.324724
887.995918	51.125480	70.329729
887.697304	44.816175	70.334734
887.366654	44.151266	70.339738
885.861407	44.958918	70.344743
885.231588	50.197307	70.349748
884.709284	49.149983	70.354753
884.373027	50.066871	70.359758
883.762955	49.859142	70.364762
882.682028	47.770717	70.369767
882.137628	43.918776	70.374772
881.431166	56.011112	70.379777
881.404116	50.468801	70.384782
879.936811	49.635439	70.389786
878.940696	50.258001	70.394791
878.484438	47.914171	70.399796
877.998090	52.775505	70.404801
877.929568	39.653471	70.409806
877.493867	44.312718	70.414810
876.484501	45.397788	70.419815
875.930773	41.865193	70.424820
875.155749	48.671395	70.429825
874.312515	56.948942	70.434830
873.209041	45.814337	70.439834
872.323073	53.025970	70.444839
872.242718	39.085745	70.449844
871.736801	49.723145	70.454849
871.580047	45.715999	70.459854
870.512949	49.262538	70.464858
869.361690	49.406833	70.469863
868.951178	48.845599	70.474868
868.019550	48.741498	70.479873
868.198131	52.806480	70.484878
867.113548	51.411806	70.489882
866.446031	50.454484	70.494887
865.728777	51.229406	70.499892
864.902680	56.864555	70.504897
864.015280	47.559159	70.509902
863.368123	50.856149	70.514906
862.620747	50.696018	70.519911
862.425839	43.192306	70.524916
861.963362	51.301219	70.529921
861.574106	48.655799	70.534926
860.356574	47.346264	70.539930
859.838832	49.635877	70.544935
859.123911	36.696009	70.549940
858.495933	47.331816	70.554945
857.483760	53.314214	70.559950
857.210879	50.179149	70.564954
856.313428	58.252838	70.569959
856.188044	50.429732	70.574964
855.222907	54.285240	70.579969
854.206757	51.917714	70.584974
853.672066	52.153763	70.589978
852.860806	54.866659	70.594983
852.525062	51.958666	70.599988
851.713473	50.430004	70.604993
851.339842	48.363719	70.609998
850.364580	45.473299	70.615002
849.571506	53.482532	70.620007
849.409969	45.970341	70.625012
848.594088	55.471165	70.630017
848.132131	43.695796	70.635022
847.115448	45.012244	70.640026
846.340648	44.505515	70.645031
845.969132	47.780555	70.650036
845.021689	55.889648	70.655041
844.098579	46.849704	70.660046
843.523000	49.220669	70.665050
842.440369	56.680717	70.670055
842.622317	45.386735	70.675060
841.968809	46.434936	70.680065
842.123321	48.386388	70.685070
841.375278	50.257186	70.690074
840.108814	48.145686	70.695079
839.694372	49.778958	70.700084
838.148415	48.025578	70.705089
837.474941	48.373422	70.710094
837.091308	48.070073	70.715098
836.660759	46.360100	70.720103
836.275962	44.605187	70.725108
835.370465	45.557612	70.730113
834.350109	45.952637	70.735118
833.771346	48.607948	70.740122
833.170567	45.441030	70.745127
833.292605	42.678827	70.750132
832.145957	48.911617	70.755137
831.261601	49.884893	70.760142
831.015927	49.274508	70.765146
830.275736	60.559511	70.770151
829.346638	37.376756	70.775156
828.043589	48.668562	70.780161
827.845650	43.482748	70.785166
827.690203	38.518988	70.790170
826.873814	35.503472	70.795175
826.392909	40.697407	70.800180
825.389689	40.146523	70.805185
824.903621	36.433015	70.810190
824.259659	41.298453	70.815194
822.834878	43.037289	70.820199
822.311283	39.798735	70.825204
821.854014	44.033018	70.830209
821.201094	41.166728	70.835214
820.817789	42.190358	70.840218
820.039054	46.369974	70.845223
820.024263	39.164610	70.850228
818.789056	43.584248	70.855233
817.970139	38.506779	70.860238
817.731525	47.903983	70.865242
816.792433	46.319408	70.870247
815.712805	37.809155	70.875252
815.187543	51.206560	70.880257
814.525590	46.859267	70.885262
814.095381	41.016174	70.890266
813.787650	45.975196	70.895271
813.321077	35.458984	70.900276
812.538767	43.416637	70.905281
811.667992	37.714534	70.910286
811.168276	33.259328	70.915290
810.057652	48.756626	70.920295
809.231014	40.475392	70.925300
808.519942	45.666521	70.930305
808.191703	46.396919	70.935310
807.392085	45.537625	70.940314
807.092368	49.392441	70.945319
806.341454	48.917152	70.950324
805.038296	45.100067	70.955329
804.770921	43.720549	70.960334
804.439106	47.787299	70.965338
803.894094	47.235295	70.970343
803.316100	38.578727	70.975348
802.273889	53.460003	70.980353
801.828385	43.808948	70.985358
801.317523	44.940082	70.990362
800.170543	48.847271	70.995367
799.300267	34.920404	71.000372
798.751815	43.546513	71.005377
798.083206	36.506434	71.010382
798.115860	35.927713	71.015386
796.469005	44.090299	71.020391
796.080938	28.437245	71.025396
795.540422	37.200536	71.030401
794.970253	34.183505	71.035406
794.558069	45.021939	71.040410
794.025476	44.602407	71.045415
793.179566	39.573381	71.050420
792.189331	37.326952	71.055425
791.698456	43.448599	71.060430
791.241020	39.850183	71.065434
790.229011	45.997945	71.070439
789.619200	37.112370	71.075444
788.845790	45.335329	71.080449
788.382473	40.201294	71.085454
788.231324	39.798918	71.090458
786.769066	42.693595	71.095463
786.337460	40.356607	71.100468
785.444886	47.609245	71.105473
785.433616	44.966581	71.110478
785.205601	45.608764	71.115482
783.769998	46.600691	71.120487
783.181672	39.139515	71.125492
782.467663	48.533288	71.130497
781.570522	40.455970	71.135502
781.087839	49.893402	71.140506
780.524845	47.175521	71.145511
780.429440	35.356725	71.150516
779.407045	41.648758	71.155521
778.270795	41.335397	71.160526
777.808435	40.826473	71.165530
777.030298	42.855583	71.170535
776.763982	38.968260	71.175540
775.764999	40.544965	71.180545
774.629328	37.057208	71.185550
773.937543	41.141411	71.190554
773.337349	48.413041	71.195559
773.365857	43.332513	71.200564
772.932052	53.948484	71.205569
772.467277	42.319265	71.210574
771.889078	39.276378	71.215578
770.774360	40.512929	71.220583
770.188751	49.026992	71.225588
768.722076	43.155017	71.230593
768.163985	51.727127	71.235598
767.832484	41.426981	71.240602
767.151603	49.537782	71.245607
766.561248	44.672208	71.250612
765.938715	52.049503	71.255617
764.801739	44.602581	71.260622
763.944055	40.089891	71.265626
763.739500	53.724448	71.270631
763.604240	36.196214	71.275636
763.025233	43.347771	71.280641
762.743066	42.921658	71.285646
761.954886	36.139689	71.290650
760.655407	45.979524	71.295655
760.139031	29.909534	71.300660
758.836396	43.424703	71.305665
757.765008	42.427247	71.310670
757.236210	41.812475	71.315674
757.090174	47.375343	71.320679
756.536411	31.912118	71.325684
756.063358	42.300738	71.330689
755.972984	34.462180	71.335694
755.574690	40.151149	71.340698
754.196452	44.098356	71.345703
753.871563	26.393025	71.350708
752.426518	38.696341	71.355713
751.427146	33.027336	71.360718
750.953003	35.437375	71.365722
750.328072	43.233475	71.370727
750.633366	38.323023	71.375732
749.871733	34.825669	71.380737
749.369616	37.086168	71.385742
748.297685	37.640037	71.390746
747.436644	41.472201	71.395751
747.326494	30.230249	71.400756
746.152405	36.895226	71.405761
745.388986	40.637250	71.410766
745.108551	35.215724	71.415770
744.108158	45.710472	71.420775
743.203669	41.822744	71.425780
742.034560	36.399121	71.430785
741.717147	47.369732	71.435790
741.554588	44.050395	71.440794
741.070195	47.074001	71.445799
740.803931	42.709067	71.450804
739.568995	47.948499	71.455809
738.528682	36.229213	71.460814
737.992758	40.547232	71.465818
737.292568	48.493983	71.470823
737.052420	41.396305	71.475828
735.967953	41.999295	71.480833
735.396153	47.211176	71.485838
734.917165	38.934745	71.490842
734.092591	54.996043	71.495847
733.730192	35.804320	71.500852
733.169191	41.712599	71.505857
732.148618	35.682908	71.510862
731.597301	50.647449	71.515866
730.927258	55.492500	71.520871
730.708293	40.837135	71.525876
729.908675	47.017991	71.530881
729.345219	37.848977	71.535886
728.954142	36.232118	71.540890
727.553771	43.710295	71.545895
726.741531	36.711415	71.550900
726.229163	48.009486	71.555905
725.624551	42.355748	71.560910
725.365976	49.132303	71.565914
724.208774	48.761758	71.570919
723.702621	41.808329	71.575924
722.921442	47.678940	71.580929
722.421286	40.409503	71.585934
721.705707	39.360574	71.590938
720.357538	38.026091	71.595943
719.723981	44.258231	71.600948
719.183860	45.452014	71.605953
718.963054	44.626203	71.610958
718.884302	44.374839	71.615962
718.317974	49.740118	71.620967
717.683061	40.993060	71.625972
716.494560	42.130953	71.630977
715.450784	40.687880	71.635982
715.193733	34.965133	71.640986
713.491378	45.801967	71.645991
713.591675	45.707814	71.650996
712.749643	44.146501	71.656001
712.248344	39.778416	71.661006
711.905547	33.247379	71.666010
711.343025	44.057093	71.671015
711.000446	39.368940	71.676020
710.055098	39.352083	71.681025
709.374856	39.591768	71.686030
708.642709	35.103373	71.691034
707.337638	48.375826	71.696039
706.670201	41.771724	71.701044
706.076845	39.185365	71.706049
705.779419	46.338027	71.711054
705.721203	38.053856	71.716058
704.493803	51.218274	71.721063
703.772184	32.015476	71.726068
703.090974	36.008274	71.731073
702.666157	43.551421	71.736078
702.355150	41.864403	71.741082
701.136857	42.792284	71.746087
700.263158	39.696616	71.751092
699.705193	42.370480	71.756097
699.132853	44.636303	71.761102
698.974406	42.383574	71.766106
698.071042	50.726694	71.771111
697.021466	43.523359	71.776116
696.488298	39.351384	71.781121
696.024656	38.936235	71.786126
695.719595	39.511493	71.791130
694.641907	41.561144	71.796135
693.713212	37.829541	71.801140
693.293084	36.533434	71.806145
692.740499	48.613614	71.811150
692.314757	43.125018	71.816154
691.481973	46.918404	71.821159
690.788842	39.059173	71.826164
690.044919	40.872840	71.831169
689.165868	41.950226	71.836174
688.361441	45.166813	71.841178
687.874707	48.339237	71.846183
687.199901	44.168239	71.851188
686.897608	38.805724	71.856193
686.010347	39.081273	71.861198
685.215564	43.223392	71.866202
684.256085	41.673522	71.871207
683.884406	42.488733	71.876212
683.775268	43.281465	71.881217
683.195199	36.677401	71.886222
682.390460	33.977269	71.891226
680.949961	45.412635	71.896231
680.742484	35.635967	71.901236
680.360157	43.110654	71.906241
679.172977	41.741497	71.911246
678.841691	44.876632	71.916250
678.205102	47.162938	71.921255
677.799353	48.413042	71.926260
676.937297	45.535239	71.931265
675.944850	49.150730	71.936270
675.637549	44.409959	71.941274
674.876503	47.908047	71.946279
674.347745	40.370376	71.951284
672.860078	44.272407	71.956289
672.231534	41.959304	71.961294
671.853723	37.554676	71.966298
671.132164	38.480748	71.971303
671.244612	41.963785	71.976308
670.366779	44.069592	71.981313
669.898880	46.588695	71.986318
669.266188	45.190067	71.991322
668.400363	49.774600	71.996327
667.356065	42.397880	72.001332
666.336422	44.937302	72.006337
665.394605	43.228103	72.011342
665.313232	39.990384	72.016346
664.775577	47.665359	72.021351
664.581739	43.618400	72.026356
664.369833	40.663161	72.031361
663.331643	45.288276	72.036366
662.413371	47.153921	72.041370
661.791042	46.329802	72.046375
660.834938	45.324459	72.051380
659.991924	48.122159	72.056385
659.135619	48.318597	72.061390
658.852791	35.077010	72.066394
658.264073	43.308990	72.071399
657.981027	39.482963	72.076404
657.205314	40.882894	72.081409
655.977082	37.002893	72.086414
655.848981	30.545602	72.091418
655.411402	44.973966	72.096423
654.752806	41.268330	72.101428
653.444915	38.510335	72.106433
652.862111	41.667247	72.111438
652.538898	43.575410	72.116442
651.414990	45.320771	72.121447
650.744678	37.285150	72.126452
649.998138	45.649559	72.131457
649.307483	45.216469	72.136462
649.200225	45.121955	72.141466
648.623619	41.400299	72.146471
647.967047	29.200065	72.151476
646.692291	43.987373	72.156481
646.083783	38.139725	72.161486
645.914538	37.290875	72.166490
645.290046	46.984693	72.171495
644.705914	39.093378	72.176500
643.831237	41.036421	72.181505
642.622133	38.453730	72.186510
642.487460	40.522212	72.191514
641.937044	42.560087	72.196519
641.046465	41.855346	72.201524
639.889594	45.272052	72.206529
639.358778	44.790658	72.211534
639.531750	40.526525	72.216538
638.651729	46.183564	72.221543
637.973580	41.817370	72.226548
637.129904	44.738337	72.231553
636.264311	45.511864	72.236558
636.177978	38.557970	72.241562
635.376275	48.700153	72.246567
634.112254	39.241867	72.251572
633.566611	45.420269	72.256577
633.045021	50.115162	72.261582
632.985900	43.242651	72.266586
632.124553	43.238259	72.271591
631.263987	40.610066	72.276596
630.481589	35.681112	72.281601
629.692898	44.630210	72.286606
629.661238	44.932459	72.291610
628.548996	47.544987	72.296615
627.944337	36.684598	72.301620
627.497262	46.879700	72.306625
626.840128	51.803463	72.311630
626.096198	41.657683	72.316634
625.255395	46.016499	72.321639
624.725904	39.575481	72.326644
624.203773	38.059239	72.331649
622.947481	47.549086	72.336654
622.342964	40.519772	72.341658
621.904203	48.746588	72.346663
621.299976	40.561500	72.351668
620.694470	47.174478	72.356673
619.744026	45.000609	72.361678
618.957057	35.100222	72.366682
618.034813	37.625727	72.371687
617.703086	37.342318	72.376692
617.653834	42.204163	72.381697
616.928455	36.314575	72.386702
616.666581	38.037372	72.391706
615.681639	45.576232	72.396711
614.793782	44.723012	72.401716
614.173986	44.815782	72.406721
612.925148	44.565959	72.411726
612.299706	36.507266	72.416730
611.564072	44.742316	72.421735
611.046175	43.941362	72.426740
610.790500	48.258740	72.431745
610.237574	54.408397	72.436750
609.939894	35.990313	72.441754
608.886626	48.513492	72.446759
608.047247	47.624732	72.451764
607.607494	53.388308	72.456769
606.659390	47.053353	72.461774
605.961660	44.177804	72.466778
605.029426	44.423575	72.471783
604.615274	47.972362	72.476788
604.077719	43.878911	72.481793
603.354709	46.056091	72.486798
603.388537	43.806343	72.491802
602.289313	49.121624	72.496807
601.547714	48.377945	72.501812
600.887922	49.358572	72.506817
599.840383	49.264515	72.511822
599.023936	43.183307	72.516826
598.220316	50.939774	72.521831
597.851879	48.802760	72.526836
597.040864	53.147400	72.531841
597.140011	46.499602	72.536846
596.828051	42.841156	72.541850
596.486603	46.258677	72.546855
595.097927	46.273199	72.551860
594.575705	42.614861	72.556865
593.349953	45.681820	72.561870
592.454869	44.377105	72.566874
591.921210	48.337926	72.571879
591.666897	36.652956	72.576884
591.403148	37.900445	72.581889
591.020446	48.881841	72.586894
589.870174	42.072350	72.591898
588.752926	41.479084	72.596903
588.330233	40.911280	72.601908
587.137425	45.467773	72.606913
586.696467	48.798140	72.611918
586.122776	35.264582	72.616922
585.536777	44.640770	72.621927
584.966150	44.387639	72.626932
584.614079	51.080348	72.631937
583.401298	53.719191	72.636942
582.905283	42.302198	72.641946
582.186995	44.364894	72.646951
582.049871	47.082314	72.651956
581.302325	40.453283	72.656961
580.155427	42.767038	72.661966
579.717129	34.862199	72.666970
579.006745	40.395052	72.671975
578.478321	36.806460	72.676980
577.680923	42.263833	72.681985
576.772976	45.868414	72.686990
576.246876	41.340398	72.691994
575.819253	49.733850	72.696999
575.366255	41.621933	72.702004
574.343205	41.288831	72.707009
573.518728	41.528381	72.712014
573.103266	33.916060	72.717018
572.207729	46.228278	72.722023
571.980833	46.149528	72.727028
571.135155	33.538844	72.732033
570.287827	42.556410	72.737038
569.897614	32.047300	72.742042
569.315569	43.868458	72.747047
568.386769	36.393828	72.752052
567.430426	45.431654	72.757057
566.429702	42.831041	72.762062
566.478597	41.201571	72.767066
565.867727	48.833045	72.772071
565.592899	40.895064	72.777076
565.119820	49.432875	72.782081
563.862994	45.101114	72.787086
563.346534	43.858629	72.792090
562.590215	43.091427	72.797095
561.434963	40.413484	72.802100
560.787624	44.362207	72.807105
559.909787	46.016085	72.812110
560.050939	43.736501	72.817114
559.515959	42.938875	72.822119
558.701269	33.434812	72.827124
557.924923	31.873327	72.832129
557.215585	43.020415	72.837134
556.890547	38.560183	72.842138
555.987989	42.032008	72.847143
555.045927	37.566586	72.852148
554.540645	44.652629	72.857153
553.819822	47.195736	72.862158
553.507385	39.877982	72.867162
552.804079	46.411016	72.872167
551.709876	44.995963	72.877172
551.279837	40.911728	72.882177
550.555172	46.404798	72.887182
550.345562	40.098840	72.892186
549.161249	45.747244	72.897191
548.047611	46.822615	72.902196
547.777365	51.907054	72.907201
547.528573	51.153543	72.912206
547.509899	38.149331	72.917210
546.263869	38.052588	72.922215
545.272091	40.073340	72.927220
544.942642	39.438250	72.932225
544.178344	40.116678	72.937230
543.303006	34.253196	72.942234
542.342625	45.758284	72.947239
541.769634	36.445691	72.952244
541.340835	38.232617	72.957249
541.022303	42.271834	72.962254
540.440967	35.971156	72.967258
538.961032	41.425887	72.972263
538.209494	49.960494	72.977268
537.687447	45.249431	72.982273
537.371693	42.519615	72.987278
537.134884	35.038916	72.992282
535.907361	36.570752	72.997287
535.472338	39.615120	73.002292
534.677699	35.563759	73.007297
534.223837	41.615524	73.012302
534.113841	33.003555	73.017306
532.811933	38.518565	73.022311
532.183632	34.182534	73.027316
531.882031	38.295424	73.032321
530.789514	37.896081	73.037326
529.839445	40.947787	73.042330
528.776370	39.008752	73.047335
528.360593	39.263931	73.052340
528.134921	44.002854	73.057345
527.526720	47.468454	73.062350
527.247110	35.624420	73.067354
525.992637	40.665147	73.072359
525.391944	44.653641	73.077364
525.441628	42.774971	73.082369
524.450520	50.704089	73.087374
524.102180	45.980630	73.092378
522.685401	38.677254	73.097383
522.261627	47.698035	73.102388
521.835812	42.141981	73.107393
520.136451	45.382868	73.112398
519.538547	44.694312	73.117402
519.360157	43.347722	73.122407
519.150060	46.833128	73.127412
518.787833	37.947028	73.132417
517.937471	46.958806	73.137422
517.271628	46.577138	73.142426
516.284960	41.584136	73.147431
515.917142	43.588365	73.152436
514.830824	42.620365	73.157441
513.769913	50.710252	73.162446
513.389131	40.722922	73.167450
512.614098	52.733462	73.172455
512.373945	42.258639	73.177460
512.342406	32.853274	73.182465
511.127017	39.391166	73.187470
510.536761	35.512803	73.192474
509.624609	38.139618	73.197479
509.044311	37.170169	73.202484
507.898612	30.828450	73.207489
506.938779	45.005658	73.212494
506.921794	35.876861	73.217498
506.148507	45.122917	73.222503
505.620338	38.429472	73.227508
505.513223	35.438922	73.232513
504.895678	46.434503	73.237518
503.952540	41.765999	73.242522
503.616959	39.294965	73.247527
502.299280	39.010391	73.252532
501.309935	37.076491	73.257537
500.819802	40.874340	73.262542
500.694004	41.141408	73.267546
499.925239	39.080504	73.272551
499.035034	37.606430	73.277556
498.146510	39.536475	73.282561
497.472261	38.193150	73.287566
497.219192	38.566494	73.292570
496.729180	32.401353	73.297575
496.141678	43.213767	73.302580
495.100883	40.267954	73.307585
494.144039	45.685953	73.312590
493.936459	40.743785	73.317594
493.300418	43.688795	73.322599
492.462719	47.832372	73.327604
491.665667	44.680195	73.332609
490.945561	40.903028	73.337614
490.929339	37.847564	73.342618
490.449026	44.958144	73.347623
489.269958	42.303642	73.352628
488.903587	42.842842	73.357633
487.849871	42.676057	73.362638
487.204616	36.969334	73.367642
486.236550	44.518343	73.372647
485.535954	42.371949	73.377652
485.026192	43.214783	73.382657
483.916494	55.474505	73.387662
483.636606	47.692523	73.392666
483.298820	43.482758	73.397671
483.043097	39.074995	73.402676
482.032509	38.337169	73.407681
481.168352	44.427273	73.412686
480.888560	38.433333	73.417690
480.196827	43.927475	73.422695
479.140831	37.980894	73.427700
478.833630	40.438131	73.432705
478.016698	43.732279	73.437710
477.729798	38.719632	73.442714
476.104340	50.110157	73.447719
475.352848	49.501608	73.452724
475.015833	37.403356	73.457729
474.260740	49.323641	73.462734
474.352456	39.623224	73.467738
473.804497	39.935004	73.472743
472.911046	43.259238	73.477748
472.137073	35.141166	73.482753
471.096368	45.924277	73.487758
470.920508	46.760813	73.492762
469.915296	46.653216	73.497767
469.052052	43.583436	73.502772
468.208565	38.685509	73.507777
467.798185	54.263352	73.512782
467.521606	41.988961	73.517786
467.010948	48.603457	73.522791
466.269576	48.618796	73.527796
465.731522	41.508655	73.532801
464.632314	48.656613	73.537806
464.044130	40.911284	73.542810
463.540653	42.924159	73.547815
462.810297	43.612572	73.552820
462.014647	38.218583	73.557825
461.198277	44.794682	73.562830
461.019455	43.067664	73.567834
460.535450	48.025715	73.572839
459.441929	45.804167	73.577844
458.591197	43.764027	73.582849
457.962238	50.301302	73.587854
458.015896	49.117042	73.592858
456.412022	42.689255	73.597863
455.791377	42.423002	73.602868
455.554982	42.834147	73.607873
454.687584	49.857125	73.612878
454.940956	53.405601	73.617882
453.550186	43.990809	73.622887
452.602146	43.955518	73.627892
452.174397	37.894574	73.632897
451.463309	47.193919	73.637902
451.205149	38.202371	73.642906
449.945536	37.880232	73.647911
449.657712	42.848871	73.652916
448.999653	38.771360	73.657921
448.323915	43.502150	73.662926
447.891076	39.228553	73.667930
446.835271	46.934700	73.672935
446.183418	45.512943	73.677940
445.777654	43.256034	73.682945
444.563465	53.486680	73.687950
443.939403	36.463442	73.692954
443.350036	40.571177	73.697959
442.874940	48.642388	73.702964
442.451873	44.835641	73.707969
442.157503	49.785273	73.712974
441.476148	42.996123	73.717978
440.323474	42.915382	73.722983
439.599290	40.177810	73.727988
439.156822	45.068352	73.732993
437.635462	50.192335	73.737998
437.279710	50.057521	73.743002
436.629448	52.862088	73.748007
436.338123	51.766946	73.753012
435.890460	51.055023	73.758017
435.354756	59.310300	73.763022
434.823821	46.374937	73.768026
433.771117	40.188608	73.773031
433.060227	47.694736	73.778036
432.450152	41.169278	73.783041
431.471057	51.434238	73.788046
430.936651	33.018486	73.793050
430.720015	42.877267	73.798055
430.150523	38.934572	73.803060
429.345612	41.374874	73.808065
428.471493	45.771791	73.813070
427.605833	36.395701	73.818074
427.421155	47.125666	73.823079
426.495323	43.838871	73.828084
425.863268	38.542769	73.833089
425.413476	42.862626	73.838094
424.658815	43.210624	73.843098
423.727858	44.499835	73.848103
422.579987	47.110222	73.853108
422.167337	41.241682	73.858113
421.218176	48.781145	73.863118
421.061409	40.830452	73.868122
420.625857	39.647141	73.873127
420.269026	41.359773	73.878132
419.472865	44.899039	73.883137
418.520989	53.042092	73.888142
418.197241	44.610044	73.893146
416.808629	45.050503	73.898151
416.063037	45.197224	73.903156
415.820998	41.077632	73.908161
415.014236	48.509407	73.913166
414.677932	49.960774	73.918170
414.403269	47.915861	73.923175
413.308532	49.095386	73.928180
412.637101	37.233263	73.933185
411.791561	47.577565	73.938190
411.735418	39.362538	73.943194
410.704224	36.754950	73.948199
409.547811	40.718697	73.953204
408.825580	37.783834	73.958209
407.880441	44.475158	73.963214
407.692816	43.488556	73.968218
407.736667	44.457956	73.973223
406.718359	39.377253	73.978228
405.976898	39.110002	73.983233
404.899142	51.078878	73.988238
404.689437	43.901818	73.993242
404.564396	47.300416	73.998247
403.319566	41.621466	74.003252
402.629864	40.646308	74.008257
401.666879	49.545168	74.013262
401.487971	30.866016	74.018266
401.131001	42.319803	74.023271
400.187500	42.899104	74.028276
399.550289	34.965626	74.033281
398.841413	41.234377	74.038286
398.477316	41.181123	74.043290
397.239958	34.841332	74.048295
396.107304	39.378474	74.053300
396.082829	32.790560	74.058305
395.111649	45.975042	74.063310
395.125890	37.067864	74.068314
394.133839	42.717686	74.073319
392.880096	41.184760	74.078324
392.137577	38.758216	74.083329
391.750769	45.688967	74.088334
391.497993	39.429502	74.093338
390.964248	39.783853	74.098343
390.328895	42.568896	74.103348
389.630051	41.398739	74.108353
388.327143	43.944130	74.113358
388.520084	35.700630	74.118362
387.726038	34.487978	74.123367
387.205654	37.728946	74.128372
386.362483	33.111233	74.133377
385.199518	36.330887	74.138382
385.224892	31.581690	74.143386
384.151296	39.685604	74.148391
382.550533	36.792765	74.153396
382.626108	31.740114	74.158401
382.188458	35.965527	74.163406
381.854467	36.575759	74.168410
381.405076	40.136120	74.173415
380.153597	44.941512	74.178420
379.601621	36.858438	74.183425
378.957901	47.087237	74.188430
378.560115	41.806253	74.193434
377.105859	42.190083	74.198439
376.191186	33.794984	74.203444
376.236905	37.379037	74.208449
375.866301	40.355141	74.213454
375.156182	30.674929	74.218458
374.518580	38.078107	74.223463
373.636316	41.426095	74.228468
373.528962	37.479202	74.233473
372.614577	36.698863	74.238478
371.441801	36.946433	74.243482
371.215114	34.215974	74.248487
370.136037	37.433097	74.253492
369.725796	41.745783	74.258497
368.314905	43.140150	74.263502
367.893042	34.413502	74.268506
367.225302	32.953036	74.273511
366.727732	41.200585	74.278516
366.367475	31.900519	74.283521
365.754933	37.973167	74.288526
365.547207	40.709395	74.293530
364.573893	36.516598	74.298535
363.392253	46.424718	74.303540
363.266460	40.895422	74.308545
362.566754	47.130635	74.313550
361.569388	40.088577	74.318554
360.944172	48.860082	74.323559
360.382663	41.511627	74.328564
360.185024	35.874259	74.333569
358.840616	47.547015	74.338574
358.359370	51.157047	74.343578
357.728160	45.276240	74.348583
357.285821	51.563656	74.353588
357.120537	52.917430	74.358593
355.444502	53.717413	74.363598
354.889950	53.186834	74.368602
354.313614	53.246928	74.373607
353.605728	45.453456	74.378612
353.256030	52.612705	74.383617
352.018788	51.236425	74.388622
351.240485	47.443601	74.393626
350.841620	57.533342	74.398631
350.030483	53.750486	74.403636
349.840457	49.755397	74.408641
349.808698	53.895068	74.413646
349.426262	48.082934	74.418650
348.012159	44.964310	74.423655
347.485595	48.922352	74.428660
346.789707	39.358117	74.433665
345.212069	48.322462	74.438670
344.805983	47.228050	74.443674
344.502489	45.867385	74.448679
343.925825	48.884334	74.453684
343.940884	46.438082	74.458689
342.543982	50.379907	74.463694
341.826021	51.986291	74.468698
341.686670	43.916576	74.473703
340.584736	45.455355	74.478708
339.709653	40.588135	74.483713
338.959705	49.436674	74.488718
338.222312	43.280403	74.493722
338.002106	52.779423	74.498727
337.474630	54.150672	74.503732
337.173333	42.260652	74.508737
335.871364	45.418885	74.513742
335.390768	48.780533	74.518746
334.727933	49.864736	74.523751
333.295703	60.591825	74.528756
332.987958	46.768022	74.533761
332.229611	47.846887	74.538766
331.798449	43.395790	74.543770
331.442991	41.055277	74.548775
330.686847	50.039476	74.553780
330.780383	49.509922	74.558785
329.395718	51.597658	74.563790
328.881795	41.459508	74.568794
328.328906	38.858378	74.573799
327.201640	46.815591	74.578804
326.483663	47.257575	74.583809
325.751165	46.759867	74.588814
325.185332	46.136100	74.593818
325.054851	41.173629	74.598823
324.564470	45.606626	74.603828
323.485709	45.251551	74.608833
322.715752	43.768350	74.613838
322.509857	42.844090	74.618842
321.772827	48.275357	74.623847
320.383179	48.074219	74.628852
319.955461	45.828981	74.633857
319.287607	50.916439	74.638862
318.968951	43.393744	74.643866
317.982665	40.157992	74.648871
317.107091	45.191056	74.653876
316.819727	43.050440	74.658881
315.988697	44.939874	74.663886
315.530664	36.659144	74.668890
315.625651	34.240245	74.673895
314.026062	47.526518	74.678900
313.514609	40.614335	74.683905
312.811279	47.988921	74.688910
312.246017	42.390882	74.693914
311.223353	40.583124	74.698919
310.460281	44.794455	74.703924
309.819968	30.668483	74.708929
309.098120	38.526604	74.713934
308.984154	35.835642	74.718938
308.669594	42.832558	74.723943
307.596017	40.226338	74.728948
306.685114	39.025046	74.733953
305.993098	53.845142	74.738958
305.609495	41.445452	74.743962
305.366056	38.396967	74.748967
304.501352	44.863741	74.753972
304.033570	42.256711	74.758977
303.070427	38.416243	74.763982
302.429238	39.937634	74.768986
301.243408	45.435170	74.773991
300.307912	45.610905	74.778996
300.257672	40.544295	74.784001
299.694335	43.321345	74.789006
299.191615	46.825331	74.794010
298.354753	38.908727	74.799015
297.272783	45.264329	74.804020
297.005083	37.602651	74.809025
296.195033	44.101897	74.814030
296.238055	42.114247	74.819034
295.135799	42.008322	74.824039
293.777037	41.853210	74.829044
293.659977	38.409667	74.834049
293.154530	36.606809	74.839054
292.585454	39.290901	74.844058
291.771281	44.368705	74.849063
290.781651	51.246083	74.854068
290.682346	39.992859	74.859073
290.025861	53.049603	74.864078
288.948084	48.478434	74.869082
288.225780	45.607154	74.874087
287.421619	47.256344	74.879092
287.300681	47.129449	74.884097
286.392203	50.114467	74.889102
285.982851	39.418831	74.894106
285.009085	48.456122	74.899111
283.947280	52.456177	74.904116
284.077775	45.618297	74.909121
283.282183	53.883385	74.914126
282.821250	51.733049	74.919130
281.481030	46.728475	74.924135
280.657191	58.508591	74.929140
280.728951	44.573966	74.934145
280.069263	49.224659	74.939150
279.249530	47.897620	74.944154
278.733165	46.016902	74.949159
278.086979	52.196769	74.954164
277.704553	39.071402	74.959169
276.085225	46.056318	74.964174
275.428958	43.785526	74.969178
275.167694	49.362210	74.974183
274.539373	51.110334	74.979188
274.083532	40.316885	74.984193
273.088986	47.895327	74.989198
272.296554	44.871870	74.994202
271.629060	42.790887	74.999207
271.189756	46.413076	75.004212
271.130165	41.252944	75.009217
269.787171	54.382362	75.014222
268.931056	45.535566	75.019226
268.712970	43.930151	75.024231
267.885432	50.018741	75.029236
267.768972	40.399021	75.034241
266.346847	51.078993	75.039246
265.648789	46.100529	75.044250
265.548230	43.829219	75.049255
265.137393	55.027784	75.054260
263.817772	43.559811	75.059265
262.888175	41.676904	75.064270
262.189101	41.627003	75.069274
261.691478	47.835085	75.074279
261.253134	56.134462	75.079284
261.442219	49.196939	75.084289
260.244645	52.860292	75.089294
259.239910	50.653180	75.094298
259.311315	43.820693	75.099303
257.574570	52.699445	75.104308
257.156784	43.980008	75.109313
256.204774	56.222198	75.114318
255.811747	49.450766	75.119322
255.863480	46.599569	75.124327
254.713246	46.598187	75.129332
254.404008	45.357323	75.134337
253.040713	41.965171	75.139342
253.046669	43.996130	75.144346
252.652364	40.293814	75.149351
251.279427	45.919741	75.154356
250.505251	42.009792	75.159361
249.927157	49.426070	75.164366
249.259443	43.478520	75.169370
248.870371	49.821935	75.174375
248.511668	49.447656	75.179380
247.189253	44.330312	75.184385
246.333908	57.098665	75.189390
246.240917	55.406679	75.194394
245.791351	37.786390	75.199399
244.579409	54.721667	75.204404
243.799760	38.299468	75.209409
243.180634	52.269488	75.214414
242.501056	42.525255	75.219418
242.301519	44.460789	75.224423
241.498539	50.415312	75.229428
241.399669	41.757259	75.234433
240.426688	48.696521	75.239438
239.598842	54.972263	75.244442
239.398750	43.479758	75.249447
237.802790	56.169020	75.254452
237.201375	46.221927	75.259457
236.675326	49.742152	75.264462
236.274872	59.261804	75.269466
235.880060	55.743905	75.274471
235.081468	50.282183	75.279476
234.409131	46.134530	75.284481
233.052719	52.275888	75.289486
232.439160	44.878356	75.294490
232.684447	43.507312	75.299495
231.879907	50.928856	75.304500
230.780701	51.789470	75.309505
229.849507	51.791993	75.314510
229.960309	44.584093	75.319514
229.549829	42.376961	75.324519
228.162253	53.298504	75.329524
227.721814	42.447954	75.334529
227.037200	51.651595	75.339534
226.710642	43.373604	75.344538
225.693232	35.328506	75.349543
224.259957	47.544642	75.354548
223.982142	38.704910	75.359553
223.270277	44.961953	75.364558
222.874215	39.213357	75.369562
223.032994	43.814934	75.374567
221.918034	49.707681	75.379572
221.270489	44.313620	75.384577
220.918735	41.994982	75.389582
219.868567	39.698174	75.394586
218.758309	42.023885	75.399591
218.004869	44.438423	75.404596
218.042194	43.999024	75.409601
217.186229	44.292582	75.414606
216.346932	42.910097	75.419610
215.517272	45.532294	75.424615
214.991781	48.144586	75.429620
214.779039	48.007379	75.434625
213.946012	45.318898	75.439630
212.645715	49.419054	75.444634
211.955444	42.109279	75.449639
211.469387	46.884547	75.454644
211.145511	42.763608	75.459649
210.812304	45.567926	75.464654
210.135465	45.656712	75.469658
209.095946	43.358081	75.474663
208.571719	54.025456	75.479668
208.513210	39.083371	75.484673
207.253110	53.372463	75.489678
206.351194	49.129571	75.494682
205.622778	50.107804	75.499687
204.828742	44.529264	75.504692
204.481450	39.350170	75.509697
204.072676	49.560015	75.514702
203.031559	47.171664	75.519706
202.196299	40.256197	75.524711
201.264436	44.872242	75.529716
201.474104	40.162902	75.534721
200.640355	44.277420	75.539726
200.221499	42.681164	75.544730
199.399513	39.724364	75.549735
198.334362	38.680580	75.554740
198.161420	38.235386	75.559745
197.476729	49.493914	75.564750
196.390007	42.670892	75.569754
196.078215	38.883391	75.574759
195.287903	44.563788	75.579764
195.159720	36.431394	75.584769
193.787431	48.653660	75.589774
192.990163	42.442954	75.594778
192.321304	36.638501	75.599783
191.893579	43.860065	75.604788
191.896901	34.808737	75.609793
190.777890	44.896002	75.614798
189.810451	34.406183	75.619802
189.358029	37.691565	75.624807
188.833264	36.118597	75.629812
188.199942	38.220065	75.634817
187.182569	41.203239	75.639822
186.621930	43.331720	75.644826
186.065284	42.617980	75.649831
185.375569	46.330070	75.654836
184.589083	34.423398	75.659841
183.781148	32.253618	75.664846
182.844847	31.880076	75.669850
182.649657	32.300353	75.674855
181.940910	33.446522	75.679860
182.111433	29.497007	75.684865
181.009573	28.922123	75.689870
180.171330	35.666591	75.694874
179.744165	25.732677	75.699879
178.514182	40.233295	75.704884
177.683256	40.076938	75.709889
176.721127	39.287850	75.714894
176.355756	31.446368	75.719898
176.374481	26.150067	75.724903
175.907702	37.295052	75.729908
175.302393	34.376899	75.734913
174.058459	42.810026	75.739918
173.450493	38.798974	75.744922
173.338869	36.220901	75.749927
172.462780	43.934170	75.754932
171.105081	43.137109	75.759937
170.768723	41.692888	75.764942
170.727928	41.613833	75.769946
169.904956	39.241777	75.774951
168.436942	39.861305	75.779956
168.010989	39.837620	75.784961
167.461224	47.385219	75.789966
167.005604	34.443340	75.794970
166.516006	32.590416	75.799975
164.962278	39.047040	75.804980
164.475531	30.638642	75.809985
164.079588	37.257161	75.814990
163.680967	34.631188	75.819994
163.515327	33.914366	75.824999
162.387571	36.207958	75.830004
161.670521	40.601273	75.835009
161.154041	38.623887	75.840014
160.116684	41.988626	75.845018
159.284545	44.285224	75.850023
158.366640	51.985142	75.855028
158.008421	45.548791	75.860033
157.571278	47.931613	75.865038
157.196894	46.756395	75.870042
156.909556	36.320512	75.875047
155.906710	47.065195	75.880052
154.990335	40.289954	75.885057
154.320969	42.049863	75.890062
153.689993	44.635246	75.895066
152.754523	44.047633	75.900071
152.196532	41.850404	75.905076
152.027391	41.487055	75.910081
151.352833	36.544061	75.915086
150.512679	38.705068	75.920090
149.367828	35.448782	75.925095
148.317677	42.117880	75.930100
147.990690	43.210844	75.935105
148.023928	44.292577	75.940110
147.255302	45.816494	75.945114
146.854587	33.759231	75.950119
145.960961	41.957057	75.955124
145.465727	39.755781	75.960129
144.468783	42.459162	75.965134
143.005355	47.516059	75.970138
142.669638	44.062249	75.975143
141.946732	54.565538	75.980148
141.753392	40.392980	75.985153
141.486256	43.785935	75.990158
141.233552	49.836780	75.995162
140.185767	46.743843	76.000167
138.937903	51.572746	76.005172
138.553535	43.305863	76.010177
137.781639	50.649588	76.015182
136.791248	38.681573	76.020186
136.157440	34.915733	76.025191
135.388994	45.701938	76.030196
135.133158	45.130834	76.035201
134.533108	42.315989	76.040206
134.123137	37.274747	76.045210
133.285466	34.358938	76.050215
132.478695	38.961440	76.055220
132.118570	42.227846	76.060225
131.337895	35.508686	76.065230
130.481038	43.411676	76.070234
129.674391	37.750061	76.075239
129.072052	40.834979	76.080244
128.401697	37.513141	76.085249
128.522615	46.616974	76.090254
127.084114	39.432730	76.095258
126.265352	42.855521	76.100263
126.023641	46.226752	76.105268
125.505524	45.447997	76.110273
124.576867	42.141233	76.115278
123.369669	48.028495	76.120282
122.884119	39.266627	76.125287
122.091585	54.265391	76.130292
122.023348	41.453276	76.135297
121.325157	49.256836	76.140302
121.099983	45.210165	76.145306
120.776661	40.829817	76.150311
119.724813	40.392812	76.155316
119.331035	40.040346	76.160321
117.994953	43.659583	76.165326
117.070976	48.868726	76.170330
116.697858	42.862411	76.175335
116.045750	50.908714	76.180340
115.116752	39.541985	76.185345
114.240923	47.785315	76.190350
113.576323	55.862577	76.195354
113.479098	44.668621	76.200359
112.687229	43.179742	76.205364
112.591628	45.230872	76.210369
111.425871	46.948397	76.215374
110.589313	51.004993	76.220378
110.174838	44.061222	76.225383
109.862409	50.610959	76.230388
108.786040	44.480488	76.235393
107.876354	48.302137	76.240398
107.286565	51.395169	76.245402
106.951494	50.593719	76.250407
106.386986	48.398402	76.255412
105.494684	44.007845	76.260417
104.472687	44.795649	76.265422
104.010069	47.200210	76.270426
103.608382	47.186580	76.275431
102.774710	51.413593	76.280436
101.785254	47.630181	76.285441
101.191935	44.244617	76.290446
100.200666	49.310572	76.295450
100.400748	44.041200	76.300455
99.644178	52.134622	76.305460
99.478558	41.865761	76.310465
98.616403	39.283740	76.315470
97.598036	44.407231	76.320474
97.144007	45.204236	76.325479
95.802908	43.705712	76.330484
95.283735	41.458813	76.335489
94.789165	44.722219	76.340494
94.413659	38.882492	76.345498
94.051494	42.633955	76.350503
92.738980	46.733471	76.355508
91.747917	38.582455	76.360513
91.348646	40.878661	76.365518
90.953277	40.630279	76.370522
90.692653	36.517853	76.375527
89.601787	40.356751	76.380532
89.187936	38.472693	76.385537
88.190486	42.112429	76.390542
87.776617	35.614191	76.395546
86.991901	32.278813	76.400551
86.081079	43.763202	76.405556
85.254051	32.604386	76.410561
84.897129	43.502396	76.415566
84.402120	40.745729	76.420570
83.936762	41.935047	76.425575
82.617250	48.742307	76.430580
81.883352	35.259641	76.435585
81.466156	40.875290	76.440590
80.962451	46.182110	76.445594
81.157623	47.517509	76.450599
79.527816	47.669835	76.455604
78.957873	45.994896	76.460609
78.260184	43.044441	76.465614
77.960709	37.261545	76.470618
77.178922	30.997694	76.475623
76.061535	39.898978	76.480628
75.463788	34.226035	76.485633
75.260926	33.476916	76.490638
74.628460	33.947300	76.495642
74.105244	32.475128	76.500647
72.811478	36.116724	76.505652
72.362140	37.913915	76.510657
72.077818	36.104752	76.515662
71.239339	34.066144	76.520666
70.217843	30.395995	76.525671
69.684522	39.769869	76.530676
69.376209	41.313555	76.535681
68.840396	39.245949	76.540686
67.411703	44.549525	76.545690
66.381217	41.076693	76.550695
65.971703	43.440574	76.555700
65.568642	40.514997	76.560705
65.463327	32.651840	76.565710
64.854237	47.424159	76.570714
64.595211	38.066527	76.575719
62.821243	47.168014	76.580724
62.175797	38.696056	76.585729
62.074956	41.519351	76.590734
61.168396	43.379147	76.595738
60.574874	29.299698	76.600743
59.369857	39.285677	76.605748
58.791079	35.397923	76.610753
58.637486	38.049484	76.615758
58.181220	41.427502	76.620762
57.962841	38.907209	76.625767
56.683087	46.811666	76.630772
55.941487	43.084845	76.635777
55.582059	46.497179	76.640782
53.916035	40.531766	76.645786
53.496890	47.119139	76.650791
52.887395	47.509804	76.655796
52.437575	42.266997	76.660801
52.239382	35.605873	76.665806
51.683062	45.626680	76.670810
50.820654	39.945435	76.675815
49.664128	47.210252	76.680820
49.127235	48.153302	76.685825
48.643772	38.471413	76.690830
48.225815	48.725062	76.695834
47.255565	40.505362	76.700839
46.599974	33.556765	76.705844
46.153995	36.135701	76.710849
45.490472	29.837766	76.715854
44.601641	47.738376	76.720858
44.228964	40.021710	76.725863
43.162018	42.343190	76.730868
42.774061	36.957946	76.735873
42.561022	36.788037	76.740878
41.039334	42.194795	76.745882
40.519612	30.939097	76.750887
39.660156	41.373826	76.755892
39.288357	40.673015	76.760897
39.351303	33.393999	76.765902
38.310794	31.905531	76.770906
37.720512	41.871768	76.775911
36.606664	42.751909	76.780916
36.115100	43.636271	76.785921
34.829930	42.691035	76.790926
33.901648	36.833207	76.795930
34.298852	27.515430	76.800935
33.403880	36.545942	76.805940
32.957947	39.105136	76.810945
32.553169	34.414313	76.815950
31.594484	40.361212	76.820954
31.184756	35.484539	76.825959
30.145465	41.196985	76.830964
29.460464	33.737546	76.835969
28.284840	38.119111	76.840974
27.632511	39.953874	76.845978
27.050395	39.203472	76.850983
26.799694	40.545846	76.855988
26.316195	38.863989	76.860993
26.061663	44.570165	76.865998
25.249730	34.526207	76.871002
24.215410	38.685006	76.876007
23.518380	38.597293	76.881012
22.857563	40.344701	76.886017
22.610268	41.182445	76.891022
21.684628	37.186417	76.896026
20.868076	29.686383	76.901031
20.227341	41.866525	76.906036
19.585989	41.210748	76.911041
18.913871	33.195717	76.916046
18.430194	49.113694	76.921050
17.795509	38.206898	76.926055
17.022156	47.127359	76.931060
15.979092	40.905160	76.936065
15.444300	34.499505	76.941070
14.644266	46.063189	76.946074
14.989502	34.854570	76.951079
14.157257	44.933740	76.956084
12.773768	40.249686	76.961089
12.253206	43.369143	76.966094
11.563660	42.104697	76.971098
11.037803	39.960791	76.976103
10.295799	42.428656	76.981108
9.193930	39.361606	76.986113
8.854534	40.596039	76.991118
7.970221	44.246389	76.996122
7.984297	39.405203	77.001127
7.436726	46.153140	77.006132
6.431014	43.643909	77.011137
5.594417	39.879706	77.016142
4.984557	42.680944	77.021147
4.744897	41.116743	77.026151
4.101192	47.315542	77.031156
2.697591	45.360425	77.036161