Tue Jun 08 17:33:20 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.900220	97.042784	0.000000
-1.284679	83.380987	0.005005
-1.741062	57.133102	0.010010
-3.550462	7.315762	0.015014
-7.915388	-1.893967	0.020019
-13.051058	-3.279805	0.025024
-18.714596	2.004309	0.030029
-22.869387	6.643704	0.035034
-26.563795	3.118509	0.040038
-30.541794	3.119347	0.045043
-33.782534	-1.369360	0.050048
-37.548158	-3.601102	0.055053
-41.361258	-7.591423	0.060058
-44.717469	-7.664034	0.065062
-49.291264	-5.929284	0.070067
-52.299404	-8.132225	0.075072
-56.299534	4.526063	0.080077
-59.996627	1.514876	0.085082
-64.104725	-2.564964	0.090086
-67.723664	-1.100896	0.095091
-71.175800	-9.066642	0.100096
-75.011975	-2.258830	0.105101
-78.888889	-0.675917	0.110106
-82.380886	-8.097222	0.115110
-86.189833	2.817234	0.120115
-90.395479	-4.429589	0.125120
-94.157957	-10.989819	0.130125
-97.943997	-3.334461	0.135130
-101.589284	-2.165434	0.140134
-105.253665	-4.603939	0.145139
-108.886939	-9.557738	0.150144
-112.998237	-2.534966	0.155149
-116.895819	-11.390930	0.160154
-120.325983	-9.694343	0.165158
-124.214080	-4.019882	0.170163
-127.083203	-15.611108	0.175168
-131.462351	-15.158519	0.180173
-135.444400	-18.305494	0.185178
-139.203376	-16.191347	0.190182
-143.082337	-5.788234	0.195187
-146.443592	-5.126533	0.200192
-151.057169	-2.541365	0.205197
-155.301663	-1.158621	0.210202
-158.215096	-3.869146	0.215206
-162.163846	-1.962417	0.220211
-165.650366	-1.989698	0.225216
-169.231223	-0.579447	0.230221
-173.002310	2.928950	0.235226
-176.521494	-9.033095	0.240230
-180.419473	-0.854432	0.245235
-183.964193	-8.611980	0.250240
-187.908959	-2.081490	0.255245
-192.038265	2.619201	0.260250
-195.415054	-1.643959	0.265254
-199.525547	8.101855	0.270259
-203.225286	4.341294	0.275264
-206.940743	-0.596750	0.280269
-210.552494	5.740077	0.285274
-214.219409	0.758585	0.290278
-218.324494	-2.124470	0.295283
-222.119255	-3.334678	0.300288
-225.932265	-9.877834	0.305293
-228.877154	0.748012	0.310298
-232.744839	-3.337771	0.315302
-236.916924	4.164052	0.320307
-240.928337	0.447903	0.325312
-244.927029	5.588049	0.330317
-248.819990	8.365093	0.335322
-251.731543	-5.332440	0.340326
-255.882401	1.735130	0.345331
-259.456497	-8.391099	0.350336
-263.382581	-9.137066	0.355341
-267.194849	-1.173155	0.360346
-270.803792	-3.715761	0.365350
-274.850599	3.429498	0.370355
-278.258406	-2.521185	0.375360
-281.825807	-5.289971	0.380365
-285.782187	-3.644309	0.385370
-289.502711	-9.851583	0.390374
-293.714939	3.015355	0.395379
-297.253087	-2.015781	0.400384
-301.199012	-3.995332	0.405389
-304.882697	1.640266	0.410394
-308.139270	-6.796950	0.415398
-312.361402	3.068752	0.420403
-316.053822	-0.715069	0.425408
-319.783188	0.283830	0.430413
-323.766324	1.603348	0.435418
-327.201576	-9.874436	0.440422
-331.426536	-9.555069	0.445427
-334.576460	6.936259	0.450432
-338.260873	-5.530155	0.455437
-341.899744	-2.162322	0.460442
-345.535422	-6.390819	0.465446
-349.724319	-3.758703	0.470451
-353.788676	-6.499810	0.475456
-357.411436	-1.784033	0.480461
-361.617169	-6.123136	0.485466
-364.967505	-4.137319	0.490470
-368.904551	-5.201027	0.495475
-372.640251	-6.271247	0.500480
-375.968884	-3.916539	0.505485
-379.901437	-8.204598	0.510490
-383.532383	-7.502378	0.515494
-387.733227	-9.317733	0.520499
-391.405366	-2.834243	0.525504
-394.810654	-6.499104	0.530509
-399.059254	-6.480333	0.535514
-402.439568	-3.971092	0.540518
-406.622109	-0.212331	0.545523
-410.042873	-15.756447	0.550528
-413.720375	-2.971678	0.555533
-417.718163	-5.830321	0.560538
-420.973961	-4.487084	0.565542
-425.218109	7.992703	0.570547
-428.970708	-6.488757	0.575552
-432.550342	-9.727389	0.580557
-436.618246	-8.876353	0.585562
-439.755315	-6.995353	0.590566
-443.858912	-4.517513	0.595571
-447.429918	-9.489201	0.600576
-451.734851	-1.026183	0.605581
-455.646119	2.480440	0.610586
-458.886134	-7.803178	0.615590
-462.611539	-1.018015	0.620595
-466.310851	-12.558914	0.625600
-470.014394	-5.746316	0.630605
-474.479955	-3.476723	0.635610
-477.497833	-18.853068	0.640614
-481.897918	1.098899	0.645619
-485.613627	-3.163112	0.650624
-489.081884	-6.604741	0.655629
-492.597201	0.998550	0.660634
-496.492782	-1.859794	0.665638
-501.086445	9.043166	0.670643
-504.284038	-0.954428	0.675648
-507.779860	-1.971354	0.680653
-511.592028	0.579696	0.685658
-515.032249	-0.459790	0.690662
-519.034541	-1.163246	0.695667
-522.880960	-9.243704	0.700672
-526.436611	4.654238	0.705677
-530.761396	-2.295398	0.710682
-534.290621	-2.320195	0.715686
-538.172250	-4.421870	0.720691
-541.772832	-4.660585	0.725696
-545.390890	-5.124835	0.730701
-548.866566	0.708138	0.735706
-552.553565	-11.291469	0.740710
-556.881697	-1.934706	0.745715
-560.823242	-10.800063	0.750720
-564.291418	-3.715958	0.755725
-568.052267	-2.277271	0.760730
-571.647088	-2.295914	0.765734
-575.621923	3.090267	0.770739
-579.780992	-5.298439	0.775744
-583.170035	-2.599292	0.780749
-587.215086	-0.863157	0.785754
-590.636487	-6.686911	0.790758
-594.596143	-8.935397	0.795763
-597.724033	-8.211963	0.800768
-601.517437	0.911779	0.805773
-605.994586	-4.304123	0.810778
-609.400334	-8.048857	0.815782
-613.041301	-7.664050	0.820787
-616.518383	-8.116118	0.825792
-620.552478	-10.274443	0.830797
-624.209871	-3.784623	0.835802
-628.125935	-4.818937	0.840806
-632.625868	4.500278	0.845811
-636.150508	-7.212136	0.850816
-639.733542	-5.966522	0.855821
-643.537236	-2.791204	0.860826
-646.958978	-6.994181	0.865830
-651.252808	5.444977	0.870835
-654.981119	5.526278	0.875840
-658.363277	-1.820624	0.880845
-661.811706	-4.059680	0.885850
-665.749589	-2.290553	0.890854
-669.625489	7.804569	0.895859
-673.200621	-1.838377	0.900864
-676.695799	-6.164507	0.905869
-680.739522	-4.301419	0.910874
-684.517491	-5.831057	0.915878
-688.491487	-4.687245	0.920883
-692.732609	-3.502717	0.925888
-696.075074	1.945161	0.930893
-700.107306	0.824671	0.935898
-703.166422	-8.756416	0.940902
-707.109892	0.398293	0.945907
-711.038744	-1.289361	0.950912
-714.634750	2.579793	0.955917
-718.603096	1.989502	0.960922
-722.247590	-5.592170	0.965926
-726.377537	-4.741667	0.970931
-729.797806	-2.229668	0.975936
-733.524854	0.183021	0.980941
-737.392507	7.495276	0.985946
-740.832496	-5.379378	0.990950
-744.695503	-3.894196	0.995955
-748.564999	-2.009637	1.000960
-752.135999	-4.187717	1.005965
-756.554443	-4.865711	1.010970
-759.598168	-9.090056	1.015974
-763.508768	-1.484250	1.020979
-767.479215	4.145271	1.025984
-771.357910	-8.567221	1.030989
-775.331306	-4.883886	1.035994
-778.289392	-1.873720	1.040998
-782.367635	-2.650734	1.046003
-786.120009	-1.535398	1.051008
-789.808085	-9.075975	1.056013
-793.859476	-5.473967	1.061018
-797.159428	-13.551643	1.066022
-801.445858	-10.312678	1.071027
-805.312559	0.491440	1.076032
-809.216072	-3.884877	1.081037
-812.574667	-3.940710	1.086042
-816.177160	-12.430616	1.091046
-820.366698	-4.154829	1.096051
-823.917292	-0.173392	1.101056
-827.349381	-0.310144	1.106061
-831.607834	2.198972	1.111066
-835.208507	-10.655113	1.116070
-838.649755	-5.485816	1.121075
-842.350622	-2.716373	1.126080
-846.415208	3.052917	1.131085
-850.526178	3.396634	1.136090
-853.741570	-7.754098	1.141094
-857.933146	-0.057750	1.146099
-861.635796	-1.585950	1.151104
-865.027526	-7.195107	1.156109
-868.580050	-4.262831	1.161114
-872.490491	-6.086906	1.166118
-876.731528	5.565415	1.171123
-880.343998	-1.630059	1.176128
-884.189122	-5.128631	1.181133
-887.976461	1.779592	1.186138
-891.258944	-4.119855	1.191142
-895.216744	-4.115787	1.196147
-899.093921	-4.088846	1.201152
-902.801918	-4.088576	1.206157
-906.958965	-5.095872	1.211162
-910.345586	-6.208578	1.216166
-914.163780	1.839745	1.221171
-917.914115	-3.909109	1.226176
-921.443877	-11.129791	1.231181
-925.283160	3.134449	1.236186
-928.761862	-9.851001	1.241190
-933.126070	6.472947	1.246195
-936.802063	-0.725781	1.251200
-940.421006	-3.771324	1.256205
-944.262979	7.907278	1.261210
-948.132703	-1.300788	1.266214
-951.936590	0.084434	1.271219
-955.266805	0.266190	1.276224
-959.234644	5.058650	1.281229
-963.159211	-0.466450	1.286234
-966.926991	-6.765245	1.291238
-970.299968	2.610265	1.296243
-974.552479	-3.100082	1.301248
-977.862919	-2.573572	1.306253
-982.053171	3.410029	1.311258
-985.554726	-4.345532	1.316262
-989.620482	0.552967	1.321267
-992.968141	0.611442	1.326272
-996.757090	-3.787916	1.331277
-1000.920114	-2.033122	1.336282
-1004.239764	-4.899090	1.341286
-1007.907108	1.714702	1.346291
-1011.948437	3.550448	1.351296
-1015.898183	-3.634754	1.356301
-1019.459337	1.357124	1.361306
-1022.980359	-8.494108	1.366310
-1027.089979	-3.870654	1.371315
-1030.911496	1.193564	1.376320
-1034.040169	-6.134169	1.381325
-1038.042519	5.741368	1.386330
-1041.893565	-13.469293	1.391334
-1045.785019	-8.246227	1.396339
-1049.681708	-9.596087	1.401344
-1053.542254	-9.860392	1.406349
-1057.296171	9.578101	1.411354
-1060.536793	-4.990619	1.416358
-1064.418769	3.409013	1.421363
-1068.037222	2.269533	1.426368
-1071.656827	-2.733524	1.431373
-1075.929617	2.373483	1.436378
-1079.800408	-7.534473	1.441382
-1083.771357	-1.131760	1.446387
-1087.573167	-3.247819	1.451392
-1090.574221	0.426327	1.456397
-1094.642935	4.498915	1.461402
-1098.040806	-3.011474	1.466406
-1102.288193	8.559246	1.471411
-1106.121747	13.502055	1.476416
-1109.741316	-5.876961	1.481421
-1113.822887	-6.106417	1.486426
-1116.895048	-2.476488	1.491430
-1120.863740	-4.183758	1.496435
-1124.797285	3.048950	1.501440
-1128.615117	1.828900	1.506445
-1132.775205	-2.494760	1.511450
-1136.148325	-7.810850	1.516454
-1139.938183	-2.973408	1.521459
-1143.867898	-9.123841	1.526464
-1147.169693	-11.448064	1.531469
-1151.300623	0.573579	1.536474
-1154.705215	-10.563736	1.541478
-1158.646343	-3.656516	1.546483
-1162.355020	-1.737634	1.551488
-1166.066440	-6.033708	1.556493
-1170.154934	7.304117	1.561498
-1173.612247	-1.292096	1.566502
-1177.248538	-1.658347	1.571507
-1181.120439	1.693734	1.576512
-1184.822776	-7.131946	1.581517
-1188.700444	-1.767844	1.586522
-1192.542105	-1.840281	1.591526
-1196.558088	7.270447	1.596531
-1200.046744	-1.332990	1.601536
-1203.514708	-5.236268	1.606541
-1207.574773	1.742734	1.611546
-1211.042610	-1.474562	1.616550
-1215.361507	7.434013	1.621555
-1218.694568	3.149975	1.626560
-1222.763551	3.222780	1.631565
-1226.405129	2.345547	1.636570
-1229.825836	-1.400444	1.641574
-1233.973966	0.406092	1.646579
-1237.778662	0.946640	1.651584
-1241.433387	-4.939501	1.656589
-1244.685412	-1.789737	1.661594
-1248.733825	-4.875713	1.666598
-1253.001253	-3.768218	1.671603
-1256.692044	6.401358	1.676608
-1260.173266	-2.614582	1.681613
-1263.672535	1.518242	1.686618
-1267.463068	-3.409494	1.691622
-1271.518863	5.226989	1.696627
-1275.336791	-2.421870	1.701632
-1278.632268	-9.343414	1.706637
-1282.994869	2.368028	1.711642
-1286.244527	-9.528744	1.716646
-1290.394585	-1.674941	1.721651
-1294.240793	-9.034733	1.726656
-1297.784871	-4.876030	1.731661
-1301.667168	2.025552	1.736666
-1305.177433	-11.112784	1.741670
-1309.062577	2.275875	1.746675
-1312.838592	-6.838185	1.751680
-1316.507505	-11.877148	1.756685
-1320.170690	-0.362378	1.761690
-1323.745843	0.884814	1.766694
-1327.561728	-3.554601	1.771699
-1331.571132	-0.021677	1.776704
-1335.137689	-6.333762	1.781709
-1339.617277	3.789405	1.786714
-1342.702387	-8.483316	1.791718
-1346.686700	-9.037120	1.796723
-1350.498744	4.715960	1.801728
-1354.398854	-6.516438	1.806733
-1358.007987	-4.434895	1.811738
-1361.644871	-2.444101	1.816742
-1365.536352	-5.692695	1.821747
-1369.268402	-6.356120	1.826752
-1372.937566	-2.094166	1.831757
-1376.755173	5.133053	1.836762
-1379.907238	-0.883511	1.841766
-1384.395607	2.490572	1.846771
-1388.429186	-0.651099	1.851776
-1391.991735	-4.790971	1.856781
-1395.691188	3.574425	1.861786
-1399.421943	-0.859415	1.866790
-1403.099845	-5.832418	1.871795
-1407.172253	-5.025879	1.876800
-1410.469688	-4.926757	1.881805
-1414.415506	-1.890166	1.886810
-1418.121075	-6.352785	1.891814
-1422.084727	-4.597888	1.896819
-1425.996069	0.940744	1.901824
-1429.413135	-9.267406	1.906829
-1433.201153	2.144169	1.911834
-1436.513116	-7.971909	1.916838
-1440.264267	3.407288	1.921843
-1444.438091	-2.669333	1.926848
-1448.121893	-0.963670	1.931853
-1452.513956	0.345817	1.936858
-1456.038379	-12.426019	1.941862
-1459.355988	-5.973786	1.946867
-1463.206642	-1.797410	1.951872
-1466.560725	-6.856376	1.956877
-1470.861749	-9.687168	1.961882
-1474.665293	-5.353101	1.966886
-1478.429620	-5.057671	1.971891
-1481.945735	-0.667985	1.976896
-1485.751914	-3.376952	1.981901
-1489.577230	-5.843437	1.986906
-1493.382288	-4.262154	1.991910
-1496.933887	-11.332120	1.996915
-1501.406560	-6.234430	2.006912
-1502.061154	4.232945	2.016909
-1498.992796	-1.220476	2.026906
-1496.991342	-4.537075	2.036902
-1494.823103	2.678861	2.046899
-1492.295440	-4.417423	2.056896
-1490.583632	-11.563237	2.066893
-1488.689354	-8.734881	2.076890
-1487.026844	-6.296298	2.086886
-1485.285483	-7.907931	2.096883
-1483.184563	-6.858342	2.106880
-1480.911652	-2.817317	2.116877
-1479.307589	-11.205336	2.126874
-1477.495846	-10.924147	2.136870
-1475.652901	-5.112618	2.146867
-1473.834483	-5.663305	2.156864
-1471.790073	-7.464924	2.166861
-1469.766652	-8.901319	2.176858
-1467.985092	-8.508235	2.186854
-1466.359626	-14.794644	2.196851
-1463.900346	-12.989712	2.206848
-1462.334590	-10.773599	2.216845
-1460.530325	-4.278818	2.226842
-1458.458481	-7.013886	2.236838
-1456.861962	-6.497319	2.246835
-1454.790029	-1.347176	2.256832
-1452.634551	-1.916238	2.266829
-1451.077743	-5.373399	2.276826
-1448.919068	-7.213212	2.286822
-1447.068528	-7.965035	2.296819
-1445.391284	-5.897696	2.306816
-1443.580699	-4.239778	2.316813
-1441.425423	-4.912344	2.326810
-1439.552098	-7.303851	2.336806
-1437.779917	-9.683909	2.346803
-1435.891103	-4.953629	2.356800
-1434.136401	-6.864731	2.366797
-1432.616161	-2.028054	2.376794
-1430.265005	-5.116194	2.386790
-1428.072537	-11.627253	2.396787
-1426.310162	-6.592277	2.406784
-1424.789418	-1.454138	2.416781
-1422.648676	-8.347567	2.426778
-1420.967604	-8.834721	2.436774
-1419.040974	-15.307222	2.446771
-1417.005190	-10.625498	2.456768
-1415.536773	-7.168284	2.466765
-1413.227279	-6.230369	2.476762
-1411.466122	-7.055349	2.486758
-1409.741328	-12.230874	2.496755
-1407.870501	-9.327707	2.506752
-1405.692419	-10.759023	2.516749
-1403.992316	-10.872410	2.526746
-1402.205108	-10.305584	2.536742
-1400.091874	-13.236644	2.546739
-1398.321095	-9.342095	2.556736
-1396.518173	-4.180884	2.566733
-1394.599795	-5.980972	2.576730
-1392.392394	-5.444035	2.586726
-1390.822510	-9.070200	2.596723
-1388.760302	-5.398017	2.606720
-1387.333030	-6.011501	2.616717
-1385.332479	-10.005679	2.626714
-1383.429317	-10.181603	2.636710
-1381.388204	-6.850416	2.646707
-1379.292384	-12.252490	2.656704
-1377.414849	-11.347457	2.666701
-1375.722868	-2.205198	2.676698
-1374.133903	-11.594426	2.686694
-1372.336512	-5.916505	2.696691
-1369.959866	-10.036932	2.706688
-1368.163394	-14.667113	2.716685
-1366.288332	-10.455719	2.726682
-1364.525184	-10.982242	2.736678
-1362.954600	-8.898523	2.746675
-1361.094303	1.868393	2.756672
-1358.521301	-3.640144	2.766669
-1357.228153	-5.516988	2.776666
-1355.117093	-5.541280	2.786662
-1353.120235	-6.839081	2.796659
-1351.705008	-4.635007	2.806656
-1349.316696	-3.703480	2.816653
-1347.609117	-8.202984	2.826650
-1345.833101	0.397646	2.836646
-1343.803515	-3.543406	2.846643
-1341.634186	-3.455580	2.856640
-1340.309321	-6.730983	2.866637
-1338.431982	-5.164316	2.876634
-1336.319222	1.513878	2.886630
-1334.121580	-8.053795	2.896627
-1332.872971	-5.473310	2.906624
-1330.636171	-3.025410	2.916621
-1328.807895	-1.092250	2.926618
-1326.988649	-0.083516	2.936614
-1324.932056	-4.175822	2.946611
-1323.283683	-1.954082	2.956608
-1321.368829	-2.516130	2.966605
-1319.167614	-3.507554	2.976602
-1317.491256	-7.321924	2.986598
-1315.492794	-7.167981	2.996595
-1314.142621	-2.643900	3.006592
-1312.160583	-1.091251	3.016589
-1310.100555	-4.376726	3.026586
-1308.042365	-1.974805	3.036582
-1306.209007	-3.219605	3.046579
-1304.374691	-6.203098	3.056576
-1302.763617	-9.530021	3.066573
-1300.981857	-7.614153	3.076570
-1298.633866	-6.203790	3.086566
-1296.981257	-9.042250	3.096563
-1294.907439	-8.742761	3.106560
-1293.096966	-1.188610	3.116557
-1291.313607	-3.125524	3.126554
-1289.721795	-1.262391	3.136550
-1287.696350	-4.554563	3.146547
-1285.517167	-9.033475	3.156544
-1283.620871	-4.675505	3.166541
-1281.917317	-7.127895	3.176538
-1280.093449	-3.733653	3.186534
-1278.115080	-6.499218	3.196531
-1276.171712	-11.899171	3.206528
-1274.621863	-0.661942	3.216525
-1272.163131	2.558848	3.226522
-1270.696075	-1.078073	3.236518
-1268.878387	-0.862233	3.246515
-1266.781568	-2.720973	3.256512
-1265.071389	-1.893061	3.266509
-1263.339995	3.425150	3.276506
-1261.250342	1.071258	3.286502
-1259.381271	0.948671	3.296499
-1257.480342	-0.933726	3.306496
-1255.538575	4.423053	3.316493
-1253.632301	-3.580496	3.326490
-1252.055754	4.142298	3.336486
-1249.891831	1.538925	3.346483
-1247.990603	-3.175601	3.356480
-1246.162187	4.726047	3.366477
-1244.593346	1.949416	3.376474
-1242.424446	-0.722389	3.386470
-1240.390434	-0.188394	3.396467
-1239.067596	1.488964	3.406464
-1237.237189	1.113769	3.416461
-1234.548190	3.974520	3.426458
-1233.151755	-1.355596	3.436454
-1231.218572	5.665322	3.446451
-1229.373142	-7.469065	3.456448
-1227.453778	-3.641054	3.466445
-1225.787138	4.238592	3.476442
-1223.712444	-6.244572	3.486438
-1221.756671	-2.395936	3.496435
-1219.877578	0.176298	3.506432
-1218.105272	-3.226897	3.516429
-1216.174050	0.985601	3.526426
-1214.504806	-7.326196	3.536422
-1212.731978	-6.655644	3.546419
-1210.487870	-3.863518	3.556416
-1208.679154	5.228747	3.566413
-1206.849274	-0.837383	3.576410
-1204.801008	-2.122209	3.586406
-1203.165228	-2.544983	3.596403
-1201.131170	-5.797888	3.606400
-1199.644918	3.207482	3.616397
-1197.345188	-3.167765	3.626394
-1195.511249	-4.682546	3.636390
-1193.342572	-2.527972	3.646387
-1191.925706	1.843216	3.656384
-1190.204708	7.529609	3.666381
-1187.927136	4.036889	3.676378
-1186.091162	8.195808	3.686374
-1184.306836	-3.628225	3.696371
-1182.346109	-0.201715	3.706368
-1180.469042	7.399948	3.716365
-1178.884423	3.328289	3.726362
-1176.737436	-2.723518	3.736358
-1175.056795	0.969251	3.746355
-1173.179005	2.507463	3.756352
-1171.272896	3.211265	3.766349
-1169.055175	4.802159	3.776346
-1167.303583	7.180529	3.786342
-1165.528758	1.776756	3.796339
-1163.907104	-1.810404	3.806336
-1162.014874	2.249152	3.816333
-1159.951904	1.831682	3.826330
-1157.896110	1.178714	3.836326
-1156.048583	-5.603782	3.846323
-1154.145238	-0.089779	3.856320
-1152.429846	1.950979	3.866317
-1150.710933	12.063722	3.876314
-1148.719396	0.637660	3.886310
-1146.771314	4.755609	3.896307
-1144.791770	3.609871	3.906304
-1142.975510	5.560593	3.916301
-1141.252065	3.221822	3.926298
-1139.008935	-4.079932	3.936294
-1137.444394	-0.381043	3.946291
-1135.915123	1.030889	3.956288
-1133.728841	-0.629341	3.966285
-1131.808125	-0.016161	3.976282
-1129.770943	-1.882380	3.986278
-1127.845458	0.814327	3.996275
-1126.207530	-0.423713	4.006272
-1124.206094	8.963926	4.016269
-1122.451084	8.164228	4.026266
-1120.474517	6.556219	4.036262
-1118.642579	1.728755	4.046259
-1116.864017	-0.256272	4.056256
-1114.758035	0.653129	4.066253
-1113.109030	1.626375	4.076250
-1111.021531	-3.479723	4.086246
-1109.150157	-2.262082	4.096243
-1107.432470	-8.400992	4.106240
-1105.656537	-1.757705	4.116237
-1103.388637	-4.751544	4.126234
-1101.627155	-6.735607	4.136230
-1099.853929	-1.631595	4.146227
-1098.132284	-2.787963	4.156224
-1096.042140	4.000170	4.166221
-1094.291949	-2.107960	4.176218
-1092.434844	0.625009	4.186214
-1090.426573	-1.310528	4.196211
-1088.331579	-0.447443	4.206208
-1086.916099	-5.982741	4.216205
-1084.964973	-5.681842	4.226202
-1082.726984	-0.846535	4.236198
-1081.139699	-7.211239	4.246195
-1079.447998	-3.173332	4.256192
-1077.261275	-1.813798	4.266189
-1075.405332	-0.855122	4.276186
-1073.649490	0.423474	4.286182
-1071.550559	0.107370	4.296179
-1069.647599	3.865955	4.306176
-1068.231534	-1.037497	4.316173
-1065.896490	3.380412	4.326170
-1063.953233	-6.966302	4.336166
-1062.418467	-3.920297	4.346163
-1060.678123	-9.547726	4.356160
-1058.752979	-7.337039	4.366157
-1056.799144	-5.534787	4.376154
-1054.821841	-6.106252	4.386150
-1052.756745	-12.805130	4.396147
-1051.033673	-2.945205	4.406144
-1049.151923	-3.346129	4.416141
-1047.328549	-2.921708	4.426138
-1045.552724	-3.415497	4.436134
-1043.416237	-2.716019	4.446131
-1041.941428	-3.207920	4.456128
-1039.895151	-3.143074	4.466125
-1037.939635	1.551848	4.476122
-1035.903490	-0.169898	4.486118
-1034.352381	3.057483	4.496115
-1032.570141	3.893275	4.506112
-1030.179652	0.301809	4.516109
-1028.631921	1.076692	4.526106
-1026.769653	-0.020402	4.536102
-1024.471160	-3.728465	4.546099
-1022.850244	-2.816360	4.556096
-1021.114138	0.521539	4.566093
-1019.367474	-6.687809	4.576090
-1017.199111	-2.125853	4.586086
-1015.067566	-6.771935	4.596083
-1013.729291	-1.497959	4.606080
-1011.758639	-0.456590	4.616077
-1009.803257	0.166108	4.626074
-1007.875489	-10.900768	4.636070
-1006.318392	-9.013779	4.646067
-1004.178066	-8.260006	4.656064
-1002.347327	-3.255536	4.666061
-1000.309265	-6.259660	4.676058
-998.364936	-3.352317	4.686054
-996.288168	-7.215557	4.696051
-994.715471	-6.799453	4.706048
-992.918865	-1.891873	4.716045
-991.015104	-5.621863	4.726042
-989.577689	-1.356090	4.736038
-987.159755	-6.367497	4.746035
-985.331300	-1.761000	4.756032
-983.679617	-3.197768	4.766029
-981.888833	1.146851	4.776026
-979.794464	-1.328258	4.786022
-977.711142	-6.478635	4.796019
-976.012070	-5.620241	4.806016
-974.083890	-3.323088	4.816013
-972.365595	-3.789186	4.826010
-970.505540	-4.719492	4.836006
-968.487748	-5.117257	4.846003
-966.685832	3.977882	4.856000
-964.400651	2.252936	4.865997
-962.847453	-0.811394	4.875994
-961.137680	0.967198	4.885990
-959.131678	2.658972	4.895987
-957.342933	3.481428	4.905984
-955.660990	1.907474	4.915981
-953.216361	-0.700869	4.925978
-951.704352	-3.391763	4.935974
-949.658180	-1.153584	4.945971
-947.936156	-5.290647	4.955968
-945.799746	-1.922634	4.965965
-944.289960	0.772016	4.975962
-941.955272	1.054165	4.985958
-940.126412	-7.590845	4.995955
-938.502644	-5.279356	5.005952
-936.606144	-2.482336	5.015949
-934.820667	-2.719664	5.025946
-932.922146	2.822946	5.035942
-930.981078	-3.118709	5.045939
-929.360325	3.576205	5.055936
-927.166207	-1.657986	5.065933
-925.357803	-6.493191	5.075930
-923.442941	-10.234939	5.085926
-921.349008	-4.869334	5.095923
-919.707040	-2.421451	5.105920
-917.895507	3.117524	5.115917
-916.182038	-3.189356	5.125914
-913.965427	2.101447	5.135910
-912.438402	1.446098	5.145907
-910.509378	2.632986	5.155904
-908.480564	0.998714	5.165901
-906.365898	2.993167	5.175898
-904.917302	4.832427	5.185894
-902.903209	-3.425446	5.195891
-900.850058	-0.318184	5.205888
-899.036961	-5.769926	5.215885
-897.140389	-4.946985	5.225882
-895.600348	-4.031618	5.235878
-893.004631	-2.271893	5.245875
-891.517267	-4.117920	5.255872
-890.003106	1.631386	5.265869
-887.924878	-1.108864	5.275866
-885.857188	-1.244041	5.285862
-883.883578	-0.778548	5.295859
-882.099469	-6.697981	5.305856
-880.309459	-1.744951	5.315853
-878.321294	-1.854221	5.325850
-876.633934	-0.530983	5.335846
-874.825253	-2.081213	5.345843
-873.030957	0.325918	5.355840
-870.967487	-0.154338	5.365837
-868.848858	0.708356	5.375834
-867.298969	-0.454403	5.385830
-865.273628	-3.365782	5.395827
-863.187522	-3.214418	5.405824
-861.395713	-3.868565	5.415821
-859.727649	-3.044323	5.425818
-857.748917	-4.442729	5.435814
-856.044165	-6.176274	5.445811
-853.998227	-0.196926	5.455808
-852.193464	1.690294	5.465805
-850.529575	0.684237	5.475802
-848.521482	0.918951	5.485798
-846.462670	0.936289	5.495795
-844.599136	-1.845341	5.505792
-842.970983	3.856358	5.515789
-840.917953	-0.026453	5.525786
-838.717655	-4.876332	5.535782
-836.886147	1.421619	5.545779
-835.353277	-0.951116	5.555776
-833.554607	0.900403	5.565773
-831.786119	-3.512153	5.575770
-829.869237	-1.976543	5.585766
-827.238779	0.090268	5.595763
-825.527002	0.633534	5.605760
-824.273704	1.975574	5.615757
-822.415821	0.471064	5.625754
-820.408601	2.223953	5.635750
-818.392055	-6.286058	5.645747
-816.404170	-1.974798	5.655744
-814.594136	2.759436	5.665741
-812.910576	4.119712	5.675738
-810.954657	-3.367356	5.685734
-808.884628	-2.723143	5.695731
-807.212574	-6.505767	5.705728
-805.344520	-6.852857	5.715725
-803.377540	-6.702754	5.725722
-801.105989	-4.478288	5.735718
-799.690419	-3.241160	5.745715
-797.927361	-6.543410	5.755712
-796.091946	-6.121342	5.765709
-793.928264	-0.565289	5.775706
-792.227513	-3.226479	5.785702
-790.186822	1.678035	5.795699
-788.301268	0.645417	5.805696
-786.505300	4.169961	5.815693
-784.647294	-2.309889	5.825690
-782.707701	0.755667	5.835686
-780.776921	-2.904972	5.845683
-778.981794	-3.729992	5.855680
-777.141119	2.765997	5.865677
-775.399550	4.289040	5.875674
-773.203661	0.086910	5.885670
-771.664879	-1.733915	5.895667
-769.638872	-1.657162	5.905664
-768.049126	1.090623	5.915661
-765.893726	2.186951	5.925658
-763.739150	-1.491935	5.935654
-762.075704	-0.487830	5.945651
-759.888636	2.874355	5.955648
-758.398888	3.370389	5.965645
-756.369784	3.150602	5.975642
-754.773062	2.863935	5.985638
-752.651341	2.242527	5.995635
-750.539457	1.879301	6.005632
-748.916511	8.245105	6.015629
-747.082416	5.737310	6.025626
-745.528471	3.021104	6.035622
-743.552559	2.202616	6.045619
-741.373647	-1.508893	6.055616
-739.486622	3.092018	6.065613
-737.620694	3.284789	6.075610
-736.228396	0.682090	6.085606
-733.643795	5.170793	6.095603
-731.748982	2.575122	6.105600
-730.189941	6.085815	6.115597
-728.545324	2.592873	6.125594
-726.495013	2.408587	6.135590
-724.522228	-2.593083	6.145587
-722.794824	-0.172824	6.155584
-720.620731	3.188447	6.165581
-718.965828	3.096924	6.175578
-717.268988	1.130031	6.185574
-715.282001	1.604373	6.195571
-713.158666	2.810172	6.205568
-711.060099	3.258252	6.215565
-709.650175	5.584798	6.225562
-707.716398	7.925382	6.235558
-705.809789	6.427180	6.245555
-704.204502	-0.992561	6.255552
-702.191292	3.106134	6.265549
-699.929011	0.064451	6.275546
-698.172127	2.280868	6.285542
-696.455795	-1.108573	6.295539
-694.311466	0.594368	6.305536
-692.808814	7.659818	6.315533
-690.961743	0.478397	6.325530
-688.977103	3.065173	6.335526
-686.936723	11.316069	6.345523
-685.191949	11.006391	6.355520
-683.269951	10.219313	6.365517
-681.604202	7.672062	6.375514
-679.430240	3.419197	6.385510
-677.661267	2.341422	6.395507
-675.816073	2.729455	6.405504
-673.870424	4.607199	6.415501
-672.070172	5.104911	6.425498
-669.998872	-0.274473	6.435494
-668.339978	1.054525	6.445491
-666.342655	0.168372	6.455488
-664.724800	1.432880	6.465485
-662.825146	0.352050	6.475482
-660.525531	-4.456300	6.485478
-658.971719	-8.949727	6.495475
-657.003751	-1.613169	6.505472
-655.075238	-3.793294	6.515469
-653.151892	-5.459940	6.525466
-651.566063	-9.154995	6.535462
-649.311320	-5.491356	6.545459
-647.562584	-0.346569	6.555456
-645.768812	-6.217783	6.565453
-643.834296	-3.557965	6.575450
-641.818048	-7.435563	6.585446
-640.079310	-9.710768	6.595443
-638.281766	-8.713423	6.605440
-637.115707	-7.584791	6.615437
-634.600170	-4.455566	6.625434
-632.323323	-8.692073	6.635430
-630.656134	-12.974141	6.645427
-628.991380	-10.986524	6.655424
-627.023352	-4.805171	6.665421
-624.974136	-4.321706	6.675418
-623.254472	-8.749916	6.685414
-621.503773	-9.681861	6.695411
-619.434391	-6.736118	6.705408
-617.400313	-5.865115	6.715405
-615.800207	-6.713515	6.725402
-613.860456	-4.430824	6.735398
-612.177339	-5.084400	6.745395
-610.214487	-6.740812	6.755392
-608.019981	-6.523351	6.765389
-606.329552	-5.703242	6.775386
-604.340859	-7.098107	6.785382
-602.494923	-10.446913	6.795379
-601.048427	-10.050112	6.805376
-598.779347	-7.582450	6.815373
-597.001189	-7.863833	6.825370
-595.040840	-11.850383	6.835366
-592.794445	-12.604953	6.845363
-591.148362	-10.203884	6.855360
-589.444726	-9.001098	6.865357
-587.704851	-4.507262	6.875354
-585.882225	-1.027910	6.885350
-584.286954	-1.765600	6.895347
-582.013891	-7.866052	6.905344
-579.932183	0.476215	6.915341
-578.231209	2.049779	6.925338
-576.612206	-0.653427	6.935334
-574.253231	-6.666652	6.945331
-572.225689	1.419725	6.955328
-570.645700	-3.778091	6.965325
-568.947570	-1.270541	6.975322
-566.852473	-2.738582	6.985318
-565.153692	-5.634504	6.995315
-563.053865	-1.090573	7.005312
-561.358290	0.290664	7.015309
-559.385348	-1.688767	7.025306
-557.785991	6.468721	7.035302
-556.065067	7.245677	7.045299
-553.784436	1.445088	7.055296
-551.845760	-0.911422	7.065293
-550.166846	-0.330396	7.075290
-548.194310	2.341125	7.085286
-546.046761	0.119905	7.095283
-544.309518	-4.464244	7.105280
-542.828688	-1.298122	7.115277
-540.659284	-1.998353	7.125274
-538.504952	4.512309	7.135270
-537.013047	-2.629855	7.145267
-535.162096	-6.064072	7.155264
-533.332373	-1.923140	7.165261
-531.179150	-4.141374	7.175258
-529.619494	-3.847354	7.185254
-527.662181	-6.203495	7.195251
-525.489493	-1.991774	7.205248
-523.883093	-0.178270	7.215245
-521.972728	3.790352	7.225242
-519.943043	4.149959	7.235238
-518.237558	4.923651	7.245235
-516.141184	0.877432	7.255232
-514.469983	5.689772	7.265229
-512.483169	4.949348	7.275226
-510.603066	5.400625	7.285222
-508.869776	5.760108	7.295219
-506.861918	3.934770	7.305216
-505.082886	-1.956790	7.315213
-503.148617	2.253957	7.325210
-501.375337	-1.257426	7.335206
-499.153093	4.494652	7.345203
-497.583668	1.947789	7.355200
-496.000439	0.256568	7.365197
-493.756088	-2.754669	7.375194
-491.803688	2.005087	7.385190
-489.748239	0.019434	7.395187
-488.090275	-1.901183	7.405184
-486.403145	0.305950	7.415181
-484.211527	0.629491	7.425178
-482.294851	-1.084155	7.435174
-480.811553	-2.750716	7.445171
-478.860648	-8.611680	7.455168
-476.810049	-1.411325	7.465165
-475.093351	-2.254780	7.475162
-473.221499	-1.784288	7.485158
-471.264037	-0.495371	7.495155
-469.236667	-3.380447	7.505152
-467.510713	1.380626	7.515149
-465.397859	4.346260	7.525146
-463.897311	4.916424	7.535142
-461.715861	-0.663571	7.545139
-460.090266	-0.463043	7.555136
-457.799898	1.738227	7.565133
-456.231324	2.342172	7.575130
-454.324741	-0.232484	7.585126
-452.833042	-1.779147	7.595123
-450.681791	4.064971	7.605120
-448.743439	7.193740	7.615117
-446.913185	1.714709	7.625114
-444.974511	1.221678	7.635110
-443.062086	-2.973168	7.645107
-441.343069	-6.170509	7.655104
-439.145176	1.205762	7.665101
-437.320038	-5.961531	7.675098
-435.638375	-3.019132	7.685094
-433.960731	1.877898	7.695091
-431.848044	0.612017	7.705088
-429.849745	2.178502	7.715085
-428.218675	1.265968	7.725082
-426.033907	0.634690	7.735078
-424.116620	0.913635	7.745075
-422.342456	-2.042991	7.755072
-420.821728	-0.433699	7.765069
-419.128776	4.848418	7.775066
-416.909430	-1.602788	7.785062
-414.553148	0.801799	7.795059
-412.998159	-3.318675	7.805056
-411.336983	-3.846290	7.815053
-409.391466	-0.651548	7.825050
-407.558254	-0.369634	7.835046
-405.442142	-5.684667	7.845043
-403.517919	-2.123067	7.855040
-401.539251	-7.103485	7.865037
-400.300316	-5.753322	7.875034
-398.212369	-6.975817	7.885030
-395.998012	-11.214534	7.895027
-394.262253	-4.495246	7.905024
-392.898697	-4.684872	7.915021
-390.399373	-6.021408	7.925018
-388.481057	-4.289026	7.935014
-386.465820	-0.409470	7.945011
-385.408836	1.578566	7.955008
-383.199537	-1.143238	7.965005
-381.125679	-2.141988	7.975002
-379.348962	-0.923988	7.984998
-377.074296	-2.717182	7.994995
-375.378506	-4.271956	8.004992
-373.951309	-2.726436	8.014989
-371.857269	-3.729039	8.024986
-369.930767	-1.120677	8.034982
-367.897774	0.835496	8.044979
-366.450657	-1.462700	8.054976
-364.476592	-5.855421	8.064973
-362.336159	-6.880601	8.074970
-360.333884	-4.973301	8.084966
-358.517919	-10.081506	8.094963
-356.638917	-12.089790	8.104960
-355.037613	-3.964168	8.114957
-353.046564	-9.243496	8.124954
-351.154739	-6.263999	8.134950
-349.188910	-6.870726	8.144947
-347.364445	-7.233463	8.154944
-345.878610	-10.473766	8.164941
-343.793085	-1.890150	8.174938
-341.692276	-4.422987	8.184934
-339.742063	3.591023	8.194931
-338.119366	3.873902	8.204928
-336.252288	-2.293942	8.214925
-334.127096	-7.856720	8.224922
-332.337234	-4.682668	8.234918
-330.519212	-0.291441	8.244915
-328.572142	-8.607951	8.254912
-327.036440	-3.921682	8.264909
-325.040668	-3.537198	8.274906
-323.079408	-6.527855	8.284902
-320.945485	-11.785042	8.294899
-318.976997	-2.926820	8.304896
-317.490382	-3.930333	8.314893
-315.524046	-3.115545	8.324890
-313.533364	-1.376176	8.334886
-312.243785	-5.511561	8.344883
-309.492390	-8.389944	8.354880
-308.461163	-5.228821	8.364877
-305.979112	-1.401237	8.374874
-304.026513	2.500171	8.384870
-302.082443	-0.973250	8.394867
-300.431436	-0.297231	8.404864
-298.976353	-2.747745	8.414861
-296.733268	-1.488375	8.424858
-294.555759	-3.765600	8.434854
-292.804018	-11.681833	8.444851
-291.431101	-7.369563	8.454848
-289.461932	-4.466538	8.464845
-287.243518	-8.863594	8.474842
-285.645573	-6.661635	8.484838
-283.656263	-7.597622	8.494835
-281.546567	-2.457278	8.504832
-279.670488	-5.312766	8.514829
-278.065480	-3.298952	8.524826
-276.181915	-0.627061	8.534822
-274.093755	-4.985567	8.544819
-272.227004	-6.072842	8.554816
-270.569551	-6.239331	8.564813
-268.598113	-5.767257	8.574810
-266.657209	-8.154859	8.584807
-264.869346	-10.642678	8.594803
-263.005075	-4.776903	8.604800
-261.182312	-7.564748	8.614797
-258.979840	-8.707228	8.624794
-257.459616	-7.799694	8.634791
-255.462248	-18.043175	8.644787
-253.740918	-17.706044	8.654784
-251.867206	-10.587869	8.664781
-249.609138	-10.752238	8.674778
-248.032643	-9.304213	8.684775
-246.079843	-9.024564	8.694771
-244.417034	-14.677940	8.704768
-242.112342	-10.549179	8.714765
-240.444019	-6.562626	8.724762
-238.495853	-6.976967	8.734759
-236.783970	-7.761016	8.744755
-234.840367	-7.602696	8.754752
-232.831351	-10.112231	8.764749
-230.746867	-13.702974	8.774746
-228.975651	-15.222019	8.784743
-227.358859	-20.729170	8.794739
-225.261515	-19.519860	8.804736
-223.569252	-15.840934	8.814733
-221.772557	-14.370989	8.824730
-219.967302	-13.989352	8.834727
-217.655481	-15.036349	8.844723
-216.052769	-20.670713	8.854720
-214.165247	-14.146525	8.864717
-212.578076	-14.444007	8.874714
-210.269571	-13.838829	8.884711
-208.422236	-9.277101	8.894707
-206.859691	-20.554172	8.904704
-204.771579	-14.746128	8.914701
-202.775502	-10.891259	8.924698
-201.222156	-17.281498	8.934695
-199.395551	-12.878250	8.944691
-197.267331	-10.837551	8.954688
-195.068712	-11.620484	8.964685
-193.574706	-13.376529	8.974682
-192.018445	-13.645780	8.984679
-189.699080	-13.054309	8.994675
-187.894430	-13.325451	9.004672
-185.938884	-12.799633	9.014669
-184.375945	-9.464874	9.024666
-182.216951	-12.436821	9.034663
-180.472514	-17.795908	9.044659
-178.523620	-10.426587	9.054656
-176.600459	-0.560618	9.064653
-174.676274	-10.475354	9.074650
-172.690663	-21.790193	9.084647
-171.287102	-17.903647	9.094643
-169.482856	-16.787507	9.104640
-167.206340	-17.780999	9.114637
-165.383208	-13.332085	9.124634
-163.349253	-15.060179	9.134631
-161.632430	-11.133686	9.144627
-159.899358	-12.895544	9.154624
-158.230342	-10.183251	9.164621
-155.680807	-11.720740	9.174618
-154.056127	-16.595693	9.184615
-152.249564	-19.355028	9.194611
-150.225410	-16.253487	9.204608
-148.702785	-9.986022	9.214605
-146.844275	-18.302691	9.224602
-144.859112	-15.632754	9.234599
-143.052109	-14.745511	9.244595
-140.780895	-14.223615	9.254592
-138.932382	-15.275696	9.264589
-137.622557	-10.917773	9.274586
-135.295486	-10.950456	9.284583
-133.249301	-14.644855	9.294579
-131.395881	-10.508991	9.304576
-129.929756	1.013475	9.314573
-128.005523	-1.932814	9.324570
-125.840807	-6.088204	9.334567
-124.331679	1.087424	9.344563
-122.381909	-2.637074	9.354560
-120.615641	-8.742103	9.364557
-118.791828	-4.732762	9.374554
-116.347465	-9.815853	9.384551
-114.558355	-7.965945	9.394547
-112.939573	-13.412148	9.404544
-111.219302	-7.371820	9.414541
-109.091884	-5.177990	9.424538
-107.247198	-11.933944	9.434535
-105.232317	-4.233246	9.444531
-103.424537	-6.296009	9.454528
-101.650794	-3.076013	9.464525
-99.714760	-3.869598	9.474522
-97.947880	-10.229243	9.484519
-95.998572	-5.907455	9.494515
-94.094932	-3.524667	9.504512
-92.228654	-6.367732	9.514509
-90.420077	-3.980892	9.524506
-88.273130	-0.530057	9.534503
-86.633234	-6.977004	9.544499
-84.896000	-10.050480	9.554496
-82.883670	-7.061885	9.564493
-80.831904	-7.526727	9.574490
-79.105351	-5.868032	9.584487
-77.377507	-5.338690	9.594483
-75.217332	-0.363398	9.604480
-73.650507	0.056418	9.614477
-71.805494	-3.573030	9.624474
-69.756961	-5.190553	9.634471
-67.784703	-5.180539	9.644467
-65.745326	-10.325371	9.654464
-64.152035	-5.948843	9.664461
-62.064096	-4.293223	9.674458
-60.604565	-5.764293	9.684455
-58.642936	-6.322354	9.694451
-56.385707	-5.522552	9.704448
-54.656771	-8.545588	9.714445
-52.861386	-11.702929	9.724442
-50.780986	-7.874301	9.734439
-49.199936	-13.117592	9.744435
-47.258221	-13.287688	9.754432
-45.158824	-8.801514	9.764429
-43.462362	-1.571029	9.774426
-41.848012	-5.861236	9.784423
-39.737435	-8.914138	9.794419
-37.598731	-10.293379	9.804416
-36.110691	-10.714103	9.814413
-34.256564	-7.983309	9.824410
-32.113256	-2.925664	9.834407
-30.260612	-2.532710	9.844403
-28.621378	-3.452035	9.854400
-26.276458	-6.325769	9.864397
-24.653795	-0.198315	9.874394
-22.922154	-5.715223	9.884391
-20.821079	-8.291438	9.894387
-19.043550	-4.706482	9.904384
-16.970283	-5.004644	9.914381
-15.649738	-1.527082	9.924378
-13.243727	-1.122295	9.934375
-11.290061	-3.711567	9.944371
-9.651262	-6.905675	9.954368
-7.640520	-2.580940	9.964365
-6.010923	-2.525188	9.974362
-4.517136	9.126972	9.984359
-3.120907	34.548233	9.994355
-2.273041	88.207835	10.004352
-1.006255	156.954062	10.014349
0.000000	220.634198	10.019354
0.937368	266.303293	10.024359
1.359458	307.417797	10.029363
1.979056	353.112818	10.034368
2.588242	375.667681	10.039373
2.851864	396.462163	10.044378
3.049842	421.579471	10.049383
3.799378	427.211930	10.054387
4.145921	452.428152	10.059392
4.370483	463.856349	10.064397
4.519152	470.630363	10.069402
4.236948	472.114764	10.074407
4.093457	467.960844	10.079411
3.932528	481.580337	10.084416
4.609351	473.740756	10.089421
4.378833	475.554178	10.094426
4.320612	482.511692	10.099431
4.690473	473.679517	10.104435
4.517049	483.966931	10.109440
4.412950	483.073376	10.114445
4.521090	496.958974	10.119450
4.784935	514.216854	10.124455
5.149029	519.731098	10.129459
5.174927	530.891838	10.134464
4.915495	509.243089	10.139469
5.107480	508.207980	10.144474
5.000876	515.114990	10.149479
5.434006	528.626351	10.154483
5.076631	522.117061	10.159488
4.993433	505.572671	10.164493
4.832789	521.640621	10.169498
4.884626	540.590354	10.174503
5.085838	539.828784	10.179507
4.916554	546.085392	10.184512
5.182258	547.715058	10.189517
4.992356	550.613332	10.194522
4.978278	564.362845	10.199527
5.536549	561.090388	10.204531
5.350263	577.889482	10.209536
5.687838	583.383823	10.214541
5.749034	585.589332	10.219546
5.616581	581.688482	10.224551
6.077105	582.046889	10.229555
5.628489	588.367591	10.234560
5.785347	591.063527	10.239565
5.866371	582.767907	10.244570
5.898375	589.483031	10.249575
6.544497	592.613748	10.254579
6.273446	601.700644	10.259584
6.439598	606.813870	10.264589
6.410789	594.512053	10.269594
5.968898	602.813922	10.274599
5.953001	597.215891	10.279603
5.918771	609.144475	10.284608
5.781831	605.634773	10.289613
6.123703	608.784108	10.294618
5.967643	616.944610	10.299623
6.166047	606.826924	10.304627
6.191323	614.285693	10.309632
6.180460	635.015455	10.314637
6.407491	642.869107	10.319642
6.482179	647.697643	10.324647
6.448706	649.188753	10.329651
6.257964	656.402350	10.334656
6.258719	652.642059	10.339661
6.741240	653.311689	10.344666
6.680128	651.993527	10.349671
7.025378	656.753965	10.354675
6.776247	657.934297	10.359680
6.691757	652.955494	10.364685
6.940347	668.827510	10.369690
7.173689	682.495626	10.374695
7.422981	678.564428	10.379699
7.106017	674.727164	10.384704
7.309592	670.229083	10.389709
7.136942	669.729367	10.394714
7.163918	681.981058	10.399719
7.547333	685.457620	10.404723
7.771394	676.670067	10.409728
7.520880	670.974872	10.414733
7.851122	673.170578	10.419738
7.256079	676.942797	10.424743
7.437180	672.541330	10.429747
7.263712	672.159383	10.434752
7.450102	670.796020	10.439757
7.520683	673.839124	10.444762
7.664433	692.075403	10.449767
7.888272	693.395296	10.454771
7.705413	699.712712	10.459776
7.535732	696.796354	10.464781
7.609741	698.811002	10.469786
7.618058	701.211906	10.474791
7.797708	696.607001	10.479795
7.650827	704.794001	10.484800
8.179743	712.855659	10.489805
8.143144	702.265848	10.494810
7.597959	710.259438	10.499815
7.915047	710.602969	10.504819
8.379761	717.596054	10.509824
8.293120	713.153643	10.514829
8.402792	717.352924	10.519834
7.949242	724.411091	10.524839
8.057198	736.336709	10.529843
8.495402	747.138756	10.534848
8.432593	749.992382	10.539853
8.693026	750.487336	10.544858
8.785381	749.211930	10.549863
8.875073	746.043462	10.554867
8.848596	755.195484	10.559872
8.861460	750.066144	10.564877
8.719143	756.782414	10.569882
8.235520	757.668623	10.574887
8.935912	743.136960	10.579891
8.939975	760.792938	10.584896
8.819822	748.342059	10.589901
8.700628	753.658598	10.594906
8.343323	758.082824	10.599911
8.835583	755.697158	10.604915
8.684696	765.787080	10.609920
8.850458	772.136723	10.614925
8.979485	778.243988	10.619930
8.843953	784.449114	10.624935
9.361359	785.771575	10.629939
9.242617	791.683699	10.634944
9.507033	786.146090	10.639949
9.445956	787.015508	10.644954
9.137742	796.181124	10.649959
9.568777	788.538661	10.654963
9.727054	787.649443	10.659968
9.759367	786.690640	10.664973
9.881278	784.360574	10.669978
9.849038	791.671002	10.674983
10.302205	789.740448	10.679987
9.884412	794.670443	10.684992
9.930435	790.877489	10.689997
9.979990	787.498793	10.695002
9.798302	790.117418	10.700007
9.891228	777.084463	10.705011
9.412584	793.327608	10.710016
9.486443	790.124742	10.715021
9.580776	788.253739	10.720026
9.516846	795.529735	10.725031
9.898726	799.256846	10.730035
10.001113	812.414249	10.735040
9.989732	822.558445	10.740045
10.245062	825.021619	10.745050
9.917950	832.866566	10.750055
10.180295	825.982868	10.755059
10.193312	830.554800	10.760064
10.147383	832.979236	10.765069
10.557857	831.986380	10.770074
10.429405	841.557774	10.775079
11.025380	826.354340	10.780083
10.759745	831.388519	10.785088
10.662841	833.042494	10.790093
10.550584	836.016323	10.795098
10.686641	840.123483	10.800103
10.691248	833.731994	10.805107
10.927761	842.763186	10.810112
10.893844	840.281806	10.815117
10.949716	835.340456	10.820122
10.817743	844.800747	10.825127
11.094261	844.475456	10.830131
11.178998	862.432713	10.835136
11.076636	865.469587	10.840141
11.709441	853.890564	10.845146
11.123767	845.207805	10.850151
11.030499	839.591770	10.855155
11.318124	845.022139	10.860160
11.820595	849.282395	10.865165
11.105676	843.577949	10.870170
11.182698	852.881622	10.875175
11.554074	859.236309	10.880179
11.744026	862.574375	10.885184
11.294243	851.577284	10.890189
11.825514	859.132569	10.895194
11.863046	873.010871	10.900199
11.699860	857.043108	10.905203
11.741681	859.135927	10.910208
11.292648	851.008414	10.915213
11.745885	856.985516	10.920218
11.926247	880.140422	10.925223
12.023484	866.025085	10.930227
11.923852	875.975633	10.935232
11.667926	874.946247	10.940237
12.052237	884.609748	10.945242
12.063493	879.194459	10.950247
12.089067	870.345699	10.955251
12.023343	886.103672	10.960256
11.879421	876.667397	10.965261
12.211261	874.212509	10.970266
12.026477	885.202390	10.975271
12.009805	884.301717	10.980275
12.416866	884.001805	10.985280
12.166118	883.294817	10.990285
12.368981	891.418395	10.995290
12.586952	909.168522	11.000295
12.577438	908.634511	11.005299
12.709035	912.935480	11.010304
12.343610	914.913002	11.015309
12.825946	909.321802	11.020314
12.666578	913.516740	11.025319
12.440370	919.834572	11.030323
12.313107	922.797963	11.035328
12.141207	915.707630	11.040333
12.167663	915.934025	11.045338
12.764721	930.171966	11.050343
12.970319	930.149358	11.055347
12.878406	939.455601	11.060352
13.149086	942.214977	11.065357
13.104609	946.923512	11.070362
13.104905	945.620848	11.075367
13.371175	937.602750	11.080371
13.493961	940.837875	11.085376
13.355844	944.868126	11.090381
13.507502	938.957825	11.095386
13.294258	950.138946	11.100391
13.505211	941.682701	11.105395
13.814187	949.047987	11.110400
13.474601	950.155035	11.115405
13.829198	947.180710	11.120410
13.461426	946.145233	11.125415
13.942631	949.639826	11.130419
14.014268	939.233794	11.135424
14.116420	947.786378	11.140429
13.949039	944.738526	11.145434
13.695455	939.515072	11.150439
14.056526	937.945684	11.155443
13.687950	937.165738	11.160448
13.940015	946.187219	11.165453
14.022079	940.324771	11.170458
13.513566	950.070342	11.175463
14.357042	937.737114	11.180467
14.141570	938.198016	11.185472
14.451273	940.779386	11.190477
14.589918	938.248272	11.195482
14.057721	946.713436	11.200487
14.484442	948.189223	11.205491
14.074118	953.479563	11.210496
14.206230	948.993261	11.215501
14.345776	953.264457	11.220506
14.421454	951.953210	11.225511
14.677563	940.272923	11.230515
14.454661	943.021008	11.235520
14.401304	939.558871	11.240525
14.776076	949.747862	11.245530
14.419463	954.226497	11.250535
14.583464	939.225308	11.255539
14.388673	946.792626	11.260544
14.525724	951.961877	11.265549
15.080250	963.060314	11.270554
15.002355	979.959281	11.275559
15.055917	973.073421	11.280563
14.882108	977.201378	11.285568
15.413158	978.221124	11.290573
15.303414	975.138910	11.295578
14.996636	970.100223	11.300583
15.489901	961.736483	11.305587
15.125162	961.864953	11.310592
15.071609	954.215892	11.315597
15.365125	958.899636	11.320602
15.502082	982.473055	11.325607
15.525707	978.980737	11.330611
15.956254	976.907198	11.335616
15.545344	963.218372	11.340621
15.593373	954.625844	11.345626
15.417557	959.551506	11.350631
15.410226	947.379937	11.355635
15.802012	963.189412	11.360640
15.444953	968.500230	11.365645
16.021369	974.788626	11.370650
16.042326	982.706204	11.375655
16.061092	983.052340	11.380659
15.761226	961.452131	11.385664
15.834742	960.054413	11.390669
15.947453	975.353990	11.395674
15.827777	978.832010	11.400679
15.818460	980.561378	11.405683
15.479021	982.080111	11.410688
15.768326	982.094072	11.415693
16.203182	977.017040	11.420698
16.414319	986.066088	11.425703
16.413442	983.339022	11.430707
16.135948	981.660828	11.435712
16.165886	979.175582	11.440717
16.270828	975.492087	11.445722
16.242444	982.886811	11.450727
16.420987	991.185532	11.455731
16.457320	1002.876924	11.460736
16.419472	1016.600911	11.465741
16.651459	1011.359309	11.470746
16.684706	1020.198483	11.475751
16.771031	1015.732644	11.480755
16.617258	1010.482184	11.485760
16.465301	1011.772591	11.490765
17.045692	1013.484932	11.495770
16.620607	1013.739407	11.500775
17.005619	1012.746564	11.505779
16.910263	1018.937790	11.510784
16.673116	1017.155569	11.515789
16.753881	1019.511732	11.520794
16.839146	1022.257519	11.525799
17.167462	1030.922555	11.530803
17.463789	1044.168479	11.535808
17.437636	1030.882177	11.540813
17.539437	1017.702631	11.545818
17.120637	1024.612868	11.550823
17.023529	1018.882558	11.555827
17.362132	1036.628726	11.560832
17.323448	1053.542365	11.565837
17.645629	1044.914230	11.570842
17.744644	1049.893061	11.575847
17.447302	1050.414187	11.580851
17.528331	1042.438059	11.585856
17.670148	1058.650886	11.590861
17.606911	1036.039342	11.595866
17.690109	1054.571427	11.600871
17.957852	1049.297630	11.605875
18.205652	1046.690546	11.610880
17.852789	1061.012926	11.615885
17.891481	1042.701538	11.620890
17.690096	1063.138087	11.625895
17.929214	1055.263532	11.630899
17.828860	1051.087454	11.635904
17.681329	1049.993286	11.640909
18.283463	1046.799659	11.645914
18.071180	1055.715688	11.650919
17.962513	1048.756557	11.655923
18.055378	1060.971985	11.660928
18.159989	1068.044341	11.665933
18.272285	1065.715488	11.670938
17.889837	1073.605569	11.675943
18.632990	1065.143666	11.680947
18.756302	1070.631892	11.685952
19.075778	1073.794637	11.690957
18.616291	1060.172869	11.695962
18.728898	1071.308076	11.700967
18.929325	1059.428431	11.705971
18.769002	1062.819097	11.710976
18.841176	1070.024121	11.715981
18.785562	1068.378138	11.720986
19.012781	1066.681293	11.725991
19.012644	1074.203850	11.730995
18.976543	1063.175153	11.736000
19.177601	1065.237540	11.741005
19.696569	1063.598041	11.746010
19.138267	1068.024842	11.751015
18.964672	1051.477609	11.756019
19.019072	1066.871352	11.761024
19.189951	1062.919557	11.766029
19.488944	1067.646606	11.771034
19.331050	1071.520016	11.776039
19.596997	1070.413374	11.781043
19.459967	1065.581605	11.786048
19.411045	1074.619241	11.791053
19.752356	1057.196216	11.796058
19.646274	1062.337322	11.801063
19.857051	1063.288434	11.806067
19.662595	1053.359793	11.811072
19.009484	1050.224675	11.816077
19.358218	1056.473195	11.821082
19.347347	1064.241140	11.826087
19.589100	1063.270489	11.831091
19.552556	1059.481364	11.836096
19.125005	1069.389970	11.841101
19.441715	1072.741479	11.846106
19.751998	1096.883382	11.851111
20.084977	1099.614736	11.856115
20.552184	1092.790139	11.861120
20.202817	1097.963891	11.866125
20.282989	1094.333167	11.871130
20.074997	1104.432704	11.876135
20.466939	1096.636925	11.881139
20.200853	1093.842416	11.886144
20.069779	1100.007429	11.891149
20.109074	1093.436595	11.896154
20.220538	1095.734217	11.901159
20.222983	1094.700779	11.906163
20.175144	1094.087280	11.911168
20.336531	1098.272667	11.916173
20.924525	1094.091450	11.921178
20.499857	1103.632082	11.926183
20.450737	1092.465859	11.931187
20.620718	1100.608606	11.936192
20.421627	1110.997543	11.941197
20.859650	1119.560134	11.946202
20.887481	1127.636872	11.951207
20.770711	1120.618309	11.956211
21.160049	1130.865711	11.961216
20.973803	1126.917104	11.966221
21.423700	1124.860755	11.971226
21.231666	1132.884403	11.976231
21.599071	1115.334864	11.981235
21.352361	1097.435900	11.986240
21.351375	1102.081366	11.991245
21.437162	1092.186362	11.996250
21.627561	1097.427042	12.001255
21.492972	1094.499064	12.006259
21.934477	1097.951551	12.011264
21.391814	1105.581353	12.016269
21.413614	1096.044687	12.021274
21.310164	1103.764578	12.026279
21.246155	1102.502927	12.031283
21.335439	1099.001693	12.036288
21.143659	1096.070100	12.041293
21.763166	1099.087856	12.046298
21.478256	1103.988846	12.051303
21.586861	1103.890500	12.056307
21.510021	1099.964589	12.061312
21.282651	1105.783745	12.066317
21.387816	1102.408867	12.071322
21.336000	1106.060019	12.076327
21.113647	1092.425196	12.081331
21.533680	1098.935062	12.086336
21.363872	1095.709174	12.091341
21.589382	1109.741774	12.096346
21.845625	1111.649047	12.101351
21.741285	1101.174000	12.106355
21.290886	1105.808101	12.111360
20.678014	1114.417845	12.116365
21.221485	1114.105200	12.121370
21.019051	1112.417675	12.126375
21.252165	1110.925078	12.131379
21.361716	1126.372978	12.136384
21.306851	1135.445221	12.141389
21.539366	1136.941298	12.146394
21.303251	1133.746114	12.151399
21.481174	1135.623001	12.156403
21.485492	1135.435956	12.161408
21.488359	1144.493964	12.166413
21.605085	1138.660630	12.171418
21.793151	1139.587615	12.176423
21.116188	1126.285710	12.181427
21.601512	1123.412098	12.186432
21.366237	1133.680148	12.191437
21.548709	1131.869783	12.196442
21.453402	1118.922107	12.201447
21.346027	1112.884442	12.206451
21.170312	1124.696756	12.211456
21.243020	1139.903484	12.216461
21.511981	1135.355770	12.221466
21.482850	1136.350784	12.226471
21.799309	1134.001916	12.231475
21.894863	1132.055269	12.236480
21.373374	1126.505446	12.241485
21.560591	1110.616686	12.246490
21.549231	1111.277465	12.251495
21.283985	1112.172828	12.256499
21.341875	1101.937994	12.261504
21.291439	1115.670936	12.266509
21.764590	1105.932929	12.271514
21.430335	1122.646267	12.276519
21.087895	1115.399949	12.281523
21.264428	1115.379957	12.286528
21.150227	1138.747989	12.291533
21.705416	1147.593272	12.296538
21.581788	1142.474179	12.301543
21.627696	1136.617462	12.306547
21.541181	1126.847110	12.311552
20.924744	1128.844011	12.316557
21.725297	1137.070110	12.321562
21.751079	1141.843631	12.326567
22.008165	1125.495636	12.331571
21.923428	1103.579658	12.336576
21.998793	1118.285381	12.341581
21.878724	1117.866240	12.346586
22.055541	1108.445884	12.351591
22.265401	1103.904759	12.356595
21.885831	1086.115825	12.361600
21.409519	1091.567131	12.366605
21.743193	1075.950138	12.371610
21.671834	1081.018981	12.376615
21.675928	1080.208683	12.381619
21.263724	1074.226061	12.386624
21.104963	1083.736089	12.391629
21.043417	1072.654511	12.396634
20.825643	1076.270952	12.401639
20.981830	1081.928020	12.406643
21.574211	1081.995018	12.411648
20.667906	1086.687150	12.416653
21.483068	1104.652477	12.421658
21.381374	1115.477878	12.426663
21.359200	1114.423397	12.431667
21.699591	1116.178873	12.436672
21.376413	1117.870885	12.441677
21.803696	1108.912060	12.446682
21.651260	1117.488651	12.451687
21.941933	1109.357333	12.456691
21.696182	1097.054420	12.461696
21.190440	1093.435339	12.466701
21.418499	1079.898565	12.471706
21.629191	1082.104566	12.476711
21.662698	1083.022521	12.481715
21.663658	1091.125558	12.486720
21.183131	1102.163140	12.491725
21.243341	1082.645246	12.496730
21.211240	1088.141178	12.501735
21.342565	1087.098275	12.506739
21.667580	1081.396224	12.511744
21.339467	1086.400143	12.516749
21.267785	1088.274822	12.521754
21.452428	1088.140149	12.526759
21.269181	1092.461992	12.531763
21.647589	1086.273941	12.536768
21.503340	1093.177793	12.541773
21.749094	1090.793685	12.546778
21.443854	1094.620128	12.551783
21.557362	1085.974064	12.556787
21.743161	1084.568925	12.561792
21.592390	1089.340333	12.566797
21.184665	1086.983400	12.571802
21.641664	1096.111148	12.576807
21.425186	1097.761574	12.581811
21.513399	1091.558144	12.586816
21.558624	1095.706210	12.591821
21.544710	1086.621728	12.596826
21.230542	1086.034946	12.601831
21.436105	1101.297805	12.606835
21.626044	1098.905503	12.611840
21.481328	1090.017131	12.616845
21.747711	1095.303598	12.621850
21.796681	1098.101411	12.626855
21.519099	1103.752332	12.631859
21.715281	1096.707754	12.636864
21.374104	1097.798504	12.641869
21.492904	1089.461796	12.646874
21.578615	1099.544525	12.651879
21.546832	1098.151427	12.656883
21.628865	1102.434105	12.661888
21.390721	1101.190074	12.666893
21.612205	1095.694455	12.671898
21.373115	1083.390410	12.676903
21.475873	1095.675617	12.681907
21.610205	1088.795989	12.686912
21.259071	1074.057863	12.691917
21.306713	1076.465504	12.696922
21.674499	1087.171706	12.701927
21.610549	1083.578722	12.706931
21.669069	1078.154471	12.711936
21.054687	1085.366690	12.716941
21.273508	1077.176655	12.721946
21.508082	1083.723050	12.726951
21.444158	1094.826567	12.731955
21.826399	1089.559572	12.736960
21.411179	1088.786431	12.741965
21.707313	1074.783646	12.746970
21.413119	1079.173061	12.751975
21.176347	1085.943167	12.756979
21.169841	1069.158450	12.761984
21.343772	1085.093430	12.766989
21.543186	1091.090459	12.771994
21.824328	1100.445731	12.776999
21.665564	1097.304397	12.782003
21.838765	1089.518100	12.787008
21.471532	1094.687809	12.792013
21.438504	1073.875380	12.797018
21.390980	1081.114354	12.802023
21.517089	1085.571444	12.807027
21.770224	1079.535138	12.812032
21.488396	1083.128616	12.817037
21.543349	1078.303005	12.822042
21.524238	1075.170099	12.827047
21.738994	1084.032663	12.832051
21.591076	1079.997759	12.837056
21.549016	1092.092266	12.842061
21.523636	1088.686484	12.847066
21.386590	1089.162758	12.852071
21.299915	1087.963021	12.857075
21.571162	1072.584105	12.862080
21.132345	1080.653591	12.867085
21.592989	1077.530402	12.872090
21.405446	1081.792979	12.877095
21.046226	1082.991823	12.882099
21.438288	1078.540651	12.887104
21.336812	1089.676656	12.892109
21.659314	1089.064397	12.897114
21.460218	1090.006444	12.902119
21.616637	1088.265288	12.907123
21.909634	1093.753639	12.912128
21.466140	1097.694972	12.917133
21.551429	1097.044832	12.922138
21.404583	1094.909222	12.927143
21.354254	1096.947215	12.932147
21.741474	1091.983314	12.937152
21.760776	1102.251906	12.942157
21.522360	1079.634807	12.947162
21.286104	1072.808857	12.952167
21.061118	1082.704846	12.957171
21.647864	1086.344797	12.962176
21.213677	1094.127311	12.967181
21.138268	1095.721575	12.972186
21.366130	1088.730779	12.977191
21.639800	1089.542820	12.982195
21.508506	1089.152052	12.987200
21.303644	1100.113158	12.992205
21.640892	1098.462971	12.997210
21.899378	1099.214063	13.002215
21.986809	1095.798805	13.007219
21.936360	1077.355817	13.012224
21.313132	1073.460436	13.017229
21.547782	1067.558357	13.022234
21.645847	1062.286016	13.027239
21.217976	1067.706903	13.032243
21.382427	1064.527921	13.037248
21.078347	1061.150588	13.042253
21.099795	1056.953230	13.047258
21.092361	1067.844937	13.052263
21.123196	1085.465903	13.057267
21.467529	1091.340190	13.062272
21.394603	1096.860888	13.067277
21.488709	1089.578813	13.072282
21.433548	1090.769340	13.077287
21.634222	1092.455611	13.082291
21.402287	1089.813931	13.087296
21.184444	1097.056851	13.092301
21.427315	1104.807759	13.097306
21.729934	1094.755180	13.102311
21.165185	1101.570474	13.107315
21.483497	1090.166385	13.112320
21.392625	1101.092947	13.117325
21.397704	1095.748511	13.122330
21.265274	1098.520979	13.127335
21.348128	1098.515469	13.132339
21.609084	1095.043618	13.137344
21.734420	1109.643265	13.142349
21.474303	1102.766524	13.147354
21.772873	1100.772441	13.152359
21.324863	1105.790607	13.157363
21.541474	1098.066337	13.162368
21.796261	1103.140847	13.167373
21.429827	1098.931035	13.172378
21.748408	1102.656442	13.177383
21.448680	1092.044375	13.182387
21.348762	1070.545522	13.187392
20.962345	1086.200392	13.192397
21.206091	1088.461122	13.197402
21.716795	1090.223315	13.202407
21.378885	1100.139860	13.207411
22.015004	1105.061751	13.212416
21.348728	1095.429112	13.217421
21.373808	1088.932560	13.222426
21.761643	1091.527402	13.227431
21.163438	1079.194143	13.232435
21.431760	1084.744749	13.237440
21.348174	1102.573249	13.242445
21.222564	1105.423496	13.247450
21.790294	1103.277078	13.252455
21.577405	1099.009360	13.257459
21.520233	1090.751375	13.262464
21.000009	1079.283039	13.267469
21.192342	1095.688560	13.272474
21.355823	1105.031640	13.277479
21.389673	1104.468872	13.282483
21.444126	1103.925466	13.287488
20.824097	1118.732655	13.292493
21.234551	1115.247010	13.297498
21.658562	1109.644029	13.302503
21.283669	1112.482544	13.307507
21.463085	1102.007793	13.312512
21.605201	1115.369825	13.317517
21.563153	1109.026090	13.322522
21.617601	1110.251905	13.327527
21.365168	1111.917576	13.332531
21.828199	1113.668998	13.337536
21.645766	1115.795170	13.342541
21.394678	1107.894900	13.347546
21.617211	1117.307994	13.352551
21.114795	1111.532668	13.357555
21.446235	1108.910839	13.362560
21.429828	1115.295015	13.367565
21.540638	1111.217321	13.372570
21.547463	1107.070615	13.377575
21.723138	1108.350250	13.382579
21.920399	1101.271931	13.387584
21.604311	1101.671140	13.392589
21.680967	1087.990581	13.397594
21.536716	1081.442538	13.402599
21.478945	1082.742855	13.407603
21.340298	1074.911744	13.412608
21.650413	1082.815717	13.417613
21.533877	1075.441079	13.422618
21.824535	1076.304286	13.427623
21.359016	1085.265329	13.432627
21.772769	1079.505828	13.437632
21.105457	1087.623574	13.442637
21.432220	1081.835960	13.447642
21.630430	1083.090019	13.452647
21.224019	1089.473158	13.457651
21.468993	1073.855586	13.462656
21.186833	1078.915177	13.467661
21.113501	1080.085924	13.472666
21.369376	1074.220467	13.477671
21.366662	1082.604393	13.482675
21.355957	1082.432556	13.487680
21.632935	1081.596786	13.492685
21.342915	1082.226000	13.497690
21.520015	1074.457990	13.502695
21.585671	1079.205708	13.507699
21.611993	1076.754225	13.512704
21.294521	1081.333948	13.517709
21.580067	1078.088017	13.522714
21.480543	1075.213637	13.527719
21.305571	1078.849976	13.532723
21.491127	1075.571058	13.537728
21.682688	1079.370344	13.542733
21.717793	1085.075805	13.547738
21.741400	1080.971623	13.552743
21.436262	1085.765549	13.557747
22.006494	1076.144337	13.562752
21.737369	1082.435645	13.567757
22.137560	1078.325317	13.572762
22.044734	1063.058570	13.577767
21.833803	1059.186844	13.582771
21.639809	1054.482477	13.587776
20.984388	1056.278026	13.592781
20.700625	1055.437742	13.597786
21.358307	1053.312618	13.602791
20.957538	1058.518065	13.607795
21.673335	1066.214710	13.612800
21.654751	1077.980706	13.617805
21.660722	1072.404019	13.622810
22.153737	1063.327371	13.627815
21.645827	1057.705376	13.632819
21.867280	1054.498860	13.637824
21.669667	1058.801447	13.642829
21.476222	1051.021980	13.647834
21.579582	1049.420584	13.652839
21.363209	1049.630985	13.657843
21.073970	1043.951765	13.662848
21.197762	1049.035691	13.667853
20.902256	1057.977832	13.672858
21.283853	1050.800825	13.677863
20.844759	1056.088237	13.682867
21.116892	1062.912000	13.687872
21.226816	1078.115050	13.692877
21.299935	1087.414007	13.697882
21.616172	1082.997150	13.702887
21.503111	1083.653655	13.707891
22.059037	1077.128459	13.712896
21.756065	1076.075546	13.717901
21.257961	1068.893440	13.722906
21.124585	1065.570916	13.727911
21.328420	1088.416581	13.732915
21.341043	1083.334935	13.737920
21.277337	1087.700624	13.742925
21.490780	1092.304980	13.747930
21.596046	1091.019043	13.752935
21.439688	1095.125882	13.757939
21.698058	1089.967362	13.762944
21.285047	1092.254645	13.767949
21.284134	1099.190765	13.772954
21.934510	1090.839888	13.777959
21.765135	1094.646983	13.782963
21.719364	1072.798578	13.787968
21.658509	1065.796899	13.792973
21.624632	1062.771923	13.797978
21.258488	1057.801017	13.802983
21.746861	1065.366523	13.807987
21.604773	1055.379164	13.812992
21.886174	1056.171325	13.817997
21.604053	1068.700132	13.823002
21.421307	1054.481445	13.828007
21.501375	1066.066307	13.833011
21.286645	1062.344837	13.838016
21.672412	1060.224098	13.843021
21.183857	1064.523675	13.848026
21.539018	1059.758703	13.853031
21.471033	1064.841962	13.858035
21.598856	1060.133336	13.863040
21.496238	1060.185285	13.868045
21.573683	1057.003065	13.873050
21.730006	1054.605481	13.878055
21.183259	1063.459255	13.883059
21.437669	1059.974323	13.888064
21.400261	1067.102608	13.893069
21.453832	1066.453960	13.898074
21.451285	1053.762013	13.903079
21.342237	1068.680887	13.908083
21.646634	1060.740268	13.913088
21.022134	1052.847997	13.918093
21.397029	1069.281399	13.923098
21.508152	1062.805237	13.928103
21.031230	1058.770300	13.933107
21.080939	1059.488502	13.938112
21.260701	1068.030213	13.943117
21.165172	1071.437404	13.948122
21.303192	1064.895839	13.953127
21.230976	1066.938370	13.958131
21.459737	1066.594422	13.963136
21.564982	1070.626400	13.968141
21.363527	1074.183200	13.973146
21.612326	1059.817885	13.978151
21.643526	1070.157837	13.983155
21.513057	1069.959165	13.988160
21.706838	1076.323077	13.993165
21.565596	1072.743348	13.998170
21.675239	1071.073766	14.003175
21.476065	1082.067438	14.008179
21.560467	1066.741484	14.013184
21.320329	1076.208223	14.018189
21.755615	1081.602784	14.023207
21.629999	1080.147448	14.028224
21.152035	1080.664090	14.033242
21.068810	1065.309868	14.038259
21.265345	1078.557911	14.043277
21.155303	1075.237163	14.048295
21.422845	1068.136431	14.053312
21.726779	1099.525353	14.058330
21.565234	1090.835451	14.063347
21.955131	1087.204162	14.068365
21.437886	1077.413354	14.073383
21.517409	1071.591017	14.078400
21.434672	1079.143985	14.083418
21.459892	1097.280061	14.088435
21.507678	1100.878068	14.093453
21.721608	1115.093315	14.098471
21.706256	1100.753881	14.103488
21.561993	1123.398926	14.108506
21.593326	1115.656728	14.113523
21.850925	1115.793296	14.118541
21.580013	1113.834087	14.123559
21.631066	1103.215451	14.128576
21.828823	1110.139980	14.133594
22.239498	1104.425433	14.138611
21.897720	1101.991329	14.143629
21.661981	1106.015539	14.148647
22.039662	1104.597539	14.153664
21.588471	1122.704296	14.158682
21.872271	1104.393174	14.163699
22.079165	1107.220144	14.168717
21.742338	1113.900479	14.173735
21.853553	1107.352953	14.178752
21.743893	1105.688563	14.183770
21.729640	1110.615424	14.188787
21.897490	1124.188135	14.193805
21.951575	1142.368137	14.198823
22.058179	1140.090633	14.203840
21.918993	1147.532829	14.208858
21.921653	1147.924543	14.213875
22.465311	1142.198600	14.218893
22.438623	1143.757645	14.223911
22.986894	1136.956809	14.228928
22.479572	1130.820468	14.233946
22.614488	1116.324535	14.238963
22.679682	1106.327932	14.243981
21.612890	1105.860014	14.248999
21.969903	1114.027024	14.254016
21.962140	1114.392964	14.259034
22.178414	1131.288745	14.264051
22.460769	1138.495263	14.269069
22.051402	1147.233885	14.274087
22.077779	1146.841941	14.279104
22.392444	1146.794302	14.284122
22.346990	1149.305462	14.289139
22.246718	1144.281310	14.294157
22.364191	1156.373195	14.299175
22.276028	1144.185750	14.304192
22.174318	1153.482700	14.309210
22.286794	1147.262526	14.314227
22.479840	1143.271243	14.319245
22.437666	1150.719251	14.324263
22.007263	1142.279372	14.329280
22.344248	1157.146448	14.334298
22.472208	1163.894764	14.339315
22.838944	1174.906832	14.344333
22.346143	1178.725508	14.349351
22.781553	1174.201676	14.354368
22.975391	1176.041444	14.359386
22.742610	1168.073222	14.364403
22.469273	1161.478999	14.369421
22.383433	1179.644449	14.374439
22.510449	1172.963073	14.379456
22.742372	1183.883292	14.384474
22.693336	1180.318577	14.389491
22.444824	1173.176740	14.394509
22.073923	1182.113134	14.399527
22.518778	1167.112401	14.404544
22.657870	1180.481019	14.409562
22.452608	1185.301272	14.414579
23.307980	1198.437243	14.419597
23.118714	1198.353948	14.424615
23.042579	1190.629745	14.429632
22.835387	1182.395689	14.434650
23.238494	1193.904332	14.439667
23.185305	1174.581526	14.444685
22.907590	1174.299599	14.449703
23.081540	1170.163146	14.454720
22.921515	1172.430545	14.459738
22.875779	1168.657376	14.464755
23.212229	1171.714528	14.469773
23.266661	1177.386783	14.474791
23.100286	1164.029170	14.479808
23.088158	1171.648035	14.484826
23.146813	1170.920607	14.489843
23.213326	1179.539069	14.494861
23.201097	1189.547924	14.499879
23.169236	1198.784495	14.504896
23.578095	1187.358721	14.509914
23.404949	1188.095173	14.514931
23.785362	1167.363274	14.519949
23.312308	1169.857586	14.524967
23.715006	1166.968241	14.529984
23.505105	1172.264521	14.535002
24.001170	1168.196078	14.540019
23.716555	1163.188172	14.545037
23.870383	1169.249321	14.550055
23.751148	1155.726532	14.555072
23.332342	1141.855086	14.560090
23.369879	1145.644641	14.565107
23.465131	1130.051075	14.570125
23.356215	1140.359964	14.575143
23.306242	1153.071942	14.580160
23.489742	1157.794820	14.585178
23.248247	1159.993108	14.590195
23.578100	1163.459297	14.595213
23.181077	1165.795285	14.600231
23.212958	1163.293955	14.605248
23.514766	1165.155371	14.610266
22.780992	1164.839031	14.615283
23.065396	1160.154071	14.620301
23.084067	1181.663299	14.625319
23.444631	1193.082378	14.630336
23.615922	1203.362164	14.635354
23.843344	1205.607236	14.640371
23.457777	1202.726648	14.645389
23.309390	1206.532739	14.650407
23.741695	1196.491641	14.655424
23.966716	1194.545824	14.660442
23.359510	1200.099226	14.665459
24.011689	1214.817819	14.670477
24.176691	1218.488678	14.675495
23.839841	1215.450509	14.680512
24.227332	1197.098271	14.685530
23.814158	1201.534849	14.690547
23.889736	1194.021661	14.695565
23.872905	1194.704537	14.700583
24.061767	1192.902334	14.705600
24.512360	1199.573299	14.710618
24.238866	1204.077275	14.715635
24.023030	1202.067269	14.720653
23.971037	1198.187282	14.725671
23.976650	1202.893032	14.730688
24.281670	1199.409746	14.735706
24.209129	1199.181230	14.740723
24.105831	1194.266646	14.745741
24.004383	1205.402713	14.750759
24.161769	1201.919147	14.755776
24.264910	1196.583307	14.760794
23.845177	1204.885118	14.765811
24.252308	1216.850608	14.770829
24.046274	1229.548458	14.775847
24.383398	1233.026409	14.780864
24.415640	1231.896385	14.785882
24.353139	1228.759596	14.790899
24.096257	1229.024538	14.795917
24.588756	1227.645114	14.800935
24.160177	1229.535695	14.805952
24.729112	1228.982215	14.810970
24.406152	1233.337581	14.815987
24.161442	1228.900420	14.821005
24.374977	1231.577442	14.826023
24.352020	1229.239455	14.831040
24.686397	1224.897513	14.836058
24.308476	1232.319653	14.841075
24.423390	1225.602531	14.846093
24.558501	1232.860718	14.851111
24.459413	1227.958395	14.856128
24.646641	1231.667969	14.861146
24.579088	1231.550812	14.866163
24.595763	1222.052261	14.871181
24.741970	1230.075146	14.876199
24.476349	1229.040292	14.881216
25.051403	1236.472284	14.886234
24.759311	1241.671253	14.891251
25.165977	1220.952500	14.896269
25.296333	1230.464452	14.901287
24.867061	1229.567509	14.906304
24.714228	1230.681221	14.911322
24.309323	1232.972504	14.916339
24.398267	1225.338888	14.921357
24.439717	1239.337737	14.926375
24.726349	1255.248670	14.931392
25.163388	1249.863437	14.936410
25.103128	1260.907042	14.941427
25.265659	1255.701562	14.946445
25.128026	1253.754919	14.951463
25.175477	1254.666562	14.956480
25.287752	1255.464326	14.961498
24.958838	1240.718641	14.966515
25.019714	1244.456970	14.971533
25.314598	1252.340980	14.976551
25.030173	1260.461733	14.981568
25.402958	1252.411689	14.986586
25.023782	1250.389127	14.991603
25.600380	1247.496331	14.996621
25.360546	1231.514803	15.001639
24.778202	1231.825703	15.006656
25.397806	1242.701148	15.011674
25.388546	1257.318604	15.016691
25.415159	1248.580998	15.021709
25.422018	1235.899195	15.026727
24.778873	1243.811342	15.031744
25.262166	1241.204254	15.036762
25.225750	1250.311309	15.041779
25.474938	1245.944988	15.046797
25.433695	1252.938908	15.051815
24.780356	1250.731049	15.056832
25.735885	1248.103627	15.061850
25.270084	1252.861081	15.066867
25.314372	1255.050151	15.071885
25.746810	1255.042167	15.076903
25.631678	1261.504223	15.081920
25.537866	1244.452276	15.086938
25.191659	1256.546173	15.091955
25.390630	1255.725781	15.096973
25.713070	1264.360651	15.101991
25.664401	1273.178850	15.107008
25.807893	1274.931978	15.112026
25.956095	1288.721212	15.117043
25.742016	1269.666053	15.122061
25.826571	1259.577048	15.127079
25.390339	1261.874493	15.132096
25.920608	1256.800075	15.137114
25.387114	1272.249619	15.142131
25.924705	1282.124102	15.147149
25.758308	1274.068846	15.152167
25.648616	1281.556447	15.157184
25.996595	1275.621858	15.162202
25.952033	1280.455142	15.167219
26.052568	1283.543315	15.172237
26.248233	1281.182404	15.177255
25.660060	1278.977148	15.182272
26.082149	1273.399178	15.187290
26.160944	1272.357242	15.192307
25.792216	1277.508333	15.197325
25.572372	1280.610488	15.202343
26.297239	1288.904695	15.207360
26.323719	1282.605109	15.212378
25.993052	1284.094229	15.217395
26.020885	1284.371778	15.222413
26.034888	1281.796716	15.227431
25.813241	1281.238614	15.232448
26.230463	1274.568073	15.237466
26.364381	1283.317961	15.242483
26.477688	1283.511164	15.247501
26.488084	1285.282782	15.252519
25.968428	1289.830170	15.257536
26.289826	1286.782679	15.262554
25.995224	1302.013324	15.267571
26.401517	1315.576818	15.272589
26.657181	1315.300691	15.277607
26.109647	1319.744589	15.282624
26.728745	1312.380696	15.287642
26.693984	1319.619226	15.292659
26.716434	1321.982538	15.297677
26.970413	1309.400838	15.302695
26.500566	1299.193851	15.307712
26.538972	1298.630929	15.312730
26.855006	1306.747582	15.317747
26.656193	1300.512210	15.322765
26.721716	1284.906263	15.327783
26.488091	1290.992155	15.332800
26.596224	1293.432905	15.337818
26.680860	1308.626096	15.342835
26.580785	1316.400674	15.347853
26.968669	1300.019297	15.352871
26.997868	1311.329908	15.357888
26.967839	1318.908209	15.362906
26.724635	1318.255367	15.367923
26.640100	1322.137554	15.372941
26.890662	1313.935584	15.377959
26.682083	1315.624266	15.382976
27.065590	1312.904736	15.387994
27.042115	1307.996510	15.393011
26.666184	1315.591199	15.398029
26.902681	1309.205983	15.403047
26.786107	1323.283974	15.408064
26.792043	1313.279287	15.413082
26.899857	1312.529251	15.418099
27.004013	1322.433976	15.423117
27.158943	1313.248704	15.428135
26.964930	1318.434425	15.433152
26.963405	1316.857387	15.438170
26.884557	1322.029664	15.443187
27.289802	1334.627516	15.448205
27.576623	1332.363971	15.453223
27.354854	1332.628013	15.458240
27.211579	1322.290995	15.463258
27.453657	1313.043532	15.468275
27.414130	1316.797518	15.473293
27.320397	1311.128037	15.478311
27.358746	1324.553032	15.483328
27.725969	1310.717154	15.488346
27.863518	1307.097189	15.493363
27.815170	1314.948339	15.498381
28.109264	1308.697750	15.503399
27.687092	1315.727086	15.508416
27.534318	1309.558233	15.513434
27.900582	1312.833550	15.518451
27.560739	1310.005343	15.523469
27.419480	1305.403560	15.528487
26.816991	1313.218211	15.533504
27.316359	1316.302188	15.538522
27.208255	1312.435731	15.543539
27.161670	1322.888791	15.548557
27.704569	1316.262044	15.553575
28.105962	1334.219321	15.558592
27.787756	1325.769948	15.563610
27.795806	1327.582135	15.568627
27.747061	1328.047634	15.573645
27.733685	1326.531294	15.578663
27.908918	1345.065205	15.583680
27.840814	1341.947466	15.588698
27.977351	1338.581234	15.593715
27.891514	1348.271284	15.598733
27.961031	1339.716446	15.603751
28.192370	1344.185092	15.608768
27.868240	1334.485826	15.613786
28.497907	1333.008459	15.618803
27.879543	1326.522933	15.623821
28.161378	1318.873524	15.628839
28.167962	1337.287115	15.633856
28.194799	1329.167988	15.638874
28.670701	1322.434998	15.643891
28.372263	1321.421907	15.648909
28.497333	1306.350268	15.653927
28.197789	1308.132112	15.658944
28.106530	1305.264042	15.663962
28.367353	1296.217330	15.668979
27.906735	1302.218512	15.673997
28.281958	1301.509250	15.679015
28.157028	1307.475715	15.684032
28.448701	1304.573882	15.689050
28.408533	1299.393692	15.694067
28.174847	1303.649511	15.699085
28.415106	1314.895194	15.704103
28.542538	1328.041902	15.709120
28.492705	1335.747240	15.714138
28.656747	1324.103082	15.719155
28.413448	1333.177541	15.724173
28.716806	1326.152843	15.729191
28.600101	1331.640698	15.734208
28.345335	1335.080771	15.739226
28.804295	1332.128989	15.744243
28.789942	1339.124243	15.749261
28.619303	1330.460573	15.754279
28.956024	1340.154947	15.759296
28.645191	1334.113981	15.764314
28.485290	1322.123360	15.769331
28.447417	1329.123823	15.774349
28.851033	1334.929198	15.779367
28.938103	1336.210072	15.784384
28.933768	1328.666422	15.789402
28.939952	1329.310710	15.794419
28.953788	1337.854818	15.799437
28.765969	1334.289452	15.804455
29.138110	1332.659764	15.809472
29.112957	1333.489756	15.814490
29.089905	1327.141160	15.819507
29.110865	1336.716032	15.824525
29.153311	1330.990909	15.829543
29.045876	1333.777710	15.834560
29.050418	1342.502959	15.839578
29.281181	1338.099217	15.844595
28.952865	1334.098447	15.849613
29.278102	1330.676240	15.854631
29.261892	1332.495736	15.859648
28.935150	1339.053560	15.864666
28.866413	1335.934355	15.869683
28.822741	1334.624803	15.874701
29.017908	1335.899349	15.879719
29.115496	1324.601262	15.884736
28.996814	1339.315121	15.889754
29.693160	1352.657641	15.894771
29.169329	1369.267151	15.899789
29.488437	1355.958037	15.904807
29.988532	1350.921836	15.909824
29.699460	1352.651097	15.914842
29.613013	1334.980801	15.919859
29.388081	1332.842797	15.924877
29.394706	1330.262693	15.929895
29.857952	1344.787011	15.934912
29.546087	1348.934975	15.939930
29.686048	1345.337424	15.944947
30.081403	1354.715033	15.949965
29.450984	1334.050310	15.954983
29.698033	1333.733135	15.960000
29.701174	1354.008535	15.965018
30.078516	1351.372346	15.970035
29.718245	1345.614287	15.975053
29.599091	1331.323543	15.980071
29.563822	1347.320474	15.985088
29.605854	1356.444853	15.990106
29.846745	1349.958858	15.995123
29.631221	1354.656107	16.000141
30.130829	1361.863673	16.005159
30.193004	1368.270173	16.010176
29.795507	1361.712902	16.015194
30.247521	1360.662093	16.020211
30.064862	1360.941872	16.025229
30.031621	1360.923959	16.030247
30.157058	1361.116658	16.035264
30.058090	1362.099085	16.040282
29.997481	1362.163431	16.045299
29.712757	1357.463777	16.050317
29.866090	1360.129882	16.055335
30.422855	1361.746014	16.060352
30.014804	1357.917586	16.065370
30.020622	1356.879494	16.070387
30.272783	1364.157442	16.075405
30.317315	1382.915796	16.080423
30.338039	1386.296047	16.085440
30.371347	1386.428550	16.090458
30.258594	1396.633137	16.095475
30.333641	1390.247614	16.100493
30.245300	1391.264839	16.105511
30.601057	1380.910732	16.110528
30.699326	1389.033660	16.115546
30.780064	1379.298022	16.120563
31.007638	1377.333633	16.125581
30.908486	1380.511187	16.130599
30.948909	1368.264902	16.135616
30.810782	1365.303272	16.140634
30.825760	1350.706809	16.145651
30.772021	1348.511496	16.150669
30.673930	1351.359302	16.155687
30.781276	1348.764288	16.160704
30.931887	1348.045498	16.165722
30.743329	1336.011350	16.170739
30.665812	1350.508694	16.175757
30.330019	1365.024347	16.180775
30.779184	1371.488131	16.185792
30.800790	1373.851202	16.190810
30.843791	1373.838723	16.195827
31.089736	1376.314919	16.200845
30.784647	1383.294680	16.205863
30.903723	1370.757323	16.210880
30.943015	1379.079746	16.215898
30.861774	1370.777533	16.220915
30.939401	1381.256190	16.225933
30.804558	1378.911377	16.230951
31.220316	1388.058714	16.235968
31.201604	1410.285366	16.240986
31.375424	1403.802580	16.246003
31.453125	1400.587381	16.251021
31.259265	1390.832276	16.256039
31.603193	1369.642540	16.261056
31.323512	1373.117212	16.266074
31.379557	1361.489968	16.271091
31.374620	1366.041654	16.276109
31.195278	1366.087378	16.281127
31.607294	1380.426006	16.286144
31.640238	1393.572826	16.291162
31.561662	1377.717451	16.296179
31.648792	1370.921951	16.301197
31.230277	1377.830203	16.306215
31.646797	1385.025252	16.311232
31.621560	1393.331578	16.316250
31.773383	1387.742420	16.321267
31.803310	1393.956016	16.326285
32.032875	1388.496456	16.331303
32.174276	1367.381609	16.336320
31.869467	1371.377961	16.341338
31.747083	1365.014093	16.346355
31.677291	1361.255239	16.351373
31.915646	1373.476582	16.356391
32.032750	1363.287825	16.361408
32.235078	1363.785088	16.366426
32.050603	1357.545659	16.371443
32.262823	1364.626106	16.376461
32.369885	1360.225454	16.381479
32.287957	1357.597923	16.386496
32.622846	1360.971946	16.391514
32.266992	1357.301513	16.396531
32.606379	1358.333991	16.401549
32.243374	1343.289694	16.406567
32.625523	1332.580273	16.411584
32.373772	1328.247844	16.416602
32.069928	1320.234634	16.421619
32.223059	1324.807244	16.426637
32.008086	1322.914407	16.431655
32.397650	1323.817008	16.436672
32.329711	1328.275146	16.441690
32.329269	1319.625611	16.446707
32.318585	1320.742125	16.451725
32.271856	1332.211846	16.456743
32.654298	1335.597791	16.461760
32.390806	1350.332946	16.466778
32.625612	1345.561938	16.471795
32.893750	1348.131578	16.476813
32.277964	1352.417093	16.481831
32.452686	1355.593358	16.486848
32.416729	1353.777315	16.491866
32.225183	1358.730321	16.496883
32.691799	1362.568813	16.501901
32.708157	1368.890248	16.506919
32.794358	1356.791650	16.511936
32.477000	1361.425251	16.516954
32.405915	1364.098334	16.521971
32.568127	1364.659567	16.526989
31.960602	1366.016618	16.532007
32.376129	1367.049035	16.537024
32.738815	1385.350442	16.542042
32.876704	1392.085737	16.547059
33.302837	1396.865522	16.552077
33.285408	1399.573117	16.557095
33.373533	1394.306326	16.562112
33.160290	1394.262577	16.567130
33.011187	1403.774120	16.572147
33.141461	1390.730053	16.577165
33.014037	1397.754169	16.582183
32.950950	1393.581519	16.587200
32.921610	1392.605364	16.592218
33.241958	1397.400530	16.597235
33.533652	1394.160849	16.602253
33.052797	1391.335542	16.607271
32.758705	1392.194324	16.612288
32.732295	1393.489541	16.617306
32.434015	1396.381129	16.622323
33.100125	1417.847007	16.627341
33.195471	1427.365476	16.632359
33.664569	1420.256803	16.637376
33.699844	1425.238664	16.642394
33.385379	1429.161875	16.647411
33.601591	1426.200510	16.652429
33.747317	1434.804744	16.657447
33.615313	1423.361679	16.662464
33.495463	1429.135568	16.667482
33.541373	1430.468000	16.672499
33.831451	1430.795480	16.677517
33.408508	1434.658150	16.682535
33.563652	1424.199814	16.687552
33.887610	1432.473852	16.692570
33.513252	1422.163394	16.697587
33.866366	1429.724488	16.702605
33.802791	1435.399746	16.707623
33.806839	1429.534305	16.712640
33.993541	1423.031584	16.717658
33.927902	1426.399877	16.722675
33.709366	1431.818996	16.727693
33.848336	1452.735869	16.732711
33.911750	1455.031147	16.737728
33.886247	1450.478378	16.742746
34.119933	1462.427335	16.747763
34.091077	1453.047878	16.752781
33.888398	1458.567448	16.757799
34.074580	1461.640579	16.762816
34.057527	1461.541142	16.767834
34.255297	1469.745881	16.772851
34.195733	1466.787299	16.777869
34.089754	1463.847306	16.782887
34.213231	1462.541371	16.787904
34.640445	1465.848795	16.792922
34.379972	1467.696013	16.797939
34.414409	1466.118700	16.802957
34.511290	1464.523594	16.807975
34.656510	1461.432648	16.812992
34.372688	1467.339006	16.818010
34.382006	1468.188295	16.823027
34.693514	1467.207638	16.828045
34.481898	1487.705090	16.833063
34.514464	1481.773316	16.838080
34.987223	1481.905680	16.843098
34.837272	1483.272091	16.848115
34.759881	1483.674389	16.853133
34.984121	1493.001490	16.858151
34.882694	1482.204388	16.863168
35.104735	1476.007429	16.868186
34.845736	1467.472230	16.873203
34.760559	1453.466129	16.878221
34.784388	1457.256928	16.883239
35.069759	1469.193091	16.888256
35.046324	1477.645232	16.893274
34.932970	1480.286602	16.898291
35.055258	1476.787731	16.903309
35.167190	1488.021680	16.908327
35.234196	1483.115604	16.913344
35.183322	1482.809346	16.918362
35.104380	1485.400718	16.923379
35.209416	1478.482010	16.928397
35.051702	1474.672448	16.933415
35.462724	1480.304938	16.938432
35.540657	1478.499278	16.943450
34.697562	1487.629020	16.948467
35.276147	1476.021953	16.953485
35.415798	1474.180119	16.958503
35.334196	1477.606283	16.963520
35.505080	1474.140817	16.968538
35.449941	1477.418729	16.973555
35.418774	1477.292575	16.978573
35.236778	1482.311706	16.983591
35.563772	1485.991079	16.988608
35.611132	1482.890132	16.993626
35.384933	1502.632545	16.998643
35.129507	1509.454619	17.003661
35.383078	1511.889762	17.008679
35.439284	1512.484138	17.013696
35.937137	1513.108315	17.018714
35.583453	1507.579011	17.023731
35.893328	1516.265000	17.028749
35.602183	1512.171975	17.033767
35.877895	1507.746698	17.038784
36.000750	1504.987958	17.043802
35.918508	1515.456317	17.048819
36.393701	1522.133836	17.053837
36.580415	1518.653046	17.058855
36.654115	1516.070467	17.063872
36.508639	1505.221446	17.068890
36.282545	1516.812615	17.073907
36.679975	1513.962698	17.078925
36.384773	1515.216206	17.083943
35.999182	1519.199277	17.088960
36.083116	1509.739418	17.093978
35.845434	1512.204057	17.098995
36.170897	1515.330098	17.104013
36.109854	1509.497837	17.109031
35.994684	1509.137241	17.114048
36.066609	1498.857313	17.119066
35.961055	1512.687891	17.124083
36.195811	1527.175170	17.129101
36.409250	1546.318583	17.134119
36.168500	1541.127423	17.139136
36.448744	1536.548982	17.144154
36.443678	1537.940169	17.149171
36.446284	1534.739787	17.154189
36.432839	1543.393421	17.159207
36.278029	1562.986254	17.164224
36.389454	1564.443700	17.169242
36.717956	1571.755118	17.174259
36.843827	1574.014506	17.179277
37.147890	1574.253363	17.184295
37.013871	1571.931216	17.189312
37.133239	1566.466470	17.194330
36.881111	1573.082471	17.199347
37.051826	1570.193060	17.204365
37.265374	1574.312817	17.209383
37.255686	1571.682708	17.214400
37.068193	1565.212585	17.219418
37.223709	1577.364817	17.224435
37.201560	1575.717659	17.229453
37.460243	1568.016581	17.234471
37.375679	1572.093738	17.239488
37.595487	1566.249134	17.244506
37.343737	1568.136604	17.249523
37.430422	1563.455894	17.254541
38.103531	1561.245391	17.259559
37.399293	1541.648279	17.264576
37.359112	1532.008483	17.269594
37.350204	1532.671117	17.274611
37.254093	1530.755119	17.279629
37.588001	1547.774901	17.284647
37.365984	1562.935080	17.289664
37.616035	1561.601136	17.294682
37.428109	1570.327224	17.299699
37.591191	1563.026833	17.304717
37.804200	1555.499358	17.309735
37.281642	1563.272077	17.314752
37.547801	1558.624777	17.319770
37.966862	1567.426341	17.324787
37.942044	1554.484328	17.329805
37.895619	1550.950186	17.334823
37.520945	1563.155904	17.339840
37.636314	1560.076356	17.344858
37.500869	1567.422825	17.349875
37.503144	1572.553319	17.354893
37.990119	1584.236478	17.359911
37.639646	1580.065801	17.364928
38.179052	1574.786938	17.369946
37.941741	1589.948978	17.374963
37.908270	1588.997537	17.379981
37.930043	1584.879192	17.384999
38.113031	1591.838755	17.390016
38.187214	1582.773480	17.395034
38.092732	1586.378667	17.400051
38.270043	1603.378897	17.405069
38.658089	1607.723103	17.410087
38.677007	1604.254133	17.415104
38.557765	1585.932803	17.420122
38.310234	1585.259035	17.425139
38.230945	1594.287412	17.430157
38.739570	1595.541706	17.435175
38.576536	1615.127745	17.440192
38.927228	1615.829133	17.445210
38.983411	1601.917179	17.450227
38.742413	1592.144830	17.455245
39.090099	1578.704629	17.460263
38.881893	1580.126711	17.465280
38.922985	1564.152586	17.470298
38.790825	1570.676750	17.475315
38.828909	1567.569502	17.480333
39.069384	1568.125593	17.485351
39.003626	1576.625205	17.490368
39.074468	1573.741105	17.495386
39.037255	1575.263804	17.500403
38.793943	1577.304963	17.505421
38.912249	1577.287054	17.510439
38.779709	1579.272997	17.515456
39.333300	1596.928863	17.520474
39.042332	1604.063798	17.525491
39.239313	1599.251950	17.530509
39.348642	1602.130388	17.535527
38.976440	1605.471350	17.540544
39.400149	1607.236322	17.545562
39.518738	1602.475712	17.550579
39.438706	1608.155429	17.555597
39.714981	1611.675005	17.560615
39.257655	1609.766592	17.565632
39.421247	1607.447356	17.570650
39.350744	1610.354266	17.575667
39.389124	1609.035348	17.580685
40.188355	1602.860652	17.585703
39.782719	1603.486572	17.590720
39.592087	1595.697144	17.595738
39.663606	1602.651806	17.600755
39.483073	1599.535572	17.605773
39.578613	1592.466851	17.610791
39.663317	1601.335998	17.615808
39.686921	1598.598197	17.620826
39.677228	1607.318947	17.625843
39.563377	1611.028259	17.630861
39.645251	1620.351890	17.635879
39.718571	1626.815254	17.640896
39.793283	1636.763815	17.645914
39.975535	1632.857339	17.650931
39.765739	1635.407778	17.655949
39.812636	1632.052916	17.660967
39.974711	1635.229044	17.665984
40.013841	1652.269556	17.671002
40.417937	1665.058448	17.676019
40.183069	1669.323624	17.681037
40.438619	1658.546307	17.686055
40.487969	1665.694583	17.691072
40.255855	1652.204105	17.696090
40.805503	1652.192959	17.701107
40.476734	1650.284155	17.706125
40.973929	1641.381779	17.711143
40.733133	1631.137269	17.716160
40.887850	1619.097202	17.721178
40.797705	1620.923109	17.726195
40.702304	1616.970530	17.731213
40.911045	1616.395717	17.736231
40.739827	1616.580220	17.741248
40.537535	1619.584145	17.746266
41.198616	1615.642433	17.751283
40.838588	1612.996784	17.756301
40.754346	1619.141058	17.761319
40.883530	1622.138551	17.766336
40.959135	1617.311676	17.771354
40.915902	1611.975197	17.776371
40.579427	1625.097745	17.781389
41.438814	1643.955313	17.786407
41.413918	1653.819770	17.791424
41.317231	1653.892665	17.796442
41.767000	1627.206646	17.801459
41.549241	1627.918085	17.806477
41.465515	1620.656440	17.811495
41.292305	1624.657066	17.816512
40.960044	1625.800781	17.821530
41.364994	1618.923121	17.826547
41.155143	1620.276189	17.831565
41.382418	1626.136321	17.836583
41.588020	1639.745927	17.841600
41.499658	1651.173408	17.846618
41.506266	1649.579193	17.851635
40.809802	1657.649522	17.856653
41.153129	1650.021696	17.861671
41.246197	1649.894716	17.866688
41.242182	1650.493910	17.871706
41.572550	1658.506704	17.876723
41.491040	1674.094133	17.881741
41.981735	1677.761629	17.886759
41.531794	1683.350052	17.891776
41.560271	1679.459693	17.896794
41.991744	1673.145637	17.901811
41.948711	1679.970350	17.906829
41.899178	1674.273472	17.911847
41.670542	1678.839978	17.916864
41.689967	1680.835710	17.921882
42.097558	1687.057121	17.926899
41.951419	1703.092718	17.931917
41.958895	1703.377702	17.936935
42.398438	1705.132884	17.941952
42.437074	1712.057401	17.946970
42.704022	1707.184306	17.951987
42.576085	1709.543142	17.957005
42.996558	1703.599901	17.962023
42.779302	1682.293336	17.967040
42.726452	1677.946000	17.972058
42.862234	1666.633243	17.977075
42.707893	1672.404472	17.982093
42.564034	1670.762816	17.987111
42.859828	1667.406615	17.992128
42.366259	1673.419492	17.997146
42.876254	1664.466872	18.002163
42.679771	1667.774176	18.007181
42.969139	1666.323627	18.012199
42.961477	1673.567518	18.017216
42.268115	1674.531782	18.022234
42.820233	1661.039136	18.027251
42.328621	1675.752677	18.032269
42.367744	1689.769260	18.037287
42.525796	1694.410040	18.042304
42.837767	1710.966384	18.047322
42.596110	1704.419260	18.052339
42.815737	1717.075630	18.057357
42.749274	1731.276908	18.062375
42.964981	1732.774765	18.067392
43.175007	1734.411409	18.072410
43.185385	1726.304347	18.077427
43.262234	1734.295678	18.082445
43.363042	1733.470043	18.087463
43.427839	1734.952824	18.092480
43.021661	1744.538181	18.097498
43.339408	1731.730223	18.102515
43.087899	1734.517384	18.107533
43.344607	1751.873499	18.112551
43.849731	1764.845963	18.117568
43.809870	1772.617531	18.122586
44.319811	1754.643696	18.127603
44.257544	1751.939884	18.132621
44.205133	1740.373872	18.137639
44.026017	1736.061162	18.142656
44.111976	1738.239611	18.147674
44.178898	1728.674256	18.152691
44.113198	1722.382816	18.157709
44.075989	1725.815205	18.162727
44.294677	1726.793985	18.167744
43.948296	1724.394431	18.172762
44.162854	1720.283947	18.177779
44.025154	1724.648633	18.182797
43.762530	1729.733641	18.187815
44.204654	1717.996232	18.192832
43.688930	1726.731359	18.197850
43.786522	1728.701489	18.202867
44.060707	1748.501744	18.207885
44.238990	1758.446406	18.212903
44.801675	1756.758415	18.217920
44.229934	1771.744476	18.222938
44.120935	1756.751910	18.227955
44.186871	1764.978621	18.232973
44.528928	1757.208031	18.237991
44.306389	1760.361928	18.243008
44.172130	1759.192689	18.248026
44.261813	1768.512707	18.253043
44.412622	1782.852786	18.258061
44.388364	1790.631138	18.263079
45.082488	1783.308897	18.268096
44.999553	1789.067927	18.273114
45.307405	1779.913256	18.278131
45.097949	1791.845519	18.283149
45.382316	1784.876636	18.288167
45.503140	1779.772634	18.293184
44.890841	1779.503564	18.298202
45.127363	1774.715989	18.303219
44.908228	1781.979257	18.308237
45.039951	1780.975069	18.313255
45.177044	1775.987585	18.318272
45.125852	1785.745203	18.323290
45.153990	1777.257465	18.328307
45.077537	1783.742241	18.333325
45.053432	1778.504801	18.338343
45.515299	1771.695672	18.343360
45.163942	1778.748902	18.348378
45.349742	1796.961422	18.353395
45.749271	1810.137878	18.358413
45.789847	1807.893255	18.363431
45.916092	1807.198704	18.368448
45.528512	1806.015013	18.373466
45.586978	1807.183887	18.378483
45.779815	1811.699432	18.383501
45.726055	1810.326600	18.388519
45.850630	1798.419532	18.393536
45.672565	1814.245730	18.398554
45.630195	1813.992344	18.403571
46.039745	1815.023063	18.408589
45.971141	1810.093279	18.413607
46.094191	1805.132212	18.418624
45.737754	1812.211135	18.423642
46.199936	1811.478675	18.428659
46.096439	1807.962135	18.433677
46.297212	1823.306015	18.438695
46.513786	1828.769977	18.443712
46.183157	1829.023551	18.448730
46.530247	1826.097160	18.453747
46.282779	1827.546863	18.458765
46.498714	1840.372098	18.463783
46.194568	1835.175171	18.468800
46.217009	1849.380607	18.473818
46.233986	1840.384447	18.478835
46.480984	1840.500399	18.483853
46.196411	1843.680305	18.488871
46.480575	1843.733184	18.493888
46.513045	1840.985945	18.498906
46.651193	1853.418571	18.503923
46.943147	1869.474514	18.508941
46.552905	1874.077053	18.513959
47.126446	1869.215130	18.518976
46.878331	1872.444703	18.523994
47.020643	1868.661174	18.529011
47.241774	1871.857545	18.534029
47.293799	1876.873691	18.539047
47.504761	1866.553540	18.544064
46.963850	1867.413319	18.549082
47.224982	1862.894761	18.554099
47.481862	1862.421543	18.559117
47.204520	1860.236144	18.564135
47.233789	1870.167838	18.569152
47.389292	1873.404993	18.574170
47.621527	1866.808050	18.579187
47.904310	1867.199399	18.584205
47.393731	1867.003056	18.589223
47.680212	1875.373926	18.594240
47.120258	1873.923681	18.599258
47.570383	1865.257626	18.604275
47.746265	1866.542612	18.609293
47.186283	1868.330581	18.614311
47.675134	1863.151642	18.619328
47.251237	1862.655755	18.624346
47.582271	1887.415577	18.629363
48.021860	1888.323813	18.634381
47.835241	1889.778839	18.639399
47.981619	1893.100250	18.644416
47.882874	1889.413564	18.649434
47.566329	1892.293410	18.654451
47.658475	1886.539088	18.659469
48.172926	1903.137703	18.664487
48.533177	1909.520489	18.669504
48.435690	1926.779237	18.674522
48.581811	1922.339443	18.679539
48.490433	1907.490975	18.684557
48.267747	1912.298292	18.689575
48.801315	1912.718308	18.694592
48.706296	1901.628047	18.699610
48.541177	1897.992901	18.704627
48.831877	1890.226327	18.709645
48.707538	1892.398722	18.714663
49.306809	1885.797906	18.719680
49.101934	1884.549808	18.724698
49.178808	1887.713428	18.729715
48.980459	1882.170744	18.734733
48.486362	1895.669012	18.739751
48.554256	1884.152748	18.744768
48.926389	1882.920304	18.749786
48.614656	1884.418831	18.754803
48.567365	1883.469741	18.759821
49.127004	1912.146036	18.764839
49.372015	1907.768830	18.769856
49.139887	1924.163930	18.774874
48.997062	1913.436628	18.779891
49.067619	1917.540829	18.784909
49.166865	1919.087022	18.789927
49.093582	1918.848778	18.794944
49.058780	1921.190103	18.799962
49.079153	1920.152628	18.804979
49.386261	1917.409083	18.809997
49.085438	1933.216285	18.815015
48.948126	1941.622837	18.820032
49.375017	1951.067456	18.825050
49.111800	1956.559780	18.830067
49.499243	1951.627362	18.835085
49.473638	1964.483085	18.840103
49.640267	1977.713002	18.845120
49.910367	1986.140291	18.850138
49.761386	1986.176871	18.855155
50.036701	1990.218423	18.860173
49.994603	1984.915879	18.865191
49.858424	1981.856145	18.870208
49.830801	1980.350847	18.875226
49.841493	1984.712607	18.880243
50.275431	1979.968693	18.885261
50.157275	1984.437989	18.890279
50.340838	1981.758927	18.895296
50.160933	1983.425044	18.900314
50.204268	1988.187563	18.905331
50.508914	1998.924997	18.910349
50.120097	1999.758312	18.915367
50.453683	1999.248313	18.920384
50.597757	1996.794160	18.925402
50.692945	2005.289247	18.930419
50.802012	1997.709687	18.935437
50.443386	1999.139876	18.940455
50.289799	1998.644496	18.945472
50.688582	1990.598676	18.950490
50.653367	2003.472617	18.955507
50.740405	1993.952870	18.960525
50.880323	2012.178625	18.965543
51.076194	2021.374668	18.970560
51.092340	2024.504626	18.975578
50.912653	2034.470675	18.980595
51.420913	2026.906136	18.985613
51.209917	2030.614483	18.990631
51.133165	2032.275126	18.995648
51.561779	2029.211476	19.000666
50.979819	2031.839961	19.005683
51.569274	2027.658427	19.010701
51.394949	2030.776548	19.015719
51.267105	2027.231452	19.020736
51.330587	2030.232413	19.025754
51.335459	2025.034810	19.030771
51.619457	2030.466414	19.035789
51.618325	2036.604477	19.040807
51.517440	2029.125868	19.045824
51.849512	2029.953714	19.050842
51.395885	2026.386116	19.055859
51.757221	2027.459373	19.060877
51.741447	2034.847362	19.065895
51.644243	2043.685341	19.070912
51.813831	2053.553325	19.075930
51.666583	2062.946822	19.080947
51.969466	2053.988147	19.085965
51.926221	2057.774054	19.090983
51.834430	2060.647291	19.096000
51.932276	2056.007046	19.101018
51.667338	2064.579266	19.106035
52.039187	2075.292630	19.111053
52.091427	2088.615491	19.116071
52.004831	2092.726207	19.121088
52.267170	2086.550844	19.126106
52.259604	2088.533537	19.131123
52.633659	2082.804048	19.136141
52.508521	2093.213208	19.141159
52.681172	2110.747542	19.146176
52.745180	2111.833587	19.151194
52.663165	2122.425558	19.156211
53.019029	2115.014682	19.161229
52.825993	2116.757484	19.166247
53.121231	2116.668290	19.171264
53.006236	2113.626949	19.176282
52.780529	2117.409503	19.181299
53.387376	2111.655842	19.186317
53.228705	2115.502504	19.191335
53.112598	2111.109979	19.196352
53.092660	2113.142046	19.201370
53.501804	2117.213450	19.206387
53.170919	2111.600875	19.211405
53.081723	2115.334824	19.216423
53.302171	2119.896126	19.221440
53.376972	2103.191159	19.226458
53.564226	2112.983306	19.231475
53.676523	2109.301336	19.236493
53.257877	2115.847281	19.241511
53.370979	2109.666389	19.246528
53.501436	2125.932200	19.251546
53.419698	2150.645869	19.256563
53.718246	2142.506905	19.261581
54.039783	2144.921440	19.266599
53.643709	2151.144585	19.271616
53.855268	2140.410707	19.276634
53.638428	2142.901796	19.281651
54.261178	2146.775144	19.286669
54.125606	2143.909004	19.291687
53.868944	2136.740163	19.296704
54.347944	2140.123908	19.301722
54.188244	2140.575772	19.306739
54.359210	2139.729818	19.311757
54.362837	2136.579933	19.316775
54.315360	2149.015087	19.321792
54.272381	2140.251901	19.326810
54.265932	2153.487228	19.331827
54.454652	2171.606362	19.336845
54.101373	2173.074238	19.341863
54.525091	2174.244306	19.346880
54.765432	2175.515116	19.351898
54.695039	2176.007583	19.356915
54.710406	2167.854156	19.361933
55.113439	2169.523906	19.366951
54.553355	2166.476963	19.371968
54.845663	2162.041965	19.376986
55.047138	2170.744149	19.382003
55.170096	2179.036116	19.387021
55.419826	2173.753957	19.392039
55.106431	2169.763011	19.397056
54.797336	2160.854073	19.402074
54.880903	2186.641194	19.407091
54.645471	2198.281717	19.412109
54.752580	2204.380024	19.417127
54.845772	2209.989308	19.422144
55.187111	2220.757617	19.427162
55.647006	2235.355008	19.432179
55.826968	2240.379261	19.437197
56.143967	2234.492546	19.442215
55.993579	2235.694110	19.447232
56.420579	2234.136438	19.452250
56.056605	2220.000651	19.457267
55.982684	2211.774307	19.462285
56.196198	2196.166099	19.467303
55.735746	2205.158194	19.472320
55.842390	2197.259220	19.477338
55.743749	2209.708707	19.482355
55.827583	2231.895318	19.487373
55.947292	2228.651486	19.492391
55.494286	2239.466220	19.497408
55.853302	2231.763367	19.502426
55.895562	2236.717513	19.507443
55.767604	2240.371509	19.512461
56.124336	2254.187270	19.517479
56.150619	2272.802159	19.522496
56.276050	2264.084846	19.527514
56.751598	2246.501446	19.532531
56.879910	2242.687545	19.537549
57.602972	2235.224684	19.542567
57.464445	2243.542615	19.547584
57.600466	2235.881142	19.552602
57.329660	2225.684306	19.557619
57.089349	2216.267406	19.562637
57.301667	2211.740580	19.567655
57.342906	2204.340291	19.572672
57.617582	2204.413701	19.577690
57.537967	2200.978818	19.582707
57.358407	2203.389497	19.587725
57.676896	2202.602513	19.592743
57.429325	2206.901511	19.597760
57.463130	2195.901964	19.602778
57.147111	2189.967079	19.607795
57.330718	2198.258895	19.612813
57.242716	2193.468556	19.617831
57.153898	2200.461999	19.622848
57.391218	2204.399082	19.627866
56.815315	2193.666298	19.632883
57.203652	2206.743420	19.637901
57.669256	2227.402149	19.642919
57.688153	2234.354301	19.647936
57.807309	2238.822752	19.652954
57.596598	2244.165206	19.657971
57.925710	2246.139809	19.662989
58.207758	2246.232431	19.668007
57.961774	2248.126079	19.673024
58.009452	2245.032409	19.678042
57.964452	2235.973409	19.683059
57.780983	2244.625867	19.688077
58.220600	2255.759299	19.693095
58.341700	2270.386458	19.698112
58.387430	2275.837735	19.703130
58.548838	2276.695250	19.708147
58.467210	2275.991037	19.713165
59.089484	2268.466687	19.718183
58.885883	2275.019929	19.723200
59.023563	2267.243179	19.728218
59.033563	2276.011326	19.733235
58.768916	2268.464995	19.738253
58.875438	2262.990791	19.743271
58.834519	2263.249826	19.748288
58.745649	2265.527625	19.753306
58.718397	2277.201817	19.758323
58.711823	2270.809848	19.763341
59.473927	2268.285919	19.768359
59.194580	2274.381997	19.773376
58.980585	2272.711349	19.778394
58.997080	2267.643189	19.783411
59.047365	2273.864670	19.788429
59.003690	2272.227036	19.793447
59.148235	2294.960106	19.798464
59.488442	2302.343102	19.803482
59.437112	2299.998006	19.808499
59.098865	2299.290537	19.813517
58.934052	2293.898281	19.818535
58.961023	2312.270541	19.823552
59.074495	2318.799366	19.828570
59.442447	2315.146756	19.833587
59.266271	2336.718936	19.838605
59.588462	2339.437374	19.843623
59.499197	2354.777163	19.848640
59.940531	2353.408391	19.853658
59.951350	2352.624534	19.858675
59.792221	2358.275557	19.863693
60.260901	2355.746794	19.868711
60.014747	2361.089064	19.873728
60.216108	2371.731847	19.878746
61.199048	2371.823220	19.883763
60.944946	2360.440566	19.888781
60.740421	2350.810329	19.893799
60.999833	2345.892653	19.898816
60.658321	2345.333009	19.903834
61.031558	2344.386214	19.908851
61.006781	2340.962373	19.913869
60.913934	2343.510987	19.918887
60.903644	2338.434009	19.923904
61.057825	2340.177158	19.928922
61.055901	2329.615994	19.933939
60.660573	2350.665836	19.938957
61.023530	2336.528167	19.943975
60.785042	2342.559776	19.948992
61.070505	2346.274434	19.954010
61.435937	2362.108805	19.959027
61.145633	2380.007110	19.964045
61.280128	2376.899317	19.969063
61.592578	2371.689030	19.974080
61.432389	2378.143519	19.979098
61.925466	2379.248949	19.984115
61.562458	2380.252294	19.989133
61.865399	2379.222258	19.994151
61.287393	2377.085576	19.999168
61.403993	2374.243099	20.004186
61.584043	2374.507564	20.009203
61.469940	2380.335156	20.014221
61.822315	2390.063729	20.019239
62.038910	2404.317103	20.024256
61.731933	2408.001042	20.029274
61.951136	2409.193594	20.034291
61.633506	2417.673053	20.039309
62.075268	2401.280507	20.044327
62.194997	2401.048146	20.049344
62.337734	2406.229253	20.054362
62.411194	2405.785105	20.059379
62.504573	2419.428807	20.064397
62.495711	2418.579806	20.069415
62.735453	2426.529782	20.074432
62.860952	2420.273402	20.079450
62.869406	2413.644903	20.084467
62.792170	2422.902969	20.089485
62.798352	2416.680435	20.094503
62.738849	2422.242734	20.099520
62.529691	2422.666859	20.104538
63.110554	2417.179792	20.109555
63.170993	2416.487441	20.114573
62.937322	2411.220354	20.119591
63.019327	2412.052901	20.124608
63.183961	2413.624159	20.129626
63.518006	2406.702007	20.134643
62.993065	2420.843121	20.139661
63.054229	2407.706104	20.144679
62.956804	2424.060909	20.149696
63.458043	2439.334192	20.154714
63.366772	2439.493183	20.159731
63.404743	2445.035628	20.164749
63.792574	2445.958287	20.169767
63.697878	2446.989662	20.174784
63.171866	2444.852720	20.179802
63.882132	2451.224154	20.184819
64.079613	2470.469878	20.189837
64.253322	2470.277876	20.194855
64.377436	2469.636821	20.199872
64.467413	2469.899406	20.204890
64.753064	2456.878217	20.209907
63.935193	2456.337235	20.214925
64.096271	2446.356809	20.219943
64.392270	2457.289774	20.224960
64.332095	2465.467597	20.229978
64.522263	2462.553426	20.234995
64.573501	2467.012323	20.240013
64.442404	2467.581359	20.245031
64.581305	2464.832695	20.250048
64.741080	2464.978572	20.255066
65.158308	2456.842725	20.260083
64.530232	2459.275212	20.265101
64.589690	2464.226482	20.270119
64.907494	2465.776211	20.275136
64.689445	2488.774911	20.280154
64.990476	2493.683198	20.285171
64.810444	2497.438323	20.290189
65.042251	2502.711296	20.295207
65.114333	2497.645345	20.300224
65.042253	2505.481077	20.305242
65.210300	2496.769717	20.310259
65.285521	2511.078927	20.315277
65.344724	2523.448048	20.320295
65.281713	2525.693888	20.325312
65.276392	2530.347571	20.330330
65.343968	2525.235919	20.335347
65.838601	2537.265785	20.340365
65.735553	2542.639496	20.345383
65.508089	2562.323604	20.350400
65.528413	2567.435973	20.355418
65.857094	2564.814626	20.360435
65.392201	2562.916837	20.365453
65.877620	2569.569431	20.370471
66.247405	2584.258201	20.375488
66.400846	2597.038068	20.380506
66.531574	2593.730844	20.385523
66.614938	2591.708341	20.390541
66.612056	2590.748050	20.395559
66.503098	2590.054021	20.400576
66.521505	2593.436505	20.405594
66.884591	2587.273207	20.410611
66.944173	2587.722139	20.415629
66.839762	2579.818207	20.420647
67.159170	2582.619858	20.425664
66.837953	2584.053133	20.430682
66.998715	2584.463454	20.435699
67.127759	2590.261250	20.440717
67.131847	2595.681189	20.445735
67.125792	2590.740435	20.450752
66.965288	2602.299107	20.455770
67.287111	2579.547086	20.460787
67.303611	2584.701068	20.465805
67.393083	2587.967412	20.470823
67.377213	2582.074635	20.475840
67.052519	2584.939463	20.480858
67.051158	2594.301965	20.485875
67.268485	2615.766110	20.490893
67.473805	2618.346341	20.495911
67.464684	2617.091791	20.500928
67.356379	2625.954445	20.505946
67.725083	2632.057685	20.510963
67.705813	2639.627692	20.515981
67.891502	2646.701064	20.520999
68.512049	2645.842584	20.526016
68.599435	2645.556700	20.531034
68.447167	2643.996710	20.536051
68.843546	2645.730659	20.541069
68.711630	2637.305335	20.546087
69.171819	2636.651545	20.551104
69.112851	2618.545878	20.556122
68.883341	2606.642202	20.561139
68.965115	2600.796468	20.566157
68.647037	2601.944905	20.571175
68.867905	2592.156533	20.576192
68.836684	2606.646312	20.581210
68.510278	2593.403116	20.586227
68.790241	2612.663225	20.591245
68.492088	2623.735973	20.596263
69.246810	2630.226655	20.601280
69.248889	2641.408601	20.606298
69.128012	2635.596810	20.611315
69.113774	2633.623323	20.616333
68.717234	2640.819352	20.621351
69.069768	2650.652016	20.626368
68.878327	2671.365701	20.631386
68.853173	2671.548798	20.636403
69.383834	2667.841436	20.641421
69.555886	2675.283366	20.646439
69.944305	2682.688205	20.651456
69.852061	2696.460052	20.656474
69.864498	2686.674279	20.661491
69.876343	2691.210085	20.666509
69.887652	2693.521961	20.671527
69.847127	2689.664446	20.676544
69.797657	2698.561156	20.681562
69.982210	2696.970978	20.686579
69.850370	2698.499378	20.691597
69.751256	2708.616635	20.696615
70.069353	2720.445372	20.701632
70.060775	2738.823438	20.706650
70.276281	2729.012275	20.711667
70.434648	2729.221399	20.716685
70.528056	2736.435853	20.721703
70.877837	2741.813900	20.726720
70.424947	2754.152867	20.731738
70.841689	2756.204656	20.736755
70.960468	2757.422328	20.741773
70.813650	2753.354631	20.746791
71.062483	2756.818140	20.751808
71.242709	2769.297438	20.756826
71.527978	2764.223991	20.761843
71.481791	2754.080442	20.766861
71.321663	2757.073809	20.771879
71.376974	2761.278501	20.776896
71.034016	2758.882528	20.781914
71.003897	2760.674648	20.786931
71.538093	2776.874279	20.791949
71.780779	2784.698713	20.796967
71.890483	2786.721241	20.801984
71.831754	2785.672070	20.807002
71.884114	2786.996424	20.812019
71.788295	2785.247969	20.817037
71.635361	2788.848883	20.822055
71.552112	2787.233730	20.827072
72.170274	2807.908023	20.832090
71.898381	2820.259325	20.837107
72.264361	2823.951630	20.842125
72.050417	2813.549349	20.847143
72.492334	2808.468720	20.852160
72.591829	2807.900389	20.857178
73.056469	2811.385977	20.862195
73.029605	2814.797535	20.867213
72.788079	2817.576478	20.872231
72.955762	2814.700750	20.877248
72.924294	2811.983598	20.882266
72.932439	2819.408807	20.887283
72.642164	2817.895299	20.892301
72.361634	2830.545784	20.897319
72.950964	2840.889255	20.902336
72.789642	2846.328977	20.907354
72.491798	2848.931719	20.912371
72.443149	2852.108391	20.917389
72.803631	2869.887014	20.922407
72.745203	2870.300271	20.927424
72.865648	2888.972988	20.932442
73.034631	2902.348192	20.937459
73.513322	2900.688665	20.942477
73.151875	2910.157192	20.947495
73.777648	2922.027050	20.952512
73.689217	2933.536593	20.957530
73.852061	2941.190505	20.962547
74.408599	2923.234131	20.967565
74.363804	2925.204410	20.972583
74.535365	2922.210652	20.977600
75.055749	2920.836945	20.982618
74.941543	2908.587223	20.987635
75.110798	2896.459812	20.992653
74.436868	2894.473386	20.997671
74.868569	2885.382686	21.002688
75.060979	2895.072058	21.007706
74.603074	2886.702489	21.012723
75.316319	2887.834004	21.017741
74.686328	2892.312159	21.022759
74.923798	2891.424051	21.027776
74.956603	2891.372760	21.032794
74.995297	2893.427166	21.037811
75.042004	2882.061865	21.042829
74.821945	2892.266918	21.047847
75.102155	2895.027305	21.052864
75.248067	2902.126514	21.057882
75.294886	2914.086174	21.062899
75.479258	2918.212866	21.067917
75.129919	2920.357428	21.072935
75.582846	2932.011998	21.077952
75.529178	2928.248034	21.082970
75.238200	2934.985066	21.087987
75.439239	2948.541465	21.093005
75.154196	2967.383026	21.098023
75.376212	2963.220538	21.103040
75.499983	2967.587599	21.108058
75.701857	2983.555385	21.113075
76.243367	2989.175506	21.118093
76.223626	2988.028280	21.123111
76.243899	2986.667066	21.128128
76.436641	2989.142407	21.133146
76.460831	2993.194986	21.138163
76.580798	2983.507152	21.143181
76.656502	2986.225436	21.148199
76.800158	2988.274461	21.153216
76.600130	2991.299913	21.158234
76.485121	3013.668205	21.163251
76.813713	3009.295269	21.168269
76.964502	3023.713275	21.173287
76.613848	3022.570800	21.178304
77.007263	3019.872913	21.183322
76.866518	3021.779324	21.188339
77.061823	3030.761054	21.193357
77.044141	3051.267459	21.198375
77.570045	3049.213917	21.203392
77.326587	3049.314736	21.208410
77.678736	3052.405408	21.213427
77.811338	3045.472623	21.218445
77.780758	3045.882684	21.223463
77.844696	3043.093219	21.228480
77.972606	3048.704727	21.233498
77.765750	3049.925483	21.238515
77.821229	3042.692473	21.243533
77.828378	3050.828342	21.248551
77.797997	3052.214945	21.253568
78.068675	3061.275128	21.258586
77.942298	3078.650744	21.263603
77.919214	3077.771856	21.268621
78.006212	3073.448197	21.273639
78.183844	3084.116009	21.278656
78.419641	3094.401339	21.283674
78.441061	3108.724255	21.288691
78.713109	3108.357875	21.293709
78.354840	3104.683105	21.298727
78.978806	3102.058300	21.303744
79.145297	3097.481587	21.308762
78.747436	3114.476140	21.313779
79.049320	3125.003755	21.318797
79.267048	3133.099626	21.323815
79.247110	3137.204699	21.328832
79.696758	3131.627263	21.333850
79.562072	3126.428021	21.338867
79.529749	3132.355278	21.343885
79.597808	3133.552535	21.348903
79.494891	3127.048363	21.353920
79.865056	3123.466859	21.358938
79.881427	3131.535821	21.363955
80.053699	3138.340793	21.368973
79.829846	3129.029992	21.373991
79.680628	3133.861311	21.379008
79.844918	3139.654056	21.384026
79.948258	3154.524503	21.389043
80.129953	3151.046974	21.394061
79.911782	3159.180575	21.399079
80.165456	3162.841812	21.404096
80.146046	3166.626261	21.409114
80.093756	3184.105851	21.414131
80.821189	3191.587485	21.419149
80.483711	3192.046227	21.424167
80.200361	3199.998857	21.429184
80.844747	3200.489309	21.434202
80.795549	3221.276988	21.439219
81.712734	3204.182285	21.444237
81.915906	3201.891867	21.449255
81.666918	3185.268827	21.454272
81.694062	3174.777719	21.459290
81.772469	3170.686265	21.464307
81.620034	3166.802926	21.469325
81.862295	3163.785188	21.474343
81.507816	3164.427198	21.479360
81.738162	3157.726478	21.484378
81.516162	3173.575749	21.489395
81.852313	3170.230036	21.494413
81.942258	3159.525766	21.499431
81.794691	3167.926066	21.504448
82.075827	3163.228083	21.509466
82.020975	3180.434823	21.514483
82.246400	3188.701881	21.519501
82.612122	3193.139359	21.524519
82.113077	3199.123819	21.529536
82.266453	3201.157816	21.534554
82.092350	3203.892189	21.539571
82.500110	3189.708274	21.544589
82.450588	3199.956744	21.549607
82.505250	3201.635145	21.554624
82.623303	3211.956490	21.559642
82.654387	3229.060342	21.564659
82.759306	3229.392835	21.569677
82.700708	3226.062020	21.574695
82.802319	3234.444051	21.579712
82.730141	3248.012896	21.584730
82.945291	3253.948177	21.589747
83.339698	3249.930112	21.594765
83.224365	3253.124598	21.599783
83.240121	3260.047814	21.604800
83.730229	3273.739227	21.609818
83.514053	3291.629007	21.614835
83.644993	3297.290489	21.619853
84.129710	3291.021797	21.624871
84.021950	3298.085130	21.629888
84.272281	3288.918972	21.634906
83.950694	3293.260880	21.639923
83.966637	3294.146542	21.644941
83.910038	3288.745628	21.649959
83.931894	3291.700807	21.654976
84.149367	3301.790945	21.659994
84.235310	3302.746515	21.665011
84.307712	3316.865561	21.670029
84.332492	3316.510067	21.675047
84.677053	3329.680692	21.680064
85.053170	3336.758744	21.685082
84.932264	3350.311617	21.690099
85.460720	3349.384623	21.695117
85.493178	3339.472939	21.700135
85.482377	3354.506482	21.705152
85.724718	3340.028675	21.710170
85.487666	3330.564864	21.715187
85.474499	3338.795724	21.720205
86.098141	3325.513467	21.725223
85.574517	3316.455567	21.730240
85.517262	3324.034778	21.735258
85.397577	3336.218624	21.740275
85.168139	3337.118004	21.745293
85.804210	3336.649045	21.750311
85.235463	3346.731452	21.755328
85.532790	3359.227372	21.760346
85.867249	3368.847004	21.765363
85.442888	3377.219261	21.770381
86.012084	3384.894296	21.775399
85.466254	3401.491595	21.780416
85.827585	3401.244578	21.785434
85.952711	3408.684663	21.790451
86.349196	3423.905986	21.795469
86.684419	3425.178750	21.800487
86.756235	3439.549245	21.805504
86.741598	3421.395675	21.810522
86.782606	3428.419385	21.815539
87.089945	3424.469759	21.820557
87.153279	3416.367317	21.825575
86.795564	3427.489430	21.830592
87.396480	3450.406620	21.835610
88.251973	3445.000497	21.840627
88.548413	3419.847134	21.845645
88.492259	3402.900975	21.850663
88.204009	3395.401462	21.855680
88.468635	3389.200392	21.860698
88.569768	3389.681603	21.865715
88.422143	3387.930935	21.870733
88.589548	3370.155755	21.875751
88.289628	3362.116405	21.880768
88.343963	3356.940598	21.885786
88.529819	3369.231177	21.890803
88.386157	3357.481542	21.895821
88.505217	3358.611004	21.900839
88.523167	3363.489341	21.905856
88.571171	3360.233156	21.910874
88.762303	3361.653480	21.915891
88.638987	3373.100805	21.920909
88.973541	3382.266784	21.925927
88.553244	3390.704509	21.930944
88.800389	3394.367707	21.935962
88.830610	3405.428809	21.940979
88.855266	3402.223873	21.945997
88.980228	3399.847600	21.951015
89.104942	3434.608116	21.956032
88.964418	3433.127941	21.961050
89.122249	3436.572550	21.966067
88.791580	3449.867703	21.971085
89.339211	3455.068739	21.976103
89.071670	3462.382423	21.981120
89.454047	3472.457002	21.986138
89.622152	3496.939356	21.991155
89.256773	3509.916813	21.996173
89.977291	3499.802006	22.001191
89.614007	3503.689595	22.006208
89.943360	3525.535083	22.011226
90.073833	3525.358360	22.016243
90.121694	3539.581837	22.021261
90.604304	3541.968980	22.026279
89.993821	3549.090259	22.031296
90.440209	3560.163605	22.036314
90.897165	3566.255233	22.041331
91.210455	3560.494679	22.046349
91.335802	3557.375622	22.051367
91.563467	3558.912565	22.056384
91.400513	3562.642172	22.061402
91.678660	3551.947114	22.066419
91.637230	3556.645094	22.071437
91.458469	3545.483363	22.076455
91.617008	3543.064296	22.081472
91.767023	3549.403861	22.086490
91.686774	3546.105043	22.091507
91.739454	3544.397200	22.096525
91.702003	3550.740553	22.101543
91.796247	3549.353219	22.106560
91.766412	3548.311644	22.111578
91.759471	3549.984892	22.116595
91.656472	3564.851723	22.121613
91.941236	3571.144568	22.126631
91.762621	3578.782511	22.131648
91.848748	3589.534874	22.136666
92.514449	3602.553012	22.141683
92.271739	3613.316875	22.146701
92.605538	3615.326295	22.151719
92.437472	3620.086172	22.156736
92.931618	3626.581783	22.161754
92.802208	3631.754034	22.166771
92.537575	3651.437208	22.171789
92.852634	3645.877155	22.176807
92.755845	3647.657965	22.181824
93.065346	3667.144280	22.186842
93.413069	3678.429161	22.191859
93.021275	3687.140175	22.196877
93.332986	3679.141509	22.201895
93.695446	3685.041460	22.206912
93.511634	3703.428640	22.211930
93.951919	3710.016217	22.216947
94.033258	3713.639395	22.221965
94.479806	3704.666186	22.226983
94.625874	3697.170040	22.232000
94.364984	3702.226239	22.237018
94.776335	3701.028682	22.242035
94.655061	3700.744687	22.247053
94.868360	3691.925674	22.252071
94.748739	3695.849508	22.257088
94.742754	3696.873630	22.262106
94.926099	3689.003291	22.267123
94.954920	3690.998062	22.272141
94.878629	3692.569801	22.277159
95.161876	3690.779884	22.282176
95.174001	3701.927782	22.287194
95.462251	3703.746549	22.292211
95.099108	3723.545938	22.297229
95.627460	3729.377297	22.302247
95.732052	3732.136440	22.307264
95.469370	3736.069846	22.312282
95.602444	3730.999344	22.317299
95.619225	3738.449496	22.322317
95.643946	3731.791662	22.327335
95.697891	3726.251144	22.332352
95.753514	3745.661367	22.337370
96.230066	3756.769849	22.342387
95.450698	3764.795984	22.347405
95.912264	3761.205758	22.352423
96.038563	3770.557311	22.357440
96.094278	3794.144206	22.362458
96.028803	3782.043758	22.367475
96.265738	3802.793387	22.372493
96.299267	3807.566014	22.377511
96.409578	3819.402062	22.382528
96.373157	3817.309365	22.387546
96.844676	3830.613015	22.392563
96.640012	3864.603178	22.397581
97.020212	3856.423347	22.402599
97.588465	3858.873042	22.407616
97.329730	3850.748409	22.412634
97.656986	3849.899202	22.417651
97.492919	3858.503535	22.422669
97.845546	3866.527826	22.427687
98.130974	3870.392501	22.432704
98.250009	3876.046782	22.437722
98.674753	3862.881663	22.442739
98.478805	3874.711975	22.447757
98.394838	3871.926455	22.452775
98.571973	3863.720001	22.457792
98.400500	3872.834402	22.462810
98.665401	3870.397052	22.467827
98.830765	3872.193589	22.472845
98.857992	3865.575437	22.477863
99.182904	3863.966595	22.482880
98.730068	3871.313810	22.487898
98.960852	3860.466780	22.492915
98.714197	3866.004965	22.497933
98.570081	3878.266664	22.502951
99.030085	3893.041220	22.507968
99.191817	3900.181486	22.512986
98.993262	3901.574155	22.518003
98.956790	3903.873923	22.523021
99.412689	3924.709827	22.528039
99.697802	3931.932919	22.533056
100.095684	3934.856831	22.538074
100.132411	3929.989446	22.543091
99.653150	3938.688815	22.548109
99.785146	3958.434327	22.553127
100.200337	3958.471061	22.558144
100.107819	3967.841343	22.563162
100.163244	3967.573518	22.568179
100.595297	3967.957846	22.573197
100.486889	3972.311435	22.578215
100.815282	3977.421065	22.583232
100.861734	3981.317286	22.588250
101.381068	3969.508663	22.593267
101.490813	3970.060088	22.598285
101.833749	3967.365187	22.603303
101.528519	3953.268170	22.608320
101.322659	3948.621942	22.613338
101.707464	3940.673623	22.618355
101.496878	3936.952070	22.623373
101.846687	3948.940120	22.628391
102.100449	3952.518830	22.633408
102.096613	3953.162974	22.638426
101.543258	3945.278613	22.643443
101.843395	3958.835434	22.648461
101.751316	3962.582914	22.653479
101.803292	3965.622842	22.658496
101.825564	3976.264337	22.663514
102.306766	3982.592192	22.668531
102.112569	3997.038730	22.673549
102.535893	3999.307728	22.678567
102.045360	3978.558811	22.683584
102.065258	4015.176851	22.688602
102.546229	4023.134327	22.693619
102.441728	4031.317409	22.698637
102.473609	4044.183090	22.703655
102.792508	4056.810548	22.708672
103.220090	4057.266531	22.713690
103.269038	4058.980659	22.718707
103.513830	4062.086001	22.723725
103.552418	4065.908767	22.728743
104.284795	4071.646995	22.733760
104.226081	4076.473324	22.738778
104.227889	4057.857025	22.743795
104.355574	4050.891564	22.748813
104.103362	4048.690910	22.753831
104.881730	4054.285778	22.758848
104.729426	4051.131526	22.763866
104.598714	4047.553776	22.768883
104.901963	4044.575037	22.773901
104.822541	4040.013433	22.778919
104.980490	4030.834332	22.783936
104.720124	4044.984301	22.788954
105.187840	4052.735347	22.793971
105.148211	4072.604939	22.798989
104.922219	4084.706772	22.804007
105.384155	4077.558765	22.809024
105.237498	4078.795268	22.814042
104.902714	4075.577781	22.819059
105.336637	4080.502381	22.824077
105.301258	4097.766640	22.829095
105.483293	4103.407839	22.834112
105.423902	4122.206576	22.839130
105.784357	4110.243936	22.844147
105.454253	4119.916526	22.849165
106.006712	4135.629263	22.854183
106.308065	4138.564250	22.859200
106.155831	4144.893651	22.864218
106.423752	4142.214731	22.869235
106.305897	4145.849318	22.874253
106.537486	4143.229397	22.879271
106.387081	4149.503353	22.884288
106.141623	4174.632619	22.889306
106.697022	4172.945640	22.894323
107.166387	4170.693724	22.899341
106.678683	4176.010277	22.904359
107.371988	4183.580943	22.909376
107.828903	4187.087861	22.914394
107.655482	4188.749548	22.919411
107.657490	4193.967188	22.924429
107.600092	4182.410079	22.929447
108.405890	4179.558604	22.934464
108.059377	4173.162708	22.939482
107.965725	4182.326955	22.944499
108.273677	4172.391146	22.949517
107.748573	4178.899476	22.954535
108.332021	4175.964828	22.959552
107.965710	4174.468157	22.964570
107.941363	4192.761620	22.969587
108.393607	4205.426196	22.974605
108.212919	4208.985719	22.979623
108.440715	4203.163979	22.984640
108.663475	4218.721452	22.989658
108.868164	4234.004009	22.994675
109.114071	4235.912012	22.999693
108.986813	4245.638904	23.004711
108.811155	4241.415090	23.009728
109.126477	4262.359030	23.014746
109.205743	4272.809800	23.019763
109.310044	4271.707376	23.024781
109.568652	4292.897365	23.029799
109.697137	4304.069058	23.034816
109.750689	4304.404081	23.039834
109.933435	4294.267552	23.044851
109.977832	4299.684316	23.049869
110.137434	4324.774308	23.054887
111.017703	4316.052477	23.059904
110.885745	4318.511234	23.064922
111.085188	4325.441234	23.069939
111.240647	4311.409840	23.074957
110.968232	4310.071911	23.079975
111.163948	4305.384299	23.084992
111.633881	4314.279513	23.090010
111.381233	4318.160146	23.095027
111.434020	4307.986027	23.100045
111.145747	4309.572903	23.105063
110.985036	4305.879730	23.110080
111.796011	4310.236470	23.115098
111.622405	4313.290722	23.120115
111.384517	4312.711657	23.125133
111.494335	4336.341282	23.130151
111.971864	4345.080837	23.135168
111.956279	4347.540915	23.140186
112.010239	4354.612436	23.145203
112.417072	4338.423935	23.150221
112.260936	4348.099132	23.155239
112.537248	4367.091073	23.160256
112.462370	4380.257300	23.165274
112.706020	4380.956699	23.170291
112.966943	4373.869801	23.175309
112.961739	4371.631481	23.180327
113.099940	4374.959943	23.185344
112.781662	4380.920151	23.190362
112.918718	4395.574118	23.195379
113.432184	4395.430182	23.200397
113.013168	4409.828210	23.205415
113.563109	4408.930560	23.210432
114.106455	4411.315305	23.215450
113.914646	4417.807549	23.220467
114.197131	4427.770697	23.225485
114.081952	4435.015387	23.230503
114.546780	4428.799283	23.235520
114.628854	4438.517974	23.240538
114.467884	4436.810432	23.245555
114.593887	4430.006558	23.250573
114.194036	4430.708373	23.255591
114.435284	4432.014662	23.260608
114.769720	4446.553712	23.265626
115.012462	4458.224975	23.270643
114.790199	4461.461664	23.275661
114.539754	4473.985429	23.280679
115.249710	4474.920732	23.285696
115.279529	4484.042720	23.290714
115.212983	4494.973887	23.295731
115.757021	4484.967480	23.300749
115.389802	4499.370099	23.305767
115.252677	4500.378949	23.310784
115.930360	4517.125241	23.315802
116.044729	4524.593690	23.320819
115.754309	4516.793135	23.325837
115.915473	4531.851877	23.330855
116.199759	4548.204091	23.335872
116.635151	4551.904601	23.340890
116.541444	4558.267453	23.345907
116.403594	4552.700454	23.350925
116.532229	4569.248715	23.355943
116.591894	4591.338824	23.360960
116.546364	4586.415239	23.365978
116.813793	4601.770885	23.370995
117.419813	4608.007498	23.376013
117.459098	4628.046989	23.381031
117.531994	4617.621119	23.386048
117.501376	4611.844319	23.391066
117.649021	4630.603439	23.396083
117.890041	4637.857257	23.401101
117.786435	4639.554281	23.406119
117.782202	4646.394892	23.411136
117.929364	4645.263827	23.416154
118.126360	4651.119260	23.421171
118.524288	4654.519038	23.426189
118.356430	4671.715267	23.431207
118.548666	4668.955506	23.436224
118.838129	4664.200521	23.441242
118.957825	4664.720336	23.446259
119.219511	4662.886751	23.451277
119.452487	4664.745828	23.456295
119.293149	4665.833322	23.461312
119.514894	4675.598314	23.466330
119.932235	4690.515622	23.471347
120.092803	4691.456120	23.476365
119.929051	4684.684483	23.481383
120.292267	4686.967828	23.486400
120.283607	4670.302808	23.491418
119.826968	4686.045739	23.496435
120.197579	4683.679148	23.501453
120.302154	4677.854730	23.506471
120.416334	4685.453248	23.511488
121.005096	4680.928137	23.516506
120.431341	4675.082172	23.521523
120.560983	4679.237615	23.526541
120.421703	4705.567214	23.531559
120.551083	4710.280362	23.536576
120.830032	4709.790685	23.541594
120.473226	4734.297995	23.546611
121.049046	4734.834134	23.551629
120.739135	4751.115929	23.556647
120.787845	4778.778412	23.561664
121.284777	4784.695896	23.566682
121.372936	4808.222031	23.571699
121.754939	4802.189327	23.576717
122.243658	4812.882169	23.581735
122.110554	4819.621286	23.586752
122.298175	4808.193424	23.591770
122.417280	4831.033759	23.596787
122.964247	4835.329577	23.601805
122.921001	4836.053765	23.606823
122.536527	4837.088499	23.611840
122.977902	4842.621704	23.616858
123.040584	4844.957382	23.621875
123.283665	4827.518100	23.626893
123.291548	4842.700296	23.631911
123.478615	4861.210335	23.636928
123.970530	4861.311902	23.641946
123.792631	4863.977895	23.646963
123.894002	4865.090022	23.651981
124.353062	4852.785408	23.656999
124.130963	4859.909208	23.662016
124.457344	4858.066874	23.667034
124.309972	4861.801202	23.672051
124.163313	4850.067509	23.677069
124.280642	4853.379171	23.682087
124.311720	4877.541377	23.687104
124.134576	4882.260654	23.692122
124.435943	4888.101432	23.697139
124.615002	4897.963672	23.702157
124.961395	4915.839968	23.707175
124.749378	4921.597061	23.712192
124.726483	4923.941121	23.717210
125.163556	4939.997381	23.722227
124.780375	4959.209426	23.727245
125.352216	4963.718409	23.732263
125.294138	4975.883501	23.737280
125.342861	4982.264637	23.742298
125.478601	4990.136074	23.747315
125.825260	4998.180085	23.752333
126.626676	5013.931361	23.757351
126.580860	5017.430134	23.762368
126.675543	5018.125171	23.767386
126.533465	5018.790694	23.772403
126.916041	5019.901884	23.777421
126.883500	5017.994250	23.782439
126.777921	5028.109371	23.787456
127.068790	5040.109932	23.792474
127.054940	5045.375467	23.797491
127.039485	5050.034779	23.802509
127.334568	5059.010015	23.807527
127.655446	5070.150841	23.812544
127.985925	5078.256742	23.817562
127.927568	5078.532201	23.822579
127.821062	5080.776405	23.827597
128.717488	5073.294330	23.832615
128.614708	5089.078604	23.837632
128.492299	5080.085589	23.842650
128.806242	5085.109054	23.847667
128.856851	5100.785126	23.852685
129.222997	5096.741518	23.857703
129.204553	5104.649683	23.862720
129.208117	5108.630725	23.867738
129.424126	5105.682501	23.872755
129.056937	5105.446936	23.877773
128.670999	5105.639925	23.882791
128.898050	5123.052501	23.887808
128.912298	5127.631916	23.892826
129.366231	5147.096874	23.897843
129.457035	5160.707156	23.902861
130.013384	5164.411495	23.907879
129.905802	5169.723859	23.912896
129.736142	5174.924778	23.917914
130.056947	5198.013835	23.922931
130.436919	5194.289202	23.927949
130.867786	5190.353413	23.932967
130.707715	5206.765944	23.937984
130.939615	5206.762433	23.943002
131.445615	5216.574337	23.948019
131.288204	5217.443353	23.953037
131.451137	5211.300758	23.958055
131.046274	5204.986908	23.963072
131.134515	5211.450369	23.968090
131.722192	5226.692647	23.973107
131.989257	5230.486766	23.978125
131.993559	5224.556462	23.983143
131.949087	5238.006474	23.988160
132.317329	5221.844173	23.993178
132.574635	5218.044467	23.998195
132.427516	5226.500914	24.003213
132.559193	5221.351411	24.008231
132.948031	5252.805753	24.013248
133.005650	5261.220820	24.018266
132.902017	5267.420245	24.023283
133.030946	5262.599659	24.028301
132.931028	5254.057964	24.033319
132.824645	5274.977080	24.038336
132.891796	5283.017954	24.043354
133.470466	5288.413569	24.048371
133.263573	5305.737689	24.053389
133.347220	5317.243881	24.058407
133.691530	5329.352076	24.063424
133.930490	5337.364312	24.068442
134.086160	5351.182611	24.073459
134.277308	5364.647475	24.078477
134.400403	5349.800743	24.083495
134.217884	5358.970663	24.088512
134.765186	5370.651040	24.093530
135.232978	5384.811274	24.098547
134.899999	5386.762734	24.103565
135.222183	5392.589104	24.108583
135.362549	5397.940957	24.113600
135.675954	5393.726725	24.118618
135.725366	5404.506309	24.123635
135.624421	5417.343100	24.128653
135.936569	5417.752755	24.133671
136.077153	5415.421555	24.138688
135.901159	5412.942980	24.143706
136.640425	5410.055445	24.148723
136.608551	5425.361590	24.153741
136.918008	5426.014313	24.158759
136.894138	5433.829838	24.163776
136.993402	5433.828586	24.168794
137.331858	5438.349361	24.173811
136.919349	5437.844296	24.178829
137.123603	5427.619077	24.183847
137.135745	5439.548785	24.188864
137.505461	5460.180942	24.193882
137.753454	5461.069480	24.198899
137.893430	5472.771712	24.203917
138.094019	5474.976718	24.208935
137.855127	5478.899381	24.213952
138.229872	5468.891453	24.218970
138.430362	5469.966938	24.223987
138.447709	5491.277873	24.229005
138.646828	5492.353595	24.234023
138.612240	5499.459712	24.239040
138.785140	5501.408745	24.244058
138.973584	5496.276203	24.249075
139.110374	5495.858924	24.254093
139.436644	5484.154750	24.259111
139.292069	5501.539291	24.264128
139.218692	5511.456216	24.269146
139.383162	5524.101084	24.274163
139.379513	5534.053330	24.279181
139.478677	5538.363097	24.284199
139.852552	5543.268522	24.289216
139.549157	5558.741071	24.294234
140.042742	5549.669758	24.299251
140.059974	5570.354608	24.304269
140.210414	5574.999814	24.309287
140.159727	5586.830914	24.314304
140.501220	5599.871634	24.319322
140.826779	5604.917693	24.324339
140.803239	5629.180201	24.329357
141.326089	5612.227730	24.334375
141.417452	5625.160902	24.339392
141.171766	5648.164984	24.344410
141.569747	5644.532471	24.349427
141.417403	5658.336099	24.354445
141.500537	5659.434867	24.359463
142.223539	5668.435552	24.364480
142.850332	5658.686771	24.369498
143.135289	5650.909897	24.374515
143.488471	5648.007376	24.379533
143.396722	5643.546671	24.384551
143.222522	5640.257219	24.389568
143.410056	5640.507076	24.394586
143.764926	5630.251181	24.399603
143.954322	5625.282274	24.404621
143.967400	5611.011843	24.409639
143.631618	5608.230588	24.414656
143.762413	5606.829723	24.419674
143.714470	5612.903157	24.424691
143.574893	5633.583464	24.429709
143.662054	5632.898210	24.434727
144.112844	5644.715853	24.439744
144.253014	5666.844858	24.444762
144.250798	5668.551390	24.449779
144.479422	5677.376106	24.454797
144.305919	5672.070824	24.459815
144.511715	5692.780222	24.464832
144.541142	5706.342417	24.469850
145.081030	5711.399030	24.474867
144.934310	5727.709771	24.479885
145.110521	5731.847268	24.484903
145.195794	5748.575123	24.489920
145.369330	5764.281189	24.494938
145.713191	5767.193444	24.499955
146.374608	5775.036595	24.504973
145.661840	5780.456847	24.509991
146.091603	5787.686715	24.515008
146.382064	5807.873684	24.520026
146.262845	5797.704469	24.525043
146.460005	5800.002268	24.530061
146.471919	5815.476151	24.535079
146.506461	5827.366075	24.540096
146.668343	5838.025846	24.545114
146.793066	5839.593268	24.550131
146.722087	5855.625701	24.555149
147.058208	5869.311115	24.560167
147.616113	5877.461148	24.565184
147.733510	5887.091175	24.570202
148.015321	5882.972819	24.575219
147.998343	5896.492718	24.580237
148.492038	5906.478881	24.585255
149.024090	5908.878403	24.590272
148.604253	5918.313822	24.595290
148.535576	5911.510394	24.600307
148.319061	5920.200450	24.605325
148.532662	5937.086100	24.610343
148.876501	5948.837232	24.615360
148.490580	5962.687467	24.620378
149.080590	5969.530753	24.625395
148.928567	5984.438185	24.630413
149.073607	5994.878027	24.635431
149.474787	6006.253088	24.640448
149.482260	6016.304556	24.645466
149.934666	6027.775616	24.650483
150.259245	6039.771157	24.655501
149.860591	6048.924959	24.660519
150.577651	6068.104902	24.665536
150.289107	6073.838505	24.670554
150.539786	6074.843988	24.675571
151.182032	6092.735487	24.680589
151.115151	6094.081350	24.685607
151.884388	6098.170846	24.690624
151.644666	6093.249363	24.695642
152.132580	6088.986131	24.700659
152.282315	6084.321636	24.705677
152.616408	6080.948108	24.710695
152.890875	6075.498153	24.715712
152.508139	6079.712655	24.720730
153.053698	6067.741239	24.725747
152.967722	6072.595690	24.730765
152.792353	6078.577715	24.735783
153.380625	6087.277989	24.740800
153.337170	6103.657272	24.745818
153.113468	6097.645209	24.750835
153.379868	6098.342366	24.755853
153.172491	6100.693805	24.760871
153.799962	6112.843070	24.765888
153.753273	6125.008662	24.770906
154.200338	6128.119915	24.775923
153.913040	6143.630442	24.780941
154.353076	6139.483322	24.785959
154.221930	6133.624737	24.790976
154.033439	6157.568157	24.795994
154.083065	6167.392721	24.801011
154.133512	6173.733080	24.806029
154.085554	6195.497273	24.811047
154.315525	6210.617495	24.816064
154.372671	6220.399842	24.821082
154.666940	6233.242008	24.826099
155.207510	6256.662797	24.831117
155.295713	6268.159443	24.836135
155.838746	6262.907579	24.841152
155.808143	6289.396827	24.846170
156.038255	6297.591455	24.851187
156.428924	6293.737126	24.856205
156.486642	6305.213030	24.861223
156.529940	6303.838920	24.866240
156.554948	6314.345236	24.871258
156.839176	6323.857916	24.876275
157.572290	6330.431059	24.881293
157.749190	6330.027364	24.886311
157.918052	6317.177434	24.891328
157.854724	6313.296160	24.896346
157.989040	6309.934775	24.901363
158.129658	6316.853676	24.906381
158.430490	6327.754631	24.911399
158.311588	6324.767496	24.916416
158.185393	6341.784296	24.921434
158.326251	6342.741667	24.926451
158.576804	6351.311715	24.931469
158.222397	6362.474686	24.936487
158.883793	6364.028146	24.941504
158.535519	6377.569797	24.946522
158.585490	6397.746751	24.951539
159.266729	6402.817169	24.956557
159.300817	6414.919507	24.961575
159.775857	6425.878104	24.966592
159.718734	6444.256184	24.971610
159.832670	6445.870417	24.976627
160.214208	6449.947696	24.981645
160.114906	6456.437512	24.986663
160.716167	6456.369900	24.991680
160.994537	6461.176977	24.996698
160.982683	6455.579044	25.001715
161.086537	6461.756755	25.006733
161.557550	6476.424714	25.011751
161.954866	6476.750482	25.016768
161.882839	6486.527564	25.021786
162.068032	6476.283675	25.026803
162.586293	6463.504494	25.031821
162.294852	6464.962142	25.036839
162.944425	6461.265838	25.041856
163.034005	6464.126499	25.046874
163.125503	6456.727426	25.051891
163.489049	6453.534676	25.056909
163.435864	6447.395571	25.061927
163.485990	6430.561872	25.066944
163.233600	6420.662434	25.071962
163.366003	6424.522464	25.076979
163.895480	6432.813150	25.081997
163.593970	6441.688208	25.087015
163.779480	6444.078688	25.092032
163.619269	6449.945608	25.097050
163.971558	6452.138138	25.102067
164.212390	6453.221744	25.107085
163.975818	6467.006637	25.112103
164.693192	6477.006808	25.117120
164.693209	6478.846959	25.122138
165.005625	6486.608503	25.127155
164.926747	6477.819921	25.132173
164.788671	6508.673085	25.137191
164.484480	6517.610088	25.142208
164.782770	6523.907312	25.147226
164.735444	6539.112406	25.152243
165.181096	6558.321353	25.157261
164.994417	6577.423669	25.162279
165.265059	6595.388104	25.167296
165.596213	6617.296633	25.172314
165.543632	6636.305922	25.177331
166.005936	6653.955557	25.182349
165.782210	6674.019079	25.187367
166.326249	6690.320309	25.192384
166.272359	6705.236009	25.197402
166.496652	6731.383739	25.202419
166.980761	6739.347571	25.207437
167.133808	6759.747575	25.212455
167.160869	6758.991439	25.217472
167.628444	6786.412302	25.222490
167.785875	6787.537800	25.227507
168.086048	6800.425103	25.232525
168.175886	6820.489410	25.237543
168.540757	6815.627912	25.242560
169.203576	6813.807251	25.247578
169.246940	6814.575761	25.252595
169.702804	6836.400980	25.257613
169.340192	6846.049277	25.262631
169.194190	6844.449977	25.267648
169.461741	6839.604367	25.272666
169.511279	6851.968284	25.277683
169.972760	6856.967813	25.282701
169.885526	6876.508756	25.287719
170.183840	6874.947512	25.292736
170.435222	6875.731570	25.297754
170.302509	6898.933140	25.302771
171.137694	6896.466900	25.307789
170.808333	6900.665374	25.312807
171.017099	6892.939562	25.317824
171.159766	6917.878211	25.322842
171.215476	6916.894223	25.327859
171.659142	6918.029745	25.332877
171.779875	6935.744547	25.337895
171.880693	6943.495323	25.342912
171.953127	6960.347963	25.347930
172.116471	6956.199227	25.352947
172.183087	6960.440122	25.357965
172.464218	6978.202313	25.362983
172.539320	6981.579166	25.368000
172.588139	6987.038628	25.373018
172.218859	7002.621545	25.378035
172.388708	7008.766097	25.383053
172.733529	7028.379685	25.388071
172.928069	7042.691440	25.393088
173.272559	7057.690427	25.398106
173.543069	7075.716870	25.403123
174.174408	7080.203667	25.408141
173.725414	7093.102254	25.413159
173.955847	7105.646478	25.418176
174.866122	7104.895688	25.423194
174.856695	7110.491218	25.428211
175.205659	7114.880695	25.433229
175.647721	7137.652432	25.438247
175.691541	7139.332324	25.443264
176.048187	7125.687787	25.448282
176.235408	7132.703827	25.453299
176.258502	7130.124681	25.458317
176.155627	7130.979721	25.463335
176.548623	7123.670454	25.468352
176.882318	7121.773049	25.473370
176.409623	7125.154820	25.478387
176.942957	7125.584118	25.483405
176.846530	7149.133536	25.488423
177.051434	7153.347626	25.493440
177.412637	7150.552964	25.498458
176.989652	7160.813650	25.503475
177.105673	7178.797369	25.508493
177.271573	7186.296049	25.513511
177.449309	7194.251972	25.518528
177.892441	7201.180058	25.523546
177.886563	7216.429895	25.528563
178.483502	7231.003702	25.533581
178.465469	7241.322640	25.538599
178.740661	7244.590411	25.543616
179.341946	7246.026651	25.548634
179.345409	7252.722111	25.553651
180.091322	7253.324520	25.558669
180.353303	7256.944329	25.563687
180.273597	7256.434925	25.568704
180.521541	7247.578079	25.573722
180.245375	7246.795911	25.578739
180.426173	7250.756559	25.583757
180.359404	7262.152080	25.588775
180.277740	7260.292773	25.593792
180.595494	7273.923464	25.598810
180.392839	7294.178729	25.603827
180.529332	7297.779881	25.608845
181.050545	7310.837678	25.613863
181.749949	7298.597921	25.618880
182.285577	7290.459026	25.623898
182.009992	7307.823872	25.628915
182.279783	7294.175963	25.633933
182.652202	7297.434168	25.638951
182.743901	7293.582800	25.643968
183.016548	7295.280990	25.648986
182.793305	7305.944741	25.654003
182.955767	7316.421063	25.659021
183.023709	7330.813075	25.664039
183.257827	7333.155970	25.669056
183.914532	7317.495915	25.674074
183.635116	7320.189954	25.679092
183.874818	7316.950518	25.684109
184.195072	7332.721998	25.689127
184.317402	7348.191829	25.694144
184.732032	7340.436815	25.699162
184.763434	7339.345104	25.704180
184.813752	7351.174375	25.709197
185.049409	7340.153993	25.714215
184.929026	7369.126939	25.719232
185.165233	7369.908110	25.724250
185.185702	7372.427859	25.729268
185.258742	7378.297672	25.734285
185.611033	7394.629344	25.739303
185.388485	7414.150024	25.744320
185.691660	7420.298665	25.749338
185.691546	7444.088034	25.754356
186.105413	7456.047281	25.759373
186.026916	7477.051941	25.764391
185.953992	7490.733244	25.769408
186.057308	7509.904337	25.774426
186.595388	7531.337491	25.779444
186.489212	7545.341229	25.784461
186.973382	7573.130859	25.789479
187.068008	7585.638868	25.794496
187.248558	7595.585244	25.799514
188.123452	7608.886744	25.804532
188.474930	7628.539317	25.809549
188.727913	7638.134555	25.814567
188.684380	7636.550696	25.819584
189.205020	7632.762006	25.824602
189.205853	7648.240349	25.829620
189.490499	7664.401125	25.834637
189.875045	7666.741130	25.839655
189.594527	7670.450877	25.844672
189.861102	7672.569253	25.849690
189.990767	7684.609688	25.854708
190.527941	7676.727156	25.859725
191.574747	7676.041964	25.864743
191.864893	7673.319267	25.869760
191.840738	7665.083922	25.874778
191.717096	7652.607633	25.879796
191.819715	7639.575779	25.884813
191.975130	7631.474317	25.889831
191.691736	7633.619213	25.894848
191.551809	7640.540301	25.899866
192.181379	7668.120042	25.904884
191.892698	7665.480024	25.909901
192.216400	7669.651830	25.914919
191.475504	7681.094668	25.919936
192.155944	7698.772668	25.924954
192.195294	7703.233502	25.929972
192.003403	7734.669398	25.934989
192.313351	7754.563220	25.940007
192.479244	7779.848224	25.945024
192.752918	7788.491499	25.950042
193.334768	7810.493405	25.955060
193.417645	7824.814761	25.960077
193.536552	7831.886935	25.965095
193.630421	7852.106253	25.970112
193.791168	7857.520040	25.975130
194.568502	7889.142240	25.980148
194.061655	7909.009254	25.985165
194.648006	7914.601413	25.990183
194.440545	7950.750669	25.995200
194.773487	7950.848019	26.000218
195.049093	7969.684459	26.005236
195.263139	7994.466017	26.010253
195.672008	8002.998787	26.015271
195.521753	8020.925105	26.020288
195.839657	8027.655222	26.025306
196.497062	8044.436301	26.030324
196.539201	8056.188713	26.035341
197.175233	8059.133246	26.040359
197.187577	8078.123660	26.045376
197.657632	8081.125010	26.050394
197.840679	8091.463596	26.055412
198.197180	8084.665140	26.060429
198.327408	8082.746569	26.065447
198.432576	8090.488489	26.070464
198.618445	8105.989125	26.075482
198.838456	8113.424606	26.080500
198.541767	8112.823168	26.085517
199.042193	8110.597701	26.090535
199.147449	8127.804397	26.095552
199.578112	8142.995252	26.100570
199.958804	8142.733053	26.105588
199.936381	8145.785747	26.110605
200.162868	8155.567822	26.115623
200.040437	8178.353511	26.120640
199.963758	8176.603537	26.125658
200.476157	8191.432212	26.130676
200.274141	8208.445080	26.135693
200.551872	8213.839722	26.140711
200.322996	8242.280578	26.145728
200.707516	8247.897999	26.150746
201.041906	8271.890445	26.155764
201.239108	8281.900569	26.160781
201.540757	8304.000029	26.165799
202.015604	8324.229477	26.170816
201.991309	8328.838476	26.175834
202.640231	8342.354223	26.180852
202.598042	8345.446583	26.185869
203.200620	8340.732962	26.190887
203.180083	8353.723763	26.195904
203.219484	8363.070067	26.200922
203.410036	8367.485471	26.205940
203.541225	8367.635529	26.210957
204.247306	8369.891374	26.215975
204.713928	8391.718450	26.220992
204.688507	8386.197012	26.226010
204.929303	8380.866290	26.231028
204.809526	8385.712263	26.236045
205.202252	8380.669840	26.241063
205.390108	8391.413525	26.246080
205.408090	8410.340338	26.251098
205.381148	8426.158229	26.256116
205.275471	8431.071915	26.261133
205.372660	8441.313572	26.266151
205.680287	8454.686235	26.271168
205.885933	8472.704099	26.276186
206.046106	8493.242958	26.281204
206.211256	8503.041274	26.286221
206.441482	8512.609423	26.291239
206.764549	8527.384203	26.296256
207.054403	8543.697025	26.301274
207.428468	8552.382592	26.306292
208.025384	8575.948392	26.311309
207.933705	8579.324234	26.316327
208.329146	8587.294741	26.321344
208.233728	8583.380601	26.326362
208.751425	8600.777877	26.331380
208.785059	8609.907082	26.336397
209.114401	8613.261972	26.341415
209.413917	8618.140135	26.346432
209.559593	8627.379350	26.351450
210.085625	8625.435412	26.356468
209.571691	8630.378960	26.361485
210.130577	8640.237497	26.366503
210.369285	8652.957992	26.371520
210.422297	8662.318681	26.376538
210.489977	8656.332911	26.381556
210.490833	8685.054242	26.386573
210.645715	8699.060715	26.391591
210.924727	8714.697239	26.396608
211.213792	8727.259470	26.401626
211.280504	8734.417410	26.406644
211.445055	8759.527707	26.411661
211.754390	8771.928930	26.416679
211.631904	8793.508519	26.421696
211.875309	8813.030591	26.426714
212.292082	8812.527423	26.431732
212.391501	8842.431240	26.436749
212.875037	8852.743232	26.441767
213.311569	8874.770721	26.446784
213.378990	8884.534811	26.451802
213.307484	8895.572252	26.456820
213.619994	8908.288175	26.461837
213.793622	8923.006998	26.466855
213.985120	8928.087342	26.471872
213.952709	8949.309771	26.476890
214.570956	8945.871191	26.481908
214.345607	8971.820748	26.486925
214.822773	8981.875498	26.491943
215.375598	9003.824929	26.496960
215.255442	9017.231206	26.501978
215.899940	9005.855981	26.506996
216.049900	9032.447221	26.512013
216.720302	9037.814226	26.517031
217.242301	9038.975878	26.522048
217.275532	9037.361389	26.527066
217.794769	9031.032571	26.532084
217.742479	9041.904519	26.537101
217.875071	9039.626956	26.542119
217.923392	9028.905406	26.547136
217.864788	9046.944786	26.552154
218.065198	9055.964507	26.557172
217.788031	9072.601175	26.562189
218.158193	9089.475134	26.567207
218.148141	9097.295590	26.572224
218.430295	9124.026621	26.577242
218.707235	9135.144736	26.582260
218.851798	9160.318961	26.587277
219.071917	9169.551241	26.592295
219.028014	9191.069042	26.597312
219.373332	9209.278876	26.602330
219.535192	9221.683665	26.607348
219.893002	9244.002482	26.612365
220.354345	9260.619903	26.617383
220.809110	9265.929405	26.622400
220.754304	9293.889248	26.627418
220.887207	9303.302008	26.632436
220.933922	9317.409498	26.637453
220.996737	9329.199474	26.642471
221.293611	9352.190698	26.647488
221.680126	9372.613880	26.652506
221.902718	9388.982421	26.657524
221.669987	9410.266579	26.662541
222.023397	9432.701441	26.667559
222.475193	9454.355229	26.672576
222.494320	9471.072304	26.677594
222.711036	9488.348013	26.682612
223.418375	9504.496489	26.687629
223.242709	9530.335999	26.692647
223.999817	9543.225186	26.697664
224.308699	9568.827275	26.702682
224.732369	9569.118668	26.707700
224.505020	9588.322126	26.712717
224.764709	9599.519156	26.717735
224.841697	9601.193620	26.722752
225.244649	9620.240226	26.727770
225.241626	9637.886248	26.732788
225.781270	9641.947496	26.737805
225.920488	9656.994345	26.742823
226.195911	9673.469149	26.747840
226.311263	9679.725706	26.752858
226.499026	9692.406905	26.757876
226.558455	9708.849435	26.762893
227.245750	9713.800920	26.767911
227.884707	9718.729178	26.772928
228.737307	9697.505420	26.777946
229.040455	9699.334949	26.782964
229.274762	9694.769162	26.787981
229.121538	9697.316684	26.792999
229.291723	9695.042041	26.798016
229.799743	9703.205750	26.803034
229.820913	9687.395502	26.808052
229.814352	9706.561255	26.813069
229.693543	9700.946990	26.818087
230.041978	9692.871292	26.823104
230.238425	9701.359440	26.828122
230.475779	9706.577142	26.833140
230.434192	9731.621860	26.838157
231.133808	9732.965852	26.843175
230.972550	9730.086188	26.848192
230.748679	9741.607299	26.853210
230.847576	9757.764201	26.858228
231.020664	9779.409471	26.863245
230.865458	9804.952816	26.868263
230.885885	9813.463316	26.873280
231.074436	9838.235532	26.878298
231.593931	9865.655123	26.883316
231.496755	9885.660761	26.888333
231.512619	9914.203636	26.893351
232.298607	9939.382584	26.898368
232.240390	9976.827368	26.903386
232.742206	10000.323310	26.908404
232.887093	10023.106745	26.913421
233.086371	10046.668795	26.918439
233.568508	10064.150178	26.923456
233.693962	10093.022836	26.928474
234.272387	10105.237138	26.933492
234.647227	10128.677817	26.938509
234.728004	10143.497186	26.943527
235.219008	10159.710192	26.948544
235.386209	10172.365350	26.953562
236.275319	10180.668837	26.958580
236.655481	10186.615461	26.963597
236.404806	10197.303148	26.968615
236.929815	10203.275376	26.973632
237.302000	10211.872343	26.978650
237.769373	10216.866411	26.983668
238.222963	10212.031248	26.988685
238.125708	10211.033097	26.993703
238.464437	10204.093408	26.998720
238.508869	10212.869469	27.003738
238.777156	10202.273327	27.008756
238.879061	10207.801209	27.013773
238.913505	10231.231048	27.018791
239.463561	10234.301043	27.023808
239.030145	10235.179020	27.028826
239.190371	10244.170049	27.033844
239.421875	10255.870329	27.038861
239.581659	10263.452650	27.043879
239.557922	10287.366868	27.048896
239.407433	10308.792538	27.053914
239.669137	10328.489799	27.058932
239.748823	10333.446351	27.063949
240.082305	10372.697005	27.068967
240.670434	10399.198051	27.073984
241.179869	10417.909025	27.079002
241.573648	10435.396500	27.084020
241.887004	10438.592204	27.089037
242.461779	10465.658226	27.094055
242.320960	10463.310717	27.099072
242.442682	10480.250776	27.104090
243.066601	10496.372000	27.109108
243.260644	10492.047697	27.114125
243.353039	10514.388550	27.119143
244.063939	10516.635222	27.124160
244.012593	10525.587032	27.129178
244.495159	10534.147916	27.134196
244.789216	10540.035365	27.139213
244.902484	10544.029679	27.144231
245.212098	10550.825312	27.149248
245.157887	10554.678142	27.154266
245.633593	10571.718360	27.159284
245.853792	10579.923972	27.164301
245.753110	10584.432455	27.169319
246.028074	10598.453084	27.174336
246.391998	10605.518360	27.179354
246.998912	10624.389363	27.184372
246.872253	10635.777828	27.189389
246.955529	10649.059182	27.194407
247.269591	10666.399832	27.199424
247.695983	10682.012999	27.204442
247.941184	10685.138489	27.209460
248.282552	10694.547844	27.214477
248.057436	10706.641892	27.219495
248.503741	10720.885399	27.224512
248.639432	10739.386606	27.229530
248.505490	10747.249579	27.234548
248.932629	10770.374926	27.239565
248.967603	10793.487155	27.244583
249.197028	10816.518811	27.249600
249.163814	10837.512192	27.254618
249.546789	10857.320108	27.259636
250.145047	10869.005243	27.264653
250.423509	10894.537424	27.269671
250.314509	10908.444483	27.274688
250.810981	10922.682720	27.279706
250.817399	10941.704299	27.284724
251.543976	10952.726109	27.289741
251.635545	10971.046034	27.294759
251.867808	10983.703281	27.299776
252.373515	11000.275492	27.304794
252.280799	11012.227303	27.309812
253.006137	11021.935068	27.314829
252.812708	11042.327387	27.319847
253.464547	11058.764297	27.324864
254.078724	11066.190314	27.329882
254.142823	11071.736002	27.334900
254.225627	11089.578486	27.339917
254.561433	11097.034896	27.344935
254.814001	11103.413467	27.349952
254.709676	11123.672422	27.354970
255.095356	11123.242290	27.359988
255.785915	11139.743562	27.365005
255.853020	11164.894777	27.370023
255.413957	11168.823173	27.375040
255.829852	11188.854360	27.380058
255.902091	11211.825266	27.385076
256.397380	11217.481479	27.390093
256.447854	11243.672626	27.395111
256.970022	11263.483969	27.400128
257.132437	11287.905141	27.405146
257.411455	11305.893886	27.410164
257.774740	11325.805032	27.415181
257.587832	11342.548316	27.420199
257.818926	11365.310977	27.425216
257.842921	11384.262293	27.430234
258.116305	11413.509078	27.435252
259.259037	11421.079478	27.440269
259.635404	11441.975066	27.445287
260.203114	11459.520510	27.450304
260.626433	11458.880622	27.455322
260.430728	11472.468922	27.460340
260.819740	11472.449535	27.465357
261.182258	11487.612673	27.470375
261.554148	11492.577805	27.475392
261.843561	11499.627877	27.480410
262.024901	11507.063674	27.485428
262.808922	11503.602464	27.490445
263.388289	11490.381789	27.495463
263.995685	11473.415013	27.500480
263.975064	11479.326799	27.505498
264.284245	11477.551302	27.510516
264.154936	11464.616016	27.515533
264.390929	11470.209599	27.520551
264.649595	11475.692133	27.525568
264.845154	11468.787482	27.530586
264.573861	11467.771805	27.535604
264.681769	11480.868382	27.540621
264.995268	11505.673732	27.545639
264.877546	11509.422629	27.550656
265.323406	11518.967421	27.555674
265.460258	11546.293119	27.560692
265.423130	11548.092935	27.565709
265.620849	11572.798460	27.570727
265.815238	11589.270191	27.575744
265.984975	11599.410793	27.580762
266.375808	11624.652219	27.585780
266.555696	11640.694673	27.590797
266.651809	11661.424248	27.595815
266.914890	11673.662271	27.600832
267.288584	11695.594056	27.605850
267.128532	11728.275671	27.610868
267.707843	11745.723303	27.615885
267.938665	11769.879740	27.620903
267.963203	11806.252334	27.625920
268.599801	11826.829591	27.630938
268.653064	11845.601492	27.635956
269.283258	11852.686291	27.640973
269.261176	11883.850532	27.645991
269.711029	11916.327121	27.651008
269.753753	11936.506718	27.656026
270.185222	11962.756642	27.661044
270.661526	11972.280723	27.666061
270.793168	12003.666276	27.671079
271.089259	12026.064118	27.676096
271.431252	12048.999422	27.681114
271.406378	12077.515245	27.686132
271.779759	12084.735572	27.691149
272.376617	12114.345813	27.696167
272.284971	12134.421028	27.701184
272.906243	12165.924698	27.706202
273.168769	12190.221316	27.711220
273.407594	12204.504840	27.716237
273.649082	12226.274028	27.721255
273.860109	12239.793248	27.726272
274.330436	12269.589364	27.731290
274.280140	12283.977675	27.736308
274.563286	12309.517573	27.741325
274.953791	12326.167621	27.746343
275.320493	12358.883137	27.751360
275.876686	12366.756256	27.756378
276.489418	12384.978984	27.761396
276.935499	12388.956108	27.766413
277.191867	12393.150147	27.771431
277.365507	12414.677472	27.776448
277.837383	12419.419291	27.781466
277.964336	12438.398311	27.786484
278.095619	12447.775346	27.791501
277.954219	12462.103778	27.796519
278.268613	12476.951421	27.801536
278.163744	12485.694406	27.806554
278.289104	12517.808579	27.811572
278.683511	12536.721382	27.816589
278.745096	12564.972641	27.821607
279.063021	12584.073550	27.826624
279.588044	12602.549539	27.831642
280.218548	12625.229737	27.836660
279.842086	12640.145506	27.841677
280.562248	12657.237424	27.846695
281.133018	12671.855326	27.851712
282.132622	12674.894454	27.856730
282.197200	12671.568931	27.861748
282.947401	12681.727343	27.866765
282.899762	12672.244450	27.871783
283.166569	12681.117690	27.876800
283.329520	12688.925978	27.881818
283.388382	12700.823095	27.886836
283.753345	12705.316968	27.891853
283.844989	12706.111372	27.896871
284.351529	12720.128812	27.901888
284.672580	12727.150354	27.906906
284.996029	12728.458229	27.911924
285.430349	12733.967821	27.916941
285.829887	12756.493933	27.921959
285.635673	12768.581051	27.926976
286.193359	12759.361581	27.931994
286.498594	12780.269500	27.937012
286.197751	12794.209465	27.942029
286.550837	12795.104062	27.947047
286.354432	12816.110616	27.952064
286.800120	12830.485318	27.957082
286.631882	12858.101911	27.962100
286.717569	12876.245306	27.967117
287.295320	12899.362047	27.972135
287.409676	12921.114547	27.977152
288.284548	12939.727967	27.982170
288.212037	12978.168714	27.987188
288.826715	12991.589426	27.992205
288.938159	13008.475556	27.997223
289.275387	13039.808943	28.002240
289.664250	13048.437657	28.007258
289.841861	13072.289916	28.012276
290.066525	13092.704538	28.017293
290.788302	13115.897770	28.022311
290.525160	13137.195142	28.027328
291.042079	13159.843540	28.032346
291.290099	13194.641047	28.037364
291.411287	13211.809417	28.042381
291.810972	13237.975421	28.047399
291.587124	13259.904545	28.052416
292.273349	13280.484590	28.057434
292.693835	13297.701046	28.062452
292.291422	13335.893404	28.067469
293.225963	13365.917720	28.072487
293.097531	13397.226000	28.077504
293.789362	13417.803680	28.082522
293.877462	13430.375628	28.087540
294.313399	13458.116637	28.092557
294.832956	13483.827472	28.097575
294.800956	13512.416357	28.102592
295.390338	13522.434214	28.107610
295.649927	13546.435453	28.112628
295.901425	13553.089420	28.117645
296.917752	13569.972344	28.122663
296.955983	13580.650540	28.127680
297.367007	13601.659585	28.132698
297.409451	13605.313731	28.137716
297.737528	13623.972789	28.142733
298.100169	13635.712914	28.147751
298.137587	13648.903689	28.152768
298.844729	13663.757597	28.157786
298.771046	13676.122615	28.162804
299.355521	13703.037888	28.167821
299.832901	13704.336800	28.172839
300.195754	13730.167874	28.177856
299.914021	13741.522024	28.182874
300.141568	13752.628125	28.187892
300.200089	13775.135276	28.192909
300.366941	13800.744715	28.197927
300.552027	13828.655438	28.202944
300.648088	13850.617205	28.207962
301.306812	13879.953662	28.212980
301.347872	13915.952964	28.217997
301.849642	13933.439869	28.223015
301.721792	13965.778378	28.228032
302.246852	13984.148740	28.233050
303.137138	14005.132901	28.238068
303.420938	14040.802428	28.243085
304.109746	14056.263518	28.248103
304.596121	14081.084119	28.253120
304.932469	14093.634517	28.258138
305.286758	14102.049045	28.263156
305.343783	14116.582911	28.268173
305.693797	14117.873740	28.273191
305.922142	14141.066304	28.278208
306.304030	14135.356469	28.283226
307.052906	14153.288305	28.288244
307.016611	14173.818348	28.293261
307.494091	14180.920888	28.298279
307.515133	14201.961289	28.303296
307.836105	14211.891595	28.308314
308.043141	14228.163631	28.313332
308.247269	14252.523749	28.318349
308.836058	14262.871593	28.323367
308.914429	14276.594918	28.328384
309.531364	14299.196222	28.333402
309.360518	14314.890012	28.338420
309.148932	14339.173343	28.343437
309.821350	14349.254712	28.348455
309.726832	14384.858996	28.353472
310.200805	14409.929687	28.358490
310.648958	14430.750586	28.363508
310.475876	14460.712972	28.368525
311.234654	14476.955315	28.373543
311.507829	14504.098641	28.378560
311.900530	14529.399388	28.383578
312.183045	14540.151402	28.388596
312.130157	14568.856032	28.393613
312.924500	14589.162261	28.398631
312.602702	14620.217545	28.403648
312.787002	14631.895950	28.408666
313.423984	14660.797751	28.413684
313.776781	14691.988174	28.418701
313.996956	14706.130481	28.423719
314.211113	14738.675117	28.428736
314.864346	14768.091336	28.433754
315.054979	14783.461954	28.438772
315.496661	14810.107174	28.443789
316.127351	14826.951884	28.448807
316.188349	14857.558970	28.453824
316.092466	14881.623077	28.458842
317.134166	14905.225857	28.463860
317.377389	14935.511820	28.468877
317.639805	14945.681166	28.473895
318.113784	14978.299964	28.478912
318.069630	14993.610136	28.483930
318.474187	15012.334897	28.488948
319.358220	15040.364317	28.493965
320.112694	15040.142018	28.498983
319.945310	15056.816369	28.504000
319.848364	15068.242213	28.509018
320.840054	15081.700908	28.514036
320.645918	15100.974471	28.519053
321.096514	15112.375860	28.524071
321.411595	15124.388441	28.529088
321.328258	15153.288458	28.534106
321.999685	15173.427319	28.539124
321.576014	15195.390100	28.544141
322.270051	15228.171866	28.549159
322.247551	15247.165549	28.554176
322.484535	15273.310653	28.559194
323.105753	15297.345462	28.564212
322.956829	15338.224438	28.569229
323.655002	15368.269281	28.574247
323.864233	15393.412060	28.579264
324.094586	15423.366940	28.584282
324.799574	15447.415983	28.589300
324.950480	15478.339834	28.594317
325.807966	15501.506871	28.599335
325.989977	15515.235528	28.604352
326.326620	15539.571676	28.609370
326.876179	15565.919036	28.614388
327.202141	15599.076737	28.619405
327.155188	15611.262065	28.624423
327.641485	15626.381020	28.629440
327.794197	15648.171523	28.634458
328.124690	15674.627537	28.639476
328.269635	15704.663769	28.644493
328.544451	15726.485467	28.649511
328.612343	15748.416747	28.654528
329.133650	15772.444148	28.659546
329.338137	15801.103644	28.664564
329.399504	15829.882300	28.669581
330.102885	15859.761624	28.674599
329.989581	15884.601014	28.679616
330.173613	15923.286801	28.684634
330.779289	15943.221907	28.689652
331.218002	15986.274896	28.694669
331.637390	16004.668775	28.699687
331.920627	16042.231215	28.704704
332.361742	16069.966266	28.709722
333.075024	16085.823898	28.714740
333.331853	16115.220597	28.719757
333.791659	16137.372125	28.724775
334.521095	16157.735550	28.729792
334.913196	16169.303758	28.734810
335.587327	16180.309730	28.739828
335.511676	16189.711749	28.744845
335.824140	16199.168638	28.749863
336.033189	16216.128017	28.754880
335.848567	16239.529867	28.759898
336.718383	16246.022202	28.764916
336.744675	16275.285291	28.769933
337.377716	16292.853091	28.774951
337.278647	16319.648590	28.779968
337.422408	16353.412837	28.784986
337.864033	16378.796303	28.790004
337.908923	16408.054860	28.795021
338.121717	16430.069400	28.800039
338.767741	16462.710500	28.805056
339.007862	16499.188898	28.810074
339.330934	16531.322696	28.815092
339.509810	16564.551670	28.820109
339.662172	16597.613422	28.825127
340.040227	16629.842032	28.830144
340.456057	16668.548151	28.835162
340.865490	16703.661152	28.840180
341.424633	16737.012894	28.845197
341.956298	16760.135065	28.850215
342.770645	16786.848860	28.855232
342.520205	16809.753592	28.860250
343.256486	16821.726746	28.865268
344.163843	16849.838788	28.870285
344.558912	16860.465820	28.875303
345.260134	16877.228017	28.880320
345.079821	16883.200632	28.885338
345.656470	16900.614789	28.890356
345.587276	16921.198002	28.895373
345.949978	16935.248417	28.900391
346.372032	16949.339119	28.905408
346.546516	16984.753097	28.910426
346.514705	16995.439188	28.915444
346.943610	17022.684483	28.920461
346.831685	17049.261071	28.925479
347.334428	17063.724279	28.930496
347.284864	17102.429189	28.935514
347.788969	17132.119517	28.940532
347.793183	17163.301803	28.945549
348.284390	17199.570013	28.950567
348.888437	17220.634128	28.955584
349.038809	17274.496312	28.960602
349.326533	17300.667433	28.965620
349.762478	17334.865997	28.970637
349.751868	17360.495575	28.975655
350.271947	17384.724156	28.980672
350.652834	17427.428180	28.985690
351.361913	17447.694204	28.990708
351.366453	17482.865623	28.995725
352.002116	17516.398145	29.000743
352.759887	17540.059656	29.005760
353.049972	17568.906161	29.010778
353.531321	17581.232557	29.015796
354.317060	17601.911294	29.020813
354.260595	17624.656195	29.025831
355.283389	17631.483892	29.030848
355.241598	17661.451597	29.035866
355.846212	17666.487508	29.040884
356.484893	17693.551327	29.045901
356.411617	17708.788576	29.050919
357.194296	17715.072562	29.055936
357.496797	17719.996307	29.060954
358.230287	17725.891438	29.065972
358.859417	17748.709771	29.070989
358.921375	17754.360548	29.076007
359.421107	17747.666026	29.081024
359.013466	17758.169496	29.086042
359.376114	17767.383772	29.091060
359.920380	17789.272351	29.096077
359.931275	17813.536795	29.101095
360.207892	17817.022458	29.106112
360.598348	17841.261306	29.111130
361.126639	17863.986720	29.116148
361.426733	17881.852899	29.121165
361.578176	17904.816374	29.126183
362.035729	17928.260298	29.131200
362.006798	17958.114393	29.136218
362.657437	17979.582966	29.141236
362.715428	17996.210585	29.146253
362.733928	18035.850351	29.151271
363.115907	18055.812139	29.156288
363.531034	18095.193305	29.161306
363.674322	18126.351970	29.166324
364.501701	18163.263084	29.171341
364.236997	18195.885502	29.176359
364.627939	18232.852647	29.181376
364.777847	18265.670588	29.186394
365.244457	18302.462529	29.191412
365.960191	18334.672815	29.196429
366.422028	18378.380721	29.201447
366.476024	18398.982472	29.206464
366.730692	18429.496697	29.211482
366.792605	18461.477154	29.216500
366.971375	18495.236565	29.221517
367.170878	18540.170736	29.226535
367.821650	18577.641197	29.231552
368.116704	18629.740762	29.236570
368.835780	18666.833938	29.241588
369.347348	18703.891810	29.246605
369.445964	18747.667653	29.251623
369.983384	18772.937434	29.256640
369.743050	18820.657983	29.261658
370.087835	18863.857455	29.266676
370.689858	18899.638934	29.271693
371.555651	18929.795490	29.276711
372.976208	18943.645803	29.281728
373.324989	18971.835076	29.286746
374.079638	18992.049443	29.291764
374.924207	18995.789615	29.296781
375.019772	19005.129179	29.301799
375.592849	19018.828383	29.306816
375.939332	19031.456457	29.311834
376.117846	19040.482259	29.316852
376.295401	19054.484199	29.321869
376.188106	19073.380080	29.326887
376.542427	19095.908361	29.331904
376.841809	19116.659713	29.336922
377.166676	19137.545472	29.341940
377.683066	19164.454461	29.346957
377.959783	19196.333279	29.351975
377.950010	19221.815763	29.356992
378.252385	19250.365056	29.362010
378.399921	19290.800807	29.367028
378.895504	19326.344435	29.372045
379.248315	19361.898416	29.377063
379.633134	19399.070989	29.382080
379.765931	19436.383014	29.387098
380.351228	19467.618196	29.392116
380.781347	19504.529388	29.397133
380.825953	19544.169801	29.402151
381.563426	19576.050786	29.407168
382.588893	19606.141775	29.412186
382.865273	19635.181804	29.417204
383.043734	19666.556453	29.422221
383.509055	19705.223255	29.427239
383.606491	19724.384355	29.432256
383.819058	19754.362643	29.437274
383.769984	19789.436117	29.442292
384.250616	19822.039580	29.447309
384.765056	19862.025940	29.452327
385.761608	19891.764474	29.457344
386.163232	19914.388230	29.462362
387.040920	19946.660571	29.467380
387.410079	19959.072594	29.472397
387.683659	19978.918065	29.477415
388.305661	19997.816134	29.482432
388.668730	20011.134298	29.487450
389.007726	20041.871925	29.492468
389.754335	20040.911457	29.497485
389.748181	20069.718412	29.502503
390.200713	20077.513659	29.507520
390.564768	20096.068160	29.512538
390.652637	20125.248557	29.517556
391.023215	20135.842452	29.522573
391.335625	20161.875040	29.527591
391.206561	20185.238160	29.532608
392.028375	20209.176287	29.537626
391.748825	20245.818100	29.542644
392.341597	20268.035875	29.547661
391.963329	20304.049827	29.552679
392.986818	20335.955765	29.557696
393.531065	20378.379108	29.562714
393.416643	20412.862734	29.567732
393.913222	20452.572881	29.572749
394.241831	20495.063430	29.577767
395.003863	20525.213822	29.582784
396.008749	20552.828137	29.587802
396.379606	20582.873797	29.592820
397.113934	20608.416911	29.597837
397.094436	20638.228394	29.602855
397.437471	20662.873635	29.607872
397.805017	20688.173823	29.612890
398.128409	20704.632479	29.617908
398.744711	20738.152669	29.622925
398.961007	20762.353034	29.627943
399.246495	20797.812768	29.632960
399.680952	20827.748622	29.637978
399.835350	20871.752194	29.642996
400.534223	20893.071155	29.648013
400.868433	20934.461209	29.653031
401.032317	20972.261685	29.658048
401.122842	20998.549611	29.663066
401.788174	21041.870013	29.668084
402.761235	21073.087439	29.673101
402.805642	21113.363872	29.678119
403.243778	21143.184541	29.683136
403.278857	21173.574202	29.688154
403.869401	21221.009309	29.693172
404.623559	21236.737105	29.698189
405.216040	21279.162318	29.703207
405.691021	21300.569045	29.708224
406.419919	21316.146710	29.713242
406.427931	21340.306324	29.718260
406.886673	21370.308356	29.723277
407.201354	21397.110393	29.728295
407.150725	21428.128606	29.733312
407.605771	21463.414019	29.738330
407.719274	21493.325627	29.743348
408.317310	21529.114932	29.748365
408.423627	21573.598473	29.753383
408.648899	21601.994635	29.758400
409.690126	21635.688198	29.763418
409.945662	21668.997668	29.768436
410.611507	21698.464905	29.773453
410.821255	21729.087391	29.778471
411.527806	21759.501794	29.783488
412.440200	21779.432282	29.788506
412.613421	21799.582504	29.793524
413.220195	21815.432290	29.798541
413.471552	21843.551576	29.803559
413.782952	21860.932758	29.808576
414.575372	21872.724880	29.813594
414.963567	21888.418229	29.818612
414.694913	21905.775860	29.823629
415.238437	21938.997082	29.828647
415.718065	21962.215747	29.833664
415.950726	21988.879808	29.838682
416.230884	22031.983313	29.843700
416.317995	22061.536165	29.848717
416.909849	22095.528422	29.853735
417.107915	22126.888483	29.858752
417.816939	22159.842077	29.863770
418.079309	22199.795137	29.868788
418.425424	22236.498007	29.873805
419.191400	22270.132765	29.878823
419.650527	22311.938423	29.883840
419.760131	22335.921184	29.888858
420.287197	22376.649323	29.893876
420.785066	22407.324577	29.898893
421.378178	22441.358309	29.903911
421.290625	22487.478090	29.908928
422.253665	22513.074766	29.913946
422.232741	22554.174787	29.918964
422.695244	22582.389996	29.923981
422.833702	22617.271566	29.928999
423.701439	22658.033462	29.934016
424.077233	22691.587677	29.939034
424.630920	22740.209773	29.944052
424.948978	22770.597936	29.949069
425.547261	22809.472949	29.954087
425.494639	22848.629913	29.959104
426.112709	22882.833720	29.964122
426.694919	22925.247440	29.969140
427.295744	22958.678455	29.974157
427.680324	22994.310285	29.979175
427.981085	23014.558360	29.984192
429.059360	23042.914824	29.989210
429.355981	23081.451044	29.994228
429.484606	23111.701954	29.999245
430.087276	23136.266853	30.004263
430.250813	23172.400584	30.009280
430.675948	23195.286468	30.014298
430.835953	23229.083730	30.019316
431.652823	23257.289792	30.024333
431.856926	23300.352747	30.029351
432.128066	23337.143368	30.034368
432.563718	23361.238858	30.039386
432.793080	23394.863701	30.044404
433.280764	23429.018397	30.049421
434.009128	23461.125873	30.054439
434.186571	23497.658483	30.059456
434.557333	23540.318134	30.064474
434.537017	23586.423032	30.069492
434.797659	23631.599889	30.074509
435.336080	23674.899830	30.079527
435.845369	23721.658724	30.084544
436.378827	23766.076333	30.089562
436.537384	23809.126286	30.094580
437.116884	23851.700471	30.099597
438.071880	23896.191274	30.104615
438.259265	23941.053456	30.109632
439.272305	23966.164299	30.114650
439.983323	24003.612751	30.119668
440.237338	24034.017278	30.124685
440.881680	24057.491291	30.129703
440.791013	24096.626069	30.134720
441.403247	24129.830304	30.139738
441.816734	24157.914562	30.144756
442.308158	24192.530659	30.149773
443.311359	24231.465677	30.154791
443.253329	24259.911635	30.159808
443.789553	24287.363138	30.164826
443.934117	24321.032709	30.169844
444.541241	24367.442235	30.174861
444.956847	24397.614682	30.179879
445.135062	24443.249396	30.184896
445.663060	24483.493453	30.189914
445.539322	24528.684905	30.194932
446.122332	24571.916373	30.199949
446.823129	24613.364476	30.204967
446.741900	24664.305715	30.209984
447.444512	24716.141112	30.215002
447.537099	24762.415910	30.220020
447.951469	24814.815163	30.225037
448.094775	24861.450599	30.230055
448.717397	24928.772733	30.235072
449.440220	24983.958622	30.240090
449.790314	25028.675876	30.245108
449.797306	25087.227526	30.250125
450.398592	25133.548630	30.255143
450.764741	25206.322537	30.260160
451.421801	25253.839414	30.265178
451.864742	25310.061656	30.270196
452.868452	25351.358677	30.275213
453.452336	25396.670872	30.280231
454.141252	25439.350094	30.285248
454.780254	25477.407135	30.290266
455.183073	25519.785430	30.295284
455.154118	25557.837236	30.300301
456.047647	25598.869820	30.305319
456.204076	25635.246512	30.310336
457.200601	25679.460353	30.315354
457.106929	25713.047270	30.320372
457.434129	25756.275059	30.325389
458.164344	25786.225670	30.330407
457.997156	25836.686654	30.335424
458.716291	25879.743488	30.340442
459.054474	25930.525087	30.345460
459.260695	25979.569173	30.350477
460.091584	26022.152945	30.355495
460.185178	26071.080939	30.360512
460.748477	26112.060914	30.365530
461.301257	26159.850514	30.370548
461.411950	26208.022003	30.375565
461.880192	26256.709658	30.380583
462.347047	26313.107710	30.385600
462.985999	26369.072654	30.390618
463.591585	26420.967630	30.395636
463.948120	26464.946125	30.400653
465.762428	26481.260525	30.405671
466.658570	26515.218830	30.410688
467.235641	26543.376723	30.415706
467.731172	26565.482107	30.420724
467.836341	26597.361498	30.425741
468.598448	26622.314158	30.430759
468.435037	26662.233779	30.435776
468.844484	26681.969081	30.440794
468.740908	26721.742931	30.445812
468.938141	26768.244895	30.450829
469.622088	26807.660005	30.455847
469.913217	26858.963445	30.460864
470.175559	26907.905883	30.465882
470.272788	26959.987374	30.470900
470.521559	27021.002688	30.475917
471.001974	27076.760460	30.480935
471.662606	27141.421988	30.485952
472.499265	27205.479411	30.490970
472.953991	27261.078122	30.495988
473.308055	27327.256718	30.501005
473.886172	27370.688438	30.506023
474.315195	27428.550969	30.511040
474.642501	27480.805961	30.516058
475.522571	27531.180719	30.521076
475.940157	27580.906089	30.526093
476.644409	27633.658518	30.531111
477.013931	27682.676248	30.536128
477.252948	27729.170450	30.541146
478.018040	27779.467823	30.546164
478.165984	27842.673873	30.551181
479.149829	27887.403446	30.556199
479.185875	27941.037956	30.561216
479.619583	27987.338577	30.566234
480.591957	28031.196554	30.571252
480.758855	28085.395910	30.576269
481.332632	28129.997605	30.581287
481.451071	28183.281150	30.586304
481.915130	28223.819300	30.591322
482.530581	28275.298474	30.596340
482.384523	28326.718985	30.601357
483.097743	28384.832545	30.606375
483.569224	28434.800349	30.611392
483.750646	28493.434481	30.616410
484.341523	28543.785984	30.621428
484.823799	28602.397322	30.626445
485.865955	28638.306667	30.631463
486.245538	28692.783803	30.636480
486.894016	28742.633809	30.641498
487.950291	28787.451076	30.646516
488.197311	28841.071108	30.651533
488.752648	28883.693300	30.656551
489.004361	28936.293708	30.661568
489.197857	28986.417986	30.666586
489.385345	29041.159441	30.671604
490.093596	29088.264656	30.676621
490.526792	29144.040242	30.681639
491.493502	29196.900687	30.686656
491.145476	29252.305648	30.691674
492.328939	29307.300063	30.696692
492.507642	29368.789883	30.701709
492.759600	29421.189759	30.706727
493.170175	29481.608478	30.711744
493.556696	29551.718158	30.716762
494.035854	29613.655876	30.721780
494.740304	29673.602090	30.726797
495.127978	29730.434878	30.731815
495.592823	29806.855345	30.736832
496.108191	29862.167908	30.741850
496.744682	29917.904790	30.746868
496.872241	29996.968078	30.751885
497.642758	30054.572470	30.756903
498.049829	30120.963886	30.761920
498.770728	30190.785303	30.766938
499.244557	30249.605499	30.771956
500.336894	30302.239472	30.776973
500.911987	30338.705627	30.781991
501.903198	30391.874681	30.787008
502.477602	30437.406638	30.792026
503.628660	30467.438299	30.797044
503.849637	30509.604218	30.802061
504.922963	30543.817647	30.807079
505.597775	30560.293300	30.812096
506.238783	30587.932392	30.817114
506.738641	30610.234614	30.822132
507.223308	30644.176761	30.827149
507.388014	30671.462146	30.832167
507.853655	30690.169958	30.837184
507.671389	30736.494985	30.842202
508.533619	30767.226674	30.847220
508.872175	30812.645391	30.852237
509.141833	30841.153156	30.857255
509.711097	30876.725261	30.862272
510.091057	30913.254434	30.867290
510.584642	30952.288617	30.872308
510.679137	31004.716999	30.877325
511.280967	31044.155675	30.882343
511.377739	31089.288352	30.887360
511.418052	31133.594601	30.892378
511.868990	31179.884860	30.897396
512.059669	31245.702228	30.902413
512.582315	31306.574982	30.907431
513.239217	31366.099598	30.912448
513.540425	31439.437418	30.917466
513.808736	31504.131669	30.922484
513.755214	31577.641284	30.927501
514.536238	31647.174117	30.932519
514.992491	31723.083617	30.937536
515.474838	31799.840994	30.942554
515.932391	31867.697658	30.947572
516.453334	31945.913278	30.952589
516.782595	32030.120035	30.957607
517.337171	32108.661952	30.962624
517.721041	32184.806714	30.967642
518.791532	32260.635337	30.972660
519.612538	32338.854908	30.977677
520.308336	32394.778734	30.982695
521.273776	32456.889178	30.987712
521.634728	32524.667056	30.992730
522.527286	32579.431131	30.997748
523.195807	32647.055786	31.002765
523.334302	32704.786518	31.007783
524.144655	32763.926577	31.012800
525.427430	32813.048166	31.017818
526.839332	32842.821405	31.022836
527.498415	32865.638819	31.027853
528.817056	32883.372794	31.032871
529.413197	32915.990491	31.037888
529.784827	32942.297134	31.042906
530.021540	32959.717943	31.047924
530.889755	32979.798256	31.052941
531.131466	33014.490302	31.057959
531.332067	33033.422719	31.062976
531.705705	33062.623129	31.067994
531.903389	33093.027723	31.073012
532.411622	33130.647168	31.078029
532.619889	33170.019117	31.083047
532.996152	33206.465248	31.088064
533.313822	33255.725017	31.093082
533.939700	33300.365497	31.098100
534.070168	33351.844655	31.103117
534.159538	33405.975678	31.108135
534.903951	33461.096051	31.113152
535.518403	33527.865406	31.118170
535.964769	33577.823564	31.123188
536.362705	33632.729260	31.128205
536.710835	33695.789259	31.133223
537.073299	33736.489944	31.138240
537.181836	33806.938541	31.143258
538.192099	33860.269314	31.148276
538.442534	33920.064580	31.153293
538.790771	33986.013340	31.158311
539.550666	34043.834414	31.163328
539.959219	34120.011551	31.168346
540.204345	34177.918100	31.173364
540.754672	34244.275026	31.178381
541.295958	34308.626469	31.183399
542.085414	34372.001413	31.188416
542.444905	34445.754973	31.193434
542.836543	34507.986606	31.198452
543.372271	34573.397247	31.203469
543.963672	34646.455412	31.208487
544.649605	34714.283690	31.213504
545.097499	34790.977679	31.218522
546.290477	34846.423108	31.223540
547.384338	34893.704828	31.228557
548.291108	34962.575618	31.233575
549.032421	35003.902300	31.238592
549.302512	35056.703783	31.243610
550.282693	35107.003954	31.248628
550.583249	35143.621625	31.253645
551.272689	35196.402164	31.258663
551.964132	35241.664309	31.263680
552.124122	35291.556335	31.268698
552.657421	35327.197088	31.273716
553.267231	35387.323847	31.278733
553.639317	35446.923405	31.283751
554.750194	35479.959402	31.288768
554.764880	35533.629827	31.293786
555.699744	35575.063528	31.298804
557.506231	35596.987115	31.303821
558.154186	35610.726039	31.308839
558.512060	35643.310590	31.313856
558.802819	35682.134144	31.318874
559.522405	35711.491041	31.323892
559.542011	35740.077829	31.328909
560.084422	35790.641131	31.333927
560.831049	35825.040587	31.338944
561.286130	35875.047785	31.343962
561.098163	35915.352131	31.348980
561.875053	35962.331128	31.353997
562.118240	36014.095242	31.359015
562.689296	36065.430871	31.364032
563.362907	36115.666427	31.369050
563.711675	36171.121677	31.374068
564.408105	36221.091631	31.379085
564.629101	36284.204515	31.384103
565.271096	36337.151165	31.389120
565.217851	36390.122395	31.394138
566.112941	36452.959387	31.399156
567.193335	36505.297970	31.404173
567.384008	36559.540993	31.409191
568.113777	36603.262757	31.414208
568.258808	36661.661536	31.419226
568.914887	36713.969254	31.424244
569.670257	36765.720345	31.429261
569.928401	36818.645777	31.434279
570.181445	36871.445976	31.439296
570.805154	36932.497168	31.444314
571.268278	36990.801461	31.449332
571.550455	37042.905876	31.454349
571.738383	37125.683292	31.459367
572.705434	37191.433493	31.464384
572.692326	37275.041489	31.469402
573.593158	37343.830770	31.474420
574.199967	37402.054936	31.479437
574.604494	37488.483823	31.484455
575.303440	37557.557872	31.489472
576.500580	37620.820627	31.494490
577.257751	37689.294900	31.499508
577.850312	37755.502718	31.504525
578.456633	37819.059943	31.509543
579.016702	37878.957214	31.514560
579.198941	37954.340010	31.519578
580.071846	38016.684256	31.524596
581.051229	38070.241032	31.529613
581.570473	38130.370246	31.534631
582.433118	38185.595186	31.539648
583.430039	38233.520924	31.544666
583.832948	38287.893691	31.549684
584.892104	38329.066130	31.554701
584.991717	38380.880472	31.559719
585.658762	38433.513215	31.564736
586.518627	38498.835046	31.569754
586.955993	38547.182624	31.574772
587.812137	38592.743702	31.579789
587.447446	38647.072261	31.584807
588.580950	38710.059247	31.589824
588.843346	38765.410869	31.594842
589.142178	38822.710518	31.599860
589.838788	38880.352589	31.604877
590.519563	38943.313762	31.609895
590.790646	39007.794362	31.614912
591.303886	39076.669167	31.619930
591.846266	39139.872549	31.624948
592.629780	39191.710898	31.629965
593.788268	39238.301444	31.634983
594.536295	39296.387449	31.640000
595.467611	39353.403592	31.645018
595.852139	39410.744051	31.650036
596.677332	39448.360132	31.655053
597.558290	39499.289226	31.660071
598.271411	39532.211295	31.665088
598.568283	39576.958255	31.670106
599.076027	39633.997323	31.675124
599.697807	39678.505756	31.680141
599.803159	39730.300798	31.685159
600.462985	39774.083140	31.690176
600.637747	39828.373251	31.695194
601.260764	39878.952952	31.700212
601.369292	39926.978477	31.705229
601.748455	39998.001228	31.710247
602.180616	40063.679696	31.715264
602.855350	40137.237992	31.720282
603.049404	40208.558458	31.725300
603.392099	40287.784423	31.730317
604.383580	40360.904169	31.735335
604.744845	40434.605748	31.740352
604.993711	40501.924156	31.745370
605.695750	40596.260026	31.750388
606.418209	40672.647408	31.755405
607.445742	40760.115132	31.760423
607.868264	40831.285181	31.765440
608.181162	40893.305698	31.770458
608.887031	40979.936069	31.775476
609.832462	41061.392103	31.780493
610.034974	41147.408580	31.785511
610.500220	41239.957061	31.790528
611.067643	41313.260549	31.795546
611.842820	41400.723997	31.800564
613.128103	41469.945844	31.805581
613.572851	41543.299668	31.810599
614.498442	41622.791375	31.815616
615.362925	41693.380658	31.820634
615.670311	41780.613451	31.825652
616.530472	41840.765750	31.830669
617.399586	41910.047901	31.835687
617.776646	41969.247755	31.840704
618.464472	42033.575876	31.845722
619.410833	42112.267279	31.850740
619.920917	42170.677724	31.855757
620.741461	42236.931947	31.860775
621.246956	42304.386540	31.865792
622.099037	42366.884754	31.870810
622.825202	42439.698152	31.875828
623.485216	42493.284536	31.880845
623.948307	42556.048946	31.885863
624.299157	42617.945533	31.890880
625.263157	42687.280610	31.895898
625.565630	42757.616546	31.900916
625.988859	42812.239033	31.905933
626.505538	42887.628726	31.910951
627.371517	42951.001149	31.915968
627.972012	43018.066278	31.920986
628.247639	43101.505758	31.926004
628.940360	43166.184259	31.931021
629.320591	43249.568582	31.936039
630.236893	43324.913665	31.941056
631.040391	43397.834357	31.946074
631.586670	43474.345449	31.951092
631.732540	43547.534111	31.956109
632.826019	43619.285005	31.961127
633.305510	43680.897799	31.966144
634.628110	43735.855167	31.971162
634.794470	43802.700639	31.976180
635.650037	43861.871836	31.981197
636.212609	43917.569383	31.986215
636.514756	43987.632080	31.991232
637.159122	44046.091652	31.996250
637.686465	44126.470564	32.001268
638.414771	44187.650820	32.006285
638.954629	44254.686523	32.011303
639.923593	44323.373108	32.016320
640.892369	44386.098025	32.021338
641.388829	44464.857392	32.026356
642.193608	44524.617247	32.031373
642.910292	44578.259849	32.036391
643.635636	44641.800991	32.041408
644.710961	44689.218335	32.046426
644.983836	44752.341579	32.051444
645.654508	44813.334785	32.056461
646.602016	44861.747088	32.061479
647.027350	44919.681618	32.066496
647.778306	44972.829992	32.071514
647.606931	45037.261875	32.076532
648.581861	45107.011341	32.081549
649.163442	45172.628387	32.086567
649.614441	45246.134493	32.091584
649.997426	45304.579566	32.096602
650.940207	45374.547105	32.101620
651.551857	45441.047317	32.106637
652.324225	45509.658192	32.111655
652.660999	45582.878841	32.116672
653.820151	45655.017794	32.121690
654.144880	45718.024826	32.126708
654.419796	45791.073706	32.131725
655.294467	45867.648724	32.136743
655.971397	45950.340371	32.141760
656.258426	46001.433082	32.146778
658.168318	46068.913145	32.151796
658.987914	46127.683862	32.156813
659.895727	46182.792031	32.161831
660.629218	46232.501418	32.166848
661.414755	46287.722424	32.171866
662.085414	46341.943191	32.176884
662.654627	46394.940341	32.181901
663.500663	46445.521600	32.186919
663.570328	46512.494216	32.191936
664.258287	46561.286917	32.196954
665.018799	46616.920566	32.201972
665.783205	46672.032608	32.206989
666.204992	46732.935636	32.212007
666.643998	46798.626914	32.217024
667.358966	46856.479809	32.222042
667.851975	46922.714948	32.227060
667.996573	46997.575159	32.232077
668.657283	47070.922871	32.237095
669.070530	47142.453037	32.242112
669.629599	47206.527059	32.247130
670.176338	47283.672409	32.252148
670.521127	47361.572758	32.257165
670.787578	47442.683059	32.262183
671.009287	47528.870487	32.267200
671.833135	47612.978022	32.272218
672.673488	47708.254214	32.277236
672.904490	47801.298068	32.282253
674.064675	47894.950680	32.287271
674.676460	47990.497987	32.292288
675.245680	48085.017095	32.297306
676.549782	48173.735062	32.302324
677.346660	48243.731766	32.307341
678.727902	48311.998851	32.312359
679.409360	48386.541918	32.317376
680.561077	48446.418842	32.322394
680.985169	48523.141659	32.327412
682.038653	48598.815724	32.332429
682.808744	48655.063221	32.337447
682.716545	48738.242904	32.342464
683.697288	48807.531070	32.347482
683.941420	48878.063800	32.352500
684.448560	48957.698931	32.357517
684.955491	49033.323032	32.362535
685.505561	49126.678680	32.367552
686.265348	49206.745341	32.372570
686.504090	49304.059211	32.377588
686.937268	49397.360378	32.382605
687.915729	49489.475688	32.387623
688.084005	49588.009655	32.392640
689.320765	49682.431678	32.397658
689.984283	49773.079800	32.402676
690.187297	49880.984312	32.407693
690.858627	49969.427227	32.412711
691.747985	50082.610387	32.417728
692.095254	50172.152123	32.422746
692.890764	50276.425828	32.427764
693.316323	50393.171216	32.432781
694.507344	50492.469551	32.437799
694.961338	50606.564258	32.442816
696.192203	50704.947105	32.447834
697.186840	50800.477398	32.452852
697.634675	50897.447511	32.457869
698.308205	50994.076187	32.462887
699.468889	51085.656082	32.467904
699.916527	51172.506450	32.472922
700.903921	51264.369581	32.477940
701.692697	51350.119847	32.482957
702.627478	51442.144454	32.487975
703.440158	51524.738742	32.492992
704.511257	51609.247685	32.498010
705.152415	51694.569850	32.503028
705.902950	51778.616359	32.508045
706.739544	51848.906695	32.513063
706.869110	51933.938454	32.518080
707.910035	51997.541371	32.523098
708.401500	52077.867946	32.528116
708.903208	52152.784748	32.533133
709.679676	52214.892040	32.538151
710.782193	52289.163077	32.543168
711.912656	52357.281974	32.548186
712.395344	52419.882515	32.553204
712.666961	52495.535043	32.558221
713.387136	52570.605559	32.563239
713.578587	52655.257047	32.568256
714.231755	52740.891287	32.573274
715.205580	52832.271238	32.578292
715.452717	52923.283261	32.583309
716.265105	53009.150443	32.588327
716.925519	53106.044476	32.593344
717.523322	53192.878029	32.598362
718.089925	53280.943100	32.603380
718.426850	53391.630413	32.608397
719.350657	53485.833709	32.613415
719.455218	53594.413637	32.618432
720.411598	53696.712828	32.623450
721.052009	53805.972996	32.628468
721.971378	53913.182945	32.633485
722.955762	54013.267418	32.638503
723.721687	54130.684339	32.643520
724.470142	54227.966852	32.648538
725.503984	54334.887757	32.653556
726.023966	54429.297399	32.658573
726.773187	54535.143373	32.663591
727.572356	54624.362516	32.668608
728.636092	54718.914187	32.673626
729.664200	54813.466090	32.678644
730.231159	54922.321593	32.683661
730.645678	55000.208760	32.688679
731.353869	55097.736220	32.693696
732.216030	55189.348356	32.698714
733.714467	55289.281671	32.703732
733.909769	55371.915610	32.708749
734.809792	55466.353523	32.713767
735.701706	55562.575298	32.718784
736.540774	55652.948621	32.723802
737.250715	55739.843580	32.728820
737.699937	55834.499475	32.733837
738.588130	55924.189438	32.738855
739.394054	56020.756748	32.743872
739.974295	56116.927142	32.748890
740.741898	56201.204302	32.753908
741.343707	56301.770219	32.758925
742.218844	56386.642725	32.763943
743.356694	56484.507780	32.768960
743.842773	56565.390545	32.773978
744.681209	56655.825367	32.778996
745.411775	56751.164135	32.784013
745.832792	56840.691748	32.789031
746.630160	56926.211815	32.794048
747.201667	57014.715914	32.799066
747.803981	57101.237049	32.804084
748.059361	57207.453464	32.809101
748.615251	57295.076700	32.814119
748.966418	57393.447470	32.819136
749.693198	57505.626447	32.824154
750.609549	57607.800794	32.829172
750.755569	57724.624463	32.834189
751.524994	57833.745431	32.839207
752.738548	57951.089056	32.844224
753.354006	58063.467150	32.849242
754.493009	58171.022461	32.854260
755.620966	58284.495842	32.859277
756.488474	58384.179711	32.864295
757.161633	58479.283646	32.869312
758.317804	58573.066534	32.874330
759.932071	58664.698356	32.879348
760.404082	58758.472887	32.884365
761.129650	58836.624956	32.889383
762.292086	58921.439923	32.894400
762.733606	59008.142099	32.899418
763.605194	59098.815999	32.904436
764.088249	59191.042143	32.909453
764.803487	59274.999767	32.914471
765.773343	59372.313433	32.919488
766.516952	59471.556136	32.924506
767.438537	59562.419465	32.929524
767.954294	59651.898995	32.934541
769.033656	59736.112169	32.939559
770.094611	59820.941939	32.944576
770.655605	59913.714202	32.949594
771.535504	59990.820316	32.954612
772.412083	60075.531029	32.959629
773.197184	60160.504267	32.964647
774.253209	60237.037562	32.969664
775.021269	60322.406274	32.974682
776.233603	60403.995282	32.979700
776.722751	60487.693212	32.984717
777.142905	60569.197342	32.989735
778.165734	60645.187937	32.994752
778.392960	60735.890970	32.999770
779.232651	60821.337977	33.004788
780.310475	60898.527377	33.009805
781.434619	60974.723068	33.014823
782.678106	61053.806237	33.019840
783.159571	61133.045519	33.024858
784.442724	61195.144310	33.029876
785.261560	61266.975008	33.034893
785.660869	61336.039670	33.039911
786.413583	61409.272817	33.044928
786.850177	61489.342891	33.049946
787.421633	61573.581069	33.054964
787.909313	61658.674651	33.059981
788.366809	61744.481722	33.064999
788.786039	61827.356353	33.070016
788.886940	61919.843513	33.075034
789.779666	62011.215664	33.080052
790.269994	62109.243907	33.085069
791.087392	62210.105425	33.090087
791.880609	62309.972806	33.095104
792.576615	62413.555316	33.100122
793.469364	62514.715155	33.105140
794.243659	62620.396633	33.110157
795.111180	62720.227974	33.115175
795.845830	62819.696943	33.120192
796.492801	62939.094194	33.125210
797.360090	63040.178772	33.130228
798.549516	63136.511727	33.135245
799.539237	63235.186724	33.140263
800.872256	63331.085080	33.145280
801.770802	63430.035804	33.150298
802.531949	63535.155226	33.155316
803.333645	63634.142472	33.160333
803.989369	63722.186932	33.165351
804.974811	63817.685572	33.170368
805.580524	63920.513460	33.175386
806.490946	64007.371246	33.180404
807.005758	64109.482298	33.185421
807.498560	64214.284428	33.190439
808.636780	64315.998899	33.195456
809.152739	64433.239737	33.200474
809.289708	64539.495273	33.205492
810.200864	64649.595304	33.210509
811.453167	64764.865835	33.215527
812.007204	64864.963423	33.220544
812.534608	64991.530520	33.225562
813.507238	65107.647423	33.230580
815.177891	65221.205035	33.235597
815.218803	65333.265853	33.240615
815.873741	65444.172597	33.245632
816.430327	65571.496850	33.250650
817.018395	65688.530010	33.255668
817.847066	65813.147407	33.260685
818.998596	65935.668095	33.265703
820.499451	66047.311933	33.270720
821.371002	66167.510999	33.275738
822.314169	66274.813168	33.280756
823.278985	66383.117460	33.285773
824.123064	66491.904535	33.290791
825.221070	66598.302982	33.295808
827.158593	66669.334696	33.300826
828.209128	66757.621386	33.305844
829.197290	66846.500815	33.310861
829.694522	66939.245690	33.315879
830.611060	67016.086988	33.320896
831.050391	67115.810218	33.325914
831.818993	67208.573015	33.330932
832.710061	67292.956459	33.335949
833.045917	67388.354905	33.340967
834.029504	67469.201370	33.345984
834.686726	67566.094674	33.351002
835.122097	67655.299786	33.356020
835.762254	67750.198800	33.361037
835.909439	67867.357414	33.366055
837.000644	67966.524035	33.371072
836.892680	68081.805324	33.376090
837.688373	68204.532819	33.381108
838.186475	68318.883251	33.386125
838.699252	68454.193083	33.391143
839.876776	68589.105368	33.396160
840.196829	68733.119091	33.401178
840.797762	68862.276516	33.406196
841.633061	68993.025995	33.411213
842.525767	69137.153011	33.416231
843.815112	69277.861648	33.421248
844.282781	69425.832149	33.426266
845.309310	69569.856934	33.431284
846.190847	69705.250588	33.436301
847.120347	69843.849254	33.441319
847.967812	69979.421199	33.446336
849.078715	70123.941118	33.451354
850.748623	70249.799875	33.456372
851.872036	70375.955325	33.461389
852.869116	70509.601522	33.466407
853.930168	70617.303648	33.471424
855.029997	70743.098494	33.476442
855.783461	70857.456585	33.481460
856.949250	70979.839262	33.486477
857.298700	71097.764936	33.491495
858.321753	71210.497725	33.496512
859.431760	71327.421673	33.501530
859.981276	71453.833453	33.506548
861.255188	71564.672166	33.511565
862.048195	71691.827809	33.516583
862.846314	71810.521602	33.521600
863.096768	71927.595984	33.526618
863.745105	72053.722371	33.531636
864.811943	72188.340856	33.536653
865.018063	72324.498929	33.541671
865.885211	72462.119394	33.546688
866.538424	72605.045570	33.551706
867.735055	72731.809258	33.556724
869.368401	72847.285631	33.561741
871.643443	72946.999620	33.566759
873.529896	73028.888594	33.571776
874.509940	73121.754380	33.576794
875.351798	73216.351856	33.581812
876.355210	73309.480064	33.586829
877.186266	73388.660803	33.591847
877.300278	73473.138180	33.596864
878.365376	73570.867585	33.601882
878.744927	73673.300233	33.606900
880.105021	73752.157659	33.611917
881.144008	73846.034684	33.616935
882.511565	73922.367872	33.621952
883.130609	73997.045932	33.626970
884.007916	74067.714363	33.631988
884.599979	74157.906002	33.637005
885.505279	74239.815732	33.642023
886.135867	74307.219288	33.647040
886.793108	74400.733960	33.652058
887.309611	74496.214881	33.657076
888.680589	74579.810769	33.662093
889.287290	74686.155970	33.667111
889.569111	74783.246914	33.672128
890.376840	74888.160828	33.677146
890.654659	74998.706748	33.682164
891.034691	75098.533651	33.687181
891.269581	75226.747723	33.692199
892.220704	75357.256081	33.697216
893.076738	75510.425730	33.702234
893.445472	75647.537845	33.707252
894.522445	75778.596388	33.712269
895.702069	75906.317326	33.717287
896.815936	76042.374429	33.722304
897.803666	76173.286112	33.727322
899.145427	76294.542247	33.732340
900.638467	76412.597748	33.737357
901.080766	76531.599209	33.742375
902.260040	76657.838006	33.747392
903.485021	76777.478443	33.752410
904.976908	76883.688839	33.757428
906.676456	76987.618577	33.762445
907.282711	77103.103243	33.767463
908.741796	77195.056374	33.772480
909.346117	77300.313752	33.777498
909.815947	77412.660512	33.782516
910.749806	77512.959994	33.787533
911.299644	77627.533447	33.792551
912.097450	77738.098713	33.797568
912.728222	77856.790241	33.802586
913.257640	77973.962554	33.807604
914.378734	78095.645753	33.812621
915.005920	78226.612157	33.817639
915.932748	78354.238476	33.822656
916.687816	78479.718770	33.827674
917.330849	78614.239937	33.832692
918.034907	78749.953412	33.837709
918.852701	78896.712672	33.842727
919.285586	79039.863274	33.847744
920.142606	79188.243530	33.852762
920.787175	79340.621389	33.857780
921.302688	79488.144772	33.862797
921.961161	79658.096906	33.867815
923.046149	79821.815329	33.872832
923.874353	79986.660727	33.877850
924.669774	80160.623099	33.882868
925.755700	80317.809626	33.887885
926.922314	80484.644130	33.892903
928.108307	80629.598998	33.897920
929.313544	80765.491682	33.902938
930.254824	80909.914501	33.907956
931.564008	81041.836821	33.912973
932.508603	81189.772178	33.917991
933.239302	81324.914299	33.923008
934.315070	81471.158714	33.928026
935.460722	81612.659561	33.933044
936.397271	81735.551576	33.938061
937.666405	81874.736201	33.943079
938.776806	82012.493635	33.948096
939.656001	82145.520884	33.953114
940.945207	82281.806732	33.958132
941.766542	82405.000426	33.963149
942.901558	82532.899080	33.968167
943.592230	82661.368056	33.973184
944.486314	82794.934291	33.978202
945.195298	82935.353789	33.983220
946.308693	83082.152406	33.988237
946.838522	83221.705833	33.993255
947.401584	83360.874760	33.998272
948.833368	83502.793708	34.003290
949.793563	83656.177386	34.008308
950.855389	83794.883838	34.013325
952.393167	83918.525995	34.018343
954.110925	84043.036501	34.023360
955.311455	84161.061866	34.028378
956.471612	84283.315272	34.033396
957.448745	84413.839284	34.038413
958.121587	84523.313245	34.043431
958.347253	84659.592636	34.048448
959.111842	84784.472799	34.053466
959.758165	84925.864138	34.058484
960.650537	85063.132731	34.063501
961.694824	85223.226098	34.068519
962.192111	85374.574107	34.073536
962.768085	85523.194912	34.078554
963.365639	85686.202849	34.083572
964.081474	85845.103730	34.088589
964.977947	86017.092889	34.093607
965.565584	86193.293775	34.098624
966.596410	86357.447134	34.103642
967.415572	86543.761391	34.108660
968.270562	86725.932270	34.113677
969.599036	86891.506509	34.118695
970.912045	87054.097554	34.123712
972.220441	87211.963170	34.128730
973.496047	87379.315479	34.133748
974.377508	87549.875396	34.138765
975.678840	87689.082619	34.143783
976.280555	87854.066534	34.148800
978.040825	88011.986625	34.153818
979.377060	88161.550585	34.158836
980.229763	88309.730020	34.163853
981.120815	88451.878836	34.168871
981.900866	88597.863757	34.173888
983.079679	88727.231416	34.178906
984.119772	88870.173598	34.183924
984.940308	88996.705443	34.188941
986.188703	89127.829098	34.193959
986.885879	89269.091913	34.198976
988.251476	89394.855308	34.203994
988.965037	89532.199210	34.209012
990.606156	89662.790170	34.214029
991.214664	89796.324478	34.219047
992.207487	89942.350709	34.224064
993.107119	90081.089913	34.229082
993.819799	90220.969535	34.234100
994.585732	90349.676060	34.239117
996.199206	90494.238541	34.244135
997.079015	90630.142428	34.249152
998.337616	90772.748282	34.254170
999.252618	90919.996286	34.259188
1000.138175	91053.686263	34.264205
1001.654211	91179.907851	34.269223
1002.397030	91324.409146	34.274240
1003.679357	91465.084487	34.279258
1004.406898	91606.070843	34.284276
1005.100310	91746.981569	34.289293
1006.024658	91896.082089	34.294311
1006.534132	92035.557491	34.299328
1008.116315	92179.983392	34.304346
1008.794953	92339.408133	34.309364
1009.912875	92491.549048	34.314381
1010.993421	92642.190802	34.319399
1011.284611	92802.583718	34.324416
1012.615158	92958.311789	34.329434
1013.896708	93118.980266	34.334452
1014.518819	93279.870317	34.339469
1016.144051	93440.323779	34.344487
1016.711057	93585.950881	34.349504
1018.213191	93727.532021	34.354522
1019.717926	93876.526126	34.359540
1020.634396	94020.222209	34.364557
1022.148903	94167.102102	34.369575
1023.443952	94291.725282	34.374592
1024.410047	94429.021675	34.379610
1025.575184	94559.226432	34.384628
1026.201948	94708.040346	34.389645
1027.008937	94838.086322	34.394663
1027.812728	94994.803611	34.399680
1029.388609	95129.252028	34.404698
1029.652207	95282.771776	34.409716
1030.760206	95425.829091	34.414733
1032.700608	95572.846901	34.419751
1033.206140	95712.653808	34.424768
1034.918106	95842.214508	34.429786
1035.621121	95982.217001	34.434804
1036.346689	96121.127527	34.439821
1037.331135	96258.956247	34.444839
1038.295209	96400.575017	34.449856
1038.959778	96531.135280	34.454874
1040.344177	96677.488720	34.459892
1041.058427	96808.947222	34.464909
1042.068499	96942.799488	34.469927
1042.278546	97096.959873	34.474944
1043.119160	97255.926074	34.479962
1043.886823	97405.023014	34.484980
1044.237841	97582.878272	34.489997
1045.084491	97748.874018	34.495015
1045.978963	97936.825463	34.500032
1046.552537	98114.000537	34.505050
1047.257446	98305.557957	34.510068
1048.001853	98505.720623	34.515085
1048.984005	98702.969709	34.520103
1049.875709	98912.879617	34.525120
1050.721973	99119.462342	34.530138
1051.933201	99329.251292	34.535156
1053.024136	99541.620501	34.540173
1054.358220	99761.554095	34.545191
1055.330811	99969.698577	34.550208
1056.620413	100175.669328	34.555226
1057.742939	100379.656825	34.560244
1058.860865	100592.916496	34.565261
1060.282797	100797.596837	34.570279
1061.835058	101011.950644	34.575296
1063.591518	101197.935688	34.580314
1064.940693	101385.220211	34.585332
1066.092626	101576.541712	34.590349
1067.042622	101755.412284	34.595367
1068.229703	101948.250192	34.600384
1069.404670	102133.530956	34.605402
1070.626623	102315.968142	34.610420
1071.965092	102493.764083	34.615437
1073.445351	102659.416886	34.620455
1074.371539	102846.455005	34.625472
1075.873733	103023.327298	34.630490
1077.394831	103176.362212	34.635508
1078.342446	103338.488333	34.640525
1079.683796	103497.508422	34.645543
1080.807067	103662.684060	34.650560
1081.944990	103817.612076	34.655578
1083.031576	103976.488687	34.660596
1083.956718	104140.358709	34.665613
1085.162109	104299.748857	34.670631
1085.648939	104465.570414	34.675648
1086.896388	104633.415918	34.680666
1087.988235	104787.914187	34.685684
1088.733655	104960.863310	34.690701
1090.063712	105126.519266	34.695719
1090.817307	105296.746013	34.700736
1092.158879	105467.455803	34.705754
1093.470612	105631.332120	34.710772
1094.116299	105811.308142	34.715789
1095.400698	105970.593403	34.720807
1096.569030	106118.892478	34.725824
1098.535431	106263.217822	34.730842
1099.698046	106406.845581	34.735860
1100.949790	106540.376323	34.740877
1101.787595	106684.732499	34.745895
1102.713494	106831.189688	34.750912
1103.302345	106986.141394	34.755930
1104.244039	107129.747489	34.760948
1104.772736	107304.889468	34.765965
1105.598209	107472.267610	34.770983
1106.207295	107653.186851	34.776000
1106.947311	107834.667563	34.781018
1108.046018	108005.891001	34.786036
1109.564220	108191.294343	34.791053
1110.338592	108377.358330	34.796071
1111.418909	108569.084208	34.801088
1112.443610	108759.528865	34.806106
1113.632952	108953.632930	34.811124
1114.717948	109155.192169	34.816141
1115.664879	109350.442631	34.821159
1117.096619	109539.467554	34.826176
1118.388813	109724.349907	34.831194
1120.567990	109891.574407	34.836212
1121.795547	110079.219171	34.841229
1123.012543	110250.030975	34.846247
1124.317948	110425.908676	34.851264
1125.361249	110593.775293	34.856282
1126.684150	110760.505570	34.861300
1127.733802	110937.190407	34.866317
1128.656589	111108.551941	34.871335
1130.153610	111279.955570	34.876352
1131.609156	111452.697572	34.881370
1132.540709	111626.417176	34.886388
1133.905888	111787.850797	34.891405
1134.643556	111959.958711	34.896423
1135.546270	112139.843561	34.901440
1136.715099	112316.567396	34.906458
1137.778433	112493.259728	34.911476
1138.198164	112692.994795	34.916493
1139.398200	112874.543798	34.921511
1140.282745	113079.510496	34.926528
1140.620473	113274.259272	34.931546
1142.148799	113466.372973	34.936564
1142.700437	113679.205518	34.941581
1143.693322	113889.797571	34.946599
1145.361595	114096.727971	34.951616
1146.180801	114311.432601	34.956634
1147.386601	114522.512355	34.961652
1148.612201	114750.175599	34.966669
1149.727052	114962.553871	34.971687
1150.684852	115180.573598	34.976704
1151.605757	115409.662657	34.981722
1152.685104	115625.118179	34.986740
1154.225682	115843.093843	34.991757
1155.125225	116047.597811	34.996775
1156.964830	116246.367096	35.001792
1157.924816	116453.385096	35.006810
1159.377932	116644.937484	35.011828
1160.211057	116850.864993	35.016845
1161.326355	117050.676132	35.021863
1162.816037	117252.109834	35.026880
1163.925246	117450.277490	35.031898
1165.717659	117634.758360	35.036916
1166.709501	117830.883245	35.041933
1168.053877	118029.496094	35.046951
1168.890522	118220.353409	35.051968
1169.485124	118433.036277	35.056986
1171.266062	118620.363821	35.062004
1172.396098	118823.732699	35.067021
1173.495818	119020.379294	35.072039
1174.810878	119224.809064	35.077056
1175.890525	119433.855241	35.082074
1177.043276	119643.447963	35.087092
1178.302745	119850.159927	35.092109
1179.512808	120055.361087	35.097127
1180.227205	120261.560951	35.102144
1181.419493	120491.124941	35.107162
1182.511194	120698.213688	35.112180
1183.462361	120915.656337	35.117197
1184.611183	121136.019536	35.122215
1185.859027	121358.192327	35.127232
1187.029707	121592.850382	35.132250
1188.435057	121806.799983	35.137268
1189.377839	122035.962292	35.142285
1191.080798	122265.984732	35.147303
1192.181855	122474.858419	35.152320
1193.827604	122688.088745	35.157338
1195.714953	122887.109986	35.162356
1196.673188	123105.099531	35.167373
1197.773658	123320.417443	35.172391
1199.504166	123522.840962	35.177408
1200.577570	123729.598786	35.182426
1201.511592	123935.507355	35.187444
1202.744365	124150.821153	35.192461
1204.039822	124362.716337	35.197479
1205.542736	124558.480956	35.202496
1206.482522	124769.121696	35.207514
1208.027380	124966.846284	35.212532
1208.965685	125179.796860	35.217549
1209.855767	125385.279053	35.222567
1211.317481	125599.765287	35.227584
1212.215325	125815.033985	35.232602
1213.570469	126040.518007	35.237620
1214.339269	126260.932597	35.242637
1215.251392	126483.783199	35.247655
1216.851498	126706.745771	35.252672
1217.588533	126941.823252	35.257690
1218.724523	127156.832292	35.262708
1220.065780	127389.629512	35.267725
1221.005340	127609.048350	35.272743
1222.261975	127827.907406	35.277760
1223.407362	128046.457456	35.282778
1225.126568	128244.844809	35.287796
1226.391229	128459.561849	35.292813
1227.424794	128679.605835	35.297831
1228.628405	128886.667188	35.302848
1229.515780	129108.450455	35.307866
1230.606078	129329.439947	35.312884
1232.160541	129551.213508	35.317901
1233.212376	129775.305722	35.322919
1234.692895	129983.315563	35.327936
1235.874309	130213.194544	35.332954
1237.195011	130432.770454	35.337972
1238.495432	130653.276746	35.342989
1239.673702	130883.439947	35.348007
1240.985831	131103.643067	35.353024
1241.966588	131337.646428	35.358042
1243.112913	131568.973595	35.363060
1244.692922	131795.816462	35.368077
1245.767199	132023.508131	35.373095
1247.741513	132247.548330	35.378112
1249.082162	132469.670130	35.383130
1250.684776	132680.807773	35.388148
1252.229253	132905.128906	35.393165
1253.240122	133111.793957	35.398183
1254.928277	133310.433355	35.403200
1256.280781	133528.680860	35.408218
1257.567166	133742.516482	35.413236
1258.703510	133952.651796	35.418253
1259.301502	134172.199102	35.423271
1260.967356	134384.668056	35.428288
1262.300137	134601.151047	35.433306
1263.718270	134810.026427	35.438324
1265.373566	135025.163763	35.443341
1266.540972	135231.650421	35.448359
1267.794081	135438.529403	35.453376
1268.690235	135660.723357	35.458394
1269.990983	135863.425481	35.463412
1271.535145	136076.851590	35.468429
1272.681549	136293.237961	35.473447
1273.874509	136502.124393	35.478464
1275.288674	136720.115949	35.483482
1276.480646	136936.105580	35.488500
1277.981487	137142.382045	35.493517
1279.235470	137360.861596	35.498535
1280.599708	137558.846262	35.503552
1281.622038	137783.543099	35.508570
1282.940656	137987.814462	35.513588
1284.219333	138200.576630	35.518605
1284.987244	138436.720397	35.523623
1286.674230	138649.225256	35.528640
1287.816172	138870.599281	35.533658
1288.828168	139098.654010	35.538676
1290.104774	139321.364642	35.543693
1291.439816	139538.347916	35.548711
1293.192777	139732.436448	35.553728
1294.111757	139946.513622	35.558746
1295.243561	140157.182678	35.563764
1297.224154	140353.049015	35.568781
1297.956813	140566.718070	35.573799
1299.398084	140769.907012	35.578816
1300.513132	140990.056428	35.583834
1301.673964	141200.080074	35.588852
1302.520267	141418.350686	35.593869
1303.385455	141642.059563	35.598887
1304.702728	141864.500449	35.603904
1305.437787	142104.402903	35.608922
1306.138372	142344.705997	35.613940
1307.136736	142590.273222	35.618957
1308.304274	142856.065421	35.623975
1309.319754	143116.419890	35.628992
1310.505695	143396.657215	35.634010
1311.667670	143669.431297	35.639028
1313.622933	143936.770660	35.644045
1314.933988	144208.191714	35.649063
1316.032310	144476.708996	35.654080
1317.460023	144753.808392	35.659098
1318.654250	145047.500138	35.664116
1320.476958	145313.578768	35.669133
1321.276712	145599.454095	35.674151
1322.561026	145871.120417	35.679168
1323.958612	146157.506523	35.684186
1325.449980	146439.833031	35.689204
1326.890473	146727.065961	35.694221
1327.954163	147014.467081	35.699239
1329.494859	147292.314597	35.704256
1330.610071	147581.816663	35.709274
1332.099180	147875.188762	35.714292
1333.696072	148153.464307	35.719309
1335.435634	148443.373510	35.724327
1338.005448	148709.374039	35.729344
1339.625962	148978.430786	35.734362
1340.702925	149242.077791	35.739380
1342.516940	149496.024267	35.744397
1343.623755	149762.675825	35.749415
1344.641925	150028.494604	35.754432
1345.806194	150287.123778	35.759450
1346.751192	150557.169843	35.764468
1348.318408	150831.550764	35.769485
1349.238867	151116.280539	35.774503
1350.724446	151388.053761	35.779520
1352.160778	151654.547917	35.784538
1353.454203	151943.317020	35.789556
1355.091143	152211.011063	35.794573
1356.230269	152497.552831	35.799591
1357.645015	152767.229485	35.804608
1359.118149	153037.925479	35.809626
1360.644513	153317.075104	35.814644
1362.746076	153577.214838	35.819661
1363.972813	153836.529269	35.824679
1365.829200	154078.117861	35.829696
1367.318968	154310.827547	35.834714
1369.071197	154544.140628	35.839732
1370.301172	154766.876013	35.844749
1371.755070	155005.596112	35.849767
1373.453531	155225.069804	35.854784
1374.249812	155457.270594	35.859802
1375.539006	155700.983115	35.864820
1377.175594	155925.025400	35.869837
1378.597400	156159.482733	35.874855
1379.771548	156387.729643	35.879872
1381.476613	156615.988455	35.884890
1382.900861	156857.198367	35.889908
1384.161241	157092.094671	35.894925
1385.204433	157329.579432	35.899943
1386.113014	157574.345181	35.904960
1387.394238	157814.874787	35.909978
1388.368995	158080.742378	35.914996
1389.600600	158335.619229	35.920013
1390.842058	158606.443055	35.925031
1391.578135	158878.433518	35.930048
1393.079691	159150.079066	35.935066
1393.674986	159435.938558	35.940084
1394.964655	159732.680760	35.945101
1396.200215	160026.973030	35.950119
1397.442444	160327.571730	35.955136
1399.133543	160623.096970	35.960154
1400.184891	160940.188045	35.965172
1401.673935	161231.311537	35.970189
1402.997602	161550.593535	35.975207
1404.773906	161854.359628	35.980224
1406.345037	162153.417788	35.985242
1407.551049	162462.906436	35.990260
1409.110848	162773.339092	35.995277
1410.233478	163092.007157	36.000295
1411.737353	163398.038438	36.005312
1413.371172	163704.684033	36.010330
1414.837365	164023.388916	36.015348
1416.386771	164330.979580	36.020365
1417.767942	164647.191243	36.025383
1419.074184	164963.278416	36.030400
1420.623365	165279.516591	36.035418
1422.426659	165582.694928	36.040436
1425.130444	165853.644004	36.045453
1427.020431	166135.646404	36.050471
1429.151426	166420.299378	36.055488
1431.108570	166677.727935	36.060506
1432.785886	166953.782649	36.065524
1434.665793	167197.358229	36.070541
1436.297436	167456.864495	36.075559
1437.520405	167700.479063	36.080576
1439.410460	167955.718408	36.085594
1441.001032	168188.778570	36.090612
1442.256136	168424.232191	36.095629
1444.042641	168656.969333	36.100647
1445.574740	168870.742159	36.105664
1446.990515	169084.624708	36.110682
1447.940024	169301.620883	36.115700
1448.982499	169519.426993	36.120717
1450.404637	169742.613084	36.125735
1451.704053	169968.803368	36.130752
1453.408720	170180.154275	36.135770
1454.453190	170409.803912	36.140788
1455.584207	170643.830624	36.145805
1456.920212	170875.069650	36.150823
1458.085588	171110.412560	36.155840
1459.876819	171350.814467	36.160858
1460.632149	171602.587745	36.165876
1461.504636	171863.047915	36.170893
1462.774773	172118.720587	36.175911
1463.913142	172394.874324	36.180928
1464.729318	172672.531508	36.185946
1465.644144	172967.178929	36.190964
1466.984140	173261.717299	36.195981
1468.238649	173563.023607	36.200999
1469.356370	173872.083954	36.206016
1470.632294	174187.033179	36.211034
1471.862034	174506.053466	36.216052
1473.508145	174827.771226	36.221069
1474.741659	175141.515421	36.226087
1476.357990	175476.631741	36.231104
1477.775614	175800.971214	36.236122
1479.191654	176148.284673	36.241140
1480.916949	176470.583229	36.246157
1482.591017	176804.200878	36.251175
1483.862396	177142.077904	36.256192
1485.919216	177469.390051	36.261210
1487.402321	177805.141056	36.266228
1488.835547	178132.526059	36.271245
1490.237587	178464.386079	36.276263
1492.041180	178800.012527	36.281280
1493.753257	179129.856436	36.286298
1494.795119	179476.913673	36.291316
1496.514849	179806.798591	36.296333
1498.414462	180138.317496	36.301351
1499.039362	180486.061934	36.306368
1500.810869	180823.559835	36.311386
1502.449302	181165.677398	36.316404
1503.893000	181503.464130	36.321421
1505.523106	181831.853719	36.326439
1507.077667	182176.390972	36.331456
1508.724448	182518.706025	36.336474
1510.421988	182865.114404	36.341492
1511.967801	183202.513364	36.346509
1513.644199	183539.054273	36.351527
1515.172137	183874.124807	36.356544
1516.685974	184214.987964	36.361562
1518.753777	184560.556535	36.366580
1519.592796	184880.620301	36.371597
1521.295516	185218.689993	36.376615
1522.760825	185541.036706	36.381632
1524.074503	185866.940058	36.386650
1525.439868	186204.476691	36.391668
1526.888857	186531.744276	36.396685
1529.026308	186843.231480	36.401703
1530.651721	187168.200226	36.406720
1531.719806	187483.986721	36.411738
1533.430262	187834.980311	36.416756
1534.421365	188199.555041	36.421773
1535.834267	188539.635840	36.426791
1537.181688	188878.536500	36.431808
1538.964725	189214.876401	36.436826
1540.440487	189543.996758	36.441844
1541.966573	189886.668183	36.446861
1543.632063	190235.753906	36.451879
1544.920000	190576.045252	36.456896
1546.601338	190921.894985	36.461914
1547.950730	191265.505667	36.466932
1549.396398	191610.612476	36.471949
1551.311603	191954.993390	36.476967
1552.740308	192299.649866	36.481984
1554.784176	192652.708751	36.487002
1556.391819	192998.836440	36.492020
1558.260431	193343.639114	36.497037
1559.772399	193675.174469	36.502055
1561.554857	194025.353000	36.507072
1562.742648	194377.526812	36.512090
1564.329066	194721.559889	36.517108
1565.885680	195084.084799	36.522125
1566.811623	195433.579495	36.527143
1568.309756	195805.932181	36.532160
1569.484116	196167.703172	36.537178
1571.311411	196536.740738	36.542196
1573.171729	196905.533440	36.547213
1575.060762	197263.836237	36.552231
1576.899786	197626.136063	36.557248
1578.775342	197970.377488	36.562266
1581.099900	198307.205329	36.567284
1583.298167	198649.426968	36.572301
1585.165783	198976.141042	36.577319
1586.836017	199307.308777	36.582336
1588.363668	199644.774545	36.587354
1589.843713	199977.577703	36.592372
1591.348259	200310.136974	36.597389
1593.093719	200641.716995	36.602407
1593.890264	200992.988535	36.607424
1595.532341	201321.808743	36.612442
1597.002859	201654.925930	36.617460
1598.602552	202018.215858	36.622477
1599.982137	202366.765896	36.627495
1601.323097	202720.466475	36.632512
1602.415885	203069.513237	36.637530
1603.371627	203437.122945	36.642548
1604.447278	203812.040213	36.647565
1605.913235	204184.556214	36.652583
1607.054259	204562.005392	36.657600
1608.546631	204935.193421	36.662618
1609.871157	205308.361148	36.667636
1611.358678	205693.705090	36.672653
1612.490461	206083.009927	36.677671
1613.754129	206478.350870	36.682688
1615.416563	206879.606143	36.687706
1617.224601	207288.152405	36.692724
1618.079467	207698.146266	36.697741
1620.112720	208106.035829	36.702759
1621.840240	208507.808463	36.707776
1623.372406	208914.238521	36.712794
1625.665750	209332.832048	36.717812
1626.754515	209754.147956	36.722829
1628.619055	210169.390395	36.727847
1630.133204	210604.123147	36.732864
1631.475734	211024.995395	36.737882
1633.604299	211440.909736	36.742900
1635.547475	211866.584750	36.747917
1637.651271	212278.088108	36.752935
1639.440694	212706.358445	36.757952
1640.826476	213124.159945	36.762970
1642.995715	213541.905453	36.767988
1644.022999	213970.032602	36.773005
1645.696043	214397.111470	36.778023
1647.207032	214822.721489	36.783040
1649.192867	215247.058423	36.788058
1650.894206	215673.960263	36.793076
1652.240285	216115.630209	36.798093
1654.572481	216527.290502	36.803111
1656.177673	216959.903451	36.808128
1658.361020	217366.512940	36.813146
1660.540974	217783.436394	36.818164
1661.802560	218207.071472	36.823181
1663.902223	218619.694212	36.828199
1665.330510	219043.431087	36.833216
1666.844485	219452.220412	36.838234
1669.087006	219857.813336	36.843252
1670.783459	220278.486631	36.848269
1672.716802	220679.208027	36.853287
1675.020381	221073.720876	36.858304
1676.585974	221470.952083	36.863322
1678.480091	221870.058802	36.868340
1680.316855	222268.871900	36.873357
1682.381472	222655.760345	36.878375
1684.265051	223037.499479	36.883392
1685.861964	223418.984065	36.888410
1687.855084	223791.537509	36.893428
1689.342891	224180.307473	36.898445
1691.069892	224552.603923	36.903463
1692.549786	224941.834787	36.908480
1694.156595	225319.564253	36.913498
1696.065362	225708.851055	36.918516
1697.609697	226089.539858	36.923533
1699.218986	226461.582515	36.928551
1700.509590	226826.390796	36.933568
1702.254199	227187.388506	36.938586
1703.946942	227543.874733	36.943604
1705.621221	227919.974312	36.948621
1707.020415	228276.512617	36.953639
1709.229666	228644.749972	36.958656
1710.838940	229002.244757	36.963674
1713.179027	229367.489653	36.968692
1714.382354	229726.554289	36.973709
1716.299212	230097.207567	36.978727
1717.825591	230466.937904	36.983744
1719.284830	230831.879795	36.988762
1720.937053	231202.199967	36.993780
1722.419994	231583.421689	36.998797
1724.025983	231961.778309	37.003815
1725.468413	232346.717330	37.008832
1726.650813	232749.279505	37.013850
1728.300724	233140.509794	37.018868
1729.889816	233552.885451	37.023885
1731.624754	233955.635318	37.028903
1733.176279	234374.217298	37.033920
1735.061422	234784.182784	37.038938
1737.078816	235197.631994	37.043956
1739.090794	235590.913986	37.048973
1741.315747	235981.620158	37.053991
1743.446650	236387.330330	37.059008
1744.904948	236787.847377	37.064026
1746.505620	237192.328969	37.069044
1748.203433	237607.234976	37.074061
1749.430677	238027.328118	37.079079
1751.375983	238448.747150	37.084096
1752.465791	238864.801050	37.089114
1754.424976	239297.548679	37.094132
1755.522777	239731.079527	37.099149
1757.183708	240167.969539	37.104167
1758.696933	240604.733180	37.109184
1759.986883	241071.332838	37.114202
1761.903199	241524.388259	37.119220
1763.564156	241985.820159	37.124237
1765.315884	242452.495634	37.129255
1766.876336	242919.814254	37.134272
1767.988301	243405.601858	37.139290
1769.613339	243874.663695	37.144308
1771.488248	244362.887944	37.149325
1773.359818	244848.217570	37.154343
1775.662919	245326.412081	37.159360
1777.676365	245803.564460	37.164378
1780.203907	246264.778114	37.169396
1782.478883	246726.645190	37.174413
1784.158023	247197.810576	37.179431
1786.095424	247653.741336	37.184448
1787.955173	248121.828464	37.189466
1790.025881	248583.707038	37.194484
1791.605172	249044.958817	37.199501
1793.134924	249495.219954	37.204519
1795.293075	249936.889328	37.209536
1796.918689	250382.638411	37.214554
1798.899931	250806.327883	37.219572
1800.788063	251244.106869	37.224589
1802.361674	251684.277005	37.229607
1804.163436	252116.431764	37.234624
1805.771365	252552.633592	37.239642
1807.449953	252992.684808	37.244660
1809.224666	253437.012894	37.249677
1811.126911	253877.686669	37.254695
1813.455321	254314.985265	37.259712
1815.052373	254761.935280	37.264730
1816.918040	255203.149125	37.269748
1818.605468	255645.841516	37.274765
1820.205456	256099.015037	37.279783
1822.006218	256553.144971	37.284800
1823.441053	257022.147579	37.289818
1825.393262	257479.808050	37.294836
1826.807856	257949.652371	37.299853
1828.259933	258433.157135	37.304871
1830.445282	258901.142036	37.309888
1832.321078	259391.051914	37.314906
1834.121011	259861.541183	37.319924
1835.991318	260349.343205	37.324941
1837.496725	260833.778008	37.329959
1839.310042	261316.483299	37.334976
1840.582454	261822.016652	37.339994
1842.719438	262316.884909	37.345012
1844.146975	262809.486296	37.350029
1846.617358	263329.674495	37.355047
1848.953912	263817.953517	37.360064
1850.694993	264316.469791	37.365082
1852.552633	264821.951493	37.370100
1854.549649	265321.235924	37.375117
1856.554020	265813.380345	37.380135
1859.196791	266293.399446	37.385152
1861.393663	266788.354972	37.390170
1863.317642	267267.860828	37.395188
1865.215110	267760.351472	37.400205
1867.262255	268241.638630	37.405223
1868.838694	268714.800558	37.410240
1871.390252	269191.249807	37.415258
1873.204574	269661.473795	37.420276
1875.057119	270139.260535	37.425293
1876.648685	270619.047166	37.430311
1878.868612	271105.253994	37.435328
1880.608710	271584.912007	37.440346
1882.518514	272046.224969	37.445364
1884.423649	272530.323914	37.450381
1886.110573	273014.383070	37.455399
1888.194344	273492.835704	37.460416
1890.011931	273979.131429	37.465434
1891.410968	274453.634906	37.470452
1893.420512	274942.054983	37.475469
1894.766331	275428.402941	37.480487
1896.571830	275895.899066	37.485504
1897.658059	276373.296965	37.490522
1899.558799	276865.185974	37.495540
1901.114631	277349.054985	37.500557
1902.230826	277853.192459	37.505575
1904.233045	278349.480340	37.510592
1905.897469	278872.293250	37.515610
1907.111252	279388.958362	37.520628
1909.219652	279917.610912	37.525645
1910.827926	280448.989169	37.530663
1913.167306	280976.455933	37.535680
1914.540685	281519.631864	37.540698
1916.381600	282059.855701	37.545716
1918.286339	282604.918427	37.550733
1920.124554	283161.192506	37.555751
1922.042530	283711.735729	37.560768
1923.651596	284280.542194	37.565786
1925.483243	284849.791022	37.570804
1927.320875	285427.952222	37.575821
1929.208746	286005.518270	37.580839
1931.264772	286581.554540	37.585856
1933.261402	287162.932613	37.590874
1935.379745	287744.134950	37.595892
1938.199614	288313.581488	37.600909
1940.291422	288891.862240	37.605927
1942.269554	289461.701642	37.610944
1944.454730	290022.841713	37.615962
1946.870127	290588.918171	37.620980
1949.445690	291151.230850	37.625997
1951.760711	291700.098340	37.631015
1954.315330	292237.695789	37.636032
1956.159627	292797.788875	37.641050
1958.400118	293345.772287	37.646068
1960.431103	293874.485662	37.651085
1961.921715	294429.881449	37.656103
1964.263201	294969.762676	37.661120
1966.134692	295508.019854	37.666138
1967.784361	296062.287813	37.671156
1969.508097	296614.711471	37.676173
1971.287925	297172.481559	37.681191
1973.105928	297719.092323	37.686208
1975.169236	298291.487739	37.691226
1976.725222	298852.867795	37.696244
1978.996554	299412.598406	37.701261
1980.563070	299987.278359	37.706279
1982.733628	300552.733901	37.711296
1984.812381	301127.014500	37.716314
1986.519648	301703.437593	37.721332
1988.549722	302273.300249	37.726349
1990.244016	302854.416608	37.731367
1992.251781	303435.043803	37.736384
1994.522347	304021.793486	37.741402
1996.436478	304599.660719	37.746420
1998.453224	305179.919100	37.751437
2000.511771	305757.448992	37.756455
2001.995891	306321.613472	37.761472
2004.102038	306881.198119	37.766490
2005.296984	307449.848472	37.771508
2007.609807	308025.058708	37.776525
2009.495535	308596.680970	37.781543
2011.702703	309156.613355	37.786560
2013.674718	309727.044453	37.791578
2016.130577	310312.244237	37.796596
2018.519863	310867.536672	37.801613
2020.771738	311438.872071	37.806631
2022.708759	312011.577413	37.811648
2024.889512	312577.075660	37.816666
2026.927075	313140.994242	37.821684
2029.204014	313703.674015	37.826701
2031.093170	314270.478552	37.831719
2033.652098	314833.736003	37.836736
2035.765030	315397.928554	37.841754
2037.587477	315971.485180	37.846772
2039.860189	316529.267720	37.851789
2041.732387	317105.167819	37.856807
2044.033031	317660.524064	37.861824
2046.409995	318222.185124	37.866842
2048.463716	318792.758249	37.871860
2050.352339	319352.284174	37.876877
2052.155679	319936.245822	37.881895
2054.087990	320509.973128	37.886912
2055.934287	321089.346653	37.891930
2057.901698	321680.830638	37.896948
2059.525580	322276.811024	37.901965
2061.365656	322870.336723	37.906983
2063.410230	323467.655535	37.912000
2065.524514	324067.546280	37.917018
2066.810006	324677.626802	37.922036
2069.249471	325284.964932	37.927053
2071.066603	325905.452889	37.932071
2073.147074	326528.529645	37.937088
2075.175124	327155.366116	37.942106
2077.143291	327791.117062	37.947124
2079.539271	328409.854529	37.952141
2080.994239	329036.159175	37.957159
2083.720630	329675.516680	37.962176
2085.884526	330299.502761	37.967194
2088.007124	330928.997662	37.972212
2089.859043	331556.881566	37.977229
2092.105996	332203.222103	37.982247
2093.960604	332838.122509	37.987264
2095.739918	333468.865147	37.992282
2097.889542	334128.526178	37.997300
2100.135984	334778.922523	38.002317
2102.260185	335436.109191	38.007335
2103.863814	336087.741377	38.012352
2106.107239	336738.494400	38.017370
2107.628408	337418.375354	38.022388
2109.402148	338086.172612	38.027405
2111.870338	338754.146815	38.032423
2113.817341	339400.956471	38.037440
2116.317058	340047.663134	38.042458
2117.744409	340695.432966	38.047476
2120.272319	341344.198873	38.052493
2122.630460	341997.959673	38.057511
2124.669196	342645.040383	38.062528
2127.002466	343298.406883	38.067546
2128.798141	343952.313076	38.072564
2131.133893	344584.063248	38.077581
2133.736014	345237.128267	38.082599
2136.376669	345871.371973	38.087616
2139.156533	346506.953497	38.092634
2141.736404	347137.789295	38.097652
2144.570513	347755.757187	38.102669
2146.807755	348376.762348	38.107687
2148.857939	348998.958151	38.112704
2151.476827	349607.852234	38.117722
2154.040569	350218.955009	38.122740
2156.499736	350818.774923	38.127757
2159.029156	351421.315051	38.132775
2160.997254	352016.000354	38.137792
2163.364908	352613.019659	38.142810
2165.073155	353227.905302	38.147828
2166.727615	353826.222045	38.152845
2168.613934	354438.471423	38.157863
2170.319529	355062.338239	38.162880
2172.505532	355686.341877	38.167898
2174.127138	356323.575443	38.172916
2176.447515	356960.197540	38.177933
2178.336263	357601.196632	38.182951
2180.176529	358246.405453	38.187968
2182.556833	358895.190323	38.192986
2184.210814	359560.630274	38.198004
2186.227553	360222.876529	38.203021
2187.812511	360889.193842	38.208039
2190.088289	361579.989640	38.213056
2192.138420	362251.201833	38.218074
2193.840419	362948.996933	38.223092
2195.711476	363645.684990	38.228109
2197.593548	364357.299694	38.233127
2199.277651	365078.117609	38.238144
2202.013613	365799.452114	38.243162
2203.841229	366528.791356	38.248180
2206.290289	367255.879327	38.253197
2208.376978	367994.505114	38.258215
2210.295328	368733.373054	38.263232
2212.718467	369477.897223	38.268250
2215.175585	370216.668162	38.273268
2217.254137	370956.021226	38.278285
2219.834695	371694.436173	38.283303
2222.037850	372440.889137	38.288320
2225.042116	373183.917723	38.293338
2227.158089	373921.224112	38.298356
2229.599374	374650.217248	38.303373
2232.443330	375370.148907	38.308391
2234.741870	376067.462495	38.313408
2237.236376	376754.407456	38.318426
2239.493497	377450.305052	38.323444
2241.634779	378130.182241	38.328461
2243.728876	378831.074519	38.333479
2245.506633	379522.852518	38.338496
2247.781866	380207.558188	38.343514
2249.885304	380915.504392	38.348532
2251.936410	381618.246535	38.353549
2254.394225	382322.070275	38.358567
2256.627266	383031.089277	38.363584
2259.344514	383734.584341	38.368602
2261.135289	384446.005545	38.373620
2263.868868	385149.999034	38.378637
2265.990467	385864.348781	38.383655
2268.071165	386584.190428	38.388672
2270.626225	387297.596893	38.393690
2272.653458	388023.397143	38.398708
2274.818810	388736.304840	38.403725
2277.150197	389457.532620	38.408743
2279.188768	390189.312808	38.413760
2281.365309	390917.832740	38.418778
2283.453560	391667.590658	38.423796
2285.797677	392412.369068	38.428813
2288.208705	393148.981685	38.433831
2289.843195	393917.186899	38.438848
2292.513215	394668.138666	38.443866
2294.671434	395439.661544	38.448884
2296.703320	396200.465757	38.453901
2299.220074	396957.999465	38.458919
2301.510323	397734.760820	38.463936
2304.443566	398495.528068	38.468954
2306.816034	399269.370390	38.473972
2309.514801	400039.005616	38.478989
2311.548432	400798.978290	38.484007
2313.477683	401588.340296	38.489024
2315.795103	402358.180104	38.494042
2318.421336	403135.749510	38.499060
2320.119642	403900.889201	38.504077
2322.863022	404675.608364	38.509095
2325.329058	405459.372099	38.514112
2328.067608	406243.674753	38.519130
2330.114148	407019.865196	38.524148
2332.203090	407815.962495	38.529165
2334.553112	408595.247524	38.534183
2336.394423	409399.446171	38.539200
2338.916342	410186.761097	38.544218
2340.931712	410996.834077	38.549236
2343.005933	411804.491193	38.554253
2345.869238	412605.175384	38.559271
2348.169916	413412.440104	38.564288
2350.707667	414219.867070	38.569306
2353.055967	415021.881525	38.574324
2355.540971	415829.469532	38.579341
2358.190201	416616.339831	38.584359
2360.329832	417401.981372	38.589376
2362.880338	418167.422528	38.594394
2365.235886	418927.505576	38.599412
2367.155411	419705.794855	38.604429
2369.638516	420475.658592	38.609447
2371.647511	421251.402791	38.614464
2374.431582	422030.585257	38.619482
2377.001840	422813.678381	38.624500
2379.379777	423586.905822	38.629517
2381.875055	424362.012589	38.634535
2383.991966	425142.475311	38.639552
2386.606175	425920.043174	38.644570
2389.352666	426698.271953	38.649588
2391.465329	427480.329908	38.654605
2394.094168	428259.945197	38.659623
2396.431552	429047.582762	38.664640
2398.608472	429836.537486	38.669658
2400.797644	430635.030327	38.674676
2403.150646	431432.911017	38.679693
2405.551872	432232.527517	38.684711
2407.703225	433046.026918	38.689728
2410.231817	433859.989750	38.694746
2412.808217	434670.170356	38.699764
2414.985947	435489.448973	38.704781
2417.305837	436316.163271	38.709799
2419.569307	437148.979935	38.714816
2421.876256	437973.864393	38.719834
2424.527349	438816.824904	38.724852
2426.455276	439660.130048	38.729869
2428.502137	440503.585111	38.734887
2430.658697	441364.595835	38.739904
2433.104777	442225.776213	38.744922
2435.607593	443099.003899	38.749940
2437.618165	443981.133482	38.754957
2439.810902	444856.164490	38.759975
2442.172304	445751.212816	38.764992
2444.467184	446641.227499	38.770010
2446.579042	447545.095055	38.775028
2448.936160	448455.912395	38.780045
2451.415925	449360.651003	38.785063
2453.295092	450299.084250	38.790080
2456.026721	451228.429215	38.795098
2458.651130	452152.137864	38.800116
2460.710940	453092.588568	38.805133
2463.543238	454025.178587	38.810151
2466.225360	454965.639396	38.815168
2468.784454	455890.505639	38.820186
2471.720552	456824.062166	38.825204
2474.624219	457762.737620	38.830221
2477.129761	458684.653973	38.835239
2480.074169	459615.956179	38.840256
2482.087984	460548.789190	38.845274
2484.863282	461472.097314	38.850292
2487.374875	462397.479530	38.855309
2490.460720	463300.077926	38.860327
2493.924869	464169.113797	38.865344
2496.654127	465031.970005	38.870362
2499.732188	465885.682658	38.875380
2502.136939	466748.214528	38.880397
2505.035413	467586.268275	38.885415
2507.217332	468435.675276	38.890432
2509.249571	469281.078556	38.895450
2511.989817	470128.899819	38.900468
2513.885386	470987.790271	38.905485
2516.314298	471845.590552	38.910503
2518.790950	472716.628981	38.915520
2521.215630	473580.008181	38.920538
2524.030702	474450.958198	38.925556
2525.672444	475331.613844	38.930573
2528.327915	476218.518944	38.935591
2531.239828	477093.216554	38.940608
2533.752918	477967.889982	38.945626
2536.293633	478838.426298	38.950644
2538.689714	479745.151289	38.955661
2541.044376	480633.407695	38.960679
2543.723602	481532.824292	38.965696
2546.083105	482428.817159	38.970714
2548.565332	483332.518908	38.975732
2550.495492	484244.851230	38.980749
2552.992912	485164.611700	38.985767
2555.564222	486091.277522	38.990784
2558.241377	487018.633461	38.995802
2561.504424	487938.571987	39.000820
2563.816814	488860.037512	39.005837
2566.868634	489775.322070	39.010855
2569.316584	490707.062331	39.015872
2572.024956	491634.771564	39.020890
2574.915018	492556.041622	39.025908
2577.117702	493497.057410	39.030925
2580.059129	494421.497375	39.035943
2582.590875	495360.234441	39.040960
2584.645903	496296.326923	39.045978
2587.556832	497231.363357	39.050996
2589.816573	498178.464055	39.056013
2592.338511	499128.139358	39.061031
2594.880221	500071.956666	39.066048
2597.130739	501037.456294	39.071066
2599.585233	501997.670016	39.076084
2601.835448	502979.344578	39.081101
2604.449974	503947.535257	39.086119
2606.919225	504924.567274	39.091136
2608.904786	505918.008995	39.096154
2610.890671	506923.186634	39.101172
2613.668648	507928.266776	39.106189
2615.868527	508950.571973	39.111207
2618.748613	509966.696964	39.116224
2620.954262	510992.902148	39.121242
2623.562984	512020.987688	39.126260
2626.197584	513067.093675	39.131277
2628.699782	514096.018877	39.136295
2631.471082	515102.558086	39.141312
2633.853433	516119.377218	39.146330
2636.385875	517138.270262	39.151348
2639.002668	518140.657771	39.156365
2641.702688	519143.670780	39.161383
2644.155308	520160.512688	39.166400
2646.774055	521180.481862	39.171418
2649.646018	522204.620191	39.176436
2652.712047	523235.051867	39.181453
2655.007334	524267.659653	39.186471
2658.149438	525292.951359	39.191488
2660.994576	526324.668343	39.196506
2664.002400	527345.611923	39.201524
2666.679603	528379.127784	39.206541
2669.077164	529409.497733	39.211559
2671.494912	530442.157762	39.216576
2674.150828	531485.274357	39.221594
2677.134344	532523.378133	39.226612
2679.399549	533581.963145	39.231629
2682.199218	534642.694119	39.236647
2684.872913	535690.889095	39.241664
2687.728273	536749.442078	39.246682
2691.152459	537808.825583	39.251700
2693.678514	538870.346228	39.256717
2696.453014	539918.363764	39.261735
2699.828464	540969.420000	39.266752
2702.561737	542022.116824	39.271770
2705.751192	543063.491354	39.276788
2708.543594	544117.428358	39.281805
2711.070587	545166.201563	39.286823
2713.845757	546212.640446	39.291840
2716.208218	547276.466664	39.296858
2719.173470	548310.093663	39.301876
2722.077701	549379.747226	39.306893
2724.737007	550432.016697	39.311911
2727.706334	551485.760031	39.316928
2730.545446	552541.303073	39.321946
2733.655763	553581.288834	39.326964
2736.505886	554646.665435	39.331981
2739.297088	555690.612284	39.336999
2742.091119	556734.426604	39.342016
2744.834711	557793.992754	39.347034
2748.254202	558830.401132	39.352052
2750.751953	559874.168971	39.357069
2753.949459	560909.999309	39.362087
2756.874701	561946.246147	39.367104
2759.375146	562998.703947	39.372122
2762.564810	564016.511195	39.377140
2764.773626	565077.637707	39.382157
2766.955737	566117.544383	39.387175
2770.168488	567160.454013	39.392192
2772.224544	568222.501630	39.397210
2774.902562	569280.037866	39.402228
2777.445865	570347.095500	39.407245
2779.531427	571409.323597	39.412263
2782.012245	572454.684219	39.417280
2784.179542	573505.982682	39.422298
2786.515396	574556.612272	39.427316
2789.149274	575624.461138	39.432333
2791.596442	576697.216608	39.437351
2794.372855	577769.973520	39.442368
2796.561808	578864.054030	39.447386
2799.252724	579971.442363	39.452404
2801.467918	581079.865108	39.457421
2803.803886	582209.828261	39.462439
2806.495291	583335.414296	39.467456
2808.821334	584494.547475	39.472474
2811.494742	585648.547496	39.477492
2814.793614	586809.748346	39.482509
2818.143726	587962.358028	39.487527
2821.383482	589126.902689	39.492544
2824.185361	590301.229579	39.497562
2827.202910	591456.113461	39.502580
2830.044829	592626.545358	39.507597
2832.999311	593796.891805	39.512615
2836.401632	594969.950161	39.517632
2839.256652	596141.982620	39.522650
2842.300787	597304.600266	39.527668
2845.025912	598489.288509	39.532685
2847.778222	599673.199837	39.537703
2850.615735	600856.223987	39.542720
2853.001846	602055.071753	39.547738
2855.969662	603248.639127	39.552756
2858.517310	604454.264756	39.557773
2861.038514	605665.571755	39.562791
2863.746883	606885.723675	39.567808
2866.637015	608119.671157	39.572826
2869.877560	609343.117788	39.577844
2873.080544	610571.238918	39.582861
2875.652667	611812.536333	39.587879
2878.456709	613032.951481	39.592896
2881.319523	614283.124107	39.597914
2884.227810	615527.597316	39.602932
2887.641119	616762.194620	39.607949
2890.597155	618008.377516	39.612967
2893.658649	619249.701634	39.617984
2896.482113	620485.227264	39.623002
2899.775265	621720.881284	39.628020
2903.054178	622956.445977	39.633037
2905.980823	624196.974382	39.638055
2909.698055	625425.085471	39.643072
2912.680998	626661.221823	39.648090
2915.604586	627877.447913	39.653108
2918.917474	629098.910616	39.658125
2921.675052	630329.413763	39.663143
2924.813792	631541.385840	39.668160
2927.568532	632768.258456	39.673178
2930.441025	633976.549285	39.678196
2933.968076	635187.083164	39.683213
2936.816262	636374.188396	39.688231
2940.263935	637555.266987	39.693248
2943.488112	638723.077547	39.698266
2946.053743	639865.876162	39.703284
2949.006445	641012.171853	39.708301
2951.567966	642174.713524	39.713319
2954.346733	643330.951481	39.718336
2956.729256	644499.689898	39.723354
2959.057620	645671.492903	39.728372
2962.471310	646850.301775	39.733389
2964.347512	648050.716894	39.738407
2967.203749	649245.238683	39.743424
2969.793714	650464.528219	39.748442
2972.055076	651682.926889	39.753460
2974.727391	652918.840646	39.758477
2977.249487	654173.852558	39.763495
2979.881819	655426.593467	39.768512
2982.985207	656703.794014	39.773530
2985.970899	657981.096393	39.778548
2989.409673	659259.696906	39.783565
2991.867779	660552.582836	39.788583
2995.063745	661837.405038	39.793600
2998.360927	663130.100435	39.798618
3001.365804	664435.857633	39.803636
3004.686498	665742.327684	39.808653
3007.542324	667057.055061	39.813671
3010.956606	668360.960210	39.818688
3013.932151	669683.310366	39.823706
3016.721898	671003.766233	39.828724
3019.673796	672335.145411	39.833741
3022.527790	673678.580589	39.838759
3025.620873	675012.735245	39.843776
3028.735390	676360.758599	39.848794
3031.754561	677708.502474	39.853812
3034.593111	679054.291662	39.858829
3037.800260	680411.742635	39.863847
3040.948271	681767.115091	39.868864
3044.041559	683124.132933	39.873882
3047.151653	684488.691073	39.878900
3050.840119	685841.129447	39.883917
3053.461456	687211.317546	39.888935
3056.436995	688566.198683	39.893952
3060.134741	689934.943609	39.898970
3062.963616	691293.158504	39.903988
3066.418647	692656.466376	39.909005
3069.089462	694019.946629	39.914023
3072.463071	695380.864932	39.919040
3075.903807	696739.528558	39.924058
3078.587321	698116.008228	39.929076
3081.937583	699481.103703	39.934093
3085.585356	700841.375014	39.939111
3088.822840	702192.980283	39.944128
3092.235932	703538.845038	39.949146
3095.517364	704888.931188	39.954164
3098.821447	706232.511239	39.959181
3101.758652	707557.917304	39.964199
3105.042519	708860.727521	39.969216
3108.132124	710155.103912	39.974234
3110.672176	711448.782769	39.979252
3114.581579	712741.881502	39.984269
3117.126053	714039.814999	39.989287
3120.113412	715330.941583	39.994304
3123.227814	716643.366523	39.999322
3125.699892	717939.224397	40.004340
3128.596462	719248.358370	40.009357
3131.375465	720570.903464	40.014375
3133.988237	721897.517176	40.019392
3137.573136	723231.215351	40.024410
3140.425133	724579.648711	40.029428
3144.056003	725921.501072	40.034445
3146.818655	727274.249142	40.039463
3149.418737	728637.222930	40.044480
3152.677074	729998.867598	40.049498
3155.273617	731384.345378	40.054516
3158.165054	732753.488901	40.059533
3161.572924	734144.030711	40.064551
3164.504790	735544.678048	40.069568
3167.588340	736953.787873	40.074586
3170.569368	738375.641193	40.079604
3174.312517	739794.051011	40.084621
3177.379396	741227.166697	40.089639
3180.491438	742656.167653	40.094656
3183.824299	744089.603600	40.099674
3186.656093	745525.721328	40.104692
3190.277861	746956.708421	40.109709
3193.706552	748403.725246	40.114727
3197.185433	749854.354954	40.119744
3200.345277	751305.554504	40.124762
3203.156962	752759.051211	40.129780
3206.325701	754211.029654	40.134797
3209.642220	755687.566592	40.139815
3212.331112	757157.329171	40.144832
3215.297825	758630.597847	40.149850
3218.402226	760123.186112	40.154868
3222.016600	761611.112263	40.159885
3225.149658	763096.071766	40.164903
3228.443354	764592.657286	40.169920
3231.427220	766100.203692	40.174938
3234.321074	767622.990821	40.179956
3237.522773	769135.486332	40.184973
3240.799047	770655.077679	40.189991
3243.386436	772182.282637	40.195008
3246.515974	773723.318339	40.200026
3249.631546	775275.863971	40.205044
3252.577329	776823.689698	40.210061
3255.759988	778383.070463	40.215079
3258.688278	779946.230846	40.220096
3262.048465	781519.868681	40.225114
3264.619466	783111.786160	40.230132
3267.653793	784693.954000	40.235149
3270.682474	786281.213230	40.240167
3273.637584	787862.690123	40.245184
3276.810498	789423.049216	40.250202
3279.890658	790999.196777	40.255220
3282.631046	792585.530525	40.260237
3286.113151	794177.009797	40.265255
3288.840568	795775.402807	40.270272
3292.387818	797379.651555	40.275290
3295.324648	798992.294602	40.280308
3298.593286	800616.245971	40.285325
3302.552294	802216.659407	40.290343
3305.799345	803847.529818	40.295360
3309.659664	805456.933668	40.300378
3313.212959	807081.650047	40.305396
3316.895934	808697.892810	40.310413
3320.693575	810313.094746	40.315431
3324.830610	811932.491609	40.320448
3328.576953	813526.954816	40.325466
3331.413156	815146.676456	40.330484
3335.177250	816747.495556	40.335501
3339.061818	818353.178405	40.340519
3342.337913	819963.405453	40.345536
3346.207767	821546.705005	40.350554
3349.314870	823156.229749	40.355572
3352.543768	824751.299770	40.360589
3355.848218	826363.171016	40.365607
3358.906267	827967.815664	40.370624
3362.697546	829572.766659	40.375642
3366.090112	831184.010598	40.380660
3369.664075	832799.494877	40.385677
3373.217289	834400.899267	40.390695
3376.346761	836021.342992	40.395712
3379.603980	837637.267080	40.400730
3382.780051	839254.253737	40.405748
3386.320702	840880.831099	40.410765
3389.523976	842514.630847	40.415783
3393.216402	844158.226314	40.420800
3396.290289	845781.479368	40.425818
3399.419896	847417.999565	40.430836
3402.332605	849073.940128	40.435853
3405.667670	850718.880954	40.440871
3408.712109	852393.137856	40.445888
3411.930449	854061.185322	40.450906
3415.752044	855743.132945	40.455924
3418.260115	857430.274661	40.460941
3421.539008	859121.860937	40.465959
3424.469280	860833.005475	40.470976
3428.174392	862550.415574	40.475994
3431.271989	864276.257558	40.481012
3434.228696	866010.733309	40.486029
3437.427791	867758.318798	40.491047
3440.417825	869517.625701	40.496064
3443.372445	871283.386619	40.501082
3446.410968	873065.440726	40.506100
3449.578392	874860.572166	40.511117
3453.129154	876633.984126	40.516122
3455.811499	878376.498544	40.521127
3458.806668	880062.740908	40.526132
3462.369491	881690.196643	40.531136
3465.650804	883248.505207	40.536141
3469.184451	884734.242007	40.541146
3472.500537	886157.992847	40.546151
3475.650902	887477.515706	40.551156
3478.825608	888738.019706	40.556160
3481.697505	889920.644629	40.561165
3484.247531	891029.695559	40.566170
3486.737561	892062.463399	40.571175
3489.331136	893024.180489	40.576180
3491.391541	893913.928169	40.581184
3493.516601	894744.392241	40.586189
3495.782592	895495.587190	40.591194
3497.962077	896183.135610	40.596199
3499.927284	896800.611013	40.601204
3501.928944	897372.717587	40.606208
3503.839251	897881.625549	40.611213
3505.373776	898332.711430	40.616218
3506.700282	898733.008986	40.621223
3508.496394	899066.386232	40.626228
3510.007082	899372.953253	40.631232
3511.334642	899619.487432	40.636237
3513.283568	899824.201246	40.641242
3514.361970	899988.319263	40.646247
3515.368668	900096.746347	40.651252
3516.595443	900176.850528	40.656256
3517.493517	900219.073772	40.661261
3518.933961	900231.473229	40.666266
3519.943097	900209.871480	40.671271
3520.832874	900157.303858	40.676276
3521.479886	900065.295755	40.681280
3522.261049	899950.095150	40.686285
3522.834597	899809.635157	40.691290
3523.866716	899648.144425	40.696295
3524.338599	899449.575936	40.701300
3524.852318	899246.552174	40.706304
3525.493229	899019.748141	40.711309
3526.304283	898773.498573	40.716314
3526.121099	898511.282678	40.721319
3526.888260	898244.450431	40.726324
3527.502044	897945.474562	40.731328
3527.777368	897632.537440	40.736333
3528.150802	897306.817749	40.741338
3528.502981	896980.889714	40.746343
3529.042230	896631.149631	40.751348
3529.488881	896270.778046	40.756352
3529.433699	895909.889535	40.761357
3530.305690	895515.006357	40.766362
3530.148191	895132.348451	40.771367
3530.345378	894721.390168	40.776372
3530.649812	894315.891724	40.781376
3530.607893	893906.751209	40.786381
3530.737977	893476.000134	40.791386
3530.927370	893056.224602	40.796391
3531.288035	892618.893566	40.801396
3531.334158	892177.522632	40.806400
3531.110030	891737.033705	40.811405
3531.753784	891294.428967	40.816410
3531.618103	890834.518893	40.821415
3532.463231	890375.564733	40.826420
3532.571182	889904.031225	40.831424
3532.570654	889434.798502	40.836429
3532.416278	888945.919199	40.841434
3532.814305	888470.639504	40.846439
3532.679730	887976.644294	40.851444
3532.635892	887487.912141	40.856448
3532.512302	886995.281897	40.861453
3532.789756	886497.412617	40.866458
3532.867198	886008.921241	40.871463
3533.142631	885508.547650	40.876468
3533.309027	885003.793871	40.881472
3532.863400	884498.519706	40.886477
3533.339816	883980.749814	40.891482
3533.239007	883483.072511	40.896487
3532.993133	882957.686263	40.901492
3533.145280	882447.677369	40.906496
3533.147330	881944.428035	40.911501
3533.240856	881421.750079	40.916506
3533.138168	880905.644895	40.921511
3533.436392	880388.747504	40.926516
3533.554505	879859.919648	40.931520
3533.288519	879329.656231	40.936525
3533.508547	878805.850317	40.941530
3533.376227	878281.282466	40.946535
3533.499040	877744.026003	40.951540
3533.500929	877210.908399	40.956544
3533.227353	876683.314176	40.961549
3533.427116	876149.291023	40.966554
3533.315308	875616.242014	40.971559
3533.478030	875082.031412	40.976564
3533.658015	874540.982179	40.981568
3533.259504	874002.988167	40.986573
3533.504457	873473.175485	40.991578
3533.840600	872934.182960	40.996583
3533.761321	872391.138441	41.001588
3533.616055	871850.189544	41.006592
3533.750457	871299.636195	41.011597
3533.970042	870752.607140	41.016602
3533.735589	870211.912359	41.021607
3533.826876	869655.974470	41.026612
3533.776491	869112.043111	41.031616
3533.640052	868557.400377	41.036621
3534.110890	868002.893678	41.041626
3533.809586	867449.243994	41.046631
3533.745098	866893.949297	41.051636
3533.862276	866333.814485	41.056640
3533.844432	865785.108698	41.061645
3533.789263	865225.191184	41.066650
3534.045313	864667.110848	41.071655
3534.250107	864104.519511	41.076660
3534.106190	863536.009647	41.081664
3534.013728	862977.929545	41.086669
3534.263193	862413.132763	41.091674
3533.991720	861847.691998	41.096679
3534.068808	861269.408805	41.101684
3534.197592	860711.664983	41.106688
3534.212665	860144.850230	41.111693
3534.373079	859566.682161	41.116698
3534.600585	858995.544239	41.121703
3534.031306	858414.183231	41.126708
3534.099245	857833.727546	41.131712
3534.060447	857265.389964	41.136717
3534.315815	856683.139868	41.141722
3534.470682	856115.343105	41.146727
3534.112613	855532.504756	41.151732
3534.260877	854947.870865	41.156736
3534.191458	854377.811441	41.161741
3534.477108	853798.784665	41.166746
3534.028507	853227.418521	41.171751
3534.007655	852638.117974	41.176756
3534.068211	852061.983169	41.181760
3534.091245	851485.411708	41.186765
3534.257164	850897.275856	41.191770
3533.850493	850325.244689	41.196775
3533.915340	849744.902062	41.201780
3533.889202	849166.565442	41.206784
3533.506868	848587.456781	41.211789
3533.549696	848010.364130	41.216794
3533.540123	847434.103519	41.221799
3533.282806	846853.156536	41.226804
3533.396585	846278.229197	41.231808
3533.123702	845714.323717	41.236813
3533.126869	845145.935899	41.241818
3533.240088	844576.113577	41.246823
3533.225208	844001.681273	41.251828
3533.367474	843432.042494	41.256832
3533.014616	842861.656904	41.261837
3533.212162	842279.623567	41.266842
3533.027145	841715.831381	41.271847
3533.061762	841152.828765	41.276852
3533.586952	840573.896955	41.281856
3533.384008	840000.935872	41.286861
3533.303764	839423.416102	41.291866
3533.065832	838856.988885	41.296871
3533.373205	838272.227359	41.301876
3532.973990	837698.116421	41.306880
3533.016032	837137.292133	41.311885
3533.208864	836550.294516	41.316890
3533.041157	835978.623318	41.321895
3533.066806	835397.792886	41.326900
3533.011294	834817.509091	41.331904
3533.013781	834250.826635	41.336909
3533.215753	833665.368189	41.341914
3532.862894	833100.255260	41.346919
3532.832370	832516.488852	41.351924
3533.033098	831939.464366	41.356928
3532.735710	831371.163407	41.361933
3533.023582	830782.889252	41.366938
3532.900169	830209.915527	41.371943
3532.672403	829637.934346	41.376948
3533.059188	829059.204482	41.381952
3532.868489	828486.382685	41.386957
3532.823815	827902.787807	41.391962
3532.753471	827324.372018	41.396967
3532.751648	826750.485558	41.401972
3532.754547	826173.371789	41.406976
3532.541505	825588.914086	41.411981
3533.124010	825020.346167	41.416986
3533.033531	824435.129006	41.421991
3532.552549	823843.229908	41.426996
3532.598414	823266.487502	41.432000
3532.593273	822694.689507	41.437005
3532.689721	822113.975181	41.442010
3532.754433	821533.557257	41.447015
3532.970886	820949.737109	41.452020
3533.071877	820364.760188	41.457024
3532.340318	819794.448111	41.462029
3532.542719	819209.009152	41.467034
3532.560247	818625.457701	41.472039
3532.466437	818048.576004	41.477044
3532.718109	817465.078122	41.482048
3532.642386	816892.545041	41.487053
3532.400342	816303.940841	41.492058
3532.442791	815720.276637	41.497063
3532.421064	815136.963821	41.502068
3532.517605	814558.082908	41.507072
3532.415593	813978.255684	41.512077
3532.323431	813385.795099	41.517082
3532.483044	812807.584209	41.522087
3532.338068	812217.575272	41.527092
3532.569838	811641.650844	41.532096
3532.501999	811052.603752	41.537101
3532.714654	810459.490160	41.542106
3532.369438	809880.917877	41.547111
3532.572571	809295.687413	41.552116
3532.407930	808700.132368	41.557120
3532.547822	808125.295082	41.562125
3532.646786	807536.206754	41.567130
3532.478834	806947.308848	41.572135
3532.450131	806351.671291	41.577140
3532.656465	805760.940500	41.582144
3532.355591	805176.077787	41.587149
3532.476913	804584.867448	41.592154
3532.436565	804000.986962	41.597159
3532.156924	803414.400961	41.602164
3532.555415	802810.733084	41.607168
3532.211702	802226.311714	41.612173
3532.221796	801642.270564	41.617178
3532.009232	801050.615959	41.622183
3531.951600	800467.075073	41.627188
3532.280749	799878.464439	41.632192
3531.921460	799298.015435	41.637197
3532.062024	798703.842499	41.642202
3532.098083	798119.743725	41.647207
3531.660137	797534.106387	41.652212
3531.604402	796949.335783	41.657216
3531.746641	796376.849586	41.662221
3531.808022	795787.446076	41.667226
3531.902696	795201.275696	41.672231
3531.882114	794625.433586	41.677236
3531.658748	794040.348966	41.682240
3531.845337	793454.998064	41.687245
3531.653233	792867.060431	41.692250
3531.797966	792285.890777	41.697255
3531.406310	791700.835729	41.702260
3531.957332	791119.058105	41.707264
3531.615701	790536.107670	41.712269
3531.835960	789952.767424	41.717274
3531.933524	789359.279827	41.722279
3531.790225	788780.866501	41.727284
3532.080259	788184.102962	41.732288
3531.135850	787607.548398	41.737293
3531.594521	787009.576046	41.742298
3531.414902	786425.325082	41.747303
3531.166164	785840.742960	41.752308
3531.557792	785253.693196	41.757312
3530.723457	784693.989158	41.762317
3530.962947	784113.262066	41.767322
3531.234356	783531.302304	41.772327
3531.044840	782950.603135	41.777332
3530.839991	782374.481896	41.782336
3531.048826	781799.620730	41.787341
3530.881465	781225.613852	41.792346
3531.196901	780646.658434	41.797351
3531.002303	780067.448371	41.802356
3531.199583	779485.222376	41.807360
3530.785268	778901.823847	41.812365
3531.088027	778330.949980	41.817370
3531.157925	777754.854965	41.822375
3530.833384	777181.734069	41.827380
3531.063622	776600.303644	41.832384
3530.885738	776021.308020	41.837389
3530.946351	775439.321482	41.842394
3531.021580	774861.371669	41.847399
3530.623595	774283.358362	41.852404
3530.997551	773698.865595	41.857408
3530.680568	773118.235339	41.862413
3530.700636	772547.940648	41.867418
3530.678683	771968.005931	41.872423
3530.712402	771400.919139	41.877428
3530.666959	770818.287424	41.882432
3530.792785	770236.663978	41.887437
3530.685824	769659.861904	41.892442
3530.304103	769070.646947	41.897447
3530.416249	768507.462231	41.902452
3530.345686	767933.770845	41.907456
3530.515736	767359.106967	41.912461
3530.301411	766788.554399	41.917466
3530.399000	766206.520209	41.922471
3530.564834	765638.574314	41.927476
3530.615693	765056.655292	41.932480
3530.542203	764489.697777	41.937485
3530.437195	763913.878082	41.942490
3530.240476	763334.331973	41.947495
3530.061747	762759.274097	41.952500
3530.156986	762185.062207	41.957504
3530.080090	761618.035599	41.962509
3530.080146	761040.448381	41.967514
3530.310403	760477.327353	41.972519
3530.145510	759898.003706	41.977524
3530.404092	759324.038781	41.982528
3529.640172	758750.747453	41.987533
3529.872956	758176.601120	41.992538
3530.175866	757601.905884	41.997543
3529.922347	757033.824826	42.002548
3529.946669	756459.732109	42.007552
3530.225914	755894.386406	42.012557
3529.979881	755313.985762	42.017562
3529.691357	754739.718017	42.022567
3529.636049	754176.325705	42.027572
3529.625366	753606.516017	42.032576
3529.516789	753043.987331	42.037581
3529.479888	752476.270280	42.042586
3529.588829	751906.511240	42.047591
3529.386066	751350.886026	42.052596
3529.850178	750780.982944	42.057600
3529.287069	750218.621250	42.062605
3529.398869	749655.658799	42.067610
3529.431843	749093.014534	42.072615
3529.078954	748522.046828	42.077620
3528.994461	747960.674046	42.082624
3529.054826	747411.834371	42.087629
3528.922127	746844.312128	42.092634
3529.183663	746286.168438	42.097639
3529.196653	745734.500716	42.102644
3529.315375	745162.365440	42.107648
3529.155139	744604.173309	42.112653
3529.297841	744038.574371	42.117658
3529.165789	743472.042273	42.122663
3528.836902	742914.796457	42.127668
3529.096096	742352.021941	42.132672
3528.824555	741811.299085	42.137677
3529.064151	741247.460023	42.142682
3529.174489	740676.581013	42.147687
3528.773562	740114.946011	42.152692
3528.722161	739552.865202	42.157696
3528.773423	739005.069975	42.162701
3529.030648	738445.281291	42.167706
3528.836485	737885.826944	42.172711
3528.300574	737331.734188	42.177716
3529.013467	736767.742436	42.182720
3528.670291	736219.080214	42.187725
3528.486775	735664.118538	42.192730
3528.635250	735104.509155	42.197735
3528.619463	734559.487137	42.202740
3528.435767	734002.183188	42.207744
3528.779262	733456.975310	42.212749
3528.858148	732893.511305	42.217754
3528.961704	732336.191091	42.222759
3528.631176	731774.599565	42.227764
3529.116144	731212.681142	42.232768
3528.574970	730648.918345	42.237773
3528.696798	730089.112659	42.242778
3528.802114	729530.112845	42.247783
3528.636433	728981.520064	42.252788
3528.812735	728420.005054	42.257792
3528.206758	727856.603667	42.262797
3528.289594	727303.199484	42.267802
3528.152602	726745.832476	42.272807
3528.097545	726206.989986	42.277812
3528.074603	725640.759861	42.282816
3528.044748	725100.056586	42.287821
3527.829459	724549.092902	42.292826
3528.125005	724001.275335	42.297831
3527.943521	723457.665201	42.302836
3527.939895	722905.365739	42.307840
3527.735983	722372.838160	42.312845
3528.115891	721818.269207	42.317850
3528.126870	721273.292475	42.322855
3527.506133	720726.404816	42.327860
3528.020266	720177.552166	42.332864
3527.823987	719637.063831	42.337869
3527.729311	719093.151464	42.342874
3527.856866	718546.934278	42.347879
3527.650451	718007.085359	42.352884
3527.929832	717448.423032	42.357888
3527.631674	716908.518612	42.362893
3527.647355	716362.970882	42.367898
3527.645352	715812.480193	42.372903
3527.274376	715275.260332	42.377908
3527.401851	714728.843000	42.382912
3527.580958	714191.559051	42.387917
3527.346861	713655.055498	42.392922
3527.330881	713115.602795	42.397927
3527.014734	712579.739377	42.402932
3527.337051	712036.190369	42.407936
3526.819762	711505.701952	42.412941
3527.090204	710963.532000	42.417946
3527.426761	710426.874818	42.422951
3527.128734	709893.667198	42.427956
3527.221664	709362.295241	42.432960
3527.680139	708815.637563	42.437965
3527.465163	708280.279364	42.442970
3527.376004	707740.795010	42.447975
3527.363369	707213.626455	42.452980
3527.082587	706657.572879	42.457984
3527.244882	706126.136584	42.462989
3527.155638	705587.112371	42.467994
3527.343868	705050.738410	42.472999
3526.870342	704519.410564	42.478004
3527.099907	703981.919947	42.483008
3526.902316	703449.684321	42.488013
3526.803466	702912.133462	42.493018
3526.943753	702368.894711	42.498023
3526.775189	701846.342034	42.503028
3526.753344	701314.491531	42.508032
3526.804987	700788.757125	42.513037
3526.506547	700245.410606	42.518042
3526.956673	699709.107926	42.523047
3526.437285	699178.255297	42.528052
3526.399498	698653.550288	42.533056
3526.498232	698127.796418	42.538061
3526.427366	697599.554642	42.543066
3526.233478	697076.123743	42.548071
3525.986136	696550.582860	42.553076
3525.828963	696035.982015	42.558080
3526.254092	695517.920600	42.563085
3525.976516	695000.893374	42.568090
3526.375336	694476.560235	42.573095
3526.230202	693971.532810	42.578100
3526.199925	693436.768787	42.583104
3526.298442	692911.349821	42.588109
3526.139382	692389.474873	42.593114
3526.108853	691864.911204	42.598119
3525.809357	691351.007011	42.603124
3525.710174	690832.313314	42.608128
3525.993932	690326.905844	42.613133
3525.928686	689798.346196	42.618138
3526.143556	689286.075946	42.623143
3525.863452	688767.989790	42.628148
3525.909493	688237.677060	42.633152
3525.662912	687737.836581	42.638157
3525.762306	687218.949310	42.643162
3526.311867	686696.222778	42.648167
3525.809379	686184.644566	42.653172
3526.216159	685656.755914	42.658176
3525.456687	685146.855014	42.663181
3525.366582	684633.724856	42.668186
3525.736873	684114.662688	42.673191
3525.255946	683610.999688	42.678196
3525.060154	683093.767987	42.683200
3525.316366	682582.006083	42.688205
3525.493477	682077.548338	42.693210
3525.433029	681569.219264	42.698215
3525.285236	681065.308770	42.703220
3525.403139	680556.992528	42.708224
3525.558604	680046.400520	42.713229
3525.328819	679532.259835	42.718234
3525.477177	679023.604344	42.723239
3525.246819	678516.878189	42.728244
3525.113820	678006.919417	42.733248
3525.253843	677502.714372	42.738253
3525.334578	676998.043529	42.743258
3525.201383	676487.402988	42.748263
3524.947684	675987.915616	42.753268
3524.972943	675483.221448	42.758272
3524.827583	674977.930991	42.763277
3524.649956	674483.581812	42.768282
3525.216592	673981.753462	42.773287
3524.886461	673480.300376	42.778292
3524.935815	672970.182882	42.783296
3524.806924	672476.915133	42.788301
3524.653142	671977.195439	42.793306
3524.839247	671477.440899	42.798311
3524.605750	670990.543224	42.803316
3524.406624	670485.268079	42.808321
3524.542678	669990.029504	42.813325
3524.537189	669502.816420	42.818330
3524.498801	668995.439486	42.823335
3524.590948	668509.803893	42.828340
3524.331038	668007.647506	42.833345
3524.186895	667519.508034	42.838349
3524.079381	667031.486779	42.843354
3524.273446	666549.772940	42.848359
3524.082322	666068.698972	42.853364
3524.521313	665575.422116	42.858369
3524.485626	665090.132109	42.863373
3524.237710	664597.620286	42.868378
3524.561567	664109.325685	42.873383
3524.283421	663616.818364	42.878388
3524.287787	663120.246044	42.883393
3524.328528	662620.248901	42.888397
3524.315289	662138.248151	42.893402
3524.569934	661647.844107	42.898407
3524.478846	661155.228471	42.903412
3524.370919	660657.051003	42.908417
3524.512417	660170.583590	42.913421
3524.140135	659681.683874	42.918426
3524.147820	659180.415914	42.923431
3523.427548	658700.260886	42.928436
3523.599689	658212.841336	42.933441
3523.397047	657737.791758	42.938445
3523.521082	657262.413597	42.943450
3523.748138	656769.320970	42.948455
3523.418467	656311.397956	42.953460
3523.759437	655827.924373	42.958465
3523.775862	655354.968227	42.963469
3523.481323	654875.550735	42.968474
3523.402557	654393.725886	42.973479
3523.362044	653921.659153	42.978484
3523.670879	653436.824679	42.983489
3523.595091	652962.920036	42.988493
3523.230695	652494.486159	42.993498
3523.183433	652012.039891	42.998503
3522.895790	651546.395086	43.003508
3523.074970	651083.645947	43.008513
3523.088834	650611.961134	43.013517
3523.242812	650138.980995	43.018522
3523.300613	649668.442887	43.023527
3523.578398	649202.191843	43.028532
3523.223379	648726.433465	43.033537
3522.911747	648268.683710	43.038541
3522.949505	647793.513364	43.043546
3523.203905	647322.131413	43.048551
3522.685460	646860.754426	43.053556
3522.835611	646385.398124	43.058561
3523.033149	645921.006932	43.063565
3522.881002	645460.752575	43.068570
3522.894161	644998.649489	43.073575
3522.346257	644532.522047	43.078580
3522.584154	644073.387426	43.083585
3522.640763	643616.112599	43.088589
3522.504313	643158.250139	43.093594
3522.849309	642697.135019	43.098599
3522.368921	642247.139558	43.103604
3522.703517	641786.734843	43.108609
3522.422747	641323.464166	43.113613
3522.279014	640870.100090	43.118618
3522.399865	640412.320022	43.123623
3522.187985	639964.728234	43.128628
3522.076732	639515.149200	43.133633
3522.317293	639073.242553	43.138637
3522.194811	638612.872784	43.143642
3522.556065	638150.349012	43.148647
3522.327371	637712.865550	43.153652
3522.086415	637250.454136	43.158657
3522.904147	636808.101437	43.163661
3522.222736	636344.423926	43.168666
3522.390733	635896.339909	43.173671
3522.415330	635450.612456	43.178676
3522.018121	634992.379316	43.183681
3521.707496	634539.364935	43.188685
3521.749832	634095.877879	43.193690
3522.227172	633647.844042	43.198695
3521.850557	633200.937572	43.203700
3521.713449	632755.872744	43.208705
3521.747957	632301.350822	43.213709
3521.784328	631871.482978	43.218714
3521.568481	631425.674249	43.223719
3521.775189	630987.632758	43.228724
3521.760810	630544.705305	43.233729
3522.296351	630107.271715	43.238733
3521.917453	629660.564876	43.243738
3522.090121	629210.641093	43.248743
3522.189725	628771.324102	43.253748
3522.152933	628311.985778	43.258753
3522.228193	627866.377076	43.263757
3521.994787	627419.049859	43.268762
3521.884120	626962.719872	43.273767
3521.879821	626534.293596	43.278772
3521.625833	626088.716486	43.283777
3521.633801	625645.629994	43.288781
3521.668670	625207.578617	43.293786
3521.810963	624760.175547	43.298791
3521.563758	624326.242937	43.303796
3521.390429	623883.414757	43.308801
3521.111391	623443.090750	43.313805
3520.898021	623008.598076	43.318810
3521.286432	622572.632569	43.323815
3521.041367	622127.940836	43.328820
3521.386518	621697.006823	43.333825
3521.546369	621256.368023	43.338829
3521.535941	620831.021108	43.343834
3521.015089	620389.761750	43.348839
3521.231849	619962.989121	43.353844
3520.886536	619526.274252	43.358849
3521.107016	619097.462638	43.363853
3520.832318	618668.568307	43.368858
3520.605991	618243.908397	43.373863
3520.942041	617824.798888	43.378868
3520.949468	617389.742121	43.383873
3520.957764	616958.927969	43.388877
3520.534928	616540.901114	43.393882
3520.919843	616112.846219	43.398887
3520.551911	615691.770215	43.403892
3520.713468	615269.484865	43.408897
3520.653160	614849.727588	43.413901
3520.808177	614433.426655	43.418906
3520.928294	614003.931163	43.423911
3520.586254	613585.828183	43.428916
3520.946983	613159.417200	43.433921
3520.951257	612742.225894	43.438925
3520.777326	612318.982361	43.443930
3520.954709	611887.439421	43.448935
3520.752616	611464.017645	43.453940
3520.957227	611040.610591	43.458945
3520.997437	610619.672729	43.463949
3520.869567	610197.293325	43.468954
3520.765553	609765.264783	43.473959
3520.654030	609349.520649	43.478964
3520.566064	608917.055355	43.483969
3520.861191	608496.495516	43.488973
3520.535934	608084.051264	43.493978
3520.265760	607663.707202	43.498983
3520.429920	607252.202230	43.503988
3520.372607	606838.713447	43.508993
3520.189028	606411.786458	43.513997
3519.973935	606007.424418	43.519002
3519.987607	605596.938276	43.524007
3519.989909	605192.560147	43.529012
3520.057274	604772.351773	43.534017
3520.278168	604360.581286	43.539021
3519.906827	603960.738827	43.544026
3519.790320	603543.727731	43.549031
3519.729965	603140.090080	43.554036
3519.731427	602733.717718	43.559041
3519.550743	602332.179694	43.564045
3519.354234	601935.648882	43.569050
3519.425587	601535.896754	43.574055
3519.363606	601153.368493	43.579060
3519.252607	600748.952421	43.584065
3519.476657	600349.082673	43.589069
3519.076444	599972.395222	43.594074
3519.240768	599567.187852	43.599079
3519.255422	599183.024862	43.604084
3519.282846	598782.130332	43.609089
3519.340119	598390.303301	43.614093
3519.341583	598007.810348	43.619098
3519.419559	597599.335705	43.624103
3519.320292	597220.649559	43.629108
3519.183051	596828.200449	43.634113
3519.209136	596427.375324	43.639117
3518.815268	596044.031603	43.644122
3519.148818	595658.140832	43.649127
3519.017032	595269.203412	43.654132
3518.838614	594885.182249	43.659137
3519.072840	594494.097664	43.664141
3518.978129	594115.711648	43.669146
3519.405875	593725.773669	43.674151
3519.187881	593339.247736	43.679156
3518.682791	592956.977010	43.684161
3518.832902	592569.710012	43.689165
3518.519093	592190.998079	43.694170
3518.725451	591818.262995	43.699175
3518.794934	591435.744379	43.704180
3518.341936	591054.357490	43.709185
3518.474649	590679.388829	43.714189
3518.578642	590306.071009	43.719194
3518.324899	589925.317079	43.724199
3518.633059	589559.577098	43.729204
3518.313664	589187.703133	43.734209
3518.681446	588812.082766	43.739213
3518.341140	588436.571464	43.744218
3518.421455	588050.726394	43.749223
3518.268971	587678.776901	43.754228
3518.328348	587314.518011	43.759233
3518.559715	586939.213835	43.764237
3518.253229	586564.793782	43.769242
3518.067735	586197.075380	43.774247
3518.318914	585836.558168	43.779252
3518.158363	585471.275826	43.784257
3518.474774	585094.994961	43.789261
3517.667849	584734.776225	43.794266
3517.775323	584362.076632	43.799271
3517.773182	584004.362570	43.804276
3517.993114	583637.552469	43.809281
3517.577483	583283.305687	43.814285
3517.839683	582927.676157	43.819290
3517.831154	582558.710980	43.824295
3517.498828	582210.702292	43.829300
3517.428815	581857.712260	43.834305
3517.876229	581497.484895	43.839309
3517.533712	581146.933937	43.844314
3517.644342	580793.982863	43.849319
3517.914162	580438.581116	43.854324
3517.852598	580075.080460	43.859329
3517.616867	579718.738584	43.864333
3517.954111	579365.506580	43.869338
3517.644946	579008.251566	43.874343
3517.762010	578653.729357	43.879348
3517.625545	578300.044816	43.884353
3517.745691	577933.332114	43.889357
3517.518991	577588.493220	43.894362
3517.595579	577225.639220	43.899367
3517.839214	576874.262933	43.904372
3517.613116	576528.187402	43.909377
3517.981934	576161.128299	43.914381
3517.295592	575813.501993	43.919386
3517.302442	575467.357142	43.924391
3517.651539	575114.806556	43.929396
3517.173335	574757.608706	43.934401
3517.371750	574409.339461	43.939405
3517.394601	574057.267436	43.944410
3517.285380	573718.236980	43.949415
3517.647445	573377.104642	43.954420
3517.542403	573021.604538	43.959425
3517.473285	572653.863161	43.964429
3517.418574	572324.797238	43.969434
3517.620620	571969.718063	43.974439
3517.492275	571619.112847	43.979444
3517.145528	571269.440837	43.984449
3517.591260	570923.196270	43.989453
3517.666816	570577.609235	43.994458
3517.425699	570218.329845	43.999463
3517.650450	569870.383388	44.004468
3517.538121	569517.100550	44.009473
3517.685588	569163.612565	44.014477
3517.223582	568815.251241	44.019482
3516.893646	568464.643510	44.024487
3517.060376	568127.428967	44.029492
3517.133774	567787.403070	44.034497
3517.115202	567447.081852	44.039501
3517.076861	567104.339073	44.044506
3517.051859	566764.604784	44.049511
3517.092458	566407.233511	44.054516
3516.902946	566069.522257	44.059521
3517.093066	565726.300988	44.064525
3516.785584	565397.602442	44.069530
3517.159898	565057.201141	44.074535
3516.750712	564713.199448	44.079540
3516.595683	564385.707595	44.084545
3516.682370	564036.669750	44.089549
3516.686130	563706.666793	44.094554
3516.387306	563376.958822	44.099559
3516.563870	563040.867954	44.104564
3516.096006	562707.949654	44.109569
3516.554031	562379.043747	44.114573
3516.311864	562060.621314	44.119578
3516.377350	561723.105559	44.124583
3516.556479	561394.574898	44.129588
3516.204673	561074.183336	44.134593
3516.363509	560740.755328	44.139597
3516.354984	560419.886289	44.144602
3516.064507	560089.640554	44.149607
3516.021738	559768.660713	44.154612
3515.959664	559447.172719	44.159617
3516.372023	559123.682113	44.164621
3516.249197	558811.505914	44.169626
3516.129808	558483.003693	44.174631
3516.377202	558156.344565	44.179636
3515.935755	557838.357333	44.184641
3516.074632	557511.297859	44.189645
3515.961118	557195.153166	44.194650
3515.942388	556879.286973	44.199655
3516.045774	556560.218997	44.204660
3515.790990	556243.269800	44.209665
3515.908314	555928.919342	44.214669
3515.710303	555621.113708	44.219674
3515.989983	555300.474175	44.224679
3515.899058	554980.847390	44.229684
3515.662045	554671.313667	44.234689
3515.964420	554351.604686	44.239693
3516.070276	554045.474167	44.244698
3515.620091	553722.755037	44.249703
3516.061150	553414.638360	44.254708
3515.664405	553095.321102	44.259713
3515.974973	552776.933601	44.264717
3515.685307	552470.985892	44.269722
3515.648438	552156.119748	44.274727
3515.413851	551842.590139	44.279732
3515.239576	551528.589439	44.284737
3515.537029	551229.416857	44.289741
3515.539554	550924.845597	44.294746
3515.600104	550615.419765	44.299751
3515.518139	550312.310599	44.304756
3515.484729	550008.884001	44.309761
3515.592280	549686.779532	44.314765
3515.157984	549390.362428	44.319770
3514.876774	549087.965580	44.324775
3515.019877	548789.824047	44.329780
3515.069261	548486.853430	44.334785
3515.227386	548186.881712	44.339789
3514.810341	547897.687281	44.344794
3514.794187	547594.607295	44.349799
3514.987744	547305.044083	44.354804
3514.790060	547008.534953	44.359809
3514.941025	546714.833175	44.364813
3514.658149	546423.467627	44.369818
3514.734488	546130.018163	44.374823
3514.765459	545844.484817	44.379828
3514.534483	545553.949028	44.384833
3514.648168	545266.373103	44.389837
3514.883563	544978.165443	44.394842
3515.069158	544684.969128	44.399847
3514.957002	544391.968700	44.404852
3515.031465	544107.249174	44.409857
3515.325946	543800.150654	44.414861
3515.261417	543522.299859	44.419866
3514.825759	543215.867724	44.424871
3515.026380	542917.236498	44.429876
3514.984052	542635.179182	44.434881
3514.813118	542340.985884	44.439885
3514.674689	542053.789964	44.444890
3514.641282	541766.065955	44.449895
3514.739222	541472.262325	44.454900
3514.597974	541190.646631	44.459905
3514.952847	540906.166962	44.464909
3514.948584	540615.489480	44.469914
3514.379875	540323.288555	44.474919
3514.570923	540034.582991	44.479924
3514.282254	539754.627994	44.484929
3514.209019	539464.795921	44.489933
3514.253679	539200.710350	44.494938
3514.229546	538912.018577	44.499943
3514.131426	538637.002128	44.504948
3514.094040	538364.794529	44.509953
3514.169159	538084.643500	44.514957
3513.878062	537823.414203	44.519962
3513.816918	537547.311078	44.524967
3514.116441	537267.559606	44.529972
3513.792170	536994.466786	44.534977
3514.346809	536723.841777	44.539981
3514.107318	536461.922922	44.544986
3514.423298	536187.646000	44.549991
3514.008739	535913.690340	44.554996
3513.869352	535638.421250	44.560001
3514.006006	535366.732077	44.565005
3513.904259	535094.927115	44.570010
3513.656488	534816.129246	44.575015
3513.902596	534555.505265	44.580020
3513.683979	534298.588516	44.585025
3513.658080	534023.370011	44.590029
3513.488741	533761.440343	44.595034
3513.587833	533496.634574	44.600039
3513.546147	533233.563511	44.605044
3513.312229	532982.176161	44.610049
3513.511570	532713.605087	44.615053
3513.766661	532456.372861	44.620058
3513.492182	532193.524491	44.625063
3513.526770	531938.490523	44.630068
3513.441031	531680.041210	44.635073
3513.528878	531413.634994	44.640077
3513.230889	531157.634863	44.645082
3513.439479	530907.094855	44.650087
3513.348097	530638.232301	44.655092
3513.280176	530385.812866	44.660097
3513.554251	530129.898902	44.665101
3513.466681	529876.515153	44.670106
3513.175220	529620.436502	44.675111
3513.297374	529363.525708	44.680116
3513.148776	529112.359851	44.685121
3513.186808	528856.363022	44.690125
3512.958562	528610.451244	44.695130
3512.960012	528359.852584	44.700135
3513.026564	528101.515980	44.705140
3512.906477	527863.396780	44.710145
3513.115295	527623.955684	44.715149
3512.923709	527369.587467	44.720154
3512.955652	527128.048512	44.725159
3512.772608	526887.551892	44.730164
3512.692672	526638.300846	44.735169
3512.720614	526393.015123	44.740173
3513.014837	526159.542907	44.745178
3512.914352	525911.999526	44.750183
3512.894755	525665.498349	44.755188
3512.841646	525423.996672	44.760193
3512.180436	525190.924805	44.765197
3512.620667	524953.016613	44.770202
3512.420614	524712.790633	44.775207
3512.594198	524481.281669	44.780212
3512.541876	524242.840431	44.785217
3512.673991	523997.648969	44.790221
3512.455655	523763.873368	44.795226
3512.424098	523537.130805	44.800231
3512.782805	523301.431842	44.805236
3512.365149	523060.661126	44.810241
3512.553326	522829.275646	44.815245
3512.369576	522592.799830	44.820250
3512.220552	522359.949923	44.825255
3512.100847	522128.454766	44.830260
3512.311974	521898.919384	44.835265
3512.199995	521667.163359	44.840269
3512.302119	521442.891253	44.845274
3512.225347	521208.799341	44.850279
3512.429619	520982.129583	44.855284
3512.390295	520765.850342	44.860289
3512.505906	520529.644635	44.865293
3512.286649	520301.522030	44.870298
3512.384927	520067.382622	44.875303
3512.641296	519838.616351	44.880308
3511.962861	519604.854955	44.885313
3512.182345	519369.522557	44.890317
3512.230104	519157.649913	44.895322
3512.760296	518924.681821	44.900327
3512.553928	518694.361238	44.905332
3512.469144	518462.602240	44.910337
3512.269659	518231.010841	44.915341
3512.329457	518003.513345	44.920346
3512.196536	517771.449065	44.925351
3512.393051	517545.739764	44.930356
3511.993975	517324.573761	44.935361
3512.087135	517097.208679	44.940365
3512.040177	516875.824571	44.945370
3511.963652	516642.672881	44.950375
3512.049279	516428.028403	44.955380
3511.786332	516208.237505	44.960385
3512.168049	515991.616872	44.965389
3512.026949	515771.293809	44.970394
3512.100284	515544.212333	44.975399
3511.980499	515326.253563	44.980404
3511.717803	515115.893780	44.985409
3511.635452	514894.840977	44.990413
3511.808001	514670.457764	44.995418
3511.481589	514456.260472	45.000423
3511.698862	514239.643457	45.005428
3511.682599	514028.974286	45.010433
3511.703477	513817.942272	45.015437
3511.596094	513600.159279	45.020442
3511.790118	513388.687718	45.025447
3511.993317	513173.776102	45.030452
3511.925027	512959.867855	45.035457
3511.821614	512738.687032	45.040461
3511.864378	512524.248620	45.045466
3511.452611	512313.825970	45.050471
3511.611364	512092.035469	45.055476
3511.540479	511883.367834	45.060481
3511.219684	511677.013895	45.065485
3511.501195	511472.272411	45.070490
3511.505769	511264.038445	45.075495
3511.636344	511047.341573	45.080500
3511.199798	510845.038962	45.085505
3511.564727	510627.689937	45.090509
3511.380642	510427.056960	45.095514
3511.118116	510226.586430	45.100519
3511.154239	510014.692200	45.105524
3510.881085	509816.593395	45.110529
3511.302981	509610.692065	45.115533
3511.074063	509415.865502	45.120538
3510.915284	509222.995502	45.125543
3511.163217	509022.372057	45.130548
3510.999316	508827.779871	45.135553
3511.328764	508616.777128	45.140557
3511.664978	508419.719255	45.145562
3511.328417	508222.874899	45.150567
3511.285259	508009.148048	45.155572
3511.424870	507810.802175	45.160577
3511.444305	507596.402084	45.165581
3511.524736	507397.808486	45.170586
3511.379848	507195.662341	45.175591
3511.596895	506986.577907	45.180596
3511.396646	506794.747072	45.185601
3511.343711	506579.486481	45.190605
3511.395938	506377.852374	45.195610
3510.754401	506174.565074	45.200615
3510.755251	505967.728332	45.205620
3510.618827	505775.975538	45.210625
3510.639220	505589.551786	45.215629
3510.659279	505404.288556	45.220634
3510.404292	505218.564671	45.225639
3510.605107	505013.147478	45.230644
3510.506822	504832.599041	45.235649
3510.752213	504653.152583	45.240653
3510.705812	504461.672127	45.245658
3510.642323	504272.214416	45.250663
3510.762352	504080.650493	45.255668
3510.627905	503893.424798	45.260673
3510.645365	503700.003424	45.265677
3510.312893	503515.941539	45.270682
3510.315781	503337.078044	45.275687
3510.652434	503139.348878	45.280692
3510.494884	502967.839302	45.285697
3510.533599	502770.004860	45.290701
3510.420104	502590.596924	45.295706
3510.534536	502408.822433	45.300711
3510.525038	502233.032990	45.305716
3510.692522	502053.267832	45.310721
3510.775812	501862.442511	45.315725
3510.632157	501679.035514	45.320730
3510.423324	501492.047778	45.325735
3510.704027	501304.215905	45.330740
3510.349051	501129.080349	45.335745
3510.467260	500942.890074	45.340749
3510.299642	500759.173522	45.345754
3510.144263	500579.801302	45.350759
3509.960883	500404.274787	45.355764
3510.341545	500226.829768	45.360769
3510.427929	500047.663304	45.365773
3510.609782	499869.995571	45.370778
3510.330815	499700.343523	45.375783
3510.856829	499511.589716	45.380788
3510.860186	499335.615429	45.385793
3510.374045	499146.372900	45.390797
3510.585596	498956.402262	45.395802
3510.397737	498778.836517	45.400807
3510.517077	498596.816859	45.405812
3510.622853	498425.214990	45.410817
3510.708849	498232.577292	45.415821
3510.501121	498056.018634	45.420826
3510.370709	497868.571948	45.425831
3510.249926	497686.482191	45.430836
3509.997829	497514.375745	45.435841
3510.307397	497344.599151	45.440845
3510.008260	497162.028390	45.445850
3510.059719	496983.795762	45.450855
3509.849056	496813.647432	45.455860
3510.083054	496645.899654	45.460865
3509.745659	496463.428955	45.465869
3509.681099	496303.719759	45.470874
3509.431319	496141.511812	45.475879
3509.523185	495973.983893	45.480884
3509.415384	495809.826552	45.485889
3509.366586	495649.450929	45.490893
3509.617406	495482.042705	45.495898
3509.304693	495330.509866	45.500903
3509.570920	495172.453152	45.505908
3509.679172	495010.830713	45.510913
3510.043669	494845.774049	45.515917
3509.669646	494678.262212	45.520922
3509.585049	494517.527867	45.525927
3509.846917	494345.149447	45.530932
3509.615418	494194.806528	45.535937
3509.810866	494036.751281	45.540941
3509.698429	493863.926040	45.545946
3509.328153	493709.049950	45.550951
3509.372432	493539.735556	45.555956
3509.408185	493386.608254	45.560961
3509.424930	493224.680883	45.565965
3509.350463	493065.600379	45.570970
3509.203157	492919.126931	45.575975
3509.309505	492760.063285	45.580980
3509.205511	492613.680989	45.585985
3508.928935	492455.135168	45.590989
3509.343026	492300.264092	45.595994
3509.295444	492149.163440	45.600999
3509.405884	491993.380237	45.606004
3509.608398	491840.311753	45.611009
3509.062254	491686.104967	45.616013
3509.030872	491540.864661	45.621018
3508.866150	491397.568358	45.626023
3509.029336	491245.563690	45.631028
3509.220655	491090.820895	45.636033
3509.043720	490951.317362	45.641037
3509.304139	490794.536397	45.646042
3509.227921	490641.707179	45.651047
3509.365236	490492.938253	45.656052
3509.276116	490350.176837	45.661057
3509.355637	490199.391469	45.666061
3509.181307	490048.749316	45.671066
3509.209672	489901.258764	45.676071
3509.251410	489742.987698	45.681076
3509.071030	489594.973614	45.686081
3508.842139	489444.284904	45.691085
3508.892620	489300.883806	45.696090
3508.850051	489167.363984	45.701095
3508.731013	489011.086984	45.706100
3508.690036	488874.174545	45.711105
3508.583398	488726.899424	45.716109
3509.032857	488586.763834	45.721114
3508.860466	488452.147480	45.726119
3508.960847	488306.047840	45.731124
3508.856154	488167.268492	45.736129
3508.900255	488022.744703	45.741133
3508.919355	487883.081732	45.746138
3509.008314	487742.191265	45.751143
3509.431409	487587.073939	45.756148
3509.134870	487456.822889	45.761153
3509.249418	487302.008725	45.766157
3509.185631	487151.271932	45.771162
3509.075986	487015.419271	45.776167
3509.318340	486860.832396	45.781172
3509.135008	486720.891062	45.786177
3508.816853	486572.065089	45.791181
3508.770060	486427.948460	45.796186
3508.828439	486289.581793	45.801191
3509.056927	486145.213413	45.806196
3509.104641	486005.024485	45.811201
3509.016852	485856.001280	45.816205
3509.093601	485711.705853	45.821210
3508.562487	485576.268255	45.826215
3508.761436	485438.731224	45.831220
3508.750471	485303.101493	45.836225
3508.733517	485154.313293	45.841229
3509.182865	485012.377769	45.846234
3508.875862	484875.428828	45.851239
3508.752203	484727.465011	45.856244
3508.952955	484588.503943	45.861249
3508.689502	484458.478046	45.866253
3508.759087	484322.422134	45.871258
3508.317724	484194.854041	45.876263
3508.484733	484047.189185	45.881268
3508.808440	483921.361158	45.886273
3508.797028	483775.293503	45.891277
3508.368642	483649.642576	45.896282
3508.542292	483514.473740	45.901287
3508.770464	483377.776131	45.906292
3508.514865	483252.852110	45.911297
3508.376085	483122.896357	45.916301
3508.533240	482987.220176	45.921306
3508.342488	482857.220741	45.926311
3508.578822	482710.444025	45.931316
3508.400278	482594.967496	45.936321
3508.554070	482466.019946	45.941325
3508.540618	482325.660468	45.946330
3508.317333	482191.662951	45.951335
3508.674505	482063.841983	45.956340
3508.524544	481941.674738	45.961345
3508.584514	481809.397641	45.966349
3508.472930	481672.238783	45.971354
3508.410159	481548.737864	45.976359
3508.599691	481420.890309	45.981364
3508.663839	481286.533216	45.986369
3508.478476	481148.370536	45.991373
3508.378165	481015.709983	45.996378
3508.358639	480892.399646	46.001383
3508.539035	480766.624476	46.006388
3508.448159	480640.591012	46.011393
3508.189772	480507.801833	46.016397
3508.134426	480376.647566	46.021402
3507.821091	480260.419660	46.026407
3507.785588	480136.145026	46.031412
3508.146443	480022.027910	46.036417
3508.114723	479902.155306	46.041421
3508.207254	479774.160741	46.046426
3508.238410	479662.983258	46.051431
3508.120382	479521.860351	46.056436
3507.850818	479403.391934	46.061441
3507.759313	479290.410578	46.066445
3507.942496	479170.547055	46.071450
3507.706167	479052.070663	46.076455
3507.983703	478936.037109	46.081460
3507.861576	478818.450977	46.086465
3507.609896	478695.772806	46.091469
3507.819244	478586.937796	46.096474
3507.870354	478476.914073	46.101479
3507.853191	478358.851388	46.106484
3507.875141	478243.970883	46.111489
3507.756669	478130.328732	46.116493
3507.913299	478010.158309	46.121498
3507.787635	477897.933565	46.126503
3507.766376	477775.614881	46.131508
3507.738814	477671.675356	46.136513
3507.772339	477552.333023	46.141517
3507.883062	477434.698191	46.146522
3507.619830	477321.025080	46.151527
3507.693394	477213.268312	46.156532
3507.637021	477108.520391	46.161537
3507.336215	476993.585856	46.166541
3507.851670	476883.220071	46.171546
3507.378118	476778.946556	46.176551
3507.538338	476666.412267	46.181556
3507.569515	476561.089297	46.186561
3507.540915	476444.990900	46.191565
3507.676288	476339.699503	46.196570
3507.533952	476241.948829	46.201575
3507.227748	476128.984538	46.206580
3507.367892	476014.829366	46.211585
3507.122965	475918.866719	46.216589
3507.485099	475814.900753	46.221594
3507.089401	475718.861534	46.226599
3507.393225	475617.588115	46.231604
3507.297585	475516.432982	46.236609
3507.037484	475410.444242	46.241613
3507.171784	475304.488825	46.246618
3507.017787	475217.216573	46.251623
3507.404130	475111.875300	46.256628
3507.253061	475011.992805	46.261633
3506.910753	474915.484541	46.266637
3507.525719	474814.204226	46.271642
3507.237481	474720.116355	46.276647
3507.236066	474614.483985	46.281652
3507.211604	474510.424764	46.286657
3507.300386	474409.687833	46.291661
3507.359830	474314.171265	46.296666
3507.078408	474218.256644	46.301671
3507.320730	474107.515758	46.306676
3507.170395	474007.830279	46.311681
3506.869433	473916.677654	46.316685
3507.290510	473817.551919	46.321690
3507.204609	473715.372450	46.326695
3507.193040	473624.472827	46.331700
3506.976297	473520.137032	46.336705
3506.820570	473420.449320	46.341709
3507.135365	473331.974013	46.346714
3507.056452	473245.034148	46.351719
3507.137710	473146.216073	46.356724
3507.232423	473045.318802	46.361729
3507.057459	472956.469547	46.366733
3507.102307	472859.529979	46.371738
3506.895796	472761.923808	46.376743
3507.198250	472671.877512	46.381748
3507.063887	472572.839995	46.386753
3507.126312	472483.593443	46.391757
3506.984896	472391.646438	46.396762
3506.977653	472299.422845	46.401767
3506.974707	472203.956749	46.406772
3506.997596	472114.461959	46.411777
3506.594845	472029.445621	46.416781
3506.675542	471934.419683	46.421786
3506.740274	471849.525293	46.426791
3506.999736	471756.291204	46.431796
3507.159008	471666.112578	46.436801
3506.654789	471570.070432	46.441805
3506.857177	471478.313477	46.446810
3506.900468	471403.347638	46.451815
3506.880108	471305.499499	46.456820
3506.841664	471216.416081	46.461825
3506.491233	471136.147691	46.466829
3506.809661	471045.432428	46.471834
3506.586108	470955.670300	46.476839
3506.816651	470860.157502	46.481844
3506.714946	470786.176296	46.486849
3506.948923	470705.401089	46.491853
3506.841244	470609.742174	46.496858
3506.474014	470526.485712	46.501863
3506.410088	470449.204477	46.506868
3506.751130	470364.762711	46.511873
3506.494771	470280.574524	46.516877
3506.477135	470193.964605	46.521882
3506.471950	470113.987468	46.526887
3506.548823	470039.466330	46.531892
3506.663645	469949.945548	46.536897
3506.360634	469871.385831	46.541901
3506.497740	469790.927166	46.546906
3506.617506	469716.144172	46.551911
3506.396110	469634.884969	46.556916
3506.440939	469544.513129	46.561921
3506.282984	469477.627779	46.566925
3506.504971	469402.268911	46.571930
3506.292864	469322.627681	46.576935
3506.090116	469236.652830	46.581940
3506.435788	469174.289889	46.586945
3506.234811	469100.015114	46.591949
3506.703183	469009.315138	46.596954
3506.609775	468929.955918	46.601959
3506.601044	468853.063982	46.606964
3506.436595	468769.866478	46.611969
3506.320315	468694.106667	46.616973
3506.641723	468613.256958	46.621978
3506.574798	468532.675835	46.626983
3506.791803	468454.730638	46.631988
3506.614983	468362.162176	46.636993
3506.412187	468297.509187	46.641997
3506.742725	468206.423676	46.647002
3506.354570	468131.011985	46.652007
3506.138130	468063.169173	46.657012
3506.267587	467982.856134	46.662017
3506.498710	467910.326586	46.667021
3506.735672	467827.968259	46.672026
3506.286149	467760.214826	46.677031
3506.467254	467674.876587	46.682036
3506.349665	467592.273837	46.687041
3506.081362	467526.514948	46.692045
3506.349684	467439.793001	46.697050
3506.390665	467378.134773	46.702055
3505.912362	467300.050296	46.707060
3506.174893	467227.006209	46.712065
3506.186446	467157.956103	46.717069
3506.172007	467081.868554	46.722074
3506.096727	467013.947259	46.727079
3506.072500	466950.728349	46.732084
3506.376211	466871.191448	46.737089
3506.143471	466811.047268	46.742093
3506.366395	466738.514686	46.747098
3506.156862	466667.727461	46.752103
3505.983041	466588.270927	46.757108
3506.492315	466522.223844	46.762113
3506.452623	466454.649120	46.767117
3506.455015	466368.423690	46.772122
3506.123333	466297.351991	46.777127
3506.452291	466225.002014	46.782132
3506.117478	466149.522753	46.787137
3505.931116	466086.126038	46.792141
3506.074344	466015.022869	46.797146
3506.199014	465951.116644	46.802151
3506.394660	465876.761634	46.807156
3506.428609	465800.914069	46.812161
3506.114278	465739.513906	46.817165
3506.571125	465661.364422	46.822170
3506.412582	465588.183363	46.827175
3506.171015	465521.146469	46.832180
3506.508801	465456.340941	46.837185
3506.224147	465378.418249	46.842189
3506.141816	465307.452318	46.847194
3506.244036	465241.926336	46.852199
3506.291973	465163.844663	46.857204
3506.076561	465091.178076	46.862209
3505.991965	465025.277943	46.867213
3505.991703	464949.939528	46.872218
3505.913711	464888.090988	46.877223
3505.719785	464827.984661	46.882228
3505.607787	464754.893833	46.887233
3505.733340	464704.358987	46.892237
3505.914219	464639.628186	46.897242
3505.694589	464578.258833	46.902247
3505.922111	464513.468982	46.907252
3505.643510	464454.490607	46.912257
3505.634843	464394.503304	46.917261
3506.029836	464335.206889	46.922266
3505.548976	464280.619835	46.927271
3505.916801	464210.181025	46.932276
3505.867223	464152.682632	46.937281
3505.615201	464096.586647	46.942285
3505.846954	464032.250475	46.947290
3505.566195	463970.332300	46.952295
3505.681506	463923.546561	46.957300
3506.028694	463861.166147	46.962305
3505.696575	463793.378727	46.967309
3506.011761	463737.640870	46.972314
3505.934946	463683.489831	46.977319
3505.759430	463616.739088	46.982324
3506.407428	463535.660323	46.987329
3506.241788	463485.982732	46.992333
3506.370293	463415.936598	46.997338
3506.386790	463352.800323	47.002343
3505.721611	463283.598599	47.007348
3506.142329	463211.475071	47.012353
3505.784297	463154.837114	47.017357
3506.304346	463078.338556	47.022362
3506.183318	463023.179841	47.027367
3506.268796	462954.254137	47.032372
3506.197920	462880.642557	47.037377
3506.127345	462830.440365	47.042381
3506.389763	462765.081378	47.047386
3506.191966	462700.054107	47.052391
3506.070269	462629.237147	47.057396
3506.445398	462555.902890	47.062401
3505.981715	462503.081415	47.067405
3506.068200	462421.840562	47.072410
3505.844078	462370.548639	47.077415
3505.563789	462298.440104	47.082420
3505.755738	462245.049941	47.087425
3505.587681	462198.055102	47.092429
3506.219679	462123.560588	47.097434
3505.754525	462066.431052	47.102439
3505.661835	462001.028811	47.107444
3505.661888	461944.174195	47.112449
3505.346535	461901.004244	47.117453
3505.897517	461836.150296	47.122458
3506.101754	461771.659379	47.127463
3505.973542	461716.599564	47.132468
3506.196415	461652.966521	47.137473
3505.918031	461598.894813	47.142477
3505.822673	461532.630021	47.147482
3505.737051	461474.825879	47.152487
3505.463965	461420.246037	47.157492
3505.914931	461357.535901	47.162497
3505.172911	461305.062774	47.167501
3505.524303	461245.460415	47.172506
3505.569238	461202.328763	47.177511
3505.197533	461149.741318	47.182516
3505.488175	461089.996839	47.187521
3505.338156	461057.843920	47.192525
3505.472394	461001.014348	47.197530
3505.540278	460949.263462	47.202535
3505.483682	460889.324290	47.207540
3505.897726	460841.365343	47.212545
3505.628409	460790.229047	47.217549
3505.721731	460723.473243	47.222554
3505.680213	460662.263915	47.227559
3505.672793	460613.464213	47.232564
3505.707347	460555.332805	47.237569
3505.393161	460511.703527	47.242573
3505.459172	460449.715037	47.247578
3505.322907	460402.609139	47.252583
3505.601462	460347.121316	47.257588
3505.981897	460288.626007	47.262593
3505.448446	460245.084258	47.267597
3505.321534	460192.959241	47.272602
3505.335611	460143.952004	47.277607
3505.466925	460097.762562	47.282612
3505.578853	460047.927542	47.287617
3505.323476	459997.901726	47.292621
3505.524324	459947.696529	47.297626
3505.462052	459891.454785	47.302631
3505.313384	459845.160527	47.307636
3505.582402	459791.699903	47.312641
3505.475369	459757.510408	47.317645
3505.200763	459696.084507	47.322650
3505.325856	459659.321288	47.327655
3504.983179	459598.058743	47.332660
3505.368182	459562.061824	47.337665
3505.337985	459520.966493	47.342669
3505.385628	459461.309282	47.347674
3504.978215	459417.389443	47.352679
3505.131531	459382.648058	47.357684
3505.485365	459329.475787	47.362689
3505.230850	459286.644498	47.367693
3505.364123	459230.620895	47.372698
3505.170224	459188.133801	47.377703
3504.762935	459139.449435	47.382708
3505.391190	459102.649956	47.387713
3504.835197	459060.579176	47.392717
3505.176984	459006.698582	47.397722
3505.248671	458975.011235	47.402727
3505.284139	458933.802121	47.407732
3505.491199	458879.741468	47.412737
3504.989244	458845.364437	47.417741
3504.828788	458796.991853	47.422746
3505.249954	458745.428313	47.427751
3504.923483	458709.956788	47.432756
3505.302243	458667.725572	47.437761
3504.826367	458636.333907	47.442765
3504.942410	458596.934860	47.447770
3504.783469	458547.902559	47.452775
3504.734083	458523.786684	47.457780
3505.196225	458479.766987	47.462785
3504.645633	458439.974642	47.467789
3504.765449	458406.301594	47.472794
3504.644962	458364.712483	47.477799
3504.716069	458332.922855	47.482804
3504.955136	458300.648359	47.487809
3505.063971	458268.902869	47.492813
3504.914341	458216.877929	47.497818
3504.810347	458196.065323	47.502823
3504.631919	458147.136732	47.507828
3504.763422	458109.812063	47.512833
3504.454321	458083.003152	47.517837
3504.848752	458050.042854	47.522842
3504.614878	458009.283287	47.527847
3504.818401	457975.291126	47.532852
3505.267917	457946.477239	47.537857
3504.971416	457912.671716	47.542861
3505.273649	457875.570875	47.547866
3505.258522	457835.179068	47.552871
3504.938247	457805.685488	47.557876
3505.169768	457756.077748	47.562881
3504.991119	457721.542214	47.567885
3504.937554	457674.010285	47.572890
3504.965583	457633.610704	47.577895
3504.841206	457599.876632	47.582900
3504.827219	457560.700488	47.587905
3504.504663	457519.955069	47.592909
3504.914810	457484.102178	47.597914
3504.749710	457455.189795	47.602919
3504.562509	457421.516835	47.607924
3504.679066	457385.916635	47.612929
3504.537656	457375.702572	47.617933
3504.596796	457337.527192	47.622938
3504.833905	457288.931034	47.627943
3504.796345	457266.839009	47.632948
3504.982472	457233.051304	47.637953
3504.576564	457207.778292	47.642957
3504.896704	457167.733377	47.647962
3505.026294	457141.152411	47.652967
3504.934592	457099.099600	47.657972
3504.952730	457058.649870	47.662977
3504.772981	457031.665413	47.667981
3505.047948	456987.167560	47.672986
3504.925732	456972.388342	47.677991
3504.716599	456927.162050	47.682996
3504.982830	456890.014857	47.688001
3504.967304	456866.246009	47.693005
3504.936689	456813.690261	47.698010
3505.013517	456786.306866	47.703015
3504.773628	456754.010301	47.708020
3504.947694	456706.133106	47.713025
3504.985494	456686.561876	47.718029
3504.923959	456639.991903	47.723034
3504.959089	456610.081083	47.728039
3505.000964	456579.104655	47.733044
3504.837692	456527.483166	47.738049
3504.703687	456504.088927	47.743053
3504.878261	456473.748604	47.748058
3504.866808	456432.694433	47.753063
3504.308711	456411.146532	47.758068
3504.687852	456381.734188	47.763073
3504.969801	456351.172601	47.768077
3504.886352	456315.249856	47.773082
3504.909041	456290.460067	47.778087
3504.823060	456249.874435	47.783092
3504.765641	456210.145527	47.788097
3504.574757	456195.782962	47.793101
3504.714627	456161.798616	47.798106
3504.774988	456115.561433	47.803111
3504.564111	456090.304406	47.808116
3504.793621	456073.487661	47.813121
3504.644226	456034.838552	47.818125
3504.733218	456001.775002	47.823130
3504.890872	455979.090672	47.828135
3504.775830	455947.886633	47.833140
3505.150099	455904.281826	47.838145
3504.690579	455882.767216	47.843149
3504.800199	455840.677413	47.848154
3504.794944	455804.943164	47.853159
3504.739523	455789.644794	47.858164
3504.613263	455748.304710	47.863169
3504.759488	455708.286605	47.868173
3504.846883	455688.756631	47.873178
3504.686339	455665.365954	47.878183
3504.546449	455624.737586	47.883188
3504.757687	455594.744509	47.888193
3504.558371	455574.198916	47.893197
3504.512034	455548.406231	47.898202
3504.667400	455509.247883	47.903207
3504.511177	455481.598385	47.908212
3504.718401	455467.167328	47.913217
3504.441974	455442.833089	47.918221
3504.544187	455408.042886	47.923226
3504.500410	455381.641281	47.928231
3504.822016	455366.176837	47.933236
3504.850752	455334.186965	47.938241
3504.732768	455303.844158	47.943245
3504.455427	455273.376446	47.948250
3504.731164	455253.205621	47.953255
3504.306189	455224.790628	47.958260
3504.397913	455193.144607	47.963265
3504.593600	455162.849410	47.968269
3504.476236	455137.777989	47.973274
3504.770282	455127.133607	47.978279
3504.536886	455091.538439	47.983284
3504.687574	455048.679635	47.988289
3504.590499	455035.364722	47.993293
3504.781873	455017.489124	47.998298
3504.726375	454969.292200	48.003303
3504.361477	454952.170500	48.008308
3504.446669	454931.727750	48.013313
3504.612818	454909.902514	48.018317
3504.521568	454871.089191	48.023322
3504.633043	454839.591321	48.028327
3504.654381	454819.463505	48.033332
3504.793807	454788.112854	48.038337
3504.639583	454762.337594	48.043341
3504.364966	454731.665843	48.048346
3504.531606	454711.056892	48.053351
3504.508534	454702.646147	48.058356
3504.559965	454666.342620	48.063361
3504.388871	454641.938746	48.068365
3504.676108	454606.304525	48.073370
3504.829444	454593.757626	48.078375
3504.812150	454578.553217	48.083380
3505.070880	454538.057382	48.088385
3504.909216	454519.633333	48.093389
3504.162719	454482.147746	48.098394
3504.606877	454449.021031	48.103399
3504.654908	454418.851326	48.108404
3505.020265	454403.784217	48.113409
3504.765475	454377.721493	48.118413
3504.970237	454338.907307	48.123418
3505.271833	454309.302447	48.128423
3504.853452	454273.838821	48.133428
3504.738219	454241.618358	48.138433
3504.750613	454220.984559	48.143437
3505.088729	454184.428457	48.148442
3505.066064	454155.132202	48.153447
3504.730043	454119.755630	48.158452
3504.483717	454074.985569	48.163457
3504.269157	454069.040499	48.168461
3504.277001	454045.821981	48.173466
3504.478543	454029.211098	48.178471
3504.457321	454000.015760	48.183476
3504.758517	453964.479424	48.188481
3504.798755	453945.462762	48.193485
3504.495681	453926.200544	48.198490
3504.694535	453890.123932	48.203495
3504.810906	453865.264503	48.208500
3505.080431	453836.526219	48.213505
3504.687816	453815.961165	48.218509
3504.868670	453781.661696	48.223514
3504.835840	453766.459337	48.228519
3504.486282	453730.019844	48.233524
3504.693466	453691.457485	48.238529
3504.737288	453675.836422	48.243533
3504.335881	453657.807386	48.248538
3504.447751	453627.017292	48.253543
3504.330298	453603.718280	48.258548
3504.537417	453571.137559	48.263553
3504.347341	453558.496583	48.268557
3504.242061	453546.500139	48.273562
3504.408597	453526.701117	48.278567
3504.246178	453503.865914	48.283572
3504.326612	453463.499788	48.288577
3504.491326	453446.134312	48.293581
3504.292217	453421.683072	48.298586
3504.555122	453411.144507	48.303591
3504.303835	453391.872944	48.308596
3504.232635	453375.967128	48.313601
3504.254134	453347.422592	48.318605
3504.266915	453313.455205	48.323610
3504.604611	453290.280899	48.328615
3504.279321	453291.603815	48.333620
3504.099461	453268.061606	48.338625
3504.053367	453256.612526	48.343629
3503.927744	453249.942309	48.348634
3504.227265	453235.899477	48.353639
3504.257357	453230.622114	48.358644
3504.348571	453204.650900	48.363649
3504.390502	453176.204027	48.368653
3504.273463	453146.719667	48.373658
3504.354721	453129.621648	48.378663
3504.003359	453114.878754	48.383668
3504.180153	453098.169955	48.388673
3504.110448	453100.919395	48.393677
3504.166979	453086.309612	48.398682
3504.371729	453065.489722	48.403687
3504.242517	453053.142212	48.408692
3504.327301	453012.723763	48.413697
3504.102372	452993.396631	48.418701
3504.176872	452980.000389	48.423706
3504.348874	452971.859796	48.428711
3504.280226	452953.722627	48.433716
3504.170263	452932.804253	48.438721
3504.015999	452921.474848	48.443725
3503.844488	452916.992258	48.448730
3504.440861	452900.363743	48.453735
3504.212437	452895.485302	48.458740
3504.005269	452857.093520	48.463745
3504.150795	452830.554910	48.468749
3504.026322	452807.104107	48.473754
3504.336704	452795.239034	48.478759
3504.073174	452784.384471	48.483764
3504.281137	452768.177040	48.488769
3504.054039	452757.366938	48.493773
3504.118027	452748.129393	48.498778
3503.995883	452742.725811	48.503783
3503.882507	452736.458902	48.508788
3504.313460	452720.720317	48.513793
3504.103080	452706.155840	48.518797
3504.107539	452692.315108	48.523802
3504.318998	452683.559313	48.528807
3504.010704	452678.745154	48.533812
3504.309881	452648.225790	48.538817
3504.308856	452620.140356	48.543821
3504.369469	452608.824784	48.548826
3504.060932	452587.382309	48.553831
3503.864466	452574.944602	48.558836
3504.028494	452552.407476	48.563841
3504.028873	452541.152849	48.568845
3504.126109	452531.554656	48.573850
3504.412322	452523.292993	48.578855
3503.748251	452512.608070	48.583860
3504.007748	452493.501932	48.588865
3503.899629	452497.576117	48.593869
3504.055985	452482.087024	48.598874
3503.960742	452458.478743	48.603879
3503.838844	452463.163647	48.608884
3504.265046	452448.084720	48.613889
3504.463760	452441.967219	48.618893
3504.261546	452417.971585	48.623898
3504.919831	452379.126959	48.628903
3504.576850	452354.952501	48.633908
3504.485293	452337.528456	48.638913
3504.442618	452335.609276	48.643917
3504.244684	452305.782649	48.648922
3504.108584	452277.719812	48.653927
3504.064261	452264.242002	48.658932
3504.307773	452245.493242	48.663937
3504.118546	452242.027470	48.668941
3504.114568	452235.741729	48.673946
3504.154632	452218.295109	48.678951
3503.952645	452214.223145	48.683956
3503.929030	452195.519952	48.688961
3504.156256	452190.005874	48.693965
3503.989557	452179.540035	48.698970
3504.257041	452169.253541	48.703975
3504.193763	452155.728199	48.708980
3504.184100	452141.382537	48.713985
3504.268497	452130.316129	48.718989
3504.016023	452103.692452	48.723994
3504.189562	452077.857856	48.728999
3503.892402	452064.676573	48.734004
3503.762936	452047.157361	48.739009
3504.045611	452029.871947	48.744013
3504.034355	452021.863667	48.749018
3504.223895	452008.396455	48.754023
3503.902554	452007.335989	48.759028
3503.987461	451987.650823	48.764033
3503.823429	451975.105821	48.769037
3504.167385	451973.171289	48.774042
3504.218170	451962.364020	48.779047
3503.875034	451955.426336	48.784052
3504.144773	451948.586793	48.789057
3504.149602	451937.128286	48.794061
3504.345052	451926.803275	48.799066
3504.423716	451916.903781	48.804071
3504.013599	451914.692418	48.809076
3504.231819	451901.575124	48.814081
3504.281323	451888.131746	48.819085
3504.122473	451862.505729	48.824090
3504.097597	451834.271206	48.829095
3504.063921	451819.371743	48.834100
3504.290521	451803.363167	48.839105
3503.945606	451806.311864	48.844109
3503.869183	451786.552658	48.849114
3504.187875	451775.496754	48.854119
3504.341147	451781.351582	48.859124
3504.177625	451760.187674	48.864129
3504.275564	451749.524337	48.869133
3504.346169	451744.645262	48.874138
3504.646939	451726.748128	48.879143
3504.476696	451699.095923	48.884148
3504.340894	451677.775103	48.889153
3504.319691	451673.722862	48.894157
3504.222602	451654.220550	48.899162
3504.523600	451640.227084	48.904167
3504.061348	451625.806248	48.909172
3503.665868	451595.860231	48.914177
3504.305031	451606.904799	48.919181
3504.038159	451588.039798	48.924186
3504.067291	451550.872706	48.929191
3504.066152	451550.416624	48.934196
3503.958867	451531.980612	48.939201
3503.875852	451525.150464	48.944205
3503.996618	451513.570529	48.949210
3504.197253	451501.926252	48.954215
3504.159099	451504.924010	48.959220
3504.256441	451487.973984	48.964225
3504.271882	451481.684698	48.969229
3504.110083	451473.600513	48.974234
3503.891190	451462.129245	48.979239
3503.864017	451447.836791	48.984244
3504.155284	451437.799370	48.989249
3504.321266	451428.645219	48.994253
3503.754504	451428.742005	48.999258
3504.112069	451411.088396	49.004263
3503.827004	451417.829358	49.009268
3503.964449	451403.204571	49.014273
3504.159545	451390.800691	49.019277
3503.784318	451382.144523	49.024282
3504.001153	451367.201960	49.029287
3504.056092	451361.869178	49.034292
3504.023506	451347.932474	49.039297
3503.983761	451341.246975	49.044301
3504.159115	451336.197821	49.049306
3504.274937	451324.263731	49.054311
3503.811561	451308.930278	49.059316
3503.696908	451296.427133	49.064321
3504.275467	451292.728704	49.069325
3503.915148	451274.234268	49.074330
3504.111244	451263.908817	49.079335
3504.030904	451244.200463	49.084340
3504.166606	451232.871319	49.089345
3504.467349	451223.187073	49.094349
3503.935989	451214.101198	49.099354
3504.381780	451185.684028	49.104359
3504.458243	451190.233949	49.109364
3504.322153	451176.213404	49.114369
3504.332724	451168.150367	49.119373
3504.380357	451153.946338	49.124378
3504.369679	451127.736417	49.129383
3503.770741	451126.571202	49.134388
3503.527545	451106.484926	49.139393
3503.972501	451097.637895	49.144397
3504.072921	451097.924959	49.149402
3504.119811	451076.673727	49.154407
3503.808952	451080.326508	49.159412
3503.788043	451061.773930	49.164417
3504.160516	451046.703163	49.169421
3504.103195	451043.113266	49.174426
3504.154807	451035.955769	49.179431
3504.315916	451028.627474	49.184436
3504.299187	451019.757842	49.189441
3504.179319	451020.386721	49.194445
3503.893759	451017.089291	49.199450
3504.073748	450998.806553	49.204455
3504.141432	450993.775701	49.209460
3503.963130	450980.624133	49.214465
3504.185915	450982.816910	49.219469
3503.718197	450969.816152	49.224474
3503.933157	450957.712823	49.229479
3504.056545	450955.562360	49.234484
3503.741373	450943.194641	49.239489
3504.192561	450936.019584	49.244493
3503.646928	450939.408276	49.249498
3504.197847	450920.707233	49.254503
3504.140405	450924.164670	49.259508
3503.922596	450905.493472	49.264513
3503.793951	450902.422732	49.269517
3503.907445	450894.342015	49.274522
3504.453261	450877.162815	49.279527
3504.219882	450880.447499	49.284532
3504.113747	450851.769211	49.289537
3503.980280	450822.335044	49.294541
3503.848093	450807.958680	49.299546
3504.031616	450799.358964	49.304551
3503.669322	450793.336770	49.309556
3503.876285	450805.773780	49.314561
3504.138071	450814.905888	49.319565
3503.885493	450795.632121	49.324570
3504.447706	450784.990417	49.329575
3503.837301	450767.856447	49.334580
3504.292328	450747.346400	49.339585
3504.129737	450735.560912	49.344589
3503.896875	450735.448583	49.349594
3503.999164	450727.673919	49.354599
3504.057982	450720.058778	49.359604
3504.008105	450696.035138	49.364609
3503.912948	450700.411667	49.369613
3503.938993	450700.610035	49.374618
3504.414200	450683.848338	49.379623
3503.985201	450683.769499	49.384628
3504.010593	450675.805142	49.389633
3504.116456	450666.863726	49.394637
3503.948069	450665.168660	49.399642
3504.259541	450647.725080	49.404647
3503.915341	450647.631761	49.409652
3503.989511	450637.022613	49.414657
3503.984519	450624.753844	49.419661
3503.984139	450622.168171	49.424666
3503.966946	450616.289803	49.429671
3503.916485	450602.304951	49.434676
3504.102516	450596.442579	49.439681
3504.173316	450586.036785	49.444685
3503.982321	450584.599078	49.449690
3503.858271	450572.604112	49.454695
3503.902055	450573.712073	49.459700
3503.745058	450568.161770	49.464705
3503.799769	450561.865500	49.469709
3503.768518	450556.040218	49.474714
3503.871929	450546.237249	49.479719
3504.229284	450546.226945	49.484724
3504.320829	450539.366667	49.489729
3504.292828	450527.963690	49.494733
3504.331930	450510.667904	49.499738
3504.441689	450480.786114	49.504743
3504.369740	450465.689409	49.509748
3504.207705	450458.618896	49.514753
3504.020904	450448.865435	49.519757
3503.784068	450446.928531	49.524762
3503.839102	450436.221146	49.529767
3503.847911	450434.749312	49.534772
3503.817383	450420.963740	49.539777
3504.158541	450423.592679	49.544781
3503.640251	450410.397399	49.549786
3504.008873	450407.697991	49.554791
3504.022836	450398.417241	49.559796
3503.894183	450390.783289	49.564801
3503.884453	450386.019016	49.569805
3503.617186	450382.464852	49.574810
3503.804319	450369.047693	49.579815
3503.922025	450361.777278	49.584820
3504.099268	450357.133178	49.589825
3504.032833	450341.528426	49.594829
3503.471951	450341.218594	49.599834
3503.988931	450327.846492	49.604839
3503.973369	450327.342144	49.609844
3503.411917	450322.012940	49.614849
3504.053725	450337.215277	49.619853
3504.019279	450345.384139	49.624858
3504.058160	450335.287880	49.629863
3503.905041	450336.936491	49.634868
3503.896346	450321.778180	49.639873
3504.037688	450308.115293	49.644877
3503.955301	450308.180074	49.649882
3503.764553	450300.810199	49.654887
3503.713645	450308.424167	49.659892
3503.744749	450306.187992	49.664897
3504.200274	450297.997942	49.669901
3503.606653	450295.969839	49.674906
3503.800214	450278.698189	49.679911
3503.567179	450283.098347	49.684916
3503.550444	450275.546646	49.689921
3504.020405	450264.768325	49.694925
3503.922913	450261.894978	49.699930
3503.796025	450249.951013	49.704935
3503.958738	450246.729023	49.709940
3504.182206	450229.908544	49.714945
3503.719058	450219.137420	49.719949
3503.535461	450224.796698	49.724954
3503.830522	450215.873486	49.729959
3504.054562	450212.894529	49.734964
3503.851290	450210.444852	49.739969
3504.009493	450200.328154	49.744973
3503.696326	450195.057927	49.749978
3503.752401	450197.482061	49.754983
3503.540521	450209.382520	49.759988
3503.691076	450217.063526	49.764993
3503.960737	450212.302210	49.769997
3503.806131	450215.877760	49.775002
3503.955734	450212.252387	49.780007
3503.752762	450203.464909	49.785012
3503.865707	450192.291193	49.790017
3503.895292	450185.492080	49.795021
3504.036715	450181.513185	49.800026
3503.497771	450181.960135	49.805031
3503.803548	450180.336172	49.810036
3503.661681	450173.110012	49.815041
3503.932315	450166.219033	49.820045
3503.871243	450159.486093	49.825050
3503.702481	450147.245007	49.830055
3503.795667	450143.781362	49.835060
3503.529657	450162.840092	49.840065
3503.743432	450155.147584	49.845069
3503.727336	450158.395279	49.850074
3503.808967	450152.499907	49.855079
3503.613400	450152.431908	49.860084
3503.549274	450145.750188	49.865089
3503.881261	450137.429063	49.870093
3503.806696	450142.968342	49.875098
3503.804028	450127.504648	49.880103
3503.737056	450125.133093	49.885108
3503.552843	450118.978890	49.890113
3503.994659	450128.942498	49.895117
3503.839654	450141.948732	49.900122
3503.889039	450138.492565	49.905127
3503.802560	450140.180514	49.910132
3504.007412	450137.509036	49.915137
3504.184963	450128.149532	49.920141
3504.008717	450134.111792	49.925146
3504.042862	450112.557541	49.930151
3503.995262	450097.507115	49.935156
3503.849925	450093.577166	49.940161
3503.741901	450089.336632	49.945165
3503.469701	450095.873013	49.950170
3503.549028	450089.217482	49.955175
3503.736539	450095.168345	49.960180
3503.509680	450086.942622	49.965185
3503.938436	450077.793714	49.970189
3503.742337	450074.937178	49.975194
3503.567485	450074.865641	49.980199
3503.676858	450073.680825	49.985204
3503.321493	450091.487318	49.990209
3503.805616	450092.266606	49.995213
3503.517445	450096.524111	50.000218
3503.625902	450080.382279	50.005223
3503.717574	450090.000073	50.010228
3503.903228	450067.710073	50.015233
3503.942765	450062.176780	50.020237
3503.594753	450064.264308	50.025242
3503.486971	450073.713357	50.030247
3503.805685	450092.368096	50.035252
3503.587040	450093.926509	50.040257
3503.939365	450084.537143	50.045261
3503.614633	450081.753274	50.050266
3503.860231	450076.184800	50.055271
3504.084206	450079.188707	50.060276
3504.421325	450070.613168	50.065281
3503.977656	450063.996228	50.070285
3504.017716	450066.169600	50.075290
3503.999565	450050.302874	50.080295
3504.047740	450043.449839	50.085300
3503.755915	450050.952930	50.090305
3504.376981	450043.647158	50.095309
3504.179721	450040.588006	50.100314
3504.122086	450005.765283	50.105319
3503.910286	449999.565053	50.110324
3503.650778	449976.083404	50.115329
3503.796499	449993.703016	50.120333
3503.592550	450000.126367	50.125338
3503.704736	450000.563546	50.130343
3503.974246	450002.241425	50.135348
3504.033331	449991.279608	50.140353
3503.837366	449991.160973	50.145357
3503.819334	449990.150013	50.150362
3504.237645	449979.177555	50.155367
3504.118550	449977.981042	50.160372
3504.035596	449972.367234	50.165377
3504.234959	449962.649014	50.170381
3503.754822	449969.119533	50.175386
3503.890352	449943.339482	50.180391
3503.649139	449953.267692	50.185396
3503.806481	449942.491882	50.190401
3503.851506	449938.123779	50.195405
3503.671471	449938.712261	50.200410
3503.758755	449927.847001	50.205415
3503.880894	449929.550049	50.210420
3503.998207	449933.332729	50.215425
3504.427938	449919.113320	50.220429
3503.912494	449916.970424	50.225434
3504.361532	449914.358629	50.230439
3503.765975	449905.131032	50.235444
3503.725879	449902.247835	50.240449
3503.991492	449900.022276	50.245453
3503.404875	449898.499964	50.250458
3503.541544	449886.358682	50.255463
3503.861301	449886.760421	50.260468
3503.745241	449879.986078	50.265473
3504.787034	449868.400076	50.270477
3504.175474	449878.188746	50.275482
3504.070402	449871.108307	50.280487
3504.120370	449864.153501	50.285492
3503.982521	449856.723734	50.290497
3504.299927	449853.171053	50.295501
3503.936578	449846.134706	50.300506
3504.405398	449837.739396	50.305511
3504.192991	449839.651683	50.310516
3504.472721	449817.345354	50.315521
3504.231548	449788.637960	50.320525
3504.134180	449778.057666	50.325530
3503.861047	449772.932605	50.330535
3503.676106	449762.975693	50.335540
3503.547532	449756.203446	50.340545
3503.624932	449749.852356	50.345549
3503.359690	449771.345059	50.350554
3503.541105	449774.761901	50.355559
3503.454039	449790.089093	50.360564
3503.534162	449780.593960	50.365569
3503.586911	449781.193402	50.370573
3503.856468	449780.184030	50.375578
3503.797350	449764.932519	50.380583
3503.649390	449773.475909	50.385588
3503.511415	449795.656699	50.390593
3503.733746	449789.382279	50.395597
3503.478733	449794.394728	50.400602
3503.701123	449783.455621	50.405607
3504.112951	449780.343133	50.410612
3503.445581	449785.780915	50.415617
3503.457795	449774.573472	50.420621
3503.647094	449775.200301	50.425626
3503.833822	449793.776437	50.430631
3503.548930	449802.546008	50.435636
3503.523641	449805.339001	50.440641
3503.738435	449796.429317	50.445645
3503.514382	449791.143771	50.450650
3503.836523	449786.626913	50.455655
3503.735483	449786.187851	50.460660
3503.425751	449784.212628	50.465665
3503.679027	449789.239695	50.470669
3503.547613	449807.363112	50.475674
3503.436637	449808.903161	50.480679
3503.412275	449815.194499	50.485684
3503.603305	449808.621213	50.490689
3503.807467	449801.437246	50.495693
3503.434137	449807.889577	50.500698
3503.236490	449812.283792	50.505703
3503.517463	449824.049612	50.510708
3503.684944	449829.294131	50.515713
3503.807766	449827.346461	50.520717
3503.510709	449826.433839	50.525722
3503.339761	449819.466037	50.530727
3503.771224	449819.290971	50.535732
3503.671354	449795.832565	50.540737
3504.090808	449766.454607	50.545741
3503.936386	449723.332636	50.550746
3503.866951	449660.624594	50.555751
3504.078577	449589.502299	50.560756
3503.896307	449518.294909	50.565761
3503.959427	449417.535725	50.570765
3503.730606	449329.907572	50.575770
3503.425653	449202.032777	50.580775
3503.666309	449090.847301	50.585780
3503.327309	448955.066881	50.590785
3503.673855	448807.658411	50.595789
3503.772828	448657.806601	50.600794
3503.548314	448486.509564	50.605799
3503.806386	448307.421335	50.610804
3503.713757	448118.047236	50.615809
3503.816199	447910.636965	50.620813
3503.996333	447694.692444	50.625818
3503.772957	447455.640793	50.630823
3503.910928	447213.685030	50.635828
3503.547627	446955.534258	50.640833
3503.723926	446686.233336	50.645837
3503.446429	446411.833961	50.650842
3503.209095	446117.443751	50.655847
3503.506822	445813.221317	50.660852
3503.358548	445505.165790	50.665857
3503.418770	445182.921025	50.670861
3503.097820	444848.514239	50.675866
3503.332472	444496.358346	50.680871
3503.178092	444136.757085	50.685876
3503.128608	443765.974106	50.690881
3503.131882	443370.171660	50.695885
3503.332672	442982.696929	50.700890
3503.043124	442558.222590	50.705895
3503.202508	442124.634948	50.710900
3502.737598	441681.153015	50.715905
3503.228954	441227.049816	50.720909
3503.066901	440755.193818	50.725914
3502.714138	440260.127988	50.730919
3502.800643	439770.911053	50.735924
3502.855767	439253.078182	50.740929
3502.918669	438714.635909	50.745933
3502.811018	438172.455681	50.750938
3502.842667	437608.474661	50.755943
3502.705172	437032.738288	50.760948
3502.437348	436446.253759	50.765953
3502.942128	435838.769734	50.770957
3502.615172	435207.209885	50.775962
3502.726558	434569.164566	50.780967
3502.656285	433908.908339	50.785972
3502.362496	433238.218485	50.790977
3502.827683	432529.575990	50.795981
3502.389313	431814.824412	50.800986
3502.405609	431094.340297	50.805991
3502.481254	430343.425851	50.810996
3502.301098	429581.315312	50.816001
3502.400335	428785.179839	50.821005
3501.955376	427983.679821	50.826010
3501.709910	427165.927885	50.831015
3501.479940	426333.527355	50.836020
3501.409077	425488.533403	50.841025
3501.599809	424613.922774	50.846029
3501.584634	423729.010971	50.851034
3501.583064	422824.469800	50.856039
3501.210015	421885.285622	50.861044
3501.136020	420954.188015	50.866049
3501.197980	419982.162613	50.871053
3500.724718	419009.835153	50.876058
3500.713216	418003.347341	50.881063
3500.607808	416992.062363	50.886068
3500.369401	415959.712338	50.891073
3500.844420	414899.193610	50.896077
3500.799080	413833.514735	50.901082
3500.315516	412742.500092	50.906087
3500.160124	411624.593918	50.911092
3500.108659	410495.651992	50.916097
3500.024557	409345.893991	50.921101
3499.642832	408184.937277	50.926106
3499.522548	406994.576885	50.931111
3499.494098	405787.969406	50.936116
3499.172780	404572.443143	50.941121
3499.401026	403329.895051	50.946125
3499.085266	402079.814279	50.951130
3498.949446	400796.673453	50.956135
3499.181612	399507.669976	50.961140
3498.585686	398194.156910	50.966145
3498.545691	396854.091215	50.971149
3498.447643	395521.265538	50.976154
3498.192229	394152.350561	50.981159
3497.868690	392760.514576	50.986164
3497.706319	391363.071909	50.991169
3497.860573	389947.365835	50.996173
3497.640386	388512.368894	51.001178
3497.537393	387057.664760	51.006183
3496.988759	385586.651643	51.011188
3497.016572	384102.737357	51.016193
3496.567162	382594.814984	51.021197
3496.068514	381086.347623	51.026202
3495.914938	379558.660582	51.031207
3495.976692	378017.799279	51.036212
3495.473046	376455.506424	51.041217
3495.468318	374867.682860	51.046221
3495.506241	373288.118375	51.051226
3495.067091	371681.738561	51.056231
3495.784107	370043.506834	51.061236
3495.249492	368397.810757	51.066241
3495.061245	366725.355655	51.071245
3494.524403	365050.061546	51.076250
3494.189728	363351.794285	51.081255
3494.352830	361647.008000	51.086260
3493.734558	359923.585597	51.091265
3493.738879	358183.270124	51.096269
3493.584474	356442.626427	51.101274
3493.075960	354665.694180	51.106279
3492.743991	352880.744187	51.111284
3492.278111	351088.923779	51.116289
3492.371811	349275.333669	51.121293
3491.987843	347464.981513	51.126298
3491.982842	345632.025043	51.131303
3491.925245	343775.188182	51.136308
3491.157868	341911.248615	51.141313
3490.518829	340013.650573	51.146317
3490.601889	338118.883776	51.151322
3490.581051	336213.272823	51.156327
3490.023280	334296.179557	51.161332
3489.590155	332366.040790	51.166337
3489.726605	330416.570816	51.171341
3489.109429	328462.121226	51.176346
3488.990518	326488.556806	51.181351
3488.867646	324504.999334	51.186356
3488.170544	322511.292556	51.191361
3488.112596	320499.975421	51.196365
3487.649154	318474.765046	51.201370
3487.022809	316442.214093	51.206375
3487.140015	314405.376834	51.211380
3486.871487	312351.183966	51.216385
3486.423695	310270.333725	51.221389
3486.038274	308209.681864	51.226394
3485.703830	306119.840731	51.231399
3485.253039	304011.914462	51.236404
3484.787376	301897.471760	51.241409
3484.534719	299765.781375	51.246413
3484.595632	297634.676805	51.251418
3483.815167	295484.037869	51.256423
3483.682589	293327.285580	51.261428
3483.304614	291163.734250	51.266433
3483.057369	288981.480567	51.271437
3482.793909	286791.475782	51.276442
3481.975689	284579.604170	51.281447
3481.865002	282359.734527	51.286452
3481.201996	280143.060356	51.291457
3481.028407	277908.778486	51.296461
3480.649171	275667.603977	51.301466
3480.192289	273421.274733	51.306471
3479.663683	271154.613725	51.311476
3479.118566	268890.789442	51.316481
3478.841554	266612.106955	51.321485
3478.579741	264318.586595	51.326490
3477.931574	262021.200001	51.331495
3477.738391	259702.793690	51.336500
3477.191917	257398.705605	51.341505
3476.565557	255064.781216	51.346509
3476.199612	252731.552760	51.351514
3475.079935	250389.646003	51.356519
3475.021690	248042.650772	51.361524
3474.524075	245701.930557	51.366529
3473.881765	243326.689830	51.371533
3473.549250	240967.127683	51.376538
3472.856493	238601.434113	51.381543
3472.334656	236215.234888	51.386548
3471.853849	233832.876787	51.391553
3471.622733	231443.580584	51.396557
3470.798719	229040.439758	51.401562
3470.304638	226632.239109	51.406567
3469.888955	224220.247579	51.411572
3469.532578	221812.162333	51.416577
3468.826453	219378.823843	51.421581
3468.352025	216964.164049	51.426586
3467.688777	214527.007337	51.431591
3467.213923	212080.076422	51.436596
3466.686420	209638.489936	51.441601
3466.177090	207191.609100	51.446605
3465.422321	204727.045836	51.451610
3464.990568	202271.440346	51.456615
3464.609054	199796.570654	51.461620
3463.784326	197330.682461	51.466625
3463.348551	194848.943706	51.471629
3462.670132	192374.695792	51.476634
3461.857060	189890.945061	51.481639
3461.444323	187396.612362	51.486644
3460.817051	184908.988087	51.491649
3460.635978	182410.820988	51.496653
3459.969549	179908.472449	51.501658
3459.032018	177395.051889	51.506663
3458.762716	174885.354777	51.511668
3457.779465	172370.765217	51.516673
3456.879604	169854.281434	51.521677
3456.169521	167343.840563	51.526682
3455.048772	164823.214269	51.531687
3454.574595	162307.402965	51.536692
3453.572831	159800.540604	51.541697
3453.118438	157292.703339	51.546701
3452.009390	154777.080178	51.551706
3451.752660	152276.729762	51.556711
3450.779518	149758.031824	51.561716
3450.054501	147245.421002	51.566721
3449.332006	144669.939556	51.571725
3448.477191	142171.580646	51.576730
3447.474153	139659.526838	51.581735
3447.027212	137157.029220	51.586740
3446.096080	134657.238074	51.591745
3445.308340	132155.372221	51.596749
3444.635751	129664.505745	51.601754
3443.847906	127166.150951	51.606759
3443.233167	124663.123321	51.611764
3441.737079	122178.974303	51.616769
3441.008144	119684.212913	51.621773
3440.275803	117205.426707	51.626778
3439.161042	114733.877153	51.631783
3438.406169	112259.290749	51.636788
3437.308815	109800.969883	51.641793
3436.913423	107333.451021	51.646797
3435.795622	104868.996211	51.651802
3434.629816	102425.434232	51.656807
3434.019421	99970.444000	51.661812
3432.715404	97535.335106	51.666817
3431.728505	95097.649486	51.671821
3430.583080	92680.870948	51.676826
3429.893146	90265.627119	51.681831
3429.150563	87855.776722	51.686836
3427.731135	85447.964331	51.691841
3426.556523	83047.554400	51.696845
3425.343056	80676.371942	51.701850
3424.360986	78307.448500	51.706855
3423.701736	75948.133745	51.711860
3422.261578	73603.689268	51.716865
3421.085480	71255.738560	51.721869
3420.189471	68936.437787	51.726874
3418.652547	66607.600364	51.731879
3417.737277	64305.835801	51.736884
3416.245983	62019.269882	51.741889
3415.201614	59743.518314	51.746893
3413.953898	57473.736707	51.751898
3412.442290	55246.853054	51.756903
3411.585829	53008.625607	51.761908
3409.745325	50800.835206	51.766913
3408.832756	48607.257570	51.771917
3407.544264	46437.393718	51.776922
3405.686693	44275.248427	51.781927
3404.233951	42132.817557	51.786932
3402.613590	40029.065829	51.791937
3400.911028	37930.834899	51.796941
3399.215431	35872.043205	51.801946
3397.210255	33836.691469	51.806951
3395.053431	31834.779513	51.811956
3391.685459	29899.366734	51.816961
3386.671933	28049.638380	51.821965
3381.275290	26285.777536	51.826970
3375.880919	24602.314514	51.831975
3370.922083	23002.723424	51.836980
3366.152872	21489.933068	51.841985
3361.368138	20067.783695	51.846989
3356.851767	18735.735457	51.851994
3352.923946	17494.631393	51.856999
3349.077537	16335.185183	51.862004
3345.316911	15279.464013	51.867009
3341.831512	14292.538876	51.872013
3338.976314	13380.569510	51.877018
3335.577482	12542.230472	51.882023
3332.745552	11765.122945	51.887028
3330.374645	11063.512718	51.892033
3327.761062	10416.889135	51.897037
3325.612598	9834.953234	51.902042
3323.444371	9301.273400	51.907047
3321.240288	8803.053083	51.912052
3319.010942	8362.725724	51.917057
3317.434003	7965.783814	51.922061
3316.220003	7620.637904	51.927066
3314.521647	7296.175694	51.932071
3313.199530	6996.829767	51.937076
3312.285525	6746.689645	51.942081
3311.112604	6501.768296	51.947085
3309.868761	6289.314949	51.952090
3308.629580	6091.661236	51.957095
3308.192524	5916.224296	51.962100
3307.242726	5762.103426	51.967105
3306.549314	5612.798665	51.972109
3306.109133	5480.586669	51.977114
3305.120977	5364.058404	51.982119
3304.410555	5244.127268	51.987124
3303.800328	5149.459227	51.992129
3303.449079	5053.709837	51.997133
3302.611405	4958.987805	52.002138
3302.037065	4882.672551	52.007143
3302.052537	4807.814965	52.012148
3301.582603	4725.268553	52.017153
3300.975979	4653.200531	52.022157
3300.852153	4584.944268	52.027162
3300.510483	4512.518907	52.032167
3300.025754	4437.396313	52.037172
3299.314177	4360.336286	52.042177
3299.126789	4294.152373	52.047181
3298.936241	4221.669354	52.052186
3298.226148	4155.411062	52.057191
3298.008847	4077.487787	52.062196
3297.540909	4001.717657	52.067201
3297.195187	3931.855680	52.072205
3296.877712	3861.260344	52.077210
3296.421880	3782.152159	52.082215
3296.100897	3701.873991	52.087220
3295.130946	3624.373679	52.092225
3294.809964	3544.424795	52.097229
3294.451399	3466.313872	52.102234
3293.789800	3389.866717	52.107239
3293.644586	3299.248913	52.112244
3293.179499	3214.937624	52.117249
3292.494674	3142.712945	52.122253
3292.348493	3056.170284	52.127258
3291.699551	2970.014820	52.132263
3291.347021	2872.337957	52.137268
3290.818437	2795.229011	52.142273
3290.411886	2687.127293	52.147277
3290.181024	2584.445192	52.152282
3289.291773	2491.345608	52.157287
3288.948221	2386.920920	52.162292
3288.315866	2305.326017	52.167297
3287.270838	2193.939244	52.172301
3286.656505	2097.111724	52.177306
3286.060635	2006.875975	52.182311
3285.545299	1907.111371	52.187316
3284.315478	1820.111596	52.192321
3283.842461	1723.730429	52.197325
3283.372689	1640.366321	52.202330
3282.362312	1568.469751	52.207335
3281.370417	1473.143961	52.212340
3280.552535	1393.269538	52.217345
3279.576443	1328.139143	52.222349
3278.744812	1242.697398	52.227354
3278.139937	1180.820154	52.232359
3277.708432	1130.792853	52.237364
3276.840441	1071.438464	52.242369
3276.129202	1016.183850	52.247373
3275.812261	952.342594	52.252378
3275.129026	893.136535	52.257383
3274.556580	827.461622	52.262388
3273.711150	766.877268	52.267393
3273.074656	707.614583	52.272397
3272.624122	645.031368	52.277402
3271.609947	595.935457	52.282407
3271.096470	527.981577	52.287412
3270.061079	486.591774	52.292417
3269.213753	431.193923	52.297421
3268.244233	371.195592	52.302426
3267.600627	340.668265	52.307431
3266.769951	303.096580	52.312436
3266.084437	254.894536	52.317441
3265.352895	220.685806	52.322445
3264.901969	190.350854	52.327450
3263.502350	164.894651	52.332455
3262.603318	140.611762	52.337460
3260.714379	151.078608	52.342465
3259.463326	157.140255	52.347469
3258.994509	151.652705	52.352474
3258.506335	160.823568	52.357479
3258.433715	150.663818	52.362484
3257.705586	155.990749	52.367489
3257.174036	159.492818	52.372493
3256.771143	162.362657	52.377498
3255.865143	166.940389	52.382503
3255.226347	165.375483	52.387508
3254.734555	167.328950	52.392513
3254.628548	166.354722	52.397517
3253.807867	165.231014	52.402522
3252.835044	169.689506	52.407527
3252.270788	165.389814	52.412532
3251.567444	160.908625	52.417537
3250.747951	165.175926	52.422541
3250.601397	162.722075	52.427546
3249.967722	165.811338	52.432551
3249.630459	156.305865	52.437556
3248.837803	162.629460	52.442561
3247.724377	159.135681	52.447565
3247.594040	158.192057	52.452570
3246.647154	166.428808	52.457575
3246.326207	163.179372	52.462580
3245.392208	162.331203	52.467585
3244.693403	153.618536	52.472589
3244.090308	157.997284	52.477594
3243.821218	160.613348	52.482599
3242.962990	154.836280	52.487604
3242.242019	156.901134	52.492609
3241.534959	163.646677	52.497613
3241.481439	160.740363	52.502618
3240.513814	167.518976	52.507623
3239.711432	158.317565	52.512628
3239.595287	162.285104	52.517633
3238.686324	169.187904	52.522637
3238.237446	154.101084	52.527642
3237.288877	159.086737	52.532647
3236.698530	159.179709	52.537652
3235.883615	151.062002	52.542657
3234.584589	162.896076	52.547661
3234.658018	160.296489	52.552666
3233.958426	162.938339	52.557671
3233.473308	163.007413	52.562676
3233.093403	161.109341	52.567681
3232.026846	160.076982	52.572685
3231.385425	156.412177	52.577690
3230.554707	164.775131	52.582695
3230.362887	154.326280	52.587700
3229.531244	157.251999	52.592705
3228.917239	157.043099	52.597709
3228.507958	152.402338	52.602714
3227.583746	165.536565	52.607719
3227.141342	151.108631	52.612724
3226.859479	154.858959	52.617729
3225.757449	159.383341	52.622733
3225.248798	152.764597	52.627738
3224.447074	154.394441	52.632743
3223.740617	150.542200	52.637748
3222.914103	153.561384	52.642753
3222.341888	165.034454	52.647757
3222.231318	160.568839	52.652762
3221.285956	157.878047	52.657767
3220.772303	152.988677	52.662772
3219.856660	151.237001	52.667777
3219.132272	159.583761	52.672781
3218.561046	158.819275	52.677786
3217.904688	153.079565	52.682791
3217.271925	150.707600	52.687796
3216.290786	154.020432	52.692801
3215.747586	155.784528	52.697805
3215.319256	151.689381	52.702810
3215.038262	151.866080	52.707815
3214.649400	149.577181	52.712820
3213.518659	146.858459	52.717825
3212.371842	154.819107	52.722829
3211.932435	147.636312	52.727834
3211.406890	153.957297	52.732839
3211.241937	152.372629	52.737844
3210.313206	152.918933	52.742849
3209.268207	150.372665	52.747853
3208.911790	148.807681	52.752858
3208.440471	157.070943	52.757863
3207.908153	149.547975	52.762868
3206.860288	145.822749	52.767873
3206.239146	154.903826	52.772877
3205.953155	142.790714	52.777882
3204.888910	144.995136	52.782887
3204.300023	156.058161	52.787892
3204.235688	150.651118	52.792897
3203.495813	138.876075	52.797901
3203.053777	140.270394	52.802906
3202.028339	146.601388	52.807911
3200.747049	149.495379	52.812916
3200.379702	145.287188	52.817921
3199.486679	150.797025	52.822925
3199.275506	144.622061	52.827930
3198.137042	145.916684	52.832935
3197.723194	143.076673	52.837940
3196.993773	152.001777	52.842945
3196.515601	143.312220	52.847949
3195.736356	139.413212	52.852954
3195.715442	144.809183	52.857959
3195.011070	143.492723	52.862964
3194.196532	139.302515	52.867969
3193.116084	154.420094	52.872973
3192.361474	143.849121	52.877978
3191.758789	153.060067	52.882983
3191.487409	140.677232	52.887988
3190.601452	140.755583	52.892993
3189.981875	147.542227	52.897997
3189.092540	136.128638	52.903002
3188.705584	145.368248	52.908007
3188.073626	146.479234	52.913012
3187.332040	139.506359	52.918017
3186.411590	146.576507	52.923021
3185.882754	137.290887	52.928026
3185.477460	138.638667	52.933031
3184.929162	127.396157	52.938036
3184.195754	136.239436	52.943041
3183.054740	140.714428	52.948045
3183.250404	136.356763	52.953050
3182.514958	145.364207	52.958055
3181.720803	139.046091	52.963060
3180.993569	143.277894	52.968065
3180.168258	138.223890	52.973069
3179.441194	141.230427	52.978074
3178.380640	147.507030	52.983079
3178.146109	128.854360	52.988084
3178.015718	138.001975	52.993089
3176.723655	143.929323	52.998093
3176.087625	130.900656	53.003098
3175.384743	139.328204	53.008103
3174.509255	140.273171	53.013108
3174.573952	142.723655	53.018113
3174.083733	148.461117	53.023117
3173.612696	145.827847	53.028122
3172.373970	143.327712	53.033127
3171.584534	133.342558	53.038132
3171.385861	139.883607	53.043137
3170.278321	147.356766	53.048141
3169.419187	140.990149	53.053146
3168.748531	141.683415	53.058151
3168.996126	136.993595	53.063156
3168.098195	139.236316	53.068161
3167.076833	139.175571	53.073165
3167.091152	131.925929	53.078170
3166.129585	146.202944	53.083175
3165.366324	130.648046	53.088180
3164.619462	130.984472	53.093185
3163.498952	141.219388	53.098189
3162.860762	134.135699	53.103194
3161.839433	138.954579	53.108199
3161.763747	137.897020	53.113204
3161.096407	133.442465	53.118209
3160.364807	143.751855	53.123213
3160.017806	135.549886	53.128218
3158.860584	135.628405	53.133223
3158.136562	132.349168	53.138228
3157.827912	127.630837	53.143233
3157.556948	140.594225	53.148237
3157.438857	131.939474	53.153242
3156.248155	139.430391	53.158247
3155.018218	136.648108	53.163252
3154.598019	128.254576	53.168257
3153.845492	132.998714	53.173261
3153.697136	132.732764	53.178266
3152.637711	141.416621	53.183271
3152.276431	139.882079	53.188276
3151.453202	134.299580	53.193281
3150.536114	134.571541	53.198285
3149.883840	127.384871	53.203290
3149.134912	131.265914	53.208295
3148.337447	135.216039	53.213300
3148.216373	130.926307	53.218305
3147.635973	139.320299	53.223309
3147.492125	127.669623	53.228314
3146.315339	139.905162	53.233319
3144.877037	135.241682	53.238324
3144.215795	132.550128	53.243329
3143.797862	133.463896	53.248333
3143.538625	128.198715	53.253338
3142.467429	143.396807	53.258343
3142.100757	138.980881	53.263348
3142.424458	128.565951	53.268353
3141.152483	131.938347	53.273357
3139.989555	132.683751	53.278362
3139.280602	133.395010	53.283367
3139.110075	137.252230	53.288372
3138.663480	135.995549	53.293377
3137.220876	130.929790	53.298381
3137.038951	131.695474	53.303386
3136.641508	140.848058	53.308391
3135.508275	139.809349	53.313396
3135.183655	132.786956	53.318401
3134.225232	142.206700	53.323405
3133.861222	138.016105	53.328410
3132.833815	141.518030	53.333415
3132.349901	136.065451	53.338420
3131.650305	134.532268	53.343425
3130.652830	135.054014	53.348429
3130.186287	131.634081	53.353434
3129.398694	138.823238	53.358439
3128.199758	130.862755	53.363444
3128.115452	137.998063	53.368449
3128.126624	139.260481	53.373453
3127.594790	134.918566	53.378458
3126.264793	135.938827	53.383463
3125.153523	134.781897	53.388468
3125.083493	133.971656	53.393473
3125.090623	138.752185	53.398477
3124.209228	133.671066	53.403482
3122.759923	124.256164	53.408487
3121.805380	126.421327	53.413492
3122.203678	127.382736	53.418497
3121.509663	129.667198	53.423501
3120.559899	123.132931	53.428506
3119.268639	132.969529	53.433511
3119.198067	125.328222	53.438516
3119.254710	123.503204	53.443521
3118.079398	130.337034	53.448525
3116.866410	125.854537	53.453530
3115.863752	135.644195	53.458535
3116.195436	130.175028	53.463540
3115.595430	121.991828	53.468545
3114.477423	133.902329	53.473549
3113.951719	121.630870	53.478554
3113.220036	126.951698	53.483559
3112.820248	122.300260	53.488564
3111.987632	124.836951	53.493569
3110.551813	127.540652	53.498573
3110.824153	119.292087	53.503578
3110.297628	127.662657	53.508583
3109.732408	123.159088	53.513588
3108.115105	126.892459	53.518593
3107.729066	130.744263	53.523597
3107.614773	124.362900	53.528602
3107.264573	136.135109	53.533607
3105.423960	127.240612	53.538612
3105.473586	124.313924	53.543617
3104.933202	128.784586	53.548621
3104.114686	119.129287	53.553626
3102.751826	133.533277	53.558631
3102.632720	136.730015	53.563636
3102.942923	129.406139	53.568641
3101.559932	126.112403	53.573645
3100.563053	130.358307	53.578650
3099.351721	131.184224	53.583655
3099.260715	128.617082	53.588660
3099.230078	120.093056	53.593665
3097.856177	133.197121	53.598669
3097.129149	127.646750	53.603674
3097.254851	121.180963	53.608679
3096.222284	129.040775	53.613684
3095.418072	125.945773	53.618689
3094.436341	128.622416	53.623693
3093.898608	127.656437	53.628698
3093.636300	126.654845	53.633703
3093.262548	131.150325	53.638708
3092.358672	117.837068	53.643713
3091.342915	128.606702	53.648717
3090.518709	121.795205	53.653722
3089.769533	124.109620	53.658727
3089.607855	128.628862	53.663732
3089.066244	126.066479	53.668737
3087.781295	132.676289	53.673741
3088.131491	131.172551	53.678746
3086.703108	125.313740	53.683751
3085.882060	126.776378	53.688756
3085.644915	119.260247	53.693761
3084.677544	127.615355	53.698765
3084.651917	122.415264	53.703770
3083.584603	129.765895	53.708775
3082.944572	123.259633	53.713780
3082.478001	119.889843	53.718785
3081.661334	128.095257	53.723789
3081.344092	120.128218	53.728794
3080.955291	124.171542	53.733799
3079.968959	126.924760	53.738804
3079.328001	122.166511	53.743809
3078.026953	126.392154	53.748813
3077.294925	119.734644	53.753818
3077.224357	127.256404	53.758823
3076.603337	126.990299	53.763828
3075.531017	126.194611	53.768833
3074.307446	136.839500	53.773837
3074.842250	128.861473	53.778842
3073.904088	127.889708	53.783847
3072.887955	131.066037	53.788852
3071.813876	125.636943	53.793857
3071.884588	124.459637	53.798861
3072.094765	118.468880	53.803866
3070.930523	122.633649	53.808871
3069.591855	128.573708	53.813876
3069.526949	124.753980	53.818881
3068.494544	133.889923	53.823885
3067.846064	123.159943	53.828890
3067.192543	130.168300	53.833895
3066.333053	126.976566	53.838900
3065.711852	128.828207	53.843905
3065.220133	127.471483	53.848909
3064.458875	119.575973	53.853914
3063.714276	115.755941	53.858919
3062.960578	116.119205	53.863924
3062.330995	114.890247	53.868929
3061.999320	126.721253	53.873933
3061.710551	125.329852	53.878938
3060.558318	119.370578	53.883943
3059.336125	130.346010	53.888948
3058.864011	119.990494	53.893953
3058.170503	119.886380	53.898957
3058.373923	121.995003	53.903962
3057.569593	133.152846	53.908967
3056.243667	122.366918	53.913972
3055.801315	121.479775	53.918977
3055.179543	130.108984	53.923981
3054.860449	116.545821	53.928986
3054.135639	130.020939	53.933991
3053.551233	126.497211	53.938996
3053.083590	120.297807	53.944001
3052.412621	130.855376	53.949005
3051.061724	116.433544	53.954010
3050.502485	121.200711	53.959015
3049.640494	123.374542	53.964020
3049.572816	123.438222	53.969025
3048.564114	125.640281	53.974029
3048.041385	122.157330	53.979034
3046.994365	115.340893	53.984039
3046.653350	128.497805	53.989044
3046.638875	117.320429	53.994049
3045.409639	119.720824	53.999053
3045.031074	116.501392	54.004058
3044.625459	112.259504	54.009063
3043.466795	123.522491	54.014068
3042.501958	113.856292	54.019073
3041.713160	127.956932	54.024077
3041.803138	120.693192	54.029082
3040.676270	118.488577	54.034087
3039.649159	119.667886	54.039092
3039.594952	117.888652	54.044097
3038.577818	120.405170	54.049101
3038.125171	113.358493	54.054106
3037.423226	125.171451	54.059111
3036.826706	114.677337	54.064116
3036.413482	110.916343	54.069121
3035.629221	122.738628	54.074125
3035.355706	117.668134	54.079130
3034.729196	116.802198	54.084135
3033.422295	128.061309	54.089140
3032.410004	123.288363	54.094145
3031.957489	122.738081	54.099149
3031.975582	114.482837	54.104154
3030.768132	125.368120	54.109159
3029.665848	125.899502	54.114164
3029.523033	115.751404	54.119169
3028.522722	128.025074	54.124173
3028.458232	124.735791	54.129178
3027.872350	119.167633	54.134183
3027.229080	116.379083	54.139188
3026.710626	112.855145	54.144193
3026.086697	128.634807	54.149197
3025.030990	109.106884	54.154202
3023.884439	121.728031	54.159207
3022.784056	120.415714	54.164212
3023.464509	122.416770	54.169217
3022.462734	124.581333	54.174221
3021.662079	122.087696	54.179226
3021.067068	120.939675	54.184231
3020.147029	128.714346	54.189236
3019.846382	115.617765	54.194241
3019.330080	129.050937	54.199245
3018.872232	120.997014	54.204250
3017.883072	123.132581	54.209255
3016.244123	129.054488	54.214260
3016.534662	120.715977	54.219265
3015.317888	118.844091	54.224269
3014.987104	115.441634	54.229274
3014.493054	118.623096	54.234279
3014.037465	125.071064	54.239284
3013.545747	112.513177	54.244289
3012.855146	125.991918	54.249293
3012.296717	126.437476	54.254298
3010.823455	119.893614	54.259303
3009.605962	121.445714	54.264308
3010.352341	117.100528	54.269313
3008.970420	121.959724	54.274317
3008.238379	124.828179	54.279322
3007.392242	112.701899	54.284327
3006.597385	115.192281	54.289332
3007.068182	113.891349	54.294337
3005.981412	122.863295	54.299341
3005.409837	113.140170	54.304346
3004.959181	119.471638	54.309351
3004.154818	113.750561	54.314356
3003.192865	113.520619	54.319361
3002.037505	120.957745	54.324365
3001.252770	109.609641	54.329370
3001.820092	113.437478	54.334375
3000.498253	121.124100	54.339380
3000.137501	114.652237	54.344385
2999.634991	121.591762	54.349389
2998.745456	116.834558	54.354394
2998.454265	120.228851	54.359399
2996.674011	125.610053	54.364404
2996.154356	119.957163	54.369409
2996.159714	119.761265	54.374413
2995.016956	119.398803	54.379418
2994.095805	115.042519	54.384423
2993.952798	113.039652	54.389428
2993.768208	119.182369	54.394433
2992.838355	119.065755	54.399437
2991.969952	115.381757	54.404442
2991.522840	109.066362	54.409447
2990.964516	116.770535	54.414452
2990.433373	118.128383	54.419457
2989.096444	116.888072	54.424461
2988.347051	114.903564	54.429466
2987.912332	115.867971	54.434471
2987.130191	119.558126	54.439476
2986.621815	112.644529	54.444481
2985.934998	113.044531	54.449485
2985.927484	112.815701	54.454490
2985.330359	111.779359	54.459495
2984.004350	114.229854	54.464500
2983.129822	112.073314	54.469505
2982.081218	112.902629	54.474509
2982.441591	109.694298	54.479514
2981.469468	113.151266	54.484519
2980.961898	114.155358	54.489524
2980.734170	106.240148	54.494529
2980.119527	112.073860	54.499533
2978.866793	113.592121	54.504538
2978.254526	109.648837	54.509543
2977.520704	110.992768	54.514548
2976.883808	113.770757	54.519553
2976.115510	115.270577	54.524557
2975.911646	121.504612	54.529562
2974.829804	117.571702	54.534567
2973.419958	113.195121	54.539572
2973.641110	110.929504	54.544577
2972.680367	111.694861	54.549581
2971.815003	115.425290	54.554586
2971.108070	111.060037	54.559591
2970.527858	121.414990	54.564596
2970.910413	114.678351	54.569601
2969.502562	117.738082	54.574605
2969.061362	99.774088	54.579610
2969.116713	109.282287	54.584615
2967.788370	119.830608	54.589620
2966.077716	110.509771	54.594625
2965.519335	122.152539	54.599629
2965.836342	113.801617	54.604634
2964.959772	111.443329	54.609639
2963.349927	116.577132	54.614644
2963.738122	106.971843	54.619649
2962.884481	114.158074	54.624653
2962.026830	113.264937	54.629658
2961.342252	118.214179	54.634663
2960.746254	122.906712	54.639668
2960.440621	110.996363	54.644673
2959.938458	117.236372	54.649677
2959.673437	117.523640	54.654682
2959.217417	115.213089	54.659687
2957.837548	118.971049	54.664692
2956.934446	121.547434	54.669697
2956.163367	126.403700	54.674701
2956.058267	118.927782	54.679706
2955.338303	116.815489	54.684711
2953.969270	113.961505	54.689716
2953.261386	109.832070	54.694721
2953.091784	120.013040	54.699725
2952.030509	117.661450	54.704730
2951.246424	112.305199	54.709735
2950.896251	118.425291	54.714740
2950.312594	103.327280	54.719745
2949.533143	106.422124	54.724749
2949.085440	113.843715	54.729754
2949.077152	111.372576	54.734759
2948.703178	116.940959	54.739764
2947.674575	103.041589	54.744769
2946.765138	112.033755	54.749773
2945.693321	105.849596	54.754778
2945.159333	109.100251	54.759783
2944.330421	112.466436	54.764788
2943.758763	98.423460	54.769793
2943.497412	109.295479	54.774797
2942.246731	109.682504	54.779802
2941.390809	102.726077	54.784807
2940.520911	108.651962	54.789812
2940.730085	110.319868	54.794817
2939.462878	113.803584	54.799821
2939.173735	113.901560	54.804826
2939.010899	110.919214	54.809831
2938.324685	113.423010	54.814836
2937.943209	104.676339	54.819841
2936.170821	109.543852	54.824845
2935.224452	108.175235	54.829850
2934.679375	109.066928	54.834855
2934.420794	114.458489	54.839860
2934.775039	108.361017	54.844865
2933.822940	109.337265	54.849869
2932.750373	107.815351	54.854874
2932.440567	112.709627	54.859879
2931.103313	112.396205	54.864884
2930.373309	96.015882	54.869889
2929.508868	117.343848	54.874893
2929.211066	109.265754	54.879898
2929.060682	98.333074	54.884903
2927.943485	120.206724	54.889908
2928.131072	109.485483	54.894913
2926.461122	108.015134	54.899917
2925.678799	117.069658	54.904922
2924.916188	109.931106	54.909927
2923.998753	115.250923	54.914932
2923.750412	107.589499	54.919937
2923.089302	110.703989	54.924941
2922.822701	108.417123	54.929946
2922.598431	109.360964	54.934951
2922.030614	115.470091	54.939956
2921.435171	109.248737	54.944961
2920.124853	111.034606	54.949965
2919.107504	110.253633	54.954970
2919.062528	112.603244	54.959975
2918.180652	111.277686	54.964980
2917.685519	102.797146	54.969985
2916.239645	112.462026	54.974989
2915.681434	118.688720	54.979994
2915.149742	107.029378	54.984999
2914.514028	112.553676	54.990004
2914.333517	107.093103	54.995009
2913.472145	111.671517	55.000013
2913.072692	117.218597	55.005018
2912.588891	110.626858	55.010023
2911.718496	121.077584	55.015028
2911.579673	115.268051	55.020033
2910.091174	112.942113	55.025037
2909.324976	110.841676	55.030042
2909.180051	112.490360	55.035047
2908.456520	118.971485	55.040052
2907.273166	108.319539	55.045057
2906.141221	107.328028	55.050061
2905.520730	104.962303	55.055066
2905.956894	101.422870	55.060071
2904.860291	108.400368	55.065076
2904.322076	106.182421	55.070081
2903.550504	110.306554	55.075085
2902.987743	102.653474	55.080090
2902.855965	105.053837	55.085095
2901.538241	107.509247	55.090100
2901.145383	106.842996	55.095105
2900.173318	105.612589	55.100109
2899.276293	121.674559	55.105114
2899.187111	111.443107	55.110119
2898.316173	118.575460	55.115124
2897.817108	106.042148	55.120129
2896.718323	107.933973	55.125133
2895.722946	102.357274	55.130138
2895.307481	99.678626	55.135143
2894.580139	101.109878	55.140148
2894.088152	105.689111	55.145153
2893.832286	109.649323	55.150157
2893.324028	106.832984	55.155162
2893.502729	104.157002	55.160167
2891.814009	109.282588	55.165172
2891.337109	108.259658	55.170177
2890.206374	114.034341	55.175181
2889.556150	108.960745	55.180186
2889.417765	98.770079	55.185191
2888.491341	111.127033	55.190196
2887.446667	96.354143	55.195201
2886.475849	104.238540	55.200205
2885.709001	105.378526	55.205210
2886.331342	97.413184	55.210215
2885.473015	109.765999	55.215220
2884.978267	104.733728	55.220225
2884.519440	106.941307	55.225229
2883.005870	105.655029	55.230234
2882.345604	111.928767	55.235239
2881.904800	115.471389	55.240244
2881.394117	104.987119	55.245249
2880.898626	104.512088	55.250253
2879.817798	110.414818	55.255258
2878.854933	107.118820	55.260263
2878.039446	104.558667	55.265268
2877.460781	99.151935	55.270273
2877.174300	106.417683	55.275277
2876.304150	106.808372	55.280282
2875.826085	98.172561	55.285287
2875.733725	115.551571	55.290292
2875.032991	104.434668	55.295297
2874.060717	112.178007	55.300301
2873.249700	117.516353	55.305306
2872.855132	110.578590	55.310311
2871.747906	109.364972	55.315316
2871.123593	103.846043	55.320321
2870.396427	106.611047	55.325325
2869.542154	112.925837	55.330330
2868.861535	102.601268	55.335335
2867.912147	110.040703	55.340340
2867.988635	104.395296	55.345345
2867.383504	109.036498	55.350349
2866.744034	104.216457	55.355354
2866.391241	100.052010	55.360359
2866.020226	103.814802	55.365364
2864.754091	104.939465	55.370369
2863.669167	103.353758	55.375373
2863.173209	108.536418	55.380378
2863.157998	106.312380	55.385383
2862.084944	110.831058	55.390388
2860.916891	107.193167	55.395393
2860.355544	101.815055	55.400397
2859.736455	108.445298	55.405402
2859.347015	94.755273	55.410407
2858.692345	105.522797	55.415412
2858.293039	102.718631	55.420417
2858.069197	104.753028	55.425421
2856.850545	107.703080	55.430426
2856.121634	97.575054	55.435431
2855.320358	106.486371	55.440436
2854.687534	101.253893	55.445441
2854.282203	112.796681	55.450445
2853.523709	112.044505	55.455450
2852.216459	99.619727	55.460455
2851.684464	111.947166	55.465460
2850.854007	108.326578	55.470465
2850.669926	102.347558	55.475469
2850.118789	101.227980	55.480474
2849.804361	102.909580	55.485479
2849.027589	107.754585	55.490484
2848.997504	98.463549	55.495489
2847.564653	102.011115	55.500493
2846.441600	110.841642	55.505498
2846.364221	105.539893	55.510503
2845.713811	109.104522	55.515508
2845.191397	102.060330	55.520513
2843.757347	102.424243	55.525517
2843.036770	100.726536	55.530522
2842.514049	94.159624	55.535527
2842.172324	104.525515	55.540532
2841.658424	96.796205	55.545537
2841.176266	102.786483	55.550541
2840.502357	99.364138	55.555546
2840.139135	96.598017	55.560551
2838.491868	101.097994	55.565556
2838.244114	100.520629	55.570561
2837.805073	101.054348	55.575565
2837.249451	100.929064	55.580570
2836.243428	97.953864	55.585575
2835.279837	106.982921	55.590580
2834.203043	98.531943	55.595585
2833.746417	101.485968	55.600589
2833.374911	101.369084	55.605594
2833.128020	97.705211	55.610599
2832.674406	105.046495	55.615604
2832.404618	99.968285	55.620609
2831.287142	100.643217	55.625613
2830.164720	106.707003	55.630618
2829.890946	100.191488	55.635623
2828.902576	107.611536	55.640628
2828.643127	99.888080	55.645633
2827.819716	104.445408	55.650637
2826.822785	107.125078	55.655642
2826.160273	100.821261	55.660647
2825.677884	106.406197	55.665652
2825.569155	108.117771	55.670657
2824.874705	107.436757	55.675661
2823.113921	104.401087	55.680666
2822.421845	104.200838	55.685671
2821.587632	118.008841	55.690676
2821.758308	111.617882	55.695681
2821.280268	103.799157	55.700685
2820.499125	112.508490	55.705690
2820.106691	101.038525	55.710695
2819.278215	111.210117	55.715700
2818.684467	108.103275	55.720705
2817.718132	102.552419	55.725709
2816.772038	112.857006	55.730714
2816.719755	105.818912	55.735719
2816.113850	107.318230	55.740724
2815.484130	98.714271	55.745729
2814.605588	104.267047	55.750733
2813.482003	101.829430	55.755738
2812.831529	104.353180	55.760743
2812.317868	105.325564	55.765748
2812.309026	103.542137	55.770753
2811.851541	103.646785	55.775757
2810.271937	108.123364	55.780762
2809.830880	104.649384	55.785767
2808.966893	105.914531	55.790772
2808.696668	96.507442	55.795777
2808.055913	101.407358	55.800781
2807.041018	108.850494	55.805786
2806.469959	105.737802	55.810791
2805.652081	109.534735	55.815796
2805.104524	103.833362	55.820801
2804.377922	103.837169	55.825805
2803.901415	105.794754	55.830810
2803.758638	98.939494	55.835815
2802.219415	103.480618	55.840820
2801.554314	105.943713	55.845825
2801.148189	105.355129	55.850829
2800.263533	113.274547	55.855834
2800.324910	101.701365	55.860839
2799.508105	105.048917	55.865844
2799.205278	102.450103	55.870849
2798.233930	102.853363	55.875853
2797.257749	103.430733	55.880858
2797.290597	94.749852	55.885863
2796.010482	104.069448	55.890868
2794.963618	106.379904	55.895873
2794.204455	100.973246	55.900877
2793.437433	110.242255	55.905882
2793.195366	97.720310	55.910887
2792.654078	99.161614	55.915892
2792.103084	100.025120	55.920897
2791.784002	99.955724	55.925901
2791.060998	107.592913	55.930906
2790.193228	99.104643	55.935911
2789.192421	104.043205	55.940916
2788.625551	101.656096	55.945921
2788.158075	97.468234	55.950925
2787.776601	98.438157	55.955930
2787.108366	98.893819	55.960935
2785.899554	96.548142	55.965940
2784.978415	94.804200	55.970945
2784.705808	91.820893	55.975949
2783.701414	100.448382	55.980954
2783.612875	93.720826	55.985959
2783.317609	105.070718	55.990964
2782.278255	100.169044	55.995969
2781.414828	97.681444	56.000973
2780.489668	103.363371	56.005978
2780.322805	99.204259	56.010983
2779.635328	103.974799	56.015988
2778.812413	102.401563	56.020993
2777.919016	102.742162	56.025997
2776.892839	109.303834	56.031002
2777.204515	105.974351	56.036007
2776.317096	114.993160	56.041012
2775.989817	107.056307	56.046017
2775.076692	105.274681	56.051021
2774.174126	113.353473	56.056026
2773.752745	98.078967	56.061031
2772.891502	104.209827	56.066036
2772.249918	96.233545	56.071041
2771.235219	98.619030	56.076045
2770.199191	109.265033	56.081050
2770.066471	101.844387	56.086055
2769.212596	109.355924	56.091060
2768.484790	103.094461	56.096065
2768.238912	99.647519	56.101069
2767.629058	105.733044	56.106074
2767.751139	95.014734	56.111079
2767.119543	101.035291	56.116084
2765.796855	111.420037	56.121089
2765.323922	103.389665	56.126093
2764.036228	102.883869	56.131098
2763.413086	100.017317	56.136103
2762.458279	106.845861	56.141108
2761.793722	104.950701	56.146113
2761.196959	104.888902	56.151117
2760.400690	93.303246	56.156122
2760.362061	89.340503	56.161127
2760.118503	98.328989	56.166132
2759.902780	97.986936	56.171137
2759.015283	105.616320	56.176141
2757.732949	104.856591	56.181146
2757.165493	102.520900	56.186151
2756.839979	109.682400	56.191156
2755.790329	113.766842	56.196161
2754.798715	102.116678	56.201165
2753.727384	105.412610	56.206170
2753.688084	102.630999	56.211175
2752.887180	106.245435	56.216180
2752.784500	109.421592	56.221185
2752.355788	100.773814	56.226189
2751.256459	110.904469	56.231194
2750.487044	98.690161	56.236199
2749.890376	102.925722	56.241204
2749.467490	105.784777	56.246209
2748.235106	96.747805	56.251213
2747.218990	103.421438	56.256218
2746.569442	92.520820	56.261223
2746.263559	97.929142	56.266228
2745.820056	104.560165	56.271233
2745.800812	94.155347	56.276237
2744.927884	101.106076	56.281242
2743.960249	94.015639	56.286247
2742.942062	102.234581	56.291252
2741.891477	98.094683	56.296257
2742.021650	89.724796	56.301261
2741.274488	105.629293	56.306266
2740.867796	93.896925	56.311271
2739.833994	102.225902	56.316276
2739.103602	101.024873	56.321281
2738.341694	92.629443	56.326285
2737.939797	103.880718	56.331290
2737.583172	92.384523	56.336295
2736.726260	104.711438	56.341300
2735.549052	94.461521	56.346305
2735.126158	97.214791	56.351309
2734.287087	101.873880	56.356314
2734.031009	90.212479	56.361319
2733.392036	107.737779	56.366324
2732.982038	103.640359	56.371329
2731.737048	93.867016	56.376333
2730.738853	102.617395	56.381338
2730.385503	102.600043	56.386343
2729.736097	103.600373	56.391348
2729.426090	110.581990	56.396353
2728.819295	105.223113	56.401357
2728.418377	111.930936	56.406362
2727.550830	97.352424	56.411367
2726.516933	101.542329	56.416372
2726.206348	101.117021	56.421377
2725.889869	97.592549	56.426381
2724.360230	95.042785	56.431386
2723.680529	94.995166	56.436391
2723.243554	95.875898	56.441396
2722.756602	100.792554	56.446401
2722.501607	97.104024	56.451405
2721.753167	105.141077	56.456410
2720.696931	93.480661	56.461415
2720.088790	98.982094	56.466420
2719.257239	99.172003	56.471425
2719.459856	90.094624	56.476429
2718.061653	107.931270	56.481434
2717.284584	88.657834	56.486439
2716.220994	99.231178	56.491444
2715.424950	90.512782	56.496449
2715.264344	93.541341	56.501453
2714.751050	91.258372	56.506458
2714.680755	89.123095	56.511463
2713.667843	90.068326	56.516468
2712.544758	87.430523	56.521473
2712.221597	85.285576	56.526477
2711.371872	90.793170	56.531482
2711.351718	90.226644	56.536487
2710.317934	92.424747	56.541492
2709.149976	90.509067	56.546497
2708.346266	85.484244	56.551501
2707.711130	91.145416	56.556506
2707.859145	97.159817	56.561511
2707.141194	95.496417	56.566516
2706.678631	92.778474	56.571521
2706.150692	94.188293	56.576525
2704.550452	102.456204	56.581530
2704.400309	97.447160	56.586535
2703.889286	95.342219	56.591540
2702.427244	101.329864	56.596545
2702.039088	95.772970	56.601549
2701.333704	98.020333	56.606554
2701.229753	89.019830	56.611559
2700.753117	96.593591	56.616564
2699.828930	94.065077	56.621569
2699.054438	80.264475	56.626573
2697.898851	87.177072	56.631578
2697.248901	91.604104	56.636583
2696.855168	96.624822	56.641588
2696.150319	97.603054	56.646593
2696.211278	88.893696	56.651597
2694.891074	101.442296	56.656602
2693.878688	86.143321	56.661607
2693.483089	94.327288	56.666612
2692.874521	102.066887	56.671617
2692.763265	99.428627	56.676621
2691.641592	103.286578	56.681626
2690.897707	97.286820	56.686631
2690.535700	96.191377	56.691636
2689.911214	97.668226	56.696641
2689.695303	89.765251	56.701645
2688.398168	97.171377	56.706650
2687.784545	88.213392	56.711655
2686.847569	98.979826	56.716660
2686.497921	93.148333	56.721665
2685.822156	95.950355	56.726669
2684.825158	93.652968	56.731674
2683.994896	94.067260	56.736679
2683.544530	94.244911	56.741684
2682.909533	88.764950	56.746689
2682.343880	97.031274	56.751693
2681.976830	96.613253	56.756698
2681.144263	96.476115	56.761703
2680.105760	94.203191	56.766708
2679.618643	101.805981	56.771713
2679.066473	92.745520	56.776717
2678.460469	103.331833	56.781722
2677.833209	92.492551	56.786727
2677.521555	89.579084	56.791732
2676.614857	93.550283	56.796737
2675.715279	88.201601	56.801741
2674.947599	88.118107	56.806746
2674.686066	90.044478	56.811751
2674.270757	89.793780	56.816756
2672.999395	83.659204	56.821761
2672.388784	84.514358	56.826765
2671.767352	92.503250	56.831770
2671.285652	88.843216	56.836775
2670.735175	94.318609	56.841780
2669.931825	95.816560	56.846785
2669.047429	87.176436	56.851789
2668.217286	86.538769	56.856794
2667.569891	89.844742	56.861799
2667.124734	86.249119	56.866804
2666.469620	101.256848	56.871809
2666.561986	93.541171	56.876813
2665.030106	92.983985	56.881818
2664.187988	85.325422	56.886823
2663.670563	86.093203	56.891828
2663.251072	86.040584	56.896833
2662.985149	82.290775	56.901837
2662.393329	89.988823	56.906842
2661.690010	86.887711	56.911847
2660.549762	86.333843	56.916852
2659.674401	98.196553	56.921857
2659.627058	91.380259	56.926861
2659.128669	96.152034	56.931866
2657.706164	90.196448	56.936871
2656.937540	92.463309	56.941876
2655.657135	90.289371	56.946881
2656.032869	94.590418	56.951885
2655.194954	90.536553	56.956890
2655.132891	91.888449	56.961895
2654.706689	86.105180	56.966900
2653.050910	92.385678	56.971905
2652.653775	90.832837	56.976909
2652.299613	92.422553	56.981914
2651.609580	86.310185	56.986919
2650.741565	87.591830	56.991924
2649.497836	86.946709	56.996929
2649.258475	83.119337	57.001933
2648.441705	97.772997	57.006938
2648.046837	89.874566	57.011943
2647.891318	89.666302	57.016948
2647.091042	87.462396	57.021953
2646.140664	96.730378	57.026957
2645.403133	92.905269	57.031962
2644.880027	94.231769	57.036967
2644.740440	94.424585	57.041972
2643.503769	94.520736	57.046977
2642.620016	92.565567	57.051981
2641.641404	100.769463	57.056986
2641.426907	99.745121	57.061991
2641.160839	89.274751	57.066996
2640.282946	96.655796	57.072001
2639.902485	88.566620	57.077005
2638.425841	87.020688	57.082010
2637.908291	90.193550	57.087015
2637.914015	88.941307	57.092020
2636.883630	89.343238	57.097025
2635.942943	82.052443	57.102029
2635.446178	93.553599	57.107034
2634.623493	89.308852	57.112039
2634.481828	82.749470	57.117044
2633.845797	92.405017	57.122049
2633.222436	90.991504	57.127053
2631.944420	101.683613	57.132058
2631.874764	87.090716	57.137063
2631.340051	88.184734	57.142068
2630.377880	95.775574	57.147073
2629.271205	87.690941	57.152077
2628.267737	92.550240	57.157082
2627.699737	86.574905	57.162087
2628.008885	87.041922	57.167092
2627.464829	102.146320	57.172097
2626.852929	89.573163	57.177101
2625.237838	95.493435	57.182106
2624.530899	93.532911	57.187111
2624.119360	95.045598	57.192116
2623.595791	104.147864	57.197121
2623.923156	92.113990	57.202125
2622.851197	96.964079	57.207130
2621.905738	96.520205	57.212135
2621.494915	92.732801	57.217140
2620.177799	99.417639	57.222145
2619.191749	93.228775	57.227149
2618.342669	95.610839	57.232154
2617.958257	91.136836	57.237159
2617.815499	92.752387	57.242164
2617.105484	98.743331	57.247169
2617.117570	96.136093	57.252173
2615.876854	97.915259	57.257178
2614.802085	94.743049	57.262183
2614.633297	98.269966	57.267188
2613.596444	97.773035	57.272193
2613.476964	93.044539	57.277197
2612.095366	94.667398	57.282202
2611.390777	85.644458	57.287207
2610.813822	90.552028	57.292212
2610.367702	99.174882	57.297217
2609.734745	86.420205	57.302221
2609.689191	94.623276	57.307226
2608.331477	92.918867	57.312231
2607.629130	91.892664	57.317236
2607.061908	91.654520	57.322241
2606.979372	93.342669	57.327245
2606.106865	90.359300	57.332250
2605.039148	94.780389	57.337255
2604.109561	99.176683	57.342260
2603.445432	102.165797	57.347265
2603.315114	93.558615	57.352269
2602.709407	86.504237	57.357274
2602.485429	88.211828	57.362279
2601.283885	92.030156	57.367284
2599.770592	100.807813	57.372289
2600.009186	93.897644	57.377293
2599.443835	98.006678	57.382298
2598.710722	89.871219	57.387303
2598.113563	95.879184	57.392308
2596.841184	91.231334	57.397313
2596.567828	89.949434	57.402317
2596.069259	99.135447	57.407322
2595.710259	90.504994	57.412327
2594.812425	87.309254	57.417332
2593.841542	94.401470	57.422337
2593.549223	88.392038	57.427341
2592.567787	91.013829	57.432346
2591.656531	95.180417	57.437351
2590.708367	94.517150	57.442356
2590.418608	89.346465	57.447361
2589.831420	79.473357	57.452365
2588.652525	88.406994	57.457370
2588.494851	90.074041	57.462375
2587.976029	85.142247	57.467380
2587.696725	100.688471	57.472385
2587.302257	84.250906	57.477389
2586.295831	97.169412	57.482394
2585.127938	93.364991	57.487399
2584.906007	95.251438	57.492404
2584.297727	93.806537	57.497409
2583.536831	88.541927	57.502413
2582.613082	87.171878	57.507418
2582.024607	88.220225	57.512423
2581.711440	89.295320	57.517428
2580.680062	91.005943	57.522433
2580.052168	82.749876	57.527437
2578.827173	90.796951	57.532442
2578.610408	89.414986	57.537447
2578.046419	79.696594	57.542452
2577.383400	93.810824	57.547457
2577.379945	90.867571	57.552461
2576.087421	84.300075	57.557466
2575.494033	88.272985	57.562471
2574.993417	87.809913	57.567476
2574.278482	94.670487	57.572481
2573.436088	87.382243	57.577485
2572.248010	94.785530	57.582490
2571.955080	86.989288	57.587495
2571.763424	90.296698	57.592500
2571.106051	95.400382	57.597505
2570.204010	84.782573	57.602509
2569.066815	86.428790	57.607514
2568.454588	85.356398	57.612519
2568.215744	87.558357	57.617524
2567.999229	96.698518	57.622529
2567.652207	86.242002	57.627533
2566.331497	87.881304	57.632538
2565.333428	85.703332	57.637543
2564.911265	72.641466	57.642548
2564.310912	80.559647	57.647553
2563.876815	93.055844	57.652557
2562.665625	92.846482	57.657562
2561.369591	92.882933	57.662567
2561.157820	88.676257	57.667572
2560.583893	94.581570	57.672577
2560.534169	89.139729	57.677581
2560.171108	93.097343	57.682586
2559.066435	87.788880	57.687591
2558.052564	90.280436	57.692596
2557.261509	96.271421	57.697601
2557.270904	84.093766	57.702605
2556.530830	92.271095	57.707610
2555.805882	91.990450	57.712615
2555.236142	82.640927	57.717620
2554.061652	95.938680	57.722625
2553.873232	92.419963	57.727629
2553.282490	83.067321	57.732634
2552.105854	87.776238	57.737639
2551.597263	83.734383	57.742644
2550.935667	85.919012	57.747649
2550.898602	83.714906	57.752653
2549.536232	83.843619	57.757658
2548.744748	85.665993	57.762663
2548.210493	84.302387	57.767668
2547.459958	93.439107	57.772673
2547.381366	85.616489	57.777677
2546.858182	90.059752	57.782682
2545.783793	90.955523	57.787687
2544.852875	83.180727	57.792692
2544.181967	86.515597	57.797697
2543.937448	77.871903	57.802701
2543.678590	89.167780	57.807706
2542.385745	85.215003	57.812711
2541.708225	80.392056	57.817716
2540.822283	86.518862	57.822721
2540.732562	77.048204	57.827725
2540.069672	79.138716	57.832730
2538.627387	89.703784	57.837735
2538.595792	79.702547	57.842740
2537.796046	86.152106	57.847745
2537.546917	77.197764	57.852749
2536.955833	85.817368	57.857754
2535.564346	91.071030	57.862759
2534.734586	80.327196	57.867764
2534.089170	93.489104	57.872769
2533.770021	77.434986	57.877773
2533.012337	88.556414	57.882778
2532.283214	87.427434	57.887783
2532.361187	81.939292	57.892788
2531.262205	82.866506	57.897793
2530.659842	77.747696	57.902797
2529.638560	90.232173	57.907802
2529.318824	76.542951	57.912807
2528.643572	81.345752	57.917812
2527.923575	91.259988	57.922817
2526.924855	73.480669	57.927821
2526.340438	83.576583	57.932826
2526.185892	80.744426	57.937831
2525.830789	76.963299	57.942836
2524.261796	86.418751	57.947841
2523.633833	80.335270	57.952845
2523.324419	84.474363	57.957850
2522.617439	94.509530	57.962855
2522.233552	81.735586	57.967860
2520.989692	87.577017	57.972865
2520.513946	86.671159	57.977869
2519.960981	87.467528	57.982874
2519.728827	89.367170	57.987879
2519.371531	87.629114	57.992884
2517.978092	95.382902	57.997889
2516.721466	92.677188	58.002893
2516.518352	98.162673	58.007898
2516.094740	89.085794	58.012903
2515.965046	81.088371	58.017908
2514.701429	92.080384	58.022913
2513.998024	87.326994	58.027917
2513.219201	85.125760	58.032922
2512.508492	85.763972	58.037927
2512.631244	79.157818	58.042932
2511.362238	90.228511	58.047937
2510.635913	80.761696	58.052941
2509.878161	80.106151	58.057946
2509.881717	83.269267	58.062951
2508.776874	79.793158	58.067956
2507.282148	92.386211	58.072961
2506.969755	81.429594	58.077965
2506.908382	80.506972	58.082970
2506.258281	83.206728	58.087975
2506.029476	73.724725	58.092980
2504.651610	81.412296	58.097985
2503.713352	78.565712	58.102989
2503.096980	79.378449	58.107994
2502.609127	80.321971	58.112999
2502.482495	79.065912	58.118004
2501.797304	87.377537	58.123009
2501.066057	80.877127	58.128013
2500.430361	79.967435	58.133018
2499.313429	84.822068	58.138023
2498.864301	85.722260	58.143028
2497.800191	88.335701	58.148033
2496.864491	81.176716	58.153037
2496.561778	82.209766	58.158042
2495.839654	79.127685	58.163047
2495.467976	77.002499	58.168052
2494.721782	88.477609	58.173057
2494.762875	78.930908	58.178061
2494.089364	79.816965	58.183066
2493.063284	81.514854	58.188071
2492.645550	91.701876	58.193076
2491.830987	90.037659	58.198081
2490.702935	79.830346	58.203085
2489.460365	74.931522	58.208090
2488.853463	82.409130	58.213095
2488.927271	82.882823	58.218100
2488.009288	86.938864	58.223105
2488.039175	84.628579	58.228109
2487.545816	76.598604	58.233114
2486.485920	74.220043	58.238119
2485.840345	80.069316	58.243124
2485.072029	89.398543	58.248129
2484.349409	83.561375	58.253133
2483.280638	83.778851	58.258138
2482.391557	91.980870	58.263143
2481.992087	78.263843	58.268148
2481.714862	83.739493	58.273153
2480.956288	82.877653	58.278157
2481.118193	89.007677	58.283162
2480.221719	85.048331	58.288167
2479.273050	75.101663	58.293172
2478.140145	79.827586	58.298177
2477.601682	75.070874	58.303181
2477.319909	84.850185	58.308186
2476.163915	85.610715	58.313191
2475.942563	84.373614	58.318196
2475.041185	88.691679	58.323201
2474.904268	87.785920	58.328205
2473.664096	81.519364	58.333210
2472.701749	84.554342	58.338215
2471.999244	75.910806	58.343220
2471.409800	86.243231	58.348225
2471.341301	81.198937	58.353229
2470.817514	85.893745	58.358234
2469.806411	86.355171	58.363239
2469.496327	79.301987	58.368244
2468.549770	86.691621	58.373249
2467.972847	76.932441	58.378253
2467.033525	76.618989	58.383258
2465.821288	83.952602	58.388263
2465.600251	82.743474	58.393268
2465.188921	87.861146	58.398273
2464.776478	82.002133	58.403277
2464.722914	85.829072	58.408282
2463.137011	90.485614	58.413287
2462.699545	77.903603	58.418292
2461.959006	81.812865	58.423297
2461.186339	72.550956	58.428301
2460.353541	85.892914	58.433306
2459.913902	85.541396	58.438311
2459.417208	72.286251	58.443316
2458.685562	80.921201	58.448321
2457.593049	77.228661	58.453325
2457.017966	79.018389	58.458330
2456.027247	77.276537	58.463335
2455.892699	69.716916	58.468340
2454.985702	77.982385	58.473345
2454.839008	72.917913	58.478349
2454.506345	80.631650	58.483354
2453.203348	83.716189	58.488359
2452.715849	83.340093	58.493364
2451.439935	82.259615	58.498369
2451.761779	82.703530	58.503373
2451.288039	90.869668	58.508378
2449.853640	85.781025	58.513383
2449.293928	77.465173	58.518388
2448.525495	84.592651	58.523393
2448.038275	71.962315	58.528397
2447.092247	80.982460	58.533402
2445.927252	79.585397	58.538407
2446.055676	74.064164	58.543412
2445.079283	89.012332	58.548417
2444.653581	80.421734	58.553421
2444.139550	80.020966	58.558426
2443.636906	86.232635	58.563431
2442.730628	70.607737	58.568436
2441.885165	84.429869	58.573441
2441.578590	74.400664	58.578445
2441.167014	84.514392	58.583450
2440.123180	79.613179	58.588455
2439.419556	75.281803	58.593460
2438.377347	88.873113	58.598465
2437.971442	77.580801	58.603469
2437.703731	84.805424	58.608474
2436.665961	85.192865	58.613479
2435.814884	84.186195	58.618484
2435.192423	81.081163	58.623489
2434.754589	81.977455	58.628493
2434.390584	83.016251	58.633498
2434.077162	82.892621	58.638503
2433.147982	72.170555	58.643508
2431.654654	84.017346	58.648513
2430.804896	71.469131	58.653517
2430.657531	77.513082	58.658522
2429.997539	74.975766	58.663527
2430.150503	77.704399	58.668532
2428.988977	80.784096	58.673537
2428.468661	81.854354	58.678541
2427.782256	72.925061	58.683546
2426.845927	77.787901	58.688551
2425.884208	75.844131	58.693556
2425.186243	82.981665	58.698561
2425.128435	77.834104	58.703565
2424.606157	81.731708	58.708570
2423.561926	89.741580	58.713575
2422.771529	77.065586	58.718580
2422.185110	82.229378	58.723585
2421.553077	77.626036	58.728589
2421.199089	78.943373	58.733594
2419.881703	81.773019	58.738599
2418.976619	75.061570	58.743604
2418.335004	76.389797	58.748609
2418.192322	77.787448	58.753613
2417.497513	80.024741	58.758618
2416.921945	79.808175	58.763623
2416.583265	69.144226	58.768628
2416.092988	82.045128	58.773633
2415.101013	61.265209	58.778637
2414.537825	71.517742	58.783642
2413.989590	72.100950	58.788647
2413.054989	76.395489	58.793652
2412.520949	73.653883	58.798657
2411.690354	70.342084	58.803661
2411.216404	74.753643	58.808666
2409.999237	83.758576	58.813671
2409.240547	82.041400	58.818676
2408.258966	78.837519	58.823681
2408.347491	79.524608	58.828685
2407.831478	80.488741	58.833690
2406.946343	87.945640	58.838695
2406.873190	76.357237	58.843700
2406.126366	80.537174	58.848705
2404.920462	74.797658	58.853709
2404.449092	76.461503	58.858714
2404.145785	80.886516	58.863719
2403.133414	69.842776	58.868724
2402.131953	66.621772	58.873729
2401.247104	75.633036	58.878733
2401.086966	75.746479	58.883738
2400.710256	78.115692	58.888743
2400.002005	83.937006	58.893748
2398.393205	80.114080	58.898753
2398.015672	82.927499	58.903757
2397.424923	77.725806	58.908762
2396.988673	80.735574	58.913767
2396.759819	74.287833	58.918772
2396.188537	84.063354	58.923777
2395.683999	83.758464	58.928781
2394.634870	76.057605	58.933786
2393.370435	80.727086	58.938791
2393.210445	75.432400	58.943796
2392.738737	80.411979	58.948801
2391.870259	77.178499	58.953805
2391.081206	75.161793	58.958810
2390.597633	82.383455	58.963815
2390.583187	74.843169	58.968820
2389.343892	83.331249	58.973825
2388.307181	83.320637	58.978829
2388.160039	81.772441	58.983834
2387.202035	86.502025	58.988839
2386.681570	77.746069	58.993844
2385.527913	86.015040	58.998849
2384.659043	85.049709	59.003853
2384.321853	83.250203	59.008858
2383.826564	79.526217	59.013863
2383.880467	80.725261	59.018868
2383.054542	84.643210	59.023873
2381.830934	86.312527	59.028877
2381.175406	79.049615	59.033882
2380.158184	83.493282	59.038887
2380.193302	78.586799	59.043892
2379.869163	84.450195	59.048897
2378.327645	86.042034	59.053901
2377.806403	80.447551	59.058906
2377.105067	81.923358	59.063911
2377.098002	77.806430	59.068916
2376.353461	85.030876	59.073921
2374.998722	80.662428	59.078925
2374.641285	73.219081	59.083930
2374.029083	82.782131	59.088935
2373.752783	76.541051	59.093940
2372.776762	82.066322	59.098945
2371.763582	78.829958	59.103949
2371.148300	84.148288	59.108954
2370.564465	96.344432	59.113959
2370.311944	77.124330	59.118964
2369.793494	85.507708	59.123969
2368.631960	82.336972	59.128973
2367.986611	77.569738	59.133978
2367.042834	80.529320	59.138983
2366.664686	80.148745	59.143988
2366.241728	78.375748	59.148993
2365.523748	80.957259	59.153997
2364.618668	79.335383	59.159002
2363.690318	80.039642	59.164007
2363.750721	72.353540	59.169012
2363.208737	80.397924	59.174017
2362.194488	76.262566	59.179021
2361.716437	69.873232	59.184026
2360.698883	73.516063	59.189031
2360.534919	74.609469	59.194036
2359.490280	83.116371	59.199041
2358.017324	77.130437	59.204045
2357.958648	80.631019	59.209050
2357.749212	81.342215	59.214055
2357.694775	69.822068	59.219060
2356.166497	73.041854	59.224065
2355.292688	70.024813	59.229069
2354.726788	71.020375	59.234074
2353.993477	83.265357	59.239079
2354.145277	74.847992	59.244084
2352.976126	78.656875	59.249089
2351.970815	70.634733	59.254093
2351.712901	70.333859	59.259098
2351.088475	72.567806	59.264103
2350.160343	74.662639	59.269108
2349.293308	78.947213	59.274113
2348.371222	75.140298	59.279117
2347.903492	75.070294	59.284122
2347.584291	81.320462	59.289127
2347.297683	74.532878	59.294132
2346.865383	82.112866	59.299137
2345.625056	85.613802	59.304141
2344.804273	79.882261	59.309146
2344.013379	75.593850	59.314151
2343.809575	77.367072	59.319156
2343.369246	84.470425	59.324161
2342.419870	75.329151	59.329165
2341.899641	72.567431	59.334170
2340.807368	91.098187	59.339175
2340.256716	77.816767	59.344180
2339.098597	78.342827	59.349185
2338.144884	82.781562	59.354189
2338.373030	77.591425	59.359194
2337.635567	83.079459	59.364199
2337.444855	83.521805	59.369204
2337.134995	75.808230	59.374209
2336.082156	81.032440	59.379213
2334.918282	77.500549	59.384218
2334.210413	82.621562	59.389223
2333.806467	80.868605	59.394228
2332.571331	71.115829	59.399233
2331.819666	80.635624	59.404237
2331.608924	77.691118	59.409242
2331.036435	84.557737	59.414247
2330.587905	73.628777	59.419252
2330.301143	76.036690	59.424257
2329.049921	77.875732	59.429261
2328.515684	80.170837	59.434266
2327.624061	86.166796	59.439271
2327.612718	70.040365	59.444276
2326.828460	76.734779	59.449281
2325.507805	82.740945	59.454285
2324.941647	73.229422	59.459290
2324.027797	85.673430	59.464295
2324.040258	71.767587	59.469300
2323.428819	74.739421	59.474305
2322.457459	71.804987	59.479309
2321.261290	69.798700	59.484314
2320.813869	71.663710	59.489319
2320.443989	72.683385	59.494324
2319.840134	73.752148	59.499329
2319.427250	76.827394	59.504333
2319.243785	73.942171	59.509338
2317.741916	73.625470	59.514343
2317.120950	63.972542	59.519348
2317.274216	71.620940	59.524353
2316.016804	72.261481	59.529357
2315.064381	74.758354	59.534362
2314.242235	75.021712	59.539367
2313.794062	73.671439	59.544372
2313.250158	73.968136	59.549377
2312.659052	79.439038	59.554381
2311.993796	71.380072	59.559386
2311.076472	78.150924	59.564391
2310.752477	67.750527	59.569396
2310.153039	68.986687	59.574401
2309.014788	73.102913	59.579405
2308.326019	72.302185	59.584410
2307.468259	76.608465	59.589415
2307.011907	69.020208	59.594420
2306.781979	73.773712	59.599425
2306.530251	77.494798	59.604429
2306.127166	74.201094	59.609434
2304.661474	75.353290	59.614439
2304.626194	83.494970	59.619444
2303.558569	76.193601	59.624449
2302.130395	76.652958	59.629453
2301.604440	67.972960	59.634458
2301.193862	81.400602	59.639463
2300.662846	76.013455	59.644468
2300.459735	75.833471	59.649473
2299.595878	78.562298	59.654477
2298.917910	73.613556	59.659482
2297.610720	81.407097	59.664487
2297.611184	72.539976	59.669492
2297.272520	80.993656	59.674497
2295.913454	70.407510	59.679501
2295.502404	67.375293	59.684506
2294.885310	76.457220	59.689511
2294.126015	79.755516	59.694516
2293.195177	79.071577	59.699521
2292.152356	76.942366	59.704525
2291.752832	78.033031	59.709530
2291.071185	86.485762	59.714535
2291.093043	73.911690	59.719540
2290.739656	73.548201	59.724545
2289.577459	79.896736	59.729549
2288.816323	76.285329	59.734554
2287.887717	82.475503	59.739559
2287.562652	77.244579	59.744564
2286.984703	81.633667	59.749569
2286.060003	84.919593	59.754573
2285.293815	72.602647	59.759578
2284.788393	76.593687	59.764583
2284.368750	72.750205	59.769588
2284.155143	67.738243	59.774593
2282.918502	80.462834	59.779597
2282.691117	71.350477	59.784602
2281.855446	79.910463	59.789607
2281.175504	73.345277	59.794612
2280.017813	84.145123	59.799617
2278.947183	68.874033	59.804621
2278.754982	69.146904	59.809626
2278.288944	80.069251	59.814631
2277.869467	73.806880	59.819636
2277.125878	71.738209	59.824641
2276.262339	75.037753	59.829645
2275.262464	71.557172	59.834650
2274.856925	72.568737	59.839655
2274.774282	66.037198	59.844660
2273.528114	72.203520	59.849665
2272.316013	78.176921	59.854669
2272.310560	69.922240	59.859674
2271.180568	77.435623	59.864679
2270.949946	72.845370	59.869684
2270.979003	77.661951	59.874689
2269.496480	82.585848	59.879693
2269.062199	74.537915	59.884698
2268.129600	78.895681	59.889703
2267.666046	77.741062	59.894708
2267.329348	70.322210	59.899713
2266.396693	74.290393	59.904718
2265.749486	69.702306	59.909722
2264.995580	84.390196	59.914727
2264.236272	72.319177	59.919732
2264.169639	81.512624	59.924737
2262.690365	72.351075	59.929742
2262.165622	64.352170	59.934746
2261.479085	74.048712	59.939751
2261.061839	71.922657	59.944756
2260.818674	70.381415	59.949761
2259.712548	78.244390	59.954766
2259.018066	73.720042	59.959770
2257.973843	73.674425	59.964775
2257.977820	66.864794	59.969780
2257.569748	69.743436	59.974785
2256.164812	73.463581	59.979790
2255.805920	72.701182	59.984794
2254.981702	67.327476	59.989799
2254.657316	74.207320	59.994804
2254.429661	65.638945	59.999809
2253.438565	77.653675	60.004814
2252.765255	71.249197	60.009818
2252.010700	73.537774	60.014823
2251.040217	67.961327	60.019828
2250.069235	76.526296	60.024833
2249.253174	81.940544	60.029838
2249.192491	70.369771	60.034842
2248.124829	80.136232	60.039847
2248.325768	76.197679	60.044852
2247.492409	69.235989	60.049857
2246.729992	77.063474	60.054862
2246.223489	73.603917	60.059866
2245.190680	71.615105	60.064871
2244.459098	62.167420	60.069876
2243.671727	68.336598	60.074881
2242.801133	79.473780	60.079886
2242.685669	71.531194	60.084890
2242.533981	81.501394	60.089895
2241.266578	78.566683	60.094900
2240.083348	72.402564	60.099905
2239.138697	76.913178	60.104910
2239.496633	73.291580	60.109914
2239.046553	82.394685	60.114919
2238.271566	82.319212	60.119924
2237.918468	77.125060	60.124929
2236.767800	79.626639	60.129934
2236.110056	72.590314	60.134938
2235.399312	80.025689	60.139943
2234.358529	71.154676	60.144948
2233.800667	70.161446	60.149953
2232.919468	68.978390	60.154958
2232.605001	73.532806	60.159962
2232.227513	76.042286	60.164967
2231.736999	66.819023	60.169972
2230.858509	69.489178	60.174977
2229.861418	75.530021	60.179982
2229.386808	71.973831	60.184986
2228.921519	75.699072	60.189991
2227.991262	72.995251	60.194996
2227.058048	71.130326	60.200001
2226.034670	75.601118	60.205006
2226.198357	65.726786	60.210010
2225.921253	72.058957	60.215015
2225.296295	75.721113	60.220020
2224.260432	67.910672	60.225025
2223.613216	77.579573	60.230030
2223.438004	67.276111	60.235034
2221.888588	74.313747	60.240039
2220.936883	74.731508	60.245044
2220.104634	63.677155	60.250049
2219.389715	79.718191	60.255054
2219.412674	70.981831	60.260058
2218.610577	73.271437	60.265063
2218.292136	67.020613	60.270068
2218.367164	66.621756	60.275073
2216.781092	76.811205	60.280078
2216.428662	74.801564	60.285082
2215.578214	73.274580	60.290087
2214.700700	77.658851	60.295092
2213.615193	68.710234	60.300097
2212.610330	79.528550	60.305102
2213.070235	81.764563	60.310106
2212.308202	81.434651	60.315111
2211.796315	79.462148	60.320116
2211.532061	79.733134	60.325121
2210.032591	81.201383	60.330126
2209.667182	79.987749	60.335130
2208.758500	80.486967	60.340135
2208.558673	71.345040	60.345140
2207.698722	69.516141	60.350145
2206.327397	79.773469	60.355150
2205.874987	76.635048	60.360154
2205.876523	81.792637	60.365159
2205.357701	71.140980	60.370164
2204.705176	73.224225	60.375169
2203.728534	73.536521	60.380174
2203.583209	72.857992	60.385178
2202.545082	76.845406	60.390183
2201.158602	74.373161	60.395188
2200.849474	71.566277	60.400193
2200.376161	79.286298	60.405198
2199.997870	84.162280	60.410202
2198.808805	73.611433	60.415207
2197.703347	73.385649	60.420212
2197.231906	64.257813	60.425217
2196.570289	69.781828	60.430222
2196.347811	69.366353	60.435226
2195.964601	77.248589	60.440231
2195.612541	75.547165	60.445236
2194.583615	64.930650	60.450241
2193.780476	73.659146	60.455246
2193.168581	61.821487	60.460250
2192.330596	66.292546	60.465255
2191.633676	67.132905	60.470260
2190.935591	67.310724	60.475265
2190.043710	68.185216	60.480270
2189.951478	76.969757	60.485274
2189.283485	71.847230	60.490279
2188.576502	74.497139	60.495284
2187.741737	69.336427	60.500289
2186.959794	72.417166	60.505294
2186.683684	66.387652	60.510298
2185.847356	71.956547	60.515303
2184.847855	66.036540	60.520308
2184.117668	72.094895	60.525313
2183.236552	75.430219	60.530318
2183.281546	69.533675	60.535322
2182.730563	79.742678	60.540327
2182.501247	71.474582	60.545332
2181.580578	70.717875	60.550337
2180.536732	83.146619	60.555342
2179.962623	70.617255	60.560346
2179.135175	72.501875	60.565351
2178.006796	66.977318	60.570356
2177.455493	70.643458	60.575361
2176.882565	74.980377	60.580366
2176.722048	66.957088	60.585370
2176.422332	74.102701	60.590375
2175.541515	69.744049	60.595380
2174.831245	65.861475	60.600385
2173.982873	75.006246	60.605390
2173.376625	62.086481	60.610394
2172.197997	81.444727	60.615399
2170.943489	72.650546	60.620404
2171.151980	69.952894	60.625409
2170.619406	71.369862	60.630414
2170.491951	71.289834	60.635418
2169.841793	69.157440	60.640423
2168.834976	77.206327	60.645428
2168.137088	74.619086	60.650433
2167.384122	78.899170	60.655438
2166.812838	68.553722	60.660442
2165.709547	75.051272	60.665447
2164.848306	69.961011	60.670452
2164.371908	69.440944	60.675457
2163.752040	73.476825	60.680462
2163.423280	67.279087	60.685466
2162.763504	72.948048	60.690471
2162.207983	81.288423	60.695476
2161.322296	75.899591	60.700481
2160.186591	80.339079	60.705486
2160.239879	75.239244	60.710490
2159.327099	78.659721	60.715495
2158.611225	79.956072	60.720500
2157.874572	71.245427	60.725505
2156.965033	73.336714	60.730510
2157.159326	75.029617	60.735514
2156.305181	73.751160	60.740519
2155.419300	70.238479	60.745524
2154.848686	70.439894	60.750529
2153.608169	71.175079	60.755534
2153.491860	62.168481	60.760538
2153.423416	75.699034	60.765543
2152.155188	69.648948	60.770548
2151.411359	69.660918	60.775553
2150.668899	71.412984	60.780558
2150.374191	67.872219	60.785562
2149.597022	74.487672	60.790567
2148.822337	73.291939	60.795572
2148.270222	66.484270	60.800577
2147.582953	80.743536	60.805582
2146.933790	62.553681	60.810586
2145.692168	75.739772	60.815591
2144.754544	71.202165	60.820596
2144.599271	69.861811	60.825601
2143.732037	73.023456	60.830606
2143.887059	70.825194	60.835610
2143.460318	68.243292	60.840615
2142.571439	68.390594	60.845620
2142.042161	71.578908	60.850625
2141.160179	72.875250	60.855630
2139.980689	63.450909	60.860634
2138.764745	71.266363	60.865639
2138.017063	67.796757	60.870644
2137.977425	65.969275	60.875649
2137.571991	70.669508	60.880654
2137.257743	65.728850	60.885658
2136.764652	70.916162	60.890663
2135.880014	72.140331	60.895668
2134.962681	72.669066	60.900673
2134.148641	68.230715	60.905678
2133.950295	62.801701	60.910682
2132.956752	75.983651	60.915687
2131.787674	73.306486	60.920692
2131.465474	61.306798	60.925697
2131.368158	75.404370	60.930702
2130.649419	65.318222	60.935706
2129.363980	71.963766	60.940711
2128.811112	71.974262	60.945716
2128.219614	70.556551	60.950721
2127.821497	73.842823	60.955726
2127.306830	65.813799	60.960730
2126.188701	73.587264	60.965735
2125.068333	69.206044	60.970740
2124.871599	66.616383	60.975745
2124.361153	70.193041	60.980750
2124.001222	68.464945	60.985754
2123.810150	66.048782	60.990759
2122.569960	62.949984	60.995764
2121.851383	64.420874	61.000769
2121.101929	79.212201	61.005774
2120.234785	67.654650	61.010778
2119.468776	65.974299	61.015783
2118.727612	75.674663	61.020788
2118.417165	69.884308	61.025793
2117.642632	75.943939	61.030798
2117.508909	68.320664	61.035802
2116.974227	72.186062	61.040807
2115.345871	77.147960	61.045812
2115.238983	73.511128	61.050817
2114.374743	76.797392	61.055822
2114.253645	63.983733	61.060826
2112.940208	68.088113	61.065831
2112.100186	65.645977	61.070836
2111.832855	68.358059	61.075841
2111.340594	72.305409	61.080846
2110.847933	65.114172	61.085850
2109.646971	70.037309	61.090855
2108.877819	73.426910	61.095860
2108.529197	70.974540	61.100865
2108.177527	71.684018	61.105870
2107.109935	65.199383	61.110874
2106.656913	66.671826	61.115879
2105.548976	71.986801	61.120884
2105.371431	65.632950	61.125889
2104.861779	69.624326	61.130894
2103.862128	68.308795	61.135898
2102.851874	62.973258	61.140903
2102.146685	64.767899	61.145908
2101.972117	53.988714	61.150913
2101.500452	71.897398	61.155918
2100.762852	63.665730	61.160922
2100.028303	60.130731	61.165927
2098.373705	64.484509	61.170932
2098.755740	59.031623	61.175937
2097.998941	72.207420	61.180942
2098.201045	67.157924	61.185946
2097.226558	70.868819	61.190951
2096.114975	73.529521	61.195956
2094.834423	62.753585	61.200961
2093.772137	72.325721	61.205966
2093.450728	70.893396	61.210970
2093.651715	70.040378	61.215975
2092.385992	68.904169	61.220980
2092.267115	64.333506	61.225985
2091.813555	68.211476	61.230990
2090.752911	68.354219	61.235994
2089.972048	77.533238	61.240999
2089.326539	75.336509	61.246004
2089.179524	67.144348	61.251009
2087.679329	76.360352	61.256014
2087.188123	70.785254	61.261018
2086.348972	63.551447	61.266023
2085.848517	74.991230	61.271028
2085.600622	63.136334	61.276033
2085.313272	70.312985	61.281038
2084.372803	68.596561	61.286042
2083.549686	68.682100	61.291047
2082.426437	73.909702	61.296052
2082.394660	74.610649	61.301057
2080.815839	75.043333	61.306062
2080.166809	67.942396	61.311066
2079.513877	74.775805	61.316071
2079.042268	75.670004	61.321076
2078.679195	66.764039	61.326081
2078.347297	73.000979	61.331086
2078.073336	69.142473	61.336090
2077.592328	74.237725	61.341095
2076.147097	76.056718	61.346100
2075.968385	73.618312	61.351105
2074.303839	80.968558	61.356110
2073.839230	69.818991	61.361114
2073.212306	67.738293	61.366119
2072.328632	70.300808	61.371124
2072.629898	63.206272	61.376129
2071.815247	70.713500	61.381134
2071.465757	70.813947	61.386138
2070.243501	65.608228	61.391143
2069.518337	75.333487	61.396148
2069.536065	59.840406	61.401153
2067.727865	68.490169	61.406158
2066.939287	63.579338	61.411162
2066.566301	66.974203	61.416167
2065.787551	70.023621	61.421172
2065.707641	54.148577	61.426177
2065.437069	66.649120	61.431182
2064.700537	65.356879	61.436186
2063.594651	62.672081	61.441191
2062.891056	72.560617	61.446196
2062.804196	62.196676	61.451201
2061.490130	69.982347	61.456206
2060.803382	61.809488	61.461210
2060.220345	65.309358	61.466215
2059.369031	66.804933	61.471220
2059.616279	66.275173	61.476225
2058.217169	58.929136	61.481230
2057.808150	64.619154	61.486234
2057.024858	70.392139	61.491239
2056.536598	65.900843	61.496244
2055.758080	60.480683	61.501249
2054.691895	66.813614	61.506254
2054.146930	58.502038	61.511258
2054.211564	66.948691	61.516263
2053.355747	59.838530	61.521268
2052.463473	56.941547	61.526273
2051.506583	68.203616	61.531278
2051.160317	59.832395	61.536282
2050.346111	61.378858	61.541287
2049.311210	67.255273	61.546292
2048.861232	63.189256	61.551297
2047.506318	62.787892	61.556302
2047.519773	64.782894	61.561306
2047.372362	54.406423	61.566311
2046.430118	66.113995	61.571316
2046.228834	58.636888	61.576321
2045.380838	73.181390	61.581326
2044.359844	75.928050	61.586330
2043.838016	69.539544	61.591335
2043.740678	72.068609	61.596340
2042.681863	73.329690	61.601345
2041.310664	68.108799	61.606350
2040.864081	71.724668	61.611354
2040.863964	64.072234	61.616359
2039.787452	65.607910	61.621364
2039.076569	66.991049	61.626369
2038.076208	72.948793	61.631374
2037.432902	74.001043	61.636378
2037.333131	65.886857	61.641383
2036.818293	74.043042	61.646388
2036.368277	67.570415	61.651393
2035.312522	74.302210	61.656398
2034.642294	64.731978	61.661402
2034.024352	60.335893	61.666407
2032.937638	79.655522	61.671412
2032.080204	69.795216	61.676417
2031.558827	66.420336	61.681422
2031.010383	73.038118	61.686426
2030.861491	68.813631	61.691431
2030.394290	70.339030	61.696436
2029.439723	62.376982	61.701441
2028.607078	64.384084	61.706446
2027.421667	70.589394	61.711450
2027.455315	66.444206	61.716455
2027.023398	69.188390	61.721460
2026.526413	66.940609	61.726465
2025.549967	65.350346	61.731470
2024.373224	65.578091	61.736474
2023.525684	61.438378	61.741479
2022.489967	72.255269	61.746484
2022.150367	71.195914	61.751489
2021.681819	59.733631	61.756494
2021.608586	72.402911	61.761498
2021.254967	69.508132	61.766503
2020.496013	73.538210	61.771508
2019.585758	70.910743	61.776513
2018.572796	71.902285	61.781518
2018.061171	68.142068	61.786522
2018.067090	63.815711	61.791527
2016.417691	74.659423	61.796532
2015.815741	59.809961	61.801537
2015.054373	65.586697	61.806542
2015.063782	64.963019	61.811546
2014.601936	67.989811	61.816551
2013.250223	68.375378	61.821556
2012.532375	66.616545	61.826561
2011.823944	60.067344	61.831566
2011.244104	64.538868	61.836570
2010.919781	62.553254	61.841575
2009.484769	61.808379	61.846580
2009.215430	62.761533	61.851585
2008.148407	69.223293	61.856590
2007.835243	65.317819	61.861594
2007.595497	59.738800	61.866599
2006.827964	66.404714	61.871604
2006.615431	62.838461	61.876609
2005.452848	63.086286	61.881614
2004.408165	61.401125	61.886618
2004.687355	65.972408	61.891623
2003.634156	69.583891	61.896628
2002.757182	68.236738	61.901633
2001.931558	71.609169	61.906638
2000.683687	66.544030	61.911642
2001.081461	64.235167	61.916647
2000.311743	69.230997	61.921652
2000.223423	57.319615	61.926657
1998.932405	64.932410	61.931662
1998.334145	63.687576	61.936666
1997.929103	60.873830	61.941671
1997.067874	62.271640	61.946676
1995.998631	54.385667	61.951681
1995.572012	58.928872	61.956686
1994.887555	62.712137	61.961690
1994.501295	61.251835	61.966695
1993.435277	67.369228	61.971700
1992.956453	62.840014	61.976705
1992.671979	68.054800	61.981710
1991.896140	65.048703	61.986714
1991.038853	63.106498	61.991719
1990.225159	68.236162	61.996724
1989.918822	64.477937	62.001729
1989.062419	65.987418	62.006734
1988.012804	69.644472	62.011738
1987.107748	63.184565	62.016743
1986.486542	70.287275	62.021748
1986.483333	60.115476	62.026753
1985.821195	61.225030	62.031758
1985.372811	61.694885	62.036762
1984.216383	58.079712	62.041767
1983.274948	67.173306	62.046772
1982.832118	69.359644	62.051777
1982.122825	65.744163	62.056782
1981.649670	65.705908	62.061786
1981.672085	60.432558	62.066791
1980.747168	67.271444	62.071796
1979.875038	69.758184	62.076801
1979.379098	68.543610	62.081806
1978.170125	72.214112	62.086810
1977.746469	65.527783	62.091815
1976.682574	67.113811	62.096820
1976.406741	68.341224	62.101825
1975.657657	71.939766	62.106830
1975.109578	66.752953	62.111834
1974.143066	66.951456	62.116839
1973.282744	66.086968	62.121844
1973.342715	61.554796	62.126849
1972.891439	65.887098	62.131854
1972.197841	67.775295	62.136858
1970.933500	62.624171	62.141863
1969.664110	68.695834	62.146868
1969.405048	53.759315	62.151873
1969.133579	64.178638	62.156878
1968.795653	63.724899	62.161882
1968.468950	62.217703	62.166887
1967.105500	62.591078	62.171892
1966.493530	59.279466	62.176897
1965.730106	62.967694	62.181902
1965.825895	65.531217	62.186906
1964.514102	55.429335	62.191911
1963.599189	60.189881	62.196916
1962.840911	59.175707	62.201921
1962.782689	64.514413	62.206926
1962.297049	73.265974	62.211930
1961.377193	63.106119	62.216935
1960.261517	65.568604	62.221940
1960.035038	62.245125	62.226945
1959.655423	61.025260	62.231950
1958.233347	60.946054	62.236954
1957.414332	62.612558	62.241959
1957.046735	68.289177	62.246964
1956.790448	70.627150	62.251969
1956.064188	61.377959	62.256974
1955.665894	64.832418	62.261978
1954.856627	61.703762	62.266983
1953.776939	72.681728	62.271988
1953.233780	63.293849	62.276993
1952.892770	72.414995	62.281998
1951.729025	72.902626	62.287002
1951.217235	72.906113	62.292007
1950.078983	72.428239	62.297012
1949.998466	63.547378	62.302017
1949.695391	68.790214	62.307022
1948.713616	55.397932	62.312026
1947.650547	48.534036	62.317031
1946.966215	60.405505	62.322036
1947.110938	62.884475	62.327041
1946.370873	65.783609	62.332046
1945.564130	70.549340	62.337050
1944.407553	54.336287	62.342055
1943.543395	58.680012	62.347060
1943.408803	60.984535	62.352065
1942.975149	66.004981	62.357070
1942.502313	67.007554	62.362074
1941.922571	51.334486	62.367079
1941.169918	63.138306	62.372084
1940.660208	49.107141	62.377089
1939.250249	57.761431	62.382094
1938.347166	56.198109	62.387098
1938.138667	53.436797	62.392103
1937.657625	57.258686	62.397108
1936.709532	49.431741	62.402113
1935.810071	55.916549	62.407118
1935.066686	57.762741	62.412122
1934.814744	55.182539	62.417127
1934.166833	61.398931	62.422132
1933.744926	60.308666	62.427137
1932.726442	59.600710	62.432142
1931.995716	63.249796	62.437146
1931.634184	49.449458	62.442151
1930.976605	64.583851	62.447156
1930.472578	58.416130	62.452161
1929.275502	61.129773	62.457166
1928.695406	57.388390	62.462170
1928.584883	54.566899	62.467175
1927.585223	65.365388	62.472180
1926.647484	61.678476	62.477185
1925.859408	63.542973	62.482190
1925.183847	67.586423	62.487194
1924.787903	59.322796	62.492199
1924.398449	68.505513	62.497204
1923.939016	58.337167	62.502209
1922.823788	55.196126	62.507214
1922.412519	59.960909	62.512218
1921.487551	52.018700	62.517223
1921.154577	59.976010	62.522228
1920.638044	56.607817	62.527233
1919.573394	57.562036	62.532238
1918.607643	56.877823	62.537242
1918.648234	52.142138	62.542247
1917.953446	61.966008	62.547252
1916.885500	57.009059	62.552257
1916.187057	57.567880	62.557262
1915.754543	59.578384	62.562266
1915.294915	52.410350	62.567271
1913.936564	61.424487	62.572276
1913.119171	58.255785	62.577281
1912.872981	60.441247	62.582286
1912.052553	66.166519	62.587290
1912.104063	60.992007	62.592295
1911.172581	61.862265	62.597300
1910.447813	56.772795	62.602305
1909.994478	56.437878	62.607310
1909.234489	60.933517	62.612314
1908.451801	53.045914	62.617319
1907.070308	48.556672	62.622324
1906.433245	56.855332	62.627329
1906.194571	59.318971	62.632334
1905.418452	61.003406	62.637338
1905.123493	60.126679	62.642343
1904.554607	59.505228	62.647348
1904.197705	53.906398	62.652353
1903.378964	57.457258	62.657358
1902.297566	71.066333	62.662362
1902.207734	63.464389	62.667367
1901.289861	59.004774	62.672372
1900.381784	58.244385	62.677377
1899.394357	56.481560	62.682382
1898.673451	63.008852	62.687386
1898.758668	49.245771	62.692391
1898.120570	61.582997	62.697396
1897.485809	49.603679	62.702401
1896.546468	53.428187	62.707406
1895.414193	59.447982	62.712410
1895.131885	47.521259	62.717415
1894.745827	59.256440	62.722420
1893.911567	55.226584	62.727425
1892.954195	50.060076	62.732430
1892.081190	58.697117	62.737434
1892.107497	55.444472	62.742439
1891.546696	61.893059	62.747444
1890.818600	58.077532	62.752449
1890.062972	53.411750	62.757454
1889.742181	59.098516	62.762458
1888.667592	51.179150	62.767463
1887.346541	57.947264	62.772468
1886.739348	53.296351	62.777473
1886.718125	51.247447	62.782478
1886.011051	59.145999	62.787482
1885.744953	51.894336	62.792487
1884.464473	60.426227	62.797492
1883.998648	47.954216	62.802497
1883.757250	54.993919	62.807502
1882.425131	53.174810	62.812506
1881.558376	50.475199	62.817511
1880.906059	57.575731	62.822516
1880.533240	59.491949	62.827521
1880.061093	52.326457	62.832526
1879.523363	65.629368	62.837530
1879.301266	60.022081	62.842535
1878.174841	64.215297	62.847540
1877.193954	65.182035	62.852545
1876.777706	65.503513	62.857550
1876.040216	63.060459	62.862554
1874.871075	55.370814	62.867559
1873.971347	59.794840	62.872564
1873.868020	59.876475	62.877569
1873.356167	59.326976	62.882574
1873.050341	66.738087	62.887578
1872.516321	56.972102	62.892583
1871.547988	64.856935	62.897588
1870.934552	59.870789	62.902593
1869.982208	54.385280	62.907598
1869.504976	67.022211	62.912602
1868.408197	52.440208	62.917607
1867.267625	54.862366	62.922612
1866.887346	58.494921	62.927617
1866.647222	64.203018	62.932622
1866.135439	59.613148	62.937626
1866.341732	49.301716	62.942631
1865.254080	56.200027	62.947636
1864.574889	57.090679	62.952641
1863.803007	58.037451	62.957646
1862.635344	60.605949	62.962650
1861.953608	55.981608	62.967655
1861.405988	60.395919	62.972660
1860.832050	57.433855	62.977665
1860.690654	56.380866	62.982670
1859.527710	56.845881	62.987674
1858.967629	55.067582	62.992679
1857.950148	64.864956	62.997684
1857.690142	58.477480	63.002689
1857.063043	60.507463	63.007694
1855.781638	61.511014	63.012698
1855.101108	53.641470	63.017703
1854.565366	55.139134	63.022708
1854.073834	62.718982	63.027713
1854.182531	54.940983	63.032718
1853.046202	58.914063	63.037722
1852.469424	59.324188	63.042727
1851.955892	67.555934	63.047732
1850.780113	64.246460	63.052737
1850.323810	56.329475	63.057742
1849.188308	61.351188	63.062746
1848.709196	55.229743	63.067751
1848.627541	66.106434	63.072756
1847.550500	57.003334	63.077761
1847.621280	55.454590	63.082766
1846.517626	52.053047	63.087770
1845.985535	53.638109	63.092775
1845.052010	54.300315	63.097780
1843.586599	52.181929	63.102785
1843.117197	50.950200	63.107790
1842.156220	56.737809	63.112794
1841.903689	55.645021	63.117799
1841.895912	60.093284	63.122804
1841.520856	56.616821	63.127809
1841.280689	55.724015	63.132814
1840.368652	54.446047	63.137818
1839.493150	50.204189	63.142823
1837.887038	54.460532	63.147828
1836.767028	51.696500	63.152833
1836.636036	54.730639	63.157838
1835.922760	55.361874	63.162842
1835.553100	46.680104	63.167847
1835.203899	56.515107	63.172852
1835.186744	52.963993	63.177857
1834.625707	53.109727	63.182862
1832.716764	63.044228	63.187866
1832.937024	51.864785	63.192871
1831.614262	49.279516	63.197876
1830.426308	46.610397	63.202881
1829.957009	49.036128	63.207886
1829.178918	52.810163	63.212890
1829.326899	49.726565	63.217895
1828.632338	52.705947	63.222900
1828.225447	44.190017	63.227905
1827.941941	50.052366	63.232910
1826.497469	45.899964	63.237914
1825.997978	46.070299	63.242919
1825.089222	53.970990	63.247924
1823.880914	52.594905	63.252929
1823.487895	52.484535	63.257934
1822.730630	51.401528	63.262938
1822.758960	51.178808	63.267943
1822.107893	60.697186	63.272948
1821.851960	58.935535	63.277953
1820.526092	51.062733	63.282958
1819.628875	54.988592	63.287962
1819.624875	54.482863	63.292967
1818.539395	47.944535	63.297972
1817.639251	57.370531	63.302977
1816.993276	48.846561	63.307982
1816.022706	57.358989	63.312986
1815.853556	44.210210	63.317991
1815.355724	54.974550	63.322996
1814.872476	61.321059	63.328001
1814.501282	64.735756	63.333006
1813.559499	59.096090	63.338010
1812.858135	55.321791	63.343015
1811.670728	57.303175	63.348020
1810.780069	54.835815	63.353025
1810.511397	49.425184	63.358030
1809.695567	54.402470	63.363034
1809.137118	50.822395	63.368039
1808.912880	60.966005	63.373044
1808.194611	51.566284	63.378049
1807.799044	50.796379	63.383054
1806.799330	50.311412	63.388058
1806.636564	49.100247	63.393063
1805.017753	52.518411	63.398068
1803.897831	46.684635	63.403073
1803.639374	47.651723	63.408078
1803.224655	52.215000	63.413082
1803.056680	45.836262	63.418087
1802.271603	48.757715	63.423092
1801.794685	58.060382	63.428097
1800.850153	57.533608	63.433102
1799.978827	55.416217	63.438106
1799.488770	48.801281	63.443111
1798.491338	59.608078	63.448116
1797.683058	58.037640	63.453121
1797.421349	53.915369	63.458126
1796.816100	59.584097	63.463130
1796.584051	52.262676	63.468135
1795.244877	52.650099	63.473140
1794.126672	56.922049	63.478145
1793.898153	54.570340	63.483150
1793.696321	59.909924	63.488154
1793.071944	61.738930	63.493159
1792.459913	62.700991	63.498164
1791.329458	54.983833	63.503169
1790.918045	54.457420	63.508174
1789.982831	58.498729	63.513178
1789.416538	49.585752	63.518183
1789.224315	54.245561	63.523188
1788.128916	51.234972	63.528193
1787.648174	47.418194	63.533198
1787.300847	58.147311	63.538202
1786.146294	51.239509	63.543207
1785.266152	47.581854	63.548212
1784.743472	53.815507	63.553217
1784.194729	55.177249	63.558222
1783.872769	60.681065	63.563226
1783.154336	55.276340	63.568231
1782.052645	57.607391	63.573236
1781.458877	57.319802	63.578241
1781.460124	49.350598	63.583246
1779.786200	50.507376	63.588250
1779.117503	48.828589	63.593255
1778.626789	53.322374	63.598260
1777.906946	52.107450	63.603265
1777.565328	48.873554	63.608270
1777.138710	52.383387	63.613274
1776.662624	52.798396	63.618279
1775.558184	62.183172	63.623284
1774.808710	57.394391	63.628289
1774.436793	49.003926	63.633294
1773.971517	50.883470	63.638298
1773.268104	56.505444	63.643303
1772.445821	47.443648	63.648308
1771.712063	50.566710	63.653313
1771.196412	50.169445	63.658318
1770.111741	55.409830	63.663322
1769.174678	52.543462	63.668327
1768.664602	52.486281	63.673332
1768.007313	55.541394	63.678337
1767.966869	51.054045	63.683342
1767.169771	53.689414	63.688346
1767.173800	52.585495	63.693351
1765.628246	55.595232	63.698356
1764.872929	54.100208	63.703361
1764.876216	54.362146	63.708366
1763.412195	57.480692	63.713370
1762.747089	44.912156	63.718375
1762.160412	50.551258	63.723380
1761.607950	49.925040	63.728385
1761.584362	47.519323	63.733390
1760.416767	50.062566	63.738394
1759.968845	39.246534	63.743399
1759.075689	52.946940	63.748404
1758.478401	53.574127	63.753409
1758.336371	47.493704	63.758414
1756.623245	55.150338	63.763418
1756.111915	50.534753	63.768423
1755.440663	42.625361	63.773428
1754.725998	55.293035	63.778433
1754.512454	49.409577	63.783438
1754.211634	57.331381	63.788442
1753.899879	53.476614	63.793447
1752.431463	52.992121	63.798452
1751.724782	51.234972	63.803457
1751.649009	47.516269	63.808462
1750.381321	58.229185	63.813466
1749.549662	41.370917	63.818471
1748.995822	56.514780	63.823476
1748.248744	57.558372	63.828481
1748.206127	56.613611	63.833486
1747.433361	58.130920	63.838490
1746.888244	54.852507	63.843495
1746.075424	48.856073	63.848500
1745.365326	49.562956	63.853505
1744.538655	45.760772	63.858510
1743.441705	54.555739	63.863514
1742.900022	47.466905	63.868519
1742.998364	50.595612	63.873524
1742.446474	51.009384	63.878529
1741.406372	40.158898	63.883534
1740.143893	52.180994	63.888538
1739.844954	40.870546	63.893543
1739.044744	45.371105	63.898548
1738.863703	48.651427	63.903553
1738.129297	42.077920	63.908558
1737.457797	48.067443	63.913562
1736.466903	39.602514	63.918567
1736.513390	46.497032	63.923572
1735.601625	52.174394	63.928577
1734.223803	43.941057	63.933582
1733.674091	45.055480	63.938586
1732.920015	45.070447	63.943591
1732.863057	53.892323	63.948596
1732.060412	44.337332	63.953601
1732.127130	41.440923	63.958606
1730.596040	45.413282	63.963610
1730.072110	44.351546	63.968615
1729.771789	46.279048	63.973620
1728.979884	44.527803	63.978625
1727.802712	45.717618	63.983630
1727.102698	55.508043	63.988634
1726.618100	49.405716	63.993639
1726.307851	49.242903	63.998644
1725.388152	58.242797	64.003649
1724.916067	50.450507	64.008654
1724.166634	61.676697	64.013658
1723.483041	53.560612	64.018663
1723.042649	55.851147	64.023668
1721.833826	54.438466	64.028673
1721.269605	53.578222	64.033678
1720.628878	64.497274	64.038682
1720.332522	47.260847	64.043687
1719.943358	48.553054	64.048692
1718.577054	57.044392	64.053697
1718.039226	49.925298	64.058702
1717.262797	61.750161	64.063706
1716.940818	54.279144	64.068711
1717.022473	48.872918	64.073716
1716.021300	56.673781	64.078721
1715.288383	52.105196	64.083726
1713.794506	53.550514	64.088730
1713.005014	50.954157	64.093735
1712.623109	50.447569	64.098740
1711.813035	56.042801	64.103745
1711.707551	46.996520	64.108750
1710.974161	52.873879	64.113754
1710.535296	49.620710	64.118759
1709.827107	56.978299	64.123764
1708.782462	58.019132	64.128769
1708.278518	50.295056	64.133774
1707.898396	45.526771	64.138778
1706.892770	48.545577	64.143783
1706.018515	56.182229	64.148788
1704.928815	58.416510	64.153793
1704.896493	56.967905	64.158798
1704.219628	60.149921	64.163802
1704.125688	58.885537	64.168807
1702.990851	62.504325	64.173812
1701.999775	59.202364	64.178817
1701.774909	48.131468	64.183822
1700.852864	56.503766	64.188826
1700.876052	53.492441	64.193831
1700.171031	51.092807	64.198836
1699.009062	55.515940	64.203841
1698.478205	41.317153	64.208846
1696.918582	55.917491	64.213850
1696.593589	60.907901	64.218855
1695.687123	59.213761	64.223860
1696.101204	57.049719	64.228865
1695.852107	56.794342	64.233870
1694.999693	52.395808	64.238874
1693.748497	47.109502	64.243879
1693.238969	51.709137	64.248884
1692.411026	52.854990	64.253889
1692.194090	39.448374	64.258894
1690.471357	48.958688	64.263898
1690.066591	52.036909	64.268903
1689.562553	41.056421	64.273908
1689.295681	51.173366	64.278913
1688.659247	46.375919	64.283918
1687.645202	56.165610	64.288922
1686.762473	58.669597	64.293927
1686.428280	56.405843	64.298932
1685.758811	57.416032	64.303937
1685.804335	58.676489	64.308942
1684.471684	54.388948	64.313946
1684.145470	55.684595	64.318951
1683.453010	51.205011	64.323956
1682.475423	52.522124	64.328961
1681.626579	53.437487	64.333966
1681.144444	67.954114	64.338970
1680.736918	56.126612	64.343975
1679.695121	48.169725	64.348980
1679.039291	58.945706	64.353985
1678.420734	46.960515	64.358990
1677.485058	57.204145	64.363994
1677.150116	56.666629	64.368999
1676.622783	53.674513	64.374004
1675.875400	54.447388	64.379009
1675.675843	54.914556	64.384014
1674.346511	55.045731	64.389018
1673.750420	58.475628	64.394023
1673.290074	52.174956	64.399028
1672.954102	62.060584	64.404033
1672.216726	52.786922	64.409038
1670.852519	66.228094	64.414042
1670.245300	51.736069	64.419047
1670.013832	50.406408	64.424052
1669.127126	52.273605	64.429057
1668.944067	43.557960	64.434062
1668.112928	52.095090	64.439066
1667.087577	53.276701	64.444071
1666.654273	55.941010	64.449076
1666.106627	58.228193	64.454081
1665.638029	53.951478	64.459086
1664.439630	53.679346	64.464090
1663.735183	50.580177	64.469095
1663.459202	53.820302	64.474100
1662.701028	48.433455	64.479105
1661.969557	45.389831	64.484110
1661.182122	53.549631	64.489114
1660.738602	50.213189	64.494119
1660.499200	39.423072	64.499124
1659.694600	47.168982	64.504129
1658.527200	45.938695	64.509134
1657.830883	47.851072	64.514138
1657.250490	51.460248	64.519143
1657.012273	55.975170	64.524148
1656.110253	54.950906	64.529153
1655.338127	45.369397	64.534158
1654.414896	56.249554	64.539162
1654.052142	56.086257	64.544167
1653.829073	42.425311	64.549172
1652.449242	49.070107	64.554177
1651.435467	48.402454	64.559182
1650.892003	53.069079	64.564186
1650.557841	54.495162	64.569191
1650.594028	59.218511	64.574196
1649.843685	51.098077	64.579201
1649.344575	48.863339	64.584206
1648.091811	55.917428	64.589210
1647.344308	54.136493	64.594215
1646.821126	49.104945	64.599220
1646.353492	54.514482	64.604225
1645.736081	40.435912	64.609230
1644.759602	57.387279	64.614234
1644.260237	48.123421	64.619239
1643.771817	46.202630	64.624244
1641.926670	48.786056	64.629249
1642.370945	50.802054	64.634254
1641.078737	56.145865	64.639258
1640.763458	50.929536	64.644263
1640.788897	56.822303	64.649268
1639.663065	53.282507	64.654273
1639.440970	53.124745	64.659278
1638.356141	54.349302	64.664282
1637.587036	51.496455	64.669287
1637.406291	51.202938	64.674292
1636.202161	57.871356	64.679297
1635.651507	49.860431	64.684302
1635.320199	50.193838	64.689306
1634.141375	51.352378	64.694311
1633.492337	50.180226	64.699316
1632.616154	53.541219	64.704321
1632.039058	47.787880	64.709326
1631.760747	56.489346	64.714330
1631.252086	54.696750	64.719335
1630.199362	60.324831	64.724340
1629.142124	55.102452	64.729345
1628.744684	54.637211	64.734350
1628.365501	54.713954	64.739354
1627.537335	54.535572	64.744359
1627.819309	61.663330	64.749364
1626.516409	64.328436	64.754369
1625.705123	51.799156	64.759374
1625.128184	51.457787	64.764378
1624.567438	59.758397	64.769383
1623.596088	53.185591	64.774388
1622.907890	58.430779	64.779393
1622.479228	56.804091	64.784398
1622.054039	60.584466	64.789402
1620.879417	58.330336	64.794407
1620.252737	60.364612	64.799412
1619.398112	67.763454	64.804417
1619.104278	58.960980	64.809422
1618.618361	57.104890	64.814426
1618.018137	58.461248	64.819431
1616.704536	55.908417	64.824436
1616.367053	63.266519	64.829441
1616.101660	55.743203	64.834446
1615.323453	64.194313	64.839450
1614.210269	62.049270	64.844455
1613.509680	52.122383	64.849460
1613.006129	59.269703	64.854465
1612.679465	62.911644	64.859470
1612.318457	63.400523	64.864474
1611.090286	60.761628	64.869479
1610.426279	49.806554	64.874484
1609.808998	62.360467	64.879489
1609.449656	64.575169	64.884494
1608.733347	65.442600	64.889498
1607.277774	67.400055	64.894503
1606.983148	53.362950	64.899508
1606.234596	65.867096	64.904513
1606.125002	63.790298	64.909518
1605.925594	60.308274	64.914522
1604.487107	66.590904	64.919527
1603.779226	58.537023	64.924532
1603.474221	64.960004	64.929537
1602.663839	56.063572	64.934542
1601.558165	61.502569	64.939546
1600.765633	54.035916	64.944551
1600.330777	51.489016	64.949556
1599.735343	66.261857	64.954561
1599.489218	54.164789	64.959566
1599.180848	52.082932	64.964570
1598.248486	60.976852	64.969575
1597.163680	60.835684	64.974580
1596.370911	60.482309	64.979585
1596.272490	53.526448	64.984590
1595.789649	63.827586	64.989594
1594.278606	59.468367	64.994599
1593.941323	56.828194	64.999604
1593.554074	67.093238	65.004609
1592.963168	46.960275	65.009614
1591.475581	50.971408	65.014618
1590.546331	58.036060	65.019623
1590.300148	53.863391	65.024628
1589.787211	57.067099	65.029633
1589.460494	51.013560	65.034638
1589.196997	55.786613	65.039642
1588.581370	56.243281	65.044647
1587.624573	50.127448	65.049652
1586.905609	63.043352	65.054657
1586.343552	53.487482	65.059662
1585.494018	60.759932	65.064666
1584.563452	67.279707	65.069671
1584.204257	56.195105	65.074676
1583.638977	55.715567	65.079681
1582.975160	56.077857	65.084686
1581.971547	56.829072	65.089690
1581.105121	61.286513	65.094695
1581.092709	56.769508	65.099700
1580.002860	69.349829	65.104705
1579.213329	60.204711	65.109710
1578.466273	57.886103	65.114714
1577.781222	58.474648	65.119719
1577.761307	55.692140	65.124724
1577.155921	58.061445	65.129729
1576.241257	50.669382	65.134734
1575.323208	50.977291	65.139738
1574.641918	52.893817	65.144743
1574.347119	50.287821	65.149748
1573.417541	63.271348	65.154753
1573.252638	52.400594	65.159758
1571.787032	58.066186	65.164762
1571.213003	55.995455	65.169767
1571.123600	48.160595	65.174772
1570.657324	56.990143	65.179777
1569.776332	57.846686	65.184782
1568.594804	60.381301	65.189786
1567.952033	59.151640	65.194791
1567.902903	56.767667	65.199796
1566.814939	56.389030	65.204801
1566.004998	48.867343	65.209806
1565.288556	61.219155	65.214810
1564.910186	60.665002	65.219815
1564.704939	51.778698	65.224820
1564.001721	56.945149	65.229825
1562.912854	52.416591	65.234830
1562.008153	49.969842	65.239834
1561.481050	48.681704	65.244839
1561.494129	47.230860	65.249844
1559.868364	47.976455	65.254849
1559.282247	46.504216	65.259854
1559.113026	46.981590	65.264858
1558.418206	52.605660	65.269863
1558.249227	50.719020	65.274868
1556.646911	51.847428	65.279873
1555.868711	47.375437	65.284878
1555.592832	49.894789	65.289882
1554.854812	61.113503	65.294887
1554.988046	46.321511	65.299892
1553.925844	60.925950	65.304897
1552.931265	55.075132	65.309902
1552.493342	47.975679	65.314906
1552.009865	52.685725	65.319911
1551.628561	44.440978	65.324916
1550.115307	55.128448	65.329921
1549.443852	53.109524	65.334926
1548.495727	45.067175	65.339930
1548.155875	46.829747	65.344935
1547.915989	47.460524	65.349940
1547.100113	53.115576	65.354945
1546.269939	53.561996	65.359950
1545.602706	49.832428	65.364954
1545.420562	57.913512	65.369959
1545.297525	55.238256	65.374964
1543.585289	55.792217	65.379969
1543.210691	60.274826	65.384974
1542.692085	46.497511	65.389978
1541.921926	63.090300	65.394983
1540.981937	50.231378	65.399988
1539.752593	59.297308	65.404993
1539.454503	51.766179	65.409998
1539.341826	46.889777	65.415002
1538.611259	53.878984	65.420007
1538.372537	49.291774	65.425012
1536.898787	50.024780	65.430017
1536.752842	52.605969	65.435022
1536.282732	48.009415	65.440026
1535.397998	51.654108	65.445031
1535.086177	45.048976	65.450036
1533.740538	46.195431	65.455041
1533.268717	49.857478	65.460046
1532.596089	53.645468	65.465050
1531.155177	55.924101	65.470055
1530.650722	47.392947	65.475060
1530.600370	60.728077	65.480065
1530.016863	48.071033	65.485070
1529.660297	54.229293	65.490074
1528.694264	49.628804	65.495079
1528.076037	52.230037	65.500084
1527.268659	66.324312	65.505089
1527.008901	57.911529	65.510094
1525.924753	58.012226	65.515098
1524.529073	57.602584	65.520103
1524.477666	59.414076	65.525108
1523.784924	55.038774	65.530113
1522.983731	52.278278	65.535118
1522.987603	50.154040	65.540122
1522.292529	54.832411	65.545127
1521.742723	56.596973	65.550132
1520.679149	59.675463	65.555137
1520.395876	54.679843	65.560142
1519.337296	51.980372	65.565146
1518.470599	57.717544	65.570151
1517.951040	63.502669	65.575156
1517.329190	59.290884	65.580161
1516.776837	54.517363	65.585166
1516.223382	56.462936	65.590170
1515.464658	54.926300	65.595175
1514.976391	46.566845	65.600180
1514.233891	57.830533	65.605185
1513.138104	62.050539	65.610190
1512.323741	51.755930	65.615194
1511.251673	56.783418	65.620199
1511.277463	45.880435	65.625204
1510.912493	52.368539	65.630209
1510.459361	48.920477	65.635214
1510.143577	52.845937	65.640218
1508.868081	50.559367	65.645223
1508.017950	47.282275	65.650228
1507.408318	54.592612	65.655233
1506.993905	47.652952	65.660238
1506.061185	51.066662	65.665242
1505.115185	50.805051	65.670247
1504.850060	41.526001	65.675252
1504.145888	50.946500	65.680257
1503.898837	47.962487	65.685262
1503.116426	48.796642	65.690266
1501.906960	49.001684	65.695271
1501.625046	46.592823	65.700276
1500.891670	52.673871	65.705281
1500.317190	56.424935	65.710286
1499.504524	46.471079	65.715290
1498.729988	55.671924	65.720295
1498.783928	49.601403	65.725300
1497.654239	48.353252	65.730305
1496.653784	55.490098	65.735310
1495.779710	50.357980	65.740314
1495.408669	54.057646	65.745319
1495.344427	54.361535	65.750324
1494.503218	53.124797	65.755329
1493.634768	48.197366	65.760334
1492.867847	53.025003	65.765338
1491.893360	56.851636	65.770343
1492.286036	45.276021	65.775348
1490.850227	60.588983	65.780353
1490.046830	50.847479	65.785358
1489.437616	40.746707	65.790362
1489.256646	52.290055	65.795367
1488.699159	39.171097	65.800372
1487.622196	44.686110	65.805377
1487.177794	45.906078	65.810382
1486.483060	42.328065	65.815386
1485.684612	45.961942	65.820391
1485.143134	40.137801	65.825396
1484.102745	49.691237	65.830401
1483.996536	43.941405	65.835406
1483.487997	37.574811	65.840410
1482.059809	45.664296	65.845415
1481.496062	39.047031	65.850420
1480.933686	44.767246	65.855425
1479.787978	40.501851	65.860430
1479.848194	48.654730	65.865434
1479.230168	47.829381	65.870439
1478.751914	50.315086	65.875444
1477.702439	47.921948	65.880449
1476.881968	47.594648	65.885454
1476.762462	51.176266	65.890458
1475.460126	48.301037	65.895463
1475.056834	40.660830	65.900468
1474.199851	46.770928	65.905473
1473.594889	50.171173	65.910478
1473.498257	39.032981	65.915482
1472.513124	47.770550	65.920487
1471.731924	43.822882	65.925492
1470.533642	52.898895	65.930497
1470.237248	49.804125	65.935502
1470.387612	42.279934	65.940506
1469.198580	54.270940	65.945511
1468.777329	46.741562	65.950516
1467.591330	51.598301	65.955521
1466.936130	53.615764	65.960526
1466.746735	52.471931	65.965530
1466.177532	55.200957	65.970535
1465.304319	47.993663	65.975540
1464.522974	52.477209	65.980545
1463.901219	47.478351	65.985550
1463.476932	42.580295	65.990554
1461.789729	52.510484	65.995559
1461.783547	40.467115	66.000564
1461.012938	47.519623	66.005569
1460.524901	55.805815	66.010574
1460.137787	46.764744	66.015578
1459.503677	61.446698	66.020583
1458.433957	44.690456	66.025588
1457.724895	51.814927	66.030593
1457.385900	57.215479	66.035598
1457.036203	45.233667	66.040602
1455.974706	59.446428	66.045607
1455.296142	44.235268	66.050612
1454.595601	52.606381	66.055617
1453.827755	46.283777	66.060622
1453.558440	44.145120	66.065626
1452.406723	57.720063	66.070631
1451.635946	54.307825	66.075636
1450.712289	57.180413	66.080641
1450.540897	57.364490	66.085646
1450.186936	52.680964	66.090650
1449.727335	58.385568	66.095655
1449.155965	51.680797	66.100660
1447.916962	49.788636	66.105665
1447.546482	50.785965	66.110670
1447.164041	57.601125	66.115674
1445.407447	47.722406	66.120679
1445.023221	50.854357	66.125684
1444.473852	55.614764	66.130689
1444.424196	56.002205	66.135694
1444.182961	48.359522	66.140698
1442.664305	47.951216	66.145703
1442.418424	48.028839	66.150708
1441.578349	51.419596	66.155713
1440.283537	48.774789	66.160718
1439.660389	46.254611	66.165722
1438.764329	54.914575	66.170727
1438.677854	49.286099	66.175732
1437.993458	49.073666	66.180737
1437.763136	53.811435	66.185742
1437.668060	45.195229	66.190746
1436.159452	56.899903	66.195751
1435.352233	54.823713	66.200756
1434.666900	50.211513	66.205761
1433.823035	51.160798	66.210766
1433.762276	43.852736	66.215770
1432.698334	51.941858	66.220775
1432.354774	39.944005	66.225780
1431.989494	45.964813	66.230785
1430.871334	40.767523	66.235790
1429.677037	42.412681	66.240794
1429.196859	44.753066	66.245799
1428.841989	39.476441	66.250804
1428.356992	50.238572	66.255809
1428.001610	40.785913	66.260814
1427.141505	47.440867	66.265818
1426.226796	47.972036	66.270823
1425.684919	40.678437	66.275828
1425.127592	50.867581	66.280833
1424.074423	46.821613	66.285838
1423.521057	47.545525	66.290842
1422.757152	55.418300	66.295847
1422.479041	46.020305	66.300852
1421.866994	55.020454	66.305857
1420.512110	49.754347	66.310862
1420.116792	50.214375	66.315866
1419.436954	49.900906	66.320871
1419.472179	46.580044	66.325876
1418.369361	56.328509	66.330881
1417.181558	54.673107	66.335886
1417.005174	48.777009	66.340890
1416.309982	56.225938	66.345895
1415.740660	47.434342	66.350900
1415.464491	55.497567	66.355905
1413.940450	47.000833	66.360910
1413.685419	43.366909	66.365914
1412.929174	48.751252	66.370919
1412.481539	48.446588	66.375924
1412.187301	53.317265	66.380929
1411.168072	51.106851	66.385934
1410.601175	40.442696	66.390938
1409.652868	39.426008	66.395943
1408.711652	45.986694	66.400948
1407.983845	48.202503	66.405953
1407.729871	51.909764	66.410958
1407.349030	42.695928	66.415962
1406.448122	53.703323	66.420967
1406.049901	43.063188	66.425972
1404.664719	43.742783	66.430977
1404.098193	44.523815	66.435982
1403.766540	43.690508	66.440986
1403.540419	55.237631	66.445991
1402.927075	45.568616	66.450996
1401.615949	48.593977	66.456001
1400.856629	42.644515	66.461006
1400.376669	37.216814	66.466010
1399.658110	50.816290	66.471015
1399.522646	43.086435	66.476020
1398.372249	42.439457	66.481025
1397.341778	42.388106	66.486030
1397.328105	46.081073	66.491034
1396.449928	50.081882	66.496039
1396.250392	51.116265	66.501044
1394.869204	53.363001	66.506049
1394.142656	52.302435	66.511054
1393.821056	48.219270	66.516058
1393.302389	52.547339	66.521063
1393.105092	50.637530	66.526068
1391.678885	50.005398	66.531073
1390.652265	54.395548	66.536078
1390.546015	60.817264	66.541082
1390.380372	54.140943	66.546087
1389.690709	47.179737	66.551092
1388.289608	42.255485	66.556097
1387.511395	47.501886	66.561102
1387.179281	46.424328	66.566106
1386.750932	48.183110	66.571111
1385.982120	40.970599	66.576116
1384.865939	47.263620	66.581121
1383.993629	40.942338	66.586126
1383.881766	45.797189	66.591130
1383.307168	49.331185	66.596135
1383.085397	46.828358	66.601140
1382.439400	49.321469	66.606145
1381.684418	52.192823	66.611150
1381.158638	41.402037	66.616154
1379.867976	54.362113	66.621159
1379.206947	53.700841	66.626164
1378.345934	45.656652	66.631169
1378.305862	54.929533	66.636174
1377.875261	39.551619	66.641178
1376.413752	52.880397	66.646183
1375.629395	52.400492	66.651188
1375.113106	53.615802	66.656193
1374.110617	44.554961	66.661198
1374.188071	42.934423	66.666202
1373.719576	51.233056	66.671207
1373.031337	39.869321	66.676212
1371.988941	45.331069	66.681217
1371.082225	46.232308	66.686222
1370.550317	38.489404	66.691226
1370.532140	51.146793	66.696231
1369.451962	50.302283	66.701236
1368.426197	44.799865	66.706241
1367.986667	45.810202	66.711246
1367.765244	48.379050	66.716250
1367.254643	53.074801	66.721255
1366.358855	43.526377	66.726260
1365.045081	46.298790	66.731265
1364.746820	50.317565	66.736270
1364.353135	48.536503	66.741274
1363.228335	50.677782	66.746279
1362.604863	45.767258	66.751284
1361.514932	41.191178	66.756289
1361.298835	52.707372	66.761294
1361.350316	41.994213	66.766298
1360.697185	44.869054	66.771303
1359.698543	46.298770	66.776308
1359.162105	40.669173	66.781313
1358.115449	47.519086	66.786318
1357.689361	41.515353	66.791322
1356.809467	48.446847	66.796327
1355.978884	39.878404	66.801332
1355.739082	43.364168	66.806337
1354.972740	40.071976	66.811342
1354.268363	37.452434	66.816346
1353.152382	44.278688	66.821351
1352.415223	36.670788	66.826356
1352.116974	47.035832	66.831361
1351.564033	46.007526	66.836366
1351.371309	38.831796	66.841370
1350.759131	34.925876	66.846375
1349.562787	44.183534	66.851380
1349.164844	49.449313	66.856385
1348.160449	44.056131	66.861390
1347.309457	31.391255	66.866394
1346.357927	44.722332	66.871399
1346.106367	36.669350	66.876404
1346.024124	41.723986	66.881409
1345.440109	47.036617	66.886414
1344.503163	34.894454	66.891418
1343.786502	41.145534	66.896423
1343.104160	36.047341	66.901428
1342.496144	38.424615	66.906433
1341.353170	45.711392	66.911438
1340.777521	42.729568	66.916442
1339.850814	46.316738	66.921447
1339.479423	49.770953	66.926452
1339.175440	41.503534	66.931457
1338.827496	52.137207	66.936462
1337.836677	44.516679	66.941466
1336.724891	44.533336	66.946471
1336.324199	46.507639	66.951476
1335.886891	46.165295	66.956481
1335.181055	46.695063	66.961486
1334.554070	37.933492	66.966490
1333.572589	46.355069	66.971495
1332.849359	55.562533	66.976500
1332.758469	51.377120	66.981505
1332.240004	46.773479	66.986510
1331.249977	44.260073	66.991514
1330.530395	48.438599	66.996519
1330.166092	43.158074	67.001524
1329.190244	43.868664	67.006529
1327.845291	50.676099	67.011534
1327.941476	36.602561	67.016538
1327.076085	51.122391	67.021543
1326.730432	45.853672	67.026548
1325.818376	43.124430	67.031553
1325.097087	57.242248	67.036558
1324.396786	53.220761	67.041562
1324.024136	50.178530	67.046567
1323.604568	56.604933	67.051572
1322.257982	39.122893	67.056577
1321.408162	47.599298	67.061582
1321.200177	38.362205	67.066586
1320.683309	40.526125	67.071591
1320.258848	45.987881	67.076596
1319.210589	43.802194	67.081601
1318.226223	47.865794	67.086606
1317.697053	39.900599	67.091610
1316.946828	45.306417	67.096615
1316.819523	47.721002	67.101620
1316.000357	49.481169	67.106625
1315.104702	51.852822	67.111630
1314.739736	41.250827	67.116634
1314.021438	45.174936	67.121639
1313.514539	47.190315	67.126644
1312.518513	51.621027	67.131649
1311.349997	45.654400	67.136654
1311.361048	48.137664	67.141658
1310.821238	46.198868	67.146663
1310.350894	48.487056	67.151668
1309.472002	49.079215	67.156673
1308.749409	52.745127	67.161678
1308.558116	51.618600	67.166682
1307.499060	56.960850	67.171687
1306.467181	43.702498	67.176692
1305.710461	40.021450	67.181697
1305.227337	55.884987	67.186702
1305.025752	45.087661	67.191706
1303.762447	50.248964	67.196711
1302.845793	45.685470	67.201716
1302.559055	42.058169	67.206721
1302.162041	51.131237	67.211726
1301.511528	41.930036	67.216730
1301.215783	55.583048	67.221735
1299.870992	47.532097	67.226740
1299.491284	49.754245	67.231745
1298.787299	51.765867	67.236750
1298.809676	41.948576	67.241754
1297.178572	47.649664	67.246759
1296.387404	45.138141	67.251764
1295.698896	49.672518	67.256769
1295.311074	45.204800	67.261774
1295.389830	43.578118	67.266778
1294.297171	48.100766	67.271783
1293.349903	41.613135	67.276788
1292.786571	44.317091	67.281793
1291.919469	50.022777	67.286798
1291.851103	47.033454	67.291802
1290.691115	45.629890	67.296807
1289.914178	53.481615	67.301812
1289.623851	44.433085	67.306817
1288.556798	51.832790	67.311822
1288.552765	41.151642	67.316826
1287.509340	49.484756	67.321831
1286.523737	50.658844	67.326836
1285.925872	39.271372	67.331841
1285.504920	53.391057	67.336846
1285.666091	41.268932	67.341850
1284.533800	54.100464	67.346855
1283.263765	59.369106	67.351860
1282.861463	48.811001	67.356865
1282.653198	49.363353	67.361870
1281.525499	36.411143	67.366874
1280.997405	48.815567	67.371879
1280.479645	44.154974	67.376884
1280.337900	44.366744	67.381889
1278.766659	52.597203	67.386894
1278.308760	34.802794	67.391898
1277.646991	49.722348	67.396903
1276.998655	52.742818	67.401908
1275.800412	49.855747	67.406913
1275.081957	53.201232	67.411918
1274.954156	46.851590	67.416922
1274.362149	46.891376	67.421927
1273.890855	43.863672	67.426932
1273.487752	46.547698	67.431937
1272.294988	47.836593	67.436942
1271.618018	42.326986	67.441946
1270.911741	47.186496	67.446951
1270.425663	45.682564	67.451956
1269.555105	47.771651	67.456961
1268.895135	49.023804	67.461966
1267.982686	47.125916	67.466970
1267.498644	48.677934	67.471975
1267.326350	42.464195	67.476980
1266.711577	38.723724	67.481985
1265.923289	50.801659	67.486990
1264.851736	37.503937	67.491994
1264.305279	47.477281	67.496999
1263.877527	44.633562	67.502004
1262.928950	44.362965	67.507009
1261.785398	56.785528	67.512014
1261.696906	46.138575	67.517018
1260.677534	46.144164	67.522023
1260.505419	46.906633	67.527028
1260.313651	49.904200	67.532033
1259.154031	50.585479	67.537038
1258.742423	46.788516	67.542042
1257.757050	51.700941	67.547047
1257.245069	56.289176	67.552052
1256.579292	46.204850	67.557057
1255.641381	45.517185	67.562062
1255.529061	41.519781	67.567066
1254.662721	45.713966	67.572071
1253.883466	36.622842	67.577076
1252.803072	42.857258	67.582081
1252.035406	50.352941	67.587086
1251.683261	45.178496	67.592090
1251.637639	40.636411	67.597095
1251.081603	40.787667	67.602100
1249.948739	41.624623	67.607105
1248.662394	48.542427	67.612110
1248.580124	44.265550	67.617114
1248.239778	45.115633	67.622119
1247.007312	44.247095	67.627124
1246.091309	36.832461	67.632129
1245.375289	44.224567	67.637134
1245.092545	32.910654	67.642138
1244.712928	42.909113	67.647143
1244.243433	44.651264	67.652148
1243.925777	43.230996	67.657153
1242.964973	51.603257	67.662158
1242.464032	40.029867	67.667162
1241.599759	50.419186	67.672167
1240.397020	37.643250	67.677172
1239.668340	41.670585	67.682177
1238.648118	47.324337	67.687182
1238.422550	39.695976	67.692186
1238.161829	48.354543	67.697191
1237.428087	47.445226	67.702196
1236.511628	37.346594	67.707201
1235.350208	50.601120	67.712206
1235.319828	49.846107	67.717210
1234.560492	45.920399	67.722215
1234.542221	55.446496	67.727220
1233.682666	46.163865	67.732225
1232.424812	46.816971	67.737230
1232.513480	38.538789	67.742234
1231.951097	47.245449	67.747239
1230.898399	49.029821	67.752244
1230.682035	42.589169	67.757249
1229.672953	52.446335	67.762254
1228.409853	52.784960	67.767258
1227.682779	53.242989	67.772263
1226.767863	49.469438	67.777268
1226.552379	43.315989	67.782273
1225.836532	51.409878	67.787278
1225.686896	33.584813	67.792282
1225.085277	41.132192	67.797287
1223.900007	48.823710	67.802292
1223.369877	50.593612	67.807297
1222.407281	51.198933	67.812302
1222.223294	49.099760	67.817306
1221.626930	56.283107	67.822311
1220.574854	51.207579	67.827316
1220.155045	42.834092	67.832321
1218.927563	50.023652	67.837326
1218.739461	44.084584	67.842330
1218.631047	50.896639	67.847335
1217.744830	56.402723	67.852340
1216.874738	55.787924	67.857345
1215.899710	52.907255	67.862350
1215.905419	52.026069	67.867354
1215.066350	54.451600	67.872359
1213.726012	55.176066	67.877364
1212.960736	55.105795	67.882369
1212.510679	56.144393	67.887374
1212.477726	53.609250	67.892378
1212.104815	49.476077	67.897383
1211.155107	48.908461	67.902388
1210.403098	48.426992	67.907393
1209.437750	52.260391	67.912398
1209.022315	50.279788	67.917402
1208.180486	54.356501	67.922407
1207.124538	59.175234	67.927412
1206.666033	50.096695	67.932417
1205.980817	54.752091	67.937422
1206.136272	53.748561	67.942426
1205.621152	49.744731	67.947431
1204.267820	53.612981	67.952436
1203.410056	48.929300	67.957441
1202.879439	58.662714	67.962446
1202.470015	50.542041	67.967450
1201.499849	47.505815	67.972455
1200.855576	59.171094	67.977460
1200.453401	51.521657	67.982465
1199.593026	57.272385	67.987470
1199.432052	49.929793	67.992474
1198.161983	48.326031	67.997479
1197.538104	60.672654	68.002484
1197.332251	59.049307	68.007489
1196.723466	58.649497	68.012494
1195.912251	48.313387	68.017498
1194.875530	51.480489	68.022503
1194.150344	54.682274	68.027508
1194.167063	43.163151	68.032513
1193.122913	56.956922	68.037518
1192.085298	59.768933	68.042522
1191.877328	49.670575	68.047527
1190.952664	53.765420	68.052532
1190.282636	44.648106	68.057537
1189.630413	53.381204	68.062542
1189.340924	48.612071	68.067546
1188.480486	57.318060	68.072551
1187.778030	52.643710	68.077556
1187.284371	44.420234	68.082561
1186.176860	53.176813	68.087566
1185.508216	45.616423	68.092570
1184.970154	52.922019	68.097575
1184.308918	49.220696	68.102580
1184.197617	50.963100	68.107585
1183.608603	56.187393	68.112590
1182.631603	50.680620	68.117594
1181.684390	53.498468	68.122599
1181.147924	49.777757	68.127604
1181.196826	47.540033	68.132609
1179.770295	44.727995	68.137614
1178.989891	45.667637	68.142618
1178.552478	53.633730	68.147623
1178.179230	52.980052	68.152628
1177.383413	44.995013	68.157633
1176.014010	50.958416	68.162638
1175.712069	51.182222	68.167642
1175.023361	50.501640	68.172647
1174.441421	54.240979	68.177652
1174.379244	37.188013	68.182657
1173.228947	44.706978	68.187662
1172.608743	37.949445	68.192666
1172.151766	47.327234	68.197671
1171.480889	48.589950	68.202676
1170.638312	41.002902	68.207681
1169.635882	46.281003	68.212686
1169.399114	48.175936	68.217690
1168.898002	51.784994	68.222695
1167.872553	63.538829	68.227700
1167.351308	50.682540	68.232705
1166.506029	51.248443	68.237710
1166.144294	44.392972	68.242714
1166.106771	50.771328	68.247719
1164.789538	58.588870	68.252724
1164.165753	54.963238	68.257729
1163.297291	52.992710	68.262734
1162.566052	47.540570	68.267738
1161.458132	53.718930	68.272743
1160.501352	54.554966	68.277748
1160.367722	52.427438	68.282753
1159.710887	58.354495	68.287758
1159.506859	47.581686	68.292762
1159.237186	54.898169	68.297767
1158.516995	52.923175	68.302772
1157.862494	48.917956	68.307777
1156.671000	59.002540	68.312782
1156.484046	51.987674	68.317786
1155.494088	57.187860	68.322791
1154.185010	52.483178	68.327796
1153.997239	48.121744	68.332801
1153.434499	54.832386	68.337806
1152.861842	57.347698	68.342810
1152.528435	44.206637	68.347815
1150.943718	49.958240	68.352820
1150.384871	46.511747	68.357825
1149.682770	55.589687	68.362830
1149.226669	49.459286	68.367834
1149.083459	44.489464	68.372839
1148.312329	43.504856	68.377844
1147.545169	42.839290	68.382849
1146.543566	53.181870	68.387854
1146.121082	41.346790	68.392858
1145.808649	45.210896	68.397863
1144.873544	47.626433	68.402868
1144.280812	41.265232	68.407873
1143.007059	50.986943	68.412878
1142.863271	47.141769	68.417882
1142.253039	49.978104	68.422887
1141.680281	46.250588	68.427892
1141.239289	47.120674	68.432897
1140.043091	58.048391	68.437902
1139.747764	47.858032	68.442906
1139.147241	53.932545	68.447911
1138.057956	53.933552	68.452916
1137.423662	52.145160	68.457921
1136.567361	52.092460	68.462926
1136.241749	47.740418	68.467930
1135.912589	45.823601	68.472935
1135.156524	53.048899	68.477940
1134.094028	54.246050	68.482945
1133.703038	53.289113	68.487950
1133.411293	53.163036	68.492954
1132.669979	43.614280	68.497959
1131.358430	55.597880	68.502964
1131.210186	41.231891	68.507969
1130.363308	52.777918	68.512974
1129.976178	50.659852	68.517978
1129.031308	45.187065	68.522983
1128.269693	45.752858	68.527988
1128.149121	40.721139	68.532993
1126.821952	51.195251	68.537998
1125.878016	43.404131	68.543002
1125.012068	44.028051	68.548007
1124.490479	50.137202	68.553012
1124.340435	51.321796	68.558017
1123.873223	46.568497	68.563022
1123.598052	42.105985	68.568026
1123.086990	47.261670	68.573031
1121.893388	49.239129	68.578036
1121.457969	45.202325	68.583041
1120.327321	50.937762	68.588046
1119.430165	43.885045	68.593050
1118.740427	44.644969	68.598055
1118.433136	55.697968	68.603060
1118.199409	47.001727	68.608065
1117.130537	54.383216	68.613070
1116.274148	47.518902	68.618074
1116.067289	52.837227	68.623079
1115.126119	52.546444	68.628084
1114.863051	51.001186	68.633089
1113.686041	65.596495	68.638094
1112.891780	47.263691	68.643098
1112.297221	53.380207	68.648103
1111.653944	55.265805	68.653108
1111.245959	46.045617	68.658113
1110.493103	51.948066	68.663118
1109.634133	44.609352	68.668122
1109.275388	44.438304	68.673127
1108.886493	52.033343	68.678132
1108.189992	42.995974	68.683137
1106.759631	40.533150	68.688142
1106.250516	54.413327	68.693146
1105.678319	46.423171	68.698151
1105.550558	50.735633	68.703156
1105.267895	48.642312	68.708161
1104.165745	58.210708	68.713166
1103.197437	49.693538	68.718170
1102.831264	40.368305	68.723175
1101.716949	47.720471	68.728180
1100.767133	44.445927	68.733185
1099.972684	49.814341	68.738190
1099.741209	51.724158	68.743194
1099.583597	45.025972	68.748199
1099.156509	56.654060	68.753204
1097.886689	42.401578	68.758209
1096.986850	57.511497	68.763214
1096.311633	53.441549	68.768218
1096.049450	46.849290	68.773223
1095.650047	48.009085	68.778228
1095.290204	42.451131	68.783233
1093.829866	51.799820	68.788238
1093.149129	41.044316	68.793242
1092.836884	45.205218	68.798247
1091.831985	49.272368	68.803252
1091.053689	44.246702	68.808257
1090.318585	51.581698	68.813262
1090.002667	51.764483	68.818266
1089.780278	46.252857	68.823271
1088.870877	50.892573	68.828276
1087.996409	46.200332	68.833281
1087.290900	60.200585	68.838286
1086.757297	55.144068	68.843290
1086.418647	49.814577	68.848295
1085.624500	54.377720	68.853300
1084.449707	49.059177	68.858305
1084.010743	50.974920	68.863310
1083.718789	49.473293	68.868314
1083.056016	46.204466	68.873319
1081.898425	43.774281	68.878324
1081.580641	48.459131	68.883329
1080.806317	46.264485	68.888334
1080.532255	52.347437	68.893338
1079.506867	46.713589	68.898343
1078.805037	49.790604	68.903348
1078.342371	47.110771	68.908353
1077.567367	54.427339	68.913358
1077.034354	48.482217	68.918362
1075.900321	48.122235	68.923367
1075.289021	49.975520	68.928372
1074.784355	39.643007	68.933377
1074.565483	54.330017	68.938382
1073.517312	40.726004	68.943386
1072.767577	35.369418	68.948391
1071.734129	47.453023	68.953396
1071.521709	44.152869	68.958401
1071.232734	53.797140	68.963406
1070.300185	47.645318	68.968410
1069.743902	49.153278	68.973415
1068.533942	52.640579	68.978420
1068.300442	49.341665	68.983425
1067.674171	50.350452	68.988430
1066.718988	48.831746	68.993434
1066.217280	51.375966	68.998439
1065.099536	52.260897	69.003444
1065.205580	50.812296	69.008449
1064.481559	52.187147	69.013454
1063.456084	49.884334	69.018458
1062.942584	47.831728	69.023463
1062.098646	48.393472	69.028468
1061.870345	46.533990	69.033473
1060.896800	48.793895	69.038478
1059.815376	45.009819	69.043482
1059.207014	43.420278	69.048487
1058.604583	44.972850	69.053492
1058.751613	41.721271	69.058497
1057.847250	50.846084	69.063502
1057.510187	50.444364	69.068506
1056.443193	47.626847	69.073511
1055.756324	46.820842	69.078516
1055.197852	41.562946	69.083521
1054.334888	44.823468	69.088526
1053.506145	50.538795	69.093530
1052.767039	39.153068	69.098535
1052.366656	53.058830	69.103540
1052.092475	41.743083	69.108545
1051.270860	50.127842	69.113550
1050.199296	52.397035	69.118554
1049.693138	51.039059	69.123559
1049.074517	50.906991	69.128564
1048.798772	45.996975	69.133569
1047.186303	49.775432	69.138574
1046.718336	49.491651	69.143578
1046.337951	41.737465	69.148583
1045.396703	47.350090	69.153588
1045.717179	45.633071	69.158593
1044.980380	47.073662	69.163598
1043.751725	37.892187	69.168602
1043.382032	39.361487	69.173607
1042.428668	44.304773	69.178612
1041.752247	38.946295	69.183617
1040.838698	42.623618	69.188622
1040.465194	40.532438	69.193626
1040.186596	36.582076	69.198631
1039.134593	43.871081	69.203636
1038.933104	43.360888	69.208641
1037.464165	44.517928	69.213646
1036.746504	48.466429	69.218650
1036.291202	43.131661	69.223655
1035.785500	42.027017	69.228660
1035.733587	45.714677	69.233665
1034.589474	45.917323	69.238670
1033.663095	50.804284	69.243674
1033.135934	37.597755	69.248679
1032.821660	46.839795	69.253684
1032.772570	39.848706	69.258689
1031.312710	48.107905	69.263694
1030.815927	49.298196	69.268698
1030.129185	40.634157	69.273703
1028.838005	36.731282	69.278708
1028.343566	35.910880	69.283713
1027.592741	37.968053	69.288718
1027.256371	40.952489	69.293722
1027.143602	39.305715	69.298727
1026.218305	44.220119	69.303732
1025.247026	36.975660	69.308737
1024.608024	47.391935	69.313742
1023.499420	42.147730	69.318746
1023.748396	41.617631	69.323751
1022.097808	47.753553	69.328756
1021.680066	40.456930	69.333761
1021.138575	47.287087	69.338766
1020.590489	48.040529	69.343770
1020.670976	38.640401	69.348775
1019.599281	42.913595	69.353780
1018.055171	38.796682	69.358785
1017.674391	38.498763	69.363790
1017.537117	53.210473	69.368794
1017.269480	45.875907	69.373799
1016.323928	59.608203	69.378804
1015.319845	47.579471	69.383809
1014.800193	52.315866	69.388814
1014.476701	48.349114	69.393818
1013.179819	45.201126	69.398823
1012.223626	51.247347	69.403828
1011.899383	37.955549	69.408833
1011.537742	46.211015	69.413838
1011.092419	45.465883	69.418842
1010.438698	40.082209	69.423847
1009.401804	49.788639	69.428852
1008.712275	43.900332	69.433857
1008.271862	46.277357	69.438862
1007.599927	45.713526	69.443866
1006.587244	43.969034	69.448871
1005.487627	37.760584	69.453876
1005.353438	38.708791	69.458881
1004.600500	44.917560	69.463886
1004.256811	44.196864	69.468890
1004.249650	44.523349	69.473895
1002.744704	51.174309	69.478900
1002.400766	34.728946	69.483905
1001.718245	43.068570	69.488910
1000.723399	46.483914	69.493914
999.887551	40.141878	69.498919
998.917249	40.774216	69.503924
998.905304	39.811193	69.508929
998.429205	37.099331	69.513934
998.435095	37.061626	69.518938
996.999307	43.858232	69.523943
995.768907	42.852043	69.528948
995.363264	38.257555	69.533953
995.112371	39.429817	69.538958
994.370430	29.926210	69.543962
993.413485	35.410875	69.548967
992.739137	37.458902	69.553972
992.121131	30.490648	69.558977
992.019104	37.970635	69.563982
991.137184	39.081629	69.568986
990.342189	37.188157	69.573991
989.414473	45.448201	69.578996
989.191080	32.990939	69.584001
988.566955	30.642702	69.589006
987.267410	40.267405	69.594010
986.620483	33.821971	69.599015
986.153495	40.063871	69.604020
985.692848	29.372153	69.609025
985.060726	38.271930	69.614030
984.559943	44.589484	69.619034
983.714833	37.093309	69.624039
982.818587	37.988875	69.629044
982.449228	38.618559	69.634049
982.256606	35.680531	69.639054
980.948606	38.455596	69.644058
980.285167	37.655853	69.649063
979.520912	40.714753	69.654068
979.261320	37.948053	69.659073
978.475443	44.462450	69.664078
977.676145	45.227736	69.669082
977.241777	41.699956	69.674087
976.436606	41.867857	69.679092
976.195291	37.827831	69.684097
974.998171	46.605306	69.689102
974.223986	41.552515	69.694106
973.490299	41.898823	69.699111
973.103930	43.126259	69.704116
972.806990	45.426217	69.709121
971.943782	43.774944	69.714126
971.067647	52.133917	69.719130
970.555884	39.473026	69.724135
969.932686	45.963511	69.729140
969.459919	44.036961	69.734145
968.459590	45.963197	69.739150
967.453652	43.272213	69.744154
967.436457	39.076574	69.749159
966.777431	44.709161	69.754164
965.455162	45.520198	69.759169
964.908841	44.179374	69.764174
964.517952	43.747409	69.769178
963.910513	41.530125	69.774183
963.438711	42.673908	69.779188
962.441244	45.951557	69.784193
961.359076	41.333600	69.789198
960.781450	42.272097	69.794202
960.911028	42.355307	69.799207
960.302328	47.622059	69.804212
959.808609	39.232069	69.809217
958.916259	49.945538	69.814222
957.678161	44.733791	69.819226
957.780393	45.343893	69.824231
956.386878	41.237130	69.829236
955.816627	36.903721	69.834241
955.198343	37.715374	69.839246
954.553880	44.299101	69.844250
954.469032	33.831565	69.849255
953.174329	41.161356	69.854260
952.376957	38.211248	69.859265
951.834907	28.124370	69.864270
951.208148	36.645485	69.869274
951.072160	34.744547	69.874279
949.930220	45.594701	69.879284
948.940333	39.915734	69.884289
948.577384	48.973093	69.889294
947.932393	43.349131	69.894298
947.897035	37.529189	69.899303
946.209420	42.524821	69.904308
945.497906	40.206160	69.909313
945.148824	46.862058	69.914318
944.348410	42.052569	69.919322
944.219000	36.795813	69.924327
943.743586	40.591918	69.929332
943.429388	30.467202	69.934337
942.091137	39.249901	69.939342
941.444493	39.546571	69.944346
941.110988	34.045311	69.949351
939.720512	37.687492	69.954356
939.025903	43.204602	69.959361
938.592560	40.441217	69.964366
938.191410	40.587296	69.969370
937.960842	37.249606	69.974375
937.237467	38.539103	69.979380
936.402932	34.360298	69.984385
935.739677	43.755648	69.989390
934.496186	41.320477	69.994394
933.539099	39.773312	69.999399
932.716606	45.874401	70.004404
932.807806	43.130911	70.009409
932.143193	37.697015	70.014414
931.439239	46.388849	70.019418
931.480798	40.928346	70.024423
930.882626	42.147851	70.029428
929.858090	39.616370	70.034433
929.019933	43.553151	70.039438
927.906909	45.821178	70.044442
927.213539	39.064777	70.049447
926.618693	40.257267	70.054452
926.176369	42.933818	70.059457
925.959311	47.729308	70.064462
925.003098	37.277596	70.069466
923.974885	37.228324	70.074471
923.159897	43.375099	70.079476
922.860146	39.995578	70.084481
922.236593	42.684222	70.089486
921.615139	49.358745	70.094490
921.272554	35.050953	70.099495
920.388812	45.808339	70.104500
919.953076	40.780880	70.109505
919.534834	32.675196	70.114510
917.880673	41.562530	70.119514
917.345922	44.000715	70.124519
916.474559	40.700541	70.129524
916.453106	35.559501	70.134529
915.800878	35.199535	70.139534
915.124876	42.367714	70.144538
914.109240	37.274189	70.149543
913.340931	41.427155	70.154548
912.928111	44.770461	70.159553
912.664663	42.117710	70.164558
911.845567	41.283850	70.169562
911.041096	36.004563	70.174567
910.241484	48.324432	70.179572
909.563350	47.888381	70.184577
909.550427	48.498469	70.189582
908.572898	47.776608	70.194586
907.693620	40.595760	70.199591
906.803634	44.252884	70.204596
906.645818	50.442232	70.209601
906.291077	41.555973	70.214606
904.661800	49.387924	70.219610
904.181777	37.627489	70.224615
903.369683	39.364004	70.229620
903.164091	37.532223	70.234625
903.136736	38.357929	70.239630
901.937305	47.264093	70.244634
901.327264	33.936407	70.249639
900.395148	46.980774	70.254644
900.173779	49.338052	70.259649
898.577768	38.888170	70.264654
897.984559	43.700321	70.269658
897.925077	37.584137	70.274663
897.207516	38.519767	70.279668
896.565249	37.741277	70.284673
896.296935	39.196380	70.289678
894.767110	38.063484	70.294682
894.661326	39.159978	70.299687
893.908276	44.224495	70.304692
893.567614	42.055077	70.309697
892.257391	44.508062	70.314702
891.450136	41.408087	70.319706
890.973626	37.256781	70.324711
890.172004	49.053208	70.329716
890.034025	47.181031	70.334721
889.802508	29.037326	70.339726
888.468634	38.712526	70.344730
887.982501	31.767888	70.349735
887.463035	38.549276	70.354740
886.984123	40.628181	70.359745
885.649190	35.841576	70.364750
885.482389	44.969145	70.369754
884.808788	34.343918	70.374759
884.068184	41.942351	70.379764
883.207239	46.926671	70.384769
882.593188	43.875706	70.389774
881.884251	50.348517	70.394778
881.671954	36.259984	70.399783
880.490842	39.278194	70.404788
879.661042	37.661084	70.409793
879.515663	35.344148	70.414798
878.404138	33.953308	70.419802
878.508177	34.815321	70.424807
877.209913	44.102343	70.429812
876.726435	47.347627	70.434817
876.514868	39.967955	70.439822
875.590690	46.168173	70.444826
874.791644	39.357651	70.449831
873.828396	43.522300	70.454836
873.185544	41.826199	70.459841
873.017341	38.366918	70.464846
872.149181	50.176716	70.469850
871.252770	47.257006	70.474855
870.432399	46.226408	70.479860
869.904586	52.854109	70.484865
869.334653	37.029296	70.489870
868.704733	51.253816	70.494874
868.132014	43.519576	70.499879
866.924303	38.525669	70.504884
866.625079	41.492302	70.509889
866.560525	39.135472	70.514894
865.792744	45.129702	70.519898
865.579814	45.308282	70.524903
864.353623	52.326376	70.529908
863.565069	46.835960	70.534913
862.659075	42.002338	70.539918
861.618087	43.180860	70.544922
861.213871	43.083536	70.549927
860.214963	43.367136	70.554932
859.578671	51.200721	70.559937
859.840936	44.396698	70.564942
859.189722	46.675241	70.569946
858.466494	35.668935	70.574951
857.381674	38.838411	70.579956
856.806041	37.747346	70.584961
856.468287	41.821045	70.589966
855.963787	48.272655	70.594970
855.341360	38.018385	70.599975
853.997311	41.206607	70.604980
853.464446	37.696109	70.609985
853.337812	41.209860	70.614990
851.961130	46.547769	70.619994
851.447996	43.247432	70.624999
850.277074	50.520125	70.630004
850.107913	34.381952	70.635009
850.095438	36.010329	70.640014
849.026247	42.854301	70.645018
848.086719	35.430383	70.650023
847.524577	39.934469	70.655028
846.966816	37.560676	70.660033
846.612528	28.975919	70.665038
845.494070	39.928237	70.670042
844.812121	36.470118	70.675047
843.888338	39.662932	70.680052
843.600936	45.053463	70.685057
843.300655	37.852009	70.690062
842.657855	38.738923	70.695066
842.020461	36.265092	70.700071
840.985823	39.108625	70.705076
840.315821	39.138929	70.710081
839.797792	33.812175	70.715086
838.276416	41.850250	70.720090
838.126804	34.330507	70.725095
837.487491	39.537774	70.730100
837.192473	40.470113	70.735105
836.779420	36.785946	70.740110
835.996554	39.115460	70.745114
835.339749	41.387067	70.750119
834.534994	43.338246	70.755124
834.084897	39.146109	70.760129
833.081047	42.079892	70.765134
831.873053	44.552089	70.770138
831.699758	39.211284	70.775143
830.999515	38.205905	70.780148
830.815580	34.906419	70.785153
830.205307	35.095037	70.790158
829.274865	38.354911	70.795162
828.621341	38.106488	70.800167
827.924129	42.020324	70.805172
826.979548	44.192417	70.810177
826.326261	36.918017	70.815182
825.525348	42.202306	70.820186
825.531841	35.851023	70.825191
824.866598	41.149966	70.830196
823.916405	38.491308	70.835201
823.246326	46.218976	70.840206
822.241250	47.077951	70.845210
822.176770	33.047004	70.850215
821.205971	38.058828	70.855220
819.868791	44.985417	70.860225
819.450406	40.189462	70.865230
818.896822	44.573670	70.870234
819.234948	40.447038	70.875239
818.396935	29.982222	70.880244
817.423866	42.166415	70.885249
816.191406	37.618845	70.890254
815.078689	44.181740	70.895258
815.362172	39.727775	70.900263
814.923283	43.406717	70.905268
814.560088	34.175366	70.910273
813.252375	34.341747	70.915278
812.602060	41.709205	70.920282
811.921493	41.256612	70.925287
811.219985	43.331023	70.930292
810.042091	43.946064	70.935297
809.747501	39.069303	70.940302
808.848370	44.283581	70.945306
808.618714	32.095043	70.950311
808.085999	47.067076	70.955316
807.834607	36.759525	70.960321
807.254775	41.467949	70.965326
805.760720	41.674146	70.970330
805.423370	30.640443	70.975335
804.942317	31.226117	70.980340
803.845513	47.412608	70.985345
803.224015	38.120507	70.990350
802.337723	45.169987	70.995354
802.101929	42.616713	71.000359
801.474200	46.153539	71.005364
801.189544	53.195882	71.010369
800.568378	37.623405	71.015374
799.740654	46.536962	71.020378
798.631999	45.812717	71.025383
797.849730	47.168766	71.030388
796.928813	49.844811	71.035393
797.012505	48.401617	71.040398
796.014664	54.529206	71.045402
795.402692	40.417970	71.050407
794.470827	45.384055	71.055412
793.539430	43.533718	71.060417
793.138049	46.291681	71.065422
792.684689	46.639337	71.070426
792.605078	45.576991	71.075431
792.105170	43.171191	71.080436
790.892572	42.501857	71.085441
790.230854	41.768158	71.090446
789.264563	53.484647	71.095450
789.013202	49.286102	71.100455
787.637005	49.247917	71.105460
786.907755	49.257589	71.110465
786.424968	42.813285	71.115470
786.155354	46.246929	71.120474
785.897433	41.616902	71.125479
785.932983	43.604927	71.130484
784.923756	48.256257	71.135489
784.139913	50.238202	71.140494
782.589201	47.374540	71.145498
782.092211	45.576103	71.150503
781.342316	44.966057	71.155508
780.623816	46.262635	71.160513
780.190298	39.599510	71.165518
779.726398	48.567978	71.170522
778.883120	37.836848	71.175527
777.901051	45.237455	71.180532
777.246034	38.367155	71.185537
777.098911	36.728250	71.190542
776.392456	40.392240	71.195546
775.968136	40.561248	71.200551
775.014311	41.146993	71.205556
774.361315	44.100418	71.210561
774.097488	40.320832	71.215566
772.798300	48.128638	71.220570
772.144493	45.002401	71.225575
771.452302	42.930314	71.230580
770.855270	39.691332	71.235585
770.628849	33.375610	71.240590
770.100098	40.579754	71.245594
769.088716	41.875190	71.250599
768.541206	42.037671	71.255604
767.897455	45.497117	71.260609
767.091621	32.812449	71.265614
765.915796	39.984155	71.270618
765.212658	34.344930	71.275623
764.883899	38.322359	71.280628
764.442207	40.806191	71.285633
764.296503	41.456391	71.290638
763.080713	42.371209	71.295642
762.309472	35.698444	71.300647
761.585321	35.699748	71.305652
761.670265	43.673850	71.310657
760.632537	41.366498	71.315662
759.362930	43.592307	71.320666
759.082941	33.772402	71.325671
758.279565	44.045530	71.330676
757.412910	45.003168	71.335681
757.730843	36.711800	71.340686
756.059270	43.356228	71.345690
755.753609	36.408721	71.350695
755.031591	46.971450	71.355700
754.364020	43.646664	71.360705
754.216519	34.004580	71.365710
753.047953	42.287746	71.370714
752.566924	34.688214	71.375719
752.141896	37.223662	71.380724
751.444343	43.151006	71.385729
750.516916	44.714286	71.390734
749.479328	48.164625	71.395738
748.778171	40.588984	71.400743
748.715514	39.363086	71.405748
747.859406	45.642443	71.410753
747.621242	46.066128	71.415758
746.029171	48.686240	71.420762
745.711023	47.174126	71.425767
744.974645	42.159117	71.430772
744.856293	51.575207	71.435777
744.446610	39.653554	71.440782
742.982785	41.659229	71.445786
742.469953	39.263149	71.450791
742.177620	40.545935	71.455796
741.803369	44.834300	71.460801
741.009777	35.657744	71.465806
739.606527	41.544934	71.470810
739.440537	41.759292	71.475815
738.969843	40.109900	71.480820
737.554199	47.912400	71.485825
737.082332	37.029637	71.490830
736.287597	38.541374	71.495834
735.970540	41.434491	71.500839
735.567257	39.309366	71.505844
734.997208	39.921345	71.510849
734.109870	32.501151	71.515854
733.212998	39.453374	71.520858
732.837643	48.096427	71.525863
732.226640	42.982973	71.530868
731.043409	41.137109	71.535873
730.284485	34.831301	71.540878
729.676947	39.117000	71.545882
729.381511	42.237716	71.550887
728.755240	37.035701	71.555892
728.508359	35.910439	71.560897
727.961631	37.972158	71.565902
726.543102	40.385713	71.570906
726.133355	37.069658	71.575911
725.752040	34.341200	71.580916
724.880790	46.118771	71.585921
724.160556	32.856588	71.590926
723.234068	37.394678	71.595930
723.100203	35.918889	71.600935
721.852064	38.187210	71.605940
720.833714	37.668160	71.610945
721.122218	35.995681	71.615950
720.515266	36.867390	71.620954
720.104766	32.623491	71.625959
718.796027	39.093276	71.630964
718.072320	37.564595	71.635969
717.747902	34.129719	71.640974
716.963552	38.613067	71.645978
715.787341	34.887162	71.650983
715.358901	45.297367	71.655988
714.590328	36.585453	71.660993
714.411649	33.386123	71.665998
714.102949	42.732583	71.671002
712.794002	37.282408	71.676007
711.663024	40.083656	71.681012
711.208791	45.204363	71.686017
710.870864	38.536716	71.691022
709.879543	39.214551	71.696026
710.069832	36.608423	71.701031
709.015098	30.774853	71.706036
707.907372	36.976533	71.711041
707.371938	35.609800	71.716046
707.395584	42.263418	71.721050
706.499439	29.180187	71.726055
705.494393	35.814647	71.731060
704.677086	39.016477	71.736065
704.314362	31.989550	71.741070
703.534837	38.256183	71.746074
703.303977	33.492460	71.751079
702.179590	37.895122	71.756084
701.007799	41.208994	71.761089
701.000831	33.944288	71.766094
700.320905	45.627508	71.771098
700.255856	39.209151	71.776103
699.064245	41.698701	71.781108
698.290950	45.555721	71.786113
698.089446	39.418095	71.791118
697.473054	40.239716	71.796122
695.933663	34.231428	71.801127
695.284510	42.331284	71.806132
694.750347	36.363932	71.811137
694.665845	35.543993	71.816142
693.850954	38.537397	71.821146
693.295086	34.507867	71.826151
692.601790	43.821140	71.831156
691.543524	45.746695	71.836161
691.615036	41.296280	71.841166
690.263001	46.069113	71.846170
689.375465	36.474872	71.851175
688.884309	36.684546	71.856180
688.243490	39.430641	71.861185
688.227162	36.541375	71.866190
687.136542	43.148660	71.871194
686.248653	44.806620	71.876199
685.429462	43.198780	71.881204
684.790082	45.874370	71.886209
684.719270	37.503558	71.891214
684.131922	41.420296	71.896218
683.773270	38.498101	71.901223
682.982512	36.997885	71.906228
681.944348	40.388731	71.911233
680.788777	35.970128	71.916238
679.953074	38.355291	71.921242
679.180871	45.989941	71.926247
678.989259	42.744672	71.931252
678.531710	44.734675	71.936257
678.229035	37.648122	71.941262
677.935091	45.231231	71.946266
676.653356	42.928599	71.951271
676.115715	35.160762	71.956276
675.277367	45.124510	71.961281
674.418988	37.048483	71.966286
673.397395	39.765082	71.971290
673.056294	36.088345	71.976295
672.658361	37.810780	71.981300
672.307518	37.561047	71.986305
671.809619	41.788102	71.991310
670.850992	40.044688	71.996314
669.775458	36.738892	72.001319
669.726241	33.038202	72.006324
667.939988	43.303283	72.011329
667.448109	34.247549	72.016334
666.903320	38.317250	72.021338
666.563156	45.859728	72.026343
666.375150	44.247172	72.031348
665.765162	53.055154	72.036353
664.997801	46.452397	72.041358
663.972222	42.912661	72.046362
663.360804	33.965428	72.051367
663.059516	41.134948	72.056372
662.005433	45.027840	72.061377
661.294623	36.447746	72.066382
660.712058	47.622473	72.071386
660.522939	48.991390	72.076391
659.498002	39.612922	72.081396
658.271794	42.928232	72.086401
658.000144	40.092182	72.091406
657.441110	41.915635	72.096410
657.126117	39.883150	72.101415
656.079443	36.703064	72.106420
654.852970	43.428755	72.111425
654.314355	23.172323	72.116430
654.009889	37.994320	72.121434
653.281347	37.600098	72.126439
653.142204	40.103152	72.131444
652.478529	46.968859	72.136449
651.400870	39.897851	72.141454
650.757489	41.827329	72.146458
650.497829	41.740387	72.151463
649.160233	38.452653	72.156468
648.531861	41.124782	72.161473
647.934653	45.130050	72.166478
647.282311	48.600454	72.171482
647.001303	39.471489	72.176487
646.693466	44.469228	72.181492
645.622768	48.847312	72.186497
644.996703	43.783425	72.191502
644.432434	40.097164	72.196506
643.309648	38.779359	72.201511
642.627306	40.388690	72.206516
641.750969	40.633572	72.211521
641.254432	35.933528	72.216526
640.891997	50.046691	72.221530
640.769924	43.418251	72.226535
640.008400	33.360357	72.231540
638.648397	49.192104	72.236545
638.165327	40.657859	72.241550
637.711163	47.724107	72.246554
637.194326	38.032819	72.251559
635.816447	42.564579	72.256564
635.466139	43.062347	72.261569
634.973848	35.893425	72.266574
634.879872	45.613203	72.271578
633.811015	44.657193	72.276583
632.938860	40.560287	72.281588
632.473961	35.782986	72.286593
631.930525	26.551764	72.291598
630.814618	36.150586	72.296602
629.899921	46.863955	72.301607
629.525186	39.061111	72.306612
628.722501	49.088224	72.311617
628.488145	41.251065	72.316622
628.215257	41.806223	72.321626
626.875170	33.626041	72.326631
626.281135	44.025932	72.331636
625.586542	43.961800	72.336641
625.150942	43.202806	72.341646
624.714763	44.205917	72.346650
623.722425	40.643524	72.351655
623.465937	34.845704	72.356660
622.652987	45.036406	72.361665
621.470419	35.817189	72.366670
620.428753	39.272984	72.371674
620.319754	47.093602	72.376679
620.096215	35.983592	72.381684
619.301932	44.595001	72.386689
618.620926	41.907637	72.391694
617.389503	36.756431	72.396698
616.789581	42.621272	72.401703
616.580230	37.024180	72.406708
615.891934	45.720846	72.411713
615.369594	35.945249	72.416718
614.259715	41.630239	72.421722
613.483346	40.497023	72.426727
613.243615	40.514031	72.431732
612.643237	40.983597	72.436737
611.997439	39.234754	72.441742
611.070073	30.557181	72.446746
610.276377	37.616864	72.451751
610.059360	45.414147	72.456756
609.465624	47.489064	72.461761
608.451777	31.642896	72.466766
607.616270	45.015704	72.471770
606.734006	42.930029	72.476775
606.702532	39.376292	72.481780
606.067143	37.880653	72.486785
605.166910	34.264197	72.491790
604.411688	47.679302	72.496794
603.832953	42.320750	72.501799
603.413756	40.736757	72.506804
602.692486	47.880347	72.511809
602.141029	34.952419	72.516814
601.267265	43.494162	72.521818
600.712318	41.003480	72.526823
600.295408	29.938056	72.531828
599.075719	37.575567	72.536833
598.124309	39.474937	72.541838
597.537438	43.020963	72.546842
597.019045	39.403030	72.551847
597.054976	37.140303	72.556852
596.379694	40.696346	72.561857
595.394688	37.835296	72.566862
594.699600	43.446064	72.571866
594.084685	43.779972	72.576871
593.723003	37.689933	72.581876
592.503359	33.997162	72.586881
591.529466	31.927980	72.591886
590.969219	38.478352	72.596890
590.204911	38.911669	72.601895
590.470031	35.387638	72.606900
589.770473	34.944252	72.611905
588.771763	32.011741	72.616910
588.186487	33.590632	72.621914
587.643897	32.365264	72.626919
586.536678	31.309660	72.631924
585.632254	31.864873	72.636929
585.081475	36.150726	72.641934
584.255463	44.058666	72.646938
583.945056	43.392298	72.651943
583.667215	38.138110	72.656948
583.159318	41.497327	72.661953
582.564037	34.077655	72.666958
581.289459	40.617796	72.671962
580.566947	42.548605	72.676967
580.297923	32.862239	72.681972
579.440315	39.665260	72.686977
578.706744	37.472408	72.691982
577.966381	36.254876	72.696986
577.659798	39.773405	72.701991
577.331871	39.878943	72.706996
576.071785	37.936558	72.712001
575.363404	35.281129	72.717006
574.671550	36.994723	72.722010
574.394635	35.019271	72.727015
573.863694	33.724807	72.732020
572.903159	37.844829	72.737025
572.273660	27.126478	72.742030
571.640585	35.328575	72.747034
570.842476	35.361130	72.752039
570.030509	34.382434	72.757044
569.137039	35.742570	72.762049
568.989359	36.095104	72.767054
568.702799	32.678625	72.772058
567.679133	35.441779	72.777063
566.571532	31.537987	72.782068
565.810441	38.826943	72.787073
565.405746	33.161492	72.792078
565.086483	36.723638	72.797082
564.567820	35.828496	72.802087
564.034555	33.279635	72.807092
562.765224	42.435047	72.812097
562.509443	36.104249	72.817102
561.814860	35.843162	72.822106
560.571045	45.567330	72.827111
560.034991	37.139281	72.832116
559.163978	45.362812	72.837121
558.948972	41.368050	72.842126
558.511033	45.124601	72.847130
557.945612	43.122008	72.852135
557.119640	39.352320	72.857140
556.339054	40.087625	72.862145
555.973257	40.110053	72.867150
555.281717	41.703209	72.872154
553.908348	50.005318	72.877159
553.741811	39.583406	72.882164
552.644505	41.263850	72.887169
552.748807	39.347809	72.892174
552.333638	38.672553	72.897178
551.143100	39.433499	72.902183
550.332315	35.034010	72.907188
549.792909	35.909559	72.912193
549.510891	38.030933	72.917198
548.184821	42.376214	72.922202
547.285911	36.882678	72.927207
547.355406	31.949881	72.932212
546.574397	40.460735	72.937217
545.540827	32.556466	72.942222
544.968306	32.216444	72.947226
544.088924	28.166982	72.952231
543.750173	27.575734	72.957236
543.083443	33.262955	72.962241
542.956681	26.052342	72.967246
541.803814	26.866436	72.972250
541.067697	37.605651	72.977255
540.783704	27.798709	72.982260
540.350648	32.900791	72.987265
539.050167	22.997644	72.992270
538.344864	36.066705	72.997274
537.478785	44.363204	73.002279
537.362258	34.344415	73.007284
536.598038	40.298593	73.012289
536.125170	45.329347	73.017294
535.221970	40.645712	73.022298
534.658514	39.634703	73.027303
534.434450	37.683354	73.032308
532.953371	41.544833	73.037313
532.255351	29.959597	73.042318
531.579656	33.229943	73.047322
531.321612	40.517965	73.052327
531.048894	34.697675	73.057332
529.513596	35.447046	73.062337
528.937739	33.011666	73.067342
528.324232	40.554006	73.072346
528.010680	38.937709	73.077351
527.540437	25.728276	73.082356
526.592343	32.103935	73.087361
525.810107	33.134379	73.092366
525.620543	28.888963	73.097370
524.678600	31.580887	73.102375
524.368303	25.524292	73.107380
523.412644	39.371607	73.112385
522.725511	31.909665	73.117390
522.269625	31.508216	73.122394
521.288937	35.101992	73.127399
520.375824	23.705585	73.132404
519.291697	36.734959	73.137409
519.202042	29.713768	73.142414
518.695257	40.102260	73.147418
518.230020	39.266648	73.152423
518.059794	28.381987	73.157428
516.869479	38.633011	73.162433
516.111808	38.974812	73.167438
515.511545	41.295185	73.172442
514.173810	32.217062	73.177447
513.700507	36.070458	73.182452
513.071936	36.799457	73.187457
512.853847	34.832481	73.192462
512.259569	31.797137	73.197466
511.819731	34.588938	73.202471
511.221461	29.575973	73.207476
510.118858	37.913789	73.212481
509.372758	31.048105	73.217486
509.112425	38.158501	73.222490
508.344203	36.062779	73.227495
507.396678	34.021464	73.232500
506.493629	43.306348	73.237505
506.272585	40.689784	73.242510
505.658026	39.021258	73.247514
504.270769	45.336001	73.252519
503.796735	40.540153	73.257524
503.099214	51.504857	73.262529
502.593049	37.411100	73.267534
502.476985	43.271585	73.272538
501.929669	40.450813	73.277543
501.148441	41.084005	73.282548
500.106265	46.865962	73.287553
499.454052	42.851786	73.292558
499.213946	42.146142	73.297562
497.813859	35.692506	73.302567
497.394160	38.060487	73.307572
496.398821	40.934058	73.312577
496.536008	34.438042	73.317582
495.956155	40.468783	73.322586
495.164983	44.965168	73.327591
494.149657	30.274628	73.332596
493.353787	37.565207	73.337601
493.018071	30.595655	73.342606
492.512089	38.112465	73.347610
491.573748	43.485072	73.352615
490.936109	41.530388	73.357620
489.977319	36.782874	73.362625
489.858692	32.403732	73.367630
489.076316	38.872574	73.372634
487.844855	35.631438	73.377639
487.710775	40.856756	73.382644
487.038608	34.542848	73.387649
486.723891	36.731007	73.392654
486.245344	42.055219	73.397658
485.144673	35.014258	73.402663
484.638752	34.923343	73.407668
483.639055	38.565381	73.412673
482.455636	34.543559	73.417678
481.623964	36.734255	73.422682
481.379745	45.990321	73.427687
481.058407	35.901247	73.432692
480.644973	42.167535	73.437697
480.199410	38.817386	73.442702
479.050508	32.960941	73.447706
477.982142	36.303317	73.452711
477.386477	31.210968	73.457716
477.105921	45.906891	73.462721
476.660691	34.516756	73.467726
475.911375	35.950095	73.472730
474.720090	40.071387	73.477735
474.226346	27.517271	73.482740
474.077898	43.446926	73.487745
473.613957	37.614019	73.492750
472.465809	45.776896	73.497754
471.908702	44.764807	73.502759
471.565561	37.223797	73.507764
470.801171	35.834358	73.512769
469.792266	37.326786	73.517774
469.016462	34.934756	73.522778
468.354341	36.794444	73.527783
468.118515	35.128125	73.532788
466.773036	42.344742	73.537793
465.915603	35.501697	73.542798
465.410296	38.740090	73.547802
464.902829	36.742579	73.552807
464.752162	36.132920	73.557812
464.050514	36.077916	73.562817
463.805981	32.999619	73.567822
462.869245	38.901660	73.572826
461.489621	37.211490	73.577831
461.722134	31.573827	73.582836
460.135402	39.066246	73.587841
459.521014	38.829325	73.592846
459.048822	34.957194	73.597850
458.467670	45.551053	73.602855
458.381659	37.234578	73.607860
457.796762	37.928864	73.612865
456.815050	41.207847	73.617870
455.687135	38.791294	73.622874
455.155300	44.530800	73.627879
454.967339	34.119288	73.632884
453.547520	41.879142	73.637889
452.885817	39.338491	73.642894
452.687633	38.639086	73.647898
451.686465	40.126639	73.652903
451.687148	37.112105	73.657908
451.210617	41.614178	73.662913
449.936452	42.940105	73.667918
449.921826	39.838199	73.672922
448.731155	41.205868	73.677927
448.030378	36.877939	73.682932
446.899824	37.421011	73.687937
446.639196	40.138688	73.692942
446.338453	36.515846	73.697946
445.558791	29.048860	73.702951
444.832722	35.281489	73.707956
443.939541	31.383222	73.712961
443.946126	38.694572	73.717966
442.937126	36.228042	73.722970
441.469646	43.931334	73.727975
441.414731	32.187760	73.732980
440.418648	38.271674	73.737985
440.031915	34.894082	73.742990
439.623277	33.877869	73.747994
438.499083	32.413524	73.752999
437.881096	23.774956	73.758004
437.236788	25.636331	73.763009
436.585320	30.483362	73.768014
436.249149	22.762759	73.773018
435.599980	30.393705	73.778023
434.722748	31.943701	73.783028
433.837007	39.812154	73.788033
433.591332	34.994157	73.793038
433.111803	22.115928	73.798042
432.532163	32.954242	73.803047
431.731390	30.271648	73.808052
430.896785	31.329237	73.813057
430.361939	35.803805	73.818062
429.925919	45.642968	73.823066
428.081380	34.285024	73.828071
427.810951	31.663510	73.833076
427.280188	38.796171	73.838081
426.933225	39.106285	73.843086
426.734153	35.623119	73.848090
425.916392	38.167472	73.853095
424.955983	29.507458	73.858100
424.251073	34.957298	73.863105
423.704237	37.881119	73.868110
422.759909	38.591219	73.873114
421.824473	42.050555	73.878119
421.673591	38.610048	73.883124
421.117041	41.012144	73.888129
420.536164	35.001140	73.893134
419.955158	34.326292	73.898138
418.552994	39.683663	73.903143
417.977876	33.468790	73.908148
417.502202	36.487778	73.913153
417.190676	34.992715	73.918158
416.668798	33.849078	73.923162
415.302627	40.099834	73.928167
414.780536	33.026450	73.933172
414.127744	26.035859	73.938177
414.032591	37.385192	73.943182
413.404032	37.831981	73.948186
412.171815	39.430581	73.953191
411.749982	27.841467	73.958196
411.148073	43.951451	73.963201
410.367394	40.832020	73.968206
409.369794	31.177784	73.973210
408.450631	44.284687	73.978215
408.009226	26.404035	73.983220
407.765629	37.115688	73.988225
407.632033	31.264073	73.993230
406.687826	35.612625	73.998234
405.418451	39.482066	74.003239
405.241242	30.199576	74.008244
404.284937	37.005713	74.013249
403.927750	35.377564	74.018254
403.162242	36.770665	74.023258
401.824281	35.917271	74.028263
401.743148	31.008321	74.033268
400.978278	32.251715	74.038273
400.594417	35.412066	74.043278
400.320259	33.688377	74.048282
398.958767	38.179491	74.053287
398.418920	31.596231	74.058292
397.926413	33.392914	74.063297
397.796892	29.404045	74.068302
396.900672	34.486830	74.073306
395.811131	35.511146	74.078311
395.216600	31.695121	74.083316
393.930813	38.884944	74.088321
393.345901	28.048871	74.093326
392.709746	32.893677	74.098330
391.925306	36.880133	74.103335
391.986124	29.596338	74.108340
391.373982	39.318451	74.113345
390.946066	30.924405	74.118350
390.677160	32.503963	74.123354
389.274685	37.402737	74.128359
388.814736	31.964269	74.133364
388.303256	35.740930	74.138369
386.908544	37.413565	74.143374
386.339448	29.295148	74.148378
385.362645	34.729225	74.153383
385.540121	31.911355	74.158388
384.925746	36.383767	74.163393
384.335042	48.012231	74.168398
383.480186	36.915724	74.173402
382.641485	38.587803	74.178407
382.178546	28.233694	74.183412
381.113070	41.732755	74.188417
380.118317	35.884261	74.193422
379.906448	33.892940	74.198426
378.956705	41.237137	74.203431
379.127792	37.014392	74.208436
378.136834	40.200241	74.213441
377.102411	37.985174	74.218446
376.733621	35.241977	74.223450
376.027322	30.407409	74.228455
375.808219	33.607020	74.233460
374.685149	32.343013	74.238465
373.863009	31.617528	74.243470
373.507866	25.382335	74.248474
372.768845	37.885237	74.253479
372.510265	36.540569	74.258484
371.471131	37.018652	74.263489
371.140643	30.189529	74.268494
370.184321	27.832009	74.273498
368.656958	34.736415	74.278503
368.318752	29.498126	74.283508
368.004667	28.963055	74.288513
367.429965	36.654661	74.293518
367.477793	27.212434	74.298522
366.176978	37.256640	74.303527
365.329471	28.802676	74.308532
364.887154	30.447874	74.313537
364.431192	30.781410	74.318542
363.557022	27.108837	74.323546
362.203546	32.886139	74.328551
361.938227	25.566669	74.333556
361.565268	27.102881	74.338561
360.662553	30.589378	74.343566
360.752212	20.677777	74.348570
359.224512	35.440190	74.353575
358.332537	25.239351	74.358580
357.872377	37.898133	74.363585
357.561340	30.205204	74.368590
357.327430	27.305875	74.373594
356.466055	32.226386	74.378599
355.784858	26.397186	74.383604
354.924652	32.766094	74.388609
354.126061	25.388424	74.393614
353.814409	29.229911	74.398618
352.363395	40.232175	74.403623
352.003433	29.328349	74.408628
351.318379	31.936410	74.413633
350.721098	36.849554	74.418638
350.506582	35.071834	74.423642
349.950863	33.506925	74.428647
349.039418	37.472919	74.433652
348.132540	40.303726	74.438657
347.603103	37.123881	74.443662
347.556947	30.294186	74.448666
346.050870	36.056991	74.453671
345.332729	33.145528	74.458676
345.048280	35.914260	74.463681
344.511202	34.696662	74.468686
343.985204	28.889414	74.473690
342.715936	37.135825	74.478695
341.907231	27.835268	74.483700
341.782444	33.909594	74.488705
341.135192	34.666288	74.493710
340.688549	30.764535	74.498714
339.185402	36.027922	74.503719
338.698354	36.384156	74.508724
338.223556	29.413992	74.513729
337.740074	39.615736	74.518734
337.445831	25.467950	74.523738
336.469845	35.050328	74.528743
335.707136	24.144093	74.533748
335.324774	31.023964	74.538753
334.771181	30.163256	74.543758
333.975596	32.170958	74.548762
332.650091	39.401151	74.553767
332.029590	42.522726	74.558772
331.764915	29.002991	74.563777
331.287514	32.746184	74.568782
330.847005	28.572608	74.573786
329.576705	39.328391	74.578791
328.844920	25.902138	74.583796
328.606120	31.594185	74.588801
328.113225	35.397662	74.593806
327.195974	30.360458	74.598810
326.003002	36.957709	74.603815
325.458147	30.603466	74.608820
325.427984	38.061622	74.613825
324.797358	36.345353	74.618830
323.965063	39.326792	74.623834
322.732310	43.009197	74.628839
322.261687	29.941184	74.633844
322.174134	38.348593	74.638849
321.657636	32.691684	74.643854
320.811007	28.692315	74.648858
319.780152	36.987467	74.653863
319.337176	33.227974	74.658868
318.810966	37.485162	74.663873
317.904570	39.181485	74.668878
317.137724	26.804471	74.673882
316.474818	30.719976	74.678887
316.201788	27.168580	74.683892
315.216529	35.254614	74.688897
314.163451	32.023217	74.693902
313.891546	30.622814	74.698906
313.068589	33.173600	74.703911
312.860988	32.220043	74.708916
312.117331	34.161220	74.713921
311.096410	36.788960	74.718926
310.677758	32.628613	74.723930
310.069510	41.371568	74.728935
309.878280	33.108274	74.733940
308.891025	35.126333	74.738945
307.834732	38.108273	74.743950
307.863575	35.108259	74.748954
306.313459	45.219681	74.753959
305.767981	35.891775	74.758964
305.173546	37.368062	74.763969
304.524932	39.752397	74.768974
304.117915	37.401789	74.773978
303.810622	40.869924	74.778983
302.973416	34.115028	74.783988
302.037346	32.121925	74.788993
301.138808	37.605360	74.793998
301.187727	28.732127	74.799002
299.620672	34.435926	74.804007
299.332630	37.625645	74.809012
298.676664	47.493426	74.814017
298.173060	37.004992	74.819022
297.963809	31.199511	74.824026
296.519488	38.695981	74.829031
296.246621	33.500578	74.834036
295.544072	33.587849	74.839041
294.969439	37.841892	74.844046
293.804948	31.459656	74.849050
292.905005	41.061769	74.854055
292.427849	35.609292	74.859060
292.148872	35.670146	74.864065
291.314844	35.897184	74.869070
291.507190	24.683589	74.874074
290.418285	40.819012	74.879079
289.305224	33.725371	74.884084
288.560769	40.395352	74.889089
287.904843	43.363145	74.894094
287.855367	35.172656	74.899098
286.624555	45.766164	74.904103
285.794113	34.502488	74.909108
285.093827	34.593320	74.914113
284.671270	43.504570	74.919118
284.442891	34.942138	74.924122
284.030818	29.414171	74.929127
283.002743	34.626933	74.934132
282.412060	35.669184	74.939137
281.821184	40.697282	74.944142
281.312781	35.150300	74.949146
279.888669	30.201169	74.954151
279.272319	39.028007	74.959156
278.580908	39.026536	74.964161
278.173376	45.408258	74.969166
277.977818	41.511630	74.974170
277.169151	39.829832	74.979175
276.240166	39.504366	74.984180
275.893129	35.086237	74.989185
275.115728	38.502720	74.994190
274.394457	35.322217	74.999194
273.156406	50.288417	75.004199
272.775530	32.985940	75.009204
272.217693	43.667771	75.014209
271.798035	38.929345	75.019214
271.341701	36.023544	75.024218
270.191906	43.063380	75.029223
269.681456	40.028705	75.034228
269.024579	36.684806	75.039233
268.523024	48.569157	75.044238
268.274374	38.991839	75.049242
267.026512	42.742369	75.054247
266.303011	37.216075	75.059252
266.200616	37.192193	75.064257
264.792869	46.616105	75.069262
264.062981	38.590397	75.074266
263.354070	32.633341	75.079271
262.896452	33.310571	75.084276
262.777098	39.095428	75.089281
261.862326	38.362159	75.094286
261.192175	32.719756	75.099290
260.459857	45.883847	75.104295
260.032121	35.302686	75.109300
259.390288	36.808416	75.114305
257.796981	43.076037	75.119310
257.531637	35.076491	75.124314
256.972424	40.217182	75.129319
256.446391	42.564329	75.134324
256.106542	41.271096	75.139329
255.523257	41.025318	75.144334
254.782927	37.011688	75.149338
253.921232	42.858267	75.154343
253.185202	33.623427	75.159348
251.811502	31.396683	75.164353
251.368425	36.553385	75.169358
251.211545	29.274943	75.174362
250.684994	41.415794	75.179367
250.199106	38.142847	75.184372
249.698328	34.656150	75.189377
248.323442	37.314576	75.194382
248.224810	31.766043	75.199386
247.470440	40.250248	75.204391
246.798581	33.590175	75.209396
246.133848	29.610957	75.214401
245.116270	36.737862	75.219406
244.991668	33.170108	75.224410
243.696169	33.487306	75.229415
242.859107	36.256823	75.234420
242.131633	36.902551	75.239425
241.356794	41.797985	75.244430
241.524348	29.415949	75.249434
240.333970	39.060744	75.254439
240.070168	40.314191	75.259444
239.981292	33.783913	75.264449
238.571989	40.751401	75.269454
238.591109	36.908369	75.274458
237.134126	31.132438	75.279463
236.158087	35.704747	75.284468
235.624824	34.668472	75.289473
234.741397	34.614268	75.294478
234.608314	28.190644	75.299482
234.065794	39.743346	75.304487
233.451862	33.922769	75.309492
233.371442	28.697939	75.314497
232.726251	43.461073	75.319502
231.390522	32.059831	75.324506
230.684836	32.322507	75.329511
229.659184	41.075833	75.334516
228.957205	40.865403	75.339521
227.943826	43.545943	75.344526
228.069074	36.229008	75.349530
227.763545	41.874867	75.354535
227.385097	42.216444	75.359540
226.746905	34.540929	75.364545
225.496125	49.256304	75.369550
225.192587	37.940613	75.374554
223.777455	43.175131	75.379559
223.040350	38.008393	75.384564
222.543639	40.506033	75.389569
222.265844	41.832138	75.394574
221.927093	36.089122	75.399578
220.741670	45.966351	75.404583
220.115753	33.359558	75.409588
219.594738	40.780275	75.414593
218.572745	40.078024	75.419598
218.786133	34.071033	75.424602
217.242414	36.647494	75.429607
216.405404	43.538993	75.434612
216.235427	37.551138	75.439617
215.404037	44.273921	75.444622
215.440760	40.216700	75.449626
214.160764	46.721926	75.454631
213.391812	43.846825	75.459636
212.916566	45.293614	75.464641
212.246845	43.936542	75.469646
211.582498	36.205912	75.474650
210.554293	37.289224	75.479655
209.917187	41.851597	75.484660
209.406686	34.511412	75.489665
208.963585	41.951930	75.494670
208.938956	40.730186	75.499674
208.110438	42.351603	75.504679
207.634665	39.007064	75.509684
206.534696	33.565447	75.514689
205.188652	44.512251	75.519694
204.560317	36.457705	75.524698
203.987446	39.616914	75.529703
203.713636	41.364679	75.534708
203.294259	39.819047	75.539713
202.486837	43.832756	75.544718
201.501618	33.744647	75.549722
201.038363	35.994200	75.554727
200.443979	45.790641	75.559732
199.429893	45.785681	75.564737
198.304290	53.607656	75.569742
197.708515	34.258740	75.574746
197.527621	42.755164	75.579751
197.241413	41.336301	75.584756
196.914735	36.776541	75.589761
196.163971	47.508024	75.594766
195.233033	35.562170	75.599770
194.315267	40.545658	75.604775
193.764918	33.362693	75.609780
193.379415	28.151482	75.614785
192.266921	41.343241	75.619790
191.957790	36.828234	75.624794
190.885751	40.207215	75.629799
190.598860	37.433815	75.634804
189.518347	37.952582	75.639809
188.638408	38.258951	75.644814
188.533726	34.874484	75.649818
187.781503	30.875540	75.654823
187.546389	40.409483	75.659828
187.301511	35.076670	75.664833
185.499571	48.365702	75.669838
184.932192	37.847964	75.674842
184.424109	39.141315	75.679847
183.658649	36.144840	75.684852
182.743548	34.136722	75.689857
181.951899	36.682161	75.694862
181.407910	36.275719	75.699866
181.020543	36.014523	75.704871
180.659559	35.382116	75.709876
180.229917	27.349964	75.714881
179.546700	32.202065	75.719886
178.721177	40.400069	75.724890
177.951849	50.196504	75.729895
177.541927	34.581298	75.734900
176.840037	31.508801	75.739905
175.615268	34.447020	75.744910
175.239480	30.610113	75.749914
174.646850	32.750800	75.754919
174.075043	33.967054	75.759924
173.136637	32.395144	75.764929
172.383452	37.490148	75.769934
172.258312	33.856180	75.774938
171.311650	40.318875	75.779943
170.751003	42.758799	75.784948
170.286609	35.633731	75.789953
169.135503	44.385678	75.794958
169.106173	37.470221	75.799962
167.743221	36.478690	75.804967
166.781411	34.026242	75.809972
166.451553	39.664430	75.814977
165.819111	41.091199	75.819982
165.559217	37.074171	75.824986
165.311379	38.197392	75.829991
164.259885	49.813274	75.834996
163.506656	42.367082	75.840001
162.669725	41.513127	75.845006
161.887736	30.362757	75.850010
160.794560	33.664450	75.855015
160.050351	32.133458	75.860020
160.100918	36.740963	75.865025
159.558795	38.421049	75.870030
159.130478	31.186780	75.875034
158.363629	35.753634	75.880039
157.712469	30.478633	75.885044
156.854584	30.797015	75.890049
156.268505	39.778528	75.895054
155.727624	31.900438	75.900058
154.648121	39.873974	75.905063
154.027704	36.772514	75.910068
153.721415	26.772104	75.915073
152.575425	38.679293	75.920078
151.987549	28.924510	75.925082
151.134869	34.865073	75.930087
150.541651	41.387568	75.935092
150.334816	35.561163	75.940097
149.843889	37.943350	75.945102
148.815049	30.444158	75.950106
147.852439	39.784675	75.955111
147.256640	37.891553	75.960116
146.852039	34.363516	75.965121
146.055245	35.814120	75.970126
145.918995	30.928452	75.975130
144.962912	32.166378	75.980135
144.219575	37.111285	75.985140
143.829370	35.665257	75.990145
142.480311	39.089368	75.995150
141.732232	29.435468	76.000154
141.241680	39.462380	76.005159
140.659227	38.701375	76.010164
140.343685	37.307675	76.015169
139.463262	34.556694	76.020174
139.359525	31.391135	76.025178
138.050266	29.863862	76.030183
137.371808	35.931261	76.035188
136.917813	32.423141	76.040193
136.558658	38.776044	76.045198
135.604754	35.186660	76.050202
134.630601	37.442097	76.055207
133.702600	34.053524	76.060212
133.690517	29.386951	76.065217
133.006352	40.920911	76.070222
132.691215	32.204044	76.075226
131.924186	38.343862	76.080231
130.956614	37.230485	76.085236
130.716743	31.967475	76.090241
129.773973	33.836634	76.095246
128.541791	35.847772	76.100250
128.017467	37.316006	76.105255
127.088896	43.017759	76.110260
126.911451	35.658780	76.115265
126.511454	36.928475	76.120270
126.488289	32.064077	76.125274
125.074368	40.366905	76.130279
124.435412	39.389418	76.135284
123.952404	28.442789	76.140289
123.192105	34.059642	76.145294
122.062699	27.233318	76.150298
121.314333	34.816161	76.155303
120.751132	41.689542	76.160308
120.719129	33.389109	76.165313
120.046270	37.005965	76.170318
119.491474	45.414523	76.175322
118.692036	44.010630	76.180327
118.060242	38.949010	76.185332
117.199948	31.675917	76.190337
116.043309	33.313734	76.195342
115.682264	34.901995	76.200346
114.990525	37.023761	76.205351
115.013882	38.282454	76.210356
113.920723	32.710627	76.215361
112.629887	34.013052	76.220366
112.553569	36.286271	76.225370
111.980725	36.817489	76.230375
111.310751	29.062983	76.235380
110.487488	37.209686	76.240385
109.910243	33.843086	76.245390
109.167097	26.705430	76.250394
108.894145	38.435717	76.255399
108.053516	38.456300	76.260404
107.289496	32.348472	76.265409
106.445288	44.374450	76.270414
106.083966	29.103413	76.275418
105.010962	34.586785	76.280423
103.908415	36.122574	76.285428
103.615628	31.124018	76.290433
103.235744	38.698952	76.295438
103.057205	31.754613	76.300442
102.180892	37.486880	76.305447
101.082405	39.149072	76.310452
100.581298	35.372339	76.315457
99.763721	37.544890	76.320462
99.861831	29.704492	76.325466
98.359207	29.146639	76.330471
97.021749	33.957369	76.335476
97.030923	32.023692	76.340481
96.298342	37.166485	76.345486
96.062646	28.696517	76.350490
95.820162	35.958964	76.355495
95.141638	26.189738	76.360500
94.508101	34.157477	76.365505
93.457959	38.119264	76.370510
92.427850	31.130275	76.375514
91.591131	34.320123	76.380519
90.853834	40.554711	76.385524
90.753192	28.576675	76.390529
89.837120	38.558125	76.395534
89.945095	29.863852	76.400538
89.138157	33.780392	76.405543
87.780846	42.180490	76.410548
87.278765	32.405880	76.415553
86.437164	35.981016	76.420558
86.642468	31.084556	76.425562
85.381575	39.886913	76.430567
84.312715	31.912657	76.435572
83.971550	32.484286	76.440577
83.464709	32.663160	76.445582
82.710325	28.945248	76.450586
82.317893	34.288656	76.455591
81.188701	37.958491	76.460596
80.659722	24.583988	76.465601
79.809132	37.339693	76.470606
79.649708	35.440447	76.475610
78.778955	31.966288	76.480615
78.478846	38.446823	76.485620
77.844109	33.581890	76.490625
76.755468	29.693142	76.495630
76.328142	27.679181	76.500634
75.177257	32.389248	76.505639
74.086880	32.439235	76.510644
74.149834	28.172670	76.515649
73.614928	34.706089	76.520654
73.325078	37.032889	76.525658
72.833430	33.627147	76.530663
71.399420	39.540686	76.535668
71.036559	26.715956	76.540673
70.258818	37.159581	76.545678
69.397296	35.794367	76.550682
68.472424	35.084973	76.555687
68.074555	28.365731	76.560692
67.919429	28.303134	76.565697
67.362813	36.355970	76.570702
66.543211	30.138085	76.575706
65.733652	35.145666	76.580711
65.178330	36.121884	76.585716
64.639719	30.365397	76.590721
63.057866	36.719126	76.595726
62.498880	34.286450	76.600730
61.937283	41.900828	76.605735
61.475307	40.852352	76.610740
61.261736	27.452195	76.615745
60.585160	35.606908	76.620750
59.939234	39.783987	76.625754
59.224100	32.507336	76.630759
58.517825	43.055547	76.635764
57.484729	33.217652	76.640769
56.264931	43.199080	76.645774
55.726777	27.980873	76.650778
55.353021	32.676910	76.655783
54.705075	32.734331	76.660788
54.944514	28.611576	76.665793
54.422601	38.139028	76.670798
53.677349	34.074182	76.675802
52.771239	27.334719	76.680807
51.583194	35.235698	76.685812
50.652192	21.049530	76.690817
49.926165	28.253175	76.695822
49.472396	25.071851	76.700826
49.254737	27.500345	76.705831
48.318914	35.536491	76.710836
48.171750	33.850263	76.715841
47.509375	40.110296	76.720846
46.779118	40.447472	76.725850
45.844900	32.613555	76.730855
44.938867	38.637486	76.735860
44.351754	35.015236	76.740865
43.512239	41.511680	76.745870
43.014972	31.850721	76.750874
42.454041	35.347349	76.755879
41.671443	36.683042	76.760884
41.534523	31.659349	76.765889
40.298871	37.956490	76.770894
39.615285	31.703844	76.775898
39.364232	30.921952	76.780903
38.776640	37.826753	76.785908
37.684189	22.622677	76.790913
37.284637	28.174923	76.795918
36.678862	21.790527	76.800922
36.664375	27.507658	76.805927
35.378785	28.142142	76.810932
34.584845	22.360366	76.815937
33.508762	29.815071	76.820942
33.579628	28.117514	76.825946
32.489399	30.902444	76.830951
31.337934	37.574733	76.835956
31.001647	25.465807	76.840961
30.419136	24.393399	76.845966
30.094235	28.035468	76.850970
29.906170	25.708533	76.855975
28.503928	29.361249	76.860980
28.243596	26.322409	76.865985
27.230561	36.344170	76.870990
26.384531	29.291274	76.875994
25.546555	30.704355	76.880999
24.583748	30.162123	76.886004
24.738385	26.317181	76.891009
23.886860	35.296841	76.896014
23.748654	29.519076	76.901018
23.116171	26.671930	76.906023
21.689114	35.167675	76.911028
20.675751	21.556524	76.916033
20.393561	35.317204	76.921038
20.276717	28.572679	76.926042
19.682087	24.453599	76.931047
18.730867	33.475614	76.936052
18.047880	35.415508	76.941057
17.576652	42.636655	76.946062
17.274527	37.273810	76.951066
16.255618	30.343710	76.956071
14.999150	34.976373	76.961076
14.756270	35.000267	76.966081
14.385421	40.389317	76.971086
13.251743	41.756397	76.976090
12.497956	33.114759	76.981095
11.270290	42.203126	76.986100
11.311657	32.329827	76.991105
10.849317	39.245915	76.996110
10.519160	36.970973	77.001114
9.875008	37.782834	77.006119
8.533925	40.952601	77.011124
7.951659	29.213068	77.016129
7.528437	31.331436	77.021134
7.168705	34.315574	77.026139
6.002020	34.191567	77.031143
5.175060	33.478819	77.036148
4.691705	32.859516	77.041153
4.321383	39.405375	77.046158