Tue Jun 08 17:36:27 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.027013	96.527453	0.000000
-1.389698	72.579680	0.005005
-2.463605	54.869948	0.010010
-4.957820	16.969582	0.015014
-9.143402	14.798374	0.020019
-14.189084	22.076400	0.025024
-18.530120	17.507936	0.030029
-23.261509	10.162918	0.035034
-26.784774	13.764479	0.040038
-30.750343	15.773837	0.045043
-34.512134	23.313283	0.050048
-37.988188	13.691848	0.055053
-41.959611	19.839576	0.060058
-45.286983	9.317976	0.065062
-49.279888	9.844769	0.070067
-52.965873	20.331951	0.075072
-56.702972	13.927188	0.080077
-60.740610	25.801301	0.085082
-64.523035	12.287686	0.090086
-67.890024	12.509810	0.095091
-71.777004	14.380604	0.100096
-75.011265	10.289078	0.105101
-79.217037	16.001790	0.110106
-83.283018	17.194784	0.115110
-87.075380	10.207461	0.120115
-90.640133	13.986304	0.125120
-94.429860	7.575209	0.130125
-98.635235	10.044535	0.135130
-102.120085	5.637606	0.140134
-105.563807	9.604110	0.145139
-109.502261	15.856362	0.150144
-113.214450	9.745386	0.155149
-117.078091	17.018165	0.160154
-120.630265	11.802982	0.165158
-124.307949	18.751003	0.170163
-128.433232	15.238999	0.175168
-131.960278	10.552770	0.180173
-135.719342	7.394785	0.185178
-139.515899	2.603215	0.190182
-143.892220	10.535473	0.195187
-147.725243	14.866778	0.200192
-151.318252	8.324900	0.205197
-154.907329	19.298393	0.210202
-158.346430	14.510661	0.215206
-162.476190	15.504677	0.220211
-166.186784	19.278985	0.225216
-169.816247	17.200436	0.230221
-173.565773	21.649671	0.235226
-176.771391	23.627106	0.240230
-180.975630	19.598991	0.245235
-184.652274	17.493417	0.250240
-188.319332	14.102607	0.255245
-192.670111	17.537944	0.260250
-195.682049	17.580462	0.265254
-199.402485	12.564323	0.270259
-203.567372	21.097043	0.275264
-207.115242	14.961914	0.280269
-211.396760	18.788784	0.285274
-214.971557	13.073120	0.290278
-218.354928	20.845016	0.295283
-222.349525	14.850067	0.300288
-225.979394	12.157467	0.305293
-229.888367	17.281021	0.310298
-233.488946	15.551627	0.315302
-237.460269	25.207678	0.320307
-241.393520	20.337408	0.325312
-245.345538	16.693568	0.330317
-249.069561	19.393476	0.335322
-252.350418	7.828357	0.340326
-256.233682	16.170325	0.345331
-259.893528	17.135933	0.350336
-263.465691	14.248742	0.355341
-267.716715	28.380250	0.360346
-271.421780	8.692945	0.365350
-275.211559	22.028152	0.370355
-279.430200	26.390973	0.375360
-282.555087	10.427322	0.380365
-286.401087	9.237007	0.385370
-289.808489	7.440974	0.390374
-293.792970	24.470522	0.395379
-297.606027	10.680966	0.400384
-300.974736	13.106825	0.405389
-305.583920	17.081952	0.410394
-309.179166	9.378965	0.415398
-312.708124	19.966885	0.420403
-316.530616	19.198848	0.425408
-319.901336	14.370310	0.430413
-324.229721	19.812578	0.435418
-327.501260	13.273335	0.440422
-331.593826	7.275958	0.445427
-335.494682	19.755585	0.450432
-338.516879	14.233769	0.455437
-342.858965	21.974428	0.460442
-346.644244	13.159413	0.465446
-350.223419	11.830626	0.470451
-353.930007	10.929459	0.475456
-357.853271	23.298483	0.480461
-361.962040	19.307849	0.485466
-365.402998	12.963083	0.490470
-369.317410	12.639120	0.495475
-373.341790	9.046100	0.500480
-376.147209	13.264857	0.505485
-380.351534	16.987855	0.510490
-383.844057	16.794412	0.515494
-387.781713	12.707351	0.520499
-392.029663	17.137663	0.525504
-395.615265	11.023380	0.530509
-399.389728	22.437368	0.535514
-402.999266	11.924613	0.540518
-406.455259	13.008120	0.545523
-410.338005	17.906285	0.550528
-414.013538	15.079187	0.555533
-418.125318	18.676220	0.560538
-421.826599	15.179383	0.565542
-425.539317	11.881473	0.570547
-429.407170	9.575243	0.575552
-432.999294	8.793049	0.580557
-436.531326	12.601272	0.585562
-440.393690	11.303775	0.590566
-444.385267	13.602536	0.595571
-448.322744	13.298784	0.600576
-451.692045	7.420186	0.605581
-455.693331	20.680104	0.610586
-459.510265	7.753818	0.615590
-463.193604	10.389290	0.620595
-467.134207	13.250469	0.625600
-470.566391	8.353264	0.630605
-474.644252	17.897521	0.635610
-478.286654	18.735585	0.640614
-481.817630	15.350098	0.645619
-485.893234	8.153206	0.650624
-489.214828	12.889242	0.655629
-493.104266	14.837388	0.660634
-496.973226	17.513025	0.665638
-500.904406	15.593486	0.670643
-505.181178	18.500930	0.675648
-508.139761	12.522700	0.680653
-512.030170	18.840057	0.685658
-515.705704	12.982476	0.690662
-519.381470	11.112678	0.695667
-523.317709	16.373378	0.700672
-527.053665	11.438346	0.705677
-531.134545	14.213131	0.710682
-534.735486	8.677877	0.715686
-538.823254	13.231616	0.720691
-542.411433	18.622467	0.725696
-545.588136	10.484744	0.730701
-549.829053	15.378564	0.735706
-553.478774	12.208894	0.740710
-557.154464	14.985225	0.745715
-560.875999	16.473598	0.750720
-564.498992	10.200892	0.755725
-568.646590	17.756812	0.760730
-572.356270	19.864037	0.765734
-576.402713	20.008144	0.770739
-579.929880	19.077960	0.775744
-583.439647	15.837329	0.780749
-587.346997	18.538970	0.785754
-590.940352	8.762115	0.790758
-594.643813	22.620724	0.795763
-598.642511	18.581041	0.800768
-602.300632	6.447458	0.805773
-606.551219	17.947637	0.810778
-610.012802	7.011034	0.815782
-613.738945	9.916059	0.820787
-617.244216	15.295897	0.825792
-621.011936	11.231206	0.830797
-625.286695	19.225018	0.835802
-628.720389	20.869697	0.840806
-632.448727	19.113219	0.845811
-636.226136	16.844940	0.850816
-639.906600	13.643912	0.855821
-643.895560	20.417204	0.860826
-647.657356	15.943391	0.865830
-650.914156	14.131666	0.870835
-654.631467	14.284097	0.875840
-658.478118	7.930261	0.880845
-662.801989	12.341087	0.885850
-666.606048	13.523208	0.890854
-670.100453	13.684763	0.895859
-674.046300	13.330548	0.900864
-677.417737	13.719278	0.905869
-681.360089	16.306621	0.910874
-685.047823	17.329857	0.915878
-688.664254	15.393183	0.920883
-692.480284	16.783813	0.925888
-696.385006	5.956891	0.930893
-700.628039	15.044189	0.935898
-704.075280	12.763121	0.940902
-707.245438	11.795060	0.945907
-711.239724	13.441281	0.950912
-715.058651	9.157718	0.955917
-719.189336	15.224396	0.960922
-722.990312	18.145118	0.965926
-727.043862	20.537259	0.970931
-730.360893	19.204056	0.975936
-733.521250	14.347647	0.980941
-737.851441	11.820279	0.985946
-741.300878	14.668840	0.990950
-745.248901	19.202332	0.995955
-749.169547	21.300914	1.000960
-752.541015	6.177708	1.005965
-756.485180	9.734039	1.010970
-760.542992	9.612657	1.015974
-763.860915	10.322638	1.020979
-768.008615	12.114443	1.025984
-771.508990	13.375969	1.030989
-775.347155	19.291841	1.035994
-779.129844	7.920675	1.040998
-783.123734	6.471995	1.046003
-787.132957	11.185353	1.051008
-790.435523	7.919203	1.056013
-794.279915	13.728403	1.061018
-797.999889	13.825364	1.066022
-801.747189	12.416080	1.071027
-805.497957	15.113532	1.076032
-809.012530	12.943179	1.081037
-813.141456	16.363128	1.086042
-816.313401	23.159739	1.091046
-820.397923	14.081566	1.096051
-824.703273	15.905220	1.101056
-828.189754	16.409727	1.106061
-831.883561	15.298369	1.111066
-835.731801	17.871668	1.116070
-839.363454	21.642437	1.121075
-843.148529	19.283297	1.126080
-846.536640	7.730004	1.131085
-850.685209	17.147377	1.136090
-854.302391	16.059989	1.141094
-858.314723	21.389689	1.146099
-861.894647	18.594329	1.151104
-865.768736	13.586218	1.156109
-869.542175	10.760931	1.161114
-872.888209	12.429038	1.166118
-876.568098	9.581778	1.171123
-880.518520	23.248920	1.176128
-884.232938	16.897069	1.181133
-888.664784	12.799795	1.186138
-891.916376	9.278284	1.191142
-895.848998	19.150037	1.196147
-899.818624	13.545380	1.201152
-903.465327	7.517428	1.206157
-907.349313	20.251937	1.211162
-910.694899	15.069861	1.216166
-914.076134	16.219476	1.221171
-918.101193	17.858142	1.226176
-922.015816	20.829330	1.231181
-925.976758	22.449102	1.236186
-929.400250	17.063326	1.241190
-933.322726	11.953464	1.246195
-937.342144	13.397773	1.251200
-940.863489	6.293285	1.256205
-944.834156	22.694134	1.261210
-948.646951	12.797797	1.266214
-952.186681	18.308134	1.271219
-955.939351	17.573672	1.276224
-959.642088	6.282903	1.281229
-963.726131	25.404208	1.286234
-967.387289	16.344682	1.291238
-970.749607	14.473169	1.296243
-974.636980	15.939445	1.301248
-978.407317	7.082218	1.306253
-982.299625	20.120559	1.311258
-986.059102	16.408048	1.316262
-989.647219	14.611234	1.321267
-993.600879	7.973353	1.326272
-997.278397	13.245294	1.331277
-1001.251091	22.987842	1.336282
-1004.941276	21.284347	1.341286
-1008.732932	19.033453	1.346291
-1012.540262	28.247529	1.351296
-1016.000474	17.227380	1.356301
-1019.872613	21.105895	1.361306
-1023.483549	9.474187	1.366310
-1027.575143	21.412394	1.371315
-1031.291994	27.897343	1.376320
-1034.774421	16.118455	1.381325
-1038.756612	22.834478	1.386330
-1042.324197	12.677465	1.391334
-1046.031616	9.514582	1.396339
-1050.133686	16.527095	1.401344
-1053.758751	10.440306	1.406349
-1057.798211	23.142817	1.411354
-1061.457551	17.682790	1.416358
-1064.936825	14.826907	1.421363
-1068.801643	12.856242	1.426368
-1072.302933	18.449275	1.431373
-1076.366671	22.478754	1.436378
-1080.399956	18.071297	1.441382
-1083.560740	16.984285	1.446387
-1087.447683	14.194474	1.451392
-1091.017233	11.162289	1.456397
-1095.084712	23.151671	1.461402
-1099.105906	17.668556	1.466406
-1102.807100	22.605993	1.471411
-1106.707191	21.336102	1.476416
-1109.639000	11.680198	1.481421
-1113.769216	8.696942	1.486426
-1117.771371	11.649782	1.491430
-1121.409706	12.342431	1.496435
-1125.499232	14.970440	1.501440
-1128.847890	0.158263	1.506445
-1132.932650	15.887315	1.511450
-1136.882132	8.776791	1.516454
-1139.991900	9.345141	1.521459
-1144.110239	16.247251	1.526464
-1147.523458	13.622840	1.531469
-1151.909563	18.388217	1.536474
-1155.424867	15.769896	1.541478
-1159.208946	7.618967	1.546483
-1162.981409	10.945266	1.551488
-1166.262528	14.880689	1.556493
-1170.545096	23.201181	1.561498
-1173.892275	18.679546	1.566502
-1177.532158	9.928786	1.571507
-1181.668769	17.001027	1.576512
-1185.505821	12.429725	1.581517
-1189.204588	17.598902	1.586522
-1192.985169	9.784878	1.591526
-1196.453009	13.230984	1.596531
-1200.321810	19.447316	1.601536
-1204.190147	11.107626	1.606541
-1208.001182	11.166508	1.611546
-1211.671090	15.988932	1.616550
-1215.581716	13.303961	1.621555
-1219.716971	10.875448	1.626560
-1222.739929	11.712348	1.631565
-1226.652861	11.968732	1.636570
-1230.450159	2.182515	1.641574
-1234.253767	9.084725	1.646579
-1238.209474	20.202465	1.651584
-1241.974434	10.788828	1.656589
-1246.012518	26.828491	1.661594
-1249.384163	12.442700	1.666598
-1252.795306	9.050320	1.671603
-1256.832203	20.835257	1.676608
-1260.218477	8.608663	1.681613
-1264.128248	11.159749	1.686618
-1267.992987	10.469680	1.691622
-1272.044385	14.597473	1.696627
-1276.095273	21.601004	1.701632
-1280.016682	14.708021	1.706637
-1283.200990	11.876659	1.711642
-1287.025509	21.811475	1.716646
-1290.479089	11.127134	1.721651
-1294.310614	10.641369	1.726656
-1297.911411	7.130036	1.731661
-1302.113785	3.410611	1.736666
-1305.924896	4.191115	1.741670
-1309.230889	12.343994	1.746675
-1313.330906	11.923308	1.751680
-1316.942734	2.565548	1.756685
-1321.049205	14.125660	1.761690
-1324.537673	21.173147	1.766694
-1327.985715	9.344037	1.771699
-1332.239601	19.075950	1.776704
-1335.785935	13.436913	1.781709
-1339.587109	9.887804	1.786714
-1343.270774	12.395782	1.791718
-1346.865511	15.008084	1.796723
-1350.840922	18.813450	1.801728
-1354.019319	3.089286	1.806733
-1358.396318	15.484520	1.811738
-1362.160268	12.253090	1.816742
-1365.807774	1.731996	1.821747
-1369.674647	12.383038	1.826752
-1373.322547	1.445607	1.831757
-1377.340867	4.853003	1.836762
-1381.314088	9.012462	1.841766
-1385.282389	3.957891	1.846771
-1388.759778	11.870289	1.851776
-1392.224411	9.462532	1.856781
-1395.803301	16.705194	1.861786
-1399.612075	21.084693	1.866790
-1403.125412	16.593375	1.871795
-1407.512598	21.653642	1.876800
-1410.846184	11.223122	1.881805
-1414.923837	15.105315	1.886810
-1418.704956	7.481460	1.891814
-1421.997617	12.882224	1.896819
-1426.155348	14.351146	1.901824
-1429.612578	15.275822	1.906829
-1433.896494	28.810444	1.911834
-1437.745791	16.875905	1.916838
-1440.943067	8.848246	1.921843
-1444.969513	19.487691	1.926848
-1448.541024	11.913505	1.931853
-1452.384581	19.435346	1.936858
-1456.265456	16.958635	1.941862
-1459.561796	14.485710	1.946867
-1463.720815	13.652581	1.951872
-1467.355481	5.245389	1.956877
-1471.568849	16.265491	1.961882
-1475.492136	15.889202	1.966886
-1478.927146	10.142759	1.971891
-1482.484521	20.385886	1.976896
-1485.777438	5.598812	1.981901
-1489.549967	9.695077	1.986906
-1493.683673	6.914503	1.991910
-1497.387276	14.465224	1.996915
-1501.822900	14.463527	2.006912
-1502.776553	12.350967	2.016909
-1499.866626	13.595877	2.026906
-1496.954770	8.501695	2.036902
-1494.662657	5.488455	2.046899
-1493.192668	13.019161	2.056896
-1491.357911	13.637035	2.066893
-1489.251785	13.151103	2.076890
-1487.453836	6.034732	2.086886
-1485.527592	5.132725	2.096883
-1483.383615	9.395847	2.106880
-1481.714138	7.265379	2.116877
-1479.756513	8.190964	2.126874
-1477.917975	8.397177	2.136870
-1476.065403	10.893590	2.146867
-1473.975250	2.170690	2.156864
-1472.314110	5.825152	2.166861
-1470.202045	4.664377	2.176858
-1468.580310	8.955180	2.186854
-1466.318678	1.237087	2.196851
-1464.581789	3.413498	2.206848
-1462.916695	9.173357	2.216845
-1460.923891	4.508598	2.226842
-1458.898190	13.939262	2.236838
-1457.040929	12.842819	2.246835
-1455.301807	10.832792	2.256832
-1453.149315	8.525296	2.266829
-1451.614290	9.654309	2.276826
-1449.595950	7.205850	2.286822
-1447.720595	13.191619	2.296819
-1445.697426	8.269901	2.306816
-1443.702163	10.056917	2.316813
-1442.149053	10.310204	2.326810
-1440.228069	3.888044	2.336806
-1438.173444	9.313439	2.346803
-1436.344721	7.301465	2.356800
-1434.314871	9.641370	2.366797
-1432.809432	10.718168	2.376794
-1430.779195	12.538704	2.386790
-1428.615544	6.855004	2.396787
-1427.181175	10.123988	2.406784
-1425.088221	13.374688	2.416781
-1423.388218	12.329382	2.426778
-1421.453779	4.619300	2.436774
-1419.385594	12.756282	2.446771
-1417.193370	10.119092	2.456768
-1415.953584	13.263820	2.466765
-1413.829234	7.961141	2.476762
-1411.880456	12.087501	2.486758
-1410.205544	12.062595	2.496755
-1408.030062	16.853883	2.506752
-1406.334361	17.192557	2.516749
-1404.646487	10.653949	2.526746
-1402.510969	11.232054	2.536742
-1400.095926	7.174944	2.546739
-1398.628175	5.726910	2.556736
-1396.934091	9.301447	2.566733
-1395.202472	7.870530	2.576730
-1392.933939	6.194832	2.586726
-1391.326610	8.044561	2.596723
-1389.297651	6.864905	2.606720
-1387.660723	6.859575	2.616717
-1385.624618	10.189222	2.626714
-1383.727943	6.625069	2.636710
-1381.944500	8.629903	2.646707
-1380.098046	12.838276	2.656704
-1378.185254	9.763788	2.666701
-1376.272883	8.949578	2.676698
-1374.136302	6.576483	2.686694
-1372.320862	12.743314	2.696691
-1370.722169	10.175694	2.706688
-1368.766594	8.606725	2.716685
-1366.847360	9.650012	2.726682
-1364.805197	3.242240	2.736678
-1362.900862	3.710292	2.746675
-1361.393730	7.362012	2.756672
-1359.444965	6.102085	2.766669
-1357.591088	6.768507	2.776666
-1355.556608	12.814728	2.786662
-1353.570731	4.102674	2.796659
-1351.961811	5.089007	2.806656
-1349.969169	7.508066	2.816653
-1347.900801	11.027425	2.826650
-1346.366468	7.397479	2.836646
-1344.235556	10.391533	2.846643
-1342.379393	11.039785	2.856640
-1340.587873	5.950418	2.866637
-1338.485435	10.842422	2.876634
-1336.733770	7.980981	2.886630
-1334.873298	6.365524	2.896627
-1333.242629	10.948098	2.906624
-1331.265666	14.564185	2.916621
-1329.275746	15.129793	2.926618
-1327.490515	8.014081	2.936614
-1325.369618	10.329709	2.946611
-1323.750819	10.451614	2.956608
-1321.754577	13.350645	2.966605
-1319.888355	16.009986	2.976602
-1317.993959	10.062738	2.986598
-1316.172370	12.956992	2.996595
-1313.864343	11.344108	3.006592
-1312.152142	9.493289	3.016589
-1310.479675	7.094816	3.026586
-1309.326831	13.379834	3.036582
-1306.943212	11.299083	3.046579
-1304.490652	11.101525	3.056576
-1303.106307	5.593232	3.066573
-1301.073240	7.496341	3.076570
-1299.086250	7.968801	3.086566
-1297.107764	11.179158	3.096563
-1295.706256	11.265676	3.106560
-1293.954743	14.105976	3.116557
-1291.646401	7.402347	3.126554
-1289.671466	12.311141	3.136550
-1288.026419	11.390334	3.146547
-1286.320172	11.970695	3.156544
-1284.351715	15.017979	3.166541
-1282.138171	11.799792	3.176538
-1280.293207	7.894011	3.186534
-1278.725782	14.605800	3.196531
-1276.853841	6.167463	3.206528
-1275.012586	8.925962	3.216525
-1272.755509	10.598540	3.226522
-1271.265594	16.460901	3.236518
-1269.227148	13.043570	3.246515
-1267.120245	12.888407	3.256512
-1265.384588	12.845617	3.266509
-1263.650603	12.500384	3.276506
-1261.642501	11.277340	3.286502
-1259.608630	11.155670	3.296499
-1258.289547	14.708126	3.306496
-1256.540470	14.208938	3.316493
-1253.788322	12.289401	3.326490
-1252.333529	7.967300	3.336486
-1250.300721	9.313233	3.346483
-1248.523255	10.814075	3.356480
-1246.717936	17.255405	3.366477
-1244.780177	13.106059	3.376474
-1243.196776	12.048048	3.386470
-1240.624713	13.690654	3.396467
-1239.268738	12.514014	3.406464
-1237.296959	12.025593	3.416461
-1235.390962	10.644228	3.426458
-1233.910425	9.267562	3.436454
-1231.858094	7.804948	3.446451
-1229.518158	9.954961	3.456448
-1228.172844	9.152444	3.466445
-1226.039970	7.698527	3.476442
-1223.955033	9.515306	3.486438
-1222.215939	16.739867	3.496435
-1220.594893	15.328404	3.506432
-1218.805205	16.950466	3.516429
-1216.316848	16.101433	3.526426
-1214.509355	16.924881	3.536422
-1212.946327	15.977481	3.546419
-1211.046403	14.676607	3.556416
-1209.416110	13.749669	3.566413
-1207.239644	13.166038	3.576410
-1205.503571	13.140195	3.586406
-1203.532153	11.906089	3.596403
-1201.645870	12.333842	3.606400
-1199.778451	14.629440	3.616397
-1197.822528	15.006900	3.626394
-1196.155754	7.725433	3.636390
-1194.140174	15.854588	3.646387
-1192.147073	15.411532	3.656384
-1190.373353	14.313347	3.666381
-1188.463837	16.389888	3.676378
-1186.464616	18.242354	3.686374
-1184.373708	14.642554	3.696371
-1183.039196	11.343779	3.706368
-1181.344951	21.263498	3.716365
-1179.307727	15.028168	3.726362
-1177.096216	17.048111	3.736358
-1175.438956	7.304144	3.746355
-1173.346333	9.598624	3.756352
-1171.538914	13.802341	3.766349
-1169.851308	15.172027	3.776346
-1168.085874	13.299080	3.786342
-1165.620662	9.832222	3.796339
-1164.048240	14.150597	3.806336
-1162.321767	11.846450	3.816333
-1160.556793	10.156962	3.826330
-1158.623482	11.425967	3.836326
-1156.268254	6.646537	3.846323
-1154.957105	10.744991	3.856320
-1153.026122	15.004564	3.866317
-1150.690656	10.667213	3.876314
-1149.033380	11.813288	3.886310
-1147.092705	11.685149	3.896307
-1145.598670	15.275973	3.906304
-1143.543776	13.837462	3.916301
-1141.678978	15.695644	3.926298
-1139.493364	15.039338	3.936294
-1137.484411	11.653215	3.946291
-1135.801751	13.083836	3.956288
-1134.064195	22.471698	3.966285
-1132.296702	15.832954	3.976282
-1130.931703	15.723449	3.986278
-1128.496757	10.538293	3.996275
-1126.460206	15.874882	4.006272
-1124.796596	16.396236	4.016269
-1122.942545	15.426956	4.026266
-1120.956152	12.124151	4.036262
-1118.673590	18.230660	4.046259
-1117.262672	17.212193	4.056256
-1115.526408	19.935048	4.066253
-1113.403570	18.389244	4.076250
-1111.274839	14.009950	4.086246
-1109.935155	14.289339	4.096243
-1107.692225	7.717172	4.106240
-1105.968992	17.912550	4.116237
-1103.940951	15.538461	4.126234
-1102.450420	16.430611	4.136230
-1100.443466	18.035575	4.146227
-1098.279128	12.850266	4.156224
-1096.369730	10.680327	4.166221
-1094.653540	11.334545	4.176218
-1092.820941	17.894573	4.186214
-1091.014369	9.114995	4.196211
-1089.042910	11.818423	4.206208
-1087.209617	14.872020	4.216205
-1085.323084	15.676814	4.226202
-1083.509496	11.687576	4.236198
-1081.050995	11.391115	4.246195
-1079.616041	12.044228	4.256192
-1077.876512	9.149797	4.266189
-1076.025356	10.182778	4.276186
-1073.921022	5.261906	4.286182
-1072.357006	15.046348	4.296179
-1070.258389	14.077384	4.306176
-1068.066473	7.862177	4.316173
-1066.387059	13.060932	4.326170
-1064.944950	12.627572	4.336166
-1063.013442	16.743244	4.346163
-1060.988992	14.238976	4.356160
-1059.094186	20.810474	4.366157
-1057.074062	18.561466	4.376154
-1055.110227	15.266911	4.386150
-1053.505857	13.578958	4.396147
-1051.716779	15.067617	4.406144
-1049.437596	17.874338	4.416141
-1047.403291	15.351785	4.426138
-1045.842409	14.014345	4.436134
-1043.975600	12.275802	4.446131
-1042.254039	15.182616	4.456128
-1040.223146	15.733817	4.466125
-1038.367065	16.322938	4.476122
-1036.826808	19.271160	4.486118
-1034.983258	14.678839	4.496115
-1032.731494	13.800187	4.506112
-1030.401793	9.632246	4.516109
-1028.780542	16.519864	4.526106
-1027.400663	10.785559	4.536102
-1025.454679	14.673888	4.546099
-1023.240799	20.709649	4.556096
-1021.482883	17.951985	4.566093
-1019.588856	20.338346	4.576090
-1017.855203	14.875674	4.586086
-1015.974829	18.565812	4.596083
-1013.983462	20.841007	4.606080
-1011.994863	17.782111	4.616077
-1010.150182	18.591754	4.626074
-1008.499155	19.559138	4.636070
-1006.295103	14.052858	4.646067
-1004.801277	19.584263	4.656064
-1002.848218	17.939612	4.666061
-1000.900985	14.636468	4.676058
-998.832449	17.586090	4.686054
-996.901962	13.903258	4.696051
-995.104348	10.404487	4.706048
-993.576623	12.868766	4.716045
-991.393126	16.808815	4.726042
-989.634014	17.217000	4.736038
-988.201100	15.793262	4.746035
-985.750917	18.459606	4.756032
-983.726013	18.299296	4.766029
-982.104172	22.440905	4.776026
-979.928094	17.445705	4.786022
-978.685844	12.649165	4.796019
-976.899136	15.452343	4.806016
-974.691207	16.508299	4.816013
-972.575671	15.067361	4.826010
-970.455898	21.277789	4.836006
-968.673628	15.315539	4.846003
-967.169040	13.348734	4.856000
-965.128449	17.189630	4.865997
-963.157795	15.743929	4.875994
-961.623324	11.942956	4.885990
-959.757646	14.318797	4.895987
-957.704025	15.138832	4.905984
-955.878684	15.557003	4.915981
-953.672498	19.360387	4.925978
-951.906850	20.042533	4.935974
-950.596425	17.825699	4.945971
-948.590918	19.964127	4.955968
-946.216364	18.519046	4.965965
-944.557816	20.224211	4.975962
-942.857143	20.316398	4.985958
-940.610378	16.798635	4.995955
-938.960434	14.083647	5.005952
-937.235836	22.343133	5.015949
-935.216322	23.597445	5.025946
-932.891482	20.904527	5.035942
-931.447139	16.622647	5.045939
-929.673959	15.501738	5.055936
-927.648589	17.910253	5.065933
-925.615593	20.283471	5.075930
-924.162658	16.156623	5.085926
-922.298170	16.511968	5.095923
-919.919809	18.163129	5.105920
-918.221339	17.192979	5.115917
-916.524680	21.545067	5.125914
-914.574877	20.672863	5.135910
-912.554097	17.875649	5.145907
-910.843495	20.648054	5.155904
-908.810462	20.408527	5.165901
-906.762156	20.350153	5.175898
-904.903972	18.431350	5.185894
-903.292141	11.798857	5.195891
-901.686019	13.520942	5.205888
-899.563203	16.818173	5.215885
-897.481460	20.503047	5.225882
-895.861981	18.341858	5.235878
-894.128223	14.045087	5.245875
-891.996859	17.299358	5.255872
-890.134852	20.048152	5.265869
-888.358976	18.064048	5.275866
-886.441982	20.826723	5.285862
-884.481869	21.139980	5.295859
-882.566538	28.405203	5.305856
-880.738854	24.296241	5.315853
-878.856310	22.281183	5.325850
-876.899311	23.301222	5.335846
-875.209383	24.456031	5.345843
-873.041620	16.002618	5.355840
-871.291273	15.327103	5.365837
-869.677486	22.176952	5.375834
-867.679439	23.704121	5.385830
-865.829098	20.293964	5.395827
-863.768320	16.502665	5.405824
-861.851248	25.003032	5.415821
-860.037726	21.637532	5.425818
-858.338331	17.324539	5.435814
-856.251985	13.863600	5.445811
-854.432794	17.317310	5.455808
-852.586550	17.148208	5.465805
-850.734985	22.029404	5.475802
-849.043144	27.709474	5.485798
-847.033722	17.165305	5.495795
-844.963302	25.602605	5.505792
-843.238101	21.354744	5.515789
-841.724002	21.382565	5.525786
-839.387779	18.106779	5.535782
-837.181145	17.522898	5.545779
-835.636519	15.739755	5.555776
-834.287874	16.363109	5.565773
-832.125104	22.025979	5.575770
-830.092489	17.818232	5.585766
-828.114211	19.702528	5.595763
-826.225010	14.886665	5.605760
-824.175950	21.935307	5.615757
-822.480362	22.349327	5.625754
-820.527304	23.006870	5.635750
-819.291851	22.977005	5.645747
-817.394607	15.701937	5.655744
-815.084976	18.447838	5.665741
-812.990859	14.885200	5.675738
-811.394059	19.290834	5.685734
-809.485737	17.390734	5.695731
-807.472126	19.095082	5.705728
-805.731104	18.913234	5.715725
-803.925960	20.871128	5.725722
-801.966074	21.728275	5.735718
-799.987352	20.254782	5.745715
-797.954033	13.977990	5.755712
-796.293262	17.756118	5.765709
-794.691446	20.548826	5.775706
-792.625587	16.460276	5.785702
-790.794246	17.247011	5.795699
-788.790693	12.187450	5.805696
-787.044511	19.487679	5.815693
-784.898800	20.007835	5.825690
-782.884572	25.697811	5.835686
-781.159503	21.665781	5.845683
-779.601335	15.793833	5.855680
-777.833341	17.965997	5.865677
-775.835959	16.107931	5.875674
-773.925708	18.288087	5.885670
-771.812699	12.744976	5.895667
-769.740174	17.501734	5.905664
-768.189242	25.309742	5.915661
-766.470588	19.096058	5.925658
-764.618758	21.838358	5.935654
-762.494163	27.972197	5.945651
-760.460673	28.515578	5.955648
-758.632675	25.963352	5.965645
-757.064911	27.262087	5.975642
-755.069828	22.560868	5.985638
-753.207819	24.759985	5.995635
-751.265323	24.773593	6.005632
-749.548990	23.937185	6.015629
-747.276493	23.389076	6.025626
-745.558908	21.994414	6.035622
-743.615523	18.561221	6.045619
-742.232647	26.243952	6.055616
-740.057443	25.739814	6.065613
-738.358062	20.748679	6.075610
-736.439582	21.009077	6.085606
-734.224833	22.970607	6.095603
-732.533046	19.675451	6.105600
-730.399353	19.988629	6.115597
-728.733740	19.367630	6.125594
-726.858645	23.261953	6.135590
-725.024238	19.221849	6.145587
-722.962207	17.448749	6.155584
-721.380143	20.901720	6.165581
-719.466576	23.473779	6.175578
-717.354813	22.778586	6.185574
-715.529211	25.211612	6.195571
-714.036935	21.741239	6.205568
-711.809099	26.359135	6.215565
-709.892035	24.757543	6.225562
-708.221573	23.805717	6.235558
-706.193560	16.403909	6.245555
-704.413962	20.058138	6.255552
-702.505823	20.290684	6.265549
-700.711852	14.045128	6.275546
-698.817605	14.949551	6.285542
-696.840936	16.523943	6.295539
-694.792958	21.878959	6.305536
-693.195807	23.318508	6.315533
-691.143413	17.578741	6.325530
-689.403426	19.528896	6.335526
-687.243468	16.655727	6.345523
-685.414772	15.218702	6.355520
-684.190920	17.355054	6.365517
-681.980613	26.138360	6.375514
-679.783196	19.678528	6.385510
-678.185236	16.277373	6.395507
-676.249316	21.507376	6.405504
-674.212415	21.987769	6.415501
-672.334296	18.396260	6.425498
-670.542731	22.672887	6.435494
-668.602590	24.197838	6.445491
-667.074087	21.736566	6.455488
-664.954114	14.716578	6.465485
-662.981848	20.695208	6.475482
-661.329217	24.788986	6.485478
-659.243619	17.888324	6.495475
-657.497010	12.544488	6.505472
-655.796733	15.771687	6.515469
-653.666870	16.663756	6.525466
-651.959947	19.144050	6.535462
-649.810022	17.510033	6.545459
-647.980028	11.529824	6.555456
-646.049342	11.484249	6.565453
-644.333941	16.252955	6.575450
-642.653615	20.516276	6.585446
-640.491232	11.369493	6.595443
-638.473005	16.520575	6.605440
-636.900850	16.391090	6.615437
-634.998230	12.732948	6.625434
-633.236255	12.606460	6.635430
-631.265927	12.502710	6.645427
-629.546184	12.519424	6.655424
-627.173967	10.651641	6.665421
-625.480976	11.645567	6.675418
-623.798282	10.371947	6.685414
-621.724799	9.434384	6.695411
-620.128722	11.002193	6.705408
-618.140920	9.898723	6.715405
-616.316210	15.005957	6.725402
-614.344436	7.899973	6.735398
-612.149655	5.178159	6.745395
-610.209591	9.123434	6.755392
-608.570588	11.327288	6.765389
-607.044434	12.296101	6.775386
-604.933849	12.338632	6.785382
-603.045124	10.789375	6.795379
-601.304095	11.909440	6.805376
-599.098685	12.197729	6.815373
-597.507537	10.054944	6.825370
-595.495458	9.007786	6.835366
-593.566778	7.802626	6.845363
-591.604088	8.473242	6.855360
-589.794234	3.927185	6.865357
-588.112376	10.536250	6.875354
-586.356412	16.427542	6.885350
-584.523114	17.995367	6.895347
-582.250770	9.569579	6.905344
-580.585883	14.519689	6.915341
-578.892206	12.309125	6.925338
-576.832336	16.855530	6.935334
-574.644919	21.561455	6.945331
-573.085877	14.077737	6.955328
-571.252356	12.331664	6.965325
-569.227070	13.485171	6.975322
-567.497756	14.348791	6.985318
-565.331606	9.587077	6.995315
-563.602568	14.445563	7.005312
-561.691827	18.919553	7.015309
-559.794293	17.544672	7.025306
-558.002589	21.520174	7.035302
-556.230711	17.523665	7.045299
-554.247207	13.849305	7.055296
-552.214291	16.860201	7.065293
-550.841158	11.342170	7.075290
-548.789727	15.452141	7.085286
-546.622987	17.193969	7.095283
-544.638186	11.406579	7.105280
-543.167313	16.454415	7.115277
-540.966682	17.147462	7.125274
-539.234048	15.979125	7.135270
-537.324008	12.663980	7.145267
-535.665036	9.668169	7.155264
-533.337110	12.656120	7.165261
-531.698504	13.402921	7.175258
-530.131914	22.580133	7.185254
-528.072520	18.524027	7.195251
-525.939778	20.390264	7.205248
-524.220935	11.895059	7.215245
-522.724428	16.101047	7.225242
-520.539684	15.373270	7.235238
-518.474679	17.381948	7.245235
-516.627324	12.201091	7.255232
-514.962465	8.268412	7.265229
-512.847290	15.899093	7.275226
-511.072469	19.033336	7.285222
-509.161859	17.577189	7.295219
-507.356354	19.683751	7.305216
-505.492527	17.869664	7.315213
-503.722830	15.775319	7.325210
-501.885159	18.479065	7.335206
-499.726797	12.725937	7.345203
-497.670579	12.765597	7.355200
-496.210000	11.968424	7.365197
-494.248531	19.408122	7.375194
-492.191973	14.556953	7.385190
-490.556619	16.680067	7.395187
-488.608085	16.636241	7.405184
-486.793835	12.543566	7.415181
-484.761453	10.242517	7.425178
-483.051271	9.747941	7.435174
-481.080646	13.781701	7.445171
-479.077936	10.489411	7.455168
-477.353485	6.053293	7.465165
-475.343844	13.114813	7.475162
-473.523376	10.690856	7.485158
-471.133022	10.582696	7.495155
-469.709540	15.488905	7.505152
-468.288619	15.020250	7.515149
-466.220149	13.069105	7.525146
-464.011754	14.714905	7.535142
-462.622587	13.816173	7.545139
-460.581151	13.590035	7.555136
-458.419276	11.309859	7.565133
-456.774643	7.226536	7.575130
-454.588945	9.225208	7.585126
-452.804259	16.575111	7.595123
-451.144738	14.646312	7.605120
-449.300043	13.652438	7.615117
-447.348908	16.147039	7.625114
-445.015040	14.540053	7.635110
-443.706003	15.974190	7.645107
-441.802209	10.327206	7.655104
-440.174169	17.554204	7.665101
-437.828195	15.989012	7.675098
-435.985853	13.343158	7.685094
-434.155542	16.480165	7.695091
-431.898986	15.848005	7.705088
-430.069364	23.614673	7.715085
-428.887700	13.798761	7.725082
-426.874213	18.467814	7.735078
-424.870784	17.299699	7.745075
-422.571990	15.561997	7.755072
-420.875658	10.453324	7.765069
-419.129430	14.229200	7.775066
-417.308358	20.444939	7.785062
-415.758067	17.222385	7.795059
-413.334575	12.933528	7.805056
-411.746777	11.164463	7.815053
-409.886106	9.971443	7.825050
-408.074056	14.011102	7.835046
-405.887391	8.460252	7.845043
-403.889458	7.677238	7.855040
-402.570557	11.926386	7.865037
-400.520336	16.765416	7.875034
-398.289521	15.500603	7.885030
-396.286821	12.110335	7.895027
-394.918692	10.972572	7.905024
-392.769987	9.760183	7.915021
-390.942972	14.760419	7.925018
-389.131126	9.497173	7.935014
-387.504336	15.869560	7.945011
-385.349342	12.949955	7.955008
-383.418643	17.129334	7.965005
-381.631607	14.058647	7.975002
-379.780391	13.933154	7.984998
-377.526863	10.667042	7.994995
-376.099838	14.922946	8.004992
-374.215061	16.518786	8.014989
-372.460023	13.116474	8.024986
-370.211413	14.410402	8.034982
-368.310069	16.605709	8.044979
-367.023836	21.168744	8.054976
-364.597966	20.732449	8.064973
-362.540446	20.970741	8.074970
-360.964220	16.335210	8.084966
-359.214313	19.635040	8.094963
-357.244256	16.477635	8.104960
-355.267545	14.153784	8.114957
-353.450080	18.236013	8.124954
-351.626320	17.610553	8.134950
-350.032722	16.891389	8.144947
-348.014319	20.656574	8.154944
-345.532435	15.777164	8.164941
-344.138412	20.514581	8.174938
-342.484206	21.850019	8.184934
-340.279426	16.060145	8.194931
-338.069967	11.864161	8.204928
-337.013059	12.476851	8.214925
-334.645931	18.155134	8.224922
-332.948568	17.936698	8.234918
-331.024621	19.006130	8.244915
-329.144860	12.957818	8.254912
-327.225470	15.876453	8.264909
-325.154530	13.113571	8.274906
-323.771560	21.408638	8.284902
-321.390260	12.294379	8.294899
-319.497936	16.341650	8.304896
-317.769577	14.365521	8.314893
-315.944991	16.429369	8.324890
-314.076439	16.732505	8.334886
-312.178636	20.124760	8.344883
-310.322461	18.435372	8.354880
-308.478329	13.574475	8.364877
-306.671933	11.977808	8.374874
-304.704717	19.489735	8.384870
-302.814218	13.938746	8.394867
-300.836630	12.205218	8.404864
-299.124300	15.113142	8.414861
-297.374547	19.773354	8.424858
-295.383673	12.574100	8.434854
-293.188227	11.444245	8.444851
-291.604425	17.273514	8.454848
-289.708691	18.737486	8.464845
-287.590849	16.040085	8.474842
-285.880304	14.971274	8.484838
-284.199009	13.422553	8.494835
-282.149778	13.289220	8.504832
-280.106375	15.617891	8.514829
-278.783298	17.562660	8.524826
-276.581348	17.149408	8.534822
-274.875165	22.696457	8.544819
-272.850514	16.428471	8.554816
-270.620944	20.232170	8.564813
-268.861901	14.142931	8.574810
-267.261725	14.239181	8.584807
-265.385976	22.059277	8.594803
-263.256890	16.872475	8.604800
-261.526540	18.028498	8.614797
-259.415881	21.779879	8.624794
-258.026248	24.315944	8.634791
-256.044018	20.660497	8.644787
-253.963084	14.955927	8.654784
-252.156196	17.172230	8.664781
-250.106659	13.156268	8.674778
-248.189958	16.537406	8.684775
-246.698901	17.974769	8.694771
-245.068410	16.648586	8.704768
-242.925669	15.814721	8.714765
-240.771536	20.500452	8.724762
-238.968151	22.953306	8.734759
-237.044772	21.049674	8.744755
-235.182030	18.177891	8.754752
-233.223907	22.466856	8.764749
-231.584618	22.417295	8.774746
-229.737302	15.143486	8.784743
-227.726833	22.046519	8.794739
-225.869930	19.367024	8.804736
-223.674863	14.244409	8.814733
-222.018965	12.390217	8.824730
-220.250494	10.550707	8.834727
-218.184832	8.146052	8.844723
-216.428523	10.541381	8.854720
-214.671485	14.421015	8.864717
-213.077457	14.032619	8.874714
-210.653873	11.578832	8.884711
-208.827554	3.149866	8.894707
-206.935302	6.481466	8.904704
-205.424942	11.890999	8.914701
-203.423505	9.049191	8.924698
-201.716629	9.052469	8.934695
-199.612581	10.971214	8.944691
-197.678832	8.122838	8.954688
-195.949347	6.472613	8.964685
-194.409691	6.403398	8.974682
-192.024810	11.255484	8.984679
-190.209678	11.107803	8.994675
-188.348447	10.336076	9.004672
-186.489401	9.704236	9.014669
-184.647374	9.900524	9.024666
-182.674134	8.502143	9.034663
-181.093799	11.052951	9.044659
-178.731029	4.836491	9.054656
-176.998054	4.115221	9.064653
-175.392393	12.264652	9.074650
-173.231163	7.489724	9.084647
-171.476365	12.875530	9.094643
-169.567729	8.510288	9.104640
-167.825953	9.493260	9.114637
-166.015036	10.192467	9.124634
-164.048099	9.057994	9.134631
-162.284618	7.037167	9.144627
-160.056485	-0.649710	9.154624
-158.245659	6.238583	9.164621
-156.171749	3.366582	9.174618
-154.642161	13.006383	9.184615
-152.628086	14.506240	9.194611
-151.017258	9.726909	9.204608
-148.934772	4.727182	9.214605
-147.031055	8.356021	9.224602
-145.196890	6.048009	9.234599
-143.247945	7.381983	9.244595
-141.441587	8.654648	9.254592
-139.733356	5.299968	9.264589
-137.978848	4.756819	9.274586
-135.715436	10.747438	9.284583
-134.075505	7.618284	9.294579
-131.974034	3.807673	9.304576
-130.184407	9.779951	9.314573
-128.173558	10.034258	9.324570
-126.616405	14.982882	9.334567
-124.503710	15.296002	9.344563
-122.579488	12.463912	9.354560
-120.932534	8.177552	9.364557
-118.952679	11.971985	9.374554
-116.965144	8.169062	9.384551
-114.928493	14.273672	9.394547
-113.316518	17.586194	9.404544
-111.956758	12.542847	9.414541
-109.714782	14.676694	9.424538
-107.614461	17.067221	9.434535
-105.841798	14.354003	9.444531
-103.842989	16.296375	9.454528
-102.058355	9.926153	9.464525
-100.207766	15.673786	9.474522
-98.152584	11.791291	9.484519
-96.485055	17.393262	9.494515
-94.379789	12.697127	9.504512
-92.329906	15.185234	9.514509
-91.001789	18.430643	9.524506
-89.031570	10.261985	9.534503
-87.118641	16.328940	9.544499
-85.369455	13.125340	9.554496
-83.508866	17.940139	9.564493
-81.441966	15.838855	9.574490
-79.281583	19.109518	9.584487
-77.535059	15.411567	9.594483
-75.933907	12.896923	9.604480
-74.080156	19.570413	9.614477
-71.706092	22.036930	9.624474
-70.015628	25.817780	9.634471
-68.308394	14.631299	9.644467
-66.299543	24.782973	9.654464
-64.520284	11.759037	9.664461
-62.820021	12.661827	9.674458
-60.917255	18.219524	9.684455
-59.328733	21.931305	9.694451
-57.144213	14.700116	9.704448
-55.218500	11.073413	9.714445
-52.979424	15.679466	9.724442
-51.406551	9.870418	9.734439
-49.626073	14.308100	9.744435
-47.531087	15.957356	9.754432
-45.769799	9.616053	9.764429
-43.804918	16.091863	9.774426
-41.851056	16.051269	9.784423
-40.095193	13.368621	9.794419
-38.394201	9.522777	9.804416
-36.332064	8.727727	9.814413
-34.484595	10.497288	9.824410
-32.175495	10.259436	9.834407
-30.818245	14.799734	9.844403
-28.949114	6.765811	9.854400
-27.379614	10.085253	9.864397
-25.134270	6.065056	9.874394
-23.446856	13.878831	9.884391
-21.307846	16.005481	9.894387
-19.462654	13.295271	9.904384
-17.554146	13.606302	9.914381
-15.782100	9.065744	9.924378
-13.606441	0.224408	9.934375
-11.773783	6.046293	9.944371
-10.223073	11.135973	9.954368
-8.242155	9.962808	9.964365
-6.409223	10.485991	9.974362
-5.138425	24.457937	9.984359
-3.542393	45.632680	9.994355
-2.280496	81.462501	10.004352
-0.824751	148.790138	10.014349
0.000000	207.572626	10.019354
0.831992	236.181472	10.024359
1.414448	278.863774	10.029363
1.764529	308.012071	10.034368
2.353009	337.568341	10.039373
2.504867	362.132912	10.044378
3.182570	375.498362	10.049383
3.186104	401.066542	10.054387
3.438836	405.716436	10.059392
3.178919	414.541959	10.064397
3.189268	429.464586	10.069402
3.567320	445.865172	10.074407
3.689193	456.287429	10.079411
3.936241	458.981678	10.084416
3.894710	467.949779	10.089421
3.616668	465.800037	10.094426
3.945473	474.501361	10.099431
4.060417	493.980948	10.104435
4.243550	501.108243	10.109440
4.239923	515.266006	10.114445
3.930400	505.560732	10.119450
4.892298	509.217514	10.124455
4.647211	522.155150	10.129459
4.914002	514.315199	10.134464
4.672905	509.036460	10.139469
4.416531	498.236589	10.144474
4.781107	506.873774	10.149479
4.466128	517.925562	10.154483
4.688169	517.192779	10.159488
4.738344	532.630105	10.164493
4.280517	525.336747	10.169498
4.481550	526.964460	10.174503
4.211462	530.377764	10.179507
4.649862	523.732027	10.184512
4.697531	540.243833	10.189517
4.459693	554.209693	10.194522
5.138031	563.742423	10.199527
4.772189	579.950579	10.204531
5.136822	575.051496	10.209536
4.903843	585.176272	10.214541
5.246867	581.147709	10.219546
5.397355	579.443932	10.224551
4.909587	580.037946	10.229555
5.643626	575.965628	10.234560
5.232621	591.576032	10.239565
5.327880	579.863996	10.244570
5.550646	574.830558	10.249575
5.036770	589.355342	10.254579
5.360689	583.524581	10.259584
5.554078	602.022196	10.264589
5.661591	606.976516	10.269594
6.093713	604.564071	10.274599
5.579896	614.033223	10.279603
5.677799	604.880512	10.284608
6.020884	621.742398	10.289613
6.159668	614.871688	10.294618
6.197731	615.349491	10.299623
5.252666	611.187314	10.304627
5.801186	610.182633	10.309632
6.387243	620.851454	10.314637
5.856447	626.415738	10.319642
6.201167	629.588651	10.324647
6.267801	634.183683	10.329651
6.524801	631.092727	10.334656
6.184337	631.747536	10.339661
6.372041	636.917847	10.344666
6.749589	635.997346	10.349671
6.291262	641.785651	10.354675
6.201618	638.930178	10.359680
6.260375	640.084548	10.364685
6.206051	640.888053	10.369690
6.664049	639.630873	10.374695
6.490428	641.655591	10.379699
6.403365	648.341795	10.384704
6.301788	648.353292	10.389709
6.209437	668.016266	10.394714
6.542615	678.269418	10.399719
6.110555	684.617695	10.404723
6.456133	681.206417	10.409728
6.190976	689.315378	10.414733
6.418453	702.290159	10.419738
6.677532	711.906316	10.424743
6.552045	719.156099	10.429747
6.919751	715.050640	10.434752
6.837402	721.801591	10.439757
6.956340	740.036615	10.444762
7.283472	744.237285	10.449767
7.242539	750.697337	10.454771
7.544910	755.899341	10.459776
7.407478	760.266510	10.464781
7.095082	762.594112	10.469786
7.502477	754.249548	10.474791
7.241881	757.846796	10.479795
7.555963	756.837699	10.484800
7.216548	765.187191	10.489805
7.353759	773.194442	10.494810
7.360344	776.202735	10.499815
7.346368	776.091451	10.504819
7.885660	780.269963	10.509824
8.328004	783.038545	10.514829
7.862316	780.272390	10.519834
7.923279	778.726044	10.524839
7.667381	780.009374	10.529843
7.954972	773.814515	10.534848
7.723231	785.582074	10.539853
7.804520	796.320985	10.544858
8.063008	801.070273	10.549863
7.827218	804.237364	10.554867
7.912683	808.968558	10.559872
7.937109	817.456611	10.564877
7.732953	814.014828	10.569882
8.034716	815.976611	10.574887
8.555465	832.078010	10.579891
8.664144	836.710497	10.584896
8.603499	833.478968	10.589901
8.473623	833.281768	10.594906
8.718093	824.518661	10.599911
8.673316	830.875986	10.604915
8.485376	823.683447	10.609920
8.692673	842.413433	10.614925
8.684877	846.551953	10.619930
8.673356	852.330435	10.624935
8.649023	860.863976	10.629939
8.695904	857.592295	10.634944
9.106676	856.468720	10.639949
8.633857	863.063660	10.644954
9.264963	859.304969	10.649959
8.940231	854.530709	10.654963
8.778139	860.706059	10.659968
9.033735	865.034288	10.664973
9.081208	869.032682	10.669978
9.064558	861.922465	10.674983
9.091167	872.068443	10.679987
9.154373	865.042031	10.684992
9.232438	868.173478	10.689997
9.202323	871.534263	10.695002
9.387403	882.928851	10.700007
9.429763	891.471105	10.705011
9.428999	890.720850	10.710016
9.754006	897.347954	10.715021
9.374464	901.626807	10.720026
9.600121	898.146045	10.725031
9.300416	906.703143	10.730035
9.503455	901.776798	10.735040
9.615515	907.694767	10.740045
9.564328	901.661759	10.745050
9.683546	901.379612	10.750055
9.617879	908.477122	10.755059
9.747366	914.255923	10.760064
10.139668	935.036913	10.765069
10.205909	941.990638	10.770074
10.240955	939.352938	10.775079
9.959438	942.772238	10.780083
10.411183	929.702905	10.785088
10.372334	939.249891	10.790093
10.189752	937.710157	10.795098
10.729043	940.621617	10.800103
10.141130	939.015592	10.805107
10.540492	936.927660	10.810112
10.238244	953.658188	10.815117
10.360714	945.565664	10.820122
10.290886	946.796578	10.825127
10.282046	950.114652	10.830131
10.465508	944.422709	10.835136
10.127772	951.822281	10.840141
10.325096	948.349524	10.845146
10.653697	944.570050	10.850151
10.121541	950.892570	10.855155
10.671195	967.092969	10.860160
10.892032	967.235105	10.865165
10.866465	985.165194	10.870170
11.154588	981.856860	10.875175
10.936959	986.009685	10.880179
11.373566	987.711924	10.885184
11.284662	987.415328	10.890189
11.108550	983.918172	10.895194
11.134657	985.216718	10.900199
10.997986	983.301214	10.905203
11.295206	986.868792	10.910208
11.096775	989.320175	10.915213
11.183368	985.297977	10.920218
11.393557	978.832494	10.925223
11.144359	992.379114	10.930227
11.341687	979.132311	10.935232
11.420128	984.579233	10.940237
11.540197	992.297827	10.945242
11.769295	1006.671132	10.950247
11.397028	1012.092317	10.955251
11.857458	1021.265195	10.960256
11.863231	1023.422229	10.965261
11.727749	1023.547697	10.970266
12.080578	1024.222990	10.975271
12.041927	1037.954996	10.980275
11.899279	1027.637363	10.985280
11.900555	1026.998068	10.990285
12.057390	1024.175656	10.995290
12.227664	1026.616722	11.000295
11.835645	1035.057876	11.005299
11.779498	1038.461449	11.010304
11.845029	1037.042584	11.015309
11.903599	1033.037810	11.020314
11.972161	1028.627904	11.025319
11.875345	1040.639361	11.030323
12.001389	1044.430118	11.035328
12.310008	1054.754439	11.040333
11.926094	1070.452252	11.045338
12.482864	1075.238507	11.050343
12.218319	1069.592939	11.055347
12.481831	1064.338411	11.060352
12.493357	1065.146042	11.065357
12.420380	1066.343163	11.070362
12.370506	1068.249612	11.075367
12.436458	1088.935579	11.080371
12.826470	1099.581502	11.085376
13.098179	1094.882140	11.090381
13.029835	1104.912706	11.095386
13.294883	1095.091180	11.100391
12.808435	1097.492094	11.105395
13.044338	1098.033886	11.110400
13.334739	1090.479338	11.115405
12.937088	1100.241891	11.120410
12.955387	1097.354404	11.125415
13.030072	1100.965295	11.130419
13.736164	1096.368295	11.135424
13.992859	1099.524820	11.140429
13.522388	1087.164533	11.145434
13.416446	1079.046762	11.150439
13.130197	1074.412283	11.155443
13.457929	1079.325048	11.160448
13.074994	1087.450066	11.165453
13.211240	1097.406470	11.170458
13.386874	1098.936757	11.175463
13.693440	1106.287903	11.180467
13.434381	1105.782058	11.185472
13.576101	1108.405270	11.190477
13.482195	1110.400196	11.195482
13.481848	1109.017488	11.200487
13.080194	1123.562997	11.205491
13.502081	1122.432762	11.210496
13.891106	1136.339421	11.215501
13.748569	1142.667845	11.220506
14.168012	1137.555505	11.225511
13.961777	1144.938937	11.230515
14.077859	1136.759383	11.235520
14.139771	1144.508945	11.240525
14.026829	1141.872901	11.245530
14.582508	1137.751287	11.250535
14.135722	1151.326002	11.255539
14.434865	1140.137540	11.260544
14.246637	1139.456126	11.265549
14.311987	1144.880086	11.270554
14.267568	1138.680431	11.275559
14.148914	1160.073543	11.280563
14.661906	1170.179741	11.285568
14.815766	1175.553403	11.290573
14.564193	1186.284128	11.295578
15.010827	1179.695522	11.300583
14.741278	1181.786099	11.305587
14.592862	1171.875547	11.310592
14.704384	1179.254644	11.315597
14.527273	1185.112561	11.320602
14.764249	1169.458779	11.325607
14.890263	1182.748596	11.330611
14.961012	1174.226266	11.335616
14.984237	1180.371151	11.340621
15.027481	1181.171376	11.345626
14.915379	1173.416194	11.350631
14.713356	1184.507109	11.355635
15.248566	1186.738785	11.360640
15.717692	1197.968058	11.365645
15.195773	1190.678269	11.370650
15.616687	1178.858237	11.375655
15.124110	1182.688385	11.380659
15.363074	1192.050917	11.385664
15.066634	1194.682953	11.390669
15.285946	1209.958526	11.395674
15.418672	1210.835780	11.400679
15.386978	1217.869184	11.405683
15.501444	1207.975509	11.410688
15.655770	1204.155197	11.415693
15.658832	1219.710228	11.420698
16.131450	1209.152770	11.425703
15.721350	1216.625269	11.430707
16.278363	1211.773137	11.435712
15.902085	1221.815129	11.440717
15.597100	1215.450512	11.445722
15.779046	1220.553714	11.450727
15.553728	1220.491295	11.455731
16.009256	1230.702122	11.460736
16.484644	1245.900666	11.465741
16.486022	1246.068591	11.470746
16.349650	1227.356752	11.475751
16.231451	1225.634632	11.480755
16.619628	1221.937642	11.485760
16.555092	1223.794914	11.490765
16.554013	1217.114896	11.495770
16.740201	1220.917094	11.500775
16.261812	1214.776422	11.505779
16.387399	1210.136816	11.510784
16.354849	1213.981649	11.515789
16.505546	1222.548536	11.520794
16.729249	1233.254250	11.525799
16.394618	1248.902343	11.530803
16.522582	1250.270685	11.535808
16.377466	1248.490808	11.540813
16.637032	1251.146339	11.545818
16.817789	1254.049070	11.550823
16.929278	1256.354987	11.555827
16.954173	1248.598383	11.560832
16.833472	1250.507130	11.565837
16.799297	1252.330778	11.570842
17.045228	1250.980437	11.575847
16.878478	1252.027858	11.580851
16.967727	1274.096804	11.585856
17.500396	1274.903119	11.590861
16.903395	1282.865991	11.595866
17.336532	1279.440363	11.600871
17.176803	1282.662403	11.605875
17.184734	1274.983696	11.610880
17.384897	1277.632443	11.615885
17.656757	1283.446181	11.620890
17.527960	1280.323746	11.625895
17.416619	1279.421114	11.630899
17.825678	1271.636526	11.635904
17.735020	1271.909838	11.640909
17.672780	1277.174534	11.645914
17.779506	1276.607544	11.650919
17.531904	1276.830396	11.655923
17.632874	1274.895032	11.660928
17.498696	1283.928829	11.665933
17.668178	1299.910939	11.670938
18.071186	1302.577017	11.675943
18.180104	1299.970407	11.680947
18.318398	1309.392903	11.685952
18.216172	1304.450088	11.690957
18.174650	1309.076100	11.695962
18.953916	1300.313402	11.700967
18.564372	1292.166776	11.705971
18.444903	1274.107651	11.710976
18.396120	1275.801172	11.715981
18.225596	1276.798320	11.720986
18.463069	1269.207761	11.725991
18.470625	1271.225969	11.730995
18.501463	1269.522501	11.736000
18.151813	1269.802719	11.741005
18.052757	1286.323103	11.746010
17.989164	1292.517260	11.751015
18.454928	1302.605194	11.756019
18.222321	1299.487528	11.761024
18.441159	1302.673480	11.766029
18.412672	1309.330185	11.771034
18.860515	1321.748217	11.776039
18.511103	1332.718453	11.781043
18.961312	1322.330948	11.786048
19.346929	1329.889309	11.791053
18.976501	1332.818269	11.796058
19.299922	1323.297650	11.801063
19.162568	1323.367387	11.806067
19.347304	1330.015568	11.811072
19.236937	1336.124603	11.816077
18.864000	1332.605062	11.821082
19.240155	1329.033269	11.826087
19.156763	1332.550921	11.831091
19.105884	1329.571435	11.836096
19.299573	1332.263539	11.841101
18.821135	1337.237240	11.846106
19.573396	1346.492119	11.851111
19.382561	1357.921902	11.856115
19.564227	1362.493873	11.861120
19.724689	1354.026328	11.866125
19.720021	1367.039887	11.871130
20.148216	1360.540422	11.876135
19.802824	1367.178460	11.881139
19.811822	1360.124803	11.886144
19.679663	1354.725253	11.891149
19.917248	1360.742664	11.896154
20.276963	1356.136295	11.901159
20.058289	1359.451749	11.906163
20.338869	1356.863856	11.911168
20.051382	1364.018159	11.916173
20.284607	1361.265091	11.921178
20.342914	1354.940761	11.926183
20.219488	1348.801148	11.931187
20.401421	1352.490817	11.936192
20.239272	1341.276302	11.941197
20.315401	1357.759618	11.946202
20.462940	1361.667164	11.951207
20.135492	1374.910551	11.956211
20.474361	1377.384345	11.961216
20.462351	1369.808092	11.966221
20.282997	1367.203923	11.971226
20.294483	1367.751834	11.976231
20.826645	1364.217628	11.981235
20.562182	1369.480317	11.986240
20.630075	1363.046179	11.991245
20.645180	1374.928964	11.996250
21.099220	1356.343507	12.001255
20.549513	1369.029328	12.006259
20.897703	1375.159625	12.011264
20.444337	1369.848301	12.016269
20.668905	1385.819081	12.021274
20.887338	1389.142098	12.026279
20.849626	1404.651803	12.031283
21.136530	1398.571293	12.036288
21.397392	1406.481483	12.041293
20.822661	1398.619585	12.046298
20.938337	1400.350845	12.051303
21.068717	1404.150420	12.056307
21.016247	1397.974542	12.061312
21.092023	1394.652004	12.066317
21.105125	1411.332898	12.071322
21.417390	1400.142002	12.076327
21.571551	1391.132741	12.081331
21.477599	1367.564408	12.086336
21.416495	1366.300650	12.091341
21.524132	1378.451394	12.096346
21.221061	1365.809546	12.101351
21.087001	1369.855773	12.106355
21.243418	1372.163872	12.111360
21.165272	1371.896608	12.116365
20.675561	1370.078694	12.121370
21.204329	1358.553462	12.126375
21.131543	1368.264427	12.131379
20.932026	1355.686544	12.136384
21.071626	1342.311566	12.141389
20.746298	1351.220673	12.146394
21.022133	1357.426134	12.151399
21.121412	1370.066998	12.156403
20.970819	1362.645564	12.161408
21.332243	1356.894537	12.166413
20.821210	1348.621471	12.171418
21.473523	1339.707226	12.176423
20.991378	1348.207027	12.181427
21.214969	1348.681465	12.186432
21.411806	1336.356172	12.191437
21.371813	1333.378371	12.196442
21.451079	1338.544613	12.201447
20.733314	1345.107933	12.206451
20.935024	1340.936035	12.211456
20.970078	1335.728089	12.216461
20.596401	1340.690935	12.221466
20.930075	1342.869556	12.226471
20.987258	1343.212655	12.231475
20.962079	1341.014695	12.236480
20.924523	1340.430994	12.241485
21.001891	1336.298575	12.246490
21.039626	1333.594426	12.251495
20.895493	1339.769648	12.256499
20.943846	1345.322910	12.261504
21.244052	1338.787765	12.266509
20.798505	1340.848933	12.271514
21.408548	1337.999287	12.276519
21.168964	1343.364676	12.281523
21.352987	1346.289760	12.286528
21.320602	1337.551336	12.291533
21.047109	1350.888085	12.296538
21.018045	1348.168149	12.301543
20.872630	1347.316750	12.306547
20.810564	1346.870280	12.311552
21.116629	1351.158808	12.316557
20.568131	1353.203286	12.321562
21.055633	1343.499387	12.326567
21.492983	1340.753167	12.331571
21.230132	1342.289580	12.336576
21.554381	1346.736834	12.341581
21.318813	1337.046387	12.346586
21.125405	1317.776181	12.351591
20.923513	1316.004058	12.356595
20.862834	1310.413843	12.361600
21.268746	1313.656540	12.366605
20.847567	1315.473127	12.371610
21.047970	1307.995880	12.376615
21.067735	1309.455412	12.381619
21.034793	1316.775658	12.386624
20.750278	1322.949285	12.391629
20.839275	1327.463317	12.396634
20.887448	1311.347150	12.401639
20.624379	1326.510543	12.406643
20.867525	1345.084984	12.411648
21.211234	1342.950489	12.416653
21.036742	1356.362638	12.421658
21.067816	1350.297194	12.426663
20.991062	1353.845687	12.431667
20.994772	1348.238103	12.436672
21.203633	1349.568504	12.441677
20.918288	1355.877682	12.446682
20.812794	1349.957236	12.451687
21.163281	1357.572950	12.456691
21.020851	1350.757240	12.461696
21.182036	1351.766993	12.466701
20.779686	1355.007753	12.471706
21.265380	1353.809325	12.476711
21.141136	1350.191085	12.481715
20.595602	1340.697074	12.486720
20.793577	1347.468127	12.491725
20.818532	1360.444628	12.496730
21.210802	1353.444078	12.501735
21.136353	1355.583728	12.506739
21.262560	1357.215675	12.511744
21.329145	1347.478151	12.516749
21.063390	1340.603063	12.521754
21.414451	1330.371897	12.526759
21.195389	1333.312405	12.531763
21.098214	1329.843479	12.536768
21.037837	1321.713427	12.541773
20.956012	1326.859126	12.546778
21.202162	1323.905293	12.551783
21.156986	1332.784514	12.556787
20.878570	1326.192660	12.561792
21.225010	1325.845888	12.566797
20.658054	1326.386002	12.571802
21.064671	1320.871980	12.576807
20.685478	1317.856023	12.581811
20.606833	1328.595091	12.586816
20.763143	1326.741022	12.591821
20.629626	1336.852782	12.596826
20.934061	1351.938633	12.601831
21.044170	1362.425093	12.606835
21.045910	1355.638742	12.611840
21.525836	1354.531699	12.616845
20.929062	1350.917898	12.621850
21.152788	1339.975518	12.626855
21.102020	1340.991217	12.631859
21.012952	1338.212096	12.636864
21.248902	1334.215122	12.641869
20.808981	1338.803266	12.646874
21.006833	1325.420683	12.651879
21.031583	1332.620516	12.656883
20.934946	1329.137288	12.661888
21.043102	1323.683912	12.666893
21.112856	1336.533894	12.671898
21.136867	1339.568124	12.676903
21.001386	1334.235468	12.681907
20.986364	1334.105806	12.686912
20.929946	1335.671956	12.691917
20.873051	1335.400655	12.696922
20.948918	1332.741285	12.701927
20.666270	1338.968282	12.706931
21.018648	1337.151254	12.711936
21.137564	1342.144118	12.716941
20.986091	1338.777659	12.721946
21.101759	1333.634840	12.726951
20.864513	1330.652175	12.731955
21.098130	1333.714019	12.736960
21.386675	1328.831698	12.741965
21.034625	1335.462179	12.746970
21.206144	1324.338890	12.751975
21.099724	1333.756385	12.756979
21.118495	1338.643257	12.761984
21.141799	1343.870807	12.766989
21.262627	1340.519635	12.771994
21.285293	1343.349619	12.776999
21.280960	1348.005978	12.782003
21.192653	1345.996082	12.787008
21.272078	1339.707611	12.792013
21.132735	1342.949459	12.797018
21.084682	1336.807585	12.802023
21.125932	1343.033525	12.807027
21.131218	1330.392520	12.812032
21.055770	1314.824923	12.817037
21.150187	1313.050943	12.822042
20.844724	1310.279324	12.827047
20.948167	1306.361920	12.832051
20.867978	1311.111407	12.837056
21.193613	1316.821199	12.842061
21.173269	1319.149334	12.847066
21.251759	1302.906002	12.852071
21.502386	1304.700956	12.857075
21.309879	1309.851022	12.862080
21.618229	1306.834816	12.867085
20.990544	1321.865323	12.872090
21.191605	1318.035786	12.877095
21.120118	1307.678133	12.882099
21.293254	1308.360961	12.887104
21.596150	1303.997247	12.892109
21.253358	1301.884936	12.897114
21.184481	1293.180030	12.902119
21.189365	1289.476900	12.907123
21.315370	1291.415985	12.912128
21.495253	1286.199802	12.917133
21.042793	1285.759479	12.922138
21.421813	1286.023315	12.927143
21.430330	1289.949943	12.932147
21.340252	1271.081689	12.937152
21.089914	1260.547099	12.942157
20.974098	1254.248717	12.947162
20.888329	1246.792539	12.952167
20.965737	1252.368813	12.957171
20.706462	1261.622602	12.962176
20.960482	1264.042241	12.967181
20.992535	1272.029095	12.972186
21.149413	1267.393581	12.977191
21.015058	1269.163748	12.982195
21.040676	1258.070259	12.987200
21.366220	1248.062604	12.992205
20.961303	1253.909474	12.997210
21.378703	1246.152679	13.002215
21.285782	1253.215545	13.007219
21.175496	1254.235521	13.012224
21.321393	1249.098600	13.017229
20.965131	1259.389424	13.022234
20.619984	1257.804503	13.027239
20.817819	1259.662583	13.032243
20.830366	1258.604498	13.037248
21.233446	1253.164528	13.042253
20.776557	1265.682375	13.047258
20.747779	1262.690033	13.052263
20.830484	1260.402139	13.057267
20.825190	1260.428312	13.062272
21.006643	1263.563824	13.067277
20.451088	1265.409762	13.072282
20.774774	1277.914574	13.077287
20.987816	1295.493051	13.082291
21.221905	1296.239639	13.087296
21.044996	1295.375090	13.092301
21.096822	1303.034486	13.097306
20.962418	1297.191649	13.102311
21.164064	1294.076897	13.107315
21.119934	1296.727269	13.112320
21.387186	1287.587360	13.117325
21.001763	1279.595562	13.122330
20.720202	1267.517746	13.127335
20.605617	1275.372241	13.132339
21.073848	1281.573105	13.137344
21.294967	1285.471963	13.142349
20.734704	1296.692277	13.147354
21.425135	1288.325349	13.152359
21.308816	1273.338363	13.157363
20.972805	1267.040624	13.162368
20.786812	1248.867800	13.167373
20.680884	1260.422693	13.172378
21.241493	1273.370833	13.177383
21.329820	1280.182368	13.182387
20.980674	1262.231716	13.187392
20.994695	1265.026457	13.192397
20.637494	1278.182889	13.197402
20.960254	1269.507559	13.202407
21.031864	1278.263697	13.207411
20.973863	1288.156028	13.212416
21.269556	1286.216091	13.217421
20.889107	1284.622614	13.222426
20.687956	1278.045560	13.227431
21.158631	1291.594933	13.232435
21.335826	1297.178983	13.237440
21.471191	1274.364116	13.242445
21.409243	1279.986400	13.247450
21.314843	1263.822489	13.252455
21.110487	1267.867321	13.257459
20.790083	1270.115842	13.262464
21.161463	1260.810856	13.267469
21.073280	1269.664651	13.272474
20.855501	1270.662006	13.277479
20.953423	1270.623902	13.282483
21.001853	1277.342012	13.287488
20.997575	1274.067963	13.292493
20.856408	1270.143165	13.297498
20.775478	1271.210610	13.302503
21.086623	1273.407690	13.307507
20.674117	1283.706595	13.312512
20.895924	1270.867459	13.317517
20.427818	1278.439934	13.322522
20.645890	1284.231315	13.327527
20.938322	1307.093642	13.332531
20.888142	1310.902441	13.337536
21.033288	1308.344093	13.342541
21.127691	1313.477731	13.347546
21.397387	1306.562956	13.352551
21.195313	1310.992283	13.357555
20.906864	1295.256355	13.362560
20.900255	1292.148888	13.367565
20.820130	1315.381425	13.372570
21.281489	1312.455433	13.377575
20.904307	1311.196531	13.382579
21.059612	1312.466636	13.387584
21.107437	1312.253566	13.392589
21.117902	1310.827144	13.397594
21.358732	1293.189780	13.402599
20.890857	1286.956090	13.407603
20.598689	1281.660975	13.412608
20.784434	1287.742510	13.417613
20.685870	1307.679726	13.422618
20.826512	1314.509149	13.427623
20.810569	1320.100269	13.432627
20.544363	1321.115799	13.437632
20.879671	1314.570303	13.442637
20.795017	1321.119799	13.447642
20.638508	1321.060582	13.452647
20.925372	1318.404116	13.457651
20.899416	1325.070658	13.462656
21.260806	1316.807501	13.467661
21.029827	1325.150934	13.472666
21.296015	1319.867046	13.477671
21.394136	1321.449726	13.482675
21.048619	1330.034250	13.487680
21.541288	1320.511851	13.492685
21.378984	1329.231939	13.497690
21.362666	1328.022085	13.502695
21.367460	1319.651118	13.507699
21.049870	1297.293624	13.512704
21.136629	1291.265630	13.517709
20.864043	1290.896704	13.522714
21.158946	1282.946549	13.527719
20.983673	1285.048212	13.532723
20.808705	1291.655419	13.537728
21.201006	1290.373533	13.542733
21.207772	1298.074995	13.547738
20.909679	1290.703359	13.552743
20.949441	1293.577377	13.557747
20.735896	1294.246371	13.562752
20.965953	1290.369632	13.567757
20.910501	1294.797104	13.572762
21.096516	1293.744801	13.577767
21.147985	1294.096773	13.582771
20.889413	1294.595458	13.587776
21.094981	1282.015680	13.592781
20.721048	1292.653377	13.597786
20.919068	1292.630479	13.602791
20.819179	1300.000091	13.607795
20.936475	1316.414726	13.612800
21.423931	1325.041563	13.617805
20.883653	1316.070885	13.622810
20.885664	1309.194111	13.627815
21.197945	1319.921409	13.632819
20.986258	1315.532236	13.637824
20.951305	1315.649548	13.642829
20.902552	1320.018641	13.647834
21.260085	1315.356604	13.652839
21.177301	1304.658253	13.657843
20.892654	1295.494150	13.662848
21.049914	1297.486693	13.667853
20.992697	1299.943912	13.672858
21.047601	1295.893120	13.677863
21.225319	1295.717780	13.682867
20.911142	1293.657406	13.687872
21.315308	1295.861040	13.692877
21.047596	1298.197243	13.697882
21.132984	1296.647448	13.702887
20.907223	1287.316540	13.707891
20.912295	1297.903467	13.712896
20.955876	1293.709746	13.717901
20.799931	1298.721696	13.722906
20.967930	1292.291345	13.727911
20.921338	1298.831148	13.732915
21.115395	1299.526967	13.737920
20.800268	1298.265321	13.742925
21.213464	1305.206300	13.747930
21.193780	1293.241460	13.752935
21.114929	1298.045977	13.757939
20.949304	1301.707198	13.762944
20.810856	1292.380658	13.767949
21.169387	1300.623396	13.772954
20.800207	1299.413650	13.777959
21.024516	1297.999512	13.782963
20.893813	1301.924355	13.787968
20.745763	1290.009158	13.792973
20.940140	1315.365715	13.797978
21.107247	1320.537812	13.802983
21.091536	1322.252511	13.807987
21.290215	1317.067437	13.812992
21.547165	1294.387618	13.817997
21.628896	1298.059322	13.823002
21.314440	1297.381386	13.828007
21.371149	1299.723939	13.833011
21.144909	1301.367756	13.838016
21.257210	1292.838632	13.843021
21.132407	1303.680730	13.848026
21.385909	1284.783157	13.853031
21.221577	1279.116381	13.858035
20.920160	1270.376358	13.863040
21.215336	1266.817674	13.868045
21.094137	1264.031049	13.873050
20.911630	1267.163438	13.878055
21.091347	1265.561551	13.883059
20.803811	1263.498588	13.888064
21.338298	1264.130904	13.893069
21.288881	1264.219906	13.898074
21.090211	1265.575568	13.903079
21.051439	1264.110618	13.908083
21.013482	1274.385956	13.913088
20.764039	1262.016054	13.918093
20.742711	1276.084777	13.923098
20.421089	1268.487841	13.928103
20.718584	1275.348775	13.933107
20.740162	1281.909646	13.938112
20.810998	1299.045923	13.943117
20.873060	1313.139462	13.948122
21.265332	1306.616967	13.953127
21.169102	1305.078968	13.958131
21.145713	1311.059394	13.963136
21.151122	1299.674467	13.968141
21.077936	1290.609112	13.973146
21.032545	1285.080233	13.978151
20.708200	1278.404299	13.983155
20.949348	1293.759501	13.988160
21.309794	1299.580557	13.993165
20.827516	1299.633249	13.998170
20.902121	1295.523815	14.003175
21.024942	1301.965492	14.008179
21.222031	1312.162659	14.013184
21.327911	1289.176375	14.018189
20.560155	1296.258239	14.023207
20.825787	1299.905153	14.028224
21.092384	1304.647670	14.033242
21.218877	1313.342913	14.038259
21.109893	1310.416846	14.043277
20.995831	1316.303865	14.048295
20.905535	1307.589425	14.053312
21.144412	1314.232144	14.058330
21.186789	1321.449946	14.063347
21.168238	1305.637128	14.068365
21.149098	1316.278775	14.073383
21.235041	1309.090163	14.078400
21.139848	1318.819178	14.083418
20.788070	1325.582862	14.088435
21.416289	1316.169184	14.093453
21.205987	1318.657435	14.098471
21.172584	1313.685153	14.103488
21.281693	1315.331558	14.108506
21.587826	1316.405945	14.113523
21.542330	1309.786768	14.118541
21.374307	1319.469211	14.123559
21.127093	1322.609913	14.128576
21.460790	1317.068736	14.133594
21.674781	1320.680410	14.138611
21.926799	1309.969304	14.143629
21.768656	1312.830535	14.148647
21.466080	1312.622943	14.153664
21.219115	1284.551349	14.158682
20.975917	1310.842646	14.163699
21.227455	1303.095675	14.168717
21.258531	1314.654779	14.173735
21.128434	1317.997467	14.178752
21.216527	1323.846678	14.183770
21.126076	1320.798129	14.188787
21.521114	1332.071594	14.193805
21.787780	1350.289766	14.198823
21.629823	1352.070163	14.203840
21.869205	1347.244818	14.208858
21.702761	1349.263306	14.213875
21.668545	1349.516835	14.218893
21.627947	1351.611393	14.223911
21.884459	1350.067668	14.228928
21.580061	1357.253991	14.233946
21.580619	1365.527900	14.238963
21.873894	1351.897213	14.243981
21.480553	1361.723836	14.248999
21.997373	1357.666349	14.254016
21.988460	1362.557313	14.259034
21.318674	1361.965395	14.264051
21.658669	1357.426761	14.269069
21.661437	1361.394376	14.274087
21.610903	1363.845003	14.279104
21.706470	1363.003739	14.284122
21.671034	1366.703470	14.289139
22.105476	1361.570241	14.294157
22.071404	1364.959866	14.299175
21.533723	1365.506824	14.304192
22.015006	1364.647461	14.309210
21.650110	1376.906453	14.314227
21.951889	1375.634518	14.319245
21.925012	1378.027937	14.324263
21.743216	1385.732279	14.329280
21.972319	1391.690028	14.334298
21.559965	1391.821760	14.339315
22.110477	1386.879665	14.344333
21.973452	1385.859754	14.349351
21.761268	1393.116511	14.354368
22.159097	1405.275068	14.359386
22.115013	1421.118022	14.364403
21.922661	1412.065869	14.369421
22.160781	1421.614952	14.374439
22.201647	1426.969494	14.379456
22.331696	1420.533973	14.384474
22.203496	1415.409391	14.389491
22.202052	1416.173100	14.394509
22.317695	1419.900489	14.399527
22.418067	1424.080935	14.404544
22.368856	1415.261742	14.409562
22.191267	1427.615442	14.414579
21.979248	1428.869632	14.419597
22.098692	1430.354419	14.424615
22.416566	1448.470216	14.429632
23.100337	1460.017134	14.434650
22.861571	1442.845338	14.439667
22.916602	1432.968790	14.444685
22.899129	1427.663392	14.449703
22.650565	1425.017560	14.454720
22.728674	1421.552257	14.459738
22.467553	1428.346115	14.464755
22.377280	1425.506197	14.469773
22.712080	1421.651967	14.474791
22.554300	1418.049927	14.479808
22.338185	1416.564000	14.484826
22.412582	1427.190079	14.489843
22.499109	1430.140890	14.494861
22.765085	1444.455759	14.499879
22.648054	1453.240476	14.504896
22.696908	1451.286238	14.509914
22.714399	1456.270351	14.514931
22.643575	1454.637057	14.519949
23.157975	1451.054024	14.524967
22.987228	1452.400362	14.529984
23.215780	1450.887014	14.535002
23.069857	1451.846380	14.540019
23.098202	1445.178655	14.545037
23.209898	1449.935177	14.550055
22.884482	1433.365314	14.555072
22.916360	1420.067604	14.560090
23.037915	1432.092037	14.565107
22.876387	1441.996691	14.570125
22.942681	1443.652420	14.575143
22.651027	1456.289112	14.580160
22.992144	1453.568944	14.585178
23.140646	1454.481372	14.590195
23.026538	1450.849394	14.595213
23.134342	1453.516218	14.600231
22.823355	1458.858257	14.605248
23.179125	1449.114799	14.610266
22.992760	1458.787084	14.615283
22.813734	1461.495214	14.620301
22.917645	1458.875958	14.625319
22.683071	1458.677179	14.630336
23.251237	1470.286844	14.635354
23.401837	1490.388260	14.640371
23.450536	1487.867844	14.645389
23.523923	1486.765389	14.650407
23.249445	1495.262920	14.655424
23.519684	1488.102081	14.660442
23.465374	1497.233980	14.665459
23.470484	1493.658724	14.670477
23.502608	1489.892204	14.675495
23.601961	1489.546003	14.680512
23.432585	1476.353231	14.685530
23.384324	1480.791877	14.690547
23.397357	1482.946556	14.695565
23.731778	1484.622465	14.700583
23.588312	1501.348377	14.705600
23.691191	1493.423236	14.710618
23.685628	1486.049030	14.715635
23.559357	1486.307320	14.720653
23.953979	1484.320174	14.725671
23.637499	1478.972316	14.730688
23.653159	1462.287638	14.735706
23.980723	1465.727102	14.740723
23.793658	1456.967746	14.745741
23.986768	1449.245683	14.750759
23.346641	1462.816231	14.755776
23.572167	1460.935648	14.760794
23.848334	1469.558460	14.765811
23.945736	1491.180568	14.770829
24.203984	1492.922693	14.775847
23.945403	1472.699619	14.780864
24.367151	1458.531406	14.785882
24.117719	1463.427416	14.790899
23.733916	1459.913338	14.795917
24.301791	1454.235101	14.800935
24.021386	1459.890039	14.805952
23.816377	1453.236334	14.810970
23.909893	1458.059761	14.815987
23.569740	1461.420776	14.821005
23.833420	1459.726190	14.826023
23.636628	1481.202644	14.831040
23.972089	1485.138053	14.836058
23.635469	1495.766139	14.841075
23.456643	1491.618422	14.846093
23.838002	1489.756397	14.851111
23.691669	1495.488370	14.856128
23.991449	1501.404119	14.861146
24.263205	1515.591277	14.866163
24.269536	1510.965699	14.871181
24.384254	1515.777634	14.876199
24.380172	1523.094843	14.881216
24.467508	1525.779757	14.886234
24.452252	1508.009272	14.891251
24.311378	1497.641809	14.896269
24.523429	1493.813726	14.901287
24.247849	1500.463623	14.906304
24.447043	1492.631035	14.911322
24.235680	1492.248730	14.916339
24.019622	1510.643172	14.921357
24.448272	1512.697457	14.926375
24.540002	1520.547113	14.931392
24.387251	1512.037775	14.936410
24.477214	1514.737593	14.941427
24.377494	1521.736519	14.946445
24.557710	1515.657749	14.951463
24.315456	1528.530543	14.956480
24.185684	1519.235289	14.961498
24.364566	1524.123635	14.966515
24.280929	1523.051250	14.971533
24.391569	1522.538923	14.976551
24.349883	1552.642144	14.981568
24.673946	1541.098362	14.986586
25.054154	1544.978472	14.991603
24.735839	1558.863255	14.996621
25.253888	1560.944743	15.001639
24.886265	1553.521154	15.006656
24.807232	1541.955925	15.011674
24.736344	1540.418311	15.016691
24.813513	1549.242627	15.021709
24.889692	1552.057819	15.026727
24.808222	1552.014303	15.031744
24.789035	1544.033286	15.036762
24.745066	1555.229411	15.041779
24.599205	1548.422202	15.046797
25.226233	1550.580289	15.051815
24.987412	1551.218939	15.056832
24.599093	1551.508773	15.061850
24.881356	1551.376512	15.066867
24.658469	1565.738299	15.071885
25.290712	1547.692560	15.076903
25.032230	1555.434545	15.081920
25.556052	1548.770809	15.086938
25.681163	1546.145935	15.091955
25.562587	1551.517620	15.096973
25.400155	1538.664192	15.101991
25.334302	1551.704418	15.107008
25.279511	1547.343273	15.112026
25.332349	1543.825971	15.117043
25.277917	1547.549083	15.122061
25.411537	1542.255540	15.127079
25.145064	1548.686155	15.132096
25.356843	1540.798624	15.137114
25.674372	1539.635405	15.142131
25.323308	1549.458833	15.147149
25.521720	1542.811519	15.152167
25.458699	1541.016231	15.157184
25.403545	1544.235476	15.162202
25.735863	1541.755015	15.167219
25.683263	1546.696445	15.172237
25.845367	1545.375997	15.177255
25.718778	1548.509842	15.182272
25.725869	1555.992098	15.187290
26.089305	1542.471670	15.192307
25.577340	1536.944688	15.197325
25.694680	1516.857911	15.202343
25.488204	1521.688694	15.207360
25.736308	1533.213899	15.212378
25.641412	1537.376275	15.217395
25.651014	1548.083632	15.222413
25.645581	1545.784322	15.227431
25.785659	1547.642394	15.232448
25.769587	1546.444237	15.237466
26.037710	1542.975859	15.242483
25.934586	1554.172676	15.247501
25.684960	1548.336116	15.252519
25.631430	1555.485028	15.257536
25.495772	1548.555584	15.262554
25.525507	1557.515216	15.267571
25.539733	1557.543097	15.272589
25.893338	1549.170172	15.277607
25.733704	1550.290179	15.282624
25.680688	1570.719948	15.287642
26.288576	1574.722463	15.292659
26.076241	1579.644829	15.297677
26.358321	1578.832998	15.302695
26.324755	1584.970124	15.307712
26.261646	1579.153940	15.312730
26.091177	1570.648001	15.317747
25.992456	1573.416011	15.322765
26.358403	1571.268794	15.327783
26.524616	1579.380147	15.332800
26.094747	1574.718698	15.337818
26.319987	1571.041501	15.342835
26.200296	1588.965921	15.347853
26.423157	1580.266147	15.352871
26.418673	1585.476140	15.357888
26.350714	1579.658819	15.362906
26.600981	1578.641002	15.367923
26.477766	1585.769589	15.372941
26.557795	1579.077984	15.377959
26.477258	1580.494307	15.382976
26.494377	1577.417027	15.387994
26.551904	1570.948991	15.393011
26.377317	1581.463518	15.398029
26.532265	1572.293844	15.403047
26.527489	1582.100049	15.408064
26.251958	1581.802373	15.413082
26.334688	1572.935664	15.418099
26.299655	1584.330693	15.423117
26.535206	1575.733874	15.428135
26.396517	1588.094418	15.433152
26.304618	1588.354691	15.438170
26.707241	1578.248356	15.443187
26.411179	1592.121085	15.448205
26.533695	1610.523743	15.453223
26.876205	1613.533466	15.458240
26.729235	1612.558556	15.463258
26.770286	1614.439128	15.468275
26.455797	1627.953985	15.473293
26.731769	1611.795051	15.478311
27.288734	1616.272500	15.483328
27.093017	1620.138370	15.488346
27.487332	1615.593106	15.493363
27.251794	1622.436210	15.498381
27.098895	1617.024426	15.503399
27.061154	1615.906365	15.508416
27.124917	1611.333910	15.513434
27.529441	1615.126394	15.518451
27.422100	1621.846325	15.523469
27.399373	1601.336162	15.528487
27.219777	1588.763619	15.533504
26.693988	1594.271287	15.538522
27.079678	1588.574234	15.543539
26.817066	1606.404268	15.548557
27.532772	1619.599161	15.553575
27.140054	1613.923739	15.558592
27.126904	1615.648625	15.563610
27.453958	1616.835601	15.568627
27.571669	1621.429314	15.573645
27.462177	1616.232160	15.578663
27.712860	1610.913404	15.583680
27.345387	1614.756748	15.588698
27.364329	1615.785898	15.593715
27.331064	1618.751378	15.598733
27.433136	1616.206435	15.603751
27.403008	1623.365541	15.608768
27.401051	1624.106904	15.613786
27.679940	1617.589477	15.618803
27.366037	1621.108248	15.623821
27.360000	1619.084258	15.628839
27.426977	1609.163420	15.633856
27.102603	1624.073822	15.638874
27.652805	1626.499451	15.643891
27.432326	1641.998816	15.648909
27.623126	1637.304167	15.653927
27.789837	1645.781258	15.658944
27.600219	1647.275746	15.663962
27.871638	1641.213184	15.668979
27.661461	1653.885676	15.673997
27.778012	1642.664045	15.679015
28.110406	1649.820461	15.684032
27.864453	1647.041057	15.689050
28.259849	1646.132227	15.694067
28.064624	1653.564956	15.699085
27.901121	1657.667071	15.704103
28.149775	1648.873063	15.709120
27.716832	1651.418832	15.714138
27.608609	1640.144000	15.719155
27.869758	1646.127852	15.724173
27.598692	1642.256568	15.729191
27.878414	1648.057689	15.734208
28.273543	1660.813826	15.739226
28.359555	1661.194794	15.744243
28.152494	1656.044674	15.749261
27.924653	1658.255638	15.754279
28.405076	1670.390398	15.759296
28.110777	1679.510788	15.764314
28.380139	1677.685269	15.769331
28.289178	1681.954107	15.774349
28.537384	1682.626594	15.779367
28.780372	1676.506288	15.784384
28.364378	1681.169477	15.789402
28.814622	1663.622580	15.794419
28.261342	1658.534577	15.799437
28.255544	1656.947204	15.804455
28.646471	1665.687079	15.809472
28.273996	1667.679902	15.814490
28.764602	1673.815389	15.819507
28.661307	1676.321574	15.824525
28.685169	1675.329182	15.829543
28.979025	1676.653366	15.834560
28.687695	1681.594427	15.839578
28.851607	1668.912129	15.844595
28.872736	1651.449846	15.849613
28.661192	1646.060707	15.854631
28.908179	1649.700269	15.859648
28.648094	1648.998717	15.864666
28.786092	1658.324928	15.869683
28.876330	1672.273636	15.874701
29.295697	1681.861102	15.879719
29.204006	1654.643423	15.884736
28.999366	1656.208211	15.889754
29.069517	1646.910891	15.894771
28.817885	1652.253843	15.899789
28.899424	1639.601836	15.904807
29.117493	1637.526819	15.909824
29.028306	1648.854400	15.914842
29.054629	1638.381396	15.919859
28.776843	1641.652219	15.924877
28.959884	1660.218594	15.929895
29.218999	1675.838542	15.934912
29.320521	1683.554302	15.939930
29.284057	1670.275972	15.944947
29.362937	1678.748454	15.949965
29.121194	1676.456567	15.954983
29.223667	1676.822113	15.960000
29.253191	1687.221784	15.965018
29.441029	1680.466370	15.970035
29.396987	1681.865027	15.975053
28.974597	1682.636742	15.980071
29.112329	1671.596913	15.985088
29.016145	1679.146153	15.990106
29.192664	1687.143578	15.995123
29.443339	1679.284352	16.000141
29.325111	1681.409589	16.005159
29.475713	1676.912393	16.010176
29.336421	1684.271760	16.015194
29.647761	1672.366636	16.020211
29.668727	1682.473250	16.025229
29.263527	1679.884154	16.030247
29.811500	1691.129689	16.035264
29.259120	1701.766558	16.040282
29.448277	1705.316431	16.045299
29.734601	1711.184168	16.050317
29.486587	1721.909038	16.055335
29.758467	1709.880715	16.060352
29.270671	1717.405769	16.065370
29.467543	1703.673182	16.070387
29.416773	1714.466603	16.075405
29.071236	1731.241187	16.080423
29.654697	1729.456307	16.085440
29.621109	1738.980903	16.090458
29.633950	1744.781356	16.095475
30.087052	1745.116711	16.100493
29.914221	1738.107326	16.105511
30.133145	1728.508826	16.110528
30.098714	1739.469956	16.115546
30.161454	1727.182561	16.120563
30.304234	1732.780789	16.125581
30.150485	1737.439192	16.130599
30.518962	1720.129113	16.135616
30.203597	1727.451358	16.140634
30.516974	1725.563950	16.145651
30.261908	1725.882520	16.150669
30.043356	1726.955547	16.155687
30.292231	1717.670066	16.160704
30.296593	1725.614342	16.165722
30.268728	1731.579662	16.170739
30.464736	1739.608028	16.175757
30.143849	1753.859610	16.180775
30.921956	1749.698557	16.185792
30.926021	1751.061409	16.190810
30.846912	1731.620317	16.195827
30.967124	1732.588012	16.200845
30.735230	1728.631635	16.205863
31.069817	1732.155005	16.210880
31.090350	1734.610042	16.215898
31.216122	1728.591713	16.220915
30.980187	1727.082773	16.225933
30.802904	1721.065219	16.230951
30.785672	1700.216937	16.235968
30.891608	1697.572094	16.240986
30.541188	1697.775501	16.246003
30.822611	1697.172069	16.251021
30.512212	1710.231124	16.256039
30.500873	1722.631364	16.261056
30.354107	1726.295931	16.266074
30.411515	1720.489743	16.271091
30.614573	1723.748227	16.276109
30.450597	1726.007706	16.281127
30.998376	1737.551374	16.286144
30.792285	1757.447724	16.291162
30.753383	1763.360611	16.296179
30.907353	1753.443666	16.301197
30.942392	1766.351010	16.306215
31.173092	1754.890016	16.311232
31.061341	1757.585087	16.316250
31.178058	1755.380958	16.321267
31.081566	1753.330329	16.326285
30.878241	1762.325314	16.331303
31.003434	1757.024481	16.336320
31.109866	1764.014550	16.341338
31.199552	1784.233100	16.346355
31.761307	1794.577419	16.351373
31.531191	1795.593766	16.356391
31.401371	1781.569050	16.361408
31.900016	1780.809459	16.366426
31.716305	1763.600309	16.371443
31.439569	1757.924635	16.376461
31.493671	1767.992941	16.381479
31.625497	1757.435618	16.386496
31.719550	1756.180764	16.391514
31.502239	1755.690403	16.396531
31.946543	1753.546264	16.401549
31.773366	1752.329746	16.406567
31.740591	1753.433135	16.411584
31.795610	1760.834034	16.416602
31.713961	1756.742822	16.421619
31.856394	1752.322210	16.426637
31.440025	1758.021829	16.431655
31.682448	1762.511121	16.436672
31.620252	1776.876262	16.441690
31.690630	1785.449483	16.446707
31.956295	1784.920018	16.451725
31.965132	1790.397120	16.456743
31.769640	1790.877938	16.461760
31.849514	1794.809605	16.466778
31.369940	1792.902614	16.471795
31.977918	1787.854863	16.476813
31.895395	1800.105537	16.481831
32.179619	1810.920338	16.486848
32.067440	1814.421890	16.491866
32.350126	1824.531365	16.496883
32.783863	1816.192598	16.501901
32.751304	1799.394159	16.506919
32.966761	1785.627602	16.511936
32.787802	1785.340926	16.516954
32.533961	1788.271807	16.521971
32.568181	1780.214181	16.526989
32.507294	1783.329721	16.532007
32.313992	1775.537514	16.537024
32.390740	1776.376821	16.542042
32.414705	1785.294655	16.547059
32.725283	1777.110899	16.552077
32.491695	1785.303114	16.557095
32.823487	1777.249988	16.562112
32.581059	1783.018229	16.567130
32.252874	1781.001022	16.572147
32.469676	1771.426878	16.577165
32.458057	1785.050984	16.582183
32.454771	1775.984314	16.587200
32.400168	1772.133765	16.592218
32.232587	1780.652103	16.597235
32.517516	1784.807302	16.602253
32.549242	1803.534059	16.607271
32.738000	1804.338413	16.612288
32.548879	1808.744603	16.617306
32.638274	1817.584300	16.622323
33.040076	1815.933720	16.627341
32.634478	1816.172575	16.632359
32.686851	1811.286228	16.637376
32.483694	1814.911659	16.642394
32.711981	1833.790994	16.647411
33.037227	1844.603509	16.652429
32.938060	1844.685089	16.657447
33.168479	1841.961391	16.662464
33.124477	1846.653772	16.667482
32.737233	1851.357756	16.672499
33.115238	1846.619528	16.677517
33.462178	1850.926338	16.682535
33.044569	1844.118343	16.687552
33.068538	1847.118546	16.692570
33.111221	1850.043879	16.697587
33.447759	1855.731780	16.702605
33.683651	1866.925031	16.707623
33.687120	1863.120416	16.712640
33.904063	1855.731905	16.717658
33.776326	1854.684382	16.722675
33.475011	1846.142846	16.727693
33.748638	1842.660860	16.732711
33.453167	1854.822088	16.737728
33.662614	1846.328429	16.742746
33.431242	1855.316069	16.747763
33.756600	1844.392000	16.752781
33.545738	1845.948817	16.757799
33.426768	1858.140423	16.762816
33.558734	1860.635437	16.767834
33.475579	1875.281856	16.772851
34.124131	1861.012969	16.777869
34.099526	1862.997359	16.782887
34.181702	1867.916964	16.787904
34.628089	1861.190774	16.792922
34.463733	1859.226973	16.797939
34.362519	1842.597759	16.802957
34.151823	1844.540816	16.807975
33.976060	1836.214796	16.812992
34.257631	1848.498764	16.818010
34.148383	1842.763630	16.823027
34.484340	1838.150739	16.828045
34.210444	1838.071308	16.833063
34.097429	1834.529615	16.838080
34.285646	1834.078396	16.843098
34.106836	1839.316788	16.848115
34.146113	1837.976819	16.853133
33.807668	1841.114365	16.858151
33.915296	1846.294592	16.863168
34.251040	1851.270728	16.868186
33.869807	1864.437737	16.873203
34.064203	1851.747703	16.878221
34.404542	1860.946417	16.883239
33.820619	1859.918441	16.888256
34.256212	1870.822699	16.893274
34.250182	1889.079199	16.898291
34.600536	1895.885362	16.903309
34.526799	1906.326508	16.908327
34.562647	1905.069415	16.913344
34.619142	1899.849613	16.918362
34.361768	1899.980368	16.923379
34.697304	1890.255069	16.928397
34.903989	1891.700925	16.933415
34.547771	1896.361802	16.938432
34.876658	1893.514506	16.943450
34.656397	1900.202730	16.948467
34.843990	1910.126177	16.953485
35.025280	1927.202032	16.958503
34.914347	1929.451264	16.963520
35.113390	1928.736735	16.968538
34.968439	1933.477951	16.973555
34.796207	1928.589126	16.978573
35.332040	1927.099831	16.983591
35.455258	1926.873561	16.988608
35.600173	1915.343290	16.993626
35.288001	1920.371080	16.998643
35.557836	1910.975185	17.003661
35.567546	1899.471256	17.008679
35.177502	1895.307670	17.013696
35.377457	1889.855768	17.018714
35.055281	1901.733386	17.023731
35.221720	1923.256841	17.028749
35.597779	1920.677079	17.033767
35.338019	1924.421310	17.038784
35.443171	1921.849408	17.043802
35.541192	1921.616828	17.048819
35.553307	1913.977938	17.053837
35.454473	1922.022695	17.058855
35.361403	1930.758683	17.063872
35.817504	1915.549783	17.068890
35.249698	1928.599996	17.073907
35.525124	1922.397252	17.078925
35.556826	1926.941227	17.083943
35.591650	1925.478375	17.088960
35.531492	1929.404948	17.093978
35.629899	1953.511310	17.098995
36.127667	1956.335799	17.104013
35.890149	1956.415111	17.109031
35.683964	1956.793817	17.114048
36.609922	1952.018309	17.119066
36.583541	1960.367634	17.124083
36.145078	1937.692976	17.129101
36.107234	1925.862886	17.134119
35.758593	1924.952459	17.139136
35.939400	1938.926039	17.144154
36.011693	1947.318682	17.149171
36.126488	1944.356884	17.154189
36.295607	1952.554559	17.159207
36.012841	1952.490035	17.164224
36.655020	1953.004818	17.169242
36.512611	1954.532977	17.174259
36.488691	1946.052501	17.179277
36.329109	1944.840725	17.184295
36.240057	1946.051427	17.189312
36.326042	1946.319794	17.194330
36.250265	1949.624952	17.199347
36.517171	1942.912176	17.204365
36.682338	1946.393373	17.209383
36.223674	1952.728348	17.214400
36.576647	1949.660349	17.219418
36.425020	1951.734648	17.224435
36.371330	1966.311130	17.229453
36.918422	1969.499261	17.234471
36.929444	1978.376899	17.239488
37.265970	1973.549276	17.244506
36.944260	1969.217634	17.249523
36.791263	1959.945394	17.254541
36.961916	1968.376703	17.259559
36.653832	1980.786287	17.264576
37.355772	1973.202347	17.269594
37.283550	1978.310684	17.274611
37.297055	1976.715245	17.279629
37.379262	1954.109186	17.284647
37.304919	1953.322617	17.289664
37.410596	1946.124029	17.294682
36.988090	1947.839600	17.299699
36.974430	1954.171121	17.304717
37.237385	1943.858943	17.309735
37.199614	1944.221766	17.314752
37.074908	1961.906102	17.319770
37.016852	1970.954655	17.324787
36.737956	1981.480639	17.329805
37.262807	1978.265433	17.334823
36.958375	1974.916785	17.339840
37.126291	1966.723528	17.344858
37.212517	1987.558764	17.349875
37.216448	2002.067124	17.354893
37.381921	2009.240513	17.359911
37.179359	2024.098120	17.364928
37.343940	2010.094387	17.369946
37.631775	2005.705476	17.374963
37.457637	2009.291326	17.379981
37.453600	2012.066016	17.384999
37.733718	2017.931784	17.390016
37.725216	2027.312864	17.395034
37.783426	2035.792627	17.400051
37.636691	2039.559244	17.405069
37.918510	2034.540955	17.410087
37.673542	2041.111804	17.415104
38.088912	2038.573321	17.420122
38.049049	2041.466380	17.425139
38.069810	2036.227853	17.430157
38.294670	2031.232718	17.435175
38.454577	2034.217132	17.440192
38.562669	2028.792744	17.445210
38.373166	2039.999205	17.450227
38.494853	2033.149850	17.455245
38.325721	2035.701242	17.460263
37.956177	2036.894285	17.465280
38.532608	2035.103492	17.470298
38.314400	2031.963306	17.475315
38.441327	2033.311811	17.480333
38.412028	2034.898155	17.485351
38.409267	2036.537437	17.490368
38.528713	2035.320732	17.495386
38.430849	2033.263213	17.500403
38.395666	2041.527858	17.505421
38.630828	2033.387219	17.510439
38.319807	2035.703060	17.515456
38.518389	2034.573588	17.520474
38.930484	2041.314891	17.525491
38.497386	2040.698897	17.530509
38.706364	2058.491113	17.535527
38.673144	2061.223959	17.540544
38.599905	2071.547397	17.545562
38.783121	2070.372519	17.550579
39.110965	2063.846121	17.555597
39.125837	2069.447500	17.560615
39.045985	2071.894601	17.565632
38.952268	2060.358675	17.570650
39.036662	2065.117309	17.575667
39.126558	2077.356357	17.580685
39.117740	2071.876005	17.585703
39.002103	2069.426198	17.590720
39.056891	2069.831824	17.595738
39.106575	2071.737353	17.600755
39.062999	2071.308151	17.605773
39.143022	2070.546297	17.610791
39.232215	2088.485086	17.615808
38.983235	2097.776319	17.620826
39.579867	2101.013079	17.625843
39.559366	2099.493940	17.630861
39.823491	2096.522653	17.635879
39.778492	2097.291107	17.640896
39.918448	2094.078082	17.645914
40.180187	2100.315587	17.650931
40.035470	2083.447479	17.655949
40.038914	2068.175471	17.660967
39.700476	2070.807478	17.665984
39.335183	2057.248144	17.671002
40.030039	2058.016140	17.676019
39.755735	2064.773550	17.681037
40.009468	2060.611761	17.686055
39.905786	2061.138665	17.691072
39.810935	2053.397165	17.696090
39.954373	2057.370763	17.701107
39.909130	2082.795439	17.706125
39.997682	2088.922850	17.711143
39.808462	2088.513500	17.716160
39.912713	2090.988103	17.721178
40.036261	2087.071494	17.726195
39.988783	2095.750537	17.731213
40.199305	2087.077405	17.736231
39.914522	2097.407598	17.741248
39.686388	2094.446293	17.746266
40.466917	2101.700911	17.751283
40.439592	2116.113541	17.756301
40.514961	2110.579365	17.761319
40.445221	2122.789905	17.766336
40.250662	2123.919484	17.771354
41.154655	2118.269223	17.776371
40.512006	2116.390150	17.781389
40.808220	2115.450262	17.786407
40.583840	2117.823711	17.791424
40.455156	2123.156768	17.796442
41.215878	2116.168673	17.801459
40.983421	2120.074434	17.806477
41.146675	2116.713688	17.811495
41.160494	2108.571190	17.816512
41.119573	2096.449726	17.821530
40.951152	2086.575639	17.826547
40.669958	2091.784812	17.831565
40.725048	2091.892314	17.836583
40.888209	2117.912506	17.841600
41.080826	2119.115092	17.846618
41.347029	2109.484235	17.851635
41.574506	2125.454988	17.856653
41.415772	2121.673789	17.861671
41.565390	2120.920475	17.866688
40.975644	2112.060870	17.871706
41.150231	2103.673064	17.876723
41.269475	2117.784148	17.881741
41.509854	2116.603404	17.886759
41.411427	2128.498350	17.891776
41.172318	2120.112163	17.896794
41.434949	2121.965831	17.901811
41.114585	2128.204318	17.906829
41.285315	2123.423189	17.911847
41.075138	2128.882046	17.916864
40.827787	2131.387013	17.921882
41.217798	2145.554469	17.926899
41.570066	2160.508050	17.931917
41.109713	2155.479943	17.936935
41.141408	2155.724153	17.941952
40.974034	2172.064664	17.946970
41.450065	2188.673674	17.951987
41.636731	2196.178210	17.957005
42.190916	2184.012134	17.962023
42.051863	2179.968453	17.967040
41.841260	2179.839972	17.972058
41.869007	2178.237345	17.977075
41.728443	2182.714853	17.982093
42.187166	2189.602579	17.987111
42.522440	2208.895976	17.992128
42.745570	2196.625210	17.997146
42.577149	2177.799358	18.002163
42.256594	2183.844958	18.007181
42.723440	2178.746074	18.012199
42.475448	2177.745136	18.017216
42.640950	2176.893807	18.022234
42.576233	2174.462029	18.027251
42.546028	2179.816020	18.032269
42.981289	2176.399175	18.037287
42.446469	2181.137220	18.042304
42.476912	2186.153996	18.047322
42.831951	2172.945537	18.052339
42.643672	2183.089531	18.057357
42.191604	2181.643196	18.062375
42.599103	2175.390539	18.067392
42.525739	2190.373811	18.072410
42.617918	2193.725431	18.077427
42.813640	2213.074261	18.082445
43.006602	2208.325521	18.087463
43.080547	2213.578978	18.092480
43.243979	2219.699114	18.097498
43.508649	2208.880487	18.102515
43.458343	2215.450715	18.107533
42.620528	2207.919999	18.112551
43.309751	2208.616124	18.117568
43.464041	2218.521852	18.122586
43.046228	2213.424219	18.127603
42.823654	2209.061730	18.132621
42.851262	2206.391250	18.137639
43.039255	2213.325404	18.142656
43.092170	2212.094892	18.147674
43.499603	2205.625667	18.152691
43.087421	2213.725085	18.157709
43.376711	2224.881875	18.162727
43.433550	2235.762732	18.167744
43.592236	2241.085146	18.172762
43.433961	2239.321465	18.177779
43.383225	2234.720027	18.182797
43.699258	2231.881176	18.187815
43.657145	2234.825844	18.192832
43.413945	2236.948169	18.197850
44.130571	2239.271339	18.202867
43.813656	2233.884705	18.207885
43.474700	2239.685413	18.212903
43.660203	2238.729061	18.217920
43.813287	2260.369067	18.222938
43.883341	2259.694752	18.227955
44.098004	2264.888662	18.232973
44.448677	2264.531644	18.237991
44.356305	2254.468795	18.243008
44.197804	2261.195409	18.248026
44.570413	2260.677126	18.253043
44.155785	2269.283367	18.258061
44.605870	2260.827766	18.263079
44.574499	2262.196345	18.268096
44.358225	2253.878623	18.273114
44.352761	2255.619981	18.278131
44.374103	2263.561618	18.283149
44.422169	2262.809171	18.288167
44.570132	2257.217609	18.293184
44.301001	2269.067114	18.298202
44.489481	2260.246068	18.303219
44.590045	2261.119513	18.308237
44.149456	2260.647728	18.313255
44.906425	2264.003512	18.318272
44.262048	2275.426733	18.323290
44.740012	2288.483010	18.328307
44.742314	2298.589677	18.333325
44.664409	2299.841808	18.338343
45.258525	2292.220684	18.343360
44.754945	2296.429704	18.348378
44.982481	2291.067832	18.353395
44.961805	2291.891189	18.358413
45.109142	2293.958375	18.363431
45.214678	2290.656315	18.368448
45.076455	2297.973259	18.373466
45.026777	2299.278827	18.378483
45.599314	2313.967983	18.383501
45.961777	2305.978632	18.388519
45.343693	2299.767886	18.393536
45.350967	2299.944621	18.398554
45.674179	2296.300467	18.403571
45.460357	2305.036891	18.408589
45.479108	2307.157627	18.413607
45.672009	2299.150100	18.418624
45.492439	2312.871186	18.423642
45.593287	2301.492304	18.428659
45.540476	2306.105218	18.433677
45.765710	2304.711276	18.438695
46.003797	2296.787356	18.443712
45.725231	2308.389651	18.448730
45.786127	2306.093033	18.453747
45.995059	2313.103969	18.458765
45.616177	2316.597807	18.463783
45.930795	2311.274548	18.468800
45.701897	2318.725177	18.473818
46.056619	2327.419261	18.478835
46.398933	2339.093895	18.483853
46.158399	2340.845640	18.488871
46.762012	2343.769396	18.493888
46.120428	2335.130789	18.498906
45.895442	2328.504548	18.503923
45.900707	2340.673259	18.508941
46.266509	2353.829936	18.513959
46.521402	2344.251671	18.518976
46.313733	2354.049438	18.523994
46.547478	2346.632616	18.529011
46.689577	2346.093213	18.534029
46.168733	2346.895224	18.539047
46.576271	2343.631939	18.544064
46.423153	2355.301751	18.549082
46.440482	2368.207114	18.554099
46.645463	2370.818058	18.559117
46.477679	2380.581440	18.564135
47.036725	2370.341465	18.569152
46.725893	2375.064790	18.574170
47.025784	2369.848778	18.579187
47.191972	2375.634592	18.584205
47.283330	2373.522535	18.589223
47.720682	2362.800988	18.594240
47.562902	2365.074852	18.599258
47.459779	2364.906678	18.604275
47.865019	2362.094248	18.609293
47.543918	2369.432342	18.614311
47.340067	2368.648267	18.619328
47.309837	2372.602108	18.624346
47.593001	2367.325962	18.629363
47.222879	2365.530861	18.634381
47.215899	2368.771153	18.639399
47.546575	2361.651928	18.644416
47.515498	2361.455651	18.649434
47.238645	2368.701106	18.654451
47.547319	2357.210161	18.659469
47.288735	2361.700867	18.664487
47.532599	2383.056144	18.669504
47.467434	2393.283117	18.674522
47.991980	2402.885285	18.679539
47.658040	2404.428606	18.684557
47.507935	2404.660676	18.689575
47.663200	2405.585390	18.694592
47.819570	2405.156155	18.699610
48.051862	2422.953845	18.704627
48.384168	2421.516334	18.709645
48.321567	2426.422348	18.714663
48.517901	2421.046880	18.719680
48.171384	2417.836474	18.724698
48.365381	2423.032404	18.729715
48.526008	2416.953496	18.734733
48.028692	2422.842062	18.739751
48.620025	2426.645246	18.744768
48.312174	2428.924373	18.749786
48.161997	2434.217905	18.754803
48.270639	2425.093082	18.759821
48.482717	2425.263054	18.764839
48.765551	2421.130440	18.769856
48.635277	2418.637411	18.774874
48.692679	2427.390403	18.779891
48.792668	2420.990340	18.784909
48.601395	2429.589087	18.789927
48.833406	2426.083395	18.794944
48.620453	2446.758690	18.799962
49.023314	2453.467892	18.804979
49.273627	2455.467830	18.809997
49.151379	2462.225327	18.815015
49.485277	2454.545574	18.820032
49.548501	2463.264511	18.825050
49.309331	2449.200850	18.830067
49.690023	2441.567419	18.835085
49.482637	2437.187299	18.840103
49.503643	2423.429504	18.845120
49.179556	2419.148150	18.850138
48.654657	2429.116908	18.855155
49.237565	2436.741055	18.860173
49.032616	2453.756914	18.865191
49.175595	2460.197239	18.870208
49.349093	2458.265607	18.875226
49.421538	2473.466709	18.880243
49.948077	2474.464803	18.885261
49.892666	2487.648921	18.890279
50.028520	2474.205304	18.895296
50.157389	2480.454324	18.900314
50.133577	2478.997537	18.905331
50.438822	2480.858118	18.910349
50.108242	2468.195380	18.915367
50.381063	2451.435632	18.920384
50.257716	2453.624852	18.925402
49.690234	2449.014294	18.930419
50.082847	2462.307434	18.935437
50.009458	2475.086684	18.940455
50.140422	2484.233461	18.945472
50.314712	2481.102280	18.950490
50.102022	2488.435230	18.955507
50.088626	2485.896163	18.960525
49.953638	2494.059240	18.965543
50.284165	2491.807720	18.970560
50.268988	2506.508831	18.975578
50.190791	2509.955883	18.980595
50.112565	2507.374375	18.985613
50.254323	2514.867076	18.990631
50.557779	2515.764815	18.995648
50.776096	2527.418322	19.000666
50.420941	2540.804296	19.005683
51.005152	2537.196455	19.010701
51.021308	2541.013229	19.015719
50.952762	2545.816344	19.020736
50.945791	2541.212825	19.025754
51.146086	2548.854588	19.030771
51.163956	2534.097064	19.035789
50.915541	2543.464065	19.040807
51.428874	2538.754014	19.045824
51.451765	2534.762804	19.050842
51.434831	2544.774486	19.055859
51.625812	2541.604205	19.060877
51.357956	2540.479855	19.065895
51.713226	2541.170253	19.070912
51.672321	2540.524401	19.075930
51.536024	2546.514134	19.080947
51.829695	2532.360617	19.085965
51.678534	2542.655984	19.090983
51.825321	2534.860216	19.096000
51.715037	2534.992531	19.101018
51.302323	2543.388320	19.106035
51.773709	2544.232856	19.111053
51.959007	2550.150914	19.116071
52.040044	2557.130335	19.121088
52.367924	2553.463271	19.126106
52.326431	2551.471623	19.131123
52.200798	2536.189001	19.136141
51.898351	2545.131335	19.141159
52.301268	2558.637788	19.146176
52.600232	2564.430046	19.151194
52.227835	2554.081101	19.156211
52.214803	2558.819574	19.161229
52.286858	2575.732945	19.166247
52.156344	2578.712522	19.171264
52.382792	2569.899757	19.176282
52.174957	2570.192129	19.181299
52.215784	2566.828652	19.186317
52.359322	2562.678931	19.191335
52.348017	2577.583416	19.196352
52.751375	2586.748917	19.201370
52.703312	2596.150115	19.206387
53.155871	2587.015847	19.211405
52.878533	2588.909385	19.216423
53.070375	2582.517923	19.221440
53.355234	2576.607450	19.226458
53.179349	2585.851786	19.231475
53.237493	2574.946250	19.236493
53.169206	2579.994255	19.241511
52.951989	2581.876697	19.246528
53.248671	2573.070789	19.251546
53.155072	2581.956862	19.256563
53.298753	2582.703227	19.261581
53.134552	2578.240848	19.266599
53.403187	2580.611741	19.271616
53.352402	2582.312078	19.276634
53.206955	2585.066620	19.281651
53.471568	2595.769559	19.286669
53.450315	2611.526323	19.291687
53.587265	2617.358979	19.296704
53.904498	2614.168613	19.301722
53.563165	2615.871516	19.306739
54.103367	2612.166462	19.311757
53.592881	2613.698332	19.316775
53.568897	2613.458308	19.321792
54.045307	2614.210632	19.326810
53.806695	2619.104355	19.331827
54.006953	2612.907535	19.336845
53.840252	2614.307221	19.341863
53.749774	2632.684989	19.346880
54.181920	2646.174693	19.351898
54.074331	2650.530123	19.356915
54.258758	2646.588369	19.361933
54.248924	2647.599682	19.366951
54.121960	2641.043132	19.371968
54.611553	2645.951407	19.376986
54.340799	2647.933603	19.382003
54.300274	2637.282777	19.387021
54.459319	2659.334195	19.392039
54.838434	2666.569699	19.397056
55.136616	2672.914986	19.402074
54.731420	2675.180124	19.407091
54.900057	2675.348885	19.412109
54.833180	2675.224896	19.417127
54.842404	2671.647878	19.422144
55.336191	2667.169529	19.427162
54.835326	2679.682805	19.432179
54.965600	2663.674960	19.437197
54.915632	2668.930126	19.442215
54.734573	2677.702091	19.447232
54.950790	2687.752644	19.452250
55.052007	2704.744632	19.457267
54.927349	2704.760494	19.462285
55.219085	2704.414361	19.467303
55.295018	2712.896570	19.472320
55.450604	2708.711669	19.477338
55.274778	2712.270796	19.482355
55.487432	2721.009147	19.487373
56.211125	2726.764873	19.492391
56.177912	2724.529219	19.497408
56.541860	2701.700521	19.502426
56.216399	2701.557075	19.507443
56.399876	2690.269276	19.512461
56.425780	2694.018262	19.517479
56.241130	2694.008183	19.522496
56.559701	2695.190006	19.527514
56.234828	2689.361980	19.532531
56.297816	2687.257895	19.537549
56.309613	2696.562260	19.542567
56.128295	2689.905540	19.547584
56.610209	2687.441390	19.552602
56.351970	2685.796389	19.557619
56.141329	2689.532377	19.562637
56.200398	2693.685987	19.567655
56.541747	2693.592025	19.572672
56.616901	2683.600984	19.577690
56.237085	2691.669894	19.582707
56.211072	2688.113878	19.587725
56.490740	2695.667287	19.592743
56.115851	2721.199130	19.597760
56.559821	2720.778068	19.602778
56.371004	2726.441381	19.607795
56.617548	2722.025094	19.612813
56.985207	2735.919704	19.617831
56.883043	2745.475174	19.622848
57.106078	2750.473287	19.627866
56.887903	2756.195984	19.632883
57.233666	2748.936966	19.637901
57.254491	2742.166023	19.642919
57.381360	2746.818352	19.647936
57.358272	2734.515352	19.652954
57.354418	2750.276359	19.657971
57.387141	2741.775503	19.662989
57.463967	2739.479241	19.668007
57.164471	2753.681986	19.673024
57.579037	2756.909938	19.678042
57.380855	2778.358868	19.683059
57.332547	2781.417320	19.688077
57.623420	2781.105198	19.693095
57.562487	2786.035452	19.698112
57.673559	2787.618280	19.703130
58.003275	2801.000460	19.708147
58.165758	2808.261359	19.713165
58.575557	2808.329709	19.718183
58.182517	2809.742229	19.723200
58.380768	2806.113871	19.728218
58.331164	2808.737037	19.733235
58.200255	2809.591921	19.738253
58.414935	2810.952226	19.743271
58.342729	2815.863157	19.748288
58.584064	2804.163708	19.753306
58.207357	2805.597841	19.758323
58.306943	2811.800823	19.763341
58.570414	2811.462685	19.768359
58.131167	2814.654323	19.773376
58.669648	2823.166758	19.778394
58.372162	2842.312682	19.783411
58.818604	2838.154272	19.788429
58.560570	2840.827354	19.793447
58.443021	2844.130804	19.798464
58.778075	2846.072162	19.803482
59.217698	2858.320376	19.808499
59.315730	2866.879210	19.813517
59.427646	2872.777682	19.818535
59.091410	2872.653407	19.823552
59.567937	2866.698940	19.828570
59.352413	2864.085784	19.833587
59.637293	2869.823080	19.838605
59.592306	2864.173028	19.843623
59.569558	2866.534070	19.848640
59.830360	2857.460088	19.853658
59.694395	2866.452816	19.858675
59.630591	2865.982563	19.863693
59.783411	2863.917394	19.868711
59.781011	2872.840760	19.873728
59.926675	2867.397436	19.878746
59.890473	2863.617100	19.883763
60.009007	2871.314779	19.888781
60.112128	2857.941813	19.893799
59.905734	2869.617201	19.898816
60.382012	2863.724994	19.903834
60.103273	2861.331378	19.908851
59.783910	2869.516810	19.913869
60.082230	2859.844156	19.918887
60.104184	2883.003061	19.923904
60.338990	2878.161891	19.928922
60.420202	2893.990363	19.933939
60.155740	2899.687970	19.938957
60.563531	2895.933885	19.943975
60.719907	2898.229569	19.948992
60.938889	2892.756339	19.954010
60.598880	2896.905970	19.959027
60.845459	2894.362429	19.964045
60.847900	2893.075152	19.969063
60.355756	2900.820841	19.974080
60.838560	2913.645272	19.979098
61.027600	2917.904241	19.984115
60.787305	2929.649278	19.989133
60.868269	2914.534056	19.994151
61.228978	2922.833670	19.999168
61.256723	2925.233316	20.004186
61.785100	2939.482516	20.009203
61.324715	2937.136569	20.014221
61.600154	2934.972401	20.019239
61.636480	2949.457969	20.024256
61.871015	2949.665839	20.029274
62.046787	2947.663667	20.034291
61.393811	2950.763605	20.039309
61.823938	2947.687701	20.044327
61.987527	2955.674605	20.049344
62.171766	2946.757034	20.054362
62.249001	2953.751459	20.059379
62.006026	2949.738784	20.064397
62.108230	2946.386755	20.069415
62.017106	2949.277743	20.074432
62.213896	2951.704327	20.079450
62.268327	2949.305555	20.084467
61.942683	2959.650798	20.089485
62.326303	2954.813230	20.094503
62.676235	2952.919807	20.099520
62.629309	2950.526598	20.104538
62.867956	2952.975146	20.109555
62.144230	2951.887969	20.114573
62.369305	2946.454630	20.119591
62.337751	2950.173363	20.124608
62.564932	2956.090695	20.129626
62.865299	2974.645995	20.134643
62.831850	2976.121311	20.139661
62.597446	2977.817732	20.144679
62.523333	2982.739281	20.149696
62.598181	2968.902472	20.154714
62.912463	2987.466426	20.159731
62.934256	3007.834441	20.164749
63.145078	2997.790801	20.169767
63.108260	3017.154503	20.174784
63.413919	3012.991833	20.179802
63.451660	3014.149375	20.184819
63.424248	3010.153280	20.189837
63.764164	3006.979424	20.194855
63.459755	3013.430526	20.199872
63.731495	3005.050786	20.204890
63.736686	3004.070175	20.209907
63.450288	3004.963542	20.214925
63.498372	3009.145107	20.219943
64.069655	3035.260268	20.224960
64.123343	3033.829520	20.229978
64.219058	3035.675689	20.234995
64.241278	3031.585236	20.240013
64.318140	3027.161729	20.245031
64.411611	3032.568837	20.250048
64.232654	3030.310873	20.255066
64.362091	3020.853728	20.260083
64.065361	3032.127318	20.265101
64.201101	3019.032932	20.270119
64.024193	3031.569699	20.275136
64.230396	3038.593242	20.280154
64.851472	3058.143472	20.285171
64.702832	3066.678551	20.290189
64.940840	3061.631223	20.295207
65.040100	3068.335251	20.300224
64.811195	3066.808826	20.305242
65.140419	3061.782874	20.310259
64.949524	3066.106236	20.315277
65.020743	3066.397238	20.320295
64.820033	3065.616525	20.325312
64.877799	3064.238630	20.330330
65.196109	3062.804251	20.335347
65.031462	3087.124023	20.340365
65.465417	3082.576273	20.345383
65.311829	3093.815915	20.350400
65.089867	3085.604258	20.355418
65.481277	3089.908910	20.360435
65.444693	3097.731740	20.365453
65.344277	3083.697274	20.370471
65.401699	3099.140975	20.375488
65.687039	3116.342048	20.380506
65.893092	3108.895752	20.385523
65.747359	3125.489500	20.390541
66.125176	3120.988378	20.395559
66.279688	3125.317117	20.400576
66.148431	3128.448137	20.405594
66.508393	3118.241027	20.410611
65.948584	3124.454014	20.415629
66.267798	3117.178903	20.420647
66.043754	3123.146883	20.425664
65.914169	3127.419584	20.430682
66.518699	3129.701472	20.435699
66.271368	3140.109012	20.440717
66.293810	3148.787281	20.445735
66.494053	3153.661057	20.450752
66.796844	3150.495900	20.455770
66.987259	3146.131648	20.460787
66.901345	3153.588870	20.465805
67.178246	3137.237229	20.470823
66.842499	3146.736119	20.475840
66.825946	3148.497591	20.480858
67.135988	3152.086926	20.485875
67.339453	3172.215301	20.490893
67.444160	3173.544877	20.495911
67.504624	3177.188032	20.500928
67.523546	3177.456500	20.505946
67.847306	3163.298047	20.510963
67.693271	3169.297357	20.515981
68.181706	3170.107505	20.520999
67.799145	3153.691708	20.526016
67.783051	3140.696497	20.531034
68.104532	3138.620490	20.536051
67.855603	3140.421014	20.541069
67.949564	3140.134772	20.546087
68.121244	3156.008640	20.551104
68.157476	3167.123645	20.556122
68.196072	3162.032504	20.561139
68.419096	3163.555224	20.566157
68.796601	3159.214809	20.571175
68.529242	3167.365488	20.576192
68.379910	3167.835279	20.581210
68.649483	3165.947734	20.586227
68.594754	3173.935164	20.591245
68.585357	3167.731542	20.596263
68.460254	3167.288329	20.601280
68.358135	3171.651628	20.606298
68.572855	3168.816594	20.611315
68.671379	3172.484726	20.616333
68.827022	3160.240532	20.621351
68.689014	3162.730851	20.626368
68.670297	3189.984647	20.631386
68.648765	3189.863118	20.636403
68.771620	3198.693525	20.641421
68.813856	3187.128736	20.646439
68.716794	3196.934839	20.651456
68.796401	3218.076843	20.656474
68.875810	3223.700647	20.661491
68.976911	3229.695616	20.666509
69.138037	3230.399645	20.671527
69.496299	3242.914132	20.676544
69.512916	3251.948650	20.681562
69.634846	3252.753121	20.686579
69.640717	3263.847409	20.691597
69.535494	3257.252220	20.696615
69.556698	3254.701584	20.701632
69.553414	3262.407739	20.706650
69.926646	3266.624986	20.711667
70.152898	3274.286280	20.716685
70.157555	3279.068404	20.721703
70.493843	3275.020913	20.726720
70.042405	3277.939083	20.731738
70.484872	3284.006283	20.736755
70.403179	3279.792606	20.741773
70.430972	3277.646435	20.746791
70.593385	3279.439457	20.751808
70.582731	3295.755052	20.756826
70.958068	3295.027567	20.761843
70.759706	3296.751707	20.766861
70.848160	3295.862338	20.771879
71.067419	3299.579107	20.776896
71.258605	3301.883058	20.781914
71.369752	3291.060872	20.786931
71.123107	3302.018915	20.791949
71.273144	3297.953733	20.796967
71.308530	3293.572703	20.801984
71.030877	3298.615091	20.807002
71.909308	3297.904524	20.812019
71.519092	3297.228746	20.817037
71.727242	3299.401415	20.822055
72.095654	3291.430239	20.827072
71.812576	3297.659641	20.832090
71.751550	3280.668787	20.837107
71.589959	3295.395737	20.842125
71.714391	3292.891189	20.847143
71.442731	3306.591125	20.852160
71.762979	3319.658767	20.857178
71.621110	3323.839905	20.862195
71.767392	3332.496255	20.867213
71.689249	3340.001850	20.872231
72.021476	3351.060724	20.877248
71.787568	3360.936070	20.882266
72.068344	3349.431862	20.887283
72.231049	3379.709886	20.892301
72.479620	3388.717316	20.897319
72.717548	3385.404144	20.902336
72.841036	3391.522924	20.907354
72.850427	3386.097272	20.912371
72.948625	3388.344722	20.917389
72.837077	3387.814119	20.922407
73.262755	3391.363995	20.927424
73.142215	3390.712071	20.932442
73.250015	3382.406706	20.937459
73.766595	3390.778294	20.942477
73.546266	3394.457827	20.947495
73.789426	3383.219944	20.952512
73.425075	3387.454995	20.957530
73.422785	3380.711369	20.962547
73.460983	3382.137423	20.967565
73.372914	3386.303841	20.972583
73.532343	3379.357647	20.977600
73.889842	3391.764487	20.982618
73.909873	3406.973115	20.987635
74.216607	3407.763237	20.992653
74.221986	3415.127747	20.997671
73.946676	3405.268004	21.002688
73.827066	3423.661927	21.007706
74.036545	3414.556260	21.012723
73.829658	3415.447041	21.017741
73.757451	3420.510951	21.022759
74.065132	3421.622243	21.027776
74.166979	3443.911390	21.032794
74.387604	3450.039530	21.037811
74.491504	3448.923044	21.042829
74.338581	3456.584854	21.047847
74.719875	3444.287577	21.052864
74.755150	3459.892158	21.057882
74.750371	3463.630837	21.062899
75.325733	3472.119191	21.067917
74.978949	3486.009366	21.072935
74.935264	3472.466517	21.077952
74.576097	3476.355741	21.082970
75.107707	3477.460937	21.087987
75.209066	3479.235308	21.093005
75.425175	3500.358227	21.098023
75.546413	3503.816195	21.103040
75.350507	3509.002939	21.108058
75.587007	3511.055790	21.113075
75.513462	3514.788943	21.118093
75.574921	3507.820111	21.123111
75.657866	3509.689791	21.128128
75.969257	3511.577798	21.133146
76.166126	3528.133707	21.138163
76.245858	3527.040262	21.143181
76.407959	3538.742751	21.148199
76.541270	3533.178453	21.153216
76.100035	3535.315999	21.158234
76.373321	3531.176071	21.163251
76.745327	3530.241226	21.168269
76.452198	3535.866004	21.173287
76.735958	3532.477999	21.178304
76.824780	3536.948065	21.183322
76.851167	3534.537472	21.188339
77.077741	3535.332680	21.193357
76.796419	3539.528333	21.198375
77.234219	3532.076760	21.203392
77.306983	3537.706541	21.208410
77.166599	3544.265201	21.213427
77.259559	3525.845781	21.218445
77.314243	3540.809959	21.223463
77.385228	3534.751505	21.228480
77.510134	3531.856197	21.233498
77.247734	3522.402136	21.238515
77.500249	3524.167137	21.243533
77.241504	3533.626279	21.248551
77.616541	3542.645194	21.253568
77.417037	3561.111256	21.258586
77.302427	3562.338276	21.263603
77.356943	3560.297747	21.268621
77.544723	3577.522352	21.273639
77.667521	3589.965649	21.278656
77.570125	3593.556419	21.283674
77.359779	3597.605241	21.288691
77.944078	3611.424894	21.293709
78.190390	3629.780736	21.298727
78.224596	3631.824180	21.303744
78.288388	3631.070548	21.308762
78.572667	3634.092622	21.313779
78.436845	3625.266559	21.318797
78.640886	3647.102148	21.323815
79.011283	3646.855139	21.328832
78.916451	3649.916221	21.333850
79.020426	3657.000098	21.338867
79.052786	3647.137861	21.343885
78.899740	3657.218478	21.348903
79.281157	3646.508018	21.353920
79.038405	3647.712909	21.358938
79.174965	3646.178900	21.363955
79.319145	3663.304750	21.368973
79.177244	3683.186617	21.373991
79.557652	3674.804433	21.379008
79.518565	3686.735273	21.384026
79.155645	3686.226491	21.389043
79.488791	3683.451397	21.394061
79.482568	3705.199464	21.399079
80.001262	3703.684207	21.404096
80.101258	3701.454717	21.409114
80.146819	3709.787515	21.414131
80.313680	3703.576305	21.419149
80.169456	3715.310179	21.424167
80.398432	3701.605398	21.429184
80.197595	3704.824857	21.434202
80.359695	3715.896617	21.439219
80.775597	3726.935110	21.444237
80.821842	3736.468098	21.449255
80.937247	3735.345682	21.454272
80.954812	3742.147489	21.459290
80.803972	3736.736586	21.464307
81.201285	3730.234613	21.469325
81.252164	3736.262801	21.474343
81.059305	3735.864266	21.479360
81.396702	3736.881489	21.484378
81.565130	3735.488501	21.489395
81.822073	3731.193017	21.494413
81.735296	3734.513429	21.499431
81.785815	3734.696155	21.504448
81.962893	3724.673591	21.509466
81.536334	3727.725404	21.514483
81.788838	3727.278867	21.519501
81.610891	3734.011015	21.524519
81.694261	3719.897217	21.529536
81.770659	3727.694688	21.534554
81.583452	3728.800275	21.539571
81.549919	3737.749158	21.544589
81.744630	3753.748846	21.549607
82.021052	3757.976524	21.554624
81.866075	3763.146095	21.559642
82.080414	3783.927881	21.564659
82.305056	3788.300699	21.569677
82.274517	3802.142445	21.574695
82.708401	3791.697765	21.579712
82.390197	3792.148482	21.584730
82.685124	3797.107039	21.589747
82.963624	3808.416452	21.594765
82.810933	3823.545617	21.599783
83.000201	3825.260852	21.604800
83.162853	3824.152382	21.609818
82.992205	3821.101342	21.614835
83.303692	3818.870231	21.619853
83.241985	3819.206090	21.624871
83.468337	3833.455903	21.629888
83.833552	3844.752051	21.634906
83.550061	3849.659359	21.639923
83.600960	3843.352986	21.644941
83.351175	3850.410964	21.649959
83.851230	3847.426866	21.654976
83.894740	3840.330222	21.659994
83.972849	3844.098886	21.665011
84.156122	3846.748456	21.670029
84.352631	3864.982370	21.675047
84.360105	3861.981907	21.680064
84.988066	3867.538673	21.685082
84.676519	3875.956411	21.690099
84.886600	3863.399902	21.695117
84.656273	3871.498912	21.700135
84.706366	3868.652599	21.705152
84.761841	3866.120404	21.710170
84.768539	3868.131577	21.715187
84.922233	3864.297179	21.720205
85.047744	3863.049368	21.725223
85.165969	3868.686437	21.730240
85.380188	3873.993586	21.735258
84.890536	3867.947636	21.740275
85.098057	3881.005931	21.745293
85.538504	3895.467977	21.750311
85.658120	3894.202272	21.755328
85.545279	3895.937805	21.760346
85.569280	3902.737002	21.765363
86.031011	3894.381716	21.770381
85.201476	3904.508373	21.775399
85.441545	3896.540784	21.780416
85.602141	3913.893283	21.785434
85.712824	3928.240986	21.790451
85.782369	3924.529689	21.795469
85.790382	3930.781892	21.800487
86.010071	3942.346429	21.805504
86.114290	3949.547749	21.810522
86.272693	3960.954259	21.815539
86.295600	3954.868445	21.820557
86.358227	3957.803353	21.825575
86.257455	3971.777006	21.830592
86.815417	3976.801576	21.835610
86.727392	3979.612672	21.840627
87.326418	3982.675365	21.845645
87.292274	3985.356721	21.850663
87.109677	3982.824367	21.855680
87.545148	3977.023811	21.860698
87.376772	3983.150329	21.865715
87.446514	3973.387018	21.870733
87.608979	3973.526926	21.875751
87.458969	3982.832225	21.880768
87.946479	3988.486362	21.885786
87.770084	4006.122781	21.890803
88.112889	4003.600374	21.895821
87.954156	4015.731549	21.900839
88.240647	4015.426461	21.905856
88.622803	3999.473318	21.910874
88.392672	4004.070659	21.915891
88.480118	3996.092169	21.920909
88.365538	3999.819870	21.925927
88.403432	4000.913663	21.930944
88.829783	4011.813522	21.935962
88.653526	4008.782309	21.940979
88.675012	3995.260917	21.945997
88.806955	4005.528391	21.951015
88.894201	3998.812469	21.956032
88.654556	3995.128960	21.961050
88.576379	4016.580262	21.966067
88.741021	4031.963177	21.971085
88.674670	4040.130248	21.976103
88.900409	4046.371161	21.981120
89.269936	4062.499500	21.986138
89.151479	4071.461557	21.991155
89.278175	4075.774061	21.996173
89.202262	4075.574423	22.001191
89.330325	4094.438611	22.006208
89.959359	4099.996853	22.011226
89.763382	4104.786058	22.016243
89.770427	4092.207469	22.021261
90.048096	4098.400906	22.026279
90.022275	4099.499328	22.031296
90.081267	4098.513363	22.036314
90.106696	4131.120132	22.041331
90.321408	4130.416213	22.046349
90.568389	4128.927812	22.051367
90.829696	4127.311725	22.056384
91.133567	4119.860000	22.061402
91.192316	4121.640175	22.066419
91.393480	4119.888691	22.071437
90.989882	4121.679609	22.076455
91.179991	4127.728184	22.081472
91.528537	4123.711458	22.086490
91.434142	4117.948922	22.091507
91.644631	4114.216568	22.096525
91.514215	4119.240273	22.101543
91.360521	4123.253524	22.106560
91.414173	4109.101942	22.111578
91.158881	4120.012412	22.116595
91.215231	4118.874102	22.121613
91.703458	4135.446071	22.126631
91.712209	4147.133560	22.131648
91.834028	4148.931280	22.136666
91.593982	4156.876941	22.141683
92.169123	4151.563539	22.146701
92.327037	4164.200535	22.151719
92.418561	4183.290839	22.156736
92.820600	4183.733077	22.161754
92.195769	4190.039533	22.166771
92.349153	4191.799553	22.171789
92.712447	4191.172550	22.176807
92.593991	4187.822647	22.181824
92.758092	4188.847558	22.186842
92.662874	4202.711771	22.191859
92.850302	4209.309806	22.196877
93.156296	4217.186299	22.201895
92.944719	4221.792336	22.206912
93.208993	4212.168803	22.211930
93.545137	4232.382903	22.216947
93.745839	4245.400137	22.221965
93.662340	4246.943224	22.226983
93.421190	4246.009495	22.232000
93.649975	4249.082947	22.237018
93.851765	4255.817160	22.242035
93.526191	4249.023047	22.247053
94.082086	4256.896885	22.252071
94.228147	4271.831913	22.257088
94.685771	4274.050950	22.262106
94.581077	4282.613017	22.267123
94.916658	4274.434322	22.272141
95.130669	4278.798073	22.277159
95.008007	4272.388964	22.282176
95.133416	4272.425749	22.287194
94.824969	4273.241836	22.292211
94.994138	4273.623973	22.297229
94.985829	4272.641661	22.302247
94.947876	4283.649664	22.307264
95.143685	4271.637950	22.312282
94.885014	4269.439154	22.317299
94.929816	4278.288275	22.322317
94.766694	4285.393810	22.327335
94.986708	4309.750331	22.332352
95.047746	4308.545044	22.337370
94.796740	4318.864985	22.342387
94.849381	4335.337777	22.347405
95.300615	4339.727824	22.352423
95.374170	4359.834306	22.357440
95.453347	4370.623807	22.362458
95.561039	4377.527004	22.367475
95.764966	4394.611899	22.372493
96.172084	4401.917446	22.377511
96.115222	4412.965012	22.382528
96.591395	4404.828307	22.387546
96.701146	4410.370933	22.392563
96.548996	4428.659759	22.397581
97.168775	4417.593653	22.402599
97.066543	4429.933631	22.407616
97.191883	4427.680791	22.412634
97.272375	4424.490487	22.417651
97.455371	4425.184521	22.422669
97.412666	4421.334827	22.427687
97.532975	4421.909650	22.432704
97.694493	4420.143664	22.437722
97.414251	4424.408674	22.442739
97.313654	4418.928275	22.447757
97.830306	4421.229366	22.452775
97.785769	4446.367885	22.457792
98.093321	4444.706032	22.462810
98.012287	4447.942907	22.467827
97.769660	4448.598856	22.472845
98.067717	4448.377630	22.477863
98.071185	4451.128228	22.482880
98.313058	4464.907312	22.487898
98.595415	4481.442478	22.492915
98.751798	4490.174921	22.497933
98.879426	4484.936557	22.502951
98.658032	4485.385658	22.507968
98.645787	4473.103860	22.512986
98.828306	4492.584567	22.518003
98.865993	4504.224826	22.523021
99.349578	4509.482859	22.528039
99.276037	4513.994428	22.533056
99.730748	4511.856026	22.538074
99.534223	4503.872405	22.543091
99.696299	4504.140770	22.548109
99.789389	4508.397720	22.553127
99.966191	4512.248078	22.558144
99.720898	4509.745290	22.563162
100.214202	4525.696146	22.568179
99.777072	4536.704236	22.573197
100.387402	4543.328363	22.578215
100.076335	4551.295848	22.583232
100.594496	4546.209473	22.588250
100.647035	4548.933559	22.593267
100.328289	4546.637905	22.598285
100.758312	4542.591354	22.603303
100.757237	4548.069539	22.608320
100.622828	4544.586821	22.613338
100.885689	4557.581842	22.618355
100.349673	4564.652976	22.623373
100.641788	4556.658019	22.628391
100.557915	4569.629792	22.633408
100.866890	4575.889725	22.638426
101.236001	4591.570513	22.643443
101.251490	4599.923114	22.648461
101.650581	4583.127650	22.653479
101.457813	4598.378632	22.658496
101.465445	4610.964562	22.663514
101.897627	4618.355704	22.668531
101.682583	4625.800312	22.673549
102.040596	4618.180757	22.678567
101.985827	4632.127414	22.683584
102.591141	4632.618308	22.688602
102.491478	4638.985342	22.693619
102.607210	4655.290911	22.698637
103.057192	4641.630920	22.703655
102.884625	4654.723512	22.708672
102.974098	4646.880608	22.713690
103.275248	4646.302838	22.718707
103.192463	4640.520792	22.723725
103.494792	4637.357000	22.728743
103.320721	4636.744131	22.733760
103.528339	4633.546955	22.738778
103.533203	4638.498797	22.743795
103.224142	4642.779833	22.748813
103.686870	4635.863795	22.753831
103.809624	4662.310600	22.758848
103.798669	4665.495335	22.763866
104.207115	4667.302260	22.768883
104.183113	4675.869609	22.773901
104.060162	4662.854446	22.778919
103.804585	4674.808180	22.783936
104.004802	4667.321986	22.788954
104.282775	4680.283799	22.793971
104.142130	4692.639230	22.798989
104.158530	4702.329145	22.804007
104.220777	4710.324863	22.809024
104.419359	4724.977215	22.814042
104.599529	4723.731782	22.819059
104.664817	4733.354261	22.824077
105.012702	4743.486738	22.829095
104.601465	4754.885149	22.834112
104.842684	4765.354923	22.839130
105.351948	4756.827208	22.844147
105.275015	4778.141489	22.849165
105.867505	4787.211270	22.854183
105.793051	4801.732494	22.859200
105.799334	4796.702290	22.864218
106.420448	4790.856225	22.869235
106.236160	4787.816786	22.874253
106.328089	4781.530573	22.879271
106.217727	4786.681800	22.884288
106.164106	4783.064669	22.889306
106.612795	4777.452170	22.894323
106.473769	4786.871840	22.899341
106.583855	4796.232267	22.904359
106.575900	4811.815663	22.909376
106.833167	4821.631338	22.914394
106.967746	4817.058024	22.919411
106.648552	4821.657478	22.924429
106.888400	4824.139986	22.929447
107.255958	4843.792616	22.934464
107.164816	4843.478217	22.939482
107.308429	4853.988413	22.944499
107.340741	4858.111737	22.949517
107.448630	4858.974622	22.954535
107.534657	4880.332779	22.959552
107.718846	4882.753162	22.964570
107.930588	4880.828862	22.969587
107.868150	4887.852029	22.974605
107.916699	4881.759887	22.979623
108.055443	4901.247814	22.984640
108.329853	4902.035682	22.989658
108.598967	4908.132449	22.994675
108.469408	4907.841964	22.999693
108.393182	4918.971967	23.004711
109.072429	4935.672712	23.009728
109.231845	4941.742614	23.014746
109.653133	4939.616189	23.019763
108.958388	4942.266029	23.024781
109.224950	4941.361001	23.029799
109.487443	4939.109782	23.034816
109.092167	4944.529660	23.039834
109.375314	4955.419280	23.044851
109.343735	4967.155246	23.049869
109.556803	4968.021373	23.054887
109.923432	4973.105851	23.059904
110.090986	4997.856800	23.064922
109.933999	5000.120662	23.069939
110.015826	5001.311751	23.074957
110.520914	4988.584054	23.079975
110.349620	5006.609812	23.084992
110.691649	5001.336884	23.090010
110.495292	5001.711604	23.095027
110.790449	5020.144182	23.100045
110.644158	5025.220516	23.105063
110.859688	5020.760866	23.110080
110.933996	5018.637992	23.115098
111.174852	5032.071175	23.120115
110.722826	5051.059583	23.125133
111.373891	5055.967723	23.130151
111.636535	5062.443736	23.135168
111.368509	5062.391230	23.140186
111.769486	5054.760951	23.145203
111.799941	5068.413761	23.150221
111.757651	5084.390052	23.155239
111.741155	5086.858262	23.160256
112.002883	5088.488749	23.165274
112.198143	5084.851725	23.170291
111.964200	5091.660997	23.175309
112.714265	5107.540067	23.180327
113.166961	5114.424610	23.185344
112.461572	5116.555657	23.190362
112.956298	5110.587790	23.195379
112.854417	5118.867054	23.200397
113.134841	5110.876188	23.205415
113.144342	5108.161850	23.210432
112.805415	5114.509444	23.215450
113.050531	5133.319358	23.220467
113.185412	5139.325804	23.225485
112.947454	5134.952531	23.230503
113.392869	5153.349264	23.235520
113.660257	5166.708698	23.240538
113.912473	5156.381703	23.245555
114.284504	5164.326117	23.250573
114.469455	5150.416541	23.255591
114.622536	5147.552343	23.260608
114.769517	5150.571470	23.265626
115.202487	5144.033669	23.270643
115.069845	5148.086890	23.275661
115.110827	5142.752103	23.280679
115.421658	5142.723234	23.285696
115.115463	5152.059931	23.290714
115.693852	5143.384683	23.295731
115.400960	5150.308058	23.300749
115.480716	5138.975649	23.305767
115.655675	5141.964773	23.310784
115.576597	5141.107962	23.315802
115.523980	5150.510671	23.320819
115.362121	5174.054955	23.325837
115.556926	5176.868185	23.330855
115.769144	5178.392958	23.335872
115.896781	5201.133069	23.340890
115.942311	5210.328371	23.345907
115.908136	5214.327707	23.350925
116.094936	5212.005933	23.355943
116.316326	5228.888668	23.360960
116.045511	5243.280911	23.365978
116.306929	5240.435144	23.370995
116.369812	5264.260039	23.376013
116.314871	5271.109590	23.381031
116.902736	5274.298911	23.386048
116.626624	5292.079878	23.391066
117.216054	5294.177222	23.396083
117.090520	5312.076541	23.401101
117.141602	5311.581004	23.406119
117.466739	5330.323084	23.411136
117.350780	5349.378684	23.416154
117.821660	5343.916568	23.421171
117.586321	5343.077871	23.426189
117.937307	5360.063768	23.431207
118.160672	5367.083834	23.436224
118.343353	5377.879907	23.441242
118.566680	5376.486820	23.446259
118.803132	5376.306866	23.451277
118.367380	5371.568085	23.456295
118.654143	5372.528725	23.461312
118.758239	5401.687990	23.466330
119.035760	5394.912078	23.471347
119.113705	5412.222102	23.476365
119.104329	5415.411442	23.481383
119.421137	5404.259543	23.486400
119.227730	5403.345913	23.491418
119.843912	5418.474751	23.496435
119.964246	5420.635203	23.501453
120.289168	5421.968966	23.506471
120.696866	5428.005943	23.511488
120.753572	5424.265778	23.516506
120.949223	5417.973348	23.521523
120.769314	5398.843150	23.526541
120.775159	5394.156260	23.531559
120.965661	5381.597972	23.536576
121.021452	5392.512693	23.541594
121.107525	5405.502486	23.546611
121.246484	5411.733611	23.551629
120.995532	5420.157527	23.556647
121.476087	5416.676314	23.561664
121.158484	5423.459110	23.566682
121.335269	5421.453308	23.571699
121.586596	5419.524521	23.576717
121.513877	5419.897746	23.581735
121.842931	5431.920383	23.586752
121.501204	5446.160342	23.591770
121.589205	5452.390767	23.596787
121.810783	5456.051726	23.601805
121.623856	5461.780275	23.606823
121.692978	5470.880313	23.611840
121.762918	5487.852301	23.616858
121.855778	5498.871016	23.621875
122.035966	5506.897327	23.626893
122.418906	5525.196503	23.631911
122.675707	5530.960857	23.636928
122.585051	5539.328999	23.641946
122.415130	5543.746319	23.646963
122.804345	5567.407022	23.651981
123.102013	5577.272167	23.656999
123.371291	5583.315605	23.662016
123.409443	5597.458277	23.667034
123.759496	5592.697353	23.672051
123.823616	5596.427874	23.677069
123.974853	5603.243009	23.682087
124.506086	5616.986093	23.687104
124.206373	5630.703865	23.692122
124.338754	5629.482310	23.697139
124.417620	5623.980179	23.702157
124.600191	5623.763775	23.707175
124.678699	5624.560061	23.712192
124.822195	5633.833336	23.717210
124.890416	5629.272741	23.722227
124.957216	5646.050090	23.727245
124.919146	5656.586451	23.732263
125.192646	5656.717583	23.737280
125.293338	5658.910580	23.742298
125.227836	5671.686330	23.747315
125.758075	5685.502111	23.752333
125.174654	5695.542797	23.757351
125.766874	5703.850670	23.762368
125.842727	5709.787107	23.767386
126.081006	5726.198798	23.772403
126.235932	5723.910773	23.777421
126.235573	5732.302132	23.782439
126.408505	5732.146456	23.787456
126.640267	5754.915194	23.792474
126.682470	5749.174333	23.797491
127.012392	5758.778848	23.802509
126.859442	5756.179684	23.807527
127.185353	5749.960891	23.812544
127.001972	5780.201225	23.817562
127.044856	5781.421105	23.822579
127.634503	5779.730451	23.827597
127.392365	5798.124498	23.832615
127.601563	5803.927833	23.837632
127.891160	5815.005200	23.842650
127.764728	5811.713033	23.847667
127.910690	5817.413785	23.852685
127.879800	5838.493160	23.857703
128.651327	5833.953721	23.862720
128.678598	5849.398186	23.867738
128.848681	5849.246936	23.872755
129.170930	5842.346588	23.877773
129.050091	5848.323886	23.882791
129.057140	5860.197249	23.887808
129.164662	5864.194511	23.892826
129.468112	5871.871406	23.897843
129.766395	5866.595455	23.902861
129.792112	5872.885561	23.907879
129.946865	5858.714302	23.912896
129.869567	5861.065448	23.917914
130.193800	5861.873184	23.922931
130.441983	5874.319626	23.927949
130.786707	5887.405681	23.932967
130.516197	5892.988810	23.937984
130.755164	5894.298752	23.943002
130.641792	5892.317428	23.948019
130.976034	5894.268768	23.953037
130.710858	5891.929857	23.958055
130.820246	5891.822096	23.963072
131.051573	5897.516119	23.968090
131.147489	5905.192374	23.973107
131.221555	5911.283582	23.978125
131.182199	5930.961633	23.983143
131.326456	5926.141367	23.988160
131.562736	5930.086640	23.993178
131.777930	5946.477310	23.998195
131.616616	5939.121030	24.003213
131.820064	5940.216509	24.008231
131.661908	5947.577935	24.013248
131.848018	5968.549387	24.018266
131.792339	5980.346946	24.023283
132.405061	5988.959448	24.028301
132.765863	6006.466604	24.033319
132.659093	6009.667247	24.038336
132.995449	6013.057380	24.043354
133.638241	6012.246126	24.048371
133.870391	5997.514807	24.053389
133.441616	5992.855774	24.058407
133.593985	6005.962301	24.063424
133.682209	6020.978998	24.068442
134.125727	6022.672157	24.073459
133.969375	6017.224394	24.078477
133.830879	6029.645873	24.083495
134.192600	6031.377475	24.088512
134.291393	6036.935152	24.093530
134.285914	6050.845457	24.098547
134.587527	6051.249048	24.103565
134.303404	6053.788494	24.108583
134.819657	6059.903205	24.113600
134.795136	6082.201973	24.118618
135.019977	6086.221716	24.123635
135.160234	6079.792796	24.128653
135.198493	6088.184024	24.133671
135.241046	6113.408712	24.138688
135.424957	6114.058556	24.143706
135.469072	6124.606344	24.148723
135.968980	6129.433610	24.153741
135.952090	6143.528701	24.158759
136.398479	6142.798375	24.163776
136.631215	6140.933345	24.168794
136.618787	6143.151316	24.173811
136.847544	6131.008883	24.178829
137.035912	6141.853340	24.183847
137.096543	6137.610562	24.188864
137.098649	6149.620475	24.193882
137.522961	6161.402837	24.198899
137.988461	6169.931973	24.203917
138.013892	6177.775623	24.208935
137.583706	6157.653935	24.213952
137.913566	6173.459603	24.218970
137.752365	6164.643562	24.223987
137.911841	6158.673705	24.229005
138.069151	6161.743244	24.234023
137.921737	6169.766975	24.239040
138.185379	6192.379633	24.244058
138.366452	6197.972887	24.249075
138.359041	6192.109611	24.254093
138.501889	6200.783876	24.259111
138.737983	6215.737597	24.264128
138.766258	6225.507539	24.269146
138.727225	6234.302802	24.274163
138.696885	6227.049971	24.279181
138.692845	6256.045800	24.284199
139.030488	6267.097129	24.289216
139.465259	6279.986108	24.294234
139.409810	6294.308504	24.299251
139.682392	6293.309421	24.304269
139.660555	6310.741507	24.309287
139.731021	6328.687926	24.314304
139.943329	6333.800877	24.319322
139.958416	6346.287648	24.324339
140.193809	6358.628743	24.329357
140.485600	6379.844932	24.334375
140.529983	6382.956718	24.339392
140.930049	6393.438148	24.344410
140.878598	6402.822489	24.349427
141.325318	6399.692681	24.354445
140.835113	6416.137017	24.359463
141.338052	6421.672810	24.364480
141.768290	6422.734170	24.369498
141.866400	6428.214904	24.374515
142.277573	6442.177008	24.379533
142.420745	6441.732606	24.384551
142.673991	6439.500096	24.389568
142.987125	6443.254296	24.394586
143.071477	6438.724577	24.399603
143.176986	6435.554003	24.404621
143.157075	6431.202069	24.409639
143.284880	6434.858063	24.414656
143.206610	6429.559045	24.419674
143.126052	6436.200013	24.424691
143.679832	6440.175272	24.429709
143.614907	6459.581865	24.434727
143.695156	6460.949786	24.439744
143.879580	6463.553915	24.444762
143.997765	6460.841984	24.449779
143.991779	6469.286686	24.454797
144.341806	6500.920237	24.459815
143.974294	6499.322704	24.464832
144.150996	6500.837155	24.469850
144.262028	6516.318321	24.474867
144.780969	6527.999658	24.479885
144.625620	6534.128071	24.484903
144.918646	6556.681854	24.489920
145.100852	6553.535132	24.494938
145.533773	6564.135505	24.499955
145.701233	6551.517230	24.504973
145.971977	6549.959157	24.509991
145.899736	6555.988255	24.515008
146.084827	6564.939849	24.520026
146.552971	6577.652411	24.525043
146.634029	6575.559684	24.530061
146.907209	6576.388028	24.535079
146.581458	6584.893910	24.540096
147.352784	6578.548026	24.545114
147.228547	6582.140130	24.550131
147.784295	6574.039894	24.555149
147.641880	6573.676744	24.560167
147.512575	6571.836707	24.565184
147.076431	6565.340193	24.570202
147.285241	6563.776981	24.575219
147.231746	6571.777722	24.580237
147.750140	6591.177429	24.585255
147.686721	6597.908479	24.590272
147.960563	6606.530575	24.595290
148.323758	6619.183964	24.600307
148.538754	6628.394359	24.605325
148.541895	6636.920298	24.610343
148.351347	6636.578789	24.615360
148.679905	6642.400569	24.620378
148.763866	6661.329722	24.625395
148.993233	6664.754881	24.630413
149.134020	6666.974230	24.635431
149.321721	6673.415699	24.640448
149.378494	6689.893374	24.645466
149.599341	6703.350308	24.650483
149.690820	6711.370379	24.655501
150.064877	6719.085208	24.660519
150.010918	6733.384897	24.665536
150.245218	6730.937391	24.670554
150.043467	6736.536594	24.675571
150.338811	6742.963578	24.680589
150.758874	6751.960860	24.685607
150.816368	6755.516334	24.690624
151.192452	6751.528899	24.695642
151.414441	6776.690789	24.700659
151.347234	6781.643837	24.705677
151.133193	6789.554047	24.710695
151.161286	6791.929012	24.715712
151.510944	6799.364475	24.720730
151.581592	6815.126202	24.725747
152.141909	6825.385873	24.730765
152.346231	6843.902310	24.735783
151.974975	6849.391179	24.740800
152.573500	6857.722215	24.745818
152.625692	6866.113827	24.750835
152.700811	6872.543955	24.755853
153.201974	6874.747243	24.760871
152.859105	6879.912218	24.765888
153.170155	6882.853922	24.770906
153.337846	6900.274642	24.775923
153.367673	6911.056210	24.780941
153.970145	6905.099937	24.785959
153.785483	6910.222044	24.790976
153.999940	6920.420542	24.795994
153.877055	6936.985199	24.801011
154.221717	6933.611252	24.806029
154.456854	6933.421271	24.811047
154.259894	6948.701999	24.816064
154.420513	6953.335604	24.821082
154.556406	6970.972182	24.826099
154.859626	6981.305962	24.831117
155.011772	6987.586650	24.836135
155.193586	6991.925951	24.841152
155.512429	6989.143296	24.846170
155.415654	7013.152574	24.851187
155.715559	7024.674100	24.856205
155.853014	7031.630857	24.861223
155.813266	7036.867595	24.866240
156.284229	7051.426558	24.871258
156.428722	7057.953579	24.876275
156.338855	7057.424644	24.881293
156.637485	7068.003474	24.886311
156.949394	7086.602582	24.891328
156.988969	7089.170987	24.896346
157.056869	7092.471882	24.901363
157.394951	7098.278017	24.906381
157.692977	7112.653199	24.911399
157.742729	7114.989838	24.916416
158.471796	7105.118673	24.921434
158.126643	7109.089078	24.926451
158.392647	7103.551996	24.931469
158.516657	7103.062021	24.936487
158.543142	7130.260471	24.941504
158.779179	7133.353728	24.946522
158.945435	7134.889725	24.951539
159.147437	7141.104420	24.956557
159.466431	7125.312605	24.961575
159.563131	7143.178241	24.966592
159.953995	7153.601881	24.971610
159.945896	7163.968668	24.976627
159.938049	7166.757912	24.981645
159.740042	7162.988532	24.986663
160.013857	7171.841754	24.991680
160.036802	7170.508076	24.996698
159.819592	7184.482447	25.001715
160.300668	7198.447412	25.006733
160.729353	7200.655295	25.011751
160.379626	7219.225395	25.016768
161.018203	7229.274970	25.021786
160.800607	7232.160053	25.026803
160.997005	7247.190082	25.031821
161.123512	7264.184986	25.036839
161.070409	7279.902212	25.041856
161.436146	7288.268655	25.046874
161.592061	7295.723383	25.051891
161.463516	7317.978684	25.056909
161.720027	7336.106251	25.061927
161.757390	7347.783306	25.066944
162.184560	7352.772310	25.071962
162.380845	7353.425601	25.076979
162.640488	7374.163355	25.081997
163.247395	7381.845681	25.087015
163.249241	7394.891709	25.092032
163.390137	7382.093784	25.097050
163.503796	7390.097002	25.102067
163.485412	7406.932556	25.107085
164.154208	7401.594166	25.112103
164.067290	7409.544335	25.117120
164.289807	7401.634734	25.122138
164.446530	7409.628216	25.127155
164.388551	7414.501887	25.132173
164.503780	7428.762164	25.137191
164.909269	7441.828842	25.142208
164.784897	7439.369452	25.147226
165.128288	7447.388461	25.152243
165.318496	7457.734834	25.157261
165.584444	7468.127314	25.162279
165.590249	7475.495994	25.167296
165.620484	7470.632578	25.172314
165.907415	7488.889026	25.177331
165.887303	7500.347589	25.182349
166.011385	7504.552763	25.187367
165.934760	7522.808550	25.192384
166.222218	7530.993170	25.197402
166.271253	7548.811496	25.202419
166.211850	7567.355861	25.207437
166.710631	7574.990642	25.212455
167.048836	7594.870710	25.217472
167.131900	7607.340510	25.222490
167.497306	7613.512410	25.227507
167.349316	7634.522841	25.232525
167.728974	7636.049089	25.237543
167.772975	7651.742155	25.242560
168.174026	7668.346948	25.247578
168.529294	7666.856999	25.252595
168.757501	7678.637079	25.257613
169.019449	7688.063769	25.262631
168.947816	7694.116036	25.267648
169.110421	7705.676559	25.272666
169.146014	7704.049186	25.277683
169.042242	7723.619163	25.282701
169.161029	7729.456032	25.287719
169.171874	7740.220141	25.292736
169.365359	7756.161047	25.297754
169.653717	7762.991416	25.302771
169.815876	7787.382083	25.307789
170.257801	7792.911488	25.312807
170.520603	7810.642253	25.317824
170.401156	7829.337440	25.322842
170.750266	7823.592068	25.327859
171.111565	7837.917666	25.332877
171.764769	7845.696270	25.337895
171.454975	7859.373554	25.342912
171.428117	7848.911476	25.347930
171.490994	7862.390952	25.352947
171.415877	7867.005361	25.357965
171.902976	7873.174620	25.362983
171.999948	7894.318289	25.368000
172.224169	7889.598748	25.373018
172.523043	7901.930155	25.378035
172.396473	7923.899195	25.383053
172.777970	7920.099621	25.388071
172.842315	7936.791561	25.393088
173.193252	7948.113570	25.398106
173.546626	7946.950859	25.403123
173.591414	7955.698034	25.408141
174.008559	7968.566982	25.413159
174.417716	7984.905225	25.418176
174.490588	7981.483905	25.423194
174.410029	7974.192410	25.428211
174.528899	7989.183643	25.433229
174.529468	7975.382793	25.438247
174.554674	7996.210384	25.443264
174.939465	8004.536123	25.448282
175.266447	8005.468768	25.453299
175.298829	8016.224643	25.458317
175.823902	8026.598275	25.463335
175.629392	8036.531198	25.468352
175.864711	8039.309634	25.473370
176.076119	8048.254397	25.478387
176.444468	8068.705773	25.483405
176.549157	8070.484820	25.488423
176.668200	8078.980627	25.493440
176.859011	8067.805153	25.498458
176.812778	8087.657986	25.503475
176.917213	8098.937275	25.508493
176.844846	8106.737972	25.513511
176.600019	8125.425848	25.518528
176.882077	8139.102750	25.523546
177.308285	8160.960024	25.528563
177.238214	8186.547616	25.533581
177.429970	8192.651032	25.538599
177.076049	8211.766584	25.543616
177.719111	8236.867251	25.548634
178.114337	8251.301636	25.553651
178.376383	8271.316923	25.558669
178.796554	8279.619408	25.563687
179.031635	8301.794039	25.568704
179.225800	8307.128174	25.573722
179.715841	8308.714350	25.578739
179.839688	8330.563811	25.583757
180.283515	8330.854068	25.588775
180.532844	8336.881492	25.593792
180.637131	8340.713701	25.598810
180.659422	8335.417296	25.603827
180.939749	8345.810244	25.608845
180.835130	8348.424842	25.613863
181.107599	8361.928681	25.618880
180.927704	8357.063991	25.623898
181.539262	8360.359400	25.628915
181.548097	8367.454596	25.633933
181.505915	8358.461740	25.638951
181.246725	8380.032652	25.643968
181.376499	8390.344293	25.648986
181.992922	8408.017463	25.654003
181.821953	8419.530902	25.659021
182.263243	8424.312990	25.664039
182.605305	8444.796138	25.669056
182.797085	8463.983886	25.674074
182.834095	8457.336157	25.679092
182.476517	8478.778318	25.684109
183.020383	8483.579868	25.689127
183.422705	8499.275362	25.694144
183.300058	8522.485378	25.699162
183.846367	8521.511723	25.704180
183.975984	8548.694893	25.709197
184.009201	8551.950037	25.714215
184.482614	8561.321297	25.719232
184.185100	8580.984613	25.724250
184.758818	8592.696682	25.729268
184.809207	8599.360214	25.734285
185.232701	8606.330072	25.739303
185.556585	8622.381842	25.744320
185.280453	8632.353545	25.749338
185.319594	8645.184629	25.754356
185.781299	8659.027351	25.759373
185.910622	8668.909089	25.764391
187.259214	8677.008512	25.769408
186.673320	8679.600880	25.774426
187.211488	8678.983140	25.779444
186.722239	8683.066865	25.784461
187.057507	8703.783132	25.789479
186.753663	8705.525922	25.794496
187.105527	8724.124809	25.799514
187.507610	8736.839389	25.804532
187.690623	8749.810553	25.809549
187.916280	8767.413233	25.814567
188.272849	8774.409606	25.819584
188.325750	8775.029238	25.824602
188.685403	8784.231048	25.829620
188.852773	8801.235541	25.834637
188.753571	8807.788505	25.839655
188.677159	8809.875212	25.844672
188.946216	8836.565409	25.849690
189.423760	8836.181017	25.854708
189.416526	8861.227900	25.859725
189.568388	8877.741940	25.864743
189.821534	8884.724577	25.869760
189.849436	8896.515464	25.874778
190.411718	8897.758422	25.879796
190.418729	8919.453020	25.884813
190.927549	8926.858254	25.889831
191.069063	8933.147831	25.894848
190.944204	8944.350417	25.899866
191.231269	8952.397170	25.904884
191.203774	8968.642666	25.909901
191.387372	8966.660472	25.914919
191.792778	8983.791379	25.919936
191.761414	8990.225640	25.924954
192.013863	9000.667123	25.929972
192.046614	9016.946460	25.934989
192.538584	9026.221845	25.940007
192.614572	9036.641602	25.945024
192.847350	9061.376630	25.950042
192.851200	9067.392048	25.955060
193.201631	9080.025938	25.960077
193.504009	9089.344890	25.965095
193.815508	9092.042695	25.970112
193.844324	9112.205369	25.975130
194.181189	9117.569674	25.980148
194.476769	9124.718471	25.985165
194.580512	9135.466011	25.990183
195.349848	9142.543058	25.995200
195.209510	9155.604643	26.000218
195.507589	9147.615058	26.005236
195.431443	9146.255658	26.010253
195.615738	9157.137523	26.015271
196.056088	9170.116912	26.020288
195.606925	9184.112288	26.025306
195.975596	9185.111131	26.030324
196.028482	9208.945968	26.035341
196.449138	9217.220496	26.040359
196.722678	9224.344751	26.045376
196.600670	9247.694362	26.050394
196.523097	9254.733852	26.055412
196.976482	9275.793026	26.060429
196.780249	9289.259809	26.065447
197.291566	9302.348471	26.070464
197.663390	9309.930214	26.075482
197.876006	9339.957302	26.080500
198.453895	9351.819696	26.085517
197.977786	9348.099047	26.090535
198.493222	9355.750738	26.095552
198.425356	9376.229705	26.100570
198.703842	9385.938981	26.105588
199.348115	9404.215926	26.110605
199.280786	9409.006711	26.115623
199.375563	9436.381710	26.120640
199.290703	9440.226908	26.125658
199.990109	9449.979100	26.130676
199.961279	9472.723731	26.135693
200.573341	9482.716247	26.140711
200.885585	9496.460040	26.145728
200.995004	9509.329400	26.150746
200.918426	9508.140225	26.155764
201.126727	9518.964643	26.160781
201.182933	9538.092606	26.165799
201.713218	9542.612383	26.170816
201.783358	9555.981726	26.175834
201.623443	9565.911231	26.180852
202.140237	9578.559541	26.185869
201.979824	9583.646820	26.190887
202.098055	9603.315745	26.195904
202.284207	9619.553635	26.200922
202.800852	9629.551569	26.205940
202.752576	9642.897161	26.210957
203.131493	9655.263467	26.215975
203.506951	9672.554666	26.220992
203.397363	9691.151831	26.226010
203.896219	9699.001925	26.231028
204.038826	9711.169263	26.236045
203.851017	9723.854953	26.241063
204.633318	9736.944791	26.246080
204.438612	9751.922869	26.251098
204.600628	9763.470789	26.256116
204.852699	9776.594822	26.261133
205.115579	9796.212398	26.266151
205.469599	9804.728716	26.271168
205.740492	9807.409968	26.276186
206.058073	9816.439942	26.281204
206.833250	9824.984928	26.286221
206.876949	9827.560155	26.291239
207.319857	9814.956722	26.296256
207.218694	9822.545724	26.301274
207.540522	9836.820780	26.306292
207.762517	9848.019685	26.311309
207.946425	9847.835310	26.316327
208.155644	9856.321324	26.321344
208.238087	9854.732979	26.326362
208.177622	9851.517701	26.331380
208.661212	9859.487100	26.336397
208.437309	9876.794590	26.341415
208.833598	9880.294257	26.346432
208.892859	9893.837506	26.351450
208.815293	9909.495302	26.356468
209.254084	9918.651105	26.361485
209.092033	9942.363134	26.366503
209.466429	9947.527461	26.371520
209.670526	9969.695515	26.376538
209.922901	9977.252351	26.381556
210.281786	9993.126936	26.386573
210.107567	10018.640731	26.391591
210.378580	10023.868503	26.396608
210.598665	10056.201047	26.401626
210.803775	10059.082715	26.406644
211.107802	10070.751487	26.411661
210.656874	10099.357309	26.416679
211.146926	10120.099289	26.421696
211.113360	10134.664022	26.426714
211.250956	10153.473051	26.431732
211.947681	10175.040072	26.436749
212.079573	10194.816105	26.441767
212.692443	10216.608716	26.446784
212.735817	10230.235336	26.451802
212.974466	10249.000365	26.456820
213.405071	10263.539225	26.461837
213.222832	10274.328665	26.466855
213.826927	10286.551275	26.471872
214.214929	10301.185719	26.476890
214.196764	10304.411416	26.481908
214.727393	10315.671200	26.486925
214.614460	10335.008742	26.491943
214.785515	10333.356309	26.496960
214.839496	10350.266833	26.501978
215.152183	10371.376768	26.506996
215.179566	10377.883452	26.512013
215.057806	10397.161122	26.517031
215.372383	10401.653510	26.522048
215.313529	10416.785407	26.527066
215.633266	10438.730994	26.532084
215.825144	10454.954557	26.537101
216.041647	10484.248755	26.542119
217.016301	10504.438555	26.547136
217.349422	10518.587785	26.552154
217.768880	10524.121204	26.557172
218.100339	10539.031875	26.562189
218.564826	10556.636538	26.567207
218.461986	10550.921193	26.572224
218.777226	10562.255891	26.577242
218.810481	10566.265483	26.582260
219.547153	10556.305846	26.587277
219.927129	10576.725319	26.592295
220.028661	10588.928723	26.597312
220.044674	10582.274267	26.602330
220.214866	10585.136801	26.607348
220.273080	10582.840249	26.612365
220.093144	10585.011114	26.617383
220.386374	10587.152876	26.622400
220.371812	10608.749425	26.627418
220.429690	10611.281375	26.632436
220.977076	10626.771277	26.637453
220.497122	10648.453957	26.642471
220.674322	10672.208176	26.647488
221.064034	10690.196132	26.652506
220.945679	10714.064109	26.657524
221.523211	10733.627309	26.662541
221.560415	10760.924588	26.667559
221.585353	10783.133918	26.672576
222.327615	10802.152075	26.677594
222.556956	10826.085111	26.682612
222.621755	10833.006326	26.687629
223.021562	10856.338140	26.692647
223.050180	10886.409087	26.697664
223.672576	10893.830435	26.702682
223.830635	10919.881220	26.707700
223.868753	10921.321358	26.712717
223.996127	10940.601091	26.717735
224.115748	10955.791146	26.722752
224.544363	10969.391747	26.727770
224.644568	10993.846726	26.732788
224.649289	10998.863589	26.737805
225.013580	11028.670817	26.742823
225.353441	11044.147838	26.747840
225.641555	11059.175155	26.752858
225.854912	11077.581442	26.757876
226.069137	11084.756086	26.762893
226.348919	11106.170463	26.767911
226.797202	11122.769935	26.772928
226.821542	11131.491601	26.777946
226.822769	11159.558457	26.782964
227.486393	11166.276308	26.787981
227.487824	11190.354533	26.792999
227.842612	11202.098943	26.798016
228.258841	11218.004298	26.803034
228.434001	11234.466317	26.808052
228.323315	11235.832707	26.813069
228.764987	11256.697902	26.818087
229.043933	11263.549498	26.823104
229.447551	11283.371682	26.828122
229.556191	11291.213799	26.833140
229.999104	11303.965956	26.838157
230.166660	11325.234386	26.843175
230.259981	11324.455639	26.848192
230.662841	11337.113828	26.853210
230.930886	11350.249005	26.858228
230.948521	11354.894995	26.863245
231.031797	11378.614339	26.868263
231.409425	11385.676007	26.873280
231.536700	11392.317264	26.878298
231.604422	11424.087667	26.883316
231.940616	11431.865631	26.888333
232.465367	11444.120056	26.893351
232.340868	11446.735403	26.898368
232.913764	11460.585900	26.903386
232.923937	11475.418548	26.908404
233.433727	11489.231032	26.913421
233.897583	11504.338953	26.918439
233.710187	11508.353504	26.923456
234.034000	11512.661810	26.928474
233.807384	11542.508229	26.933492
234.216198	11546.638074	26.938509
234.201424	11578.954016	26.943527
234.304077	11597.151352	26.948544
235.112889	11607.880536	26.953562
235.069382	11630.624395	26.958580
235.483197	11647.975742	26.963597
235.780798	11672.330136	26.968615
235.716877	11676.414969	26.973632
236.327280	11687.682525	26.978650
236.326254	11716.604899	26.983668
236.875959	11719.705169	26.988685
237.167389	11739.815055	26.993703
237.384585	11748.589097	26.998720
237.859902	11755.467128	27.003738
237.485705	11765.608057	27.008756
237.672931	11774.362034	27.013773
237.807748	11794.538232	27.018791
238.157408	11814.565734	27.023808
238.515127	11817.104787	27.028826
238.512630	11836.897971	27.033844
238.938330	11842.813739	27.038861
239.343198	11857.739830	27.043879
239.302948	11879.545766	27.048896
239.687587	11882.891848	27.053914
239.667952	11901.778705	27.058932
240.068284	11913.022538	27.063949
240.610766	11938.761626	27.068967
240.894072	11950.075976	27.073984
241.188407	11956.677796	27.079002
241.236873	11976.999829	27.084020
241.601493	11983.969428	27.089037
242.107734	11993.921758	27.094055
241.660520	11997.902163	27.099072
241.888511	12003.607600	27.104090
241.914842	12030.272161	27.109108
242.479691	12040.849603	27.114125
243.066054	12055.784166	27.119143
242.940245	12078.769699	27.124160
243.252097	12087.790892	27.129178
242.691263	12116.904489	27.134196
243.210879	12138.911094	27.139213
244.038254	12148.616201	27.144231
243.821973	12175.582626	27.149248
244.376170	12183.591506	27.154266
244.232360	12207.294241	27.159284
244.708465	12227.406170	27.164301
245.046506	12252.261976	27.169319
244.847463	12274.384067	27.174336
245.470767	12283.114003	27.179354
245.611979	12318.887685	27.184372
245.908782	12334.080172	27.189389
246.165174	12354.513604	27.194407
246.411661	12378.275768	27.199424
247.116438	12378.911461	27.204442
247.337051	12401.885349	27.209460
247.725316	12410.483853	27.214477
248.013553	12422.024635	27.219495
247.948654	12451.900151	27.224512
248.261688	12450.026168	27.229530
248.378125	12469.590117	27.234548
248.694483	12483.159218	27.239565
249.205797	12494.256771	27.244583
249.019992	12524.309171	27.249600
249.052703	12522.114434	27.254618
249.426236	12546.480757	27.259636
249.904949	12556.745482	27.264653
250.506019	12578.232805	27.269671
250.470737	12596.029361	27.274688
250.527145	12589.925088	27.279706
250.807213	12617.049872	27.284724
251.144633	12617.271000	27.289741
251.071489	12631.802189	27.294759
251.333846	12655.847303	27.299776
252.139698	12670.227860	27.304794
252.499238	12683.811792	27.309812
252.672033	12682.781375	27.314829
252.972080	12699.957911	27.319847
252.866683	12724.160724	27.324864
253.639356	12720.992778	27.329882
253.639546	12731.276592	27.334900
253.533516	12748.919954	27.339917
253.846849	12760.207654	27.344935
253.793380	12778.362142	27.349952
253.984786	12789.289352	27.354970
254.205350	12810.593183	27.359988
254.709354	12834.712192	27.365005
255.010879	12849.816090	27.370023
254.806349	12874.155898	27.375040
255.515000	12878.573550	27.380058
255.222882	12910.036559	27.385076
256.068903	12920.538011	27.390093
256.208342	12937.895207	27.395111
256.583510	12963.970351	27.400128
257.101453	12976.900091	27.405146
257.172390	12990.540050	27.410164
257.806206	13005.330231	27.415181
259.069899	12991.278673	27.420199
259.341043	12992.111659	27.425216
259.834471	12976.283492	27.430234
260.023384	12985.400331	27.435252
260.389629	12980.371288	27.440269
260.632397	12974.764495	27.445287
260.182463	12949.034706	27.450304
260.157967	12945.686564	27.455322
260.066773	12968.842356	27.460340
260.172993	12972.543727	27.465357
260.909067	12981.841018	27.470375
260.556393	13007.769901	27.475392
260.647433	13010.153115	27.480410
260.923858	13031.145048	27.485428
261.201874	13042.688021	27.490445
261.280783	13062.812322	27.495463
261.111929	13080.443166	27.500480
261.365713	13106.304504	27.505498
261.613975	13131.572637	27.510516
262.370201	13156.585098	27.515533
262.325556	13175.126234	27.520551
262.694751	13211.231595	27.525568
262.676578	13226.300800	27.530586
263.269640	13248.953553	27.535604
263.707503	13286.294019	27.540621
263.808512	13296.612918	27.545639
263.865773	13319.141677	27.550656
264.424001	13327.063747	27.555674
264.482676	13357.368923	27.560692
264.655728	13374.366190	27.565709
265.266342	13387.075475	27.570727
265.391038	13417.504993	27.575744
266.226884	13422.540906	27.580762
266.381673	13446.254138	27.585780
266.271448	13456.962399	27.590797
266.788581	13465.405400	27.595815
266.899612	13496.221985	27.600832
266.701585	13509.728796	27.605850
267.050586	13528.289545	27.610868
267.456800	13545.440890	27.615885
267.889981	13565.413665	27.620903
267.689772	13585.584870	27.625920
268.209028	13599.777376	27.630938
268.677031	13623.150317	27.635956
268.836677	13639.667853	27.640973
269.148987	13657.029278	27.645991
269.239539	13682.717753	27.651008
269.613291	13708.264733	27.656026
270.362904	13721.271991	27.661044
270.330568	13732.681082	27.666061
270.674979	13752.767023	27.671079
271.077247	13767.271316	27.676096
271.306252	13790.542030	27.681114
271.823209	13798.474555	27.686132
272.147935	13814.952939	27.691149
272.730146	13817.299368	27.696167
272.597602	13836.058064	27.701184
272.760628	13852.901503	27.706202
273.027833	13866.134994	27.711220
273.290789	13884.368864	27.716237
273.536892	13892.617387	27.721255
273.551127	13920.341552	27.726272
274.023321	13930.828926	27.731290
274.445614	13952.284075	27.736308
274.470847	13962.386256	27.741325
274.789794	13983.148299	27.746343
275.376909	13998.078209	27.751360
275.456405	14014.764326	27.756378
275.593693	14031.727421	27.761396
276.056397	14056.761619	27.766413
276.509261	14057.347578	27.771431
276.388028	14088.884420	27.776448
277.133373	14089.365082	27.781466
276.922275	14104.739262	27.786484
277.372358	14123.940634	27.791501
277.553886	14138.837737	27.796519
277.809140	14155.471805	27.801536
277.964313	14178.141001	27.806554
278.334684	14193.158677	27.811572
278.290824	14214.826469	27.816589
278.832080	14227.576668	27.821607
279.097932	14244.796936	27.826624
279.425117	14265.250561	27.831642
279.534059	14278.766857	27.836660
279.677162	14288.685109	27.841677
280.365368	14306.799272	27.846695
280.414001	14319.049200	27.851712
280.439837	14341.840091	27.856730
281.165425	14356.442383	27.861748
280.998851	14379.871575	27.866765
281.513318	14394.662981	27.871783
281.883116	14413.602612	27.876800
282.348303	14423.700598	27.881818
282.795951	14434.294957	27.886836
282.736509	14453.648672	27.891853
282.960120	14471.516368	27.896871
283.529443	14489.126223	27.901888
283.752168	14513.458264	27.906906
284.083908	14518.065498	27.911924
284.345117	14547.132322	27.916941
284.847762	14545.290237	27.921959
284.996061	14569.423901	27.926976
285.064897	14589.949006	27.931994
285.555802	14596.136752	27.937012
285.401534	14621.075798	27.942029
285.835019	14633.780159	27.947047
286.381909	14654.191880	27.952064
286.225956	14663.922026	27.957082
286.404952	14692.911775	27.962100
286.400411	14716.606855	27.967117
286.806088	14730.804045	27.972135
286.974472	14764.511908	27.977152
287.289655	14791.495549	27.982170
287.843870	14816.338675	27.987188
287.855877	14849.044211	27.992205
288.376919	14866.386897	27.997223
288.491890	14899.740072	28.002240
288.921977	14923.524885	28.007258
289.259425	14950.062034	28.012276
289.109989	14980.156806	28.017293
289.798405	15008.413517	28.022311
289.761445	15029.384473	28.027328
290.070942	15056.989003	28.032346
291.221001	15082.983554	28.037364
291.391348	15110.845315	28.042381
291.870184	15127.347463	28.047399
291.734021	15144.368027	28.052416
291.711179	15161.228895	28.057434
292.737956	15183.130591	28.062452
292.755433	15202.429436	28.067469
293.722292	15213.513810	28.072487
293.861633	15222.269954	28.077504
293.395704	15238.235839	28.082522
294.022251	15255.768924	28.087540
293.875947	15275.512071	28.092557
294.299244	15296.005670	28.097575
294.739959	15322.593499	28.102592
294.908566	15332.935188	28.107610
295.454665	15348.831757	28.112628
295.511833	15369.601004	28.117645
295.800883	15386.597801	28.122663
296.377621	15404.402828	28.127680
296.272708	15428.317897	28.132698
296.624064	15437.006289	28.137716
296.897913	15463.116942	28.142733
297.178408	15488.759904	28.147751
297.676930	15509.064324	28.152768
298.092481	15532.348079	28.157786
298.854233	15532.119786	28.162804
298.556792	15560.339914	28.167821
298.761991	15561.010945	28.172839
299.182251	15579.564943	28.177856
299.314919	15600.999365	28.182874
299.667059	15622.110880	28.187892
299.706028	15640.372468	28.192909
300.068167	15658.818291	28.197927
300.872995	15671.109856	28.202944
301.457650	15683.506951	28.207962
302.074254	15705.109203	28.212980
302.170588	15717.109231	28.217997
302.728416	15723.271748	28.223015
302.985995	15730.362181	28.228032
302.725505	15745.472058	28.233050
303.344277	15747.634382	28.238068
303.374750	15774.449309	28.243085
303.907388	15778.458129	28.248103
304.058058	15789.266627	28.253120
304.371074	15806.942313	28.258138
304.549745	15810.691808	28.263156
304.780909	15849.487497	28.268173
305.080643	15846.001224	28.273191
305.476966	15868.201055	28.278208
305.626181	15892.257669	28.283226
305.752682	15908.162064	28.288244
305.629537	15932.648476	28.293261
305.656740	15957.378716	28.298279
306.188756	15994.026597	28.303296
306.166069	16030.334551	28.308314
306.597528	16057.234116	28.313332
306.664837	16090.969879	28.318349
307.411771	16122.054388	28.323367
307.598037	16155.429393	28.328384
307.775141	16193.404388	28.333402
308.497744	16217.993758	28.338420
308.979557	16249.105028	28.343437
309.599897	16280.452721	28.348455
309.701211	16290.355689	28.353472
309.598338	16316.128691	28.358490
310.326046	16335.874629	28.363508
310.566219	16356.873851	28.368525
311.053113	16383.337234	28.373543
311.363939	16397.629358	28.378560
310.988781	16423.062971	28.383578
311.547651	16437.615288	28.388596
311.975382	16473.545911	28.393613
312.533343	16492.200291	28.398631
312.311477	16504.780375	28.403648
312.772618	16532.823262	28.408666
313.411669	16561.609732	28.413684
313.643769	16578.522925	28.418701
313.854723	16603.950943	28.423719
314.617102	16617.924669	28.428736
314.504763	16642.033501	28.433754
314.892244	16650.779398	28.438772
314.990120	16676.617865	28.443789
315.256903	16696.838920	28.448807
315.495868	16723.840342	28.453824
315.809977	16755.897220	28.458842
316.563595	16771.157385	28.463860
317.522071	16788.271046	28.468877
317.148784	16800.766952	28.473895
318.465026	16815.639085	28.478912
318.645488	16820.378517	28.483930
319.435107	16815.679340	28.488948
319.869397	16810.334812	28.493965
320.011851	16819.370298	28.498983
320.839098	16821.046172	28.504000
320.720603	16826.629803	28.509018
321.151137	16825.539199	28.514036
321.306850	16822.649665	28.519053
321.369443	16824.973673	28.524071
321.629686	16821.988976	28.529088
321.430361	16835.769860	28.534106
321.731766	16847.880590	28.539124
321.794130	16862.874660	28.544141
322.459389	16879.373404	28.549159
322.729691	16901.641932	28.554176
322.603398	16924.479779	28.559194
323.189553	16941.443013	28.564212
323.388513	16962.976604	28.569229
323.367687	16995.345160	28.574247
323.739354	17007.756107	28.579264
323.718849	17039.637563	28.584282
324.263766	17069.634442	28.589300
324.653186	17105.565113	28.594317
324.938272	17118.244795	28.599335
325.423950	17141.493563	28.604352
325.724164	17173.665557	28.609370
326.019146	17189.119798	28.614388
326.208144	17213.108441	28.619405
326.556155	17246.647087	28.624423
326.481763	17264.146363	28.629440
326.648268	17293.727668	28.634458
327.041699	17327.752138	28.639476
327.799245	17362.584503	28.644493
327.872109	17386.640594	28.649511
328.468590	17406.392958	28.654528
328.804185	17423.859969	28.659546
329.248900	17451.893030	28.664564
329.771673	17470.333827	28.669581
329.911585	17490.117245	28.674599
330.426177	17509.592110	28.679616
330.943137	17533.485590	28.684634
331.027671	17552.827687	28.689652
331.285098	17576.701073	28.694669
331.340404	17588.469847	28.699687
332.151006	17615.770449	28.704704
331.800343	17640.835953	28.709722
332.589803	17656.798657	28.714740
332.757422	17683.902146	28.719757
332.791419	17718.034732	28.724775
332.776076	17737.774107	28.729792
333.442327	17772.362845	28.734810
334.131931	17790.300862	28.739828
334.878873	17828.445195	28.744845
334.774893	17849.314515	28.749863
335.228508	17867.568959	28.754880
335.654684	17903.070949	28.759898
336.167207	17909.221558	28.764916
336.725597	17918.068110	28.769933
336.825097	17943.709609	28.774951
337.247253	17955.537163	28.779968
337.472823	17976.955562	28.784986
337.746941	18005.807074	28.790004
338.253774	18012.746981	28.795021
338.470745	18028.467620	28.800039
339.372862	18046.971743	28.805056
339.526860	18074.716710	28.810074
340.190244	18082.640401	28.815092
340.666727	18090.277660	28.820109
340.553104	18106.865393	28.825127
340.782349	18131.846429	28.830144
340.997394	18138.486397	28.835162
341.075970	18150.858562	28.840180
341.553818	18172.117307	28.845197
341.868916	18186.427576	28.850215
342.472791	18209.778971	28.855232
342.317752	18243.178801	28.860250
342.855124	18258.130547	28.865268
343.741873	18283.788995	28.870285
343.623950	18299.206245	28.875303
344.122105	18315.640459	28.880320
344.317293	18333.324829	28.885338
344.641988	18357.752222	28.890356
344.782058	18381.318934	28.895373
344.923355	18413.589917	28.900391
345.374851	18432.855947	28.905408
345.729588	18453.705734	28.910426
346.026497	18481.981848	28.915444
346.547127	18495.267042	28.920461
346.715453	18533.168446	28.925479
347.263274	18547.677208	28.930496
347.265766	18569.044728	28.935514
347.685739	18596.226263	28.940532
348.016214	18619.749640	28.945549
348.283061	18648.441110	28.950567
348.893784	18666.415663	28.955584
349.050753	18687.112015	28.960602
349.628346	18714.150057	28.965620
349.702785	18741.599163	28.970637
350.318366	18770.950021	28.975655
350.459110	18791.261428	28.980672
350.487824	18812.117083	28.985690
350.954317	18846.461633	28.990708
351.230431	18869.283608	28.995725
351.516131	18912.316665	29.000743
351.711100	18937.071427	29.005760
352.045196	18965.526450	29.010778
352.283874	19007.935570	29.015796
352.933621	19032.435943	29.020813
352.970894	19065.777639	29.025831
353.552137	19093.708061	29.030848
353.908750	19127.271066	29.035866
354.480661	19154.460574	29.040884
354.789158	19185.532909	29.045901
354.989110	19223.072537	29.050919
355.410895	19255.543024	29.055936
355.863615	19287.085908	29.060954
355.879574	19327.110629	29.065972
356.158117	19357.310196	29.070989
356.255265	19398.863181	29.076007
357.142208	19438.425130	29.081024
357.510334	19463.040618	29.086042
357.673632	19497.693884	29.091060
358.501954	19528.918999	29.096077
358.640037	19571.523366	29.101095
359.366564	19589.704532	29.106112
359.318825	19623.150193	29.111130
359.561137	19650.144714	29.116148
360.687931	19684.909163	29.121165
360.475510	19719.904780	29.126183
361.094547	19733.196165	29.131200
361.690255	19763.588072	29.136218
361.850566	19795.889975	29.141236
362.668452	19813.343040	29.146253
362.848273	19838.658309	29.151271
363.499037	19862.642547	29.156288
364.043332	19876.974892	29.161306
364.254100	19910.793079	29.166324
364.999794	19920.783272	29.171341
364.848771	19944.707945	29.176359
364.859770	19959.432917	29.181376
365.205255	19992.126029	29.186394
365.499837	20011.657274	29.191412
366.119029	20034.026261	29.196429
365.930031	20069.382816	29.201447
366.297788	20092.668499	29.206464
366.684287	20124.377243	29.211482
366.745035	20155.936894	29.216500
367.444549	20181.963033	29.221517
367.849536	20214.160729	29.226535
367.939564	20235.936353	29.231552
368.036161	20271.772604	29.236570
368.562929	20303.400879	29.241588
369.013909	20332.993957	29.246605
369.074085	20372.464848	29.251623
369.702906	20394.034807	29.256640
370.760441	20426.900010	29.261658
371.162387	20443.226650	29.266676
371.330261	20472.729733	29.271693
371.977377	20485.963291	29.276711
372.951993	20498.319218	29.281728
373.112005	20521.007220	29.286746
373.491821	20532.608905	29.291764
374.089635	20544.349840	29.296781
374.199924	20569.373794	29.301799
375.173612	20572.108253	29.306816
375.696287	20585.317489	29.311834
375.798520	20600.615532	29.316852
376.242792	20598.776520	29.321869
376.148036	20625.328937	29.326887
376.381914	20630.881816	29.331904
376.548037	20660.164772	29.336922
376.416829	20683.350716	29.341940
376.959826	20704.838018	29.346957
377.280164	20730.045389	29.351975
377.940668	20760.331799	29.356992
378.505318	20784.720006	29.362010
378.393271	20818.097049	29.367028
378.666580	20844.761759	29.372045
378.573982	20881.970454	29.377063
378.785082	20914.355663	29.382080
379.122750	20957.176872	29.387098
379.314315	20993.706374	29.392116
380.146828	21033.956281	29.397133
380.087379	21080.496269	29.402151
380.523143	21121.665881	29.407168
381.282947	21164.662834	29.412186
381.483222	21208.331344	29.417204
381.994261	21237.119389	29.422221
382.391942	21281.403926	29.427239
382.503758	21313.089431	29.432256
383.252641	21346.389345	29.437274
383.435494	21397.247171	29.442292
384.488452	21419.570461	29.447309
384.354432	21459.498184	29.452327
385.030892	21501.516832	29.457344
385.557634	21532.146076	29.462362
385.952507	21561.965371	29.467380
386.519905	21580.473991	29.472397
386.949244	21609.629895	29.477415
387.174394	21638.677343	29.482432
387.779107	21662.134301	29.487450
388.131232	21687.246183	29.492468
388.785786	21703.559132	29.497485
389.067765	21727.360064	29.502503
389.333303	21752.537343	29.507520
389.769807	21760.761859	29.512538
389.860423	21790.154313	29.517556
390.428067	21810.550717	29.522573
390.687270	21831.239697	29.527591
390.949198	21870.857680	29.532608
391.405642	21887.783490	29.537626
391.455196	21916.948237	29.542644
392.132586	21944.633504	29.547661
392.486956	21976.925218	29.552679
392.699610	22016.911525	29.557696
392.794345	22047.431230	29.562714
393.215965	22091.510343	29.567732
393.718883	22117.289297	29.572749
394.226316	22158.483825	29.577767
394.312013	22190.689523	29.582784
395.001614	22229.673647	29.587802
395.090749	22266.918870	29.592820
395.445070	22302.977003	29.597837
395.821868	22344.689535	29.602855
396.257047	22392.895616	29.607872
397.110214	22419.277333	29.612890
397.309499	22466.880642	29.617908
397.824118	22491.601577	29.622925
398.364664	22517.712163	29.627943
399.231212	22556.821255	29.632960
399.839156	22578.813897	29.637978
400.111719	22604.103194	29.642996
400.761418	22619.837521	29.648013
400.941819	22652.668119	29.653031
401.220003	22677.448767	29.658048
402.017017	22690.155300	29.663066
402.017276	22732.529415	29.668084
402.298988	22748.604478	29.673101
402.650463	22780.352561	29.678119
402.918209	22817.590450	29.683136
403.463901	22842.174099	29.688154
403.674529	22875.807377	29.693172
404.391946	22902.329806	29.698189
404.544777	22932.424798	29.703207
404.455011	22971.250850	29.708224
404.378432	22996.663641	29.713242
404.894456	23042.507919	29.718260
405.527588	23070.082742	29.723277
406.483247	23111.461386	29.728295
406.786701	23149.690568	29.733312
407.242202	23179.642655	29.738330
407.725969	23210.324857	29.743348
408.383509	23244.970436	29.748365
408.602995	23258.946543	29.753383
408.949883	23289.980372	29.758400
410.000823	23309.522987	29.763418
410.221728	23329.040702	29.768436
411.185133	23339.347304	29.773453
411.285135	23354.539379	29.778471
411.626022	23377.379966	29.783488
412.065189	23382.139996	29.788506
412.243911	23425.541873	29.793524
412.399463	23427.666344	29.798541
412.846933	23459.080664	29.803559
412.963017	23504.672993	29.808576
413.608441	23519.276541	29.813594
413.777852	23556.450877	29.818612
414.001902	23588.184443	29.823629
414.507332	23618.422078	29.828647
414.576141	23643.407174	29.833664
415.590542	23667.763440	29.838682
415.460853	23705.421479	29.843700
415.952862	23742.067803	29.848717
416.710596	23775.482917	29.853735
416.776206	23821.491627	29.858752
417.217133	23848.747371	29.863770
417.618587	23886.649131	29.868788
418.164824	23921.211062	29.873805
418.340236	23951.543689	29.878823
418.556936	23999.548850	29.883840
419.546257	24040.804108	29.888858
419.492820	24075.983260	29.893876
420.057455	24116.948740	29.898893
420.512601	24155.822868	29.903911
421.047672	24197.550633	29.908928
421.583827	24221.302009	29.913946
421.790226	24270.028866	29.918964
421.939686	24301.896391	29.923981
422.412076	24341.234820	29.928999
422.697682	24392.301564	29.934016
423.276708	24427.653781	29.939034
423.525427	24475.680013	29.944052
423.841659	24517.499677	29.949069
424.516366	24563.387057	29.954087
424.747180	24613.722572	29.959104
425.897553	24647.712431	29.964122
426.611440	24684.694952	29.969140
426.808063	24710.770030	29.974157
427.291924	24754.690748	29.979175
427.495735	24777.083525	29.984192
428.676528	24800.564356	29.989210
428.866205	24824.196139	29.994228
429.648555	24847.310008	29.999245
430.456416	24863.006681	30.004263
430.864216	24877.891845	30.009280
431.736690	24895.952745	30.014298
432.025948	24914.927448	30.019316
432.310738	24930.101863	30.024333
432.782449	24947.934981	30.029351
432.750367	24965.327661	30.034368
433.465662	24976.841762	30.039386
433.212462	25004.792392	30.044404
433.501391	25019.464621	30.049421
434.373219	25039.326966	30.054439
434.170356	25070.123841	30.059456
434.620118	25099.279025	30.064474
434.748728	25126.561922	30.069492
434.928546	25152.810886	30.074509
435.714254	25182.252477	30.079527
435.785573	25232.919954	30.084544
436.219821	25265.409201	30.089562
436.594836	25312.693739	30.094580
436.727705	25343.777406	30.099597
437.510257	25383.137610	30.104615
437.369942	25430.949255	30.109632
437.912498	25476.956344	30.114650
438.674691	25524.269745	30.119668
439.097984	25574.811659	30.124685
439.482149	25615.130240	30.129703
439.356667	25666.892635	30.134720
439.893377	25713.759392	30.139738
440.224364	25765.305055	30.144756
439.958699	25830.066709	30.149773
440.757575	25881.075122	30.154791
440.791478	25945.997228	30.159808
441.451126	25991.906751	30.164826
441.787913	26060.137040	30.169844
442.532805	26118.799056	30.174861
443.378446	26178.891988	30.179879
444.432252	26228.059586	30.184896
445.490430	26256.519380	30.189914
446.062019	26298.782246	30.194932
446.447778	26334.950682	30.199949
447.316809	26360.436658	30.204967
447.600164	26401.531460	30.209984
448.260135	26436.422790	30.215002
449.085994	26458.783700	30.220020
448.956684	26482.380918	30.225037
449.553877	26515.819385	30.230055
449.891646	26545.750166	30.235072
450.621475	26564.345170	30.240090
451.062071	26585.996204	30.245108
451.460088	26617.065102	30.250125
451.747783	26640.865536	30.255143
452.202025	26678.363710	30.260160
452.765366	26703.366269	30.265178
453.095306	26733.797165	30.270196
453.223042	26775.723977	30.275213
453.680688	26803.426333	30.280231
453.695279	26843.959366	30.285248
454.192440	26882.109970	30.290266
454.549696	26922.253215	30.295284
454.563783	26972.519130	30.300301
455.248685	27007.161259	30.305319
455.442329	27054.784472	30.310336
455.985486	27089.242837	30.315354
456.803999	27136.087218	30.320372
457.100366	27181.841295	30.325389
457.937021	27200.724694	30.330407
458.011559	27249.580302	30.335424
458.375817	27266.153354	30.340442
459.233613	27305.713242	30.345460
459.797864	27344.112057	30.350477
460.387829	27380.231895	30.355495
461.182851	27414.808642	30.360512
461.367414	27458.102875	30.365530
461.724505	27487.789037	30.370548
462.215949	27522.944884	30.375565
462.668330	27548.573409	30.380583
462.980484	27588.684900	30.385600
463.055343	27620.079126	30.390618
463.263768	27661.180268	30.395636
463.569732	27716.278952	30.400653
464.023990	27756.688278	30.405671
464.311367	27801.508502	30.410688
465.001880	27849.496734	30.415706
465.938827	27903.418354	30.420724
465.974732	27951.547433	30.425741
466.721115	27993.065118	30.430759
467.160031	28049.366195	30.435776
467.298684	28106.166914	30.440794
467.774585	28151.605655	30.445812
468.689761	28203.137283	30.450829
469.251403	28246.980919	30.455847
469.629294	28298.201053	30.460864
469.728018	28341.016834	30.465882
470.204005	28390.340027	30.470900
470.338996	28439.399975	30.475917
471.191745	28489.747377	30.480935
471.455367	28542.227742	30.485952
472.269550	28590.786808	30.490970
472.587428	28639.235439	30.495988
473.019549	28695.445097	30.501005
473.577561	28734.239260	30.506023
474.151940	28788.926165	30.511040
474.676558	28840.198456	30.516058
475.198465	28887.890286	30.521076
475.802593	28933.716089	30.526093
476.694114	28972.459938	30.531111
477.402962	29020.303092	30.536128
477.507621	29053.975949	30.541146
478.346831	29081.802681	30.546164
478.727077	29129.169216	30.551181
479.175986	29157.085034	30.556199
479.866582	29183.899339	30.561216
480.217008	29226.790884	30.566234
480.742679	29260.638097	30.571252
481.021600	29299.093240	30.576269
481.724605	29338.356102	30.581287
482.138747	29376.349668	30.586304
482.681303	29410.254224	30.591322
482.774203	29435.637893	30.596340
483.114082	29478.339387	30.601357
483.422765	29514.802100	30.606375
483.725588	29551.493071	30.611392
484.172964	29596.331466	30.616410
484.859213	29634.250563	30.621428
484.723572	29689.030373	30.626445
485.394896	29729.220875	30.631463
485.988556	29787.280570	30.636480
486.012872	29833.757086	30.641498
486.740829	29879.624079	30.646516
487.137864	29940.513574	30.651533
487.815377	29990.406221	30.656551
488.180535	30039.841368	30.661568
488.865638	30082.885894	30.666586
489.539171	30134.335215	30.671604
489.962554	30185.912745	30.676621
490.761954	30225.773204	30.681639
491.004159	30272.465964	30.686656
491.475167	30328.790906	30.691674
492.411399	30365.447601	30.696692
492.683743	30424.634124	30.701709
493.168429	30462.807260	30.706727
493.374398	30512.179495	30.711744
493.871585	30565.379991	30.716762
494.436478	30614.205070	30.721780
494.602009	30670.539265	30.726797
495.508470	30719.167264	30.731815
495.836099	30768.456255	30.736832
496.342895	30824.732462	30.741850
497.261082	30869.386119	30.746868
497.555682	30913.291603	30.751885
498.272297	30957.998957	30.756903
498.542890	31006.238132	30.761920
499.018722	31055.369992	30.766938
499.409303	31108.782868	30.771956
499.508586	31170.172530	30.776973
500.147515	31217.083791	30.781991
500.600001	31279.726015	30.787008
500.766038	31343.635593	30.792026
501.755133	31397.050912	30.797044
501.882743	31459.585346	30.802061
502.443237	31516.722327	30.807079
503.215015	31565.363099	30.812096
503.525866	31626.961062	30.817114
504.364035	31683.808016	30.822132
504.567821	31748.368946	30.827149
504.809222	31798.398203	30.832167
505.876136	31857.955087	30.837184
506.157003	31921.572515	30.842202
507.165468	31972.127202	30.847220
507.805079	32026.061865	30.852237
508.590823	32051.018135	30.857255
509.192357	32088.950684	30.862272
509.854487	32121.596589	30.867290
510.604361	32151.406312	30.872308
510.923043	32182.896230	30.877325
511.346686	32207.892677	30.882343
512.174069	32233.075591	30.887360
512.595306	32269.893891	30.892378
513.339064	32288.158070	30.897396
514.136395	32314.504405	30.902413
514.668373	32338.803988	30.907431
515.166536	32367.874580	30.912448
515.421074	32392.736162	30.917466
516.122910	32416.053708	30.922484
516.448639	32442.010832	30.927501
517.066758	32462.388990	30.932519
517.621983	32497.468064	30.937536
518.043400	32527.946919	30.942554
518.622772	32549.196498	30.947572
519.087204	32575.073245	30.952589
519.266225	32601.879400	30.957607
519.602810	32636.715345	30.962624
520.127340	32672.487986	30.967642
520.663716	32710.663396	30.972660
521.184271	32752.303530	30.977677
521.186044	32790.169923	30.982695
522.210703	32816.487516	30.987712
522.565324	32858.778028	30.992730
523.469346	32873.521838	30.997748
524.550610	32914.725444	31.002765
524.861675	32947.704418	31.007783
525.386201	32966.682212	31.012800
525.840938	33015.450691	31.017818
526.118778	33039.965191	31.022836
526.413434	33073.774046	31.027853
526.729927	33111.192706	31.032871
526.981212	33149.825011	31.037888
527.352318	33212.181831	31.042906
528.215850	33252.258996	31.047924
528.334926	33302.445963	31.052941
528.977562	33353.688961	31.057959
529.996143	33382.397466	31.062976
530.634300	33425.372906	31.067994
531.279126	33455.524714	31.073012
531.853087	33493.376601	31.078029
532.143083	33530.898510	31.083047
532.624302	33574.185233	31.088064
532.748191	33628.140503	31.093082
533.406159	33671.564442	31.098100
533.597694	33721.901118	31.103117
533.899882	33774.926821	31.108135
534.368131	33821.047289	31.113152
534.585435	33891.474318	31.118170
535.351149	33944.247515	31.123188
535.622998	33999.980636	31.128205
535.995857	34065.322565	31.133223
536.570045	34118.081746	31.138240
536.628234	34175.758278	31.143258
537.610021	34239.456340	31.148276
538.059123	34300.822023	31.153293
538.343120	34358.829710	31.158311
539.102411	34415.913463	31.163328
539.706466	34483.852643	31.168346
540.398351	34532.019649	31.173364
541.285940	34581.106406	31.178381
541.455050	34644.923053	31.183399
542.117806	34693.007108	31.188416
542.544196	34747.137975	31.193434
543.615460	34806.571352	31.198452
543.652797	34865.080571	31.203469
544.114122	34917.728866	31.208487
545.194831	34976.009170	31.213504
545.487488	35040.948590	31.218522
546.219630	35092.263254	31.223540
546.820142	35146.381261	31.228557
547.439679	35206.133225	31.233575
548.327564	35258.835675	31.238592
548.534378	35303.843220	31.243610
549.068862	35354.807431	31.248628
549.498908	35413.364755	31.253645
550.110696	35476.701319	31.258663
550.813042	35525.273184	31.263680
550.981666	35586.640780	31.268698
551.831043	35639.382497	31.273716
552.360830	35700.846413	31.278733
552.570118	35754.774448	31.283751
553.218381	35813.027382	31.288768
553.674657	35883.948319	31.293786
554.187241	35940.233242	31.298804
555.034107	35997.767807	31.303821
555.214459	36057.881898	31.308839
555.979529	36122.999908	31.313856
556.500734	36185.789466	31.318874
556.901057	36238.928662	31.323892
557.498743	36309.571356	31.328909
557.804818	36376.656467	31.333927
558.697479	36436.794956	31.338944
559.038686	36505.146573	31.343962
559.770030	36571.067394	31.348980
559.937310	36638.657033	31.353997
560.454962	36703.001975	31.359015
561.607867	36765.697921	31.364032
561.995280	36836.495474	31.369050
562.699521	36905.357717	31.374068
563.068871	36962.175382	31.379085
563.639790	37035.906266	31.384103
564.193318	37094.959199	31.389120
564.874754	37163.769505	31.394138
565.542534	37233.238981	31.399156
566.372358	37285.111281	31.404173
567.200664	37330.636037	31.409191
568.030228	37380.349528	31.414208
569.145816	37421.851102	31.419226
569.072836	37462.637835	31.424244
569.840031	37499.956761	31.429261
570.073347	37555.745257	31.434279
571.056952	37596.565909	31.439296
571.391551	37655.017358	31.444314
571.841027	37694.970118	31.449332
572.426290	37744.211917	31.454349
572.558125	37798.288675	31.459367
573.072377	37845.330070	31.464384
573.350882	37901.983125	31.469402
573.212453	37967.720233	31.474420
574.283264	38026.949549	31.479437
575.051005	38092.651800	31.484455
575.290477	38160.364105	31.489472
575.736868	38224.565605	31.494490
576.419067	38303.756354	31.499508
577.229262	38367.583500	31.504525
577.279813	38437.911450	31.509543
578.107573	38503.181873	31.514560
578.204573	38572.138632	31.519578
579.091565	38642.245129	31.524596
579.778955	38713.914007	31.529613
580.744347	38778.814572	31.534631
582.376252	38824.401078	31.539648
583.805920	38862.089116	31.544666
584.877670	38894.834897	31.549684
585.745990	38928.044928	31.554701
586.286992	38958.185776	31.559719
586.973308	38983.279152	31.564736
587.338806	39021.976954	31.569754
587.673838	39047.607296	31.574772
588.203653	39087.252568	31.579789
588.520207	39127.256468	31.584807
588.679669	39162.662471	31.589824
588.675978	39205.698393	31.594842
589.271145	39250.608057	31.599860
590.128297	39302.377196	31.604877
590.173778	39353.066958	31.609895
591.496455	39409.971938	31.614912
591.151138	39473.760963	31.619930
591.780758	39533.970462	31.624948
592.187616	39596.024127	31.629965
592.599745	39664.359553	31.634983
593.010033	39730.517198	31.640000
593.719099	39792.440818	31.645018
593.954307	39849.189352	31.650036
594.650294	39923.721735	31.655053
594.955928	39999.849318	31.660071
595.780170	40068.825967	31.665088
596.550277	40148.574682	31.670106
597.378701	40216.038913	31.675124
598.650333	40270.780043	31.680141
598.379727	40341.021861	31.685159
599.294762	40392.455791	31.690176
599.920589	40454.935755	31.695194
600.549692	40520.392568	31.700212
601.331510	40568.004390	31.705229
601.361060	40636.187937	31.710247
602.378765	40691.437920	31.715264
602.634932	40754.607347	31.720282
603.138497	40824.563646	31.725300
603.375409	40894.385932	31.730317
603.785522	40970.392241	31.735335
604.449513	41040.965942	31.740352
605.122726	41110.638512	31.745370
605.654723	41182.899240	31.750388
606.689003	41248.911177	31.755405
607.032247	41328.532861	31.760423
607.659846	41392.063887	31.765440
608.025241	41469.630127	31.770458
608.749504	41555.044323	31.775476
609.604109	41617.406898	31.780493
610.755582	41694.833082	31.785511
611.819303	41737.047876	31.790528
613.034068	41792.270522	31.795546
613.915861	41846.259009	31.800564
614.582583	41883.660841	31.805581
615.170500	41926.156498	31.810599
615.436713	41964.599587	31.815616
616.317352	42024.524705	31.820634
616.457697	42083.651723	31.825652
617.108072	42123.712228	31.830669
617.429420	42193.660669	31.835687
618.064898	42250.445812	31.840704
618.606697	42315.298703	31.845722
619.278541	42377.758276	31.850740
620.106390	42430.399979	31.855757
620.534678	42487.275014	31.860775
620.978597	42543.958094	31.865792
621.639677	42602.940697	31.870810
622.098211	42671.396015	31.875828
623.298537	42721.275040	31.880845
623.177197	42786.568396	31.885863
623.895667	42857.698502	31.890880
624.630780	42915.561102	31.895898
624.889125	42989.359737	31.900916
625.622914	43052.764530	31.905933
626.140266	43125.837288	31.910951
626.561490	43188.149879	31.915968
627.532091	43262.983244	31.920986
628.115201	43333.759426	31.926004
628.533450	43398.343559	31.931021
628.940982	43475.560370	31.936039
629.569051	43549.174705	31.941056
631.132089	43610.775217	31.946074
631.402637	43683.579809	31.951092
632.297178	43736.526356	31.956109
632.781843	43809.291592	31.961127
633.433036	43873.228004	31.966144
634.042543	43915.746567	31.971162
634.283029	43982.156743	31.976180
635.154661	44040.255186	31.981197
635.373100	44107.601115	31.986215
635.730319	44180.023312	31.991232
636.528196	44243.411655	31.996250
636.880129	44319.757259	32.001268
637.662812	44386.612788	32.006285
638.228254	44458.561440	32.011303
638.719497	44534.697732	32.016320
639.695478	44601.653533	32.021338
639.972623	44690.865871	32.026356
640.261160	44767.710449	32.031373
640.992232	44846.323726	32.036391
641.511518	44928.652563	32.041408
642.783569	45008.784361	32.046426
643.539690	45087.226975	32.051444
644.902367	45138.230912	32.056461
645.878039	45198.175106	32.061479
646.590197	45254.251932	32.066496
647.497153	45310.646084	32.071514
647.844853	45377.409097	32.076532
648.785722	45433.425163	32.081549
649.461114	45491.988005	32.086567
649.875053	45549.803160	32.091584
650.374096	45604.076414	32.096602
650.666336	45673.335319	32.101620
651.517260	45736.725879	32.106637
652.108991	45805.561307	32.111655
652.565017	45877.556182	32.116672
653.218607	45938.467408	32.121690
653.318763	46024.147700	32.126708
653.791012	46105.324350	32.131725
654.362963	46180.250164	32.136743
655.173491	46261.817976	32.141760
656.189801	46328.681365	32.146778
656.824568	46415.569813	32.151796
657.677696	46476.713855	32.156813
658.870998	46534.749029	32.161831
659.546897	46600.708450	32.166848
660.703698	46654.009821	32.171866
661.229465	46716.919292	32.176884
661.645483	46784.701931	32.181901
662.185269	46845.619754	32.186919
662.473837	46920.720185	32.191936
663.133937	46982.495818	32.196954
663.815290	47055.053427	32.201972
664.609038	47110.559561	32.206989
665.731659	47170.317392	32.212007
666.114786	47242.648873	32.217024
666.775646	47309.630276	32.222042
666.807010	47383.367981	32.227060
667.632762	47448.382420	32.232077
668.458342	47516.710192	32.237095
668.991078	47578.964362	32.242112
669.753906	47647.195965	32.247130
669.929828	47720.588045	32.252148
670.516233	47791.345485	32.257165
670.899610	47860.189246	32.262183
671.621939	47941.201325	32.267200
672.283768	48012.524643	32.272218
673.047084	48092.873390	32.277236
673.806056	48166.416796	32.282253
674.310546	48245.673485	32.287271
674.782434	48331.827839	32.292288
675.250802	48412.010509	32.297306
675.871176	48494.523701	32.302324
676.311578	48586.530940	32.307341
677.288410	48671.554840	32.312359
677.381621	48771.802989	32.317376
678.369168	48849.422243	32.322394
678.891332	48960.305343	32.327412
679.353334	49057.933358	32.332429
680.207061	49148.507952	32.337447
680.768205	49239.556346	32.342464
681.363382	49337.586206	32.347482
682.254182	49453.405912	32.352500
682.960473	49541.076377	32.357517
683.781079	49641.766645	32.362535
684.175105	49739.599251	32.367552
685.206027	49831.201675	32.372570
685.897801	49934.714139	32.377588
686.369053	50033.678448	32.382605
687.149659	50134.131734	32.387623
687.478877	50240.108581	32.392640
688.798659	50333.571780	32.397658
689.463435	50436.472412	32.402676
690.218721	50531.202018	32.407693
691.140056	50622.409972	32.412711
691.721931	50717.479754	32.417728
692.709623	50807.129368	32.422746
693.284264	50903.944987	32.427764
693.752628	50995.933552	32.432781
694.969725	51090.668888	32.437799
695.577877	51187.492803	32.442816
696.316087	51276.542887	32.447834
697.024021	51365.674377	32.452852
697.924870	51447.640285	32.457869
698.329923	51538.770369	32.462887
699.057082	51629.024358	32.467904
699.877686	51725.277504	32.472922
700.595232	51818.958377	32.477940
701.293690	51909.806151	32.482957
702.104739	51985.263118	32.487975
702.900679	52068.140440	32.492992
704.065095	52149.842994	32.498010
704.664491	52241.221040	32.503028
705.054388	52320.934076	32.508045
705.581980	52396.870817	32.513063
706.221970	52484.502644	32.518080
707.205362	52556.021274	32.523098
707.770278	52635.092725	32.528116
708.461244	52713.599523	32.533133
709.110262	52792.783565	32.538151
709.561535	52883.393846	32.543168
710.481310	52958.930693	32.548186
711.359955	53037.520359	32.553204
712.245397	53113.518606	32.558221
712.898257	53188.830362	32.563239
713.646529	53269.578933	32.568256
714.628019	53339.799117	32.573274
715.310070	53413.249078	32.578292
716.103013	53485.770441	32.583309
717.440570	53530.283215	32.588327
718.373834	53604.461721	32.593344
719.187962	53672.020024	32.598362
719.947232	53732.138258	32.603380
720.598763	53783.763877	32.608397
721.349926	53840.534932	32.613415
721.642918	53919.544361	32.618432
722.432337	53976.675739	32.623450
722.843652	54052.727217	32.628468
723.489567	54118.413910	32.633485
723.956262	54189.654154	32.638503
724.417162	54278.980128	32.643520
725.143530	54358.106625	32.648538
725.503816	54451.482038	32.653556
725.990511	54536.387848	32.658573
726.779322	54622.550287	32.663591
727.174176	54727.731172	32.668608
727.903502	54813.304322	32.673626
728.246017	54914.204555	32.678644
728.743901	55024.285559	32.683661
729.655327	55128.849264	32.688679
730.026223	55247.319737	32.693696
731.331330	55341.093543	32.698714
731.989073	55449.481243	32.703732
732.715634	55550.110361	32.708749
733.529638	55654.067896	32.713767
733.756508	55776.585222	32.718784
734.596344	55883.850838	32.723802
735.614171	55990.024884	32.728820
736.969538	56087.218675	32.733837
737.998163	56171.760536	32.738855
739.037922	56261.021480	32.743872
740.016791	56349.730816	32.748890
740.640022	56449.257275	32.753908
741.311218	56525.690724	32.758925
742.775121	56608.371432	32.763943
743.717569	56682.983216	32.768960
744.135541	56760.269840	32.773978
744.824895	56834.085030	32.778996
745.374838	56914.073400	32.784013
746.187567	56986.610403	32.789031
746.762698	57064.143016	32.794048
747.327707	57138.644191	32.799066
748.289928	57223.934938	32.804084
748.601010	57308.193703	32.809101
749.407454	57384.664119	32.814119
749.769944	57474.634198	32.819136
750.289641	57558.516999	32.824154
750.916218	57641.484415	32.829172
751.457821	57735.747775	32.834189
752.083422	57839.856303	32.839207
752.829108	57948.880701	32.844224
753.534118	58037.625409	32.849242
754.225583	58140.719317	32.854260
754.917106	58246.297527	32.859277
755.739671	58340.193244	32.864295
756.278790	58456.138344	32.869312
756.858529	58566.142502	32.874330
757.900879	58672.048360	32.879348
758.381823	58792.467407	32.884365
759.385619	58898.153516	32.889383
760.276113	59001.249294	32.894400
761.388835	59102.303978	32.899418
762.839674	59195.110047	32.904436
763.529386	59288.729518	32.909453
764.966146	59376.096960	32.914471
765.688462	59457.159259	32.919488
766.679870	59542.208249	32.924506
767.794899	59617.047769	32.929524
768.313047	59703.050724	32.934541
769.276751	59775.217881	32.939559
769.998310	59850.315272	32.944576
770.990749	59926.542169	32.949594
772.101731	60009.322490	32.954612
772.605098	60091.265448	32.959629
773.721820	60156.138998	32.964647
774.543917	60223.932811	32.969664
775.064433	60290.015030	32.974682
775.905613	60360.119405	32.979700
776.341887	60448.168465	32.984717
777.352867	60511.607479	32.989735
777.787209	60582.129943	32.994752
778.456271	60670.386592	32.999770
778.963052	60759.866058	33.004788
779.224333	60849.792500	33.009805
780.257798	60932.874266	33.014823
781.217073	61015.874262	33.019840
781.796957	61104.299749	33.024858
782.617402	61190.630090	33.029876
783.185776	61288.881151	33.034893
784.081862	61376.488801	33.039911
784.646497	61472.870350	33.044928
785.119545	61569.438706	33.049946
785.947451	61659.897410	33.054964
786.391049	61765.864925	33.059981
787.532021	61854.248084	33.064999
787.868742	61960.057906	33.070016
788.405201	62061.756849	33.075034
789.185389	62154.646928	33.080052
790.003527	62255.767587	33.085069
790.806279	62346.100851	33.090087
791.797344	62450.688540	33.095104
792.901851	62533.069224	33.100122
793.883585	62623.727038	33.105140
794.160707	62728.375201	33.110157
795.332085	62812.585083	33.115175
796.070051	62909.714843	33.120192
797.140709	63014.456097	33.125210
797.709781	63100.097834	33.130228
798.215184	63205.006404	33.135245
799.148756	63300.953954	33.140263
799.223184	63405.121860	33.145280
799.892356	63512.456727	33.150298
801.018654	63621.376460	33.155316
801.771370	63741.221529	33.160333
802.648151	63845.481781	33.165351
803.609509	63950.252777	33.170368
803.944413	64066.820711	33.175386
805.194635	64177.504879	33.180404
805.815718	64285.591611	33.185421
806.734930	64399.595762	33.190439
807.621729	64511.033035	33.195456
808.686962	64623.875436	33.200474
810.025305	64729.995572	33.205492
810.824463	64831.068741	33.210509
811.583953	64918.493421	33.215527
812.513033	65026.505924	33.220544
812.914919	65130.948740	33.225562
813.958542	65238.304170	33.230580
814.751873	65355.059939	33.235597
815.364888	65450.389434	33.240615
815.822823	65556.203011	33.245632
816.352887	65678.341686	33.250650
817.811803	65780.457071	33.255668
818.543756	65888.147377	33.260685
819.288230	66005.364000	33.265703
820.053201	66116.893858	33.270720
820.423075	66237.286583	33.275738
821.458504	66351.837770	33.280756
822.367733	66472.923447	33.285773
823.280352	66582.540016	33.290791
823.737203	66703.679203	33.295808
824.752914	66825.905699	33.300826
825.317317	66938.928450	33.305844
826.197625	67065.422059	33.310861
827.249844	67189.749871	33.315879
828.541983	67294.278489	33.320896
829.767079	67407.531997	33.325914
830.889573	67510.503698	33.330932
831.519898	67604.992644	33.335949
832.779363	67693.740511	33.340967
833.845614	67770.305872	33.345984
834.239292	67862.794176	33.351002
835.658687	67945.572088	33.356020
835.915452	68035.043218	33.361037
836.626138	68124.196697	33.366055
837.583973	68220.497576	33.371072
838.175450	68314.888823	33.376090
838.724974	68412.322784	33.381108
839.068499	68526.637431	33.386125
839.926020	68620.187733	33.391143
840.689510	68726.173397	33.396160
840.798629	68852.006616	33.401178
842.036649	68963.805476	33.406196
842.543520	69081.737328	33.411213
842.995675	69209.524707	33.416231
843.951130	69338.232066	33.421248
844.598596	69470.009236	33.426266
845.359172	69589.196720	33.431284
846.208046	69725.202991	33.436301
846.953088	69847.790303	33.441319
848.072631	69990.423256	33.446336
849.045904	70129.110946	33.451354
850.032402	70257.243014	33.456372
850.926476	70390.071231	33.461389
851.962510	70523.445087	33.466407
852.598662	70655.319949	33.471424
853.407000	70789.468001	33.476442
854.363139	70913.947642	33.481460
854.970509	71050.591717	33.486477
856.445772	71171.113678	33.491495
858.271657	71280.958273	33.496512
859.068705	71403.115438	33.501530
860.223312	71509.775020	33.506548
861.333888	71619.256885	33.511565
862.002439	71738.712257	33.516583
862.648570	71843.651860	33.521600
863.341605	71966.563598	33.526618
864.244216	72073.250122	33.531636
864.580109	72199.949304	33.536653
865.415549	72313.845511	33.541671
866.274355	72441.721390	33.546688
867.406027	72586.987557	33.551706
867.995432	72695.937963	33.556724
868.503738	72820.024518	33.561741
869.287786	72953.532283	33.566759
870.012894	73080.163560	33.571776
870.998644	73222.321965	33.576794
871.837113	73348.302915	33.581812
873.295708	73483.962571	33.586829
874.663511	73588.116506	33.591847
875.687145	73699.255412	33.596864
876.566270	73821.886348	33.601882
877.662182	73932.166535	33.606900
878.962766	74041.792391	33.611917
879.719957	74140.278986	33.616935
881.044997	74223.716844	33.621952
881.839093	74324.354708	33.626970
882.739450	74416.474173	33.631988
883.394567	74515.561810	33.637005
884.092792	74599.924356	33.642023
884.855087	74698.342985	33.647040
884.974250	74816.422784	33.652058
885.930087	74918.376545	33.657076
886.434865	75037.707083	33.662093
887.194151	75156.362162	33.667111
888.595509	75264.458785	33.672128
889.319559	75375.733314	33.677146
890.101890	75493.298314	33.682164
890.595863	75618.263240	33.687181
891.207487	75750.058984	33.692199
891.952392	75871.990501	33.697216
892.373079	76015.661487	33.702234
893.232632	76154.925344	33.707252
893.928717	76300.897712	33.712269
894.580839	76446.916514	33.717287
895.698611	76597.100934	33.722304
896.600301	76743.135852	33.727322
897.854564	76878.459040	33.732340
899.415291	77003.565278	33.737357
900.249127	77139.215068	33.742375
901.687208	77267.816571	33.747392
902.736466	77398.623501	33.752410
904.214198	77519.217597	33.757428
905.261735	77634.509084	33.762445
906.212216	77751.272725	33.767463
907.367285	77866.597590	33.772480
907.857612	77978.386845	33.777498
909.207057	78096.918457	33.782516
910.105025	78208.158264	33.787533
910.954460	78319.539776	33.792551
912.046452	78422.074471	33.797568
912.932043	78547.273273	33.802586
913.985581	78647.297804	33.807604
914.814305	78767.364453	33.812621
915.185357	78876.483640	33.817639
916.240948	78990.205445	33.822656
916.874951	79109.219146	33.827674
917.609536	79234.694320	33.832692
918.528482	79368.755010	33.837709
919.143968	79492.790630	33.842727
920.162833	79621.641788	33.847744
920.702843	79761.501361	33.852762
921.270143	79891.658697	33.857780
922.088239	80026.847648	33.862797
923.176472	80165.072143	33.867815
924.340023	80306.770500	33.872832
925.040546	80443.032250	33.877850
926.091720	80575.356541	33.882868
926.695799	80728.851240	33.887885
927.714152	80878.473669	33.892903
928.753437	81002.014668	33.897920
929.492762	81137.906944	33.902938
930.291044	81264.552784	33.907956
931.739187	81391.341101	33.912973
932.398836	81522.921733	33.917991
933.512729	81646.073797	33.923008
934.661378	81774.168239	33.928026
935.129476	81896.084593	33.933044
936.152441	82032.060099	33.938061
936.705291	82169.667043	33.943079
938.125771	82302.956664	33.948096
938.983661	82438.152958	33.953114
940.157906	82582.305747	33.958132
941.378899	82705.280601	33.963149
942.186138	82836.925677	33.968167
943.125328	82950.984399	33.973184
943.703342	83093.236722	33.978202
944.913808	83227.466095	33.983220
945.928272	83367.987587	33.988237
946.489186	83498.172668	33.993255
947.754433	83639.076783	33.998272
948.553256	83779.669320	34.003290
949.693930	83922.747827	34.008308
950.702365	84054.941127	34.013325
951.241710	84202.895311	34.018343
952.150137	84338.106621	34.023360
952.975991	84490.234090	34.028378
954.301475	84621.243633	34.033396
955.987819	84752.394598	34.038413
956.701064	84882.865016	34.043431
958.027992	85020.811800	34.048448
959.026252	85150.912176	34.053466
960.197648	85292.063770	34.058484
960.956747	85426.591859	34.063501
962.014380	85560.190002	34.068519
963.148914	85683.562331	34.073536
963.918790	85820.261321	34.078554
964.514260	85944.227239	34.083572
965.852487	86074.154248	34.088589
966.430976	86212.533585	34.093607
967.128690	86346.286395	34.098624
968.115448	86492.298844	34.103642
968.991424	86629.756373	34.108660
970.161342	86757.918725	34.113677
970.957473	86910.326319	34.118695
971.719597	87051.843258	34.123712
972.675927	87205.522620	34.128730
973.147603	87355.792664	34.133748
974.036599	87504.175910	34.138765
974.753904	87672.733190	34.143783
975.915270	87820.027546	34.148800
976.975888	87989.914224	34.153818
977.851018	88151.226893	34.158836
978.968182	88300.373410	34.163853
979.187810	88464.445829	34.168871
980.532526	88623.219372	34.173888
981.299760	88777.719636	34.178906
982.426337	88927.064620	34.183924
983.576035	89075.014211	34.188941
983.931998	89229.492864	34.193959
985.044464	89392.937704	34.198976
986.054094	89564.293558	34.203994
986.291261	89732.624697	34.209012
987.117386	89900.343489	34.214029
988.306401	90073.020323	34.219047
989.552907	90247.707556	34.224064
990.866904	90428.739059	34.229082
992.120164	90581.053627	34.234100
993.349983	90745.196361	34.239117
994.261309	90913.483519	34.244135
995.577302	91064.878938	34.249152
996.834212	91236.508043	34.254170
997.722488	91394.877867	34.259188
998.815774	91550.295688	34.264205
999.637523	91711.976648	34.269223
1000.943911	91870.480494	34.274240
1002.296799	92015.115433	34.279258
1003.618487	92168.149753	34.284276
1004.745765	92307.204269	34.289293
1005.770962	92466.747553	34.294311
1006.819121	92615.457617	34.299328
1007.785823	92765.056046	34.304346
1008.726015	92906.095574	34.309364
1009.690400	93058.943416	34.314381
1010.953345	93202.360061	34.319399
1012.178282	93348.898410	34.324416
1012.945034	93506.954477	34.329434
1013.731169	93648.746243	34.334452
1014.775692	93790.070455	34.339469
1015.612209	93962.296943	34.344487
1016.233706	94107.664411	34.349504
1016.866004	94271.223983	34.354522
1018.031981	94444.448209	34.359540
1019.158726	94610.470113	34.364557
1019.807611	94779.695820	34.369575
1020.764294	94941.912843	34.374592
1022.063230	95115.960902	34.379610
1022.835118	95286.485706	34.384628
1024.266053	95444.313705	34.389645
1025.223810	95615.954748	34.394663
1027.119604	95758.125566	34.399680
1028.672232	95906.262452	34.404698
1029.821457	96060.242878	34.409716
1030.847434	96202.311925	34.414733
1032.075015	96349.063669	34.419751
1033.093010	96484.241469	34.424768
1033.706624	96636.322925	34.429786
1034.964701	96789.586439	34.434804
1036.461461	96934.364575	34.439821
1037.022322	97069.952988	34.444839
1037.818814	97208.021508	34.449856
1038.634131	97335.938942	34.454874
1039.629199	97484.864305	34.459892
1040.360116	97613.487672	34.464909
1041.940085	97752.627899	34.469927
1043.603061	97873.520971	34.474944
1044.510756	98004.179996	34.479962
1045.052092	98137.491887	34.484980
1046.327052	98264.752811	34.489997
1047.127929	98415.742864	34.495015
1048.079926	98556.951374	34.500032
1048.534399	98691.806874	34.505050
1049.558861	98835.277465	34.510068
1050.521894	98985.749262	34.515085
1051.598002	99149.530300	34.520103
1052.551928	99298.992459	34.525120
1053.700170	99459.236475	34.530138
1054.251683	99629.346957	34.535156
1055.219799	99792.941638	34.540173
1056.049939	99968.553144	34.545191
1057.172744	100141.538726	34.550208
1057.981720	100316.921949	34.555226
1059.174877	100497.394652	34.560244
1060.363407	100667.409215	34.565261
1061.561529	100835.726309	34.570279
1062.845147	101002.928101	34.575296
1063.459640	101181.041524	34.580314
1064.648819	101361.539906	34.585332
1065.872787	101536.486712	34.590349
1066.716789	101717.553224	34.595367
1067.953068	101895.818342	34.600384
1068.530571	102072.095193	34.605402
1069.673761	102271.692909	34.610420
1070.743059	102450.142363	34.615437
1071.500984	102639.043993	34.620455
1072.407932	102827.364216	34.625472
1073.436579	103023.023197	34.630490
1074.028906	103228.041708	34.635508
1075.103934	103429.091005	34.640525
1075.890733	103643.616184	34.645543
1077.017586	103853.626725	34.650560
1078.190777	104062.415125	34.655578
1079.093518	104271.884745	34.660596
1080.290437	104492.299300	34.665613
1080.903418	104712.296373	34.670631
1082.334752	104931.243207	34.675648
1083.592872	105136.909726	34.680666
1084.628903	105360.132808	34.685684
1086.024179	105565.753808	34.690701
1086.907659	105780.165634	34.695719
1088.254292	105987.888106	34.700736
1090.376894	106184.206308	34.705754
1091.440614	106387.939761	34.710772
1092.947062	106574.993180	34.715789
1094.192649	106756.531935	34.720807
1095.370337	106939.058869	34.725824
1097.329115	107096.474491	34.730842
1098.785241	107248.948374	34.735860
1100.337046	107395.807977	34.740877
1101.765744	107530.465861	34.745895
1102.811623	107681.315049	34.750912
1104.009088	107819.383381	34.755930
1105.190560	107958.139176	34.760948
1106.214519	108106.296376	34.765965
1107.032408	108250.423469	34.770983
1108.165233	108397.955584	34.776000
1109.566353	108535.789998	34.781018
1110.523810	108679.059409	34.786036
1111.477348	108818.023279	34.791053
1112.339489	108962.767259	34.796071
1113.321428	109119.665119	34.801088
1114.292355	109267.989701	34.806106
1115.391318	109430.405101	34.811124
1116.363718	109588.118007	34.816141
1117.350964	109747.146742	34.821159
1117.980077	109916.625499	34.826176
1119.172648	110076.520408	34.831194
1120.043026	110261.921795	34.836212
1120.859279	110437.351088	34.841229
1121.882517	110617.598032	34.846247
1122.850641	110804.531851	34.851264
1123.516200	110983.879610	34.856282
1124.450193	111177.270056	34.861300
1125.542902	111368.696359	34.866317
1126.340855	111581.508681	34.871335
1127.102587	111781.824633	34.876352
1128.589555	111990.202007	34.881370
1129.766687	112204.297056	34.886388
1131.233983	112402.393576	34.891405
1132.576341	112597.776325	34.896423
1133.366416	112809.560434	34.901440
1134.895889	113020.738102	34.906458
1135.988680	113227.557778	34.911476
1136.423548	113431.564927	34.916493
1137.843646	113637.178622	34.921511
1138.959431	113850.891242	34.926528
1140.147536	114056.851775	34.931546
1141.670576	114276.275346	34.936564
1142.142961	114488.126390	34.941581
1143.751432	114703.154768	34.946599
1144.545683	114920.250052	34.951616
1145.637673	115127.349757	34.956634
1146.777334	115345.390086	34.961652
1148.093472	115553.974953	34.966669
1149.901917	115762.996544	34.971687
1150.864693	115977.942305	34.976704
1152.325391	116186.228249	34.981722
1153.019674	116398.917020	34.986740
1154.476593	116620.080416	34.991757
1155.786014	116822.859606	34.996775
1156.648272	117017.607197	35.001792
1157.943655	117212.611393	35.006810
1158.706492	117401.942595	35.011828
1160.202243	117593.671168	35.016845
1161.390578	117794.437760	35.021863
1162.070768	117994.608461	35.026880
1163.593191	118197.208695	35.031898
1164.510723	118400.053282	35.036916
1165.501691	118610.920682	35.041933
1166.866134	118809.788641	35.046951
1168.184082	119027.965475	35.051968
1169.134829	119236.069055	35.056986
1170.753212	119441.183197	35.062004
1171.708221	119648.123103	35.067021
1172.624507	119856.553758	35.072039
1173.680991	120074.897135	35.077056
1174.970867	120286.434981	35.082074
1175.681673	120506.640221	35.087092
1176.974379	120730.929490	35.092109
1178.255129	120943.588772	35.097127
1178.992142	121172.538735	35.102144
1180.560740	121390.183089	35.107162
1181.259114	121630.739041	35.112180
1182.048100	121867.580804	35.117197
1183.386509	122099.349727	35.122215
1184.234565	122347.667237	35.127232
1185.640870	122585.372134	35.132250
1186.769668	122837.688478	35.137268
1187.826986	123084.151190	35.142285
1188.782687	123331.989404	35.147303
1189.853431	123589.366139	35.152320
1191.068926	123836.251449	35.157338
1192.379844	124097.393581	35.162356
1193.693064	124344.164867	35.167373
1195.430382	124597.329489	35.172391
1197.307625	124832.056161	35.177408
1199.043159	125049.229200	35.182426
1201.033722	125277.970134	35.187444
1202.685978	125489.989257	35.192461
1204.064527	125687.011619	35.197479
1205.310883	125907.329081	35.202496
1206.720678	126107.225980	35.207514
1208.235839	126316.270242	35.212532
1208.902281	126529.238418	35.217549
1210.493377	126740.363937	35.222567
1211.181167	126949.363955	35.227584
1212.389614	127153.573637	35.232602
1214.008522	127350.172431	35.237620
1215.154148	127547.943585	35.242637
1217.077419	127739.384438	35.247655
1218.292340	127942.647466	35.252672
1219.486137	128133.277587	35.257690
1220.232295	128335.152993	35.262708
1221.674377	128538.964066	35.267725
1222.623835	128728.600170	35.272743
1223.070421	128923.115090	35.277760
1224.345711	129108.286373	35.282778
1225.601821	129308.293318	35.287796
1226.213429	129502.707469	35.292813
1227.652464	129708.428021	35.297831
1228.588697	129908.747018	35.302848
1230.598222	130098.197120	35.307866
1231.848896	130294.851860	35.312884
1232.800964	130491.939226	35.317901
1234.061129	130698.723574	35.322919
1234.975845	130913.402748	35.327936
1235.761701	131123.833243	35.332954
1237.097272	131334.411868	35.337972
1237.758955	131556.415296	35.342989
1238.643743	131781.652792	35.348007
1239.751698	132020.760742	35.353024
1240.956364	132256.101355	35.358042
1241.532145	132504.583874	35.363060
1242.471133	132739.897386	35.368077
1243.502801	132995.557217	35.373095
1244.629848	133267.658588	35.378112
1245.968901	133523.523461	35.383130
1247.276906	133797.880269	35.388148
1248.634028	134059.780970	35.393165
1250.199753	134317.996688	35.398183
1251.023879	134584.328745	35.403200
1252.796394	134849.980764	35.408218
1253.799753	135114.105675	35.413236
1255.000734	135382.915313	35.418253
1256.614350	135640.600572	35.423271
1257.348437	135917.849741	35.428288
1258.894412	136192.591238	35.433306
1260.165604	136461.803214	35.438324
1261.365770	136743.822798	35.443341
1262.689466	137012.041187	35.448359
1263.921769	137295.822281	35.453376
1264.903658	137573.587804	35.458394
1266.187523	137854.144127	35.463412
1267.637447	138144.602541	35.468429
1269.242225	138407.864059	35.473447
1270.179352	138702.421797	35.478464
1271.413212	138985.252952	35.483482
1272.988708	139260.508626	35.488500
1274.393860	139544.177281	35.493517
1275.861295	139810.364099	35.498535
1277.387433	140082.946521	35.503552
1278.727484	140361.890513	35.508570
1280.765249	140622.507920	35.513588
1282.377950	140877.341541	35.518605
1283.966343	141143.860198	35.523623
1285.269003	141403.784993	35.528640
1285.900702	141654.582113	35.533658
1287.465716	141898.766578	35.538676
1288.684011	142168.120800	35.543693
1289.751548	142419.317931	35.548711
1291.058473	142667.470377	35.553728
1292.204142	142907.954519	35.558746
1293.633805	143147.224966	35.563764
1294.816591	143402.340561	35.568781
1296.090677	143637.468662	35.573799
1297.451950	143887.421063	35.578816
1298.481449	144131.813920	35.583834
1299.684563	144384.688307	35.588852
1300.803435	144642.677064	35.593869
1302.243758	144892.217055	35.598887
1303.518634	145146.403410	35.603904
1304.535236	145404.326301	35.608922
1306.024140	145659.608321	35.613940
1307.221785	145929.488799	35.618957
1308.711006	146191.546925	35.623975
1309.707538	146459.550650	35.628992
1311.062330	146722.929199	35.634010
1312.574065	146981.970589	35.639028
1313.716817	147249.891599	35.644045
1315.601893	147503.583936	35.649063
1316.650402	147770.205790	35.654080
1318.241156	148039.780704	35.659098
1319.487280	148300.309935	35.664116
1320.941270	148569.835973	35.669133
1322.438088	148829.412759	35.674151
1323.793998	149095.978734	35.679168
1324.549959	149356.611859	35.684186
1325.847832	149636.509423	35.689204
1327.286228	149906.301337	35.694221
1328.849592	150174.069711	35.699239
1330.358883	150448.571753	35.704256
1331.790291	150718.154974	35.709274
1333.425735	150979.879012	35.714292
1334.917679	151233.879295	35.719309
1336.789357	151489.363746	35.724327
1338.199603	151752.387329	35.729344
1339.409317	151997.840883	35.734362
1340.810176	152254.425733	35.739380
1342.239904	152516.347593	35.744397
1343.808560	152765.930503	35.749415
1345.392928	153017.034500	35.754432
1346.153808	153260.175377	35.759450
1347.703437	153513.254660	35.764468
1348.220454	153782.051574	35.769485
1349.701903	154034.372077	35.774503
1350.821472	154308.663601	35.779520
1351.653921	154582.194300	35.784538
1352.881549	154856.331564	35.789556
1353.785226	155138.441936	35.794573
1355.557919	155419.961554	35.799591
1356.822124	155713.482075	35.804608
1358.285996	156000.006045	35.809626
1359.729960	156283.934845	35.814644
1360.598886	156579.711290	35.819661
1362.073651	156848.250656	35.824679
1363.155927	157126.170616	35.829696
1364.772766	157396.541453	35.834714
1365.946020	157666.837764	35.839732
1367.179314	157939.980020	35.844749
1368.415165	158221.585548	35.849767
1369.432884	158506.541530	35.854784
1370.663973	158788.024860	35.859802
1371.893670	159071.984254	35.864820
1372.810352	159388.731246	35.869837
1374.018429	159682.023332	35.874855
1375.592004	159983.349241	35.879872
1376.328386	160295.312859	35.884890
1378.317004	160607.863747	35.889908
1379.699830	160918.313035	35.894925
1381.364790	161228.056556	35.899943
1383.200271	161535.400580	35.904960
1384.872411	161841.696326	35.909978
1386.715297	162138.601524	35.914996
1387.826746	162443.842949	35.920013
1389.247255	162738.122074	35.925031
1390.560561	163038.625953	35.930048
1391.923845	163342.206547	35.935066
1393.684639	163646.254121	35.940084
1394.751172	163947.123701	35.945101
1396.305678	164256.755568	35.950119
1398.262737	164546.285754	35.955136
1399.532732	164848.966489	35.960154
1401.512957	165126.074498	35.965172
1403.289699	165420.297959	35.970189
1405.093809	165703.073458	35.975207
1406.640099	165978.548063	35.980224
1408.192403	166265.950868	35.985242
1409.413011	166541.180130	35.990260
1410.767503	166828.518866	35.995277
1411.651206	167106.981490	36.000295
1412.974805	167398.224677	36.005312
1414.335550	167704.880832	36.010330
1415.549730	167998.862081	36.015348
1416.801688	168292.052003	36.020365
1418.024251	168589.778979	36.025383
1419.665055	168890.177246	36.030400
1420.707657	169198.369789	36.035418
1422.139607	169497.449932	36.040436
1423.672773	169807.478698	36.045453
1425.153647	170106.592433	36.050471
1426.643356	170415.465179	36.055488
1428.501126	170709.708727	36.060506
1430.421118	171000.364828	36.065524
1431.763230	171297.682469	36.070541
1433.223337	171592.354872	36.075559
1434.918855	171874.323778	36.080576
1436.062222	172168.673222	36.085594
1437.512824	172453.783920	36.090612
1439.317506	172751.082161	36.095629
1440.879190	173020.453496	36.100647
1442.699350	173294.503055	36.105664
1444.313990	173556.406117	36.110682
1445.784262	173817.637289	36.115700
1447.020072	174085.623504	36.120717
1448.169759	174340.351081	36.125735
1449.367529	174606.481050	36.130752
1450.275777	174894.668507	36.135770
1451.265642	175164.009839	36.140788
1452.033110	175457.516893	36.145805
1452.986344	175761.794257	36.150823
1454.190671	176060.497002	36.155840
1455.482736	176385.559556	36.160858
1457.230181	176683.538450	36.165876
1458.627518	176991.199326	36.170893
1460.109301	177312.770495	36.175911
1461.801068	177625.956494	36.180928
1463.128252	177945.920832	36.185946
1464.414818	178270.374386	36.190964
1465.766380	178606.927114	36.195981
1467.260438	178932.516960	36.200999
1468.719306	179266.986748	36.206016
1469.931675	179603.633163	36.211034
1471.801356	179920.813278	36.216052
1473.990470	180253.184321	36.221069
1475.425133	180569.313123	36.226087
1476.998996	180893.670196	36.231104
1478.844970	181222.183956	36.236122
1480.450197	181535.966486	36.241140
1482.139078	181856.121037	36.246157
1483.703634	182176.577993	36.251175
1484.956457	182496.252436	36.256192
1486.209157	182819.114732	36.261210
1487.953661	183145.398071	36.266228
1489.247828	183471.074965	36.271245
1490.578676	183800.187380	36.276263
1492.320174	184125.969253	36.281280
1493.549446	184463.594838	36.286298
1495.070186	184780.774023	36.291316
1496.484492	185121.139063	36.296333
1497.310013	185466.024307	36.301351
1499.305633	185796.126238	36.306368
1500.714144	186141.448915	36.311386
1502.504906	186489.716704	36.316404
1504.022297	186834.060143	36.321421
1505.539646	187181.553753	36.326439
1507.749622	187504.113829	36.331456
1508.969708	187828.723817	36.336474
1510.615124	188217.419767	36.341492
1511.955276	188556.141948	36.346509
1513.977185	188879.198685	36.351527
1515.814881	189200.816123	36.356544
1517.933082	189515.570285	36.361562
1519.459198	189821.591934	36.366580
1521.082148	190138.630249	36.371597
1522.290639	190447.895762	36.376615
1523.870676	190733.994657	36.381632
1524.849457	191045.803362	36.386650
1525.973843	191346.518714	36.391668
1527.212527	191657.663955	36.396685
1528.052158	191968.574348	36.401703
1529.325795	192288.298606	36.406720
1530.611278	192618.991113	36.411738
1532.057604	192944.820916	36.416756
1533.428931	193287.410369	36.421773
1534.500301	193637.403620	36.426791
1535.273144	193989.239914	36.431808
1536.470618	194366.904371	36.436826
1537.758480	194742.549634	36.441844
1539.135010	195123.336321	36.446861
1540.190492	195504.853013	36.451879
1541.749280	195892.062373	36.456896
1543.259667	196290.556230	36.461914
1544.855330	196690.637543	36.466932
1546.823757	197086.759732	36.471949
1547.959908	197498.604805	36.476967
1549.407617	197900.178570	36.481984
1550.824683	198317.769932	36.487002
1552.830086	198714.110963	36.492020
1554.674399	199130.389816	36.497037
1556.349971	199531.667317	36.502055
1558.518991	199924.686038	36.507072
1560.510056	200323.361981	36.512090
1562.580903	200714.522709	36.517108
1564.941449	201085.828977	36.522125
1566.438797	201469.994384	36.527143
1568.632000	201825.347688	36.532160
1570.566430	202199.855923	36.537178
1572.189552	202569.530943	36.542196
1574.068247	202934.859729	36.547213
1575.771346	203288.488146	36.552231
1577.628345	203643.336195	36.557248
1578.850297	203996.059829	36.562266
1580.580054	204347.847457	36.567284
1582.365013	204698.522557	36.572301
1583.756986	205053.405839	36.577319
1585.073800	205401.992918	36.582336
1585.951466	205771.163232	36.587354
1587.878649	206132.854531	36.592372
1589.822463	206498.417401	36.597389
1591.681778	206862.612322	36.602407
1593.716601	207201.891168	36.607424
1595.606998	207548.383104	36.612442
1596.840382	207895.522221	36.617460
1598.260642	208246.275114	36.622477
1599.589401	208602.175119	36.627495
1601.031235	208955.568453	36.632512
1602.837349	209305.142278	36.637530
1604.135153	209667.807414	36.642548
1605.547703	210030.073488	36.647565
1606.876336	210393.853817	36.652583
1608.009936	210737.605685	36.657600
1609.319285	211089.709732	36.662618
1611.130145	211460.523008	36.667636
1612.490171	211818.640293	36.672653
1614.085740	212175.829792	36.677671
1615.314683	212549.109006	36.682688
1616.263206	212927.466364	36.687706
1618.004057	213300.280053	36.692724
1619.320616	213675.402796	36.697741
1620.817756	214072.795167	36.702759
1622.788783	214457.129908	36.707776
1624.464523	214843.904093	36.712794
1625.682643	215241.552201	36.717812
1627.571602	215637.690248	36.722829
1629.133547	216029.187188	36.727847
1631.552400	216424.247170	36.732864
1632.854487	216807.461006	36.737882
1635.303089	217205.414336	36.742900
1636.699121	217582.747974	36.747917
1638.060195	217980.763365	36.752935
1639.847098	218372.256149	36.757952
1641.698204	218779.969175	36.762970
1642.976020	219174.853838	36.767988
1645.124564	219566.339895	36.773005
1646.516902	219960.877620	36.778023
1647.868281	220360.986157	36.783040
1650.028293	220765.580417	36.788058
1651.212266	221173.289434	36.793076
1653.012949	221573.604766	36.798093
1654.613465	221975.428895	36.803111
1656.729956	222390.450076	36.808128
1658.215709	222786.632506	36.813146
1659.796596	223189.607086	36.818164
1662.113019	223587.021599	36.823181
1663.964359	224000.671289	36.828199
1665.577107	224393.509811	36.833216
1667.391215	224793.325514	36.838234
1669.584587	225179.082119	36.843252
1671.531920	225557.287318	36.848269
1672.804719	225951.890582	36.853287
1674.857407	226340.417911	36.858304
1676.543992	226734.292286	36.863322
1677.766513	227130.914251	36.868340
1679.497424	227511.702034	36.873357
1681.184808	227904.411194	36.878375
1682.906657	228289.673145	36.883392
1684.889479	228685.508998	36.888410
1686.900906	229064.068474	36.893428
1688.915758	229453.093504	36.898445
1690.008330	229831.812145	36.903463
1692.156065	230216.904668	36.908480
1693.642236	230599.876046	36.913498
1694.844969	230986.732430	36.918516
1696.426359	231368.673344	36.923533
1698.267979	231761.416983	36.928551
1699.425869	232134.008288	36.933568
1701.180666	232510.156105	36.938586
1702.853637	232890.154380	36.943604
1704.260377	233254.805743	36.948621
1706.001513	233655.293046	36.953639
1707.530077	234032.244936	36.958656
1709.119043	234425.037917	36.963674
1710.249385	234821.999882	36.968692
1711.742595	235213.286821	36.973709
1712.763842	235630.311150	36.978727
1714.501326	236043.759187	36.983744
1716.054830	236473.217381	36.988762
1717.011176	236906.792167	36.993780
1718.464669	237353.771295	36.998797
1719.788018	237805.473024	37.003815
1721.589842	238254.502822	37.008832
1722.795692	238718.826008	37.013850
1724.483924	239193.939781	37.018868
1726.057262	239671.411192	37.023885
1727.282546	240151.635753	37.028903
1729.382867	240636.868235	37.033920
1731.171424	241136.380355	37.038938
1732.498040	241636.201082	37.043956
1734.414232	242129.088584	37.048973
1736.390464	242639.773899	37.053991
1738.215331	243139.867712	37.059008
1739.991868	243624.678218	37.064026
1742.022911	244123.392028	37.069044
1744.601203	244621.428724	37.074061
1746.501679	245106.982334	37.079079
1748.284700	245604.572245	37.084096
1750.209477	246101.173273	37.089114
1751.294602	246599.163330	37.094132
1753.297032	247091.916492	37.099149
1754.568556	247607.505503	37.104167
1756.340508	248113.153144	37.109184
1758.340695	248617.492132	37.114202
1759.991010	249140.080048	37.119220
1761.648256	249642.268638	37.124237
1763.380087	250164.284707	37.129255
1764.979635	250673.469882	37.134272
1767.228876	251196.160366	37.139290
1768.995829	251719.162356	37.144308
1771.219705	252222.576904	37.149325
1773.049488	252733.781712	37.154343
1774.879219	253238.483575	37.159360
1776.976239	253752.666125	37.164378
1778.301417	254265.964781	37.169396
1780.105598	254778.241737	37.174413
1782.014780	255287.452474	37.179431
1784.337859	255796.465485	37.184448
1786.637857	256289.961147	37.189466
1788.753191	256792.735194	37.194484
1791.019070	257266.574639	37.199501
1793.128832	257738.484716	37.204519
1795.250637	258179.680211	37.209536
1797.080674	258636.726338	37.214554
1798.559100	259081.740599	37.219572
1800.285198	259523.130532	37.224589
1801.488771	259987.675801	37.229607
1803.363081	260442.046506	37.234624
1805.413984	260898.038023	37.239642
1807.050363	261363.169161	37.244660
1808.808768	261814.155042	37.249677
1810.253161	262279.115293	37.254695
1811.233689	262753.401329	37.259712
1812.974818	263236.219374	37.264730
1814.405851	263729.327526	37.269748
1815.775275	264221.886936	37.274765
1817.350742	264723.377919	37.279783
1818.651387	265246.787392	37.284800
1820.563026	265759.397136	37.289818
1821.933829	266291.481248	37.294836
1823.997127	266815.774568	37.299853
1825.452847	267353.964895	37.304871
1827.147021	267897.067232	37.309888
1829.068134	268428.622484	37.314906
1830.592260	268980.770254	37.319924
1832.802425	269528.430496	37.324941
1834.511695	270079.579438	37.329959
1836.544585	270628.995461	37.334976
1838.667328	271178.090258	37.339994
1841.158528	271731.693417	37.345012
1842.823272	272276.723779	37.350029
1844.799508	272834.223116	37.355047
1846.432315	273390.154226	37.360064
1848.431454	273937.587855	37.365082
1850.339793	274490.979878	37.370100
1851.911243	275053.471369	37.375117
1853.497929	275616.416075	37.380135
1855.348559	276184.496185	37.385152
1857.215390	276753.029225	37.390170
1859.254082	277329.558284	37.395188
1861.697219	277883.281862	37.400205
1863.813378	278438.507684	37.405223
1865.614688	279007.858250	37.410240
1868.067407	279550.220745	37.415258
1869.951343	280100.781972	37.420276
1872.017519	280659.870577	37.425293
1874.105945	281205.008208	37.430311
1876.063365	281756.491384	37.435328
1877.814468	282305.137656	37.440346
1879.220113	282868.345157	37.445364
1881.217385	283414.176758	37.450381
1883.281386	283968.504304	37.455399
1885.759104	284512.243103	37.460416
1888.773078	285038.717284	37.465434
1890.289333	285572.837304	37.470452
1892.241765	286104.924866	37.475469
1894.208478	286635.534727	37.480487
1895.928141	287141.927465	37.485504
1897.919874	287643.598115	37.490522
1899.613348	288144.657474	37.495540
1901.394702	288639.375261	37.500557
1903.540357	289138.397618	37.505575
1905.127182	289652.880490	37.510592
1906.723985	290157.123430	37.515610
1908.168919	290668.883158	37.520628
1909.925766	291182.238332	37.525645
1911.511045	291699.506740	37.530663
1913.269885	292238.434172	37.535680
1915.279077	292757.835093	37.540698
1917.271533	293302.152975	37.545716
1919.390838	293831.537337	37.550733
1921.541096	294364.901474	37.555751
1922.848197	294903.842521	37.560768
1924.892435	295451.493475	37.565786
1926.869231	296000.600833	37.570804
1928.151557	296553.405231	37.575821
1929.926173	297118.872321	37.580839
1931.624238	297686.330389	37.585856
1933.560271	298256.055734	37.590874
1935.140642	298835.667524	37.595892
1936.480615	299432.917470	37.600909
1938.526913	300028.036490	37.605927
1940.186324	300625.706856	37.610944
1942.078112	301229.606715	37.615962
1943.914381	301836.280360	37.620980
1945.905223	302441.323512	37.625997
1948.424193	303052.367414	37.631015
1949.942519	303676.885919	37.636032
1952.096996	304290.599349	37.641050
1953.893448	304915.543868	37.646068
1955.654506	305529.975969	37.651085
1958.122089	306158.935999	37.656103
1959.807616	306786.374295	37.661120
1962.235779	307400.729186	37.666138
1964.713480	308022.460880	37.671156
1967.134657	308637.264595	37.676173
1969.911488	309228.106320	37.681191
1972.715640	309814.494854	37.686208
1976.479311	310366.762680	37.691226
1979.147763	310919.010656	37.696244
1981.604511	311470.909883	37.701261
1984.072089	311996.520678	37.706279
1985.846727	312536.492017	37.711296
1987.749778	313056.478237	37.716314
1989.308672	313588.708308	37.721332
1991.391037	314121.175019	37.726349
1993.192575	314651.501994	37.731367
1994.411992	315188.602787	37.736384
1996.532034	315725.469249	37.741402
1997.951582	316281.013041	37.746420
1999.444352	316829.049175	37.751437
2001.566596	317364.962922	37.756455
2003.058632	317899.862951	37.761472
2004.911370	318436.702928	37.766490
2006.516070	318986.682813	37.771508
2007.923462	319534.863681	37.776525
2009.765722	320086.469480	37.781543
2011.039430	320660.181368	37.786560
2012.808401	321235.250651	37.791578
2014.393151	321811.082527	37.796596
2015.509902	322418.675637	37.801613
2017.297281	323026.757471	37.806631
2018.790136	323655.956787	37.811648
2020.535151	324275.737938	37.816666
2022.525453	324912.938260	37.821684
2024.160567	325558.367638	37.826701
2026.069440	326210.674159	37.831719
2028.438914	326862.691565	37.836736
2030.778098	327511.660330	37.841754
2032.965706	328167.476910	37.846772
2034.755195	328836.859962	37.851789
2037.051201	329502.086597	37.856807
2038.798945	330161.458672	37.861824
2040.839092	330837.350076	37.866842
2042.925974	331527.314329	37.871860
2045.106053	332194.686202	37.876877
2047.755496	332871.235170	37.881895
2050.159088	333551.803065	37.886912
2052.093740	334217.313241	37.891930
2053.961287	334893.310169	37.896948
2055.912429	335577.356128	37.901965
2058.422102	336258.860711	37.906983
2060.576528	336940.899271	37.912000
2062.415343	337627.780021	37.917018
2064.494651	338313.087340	37.922036
2066.589918	339002.088337	37.927053
2068.853186	339689.122013	37.932071
2070.958085	340393.483330	37.937088
2073.276661	341072.543741	37.942106
2075.602559	341753.674586	37.947124
2077.951104	342439.461878	37.952141
2080.895825	343112.320431	37.957159
2083.022611	343774.751322	37.962176
2085.045553	344448.154463	37.967194
2086.892016	345124.953427	37.972212
2089.033371	345797.656848	37.977229
2091.327353	346467.938737	37.982247
2093.230304	347154.265621	37.987264
2095.216484	347825.848928	37.992282
2097.373474	348500.311311	37.997300
2099.509629	349180.019985	38.002317
2102.531110	349848.274360	38.007335
2104.673064	350514.791115	38.012352
2106.860927	351174.260792	38.017370
2109.038455	351829.865146	38.022388
2111.239721	352490.657229	38.027405
2112.974672	353133.097039	38.032423
2115.166722	353774.941449	38.037440
2117.531911	354397.081940	38.042458
2119.478142	355018.904198	38.047476
2121.315320	355658.902699	38.052493
2123.401487	356283.371522	38.057511
2125.104565	356916.903389	38.062528
2127.257508	357561.664205	38.067546
2128.968800	358208.722919	38.072564
2130.989409	358867.972408	38.077581
2132.933867	359524.509397	38.082599
2134.680944	360190.456141	38.087616
2136.571275	360860.629207	38.092634
2138.708410	361536.101469	38.097652
2140.378823	362224.782742	38.102669
2142.216983	362905.508188	38.107687
2144.547963	363600.114900	38.112704
2146.448168	364306.857416	38.117722
2148.656372	365011.504739	38.122740
2150.468351	365720.265218	38.127757
2152.788918	366427.149691	38.132775
2155.409744	367145.967158	38.137792
2157.371117	367851.084914	38.142810
2160.048613	368567.049412	38.147828
2162.190132	369284.537214	38.152845
2164.951079	369986.382522	38.157863
2167.094584	370697.906850	38.162880
2169.436825	371400.556941	38.167898
2172.076410	372109.406655	38.172916
2174.012425	372821.760842	38.177933
2176.323204	373535.355244	38.182951
2178.082614	374245.529594	38.187968
2180.218351	374965.591423	38.192986
2182.734398	375695.843645	38.198004
2184.748871	376406.132696	38.203021
2187.260623	377131.688919	38.208039
2189.309509	377852.921848	38.213056
2191.496934	378577.031670	38.218074
2193.510708	379296.844882	38.223092
2195.118379	380039.126570	38.228109
2197.295683	380776.780920	38.233127
2199.343953	381531.250963	38.238144
2201.302424	382275.627937	38.243162
2203.534902	383019.383188	38.248180
2205.921304	383779.650470	38.253197
2208.736742	384527.555781	38.258215
2210.742108	385283.517137	38.263232
2212.880412	386045.040321	38.268250
2215.143721	386794.684974	38.273268
2216.703003	387550.972322	38.278285
2218.958976	388303.902795	38.283303
2220.845452	389082.531020	38.288320
2223.385352	389854.741478	38.293338
2226.022166	390623.012337	38.298356
2227.981549	391394.167728	38.303373
2230.301539	392144.812769	38.308391
2232.781476	392885.400209	38.313408
2234.842147	393624.545612	38.318426
2237.006196	394364.035109	38.323444
2239.019463	395100.287884	38.328461
2241.778042	395842.603822	38.333479
2244.115387	396570.401053	38.338496
2246.513021	397298.904661	38.343514
2249.165674	398034.315113	38.348532
2251.549262	398765.774309	38.353549
2253.583345	399498.364167	38.358567
2255.907583	400233.216764	38.363584
2257.880614	400967.552886	38.368602
2260.556197	401707.273400	38.373620
2262.222569	402465.465669	38.378637
2264.013964	403211.302437	38.383655
2265.894009	403973.014849	38.388672
2267.626217	404733.616765	38.393690
2269.842461	405506.300671	38.398708
2272.353722	406300.015165	38.403725
2274.508934	407084.140840	38.408743
2276.972748	407863.377889	38.413760
2279.623603	408653.300869	38.418778
2282.056810	409435.157235	38.423796
2284.364567	410229.449030	38.428813
2286.933587	411004.270193	38.433831
2289.536725	411789.194061	38.438848
2291.359771	412579.369260	38.443866
2294.020323	413370.263753	38.448884
2296.086728	414169.289363	38.453901
2298.233162	414973.316257	38.458919
2300.400356	415778.833864	38.463936
2301.876229	416585.583790	38.468954
2303.934544	417409.706606	38.473972
2306.096540	418239.456935	38.478989
2308.405840	419072.091931	38.484007
2310.863182	419911.206520	38.489024
2312.502592	420756.838432	38.494042
2315.647847	421594.158014	38.499060
2317.584870	422441.023196	38.504077
2319.894910	423281.769900	38.509095
2322.940694	424142.057619	38.514112
2325.589794	424982.231795	38.519130
2328.301569	425815.024844	38.524148
2331.011442	426659.534665	38.529165
2333.415501	427481.994434	38.534183
2335.970753	428317.865603	38.539200
2338.005842	429155.669099	38.544218
2340.123236	429991.656984	38.549236
2342.297797	430833.780572	38.554253
2344.210953	431669.642016	38.559271
2346.526880	432524.890828	38.564288
2348.808405	433378.038688	38.569306
2351.241428	434232.647219	38.574324
2353.594405	435095.486577	38.579341
2355.790442	435940.759572	38.584359
2358.555663	436764.194322	38.589376
2360.709792	437588.006999	38.594394
2363.238257	438403.376242	38.599412
2365.997891	439221.408479	38.604429
2368.194276	440032.119653	38.609447
2370.729817	440846.385950	38.614464
2372.833328	441663.731539	38.619482
2375.651583	442478.344264	38.624500
2378.315581	443286.224481	38.629517
2381.023737	444091.790609	38.634535
2384.009632	444900.668459	38.639552
2386.650557	445697.232363	38.644570
2389.087806	446493.346202	38.649588
2391.787468	447290.548797	38.654605
2394.530036	448079.722747	38.659623
2396.858014	448868.482906	38.664640
2399.208981	449658.625664	38.669658
2401.729983	450452.047360	38.674676
2404.154773	451246.871318	38.679693
2406.248550	452038.131083	38.684711
2408.842474	452835.241991	38.689728
2410.672308	453644.891615	38.694746
2413.096746	454446.014253	38.699764
2415.270045	455260.496470	38.704781
2417.929330	456070.717213	38.709799
2420.412122	456883.665800	38.714816
2422.295619	457710.687727	38.719834
2424.784234	458534.235736	38.724852
2426.766400	459360.869458	38.729869
2429.356197	460190.953982	38.734887
2431.538948	461018.293325	38.739904
2433.982887	461866.832478	38.744922
2436.586022	462705.300542	38.749940
2439.018576	463555.992520	38.754957
2441.454039	464411.751219	38.759975
2444.018482	465258.151702	38.764992
2446.098302	466125.720835	38.770010
2448.946769	466960.628232	38.775028
2450.980525	467840.710071	38.780045
2453.542992	468692.012648	38.785063
2456.068885	469557.126980	38.790080
2458.155710	470435.311463	38.795098
2460.667162	471309.795651	38.800116
2462.668123	472196.399955	38.805133
2464.413896	473085.178014	38.810151
2467.454164	473984.451524	38.815168
2469.667268	474899.632335	38.820186
2472.413830	475800.837713	38.825204
2474.951670	476697.236688	38.830221
2477.121110	477604.007720	38.835239
2480.246348	478492.087468	38.840256
2482.856090	479402.077187	38.845274
2485.487937	480299.090747	38.850292
2488.401989	481191.467134	38.855309
2491.142203	482051.464985	38.860327
2494.198787	482893.848298	38.865344
2496.696744	483745.071607	38.870362
2499.991458	484570.573742	38.875380
2502.456154	485404.710315	38.880397
2504.755379	486221.319856	38.885415
2507.658068	487047.025254	38.890432
2510.181976	487863.368382	38.895450
2512.918103	488689.024518	38.900468
2515.190680	489509.623286	38.905485
2517.473492	490342.192231	38.910503
2519.573585	491169.705818	38.915520
2521.436170	492012.055624	38.920538
2523.573588	492861.482067	38.925556
2525.973707	493711.073540	38.930573
2527.939196	494577.750000	38.935591
2530.378158	495449.901155	38.940608
2532.549225	496341.223209	38.945626
2534.583487	497235.447133	38.950644
2536.818238	498143.158031	38.955661
2538.812235	499062.966157	38.960679
2541.077587	499989.334591	38.965696
2543.120820	500937.527027	38.970714
2545.787372	501885.558302	38.975732
2547.894226	502835.647514	38.980749
2550.373573	503805.737467	38.985767
2552.786308	504776.385981	38.990784
2555.065076	505760.713224	38.995802
2557.858383	506746.858675	39.000820
2560.777799	507727.830297	39.005837
2563.349465	508731.586435	39.010855
2566.232605	509726.001663	39.015872
2568.470336	510738.156470	39.020890
2570.930711	511738.263524	39.025908
2573.514922	512753.354554	39.030925
2576.302359	513767.186032	39.035943
2579.295241	514773.811466	39.040960
2581.345510	515796.404741	39.045978
2584.086886	516822.994214	39.050996
2587.146574	517840.342046	39.056013
2590.338976	518853.922233	39.061031
2593.360952	519864.190039	39.066048
2596.090099	520878.369751	39.071066
2598.443248	521883.832390	39.076084
2601.583616	522894.532874	39.081101
2603.832264	523905.418566	39.086119
2607.142319	524904.976170	39.091136
2609.776980	525913.746611	39.096154
2612.708077	526910.616024	39.101172
2615.239950	527908.745243	39.106189
2617.351272	528914.933763	39.111207
2620.356013	529911.688545	39.116224
2622.461087	530919.200554	39.121242
2625.375389	531922.478070	39.126260
2627.918708	532922.327304	39.131277
2630.651583	533935.562479	39.136295
2633.310899	534907.726163	39.141312
2635.534465	535874.866616	39.146330
2638.048638	536853.112513	39.151348
2640.947382	537817.339405	39.156365
2643.300958	538794.070657	39.161383
2646.422073	539759.435585	39.166400
2649.364284	540732.612152	39.171418
2652.412824	541689.456758	39.176436
2655.547246	542636.765848	39.181453
2658.032586	543611.228804	39.186471
2660.819240	544569.932410	39.191488
2663.519547	545523.153727	39.196506
2665.924483	546479.376628	39.201524
2668.929240	547447.597842	39.206541
2670.979158	548418.980608	39.211559
2673.620750	549392.958157	39.216576
2675.905761	550376.578266	39.221594
2678.727570	551361.694091	39.226612
2681.616262	552351.451160	39.231629
2683.955520	553351.682668	39.236647
2686.433194	554343.323456	39.241664
2689.070083	555350.088852	39.246682
2691.423866	556352.405122	39.251700
2694.091241	557369.011338	39.256717
2696.813367	558392.563336	39.261735
2699.894777	559407.987529	39.266752
2702.599886	560438.667245	39.271770
2705.445843	561467.835533	39.276788
2708.070501	562498.768479	39.281805
2710.846986	563530.397280	39.286823
2713.652847	564549.285267	39.291840
2716.140435	565592.097052	39.296858
2718.956524	566622.468010	39.301876
2721.515033	567661.786208	39.306893
2723.798387	568711.809069	39.311911
2726.545818	569759.558002	39.316928
2729.098172	570829.236371	39.321946
2731.409705	571908.751725	39.326964
2734.011313	572984.863362	39.331981
2736.478827	574071.392395	39.336999
2739.027062	575165.338970	39.342016
2741.534059	576274.246625	39.347034
2743.681697	577378.903054	39.352052
2746.959197	578491.945138	39.357069
2749.348669	579620.435479	39.362087
2752.282724	580740.805647	39.367104
2754.559661	581875.376255	39.372122
2757.526482	583012.581377	39.377140
2760.568898	584140.642910	39.382157
2763.108459	585287.985205	39.387175
2765.936989	586433.865725	39.392192
2768.713550	587571.325874	39.397210
2771.939382	588720.077627	39.402228
2774.895201	589861.248258	39.407245
2777.627898	590996.084184	39.412263
2780.970876	592089.073025	39.417280
2784.238900	593175.661233	39.422298
2787.261846	594258.784628	39.427316
2790.386368	595317.798676	39.432333
2793.494312	596390.342054	39.437351
2796.508034	597443.071846	39.442368
2799.308224	598514.870739	39.447386
2801.882471	599584.055354	39.452404
2804.748661	600652.740442	39.457421
2806.987715	601739.604895	39.462439
2809.605705	602810.534123	39.467456
2812.063565	603912.221097	39.472474
2814.592190	605016.641823	39.477492
2816.969331	606120.180146	39.482509
2819.309809	607244.231505	39.487527
2822.081664	608368.196974	39.492544
2824.787544	609495.012572	39.497562
2827.188569	610630.620246	39.502580
2830.117700	611776.975248	39.507597
2832.640471	612939.934575	39.512615
2835.217889	614104.062425	39.517632
2837.861513	615279.805855	39.522650
2839.988515	616477.908933	39.527668
2842.552046	617678.605651	39.532685
2844.781704	618908.916949	39.537703
2847.340055	620137.133686	39.542720
2850.009355	621370.639011	39.547738
2852.918985	622628.994946	39.552756
2855.892679	623888.591461	39.557773
2858.078495	625154.518506	39.562791
2860.732931	626431.403575	39.567808
2863.706828	627724.811108	39.572826
2866.066463	629022.559891	39.577844
2869.010315	630335.028003	39.582861
2871.743330	631652.909647	39.587879
2874.823246	632979.601030	39.592896
2877.952297	634316.845923	39.597914
2881.201855	635643.019047	39.602932
2884.358342	636969.187795	39.607949
2887.089335	638297.503717	39.612967
2890.052339	639629.549089	39.617984
2893.571364	640964.568124	39.623002
2896.557889	642294.067254	39.628020
2900.002401	643615.734606	39.633037
2903.117136	644948.653323	39.638055
2905.859240	646261.767939	39.643072
2909.360515	647579.466011	39.648090
2912.196314	648906.324355	39.653108
2915.268752	650233.214820	39.658125
2917.494535	651547.367143	39.663143
2920.849220	652870.368605	39.668160
2923.709060	654203.837202	39.673178
2926.566717	655533.887814	39.678196
2929.712967	656857.184775	39.683213
2932.445545	658176.240100	39.688231
2935.258136	659465.580137	39.693248
2938.418621	660745.529802	39.698266
2941.180586	662035.332125	39.703284
2944.011648	663315.543996	39.708301
2947.098717	664607.184602	39.713319
2950.397021	665872.046882	39.718336
2953.679443	667155.895665	39.723354
2956.457016	668436.573069	39.728372
2959.190535	669711.862619	39.733389
2962.300299	671005.164307	39.738407
2964.826298	672286.604304	39.743424
2968.040767	673580.278421	39.748442
2970.463155	674883.849161	39.753460
2973.384740	676189.686306	39.758477
2976.280790	677515.120346	39.763495
2979.050248	678830.051518	39.768512
2982.022168	680151.714694	39.773530
2984.905827	681484.526770	39.778548
2987.760574	682827.081521	39.783565
2990.573980	684169.892128	39.788583
2993.511653	685511.986184	39.793600
2996.421058	686877.166532	39.798618
2999.624700	688233.751515	39.803636
3002.394843	689611.295672	39.808653
3005.322104	690984.581830	39.813671
3008.102364	692369.141038	39.818688
3011.329574	693748.100680	39.823706
3014.400867	695145.667815	39.828724
3017.348719	696549.728468	39.833741
3020.022325	697952.768718	39.838759
3022.802823	699371.031443	39.843776
3025.715298	700782.796291	39.848794
3028.496476	702210.657198	39.853812
3031.867574	703642.640953	39.858829
3034.997461	705072.694445	39.863847
3038.203979	706521.218679	39.868864
3041.815311	707959.128684	39.873882
3044.786763	709399.777387	39.878900
3048.175713	710821.349041	39.883917
3051.326931	712255.542019	39.888935
3054.493173	713687.608379	39.893952
3057.524821	715127.073640	39.898970
3060.562396	716573.958565	39.903988
3063.577771	718009.665882	39.909005
3066.354670	719447.342285	39.914023
3069.957458	720896.198391	39.919040
3073.178411	722324.597386	39.924058
3076.366140	723775.787185	39.929076
3079.565819	725216.488964	39.934093
3082.586715	726658.894538	39.939111
3085.658692	728107.063053	39.944128
3088.910763	729544.965615	39.949146
3091.866046	730989.774613	39.954164
3094.916848	732442.060289	39.959181
3097.888474	733868.526150	39.964199
3100.708506	735285.090160	39.969216
3104.150133	736680.027963	39.974234
3107.386443	738075.151063	39.979252
3110.254770	739469.697023	39.984269
3113.395976	740870.411578	39.989287
3116.181219	742274.784374	39.994304
3119.869880	743670.665980	39.999322
3122.793221	745070.915244	40.004340
3126.110195	746482.034026	40.009357
3129.343226	747873.890072	40.014375
3132.398963	749285.628040	40.019392
3135.369356	750691.605616	40.024410
3138.422198	752109.920562	40.029428
3141.437803	753523.203428	40.034445
3144.790219	754945.571078	40.039463
3147.847776	756383.819664	40.044480
3151.039363	757814.588061	40.049498
3153.720883	759255.949074	40.054516
3156.375570	760700.925956	40.059533
3159.419211	762160.068660	40.064551
3162.201232	763633.872398	40.069568
3165.442441	765115.812877	40.074586
3168.451499	766599.366166	40.079604
3171.441484	768094.667108	40.084621
3174.662325	769600.682115	40.089639
3177.714678	771101.112763	40.094656
3180.974263	772617.115295	40.099674
3184.079439	774143.339048	40.104692
3187.024613	775675.211575	40.109709
3190.373738	777193.783234	40.114727
3193.587600	778743.418588	40.119744
3196.747256	780277.226610	40.124762
3200.121026	781824.700666	40.129780
3203.241711	783372.521764	40.134797
3206.301694	784935.855622	40.139815
3208.999571	786499.447603	40.144832
3212.615297	788057.294493	40.149850
3216.176844	789625.685642	40.154868
3219.671349	791190.212237	40.159885
3222.996783	792758.778455	40.164903
3225.786983	794336.290567	40.169920
3229.089144	795905.183150	40.174938
3232.316121	797488.711805	40.179956
3235.046796	799073.969749	40.184973
3238.644141	800661.504533	40.189991
3241.763051	802263.134693	40.195008
3244.963146	803860.220639	40.200026
3248.079291	805464.672133	40.205044
3251.162805	807072.074961	40.210061
3254.378336	808670.621094	40.215079
3257.437438	810304.185951	40.220096
3260.752098	811934.722822	40.225114
3263.688126	813561.364095	40.230132
3267.084749	815197.099777	40.235149
3270.109952	816814.732648	40.240167
3273.238792	818412.729555	40.245184
3276.780583	819996.855518	40.250202
3280.129157	821577.171754	40.255220
3283.634476	823158.495778	40.260237
3287.292378	824736.390217	40.265255
3290.088734	826328.525233	40.270272
3293.311230	827909.674289	40.275290
3296.129154	829498.057713	40.280308
3299.034994	831111.506060	40.285325
3302.204267	832718.566093	40.290343
3305.394269	834338.703775	40.295360
3308.614588	835965.871954	40.300378
3311.602303	837600.887037	40.305396
3314.544306	839243.320470	40.310413
3318.215100	840896.728178	40.315431
3321.078580	842563.160773	40.320448
3324.760877	844221.625675	40.325466
3327.686676	845895.329014	40.330484
3330.617010	847583.155626	40.335501
3334.218974	849262.349685	40.340519
3337.438721	850965.331179	40.345536
3340.777937	852675.977307	40.350554
3343.924686	854402.096246	40.355572
3347.197091	856126.835913	40.360589
3350.879687	857849.371153	40.365607
3353.776370	859588.133954	40.370624
3357.473689	861323.258216	40.375642
3360.748051	863058.345478	40.380660
3364.178450	864799.882440	40.385677
3367.909740	866556.456007	40.390695
3371.147496	868305.047559	40.395712
3374.715733	870051.909526	40.400730
3378.358259	871817.211099	40.405748
3381.170125	873574.971153	40.410765
3384.338701	875337.272920	40.415783
3387.644792	877115.845042	40.420800
3391.156762	878888.044548	40.425818
3394.613225	880678.266383	40.430836
3397.803238	882457.939097	40.435853
3401.459292	884233.221287	40.440871
3404.933791	886031.831388	40.445888
3409.098366	887820.499217	40.450906
3412.230572	889604.831368	40.455924
3415.722793	891395.682132	40.460941
3419.188093	893182.119189	40.465959
3422.655749	894980.812138	40.470976
3426.280558	896777.847372	40.475994
3429.488257	898572.551777	40.481012
3433.106483	900355.733710	40.486029
3436.721976	902152.690135	40.491047
3439.881888	903952.032774	40.496064
3443.437494	905742.453988	40.501082
3446.755893	907550.030616	40.506100
3449.496006	909357.499283	40.511117
3452.897660	911141.132934	40.516122
3455.915199	912907.017842	40.521127
3459.309761	914594.667707	40.526132
3462.631424	916221.747527	40.531136
3465.752697	917786.022343	40.536141
3469.484336	919257.297133	40.541146
3472.532903	920677.028669	40.546151
3475.454572	922012.567783	40.551156
3478.495080	923271.912644	40.556160
3480.975157	924464.650166	40.561165
3483.804649	925564.053822	40.566170
3486.117754	926604.047340	40.571175
3488.235555	927577.983011	40.576180
3490.702815	928472.263384	40.581184
3493.136918	929310.133585	40.586189
3495.447356	930070.611135	40.591194
3497.281379	930771.259539	40.596199
3499.355927	931394.608081	40.601204
3501.495475	931967.968884	40.606208
3503.241422	932490.860707	40.611213
3504.915449	932951.537771	40.616218
3506.365164	933367.120126	40.621223
3508.129056	933722.464644	40.626228
3509.190864	934025.239551	40.631232
3510.679136	934286.868290	40.636237
3512.275849	934493.886360	40.641242
3513.607761	934667.370110	40.646247
3514.917586	934793.469543	40.651252
3516.315954	934897.394688	40.656256
3516.831653	934947.949108	40.661261
3518.192814	934958.650864	40.666266
3519.172797	934949.084097	40.671271
3519.765052	934905.917784	40.676276
3520.357536	934837.525424	40.681280
3521.215620	934740.599553	40.686285
3522.185793	934614.301526	40.691290
3522.775202	934473.964960	40.696295
3523.442129	934296.392586	40.701300
3523.957681	934108.191989	40.706304
3524.448076	933903.104884	40.711309
3525.232829	933665.533038	40.716314
3525.850054	933412.340655	40.721319
3526.080137	933146.249460	40.726324
3526.543311	932852.758918	40.731328
3526.810452	932562.931840	40.736333
3527.473209	932252.869218	40.741338
3527.434891	931934.750745	40.746343
3527.873673	931599.640188	40.751348
3527.991831	931256.596707	40.756352
3528.345050	930898.228897	40.761357
3528.485900	930534.881368	40.766362
3528.843561	930169.455858	40.771367
3529.404447	929783.904945	40.776372
3529.535730	929397.727200	40.781376
3529.827936	928992.001491	40.786381
3529.993069	928589.243334	40.791386
3529.905825	928170.747733	40.796391
3530.386007	927749.337018	40.801396
3530.424003	927317.882946	40.806400
3530.050098	926899.912530	40.811405
3530.854141	926451.735240	40.816410
3530.664996	926019.350108	40.821415
3530.830834	925570.343003	40.826420
3530.826901	925115.657712	40.831424
3530.756027	924671.708310	40.836429
3531.413952	924196.747036	40.841434
3531.326392	923747.630070	40.846439
3531.319516	923274.815068	40.851444
3531.514186	922803.077562	40.856448
3531.479350	922332.683749	40.861453
3531.480170	921844.935639	40.866458
3531.591412	921369.625079	40.871463
3532.187430	920881.399535	40.876468
3532.152336	920393.718364	40.881472
3532.008518	919905.434527	40.886477
3532.407687	919403.450511	40.891482
3532.055302	918906.069671	40.896487
3532.293684	918404.116493	40.901492
3532.596419	917897.968301	40.906496
3532.377227	917403.409455	40.911501
3532.446496	916884.311720	40.916506
3532.413534	916384.238817	40.921511
3532.665286	915862.028558	40.926516
3532.725210	915354.144511	40.931520
3532.556550	914838.357582	40.936525
3532.849473	914308.770713	40.941530
3532.633489	913797.900209	40.946535
3532.808003	913272.566213	40.951540
3532.848006	912740.848126	40.956544
3532.636724	912223.184128	40.961549
3532.767815	911689.325634	40.966554
3532.486304	911171.670625	40.971559
3532.866348	910641.039510	40.976564
3533.055564	910120.603664	40.981568
3532.557808	909581.926110	40.986573
3532.962043	909050.655615	40.991578
3533.057660	908509.651633	40.996583
3532.787776	907980.610010	41.001588
3532.899897	907443.740138	41.006592
3532.645190	906906.109443	41.011597
3532.975631	906368.133786	41.016602
3532.677915	905831.177454	41.021607
3532.745208	905287.259440	41.026612
3533.130936	904746.706041	41.031616
3532.878661	904205.726685	41.036621
3533.047851	903655.072223	41.041626
3533.152665	903115.855412	41.046631
3532.975424	902571.520686	41.051636
3533.066007	902023.420210	41.056640
3532.689538	901484.996496	41.061645
3533.008697	900927.774361	41.066650
3532.914790	900388.135199	41.071655
3532.906276	899840.899694	41.076660
3533.102577	899280.928377	41.081664
3532.827894	898740.196147	41.086669
3532.990955	898184.755957	41.091674
3532.664181	897628.668571	41.096679
3532.703941	897084.246943	41.101684
3532.698739	896533.308740	41.106688
3532.800954	895978.724179	41.111693
3532.797620	895431.832192	41.116698
3532.656663	894872.156869	41.121703
3533.060433	894323.252557	41.126708
3532.983297	893757.561861	41.131712
3533.087070	893206.184753	41.136717
3533.327860	892652.797611	41.141722
3533.246102	892088.874868	41.146727
3533.451968	891521.946873	41.151732
3533.247771	890954.645793	41.156736
3532.798265	890395.646202	41.161741
3533.018135	889819.940807	41.166746
3532.844695	889263.007671	41.171751
3532.825824	888696.127977	41.176756
3532.975288	888140.675050	41.181760
3532.758927	887589.197385	41.186765
3532.988972	887022.303481	41.191770
3533.085853	886448.312732	41.196775
3532.712495	885888.861078	41.201780
3532.712864	885321.645538	41.206784
3532.683161	884764.639389	41.211789
3532.706583	884187.048592	41.216794
3532.916202	883625.245417	41.221799
3532.857421	883061.884474	41.226804
3532.810593	882490.236241	41.231808
3532.542134	881926.704092	41.236813
3532.718729	881353.065918	41.241818
3532.923450	880793.120312	41.246823
3532.752624	880225.048141	41.251828
3532.813134	879659.690602	41.256832
3532.554376	879094.235959	41.261837
3532.524824	878508.533144	41.266842
3532.826459	877950.042581	41.271847
3532.969798	877375.728732	41.276852
3532.956851	876800.222265	41.281856
3532.713448	876239.335753	41.286861
3533.035724	875662.012762	41.291866
3533.180765	875092.322683	41.296871
3533.102487	874507.780493	41.301876
3532.770933	873922.350896	41.306880
3532.387625	873339.393634	41.311885
3533.093241	872759.684702	41.316890
3532.708617	872191.163177	41.321895
3532.524512	871612.463919	41.326900
3532.526976	871027.370157	41.331904
3532.221213	870465.073098	41.336909
3532.544734	869885.536861	41.341914
3532.251118	869311.387193	41.346919
3532.462248	868740.104830	41.351924
3532.430734	868162.305835	41.356928
3532.199897	867594.192521	41.361933
3532.380000	867017.217543	41.366938
3532.627238	866435.417962	41.371943
3532.282314	865866.674853	41.376948
3532.470910	865286.327561	41.381952
3532.059690	864724.091256	41.386957
3532.233294	864139.945337	41.391962
3532.193737	863564.521807	41.396967
3532.372370	862987.160318	41.401972
3532.423905	862406.947750	41.406976
3531.818971	861835.439530	41.411981
3532.458474	861259.972194	41.416986
3532.295551	860683.906926	41.421991
3532.103739	860111.679728	41.426996
3531.694077	859525.827164	41.432000
3532.109173	858970.885844	41.437005
3532.144886	858392.722505	41.442010
3532.354036	857812.335636	41.447015
3532.486838	857237.643872	41.452020
3532.355388	856653.509888	41.457024
3532.019661	856068.576934	41.462029
3532.111619	855492.269339	41.467034
3532.534999	854920.520378	41.472039
3532.304339	854337.447243	41.477044
3532.561108	853739.251919	41.482048
3532.439619	853163.929967	41.487053
3532.453959	852566.440593	41.492058
3532.647143	851985.699992	41.497063
3532.755276	851397.327306	41.502068
3532.826042	850796.834502	41.507072
3532.419353	850208.144633	41.512077
3532.396856	849614.757285	41.517082
3532.615312	849030.424960	41.522087
3532.292392	848436.586881	41.527092
3531.920634	847845.719540	41.532096
3531.908836	847260.676028	41.537101
3531.889168	846667.591564	41.542106
3531.920598	846091.684856	41.547111
3531.973108	845515.916370	41.552116
3532.188837	844922.626248	41.557120
3531.854867	844337.364239	41.562125
3532.042616	843746.208852	41.567130
3531.829374	843166.566863	41.572135
3531.892052	842582.925521	41.577140
3532.243691	841998.108498	41.582144
3531.946121	841404.184085	41.587149
3532.196585	840809.330263	41.592154
3531.639096	840225.284254	41.597159
3531.686645	839638.058047	41.602164
3531.419754	839050.684825	41.607168
3531.285812	838474.304714	41.612173
3531.565105	837885.852695	41.617178
3531.613676	837301.336516	41.622183
3531.644451	836719.891702	41.627188
3531.751222	836142.771562	41.632192
3531.728692	835556.009788	41.637197
3531.979132	834957.924909	41.642202
3531.636584	834381.112786	41.647207
3531.667932	833792.911416	41.652212
3531.526871	833202.782062	41.657216
3531.495813	832620.438442	41.662221
3531.510436	832033.689642	41.667226
3531.716584	831457.546442	41.672231
3531.503402	830867.703476	41.677236
3531.855301	830273.657283	41.682240
3531.736548	829689.013007	41.687245
3531.658075	829099.962404	41.692250
3532.034089	828510.292237	41.697255
3531.946782	827916.300154	41.702260
3532.022984	827306.300088	41.707264
3531.518537	826718.864808	41.712269
3531.562216	826123.123184	41.717274
3531.879947	825539.936475	41.722279
3531.367484	824929.961028	41.727284
3531.697222	824336.108916	41.732288
3531.504859	823747.473202	41.737293
3531.829745	823150.826131	41.742298
3531.977273	822557.137236	41.747303
3531.836940	821959.385800	41.752308
3531.493231	821361.468072	41.757312
3531.052535	820770.749938	41.762317
3531.182812	820175.382130	41.767322
3531.148042	819585.271059	41.772327
3531.032217	818990.327583	41.777332
3531.169441	818404.728681	41.782336
3531.190246	817819.440378	41.787341
3531.173312	817224.566135	41.792346
3531.050914	816640.568334	41.797351
3531.161859	816041.113631	41.802356
3531.174794	815453.024762	41.807360
3530.871768	814863.861203	41.812365
3530.938235	814272.233046	41.817370
3530.965764	813685.601355	41.822375
3530.781197	813113.005196	41.827380
3531.207810	812514.746872	41.832384
3530.938189	811932.908683	41.837389
3531.049981	811341.014080	41.842394
3530.748148	810754.965977	41.847399
3530.855636	810163.703236	41.852404
3530.966990	809570.183785	41.857408
3530.822846	808991.009054	41.862413
3530.939655	808394.789144	41.867418
3531.095334	807808.407251	41.872423
3530.663574	807221.878931	41.877428
3530.816102	806626.526437	41.882432
3530.630905	806051.959045	41.887437
3530.708765	805455.193556	41.892442
3530.802194	804871.166571	41.897447
3530.687904	804276.879650	41.902452
3530.916974	803685.669070	41.907456
3530.347766	803100.574317	41.912461
3530.606293	802508.913877	41.917466
3530.702745	801927.184784	41.922471
3530.878115	801334.211335	41.927476
3530.904174	800748.520155	41.932480
3530.644224	800155.666594	41.937485
3530.673973	799554.569485	41.942490
3530.611264	798973.451911	41.947495
3530.437623	798378.125160	41.952500
3530.861115	797783.283133	41.957504
3530.619951	797194.048610	41.962509
3530.512302	796606.409824	41.967514
3530.800491	796008.101571	41.972519
3530.239017	795417.544042	41.977524
3530.670356	794827.503268	41.982528
3530.643764	794241.418156	41.987533
3530.896553	793642.421958	41.992538
3531.122318	793050.007677	41.997543
3530.114332	792458.883304	42.002548
3530.562222	791862.746058	42.007552
3529.895284	791271.316044	42.012557
3529.953670	790687.718552	42.017562
3530.073656	790096.202732	42.022567
3530.006686	789514.690785	42.027572
3530.171113	788934.712686	42.032576
3530.038429	788356.555644	42.037581
3530.308723	787759.511992	42.042586
3530.529229	787174.417116	42.047591
3530.527878	786587.739191	42.052596
3530.585172	785977.656578	42.057600
3530.031053	785390.728450	42.062605
3530.057894	784804.537601	42.067610
3530.071441	784216.236020	42.072615
3530.065332	783626.955161	42.077620
3530.315867	783028.436242	42.082624
3530.338295	782447.953223	42.087629
3529.807687	781851.928068	42.092634
3530.220794	781261.692559	42.097639
3529.737298	780676.431105	42.102644
3530.166375	780079.996776	42.107648
3529.728914	779494.041068	42.112653
3529.715500	778901.766357	42.117658
3529.922920	778326.035844	42.122663
3529.971659	777735.475470	42.127668
3529.852934	777147.651324	42.132672
3529.678182	776556.688588	42.137677
3529.659004	775968.899621	42.142682
3529.408197	775389.765830	42.147687
3529.024722	774809.082605	42.152692
3529.208819	774218.951717	42.157696
3529.173293	773650.375196	42.162701
3529.097398	773074.572602	42.167706
3529.168035	772499.930743	42.172711
3529.054768	771928.722425	42.177716
3529.017599	771351.842206	42.182720
3528.805020	770785.486866	42.187725
3529.181218	770210.268897	42.192730
3529.013019	769636.231965	42.197735
3528.899600	769061.007917	42.202740
3529.299854	768488.607501	42.207744
3529.033567	767908.737888	42.212749
3528.905672	767332.544244	42.217754
3528.741228	766760.353040	42.222759
3528.787054	766189.609646	42.227764
3529.431554	765613.643599	42.232768
3528.633439	765044.730807	42.237773
3528.768520	764461.467503	42.242778
3529.352168	763883.455664	42.247783
3528.915831	763315.828283	42.252788
3528.727234	762735.739556	42.257792
3528.502840	762161.134814	42.262797
3528.699200	761594.649720	42.267802
3528.899337	761031.277625	42.272807
3528.764565	760448.833017	42.277812
3528.586249	759875.426706	42.282816
3528.369266	759303.019315	42.287821
3528.444085	758727.953407	42.292826
3528.512854	758159.110573	42.297831
3528.284644	757595.209749	42.302836
3528.736843	757023.946592	42.307840
3528.472214	756455.674357	42.312845
3528.681808	755882.886397	42.317850
3528.660916	755321.298320	42.322855
3528.327248	754749.653062	42.327860
3528.609002	754174.207091	42.332864
3528.717079	753608.966262	42.337869
3528.383269	753029.688698	42.342874
3528.468411	752467.132222	42.347879
3528.343902	751895.336752	42.352884
3528.661992	751324.065119	42.357888
3528.141268	750752.153501	42.362893
3528.263048	750173.027203	42.367898
3528.231331	749610.182979	42.372903
3528.211138	749045.912699	42.377908
3528.338114	748471.350503	42.382912
3528.001346	747908.681525	42.387917
3528.240169	747337.424960	42.392922
3528.096664	746767.920995	42.397927
3528.036266	746205.674342	42.402932
3528.090984	745640.797739	42.407936
3527.849511	745072.817263	42.412941
3528.082046	744501.600801	42.417946
3528.004000	743947.448263	42.422951
3527.727435	743387.160885	42.427956
3527.870994	742808.421333	42.432960
3527.860027	742252.110631	42.437965
3527.826003	741696.703882	42.442970
3528.003544	741126.684804	42.447975
3527.681613	740559.231670	42.452980
3527.555597	739999.567253	42.457984
3527.485661	739436.737870	42.462989
3527.549528	738878.296974	42.467994
3527.879533	738323.332626	42.472999
3527.705545	737762.083762	42.478004
3527.841830	737183.576094	42.483008
3527.698768	736626.842513	42.488013
3527.472767	736065.878603	42.493018
3527.685401	735508.461914	42.498023
3527.523110	734949.783735	42.503028
3527.543692	734395.093276	42.508032
3527.319492	733832.388628	42.513037
3527.446236	733271.613841	42.518042
3527.347006	732719.154113	42.523047
3527.127721	732153.262040	42.528052
3527.177128	731607.581277	42.533056
3527.197159	731059.294162	42.538061
3527.287065	730502.639936	42.543066
3527.134077	729950.494689	42.548071
3526.879071	729396.199891	42.553076
3527.547627	728834.776460	42.558080
3527.253603	728283.977848	42.563085
3527.003527	727723.525860	42.568090
3526.804390	727167.038641	42.573095
3526.694877	726626.250299	42.578100
3526.874332	726078.540458	42.583104
3527.212065	725530.519161	42.588109
3526.945242	724973.200320	42.593114
3526.804882	724423.204687	42.598119
3526.992113	723873.859513	42.603124
3526.800167	723325.136983	42.608128
3526.809844	722779.465588	42.613133
3526.696193	722222.379878	42.618138
3526.664622	721665.589464	42.623143
3526.449043	721131.743074	42.628148
3527.014485	720579.635241	42.633152
3526.511759	720044.726708	42.638157
3526.498194	719487.489142	42.643162
3526.763109	718941.173702	42.648167
3526.649888	718399.151189	42.653172
3526.687763	717848.389687	42.658176
3526.310701	717314.821160	42.663181
3526.315930	716760.521990	42.668186
3526.661169	716222.396027	42.673191
3526.397531	715677.296086	42.678196
3526.636145	715120.120339	42.683200
3526.291331	714586.124214	42.688205
3526.238798	714044.751497	42.693210
3526.415407	713498.095376	42.698215
3526.271513	712954.137803	42.703220
3526.376388	712412.782156	42.708224
3525.726109	711874.746236	42.713229
3526.048331	711332.887313	42.718234
3526.300383	710800.832354	42.723239
3525.992961	710269.087685	42.728244
3526.060195	709724.241164	42.733248
3526.229791	709192.794409	42.738253
3526.180180	708634.247308	42.743258
3525.975718	708097.335425	42.748263
3526.128261	707573.733880	42.753268
3526.288913	707026.067566	42.758272
3525.961117	706478.747523	42.763277
3526.167329	705943.517180	42.768282
3526.267852	705401.567277	42.773287
3526.016240	704866.745269	42.778292
3526.263053	704325.944199	42.783296
3526.117315	703792.328721	42.788301
3526.250209	703246.810414	42.793306
3526.235962	702706.995579	42.798311
3525.670777	702155.566410	42.803316
3525.975221	701621.342623	42.808321
3525.707146	701088.574882	42.813325
3525.541564	700545.123555	42.818330
3525.913798	700018.441699	42.823335
3525.774109	699478.944420	42.828340
3525.819449	698941.767681	42.833345
3525.288112	698414.646255	42.838349
3525.420307	697871.176254	42.843354
3525.444596	697345.287263	42.848359
3525.310914	696811.092123	42.853364
3525.613505	696281.313891	42.858369
3525.403977	695754.076975	42.863373
3525.510658	695219.495516	42.868378
3525.620662	694692.637718	42.873383
3525.187681	694169.620278	42.878388
3525.526818	693637.140939	42.883393
3525.296800	693115.767010	42.888397
3524.997697	692581.294196	42.893402
3525.202890	692056.451522	42.898407
3525.033752	691533.133957	42.903412
3525.507521	691014.550641	42.908417
3525.217904	690490.247249	42.913421
3525.086696	689951.011184	42.918426
3525.138927	689424.348154	42.923431
3524.905903	688906.559111	42.928436
3525.065982	688380.065017	42.933441
3525.296726	687864.276170	42.938445
3524.984135	687333.571787	42.943450
3524.674344	686814.331562	42.948455
3524.458762	686297.931911	42.953460
3524.897294	685769.595122	42.958465
3524.753920	685261.236624	42.963469
3524.776782	684742.766140	42.968474
3524.999923	684222.141012	42.973479
3524.700298	683706.155292	42.978484
3524.617476	683185.224213	42.983489
3524.986870	682681.164050	42.988493
3524.588965	682164.261195	42.993498
3524.559025	681638.452602	42.998503
3524.350452	681130.421829	43.003508
3524.850413	680602.570863	43.008513
3524.588481	680097.529641	43.013517
3524.676698	679565.754814	43.018522
3524.852091	679053.359616	43.023527
3524.330033	678533.533429	43.028532
3524.680712	678027.078298	43.033537
3524.496214	677506.787829	43.038541
3524.136079	676998.105974	43.043546
3524.469788	676481.704666	43.048551
3524.222849	675974.242544	43.053556
3524.654600	675450.940988	43.058561
3524.368501	674948.511858	43.063565
3524.251471	674439.847362	43.068570
3524.475796	673930.847597	43.073575
3524.085424	673414.997381	43.078580
3524.265695	672904.703146	43.083585
3524.299116	672399.041623	43.088589
3524.646795	671892.551413	43.093594
3524.133184	671373.369507	43.098599
3523.977979	670865.962537	43.103604
3524.041282	670351.012587	43.108609
3523.879849	669848.138398	43.113613
3523.740215	669340.696333	43.118618
3523.716608	668834.104691	43.123623
3523.782122	668331.509785	43.128628
3523.744656	667825.963511	43.133633
3523.991015	667328.071807	43.138637
3523.699997	666832.140905	43.143642
3523.550961	666327.830514	43.148647
3523.575294	665839.873931	43.153652
3523.604048	665321.014934	43.158657
3523.634791	664832.506844	43.163661
3523.678271	664331.898994	43.168666
3523.577355	663843.662132	43.173671
3523.432702	663343.184319	43.178676
3523.429179	662845.101106	43.183681
3523.751617	662350.030010	43.188685
3523.431993	661856.240622	43.193690
3523.359007	661354.149917	43.198695
3523.500613	660854.691273	43.203700
3523.431232	660364.475662	43.208705
3523.263631	659863.122035	43.213709
3523.476573	659372.358730	43.218714
3523.686367	658861.505257	43.223719
3523.201482	658381.293085	43.228724
3523.084904	657885.069782	43.233729
3522.948787	657396.862042	43.238733
3523.522874	656898.972878	43.243738
3523.854416	656416.277730	43.248743
3523.440284	655925.697214	43.253748
3523.865141	655425.261907	43.258753
3523.649321	654921.414945	43.263757
3523.464447	654417.786498	43.268762
3523.677283	653912.466226	43.273767
3523.286919	653427.100251	43.278772
3523.387386	652926.193431	43.283777
3523.427361	652434.511857	43.288781
3523.634012	651933.986075	43.293786
3523.514697	651436.687596	43.298791
3523.443315	650942.653013	43.303796
3523.511710	650434.082144	43.308801
3523.280470	649939.875044	43.313805
3522.999921	649445.801681	43.318810
3523.444485	648943.635494	43.323815
3523.591347	648453.886896	43.328820
3523.047595	647961.833603	43.333825
3523.271976	647476.970947	43.338829
3523.031614	646970.424909	43.343834
3523.416899	646471.393066	43.348839
3522.874503	645991.687216	43.353844
3522.833443	645491.629907	43.358849
3522.685923	645013.859291	43.363853
3522.634136	644514.355117	43.368858
3522.714677	644039.398684	43.373863
3522.653403	643553.945771	43.378868
3522.599605	643057.819425	43.383873
3522.563234	642589.914182	43.388877
3522.392310	642100.510598	43.393882
3522.642129	641617.011832	43.398887
3522.419660	641141.271373	43.403892
3522.501478	640651.954990	43.408897
3522.288500	640178.518300	43.413901
3522.321947	639707.868236	43.418906
3522.569834	639228.607606	43.423911
3522.399887	638751.796657	43.428916
3522.476870	638267.518697	43.433921
3521.964721	637788.470607	43.438925
3521.943831	637316.419575	43.443930
3522.433659	636851.313258	43.448935
3522.058943	636369.124160	43.453940
3522.026011	635894.058477	43.458945
3522.318296	635415.563305	43.463949
3522.069252	634951.648402	43.468954
3521.926396	634487.444432	43.473959
3521.613864	634011.789800	43.478964
3522.050013	633537.737026	43.483969
3521.858294	633078.882955	43.488973
3521.875448	632611.014883	43.493978
3521.836543	632136.829398	43.498983
3521.716520	631670.744364	43.503988
3521.573667	631197.384897	43.508993
3521.884297	630737.541462	43.513997
3521.781990	630272.091984	43.519002
3521.555391	629801.987636	43.524007
3521.211236	629339.591777	43.529012
3521.292293	628876.302021	43.534017
3521.398857	628423.100808	43.539021
3520.844663	627965.937494	43.544026
3521.366399	627511.024153	43.549031
3521.220341	627058.558683	43.554036
3521.295657	626601.679677	43.559041
3521.573688	626147.400458	43.564045
3521.078055	625695.387302	43.569050
3521.131982	625241.808800	43.574055
3521.084144	624795.891025	43.579060
3521.097177	624342.131030	43.584065
3521.176836	623889.141799	43.589069
3521.045106	623427.403931	43.594074
3521.342913	622969.980867	43.599079
3520.899573	622528.694685	43.604084
3520.474476	622074.162124	43.609089
3520.904548	621634.493578	43.614093
3520.665940	621191.113717	43.619098
3520.917594	620733.954238	43.624103
3520.610316	620304.678332	43.629108
3521.045087	619853.963857	43.634113
3520.789258	619416.075889	43.639117
3520.661827	618965.169926	43.644122
3520.829171	618516.700513	43.649127
3520.715106	618086.101169	43.654132
3520.828324	617645.723549	43.659137
3520.721658	617203.260748	43.664141
3520.708549	616753.797394	43.669146
3520.709079	616307.871898	43.674151
3520.358652	615873.015427	43.679156
3520.474585	615431.796352	43.684161
3520.548985	614998.887874	43.689165
3520.229779	614549.436563	43.694170
3520.441249	614113.261527	43.699175
3520.299569	613681.340778	43.704180
3520.670637	613239.488961	43.709185
3520.434088	612806.748041	43.714189
3520.414736	612368.387600	43.719194
3520.227272	611937.810499	43.724199
3520.053043	611515.638571	43.729204
3520.312204	611065.094470	43.734209
3520.455219	610638.773288	43.739213
3519.884631	610201.625024	43.744218
3520.150151	609772.842636	43.749223
3519.615948	609347.289844	43.754228
3519.754965	608916.891314	43.759233
3519.948403	608498.554853	43.764237
3519.980083	608068.894446	43.769242
3520.029299	607641.772820	43.774247
3519.671649	607226.392396	43.779252
3519.985422	606798.742134	43.784257
3519.835407	606375.870505	43.789261
3519.606109	605944.919427	43.794266
3519.683098	605527.395482	43.799271
3519.370893	605114.137054	43.804276
3519.715466	604691.820423	43.809281
3519.815815	604272.590511	43.814285
3519.683852	603851.478034	43.819290
3519.775530	603419.222061	43.824295
3519.500624	603013.558347	43.829300
3519.574190	602590.758358	43.834305
3519.291781	602174.878873	43.839309
3519.236511	601764.466055	43.844314
3519.234806	601344.192363	43.849319
3519.321261	600938.493703	43.854324
3519.312687	600519.797083	43.859329
3519.214844	600117.313203	43.864333
3519.266528	599704.449337	43.869338
3519.329228	599288.305938	43.874343
3519.364207	598884.400974	43.879348
3519.243248	598465.598698	43.884353
3519.162974	598052.196261	43.889357
3518.712623	597650.740834	43.894362
3518.964668	597240.415614	43.899367
3519.012521	596839.901415	43.904372
3518.903426	596425.692824	43.909377
3518.706244	596019.367822	43.914381
3518.703473	595626.553167	43.919386
3518.642557	595219.474040	43.924391
3518.505775	594820.729737	43.929396
3519.013312	594425.879346	43.934401
3518.928837	594026.044452	43.939405
3518.566153	593628.804763	43.944410
3518.659964	593221.780468	43.949415
3518.475415	592831.313869	43.954420
3518.589518	592437.367870	43.959425
3518.206133	592039.776697	43.964429
3518.229064	591651.194516	43.969434
3518.461094	591245.685779	43.974439
3518.502086	590867.020766	43.979444
3518.640829	590460.596862	43.984449
3518.834658	590067.512790	43.989453
3518.751812	589683.204545	43.994458
3518.802374	589274.996769	43.999463
3518.430111	588881.819439	44.004468
3518.332817	588483.105589	44.009473
3518.337677	588093.455463	44.014477
3518.217592	587703.110504	44.019482
3518.480307	587308.014299	44.024487
3518.014260	586917.300802	44.029492
3517.984439	586533.434915	44.034497
3517.683869	586151.010097	44.039501
3517.739083	585767.808798	44.044506
3517.874377	585390.160167	44.049511
3518.020785	585007.773503	44.054516
3518.427577	584621.007892	44.059521
3518.216615	584237.552141	44.064525
3518.244488	583853.591091	44.069530
3518.537760	583465.501096	44.074535
3517.922965	583084.993191	44.079540
3518.040189	582688.614427	44.084545
3517.881944	582310.970167	44.089549
3517.724915	581923.963509	44.094554
3518.065534	581535.753597	44.099559
3517.888339	581164.914208	44.104564
3517.844432	580784.739736	44.109569
3517.681032	580408.043015	44.114573
3517.553589	580032.786672	44.119578
3517.609964	579648.487215	44.124583
3517.467694	579274.115269	44.129588
3517.657853	578900.982550	44.134593
3517.623895	578531.245911	44.139597
3517.509095	578153.516380	44.144602
3517.641296	577785.790796	44.149607
3517.234527	577417.140497	44.154612
3517.436329	577038.467910	44.159617
3517.209652	576674.592730	44.164621
3517.656368	576303.198634	44.169626
3517.709818	575933.470051	44.174631
3517.210372	575573.783751	44.179636
3517.067808	575202.155607	44.184641
3516.898784	574827.452582	44.189645
3517.252520	574472.015252	44.194650
3516.951427	574108.731711	44.199655
3517.132775	573749.932977	44.204660
3517.494118	573383.949768	44.209665
3517.134650	573019.185719	44.214669
3517.260644	572657.598277	44.219674
3517.125795	572289.001501	44.224679
3517.280976	571934.532389	44.229684
3517.106458	571565.216840	44.234689
3516.916041	571203.641687	44.239693
3516.891920	570846.807839	44.244698
3517.069512	570479.312450	44.249703
3516.431807	570125.733051	44.254708
3516.857010	569762.401407	44.259713
3516.714348	569408.918792	44.264717
3516.397452	569056.512885	44.269722
3516.748903	568694.069125	44.274727
3516.462805	568342.745352	44.279732
3516.465170	568001.377836	44.284737
3516.379908	567650.202022	44.289741
3516.327178	567308.926074	44.294746
3516.427796	566943.606651	44.299751
3516.251027	566618.590619	44.304756
3516.386505	566265.527171	44.309761
3516.388429	565916.000326	44.314765
3516.237451	565581.993905	44.319770
3516.453854	565238.100116	44.324775
3516.153180	564889.905885	44.329780
3516.556835	564543.847355	44.334785
3516.435588	564203.708902	44.339789
3516.672188	563860.932879	44.344794
3516.239243	563512.371730	44.349799
3516.122330	563176.786975	44.354804
3516.193252	562822.130034	44.359809
3516.016302	562477.122421	44.364813
3515.930058	562142.160260	44.369818
3516.133630	561811.168141	44.374823
3515.741549	561472.313557	44.379828
3515.935740	561133.954333	44.384833
3515.614681	560800.961663	44.389837
3515.702302	560468.746811	44.394842
3516.050027	560126.004638	44.399847
3515.708751	559811.219914	44.404852
3516.308843	559465.748376	44.409857
3515.778001	559129.828191	44.414861
3515.647966	558796.147710	44.419866
3515.932366	558469.237598	44.424871
3515.507732	558141.130939	44.429876
3515.677436	557808.482359	44.434881
3515.742010	557480.124668	44.439885
3515.349163	557144.080028	44.444890
3515.904763	556823.177655	44.449895
3515.353332	556509.961963	44.454900
3515.349397	556174.884193	44.459905
3515.626847	555850.328581	44.464909
3515.287517	555524.107221	44.469914
3515.431925	555211.800062	44.474919
3515.402820	554883.142350	44.479924
3515.285733	554562.552271	44.484929
3515.493221	554243.612030	44.489933
3515.223830	553922.276914	44.494938
3515.313291	553593.819217	44.499943
3514.979383	553282.606764	44.504948
3514.947866	552957.277974	44.509953
3515.228561	552641.864546	44.514957
3515.002109	552327.739630	44.519962
3515.144382	552010.168386	44.524967
3514.599429	551699.912786	44.529972
3514.780935	551389.929157	44.534977
3515.119211	551078.500677	44.539981
3514.971831	550764.577891	44.544986
3514.821735	550448.884487	44.549991
3514.686446	550140.186237	44.554996
3514.476352	549830.385013	44.560001
3514.834396	549528.896217	44.565005
3514.743559	549226.419009	44.570010
3514.810912	548914.785620	44.575015
3515.178934	548610.603606	44.580020
3515.198513	548299.417951	44.585025
3514.919549	547988.679421	44.590029
3514.948759	547683.829003	44.595034
3514.602705	547368.148175	44.600039
3514.377900	547068.216834	44.605044
3514.385299	546758.157645	44.610049
3514.750044	546455.995145	44.615053
3514.147338	546164.274938	44.620058
3514.636659	545862.027737	44.625063
3514.690106	545558.386374	44.630068
3514.897051	545264.139507	44.635073
3514.904207	544957.720102	44.640077
3514.675161	544654.409620	44.645082
3514.606131	544341.788436	44.650087
3514.478400	544051.404660	44.655092
3514.395754	543746.335117	44.660097
3514.599356	543439.495718	44.665101
3514.422062	543139.521492	44.670106
3514.701819	542837.950098	44.675111
3514.585740	542542.339340	44.680116
3514.691271	542236.952520	44.685121
3514.732885	541933.586980	44.690125
3514.475631	541639.342737	44.695130
3514.632485	541328.783808	44.700135
3514.272827	541041.906999	44.705140
3514.327824	540738.210744	44.710145
3514.213918	540442.908348	44.715149
3513.980064	540148.528017	44.720154
3514.117513	539858.869301	44.725159
3514.017082	539574.540856	44.730164
3514.134445	539268.885793	44.735169
3513.955415	538982.995370	44.740173
3513.583348	538702.831557	44.745178
3513.634190	538411.644862	44.750183
3513.542571	538141.106238	44.755188
3513.662844	537853.931398	44.760193
3513.888929	537573.189192	44.765197
3513.319167	537285.868490	44.770202
3513.517906	537010.920744	44.775207
3513.635023	536732.450527	44.780212
3513.713801	536458.773734	44.785217
3513.726838	536167.648492	44.790221
3513.389507	535898.622640	44.795226
3513.554820	535618.407290	44.800231
3513.533717	535345.987479	44.805236
3513.722332	535064.798800	44.810241
3513.684848	534793.329855	44.815245
3513.488149	534517.544083	44.820250
3513.542849	534227.381406	44.825255
3513.347792	533964.803495	44.830260
3513.353145	533682.055019	44.835265
3513.275158	533409.507359	44.840269
3513.058654	533134.959931	44.845274
3513.357447	532862.741292	44.850279
3512.963104	532600.979955	44.855284
3513.214503	532338.447659	44.860289
3513.232824	532056.977180	44.865293
3512.977937	531791.544255	44.870298
3513.216537	531517.342658	44.875303
3513.163571	531256.911766	44.880308
3513.191564	530985.309753	44.885313
3513.391764	530723.514031	44.890317
3513.008791	530461.207593	44.895322
3513.092842	530189.026069	44.900327
3512.947898	529931.615275	44.905332
3512.890860	529659.700339	44.910337
3513.185978	529401.549001	44.915341
3513.420636	529135.933763	44.920346
3513.085847	528865.363776	44.925351
3513.205910	528607.934988	44.930356
3513.590694	528332.286017	44.935361
3513.713348	528069.951447	44.940365
3513.166057	527799.953385	44.945370
3513.261908	527536.705355	44.950375
3512.638824	527267.114302	44.955380
3512.687946	526998.160734	44.960385
3512.756758	526744.494072	44.965389
3512.578684	526495.761772	44.970394
3512.778890	526232.321300	44.975399
3512.571772	525975.609282	44.980404
3512.666216	525720.052923	44.985409
3512.722369	525469.547051	44.990413
3512.380192	525220.316598	44.995418
3512.495674	524952.829214	45.000423
3512.488440	524700.604755	45.005428
3512.414698	524451.063196	45.010433
3512.804803	524197.752678	45.015437
3512.238898	523946.822601	45.020442
3512.451723	523687.475104	45.025447
3512.272755	523453.182670	45.030452
3512.125838	523201.714175	45.035457
3512.390987	522960.521942	45.040461
3512.172771	522717.035221	45.045466
3512.428825	522450.388062	45.050471
3512.019204	522207.885169	45.055476
3512.259512	521966.075330	45.060481
3512.313247	521723.485541	45.065485
3512.055994	521489.125432	45.070490
3512.603746	521233.011293	45.075495
3512.188187	520994.277261	45.080500
3512.326206	520748.880056	45.085505
3512.456356	520510.499728	45.090509
3512.097833	520264.472474	45.095514
3512.381340	520009.847340	45.100519
3512.061796	519766.229451	45.105524
3511.690448	519527.212307	45.110529
3512.034137	519292.564189	45.115533
3511.756325	519059.281201	45.120538
3512.216653	518819.555421	45.125543
3511.844383	518581.937793	45.130548
3511.910612	518349.191307	45.135553
3511.726830	518106.180354	45.140557
3511.607980	517874.316893	45.145562
3511.758036	517634.221478	45.150567
3511.703005	517407.997144	45.155572
3511.469031	517178.264264	45.160577
3511.708400	516946.376154	45.165581
3511.524445	516723.901647	45.170586
3511.790066	516491.143496	45.175591
3511.787654	516259.084282	45.180596
3511.698046	516030.976622	45.185601
3511.986797	515798.810270	45.190605
3511.674093	515561.186340	45.195610
3511.898314	515326.093976	45.200615
3511.699122	515102.840990	45.205620
3511.486507	514872.463974	45.210625
3511.532658	514643.655974	45.215629
3511.500241	514426.982824	45.220634
3511.719158	514198.290337	45.225639
3511.578020	513972.737779	45.230644
3511.619547	513739.168262	45.235649
3511.838546	513518.852483	45.240653
3511.671441	513280.006812	45.245658
3511.973215	513048.049810	45.250663
3511.448242	512821.131475	45.255668
3511.333304	512593.483003	45.260673
3511.270603	512384.769786	45.265677
3511.223968	512161.196031	45.270682
3511.947369	511929.251546	45.275687
3511.562505	511705.830119	45.280692
3511.678501	511485.301239	45.285697
3511.699269	511257.357593	45.290701
3511.481285	511026.621683	45.295706
3511.538677	510804.324701	45.300711
3511.493360	510583.659163	45.305716
3511.611911	510361.547639	45.310721
3511.548968	510135.876088	45.315725
3511.448935	509923.245552	45.320730
3511.376051	509687.462414	45.325735
3510.992980	509466.889518	45.330740
3511.422152	509248.853313	45.335745
3511.420965	509025.732794	45.340749
3511.165425	508815.287077	45.345754
3511.312870	508590.265169	45.350759
3511.325769	508382.092676	45.355764
3511.091046	508152.530760	45.360769
3511.258319	507937.351573	45.365773
3511.306476	507731.337828	45.370778
3511.143437	507507.920464	45.375783
3511.040622	507295.912376	45.380788
3511.104984	507069.922934	45.385793
3511.020581	506858.461895	45.390797
3510.710159	506650.423165	45.395802
3510.975913	506436.420085	45.400807
3510.610424	506236.624315	45.405812
3511.052524	506027.438114	45.410817
3510.837375	505805.168529	45.415821
3510.701740	505598.754425	45.420826
3510.764061	505387.299550	45.425831
3510.911062	505190.739533	45.430836
3510.817591	504980.923521	45.435841
3510.839709	504775.786269	45.440845
3510.788761	504563.986115	45.445850
3510.821516	504355.808646	45.450855
3510.454092	504159.930573	45.455860
3510.560601	503952.796946	45.460865
3510.830335	503746.492226	45.465869
3510.379886	503540.408964	45.470874
3510.869655	503338.763078	45.475879
3510.811821	503134.781518	45.480884
3510.807385	502932.608321	45.485889
3510.879368	502732.997981	45.490893
3510.767130	502522.850098	45.495898
3510.966588	502307.944364	45.500903
3510.497752	502109.126563	45.505908
3510.509494	501901.730276	45.510913
3510.521272	501699.185143	45.515917
3510.080192	501502.124843	45.520922
3510.355021	501306.406223	45.525927
3510.049660	501115.233797	45.530932
3510.095390	500917.476618	45.535937
3510.405180	500727.307029	45.540941
3510.140149	500539.761583	45.545946
3510.063285	500349.906476	45.550951
3509.986987	500159.846827	45.555956
3510.636917	499962.682942	45.560961
3510.498489	499753.970520	45.565965
3510.181720	499567.990419	45.570970
3509.872101	499364.965797	45.575975
3510.009390	499191.292948	45.580980
3509.847528	498997.492525	45.585985
3510.024810	498813.897461	45.590989
3509.887397	498626.207387	45.595994
3510.094492	498434.056759	45.600999
3509.944356	498258.450991	45.606004
3509.792949	498076.926741	45.611009
3510.299375	497887.955266	45.616013
3509.965509	497702.058330	45.621018
3509.804219	497505.104929	45.626023
3509.342299	497330.806947	45.631028
3509.961473	497141.656055	45.636033
3510.193507	496955.199013	45.641037
3509.501904	496781.389693	45.646042
3509.985064	496597.262824	45.651047
3509.555833	496419.207153	45.656052
3509.458597	496235.377716	45.661057
3509.700213	496054.017282	45.666061
3509.416315	495884.933911	45.671066
3509.616745	495704.841191	45.676071
3509.250091	495530.053011	45.681076
3509.494080	495349.999636	45.686081
3509.426073	495177.786945	45.691085
3509.386966	495005.921625	45.696090
3509.618064	494820.553838	45.701095
3509.761038	494648.400885	45.706100
3509.342824	494476.544327	45.711105
3509.569285	494298.202526	45.716109
3509.434270	494122.904979	45.721114
3509.405243	493947.536937	45.726119
3509.236445	493778.311644	45.731124
3509.458513	493608.259153	45.736129
3509.613836	493434.068363	45.741133
3509.382895	493264.848563	45.746138
3509.742401	493087.938316	45.751143
3509.696486	492924.753899	45.756148
3509.446592	492751.232348	45.761153
3509.602251	492568.685734	45.766157
3509.349028	492402.496440	45.771162
3509.384671	492226.239611	45.776167
3509.169461	492064.897072	45.781172
3509.439047	491899.018327	45.786177
3509.194600	491731.303311	45.791181
3509.010578	491558.669021	45.796186
3509.465215	491392.247863	45.801191
3509.491393	491222.812146	45.806196
3509.196059	491055.048608	45.811201
3509.431967	490894.427496	45.816205
3509.024927	490734.420597	45.821210
3509.422321	490563.194819	45.826215
3509.262799	490388.419640	45.831220
3509.212847	490218.278701	45.836225
3508.973633	490052.772568	45.841229
3508.967028	489894.106154	45.846234
3509.290661	489727.084114	45.851239
3509.298675	489578.632742	45.856244
3508.929353	489419.669724	45.861249
3509.011277	489243.576796	45.866253
3509.110660	489085.492034	45.871258
3509.217043	488928.568402	45.876263
3509.512817	488760.276825	45.881268
3509.416482	488598.628508	45.886273
3509.558527	488436.381383	45.891277
3508.865037	488269.063555	45.896282
3509.397496	488101.433589	45.901287
3509.315736	487940.586278	45.906292
3508.869155	487778.382917	45.911297
3509.204515	487608.302365	45.916301
3508.778502	487454.492475	45.921306
3508.663154	487292.885877	45.926311
3508.555612	487142.662301	45.931316
3508.742457	486982.822971	45.936321
3509.176104	486820.409805	45.941325
3508.886754	486667.126300	45.946330
3509.023529	486505.671797	45.951335
3508.939155	486353.362658	45.956340
3508.943267	486185.652708	45.961345
3508.950406	486037.221901	45.966349
3508.832115	485879.094634	45.971354
3508.914802	485721.134060	45.976359
3508.618303	485564.299585	45.981364
3508.938290	485405.738970	45.986369
3508.860819	485251.799622	45.991373
3508.758977	485103.075885	45.996378
3509.103695	484937.117822	46.001383
3509.014157	484787.731393	46.006388
3508.754916	484634.273187	46.011393
3508.882645	484475.737041	46.016397
3508.530882	484318.951538	46.021402
3508.526613	484158.056324	46.026407
3508.406899	484017.778763	46.031412
3508.656675	483868.832765	46.036417
3508.518897	483714.080509	46.041421
3508.410623	483573.797483	46.046426
3508.649993	483421.002837	46.051431
3508.429507	483274.207336	46.056436
3508.449773	483130.406434	46.061441
3508.608097	482988.605424	46.066445
3508.168117	482841.590753	46.071450
3508.272355	482694.127628	46.076455
3508.290803	482549.158163	46.081460
3508.413132	482406.650032	46.086465
3508.662869	482264.625187	46.091469
3508.250673	482122.914707	46.096474
3508.266162	481971.968119	46.101479
3508.448990	481834.557571	46.106484
3508.281412	481688.347410	46.111489
3508.684914	481548.062300	46.116493
3508.306228	481400.367240	46.121498
3508.140394	481246.610767	46.126503
3508.072795	481123.158190	46.131508
3508.430826	480981.155298	46.136513
3508.523724	480833.223186	46.141517
3508.430989	480699.799497	46.146522
3508.494519	480557.134832	46.151527
3508.221898	480410.881579	46.156532
3508.239437	480264.020737	46.161537
3508.226132	480114.531528	46.166541
3508.267538	479995.254376	46.171546
3508.284640	479850.364582	46.176551
3508.232938	479713.939739	46.181556
3508.298828	479568.026852	46.186561
3508.525075	479429.881772	46.191565
3508.250810	479289.391043	46.196570
3508.409389	479139.358158	46.201575
3508.256096	479005.831035	46.206580
3508.229305	478867.623618	46.211585
3508.107651	478733.886581	46.216589
3508.254260	478600.355893	46.221594
3508.243525	478457.434203	46.226599
3508.018154	478334.394531	46.231604
3508.118652	478189.983511	46.236609
3508.017175	478047.580386	46.241613
3507.879332	477920.067563	46.246618
3508.290439	477774.790137	46.251623
3508.115714	477640.395928	46.256628
3508.211136	477503.676203	46.261633
3508.376981	477367.804165	46.266637
3508.052120	477235.002182	46.271642
3508.298847	477088.380304	46.276647
3508.282014	476956.333818	46.281652
3508.264764	476817.400364	46.286657
3508.229793	476673.608078	46.291661
3508.030521	476543.716369	46.296666
3508.169800	476410.829156	46.301671
3508.144441	476267.183944	46.306676
3508.093410	476137.264046	46.311681
3507.764470	476009.011008	46.316685
3507.698771	475874.838400	46.321690
3507.828372	475735.365326	46.326695
3507.600195	475619.852630	46.331700
3507.503086	475491.100670	46.336705
3507.930701	475360.688469	46.341709
3507.589871	475238.356620	46.346714
3507.670639	475103.900202	46.351719
3507.406795	474992.086215	46.356724
3507.161721	474870.140678	46.361729
3507.727257	474738.333298	46.366733
3507.454654	474629.658213	46.371738
3507.535989	474494.994713	46.376743
3507.718045	474381.632356	46.381748
3507.461315	474253.810543	46.386753
3507.625501	474124.700608	46.391757
3507.473427	474010.582788	46.396762
3507.428693	473881.911962	46.401767
3507.737609	473772.474224	46.406772
3507.546068	473647.219809	46.411777
3507.499649	473520.775004	46.416781
3507.185174	473408.858824	46.421786
3507.642679	473284.149492	46.426791
3507.804092	473163.490680	46.431796
3507.419734	473052.850367	46.436801
3507.907413	472914.459713	46.441805
3507.610019	472802.486329	46.446810
3507.829848	472669.811721	46.451815
3507.724491	472551.270918	46.456820
3507.722496	472427.799150	46.461825
3507.752671	472293.179097	46.466829
3507.590473	472184.268290	46.471834
3507.697677	472050.291730	46.476839
3507.578906	471933.116744	46.481844
3507.317911	471815.357548	46.486849
3507.538840	471689.513102	46.491853
3507.435792	471582.513284	46.496858
3507.350122	471457.681933	46.501863
3507.457444	471334.640126	46.506868
3507.277570	471226.689086	46.511873
3507.678635	471101.519020	46.516877
3507.484910	470995.594963	46.521882
3507.490419	470873.175309	46.526887
3507.634999	470751.541505	46.531892
3507.312600	470644.117956	46.536897
3507.326418	470516.629585	46.541901
3507.098881	470404.731260	46.546906
3507.096001	470298.618748	46.551911
3507.180638	470186.412572	46.556916
3507.243437	470073.297735	46.561921
3507.561047	469956.238536	46.566925
3506.960952	469845.920064	46.571930
3507.063794	469730.972873	46.576935
3507.187529	469623.923216	46.581940
3507.244136	469514.959609	46.586945
3507.351951	469405.226835	46.591949
3507.292009	469296.332526	46.596954
3507.572869	469173.500278	46.601959
3507.588278	469058.310672	46.606964
3507.192027	468947.394968	46.611969
3507.852694	468817.555923	46.616973
3507.280051	468722.523939	46.621978
3507.210311	468590.883174	46.626983
3506.921539	468475.336732	46.631988
3506.706325	468374.517896	46.636993
3506.988253	468261.506818	46.641997
3506.822316	468164.477670	46.647002
3507.060643	468054.765481	46.652007
3507.151631	467945.685704	46.657012
3506.978104	467832.699199	46.662017
3507.284973	467727.988504	46.667021
3507.089619	467622.248517	46.672026
3507.059543	467513.541551	46.677031
3507.022307	467409.799718	46.682036
3506.783634	467304.318662	46.687041
3507.162062	467195.134869	46.692045
3506.708705	467095.565764	46.697050
3506.805405	466976.195655	46.702055
3506.763592	466878.733516	46.707060
3506.745531	466777.973921	46.712065
3507.115137	466670.713737	46.717069
3506.797936	466574.056980	46.722074
3506.624099	466464.811352	46.727079
3506.835664	466367.860630	46.732084
3506.573877	466268.963786	46.737089
3506.702474	466164.680297	46.742093
3506.541492	466074.529717	46.747098
3506.759852	465973.168259	46.752103
3507.132412	465876.795525	46.757108
3506.569761	465782.000551	46.762113
3506.834186	465669.027864	46.767117
3506.820995	465577.887131	46.772122
3507.260116	465466.960628	46.777127
3507.168055	465365.547659	46.782132
3506.996219	465255.230899	46.787137
3507.154902	465142.627842	46.792141
3506.812624	465043.434477	46.797146
3506.887395	464943.561415	46.802151
3506.993779	464848.090311	46.807156
3506.644235	464751.733943	46.812161
3507.147617	464632.026570	46.817165
3506.698671	464552.912528	46.822170
3506.672114	464446.720967	46.827175
3506.770947	464344.712735	46.832180
3506.472618	464249.865125	46.837185
3506.665824	464144.445057	46.842189
3506.483313	464046.384658	46.847194
3506.732765	463941.713898	46.852199
3506.845988	463860.069006	46.857204
3506.437389	463768.531281	46.862209
3506.752897	463664.455770	46.867213
3506.300747	463583.007589	46.872218
3506.278872	463484.106237	46.877223
3506.572917	463383.782380	46.882228
3506.463066	463296.903646	46.887233
3506.457688	463205.041083	46.892237
3506.401601	463113.845452	46.897242
3506.339451	463017.127410	46.902247
3506.538163	462926.900800	46.907252
3506.332266	462836.489509	46.912257
3506.576052	462743.670169	46.917261
3506.274228	462655.757284	46.922266
3506.506124	462561.013617	46.927271
3506.553172	462470.456105	46.932276
3506.272010	462386.541521	46.937281
3506.375737	462296.074870	46.942285
3506.389921	462202.684114	46.947290
3506.707855	462115.524412	46.952295
3506.167413	462024.355744	46.957300
3506.380726	461935.540915	46.962305
3506.750785	461829.875495	46.967309
3506.628924	461755.964267	46.972314
3506.367810	461652.787308	46.977319
3506.241879	461563.471318	46.982324
3506.644536	461467.578408	46.987329
3506.731027	461369.560027	46.992333
3506.120855	461293.500779	46.997338
3506.354639	461196.875272	47.002343
3506.567233	461109.475735	47.007348
3506.534355	461028.553459	47.012353
3506.301847	460924.202278	47.017357
3506.032690	460850.211457	47.022362
3506.408584	460762.833181	47.027367
3506.207548	460674.539510	47.032372
3506.170020	460584.646565	47.037377
3506.097653	460494.911189	47.042381
3505.563558	460424.207303	47.047386
3505.630254	460345.393648	47.052391
3505.899731	460273.791866	47.057396
3505.795861	460191.256626	47.062401
3506.195456	460097.384689	47.067405
3506.029083	460027.832861	47.072410
3505.945544	459945.546515	47.077415
3506.096511	459865.550977	47.082420
3506.106274	459781.474291	47.087425
3506.020686	459694.119430	47.092429
3505.889535	459630.692291	47.097434
3505.962275	459545.336888	47.102439
3506.186266	459462.894679	47.107444
3505.816450	459382.884765	47.112449
3506.110678	459304.180171	47.117453
3505.935128	459224.998004	47.122458
3505.963199	459147.503870	47.127463
3506.129693	459062.941272	47.132468
3506.010892	458983.089614	47.137473
3506.387167	458899.706831	47.142477
3506.015841	458829.831050	47.147482
3505.900444	458733.709317	47.152487
3505.969093	458660.108792	47.157492
3505.838522	458584.362718	47.162497
3505.768206	458503.943373	47.167501
3505.732873	458437.201783	47.172506
3505.637791	458360.637896	47.177511
3505.920178	458293.334758	47.182516
3506.142409	458224.673246	47.187521
3506.494780	458132.726061	47.192525
3505.759564	458063.416560	47.197530
3505.789343	457980.393211	47.202535
3505.890209	457900.144946	47.207540
3505.626956	457826.040517	47.212545
3505.766213	457745.480980	47.217549
3505.993747	457688.068440	47.222554
3505.741899	457613.353077	47.227559
3505.894051	457533.195957	47.232564
3505.775484	457457.240842	47.237569
3506.431243	457373.043733	47.242573
3505.699010	457302.159879	47.247578
3505.650627	457220.870013	47.252583
3506.198738	457149.412212	47.257588
3505.755825	457075.234324	47.262593
3505.687932	456995.720859	47.267597
3505.945220	456939.314811	47.272602
3505.550790	456855.092117	47.277607
3505.813556	456779.272077	47.282612
3505.776329	456710.497646	47.287617
3505.503810	456644.550896	47.292621
3505.433062	456574.920062	47.297626
3505.656322	456500.119448	47.302631
3505.501453	456435.368403	47.307636
3505.520872	456366.735190	47.312641
3505.819747	456295.367615	47.317645
3505.409335	456227.516941	47.322650
3505.358968	456151.849392	47.327655
3505.337150	456081.955070	47.332660
3505.569474	456026.108303	47.337665
3505.502420	455951.862112	47.342669
3505.181029	455891.648984	47.347674
3505.441002	455823.327673	47.352679
3505.935337	455758.818433	47.357684
3505.761823	455698.782237	47.362689
3505.756373	455615.856557	47.367693
3505.569644	455559.826617	47.372698
3505.696192	455489.043209	47.377703
3505.697416	455415.290288	47.382708
3505.373506	455357.914605	47.387713
3505.626011	455283.256580	47.392717
3505.570186	455226.645785	47.397722
3505.626033	455149.232913	47.402727
3505.742411	455077.841533	47.407732
3505.451737	455022.081310	47.412737
3505.643033	454953.870187	47.417741
3505.673776	454888.018016	47.422746
3505.423333	454813.140003	47.427751
3505.465923	454751.239245	47.432756
3505.327779	454685.009728	47.437761
3505.998635	454621.075040	47.442765
3505.639598	454562.334450	47.447770
3505.513580	454491.134480	47.452775
3505.627141	454412.897896	47.457780
3505.535866	454346.912739	47.462785
3505.452136	454282.244074	47.467789
3505.451403	454227.800858	47.472794
3505.539568	454159.604693	47.477799
3505.499403	454082.863174	47.482804
3505.465023	454029.388335	47.487809
3505.644054	453964.724493	47.492813
3505.727880	453901.141257	47.497818
3505.472838	453833.560232	47.502823
3505.812720	453766.739188	47.507828
3505.388890	453702.228150	47.512833
3505.486979	453628.148077	47.517837
3505.594827	453569.679772	47.522842
3505.510473	453501.054630	47.527847
3505.557589	453440.467180	47.532852
3504.970748	453385.310699	47.537857
3505.477899	453313.795747	47.542861
3505.707315	453259.412053	47.547866
3505.680119	453194.071274	47.552871
3505.670039	453127.966941	47.557876
3505.844754	453054.480056	47.562881
3505.854553	452986.039899	47.567885
3505.448564	452925.224127	47.572890
3505.737768	452853.795489	47.577895
3505.711075	452797.173003	47.582900
3505.598659	452737.726030	47.587905
3505.809524	452651.304085	47.592909
3505.505470	452590.976881	47.597914
3505.639056	452524.237726	47.602919
3505.592252	452460.824433	47.607924
3505.489160	452395.747565	47.612929
3505.837371	452323.495870	47.617933
3505.376962	452263.093012	47.622938
3505.657387	452201.042564	47.627943
3505.428977	452141.816470	47.632948
3505.423037	452080.879203	47.637953
3505.777358	452011.464434	47.642957
3505.622526	451957.447106	47.647962
3505.649912	451887.530070	47.652967
3505.290523	451815.600215	47.657972
3505.212618	451752.240758	47.662977
3505.563267	451683.484596	47.667981
3505.415546	451634.382960	47.672986
3504.918213	451576.975618	47.677991
3504.908675	451515.935906	47.682996
3504.893904	451461.842671	47.688001
3504.781713	451398.133094	47.693005
3504.991106	451357.740778	47.698010
3505.075296	451301.450160	47.703015
3504.908587	451255.950528	47.708020
3505.020001	451204.826348	47.713025
3505.267973	451150.433942	47.718029
3505.101081	451096.061531	47.723034
3504.936475	451039.204286	47.728039
3505.016739	450987.882093	47.733044
3504.852265	450937.362065	47.738049
3505.180759	450880.927195	47.743053
3505.068776	450825.074388	47.748058
3504.945892	450777.893108	47.753063
3505.111181	450720.319554	47.758068
3504.795896	450657.402898	47.763073
3504.925107	450605.462993	47.768077
3505.016740	450557.179861	47.773082
3505.002346	450513.629945	47.778087
3505.078361	450459.265096	47.783092
3504.980008	450415.120892	47.788097
3505.145121	450350.296026	47.793101
3505.219218	450297.857749	47.798106
3505.223596	450244.822822	47.803111
3505.148622	450192.713947	47.808116
3505.168967	450145.557483	47.813121
3505.103497	450094.410081	47.818125
3505.195593	450031.371275	47.823130
3505.193556	449986.094264	47.828135
3505.305605	449919.299721	47.833140
3504.585741	449870.240916	47.838145
3505.167082	449822.937232	47.843149
3505.454086	449772.489404	47.848154
3505.386136	449707.448825	47.853159
3505.226806	449654.693872	47.858164
3505.042469	449595.047376	47.863169
3505.405320	449538.197387	47.868173
3505.317585	449489.080456	47.873178
3505.320156	449432.900145	47.878183
3505.436997	449369.956532	47.883188
3504.994348	449332.663178	47.888193
3504.768229	449268.662328	47.893197
3504.921532	449215.193731	47.898202
3504.832397	449158.064959	47.903207
3504.701069	449110.932065	47.908212
3504.462198	449078.673933	47.913217
3504.792904	449030.650690	47.918221
3504.999071	448985.335968	47.923226
3504.984373	448934.075657	47.928231
3504.807673	448880.510441	47.933236
3505.030429	448839.806752	47.938241
3504.542071	448781.883133	47.943245
3504.610130	448750.687611	47.948250
3504.878539	448704.550368	47.953255
3504.899751	448663.272283	47.958260
3504.716111	448613.358388	47.963265
3504.704125	448566.812368	47.968269
3504.506652	448521.514863	47.973274
3504.613228	448475.759696	47.978279
3504.727839	448435.479341	47.983284
3504.508663	448380.246796	47.988289
3504.915524	448342.350273	47.993293
3504.797032	448303.225012	47.998298
3504.278969	448254.685742	48.003303
3504.534189	448201.399997	48.008308
3504.394921	448174.143453	48.013313
3504.784063	448129.099891	48.018317
3504.478097	448087.369474	48.023322
3504.611709	448059.812653	48.028327
3505.268877	447994.693674	48.033332
3505.286781	447960.716642	48.038337
3505.044642	447910.202582	48.043341
3505.055021	447856.247868	48.048346
3505.424648	447801.876720	48.053351
3505.242334	447752.569057	48.058356
3505.045281	447697.483074	48.063361
3504.734016	447641.554408	48.068365
3504.961723	447596.942945	48.073370
3505.092505	447549.812516	48.078375
3504.887072	447497.617825	48.083380
3504.739137	447465.189572	48.088385
3504.689440	447407.795784	48.093389
3504.841374	447368.166239	48.098394
3505.116880	447311.274460	48.103399
3504.950223	447279.102665	48.108404
3504.907741	447237.579127	48.113409
3504.912502	447197.365883	48.118413
3505.005308	447147.959127	48.123418
3504.572547	447094.382396	48.128423
3504.962069	447049.742154	48.133428
3504.838810	447008.688347	48.138433
3504.600990	446958.171281	48.143437
3504.544863	446929.479062	48.148442
3504.566117	446878.004789	48.153447
3504.749871	446837.557461	48.158452
3504.728440	446791.921935	48.163457
3504.544407	446747.835386	48.168461
3504.684826	446716.827355	48.173466
3504.380727	446671.290546	48.178471
3504.344292	446632.046767	48.183476
3504.206446	446597.079933	48.188481
3504.460714	446557.329983	48.193485
3504.316203	446533.114873	48.198490
3504.305770	446494.677776	48.203495
3504.388322	446453.942734	48.208500
3504.199171	446438.203885	48.213505
3504.235362	446395.803182	48.218509
3504.188350	446348.396181	48.223514
3504.139001	446315.645072	48.228519
3504.484433	446293.678757	48.233524
3504.376276	446262.103971	48.238529
3504.740455	446217.618449	48.243533
3504.522008	446187.431598	48.248538
3504.727675	446134.047707	48.253543
3504.947629	446102.163100	48.258548
3504.700002	446054.738991	48.263553
3504.863780	446010.236543	48.268557
3504.659096	445967.368997	48.273562
3504.573348	445932.240041	48.278567
3504.719658	445889.363119	48.283572
3503.978647	445850.136783	48.288577
3504.378504	445824.154406	48.293581
3504.340425	445782.170866	48.298586
3504.309935	445742.417310	48.303591
3504.614456	445711.836214	48.308596
3504.184021	445691.675284	48.313601
3504.221094	445648.917958	48.318605
3504.408774	445618.863809	48.323610
3504.261668	445584.201175	48.328615
3504.201077	445537.758245	48.333620
3504.328857	445517.400408	48.338625
3504.343070	445488.034969	48.343629
3504.361389	445454.408859	48.348634
3504.545833	445427.296374	48.353639
3504.291356	445382.407617	48.358644
3504.211114	445345.146786	48.363649
3504.217962	445309.291005	48.368653
3504.348796	445285.940314	48.373658
3504.480049	445246.918929	48.378663
3504.331782	445203.228796	48.383668
3504.446930	445189.262772	48.388673
3504.552468	445148.673463	48.393677
3504.482842	445106.440416	48.398682
3504.246792	445078.740004	48.403687
3504.299066	445036.486005	48.408692
3504.397380	444999.650515	48.413697
3504.558182	444977.308663	48.418701
3504.430787	444934.679425	48.423706
3504.272757	444909.704065	48.428711
3504.568454	444878.108994	48.433716
3504.325046	444845.540917	48.438721
3504.450177	444809.258385	48.443725
3504.292192	444782.254271	48.448730
3504.425673	444730.704953	48.453735
3504.837642	444699.444774	48.458740
3504.418144	444670.557994	48.463745
3504.426457	444630.846468	48.468749
3504.341674	444598.504508	48.473754
3504.231526	444567.333288	48.478759
3504.481279	444522.001627	48.483764
3504.182078	444497.810628	48.488769
3504.202605	444473.260714	48.493773
3504.379136	444433.621533	48.498778
3504.114251	444404.505132	48.503783
3504.061091	444376.874019	48.508788
3504.127253	444353.127632	48.513793
3504.345726	444310.083088	48.518797
3504.220699	444283.478449	48.523802
3504.237390	444262.124070	48.528807
3504.241438	444228.549197	48.533812
3504.119182	444190.228494	48.538817
3504.363196	444170.914583	48.543821
3504.381673	444141.952309	48.548826
3504.084801	444102.139770	48.553831
3504.281160	444072.335563	48.558836
3504.202910	444050.033568	48.563841
3503.977631	444013.860248	48.568845
3504.370002	443990.717080	48.573850
3504.315474	443958.622579	48.578855
3504.313783	443951.066040	48.583860
3504.220665	443910.761905	48.588865
3504.355367	443869.455167	48.593869
3504.596391	443856.633283	48.598874
3504.454692	443819.988911	48.603879
3504.473586	443778.955362	48.608884
3504.059645	443762.897909	48.613889
3504.457614	443718.198580	48.618893
3504.558724	443686.279970	48.623898
3504.483707	443658.753105	48.628903
3504.515088	443619.390804	48.633908
3504.421476	443602.061309	48.638913
3504.527938	443556.802809	48.643917
3504.306539	443512.462402	48.648922
3504.138825	443495.297629	48.653927
3504.823616	443464.141234	48.658932
3504.828095	443427.623392	48.663937
3504.642428	443391.898731	48.668941
3504.852559	443351.034590	48.673946
3504.435813	443317.327279	48.678951
3504.303363	443280.071793	48.683956
3504.259645	443249.901699	48.688961
3504.312762	443223.366775	48.693965
3504.274612	443191.623371	48.698970
3504.178423	443160.549175	48.703975
3504.284953	443124.013397	48.708980
3503.826357	443104.362035	48.713985
3503.997176	443071.416237	48.718989
3504.378350	443029.609343	48.723994
3504.344130	443001.719644	48.728999
3504.250812	442985.251833	48.734004
3503.989136	442949.640859	48.739009
3504.090752	442907.475710	48.744013
3504.268211	442897.808718	48.749018
3504.045202	442880.094985	48.754023
3504.282751	442847.695369	48.759028
3504.071032	442817.451921	48.764033
3504.091590	442799.392216	48.769037
3504.150610	442779.601457	48.774042
3504.043027	442747.159183	48.779047
3503.789852	442705.206381	48.784052
3503.814821	442690.594785	48.789057
3503.953166	442665.667665	48.794061
3503.903933	442651.373032	48.799066
3503.843175	442647.021486	48.804071
3504.184826	442615.415268	48.809076
3503.859866	442583.517068	48.814081
3504.153948	442555.672179	48.819085
3504.029645	442539.412201	48.824090
3503.999018	442521.766768	48.829095
3504.243668	442498.545796	48.834100
3503.763994	442461.804677	48.839105
3503.980805	442431.081757	48.844109
3504.115095	442412.951591	48.849114
3504.210365	442392.494923	48.854119
3504.564519	442368.747909	48.859124
3504.324218	442342.262012	48.864129
3504.353115	442313.853446	48.869133
3504.576020	442285.665321	48.874138
3504.117057	442251.862122	48.879143
3504.139352	442220.056258	48.884148
3503.589542	442213.099916	48.889153
3504.148109	442186.223816	48.894157
3503.801705	442148.901481	48.899162
3503.703907	442129.745564	48.904167
3504.239392	442105.155761	48.909172
3503.772448	442086.062837	48.914177
3503.925386	442069.095791	48.919181
3504.069002	442060.042864	48.924186
3504.097981	442031.836803	48.929191
3504.082409	441993.341840	48.934196
3503.828517	441981.567069	48.939201
3504.227133	441948.631399	48.944205
3504.106196	441941.652461	48.949210
3503.935706	441916.929385	48.954215
3504.389606	441886.520268	48.959220
3504.110136	441866.431426	48.964225
3504.066546	441837.375233	48.969229
3503.975391	441805.537415	48.974234
3503.791834	441773.157385	48.979239
3503.827010	441755.500095	48.984244
3503.661523	441738.232110	48.989249
3503.659609	441723.167957	48.994253
3503.971453	441709.267552	48.999258
3503.695267	441701.199157	49.004263
3503.981605	441675.281914	49.009268
3503.668713	441651.901632	49.014273
3504.000533	441615.578470	49.019277
3503.875033	441602.767122	49.024282
3503.885990	441589.120908	49.029287
3504.083041	441566.109963	49.034292
3503.593288	441560.005439	49.039297
3503.680271	441537.723375	49.044301
3503.693389	441520.475443	49.049306
3503.612400	441510.496910	49.054311
3503.775552	441489.165521	49.059316
3503.849110	441460.748220	49.064321
3503.954424	441433.897869	49.069325
3503.912460	441422.644561	49.074330
3503.868904	441402.362841	49.079335
3504.362946	441392.844019	49.084340
3503.663360	441379.775506	49.089345
3504.026378	441335.077260	49.094349
3504.228150	441313.739106	49.099354
3503.952508	441303.540100	49.104359
3504.078563	441283.178585	49.109364
3503.884667	441271.038123	49.114369
3503.910508	441240.396863	49.119373
3504.061271	441209.074826	49.124378
3503.757151	441190.054761	49.129383
3503.918511	441168.824814	49.134388
3504.097778	441153.475715	49.139393
3503.776067	441137.248400	49.144397
3504.081029	441119.392362	49.149402
3504.269439	441092.476681	49.154407
3504.090078	441060.602117	49.159412
3503.684483	441048.903469	49.164417
3503.581834	441033.500976	49.169421
3504.078613	441024.082976	49.174426
3503.480292	441011.859255	49.179431
3503.968279	440984.385051	49.184436
3503.843506	440954.783587	49.189441
3503.629633	440927.479878	49.194445
3503.740756	440917.975512	49.199450
3503.623545	440906.988408	49.204455
3503.459881	440896.110678	49.209460
3503.322824	440887.409536	49.214465
3503.601806	440867.731662	49.219469
3503.589113	440851.349922	49.224474
3504.023589	440845.138108	49.229479
3504.322060	440824.696004	49.234484
3504.200344	440817.919737	49.239489
3503.462842	440775.031443	49.244493
3503.572966	440748.737401	49.249498
3503.398548	440740.752722	49.254503
3503.618899	440723.620953	49.259508
3503.393293	440719.652242	49.264513
3503.718731	440705.089463	49.269517
3504.040048	440694.483895	49.274522
3503.991883	440688.050101	49.279527
3504.133647	440666.112870	49.284532
3503.761064	440665.517070	49.289537
3503.423866	440644.321021	49.294541
3503.491427	440628.584832	49.299546
3503.716781	440618.908658	49.304551
3504.030369	440595.826074	49.309556
3503.927401	440575.350835	49.314561
3504.051678	440552.452706	49.319565
3504.010804	440539.220488	49.324570
3503.862079	440530.876272	49.329575
3503.853017	440509.319714	49.334580
3503.939367	440493.225145	49.339585
3503.781478	440459.215591	49.344589
3503.820517	440430.802853	49.349594
3503.705678	440425.699221	49.354599
3503.916845	440409.735455	49.359604
3503.568398	440402.642698	49.364609
3503.719416	440390.544305	49.369613
3503.514176	440374.347263	49.374618
3503.269994	440371.396167	49.379623
3503.518861	440350.607016	49.384628
3503.320898	440339.075437	49.389633
3503.065881	440327.046340	49.394637
3503.452653	440318.914960	49.399642
3503.367837	440307.871299	49.404647
3503.464733	440290.506646	49.409652
3503.339657	440287.839553	49.414657
3503.493607	440268.030316	49.419661
3503.813294	440257.932072	49.424666
3503.509878	440249.614163	49.429671
3503.839576	440230.231414	49.434676
3503.506643	440226.433115	49.439681
3503.861271	440206.538832	49.444685
3503.530488	440204.059031	49.449690
3503.479954	440199.908155	49.454695
3503.751258	440184.999197	49.459700
3503.938643	440186.438249	49.464705
3503.712220	440165.730080	49.469709
3504.182566	440152.562517	49.474714
3503.797414	440121.330440	49.479719
3503.718812	440091.719931	49.484724
3503.439460	440080.607921	49.489729
3503.570867	440070.440289	49.494733
3503.509538	440058.783781	49.499738
3503.485339	440051.990626	49.504743
3504.055691	440030.131760	49.509748
3503.451725	440030.387067	49.514753
3503.656813	440018.076334	49.519757
3503.805436	440006.992663	49.524762
3503.548428	440000.594328	49.529767
3503.824389	439992.684654	49.534772
3503.359451	439977.749092	49.539777
3503.573667	439971.219561	49.544781
3503.635127	439963.092871	49.549786
3503.363701	439958.928940	49.554791
3503.765857	439933.700040	49.559796
3503.596601	439934.236205	49.564801
3503.488084	439920.862987	49.569805
3503.744360	439904.536069	49.574810
3503.335355	439903.236296	49.579815
3503.667173	439878.678786	49.584820
3503.147353	439878.260282	49.589825
3503.415517	439866.801044	49.594829
3503.618621	439864.686581	49.599834
3503.488115	439859.788398	49.604839
3503.578904	439833.699473	49.609844
3503.366069	439828.358803	49.614849
3503.667517	439821.053434	49.619853
3504.012304	439815.414640	49.624858
3503.537952	439795.458630	49.629863
3503.537773	439776.131810	49.634868
3503.382762	439767.179657	49.639873
3503.724998	439754.946813	49.644877
3503.486382	439739.312997	49.649882
3503.145469	439726.689518	49.654887
3503.413713	439730.143864	49.659892
3503.760381	439735.055895	49.664897
3503.868886	439722.000588	49.669901
3503.877400	439709.114527	49.674906
3503.583788	439684.308505	49.679911
3503.772212	439669.464080	49.684916
3503.544988	439669.908695	49.689921
3503.540807	439648.147554	49.694925
3503.801490	439641.812900	49.699930
3503.711715	439647.763286	49.704935
3503.405400	439624.227541	49.709940
3503.225627	439618.475358	49.714945
3503.269761	439607.510782	49.719949
3503.492941	439597.530170	49.724954
3503.645167	439594.714190	49.729959
3503.704407	439583.087571	49.734964
3503.292215	439573.215438	49.739969
3503.382203	439562.395192	49.744973
3503.359217	439555.398769	49.749978
3503.241180	439552.527476	49.754983
3503.480342	439531.079760	49.759988
3503.199458	439520.982274	49.764993
3503.172239	439517.131652	49.769997
3503.460112	439524.184315	49.775002
3503.308043	439517.311375	49.780007
3503.417402	439514.401250	49.785012
3503.203134	439512.865292	49.790017
3503.630526	439503.001951	49.795021
3503.698834	439492.997009	49.800026
3503.387009	439492.847346	49.805031
3503.482398	439477.765041	49.810036
3503.234961	439475.169470	49.815041
3503.496787	439457.623819	49.820045
3504.079356	439455.495250	49.825050
3503.832251	439447.167422	49.830055
3503.577023	439431.536225	49.835060
3503.207369	439438.599733	49.840065
3503.167742	439425.112997	49.845069
3503.775802	439414.102763	49.850074
3503.356318	439419.855870	49.855079
3503.818732	439406.283399	49.860084
3503.878746	439392.830357	49.865089
3503.863052	439376.092942	49.870093
3503.977889	439349.847158	49.875098
3503.780038	439336.184474	49.880103
3503.920325	439320.079842	49.885108
3503.694467	439316.821107	49.890113
3503.555406	439310.503887	49.895117
3503.526046	439295.189121	49.900122
3503.428503	439301.140926	49.905127
3503.727668	439283.893129	49.910132
3503.334403	439281.626802	49.915137
3503.377298	439266.654772	49.920141
3503.082146	439258.893083	49.925146
3503.389739	439247.832616	49.930151
3503.387550	439243.318210	49.935156
3503.708418	439244.176525	49.940161
3503.599727	439223.548826	49.945165
3503.342395	439224.505869	49.950170
3503.450832	439217.436172	49.955175
3503.613601	439202.240718	49.960180
3503.402227	439202.530452	49.965185
3503.374373	439187.874818	49.970189
3503.660012	439182.296692	49.975194
3503.143098	439181.725492	49.980199
3503.346390	439164.291061	49.985204
3503.277357	439162.020086	49.990209
3503.226912	439156.752981	49.995213
3503.713301	439152.611684	50.000218
3503.322547	439149.482536	50.005223
3503.178580	439142.100816	50.010228
3503.193177	439147.779874	50.015233
3502.888018	439145.701401	50.020237
3503.342678	439138.318919	50.025242
3502.877789	439138.347573	50.030247
3503.241086	439114.138938	50.035252
3503.137625	439127.751755	50.040257
3503.209331	439138.747520	50.045261
3503.347395	439136.796278	50.050266
3502.968365	439135.186970	50.055271
3503.355393	439122.743218	50.060276
3503.870738	439113.625609	50.065281
3503.352047	439107.576066	50.070285
3503.508620	439107.650789	50.075290
3503.297623	439103.121280	50.080295
3503.505453	439081.424838	50.085300
3503.505648	439083.758306	50.090305
3503.151203	439078.238720	50.095309
3503.499911	439060.119910	50.100314
3502.937420	439057.679541	50.105319
3502.875261	439051.856399	50.110324
3503.087348	439074.698651	50.115329
3502.896044	439074.325491	50.120333
3502.914022	439074.880434	50.125338
3502.516774	439078.651430	50.130343
3503.024265	439089.927905	50.135348
3503.210116	439092.381857	50.140353
3503.110468	439100.870486	50.145357
3503.941501	439091.293139	50.150362
3503.059553	439092.407570	50.155367
3503.725325	439074.031719	50.160372
3503.648868	439064.051303	50.165377
3503.383510	439064.096614	50.170381
3503.651797	439051.470184	50.175386
3503.149357	439047.599167	50.180391
3503.504533	439038.965432	50.185396
3503.504066	439032.167912	50.190401
3503.561122	439025.157655	50.195405
3503.193306	439010.154125	50.200410
3503.064826	439022.452339	50.205415
3503.431343	439009.707656	50.210420
3503.648095	439003.583235	50.215425
3503.652315	439001.451921	50.220429
3503.360183	438993.689623	50.225434
3503.197971	438984.535469	50.230439
3503.316174	438993.392770	50.235444
3503.429772	439003.671250	50.240449
3503.083469	438999.215551	50.245453
3502.989719	438995.173284	50.250458
3503.092456	438995.105015	50.255463
3502.762845	438982.682094	50.260468
3502.961156	438994.366511	50.265473
3503.031465	439011.399263	50.270477
3503.219025	439002.439035	50.275482
3502.660911	439012.324921	50.280487
3502.930507	438997.060358	50.285492
3502.921613	439009.896173	50.290497
3502.996617	439024.391692	50.295501
3503.205549	439024.558932	50.300506
3503.028662	439021.951261	50.305511
3502.958835	439007.809958	50.310516
3503.200678	439019.233287	50.315521
3503.029825	439037.879777	50.320525
3503.068218	439038.228321	50.325530
3503.015406	439040.469388	50.330535
3503.216572	439037.695709	50.335540
3503.240749	439028.205377	50.340545
3503.588016	439026.979330	50.345549
3503.290896	439017.949683	50.350554
3502.695936	439011.101481	50.355559
3503.079445	439027.522729	50.360564
3503.137682	439031.469600	50.365569
3503.333566	439026.566230	50.370573
3503.425167	439020.818282	50.375578
3503.057612	439029.606327	50.380583
3503.093872	439014.229433	50.385588
3503.377966	439011.644505	50.390593
3503.326197	438999.884349	50.395597
3503.066237	439028.032280	50.400602
3502.876782	439040.543810	50.405607
3503.083524	439034.877662	50.410612
3503.016266	439026.975521	50.415617
3503.289650	439031.139298	50.420621
3503.275947	439014.654912	50.425626
3502.721086	439035.954122	50.430631
3502.996463	439042.653974	50.435636
3503.134030	439054.856014	50.440641
3502.955366	439040.885502	50.445645
3503.156242	439036.590022	50.450650
3503.030534	439045.996233	50.455655
3503.080036	439056.640731	50.460660
3503.158419	439060.787070	50.465665
3502.986971	439059.091584	50.470669
3503.107558	439063.027803	50.475674
3502.943884	439060.012054	50.480679
3503.054380	439061.261396	50.485684
3503.161579	439073.062785	50.490689
3503.250152	439071.576543	50.495693
3503.200075	439068.693583	50.500698
3502.798756	439078.958493	50.505703
3502.979999	439068.781892	50.510708
3503.020376	439084.754404	50.515713
3502.963667	439083.749524	50.520717
3503.503495	439096.694507	50.525722
3503.056982	439096.009827	50.530727
3502.984056	439078.064482	50.535732
3503.086548	439048.624568	50.540737
3503.109094	439025.590044	50.545741
3503.155703	438976.882782	50.550746
3502.804252	438927.279539	50.555751
3502.985198	438859.373657	50.560756
3502.899286	438797.042586	50.565761
3502.756127	438713.262717	50.570765
3503.133019	438613.870564	50.575770
3502.716157	438516.947061	50.580775
3502.876059	438392.023262	50.585780
3502.908376	438263.975282	50.590785
3502.558310	438124.678972	50.595789
3502.874346	437971.063439	50.600794
3502.591646	437811.410616	50.605799
3502.551223	437635.379730	50.610804
3502.750218	437452.204104	50.615809
3502.718328	437250.498346	50.620813
3502.948769	437042.556568	50.625818
3502.754399	436828.495931	50.630823
3502.774010	436584.057849	50.635828
3503.052603	436341.399333	50.640833
3502.681177	436073.989023	50.645837
3502.882264	435796.127708	50.650842
3502.756937	435517.659142	50.655847
3503.004967	435210.507744	50.660852
3502.727721	434897.150406	50.665857
3502.754489	434581.402868	50.670861
3502.790919	434243.171861	50.675866
3502.751497	433893.380086	50.680871
3502.734384	433526.783965	50.685876
3502.662668	433153.036738	50.690881
3502.473856	432763.218070	50.695885
3502.776421	432359.709683	50.700890
3502.498247	431948.732510	50.705895
3502.638220	431517.683035	50.710900
3502.628163	431075.030296	50.715905
3502.480974	430609.404084	50.720909
3502.728653	430136.748639	50.725914
3502.564879	429649.842605	50.730919
3502.204589	429141.695618	50.735924
3502.187484	428638.148174	50.740929
3502.278392	428106.911389	50.745933
3502.379112	427559.825828	50.750938
3502.079227	427006.248668	50.755943
3501.957811	426407.455172	50.760948
3502.125317	425815.398829	50.765953
3501.828273	425199.347543	50.770957
3501.796678	424572.321736	50.775962
3501.973591	423932.350645	50.780967
3501.826391	423267.391946	50.785972
3502.032265	422593.674112	50.790977
3501.836235	421902.695253	50.795981
3501.940315	421180.576222	50.800986
3501.279197	420458.592084	50.805991
3501.366595	419708.154731	50.810996
3501.463120	418947.158056	50.816001
3500.987078	418171.587895	50.821005
3501.295250	417363.795540	50.826010
3501.402479	416546.059452	50.831015
3501.040732	415705.831571	50.836020
3501.135234	414858.033464	50.841025
3500.854230	413971.626644	50.846029
3501.137638	413071.940084	50.851034
3500.779140	412166.999499	50.856039
3501.099317	411219.123610	50.861044
3501.129437	410273.446966	50.866049
3500.815416	409301.130133	50.871053
3501.032375	408302.122560	50.876058
3500.827708	407285.701791	50.881063
3500.788108	406247.626013	50.886068
3500.656374	405197.512443	50.891073
3500.296624	404110.516365	50.896077
3500.604016	403009.468996	50.901082
3500.289576	401911.024357	50.906087
3500.123134	400764.168900	50.911092
3499.941128	399622.274092	50.916097
3499.668424	398456.366256	50.921101
3499.846247	397261.777272	50.926106
3499.674332	396063.108037	50.931111
3499.568069	394820.853534	50.936116
3499.023091	393578.951808	50.941121
3499.125712	392317.931189	50.946125
3499.017433	391032.676128	50.951130
3498.417395	389738.937139	50.956135
3498.604467	388416.316642	50.961140
3498.698806	387073.424942	50.966145
3498.018760	385715.002140	50.971149
3498.199657	384345.546020	50.976154
3497.904307	382967.648047	50.981159
3497.717468	381551.162166	50.986164
3497.368929	380126.431458	50.991169
3497.237247	378683.578167	50.996173
3497.185616	377218.785204	51.001178
3496.719575	375746.321425	51.006183
3496.712091	374252.562323	51.011188
3496.761887	372744.566648	51.016193
3496.446320	371220.600245	51.021197
3496.220811	369679.465305	51.026202
3496.018589	368124.299729	51.031207
3496.032112	366531.114307	51.036212
3495.780564	364941.567786	51.041217
3495.423269	363342.994410	51.046221
3495.258721	361703.016872	51.051226
3495.134611	360064.845215	51.056231
3494.799851	358407.335602	51.061236
3494.925063	356721.443872	51.066241
3494.656790	355032.166262	51.071245
3494.461961	353322.786721	51.076250
3493.711164	351600.382056	51.081255
3493.801287	349863.466789	51.086260
3493.486863	348109.556307	51.091265
3492.980648	346337.163323	51.096269
3493.122013	344537.670829	51.101274
3492.832274	342746.731629	51.106279
3492.526697	340925.243099	51.111284
3492.483925	339096.999425	51.116289
3492.171740	337259.089398	51.121293
3492.159375	335387.087231	51.126298
3491.140950	333512.669639	51.131303
3491.040881	331625.583613	51.136308
3491.046289	329738.134099	51.141313
3490.363737	327825.362213	51.146317
3490.356117	325897.241084	51.151322
3490.319457	323966.083635	51.156327
3489.951566	322014.404582	51.161332
3489.608449	320044.484914	51.166337
3489.210619	318061.760585	51.171341
3488.824459	316066.602863	51.176346
3488.437688	314071.412665	51.181351
3487.873869	312059.623085	51.186356
3488.087587	310029.518708	51.191361
3487.526729	308003.158843	51.196365
3487.283635	305934.428432	51.201370
3487.044317	303871.756288	51.206375
3486.499521	301792.384059	51.211380
3486.110893	299703.134228	51.216385
3485.959313	297606.897321	51.221389
3486.039537	295493.643442	51.226394
3485.161392	293369.331942	51.231399
3484.804235	291230.528825	51.236404
3484.373475	289093.838447	51.241409
3483.918585	286942.447768	51.246413
3484.051733	284759.548460	51.251418
3483.030512	282585.624585	51.256423
3482.945957	280402.699205	51.261428
3482.260885	278208.846878	51.266433
3481.949335	276005.686132	51.271437
3482.270589	273789.380375	51.276442
3481.521893	271565.927374	51.281447
3481.249782	269318.104051	51.286452
3480.745185	267065.873154	51.291457
3480.175357	264811.577347	51.296461
3479.758690	262537.558201	51.301466
3479.346036	260264.345673	51.306471
3479.076646	257973.658179	51.311476
3478.834031	255676.393384	51.316481
3477.639066	253372.925201	51.321485
3477.309698	251057.903497	51.326490
3476.753355	248742.239997	51.331495
3475.996926	246410.677897	51.336500
3475.512274	244083.132103	51.341505
3475.374144	241748.565423	51.346509
3475.039480	239408.067092	51.351514
3474.763995	237066.435469	51.356519
3473.973459	234698.865350	51.361524
3473.518796	232332.235409	51.366529
3472.838821	229953.657026	51.371533
3472.432281	227569.695365	51.376538
3472.070219	225184.340193	51.381543
3471.460902	222791.227633	51.386548
3470.995045	220382.604588	51.391553
3470.522419	217978.719163	51.396557
3470.045210	215560.909709	51.401562
3469.166729	213144.704053	51.406567
3468.542358	210716.779001	51.411572
3468.236605	208287.796109	51.416577
3467.349027	205852.515184	51.421581
3467.373314	203416.286309	51.426586
3466.152174	200970.876518	51.431591
3465.992100	198514.929012	51.436596
3465.399234	196069.196349	51.441601
3464.267814	193615.663606	51.446605
3464.230241	191146.929123	51.451610
3463.220670	188680.290702	51.456615
3462.579713	186207.988807	51.461620
3462.046301	183745.178034	51.466625
3461.190255	181267.438102	51.471629
3461.302686	178793.590415	51.476634
3459.668466	176313.693526	51.481639
3459.396475	173831.394447	51.486644
3459.043624	171350.836902	51.491649
3458.299573	168870.779729	51.496653
3457.534889	166379.256044	51.501658
3456.588075	163898.954760	51.506663
3455.359358	161405.408765	51.511668
3455.134847	158914.710629	51.516673
3453.869558	156439.460815	51.521677
3453.353668	153956.437230	51.526682
3452.237852	151485.306985	51.531687
3451.841671	148999.231399	51.536692
3451.488594	146505.987285	51.541697
3450.443883	143975.902862	51.546701
3449.590940	141501.024435	51.551706
3448.889246	139019.008563	51.556711
3448.129227	136542.163122	51.561716
3447.380143	134081.435608	51.566721
3446.219753	131614.579869	51.571725
3445.494756	129146.501825	51.576730
3444.771705	126688.246382	51.581735
3443.827532	124222.978353	51.586740
3442.945454	121769.433976	51.591745
3441.644220	119319.743100	51.596749
3440.786342	116872.719445	51.601754
3439.667059	114438.940638	51.606759
3438.500404	112012.692784	51.611764
3437.766384	109598.797927	51.616769
3436.916731	107193.032219	51.621773
3435.994977	104784.278626	51.626778
3434.967900	102396.112915	51.631783
3433.869908	100000.888033	51.636788
3432.777104	97610.910275	51.641793
3431.424246	95255.675983	51.646797
3430.467621	92879.448681	51.651802
3429.070336	90533.227719	51.656807
3427.852662	88201.800829	51.661812
3426.915862	85877.606201	51.666817
3425.349215	83576.050772	51.671821
3424.153396	81277.277438	51.676826
3423.028670	79010.515039	51.681831
3422.008557	76745.855813	51.686836
3420.488138	74495.580519	51.691841
3418.906012	72257.285833	51.696845
3417.598999	70042.103419	51.701850
3415.935938	67862.289224	51.706855
3414.318584	65687.366395	51.711860
3413.042546	63534.423510	51.716865
3411.457461	61416.787174	51.721869
3410.057783	59296.629494	51.726874
3408.184173	57209.725599	51.731879
3406.424624	55167.713065	51.736884
3405.051692	53133.494435	51.741889
3402.982775	51140.115850	51.746893
3401.269540	49152.128809	51.751898
3399.750880	47218.830790	51.756903
3397.968757	45305.990130	51.761908
3395.681702	43417.993589	51.766913
3393.284075	41576.584741	51.771917
3391.596234	39772.334268	51.776922
3388.973003	38019.113437	51.781927
3385.414924	36324.333270	51.786932
3379.899825	34723.495782	51.791937
3374.215481	33209.459828	51.796941
3369.193436	31762.538695	51.801946
3364.396878	30429.602789	51.806951
3359.426531	29166.800868	51.811956
3355.647714	28010.277118	51.816961
3351.115445	26936.769875	51.821965
3347.268664	25943.570516	51.826970
3343.916226	25041.359377	51.831975
3340.677668	24205.786058	51.836980
3337.311335	23439.007442	51.841985
3334.662227	22755.805133	51.846989
3331.790239	22114.245922	51.851994
3329.415793	21567.819462	51.856999
3327.387824	21045.016218	51.862004
3325.443685	20584.389361	51.867009
3323.070943	20176.085762	51.872013
3321.499638	19800.577129	51.877018
3319.789269	19480.243068	51.882023
3318.826942	19189.426505	51.887028
3317.152421	18928.305813	51.892033
3315.736013	18705.927864	51.897037
3315.111342	18500.308902	51.902042
3314.131399	18319.056053	51.907047
3312.898145	18148.241280	51.912052
3312.293249	17997.463096	51.917057
3311.351884	17879.417072	51.922061
3310.125760	17761.744549	51.927066
3309.303794	17669.875348	51.932071
3308.891273	17576.224905	51.937076
3308.106812	17499.277511	51.942081
3307.586002	17443.512835	51.947085
3307.602604	17379.241472	51.952090
3306.812960	17325.155863	51.957095
3306.557622	17267.920732	51.962100
3306.110881	17210.152646	51.967105
3305.443585	17177.762147	51.972109
3305.392481	17125.099982	51.977114
3305.102531	17089.985097	51.982119
3304.595697	17045.340207	51.987124
3304.532612	16992.897039	51.992129
3303.809807	16944.514947	51.997133
3303.614147	16896.645132	52.002138
3303.178222	16864.565015	52.007143
3302.658111	16810.697395	52.012148
3302.595753	16760.089835	52.017153
3302.036534	16722.437549	52.022157
3302.019874	16660.632340	52.027162
3301.605078	16607.305308	52.032167
3301.361881	16551.251196	52.037172
3301.066200	16486.353816	52.042177
3300.496131	16427.651709	52.047181
3300.413869	16353.401334	52.052186
3299.534200	16276.317773	52.057191
3299.128487	16208.258748	52.062196
3298.853419	16136.917165	52.067201
3298.367301	16073.955227	52.072205
3297.596087	15982.878422	52.077210
3297.173200	15907.589796	52.082215
3296.676134	15848.180276	52.087220
3296.483716	15770.305218	52.092225
3295.695708	15693.275070	52.097229
3295.413986	15607.243618	52.102234
3294.636378	15536.635261	52.107239
3294.397226	15451.319591	52.112244
3294.096623	15343.034262	52.117249
3292.991745	15265.192587	52.122253
3292.588589	15171.437052	52.127258
3291.754169	15089.763400	52.132263
3291.463551	14997.332940	52.137268
3291.173366	14910.442071	52.142273
3290.082584	14820.725268	52.147277
3289.871387	14735.125610	52.152282
3289.210361	14647.028875	52.157287
3288.587269	14557.867311	52.162292
3287.778314	14467.310951	52.167297
3287.112764	14385.103057	52.172301
3286.992396	14285.461815	52.177306
3286.098790	14192.103748	52.182311
3285.627697	14098.282121	52.187316
3284.914928	14013.946015	52.192321
3284.244748	13922.142638	52.197325
3284.366165	13822.309589	52.202330
3283.459252	13725.334487	52.207335
3282.612723	13627.515274	52.212340
3281.749185	13535.911417	52.217345
3281.094409	13438.719520	52.222349
3280.370149	13340.198468	52.227354
3279.817430	13254.009018	52.232359
3279.194097	13154.831851	52.237364
3278.460714	13064.276586	52.242369
3277.816691	12962.876051	52.247373
3277.555533	12878.993209	52.252378
3276.643783	12783.859038	52.257383
3276.119233	12694.458407	52.262388
3275.098281	12601.780531	52.267393
3274.529322	12517.076718	52.272397
3274.125625	12425.517407	52.277402
3273.497472	12339.546304	52.282407
3272.643298	12245.885975	52.287412
3272.163172	12147.226067	52.292417
3271.455596	12072.387473	52.297421
3270.872926	11970.984151	52.302426
3270.506163	11884.117536	52.307431
3269.502334	11784.130375	52.312436
3268.662687	11692.614863	52.317441
3268.157966	11600.266845	52.322445
3268.076998	11518.550098	52.327450
3267.414798	11429.754998	52.332455
3266.693087	11319.635603	52.337460
3266.411834	11220.914113	52.342465
3265.472859	11136.151081	52.347469
3265.147027	11024.125349	52.352474
3264.086743	10933.438608	52.357479
3263.168556	10839.038871	52.362484
3263.061568	10741.330123	52.367489
3261.897866	10645.660502	52.372493
3261.224728	10550.327901	52.377498
3260.539514	10457.650624	52.382503
3259.622683	10369.375607	52.387508
3259.416024	10271.098969	52.392513
3258.232680	10180.775540	52.397517
3257.963831	10100.447214	52.402522
3257.249968	10006.210143	52.407527
3256.493605	9917.041228	52.412532
3256.102355	9822.666371	52.417537
3255.328328	9737.447972	52.422541
3254.702690	9645.817326	52.427546
3254.416487	9554.955467	52.432551
3253.511359	9460.733695	52.437556
3253.143101	9364.458610	52.442561
3252.197995	9270.838783	52.447565
3251.811850	9180.481096	52.452570
3250.810396	9089.775627	52.457575
3250.421309	8995.078190	52.462580
3249.974656	8896.329528	52.467585
3249.417169	8815.889405	52.472589
3248.874108	8711.311607	52.477594
3247.883346	8614.862962	52.482599
3246.994769	8515.501768	52.487604
3246.778036	8414.263426	52.492609
3245.828388	8314.539504	52.497613
3245.346735	8222.227245	52.502618
3244.312086	8129.391533	52.507623
3243.115562	8039.962978	52.512628
3243.193885	7947.056653	52.517633
3242.548782	7859.887835	52.522637
3241.518551	7767.555789	52.527642
3240.924571	7681.819859	52.532647
3240.661687	7591.196455	52.537652
3239.873321	7503.039117	52.542657
3238.789928	7411.417977	52.547661
3238.195095	7311.345042	52.552666
3237.805119	7229.776099	52.557671
3236.749865	7141.827456	52.562676
3236.122247	7047.434136	52.567681
3235.442175	6975.152748	52.572685
3234.792127	6878.897963	52.577690
3234.455154	6800.478937	52.582695
3233.698853	6712.673490	52.587700
3233.388374	6612.695327	52.592705
3232.224909	6537.176690	52.597709
3231.642236	6436.314984	52.602714
3230.865135	6349.731322	52.607719
3230.053876	6266.992991	52.612724
3229.555172	6181.680787	52.617729
3228.793282	6105.636733	52.622733
3228.514704	6011.444178	52.627738
3227.914617	5932.425963	52.632743
3227.299808	5848.661945	52.637748
3226.932189	5747.601990	52.642753
3225.632324	5667.607693	52.647757
3225.123631	5569.419947	52.652762
3224.564655	5482.561269	52.657767
3223.959164	5402.298047	52.662772
3223.176671	5314.810366	52.667777
3222.500499	5229.854183	52.672781
3221.903058	5134.471949	52.677786
3221.409466	5055.793665	52.682791
3220.804840	4971.305195	52.687796
3219.916534	4890.976779	52.692801
3219.321340	4804.589950	52.697805
3218.506288	4709.103716	52.702810
3218.227356	4621.343498	52.707815
3216.990252	4535.656106	52.712820
3216.611188	4453.929666	52.717825
3215.590252	4375.450654	52.722829
3215.177498	4280.894032	52.727834
3214.231505	4200.016723	52.732839
3213.510053	4128.314368	52.737844
3213.020337	4045.429188	52.742849
3212.166483	3965.433588	52.747853
3212.155288	3878.441907	52.752858
3211.442359	3806.224705	52.757863
3210.178528	3719.714799	52.762868
3209.717179	3642.750717	52.767873
3208.992372	3558.235019	52.772877
3208.265534	3470.283682	52.777882
3207.463785	3397.088597	52.782887
3206.749085	3335.078883	52.787892
3206.382376	3247.705266	52.792897
3205.602517	3172.317889	52.797901
3205.051826	3095.165646	52.802906
3204.923324	3018.404355	52.807911
3203.829118	2942.519059	52.812916
3203.526191	2859.218113	52.817921
3202.780894	2773.198043	52.822925
3201.928351	2685.426518	52.827930
3200.919561	2607.739834	52.832935
3200.101263	2533.272461	52.837940
3199.751260	2456.946528	52.842945
3198.764092	2383.832035	52.847949
3198.121528	2311.485681	52.852954
3197.543495	2242.558487	52.857959
3196.605614	2170.227706	52.862964
3196.254341	2094.696460	52.867969
3195.229208	2031.228966	52.872973
3194.497804	1957.616397	52.877978
3194.031244	1899.205010	52.882983
3193.342076	1831.833476	52.887988
3192.876819	1753.692591	52.892993
3191.963700	1700.095458	52.897997
3191.580320	1625.160153	52.903002
3190.932926	1544.693888	52.908007
3190.132686	1491.328463	52.913012
3189.340175	1420.393493	52.918017
3188.286135	1356.956167	52.923021
3188.090051	1285.342378	52.928026
3187.498204	1229.249213	52.933031
3186.365140	1169.713696	52.938036
3185.768303	1097.401831	52.943041
3185.059676	1042.290903	52.948045
3184.144349	984.929492	52.953050
3183.530063	930.105218	52.958055
3183.005005	867.665056	52.963060
3182.385240	810.720377	52.968065
3181.311389	765.792102	52.973069
3180.768659	720.524528	52.978074
3180.027882	666.744777	52.983079
3179.247138	621.061835	52.988084
3178.973018	550.720797	52.993089
3177.979965	511.788154	52.998093
3177.220996	463.593005	53.003098
3176.429110	409.719450	53.008103
3175.769427	374.026624	53.013108
3175.056695	322.426145	53.018113
3174.068943	285.431694	53.023117
3173.502739	244.645764	53.028122
3172.856418	213.811732	53.033127
3171.550299	190.646784	53.038132
3171.434488	147.327761	53.043137
3168.556812	155.863581	53.048141
3167.156030	166.690309	53.053146
3166.467837	159.580416	53.058151
3165.874986	165.882494	53.063156
3165.640527	163.209586	53.068161
3165.005389	164.184926	53.073165
3164.812625	166.764254	53.078170
3164.312640	164.002504	53.083175
3163.315069	170.968587	53.088180
3162.884302	159.620329	53.093185
3161.742807	165.543654	53.098189
3161.377620	176.044247	53.103194
3161.145542	165.536362	53.108199
3160.270242	177.547896	53.113204
3160.153502	157.968002	53.118209
3159.075217	161.165588	53.123213
3158.684946	164.715350	53.128218
3157.778271	164.005411	53.133223
3156.767222	167.819128	53.138228
3156.388542	164.566532	53.143233
3155.935885	169.302850	53.148237
3155.312810	167.198039	53.153242
3154.578347	160.532228	53.158247
3153.976003	164.817683	53.163252
3153.333304	158.571975	53.168257
3152.840782	166.215170	53.173261
3152.102770	167.546765	53.178266
3151.888943	169.151950	53.183271
3150.788645	170.093085	53.188276
3149.860693	160.623027	53.193281
3149.059353	168.489509	53.198285
3148.596985	170.209394	53.203290
3148.760564	155.489271	53.208295
3148.079685	166.716806	53.213300
3147.169452	160.882326	53.218305
3145.951093	160.413533	53.223309
3145.323890	157.280768	53.228314
3144.626375	160.501718	53.233319
3143.929427	175.084430	53.238324
3143.756234	172.963937	53.243329
3143.004705	167.623776	53.248333
3142.497131	161.133539	53.253338
3142.159801	161.406303	53.258343
3141.407923	163.772087	53.263348
3140.479108	163.984071	53.268353
3139.261968	166.944075	53.273357
3138.637193	159.023238	53.278362
3138.079478	165.807986	53.283367
3137.573754	164.514819	53.288372
3137.317317	157.401821	53.293377
3136.581682	158.314993	53.298381
3135.968304	158.224800	53.303386
3135.422005	154.727301	53.308391
3134.511217	156.662351	53.313396
3134.035355	157.539824	53.318401
3133.236033	153.812010	53.323405
3132.857335	159.939341	53.328410
3131.997408	155.036514	53.333415
3131.156059	159.616614	53.338420
3130.791497	154.105346	53.343425
3129.850870	161.213669	53.348429
3129.430832	154.081652	53.353434
3128.850026	158.264745	53.358439
3128.461310	164.598654	53.363444
3127.894316	155.024301	53.368449
3126.828241	161.975641	53.373453
3125.762382	156.719982	53.378458
3125.026820	157.912611	53.383463
3124.510600	157.751345	53.388468
3124.055081	152.273777	53.393473
3123.032394	166.488593	53.398477
3122.963421	163.831228	53.403482
3122.974919	157.499407	53.408487
3121.657549	164.590394	53.413492
3121.225474	154.874966	53.418497
3119.733377	158.948111	53.423501
3118.875021	159.894096	53.428506
3118.989705	159.771873	53.433511
3118.342992	165.481589	53.438516
3117.450527	156.549414	53.443521
3116.976676	161.281852	53.448525
3116.297891	157.775018	53.453530
3116.443962	153.256480	53.458535
3115.079979	165.399265	53.463540
3114.395658	155.141950	53.468545
3113.409862	161.747214	53.473549
3112.716999	150.597304	53.478554
3112.477740	150.243853	53.483559
3111.879633	158.400863	53.488564
3111.404295	155.634910	53.493569
3110.791713	159.505677	53.498573
3109.832666	157.693930	53.503578
3109.094655	154.545368	53.508583
3108.132049	157.323730	53.513588
3107.216801	149.431220	53.518593
3107.389047	157.035431	53.523597
3106.414375	162.311720	53.528602
3106.295526	153.472362	53.533607
3105.415038	163.773628	53.538612
3104.451951	153.627894	53.543617
3103.379372	153.361170	53.548621
3102.894917	154.178535	53.553626
3102.916308	146.537297	53.558631
3102.009540	159.383517	53.563636
3101.722396	154.567166	53.568641
3100.701189	163.456062	53.573645
3099.846761	147.826759	53.578650
3099.078977	155.805923	53.583655
3097.873208	161.465112	53.588660
3098.010273	155.100786	53.593665
3097.644864	152.921170	53.598669
3096.801151	156.091314	53.603674
3096.471188	155.093377	53.608679
3095.415483	158.965650	53.613684
3094.762313	149.168406	53.618689
3093.750506	155.431543	53.623693
3092.972457	156.361441	53.628698
3092.961445	152.702619	53.633703
3091.909308	151.524531	53.638708
3091.787649	147.120029	53.643713
3091.371548	148.641752	53.648717
3089.865880	154.725594	53.653722
3089.604981	151.863005	53.658727
3088.975583	153.467751	53.663732
3088.187481	155.000933	53.668737
3087.399271	153.446967	53.673741
3086.663930	150.125063	53.678746
3086.222056	147.068008	53.683751
3085.238854	159.725978	53.688756
3084.423047	148.217355	53.693761
3084.071507	146.231156	53.698765
3083.880171	155.071012	53.703770
3083.750353	146.262350	53.708775
3082.135385	158.938663	53.713780
3081.455323	157.710422	53.718785
3081.018940	152.051963	53.723789
3080.363875	160.018185	53.728794
3080.134387	144.267506	53.733799
3079.185719	161.316445	53.738804
3078.491954	141.294015	53.743809
3078.070870	154.641045	53.748813
3076.540690	151.282459	53.753818
3076.095917	151.350563	53.758823
3075.243297	161.153657	53.763828
3074.616806	155.981223	53.768833
3073.993692	159.046968	53.773837
3073.447293	153.192576	53.778842
3073.516756	155.433813	53.783847
3072.612993	154.646419	53.788852
3071.675341	155.221890	53.793857
3071.171042	155.610422	53.798861
3070.061637	150.349588	53.803866
3069.398787	146.065981	53.808871
3068.598905	156.611227	53.813876
3067.978036	154.674601	53.818881
3067.605183	153.762940	53.823885
3067.154370	152.101591	53.828890
3067.061808	144.994552	53.833895
3065.486851	153.269923	53.838900
3065.047693	152.031705	53.843905
3064.783872	149.087119	53.848909
3064.071671	150.400497	53.853914
3063.167431	150.075807	53.858919
3062.714942	155.204058	53.863924
3062.215074	152.983474	53.868929
3060.606883	154.680471	53.873933
3060.154687	149.767200	53.878938
3060.259747	150.496864	53.883943
3059.650112	155.678414	53.888948
3058.827886	145.427315	53.893953
3058.404570	148.867068	53.898957
3056.824628	151.446981	53.903962
3056.216173	149.809413	53.908967
3055.725839	154.173623	53.913972
3055.290448	149.540500	53.918977
3054.608962	148.657104	53.923981
3053.695493	151.959958	53.928986
3053.113746	148.785100	53.933991
3052.625138	162.594847	53.938996
3052.172701	147.165286	53.944001
3051.111802	155.357559	53.949005
3050.244163	153.886249	53.954010
3050.694547	149.977673	53.959015
3049.707859	155.319965	53.964020
3049.299348	139.126215	53.969025
3048.311134	153.629202	53.974029
3047.675198	156.708193	53.979034
3047.112119	151.978076	53.984039
3046.319032	159.038299	53.989044
3045.656994	152.342770	53.994049
3044.467310	146.171605	53.999053
3043.592403	151.361378	54.004058
3043.149616	148.533031	54.009063
3042.230640	162.541050	54.014068
3041.916209	146.450820	54.019073
3041.380294	154.641017	54.024077
3040.753400	154.638799	54.029082
3040.105640	135.292196	54.034087
3039.413815	135.499621	54.039092
3038.726360	144.719103	54.044097
3038.044881	141.142484	54.049101
3037.545607	142.513820	54.054106
3037.135215	141.907780	54.059111
3035.941551	146.892289	54.064116
3035.731173	139.064090	54.069121
3035.548816	145.927189	54.074125
3034.469108	147.423364	54.079130
3033.648415	147.871094	54.084135
3032.868999	155.952114	54.089140
3032.560810	141.173690	54.094145
3031.644964	137.487519	54.099149
3031.138877	142.856236	54.104154
3030.545658	142.837607	54.109159
3029.756327	141.866461	54.114164
3029.361425	144.025995	54.119169
3028.557787	139.992238	54.124173
3026.946563	142.792233	54.129178
3027.074415	143.639972	54.134183
3026.351773	145.186447	54.139188
3026.044787	144.555238	54.144193
3024.701920	147.134515	54.149197
3024.275604	151.160163	54.154202
3023.978509	144.663985	54.159207
3022.344695	142.512833	54.164212
3022.362104	139.592432	54.169217
3021.974650	140.909925	54.174221
3021.118644	149.682961	54.179226
3020.598361	141.437598	54.184231
3019.412469	134.634627	54.189236
3019.067861	133.718144	54.194241
3018.678334	136.883314	54.199245
3017.467800	138.131063	54.204250
3017.053508	136.171383	54.209255
3016.786691	144.213357	54.214260
3015.403634	139.082590	54.219265
3015.128825	138.399700	54.224269
3014.236257	136.358330	54.229274
3014.404503	133.129926	54.234279
3012.958146	136.678574	54.239284
3012.188222	138.316417	54.244289
3011.499349	140.059618	54.249293
3011.424269	141.505308	54.254298
3010.691917	131.642679	54.259303
3009.464368	143.605832	54.264308
3009.109460	142.043757	54.269313
3008.670139	137.661572	54.274317
3007.842094	146.156678	54.279322
3007.307330	145.417554	54.284327
3006.586616	148.060254	54.289332
3006.047242	135.264982	54.294337
3005.562220	140.721676	54.299341
3005.087286	132.685276	54.304346
3004.492985	138.005910	54.309351
3003.474303	144.477458	54.314356
3002.469404	139.189708	54.319361
3001.774702	142.653337	54.324365
3001.118124	143.866823	54.329370
3001.083553	134.728883	54.334375
2999.917621	136.440713	54.339380
2999.242237	135.228659	54.344385
2998.578159	148.142740	54.349389
2997.965494	147.949021	54.354394
2997.614656	133.088690	54.359399
2996.583685	146.024413	54.364404
2995.868134	132.602030	54.369409
2995.821831	139.289511	54.374413
2995.113320	137.504843	54.379418
2994.631121	143.770641	54.384423
2993.245867	144.321165	54.389428
2992.343892	142.196934	54.394433
2992.310577	141.740403	54.399437
2991.458078	148.160662	54.404442
2990.527943	132.396719	54.409447
2989.536068	137.587929	54.414452
2989.714318	137.401553	54.419457
2988.984001	144.110003	54.424461
2987.772008	142.148089	54.429466
2987.283382	138.646679	54.434471
2986.552924	137.283383	54.439476
2986.190865	134.573483	54.444481
2985.591214	138.482700	54.449485
2984.800891	137.170687	54.454490
2984.412562	134.390672	54.459495
2983.819040	137.323077	54.464500
2983.426205	131.770089	54.469505
2982.740264	132.641235	54.474509
2981.392664	138.932154	54.479514
2980.718074	128.638489	54.484519
2979.624827	134.338062	54.489524
2979.481968	132.702650	54.494529
2979.518436	140.125177	54.499533
2977.497421	134.540559	54.504538
2977.946401	127.789009	54.509543
2976.858990	135.249644	54.514548
2976.314154	127.925837	54.519553
2975.597986	131.339451	54.524557
2974.656837	139.050613	54.529562
2974.351343	133.513094	54.534567
2973.857680	138.507856	54.539572
2973.725056	128.369467	54.544577
2972.940609	131.411075	54.549581
2971.703057	134.308277	54.554586
2970.834985	131.582220	54.559591
2969.515824	142.432507	54.564596
2968.895892	128.483808	54.569601
2969.378463	133.954753	54.574605
2968.716060	138.298236	54.579610
2967.916084	134.625435	54.584615
2966.686098	137.825680	54.589620
2966.212515	135.373649	54.594625
2966.023115	135.751008	54.599629
2965.090005	134.605894	54.604634
2964.984028	125.766342	54.609639
2964.136514	127.091799	54.614644
2962.584085	120.214518	54.619649
2962.004786	135.221543	54.624653
2961.865324	137.573080	54.629658
2961.255527	136.947833	54.634663
2959.994830	131.572759	54.639668
2959.229767	133.318722	54.644673
2959.375558	137.026344	54.649677
2958.218494	139.672959	54.654682
2958.039964	133.518497	54.659687
2956.931039	140.543482	54.664692
2956.456750	135.127965	54.669697
2955.962019	135.135539	54.674701
2955.713180	138.193381	54.679706
2955.234086	130.298224	54.684711
2953.654987	141.803575	54.689716
2952.555659	135.787915	54.694721
2952.783031	141.029320	54.699725
2951.878649	140.066004	54.704730
2951.178931	132.685379	54.709735
2950.372657	142.243711	54.714740
2949.597361	141.487277	54.719745
2948.955397	133.677978	54.724749
2948.177267	139.338705	54.729754
2947.828355	128.372041	54.734759
2947.329053	140.545869	54.739764
2947.253647	132.759354	54.744769
2946.670267	127.980230	54.749773
2945.664858	136.761426	54.754778
2944.127236	132.406286	54.759783
2943.482644	140.322161	54.764788
2943.100390	129.927627	54.769793
2942.965999	117.942231	54.774797
2942.210884	130.752647	54.779802
2941.909340	125.167881	54.784807
2941.206185	131.672350	54.789812
2940.236322	132.367026	54.794817
2939.075997	129.220800	54.799821
2937.620080	134.261190	54.804826
2938.300903	123.032507	54.809831
2937.491007	136.368591	54.814836
2936.680361	128.878246	54.819841
2935.987365	127.341982	54.824845
2935.053477	140.448212	54.829850
2934.890388	132.736681	54.834855
2934.066495	137.034739	54.839860
2933.788975	131.843356	54.844865
2933.547768	130.540929	54.849869
2931.995051	137.320844	54.854874
2931.184952	127.734410	54.859879
2930.498681	133.938766	54.864884
2929.995238	130.973173	54.869889
2929.463729	130.993349	54.874893
2928.974480	132.074434	54.879898
2928.512322	129.209151	54.884903
2928.211377	132.022482	54.889908
2926.988139	134.975270	54.894913
2925.852291	138.146014	54.899917
2924.793271	130.686670	54.904922
2924.512955	129.426058	54.909927
2923.821323	131.746828	54.914932
2923.228270	129.363771	54.919937
2923.202034	131.215970	54.924941
2922.208893	131.028466	54.929946
2921.850472	134.050957	54.934951
2920.994783	130.308347	54.939956
2920.733635	127.512132	54.944961
2920.009694	124.947765	54.949965
2918.440562	136.423783	54.954970
2917.818594	128.084905	54.959975
2917.265960	131.199400	54.964980
2916.620942	132.571967	54.969985
2916.427088	129.518337	54.974989
2915.845702	130.807005	54.979994
2915.064893	126.407407	54.984999
2914.626862	138.290900	54.990004
2913.839224	132.041200	54.995009
2913.146488	126.003831	55.000013
2911.833115	130.944077	55.005018
2911.458054	130.247143	55.010023
2910.832649	126.499917	55.015028
2910.544212	129.277164	55.020033
2909.936913	130.316057	55.025037
2909.096383	135.573382	55.030042
2908.843301	126.113204	55.035047
2907.518944	133.422897	55.040052
2906.676955	131.307773	55.045057
2906.297000	130.393392	55.050061
2904.954640	127.909450	55.055066
2905.417939	131.265973	55.060071
2904.400687	133.904096	55.065076
2903.837998	130.184046	55.070081
2903.217344	124.806579	55.075085
2902.602724	134.696092	55.080090
2902.543057	128.144755	55.085095
2901.166224	126.520105	55.090100
2900.097078	132.489902	55.095105
2899.435687	131.097054	55.100109
2898.383091	138.037420	55.105114
2898.270293	131.130436	55.110119
2897.461536	133.551749	55.115124
2897.252983	131.812703	55.120129
2896.851393	134.095355	55.125133
2896.195555	130.323727	55.130138
2896.267203	126.717107	55.135143
2894.596173	133.756846	55.140148
2893.662266	134.659721	55.145153
2893.259523	130.403930	55.150157
2892.563484	130.293943	55.155162
2892.093615	126.715923	55.160167
2890.915067	123.956102	55.165172
2890.034469	131.804942	55.170177
2890.234942	126.605691	55.175181
2889.173365	122.173163	55.180186
2888.023033	117.686333	55.185191
2887.787148	123.208996	55.190196
2887.266352	127.343549	55.195201
2886.544428	119.633195	55.200205
2885.649047	132.501529	55.205210
2885.535513	126.558989	55.210215
2884.816128	129.489621	55.215220
2884.374463	130.873621	55.220225
2883.683054	127.864369	55.225229
2883.083480	133.593266	55.230234
2882.421935	120.969304	55.235239
2881.001697	131.313066	55.240244
2880.063366	133.648371	55.245249
2879.871871	124.962783	55.250253
2879.161981	130.619350	55.255258
2878.442598	125.449019	55.260263
2877.747895	131.203251	55.265268
2876.969732	125.952967	55.270273
2876.808551	124.374375	55.275277
2875.944348	127.160024	55.280282
2875.626687	136.064471	55.285287
2875.190814	125.612407	55.290292
2874.541672	126.122416	55.295297
2873.346671	120.146817	55.300301
2872.384895	136.587324	55.305306
2872.003958	124.898274	55.310311
2871.143495	127.254612	55.315316
2870.868914	126.207360	55.320321
2870.725643	125.640547	55.325325
2869.743760	122.138589	55.330330
2868.517789	124.089249	55.335335
2867.979385	128.953503	55.340340
2867.201270	124.828973	55.345345
2866.658125	127.609094	55.350349
2866.010364	132.087050	55.355354
2866.018363	123.071721	55.360359
2865.114879	127.699166	55.365364
2863.683818	130.068158	55.370369
2863.222259	119.698646	55.375373
2862.533248	126.832655	55.380378
2861.737246	123.002886	55.385383
2861.464632	120.946379	55.390388
2861.141061	125.013674	55.395393
2860.779420	121.534791	55.400397
2859.555580	136.120664	55.405402
2859.520076	130.230314	55.410407
2857.826758	134.101063	55.415412
2857.199271	136.209173	55.420417
2856.677125	122.992197	55.425421
2855.741642	127.533141	55.430426
2855.533110	117.369065	55.435431
2855.413745	123.054966	55.440436
2854.645531	122.058923	55.445441
2853.780696	117.005034	55.450445
2852.759173	124.080216	55.455450
2851.848610	119.357028	55.460455
2851.290130	125.592043	55.465460
2850.888739	122.348895	55.470465
2850.334242	125.969355	55.475469
2849.595489	129.812354	55.480474
2849.263786	117.441102	55.485479
2848.910325	120.793920	55.490484
2847.583708	111.482498	55.495489
2846.880970	117.540460	55.500493
2846.087901	128.231367	55.505498
2845.721156	117.564610	55.510503
2845.310283	118.294025	55.515508
2844.644888	120.645843	55.520513
2844.129042	114.851409	55.525517
2842.554376	125.380640	55.530522
2842.208281	115.478493	55.535527
2841.590922	121.345422	55.540532
2841.089771	123.550357	55.545537
2840.666507	122.413258	55.550541
2839.963456	118.248274	55.555546
2839.113925	113.525317	55.560551
2838.106441	126.607801	55.565556
2837.311741	123.559370	55.570561
2836.912255	121.864012	55.575565
2836.095044	119.749009	55.580570
2836.099809	109.778612	55.585575
2835.543007	117.280407	55.590580
2834.981295	117.585615	55.595585
2834.020058	110.884044	55.600589
2832.560291	119.522242	55.605594
2832.311700	115.121304	55.610599
2831.928334	123.659613	55.615604
2831.031736	121.018194	55.620609
2830.371294	118.703903	55.625613
2829.854101	125.741445	55.630618
2829.711727	124.350688	55.635623
2828.470156	120.393398	55.640628
2826.969951	117.827513	55.645633
2827.022362	116.820295	55.650637
2826.063629	124.764593	55.655642
2825.862420	117.379324	55.660647
2825.546388	117.918062	55.665652
2824.981163	124.402513	55.670657
2824.663701	126.460795	55.675661
2823.138719	120.821467	55.680666
2822.341684	118.799726	55.685671
2821.803457	127.815676	55.690676
2821.182735	122.124824	55.695681
2820.751045	118.044908	55.700685
2820.139635	129.961969	55.705690
2818.980833	117.783399	55.710695
2818.133732	115.210100	55.715700
2817.587485	120.780674	55.720705
2816.855532	113.207837	55.725709
2816.068947	124.340516	55.730714
2816.420825	115.028008	55.735719
2815.642733	117.523428	55.740724
2815.396139	116.472186	55.745729
2814.799216	119.475442	55.750733
2813.338120	124.000832	55.755738
2813.159224	119.418645	55.760743
2812.183493	115.165275	55.765748
2810.913589	122.268703	55.770753
2810.160900	119.157046	55.775757
2809.734357	119.349552	55.780762
2809.053780	111.550443	55.785767
2808.886474	116.735338	55.790772
2807.769484	114.809731	55.795777
2807.596236	103.956371	55.800781
2806.826929	122.302462	55.805786
2806.846409	120.121433	55.810791
2806.009037	117.522395	55.815796
2804.928444	109.423773	55.820801
2804.314458	120.439714	55.825805
2803.444569	121.592969	55.830810
2802.424371	118.928472	55.835815
2801.536090	118.852142	55.840820
2800.532844	118.650204	55.845825
2801.119799	111.196545	55.850829
2800.175852	118.881743	55.855834
2799.712136	113.798781	55.860839
2798.785139	119.715476	55.865844
2798.514552	121.226947	55.870849
2797.934119	108.267058	55.875853
2796.458733	113.008042	55.880858
2796.240636	114.347125	55.885863
2795.132915	116.862570	55.890868
2794.911974	115.033678	55.895873
2794.560879	109.258068	55.900877
2793.657505	112.267124	55.905882
2792.659448	118.898970	55.910887
2791.432247	114.665297	55.915892
2791.033978	128.016674	55.920897
2791.168565	122.816056	55.925901
2790.118979	117.294034	55.930906
2789.586660	112.937647	55.935911
2789.014900	105.577433	55.940916
2788.398850	120.771894	55.945921
2788.137874	112.946465	55.950925
2786.844975	124.882109	55.955930
2786.353519	115.375068	55.960935
2785.995842	121.710759	55.965940
2785.070139	126.904100	55.970945
2784.351886	121.685832	55.975949
2783.074564	121.765997	55.980954
2782.768253	120.526811	55.985959
2782.049447	119.899691	55.990964
2781.264643	123.340840	55.995969
2780.957284	123.530345	56.000973
2780.284700	126.862712	56.005978
2779.982772	127.119182	56.010983
2779.655481	128.082992	56.015988
2778.587757	120.055986	56.020993
2777.928592	113.637525	56.025997
2777.239919	125.265428	56.031002
2776.181010	121.301010	56.036007
2775.431079	116.328153	56.041012
2774.636954	116.859401	56.046017
2774.134508	119.009694	56.051021
2773.187485	121.309394	56.056026
2772.874641	117.146410	56.061031
2772.379574	126.822068	56.066036
2771.957501	114.839295	56.071041
2771.854040	110.321982	56.076045
2771.012806	121.118220	56.081050
2769.938054	117.473082	56.086055
2769.093017	114.045649	56.091060
2768.263862	115.339573	56.096065
2768.016828	112.119788	56.101069
2767.231406	115.281183	56.106074
2765.896911	109.646424	56.111079
2765.095195	113.608343	56.116084
2764.879401	120.778705	56.121089
2764.535795	115.446277	56.126093
2763.450636	115.917143	56.131098
2763.255630	114.354601	56.136103
2762.878063	117.397734	56.141108
2762.347060	120.589852	56.146113
2761.704367	107.831661	56.151117
2760.452111	118.769991	56.156122
2759.816672	112.101565	56.161127
2759.175243	116.624624	56.166132
2758.698630	117.413437	56.171137
2757.967803	113.348739	56.176141
2756.670418	117.589586	56.181146
2756.057401	116.960177	56.186151
2755.563583	116.515652	56.191156
2754.929228	113.593379	56.196161
2754.697053	104.467548	56.201165
2754.260341	111.310939	56.206170
2753.883534	107.213365	56.211175
2752.771660	115.573433	56.216180
2751.794343	121.335317	56.221185
2751.213463	112.680388	56.226189
2750.688041	123.234364	56.231194
2750.177721	116.111144	56.236199
2749.772867	115.342343	56.241204
2748.533670	114.576419	56.246209
2747.664524	113.192261	56.251213
2747.213850	116.014213	56.256218
2746.487088	109.594288	56.261223
2746.000376	117.115681	56.266228
2745.596390	118.783371	56.271233
2745.172796	108.543581	56.276237
2744.104647	114.131127	56.281242
2743.230207	109.255742	56.286247
2742.744020	109.653441	56.291252
2741.609767	113.812723	56.296257
2741.649648	106.560335	56.301261
2740.544205	111.621376	56.306266
2739.650010	107.116463	56.311271
2739.286865	117.150476	56.316276
2738.642865	112.179652	56.321281
2738.523126	112.520242	56.326285
2737.528827	117.622286	56.331290
2736.894998	111.717382	56.336295
2736.047658	118.662147	56.341300
2735.311094	114.642643	56.346305
2734.719000	109.885968	56.351309
2734.299711	115.919565	56.356314
2734.019481	113.155443	56.361319
2732.301473	113.980794	56.366324
2731.656549	120.523077	56.371329
2731.238314	112.939267	56.376333
2730.275122	123.308340	56.381338
2729.955240	107.320205	56.386343
2729.998533	118.301557	56.391348
2729.394595	123.063731	56.396353
2728.758403	122.404340	56.401357
2727.566306	117.123397	56.406362
2726.637723	121.898036	56.411367
2725.994385	125.252645	56.416372
2725.727910	119.547442	56.421377
2725.275063	109.808429	56.426381
2723.657222	124.944789	56.431386
2722.659085	118.421650	56.436391
2723.175008	114.859095	56.441396
2722.218601	118.096693	56.446401
2721.640327	112.455446	56.451405
2721.377138	119.336284	56.456410
2720.823175	119.126641	56.461415
2719.876612	112.179833	56.466420
2718.835002	117.590352	56.471425
2718.699180	109.971298	56.476429
2717.631868	120.035677	56.481434
2716.485109	114.757646	56.486439
2715.917398	110.693101	56.491444
2715.141706	120.722633	56.496449
2714.815374	109.671246	56.501453
2714.370969	114.811926	56.506458
2713.855843	107.151528	56.511463
2713.363915	109.857377	56.516468
2712.604020	118.235837	56.521473
2711.829152	113.060025	56.526477
2710.859047	115.843269	56.531482
2709.930424	117.547744	56.536487
2709.590097	111.459260	56.541492
2709.197979	118.178588	56.546497
2708.507383	116.180513	56.551501
2707.364277	118.939647	56.556506
2706.800111	114.908837	56.561511
2705.991316	112.410719	56.566516
2705.442951	108.986665	56.571521
2705.373043	105.698716	56.576525
2704.739734	112.817679	56.581530
2704.506305	110.073981	56.586535
2703.419170	106.731363	56.591540
2702.168173	110.149972	56.596545
2701.931088	108.236216	56.601549
2701.355330	116.104794	56.606554
2700.666122	115.295789	56.611559
2699.927202	119.599472	56.616564
2699.055475	113.841025	56.621569
2698.756779	108.904340	56.626573
2697.476032	115.187422	56.631578
2696.353024	115.548721	56.636583
2696.087893	114.694858	56.641588
2695.380885	115.531348	56.646593
2695.002032	106.420334	56.651597
2694.537037	114.871538	56.656602
2694.174876	109.727024	56.661607
2693.533380	116.791337	56.666612
2692.839127	118.143526	56.671617
2692.156646	105.075192	56.676621
2690.872856	115.221572	56.681626
2690.115340	120.129206	56.686631
2689.797308	118.669010	56.691636
2689.172164	119.343879	56.696641
2688.970727	117.398767	56.701645
2688.089697	115.085889	56.706650
2686.946632	112.276240	56.711655
2686.660845	108.774148	56.716660
2685.758330	113.350129	56.721665
2685.664785	105.581358	56.726669
2684.822607	108.780882	56.731674
2683.693667	108.815180	56.736679
2682.996688	103.462252	56.741684
2682.189091	115.227314	56.746689
2681.794414	112.740910	56.751693
2681.431737	118.164849	56.756698
2681.230521	110.860520	56.761703
2680.438862	105.474435	56.766708
2678.967489	117.020604	56.771713
2678.839531	113.943888	56.776717
2678.382504	117.207442	56.781722
2677.373463	114.720664	56.786727
2676.466327	107.513322	56.791732
2675.501981	110.288875	56.796737
2675.121171	106.640401	56.801741
2674.296328	120.045338	56.806746
2674.219259	113.647391	56.811751
2674.141249	114.364127	56.816756
2673.155056	115.969504	56.821761
2672.344217	115.319449	56.826765
2672.005845	114.820729	56.831770
2670.865194	107.360024	56.836775
2669.440165	112.986478	56.841780
2668.560772	110.439253	56.846785
2668.772458	102.861460	56.851789
2667.886735	108.121786	56.856794
2667.363493	109.210278	56.861799
2667.147187	104.966071	56.866804
2666.547175	107.161468	56.871809
2665.460082	99.040712	56.876813
2664.066583	111.391041	56.881818
2663.709888	107.638976	56.886823
2663.454627	97.749763	56.891828
2662.944282	113.601119	56.896833
2662.474083	110.717113	56.901837
2661.974265	112.897752	56.906842
2660.877518	104.492470	56.911847
2660.464211	108.526157	56.916852
2659.491510	115.144603	56.921857
2659.290230	108.296986	56.926861
2657.962529	112.017653	56.931866
2657.352904	116.146873	56.936871
2656.847429	119.607388	56.941876
2655.805343	114.060041	56.946881
2655.699202	110.613687	56.951885
2654.823780	120.992233	56.956890
2654.350267	114.546796	56.961895
2653.192139	107.563148	56.966900
2652.346627	116.026900	56.971905
2652.231861	114.601828	56.976909
2651.514782	114.201792	56.981914
2651.152137	109.100785	56.986919
2650.827692	110.141481	56.991924
2649.784838	112.632836	56.996929
2648.810636	111.531514	57.001933
2648.053150	120.215082	57.006938
2647.892982	114.465666	57.011943
2647.191170	102.169574	57.016948
2646.214156	115.422104	57.021953
2645.659210	109.716095	57.026957
2644.854884	115.131849	57.031962
2644.246543	109.091557	57.036967
2644.038935	111.530526	57.041972
2642.753754	102.980230	57.046977
2642.431559	103.558713	57.051981
2641.346544	106.467789	57.056986
2640.868064	114.259740	57.061991
2640.443433	98.306514	57.066996
2639.827175	104.606665	57.072001
2639.497147	105.523977	57.077005
2638.088632	110.037649	57.082010
2637.152663	108.126134	57.087015
2636.909132	99.365805	57.092020
2636.035479	111.578722	57.097025
2635.825385	103.175427	57.102029
2635.383283	106.562347	57.107034
2635.127038	98.708901	57.112039
2634.058233	103.765665	57.117044
2632.930144	106.208437	57.122049
2632.569239	101.285948	57.127053
2632.109526	99.684194	57.132058
2630.760565	100.642270	57.137063
2630.190632	101.300208	57.142068
2629.346652	98.821146	57.147073
2628.974813	97.639356	57.152077
2628.529456	102.407578	57.157082
2627.856173	105.320480	57.162087
2627.597206	102.743781	57.167092
2626.772603	106.014120	57.172097
2625.994557	104.712302	57.177101
2625.552115	107.023656	57.182106
2624.182549	104.665625	57.187111
2623.064891	98.375312	57.192116
2623.148348	108.248103	57.197121
2622.587657	105.173526	57.202125
2621.806465	108.012511	57.207130
2621.003775	101.514807	57.212135
2620.858026	99.946222	57.217140
2620.039575	99.951534	57.222145
2619.317742	96.375181	57.227149
2618.271356	110.811108	57.232154
2617.756368	108.694214	57.237159
2616.998042	103.561779	57.242164
2616.591650	105.219228	57.247169
2616.427138	97.317736	57.252173
2615.348446	94.604073	57.257178
2614.304352	99.426490	57.262183
2613.996750	102.821995	57.267188
2613.211854	113.599918	57.272193
2612.834798	96.652151	57.277197
2612.540395	104.258292	57.282202
2611.126451	108.358831	57.287207
2610.863632	100.117707	57.292212
2610.092871	108.994982	57.297217
2609.436558	111.310137	57.302221
2608.622750	110.851645	57.307226
2607.781852	115.215003	57.312231
2607.191616	111.810750	57.317236
2606.577024	110.709933	57.322241
2606.287334	108.103750	57.327245
2605.620842	115.789294	57.332250
2604.682272	115.620543	57.337255
2604.145190	114.705811	57.342260
2603.310520	111.614127	57.347265
2603.051524	103.932068	57.352269
2602.261680	108.630107	57.357274
2600.928067	115.076974	57.362279
2600.113651	109.907946	57.367284
2599.443888	116.408691	57.372289
2599.539531	113.973865	57.377293
2598.739441	116.023083	57.382298
2598.793222	116.423220	57.387303
2598.186863	105.812479	57.392308
2596.551735	114.300301	57.397313
2596.148375	113.864800	57.402317
2595.815692	109.171560	57.407322
2594.899303	116.078008	57.412327
2593.686612	108.325702	57.417332
2592.651143	113.737554	57.422337
2592.529911	106.568375	57.427341
2591.804962	108.844345	57.432346
2591.329023	114.430537	57.437351
2591.305682	117.809818	57.442356
2590.619645	119.612573	57.447361
2589.850237	110.479133	57.452365
2589.026191	111.362878	57.457370
2588.296130	107.271240	57.462375
2587.799083	107.816856	57.467380
2586.260434	110.926251	57.472385
2585.965804	107.728434	57.477389
2584.879395	111.118533	57.482394
2584.457108	110.808238	57.487399
2584.454204	107.425553	57.492404
2583.435102	117.676299	57.497409
2583.380763	105.811096	57.502413
2582.923937	111.545198	57.507418
2581.827848	117.932517	57.512423
2581.202521	103.169365	57.517428
2580.550960	112.402437	57.522433
2579.788392	105.473158	57.527437
2578.565358	106.226567	57.532442
2577.997048	111.968676	57.537447
2577.517288	100.980653	57.542452
2576.420830	105.698743	57.547457
2576.561780	104.280877	57.552461
2575.978034	103.857663	57.557466
2575.201598	108.708934	57.562471
2574.428051	108.701445	57.567476
2573.534131	114.039760	57.572481
2573.270712	107.436453	57.577485
2572.658923	106.638308	57.582490
2571.510837	107.922836	57.587495
2571.060688	101.147776	57.592500
2570.131179	108.780785	57.597505
2570.014904	102.407712	57.602509
2569.164420	104.982241	57.607514
2567.608793	109.028065	57.612519
2567.374253	102.372062	57.617524
2566.810241	108.473029	57.622529
2566.434752	102.447023	57.627533
2566.006497	112.215849	57.632538
2565.513068	105.418583	57.637543
2564.870424	104.956493	57.642548
2563.594126	104.373397	57.647553
2562.903291	101.575674	57.652557
2562.644745	99.631651	57.657562
2561.818829	101.900017	57.662567
2561.053216	105.056861	57.667572
2559.938770	104.200577	57.672577
2559.492195	108.778358	57.677581
2559.044708	110.680855	57.682586
2558.547042	112.603378	57.687591
2558.465192	101.992582	57.692596
2557.199422	104.037733	57.697601
2556.595384	103.427734	57.702605
2555.843958	103.311074	57.707610
2555.003437	104.365398	57.712615
2554.965114	103.651975	57.717620
2553.946005	108.464210	57.722625
2553.204521	108.726365	57.727629
2552.713865	109.471017	57.732634
2551.848960	110.463987	57.737639
2551.464757	110.052055	57.742644
2550.087553	109.182274	57.747649
2549.341846	110.182497	57.752653
2548.714284	115.532514	57.757658
2547.927758	114.887399	57.762663
2548.205594	112.450636	57.767668
2547.551145	109.336440	57.772673
2547.287066	107.197975	57.777677
2546.208400	108.603267	57.782682
2544.561030	115.029180	57.787687
2544.478786	97.393155	57.792692
2544.099177	104.659003	57.797697
2543.722018	98.633288	57.802701
2543.125022	102.684565	57.807706
2541.870058	104.910235	57.812711
2541.097507	106.031491	57.817716
2540.836990	115.887296	57.822721
2540.265179	109.074223	57.827725
2538.908440	109.634190	57.832730
2537.782629	112.713675	57.837735
2537.662168	109.139517	57.842740
2536.905144	109.658533	57.847745
2537.509583	102.772655	57.852749
2536.955092	108.057285	57.857754
2535.496629	112.892139	57.862759
2534.540997	116.356202	57.867764
2533.645853	120.092152	57.872769
2533.520598	109.495879	57.877773
2533.099353	112.487278	57.882778
2531.816251	117.498989	57.887783
2531.176415	114.899781	57.892788
2530.296186	122.043995	57.897793
2529.783983	109.891164	57.902797
2529.594933	107.294229	57.907802
2529.312735	114.297910	57.912807
2528.696780	106.868723	57.917812
2527.173290	111.106425	57.922817
2526.743584	101.119560	57.927821
2526.472992	107.594297	57.932826
2525.335164	113.401803	57.937831
2524.340729	105.909433	57.942836
2523.509798	109.204944	57.947841
2523.206270	108.431075	57.952845
2522.424443	113.327482	57.957850
2522.226138	118.107946	57.962855
2522.004132	110.896003	57.967860
2521.345876	108.812298	57.972865
2520.613098	106.630417	57.977869
2519.882854	110.679611	57.982874
2518.951374	112.739854	57.987879
2518.227304	110.854895	57.992884
2517.318648	112.445462	57.997889
2516.638053	110.459916	58.002893
2516.035553	112.908374	58.007898
2515.362692	114.799671	58.012903
2514.977195	111.913437	58.017908
2514.696175	116.188584	58.022913
2513.420499	108.833900	58.027917
2512.489840	102.716507	58.032922
2512.176595	104.676185	58.037927
2512.016414	104.804621	58.042932
2511.132806	112.814645	58.047937
2509.919800	105.041500	58.052941
2509.362371	110.837407	58.057946
2508.281789	111.083729	58.062951
2508.057391	107.521423	58.067956
2507.600874	109.157844	58.072961
2507.362559	110.769986	58.077965
2507.103189	110.674599	58.082970
2505.430872	107.019192	58.087975
2505.023106	107.216010	58.092980
2504.221338	110.938365	58.097985
2503.909725	101.516295	58.102989
2503.117565	109.360688	58.107994
2502.020198	105.378045	58.112999
2501.744241	98.601636	58.118004
2501.179178	106.584038	58.123009
2500.766393	98.487382	58.128013
2499.755170	102.662770	58.133018
2498.548636	103.700734	58.138023
2497.698850	102.935789	58.143028
2497.304480	97.473136	58.148033
2497.127418	96.893561	58.153037
2496.685647	102.042870	58.158042
2496.251260	104.449167	58.163047
2495.506245	95.786045	58.168052
2494.798316	105.622416	58.173057
2494.240506	104.592429	58.178061
2493.089800	101.950312	58.183066
2492.061511	105.741000	58.188071
2491.567216	96.648579	58.193076
2490.872585	105.677046	58.198081
2490.594052	103.640526	58.203085
2490.069212	102.193995	58.208090
2489.022455	102.494930	58.213095
2488.814534	98.192072	58.218100
2487.821496	100.234423	58.223105
2487.296057	93.862633	58.228109
2486.385599	100.028358	58.233114
2485.497076	98.777818	58.238119
2484.759110	98.819124	58.243124
2484.136058	99.113538	58.248129
2484.028639	94.338777	58.253133
2483.342045	97.400409	58.258138
2483.078554	105.220728	58.263143
2481.988052	93.933346	58.268148
2481.012088	107.824358	58.273153
2480.600291	102.032722	58.278157
2480.378853	96.631686	58.283162
2479.566191	99.481592	58.288167
2478.829873	96.247991	58.293172
2477.759292	103.354879	58.298177
2477.584223	106.438791	58.303181
2476.613389	95.220553	58.308186
2475.340356	102.264558	58.313191
2475.064754	107.185729	58.318196
2474.359495	108.380354	58.323201
2474.206673	104.548059	58.328205
2473.660190	106.253546	58.333210
2472.602215	104.692517	58.338215
2471.893253	100.797418	58.343220
2471.250446	111.932353	58.348225
2470.918327	111.907825	58.353229
2470.437602	102.629932	58.358234
2468.942935	105.775255	58.363239
2468.804364	99.026674	58.368244
2467.653527	105.578885	58.373249
2466.861583	98.223617	58.378253
2466.650420	98.057229	58.383258
2466.253358	106.348396	58.388263
2465.667552	104.520330	58.393268
2464.315982	108.272351	58.398273
2463.769438	110.761377	58.403277
2463.075680	101.736218	58.408282
2462.761732	104.882162	58.413287
2462.400776	99.386169	58.418292
2461.640135	108.756308	58.423297
2460.538647	96.118092	58.428301
2459.860686	102.946283	58.433306
2459.508679	110.359777	58.438311
2459.380746	107.794632	58.443316
2457.854238	112.725212	58.448321
2457.176026	100.630788	58.453325
2456.426006	105.788988	58.458330
2455.696196	112.470132	58.463335
2455.591337	103.841638	58.468340
2455.244664	110.975941	58.473345
2454.534015	110.059323	58.478349
2453.391549	93.182075	58.483354
2452.746331	100.594777	58.488359
2452.329484	101.084457	58.493364
2451.978251	109.131350	58.498369
2450.640379	93.573128	58.503373
2450.025161	98.072773	58.508378
2449.196491	94.856152	58.513383
2449.054145	98.556156	58.518388
2448.446071	100.680319	58.523393
2447.367843	107.941279	58.528397
2446.741066	106.272583	58.533402
2446.042655	103.255129	58.538407
2445.763333	102.675278	58.543412
2445.120733	104.536539	58.548417
2444.171358	92.381517	58.553421
2443.391890	93.376471	58.558426
2442.715744	104.363948	58.563431
2442.292575	95.800147	58.568436
2441.616212	101.277321	58.573441
2441.360833	93.645984	58.578445
2440.412636	91.907120	58.583450
2439.210420	101.899842	58.588455
2439.352619	95.192863	58.593460
2438.461222	94.245970	58.598465
2437.464596	100.008421	58.603469
2436.231522	94.782727	58.608474
2435.661214	104.345708	58.613479
2435.904663	107.182410	58.618484
2435.033282	106.121177	58.623489
2434.788206	95.227662	58.628493
2433.986440	96.792859	58.633498
2432.494394	105.972669	58.638503
2432.113368	98.999504	58.643508
2431.955106	96.482573	58.648513
2431.487973	99.058675	58.653517
2430.426984	91.706001	58.658522
2429.284138	102.565254	58.663527
2429.158817	100.941871	58.668532
2428.239459	98.935191	58.673537
2427.830544	104.854122	58.678541
2427.348478	104.751817	58.683546
2426.328550	105.171725	58.688551
2425.933214	97.825231	58.693556
2425.014104	97.738050	58.698561
2424.844037	99.320761	58.703565
2423.443902	100.810249	58.708570
2422.776626	109.660759	58.713575
2422.082804	98.686082	58.718580
2421.737117	107.013463	58.723585
2421.010711	105.490091	58.728589
2420.856051	105.158522	58.733594
2419.825641	104.632888	58.738599
2419.210895	98.991616	58.743604
2418.144559	105.847532	58.748609
2417.839179	100.666110	58.753613
2417.629371	101.288544	58.758618
2416.877231	109.242148	58.763623
2415.793869	98.096454	58.768628
2414.963075	107.897391	58.773633
2414.523151	97.710987	58.778637
2414.059588	91.533492	58.783642
2413.058320	97.218977	58.788647
2412.336865	94.248890	58.793652
2411.595547	104.662136	58.798657
2411.055734	105.780323	58.803661
2410.732710	104.792697	58.808666
2410.039368	107.601685	58.813671
2409.510840	101.690681	58.818676
2408.363208	102.137559	58.823681
2408.022936	101.000125	58.828685
2407.485064	105.359844	58.833690
2406.317506	102.910886	58.838695
2405.809097	92.984478	58.843700
2404.624702	100.644894	58.848705
2404.063525	98.622764	58.853709
2404.141374	100.609122	58.858714
2403.473447	102.433666	58.863719
2403.134879	102.134333	58.868724
2401.965644	104.376951	58.873729
2401.140858	107.598796	58.878733
2400.742180	105.720190	58.883738
2399.833431	108.941787	58.888743
2399.707202	101.908480	58.893748
2398.799785	106.688611	58.898753
2397.572946	105.050291	58.903757
2397.460559	107.228646	58.908762
2396.631600	106.093063	58.913767
2396.303243	95.697331	58.918772
2395.251328	100.692030	58.923777
2394.479533	104.968200	58.928781
2394.054177	95.662701	58.933786
2393.314001	109.969305	58.938791
2393.107212	102.973851	58.943796
2391.937451	110.810976	58.948801
2390.708502	108.540670	58.953805
2390.620464	105.962787	58.958810
2389.862166	104.097122	58.963815
2389.967633	100.253431	58.968820
2389.466154	107.477752	58.973825
2388.292424	100.106074	58.978829
2387.355202	99.498988	58.983834
2386.688268	99.257382	58.988839
2386.396376	92.054256	58.993844
2385.127097	100.966646	58.998849
2384.382864	102.323861	59.003853
2384.143697	95.397498	59.008858
2383.397209	103.423553	59.013863
2383.444305	100.393105	59.018868
2382.298314	105.080616	59.023873
2381.194857	101.313774	59.028877
2380.566418	104.925191	59.033882
2380.233183	101.962934	59.038887
2379.918407	102.349116	59.043892
2379.193915	106.278526	59.048897
2377.972336	103.676186	59.053901
2377.420705	105.806888	59.058906
2376.648570	104.215950	59.063911
2376.064438	101.563822	59.068916
2375.453922	101.735319	59.073921
2374.619260	99.325365	59.078925
2374.355968	94.409112	59.083930
2373.220850	102.338203	59.088935
2373.014825	95.680508	59.093940
2372.548665	96.349540	59.098945
2371.723305	99.335440	59.103949
2370.958595	104.539578	59.108954
2369.920234	98.295379	59.113959
2369.773829	98.496856	59.118964
2369.197245	103.750533	59.123969
2368.750886	102.988861	59.128973
2367.659280	98.258846	59.133978
2366.848282	104.340080	59.138983
2366.333184	103.410958	59.143988
2365.802640	103.495757	59.148993
2364.691769	94.395111	59.153997
2364.220649	96.770590	59.159002
2362.994191	104.139401	59.164007
2363.145621	99.099735	59.169012
2362.630415	102.567848	59.174017
2362.002436	101.681317	59.179021
2360.949301	98.264680	59.184026
2359.821789	103.387176	59.189031
2359.743545	93.131046	59.194036
2359.130830	96.712143	59.199041
2358.755066	96.592457	59.204045
2357.856635	94.539583	59.209050
2356.915627	98.434966	59.214055
2357.247178	94.018164	59.219060
2355.508261	90.554984	59.224065
2354.682456	95.785357	59.229069
2354.219451	95.474543	59.234074
2353.425663	99.090156	59.239079
2353.307512	100.144536	59.244084
2352.841676	97.151274	59.249089
2351.766737	91.642784	59.254093
2351.052406	89.260416	59.259098
2349.857384	89.035697	59.264103
2349.804581	90.694274	59.269108
2349.212002	102.912416	59.274113
2348.533214	99.093888	59.279117
2347.993083	100.315157	59.284122
2346.476238	93.731220	59.289127
2346.349723	86.698763	59.294132
2345.889262	93.921196	59.299137
2345.387625	91.501274	59.304141
2344.819804	95.105484	59.309146
2343.599476	94.184065	59.314151
2343.311270	86.362971	59.319156
2342.837664	96.154139	59.324161
2342.087804	95.254900	59.329165
2340.905254	89.520088	59.334170
2339.706108	96.452007	59.339175
2339.300204	91.603169	59.344180
2339.380987	99.972088	59.349185
2338.570423	92.436096	59.354189
2338.197112	98.069078	59.359194
2337.826931	100.096916	59.364199
2336.843489	92.677325	59.369204
2336.122201	96.377644	59.374209
2335.024347	98.640040	59.379213
2335.104320	91.687532	59.384218
2333.876834	91.972823	59.389223
2333.269774	93.113173	59.394228
2332.632470	96.767948	59.399233
2332.242453	100.315704	59.404237
2331.390933	91.775831	59.409242
2330.489751	96.683187	59.414247
2329.871205	95.939120	59.419252
2329.575664	99.749790	59.424257
2329.063964	98.205112	59.429261
2328.021472	93.698808	59.434266
2327.029606	100.903564	59.439271
2326.475590	96.326756	59.444276
2325.920866	98.502594	59.449281
2325.578818	88.436051	59.454285
2324.729054	91.880849	59.459290
2323.369351	94.696821	59.464295
2323.147403	93.754678	59.469300
2322.401784	93.521799	59.474305
2321.796917	97.072348	59.479309
2321.588049	91.725231	59.484314
2321.162322	97.829002	59.489319
2320.471974	91.076902	59.494324
2319.285450	95.459125	59.499329
2318.379202	89.798645	59.504333
2318.444511	86.725615	59.509338
2317.337643	97.283075	59.514343
2316.819086	85.901108	59.519348
2315.827671	94.131669	59.524353
2315.228795	95.286411	59.529357
2314.885365	86.858206	59.534362
2314.033172	99.083635	59.539367
2313.715520	95.233357	59.544372
2312.487847	94.550430	59.549377
2312.051964	98.717060	59.554381
2311.791520	92.700629	59.559386
2311.050854	104.008996	59.564391
2310.155693	92.152234	59.569396
2309.295946	102.391528	59.574401
2308.789304	99.590374	59.579405
2308.560471	95.480969	59.584410
2307.531596	99.872551	59.589415
2306.573249	91.811200	59.594420
2305.861522	91.903699	59.599425
2305.069259	92.700735	59.604429
2304.759003	94.211503	59.609434
2304.232528	94.148776	59.614439
2304.064464	88.155233	59.619444
2303.095797	93.485037	59.624449
2302.137834	92.984930	59.629453
2301.846116	79.633592	59.634458
2301.108870	91.413058	59.639463
2300.602645	88.420395	59.644468
2299.459063	93.937999	59.649473
2298.951437	94.452687	59.654477
2298.242740	90.078382	59.659482
2297.914217	94.306387	59.664487
2296.758130	96.007978	59.669492
2295.825665	98.201048	59.674497
2295.080456	95.724892	59.679501
2294.889407	93.590536	59.684506
2294.457372	100.178923	59.689511
2294.331224	88.346579	59.694516
2293.451998	90.903951	59.699521
2292.510982	98.616707	59.704525
2291.795186	94.087306	59.709530
2290.626482	95.905526	59.714535
2289.661159	93.677400	59.719540
2289.418200	93.896179	59.724545
2288.977421	102.641248	59.729549
2288.581154	89.195286	59.734554
2287.978748	102.233367	59.739559
2287.252367	90.090391	59.744564
2286.152439	93.810861	59.749569
2285.252791	100.608681	59.754573
2285.219875	100.624180	59.759578
2284.517109	104.938685	59.764583
2284.189258	100.559250	59.769588
2282.910853	95.455821	59.774593
2282.137058	101.338469	59.779597
2281.891020	98.046321	59.784602
2280.991275	100.804567	59.789607
2280.830288	97.661290	59.794612
2280.073696	96.627032	59.799617
2278.681785	95.125914	59.804621
2278.271287	89.407507	59.809626
2277.847001	92.663108	59.814631
2277.966268	95.955621	59.819636
2276.924458	97.085062	59.824641
2275.990574	96.060203	59.829645
2275.830018	99.892394	59.834650
2274.016477	96.288456	59.839655
2273.477404	92.251846	59.844660
2272.585971	95.125508	59.849665
2271.979837	101.806823	59.854669
2271.958631	88.137654	59.859674
2271.124630	92.548018	59.864679
2271.277243	93.312156	59.869684
2270.244674	85.765201	59.874689
2269.468649	91.860983	59.879693
2268.742280	88.726372	59.884698
2267.238918	94.048938	59.889703
2266.977250	94.278812	59.894708
2266.263881	92.056155	59.899713
2265.827537	93.513489	59.904718
2265.621289	92.479853	59.909722
2264.861914	93.808093	59.914727
2263.949539	98.960520	59.919732
2262.915392	92.809968	59.924737
2262.174528	96.757580	59.929742
2261.568542	91.507195	59.934746
2261.238758	99.442257	59.939751
2260.813408	88.718941	59.944756
2260.434684	99.781074	59.949761
2259.263564	104.822231	59.954766
2258.685829	92.456874	59.959770
2257.849847	103.604706	59.964775
2257.536577	93.905473	59.969780
2256.661139	94.953968	59.974785
2255.701500	101.643634	59.979790
2255.396348	92.056695	59.984794
2254.582546	99.780856	59.989799
2254.217499	97.193117	59.994804
2253.671554	94.005943	59.999809
2252.790395	94.910554	60.004814
2251.973842	89.631841	60.009818
2251.447035	93.455219	60.014823
2250.613889	91.516722	60.019828
2250.200181	94.079751	60.024833
2248.884280	94.003616	60.029838
2248.861971	84.766587	60.034842
2248.059229	90.775363	60.039847
2247.735925	92.818477	60.044852
2247.453751	94.566014	60.049857
2246.054710	97.093872	60.054862
2244.977460	94.217026	60.059866
2244.353150	97.924847	60.064871
2244.399116	86.340568	60.069876
2243.569411	81.099634	60.074881
2242.528348	92.245427	60.079886
2242.346065	85.909730	60.084890
2241.548910	100.275011	60.089895
2240.947378	93.322219	60.094900
2240.036289	84.942159	60.099905
2238.686883	86.933786	60.104910
2238.527953	80.241611	60.109914
2238.180573	96.331877	60.114919
2237.634549	80.930038	60.119924
2237.312678	86.667506	60.124929
2236.337547	87.468194	60.129934
2235.140885	82.141996	60.134938
2234.550865	88.340569	60.139943
2234.294185	87.648310	60.144948
2233.939388	88.396989	60.149953
2233.343268	94.277672	60.154958
2232.136162	89.645602	60.159962
2231.534109	89.120956	60.164967
2231.592543	85.394654	60.169972
2230.295935	85.059445	60.174977
2229.004397	91.649560	60.179982
2228.905479	91.159655	60.184986
2228.319008	94.199845	60.189991
2228.034683	79.470071	60.194996
2227.513431	80.407473	60.200001
2226.427560	84.429087	60.205006
2225.559141	87.786696	60.210010
2225.059396	86.628788	60.215015
2224.385479	88.503713	60.220020
2222.737205	91.562865	60.225025
2222.209316	95.040258	60.230030
2222.119835	81.718293	60.235034
2221.311209	94.946363	60.240039
2221.226328	88.029162	60.245044
2220.879150	86.675432	60.250049
2219.701243	89.476913	60.255054
2218.910233	85.676812	60.260058
2217.935120	89.673566	60.265063
2217.773319	89.061789	60.270068
2217.455588	80.145279	60.275073
2216.578977	88.923824	60.280078
2215.770945	80.130637	60.285082
2214.793276	89.889192	60.290087
2214.315970	92.143374	60.295092
2214.119721	86.339391	60.300097
2213.374131	99.759967	60.305102
2212.717967	86.554255	60.310106
2211.586155	96.761134	60.315111
2211.331819	81.863212	60.320116
2210.307617	90.990671	60.325121
2208.812483	86.247610	60.330126
2208.884318	94.224504	60.335130
2208.238609	101.676773	60.340135
2207.904833	96.345106	60.345140
2207.910729	92.611999	60.350145
2206.674877	104.464117	60.355150
2205.460096	97.127936	60.360154
2204.950705	102.479073	60.365159
2204.712292	90.379373	60.370164
2204.162092	93.611907	60.375169
2202.744402	101.129493	60.380174
2202.142205	93.264618	60.385178
2201.631021	102.641834	60.390183
2201.165701	97.648048	60.395188
2200.814993	91.889032	60.400193
2200.304954	102.699290	60.405198
2199.361828	88.931626	60.410202
2198.401678	95.941503	60.415207
2197.887469	85.924952	60.420212
2197.359335	85.339907	60.425217
2196.225943	92.565325	60.430222
2195.638891	86.992385	60.435226
2194.833643	97.946676	60.440231
2194.614326	90.083425	60.445236
2194.216124	90.248235	60.450241
2193.936940	94.799370	60.455246
2192.938755	90.827475	60.460250
2191.802211	96.710195	60.465255
2191.488347	88.566284	60.470260
2190.910755	85.864514	60.475265
2189.661488	89.598697	60.480270
2189.199540	80.269504	60.485274
2188.290316	89.056391	60.490279
2187.886803	93.882595	60.495284
2187.507850	88.002102	60.500289
2186.532000	98.060737	60.505294
2185.318779	90.662721	60.510298
2184.674792	97.491033	60.515303
2184.572264	93.511217	60.520308
2184.095819	91.334892	60.525313
2183.128940	93.742277	60.530318
2183.013507	80.951316	60.535322
2182.462038	91.793914	60.540327
2181.510793	91.760426	60.545332
2180.945077	90.075009	60.550337
2180.182546	102.127614	60.555342
2179.652454	83.915798	60.560346
2178.576673	89.190911	60.565351
2177.868964	87.000062	60.570356
2177.373664	89.428633	60.575361
2177.083013	92.265082	60.580366
2176.313377	86.011687	60.585370
2175.369807	91.253138	60.590375
2175.049104	97.403683	60.595380
2174.392712	96.497167	60.600385
2173.325835	93.999470	60.605390
2172.629827	89.265005	60.610394
2171.875328	95.762099	60.615399
2171.097489	95.404887	60.620404
2171.116313	88.210227	60.625409
2170.438964	89.903384	60.630414
2169.776064	89.481122	60.635418
2169.258565	92.349658	60.640423
2168.574600	89.650295	60.645428
2167.434916	94.918973	60.650433
2166.240474	101.152245	60.655438
2165.679862	100.232113	60.660442
2165.440189	94.900541	60.665447
2164.871325	98.138639	60.670452
2164.945995	95.310711	60.675457
2163.457509	99.189627	60.680462
2162.630088	88.107613	60.685466
2161.783109	94.186329	60.690471
2161.690515	87.897272	60.695476
2161.101076	81.483990	60.700481
2160.191760	95.474122	60.705486
2159.762393	87.619566	60.710490
2158.410333	88.417631	60.715495
2158.493898	82.642374	60.720500
2158.046610	90.115175	60.725505
2156.670940	95.099359	60.730510
2155.756533	85.718873	60.735514
2155.487974	87.626315	60.740519
2154.976312	94.593437	60.745524
2154.713605	94.362853	60.750529
2153.689530	92.252168	60.755534
2153.036986	96.972945	60.760538
2151.842407	102.415220	60.765543
2151.637587	95.922337	60.770548
2151.198077	93.822195	60.775553
2150.378139	101.629120	60.780558
2149.396374	92.899603	60.785562
2148.535731	103.643513	60.790567
2148.215139	95.595489	60.795572
2147.790795	94.674946	60.800577
2147.430675	97.819320	60.805582
2147.112885	87.796420	60.810586
2146.051032	90.315576	60.815591
2145.116641	86.820659	60.820596
2144.664934	93.581349	60.825601
2143.234811	96.379800	60.830606
2142.434381	87.564802	60.835610
2142.023054	90.359524	60.840615
2141.830313	86.892097	60.845620
2141.250766	81.871679	60.850625
2140.500934	86.429100	60.855630
2140.361450	87.513181	60.860634
2138.824600	80.774855	60.865639
2138.432959	87.461325	60.870644
2138.126535	87.384661	60.875649
2136.995839	95.355257	60.880654
2136.380448	82.925328	60.885658
2135.996802	95.736911	60.890663
2135.311836	81.206726	60.895668
2135.077949	87.423336	60.900673
2133.834120	88.416441	60.905678
2133.329459	82.109843	60.910682
2132.716042	91.662032	60.915687
2130.915543	95.650370	60.920692
2130.923624	89.982361	60.925697
2129.971474	92.198952	60.930702
2129.767970	88.447982	60.935706
2129.057234	89.985412	60.940711
2128.787989	93.314366	60.945716
2128.054436	83.003781	60.950721
2127.178273	96.505895	60.955726
2126.543528	90.518769	60.960730
2125.501680	96.850680	60.965735
2125.100846	94.255260	60.970740
2124.590659	93.358085	60.975745
2124.248156	95.721843	60.980750
2123.602566	85.764488	60.985754
2122.457402	97.476761	60.990759
2121.819041	88.728781	60.995764
2121.843236	99.074648	61.000769
2121.056865	100.126482	61.005774
2119.962443	86.183810	61.010778
2119.520397	86.418096	61.015783
2118.390706	89.387790	61.020788
2117.471888	88.509983	61.025793
2116.615441	89.470386	61.030798
2116.901695	83.136668	61.035802
2115.886933	93.393795	61.040807
2115.423851	94.809924	61.045812
2115.073716	94.017213	61.050817
2114.110149	80.597277	61.055822
2113.648787	82.491514	61.060826
2112.633620	94.037082	61.065831
2112.220234	85.060765	61.070836
2111.174585	88.926314	61.075841
2109.904007	96.903077	61.080846
2109.574558	91.679627	61.085850
2109.079169	94.755956	61.090855
2108.688634	92.000493	61.095860
2108.328040	100.511589	61.100865
2107.624122	97.512500	61.105870
2107.433449	91.531921	61.110874
2106.274585	86.800454	61.115879
2105.561536	83.795036	61.120884
2105.281726	92.892286	61.125889
2103.427342	89.643150	61.130894
2103.274001	95.884669	61.135898
2102.725155	95.890523	61.140903
2102.004345	94.861224	61.145908
2101.895349	93.945167	61.150913
2100.581290	97.173760	61.155918
2099.776927	89.974251	61.160922
2099.079359	102.353627	61.165927
2098.372247	90.799489	61.170932
2098.383022	94.010683	61.175937
2097.779228	104.786846	61.180942
2097.479868	92.648642	61.185946
2096.498039	89.862479	61.190951
2095.630063	94.337486	61.195956
2095.136948	96.211105	61.200961
2093.719516	95.656999	61.205966
2093.170999	83.135119	61.210970
2092.694956	91.149265	61.215975
2092.373340	103.428419	61.220980
2091.737500	97.253992	61.225985
2090.906384	97.191289	61.230990
2089.808916	93.396656	61.235994
2089.142242	93.935013	61.240999
2088.515691	89.661955	61.246004
2088.553463	85.098829	61.251009
2087.932494	94.807832	61.256014
2087.320706	90.773029	61.261018
2086.000993	92.431598	61.266023
2085.644601	85.973730	61.271028
2085.501534	85.661505	61.276033
2084.541423	87.325275	61.281038
2083.788208	82.117869	61.286042
2082.767081	96.211203	61.291047
2082.547879	98.096785	61.296052
2081.833932	88.081659	61.301057
2080.467590	98.400901	61.306062
2080.068500	101.894562	61.311066
2079.294757	93.633937	61.316071
2079.120563	96.345474	61.321076
2078.903958	90.009347	61.326081
2077.400621	95.137353	61.331086
2076.310618	89.951632	61.336090
2075.620852	94.447078	61.341095
2075.224910	96.101191	61.346100
2075.025131	92.710363	61.351105
2074.362137	91.316719	61.356110
2074.145145	93.351128	61.361114
2073.633424	99.441586	61.366119
2072.805978	99.204581	61.371124
2072.158435	95.148264	61.376129
2071.171947	95.327263	61.381134
2070.245433	88.882443	61.386138
2069.514240	91.057302	61.391143
2068.725385	98.712868	61.396148
2068.554030	87.418403	61.401153
2067.917985	93.906689	61.406158
2067.743366	95.981612	61.411162
2066.588095	94.032722	61.416167
2065.751528	92.435094	61.421172
2065.114844	85.488745	61.426177
2064.427309	95.007827	61.431182
2063.734853	89.389387	61.436186
2062.944739	97.449757	61.441191
2062.601614	93.877799	61.446196
2061.948364	90.827028	61.451201
2061.306648	101.325080	61.456206
2060.585562	94.636708	61.461210
2059.681477	94.217822	61.466215
2058.881611	86.140483	61.471220
2058.907860	93.116251	61.476225
2057.734239	103.664235	61.481230
2056.993686	95.471751	61.486234
2056.432539	92.288388	61.491239
2055.760814	101.468467	61.496244
2055.729832	96.751317	61.501249
2054.611384	92.900283	61.506254
2053.909151	86.518153	61.511258
2053.118084	98.191969	61.516263
2052.572784	94.988528	61.521268
2052.416240	87.598093	61.526273
2051.014813	100.210753	61.531278
2050.497315	93.201387	61.536282
2049.985453	102.113736	61.541287
2049.822547	99.101455	61.546292
2049.062794	92.105108	61.551297
2047.639836	107.413458	61.556302
2047.203281	96.830643	61.561306
2046.521423	91.852605	61.566311
2046.223717	95.799827	61.571316
2045.033255	95.700312	61.576321
2043.862137	101.046621	61.581326
2043.100468	96.262227	61.586330
2043.066576	97.577713	61.591335
2042.667255	100.649062	61.596340
2042.618928	87.229690	61.601345
2041.633818	94.625153	61.606350
2040.971969	90.539711	61.611354
2039.752680	94.404581	61.616359
2039.025907	92.652787	61.621364
2038.721244	90.718663	61.626369
2038.363113	94.967130	61.631374
2037.855814	89.401888	61.636378
2036.948884	103.095580	61.641383
2036.251585	93.225635	61.646388
2035.881143	84.632760	61.651393
2034.159721	92.325480	61.656398
2033.727731	89.045031	61.661402
2033.303100	101.178386	61.666407
2032.670341	93.230749	61.671412
2032.780031	92.899368	61.676417
2031.322068	94.620281	61.681422
2030.537341	87.515716	61.686426
2029.899879	98.693144	61.691431
2029.191438	101.695796	61.696436
2028.796766	94.203204	61.701441
2028.459091	102.632618	61.706446
2027.703118	95.627732	61.711450
2026.857893	90.808690	61.716455
2026.203990	96.061793	61.721460
2026.075010	92.453208	61.726465
2024.413407	101.637223	61.731470
2023.943594	95.046398	61.736474
2023.689302	95.459751	61.741479
2023.204021	89.551680	61.746484
2022.188646	88.296476	61.751489
2020.911891	99.490105	61.756494
2020.608769	94.617805	61.761498
2019.702470	87.478777	61.766503
2019.584844	99.226074	61.771508
2019.418317	89.187584	61.776513
2018.972029	95.557759	61.781518
2017.582308	86.193883	61.786522
2017.111036	92.770823	61.791527
2016.724408	94.265062	61.796532
2015.588836	86.344628	61.801537
2014.465684	93.707655	61.806542
2014.366775	89.894199	61.811546
2014.021298	83.622362	61.816551
2012.388651	91.039385	61.821556
2012.128535	83.944162	61.826561
2011.159123	87.957337	61.831566
2010.856262	85.143863	61.836570
2010.699281	85.998843	61.841575
2009.850243	85.049122	61.846580
2009.590374	77.503483	61.851585
2008.065343	90.993829	61.856590
2007.740275	83.048436	61.861594
2007.222133	80.273368	61.866599
2006.083116	94.905928	61.871604
2005.088319	86.903787	61.876609
2004.525147	86.618824	61.881614
2004.076766	85.929765	61.886618
2003.875251	77.510101	61.891623
2003.405468	91.356364	61.896628
2003.335178	85.645326	61.901633
2001.739477	95.034375	61.906638
2001.168024	81.239519	61.911642
2000.813617	95.257490	61.916647
1999.679894	90.350046	61.921652
1998.926883	83.892539	61.926657
1998.139655	97.300892	61.931662
1997.933746	86.885079	61.936666
1997.498290	90.197863	61.941671
1996.181127	93.073732	61.946676
1995.333669	88.452835	61.951681
1994.553337	93.054171	61.956686
1994.045769	89.939807	61.961690
1993.667352	87.565953	61.966695
1993.490568	93.510305	61.971700
1993.017102	81.560195	61.976705
1991.625412	88.831007	61.981710
1991.172490	88.348771	61.986714
1990.632960	93.516787	61.991719
1989.996962	90.046250	61.996724
1989.731818	92.397964	62.001729
1987.953431	98.787994	62.006734
1987.644588	92.141220	62.011738
1987.032499	96.261427	62.016743
1986.475487	97.332069	62.021748
1986.253570	91.273955	62.026753
1985.214737	92.992654	62.031758
1984.388587	88.059837	62.036762
1983.942238	95.051709	62.041767
1983.408090	92.824885	62.046772
1983.032952	85.354225	62.051777
1981.578583	87.232029	62.056782
1981.110720	85.216490	62.061786
1980.572909	82.803196	62.066791
1979.890453	91.324344	62.071796
1979.830977	81.710824	62.076801
1978.865402	79.595302	62.081806
1978.016439	79.235287	62.086810
1977.327122	79.543461	62.091815
1976.085109	88.750040	62.096820
1975.772729	85.143625	62.101825
1974.899945	92.561719	62.106830
1974.694699	89.114994	62.111834
1974.035466	91.384129	62.116839
1973.584533	86.979605	62.121844
1972.592179	80.555548	62.126849
1971.571106	89.723544	62.131854
1971.212929	88.972481	62.136858
1970.808505	87.781715	62.141863
1970.090746	91.071348	62.146868
1969.674996	78.627839	62.151873
1968.758546	88.862631	62.156878
1968.324106	80.050990	62.161882
1967.854500	95.056519	62.166887
1966.623379	95.544218	62.171892
1965.971075	78.290052	62.176897
1965.321408	86.832824	62.181902
1964.693910	86.158621	62.186906
1964.187700	87.342148	62.191911
1963.558158	90.579587	62.196916
1962.601730	80.235727	62.201921
1961.923059	89.109896	62.206926
1961.526955	84.003654	62.211930
1960.981901	80.022587	62.216935
1960.052105	88.927084	62.221940
1959.133978	87.201722	62.226945
1958.589796	86.765889	62.231950
1958.515610	86.581221	62.236954
1957.911048	84.864585	62.241959
1956.514154	89.078785	62.246964
1956.009481	82.784849	62.251969
1955.094914	92.371585	62.256974
1955.270676	82.686642	62.261978
1954.824121	89.770517	62.266983
1953.479506	85.961753	62.271988
1953.075759	80.078826	62.276993
1952.258694	87.500019	62.281998
1951.509644	84.801168	62.287002
1950.292801	83.730832	62.292007
1949.202578	93.919568	62.297012
1949.620186	87.638377	62.302017
1948.780733	89.905583	62.307022
1948.711907	89.699472	62.312026
1947.923521	87.774688	62.317031
1946.777605	86.689456	62.322036
1945.959429	84.825424	62.327041
1945.273670	91.336035	62.332046
1944.924563	89.222029	62.337050
1944.867934	84.783212	62.342055
1944.093145	91.663513	62.347060
1943.413055	79.153129	62.352065
1942.562063	96.031328	62.357070
1941.467405	91.718771	62.362074
1940.026229	92.791467	62.367079
1939.508243	94.676851	62.372084
1938.990182	83.889730	62.377089
1938.952596	87.916394	62.382094
1938.598036	82.911991	62.387098
1938.280769	81.463171	62.392103
1937.193253	88.301841	62.397108
1936.421851	84.756193	62.402113
1935.849703	90.936723	62.407118
1935.312908	82.486398	62.412122
1934.509805	86.919141	62.417127
1933.046872	90.038636	62.422132
1932.659353	83.268364	62.427137
1932.137140	94.503044	62.432142
1931.336139	85.411103	62.437146
1930.955418	89.553702	62.442151
1930.619248	88.274688	62.447156
1930.330440	90.428749	62.452161
1929.167084	92.376778	62.457166
1928.513098	94.705807	62.462170
1927.907776	86.355228	62.467175
1927.303395	88.560907	62.472180
1926.752221	80.081467	62.477185
1925.887981	80.564041	62.482190
1925.153778	85.879829	62.487194
1924.013043	85.248040	62.492199
1922.835052	85.149577	62.497204
1922.776877	82.255964	62.502209
1922.087047	88.019275	62.507214
1921.742742	81.690806	62.512218
1921.206738	83.596641	62.517223
1920.860301	81.955846	62.522228
1920.584737	81.386041	62.527233
1919.281768	80.081773	62.532238
1918.673843	89.641707	62.537242
1918.037843	74.729414	62.542247
1916.814088	87.212215	62.547252
1916.325848	78.036778	62.552257
1915.642731	86.695006	62.557262
1915.230582	87.516275	62.562266
1914.901305	83.363305	62.567271
1914.089731	86.841090	62.572276
1913.175445	81.255895	62.577281
1912.191789	89.250306	62.582286
1912.015593	87.053041	62.587290
1911.704668	90.307420	62.592295
1910.226340	90.072059	62.597300
1909.655424	84.228392	62.602305
1908.969237	87.862747	62.607310
1908.753013	82.546141	62.612314
1908.431526	81.903670	62.617319
1907.235706	81.613663	62.622324
1906.978113	76.665306	62.627329
1906.047660	83.085151	62.632334
1905.454244	83.754676	62.637338
1904.562436	82.939390	62.642343
1903.319987	89.242489	62.647348
1903.076445	79.118122	62.652353
1902.452299	81.368234	62.657358
1901.856042	82.475596	62.662362
1901.684528	81.777469	62.667367
1900.962371	79.909650	62.672372
1899.966344	82.144044	62.677377
1899.526599	82.910038	62.682382
1898.789548	78.534344	62.687386
1898.099217	77.745773	62.692391
1897.062148	86.674942	62.697396
1896.049846	80.420100	62.702401
1895.301379	83.328561	62.707406
1895.072886	89.181495	62.712410
1895.167793	78.352676	62.717415
1894.659915	83.804213	62.722420
1893.977682	79.103365	62.727425
1892.633826	84.841205	62.732430
1892.068926	79.027302	62.737434
1891.822427	80.608490	62.742439
1890.511645	93.305916	62.747444
1889.721454	76.198519	62.752449
1888.935692	89.447543	62.757454
1888.941485	92.983252	62.762458
1888.348732	87.228584	62.767463
1887.854863	94.381737	62.772468
1886.931923	82.762747	62.777473
1886.173002	86.434019	62.782478
1885.906696	84.537555	62.787482
1885.032785	88.384809	62.792487
1883.879788	85.583768	62.797492
1883.515349	86.562265	62.802497
1883.147272	91.194131	62.807502
1882.311391	89.551419	62.812506
1881.543616	87.004198	62.817511
1880.358063	90.189536	62.822516
1879.990700	79.508090	62.827521
1879.505824	90.707563	62.832526
1878.940609	85.592765	62.837530
1878.680098	86.259415	62.842535
1877.448844	86.298754	62.847540
1877.013484	87.783180	62.852545
1876.297912	90.566022	62.857550
1875.468573	83.588726	62.862554
1874.354815	84.132153	62.867559
1873.874928	94.268187	62.872564
1873.133218	85.939374	62.877569
1872.705602	91.160482	62.882574
1872.471589	83.975156	62.887578
1872.385960	83.540221	62.892583
1871.378616	84.621999	62.897588
1870.616497	81.987369	62.902593
1869.663795	84.684468	62.907598
1868.903252	85.902042	62.912602
1867.954797	84.442007	62.917607
1867.063843	90.210128	62.922612
1866.633610	82.344719	62.927617
1866.324404	95.081971	62.932622
1866.068311	88.271065	62.937626
1865.564897	87.481703	62.942631
1864.590445	87.652760	62.947636
1864.359213	84.927699	62.952641
1863.064950	85.023213	62.957646
1861.784895	90.061752	62.962650
1861.288978	90.228700	62.967655
1860.480868	91.884659	62.972660
1860.026317	84.399185	62.977665
1859.554230	92.075958	62.982670
1859.244490	82.661972	62.987674
1859.153700	86.496033	62.992679
1857.933535	85.705750	62.997684
1857.085690	84.965448	63.002689
1856.582599	80.487763	63.007694
1856.046285	80.798590	63.012698
1854.917248	81.244771	63.017703
1854.034280	89.688916	63.022708
1854.189710	88.505004	63.027713
1853.526833	82.816812	63.032718
1852.515578	89.451797	63.037722
1851.981232	83.481494	63.042727
1851.005284	87.523440	63.047732
1851.063423	85.245825	63.052737
1849.589667	80.749875	63.057742
1848.652467	79.739874	63.062746
1848.185337	84.358686	63.067751
1847.113604	88.177820	63.072756
1847.126157	90.448475	63.077761
1846.429936	96.405511	63.082766
1846.246452	89.002735	63.087770
1845.591968	80.955838	63.092775
1844.449239	86.425208	63.097780
1843.991801	77.952643	63.102785
1843.457129	84.367147	63.107790
1842.434008	89.525935	63.112794
1841.342911	82.000957	63.117799
1841.003236	90.079399	63.122804
1840.493826	84.643231	63.127809
1840.166378	85.644216	63.132814
1839.555044	86.434834	63.137818
1838.781461	84.134920	63.142823
1837.717412	97.102760	63.147828
1837.325502	88.228206	63.152833
1836.932758	86.079047	63.157838
1836.341053	87.724035	63.162842
1835.412300	92.864706	63.167847
1834.643248	96.670345	63.172852
1833.996437	88.910280	63.177857
1832.620067	82.352626	63.182862
1832.271693	82.117376	63.187866
1831.965342	82.200185	63.192871
1831.438353	93.323577	63.197876
1830.852278	85.979816	63.202881
1830.410395	84.891389	63.207886
1829.331497	88.314268	63.212890
1828.869184	79.842144	63.217895
1827.967064	100.260655	63.222900
1827.495782	88.153894	63.227905
1826.490202	96.028915	63.232910
1825.414807	88.757819	63.237914
1825.293973	83.413454	63.242919
1824.451491	93.014707	63.247924
1823.984121	78.067270	63.252929
1823.301892	84.955818	63.257934
1823.284187	82.876304	63.262938
1822.194978	83.459750	63.267943
1821.060508	84.843539	63.272948
1820.954641	81.538108	63.277953
1820.405328	79.616651	63.282958
1819.628809	80.793150	63.287962
1818.665987	83.079111	63.292967
1817.856328	85.297817	63.297972
1817.856589	78.809361	63.302977
1816.390825	89.052492	63.307982
1815.692171	83.743044	63.312986
1815.292466	87.922841	63.317991
1814.393989	88.641806	63.322996
1814.137397	84.517067	63.328001
1813.514370	89.686349	63.333006
1813.602471	94.611994	63.338010
1812.796607	90.992924	63.343015
1811.715398	89.658636	63.348020
1810.555248	85.519945	63.353025
1809.491392	91.318050	63.358030
1808.709803	88.638210	63.363034
1809.012359	86.187335	63.368039
1808.327843	96.016946	63.373044
1807.983515	87.737785	63.378049
1807.225905	88.410545	63.383054
1806.215743	83.778055	63.388058
1805.604478	83.581470	63.393063
1804.569773	84.766227	63.398068
1804.396267	84.753679	63.403073
1803.810456	94.732185	63.408078
1802.542405	91.659150	63.413082
1802.384047	77.233167	63.418087
1801.548706	86.198090	63.423092
1801.537872	80.829381	63.428097
1800.054146	93.812976	63.433102
1799.482037	84.424942	63.438106
1798.925714	80.400829	63.443111
1797.955076	91.778935	63.448116
1797.874573	84.801818	63.453121
1797.429526	87.574300	63.458126
1796.098576	94.541086	63.463130
1795.802396	84.155751	63.468135
1794.909566	89.806179	63.473140
1794.901547	86.198229	63.478145
1793.308765	85.795387	63.483150
1792.708101	87.595458	63.488154
1792.160187	78.746820	63.493159
1791.499827	86.443568	63.498164
1791.395893	77.809480	63.503169
1790.413122	85.427187	63.508174
1789.479705	86.818817	63.513178
1789.121263	80.002148	63.518183
1788.380010	86.052543	63.523188
1787.944360	83.882310	63.528193
1787.209422	82.919421	63.533198
1786.308592	85.630157	63.538202
1785.906965	78.743907	63.543207
1784.991481	78.433594	63.548212
1784.696888	79.541455	63.553217
1783.498832	82.179499	63.558222
1782.967422	88.439903	63.563226
1782.634620	82.948264	63.568231
1781.804373	79.638099	63.573236
1781.333061	72.931137	63.578241
1780.414037	72.600115	63.583246
1779.799015	83.318580	63.588250
1779.540857	81.962681	63.593255
1778.324785	89.708331	63.598260
1777.305668	86.792834	63.603265
1776.690351	82.769344	63.608270
1776.241448	84.507136	63.613274
1775.996072	72.971193	63.618279
1775.342384	79.458954	63.623284
1774.921607	81.608758	63.628289
1773.792934	84.268089	63.633294
1772.793149	87.116148	63.638298
1772.656435	77.944536	63.643303
1772.148354	83.030996	63.648308
1771.601130	79.820427	63.653313
1770.433298	82.362122	63.658318
1769.845060	88.614882	63.663322
1769.250626	79.837757	63.668327
1768.678228	86.841721	63.673332
1768.161828	76.245402	63.678337
1767.176459	85.680847	63.683342
1766.423899	85.220691	63.688346
1766.145410	83.037385	63.693351
1765.356840	87.612521	63.698356
1764.459461	77.934773	63.703361
1763.694246	88.942614	63.708366
1763.163386	89.763680	63.713370
1762.854226	84.652061	63.718375
1762.371478	91.787129	63.723380
1761.291030	77.452220	63.728385
1760.687662	86.699940	63.733390
1760.078948	85.531123	63.738394
1759.457258	81.345707	63.743399
1757.823928	87.041923	63.748404
1757.924216	75.603935	63.753409
1757.048795	84.423751	63.758414
1756.585271	82.024616	63.763418
1756.180562	77.237231	63.768423
1755.795044	85.464033	63.773428
1755.056645	78.536337	63.778433
1754.036142	81.511886	63.783438
1753.280140	76.239106	63.788442
1753.209847	84.267898	63.793447
1751.929804	90.062345	63.798452
1751.693717	82.089924	63.803457
1751.378498	90.067473	63.808462
1750.030311	86.573973	63.813466
1748.889935	81.479852	63.818471
1748.042304	80.479412	63.823476
1747.867899	80.818716	63.828481
1747.497050	81.843710	63.833486
1747.129971	91.187575	63.838490
1746.531535	82.196017	63.843495
1745.639288	90.878590	63.848500
1745.106104	87.132354	63.853505
1744.402173	89.455341	63.858510
1743.494047	86.957816	63.863514
1742.483693	82.657335	63.868519
1741.734826	89.688338	63.873524
1741.344050	76.494981	63.878529
1740.651054	81.030870	63.883534
1740.585937	86.034038	63.888538
1739.751354	77.733783	63.893543
1738.602334	84.213939	63.898548
1738.309792	76.989309	63.903553
1738.069615	82.153476	63.908558
1736.751951	81.838570	63.913562
1736.003425	80.990904	63.918567
1735.342374	81.098491	63.923572
1734.651301	74.992799	63.928577
1734.169593	82.763974	63.933582
1733.800580	90.065493	63.938586
1732.817681	84.632206	63.943591
1732.083748	80.818485	63.948596
1731.622658	76.644672	63.953601
1730.905566	89.324207	63.958606
1730.261875	83.167775	63.963610
1729.649228	74.082740	63.968615
1728.416316	81.275904	63.973620
1727.722641	83.233206	63.978625
1727.760773	82.511845	63.983630
1727.206349	86.042752	63.988634
1727.176662	78.888009	63.993639
1725.549406	84.218077	63.998644
1725.240847	85.445958	64.003649
1724.739258	84.043693	64.008654
1723.238525	93.358523	64.013658
1722.367851	80.233862	64.018663
1721.742195	87.542981	64.023668
1721.488495	81.536916	64.028673
1720.884132	83.471437	64.033678
1720.767536	79.693394	64.038682
1720.493868	78.920785	64.043687
1719.264231	81.850418	64.048692
1718.587437	81.929518	64.053697
1717.893770	80.293291	64.058702
1716.400776	85.362767	64.063706
1715.783206	79.238184	64.068711
1714.994810	88.682954	64.073716
1715.366559	82.382375	64.078721
1714.668388	81.322814	64.083726
1714.198470	91.842779	64.088730
1713.930193	84.573735	64.093735
1712.907659	83.288242	64.098740
1712.273218	87.100857	64.103745
1711.036085	80.247458	64.108750
1710.159352	84.718874	64.113754
1709.550484	75.545962	64.118759
1708.943845	78.117161	64.123764
1708.688006	73.761789	64.128769
1707.696262	80.679226	64.133774
1706.549625	81.058584	64.138778
1706.003492	74.266152	64.143783
1705.426238	87.020436	64.148788
1705.059786	77.146861	64.153793
1704.534784	75.813734	64.158798
1704.338921	87.829365	64.163802
1704.022099	71.879667	64.168807
1702.583654	77.772667	64.173812
1701.852510	77.474245	64.178817
1701.346861	73.103202	64.183822
1699.918836	79.650840	64.188826
1699.799552	74.671339	64.193831
1699.232071	80.084530	64.198836
1698.858723	79.384240	64.203841
1698.404413	78.522548	64.208846
1697.160596	84.121734	64.213850
1696.103505	72.725887	64.218855
1695.747352	80.014544	64.223860
1695.428537	81.579298	64.228865
1695.231862	77.499185	64.233870
1693.813971	81.533489	64.238874
1693.259622	77.424585	64.243879
1692.613620	81.435749	64.248884
1692.191159	79.952845	64.253889
1691.248893	74.843788	64.258894
1690.191753	79.661062	64.263898
1689.780874	70.822946	64.268903
1689.216597	70.982660	64.273908
1689.229335	80.068901	64.278913
1688.335300	71.099918	64.283918
1687.166037	77.328554	64.288922
1686.742174	78.957861	64.293927
1686.270623	82.722078	64.298932
1685.513232	85.187240	64.303937
1684.338362	81.911987	64.308942
1683.482859	84.596430	64.313946
1683.281078	86.212207	64.318951
1682.600100	89.152563	64.323956
1682.338950	86.716044	64.328961
1681.319774	80.726897	64.333966
1679.871894	88.449073	64.338970
1680.022408	85.279770	64.343975
1679.221609	83.391892	64.348980
1678.886593	83.075027	64.353985
1678.759464	85.152483	64.358990
1677.746665	87.232292	64.363994
1677.075923	84.596664	64.368999
1675.973221	84.933380	64.374004
1675.741544	79.886273	64.379009
1674.622055	72.651194	64.384014
1673.627380	78.182092	64.389018
1673.500495	77.672513	64.394023
1672.992406	87.179840	64.399028
1672.332469	81.332897	64.404033
1671.254113	79.297920	64.409038
1670.596357	79.773225	64.414042
1669.907128	69.946606	64.419047
1668.950996	87.434071	64.424052
1669.174415	71.506797	64.429057
1668.376019	75.506147	64.434062
1667.985824	80.219558	64.439066
1667.238446	67.828135	64.444071
1666.299311	81.203657	64.449076
1665.444519	78.410061	64.454081
1664.656333	81.674276	64.459086
1664.008222	83.533792	64.464090
1663.798059	74.886716	64.469095
1663.314697	80.105523	64.474100
1662.385506	76.706529	64.479105
1661.467134	77.935743	64.484110
1660.631425	79.196600	64.489114
1660.470188	79.832456	64.494119
1659.492196	84.931442	64.499124
1658.380755	82.584380	64.504129
1657.523599	73.365551	64.509134
1657.092468	78.675284	64.514138
1656.950819	78.853071	64.519143
1656.352075	83.663352	64.524148
1655.944713	77.936212	64.529153
1655.739688	79.743194	64.534158
1654.134951	74.732117	64.539162
1653.791108	71.773329	64.544167
1653.287738	75.827584	64.549172
1652.641801	75.667344	64.554177
1652.124670	76.897368	64.559182
1651.056851	79.157509	64.564186
1650.302453	74.556684	64.569191
1649.071942	83.473191	64.574196
1648.514541	79.908739	64.579201
1648.128668	72.965740	64.584206
1647.450191	84.110309	64.589210
1647.252574	80.485867	64.594215
1646.754910	72.971104	64.599220
1646.332243	79.637618	64.604225
1645.199989	80.295568	64.609230
1643.982962	81.076573	64.614234
1644.135297	75.104057	64.619239
1643.243477	79.273338	64.624244
1642.092923	80.090335	64.629249
1641.380702	75.483478	64.634254
1640.856092	83.082003	64.639258
1640.712762	66.916328	64.644263
1640.236992	81.935112	64.649268
1639.278549	76.081236	64.654273
1638.383070	75.606875	64.659278
1637.638713	75.710574	64.664282
1637.478813	86.471152	64.669287
1636.288483	90.275485	64.674292
1635.384314	81.249827	64.679297
1634.893636	79.807022	64.684302
1634.391664	86.992746	64.689306
1634.147271	81.897295	64.694311
1633.404925	80.352696	64.699316
1632.696679	74.742968	64.704321
1631.707195	78.545691	64.709326
1631.355979	80.276643	64.714330
1630.887043	66.593822	64.719335
1629.680746	75.501446	64.724340
1628.696545	86.233356	64.729345
1628.514410	84.493815	64.734350
1627.685312	82.932485	64.739354
1628.076036	76.084737	64.744359
1626.710505	74.085889	64.749364
1625.778045	74.504004	64.754369
1625.172882	75.940929	64.759374
1624.465351	82.588301	64.764378
1624.481363	76.198608	64.769383
1623.022596	80.805951	64.774388
1622.123274	78.839422	64.779393
1621.881755	73.776244	64.784398
1621.060487	81.749996	64.789402
1621.039127	74.169910	64.794407
1619.829642	77.662536	64.799412
1618.987399	73.351870	64.804417
1618.436987	78.243088	64.809422
1617.801911	86.938893	64.814426
1617.628386	78.777372	64.819431
1616.909927	80.854975	64.824436
1615.730316	72.253421	64.829441
1615.410373	75.451719	64.834446
1614.706982	75.720508	64.839450
1614.663040	70.924297	64.844455
1613.390401	78.620834	64.849460
1612.620157	67.820901	64.854465
1612.334393	70.164308	64.859470
1611.346996	80.261264	64.864474
1610.461442	70.630092	64.869479
1609.366913	72.072216	64.874484
1608.800960	69.769573	64.879489
1608.689243	72.807505	64.884494
1608.056603	78.752092	64.889498
1607.944053	73.276862	64.894503
1607.255605	77.085700	64.899508
1605.923052	72.157135	64.904513
1605.520828	78.407668	64.909518
1604.607312	71.594052	64.914522
1604.386741	72.519919	64.919527
1603.285360	68.925417	64.924532
1602.446461	75.780787	64.929537
1602.050902	71.924974	64.934542
1601.510103	84.627227	64.939546
1601.431209	72.097341	64.944551
1600.389446	88.039925	64.949556
1599.244908	76.286853	64.954561
1598.720711	76.047367	64.959566
1598.138263	77.577114	64.964570
1598.034095	76.216188	64.969575
1596.601290	73.453239	64.974580
1596.542582	70.637888	64.979585
1596.020087	79.766376	64.984590
1594.753990	74.654738	64.989594
1593.791604	72.627564	64.994599
1593.059344	74.023088	64.999604
1592.428633	80.942697	65.004609
1592.409100	69.247354	65.009614
1591.949203	82.559022	65.014618
1591.392828	69.784421	65.019623
1590.342808	78.387426	65.024628
1589.929375	72.951454	65.029633
1589.292092	73.181697	65.034638
1587.697559	82.001832	65.039642
1587.434342	78.942413	65.044647
1586.737130	86.228653	65.049652
1586.451714	79.542404	65.054657
1585.959997	73.305129	65.059662
1584.623262	82.540205	65.064666
1583.838653	73.895534	65.069671
1583.466544	80.275513	65.074676
1582.997778	78.116102	65.079681
1582.872464	76.289474	65.084686
1581.727976	88.075485	65.089690
1580.684253	71.507355	65.094695
1579.912317	77.920235	65.099700
1579.768818	80.566520	65.104705
1579.702998	82.819397	65.109710
1577.973482	91.493306	65.114714
1577.590869	79.532873	65.119719
1576.827884	88.337408	65.124724
1576.417638	79.290393	65.129729
1575.945200	70.826368	65.134734
1575.550586	83.337030	65.139738
1574.700912	78.312412	65.144743
1573.906469	77.241324	65.149748
1572.827469	82.968238	65.154753
1571.944124	72.977108	65.159758
1571.182487	78.865223	65.164762
1571.092060	71.915488	65.169767
1570.547027	77.273924	65.174772
1570.112001	69.119275	65.179777
1569.792779	78.350336	65.184782
1568.322182	75.926217	65.189786
1567.796610	76.650084	65.194791
1567.215675	83.144353	65.199796
1566.420487	75.091996	65.204801
1565.688761	71.460291	65.209806
1564.746901	84.407225	65.214810
1564.282537	71.025199	65.219815
1563.874845	80.890322	65.224820
1563.686726	80.338334	65.229825
1562.735721	71.693332	65.234830
1561.621736	78.000944	65.239834
1561.249110	73.618603	65.244839
1560.673222	80.959864	65.249844
1559.742195	76.985311	65.254849
1558.648379	72.328519	65.259854
1558.032669	76.930534	65.264858
1557.759006	73.365298	65.269863
1557.288844	75.337258	65.274868
1556.807936	77.459077	65.279873
1556.727333	69.670069	65.284878
1555.327106	80.552913	65.289882
1554.751152	78.307644	65.294887
1553.960806	75.762371	65.299892
1553.344973	80.735839	65.304897
1552.554334	70.002172	65.309902
1551.333341	80.542120	65.314906
1550.942078	79.006130	65.319911
1550.363951	75.430241	65.324916
1550.188409	73.290515	65.329921
1549.670722	71.453283	65.334926
1548.584364	78.306012	65.339930
1548.151295	77.199922	65.344935
1547.512727	76.991068	65.349940
1546.599930	74.936864	65.354945
1546.322506	72.228812	65.359950
1545.572871	84.525509	65.364954
1544.833790	73.425402	65.369959
1543.645576	82.960314	65.374964
1542.962505	82.033583	65.379969
1542.569486	70.323224	65.384974
1541.615645	84.476498	65.389978
1541.324565	78.946962	65.394983
1541.217335	77.993517	65.399988
1540.015197	75.991203	65.404993
1539.532662	76.950460	65.409998
1538.715215	82.632615	65.415002
1538.528331	72.697947	65.420007
1537.409632	81.825058	65.425012
1536.184026	81.837460	65.430017
1535.763357	76.829029	65.435022
1535.232983	72.793412	65.440026
1535.309348	72.032351	65.445031
1534.520136	84.110832	65.450036
1533.297309	85.394148	65.455041
1532.492363	82.616520	65.460046
1531.913888	87.165195	65.465050
1531.628941	83.714385	65.470055
1531.109787	79.698160	65.475060
1529.646722	69.904152	65.480065
1529.228847	71.972160	65.485070
1528.300308	81.206852	65.490074
1527.949723	76.362473	65.495079
1527.980502	82.418511	65.500084
1527.426388	88.260854	65.505089
1526.841167	74.989514	65.510094
1525.544218	80.415067	65.515098
1525.026191	75.624608	65.520103
1524.003921	80.790397	65.525108
1522.923909	81.688106	65.530113
1522.958098	68.422465	65.535118
1521.870537	83.512793	65.540122
1522.085822	73.837701	65.545127
1520.951520	76.874999	65.550132
1519.971438	83.256408	65.555137
1519.643323	76.099867	65.560142
1519.183495	75.038226	65.565146
1518.551846	73.048404	65.570151
1517.396181	79.110932	65.575156
1516.560608	73.501310	65.580161
1516.338169	73.840948	65.585166
1515.922341	78.859920	65.590170
1515.298915	80.185119	65.595175
1513.848189	74.619600	65.600180
1513.222638	75.036915	65.605185
1512.695493	70.770233	65.610190
1512.107044	80.440907	65.615194
1512.078620	77.521301	65.620199
1511.227692	79.191345	65.625204
1510.000225	77.887683	65.630209
1509.486379	70.897139	65.635214
1508.923984	82.020261	65.640218
1508.830146	72.071252	65.645223
1507.726598	75.512217	65.650228
1506.552115	75.939803	65.655233
1506.571981	72.582084	65.660238
1505.821685	86.062658	65.665242
1505.428432	72.164812	65.670247
1504.458180	76.685807	65.675252
1503.233645	78.941221	65.680257
1502.687687	76.120851	65.685262
1502.134615	80.830171	65.690266
1502.227378	78.561635	65.695271
1501.239133	78.495132	65.700276
1499.924190	87.492820	65.705281
1499.913893	80.163863	65.710286
1499.060665	85.597159	65.715290
1498.909112	83.330967	65.720295
1498.092972	76.604914	65.725300
1496.694807	83.106434	65.730305
1496.254541	71.883358	65.735310
1496.067848	78.320809	65.740314
1495.453473	70.707634	65.745319
1494.336547	75.362677	65.750324
1493.859413	80.412274	65.755329
1493.830473	78.014180	65.760334
1492.357758	85.482497	65.765338
1491.391315	77.392760	65.770343
1490.744651	78.655626	65.775348
1490.453692	84.613185	65.780353
1490.195796	77.417788	65.785358
1489.341582	83.110189	65.790362
1488.440456	70.058319	65.795367
1487.504478	72.473547	65.800372
1487.293480	80.199967	65.805377
1486.797204	73.211155	65.810382
1486.193938	73.551636	65.815386
1485.281119	78.795008	65.820391
1484.528112	77.316203	65.825396
1483.907551	76.126557	65.830401
1483.472288	76.023039	65.835406
1482.247704	88.564839	65.840410
1481.491119	71.007776	65.845415
1481.128999	77.196580	65.850420
1480.371687	82.941867	65.855425
1480.135618	77.748302	65.860430
1479.546572	78.094639	65.865434
1478.530350	75.245820	65.870439
1477.968603	76.020490	65.875444
1477.365249	76.488087	65.880449
1477.165651	71.320255	65.885454
1475.862786	76.507235	65.890458
1475.075744	71.277720	65.895463
1474.569777	75.257827	65.900468
1473.768086	77.848222	65.905473
1474.004084	81.730940	65.910478
1472.877885	74.240107	65.915482
1471.995413	75.829902	65.920487
1471.305156	79.896024	65.925492
1470.768480	83.663505	65.930497
1469.790665	74.952066	65.935502
1468.978317	86.535980	65.940506
1468.372303	74.749199	65.945511
1467.968263	80.629405	65.950516
1467.451835	68.527310	65.955521
1467.217216	74.867966	65.960526
1466.262912	78.753109	65.965530
1465.444131	71.184400	65.970535
1464.980909	71.736955	65.975540
1464.140026	71.667735	65.980545
1463.241441	71.924956	65.985550
1462.406533	76.327665	65.990554
1461.762007	70.665621	65.995559
1461.163403	78.341940	66.000564
1460.572193	80.715925	66.005569
1460.739100	72.368269	66.010574
1459.745497	83.204030	66.015578
1459.057867	71.876072	66.020583
1457.960918	78.112103	66.025588
1457.784313	80.790500	66.030593
1456.830528	77.463257	66.035598
1456.326888	78.421396	66.040602
1455.643766	82.671423	66.045607
1455.103971	74.475120	66.050612
1454.310625	74.189354	66.055617
1453.347642	72.806887	66.060622
1452.652657	74.289202	66.065626
1452.018508	78.755046	66.070631
1451.627917	73.408337	66.075636
1450.758543	70.250588	66.080641
1449.962368	73.345675	66.085646
1449.127307	81.340747	66.090650
1448.703323	77.345349	66.095655
1448.349224	75.640383	66.100660
1447.857776	75.169924	66.105665
1447.770320	64.657360	66.110670
1445.984842	74.971058	66.115674
1445.764224	68.882791	66.120679
1445.145477	77.414361	66.125684
1443.857784	76.046818	66.130689
1443.572126	78.089438	66.135694
1442.418641	78.447922	66.140698
1442.296067	77.863406	66.145703
1442.032512	85.961174	66.150708
1441.376326	85.653117	66.155713
1440.472184	79.013584	66.160718
1439.646232	76.345354	66.165722
1439.016528	71.953350	66.170727
1438.007711	80.388669	66.175732
1436.897321	87.120011	66.180737
1436.622898	76.601551	66.185742
1436.235184	88.070549	66.190746
1435.555091	76.959187	66.195751
1435.615911	79.313143	66.200756
1434.794417	79.391786	66.205761
1434.060691	72.219822	66.210766
1433.249469	74.283325	66.215770
1432.457079	76.853977	66.220775
1431.442666	81.426357	66.225780
1430.396489	82.204218	66.230785
1430.135302	82.688249	66.235790
1429.490208	83.290489	66.240794
1429.232961	77.090865	66.245799
1428.921239	78.146414	66.250804
1428.430142	77.657344	66.255809
1427.738665	72.171098	66.260814
1426.726650	80.772354	66.265818
1425.655838	76.303492	66.270823
1424.914972	79.965406	66.275828
1424.189048	84.621033	66.280833
1423.969425	79.794905	66.285838
1423.365055	80.910414	66.290842
1422.667110	75.147788	66.295847
1421.840195	77.648170	66.300852
1421.175076	75.370815	66.305857
1420.808104	67.377036	66.310862
1419.427673	73.312663	66.315866
1418.475983	71.230408	66.320871
1417.956510	71.381693	66.325876
1417.173366	75.071369	66.330881
1416.906042	69.293060	66.335886
1416.394194	73.224836	66.340890
1416.066624	62.861926	66.345895
1416.084995	69.556361	66.350900
1414.956610	79.559050	66.355905
1414.482827	69.884291	66.360910
1413.056905	76.674773	66.365914
1412.482418	79.753234	66.370919
1411.768195	73.061861	66.375924
1411.517437	83.843891	66.380929
1410.865312	72.539076	66.385934
1410.135213	76.693730	66.390938
1409.147441	76.569929	66.395943
1408.550692	77.199421	66.400948
1407.665990	82.231553	66.405953
1407.516082	71.786125	66.410958
1406.733339	73.109397	66.415962
1404.988711	72.731485	66.420967
1404.712099	74.778872	66.425972
1404.348803	79.132044	66.430977
1404.317325	66.984058	66.435982
1403.392469	77.157556	66.440986
1403.282240	71.417881	66.445991
1402.222607	65.572706	66.450996
1401.273380	78.961804	66.456001
1400.723968	63.887619	66.461006
1400.105302	71.212914	66.466010
1399.393312	68.717019	66.471015
1398.233598	76.234794	66.476020
1397.797773	79.327809	66.481025
1397.632235	67.629462	66.486030
1396.872258	79.928322	66.491034
1396.692070	64.725017	66.496039
1395.332888	76.055178	66.501044
1394.708936	74.257074	66.506049
1394.236954	70.091883	66.511054
1393.210736	76.043065	66.516058
1392.763943	75.243666	66.521063
1392.224350	79.347556	66.526068
1391.582255	82.699685	66.531073
1390.962857	73.315105	66.536078
1389.734626	69.200423	66.541082
1389.203310	73.589459	66.546087
1388.710002	70.245776	66.551092
1388.486095	70.967362	66.556097
1387.798314	63.928067	66.561102
1386.187397	74.140848	66.566106
1385.816004	76.866404	66.571111
1385.391591	74.061954	66.576116
1384.884994	78.683196	66.581121
1384.965984	69.147152	66.586126
1383.555957	68.724207	66.591130
1382.632783	77.798525	66.596135
1381.930940	74.345282	66.601140
1381.239678	85.468754	66.606145
1381.430316	80.414910	66.611150
1380.006244	86.121978	66.616154
1379.470824	76.678420	66.621159
1378.822537	71.787130	66.626164
1378.059469	75.218781	66.631169
1377.954241	62.803571	66.636174
1377.084886	72.362859	66.641178
1375.987504	69.818471	66.646183
1375.238828	62.456856	66.651188
1374.722552	69.983693	66.656193
1374.503121	68.991437	66.661198
1373.539592	69.698323	66.666202
1372.690561	69.193560	66.671207
1371.917050	71.037469	66.676212
1371.424867	74.170525	66.681217
1370.751232	75.349999	66.686222
1370.651767	78.639241	66.691226
1370.010097	71.678102	66.696231
1369.265291	75.778437	66.701236
1368.232249	84.977352	66.706241
1367.993949	78.131100	66.711246
1366.582929	85.262054	66.716250
1366.041933	77.648183	66.721255
1365.715004	69.449803	66.726260
1365.182494	72.383720	66.731265
1364.511469	66.376117	66.736270
1363.849104	79.022987	66.741274
1362.876443	74.688123	66.746279
1362.262480	76.018034	66.751284
1361.376832	78.019686	66.756289
1361.227778	74.692072	66.761294
1360.895527	79.836077	66.766298
1359.775694	73.610445	66.771303
1359.252940	73.570466	66.776308
1358.845835	66.622070	66.781313
1357.748523	70.510787	66.786318
1356.701706	67.455272	66.791322
1356.077068	64.213809	66.796327
1355.606485	65.083012	66.801332
1355.251580	75.073688	66.806337
1354.905374	60.993368	66.811342
1353.404214	66.172868	66.816346
1353.048702	67.287624	66.821351
1352.345201	74.410351	66.826356
1351.897999	66.172961	66.831361
1351.620192	62.940019	66.836366
1350.173577	68.661999	66.841370
1349.711561	70.814149	66.846375
1349.077457	74.790541	66.851380
1348.715621	68.978684	66.856385
1348.187853	65.589988	66.861390
1346.976434	64.879252	66.866394
1346.313895	67.698855	66.871399
1346.187326	62.051191	66.876404
1345.103023	67.644048	66.881409
1344.146547	65.100414	66.886414
1343.172263	69.495417	66.891418
1343.153622	69.856618	66.896423
1342.603899	65.023066	66.901428
1342.185601	71.238853	66.906433
1342.072055	66.537861	66.911438
1340.945380	75.695962	66.916442
1340.381755	70.878208	66.921447
1339.566703	69.631091	66.926452
1338.313661	74.588527	66.931457
1337.706351	73.162170	66.936462
1336.851652	75.850468	66.941466
1336.533254	72.032002	66.946471
1336.073088	78.251407	66.951476
1335.142133	77.831724	66.956481
1334.672904	74.794962	66.961486
1333.752922	79.020417	66.966490
1333.560611	77.168956	66.971495
1333.144919	75.897682	66.976500
1331.595510	82.689193	66.981505
1331.104388	79.093705	66.986510
1330.247653	80.537413	66.991514
1330.072226	74.066439	66.996519
1329.812112	75.944434	67.001524
1328.827192	75.393076	67.006529
1328.183127	69.319288	67.011534
1327.557527	73.875251	67.016538
1327.248246	70.546649	67.021543
1326.165689	72.897789	67.026548
1325.121752	77.127491	67.031553
1324.607451	71.952366	67.036558
1324.417367	79.912424	67.041562
1323.470795	72.892574	67.046567
1322.551962	63.461779	67.051572
1321.693952	76.557777	67.056577
1321.410235	63.734599	67.061582
1320.686049	82.612806	67.066586
1319.988520	75.566505	67.071591
1318.975671	76.289739	67.076596
1318.245030	80.639486	67.081601
1318.197597	73.484660	67.086606
1317.596139	78.520415	67.091610
1317.408573	76.042120	67.096615
1316.590806	64.904237	67.101620
1315.284566	67.371035	67.106625
1314.707181	68.517855	67.111630
1314.358287	72.243329	67.116634
1313.803581	66.438839	67.121639
1312.513012	69.695154	67.126644
1311.824747	78.910439	67.131649
1311.600549	69.788208	67.136654
1310.949397	74.909440	67.141658
1310.402142	75.074571	67.146663
1309.159075	83.370411	67.151668
1308.203544	78.388842	67.156673
1308.172462	73.264805	67.161678
1307.598020	84.788654	67.166682
1307.647870	79.411956	67.171687
1306.112893	75.230604	67.176692
1305.330380	78.232981	67.181697
1305.036854	64.460609	67.186702
1304.611564	74.079271	67.191706
1303.693444	76.659622	67.196711
1302.848472	69.003863	67.201716
1302.409849	80.722736	67.206721
1301.743330	64.749721	67.211726
1301.246187	77.356068	67.216730
1300.030174	81.134467	67.221735
1299.370060	64.888396	67.226740
1298.559268	72.567493	67.231745
1298.541168	73.325293	67.236750
1298.107560	79.094516	67.241754
1296.905469	67.375488	67.246759
1296.421982	71.128345	67.251764
1295.633097	85.178786	67.256769
1295.408981	78.645099	67.261774
1294.040047	71.192325	67.266778
1293.155308	71.428654	67.271783
1292.773370	73.015678	67.276788
1291.834117	78.406092	67.281793
1291.860834	70.101788	67.286798
1291.211952	80.478302	67.291802
1290.739194	82.174029	67.296807
1289.591416	74.480509	67.301812
1289.007482	81.841708	67.306817
1288.677865	71.154313	67.311822
1287.856034	81.696219	67.316826
1286.604057	78.497823	67.321831
1286.324502	78.489633	67.326836
1285.378373	77.229046	67.331841
1285.289361	76.627342	67.336846
1284.894316	77.730319	67.341850
1284.133634	71.224156	67.346855
1283.180620	66.902134	67.351860
1282.371936	77.524677	67.356865
1282.037622	85.323121	67.361870
1280.869672	76.337591	67.366874
1280.334345	75.121539	67.371879
1279.519577	77.923399	67.376884
1278.911894	74.618652	67.381889
1278.771776	74.650535	67.386894
1278.078283	85.223365	67.391898
1276.922572	79.529662	67.396903
1276.604974	78.368699	67.401908
1275.713350	87.109224	67.406913
1275.560092	82.052679	67.411918
1274.795192	86.391719	67.416922
1273.743316	72.930745	67.421927
1273.128872	74.375216	67.426932
1272.669209	84.608424	67.431937
1272.085561	75.627860	67.436942
1270.748583	70.771209	67.441946
1269.968725	81.169752	67.446951
1269.802478	78.825171	67.451956
1269.040443	85.775174	67.456961
1268.776475	75.941763	67.461966
1268.423906	81.575934	67.466970
1267.224244	75.144927	67.471975
1266.733279	72.240969	67.476980
1265.874579	77.702854	67.481985
1265.530996	78.561771	67.486990
1264.570934	77.406989	67.491994
1263.682522	75.381034	67.496999
1263.644054	70.895734	67.502004
1263.065835	74.219571	67.507009
1262.272597	66.269980	67.512014
1261.005912	72.962576	67.517018
1260.301182	68.000845	67.522023
1259.984627	75.101540	67.527028
1259.177638	68.633311	67.532033
1258.846891	66.110852	67.537038
1257.729290	71.850734	67.542042
1256.890407	65.134558	67.547047
1256.616847	73.187449	67.552052
1255.947757	77.314701	67.557057
1255.701769	64.601912	67.562062
1254.931629	72.732319	67.567066
1254.045095	75.532653	67.572071
1253.618956	67.885724	67.577076
1252.981358	71.571815	67.582081
1252.150513	68.636052	67.587086
1251.149484	70.870227	67.592090
1250.453626	67.644525	67.597095
1250.163654	69.330275	67.602100
1249.742499	77.692634	67.607105
1248.789789	65.000187	67.612110
1247.817784	72.718729	67.617114
1247.079853	65.320963	67.622119
1246.520119	72.911689	67.627124
1246.131347	80.321972	67.632129
1246.153189	69.820719	67.637134
1244.698827	74.674094	67.642138
1243.665196	73.388629	67.647143
1243.180345	70.913475	67.652148
1242.732604	77.407846	67.657153
1242.532835	74.283123	67.662158
1241.572595	74.265558	67.667162
1240.439359	82.729701	67.672167
1240.123890	71.302954	67.677172
1239.140410	74.906955	67.682177
1239.134427	74.147754	67.687182
1238.602434	75.827575	67.692186
1237.713280	71.913819	67.697191
1237.054643	74.379494	67.702196
1236.559556	83.126338	67.707201
1235.820364	71.458730	67.712206
1234.704336	74.062711	67.717210
1233.986959	65.800154	67.722215
1233.860012	68.708458	67.727220
1233.183692	76.539399	67.732225
1232.099846	74.350737	67.737230
1231.258558	73.957167	67.742234
1230.801018	73.451321	67.747239
1230.364521	68.559324	67.752244
1230.102596	69.283873	67.757249
1228.892110	75.282019	67.762254
1227.984223	70.555592	67.767258
1227.254837	70.006292	67.772263
1227.282126	69.472306	67.777268
1226.348130	80.288800	67.782273
1225.305656	73.973387	67.787278
1224.615197	77.069745	67.792282
1224.139724	75.056386	67.797287
1223.874601	80.841762	67.802292
1223.493087	84.261788	67.807297
1222.543833	77.830551	67.812302
1221.440111	71.223274	67.817306
1220.822694	79.292014	67.822311
1220.604965	72.576860	67.827316
1219.931794	74.461239	67.832321
1218.747329	72.862936	67.837326
1217.802423	75.925888	67.842330
1217.194006	73.764379	67.847335
1217.482762	70.481417	67.852340
1216.707360	84.006153	67.857345
1216.343650	69.745309	67.862350
1214.987983	82.317469	67.867354
1214.143089	78.962164	67.872359
1213.967215	70.036532	67.877364
1213.367401	65.621293	67.882369
1212.649228	64.620889	67.887374
1211.625104	65.452647	67.892378
1210.956892	72.772619	67.897383
1210.719570	67.584037	67.902388
1209.122640	77.524870	67.907393
1208.691721	71.757621	67.912398
1208.071466	67.423247	67.917402
1208.030035	69.744964	67.922407
1207.739008	73.654340	67.927412
1206.717018	71.697450	67.932417
1205.987262	64.986285	67.937422
1205.334531	68.513136	67.942426
1204.358802	71.018105	67.947431
1204.412739	66.704875	67.952436
1203.006644	72.214304	67.957441
1202.444016	69.317493	67.962446
1201.508033	74.669465	67.967450
1200.898626	73.526498	67.972455
1200.832236	66.987532	67.977460
1200.122831	75.914348	67.982465
1199.416136	71.507147	67.987470
1198.520102	76.212443	67.992474
1198.151227	70.196559	67.997479
1197.249390	72.055752	68.002484
1196.373317	80.634546	68.007489
1195.670859	73.619510	68.012494
1195.262695	77.400134	68.017498
1194.735771	76.471192	68.022503
1194.322760	68.252448	68.027508
1193.096663	72.306132	68.032513
1192.341556	65.152097	68.037518
1192.249384	73.377209	68.042522
1191.643168	79.335848	68.047527
1190.198992	73.245136	68.052532
1189.674614	78.193496	68.057537
1189.668319	68.276513	68.062542
1188.800247	72.849528	68.067546
1188.286593	75.139208	68.072551
1186.914040	65.527596	68.077556
1186.383552	74.064585	68.082561
1186.022353	67.137960	68.087566
1185.697567	67.758411	68.092570
1184.923836	71.476499	68.097575
1183.843056	61.935717	68.102580
1182.927307	71.478095	68.107585
1182.955833	66.237683	68.112590
1182.580216	72.542081	68.117594
1181.526801	73.996988	68.122599
1180.938888	68.884224	68.127604
1180.095015	81.995177	68.132609
1179.722020	68.294458	68.137614
1178.437675	69.059072	68.142618
1177.492523	76.881573	68.147623
1177.141706	64.369108	68.152628
1177.090708	78.938961	68.157633
1176.355414	73.343430	68.162638
1175.813296	70.772305	68.167642
1174.687896	78.539621	68.172647
1174.259470	70.370490	68.177652
1173.065246	84.374285	68.182657
1172.677711	72.292027	68.187662
1172.328067	68.494718	68.192666
1171.204561	64.155338	68.197671
1170.581948	63.789862	68.202676
1169.960872	72.906806	68.207681
1169.827997	73.014817	68.212686
1169.176364	73.462296	68.217690
1168.071166	77.887635	68.222695
1167.209437	77.558363	68.227700
1166.807467	75.438483	68.232705
1166.428060	68.511820	68.237710
1166.037561	72.468226	68.242714
1164.879548	71.869174	68.247719
1164.524576	70.201882	68.252724
1163.152352	77.411491	68.257729
1162.876346	62.942632	68.262734
1161.823845	77.251744	68.267738
1161.058892	72.841894	68.272743
1160.668958	66.610159	68.277748
1160.261849	74.271067	68.282753
1159.861126	69.638994	68.287758
1159.295849	73.660061	68.292762
1158.610701	78.075057	68.297767
1158.018281	65.759086	68.302772
1157.234056	75.098167	68.307777
1156.494922	74.194513	68.312782
1155.239543	68.556992	68.317786
1154.394189	73.452158	68.322791
1154.135030	62.373406	68.327796
1153.456266	76.247887	68.332801
1153.322187	74.691977	68.337806
1152.825688	70.042358	68.342810
1151.456579	78.670838	68.347815
1151.101958	70.709326	68.352820
1150.739701	73.593188	68.357825
1149.583620	73.034070	68.362830
1148.179340	72.971374	68.367834
1147.571083	74.063106	68.372839
1147.445318	70.033265	68.377844
1146.955081	83.240766	68.382849
1146.727953	71.640629	68.387854
1146.365555	76.445209	68.392858
1145.384546	79.732634	68.397863
1144.309091	71.348258	68.402868
1143.527194	80.109079	68.407873
1143.641633	70.094062	68.412878
1142.391726	80.358368	68.417882
1141.378429	76.143800	68.422887
1140.966861	64.152508	68.427892
1140.467371	70.412198	68.432897
1140.049149	72.494499	68.437902
1139.469882	74.352545	68.442906
1138.317993	75.893791	68.447911
1137.925057	72.673869	68.452916
1137.006581	75.292199	68.457921
1136.865975	77.882727	68.462926
1135.883885	74.666188	68.467930
1134.897324	78.231656	68.472935
1134.876437	76.649655	68.477940
1133.948361	70.868865	68.482945
1133.006264	72.155911	68.487950
1132.379265	71.060175	68.492954
1131.650687	78.210499	68.497959
1131.656278	71.686447	68.502964
1130.783946	75.436030	68.507969
1129.694422	73.431119	68.512974
1128.801542	69.163175	68.517978
1128.347960	66.072844	68.522983
1128.012041	74.248904	68.527988
1126.993166	79.011557	68.532993
1126.929853	76.357269	68.537998
1125.895423	74.275823	68.543002
1125.094035	68.528209	68.548007
1124.758732	68.164461	68.553012
1124.180800	78.589614	68.558017
1123.108179	70.936960	68.563022
1122.308864	82.899159	68.568026
1121.624230	80.945308	68.573031
1121.692374	75.376813	68.578036
1120.967102	77.624580	68.583041
1120.118802	75.782435	68.588046
1119.527903	73.402424	68.593050
1118.748802	75.750983	68.598055
1118.582928	70.312951	68.603060
1117.173027	78.122674	68.608065
1116.711996	69.159440	68.613070
1115.921084	71.573570	68.618074
1115.004716	71.288399	68.623079
1114.685550	66.809333	68.628084
1113.390268	72.474668	68.633089
1112.934374	64.888909	68.638094
1112.768212	72.263438	68.643098
1112.195003	75.671293	68.648103
1112.041240	64.906063	68.653108
1111.127753	78.213267	68.658113
1110.347638	71.759416	68.663118
1109.470999	69.459517	68.668122
1108.202634	71.301753	68.673127
1107.419059	72.083263	68.678132
1106.705517	82.428618	68.683137
1107.380021	73.283575	68.688142
1106.609380	65.674742	68.693146
1105.779362	67.256006	68.698151
1104.841869	67.309569	68.703156
1103.916154	76.920764	68.708161
1103.011812	72.567161	68.713166
1102.896608	70.550150	68.718170
1102.167581	77.955145	68.723175
1101.575642	66.764838	68.728180
1100.777834	67.360112	68.733185
1100.178427	68.579406	68.738190
1099.678126	72.007538	68.743194
1099.010496	71.332032	68.748199
1098.112107	69.597937	68.753204
1097.058168	71.260965	68.758209
1096.838775	68.344473	68.763214
1096.441098	72.162776	68.768218
1095.777888	76.328900	68.773223
1095.132907	68.430539	68.778228
1093.762972	72.361249	68.783233
1093.450753	72.963370	68.788238
1093.048090	72.745362	68.793242
1092.023787	75.474184	68.798247
1091.226781	69.802007	68.803252
1090.294709	80.447663	68.808257
1090.000686	77.821435	68.813262
1089.855686	66.337111	68.818266
1089.124779	67.646420	68.823271
1088.846486	65.399981	68.828276
1087.536377	66.456383	68.833281
1087.026032	69.847948	68.838286
1086.490223	71.295946	68.843290
1085.643073	72.549376	68.848295
1085.174811	73.014015	68.853300
1084.751608	76.632621	68.858305
1083.855957	70.093171	68.863310
1082.603040	69.105016	68.868314
1081.413265	81.061448	68.873319
1081.048834	68.436862	68.878324
1080.612669	75.193318	68.883329
1080.383986	73.209949	68.888334
1080.060436	74.781857	68.893338
1079.895248	78.589954	68.898343
1078.888992	73.947902	68.903348
1077.486394	82.358328	68.908353
1077.334563	79.427504	68.913358
1076.576510	74.169032	68.918362
1075.387273	84.685447	68.923367
1075.094275	78.246867	68.928372
1074.585578	75.085062	68.933377
1074.137890	74.350582	68.938382
1072.979709	76.748272	68.943386
1072.148380	81.033578	68.948391
1072.056893	70.342945	68.953396
1071.101971	77.089554	68.958401
1069.977984	72.339382	68.963406
1069.428864	70.871915	68.968410
1068.559955	77.017246	68.973415
1068.380735	70.201968	68.978420
1067.812808	75.041349	68.983425
1067.522296	73.717089	68.988430
1067.255314	68.482682	68.993434
1065.688686	63.500433	68.998439
1065.584850	70.196426	69.003444
1064.499562	80.533206	69.008449
1063.208082	69.057717	69.013454
1062.973591	69.665081	69.018458
1062.207733	71.048665	69.023463
1061.945860	66.864121	69.028468
1061.740304	73.821074	69.033473
1060.650515	72.041608	69.038478
1060.108501	70.926986	69.043482
1059.194470	70.308679	69.048487
1059.020794	68.962044	69.053492
1057.753736	76.650218	69.058497
1057.047992	70.479681	69.063502
1056.197343	66.771731	69.068506
1055.469742	73.709139	69.073511
1055.137297	66.552227	69.078516
1054.853688	74.011205	69.083521
1054.097942	66.206028	69.088526
1053.501694	68.753797	69.093530
1052.248107	70.428918	69.098535
1051.995934	64.741606	69.103540
1051.286527	73.378706	69.108545
1050.325540	64.468340	69.113550
1049.519702	66.416111	69.118554
1048.871480	72.661802	69.123559
1048.885340	69.114875	69.128564
1048.167362	70.497761	69.133569
1047.631552	74.902192	69.138574
1046.356168	76.921293	69.143578
1045.858222	74.265652	69.148583
1045.346065	65.235403	69.153588
1045.043790	70.712942	69.158593
1044.138915	66.043277	69.163598
1043.239505	66.109276	69.168602
1042.124073	71.052677	69.173607
1042.387001	62.546115	69.178612
1041.873726	71.293304	69.183617
1040.706910	70.938540	69.188622
1040.052272	72.332685	69.193626
1039.367024	74.359672	69.198631
1039.364296	61.994460	69.203636
1038.178138	69.545628	69.208641
1037.276415	74.167054	69.213646
1037.073504	70.068725	69.218650
1035.969663	79.417157	69.223655
1035.444970	67.514333	69.228660
1034.081877	74.650564	69.233665
1033.983351	76.145257	69.238670
1033.817317	73.043983	69.243674
1033.181199	79.679953	69.248679
1032.182022	68.090872	69.253684
1031.390030	69.198687	69.258689
1030.970740	73.521194	69.263694
1030.711905	69.516122	69.268698
1029.188212	73.901446	69.273703
1028.632385	68.125222	69.278708
1027.813966	82.637011	69.283713
1027.248261	66.544979	69.288718
1027.174085	77.865919	69.293722
1026.195124	80.076225	69.298727
1025.744035	74.849271	69.303732
1024.601115	71.226508	69.308737
1024.169168	70.912078	69.313742
1023.698486	73.955426	69.318746
1022.553106	77.542584	69.323751
1022.096344	77.383581	69.328756
1021.185821	79.110876	69.333761
1020.933779	80.700145	69.338766
1020.537275	68.336052	69.343770
1019.807142	73.084798	69.348775
1018.951116	76.341366	69.353780
1017.891953	71.677997	69.358785
1017.197993	68.266890	69.363790
1017.042422	63.188665	69.368794
1016.693373	74.612724	69.373799
1015.947356	66.566691	69.378804
1014.452424	72.017959	69.383809
1014.063980	72.993119	69.388814
1014.080292	63.270829	69.393818
1012.900573	70.014888	69.398823
1012.470170	62.006384	69.403828
1011.183823	70.542164	69.408833
1010.831822	60.926764	69.413838
1010.360008	72.343424	69.418842
1010.021514	68.437650	69.423847
1009.105649	64.259325	69.428852
1008.065516	67.092314	69.433857
1007.593296	74.784502	69.438862
1007.292148	67.294227	69.443866
1006.146341	79.659168	69.448871
1005.595625	64.072578	69.453876
1004.758749	76.426845	69.458881
1004.141000	68.915793	69.463886
1004.028150	76.837345	69.468890
1003.437357	74.390626	69.473895
1002.549697	67.793779	69.478900
1001.704506	68.929260	69.483905
1001.231807	74.876490	69.488910
1000.784579	68.809318	69.493914
999.689991	68.779283	69.498919
999.098599	58.162437	69.503924
998.244934	74.901323	69.508929
997.808295	62.381884	69.513934
997.326847	66.542939	69.518938
996.142223	65.503246	69.523943
995.716193	65.263196	69.528948
995.048701	76.960463	69.533953
994.666919	65.408157	69.538958
994.212191	66.539926	69.543962
992.806628	68.920789	69.548967
992.093829	64.003912	69.553972
991.434219	63.053115	69.558977
991.198660	66.707874	69.563982
991.161301	65.508810	69.568986
989.862591	64.580230	69.573991
989.185988	60.802623	69.578996
988.885415	61.345915	69.584001
987.753451	65.232737	69.589006
987.013575	65.055516	69.594010
986.015214	67.598738	69.599015
985.615907	62.336480	69.604020
984.974823	72.808759	69.609025
984.454684	68.406360	69.614030
984.287020	63.254029	69.619034
983.615967	70.264252	69.624039
983.270081	69.503268	69.629044
982.451050	75.669275	69.634049
981.367618	66.152693	69.639054
980.498990	65.347819	69.644058
979.548482	69.519341	69.649063
979.188794	67.216986	69.654068
978.872132	73.321825	69.659073
977.901611	75.460040	69.664078
977.195874	64.360698	69.669082
976.318154	75.832270	69.674087
975.837631	65.794038	69.679092
975.416159	67.739938	69.684097
974.870026	67.417044	69.689102
973.947079	76.011776	69.694106
972.992314	80.002460	69.699111
972.525832	67.948769	69.704116
972.215731	73.710265	69.709121
971.405612	74.983817	69.714126
970.461517	66.290043	69.719130
969.894130	80.641213	69.724135
969.766651	70.420944	69.729140
968.985973	66.234870	69.734145
967.934840	63.137560	69.739150
967.434063	66.511310	69.744154
966.672191	69.755311	69.749159
966.101828	68.102427	69.754164
965.624145	73.368046	69.759169
964.920684	68.877052	69.764174
964.051818	64.930281	69.769178
963.337846	79.756531	69.774183
963.219705	63.606816	69.779188
961.788491	73.498794	69.784193
961.040002	71.476568	69.789198
960.773509	64.332848	69.794202
959.906271	69.463087	69.799207
959.886608	65.211810	69.804212
958.679522	69.193210	69.809217
958.103066	72.864514	69.814222
957.268673	72.771375	69.819226
956.865743	69.070448	69.824231
956.668681	68.245691	69.829236
955.565863	60.643262	69.834241
954.526154	69.500345	69.839246
954.154835	69.359082	69.844250
953.214997	70.939443	69.849255
953.219894	76.656861	69.854260
952.385552	80.463907	69.859265
951.292002	73.592875	69.864270
950.920531	70.070104	69.869274
949.902640	71.511867	69.874279
949.595273	66.104400	69.879284
949.083523	69.435428	69.884289
948.289601	76.676688	69.889294
947.654743	68.092976	69.894298
946.906551	68.851083	69.899303
946.548444	65.862839	69.904308
945.475762	72.187941	69.909313
944.828217	73.342079	69.914318
944.170362	63.715916	69.919322
943.750084	70.969757	69.924327
943.065716	62.717011	69.929332
942.026803	65.004305	69.934337
941.313983	66.462502	69.939342
941.007508	63.108592	69.944346
940.373664	73.152944	69.949351
940.246864	64.513011	69.954356
939.109188	67.132993	69.959361
938.253101	68.486260	69.964366
938.002935	65.315722	69.969370
937.058526	76.606098	69.974375
936.432103	57.395584	69.979380
935.461553	65.962548	69.984385
935.152017	68.065718	69.989390
934.877526	69.156360	69.994394
933.387519	69.291556	69.999399
933.042980	69.695548	70.004404
932.480202	63.714886	70.009409
932.056925	70.240989	70.014414
930.911547	65.369791	70.019418
929.710098	71.487620	70.024423
929.646559	67.633049	70.029428
928.835602	67.246574	70.034433
928.347982	66.063445	70.039438
928.173527	72.006962	70.044442
927.361121	66.741650	70.049447
926.464561	63.414598	70.054452
925.606906	68.522280	70.059457
924.544177	77.343446	70.064462
924.588492	74.045898	70.069466
923.987945	74.618862	70.074471
923.302124	76.249665	70.079476
922.295192	75.571509	70.084481
921.484402	74.017042	70.089486
921.415904	62.868573	70.094490
920.801327	73.044223	70.099495
919.772463	73.259910	70.104500
919.019298	77.542504	70.109505
918.348960	77.878750	70.114510
918.308903	66.704094	70.119514
916.890416	76.123400	70.124519
916.486115	75.844901	70.129524
915.649971	77.650654	70.134529
915.233011	81.426481	70.139534
914.995713	64.361706	70.144538
913.954331	74.175874	70.149543
913.025665	70.013183	70.154548
912.613243	71.026797	70.159553
911.858542	76.877073	70.164558
911.712241	69.725403	70.169562
910.316221	71.824405	70.174567
909.922964	69.645431	70.179572
909.524459	75.017485	70.184577
908.787512	72.903296	70.189582
907.664579	67.813535	70.194586
906.726439	75.399218	70.199591
906.477138	65.431129	70.204596
906.081930	68.233806	70.209601
905.370124	78.352695	70.214606
905.166278	69.540838	70.219610
903.862739	77.435013	70.224615
903.049325	67.266320	70.229620
902.688767	76.174057	70.234625
902.029479	73.623432	70.239630
901.719068	63.699758	70.244634
900.663228	73.965195	70.249639
899.720169	69.662085	70.254644
899.308760	70.878016	70.259649
898.851522	74.567982	70.264654
898.119267	75.069565	70.269658
896.918767	70.342414	70.274663
896.537612	69.671158	70.279668
895.808267	65.052381	70.284673
895.490819	63.633674	70.289678
895.234627	61.798708	70.294682
894.048768	74.273930	70.299687
893.425225	60.509228	70.304692
892.961112	69.648633	70.309697
892.438701	69.819817	70.314702
891.239643	65.059661	70.319706
890.167903	71.904057	70.324711
890.108256	74.407301	70.329716
889.736371	65.748959	70.334721
889.069992	70.233390	70.339726
888.123329	65.527106	70.344730
886.897709	75.543350	70.349735
886.698442	63.609695	70.354740
886.193206	64.825908	70.359745
885.710037	70.675859	70.364750
885.101866	60.946865	70.369754
883.704730	72.776995	70.374759
883.354975	74.790351	70.379764
882.971338	65.288146	70.384769
882.415906	65.880228	70.389774
881.813156	64.534070	70.394778
880.606571	73.699600	70.399783
880.302317	72.288896	70.404788
879.978722	76.040837	70.409793
878.876264	69.255034	70.414798
877.998185	61.229683	70.419802
877.212069	76.350112	70.424807
876.739087	74.849498	70.429812
876.399899	77.289312	70.434817
875.586655	74.618227	70.439822
874.764053	69.070082	70.444826
873.614416	74.345802	70.449831
873.149102	62.689021	70.454836
873.042503	69.467578	70.459841
872.783874	72.821175	70.464846
872.453133	67.302859	70.469850
870.944205	68.807821	70.474855
870.654355	70.785655	70.479860
869.782740	72.180275	70.484865
868.700184	71.064319	70.489870
868.122416	65.330170	70.494874
867.273678	67.165716	70.499879
866.990530	69.620009	70.504884
866.845495	69.619985	70.509889
865.755947	73.330628	70.514894
864.753718	73.742674	70.519898
864.166155	74.581433	70.524903
864.135705	67.701226	70.529908
863.339489	72.547354	70.534913
862.304814	74.502376	70.539918
861.856420	68.316223	70.544922
861.332270	81.800293	70.549927
860.560086	73.589048	70.554932
859.324560	69.125263	70.559937
858.282492	75.156205	70.564942
858.214248	72.756181	70.569946
857.476957	69.390416	70.574951
857.159111	67.309842	70.579956
857.021725	69.976392	70.584961
855.939560	73.453680	70.589966
855.359779	69.143617	70.594970
854.329004	72.661442	70.599975
854.137078	70.502460	70.604980
852.829394	70.914331	70.609985
851.477191	63.239392	70.614990
851.180058	75.575421	70.619994
850.663117	72.229938	70.624999
850.774291	73.172425	70.630004
850.675629	66.656780	70.635009
849.981248	66.394027	70.640014
848.488076	68.371141	70.645018
847.670407	69.699290	70.650023
847.309213	69.358549	70.655028
846.257676	69.082371	70.660033
845.579067	70.454199	70.665038
844.941608	60.574713	70.670042
844.054622	65.493622	70.675047
844.168587	63.005157	70.680052
843.582938	66.516999	70.685057
842.766446	65.855580	70.690062
842.013758	68.293593	70.695066
841.370118	72.707032	70.700071
840.886776	69.586705	70.705076
839.809146	73.341099	70.710081
838.740674	78.918302	70.715086
838.431571	70.399599	70.720090
838.092318	75.943865	70.725095
837.580235	68.674472	70.730100
836.441503	72.754710	70.735105
835.278282	75.330145	70.740110
835.157688	64.405731	70.745114
834.568745	77.055808	70.750119
834.193591	70.631730	70.755124
833.947334	71.013762	70.760129
832.942123	72.591526	70.765134
832.088137	73.057130	70.770138
831.486354	79.191863	70.775143
830.770066	70.318587	70.780148
829.758289	72.781640	70.785153
829.097917	79.924645	70.790158
829.007124	67.457311	70.795162
828.258059	72.782840	70.800167
827.308189	69.805185	70.805172
826.634921	70.031820	70.810177
826.066041	74.209046	70.815182
825.677024	72.886677	70.820186
824.675971	77.488438	70.825191
824.185297	70.341688	70.830196
823.540463	75.212020	70.835201
822.941064	72.868639	70.840206
822.283062	70.747258	70.845210
821.200034	77.217830	70.850215
820.517206	72.897793	70.855220
820.245426	64.273630	70.860225
819.742070	71.453285	70.865230
818.851650	70.018261	70.870234
817.867442	76.829124	70.875239
817.067426	72.136419	70.880244
816.539629	65.759411	70.885249
816.075439	77.084769	70.890254
815.894453	64.203438	70.895258
814.889521	71.789124	70.900263
814.290452	68.507449	70.905268
813.321224	70.436665	70.910273
813.276616	73.762682	70.915278
812.385463	62.787904	70.920282
811.883950	73.241409	70.925287
810.922539	68.977778	70.930292
809.959782	69.014015	70.935297
808.972422	66.113440	70.940302
808.368906	58.660388	70.945306
807.877544	65.576685	70.950311
807.427673	63.926866	70.955316
807.421727	71.260122	70.960321
806.693010	71.391657	70.965326
805.929431	61.924552	70.970330
804.876859	74.123940	70.975335
804.315939	69.563168	70.980340
803.786469	65.537376	70.985345
802.589672	68.550387	70.990350
802.083640	61.920196	70.995354
801.099643	74.502948	71.000359
800.930792	66.586643	71.005364
800.515160	62.718974	71.010369
799.615080	70.998372	71.015374
798.763627	62.077214	71.020378
797.641373	75.990947	71.025383
797.751085	68.157576	71.030388
797.226736	64.768769	71.035393
796.775241	74.228497	71.040398
796.073815	69.191295	71.045402
794.627086	67.200683	71.050407
794.167047	63.874672	71.055412
793.673558	63.695930	71.060417
793.017843	72.187273	71.065422
792.218020	67.452702	71.070426
791.367941	71.302329	71.075431
791.004201	70.164702	71.080436
790.234471	67.385134	71.085441
790.093803	69.389914	71.090446
789.914554	62.525336	71.095450
788.277841	68.713406	71.100455
787.696757	68.722556	71.105460
787.294376	63.565057	71.110465
785.839069	67.921756	71.115470
785.169565	68.877186	71.120474
784.605092	74.700018	71.125479
784.289096	79.665596	71.130484
783.841301	70.135715	71.135489
783.364488	75.458427	71.140494
783.124355	63.691254	71.145498
782.146686	73.277034	71.150503
781.227785	66.940187	71.155508
780.872500	69.592750	71.160513
779.454952	72.396489	71.165518
778.872820	65.028982	71.170522
778.198407	76.436530	71.175527
778.059779	70.698615	71.180532
777.808095	65.425308	71.185537
776.430488	72.734987	71.190542
775.720299	60.669017	71.195546
774.923580	76.039932	71.200551
774.419698	64.101636	71.205556
774.113266	66.747804	71.210561
772.879170	72.607978	71.215566
772.309778	57.953821	71.220570
771.655863	59.896132	71.225575
771.369313	60.735834	71.230580
771.192241	73.605075	71.235585
769.871808	76.319948	71.240590
769.708922	61.744171	71.245594
768.853486	67.438828	71.250599
767.703082	64.049906	71.255604
767.254649	66.810788	71.260609
766.393407	71.025863	71.265614
766.418241	68.798968	71.270618
765.305254	75.894778	71.275623
764.388020	58.800474	71.280628
763.460059	64.239147	71.285633
762.463060	74.564779	71.290638
762.399861	64.820216	71.295642
762.065241	64.527426	71.300647
761.785167	66.113610	71.305652
761.403202	65.738935	71.310657
759.802950	70.961215	71.315662
759.519716	64.554166	71.320666
758.799909	66.840907	71.325671
757.882354	67.735811	71.330676
756.989973	67.249241	71.335681
756.468868	66.444085	71.340686
756.068726	65.884245	71.345690
755.643315	73.614994	71.350695
755.061676	66.905397	71.355700
753.803836	64.790472	71.360705
753.135243	70.658771	71.365710
752.868448	68.311316	71.370714
752.304981	70.592591	71.375719
751.454439	71.491016	71.380724
750.532820	67.262423	71.385729
749.652663	74.845690	71.390734
749.478532	58.039731	71.395738
749.318258	72.428112	71.400743
748.459804	65.632523	71.405748
747.254753	63.377906	71.410753
746.865276	71.298277	71.415758
746.419121	59.829682	71.420762
744.948218	75.938553	71.425767
743.958152	66.023576	71.430772
743.931620	63.938895	71.435777
743.335975	68.055188	71.440782
742.854626	52.671132	71.445786
742.446051	63.727623	71.450791
742.057778	66.460833	71.455796
741.310852	68.773142	71.460801
739.934977	63.914645	71.465806
739.996460	63.567422	71.470810
739.078242	60.145839	71.475815
737.948429	56.084357	71.480820
737.102615	58.608594	71.485825
736.456727	70.374785	71.490830
736.403715	62.015905	71.495834
735.819625	66.192189	71.500839
735.112083	59.047482	71.505844
734.193411	59.167756	71.510849
733.524417	70.819096	71.515854
733.315510	64.272614	71.520858
732.010540	53.792681	71.525863
731.146841	57.405053	71.530868
730.690195	50.474725	71.535873
730.097285	63.782275	71.540878
730.246017	68.894015	71.545882
729.149299	67.119370	71.550887
727.782066	71.582175	71.555892
727.898465	60.630600	71.560897
726.898634	65.978175	71.565902
726.546108	62.442318	71.570906
726.024498	66.559349	71.575911
724.805129	64.841241	71.580916
724.556336	56.509195	71.585921
723.828277	61.544174	71.590926
722.594960	63.453519	71.595930
722.159752	57.764843	71.600935
721.565377	64.086980	71.605940
721.597236	57.961468	71.610945
720.636266	62.132845	71.615950
719.377362	60.390724	71.620954
718.856366	71.005450	71.625959
718.469676	63.136343	71.630964
718.016822	58.068814	71.635969
717.102707	67.738835	71.640974
716.382748	63.279531	71.645978
715.302665	67.385268	71.650983
714.966447	61.204791	71.655988
714.816995	57.793218	71.660993
713.835020	68.680324	71.665998
712.951699	62.678436	71.671002
712.579121	69.869240	71.676007
711.688095	69.440470	71.681012
711.459919	64.631670	71.686017
709.975875	69.489074	71.691022
709.588613	65.651686	71.696026
709.086613	68.511349	71.701031
708.525195	73.043338	71.706036
708.101259	71.956687	71.711041
707.241211	72.222046	71.716046
706.680486	66.144762	71.721050
705.634572	62.384687	71.726055
705.392057	66.047350	71.731060
704.561638	67.267186	71.736065
703.268963	68.628183	71.741070
703.031806	61.604993	71.746074
701.827205	69.104509	71.751079
701.720393	64.456488	71.756084
701.564262	63.301855	71.761089
701.073075	71.279910	71.766094
700.162166	67.700775	71.771098
699.304631	72.497429	71.776103
698.726808	66.798844	71.781108
698.498520	69.340448	71.786113
697.095308	73.363002	71.791118
696.326088	61.101520	71.796122
695.473584	70.443244	71.801127
695.411942	75.179730	71.806132
695.014910	63.684966	71.811137
694.025819	71.690298	71.816142
693.019880	60.533128	71.821146
692.572651	59.420866	71.826151
692.003713	69.717770	71.831156
691.169074	56.202834	71.836161
690.010271	64.210396	71.841166
689.972167	62.066913	71.846170
689.375602	63.508778	71.851175
688.928998	71.674186	71.856180
688.500854	66.985693	71.861185
686.875495	72.089933	71.866190
686.402608	62.609372	71.871194
685.715011	60.593737	71.876199
685.441750	60.159001	71.881204
685.023481	64.154520	71.886209
683.716342	64.334250	71.891214
683.484998	60.280297	71.896218
683.043937	65.214405	71.901223
682.305864	60.757423	71.906228
681.298649	61.200753	71.911233
680.132055	63.667462	71.916238
680.125276	60.287497	71.921242
679.641242	63.463408	71.926247
679.063285	59.593962	71.931252
678.456066	58.905404	71.936257
677.353147	60.419415	71.941262
677.482055	52.173057	71.946266
676.130689	61.973247	71.951271
674.823660	59.512319	71.956276
674.526312	60.632149	71.961281
673.709122	64.772587	71.966286
673.521287	63.464711	71.971290
673.134992	62.703176	71.976295
672.781894	70.566789	71.981300
672.085641	64.384055	71.986305
670.790158	72.608055	71.991310
670.171042	61.051877	71.996314
668.740261	68.681327	72.001319
668.016640	68.141390	72.006324
667.705414	61.769543	72.011329
667.427217	62.342965	72.016334
666.996761	56.171537	72.021338
666.481551	65.886898	72.026343
665.745881	61.108999	72.031348
665.302073	60.063255	72.036353
664.009638	70.737123	72.041358
663.727587	60.842974	72.046362
663.442123	63.676199	72.051367
662.329807	62.690515	72.056372
661.737253	56.427655	72.061377
660.812099	63.808252	72.066382
660.626571	63.363617	72.071386
659.430521	60.189771	72.076391
658.692720	67.045273	72.081396
658.153252	69.264027	72.086401
657.520946	67.230634	72.091406
657.241741	65.418574	72.096410
656.010435	72.374810	72.101415
655.080711	67.996453	72.106420
654.591385	66.112634	72.111425
653.951430	68.937519	72.116430
654.055345	66.062771	72.121434
653.484302	72.981674	72.126439
652.761372	68.755378	72.131444
651.973349	71.373934	72.136449
650.971384	73.849153	72.141454
650.423109	66.459293	72.146458
649.355725	65.030938	72.151463
648.770315	57.654944	72.156468
648.153448	61.696331	72.161473
647.549696	66.283730	72.166478
647.302480	60.391155	72.171482
646.671023	62.595671	72.176487
645.621371	62.624329	72.181492
645.104135	53.158880	72.186497
644.377243	59.006383	72.191502
644.047762	55.039903	72.196506
643.156594	59.609046	72.201511
642.225660	57.407753	72.206516
641.574037	62.387016	72.211521
640.955225	56.715204	72.216526
640.769833	58.106760	72.221530
639.519421	63.886072	72.226535
638.658529	68.103077	72.231540
638.270055	64.089469	72.236545
637.814874	70.895764	72.241550
637.567308	64.510644	72.246554
637.022002	66.589882	72.251559
635.488078	66.231011	72.256564
635.140910	63.774581	72.261569
634.405111	71.927960	72.266574
634.389235	63.608515	72.271578
632.985276	72.984728	72.276583
632.187438	68.507601	72.281588
631.705066	65.665410	72.286593
630.939459	71.911109	72.291598
630.771900	68.156477	72.296602
629.875054	72.427404	72.301607
628.897145	78.182140	72.306612
628.662400	68.703416	72.311617
627.957129	66.964750	72.316622
627.854191	59.329266	72.321626
626.592949	65.662643	72.326631
626.009845	70.899760	72.331636
625.859419	59.195009	72.336641
624.554862	75.891545	72.341646
623.781337	68.786978	72.346650
622.915923	66.952599	72.351655
622.472522	70.997820	72.356660
622.383370	65.380517	72.361665
621.122722	71.998385	72.366670
620.320593	59.799404	72.371674
619.654554	65.608855	72.376679
619.106721	71.038077	72.381684
618.839510	60.786938	72.386689
618.257970	59.674013	72.391694
617.384849	63.210259	72.396698
616.464656	63.021359	72.401703
615.725263	72.557251	72.406708
615.481850	60.971453	72.411713
614.995684	65.394637	72.416718
614.002855	64.469014	72.421722
613.040956	66.105317	72.426727
612.816807	61.818834	72.431732
612.454539	57.799162	72.436737
611.451274	65.474579	72.441742
610.783801	65.953657	72.446746
609.884870	65.341534	72.451751
609.552586	68.050160	72.456756
609.031252	60.616223	72.461761
607.689795	68.483789	72.466766
607.360886	56.202946	72.471770
606.622600	64.921981	72.476775
606.202210	69.518229	72.481780
605.875014	57.619570	72.486785
604.596308	66.063719	72.491790
603.895591	55.322419	72.496794
603.344973	63.195793	72.501799
603.132888	61.057650	72.506804
602.478001	61.236958	72.511809
601.072037	61.658629	72.516814
600.600242	63.087810	72.521818
600.104897	58.097838	72.526823
599.745830	52.322720	72.531828
599.470206	51.489733	72.536833
598.256638	59.094608	72.541838
597.266872	53.107043	72.546842
596.610288	54.443156	72.551847
596.391078	61.585969	72.556852
595.289549	64.820714	72.561857
594.283511	65.435167	72.566862
594.055877	62.689065	72.571866
594.023507	56.389050	72.576871
593.419946	59.438217	72.581876
592.166854	61.268486	72.586881
591.082569	62.518415	72.591886
590.524235	63.180890	72.596890
590.295805	63.657769	72.601895
589.886821	60.510527	72.606900
588.914761	58.859814	72.611905
588.074410	61.089865	72.616910
587.656276	58.156548	72.621914
587.377636	51.476782	72.626919
586.509021	54.602544	72.631924
585.390448	57.402472	72.636929
584.388626	64.890156	72.641934
583.965041	55.285127	72.646938
583.634742	61.005872	72.651943
582.964783	60.912254	72.656948
583.203623	52.710221	72.661953
582.189676	67.179716	72.666958
581.189445	53.002834	72.671962
580.360116	59.958490	72.676967
579.364078	54.547892	72.681972
578.838149	57.665465	72.686977
578.191991	64.116081	72.691982
577.913928	56.747833	72.696986
577.642741	53.260028	72.701991
576.580499	57.720737	72.706996
575.748650	58.887156	72.712001
574.787762	60.673283	72.717006
574.451053	57.331697	72.722010
573.333385	58.232897	72.727015
572.511606	58.625531	72.732020
571.933897	56.679108	72.737025
571.502827	64.887243	72.742030
571.272201	59.569302	72.747034
570.850597	59.383399	72.752039
569.760239	59.428521	72.757044
568.972856	56.575053	72.762049
568.241660	65.156304	72.767054
567.703955	58.371329	72.772058
567.166235	59.324336	72.777063
567.194238	58.361568	72.782068
565.923942	47.496442	72.787073
565.112103	56.016116	72.792078
565.091441	52.309739	72.797082
563.741209	65.541007	72.802087
563.173940	65.654390	72.807092
563.058688	51.832300	72.812097
561.970821	58.779759	72.817102
560.888195	51.691469	72.822106
560.175354	57.415788	72.827111
559.428571	58.179631	72.832116
559.255921	56.940998	72.837121
558.793023	60.081718	72.842126
558.158698	56.104721	72.847130
556.995948	57.668085	72.852135
556.600191	61.106757	72.857140
556.393685	57.991928	72.862145
554.922901	56.208399	72.867150
554.063726	58.446417	72.872154
553.435374	57.494276	72.877159
552.895554	57.034568	72.882164
552.732542	57.911136	72.887169
552.325548	58.469135	72.892174
551.776749	61.016715	72.897178
550.477434	63.763546	72.902183
549.548832	66.642241	72.907188
549.185786	57.654440	72.912193
548.946592	62.631328	72.917198
548.114877	53.509505	72.922202
546.741439	54.223233	72.927207
546.286184	57.239098	72.932212
546.268546	50.079246	72.937217
545.474228	61.426021	72.942222
544.841006	54.404012	72.947226
544.078028	56.991053	72.952231
543.098668	65.018020	72.957236
542.536832	52.018859	72.962241
542.095877	53.464864	72.967246
541.737586	54.805921	72.972250
540.699315	55.242366	72.977255
539.750937	56.996357	72.982260
539.620826	49.487904	72.987265
538.866739	56.790649	72.992270
538.065118	53.711482	72.997274
537.424529	44.557707	73.002279
536.543175	62.698213	73.007284
536.507333	49.548536	73.012289
535.627507	53.975626	73.017294
534.496372	49.146711	73.022298
534.086582	50.631189	73.027303
533.439831	52.926358	73.032308
533.069121	50.781851	73.037313
531.524618	54.005278	73.042318
530.880899	51.237326	73.047322
530.595211	59.391733	73.052327
529.958445	57.981195	73.057332
529.539695	45.909575	73.062337
529.042548	56.082466	73.067342
529.146213	45.526238	73.072346
527.883660	49.047912	73.077351
527.249991	56.934726	73.082356
527.048570	50.183319	73.087361
525.462196	57.333037	73.092366
525.034032	54.401447	73.097370
523.906238	53.770140	73.102375
522.581512	54.531183	73.107380
522.341447	49.959694	73.112385
522.030453	49.893781	73.117390
521.445888	45.576312	73.122394
521.236079	57.808134	73.127399
520.552621	59.250697	73.132404
519.755256	56.433684	73.137409
518.617607	56.169572	73.142414
518.170109	46.095791	73.147418
517.804673	44.522718	73.152423
517.092714	48.369629	73.157428
516.409902	47.492348	73.162433
515.544491	51.108990	73.167438
514.911356	47.011017	73.172442
514.340568	58.958530	73.177447
513.711373	58.372834	73.182452
512.966851	50.868223	73.187457
512.096119	58.558042	73.192462
511.706062	56.243178	73.197466
511.337087	55.716307	73.202471
510.032685	59.555403	73.207476
509.601587	51.328441	73.212481
508.487109	55.406950	73.217486
508.322056	49.639651	73.222490
507.878845	53.026853	73.227495
507.060761	53.261768	73.232500
506.371910	55.088524	73.237505
505.542175	53.390549	73.242510
505.061809	50.926959	73.247514
504.800769	45.729104	73.252519
503.887166	51.781495	73.257524
502.682202	48.625802	73.262529
501.981249	55.163173	73.267534
501.685622	48.892885	73.272538
501.253812	48.843334	73.277543
500.701453	55.418002	73.282548
500.053840	51.173309	73.287553
498.950056	60.982418	73.292558
498.460225	55.862446	73.297562
498.089839	55.428577	73.302567
496.703885	55.780933	73.307572
496.679483	48.921043	73.312577
495.758655	52.012347	73.317582
495.467229	49.672689	73.322586
494.677109	50.825656	73.327591
493.292585	60.615771	73.332596
492.917816	52.063388	73.337601
492.349461	54.808916	73.342606
492.076316	58.986404	73.347610
491.591798	49.539856	73.352615
490.221697	59.353945	73.357620
489.594383	46.575616	73.362625
489.012938	61.139935	73.367630
488.559780	61.684536	73.372634
488.262468	58.485410	73.377639
487.035531	63.410121	73.382644
486.512171	48.596989	73.387649
485.835178	52.011228	73.392654
485.457987	54.218371	73.397658
484.641114	51.971911	73.402663
483.412519	53.987865	73.407668
483.124261	50.572466	73.412673
482.284449	61.419042	73.417678
481.842943	50.117075	73.422682
481.839542	52.231351	73.427687
480.819636	56.530093	73.432692
479.879827	41.613474	73.437697
479.652506	50.743078	73.442702
478.591371	53.132944	73.447706
477.471028	54.350000	73.452711
476.734871	62.027027	73.457716
476.819641	48.420533	73.462721
476.333877	49.597922	73.467726
475.622952	55.181402	73.472730
474.738323	56.746465	73.477735
473.785119	56.875074	73.482740
473.537234	54.619530	73.487745
472.899965	65.846246	73.492750
471.737374	55.977504	73.497754
470.913982	52.465134	73.502759
469.937025	58.105255	73.507764
469.920107	46.014918	73.512769
469.413761	62.670192	73.517774
469.103124	51.286199	73.522778
468.778496	58.370496	73.527783
467.710496	58.255899	73.532788
467.512261	52.563759	73.537793
466.083303	59.988474	73.542798
465.029189	60.053067	73.547802
464.544224	55.572887	73.552807
464.096421	54.683367	73.557812
463.982690	53.595686	73.562817
462.106589	55.956669	73.567822
461.643424	58.440242	73.572826
461.294619	56.094236	73.577831
460.666766	60.508157	73.582836
460.335010	55.293212	73.587841
459.556553	57.962649	73.592846
458.769887	61.353057	73.597850
457.725088	57.005523	73.602855
456.909147	61.410626	73.607860
456.806473	61.239549	73.612865
456.364886	61.558761	73.617870
456.034959	58.403515	73.622874
455.268681	60.632339	73.627879
454.482148	59.354050	73.632884
453.715993	59.479029	73.637889
452.579499	59.075401	73.642894
451.612362	60.908803	73.647898
451.056229	54.328313	73.652903
450.711958	66.177807	73.657908
450.642642	60.106357	73.662913
450.390371	63.261908	73.667918
449.302363	61.357953	73.672922
448.087814	61.731474	73.677927
447.671874	60.152850	73.682932
447.115943	54.411094	73.687937
445.846380	51.622124	73.692942
445.243712	64.038892	73.697946
445.014915	48.657428	73.702951
444.358940	64.297878	73.707956
443.779743	56.894811	73.712961
442.358551	62.959203	73.717966
442.004707	59.636751	73.722970
441.558292	56.409895	73.727975
440.812513	57.858411	73.732980
440.939998	56.414018	73.737985
439.769527	63.784182	73.742990
438.660025	58.742386	73.747994
438.400174	62.490518	73.752999
437.482212	55.278525	73.758004
437.378267	51.110007	73.763009
436.264335	61.153744	73.768014
435.270884	61.730548	73.773018
434.882010	62.056913	73.778023
434.386031	62.991334	73.783028
434.272002	58.692314	73.788033
433.042255	62.663890	73.793038
432.275746	54.477052	73.798042
431.827501	50.528976	73.803047
431.488880	62.542883	73.808052
431.100268	55.259123	73.813057
429.857879	63.970219	73.818062
429.220769	58.978123	73.823066
428.297149	48.692681	73.828071
427.033356	54.384726	73.833076
426.916042	47.846273	73.838081
426.365841	61.455555	73.843086
426.047084	57.194778	73.848090
425.679109	47.880237	73.853095
424.593606	57.503073	73.858100
423.993056	49.482788	73.863105
423.388288	56.043153	73.868110
422.602366	56.945953	73.873114
421.668210	50.796153	73.878119
420.667064	55.935588	73.883124
420.181360	57.256648	73.888129
419.893277	53.893720	73.893134
419.255314	51.052963	73.898138
418.470843	51.389495	73.903143
417.239481	61.348365	73.908148
416.650125	60.162600	73.913153
416.277644	56.903342	73.918158
415.676509	67.631660	73.923162
415.284420	58.927132	73.928167
414.883505	60.707713	73.933172
414.539260	59.460602	73.938177
413.602909	62.641024	73.943182
412.722979	58.843108	73.948186
411.801488	55.737933	73.953191
410.515224	63.550289	73.958196
410.435379	49.377970	73.963201
409.891424	51.355159	73.968206
409.533018	54.560869	73.973210
409.237782	59.175145	73.978215
407.905664	57.193832	73.983220
407.109520	55.229214	73.988225
406.391559	61.783719	73.993230
406.281146	59.739080	73.998234
405.926368	57.299371	74.003239
404.445724	64.815850	74.008244
403.942656	56.719258	74.013249
403.196904	67.035412	74.018254
402.736724	57.046317	74.023258
401.797872	54.641184	74.028263
400.504092	53.889152	74.033268
400.672998	59.304884	74.038273
400.090499	57.927695	74.043278
399.696020	63.011716	74.048282
399.115455	58.227422	74.053287
398.080614	66.458508	74.058292
397.637725	60.466873	74.063297
396.838525	59.190371	74.068302
395.619432	65.394208	74.073306
394.945161	56.063086	74.078311
394.134486	58.226505	74.083316
393.887565	55.001780	74.088321
393.258515	57.901395	74.093326
393.206511	58.059116	74.098330
392.916800	46.155269	74.103335
391.355291	60.474281	74.108340
390.618298	58.725699	74.113345
390.109765	68.919889	74.118350
389.508678	59.003100	74.123354
388.656152	62.018379	74.128359
387.741622	63.324519	74.133364
387.654537	59.980038	74.138369
387.126221	58.269504	74.143374
386.663182	61.503412	74.148378
385.097440	56.479432	74.153383
384.308276	62.714978	74.158388
384.409930	71.294422	74.163393
384.017337	58.166035	74.168398
382.992931	66.610060	74.173402
382.061523	62.878600	74.178407
381.064283	65.649093	74.183412
381.262799	60.199603	74.188417
380.744930	58.418205	74.193422
379.315877	58.386031	74.198426
378.794519	59.012194	74.203431
378.149888	69.551006	74.208436
377.698374	63.704132	74.213441
376.594523	64.500778	74.218446
375.705386	56.797575	74.223450
375.403257	61.990103	74.228455
374.821013	62.601045	74.233460
374.188345	64.505027	74.238465
373.881075	67.700004	74.243470
373.352999	63.282090	74.248474
372.343840	49.681522	74.253479
371.778305	60.781475	74.258484
371.262513	53.327692	74.263489
370.084044	58.432793	74.268494
369.507303	52.177149	74.273498
369.202104	58.826300	74.278503
368.261673	58.605788	74.283508
367.721394	51.198043	74.288513
366.731700	62.560154	74.293518
365.969454	62.316998	74.298522
365.672069	58.582271	74.303527
365.420655	61.583738	74.308532
365.007658	52.474278	74.313537
363.835298	59.780043	74.318542
362.996823	58.545803	74.323546
362.532309	48.704693	74.328551
361.485134	61.505911	74.333556
360.848565	58.480592	74.338561
359.740368	67.467107	74.343566
359.041697	69.639361	74.348570
359.396827	65.169153	74.353575
358.906596	72.001986	74.358580
358.479060	64.242960	74.363585
357.155976	61.836981	74.368590
356.320989	62.908059	74.373594
355.970742	61.138986	74.378599
354.586678	69.153238	74.383604
353.693227	57.244317	74.388609
353.374440	59.971559	74.393614
353.495478	62.904061	74.398618
352.531105	59.610865	74.403623
351.859634	69.559050	74.408628
351.536886	64.812677	74.413633
350.458447	65.387486	74.418638
350.379951	69.437282	74.423642
349.626034	62.620327	74.428647
347.910158	74.878967	74.433652
347.280307	63.676005	74.438657
346.733649	68.759666	74.443662
346.097333	71.368840	74.448666
345.880516	58.902269	74.453671
345.400707	65.565561	74.458676
345.132460	67.959292	74.463681
344.009887	69.192550	74.468686
343.008954	66.653998	74.473690
342.846694	73.745603	74.478695
341.906179	73.546030	74.483700
340.962883	62.483630	74.488705
340.397073	61.314365	74.493710
339.593772	66.488193	74.498714
339.228149	63.355653	74.503719
338.765810	67.003499	74.508724
338.572868	61.218888	74.513729
337.012283	70.375700	74.518734
336.512153	65.182521	74.523738
335.987057	63.321056	74.528743
335.287501	67.299279	74.533748
334.893452	58.793643	74.538753
334.275010	59.899054	74.543758
333.277738	66.499070	74.548762
332.997077	62.861341	74.553767
331.454006	74.436721	74.558772
330.783320	57.965026	74.563777
330.496341	63.264689	74.568782
330.168412	68.192842	74.573786
329.996709	63.616756	74.578791
328.941993	72.892910	74.583796
328.165167	59.531987	74.588801
327.724136	65.917070	74.593806
326.354943	71.312225	74.598810
325.632851	62.321660	74.603815
324.886481	61.722128	74.608820
324.311018	64.507179	74.613825
323.913297	65.293331	74.618830
323.423701	65.697358	74.623834
323.227701	62.646663	74.628839
322.766817	66.399649	74.633844
321.839202	62.220738	74.638849
321.239362	66.017276	74.643854
319.687680	62.719754	74.648858
319.257919	53.666067	74.653863
318.800680	63.945404	74.658868
318.535464	61.969141	74.663873
317.598270	66.402939	74.668878
316.714040	63.594932	74.673882
316.147249	63.548403	74.678887
315.298370	59.172853	74.683892
315.438800	53.699376	74.688897
314.327709	64.937441	74.693902
313.174973	60.349118	74.698906
312.769343	54.386637	74.703911
311.731222	61.618091	74.708916
311.657618	56.837312	74.713921
310.621189	67.451171	74.718926
309.615619	65.651535	74.723930
309.304840	57.008087	74.728935
308.534883	70.592674	74.733940
308.251260	65.567642	74.738945
308.215448	53.904087	74.743950
307.201546	59.616088	74.748954
306.367770	60.977475	74.753959
305.759251	64.206325	74.758964
305.434324	68.187047	74.763969
304.249135	63.447587	74.768974
302.893699	61.269394	74.773978
302.543363	58.675391	74.778983
302.060290	67.255181	74.783988
301.359903	57.776592	74.788993
301.489131	61.559479	74.793998
300.347083	60.639766	74.799002
299.630152	56.346598	74.804007
298.830265	66.575725	74.809012
298.535844	62.533409	74.814017
298.100600	66.359760	74.819022
297.088138	54.737294	74.824026
296.417839	58.738134	74.829031
295.918944	62.118711	74.834036
294.874581	59.066594	74.839041
293.688929	62.356867	74.844046
292.765919	60.579399	74.849050
292.483023	51.282665	74.854055
292.082874	59.065917	74.859060
291.920212	49.831859	74.864065
291.388439	59.252837	74.869070
290.663018	59.377570	74.874074
289.859203	46.103397	74.879079
289.124076	60.943507	74.884084
288.776897	58.581846	74.889089
287.975755	66.616584	74.894094
286.617307	61.654210	74.899098
285.984733	50.103210	74.904103
285.581044	70.490654	74.909108
285.402235	68.246176	74.914113
284.906178	72.506480	74.919118
283.519601	73.467653	74.924122
283.418647	58.332313	74.929127
282.329018	59.495599	74.934132
282.114461	63.138080	74.939137
281.270466	56.585254	74.944142
279.795739	58.334779	74.949146
279.900559	62.983112	74.954151
279.470374	59.694682	74.959156
278.764358	59.044822	74.964161
277.397007	58.699753	74.969166
276.695283	55.409713	74.974170
276.249338	50.026877	74.979175
275.666546	60.950194	74.984180
275.508766	58.779872	74.989185
275.175099	61.971087	74.994190
274.374205	60.260318	74.999194
273.741091	53.764896	75.004199
272.332367	61.309732	75.009204
271.487411	62.701461	75.014209
270.702008	61.283678	75.019214
270.237915	62.409612	75.024218
270.056115	52.371253	75.029223
269.451855	65.538643	75.034228
268.703684	64.663129	75.039233
267.850905	62.696007	75.044238
266.990778	68.821369	75.049242
266.605824	61.688576	75.054247
265.999327	73.292108	75.059252
265.435549	57.703240	75.064257
264.311178	61.633108	75.069262
264.006866	68.818131	75.074266
263.599459	54.974725	75.079271
262.939513	64.814757	75.084276
261.874569	64.215370	75.089281
261.300347	62.547456	75.094286
260.886935	60.861452	75.099290
260.506863	56.936842	75.104295
258.705066	65.653860	75.109300
258.163605	59.753350	75.114305
258.034095	56.795468	75.119310
256.828786	64.745942	75.124314
257.102149	56.988764	75.129319
256.268538	57.981864	75.134324
255.434797	58.858547	75.139329
254.432550	60.205007	75.144334
253.615797	63.741117	75.149338
253.489283	58.976120	75.154343
252.846596	64.214000	75.159348
252.432470	55.941544	75.164353
251.327153	65.450179	75.169358
250.444327	69.043008	75.174362
250.133141	58.131617	75.179367
249.926116	62.288302	75.184372
249.030512	53.659458	75.189377
247.855218	57.925273	75.194382
247.329739	59.934835	75.199386
247.338632	55.455295	75.204391
246.098284	62.400522	75.209396
245.258121	56.561873	75.214401
244.584636	55.105175	75.219406
244.001005	60.723697	75.224410
244.038459	54.667121	75.229415
242.649859	64.317466	75.234420
241.881389	65.666486	75.239425
241.229798	54.310190	75.244430
240.949970	57.494545	75.249434
240.694173	62.115483	75.254439
239.353126	68.232894	75.259444
238.810288	52.482564	75.264449
238.439113	49.104295	75.269454
237.723302	56.010132	75.274458
236.886417	55.369686	75.279463
235.847329	61.380866	75.284468
235.189500	60.472110	75.289473
234.758007	67.994308	75.294478
234.445534	62.923707	75.299482
234.000252	59.267631	75.304487
232.825043	64.841515	75.309492
232.337440	62.933377	75.314497
231.628714	58.500271	75.319502
231.088468	64.999068	75.324506
230.219956	58.925690	75.329511
229.585494	61.292994	75.334516
228.864140	62.219886	75.339521
228.287915	61.185439	75.344526
227.677522	63.656769	75.349530
226.923412	57.941523	75.354535
225.923429	67.170412	75.359540
224.878344	64.566829	75.364545
224.191702	59.431693	75.369550
224.000114	62.213710	75.374554
224.185452	56.099813	75.379559
223.459436	62.840834	75.384564
222.886337	64.635549	75.389569
221.927927	57.732504	75.394574
221.142343	71.520285	75.399578
220.854657	57.955953	75.404583
219.797778	65.731789	75.409588
219.061705	64.807634	75.414593
218.896442	61.225920	75.419598
217.602115	66.241578	75.424602
217.080054	60.644441	75.429607
216.240329	63.655973	75.434612
215.892908	55.306963	75.439617
215.429875	53.604208	75.444622
213.834741	61.130883	75.449626
213.312283	60.964274	75.454631
212.786010	68.503508	75.459636
212.567512	58.042393	75.464641
212.400348	54.784277	75.469646
210.968587	60.141630	75.474650
210.334263	56.472571	75.479655
209.231994	56.955977	75.484660
209.271359	55.047110	75.489665
208.927733	50.269602	75.494670
207.945345	54.801550	75.499674
207.421639	55.430107	75.504679
206.144625	54.224889	75.509684
205.841082	56.547705	75.514689
205.638378	56.801124	75.519694
204.409374	49.733301	75.524698
203.886626	52.934824	75.529703
202.997013	56.593160	75.534708
202.704400	61.123309	75.539713
201.817272	55.093787	75.544718
200.774088	53.356281	75.549722
200.355766	62.213505	75.554727
199.616956	60.110816	75.559732
199.473925	62.474008	75.564737
199.058183	60.692495	75.569742
197.897380	67.722775	75.574746
197.279476	59.929706	75.579751
196.712118	57.323577	75.584756
196.048334	50.271359	75.589761
195.197071	59.535934	75.594766
194.411619	59.034302	75.599770
193.891350	50.830183	75.604775
193.311477	61.752211	75.609780
192.887803	60.308353	75.614785
191.765177	57.011537	75.619790
190.686099	62.135160	75.624794
190.806224	57.459329	75.629799
190.007405	59.445889	75.634804
189.476994	58.772651	75.639809
189.251870	66.090535	75.644814
188.162832	61.479489	75.649818
187.658836	51.893850	75.654823
186.463615	60.685710	75.659828
185.386411	60.133441	75.664833
185.000058	52.511856	75.669838
184.289354	61.148427	75.674842
184.019271	53.392050	75.679847
183.582482	59.669440	75.684852
183.198674	54.610287	75.689857
182.238101	54.203410	75.694862
181.270344	62.284479	75.699866
180.758563	60.998612	75.704871
180.193164	57.911390	75.709876
179.998340	55.730452	75.714881
178.780084	55.577340	75.719886
177.680908	58.090229	75.724890
177.547711	49.266374	75.729895
176.848662	57.284011	75.734900
175.954521	51.500026	75.739905
175.367801	54.771725	75.744910
174.725982	51.595375	75.749914
174.378292	52.599132	75.754919
173.383677	57.676700	75.759924
172.647979	52.635244	75.764929
172.015949	57.887089	75.769934
171.355724	64.182259	75.774938
170.936849	47.051709	75.779943
170.556607	54.746683	75.784948
169.581947	60.080158	75.789953
169.028869	55.532364	75.794958
168.338175	60.720456	75.799962
167.819972	49.344869	75.804967
166.390356	61.625516	75.809972
165.914916	55.677392	75.814977
165.282363	62.720535	75.819982
164.963768	59.263395	75.824986
164.486831	55.910763	75.829991
163.460064	61.378691	75.834996
162.729191	59.190969	75.840001
162.681138	54.747641	75.845006
161.670776	54.611787	75.850010
161.444694	49.169965	75.855015
160.392636	50.506431	75.860020
159.973869	58.579830	75.865025
159.051387	56.437192	75.870030
158.021139	56.808401	75.875034
157.098582	50.948771	75.880039
156.748526	65.047520	75.885044
156.272934	56.164736	75.890049
156.051027	63.160770	75.895054
155.144499	60.920272	75.900058
154.074558	57.191698	75.905063
153.549285	57.556467	75.910068
152.715461	63.150784	75.915073
152.377995	60.590510	75.920078
152.016912	62.239156	75.925082
151.103171	53.647789	75.930087
150.404466	58.258212	75.935092
149.921995	55.337162	75.940097
149.203681	55.204531	75.945102
148.005538	60.168584	75.950106
147.608789	50.152490	75.955111
147.269934	57.245539	75.960116
146.477889	52.157699	75.965121
146.008052	61.525432	75.970126
144.616687	55.549211	75.975130
144.336054	53.135501	75.980135
143.439432	53.929830	75.985140
142.997756	54.782343	75.990145
142.814406	57.077057	75.995150
141.795548	60.212066	76.000154
140.478991	57.143893	76.005159
140.011841	60.060777	76.010164
139.627612	54.183859	76.015169
139.493608	58.010281	76.020174
138.719892	64.632785	76.025178
138.030241	62.171175	76.030183
136.871874	60.836696	76.035188
136.385670	55.454467	76.040193
135.954062	51.657123	76.045198
135.336127	58.673681	76.050202
134.286345	53.114534	76.055207
133.370274	64.865468	76.060212
133.063050	59.975154	76.065217
132.877353	53.341483	76.070222
131.930723	56.272282	76.075226
131.199402	51.118381	76.080231
130.295017	52.720045	76.085236
130.421647	52.870432	76.090241
129.854935	55.067457	76.095246
128.512413	56.858701	76.100250
128.149727	53.638847	76.105255
127.286315	58.412501	76.110260
126.607935	57.854237	76.115265
126.006091	59.290360	76.120270
124.788500	61.430428	76.125274
124.532312	55.200397	76.130279
123.723050	51.675416	76.135284
123.364012	54.642052	76.140289
122.340238	56.264185	76.145294
121.220081	51.362462	76.150298
120.914333	60.934944	76.155303
120.496785	60.253023	76.160308
120.186289	59.073963	76.165313
120.325659	61.064289	76.170318
119.216214	60.626108	76.175322
118.375328	50.567353	76.180327
117.330456	60.000512	76.185332
116.216363	53.812171	76.190337
115.828637	52.513729	76.195342
114.902743	57.820300	76.200346
114.878184	54.179345	76.205351
114.168679	58.708339	76.210356
113.638504	63.156463	76.215361
112.520394	52.354231	76.220366
111.722250	63.318811	76.225370
111.321065	53.582544	76.230375
111.199434	50.551484	76.235380
110.636168	58.039431	76.240385
109.824531	53.244282	76.245390
108.939794	63.382971	76.250394
108.358660	60.295695	76.255399
106.829842	60.008751	76.260404
106.354502	63.453983	76.265409
106.159067	59.120393	76.270414
105.310016	58.324172	76.275418
105.226535	47.974925	76.280423
104.002860	62.757486	76.285428
103.115132	62.090652	76.290433
102.935365	53.573191	76.295438
102.081795	61.250243	76.300442
101.814237	54.033016	76.305447
100.634363	55.846906	76.310452
99.651986	55.039204	76.315457
99.676883	55.626610	76.320462
98.927368	61.901963	76.325466
98.433584	55.669251	76.330471
97.330452	53.408792	76.335476
96.278020	51.094644	76.340481
95.997604	55.841373	76.345486
95.587792	61.315638	76.350490
95.140881	51.695761	76.355495
94.347048	56.569983	76.360500
93.473712	60.289883	76.365505
93.046502	56.721906	76.370510
92.055335	56.959727	76.375514
92.141125	59.500387	76.380519
90.741766	57.320713	76.385524
89.798627	57.553458	76.390529
89.619087	50.154575	76.395534
89.078444	53.593635	76.400538
88.472946	53.393122	76.405543
87.558682	62.609302	76.410548
86.733028	59.189368	76.415553
86.422440	56.478449	76.420558
85.560553	64.221268	76.425562
85.211585	53.332573	76.430567
84.142008	50.669679	76.435572
83.390412	57.475881	76.440577
83.250103	53.134818	76.445582
82.243419	62.708268	76.450586
82.025068	56.286241	76.455591
80.836054	65.263755	76.460596
80.179063	62.854973	76.465601
79.929088	49.396311	76.470606
79.178576	67.086121	76.475610
78.491890	56.806738	76.480615
77.350949	58.512517	76.485620
76.558226	60.546204	76.490625
76.531662	52.742171	76.495630
75.872221	57.756765	76.500634
75.126568	53.690397	76.505639
74.367844	63.184629	76.510644
73.299165	57.019302	76.515649
73.512055	57.146609	76.520654
72.754948	64.521356	76.525658
71.929313	52.688135	76.530663
71.238686	50.827852	76.535668
70.469136	56.402869	76.540673
70.165105	57.259813	76.545678
68.848191	61.647047	76.550682
68.410105	62.795379	76.555687
68.081687	65.040367	76.560692
67.352020	57.630019	76.565697
66.069196	54.135324	76.570702
64.956554	62.592541	76.575706
64.487199	56.502084	76.580711
64.069234	64.347995	76.585716
63.751228	60.602624	76.590721
63.674639	53.942361	76.595726
62.819222	61.666310	76.600730
62.413611	47.755550	76.605735
61.267863	56.745381	76.610740
60.494534	59.623192	76.615745
60.101196	54.200977	76.620750
58.352038	62.078947	76.625754
57.965494	54.059151	76.630759
57.146029	58.937378	76.635764
57.290821	59.364106	76.640769
57.090717	54.019675	76.645774
56.360334	59.460882	76.650778
55.689431	49.116045	76.655783
54.675377	58.724705	76.660788
53.959470	62.912195	76.665793
53.565812	51.109516	76.670798
52.557015	58.696746	76.675802
51.577185	55.725991	76.680807
51.048198	47.450772	76.685812
50.415625	55.954749	76.690817
50.288131	57.229425	76.695822
49.202282	59.525334	76.700826
48.736371	55.010375	76.705831
47.913169	62.251595	76.710836
47.439547	54.208049	76.715841
47.124946	54.160549	76.720846
46.079791	64.991838	76.725850
45.285754	58.660228	76.730855
44.552393	58.276393	76.735860
44.324861	64.397129	76.740865
43.537212	53.683911	76.745870
42.324059	60.550308	76.750874
41.978911	54.258571	76.755879
41.369565	54.854069	76.760884
40.962631	60.807417	76.765889
40.232531	57.270854	76.770894
39.166145	60.609019	76.775898
38.822851	57.285199	76.780903
37.835712	57.176967	76.785908
37.400518	62.711635	76.790913
36.454457	58.522144	76.795918
35.517094	60.864039	76.800922
35.014922	51.919133	76.805927
34.835159	63.688688	76.810932
34.366852	62.222502	76.815937
33.900796	58.467784	76.820942
32.882971	68.535360	76.825946
31.854929	62.698581	76.830951
31.580028	61.487374	76.835956
30.867430	59.686124	76.840961
30.669141	59.167132	76.845966
29.276879	63.487957	76.850970
28.944216	59.944038	76.855975
28.318255	63.997695	76.860980
27.377433	68.283353	76.865985
26.670673	61.347083	76.870990
25.652923	65.759608	76.875994
25.403243	55.180326	76.880999
24.881892	58.362679	76.886004
25.166498	68.904795	76.891009
24.029429	63.514580	76.896014
22.759010	55.967632	76.901018
22.263329	60.950601	76.906023
21.142206	55.133340	76.911028
20.206438	57.105909	76.916033
19.483360	51.713792	76.921038
19.450359	51.918386	76.926042
19.538706	50.048490	76.931047
18.850035	61.079167	76.936052
17.860443	67.743039	76.941057
16.905672	60.577338	76.946062
16.361325	61.642453	76.951066
15.994565	60.949071	76.956071
14.836016	65.773741	76.961076
14.099206	66.007437	76.966081
13.635405	58.599277	76.971086
13.133226	64.338051	76.976090
12.631549	54.742973	76.981095
11.565156	55.465784	76.986100
10.822648	63.872966	76.991105
10.409197	53.062443	76.996110
9.730376	63.798162	77.001114
9.166356	59.149250	77.006119
8.118396	61.765492	77.011124
7.066239	64.663884	77.016129
7.018055	61.130003	77.021134
6.383287	61.992347	77.026139
6.449141	65.364923	77.031143
5.010837	64.151104	77.036148
4.093493	67.007830	77.041153
3.929664	62.849607	77.046158