Tue Jun 08 17:39:35 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.087109	98.392579	0.000000
-0.171802	90.116149	0.005005
-0.864481	44.816120	0.010010
-2.602668	0.016783	0.015014
-6.844803	-10.446295	0.020019
-12.103740	-16.098748	0.025024
-17.409969	-10.065178	0.030029
-21.881325	-11.357303	0.035034
-26.073145	-8.461716	0.040038
-29.726651	-10.626256	0.045043
-32.922301	-9.368218	0.050048
-36.798455	-7.822977	0.055053
-40.595465	-12.697456	0.060058
-43.948152	-15.133419	0.065062
-47.995190	-11.755830	0.070067
-51.595207	-14.206216	0.075072
-55.542414	-11.957638	0.080077
-59.179532	-18.793202	0.085082
-63.140625	-17.494278	0.090086
-66.894802	-14.182681	0.095091
-70.560926	-15.925840	0.100096
-74.308892	-13.454850	0.105101
-78.035921	-16.967702	0.110106
-81.914225	-8.543045	0.115110
-85.331899	-15.503843	0.120115
-89.465364	-17.524059	0.125120
-93.593975	-11.381708	0.130125
-96.974571	-13.181703	0.135130
-100.612220	-8.917495	0.140134
-104.279657	-4.380955	0.145139
-107.885468	-11.629190	0.150144
-111.940689	-2.215416	0.155149
-116.084565	-14.219204	0.160154
-119.635829	-3.710875	0.165158
-123.263392	-13.201266	0.170163
-126.652565	-11.682229	0.175168
-130.630970	-9.320876	0.180173
-134.127571	-24.367545	0.185178
-138.401387	-19.509510	0.190182
-141.957521	-19.805125	0.195187
-145.663039	-22.798221	0.200192
-150.140688	-9.337645	0.205197
-153.612283	-11.102650	0.210202
-157.469392	-2.764456	0.215206
-161.296314	-14.592042	0.220211
-164.641101	-15.022561	0.225216
-168.755982	-11.903611	0.230221
-171.959590	-12.747127	0.235226
-176.046191	-8.532173	0.240230
-179.817659	-15.595627	0.245235
-183.318914	-18.704245	0.250240
-187.501260	-9.313215	0.255245
-191.199013	-9.778306	0.260250
-194.831820	-5.822730	0.265254
-198.622315	-4.545843	0.270259
-201.973424	-10.929844	0.275264
-206.131907	-5.810097	0.280269
-209.739147	-10.199508	0.285274
-213.107211	-2.239994	0.290278
-217.398728	-7.402506	0.295283
-221.145412	-13.044877	0.300288
-225.659405	-3.587854	0.305293
-228.538742	-7.108608	0.310298
-232.298855	-3.709024	0.315302
-236.035253	-3.809053	0.320307
-239.771739	-7.328436	0.325312
-243.644881	-7.900761	0.330317
-247.254213	-6.317823	0.335322
-251.514484	-6.666649	0.340326
-255.059995	-8.617041	0.345331
-258.674213	-14.616416	0.350336
-262.588545	-1.700353	0.355341
-266.288266	-9.833069	0.360346
-270.419043	-1.306148	0.365350
-273.830471	-6.580875	0.370355
-277.027308	-11.338232	0.375360
-281.397313	-6.106355	0.380365
-284.858267	-4.281225	0.385370
-288.620060	-3.809657	0.390374
-292.713102	-5.591899	0.395379
-296.169865	-13.444571	0.400384
-300.224009	-7.377970	0.405389
-303.593818	-4.781409	0.410394
-307.652408	-3.862234	0.415398
-311.470358	-4.027943	0.420403
-315.186557	-4.444771	0.425408
-318.784735	-5.155373	0.430413
-322.513988	-10.169504	0.435418
-326.500767	-1.796701	0.440422
-330.639767	-10.408969	0.445427
-333.840589	-17.418992	0.450432
-337.735046	3.642492	0.455437
-341.383012	-13.616030	0.460442
-345.073801	-11.261991	0.465446
-348.868703	-10.552210	0.470451
-352.813105	-13.987277	0.475456
-356.801183	-7.365159	0.480461
-360.201519	1.311651	0.485466
-364.013586	0.414765	0.490470
-367.840267	-1.862673	0.495475
-371.651514	-16.526357	0.500480
-375.759774	-5.482206	0.505485
-379.229840	-10.750338	0.510490
-382.842468	-4.770064	0.515494
-386.473568	-11.272451	0.520499
-390.433452	-11.016667	0.525504
-394.262013	-5.705870	0.530509
-397.702340	-13.914933	0.535514
-401.953439	-8.225746	0.540518
-405.860636	-13.433470	0.545523
-409.057599	-8.480075	0.550528
-412.993509	-7.321737	0.555533
-416.643886	-7.600177	0.560538
-420.308862	-11.202320	0.565542
-424.078848	-6.390199	0.570547
-427.791990	-6.743119	0.575552
-431.939460	-6.119614	0.580557
-435.665395	-10.788842	0.585562
-439.232075	-7.427013	0.590566
-443.084719	-9.003662	0.595571
-446.642220	-18.354206	0.600576
-450.367943	-16.463792	0.605581
-454.515685	-13.631036	0.610586
-457.763932	-8.166740	0.615590
-461.942150	-4.244482	0.620595
-465.526694	-7.476730	0.625600
-469.983416	-4.215186	0.630605
-473.059672	-14.213496	0.635610
-477.164356	-9.975444	0.640614
-480.903771	-3.249448	0.645619
-484.495539	-6.105073	0.650624
-488.205466	-6.760840	0.655629
-491.652395	-8.773738	0.660634
-495.563728	-2.655294	0.665638
-499.482035	-10.424658	0.670643
-503.199775	-8.324795	0.675648
-507.202611	-2.400232	0.680653
-510.653097	-8.654439	0.685658
-514.525459	-11.417292	0.690662
-518.470478	-5.507377	0.695667
-521.730316	-13.191156	0.700672
-525.775636	-13.122289	0.705677
-529.700895	-23.981383	0.710682
-533.817248	-9.233752	0.715686
-537.512162	-10.876062	0.720691
-540.696053	-11.100632	0.725696
-544.599860	-9.234054	0.730701
-548.382237	-12.096784	0.735706
-552.018465	-21.395830	0.740710
-556.061850	-19.325308	0.745715
-559.322746	-12.168240	0.750720
-563.490451	-11.424702	0.755725
-567.039488	-17.931531	0.760730
-570.847502	-10.875958	0.765734
-574.882808	-0.566873	0.770739
-578.323191	-10.447361	0.775744
-582.695194	-6.215842	0.780749
-586.411148	-11.381217	0.785754
-589.795801	-10.856880	0.790758
-593.425912	0.342622	0.795763
-596.947505	-8.165724	0.800768
-600.921599	-10.816707	0.805773
-604.669583	-13.758309	0.810778
-608.801815	-3.138114	0.815782
-612.828939	-3.209648	0.820787
-616.037873	-14.072774	0.825792
-620.182116	-8.128194	0.830797
-623.446321	-7.480827	0.835802
-627.413892	-3.744160	0.840806
-631.120638	-3.807896	0.845811
-634.824146	-9.928978	0.850816
-638.946380	1.982988	0.855821
-642.518575	-15.203366	0.860826
-646.167593	-7.455069	0.865830
-649.835696	-4.812986	0.870835
-653.431981	-13.862631	0.875840
-657.602605	-4.517819	0.880845
-661.372888	0.487558	0.885850
-665.033629	-9.115451	0.890854
-669.326973	-9.293209	0.895859
-672.372409	-14.509629	0.900864
-676.296702	-12.698628	0.905869
-680.137424	-12.629995	0.910874
-683.868254	-7.931745	0.915878
-687.411358	-13.185898	0.920883
-691.262900	-9.414619	0.925888
-695.184934	-6.527621	0.930893
-698.770270	-12.186196	0.935898
-702.506545	-11.368551	0.940902
-706.454146	-13.043528	0.945907
-710.116433	-14.660105	0.950912
-713.841919	-9.711320	0.955917
-717.592385	-13.036051	0.960922
-721.426276	-12.310577	0.965926
-725.248285	-1.068970	0.970931
-728.795923	-6.414277	0.975936
-732.330544	-11.276323	0.980941
-736.450544	-9.002239	0.985946
-740.840273	-16.312324	0.990950
-744.300810	-11.212423	0.995955
-747.592155	-14.567376	1.000960
-751.605818	-10.839664	1.005965
-755.349236	-13.034735	1.010970
-758.726358	-7.268663	1.015974
-763.011970	-2.439607	1.020979
-766.099666	-4.809969	1.025984
-770.518799	-4.967617	1.030989
-774.200948	-14.535662	1.035994
-777.856583	-7.079003	1.040998
-781.985528	-9.316425	1.046003
-785.188440	-18.637525	1.051008
-789.453085	-7.243723	1.056013
-792.782887	-10.279037	1.061018
-796.516251	-0.480641	1.066022
-800.235286	-14.498972	1.071027
-804.120899	-9.676566	1.076032
-808.471677	-9.862090	1.081037
-811.916077	-21.348130	1.086042
-815.468149	-18.451903	1.091046
-819.370543	-9.341665	1.096051
-822.894294	-24.572867	1.101056
-826.443076	-13.237969	1.106061
-830.400909	-14.406638	1.111066
-834.400123	-17.119004	1.116070
-838.201374	-8.230175	1.121075
-841.503329	-16.281033	1.126080
-845.933772	-4.554797	1.131085
-849.380992	-6.128047	1.136090
-853.441332	-7.318965	1.141094
-857.045671	-10.253422	1.146099
-860.497939	-11.794613	1.151104
-864.395346	-2.586515	1.156109
-867.895723	-10.671183	1.161114
-871.695722	-8.575052	1.166118
-875.620177	-10.883402	1.171123
-879.126999	-8.207638	1.176128
-882.931047	-9.782366	1.181133
-886.872673	-10.843641	1.186138
-890.706326	-9.351934	1.191142
-894.665903	-7.787294	1.196147
-898.433466	-11.531264	1.201152
-902.120587	-5.122970	1.206157
-905.325042	-9.227658	1.211162
-909.156449	-6.032765	1.216166
-913.302375	-3.402382	1.221171
-917.143439	-12.375028	1.226176
-920.777625	1.746633	1.231181
-924.533946	-8.571903	1.236186
-928.051142	-4.539291	1.241190
-932.430832	-1.867575	1.246195
-936.190231	-10.307949	1.251200
-940.043531	-7.260838	1.256205
-943.449177	-10.568383	1.261210
-947.228426	-12.123232	1.266214
-950.607644	1.128951	1.271219
-953.895763	-11.428583	1.276224
-958.358359	-3.453541	1.281229
-962.564000	-6.256259	1.286234
-966.117852	-5.970589	1.291238
-970.124626	-3.094063	1.296243
-973.353093	-11.495296	1.301248
-977.076746	-1.984594	1.306253
-980.742767	-10.245575	1.311258
-984.674526	-10.625217	1.316262
-988.544219	-15.420434	1.321267
-992.088403	-4.735100	1.326272
-995.813441	-16.370145	1.331277
-999.966711	-9.192194	1.336282
-1003.627339	-12.116069	1.341286
-1007.433991	-14.003633	1.346291
-1010.732667	-19.672460	1.351296
-1015.272411	-12.196451	1.356301
-1018.546840	-17.433286	1.361306
-1022.563234	-15.882458	1.366310
-1026.266691	-7.912964	1.371315
-1029.935374	-9.208454	1.376320
-1033.790172	-4.717958	1.381325
-1037.063254	-7.300218	1.386330
-1040.784593	-8.351808	1.391334
-1044.688601	-13.912335	1.396339
-1048.741978	-14.568644	1.401344
-1052.829534	-6.897494	1.406349
-1056.380754	-7.336092	1.411354
-1059.966440	-8.910260	1.416358
-1063.658686	-2.013101	1.421363
-1067.548092	-13.915489	1.426368
-1071.343999	-7.883484	1.431373
-1074.909513	1.210172	1.436378
-1078.883543	-1.738373	1.441382
-1082.642384	-4.050888	1.446387
-1085.973822	-15.717508	1.451392
-1089.648265	-12.633089	1.456397
-1093.811736	-13.468989	1.461402
-1097.707398	-11.627004	1.466406
-1101.464447	-5.818340	1.471411
-1105.066683	-10.740286	1.476416
-1108.942085	-14.688552	1.481421
-1112.599770	-11.398192	1.486426
-1116.187693	-12.497885	1.491430
-1120.245741	-9.134825	1.496435
-1123.952993	-11.178681	1.501440
-1127.923904	0.446407	1.506445
-1131.414980	-3.392981	1.511450
-1135.133070	-13.131730	1.516454
-1139.125324	-14.891388	1.521459
-1142.360151	-23.261775	1.526464
-1146.290448	-13.645207	1.531469
-1150.100178	-13.182034	1.536474
-1153.927100	-8.806347	1.541478
-1158.261581	-7.963341	1.546483
-1161.561971	-28.395309	1.551488
-1165.259338	-9.645772	1.556493
-1169.281216	-5.806546	1.561498
-1172.550681	-3.733765	1.566502
-1176.598922	-12.162587	1.571507
-1180.369965	-16.132258	1.576512
-1184.091187	-8.941895	1.581517
-1188.140378	-10.410304	1.586522
-1191.720281	-9.070845	1.591526
-1195.783087	-6.796679	1.596531
-1198.901504	-22.880608	1.601536
-1202.569630	-1.684545	1.606541
-1206.392198	-9.680420	1.611546
-1210.136361	-7.224928	1.616550
-1214.186352	-2.686546	1.621555
-1217.979628	-12.995676	1.626560
-1221.763013	-3.496236	1.631565
-1225.446351	-10.309388	1.636570
-1228.793292	-16.338004	1.641574
-1232.809934	-8.209965	1.646579
-1236.423919	-4.623478	1.651584
-1240.632449	-3.711238	1.656589
-1244.720551	-6.735942	1.661594
-1248.426859	-12.615200	1.666598
-1251.995542	-12.604222	1.671603
-1255.798115	-14.487127	1.676608
-1259.392093	-6.744655	1.681613
-1262.889381	-0.096724	1.686618
-1266.524183	-3.698563	1.691622
-1270.677899	-1.692111	1.696627
-1274.129338	-12.014109	1.701632
-1278.385102	-3.545377	1.706637
-1281.933767	-5.852363	1.711642
-1285.494912	-15.834215	1.716646
-1289.272325	-6.976356	1.721651
-1293.154598	-11.700834	1.726656
-1297.171634	-12.973753	1.731661
-1300.657781	-9.584421	1.736666
-1304.341772	-14.929869	1.741670
-1308.111340	-9.352156	1.746675
-1312.168480	-18.585685	1.751680
-1315.929234	-12.423344	1.756685
-1319.609988	-7.848032	1.761690
-1323.111135	-10.876375	1.766694
-1327.244259	-7.059342	1.771699
-1331.155369	-7.074342	1.776704
-1334.601274	-3.498488	1.781709
-1338.230227	-12.899480	1.786714
-1341.643602	-9.449594	1.791718
-1345.541517	-6.690098	1.796723
-1349.553634	-9.008991	1.801728
-1353.575168	-7.711555	1.806733
-1357.230435	-12.184855	1.811738
-1360.801640	-13.318784	1.816742
-1364.818811	-15.986895	1.821747
-1368.344899	-20.733798	1.826752
-1372.023149	-14.024707	1.831757
-1375.680537	-1.312182	1.836762
-1379.605250	-5.320002	1.841766
-1383.485092	-3.785188	1.846771
-1386.644455	-15.267948	1.851776
-1390.639136	-11.334122	1.856781
-1394.570192	-3.592453	1.861786
-1398.635242	-20.755329	1.866790
-1402.708835	-3.218260	1.871795
-1405.946807	-11.279227	1.876800
-1410.225880	-9.599236	1.881805
-1413.848521	-11.707097	1.886810
-1417.258269	-2.768224	1.891814
-1421.219783	-3.799924	1.896819
-1424.773184	-15.165622	1.901824
-1428.568213	-7.748453	1.906829
-1432.284326	3.453804	1.911834
-1435.487456	-14.582570	1.916838
-1439.874964	-7.794603	1.921843
-1443.487839	-12.897159	1.926848
-1447.779687	-9.729267	1.931853
-1450.866246	-9.903962	1.936858
-1454.722909	-17.089319	1.941862
-1459.072303	-11.059003	1.946867
-1462.172496	-3.585529	1.951872
-1466.329456	-8.772606	1.956877
-1469.891000	-13.600558	1.961882
-1473.567383	-7.820442	1.966886
-1477.506080	-7.678999	1.971891
-1480.951973	-6.396659	1.976896
-1485.230581	-2.417518	1.981901
-1488.961856	2.614212	1.986906
-1492.465167	-7.466979	1.991910
-1496.533794	-8.488493	1.996915
-1500.353110	-12.205445	2.006912
-1500.908427	-8.641282	2.016909
-1498.268050	-12.194139	2.026906
-1496.038149	-10.712641	2.036902
-1494.040615	-12.804227	2.046899
-1491.705797	-4.273219	2.056896
-1489.744092	-9.848744	2.066893
-1487.872724	-10.749226	2.076890
-1486.331349	-3.069133	2.086886
-1484.388400	-11.280247	2.096883
-1482.166650	-11.463941	2.106880
-1480.248226	-9.778743	2.116877
-1478.326484	-13.086797	2.126874
-1476.659133	-10.806357	2.136870
-1474.700128	-10.743350	2.146867
-1472.942460	-8.232998	2.156864
-1470.913853	-13.099935	2.166861
-1468.732502	-13.149028	2.176858
-1467.078317	-3.805900	2.186854
-1465.392148	-12.374822	2.196851
-1463.592522	-15.104249	2.206848
-1461.435393	-14.230711	2.216845
-1459.281199	-14.905888	2.226842
-1457.831649	-6.619960	2.236838
-1455.914001	-7.453684	2.246835
-1454.061929	-6.822561	2.256832
-1452.218717	-6.725028	2.266829
-1449.927633	-6.683884	2.276826
-1448.330420	-6.748413	2.286822
-1446.570725	-4.967164	2.296819
-1444.360277	-7.905879	2.306816
-1442.619407	-8.061084	2.316813
-1440.569428	-8.486756	2.326810
-1438.848844	-9.640727	2.336806
-1436.787791	-8.329771	2.346803
-1434.962064	-8.469119	2.356800
-1433.229999	-13.572810	2.366797
-1431.726789	-12.143494	2.376794
-1429.544462	-14.143095	2.386790
-1427.793848	-6.560969	2.396787
-1425.464520	-7.338538	2.406784
-1423.457888	-5.994119	2.416781
-1421.879625	-10.658391	2.426778
-1420.270558	-13.953019	2.436774
-1418.237024	-11.292823	2.446771
-1415.903668	-7.153877	2.456768
-1414.333213	-13.550591	2.466765
-1412.782718	-9.719006	2.476762
-1410.641250	-11.122320	2.486758
-1409.114283	-10.068969	2.496755
-1406.709705	-17.913159	2.506752
-1404.844204	-9.742531	2.516749
-1403.021020	-8.981536	2.526746
-1401.395274	-10.867332	2.536742
-1399.579629	-11.664539	2.546739
-1397.293032	-15.464826	2.556736
-1395.514695	-10.555904	2.566733
-1393.746294	-8.690763	2.576730
-1391.918970	-7.970785	2.586726
-1389.774475	-7.181193	2.596723
-1387.938936	-9.297861	2.606720
-1386.432712	-7.662746	2.616717
-1384.437792	-5.653133	2.626714
-1382.587739	-8.038663	2.636710
-1380.552892	-7.607262	2.646707
-1378.605443	-9.265736	2.656704
-1376.474606	-12.645628	2.666701
-1375.105537	-5.348882	2.676698
-1373.201778	-5.922111	2.686694
-1370.824299	-7.849288	2.696691
-1368.913885	-9.205779	2.706688
-1367.563715	-7.532785	2.716685
-1365.534415	-7.316603	2.726682
-1363.698089	-4.802719	2.736678
-1362.070455	-5.770753	2.746675
-1360.147828	-5.115741	2.756672
-1358.131588	-6.921975	2.766669
-1356.313224	-11.107371	2.776666
-1354.305594	-7.113205	2.786662
-1352.241520	-2.387712	2.796659
-1350.456566	-6.753908	2.806656
-1348.320647	-7.093123	2.816653
-1346.997442	-8.210812	2.826650
-1345.026536	-10.440426	2.836646
-1342.822537	-9.467378	2.846643
-1341.001379	-2.036042	2.856640
-1339.375260	-7.998475	2.866637
-1337.495945	-8.127620	2.876634
-1335.798658	-2.235295	2.886630
-1333.709691	-4.007375	2.896627
-1331.618302	-7.497848	2.906624
-1329.421340	-7.041705	2.916621
-1328.097197	-1.710111	2.926618
-1326.366843	-3.449441	2.936614
-1324.317662	-3.304235	2.946611
-1322.296508	-3.928431	2.956608
-1320.277495	-3.498232	2.966605
-1318.418312	-3.656713	2.976602
-1316.723271	-4.877386	2.986598
-1314.776034	-9.512124	2.996595
-1313.281534	-14.224417	3.006592
-1311.201653	-10.065979	3.016589
-1309.123708	-5.477218	3.026586
-1307.136096	-11.004159	3.036582
-1305.426212	-9.714234	3.046579
-1303.812302	-5.552428	3.056576
-1301.656633	-9.428983	3.066573
-1299.663492	-6.964530	3.076570
-1297.928260	-6.727053	3.086566
-1296.062689	-13.630492	3.096563
-1294.350057	-6.145715	3.106560
-1292.450678	-2.788182	3.116557
-1290.030305	-6.173105	3.126554
-1288.791976	-7.506211	3.136550
-1286.721549	-4.779564	3.146547
-1284.999605	-14.436660	3.156544
-1282.662379	-12.619765	3.166541
-1280.863225	-6.155257	3.176538
-1279.381395	-3.294711	3.186534
-1277.520204	-1.967921	3.196531
-1275.286331	-2.858643	3.206528
-1273.423623	-7.896584	3.216525
-1271.766375	-1.120775	3.226522
-1269.696025	-0.812794	3.236518
-1267.769243	-3.843398	3.246515
-1265.973065	-2.488048	3.256512
-1264.005422	-10.384782	3.266509
-1262.543071	-6.108402	3.276506
-1260.586978	-4.400322	3.286502
-1258.230340	-4.089732	3.296499
-1256.855584	-8.671970	3.306496
-1254.864556	-11.405732	3.316493
-1252.828533	-4.604465	3.326490
-1251.187091	-4.439388	3.336486
-1248.758597	-9.652346	3.346483
-1247.332450	-4.433488	3.356480
-1245.572717	-8.638808	3.366477
-1243.478506	-4.824256	3.376474
-1241.614507	-9.041949	3.386470
-1239.859747	-10.077614	3.396467
-1238.209556	-0.367322	3.406464
-1235.850262	-5.500810	3.416461
-1234.157578	-0.895243	3.426458
-1232.716514	-5.667498	3.436454
-1230.465320	-10.540942	3.446451
-1228.347312	-7.784101	3.456448
-1226.243634	-12.883958	3.466445
-1224.848596	-4.168456	3.476442
-1222.971753	-3.007947	3.486438
-1221.272291	-7.196190	3.496435
-1218.840232	-11.407095	3.506432
-1217.138473	-10.414121	3.516429
-1215.528455	-11.765590	3.526426
-1213.585105	-9.318232	3.536422
-1211.701517	-5.764295	3.546419
-1209.737717	-8.760524	3.556416
-1207.891133	-15.303793	3.566413
-1205.944479	-10.083805	3.576410
-1204.308205	-10.927586	3.586406
-1202.126944	-12.740745	3.596403
-1200.445722	-16.669354	3.606400
-1198.356845	-10.581401	3.616397
-1196.349032	-11.875105	3.626394
-1195.000248	-9.754831	3.636390
-1192.563287	-7.425824	3.646387
-1190.741633	-6.793310	3.656384
-1189.210633	-9.996595	3.666381
-1187.402032	-17.555348	3.676378
-1185.366633	-12.034422	3.686374
-1183.352570	-15.230552	3.696371
-1181.718495	-8.260628	3.706368
-1179.827939	-17.254632	3.716365
-1177.697014	-10.143573	3.726362
-1175.870918	-9.302749	3.736358
-1174.190565	-6.410255	3.746355
-1172.090187	-6.411300	3.756352
-1170.324583	-10.325539	3.766349
-1168.369878	-8.025546	3.776346
-1166.471831	-14.122751	3.786342
-1164.614023	-3.809417	3.796339
-1163.111823	-11.101344	3.806336
-1161.095990	-7.966094	3.816333
-1159.087037	-11.885363	3.826330
-1157.341015	-7.259676	3.836326
-1155.177511	-12.754316	3.846323
-1153.484967	-11.128976	3.856320
-1151.454353	-10.458819	3.866317
-1149.684030	-8.127155	3.876314
-1147.834235	-5.769616	3.886310
-1145.980923	-7.753679	3.896307
-1144.101958	-7.163393	3.906304
-1141.616196	-7.863729	3.916301
-1140.182615	-6.118430	3.926298
-1138.744293	-0.704802	3.936294
-1136.831905	-6.669298	3.946291
-1134.827894	-7.111431	3.956288
-1132.534607	-4.275953	3.966285
-1131.208920	-6.502966	3.976282
-1129.109128	-6.373470	3.986278
-1126.876492	-11.556685	3.996275
-1125.201277	-6.488835	4.006272
-1123.392558	-11.247518	4.016269
-1121.524930	-7.105093	4.026266
-1119.796519	-8.003394	4.036262
-1117.778761	-8.887354	4.046259
-1115.881861	-9.173948	4.056256
-1113.716433	-8.474359	4.066253
-1111.982680	-10.650501	4.076250
-1110.629111	-8.991440	4.086246
-1108.624530	-10.768683	4.096243
-1106.593198	-14.805197	4.106240
-1104.253952	-11.864961	4.116237
-1102.389542	-9.846631	4.126234
-1100.950936	-8.184384	4.136230
-1099.124848	-6.354706	4.146227
-1097.436151	-9.494141	4.156224
-1095.526746	-7.979128	4.166221
-1093.300170	-15.397391	4.176218
-1091.529334	-10.661720	4.186214
-1089.210377	-8.839206	4.196211
-1087.688555	-13.271964	4.206208
-1085.994458	-14.856374	4.216205
-1084.285644	-8.757241	4.226202
-1082.223571	-8.886432	4.236198
-1080.124549	-5.685986	4.246195
-1078.791176	-15.413438	4.256192
-1076.374825	-4.412651	4.266189
-1074.121479	-7.064908	4.276186
-1072.797176	-12.855287	4.286182
-1071.049349	-9.252678	4.296179
-1069.083443	-13.845071	4.306176
-1066.987074	-18.162268	4.316173
-1064.894042	-11.009464	4.326170
-1063.522707	-16.558537	4.336166
-1061.752467	-11.069082	4.346163
-1059.780792	-11.485077	4.356160
-1057.854326	-11.892123	4.366157
-1055.516029	-9.330307	4.376154
-1053.618286	-10.124470	4.386150
-1052.086365	-7.369264	4.396147
-1050.613772	-13.825736	4.406144
-1048.384058	-15.517905	4.416141
-1046.556320	-16.258547	4.426138
-1044.697398	-14.175224	4.436134
-1042.602266	-4.992564	4.446131
-1040.689588	-11.615889	4.456128
-1039.001544	-12.220303	4.466125
-1037.248804	-14.240801	4.476122
-1035.145109	-9.601380	4.486118
-1033.393189	-9.360335	4.496115
-1031.434164	-9.222035	4.506112
-1029.633858	-8.279496	4.516109
-1027.693737	-17.683887	4.526106
-1025.861403	-11.652966	4.536102
-1024.041254	-10.399243	4.546099
-1022.012932	-12.438596	4.556096
-1020.256373	-6.583966	4.566093
-1018.243747	-11.230600	4.576090
-1016.441496	-9.509427	4.586086
-1014.511766	-14.093215	4.596083
-1012.637994	-17.384933	4.606080
-1010.899005	-16.954724	4.616077
-1008.799968	-19.093552	4.626074
-1007.007334	-18.267461	4.636070
-1005.169599	-20.388299	4.646067
-1003.534591	-16.602279	4.656064
-1001.749348	-13.098148	4.666061
-999.378600	-18.325169	4.676058
-997.616264	-15.437191	4.686054
-995.935655	-16.224481	4.696051
-993.870350	-19.573181	4.706048
-992.020778	-18.046664	4.716045
-989.943117	-11.983543	4.726042
-988.151550	-13.056647	4.736038
-986.213672	-13.222565	4.746035
-984.868817	-13.372827	4.756032
-982.504300	-15.488455	4.766029
-980.845341	-16.720587	4.776026
-978.932348	-9.027001	4.786022
-977.305993	-11.186234	4.796019
-975.278836	-12.822644	4.806016
-973.207893	-19.540298	4.816013
-971.481887	-18.262882	4.826010
-969.535243	-18.340189	4.836006
-967.716326	-16.191077	4.846003
-965.814085	-10.470907	4.856000
-963.746164	-16.256524	4.865997
-961.874905	-8.808700	4.875994
-960.354098	-11.201953	4.885990
-958.134321	-17.674037	4.895987
-956.445229	-16.355498	4.905984
-954.454597	-14.247715	4.915981
-952.593551	-14.127337	4.925978
-951.218118	-12.354599	4.935974
-948.855615	-14.197167	4.945971
-946.780176	-14.468887	4.955968
-945.319854	-13.032027	4.965965
-942.795318	-11.799600	4.975962
-941.538404	-10.849104	4.985958
-940.040935	-9.492129	4.995955
-937.860000	-7.732386	5.005952
-935.577773	-20.021634	5.015949
-933.760938	-16.382991	5.025946
-931.764898	-15.356635	5.035942
-930.272380	-14.976561	5.045939
-928.401099	-6.028498	5.055936
-926.240799	-12.961847	5.065933
-924.621283	-14.182049	5.075930
-922.553064	-13.259373	5.085926
-921.037437	-12.040671	5.095923
-918.683943	-16.168373	5.105920
-916.825526	-21.662697	5.115917
-915.046218	-19.867986	5.125914
-912.942357	-16.943748	5.135910
-911.466195	-12.897640	5.145907
-909.690413	-24.492890	5.155904
-907.619278	-19.732806	5.165901
-905.585903	-15.140921	5.175898
-903.983450	-19.870830	5.185894
-902.032609	-19.041815	5.195891
-900.095037	-22.320726	5.205888
-898.209741	-23.562830	5.215885
-896.465446	-21.054276	5.225882
-894.499295	-15.852495	5.235878
-892.619729	-18.844402	5.245875
-890.835148	-18.263886	5.255872
-888.961086	-12.215162	5.265869
-886.608828	-13.141813	5.275866
-884.674712	-11.229409	5.285862
-883.434038	-13.399074	5.295859
-881.501661	-13.583366	5.305856
-879.350640	-16.698537	5.315853
-877.538737	-14.863954	5.325850
-875.980758	-9.866768	5.335846
-874.051887	-14.816714	5.345843
-871.696050	-10.315732	5.355840
-869.842835	-8.408008	5.365837
-868.331548	-4.031190	5.375834
-866.464857	-11.955104	5.385830
-864.620308	-6.720179	5.395827
-862.591171	-13.414015	5.405824
-860.617269	-12.327309	5.415821
-858.935385	-9.428224	5.425818
-857.015912	-13.879769	5.435814
-854.813811	-9.665790	5.445811
-852.671524	-14.023183	5.455808
-851.668890	-10.974304	5.465805
-849.818220	-10.616553	5.475802
-847.684981	-10.739666	5.485798
-845.614473	-9.598793	5.495795
-843.601889	-12.881468	5.505792
-842.269881	-12.554830	5.515789
-840.011079	-14.808345	5.525786
-837.982756	-12.157235	5.535782
-836.421674	-5.234693	5.545779
-834.250977	-7.598366	5.555776
-832.470834	-9.874054	5.565773
-830.839595	-9.596008	5.575770
-828.947674	-11.704341	5.585766
-827.028906	-5.945043	5.595763
-824.852193	-7.343449	5.605760
-823.144015	-7.669054	5.615757
-821.375149	-7.998356	5.625754
-819.478013	0.985644	5.635750
-817.674632	-3.704036	5.645747
-815.586768	-4.991150	5.655744
-813.725588	-7.818625	5.665741
-811.822277	-4.546900	5.675738
-809.836876	-6.243255	5.685734
-808.413495	-5.101158	5.695731
-806.155033	-6.142482	5.705728
-804.569266	-8.396653	5.715725
-802.462480	-3.632351	5.725722
-800.593501	-5.603943	5.735718
-798.115110	-9.004886	5.745715
-797.013302	-10.157524	5.755712
-795.385552	-12.365939	5.765709
-793.396818	-8.918771	5.775706
-791.242548	-5.654937	5.785702
-789.365386	-10.257278	5.795699
-787.621876	-15.679272	5.805696
-785.466264	-11.462018	5.815693
-783.716132	-9.934147	5.825690
-782.001047	-8.591938	5.835686
-779.909581	-10.509624	5.845683
-778.225621	-15.264154	5.855680
-776.315016	-11.574345	5.865677
-774.252573	-7.721684	5.875674
-772.336140	-8.640657	5.885670
-770.935156	-7.876874	5.895667
-768.982816	-12.699597	5.905664
-766.806444	-4.131046	5.915661
-764.952600	-6.191319	5.925658
-763.189090	-6.408624	5.935654
-761.294213	-3.530245	5.945651
-759.252254	-8.589666	5.955648
-757.232881	-7.486607	5.965645
-755.605747	-11.685589	5.975642
-753.636255	-4.547368	5.985638
-752.031047	-0.697631	5.995635
-750.211642	-9.081719	6.005632
-748.218620	-8.120362	6.015629
-745.917962	-5.762558	6.025626
-744.196885	-8.438701	6.035622
-742.985259	-5.882921	6.045619
-740.655064	-9.209788	6.055616
-738.619462	-2.978456	6.065613
-736.763159	-9.568281	6.075610
-734.851313	-8.633693	6.085606
-733.011700	-7.116415	6.095603
-731.353513	-5.956098	6.105600
-729.454217	-7.947092	6.115597
-727.446546	-9.325924	6.125594
-725.260436	2.237489	6.135590
-723.645011	-6.741949	6.145587
-722.137422	0.144377	6.155584
-720.081877	-7.847865	6.165581
-718.210122	-14.862816	6.175578
-716.113590	-1.527701	6.185574
-714.529768	-6.564993	6.195571
-712.212018	-6.724054	6.205568
-710.550223	-13.908875	6.215565
-708.634282	-7.546728	6.225562
-706.914057	-3.239691	6.235558
-704.998544	-0.636733	6.245555
-703.020899	-0.791565	6.255552
-701.511076	0.437700	6.265549
-699.325435	-3.061551	6.275546
-696.867369	-4.050128	6.285542
-695.654249	-4.835327	6.295539
-693.848857	-10.224831	6.305536
-691.720832	-10.602281	6.315533
-689.758789	-9.878242	6.325530
-688.129960	-2.555053	6.335526
-686.293150	-8.468467	6.345523
-684.465716	-8.132741	6.355520
-682.320954	-12.605095	6.365517
-680.509750	-5.501324	6.375514
-678.754560	-5.495848	6.385510
-676.491936	-4.754618	6.395507
-675.125481	-1.566962	6.405504
-672.911469	-11.432420	6.415501
-670.925258	-8.657411	6.425498
-669.531165	-14.691659	6.435494
-667.518627	-4.144556	6.445491
-665.741951	-7.736831	6.455488
-663.527151	-14.455336	6.465485
-662.150475	-5.507617	6.475482
-659.900229	-6.756920	6.485478
-657.927876	-0.002493	6.495475
-655.971100	-5.714375	6.505472
-654.108024	-12.552735	6.515469
-652.518856	-6.591349	6.525466
-650.510604	-4.255242	6.535462
-648.997753	-7.854010	6.545459
-646.734065	-3.961516	6.555456
-644.949329	-5.054256	6.565453
-643.040481	-11.405265	6.575450
-641.152180	-9.916063	6.585446
-639.125038	-12.032108	6.595443
-637.244313	-15.293253	6.605440
-635.645061	-17.337845	6.615437
-633.967633	-11.274221	6.625434
-631.860318	-10.113870	6.635430
-630.214299	-10.405020	6.645427
-627.920894	-12.809413	6.655424
-626.010347	-8.020037	6.665421
-624.009308	-8.015229	6.675418
-622.216934	-13.922969	6.685414
-620.594475	-8.411108	6.695411
-618.402995	-8.614056	6.705408
-616.703616	-18.610521	6.715405
-615.214628	-13.392717	6.725402
-613.416023	-10.704842	6.735398
-611.062891	-4.188441	6.745395
-609.399819	-5.400196	6.755392
-607.326395	-5.153283	6.765389
-605.513871	-7.765235	6.775386
-603.316335	-8.216223	6.785382
-601.511032	-10.368486	6.795379
-599.738255	-10.188940	6.805376
-598.214396	-5.484563	6.815373
-595.969970	-7.481370	6.825370
-594.388088	-9.139611	6.835366
-592.336072	-8.775592	6.845363
-590.561736	-3.140781	6.855360
-588.610501	-10.134548	6.865357
-586.696001	-7.461410	6.875354
-584.695593	-8.346101	6.885350
-583.421480	-11.457687	6.895347
-581.460275	-8.501288	6.905344
-579.212669	-8.585798	6.915341
-577.111538	-14.913655	6.925338
-575.484572	-13.651489	6.935334
-573.754153	-6.414054	6.945331
-571.521026	-13.172419	6.955328
-569.835834	-14.382421	6.965325
-568.175816	-15.464006	6.975322
-566.006442	-6.069326	6.985318
-564.075566	-10.554725	6.995315
-562.477216	-9.857541	7.005312
-560.716163	-9.193017	7.015309
-558.372448	-6.148897	7.025306
-556.559515	-7.622288	7.035302
-555.105003	-4.342993	7.045299
-552.688661	-7.963173	7.055296
-551.110096	-9.093220	7.065293
-549.166002	-12.567554	7.075290
-547.371729	-12.153361	7.085286
-545.758719	-14.564275	7.095283
-543.468675	-12.047639	7.105280
-541.597868	-11.449364	7.115277
-539.864386	-11.519940	7.125274
-537.810745	-13.568164	7.135270
-536.136727	-12.363852	7.145267
-534.214547	-14.983524	7.155264
-532.379236	-14.160997	7.165261
-530.379663	-17.598205	7.175258
-528.757977	-15.004431	7.185254
-526.753854	-10.882376	7.195251
-524.894042	-12.206898	7.205248
-522.965916	-16.609604	7.215245
-520.811335	-17.807249	7.225242
-519.218572	-12.499318	7.235238
-517.734013	-15.247828	7.245235
-515.462816	-11.094919	7.255232
-513.489780	-15.270965	7.265229
-511.348421	-11.280738	7.275226
-509.762483	-14.361625	7.285222
-507.999828	-10.171651	7.295219
-505.953508	-12.371552	7.305216
-504.126077	-15.131065	7.315213
-502.584761	-15.415269	7.325210
-500.768163	-8.420625	7.335206
-498.472537	-4.480569	7.345203
-496.405413	-13.721610	7.355200
-494.630667	-18.045030	7.365197
-492.881446	-19.804271	7.375194
-491.187615	-13.404699	7.385190
-489.122958	-17.494489	7.395187
-487.364184	-22.447112	7.405184
-485.214737	-16.137960	7.415181
-483.699996	-17.470843	7.425178
-481.748866	-18.275896	7.435174
-480.003654	-15.036964	7.445171
-477.668748	-18.371226	7.455168
-475.825200	-20.458862	7.465165
-474.215476	-16.535886	7.475162
-472.386037	-18.940038	7.485158
-470.286629	-15.523952	7.495155
-468.687956	-15.566234	7.505152
-466.677201	-14.333116	7.515149
-464.812820	-13.900091	7.525146
-462.719906	-17.775769	7.535142
-460.938510	-13.088255	7.545139
-459.166502	-5.342146	7.555136
-457.201817	-11.541815	7.565133
-455.286871	-13.674495	7.575130
-453.577441	-11.464083	7.585126
-451.371398	-11.883258	7.595123
-449.987330	-9.572761	7.605120
-447.973204	-14.389359	7.615117
-445.865320	-8.961097	7.625114
-444.394547	-6.478537	7.635110
-442.304653	-5.075208	7.645107
-440.077217	-9.533185	7.655104
-438.579844	-5.692092	7.665101
-436.747475	-12.589924	7.675098
-434.705397	-8.653366	7.685094
-432.697051	-7.315086	7.695091
-430.962341	-8.190486	7.705088
-429.246351	-8.827918	7.715085
-427.201967	-7.929368	7.725082
-425.514094	-2.697783	7.735078
-423.392360	-12.391203	7.745075
-421.676084	-15.904653	7.755072
-419.900972	-11.598214	7.765069
-417.934115	-7.280008	7.775066
-415.961964	-6.469840	7.785062
-413.917376	-12.035049	7.795059
-412.225860	-17.883126	7.805056
-410.473741	-19.221139	7.815053
-408.283869	-9.325194	7.825050
-406.634056	-13.333112	7.835046
-404.854976	-12.238067	7.845043
-402.697870	-9.220339	7.855040
-401.056517	-15.686617	7.865037
-399.021354	-14.378612	7.875034
-397.057366	-16.225247	7.885030
-395.232527	-7.515154	7.895027
-393.562626	-11.369219	7.905024
-391.947769	-11.794446	7.915021
-389.765405	-10.638552	7.925018
-387.940421	-18.986720	7.935014
-385.833728	-13.498942	7.945011
-383.959142	-12.139274	7.955008
-382.057116	-13.120425	7.965005
-380.267769	-18.231996	7.975002
-378.603503	-18.764893	7.984998
-376.710840	-13.950198	7.994995
-374.717975	-6.035239	8.004992
-372.870394	-11.574935	8.014989
-370.840761	-15.136195	8.024986
-368.802051	-14.171434	8.034982
-367.137877	-7.353717	8.044979
-365.542398	-15.802812	8.054976
-363.236682	-13.482421	8.064973
-361.371701	-16.072054	8.074970
-359.702397	-15.317410	8.084966
-358.186331	-18.875536	8.094963
-355.952433	-12.247237	8.104960
-354.049500	-15.568992	8.114957
-352.100682	-18.286429	8.124954
-350.146146	-12.031503	8.134950
-348.368368	-10.945301	8.144947
-346.635151	-9.851455	8.154944
-344.738880	-14.763197	8.164941
-342.645653	-13.184127	8.174938
-340.591555	-15.497136	8.184934
-339.478601	-9.787096	8.194931
-337.622660	-17.810160	8.204928
-335.330419	-13.703839	8.214925
-333.129843	-17.270297	8.224922
-331.645289	-18.179421	8.234918
-329.580202	-16.133117	8.244915
-327.703401	-9.024619	8.254912
-325.796029	-10.588419	8.264909
-324.070145	-11.799383	8.274906
-322.380867	-15.462698	8.284902
-320.441251	-11.531035	8.294899
-318.483715	-9.586026	8.304896
-316.298517	-18.655178	8.314893
-314.684377	-14.639229	8.324890
-312.434251	-18.764710	8.334886
-310.856733	-9.948523	8.344883
-309.182250	-8.763173	8.354880
-307.273119	-13.800019	8.364877
-305.361526	-14.529052	8.374874
-303.455023	-14.398013	8.384870
-301.766032	-19.716825	8.394867
-299.454556	-14.887380	8.404864
-297.678295	-14.221010	8.414861
-295.801960	-17.235841	8.424858
-294.077629	-14.352103	8.434854
-292.168344	-12.321345	8.444851
-290.405266	-13.337907	8.454848
-288.307449	-21.862470	8.464845
-286.316982	-22.986800	8.474842
-284.159982	-15.602268	8.484838
-282.698684	-12.806596	8.494835
-281.127242	-15.657674	8.504832
-279.096546	-11.645577	8.514829
-277.168758	-22.665604	8.524826
-275.442815	-19.535522	8.534822
-273.218048	-11.511687	8.544819
-271.306858	-14.253465	8.554816
-269.731481	-17.304402	8.564813
-267.642996	-17.066633	8.574810
-265.908632	-26.549686	8.584807
-263.993315	-17.488292	8.594803
-262.500978	-20.469653	8.604800
-260.108872	-18.989628	8.614797
-258.207392	-17.365774	8.624794
-256.802828	-16.979472	8.634791
-255.006874	-13.933318	8.644787
-252.522498	-9.744897	8.654784
-250.321838	-20.144993	8.664781
-248.746332	-16.050857	8.674778
-247.040829	-18.184680	8.684775
-245.285043	-13.851135	8.694771
-243.579730	-18.367280	8.704768
-241.618251	-14.332227	8.714765
-239.648837	-12.997061	8.724762
-237.794055	-10.893300	8.734759
-236.214121	-13.332821	8.744755
-233.886840	-15.086378	8.754752
-231.911042	-9.035412	8.764749
-230.011344	-20.888859	8.774746
-227.906236	-23.001893	8.784743
-226.590894	-21.898378	8.794739
-224.760798	-20.452364	8.804736
-222.602733	-23.908329	8.814733
-220.942956	-19.785557	8.824730
-218.863255	-21.189957	8.834727
-217.199282	-20.969070	8.844723
-215.070133	-23.871909	8.854720
-213.442054	-29.589684	8.864717
-211.491269	-24.681732	8.874714
-209.348153	-25.095134	8.884711
-207.995215	-15.870466	8.894707
-205.622480	-18.798874	8.904704
-203.736384	-24.819371	8.914701
-202.309949	-19.089545	8.924698
-200.257049	-23.751049	8.934695
-198.586687	-25.726274	8.944691
-196.675800	-21.938624	8.954688
-194.402698	-20.715990	8.964685
-192.671612	-25.870461	8.974682
-190.992532	-23.802549	8.984679
-188.797707	-18.236512	8.994675
-186.933673	-20.663086	9.004672
-185.212346	-22.130502	9.014669
-183.439222	-22.916754	9.024666
-181.285003	-22.798902	9.034663
-179.411355	-18.043693	9.044659
-177.941082	-20.115808	9.054656
-175.849833	-14.994796	9.064653
-173.979123	-18.352847	9.074650
-172.210585	-15.058503	9.084647
-169.984448	-16.516845	9.094643
-168.109806	-14.040216	9.104640
-166.635928	-13.257120	9.114637
-164.503922	-17.932968	9.124634
-162.634545	-16.680206	9.134631
-160.874769	-15.151361	9.144627
-159.039944	-16.599896	9.154624
-157.192638	-11.454822	9.164621
-154.799328	-11.005667	9.174618
-153.163574	-12.423222	9.184615
-151.493122	-9.193460	9.194611
-149.528552	-14.325123	9.204608
-147.550547	-14.944938	9.214605
-146.020844	-16.921712	9.224602
-144.304298	-17.892693	9.234599
-141.949575	-13.021568	9.244595
-140.146134	-12.277987	9.254592
-138.328639	-12.768306	9.264589
-136.372524	-14.155823	9.274586
-134.569958	-18.566489	9.284583
-132.660195	-9.587064	9.294579
-130.909135	-10.890802	9.304576
-128.897295	-3.962260	9.314573
-126.814020	-7.963404	9.324570
-125.234625	-12.520362	9.334567
-123.419895	-6.499816	9.344563
-121.398280	-0.626590	9.354560
-119.483067	-6.412161	9.364557
-118.040332	-9.409874	9.374554
-115.506580	-18.842247	9.384551
-113.810658	-13.741146	9.394547
-112.005182	-12.426026	9.404544
-110.454218	-12.963899	9.414541
-108.211455	-6.666190	9.424538
-106.195175	-7.342348	9.434535
-104.346004	-7.202184	9.444531
-102.751739	-6.411256	9.454528
-100.706761	-7.841662	9.464525
-98.702902	-8.635832	9.474522
-97.230045	-10.690187	9.484519
-94.939936	-4.865758	9.494515
-93.414183	-8.480799	9.504512
-91.585066	-13.009036	9.514509
-89.671918	-11.636093	9.524506
-87.431943	-11.922979	9.534503
-85.934264	-8.484136	9.544499
-83.965784	-5.901437	9.554496
-81.662261	-13.881817	9.564493
-80.284512	-12.824527	9.574490
-77.978031	-12.869085	9.584487
-76.613640	-12.365967	9.594483
-74.504985	1.119232	9.604480
-72.698907	-1.858569	9.614477
-70.602435	-8.953727	9.624474
-68.866648	-4.272046	9.634471
-67.007367	-7.460132	9.644467
-65.152382	-7.636331	9.654464
-63.513394	-6.567712	9.664461
-61.403483	-1.795650	9.674458
-59.329698	-7.813507	9.684455
-57.383757	-8.611165	9.694451
-55.994512	-3.836462	9.704448
-54.065844	-2.774432	9.714445
-51.844814	-8.280832	9.724442
-50.000373	-10.989341	9.734439
-48.109630	-3.023102	9.744435
-46.082391	-4.485222	9.754432
-44.626336	-7.011334	9.764429
-42.750115	-14.628338	9.774426
-40.697488	-9.570585	9.784423
-39.022872	-8.422304	9.794419
-36.816489	-9.879963	9.804416
-35.271417	-9.920804	9.814413
-33.174461	-10.326209	9.824410
-31.213594	-9.883066	9.834407
-29.526374	1.167174	9.844403
-27.638734	-0.734195	9.854400
-25.985142	-2.651947	9.864397
-23.708941	-4.137776	9.874394
-21.606574	-6.114297	9.884391
-20.333471	-9.322397	9.894387
-18.144548	-8.334223	9.904384
-16.094308	-10.599795	9.914381
-14.416865	-8.560382	9.924378
-12.774307	-6.076692	9.934375
-10.614057	-4.312531	9.944371
-8.665194	-6.619210	9.954368
-7.183168	-12.738721	9.964365
-5.278655	-5.038037	9.974362
-3.722396	17.046200	9.984359
-2.760447	55.721638	9.994355
-1.291867	106.773928	10.004352
0.000000	152.179221	10.009357
-0.047930	191.662524	10.014362
0.651364	224.090529	10.019367
1.307952	260.368104	10.024371
1.769595	289.802011	10.029376
1.882939	315.398633	10.034381
2.036727	332.568600	10.039386
2.604810	343.274671	10.044391
2.654720	358.958597	10.049395
2.815348	368.008042	10.054400
3.157489	378.153692	10.059405
3.164367	398.977983	10.064410
2.847878	403.807192	10.069415
3.152799	408.684980	10.074419
3.183332	416.571016	10.079424
3.111359	415.765495	10.084429
3.555883	425.180360	10.089434
3.789098	431.558156	10.094439
3.977815	443.696264	10.099443
3.595789	432.346802	10.104448
3.796267	419.137012	10.109453
3.749130	444.124281	10.114458
3.979414	439.889691	10.119463
4.122234	446.452328	10.124467
3.786149	447.657413	10.129472
3.751337	440.518122	10.134477
4.045646	454.910155	10.139482
4.237672	448.421547	10.144487
3.849847	455.627390	10.149491
4.138045	466.627053	10.154496
4.053741	461.920625	10.159501
4.023380	469.339120	10.164506
4.300670	460.027830	10.169511
3.977102	470.616092	10.174515
4.395344	464.118690	10.179520
4.590904	460.924616	10.184525
4.309551	473.376628	10.189530
4.640002	464.241345	10.194535
4.443393	469.373691	10.199539
4.394106	475.996516	10.204544
4.854082	472.735393	10.209549
4.363727	483.936057	10.214554
4.676774	486.435058	10.219559
4.613054	491.702516	10.224563
4.688559	490.870521	10.229568
5.168750	507.912877	10.234573
5.041124	506.862692	10.239578
5.300988	502.818007	10.244583
5.172470	498.794916	10.249587
5.265861	491.523492	10.254592
5.022178	485.976783	10.259597
5.239869	489.291055	10.264602
4.905078	498.943003	10.269607
4.898788	495.995498	10.274611
4.772351	504.836094	10.279616
4.897290	520.715338	10.284621
4.660384	528.765703	10.289626
5.341136	528.457147	10.294631
4.872443	535.982408	10.299635
4.837664	540.965061	10.304640
5.388055	552.225345	10.309645
5.630389	568.174901	10.314650
5.516250	564.788388	10.319655
5.488175	570.022919	10.324659
5.456898	563.131248	10.329664
5.630339	571.510740	10.334669
5.326075	575.269383	10.339674
5.598283	567.095710	10.344679
5.552216	574.124591	10.349683
5.538457	595.787133	10.354688
5.619843	602.379711	10.359693
5.692654	617.962473	10.364698
6.165566	606.158014	10.369703
6.192639	616.564283	10.374707
5.984759	612.985023	10.379712
6.331680	611.892937	10.384717
6.159527	629.458188	10.389722
5.982811	619.823604	10.394727
6.026183	624.753411	10.399731
5.965785	634.757069	10.404736
6.232777	630.644420	10.409741
6.051976	646.256880	10.414746
6.180736	650.743380	10.419751
6.411592	660.060815	10.424755
6.416888	667.746048	10.429760
6.611663	657.737884	10.434765
6.508705	667.199794	10.439770
6.497385	660.020060	10.444775
6.856607	667.680133	10.449779
6.544182	664.901926	10.454784
6.661805	672.968155	10.459789
6.793498	670.929307	10.464794
6.922143	666.621295	10.469799
6.688581	665.114800	10.474803
6.940204	688.614820	10.479808
7.040742	696.142028	10.484813
6.915297	708.762490	10.489818
7.602995	697.624542	10.494823
7.588705	705.514858	10.499827
7.252789	697.484464	10.504832
7.164299	686.146064	10.509837
6.767436	687.175670	10.514842
6.951579	708.971801	10.519847
6.748105	713.450943	10.524851
7.010614	716.773369	10.529856
7.155261	707.278627	10.534861
7.078310	727.627081	10.539866
7.395105	733.105688	10.544871
7.606312	745.768718	10.549875
7.643134	750.854027	10.554880
8.041968	748.953309	10.559885
7.767590	748.424839	10.564890
7.944285	751.876062	10.569895
7.888068	748.017350	10.574899
7.785304	752.859755	10.579904
8.049173	755.244867	10.584909
7.842344	760.159590	10.589914
8.250065	758.888125	10.594919
8.264585	757.563291	10.599923
8.183847	757.702266	10.604928
8.289442	766.217440	10.609933
7.958298	760.243136	10.614938
8.135596	758.778289	10.619943
8.241822	772.423272	10.624947
8.100928	773.855435	10.629952
8.514911	768.703485	10.634957
8.463632	776.100449	10.639962
8.264691	767.300493	10.644967
8.396983	762.433682	10.649971
8.040736	768.707426	10.654976
8.251464	764.161502	10.659981
8.138317	776.727016	10.664986
8.802603	796.102560	10.669991
8.646527	800.515970	10.674995
8.362290	804.674254	10.680000
8.928969	805.048797	10.685005
8.691150	804.542082	10.690010
8.712309	806.773425	10.695015
8.801992	806.083059	10.700019
8.682890	811.493934	10.705024
8.765024	805.424673	10.710029
8.797963	813.671282	10.715034
8.959291	816.064117	10.720039
9.109225	830.915851	10.725043
8.812616	842.606570	10.730048
8.965700	839.069970	10.735053
8.728410	846.572282	10.740058
9.013092	844.973358	10.745063
9.473466	850.257653	10.750067
8.900942	847.873742	10.755072
8.920386	856.866758	10.760077
9.019535	873.387486	10.765082
9.502095	873.245933	10.770087
9.616928	878.495933	10.775091
9.470861	884.241453	10.780096
9.683708	877.606599	10.785101
9.248385	888.689958	10.790106
9.567819	879.444219	10.795111
9.357625	882.407997	10.800115
9.334560	892.062395	10.805120
9.243662	906.633786	10.810125
9.272628	913.853637	10.815130
9.347170	917.044915	10.820135
9.727498	935.821562	10.825139
9.997898	949.618550	10.830144
10.243815	943.972730	10.835149
10.308214	959.970958	10.840154
10.406695	957.162902	10.845159
10.359465	957.944287	10.850163
10.171188	958.290385	10.855168
10.663511	961.140830	10.860173
10.159017	970.994269	10.865178
10.511177	962.297869	10.870183
10.222806	962.144420	10.875187
10.078511	963.761130	10.880192
10.584516	958.053343	10.885197
10.293076	971.677473	10.890202
10.220064	968.436978	10.895207
10.360470	961.369249	10.900211
10.603974	976.197973	10.905216
10.890421	980.738847	10.910221
10.837215	996.820830	10.915226
10.830543	994.131454	10.920231
11.125592	998.933359	10.925235
11.247811	1003.244635	10.930240
11.391076	994.888770	10.935245
10.901662	980.770088	10.940250
10.823950	976.802109	10.945255
11.217427	986.232383	10.950259
11.108233	1008.342911	10.955264
11.303729	1002.534400	10.960269
11.269206	1012.411100	10.965274
11.346082	1001.658327	10.970279
11.657320	1001.792859	10.975283
11.208231	1017.709451	10.980288
11.296967	1015.252792	10.985293
11.340652	1019.712539	10.990298
11.343493	1011.096531	10.995303
11.472289	1016.015368	11.000307
11.322400	1014.254096	11.005312
11.491877	1013.112672	11.010317
11.472585	1020.575715	11.015322
11.214919	1016.818976	11.020327
11.402358	1019.856312	11.025331
11.419836	1037.594374	11.030336
11.909105	1043.474966	11.035341
11.915270	1044.399965	11.040346
11.863608	1042.604875	11.045351
11.987289	1043.582356	11.050355
11.790847	1044.764725	11.055360
11.931619	1047.073488	11.060365
12.070432	1056.676153	11.065370
11.994591	1048.752170	11.070375
11.885501	1049.401272	11.075379
11.932188	1050.753929	11.080384
12.330471	1064.117380	11.085389
12.153464	1075.253290	11.090394
12.350822	1077.197881	11.095399
12.463224	1083.411922	11.100403
12.479605	1083.272535	11.105408
12.668156	1075.014653	11.110413
12.353937	1085.187250	11.115418
12.744041	1089.003013	11.120423
12.745482	1079.945495	11.125427
12.528248	1091.488184	11.130432
12.920830	1089.786656	11.135437
12.714283	1085.455475	11.140442
12.845985	1083.090123	11.145447
13.165093	1087.482534	11.150451
12.926872	1088.377200	11.155456
12.959764	1082.280748	11.160461
13.005754	1092.537643	11.165466
12.711777	1091.901205	11.170471
13.007739	1090.519797	11.175475
12.954442	1096.808044	11.180480
13.053108	1094.844672	11.185485
13.009894	1099.149998	11.190490
13.128124	1101.500134	11.195495
13.386204	1103.538923	11.200499
13.274571	1122.615278	11.205504
13.621565	1113.909812	11.210509
13.163479	1119.103781	11.215514
13.326132	1125.261065	11.220519
13.831731	1129.152562	11.225523
13.739969	1140.865616	11.230528
13.613311	1136.416907	11.235533
13.345192	1139.525271	11.240538
13.640763	1132.492044	11.245543
13.475404	1127.739313	11.250547
13.695238	1137.914719	11.255552
13.879653	1134.486367	11.260557
13.456313	1142.452564	11.265562
13.642243	1142.173184	11.270567
13.947497	1142.251506	11.275571
13.634188	1135.026227	11.280576
13.993196	1147.358319	11.285581
13.896198	1161.398489	11.290586
13.709071	1159.354636	11.295591
14.120562	1157.518806	11.300595
14.112159	1168.182975	11.305600
14.699297	1158.089850	11.310605
13.809941	1165.787405	11.315610
13.927038	1160.565046	11.320615
14.215707	1160.786740	11.325619
14.070737	1169.188384	11.330624
14.737032	1176.107237	11.335629
14.483759	1187.471831	11.340634
15.217533	1168.713469	11.345639
15.067138	1151.377396	11.350643
15.051651	1148.268317	11.355648
15.470147	1135.982919	11.360653
15.333153	1155.041163	11.365658
15.608310	1146.108783	11.370663
15.451043	1131.975250	11.375667
15.365252	1129.834683	11.380672
15.073222	1127.362765	11.385677
14.971681	1123.938444	11.390682
15.004382	1124.219420	11.395687
15.356997	1124.780282	11.400691
14.891425	1131.380022	11.405696
15.184279	1123.981341	11.410701
14.990417	1123.812081	11.415706
15.089545	1125.314833	11.420711
15.116993	1116.256388	11.425715
14.860319	1127.006518	11.430720
15.303224	1137.960393	11.435725
15.390057	1156.009596	11.440730
15.273068	1155.971235	11.445735
15.482680	1149.283532	11.450739
15.307634	1157.283744	11.455744
15.493779	1147.392407	11.460749
15.586927	1144.661021	11.465754
15.484064	1148.686059	11.470759
15.426174	1149.119148	11.475763
15.529409	1151.445810	11.480768
15.804401	1144.844794	11.485773
15.624991	1152.249695	11.490778
15.787506	1159.901502	11.495783
16.170744	1165.161632	11.500787
16.187155	1175.868525	11.505792
16.112555	1162.057110	11.510797
16.061179	1160.147878	11.515802
15.757025	1163.390320	11.520807
16.205749	1170.497266	11.525811
16.075473	1187.864908	11.530816
16.333217	1188.178748	11.535821
16.263259	1188.156007	11.540826
16.558835	1184.485555	11.545831
16.286965	1183.499924	11.550835
16.027645	1189.286684	11.555840
16.418288	1180.445012	11.560845
16.166113	1193.665888	11.565850
16.108020	1199.851971	11.570855
16.136097	1198.649513	11.575859
16.352757	1207.233124	11.580864
16.697020	1219.332535	11.585869
16.495967	1228.774498	11.590874
16.885042	1216.862771	11.595879
16.860696	1221.410819	11.600883
16.906688	1218.691848	11.605888
16.957868	1224.130512	11.610893
16.918061	1218.627138	11.615898
16.765641	1221.014223	11.620903
16.986921	1218.594808	11.625907
17.069885	1215.759365	11.630912
17.371542	1212.328263	11.635917
17.217448	1217.410536	11.640922
17.461345	1215.642119	11.645927
17.333955	1216.944505	11.650931
16.947185	1224.908421	11.655936
17.137806	1218.168286	11.660941
16.991588	1222.368936	11.665946
16.972566	1224.615912	11.670951
17.221226	1233.730505	11.675955
17.370147	1253.331169	11.680960
17.464829	1259.010285	11.685965
17.266694	1251.375197	11.690970
17.629538	1254.384874	11.695975
17.765660	1248.530004	11.700979
17.788697	1262.813767	11.705984
17.808912	1252.380805	11.710989
17.550744	1258.181604	11.715994
17.844334	1250.796554	11.720999
18.007489	1254.117578	11.726003
17.601111	1251.585902	11.731008
17.703043	1251.885010	11.736013
17.907619	1264.045118	11.741018
17.610348	1274.952707	11.746023
18.170558	1275.726276	11.751027
18.399781	1289.306411	11.756032
18.410229	1276.212563	11.761037
18.566174	1278.766658	11.766042
18.863689	1272.806343	11.771047
19.056033	1272.107039	11.776051
18.500144	1260.966388	11.781056
18.614328	1248.150044	11.786061
18.398529	1249.977203	11.791066
18.244938	1238.760091	11.796071
18.587394	1240.788773	11.801075
18.520256	1248.824610	11.806080
18.491024	1253.086133	11.811085
18.741998	1270.230602	11.816090
18.702661	1274.906370	11.821095
18.850981	1277.480325	11.826099
18.778973	1281.844718	11.831104
19.172154	1275.892867	11.836109
19.183469	1276.383569	11.841114
19.179566	1276.064497	11.846119
18.898244	1257.197440	11.851123
18.782094	1265.814855	11.856128
19.244022	1273.430382	11.861133
19.297561	1271.931049	11.866138
19.399853	1274.090126	11.871143
19.394740	1276.886180	11.876147
19.292416	1290.982250	11.881152
19.290704	1288.464871	11.886157
19.226412	1287.063109	11.891162
19.089049	1285.854668	11.896167
19.225923	1281.424681	11.901171
19.254216	1286.943871	11.906176
19.164319	1277.406496	11.911181
19.430710	1280.483637	11.916186
19.493410	1281.763305	11.921191
19.388144	1282.536894	11.926195
19.369240	1300.622157	11.931200
19.584183	1304.926303	11.936205
19.479077	1311.225493	11.941210
19.369194	1319.635807	11.946215
19.980965	1317.417455	11.951219
19.556233	1321.543909	11.956224
19.478343	1310.632720	11.961229
19.652698	1324.216767	11.966234
19.840045	1341.181956	11.971239
20.091980	1345.819251	11.976243
20.265522	1355.671547	11.981248
20.445251	1348.301237	11.986253
20.091398	1360.679143	11.991258
20.459375	1351.916657	11.996263
20.474481	1349.064798	12.001267
20.276900	1352.118476	12.006272
20.596709	1343.616891	12.011277
21.000583	1351.264910	12.016282
20.640657	1333.760871	12.021287
20.942639	1312.386977	12.026291
20.612380	1321.051397	12.031296
20.115801	1315.184586	12.036301
20.219703	1311.540653	12.041306
20.381882	1318.586664	12.046311
20.542045	1318.597495	12.051315
20.020171	1318.059332	12.056320
20.393466	1322.060801	12.061325
20.568316	1322.082535	12.066330
20.424062	1317.056911	12.071335
20.502264	1315.192549	12.076339
20.102994	1320.460974	12.081344
20.459382	1322.530306	12.086349
20.383298	1329.062952	12.091354
20.394130	1345.021417	12.096359
20.473094	1342.961916	12.101363
20.376228	1345.103833	12.106368
20.299789	1339.520642	12.111373
20.527096	1350.722033	12.116378
20.664858	1354.239673	12.121383
20.814234	1338.239129	12.126387
20.442616	1333.324326	12.131392
20.491548	1317.344183	12.136397
20.524089	1314.503947	12.141402
20.812743	1319.412050	12.146407
20.728121	1320.141048	12.151411
20.313053	1330.124248	12.156416
20.298341	1313.667117	12.161421
20.601995	1325.639361	12.166426
20.394535	1317.871627	12.171431
20.701914	1318.754470	12.176435
20.846718	1328.580886	12.181440
21.036443	1318.878698	12.186445
20.967736	1311.832849	12.191450
21.076234	1295.138291	12.196455
20.932111	1289.754226	12.201459
20.725368	1285.065385	12.206464
20.617524	1281.255261	12.211469
20.502799	1289.792313	12.216474
20.278467	1297.978681	12.221479
20.899929	1299.663477	12.226483
20.151556	1279.024334	12.231488
20.350612	1286.899679	12.236493
20.322312	1288.467322	12.241498
20.461661	1290.700575	12.246503
20.453832	1287.200149	12.251507
20.358439	1295.119274	12.256512
20.471222	1292.594894	12.261517
20.246778	1289.579642	12.266522
20.158707	1298.577531	12.271527
20.388862	1290.567012	12.276531
20.213471	1294.436757	12.281536
20.422238	1289.680225	12.286541
20.267455	1291.157448	12.291546
20.037743	1296.124025	12.296551
20.540951	1291.173717	12.301555
20.373361	1299.721812	12.306560
20.335263	1290.987931	12.311565
20.270426	1298.099698	12.316570
20.367634	1301.715466	12.321575
20.513992	1294.610249	12.326579
20.157753	1307.402214	12.331584
20.102532	1304.269521	12.336589
20.347305	1298.296529	12.341594
20.376804	1309.195089	12.346599
20.541987	1300.798592	12.351603
19.964372	1305.750216	12.356608
20.637747	1316.554174	12.361613
20.289269	1318.706859	12.366618
20.515966	1325.545228	12.371623
20.705119	1305.818220	12.376627
20.431938	1310.172507	12.381632
20.661353	1307.608391	12.386637
20.450148	1314.324465	12.391642
20.750524	1313.803614	12.396647
20.352823	1307.245630	12.401651
20.326501	1311.742727	12.406656
20.464140	1315.285248	12.411661
20.701053	1318.980884	12.416666
20.425880	1316.262092	12.421671
20.595036	1314.659641	12.426675
20.305019	1325.461019	12.431680
20.509765	1314.783213	12.436685
20.738296	1312.277276	12.441690
20.262007	1312.347888	12.446695
20.716407	1313.115916	12.451699
20.691640	1317.019052	12.456704
20.383458	1318.022043	12.461709
20.573940	1323.510280	12.466714
20.471232	1318.006602	12.471719
20.814706	1317.057565	12.476723
20.388626	1315.534275	12.481728
20.487543	1316.080222	12.486733
20.661064	1317.475104	12.491738
20.175035	1304.912417	12.496743
20.524959	1303.961090	12.501747
20.381784	1307.072143	12.506752
20.288977	1300.981763	12.511757
20.307346	1306.000547	12.516762
20.062822	1321.073937	12.521767
20.394653	1319.985182	12.526771
20.205194	1326.910694	12.531776
20.375677	1325.060509	12.536781
20.470581	1321.594173	12.541786
20.597310	1315.560096	12.546791
20.676412	1314.573096	12.551795
20.464091	1320.578034	12.556800
20.348652	1317.224344	12.561805
20.773797	1320.992314	12.566810
20.657062	1327.450217	12.571815
20.779628	1297.770893	12.576819
20.478428	1296.204877	12.581824
20.447122	1295.278651	12.586829
20.395910	1294.240179	12.591834
20.353454	1293.389287	12.596839
20.699133	1287.658739	12.601843
20.384356	1298.333683	12.606848
20.182919	1290.251108	12.611853
20.290290	1287.438311	12.616858
20.295869	1294.536820	12.621863
20.387009	1287.803843	12.626867
20.411865	1290.362653	12.631872
20.477788	1293.646276	12.636877
20.207925	1294.254663	12.641882
20.471937	1295.491920	12.646887
20.897543	1287.030647	12.651891
20.716934	1295.923214	12.656896
20.443196	1288.787395	12.661901
20.246805	1296.764890	12.666906
20.450955	1291.795988	12.671911
20.407423	1299.142133	12.676915
20.860981	1299.105423	12.681920
20.549329	1298.798063	12.686925
20.767015	1300.069712	12.691930
20.530491	1301.580293	12.696935
20.646673	1299.833765	12.701939
20.106601	1304.764741	12.706944
20.546248	1302.256951	12.711949
20.260613	1293.765250	12.716954
20.264411	1301.479867	12.721959
20.488113	1297.961057	12.726963
20.400094	1298.390237	12.731968
20.517363	1301.403738	12.736973
20.509111	1297.263108	12.741978
20.471771	1300.353250	12.746983
20.556791	1294.245410	12.751987
20.480179	1302.378426	12.756992
20.833924	1294.357768	12.761997
20.895991	1296.115974	12.767002
20.142971	1289.246282	12.772007
20.726435	1285.072492	12.777011
20.381640	1278.921903	12.782016
20.234481	1270.930691	12.787021
20.305904	1278.214485	12.792026
20.209021	1287.910995	12.797031
20.446588	1298.302155	12.802035
20.475818	1307.527836	12.807040
20.366428	1301.735962	12.812045
20.677312	1296.346119	12.817050
20.366890	1296.738824	12.822055
20.883786	1295.238992	12.827059
20.338546	1279.326814	12.832064
20.505068	1263.775387	12.837069
20.368565	1274.557119	12.842074
20.529764	1270.914425	12.847079
20.494534	1270.167297	12.852083
19.828701	1272.473863	12.857088
20.181307	1282.514099	12.862093
20.338605	1289.427905	12.867098
20.351169	1305.004314	12.872103
20.728632	1307.657804	12.877107
20.435195	1304.899514	12.882112
20.712154	1298.374283	12.887117
20.702502	1290.428565	12.892122
20.598078	1279.353390	12.897127
20.913073	1269.819232	12.902131
20.318864	1274.763823	12.907136
20.452709	1275.886421	12.912141
20.626030	1279.185180	12.917146
20.219817	1284.242807	12.922151
20.439436	1276.658451	12.927155
20.262731	1276.592432	12.932160
20.334191	1278.215998	12.937165
20.597896	1281.999795	12.942170
20.120577	1282.670594	12.947175
20.616796	1274.535515	12.952179
20.360674	1290.204558	12.957184
20.318345	1279.871118	12.962189
20.569133	1277.758876	12.967194
20.328299	1276.990552	12.972199
20.576971	1284.652517	12.977203
20.253687	1278.426002	12.982208
20.598268	1288.291956	12.987213
20.374886	1280.944214	12.992218
20.282708	1279.666052	12.997223
20.588352	1278.532842	13.002227
20.454742	1281.886596	13.007232
20.240068	1283.769225	13.012237
20.372468	1284.519038	13.017242
20.185643	1279.764414	13.022247
20.354544	1274.864325	13.027251
20.012231	1274.563802	13.032256
20.466396	1293.946390	13.037261
20.649910	1304.546956	13.042266
20.332305	1293.239898	13.047271
20.505081	1281.827057	13.052275
20.495539	1288.610387	13.057280
20.461359	1287.235042	13.062285
20.333295	1285.709212	13.067290
20.249734	1282.588488	13.072295
20.585017	1288.283599	13.077299
20.274358	1290.958358	13.082304
20.345372	1292.296207	13.087309
20.497318	1300.110161	13.092314
20.491748	1307.282825	13.097319
20.529643	1289.763521	13.102323
20.325176	1286.432997	13.107328
20.250346	1285.299099	13.112333
20.523800	1293.854072	13.117338
20.254545	1297.546882	13.122343
20.424039	1306.163897	13.127347
20.348712	1323.403056	13.132352
20.664768	1320.268282	13.137357
20.736664	1300.246380	13.142362
20.412666	1297.342933	13.147367
20.559898	1288.434775	13.152371
20.228061	1286.196239	13.157376
20.437134	1283.859434	13.162381
20.501255	1287.150865	13.167386
20.465630	1287.484218	13.172391
20.705955	1281.203699	13.177395
20.438623	1293.513428	13.182400
20.457117	1288.892548	13.187405
20.551471	1289.943758	13.192410
20.406457	1291.356147	13.197415
20.862043	1285.362804	13.202419
20.736904	1296.705508	13.207424
20.449273	1289.155616	13.212429
20.446493	1292.100092	13.217434
20.448232	1294.606023	13.222439
20.637283	1285.923989	13.227443
20.372108	1296.087524	13.232448
20.411385	1299.861648	13.237453
20.556258	1292.925637	13.242458
20.575281	1292.947640	13.247463
20.756710	1293.733654	13.252467
20.646528	1298.110517	13.257472
20.398342	1292.625081	13.262477
20.493917	1277.251203	13.267482
20.031855	1278.511105	13.272487
20.264159	1284.862961	13.277491
20.339069	1294.391860	13.282496
20.278814	1294.402193	13.287501
20.327221	1291.710427	13.292506
20.323135	1299.035599	13.297511
20.102068	1291.543768	13.302515
20.329643	1298.334606	13.307520
20.066583	1298.727085	13.312525
20.149451	1289.311269	13.317530
20.153148	1302.624157	13.322535
20.646376	1299.502038	13.327539
20.602834	1295.491408	13.332544
20.433222	1295.571413	13.337549
20.635455	1293.025776	13.342554
20.797997	1305.450102	13.347559
20.611700	1292.526949	13.352563
20.412683	1296.474562	13.357568
20.392328	1291.771130	13.362573
20.563294	1293.032630	13.367578
20.513987	1300.639903	13.372583
20.819603	1295.543863	13.377587
20.741385	1297.462704	13.382592
21.042393	1292.300744	13.387597
21.109946	1276.777720	13.392602
20.348840	1271.425630	13.397607
20.286051	1260.698599	13.402611
20.475016	1271.849270	13.407616
20.286018	1267.984773	13.412621
20.463550	1267.787754	13.417626
20.232935	1271.557618	13.422631
20.147488	1265.047563	13.427635
20.490321	1270.355315	13.432640
20.142778	1267.247092	13.437645
20.337231	1264.957403	13.442650
20.336658	1265.359351	13.447655
20.219647	1262.945035	13.452659
20.074977	1273.447505	13.457664
20.536840	1292.378764	13.462669
20.540109	1298.653446	13.467674
20.553951	1300.438869	13.472679
20.375492	1297.264938	13.477683
20.535006	1293.293311	13.482688
20.093272	1294.666968	13.487693
20.299227	1295.291274	13.492698
20.264629	1312.809232	13.497703
20.768621	1300.426151	13.502707
20.706603	1305.509246	13.507712
20.919708	1302.669237	13.512717
20.871312	1288.233865	13.517722
20.577705	1287.495904	13.522727
21.062381	1277.792514	13.527731
20.921922	1277.427381	13.532736
20.779276	1275.731944	13.537741
21.087214	1261.511821	13.542746
20.228368	1247.759398	13.547751
20.075783	1237.738184	13.552755
20.231488	1247.546890	13.557760
20.154386	1254.981666	13.562765
20.202630	1267.273188	13.567770
20.400205	1273.706785	13.572775
20.217132	1277.043360	13.577779
20.214648	1282.262294	13.582784
20.060280	1271.899911	13.587789
20.650502	1270.460536	13.592794
20.328542	1272.957620	13.597799
20.646754	1277.448925	13.602803
20.682012	1283.307188	13.607808
20.638212	1269.756454	13.612813
20.641314	1265.871258	13.617818
20.234253	1276.538326	13.622823
20.564065	1271.941443	13.627827
20.269921	1271.698978	13.632832
20.349125	1273.120686	13.637837
20.369265	1269.848367	13.642842
20.266442	1277.973233	13.647847
20.465193	1269.171517	13.652851
20.233146	1273.189526	13.657856
20.239069	1273.679572	13.662861
20.234648	1269.661058	13.667866
20.119447	1280.202296	13.672871
20.431437	1277.140072	13.677875
20.379753	1280.501095	13.682880
20.381722	1278.493884	13.687885
20.644667	1276.062184	13.692890
20.299950	1277.320520	13.697895
20.659694	1270.300308	13.702899
20.251707	1281.890054	13.707904
20.419630	1282.635750	13.712909
20.753282	1282.954341	13.717914
20.434118	1290.826565	13.722919
20.700920	1281.268688	13.727923
20.510947	1285.288565	13.732928
20.759645	1280.738351	13.737933
20.672388	1277.931294	13.742938
20.280642	1281.729971	13.747943
20.593653	1276.802015	13.752947
20.488193	1281.393989	13.757952
20.275935	1273.849339	13.762957
20.734254	1275.727106	13.767962
20.212399	1266.990128	13.772967
20.285674	1269.226022	13.777971
20.355981	1274.997745	13.782976
20.404414	1280.755852	13.787981
20.347141	1283.295584	13.792986
20.096611	1284.404348	13.797991
20.691867	1282.225544	13.802995
20.387399	1280.324558	13.808000
20.401338	1277.640284	13.813005
20.290589	1277.270847	13.818010
20.107067	1277.122312	13.823015
20.582356	1283.721458	13.828019
20.250252	1277.883699	13.833024
20.183551	1283.975368	13.838029
20.186111	1287.319198	13.843034
20.187335	1277.469353	13.848039
20.778596	1277.019420	13.853043
20.496775	1282.770599	13.858048
20.465463	1275.927173	13.863053
20.618107	1278.841840	13.868058
20.155715	1285.406360	13.873063
20.359340	1280.910849	13.878067
20.679124	1287.345208	13.883072
20.314137	1280.874786	13.888077
20.511898	1280.138631	13.893082
20.819165	1288.880439	13.898087
20.621347	1280.117895	13.903091
20.285658	1284.997638	13.908096
20.267202	1284.784485	13.913101
20.168881	1272.953124	13.918106
20.533509	1284.481455	13.923111
20.489188	1282.452180	13.928115
20.853783	1287.464096	13.933120
20.597795	1288.193263	13.938125
20.346965	1279.344676	13.943130
20.208046	1287.699951	13.948135
20.462360	1287.933853	13.953139
20.388576	1289.060077	13.958144
20.241453	1289.502548	13.963149
20.520617	1284.281966	13.968154
20.231692	1295.832360	13.973159
20.314878	1286.575177	13.978163
20.564305	1296.295606	13.983168
20.536793	1295.227806	13.988173
20.484723	1296.611628	13.993178
20.162469	1294.109733	13.998183
20.516292	1293.016814	14.003187
20.341444	1297.345159	14.008192
20.393416	1291.780617	14.013210
20.541855	1286.408619	14.018227
20.478601	1291.353379	14.023245
20.679567	1289.953445	14.028263
20.348891	1296.032345	14.033280
20.506264	1293.099587	14.038298
20.452439	1297.179268	14.043315
20.354861	1296.774701	14.048333
20.692033	1296.859819	14.053351
20.598301	1294.621749	14.058368
20.489320	1299.831068	14.063386
20.534127	1295.383611	14.068403
20.462495	1304.556181	14.073421
20.251532	1291.256490	14.078439
20.401634	1292.789953	14.083456
20.160276	1291.192605	14.088474
20.476919	1299.853284	14.093491
20.632619	1321.504966	14.098509
20.848692	1315.429172	14.103527
20.870705	1326.505562	14.108544
20.717938	1325.842716	14.113562
21.105387	1321.167197	14.118579
20.917419	1319.836702	14.123597
20.783658	1304.596418	14.128615
20.699859	1305.680965	14.133632
20.361012	1325.577907	14.138650
20.750064	1321.028109	14.143667
20.475591	1332.538838	14.148685
20.504108	1325.453368	14.153703
20.467519	1325.945515	14.158720
20.259788	1328.198269	14.163738
21.078900	1339.873896	14.168755
20.757871	1363.287848	14.173773
20.831751	1368.950922	14.178791
20.907242	1361.469549	14.183808
21.176289	1373.388741	14.188826
21.468172	1365.247763	14.193843
21.358770	1362.946222	14.198861
21.321615	1362.377342	14.203879
21.251037	1341.833165	14.208896
21.180085	1347.418692	14.213914
21.184683	1323.689696	14.218931
21.080229	1325.395559	14.223949
21.372817	1323.534202	14.228967
21.575705	1323.058432	14.233984
21.485831	1333.027527	14.239002
21.690029	1321.300877	14.244019
21.377809	1335.999478	14.249037
21.616683	1330.686770	14.254055
21.621808	1326.769385	14.259072
20.982854	1333.729186	14.264090
21.309325	1324.627092	14.269107
21.138824	1327.826308	14.274125
21.140883	1329.513121	14.279143
21.200083	1330.899166	14.284160
20.951124	1332.188427	14.289178
21.277608	1323.865538	14.294195
21.205767	1334.311902	14.299213
21.210986	1353.100182	14.304231
21.444201	1355.881725	14.309248
21.151904	1366.436782	14.314266
21.512992	1364.158913	14.319283
21.578550	1369.970673	14.324301
21.590175	1369.306413	14.329319
21.637461	1362.381504	14.334336
21.420802	1365.058669	14.339354
21.787144	1373.353747	14.344371
21.441798	1369.223582	14.349389
21.441390	1376.885808	14.354407
21.836873	1375.538744	14.359424
21.601399	1380.998934	14.364442
21.669977	1368.495029	14.369459
21.954774	1375.564995	14.374477
21.927836	1380.924857	14.379495
22.189983	1379.654990	14.384512
21.880376	1373.618119	14.389530
22.119829	1368.068268	14.394547
22.050254	1377.157843	14.399565
21.923878	1365.904413	14.404583
21.840238	1355.724082	14.409600
21.944916	1361.857116	14.414618
21.810365	1358.994873	14.419635
21.908135	1364.890486	14.424653
22.094875	1365.875103	14.429671
22.049323	1353.265570	14.434688
21.669505	1364.138023	14.439706
22.077736	1364.406646	14.444723
22.074071	1372.530102	14.449741
22.023678	1371.248462	14.454759
22.030286	1370.198805	14.459776
21.860456	1376.532862	14.464794
21.582305	1371.406041	14.469811
21.839984	1372.431256	14.474829
21.594718	1375.633457	14.479847
21.986159	1373.220842	14.484864
21.745661	1388.850593	14.489882
22.134763	1373.366248	14.494899
22.547449	1385.739608	14.499917
22.523320	1383.807732	14.504935
22.667053	1369.910492	14.509952
22.143496	1376.808003	14.514970
22.290527	1374.370752	14.519987
22.241794	1378.722835	14.525005
22.356704	1378.618874	14.530023
22.698473	1381.331411	14.535040
22.367991	1379.919824	14.540058
22.520359	1377.864371	14.545075
22.116141	1375.696849	14.550093
22.218481	1375.786400	14.555111
22.300795	1372.187298	14.560128
22.135587	1382.543787	14.565146
22.301860	1392.011871	14.570163
22.429852	1396.052923	14.575181
22.529377	1406.319939	14.580199
22.433601	1407.017137	14.585216
22.292310	1414.527141	14.590234
22.449383	1404.862254	14.595251
22.272843	1403.469157	14.600269
22.372478	1415.487119	14.605287
22.424935	1400.727462	14.610304
22.222565	1413.866600	14.615322
22.284716	1404.868840	14.620339
22.719569	1417.687681	14.625357
22.591909	1427.230201	14.630375
22.616023	1432.887263	14.635392
22.611296	1444.537276	14.640410
22.515655	1442.634191	14.645427
22.733315	1437.672757	14.650445
22.782547	1446.332512	14.655463
22.975239	1435.585013	14.660480
22.896001	1440.461687	14.665498
22.850276	1434.505150	14.670515
23.068732	1427.698910	14.675533
23.021721	1433.915466	14.680551
23.483170	1429.605612	14.685568
22.781634	1434.075937	14.690586
23.048384	1436.698186	14.695603
22.930872	1427.191400	14.700621
23.358098	1431.595763	14.705639
23.223966	1417.712261	14.710656
22.934733	1408.441642	14.715674
22.934292	1420.947286	14.720691
23.332428	1418.461856	14.725709
23.280182	1423.822527	14.730727
23.390318	1401.555780	14.735744
23.304478	1392.152257	14.740762
22.935797	1386.785021	14.745779
23.307921	1392.395788	14.750797
22.750278	1395.973630	14.755815
23.330372	1398.669326	14.760832
23.140298	1417.143102	14.765850
23.452739	1417.001730	14.770867
23.522345	1414.284411	14.775885
23.038678	1426.244109	14.780903
23.646304	1426.369086	14.785920
23.415935	1431.921341	14.790938
23.632793	1430.572612	14.795955
23.478005	1409.640775	14.800973
23.349380	1401.952230	14.805991
23.238974	1406.761789	14.811008
23.418635	1415.439720	14.816026
23.385622	1417.701117	14.821043
23.834120	1421.352543	14.826061
23.405605	1421.484290	14.831079
23.701833	1428.973622	14.836096
23.416921	1427.213631	14.841114
23.750794	1426.075178	14.846131
23.799407	1420.176496	14.851149
23.262330	1415.759475	14.856167
23.448128	1418.651925	14.861184
23.629993	1424.788680	14.866202
23.413814	1436.320989	14.871219
23.782789	1427.054052	14.876237
23.400244	1425.755335	14.881255
24.032721	1426.734798	14.886272
23.691020	1431.613158	14.891290
23.258001	1433.136761	14.896307
24.083649	1420.232118	14.901325
23.613444	1433.041960	14.906343
23.762274	1423.726935	14.911360
23.458183	1424.344485	14.916378
23.746592	1428.663189	14.921395
23.676255	1428.041329	14.926413
23.696612	1435.877206	14.931431
23.649291	1447.035655	14.936448
23.730967	1459.103979	14.941466
23.627131	1457.794090	14.946483
23.832221	1456.700552	14.951501
23.540287	1465.421569	14.956519
23.975156	1456.491778	14.961536
24.426597	1454.727986	14.966554
24.561741	1464.550306	14.971571
24.430990	1455.130032	14.976589
24.085171	1459.056649	14.981607
24.012047	1456.587440	14.986624
24.358255	1458.490092	14.991642
23.832039	1462.377553	14.996659
23.542377	1450.880772	15.001677
23.906005	1466.490492	15.006695
24.489907	1481.636433	15.011712
24.188228	1486.266979	15.016730
24.588560	1481.416351	15.021747
24.791273	1480.892570	15.026765
24.786556	1472.875233	15.031783
24.856383	1447.456740	15.036800
24.802079	1458.490398	15.041818
24.431871	1454.155002	15.046835
25.033030	1446.352334	15.051853
24.858908	1448.640292	15.056871
24.748718	1445.772674	15.061888
24.691091	1445.704596	15.066906
24.850630	1447.645552	15.071923
24.942200	1431.302623	15.076941
24.507253	1417.369507	15.081959
24.664315	1415.393567	15.086976
24.610012	1417.159352	15.091994
24.723528	1418.532943	15.097011
24.719624	1412.318432	15.102029
24.643640	1425.526076	15.107047
24.844771	1415.575648	15.112064
24.801727	1409.708828	15.117082
24.488065	1417.637009	15.122099
25.030404	1420.506915	15.127117
24.891205	1417.335585	15.132135
24.473982	1415.211629	15.137152
24.557593	1428.024159	15.142170
24.514247	1446.421626	15.147187
24.899113	1445.992611	15.152205
24.960284	1457.334455	15.157223
25.148453	1456.319023	15.162240
24.705614	1457.857699	15.167258
24.904458	1460.958966	15.172275
24.950127	1447.856503	15.177293
24.575678	1457.135418	15.182311
24.633926	1446.224330	15.187328
25.167183	1449.595456	15.192346
24.626671	1454.530354	15.197363
24.952385	1448.821182	15.202381
24.759429	1454.083536	15.207399
25.240609	1471.331937	15.212416
25.149230	1479.105096	15.217434
25.381240	1484.999394	15.222451
25.610363	1473.859362	15.227469
25.240015	1466.376420	15.232487
25.497850	1453.593123	15.237504
25.742892	1454.602792	15.242522
25.647920	1455.516412	15.247539
25.912083	1445.288990	15.252557
25.676837	1449.278937	15.257575
25.932791	1443.180506	15.262592
25.752184	1437.399472	15.267610
25.931277	1431.282725	15.272627
25.512774	1418.473672	15.277645
25.572600	1418.114169	15.282663
25.506545	1416.596210	15.287680
25.660827	1410.685714	15.292698
25.208091	1412.358772	15.297715
25.091818	1404.965775	15.302733
25.301518	1422.294924	15.307751
25.232763	1427.584404	15.312768
25.431045	1443.041725	15.317786
25.530990	1448.360562	15.322803
25.769599	1440.423581	15.327821
25.618255	1446.862776	15.332839
25.207996	1445.849939	15.337856
25.563739	1449.125897	15.342874
25.139988	1449.542289	15.347891
25.542515	1458.465131	15.352909
26.023704	1472.507694	15.357927
25.646614	1479.553383	15.362944
25.834169	1480.428407	15.367962
25.995762	1477.979193	15.372979
26.070883	1482.246284	15.377997
25.934896	1483.633128	15.383015
25.821321	1481.897303	15.388032
25.853800	1475.680073	15.393050
25.895696	1489.704654	15.398067
25.782362	1477.060575	15.403085
25.968754	1487.206441	15.408103
25.678378	1479.820422	15.413120
25.762322	1487.016224	15.418138
26.071422	1492.582315	15.423155
26.230726	1482.418127	15.428173
26.120446	1481.921629	15.433191
26.226693	1492.871479	15.438208
26.252445	1481.987986	15.443226
26.028676	1486.800469	15.448243
26.040892	1479.970113	15.453261
26.357853	1482.414058	15.458279
26.112124	1485.828981	15.463296
26.329128	1477.874818	15.468314
26.146461	1500.297041	15.473331
26.268379	1504.439960	15.478349
26.944223	1512.265075	15.483367
26.519825	1498.956913	15.488384
26.505318	1477.971796	15.493402
26.129503	1484.841265	15.498419
26.506264	1491.426570	15.503437
27.084234	1503.750423	15.508455
26.685726	1492.115563	15.513472
26.418844	1480.127008	15.518490
26.568992	1477.766380	15.523507
26.500520	1474.157671	15.528525
26.532817	1480.358285	15.533543
26.355447	1502.426023	15.538560
26.641519	1495.751482	15.543578
26.292038	1509.055308	15.548595
26.277763	1495.708331	15.553613
26.195737	1504.647737	15.558631
26.200565	1512.685155	15.563648
26.346027	1515.345538	15.568666
26.589757	1538.955078	15.573683
26.716386	1527.811318	15.578701
26.777397	1535.242989	15.583719
26.597893	1543.927054	15.588736
26.892536	1537.368755	15.593754
26.891421	1543.386914	15.598771
27.179747	1537.932966	15.603789
27.300008	1538.354915	15.608807
26.891603	1535.964048	15.613824
27.388903	1527.838559	15.618842
27.225825	1537.515580	15.623859
26.901466	1533.205375	15.628877
27.178913	1528.576217	15.633895
27.109435	1535.600295	15.638912
27.683936	1530.654429	15.643930
27.299132	1539.795783	15.648947
27.591884	1538.502151	15.653965
27.185656	1534.089435	15.658983
27.613492	1536.786850	15.664000
27.727357	1521.816135	15.669018
27.217656	1517.922005	15.674035
26.990801	1502.323827	15.679053
27.367524	1512.484719	15.684071
27.425386	1536.991175	15.689088
27.983628	1525.366285	15.694106
27.364151	1516.040007	15.699123
27.413544	1504.966598	15.704141
27.129141	1504.663751	15.709159
27.058298	1521.104398	15.714176
27.417910	1523.798545	15.719194
27.432226	1530.242445	15.724211
27.875566	1520.953647	15.729229
27.978075	1531.178103	15.734247
27.865426	1537.304368	15.739264
27.847939	1523.710648	15.744282
27.481935	1524.338817	15.749299
27.307717	1528.047032	15.754317
27.728522	1523.823263	15.759335
27.609552	1532.338659	15.764352
27.622067	1531.444687	15.769370
27.819622	1531.390342	15.774387
27.711250	1531.196698	15.779405
27.999726	1531.749271	15.784423
27.772801	1539.582712	15.789440
28.136101	1532.377143	15.794458
27.727388	1538.917595	15.799475
27.833484	1535.717964	15.804493
27.625503	1537.697139	15.809511
27.585061	1534.119047	15.814528
27.889136	1528.451750	15.819546
27.631084	1542.864850	15.824563
27.738083	1553.794532	15.829581
27.618059	1556.717000	15.834599
27.427833	1564.068913	15.839616
27.837196	1556.411686	15.844634
28.045032	1558.036862	15.849651
27.927237	1561.095184	15.854669
28.098536	1572.063466	15.859687
28.351326	1589.299576	15.864704
28.688040	1585.308737	15.869722
29.017713	1577.288350	15.874739
28.847682	1558.833213	15.879757
29.026218	1547.015113	15.884775
28.588306	1558.169343	15.889792
28.890147	1545.184705	15.894810
28.563350	1541.846279	15.899827
28.491471	1553.465363	15.904845
28.871646	1553.127711	15.909863
28.733380	1546.938940	15.914880
28.796554	1528.246195	15.919898
28.720348	1522.135780	15.924915
28.305142	1517.581285	15.929933
28.432327	1508.471910	15.934951
28.273366	1526.290806	15.939968
28.839387	1540.271243	15.944986
28.798763	1545.915428	15.950003
28.723792	1554.390217	15.955021
28.617322	1552.751208	15.960039
28.827787	1555.347692	15.965056
28.835441	1544.244007	15.970074
29.086494	1556.923198	15.975091
29.051740	1541.690119	15.980109
29.114618	1534.471878	15.985127
28.942345	1526.283614	15.990144
28.836396	1528.649668	15.995162
28.277495	1524.999036	16.000179
28.485118	1537.971516	16.005197
28.699421	1545.457626	16.010215
28.830148	1550.474731	16.015232
28.731921	1553.923046	16.020250
28.848279	1554.828394	16.025267
28.773366	1557.942362	16.030285
29.148676	1552.673517	16.035303
28.910344	1568.043205	16.040320
28.945488	1576.800734	16.045338
29.162095	1592.620062	16.050355
29.091510	1595.247808	16.055373
29.180299	1590.951012	16.060391
29.212890	1591.274596	16.065408
29.123978	1593.071534	16.070426
29.199281	1597.543766	16.075443
29.190919	1600.641607	16.080461
29.504439	1582.264575	16.085479
29.238422	1588.930205	16.090496
29.406213	1585.724317	16.095514
29.481716	1593.090138	16.100531
29.600102	1585.809988	16.105549
29.905000	1570.273738	16.110567
29.593559	1583.130110	16.115584
29.460317	1576.838487	16.120602
29.624495	1574.312429	16.125619
29.680787	1582.985224	16.130637
29.865538	1576.610729	16.135655
29.913991	1578.146687	16.140672
30.320357	1578.873165	16.145690
30.052402	1580.485422	16.150707
29.664151	1582.378963	16.155725
29.840680	1580.472508	16.160743
29.749833	1577.850789	16.165760
29.749362	1578.897836	16.170778
29.607058	1576.909418	16.175795
29.734656	1583.472909	16.180813
30.232056	1572.653385	16.185831
29.803016	1578.987473	16.190848
29.880503	1574.399674	16.195866
30.255086	1584.616104	16.200883
29.934563	1589.823202	16.205901
30.607561	1574.660890	16.210919
30.479815	1584.166116	16.215936
30.346047	1581.865176	16.220954
30.610710	1573.287371	16.225971
30.042917	1570.639542	16.230989
30.473015	1577.270864	16.236007
30.220764	1566.751941	16.241024
30.445336	1575.458485	16.246042
30.692844	1569.865052	16.251059
30.244718	1559.099766	16.256077
30.543829	1545.942348	16.261095
29.973989	1553.905070	16.266112
30.242022	1572.015414	16.271130
30.490798	1576.963857	16.276147
30.447548	1580.034995	16.281165
30.837279	1569.858411	16.286183
30.839550	1577.936070	16.291200
30.376177	1565.826789	16.296218
30.410474	1565.005074	16.301235
30.219932	1566.279612	16.306253
30.770642	1559.371068	16.311271
30.505744	1568.971854	16.316288
30.541364	1573.973774	16.321306
31.083518	1583.066471	16.326323
30.633527	1581.356816	16.331341
30.784928	1572.308614	16.336359
30.693449	1579.750308	16.341376
30.752279	1575.309817	16.346394
31.103755	1582.194017	16.351411
30.668363	1582.650994	16.356429
30.552177	1569.688002	16.361447
30.755405	1585.970297	16.366464
30.718191	1581.653764	16.371482
30.866303	1579.346626	16.376499
30.450049	1570.140606	16.381517
30.935645	1580.564008	16.386535
30.842387	1598.848939	16.391552
30.501926	1609.656932	16.396570
31.066173	1610.359887	16.401587
30.856698	1605.809073	16.406605
30.840067	1607.054584	16.411623
30.649432	1606.713214	16.416640
30.498354	1622.330229	16.421658
31.135859	1632.189765	16.426675
31.116984	1639.071732	16.431693
31.374375	1635.921740	16.436711
31.337618	1637.624299	16.441728
31.080236	1631.841787	16.446746
31.494967	1631.402136	16.451763
31.361405	1633.900907	16.456781
31.637425	1629.208178	16.461799
31.619923	1631.934716	16.466816
31.565857	1634.616336	16.471834
31.671863	1625.965301	16.476851
31.416488	1634.556507	16.481869
31.671240	1625.818544	16.486887
31.966463	1627.023187	16.491904
31.732182	1629.377791	16.496922
31.850089	1620.270730	16.501939
31.810591	1629.320251	16.506957
31.771277	1626.109309	16.511975
32.189157	1635.601339	16.516992
32.119900	1629.983052	16.522010
31.858717	1626.122671	16.527027
31.767017	1631.341737	16.532045
31.975057	1624.676977	16.537063
32.014673	1622.506557	16.542080
31.873135	1624.625943	16.547098
32.008498	1627.417620	16.552115
31.753394	1634.478292	16.557133
32.087471	1620.913590	16.562151
31.929935	1630.814940	16.567168
31.872088	1625.804610	16.572186
31.932536	1622.588376	16.577203
32.098220	1623.537245	16.582221
31.947362	1625.878332	16.587239
32.335748	1625.733782	16.592256
32.061015	1636.811265	16.597274
32.254125	1630.078188	16.602291
32.056720	1635.678806	16.607309
32.136721	1644.539324	16.612327
32.517953	1654.115611	16.617344
32.558485	1661.263419	16.622362
33.170250	1655.489378	16.627379
32.595662	1642.031234	16.632397
32.834054	1631.401764	16.637415
32.706307	1629.241926	16.642432
32.266271	1628.581464	16.647450
32.411006	1625.480714	16.652467
32.352170	1633.632665	16.657485
32.249921	1623.678603	16.662503
32.546148	1635.505924	16.667520
32.581071	1646.198788	16.672538
32.931949	1648.561741	16.677555
32.686018	1654.984951	16.682573
32.645739	1654.672137	16.687591
32.760545	1652.660495	16.692608
32.470982	1655.369108	16.697626
32.639118	1652.444676	16.702643
32.686112	1659.867391	16.707661
32.658236	1657.059252	16.712679
32.704975	1655.921189	16.717696
32.673632	1661.243709	16.722714
32.945482	1677.252493	16.727731
33.064859	1689.725602	16.732749
33.080230	1691.056195	16.737767
33.420602	1676.904076	16.742784
33.244335	1680.193732	16.747802
33.645312	1678.712616	16.752819
33.183553	1673.572287	16.757837
33.269219	1666.819817	16.762855
33.378623	1665.963563	16.767872
33.245310	1679.267088	16.772890
33.738345	1669.323544	16.777907
33.347081	1662.827277	16.782925
33.130996	1649.112755	16.787943
33.436664	1655.746151	16.792960
33.356900	1664.290727	16.797978
33.490465	1674.120931	16.802995
33.984482	1684.420899	16.808013
34.162062	1664.792127	16.813031
34.006376	1654.312106	16.818048
33.791643	1658.680522	16.823066
33.758853	1648.460176	16.828083
33.872052	1644.728929	16.833101
33.955205	1645.460822	16.838119
34.006842	1645.049168	16.843136
33.636194	1640.071596	16.848154
33.600016	1639.936052	16.853171
33.541666	1640.320116	16.858189
33.730011	1640.170883	16.863207
33.678862	1641.947965	16.868224
33.513933	1641.799846	16.873242
33.766601	1642.615680	16.878259
33.807888	1652.134095	16.883277
34.237339	1659.920813	16.888295
33.942032	1655.031118	16.893312
34.161031	1674.585585	16.898330
33.976926	1651.082562	16.903347
34.084047	1659.758104	16.908365
34.252306	1674.703027	16.913383
34.575742	1674.870435	16.918400
34.088222	1661.623749	16.923418
34.141749	1661.544880	16.928435
33.836593	1674.294332	16.933453
33.763174	1666.673759	16.938471
34.098666	1682.286159	16.943488
33.788445	1684.495111	16.948506
34.113168	1668.330883	16.953523
34.457736	1686.171121	16.958541
34.227578	1696.813789	16.963559
34.288465	1693.253724	16.968576
33.915057	1699.964981	16.973594
33.924368	1696.417696	16.978611
34.323357	1702.425198	16.983629
34.337043	1695.763412	16.988647
34.602515	1718.884401	16.993664
34.789191	1729.414279	16.998682
34.732118	1729.460685	17.003699
34.596376	1735.099196	17.008717
34.432069	1726.496813	17.013735
34.629621	1730.612650	17.018752
34.501459	1739.945579	17.023770
34.960841	1729.867200	17.028787
34.842766	1723.437467	17.033805
34.513440	1727.267609	17.038823
35.063036	1728.619221	17.043840
34.894098	1735.980952	17.048858
34.995623	1737.316070	17.053875
34.945923	1744.246681	17.058893
35.016607	1747.733015	17.063911
35.393413	1753.641572	17.068928
35.234803	1755.419767	17.073946
35.368796	1755.336945	17.078963
35.497311	1735.592073	17.083981
35.127533	1735.841717	17.088999
35.351240	1724.778035	17.094016
34.985508	1732.638127	17.099034
35.226024	1747.076182	17.104051
35.482267	1737.686642	17.109069
35.210652	1746.587817	17.114087
35.549224	1748.591829	17.119104
35.315462	1765.011446	17.124122
35.314098	1757.506443	17.129139
35.686942	1758.393027	17.134157
35.729609	1758.950349	17.139175
35.474428	1756.693430	17.144192
35.761788	1770.939990	17.149210
35.405204	1758.068065	17.154227
35.757566	1758.032459	17.159245
35.775336	1750.936039	17.164263
35.848694	1753.086716	17.169280
35.683709	1763.244969	17.174298
35.803922	1755.601391	17.179315
36.000892	1758.365991	17.184333
35.629573	1763.983084	17.189351
36.453503	1754.252472	17.194368
35.842290	1761.436863	17.199386
35.773334	1761.752268	17.204403
35.502736	1761.124961	17.209421
35.737635	1787.268981	17.214439
36.355799	1780.925224	17.219456
36.295394	1783.623313	17.224474
36.386968	1782.301549	17.229491
36.631818	1779.950232	17.234509
36.565712	1774.028561	17.239527
36.422445	1769.975070	17.244544
36.552281	1772.038498	17.249562
36.417614	1759.427379	17.254579
36.466752	1749.223238	17.259597
36.626800	1746.414756	17.264615
36.568179	1737.461924	17.269632
36.223148	1744.312053	17.274650
36.477408	1760.297557	17.279667
36.856765	1758.829591	17.284685
36.720166	1778.067552	17.289703
36.939769	1765.075963	17.294720
36.980889	1747.206916	17.299738
36.595691	1738.379376	17.304755
36.804009	1739.129975	17.309773
36.886062	1739.932148	17.314791
36.852084	1735.822916	17.319808
36.939589	1740.667551	17.324826
36.918907	1737.186430	17.329843
37.092045	1733.559466	17.334861
36.742580	1737.058772	17.339879
37.228225	1734.653184	17.344896
36.866266	1739.187038	17.349914
36.732204	1735.406421	17.354931
36.813554	1752.933162	17.359949
36.390172	1767.286614	17.364967
36.910900	1766.688219	17.369984
37.008491	1775.745033	17.375002
36.765950	1777.980587	17.380019
37.110012	1776.145004	17.385037
36.940324	1772.494910	17.390055
37.244491	1780.615412	17.395072
37.224338	1798.221425	17.400090
37.157793	1802.073074	17.405107
37.272350	1800.921798	17.410125
37.123366	1802.653854	17.415143
37.765226	1799.880486	17.420160
37.457969	1799.665024	17.425178
37.377266	1801.639341	17.430195
37.364790	1802.981017	17.435213
37.542624	1801.506255	17.440231
37.951033	1800.124261	17.445248
37.392287	1807.538290	17.450266
37.455553	1805.648471	17.455283
37.459783	1799.572981	17.460301
37.545653	1819.838729	17.465319
38.113802	1817.540652	17.470336
38.280963	1825.687030	17.475354
37.984970	1807.606388	17.480371
37.918805	1805.128843	17.485389
37.614471	1821.576763	17.490407
38.205573	1818.854619	17.495424
38.250139	1828.521418	17.500442
38.385798	1827.675222	17.505459
38.361133	1811.372694	17.510477
38.272077	1800.598045	17.515495
38.478447	1792.479384	17.520512
38.377311	1796.650387	17.525530
38.145182	1799.886645	17.530547
38.206782	1795.567286	17.535565
38.023723	1801.150146	17.540583
38.033007	1803.236610	17.545600
38.480117	1826.146278	17.550618
38.282571	1832.427783	17.555635
38.736600	1822.325456	17.560653
38.391760	1828.399901	17.565671
38.522239	1820.223362	17.570688
38.806849	1828.418905	17.575706
38.682340	1824.862247	17.580723
38.481230	1826.956436	17.585741
38.172016	1826.508997	17.590759
38.019165	1824.671192	17.595776
38.445048	1827.015013	17.600794
38.553751	1846.719332	17.605811
38.806232	1848.627867	17.610829
38.896970	1861.997476	17.615847
38.957671	1855.366936	17.620864
39.137008	1856.570993	17.625882
38.769875	1860.150529	17.630899
38.951712	1853.413384	17.635917
39.212345	1854.795258	17.640935
38.999904	1862.073944	17.645952
39.074543	1851.900014	17.650970
39.044965	1853.107208	17.655987
39.165158	1851.089892	17.661005
38.878051	1857.730113	17.666023
38.757254	1847.271150	17.671040
39.366737	1848.822376	17.676058
39.095181	1845.961875	17.681075
39.325925	1847.092542	17.686093
39.414090	1850.779077	17.691111
39.431641	1848.808892	17.696128
39.510653	1867.960777	17.701146
39.456101	1883.839885	17.706163
39.869478	1880.051211	17.711181
39.620696	1882.788308	17.716199
39.789399	1885.566439	17.721216
39.418163	1870.114711	17.726234
39.750539	1887.908840	17.731251
40.065752	1881.857174	17.736269
39.952997	1895.162475	17.741287
40.018800	1879.523193	17.746304
40.139464	1867.523806	17.751322
39.584010	1864.027244	17.756339
39.765018	1859.026287	17.761357
39.732642	1874.859452	17.766375
39.756551	1885.146836	17.771392
39.856946	1885.163487	17.776410
39.902001	1896.645832	17.781427
40.001993	1887.045954	17.786445
40.097286	1894.474281	17.791463
40.133291	1888.030663	17.796480
40.359506	1885.959333	17.801498
40.058673	1892.942124	17.806515
40.240868	1886.621886	17.811533
40.032472	1890.804610	17.816551
40.297679	1903.316282	17.821568
40.585903	1909.396012	17.826586
40.557902	1927.229135	17.831603
40.741165	1919.292740	17.836621
40.413837	1915.445202	17.841639
40.808032	1922.187959	17.846656
40.983740	1897.735750	17.851674
40.452292	1887.581843	17.856691
40.873831	1887.569028	17.861709
40.486850	1884.783829	17.866727
40.394981	1900.638640	17.871744
40.853391	1908.355549	17.876762
40.705171	1920.907405	17.881779
40.637380	1918.176544	17.886797
40.612737	1912.066585	17.891815
41.069173	1919.898814	17.896832
41.148226	1913.104452	17.901850
40.618539	1914.184769	17.906867
41.156617	1909.208020	17.911885
41.200162	1912.113928	17.916903
41.177466	1908.806759	17.921920
41.377790	1907.456889	17.926938
41.262620	1909.240646	17.931955
41.206009	1908.744776	17.936973
40.817267	1917.734642	17.941991
41.084614	1910.867048	17.947008
40.985513	1916.906088	17.952026
40.838571	1922.729288	17.957043
41.885198	1931.462827	17.962061
41.515757	1946.040296	17.967079
41.614609	1946.959300	17.972096
41.938704	1942.953998	17.977114
41.497654	1939.477179	17.982131
42.032780	1930.989441	17.987149
42.021563	1934.098469	17.992167
41.781110	1907.753951	17.997184
41.813358	1904.606282	18.002202
41.563807	1907.067101	18.007219
41.813155	1920.442248	18.012237
41.768009	1925.264402	18.017255
41.886556	1935.489917	18.022272
42.258799	1934.272401	18.027290
41.878656	1936.621345	18.032307
42.148459	1933.545948	18.037325
42.189664	1929.770278	18.042343
41.920102	1934.587204	18.047360
42.005103	1924.534302	18.052378
42.331394	1933.021218	18.057395
42.422349	1932.164175	18.062413
42.529009	1928.762373	18.067431
42.424003	1934.001539	18.072448
42.687733	1925.585929	18.077466
42.301806	1941.651455	18.082483
42.175291	1934.418251	18.087501
42.311434	1939.716087	18.092519
42.358159	1939.719890	18.097536
42.546401	1934.469605	18.102554
42.466308	1929.284227	18.107571
42.498128	1931.579864	18.112589
42.408261	1934.652370	18.117607
42.316467	1934.732685	18.122624
42.531367	1932.231737	18.127642
42.527539	1954.824368	18.132659
42.737927	1951.971388	18.137677
43.173953	1964.370346	18.142695
42.977680	1965.838837	18.147712
43.089802	1963.111378	18.152730
43.117472	1972.813056	18.157747
42.820671	1962.652338	18.162765
42.932548	1962.852085	18.167783
42.751381	1966.999842	18.172800
42.839059	1958.004475	18.177818
42.343723	1967.109114	18.182835
42.708268	1959.501903	18.187853
42.856932	1988.170829	18.192871
42.963813	1991.946327	18.197888
43.045383	1993.962934	18.202906
42.828464	1993.637873	18.207923
42.837546	2003.220300	18.212941
43.152867	2000.048491	18.217959
43.152543	2017.811215	18.222976
43.845021	2013.000507	18.227994
43.680194	2016.995061	18.233011
44.227391	2013.558267	18.238029
44.153915	2025.031103	18.243047
44.140096	1999.803244	18.248064
44.410782	1980.853091	18.253082
44.122373	1984.500665	18.258099
44.019190	1977.867459	18.263117
44.226477	1974.761822	18.268135
43.967219	1979.620702	18.273152
44.102933	1971.507369	18.278170
44.087308	1973.145309	18.283187
43.975127	1968.799784	18.288205
44.221729	1974.356290	18.293223
43.927196	1984.725899	18.298240
44.240621	1977.080193	18.303258
44.233352	1978.521005	18.308275
44.185486	1975.318151	18.313293
44.271697	1968.706815	18.318311
44.378517	1978.967445	18.323328
44.293503	1978.360285	18.328346
44.207860	1976.629853	18.333363
44.181271	1972.667344	18.338381
44.117450	1979.419747	18.343399
44.165945	1994.160676	18.348416
44.585242	1994.042719	18.353434
44.618552	2007.023425	18.358451
44.698133	2012.855465	18.363469
44.869101	2003.578826	18.368487
44.585557	2012.477865	18.373504
44.698092	2004.970540	18.378522
44.335103	2006.727496	18.383539
44.684167	2000.211257	18.388557
44.690778	2004.909191	18.393575
44.676852	2010.523372	18.398592
44.985669	2029.676218	18.403610
44.550865	2035.739785	18.408627
44.884001	2032.744074	18.413645
45.337606	2028.584244	18.418663
45.176878	2033.717233	18.423680
45.541028	2028.155615	18.428698
45.211795	2030.057989	18.433715
45.220589	2026.335102	18.438733
45.549328	2025.369955	18.443751
45.403261	2031.938423	18.448768
45.663437	2025.241324	18.453786
45.383491	2032.839971	18.458803
45.704901	2031.155508	18.463821
45.903909	2023.658548	18.468839
45.866871	2032.493284	18.473856
45.615920	2033.071031	18.478874
45.750766	2031.548887	18.483891
45.653389	2027.941855	18.488909
45.875731	2035.424855	18.493927
45.542237	2036.751108	18.498944
45.742908	2025.135969	18.503962
45.831576	2029.024457	18.508979
45.562873	2024.061963	18.513997
45.821998	2026.148540	18.519015
45.825748	2028.311189	18.524032
45.887063	2027.462767	18.529050
45.634048	2035.163113	18.534067
45.859274	2056.812558	18.539085
46.055693	2057.554189	18.544103
45.713217	2065.138373	18.549120
45.911587	2057.169393	18.554138
46.114508	2061.801005	18.559155
45.884356	2063.463135	18.564173
46.179926	2077.441995	18.569191
46.558022	2091.980421	18.574208
46.466993	2092.336236	18.579226
46.581841	2092.351985	18.584243
46.411221	2097.291387	18.589261
46.994667	2087.520690	18.594279
46.762931	2097.012948	18.599296
46.949102	2092.030720	18.604314
46.889187	2081.197724	18.609331
46.983924	2092.349996	18.614349
46.966194	2094.938444	18.619367
47.133203	2099.975101	18.624384
47.186203	2088.556518	18.629402
46.775676	2091.705295	18.634419
47.049876	2094.282280	18.639437
46.874756	2086.065072	18.644455
47.207007	2097.041566	18.649472
47.020354	2092.555604	18.654490
47.061003	2090.742868	18.659507
46.793055	2096.139177	18.664525
47.085436	2089.225869	18.669543
46.971549	2087.302601	18.674560
47.224937	2102.877918	18.679578
47.148022	2107.414588	18.684595
47.110983	2109.219622	18.689613
47.338685	2115.614578	18.694631
47.183437	2117.716298	18.699648
47.432452	2112.272043	18.704666
47.741196	2114.604492	18.709683
47.422980	2119.781048	18.714701
47.298488	2124.338480	18.719719
47.742542	2133.700720	18.724736
47.929018	2137.206271	18.729754
48.314901	2139.631813	18.734771
48.069147	2139.200652	18.739789
48.349328	2136.394736	18.744807
48.113250	2121.463759	18.749824
48.343744	2106.692993	18.754842
48.030195	2104.957521	18.759859
48.201724	2104.104374	18.764877
48.197680	2095.704658	18.769895
47.933765	2108.250906	18.774912
48.276796	2116.958706	18.779930
48.250917	2122.308009	18.784947
48.557060	2129.540825	18.789965
48.456326	2131.337883	18.794983
48.143024	2133.861249	18.800000
48.675614	2139.952724	18.805018
48.973942	2132.342213	18.810035
48.710783	2129.519990	18.815053
48.920485	2125.799254	18.820071
48.776790	2132.124803	18.825088
48.771502	2129.604874	18.830106
49.082017	2127.978969	18.835123
48.840701	2123.699249	18.840141
49.282907	2124.203045	18.845159
48.830020	2131.283281	18.850176
48.954714	2121.975523	18.855194
49.059951	2115.622712	18.860211
48.762372	2126.441427	18.865229
49.056375	2124.586036	18.870247
49.046260	2120.270615	18.875264
48.945659	2128.736327	18.880282
49.000845	2128.067716	18.885299
48.676718	2128.294968	18.890317
48.857136	2139.862567	18.895335
49.315452	2152.869360	18.900352
49.131717	2148.433282	18.905370
49.339989	2151.834298	18.910387
49.466911	2158.807262	18.915405
49.312183	2151.008238	18.920423
49.301334	2156.115570	18.925440
49.225515	2150.841972	18.930458
49.683323	2164.779707	18.935475
49.925603	2178.814257	18.940493
50.016613	2178.838819	18.945511
49.737078	2184.845108	18.950528
49.820799	2184.887457	18.955546
50.238181	2182.418693	18.960563
50.049454	2182.988140	18.965581
50.322467	2178.582421	18.970599
50.458861	2178.075502	18.975616
50.502851	2168.645313	18.980634
50.314768	2162.167157	18.985651
50.165571	2158.450458	18.990669
50.495887	2153.992396	18.995687
50.447135	2151.171996	19.000704
50.178259	2144.543108	19.005722
50.533660	2154.170203	19.010739
50.442244	2169.810216	19.015757
50.343511	2176.562784	19.020775
50.522927	2181.501262	19.025792
50.346865	2176.463772	19.030810
50.422930	2167.491145	19.035827
50.031530	2182.874684	19.040845
50.412234	2173.019780	19.045863
50.253098	2176.853138	19.050880
50.513426	2199.497698	19.055898
50.926116	2203.342488	19.060915
50.820896	2209.376390	19.065933
50.844455	2208.850227	19.070951
51.000333	2214.776363	19.075968
50.557841	2213.449657	19.080986
51.017441	2205.183809	19.086003
50.958898	2225.826077	19.091021
51.001809	2227.618993	19.096039
51.377474	2230.515663	19.101056
51.256546	2242.132641	19.106074
51.546730	2235.682708	19.111091
51.381495	2246.357536	19.116109
51.483649	2235.729753	19.121127
51.818431	2236.174795	19.126144
51.735207	2240.519642	19.131162
51.715993	2241.682169	19.136179
51.554967	2236.071916	19.141197
51.738868	2228.625095	19.146215
51.952245	2233.564067	19.151232
51.762380	2228.502938	19.156250
52.163752	2228.886949	19.161267
51.899120	2230.204955	19.166285
51.563921	2225.307348	19.171303
51.736235	2228.545229	19.176320
51.842084	2225.581756	19.181338
52.022626	2223.383549	19.186355
51.863314	2243.939952	19.191373
52.048806	2250.061055	19.196391
52.344523	2264.155035	19.201408
52.106267	2261.942785	19.206426
52.516835	2258.940451	19.211443
52.035439	2259.185217	19.216461
52.387549	2261.022777	19.221479
52.594502	2257.319020	19.226496
52.511459	2259.472169	19.231514
52.431998	2257.956426	19.236531
52.458485	2259.226885	19.241549
52.680970	2255.640955	19.246567
53.013973	2269.331637	19.251584
52.746786	2278.354418	19.256602
53.275292	2276.752551	19.261619
53.026390	2262.704088	19.266637
53.250955	2249.576976	19.271655
53.490372	2244.147709	19.276672
53.059137	2246.528295	19.281690
53.320070	2244.773852	19.286707
53.134704	2245.199395	19.291725
53.055510	2244.875915	19.296743
53.424005	2235.313661	19.301760
53.026683	2241.281889	19.306778
53.164304	2244.991146	19.311795
53.412909	2249.930384	19.316813
53.573995	2256.439985	19.321831
53.567069	2272.221543	19.326848
53.673861	2275.501380	19.331866
53.701921	2276.785746	19.336883
53.608133	2273.646224	19.341901
53.676254	2276.233371	19.346919
54.394500	2275.750332	19.351936
53.913990	2277.362086	19.356954
54.030232	2274.794522	19.361971
53.770313	2279.353955	19.366989
53.718898	2275.292853	19.372007
53.864243	2273.533023	19.377024
53.544859	2276.466966	19.382042
53.806684	2263.774467	19.387059
53.861978	2274.929694	19.392077
53.923013	2283.620572	19.397095
54.395704	2300.276770	19.402112
54.386564	2305.828808	19.407130
54.808831	2301.409279	19.412147
54.276083	2308.339480	19.417165
54.307624	2300.514747	19.422183
54.623537	2301.432390	19.427200
54.535792	2307.672814	19.432218
54.955503	2293.702633	19.437235
54.756449	2301.760055	19.442253
54.596169	2300.768481	19.447271
55.010714	2286.156572	19.452288
54.394101	2303.021584	19.457306
54.599881	2289.913409	19.462323
54.842196	2291.124029	19.467341
54.777232	2294.806603	19.472359
55.106795	2301.410191	19.477376
55.425638	2322.179252	19.482394
55.162703	2321.399007	19.487411
55.315589	2319.721357	19.492429
55.446284	2329.932054	19.497447
55.546693	2325.946500	19.502464
55.099448	2327.329686	19.507482
55.523472	2323.446154	19.512499
55.348968	2328.823371	19.517517
55.152238	2332.081231	19.522535
55.335121	2326.341893	19.527552
55.406996	2325.799568	19.532570
55.608593	2325.583087	19.537587
55.652764	2322.592370	19.542605
55.328790	2322.568377	19.547623
55.444744	2327.309876	19.552640
55.855009	2347.149766	19.557658
56.065849	2337.564866	19.562675
55.998817	2350.132677	19.567693
55.846146	2347.038674	19.572711
56.272448	2351.851401	19.577728
56.076365	2353.968816	19.582746
56.319488	2348.523915	19.587763
56.821245	2344.161623	19.592781
56.315060	2339.120828	19.597799
56.534218	2349.212417	19.602816
56.589905	2352.743590	19.607834
56.744828	2339.511790	19.612851
56.744705	2348.821159	19.617869
56.543906	2349.132797	19.622887
56.536837	2342.280170	19.627904
56.581535	2353.192348	19.632922
56.610125	2350.158621	19.637939
56.714841	2342.525290	19.642957
56.680736	2346.272676	19.647975
56.935184	2352.433974	19.652992
56.840535	2357.468323	19.658010
57.072971	2371.092858	19.663027
57.272289	2374.652963	19.668045
57.258144	2380.277551	19.673063
57.228673	2380.041622	19.678080
56.959155	2390.508406	19.683098
56.802353	2383.923991	19.688115
57.469014	2390.347754	19.693133
57.268199	2387.166707	19.698151
57.342504	2381.346736	19.703168
57.060276	2383.904978	19.708186
57.222548	2383.029778	19.713203
57.627029	2394.541824	19.718221
57.738622	2408.129621	19.723239
58.096151	2394.742545	19.728256
57.958790	2404.564533	19.733274
58.349161	2396.229339	19.738291
58.712368	2395.333864	19.743309
58.300517	2380.471363	19.748327
58.259263	2369.482188	19.753344
58.184977	2362.678089	19.758362
57.980795	2356.766481	19.763379
58.109704	2361.857007	19.768397
58.064090	2358.753310	19.773415
58.770079	2360.409719	19.778432
58.135394	2358.292985	19.783450
58.754325	2366.088919	19.788467
58.778849	2363.942642	19.793485
58.315305	2367.636080	19.798503
58.423046	2365.329055	19.803520
58.649407	2384.965053	19.808538
58.336090	2385.086500	19.813555
58.553099	2384.695696	19.818573
58.205935	2395.668788	19.823591
58.543348	2389.910021	19.828608
58.574628	2394.625894	19.833626
58.340890	2405.210983	19.838643
58.883783	2420.670829	19.843661
58.707933	2421.690905	19.848679
58.652845	2422.712328	19.853696
58.707842	2425.691577	19.858714
59.280117	2431.472378	19.863731
59.318442	2452.681897	19.868749
59.355574	2461.954233	19.873767
59.633861	2454.535224	19.878784
59.429153	2459.646753	19.883802
59.289368	2456.999412	19.888819
60.022791	2452.891909	19.893837
59.863107	2459.459740	19.898855
59.996975	2451.924524	19.903872
59.595388	2455.862520	19.908890
59.805909	2448.685092	19.913907
59.421170	2453.623514	19.918925
59.509185	2454.678681	19.923943
60.065764	2445.731404	19.928960
59.688876	2452.837342	19.933978
59.476910	2451.046611	19.938995
59.806935	2474.703411	19.944013
59.695016	2481.449707	19.949031
59.896763	2486.767983	19.954048
60.371417	2477.144067	19.959066
60.555171	2480.799006	19.964083
60.370216	2472.760081	19.969101
60.708626	2483.233741	19.974119
60.603108	2471.652261	19.979136
60.500901	2476.948618	19.984154
60.490090	2482.636462	19.989171
61.151338	2480.184120	19.994189
61.124003	2486.937968	19.999207
61.106401	2490.449449	20.004224
61.234146	2477.331659	20.009242
61.075399	2472.569103	20.014259
60.899957	2464.338757	20.019277
60.973763	2471.900591	20.024295
61.444374	2482.628796	20.029312
61.463434	2486.364738	20.034330
61.566743	2484.862527	20.039347
61.802421	2478.085564	20.044365
61.748210	2468.507437	20.049383
61.575146	2460.348350	20.054400
61.477108	2462.042603	20.059418
61.449820	2466.327521	20.064435
61.582556	2456.354297	20.069453
61.550644	2465.087988	20.074471
61.985111	2470.337221	20.079488
61.923495	2478.051431	20.084506
61.354591	2482.040958	20.089523
61.471091	2476.692538	20.094541
61.541489	2477.432564	20.099559
61.641246	2473.002916	20.104576
61.522258	2477.834356	20.109594
61.810538	2490.916262	20.114611
61.994183	2501.131380	20.119629
61.940602	2509.616800	20.124647
62.257062	2506.051717	20.129664
62.579312	2506.658786	20.134682
61.895246	2508.546446	20.139699
62.077813	2514.161770	20.144717
62.347829	2519.280919	20.149735
62.470310	2536.194296	20.154752
62.535861	2540.922450	20.159770
62.475609	2541.936890	20.164787
62.785247	2537.363349	20.169805
62.675165	2541.804238	20.174823
62.834071	2535.649178	20.179840
63.003673	2535.182232	20.184858
62.967691	2540.014423	20.189875
62.767454	2533.550009	20.194893
63.492996	2552.435166	20.199911
63.535678	2549.465138	20.204928
64.094158	2540.693890	20.209946
63.388729	2519.806537	20.214963
63.839296	2505.941921	20.219981
63.727770	2513.368593	20.224999
63.870303	2508.530746	20.230016
63.948399	2503.840979	20.235034
63.840549	2512.569603	20.240051
63.816261	2497.126283	20.245069
63.984458	2511.254951	20.250087
63.938652	2509.557006	20.255104
63.902183	2509.055301	20.260122
64.054309	2509.978200	20.265139
64.025545	2504.832658	20.270157
63.725264	2508.837565	20.275175
63.821679	2506.436382	20.280192
64.203913	2507.254464	20.285210
64.181794	2535.349635	20.290227
64.197178	2532.989117	20.295245
64.024174	2535.761767	20.300263
64.174775	2541.232162	20.305280
64.614627	2539.769113	20.310298
64.133641	2543.975905	20.315315
64.605910	2540.062000	20.320333
64.807464	2549.835422	20.325351
64.777797	2546.856535	20.330368
64.674413	2559.045640	20.335386
64.832211	2575.506471	20.340403
64.866185	2557.285696	20.345421
64.913000	2567.870834	20.350439
64.926879	2571.786455	20.355456
64.643527	2579.226079	20.360474
64.675097	2576.152420	20.365491
65.559444	2566.503888	20.370509
65.217049	2575.024683	20.375527
65.097545	2578.397722	20.380544
65.399520	2586.560762	20.385562
65.412171	2590.738061	20.390579
65.634638	2596.315072	20.395597
65.595436	2599.952349	20.400615
65.724455	2592.579344	20.405632
66.006285	2594.030500	20.410650
65.608976	2593.542617	20.415667
65.841159	2588.394048	20.420685
65.832753	2594.911586	20.425703
65.689575	2592.282917	20.430720
66.187282	2586.428081	20.435738
65.831231	2594.863024	20.440755
66.276684	2590.833210	20.445773
66.161949	2595.130005	20.450791
66.501610	2607.403061	20.455808
66.258150	2622.475000	20.460826
66.489957	2626.365872	20.465843
66.607694	2620.906148	20.470861
66.462835	2629.773488	20.475879
66.789190	2624.651289	20.480896
67.154040	2617.140184	20.485914
66.794732	2631.145976	20.490931
66.866071	2622.792906	20.495949
66.810589	2622.329896	20.500967
66.594567	2631.306305	20.505984
67.196368	2627.710388	20.511002
66.942739	2622.549019	20.516019
67.264325	2617.943479	20.521037
67.163317	2621.415737	20.526055
66.814815	2633.751668	20.531072
67.240371	2637.180903	20.536090
67.461146	2648.999487	20.541107
67.409651	2657.038880	20.546125
67.376183	2652.947039	20.551143
67.355274	2653.957892	20.556160
67.524526	2652.749138	20.561178
67.241377	2652.203091	20.566195
67.253066	2666.628858	20.571213
67.484509	2675.069438	20.576231
67.186893	2686.214584	20.581248
67.913926	2682.731854	20.586266
67.917965	2695.005028	20.591283
68.033782	2709.076701	20.596301
68.633749	2711.622353	20.601319
67.971241	2713.251175	20.606336
68.178503	2710.546654	20.611354
68.428088	2712.756243	20.616371
68.636929	2707.499806	20.621389
68.459504	2705.616494	20.626407
68.196292	2713.695364	20.631424
68.836069	2706.583620	20.636442
69.039160	2708.763377	20.641459
68.801781	2702.949472	20.646477
68.844714	2699.442267	20.651495
68.782350	2693.903138	20.656512
69.108190	2699.637299	20.661530
68.779055	2708.833180	20.666547
69.234206	2707.381671	20.671565
68.868201	2712.509909	20.676583
69.227570	2725.455392	20.681600
69.489089	2723.967774	20.686618
69.533303	2725.072997	20.691635
69.654228	2723.575619	20.696653
69.620996	2724.079834	20.701671
69.699552	2719.975858	20.706688
69.902288	2713.584039	20.711706
69.501710	2719.155294	20.716723
69.755451	2715.549727	20.721741
69.867047	2717.000942	20.726759
69.699168	2716.634379	20.731776
70.291502	2716.369805	20.736794
70.110936	2715.726626	20.741811
70.157734	2717.870964	20.746829
69.974789	2719.394729	20.751847
69.878451	2720.264946	20.756864
70.368448	2725.311009	20.761882
69.997568	2741.657892	20.766899
70.242807	2736.392843	20.771917
70.714203	2748.529230	20.776935
70.578614	2758.367673	20.781952
70.704473	2750.194987	20.786970
70.349547	2753.235128	20.791987
70.704701	2757.549063	20.797005
71.132079	2748.003968	20.802023
70.768479	2754.596644	20.807040
70.962199	2750.520956	20.812058
70.738291	2758.652177	20.817075
71.258566	2773.283027	20.822093
70.963250	2775.500203	20.827111
71.056041	2785.627916	20.832128
71.712021	2777.316289	20.837146
71.259526	2782.274304	20.842163
71.460514	2783.808643	20.847181
71.523521	2781.209959	20.852199
71.499158	2784.257224	20.857216
71.949179	2778.921613	20.862234
71.438987	2779.084689	20.867251
71.662038	2802.326386	20.872269
72.000842	2804.727817	20.877287
71.855996	2809.093625	20.882304
72.258339	2807.438522	20.887322
72.091704	2817.648535	20.892339
71.997098	2806.782395	20.897357
72.124016	2804.838229	20.902375
72.270706	2811.611208	20.907392
72.650635	2799.328820	20.912410
72.600887	2800.884097	20.917427
72.537036	2800.473707	20.922445
72.510916	2799.949741	20.927463
72.673174	2808.386504	20.932480
72.884838	2793.907353	20.937498
72.777058	2796.927969	20.942515
73.022488	2798.252291	20.947533
72.831888	2797.145386	20.952551
73.065404	2798.142555	20.957568
73.169108	2804.202293	20.962586
73.227603	2818.830452	20.967603
73.098676	2828.959977	20.972621
73.329419	2830.002514	20.977639
73.249635	2836.312662	20.982656
73.703234	2827.322973	20.987674
73.619017	2830.759320	20.992691
73.471777	2827.402823	20.997709
73.495559	2819.351559	21.002727
73.872291	2831.096289	21.007744
73.221512	2823.871831	21.012762
73.628897	2830.564684	21.017779
73.666941	2827.753696	21.022797
73.499100	2840.747922	21.027815
73.806656	2859.656286	21.032832
73.658541	2858.743707	21.037850
74.436627	2862.973349	21.042867
74.416000	2860.359851	21.047885
74.694397	2857.923477	21.052903
74.545501	2860.910990	21.057920
74.604080	2860.548125	21.062938
74.325045	2855.988786	21.067955
73.911502	2866.324642	21.072973
74.600748	2875.228679	21.077991
74.386879	2881.567346	21.083008
74.640293	2879.747969	21.088026
74.794228	2875.547549	21.093043
74.947352	2880.727811	21.098061
75.211285	2894.775044	21.103079
74.818653	2908.424520	21.108096
75.468509	2907.016005	21.113114
74.760504	2919.045217	21.118131
74.741556	2912.129011	21.123149
75.384245	2911.990475	21.128167
75.239645	2914.539380	21.133184
75.720698	2930.764026	21.138202
75.328165	2943.941769	21.143219
75.472617	2944.682510	21.148237
75.763716	2941.862769	21.153255
75.353572	2947.841334	21.158272
75.685622	2943.387481	21.163290
75.674275	2958.356941	21.168307
75.715985	2972.207651	21.173325
76.200223	2972.580628	21.178343
75.908564	2973.398502	21.183360
76.420865	2972.966510	21.188378
76.503032	2970.109341	21.193395
76.620524	2974.940555	21.198413
76.577583	2968.256829	21.203431
76.183634	2966.955596	21.208448
76.927690	2983.608528	21.213466
76.930514	2985.895902	21.218483
76.736301	2999.527189	21.223501
77.242037	2999.456237	21.228519
76.976670	2996.874437	21.233536
76.782255	2998.185978	21.238554
77.142399	2997.517815	21.243571
77.150980	2995.558474	21.248589
77.498942	2993.529922	21.253607
77.191560	2996.591885	21.258624
76.952736	2992.630458	21.263642
77.282590	2990.867268	21.268659
77.139884	3007.327305	21.273677
77.323393	3016.017281	21.278695
77.367207	3024.442964	21.283712
77.795025	3023.365480	21.288730
77.552748	3025.593286	21.293747
77.781098	3021.639964	21.298765
77.912703	3029.382747	21.303783
78.090992	3048.380444	21.308800
78.548780	3041.532084	21.313818
78.654584	3046.014071	21.318835
78.503507	3046.227413	21.323853
78.619663	3046.531976	21.328871
78.599989	3048.705082	21.333888
78.554622	3042.980203	21.338906
78.502542	3044.389417	21.343923
78.434857	3049.625705	21.348941
78.613810	3035.653618	21.353959
78.558903	3046.299834	21.358976
78.449008	3049.164136	21.363994
78.905175	3055.642382	21.369011
79.160584	3072.384697	21.374029
79.156358	3076.885557	21.379047
79.351448	3069.949124	21.384064
79.675028	3079.138062	21.389082
79.283304	3068.861373	21.394099
79.674689	3073.288107	21.399117
79.573635	3064.992711	21.404135
79.687875	3076.991332	21.409152
79.568581	3067.403521	21.414170
79.957666	3068.763092	21.419187
79.882856	3074.724381	21.424205
79.985466	3074.138170	21.429223
79.876902	3074.824638	21.434240
80.164001	3089.903719	21.439258
80.536529	3089.981615	21.444275
80.317554	3101.807414	21.449293
80.488731	3089.391264	21.454311
80.428070	3099.645508	21.459328
80.137043	3099.815114	21.464346
80.390354	3094.488709	21.469363
79.975010	3102.575745	21.474381
80.276315	3088.939400	21.479399
80.414620	3102.515343	21.484416
80.692229	3121.426795	21.489434
80.869338	3128.152168	21.494451
80.600751	3135.714744	21.499469
80.888327	3131.854412	21.504487
81.012506	3123.840122	21.509504
81.195022	3125.410740	21.514522
81.285607	3127.063275	21.519539
81.474016	3146.875274	21.524557
81.630315	3154.606010	21.529575
81.766432	3149.442228	21.534592
81.860769	3149.884419	21.539610
82.101942	3147.610323	21.544627
81.820392	3152.754937	21.549645
81.890795	3148.386050	21.554663
81.827713	3153.037997	21.559680
82.064424	3151.290759	21.564698
82.368411	3143.504742	21.569715
82.189642	3155.942716	21.574733
82.140654	3144.993702	21.579751
82.294665	3146.122659	21.584768
82.055495	3149.547838	21.589786
82.486621	3161.535513	21.594803
81.946142	3172.537560	21.599821
82.291210	3180.823471	21.604839
82.301400	3184.896604	21.609856
82.485307	3173.333505	21.614874
83.071199	3191.688933	21.619891
83.079188	3210.604975	21.624909
83.181606	3206.796846	21.629927
82.850161	3202.349563	21.634944
82.631021	3199.558186	21.639962
82.781479	3205.111533	21.644979
82.705515	3221.449303	21.649997
83.362474	3229.624277	21.655015
83.008445	3227.748338	21.660032
83.162103	3244.916244	21.665050
83.742064	3253.562797	21.670067
83.422146	3264.892528	21.675085
83.724028	3263.976019	21.680103
83.773285	3269.433329	21.685120
83.716890	3273.222560	21.690138
84.223228	3270.832891	21.695155
84.335390	3294.456611	21.700173
84.531901	3287.612773	21.705191
84.992050	3293.037450	21.710208
84.827316	3289.479871	21.715226
85.176376	3263.116669	21.720243
84.971495	3256.777188	21.725261
85.060857	3262.682836	21.730279
85.188956	3253.209225	21.735296
85.295955	3257.325634	21.740314
85.111558	3243.443222	21.745331
85.110245	3246.566957	21.750349
85.162786	3239.376088	21.755367
85.235045	3242.904621	21.760384
85.172333	3249.072608	21.765402
85.523951	3241.849366	21.770419
85.438095	3245.684595	21.775437
85.311177	3252.596819	21.780455
85.591709	3259.421078	21.785472
85.310483	3275.253820	21.790490
85.853892	3274.241561	21.795507
85.514794	3288.575250	21.800525
85.561354	3283.414176	21.805543
86.120955	3280.725548	21.810560
85.691087	3283.627422	21.815578
85.787669	3289.141993	21.820595
85.695054	3307.693427	21.825613
85.722752	3304.578549	21.830631
86.269211	3304.382480	21.835648
86.603449	3325.733038	21.840666
86.747187	3322.934557	21.845683
86.614212	3327.674932	21.850701
86.795937	3332.530685	21.855719
87.129712	3325.335666	21.860736
87.181817	3323.761823	21.865754
87.344156	3319.470848	21.870771
87.229001	3322.144721	21.875789
87.196608	3321.691907	21.880807
87.340007	3317.329361	21.885824
87.606819	3314.258544	21.890842
87.900701	3321.638932	21.895859
87.996005	3323.499387	21.900877
87.922179	3316.456948	21.905895
88.025204	3317.965607	21.910912
87.478232	3320.238602	21.915930
87.737405	3318.353608	21.920947
87.696172	3327.618625	21.925965
87.711844	3331.697157	21.930983
87.889983	3341.988588	21.936000
88.024125	3354.369922	21.941018
88.433932	3348.336135	21.946035
88.081524	3351.181425	21.951053
88.226423	3356.853915	21.956071
88.309823	3367.000939	21.961088
88.041259	3383.942104	21.966106
88.326350	3373.636601	21.971123
88.275799	3380.715356	21.976141
88.262615	3401.824725	21.981159
88.314372	3410.047633	21.986176
88.730449	3418.809797	21.991194
89.120252	3423.748829	21.996211
89.347970	3441.396490	22.001229
89.166976	3439.931905	22.006247
89.324736	3437.948509	22.011264
89.208234	3434.508641	22.016282
89.816841	3437.184463	22.021299
89.780067	3428.503753	22.026317
89.447236	3433.489496	22.031335
89.986206	3439.383498	22.036352
90.150526	3440.406749	22.041370
90.310323	3424.789195	22.046387
90.302687	3433.336542	22.051405
89.704189	3439.984736	22.056423
89.915764	3457.956516	22.061440
89.833116	3462.682003	22.066458
90.415310	3465.421426	22.071475
90.603998	3472.360760	22.076493
90.890019	3461.610055	22.081511
90.959038	3461.262714	22.086528
90.775740	3467.442008	22.091546
90.748697	3474.546703	22.096563
91.310121	3488.460770	22.101581
90.930579	3500.123800	22.106599
90.875482	3494.750899	22.111616
91.175210	3496.317999	22.116634
91.237159	3499.810554	22.121651
91.241113	3500.546269	22.126669
91.191538	3491.921275	22.131687
91.593855	3504.760017	22.136704
91.643182	3528.974523	22.141722
91.903189	3522.318958	22.146739
91.785858	3523.329069	22.151757
92.170220	3525.494405	22.156775
92.113105	3516.624176	22.161792
91.769908	3524.843185	22.166810
91.979551	3527.045563	22.171827
92.450677	3541.602076	22.176845
92.251387	3547.235982	22.181863
92.647173	3550.475206	22.186880
92.382856	3562.409146	22.191898
92.390354	3553.779059	22.196915
92.656526	3553.448322	22.201933
92.679297	3564.194982	22.206951
92.977318	3570.112228	22.211968
92.823760	3580.778080	22.216986
93.138536	3578.413333	22.222003
93.133451	3581.815799	22.227021
93.070747	3589.726062	22.232039
93.303870	3581.609378	22.237056
93.084915	3606.329162	22.242074
93.205914	3612.257870	22.247091
93.356471	3607.925520	22.252109
93.065647	3626.295510	22.257127
93.597202	3633.851098	22.262144
93.780087	3642.874679	22.267162
93.750011	3638.269279	22.272179
94.109575	3638.214725	22.277197
94.116103	3641.444306	22.282215
94.315068	3651.040076	22.287232
94.426224	3667.887304	22.292250
94.730308	3657.271987	22.297267
94.867130	3662.724660	22.302285
94.654303	3676.877169	22.307303
94.700687	3667.670137	22.312320
94.685827	3669.100591	22.317338
94.712795	3665.656553	22.322355
94.878888	3663.362177	22.327373
94.771859	3679.130017	22.332391
95.125268	3693.677711	22.337408
95.312505	3697.229165	22.342426
95.185728	3701.040804	22.347443
95.606064	3694.744388	22.352461
95.450481	3706.237645	22.357479
95.916377	3698.043978	22.362496
95.561504	3706.519475	22.367514
95.615421	3706.677991	22.372531
96.268930	3720.795429	22.377549
95.782331	3736.247203	22.382567
96.589746	3736.154462	22.387584
96.088246	3732.785258	22.392602
96.431973	3730.678582	22.397619
96.654614	3728.862024	22.402637
96.758486	3733.891130	22.407655
96.615636	3734.402356	22.412672
96.444081	3734.608191	22.417690
96.471272	3734.982364	22.422707
96.841093	3746.887274	22.427725
96.870239	3755.649016	22.432743
96.880462	3753.440419	22.437760
97.006959	3754.719056	22.442778
97.100463	3752.920696	22.447795
97.321255	3773.246171	22.452813
96.702872	3793.203600	22.457831
97.202851	3788.998745	22.462848
97.289292	3795.503668	22.467866
97.601524	3809.793897	22.472883
97.886159	3808.673965	22.477901
97.336447	3815.050104	22.482919
97.909316	3817.092589	22.487936
98.018022	3824.229301	22.492954
98.018699	3840.481326	22.497971
98.571785	3840.853554	22.502989
98.717107	3840.944419	22.508007
98.854425	3833.502466	22.513024
98.707888	3842.472373	22.518042
98.699710	3842.250098	22.523059
99.292803	3845.467372	22.528077
98.952296	3834.882110	22.533095
98.921097	3836.931284	22.538112
98.854610	3844.176800	22.543130
99.258399	3864.563168	22.548147
99.492239	3862.407581	22.553165
99.560048	3867.254676	22.558183
99.609615	3860.580702	22.563200
100.058814	3851.968452	22.568218
100.085883	3841.817932	22.573235
100.603578	3838.759137	22.578253
100.137228	3831.664834	22.583271
100.531704	3807.024874	22.588288
100.899354	3806.729505	22.593306
100.286377	3801.211924	22.598323
100.796765	3791.801617	22.603341
100.540200	3806.998221	22.608359
100.888682	3795.782926	22.613376
100.979749	3803.753569	22.618394
100.681312	3796.714768	22.623411
100.686047	3796.747037	22.628429
100.980107	3802.294879	22.633447
100.999318	3798.296884	22.638464
100.744876	3798.446833	22.643482
100.635603	3817.768843	22.648499
101.364841	3820.435080	22.653517
100.991985	3830.723631	22.658535
101.067461	3827.950940	22.663552
101.669113	3843.946357	22.668570
101.123381	3861.377393	22.673587
101.571015	3859.457664	22.678605
101.925809	3858.823466	22.683623
102.204634	3855.488216	22.688640
102.275873	3854.021304	22.693658
102.119089	3860.770367	22.698675
102.202705	3856.855041	22.703693
102.345072	3871.338269	22.708711
102.575247	3874.901304	22.713728
102.471211	3876.696761	22.718746
102.740612	3883.645280	22.723763
102.890606	3876.502785	22.728781
103.058904	3884.945393	22.733799
102.910395	3881.555020	22.738816
103.067678	3883.029228	22.743834
103.032523	3876.847060	22.748851
103.088947	3874.649428	22.753869
103.149957	3896.353981	22.758887
103.083665	3903.300988	22.763904
103.492240	3900.149050	22.768922
103.624185	3909.164190	22.773939
103.742024	3908.704506	22.778957
103.546133	3918.918669	22.783975
103.803330	3921.343719	22.788992
104.031821	3929.378291	22.794010
103.883719	3935.758873	22.799027
104.208561	3925.365861	22.804045
104.187047	3941.353221	22.809063
104.265375	3958.877429	22.814080
104.564573	3965.441249	22.819098
104.544152	3968.104501	22.824115
104.781062	3972.495755	22.829133
104.710924	3967.526163	22.834151
105.243456	3967.583726	22.839168
104.943823	3975.293793	22.844186
104.863403	3990.698233	22.849203
105.357210	3994.921796	22.854221
104.917371	4003.107213	22.859239
104.615188	3991.502408	22.864256
105.156276	4011.204626	22.869274
105.533090	4026.131395	22.874291
105.629537	4026.114074	22.879309
106.002623	4033.263839	22.884327
106.034600	4028.146766	22.889344
106.019420	4025.744796	22.894362
105.842394	4042.859210	22.899379
106.207972	4049.395146	22.904397
106.055660	4067.747414	22.909415
106.127432	4066.433975	22.914432
106.438067	4066.063314	22.919450
106.317962	4089.486248	22.924467
106.696496	4087.104196	22.929485
106.872546	4097.393329	22.934503
106.587129	4093.470326	22.939520
106.658840	4097.204712	22.944538
106.644261	4113.874706	22.949555
106.846496	4122.373844	22.954573
106.759832	4125.817980	22.959591
106.994368	4145.801328	22.964608
107.652062	4150.608028	22.969626
107.573087	4152.471681	22.974643
107.840573	4157.698919	22.979661
108.098547	4179.418138	22.984679
108.083156	4175.736302	22.989696
108.115688	4166.102890	22.994714
108.116551	4178.717227	22.999731
108.171599	4177.647657	23.004749
108.473127	4183.090389	23.009767
108.217498	4197.489349	23.014784
108.842332	4202.537197	23.019802
108.445375	4205.679329	23.024819
108.961915	4210.163695	23.029837
108.486049	4216.812450	23.034855
108.522000	4223.099371	23.039872
109.067006	4231.609903	23.044890
109.287970	4240.350844	23.049907
109.178238	4247.253466	23.054925
109.904613	4249.836783	23.059943
110.242680	4263.062856	23.064960
110.408086	4255.278000	23.069978
110.411581	4260.547380	23.074995
110.548266	4246.405044	23.080013
110.481377	4238.107898	23.085031
110.333093	4227.971440	23.090048
110.969949	4229.522565	23.095066
110.466617	4225.347043	23.100083
110.583048	4243.651079	23.105101
110.751598	4260.035430	23.110119
110.320294	4259.903016	23.115136
110.739628	4257.739992	23.120154
110.381915	4256.084304	23.125171
111.081451	4258.258721	23.130189
111.169429	4285.305563	23.135207
111.150235	4287.865480	23.140224
111.556106	4289.479052	23.145242
111.220140	4294.833418	23.150259
111.003426	4289.268994	23.155277
111.429583	4302.027115	23.160295
111.529336	4311.713546	23.165312
111.381910	4322.015750	23.170330
111.510575	4328.178127	23.175347
111.777869	4334.985434	23.180365
111.674876	4353.734417	23.185383
111.645490	4356.391395	23.190400
112.155537	4372.327442	23.195418
112.127182	4392.605063	23.200435
112.361202	4387.324853	23.205453
112.292728	4392.777531	23.210471
112.259040	4402.590861	23.215488
112.970529	4411.124933	23.220506
112.948127	4416.947782	23.225523
113.231519	4436.452120	23.230541
113.204141	4440.862035	23.235559
113.360932	4442.778242	23.240576
113.860972	4432.801452	23.245594
113.807771	4446.922557	23.250611
113.725571	4441.519323	23.255629
114.169770	4431.588338	23.260647
113.896023	4447.049993	23.265664
114.459264	4456.891769	23.270682
114.404636	4473.974638	23.275699
114.683569	4464.273598	23.280717
115.138475	4463.379626	23.285735
114.746374	4473.528541	23.290752
114.817883	4465.906180	23.295770
115.067917	4465.142633	23.300787
115.195806	4467.211086	23.305805
114.959610	4465.738538	23.310823
114.480754	4462.026610	23.315840
114.940920	4486.252488	23.320858
114.918053	4502.050039	23.325875
115.177075	4495.183151	23.330893
115.484919	4490.754285	23.335911
115.152060	4523.681690	23.340928
115.756757	4522.991236	23.345946
116.101151	4524.250698	23.350963
115.839020	4531.380417	23.355981
115.911661	4541.066123	23.360999
116.033578	4554.742218	23.366016
116.255148	4551.868744	23.371034
116.130722	4559.927120	23.376051
116.245955	4571.580149	23.381069
116.668623	4584.529705	23.386087
116.869096	4589.644130	23.391104
117.318188	4582.701299	23.396122
117.163056	4587.247363	23.401139
117.365778	4582.561608	23.406157
117.592340	4574.045424	23.411175
117.681967	4577.178248	23.416192
117.787388	4579.721575	23.421210
117.647465	4583.122955	23.426227
117.580001	4599.191319	23.431245
117.578437	4603.174679	23.436263
117.650941	4614.188413	23.441280
118.031520	4608.266283	23.446298
118.168939	4612.524334	23.451315
118.257522	4626.031349	23.456333
118.644352	4632.702510	23.461351
118.577811	4639.219043	23.466368
118.470640	4633.120600	23.471386
118.448247	4645.002851	23.476403
118.571481	4639.580085	23.481421
118.794333	4650.595637	23.486439
119.042190	4669.284844	23.491456
118.857682	4669.420446	23.496474
118.850906	4680.341485	23.501491
119.304989	4687.585571	23.506509
119.549333	4696.573227	23.511527
119.576519	4697.598806	23.516544
119.534401	4696.844377	23.521562
119.818631	4714.458570	23.526579
120.097025	4727.328221	23.531597
120.235763	4726.392345	23.536615
120.014232	4733.703441	23.541632
120.324433	4739.626131	23.546650
120.362610	4756.131802	23.551667
120.467343	4755.563284	23.556685
120.900902	4759.701293	23.561703
120.941071	4765.675011	23.566720
121.037073	4762.510329	23.571738
120.800191	4775.654240	23.576755
121.137960	4789.844887	23.581773
121.564612	4792.140204	23.586791
121.430434	4786.673300	23.591808
121.568879	4788.262671	23.596826
121.651542	4809.304714	23.601843
121.477210	4821.193453	23.606861
122.027951	4812.286028	23.611879
122.154870	4822.546249	23.616896
122.051032	4823.864462	23.621914
122.554397	4843.738807	23.626931
122.618058	4848.490033	23.631949
122.880624	4851.457001	23.636967
122.891375	4855.485572	23.641984
122.914108	4850.789636	23.647002
122.904468	4863.013280	23.652019
122.734630	4850.825922	23.657037
122.965690	4868.756586	23.662055
123.213729	4885.102753	23.667072
123.287063	4880.474536	23.672090
123.443027	4882.858806	23.677107
123.608953	4881.819016	23.682125
123.672247	4894.001037	23.687143
123.738815	4899.625288	23.692160
123.680692	4904.895206	23.697178
123.988845	4912.811077	23.702195
123.759318	4906.971376	23.707213
124.182280	4924.780201	23.712231
124.526783	4933.733493	23.717248
124.910209	4930.077630	23.722266
125.143598	4934.412258	23.727283
125.051322	4937.392814	23.732301
125.177135	4926.791461	23.737319
124.678976	4936.454752	23.742336
125.177047	4943.259780	23.747354
125.298684	4964.724620	23.752371
125.432154	4967.300221	23.757389
125.748228	4960.022436	23.762407
125.862308	4964.801286	23.767424
126.295596	4961.696104	23.772442
125.903108	4960.882791	23.777459
125.950704	4964.400185	23.782477
126.197585	4972.594393	23.787495
126.118454	4981.555750	23.792512
126.173997	4988.059373	23.797530
126.282611	5000.001348	23.802547
126.407651	5013.593024	23.807565
126.559392	5014.546073	23.812583
126.602938	5025.318519	23.817600
127.217350	5038.907452	23.822618
127.141985	5049.515988	23.827635
127.286762	5053.346771	23.832653
127.498286	5049.890486	23.837671
127.353037	5055.115528	23.842688
127.801290	5073.306138	23.847706
127.890655	5075.726271	23.852723
127.880862	5075.710623	23.857741
128.091144	5080.531303	23.862759
128.347728	5075.309224	23.867776
128.580047	5073.440447	23.872794
128.700057	5092.418301	23.877811
128.679633	5099.077560	23.882829
128.919773	5086.957577	23.887847
128.697645	5094.995954	23.892864
128.741267	5090.146711	23.897882
128.927820	5103.263986	23.902899
128.623735	5126.129241	23.907917
129.104755	5135.446776	23.912935
128.709128	5149.449983	23.917952
129.514177	5156.698707	23.922970
129.642657	5162.364424	23.927987
129.005668	5176.602798	23.933005
130.147872	5188.277929	23.938023
130.352187	5191.272276	23.943040
130.688102	5187.359055	23.948058
130.971169	5182.945275	23.953075
130.932132	5182.952756	23.958093
131.535832	5168.191562	23.963111
131.303150	5166.957795	23.968128
131.449846	5168.206306	23.973146
131.825065	5166.936065	23.978163
131.529819	5155.137023	23.983181
131.835888	5130.421164	23.988199
131.273092	5131.516406	23.993216
131.461466	5148.273207	23.998234
131.820303	5158.234747	24.003251
132.142806	5168.093035	24.008269
132.054991	5168.625588	24.013287
132.049759	5163.616137	24.018304
131.995433	5170.163088	24.023322
132.392446	5172.164231	24.028339
132.261060	5188.992433	24.033357
132.658626	5189.196812	24.038375
132.614307	5190.972726	24.043392
132.742730	5202.165536	24.048410
132.797271	5202.355467	24.053427
133.086177	5215.159125	24.058445
133.172998	5220.637450	24.063463
132.914936	5234.352491	24.068480
133.209508	5233.614358	24.073498
133.300969	5245.653978	24.078515
133.407251	5262.893638	24.083533
133.367104	5262.665008	24.088551
133.704525	5277.742284	24.093568
133.536026	5296.124738	24.098586
133.689291	5299.574469	24.103603
133.834384	5321.321696	24.108621
134.131990	5322.543560	24.113639
134.483558	5332.176420	24.118656
134.803317	5351.634693	24.123674
135.075640	5351.997601	24.128691
134.698348	5354.828601	24.133709
135.480975	5350.208620	24.138727
135.203495	5351.451883	24.143744
135.198532	5367.938805	24.148762
135.510943	5370.554687	24.153779
135.476605	5382.786903	24.158797
135.722631	5388.621592	24.163815
135.776935	5412.675076	24.168832
135.646874	5413.743412	24.173850
136.103660	5414.083364	24.178867
136.271008	5426.895428	24.183885
136.564808	5440.605836	24.188903
136.825941	5445.139071	24.193920
136.846939	5439.238109	24.198938
137.242599	5440.108409	24.203955
136.925161	5445.292206	24.208973
137.018927	5463.114749	24.213991
136.861789	5468.914609	24.219008
137.058093	5482.621287	24.224026
137.381771	5491.833676	24.229043
137.616887	5501.733147	24.234061
137.773528	5499.433829	24.239079
137.727164	5507.024021	24.244096
137.926308	5510.193394	24.249114
138.272450	5532.056891	24.254131
138.303596	5530.445463	24.259149
138.719963	5520.411451	24.264167
138.551478	5534.607635	24.269184
138.566635	5538.996383	24.274202
138.970453	5545.259362	24.279219
138.806801	5552.612110	24.284237
139.352738	5559.223306	24.289255
139.575589	5556.213164	24.294272
139.558940	5558.750007	24.299290
139.882971	5563.278795	24.304307
140.125825	5582.562278	24.309325
140.054985	5576.395017	24.314343
140.505994	5581.509349	24.319360
140.170946	5575.474814	24.324378
140.512851	5578.344037	24.329395
140.445471	5587.077653	24.334413
140.739406	5581.889179	24.339431
140.490757	5587.719736	24.344448
140.569839	5608.289263	24.349466
140.771638	5609.199897	24.354483
140.753316	5622.905681	24.359501
141.542211	5636.650326	24.364519
141.750537	5645.099615	24.369536
141.385873	5649.079317	24.374554
141.702631	5644.966834	24.379571
141.507914	5650.940192	24.384589
141.826240	5669.553909	24.389607
141.971355	5673.691986	24.394624
141.678627	5682.512335	24.399642
142.087987	5692.222153	24.404659
142.262955	5706.287932	24.409677
142.228101	5707.469147	24.414695
142.240560	5723.780158	24.419712
142.495083	5739.620395	24.424730
143.346008	5744.451183	24.429747
143.300611	5763.045442	24.434765
143.605071	5764.141711	24.439783
143.816169	5760.241873	24.444800
143.747552	5761.735295	24.449818
143.904596	5760.113289	24.454835
144.173633	5765.477069	24.459853
144.309582	5782.547578	24.464871
144.779339	5778.938953	24.469888
144.298905	5790.118398	24.474906
144.434802	5789.680774	24.479923
144.675923	5789.696942	24.484941
144.609259	5792.069103	24.489959
144.974700	5806.137764	24.494976
144.935142	5825.316354	24.499994
145.091362	5819.188843	24.505011
145.064261	5818.695665	24.510029
145.401274	5835.866459	24.515047
145.827012	5842.997783	24.520064
145.645627	5850.828691	24.525082
146.321294	5851.337511	24.530099
145.740191	5853.713585	24.535117
146.118811	5862.047150	24.540135
146.206586	5868.970180	24.545152
146.436906	5874.164189	24.550170
146.904079	5873.200302	24.555187
146.496386	5881.442603	24.560205
146.632518	5887.365634	24.565223
146.774891	5897.903537	24.570240
146.648579	5912.945122	24.575258
147.240693	5923.016817	24.580275
147.599328	5936.534580	24.585293
147.730056	5946.010321	24.590311
147.909598	5940.683801	24.595328
148.094863	5945.394816	24.600346
148.250303	5959.798942	24.605363
148.438309	5977.145885	24.610381
148.816925	5963.749833	24.615399
149.271150	5961.310424	24.620416
148.916478	5962.436993	24.625434
149.145098	5952.783850	24.630451
149.369068	5951.776579	24.635469
149.368351	5955.275693	24.640487
149.494452	5950.977622	24.645504
149.595459	5949.686588	24.650522
149.844420	5969.015181	24.655539
149.764497	5980.439606	24.660557
149.709958	5980.425326	24.665575
150.223797	5980.560950	24.670592
150.407989	5988.179590	24.675610
150.362800	5982.153499	24.680627
150.721636	5985.943088	24.685645
150.937496	5991.949378	24.690663
151.523737	5983.441679	24.695680
151.189578	5996.331511	24.700698
151.272855	5981.613885	24.705715
151.056246	5991.799844	24.710733
151.238295	5982.201141	24.715751
151.404988	5995.229609	24.720768
151.520135	6016.166855	24.725786
151.717593	6017.758050	24.730803
151.731686	6023.760343	24.735821
151.844277	6048.729567	24.740839
152.178236	6054.240646	24.745856
152.052426	6057.802188	24.750874
152.347847	6067.660955	24.755891
152.512111	6087.729694	24.760909
152.473295	6096.509894	24.765927
153.146983	6104.693752	24.770944
153.131238	6121.529109	24.775962
153.181783	6120.430249	24.780979
153.467497	6113.499802	24.785997
153.361261	6119.861476	24.791015
153.574818	6130.481856	24.796032
153.775330	6141.519605	24.801050
153.816461	6134.857939	24.806067
153.920932	6145.430861	24.811085
154.570151	6155.841087	24.816103
154.569935	6166.096402	24.821120
154.783798	6172.258283	24.826138
154.911478	6166.854717	24.831155
154.801357	6176.382124	24.836173
154.856597	6177.443951	24.841191
155.116200	6191.851699	24.846208
155.140166	6207.360124	24.851226
155.494675	6201.092133	24.856243
155.357048	6225.272697	24.861261
155.547697	6233.830098	24.866279
155.875067	6233.505367	24.871296
155.686723	6255.860860	24.876314
155.774379	6270.486421	24.881331
155.910891	6276.485941	24.886349
156.587845	6287.099457	24.891367
156.910310	6291.330965	24.896384
157.178171	6297.389111	24.901402
157.572387	6297.962740	24.906419
158.416028	6293.958278	24.911437
158.603997	6279.877816	24.916455
159.110288	6259.031414	24.921472
159.036827	6264.976336	24.926490
158.759970	6246.349301	24.931507
159.031771	6228.373416	24.936525
159.104214	6224.958839	24.941543
159.338503	6230.561111	24.946560
158.715536	6225.306687	24.951578
158.624779	6227.077286	24.956595
158.831847	6227.233206	24.961613
158.927784	6237.309814	24.966631
159.305827	6242.725177	24.971648
159.218637	6248.525144	24.976666
158.794013	6260.790279	24.981683
159.603656	6276.325569	24.986701
159.360153	6289.668790	24.991719
159.508718	6290.841449	24.996736
159.511432	6319.842593	25.001754
159.691658	6334.126226	25.006771
159.805770	6347.526350	25.011789
159.731218	6365.518185	25.016807
160.065364	6383.401380	25.021824
160.087016	6397.140363	25.026842
160.380629	6419.513507	25.031859
160.640106	6422.133914	25.036877
160.853765	6447.963968	25.041895
161.489133	6448.221346	25.046912
161.312824	6462.728485	25.051930
161.734590	6481.535746	25.056947
161.913995	6481.556195	25.061965
162.028654	6492.051191	25.066983
162.058315	6484.381473	25.072000
162.451397	6511.475116	25.077018
162.516903	6522.569357	25.082035
162.900921	6521.024164	25.087053
162.611832	6525.396807	25.092071
162.977611	6535.655001	25.097088
163.177634	6553.369960	25.102106
163.234186	6552.126673	25.107123
163.664205	6550.123795	25.112141
163.377024	6573.509702	25.117159
163.678760	6570.952189	25.122176
163.663147	6576.073579	25.127194
163.913556	6601.236670	25.132211
164.463004	6598.813142	25.137229
164.346969	6613.134419	25.142247
165.103691	6620.308612	25.147264
164.756611	6644.101911	25.152282
164.563188	6646.156411	25.157299
164.880153	6652.189734	25.162317
164.544725	6672.240886	25.167335
165.039553	6677.902636	25.172352
165.136833	6697.782751	25.177370
165.345735	6702.527752	25.182387
165.886976	6718.463971	25.187405
165.920987	6733.306328	25.192423
166.221197	6734.506592	25.197440
166.527944	6753.307895	25.202458
166.779644	6757.012054	25.207475
167.827749	6743.747938	25.212493
168.059359	6746.713483	25.217511
168.194689	6743.006003	25.222528
168.242704	6741.588498	25.227546
168.086776	6727.922656	25.232563
168.035700	6717.375646	25.237581
168.245761	6734.761384	25.242599
168.273233	6730.249203	25.247616
168.260222	6733.506395	25.252634
168.078507	6733.165731	25.257651
168.929604	6731.215900	25.262669
168.428926	6755.376788	25.267687
168.646588	6762.046343	25.272704
168.891103	6776.961365	25.277722
168.867200	6776.733867	25.282739
169.222519	6801.421608	25.287757
169.272833	6812.673055	25.292775
169.647059	6816.551586	25.297792
169.529216	6831.209737	25.302810
169.535497	6844.253793	25.307827
169.923676	6849.540800	25.312845
170.298521	6871.193253	25.317863
170.089012	6879.220119	25.322880
170.440937	6884.110811	25.327898
170.205909	6902.659341	25.332915
170.778330	6900.639887	25.337933
170.854914	6920.540370	25.342951
170.922983	6931.595857	25.347968
171.532203	6926.914573	25.352986
171.662910	6943.008046	25.358003
172.021377	6957.019841	25.363021
172.116517	6966.556645	25.368039
172.335728	6961.292310	25.373056
172.475526	6958.655362	25.378074
172.472826	6964.199262	25.383091
172.892180	6976.791343	25.388109
172.997674	6986.791948	25.393127
172.729241	6983.348991	25.398144
172.904074	6985.517651	25.403162
172.667490	7014.734382	25.408179
173.328973	7016.269769	25.413197
173.384993	7022.075400	25.418215
173.631197	7045.955866	25.423232
173.605696	7057.103104	25.428250
173.642276	7073.173455	25.433267
174.238234	7073.248542	25.438285
174.500581	7088.503474	25.443303
174.461325	7108.018350	25.448320
174.543544	7111.549978	25.453338
175.095975	7123.048792	25.458355
175.842125	7135.440817	25.463373
176.128771	7137.869987	25.468391
176.269657	7134.868877	25.473408
176.659500	7130.140851	25.478426
176.402196	7134.774474	25.483443
176.510483	7131.271632	25.488461
176.438696	7130.672635	25.493479
176.239108	7126.216597	25.498496
176.791442	7134.992138	25.503514
176.669467	7156.703360	25.508531
176.858191	7156.861649	25.513549
177.211933	7165.735847	25.518567
177.180842	7189.349743	25.523584
177.657831	7189.954911	25.528602
177.643334	7188.585896	25.533619
177.781675	7209.752335	25.538637
177.842660	7223.389177	25.543655
177.677204	7224.945024	25.548672
178.160084	7254.686406	25.553690
178.228740	7253.342519	25.558707
178.690839	7261.319832	25.563725
178.695332	7284.591391	25.568743
178.234776	7301.970600	25.573760
178.862256	7310.760141	25.578778
179.069747	7337.019661	25.583795
179.500629	7346.561373	25.588813
179.151513	7365.720825	25.593831
179.547545	7380.732542	25.598848
180.307656	7386.872944	25.603866
180.006263	7404.087118	25.608883
180.251893	7402.946064	25.613901
180.858103	7421.586531	25.618919
180.631479	7433.936783	25.623936
181.047197	7431.119325	25.628954
181.158979	7441.037995	25.633971
181.551646	7449.799329	25.638989
181.183160	7460.399839	25.644007
181.650602	7459.655613	25.649024
181.713415	7469.726071	25.654042
181.465205	7495.910352	25.659059
181.756447	7492.030234	25.664077
181.878416	7522.016745	25.669095
182.103849	7526.853693	25.674112
182.891137	7543.329157	25.679130
183.006602	7559.184012	25.684148
182.851664	7558.867886	25.689165
183.444948	7580.155349	25.694183
183.408624	7586.110938	25.699200
184.012238	7597.188521	25.704218
183.616413	7609.382782	25.709236
183.863819	7622.670529	25.714253
183.741898	7628.781033	25.719271
183.910361	7657.249636	25.724288
184.156307	7662.035842	25.729306
184.146427	7688.374164	25.734324
184.368806	7702.480844	25.739341
184.382433	7726.467579	25.744359
184.336594	7744.439495	25.749376
184.858385	7761.152129	25.754394
184.703755	7787.074262	25.759412
185.141176	7801.126046	25.764429
185.514887	7817.513554	25.769447
185.609352	7844.878077	25.774464
185.882044	7856.322173	25.779482
186.251876	7881.628304	25.784500
186.789656	7896.994351	25.789517
186.960763	7901.952594	25.794535
187.101664	7920.531602	25.799552
187.943131	7910.130173	25.804570
187.862311	7922.729172	25.809588
188.449424	7917.412490	25.814605
188.956438	7920.391707	25.819623
188.795624	7928.170467	25.824640
189.170385	7915.792084	25.829658
189.108077	7926.410529	25.834676
189.097145	7913.562556	25.839693
189.394592	7924.610132	25.844711
189.501311	7929.572330	25.849728
189.361905	7927.944205	25.854746
189.186282	7940.568923	25.859764
189.809119	7943.983641	25.864781
190.369330	7951.608879	25.869799
189.984613	7969.181421	25.874816
190.463616	7973.185658	25.879834
190.263780	7977.555995	25.884852
190.683330	7986.401250	25.889869
190.429732	7997.540184	25.894887
190.457551	8011.860107	25.899904
190.956869	8020.111881	25.904922
190.711905	8045.197506	25.909940
190.838773	8049.379508	25.914957
191.192375	8065.229492	25.919975
191.025780	8087.362431	25.924992
191.505599	8105.009873	25.930010
191.453011	8113.853412	25.935028
191.777395	8144.867570	25.940045
192.200891	8161.332768	25.945063
192.391759	8179.539540	25.950080
192.886243	8186.649109	25.955098
192.725562	8196.780393	25.960116
193.407482	8205.213671	25.965133
193.563451	8221.122898	25.970151
193.529191	8243.298754	25.975168
193.922771	8236.488353	25.980186
193.987782	8252.192613	25.985204
194.485617	8262.387528	25.990221
194.757129	8267.804515	25.995239
194.548248	8276.914432	26.000256
194.881379	8296.124267	26.005274
195.040541	8314.236574	26.010292
195.353798	8308.862717	26.015309
195.288753	8323.784975	26.020327
195.594623	8336.801735	26.025344
195.764772	8347.702830	26.030362
195.829998	8364.681073	26.035380
195.928497	8373.629634	26.040397
196.489576	8381.250202	26.045415
196.537656	8401.498535	26.050432
196.661719	8405.620448	26.055450
197.348447	8425.185797	26.060468
197.323341	8432.052080	26.065485
197.654699	8430.925411	26.070503
197.421739	8458.440856	26.075520
197.932996	8455.032521	26.080538
198.082356	8468.648180	26.085556
198.692114	8482.172325	26.090573
198.753447	8484.900311	26.095591
198.907383	8485.505765	26.100608
199.342991	8489.246558	26.105626
199.274711	8491.794291	26.110644
199.372772	8496.930683	26.115661
199.727893	8514.985203	26.120679
199.799896	8521.378723	26.125696
200.007799	8526.103956	26.130714
200.087792	8544.222214	26.135732
200.255306	8547.767112	26.140749
200.288153	8552.713016	26.145767
200.148777	8575.175999	26.150784
200.513286	8582.207183	26.155802
200.811696	8593.266084	26.160820
200.811893	8614.094861	26.165837
200.974147	8614.415273	26.170855
200.922167	8638.806956	26.175872
201.499825	8644.365401	26.180890
201.483007	8658.186970	26.185908
201.758476	8673.139419	26.190925
202.291495	8678.841824	26.195943
202.661233	8702.109548	26.200960
202.928241	8703.174636	26.205978
203.144605	8700.684213	26.210996
203.032874	8723.002427	26.216013
203.889554	8723.418099	26.221031
203.787430	8729.899062	26.226048
203.782887	8726.720111	26.231066
204.233766	8752.126383	26.236084
204.471114	8766.626142	26.241101
204.548273	8765.530419	26.246119
204.583165	8767.379025	26.251136
204.571475	8778.707079	26.256154
204.669279	8789.036294	26.261172
204.896619	8810.225037	26.266189
205.005762	8822.885930	26.271207
205.190960	8839.151591	26.276224
205.371335	8858.244895	26.281242
205.428077	8883.128049	26.286260
205.658363	8902.572109	26.291277
206.422487	8911.610135	26.296295
206.311753	8934.814015	26.301312
206.659139	8935.821222	26.306330
206.797713	8954.275766	26.311348
207.003027	8964.536241	26.316365
207.567068	8969.005958	26.321383
207.685299	8981.336094	26.326400
208.001461	8979.594317	26.331418
208.031671	9000.052882	26.336436
208.173177	9020.144163	26.341453
208.685321	9010.802217	26.346471
208.620659	9034.575053	26.351488
208.959040	9044.114729	26.356506
209.343277	9048.155180	26.361524
209.106050	9064.518690	26.366541
209.512863	9080.259710	26.371559
209.561051	9089.953153	26.376576
209.997317	9105.695452	26.381594
210.069590	9115.685745	26.386612
210.112195	9126.481597	26.391629
210.399997	9135.886606	26.396647
210.236296	9153.928354	26.401664
210.764935	9181.023757	26.406682
211.022110	9185.171113	26.411700
211.255042	9207.816969	26.416717
211.322684	9213.148680	26.421735
211.588119	9232.294028	26.426752
212.007530	9248.787829	26.431770
211.936666	9266.440340	26.436788
212.331040	9283.285130	26.441805
212.762541	9281.783547	26.446823
212.478593	9292.154886	26.451840
212.958088	9314.865778	26.456858
212.959697	9322.039855	26.461876
212.710027	9344.292753	26.466893
213.474903	9345.044061	26.471911
213.417590	9372.394650	26.476928
213.600146	9391.557543	26.481946
214.179217	9407.357597	26.486964
213.884880	9428.666514	26.491981
214.173806	9429.820865	26.496999
214.279013	9460.452824	26.502016
214.448518	9474.599273	26.507034
214.916846	9488.807966	26.512052
215.229451	9522.226675	26.517069
215.488009	9533.726389	26.522087
215.723064	9553.964601	26.527104
215.454317	9561.129975	26.532122
215.847989	9584.648568	26.537140
216.011252	9604.095507	26.542157
216.446442	9618.294238	26.547175
216.451648	9646.731308	26.552192
216.875934	9656.978326	26.557210
217.767792	9670.742699	26.562228
218.010987	9685.691377	26.567245
218.632458	9682.381296	26.572263
218.378705	9690.335197	26.577280
218.526260	9686.239672	26.582298
219.121947	9702.323959	26.587316
219.045496	9719.479975	26.592333
219.912112	9712.322356	26.597351
219.834629	9709.448811	26.602368
220.077229	9711.867020	26.607386
220.525315	9719.339778	26.612404
220.431566	9732.151193	26.617421
220.411196	9738.555514	26.622439
220.526079	9749.736490	26.627456
220.751906	9749.737176	26.632474
220.618847	9756.687132	26.637492
220.685855	9778.021236	26.642509
221.023355	9789.414630	26.647527
221.136338	9803.473357	26.652544
221.260718	9822.337879	26.657562
221.485152	9845.885862	26.662580
221.234772	9869.196958	26.667597
221.649646	9885.726856	26.672615
222.025967	9911.243858	26.677632
222.336252	9934.602340	26.682650
222.593038	9946.244474	26.687668
222.615476	9975.925628	26.692685
223.473612	9986.924212	26.697703
223.672638	9995.386850	26.702720
224.104635	10016.693372	26.707738
224.139413	10012.801467	26.712756
224.287278	10029.199214	26.717773
224.754207	10035.813224	26.722791
224.730931	10051.737646	26.727808
224.695383	10046.107059	26.732826
225.336357	10066.870415	26.737844
225.217914	10082.704025	26.742861
225.477840	10086.876356	26.747879
225.951270	10106.358979	26.752896
225.655676	10111.786341	26.757914
225.936312	10132.569000	26.762932
226.292394	10141.898285	26.767949
226.813660	10142.812734	26.772967
227.439676	10152.020115	26.777984
227.614942	10157.459755	26.783002
227.715971	10151.405462	26.788020
227.597251	10174.853586	26.793037
228.057110	10187.234815	26.798055
227.703701	10206.671764	26.803072
228.072522	10224.057699	26.808090
228.134879	10232.288603	26.813108
228.228228	10253.869375	26.818125
228.796670	10271.775836	26.823143
228.751077	10291.760517	26.828160
229.043493	10312.300285	26.833178
229.572919	10326.779744	26.838196
229.249422	10334.963379	26.843213
229.872344	10359.750176	26.848231
230.387828	10373.921626	26.853248
230.129418	10397.543720	26.858266
230.637012	10408.954095	26.863284
231.170188	10426.077273	26.868301
231.847430	10427.759232	26.873319
231.427853	10440.742093	26.878336
231.728259	10461.020665	26.883354
231.833286	10459.790833	26.888372
232.569672	10485.924639	26.893389
232.359962	10491.901561	26.898407
232.658064	10510.395145	26.903424
232.766121	10522.811720	26.908442
232.997871	10528.580614	26.913460
232.889386	10556.832328	26.918477
233.292784	10552.721098	26.923495
233.563903	10580.906211	26.928512
233.547638	10600.925641	26.933530
234.137015	10621.852990	26.938548
234.126692	10633.669049	26.943565
234.564539	10657.832464	26.948583
235.019299	10655.571934	26.953600
235.125205	10687.247740	26.958618
235.481844	10696.241588	26.963636
235.598202	10718.641640	26.968653
235.914970	10729.337985	26.973671
236.474689	10732.825594	26.978688
236.852700	10754.394482	26.983706
237.115138	10749.190066	26.988724
237.185745	10756.285188	26.993741
237.256311	10751.603758	26.998759
237.786788	10768.529201	27.003776
237.862384	10777.024437	27.008794
238.270389	10779.067762	27.013812
238.172352	10781.246680	27.018829
238.400808	10786.418971	27.023847
238.700141	10800.824832	27.028864
238.586296	10811.757359	27.033882
239.028956	10823.046783	27.038900
238.697508	10846.450391	27.043917
239.107426	10852.318084	27.048935
239.360078	10874.903007	27.053952
239.082456	10892.900023	27.058970
239.380626	10912.588582	27.063988
239.572024	10949.915594	27.069005
239.720490	10970.863813	27.074023
240.212303	10998.390916	27.079040
240.602786	11031.791506	27.084058
241.355973	11038.446691	27.089076
241.489335	11053.007297	27.094093
241.179565	11057.956748	27.099111
241.481693	11085.571669	27.104128
241.471106	11101.627320	27.109146
242.102802	11128.549154	27.114164
242.051180	11161.504162	27.119181
242.470529	11178.051949	27.124199
242.675596	11202.353782	27.129216
242.519453	11230.816551	27.134234
243.071528	11247.040656	27.139252
243.072250	11282.275184	27.144269
243.230694	11311.147494	27.149287
244.440715	11328.122516	27.154304
244.452128	11348.119207	27.159322
244.485831	11368.099495	27.164340
244.824602	11384.040383	27.169357
245.307692	11407.209042	27.174375
245.690775	11422.885494	27.179392
245.878079	11444.990713	27.184410
246.290322	11447.042855	27.189428
246.737205	11461.725017	27.194445
246.594807	11474.316052	27.199463
246.940270	11485.403541	27.204480
247.265267	11509.102172	27.209498
247.610311	11513.466734	27.214516
247.666822	11536.007396	27.219533
247.947450	11547.422808	27.224551
248.282498	11562.614353	27.229568
248.474452	11577.679148	27.234586
249.038625	11577.842480	27.239604
249.456397	11596.486991	27.244621
249.791531	11606.274589	27.249639
249.856812	11604.329694	27.254656
250.129493	11602.673898	27.259674
250.476306	11609.165734	27.264692
250.324848	11628.281354	27.269709
250.753937	11635.222431	27.274727
250.869230	11634.936333	27.279744
250.394036	11647.162184	27.284762
250.482579	11658.128353	27.289780
250.692904	11684.078466	27.294797
251.095893	11704.969818	27.299815
251.223038	11719.202706	27.304832
251.274250	11749.454238	27.309850
251.520228	11769.061372	27.314868
251.822203	11801.419654	27.319885
251.717716	11821.997840	27.324903
252.109748	11850.214856	27.329920
252.220038	11873.829468	27.334938
252.718663	11905.651509	27.339956
253.164712	11932.983157	27.344973
253.172271	11967.940616	27.349991
253.847724	11984.629718	27.355008
254.100580	12014.941738	27.360026
254.661690	12029.213984	27.365044
255.048808	12043.289122	27.370061
255.434524	12058.210828	27.375079
255.694877	12077.647236	27.380096
255.939978	12089.794082	27.385114
256.626607	12094.207421	27.390132
257.072299	12109.456160	27.395149
257.009689	12124.817255	27.400167
257.270901	12118.638642	27.405184
257.320438	12128.552731	27.410202
257.554264	12132.988533	27.415220
257.712407	12149.221173	27.420237
258.128257	12173.850807	27.425255
258.133019	12171.449718	27.430272
258.251074	12193.864112	27.435290
258.852551	12201.073751	27.440308
259.013370	12224.933949	27.445325
258.791124	12248.095469	27.450343
259.530559	12261.473693	27.455360
259.135278	12289.057315	27.460378
259.401040	12302.387527	27.465396
259.850066	12324.436468	27.470413
259.840399	12355.577405	27.475431
260.462090	12372.328130	27.480448
260.664669	12392.595930	27.485466
261.055202	12412.718065	27.490484
261.374134	12430.450608	27.495501
261.619946	12451.133449	27.500519
261.492877	12468.480699	27.505536
261.726976	12495.871683	27.510554
262.433541	12517.153334	27.515572
263.398405	12542.433317	27.520589
262.916747	12553.680642	27.525607
263.505335	12543.644314	27.530624
263.914563	12566.970703	27.535642
264.061626	12586.241160	27.540660
264.176471	12589.047348	27.545677
264.260650	12610.156838	27.550695
264.577961	12623.954447	27.555712
264.778664	12631.872855	27.560730
265.303008	12643.505735	27.565748
265.644089	12654.411949	27.570765
265.681373	12670.895928	27.575783
265.845653	12681.681161	27.580800
265.746389	12694.495844	27.585818
265.914947	12717.200174	27.590836
266.446909	12732.017051	27.595853
266.584682	12750.006370	27.600871
267.093574	12762.819311	27.605888
267.193621	12785.489772	27.610906
267.799151	12802.768544	27.615924
267.984685	12808.875571	27.620941
268.437766	12845.136030	27.625959
269.050354	12842.446258	27.630976
268.958412	12847.363635	27.635994
269.238604	12877.256480	27.641012
269.534077	12882.875018	27.646029
269.848844	12903.582862	27.651047
270.250409	12909.424366	27.656064
270.642722	12921.283392	27.661082
270.610374	12945.508727	27.666100
271.006075	12944.717478	27.671117
270.915498	12964.205633	27.676135
271.378609	12973.121027	27.681152
271.642963	12996.135576	27.686170
272.021642	13016.176952	27.691188
272.239637	13025.589880	27.696205
272.057842	13043.120486	27.701223
272.630278	13059.205789	27.706240
272.296897	13076.641053	27.711258
272.761133	13093.619673	27.716276
273.154145	13122.990850	27.721293
273.334597	13153.287441	27.726311
273.474674	13169.555710	27.731328
273.991383	13185.278726	27.736346
273.982764	13219.152528	27.741364
274.872200	13234.012613	27.746381
274.845541	13251.378151	27.751399
275.318389	13265.080293	27.756416
275.564680	13301.711343	27.761434
275.703994	13306.656993	27.766452
276.397230	13321.183549	27.771469
276.406839	13347.600983	27.776487
276.396091	13356.219535	27.781504
276.875398	13373.742780	27.786522
276.726768	13398.779931	27.791540
277.173937	13419.394807	27.796557
277.434854	13452.431669	27.801575
277.592898	13480.045383	27.806592
277.935188	13501.159061	27.811610
277.983896	13519.219653	27.816628
278.573117	13543.347211	27.821645
278.507742	13576.329917	27.826663
279.050481	13590.080246	27.831680
279.127630	13614.174313	27.836698
279.372788	13641.811194	27.841716
279.898577	13661.886462	27.846733
279.990709	13692.082546	27.851751
280.246438	13712.185250	27.856768
280.734911	13728.477894	27.861786
281.179538	13753.122308	27.866804
281.679342	13765.212556	27.871821
281.550049	13786.388516	27.876839
282.386124	13796.071077	27.881856
282.357917	13815.461282	27.886874
282.643303	13821.997630	27.891892
283.096648	13842.720735	27.896909
283.406432	13868.458659	27.901927
283.531625	13882.168891	27.906944
283.854192	13899.421665	27.911962
284.314220	13924.106253	27.916980
284.591051	13931.449542	27.921997
285.011016	13955.070813	27.927015
286.275617	13932.374478	27.932032
286.468067	13939.555701	27.937050
286.697711	13946.550867	27.942068
287.314035	13956.863836	27.947085
287.371905	13963.287923	27.952103
287.236687	13963.511277	27.957120
287.584406	13965.068851	27.962138
287.589318	13979.564233	27.967156
287.721710	13961.568247	27.972173
287.557490	13989.890593	27.977191
288.052884	14002.612250	27.982208
288.346432	14020.800079	27.987226
288.361219	14035.054235	27.992244
288.712840	14052.306919	27.997261
289.062911	14078.790114	28.002279
289.247812	14091.973294	28.007296
290.172526	14117.834760	28.012314
289.522602	14139.880628	28.017332
289.957669	14147.999183	28.022349
290.516420	14174.192994	28.027367
290.689596	14190.261150	28.032384
291.068477	14215.984622	28.037402
291.162444	14240.051502	28.042420
291.762921	14251.997182	28.047437
291.577969	14276.520161	28.052455
291.844146	14294.583734	28.057472
292.228095	14312.152698	28.062490
292.043924	14346.214949	28.067508
292.827029	14362.621652	28.072525
292.928542	14380.537004	28.077543
293.422490	14400.594990	28.082560
293.678697	14412.003978	28.087578
294.313503	14439.321640	28.092596
294.501411	14463.479928	28.097613
294.640736	14481.396790	28.102631
295.100275	14495.986513	28.107648
295.979932	14502.309365	28.112666
295.741415	14531.171836	28.117684
295.969917	14538.315617	28.122701
296.323922	14555.182239	28.127719
296.377045	14574.885678	28.132736
296.580119	14597.673380	28.137754
296.710867	14610.503718	28.142772
297.034303	14638.161954	28.147789
297.136609	14663.522126	28.152807
297.192331	14687.608822	28.157824
297.756373	14724.546382	28.162842
297.655674	14751.831421	28.167860
298.242425	14776.607482	28.172877
298.400192	14815.236857	28.177895
298.761188	14851.924198	28.182912
299.535320	14866.132465	28.187930
299.365462	14900.901149	28.192948
300.108213	14916.251335	28.197965
300.552416	14940.018033	28.202983
300.928842	14964.535660	28.208000
301.422461	14985.287979	28.213018
301.523153	15007.017189	28.218036
301.835226	15019.739528	28.223053
302.345401	15040.216381	28.228071
302.299331	15060.582102	28.233088
303.097835	15082.059400	28.238106
302.990780	15107.766665	28.243124
303.292512	15123.038155	28.248141
303.285794	15146.034386	28.253159
303.474454	15176.273383	28.258176
303.589435	15194.437940	28.263194
303.867852	15235.594928	28.268212
304.344118	15270.810082	28.273229
304.661255	15295.232748	28.278247
304.832498	15329.937562	28.283264
305.111356	15350.106078	28.288282
305.671046	15385.997607	28.293300
306.046545	15411.939477	28.298317
306.311422	15432.808803	28.303335
306.782726	15458.110098	28.308352
307.172529	15475.025119	28.313370
307.142908	15507.116491	28.318388
307.804450	15518.332241	28.323405
308.433272	15548.398743	28.328423
308.776746	15571.497905	28.333440
308.635725	15589.290617	28.338458
308.851879	15622.211805	28.343476
309.566450	15639.353497	28.348493
309.938420	15666.975182	28.353511
310.088119	15696.881313	28.358528
310.523438	15704.381088	28.363546
310.299890	15729.899625	28.368564
310.839409	15751.729573	28.373581
311.126022	15773.126835	28.378599
311.123477	15792.042045	28.383616
311.449404	15823.171408	28.388634
311.558633	15849.741278	28.393652
311.887110	15868.366537	28.398669
312.366788	15905.811442	28.403687
312.521917	15939.978019	28.408704
312.995659	15971.214741	28.413722
312.980767	16000.355132	28.418740
313.300337	16021.597308	28.423757
314.082502	16048.227138	28.428775
314.471158	16080.511182	28.433792
314.607279	16094.506701	28.438810
315.615552	16109.216615	28.443828
315.993289	16127.321394	28.448845
316.380607	16138.111648	28.453863
316.310123	16164.575676	28.458880
316.844856	16172.400704	28.463898
317.116200	16199.343752	28.468916
317.002714	16213.817239	28.473933
317.417347	16241.323795	28.478951
317.660952	16271.085598	28.483968
317.928270	16295.327528	28.488986
318.102744	16322.599508	28.494004
318.353885	16352.308143	28.499021
318.671601	16380.537774	28.504039
318.866536	16410.580889	28.509056
319.232750	16430.310111	28.514074
319.362416	16476.179218	28.519092
319.617936	16509.498979	28.524109
320.312043	16534.189908	28.529127
320.537342	16564.645850	28.534144
321.322523	16581.795336	28.539162
321.722657	16607.760073	28.544180
322.233444	16616.841111	28.549197
322.617063	16641.902279	28.554215
322.721248	16679.648172	28.559232
323.179042	16682.596491	28.564250
323.591492	16701.430571	28.569268
324.060542	16717.578158	28.574285
324.324665	16730.193372	28.579303
324.672735	16765.428937	28.584320
324.851658	16775.247968	28.589338
325.054041	16794.498082	28.594356
325.687186	16813.154159	28.599373
325.727328	16832.375371	28.604391
325.972203	16852.869980	28.609408
326.658558	16868.378261	28.614426
326.108620	16906.301411	28.619444
326.506959	16924.278986	28.624461
326.945743	16943.881297	28.629479
326.963313	16982.259119	28.634496
327.228045	17004.840919	28.639514
327.455563	17039.952688	28.644532
327.979708	17066.915294	28.649549
328.237058	17084.359130	28.654567
328.820254	17118.532003	28.659584
329.360191	17134.059321	28.664602
329.548331	17159.372325	28.669620
329.997037	17180.601731	28.674637
330.487754	17200.122925	28.679655
330.206799	17230.632165	28.684672
330.561733	17248.924947	28.689690
331.309255	17277.107656	28.694708
331.354699	17303.504745	28.699725
331.493363	17333.677402	28.704743
331.893597	17368.011417	28.709760
332.421654	17393.231834	28.714778
332.483851	17423.537574	28.719796
332.640291	17448.547451	28.724813
333.461680	17473.670421	28.729831
333.956221	17510.622934	28.734848
334.386586	17530.206882	28.739866
334.122409	17552.093383	28.744884
334.681702	17582.818703	28.749901
335.285249	17613.082454	28.754919
335.260933	17653.941000	28.759936
335.403498	17679.489624	28.764954
335.821962	17717.751549	28.769972
335.833679	17742.591177	28.774989
336.305490	17781.020677	28.780007
336.766161	17817.922917	28.785024
337.165987	17843.131306	28.790042
337.866060	17883.227754	28.795060
338.074948	17903.851214	28.800077
338.504119	17937.907116	28.805095
338.605105	17975.716387	28.810112
339.142541	17996.843335	28.815130
339.440652	18023.307037	28.820148
339.686483	18045.586048	28.825165
340.784342	18073.178753	28.830183
340.974487	18097.556343	28.835200
341.296361	18105.469220	28.840218
342.140780	18131.620318	28.845236
342.605610	18149.441195	28.850253
343.170103	18169.289843	28.855271
343.120878	18185.779932	28.860288
343.399698	18194.102259	28.865306
343.556317	18206.051197	28.870324
343.923924	18233.360985	28.875341
344.094425	18244.126702	28.880359
344.083880	18274.845323	28.885376
343.957197	18284.477975	28.890394
344.588982	18325.635624	28.895412
344.603715	18353.591003	28.900429
345.092020	18376.514721	28.905447
345.482482	18418.983126	28.910464
345.511052	18451.426484	28.915482
346.084321	18482.966170	28.920500
346.701086	18507.996484	28.925517
347.147930	18539.001397	28.930535
347.372647	18566.556943	28.935552
348.196054	18580.889243	28.940570
348.357257	18606.390360	28.945588
348.720425	18618.512307	28.950605
349.028534	18644.741933	28.955623
348.882387	18668.651392	28.960640
349.362455	18693.349092	28.965658
349.543234	18724.890281	28.970676
349.595555	18763.449107	28.975693
350.245471	18783.093069	28.980711
350.311098	18824.063596	28.985728
350.733194	18851.760789	28.990746
350.844002	18891.511292	28.995764
351.310713	18928.451201	29.000781
351.909200	18957.991408	29.005799
352.103737	18993.024622	29.010816
352.300428	19024.153711	29.015834
353.095817	19057.603593	29.020852
353.211171	19093.670692	29.025869
354.149130	19129.469176	29.030887
353.853950	19159.862942	29.035904
354.501933	19199.591482	29.040922
354.647744	19240.900879	29.045940
354.788934	19275.924902	29.050957
355.639865	19299.839385	29.055975
355.867644	19322.452710	29.060992
356.520318	19348.361072	29.066010
357.076231	19373.761016	29.071028
356.890170	19418.594887	29.076045
357.398103	19448.175125	29.081063
357.425398	19484.795807	29.086080
357.971125	19527.714987	29.091098
358.643333	19542.449284	29.096116
359.072557	19572.347535	29.101133
359.961097	19594.062776	29.106151
360.043157	19626.953322	29.111168
360.426056	19655.965658	29.116186
361.119804	19679.221744	29.121204
361.040119	19707.597613	29.126221
361.432651	19733.384017	29.131239
361.867155	19762.177986	29.136256
362.001624	19796.027994	29.141274
362.402875	19819.014323	29.146292
362.525522	19850.126089	29.151309
363.314908	19871.134957	29.156327
363.631660	19901.762602	29.161344
364.005785	19922.309761	29.166362
364.657818	19942.353634	29.171380
364.588241	19982.309483	29.176397
365.054661	20004.862326	29.181415
364.886313	20030.532445	29.186432
365.473088	20049.237922	29.191450
366.168956	20085.485158	29.196468
366.231515	20110.305367	29.201485
366.659079	20129.140709	29.206503
366.712953	20164.079045	29.211520
366.789137	20184.906216	29.216538
367.058224	20213.158510	29.221556
367.477997	20251.326630	29.226573
367.737562	20282.641205	29.231591
368.322867	20330.807910	29.236608
369.167671	20358.988587	29.241626
370.232037	20366.543495	29.246644
370.252746	20387.213282	29.251661
371.020740	20406.588195	29.256679
371.662490	20422.563116	29.261696
371.689869	20433.928715	29.266714
372.386613	20445.513888	29.271732
372.588607	20468.167855	29.276749
372.683907	20484.851437	29.281767
372.844970	20506.763489	29.286784
373.154847	20537.749822	29.291802
373.272081	20558.185674	29.296820
373.475726	20585.224623	29.301837
373.750445	20613.766754	29.306855
374.182967	20649.136316	29.311872
374.347763	20687.967231	29.316890
374.844572	20715.433922	29.321908
375.101848	20747.833027	29.326925
375.504703	20790.532334	29.331943
375.682524	20826.283357	29.336960
376.236658	20858.639682	29.341978
376.931346	20892.102576	29.346996
377.168468	20931.669075	29.352013
377.830154	20959.902636	29.357031
378.017141	20988.175022	29.362048
378.094206	21021.605255	29.367066
378.831366	21048.367440	29.372084
378.811492	21093.063716	29.377101
379.013020	21133.248605	29.382119
379.378516	21181.332399	29.387136
379.554992	21217.527575	29.392154
380.274318	21253.869480	29.397172
380.615544	21297.102566	29.402189
381.237713	21338.158823	29.407207
381.949293	21371.999797	29.412224
381.611039	21405.624956	29.417242
381.882206	21449.977412	29.422260
382.335334	21499.150910	29.427277
382.910973	21545.873550	29.432295
382.944550	21578.591684	29.437312
383.463668	21628.496968	29.442330
384.144583	21674.069696	29.447348
383.869607	21717.808410	29.452365
384.275340	21762.745729	29.457383
384.775717	21807.748948	29.462400
385.249191	21846.762988	29.467418
386.163118	21892.674831	29.472436
386.194906	21930.828059	29.477453
386.678035	21956.660663	29.482471
388.075475	21981.554452	29.487488
388.905859	21991.230187	29.492506
389.485271	21990.159496	29.497524
389.614761	22019.585152	29.502541
390.121249	22031.656604	29.507559
390.615756	22040.907383	29.512576
390.737064	22070.883308	29.517594
390.891651	22080.378442	29.522612
391.012098	22104.292775	29.527629
391.609573	22133.029722	29.532647
391.835876	22158.439868	29.537664
391.868751	22198.791787	29.542682
392.239619	22215.885581	29.547700
392.143855	22251.793712	29.552717
392.727818	22284.355796	29.557735
393.327715	22322.882476	29.562752
393.348092	22362.637674	29.567770
394.183735	22391.605480	29.572788
393.874847	22429.218951	29.577805
394.455925	22473.047857	29.582823
394.826648	22515.509404	29.587840
395.614334	22541.252853	29.592858
395.890746	22572.893612	29.597876
396.057487	22621.786676	29.602893
396.740074	22657.861898	29.607911
397.579023	22690.172894	29.612928
397.303859	22728.241725	29.617946
398.344745	22768.283462	29.622964
399.022001	22796.597830	29.627981
399.858556	22809.496400	29.632999
400.039887	22837.091545	29.638016
399.676145	22858.841078	29.643034
400.399762	22891.380386	29.648052
400.701390	22911.889964	29.653069
400.772028	22955.078995	29.658087
401.566525	22987.678883	29.663104
401.305435	23025.392705	29.668122
401.760180	23060.511134	29.673140
402.147789	23105.598599	29.678157
402.729583	23136.699181	29.683175
402.801909	23181.976504	29.688192
403.401547	23223.514272	29.693210
404.045937	23268.349988	29.698228
404.099318	23307.423581	29.703245
404.790306	23354.841076	29.708263
405.213856	23386.959629	29.713280
405.417836	23426.685825	29.718298
405.896096	23452.777011	29.723316
406.460630	23504.124585	29.728333
406.565101	23541.855745	29.733351
407.224299	23579.968203	29.738368
407.347438	23621.121773	29.743386
408.134634	23646.737650	29.748404
408.343240	23681.864836	29.753421
408.765513	23712.088545	29.758439
409.461936	23740.893245	29.763456
409.393271	23774.323860	29.768474
410.135567	23804.729455	29.773492
410.276567	23845.088790	29.778509
410.851303	23875.397056	29.783527
411.383715	23917.149893	29.788544
411.222024	23957.971415	29.793562
411.979152	23985.135378	29.798580
412.131638	24036.760181	29.803597
412.336188	24078.840862	29.808615
413.001608	24125.176641	29.813632
413.091478	24169.664983	29.818650
413.481605	24209.219140	29.823668
413.729903	24261.566300	29.828685
413.932002	24308.805244	29.833703
414.320093	24350.486079	29.838720
414.685613	24408.592306	29.843738
415.649241	24455.521352	29.848756
415.803745	24505.055883	29.853773
416.368233	24567.096713	29.858791
417.220996	24606.339076	29.863808
417.404905	24652.960669	29.868826
417.922500	24694.616987	29.873844
418.384520	24744.730381	29.878861
418.793555	24779.197729	29.883879
419.191232	24819.345016	29.888896
419.610794	24861.087933	29.893914
420.469023	24901.522398	29.898932
420.846707	24941.540910	29.903949
421.261280	24981.080028	29.908967
421.847683	25011.227416	29.913984
422.680746	25052.496166	29.919002
422.619646	25078.783187	29.924020
423.301524	25114.182326	29.929037
423.453617	25165.299542	29.934055
423.986758	25195.443761	29.939072
424.408734	25240.594009	29.944090
424.818099	25275.065443	29.949108
425.128045	25314.433983	29.954125
425.602006	25357.698704	29.959143
426.001020	25392.963926	29.964160
426.128740	25433.288233	29.969178
427.098092	25463.802955	29.974196
427.469391	25502.467413	29.979213
428.217226	25526.048702	29.984231
428.758765	25543.012462	29.989248
429.390339	25581.796531	29.994266
429.722380	25605.638454	29.999284
430.224293	25638.924417	30.004301
430.366957	25674.871362	30.009319
430.876437	25693.011104	30.014336
431.200066	25719.513921	30.019354
431.956598	25735.709168	30.024372
432.598745	25758.652736	30.029389
433.179729	25777.212490	30.034407
433.749347	25791.215844	30.039424
434.074352	25822.368434	30.044442
434.127208	25829.747418	30.049460
434.606393	25855.526623	30.054477
434.556923	25884.689858	30.059495
434.935194	25906.410693	30.064512
434.962056	25942.444284	30.069530
435.356962	25976.600976	30.074548
435.464346	26018.441186	30.079565
435.611294	26058.315694	30.084583
436.287817	26085.414759	30.089600
436.436010	26145.185532	30.094618
436.957559	26188.472562	30.099636
437.207124	26231.273170	30.104653
437.380854	26286.629839	30.109671
438.178005	26335.021580	30.114688
438.492615	26386.584585	30.119706
438.823381	26432.567471	30.124724
439.650048	26485.421622	30.129741
440.006687	26542.179994	30.134759
440.712117	26588.294680	30.139776
440.562021	26650.272976	30.144794
441.095452	26689.672582	30.149812
441.374427	26739.498164	30.154829
441.688804	26797.829366	30.159847
442.181790	26845.820364	30.164864
442.740917	26905.558024	30.169882
443.083257	26964.452851	30.174900
443.654873	27024.333898	30.179917
443.641421	27081.248930	30.184935
444.261178	27134.023776	30.189952
445.516931	27174.281848	30.194970
446.561929	27215.771811	30.199988
447.635074	27253.067418	30.205005
448.055021	27286.332720	30.210023
448.563016	27307.928966	30.215040
449.259205	27344.396541	30.220058
449.517976	27368.474275	30.225076
449.964962	27390.251440	30.230093
450.089205	27429.792244	30.235111
451.064570	27450.929992	30.240128
451.751687	27495.072105	30.245146
451.362942	27511.452652	30.250164
451.789843	27543.007301	30.255181
451.766933	27576.771800	30.260199
452.123305	27618.601570	30.265216
452.610725	27671.870800	30.270234
452.758809	27714.216039	30.275252
453.435405	27754.928050	30.280269
453.679657	27803.257709	30.285287
454.351186	27847.649468	30.290304
454.474124	27890.292850	30.295322
454.581351	27938.643207	30.300340
455.538323	27982.563629	30.305357
455.546838	28034.710826	30.310375
456.057049	28082.459331	30.315392
456.623658	28126.932876	30.320410
456.476298	28173.055904	30.325428
457.420494	28224.017947	30.330445
457.300591	28275.632580	30.335463
457.717048	28326.720059	30.340480
458.234830	28389.438756	30.345498
458.512862	28445.386989	30.350516
459.019246	28500.870335	30.355533
459.816664	28571.609273	30.360551
459.991109	28623.202881	30.365568
460.502663	28689.763459	30.370586
461.061017	28740.521780	30.375604
462.056625	28798.048775	30.380621
462.445800	28844.037446	30.385639
463.081892	28891.877009	30.390656
463.428390	28951.430905	30.395674
463.671767	29002.714072	30.400692
464.456949	29050.537983	30.405709
464.875317	29108.212235	30.410727
465.248751	29152.749873	30.415744
466.041331	29214.048758	30.420762
466.203476	29261.863263	30.425780
466.902317	29312.690659	30.430797
467.479513	29374.023852	30.435815
468.163037	29415.227584	30.440832
468.264389	29461.923475	30.445850
468.514187	29522.552873	30.450868
468.930447	29566.935920	30.455885
469.762105	29630.889439	30.460903
470.425349	29682.651650	30.465920
470.538661	29727.888455	30.470938
470.696317	29779.948990	30.475956
471.325541	29827.514601	30.480973
471.626759	29883.453953	30.485991
472.424146	29932.871599	30.491008
472.943423	29990.515662	30.496026
473.468452	30041.210861	30.501044
474.182880	30091.381516	30.506061
474.860300	30150.368423	30.511079
475.135594	30190.807746	30.516096
475.449043	30232.392335	30.521114
476.175314	30272.801899	30.526132
476.965077	30312.339253	30.531149
477.089052	30371.387023	30.536167
477.709239	30415.860316	30.541184
478.501689	30459.026258	30.546202
478.793274	30506.673638	30.551220
479.782295	30544.871023	30.556237
479.939349	30586.966024	30.561255
480.657569	30623.424002	30.566272
481.149735	30656.342509	30.571290
481.363411	30691.312512	30.576308
481.830595	30722.193840	30.581325
481.963533	30758.215958	30.586343
482.416457	30800.453250	30.591360
482.590317	30834.392206	30.596378
483.011823	30880.497383	30.601396
483.704667	30930.431140	30.606413
483.859264	30981.063125	30.611431
484.416878	31036.592982	30.616448
484.663325	31083.116811	30.621466
484.603558	31136.518657	30.626484
485.252324	31188.041613	30.631501
485.461097	31257.525809	30.636519
486.344273	31315.007683	30.641536
486.665911	31366.489388	30.646554
486.935351	31427.847708	30.651572
487.930405	31493.509208	30.656589
487.890874	31556.943655	30.661607
488.597789	31613.068225	30.666624
489.178532	31672.354446	30.671642
489.648233	31731.180233	30.676660
490.790811	31793.485203	30.681677
491.284683	31854.790755	30.686695
492.155417	31894.803732	30.691712
493.005317	31919.928731	30.696730
493.749859	31960.973295	30.701748
494.662414	32002.371004	30.706765
494.863077	32034.496286	30.711783
495.614918	32077.313369	30.716800
495.866002	32116.839751	30.721818
495.844888	32157.176544	30.726836
496.686160	32192.998136	30.731853
496.801559	32235.107321	30.736871
497.221558	32273.781460	30.741888
498.084895	32313.515784	30.746906
498.287793	32356.680059	30.751924
498.845715	32408.136902	30.756941
499.015733	32464.750619	30.761959
499.464390	32507.598594	30.766976
499.983090	32556.803048	30.771994
500.493729	32612.295365	30.777012
501.201249	32649.882792	30.782029
501.212563	32710.784815	30.787047
501.486745	32770.767838	30.792064
501.797790	32826.973522	30.797082
502.355700	32888.722928	30.802100
502.855044	32953.168215	30.807117
503.117888	33012.869962	30.812135
503.222527	33074.656649	30.817152
503.697193	33146.854542	30.822170
504.347882	33216.254836	30.827188
504.959213	33285.204535	30.832205
506.022459	33350.425656	30.837223
506.474061	33401.180858	30.842240
507.293996	33459.002369	30.847258
507.418626	33517.744820	30.852276
507.842788	33567.940278	30.857293
508.633055	33624.255698	30.862311
508.886098	33668.538058	30.867328
509.528787	33719.807401	30.872346
509.529047	33777.593651	30.877364
510.464694	33832.051174	30.882381
511.153538	33893.677447	30.887399
511.408803	33948.220343	30.892416
512.129190	33998.274718	30.897434
512.355961	34062.663377	30.902452
513.277078	34110.960467	30.907469
513.686770	34167.721524	30.912487
514.199174	34229.101442	30.917504
514.840519	34283.241496	30.922522
515.355124	34344.978068	30.927540
515.988403	34391.475755	30.932557
516.301132	34442.772131	30.937575
516.805604	34498.716334	30.942592
517.459015	34554.461603	30.947610
517.647151	34617.470158	30.952628
517.982785	34677.332218	30.957645
518.208038	34736.986145	30.962663
518.777966	34800.166629	30.967680
519.215339	34867.731903	30.972698
519.614708	34946.088690	30.977716
520.820938	35002.015204	30.982733
521.241538	35060.068084	30.987751
522.028493	35126.150965	30.992768
522.743926	35183.143725	30.997786
523.512779	35240.929200	31.002804
523.847368	35291.498294	31.007821
524.295513	35345.488411	31.012839
524.834958	35406.334277	31.017856
525.485807	35463.929211	31.022874
525.870634	35533.415526	31.027892
526.013524	35580.704150	31.032909
526.344407	35638.019891	31.037927
526.510896	35706.281748	31.042944
527.349280	35777.493549	31.047962
527.747070	35857.956669	31.052980
528.371675	35930.654471	31.057997
528.631985	36006.606093	31.063015
529.142807	36073.503580	31.068032
529.650044	36145.035541	31.073050
530.180613	36222.403173	31.078068
530.750183	36293.887161	31.083085
531.501008	36358.696044	31.088103
531.978431	36437.430968	31.093120
532.718133	36507.242123	31.098138
532.889861	36580.881833	31.103156
533.472885	36653.791658	31.108173
533.944353	36714.956566	31.113191
534.765073	36791.036384	31.118208
535.062740	36857.682868	31.123226
535.593825	36929.330608	31.128244
536.030752	36987.068020	31.133261
536.796851	37049.768158	31.138279
537.529723	37116.981801	31.143296
538.115057	37170.552932	31.148314
538.433013	37240.764281	31.153332
539.261254	37305.967305	31.158349
539.543283	37366.671263	31.163367
539.898201	37432.811283	31.168384
540.746739	37496.761482	31.173402
540.949881	37564.970335	31.178420
541.792545	37634.143132	31.183437
542.261825	37690.488283	31.188455
542.515171	37761.325090	31.193472
542.912719	37822.986181	31.198490
543.477894	37912.101118	31.203508
544.137735	37985.839613	31.208525
544.650662	38058.284057	31.213543
545.044042	38132.037226	31.218560
545.690916	38207.003650	31.223578
546.476473	38292.060945	31.228596
546.873860	38365.040949	31.233613
548.136821	38418.670086	31.238631
549.604766	38454.232548	31.243648
550.781114	38506.895016	31.248666
551.060498	38558.978935	31.253684
551.469388	38603.328661	31.258701
552.482181	38653.629848	31.263719
552.275398	38697.043530	31.268736
552.961904	38739.414023	31.273754
553.305341	38793.987865	31.278772
553.303832	38853.507817	31.283789
554.012615	38907.492197	31.288807
554.292796	38979.535022	31.293824
554.712557	39028.903380	31.298842
555.005931	39103.880353	31.303860
555.551037	39174.906216	31.308877
555.988752	39248.046963	31.313895
556.301489	39322.860503	31.318912
556.739079	39398.117027	31.323930
557.388969	39472.835521	31.328948
557.924982	39544.508385	31.333965
559.457417	39611.843551	31.338983
559.767365	39683.921901	31.344000
560.254061	39751.389395	31.349018
560.752469	39812.335834	31.354036
561.738406	39878.733256	31.359053
562.409650	39929.784680	31.364071
562.496114	40007.727359	31.369088
563.851247	40066.788300	31.374106
563.554460	40136.595078	31.379124
563.999095	40203.935669	31.384141
564.988662	40273.519405	31.389159
565.193245	40341.122621	31.394176
565.808652	40406.189964	31.399194
566.028451	40468.774337	31.404212
566.184005	40538.615620	31.409229
567.060933	40609.858485	31.414247
567.260008	40691.020838	31.419264
568.234251	40756.204727	31.424282
568.507822	40832.376025	31.429300
568.664278	40912.637366	31.434317
569.475161	40988.193140	31.439335
570.069707	41053.477855	31.444352
570.812439	41124.745683	31.449370
571.383780	41207.564052	31.454388
572.083409	41285.239682	31.459405
572.693441	41355.047198	31.464423
573.048540	41444.758176	31.469440
573.752535	41515.431084	31.474458
574.340968	41581.024953	31.479476
575.160963	41657.889017	31.484493
576.003343	41724.968040	31.489511
576.776648	41796.763632	31.494528
577.292278	41869.528763	31.499546
577.419658	41938.316065	31.504564
577.989729	42013.639395	31.509581
578.531337	42095.541669	31.514599
579.027977	42169.116360	31.519616
579.422323	42249.080607	31.524634
580.313744	42323.245015	31.529652
580.833240	42391.133223	31.534669
581.734210	42464.949233	31.539687
582.180599	42547.027666	31.544704
582.659950	42621.566974	31.549722
583.131540	42701.775673	31.554740
583.232752	42783.450120	31.559757
584.156825	42856.749032	31.564775
584.623043	42950.635090	31.569792
585.356518	43033.070625	31.574810
586.049228	43106.097548	31.579828
586.620363	43188.675252	31.584845
587.414633	43269.667852	31.589863
587.894784	43350.395696	31.594880
588.286053	43423.437603	31.599898
589.177486	43505.756572	31.604916
590.005217	43591.219231	31.609933
590.720536	43650.622169	31.614951
591.727067	43728.908971	31.619968
592.567916	43791.789581	31.624986
593.079322	43853.081670	31.630004
593.875896	43910.993693	31.635021
594.416172	43968.229841	31.640039
594.864953	44030.790017	31.645056
595.429298	44102.222862	31.650074
595.746155	44164.032429	31.655092
596.365336	44241.443545	31.660109
597.125516	44303.300766	31.665127
597.244878	44372.085689	31.670144
598.304311	44442.023452	31.675162
598.342411	44492.608434	31.680180
598.882163	44563.968288	31.685197
600.245450	44612.987625	31.690215
600.320198	44686.846522	31.695232
600.692508	44746.497983	31.700250
601.709734	44806.512823	31.705268
602.058813	44878.762314	31.710285
602.754514	44939.915819	31.715303
603.199253	45009.840992	31.720320
603.974058	45072.276115	31.725338
604.626602	45135.262924	31.730356
604.785999	45198.792334	31.735373
605.687566	45265.899084	31.740391
605.856092	45348.466762	31.745408
606.471043	45421.367515	31.750426
607.012309	45499.615027	31.755444
607.392773	45576.358775	31.760461
608.211132	45650.596132	31.765479
608.912679	45740.372373	31.770496
609.701154	45812.682764	31.775514
610.721780	45871.560330	31.780532
610.840710	45946.149207	31.785549
611.670506	46017.275335	31.790567
612.493570	46082.333027	31.795584
613.283814	46161.851206	31.800602
613.574113	46235.098079	31.805620
614.080544	46316.860419	31.810637
615.256043	46385.803270	31.815655
615.456520	46460.465450	31.820672
615.568967	46533.980797	31.825690
616.504391	46599.109427	31.830708
616.848229	46684.485724	31.835725
617.559428	46754.166353	31.840743
618.146759	46839.804813	31.845760
618.371500	46923.967717	31.850778
619.338652	47006.228863	31.855796
620.084923	47093.499304	31.860813
620.907822	47162.322182	31.865831
621.593038	47243.018770	31.870848
622.634456	47310.355090	31.875866
623.487873	47379.779913	31.880884
623.406615	47462.023656	31.885901
624.169478	47521.057844	31.890919
624.814029	47611.035800	31.895936
625.548621	47684.294200	31.900954
626.360269	47755.695192	31.905972
626.781503	47831.515581	31.910989
627.443485	47895.179435	31.916007
628.103773	47977.449936	31.921024
628.699189	48048.816416	31.926042
629.461229	48117.795269	31.931060
629.586510	48197.464228	31.936077
630.348195	48276.929733	31.941095
630.917012	48350.847599	31.946112
631.640277	48439.306187	31.951130
632.145459	48498.921301	31.956148
632.354742	48572.547859	31.961165
633.479207	48643.251052	31.966183
633.916155	48721.431650	31.971200
634.369222	48796.438631	31.976218
634.991703	48863.236238	31.981236
635.375477	48950.068658	31.986253
635.901560	49037.609876	31.991271
636.494967	49120.004087	31.996288
636.849369	49205.964596	32.001306
637.307554	49290.549499	32.006324
637.746331	49397.488583	32.011341
639.004612	49477.338257	32.016359
639.275051	49573.220296	32.021376
640.279610	49660.581273	32.026394
641.304069	49742.815836	32.031412
641.954555	49832.493550	32.036429
643.221744	49906.834683	32.041447
643.801365	49982.096211	32.046464
644.392983	50058.587885	32.051482
645.097302	50129.103140	32.056500
645.145049	50216.339927	32.061517
645.778196	50290.778515	32.066535
646.541074	50387.401479	32.071552
646.966674	50475.939291	32.076570
647.760318	50557.951499	32.081588
648.278033	50647.011305	32.086605
648.877250	50730.700142	32.091623
649.566904	50827.154613	32.096640
649.744549	50915.882203	32.101658
650.370275	51010.093086	32.106676
650.807828	51112.853084	32.111693
651.774310	51203.171600	32.116711
652.623955	51305.659840	32.121728
652.741978	51408.792023	32.126746
653.667957	51501.879785	32.131764
654.299651	51603.591904	32.136781
655.452715	51693.590087	32.141799
656.527979	51793.944646	32.146816
656.793663	51871.585945	32.151834
658.398899	51947.216363	32.156852
659.243573	52034.116212	32.161869
660.442619	52079.919405	32.166887
661.933668	52134.789775	32.171904
662.463948	52199.915012	32.176922
663.632569	52252.155723	32.181940
664.329243	52307.762893	32.186957
665.352455	52343.607742	32.191975
665.951845	52383.910117	32.196992
666.547224	52433.020897	32.202010
667.112315	52474.296025	32.207028
667.402229	52534.339437	32.212045
667.760218	52572.478473	32.217063
668.634917	52626.792388	32.222080
668.783317	52678.311809	32.227098
669.445455	52727.576164	32.232116
669.781779	52773.686731	32.237133
670.292330	52825.037083	32.242151
670.673908	52876.365433	32.247168
671.468360	52942.338761	32.252186
672.428985	53001.624216	32.257204
672.873020	53071.967177	32.262221
673.143979	53136.609182	32.267239
673.589113	53196.470053	32.272256
673.860606	53273.376610	32.277274
675.134703	53340.362202	32.282292
675.545020	53416.493626	32.287309
676.116393	53474.122214	32.292327
676.977836	53550.353790	32.297344
677.483866	53627.758625	32.302362
678.141246	53696.076886	32.307380
678.484175	53782.975608	32.312397
679.535275	53862.114079	32.317415
680.291993	53939.774164	32.322432
680.664666	54021.474840	32.327450
681.585522	54093.060359	32.332468
681.843895	54183.532789	32.337485
682.672390	54255.678133	32.342503
683.331071	54338.740215	32.347520
683.686141	54432.287130	32.352538
684.282798	54523.113879	32.357556
684.866765	54620.097866	32.362573
685.637084	54707.186483	32.367591
686.722725	54793.254657	32.372608
687.166036	54893.954366	32.377626
687.977242	54976.297882	32.382644
688.625577	55062.157772	32.387661
689.266556	55150.907126	32.392679
690.338387	55242.938528	32.397696
691.168583	55327.011681	32.402714
692.512919	55384.835665	32.407732
693.632744	55449.579892	32.412749
694.334927	55513.321606	32.417767
695.322631	55570.689046	32.422784
695.766493	55648.775899	32.427802
696.631711	55708.945197	32.432820
696.995308	55779.595870	32.437837
697.739613	55849.802414	32.442855
698.321167	55916.352901	32.447872
698.909903	55997.771872	32.452890
699.458877	56062.919205	32.457908
699.587210	56148.986584	32.462925
699.885312	56231.132466	32.467943
700.268464	56316.202670	32.472960
700.635105	56412.575342	32.477978
701.335166	56517.119400	32.482996
702.098682	56616.565873	32.488013
702.859590	56714.035248	32.493031
703.630482	56811.541302	32.498048
704.516291	56896.325620	32.503066
705.734418	56967.870504	32.508084
706.538324	57056.928996	32.513101
706.893371	57135.517130	32.518119
707.957173	57215.993842	32.523136
708.347535	57294.102561	32.528154
709.056486	57379.216236	32.533172
709.465965	57466.467115	32.538189
710.454147	57558.226420	32.543207
710.962571	57643.084841	32.548224
711.553909	57735.235244	32.553242
712.650604	57813.730565	32.558260
713.426698	57905.034818	32.563277
713.867642	57994.766333	32.568295
714.414122	58083.266720	32.573312
715.057354	58178.153139	32.578330
715.472911	58262.157891	32.583348
716.362316	58355.713671	32.588365
717.080912	58455.872095	32.593383
717.870794	58546.614378	32.598400
718.903531	58640.981182	32.603418
719.825129	58732.719285	32.608436
720.298193	58820.502311	32.613453
721.387245	58913.798931	32.618471
721.922419	58993.640102	32.623488
722.612593	59101.523674	32.628506
723.379853	59194.175142	32.633524
723.704671	59290.872035	32.638541
724.414088	59387.661515	32.643559
725.211351	59478.109620	32.648576
725.763085	59584.464623	32.653594
726.481747	59684.268800	32.658612
727.365874	59784.797266	32.663629
727.700416	59887.954925	32.668647
728.551494	59994.684260	32.673664
728.952489	60117.577324	32.678682
729.200829	60227.723146	32.683700
729.984308	60338.612225	32.688717
730.599750	60456.534094	32.693735
731.851329	60570.921795	32.698752
732.176337	60691.991956	32.703770
732.722129	60817.259994	32.708788
734.043635	60931.625082	32.713805
734.165833	61054.002614	32.718823
735.751829	61176.970816	32.723840
736.261425	61287.463132	32.728858
736.827506	61395.411622	32.733876
737.637838	61516.460376	32.738893
738.602147	61633.595971	32.743911
739.461144	61741.097860	32.748928
740.451471	61861.510971	32.753946
741.483707	61953.977782	32.758964
742.259129	62064.175864	32.763981
743.384368	62162.411626	32.768999
744.223427	62248.332385	32.774016
744.952956	62346.409235	32.779034
746.264552	62425.479630	32.784052
746.825289	62509.811914	32.789069
747.392274	62591.418940	32.794087
748.888711	62654.269405	32.799104
749.422143	62732.728338	32.804122
750.231859	62814.534878	32.809140
751.150668	62881.979554	32.814157
751.028349	62974.813045	32.819175
751.753583	63046.710165	32.824192
752.326476	63135.360527	32.829210
752.845186	63225.152114	32.834228
753.569931	63322.355684	32.839245
754.044646	63420.158842	32.844263
755.046658	63514.584853	32.849280
755.297308	63625.721886	32.854298
756.258424	63721.464436	32.859316
757.177209	63821.494526	32.864333
757.794817	63926.678394	32.869351
758.876520	64011.370043	32.874368
759.699417	64110.191501	32.879386
760.545222	64194.209926	32.884404
761.572870	64292.706367	32.889421
761.971862	64396.393811	32.894439
762.794712	64490.816987	32.899456
763.282880	64592.435478	32.904474
763.961783	64692.732090	32.909492
765.327083	64788.568337	32.914509
765.887273	64893.495039	32.919527
766.105884	64991.501128	32.924544
767.232447	65096.015718	32.929562
767.972993	65201.880355	32.934580
768.888318	65305.976972	32.939597
769.151826	65421.104310	32.944615
770.090831	65522.713288	32.949632
770.651450	65628.383283	32.954650
771.374953	65743.888796	32.959668
772.254931	65846.843464	32.964685
772.647043	65970.309974	32.969703
773.333514	66090.982832	32.974720
774.155684	66212.290673	32.979738
774.657711	66324.024817	32.984756
775.952147	66432.038920	32.989773
776.650765	66562.898048	32.994791
777.365285	66661.162026	32.999808
777.968400	66782.093354	33.004826
778.781857	66905.486811	33.009844
780.046086	67020.078381	33.014861
780.765582	67132.816458	33.019879
781.857271	67254.381258	33.024896
782.623985	67362.439904	33.029914
783.241373	67468.520322	33.034932
784.423782	67578.652316	33.039949
784.785815	67692.131132	33.044967
786.185011	67790.333630	33.049984
786.817057	67900.631110	33.055002
787.364515	68008.041371	33.060020
788.628050	68105.573023	33.065037
788.743265	68211.426991	33.070055
789.380540	68314.941025	33.075072
790.219718	68417.434564	33.080090
790.550758	68513.692441	33.085108
791.783581	68627.861722	33.090125
792.201900	68744.371617	33.095143
793.031508	68856.733174	33.100160
793.509445	68961.890060	33.105178
793.954478	69084.239968	33.110196
795.469976	69195.600544	33.115213
796.175874	69305.298194	33.120231
798.026733	69414.357648	33.125248
798.804014	69520.414507	33.130266
799.359397	69615.323601	33.135284
800.204114	69724.436815	33.140301
800.751083	69834.752471	33.145319
801.687174	69939.626973	33.150336
802.655893	70043.952564	33.155354
803.509878	70149.082445	33.160372
804.360412	70252.948689	33.165389
804.945675	70372.524746	33.170407
805.767666	70471.894432	33.175424
806.518064	70581.502407	33.180442
807.516918	70684.118497	33.185460
808.456840	70787.263723	33.190477
809.093360	70904.652204	33.195495
809.949340	71006.895887	33.200512
810.970030	71117.636521	33.205530
811.867899	71224.092126	33.210548
813.117713	71308.758680	33.215565
813.894339	71415.444680	33.220583
814.615243	71502.055521	33.225600
815.583535	71608.355489	33.230618
816.306858	71706.242585	33.235636
817.454218	71798.662993	33.240653
818.007430	71901.462342	33.245671
818.805978	71998.167890	33.250688
819.224977	72097.234571	33.255706
820.005900	72203.076237	33.260724
820.826006	72304.219078	33.265741
821.086592	72421.205787	33.270759
821.784224	72540.641682	33.275776
822.555989	72653.235185	33.280794
823.014107	72776.046340	33.285812
823.791572	72900.643902	33.290829
824.427181	73025.614316	33.295847
824.884429	73151.520397	33.300864
826.228352	73285.687012	33.305882
826.769866	73419.827441	33.310900
827.814751	73545.616151	33.315917
828.815593	73676.175612	33.320935
829.872812	73793.412649	33.325952
831.096211	73901.381384	33.330970
831.843575	74022.442261	33.335988
832.770285	74120.545623	33.341005
833.660706	74233.822610	33.346023
834.449968	74346.972031	33.351040
835.025916	74441.190168	33.356058
835.859738	74550.253432	33.361076
837.172295	74653.656616	33.366093
837.993532	74761.736382	33.371111
838.729496	74868.009671	33.376128
839.940070	74973.278722	33.381146
840.666769	75074.336414	33.386164
841.435742	75178.543558	33.391181
842.334005	75287.080745	33.396199
842.874611	75399.810059	33.401216
843.832049	75500.267225	33.406234
844.560005	75629.714765	33.411252
845.546712	75738.827252	33.416269
846.155856	75852.818496	33.421287
846.551759	75969.098665	33.426304
847.578306	76091.324806	33.431322
848.140188	76213.435113	33.436340
849.329272	76334.274781	33.441357
849.851412	76462.819903	33.446375
850.654090	76578.571806	33.451392
851.223163	76712.284587	33.456410
851.546145	76850.759200	33.461428
852.824460	76984.889804	33.466445
853.605627	77133.819853	33.471463
854.291942	77274.891627	33.476480
855.075324	77404.099540	33.481498
855.343833	77546.281991	33.486516
856.877987	77673.952217	33.491533
857.624908	77816.193598	33.496551
858.644862	77962.254235	33.501568
859.832724	78099.683783	33.506586
860.607216	78247.464676	33.511604
861.601388	78384.606503	33.516621
863.028427	78500.514380	33.521639
864.594050	78610.566470	33.526656
866.034546	78724.992890	33.531674
867.059484	78836.207792	33.536692
868.863172	78931.436479	33.541709
869.681688	79021.336833	33.546727
870.410230	79114.359125	33.551744
871.512990	79211.524660	33.556762
871.784484	79311.180027	33.561780
872.678747	79404.288995	33.566797
873.365427	79510.415520	33.571815
874.097340	79604.780421	33.576832
875.176304	79711.783324	33.581850
875.499495	79821.446735	33.586868
876.764923	79921.282491	33.591885
877.624637	80027.837290	33.596903
878.131144	80142.968551	33.601920
878.814799	80244.803310	33.606938
878.991332	80363.737501	33.611956
879.894552	80476.904526	33.616973
880.785718	80590.997863	33.621991
881.448408	80699.000365	33.627008
882.143978	80816.772477	33.632026
882.782863	80936.282096	33.637044
883.459488	81063.415941	33.642061
884.219097	81184.709300	33.647079
884.966873	81323.296541	33.652096
886.301845	81451.983735	33.657114
887.040251	81572.903157	33.662132
887.886614	81693.754107	33.667149
888.882118	81834.206396	33.672167
889.905969	81963.038301	33.677184
891.290742	82077.604913	33.682202
891.621137	82203.956512	33.687220
893.022333	82322.975784	33.692237
893.966659	82451.963227	33.697255
894.945373	82583.223280	33.702272
895.644069	82698.201511	33.707290
896.402674	82828.178259	33.712308
896.980491	82965.222626	33.717325
897.998316	83093.789771	33.722343
899.240218	83226.254861	33.727360
900.174776	83352.433302	33.732378
900.922516	83489.109970	33.737396
902.095911	83621.247356	33.742413
902.770298	83758.653166	33.747431
903.275430	83886.926510	33.752448
905.025049	83999.086269	33.757466
906.152705	84133.512305	33.762484
906.540148	84259.738723	33.767501
907.488380	84394.260259	33.772519
908.473124	84525.353029	33.777536
909.247997	84661.861046	33.782554
909.560449	84809.604915	33.787572
910.682570	84946.124719	33.792589
911.451837	85081.427518	33.797607
912.323003	85230.603353	33.802624
913.085671	85370.135968	33.807642
913.914090	85521.529409	33.812660
914.848349	85671.912196	33.817677
915.722994	85819.623057	33.822695
916.647198	85968.794468	33.827712
917.471304	86109.966228	33.832730
918.146705	86266.908764	33.837748
919.575570	86399.467298	33.842765
921.079509	86543.031176	33.847783
921.813362	86690.550084	33.852800
923.229804	86829.852765	33.857818
924.122423	86968.878925	33.862836
925.067267	87104.846669	33.867853
925.861482	87238.208362	33.872871
926.550537	87386.650542	33.877888
927.358241	87513.240006	33.882906
927.907303	87652.436567	33.887924
929.216336	87790.706389	33.892941
930.061218	87923.398725	33.897959
930.845246	88056.652809	33.902976
931.104691	88188.725407	33.907994
932.457742	88334.161214	33.913012
933.311360	88467.943603	33.918029
934.303999	88615.524993	33.923047
935.149341	88766.923480	33.928064
935.732701	88914.924880	33.933082
936.004926	89071.347282	33.938100
937.000154	89226.520327	33.943117
937.901834	89392.108916	33.948135
938.673003	89562.581686	33.953152
939.589549	89721.727029	33.958170
940.601887	89898.648166	33.963188
941.402879	90064.764924	33.968205
942.157799	90234.181897	33.973223
943.275794	90421.664859	33.978240
944.349369	90588.099279	33.983258
944.831971	90772.345552	33.988276
945.842133	90949.648135	33.993293
947.328248	91124.066556	33.998311
948.082615	91303.687781	34.003328
949.228653	91474.135056	34.008346
950.173321	91645.801632	34.013364
951.459901	91818.145092	34.018381
952.452678	91985.786501	34.023399
953.813983	92154.195134	34.028416
955.356556	92305.850690	34.033434
956.470146	92462.802716	34.038452
957.513031	92605.829580	34.043469
959.693585	92732.059240	34.048487
960.913049	92864.897957	34.053504
962.641623	92982.926812	34.058522
963.572133	93107.802645	34.063540
964.723820	93226.564451	34.068557
965.718142	93340.378389	34.073575
966.749739	93465.612187	34.078592
968.012922	93568.607405	34.083610
968.519779	93687.792022	34.088628
969.121576	93813.493645	34.093645
970.067469	93934.604583	34.098663
970.554795	94065.517814	34.103680
971.167388	94193.352782	34.108698
971.624032	94332.957744	34.113716
972.443268	94470.045239	34.118733
973.522926	94618.299910	34.123751
974.227956	94773.658989	34.128768
975.043635	94904.748286	34.133786
976.347731	95061.354941	34.138804
977.015653	95215.349408	34.143821
978.471462	95348.002655	34.148839
978.957135	95498.257080	34.153856
979.950627	95642.797544	34.158874
980.865103	95796.468478	34.163892
981.754059	95936.508461	34.168909
982.813402	96074.063734	34.173927
983.318205	96224.002679	34.178944
983.888007	96366.897892	34.183962
984.632481	96526.046850	34.188980
985.375065	96690.837923	34.193997
986.195189	96844.132548	34.199015
987.068342	97015.880023	34.204032
988.003152	97186.459532	34.209050
989.093803	97363.869998	34.214068
990.088067	97534.422670	34.219085
991.037219	97701.983266	34.224103
992.085678	97896.992494	34.229120
993.090946	98066.571847	34.234138
994.185928	98234.826396	34.239156
994.723986	98412.066541	34.244173
995.926055	98592.739749	34.249191
996.569766	98780.506012	34.254208
997.598657	98960.666971	34.259226
998.983647	99152.544737	34.264244
999.881722	99342.417917	34.269261
1001.470764	99520.315170	34.274279
1002.770991	99697.395679	34.279296
1004.060349	99871.072843	34.284314
1004.779677	100044.253607	34.289332
1006.119919	100216.639048	34.294349
1007.407758	100373.775055	34.299367
1008.512468	100539.947200	34.304384
1009.630606	100692.536305	34.309402
1010.799258	100857.844737	34.314420
1012.116449	101016.575247	34.319437
1013.547964	101174.286700	34.324455
1014.513090	101333.022440	34.329472
1015.428597	101483.048430	34.334490
1016.432444	101640.114083	34.339508
1017.263653	101804.162899	34.344525
1018.055348	101943.182196	34.349543
1019.228826	102105.857209	34.354560
1020.352819	102260.867052	34.359578
1021.238049	102418.324955	34.364596
1022.559207	102578.735994	34.369613
1024.043065	102720.819705	34.374631
1024.920037	102877.762523	34.379648
1026.202475	103015.031718	34.384666
1027.466418	103154.901095	34.389684
1027.911153	103320.431358	34.394701
1029.484805	103461.123208	34.399719
1030.307445	103612.950369	34.404736
1031.181173	103748.824214	34.409754
1032.141920	103900.021446	34.414772
1032.856750	104051.337640	34.419789
1033.784872	104199.781130	34.424807
1034.872166	104373.022476	34.429824
1035.891718	104520.236217	34.434842
1037.014785	104662.126162	34.439860
1037.698769	104806.967153	34.444877
1038.758458	104948.654160	34.449895
1039.453143	105104.058150	34.454912
1040.544590	105261.104999	34.459930
1041.771071	105400.042676	34.464948
1042.915399	105543.263587	34.469965
1043.843259	105684.964401	34.474983
1045.208735	105841.461088	34.480000
1046.103018	105990.452303	34.485018
1047.419279	106129.391053	34.490036
1047.857871	106284.757069	34.495053
1049.169924	106440.544409	34.500071
1049.837456	106604.410242	34.505088
1050.792578	106769.899815	34.510106
1051.679801	106923.850032	34.515124
1052.661997	107094.517619	34.520141
1053.692965	107260.668543	34.525159
1054.565451	107439.425850	34.530176
1055.385569	107616.470590	34.535194
1056.125131	107795.481003	34.540212
1056.709377	107974.012501	34.545229
1058.037915	108165.350971	34.550247
1058.708917	108364.859790	34.555264
1059.583795	108559.052840	34.560282
1060.750762	108756.604815	34.565300
1061.574355	108956.091814	34.570317
1062.707841	109155.159837	34.575335
1063.962620	109362.873301	34.580352
1064.884562	109561.131743	34.585370
1066.156854	109765.652940	34.590388
1067.165021	109971.601698	34.595405
1068.180417	110180.033712	34.600423
1069.766321	110374.295179	34.605440
1070.754801	110578.034877	34.610458
1072.398058	110761.128425	34.615476
1073.662389	110950.394286	34.620493
1075.303755	111122.532277	34.625511
1076.847703	111307.153990	34.630528
1078.474429	111478.207181	34.635546
1079.967700	111644.710825	34.640564
1080.824252	111798.288179	34.645581
1081.870561	111970.799340	34.650599
1082.916803	112136.064876	34.655616
1083.859112	112296.572920	34.660634
1085.047768	112464.286484	34.665652
1086.286794	112636.135278	34.670669
1087.290750	112794.203108	34.675687
1088.302383	112961.151774	34.680704
1088.976492	113135.836937	34.685722
1090.248807	113304.934826	34.690740
1091.015919	113472.992629	34.695757
1091.723671	113647.497814	34.700775
1092.746433	113827.258788	34.705792
1093.603051	114012.649439	34.710810
1094.427287	114190.748938	34.715828
1095.026079	114371.612213	34.720845
1096.370200	114543.315217	34.725863
1097.405907	114728.679864	34.730880
1097.836160	114914.782894	34.735898
1099.206562	115097.520557	34.740916
1100.265721	115297.658536	34.745933
1101.167480	115483.190378	34.750951
1102.258389	115671.326522	34.755968
1103.410097	115872.288920	34.760986
1104.516352	116070.206838	34.766004
1104.743273	116287.536429	34.771021
1106.109879	116484.766396	34.776039
1107.010885	116701.730264	34.781056
1107.939637	116921.250582	34.786074
1109.172296	117137.172570	34.791092
1110.120408	117359.949403	34.796109
1111.106179	117580.275900	34.801127
1112.263119	117809.926365	34.806144
1113.216462	118036.027413	34.811162
1114.531718	118261.244580	34.816180
1115.592591	118492.792270	34.821197
1117.191189	118710.272557	34.826215
1118.778696	118944.622847	34.831232
1119.433109	119166.868119	34.836250
1120.916548	119381.775292	34.841268
1121.924257	119610.793753	34.846285
1122.559937	119836.354743	34.851303
1123.913453	120059.500819	34.856320
1125.150170	120293.326246	34.861338
1126.747799	120512.872923	34.866356
1127.671437	120747.338463	34.871373
1128.876349	120967.196506	34.876391
1130.065093	121200.226189	34.881408
1131.230671	121426.874405	34.886426
1132.618129	121642.866202	34.891444
1133.612516	121879.571646	34.896461
1134.742325	122101.225118	34.901479
1135.945190	122314.262417	34.906496
1136.847250	122547.896583	34.911514
1137.994257	122776.788681	34.916532
1139.136387	123009.865686	34.921549
1140.068960	123240.369542	34.926567
1141.207956	123477.176784	34.931584
1142.121871	123722.097782	34.936602
1143.648138	123956.751223	34.941620
1144.444346	124199.959841	34.946637
1145.602192	124431.422710	34.951655
1146.585765	124673.918592	34.956672
1148.261294	124912.280082	34.961690
1149.441926	125139.789920	34.966708
1150.534969	125379.256043	34.971725
1152.151650	125602.004975	34.976743
1155.036784	125805.183728	34.981760
1156.261900	126004.908892	34.986778
1157.564982	126184.088358	34.991796
1159.401499	126366.650522	34.996813
1160.501669	126533.736621	35.001831
1162.266690	126699.556340	35.006848
1163.855162	126859.855362	35.011866
1164.957284	127015.827426	35.016884
1165.637726	127189.364627	35.021901
1166.956561	127350.105264	35.026919
1167.895256	127513.370876	35.031936
1168.877630	127675.501721	35.036954
1170.995803	127825.878672	35.041972
1172.430550	127989.404076	35.046989
1173.495910	128132.953016	35.052007
1173.961527	128291.829074	35.057024
1174.784441	128459.543309	35.062042
1175.792641	128613.181634	35.067060
1176.603419	128787.212359	35.072077
1177.300500	128969.452328	35.077095
1178.577436	129153.241985	35.082112
1179.303830	129344.377827	35.087130
1180.334820	129540.520562	35.092148
1181.430370	129743.879058	35.097165
1182.098660	129939.046858	35.102183
1183.285306	130152.546301	35.107200
1184.111877	130352.633421	35.112218
1185.599352	130563.244501	35.117236
1186.138998	130776.047532	35.122253
1186.988592	131004.188783	35.127271
1188.175527	131231.310432	35.132288
1188.977942	131457.421944	35.137306
1190.716800	131698.333896	35.142324
1191.838647	131920.337217	35.147341
1192.911391	132142.857556	35.152359
1194.118000	132371.479746	35.157376
1195.131222	132614.094712	35.162394
1196.822477	132841.255355	35.167412
1198.156834	133067.794071	35.172429
1199.460435	133298.269761	35.177447
1201.328185	133522.286138	35.182464
1202.095627	133747.113631	35.187482
1203.652589	133971.110192	35.192500
1204.581821	134195.596081	35.197517
1206.459568	134411.984479	35.202535
1208.008972	134618.655450	35.207552
1209.117350	134831.095843	35.212570
1210.721340	135037.734714	35.217588
1211.980478	135248.605174	35.222605
1213.505208	135448.007971	35.227623
1214.896036	135642.819799	35.232640
1216.121274	135853.065928	35.237658
1217.744839	136040.537195	35.242676
1218.403930	136241.221319	35.247693
1219.610168	136442.218700	35.252711
1220.588822	136644.866492	35.257728
1221.190238	136859.853583	35.262746
1222.562051	137057.795936	35.267764
1223.506352	137261.809982	35.272781
1224.478333	137467.025063	35.277799
1225.737459	137662.923474	35.282816
1226.532901	137880.356308	35.287834
1227.572980	138087.376645	35.292852
1228.603509	138313.787255	35.297869
1229.283201	138531.218672	35.302887
1230.369166	138753.362253	35.307904
1231.638698	138988.815234	35.312922
1233.012199	139222.590927	35.317940
1234.077510	139470.115583	35.322957
1234.815477	139710.850681	35.327975
1235.854125	139949.646596	35.332992
1236.792499	140197.058674	35.338010
1237.975500	140449.693064	35.343028
1239.783444	140696.845699	35.348045
1241.042989	140958.562690	35.353063
1242.747226	141210.377854	35.358080
1243.714073	141468.217683	35.363098
1245.126625	141714.443367	35.368116
1246.522220	141969.804069	35.373133
1247.971967	142221.061313	35.378151
1249.065627	142470.910261	35.383168
1250.091845	142727.633137	35.388186
1251.156403	142982.411030	35.393204
1252.647801	143239.806162	35.398221
1254.039317	143509.889218	35.403239
1255.475698	143761.793674	35.408256
1256.798889	144021.150826	35.413274
1257.741785	144278.266832	35.418292
1259.348017	144541.497986	35.423309
1260.010493	144805.171612	35.428327
1261.027590	145072.033089	35.433344
1262.306490	145342.237880	35.438362
1263.443374	145627.180561	35.443380
1264.692887	145905.904439	35.448397
1265.553295	146185.724329	35.453415
1267.043289	146460.606469	35.458432
1268.231102	146756.177277	35.463450
1269.492375	147037.051087	35.468468
1270.301659	147327.973220	35.473485
1271.479143	147625.112725	35.478503
1273.311911	147917.360866	35.483520
1274.800268	148202.009547	35.488538
1276.338781	148474.539180	35.493556
1277.974905	148766.891026	35.498573
1279.474545	149039.406038	35.503591
1281.088615	149314.008917	35.508608
1282.227222	149583.152378	35.513626
1284.178309	149852.095250	35.518644
1285.628216	150101.148639	35.523661
1287.218266	150366.110772	35.528679
1288.990810	150614.769816	35.533696
1290.250334	150866.613227	35.538714
1291.453532	151097.272549	35.543732
1292.759548	151324.541623	35.548749
1294.195172	151546.728776	35.553767
1295.587913	151768.138110	35.558784
1296.816181	152002.438987	35.563802
1297.846046	152230.229975	35.568820
1299.084675	152469.047613	35.573837
1300.381984	152700.626349	35.578855
1301.867504	152930.347622	35.583872
1302.859585	153167.359739	35.588890
1304.095945	153397.735274	35.593908
1305.007953	153638.087402	35.598925
1306.727142	153886.472063	35.603943
1307.837987	154114.120586	35.608960
1309.060155	154364.191658	35.613978
1310.573661	154605.613745	35.618996
1312.274572	154849.009520	35.624013
1313.143092	155097.154109	35.629031
1314.393209	155335.708020	35.634048
1315.640527	155588.395688	35.639066
1317.055705	155831.516511	35.644084
1318.590533	156082.775318	35.649101
1319.970600	156327.757273	35.654119
1321.826940	156564.222996	35.659136
1323.456656	156806.336132	35.664154
1324.388792	157047.352241	35.669172
1326.627701	157279.874679	35.674189
1327.548089	157518.853098	35.679207
1328.619041	157750.702771	35.684224
1330.007166	157995.363511	35.689242
1330.600162	158236.875994	35.694260
1332.146029	158496.533542	35.699277
1332.797910	158743.823991	35.704295
1334.116535	158993.805558	35.709312
1334.872878	159261.671798	35.714330
1336.272608	159538.031355	35.719348
1337.575139	159797.408802	35.724365
1338.416764	160081.619219	35.729383
1339.649431	160359.218046	35.734400
1340.506538	160645.992419	35.739418
1341.483249	160948.061871	35.744436
1342.685869	161243.674965	35.749453
1344.132902	161543.409776	35.754471
1346.038905	161838.361030	35.759488
1347.122196	162142.869395	35.764506
1348.287019	162432.914580	35.769524
1349.754574	162746.699639	35.774541
1350.742554	163062.535689	35.779559
1351.911706	163358.169027	35.784576
1353.054157	163676.355753	35.789594
1354.621690	163990.158036	35.794612
1356.147040	164295.570116	35.799629
1357.500652	164615.706882	35.804647
1358.847508	164931.482278	35.809664
1360.647483	165241.383682	35.814682
1362.217851	165531.214999	35.819700
1364.522275	165811.177598	35.824717
1366.355145	166074.371900	35.829735
1367.990846	166343.045030	35.834752
1369.580872	166611.816403	35.839770
1371.281849	166865.191261	35.844788
1372.631887	167119.287435	35.849805
1373.673026	167389.667374	35.854823
1375.188001	167649.829092	35.859840
1376.095071	167909.741037	35.864858
1376.908218	168192.866773	35.869876
1378.108586	168465.306871	35.874893
1379.376143	168749.005411	35.879911
1380.573496	169025.129299	35.884928
1381.968467	169317.831847	35.889946
1382.614654	169618.976213	35.894964
1384.363716	169913.994888	35.899981
1385.626990	170212.524854	35.904999
1387.307116	170512.064021	35.910016
1388.871772	170808.972615	35.915034
1390.206403	171103.650891	35.920052
1391.682284	171394.702778	35.925069
1393.214968	171692.701034	35.930087
1395.129759	171984.163623	35.935104
1395.941533	172294.509892	35.940122
1397.494436	172597.243858	35.945140
1399.046375	172882.454061	35.950157
1400.333705	173191.328711	35.955175
1401.822611	173487.505368	35.960192
1403.354514	173788.803585	35.965210
1404.601918	174088.045639	35.970228
1406.205445	174383.700444	35.975245
1407.203782	174691.212586	35.980263
1408.650431	175004.576702	35.985280
1409.601419	175312.583053	35.990298
1411.000309	175629.487443	35.995316
1412.634439	175941.340446	36.000333
1413.421348	176270.283577	36.005351
1415.139462	176587.558172	36.010368
1416.350597	176907.332938	36.015386
1417.799274	177226.751757	36.020404
1419.119110	177555.523131	36.025421
1420.575455	177885.402824	36.030439
1422.084926	178220.593487	36.035456
1423.671186	178542.649540	36.040474
1424.915888	178876.417459	36.045492
1426.776168	179203.406025	36.050509
1428.072603	179539.301606	36.055527
1429.935572	179855.429119	36.060544
1431.385414	180184.474024	36.065562
1432.344511	180512.145304	36.070580
1433.835772	180841.441022	36.075597
1435.223893	181176.582373	36.080615
1436.254009	181508.931193	36.085632
1437.323873	181840.513676	36.090650
1438.770598	182171.982909	36.095668
1440.688053	182486.606091	36.100685
1441.787690	182813.822978	36.105703
1443.233055	183136.121148	36.110720
1444.837839	183466.086024	36.115738
1445.627368	183803.452968	36.120756
1447.302768	184141.736585	36.125773
1448.281467	184470.748293	36.130791
1449.610335	184808.942903	36.135808
1450.958007	185163.206459	36.140826
1452.298438	185515.328218	36.145844
1453.632588	185862.642269	36.150861
1455.542077	186223.823215	36.155879
1456.527097	186568.979840	36.160896
1458.262800	186928.366989	36.165914
1459.933299	187284.962111	36.170932
1461.195072	187690.032286	36.175949
1462.964593	188072.790663	36.180967
1464.415775	188429.201732	36.185984
1466.208002	188784.388677	36.191002
1467.895737	189147.669309	36.196020
1469.305223	189491.881716	36.201037
1470.961427	189849.421318	36.206055
1472.684926	190200.629529	36.211072
1474.806178	190536.918776	36.216090
1476.461327	190883.661328	36.221108
1478.113829	191218.181056	36.226125
1479.561375	191559.948416	36.231143
1481.140137	191898.876883	36.236160
1483.131068	192230.144949	36.241178
1484.699675	192565.194024	36.246196
1486.395114	192885.318917	36.251213
1487.500299	193212.655811	36.256231
1488.712267	193543.645068	36.261248
1490.560576	193877.853337	36.266266
1491.669216	194220.962517	36.271284
1493.339735	194551.726099	36.276301
1494.870829	194889.218516	36.281319
1496.026876	195225.964315	36.286336
1497.782126	195559.346466	36.291354
1499.070508	195906.889879	36.296372
1500.684104	196232.847165	36.301389
1502.782631	196575.303988	36.306407
1504.144487	196915.819153	36.311424
1505.424959	197250.649394	36.316442
1506.662353	197590.795639	36.321460
1508.581409	197933.734347	36.326477
1509.589750	198265.721344	36.331495
1511.068845	198606.935787	36.336512
1512.809651	198948.094408	36.341530
1514.177226	199291.299197	36.346548
1515.462787	199641.134575	36.351565
1516.721724	199989.528810	36.356583
1518.146861	200345.298444	36.361600
1519.347892	200686.341891	36.366618
1520.916144	201037.697365	36.371636
1522.868124	201370.261019	36.376653
1524.132399	201693.700517	36.381671
1526.276794	202018.692210	36.386688
1528.139289	202345.295291	36.391706
1529.756642	202668.234204	36.396724
1531.407945	202971.767501	36.401741
1533.533478	203296.590189	36.406759
1535.227790	203609.920886	36.411776
1537.370721	203905.399919	36.416794
1538.588447	204213.697630	36.421812
1540.631336	204517.474770	36.426829
1542.199511	204804.230910	36.431847
1543.586175	205112.135034	36.436864
1545.405654	205409.947959	36.441882
1546.283439	205716.824129	36.446900
1548.220949	206011.546297	36.451917
1549.611659	206319.454392	36.456935
1550.525570	206634.327401	36.461952
1552.070239	206955.772712	36.466970
1552.855018	207280.752325	36.471988
1555.049152	207600.349423	36.477005
1556.539059	207925.820406	36.482023
1557.954233	208254.479932	36.487040
1559.190974	208582.460187	36.492058
1560.297482	208925.422299	36.497076
1561.250282	209267.040695	36.502093
1562.586909	209625.076972	36.507111
1563.767287	209985.300161	36.512128
1565.424157	210351.665448	36.517146
1566.931958	210718.616496	36.522164
1568.310625	211084.245131	36.527181
1570.205935	211457.786860	36.532199
1571.552661	211835.411328	36.537216
1572.922801	212225.401720	36.542234
1574.067597	212610.403693	36.547252
1575.668675	213003.989659	36.552269
1576.954339	213392.120026	36.557287
1578.704087	213787.918813	36.562304
1580.946114	214159.939076	36.567322
1583.124307	214536.263913	36.572340
1584.929305	214911.612764	36.577357
1587.028850	215297.909938	36.582375
1588.392631	215665.108262	36.587392
1590.581430	216031.176251	36.592410
1592.143384	216408.553422	36.597428
1593.171395	216785.896370	36.602445
1594.979945	217163.919901	36.607463
1596.202724	217538.362276	36.612480
1597.816251	217916.091742	36.617498
1599.471875	218300.317408	36.622516
1600.995001	218684.008364	36.627533
1602.472299	219060.901656	36.632551
1603.736928	219457.618381	36.637568
1605.263402	219832.397821	36.642586
1606.617651	220214.395934	36.647604
1608.198509	220590.387779	36.652621
1609.931248	220955.560215	36.657639
1610.961331	221347.040740	36.662656
1612.366853	221723.269512	36.667674
1613.959266	222117.628150	36.672692
1615.103184	222507.848517	36.677709
1616.973141	222898.809521	36.682727
1618.330337	223304.997769	36.687744
1620.036480	223701.704329	36.692762
1621.087604	224115.999369	36.697780
1622.466506	224534.659293	36.702797
1624.454302	224959.464834	36.707815
1625.448878	225385.279925	36.712832
1627.509280	225809.974237	36.717850
1629.279796	226239.037569	36.722868
1630.822076	226660.445007	36.727885
1632.617207	227089.710039	36.732903
1634.126465	227529.261745	36.737920
1635.963027	227949.708357	36.742938
1637.584564	228396.279534	36.747956
1639.453900	228841.641262	36.752973
1641.113311	229271.672740	36.757991
1642.435731	229709.586608	36.763008
1644.354862	230155.197761	36.768026
1645.401583	230590.468825	36.773044
1647.229955	231039.527197	36.778061
1649.295486	231478.233364	36.783079
1651.137082	231931.254565	36.788096
1653.207251	232365.440896	36.793114
1654.930013	232809.873765	36.798132
1656.374561	233252.120061	36.803149
1658.519773	233678.016008	36.808167
1659.985283	234127.652777	36.813184
1661.946478	234561.456815	36.818202
1663.465834	234998.715903	36.823220
1664.880826	235436.222480	36.828237
1667.245787	235879.714773	36.833255
1668.428017	236327.500135	36.838272
1670.444098	236768.336106	36.843290
1672.157807	237200.588074	36.848308
1673.790576	237647.664194	36.853325
1676.190731	238079.775114	36.858343
1677.562868	238517.981479	36.863360
1679.053510	238953.501191	36.868378
1680.635443	239389.082318	36.873396
1681.995644	239833.542194	36.878413
1683.438744	240284.440905	36.883431
1684.581164	240739.430861	36.888448
1686.194384	241197.109947	36.893466
1688.329614	241651.449002	36.898484
1690.092773	242107.656057	36.903501
1691.903522	242548.283933	36.908519
1693.551386	243022.039967	36.913536
1694.875212	243471.338624	36.918554
1696.693697	243918.902134	36.923572
1698.241003	244358.841042	36.928589
1700.005967	244792.494219	36.933607
1701.145049	245244.418025	36.938624
1702.792454	245689.828523	36.943642
1704.129206	246152.211010	36.948660
1705.309558	246617.770766	36.953677
1707.228722	247083.788928	36.958695
1708.444814	247560.698736	36.963712
1709.718963	248030.130649	36.968730
1711.791692	248512.407340	36.973748
1713.375439	248989.738358	36.978765
1715.669079	249476.626919	36.983783
1716.733901	249972.998247	36.988800
1718.951486	250450.984160	36.993818
1720.630720	250944.151970	36.998836
1722.400430	251444.188891	37.003853
1724.586311	251919.412285	37.008871
1726.237590	252408.953168	37.013888
1728.550257	252895.180359	37.018906
1730.302353	253390.013736	37.023924
1732.067222	253874.328213	37.028941
1733.902427	254345.827614	37.033959
1735.658753	254836.215214	37.038976
1737.642019	255320.060884	37.043994
1739.757246	255804.290511	37.049012
1741.295245	256290.651198	37.054029
1743.343661	256776.010077	37.059047
1745.469281	257253.988817	37.064064
1747.456749	257734.988741	37.069082
1749.233746	258204.008902	37.074100
1751.105201	258674.054355	37.079117
1752.934900	259147.256844	37.084135
1754.228473	259626.114213	37.089152
1756.020655	260097.290575	37.094170
1757.654545	260580.179287	37.099188
1759.198401	261066.055351	37.104205
1760.578835	261548.961553	37.109223
1762.499602	262041.656858	37.114240
1764.207567	262526.437081	37.119258
1766.039442	263015.184059	37.124276
1767.808841	263508.361492	37.129293
1770.061480	264006.968314	37.134311
1771.545411	264504.410643	37.139328
1773.057650	264999.764613	37.144346
1774.938494	265504.123891	37.149364
1776.278396	266010.505784	37.154381
1778.172805	266509.399991	37.159399
1780.081072	266997.190174	37.164416
1781.472211	267492.638271	37.169434
1783.410759	268007.374426	37.174452
1785.311373	268519.144215	37.179469
1787.198989	269032.642859	37.184487
1788.886709	269542.034265	37.189504
1790.694867	270031.209143	37.194522
1792.520620	270523.479353	37.199540
1793.913646	271016.838872	37.204557
1795.537214	271502.994590	37.209575
1796.924159	271996.251822	37.214592
1798.711990	272494.748679	37.219610
1800.347477	273000.891352	37.224628
1802.400882	273501.754039	37.229645
1804.456242	273991.463761	37.234663
1806.567357	274507.301824	37.239680
1807.917816	275008.611797	37.244698
1810.306283	275507.710916	37.249716
1811.670957	276022.352261	37.254733
1813.553242	276535.684519	37.259751
1815.380770	277045.443196	37.264768
1817.045160	277554.949067	37.269786
1818.762023	278074.554553	37.274804
1820.503018	278603.426129	37.279821
1822.891206	279116.842906	37.284839
1824.293223	279650.951403	37.289856
1825.890667	280165.541922	37.294874
1827.910615	280700.151177	37.299892
1828.988999	281243.861088	37.304909
1831.183271	281782.501306	37.309927
1832.436711	282331.613554	37.314944
1834.404388	282877.883825	37.319962
1835.903857	283430.125306	37.324980
1837.389342	284002.129086	37.329997
1839.620162	284572.682348	37.335015
1841.757305	285134.409973	37.340032
1843.651104	285698.717090	37.345050
1845.577914	286253.922924	37.350068
1847.423615	286832.864372	37.355085
1850.022234	287381.016420	37.360103
1852.103833	287950.565402	37.365120
1853.970704	288510.572809	37.370138
1855.754398	289059.797022	37.375156
1857.354195	289626.423799	37.380173
1860.007874	290181.590246	37.385191
1861.842845	290733.871654	37.390208
1864.031783	291281.314873	37.395226
1866.317598	291826.884832	37.400244
1868.177659	292368.588173	37.405261
1870.400538	292903.699316	37.410279
1872.570934	293448.900311	37.415296
1874.183130	293992.771773	37.420314
1875.700734	294523.169972	37.425332
1877.368003	295076.170159	37.430349
1879.687394	295611.683354	37.435367
1881.274774	296154.506767	37.440384
1882.993642	296693.266525	37.445402
1885.306582	297236.112520	37.450420
1887.002437	297788.407594	37.455437
1889.083789	298322.753593	37.460455
1891.138664	298860.174335	37.465472
1893.439687	299391.302198	37.470490
1895.654324	299896.206362	37.475508
1897.351408	300406.758358	37.480525
1898.969768	300903.047839	37.485543
1900.740550	301411.981691	37.490560
1902.526124	301918.014937	37.495578
1904.370121	302432.213101	37.500596
1906.255276	302958.515429	37.505613
1907.556365	303472.063934	37.510631
1909.031447	304006.226824	37.515648
1910.432457	304542.659334	37.520666
1912.179158	305087.181448	37.525684
1913.793781	305651.074220	37.530701
1915.129798	306200.154409	37.535719
1917.402728	306765.247591	37.540736
1918.876842	307331.844828	37.545754
1920.755047	307907.384225	37.550772
1922.370040	308493.833498	37.555789
1924.023820	309068.666404	37.560807
1926.439777	309661.039291	37.565824
1928.203716	310260.350214	37.570842
1929.837411	310851.908109	37.575860
1932.206058	311446.205177	37.580877
1934.581575	312050.603028	37.585895
1936.484432	312650.074252	37.590912
1938.462390	313243.865008	37.595930
1940.605750	313831.680616	37.600948
1942.622289	314435.815299	37.605965
1945.003741	315041.761467	37.610983
1946.612687	315647.859904	37.616000
1948.403395	316258.924216	37.621018
1950.405651	316853.112027	37.626036
1952.240760	317471.673909	37.631053
1954.189708	318085.284677	37.636071
1956.070030	318700.983607	37.641088
1957.594035	319327.351174	37.646106
1959.979993	319928.733116	37.651124
1961.994372	320546.372181	37.656141
1964.402524	321171.478857	37.661159
1966.682804	321770.906497	37.666176
1969.089232	322386.784825	37.671194
1971.428882	323001.068929	37.676212
1973.251298	323619.827713	37.681229
1974.906196	324216.672736	37.686247
1976.935835	324833.606485	37.691264
1978.461495	325450.899347	37.696282
1980.787458	326059.975456	37.701300
1982.388236	326671.784249	37.706317
1985.003182	327278.335636	37.711335
1986.891976	327889.066843	37.716352
1988.850162	328499.728904	37.721370
1991.050306	329119.888510	37.726388
1993.006620	329743.992534	37.731405
1994.889634	330354.520424	37.736423
1997.129176	330968.179260	37.741440
1998.242730	331589.334917	37.746458
2000.449674	332182.448609	37.751476
2002.291586	332786.686181	37.756493
2004.035054	333377.911308	37.761511
2005.833338	333983.234364	37.766528
2007.764527	334604.748359	37.771546
2009.828546	335197.370587	37.776564
2011.792247	335802.948940	37.781581
2013.788679	336406.204691	37.786599
2016.525496	337019.860733	37.791616
2018.359335	337636.430514	37.796634
2020.463916	338237.793071	37.801652
2022.413422	338855.977967	37.806669
2023.877834	339480.380551	37.811687
2026.307640	340106.133028	37.816704
2027.421876	340737.762500	37.821722
2029.452991	341369.379246	37.826740
2031.368646	342024.179943	37.831757
2032.978005	342676.612930	37.836775
2034.951891	343333.365331	37.841792
2036.923732	344007.899973	37.846810
2039.323829	344648.698864	37.851828
2041.676881	345309.723865	37.856845
2044.528026	345958.624809	37.861863
2047.021808	346595.015488	37.866880
2049.107594	347240.831395	37.871898
2051.884994	347876.724106	37.876916
2053.896882	348506.495934	37.881933
2056.049808	349150.318758	37.886951
2058.471959	349778.834999	37.891968
2060.265389	350413.362326	37.896986
2062.246863	351045.970453	37.902004
2064.409905	351688.180837	37.907021
2066.005500	352329.184534	37.912039
2068.390576	352967.227033	37.917056
2070.348076	353614.746797	37.922074
2072.579093	354248.330444	37.927092
2074.553617	354892.478245	37.932109
2076.067191	355549.711145	37.937127
2078.266000	356187.584084	37.942144
2079.683169	356870.413148	37.947162
2081.588223	357534.879773	37.952180
2083.556838	358213.760813	37.957197
2085.495683	358890.707288	37.962215
2087.664024	359566.410625	37.967232
2089.477931	360266.086844	37.972250
2091.393389	360953.200762	37.977268
2093.303529	361639.517074	37.982285
2095.328651	362338.561966	37.987303
2097.375015	363037.996446	37.992320
2098.975211	363745.333040	37.997338
2101.264447	364463.142125	38.002356
2102.902229	365178.664513	38.007373
2105.202475	365904.333283	38.012391
2107.689832	366622.320881	38.017408
2109.499621	367346.320509	38.022426
2111.750195	368044.662950	38.027444
2113.399417	368736.753838	38.032461
2115.185340	369453.994332	38.037479
2117.934501	370148.964540	38.042496
2119.569167	370856.438133	38.047514
2121.510868	371563.236507	38.052532
2123.221823	372286.291724	38.057549
2125.327305	373008.351642	38.062567
2127.530671	373738.825021	38.067584
2129.258647	374476.845574	38.072602
2131.524671	375209.762545	38.077620
2133.454282	375954.259747	38.082637
2135.255297	376704.595144	38.087655
2137.607860	377462.427002	38.092672
2139.519930	378222.802155	38.097690
2141.869234	378988.765193	38.102708
2143.989279	379743.618462	38.107725
2145.869760	380524.003147	38.112743
2148.365989	381297.874580	38.117760
2150.246125	382079.692862	38.122778
2153.151297	382862.812919	38.127796
2155.320071	383645.456748	38.132813
2157.929862	384426.256741	38.137831
2160.473591	385191.964530	38.142848
2162.265315	385967.339801	38.147866
2164.624633	386736.565477	38.152884
2167.342946	387505.558756	38.157901
2169.334815	388282.033890	38.162919
2172.092027	389036.432008	38.167936
2174.015102	389815.744677	38.172954
2176.507673	390579.782319	38.177972
2178.362199	391351.995471	38.182989
2180.161982	392122.195893	38.188007
2182.362594	392899.075284	38.193024
2184.681490	393696.266145	38.198042
2186.440602	394475.612981	38.203060
2188.753311	395262.701070	38.208077
2190.992662	396064.986268	38.213095
2193.225655	396842.313851	38.218112
2195.381462	397645.811495	38.223130
2197.542656	398442.013047	38.228148
2200.044476	399240.009414	38.233165
2201.735112	400048.637942	38.238183
2204.402864	400837.920390	38.243200
2206.222565	401649.293655	38.248218
2208.732587	402449.047699	38.253236
2211.036584	403248.332629	38.258253
2212.806528	404071.121302	38.263271
2215.443291	404862.195272	38.268288
2217.786343	405674.070650	38.273306
2220.435593	406481.841491	38.278324
2222.816693	407276.207802	38.283341
2224.770051	408078.375412	38.288359
2227.201762	408870.355456	38.293376
2229.551261	409659.185079	38.298394
2231.933429	410438.259086	38.303412
2234.108635	411196.043864	38.308429
2235.940582	411981.118610	38.313447
2238.163937	412737.482872	38.318464
2239.908733	413517.511438	38.323482
2241.831804	414297.308743	38.328500
2244.581873	415062.885589	38.333517
2247.120354	415841.543125	38.338535
2249.532711	416618.780321	38.343552
2251.520282	417403.283340	38.348570
2253.783526	418169.432332	38.353588
2256.209330	418956.774726	38.358605
2258.375526	419744.389913	38.363623
2260.653366	420523.757509	38.368640
2262.812220	421308.842980	38.373658
2265.545462	422104.135009	38.378676
2267.966548	422893.125296	38.383693
2269.768606	423679.866789	38.388711
2271.703726	424472.078851	38.393728
2274.316706	425266.478022	38.398746
2276.557298	426068.205023	38.403764
2279.153928	426867.920513	38.408781
2281.305132	427666.369066	38.413799
2284.099851	428459.010975	38.418816
2286.445355	429269.724130	38.423834
2288.607479	430074.821913	38.428852
2291.260121	430876.062415	38.433869
2293.192602	431684.282176	38.438887
2295.339971	432491.171647	38.443904
2297.191465	433318.176491	38.448922
2299.239687	434131.351876	38.453940
2301.584334	434960.642362	38.458957
2303.601789	435802.559575	38.463975
2306.186324	436628.711629	38.468992
2308.528759	437472.079735	38.474010
2310.990276	438298.748003	38.479028
2314.201521	439123.840680	38.484045
2316.378856	439948.421655	38.489063
2319.511412	440759.400785	38.494080
2322.117576	441569.782271	38.499098
2324.789042	442373.343312	38.504116
2327.543677	443176.405203	38.509133
2329.730349	443990.259102	38.514151
2332.151086	444782.239758	38.519168
2334.508156	445581.132174	38.524186
2336.540819	446398.866849	38.529204
2339.076908	447194.380516	38.534221
2341.537428	448002.521905	38.539239
2343.409229	448800.466014	38.544256
2345.353912	449616.068525	38.549274
2347.386756	450425.858965	38.554292
2349.592539	451251.315888	38.559309
2351.701313	452090.258414	38.564327
2354.492140	452891.529975	38.569344
2356.804020	453700.841450	38.574362
2359.008383	454505.032561	38.579380
2361.480418	455294.685929	38.584397
2363.610292	456091.748708	38.589415
2365.945380	456886.571128	38.594432
2368.498589	457679.707215	38.599450
2370.492980	458475.384612	38.604468
2372.549953	459280.523219	38.609485
2374.775639	460096.266234	38.614503
2377.426000	460895.172255	38.619520
2380.071472	461711.939582	38.624538
2382.154603	462525.180655	38.629556
2384.987414	463334.166115	38.634573
2387.138274	464159.204701	38.639591
2389.609064	464978.948419	38.644608
2391.750272	465805.434804	38.649626
2394.311256	466640.404436	38.654644
2396.822926	467456.296618	38.659661
2399.295477	468283.377789	38.664679
2401.681871	469108.770490	38.669696
2404.190611	469940.825961	38.674714
2406.621947	470780.789816	38.679732
2409.320436	471614.103171	38.684749
2411.790866	472453.025800	38.689767
2414.027967	473295.638176	38.694784
2416.794371	474129.080373	38.699802
2419.170857	474973.865847	38.704820
2421.342837	475818.698149	38.709837
2423.281670	476695.450443	38.714855
2425.594889	477548.714282	38.719872
2428.158125	478410.631973	38.724890
2430.193155	479286.283880	38.729908
2432.513021	480157.401200	38.734925
2435.103193	481031.257818	38.739943
2436.890563	481914.852733	38.744960
2439.461056	482811.851301	38.749978
2441.231485	483708.890965	38.754996
2443.797904	484610.090720	38.760013
2446.282880	485534.378168	38.765031
2448.449394	486432.978642	38.770048
2451.398094	487343.917044	38.775066
2453.470748	488263.386433	38.780084
2455.947976	489185.917604	38.785101
2458.592922	490116.344651	38.790119
2461.044778	491042.111821	38.795136
2463.063462	491975.320884	38.800154
2465.598677	492908.087994	38.805172
2467.900127	493852.549637	38.810189
2470.088435	494808.733489	38.815207
2472.121576	495766.504127	38.820224
2474.335677	496724.441544	38.825242
2476.776721	497702.916968	38.830260
2479.709763	498669.548607	38.835277
2481.824866	499650.840374	38.840295
2484.508027	500631.422067	38.845312
2486.582822	501596.213714	38.850330
2489.202530	502557.426327	38.855348
2491.481108	503503.966694	38.860365
2493.479406	504468.853959	38.865383
2495.563993	505451.820297	38.870400
2497.883485	506421.729466	38.875418
2500.245288	507401.252387	38.880436
2502.953876	508375.715860	38.885453
2505.614002	509362.528395	38.890471
2507.784385	510350.976273	38.895488
2510.885548	511349.686834	38.900506
2513.140662	512351.704163	38.905524
2515.381006	513351.341868	38.910541
2518.173043	514364.225570	38.915559
2520.512463	515363.818144	38.920576
2522.995856	516380.452647	38.925594
2524.904236	517411.326167	38.930612
2527.948302	518443.145582	38.935629
2530.103089	519491.217825	38.940647
2532.479064	520526.486615	38.945664
2534.971371	521582.567721	38.950682
2537.196090	522636.203323	38.955700
2540.241909	523677.991502	38.960717
2543.049900	524747.394242	38.965735
2545.567989	525807.907687	38.970752
2548.702349	526853.789677	38.975770
2551.355369	527921.178152	38.980788
2554.511720	528976.472091	38.985805
2557.303568	530019.369019	38.990823
2560.245949	531067.501525	38.995840
2563.282289	532119.770530	39.000858
2565.947219	533157.733413	39.005876
2568.324877	534182.586386	39.010893
2571.191102	535236.771355	39.015911
2573.948816	536271.726371	39.020928
2577.019001	537298.854998	39.025946
2579.476243	538329.737262	39.030964
2582.398401	539363.835730	39.035981
2584.858950	540387.273139	39.040999
2587.542642	541420.557327	39.046016
2590.672784	542439.958346	39.051034
2593.030253	543464.798283	39.056052
2595.610760	544492.189953	39.061069
2598.022160	545529.943341	39.066087
2600.069538	546576.128181	39.071104
2602.797992	547604.268784	39.076122
2605.022873	548662.984487	39.081140
2607.525526	549697.190063	39.086157
2609.905141	550750.187651	39.091175
2612.265602	551819.290964	39.096192
2615.454695	552862.486451	39.101210
2617.612019	553916.280395	39.106228
2620.744925	554965.252095	39.111245
2623.763840	556015.266296	39.116263
2626.357513	557073.861661	39.121280
2629.118227	558107.576727	39.126298
2631.704656	559144.355193	39.131316
2633.941731	560170.965248	39.136333
2636.255331	561183.016775	39.141351
2638.561825	562206.391602	39.146368
2640.972627	563239.209665	39.151386
2643.156907	564286.646784	39.156404
2645.926536	565322.852838	39.161421
2648.244198	566373.110484	39.166439
2650.245333	567437.443042	39.171456
2652.873246	568507.704087	39.176474
2654.988290	569594.125178	39.181492
2657.486103	570677.828306	39.186509
2660.295570	571774.182484	39.191527
2662.355515	572878.196803	39.196544
2665.116527	573983.499592	39.201562
2667.085873	575117.889265	39.206580
2669.536878	576253.899450	39.211597
2671.916484	577408.026793	39.216615
2674.381704	578569.756107	39.221632
2677.505346	579717.421304	39.226650
2680.204214	580881.349896	39.231668
2683.065800	582054.165706	39.236685
2685.895698	583228.478482	39.241703
2688.466356	584419.967839	39.246720
2691.655216	585589.879466	39.251738
2694.535464	586777.223326	39.256756
2697.005413	587958.004403	39.261773
2699.899132	589154.532590	39.266791
2702.659041	590349.059305	39.271808
2705.319587	591541.528697	39.276826
2708.183450	592741.357807	39.281844
2710.277006	593938.240764	39.286861
2713.218013	595150.684676	39.291879
2715.892355	596359.492458	39.296896
2719.232468	597561.901405	39.301914
2721.650702	598793.234993	39.306932
2724.794480	599999.279826	39.311949
2727.596218	601219.524343	39.316967
2730.378337	602434.336351	39.321984
2733.361748	603649.235022	39.327002
2735.601514	604873.739842	39.332020
2738.541954	606090.736843	39.337037
2741.516385	607310.448894	39.342055
2744.199649	608546.187992	39.347072
2746.728097	609769.111218	39.352090
2749.416140	611009.329745	39.357108
2752.092562	612249.211967	39.362125
2755.059191	613475.403941	39.367143
2757.885099	614717.634380	39.372160
2761.071506	615948.413848	39.377178
2763.581636	617183.069914	39.382196
2766.271783	618413.856782	39.387213
2768.878762	619659.912232	39.392231
2771.059778	620908.845677	39.397248
2774.246574	622137.775657	39.402266
2776.091840	623380.534013	39.407284
2778.822586	624607.460735	39.412301
2781.496787	625824.915492	39.417319
2784.149024	627063.061713	39.422336
2786.821607	628286.727499	39.427354
2789.409600	629539.826417	39.432372
2792.295268	630770.457925	39.437389
2795.333671	632014.896952	39.442407
2797.650413	633270.292498	39.447424
2800.771416	634522.754204	39.452442
2802.925349	635781.817217	39.457460
2805.629932	637062.986762	39.462477
2808.864776	638335.425034	39.467495
2811.682780	639621.495067	39.472512
2814.234586	640914.332107	39.477530
2816.924146	642216.058328	39.482548
2819.231496	643519.528032	39.487565
2821.824888	644831.556159	39.492583
2824.189228	646149.634381	39.497600
2827.444401	647472.023140	39.502618
2830.082659	648819.112589	39.507636
2833.299434	650158.296863	39.512653
2836.348406	651494.638657	39.517671
2838.731053	652841.375794	39.522688
2841.149786	654209.939743	39.527706
2844.038431	655577.485687	39.532724
2846.842064	656953.619493	39.537741
2849.621811	658327.023799	39.542759
2852.001084	659729.724560	39.547776
2854.594954	661122.827344	39.552794
2857.430958	662539.427399	39.557812
2860.152296	663954.245677	39.562829
2863.274895	665367.442785	39.567847
2866.081252	666785.707776	39.572864
2869.290170	668216.674161	39.577882
2872.433129	669640.373314	39.582900
2875.552447	671075.297986	39.587917
2878.577663	672496.794623	39.592935
2881.806678	673921.569683	39.597952
2885.057773	675338.717444	39.602970
2888.325827	676751.123691	39.607988
2891.477061	678168.253068	39.613005
2894.677731	679575.667266	39.618023
2897.615055	680993.142874	39.623040
2900.971388	682398.209216	39.628058
2903.771175	683801.465572	39.633076
2906.851847	685210.960921	39.638093
2910.293859	686609.253919	39.643111
2913.240899	688000.565099	39.648128
2916.187665	689386.549313	39.653146
2919.398570	690791.822964	39.658164
2922.220808	692178.982752	39.663181
2925.664519	693549.004673	39.668199
2928.401287	694944.525903	39.673216
2930.654764	696312.636352	39.678234
2933.620217	697662.514299	39.683252
2935.801731	699014.548814	39.688269
2938.828896	700364.841720	39.693287
2940.957820	701725.782506	39.698304
2943.778867	703073.905368	39.703322
2946.851653	704442.928570	39.708340
2949.501336	705819.533403	39.713357
2952.641286	707195.387947	39.718375
2955.302169	708571.499079	39.723392
2958.413158	709965.431165	39.728410
2961.463185	711354.541363	39.733428
2964.724487	712750.415336	39.738445
2967.796487	714136.094902	39.743463
2970.361356	715537.464836	39.748480
2973.256728	716936.466283	39.753498
2976.579316	718355.191167	39.758516
2979.281662	719767.944884	39.763533
2982.153268	721191.899500	39.768551
2985.385552	722605.907584	39.773568
2988.099735	724026.433674	39.778586
2991.160457	725463.653862	39.783604
2993.773163	726905.984557	39.788621
2997.006624	728350.917871	39.793639
2999.854628	729801.537287	39.798656
3003.157108	731249.251226	39.803674
3006.349016	732705.117385	39.808692
3009.219452	734169.956218	39.813709
3012.963737	735610.194332	39.818727
3016.176981	737067.336623	39.823744
3019.093546	738517.996899	39.828762
3021.923019	739985.473694	39.833780
3024.809315	741449.659746	39.838797
3028.028507	742913.911039	39.843815
3030.709687	744394.446861	39.848832
3033.529960	745865.559863	39.853850
3036.864923	747343.945653	39.858868
3039.719710	748825.186695	39.863885
3042.829026	750311.962809	39.868903
3045.901261	751799.689819	39.873920
3049.014773	753290.125483	39.878938
3052.127630	754781.354231	39.883956
3055.267775	756288.678241	39.888973
3058.759548	757769.756983	39.893991
3061.316530	759270.239851	39.899008
3064.540077	760759.045273	39.904026
3067.991554	762263.157874	39.909044
3070.988290	763769.554345	39.914061
3073.865319	765259.099149	39.919079
3077.083747	766776.699233	39.924096
3080.144725	768281.877190	39.929114
3083.395416	769801.014661	39.934132
3086.090720	771308.733540	39.939149
3089.094528	772813.929311	39.944167
3092.033239	774340.678171	39.949184
3095.030803	775844.170656	39.954202
3098.668539	777326.382293	39.959220
3101.640840	778805.214610	39.964237
3104.474421	780270.226226	39.969255
3107.371724	781743.366188	39.974272
3110.407040	783215.346460	39.979290
3113.128949	784693.844018	39.984308
3115.974170	786178.141893	39.989325
3119.165025	787663.051002	39.994343
3122.164764	789174.094008	39.999360
3124.767518	790686.302164	40.004378
3127.659721	792200.536025	40.009396
3130.204410	793738.693987	40.014413
3133.537674	795269.083737	40.019431
3136.592134	796813.135433	40.024448
3139.859015	798359.988439	40.029466
3143.318237	799918.254272	40.034484
3146.349790	801476.876878	40.039501
3149.665066	803031.625262	40.044519
3153.217877	804601.675129	40.049536
3156.342626	806169.383841	40.054554
3160.035785	807722.608060	40.059572
3163.594768	809297.779608	40.064589
3166.776103	810863.269421	40.069607
3170.239408	812435.428583	40.074624
3173.194249	813996.955139	40.079642
3176.788205	815569.918808	40.084660
3179.450213	817141.596771	40.089677
3183.135783	818710.971713	40.094695
3186.126233	820293.361506	40.099712
3189.197692	821875.358076	40.104730
3192.311236	823452.383872	40.109748
3195.151581	825037.997222	40.114765
3198.454288	826629.189706	40.119783
3201.570033	828226.407706	40.124800
3204.804328	829825.696524	40.129818
3208.046001	831425.026907	40.134836
3210.735160	833048.640502	40.139853
3213.975607	834661.820571	40.144871
3217.038860	836291.947342	40.149888
3220.138605	837932.110615	40.154906
3223.153386	839567.147817	40.159924
3226.204277	841217.364731	40.164941
3229.378334	842863.337939	40.169959
3233.013656	844506.955300	40.174976
3236.084348	846160.829652	40.179994
3239.362521	847806.945414	40.185012
3242.163200	849487.086825	40.190029
3245.649237	851154.034972	40.195047
3248.709430	852826.624652	40.200064
3251.612142	854511.984563	40.205082
3255.050131	856191.843366	40.210100
3257.842697	857878.043410	40.215117
3261.156857	859578.522885	40.220135
3264.239658	861272.944505	40.225152
3267.008071	862963.166924	40.230170
3270.599235	864620.032066	40.235188
3273.484369	866277.142771	40.240205
3276.565116	867941.604978	40.245223
3280.273873	869602.399189	40.250240
3283.129612	871271.488489	40.255258
3286.552301	872942.043511	40.260276
3289.466748	874617.339615	40.265293
3292.881084	876301.163091	40.270311
3296.168655	877996.511512	40.275328
3299.202010	879678.271161	40.280346
3302.558438	881374.271426	40.285364
3305.745945	883078.787618	40.290381
3308.818305	884791.221970	40.295399
3312.041358	886510.651566	40.300416
3314.916529	888244.196903	40.305434
3317.980848	889980.948369	40.310452
3321.105045	891736.062353	40.315469
3324.204259	893497.195402	40.320487
3327.669448	895263.116699	40.325504
3330.556028	897051.129046	40.330522
3333.960602	898834.152511	40.335540
3337.081718	900633.122162	40.340557
3340.574335	902426.927179	40.345575
3344.557431	904229.789698	40.350592
3348.046112	906036.095758	40.355610
3352.093116	907819.506766	40.360628
3356.234699	909617.416728	40.365645
3359.405360	911412.406776	40.370663
3363.153403	913192.206099	40.375680
3366.575711	914986.365605	40.380698
3370.112407	916769.547150	40.385716
3373.152973	918568.733287	40.390733
3376.600921	920362.358984	40.395751
3379.888368	922160.114331	40.400768
3382.809088	923969.314027	40.405786
3385.930969	925783.234697	40.410804
3388.660478	927606.952149	40.415821
3392.042507	929442.765581	40.420839
3395.501376	931280.131549	40.425856
3398.766419	933127.705302	40.430874
3402.101550	934968.782347	40.435892
3405.022727	936835.008925	40.440909
3408.556657	938692.433677	40.445927
3411.825634	940568.258209	40.450944
3415.358682	942444.314390	40.455962
3418.930445	944320.637709	40.460980
3422.551366	946213.069914	40.465997
3425.855340	948086.440906	40.471015
3429.776748	949972.470024	40.476032
3432.937118	951896.272740	40.481050
3436.224852	953836.509285	40.486068
3439.220428	955793.841318	40.491085
3442.388291	957770.712747	40.496103
3445.680068	959742.487794	40.501120
3448.617765	961693.521092	40.506125
3452.029313	963599.466674	40.511130
3455.709491	965470.090766	40.516135
3458.517609	967261.792982	40.521140
3462.221978	968999.186859	40.526144
3465.451427	970657.231505	40.531149
3469.093022	972211.797938	40.536154
3471.934682	973709.302067	40.541159
3475.348181	975118.681632	40.546164
3478.852560	976436.664846	40.551168
3481.373481	977683.517284	40.556173
3484.081625	978839.949200	40.561178
3486.324212	979927.211915	40.566183
3488.982246	980942.656920	40.571188
3491.045486	981880.737492	40.576192
3492.767599	982758.815560	40.581197
3495.273827	983553.606475	40.586202
3497.082914	984294.757869	40.591207
3499.106672	984969.358661	40.596212
3500.995690	985585.878775	40.601216
3502.634583	986123.002118	40.606221
3504.590997	986613.902429	40.611226
3505.814090	987058.088568	40.616231
3507.380311	987441.154622	40.621236
3509.277966	987767.404130	40.626240
3510.765637	988057.346118	40.631245
3512.230066	988295.421996	40.636250
3513.223166	988476.159006	40.641255
3514.053859	988631.186756	40.646260
3515.533174	988731.811674	40.651264
3516.348004	988814.614908	40.656269
3517.238416	988841.850192	40.661274
3518.178262	988851.825950	40.666279
3518.960970	988820.893904	40.671284
3519.905276	988773.365164	40.676288
3520.581513	988688.942306	40.681293
3521.645780	988564.782590	40.686298
3522.390530	988431.902381	40.691303
3522.939788	988265.131857	40.696308
3523.862237	988075.873201	40.701312
3524.600306	987856.518413	40.706317
3525.057945	987621.605575	40.711322
3525.575300	987370.879719	40.716327
3526.074001	987089.143184	40.721332
3526.860796	986787.453852	40.726336
3526.992346	986487.615437	40.731341
3527.751770	986145.530073	40.736346
3528.128677	985818.116735	40.741351
3528.683884	985468.126783	40.746356
3528.680474	985094.413986	40.751360
3529.061275	984714.271353	40.756365
3529.407093	984315.088863	40.761370
3529.623150	983916.680921	40.766375
3530.176644	983502.481201	40.771380
3530.514789	983081.849036	40.776384
3530.257764	982653.579429	40.781389
3530.657791	982208.284673	40.786394
3530.935798	981758.584647	40.791399
3531.309644	981306.783345	40.796404
3531.831035	980833.156183	40.801408
3531.598104	980366.743873	40.806413
3531.912002	979870.524579	40.811418
3532.104560	979401.617916	40.816423
3532.091013	978906.054013	40.821428
3532.726970	978411.117350	40.826432
3532.395364	977911.811021	40.831437
3532.937991	977387.994635	40.836442
3532.922573	976881.512760	40.841447
3532.861640	976358.193310	40.846452
3533.245735	975831.917070	40.851456
3533.340504	975309.451868	40.856461
3533.419920	974770.624957	40.861466
3533.285855	974245.463571	40.866471
3533.284724	973703.911643	40.871476
3533.743309	973156.463806	40.876480
3533.363227	972618.294418	40.881485
3533.572787	972072.544750	40.886490
3533.865270	971517.735016	40.891495
3533.998095	970956.934862	40.896500
3534.488629	970402.667710	40.901504
3534.702838	969832.845763	40.906509
3534.795375	969265.628485	40.911514
3534.504605	968693.334496	40.916519
3534.939774	968100.806796	40.921524
3534.374137	967529.421741	40.926528
3534.404832	966953.083926	40.931533
3534.769138	966362.149839	40.936538
3534.483662	965787.412348	40.941543
3534.504864	965205.812119	40.946548
3534.720648	964617.561992	40.951552
3534.438334	964040.985249	40.956557
3535.036209	963436.397561	40.961562
3535.026165	962855.641622	40.966567
3535.016488	962256.320547	40.971572
3535.492809	961648.921895	40.976576
3534.946765	961055.736732	40.981581
3535.211940	960444.721227	40.986586
3534.938570	959841.177659	40.991591
3534.868476	959242.042684	40.996596
3535.573954	958635.854444	41.001600
3535.453841	958024.745886	41.006605
3535.509802	957399.332430	41.011610
3535.449843	956800.235773	41.016615
3535.153672	956182.787283	41.021620
3535.214200	955558.643674	41.026624
3535.439019	954946.561707	41.031629
3535.169518	954323.419265	41.036634
3535.503488	953709.030266	41.041639
3535.649018	953090.685121	41.046644
3535.803791	952464.229300	41.051648
3535.449899	951845.836135	41.056653
3535.510364	951209.352781	41.061658
3535.567745	950593.261233	41.066663
3535.534248	949973.403556	41.071668
3535.560138	949358.529540	41.076672
3535.487500	948751.155128	41.081677
3535.640680	948127.119231	41.086682
3535.723211	947512.874300	41.091687
3535.688686	946899.819621	41.096692
3535.865077	946277.946585	41.101696
3535.445230	945657.344233	41.106701
3535.718782	945038.558769	41.111706
3535.613252	944427.326851	41.116711
3535.470185	943798.315124	41.121716
3535.803141	943174.986801	41.126720
3535.479980	942555.909185	41.131725
3535.578283	941918.103285	41.136730
3535.963848	941294.634918	41.141735
3535.621317	940669.874481	41.146740
3535.637150	940043.731928	41.151744
3535.412126	939427.904660	41.156749
3535.390553	938793.280502	41.161754
3535.312039	938167.982325	41.166759
3535.297294	937541.351961	41.171764
3535.458173	936917.780264	41.176768
3535.329757	936292.457508	41.181773
3535.520178	935667.676830	41.186778
3536.044912	935040.942215	41.191783
3535.599335	934409.598095	41.196788
3535.651738	933761.784171	41.201792
3535.573103	933134.061404	41.206797
3535.963365	932487.759854	41.211802
3535.932481	931859.397140	41.216807
3535.468322	931215.292678	41.221812
3535.985257	930571.230126	41.226816
3535.862416	929935.838695	41.231821
3535.945489	929290.350205	41.236826
3536.220729	928638.892613	41.241831
3536.024697	928002.417595	41.246836
3536.354758	927348.775541	41.251840
3535.787940	926695.206266	41.256845
3535.633746	926037.259052	41.261850
3535.718064	925391.200715	41.266855
3535.752852	924753.721447	41.271860
3535.668287	924106.191184	41.276864
3535.877853	923455.360382	41.281869
3535.717974	922803.744551	41.286874
3535.691539	922154.911129	41.291879
3535.597247	921510.337939	41.296884
3535.512884	920864.147137	41.301888
3535.352084	920223.758754	41.306893
3535.919095	919565.374886	41.311898
3535.652465	918914.749225	41.316903
3535.630036	918272.951425	41.321908
3535.802994	917607.853947	41.326912
3535.743759	916956.668848	41.331917
3535.791044	916296.340077	41.336922
3535.766697	915642.392718	41.341927
3536.030183	914976.668749	41.346932
3536.048414	914316.489747	41.351936
3535.921150	913661.648207	41.356941
3535.793241	912993.052708	41.361946
3536.069678	912335.864663	41.366951
3535.557100	911666.980174	41.371956
3535.872751	911000.473921	41.376960
3535.736563	910344.755478	41.381965
3535.937023	909690.057728	41.386970
3535.666748	909030.254521	41.391975
3535.755880	908364.816853	41.396980
3535.830818	907693.710191	41.401984
3535.632564	907040.693969	41.406989
3536.052755	906370.331879	41.411994
3536.031083	905702.857146	41.416999
3535.967900	905031.162007	41.422004
3535.686142	904358.651289	41.427008
3535.796873	903687.342818	41.432013
3535.877813	903012.388723	41.437018
3535.739198	902348.583556	41.442023
3535.715888	901675.415404	41.447028
3535.840713	901006.001545	41.452032
3535.417723	900332.064383	41.457037
3535.501656	899664.041601	41.462042
3535.767916	898992.818594	41.467047
3535.216711	898325.227768	41.472052
3535.301636	897654.069087	41.477056
3535.633941	896989.838936	41.482061
3535.432651	896314.609745	41.487066
3535.594535	895646.676654	41.492071
3535.600298	894975.309706	41.497076
3535.430316	894294.230144	41.502080
3535.347449	893626.197271	41.507085
3535.379087	892950.334015	41.512090
3535.799996	892273.647355	41.517095
3535.640543	891596.592682	41.522100
3535.451426	890918.979255	41.527104
3535.353014	890240.786446	41.532109
3535.568540	889570.486618	41.537114
3535.529781	888895.218919	41.542119
3535.514228	888214.257189	41.547124
3535.476943	887532.831431	41.552128
3534.968585	886852.759916	41.557133
3535.372918	886177.290655	41.562138
3535.406325	885501.708809	41.567143
3535.056951	884840.051066	41.572148
3535.543789	884152.522417	41.577152
3535.201991	883487.901466	41.582157
3535.066685	882798.188401	41.587162
3535.277477	882116.081164	41.592167
3534.892092	881443.196123	41.597172
3535.286125	880767.291337	41.602176
3535.181950	880090.327658	41.607181
3535.057362	879410.576270	41.612186
3534.876269	878734.921808	41.617191
3534.949331	878058.855232	41.622196
3535.222425	877378.606110	41.627200
3534.980476	876708.737082	41.632205
3535.237408	876021.548735	41.637210
3535.495636	875340.581536	41.642215
3535.330089	874661.353244	41.647220
3535.431167	873961.831379	41.652224
3535.621116	873275.304092	41.657229
3535.797727	872584.431724	41.662234
3534.633638	871895.550740	41.667239
3534.817633	871211.501434	41.672244
3535.353039	870529.933109	41.677248
3535.096991	869843.472887	41.682253
3535.133826	869160.765524	41.687258
3534.949075	868472.679544	41.692263
3534.763269	867794.706973	41.697268
3534.902368	867109.612169	41.702272
3535.149834	866423.352492	41.707277
3534.750501	865734.017378	41.712282
3535.034123	865042.738479	41.717287
3534.846901	864371.177263	41.722292
3534.913306	863676.087705	41.727296
3535.112784	862995.759120	41.732301
3534.819082	862296.977733	41.737306
3534.940432	861618.159173	41.742311
3534.863811	860929.288610	41.747316
3535.250937	860234.720651	41.752320
3534.814003	859543.130082	41.757325
3534.825868	858849.828817	41.762330
3535.031041	858161.860319	41.767335
3534.638306	857476.638944	41.772340
3535.396741	856771.402820	41.777344
3534.427855	856086.415704	41.782349
3534.276251	855390.707279	41.787354
3535.038563	854710.037082	41.792359
3534.723979	854026.556575	41.797364
3535.034748	853328.200666	41.802368
3534.815990	852637.349163	41.807373
3534.984265	851933.604688	41.812378
3534.877008	851244.038125	41.817383
3535.016783	850551.724183	41.822388
3534.598878	849855.241720	41.827392
3534.640629	849168.728911	41.832397
3534.923147	848468.660840	41.837402
3534.747249	847775.409585	41.842407
3534.598294	847076.037747	41.847412
3534.733767	846373.226971	41.852416
3534.488980	845685.502610	41.857421
3534.878268	844986.681889	41.862426
3534.523084	844285.864021	41.867431
3534.198149	843595.195526	41.872436
3534.588427	842894.874852	41.877440
3534.266522	842214.678046	41.882445
3534.160159	841517.895716	41.887450
3534.351712	840824.398052	41.892455
3534.209608	840139.218265	41.897460
3534.487298	839442.872997	41.902464
3534.522613	838746.492637	41.907469
3534.601155	838051.394094	41.912474
3534.270643	837349.558358	41.917479
3533.995970	836661.977342	41.922484
3534.123761	835960.349399	41.927488
3534.192614	835283.538142	41.932493
3534.222522	834584.557001	41.937498
3534.305712	833883.733609	41.942503
3534.168905	833190.875624	41.947508
3534.217153	832490.296534	41.952512
3534.399951	831797.966063	41.957517
3534.192809	831100.061915	41.962522
3534.250376	830400.425741	41.967527
3534.121655	829704.163980	41.972532
3534.447990	829000.570274	41.977536
3533.770372	828315.046288	41.982541
3533.686689	827618.308498	41.987546
3533.936638	826928.327579	41.992551
3534.068299	826230.671576	41.997556
3534.028948	825536.488392	42.002560
3533.858513	824846.163390	42.007565
3534.132167	824142.200044	42.012570
3533.914675	823447.238921	42.017575
3533.465323	822756.301241	42.022580
3533.759886	822054.701170	42.027584
3533.631351	821362.437672	42.032589
3533.642366	820672.473751	42.037594
3533.992140	819975.924170	42.042599
3533.730325	819289.872641	42.047604
3533.854277	818582.307485	42.052608
3533.595030	817899.242077	42.057613
3533.890766	817196.196177	42.062618
3533.670938	816503.488599	42.067623
3533.697442	815803.815642	42.072628
3533.609442	815107.759456	42.077632
3533.502735	814414.521772	42.082637
3533.356550	813715.638336	42.087642
3533.336377	813020.577035	42.092647
3533.585460	812332.252489	42.097652
3533.570640	811634.647535	42.102656
3533.215970	810952.503623	42.107661
3533.370806	810259.036703	42.112666
3533.169197	809566.245089	42.117671
3533.054687	808870.771186	42.122676
3533.189057	808177.877896	42.127680
3533.156814	807497.191635	42.132685
3533.247858	806798.922056	42.137690
3533.529786	806096.186437	42.142695
3533.460861	805407.259782	42.147700
3533.403971	804706.644205	42.152704
3533.334376	804019.391137	42.157709
3532.999015	803322.750038	42.162714
3533.431962	802628.162390	42.167719
3533.047834	801937.664962	42.172724
3533.379993	801240.649310	42.177728
3533.161173	800544.834223	42.182733
3533.061491	799848.192705	42.187738
3533.169755	799162.139862	42.192743
3532.859628	798461.322540	42.197748
3532.998821	797767.030679	42.202752
3532.829043	797073.507155	42.207757
3532.909925	796383.454161	42.212762
3532.815541	795691.890116	42.217767
3532.478944	795007.956256	42.222772
3532.951600	794310.807843	42.227776
3532.929629	793619.173091	42.232781
3532.880127	792930.960829	42.237786
3532.584201	792235.160634	42.242791
3532.663202	791544.040290	42.247796
3532.763040	790855.058611	42.252800
3532.394706	790177.338021	42.257805
3532.539410	789482.565496	42.262810
3532.805685	788789.816418	42.267815
3532.355997	788118.200606	42.272820
3532.613098	787418.734717	42.277824
3532.735979	786726.594428	42.282829
3532.626532	786036.932946	42.287834
3532.689767	785349.092100	42.292839
3532.633183	784650.685259	42.297844
3532.604037	783964.053804	42.302848
3532.213055	783272.894617	42.307853
3532.303901	782579.226078	42.312858
3532.441394	781890.154329	42.317863
3532.321884	781200.371733	42.322868
3532.434954	780522.780064	42.327872
3532.511187	779839.473828	42.332877
3532.657390	779133.607988	42.337882
3532.780048	778443.126449	42.342887
3532.408083	777745.430111	42.347892
3532.658661	777041.458116	42.352896
3532.505252	776355.598161	42.357901
3532.333645	775656.731613	42.362906
3532.569676	774954.184144	42.367911
3532.270724	774265.001571	42.372916
3532.574495	773565.853373	42.377920
3532.441932	772883.109448	42.382925
3532.354643	772191.331776	42.387930
3532.303621	771485.840844	42.392935
3532.329722	770798.985176	42.397940
3532.076353	770107.187324	42.402944
3532.096321	769415.228589	42.407949
3531.632476	768720.972021	42.412954
3531.963256	768034.250213	42.417959
3531.402731	767342.492154	42.422964
3531.790907	766654.548605	42.427968
3531.550343	765971.182915	42.432973
3531.640251	765293.366335	42.437978
3531.647708	764614.812042	42.442983
3531.618342	763936.744607	42.447988
3531.657075	763242.876298	42.452992
3531.767065	762568.999751	42.457997
3531.441205	761885.619787	42.463002
3531.603179	761188.285652	42.468007
3531.303321	760510.348948	42.473012
3531.361716	759824.003342	42.478016
3531.586047	759147.383657	42.483021
3531.389961	758473.883224	42.488026
3531.675608	757795.010677	42.493031
3531.350382	757113.961157	42.498036
3531.695912	756425.185800	42.503040
3531.627928	755752.310064	42.508045
3531.674591	755059.859430	42.513050
3531.283141	754373.788302	42.518055
3531.286180	753684.280705	42.523060
3531.537213	753008.442851	42.528064
3531.315517	752336.131669	42.533069
3531.325751	751644.563083	42.538074
3531.232380	750963.369799	42.543079
3531.257542	750286.491488	42.548084
3531.258531	749598.790483	42.553088
3531.223057	748924.124452	42.558093
3531.188491	748243.174970	42.563098
3531.062195	747563.119990	42.568103
3531.037320	746885.162100	42.573108
3531.120714	746201.542874	42.578112
3531.008563	745522.641110	42.583117
3530.901923	744839.972637	42.588122
3531.224377	744172.097992	42.593127
3530.914137	743488.357701	42.598132
3530.970727	742798.562915	42.603136
3530.644016	742134.876842	42.608141
3530.718241	741448.470646	42.613146
3531.257008	740774.188336	42.618151
3531.003627	740094.296640	42.623156
3531.360230	739403.807010	42.628160
3531.182028	738726.504920	42.633165
3531.063733	738048.095942	42.638170
3530.883450	737360.537258	42.643175
3530.646855	736683.367565	42.648180
3531.120254	735995.232980	42.653184
3530.961513	735322.486275	42.658189
3530.882686	734641.553582	42.663194
3531.122785	733956.450298	42.668199
3530.992846	733275.410156	42.673204
3531.135485	732593.671711	42.678208
3531.038976	731910.084686	42.683213
3530.772774	731226.419094	42.688218
3530.873189	730551.396421	42.693223
3530.165770	729870.364892	42.698228
3530.800698	729180.281932	42.703232
3530.110727	728504.233033	42.708237
3530.254968	727834.473533	42.713242
3530.772640	727157.462553	42.718247
3530.844902	726489.437346	42.723252
3530.770012	725797.652924	42.728256
3530.722544	725131.072770	42.733261
3530.776295	724439.399223	42.738266
3530.157183	723766.612095	42.743271
3529.813489	723096.993535	42.748276
3530.316343	722412.654731	42.753280
3530.260129	721742.976081	42.758285
3529.861722	721069.881279	42.763290
3530.150796	720401.224540	42.768295
3529.934647	719734.037780	42.773300
3529.932032	719061.356608	42.778304
3529.978913	718393.521382	42.783309
3529.923306	717728.823715	42.788314
3529.754682	717060.968002	42.793319
3529.486317	716401.904037	42.798324
3529.838211	715728.050132	42.803329
3529.954540	715065.591226	42.808333
3529.778996	714403.973174	42.813338
3529.464755	713729.030646	42.818343
3529.897681	713070.478205	42.823348
3529.792666	712408.343910	42.828353
3529.820285	711739.932065	42.833357
3529.650745	711068.573014	42.838362
3529.910861	710400.611257	42.843367
3529.207785	709740.603786	42.848372
3529.772728	709076.704895	42.853377
3529.549387	708419.143876	42.858381
3529.353010	707756.066361	42.863386
3529.738860	707084.099392	42.868391
3529.612426	706424.332564	42.873396
3529.559328	705763.062318	42.878401
3529.344633	705103.208931	42.883405
3529.226999	704440.258685	42.888410
3529.575097	703772.161209	42.893415
3529.200739	703115.709380	42.898420
3529.310492	702456.690816	42.903425
3529.230289	701810.323286	42.908429
3529.079570	701147.126006	42.913434
3529.342427	700482.217419	42.918439
3529.217147	699832.828429	42.923444
3528.984221	699170.190146	42.928449
3529.183806	698515.429453	42.933453
3528.798478	697868.423692	42.938458
3529.111157	697209.171996	42.943463
3528.735741	696561.222996	42.948468
3529.086746	695900.176275	42.953473
3528.913477	695248.914290	42.958477
3529.068012	694596.653216	42.963482
3528.709378	693932.447571	42.968487
3528.816380	693287.755829	42.973492
3528.793085	692627.820982	42.978497
3528.837837	691982.895793	42.983501
3528.858360	691326.587058	42.988506
3529.029248	690673.437662	42.993511
3528.414229	690026.045880	42.998516
3528.737813	689368.596101	43.003521
3528.890765	688724.959127	43.008525
3528.587981	688079.214110	43.013530
3528.550940	687420.488798	43.018535
3528.162522	686774.614873	43.023540
3528.481985	686124.393132	43.028545
3528.245509	685489.101637	43.033549
3528.234181	684841.481982	43.038554
3528.837419	684191.520749	43.043559
3528.284553	683552.065350	43.048564
3528.491556	682903.423694	43.053569
3528.415928	682259.663560	43.058573
3528.441814	681611.608100	43.063578
3528.310488	680959.001867	43.068583
3528.257575	680321.724324	43.073588
3528.393271	679675.455169	43.078593
3528.065090	679034.200535	43.083597
3528.020945	678385.281255	43.088602
3528.334163	677746.816093	43.093607
3527.937879	677106.684205	43.098612
3528.273888	676456.916697	43.103617
3528.144573	675821.233883	43.108621
3528.223856	675175.057559	43.113626
3528.260316	674524.408469	43.118631
3527.914777	673887.882710	43.123636
3527.971384	673240.080742	43.128641
3527.677912	672615.620086	43.133645
3527.777282	671964.532408	43.138650
3528.027739	671325.636722	43.143655
3527.631889	670702.212480	43.148660
3527.888771	670056.200027	43.153665
3527.681581	669424.681835	43.158669
3527.782024	668788.331812	43.163674
3527.647650	668143.651280	43.168679
3527.235244	667518.174213	43.173684
3527.638261	666879.749094	43.178689
3527.879806	666253.378745	43.183693
3527.564030	665619.879587	43.188698
3527.863819	664985.085882	43.193703
3527.534556	664353.051211	43.198708
3527.529365	663718.424919	43.203713
3527.147840	663092.302629	43.208717
3527.176221	662462.427039	43.213722
3527.203785	661826.921528	43.218727
3527.272056	661209.232331	43.223732
3527.090376	660572.132755	43.228737
3526.957012	659956.044642	43.233741
3526.930475	659339.050530	43.238746
3527.094917	658715.994635	43.243751
3526.800802	658094.524513	43.248756
3526.864233	657460.622846	43.253761
3526.704087	656842.594348	43.258765
3526.724547	656223.097855	43.263770
3527.087685	655600.607545	43.268775
3526.981444	654977.458697	43.273780
3527.174756	654360.061843	43.278785
3527.098226	653748.165769	43.283789
3526.710886	653117.156050	43.288794
3527.215281	652492.946321	43.293799
3526.936792	651878.571151	43.298804
3526.595118	651258.523824	43.303809
3526.820382	650638.191015	43.308813
3526.692721	650022.975592	43.313818
3526.934705	649404.461345	43.318823
3526.405163	648783.492124	43.323828
3526.815636	648168.120175	43.328833
3526.523600	647557.277797	43.333837
3526.674757	646933.428825	43.338842
3526.415798	646298.315909	43.343847
3526.193511	645681.899678	43.348852
3526.510740	645068.452613	43.353857
3526.550643	644461.064065	43.358861
3526.542100	643845.298799	43.363866
3526.475243	643224.006677	43.368871
3526.309611	642623.491974	43.373876
3526.540204	642003.924182	43.378881
3526.405220	641392.631505	43.383885
3526.124752	640782.277074	43.388890
3526.142728	640167.884468	43.393895
3525.886962	639558.052725	43.398900
3526.132841	638953.600620	43.403905
3526.009009	638349.626163	43.408909
3525.893971	637749.666351	43.413914
3526.544312	637139.186010	43.418919
3526.302219	636528.271589	43.423924
3526.583896	635911.778377	43.428929
3526.491070	635309.571605	43.433933
3525.820577	634698.772335	43.438938
3526.000038	634087.992147	43.443943
3525.999547	633485.563686	43.448948
3525.936507	632876.505233	43.453953
3525.714412	632267.038000	43.458957
3525.952048	631669.518765	43.463962
3525.902713	631063.905875	43.468967
3525.563967	630464.364157	43.473972
3525.607046	629855.462202	43.478977
3525.581202	629264.308583	43.483981
3525.193223	628670.680431	43.488986
3525.319513	628076.029897	43.493991
3525.318953	627490.730645	43.498996
3525.315170	626888.725450	43.504001
3525.023417	626300.756393	43.509005
3525.233424	625712.068218	43.514010
3525.099943	625123.406155	43.519015
3524.956800	624539.571378	43.524020
3524.986779	623958.379815	43.529025
3525.082602	623372.937979	43.534029
3525.381447	622787.028793	43.539034
3525.301045	622194.489827	43.544039
3525.157680	621604.784535	43.549044
3525.064709	621014.938182	43.554049
3524.947412	620430.224354	43.559053
3524.899674	619839.554597	43.564058
3524.947627	619251.091180	43.569063
3525.034358	618672.561324	43.574068
3525.166739	618084.070407	43.579073
3525.045201	617499.901059	43.584077
3524.719554	616908.367793	43.589082
3524.723564	616329.577388	43.594087
3524.568168	615754.192062	43.599092
3524.808511	615173.846680	43.604097
3524.743941	614600.841629	43.609101
3524.634049	614019.642944	43.614106
3524.792439	613437.214721	43.619111
3524.815992	612859.892838	43.624116
3524.777408	612271.069361	43.629121
3524.843838	611702.705064	43.634125
3524.958853	611115.348458	43.639130
3525.203907	610533.755808	43.644135
3524.999382	609952.360018	43.649140
3524.773016	609367.426953	43.654145
3524.444704	608775.709658	43.659149
3524.470800	608207.625548	43.664154
3524.530706	607628.872789	43.669159
3524.382463	607051.831339	43.674164
3524.515112	606470.799408	43.679169
3524.507819	605899.995867	43.684173
3524.084433	605327.729404	43.689178
3524.482033	604750.176121	43.694183
3524.171264	604184.555984	43.699188
3524.146208	603610.579407	43.704193
3524.181542	603047.151833	43.709197
3524.024384	602473.491793	43.714202
3524.257424	601906.511475	43.719207
3524.128655	601343.479564	43.724212
3524.147211	600770.808317	43.729217
3523.937797	600203.066421	43.734221
3523.686023	599635.404126	43.739226
3524.106608	599074.375896	43.744231
3523.541301	598516.350191	43.749236
3523.857123	597937.764474	43.754241
3523.677055	597383.785288	43.759245
3523.843730	596824.147324	43.764250
3524.037362	596254.084175	43.769255
3523.724083	595701.453470	43.774260
3523.464982	595138.693989	43.779265
3523.563216	594582.676058	43.784269
3523.282372	594038.799564	43.789274
3523.726318	593478.351261	43.794279
3523.365903	592924.542831	43.799284
3523.663590	592372.454399	43.804289
3523.262109	591815.788110	43.809293
3523.274583	591264.449987	43.814298
3523.539769	590707.969336	43.819303
3523.079324	590166.406338	43.824308
3523.547607	589610.944770	43.829313
3523.805277	589059.311587	43.834317
3523.661702	588503.701865	43.839322
3523.483441	587950.936236	43.844327
3523.176984	587400.428124	43.849332
3522.993672	586839.622510	43.854337
3522.854313	586291.698253	43.859341
3522.619913	585759.243920	43.864346
3522.907829	585212.152407	43.869351
3522.646313	584681.213067	43.874356
3522.822700	584131.076025	43.879361
3522.778372	583597.136811	43.884365
3522.594099	583052.843059	43.889370
3522.475359	582517.511859	43.894375
3522.280683	581987.347991	43.899380
3522.635652	581443.644267	43.904385
3522.818971	580910.805154	43.909389
3522.497731	580392.207273	43.914394
3522.815066	579844.366422	43.919399
3522.480415	579304.557011	43.924404
3522.525953	578770.190259	43.929409
3522.391154	578239.904319	43.934413
3522.627341	577708.727637	43.939418
3522.542522	577174.666082	43.944423
3522.665441	576647.989376	43.949428
3522.685996	576101.441250	43.954433
3522.545898	575577.228498	43.959437
3522.196784	575038.744346	43.964442
3522.436316	574501.192773	43.969447
3522.199307	573980.249347	43.974452
3522.074183	573447.091144	43.979457
3522.266619	572921.050083	43.984461
3522.270932	572391.598035	43.989466
3522.207311	571866.311215	43.994471
3522.057341	571350.526628	43.999476
3522.166793	570813.191641	44.004481
3522.069393	570292.977405	44.009485
3521.900705	569773.508791	44.014490
3521.949062	569244.370265	44.019495
3522.056462	568735.329473	44.024500
3522.129757	568199.802379	44.029505
3521.855056	567682.027940	44.034509
3521.805466	567167.868237	44.039514
3521.842387	566649.847836	44.044519
3521.499585	566132.576039	44.049524
3521.709693	565606.581426	44.054529
3521.599702	565094.664520	44.059533
3521.709173	564585.106187	44.064538
3522.231690	564068.459589	44.069543
3521.941781	563547.903499	44.074548
3522.055182	563031.084012	44.079553
3521.700344	562514.726699	44.084557
3521.637148	562001.571906	44.089562
3521.770275	561472.200130	44.094567
3521.547947	560965.678345	44.099572
3521.545255	560445.553469	44.104577
3521.646584	559931.987197	44.109581
3521.470426	559426.153411	44.114586
3521.212688	558919.004669	44.119591
3521.160549	558406.764840	44.124596
3521.628837	557898.042673	44.129601
3521.236801	557404.054686	44.134605
3521.332406	556880.850934	44.139610
3521.380622	556376.473921	44.144615
3521.242185	555870.396916	44.149620
3521.579194	555363.715742	44.154625
3521.505924	554857.337269	44.159629
3521.535266	554348.856511	44.164634
3521.473400	553837.953684	44.169639
3521.584917	553339.043529	44.174644
3521.228040	552826.137213	44.179649
3521.106187	552319.469678	44.184653
3520.780029	551817.252265	44.189658
3520.909720	551311.410953	44.194663
3520.730642	550817.546653	44.199668
3520.749618	550319.548548	44.204673
3520.555136	549815.672189	44.209677
3520.666794	549325.382968	44.214682
3520.359405	548830.057202	44.219687
3520.478850	548346.938770	44.224692
3520.637242	547849.935484	44.229697
3520.545184	547361.576360	44.234701
3520.244892	546874.142755	44.239706
3520.593388	546386.681917	44.244711
3520.094807	545910.943064	44.249716
3520.385000	545421.239956	44.254721
3520.332291	544941.610604	44.259725
3520.146726	544453.668587	44.264730
3520.087105	543970.780158	44.269735
3520.130754	543498.848897	44.274740
3520.249403	543010.400904	44.279745
3520.120749	542525.507679	44.284749
3520.029606	542056.374341	44.289754
3520.158261	541572.715202	44.294759
3519.839141	541104.345306	44.299764
3519.885887	540627.072001	44.304769
3519.985360	540149.370047	44.309773
3520.064085	539684.465632	44.314778
3520.153310	539202.345620	44.319783
3519.839099	538731.777737	44.324788
3519.811156	538251.915031	44.329793
3519.567103	537779.689526	44.334797
3519.441863	537305.006822	44.339802
3519.569704	536827.490670	44.344807
3519.653134	536372.464852	44.349812
3519.621352	535897.769818	44.354817
3519.777890	535433.671605	44.359821
3519.490851	534970.996275	44.364826
3519.650105	534503.436894	44.369831
3519.269095	534034.037327	44.374836
3519.728311	533570.432752	44.379841
3519.616170	533103.378865	44.384845
3519.191277	532651.097214	44.389850
3519.651238	532186.691304	44.394855
3519.466911	531732.876604	44.399860
3519.458673	531260.447151	44.404865
3519.318119	530797.209609	44.409869
3519.176947	530340.467662	44.414874
3519.630492	529870.740516	44.419879
3519.272038	529416.227423	44.424884
3519.434157	528954.141606	44.429889
3518.939351	528492.052481	44.434893
3518.925757	528049.652695	44.439898
3519.373617	527588.535203	44.444903
3519.080821	527130.356531	44.449908
3519.188280	526669.672335	44.454913
3519.223178	526216.255444	44.459917
3518.994095	525767.160777	44.464922
3519.117272	525313.398386	44.469927
3518.929196	524873.457813	44.474932
3518.965806	524407.313750	44.479937
3518.768187	523953.059928	44.484941
3518.766052	523513.905923	44.489946
3518.594374	523064.164835	44.494951
3518.840938	522613.430013	44.499956
3518.771626	522173.389953	44.504961
3518.713117	521732.022325	44.509965
3518.517445	521279.404325	44.514970
3518.572554	520835.264281	44.519975
3518.560099	520398.344311	44.524980
3518.690399	519960.932889	44.529985
3518.452127	519522.511263	44.534989
3517.857396	519085.653029	44.539994
3518.064719	518649.908007	44.544999
3518.403225	518219.431466	44.550004
3517.908977	517778.124586	44.555009
3518.179648	517352.989264	44.560013
3517.928700	516919.394770	44.565018
3517.971259	516482.505114	44.570023
3517.614022	516074.919288	44.575028
3517.656921	515635.227311	44.580033
3517.764006	515221.225222	44.585037
3517.428686	514791.879423	44.590042
3517.919335	514367.281183	44.595047
3517.979356	513942.845933	44.600052
3517.875563	513516.810369	44.605057
3517.741186	513095.265060	44.610061
3517.308601	512673.355104	44.615066
3517.629839	512252.366144	44.620071
3517.193625	511845.441021	44.625076
3517.457507	511427.976744	44.630081
3517.465308	511019.236441	44.635085
3517.346090	510612.983315	44.640090
3517.317648	510187.552047	44.645095
3517.408228	509790.388540	44.650100
3517.361839	509364.685569	44.655105
3517.312791	508953.475902	44.660109
3516.994899	508544.828450	44.665114
3517.389103	508129.680886	44.670119
3517.007628	507736.286671	44.675124
3517.247763	507322.761774	44.680129
3517.290492	506911.130035	44.685133
3517.195263	506507.446890	44.690138
3517.252670	506089.271250	44.695143
3517.121038	505699.221590	44.700148
3517.215605	505288.499888	44.705153
3517.225527	504883.747132	44.710157
3516.970157	504472.255639	44.715162
3516.913480	504070.324813	44.720167
3516.780174	503674.969149	44.725172
3517.357179	503267.298769	44.730177
3517.303442	502871.050555	44.735181
3516.944189	502463.621055	44.740186
3517.061887	502058.071766	44.745191
3516.835328	501664.402321	44.750196
3516.493094	501262.906144	44.755201
3516.745813	500871.512243	44.760205
3516.780781	500470.994142	44.765210
3516.787724	500068.145099	44.770215
3516.489501	499683.997328	44.775220
3516.193201	499283.860958	44.780225
3516.535845	498896.804279	44.785229
3516.366673	498500.875083	44.790234
3516.445058	498119.256393	44.795239
3516.502499	497733.081028	44.800244
3516.431683	497334.275250	44.805249
3516.222644	496957.230663	44.810253
3516.052885	496572.331625	44.815258
3516.335917	496177.837965	44.820263
3516.156417	495799.851913	44.825268
3515.983664	495417.202920	44.830273
3516.072664	495033.236030	44.835277
3515.908981	494656.789620	44.840282
3516.092994	494273.699708	44.845287
3516.099433	493896.145087	44.850292
3515.977570	493514.860679	44.855297
3515.837672	493145.863209	44.860301
3515.584896	492768.074840	44.865306
3515.992276	492395.072442	44.870311
3515.958187	492026.943266	44.875316
3515.930944	491653.998899	44.880321
3516.018764	491272.476782	44.885325
3515.748107	490898.899853	44.890330
3516.064225	490518.030289	44.895335
3516.241036	490150.431957	44.900340
3516.006197	489778.494221	44.905345
3515.728013	489399.978249	44.910349
3515.674379	489027.791025	44.915354
3515.981989	488655.888320	44.920359
3515.714125	488291.817760	44.925364
3515.731777	487922.782485	44.930369
3515.835163	487548.411487	44.935373
3515.786787	487188.530986	44.940378
3515.993214	486811.697622	44.945383
3515.546252	486445.999750	44.950388
3515.873659	486072.216764	44.955393
3515.666797	485702.363239	44.960397
3515.480225	485341.000764	44.965402
3515.612016	484967.075860	44.970407
3515.479402	484610.598362	44.975412
3515.230236	484240.114043	44.980417
3515.496060	483889.020068	44.985421
3515.320641	483530.706056	44.990426
3515.453568	483165.195436	44.995431
3514.961979	482807.629439	45.000436
3514.989859	482449.258925	45.005441
3515.141753	482100.781196	45.010445
3515.335598	481748.898029	45.015450
3515.179160	481380.464349	45.020455
3514.784800	481024.668396	45.025460
3515.051237	480675.586557	45.030465
3515.189723	480316.040802	45.035469
3515.069890	479975.516033	45.040474
3515.247656	479613.013356	45.045479
3514.553535	479264.169456	45.050484
3514.914918	478917.366202	45.055489
3515.186621	478562.268630	45.060493
3514.768909	478218.977139	45.065498
3514.692108	477864.583621	45.070503
3514.811361	477523.718838	45.075508
3514.894396	477175.613510	45.080513
3514.550977	476827.321205	45.085517
3514.593681	476498.804803	45.090522
3514.596022	476147.098702	45.095527
3514.340797	475802.164396	45.100532
3514.272668	475468.635559	45.105537
3514.308103	475132.500487	45.110541
3514.013105	474809.581713	45.115546
3514.311059	474460.476784	45.120551
3514.210759	474138.424560	45.125556
3514.187397	473799.186247	45.130561
3514.469098	473467.840462	45.135565
3513.975678	473137.279484	45.140570
3514.243179	472805.873702	45.145575
3514.075011	472483.348617	45.150580
3513.821863	472149.335909	45.155585
3514.314709	471828.915085	45.160589
3513.862270	471503.939981	45.165594
3514.265360	471175.014550	45.170599
3514.122016	470844.302649	45.175604
3514.089584	470508.349044	45.180609
3514.083630	470186.871117	45.185613
3513.820929	469857.529873	45.190618
3514.048606	469541.674094	45.195623
3513.725371	469220.689803	45.200628
3513.656354	468892.767677	45.205633
3513.829414	468573.359305	45.210637
3513.572326	468255.133458	45.215642
3513.765185	467938.091897	45.220647
3513.666386	467617.700802	45.225652
3513.704934	467300.067117	45.230657
3513.502014	466987.383365	45.235661
3513.337089	466672.053695	45.240666
3513.496509	466353.370496	45.245671
3513.472504	466047.480158	45.250676
3513.589960	465730.921631	45.255681
3513.561420	465413.268243	45.260685
3513.465574	465113.252351	45.265690
3513.506241	464799.275570	45.270695
3513.697409	464492.969247	45.275700
3513.425812	464182.025096	45.280705
3513.344613	463873.222173	45.285709
3513.484370	463566.352698	45.290714
3513.395185	463245.786124	45.295719
3513.445206	462944.445150	45.300724
3513.276988	462643.592839	45.305729
3513.100297	462331.386915	45.310733
3513.044280	462026.604268	45.315738
3513.501354	461720.158421	45.320743
3513.180562	461425.242269	45.325748
3513.256093	461104.865986	45.330753
3513.275947	460806.081811	45.335757
3513.105775	460505.906634	45.340762
3513.609248	460204.344960	45.345767
3513.198518	459901.211755	45.350772
3513.040643	459586.982806	45.355777
3513.013265	459283.267940	45.360781
3512.963792	458984.265478	45.365786
3512.926246	458687.131698	45.370791
3513.349656	458393.766606	45.375796
3512.780163	458094.839638	45.380801
3513.139698	457796.915298	45.385805
3513.179104	457498.585046	45.390810
3513.133928	457193.726486	45.395815
3512.717960	456912.596732	45.400820
3512.698087	456617.456737	45.405825
3512.689556	456308.726400	45.410829
3512.520615	456024.348832	45.415834
3512.976762	455734.335510	45.420839
3512.664041	455452.052691	45.425844
3512.737397	455153.935503	45.430849
3512.731554	454861.403434	45.435853
3512.632911	454585.256291	45.440858
3512.321798	454283.542255	45.445863
3512.347980	453997.734379	45.450868
3512.184429	453718.595747	45.455873
3512.537961	453436.627546	45.460877
3512.288576	453162.666805	45.465882
3512.509988	452871.993921	45.470887
3512.549880	452594.833112	45.475892
3512.515820	452307.136264	45.480897
3512.292847	452025.196490	45.485901
3512.179963	451751.345794	45.490906
3512.070851	451461.317883	45.495911
3512.229253	451192.888976	45.500916
3512.071136	450911.734184	45.505921
3512.715012	450631.807582	45.510925
3512.272132	450353.228921	45.515930
3511.997661	450070.865815	45.520935
3512.257221	449802.807357	45.525940
3511.923344	449515.985045	45.530945
3511.908876	449257.447982	45.535949
3512.047913	448982.402425	45.540954
3512.149258	448701.376445	45.545959
3511.727940	448438.842337	45.550964
3511.898073	448175.849022	45.555969
3512.059084	447902.813900	45.560973
3511.858974	447627.757879	45.565978
3511.999527	447360.550699	45.570983
3511.998953	447098.942291	45.575988
3511.855795	446818.338717	45.580993
3511.548970	446552.972621	45.585997
3511.497334	446297.144097	45.591002
3511.834028	446024.663376	45.596007
3511.539276	445765.523000	45.601012
3511.744773	445507.460472	45.606017
3511.694391	445239.600037	45.611021
3511.693033	444979.182920	45.616026
3511.619086	444720.550069	45.621031
3511.338930	444462.507192	45.626036
3511.348325	444194.623531	45.631041
3511.631764	443941.701970	45.636045
3511.606274	443689.083787	45.641050
3511.422400	443414.934486	45.646055
3511.304559	443175.411362	45.651060
3511.009888	442915.830938	45.656065
3511.133449	442669.464621	45.661069
3511.118108	442417.489258	45.666074
3511.207708	442160.471674	45.671079
3511.111414	441919.358688	45.676084
3511.084419	441671.637319	45.681089
3511.098073	441427.051019	45.686093
3510.703124	441181.466564	45.691098
3510.951177	440920.704554	45.696103
3511.063352	440674.266975	45.701108
3510.743998	440433.784430	45.706113
3510.911479	440193.114682	45.711117
3510.967683	439954.338177	45.716122
3511.182398	439705.843216	45.721127
3511.039905	439466.740283	45.726132
3510.772168	439222.583368	45.731137
3510.787098	438978.679869	45.736141
3510.741352	438734.530406	45.741146
3510.806055	438500.200933	45.746151
3510.888594	438267.286390	45.751156
3510.225248	438016.183026	45.756161
3510.582780	437790.572491	45.761165
3510.537333	437553.816791	45.766170
3510.885665	437317.955263	45.771175
3510.817182	437087.337162	45.776180
3510.746113	436847.889547	45.781185
3510.773143	436609.843176	45.786189
3510.359332	436376.181979	45.791194
3510.496473	436146.178662	45.796199
3510.601127	435909.177067	45.801204
3510.743525	435677.747492	45.806209
3510.439662	435449.435933	45.811213
3510.501833	435217.964619	45.816218
3510.495566	434979.703810	45.821223
3510.247467	434761.371080	45.826228
3510.139657	434532.813870	45.831233
3510.632946	434300.244829	45.836237
3510.234978	434076.907965	45.841242
3510.173318	433838.898375	45.846247
3510.427653	433619.606340	45.851252
3510.112963	433398.227504	45.856257
3510.219582	433171.649701	45.861261
3510.053975	432943.390917	45.866266
3510.085375	432720.627157	45.871271
3510.018680	432502.343371	45.876276
3509.922853	432287.665274	45.881281
3510.309308	432060.064619	45.886285
3510.114002	431842.811431	45.891290
3510.005215	431620.314704	45.896295
3510.082355	431404.736209	45.901300
3509.871043	431189.509438	45.906305
3510.031945	430968.939499	45.911309
3509.747873	430757.070401	45.916314
3510.077468	430533.574962	45.921319
3510.493458	430328.230320	45.926324
3509.957542	430115.180442	45.931329
3510.051678	429887.253178	45.936333
3509.835789	429673.078903	45.941338
3509.879389	429453.732650	45.946343
3510.067324	429243.849965	45.951348
3510.021412	429028.727280	45.956353
3509.856116	428817.327833	45.961357
3509.950596	428605.222362	45.966362
3510.166554	428386.547243	45.971367
3509.806359	428171.368887	45.976372
3509.920004	427957.681000	45.981377
3510.094668	427745.351103	45.986381
3509.743303	427536.408117	45.991386
3509.808345	427322.164506	45.996391
3509.841601	427116.857208	46.001396
3509.712896	426897.415121	46.006401
3509.857906	426688.176899	46.011405
3509.527599	426480.997484	46.016410
3509.757454	426274.278944	46.021415
3509.325538	426073.965464	46.026420
3509.382486	425868.389590	46.031425
3509.600958	425661.921490	46.036429
3509.411388	425464.099415	46.041434
3509.330788	425256.105388	46.046439
3509.516348	425058.317436	46.051444
3509.170597	424860.161747	46.056449
3509.576564	424655.937169	46.061453
3509.245084	424466.557260	46.066458
3509.540883	424255.038627	46.071463
3509.175948	424060.128329	46.076468
3508.667321	423860.672462	46.081473
3509.551232	423667.068608	46.086477
3509.604391	423478.021385	46.091482
3509.604604	423273.752914	46.096487
3509.600817	423067.046779	46.101492
3509.539430	422864.917449	46.106497
3509.544686	422661.505965	46.111501
3509.316094	422467.574901	46.116506
3509.303360	422269.848844	46.121511
3509.383017	422072.359240	46.126516
3509.118785	421885.689081	46.131521
3509.246977	421681.994640	46.136525
3509.204378	421483.759685	46.141530
3509.230599	421299.573800	46.146535
3509.296973	421101.291775	46.151540
3508.998547	420903.349667	46.156545
3509.148937	420701.648651	46.161549
3508.668466	420515.106561	46.166554
3508.889181	420328.443336	46.171559
3508.942557	420149.854199	46.176564
3508.751504	419966.710866	46.181569
3508.850620	419767.194091	46.186573
3508.726877	419590.255812	46.191578
3509.108221	419402.085860	46.196583
3508.858185	419222.348756	46.201588
3509.091972	419032.221136	46.206593
3509.001585	418832.526152	46.211597
3508.754175	418657.963270	46.216602
3508.800750	418467.127123	46.221607
3508.555471	418289.337247	46.226612
3508.638511	418108.621355	46.231617
3508.791559	417924.464983	46.236621
3508.341018	417745.208479	46.241626
3508.722725	417576.750482	46.246631
3508.555570	417401.200448	46.251636
3508.395731	417218.488649	46.256641
3508.588326	417032.592655	46.261645
3508.426454	416859.170524	46.266650
3508.256587	416680.213963	46.271655
3508.284772	416512.012342	46.276660
3508.716237	416343.664581	46.281665
3508.710863	416165.844173	46.286669
3508.282785	415989.491084	46.291674
3508.602475	415819.229390	46.296679
3508.440342	415640.975082	46.301684
3508.386372	415466.839520	46.306689
3508.564571	415290.987421	46.311693
3508.158103	415123.079353	46.316698
3508.228088	414949.071439	46.321703
3508.053646	414770.838557	46.326708
3507.829627	414611.833269	46.331713
3508.198366	414446.022734	46.336717
3508.225765	414285.550639	46.341722
3508.171248	414114.859096	46.346727
3508.582490	413954.268615	46.351732
3508.187023	413780.154531	46.356737
3508.217009	413607.591661	46.361741
3508.378720	413444.628459	46.366746
3508.430192	413270.561584	46.371751
3508.403139	413105.978036	46.376756
3508.307907	412934.549294	46.381761
3508.270497	412762.779452	46.386765
3508.050817	412604.065770	46.391770
3508.104517	412437.737535	46.396775
3508.138648	412279.486382	46.401780
3507.856766	412118.926715	46.406785
3508.328191	411958.008897	46.411789
3507.554570	411789.786375	46.416794
3507.936905	411629.846682	46.421799
3507.695723	411473.643713	46.426804
3507.691598	411308.968727	46.431809
3508.267212	411148.053538	46.436813
3508.075583	410997.502036	46.441818
3508.207731	410831.937406	46.446823
3507.807962	410679.057993	46.451828
3507.663484	410520.801327	46.456833
3507.439125	410361.338424	46.461837
3507.221835	410222.214312	46.466842
3507.583275	410070.725063	46.471847
3507.894803	409915.764389	46.476852
3507.662119	409763.359039	46.481857
3507.521646	409604.918443	46.486861
3507.573229	409454.545173	46.491866
3507.523128	409302.334555	46.496871
3507.422012	409160.416942	46.501876
3507.123156	409019.700535	46.506881
3507.911978	408865.845834	46.511885
3507.582967	408715.254021	46.516890
3507.393351	408563.291566	46.521895
3507.403459	408409.084677	46.526900
3507.571016	408268.310063	46.531905
3507.672398	408124.193678	46.536909
3507.377542	407974.150582	46.541914
3507.522720	407830.025137	46.546919
3507.412714	407688.177417	46.551924
3507.178870	407539.823065	46.556929
3507.469202	407398.997532	46.561933
3507.336352	407253.849795	46.566938
3507.522628	407101.383124	46.571943
3507.218077	406965.050656	46.576948
3507.272398	406816.084369	46.581953
3507.539806	406674.039880	46.586957
3507.536458	406537.933202	46.591962
3507.492345	406392.994270	46.596967
3507.292084	406248.665385	46.601972
3507.123199	406110.400580	46.606977
3507.337230	405962.291272	46.611981
3507.412424	405821.900647	46.616986
3507.690388	405677.588666	46.621991
3507.341704	405533.281327	46.626996
3507.211695	405391.348791	46.632001
3507.440661	405251.005166	46.637005
3506.919650	405112.541431	46.642010
3507.077865	404975.789772	46.647015
3506.983901	404846.573350	46.652020
3506.706880	404707.100720	46.657025
3507.120427	404572.741818	46.662029
3507.193017	404442.834661	46.667034
3507.119700	404308.481400	46.672039
3506.857020	404176.369630	46.677044
3506.640066	404038.381955	46.682049
3506.999862	403906.696008	46.687053
3506.585035	403782.863455	46.692058
3506.984447	403653.252375	46.697063
3507.103299	403516.982797	46.702068
3506.590577	403391.133144	46.707073
3507.023103	403258.085441	46.712077
3506.797110	403132.160249	46.717082
3506.883960	402992.413603	46.722087
3506.694476	402864.118645	46.727092
3506.904548	402740.962170	46.732097
3507.112499	402614.808125	46.737101
3506.545830	402491.605365	46.742106
3506.954197	402360.843644	46.747111
3506.851487	402233.115202	46.752116
3506.711110	402104.935369	46.757121
3506.592185	401977.589556	46.762125
3506.496901	401863.448304	46.767130
3506.651154	401732.371401	46.772135
3506.521789	401615.288280	46.777140
3506.801479	401492.216018	46.782145
3506.734740	401360.971892	46.787149
3506.305671	401239.442096	46.792154
3506.589903	401121.905250	46.797159
3506.830937	401004.781739	46.802164
3506.587549	400885.606593	46.807169
3506.752830	400756.123648	46.812173
3506.821496	400638.697805	46.817178
3506.754568	400511.336463	46.822183
3506.347938	400392.415737	46.827188
3506.529685	400259.879273	46.832193
3506.753445	400140.494195	46.837197
3506.126224	400030.932813	46.842202
3506.419145	399905.133146	46.847207
3506.669196	399792.321754	46.852212
3506.288851	399676.391218	46.857217
3506.068623	399554.157997	46.862221
3506.159127	399454.303311	46.867226
3506.211151	399334.639315	46.872231
3505.974624	399227.624786	46.877236
3505.861839	399111.570047	46.882241
3506.105519	399015.599997	46.887245
3506.288545	398900.408462	46.892250
3506.293329	398782.706395	46.897255
3506.382102	398676.650455	46.902260
3506.392234	398563.265442	46.907265
3506.541803	398438.957285	46.912269
3506.454425	398332.777718	46.917274
3506.714717	398220.136200	46.922279
3506.714997	398105.988895	46.927284
3506.657695	397984.635741	46.932289
3506.730963	397865.139811	46.937293
3506.734185	397748.170534	46.942298
3506.578312	397621.903928	46.947303
3506.838906	397504.229156	46.952308
3506.594826	397391.009956	46.957313
3506.595966	397272.946638	46.962317
3506.466175	397157.166369	46.967322
3506.206624	397035.361031	46.972327
3506.319877	396929.472318	46.977332
3505.916516	396824.890956	46.982337
3506.073927	396711.905422	46.987341
3505.779546	396614.113727	46.992346
3505.883044	396495.877321	46.997351
3506.282565	396393.215279	47.002356
3505.949344	396289.560075	47.007361
3506.229769	396183.995799	47.012365
3506.096856	396078.832017	47.017370
3505.639563	395962.823424	47.022375
3506.044621	395868.111136	47.027380
3505.969931	395771.142952	47.032385
3506.172133	395655.655719	47.037389
3505.890488	395564.388122	47.042394
3506.113100	395458.831097	47.047399
3506.092094	395347.522256	47.052404
3505.893365	395243.052721	47.057409
3505.951282	395134.397449	47.062413
3505.832590	395034.486984	47.067418
3506.114610	394931.407932	47.072423
3505.541986	394830.329271	47.077428
3505.640237	394727.560376	47.082433
3505.736458	394632.769790	47.087437
3505.996113	394533.834776	47.092442
3506.099737	394426.846063	47.097447
3506.174452	394327.382940	47.102452
3505.457018	394227.724428	47.107457
3506.116794	394122.265823	47.112461
3505.845402	394043.899574	47.117466
3505.471711	393933.916069	47.122471
3505.695703	393844.894448	47.127476
3505.601946	393755.901408	47.132481
3505.715431	393639.201763	47.137485
3505.690550	393553.702867	47.142490
3505.522441	393466.246229	47.147495
3505.786574	393372.617188	47.152500
3505.547200	393274.500060	47.157505
3505.596568	393169.320167	47.162509
3505.491671	393083.808173	47.167514
3505.711504	392991.608458	47.172519
3505.680726	392900.010274	47.177524
3505.449997	392809.386129	47.182529
3506.011509	392709.986927	47.187533
3505.525855	392612.773623	47.192538
3505.491096	392525.901303	47.197543
3505.570971	392431.690921	47.202548
3505.183695	392343.277400	47.207553
3505.673655	392255.222041	47.212557
3505.440543	392166.248048	47.217562
3505.404181	392066.770926	47.222567
3505.249066	391984.466130	47.227572
3505.089700	391895.529565	47.232577
3505.800305	391811.094411	47.237581
3505.196114	391726.807294	47.242586
3505.476378	391642.724674	47.247591
3505.467594	391553.100691	47.252596
3505.210042	391471.091506	47.257601
3505.296916	391373.141140	47.262605
3505.381832	391289.268770	47.267610
3505.501000	391202.849161	47.272615
3505.658326	391120.056655	47.277620
3505.180269	391040.752176	47.282625
3505.400765	390939.702770	47.287629
3505.206244	390864.161183	47.292634
3505.055084	390776.846277	47.297639
3505.315428	390693.857132	47.302644
3505.354791	390608.084752	47.307649
3505.420073	390522.587237	47.312653
3505.221142	390451.111319	47.317658
3505.237552	390358.938276	47.322663
3505.457237	390283.629464	47.327668
3505.251219	390196.093543	47.332673
3504.951510	390104.100768	47.337677
3505.054976	390020.882449	47.342682
3504.939773	389955.235959	47.347687
3505.246614	389876.963395	47.352692
3504.772814	389806.574818	47.357697
3505.511613	389724.187476	47.362701
3504.827085	389646.591857	47.367706
3505.154274	389563.308676	47.372711
3505.170719	389487.422692	47.377716
3504.871221	389410.472293	47.382721
3505.032009	389338.119123	47.387725
3504.996251	389269.103060	47.392730
3505.000062	389175.429216	47.397735
3505.209255	389105.557733	47.402740
3505.057741	389026.624274	47.407745
3505.047202	388951.097358	47.412749
3504.946823	388880.312512	47.417754
3504.777931	388792.740821	47.422759
3504.654657	388721.349592	47.427764
3504.881397	388645.806823	47.432769
3505.034088	388573.631132	47.437773
3504.959227	388503.400165	47.442778
3504.928082	388432.297500	47.447783
3505.031621	388360.078875	47.452788
3504.712324	388274.564509	47.457793
3505.085376	388208.068489	47.462797
3504.509552	388138.989625	47.467802
3504.944724	388066.612029	47.472807
3505.047180	387990.478939	47.477812
3504.628855	387932.453333	47.482817
3504.877967	387844.909233	47.487821
3504.883520	387781.931405	47.492826
3504.823758	387705.164538	47.497831
3504.902334	387641.030304	47.502836
3504.975742	387561.520986	47.507841
3505.035385	387480.971814	47.512845
3504.887396	387424.805196	47.517850
3505.019792	387348.080879	47.522855
3504.894347	387274.424766	47.527860
3504.561815	387209.292416	47.532865
3504.715651	387137.341918	47.537869
3504.429046	387068.312942	47.542874
3504.577916	387001.598470	47.547879
3504.455181	386941.156936	47.552884
3504.684249	386872.217379	47.557889
3504.878260	386807.045108	47.562893
3504.630889	386746.548234	47.567898
3504.873206	386669.625571	47.572903
3505.179682	386598.766043	47.577908
3504.851953	386542.043972	47.582913
3505.149483	386464.475992	47.587917
3504.718708	386395.902211	47.592922
3505.109934	386328.992428	47.597927
3505.255396	386260.904516	47.602932
3504.816108	386190.196822	47.607937
3505.327075	386111.803637	47.612941
3504.872277	386042.699454	47.617946
3504.649733	385975.309157	47.622951
3504.675088	385895.727559	47.627956
3504.261484	385841.992553	47.632961
3504.467204	385775.418259	47.637965
3504.482569	385716.856987	47.642970
3504.613336	385645.542406	47.647975
3504.315362	385577.401652	47.652980
3504.345821	385526.691059	47.657985
3504.394095	385463.040444	47.662989
3504.167097	385412.856540	47.667994
3504.434243	385351.582881	47.672999
3504.246139	385285.608546	47.678004
3504.427505	385234.363386	47.683009
3504.548780	385179.392174	47.688013
3504.180963	385120.666478	47.693018
3504.487214	385064.850150	47.698023
3504.585917	385003.553746	47.703028
3504.372555	384947.088854	47.708033
3504.658891	384877.982650	47.713037
3504.321289	384819.556236	47.718042
3504.123786	384757.039092	47.723047
3504.298106	384705.031774	47.728052
3504.061801	384657.186618	47.733057
3504.271426	384587.635375	47.738061
3504.078346	384546.848599	47.743066
3504.004388	384488.325723	47.748071
3504.153393	384437.745648	47.753076
3503.728322	384382.434255	47.758081
3504.177208	384324.889322	47.763085
3504.326005	384282.467962	47.768090
3503.981423	384221.220324	47.773095
3504.005623	384178.032165	47.778100
3503.987091	384126.056832	47.783105
3504.372188	384080.519351	47.788109
3503.997354	384019.683171	47.793114
3503.985126	383972.535829	47.798119
3504.178446	383920.498568	47.803124
3503.894579	383866.610969	47.808129
3504.227208	383823.115488	47.813133
3504.072882	383770.018970	47.818138
3504.107446	383723.219117	47.823143
3504.418041	383665.722029	47.828148
3504.248909	383620.024353	47.833153
3504.037912	383560.633554	47.838157
3503.976271	383522.339389	47.843162
3503.851201	383459.883587	47.848167
3504.074167	383420.447733	47.853172
3503.754750	383381.206116	47.858177
3504.188150	383321.959020	47.863181
3504.294808	383285.211752	47.868186
3504.392839	383229.834459	47.873191
3504.423353	383181.001060	47.878196
3504.300774	383129.804419	47.883201
3504.544724	383070.665465	47.888205
3504.107922	383020.386525	47.893210
3504.102967	382972.677269	47.898215
3504.175496	382914.761959	47.903220
3504.078312	382880.972145	47.908225
3504.265327	382815.284504	47.913229
3504.227327	382775.485726	47.918234
3504.290945	382715.385592	47.923239
3503.985218	382667.168035	47.928244
3504.198428	382616.040333	47.933249
3504.255675	382562.651507	47.938253
3503.945778	382508.333955	47.943258
3503.973503	382468.955694	47.948263
3504.266430	382417.636135	47.953268
3503.557924	382385.882012	47.958273
3503.854873	382335.985088	47.963277
3504.210124	382287.298235	47.968282
3503.924791	382236.941371	47.973287
3504.441561	382197.784299	47.978292
3504.303066	382147.173452	47.983297
3504.035256	382089.873995	47.988301
3503.937575	382053.897368	47.993306
3503.902812	382000.370810	47.998311
3504.354376	381944.320888	48.003316
3503.905915	381907.133040	48.008321
3504.439018	381853.687210	48.013325
3503.978690	381809.968548	48.018330
3504.373427	381757.664631	48.023335
3504.225518	381701.055752	48.028340
3504.254025	381647.746584	48.033345
3504.286331	381612.865723	48.038349
3504.241139	381562.721001	48.043354
3504.341358	381514.813702	48.048359
3504.145532	381455.314762	48.053364
3504.142623	381413.983150	48.058369
3504.108479	381357.557604	48.063373
3504.075028	381310.867550	48.068378
3503.833398	381275.016319	48.073383
3504.166000	381230.576830	48.078388
3503.998282	381185.027988	48.083393
3504.446922	381129.485558	48.088397
3504.212921	381091.878861	48.093402
3504.189347	381040.026519	48.098407
3504.034024	380987.789875	48.103412
3503.783848	380945.279740	48.108417
3503.986929	380906.555980	48.113421
3503.675466	380851.346230	48.118426
3503.714805	380805.481882	48.123431
3503.747580	380790.478489	48.128436
3503.602427	380756.821756	48.133441
3504.044474	380697.212515	48.138445
3503.856707	380666.028712	48.143450
3503.581700	380629.114827	48.148455
3503.777045	380574.987396	48.153460
3503.574614	380538.569421	48.158465
3503.833561	380507.360028	48.163469
3503.910537	380465.581435	48.168474
3503.551239	380425.987168	48.173479
3503.756335	380393.032863	48.178484
3503.702889	380344.285799	48.183489
3503.519161	380303.059922	48.188493
3503.767163	380277.648027	48.193498
3503.686614	380250.029797	48.198503
3503.945642	380187.324171	48.203508
3503.604578	380161.606045	48.208513
3503.882376	380125.690281	48.213517
3503.574687	380074.240815	48.218522
3503.657868	380048.551841	48.223527
3503.699420	380015.675926	48.228532
3503.589124	379978.224772	48.233537
3503.384102	379935.603937	48.238541
3503.287250	379906.869693	48.243546
3503.454805	379879.488415	48.248551
3503.773446	379851.623742	48.253556
3503.242745	379806.694223	48.258561
3503.662879	379764.271467	48.263565
3503.582051	379747.532962	48.268570
3503.551729	379717.999149	48.273575
3503.838244	379679.005490	48.278580
3503.568420	379652.868068	48.283585
3503.637317	379617.775471	48.288589
3503.692395	379593.489092	48.293594
3503.476848	379528.905840	48.298599
3503.815649	379505.791156	48.303604
3503.549427	379483.999976	48.308609
3503.650562	379440.258540	48.313613
3503.683548	379396.503263	48.318618
3503.513425	379369.306328	48.323623
3503.901309	379341.759878	48.328628
3503.651080	379309.136452	48.333633
3503.680504	379262.280226	48.338637
3503.728855	379239.037004	48.343642
3503.659369	379203.154119	48.348647
3503.941254	379159.737347	48.353652
3503.955611	379128.848053	48.358657
3503.981236	379084.153033	48.363661
3503.624217	379048.624134	48.368666
3503.684520	379011.193599	48.373671
3503.703395	378981.955786	48.378676
3503.611658	378936.975552	48.383681
3503.966502	378896.088120	48.388685
3503.779044	378863.784017	48.393690
3503.687250	378830.980539	48.398695
3503.769934	378800.816497	48.403700
3503.689859	378769.866729	48.408705
3503.782852	378723.100574	48.413709
3503.658630	378688.777198	48.418714
3503.730017	378662.656996	48.423719
3503.796512	378613.556422	48.428724
3503.724375	378586.265850	48.433729
3503.367961	378549.821134	48.438733
3503.652749	378522.266188	48.443738
3503.517969	378490.867911	48.448743
3503.484679	378449.817413	48.453748
3503.416284	378437.118191	48.458753
3503.844329	378404.276371	48.463757
3503.547564	378352.618992	48.468762
3503.672952	378323.438680	48.473767
3503.566281	378298.797646	48.478772
3503.123072	378284.382833	48.483777
3503.656613	378240.718518	48.488781
3503.444726	378206.867210	48.493786
3503.571653	378173.720674	48.498791
3503.614773	378153.172321	48.503796
3503.806148	378120.090993	48.508801
3503.905568	378081.890074	48.513805
3503.419772	378050.627588	48.518810
3503.446958	378035.267993	48.523815
3503.536240	377981.052753	48.528820
3503.541472	377959.087110	48.533825
3503.382488	377920.243732	48.538829
3503.509768	377906.824496	48.543834
3503.265125	377886.655606	48.548839
3503.258634	377840.947517	48.553844
3503.209527	377811.771133	48.558849
3503.441349	377784.072091	48.563853
3503.071382	377767.839564	48.568858
3503.032858	377741.254388	48.573863
3503.443748	377721.329375	48.578868
3503.443681	377715.889003	48.583873
3503.698882	377674.991674	48.588877
3503.413229	377642.448933	48.593882
3503.189316	377617.013901	48.598887
3503.426349	377598.415047	48.603892
3503.415059	377584.815964	48.608897
3503.456554	377553.005371	48.613901
3503.464859	377508.082400	48.618906
3503.070048	377478.837645	48.623911
3503.515755	377449.296805	48.628916
3503.321275	377433.517180	48.633921
3503.494255	377412.946200	48.638925
3503.443897	377375.532731	48.643930
3503.471795	377342.427707	48.648935
3503.759907	377316.371141	48.653940
3503.307460	377288.178391	48.658945
3503.637284	377276.046298	48.663949
3503.524796	377243.880366	48.668954
3503.341806	377211.345101	48.673959
3503.423419	377177.900248	48.678964
3503.114466	377154.843704	48.683969
3503.699420	377146.023806	48.688973
3503.480773	377108.689623	48.693978
3503.684120	377074.461197	48.698983
3503.703438	377057.297477	48.703988
3503.379957	377024.226718	48.708993
3503.124643	376981.992040	48.713997
3502.986127	376955.601279	48.719002
3502.856749	376932.361382	48.724007
3503.066791	376908.249976	48.729012
3503.048785	376891.753542	48.734017
3503.166053	376876.835650	48.739021
3503.253112	376858.668766	48.744026
3503.089132	376840.468469	48.749031
3503.264843	376818.701779	48.754036
3502.959139	376807.389883	48.759041
3503.191605	376786.884634	48.764045
3502.930118	376771.650024	48.769050
3502.646252	376760.258114	48.774055
3502.862350	376738.408208	48.779060
3503.048052	376723.071793	48.784065
3502.919172	376697.441878	48.789069
3503.046740	376687.505076	48.794074
3502.990356	376666.413498	48.799079
3503.256056	376650.783736	48.804084
3502.879970	376638.593991	48.809089
3503.049261	376623.285757	48.814093
3503.076486	376607.213656	48.819098
3502.730836	376587.798507	48.824103
3503.533490	376565.797485	48.829108
3503.363117	376537.022054	48.834113
3503.102787	376511.211057	48.839117
3502.947631	376486.831209	48.844122
3502.912849	376463.727378	48.849127
3502.881652	376447.283827	48.854132
3502.796416	376436.900246	48.859137
3503.308684	376419.906263	48.864141
3502.932132	376408.097864	48.869146
3502.795389	376393.401097	48.874151
3503.307800	376379.457871	48.879156
3502.925525	376358.345479	48.884161
3502.882844	376353.420633	48.889165
3502.913816	376331.017338	48.894170
3502.945862	376322.672991	48.899175
3502.934544	376306.175131	48.904180
3502.830691	376291.320163	48.909185
3502.715372	376271.941773	48.914189
3502.503210	376253.215496	48.919194
3502.690522	376237.726047	48.924199
3502.987397	376215.709470	48.929204
3503.152808	376208.893155	48.934209
3503.049770	376186.919424	48.939213
3502.925746	376168.966179	48.944218
3502.609406	376157.757576	48.949223
3503.166098	376142.408398	48.954228
3502.458934	376134.139382	48.959233
3502.819359	376119.103367	48.964237
3503.080277	376096.991159	48.969242
3502.841955	376090.777655	48.974247
3503.171234	376075.874057	48.979252
3502.841763	376058.743966	48.984257
3502.918135	376040.756435	48.989261
3502.795790	376042.480709	48.994266
3502.632324	376022.195149	48.999271
3503.067424	376017.544601	49.004276
3502.781840	376009.737464	49.009281
3503.082660	376006.253907	49.014285
3503.147539	375987.378482	49.019290
3502.952880	375962.394836	49.024295
3502.856353	375935.131705	49.029300
3502.896357	375925.514718	49.034305
3502.921303	375903.417255	49.039309
3503.015450	375898.367283	49.044314
3503.053504	375885.496381	49.049319
3503.357955	375862.130825	49.054324
3502.686908	375861.558970	49.059329
3503.264484	375833.519634	49.064333
3503.332202	375825.702974	49.069338
3502.915570	375821.680890	49.074343
3503.130792	375806.059360	49.079348
3502.887078	375795.270440	49.084353
3503.190692	375781.998219	49.089357
3503.232242	375771.999567	49.094362
3503.500897	375753.851932	49.099367
3503.126404	375726.178470	49.104372
3503.163945	375695.129525	49.109377
3503.255812	375672.944214	49.114381
3503.240587	375650.929719	49.119386
3503.036538	375648.015390	49.124391
3503.405008	375624.384501	49.129396
3503.280971	375610.371672	49.134401
3503.622587	375592.135221	49.139405
3503.080314	375565.405540	49.144410
3502.700733	375541.520968	49.149415
3502.931461	375522.667815	49.154420
3502.568671	375521.382293	49.159425
3502.868928	375522.017472	49.164429
3503.129280	375518.083144	49.169434
3502.762613	375509.272777	49.174439
3502.886550	375498.954889	49.179444
3503.013944	375487.975383	49.184449
3502.784512	375466.658371	49.189453
3502.600943	375456.570947	49.194458
3502.367298	375450.788737	49.199463
3502.689224	375427.089388	49.204468
3502.755771	375422.679661	49.209473
3502.703310	375409.696915	49.214477
3502.792345	375398.012055	49.219482
3502.496490	375385.833584	49.224487
3502.682561	375367.648998	49.229492
3503.082781	375383.165640	49.234497
3503.173275	375365.022797	49.239501
3503.100333	375350.390958	49.244506
3502.769546	375327.413173	49.249511
3502.962476	375308.312115	49.254516
3502.647783	375308.009914	49.259521
3502.722032	375285.395150	49.264525
3502.811447	375294.049527	49.269530
3502.868396	375297.319522	49.274535
3503.107084	375287.973519	49.279540
3502.498966	375291.077413	49.284545
3502.761005	375272.167928	49.289549
3503.002308	375261.473989	49.294554
3502.647306	375252.636139	49.299559
3503.095119	375240.813690	49.304564
3502.850119	375229.033267	49.309569
3502.714547	375213.217125	49.314573
3502.779786	375208.502503	49.319578
3502.588557	375191.068704	49.324583
3502.715075	375179.453643	49.329588
3502.600152	375173.854507	49.334593
3502.733119	375160.967125	49.339597
3502.644902	375149.871782	49.344602
3502.048101	375148.575356	49.349607
3502.918421	375145.935165	49.354612
3503.167348	375152.121610	49.359617
3502.666883	375142.113629	49.364621
3502.350365	375135.099726	49.369626
3502.268200	375124.638949	49.374631
3502.487931	375102.838224	49.379636
3502.490000	375102.659902	49.384641
3502.387765	375115.745456	49.389645
3502.900448	375120.666502	49.394650
3502.692042	375121.413970	49.399655
3502.967323	375106.951385	49.404660
3502.759154	375095.901931	49.409665
3502.943251	375084.302430	49.414669
3503.024995	375073.533981	49.419674
3502.521494	375061.263729	49.424679
3502.789637	375044.870086	49.429684
3502.720239	375037.941088	49.434689
3502.880601	375025.048977	49.439693
3503.118354	375018.753985	49.444698
3502.686427	375014.378475	49.449703
3502.751468	374989.375196	49.454708
3502.479858	374985.887586	49.459713
3502.449916	374977.019583	49.464717
3502.477256	374987.896561	49.469722
3502.415049	374993.602249	49.474727
3503.063670	374977.524972	49.479732
3502.648718	374982.070524	49.484737
3502.403494	374964.747527	49.489741
3502.418217	374954.219305	49.494746
3502.285277	374955.004740	49.499751
3502.580179	374966.039432	49.504756
3503.100207	374967.348978	49.509761
3502.579768	374956.886714	49.514765
3502.698027	374958.112319	49.519770
3502.584600	374941.097323	49.524775
3502.535577	374925.520514	49.529780
3502.404049	374932.661819	49.534785
3502.785776	374913.452030	49.539789
3503.067946	374923.192263	49.544794
3503.083256	374922.884557	49.549799
3503.064997	374895.988601	49.554804
3502.937219	374887.645771	49.559809
3503.075865	374876.282781	49.564813
3503.130892	374868.086702	49.569818
3502.675987	374849.833321	49.574823
3502.565971	374844.970604	49.579828
3502.607108	374848.014522	49.584833
3502.720619	374851.859665	49.589837
3502.961875	374847.445456	49.594842
3502.787508	374854.136451	49.599847
3502.970136	374839.206509	49.604852
3502.844577	374829.134419	49.609857
3502.620399	374813.256950	49.614861
3503.010819	374809.961370	49.619866
3502.728280	374803.424663	49.624871
3503.014439	374789.799096	49.629876
3502.877124	374789.695422	49.634881
3503.055981	374768.715052	49.639885
3502.956044	374758.384320	49.644890
3502.537969	374765.701712	49.649895
3502.669051	374738.347914	49.654900
3502.768404	374745.017616	49.659905
3502.787806	374727.725586	49.664909
3502.515349	374717.678548	49.669914
3502.364649	374719.229758	49.674919
3502.717761	374721.152582	49.679924
3502.735845	374731.675277	49.684929
3502.785834	374733.726134	49.689933
3502.641921	374726.301305	49.694938
3502.509829	374713.382742	49.699943
3502.625777	374704.057540	49.704948
3502.665003	374703.135557	49.709953
3502.641443	374686.232213	49.714957
3502.482148	374674.335265	49.719962
3502.403636	374679.255627	49.724967
3502.774579	374686.514579	49.729972
3502.571721	374693.235895	49.734977
3502.849372	374676.815029	49.739981
3502.561275	374670.202972	49.744986
3502.516168	374656.862740	49.749991
3502.873938	374652.708283	49.754996
3502.781252	374651.325755	49.760001
3502.881225	374634.833511	49.765005
3502.856026	374617.472768	49.770010
3502.855888	374621.617015	49.775015
3502.860323	374604.454603	49.780020
3502.610034	374605.590604	49.785025
3502.626834	374607.926808	49.790029
3502.621857	374618.097529	49.795034
3502.576793	374614.494922	49.800039
3502.880342	374602.951136	49.805044
3502.600621	374603.583670	49.810049
3503.075166	374596.027782	49.815053
3502.843140	374586.812816	49.820058
3502.253215	374586.862702	49.825063
3502.534917	374567.898623	49.830068
3502.609499	374560.792394	49.835073
3502.792142	374566.100398	49.840077
3502.722964	374571.909046	49.845082
3502.747150	374571.879493	49.850087
3502.768778	374561.019450	49.855092
3502.607898	374565.903043	49.860097
3502.304360	374553.928985	49.865101
3502.686214	374544.329512	49.870106
3502.134626	374536.948830	49.875111
3502.742612	374544.853804	49.880116
3502.543832	374574.482117	49.885121
3502.625832	374564.959276	49.890125
3502.773521	374555.908285	49.895130
3502.504038	374547.564145	49.900135
3502.961962	374534.799014	49.905140
3502.645917	374537.853100	49.910145
3502.754399	374528.402001	49.915149
3502.411005	374518.646689	49.920154
3502.025929	374517.797154	49.925159
3502.261504	374525.257229	49.930164
3502.578274	374538.779949	49.935169
3502.761166	374530.638231	49.940173
3502.732327	374525.329386	49.945178
3502.604116	374521.562994	49.950183
3502.261694	374514.909334	49.955188
3502.199234	374527.861195	49.960193
3502.229393	374527.932321	49.965197
3502.314851	374521.993766	49.970202
3502.363679	374537.240272	49.975207
3502.694259	374538.988981	49.980212
3502.769398	374552.934326	49.985217
3502.455968	374545.818076	49.990221
3503.107631	374542.121916	49.995226
3503.012180	374540.027964	50.000231
3503.015394	374524.060683	50.005236
3503.001058	374527.495472	50.010241
3502.822352	374512.983035	50.015245
3503.051881	374503.460411	50.020250
3502.872774	374502.626554	50.025255
3503.148806	374494.214676	50.030260
3503.209732	374484.924234	50.035265
3502.856778	374486.382867	50.040269
3503.314993	374461.413768	50.045274
3503.014300	374459.507406	50.050279
3502.835434	374437.392952	50.055284
3502.417805	374438.481258	50.060289
3502.819233	374431.903963	50.065293
3503.122795	374429.818145	50.070298
3502.695437	374427.018117	50.075303
3503.085741	374414.747559	50.080308
3503.049609	374403.821056	50.085313
3502.834563	374396.001504	50.090317
3503.115620	374394.682272	50.095322
3503.193024	374391.796050	50.100327
3503.323918	374376.493369	50.105332
3502.831810	374351.864438	50.110337
3502.904196	374323.249092	50.115341
3503.280058	374316.193067	50.120346
3502.900560	374308.198178	50.125351
3503.000131	374301.138479	50.130356
3502.740244	374294.267283	50.135361
3502.920157	374289.660080	50.140365
3503.131088	374275.309834	50.145370
3502.421913	374268.133977	50.150375
3502.907631	374261.949056	50.155380
3502.323370	374263.548895	50.160385
3502.324819	374281.956296	50.165389
3502.398418	374275.358675	50.170394
3502.217677	374275.694638	50.175399
3502.548883	374271.264997	50.180404
3502.398766	374283.697995	50.185409
3502.328463	374300.363318	50.190413
3502.576054	374298.439599	50.195418
3502.395727	374292.266715	50.200423
3502.597672	374281.401219	50.205428
3502.623271	374283.151169	50.210433
3502.633808	374304.455446	50.215437
3502.856425	374305.078482	50.220442
3502.492113	374301.199832	50.225447
3502.561765	374292.085823	50.230452
3502.408499	374286.086291	50.235457
3502.539230	374279.199241	50.240461
3502.647426	374274.756831	50.245466
3502.543901	374280.647667	50.250471
3503.088385	374288.690669	50.255476
3502.675958	374293.007055	50.260481
3502.629773	374299.599994	50.265485
3502.598833	374284.401182	50.270490
3502.517185	374282.635381	50.275495
3502.603497	374273.442247	50.280500
3502.625284	374267.895894	50.285505
3502.733685	374260.529581	50.290509
3502.550051	374259.365967	50.295514
3502.265354	374264.270745	50.300519
3502.501790	374267.484765	50.305524
3502.407797	374270.043309	50.310529
3502.511374	374270.966347	50.315533
3502.348386	374266.951616	50.320538
3502.377710	374269.921327	50.325543
3502.690503	374284.894046	50.330548
3502.686450	374297.912295	50.335553
3502.720704	374289.490802	50.340557
3502.890871	374285.597160	50.345562
3502.251973	374286.646979	50.350567
3502.725470	374268.260184	50.355572
3502.629191	374265.784982	50.360577
3502.198395	374263.621151	50.365581
3502.762325	374276.186472	50.370586
3502.201971	374285.028330	50.375591
3502.657427	374280.577474	50.380596
3502.566586	374283.262604	50.385601
3502.850482	374265.874330	50.390605
3502.835055	374262.139501	50.395610
3502.671294	374266.159180	50.400615
3502.681321	374257.843516	50.405620
3502.687826	374281.335040	50.410625
3502.407255	374289.137551	50.415629
3502.455944	374274.204811	50.420634
3502.557251	374272.356919	50.425639
3502.664677	374271.041906	50.430644
3502.532497	374267.733812	50.435649
3502.548269	374252.349035	50.440653
3502.527007	374263.336240	50.445658
3502.380054	374285.353895	50.450663
3502.537472	374268.749966	50.455668
3502.384707	374275.717058	50.460673
3502.672018	374278.973240	50.465677
3502.501568	374269.925649	50.470682
3502.594392	374273.087916	50.475687
3502.389020	374292.115400	50.480692
3502.350649	374296.673013	50.485697
3502.518005	374289.194939	50.490701
3502.286501	374285.725833	50.495706
3502.254882	374288.222875	50.500711
3502.553784	374287.968438	50.505716
3502.416280	374291.093759	50.510721
3502.179265	374292.380053	50.515725
3502.800320	374292.248581	50.520730
3502.374423	374284.948081	50.525735
3502.404456	374268.543879	50.530740
3502.533474	374255.428009	50.535745
3502.031410	374202.095904	50.540749
3502.553848	374157.919756	50.545754
3502.396985	374102.469125	50.550759
3502.628715	374015.755450	50.555764
3502.063850	373935.355899	50.560769
3502.516312	373842.629183	50.565773
3502.311768	373719.554873	50.570778
3502.174517	373613.147709	50.575783
3502.362704	373486.852764	50.580788
3502.387258	373344.109513	50.585793
3502.554825	373188.272440	50.590797
3502.747186	373005.326490	50.595802
3502.608490	372841.632727	50.600807
3502.593482	372646.414139	50.605812
3502.480770	372443.023892	50.610817
3502.684074	372223.890410	50.615821
3502.458544	371992.420618	50.620826
3502.368794	371747.704209	50.625831
3502.252014	371492.311405	50.630836
3502.361850	371244.862182	50.635841
3502.307866	370955.433285	50.640845
3502.480882	370669.446844	50.645850
3502.268094	370377.497618	50.650855
3502.586860	370063.485488	50.655860
3502.311156	369731.899527	50.660865
3502.122598	369394.091091	50.665869
3502.508905	369035.584099	50.670874
3502.301829	368676.488301	50.675879
3502.414118	368292.973246	50.680884
3502.320324	367905.700355	50.685889
3502.216633	367498.132110	50.690893
3502.113804	367073.571921	50.695898
3501.838948	366659.666099	50.700903
3502.086900	366221.252966	50.705908
3501.986787	365748.791189	50.710913
3501.864594	365284.948403	50.715917
3501.926380	364793.322581	50.720922
3502.184545	364292.704761	50.725927
3502.160564	363767.637194	50.730932
3501.979913	363241.724416	50.735937
3501.807701	362695.838042	50.740941
3502.074743	362113.473721	50.745946
3501.913840	361548.494093	50.750951
3501.970337	360944.631165	50.755956
3501.968564	360328.407650	50.760961
3501.514826	359693.099109	50.765965
3501.698115	359045.488022	50.770970
3501.568964	358389.602233	50.775975
3501.666494	357698.412362	50.780980
3501.733409	357015.050361	50.785985
3501.428015	356298.773925	50.790989
3501.576307	355544.073026	50.795994
3501.217767	354801.146347	50.800999
3501.271231	354015.958948	50.806004
3501.065232	353236.346818	50.811009
3500.785085	352428.571430	50.816013
3501.362009	351604.454519	50.821018
3500.600320	350753.812421	50.826023
3501.221550	349885.439498	50.831028
3500.610254	349016.725510	50.836033
3500.657492	348108.319640	50.841037
3500.914912	347190.903579	50.846042
3501.023660	346245.506833	50.851047
3501.156669	345274.464580	50.856052
3500.639529	344272.267416	50.861057
3500.509955	343262.857944	50.866061
3500.381982	342223.579245	50.871066
3499.992486	341176.027175	50.876071
3500.334518	340102.652020	50.881076
3500.080074	339018.438381	50.886081
3499.989561	337910.659481	50.891085
3499.838816	336783.703986	50.896090
3499.856237	335636.564913	50.901095
3499.726609	334461.940278	50.906100
3499.788815	333276.033172	50.911105
3499.371443	332067.861536	50.916109
3499.477782	330828.166980	50.921114
3498.958205	329590.256577	50.926119
3498.855296	328313.102272	50.931124
3498.427085	327022.713983	50.936129
3498.332029	325714.397322	50.941133
3498.177159	324393.793125	50.946138
3497.478969	323062.256422	50.951143
3497.676739	321691.260878	50.956148
3497.503489	320333.510074	50.961153
3497.456406	318934.902916	50.966157
3497.188465	317515.454638	50.971162
3497.038830	316086.664210	50.976167
3496.953944	314627.411062	50.981172
3496.822124	313161.516497	50.986177
3496.693876	311672.576861	50.991181
3496.387262	310157.236548	50.996186
3496.468655	308634.594713	51.001191
3496.224228	307087.129773	51.006196
3495.437649	305525.062401	51.011201
3495.603872	303937.952943	51.016205
3495.610487	302343.075689	51.021210
3494.893594	300725.784962	51.026215
3494.878572	299095.105543	51.031220
3494.626811	297448.728180	51.036225
3494.562680	295785.969584	51.041229
3494.413658	294106.138166	51.046234
3493.894973	292415.674407	51.051239
3493.678154	290690.273028	51.056244
3493.673669	288960.710613	51.061249
3493.143640	287210.714650	51.066253
3492.926892	285445.719330	51.071258
3492.297727	283676.417685	51.076263
3492.349285	281883.881138	51.081268
3492.390186	280084.959815	51.086273
3491.785120	278271.359414	51.091277
3491.609407	276436.097645	51.096282
3491.468552	274586.908391	51.101287
3491.375937	272709.070422	51.106292
3490.811276	270824.855752	51.111297
3490.377395	268928.712849	51.116301
3490.329311	267025.591303	51.121306
3489.910533	265106.275136	51.126311
3489.271560	263162.921467	51.131316
3488.992697	261214.584745	51.136321
3489.161739	259265.428524	51.141325
3488.980235	257284.265099	51.146330
3488.267580	255300.746618	51.151335
3488.215018	253300.969694	51.156340
3487.650424	251282.946239	51.161345
3487.036275	249255.105717	51.166349
3486.943314	247209.457734	51.171354
3486.571138	245161.600231	51.176359
3485.981457	243097.415739	51.181364
3486.173088	241024.987591	51.186369
3485.482573	238943.456190	51.191373
3485.377807	236848.498576	51.196378
3484.531213	234746.456103	51.201383
3483.944319	232617.754828	51.206388
3483.800864	230499.827287	51.211393
3483.291530	228361.770869	51.216397
3483.092526	226215.696701	51.221402
3482.381924	224066.815450	51.226407
3482.345060	221899.495792	51.231412
3482.178195	219727.323433	51.236417
3481.489390	217537.661818	51.241421
3480.843690	215336.936597	51.246426
3480.517117	213133.786615	51.251431
3480.119275	210917.154543	51.256436
3479.930259	208695.703881	51.261441
3478.992914	206465.400170	51.266445
3478.958469	204222.731472	51.271450
3478.335212	201982.302446	51.276455
3477.708417	199719.181261	51.281460
3477.330852	197454.026513	51.286465
3476.272485	195188.145615	51.291469
3475.727615	192904.193184	51.296474
3475.294302	190618.444579	51.301479
3474.813648	188333.589979	51.306484
3474.533547	186050.875241	51.311489
3473.779061	183753.849218	51.316493
3473.041977	181442.903475	51.321498
3472.603290	179143.240780	51.326503
3472.242084	176827.110679	51.331508
3471.481362	174508.328696	51.336513
3470.936011	172189.795897	51.341517
3470.390128	169863.613392	51.346522
3469.859103	167536.499872	51.351527
3469.283503	165200.225438	51.356532
3468.932460	162850.589098	51.361537
3467.966234	160508.714477	51.366541
3468.135730	158150.481681	51.371546
3466.725597	155799.520466	51.376551
3465.870573	153441.110114	51.381556
3465.528506	151077.055435	51.386561
3464.929309	148716.698619	51.391565
3464.239202	146354.381014	51.396570
3463.590365	143970.706943	51.401575
3463.141995	141537.013142	51.406580
3462.310737	139171.233850	51.411585
3461.522283	136793.532045	51.416589
3460.963945	134427.638211	51.421594
3460.042817	132058.745580	51.426599
3459.265838	129675.206287	51.431604
3458.597054	127298.192059	51.436609
3457.691486	124930.991305	51.441613
3457.066273	122550.391562	51.446618
3456.186748	120186.258801	51.451623
3455.764975	117816.759440	51.456628
3454.983148	115447.334938	51.461633
3453.946960	113083.699193	51.466637
3453.801668	110707.356343	51.471642
3452.649593	108339.198173	51.476647
3451.955970	105969.807162	51.481652
3450.878394	103614.872783	51.486657
3449.898738	101248.398549	51.491661
3449.084373	98888.095794	51.496666
3448.174992	96540.579853	51.501671
3447.390449	94203.724905	51.506676
3446.343592	91853.736614	51.511681
3444.712431	89526.756467	51.516685
3444.072765	87206.516941	51.521690
3443.142271	84890.573684	51.526695
3442.281444	82583.681718	51.531700
3441.287462	80276.875618	51.536705
3439.797705	77997.707533	51.541709
3438.864045	75715.800325	51.546714
3437.636274	73452.012475	51.551719
3436.527011	71186.267370	51.556724
3435.830515	68943.325219	51.561729
3434.414599	66712.484845	51.566733
3433.634508	64482.060558	51.571738
3431.857966	62271.657227	51.576743
3430.667939	60063.922859	51.581748
3429.875665	57893.215160	51.586753
3428.649712	55719.125407	51.591757
3427.292019	53559.989691	51.596762
3425.784972	51413.788149	51.601767
3424.443859	49291.979655	51.606772
3423.339392	47183.024009	51.611777
3421.767326	45090.158295	51.616781
3420.561102	43018.989430	51.621786
3419.231751	40970.295659	51.626791
3417.616788	38934.123375	51.631796
3416.358378	36934.352619	51.636801
3414.447266	34938.496070	51.641805
3413.174950	32966.760833	51.646810
3411.287388	31029.659279	51.651815
3409.463197	29108.529046	51.656820
3407.720447	27216.120076	51.661825
3405.129901	25363.931241	51.666829
3403.328196	23540.119922	51.671834
3400.567249	21771.436950	51.676839
3397.249014	20063.595142	51.681844
3391.214339	18489.966624	51.686849
3384.253819	17000.581320	51.691853
3378.331957	15584.670397	51.696858
3371.753462	14307.079767	51.701863
3365.581820	13145.432705	51.706868
3359.603368	12103.074134	51.711873
3353.725597	11183.140154	51.716877
3348.623543	10360.865601	51.721882
3344.018525	9656.895863	51.726887
3339.486071	9041.796518	51.731892
3335.921378	8522.116962	51.736897
3332.301132	8079.221996	51.741901
3330.103928	7716.885652	51.746906
3327.542398	7428.509542	51.751911
3325.287251	7196.455592	51.756916
3323.872218	7006.768423	51.761921
3322.061101	6872.618200	51.766925
3321.606015	6756.986198	51.771930
3320.348175	6690.502905	51.776935
3319.791411	6636.646399	51.781940
3319.349297	6607.354731	51.786945
3319.098428	6588.644280	51.791949
3318.513265	6588.910886	51.796954
3318.078422	6603.719289	51.801959
3317.823825	6608.921622	51.806964
3317.928952	6631.293146	51.811969
3317.864020	6669.359874	51.816973
3318.029474	6687.396321	51.821978
3318.076390	6717.418278	51.826983
3317.908586	6732.972546	51.831988
3317.455322	6766.562204	51.836993
3317.567494	6784.781615	51.841997
3317.827443	6802.152054	51.847002
3317.216088	6821.889082	51.852007
3317.564294	6832.392259	51.857012
3317.477588	6825.184438	51.862017
3317.488841	6831.627997	51.867021
3317.347646	6823.170559	51.872026
3317.159194	6815.876660	51.877031
3317.465940	6794.300133	51.882036
3317.238932	6770.093205	51.887041
3316.768566	6745.462701	51.892045
3316.765383	6694.862500	51.897050
3316.463454	6663.842429	51.902055
3316.680215	6607.074642	51.907060
3316.699246	6553.469139	51.912065
3316.111440	6499.379096	51.917069
3315.801817	6433.385667	51.922074
3314.891863	6384.774401	51.927079
3314.573303	6310.151626	51.932084
3314.148618	6259.035637	51.937089
3313.354582	6190.352313	51.942093
3313.459531	6119.399168	51.947098
3312.425398	6054.494567	51.952103
3311.565316	5981.542175	51.957108
3311.380014	5902.309305	51.962113
3310.375651	5838.294488	51.967117
3310.405921	5768.639773	51.972122
3309.554953	5711.568702	51.977127
3309.247455	5641.721894	51.982132
3308.601809	5573.566315	51.987137
3308.106373	5488.475776	51.992141
3307.298573	5398.950281	51.997146
3306.590025	5326.654943	52.002151
3306.250132	5253.075270	52.007156
3305.813071	5185.852323	52.012161
3304.946376	5118.403753	52.017165
3304.748376	5045.054296	52.022170
3303.910798	4958.931290	52.027175
3303.409749	4874.540708	52.032180
3302.877942	4799.257006	52.037185
3301.814548	4719.107608	52.042189
3301.513814	4633.818586	52.047194
3300.858875	4561.853175	52.052199
3299.952721	4478.578640	52.057204
3299.570520	4420.538996	52.062209
3298.810949	4340.821304	52.067213
3298.160865	4245.210706	52.072218
3297.458328	4183.755291	52.077223
3297.241791	4103.944442	52.082228
3296.369630	4028.864669	52.087233
3295.814548	3949.098217	52.092237
3295.157497	3874.822611	52.097242
3294.623613	3796.856063	52.102247
3294.178891	3718.461686	52.107252
3293.633274	3629.584397	52.112257
3292.732240	3548.065276	52.117261
3292.404726	3471.750139	52.122266
3291.664144	3401.784998	52.127271
3290.654195	3317.709926	52.132276
3290.313320	3237.518023	52.137281
3289.604503	3159.541856	52.142285
3289.125860	3073.547795	52.147290
3288.417731	2997.796624	52.152295
3287.662274	2914.529043	52.157300
3287.121716	2831.060164	52.162305
3285.947336	2749.017826	52.167309
3285.359073	2672.627122	52.172314
3284.578532	2608.475770	52.177319
3284.228393	2527.013879	52.182324
3283.394098	2451.066594	52.187329
3282.345068	2394.325545	52.192333
3281.962310	2312.735317	52.197338
3281.392430	2244.052090	52.202343
3280.555469	2173.141645	52.207348
3279.862936	2103.808857	52.212353
3279.172989	2039.364055	52.217357
3278.656949	1963.129468	52.222362
3278.009058	1906.372974	52.227367
3277.476846	1834.106088	52.232372
3277.103338	1766.883632	52.237377
3275.802049	1701.171645	52.242381
3275.287892	1627.967022	52.247386
3274.852793	1567.346958	52.252391
3273.924656	1503.892083	52.257396
3273.156495	1445.184382	52.262401
3272.294025	1382.661470	52.267405
3271.760704	1318.623156	52.272410
3270.829509	1272.865585	52.277415
3270.364089	1217.777075	52.282420
3269.983469	1137.881341	52.287425
3269.091479	1093.701744	52.292429
3268.291831	1029.592472	52.297434
3267.108072	975.640463	52.302439
3266.117787	921.970992	52.307444
3265.824701	877.033622	52.312449
3265.140340	840.722113	52.317453
3264.750030	790.847532	52.322458
3264.102761	732.899498	52.327463
3263.149293	684.435171	52.332468
3262.725159	636.263860	52.337473
3261.667131	594.314329	52.342477
3261.633003	553.451973	52.347482
3260.810770	506.659605	52.352487
3260.066121	447.294393	52.357492
3259.036389	400.964501	52.362497
3258.604766	366.761436	52.367501
3257.977941	330.356813	52.372506
3257.296828	294.384702	52.377511
3256.467791	250.105951	52.382516
3255.764090	197.184215	52.387521
3254.696988	158.938004	52.392525
3254.019927	115.866411	52.397530
3253.463894	93.820725	52.402535
3252.912282	78.443624	52.407540
3252.368303	41.399091	52.412545
3251.593626	22.040262	52.417549
3250.587965	-10.161329	52.422554
3249.160606	-26.053432	52.427559
3247.043562	-13.042018	52.432564
3245.957833	-12.886137	52.437569
3244.820711	3.536459	52.442573
3245.029983	6.909557	52.447578
3244.361177	10.058859	52.452583
3244.721521	16.956311	52.457588
3244.356658	12.369962	52.462593
3242.921772	34.354223	52.467597
3242.213368	38.835391	52.472602
3241.555524	46.903880	52.477607
3241.030240	45.146696	52.482612
3240.703762	53.147920	52.487617
3239.306735	64.423934	52.492621
3239.334665	63.844047	52.497626
3238.464852	67.122435	52.502631
3238.091816	78.849953	52.507636
3237.359232	68.490371	52.512641
3236.537998	76.734811	52.517645
3236.105084	77.816115	52.522650
3235.430607	81.453100	52.527655
3234.956260	85.663775	52.532660
3234.125307	87.463197	52.537665
3233.821417	100.045343	52.542669
3233.021675	101.500363	52.547674
3232.555524	102.753528	52.552679
3231.323214	100.861738	52.557684
3231.374315	93.857254	52.562689
3230.310888	109.895931	52.567693
3229.461705	107.727113	52.572698
3228.948831	102.208812	52.577703
3228.342146	109.101777	52.582708
3228.304834	112.520181	52.587713
3227.190196	117.190376	52.592717
3226.983211	108.128051	52.597722
3226.462263	116.809884	52.602727
3224.907915	127.028897	52.607732
3224.820843	114.251031	52.612737
3223.881802	126.363038	52.617741
3223.542994	120.493684	52.622746
3222.940446	120.165188	52.627751
3222.057556	122.179536	52.632756
3221.703204	120.961156	52.637761
3220.750843	127.202676	52.642765
3220.405802	119.050885	52.647770
3219.874848	125.643952	52.652775
3219.225064	127.477559	52.657780
3218.358437	119.543164	52.662785
3217.549151	135.877915	52.667789
3216.878005	122.177877	52.672794
3216.129829	128.391224	52.677799
3215.358616	131.053585	52.682804
3214.723973	122.028396	52.687809
3214.416008	126.162105	52.692813
3213.678029	115.636054	52.697818
3212.932931	121.115073	52.702823
3212.382164	132.987070	52.707828
3211.969534	120.035484	52.712833
3211.082708	131.347144	52.717837
3211.158037	124.455742	52.722842
3210.474239	126.698967	52.727847
3209.428002	123.378053	52.732852
3208.243237	129.189552	52.737857
3207.230302	129.204322	52.742861
3206.911253	131.247867	52.747866
3206.749989	133.770103	52.752871
3206.329037	130.839719	52.757876
3205.790403	133.481293	52.762881
3204.817743	132.786566	52.767885
3203.768304	128.169517	52.772890
3202.957125	128.559152	52.777895
3202.910572	134.578029	52.782900
3202.149620	126.007830	52.787905
3201.037135	133.830755	52.792909
3201.076994	125.270581	52.797914
3200.782972	129.495065	52.802919
3199.808946	132.863116	52.807924
3198.834362	125.025718	52.812929
3197.465127	131.786084	52.817933
3197.370107	123.900651	52.822938
3196.629393	135.539054	52.827943
3195.865728	135.353348	52.832948
3195.568098	123.546564	52.837953
3194.781474	130.778169	52.842957
3194.445887	125.154577	52.847962
3193.240979	130.499005	52.852967
3192.677210	141.131019	52.857972
3192.749882	126.360898	52.862977
3191.769194	127.008832	52.867981
3191.254027	127.395657	52.872986
3190.120426	120.863955	52.877991
3189.184179	133.714027	52.882996
3189.360971	131.461504	52.888001
3188.651293	134.412559	52.893005
3187.980464	127.877184	52.898010
3186.912812	132.578440	52.903015
3185.543466	129.202998	52.908020
3186.071451	130.095667	52.913025
3185.215777	136.418962	52.918029
3184.848898	134.729050	52.923034
3184.151836	138.304385	52.928039
3182.776814	130.850001	52.933044
3181.799697	121.926354	52.938049
3181.418275	136.250680	52.943053
3181.455801	136.435319	52.948058
3180.623844	138.463867	52.953063
3179.596461	130.114450	52.958068
3179.265225	130.485246	52.963073
3178.764869	132.593715	52.968077
3178.486739	133.317010	52.973082
3178.036858	135.368699	52.978087
3176.886149	136.136471	52.983092
3175.604904	132.007836	52.988097
3175.192981	141.728137	52.993101
3174.542691	134.121513	52.998106
3173.661132	132.163491	53.003111
3172.735979	130.276074	53.008116
3172.555277	128.078314	53.013121
3172.117687	136.943675	53.018125
3171.826975	130.188231	53.023130
3170.871921	128.486708	53.028135
3170.155099	130.467559	53.033140
3169.541683	122.737802	53.038145
3168.081524	136.411976	53.043149
3167.718480	123.909019	53.048154
3167.186796	126.767298	53.053159
3166.494761	126.242917	53.058164
3166.245674	128.607661	53.063169
3165.300637	133.601780	53.068173
3164.529249	124.933902	53.073178
3164.217982	124.086709	53.078183
3164.122345	136.059759	53.083188
3163.291728	128.999464	53.088193
3161.811552	123.379594	53.093197
3161.573958	131.149752	53.098202
3161.609379	133.214446	53.103207
3160.377333	139.898488	53.108212
3159.557314	129.512771	53.113217
3158.782144	128.563658	53.118221
3158.258946	123.814869	53.123226
3157.416048	120.899741	53.128231
3156.600215	132.699000	53.133236
3156.075692	119.214713	53.138241
3155.090823	130.708911	53.143245
3155.139384	125.896382	53.148250
3154.568158	125.670697	53.153255
3153.811469	134.220715	53.158260
3153.465851	120.768228	53.163265
3152.455520	131.271668	53.168269
3151.635146	123.917529	53.173274
3150.615503	121.827187	53.178279
3149.840830	133.373498	53.183284
3148.980228	119.542037	53.188289
3148.628003	130.612758	53.193293
3149.207063	130.700925	53.198298
3148.264962	131.532138	53.203303
3146.610500	132.920050	53.208308
3146.413263	132.025745	53.213313
3146.073909	137.285849	53.218317
3145.574160	128.664323	53.223322
3144.213012	122.587159	53.228327
3143.585148	125.956071	53.233332
3143.466338	125.974398	53.238337
3142.776163	132.041265	53.243341
3142.239326	139.061651	53.248346
3141.461018	135.314848	53.253351
3140.058560	132.899921	53.258356
3139.452482	121.850438	53.263361
3139.035669	129.645295	53.268365
3138.593696	124.410141	53.273370
3138.270194	131.411047	53.278375
3137.543250	131.964321	53.283380
3136.356592	121.906909	53.288385
3135.561945	128.290039	53.293389
3134.991731	128.245363	53.298394
3134.476921	121.634003	53.303399
3133.574678	125.710964	53.308404
3133.222156	115.117891	53.313409
3133.013636	131.503539	53.318413
3131.947904	118.755135	53.323418
3131.050657	123.099262	53.328423
3130.664496	120.476356	53.333428
3130.641811	113.812890	53.338433
3129.082171	122.430620	53.343437
3128.653645	121.451890	53.348442
3128.564968	115.411131	53.353447
3126.796903	125.792198	53.358452
3126.551427	121.457399	53.363457
3125.889461	128.690603	53.368461
3125.330431	121.679441	53.373466
3124.877169	123.007383	53.378471
3124.164794	121.272696	53.383476
3123.275240	110.754806	53.388481
3122.502667	124.330045	53.393485
3121.545629	122.411771	53.398490
3121.579424	122.042455	53.403495
3120.666831	117.620330	53.408500
3120.387263	116.900354	53.413505
3119.666617	119.738420	53.418509
3118.982099	112.962252	53.423514
3118.649080	116.512886	53.428519
3117.402780	116.366628	53.433524
3116.936980	113.753385	53.438529
3115.943437	126.464824	53.443533
3115.063818	118.542147	53.448538
3114.264705	117.649236	53.453543
3113.677062	126.677592	53.458548
3114.232275	116.810063	53.463553
3112.860867	124.976041	53.468557
3112.074487	116.694811	53.473562
3111.498835	113.752978	53.478567
3110.456284	120.461483	53.483572
3110.853458	114.183375	53.488577
3109.948949	124.137034	53.493581
3108.815610	116.774803	53.498586
3108.095592	119.377901	53.503591
3107.184314	124.947294	53.508596
3107.653788	110.259795	53.513601
3106.065557	114.585803	53.518605
3105.375621	113.483586	53.523610
3105.158472	117.087448	53.528615
3104.709489	117.865989	53.533620
3104.043123	115.099916	53.538625
3102.913765	121.792070	53.543629
3102.484928	123.488859	53.548634
3101.833129	124.232977	53.553639
3100.619153	121.038639	53.558644
3099.984147	119.149818	53.563649
3099.084485	121.182047	53.568653
3099.429295	119.777507	53.573658
3098.621572	124.207786	53.578663
3097.615997	122.715826	53.583668
3096.533272	118.904604	53.588673
3096.485360	122.294423	53.593677
3096.358787	122.227632	53.598682
3095.128755	116.211764	53.603687
3094.256366	119.462989	53.608692
3093.913070	112.099588	53.613697
3092.624482	121.052317	53.618701
3092.012296	118.990655	53.623706
3092.656348	121.657125	53.628711
3091.335598	121.698063	53.633716
3090.948808	119.494864	53.638721
3089.634187	122.806652	53.643725
3089.078832	119.667541	53.648730
3088.986174	116.916335	53.653735
3088.187175	120.081601	53.658740
3087.602056	113.837915	53.663745
3086.671197	125.115257	53.668749
3085.260269	117.230871	53.673754
3085.098657	113.589495	53.678759
3084.679011	114.772752	53.683764
3084.398805	113.305273	53.688769
3082.921691	120.553416	53.693773
3082.212343	123.581000	53.698778
3082.212627	116.976373	53.703783
3081.063147	119.982056	53.708788
3080.780318	109.141831	53.713793
3079.529681	118.370700	53.718797
3078.994290	113.850977	53.723802
3079.201736	105.879938	53.728807
3078.344487	119.030309	53.733812
3077.622933	122.336683	53.738817
3076.242353	116.936661	53.743821
3075.548573	117.582168	53.748826
3075.223204	117.305404	53.753831
3074.228045	124.475147	53.758836
3074.117268	111.245052	53.763841
3073.246107	122.220094	53.768845
3072.343665	119.692515	53.773850
3072.722231	115.600823	53.778855
3071.732386	122.230066	53.783860
3071.153498	113.457878	53.788865
3070.332358	118.524777	53.793869
3069.733493	113.159343	53.798874
3068.985294	111.450917	53.803879
3067.544226	111.156375	53.808884
3068.039404	112.101610	53.813889
3066.478664	121.339655	53.818893
3065.497384	112.269128	53.823898
3065.210479	114.317446	53.828903
3065.326460	124.079369	53.833908
3064.760639	113.776565	53.838913
3063.099583	116.441384	53.843917
3062.078581	117.916075	53.848922
3062.127995	124.317612	53.853927
3061.654686	121.555266	53.858932
3061.118390	122.549250	53.863937
3059.636835	128.159646	53.868941
3059.073924	124.546183	53.873946
3059.215725	111.302143	53.878951
3058.066331	120.730027	53.883956
3057.670390	110.020840	53.888961
3056.685936	120.970636	53.893965
3056.321983	121.883858	53.898970
3056.086968	113.720005	53.903975
3054.847596	114.095590	53.908980
3054.485878	108.046628	53.913985
3054.009522	114.813123	53.918989
3053.383089	114.491490	53.923994
3052.415217	118.261127	53.928999
3051.102195	118.234045	53.934004
3050.765059	109.144246	53.939009
3050.325693	112.146619	53.944013
3049.507891	115.705091	53.949018
3049.019595	106.224686	53.954023
3048.236537	122.931110	53.959028
3048.315423	109.097443	53.964033
3047.290264	110.636003	53.969037
3046.619251	108.203093	53.974042
3046.078682	105.638950	53.979047
3044.451956	109.933261	53.984052
3044.386152	106.907477	53.989057
3043.091726	121.935665	53.994061
3043.226673	113.360843	53.999066
3042.522232	111.774019	54.004071
3041.183502	106.023448	54.009076
3041.213011	106.754179	54.014081
3040.314304	115.721605	54.019085
3039.605826	119.127192	54.024090
3038.695984	111.437064	54.029095
3038.058811	117.366588	54.034100
3038.243497	98.716944	54.039105
3037.514444	110.187551	54.044109
3036.982285	113.154466	54.049114
3036.713202	110.731034	54.054119
3034.926005	111.285493	54.059124
3034.401919	103.660109	54.064129
3033.006760	114.946126	54.069133
3033.010337	115.890888	54.074138
3032.832800	108.927847	54.079143
3031.478038	105.587853	54.084148
3031.010747	107.333056	54.089153
3030.158736	109.441227	54.094157
3030.120138	112.581167	54.099162
3029.333722	114.624842	54.104167
3028.662419	113.539187	54.109172
3028.261388	111.934072	54.114177
3027.148666	119.634288	54.119181
3026.790769	112.920349	54.124186
3026.054171	108.209233	54.129191
3025.385266	116.042026	54.134196
3024.595645	109.620933	54.139201
3023.434517	107.499138	54.144205
3023.158659	115.857254	54.149210
3022.825420	110.867613	54.154215
3021.512551	118.071911	54.159220
3020.808745	101.637723	54.164225
3020.553471	102.420669	54.169229
3020.628059	108.107385	54.174234
3019.513014	107.833723	54.179239
3018.539555	110.060935	54.184244
3018.023826	101.562175	54.189249
3017.595698	112.719264	54.194253
3017.085249	111.689412	54.199258
3016.215733	111.922466	54.204263
3014.605491	112.451036	54.209268
3014.683776	104.068661	54.214273
3013.971401	118.726211	54.219277
3013.142264	110.871908	54.224282
3012.493170	105.196524	54.229287
3011.789248	116.502187	54.234292
3011.438084	111.839287	54.239297
3010.779074	108.987105	54.244301
3009.905139	109.120259	54.249306
3009.750656	106.818164	54.254311
3008.810940	108.623964	54.259316
3008.861484	110.523044	54.264321
3007.877856	105.774014	54.269325
3006.635994	107.775520	54.274330
3005.947301	109.550268	54.279335
3005.254306	110.519324	54.284340
3004.647022	105.351126	54.289345
3003.920152	109.955879	54.294349
3003.357001	118.016912	54.299354
3003.070108	101.135708	54.304359
3002.228766	106.633945	54.309364
3001.862318	105.782773	54.314369
3001.252191	109.657858	54.319373
3000.187702	108.646894	54.324378
2999.864180	111.783812	54.329383
2998.319140	109.768677	54.334388
2998.077908	107.063391	54.339393
2997.376674	114.859868	54.344397
2996.813459	108.884423	54.349402
2996.554434	99.444194	54.354407
2995.845479	113.088285	54.359412
2995.249801	109.423198	54.364417
2994.353981	103.915107	54.369421
2993.844272	104.948368	54.374426
2993.112667	108.485405	54.379431
2991.911192	113.246258	54.384436
2991.514580	106.363684	54.389441
2990.711306	108.951413	54.394445
2990.063314	112.463111	54.399450
2990.142563	102.767713	54.404455
2989.334638	114.039437	54.409460
2988.629410	97.007496	54.414465
2987.301605	107.490182	54.419469
2986.297259	104.180318	54.424474
2986.160157	106.664080	54.429479
2985.382170	114.270783	54.434484
2984.777616	102.940831	54.439489
2984.126007	113.916246	54.444493
2984.057168	110.800590	54.449498
2983.119200	108.676985	54.454503
2982.424240	110.793455	54.459508
2982.092514	103.778614	54.464513
2981.283936	106.649086	54.469517
2980.631317	107.125336	54.474522
2979.914795	105.626637	54.479527
2978.635574	107.856369	54.484532
2978.047331	95.935494	54.489537
2977.535088	105.592385	54.494541
2976.667812	113.113296	54.499546
2976.811768	102.053718	54.504551
2976.083635	107.750107	54.509556
2975.656171	106.643712	54.514561
2975.072137	110.007905	54.519565
2973.923404	102.733611	54.524570
2973.174918	100.058958	54.529575
2971.945092	110.848581	54.534580
2971.863552	97.361289	54.539585
2971.289737	100.883203	54.544589
2970.632301	103.338648	54.549594
2970.254473	105.006199	54.554599
2969.114916	114.309647	54.559604
2968.100434	103.712102	54.564609
2967.356821	107.357768	54.569613
2967.037367	109.621251	54.574618
2966.368500	105.816706	54.579623
2965.957806	108.467217	54.584628
2965.416291	98.720407	54.589633
2964.829426	103.490310	54.594637
2964.030465	112.077545	54.599642
2963.569343	100.648487	54.604647
2962.838309	105.280004	54.609652
2961.912091	103.411758	54.614657
2961.061994	98.515978	54.619661
2960.330344	108.652852	54.624666
2960.050604	103.980912	54.629671
2959.409285	115.924807	54.634676
2958.873556	104.764278	54.639681
2958.379761	107.864769	54.644685
2957.143952	111.422052	54.649690
2956.674494	102.067918	54.654695
2955.498675	113.700924	54.659700
2954.921730	103.158873	54.664705
2954.604023	103.456713	54.669709
2954.156258	108.929539	54.674714
2953.486779	102.538458	54.679719
2953.061139	103.299204	54.684724
2952.523285	99.453328	54.689729
2951.260044	111.591127	54.694733
2950.429816	107.582455	54.699738
2949.709862	109.010060	54.704743
2949.251578	114.325610	54.709748
2948.770493	105.040171	54.714753
2947.955925	108.241662	54.719757
2948.093438	117.818707	54.724762
2947.886109	101.758766	54.729767
2946.500980	103.490694	54.734772
2945.538077	99.547328	54.739777
2944.682431	104.306718	54.744781
2943.914689	104.122926	54.749786
2943.883924	103.068345	54.754791
2942.763710	98.427934	54.759796
2941.679163	97.041078	54.764801
2941.199421	109.672995	54.769805
2940.245282	103.394113	54.774810
2939.839351	103.304015	54.779815
2939.209843	111.609668	54.784820
2938.787079	96.993355	54.789825
2938.656636	100.503450	54.794829
2938.003871	102.554688	54.799834
2937.296942	98.311008	54.804839
2936.197735	99.653428	54.809844
2935.429463	102.601488	54.814849
2934.360501	100.934083	54.819853
2933.962087	102.654494	54.824858
2933.716699	103.273521	54.829863
2932.797820	102.859776	54.834868
2932.324779	101.628546	54.839873
2931.407178	106.936537	54.844877
2930.795361	110.122723	54.849882
2931.118433	106.874177	54.854887
2929.895732	99.128997	54.859892
2928.532340	99.687640	54.864897
2927.995136	95.447326	54.869901
2927.234005	97.876284	54.874906
2927.524866	95.417960	54.879911
2926.761985	101.803164	54.884916
2925.711684	98.619981	54.889921
2924.650904	109.531899	54.894925
2923.478036	102.011881	54.899930
2923.886180	100.352571	54.904935
2922.842016	105.631272	54.909940
2922.414611	100.054991	54.914945
2921.595254	98.148360	54.919949
2921.170727	106.277274	54.924954
2920.804202	103.981422	54.929959
2920.641590	109.059738	54.934964
2919.102182	95.874883	54.939969
2918.525593	95.046208	54.944973
2917.719500	100.078966	54.949978
2917.621446	94.727448	54.954983
2916.055653	94.870696	54.959988
2915.256267	95.777418	54.964993
2914.440497	97.592838	54.969997
2914.295445	98.202612	54.975002
2913.810173	94.091184	54.980007
2912.970713	95.199750	54.985012
2912.765675	93.950748	54.990017
2912.376196	101.399478	54.995021
2911.708921	95.791958	55.000026
2910.838938	101.342068	55.005031
2909.443134	98.491873	55.010036
2909.117324	102.553630	55.015041
2908.715600	97.000594	55.020045
2908.061210	95.319582	55.025050
2907.275232	97.436613	55.030055
2905.793474	95.992519	55.035060
2905.042041	95.734895	55.040065
2905.008338	96.537609	55.045069
2904.918520	100.682190	55.050074
2904.090169	89.896552	55.055079
2903.211873	99.796779	55.060084
2902.822250	98.055125	55.065089
2902.246761	100.188289	55.070093
2901.088700	101.674586	55.075098
2900.103985	89.628469	55.080103
2899.276903	95.500448	55.085108
2899.128808	102.527411	55.090113
2898.773298	97.598830	55.095117
2897.830390	100.649762	55.100122
2897.479912	92.491462	55.105127
2896.653059	96.893838	55.110132
2896.270230	93.989346	55.115137
2895.520512	96.070182	55.120141
2894.099787	95.187224	55.125146
2893.645637	92.157161	55.130151
2893.374969	97.802608	55.135156
2893.004772	94.967007	55.140161
2892.478397	100.335637	55.145165
2891.409344	105.180449	55.150170
2890.828858	98.504180	55.155175
2889.994399	104.385319	55.160180
2889.433947	94.204801	55.165185
2888.957251	88.256437	55.170189
2888.369489	90.174204	55.175194
2886.921909	91.826425	55.180199
2885.741470	94.330599	55.185204
2886.120164	98.779180	55.190209
2885.825731	91.150895	55.195213
2884.365233	98.575824	55.200218
2884.124484	91.771237	55.205223
2883.394699	96.910162	55.210228
2882.809721	87.150673	55.215233
2882.308146	93.868973	55.220237
2881.824422	98.921243	55.225242
2880.588928	81.905765	55.230247
2879.753174	99.901653	55.235252
2879.484269	84.521329	55.240257
2878.950827	93.006734	55.245261
2878.350470	90.951371	55.250266
2878.207467	90.449248	55.255271
2876.367960	94.843115	55.260276
2875.821706	92.005632	55.265281
2875.104233	84.392020	55.270285
2874.559267	96.202593	55.275290
2874.512999	90.833545	55.280295
2873.664019	94.907346	55.285300
2873.277993	95.939214	55.290305
2872.069340	102.434946	55.295309
2871.111730	100.625764	55.300314
2870.553929	94.482451	55.305319
2870.059183	93.991890	55.310324
2869.517522	89.915368	55.315329
2869.311390	97.389208	55.320333
2868.517717	94.644535	55.325338
2867.941742	91.485299	55.330343
2866.576347	93.454260	55.335348
2865.432499	89.666965	55.340353
2864.996593	97.975051	55.345357
2864.713305	96.610743	55.350362
2864.702899	84.410760	55.355367
2864.077405	94.805792	55.360372
2863.548459	93.125452	55.365377
2862.566767	100.375401	55.370381
2861.128702	97.821381	55.375386
2860.934034	98.837520	55.380391
2859.915454	103.923966	55.385396
2859.587708	97.541210	55.390401
2859.122072	95.768342	55.395405
2858.741054	97.227239	55.400410
2858.000356	88.461051	55.405415
2856.540016	102.953524	55.410420
2856.124203	98.091305	55.415425
2855.661333	95.230100	55.420429
2855.177713	90.626965	55.425434
2855.123671	93.791640	55.430439
2853.572663	92.460445	55.435444
2852.577289	91.235206	55.440449
2851.947746	91.882784	55.445453
2851.212471	96.411220	55.450458
2851.190218	90.614529	55.455463
2850.691844	96.669538	55.460468
2850.319651	95.192140	55.465473
2849.488284	101.203801	55.470477
2848.229511	94.395577	55.475482
2848.050197	89.410444	55.480487
2846.935681	93.397790	55.485492
2846.346635	91.106425	55.490497
2845.935582	90.450383	55.495501
2845.397278	91.962607	55.500506
2844.403687	94.769583	55.505511
2843.711668	99.352204	55.510516
2843.359537	91.245511	55.515521
2842.706540	92.826678	55.520525
2842.038720	92.310832	55.525530
2841.221296	85.707439	55.530535
2839.742933	86.870341	55.535540
2839.197383	93.530632	55.540545
2838.666156	87.113187	55.545549
2838.707742	93.409455	55.550554
2838.225661	90.441013	55.555559
2837.315659	89.618411	55.560564
2836.929375	94.402588	55.565569
2836.286104	92.829024	55.570573
2834.942826	97.078490	55.575578
2834.642483	85.838300	55.580583
2833.175355	104.372349	55.585588
2833.168812	102.101426	55.590593
2832.803834	93.970481	55.595597
2832.305590	100.875710	55.600602
2831.512133	93.642579	55.605607
2830.001864	94.138718	55.610612
2829.871919	97.814905	55.615617
2829.100995	100.530935	55.620621
2828.138403	96.180578	55.625626
2828.189174	90.670611	55.630631
2827.721423	98.884274	55.635636
2827.345385	93.376990	55.640641
2826.124381	93.153843	55.645645
2825.368449	96.761364	55.650650
2824.519866	91.935616	55.655655
2824.004489	96.369235	55.660660
2823.714941	96.447144	55.665665
2822.393805	94.439583	55.670669
2821.785819	99.003107	55.675674
2821.351843	93.472964	55.680679
2820.679389	96.509260	55.685684
2820.461290	95.518277	55.690689
2819.949012	95.759380	55.695693
2818.739684	95.642789	55.700698
2818.303653	92.586349	55.705703
2817.322392	98.712443	55.710708
2817.233316	100.165260	55.715713
2816.000857	93.486360	55.720717
2814.980322	100.424803	55.725722
2814.334531	90.417964	55.730727
2813.902025	94.396117	55.735732
2813.438006	93.917283	55.740737
2812.912288	93.733986	55.745741
2812.212024	94.388130	55.750746
2811.782323	90.870754	55.755751
2810.698064	88.846395	55.760756
2809.738741	86.509771	55.765761
2809.370172	85.839366	55.770765
2808.444933	94.482917	55.775770
2807.986201	88.452549	55.780775
2807.381984	87.859524	55.785780
2806.992786	84.300886	55.790785
2806.655337	83.160176	55.795789
2805.450988	91.887349	55.800794
2804.824299	87.952077	55.805799
2804.210997	87.316790	55.810804
2803.601749	95.990411	55.815809
2803.097715	92.102462	55.820813
2802.342470	96.593263	55.825818
2801.406382	81.556720	55.830823
2800.724357	89.603322	55.835828
2800.141873	83.599634	55.840833
2799.817124	94.295359	55.845837
2799.098562	86.482217	55.850842
2798.535030	84.294259	55.855847
2797.436179	90.830834	55.860852
2796.787394	95.043710	55.865857
2796.433971	82.519875	55.870861
2795.257933	88.613340	55.875866
2795.177023	76.408844	55.880871
2794.272867	81.017853	55.885876
2793.297613	76.598229	55.890881
2792.748316	86.854315	55.895885
2792.027536	94.311113	55.900890
2791.712079	90.624218	55.905895
2791.286454	96.772581	55.910900
2790.603960	90.296921	55.915905
2790.224649	91.648163	55.920909
2788.970318	97.065032	55.925914
2788.092241	80.904663	55.930919
2787.686910	91.765733	55.935924
2787.057753	91.167499	55.940929
2786.657161	95.015070	55.945933
2785.316878	89.714045	55.950938
2784.961017	85.143951	55.955943
2784.506976	86.400206	55.960948
2783.233113	76.912034	55.965953
2783.320408	91.170776	55.970957
2782.543183	90.704030	55.975962
2782.314042	86.182145	55.980967
2780.916436	95.258529	55.985972
2780.578561	87.514136	55.990977
2779.992151	88.851830	55.995981
2779.375301	96.149554	56.000986
2778.276146	87.048743	56.005991
2777.291644	93.835374	56.010996
2776.699973	92.914954	56.016001
2776.266190	92.936203	56.021005
2775.772172	96.094764	56.026010
2775.343219	86.686777	56.031015
2774.631757	90.691294	56.036020
2774.103177	89.475888	56.041025
2773.357668	88.651234	56.046029
2771.874026	86.232528	56.051034
2771.688394	84.259843	56.056039
2770.902957	88.827250	56.061044
2770.437175	96.540063	56.066049
2770.285722	83.919740	56.071053
2769.565501	93.745190	56.076058
2768.557757	85.897010	56.081063
2767.658947	92.347689	56.086068
2767.303900	83.666789	56.091073
2766.968199	85.510300	56.096077
2766.100383	87.449103	56.101082
2765.061177	83.398035	56.106087
2763.946672	86.458575	56.111092
2763.877062	85.118540	56.116097
2763.554385	90.651691	56.121101
2762.849531	94.303380	56.126106
2762.343930	79.454581	56.131111
2761.524166	91.538687	56.136116
2760.831525	90.678157	56.141121
2760.159845	91.556756	56.146125
2759.107166	90.569480	56.151130
2758.745281	80.405585	56.156135
2757.231051	90.195041	56.161140
2756.635002	82.831087	56.166145
2756.629538	82.018494	56.171149
2756.110257	83.045119	56.176154
2755.860737	79.206043	56.181159
2755.159199	88.118455	56.186164
2754.208999	81.315547	56.191169
2753.140785	83.918190	56.196173
2752.601764	99.421583	56.201178
2752.157905	81.137198	56.206183
2751.631148	84.730025	56.211188
2750.917587	81.152232	56.216193
2749.707799	77.666362	56.221197
2748.674264	82.713925	56.226202
2748.643531	79.219153	56.231207
2747.640323	85.148480	56.236212
2747.400057	79.498008	56.241217
2746.985134	70.063955	56.246221
2746.392568	87.060258	56.251226
2746.098231	80.097883	56.256231
2744.662157	81.520414	56.261236
2743.959776	82.177295	56.266241
2743.694117	77.779680	56.271245
2742.979330	82.119887	56.276250
2742.187482	80.641599	56.281255
2740.997052	83.510652	56.286260
2740.503173	83.829142	56.291265
2740.272302	79.727939	56.296269
2739.668559	84.750199	56.301274
2739.362080	77.669115	56.306279
2738.312998	85.872401	56.311284
2737.293422	89.694329	56.316289
2736.769243	85.214193	56.321293
2736.055347	91.493930	56.326298
2735.743421	88.610097	56.331303
2734.908444	88.959259	56.336308
2734.012592	84.985139	56.341313
2733.188708	80.243610	56.346317
2731.959265	88.660484	56.351322
2732.362100	79.811367	56.356327
2731.609162	91.786159	56.361332
2730.990629	93.899062	56.366337
2730.485022	81.137183	56.371341
2729.894514	90.375214	56.376346
2728.992991	83.161371	56.381351
2728.255748	88.605913	56.386356
2727.437123	80.647661	56.391361
2727.145637	86.154953	56.396365
2726.331357	88.201448	56.401370
2726.255431	83.286286	56.406375
2724.656078	83.930702	56.411380
2724.053740	89.985719	56.416385
2723.856930	83.237195	56.421389
2723.079391	83.604960	56.426394
2722.637752	82.056157	56.431399
2721.391371	89.577139	56.436404
2720.804584	81.351899	56.441409
2720.394723	83.842411	56.446413
2719.683417	96.204026	56.451418
2719.264025	86.154961	56.456423
2718.175753	85.952570	56.461428
2717.123716	84.661649	56.466433
2716.821120	87.681310	56.471437
2715.948785	86.402304	56.476442
2716.134748	87.819950	56.481447
2715.372483	88.499307	56.486452
2714.867627	79.866129	56.491457
2714.193742	80.911683	56.496461
2712.623248	79.755961	56.501466
2712.679696	76.166555	56.506471
2711.857071	81.196624	56.511476
2711.323559	84.785081	56.516481
2710.572127	78.833183	56.521485
2709.494787	85.383852	56.526490
2708.876377	78.476086	56.531495
2708.400951	84.606511	56.536500
2707.832183	72.545420	56.541505
2707.702277	70.757419	56.546509
2706.108775	93.650692	56.551514
2705.979843	79.660390	56.556519
2705.017253	83.543236	56.561524
2704.637150	85.695119	56.566529
2704.414482	78.821155	56.571533
2702.840553	76.488164	56.576538
2702.051282	75.580214	56.581543
2701.482021	82.011669	56.586548
2700.825358	76.212516	56.591553
2701.047192	75.108843	56.596557
2700.226864	78.356732	56.601562
2699.469104	71.655549	56.606567
2698.447112	78.145836	56.611572
2698.028846	78.001813	56.616577
2697.416293	78.367038	56.621581
2696.467089	81.537092	56.626586
2696.255089	71.515351	56.631591
2695.273762	80.456639	56.636596
2693.892496	71.080803	56.641601
2693.652477	71.010125	56.646605
2692.916962	84.116767	56.651610
2692.574174	67.799026	56.656615
2692.238409	73.347433	56.661620
2691.687543	78.281315	56.666625
2690.659609	77.746915	56.671629
2689.768088	81.659850	56.676634
2689.814966	74.683369	56.681639
2689.010007	77.797189	56.686644
2688.010062	82.496397	56.691649
2686.777009	72.596297	56.696653
2686.146985	80.308361	56.701658
2685.900053	80.649378	56.706663
2685.344464	80.089501	56.711668
2685.142458	83.874707	56.716673
2684.907308	88.795282	56.721677
2683.288523	87.380199	56.726682
2682.977767	71.313552	56.731687
2681.886172	80.677887	56.736692
2681.482665	78.866789	56.741697
2680.085738	74.353090	56.746701
2679.213069	80.493392	56.751706
2679.478871	75.629949	56.756711
2678.655115	75.595897	56.761716
2677.938656	72.590964	56.766721
2677.866405	79.851644	56.771725
2677.278469	82.830872	56.776730
2676.459106	73.717797	56.781735
2675.421257	85.239986	56.786740
2674.577381	72.324377	56.791745
2674.650366	82.181202	56.796749
2672.954837	84.225583	56.801754
2672.403837	69.781669	56.806759
2671.682521	81.646446	56.811764
2671.108023	79.408276	56.816769
2670.578398	73.375447	56.821773
2670.044746	81.573129	56.826778
2670.371645	75.126660	56.831783
2669.478238	81.712994	56.836788
2668.763388	82.822791	56.841793
2667.766576	76.269446	56.846797
2666.886585	79.936078	56.851802
2665.748091	76.315677	56.856807
2665.032728	81.799506	56.861812
2664.446442	83.799931	56.866817
2664.007201	77.844017	56.871821
2663.354291	82.966656	56.876826
2663.488217	80.759358	56.881831
2662.936361	79.353739	56.886836
2661.961156	85.609858	56.891841
2661.050415	88.779659	56.896845
2659.787791	83.806835	56.901850
2659.845635	77.594640	56.906855
2659.297464	82.644903	56.911860
2658.092906	83.476054	56.916865
2657.265559	77.158998	56.921869
2656.516193	87.570462	56.926874
2656.632823	84.587723	56.931879
2655.795544	85.527008	56.936884
2655.115076	87.106574	56.941889
2654.151460	80.901623	56.946893
2653.414444	82.368490	56.951898
2652.571687	82.529525	56.956903
2651.963725	88.017892	56.961908
2651.705602	81.168545	56.966913
2651.855708	82.385086	56.971917
2650.933867	89.769682	56.976922
2649.598185	74.044421	56.981927
2648.973560	79.769310	56.986932
2648.427937	85.230441	56.991937
2647.997278	69.578630	56.996941
2646.671118	79.429498	57.001946
2645.756368	80.170060	57.006951
2645.278078	79.821572	57.011956
2644.759557	81.446478	57.016961
2644.721275	80.641075	57.021965
2643.732940	80.606741	57.026970
2643.668561	72.219590	57.031975
2642.438992	82.007371	57.036980
2641.719228	80.152051	57.041985
2641.096305	80.897990	57.046989
2640.470784	87.372222	57.051994
2639.946406	78.555296	57.056999
2639.131102	83.517807	57.062004
2638.047483	87.994492	57.067009
2637.695458	76.399242	57.072013
2637.107706	85.946659	57.077018
2637.012560	79.496547	57.082023
2636.238510	82.743243	57.087028
2635.258517	84.595452	57.092033
2634.490391	82.774847	57.097037
2633.740355	90.597035	57.102042
2633.274388	86.894833	57.107047
2632.433833	82.552477	57.112052
2631.531961	91.343224	57.117057
2631.122181	89.444782	57.122061
2630.314736	84.019168	57.127066
2630.281421	76.667989	57.132071
2629.941103	80.989585	57.137076
2628.511085	80.384592	57.142081
2627.224362	82.027534	57.147085
2626.917831	86.345329	57.152090
2626.414923	80.961602	57.157095
2626.212700	85.492480	57.162100
2625.828174	93.278635	57.167105
2624.941987	85.173669	57.172109
2624.099067	92.267286	57.177114
2623.620221	93.168198	57.182119
2622.172606	90.212076	57.187124
2621.241525	87.276996	57.192129
2621.531127	88.314563	57.197133
2620.246528	92.983103	57.202138
2619.935368	77.197973	57.207143
2619.201486	87.437060	57.212148
2618.422286	95.181344	57.217153
2618.594764	86.180953	57.222157
2617.548987	88.735574	57.227162
2616.615372	90.973004	57.232167
2615.728926	87.709383	57.237172
2615.303290	88.279893	57.242177
2615.188445	84.561091	57.247181
2613.850090	83.010067	57.252186
2613.042414	82.754598	57.257191
2611.897865	82.617109	57.262196
2611.628467	84.485212	57.267201
2611.195338	79.524545	57.272205
2610.815012	89.927793	57.277210
2610.486966	90.654115	57.282215
2610.080428	94.310477	57.287220
2609.259838	94.474835	57.292225
2608.560314	84.560124	57.297229
2607.917274	81.507124	57.302234
2606.910307	89.028246	57.307239
2606.063928	81.825927	57.312244
2605.525338	88.022809	57.317249
2604.998009	81.871573	57.322253
2603.382194	95.163839	57.327258
2602.800917	85.308649	57.332263
2602.836628	84.989134	57.337268
2602.116436	80.917910	57.342273
2601.421875	78.955265	57.347277
2600.813770	86.363597	57.352282
2600.460254	76.807756	57.357287
2600.009541	81.307693	57.362292
2598.367898	79.373534	57.367297
2598.165941	73.635218	57.372301
2596.957154	83.886016	57.377306
2596.795591	82.901958	57.382311
2596.110711	87.744681	57.387316
2595.904005	86.930177	57.392321
2595.435086	78.094306	57.397325
2594.179952	87.115175	57.402330
2593.697488	78.662922	57.407335
2592.879868	88.242136	57.412340
2592.238870	88.021727	57.417345
2591.048358	68.202070	57.422349
2590.424656	72.975516	57.427354
2590.476424	66.680293	57.432359
2589.909597	75.602435	57.437364
2589.338398	82.053566	57.442369
2588.343806	71.459465	57.447373
2587.027591	76.117622	57.452378
2586.653988	67.145863	57.457383
2586.312763	76.856781	57.462388
2585.822493	84.647982	57.467393
2585.605266	75.912766	57.472397
2584.150694	84.092230	57.477402
2583.349548	81.767293	57.482407
2582.952823	83.311385	57.487412
2582.342454	82.216953	57.492417
2581.941388	76.858848	57.497421
2580.884629	85.142011	57.502426
2580.181241	78.476553	57.507431
2579.518487	82.533545	57.512436
2578.833155	73.370345	57.517441
2578.628666	73.286493	57.522445
2577.898693	83.684773	57.527450
2577.674100	69.880982	57.532455
2576.150907	82.223885	57.537460
2575.484266	75.460176	57.542465
2575.181616	71.910455	57.547469
2574.717287	81.859913	57.552474
2574.349382	77.773073	57.557479
2573.549878	77.245038	57.562484
2572.679853	79.938561	57.567489
2571.321860	74.963910	57.572493
2570.023610	84.415295	57.577498
2570.069761	71.515716	57.582503
2569.807659	72.001826	57.587508
2569.459749	78.890032	57.592513
2568.882869	74.061313	57.597517
2568.005747	84.616982	57.602522
2567.127580	75.972260	57.607527
2566.216288	77.239990	57.612532
2565.189817	81.181930	57.617537
2565.205302	71.214080	57.622541
2564.858873	78.796746	57.627546
2564.435040	77.290703	57.632551
2563.170722	72.106627	57.637556
2561.945860	82.028607	57.642561
2561.626912	71.044676	57.647565
2560.929609	81.416449	57.652570
2560.803518	73.024068	57.657575
2560.368639	79.010592	57.662580
2559.078217	84.507083	57.667585
2558.313302	75.843397	57.672589
2557.869312	79.726416	57.677594
2557.160659	80.515046	57.682599
2556.935462	81.632722	57.687604
2555.801097	82.320846	57.692609
2555.015122	76.678033	57.697613
2554.291834	84.389864	57.702618
2553.780206	77.238880	57.707623
2553.306051	74.381616	57.712628
2553.048784	78.618753	57.717633
2552.541929	74.798032	57.722637
2550.897220	83.967213	57.727642
2550.494762	77.732668	57.732647
2550.218221	76.098027	57.737652
2549.577376	77.647145	57.742657
2549.113307	76.251794	57.747661
2548.131415	77.426994	57.752666
2547.521851	74.629984	57.757671
2546.737812	75.524263	57.762676
2545.604920	81.866954	57.767681
2545.410164	75.373488	57.772685
2544.847098	79.281601	57.777690
2544.064249	68.645395	57.782695
2543.697219	73.066685	57.787700
2542.363688	73.563473	57.792705
2541.397129	71.047358	57.797709
2540.627084	82.120361	57.802714
2540.361193	75.738922	57.807719
2540.066469	73.093345	57.812724
2539.416987	73.975278	57.817729
2539.333899	79.377861	57.822733
2538.574664	81.391285	57.827738
2537.533899	77.818548	57.832743
2536.775524	64.411542	57.837748
2536.217918	72.428584	57.842753
2535.673856	75.191117	57.847757
2534.291160	83.032654	57.852762
2533.401248	75.688591	57.857767
2533.077803	79.062334	57.862772
2532.637493	81.839892	57.867777
2532.290900	79.201998	57.872781
2531.614684	86.363038	57.877786
2531.209124	81.642397	57.882791
2530.713709	87.208235	57.887796
2529.474868	90.041000	57.892801
2528.885571	80.659685	57.897805
2528.315016	82.184947	57.902810
2527.690487	76.824002	57.907815
2526.868532	79.263004	57.912820
2525.758685	85.943197	57.917825
2525.263191	73.137802	57.922829
2524.927839	85.803410	57.927834
2524.850478	87.570397	57.932839
2523.516481	76.628561	57.937844
2522.365715	78.268806	57.942849
2521.894518	80.791128	57.947853
2521.662822	85.645980	57.952858
2521.265876	77.809891	57.957863
2520.437412	80.733544	57.962868
2519.536738	75.503888	57.967873
2518.842297	75.433541	57.972877
2518.024282	81.053741	57.977882
2517.832523	74.607527	57.982887
2517.595288	72.923144	57.987892
2516.037318	78.105000	57.992897
2516.078562	71.650925	57.997901
2514.958351	78.375123	58.002906
2514.747660	81.458809	58.007911
2513.395155	79.342223	58.012916
2512.224748	84.203224	58.017921
2512.035337	76.482045	58.022925
2511.560020	84.471209	58.027930
2511.184098	80.862179	58.032935
2510.625527	80.546374	58.037940
2509.962838	83.891278	58.042945
2508.984724	73.960281	58.047949
2507.849937	85.133144	58.052954
2507.514566	72.703786	58.057959
2507.316020	74.771349	58.062964
2506.903216	79.966626	58.067969
2505.809940	76.326298	58.072973
2504.657854	76.229198	58.077978
2503.803851	75.414842	58.082983
2503.872719	75.491093	58.087988
2503.040744	79.462945	58.092993
2503.001231	80.078761	58.097997
2501.839115	78.317642	58.103002
2501.091377	78.398904	58.108007
2500.621303	77.023531	58.113012
2499.578527	81.516935	58.118017
2499.439520	71.648923	58.123021
2498.314862	75.028599	58.128026
2497.761054	72.262720	58.133031
2496.871368	77.659919	58.138036
2496.660926	80.720669	58.143041
2496.111120	72.059300	58.148045
2495.039792	78.284502	58.153050
2494.557396	72.383360	58.158055
2494.009335	73.103094	58.163060
2493.359642	78.762410	58.168065
2492.568991	77.017518	58.173069
2491.380942	75.839895	58.178074
2490.827516	76.908299	58.183079
2490.138823	75.105319	58.188084
2489.645569	75.933312	58.193089
2489.717020	72.899487	58.198093
2489.127149	79.511307	58.203098
2488.339545	73.989968	58.208103
2487.418934	72.568076	58.213108
2486.369709	69.080875	58.218113
2485.874589	67.555450	58.223117
2484.520793	82.315901	58.228122
2484.220335	71.439738	58.233127
2483.758974	74.297868	58.238132
2483.169560	75.050331	58.243137
2483.058745	70.706793	58.248141
2482.474528	88.266892	58.253146
2481.822614	78.190527	58.258151
2480.832156	74.842090	58.263156
2480.216359	73.045990	58.268161
2479.720445	69.986805	58.273165
2478.234418	73.453135	58.278170
2477.638561	73.928419	58.283175
2476.917022	70.660318	58.288180
2476.333620	78.409020	58.293185
2476.431515	63.711724	58.298189
2475.639453	68.270812	58.303194
2474.443689	70.986092	58.308199
2473.802211	69.491611	58.313204
2473.446894	71.465192	58.318209
2472.910229	70.107129	58.323213
2472.288428	76.147716	58.328218
2471.105417	68.825363	58.333223
2470.245715	70.214940	58.338228
2469.660219	71.262777	58.343233
2469.501576	65.043797	58.348237
2468.945146	73.519308	58.353242
2468.559503	76.484884	58.358247
2467.303044	75.120811	58.363252
2466.262081	76.167182	58.368257
2466.238649	67.364117	58.373261
2465.342505	69.618054	58.378266
2464.993948	72.737152	58.383271
2464.601058	75.169511	58.388276
2463.450478	79.819899	58.393281
2462.951683	63.010224	58.398285
2462.468850	67.471049	58.403290
2461.436301	69.281350	58.408295
2460.707935	69.469434	58.413300
2460.013919	73.785979	58.418305
2459.654915	74.728779	58.423309
2459.652193	79.840918	58.428314
2458.413935	68.683011	58.433319
2457.649343	78.160003	58.438324
2456.934070	75.577257	58.443329
2455.995410	71.373288	58.448333
2455.148581	76.737111	58.453338
2453.955564	74.346176	58.458343
2454.292069	76.661722	58.463348
2453.485082	74.590430	58.468353
2453.179151	63.317334	58.473357
2452.551686	71.055409	58.478362
2451.927235	69.035012	58.483367
2450.940800	65.830364	58.488372
2449.859466	74.122473	58.493377
2449.746531	63.766478	58.498381
2449.215663	66.712674	58.503386
2448.159666	70.231797	58.508391
2447.077883	73.546915	58.513396
2446.613819	85.991375	58.518401
2446.692971	74.836767	58.523405
2445.720499	78.761991	58.528410
2444.978201	63.950994	58.533415
2444.508823	67.572311	58.538420
2443.714490	70.900254	58.543425
2443.350212	64.459471	58.548429
2442.545157	70.892957	58.553434
2441.332803	61.558597	58.558439
2440.658223	64.127141	58.563444
2439.951937	67.177144	58.568449
2439.336320	66.767683	58.573453
2438.864833	73.443337	58.578458
2438.772440	72.066946	58.583463
2437.901675	67.713615	58.588468
2437.179174	70.836651	58.593473
2436.607928	65.379382	58.598477
2435.489002	72.641375	58.603482
2435.118260	64.981609	58.608487
2434.576476	62.938791	58.613492
2433.371905	73.378741	58.618497
2433.107915	67.591446	58.623501
2432.363817	71.164608	58.628506
2431.973405	60.530414	58.633511
2431.432443	65.858123	58.638516
2430.347512	70.352031	58.643521
2429.445095	66.293445	58.648525
2428.490930	68.582569	58.653530
2428.203583	66.057711	58.658535
2428.096397	68.600690	58.663540
2427.288592	72.965507	58.668545
2426.870761	69.642723	58.673549
2425.294505	70.205513	58.678554
2424.941544	66.796641	58.683559
2424.597516	69.169333	58.688564
2423.918231	74.896867	58.693569
2423.673360	68.890390	58.698573
2422.364656	79.124736	58.703578
2421.723626	74.294772	58.708583
2421.288359	71.602185	58.713588
2420.686538	75.374830	58.718593
2420.378815	65.437394	58.723597
2418.988623	70.303617	58.728602
2418.387399	66.690887	58.733607
2417.850104	68.144946	58.738612
2417.399614	76.032759	58.743617
2416.630769	71.263729	58.748621
2415.448412	65.094664	58.753626
2414.854146	69.620333	58.758631
2414.633391	68.478252	58.763636
2414.121020	72.108896	58.768641
2413.920463	71.038754	58.773645
2412.432992	68.375292	58.778650
2412.023524	64.765302	58.783655
2411.537162	66.813395	58.788660
2411.070949	65.926039	58.793665
2409.897758	59.229245	58.798669
2408.590309	70.463206	58.803674
2408.114385	71.478498	58.808679
2407.785852	60.806098	58.813684
2406.969100	69.119283	58.818689
2407.061116	65.229343	58.823693
2406.258722	67.373314	58.828698
2405.232695	61.544221	58.833703
2405.078782	63.334162	58.838708
2404.193069	68.390042	58.843713
2403.569831	70.289440	58.848717
2402.652360	67.647333	58.853722
2401.816629	72.292445	58.858727
2401.455115	66.491436	58.863732
2400.734339	76.135404	58.868737
2400.567163	68.002297	58.873741
2399.512215	77.477229	58.878746
2399.094285	74.071177	58.883751
2398.273443	61.698806	58.888756
2397.369764	69.194384	58.893761
2396.279143	60.691827	58.898765
2395.263732	68.395581	58.903770
2394.720304	69.988055	58.908775
2395.173231	65.009730	58.913780
2394.201961	81.788919	58.918785
2393.784802	67.171805	58.923789
2393.289079	62.701069	58.928794
2392.101503	71.312522	58.933799
2391.292377	73.202260	58.938804
2390.515156	71.707317	58.943809
2390.194845	67.610784	58.948813
2389.760297	68.806496	58.953818
2388.435860	70.771715	58.958823
2387.759350	71.351586	58.963828
2387.127175	76.323856	58.968833
2386.758699	71.702287	58.973837
2386.387018	74.372593	58.978842
2385.779795	70.267094	58.983847
2385.196218	69.934264	58.988852
2383.923047	72.487144	58.993857
2383.688246	62.173707	58.998861
2383.151960	73.929081	59.003866
2382.350235	65.149766	59.008871
2381.817060	68.138991	59.013876
2381.253461	71.794186	59.018881
2380.722095	68.315958	59.023885
2379.378046	70.882143	59.028890
2378.389767	78.340484	59.033895
2377.860516	62.745473	59.038900
2377.270813	65.564370	59.043905
2377.405131	65.548115	59.048909
2376.592055	77.250559	59.053914
2375.780634	70.059294	59.058919
2374.545909	65.569664	59.063924
2373.360831	75.762349	59.068929
2373.416485	65.120967	59.073933
2372.671288	70.222690	59.078938
2372.257868	67.211779	59.083943
2372.212668	73.240616	59.088948
2371.525401	76.250271	59.093953
2370.448225	59.283348	59.098957
2370.302928	65.421662	59.103962
2369.435496	69.634055	59.108967
2368.199767	60.723306	59.113972
2367.179263	61.277923	59.118977
2366.794764	63.954368	59.123981
2366.329198	67.605825	59.128986
2366.049213	61.695754	59.133991
2365.592371	57.322977	59.138996
2363.947998	66.937374	59.144001
2363.761201	65.380951	59.149005
2363.358076	70.166429	59.154010
2362.489133	63.085267	59.159015
2361.521945	60.461143	59.164020
2360.409515	66.166824	59.169025
2359.998402	68.787823	59.174029
2359.325206	69.528177	59.179034
2358.993296	67.185412	59.184039
2359.327936	64.123167	59.189044
2358.043735	70.019268	59.194049
2357.496566	65.920479	59.199053
2356.318154	69.581333	59.204058
2355.536342	63.414056	59.209063
2355.435207	69.665605	59.214068
2354.205993	72.599778	59.219073
2354.032262	57.750801	59.224077
2353.230770	59.513716	59.229082
2352.602344	66.602637	59.234087
2352.282550	63.766371	59.239092
2350.769170	70.259010	59.244097
2350.178817	70.131414	59.249101
2349.653929	68.326498	59.254106
2349.065343	70.070771	59.259111
2349.240246	65.480631	59.264116
2348.325673	71.498655	59.269121
2347.284293	55.331649	59.274125
2346.422202	65.237400	59.279130
2345.851206	68.898597	59.284135
2345.602955	66.382454	59.289140
2344.395088	71.950912	59.294145
2343.494575	68.867379	59.299149
2343.411837	68.994419	59.304154
2342.352353	75.919036	59.309159
2342.082570	65.475011	59.314164
2341.484378	60.555242	59.319169
2340.514577	58.644045	59.324173
2339.830500	66.402854	59.329178
2339.253820	70.432511	59.334183
2338.689715	64.983115	59.339188
2338.372730	67.336186	59.344193
2337.314246	64.027440	59.349197
2336.511784	69.798539	59.354202
2336.180163	73.241970	59.359207
2335.923837	66.431044	59.364212
2334.483088	71.279483	59.369217
2333.781443	69.187042	59.374221
2333.043488	72.796267	59.379226
2332.187369	70.991942	59.384231
2332.235476	61.384847	59.389236
2331.643263	72.112055	59.394241
2330.784316	72.168937	59.399245
2330.118593	71.963050	59.404250
2329.534363	64.115604	59.409255
2329.129086	67.889775	59.414260
2327.592294	78.335629	59.419265
2327.139125	66.916025	59.424269
2326.636370	68.009724	59.429274
2325.869136	68.004742	59.434279
2325.654798	67.028142	59.439284
2324.850830	70.127227	59.444289
2324.760192	61.308436	59.449293
2323.985710	67.429607	59.454298
2322.780021	66.659630	59.459303
2321.512942	63.368795	59.464308
2320.497346	65.623046	59.469313
2321.138099	62.274779	59.474317
2320.270512	69.166977	59.479322
2319.780039	67.739060	59.484327
2319.308259	59.078602	59.489332
2318.142019	59.413420	59.494337
2317.402854	64.946730	59.499341
2316.638309	68.872333	59.504346
2315.801866	62.671777	59.509351
2315.869389	59.816256	59.514356
2315.271828	72.720484	59.519361
2314.028014	59.723387	59.524365
2313.347039	65.843962	59.529370
2312.822228	68.455985	59.534375
2312.373898	58.356306	59.539380
2311.299922	62.517973	59.544385
2310.839571	61.714885	59.549389
2310.504011	61.947919	59.554394
2309.653076	63.148130	59.559399
2309.280616	63.654702	59.564404
2308.208133	71.097052	59.569409
2307.386097	66.481213	59.574413
2306.539052	64.403772	59.579418
2305.705444	71.169375	59.584423
2305.622591	66.142540	59.589428
2304.997790	67.164352	59.594433
2304.540265	68.266502	59.599437
2303.492035	66.900414	59.604442
2302.670372	68.889014	59.609447
2302.411386	65.366193	59.614452
2301.748738	71.681394	59.619457
2301.265020	68.200555	59.624461
2300.476090	72.836490	59.629466
2299.647346	70.325672	59.634471
2299.242648	74.292767	59.639476
2298.501488	75.173430	59.644481
2297.703115	74.994177	59.649485
2296.765419	73.435115	59.654490
2296.038244	75.200725	59.659495
2295.906093	68.640137	59.664500
2295.481537	72.700624	59.669505
2294.888455	61.882436	59.674509
2293.604260	70.694363	59.679514
2293.011113	65.742950	59.684519
2292.559855	71.018617	59.689524
2291.412945	75.481305	59.694529
2290.583876	74.252603	59.699533
2289.948408	76.021477	59.704538
2289.110947	75.434846	59.709543
2289.065672	73.898829	59.714548
2288.502959	76.137219	59.719553
2288.504667	70.318714	59.724557
2287.665039	74.159664	59.729562
2286.591175	72.118250	59.734567
2286.131991	66.474874	59.739572
2285.071137	75.956351	59.744577
2284.322958	69.795177	59.749581
2283.229318	71.227548	59.754586
2282.816305	72.842728	59.759591
2282.546601	69.382923	59.764596
2281.865327	73.205873	59.769601
2281.520679	66.688732	59.774605
2280.782530	68.381221	59.779610
2279.637361	70.232916	59.784615
2279.174999	67.809443	59.789620
2278.490175	73.624376	59.794625
2278.271697	61.811376	59.799629
2277.357743	68.212971	59.804634
2276.480019	75.033489	59.809639
2275.880280	65.633891	59.814644
2275.604044	70.302544	59.819649
2274.621746	64.398903	59.824653
2273.312385	68.002430	59.829658
2272.819598	66.209401	59.834663
2272.499768	63.306046	59.839668
2272.028305	71.535325	59.844673
2271.883920	69.186550	59.849677
2271.235113	74.960590	59.854682
2270.011187	72.567881	59.859687
2269.582025	69.016534	59.864692
2268.315800	76.075985	59.869697
2267.550988	73.648578	59.874701
2266.958252	73.872701	59.879706
2266.315506	80.057008	59.884711
2265.994798	69.826167	59.889716
2265.104695	77.397988	59.894721
2265.356753	69.960939	59.899725
2264.158206	56.255489	59.904730
2263.316085	68.901941	59.909735
2262.888587	60.256418	59.914740
2262.187854	64.073617	59.919745
2261.257971	64.725646	59.924750
2260.084495	56.534921	59.929754
2259.207920	69.192396	59.934759
2259.155507	59.753678	59.939764
2258.602797	67.562655	59.944769
2258.271982	62.610991	59.949774
2258.140245	63.977945	59.954778
2256.818916	72.912672	59.959783
2256.123786	68.680127	59.964788
2255.117762	69.038873	59.969793
2254.888925	65.259858	59.974798
2254.509640	68.892224	59.979802
2253.420299	67.799614	59.984807
2252.590126	65.576408	59.989812
2251.636394	67.327082	59.994817
2251.113460	69.458017	59.999822
2251.300920	65.899115	60.004826
2250.370235	68.494897	60.009831
2249.627968	63.800300	60.014836
2248.413693	65.239097	60.019841
2248.382680	67.568134	60.024846
2247.966147	65.467999	60.029850
2246.444332	66.612429	60.034855
2245.778464	60.018390	60.039860
2245.068464	66.376425	60.044865
2244.923119	61.215814	60.049870
2244.291678	70.004141	60.054874
2244.010023	70.466374	60.059879
2243.001651	65.885177	60.064884
2242.083706	71.537092	60.069889
2241.695141	66.647408	60.074894
2241.407322	69.968090	60.079898
2240.186375	69.919137	60.084903
2239.656473	67.414854	60.089908
2238.952876	62.080117	60.094913
2238.828711	62.615281	60.099918
2237.549987	63.222369	60.104922
2236.387777	68.585674	60.109927
2236.344597	59.437080	60.114932
2235.745322	63.067989	60.119937
2235.440873	57.142777	60.124942
2234.278275	65.060000	60.129946
2233.233960	66.129088	60.134951
2232.709056	56.649210	60.139956
2232.092249	64.890710	60.144961
2231.835244	64.189428	60.149966
2231.186801	64.915301	60.154970
2229.958535	64.624847	60.159975
2229.427456	68.729999	60.164980
2228.439394	67.057200	60.169985
2228.453000	71.588657	60.174990
2228.149858	64.025515	60.179994
2227.212528	77.267709	60.184999
2226.458105	73.779491	60.190004
2225.681294	73.004478	60.195009
2225.507282	63.146047	60.200014
2224.538559	64.630484	60.205018
2223.393080	62.679882	60.210023
2223.316289	58.820397	60.215028
2222.803957	67.138765	60.220033
2222.207919	67.226489	60.225038
2220.870148	61.889688	60.230042
2219.997471	64.777121	60.235047
2219.910856	58.862418	60.240052
2219.050133	62.938289	60.245057
2218.438267	67.084492	60.250062
2217.090852	68.697244	60.255066
2216.514024	62.892427	60.260071
2216.865100	60.329849	60.265076
2216.324546	62.065129	60.270081
2215.845544	62.712686	60.275086
2214.006645	63.478735	60.280090
2213.429142	68.194173	60.285095
2212.910621	69.067560	60.290100
2212.224678	65.750392	60.295105
2211.949046	67.453392	60.300110
2211.632262	63.657843	60.305114
2210.523725	70.216665	60.310119
2209.881922	63.262477	60.315124
2209.028382	63.008992	60.320129
2208.911941	62.329459	60.325134
2208.011555	65.132426	60.330138
2206.385703	70.862780	60.335143
2206.153845	55.213805	60.340148
2205.186383	62.881351	60.345153
2205.393336	62.385713	60.350158
2204.918365	59.886251	60.355162
2204.306878	73.010349	60.360167
2203.573748	59.122301	60.365172
2202.443168	74.670747	60.370177
2202.260072	68.395582	60.375182
2201.508912	71.786823	60.380186
2200.224789	65.226686	60.385191
2199.843032	61.258310	60.390196
2199.090931	65.116667	60.395201
2198.649072	70.913341	60.400206
2198.014724	63.586447	60.405210
2197.136377	68.253471	60.410215
2196.577344	65.244194	60.415220
2195.421409	72.503469	60.420225
2195.324608	65.745801	60.425230
2195.137003	67.448352	60.430234
2194.287790	62.441279	60.435239
2193.622404	58.069849	60.440244
2192.202490	62.480953	60.445249
2192.529163	58.485760	60.450254
2191.653304	55.124896	60.455258
2189.912426	68.783577	60.460263
2189.500934	66.696796	60.465268
2188.846115	60.281662	60.470273
2188.467486	62.064248	60.475278
2188.452507	66.779794	60.480282
2187.712830	62.985917	60.485287
2187.406778	63.580215	60.490292
2186.579104	71.785154	60.495297
2185.811969	64.379922	60.500302
2184.619542	65.347250	60.505306
2183.476653	64.133161	60.510311
2183.279891	55.250043	60.515316
2182.485228	61.852681	60.520321
2181.853410	67.390143	60.525326
2181.454896	73.062172	60.530330
2181.109044	71.565722	60.535335
2180.212650	60.171433	60.540340
2179.302650	65.587923	60.545345
2179.087550	61.965638	60.550350
2178.805899	63.377969	60.555354
2177.256512	58.992340	60.560359
2176.812310	59.257383	60.565364
2175.899869	70.019224	60.570369
2175.343950	63.522442	60.575374
2175.065850	65.155210	60.580378
2174.164054	66.040862	60.585383
2173.171051	57.459311	60.590388
2172.372630	69.901719	60.595393
2172.037802	60.317108	60.600398
2171.556612	61.208191	60.605402
2171.020269	65.673442	60.610407
2170.902675	66.775094	60.615412
2169.622382	70.855628	60.620417
2169.101405	66.879486	60.625422
2168.581388	68.094962	60.630426
2167.695098	65.065083	60.635431
2167.146147	58.907363	60.640436
2166.137442	73.199091	60.645441
2165.669557	62.544250	60.650446
2164.817494	62.542746	60.655450
2163.458321	60.098595	60.660455
2163.052343	58.821239	60.665460
2162.652004	64.561865	60.670465
2162.656989	62.209654	60.675470
2162.067287	59.549432	60.680474
2161.246308	68.799239	60.685479
2160.427879	55.146051	60.690484
2159.803765	63.060788	60.695489
2158.501052	64.269212	60.700494
2158.294345	58.420446	60.705498
2157.782379	57.369236	60.710503
2157.102789	51.860682	60.715508
2156.110528	64.900691	60.720513
2155.394826	61.116140	60.725518
2155.037000	62.517027	60.730522
2154.362915	71.616586	60.735527
2154.334688	62.210057	60.740532
2153.238077	57.930544	60.745537
2152.094636	59.135807	60.750542
2151.949867	54.346936	60.755546
2150.968311	73.086877	60.760551
2150.332551	61.335399	60.765556
2149.675219	63.958651	60.770561
2148.713349	69.178367	60.775566
2148.461284	62.377789	60.780570
2148.079304	70.170200	60.785575
2147.451069	68.181674	60.790580
2145.940192	66.209114	60.795585
2145.451776	59.103974	60.800590
2145.204136	62.057009	60.805594
2144.563940	55.922400	60.810599
2144.446948	63.428705	60.815604
2143.615434	58.449800	60.820609
2142.559573	59.374044	60.825614
2142.044909	56.804012	60.830618
2140.823301	59.534826	60.835623
2140.369205	50.691387	60.840628
2139.363514	57.389723	60.845633
2139.316470	56.643852	60.850638
2139.086024	62.566201	60.855642
2137.869624	66.268720	60.860647
2137.452915	53.378117	60.865652
2136.669369	68.060789	60.870657
2135.977031	61.642608	60.875662
2134.950848	66.688595	60.880666
2133.958369	72.616549	60.885671
2133.329678	58.425275	60.890676
2132.834145	57.779004	60.895681
2132.551986	59.498122	60.900686
2132.540991	65.717663	60.905690
2131.623362	68.859893	60.910695
2130.347184	57.221508	60.915700
2129.698431	63.317241	60.920705
2129.214802	62.394998	60.925710
2129.039610	56.813598	60.930714
2128.129793	61.432724	60.935719
2127.267917	60.268870	60.940724
2125.964720	58.985111	60.945729
2125.753306	59.835977	60.950734
2125.467988	59.306906	60.955738
2125.079281	66.098266	60.960743
2124.425505	55.118798	60.965748
2123.174622	57.814360	60.970753
2122.581687	57.483160	60.975758
2122.122347	60.784233	60.980762
2121.279956	69.111293	60.985767
2120.311708	57.960620	60.990772
2119.189284	55.170869	60.995777
2118.718480	55.355601	61.000782
2119.094708	60.107254	61.005786
2118.483035	64.446449	61.010791
2118.217341	58.671327	61.015796
2116.797714	65.767691	61.020801
2116.093173	57.857185	61.025806
2115.468585	57.959278	61.030810
2114.773277	64.018765	61.035815
2114.104911	56.241410	61.040820
2113.507434	65.996129	61.045825
2113.134862	59.475894	61.050830
2112.588606	60.413241	61.055834
2111.116776	66.865666	61.060839
2110.487063	58.876839	61.065844
2109.849756	65.315208	61.070849
2109.497753	64.505054	61.075854
2108.994235	60.332917	61.080858
2107.935223	64.056284	61.085863
2107.355892	62.223605	61.090868
2106.566536	65.884666	61.095873
2106.128198	64.645612	61.100878
2106.132393	62.677997	61.105882
2105.069841	69.034370	61.110887
2104.124349	62.256878	61.115892
2103.360463	55.539507	61.120897
2102.720044	58.628010	61.125902
2102.504500	53.218510	61.130906
2101.224278	74.173398	61.135911
2100.317701	59.017200	61.140916
2099.907679	64.721984	61.145921
2099.325331	63.933467	61.150926
2099.191496	60.058877	61.155930
2098.473558	61.853321	61.160935
2098.105994	68.693170	61.165940
2097.107469	57.419002	61.170945
2096.193031	69.513769	61.175950
2095.935319	68.219348	61.180954
2094.534488	71.394890	61.185959
2093.660490	55.694724	61.190964
2093.180060	63.997372	61.195969
2092.975124	64.729110	61.200974
2092.666549	62.166464	61.205978
2091.708960	63.200220	61.210983
2090.826981	69.010202	61.215988
2090.225686	64.081531	61.220993
2088.959053	62.548379	61.225998
2088.915208	63.699388	61.231002
2088.124242	64.163876	61.236007
2088.142299	60.554217	61.241012
2087.791571	68.648769	61.246017
2086.384905	68.605170	61.251022
2085.817884	62.722122	61.256026
2084.855665	71.310067	61.261031
2084.236073	62.539147	61.266036
2083.326634	75.984985	61.271041
2082.880559	67.837254	61.276046
2082.681573	63.378568	61.281050
2082.149116	76.673088	61.286055
2081.141269	65.150656	61.291060
2080.063389	68.372011	61.296065
2079.301929	68.497519	61.301070
2079.399017	65.033809	61.306074
2078.313337	71.419799	61.311079
2077.961816	65.027409	61.316084
2077.037930	69.059235	61.321089
2076.291599	62.803452	61.326094
2076.118732	67.384558	61.331098
2075.283007	67.702367	61.336103
2074.396627	61.989599	61.341108
2073.560524	68.723279	61.346113
2072.456969	64.577599	61.351118
2072.467635	63.093202	61.356122
2072.029363	73.295149	61.361127
2071.679088	67.706199	61.366132
2070.415558	68.705449	61.371137
2069.661651	69.271755	61.376142
2069.171518	62.640586	61.381146
2068.518862	68.242800	61.386151
2068.324250	66.576418	61.391156
2067.254141	68.259794	61.396161
2065.986007	66.965315	61.401166
2065.885234	70.866616	61.406170
2065.626258	72.116000	61.411175
2064.772154	60.093613	61.416180
2063.589860	75.455918	61.421185
2062.962942	71.493570	61.426190
2063.127007	67.541974	61.431194
2062.270953	67.645771	61.436199
2061.413110	60.906191	61.441204
2060.739257	65.214580	61.446209
2059.831778	68.083910	61.451214
2058.877129	67.991422	61.456218
2057.966736	67.270467	61.461223
2057.588413	62.910350	61.466228
2056.850250	65.698615	61.471233
2056.464401	72.258577	61.476238
2056.165848	69.262788	61.481242
2055.323652	67.530734	61.486247
2055.315090	72.579901	61.491252
2054.207593	69.710245	61.496257
2053.281785	60.547253	61.501262
2052.630297	63.572130	61.506266
2052.084799	69.375876	61.511271
2051.691174	72.748212	61.516276
2050.678778	72.498636	61.521281
2050.087383	74.389464	61.526286
2049.508095	66.850292	61.531290
2048.031797	64.290816	61.536295
2047.788045	52.310087	61.541300
2047.293403	66.609010	61.546305
2046.419465	68.485801	61.551310
2046.534413	57.455384	61.556314
2045.677081	71.109403	61.561319
2044.668498	55.330831	61.566324
2043.771132	63.890710	61.571329
2043.103590	71.365268	61.576334
2042.979609	65.984317	61.581338
2042.021491	72.736504	61.586343
2041.590631	59.908335	61.591348
2040.756795	65.208001	61.596353
2040.229796	61.744468	61.601358
2039.759636	64.166379	61.606362
2038.496093	67.938557	61.611367
2037.808507	63.373984	61.616372
2036.903718	59.742583	61.621377
2036.455242	65.524207	61.626382
2036.282946	59.169850	61.631386
2035.592575	73.495943	61.636391
2035.622670	60.954439	61.641396
2034.553890	59.445481	61.646401
2033.505560	62.516531	61.651406
2033.468880	62.305710	61.656410
2032.185340	67.933738	61.661415
2031.287243	67.648036	61.666420
2030.657687	65.012016	61.671425
2030.325856	75.003132	61.676430
2030.067968	66.983082	61.681434
2028.736128	71.241006	61.686439
2028.008593	62.875389	61.691444
2027.202981	60.407243	61.696449
2026.758624	64.112716	61.701454
2026.683566	64.069507	61.706458
2025.255368	67.942086	61.711463
2024.449253	69.169014	61.716468
2024.035575	66.082399	61.721473
2023.569226	65.383386	61.726478
2023.405667	61.601119	61.731482
2022.854212	68.621627	61.736487
2021.561646	58.395635	61.741492
2021.071334	68.178601	61.746497
2020.569245	68.194227	61.751502
2019.616147	63.139043	61.756506
2018.454778	75.806166	61.761511
2017.912662	62.625203	61.766516
2017.878053	66.812409	61.771521
2017.282227	73.386974	61.776526
2017.136720	66.070439	61.781530
2015.715461	68.609255	61.786535
2015.080982	70.351145	61.791540
2014.521280	65.043544	61.796545
2013.051038	73.969045	61.801550
2012.470216	63.824981	61.806554
2011.865397	63.969492	61.811559
2011.707610	67.572265	61.816564
2011.096147	63.857932	61.821569
2010.551868	68.724402	61.826574
2010.348918	56.621438	61.831578
2009.026360	62.897959	61.836583
2008.619686	61.397324	61.841588
2007.633609	60.326970	61.846593
2006.936698	69.252023	61.851598
2006.868352	60.345380	61.856602
2005.164717	69.288699	61.861607
2004.574086	66.756151	61.866612
2004.352295	73.494884	61.871617
2003.704864	75.729236	61.876622
2003.792265	64.778527	61.881626
2002.306593	65.873421	61.886631
2001.545662	59.598838	61.891636
2000.951541	62.128399	61.896641
2000.114191	71.242864	61.901646
2000.322989	63.726784	61.906650
1999.247102	73.371508	61.911655
1998.347630	58.401228	61.916660
1997.741371	66.383178	61.921665
1997.181524	70.036965	61.926670
1996.761959	64.707369	61.931674
1995.774079	71.240055	61.936679
1995.187811	61.250870	61.941684
1994.184227	65.599090	61.946689
1993.655588	72.347287	61.951694
1993.557991	64.368506	61.956698
1992.799953	67.933832	61.961703
1991.609710	64.924799	61.966708
1990.853743	71.923058	61.971713
1990.338318	73.238418	61.976718
1989.999986	71.405184	61.981722
1989.622924	67.850880	61.986727
1988.976214	72.065821	61.991732
1988.236129	69.348059	61.996737
1987.235163	63.873192	62.001742
1986.907521	60.344777	62.006746
1985.894493	64.494095	62.011751
1984.863157	63.356886	62.016756
1984.399656	70.389980	62.021761
1983.855277	67.104289	62.026766
1984.192501	57.998015	62.031770
1983.230315	66.992129	62.036775
1982.043044	53.742734	62.041780
1981.386938	56.524864	62.046785
1980.455428	63.268160	62.051790
1979.935140	68.513802	62.056794
1978.887929	69.457912	62.061799
1978.816262	66.733570	62.066804
1978.514191	63.425377	62.071809
1977.583264	56.677005	62.076814
1976.553392	54.523141	62.081818
1975.857790	59.695353	62.086823
1975.090388	58.044068	62.091828
1974.835358	59.090288	62.096833
1974.037142	72.072643	62.101838
1972.784320	57.434386	62.106842
1971.890174	67.136438	62.111847
1971.934456	62.153008	62.116852
1971.577573	58.603151	62.121857
1971.082960	68.459481	62.126862
1970.763071	62.292607	62.131866
1969.151281	57.571159	62.136871
1968.688892	57.636049	62.141876
1967.935285	70.992468	62.146881
1967.271912	64.135960	62.151886
1967.108420	64.375500	62.156890
1966.483900	72.892267	62.161895
1965.597948	59.051351	62.166900
1964.638623	67.415396	62.171905
1963.825411	70.640046	62.176910
1963.815372	59.068540	62.181914
1962.477428	65.187051	62.186919
1961.681947	69.247845	62.191924
1961.020825	59.418705	62.196929
1960.666976	60.774318	62.201934
1960.624894	66.827857	62.206938
1959.881113	62.512507	62.211943
1959.646990	63.483311	62.216948
1958.404599	63.707686	62.221953
1957.491242	60.765766	62.226958
1956.847006	63.422715	62.231962
1955.565890	64.952346	62.236967
1955.524996	58.278295	62.241972
1955.040875	57.967576	62.246977
1954.081367	63.128492	62.251982
1953.786123	59.576775	62.256986
1953.298749	65.254138	62.261991
1952.216536	61.412326	62.266996
1951.450892	67.364256	62.272001
1950.530346	63.870168	62.277006
1950.684445	54.555234	62.282010
1949.815500	62.415942	62.287015
1948.449945	62.355874	62.292020
1947.655346	62.578644	62.297025
1947.301856	70.876158	62.302030
1947.654128	59.677262	62.307034
1946.745525	65.720750	62.312039
1945.821038	61.353425	62.317044
1945.051106	61.292909	62.322049
1944.135286	54.410914	62.327054
1944.177594	65.199297	62.332058
1942.923121	72.147055	62.337063
1941.955262	66.173922	62.342068
1941.588311	65.014247	62.347073
1940.831753	68.353545	62.352078
1940.802938	62.405686	62.357082
1939.813593	62.778216	62.362087
1938.856874	69.173740	62.367092
1938.547357	62.351044	62.372097
1937.481161	76.057377	62.377102
1937.419599	61.042454	62.382106
1936.697331	69.277532	62.387111
1935.698614	61.217660	62.392116
1935.001553	64.294158	62.397121
1934.569060	66.783840	62.402126
1934.113132	54.516149	62.407130
1932.589030	63.191146	62.412135
1932.206278	59.287311	62.417140
1931.569768	64.047988	62.422145
1931.175323	71.793583	62.427150
1930.864148	63.618856	62.432154
1929.641899	67.527275	62.437159
1928.750107	62.153348	62.442164
1928.398438	61.997203	62.447169
1927.819906	61.492646	62.452174
1927.437392	57.243786	62.457178
1926.671543	54.915297	62.462183
1926.095060	64.184864	62.467188
1925.350660	58.586390	62.472193
1924.668439	65.540852	62.477198
1923.694798	59.732131	62.482202
1922.693744	61.469243	62.487207
1922.020568	57.487993	62.492212
1921.790862	57.018102	62.497217
1921.422606	61.941300	62.502222
1921.159716	58.171692	62.507226
1920.185106	58.471050	62.512231
1919.292330	60.401999	62.517236
1918.870933	63.050828	62.522241
1917.871238	63.011465	62.527246
1917.460241	58.243289	62.532250
1916.397895	64.758327	62.537255
1915.888862	61.555017	62.542260
1915.315017	51.172957	62.547265
1914.883662	58.078579	62.552270
1913.797758	68.421310	62.557274
1912.873474	60.512126	62.562279
1912.459520	66.392447	62.567284
1912.098533	58.386109	62.572289
1912.011001	63.229311	62.577294
1911.232688	59.891287	62.582298
1909.379318	69.995855	62.587303
1909.185164	62.543977	62.592308
1908.678373	63.903258	62.597313
1908.027949	65.749330	62.602318
1907.561320	54.740268	62.607322
1906.469572	67.446402	62.612327
1905.989402	66.602534	62.617332
1905.891623	62.938096	62.622337
1904.409112	61.223246	62.627342
1904.012722	54.844087	62.632346
1903.018878	56.904824	62.637351
1902.589727	70.466646	62.642356
1902.386616	69.635377	62.647361
1901.520968	68.225506	62.652366
1900.580753	63.585761	62.657370
1899.858100	72.940337	62.662375
1899.117873	66.195671	62.667380
1899.502937	72.752426	62.672385
1898.163384	70.105262	62.677390
1897.257483	60.681156	62.682394
1896.489331	61.302814	62.687399
1896.037512	65.692832	62.692404
1895.517161	62.483566	62.697409
1895.162316	69.500441	62.702414
1894.118552	60.595296	62.707418
1893.407882	71.173034	62.712423
1892.693616	62.196124	62.717428
1892.278411	64.535225	62.722433
1891.619941	63.362270	62.727438
1890.734990	57.688774	62.732442
1889.778612	59.089446	62.737447
1889.319599	56.519399	62.742452
1889.194865	61.826051	62.747457
1888.453840	64.527195	62.752462
1887.871678	57.328406	62.757466
1886.531226	65.071241	62.762471
1885.870586	61.551649	62.767476
1885.729541	62.765864	62.772481
1885.203579	60.494232	62.777486
1883.952326	60.811320	62.782490
1883.164723	61.691692	62.787495
1882.543896	59.206958	62.792500
1882.575101	58.308763	62.797505
1882.492907	68.679511	62.802510
1881.478015	56.354702	62.807514
1880.370159	55.499016	62.812519
1879.856562	51.672440	62.817524
1878.596135	53.562876	62.822529
1877.375319	58.566013	62.827534
1877.154763	54.431156	62.832538
1876.470123	62.159685	62.837543
1876.246183	56.843218	62.842548
1876.028538	50.807679	62.847553
1875.616421	49.495480	62.852558
1874.948778	58.667355	62.857562
1873.792209	63.950412	62.862567
1873.069378	50.911328	62.867572
1871.765997	59.773564	62.872577
1870.970280	60.725981	62.877582
1870.815006	53.819675	62.882586
1870.201806	62.739485	62.887591
1870.192338	59.216646	62.892596
1869.537557	65.194613	62.897601
1868.397719	61.766875	62.902606
1867.678287	56.635832	62.907610
1866.833934	60.424744	62.912615
1866.760654	57.864494	62.917620
1866.455698	58.312573	62.922625
1865.149765	63.667367	62.927630
1864.561490	53.865262	62.932634
1863.741208	63.844011	62.937639
1863.067989	61.867960	62.942644
1862.361886	58.662848	62.947649
1861.470344	54.043996	62.952654
1861.304681	52.452408	62.957658
1860.824083	60.928364	62.962663
1859.677892	56.767930	62.967668
1858.654487	52.837928	62.972673
1857.980923	59.825250	62.977678
1857.552016	58.121204	62.982682
1856.714236	63.831677	62.987687
1856.451101	58.144564	62.992692
1856.284939	58.610739	62.997697
1855.277001	65.094372	63.002702
1854.493858	56.973171	63.007706
1853.685414	60.975405	63.012711
1853.043169	61.153967	63.017716
1853.000901	65.095776	63.022721
1851.696369	66.364975	63.027726
1851.148315	54.992897	63.032730
1850.504927	63.792746	63.037735
1850.124729	67.199106	63.042740
1849.530056	61.014131	63.047745
1848.333429	67.842668	63.052750
1847.690580	57.717546	63.057754
1847.269478	62.264934	63.062759
1846.965838	57.207622	63.067764
1846.354755	60.044427	63.072769
1845.269213	60.566848	63.077774
1844.325157	50.769174	63.082778
1843.992726	61.954799	63.087783
1843.306868	60.910874	63.092788
1842.125280	56.501117	63.097793
1841.108159	65.565822	63.102798
1841.653780	63.051257	63.107802
1840.461339	63.046859	63.112807
1839.668093	65.878123	63.117812
1839.815146	64.071986	63.122817
1839.119031	65.284066	63.127822
1838.490429	52.309787	63.132826
1837.329829	59.510695	63.137831
1836.818486	60.213946	63.142836
1835.962244	58.522227	63.147841
1834.717885	65.558660	63.152846
1834.441234	55.438782	63.157850
1834.041174	64.918551	63.162855
1833.494565	61.346301	63.167860
1833.048379	61.476323	63.172865
1832.153174	60.718864	63.177870
1831.371587	61.875309	63.182874
1830.555529	65.916348	63.187879
1830.216957	61.242760	63.192884
1829.872419	55.741676	63.197889
1828.307575	60.118447	63.202894
1827.851640	59.990411	63.207898
1827.157154	53.703710	63.212903
1826.642989	53.346041	63.217908
1826.383518	60.333962	63.222913
1825.714484	67.023685	63.227918
1825.059866	52.522739	63.232922
1824.357859	57.445016	63.237927
1823.633249	62.481288	63.242932
1822.621994	58.359748	63.247937
1821.761522	68.676944	63.252942
1821.483720	57.702299	63.257946
1821.069259	61.942643	63.262951
1820.367016	64.334805	63.267956
1819.930970	53.393947	63.272961
1818.397423	64.271938	63.277966
1818.207893	54.005716	63.282970
1817.686377	66.360093	63.287975
1816.930051	65.411910	63.292980
1816.090525	58.389792	63.297985
1815.405320	65.855539	63.302990
1815.299641	62.666122	63.307994
1814.665384	68.212311	63.312999
1813.617454	63.471414	63.318004
1812.859469	61.867095	63.323009
1811.713632	62.228530	63.328014
1811.517466	58.588431	63.333018
1811.129176	71.259478	63.338023
1809.867989	66.225871	63.343028
1809.210865	66.728681	63.348033
1808.851674	63.831313	63.353038
1808.578962	51.848082	63.358042
1807.692827	64.016563	63.363047
1806.833038	63.129502	63.368052
1806.047481	63.545344	63.373057
1804.969468	65.308669	63.378062
1804.584337	51.778028	63.383066
1804.446999	60.572607	63.388071
1803.698257	61.762907	63.393076
1803.881010	58.724661	63.398081
1802.589649	63.447789	63.403086
1801.824117	56.158027	63.408090
1801.226233	57.864072	63.413095
1800.397442	66.715382	63.418100
1799.543717	64.456026	63.423105
1798.938480	68.577047	63.428110
1798.464134	58.760197	63.433114
1797.933819	60.910189	63.438119
1796.648134	61.019251	63.443124
1796.228220	56.619706	63.448129
1795.116462	65.072213	63.453134
1794.784094	60.883863	63.458138
1794.836127	65.735155	63.463143
1794.381303	56.242191	63.468148
1793.362665	54.164599	63.473153
1791.872220	66.308588	63.478158
1791.310273	49.444002	63.483162
1791.162145	53.004461	63.488167
1790.466495	59.932806	63.493172
1790.341426	53.589737	63.498177
1788.720418	63.208935	63.503182
1788.610230	47.747652	63.508186
1788.129263	52.127264	63.513191
1787.402102	51.292906	63.518196
1786.128096	52.903855	63.523201
1785.898066	58.434562	63.528206
1785.634012	44.142325	63.533210
1784.427608	55.887592	63.538215
1783.565857	52.232304	63.543220
1783.017634	57.031565	63.548225
1782.495428	56.141615	63.553230
1781.904665	49.779549	63.558234
1781.659896	59.332607	63.563239
1780.228892	53.656255	63.568244
1779.670702	49.472602	63.573249
1778.593837	58.785942	63.578254
1778.487557	53.264231	63.583258
1778.056375	54.839128	63.588263
1777.530507	59.558384	63.593268
1776.736279	56.193900	63.598273
1775.759178	55.624141	63.603278
1775.394291	52.841432	63.608282
1774.515097	58.612285	63.613287
1774.016144	54.068379	63.618292
1773.269887	47.998172	63.623297
1772.488007	57.413007	63.628302
1772.394811	50.673715	63.633306
1772.057015	53.680862	63.638311
1770.496528	60.477326	63.643316
1769.857049	50.712030	63.648321
1769.081014	59.701542	63.653326
1768.519178	63.883030	63.658330
1767.915164	59.064612	63.663335
1766.934521	46.908849	63.668340
1766.288750	47.220256	63.673345
1765.673258	60.169761	63.678350
1765.645213	57.347969	63.683354
1764.649465	57.178097	63.688359
1764.364983	55.163572	63.693364
1763.637846	52.046548	63.698369
1762.457908	52.169101	63.703374
1762.390139	57.052728	63.708378
1761.345566	63.846576	63.713383
1760.357831	60.830584	63.718388
1759.541752	61.126134	63.723393
1759.042617	67.067215	63.728398
1758.601879	57.554479	63.733402
1758.069699	59.102056	63.738407
1758.109764	54.615129	63.743412
1757.250642	54.113999	63.748417
1756.263898	68.512500	63.753422
1755.560207	57.212466	63.758426
1754.922336	64.132901	63.763431
1753.602124	61.933636	63.768436
1753.239084	54.801981	63.773441
1752.266061	60.451134	63.778446
1752.253047	59.603924	63.783450
1751.759300	60.199571	63.788455
1751.188945	61.840519	63.793460
1749.837823	53.184977	63.798465
1749.294996	65.565496	63.803470
1749.287308	58.063578	63.808474
1748.724905	57.896926	63.813479
1747.464500	65.581090	63.818484
1746.878580	61.309820	63.823489
1746.137974	65.765835	63.828494
1745.707020	62.579976	63.833498
1744.641799	53.333565	63.838503
1743.718517	57.916752	63.843508
1743.660114	44.453378	63.848513
1742.996020	58.175768	63.853518
1742.824812	50.349743	63.858522
1741.494149	47.094816	63.863527
1740.748158	48.381754	63.868532
1740.188847	40.455175	63.873537
1739.513563	46.851502	63.878542
1739.231500	50.568687	63.883546
1737.492851	55.512828	63.888551
1736.842624	52.745396	63.893556
1736.761032	53.558666	63.898561
1736.396063	58.213684	63.903566
1735.978823	53.810533	63.908570
1735.448689	50.092198	63.913575
1734.432507	58.649928	63.918580
1734.201824	46.992666	63.923585
1733.184708	55.116758	63.928590
1732.236832	54.841204	63.933594
1731.367090	51.814505	63.938599
1730.518957	58.743681	63.943604
1730.234897	55.318357	63.948609
1729.600894	58.691966	63.953614
1729.422162	47.568556	63.958618
1728.868995	56.461910	63.963623
1727.754970	48.456963	63.968628
1727.006421	52.814867	63.973633
1726.716295	55.557291	63.978638
1725.308370	51.372998	63.983642
1724.498699	51.288525	63.988647
1723.774023	44.679397	63.993652
1723.321518	46.614378	63.998657
1722.618443	55.027746	64.003662
1722.505841	47.937322	64.008666
1722.373524	49.088862	64.013671
1721.532903	54.765886	64.018676
1720.645130	47.439434	64.023681
1719.644687	59.640499	64.028686
1719.226104	50.416471	64.033690
1718.594283	54.139034	64.038695
1717.747859	52.340663	64.043700
1717.469477	45.800031	64.048705
1717.085933	49.388535	64.053710
1715.759009	47.782116	64.058714
1714.734276	45.121401	64.063719
1714.197167	48.668289	64.068724
1713.970240	53.835320	64.073729
1713.051765	52.901873	64.078734
1713.259538	47.191042	64.083738
1712.085951	48.202218	64.088743
1711.245917	46.549196	64.093748
1711.063972	43.273370	64.098753
1709.441274	48.976458	64.103758
1708.631785	46.336937	64.108762
1708.274860	50.163244	64.113767
1707.542799	61.065941	64.118772
1707.365276	52.268015	64.123777
1706.728840	53.462004	64.128782
1706.034750	53.246051	64.133786
1705.163962	55.870739	64.138791
1704.467055	56.737986	64.143796
1704.359108	48.433398	64.148801
1703.452686	56.189619	64.153806
1702.455471	49.773175	64.158810
1701.811854	56.417105	64.163815
1701.247390	43.542416	64.168820
1701.152828	45.518776	64.173825
1700.056267	50.070435	64.178830
1699.371521	48.670700	64.183834
1698.619361	59.882744	64.188839
1698.153562	59.982581	64.193844
1697.334785	53.018916	64.198849
1695.622806	63.415507	64.203854
1695.228325	55.591376	64.208858
1694.962836	54.062270	64.213863
1694.553923	64.509034	64.218868
1694.206653	56.375653	64.223873
1693.944620	50.947308	64.228878
1693.341640	56.208687	64.233882
1692.231133	52.655587	64.238887
1691.523222	63.682438	64.243892
1690.980543	53.659421	64.248897
1689.460382	60.932929	64.253902
1688.999423	50.459370	64.258906
1688.503661	52.705690	64.263911
1687.952823	52.432070	64.268916
1687.767447	43.031180	64.273921
1687.038972	46.519241	64.278926
1686.323554	49.265758	64.283930
1685.616788	50.547965	64.288935
1684.609983	62.001340	64.293940
1684.307389	48.611335	64.298945
1682.680665	51.267883	64.303950
1682.085633	49.998844	64.308954
1682.062983	50.865579	64.313959
1681.033430	50.698745	64.318964
1681.072830	54.228298	64.323969
1680.354499	52.126184	64.328974
1680.047787	51.736979	64.333978
1678.873617	55.159605	64.338983
1677.861473	56.650378	64.343988
1677.499984	53.579741	64.348993
1677.212007	56.416137	64.353998
1676.523236	57.401989	64.359002
1675.590522	48.939340	64.364007
1674.196488	51.375687	64.369012
1674.333883	52.124249	64.374017
1673.941757	59.714709	64.379022
1672.897610	56.509058	64.384026
1672.146920	55.672428	64.389031
1671.266357	57.343572	64.394036
1671.300873	52.022372	64.399041
1670.245237	52.384191	64.404046
1669.503897	49.603547	64.409050
1668.601907	51.830965	64.414055
1668.229729	54.311916	64.419060
1668.075324	43.645388	64.424065
1666.905851	56.837705	64.429070
1665.969038	49.043231	64.434074
1665.952289	53.500904	64.439079
1664.986764	60.036903	64.444084
1664.395037	46.410209	64.449089
1663.612535	54.139307	64.454094
1662.777368	54.013814	64.459098
1662.522688	54.688554	64.464103
1661.748871	49.714880	64.469108
1660.995842	50.067548	64.474113
1659.593580	49.253212	64.479118
1659.652104	47.643401	64.484122
1658.955952	49.364302	64.489127
1658.386460	54.855994	64.494132
1658.210999	48.986937	64.499137
1657.130208	47.445778	64.504142
1656.503248	48.527235	64.509146
1655.816085	53.052659	64.514151
1655.098586	53.557530	64.519156
1654.418613	49.742484	64.524161
1653.009357	58.590898	64.529166
1652.748677	60.333987	64.534170
1652.092770	50.337856	64.539175
1651.590154	60.975512	64.544180
1651.851551	42.451593	64.549185
1650.459854	55.800749	64.554190
1649.773720	51.487833	64.559194
1649.102466	53.444463	64.564199
1648.836376	53.897350	64.569204
1647.833249	50.499958	64.574209
1646.661264	59.730120	64.579214
1646.017755	51.145359	64.584218
1645.761482	53.499904	64.589223
1645.132723	59.910384	64.594228
1644.537040	56.617339	64.599233
1643.910862	58.517707	64.604238
1642.979103	55.850174	64.609242
1642.299292	47.613850	64.614247
1641.609995	57.311256	64.619252
1641.447632	50.614205	64.624257
1640.937622	55.406145	64.629262
1640.182920	50.784057	64.634266
1639.455383	54.708919	64.639271
1638.604638	60.127170	64.644276
1637.547842	51.012372	64.649281
1636.814904	51.052934	64.654286
1635.931034	59.563560	64.659290
1635.804367	52.531599	64.664295
1635.292554	54.099384	64.669300
1635.188045	50.306254	64.674305
1633.981871	54.323286	64.679310
1633.316665	53.505980	64.684314
1632.734978	55.774902	64.689319
1632.236133	62.878780	64.694324
1631.568952	48.093477	64.699329
1630.342099	51.557099	64.704334
1629.670088	47.534258	64.709338
1629.068754	44.799133	64.714343
1628.795939	50.999495	64.719348
1628.499754	54.668181	64.724353
1627.276107	59.163053	64.729358
1626.907689	57.164876	64.734362
1626.375974	52.840143	64.739367
1624.863043	55.493814	64.744372
1624.409727	54.699061	64.749377
1623.527544	51.732536	64.754382
1623.370625	55.477648	64.759386
1623.143698	45.780336	64.764391
1622.020972	51.742871	64.769396
1620.956558	57.325577	64.774401
1620.422450	59.905687	64.779406
1619.962578	56.009166	64.784410
1619.723813	50.962489	64.789415
1618.946634	68.364865	64.794420
1617.909235	55.667828	64.799425
1616.804334	63.255535	64.804430
1616.261334	60.964354	64.809434
1616.247909	54.794819	64.814439
1615.573081	56.774959	64.819444
1615.464855	51.135968	64.824449
1613.969931	58.377148	64.829454
1613.392713	54.309665	64.834458
1613.174462	58.130797	64.839463
1612.301539	60.527717	64.844468
1611.415563	52.366545	64.849473
1610.687917	50.829302	64.854478
1610.400603	49.180390	64.859482
1610.030943	48.871432	64.864487
1608.751169	60.759139	64.869492
1608.017552	55.255591	64.874497
1607.415220	56.017458	64.879502
1607.050517	48.692700	64.884506
1606.106809	53.097433	64.889511
1605.359400	55.800885	64.894516
1605.124165	53.959121	64.899521
1604.195180	51.606109	64.904526
1603.156845	55.542322	64.909530
1602.366965	53.367995	64.914535
1601.269381	52.979146	64.919540
1601.776080	40.927312	64.924545
1600.709612	51.554485	64.929550
1600.442080	47.853991	64.934554
1600.039296	52.091157	64.939559
1598.910448	52.613934	64.944564
1597.719949	50.266205	64.949569
1597.431954	65.052737	64.954574
1596.673064	52.743817	64.959578
1596.328575	55.505811	64.964583
1595.626901	52.721548	64.969588
1595.853770	45.779086	64.974593
1594.285703	53.693149	64.979598
1593.839383	48.451480	64.984602
1593.394376	54.350141	64.989607
1591.898302	59.301756	64.994612
1591.098520	50.408240	64.999617
1590.449117	53.593846	65.004622
1590.223943	55.886625	65.009626
1590.019582	50.963531	65.014631
1589.197479	52.229568	65.019636
1588.246167	46.843412	65.024641
1587.626149	58.926882	65.029646
1587.201614	49.787578	65.034650
1586.858000	45.210804	65.039655
1585.683125	40.819708	65.044660
1584.991008	41.693649	65.049665
1584.136449	54.076584	65.054670
1583.801922	52.343389	65.059674
1583.146294	51.083155	65.064679
1581.899368	52.382030	65.069684
1581.659292	49.255101	65.074689
1581.192231	48.621382	65.079694
1580.497263	46.228327	65.084698
1580.256174	44.778734	65.089703
1578.976315	53.995390	65.094708
1578.517390	48.618912	65.099713
1577.242548	56.109790	65.104718
1576.865353	50.130008	65.109722
1576.739033	50.694762	65.114727
1575.907586	54.069017	65.119732
1575.014781	43.938195	65.124737
1574.209861	50.857618	65.129742
1574.212298	53.522346	65.134746
1573.789310	56.991692	65.139751
1572.294270	49.203570	65.144756
1571.869479	48.383021	65.149761
1571.076634	52.156441	65.154766
1570.601866	43.731499	65.159770
1569.835844	52.454842	65.164775
1568.770362	46.838371	65.169780
1568.431609	47.168309	65.174785
1567.605998	50.986414	65.179790
1567.170920	52.560413	65.184794
1567.189440	43.983552	65.189799
1565.900029	50.177507	65.194804
1565.354732	43.534162	65.199809
1564.630093	49.753429	65.204814
1563.871052	52.642026	65.209818
1562.988745	48.847809	65.214823
1562.172691	66.254465	65.219828
1562.190084	47.510220	65.224833
1561.522273	54.223426	65.229838
1560.854274	43.290748	65.234842
1560.086970	49.957824	65.239847
1559.203731	50.652908	65.244852
1558.600740	50.351914	65.249857
1558.180954	53.324944	65.254862
1556.894320	51.306691	65.259866
1556.513473	41.209832	65.264871
1555.747232	45.750375	65.269876
1555.566007	52.501878	65.274881
1555.053840	54.556023	65.279886
1553.828676	51.827019	65.284890
1552.945653	51.592503	65.289895
1552.804139	46.870623	65.294900
1552.508442	48.871537	65.299905
1551.679419	54.050036	65.304910
1550.683656	50.654958	65.309914
1549.983966	52.963424	65.314919
1548.930359	56.065455	65.319924
1548.607565	54.441960	65.324929
1548.051699	55.732699	65.329934
1547.105893	46.546439	65.334938
1546.359578	57.322899	65.339943
1545.403119	50.095478	65.344948
1545.589212	39.434246	65.349953
1544.833194	44.141190	65.354958
1544.691123	47.945729	65.359962
1543.303447	45.450980	65.364967
1542.617759	52.273030	65.369972
1541.949992	51.998518	65.374977
1541.604187	43.621375	65.379982
1541.346075	56.896532	65.384986
1540.327255	53.646317	65.389991
1539.702551	56.915329	65.394996
1538.986726	53.586811	65.400001
1537.904193	49.138083	65.405006
1536.957218	52.847495	65.410010
1536.844233	53.017616	65.415015
1535.673700	56.767264	65.420020
1535.902882	51.561564	65.425025
1535.126525	46.718610	65.430030
1533.689343	50.930716	65.435034
1533.478815	46.341433	65.440039
1532.876675	57.720426	65.445044
1532.576130	45.731752	65.450049
1531.632986	46.261837	65.455054
1530.636976	41.043208	65.460058
1529.858290	44.490143	65.465063
1529.582817	55.541660	65.470068
1529.438720	46.097411	65.475073
1527.939457	47.253177	65.480078
1527.424819	42.668577	65.485082
1526.956221	42.916534	65.490087
1526.362294	47.255097	65.495092
1526.000111	45.868072	65.500097
1524.817716	55.356596	65.505102
1524.045590	53.583832	65.510106
1523.585906	50.899870	65.515111
1523.147821	55.893443	65.520116
1523.006551	43.487135	65.525121
1521.280180	50.784915	65.530126
1520.403009	48.160170	65.535130
1519.940171	38.596803	65.540135
1519.323525	52.698676	65.545140
1519.158437	51.831710	65.550145
1518.691416	55.355960	65.555150
1517.377443	55.241389	65.560154
1516.857141	49.388342	65.565159
1516.165775	54.281980	65.570164
1515.900674	48.255788	65.575169
1515.686684	49.993257	65.580174
1514.479349	52.042048	65.585178
1514.172485	52.359031	65.590183
1512.940775	52.265907	65.595188
1512.583075	41.138825	65.600193
1511.777740	49.016700	65.605198
1511.087716	53.338162	65.610202
1510.591490	41.723628	65.615207
1509.233199	51.789337	65.620212
1508.666176	55.162947	65.625217
1508.117711	52.689567	65.630222
1507.712872	46.777289	65.635226
1507.263777	49.137997	65.640231
1506.962333	49.851535	65.645236
1506.093052	45.410526	65.650241
1505.089966	54.817444	65.655246
1504.122998	47.384212	65.660250
1503.918662	46.203847	65.665255
1503.536975	47.654638	65.670260
1502.182038	44.145002	65.675265
1501.580781	42.699429	65.680270
1501.198412	57.202504	65.685274
1500.789627	47.884477	65.690279
1499.151464	51.671143	65.695284
1498.967858	50.313159	65.700289
1498.526553	52.158611	65.705294
1497.718480	49.307711	65.710298
1497.852917	50.089535	65.715303
1496.512777	56.233374	65.720308
1495.199912	54.407119	65.725313
1494.812032	53.860904	65.730318
1494.410166	54.460584	65.735322
1494.162545	50.069090	65.740327
1493.567006	57.937115	65.745332
1492.929859	54.325941	65.750337
1491.896173	56.697500	65.755342
1491.389027	57.962143	65.760346
1490.742183	50.442940	65.765351
1489.939587	54.800644	65.770356
1489.125374	48.247940	65.775361
1488.712911	52.275197	65.780366
1488.068775	52.830295	65.785370
1487.718112	52.734795	65.790375
1486.157232	53.802835	65.795380
1485.730165	48.667222	65.800385
1485.169037	56.703428	65.805390
1485.302915	50.011346	65.810394
1484.567283	42.371956	65.815399
1482.674950	50.293782	65.820404
1482.565577	44.566189	65.825409
1481.999798	52.094396	65.830414
1481.501922	54.657657	65.835418
1481.287291	42.064186	65.840423
1479.781237	51.468380	65.845428
1479.148311	46.591414	65.850433
1478.704908	51.869700	65.855438
1477.886507	47.863257	65.860442
1476.931080	43.195037	65.865447
1476.363846	54.790675	65.870452
1475.558435	42.563967	65.875457
1475.215680	53.566997	65.880462
1475.202718	53.800523	65.885466
1475.086743	40.107850	65.890471
1473.465558	42.276822	65.895476
1472.446900	46.054166	65.900481
1471.702345	45.533082	65.905486
1471.387670	49.214407	65.910490
1471.024467	39.908719	65.915495
1469.857637	53.485447	65.920500
1469.038109	44.383381	65.925505
1468.307298	48.878398	65.930510
1468.051250	50.758455	65.935514
1467.966361	46.410556	65.940519
1467.074942	47.552692	65.945524
1466.227048	48.627776	65.950529
1465.470762	55.858213	65.955534
1464.895344	54.129550	65.960538
1464.531625	46.068101	65.965543
1463.239795	48.958300	65.970548
1462.427861	46.734092	65.975553
1461.807559	45.962411	65.980558
1461.558322	58.134778	65.985562
1461.515275	46.287956	65.990567
1460.006546	59.100615	65.995572
1459.600516	54.790708	66.000577
1459.129134	46.035221	66.005582
1458.578042	45.648386	66.010586
1457.659721	49.127520	66.015591
1456.377683	57.126863	66.020596
1456.082154	41.979993	66.025601
1455.973185	52.681308	66.030606
1455.075960	45.975461	66.035610
1454.160438	53.379198	66.040615
1453.065346	56.481242	66.045620
1452.949507	48.644590	66.050625
1452.449186	49.567031	66.055630
1451.684154	54.582621	66.060634
1451.166938	52.209685	66.065639
1450.063086	53.396869	66.070644
1449.517503	43.382696	66.075649
1448.930976	49.125985	66.080654
1448.573955	57.571709	66.085658
1447.840331	51.247182	66.090663
1446.705109	60.734750	66.095668
1446.210855	48.180063	66.100673
1446.087101	47.369181	66.105678
1444.972305	51.773616	66.110682
1444.499820	48.832919	66.115687
1443.298672	52.784788	66.120692
1442.839173	53.088429	66.125697
1442.329414	51.262087	66.130702
1441.856150	55.871702	66.135706
1440.914344	46.359934	66.140711
1439.796448	50.967391	66.145716
1439.422405	46.480706	66.150721
1439.130232	49.331245	66.155726
1438.742510	49.512474	66.160730
1438.200115	53.009368	66.165735
1437.015172	54.711332	66.170740
1436.632993	45.642963	66.175745
1436.325709	49.779713	66.180750
1435.033236	49.191769	66.185754
1434.502816	41.407139	66.190759
1433.507563	53.347208	66.195764
1432.947739	49.854647	66.200769
1432.577923	50.523446	66.205774
1431.984182	52.076851	66.210778
1431.065700	50.562433	66.215783
1430.011512	50.815110	66.220788
1429.739506	51.309281	66.225793
1429.215264	52.461598	66.230798
1428.376887	50.179557	66.235802
1428.066430	50.204279	66.240807
1426.623836	54.323000	66.245812
1426.213112	54.458827	66.250817
1426.212374	54.657893	66.255822
1425.560815	46.544277	66.260826
1424.691343	44.858058	66.265831
1423.407621	50.317284	66.270836
1423.016548	41.000586	66.275841
1422.399763	45.540032	66.280846
1422.144726	62.648556	66.285850
1421.711867	48.954075	66.290855
1420.408840	41.788776	66.295860
1419.385710	40.844484	66.300865
1418.853814	53.124039	66.305870
1418.909790	53.773244	66.310874
1418.075400	50.444913	66.315879
1416.997933	55.423595	66.320884
1416.515228	50.929854	66.325889
1415.895881	47.302228	66.330894
1415.349870	48.594845	66.335898
1415.148968	41.433915	66.340903
1413.832545	53.173972	66.345908
1413.554030	52.059991	66.350913
1412.986065	56.136368	66.355918
1412.115704	56.640597	66.360922
1411.024525	46.983887	66.365927
1410.195814	59.087289	66.370932
1409.674615	53.907801	66.375937
1409.571977	48.394971	66.380942
1409.056699	51.641315	66.385946
1408.397164	50.646630	66.390951
1407.484117	50.034797	66.395956
1407.066750	48.329613	66.400961
1405.928617	45.793374	66.405966
1404.872154	48.747503	66.410970
1404.300673	45.711657	66.415975
1403.679377	48.267234	66.420980
1403.556346	55.649794	66.425985
1403.313444	56.030832	66.430990
1401.901544	54.817974	66.435994
1401.245251	55.750145	66.440999
1400.442264	54.984480	66.446004
1400.275213	52.168735	66.451009
1400.054905	47.993618	66.456014
1398.817156	57.291512	66.461018
1398.040931	48.903201	66.466023
1397.257423	55.559645	66.471028
1396.912037	51.615533	66.476033
1396.477503	54.135591	66.481038
1395.339751	61.189764	66.486042
1394.851512	47.549769	66.491047
1394.165889	56.820650	66.496052
1393.907258	46.377650	66.501057
1392.724331	51.949097	66.506062
1391.910487	61.011019	66.511066
1391.677838	52.930695	66.516071
1390.991447	58.460964	66.521076
1390.638755	53.298817	66.526081
1389.442001	52.340832	66.531086
1388.763863	56.920785	66.536090
1388.151144	44.562437	66.541095
1387.606873	53.896749	66.546100
1386.875594	46.806477	66.551105
1386.313860	60.542522	66.556110
1385.054415	50.110975	66.561114
1385.030104	46.971602	66.566119
1384.291635	53.482580	66.571124
1384.028386	42.865514	66.576129
1382.776244	48.016198	66.581134
1381.522786	49.987653	66.586138
1381.400673	45.187469	66.591143
1380.908325	46.898777	66.596148
1380.374917	40.854192	66.601153
1379.819077	41.885217	66.606158
1378.760830	42.939088	66.611162
1378.601233	42.963646	66.616167
1377.682578	45.637228	66.621172
1377.174028	50.748650	66.626177
1375.949820	48.649896	66.631182
1375.193581	54.138044	66.636186
1374.999378	45.227763	66.641191
1374.184091	51.440063	66.646196
1373.928221	55.205663	66.651201
1373.367956	50.645473	66.656206
1372.043482	55.083445	66.661210
1371.330915	43.753857	66.666215
1370.492668	50.824258	66.671220
1370.707713	52.911822	66.676225
1370.261593	53.842360	66.681230
1369.535175	46.665211	66.686234
1368.512540	45.759528	66.691239
1367.592597	37.751473	66.696244
1367.204076	37.708644	66.701249
1366.023934	39.210863	66.706254
1364.881187	44.627414	66.711258
1364.707017	36.651165	66.716263
1364.207284	46.269940	66.721268
1363.972856	49.200987	66.726273
1363.987586	39.002110	66.731278
1363.339469	50.829868	66.736282
1362.169934	49.633557	66.741287
1361.011131	51.068970	66.746292
1359.966851	35.221391	66.751297
1359.574436	44.591673	66.756302
1358.843821	53.522115	66.761306
1358.560228	45.663273	66.766311
1357.869041	48.197662	66.771316
1357.221363	48.580100	66.776321
1356.313503	49.140886	66.781326
1355.687197	54.933620	66.786330
1355.278674	46.059240	66.791335
1355.057206	50.854690	66.796340
1354.015254	39.680174	66.801345
1353.194268	40.527259	66.806350
1352.070235	46.778990	66.811354
1351.886383	45.422636	66.816359
1351.422848	48.602497	66.821364
1350.827240	46.195628	66.826369
1349.642000	46.806660	66.831374
1348.738510	49.396734	66.836378
1348.803585	47.558841	66.841383
1347.727799	53.571407	66.846388
1347.709640	49.448922	66.851393
1346.361136	46.641620	66.856398
1345.328559	48.187264	66.861402
1345.315335	45.383084	66.866407
1344.632523	46.800962	66.871412
1344.508445	45.379115	66.876417
1343.641153	45.851252	66.881422
1342.770899	52.798062	66.886426
1342.282374	48.631366	66.891431
1340.993110	49.380597	66.896436
1339.856978	53.663182	66.901441
1339.662696	46.727299	66.906446
1338.863276	57.596141	66.911450
1338.553774	42.164729	66.916455
1338.216165	42.854072	66.921460
1338.091731	48.856931	66.926465
1337.346860	38.407582	66.931470
1335.938057	50.388846	66.936474
1335.434390	45.936205	66.941479
1334.794455	43.501797	66.946484
1333.623033	47.579249	66.951489
1332.812255	42.255543	66.956494
1332.340489	46.360848	66.961498
1332.239636	42.075689	66.966503
1331.768535	52.617942	66.971508
1331.262502	53.482164	66.976513
1330.209207	52.581738	66.981518
1329.355412	53.662195	66.986522
1329.001800	40.624804	66.991527
1328.120638	52.338911	66.996532
1327.132623	49.109526	67.001537
1326.651714	46.154103	67.006542
1326.017696	61.848481	67.011546
1325.867465	53.761951	67.016551
1324.916896	51.498740	67.021556
1323.924239	48.673552	67.026561
1322.886997	48.058523	67.031566
1322.663173	55.131901	67.036570
1322.275866	48.068807	67.041575
1321.600852	47.322299	67.046580
1321.397444	48.233395	67.051585
1320.323288	47.400486	67.056590
1319.225124	53.364784	67.061594
1319.117554	47.449800	67.066599
1318.088534	56.040162	67.071604
1317.011486	49.957998	67.076609
1316.536550	42.954907	67.081614
1315.780269	48.898965	67.086618
1315.597428	48.465289	67.091623
1315.255343	52.653392	67.096628
1314.752274	52.523603	67.101633
1313.623147	44.222569	67.106638
1312.543480	50.013972	67.111642
1312.349311	41.700904	67.116647
1311.879518	45.115116	67.121652
1310.669075	42.384843	67.126657
1310.116227	47.372409	67.131662
1309.475253	44.287688	67.136666
1309.342899	40.739335	67.141671
1308.526091	49.879129	67.146676
1307.593203	39.195144	67.151681
1307.057856	36.535610	67.156686
1306.251070	44.380589	67.161690
1306.090625	39.392774	67.166695
1304.870516	50.318631	67.171700
1304.086627	43.975902	67.176705
1303.877183	38.975950	67.181710
1303.100966	46.365325	67.186714
1302.584920	46.567743	67.191719
1301.368451	56.390535	67.196724
1300.960176	42.385973	67.201729
1300.578716	47.427880	67.206734
1299.741296	48.852495	67.211738
1298.741799	42.864426	67.216743
1297.640850	51.651436	67.221748
1297.364618	46.137941	67.226753
1296.873868	50.608850	67.231758
1296.613810	50.919412	67.236762
1296.402413	50.203665	67.241767
1294.976947	49.046843	67.246772
1294.313555	48.187434	67.251777
1293.857657	45.521798	67.256782
1293.070488	46.720717	67.261786
1292.771772	41.323174	67.266791
1291.821845	49.904733	67.271796
1291.205798	49.117741	67.276801
1290.853243	44.616344	67.281806
1290.005369	52.552043	67.286810
1289.347369	42.722933	67.291815
1287.610838	45.343133	67.296820
1287.530811	42.815247	67.301825
1286.712717	47.335090	67.306830
1286.741995	51.990119	67.311834
1286.154011	44.624298	67.316839
1284.695691	52.613584	67.321844
1284.122880	47.656102	67.326849
1284.008750	43.405191	67.331854
1283.223690	49.739818	67.336858
1283.001537	43.163171	67.341863
1281.641775	50.234049	67.346868
1280.777137	44.393415	67.351873
1280.536004	45.464516	67.356878
1279.795394	52.106914	67.361882
1279.466044	42.746912	67.366887
1279.300936	53.369800	67.371892
1277.924459	48.463460	67.376897
1277.354549	47.611337	67.381902
1276.582848	50.324906	67.386906
1275.934087	47.521772	67.391911
1274.642531	47.714070	67.396916
1274.393984	44.747689	67.401921
1274.053538	47.475450	67.406926
1273.601121	47.778683	67.411930
1273.153769	45.470780	67.416935
1271.909411	50.499765	67.421940
1270.983881	51.316210	67.426945
1270.828621	46.827220	67.431950
1269.972072	54.819668	67.436954
1269.206683	47.916041	67.441959
1268.428638	45.109386	67.446964
1267.720397	50.388414	67.451969
1267.712359	44.857823	67.456974
1266.906745	46.994595	67.461978
1266.094255	44.151207	67.466983
1265.054918	48.701825	67.471988
1264.833847	40.900976	67.476993
1264.645052	35.008984	67.481998
1263.263832	51.814116	67.487002
1262.553044	45.375201	67.492007
1262.029078	44.988087	67.497012
1261.377852	50.939427	67.502017
1261.229797	49.640102	67.507022
1259.815928	50.443053	67.512026
1259.305053	43.339155	67.517031
1258.513694	51.355571	67.522036
1257.958192	50.056531	67.527041
1257.873242	47.406732	67.532046
1255.981568	62.736184	67.537050
1256.159993	49.252470	67.542055
1255.243896	47.267175	67.547060
1254.637754	49.039815	67.552065
1254.582107	50.885571	67.557070
1253.689469	60.406232	67.562074
1252.844167	43.657425	67.567079
1251.955234	50.278246	67.572084
1251.601941	49.893491	67.577089
1251.359150	43.858775	67.582094
1249.667718	52.202173	67.587098
1249.266645	55.993817	67.592103
1248.580066	59.267527	67.597108
1248.113677	41.420876	67.602113
1248.132430	42.941277	67.607118
1246.740535	54.415213	67.612122
1245.841661	42.998351	67.617127
1245.483253	51.995331	67.622132
1244.936170	52.918691	67.627137
1244.762801	43.443574	67.632142
1243.605508	48.438316	67.637146
1242.800120	38.418542	67.642151
1242.172642	47.702757	67.647156
1241.372718	46.309389	67.652161
1241.245710	48.042236	67.657166
1240.112637	57.742606	67.662170
1239.604352	42.846935	67.667175
1238.963981	45.716830	67.672180
1238.432957	57.539545	67.677185
1237.603478	51.034115	67.682190
1236.537645	52.067209	67.687194
1235.924090	50.973892	67.692199
1236.055579	53.601911	67.697204
1235.243404	50.006142	67.702209
1234.585144	45.893784	67.707214
1233.594810	56.501250	67.712218
1232.804621	44.930395	67.717223
1232.370997	50.278852	67.722228
1231.762954	46.901940	67.727233
1231.118129	51.965256	67.732238
1230.485454	43.784111	67.737242
1230.213869	44.003496	67.742247
1229.113920	47.646778	67.747252
1228.080684	46.214808	67.752257
1227.748140	48.894247	67.757262
1226.814166	54.114431	67.762266
1226.732867	46.075718	67.767271
1225.724553	45.689430	67.772276
1224.776007	49.942287	67.777281
1224.241736	44.532187	67.782286
1223.658254	46.476995	67.787290
1223.395435	40.365190	67.792295
1222.358709	42.214710	67.797300
1221.357983	50.284341	67.802305
1220.960459	45.768152	67.807310
1220.282690	47.908699	67.812314
1219.934470	41.423904	67.817319
1219.428399	46.563721	67.822324
1218.225073	43.980669	67.827329
1217.420550	36.248933	67.832334
1216.856434	50.692309	67.837338
1216.527500	41.642890	67.842343
1216.081756	49.488430	67.847348
1215.374518	51.396404	67.852353
1214.216936	43.202900	67.857358
1213.290833	54.018043	67.862362
1213.304853	50.407531	67.867367
1212.475812	47.081089	67.872372
1212.037310	51.951590	67.877377
1211.441939	35.565785	67.882382
1210.409764	48.563714	67.887386
1209.527393	48.617686	67.892391
1209.511644	44.194022	67.897396
1208.602999	47.218794	67.902401
1207.729930	47.948904	67.907406
1206.955267	48.983465	67.912410
1206.955615	39.723733	67.917415
1206.524277	52.786945	67.922420
1205.356955	48.067046	67.927425
1204.529095	45.667990	67.932430
1203.688383	54.120340	67.937434
1203.386662	44.954556	67.942439
1202.797619	47.767118	67.947444
1201.809888	54.087903	67.952449
1201.286448	45.873062	67.957454
1200.590922	59.309127	67.962458
1200.335222	57.297218	67.967463
1199.613882	55.106887	67.972468
1198.264296	54.229982	67.977473
1197.944532	45.044790	67.982478
1197.222843	54.039629	67.987482
1196.657205	56.853316	67.992487
1196.298368	53.382033	67.997492
1194.887680	48.819850	68.002497
1194.522048	54.319292	68.007502
1193.943984	53.035965	68.012506
1193.620412	38.708655	68.017511
1193.099532	47.693582	68.022516
1191.968053	51.761460	68.027521
1191.661501	47.204437	68.032526
1190.695821	56.685110	68.037530
1189.775670	48.545692	68.042535
1188.833983	56.676270	68.047540
1188.438954	51.228913	68.052545
1187.945957	51.123464	68.057550
1187.396151	52.404516	68.062554
1187.202616	58.131849	68.067559
1186.684174	54.419485	68.072564
1185.290410	58.469513	68.077569
1184.930559	44.959556	68.082574
1184.370546	50.031642	68.087578
1183.646344	48.122843	68.092583
1182.397337	48.725096	68.097588
1181.489105	50.523810	68.102593
1181.452359	53.974802	68.107598
1181.091542	63.222845	68.112602
1180.551859	54.477916	68.117607
1179.208638	54.893810	68.122612
1178.371090	54.375667	68.127617
1178.135193	49.692869	68.132622
1177.389939	56.703949	68.137626
1177.401741	46.696237	68.142631
1176.570175	48.615240	68.147636
1175.296350	53.461403	68.152641
1175.097042	41.633880	68.157646
1174.467184	55.922734	68.162650
1173.302446	48.610292	68.167655
1172.599209	50.390091	68.172660
1171.915264	52.408945	68.177665
1172.056628	44.719332	68.182670
1171.257596	47.479828	68.187674
1170.502737	40.671525	68.192679
1169.402563	42.741513	68.197684
1168.910305	46.915068	68.202689
1168.957072	44.910583	68.207694
1167.528646	44.370854	68.212698
1166.038208	40.835973	68.217703
1166.058411	47.036680	68.222708
1165.183294	46.504052	68.227713
1165.292023	43.112184	68.232718
1164.499846	53.789931	68.237722
1163.399578	45.337168	68.242727
1162.746399	48.793840	68.247732
1161.922096	53.713427	68.252737
1161.512120	48.917154	68.257742
1161.445411	56.623199	68.262746
1160.386175	53.497225	68.267751
1159.639973	49.882676	68.272756
1159.209338	49.190265	68.277761
1158.819009	44.458127	68.282766
1157.438148	53.784899	68.287770
1156.533530	46.588970	68.292775
1156.240410	58.809480	68.297780
1155.437349	60.604796	68.302785
1155.152624	51.766090	68.307790
1154.439321	60.602796	68.312794
1154.163079	52.091833	68.317799
1153.124865	54.215161	68.322804
1152.172544	61.173281	68.327809
1152.207713	47.759106	68.332814
1150.991176	62.040265	68.337818
1149.993416	59.880692	68.342823
1149.614225	56.922084	68.347828
1149.036025	56.062712	68.352833
1149.066876	51.245827	68.357838
1148.079668	55.844379	68.362842
1147.246277	59.159025	68.367847
1146.797336	56.427086	68.372852
1145.870717	50.929841	68.377857
1145.370377	54.628360	68.382862
1143.852800	56.099199	68.387866
1143.310255	51.214711	68.392871
1142.768831	48.101524	68.397876
1142.532611	55.061761	68.402881
1142.183795	39.915798	68.407886
1140.911830	46.398934	68.412890
1140.206329	46.561180	68.417895
1139.536648	45.971672	68.422900
1138.994483	44.077894	68.427905
1138.898452	36.258812	68.432910
1138.263338	42.540539	68.437914
1137.600260	49.445184	68.442919
1136.656706	52.109252	68.447924
1135.939272	54.459881	68.452929
1135.559101	44.084313	68.457934
1134.324937	45.387027	68.462938
1133.492943	44.988724	68.467943
1133.126121	49.777089	68.472948
1132.606194	47.262166	68.477953
1132.468211	44.098453	68.482958
1131.198731	58.042508	68.487962
1130.303395	40.930096	68.492967
1130.136001	41.471892	68.497972
1129.620597	47.469058	68.502977
1129.036640	40.962670	68.507982
1127.479666	50.795629	68.512986
1127.016245	45.254604	68.517991
1126.608239	45.048560	68.522996
1126.344754	48.180365	68.528001
1125.658883	39.599822	68.533006
1124.419283	46.057683	68.538010
1123.836251	45.549651	68.543015
1123.474311	46.030816	68.548020
1123.039664	50.460550	68.553025
1122.316326	42.376661	68.558030
1121.080872	49.234846	68.563034
1120.522651	42.419330	68.568039
1120.214444	41.359793	68.573044
1119.559621	43.190517	68.578049
1118.604338	47.449673	68.583054
1117.437033	49.245392	68.588058
1117.578192	44.423437	68.593063
1116.883040	39.801919	68.598068
1116.129115	43.888840	68.603073
1115.408114	39.881191	68.608078
1114.477801	40.305344	68.613082
1113.954785	44.203920	68.618087
1113.836019	45.349201	68.623092
1112.643795	39.780217	68.628097
1112.078030	36.697650	68.633102
1111.092794	53.561697	68.638106
1110.453556	43.955195	68.643111
1110.014738	39.843573	68.648116
1109.513152	51.261786	68.653121
1109.282575	37.851684	68.658126
1108.217109	42.451402	68.663130
1107.332778	42.603223	68.668135
1107.084865	40.917604	68.673140
1105.948678	49.425684	68.678145
1105.306170	40.369981	68.683150
1104.252182	44.133698	68.688154
1103.447448	44.461749	68.693159
1103.505386	42.993350	68.698164
1102.894814	52.364672	68.703169
1103.133776	46.277480	68.708174
1102.116542	41.229165	68.713178
1101.032980	49.660739	68.718183
1100.061608	50.039033	68.723188
1099.626360	53.610757	68.728193
1099.366078	46.994082	68.733198
1098.009241	55.454295	68.738202
1097.679832	40.728156	68.743207
1097.481270	42.933101	68.748212
1095.923588	52.998678	68.753217
1095.292459	49.117344	68.758222
1094.337691	47.712228	68.763226
1094.363156	45.684550	68.768231
1093.781124	43.405651	68.773236
1093.341158	41.214920	68.778241
1092.233095	41.726353	68.783246
1091.496625	54.453013	68.788250
1091.098146	46.095618	68.793255
1090.529691	48.763356	68.798260
1089.411425	46.550622	68.803265
1088.745660	45.105493	68.808270
1087.919155	50.687404	68.813274
1087.364278	50.159557	68.818279
1087.034030	44.028526	68.823284
1086.681238	57.269723	68.828289
1086.323424	49.075487	68.833294
1085.138181	47.506164	68.838298
1084.528302	43.753820	68.843303
1084.021214	53.461484	68.848308
1082.791194	51.151445	68.853313
1082.010403	43.548695	68.858318
1081.469148	46.902924	68.863322
1081.524191	45.055304	68.868327
1080.412035	44.062385	68.873332
1079.517908	48.466200	68.878337
1079.052082	41.197919	68.883342
1078.602556	45.652305	68.888346
1078.299790	45.722703	68.893351
1077.319502	43.844748	68.898356
1075.941937	42.266521	68.903361
1075.507877	41.344980	68.908366
1074.887025	50.723587	68.913370
1074.625873	49.709282	68.918375
1074.133287	41.312353	68.923380
1072.963945	48.240142	68.928385
1072.500321	41.406464	68.933390
1071.811973	45.995293	68.938394
1071.094245	42.573246	68.943399
1070.833997	43.258437	68.948404
1069.852034	47.845837	68.953409
1069.418383	34.766557	68.958414
1068.553299	46.325164	68.963418
1068.081558	41.255681	68.968423
1066.870913	38.918648	68.973428
1065.756799	44.856900	68.978433
1065.505876	34.607633	68.983438
1064.764832	45.282543	68.988442
1064.707128	33.876036	68.993447
1064.280178	46.795202	68.998452
1063.820969	44.303837	69.003457
1062.930249	34.365435	69.008462
1062.043311	40.212286	69.013466
1061.400956	45.383342	69.018471
1060.301186	44.662240	69.023476
1059.461227	48.831793	69.028481
1059.080564	47.426265	69.033486
1058.361583	44.892151	69.038490
1058.168106	37.806175	69.043495
1057.776983	43.914290	69.048500
1056.778653	42.955567	69.053505
1056.299554	45.132767	69.058510
1055.393737	41.932789	69.063514
1054.713158	43.145462	69.068519
1053.921031	42.267871	69.073524
1052.919669	47.991038	69.078529
1052.656034	42.126091	69.083534
1052.214317	37.021867	69.088538
1051.732410	37.752911	69.093543
1050.518017	38.280982	69.098548
1049.253271	42.573010	69.103553
1049.559433	35.257405	69.108558
1048.726992	39.833017	69.113562
1048.421112	37.045413	69.118567
1047.500005	41.805937	69.123572
1046.565693	46.965414	69.128577
1046.474787	38.710485	69.133582
1045.674871	50.053473	69.138586
1044.703189	35.041040	69.143591
1043.934597	42.270845	69.148596
1043.223310	47.907237	69.153601
1043.434454	46.635618	69.158606
1041.849519	42.308580	69.163610
1041.135426	50.757809	69.168615
1040.867270	41.015941	69.173620
1039.734902	49.923620	69.178625
1039.594661	47.310139	69.183630
1039.087007	36.354877	69.188634
1038.044554	39.777173	69.193639
1037.491335	41.199737	69.198644
1036.834812	43.240355	69.203649
1036.440900	34.835223	69.208654
1035.187008	45.305077	69.213658
1034.159999	36.921126	69.218663
1033.841170	41.829159	69.223668
1033.458786	43.111948	69.228673
1033.296298	34.222341	69.233678
1032.745652	49.890574	69.238682
1031.914752	55.147999	69.243687
1031.108911	49.667599	69.248692
1030.240816	49.632715	69.253697
1029.276485	34.685737	69.258702
1028.224077	48.283558	69.263706
1027.916939	46.246921	69.268711
1027.325919	42.364652	69.273716
1026.909435	44.189306	69.278721
1026.908905	38.683893	69.283726
1026.106472	42.974121	69.288730
1024.795264	44.948836	69.293735
1024.424060	38.342881	69.298740
1023.753438	37.331204	69.303745
1023.113059	44.225256	69.308750
1021.808163	43.595340	69.313754
1021.320026	44.141542	69.318759
1021.541521	43.056035	69.323764
1020.522345	37.700591	69.328769
1019.656992	39.711055	69.333774
1018.483957	50.431133	69.338778
1017.594732	46.823342	69.343783
1017.347571	39.877214	69.348788
1016.916772	36.283679	69.353793
1016.716612	32.707093	69.358798
1016.035280	35.724542	69.363802
1014.990974	34.746861	69.368807
1014.268042	34.035445	69.373812
1013.615163	44.858276	69.378817
1013.078105	45.947697	69.383822
1012.582509	39.550930	69.388826
1011.592432	43.580809	69.393831
1011.040043	44.713906	69.398836
1010.424227	41.921753	69.403841
1010.035383	38.651806	69.408846
1009.024169	51.132239	69.413850
1007.772947	50.111840	69.418855
1007.871054	39.922406	69.423860
1006.806007	43.381733	69.428865
1006.818035	30.727833	69.433870
1006.174687	40.036082	69.438874
1005.112615	41.338959	69.443879
1004.435808	34.908099	69.448884
1003.562191	42.387592	69.453889
1003.415358	32.934416	69.458894
1002.182357	37.948478	69.463898
1001.656430	44.855693	69.468903
1001.074237	35.864683	69.473908
1000.579213	41.857573	69.478913
1000.125648	41.008059	69.483918
999.517417	47.960553	69.488922
998.186899	44.532544	69.493927
997.754343	40.771163	69.498932
997.143243	48.056499	69.503937
997.114895	38.515533	69.508942
995.657509	36.719696	69.513946
994.857516	45.296130	69.518951
995.046396	39.539608	69.523956
994.215651	49.132178	69.528961
992.771999	36.630860	69.533966
992.381984	40.427327	69.538970
991.985451	41.618599	69.543975
992.069488	38.401875	69.548980
990.576463	43.717827	69.553985
990.087297	44.342362	69.558990
988.804467	40.436873	69.563994
988.706964	48.062520	69.568999
988.038797	40.151575	69.574004
986.649274	48.141374	69.579009
986.155636	35.989312	69.584014
985.437226	41.326547	69.589018
985.373137	42.456150	69.594023
984.987981	37.707757	69.599028
984.387872	47.327931	69.604033
983.697118	33.481165	69.609038
982.503447	51.018374	69.614042
982.092363	48.520750	69.619047
981.796260	44.218528	69.624052
980.167237	49.012671	69.629057
979.636366	42.248153	69.634062
979.074009	45.425617	69.639066
978.274316	45.685723	69.644071
978.060188	47.879126	69.649076
977.442429	43.451605	69.654081
977.328446	40.303134	69.659086
976.578522	45.609849	69.664090
975.679479	46.160902	69.669095
975.113586	39.576454	69.674100
973.352670	41.143091	69.679105
973.164954	35.777496	69.684110
972.660199	40.927755	69.689114
971.951619	41.436718	69.694119
971.738548	33.825583	69.699124
970.914295	45.500748	69.704129
970.296184	38.663941	69.709134
969.564121	38.532354	69.714138
968.786456	40.830161	69.719143
967.856719	41.727902	69.724148
967.009285	44.104366	69.729153
966.701989	45.847170	69.734158
965.983987	53.099109	69.739162
965.741049	47.191155	69.744167
965.163724	37.364494	69.749172
964.208224	45.359698	69.754177
963.448230	41.045351	69.759182
962.963861	45.624913	69.764186
961.979027	45.102823	69.769191
961.470135	45.458385	69.774196
960.316138	47.227386	69.779201
960.092352	41.137743	69.784206
959.701633	46.832524	69.789210
959.203657	46.519540	69.794215
958.669455	39.422457	69.799220
957.011582	44.525872	69.804225
956.641222	40.720688	69.809230
956.061003	41.924869	69.814234
955.788111	40.762985	69.819239
955.214361	37.161179	69.824244
954.275732	42.137468	69.829249
953.525838	39.090011	69.834254
953.136979	43.598351	69.839258
952.371479	41.580618	69.844263
951.962654	32.061799	69.849268
950.898493	44.902991	69.854273
950.496648	34.153433	69.859278
950.014608	41.214571	69.864282
948.631272	39.147527	69.869287
947.765912	33.558930	69.874292
946.990728	32.158220	69.879297
946.757735	34.086446	69.884302
946.308352	41.678015	69.889306
946.191927	41.214428	69.894311
945.555237	32.063433	69.899316
944.405435	49.208280	69.904321
943.771216	38.255373	69.909326
943.293207	40.442656	69.914330
942.342617	46.890131	69.919335
941.100356	41.368055	69.924340
940.543306	47.394465	69.929345
939.926215	43.922049	69.934350
939.476371	43.382547	69.939354
939.259742	44.845759	69.944359
939.185521	35.911047	69.949364
937.613118	49.452282	69.954369
937.077753	43.006287	69.959374
936.492631	45.295596	69.964378
936.067366	47.859879	69.969383
935.169382	31.655851	69.974388
933.929061	38.567001	69.979393
933.561793	39.245265	69.984398
933.249277	42.543751	69.989402
932.530888	43.336621	69.994407
932.219644	30.139313	69.999412
930.914882	41.334300	70.004417
930.303079	40.768066	70.009422
930.150262	41.038964	70.014426
929.171348	47.518132	70.019431
928.287317	41.460258	70.024436
927.375607	41.203532	70.029441
927.121779	35.856765	70.034446
926.684875	42.807941	70.039450
926.443313	38.761240	70.044455
925.280139	33.441932	70.049460
924.047196	38.534943	70.054465
923.855938	34.428709	70.059470
923.303935	38.120297	70.064474
923.025735	36.865778	70.069479
922.231508	32.521779	70.074484
921.184039	45.212097	70.079489
920.973802	34.367759	70.084494
919.965951	43.067817	70.089498
918.410890	43.626636	70.094503
918.186446	37.730128	70.099508
917.577710	40.229524	70.104513
917.479662	34.085197	70.109518
916.860947	32.469809	70.114522
916.255098	37.604622	70.119527
915.557066	39.131733	70.124532
914.704190	43.043396	70.129537
914.128882	36.528859	70.134542
912.823726	43.930699	70.139546
912.014122	39.449210	70.144551
911.918814	38.335859	70.149556
911.167657	41.094109	70.154561
910.598689	35.534094	70.159566
910.123937	40.486596	70.164570
909.752586	50.242453	70.169575
908.857510	26.453865	70.174580
907.994151	37.041177	70.179585
907.573717	38.747311	70.184590
906.843347	36.438980	70.189594
905.902411	42.314044	70.194599
905.107698	39.706881	70.199604
905.040842	39.197309	70.204609
904.742330	38.737280	70.209614
903.428637	36.639771	70.214618
902.837920	29.540936	70.219623
902.310356	34.858120	70.224628
901.278125	39.284030	70.229633
900.193806	33.456644	70.234638
899.457976	38.017305	70.239642
898.864616	37.278189	70.244647
898.563640	44.833684	70.249652
898.113835	44.230629	70.254657
897.585036	35.341807	70.259662
897.452094	41.035461	70.264666
896.260576	39.429765	70.269671
895.877005	34.662956	70.274676
894.773900	38.193949	70.279681
894.207005	43.095527	70.284686
893.439787	41.969368	70.289690
892.825963	37.575924	70.294695
892.694401	40.539882	70.299700
891.520508	43.828014	70.304705
890.703725	35.802027	70.309710
889.812890	39.859924	70.314714
888.873593	36.947151	70.319719
888.750676	36.234429	70.324724
888.414533	40.358761	70.329729
888.013088	35.736717	70.334734
887.316829	35.869785	70.339738
886.154706	41.819444	70.344743
885.809908	36.770089	70.349748
884.960575	41.081786	70.354753
884.009397	34.238101	70.359758
883.184119	38.573307	70.364762
882.420332	43.265069	70.369767
882.496286	43.205091	70.374772
881.751071	51.230208	70.379777
881.155419	34.816922	70.384782
880.062161	36.119639	70.389786
879.190389	38.818029	70.394791
878.974923	40.237230	70.399796
878.374783	45.688027	70.404801
877.983641	42.070349	70.409806
876.790220	40.886541	70.414810
875.712717	43.951336	70.419815
875.593921	37.491635	70.424820
874.939756	46.429132	70.429825
874.623536	46.560659	70.434830
874.149813	37.140988	70.439834
873.587416	44.820596	70.444839
872.957827	31.020228	70.449844
871.271382	39.649029	70.454849
870.600406	35.936395	70.459854
870.353121	42.448143	70.464858
869.232941	46.979119	70.469863
869.042026	33.993304	70.474868
868.728889	45.241473	70.479873
868.270218	34.768493	70.484878
866.996210	38.453099	70.489882
866.556293	45.119414	70.494887
866.005532	35.365985	70.499892
864.892903	42.016870	70.504897
864.055255	39.556403	70.509902
863.634359	38.819723	70.514906
862.578964	38.765242	70.519911
862.488842	37.397596	70.524916
861.771918	43.161276	70.529921
861.534781	38.498066	70.534926
860.483791	35.972306	70.539930
859.921747	44.309845	70.544935
859.665049	33.237829	70.549940
858.111501	38.815218	70.554945
857.420953	30.712360	70.559950
856.718627	41.426035	70.564954
856.058203	46.591912	70.569959
856.366113	41.891791	70.574964
855.886751	41.893771	70.579969
854.876293	44.152129	70.584974
853.756104	36.209301	70.589978
853.310645	45.608788	70.594983
852.602568	39.872883	70.599988
851.404551	44.059187	70.604993
850.907064	37.505675	70.609998
850.539663	37.195994	70.615002
849.961656	35.326157	70.620007
849.363830	31.623103	70.625012
848.496954	33.646484	70.630017
847.854479	35.481833	70.635022
847.198389	39.843720	70.640026
846.794794	39.990610	70.645031
846.084908	35.103261	70.650036
844.976099	40.498299	70.655041
844.285239	40.911881	70.660046
843.766482	37.891167	70.665050
843.356195	47.141743	70.670055
842.965271	34.620430	70.675060
842.463462	41.008413	70.680065
841.550498	37.680241	70.685070
840.835384	41.550556	70.690074
839.836698	44.687511	70.695079
838.916057	36.516704	70.700084
837.872534	39.131235	70.705089
837.658780	49.297045	70.710094
837.469953	43.500227	70.715098
836.819652	46.148059	70.720103
836.918419	36.196150	70.725108
835.887372	41.409326	70.730113
834.692555	36.169275	70.735118
834.013842	40.606482	70.740122
833.045597	41.044289	70.745127
832.193254	36.536589	70.750132
831.453972	39.588062	70.755137
830.978395	39.749650	70.760142
830.503479	36.095805	70.765146
829.968322	39.076790	70.770151
829.799023	40.232309	70.775156
829.274587	48.614327	70.780161
828.398319	38.304061	70.785166
827.804421	47.746736	70.790170
827.143995	39.963967	70.795175
826.090980	36.146658	70.800180
824.858865	55.657727	70.805185
823.961173	50.244024	70.810190
824.279872	44.480662	70.815194
823.383642	42.809406	70.820199
823.110081	49.806815	70.825204
822.323866	49.043508	70.830209
821.776612	43.276903	70.835214
821.086114	35.875452	70.840218
820.004208	35.982224	70.845223
820.183391	36.759911	70.850228
818.543989	50.007133	70.855233
818.153698	43.528811	70.860238
817.784446	39.366236	70.865242
816.847507	42.144479	70.870247
816.143928	32.065548	70.875252
815.161021	43.281998	70.880257
814.633182	46.104634	70.885262
814.257476	42.158285	70.890266
813.871610	40.494738	70.895271
813.157823	37.372442	70.900276
811.907481	42.478325	70.905281
811.374354	45.041750	70.910286
811.147638	46.816940	70.915290
810.654007	47.464361	70.920295
809.960044	34.841024	70.925300
808.540909	45.614331	70.930305
808.424434	36.592535	70.935310
808.056100	41.609703	70.940314
806.543766	35.859606	70.945319
805.733427	37.486489	70.950324
805.318112	42.900894	70.955329
805.009898	38.891673	70.960334
804.752725	38.074457	70.965338
803.814142	43.447054	70.970343
803.088960	39.632012	70.975348
801.888993	41.803637	70.980353
801.690359	43.201800	70.985358
801.417499	40.176469	70.990362
800.453860	41.306220	70.995367
799.898921	40.367519	71.000372
799.040762	36.946684	71.005377
798.554464	36.026223	71.010382
797.886434	33.654342	71.015386
796.460476	48.717800	71.020391
795.692044	35.103066	71.025396
795.223146	40.412971	71.030401
795.161155	44.740201	71.035406
794.619011	38.114616	71.040410
793.913459	45.800592	71.045415
793.345974	41.861439	71.050420
792.705358	44.397096	71.055425
791.902991	45.462120	71.060430
791.717962	36.881124	71.065434
790.655716	41.978079	71.070439
789.859322	39.155712	71.075444
789.481171	42.855029	71.080449
788.490218	35.916346	71.085454
787.508060	40.918271	71.090458
786.971373	45.767316	71.095463
786.710474	38.408725	71.100468
786.093149	36.096840	71.105473
784.978002	42.889871	71.110478
784.282174	39.760952	71.115482
783.464460	45.635846	71.120487
783.436804	34.384485	71.125492
782.531760	43.323909	71.130497
782.044391	37.579816	71.135502
781.007002	35.344624	71.140506
780.288349	46.633044	71.145511
780.255330	36.912124	71.150516
779.324127	35.881176	71.155521
778.195272	41.309262	71.160526
777.368483	37.650571	71.165530
776.793917	41.464055	71.170535
776.653815	33.767424	71.175540
776.030783	45.464572	71.180545
775.420072	47.102262	71.185550
775.177280	43.220776	71.190554
773.978569	47.634966	71.195559
773.356254	44.826595	71.200564
772.898144	45.299785	71.205569
771.837033	43.296803	71.210574
770.945929	39.326648	71.215578
770.194190	46.835416	71.220583
770.015033	39.608079	71.225588
769.634201	45.984027	71.230593
769.037954	37.965290	71.235598
768.143352	42.373568	71.240602
767.346775	46.898864	71.245607
766.770420	42.049442	71.250612
766.349978	39.042291	71.255617
765.010923	44.097462	71.260622
764.679819	41.982063	71.265626
763.907668	43.058493	71.270631
763.563476	30.775894	71.275636
762.489563	40.775240	71.280641
761.399278	38.028879	71.285646
761.097152	46.144275	71.290650
760.325215	44.186887	71.295655
760.565478	41.923088	71.300660
759.842860	37.547515	71.305665
759.129438	35.406825	71.310670
758.355578	38.065172	71.315674
757.483410	43.145756	71.320679
756.981196	43.671500	71.325684
755.881460	44.198554	71.330689
754.891258	40.266297	71.335694
754.780574	48.501655	71.340698
754.244874	45.490960	71.345703
753.773785	45.517189	71.350708
753.078137	46.965364	71.355713
751.954773	43.116309	71.360718
751.107236	37.463524	71.365722
750.440666	45.212294	71.370727
750.458843	50.738751	71.375732
749.961922	39.818027	71.380737
748.651918	42.702423	71.385742
748.047040	39.825547	71.390746
747.283179	38.986190	71.395751
747.336491	39.449533	71.400756
746.299426	47.002839	71.405761
745.242948	33.635613	71.410766
744.693343	39.431424	71.415770
744.007222	39.848156	71.420775
744.191284	31.188154	71.425780
743.127272	46.866945	71.430785
741.961335	40.870830	71.435790
741.998261	34.957988	71.440794
740.869699	43.674403	71.445799
740.200475	30.010330	71.450804
739.327363	40.595378	71.455809
738.780754	35.366282	71.460814
738.663152	38.417447	71.465818
737.321811	43.311973	71.470823
736.847832	29.209082	71.475828
735.650371	40.241645	71.480833
735.286643	38.423927	71.485838
735.133698	30.776868	71.490842
734.554200	33.744140	71.495847
734.095638	35.537339	71.500852
732.924682	39.166428	71.505857
732.120540	35.368085	71.510862
731.823673	37.277261	71.515866
731.089410	38.740342	71.520871
730.637497	28.218871	71.525876
729.408649	39.828753	71.530881
728.521748	30.938555	71.535886
728.395839	31.228532	71.540890
727.795075	36.456429	71.545895
727.343244	35.635461	71.550900
726.375504	41.492641	71.555905
725.700574	40.498325	71.560910
725.246954	36.284297	71.565914
724.482403	43.634613	71.570919
723.922242	38.985309	71.575924
722.880006	42.116324	71.580929
721.970556	40.502614	71.585934
721.928173	35.743297	71.590938
721.595605	42.800937	71.595943
720.435273	31.824936	71.600948
719.435424	42.968905	71.605953
719.107302	35.739071	71.610958
718.773140	42.808431	71.615962
718.008351	45.576541	71.620967
717.360220	30.961543	71.625972
716.612223	40.861644	71.630977
715.849079	34.316169	71.635982
714.534936	33.880939	71.640986
713.801967	38.638092	71.645991
713.760890	33.912102	71.650996
713.387627	35.674506	71.656001
712.626300	42.639423	71.661006
712.380620	33.696613	71.666010
711.082017	42.560182	71.671015
710.103630	34.209841	71.676020
709.945007	39.059644	71.681025
709.290513	38.553644	71.686030
708.865949	40.309839	71.691034
707.296907	39.426462	71.696039
707.215963	39.550456	71.701044
706.249392	42.194458	71.706049
705.808915	44.112055	71.711054
705.678550	33.971661	71.716058
704.942215	32.144757	71.721063
703.959666	36.343120	71.726068
703.024721	40.703058	71.731073
702.686173	39.105227	71.736078
702.302556	37.456305	71.741082
700.801231	38.338337	71.746087
700.372549	37.439989	71.751092
699.709104	41.946037	71.756097
699.432932	37.986993	71.761102
699.238306	38.467548	71.766106
698.094300	41.809412	71.771111
697.246508	29.296540	71.776116
696.729350	41.305528	71.781121
696.306055	32.340652	71.786126
695.198559	30.078021	71.791130
693.677747	48.034817	71.796135
693.507504	35.942679	71.801140
693.162017	41.349466	71.806145
692.499343	37.412033	71.811150
692.641102	36.170448	71.816154
691.761289	35.632792	71.821159
691.399538	31.358430	71.826164
690.365322	39.911064	71.831169
689.188912	45.726240	71.836174
688.787961	40.558246	71.841178
687.980218	42.198123	71.846183
687.777962	44.209902	71.851188
687.205248	41.954727	71.856193
686.051608	39.833020	71.861198
684.970736	34.388374	71.866202
684.222617	46.204446	71.871207
684.119471	31.426623	71.876212
683.760599	41.384397	71.881217
683.153140	35.760758	71.886222
681.898677	36.109084	71.891226
681.369537	36.917328	71.896231
680.693405	38.806617	71.901236
680.020443	40.076055	71.906241
679.713574	36.933412	71.911246
679.041110	34.640068	71.916250
678.070347	37.516885	71.921255
677.630902	40.227289	71.926260
676.688856	40.281712	71.931265
676.434049	34.312280	71.936270
675.760803	38.046761	71.941274
674.414716	34.450612	71.946279
674.388616	30.279398	71.951284
673.686012	33.490385	71.956289
672.871811	26.048195	71.961294
672.149176	22.400500	71.966298
671.289884	36.020116	71.971303
670.883417	31.875778	71.976308
670.328619	31.898989	71.981313
669.132173	31.055998	71.986318
668.818218	35.381389	71.991322
667.434243	38.306106	71.996327
667.550016	32.035965	72.001332
667.408552	35.300416	72.006337
666.725298	42.835744	72.011342
666.200769	30.294339	72.016346
664.874237	47.096864	72.021351
664.289980	37.926685	72.026356
663.361697	36.125567	72.031361
662.830269	37.669954	72.036366
662.037469	39.354640	72.041370
661.439518	40.738722	72.046375
661.132345	37.702705	72.051380
660.888448	39.914239	72.056385
659.617761	34.296473	72.061390
658.998937	27.691159	72.066394
658.056082	31.371573	72.071399
657.828948	42.835113	72.076404
657.313372	37.830438	72.081409
656.253031	35.222256	72.086414
655.604747	35.012025	72.091418
654.806329	39.308318	72.096423
654.623202	30.962268	72.101428
654.136646	46.061763	72.106433
653.121956	40.305407	72.111438
652.477925	30.613006	72.116442
651.643643	37.266758	72.121447
651.174505	34.106921	72.126452
650.252192	31.079589	72.131457
649.402064	35.234355	72.136462
649.223387	33.817549	72.141466
648.369186	43.508494	72.146471
647.809295	34.073240	72.151476
647.302847	43.895649	72.156481
646.092030	39.501507	72.161486
645.494144	27.767633	72.166490
644.949100	41.985879	72.171495
645.057613	36.487464	72.176500
644.209552	33.528329	72.181505
643.148305	32.413906	72.186510
642.463839	24.968049	72.191514
642.005279	34.991841	72.196519
641.586594	25.511482	72.201524
640.189848	30.265920	72.206529
639.161021	36.406719	72.211534
638.852797	33.977167	72.216538
638.350739	32.042245	72.221543
638.292191	34.607265	72.226548
637.933785	39.736808	72.231553
637.067778	35.490031	72.236558
636.121446	31.354117	72.241562
634.893417	41.178973	72.246567
634.130429	39.032585	72.251572
633.470169	42.944047	72.256577
632.597576	44.610042	72.261582
632.913191	37.862002	72.266586
632.336320	38.236743	72.271591
631.866581	36.385490	72.276596
630.647740	43.746544	72.281601
629.784301	38.475832	72.286606
629.671845	39.222165	72.291610
628.792921	38.453460	72.296615
627.622168	32.055601	72.301620
626.906135	35.722421	72.306625
626.054928	45.940590	72.311630
626.073587	34.641054	72.316634
625.450124	44.323257	72.321639
625.224009	33.169074	72.326644
623.943860	32.391748	72.331649
623.151199	41.923737	72.336654
622.925022	39.062915	72.341658
622.088882	45.287148	72.346663
621.071078	43.000087	72.351668
620.653467	39.201855	72.356673
619.785693	37.519056	72.361678
619.534768	40.338866	72.366682
619.192912	45.040863	72.371687
618.237001	35.874769	72.376692
617.244934	40.594223	72.381697
616.310995	42.352042	72.386702
616.355569	36.627359	72.391706
615.372816	52.966413	72.396711
614.391600	37.893009	72.401716
614.342918	43.603400	72.406721
613.376451	44.523682	72.411726
613.240504	37.243570	72.416730
612.429626	39.653293	72.421735
611.346980	34.364884	72.426740
610.779610	45.200701	72.431745
609.890039	37.643942	72.436750
609.892062	37.566233	72.441754
608.462634	40.706768	72.446759
608.069769	47.833159	72.451764
607.387621	46.885488	72.456769
606.482320	41.652741	72.461774
606.238685	43.661349	72.466778
606.025974	39.957478	72.471783
604.818496	38.326569	72.476788
604.475830	41.083155	72.481793
603.508654	38.258508	72.486798
603.046495	37.494978	72.491802
601.350508	38.725374	72.496807
601.094107	37.829096	72.501812
600.489168	39.907501	72.506817
600.034684	34.918420	72.511822
599.625891	35.271078	72.516826
599.154416	34.174031	72.521831
598.624332	34.054866	72.526836
597.648209	35.352573	72.531841
596.861257	46.535469	72.536846
596.723973	32.623199	72.541850
595.736953	39.680080	72.546855
594.976826	38.114624	72.551860
594.302481	40.045062	72.556865
593.612395	47.748926	72.561870
593.207821	35.142380	72.566874
591.847318	49.277334	72.571879
591.369318	41.224164	72.576884
590.675101	41.385739	72.581889
590.385148	39.523817	72.586894
590.343875	36.988929	72.591898
588.992734	38.017358	72.596903
588.483204	38.939877	72.601908
587.582678	33.850390	72.606913
587.192987	36.480040	72.611918
586.613499	36.705243	72.616922
585.706408	39.488278	72.621927
585.539661	35.760746	72.626932
584.773060	37.965135	72.631937
583.345717	45.243508	72.636942
583.042254	33.578403	72.641946
582.168557	37.855631	72.646951
581.857803	36.037140	72.651956
581.062603	32.986466	72.656961
580.181353	34.340548	72.661966
579.691479	28.740203	72.666970
579.082075	36.328798	72.671975
578.697402	29.133544	72.676980
578.296913	30.958248	72.681985
576.646772	42.946239	72.686990
576.504319	36.730607	72.691994
575.667495	37.812620	72.696999
575.319750	38.628871	72.702004
573.984386	47.098524	72.707009
572.987401	36.666921	72.712014
573.167877	38.643913	72.717018
572.171902	45.969950	72.722023
571.832563	43.380743	72.727028
570.996896	42.422279	72.732033
570.754729	44.931134	72.737038
570.537225	37.067008	72.742042
569.229180	42.439391	72.747047
568.246270	45.268971	72.752052
568.111509	33.996913	72.757057
566.813384	42.523339	72.762062
566.026542	42.660132	72.767066
565.335843	45.112821	72.772071
564.959227	38.930206	72.777076
564.673763	43.586227	72.782081
564.199220	40.530346	72.787086
563.964900	31.003805	72.792090
562.497901	42.868056	72.797095
562.041243	35.056356	72.802100
561.563618	40.536703	72.807105
560.505540	33.925753	72.812110
559.875517	31.560425	72.817114
558.825428	39.050066	72.822119
558.857363	34.539720	72.827124
558.167623	33.172989	72.832129
557.484230	37.615759	72.837134
556.970171	30.034543	72.842138
555.954343	38.336950	72.847143
555.367770	34.912658	72.852148
554.927395	40.054274	72.857153
553.469149	36.840518	72.862158
552.877199	27.277369	72.867162
552.342259	35.608293	72.872167
551.731051	33.539725	72.877172
551.535166	34.567970	72.882177
550.926723	40.845162	72.887182
549.972683	29.970054	72.892186
548.999043	33.053426	72.897191
548.752318	28.215457	72.902196
548.267689	28.457173	72.907201
547.544662	24.889301	72.912206
546.454143	26.430026	72.917210
545.708591	32.423621	72.922215
545.495442	26.362996	72.927220
544.999589	30.610614	72.932225
544.635681	33.034939	72.937230
543.619717	29.761589	72.942234
542.668754	36.615334	72.947239
542.168995	36.832802	72.952244
541.650079	36.678179	72.957249
540.711541	35.645380	72.962254
539.993346	29.141585	72.967258
539.055926	43.296804	72.972263
538.309477	33.345283	72.977268
538.650886	36.102677	72.982273
537.753045	39.298978	72.987278
537.016678	29.181926	72.992282
536.006511	35.827145	72.997287
535.693736	33.579161	73.002292
534.900831	40.702651	73.007297
533.595312	34.293572	73.012302
533.451814	32.927979	73.017306
532.583724	43.778614	73.022311
532.497202	41.068727	73.027316
532.114012	42.224194	73.032321
530.801981	48.122241	73.037326
530.161013	41.137079	73.042330
529.240010	39.653277	73.047335
528.913831	36.848674	73.052340
528.581726	27.923073	73.057345
527.265038	46.378959	73.062350
526.848461	37.414934	73.067354
525.934440	43.210441	73.072359
525.627457	35.426387	73.077364
525.327760	38.290081	73.082369
524.496537	29.646570	73.087374
523.793746	36.368983	73.092378
522.796297	32.372505	73.097383
522.372999	33.287359	73.102388
521.078384	38.771128	73.107393
520.335259	36.588597	73.112398
520.435165	35.585484	73.117402
519.579493	41.370992	73.122407
519.457387	39.415583	73.127412
518.901646	34.117436	73.132417
517.531890	43.134538	73.137422
516.950440	35.676974	73.142426
516.321782	41.438977	73.147431
515.662512	43.630906	73.152436
515.006396	38.799143	73.157441
513.900057	39.555923	73.162446
513.532938	38.749670	73.167450
512.804261	40.746267	73.172455
512.185999	39.614385	73.177460
512.248742	30.499160	73.182465
511.361637	45.902925	73.187470
510.634398	38.025893	73.192474
509.802865	35.418802	73.197479
509.120563	34.797207	73.202484
508.059843	36.200607	73.207489
507.546849	46.500558	73.212494
507.181988	41.169309	73.217498
506.596674	45.158726	73.222503
506.013388	44.553716	73.227508
505.049584	38.080170	73.232513
504.201488	44.707888	73.237518
503.809437	30.148148	73.242522
503.193104	38.348556	73.247527
502.744319	36.029150	73.252532
501.586030	42.694626	73.257537
500.746092	38.592220	73.262542
500.175977	36.048486	73.267546
499.964465	32.089436	73.272551
499.506036	39.416126	73.277556
498.750355	35.678209	73.282561
497.411775	38.489803	73.287566
497.409987	32.861883	73.292570
496.741002	34.783125	73.297575
495.876211	35.928756	73.302580
494.774267	37.756434	73.307585
494.478784	47.322839	73.312590
493.971434	34.032915	73.317594
493.827495	40.772063	73.322599
492.568889	32.165481	73.327604
491.622228	32.915428	73.332609
490.782830	30.958598	73.337614
490.756330	30.651712	73.342618
490.004242	31.162672	73.347623
489.340146	24.754614	73.352628
488.663831	29.636676	73.357633
487.702810	34.508714	73.362638
487.462595	31.985027	73.367642
486.885301	42.150739	73.372647
485.972218	35.915994	73.377652
485.546818	30.994181	73.382657
484.344377	32.294377	73.387662
484.436104	27.271321	73.392666
483.039434	35.071792	73.397671
482.455337	38.222629	73.402676
482.160084	36.871990	73.407681
481.691107	35.999120	73.412686
481.156670	34.738017	73.417690
479.533001	37.376639	73.422695
478.779268	37.883146	73.427700
478.577804	30.463498	73.432705
478.139598	35.497776	73.437710
477.704939	38.852333	73.442714
476.464311	39.956982	73.447719
475.613119	31.409664	73.452724
475.400651	39.382982	73.457729
474.639230	35.344492	73.462734
474.788905	29.234331	73.467738
473.716885	37.151663	73.472743
472.747088	33.764240	73.477748
472.462340	31.296735	73.482753
471.447153	38.719621	73.487758
470.506426	39.804063	73.492762
469.841433	36.954900	73.497767
469.141477	31.842125	73.502772
469.030899	37.203528	73.507777
468.376339	33.008578	73.512782
467.431476	37.334329	73.517786
466.332991	32.905996	73.522791
466.189731	37.204509	73.527796
465.984467	36.046070	73.532801
465.187712	30.204269	73.537806
464.167997	27.048417	73.542810
463.489878	40.751463	73.547815
462.758160	39.318522	73.552820
462.423451	30.677966	73.557825
461.062258	36.696151	73.562830
460.503753	32.976556	73.567834
459.764874	31.654180	73.572839
459.467249	32.029243	73.577844
458.722778	24.734229	73.582849
458.110276	32.345461	73.587854
457.937387	25.664957	73.592858
456.525555	32.188369	73.597863
456.377470	33.050146	73.602868
455.711717	33.360801	73.607873
455.199747	35.754059	73.612878
454.583788	33.365812	73.617882
453.219113	35.920983	73.622887
452.767469	34.754637	73.627892
452.233136	31.703888	73.632897
451.736906	39.969370	73.637902
451.138002	31.187784	73.642906
449.910872	32.518271	73.647911
449.211900	29.406530	73.652916
449.100886	32.397356	73.657921
448.179637	34.818911	73.662926
448.118887	26.362714	73.667930
447.099189	27.505690	73.672935
446.362616	30.643185	73.677940
445.756624	27.972591	73.682945
445.007196	32.612202	73.687950
443.910011	29.157412	73.692954
443.434079	33.998825	73.697959
443.178716	29.791915	73.702964
442.716314	28.426900	73.707969
442.202520	41.667997	73.712974
441.027974	33.586601	73.717978
440.333175	37.370981	73.722983
439.729903	29.167613	73.727988
439.283118	29.201945	73.732993
437.871643	36.212378	73.737998
437.353545	28.219402	73.743002
436.518490	33.241561	73.748007
435.997058	31.591416	73.753012
435.580569	31.816334	73.758017
435.194559	40.613555	73.763022
435.044545	26.765472	73.768026
433.819234	36.426477	73.773031
432.915217	37.266228	73.778036
432.278027	26.544480	73.783041
431.753304	35.197321	73.788046
431.781788	30.586527	73.793050
430.617050	36.809855	73.798055
430.098539	35.416958	73.803060
429.797903	29.351602	73.808065
428.208255	38.797562	73.813070
427.902509	33.737232	73.818074
426.964074	37.641124	73.823079
426.518649	39.356705	73.828084
426.132379	32.523700	73.833089
425.027832	42.167567	73.838094
424.421280	30.022363	73.843098
423.760481	31.358428	73.848103
423.266837	25.390489	73.853108
422.824155	25.052694	73.858113
421.116140	32.522081	73.863118
420.815298	24.705419	73.868122
420.197140	28.401669	73.873127
419.937043	33.987234	73.878132
419.358581	29.237705	73.883137
419.057206	24.640024	73.888142
418.444126	23.220707	73.893146
417.480496	30.218338	73.898151
416.734803	42.384504	73.903156
415.551301	33.040384	73.908161
414.525963	30.812689	73.913166
414.599001	24.352924	73.918170
414.051739	30.633451	73.923175
413.592496	25.883229	73.928180
413.084192	33.341221	73.933185
411.721652	37.964731	73.938190
411.002218	32.214685	73.943194
410.820292	30.470048	73.948199
410.073710	36.480806	73.953204
409.742013	33.703607	73.958209
408.590740	39.330983	73.963214
408.112927	24.050223	73.968218
407.483867	35.663928	73.973223
406.909403	31.499866	73.978228
406.050128	29.130432	73.983233
405.095972	31.668548	73.988238
404.924272	35.789576	73.993242
404.279086	33.165176	73.998247
403.316067	35.982295	74.003252
402.133453	27.517453	74.008257
401.159521	32.118574	74.013262
401.440569	29.290444	74.018266
401.373163	31.426740	74.023271
400.966946	30.821397	74.028276
399.602818	24.669108	74.033281
398.547356	31.787869	74.038286
398.127450	23.521512	74.043290
397.485742	31.717980	74.048295
396.250771	26.072869	74.053300
395.838060	22.803930	74.058305
394.911190	29.670929	74.063310
394.513276	17.309208	74.068314
394.132057	26.526758	74.073319
393.537090	29.579206	74.078324
393.445311	24.826404	74.083329
392.430075	31.567636	74.088334
391.942615	27.280515	74.093338
390.885248	30.934020	74.098343
390.022604	29.453666	74.103348
389.411897	27.160051	74.108353
388.314208	22.587930	74.113358
388.374955	29.599866	74.118362
387.548759	31.822784	74.123367
387.166088	24.321711	74.128372
386.265538	26.691574	74.133377
385.163116	36.062726	74.138382
384.658137	26.889293	74.143386
384.192220	26.269317	74.148391
383.642080	29.026337	74.153396
383.176504	30.942730	74.158401
382.184769	34.749585	74.163406
381.719697	26.438472	74.168410
381.310036	32.404121	74.173415
379.920435	27.522050	74.178420
379.655369	23.230764	74.183425
379.000898	34.976316	74.188430
378.969018	32.574029	74.193434
377.938361	36.162568	74.198439
376.713726	42.993769	74.203444
376.547635	21.322075	74.208449
375.775067	25.034529	74.213454
375.406731	23.781683	74.218458
374.195207	38.058481	74.223463
373.292984	30.705656	74.228468
373.031076	26.940771	74.233473
372.285169	30.566162	74.238478
371.811257	28.467382	74.243482
370.623010	28.058432	74.248487
369.901771	34.929667	74.253492
369.446302	32.340649	74.258497
368.981244	28.875827	74.263502
368.719131	23.504890	74.268506
368.256056	28.915646	74.273511
366.843127	26.312706	74.278516
366.624339	23.673654	74.283521
365.810547	29.246748	74.288526
365.480103	25.661363	74.293530
365.015669	30.094648	74.298535
363.904560	31.483425	74.303540
363.185830	26.729922	74.308545
361.957198	31.427197	74.313550
361.768798	31.543956	74.318554
361.075440	29.768164	74.323559
360.492918	36.761670	74.328564
360.272635	29.820103	74.333569
358.904042	29.471274	74.338574
358.638825	30.271026	74.343578
357.922285	29.614668	74.348583
357.236658	27.543885	74.353588
356.502614	26.456737	74.358593
355.156165	35.609995	74.363598
354.846093	26.385007	74.368602
354.285022	37.819703	74.373607
354.036311	34.162681	74.378612
353.705554	24.827562	74.383617
352.701609	26.844910	74.388622
351.722099	29.720913	74.393626
351.071329	31.682469	74.398631
350.594340	38.023190	74.403636
350.254096	34.406723	74.408641
348.994356	27.960261	74.413646
348.264824	35.816150	74.418650
347.736783	36.874882	74.423655
347.299666	34.490341	74.428660
346.964418	33.424446	74.433665
345.540949	38.387605	74.438670
345.082553	28.935421	74.443674
344.375955	34.803945	74.448679
343.985643	36.939534	74.453684
343.826064	24.068841	74.458689
342.843543	33.186962	74.463694
342.079021	27.981076	74.468698
341.201963	32.818614	74.473703
340.855113	33.300800	74.478708
340.062727	28.284415	74.483713
338.881312	36.464053	74.488718
338.326480	32.103228	74.493722
337.790813	32.727505	74.498727
337.208687	36.669022	74.503732
336.840985	34.417444	74.508737
336.216846	31.256191	74.513742
335.312170	27.275834	74.518746
334.617686	42.448834	74.523751
333.858737	41.531343	74.528756
333.931683	34.200066	74.533761
332.485826	41.151291	74.538766
332.154893	28.615472	74.543770
331.431016	32.500761	74.548775
331.197843	31.186860	74.553780
330.436375	31.058833	74.558785
329.215138	33.724443	74.563790
329.005910	29.830145	74.568794
328.277929	37.867338	74.573799
326.683194	37.959490	74.578804
326.159971	33.099068	74.583809
325.765815	41.441000	74.588814
325.579684	33.204843	74.593818
325.128130	37.215950	74.598823
324.890436	38.590821	74.603828
324.171595	27.511670	74.608833
322.873016	39.602870	74.613838
322.114602	32.656438	74.618842
321.245148	39.120870	74.623847
320.088911	30.202745	74.628852
319.787462	33.039509	74.633857
319.228999	45.825656	74.638862
318.919842	35.953971	74.643866
318.751650	33.923186	74.648871
317.872890	39.269017	74.653876
316.891356	32.831326	74.658881
316.376913	41.349392	74.663886
315.700105	36.911981	74.668890
314.777971	29.862173	74.673895
313.237738	36.126985	74.678900
313.165449	29.507406	74.683905
312.558042	39.789589	74.688910
312.133409	36.754398	74.693914
311.644928	30.824667	74.698919
310.925785	37.292940	74.703924
310.564721	25.709210	74.708929
309.704895	29.384132	74.713934
309.173690	28.193546	74.718938
308.565426	37.227397	74.723943
308.185386	40.925476	74.728948
307.217125	29.702773	74.733953
306.069159	31.979274	74.738958
305.956145	34.283640	74.743962
304.979384	24.085890	74.748967
303.997311	32.373462	74.753972
303.109670	30.270606	74.758977
302.833815	40.898965	74.763982
302.532423	32.303247	74.768986
302.201420	33.919098	74.773991
300.950062	35.834792	74.778996
300.053573	28.391011	74.784001
299.278780	37.748650	74.789006
298.979019	38.403941	74.794010
298.569599	29.855160	74.799015
297.734916	35.471711	74.804020
297.425914	35.371526	74.809025
295.991520	43.219162	74.814030
295.568604	38.767052	74.819034
295.251577	33.665648	74.824039
294.577113	35.107882	74.829044
293.499121	23.413762	74.834049
292.825778	31.507901	74.839054
292.331633	31.675883	74.844058
291.605004	29.873833	74.849063
291.633728	38.345376	74.854068
290.873258	33.437602	74.859073
289.728585	45.004699	74.864078
289.278340	36.583300	74.869082
288.641548	34.401533	74.874087
286.815781	38.577922	74.879092
286.620526	38.295225	74.884097
285.776208	42.233137	74.889102
285.578307	34.571731	74.894106
285.233385	27.808237	74.899111
284.424316	31.768525	74.904116
284.710315	32.385782	74.909121
283.515380	30.173373	74.914126
282.868354	27.327481	74.919130
282.248060	34.192866	74.924135
281.435353	31.174462	74.929140
280.319809	20.515013	74.934145
279.734654	24.683615	74.939150
279.212278	24.530404	74.944154
278.817768	27.632578	74.949159
277.749279	34.251515	74.954164
276.951603	27.578652	74.959169
276.521929	32.634367	74.964174
276.443615	32.120061	74.969178
275.532430	30.933033	74.974183
274.282345	37.786375	74.979188
273.739942	30.626099	74.984193
273.232815	36.910808	74.989198
272.644941	34.326734	74.994202
272.463201	37.011148	74.999207
271.127056	37.624619	75.004212
270.923987	29.799113	75.009217
269.713881	34.514942	75.014222
269.300680	31.159659	75.019226
268.773229	42.272036	75.024231
267.473093	38.094228	75.029236
267.195996	27.429215	75.034241
266.570670	38.794009	75.039246
266.311317	26.911028	75.044250
265.821572	36.245862	75.049255
264.613834	38.068435	75.054260
264.283642	30.224458	75.059265
263.391442	34.212812	75.064270
262.446911	33.449109	75.069274
261.784155	40.599655	75.074279
260.780964	36.820136	75.079284
260.502644	37.648191	75.084289
259.883664	31.896748	75.089294
259.987299	34.481723	75.094298
259.602332	32.332581	75.099303
257.864054	36.255183	75.104308
257.339603	33.891148	75.109313
256.983400	41.739499	75.114318
255.865655	34.975850	75.119322
255.299699	36.322521	75.124327
254.554028	35.377506	75.129332
253.737112	28.505853	75.134337
253.595700	37.801505	75.139342
253.566997	36.876877	75.144346
252.711888	32.384784	75.149351
251.644262	34.891459	75.154356
250.766791	29.492203	75.159361
249.738260	37.097394	75.164366
248.504730	30.211499	75.169370
249.075401	29.735154	75.174375
247.896512	34.697069	75.179380
247.421276	34.474206	75.184385
247.269190	41.344600	75.189390
246.370392	32.527626	75.194394
245.668219	37.585845	75.199399
244.731086	37.625303	75.204404
244.233305	29.234958	75.209409
243.604276	33.021899	75.214414
243.015350	34.269489	75.219418
242.172214	31.924163	75.224423
241.266076	35.711633	75.229428
240.937895	32.906220	75.234433
240.450365	36.104074	75.239438
239.830740	28.711530	75.244442
238.780970	40.528399	75.249447
238.000314	36.083936	75.254452
238.099320	32.833874	75.259457
237.069630	31.081019	75.264462
236.097527	34.460612	75.269466
235.386333	36.890801	75.274471
234.655776	44.448079	75.279476
234.463384	31.736567	75.284481
233.940979	40.172319	75.289486
233.193142	44.090543	75.294490
232.332102	35.426958	75.299495
231.185033	49.918509	75.304500
231.276887	34.405542	75.309505
230.930984	36.991392	75.314510
229.365563	38.918309	75.319514
228.551260	32.436979	75.324519
227.954957	31.789634	75.329524
228.000014	32.973550	75.334529
227.417394	43.349377	75.339534
226.433394	30.677248	75.344538
225.961596	36.239893	75.349543
224.994882	38.604548	75.354548
225.182652	32.993097	75.359553
223.597405	41.142510	75.364558
222.692249	36.692157	75.369562
222.380502	30.849377	75.374567
221.695894	36.862160	75.379572
221.377546	32.204649	75.384577
220.250386	35.241767	75.389582
219.900541	35.014781	75.394586
219.117934	33.976241	75.399591
218.564088	36.077899	75.404596
217.844537	30.752627	75.409601
216.463075	39.246034	75.414606
216.022643	40.139772	75.419610
215.708516	33.752696	75.424615
215.095835	39.223841	75.429620
214.610422	31.466080	75.434625
214.474872	36.575585	75.439630
213.062236	32.049604	75.444634
212.970765	27.460567	75.449639
212.110489	35.912394	75.454644
211.235599	35.563844	75.459649
210.047602	41.402802	75.464654
209.516077	34.583284	75.469658
208.907074	39.805919	75.474663
208.450498	43.703428	75.479668
208.635398	23.972411	75.484673
207.450324	35.671954	75.489678
206.547562	32.050883	75.494682
206.305048	35.040959	75.499687
205.130706	31.786553	75.504692
204.345731	19.525167	75.509697
203.709085	33.948156	75.514702
203.470603	39.814209	75.519706
202.834378	29.552983	75.524711
201.888191	34.360946	75.529716
201.078544	36.575530	75.534721
200.398683	41.774789	75.539726
199.505853	34.224623	75.544730
199.608088	26.208643	75.549735
199.142540	35.078304	75.554740
197.897809	33.524547	75.559745
196.729800	29.097551	75.564750
196.299101	38.889998	75.569754
196.080080	31.158019	75.574759
195.400912	36.299531	75.579764
194.906165	29.460687	75.584769
194.111491	37.896139	75.589774
193.053754	31.414708	75.594778
192.961405	25.125796	75.599783
192.127922	44.919051	75.604788
191.589884	35.545280	75.609793
190.586717	32.342846	75.614798
189.736802	30.873376	75.619802
189.550974	32.986947	75.624807
188.689522	45.478472	75.629812
188.233717	26.962876	75.634817
187.492132	35.974192	75.639822
186.748990	38.851942	75.644826
186.365582	31.540093	75.649831
185.319158	45.025636	75.654836
184.730401	35.892652	75.659841
183.915490	38.667449	75.664846
183.223734	30.727579	75.669850
183.207093	27.899161	75.674855
182.024071	34.505380	75.679860
181.109903	31.852526	75.684865
180.314788	31.434257	75.689870
180.001313	40.992282	75.694874
179.554578	34.260859	75.699879
178.924300	43.178893	75.704884
178.843044	35.485268	75.709889
177.713784	33.625950	75.714894
176.903661	37.693006	75.719898
176.471931	30.682714	75.724903
175.603917	34.617596	75.729908
174.819814	27.331022	75.734913
173.956280	26.253471	75.739918
173.669969	34.109967	75.744922
173.215986	36.461337	75.749927
172.035686	39.526126	75.754932
171.678033	28.672057	75.759937
170.914929	38.170981	75.764942
170.654650	31.439964	75.769946
169.494698	33.039645	75.774951
168.611072	37.755974	75.779956
168.175314	35.599759	75.784961
167.758001	40.284700	75.789966
166.943987	36.369361	75.794970
165.561535	34.469376	75.799975
164.986590	40.742823	75.804980
164.960717	29.780960	75.809985
164.349380	43.585841	75.814990
164.002076	34.708690	75.819994
163.526762	36.234821	75.824999
162.241213	36.316260	75.830004
161.885392	35.541258	75.835009
161.291177	40.411647	75.840014
160.544484	35.213004	75.845018
159.588399	36.932072	75.850023
158.506622	43.788954	75.855028
158.639888	34.248798	75.860033
158.020245	29.252181	75.865038
157.102479	38.334752	75.870042
156.222483	32.357697	75.875047
155.277965	36.783694	75.880052
154.952674	32.251322	75.885057
154.950229	37.573652	75.890062
153.930599	32.064981	75.895066
153.400332	28.890824	75.900071
152.513480	31.727691	75.905076
151.976676	27.563532	75.910081
150.945903	33.675528	75.915086
149.962337	31.908866	75.920090
149.639179	26.564207	75.925095
148.870845	31.630617	75.930100
148.683692	39.343413	75.935105
147.958104	39.278340	75.940110
146.603749	33.024602	75.945114
146.141334	34.313669	75.950119
145.445054	40.830929	75.955124
144.933049	29.582166	75.960129
144.413072	35.543050	75.965134
144.121677	42.198915	75.970138
143.568379	27.641252	75.975143
142.312908	38.956977	75.980148
141.763673	36.044609	75.985153
141.566054	36.706082	75.990158
140.731870	39.656284	75.995162
139.664079	30.308611	76.000167
138.945241	37.385098	76.005172
138.481437	33.756287	76.010177
138.074307	36.424475	76.015182
136.944024	40.362881	76.020186
136.374727	35.336715	76.025191
135.434872	29.333615	76.030196
135.096061	29.956927	76.035201
134.583378	27.476427	76.040206
134.368855	33.725976	76.045210
133.381635	26.417395	76.050215
132.274821	33.150286	76.055220
131.844048	39.126667	76.060225
131.432712	28.476401	76.065230
131.230634	33.987679	76.070234
130.378924	31.511223	76.075239
129.027097	37.504195	76.080244
128.543480	37.811302	76.085249
128.206582	32.350980	76.090254
126.785814	28.870044	76.095258
126.306253	28.490445	76.100263
125.726252	32.682650	76.105268
125.639475	30.669891	76.110273
125.046580	38.215022	76.115278
124.130682	40.242582	76.120282
123.255430	35.506487	76.125287
122.429045	38.631791	76.130292
122.257752	38.224211	76.135297
121.845049	38.975844	76.140302
120.251793	41.451876	76.145306
119.819857	32.727787	76.150311
119.152965	34.943566	76.155316
119.189641	32.115876	76.160321
118.484528	31.986512	76.165326
117.231653	37.878844	76.170330
116.680235	29.420357	76.175335
116.063946	38.961611	76.180340
115.399721	30.748633	76.185345
114.541867	46.514474	76.190350
113.906048	36.617910	76.195354
113.176601	37.011371	76.200359
112.675886	41.816001	76.205364
112.360859	40.926252	76.210369
111.687594	40.180413	76.215374
110.562220	42.711623	76.220378
110.322513	33.315540	76.225383
109.560762	38.285703	76.230388
108.944790	31.519364	76.235393
107.986910	36.868128	76.240398
107.157913	36.370028	76.245402
106.823767	31.290529	76.250407
106.032048	38.901719	76.255412
105.728181	25.608199	76.260417
105.309300	33.055210	76.265422
104.020947	34.675735	76.270426
103.708645	31.924452	76.275431
102.891404	34.958591	76.280436
102.469268	34.527310	76.285441
101.224780	35.740867	76.290446
100.415611	36.017347	76.295450
99.961639	33.193647	76.300455
99.609697	44.202123	76.305460
99.428451	40.478692	76.310465
98.584146	39.840332	76.315470
97.686843	39.225662	76.320474
97.013714	36.436772	76.325479
96.174482	46.399124	76.330484
95.751156	35.617109	76.335489
94.732297	33.796909	76.340494
93.687783	35.282480	76.345498
93.384974	25.868804	76.350503
92.863739	37.974390	76.355508
92.635396	30.627683	76.360513
92.046373	25.747007	76.365518
90.813183	33.509271	76.370522
90.740207	23.753054	76.375527
89.989079	35.191122	76.380532
88.824506	30.186895	76.385537
87.974400	34.571060	76.390542
87.180043	38.617268	76.395546
87.035110	34.375277	76.400551
86.633680	30.191472	76.405556
85.955026	27.668779	76.410561
84.985500	35.472284	76.415566
84.015589	44.028181	76.420570
83.411717	34.450209	76.425575
83.052446	45.876757	76.430580
82.981899	33.246218	76.435585
81.991663	39.767304	76.440590
80.739645	37.709597	76.445594
80.328349	31.993632	76.450599
79.849807	33.469011	76.455604
79.003001	36.123773	76.460609
78.109699	32.644390	76.465614
77.204623	32.912055	76.470618
77.202252	27.064803	76.475623
76.672458	40.676106	76.480628
76.027928	29.289432	76.485633
75.352854	32.140132	76.490638
74.845530	31.741616	76.495642
74.398101	24.714695	76.500647
73.265095	34.689120	76.505652
72.613898	27.015466	76.510657
71.506336	38.191376	76.515662
71.219828	38.905589	76.520666
70.889339	31.596527	76.525671
69.172515	38.875304	76.530676
68.735150	42.096937	76.535681
68.248807	33.170619	76.540686
67.538697	44.290628	76.545690
67.319385	25.235609	76.550695
66.966404	38.878960	76.555700
66.075864	37.075843	76.560705
65.250578	28.216323	76.565710
64.722176	28.235870	76.570714
64.196600	27.021457	76.575719
63.045067	42.577530	76.580724
62.317158	38.241292	76.585729
61.680649	34.490137	76.590734
61.402548	36.752153	76.595738
61.224440	30.258100	76.600743
59.904871	35.933735	76.605748
59.350779	32.287258	76.610753
58.846413	34.207170	76.615758
57.772347	39.783087	76.620762
56.962539	35.568254	76.625767
56.303088	36.008929	76.630772
55.534459	31.731778	76.635777
55.013603	31.578727	76.640782
54.490975	33.792673	76.645786
54.429987	22.559367	76.650791
54.059498	25.920706	76.655796
52.698515	37.714768	76.660801
52.264258	31.162797	76.665806
51.746608	32.895525	76.670810
50.239333	31.835611	76.675815
49.340915	31.366397	76.680820
49.058444	34.832245	76.685825
48.709199	26.206883	76.690830
47.948222	35.701502	76.695834
47.828422	27.712153	76.700839
46.709561	36.062286	76.705844
45.956412	29.862999	76.710849
45.284589	27.485975	76.715854
44.780561	35.844371	76.720858
44.751885	30.286613	76.725863
43.283204	26.429867	76.730868
42.561557	34.519672	76.735873
41.774115	34.811778	76.740878
41.279149	36.663374	76.745882
41.403715	30.883960	76.750887
40.123855	30.288316	76.755892
39.258162	30.776590	76.760897
39.072063	33.222557	76.765902
38.374350	35.992280	76.770906
37.650067	25.039662	76.775911
36.559858	29.642620	76.780916
35.856381	32.190713	76.785921
35.478110	34.427276	76.790926
35.077065	42.817754	76.795930
34.060585	32.007592	76.800935
33.184344	40.834784	76.805940
32.870791	31.845298	76.810945
32.372919	33.012567	76.815950
31.604065	34.845601	76.820954
30.894558	27.337865	76.825959
29.836898	36.511534	76.830964
29.365372	36.378842	76.835969
29.249607	36.233702	76.840974
28.606671	28.950984	76.845978
27.872045	29.566384	76.850983
26.526981	32.608931	76.855988
26.144763	31.885832	76.860993
25.604343	28.993681	76.865998
25.086230	27.704182	76.871002
24.772582	33.615879	76.876007
23.451031	43.517651	76.881012
23.096847	34.606969	76.886017
22.508609	36.905979	76.891022
21.395272	34.089559	76.896026
20.776323	36.957878	76.901031
20.307546	33.659125	76.906036
19.887158	36.812722	76.911041
19.232188	30.677523	76.916046
17.941510	36.150067	76.921050
17.340521	26.400711	76.926055
16.761738	28.338122	76.931060
16.535806	22.300670	76.936065
16.077252	22.428633	76.941070
15.018984	31.378998	76.946074
14.147902	25.328617	76.951079
13.423623	27.978957	76.956084
13.502698	26.066442	76.961089
12.941396	26.522661	76.966094
11.651357	32.701236	76.971098
10.767326	24.352300	76.976103
10.188208	23.306933	76.981108
10.070175	20.690499	76.986113
8.944562	32.592225	76.991118
8.037999	39.665782	76.996122
7.752159	38.887082	77.001127
6.822634	39.598662	77.006132
6.763734	30.515785	77.011137
6.238791	34.536334	77.016142
4.798483	38.477794	77.021147
4.655634	29.744027	77.026151
4.088294	38.271166	77.031156
3.273589	38.336652	77.036161