Tue Jun 08 17:42:39 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.160738	100.868760	0.000000
-1.642291	95.565084	0.005005
-2.098320	57.195119	0.010010
-3.544885	14.168164	0.015014
-8.167455	3.320744	0.020019
-13.910575	17.709082	0.025024
-19.097869	6.553923	0.030029
-23.392747	-4.645693	0.035034
-27.420888	6.173678	0.040038
-31.372055	2.680671	0.045043
-34.870791	4.364084	0.050048
-38.321083	-0.145133	0.055053
-41.566148	-8.195354	0.060058
-45.276688	4.857312	0.065062
-49.201665	3.297465	0.070067
-53.280011	3.666820	0.075072
-56.929523	9.340577	0.080077
-61.023343	4.770420	0.085082
-64.859473	2.195155	0.090086
-68.391421	1.754036	0.095091
-72.507111	4.797265	0.100096
-75.716918	6.744959	0.105101
-79.114040	1.847340	0.110106
-83.031035	11.137141	0.115110
-86.908012	6.035252	0.120115
-90.599406	4.684449	0.125120
-94.648066	8.788631	0.130125
-98.257303	-2.009437	0.135130
-102.586106	14.938910	0.140134
-106.192403	14.185722	0.145139
-109.713552	13.715152	0.150144
-113.398616	10.559849	0.155149
-116.943299	9.955173	0.160154
-121.151323	11.242819	0.165158
-124.742598	3.525563	0.170163
-128.596582	8.070042	0.175168
-132.159415	10.154100	0.180173
-135.482207	2.362394	0.185178
-139.537055	-3.040893	0.190182
-143.298847	-9.163463	0.195187
-147.547322	-0.340948	0.200192
-151.594653	-5.338565	0.205197
-155.145095	3.180316	0.210202
-159.257660	15.199586	0.215206
-162.713834	13.308799	0.220211
-166.057393	5.556991	0.225216
-170.048305	7.589763	0.230221
-173.714212	8.255574	0.235226
-177.413844	10.376942	0.240230
-180.962159	8.960625	0.245235
-184.661928	12.646259	0.250240
-188.476991	8.739288	0.255245
-192.335766	1.912649	0.260250
-196.547073	11.139336	0.265254
-200.005740	2.166725	0.270259
-203.708208	5.126174	0.275264
-207.654266	11.080624	0.280269
-211.294024	10.622977	0.285274
-215.261153	14.852613	0.290278
-218.989651	6.720451	0.295283
-222.495942	11.725997	0.300288
-226.582770	6.073687	0.305293
-229.824406	-1.608709	0.310298
-233.279930	2.635029	0.315302
-237.262485	0.459609	0.320307
-241.380996	6.399455	0.325312
-245.458160	15.900394	0.330317
-248.618649	8.170145	0.335322
-252.835946	13.215561	0.340326
-256.071837	12.620002	0.345331
-259.885644	7.467570	0.350336
-264.412984	14.262637	0.355341
-267.931943	10.766760	0.360346
-271.838763	14.050242	0.365350
-275.060207	5.224888	0.370355
-279.011636	4.381443	0.375360
-282.705471	7.089228	0.380365
-286.335286	7.584740	0.385370
-290.278014	14.581905	0.390374
-293.961841	5.213813	0.395379
-297.726564	5.008577	0.400384
-301.989697	10.350036	0.405389
-305.482319	-5.011344	0.410394
-309.099831	7.796614	0.415398
-312.648607	4.352861	0.420403
-316.559587	4.460471	0.425408
-320.430759	9.619063	0.430413
-324.303591	9.751713	0.435418
-327.922837	12.682777	0.440422
-331.632900	3.696959	0.445427
-335.347813	9.055718	0.450432
-339.219753	12.987701	0.455437
-342.425932	3.270110	0.460442
-346.834062	18.034120	0.465446
-350.828772	12.083121	0.470451
-354.275625	4.186568	0.475456
-358.093610	10.140880	0.480461
-361.515188	0.935091	0.485466
-365.406133	6.753512	0.490470
-369.409682	0.793395	0.495475
-373.341561	-0.458291	0.500480
-376.975688	0.550366	0.505485
-380.113053	3.362098	0.510490
-384.354540	0.769421	0.515494
-388.323335	-3.154809	0.520499
-391.934559	8.066187	0.525504
-395.684784	7.559751	0.530509
-398.921666	2.194407	0.535514
-403.036027	1.375471	0.540518
-406.836244	-2.591080	0.545523
-410.764616	2.705282	0.550528
-414.652062	8.448938	0.555533
-417.775683	2.676574	0.560538
-422.348613	7.734995	0.565542
-425.779142	-0.640313	0.570547
-429.615045	5.819198	0.575552
-433.483701	5.796105	0.580557
-437.016014	4.035433	0.585562
-441.080152	1.375678	0.590566
-444.404160	3.445450	0.595571
-448.068477	7.133102	0.600576
-452.009691	12.567879	0.605581
-455.758303	-2.106068	0.610586
-459.412698	8.966076	0.615590
-463.178408	10.225519	0.620595
-466.973797	-0.606978	0.625600
-470.678589	5.406154	0.630605
-474.856615	6.574909	0.635610
-478.677420	8.773752	0.640614
-482.148548	3.588388	0.645619
-486.188109	4.626432	0.650624
-490.100166	11.630731	0.655629
-493.684859	1.907949	0.660634
-497.020429	10.284425	0.665638
-500.521482	5.015796	0.670643
-504.104443	13.445775	0.675648
-508.575930	13.665114	0.680653
-511.896844	9.542608	0.685658
-516.077755	10.560723	0.690662
-520.166677	7.134428	0.695667
-523.405982	7.457349	0.700672
-527.306133	19.125489	0.705677
-530.859028	3.299428	0.710682
-534.907964	13.921071	0.715686
-538.884302	7.622522	0.720691
-542.698137	-3.014116	0.725696
-546.263449	11.643730	0.730701
-549.928875	5.032128	0.735706
-553.436491	13.289752	0.740710
-557.219904	9.425837	0.745715
-560.864730	11.876376	0.750720
-565.027707	8.633739	0.755725
-568.380590	6.744105	0.760730
-572.276412	17.577517	0.765734
-576.188601	13.117994	0.770739
-580.027351	12.140625	0.775744
-584.177059	13.456981	0.780749
-587.534421	-3.735104	0.785754
-591.648321	10.649035	0.790758
-595.268353	14.971002	0.795763
-598.758205	10.832161	0.800768
-602.524901	14.148717	0.805773
-605.872202	9.083513	0.810778
-610.064735	13.688847	0.815782
-613.990724	14.553188	0.820787
-617.686307	12.781208	0.825792
-621.324227	16.968118	0.830797
-624.968289	2.491119	0.835802
-628.749745	10.548699	0.840806
-632.555978	9.998396	0.845811
-636.366733	11.004813	0.850816
-640.024815	16.351691	0.855821
-643.346037	8.969053	0.860826
-647.890100	18.166785	0.865830
-651.353326	9.809515	0.870835
-654.967933	7.541339	0.875840
-659.394061	8.294193	0.880845
-663.092398	5.510300	0.885850
-666.252932	7.124318	0.890854
-670.308656	9.351400	0.895859
-673.981659	8.752220	0.900864
-678.110929	18.038260	0.905869
-681.232928	11.151557	0.910874
-684.908132	11.378492	0.915878
-688.779231	8.304951	0.920883
-692.677155	9.958303	0.925888
-696.580024	8.713772	0.930893
-700.820850	11.441561	0.935898
-704.831150	8.959514	0.940902
-708.133837	12.770035	0.945907
-711.098591	5.511792	0.950912
-715.262142	14.849136	0.955917
-719.068669	3.685662	0.960922
-723.061465	13.307105	0.965926
-727.026307	9.425932	0.970931
-730.451572	7.917898	0.975936
-734.321667	12.576552	0.980941
-737.958442	1.957080	0.985946
-741.649796	12.275563	0.990950
-745.455713	10.669857	0.995955
-749.008227	10.852107	1.000960
-752.998940	12.976140	1.005965
-756.678632	3.258064	1.010970
-760.201335	16.039012	1.015974
-764.036721	17.307905	1.020979
-767.682825	11.920330	1.025984
-771.669488	16.557973	1.030989
-775.533230	7.935238	1.035994
-779.206519	15.097726	1.040998
-783.077371	11.773195	1.046003
-786.779346	11.314468	1.051008
-790.964313	17.373166	1.056013
-794.652480	5.823557	1.061018
-798.407839	14.898294	1.066022
-802.017088	4.228766	1.071027
-805.421126	11.152047	1.076032
-809.223726	22.986017	1.081037
-812.998427	9.576808	1.086042
-816.665931	14.325486	1.091046
-820.659064	14.282262	1.096051
-824.368624	10.959688	1.101056
-828.531036	12.964455	1.106061
-832.125256	14.945115	1.111066
-835.856023	12.582566	1.116070
-839.583820	10.310690	1.121075
-843.309433	16.011924	1.126080
-846.902370	6.013009	1.131085
-850.724429	10.513526	1.136090
-854.951848	6.511376	1.141094
-858.475211	10.047670	1.146099
-862.140929	10.420353	1.151104
-866.088746	12.850917	1.156109
-869.542871	9.364546	1.161114
-873.460449	8.950402	1.166118
-876.974817	21.761579	1.171123
-880.626460	15.450650	1.176128
-885.035953	14.085245	1.181133
-888.327334	4.259589	1.186138
-891.888545	15.544980	1.191142
-896.061069	19.818351	1.196147
-899.533172	18.706491	1.201152
-903.285900	24.190211	1.206157
-906.988570	13.543523	1.211162
-910.988273	12.085302	1.216166
-915.132224	16.489959	1.221171
-918.653403	13.553520	1.226176
-922.559429	24.475401	1.231181
-925.401494	8.207987	1.236186
-929.806669	13.255876	1.241190
-933.678110	8.811014	1.246195
-937.195448	10.528711	1.251200
-941.344024	17.200199	1.256205
-944.833935	1.181778	1.261210
-948.725367	21.506639	1.266214
-952.508140	16.860664	1.271219
-955.825959	13.131113	1.276224
-960.022611	25.820287	1.281229
-963.462476	18.664715	1.286234
-967.197708	16.714335	1.291238
-971.028409	16.847428	1.296243
-974.804453	7.875124	1.301248
-979.066941	13.073025	1.306253
-982.757218	19.663107	1.311258
-986.167613	20.169679	1.316262
-989.637170	15.197223	1.321267
-993.362638	6.992248	1.326272
-997.389331	10.419290	1.331277
-1001.071147	8.313334	1.336282
-1005.222438	18.656512	1.341286
-1009.153938	14.584372	1.346291
-1012.344147	14.111787	1.351296
-1016.106200	11.168238	1.356301
-1019.924953	12.428974	1.361306
-1024.153766	10.396822	1.366310
-1027.919065	10.550708	1.371315
-1031.183224	6.139428	1.376320
-1035.443275	12.714094	1.381325
-1038.594151	2.765770	1.386330
-1042.447554	11.787270	1.391334
-1046.399077	18.385154	1.396339
-1050.257312	17.175122	1.401344
-1054.200823	19.238828	1.406349
-1057.426114	3.841348	1.411354
-1061.360965	17.875016	1.416358
-1065.014879	8.445285	1.421363
-1068.728066	7.773613	1.426368
-1072.960996	14.514565	1.431373
-1076.623309	15.336022	1.436378
-1080.427181	8.269506	1.441382
-1084.024363	5.830960	1.446387
-1087.601273	5.262606	1.451392
-1091.623535	9.917297	1.456397
-1094.955613	6.251490	1.461402
-1098.773011	8.227270	1.466406
-1102.824022	11.025870	1.471411
-1106.525070	5.348063	1.476416
-1110.610515	11.597576	1.481421
-1114.121448	3.276152	1.486426
-1118.116831	6.057713	1.491430
-1121.772904	12.312844	1.496435
-1125.296080	15.584074	1.501440
-1129.257559	14.501968	1.506445
-1133.015118	-0.429464	1.511450
-1136.243839	4.129658	1.516454
-1140.543581	3.683892	1.521459
-1144.049102	-1.050555	1.526464
-1147.652997	11.976287	1.531469
-1151.499699	-5.654600	1.536474
-1155.391506	7.969141	1.541478
-1159.269721	5.273812	1.546483
-1162.802290	-0.183022	1.551488
-1166.965873	-0.040743	1.556493
-1170.729249	0.242404	1.561498
-1174.588210	16.007329	1.566502
-1178.283178	10.887842	1.571507
-1182.025007	10.092909	1.576512
-1185.449607	15.471960	1.581517
-1189.207394	3.795368	1.586522
-1192.956075	14.397565	1.591526
-1196.817953	19.150328	1.596531
-1200.891316	10.497310	1.601536
-1204.812964	15.445065	1.606541
-1208.081540	6.514912	1.611546
-1211.591366	7.950115	1.616550
-1215.201052	20.227276	1.621555
-1219.111696	6.160180	1.626560
-1223.267781	14.920413	1.631565
-1226.969438	-0.023677	1.636570
-1230.928277	10.384920	1.641574
-1234.433037	9.657864	1.646579
-1237.985482	4.337524	1.651584
-1242.305533	12.633736	1.656589
-1245.695191	8.637706	1.661594
-1249.582640	10.773664	1.666598
-1253.306816	16.863770	1.671603
-1256.902660	12.104670	1.676608
-1260.791183	16.909823	1.681613
-1264.221653	6.017419	1.686618
-1268.036828	5.190164	1.691622
-1272.464038	-1.308482	1.696627
-1275.903791	0.966118	1.701632
-1280.181147	16.667992	1.706637
-1283.464773	3.262165	1.711642
-1286.834534	15.240029	1.716646
-1290.553705	11.854008	1.721651
-1294.325267	0.874178	1.726656
-1298.110290	12.330524	1.731661
-1302.013789	4.122484	1.736666
-1306.160921	11.409396	1.741670
-1310.392666	10.379014	1.746675
-1313.908572	9.736433	1.751680
-1317.259981	10.750202	1.756685
-1320.602622	5.575466	1.761690
-1324.334224	13.611616	1.766694
-1328.351220	9.874186	1.771699
-1332.061583	6.021729	1.776704
-1335.861928	8.649211	1.781709
-1339.671651	12.590307	1.786714
-1343.723035	11.000074	1.791718
-1347.569560	16.639599	1.796723
-1350.799403	6.430784	1.801728
-1354.914471	13.729602	1.806733
-1358.459430	4.860871	1.811738
-1362.262851	15.943486	1.816742
-1366.409162	11.599540	1.821747
-1369.867155	7.656009	1.826752
-1374.084434	12.001851	1.831757
-1377.325381	0.035772	1.836762
-1380.982064	8.046860	1.841766
-1384.892197	10.999535	1.846771
-1388.897420	8.847252	1.851776
-1392.681790	18.510419	1.856781
-1395.938749	14.214243	1.861786
-1399.481494	13.197823	1.866790
-1403.831197	11.906769	1.871795
-1407.344100	16.763569	1.876800
-1411.334089	17.465565	1.881805
-1414.616389	12.425792	1.886810
-1418.301084	18.408208	1.891814
-1422.663882	14.535290	1.896819
-1426.130152	7.481377	1.901824
-1430.011495	18.325611	1.906829
-1433.838912	20.975198	1.911834
-1437.432643	16.839138	1.916838
-1441.188566	13.062892	1.921843
-1444.932869	17.220587	1.926848
-1448.950830	19.465982	1.931853
-1452.753468	4.939703	1.936858
-1456.404747	14.639656	1.941862
-1460.040476	13.923844	1.946867
-1463.903764	14.201129	1.951872
-1467.592680	16.209634	1.956877
-1471.757092	17.652910	1.961882
-1475.709719	18.130276	1.966886
-1479.188487	11.730215	1.971891
-1482.578349	7.270645	1.976896
-1486.359837	13.019106	1.981901
-1490.044813	9.833038	1.986906
-1494.136038	5.084665	1.991910
-1497.485185	21.642836	1.996915
-1501.876506	15.349338	2.006912
-1502.646793	12.847628	2.016909
-1499.850859	14.941306	2.026906
-1497.083259	15.213984	2.036902
-1494.967012	11.550432	2.046899
-1493.349208	13.200351	2.056896
-1491.479226	8.559074	2.066893
-1489.618813	16.221138	2.076890
-1487.602684	19.428917	2.086886
-1485.442076	12.004439	2.096883
-1483.729067	7.529642	2.106880
-1481.534605	10.251107	2.116877
-1480.306649	7.614375	2.126874
-1478.162252	10.910383	2.136870
-1475.998086	10.368671	2.146867
-1473.801021	11.848735	2.156864
-1472.509330	8.752097	2.166861
-1470.898057	16.187439	2.176858
-1468.682643	7.459243	2.186854
-1466.611937	12.310027	2.196851
-1464.561532	11.076486	2.206848
-1463.130111	9.418122	2.216845
-1461.043877	11.836096	2.226842
-1459.212707	14.415663	2.236838
-1457.230590	11.541089	2.246835
-1455.482234	11.198078	2.256832
-1453.515568	9.544988	2.266829
-1451.288538	12.829583	2.276826
-1449.570390	11.608864	2.286822
-1448.162104	15.311157	2.296819
-1446.154021	15.592227	2.306816
-1443.849362	12.077338	2.316813
-1442.196973	11.710903	2.326810
-1440.114460	14.133084	2.336806
-1438.503008	19.242997	2.346803
-1436.679578	17.719251	2.356800
-1434.983813	11.212495	2.366797
-1432.944649	8.535618	2.376794
-1430.765237	12.205830	2.386790
-1428.823729	6.190002	2.396787
-1427.027017	3.330299	2.406784
-1425.572041	12.600201	2.416781
-1423.255037	11.177421	2.426778
-1421.234401	7.218904	2.436774
-1419.736569	5.385134	2.446771
-1417.668908	2.123596	2.456768
-1415.875729	2.259010	2.466765
-1414.294307	4.253510	2.476762
-1412.149056	4.084206	2.486758
-1410.032902	7.648313	2.496755
-1407.978099	11.014291	2.506752
-1406.393666	9.835530	2.516749
-1404.840028	7.945148	2.526746
-1402.767893	6.461689	2.536742
-1400.925743	5.173845	2.546739
-1398.943752	8.021962	2.556736
-1396.964895	9.611479	2.566733
-1395.254886	3.144186	2.576730
-1393.338131	10.462668	2.586726
-1391.552014	6.438138	2.596723
-1389.769734	7.938120	2.606720
-1387.520617	0.719014	2.616717
-1385.550009	1.657066	2.626714
-1383.922910	2.015465	2.636710
-1381.943832	11.818210	2.646707
-1380.174199	1.464063	2.656704
-1378.325528	4.682085	2.666701
-1376.328604	2.501365	2.676698
-1374.408830	2.404010	2.686694
-1372.661982	0.927039	2.696691
-1370.590222	6.042089	2.706688
-1368.881936	1.014852	2.716685
-1367.232648	1.730669	2.726682
-1365.346750	9.853977	2.736678
-1363.272876	9.999295	2.746675
-1361.368533	6.789152	2.756672
-1359.265530	4.557021	2.766669
-1357.774574	0.323947	2.776666
-1355.923040	4.682460	2.786662
-1353.850803	1.761627	2.796659
-1351.509301	7.090403	2.806656
-1349.848536	5.002610	2.816653
-1348.360764	9.225610	2.826650
-1346.417372	10.118165	2.836646
-1344.816725	8.510209	2.846643
-1342.431198	2.698749	2.856640
-1340.960139	4.344689	2.866637
-1338.786890	9.360516	2.876634
-1337.068076	0.979308	2.886630
-1335.074117	9.150861	2.896627
-1333.001542	10.893858	2.906624
-1331.238260	6.829404	2.916621
-1329.484409	4.671881	2.926618
-1327.671649	13.531009	2.936614
-1325.789597	6.856342	2.946611
-1323.552828	10.772859	2.956608
-1321.894097	5.833982	2.966605
-1320.143523	8.475671	2.976602
-1318.408485	6.680630	2.986598
-1316.132794	6.198887	2.996595
-1314.216121	11.559159	3.006592
-1312.218910	8.862273	3.016589
-1310.873985	7.892649	3.026586
-1309.006976	2.980447	3.036582
-1306.978257	3.882472	3.046579
-1304.993141	9.144046	3.056576
-1303.367777	7.622363	3.066573
-1301.402001	6.923929	3.076570
-1299.315965	1.016517	3.086566
-1297.255620	6.701880	3.096563
-1295.507090	2.338034	3.106560
-1293.994091	6.014889	3.116557
-1292.155563	-0.651892	3.126554
-1290.034412	4.394647	3.136550
-1287.963999	5.825426	3.146547
-1286.450302	7.277129	3.156544
-1284.445456	6.896855	3.166541
-1282.386084	2.564596	3.176538
-1280.778055	5.048988	3.186534
-1278.823676	12.161489	3.196531
-1276.823033	10.651638	3.206528
-1275.098777	8.063697	3.216525
-1272.883230	6.990401	3.226522
-1271.285124	3.004531	3.236518
-1269.630112	13.418271	3.246515
-1267.539062	6.575731	3.256512
-1265.582844	4.777503	3.266509
-1263.667935	-0.932933	3.276506
-1261.956346	10.150854	3.286502
-1259.995906	7.785960	3.296499
-1257.841813	14.493467	3.306496
-1256.228633	11.768501	3.316493
-1254.214166	7.561738	3.326490
-1252.201620	10.760372	3.336486
-1250.741776	16.625569	3.346483
-1248.847862	17.516787	3.356480
-1246.704174	12.513616	3.366477
-1245.072940	8.709394	3.376474
-1243.468677	10.133308	3.386470
-1241.370738	10.872902	3.396467
-1239.171687	10.968329	3.406464
-1237.671453	9.941623	3.416461
-1235.767395	3.973406	3.426458
-1233.478844	13.136597	3.436454
-1231.611862	8.650070	3.446451
-1230.127155	11.829497	3.456448
-1228.106015	12.010813	3.466445
-1226.004036	14.251129	3.476442
-1224.448881	9.483413	3.486438
-1222.581235	12.742912	3.496435
-1220.480234	9.249281	3.506432
-1218.743539	7.184856	3.516429
-1217.129350	6.061917	3.526426
-1214.809326	7.742717	3.536422
-1213.237434	3.891393	3.546419
-1211.178357	2.637120	3.556416
-1209.389035	10.471204	3.566413
-1207.074391	0.724618	3.576410
-1205.623503	4.848092	3.586406
-1203.865526	7.081494	3.596403
-1201.873449	9.111473	3.606400
-1199.768185	3.702323	3.616397
-1198.080562	4.979938	3.626394
-1196.042483	7.165637	3.636390
-1194.465140	5.519846	3.646387
-1192.450252	13.610427	3.656384
-1190.739811	10.686984	3.666381
-1188.460931	16.670418	3.676378
-1186.716028	17.333924	3.686374
-1185.194779	12.269311	3.696371
-1182.979592	9.763877	3.706368
-1181.045972	9.016876	3.716365
-1179.431782	5.589869	3.726362
-1177.599744	8.475310	3.736358
-1175.503493	5.407764	3.746355
-1173.608465	8.161060	3.756352
-1171.542771	4.962811	3.766349
-1169.671886	-1.184641	3.776346
-1168.206217	3.342980	3.786342
-1166.242563	3.544078	3.796339
-1164.410239	11.954133	3.806336
-1162.269146	3.635625	3.816333
-1160.462686	7.021061	3.826330
-1159.003673	3.919884	3.836326
-1156.940124	3.930729	3.846323
-1154.804707	8.819577	3.856320
-1153.053531	13.264588	3.866317
-1151.234190	14.172609	3.876314
-1148.912723	10.621787	3.886310
-1147.357432	9.940558	3.896307
-1145.839757	7.975029	3.906304
-1143.376075	7.297084	3.916301
-1141.720793	11.305653	3.926298
-1140.144212	9.692419	3.936294
-1138.155554	13.936201	3.946291
-1135.917737	7.735235	3.956288
-1134.298469	11.622734	3.966285
-1132.132349	8.354299	3.976282
-1130.335385	12.611636	3.986278
-1129.005583	11.652174	3.996275
-1126.810889	12.988185	4.006272
-1124.759584	8.266120	4.016269
-1122.988848	7.459378	4.026266
-1121.146405	9.873943	4.036262
-1119.155689	10.711844	4.046259
-1117.493866	11.233141	4.056256
-1115.557886	1.707329	4.066253
-1113.490628	6.805114	4.076250
-1111.624096	1.242552	4.086246
-1109.938941	4.767799	4.096243
-1108.047712	0.724143	4.106240
-1105.977431	6.481811	4.116237
-1104.060594	-5.063398	4.126234
-1102.260519	7.055749	4.136230
-1100.524029	9.428049	4.146227
-1098.698036	9.742923	4.156224
-1096.516657	3.822783	4.166221
-1095.076081	8.482793	4.176218
-1093.131626	7.866762	4.186214
-1090.991205	3.245208	4.196211
-1089.061721	2.439677	4.206208
-1087.265186	2.325277	4.216205
-1085.576826	3.285061	4.226202
-1083.659205	3.339969	4.236198
-1081.977621	2.829942	4.246195
-1079.727164	2.537616	4.256192
-1077.362869	7.337411	4.266189
-1075.887267	5.078374	4.276186
-1074.788593	1.832004	4.286182
-1072.383235	5.398015	4.296179
-1070.463305	5.375861	4.306176
-1068.194068	6.509402	4.316173
-1066.512378	0.341119	4.326170
-1065.108331	2.097864	4.336166
-1063.202461	10.438038	4.346163
-1061.380359	7.713629	4.356160
-1059.208541	3.321059	4.366157
-1057.270629	5.928723	4.376154
-1055.420576	10.043398	4.386150
-1053.456283	8.130846	4.396147
-1051.522956	8.544295	4.406144
-1049.706913	4.675212	4.416141
-1048.028130	11.803936	4.426138
-1046.137758	16.509649	4.436134
-1044.042598	7.114614	4.446131
-1042.355357	3.746646	4.456128
-1040.498197	4.040781	4.466125
-1038.498168	7.229421	4.476122
-1036.897061	8.528675	4.486118
-1034.775287	14.138034	4.496115
-1032.778197	6.901099	4.506112
-1030.975158	7.745576	4.516109
-1028.937494	6.052427	4.526106
-1027.261861	5.521706	4.536102
-1025.300247	6.900950	4.546099
-1023.707785	5.234049	4.556096
-1021.795361	7.239852	4.566093
-1019.824898	4.875319	4.576090
-1018.121672	2.213230	4.586086
-1016.166143	4.367743	4.596083
-1013.796284	3.394553	4.606080
-1012.233163	3.626944	4.616077
-1010.654430	4.138440	4.626074
-1008.469296	5.133902	4.636070
-1006.597759	4.629231	4.646067
-1004.872454	3.475832	4.656064
-1002.884885	5.471904	4.666061
-1000.902530	-3.090397	4.676058
-999.015586	3.165155	4.686054
-997.588649	5.231397	4.696051
-995.404505	7.668768	4.706048
-993.360290	6.282776	4.716045
-991.893068	5.740424	4.726042
-989.901205	11.671286	4.736038
-987.611937	11.559676	4.746035
-985.911684	8.484717	4.756032
-984.385578	15.132232	4.766029
-982.241173	11.074799	4.776026
-980.091433	5.037231	4.786022
-978.691565	6.269092	4.796019
-976.996127	0.422157	4.806016
-974.590621	-0.131883	4.816013
-972.659828	-1.177480	4.826010
-970.971974	0.414777	4.836006
-968.972563	3.903523	4.846003
-967.317500	4.205906	4.856000
-965.522548	-1.069243	4.865997
-963.432497	1.372837	4.875994
-961.425744	2.486288	4.885990
-959.627417	-6.209601	4.895987
-958.201992	3.447353	4.905984
-956.159852	0.478121	4.915981
-954.039750	1.902513	4.925978
-952.093166	3.769693	4.935974
-950.368806	2.039467	4.945971
-948.705318	7.082561	4.955968
-946.578757	4.926414	4.965965
-944.392382	-1.692854	4.975962
-942.634296	3.332815	4.985958
-941.227413	3.985685	4.995955
-939.187971	1.594328	5.005952
-937.216621	3.522472	5.015949
-935.166848	-3.920675	5.025946
-933.559638	6.875307	5.035942
-932.039281	9.888273	5.045939
-929.619662	10.952996	5.055936
-927.625897	8.122104	5.065933
-926.030926	6.629490	5.075930
-924.167611	9.150036	5.085926
-922.189990	3.763314	5.095923
-920.119798	0.117026	5.105920
-918.350551	3.936581	5.115917
-916.570971	5.209591	5.125914
-914.808823	2.935404	5.135910
-912.808770	6.797545	5.145907
-910.780969	9.492604	5.155904
-908.906792	7.620879	5.165901
-907.568893	7.624412	5.175898
-905.546783	10.423997	5.185894
-903.416833	4.290661	5.195891
-901.571158	4.889166	5.205888
-899.885630	-1.657939	5.215885
-897.530994	3.813507	5.225882
-895.814667	5.860935	5.235878
-894.201483	11.696791	5.245875
-892.277909	15.033398	5.255872
-890.279740	8.442504	5.265869
-888.269202	4.526264	5.275866
-886.630903	2.733375	5.285862
-884.755263	6.716480	5.295859
-882.594066	7.887242	5.305856
-881.031820	9.726765	5.315853
-879.144455	5.613120	5.325850
-876.996480	3.315795	5.335846
-875.153777	5.990477	5.345843
-873.488886	11.330960	5.355840
-871.674733	5.945444	5.365837
-869.579148	5.627250	5.375834
-867.505370	9.029378	5.385830
-865.691076	7.676984	5.395827
-864.377412	4.717830	5.405824
-862.369283	4.289369	5.415821
-860.384768	6.802972	5.425818
-858.354005	4.385871	5.435814
-856.392080	9.606212	5.445811
-854.727972	6.205526	5.455808
-853.011615	8.878193	5.465805
-850.760832	7.708955	5.475802
-848.865919	8.317211	5.485798
-846.899943	9.165021	5.495795
-845.404564	8.459009	5.505792
-843.524191	9.486713	5.515789
-841.756665	12.047057	5.525786
-839.628960	12.466759	5.535782
-837.663377	8.330218	5.545779
-835.802301	14.151611	5.555776
-834.250836	16.396120	5.565773
-831.961261	5.670707	5.575770
-830.337682	6.592709	5.585766
-828.388735	5.164654	5.595763
-826.714055	7.876498	5.605760
-824.581979	12.499335	5.615757
-822.542707	10.620254	5.625754
-820.552489	6.492139	5.635750
-819.225267	5.236013	5.645747
-817.343042	10.929687	5.655744
-815.316105	10.315826	5.665741
-813.410708	9.378597	5.675738
-811.474934	11.929442	5.685734
-809.305105	9.128848	5.695731
-807.772555	6.246752	5.705728
-805.754228	8.001698	5.715725
-803.889989	10.530440	5.725722
-801.981064	4.445360	5.735718
-800.274106	2.390942	5.745715
-798.459260	8.017937	5.755712
-796.968678	3.746761	5.765709
-794.429010	4.369264	5.775706
-792.710076	8.550042	5.785702
-791.044260	5.760479	5.795699
-788.829735	7.477807	5.805696
-787.089464	4.321356	5.815693
-785.379407	6.424050	5.825690
-783.450119	8.758654	5.835686
-781.454028	6.655408	5.845683
-779.543737	3.040578	5.855680
-777.531656	3.282944	5.865677
-775.893563	4.091025	5.875674
-774.159677	10.494689	5.885670
-772.417398	6.763259	5.895667
-770.226080	9.212561	5.905664
-768.135845	7.440951	5.915661
-766.452898	9.082746	5.925658
-764.577544	8.847060	5.935654
-762.509624	6.824369	5.945651
-760.776123	4.443312	5.955648
-759.315968	7.505407	5.965645
-757.009412	8.691994	5.975642
-754.852888	14.349689	5.985638
-753.448553	10.735152	5.995635
-751.635827	13.002039	6.005632
-749.331360	10.489794	6.015629
-747.862613	11.542737	6.025626
-745.942262	9.235138	6.035622
-743.908443	8.451769	6.045619
-742.345138	5.550977	6.055616
-740.154657	14.658200	6.065613
-738.152444	9.492601	6.075610
-736.209971	9.605842	6.085606
-734.487980	13.897968	6.095603
-732.852408	10.863841	6.105600
-730.661453	7.944257	6.115597
-728.753618	7.651239	6.125594
-727.072351	10.524427	6.135590
-725.382683	8.039060	6.145587
-723.088187	10.003934	6.155584
-721.436180	11.941144	6.165581
-719.692899	9.120132	6.175578
-717.697328	8.959080	6.185574
-715.804963	5.501090	6.195571
-713.864232	10.243376	6.205568
-711.960936	11.369565	6.215565
-710.219896	11.775067	6.225562
-708.146428	4.601030	6.235558
-706.725370	7.546548	6.245555
-704.568499	12.384933	6.255552
-702.678867	11.374577	6.265549
-700.552118	9.863895	6.275546
-698.806416	11.370455	6.285542
-696.973715	12.383879	6.295539
-695.295764	8.945303	6.305536
-693.558855	4.053291	6.315533
-691.699040	9.114184	6.325530
-689.330504	6.298122	6.335526
-687.491045	6.493483	6.345523
-685.944822	6.951793	6.355520
-683.910759	11.695467	6.365517
-681.656633	13.390643	6.375514
-680.181065	10.122361	6.385510
-678.724431	15.753584	6.395507
-676.491967	9.801147	6.405504
-674.354553	10.845283	6.415501
-672.401426	9.356900	6.425498
-670.739532	2.824198	6.435494
-668.894877	2.804074	6.445491
-667.010063	2.673514	6.455488
-665.268871	5.155458	6.465485
-663.182889	5.104199	6.475482
-661.452058	5.769941	6.485478
-659.477290	7.507535	6.495475
-657.629253	4.467406	6.505472
-655.439773	6.551907	6.515469
-653.934613	3.850430	6.525466
-652.238293	6.144450	6.535462
-649.995548	12.947753	6.545459
-647.991320	10.195018	6.555456
-646.495018	9.513419	6.565453
-644.430961	6.606166	6.575450
-642.271548	12.007329	6.585446
-641.137147	6.903346	6.595443
-639.104273	9.800810	6.605440
-637.262529	12.801422	6.615437
-634.977185	6.176367	6.625434
-633.011827	10.179371	6.635430
-631.388640	16.545189	6.645427
-629.538803	14.443393	6.655424
-627.458008	8.862422	6.665421
-625.532479	10.069409	6.675418
-623.681233	8.805623	6.685414
-622.228308	11.853596	6.695411
-620.071138	8.941837	6.705408
-618.279960	2.263264	6.715405
-616.308957	6.958116	6.725402
-614.726972	11.755689	6.735398
-612.886294	18.375469	6.745395
-610.568044	21.203429	6.755392
-608.638755	8.056009	6.765389
-606.941965	7.137275	6.775386
-605.132670	7.100324	6.785382
-603.380382	14.199254	6.795379
-601.167975	18.735711	6.805376
-599.361017	17.539605	6.815373
-597.567642	16.176680	6.825370
-595.709168	19.132944	6.835366
-593.767168	18.629006	6.845363
-591.759030	15.125112	6.855360
-590.285532	12.672934	6.865357
-588.234040	15.784992	6.875354
-586.490514	14.372133	6.885350
-584.514970	14.351718	6.895347
-582.487451	16.812629	6.905344
-580.578145	17.165993	6.915341
-578.982814	13.440480	6.925338
-576.919285	11.952165	6.935334
-575.030939	15.388634	6.945331
-573.313535	20.832088	6.955328
-570.832603	16.488266	6.965325
-569.618146	13.898744	6.975322
-567.698792	14.274892	6.985318
-565.649178	12.977882	6.995315
-563.877909	18.159555	7.005312
-562.062617	17.090479	7.015309
-560.157037	17.367820	7.025306
-558.363658	17.591299	7.035302
-556.124604	22.936560	7.045299
-554.439929	18.155915	7.055296
-552.626986	18.244037	7.065293
-550.483032	21.041074	7.075290
-548.595721	22.338046	7.085286
-547.243596	12.516201	7.095283
-545.092717	20.911841	7.105280
-543.069715	17.187653	7.115277
-541.028259	14.956187	7.125274
-539.702247	11.855885	7.135270
-537.371041	11.931367	7.145267
-535.847606	15.117456	7.155264
-533.703696	11.590292	7.165261
-532.079926	8.934107	7.175258
-529.859449	12.579985	7.185254
-528.107155	12.226003	7.195251
-526.318827	10.387344	7.205248
-524.631033	5.808132	7.215245
-522.558148	11.616258	7.225242
-520.592834	9.046125	7.235238
-518.758502	8.616813	7.245235
-516.784763	16.053639	7.255232
-514.939007	13.407984	7.265229
-513.126939	13.546465	7.275226
-511.156432	9.029410	7.285222
-509.559767	14.511390	7.295219
-507.242312	14.945731	7.305216
-506.043296	11.178764	7.315213
-503.983736	17.375709	7.325210
-501.673386	10.780409	7.335206
-499.791234	6.012144	7.345203
-498.201744	8.775100	7.355200
-496.428872	8.125538	7.365197
-494.441186	5.700968	7.375194
-492.332368	7.844844	7.385190
-490.566473	6.024670	7.395187
-488.874198	9.909793	7.405184
-486.895471	6.160425	7.415181
-484.838937	5.462199	7.425178
-483.198472	9.570815	7.435174
-481.144933	12.518957	7.445171
-479.238112	6.222125	7.455168
-477.755456	0.980967	7.465165
-475.508345	5.338431	7.475162
-473.533728	7.414440	7.485158
-471.769021	9.292893	7.495155
-470.105854	6.065209	7.505152
-467.885777	8.994270	7.515149
-466.147901	7.789518	7.525146
-464.496105	9.398443	7.535142
-462.611237	11.057097	7.545139
-460.354945	9.809252	7.555136
-458.713976	5.515930	7.565133
-456.974206	7.022028	7.575130
-454.709354	9.872671	7.585126
-452.894985	13.901668	7.595123
-451.425539	10.148786	7.605120
-449.464410	14.852532	7.615117
-447.701442	11.427910	7.625114
-445.565889	9.459364	7.635110
-443.586729	14.779320	7.645107
-441.840173	17.117768	7.655104
-440.038922	10.199209	7.665101
-437.908299	8.807735	7.675098
-435.978750	10.725504	7.685094
-434.334358	11.202237	7.695091
-432.543826	11.046058	7.705088
-430.718129	11.389328	7.715085
-428.753203	11.663658	7.725082
-426.577206	12.131794	7.735078
-425.022487	11.029223	7.745075
-423.364520	6.136617	7.755072
-421.313588	9.017654	7.765069
-419.156692	6.253054	7.775066
-417.362173	9.578037	7.785062
-415.559439	1.444741	7.795059
-413.701449	4.015833	7.805056
-411.842071	5.155222	7.815053
-410.036831	6.752863	7.825050
-408.071908	7.075814	7.835046
-405.781901	9.284292	7.845043
-404.165628	7.368883	7.855040
-402.590562	2.469956	7.865037
-400.428383	8.062850	7.875034
-398.966844	7.378601	7.885030
-396.985679	10.166490	7.895027
-395.205220	14.989389	7.905024
-392.850997	8.173197	7.915021
-391.412052	5.657055	7.925018
-389.309651	5.708631	7.935014
-387.399287	4.249839	7.945011
-385.389971	12.918441	7.955008
-383.702485	11.893098	7.965005
-381.544756	11.792119	7.975002
-379.671312	13.276898	7.984998
-378.095342	11.992060	7.994995
-376.278058	15.089466	8.004992
-374.254621	7.683851	8.014989
-372.505017	10.648615	8.024986
-370.482902	11.072827	8.034982
-368.535302	15.931486	8.044979
-366.891329	12.433245	8.054976
-364.888695	14.309660	8.064973
-362.981245	8.880258	8.074970
-361.078127	7.806077	8.084966
-358.882820	12.342832	8.094963
-357.581237	5.684699	8.104960
-355.843935	11.383304	8.114957
-353.613670	14.110700	8.124954
-351.498017	8.718703	8.134950
-349.672874	13.143880	8.144947
-348.160867	8.360121	8.154944
-346.567481	10.261295	8.164941
-344.275805	7.038873	8.174938
-342.328973	10.156359	8.184934
-340.772518	11.913689	8.194931
-338.648603	17.773235	8.204928
-336.841795	14.495662	8.214925
-334.720185	9.035858	8.224922
-332.956065	15.754272	8.234918
-331.204954	18.202250	8.244915
-329.573954	15.536988	8.254912
-327.505505	13.605300	8.264909
-325.273057	11.188613	8.274906
-323.396122	15.687914	8.284902
-321.636840	16.950035	8.294899
-319.804165	12.532183	8.304896
-317.881799	19.526196	8.314893
-316.108758	11.872673	8.324890
-314.635077	9.739881	8.334886
-312.237358	15.391623	8.344883
-310.433981	17.575335	8.354880
-308.723336	15.087308	8.364877
-306.921139	11.112587	8.374874
-304.543688	10.176017	8.384870
-302.921341	7.078699	8.394867
-301.055700	7.611196	8.404864
-299.426519	6.379703	8.414861
-297.441841	4.165987	8.424858
-295.080025	7.266063	8.434854
-293.422281	9.753783	8.444851
-292.297452	14.367480	8.454848
-290.027945	9.655763	8.464845
-287.773908	7.933736	8.474842
-285.869309	5.410079	8.484838
-284.485872	6.870658	8.494835
-282.239840	5.059108	8.504832
-280.531109	5.741045	8.514829
-278.514035	5.052448	8.524826
-276.748173	4.893449	8.534822
-274.833414	0.933819	8.544819
-273.059079	6.249073	8.554816
-270.972647	5.971858	8.564813
-269.204446	4.629188	8.574810
-267.087422	-1.734840	8.584807
-265.647762	0.920321	8.594803
-263.571751	2.158175	8.604800
-261.646141	8.724033	8.614797
-259.797327	3.889646	8.624794
-258.146449	4.969616	8.634791
-256.010531	8.460596	8.644787
-254.252981	6.034892	8.654784
-252.236023	19.445238	8.664781
-250.534822	13.575017	8.674778
-248.325272	12.945900	8.684775
-246.829694	11.353190	8.694771
-245.047312	16.288859	8.704768
-242.847680	13.819347	8.714765
-241.108495	12.037442	8.724762
-239.155330	13.754828	8.734759
-237.137147	7.002270	8.744755
-235.356096	14.109484	8.754752
-233.323527	2.605158	8.764749
-231.499706	5.351345	8.774746
-229.793986	7.360950	8.784743
-227.782493	10.271768	8.794739
-225.901990	7.631331	8.804736
-224.459393	11.648707	8.814733
-222.222522	6.495630	8.824730
-220.206753	6.907958	8.834727
-218.580887	6.902228	8.844723
-216.861603	4.412357	8.854720
-214.921327	7.177309	8.864717
-212.975878	8.544684	8.874714
-211.089433	6.118231	8.884711
-209.021810	2.488498	8.894707
-207.373463	10.389942	8.904704
-205.428028	7.263328	8.914701
-203.541857	6.019015	8.924698
-201.966199	-0.333950	8.934695
-199.665237	3.418840	8.944691
-197.894713	4.960870	8.954688
-195.898690	9.453637	8.964685
-194.281736	5.357779	8.974682
-192.340825	5.466785	8.984679
-190.526699	3.539254	8.994675
-188.373708	9.037802	9.004672
-186.465607	12.178998	9.014669
-184.990109	8.347298	9.024666
-182.804380	11.289910	9.034663
-180.922460	9.173698	9.044659
-179.394182	14.203167	9.054656
-177.429247	7.967220	9.064653
-175.475940	10.572265	9.074650
-173.201846	12.315661	9.084647
-171.462831	12.345084	9.094643
-169.856127	6.663805	9.104640
-168.175638	13.706486	9.114637
-166.032477	15.940277	9.124634
-164.042273	5.938734	9.134631
-162.188724	2.255624	9.144627
-160.649798	7.268254	9.154624
-158.565142	10.319111	9.164621
-156.510366	2.599935	9.174618
-154.825099	11.093429	9.184615
-152.880346	10.705797	9.194611
-151.007329	7.514557	9.204608
-149.132711	2.248161	9.214605
-147.338324	6.243966	9.224602
-145.659830	9.752980	9.234599
-143.352830	9.191384	9.244595
-141.549174	2.921456	9.254592
-139.899666	11.814724	9.264589
-137.638735	9.218556	9.274586
-135.933695	0.054779	9.284583
-133.921860	12.132610	9.294579
-132.405647	13.481941	9.304576
-130.403927	15.789012	9.314573
-128.683379	6.955741	9.324570
-126.581880	12.482124	9.334567
-124.601610	10.050286	9.344563
-122.958188	12.706916	9.354560
-120.876454	13.507539	9.364557
-119.175725	13.531690	9.374554
-117.160229	12.028895	9.384551
-115.424514	9.425186	9.394547
-113.481547	8.573103	9.404544
-111.544761	7.822466	9.414541
-109.796142	12.680199	9.424538
-107.632899	14.282577	9.434535
-105.755297	12.906584	9.444531
-104.047909	15.729309	9.454528
-102.373755	13.153551	9.464525
-100.322828	14.367330	9.474522
-98.359338	10.248040	9.484519
-96.497311	16.113103	9.494515
-94.893015	13.380569	9.504512
-93.214851	12.718948	9.514509
-90.881195	13.873183	9.524506
-89.198666	9.541629	9.534503
-87.051046	11.003232	9.544499
-85.313792	11.177243	9.554496
-83.558076	9.694506	9.564493
-81.483210	9.281826	9.574490
-79.634200	5.971422	9.584487
-77.811581	10.294794	9.594483
-76.284341	15.726811	9.604480
-74.017544	11.281636	9.614477
-72.221474	11.835645	9.624474
-70.478615	9.514888	9.634471
-68.475087	12.902198	9.644467
-66.855308	14.520324	9.654464
-64.666193	11.409286	9.664461
-62.814595	12.468349	9.674458
-60.943636	7.467801	9.684455
-59.193332	11.515863	9.694451
-57.135411	6.761490	9.704448
-55.141836	11.035006	9.714445
-53.510963	10.304046	9.724442
-51.496136	15.309023	9.734439
-49.582085	14.790350	9.744435
-47.673381	20.481048	9.754432
-45.786349	17.833632	9.764429
-44.096183	23.763366	9.774426
-42.212378	13.237865	9.784423
-40.331994	15.462632	9.794419
-38.934337	14.418738	9.804416
-36.751062	21.174896	9.814413
-34.549668	20.083297	9.824410
-32.816150	10.686224	9.834407
-30.790469	11.159381	9.844403
-29.144023	14.121031	9.854400
-27.058191	14.443575	9.864397
-25.147526	7.599660	9.874394
-23.325245	6.575839	9.884391
-21.623808	14.364720	9.894387
-19.531778	12.490777	9.904384
-17.839936	17.555499	9.914381
-15.797163	11.803050	9.924378
-14.177785	4.997625	9.934375
-12.078432	7.719980	9.944371
-10.343581	8.031177	9.954368
-8.416195	11.414181	9.964365
-6.305793	8.088232	9.974362
-4.717695	12.084296	9.984359
-3.556608	35.849206	9.994355
-2.382448	64.197226	10.004352
-0.904823	131.545642	10.014349
0.000000	185.633127	10.019354
0.244659	221.901104	10.024359
1.062681	257.279053	10.029363
1.576666	290.570631	10.034368
1.687448	313.766220	10.039373
2.573590	337.724914	10.044378
2.702141	358.506578	10.049383
2.993890	366.520695	10.054387
2.946125	392.074802	10.059392
3.390091	402.679837	10.064397
3.320159	401.750826	10.069402
3.397023	406.662198	10.074407
3.769136	419.617498	10.079411
3.654266	437.602169	10.084416
3.856347	436.355737	10.089421
3.803277	440.794023	10.094426
3.637448	445.326640	10.099431
4.267605	445.173609	10.104435
3.834261	459.226219	10.109440
4.402805	452.953714	10.114445
4.514705	458.281054	10.119450
4.195652	457.422779	10.124455
4.112350	451.603475	10.129459
4.063865	462.870070	10.134464
3.997707	459.747331	10.139469
3.969738	461.554442	10.144474
4.111806	470.025313	10.149479
4.521055	478.134996	10.154483
4.583554	494.400302	10.159488
4.941894	495.870005	10.164493
4.837833	492.030231	10.169498
4.731503	482.818271	10.174503
4.773803	477.149127	10.179507
4.590702	477.255531	10.184512
4.529766	495.373911	10.189517
4.909067	501.445653	10.194522
4.835789	519.041983	10.199527
5.332042	512.262394	10.204531
4.871011	520.205932	10.209536
4.840328	519.076769	10.214541
4.719594	517.912917	10.219546
5.245731	528.165276	10.224551
5.264332	517.716520	10.229555
4.954719	520.173487	10.234560
4.996089	513.988979	10.239565
4.997675	524.195095	10.244570
5.216629	535.829953	10.249575
5.107440	522.941209	10.254579
5.086155	526.472915	10.259584
4.706632	533.940657	10.264589
5.535062	549.418268	10.269594
5.440530	565.579129	10.274599
5.709275	563.283131	10.279603
5.555090	564.428231	10.284608
5.574967	565.501646	10.289613
5.893451	566.813984	10.294618
5.819594	579.200507	10.299623
6.112272	570.598615	10.304627
6.176924	578.315473	10.309632
5.952450	582.320175	10.314637
5.809736	574.251604	10.319642
5.911317	591.851587	10.324647
5.813838	583.644206	10.329651
5.883232	584.977545	10.334656
6.048093	588.070781	10.339661
6.097491	586.863148	10.344666
5.762509	591.554281	10.349671
6.037567	588.824972	10.354675
5.630717	588.838692	10.359680
5.491881	604.689436	10.364685
6.422593	607.922935	10.369690
6.181104	622.330022	10.374695
6.323563	631.653523	10.379699
6.322971	631.864027	10.384704
6.604891	628.831174	10.389709
6.681445	632.292051	10.394714
5.854843	639.092833	10.399719
6.093022	633.935954	10.404723
5.992633	656.247362	10.409728
6.297399	670.337417	10.414733
6.593516	663.093932	10.419738
6.128859	676.687116	10.424743
6.596747	681.974415	10.429747
6.571017	698.168221	10.434752
6.621916	703.657284	10.439757
6.738928	705.085888	10.444762
6.488312	711.054143	10.449767
6.748585	712.147138	10.454771
6.872484	727.007977	10.459776
7.209718	732.433746	10.464781
7.515705	734.265732	10.469786
7.140877	742.298414	10.474791
7.449856	733.349829	10.479795
7.285742	741.045204	10.484800
7.291210	745.209860	10.489805
7.513995	743.516968	10.494810
7.291793	756.409846	10.499815
7.555555	745.010630	10.504819
7.402187	748.758055	10.509824
7.439921	753.851111	10.514829
7.914190	753.321789	10.519834
7.370747	755.250868	10.524839
7.667553	754.815524	10.529843
7.879743	758.123307	10.534848
7.967464	755.878450	10.539853
8.133919	753.995877	10.544858
7.770109	758.789500	10.549863
8.157706	758.231223	10.554867
7.640596	765.592404	10.559872
7.784340	766.084473	10.564877
7.986657	781.788877	10.569882
8.060295	799.118363	10.574887
8.358907	800.593206	10.579891
8.177839	797.774308	10.584896
8.490011	803.052822	10.589901
8.774667	799.404082	10.594906
8.268362	808.011569	10.599911
8.380031	798.154949	10.604915
8.607427	798.608597	10.609920
8.537429	810.752276	10.614925
8.675541	807.924044	10.619930
8.476796	810.582701	10.624935
8.792171	805.242006	10.629939
8.889568	803.715078	10.634944
9.008026	801.352842	10.639949
9.361464	800.974102	10.644954
8.304188	792.039874	10.649959
8.676108	787.204219	10.654963
8.622655	808.879781	10.659968
8.524602	813.393779	10.664973
8.752345	802.427795	10.669978
8.272995	812.323802	10.674983
8.809890	809.817584	10.679987
8.532708	824.957677	10.684992
8.603134	844.591812	10.689997
8.989430	849.370928	10.695002
8.700939	857.137027	10.700007
8.990647	845.995391	10.705011
9.063085	862.581872	10.710016
8.938151	878.348800	10.715021
9.297363	889.885664	10.720026
9.220641	893.796033	10.725031
9.778815	883.241493	10.730035
9.601395	885.464668	10.735040
9.607445	886.023375	10.740045
9.781323	885.071084	10.745050
9.281313	895.670942	10.750055
9.494947	891.988174	10.755059
9.351161	890.185225	10.760064
9.400695	899.827581	10.765069
9.573509	905.933702	10.770074
9.918612	921.389162	10.775079
10.021350	916.416069	10.780083
9.881169	927.892536	10.785088
9.931305	927.490403	10.790093
10.244613	929.130501	10.795098
10.027764	931.344654	10.800103
10.390302	918.944697	10.805107
10.382036	920.851509	10.810112
10.033254	924.331693	10.815117
10.538379	921.913405	10.820122
10.264637	934.239744	10.825127
10.675005	929.304296	10.830131
10.656226	934.966045	10.835136
10.491893	936.100279	10.840141
10.171640	931.916545	10.845146
10.330485	933.879178	10.850151
10.277312	937.829336	10.855155
10.260646	934.683016	10.860160
10.445047	948.703961	10.865165
10.593807	966.908511	10.870170
10.410682	978.575534	10.875175
10.679329	976.121205	10.880179
10.401438	975.992023	10.885184
10.543655	977.198042	10.890189
10.957303	974.821877	10.895194
10.930180	984.796770	10.900199
10.918285	984.351981	10.905203
11.155424	990.391448	10.910208
11.217513	1009.364064	10.915213
11.224924	1003.216765	10.920218
11.136670	1004.574802	10.925223
11.030477	1016.612741	10.930227
11.472915	1016.752421	10.935232
11.361542	1017.577581	10.940237
11.484462	1012.782577	10.945242
11.561127	1019.441280	10.950247
11.639178	1018.715016	10.955251
11.674348	1019.364656	10.960256
11.657645	1023.162136	10.965261
11.515891	1016.195670	10.970266
11.629835	1020.674563	10.975271
11.763597	1015.311647	10.980275
12.011181	1027.954463	10.985280
12.010236	1028.860164	10.990285
12.245448	1027.890243	10.995290
11.836355	1015.259750	11.000295
11.825703	1025.585923	11.005299
11.483322	1028.335165	11.010304
11.847849	1031.187413	11.015309
12.217492	1026.929970	11.020314
11.996442	1029.898015	11.025319
11.990980	1030.920543	11.030323
11.779297	1034.434482	11.035328
11.783320	1029.254858	11.040333
12.012790	1033.780263	11.045338
11.838161	1042.664562	11.050343
11.893036	1059.432290	11.055347
11.880218	1065.352012	11.060352
11.832134	1068.959882	11.065357
12.308922	1062.070501	11.070362
12.559553	1069.296635	11.075367
12.708751	1074.346211	11.080371
12.697896	1065.117143	11.085376
12.858861	1080.691570	11.090381
13.044854	1065.553471	11.095386
12.745867	1072.871474	11.100391
12.861575	1055.778062	11.105395
12.939841	1066.260332	11.110400
13.172784	1062.003029	11.115405
13.328273	1062.167435	11.120410
12.878878	1067.825695	11.125415
13.138862	1061.202040	11.130419
13.303734	1067.814061	11.135424
13.010304	1071.197550	11.140429
13.097630	1064.429023	11.145434
12.864782	1069.251601	11.150439
13.057880	1067.377055	11.155443
13.217351	1080.250548	11.160448
13.133274	1084.728280	11.165453
13.487776	1089.320290	11.170458
13.076859	1094.665646	11.175463
13.419049	1088.116701	11.180467
13.550567	1097.048013	11.185472
13.162365	1100.494337	11.190477
13.379687	1096.358124	11.195482
13.199804	1102.628611	11.200487
12.952102	1099.040684	11.205491
13.466508	1110.607157	11.210496
13.673302	1127.229304	11.215501
13.745398	1125.595367	11.220506
13.601678	1137.142462	11.225511
13.772249	1129.833052	11.230515
13.731681	1133.906230	11.235520
13.329512	1128.880298	11.240525
13.941307	1140.426147	11.245530
14.354567	1152.106309	11.250535
14.598965	1146.353718	11.255539
13.934534	1142.861311	11.260544
13.899462	1139.249155	11.265549
14.225259	1144.724794	11.270554
14.348886	1158.723584	11.275559
14.416253	1158.488623	11.280563
14.363569	1161.055980	11.285568
14.425620	1158.783493	11.290573
14.706899	1162.989787	11.295578
14.584640	1164.445643	11.300583
14.571776	1164.507862	11.305587
14.507876	1166.928325	11.310592
14.536892	1176.262919	11.315597
14.641215	1167.610890	11.320602
14.651611	1168.953211	11.325607
14.744067	1171.553710	11.330611
14.601354	1163.152068	11.335616
14.614990	1163.751721	11.340621
14.788796	1164.839443	11.345626
14.544299	1177.536751	11.350631
14.699118	1170.708448	11.355635
14.601866	1179.449688	11.360640
14.810703	1200.826608	11.365645
15.189377	1195.711379	11.370650
15.263273	1210.254011	11.375655
15.265826	1205.858932	11.380659
15.186498	1201.378813	11.385664
15.427665	1205.490153	11.390669
15.379686	1202.850074	11.395674
15.373128	1208.897462	11.400679
15.380749	1203.551373	11.405683
15.376897	1206.779845	11.410688
15.377868	1210.389205	11.415693
15.229096	1198.833416	11.420698
15.434642	1206.936564	11.425703
15.386200	1204.197089	11.430707
15.631158	1212.657040	11.435712
15.724574	1230.623094	11.440717
15.863722	1227.997111	11.445722
15.717658	1236.524907	11.450727
15.738306	1237.874556	11.455731
15.720105	1242.658015	11.460736
15.781650	1240.191786	11.465741
16.100757	1237.386523	11.470746
16.070988	1237.112558	11.475751
15.847830	1238.140451	11.480755
16.348350	1232.474969	11.485760
16.322965	1232.926182	11.490765
16.633872	1243.348157	11.495770
16.139389	1246.182331	11.500775
16.596092	1241.067130	11.505779
16.375464	1234.897258	11.510784
15.737534	1241.862528	11.515789
16.123563	1239.702642	11.520794
16.033678	1241.925464	11.525799
16.143898	1252.213298	11.530803
16.500931	1264.672933	11.535808
16.451363	1271.329308	11.540813
16.536890	1271.613082	11.545818
16.435239	1281.730812	11.550823
16.904398	1272.483663	11.555827
16.986156	1277.517631	11.560832
17.298916	1281.929353	11.565837
17.305593	1273.209532	11.570842
17.222740	1271.185299	11.575847
17.258649	1272.799969	11.580851
17.229153	1270.347370	11.585856
16.929652	1271.706518	11.590861
17.052655	1276.082482	11.595866
17.101505	1287.886018	11.600871
17.276159	1283.846678	11.605875
17.209812	1283.726617	11.610880
17.088125	1289.439297	11.615885
17.320414	1280.093807	11.620890
17.187991	1290.059316	11.625895
16.967253	1283.734704	11.630899
17.158905	1286.941515	11.635904
16.641029	1288.534688	11.640909
16.901811	1299.292536	11.645914
17.144239	1314.313614	11.650919
17.386326	1308.384515	11.655923
17.187369	1308.626276	11.660928
17.263920	1324.112786	11.665933
17.796778	1327.285972	11.670938
17.507246	1343.975685	11.675943
18.212758	1343.785258	11.680947
18.147211	1351.583245	11.685952
17.859986	1343.951166	11.690957
18.133223	1349.617471	11.695962
18.335375	1359.184600	11.700967
18.563471	1338.092186	11.705971
18.361373	1308.969073	11.710976
17.882884	1318.479978	11.715981
18.293249	1311.173581	11.720986
18.103028	1311.312789	11.725991
18.221039	1314.603680	11.730995
18.037418	1323.005723	11.736000
18.125083	1338.313891	11.741005
18.744426	1345.497068	11.746010
18.006138	1348.316614	11.751015
18.145915	1342.978213	11.756019
18.358770	1347.381425	11.761024
18.157935	1347.422977	11.766029
18.443845	1349.427826	11.771034
18.373533	1362.682010	11.776039
18.589849	1371.454069	11.781043
18.938025	1376.677263	11.786048
18.856758	1382.500680	11.791053
19.113005	1379.950518	11.796058
18.723905	1378.172204	11.801063
18.722051	1377.891476	11.806067
19.337997	1377.409689	11.811072
19.279237	1383.893999	11.816077
19.316368	1373.085434	11.821082
18.993568	1374.176605	11.826087
19.436060	1378.270842	11.831091
19.322326	1370.169652	11.836096
19.034341	1365.127222	11.841101
19.249460	1369.466103	11.846106
19.234677	1384.129499	11.851111
19.983514	1389.433610	11.856115
19.699007	1379.120724	11.861120
19.448860	1378.582955	11.866125
19.475281	1363.174685	11.871130
19.083173	1374.442825	11.876135
19.250817	1375.421485	11.881139
19.099027	1388.617817	11.886144
19.145380	1386.102457	11.891149
19.515472	1386.795743	11.896154
18.982264	1393.025081	11.901159
18.868601	1407.563738	11.906163
19.300607	1426.583569	11.911168
19.567932	1432.402107	11.916173
19.845042	1438.934250	11.921178
19.727288	1451.821634	11.926183
19.757715	1453.412788	11.931187
19.963373	1467.761748	11.936192
19.785430	1460.829710	11.941197
20.218401	1457.566322	11.946202
20.004634	1458.774597	11.951207
19.652306	1450.297816	11.956211
20.163664	1462.028894	11.961216
19.988070	1485.337694	11.966221
20.948258	1486.647067	11.971226
20.236252	1491.920623	11.976231
20.696954	1487.973507	11.981235
21.025467	1490.955573	11.986240
20.453105	1475.441825	11.991245
20.509466	1464.973725	11.996250
20.730140	1479.641840	12.001255
20.885449	1494.185778	12.006259
21.015055	1481.353593	12.011264
20.974430	1473.976809	12.016269
21.247408	1464.985032	12.021274
20.413258	1459.886211	12.026279
20.662013	1458.438272	12.031283
20.583522	1464.219795	12.036288
20.482001	1485.192410	12.041293
20.885090	1481.710713	12.046298
20.996911	1492.781217	12.051303
20.693157	1494.646785	12.056307
20.984626	1494.643799	12.061312
21.147963	1496.865084	12.066317
21.251972	1481.163913	12.071322
20.942491	1470.400498	12.076327
20.747900	1464.820167	12.081331
21.043004	1458.349407	12.086336
20.848522	1465.740466	12.091341
21.053173	1454.545481	12.096346
20.829856	1463.012828	12.101351
20.922130	1459.006122	12.106355
21.115865	1458.741990	12.111360
21.270756	1464.949696	12.116365
20.804670	1449.888686	12.121370
20.634889	1460.705862	12.126375
20.496054	1455.552565	12.131379
20.805228	1456.757234	12.136384
20.663613	1452.612205	12.141389
21.112982	1455.423144	12.146394
20.680064	1474.693175	12.151399
20.806006	1475.581489	12.156403
20.985234	1472.147650	12.161408
20.871397	1474.133026	12.166413
20.579280	1464.454169	12.171418
20.603211	1469.480350	12.176423
20.795244	1466.027737	12.181427
21.402823	1466.701625	12.186432
20.836762	1474.158766	12.191437
20.895450	1460.163988	12.196442
21.048867	1464.278994	12.201447
20.831424	1463.847723	12.206451
20.779502	1471.505667	12.211456
20.742762	1471.697510	12.216461
21.034294	1472.240450	12.221466
20.759463	1467.448765	12.226471
20.851192	1458.178586	12.231475
20.982795	1461.864294	12.236480
20.743174	1469.083879	12.241485
20.749160	1467.338475	12.246490
20.796744	1471.770453	12.251495
21.177969	1466.334164	12.256499
20.760501	1468.121328	12.261504
20.723066	1471.770493	12.266509
20.777241	1465.574729	12.271514
20.695138	1473.624701	12.276519
20.909739	1470.422041	12.281523
21.047830	1466.839331	12.286528
21.007812	1472.960850	12.291533
21.380119	1470.144057	12.296538
20.915848	1474.920383	12.301543
20.999475	1475.684105	12.306547
21.329330	1467.663524	12.311552
21.125625	1461.795012	12.316557
20.785410	1443.450232	12.321562
20.754369	1446.223535	12.326567
20.401180	1439.849330	12.331571
20.808423	1447.854073	12.336576
20.665490	1451.153022	12.341581
20.881464	1460.767976	12.346586
21.202075	1471.398445	12.351591
20.950221	1454.379856	12.356595
20.821865	1446.483639	12.361600
20.727964	1453.186377	12.366605
20.949381	1440.456907	12.371610
20.560082	1449.385348	12.376615
20.466089	1445.334001	12.381619
20.969546	1459.909796	12.386624
20.895788	1473.739022	12.391629
20.788166	1465.346596	12.396634
21.131768	1467.893426	12.401639
21.127008	1458.400968	12.406643
21.000680	1452.559062	12.411648
20.875352	1453.372031	12.416653
21.102444	1446.461346	12.421658
20.733649	1453.319377	12.426663
20.910300	1450.426000	12.431667
21.039327	1452.086304	12.436672
21.126059	1455.835363	12.441677
20.938503	1446.804923	12.446682
21.128709	1458.298159	12.451687
21.542827	1452.686099	12.456691
21.308370	1450.477435	12.461696
20.788097	1435.338490	12.466701
21.342884	1419.399035	12.471706
20.636645	1427.148222	12.476711
20.639864	1423.186400	12.481715
20.761747	1417.409715	12.486720
20.657782	1427.665702	12.491725
21.018478	1418.090872	12.496730
21.168799	1421.289402	12.501735
21.279455	1416.505062	12.506739
21.370268	1419.516026	12.511744
20.948856	1423.754054	12.516749
20.965304	1420.574720	12.521754
20.687115	1425.036093	12.526759
20.835239	1427.717882	12.531763
21.008436	1419.486153	12.536768
20.902075	1423.599899	12.541773
20.860659	1418.543203	12.546778
20.908273	1423.730313	12.551783
20.999809	1421.801294	12.556787
20.928688	1417.857746	12.561792
20.727977	1425.396305	12.566797
20.949083	1416.181734	12.571802
21.174606	1422.862851	12.576807
20.857892	1409.281833	12.581811
21.008783	1402.004881	12.586816
20.740060	1403.016517	12.591821
20.669253	1391.069050	12.596826
20.755768	1405.878918	12.601831
20.780054	1416.774898	12.606835
20.968299	1421.305511	12.611840
20.761692	1423.199810	12.616845
21.174368	1411.921029	12.621850
20.785839	1400.618966	12.626855
20.613621	1398.307662	12.631859
20.685689	1401.686188	12.636864
20.756315	1427.754990	12.641869
20.984259	1423.077647	12.646874
20.760184	1433.655423	12.651879
20.754606	1433.251382	12.656883
20.852865	1432.030570	12.661888
20.633628	1438.642684	12.666893
21.151339	1435.625304	12.671898
21.186464	1431.862093	12.676903
21.019241	1425.024552	12.681907
20.862377	1414.506199	12.686912
20.370362	1414.064374	12.691917
20.662504	1405.831996	12.696922
20.778670	1427.139061	12.701927
20.710003	1427.327694	12.706931
20.963224	1426.003732	12.711936
20.671932	1443.428871	12.716941
20.973583	1436.810151	12.721946
20.656142	1432.980281	12.726951
20.683780	1435.913262	12.731955
20.896774	1434.024604	12.736960
20.345664	1439.175817	12.741965
20.443661	1441.875677	12.746970
20.302588	1448.283730	12.751975
20.759534	1438.331980	12.756979
20.975303	1433.199210	12.761984
20.892636	1436.657564	12.766989
20.637265	1435.862129	12.771994
20.766931	1435.913728	12.776999
20.703775	1434.800725	12.782003
20.669291	1434.619146	12.787008
20.611091	1440.735479	12.792013
20.922510	1446.548435	12.797018
20.771990	1455.255145	12.802023
21.028559	1463.435734	12.807027
20.786650	1446.888750	12.812032
20.717621	1455.794652	12.817037
21.283876	1444.588203	12.822042
20.923997	1447.065772	12.827047
21.284600	1442.759636	12.832051
21.079847	1439.279137	12.837056
21.243006	1438.246544	12.842061
21.058792	1435.526360	12.847066
21.115266	1444.430474	12.852071
20.748519	1442.898195	12.857075
20.949838	1435.949301	12.862080
20.527149	1444.688064	12.867085
20.717017	1439.710131	12.872090
20.864847	1440.435606	12.877095
20.852343	1438.989831	12.882099
21.161790	1439.302323	12.887104
20.782789	1446.884094	12.892109
20.854182	1438.470067	12.897114
21.015304	1445.009074	12.902119
20.912782	1443.626496	12.907123
21.000400	1445.072446	12.912128
20.785532	1447.466730	12.917133
21.209223	1440.966825	12.922138
20.620158	1423.686736	12.927143
20.725047	1440.773937	12.932147
20.750738	1441.211662	12.937152
20.625598	1448.948860	12.942157
20.998017	1449.004628	12.947162
20.949738	1450.982314	12.952167
20.951918	1446.512229	12.957171
20.818719	1438.425394	12.962176
20.620920	1449.402503	12.967181
20.952698	1445.034595	12.972186
20.762382	1446.915051	12.977191
20.641250	1446.175944	12.982195
21.003254	1449.517401	12.987200
20.940120	1448.850852	12.992205
20.942526	1448.525181	12.997210
20.831273	1444.031913	13.002215
21.123386	1455.708601	13.007219
20.576995	1429.840169	13.012224
20.684354	1442.225120	13.017229
20.921751	1446.773761	13.022234
21.042727	1447.658188	13.027239
20.971370	1441.828571	13.032243
20.834141	1424.470222	13.037248
20.771525	1427.824080	13.042253
20.665059	1420.884542	13.047258
20.928680	1432.798604	13.052263
20.972157	1442.331804	13.057267
21.112607	1422.520258	13.062272
20.936830	1428.644114	13.067277
21.070253	1421.561995	13.072282
21.315984	1424.858249	13.077287
20.861199	1421.831160	13.082291
20.862075	1427.187341	13.087296
20.778323	1429.085050	13.092301
20.891147	1416.528170	13.097306
21.032582	1423.899906	13.102311
20.618226	1421.933675	13.107315
20.873102	1421.625113	13.112320
20.561039	1421.823503	13.117325
20.694164	1424.324306	13.122330
20.541218	1425.331488	13.127335
20.507411	1418.357388	13.132339
20.813459	1418.852046	13.137344
20.949248	1425.646446	13.142349
20.883090	1424.275794	13.147354
20.913196	1428.917604	13.152359
20.700383	1425.155457	13.157363
20.878911	1429.349835	13.162368
20.648458	1428.767239	13.167373
20.864821	1422.573291	13.172378
21.376155	1426.656527	13.177383
20.762257	1429.379756	13.182387
20.749075	1428.481612	13.187392
20.974278	1430.841889	13.192397
20.998870	1427.496943	13.197402
21.117353	1429.596038	13.202407
20.633460	1425.015478	13.207411
20.941697	1423.795376	13.212416
20.901558	1430.259934	13.217421
20.894997	1434.709475	13.222426
20.883559	1440.300277	13.227431
20.696979	1439.883453	13.232435
20.940345	1438.593154	13.237440
20.712062	1441.610675	13.242445
20.967135	1435.076918	13.247450
21.021139	1433.305916	13.252455
20.776954	1435.265476	13.257459
20.846397	1426.281776	13.262464
20.781037	1435.717182	13.267469
20.704300	1433.233578	13.272474
20.849530	1435.174925	13.277479
20.704275	1439.428373	13.282483
20.762037	1433.724651	13.287488
20.643809	1439.480214	13.292493
20.991720	1428.770303	13.297498
21.114278	1428.859043	13.302503
20.640926	1436.984367	13.307507
20.975614	1429.007978	13.312512
20.959587	1429.697204	13.317517
20.851043	1439.362653	13.322522
21.144301	1442.895900	13.327527
20.856879	1438.277703	13.332531
21.102919	1438.702912	13.337536
20.681817	1444.875153	13.342541
20.876954	1441.206876	13.347546
20.678780	1445.861778	13.352551
20.578154	1443.369241	13.357555
21.173635	1439.303105	13.362560
21.274979	1447.024365	13.367565
21.112117	1441.910325	13.372570
21.142871	1447.331260	13.377575
21.068009	1431.275139	13.382579
21.247810	1416.560537	13.387584
20.883023	1416.062160	13.392589
21.087815	1413.304099	13.397594
21.061666	1407.542930	13.402599
21.153503	1412.367577	13.407603
21.186664	1405.970961	13.412608
20.532851	1410.702395	13.417613
20.498779	1398.522435	13.422618
20.822650	1410.299830	13.427623
20.612098	1407.437716	13.432627
21.122564	1408.830111	13.437632
21.278868	1409.532421	13.442637
21.077142	1402.427246	13.447642
20.983379	1412.445416	13.452647
20.965356	1410.871902	13.457651
21.264793	1401.681015	13.462656
20.749016	1401.675511	13.467661
21.103350	1395.011460	13.472666
20.955022	1387.740422	13.477671
20.683645	1378.035562	13.482675
20.702819	1370.405411	13.487680
20.614016	1382.839343	13.492685
21.013750	1387.806985	13.497690
21.014343	1381.736102	13.502695
20.793125	1375.490485	13.507699
20.465946	1377.605982	13.512704
20.606713	1387.110230	13.517709
20.898073	1390.795767	13.522714
20.509214	1404.344608	13.527719
20.443253	1402.194695	13.532723
20.921482	1397.002725	13.537728
20.763551	1406.204111	13.542733
20.761419	1406.506076	13.547738
20.768335	1404.151031	13.552743
20.707908	1408.995072	13.557747
21.054976	1400.364849	13.562752
20.662031	1411.133015	13.567757
20.847102	1407.977275	13.572762
21.064801	1413.216536	13.577767
20.973718	1421.895668	13.582771
21.256480	1402.246068	13.587776
20.511705	1415.678701	13.592781
20.563207	1414.173400	13.597786
20.922544	1406.177006	13.602791
20.730920	1416.926844	13.607795
20.898828	1406.615319	13.612800
20.832263	1407.462818	13.617805
21.027778	1413.633932	13.622810
20.943391	1412.169299	13.627815
20.783357	1412.702421	13.632819
21.066224	1406.349836	13.637824
20.772779	1416.464220	13.642829
20.660882	1416.951588	13.647834
21.087472	1415.829618	13.652839
21.053527	1420.920182	13.657843
21.619710	1422.959094	13.662848
20.730845	1407.524548	13.667853
21.025915	1399.662337	13.672858
20.865477	1390.395565	13.677863
20.480986	1391.398628	13.682867
20.896487	1385.932015	13.687872
20.776008	1393.175349	13.692877
20.594914	1390.695038	13.697882
20.676035	1403.264066	13.702887
20.801766	1416.647318	13.707891
21.050830	1416.496073	13.712896
20.986320	1426.404628	13.717901
20.488129	1411.930227	13.722906
20.592724	1421.613991	13.727911
20.615448	1421.741164	13.732915
21.102291	1424.964103	13.737920
20.972054	1431.613455	13.742925
21.191587	1423.660365	13.747930
21.078301	1411.675560	13.752935
20.668957	1407.240912	13.757939
20.617344	1400.332242	13.762944
20.404791	1419.566792	13.767949
20.727552	1420.049900	13.772954
20.704694	1428.524702	13.777959
20.630755	1422.123547	13.782963
20.967069	1421.135874	13.787968
20.712324	1431.886676	13.792973
20.812264	1424.914904	13.797978
20.970677	1424.823413	13.802983
21.208347	1427.037469	13.807987
21.104969	1416.860480	13.812992
20.785198	1434.662738	13.817997
20.784079	1426.540632	13.823002
20.845287	1422.504918	13.828007
20.640823	1427.719459	13.833011
21.257446	1420.616074	13.838016
20.869758	1428.063927	13.843021
21.040146	1422.325504	13.848026
20.999224	1408.029290	13.853031
20.834014	1400.866143	13.858035
20.943042	1392.459504	13.863040
20.942743	1406.163178	13.868045
21.037763	1399.435820	13.873050
21.418369	1386.128035	13.878055
21.000688	1398.649158	13.883059
21.223213	1391.290059	13.888064
20.937688	1398.056024	13.893069
20.798318	1407.328046	13.898074
20.638593	1395.379637	13.903079
20.845566	1394.282296	13.908083
21.021378	1389.616665	13.913088
20.566558	1397.856821	13.918093
20.830301	1396.769484	13.923098
20.952498	1395.321539	13.928103
20.562088	1401.769560	13.933107
20.867077	1389.932139	13.938112
20.848335	1394.733897	13.943117
20.868874	1390.482527	13.948122
20.648949	1398.457010	13.953127
20.591767	1405.433307	13.958131
21.043342	1386.479931	13.963136
20.600498	1400.924624	13.968141
20.685140	1396.946874	13.973146
20.687562	1389.867099	13.978151
20.624741	1394.173113	13.983155
21.260744	1398.235360	13.988160
21.141404	1402.951734	13.993165
21.264590	1393.919758	13.998170
21.482009	1401.505829	14.003175
21.285945	1393.511508	14.008179
21.067943	1379.027782	14.013184
20.513148	1374.224521	14.018189
20.732747	1368.599069	14.023207
20.798758	1376.554667	14.028224
21.067204	1380.749218	14.033242
20.908430	1374.397889	14.038259
20.762358	1369.733917	14.043277
20.667549	1387.106968	14.048295
20.626879	1392.117980	14.053312
20.729165	1400.398899	14.058330
20.844720	1395.604620	14.063347
20.417987	1395.783715	14.068365
20.736291	1396.178409	14.073383
20.783398	1403.374589	14.078400
20.793339	1407.921373	14.083418
20.880662	1398.286973	14.088435
20.944791	1417.082553	14.093453
20.997106	1427.414381	14.098471
21.220535	1428.389965	14.103488
21.037751	1433.331254	14.108506
21.398436	1428.156320	14.113523
21.243179	1434.852906	14.118541
21.149293	1435.966369	14.123559
21.392958	1431.848215	14.128576
20.995400	1435.437214	14.133594
21.456626	1435.799136	14.138611
21.147460	1438.565026	14.143629
21.187628	1429.750190	14.148647
21.303405	1433.888245	14.153664
21.141532	1439.102749	14.158682
21.261816	1426.665157	14.163699
20.852385	1436.100078	14.168717
20.923768	1431.761438	14.173735
20.839013	1425.272189	14.178752
21.424740	1433.854526	14.183770
21.500450	1426.315221	14.188787
21.377745	1425.395629	14.193805
21.670931	1428.696099	14.198823
21.736211	1435.523000	14.203840
21.680670	1432.066837	14.208858
21.787445	1438.180649	14.213875
21.568131	1440.624804	14.218893
21.383714	1435.417331	14.223911
21.682588	1430.101011	14.228928
21.178100	1440.229859	14.233946
21.494536	1435.467667	14.238963
21.577243	1443.373188	14.243981
21.518851	1434.170482	14.248999
21.600818	1436.166484	14.254016
21.234815	1443.236643	14.259034
21.735353	1450.186974	14.264051
21.507049	1468.172039	14.269069
21.321494	1467.722715	14.274087
21.586245	1465.692882	14.279104
21.421701	1475.592977	14.284122
21.758051	1471.178972	14.289139
21.512660	1470.152446	14.294157
21.553132	1468.068143	14.299175
21.647623	1462.912064	14.304192
21.333864	1476.949972	14.309210
21.622343	1479.234621	14.314227
21.832353	1495.110892	14.319245
21.661212	1498.708728	14.324263
22.089680	1494.856934	14.329280
21.592128	1498.470966	14.334298
22.042583	1501.572029	14.339315
22.018905	1503.048695	14.344333
22.042688	1504.360515	14.349351
22.124896	1498.800976	14.354368
21.968502	1511.691346	14.359386
21.812591	1505.954892	14.364403
22.029208	1508.946033	14.369421
21.927388	1508.338241	14.374439
21.968998	1514.436482	14.379456
21.879516	1510.954227	14.384474
22.252187	1508.873992	14.389491
21.905682	1509.408268	14.394509
21.738237	1514.916302	14.399527
22.370567	1528.632579	14.404544
22.131441	1537.446960	14.409562
22.484401	1539.825692	14.414579
22.390233	1543.602880	14.419597
22.623194	1532.057794	14.424615
22.934231	1517.103697	14.429632
22.919737	1516.649061	14.434650
22.945369	1505.891589	14.439667
22.822341	1514.087170	14.444685
22.163987	1519.414780	14.449703
22.596908	1503.545217	14.454720
22.458768	1509.710499	14.459738
22.482865	1507.990454	14.464755
22.408409	1511.780398	14.469773
22.246552	1508.820449	14.474791
22.431098	1510.231097	14.479808
22.225891	1515.269179	14.484826
22.234424	1503.732668	14.489843
22.423632	1510.543472	14.494861
22.403436	1513.294085	14.499879
23.048725	1505.143646	14.504896
22.812525	1508.084458	14.509914
23.043066	1506.597943	14.514931
23.204113	1506.541994	14.519949
22.843853	1514.652253	14.524967
22.933246	1505.237534	14.529984
22.657027	1518.159085	14.535002
22.921542	1511.376426	14.540019
23.008627	1504.820276	14.545037
22.475350	1499.280035	14.550055
22.992512	1501.662106	14.555072
22.692421	1506.173090	14.560090
22.898160	1501.837775	14.565107
22.936659	1512.171634	14.570125
22.643869	1508.495868	14.575143
22.791373	1507.068476	14.580160
22.326514	1510.039044	14.585178
22.465502	1508.410335	14.590195
22.829912	1501.751513	14.595213
22.604269	1511.867247	14.600231
22.976627	1509.304731	14.605248
22.849933	1518.261259	14.610266
22.878944	1511.650488	14.615283
23.188243	1508.119155	14.620301
22.490713	1513.841316	14.625319
22.980083	1524.777084	14.630336
23.242294	1540.819667	14.635354
23.312856	1543.957523	14.640371
23.484588	1543.212662	14.645389
22.801697	1529.468449	14.650407
23.213281	1527.234279	14.655424
23.178792	1542.055554	14.660442
23.072092	1545.005669	14.665459
23.267777	1541.683198	14.670477
23.003113	1552.597071	14.675495
22.823963	1545.638078	14.680512
23.227360	1550.535598	14.685530
23.021639	1544.366284	14.690547
22.972129	1540.240882	14.695565
22.924625	1545.539760	14.700583
22.879983	1552.893881	14.705600
22.886942	1573.144487	14.710618
23.047504	1570.626938	14.715635
23.190706	1576.197492	14.720653
23.001231	1580.566683	14.725671
23.235494	1575.199574	14.730688
23.374342	1594.397956	14.735706
23.307790	1606.025618	14.740723
23.857192	1618.366670	14.745741
23.564180	1613.586857	14.750759
23.789910	1611.401867	14.755776
23.557286	1623.304500	14.760794
23.411534	1618.950275	14.765811
23.899933	1617.619560	14.770829
23.659484	1614.532499	14.775847
23.686300	1606.134860	14.780864
23.932805	1606.349330	14.785882
23.550442	1605.761285	14.790899
23.460459	1608.949518	14.795917
23.701785	1613.173587	14.800935
23.710992	1608.286835	14.805952
23.856898	1613.276560	14.810970
23.542902	1610.729728	14.815987
23.966792	1607.111395	14.821005
23.685965	1613.750838	14.826023
23.765363	1616.763558	14.831040
23.668447	1616.714038	14.836058
23.601888	1611.096099	14.841075
23.756404	1607.193994	14.846093
23.665647	1623.219218	14.851111
24.094336	1615.045617	14.856128
23.946732	1632.513828	14.861146
24.048382	1633.769784	14.866163
24.296158	1637.650589	14.871181
24.122509	1636.736175	14.876199
24.162558	1631.778372	14.881216
24.069910	1623.024392	14.886234
24.064701	1622.402788	14.891251
24.246537	1624.726218	14.896269
24.185698	1641.918904	14.901287
24.200651	1634.557651	14.906304
24.052279	1634.493330	14.911322
23.949580	1643.843891	14.916339
24.280382	1637.297085	14.921357
24.402851	1649.995252	14.926375
24.396589	1637.227575	14.931392
24.451560	1639.062071	14.936410
24.497008	1641.582923	14.941427
24.617968	1632.438731	14.946445
24.276077	1650.902980	14.951463
24.371748	1639.327804	14.956480
24.348061	1644.491121	14.961498
24.199513	1649.007268	14.966515
24.350481	1648.086020	14.971533
24.509999	1650.827894	14.976551
24.394772	1653.114456	14.981568
24.442389	1644.680155	14.986586
24.260101	1649.183187	14.991603
24.408342	1645.523121	14.996621
24.162642	1646.236202	15.001639
24.015858	1646.162158	15.006656
24.288104	1657.548678	15.011674
24.713241	1675.532587	15.016691
25.038495	1672.122512	15.021709
24.939445	1680.736165	15.026727
25.398524	1670.625606	15.031744
25.115776	1651.249837	15.036762
25.147034	1646.669170	15.041779
25.156582	1632.636046	15.046797
25.231374	1640.233539	15.051815
25.169040	1637.480149	15.056832
25.531121	1638.034293	15.061850
24.926170	1648.559281	15.066867
25.199057	1634.370362	15.071885
24.918195	1619.806267	15.076903
25.112411	1614.719270	15.081920
25.278239	1611.417260	15.086938
25.066744	1606.801445	15.091955
25.026752	1606.789415	15.096973
25.080757	1610.247875	15.101991
25.180615	1610.865877	15.107008
25.315745	1601.345216	15.112026
24.498797	1620.368098	15.117043
24.818367	1614.861925	15.122061
24.976171	1626.912605	15.127079
25.405197	1636.130258	15.132096
24.997053	1631.616270	15.137114
24.827254	1633.974791	15.142131
25.173014	1633.529652	15.147149
24.763963	1638.060536	15.152167
24.717576	1637.510566	15.157184
25.335536	1639.781272	15.162202
25.039110	1641.289359	15.167219
25.153109	1635.180953	15.172237
24.983313	1647.921353	15.177255
25.394230	1663.484578	15.182272
25.633488	1668.611088	15.187290
25.513170	1677.331547	15.192307
25.752093	1666.825616	15.197325
25.275472	1652.610445	15.202343
24.969826	1665.691511	15.207360
25.389901	1659.708196	15.212378
25.202047	1672.324138	15.217395
25.433013	1666.363401	15.222413
25.605019	1672.717724	15.227431
25.859290	1672.034304	15.232448
25.916404	1666.947960	15.237466
25.762539	1669.610875	15.242483
26.084623	1679.953710	15.247501
25.893777	1680.803074	15.252519
25.666552	1687.237272	15.257536
26.278904	1671.962044	15.262554
26.091668	1671.176743	15.267571
26.062520	1641.152751	15.272589
25.379509	1640.675708	15.277607
25.591521	1649.851828	15.282624
25.787039	1670.596669	15.287642
25.487022	1677.383540	15.292659
25.487766	1672.058011	15.297677
25.452520	1673.961922	15.302695
25.594157	1674.556226	15.307712
25.844142	1678.290584	15.312730
25.642354	1683.254502	15.317747
25.766718	1698.035694	15.322765
26.091071	1707.178411	15.327783
25.925299	1713.661146	15.332800
26.227049	1700.004289	15.337818
26.032783	1712.426459	15.342835
26.394213	1700.227652	15.347853
26.296915	1708.263787	15.352871
26.191604	1708.947682	15.357888
26.445664	1707.147237	15.362906
25.970344	1715.085571	15.367923
26.067519	1706.666365	15.372941
25.837932	1712.044949	15.377959
26.194070	1713.136791	15.382976
26.311953	1709.774075	15.387994
25.899588	1710.852388	15.393011
26.064034	1709.965838	15.398029
26.503162	1711.712034	15.403047
26.049345	1716.153360	15.408064
26.453486	1713.383764	15.413082
26.258032	1716.740907	15.418099
26.353423	1736.271755	15.423117
26.689910	1742.210852	15.428135
26.545506	1746.516843	15.433152
26.513824	1740.146331	15.438170
26.465938	1744.423961	15.443187
26.488017	1741.766329	15.448205
27.036187	1735.695267	15.453223
26.652754	1748.223923	15.458240
26.848032	1748.241642	15.463258
26.969884	1738.066797	15.468275
27.224793	1714.688065	15.473293
27.068534	1706.434766	15.478311
26.814421	1701.194267	15.483328
26.521213	1693.188498	15.488346
26.675735	1707.338077	15.493363
26.875468	1700.924360	15.498381
26.893262	1693.254683	15.503399
26.746341	1695.461242	15.508416
27.000061	1688.585860	15.513434
26.855125	1701.846905	15.518451
26.659785	1697.200338	15.523469
27.105249	1709.961692	15.528487
26.889242	1712.020237	15.533504
27.292503	1713.942681	15.538522
26.985050	1711.060812	15.543539
27.212876	1702.510927	15.548557
27.187992	1699.740473	15.553575
27.195081	1695.667538	15.558592
26.892171	1693.731854	15.563610
27.144370	1704.819449	15.568627
27.064225	1718.984468	15.573645
27.267607	1732.451204	15.578663
26.989558	1738.548032	15.583680
26.951877	1731.357983	15.588698
26.971932	1739.757129	15.593715
27.732240	1747.515520	15.598733
27.816822	1737.086011	15.603751
27.619024	1746.067853	15.608768
27.768888	1734.838870	15.613786
27.374754	1722.352218	15.618803
27.583057	1720.052471	15.623821
27.620693	1708.844717	15.628839
27.624473	1711.701896	15.633856
27.604757	1702.380578	15.638874
27.118331	1705.090675	15.643891
27.161494	1711.713591	15.648909
27.575974	1721.887050	15.653927
27.611649	1734.903746	15.658944
27.570345	1737.517843	15.663962
27.515825	1742.738847	15.668979
27.438458	1737.673962	15.673997
27.554198	1736.441389	15.679015
27.310706	1747.064330	15.684032
27.460278	1738.674316	15.689050
27.508714	1744.660046	15.694067
27.691548	1742.919058	15.699085
27.512848	1742.301602	15.704103
27.395425	1750.629038	15.709120
27.669307	1753.632458	15.714138
27.775407	1766.047271	15.719155
27.990597	1764.500364	15.724173
28.024636	1762.896710	15.729191
27.581889	1763.182896	15.734208
27.919713	1765.342578	15.739226
27.892475	1763.742343	15.744243
27.794452	1762.809835	15.749261
28.255856	1757.656113	15.754279
27.925994	1760.920154	15.759296
27.617778	1757.593472	15.764314
28.156864	1764.493236	15.769331
27.980076	1766.571051	15.774349
28.394241	1777.064324	15.779367
28.275916	1770.298763	15.784384
28.263003	1762.653611	15.789402
28.133127	1767.956844	15.794419
28.087162	1778.431359	15.799437
28.392147	1787.363639	15.804455
28.385392	1797.873182	15.809472
28.398212	1793.106240	15.814490
28.364425	1807.021234	15.819507
28.521770	1799.959153	15.824525
28.290483	1794.964345	15.829543
28.307311	1802.180075	15.834560
28.528747	1803.314313	15.839578
28.483829	1800.537827	15.844595
28.486340	1800.523629	15.849613
28.449093	1798.429376	15.854631
28.383152	1792.350185	15.859648
28.685463	1795.908257	15.864666
28.705412	1799.354091	15.869683
28.692244	1802.321687	15.874701
28.442373	1799.917390	15.879719
28.392464	1804.384776	15.884736
28.750896	1796.894076	15.889754
28.332162	1800.103275	15.894771
28.568395	1799.751723	15.899789
28.434619	1807.766994	15.904807
28.435356	1824.822930	15.909824
28.728749	1834.221455	15.914842
28.799940	1829.379526	15.919859
28.974409	1831.208125	15.924877
29.058345	1829.746322	15.929895
28.780462	1831.912354	15.934912
29.206834	1828.707771	15.939930
28.957361	1831.930087	15.944947
28.784152	1834.495941	15.949965
28.869356	1826.639423	15.954983
28.718741	1825.172160	15.960000
28.966199	1834.500205	15.965018
29.077286	1838.880541	15.970035
29.204778	1858.034337	15.975053
29.953213	1850.241675	15.980071
29.280594	1838.950066	15.985088
29.385928	1826.641114	15.990106
29.486892	1821.271576	15.995123
29.322286	1822.626748	16.000141
29.087664	1826.997841	16.005159
29.131640	1828.714939	16.010176
29.214812	1826.014530	16.015194
29.389894	1830.589429	16.020211
29.504278	1843.078483	16.025229
29.739749	1841.966729	16.030247
29.088509	1835.835885	16.035264
29.598855	1851.451944	16.040282
29.513154	1854.859205	16.045299
29.188555	1865.963515	16.050317
29.836639	1854.736043	16.055335
29.624223	1859.977465	16.060352
29.583718	1864.895281	16.065370
29.359295	1861.323866	16.070387
29.145535	1866.045375	16.075405
29.616478	1860.985665	16.080423
29.091097	1870.776595	16.085440
29.515341	1875.750576	16.090458
29.858024	1871.193623	16.095475
29.997742	1884.767481	16.100493
30.406726	1881.066986	16.105511
30.344091	1877.648166	16.110528
30.214512	1862.844100	16.115546
30.134387	1860.038595	16.120563
30.261164	1864.297730	16.125581
30.448978	1853.738619	16.130599
30.368645	1865.149911	16.135616
30.245418	1862.612853	16.140634
30.516500	1851.010990	16.145651
30.249167	1849.493649	16.150669
30.438097	1831.649194	16.155687
30.177942	1820.374686	16.160704
29.938493	1818.475355	16.165722
30.273616	1822.817275	16.170739
29.977692	1827.865498	16.175757
30.439984	1836.716104	16.180775
30.678950	1851.562842	16.185792
30.342624	1829.139355	16.190810
30.408796	1816.242957	16.195827
29.895695	1825.960091	16.200845
30.238054	1830.203122	16.205863
30.393409	1845.334696	16.210880
30.182494	1848.939037	16.215898
30.220374	1843.434226	16.220915
30.275550	1848.956577	16.225933
30.442085	1853.219916	16.230951
30.176691	1857.232469	16.235968
30.307673	1846.971332	16.240986
30.345623	1851.587467	16.246003
30.433132	1872.198713	16.251021
30.532763	1871.886330	16.256039
30.762005	1884.369112	16.261056
30.641420	1875.911156	16.266074
30.753047	1875.320697	16.271091
30.699938	1890.226999	16.276109
30.674574	1889.301714	16.281127
30.714487	1889.826448	16.286144
30.880221	1886.034964	16.291162
30.693894	1876.833458	16.296179
30.986270	1887.619375	16.301197
31.328319	1883.867356	16.306215
31.168126	1875.977287	16.311232
31.336042	1881.824852	16.316250
31.279061	1884.379842	16.321267
30.760608	1887.021435	16.326285
31.108927	1872.650843	16.331303
31.006738	1879.784245	16.336320
30.450458	1887.007319	16.341338
30.881609	1878.645734	16.346355
31.155201	1883.537266	16.351373
30.999109	1872.148410	16.356391
31.051740	1883.445174	16.361408
30.828225	1897.988918	16.366426
31.243409	1906.151094	16.371443
31.066616	1919.736724	16.376461
31.361239	1919.927200	16.381479
31.177413	1924.194323	16.386496
30.962514	1922.648297	16.391514
31.389710	1921.399715	16.396531
31.007853	1928.967361	16.401549
31.463936	1920.544385	16.406567
31.371409	1924.864762	16.411584
31.428828	1941.529166	16.416602
31.558270	1947.505022	16.421619
31.518534	1954.134772	16.426637
31.879420	1951.246551	16.431655
31.901055	1954.694493	16.436672
31.282486	1954.818674	16.441690
31.482447	1954.460345	16.446707
31.513426	1953.820317	16.451725
31.805648	1945.186808	16.456743
31.731851	1949.250403	16.461760
31.840815	1945.345393	16.466778
32.091657	1951.790658	16.471795
31.663830	1957.098182	16.476813
31.868256	1947.737894	16.481831
31.988400	1943.832937	16.486848
31.607019	1956.271237	16.491866
31.949186	1947.387793	16.496883
32.000021	1951.019729	16.501901
32.262198	1959.145954	16.506919
32.201157	1952.512244	16.511936
32.218896	1948.760294	16.516954
32.189533	1940.312257	16.521971
31.968852	1953.597133	16.526989
32.024476	1951.889746	16.532007
32.333988	1964.201327	16.537024
32.069947	1974.628706	16.542042
32.389517	1979.530498	16.547059
32.372610	1983.850526	16.552077
32.134605	1981.675693	16.557095
32.451813	1981.527606	16.562112
32.275359	1981.653949	16.567130
32.399375	1973.480031	16.572147
32.114809	1984.324770	16.577165
32.482782	1972.457748	16.582183
32.497463	1968.865394	16.587200
32.139757	1982.025735	16.592218
32.346576	1970.637980	16.597235
32.772228	1981.322361	16.602253
32.593261	1985.893826	16.607271
32.663439	1980.512581	16.612288
32.633114	1985.345214	16.617306
32.653962	1975.925427	16.622323
33.044543	1996.122620	16.627341
32.938177	1994.563097	16.632359
33.228482	1981.485990	16.637376
32.844429	1983.107965	16.642394
33.177236	1974.988418	16.647411
33.048644	1977.540739	16.652429
32.770412	1976.869461	16.657447
33.187220	1972.989234	16.662464
32.709580	1978.024165	16.667482
32.864009	1972.668247	16.672499
32.829285	1990.398642	16.677517
32.698606	1998.831252	16.682535
33.184872	2007.324255	16.687552
32.795406	2019.544669	16.692570
32.775871	2012.343898	16.697587
33.162630	2014.203059	16.702605
33.078427	2016.137063	16.707623
33.279635	2005.901582	16.712640
33.339872	2017.019949	16.717658
33.102025	2009.650282	16.722675
32.838750	2022.751548	16.727693
33.170914	2029.188415	16.732711
33.332887	2033.337216	16.737728
33.147063	2052.932818	16.742746
33.600253	2037.075781	16.747763
33.329952	2043.243062	16.752781
33.560377	2044.989641	16.757799
33.613041	2045.531095	16.762816
33.437865	2045.796608	16.767834
33.739258	2039.891775	16.772851
33.836012	2043.780463	16.777869
33.731394	2041.170491	16.782887
33.941688	2037.144922	16.787904
33.993901	2036.771365	16.792922
34.247822	2032.482770	16.797939
34.384402	2039.151627	16.802957
34.544521	2037.162105	16.807975
34.405812	2015.731775	16.812992
34.266261	2013.473513	16.818010
34.360919	2002.483363	16.823027
34.348416	2008.598161	16.828045
33.822522	2004.122759	16.833063
33.992704	1995.515266	16.838080
33.859854	1998.126202	16.843098
34.024671	1998.925628	16.848115
33.989529	1998.752902	16.853133
33.607575	2002.305489	16.858151
33.857854	1999.857934	16.863168
33.838287	2010.764752	16.868186
33.971180	2024.936833	16.873203
34.364616	2026.111293	16.878221
34.020034	2031.845181	16.883239
34.193634	2033.240429	16.888256
34.264670	2038.703033	16.893274
34.342685	2028.959591	16.898291
34.301853	2034.371679	16.903309
34.423928	2036.012408	16.908327
34.214746	2036.822802	16.913344
33.961385	2048.803732	16.918362
34.178319	2055.332029	16.923379
34.513684	2063.954886	16.928397
34.606265	2069.533903	16.933415
34.760333	2071.439661	16.938432
34.194242	2069.858150	16.943450
34.442154	2065.726503	16.948467
34.417098	2056.823665	16.953485
34.589915	2079.061335	16.958503
34.738448	2099.100526	16.963520
34.751020	2114.684067	16.968538
35.023334	2103.783088	16.973555
35.048851	2100.073476	16.978573
34.700657	2104.884256	16.983591
35.078337	2096.695921	16.988608
35.009595	2108.920085	16.993626
35.004635	2104.406133	16.998643
35.261240	2112.353052	17.003661
35.346150	2101.589733	17.008679
35.656956	2095.650977	17.013696
35.669339	2106.406694	17.018714
35.544331	2092.020978	17.023731
35.570525	2076.418239	17.028749
35.442552	2073.075941	17.033767
35.183074	2067.635029	17.038784
35.227469	2069.837976	17.043802
34.906825	2079.250182	17.048819
34.761585	2090.086463	17.053837
34.788940	2097.492677	17.058855
35.033270	2104.702223	17.063872
35.150274	2104.278180	17.068890
34.884143	2105.401928	17.073907
35.660796	2121.051350	17.078925
35.504234	2143.447568	17.083943
35.545160	2139.081667	17.088960
35.778072	2133.230672	17.093978
35.523627	2137.261499	17.098995
35.724508	2142.867256	17.104013
35.396209	2135.909157	17.109031
35.602526	2134.077475	17.114048
35.541423	2137.124623	17.119066
35.471835	2148.872910	17.124083
35.972298	2135.707273	17.129101
35.455991	2147.060428	17.134119
35.822342	2146.132150	17.139136
35.985752	2164.567461	17.144154
36.006020	2172.006820	17.149171
36.188597	2171.628235	17.154189
35.789393	2179.415935	17.159207
36.009769	2174.181338	17.164224
36.095704	2178.326283	17.169242
36.443575	2167.685574	17.174259
36.491904	2167.764716	17.179277
36.203451	2167.869311	17.184295
36.559990	2159.437681	17.189312
36.541976	2166.711135	17.194330
36.544382	2170.532555	17.199347
36.856886	2155.790230	17.204365
36.203370	2136.447504	17.209383
36.523881	2128.589866	17.214400
36.253670	2143.881713	17.219418
36.773643	2149.100431	17.224435
36.645179	2148.579871	17.229453
36.363567	2161.330014	17.234471
36.580057	2161.185020	17.239488
36.625449	2164.595072	17.244506
36.471977	2163.451936	17.249523
36.760909	2165.090059	17.254541
36.512145	2167.861468	17.259559
36.538375	2166.746585	17.264576
36.755550	2166.683375	17.269594
36.865661	2164.240533	17.274611
36.976676	2165.224021	17.279629
36.529756	2171.476366	17.284647
36.939802	2169.227017	17.289664
36.812765	2168.780238	17.294682
36.755857	2166.428245	17.299699
37.331494	2174.882785	17.304717
36.830118	2167.603115	17.309735
37.044158	2179.640641	17.314752
37.498384	2191.155035	17.319770
37.017512	2183.648186	17.324787
37.378674	2188.190106	17.329805
37.226573	2199.830513	17.334823
37.336217	2196.497850	17.339840
36.931777	2202.147560	17.344858
37.052322	2197.798705	17.349875
36.879801	2193.397720	17.354893
37.009594	2195.971139	17.359911
37.435405	2195.565813	17.364928
37.066977	2197.948235	17.369946
37.136328	2196.698379	17.374963
37.400876	2214.987256	17.379981
37.256716	2227.220899	17.384999
37.527924	2232.064123	17.390016
37.970464	2230.763669	17.395034
37.750032	2233.432579	17.400051
37.588467	2235.920506	17.405069
37.573608	2229.463827	17.410087
37.726295	2228.354035	17.415104
37.905594	2231.985274	17.420122
37.515891	2237.676571	17.425139
37.528393	2230.835616	17.430157
37.522275	2230.791789	17.435175
37.893599	2241.831385	17.440192
38.122693	2247.042519	17.445210
37.986828	2260.609613	17.450227
38.541524	2253.016533	17.455245
38.032632	2247.371432	17.460263
38.365992	2243.382200	17.465280
38.265053	2238.068006	17.470298
38.418288	2240.123163	17.475315
38.414775	2227.822715	17.480333
38.195209	2224.863861	17.485351
38.081136	2228.264254	17.490368
38.189689	2241.288563	17.495386
38.802463	2248.453905	17.500403
38.933270	2249.653723	17.505421
38.658114	2241.431158	17.510439
38.597949	2229.470393	17.515456
38.446473	2228.656880	17.520474
38.359101	2235.706789	17.525491
38.514320	2222.930244	17.530509
38.423869	2231.449403	17.535527
38.396462	2249.439505	17.540544
38.763301	2246.980985	17.545562
38.567496	2259.158143	17.550579
38.564744	2254.973740	17.555597
38.365735	2255.864696	17.560615
38.268874	2261.631797	17.565632
38.884248	2253.033674	17.570650
38.327223	2269.815194	17.575667
39.136653	2268.746366	17.580685
39.547624	2279.007419	17.585703
39.314575	2270.906772	17.590720
39.073536	2266.283620	17.595738
39.147953	2254.481679	17.600755
39.276115	2241.631793	17.605773
39.170681	2249.361285	17.610791
39.075752	2246.127476	17.615808
39.085191	2254.313725	17.620826
38.993622	2272.676327	17.625843
39.161738	2273.918577	17.630861
39.591092	2274.545083	17.635879
39.037682	2283.289337	17.640896
39.538724	2280.928293	17.645914
39.153425	2278.184486	17.650931
39.491726	2278.537584	17.655949
39.551315	2288.404488	17.660967
39.458334	2286.213804	17.665984
39.878283	2281.436369	17.671002
39.485923	2279.480507	17.676019
39.450127	2282.854104	17.681037
39.294007	2279.645741	17.686055
39.298688	2284.654382	17.691072
39.383382	2291.959899	17.696090
39.148062	2312.549107	17.701107
39.504262	2310.393236	17.706125
39.716294	2313.493603	17.711143
39.767481	2312.280716	17.716160
40.033723	2316.663329	17.721178
39.627868	2323.488311	17.726195
39.947186	2338.862765	17.731213
39.602730	2347.104225	17.736231
39.747193	2347.110971	17.741248
40.151336	2353.017439	17.746266
40.123968	2358.803374	17.751283
40.148456	2342.910066	17.756301
39.833516	2348.458642	17.761319
40.510073	2351.202165	17.766336
40.628236	2349.347771	17.771354
40.623891	2352.850657	17.776371
40.606236	2345.516319	17.781389
40.820032	2350.261533	17.786407
40.710785	2358.491810	17.791424
40.825036	2350.739516	17.796442
39.984431	2361.706624	17.801459
40.213926	2355.289115	17.806477
40.472469	2347.686914	17.811495
40.284485	2352.805787	17.816512
40.756794	2368.416285	17.821530
40.451228	2385.009121	17.826547
40.650992	2381.610567	17.831565
41.069227	2387.424067	17.836583
40.772157	2374.523337	17.841600
40.723358	2380.499598	17.846618
40.820591	2385.746774	17.851635
41.258306	2376.108795	17.856653
41.101287	2379.375617	17.861671
40.826212	2380.931694	17.866688
41.146113	2379.125399	17.871706
41.080546	2377.426144	17.876723
41.031878	2378.569328	17.881741
41.188614	2366.372814	17.886759
40.913871	2377.334268	17.891776
41.360957	2371.557507	17.896794
40.715934	2376.872876	17.901811
40.860196	2398.119279	17.906829
41.295466	2407.526508	17.911847
41.363368	2409.275006	17.916864
41.559272	2410.925955	17.921882
41.371736	2415.842376	17.926899
41.779305	2414.007659	17.931917
41.460774	2414.126861	17.936935
41.567400	2414.731529	17.941952
41.621438	2410.477496	17.946970
41.181448	2413.883405	17.951987
41.574880	2413.013472	17.957005
41.665530	2416.569388	17.962023
41.851489	2430.253132	17.967040
42.010521	2428.963469	17.972058
41.896457	2436.021194	17.977075
42.219214	2430.531125	17.982093
42.054354	2412.754937	17.987111
42.130368	2414.198059	17.992128
41.886664	2399.702075	17.997146
42.222276	2409.732001	18.002163
42.316464	2413.201469	18.007181
42.162307	2406.057462	18.012199
41.926524	2425.104916	18.017216
42.414995	2422.308929	18.022234
42.235400	2434.368463	18.027251
42.340553	2439.763930	18.032269
42.394001	2436.563707	18.037287
42.123616	2434.367192	18.042304
42.343143	2438.422361	18.047322
42.317090	2428.470886	18.052339
42.059475	2425.143653	18.057357
42.287018	2433.513109	18.062375
42.149778	2439.410840	18.067392
42.617269	2439.477182	18.072410
42.486862	2466.822155	18.077427
42.826252	2473.685597	18.082445
42.836378	2467.407245	18.087463
42.473524	2473.952432	18.092480
42.696823	2467.018531	18.097498
42.807276	2472.533593	18.102515
42.680457	2468.712981	18.107533
42.672889	2473.902552	18.112551
42.564486	2481.492486	18.117568
43.066346	2462.087508	18.122586
42.672806	2478.848308	18.127603
42.756279	2497.755272	18.132621
43.036327	2497.528500	18.137639
43.022750	2505.429802	18.142656
43.119087	2504.046927	18.147674
42.798988	2503.820671	18.152691
43.255377	2504.570134	18.157709
43.383207	2497.980202	18.162727
42.956513	2499.451243	18.167744
43.407542	2504.008561	18.172762
43.500676	2522.980840	18.177779
43.561678	2533.746233	18.182797
43.855678	2533.316247	18.187815
43.558464	2531.653542	18.192832
43.643441	2527.187838	18.197850
43.809302	2534.570118	18.202867
43.760705	2532.886838	18.207885
44.128565	2526.663683	18.212903
43.565645	2523.106049	18.217920
43.808009	2529.958587	18.222938
43.803996	2531.838346	18.227955
43.600140	2542.620804	18.232973
43.584967	2543.512546	18.237991
43.651475	2544.816341	18.243008
43.998927	2542.984828	18.248026
43.791067	2540.337345	18.253043
43.693745	2541.684191	18.258061
44.065703	2536.441600	18.263079
43.918007	2560.736426	18.268096
44.203052	2566.364919	18.273114
44.227403	2564.583287	18.278131
44.059103	2566.558158	18.283149
44.497444	2560.938760	18.288167
44.086915	2564.920852	18.293184
44.143509	2560.311161	18.298202
44.471174	2571.201756	18.303219
44.191294	2571.081221	18.308237
44.489674	2562.899548	18.313255
44.448299	2580.637262	18.318272
44.739472	2595.839598	18.323290
44.531368	2591.962801	18.328307
44.519134	2608.856035	18.333325
44.588750	2605.132442	18.338343
44.764382	2611.454631	18.343360
44.876588	2602.490541	18.348378
44.885645	2595.594104	18.353395
44.767705	2602.610040	18.358413
45.058970	2599.455639	18.363431
44.679728	2605.572907	18.368448
45.061575	2597.816352	18.373466
44.658865	2597.940537	18.378483
44.625282	2623.369639	18.383501
45.207185	2625.887666	18.388519
45.225518	2635.939846	18.393536
45.227454	2634.240803	18.398554
45.126489	2634.073842	18.403571
44.919559	2636.407375	18.408589
45.294057	2634.353066	18.413607
45.222673	2640.506557	18.418624
45.487633	2637.577170	18.423642
45.799709	2647.160023	18.428659
45.543056	2649.239832	18.433677
45.836278	2652.551585	18.438695
45.604297	2650.489424	18.443712
45.826545	2647.231866	18.448730
45.659354	2644.649059	18.453747
45.714676	2664.181632	18.458765
45.980112	2656.376490	18.463783
45.791874	2666.184528	18.468800
45.929674	2666.385365	18.473818
45.951499	2664.756150	18.478835
45.671224	2672.101579	18.483853
45.766208	2665.579424	18.488871
45.711184	2667.080475	18.493888
45.774276	2665.731637	18.498906
45.935424	2663.957254	18.503923
45.800853	2670.440544	18.508941
45.969962	2687.767421	18.513959
45.978148	2698.971193	18.518976
46.469261	2708.171356	18.523994
46.880314	2697.879366	18.529011
46.507789	2702.443272	18.534029
46.717954	2699.916252	18.539047
46.573125	2692.694911	18.544064
46.621269	2698.811393	18.549082
46.728664	2696.179137	18.554099
46.660199	2701.424901	18.559117
46.854484	2696.589165	18.564135
46.735928	2701.819103	18.569152
46.715338	2704.844451	18.574170
46.297429	2690.436344	18.579187
46.429474	2696.640034	18.584205
46.465454	2693.859363	18.589223
46.395274	2707.136790	18.594240
46.734684	2716.220421	18.599258
46.659879	2721.164075	18.604275
46.661300	2734.788369	18.609293
46.938974	2730.496694	18.614311
46.862665	2725.892415	18.619328
46.686166	2737.410608	18.624346
47.415638	2750.954981	18.629363
47.456182	2761.556290	18.634381
47.828645	2759.876399	18.639399
47.909919	2751.915350	18.644416
47.754837	2738.012632	18.649434
47.965639	2727.331257	18.654451
47.464222	2731.250218	18.659469
47.815260	2719.843103	18.664487
47.691986	2728.224824	18.669504
47.407554	2732.914605	18.674522
47.528263	2723.694612	18.679539
47.503778	2732.142878	18.684557
47.817023	2741.399545	18.689575
47.587214	2748.027565	18.694592
47.986472	2752.575720	18.699610
47.879027	2751.677451	18.704627
48.020075	2755.590224	18.709645
48.274435	2754.663000	18.714663
48.134283	2748.664678	18.719680
47.772077	2754.849174	18.724698
47.960731	2749.437115	18.729715
47.936027	2755.340083	18.734733
48.040449	2753.058786	18.739751
47.672346	2748.201323	18.744768
47.850151	2769.295994	18.749786
48.412839	2778.090941	18.754803
48.399070	2793.474908	18.759821
48.120671	2785.666862	18.764839
48.492086	2786.696313	18.769856
48.158976	2785.870596	18.774874
48.795218	2785.662295	18.779891
48.485336	2788.318282	18.784909
48.981844	2786.796682	18.789927
48.492444	2791.363325	18.794944
48.414488	2790.531664	18.799962
48.587845	2793.755316	18.804979
48.642621	2807.245305	18.809997
48.398531	2815.693465	18.815015
48.393263	2817.716807	18.820032
48.330027	2815.518587	18.825050
48.597905	2822.077848	18.830067
48.777690	2840.493819	18.835085
48.779485	2851.794089	18.840103
48.775569	2857.362760	18.845120
48.759511	2862.309774	18.850138
48.759293	2860.678017	18.855155
48.983220	2877.736601	18.860173
49.177528	2883.257907	18.865191
49.310428	2880.660626	18.870208
49.547005	2881.429681	18.875226
49.629678	2876.303518	18.880243
49.093296	2882.052482	18.885261
49.435145	2872.905532	18.890279
49.505210	2876.813967	18.895296
49.718043	2889.108200	18.900314
49.857301	2904.684979	18.905331
50.046279	2903.741392	18.910349
50.024857	2903.232381	18.915367
50.357703	2894.943033	18.920384
50.065938	2888.203574	18.925402
50.160963	2870.755612	18.930419
50.132671	2873.305056	18.935437
49.786680	2871.375032	18.940455
50.344381	2880.385106	18.945472
50.318124	2884.164360	18.950490
50.788062	2875.763312	18.955507
50.527303	2880.056089	18.960525
50.287199	2874.152036	18.965543
50.696692	2869.913329	18.970560
50.615082	2861.991963	18.975578
50.772643	2865.339621	18.980595
50.550872	2862.180984	18.985613
50.561835	2870.937480	18.990631
50.469619	2871.094276	18.995648
49.946720	2879.102776	19.000666
50.553089	2871.747835	19.005683
50.187695	2901.294105	19.010701
50.202487	2906.964330	19.015719
50.736659	2902.882226	19.020736
50.492635	2907.070546	19.025754
50.954908	2906.768426	19.030771
50.749668	2914.520080	19.035789
50.807167	2908.861898	19.040807
51.266996	2929.044484	19.045824
51.268835	2935.004398	19.050842
51.233052	2944.106810	19.055859
51.108847	2943.987145	19.060877
51.325420	2942.148100	19.065895
51.125590	2941.383005	19.070912
51.140377	2944.505503	19.075930
51.173219	2938.010429	19.080947
51.061820	2949.172664	19.085965
51.172059	2937.121504	19.090983
51.390348	2944.987210	19.096000
51.213649	2956.961591	19.101018
51.506434	2963.348105	19.106035
51.324710	2971.906938	19.111053
51.313077	2983.095409	19.116071
51.693645	2981.134523	19.121088
51.369764	2988.212717	19.126106
51.262939	2982.215679	19.131123
51.614401	2991.592739	19.136141
51.765156	3009.728789	19.141159
52.080016	3013.355871	19.146176
51.946092	3014.695643	19.151194
52.561567	3016.567695	19.156211
52.390777	3018.309144	19.161229
52.482842	3016.694627	19.166247
52.428454	3016.109358	19.171264
52.333258	3022.058376	19.176282
52.532012	3024.845351	19.181299
52.401802	3025.033076	19.186317
52.447369	3019.235140	19.191335
52.302729	3022.267640	19.196352
52.102213	3021.582990	19.201370
52.039036	3007.945435	19.206387
52.164956	3030.308658	19.211405
52.160071	3046.456069	19.216423
52.770291	3043.506792	19.221440
52.363877	3042.981876	19.226458
52.589762	3054.683330	19.231475
52.987310	3062.959396	19.236493
53.082014	3062.461973	19.241511
53.362071	3060.649045	19.246528
53.486603	3072.012699	19.251546
53.339889	3071.634634	19.256563
53.379590	3047.235491	19.261581
53.204866	3041.829716	19.266599
53.217275	3043.121564	19.271616
53.441030	3056.773385	19.276634
53.389345	3055.769456	19.281651
53.305545	3058.515099	19.286669
53.430781	3062.100671	19.291687
53.755587	3062.966444	19.296704
53.403375	3067.895549	19.301722
53.767382	3071.855232	19.306739
53.712085	3069.292549	19.311757
53.479264	3074.079902	19.316775
54.098835	3070.234346	19.321792
54.252072	3069.430763	19.326810
53.822527	3068.627077	19.331827
54.265146	3073.985381	19.336845
54.044453	3071.584152	19.341863
54.428556	3067.153644	19.346880
53.954752	3069.000603	19.351898
54.141485	3066.510621	19.356915
54.429595	3069.758759	19.361933
54.217767	3068.788586	19.366951
53.933758	3071.543354	19.371968
54.070755	3073.610856	19.376986
54.009275	3065.711139	19.382003
53.686332	3066.566682	19.387021
53.699156	3073.301301	19.392039
54.294648	3092.355101	19.397056
54.198451	3110.047680	19.402074
54.168173	3102.180398	19.407091
54.178709	3104.709834	19.412109
54.331472	3129.558084	19.417127
54.631813	3125.942086	19.422144
54.629026	3140.827556	19.427162
54.459573	3135.744536	19.432179
54.348187	3143.687341	19.437197
54.348614	3156.901061	19.442215
54.883566	3158.368738	19.447232
54.588998	3172.804159	19.452250
55.194181	3173.825061	19.457267
55.189548	3179.201014	19.462285
54.634463	3177.141411	19.467303
55.139883	3188.354789	19.472320
55.106798	3200.081850	19.477338
55.037583	3200.706458	19.482355
55.630510	3199.521909	19.487373
55.548810	3200.521177	19.492391
55.412297	3201.146297	19.497408
55.226952	3203.837706	19.502426
55.470685	3210.239818	19.507443
56.015349	3215.538147	19.512461
55.620871	3239.588866	19.517479
56.175373	3231.099101	19.522496
56.102509	3234.053968	19.527514
56.037120	3233.354804	19.532531
55.935474	3239.803542	19.537549
56.022234	3234.404063	19.542567
56.191395	3232.651083	19.547584
56.083273	3237.404504	19.552602
55.852425	3238.558508	19.557619
56.239531	3235.337933	19.562637
56.052891	3228.484221	19.567655
56.197935	3231.626973	19.572672
56.217118	3238.956762	19.577690
56.569832	3224.078175	19.582707
56.501501	3226.876325	19.587725
56.250536	3231.819624	19.592743
56.393760	3242.675365	19.597760
56.434067	3253.478663	19.602778
56.313102	3257.714496	19.607795
56.460001	3255.969268	19.612813
56.634315	3264.468794	19.617831
56.768761	3260.974141	19.622848
56.565084	3268.906054	19.627866
56.849660	3276.077737	19.632883
56.858024	3285.415350	19.637901
56.670824	3285.801865	19.642919
57.237483	3279.356104	19.647936
57.484264	3289.134837	19.652954
57.301452	3295.977912	19.657971
57.285840	3293.217007	19.662989
56.970244	3292.998628	19.668007
57.239818	3289.817883	19.673024
57.303988	3288.760210	19.678042
57.369239	3308.598246	19.683059
57.586111	3317.344889	19.688077
57.485440	3323.114605	19.693095
57.879304	3320.529216	19.698112
57.819809	3319.528971	19.703130
57.833877	3326.776983	19.708147
58.195332	3319.755230	19.713165
58.192726	3325.257685	19.718183
58.081453	3316.883595	19.723200
58.248350	3328.792260	19.728218
58.047013	3316.553231	19.733235
58.017196	3320.451336	19.738253
57.659314	3325.166485	19.743271
58.143060	3322.405807	19.748288
57.931917	3329.820807	19.753306
57.919954	3347.740996	19.758323
58.233220	3345.968811	19.763341
58.014783	3355.643840	19.768359
58.208882	3356.224097	19.773376
58.337229	3358.777480	19.778394
58.610684	3366.661505	19.783411
58.666563	3369.694347	19.788429
58.614265	3387.515961	19.793447
59.195428	3383.717871	19.798464
58.910827	3384.479436	19.803482
58.705993	3383.132368	19.808499
58.833471	3379.969667	19.813517
58.638941	3385.065579	19.818535
58.917785	3383.507212	19.823552
58.937667	3382.905257	19.828570
59.235298	3383.088940	19.833587
59.174143	3386.521463	19.838605
58.857812	3402.754926	19.843623
59.348947	3413.257369	19.848640
59.643310	3408.324713	19.853658
59.626683	3409.018283	19.858675
59.597284	3414.200092	19.863693
59.648254	3417.000661	19.868711
59.939759	3418.636904	19.873728
59.952739	3418.903256	19.878746
59.940463	3414.923374	19.883763
60.306102	3412.757075	19.888781
59.846798	3417.383316	19.893799
59.974533	3410.476414	19.898816
60.215413	3410.023225	19.903834
59.878938	3418.097692	19.908851
60.089577	3409.602993	19.913869
60.169923	3413.603521	19.918887
60.006472	3412.684100	19.923904
59.883386	3410.380282	19.928922
60.086633	3410.528168	19.933939
59.975514	3414.065347	19.938957
59.882542	3430.702376	19.943975
59.960525	3436.046926	19.948992
60.273713	3447.663611	19.954010
60.165672	3443.181124	19.959027
60.506271	3449.706917	19.964045
60.581584	3472.522064	19.969063
60.713366	3476.586247	19.974080
60.742202	3478.081660	19.979098
60.441151	3481.227698	19.984115
60.797046	3480.880014	19.989133
60.746214	3483.215261	19.994151
60.744039	3484.227690	19.999168
61.098429	3494.633132	20.004186
61.076909	3510.093947	20.009203
61.294230	3507.619917	20.014221
61.328267	3517.217893	20.019239
61.577057	3509.416762	20.024256
61.630805	3512.644530	20.029274
61.281134	3514.656126	20.034291
61.323663	3505.153737	20.039309
60.975877	3508.786644	20.044327
61.119278	3515.703836	20.049344
61.526582	3530.486286	20.054362
61.134965	3540.433696	20.059379
61.342597	3536.017562	20.064397
61.193290	3551.384551	20.069415
61.725468	3560.445074	20.074432
61.913487	3565.928320	20.079450
61.917016	3573.483048	20.084467
61.981091	3573.049929	20.089485
62.104779	3573.076779	20.094503
61.992362	3571.226335	20.099520
62.074386	3576.204011	20.104538
62.435501	3593.046104	20.109555
62.477544	3594.828309	20.114573
62.459105	3606.898912	20.119591
62.829345	3599.847176	20.124608
62.992606	3594.417919	20.129626
63.074833	3607.078493	20.134643
63.256278	3577.932635	20.139661
62.625866	3571.052470	20.144679
62.858221	3556.670696	20.149696
63.138156	3552.671396	20.154714
62.969049	3561.594613	20.159731
63.050548	3556.818119	20.164749
62.988239	3569.349864	20.169767
63.092418	3589.027211	20.174784
63.372133	3590.633990	20.179802
63.396298	3590.736972	20.184819
63.209187	3583.624857	20.189837
63.298370	3600.771121	20.194855
63.238078	3588.349393	20.199872
63.580027	3592.998981	20.204890
63.179575	3591.712211	20.209907
63.580792	3583.758896	20.214925
63.668626	3590.323358	20.219943
63.744276	3590.093814	20.224960
63.713229	3588.981563	20.229978
63.495342	3607.562697	20.234995
63.927249	3616.883022	20.240013
63.873282	3620.608921	20.245031
63.507599	3635.527146	20.250048
63.635736	3624.978265	20.255066
63.496571	3628.651040	20.260083
64.189594	3638.077827	20.265101
64.375919	3640.539407	20.270119
64.623460	3644.547557	20.275136
64.926265	3642.661358	20.280154
64.751234	3658.159663	20.285171
64.657139	3651.082763	20.290189
64.777098	3651.487509	20.295207
64.626373	3650.777753	20.300224
64.772682	3642.106512	20.305242
64.600896	3648.053932	20.310259
64.637886	3645.027194	20.315277
64.933424	3650.154947	20.320295
64.614931	3642.957429	20.325312
64.649593	3644.416418	20.330330
64.878824	3672.491774	20.335347
65.189693	3675.649503	20.340365
65.333820	3679.554891	20.345383
65.290404	3689.031572	20.350400
65.192796	3683.120898	20.355418
65.232781	3688.821739	20.360435
65.552141	3685.029085	20.365453
65.249438	3679.158300	20.370471
65.507621	3677.912970	20.375488
65.590872	3679.274634	20.380506
64.987493	3689.920807	20.385523
65.440135	3706.987546	20.390541
65.626763	3719.060882	20.395559
65.437090	3721.421542	20.400576
65.924672	3714.800142	20.405594
65.665399	3722.401573	20.410611
65.773303	3727.966344	20.415629
65.849796	3737.010584	20.420647
65.938849	3734.537245	20.425664
66.247273	3733.730652	20.430682
66.035840	3742.687217	20.435699
66.407515	3742.903892	20.440717
66.562334	3741.957450	20.445735
66.122482	3739.461375	20.450752
66.497044	3756.881796	20.455770
66.504849	3769.945121	20.460787
66.563972	3771.423556	20.465805
66.983470	3768.709260	20.470823
66.760388	3765.267130	20.475840
67.130191	3760.489190	20.480858
67.050158	3767.906331	20.485875
67.027000	3759.475944	20.490893
67.444589	3761.414309	20.495911
66.743470	3767.500569	20.500928
67.168301	3753.829897	20.505946
67.138102	3756.864969	20.510963
67.481702	3755.829454	20.515981
67.385345	3763.206075	20.520999
67.421624	3781.714696	20.526016
67.537025	3781.676809	20.531034
67.355281	3792.959601	20.536051
67.686675	3783.085393	20.541069
68.131431	3781.424509	20.546087
68.132924	3791.905615	20.551104
68.539928	3791.823248	20.556122
68.534811	3789.143155	20.561139
68.547883	3789.590645	20.566157
68.660174	3769.651496	20.571175
68.430743	3758.562893	20.576192
68.497616	3748.141785	20.581210
68.183146	3754.337385	20.586227
68.080661	3754.214777	20.591245
67.882936	3757.103724	20.596263
68.015113	3782.314890	20.601280
68.316714	3789.773725	20.606298
68.343629	3792.583211	20.611315
68.306958	3790.400777	20.616333
68.621914	3800.961251	20.621351
68.341885	3815.549921	20.626368
68.644574	3817.044884	20.631386
68.682142	3831.364103	20.636403
68.693741	3822.537074	20.641421
68.930169	3821.975949	20.646439
68.972607	3826.839202	20.651456
69.073369	3835.395752	20.656474
68.915126	3851.026835	20.661491
69.161469	3855.902394	20.666509
69.241028	3856.627537	20.671527
68.975811	3863.956756	20.676544
69.009623	3859.672722	20.681562
69.033875	3869.074114	20.686579
69.277602	3884.785171	20.691597
69.648668	3890.730187	20.696615
69.558337	3890.252648	20.701632
69.592412	3887.328751	20.706650
69.704500	3883.681850	20.711667
69.551815	3897.443045	20.716685
69.971754	3913.731950	20.721703
70.087099	3927.686651	20.726720
70.141385	3914.758283	20.731738
70.226137	3922.481189	20.736755
70.199533	3924.864329	20.741773
70.526066	3916.291994	20.746791
70.522273	3924.391592	20.751808
70.226764	3919.753660	20.756826
70.545738	3909.367985	20.761843
70.683222	3932.933964	20.766861
70.728320	3932.649009	20.771879
70.550792	3948.886800	20.776896
71.162589	3940.611304	20.781914
71.164968	3938.401676	20.786931
70.953325	3944.470244	20.791949
71.285894	3936.663991	20.796967
71.289094	3935.927045	20.801984
71.660033	3937.435522	20.807002
71.719881	3941.814599	20.812019
71.459164	3936.884796	20.817037
71.746337	3931.688576	20.822055
71.942500	3942.752314	20.827072
71.709404	3924.263096	20.832090
71.785742	3914.046609	20.837107
71.715888	3927.136767	20.842125
72.076507	3920.467740	20.847143
71.683184	3938.716254	20.852160
72.138384	3932.276740	20.857178
72.143606	3940.144033	20.862195
71.717886	3944.503181	20.867213
72.090949	3935.284111	20.872231
72.238370	3939.641085	20.877248
72.461020	3930.553344	20.882266
72.318966	3933.157905	20.887283
71.933830	3933.887898	20.892301
72.161452	3929.094116	20.897319
71.893272	3940.266603	20.902336
71.924113	3961.902374	20.907354
72.143426	3961.385922	20.912371
72.385775	3969.283459	20.917389
72.104047	3985.478507	20.922407
72.215450	4003.010476	20.927424
72.370461	4004.179503	20.932442
72.718115	4000.852913	20.937459
72.582682	4013.885077	20.942477
73.188083	4018.669199	20.947495
73.103158	4032.215691	20.952512
73.084348	4031.261196	20.957530
73.506261	4027.948648	20.962547
73.333874	4023.445523	20.967565
73.604519	4015.325353	20.972583
73.228451	4023.410065	20.977600
73.218033	4023.165343	20.982618
73.466279	4041.151973	20.987635
73.605960	4056.918057	20.992653
73.969925	4063.087251	20.997671
73.987250	4061.407469	21.002688
73.932770	4061.431787	21.007706
74.130324	4057.285025	21.012723
73.903024	4055.423502	21.017741
73.850961	4062.174392	21.022759
73.975556	4064.995534	21.027776
74.103864	4060.913412	21.032794
74.168416	4076.547477	21.037811
73.741089	4101.876340	21.042829
74.130507	4087.382096	21.047847
74.202220	4085.134570	21.052864
74.699291	4105.572195	21.057882
74.908480	4111.289862	21.062899
75.087239	4116.281842	21.067917
75.214269	4118.612679	21.072935
75.292687	4115.636244	21.077952
75.291637	4111.907085	21.082970
75.577376	4105.216952	21.087987
75.418044	4104.427526	21.093005
75.422493	4104.674875	21.098023
75.431741	4109.639206	21.103040
75.654660	4106.223714	21.108058
75.560983	4100.900555	21.113075
75.566989	4110.136670	21.118093
75.469877	4110.018650	21.123111
75.506775	4108.093710	21.128128
75.536744	4103.400710	21.133146
75.841798	4104.370746	21.138163
75.353927	4101.066876	21.143181
75.651427	4110.923275	21.148199
75.631255	4125.458227	21.153216
76.000322	4134.932980	21.158234
76.105685	4130.931961	21.163251
76.174635	4134.149374	21.168269
76.157280	4130.989301	21.173287
76.473097	4154.333647	21.178304
76.316097	4171.268336	21.183322
76.746829	4171.869491	21.188339
76.413989	4182.377458	21.193357
76.648538	4173.651418	21.198375
76.726754	4170.502519	21.203392
76.600259	4162.635451	21.208410
76.856870	4171.150499	21.213427
76.712568	4178.275618	21.218445
77.159404	4176.057494	21.223463
77.321451	4184.954216	21.228480
77.125128	4194.813418	21.233498
77.363624	4191.616558	21.238515
77.134041	4198.322329	21.243533
77.249524	4190.976909	21.248551
77.544285	4194.758936	21.253568
77.564170	4187.283410	21.258586
77.682080	4193.363307	21.263603
77.417342	4202.504909	21.268621
77.729052	4196.111156	21.273639
77.777160	4220.359211	21.278656
77.824633	4228.466716	21.283674
78.048892	4228.621248	21.288691
77.847118	4232.671139	21.293709
77.935878	4237.684101	21.298727
78.058712	4240.460682	21.303744
78.141561	4229.014975	21.308762
78.426042	4247.735203	21.313779
78.164781	4262.316340	21.318797
78.174262	4253.179898	21.323815
78.210031	4260.478964	21.328832
78.324281	4264.593614	21.333850
78.695506	4274.164958	21.338867
78.534600	4299.252343	21.343885
78.862264	4291.386111	21.348903
78.549762	4303.843189	21.353920
78.491087	4304.944907	21.358938
79.078768	4311.515338	21.363955
78.979674	4316.954343	21.368973
78.997508	4327.770105	21.373991
79.317795	4325.969832	21.379008
79.341454	4334.353991	21.384026
79.464790	4329.019543	21.389043
79.757821	4343.740437	21.394061
79.915343	4359.018587	21.399079
79.990659	4355.150258	21.404096
79.893341	4360.455864	21.409114
80.061843	4349.187568	21.414131
79.801500	4361.093861	21.419149
79.976827	4363.620450	21.424167
80.192963	4353.068600	21.429184
79.922890	4358.458957	21.434202
80.128532	4355.654421	21.439219
80.133412	4376.187807	21.444237
80.300882	4380.069677	21.449255
80.483125	4384.586993	21.454272
80.363579	4381.371141	21.459290
80.827198	4378.674385	21.464307
80.822201	4377.088974	21.469325
80.798786	4373.840102	21.474343
81.121740	4368.002779	21.479360
80.851844	4378.715894	21.484378
81.145163	4389.488407	21.489395
81.451608	4406.907836	21.494413
81.528577	4407.089197	21.499431
81.465336	4406.796815	21.504448
81.297877	4413.837008	21.509466
81.743236	4405.721343	21.514483
81.725916	4413.696702	21.519501
81.598068	4419.382473	21.524519
81.582956	4406.749149	21.529536
81.375327	4415.829098	21.534554
81.649452	4406.930743	21.539571
81.717729	4416.127218	21.544589
81.496211	4417.478186	21.549607
82.183717	4431.061144	21.554624
81.843348	4438.575215	21.559642
82.142076	4442.114032	21.564659
81.988181	4443.146233	21.569677
82.313536	4450.138184	21.574695
82.332776	4458.026172	21.579712
82.053293	4483.103458	21.584730
82.414950	4474.416110	21.589747
82.583791	4481.019038	21.594765
82.661560	4480.150349	21.599783
82.707509	4480.659171	21.604800
82.826820	4497.091586	21.609818
83.125586	4498.975592	21.614835
82.776496	4507.552132	21.619853
82.908350	4512.652309	21.624871
83.236003	4510.252151	21.629888
82.932555	4523.204056	21.634906
83.214193	4528.822027	21.639923
83.533524	4538.870285	21.644941
83.502545	4545.642183	21.649959
83.704610	4540.591892	21.654976
83.566573	4549.244116	21.659994
83.856219	4546.566132	21.665011
83.938053	4565.435685	21.670029
84.117023	4576.195637	21.675047
84.383708	4574.421854	21.680064
84.511143	4584.140727	21.685082
84.464427	4572.555520	21.690099
84.702681	4571.818415	21.695117
84.637481	4568.259250	21.700135
84.463352	4563.979957	21.705152
84.453532	4574.177609	21.710170
84.796424	4565.316209	21.715187
84.480870	4569.273060	21.720205
84.386358	4584.548954	21.725223
84.606207	4593.156386	21.730240
84.568434	4598.073009	21.735258
84.798024	4603.109200	21.740275
84.973203	4603.150856	21.745293
84.892877	4625.227190	21.750311
85.273726	4635.743847	21.755328
85.022255	4638.511419	21.760346
85.199166	4639.446749	21.765363
85.574403	4638.007212	21.770381
85.268904	4637.594892	21.775399
85.795725	4647.695863	21.780416
85.864223	4669.028415	21.785434
85.770789	4672.120187	21.790451
85.835048	4684.211302	21.795469
85.918514	4673.593769	21.800487
86.065026	4670.555147	21.805504
86.005529	4670.023463	21.810522
86.226510	4672.762027	21.815539
85.978439	4680.926733	21.820557
86.197520	4694.057780	21.825575
86.148804	4693.973991	21.830592
86.244593	4701.292112	21.835610
86.468845	4709.784644	21.840627
86.604958	4715.629267	21.845645
86.630877	4720.432615	21.850663
86.830765	4723.002311	21.855680
86.777158	4728.410028	21.860698
87.195516	4717.909121	21.865715
87.550989	4728.996507	21.870733
87.272304	4743.741751	21.875751
87.503470	4738.403644	21.880768
87.715990	4743.735024	21.885786
87.835767	4752.752734	21.890803
87.717576	4740.762993	21.895821
87.784286	4742.906566	21.900839
88.185723	4737.265956	21.905856
87.968311	4741.654193	21.910874
88.299147	4731.088730	21.915891
88.312333	4735.361817	21.920909
88.206960	4732.563278	21.925927
88.286427	4735.679767	21.930944
88.325397	4737.333455	21.935962
88.437487	4729.705603	21.940979
88.411971	4744.183753	21.945997
88.856155	4763.612873	21.951015
89.003821	4757.711731	21.956032
88.702248	4767.967402	21.961050
88.596577	4766.898579	21.966067
88.893855	4764.659545	21.971085
88.714338	4782.603784	21.976103
89.133821	4773.441647	21.981120
88.668188	4782.102901	21.986138
89.150751	4796.775972	21.991155
89.321169	4793.008592	21.996173
89.332102	4796.059653	22.001191
89.451581	4798.338327	22.006208
89.068968	4810.051677	22.011226
89.628337	4826.804389	22.016243
89.920818	4828.159426	22.021261
89.918956	4822.144481	22.026279
90.184820	4815.872549	22.031296
90.185656	4819.516083	22.036314
90.108030	4820.873133	22.041331
90.478055	4819.033560	22.046349
90.628199	4820.728846	22.051367
90.873040	4808.427131	22.056384
90.444005	4814.860960	22.061402
89.940567	4816.376865	22.066419
90.611961	4827.728370	22.071437
90.506314	4846.123941	22.076455
91.126101	4850.630178	22.081472
91.278949	4855.582727	22.086490
91.045359	4852.665946	22.091507
91.304419	4854.148013	22.096525
91.108996	4859.422558	22.101543
91.501643	4851.925345	22.106560
91.265697	4856.254567	22.111578
91.400554	4854.896392	22.116595
91.534117	4857.577512	22.121613
91.141952	4865.054979	22.126631
91.250279	4874.480362	22.131648
91.270010	4888.980030	22.136666
91.093818	4891.012461	22.141683
91.164853	4903.869756	22.146701
91.126314	4924.651529	22.151719
91.555637	4940.073467	22.156736
91.615926	4959.780523	22.161754
91.633400	4966.190636	22.166771
92.209161	4979.382070	22.171789
92.082241	4996.436932	22.176807
92.281067	4984.640769	22.181824
92.582519	4998.625946	22.186842
92.463449	5005.227255	22.191859
92.799033	5018.811981	22.196877
92.980880	5030.503549	22.201895
93.148591	5025.248690	22.206912
93.442785	5024.657145	22.211930
93.164419	5023.716369	22.216947
93.487325	5011.594090	22.221965
93.187465	5024.036959	22.226983
93.618425	5043.221366	22.232000
93.880025	5037.665274	22.237018
94.146555	5042.383360	22.242035
94.817082	5039.409213	22.247053
94.555630	5027.225634	22.252071
94.925823	4997.331190	22.257088
94.843460	4990.035860	22.262106
94.478526	4996.205934	22.267123
94.924271	4986.119977	22.272141
94.780158	4993.255668	22.277159
94.838310	4990.466068	22.282176
95.014280	4989.485211	22.287194
94.909141	4992.399465	22.292211
95.031116	4986.746029	22.297229
95.486425	4993.342593	22.302247
95.418172	4981.294486	22.307264
95.528207	4958.561986	22.312282
95.169620	4965.984908	22.317299
95.179346	4952.801044	22.322317
95.152645	4953.568085	22.327335
95.343025	4963.844300	22.332352
95.566486	4982.986230	22.337370
95.497212	4986.871817	22.342387
95.394143	4988.408891	22.347405
94.905615	4996.723679	22.352423
95.208154	4994.043411	22.357440
95.440303	5016.648010	22.362458
95.169682	5028.425812	22.367475
95.669704	5025.625828	22.372493
95.650748	5047.109360	22.377511
96.049081	5052.753984	22.382528
96.061150	5052.326591	22.387546
96.211154	5062.074970	22.392563
96.184285	5074.125294	22.397581
96.424906	5087.252188	22.402599
96.129581	5083.545682	22.407616
96.470297	5102.313993	22.412634
96.315301	5124.019442	22.417651
96.741528	5127.526317	22.422669
96.586964	5134.988380	22.427687
97.035586	5140.853625	22.432704
97.215433	5145.192771	22.437722
97.424866	5148.825036	22.442739
97.379523	5154.177133	22.447757
97.582566	5154.062782	22.452775
97.597936	5150.713369	22.457792
97.401305	5164.521003	22.462810
97.617423	5173.371992	22.467827
98.151298	5175.242556	22.472845
97.975855	5167.337695	22.477863
98.054215	5167.982763	22.482880
98.430848	5170.864866	22.487898
98.137874	5170.144769	22.492915
98.415279	5179.976926	22.497933
98.462443	5199.592798	22.502951
98.866427	5193.168650	22.507968
98.820566	5188.753772	22.512986
98.760982	5190.903305	22.518003
99.198581	5186.142464	22.523021
99.032692	5196.852475	22.528039
99.308839	5196.762612	22.533056
99.341673	5194.928031	22.538074
99.012449	5218.916209	22.543091
99.243743	5221.241938	22.548109
99.789742	5240.559671	22.553127
99.271858	5233.866633	22.558144
99.907089	5230.847304	22.563162
99.625032	5232.766387	22.568179
99.895818	5233.767578	22.573197
99.832062	5247.352436	22.578215
99.794811	5258.507523	22.583232
100.102844	5251.353089	22.588250
100.078141	5253.246959	22.593267
100.311547	5251.096788	22.598285
100.019292	5263.989875	22.603303
100.271046	5281.678788	22.608320
100.726569	5276.143717	22.613338
100.779325	5284.570651	22.618355
100.901548	5281.744811	22.623373
101.072757	5284.469173	22.628391
100.956367	5292.914870	22.633408
101.264837	5282.544281	22.638426
100.579304	5289.741417	22.643443
101.094261	5304.782764	22.648461
101.363309	5317.374083	22.653479
101.123433	5310.530954	22.658496
101.504316	5316.896235	22.663514
101.671265	5341.263473	22.668531
101.987394	5339.112500	22.673549
101.938885	5355.174436	22.678567
101.962915	5348.136388	22.683584
102.320372	5343.157664	22.688602
102.474023	5346.589229	22.693619
102.801942	5336.969076	22.698637
102.612803	5334.780272	22.703655
102.670060	5330.952612	22.708672
102.895319	5336.356050	22.713690
102.819578	5334.208456	22.718707
102.803898	5327.705755	22.723725
102.979827	5343.266050	22.728743
103.092432	5358.852182	22.733760
103.091192	5358.766551	22.738778
103.366421	5368.871735	22.743795
103.476407	5362.686964	22.748813
103.870617	5366.293903	22.753831
103.459355	5368.131180	22.758848
103.642871	5361.644726	22.763866
103.326906	5374.642790	22.768883
103.445445	5394.028479	22.773901
103.972849	5392.781765	22.778919
104.105412	5403.387974	22.783936
104.064342	5398.265670	22.788954
104.293158	5401.318878	22.793971
104.034454	5403.973607	22.798989
104.146331	5431.214422	22.804007
104.304216	5426.796057	22.809024
104.650740	5433.113714	22.814042
104.519416	5435.247221	22.819059
104.461380	5447.838006	22.824077
105.100653	5461.586086	22.829095
104.680856	5459.404513	22.834112
105.170260	5466.660235	22.839130
105.455239	5469.669958	22.844147
105.323238	5463.717252	22.849165
105.294462	5482.972344	22.854183
105.396980	5491.462535	22.859200
105.559128	5486.180910	22.864218
105.321311	5491.875676	22.869235
105.631799	5499.242429	22.874253
105.805172	5503.172401	22.879271
106.318609	5525.656248	22.884288
105.856255	5531.676239	22.889306
105.987163	5530.244643	22.894323
106.199756	5526.229617	22.899341
106.476213	5520.251764	22.904359
106.520887	5536.770518	22.909376
106.609937	5540.407758	22.914394
106.394962	5544.425585	22.919411
106.617736	5556.319262	22.924429
106.713374	5560.847037	22.929447
106.605601	5574.616162	22.934464
107.123592	5579.333047	22.939482
107.129771	5590.710139	22.944499
107.423161	5587.216874	22.949517
107.421403	5592.073279	22.954535
107.122366	5604.672421	22.959552
107.761340	5599.064830	22.964570
108.143660	5614.946831	22.969587
108.199749	5607.295865	22.974605
108.336718	5606.275971	22.979623
108.171938	5613.053145	22.984640
108.134318	5604.781006	22.989658
108.346217	5614.929499	22.994675
108.653689	5631.190623	22.999693
109.129057	5639.906056	23.004711
108.869662	5648.711225	23.009728
108.944009	5642.015732	23.014746
108.995041	5648.740957	23.019763
108.612624	5644.584512	23.024781
108.821841	5639.614569	23.029799
109.069560	5650.647821	23.034816
109.160290	5653.979963	23.039834
109.151660	5673.405123	23.044851
109.046204	5668.954643	23.049869
109.144801	5671.237811	23.054887
109.063318	5697.451211	23.059904
108.868366	5700.542468	23.064922
109.621171	5716.398078	23.069939
109.867926	5739.766053	23.074957
110.498975	5736.268432	23.079975
109.781955	5736.121189	23.084992
110.178223	5744.945552	23.090010
110.164810	5764.263728	23.095027
110.447746	5763.829265	23.100045
110.285875	5766.355599	23.105063
110.156047	5775.968857	23.110080
110.946995	5792.074792	23.115098
110.624194	5796.066268	23.120115
110.733335	5794.685642	23.125133
111.059287	5811.091869	23.130151
111.150218	5829.789647	23.135168
111.285560	5828.039821	23.140186
111.358387	5825.726481	23.145203
111.739709	5832.261252	23.150221
111.873374	5838.649434	23.155239
111.820879	5862.985775	23.160256
111.906843	5858.993950	23.165274
111.838894	5867.576583	23.170291
111.955244	5854.794325	23.175309
112.030342	5861.190982	23.180327
112.855511	5877.740915	23.185344
112.696730	5876.221103	23.190362
112.831481	5891.837044	23.195379
112.952874	5889.003363	23.200397
113.389368	5882.455212	23.205415
113.419475	5886.515392	23.210432
113.590427	5873.181820	23.215450
113.726782	5883.649852	23.220467
113.570769	5879.534877	23.225485
113.889612	5875.223491	23.230503
113.865704	5877.508785	23.235520
114.053542	5870.247863	23.240538
114.041362	5873.948220	23.245555
113.930636	5880.034879	23.250573
114.476179	5872.298301	23.255591
114.072365	5878.479316	23.260608
114.187661	5875.771139	23.265626
114.180655	5885.861234	23.270643
114.115543	5869.840323	23.275661
114.814721	5887.205869	23.280679
114.696400	5907.837186	23.285696
114.523062	5905.030398	23.290714
114.556958	5921.256010	23.295731
114.454041	5915.669945	23.300749
114.621453	5930.243707	23.305767
114.678567	5945.505153	23.310784
114.994871	5945.364293	23.315802
114.795429	5958.924181	23.320819
114.760880	5967.420008	23.325837
115.233089	5975.992806	23.330855
115.339334	5994.034356	23.335872
115.818414	6001.310999	23.340890
116.100251	5997.118567	23.345907
115.996893	6008.507646	23.350925
116.304942	6020.558772	23.355943
116.357133	6031.447787	23.360960
116.363939	6030.523438	23.365978
116.581045	6037.916692	23.370995
116.466553	6033.078530	23.376013
116.725543	6038.564650	23.381031
117.430007	6057.690795	23.386048
117.180119	6059.427224	23.391066
117.133042	6058.285251	23.396083
117.039085	6063.902780	23.401101
117.192398	6064.030113	23.406119
117.275958	6056.330899	23.411136
117.457594	6077.337163	23.416154
117.811321	6077.419899	23.421171
117.767807	6077.913390	23.426189
118.140528	6065.207533	23.431207
118.383407	6078.479011	23.436224
118.356960	6076.456777	23.441242
118.492007	6065.890127	23.446259
118.557294	6071.488237	23.451277
118.457599	6060.857068	23.456295
118.680895	6067.347345	23.461312
118.552958	6074.565818	23.466330
119.130007	6096.337719	23.471347
119.170328	6100.113414	23.476365
119.136311	6101.885310	23.481383
119.324231	6100.264291	23.486400
119.283338	6093.108648	23.491418
119.504580	6088.323980	23.496435
119.485041	6099.497100	23.501453
119.424648	6110.376325	23.506471
119.752609	6121.206310	23.511488
119.714533	6128.808773	23.516506
119.749484	6117.856727	23.521523
119.644464	6130.321406	23.526541
120.088047	6147.913805	23.531559
120.142271	6160.840379	23.536576
120.587096	6158.645180	23.541594
120.560253	6154.504050	23.546611
120.846844	6177.656308	23.551629
120.796655	6174.033553	23.556647
121.071569	6172.189657	23.561664
121.226718	6185.049322	23.566682
121.426987	6177.831029	23.571699
121.357218	6175.574380	23.576717
121.600535	6177.158527	23.581735
121.728732	6182.410323	23.586752
121.604101	6189.892954	23.591770
122.067187	6196.968412	23.596787
121.871201	6204.800425	23.601805
122.055776	6201.216978	23.606823
122.436557	6204.610580	23.611840
122.375548	6202.832145	23.616858
122.621706	6200.114083	23.621875
122.487034	6201.063539	23.626893
122.790740	6220.193203	23.631911
122.769747	6231.490336	23.636928
122.777882	6226.474337	23.641946
122.860537	6226.703586	23.646963
122.839580	6233.790359	23.651981
123.372029	6244.497936	23.656999
123.503627	6253.872097	23.662016
123.212822	6261.950407	23.667034
123.640697	6262.905831	23.672051
123.412548	6267.984793	23.677069
123.388611	6272.229998	23.682087
123.769722	6282.804425	23.687104
123.998558	6295.141891	23.692122
124.400898	6290.660112	23.697139
124.099785	6297.567290	23.702157
124.119907	6295.813535	23.707175
124.337237	6319.829400	23.712192
124.262894	6327.539791	23.717210
124.527803	6327.593643	23.722227
124.787792	6336.859194	23.727245
124.973113	6364.287521	23.732263
124.752221	6361.245395	23.737280
125.075446	6367.915597	23.742298
125.773246	6361.058569	23.747315
125.697647	6369.711315	23.752333
125.695939	6383.286503	23.757351
125.808654	6382.102146	23.762368
125.666333	6390.161367	23.767386
126.046969	6392.508146	23.772403
125.890598	6394.834341	23.777421
126.206723	6397.553747	23.782439
126.765313	6411.040783	23.787456
126.665136	6422.077496	23.792474
126.875995	6419.767977	23.797491
126.901351	6428.152950	23.802509
126.912165	6418.758237	23.807527
127.022987	6415.806540	23.812544
126.822529	6423.532296	23.817562
127.272424	6441.341351	23.822579
127.415666	6442.672490	23.827597
127.479859	6442.737120	23.832615
127.372603	6446.112035	23.837632
127.289144	6451.963432	23.842650
127.388465	6465.799439	23.847667
127.549667	6473.653850	23.852685
127.578423	6485.041887	23.857703
127.841231	6496.439436	23.862720
128.200999	6501.791856	23.867738
128.877232	6497.092916	23.872755
128.965897	6507.088230	23.877773
129.136392	6509.339500	23.882791
129.306315	6520.611986	23.887808
129.338621	6519.586347	23.892826
129.816733	6511.601860	23.897843
129.742592	6516.285051	23.902861
129.736853	6516.942229	23.907879
129.776426	6512.419386	23.912896
129.690518	6518.463434	23.917914
130.178296	6509.266546	23.922931
130.052195	6513.689239	23.927949
129.878502	6512.674494	23.932967
130.261473	6517.094205	23.937984
129.856027	6525.692511	23.943002
130.494943	6536.451355	23.948019
130.872172	6549.572582	23.953037
130.631736	6538.717873	23.958055
130.898719	6539.001390	23.963072
130.898213	6543.879927	23.968090
131.338172	6535.348192	23.973107
130.923906	6537.320025	23.978125
130.985411	6557.928443	23.983143
130.961333	6575.178475	23.988160
130.935942	6578.588223	23.993178
131.450679	6590.747718	23.998195
131.477525	6603.591117	24.003213
131.751523	6605.879011	24.008231
132.342408	6600.202913	24.013248
132.492189	6597.227961	24.018266
132.305346	6612.776066	24.023283
132.844347	6623.515862	24.028301
132.982032	6612.326874	24.033319
133.210236	6609.811907	24.038336
133.224113	6627.115356	24.043354
133.244512	6625.583660	24.048371
133.487312	6617.744230	24.053389
133.421105	6619.676886	24.058407
133.853897	6614.020006	24.063424
133.669072	6614.516469	24.068442
133.617820	6615.856546	24.073459
133.504501	6620.415718	24.078477
133.686640	6632.534584	24.083495
133.849026	6646.599409	24.088512
133.553787	6659.770627	24.093530
133.823942	6652.696112	24.098547
134.070886	6669.438957	24.103565
134.028732	6674.741388	24.108583
134.432457	6689.622729	24.113600
134.570555	6703.234090	24.118618
134.859868	6711.106043	24.123635
135.134615	6715.145764	24.128653
134.963114	6722.634315	24.133671
135.599960	6731.442408	24.138688
135.404818	6741.490460	24.143706
135.826117	6744.781917	24.148723
135.550303	6747.064043	24.153741
135.564346	6757.240884	24.158759
136.215436	6754.224078	24.163776
135.977328	6762.855267	24.168794
136.395953	6765.242068	24.173811
136.317287	6768.462478	24.178829
136.427965	6784.286659	24.183847
136.245750	6785.141104	24.188864
136.123708	6803.075396	24.193882
136.768495	6808.652408	24.198899
136.877449	6817.655028	24.203917
136.821773	6832.571930	24.208935
137.290606	6838.357935	24.213952
137.345948	6856.796760	24.218970
137.911647	6858.449388	24.223987
138.079868	6868.317066	24.229005
138.027452	6866.782074	24.234023
138.033565	6859.234395	24.239040
138.296771	6858.381055	24.244058
138.496734	6855.654260	24.249075
138.590523	6862.690919	24.254093
138.117589	6880.611402	24.259111
138.639439	6881.068654	24.264128
138.548530	6894.201884	24.269146
138.718979	6891.741676	24.274163
138.841868	6898.340887	24.279181
138.819800	6916.541758	24.284199
138.991744	6921.889495	24.289216
139.060419	6931.800273	24.294234
139.181516	6952.787347	24.299251
139.654395	6960.768963	24.304269
139.605591	6957.438050	24.309287
140.034993	6970.053608	24.314304
139.757826	6985.408015	24.319322
139.922469	6973.836819	24.324339
140.235310	6988.288937	24.329357
140.505242	7009.231664	24.334375
140.611711	7001.695860	24.339392
140.518552	7010.241676	24.344410
140.895905	7025.290129	24.349427
141.505717	7031.439615	24.354445
141.197081	7025.233799	24.359463
141.577089	7020.750921	24.364480
141.840471	7024.598094	24.369498
141.988465	7022.264606	24.374515
142.178213	7027.186301	24.379533
142.198213	7049.766349	24.384551
142.531208	7048.878192	24.389568
142.632679	7052.754703	24.394586
142.608803	7057.864278	24.399603
142.857263	7053.940407	24.404621
142.917967	7051.146073	24.409639
143.153180	7051.624109	24.414656
143.082751	7046.836379	24.419674
142.828976	7051.846718	24.424691
142.936667	7069.166073	24.429709
142.835887	7082.861247	24.434727
143.410263	7082.587913	24.439744
143.694255	7097.906099	24.444762
143.665433	7104.913467	24.449779
143.709507	7112.605511	24.454797
143.409148	7117.998043	24.459815
144.598429	7129.494032	24.464832
144.699658	7151.648300	24.469850
144.704304	7142.645737	24.474867
144.870296	7152.543121	24.479885
144.919874	7147.898643	24.484903
145.029404	7158.115300	24.489920
145.295747	7176.831853	24.494938
145.126107	7186.762373	24.499955
145.175273	7179.704242	24.504973
145.201749	7182.398602	24.509991
145.237872	7196.222443	24.515008
145.248786	7216.578844	24.520026
145.299901	7223.198370	24.525043
145.585719	7234.794960	24.530061
145.506526	7249.841538	24.535079
146.024038	7265.540521	24.540096
146.315334	7281.311386	24.545114
146.412838	7284.166896	24.550131
147.001957	7275.006557	24.555149
146.725600	7285.759746	24.560167
146.781052	7306.276421	24.565184
147.076523	7316.843374	24.570202
147.404385	7303.439962	24.575219
147.525872	7303.058349	24.580237
147.623584	7324.308309	24.585255
148.065993	7332.118874	24.590272
148.095310	7337.065804	24.595290
148.010607	7347.026766	24.600307
148.241180	7336.315285	24.605325
148.215107	7347.151653	24.610343
148.570735	7352.607482	24.615360
148.734932	7362.033427	24.620378
148.820927	7360.580222	24.625395
148.897218	7365.034626	24.630413
148.544970	7392.904281	24.635431
149.036433	7395.315719	24.640448
149.428811	7394.185757	24.645466
149.374961	7415.284569	24.650483
149.474490	7422.749829	24.655501
149.477371	7434.330469	24.660519
149.909961	7430.961049	24.665536
149.953030	7453.771682	24.670554
150.040655	7449.848503	24.675571
150.862197	7440.516669	24.680589
150.860033	7446.149669	24.685607
151.116171	7439.245010	24.690624
151.331173	7450.214221	24.695642
151.412802	7462.893726	24.700659
151.838671	7464.757096	24.705677
151.976665	7465.915910	24.710695
152.357577	7441.229379	24.715712
152.223398	7434.521617	24.720730
152.642188	7430.162750	24.725747
153.021027	7408.300021	24.730765
152.872675	7402.276129	24.735783
153.252501	7397.307909	24.740800
153.199508	7396.639519	24.745818
153.356991	7397.375103	24.750835
153.834828	7392.148236	24.755853
153.536189	7403.382716	24.760871
153.772852	7385.695185	24.765888
153.441554	7379.570317	24.770906
153.404489	7396.185361	24.775923
153.915962	7382.372275	24.780941
153.742696	7395.384536	24.785959
153.752254	7395.251352	24.790976
154.000681	7391.720506	24.795994
153.479994	7395.098744	24.801011
153.608609	7411.268668	24.806029
154.041562	7425.115274	24.811047
153.972192	7426.390774	24.816064
154.179946	7446.268630	24.821082
154.286843	7463.203324	24.826099
154.409506	7463.286297	24.831117
154.396538	7498.721319	24.836135
154.656762	7506.263058	24.841152
154.848454	7513.537674	24.846170
154.821211	7536.859932	24.851187
155.340963	7546.009969	24.856205
155.524853	7562.549495	24.861223
155.615156	7569.925022	24.866240
155.794034	7581.904942	24.871258
155.420249	7611.841878	24.876275
156.045999	7607.675944	24.881293
155.997601	7627.869723	24.886311
156.170888	7639.685208	24.891328
156.577096	7653.446001	24.896346
156.725138	7664.491436	24.901363
157.048760	7664.257144	24.906381
157.141979	7681.609578	24.911399
157.483306	7694.848196	24.916416
158.078592	7687.116409	24.921434
157.850237	7692.278570	24.926451
158.307360	7688.550387	24.931469
158.419971	7702.909067	24.936487
158.248046	7715.483345	24.941504
158.708737	7708.269355	24.946522
158.534813	7720.673817	24.951539
158.828890	7713.394639	24.956557
159.027643	7728.049753	24.961575
159.492259	7738.240573	24.966592
159.518624	7735.830147	24.971610
159.737086	7745.410876	24.976627
159.916449	7735.073445	24.981645
160.193199	7735.660977	24.986663
160.089731	7736.782425	24.991680
160.359229	7728.367517	24.996698
160.028954	7756.334873	25.001715
160.659769	7759.552815	25.006733
160.581724	7766.932870	25.011751
160.624353	7765.946347	25.016768
160.788360	7771.200407	25.021786
160.839213	7785.900623	25.026803
160.932831	7790.497918	25.031821
160.826495	7799.163793	25.036839
161.084912	7827.050050	25.041856
161.581849	7827.939381	25.046874
161.450811	7844.127468	25.051891
161.836802	7848.718777	25.056909
161.726654	7871.954895	25.061927
162.078047	7880.031854	25.066944
162.130771	7877.824080	25.071962
161.995436	7893.964109	25.076979
162.818894	7897.008040	25.081997
162.572378	7902.970636	25.087015
162.945080	7921.943195	25.092032
163.482683	7917.359791	25.097050
163.824121	7922.614998	25.102067
163.742017	7918.711346	25.107085
163.778311	7925.085546	25.112103
163.875760	7916.683490	25.117120
163.835999	7927.307526	25.122138
163.894643	7939.478489	25.127155
164.411470	7943.828388	25.132173
164.846004	7943.968194	25.137191
164.391280	7953.060203	25.142208
164.977210	7964.178100	25.147226
164.997360	7986.537280	25.152243
164.981635	7977.534591	25.157261
165.176749	7981.881352	25.162279
165.213504	7996.034288	25.167296
165.858622	7993.282201	25.172314
165.833202	8004.404874	25.177331
165.976969	8003.070909	25.182349
165.848086	8017.268014	25.187367
165.978133	8033.522616	25.192384
166.397698	8032.838579	25.197402
166.319686	8048.322148	25.202419
166.644275	8058.323681	25.207437
166.954087	8061.928381	25.212455
167.099823	8073.764666	25.217472
167.374829	8085.009213	25.222490
167.128673	8104.808922	25.227507
167.511507	8106.047923	25.232525
167.754906	8106.968129	25.237543
167.489895	8127.347775	25.242560
168.120917	8131.734085	25.247578
168.231167	8137.525315	25.252595
168.218584	8155.745661	25.257613
168.557749	8159.981117	25.262631
168.506012	8164.279645	25.267648
168.482897	8166.311453	25.272666
168.597334	8177.914473	25.277683
168.640049	8187.516928	25.282701
168.736552	8209.340220	25.287719
168.931460	8235.596265	25.292736
169.225781	8241.567902	25.297754
169.847566	8254.201918	25.302771
170.520683	8280.223224	25.307789
170.676133	8274.308427	25.312807
170.624584	8285.676846	25.317824
171.075803	8277.032760	25.322842
171.152643	8280.511217	25.327859
171.570407	8265.144107	25.332877
171.829384	8264.700301	25.337895
171.627179	8258.201597	25.342912
171.896675	8253.975248	25.347930
171.980400	8251.021559	25.352947
172.309760	8243.096387	25.357965
172.637035	8240.409775	25.362983
172.691769	8241.558497	25.368000
172.623143	8235.779815	25.373018
172.825668	8242.505373	25.378035
173.195080	8246.826267	25.383053
172.902746	8241.260827	25.388071
173.397166	8260.410665	25.393088
173.530171	8263.556485	25.398106
173.511052	8273.928261	25.403123
173.844351	8278.750893	25.408141
173.629025	8276.774939	25.413159
173.759111	8281.786031	25.418176
174.152300	8285.908268	25.423194
173.647977	8290.787042	25.428211
173.979047	8306.184188	25.433229
174.092809	8315.616977	25.438247
174.219802	8328.992915	25.443264
174.456545	8331.537189	25.448282
174.421512	8354.984870	25.453299
174.266026	8359.740053	25.458317
174.866277	8372.722134	25.463335
174.892144	8399.537631	25.468352
175.321400	8405.635885	25.473370
175.355455	8430.441074	25.478387
175.745667	8446.597135	25.483405
176.001448	8449.887389	25.488423
175.976817	8466.529769	25.493440
176.561121	8482.253167	25.498458
176.673043	8496.075375	25.503475
176.827439	8493.843785	25.508493
177.095724	8490.985255	25.513511
177.145686	8514.721125	25.518528
177.494785	8516.726988	25.523546
177.617763	8522.915607	25.528563
177.526250	8539.495471	25.533581
178.104281	8541.859949	25.538599
178.037567	8554.930512	25.543616
178.231394	8559.332012	25.548634
178.740919	8575.771855	25.553651
178.885531	8584.848927	25.558669
179.152276	8586.247315	25.563687
178.917390	8586.869014	25.568704
179.051344	8585.385420	25.573722
179.375607	8605.355036	25.578739
179.865271	8619.584511	25.583757
179.732509	8610.054772	25.588775
179.675394	8619.137294	25.593792
180.198600	8639.965469	25.598810
179.909733	8650.560203	25.603827
180.009023	8657.136610	25.608845
180.315711	8665.832994	25.613863
179.980082	8686.182907	25.618880
180.284489	8688.738487	25.623898
180.947329	8708.163307	25.628915
181.013055	8713.134357	25.633933
181.587414	8733.075442	25.638951
181.396039	8742.458368	25.643968
181.884172	8748.620719	25.648986
182.212433	8756.783236	25.654003
182.288898	8767.235849	25.659021
182.709434	8771.700177	25.664039
183.094619	8768.470182	25.669056
183.990442	8747.916229	25.674074
183.788677	8744.566258	25.679092
183.790981	8753.985320	25.684109
183.826581	8738.067967	25.689127
183.834266	8748.130559	25.694144
183.840226	8739.694912	25.699162
184.299067	8729.951027	25.704180
184.144102	8726.706486	25.709197
184.786542	8724.442415	25.714215
184.507230	8734.305237	25.719232
184.537569	8745.550433	25.724250
184.901912	8757.912269	25.729268
185.038511	8769.062058	25.734285
185.308602	8769.083527	25.739303
185.396652	8782.138775	25.744320
185.211400	8788.315729	25.749338
185.186160	8796.283602	25.754356
185.509512	8811.893699	25.759373
185.701035	8823.957466	25.764391
185.962603	8843.933400	25.769408
185.976275	8852.442972	25.774426
186.715906	8860.955736	25.779444
186.472842	8878.749214	25.784461
186.630685	8893.861480	25.789479
186.519560	8913.278984	25.794496
187.126819	8920.668937	25.799514
186.991156	8940.476728	25.804532
187.113600	8954.362918	25.809549
187.374320	8968.748551	25.814567
187.230279	8986.536203	25.819584
187.150713	9001.000681	25.824602
187.712671	9028.408396	25.829620
187.826698	9055.048359	25.834637
188.131741	9063.060592	25.839655
188.249399	9078.121617	25.844672
188.621684	9091.736618	25.849690
188.768376	9106.472822	25.854708
189.043530	9129.064050	25.859725
189.527074	9131.815899	25.864743
189.714057	9160.841780	25.869760
190.338177	9168.454286	25.874778
190.712591	9160.136468	25.879796
190.802093	9168.437818	25.884813
191.544209	9177.697220	25.889831
191.757542	9178.639191	25.894848
191.783301	9154.280372	25.899866
191.839310	9142.790060	25.904884
191.844505	9147.670774	25.909901
192.316931	9134.010223	25.914919
192.395149	9130.137884	25.919936
192.801381	9121.124465	25.924954
192.993602	9127.824587	25.929972
192.554331	9133.544135	25.934989
192.554557	9130.116913	25.940007
192.888101	9151.900850	25.945024
193.094566	9155.893023	25.950042
193.221262	9153.107498	25.955060
192.996622	9161.046702	25.960077
193.253817	9179.509530	25.965095
193.211253	9202.527196	25.970112
193.324677	9204.975358	25.975130
193.820494	9223.860597	25.980148
194.228441	9231.127287	25.985165
194.642154	9240.216115	25.990183
194.799222	9254.435411	25.995200
194.870308	9257.212289	26.000218
195.140485	9252.968232	26.005236
195.088543	9269.561759	26.010253
195.746642	9266.029617	26.015271
195.911428	9271.434519	26.020288
195.950545	9272.584417	26.025306
196.141545	9280.340555	26.030324
195.910406	9300.680418	26.035341
196.120662	9299.894338	26.040359
196.663391	9307.536621	26.045376
196.649284	9315.909383	26.050394
197.169624	9320.367788	26.055412
197.221176	9326.349931	26.060429
197.929069	9337.919028	26.065447
198.075319	9348.538115	26.070464
198.316198	9348.225810	26.075482
198.338534	9341.690539	26.080500
198.500862	9352.744929	26.085517
198.623889	9348.325953	26.090535
198.955676	9341.279096	26.095552
198.785792	9358.058383	26.100570
199.014989	9369.528349	26.105588
198.823642	9383.798029	26.110605
199.003218	9381.195641	26.115623
199.431291	9400.056458	26.120640
199.739903	9404.771785	26.125658
199.893865	9416.665952	26.130676
199.928359	9434.577916	26.135693
199.716224	9438.914520	26.140711
200.316629	9459.639920	26.145728
200.667302	9467.491686	26.150746
201.236682	9470.607063	26.155764
201.053464	9483.592772	26.160781
201.308988	9498.846437	26.165799
201.710204	9503.701920	26.170816
201.905113	9503.306098	26.175834
202.211305	9493.460289	26.180852
201.791731	9510.088716	26.185869
202.141883	9518.095021	26.190887
202.311841	9521.113421	26.195904
202.368113	9525.705008	26.200922
202.745310	9543.282590	26.205940
202.792503	9556.033467	26.210957
202.941843	9565.177252	26.215975
203.267186	9575.264696	26.220992
203.332075	9583.436538	26.226010
203.733064	9607.680332	26.231028
203.632426	9615.191954	26.236045
203.487224	9624.641536	26.241063
204.220603	9634.586588	26.246080
204.664549	9650.692105	26.251098
205.119267	9660.716456	26.256116
205.485104	9671.841757	26.261133
205.511729	9668.086862	26.266151
205.771942	9668.890037	26.271168
205.924630	9682.243785	26.276186
206.366095	9694.596274	26.281204
206.431821	9711.261479	26.286221
206.488488	9705.659341	26.291239
206.557613	9703.895239	26.296256
206.697401	9720.799883	26.301274
207.042471	9723.403814	26.306292
206.836306	9733.398099	26.311309
206.754640	9738.555460	26.316327
207.335404	9753.726827	26.321344
207.073104	9766.871290	26.326362
207.411939	9783.242355	26.331380
207.550697	9813.705339	26.336397
207.972296	9829.772319	26.341415
208.072981	9846.256757	26.346432
208.074215	9858.259370	26.351450
208.518803	9873.088607	26.356468
208.725634	9896.553006	26.361485
208.816072	9906.329521	26.366503
209.389010	9929.849397	26.371520
209.172221	9950.496472	26.376538
209.711174	9955.925712	26.381556
210.077382	9968.743566	26.386573
210.793764	9974.252705	26.391591
211.115177	9970.161990	26.396608
211.237846	9972.857662	26.401626
211.535280	9967.507262	26.406644
211.456987	10000.185562	26.411661
211.735973	10005.350523	26.416679
212.161585	10002.715318	26.421696
211.964220	10008.485101	26.426714
211.968302	10017.772227	26.431732
212.512415	10036.992092	26.436749
212.511786	10039.979950	26.441767
212.638262	10036.269311	26.446784
212.734239	10071.250081	26.451802
212.915852	10071.502610	26.456820
212.921012	10081.076386	26.461837
213.192870	10101.045809	26.466855
213.521329	10104.202610	26.471872
213.301067	10126.265587	26.476890
213.717460	10141.284275	26.481908
214.097722	10156.176801	26.486925
214.008557	10179.410275	26.491943
214.548079	10184.001157	26.496960
214.744770	10203.003428	26.501978
214.908800	10201.424711	26.506996
214.755773	10235.674787	26.512013
215.126586	10242.811205	26.517031
215.859158	10253.577790	26.522048
215.575099	10271.674501	26.527066
216.016400	10282.877111	26.532084
216.457155	10297.946923	26.537101
216.576953	10297.319704	26.542119
216.830276	10312.587121	26.547136
217.192663	10335.377822	26.552154
217.566183	10323.384710	26.557172
217.456170	10342.368804	26.562189
217.885620	10359.216583	26.567207
218.209167	10353.993953	26.572224
218.214522	10374.149644	26.577242
218.611763	10384.291456	26.582260
218.886997	10383.960639	26.587277
219.136929	10387.093136	26.592295
219.315053	10406.721287	26.597312
219.327233	10412.217341	26.602330
219.692199	10406.633028	26.607348
220.068830	10418.089498	26.612365
220.115313	10440.083540	26.617383
220.377788	10438.131784	26.622400
220.527117	10450.036959	26.627418
220.514809	10461.122042	26.632436
220.765182	10475.428849	26.637453
220.735931	10481.948453	26.642471
221.294165	10501.093962	26.647488
221.616991	10501.292351	26.652506
221.939108	10508.965147	26.657524
222.221494	10520.363779	26.662541
222.519774	10527.679798	26.667559
222.808995	10515.765605	26.672576
223.176000	10518.301297	26.677594
223.673537	10530.556569	26.682612
224.311217	10537.171465	26.687629
224.073268	10529.380248	26.692647
224.467127	10519.228836	26.697664
224.445360	10524.486489	26.702682
224.685885	10527.486679	26.707700
224.649884	10525.995798	26.712717
224.675380	10534.354521	26.717735
224.926655	10526.665398	26.722752
224.789236	10532.935668	26.727770
224.868541	10530.637093	26.732788
225.443387	10539.352349	26.737805
225.249357	10553.004202	26.742823
225.403888	10559.434028	26.747840
225.345483	10585.488330	26.752858
225.903625	10593.918096	26.757876
225.837066	10610.569079	26.762893
225.875092	10632.741328	26.767911
226.466347	10645.235913	26.772928
226.466730	10655.969111	26.777946
226.635185	10679.540502	26.782964
226.858422	10696.099350	26.787981
226.751318	10722.987977	26.792999
227.169840	10733.551848	26.798016
227.225521	10760.650592	26.803034
227.474485	10783.826970	26.808052
228.162322	10795.099566	26.813069
228.324446	10819.627231	26.818087
228.858142	10838.553570	26.823104
228.976130	10861.159976	26.828122
229.245539	10865.203246	26.833140
230.029803	10867.174218	26.838157
230.877814	10879.596609	26.843175
230.833885	10875.076615	26.848192
231.085063	10877.947397	26.853210
231.370042	10864.643741	26.858228
231.609597	10867.207639	26.863245
231.441734	10874.000151	26.868263
232.049815	10883.909151	26.873280
232.178897	10893.069767	26.878298
232.325307	10891.976228	26.883316
232.423801	10895.327043	26.888333
232.621210	10901.755959	26.893351
232.640442	10901.369734	26.898368
232.865861	10922.474894	26.903386
232.677367	10926.926030	26.908404
233.376969	10929.365382	26.913421
233.324258	10957.189035	26.918439
233.582315	10961.322525	26.923456
233.436781	10983.717400	26.928474
233.418253	11001.345488	26.933492
233.740777	11017.555130	26.938509
233.847775	11036.340517	26.943527
233.978581	11052.011001	26.948544
234.310505	11090.458344	26.953562
234.588209	11108.183907	26.958580
235.194890	11124.871304	26.963597
235.016136	11147.839428	26.968615
235.593472	11163.074170	26.973632
236.133726	11181.219706	26.978650
236.482683	11195.146212	26.983668
237.013680	11191.164255	26.988685
237.112146	11204.801186	26.993703
237.395152	11215.620262	26.998720
237.451255	11220.166657	27.003738
237.708007	11220.207761	27.008756
238.009095	11221.390115	27.013773
238.184050	11243.610641	27.018791
238.333814	11243.202033	27.023808
238.438249	11246.036574	27.028826
238.482177	11276.869988	27.033844
238.945163	11277.387920	27.038861
238.853151	11286.518889	27.043879
239.047343	11290.313554	27.048896
239.292961	11322.587556	27.053914
239.623323	11342.299482	27.058932
240.203109	11350.166478	27.063949
239.965294	11370.776405	27.068967
240.476759	11385.523075	27.073984
240.815884	11406.201205	27.079002
240.917230	11415.157268	27.084020
241.317013	11422.648560	27.089037
241.561159	11438.277925	27.094055
241.877797	11448.391671	27.099072
242.005910	11465.432513	27.104090
241.933220	11476.804427	27.109108
242.326803	11486.173768	27.114125
242.465099	11506.826562	27.119143
242.788892	11518.740440	27.124160
242.946331	11545.429059	27.129178
243.138262	11547.697070	27.134196
243.555246	11560.654048	27.139213
244.061808	11572.927476	27.144231
244.663899	11571.022965	27.149248
244.977201	11583.638415	27.154266
244.882152	11594.806218	27.159284
245.541881	11597.897079	27.164301
245.549220	11615.051760	27.169319
245.764659	11620.585876	27.174336
246.100322	11619.325894	27.179354
246.252200	11636.684338	27.184372
246.410646	11642.652165	27.189389
246.731409	11647.008326	27.194407
246.802950	11662.410610	27.199424
247.197081	11669.846251	27.204442
247.484249	11673.585670	27.209460
247.679294	11677.862527	27.214477
248.032753	11703.085249	27.219495
247.972788	11713.574179	27.224512
248.196914	11709.312170	27.229530
248.117735	11739.633305	27.234548
248.309668	11741.107052	27.239565
248.606858	11768.224386	27.244583
249.062404	11772.536991	27.249600
249.329067	11792.148486	27.254618
249.463845	11810.941037	27.259636
249.815058	11820.530591	27.264653
249.947126	11833.029156	27.269671
250.183764	11844.055173	27.274688
250.272760	11865.972933	27.279706
250.306393	11878.970658	27.284724
250.684282	11901.748294	27.289741
250.460268	11915.026608	27.294759
250.685533	11934.643794	27.299776
251.209982	11962.409630	27.304794
251.374968	11990.158328	27.309812
251.779695	12007.796907	27.314829
251.773734	12026.383731	27.319847
251.891107	12049.310243	27.324864
252.644599	12063.183914	27.329882
252.668892	12084.254133	27.334900
252.980519	12104.871670	27.339917
253.296181	12125.455445	27.344935
253.268059	12141.619141	27.349952
253.767588	12165.873508	27.354970
253.805048	12197.395335	27.359988
254.564683	12205.495118	27.365005
254.729577	12230.027581	27.370023
254.932133	12240.859553	27.375040
255.367524	12254.133862	27.380058
255.591734	12276.320560	27.385076
255.916684	12293.401024	27.390093
256.264471	12301.483190	27.395111
256.933913	12317.286361	27.400128
257.506404	12318.696509	27.405146
257.477663	12326.195477	27.410164
257.557452	12339.188808	27.415181
258.055834	12356.561122	27.420199
258.542969	12361.213623	27.425216
258.648804	12361.945688	27.430234
258.551134	12376.594358	27.435252
258.897792	12381.114915	27.440269
259.047588	12396.206606	27.445287
259.427244	12411.057179	27.450304
259.775536	12419.185022	27.455322
259.560625	12437.855410	27.460340
259.966310	12442.551840	27.465357
260.046825	12464.367836	27.470375
260.080992	12491.121681	27.475392
260.546548	12495.836234	27.480410
260.482533	12519.495835	27.485428
260.956536	12528.215269	27.490445
261.175982	12565.952503	27.495463
261.539287	12567.820912	27.500480
261.761923	12591.765609	27.505498
261.624370	12619.155877	27.510516
262.190618	12633.569623	27.515533
262.624613	12657.788672	27.520551
262.661761	12677.787304	27.525568
262.928567	12697.696162	27.530586
263.253430	12708.690304	27.535604
263.860278	12718.564394	27.540621
264.051186	12731.699749	27.545639
264.001673	12749.867744	27.550656
264.589270	12753.390433	27.555674
264.918348	12777.525198	27.560692
265.229798	12785.164652	27.565709
265.354317	12796.478462	27.570727
265.339259	12827.250832	27.575744
265.997267	12831.789073	27.580762
265.992391	12839.772770	27.585780
266.455908	12843.439681	27.590797
267.083218	12857.532671	27.595815
267.069138	12873.220279	27.600832
267.549889	12881.825269	27.605850
267.423723	12891.316028	27.610868
268.127556	12901.646432	27.615885
268.401494	12902.442699	27.620903
268.452572	12912.059123	27.625920
268.967182	12928.735787	27.630938
269.407362	12944.091852	27.635956
269.295889	12942.519120	27.640973
269.651726	12951.249579	27.645991
269.919950	12970.468198	27.651008
270.569134	12955.437646	27.656026
270.951805	12963.359706	27.661044
271.449691	12957.220609	27.666061
271.647835	12957.486118	27.671079
271.969915	12981.523091	27.676096
271.911398	12979.566168	27.681114
272.145318	12989.956683	27.686132
272.271645	12975.174917	27.691149
272.211270	12987.395283	27.696167
272.098209	13008.709310	27.701184
272.323565	13009.031623	27.706202
271.964264	13034.577156	27.711220
272.097764	13051.175842	27.716237
272.674517	13085.253215	27.721255
272.542522	13116.851560	27.726272
272.970509	13145.094588	27.731290
273.317659	13174.680184	27.736308
273.755689	13196.511529	27.741325
274.213685	13219.778476	27.746343
274.142627	13251.863112	27.751360
274.877669	13273.041573	27.756378
274.908125	13298.862729	27.761396
275.188502	13321.126326	27.766413
275.751355	13348.755541	27.771431
276.192969	13374.928747	27.776448
276.475213	13383.643681	27.781466
276.724873	13424.285676	27.786484
277.390362	13416.916668	27.791501
277.360241	13440.425204	27.796519
277.902504	13458.134768	27.801536
278.668978	13468.040272	27.806554
278.691694	13481.107336	27.811572
278.931531	13487.988660	27.816589
279.707537	13483.458228	27.821607
279.298355	13502.301820	27.826624
280.010716	13503.946594	27.831642
279.910179	13507.719792	27.836660
280.032441	13509.508264	27.841677
280.461004	13525.706952	27.846695
280.547730	13539.729269	27.851712
281.177847	13545.489281	27.856730
281.324455	13565.123479	27.861748
281.246099	13567.934589	27.866765
281.647056	13581.313602	27.871783
281.897374	13613.131079	27.876800
281.673021	13615.499103	27.881818
281.340209	13640.410571	27.886836
282.323382	13663.843471	27.891853
283.008538	13677.121838	27.896871
283.178459	13700.965282	27.901888
283.652428	13701.670563	27.906906
284.118404	13722.172265	27.911924
284.251311	13731.521381	27.916941
284.470372	13737.405505	27.921959
285.171090	13740.882231	27.926976
285.775441	13727.932901	27.931994
286.151547	13738.972544	27.937012
286.185417	13759.146432	27.942029
286.863919	13766.365644	27.947047
286.314699	13766.585885	27.952064
286.745558	13772.447907	27.957082
286.939154	13794.033504	27.962100
287.079719	13798.986978	27.967117
287.282779	13805.115024	27.972135
287.311323	13825.677645	27.977152
287.634430	13849.646361	27.982170
287.893965	13873.272944	27.987188
287.836879	13895.546298	27.992205
288.403135	13912.643836	27.997223
288.356807	13946.943277	28.002240
288.874548	13958.970705	28.007258
289.248073	13988.814893	28.012276
289.468582	14013.480771	28.017293
289.781442	14036.499495	28.022311
289.842000	14058.809648	28.027328
290.415923	14076.465593	28.032346
290.766153	14093.118028	28.037364
291.143142	14114.521297	28.042381
291.944876	14133.831099	28.047399
291.965509	14147.017263	28.052416
292.147879	14164.656874	28.057434
292.726752	14172.582146	28.062452
292.770096	14202.251611	28.067469
292.919676	14207.637121	28.072487
293.061288	14222.214895	28.077504
293.812256	14230.911416	28.082522
293.847897	14262.650302	28.087540
294.021980	14275.244406	28.092557
294.778722	14290.084068	28.097575
294.519160	14304.642407	28.102592
294.645368	14331.676645	28.107610
294.953361	14334.875619	28.112628
295.468204	14352.606613	28.117645
295.991763	14370.255743	28.122663
296.176935	14398.061793	28.127680
296.404338	14410.536525	28.132698
296.684601	14429.026568	28.137716
296.779305	14448.101694	28.142733
297.073534	14458.556886	28.147751
297.166645	14489.488782	28.152768
297.531305	14507.026585	28.157786
298.055980	14528.917358	28.162804
298.144685	14566.366340	28.167821
298.546054	14570.220838	28.172839
298.497071	14603.740278	28.177856
299.035726	14615.017461	28.182874
299.230682	14638.087181	28.187892
299.497571	14667.407068	28.192909
299.921554	14680.537135	28.197927
300.254509	14718.594017	28.202944
300.762197	14734.706252	28.207962
301.279109	14756.691658	28.212980
301.139825	14775.938096	28.217997
301.235520	14799.438036	28.223015
301.437553	14827.634409	28.228032
302.021731	14847.098983	28.233050
301.981353	14881.984140	28.238068
301.812083	14910.650972	28.243085
302.091847	14931.031620	28.248103
302.618189	14970.586504	28.253120
303.094790	15007.722525	28.258138
303.589359	15030.281164	28.263156
303.378888	15063.110422	28.268173
304.234575	15086.395392	28.273191
304.620756	15120.968344	28.278208
305.094402	15135.540457	28.283226
305.362487	15161.941707	28.288244
305.741643	15193.078099	28.293261
306.203496	15207.756333	28.298279
306.635825	15231.637402	28.303296
307.178664	15248.300552	28.308314
307.845063	15253.500094	28.313332
307.692205	15269.776507	28.318349
308.034358	15288.319956	28.323367
308.440497	15303.712438	28.328384
309.258365	15319.672775	28.333402
309.915678	15327.927226	28.338420
309.992981	15329.362627	28.343437
310.638434	15326.138786	28.348455
310.736202	15335.302522	28.353472
311.108577	15342.317964	28.358490
311.401490	15356.727362	28.363508
311.353765	15367.208636	28.368525
311.769248	15358.049944	28.373543
311.810001	15370.048239	28.378560
311.993938	15373.022774	28.383578
312.124528	15383.036855	28.388596
312.209500	15401.506286	28.393613
311.785290	15400.585920	28.398631
312.075376	15433.044803	28.403648
312.148204	15460.469929	28.408666
312.780244	15481.102992	28.413684
312.716367	15508.373501	28.418701
313.392839	15539.960863	28.423719
313.705463	15575.891989	28.428736
313.683359	15605.337155	28.433754
314.077957	15640.477234	28.438772
313.723091	15679.341496	28.443789
314.480362	15706.802627	28.448807
314.801051	15737.880703	28.453824
314.958354	15777.533868	28.458842
315.909361	15804.867375	28.463860
316.040379	15827.524092	28.468877
317.095631	15848.185966	28.473895
317.460124	15862.845213	28.478912
317.959963	15880.845251	28.483930
318.660338	15890.334786	28.488948
318.783619	15907.590713	28.493965
319.455406	15911.578889	28.498983
319.523246	15920.636155	28.504000
319.626715	15940.698306	28.509018
320.022035	15957.798891	28.514036
320.600722	15967.755442	28.519053
321.107285	15977.022872	28.524071
321.024367	15990.239283	28.529088
321.049865	16006.946151	28.534106
321.444812	16014.533391	28.539124
321.513641	16046.424487	28.544141
322.173060	16058.604149	28.549159
322.126796	16084.315112	28.554176
322.152331	16112.171890	28.559194
323.094734	16132.594935	28.564212
323.106576	16161.828759	28.569229
323.155815	16180.183797	28.574247
323.604061	16213.952309	28.579264
323.455923	16233.621272	28.584282
324.322972	16262.098631	28.589300
324.248277	16285.585738	28.594317
324.560713	16313.031106	28.599335
324.735064	16338.075660	28.604352
324.628176	16372.401527	28.609370
325.444555	16402.744831	28.614388
325.409278	16434.378637	28.619405
325.739187	16458.884375	28.624423
326.751559	16503.309592	28.629440
326.959474	16523.125961	28.634458
327.831868	16539.051336	28.639476
328.059793	16567.290365	28.644493
328.617897	16583.502962	28.649511
328.919813	16590.560963	28.654528
329.755490	16591.377803	28.659546
330.160844	16607.720647	28.664564
330.390180	16607.413360	28.669581
330.805862	16604.747311	28.674599
331.011374	16625.171144	28.679616
330.923505	16636.758875	28.684634
331.151193	16642.472304	28.689652
331.399946	16675.979574	28.694669
331.594967	16687.646549	28.699687
331.697579	16703.897918	28.704704
331.712407	16730.691885	28.709722
332.507621	16750.094155	28.714740
332.498579	16772.873903	28.719757
332.718627	16791.927085	28.724775
333.020630	16827.039823	28.729792
333.444605	16856.483264	28.734810
334.002013	16883.703141	28.739828
334.085225	16900.054190	28.744845
334.477335	16917.909865	28.749863
335.133142	16940.763495	28.754880
335.533260	16965.699357	28.759898
335.979049	16991.076726	28.764916
335.853066	17018.785996	28.769933
336.303055	17049.486501	28.774951
336.798135	17068.861760	28.779968
337.114278	17091.687104	28.784986
337.686643	17106.830487	28.790004
337.928645	17136.494788	28.795021
338.255235	17158.703603	28.800039
338.627312	17179.872048	28.805056
338.641766	17196.189452	28.810074
339.034377	17221.306704	28.815092
339.409689	17242.378508	28.820109
339.943287	17268.564182	28.825127
340.143365	17302.520895	28.830144
340.629331	17324.516588	28.835162
341.129128	17342.847709	28.840180
341.218372	17365.754881	28.845197
341.494151	17385.234306	28.850215
341.916121	17417.428518	28.855232
342.371692	17437.936609	28.860250
342.802963	17457.003222	28.865268
342.748889	17487.978528	28.870285
343.050954	17499.332916	28.875303
343.533304	17527.460597	28.880320
343.507225	17559.405531	28.885338
344.015982	17576.340145	28.890356
344.328324	17606.388933	28.895373
344.641957	17637.683017	28.900391
345.196629	17664.143171	28.905408
345.425217	17692.856950	28.910426
345.929789	17706.536856	28.915444
346.050413	17747.383393	28.920461
346.357307	17759.115501	28.925479
346.966501	17784.786110	28.930496
347.456203	17812.998146	28.935514
348.173443	17819.376942	28.940532
348.535563	17848.621474	28.945549
348.414396	17851.251454	28.950567
349.120171	17873.246459	28.955584
349.220066	17892.830717	28.960602
349.366458	17901.844065	28.965620
349.965804	17933.006177	28.970637
350.111168	17954.783599	28.975655
350.373285	17971.292644	28.980672
350.582383	17994.646798	28.985690
350.724845	18028.666884	28.990708
351.325263	18055.170267	28.995725
351.319257	18078.794736	29.000743
351.910303	18112.296670	29.005760
352.156009	18143.748387	29.010778
352.493981	18162.844407	29.015796
353.364833	18192.196272	29.020813
353.294547	18216.191413	29.025831
353.924685	18241.228497	29.030848
353.991472	18278.479885	29.035866
354.082164	18305.290168	29.040884
354.757053	18324.166242	29.045901
355.125244	18358.485702	29.050919
355.540733	18382.782519	29.055936
356.002264	18417.373045	29.060954
356.952135	18427.414089	29.065972
357.624331	18429.734763	29.070989
358.366055	18445.194041	29.076007
358.877837	18452.011908	29.081024
358.853558	18454.809840	29.086042
359.456920	18464.249691	29.091060
359.694247	18475.751426	29.096077
360.068032	18491.363672	29.101095
360.103736	18492.940489	29.106112
360.000075	18517.867255	29.111130
360.749108	18531.073948	29.116148
360.549103	18555.793400	29.121165
360.499215	18578.180560	29.126183
361.175915	18596.433865	29.131200
361.371779	18633.135748	29.136218
362.085390	18649.266947	29.141236
362.071094	18669.601661	29.146253
362.637241	18709.346219	29.151271
362.995217	18723.783642	29.156288
363.040491	18752.171177	29.161306
363.441479	18782.777625	29.166324
363.702502	18806.740477	29.171341
364.165173	18845.724228	29.176359
364.401020	18871.487291	29.181376
364.577978	18907.220216	29.186394
364.685020	18933.926217	29.191412
365.174230	18977.854854	29.196429
365.456968	19009.270310	29.201447
365.977176	19040.181587	29.206464
365.872978	19076.644176	29.211482
366.628864	19096.480046	29.216500
367.352483	19130.785893	29.221517
367.588870	19155.418821	29.226535
368.018769	19167.217554	29.231552
368.099981	19207.924607	29.236570
368.792754	19229.251957	29.241588
369.581938	19263.665090	29.246605
369.807284	19284.216475	29.251623
370.145985	19299.703043	29.256640
370.431883	19324.100689	29.261658
371.044691	19346.031576	29.266676
371.615604	19376.841756	29.271693
371.240249	19399.345697	29.276711
371.542509	19425.214901	29.281728
372.080448	19457.792058	29.286746
372.179827	19492.913566	29.291764
372.526168	19523.412472	29.296781
372.710823	19564.791680	29.301799
373.289682	19597.021522	29.306816
373.700585	19640.987382	29.311834
373.556815	19671.431797	29.316852
373.967789	19709.366843	29.321869
373.953203	19751.758226	29.326887
374.963640	19779.553208	29.331904
375.267299	19830.215421	29.336922
375.304435	19873.981048	29.341940
375.992508	19912.085075	29.346957
376.364517	19953.504079	29.351975
377.121213	19995.084310	29.356992
377.476893	20022.337550	29.362010
377.770017	20063.029264	29.367028
378.761394	20092.677573	29.372045
378.925723	20125.313739	29.377063
379.682330	20148.472981	29.382080
380.163859	20170.003288	29.387098
380.184988	20196.550984	29.392116
381.006504	20219.691316	29.397133
381.154524	20256.706090	29.402151
381.584487	20267.501174	29.407168
381.744845	20301.675723	29.412186
382.578041	20318.820830	29.417204
382.995103	20335.878015	29.422221
383.239599	20363.472523	29.427239
383.816565	20384.535785	29.432256
384.171979	20402.286353	29.437274
384.279778	20426.746071	29.442292
384.729541	20440.380839	29.447309
384.757360	20487.060415	29.452327
385.309964	20499.726794	29.457344
385.858019	20527.775701	29.462362
386.377812	20552.049888	29.467380
387.035991	20566.659774	29.472397
386.976324	20591.202041	29.477415
387.487800	20614.471736	29.482432
387.332542	20640.848523	29.487450
387.556086	20664.328466	29.492468
388.132296	20688.321967	29.497485
388.357989	20717.836112	29.502503
388.555507	20735.271918	29.507520
388.671847	20771.457526	29.512538
389.279728	20805.441287	29.517556
389.900770	20831.658525	29.522573
389.640532	20876.169929	29.527591
390.323838	20904.133208	29.532608
390.784390	20940.840464	29.537626
391.699744	20966.329431	29.542644
392.185773	20993.907225	29.547661
392.387756	21030.047168	29.552679
392.938693	21052.965373	29.557696
393.350880	21077.608815	29.562714
393.753209	21110.623956	29.567732
394.515761	21132.085252	29.572749
394.416076	21160.728732	29.577767
394.911014	21186.189159	29.582784
395.415182	21209.358427	29.587802
395.568850	21237.838778	29.592820
395.737953	21257.344115	29.597837
395.894580	21296.395422	29.602855
396.737216	21331.213596	29.607872
396.855565	21367.887383	29.612890
397.000563	21399.255187	29.617908
397.447122	21430.609215	29.622925
397.333444	21484.616777	29.627943
398.209337	21523.507497	29.632960
398.619861	21556.295024	29.637978
398.927094	21592.485931	29.642996
399.899257	21629.338803	29.648013
400.339417	21674.724136	29.653031
400.580384	21699.700590	29.658048
401.078921	21735.111558	29.663066
401.647961	21771.803593	29.668084
401.910298	21790.669102	29.673101
402.064885	21826.574434	29.678119
402.284371	21855.593307	29.683136
402.821155	21888.955917	29.688154
402.888268	21935.044529	29.693172
403.513719	21967.952133	29.698189
403.486195	22013.293936	29.703207
404.470283	22049.256279	29.708224
404.607439	22082.109011	29.713242
405.011413	22131.732719	29.718260
405.902868	22148.229458	29.723277
406.471374	22190.239982	29.728295
407.034322	22206.723689	29.733312
407.304916	22243.360650	29.738330
407.840174	22270.572529	29.743348
408.409449	22293.971816	29.748365
408.877189	22312.499925	29.753383
409.501452	22334.111021	29.758400
409.935217	22345.983854	29.763418
410.405020	22369.400292	29.768436
410.919520	22380.672679	29.773453
410.798652	22393.671936	29.778471
410.671056	22418.468170	29.783488
411.231475	22444.890679	29.788506
411.611968	22474.703043	29.793524
412.115479	22507.594739	29.798541
412.083532	22539.297741	29.803559
412.522892	22568.970868	29.808576
413.010920	22609.469684	29.813594
413.167095	22641.064940	29.818612
413.822080	22668.364172	29.823629
413.598536	22708.802232	29.828647
414.130297	22762.644869	29.833664
414.353572	22792.516269	29.838682
414.335648	22851.982402	29.843700
415.225232	22888.205571	29.848717
415.430150	22946.854795	29.853735
415.832461	22984.306594	29.858752
416.394795	23036.044242	29.863770
416.857237	23079.292599	29.868788
418.007889	23105.977702	29.873805
418.467869	23149.920559	29.878823
419.319836	23178.785977	29.883840
420.522127	23191.003968	29.888858
420.872776	23208.887599	29.893876
421.395742	23211.866940	29.898893
422.060868	23239.546994	29.903911
422.545923	23248.718055	29.908928
423.367506	23260.704852	29.913946
423.485004	23283.324996	29.918964
423.657297	23284.270107	29.923981
424.093287	23308.043734	29.928999
424.341998	23327.427397	29.934016
424.767571	23331.429616	29.939034
424.772965	23357.008718	29.944052
424.684450	23378.156615	29.949069
425.051484	23405.824939	29.954087
425.851462	23419.812123	29.959104
426.518735	23446.990637	29.964122
426.451840	23474.780745	29.969140
427.183412	23506.089741	29.974157
427.942344	23538.075406	29.979175
428.311013	23563.598870	29.984192
428.452677	23587.092134	29.989210
428.493203	23616.302366	29.994228
428.734399	23646.282579	29.999245
429.019185	23685.500316	30.004263
429.188107	23713.023295	30.009280
429.934139	23755.918803	30.014298
429.880436	23807.609790	30.019316
430.594649	23838.013952	30.024333
430.610807	23881.561604	30.029351
430.817436	23924.196693	30.034368
431.431203	23953.186247	30.039386
431.518193	24005.383629	30.044404
432.194850	24047.531578	30.049421
432.518009	24091.888265	30.054439
432.594158	24136.164377	30.059456
433.438618	24174.113927	30.064474
433.666831	24215.446471	30.069492
434.604287	24254.582048	30.074509
435.524151	24283.377762	30.079527
435.911403	24326.743081	30.084544
436.504867	24358.973123	30.089562
436.788193	24394.499018	30.094580
436.930647	24427.058821	30.099597
437.820981	24462.171711	30.104615
437.850647	24491.022536	30.109632
438.250225	24532.061509	30.114650
438.335904	24579.204428	30.119668
438.822311	24615.071344	30.124685
439.543377	24662.383191	30.129703
439.467570	24703.352625	30.134720
440.644450	24742.918286	30.139738
440.871198	24784.886476	30.144756
441.600139	24814.993328	30.149773
442.308756	24854.595328	30.154791
442.524926	24886.963563	30.159808
443.324630	24917.673579	30.164826
443.717782	24959.979592	30.169844
444.483158	24979.595175	30.174861
444.568749	25012.301465	30.179879
445.099363	25044.972563	30.184896
445.061917	25075.712757	30.189914
445.581946	25125.066552	30.194932
446.215740	25149.748855	30.199949
446.612190	25190.433473	30.204967
446.819868	25240.162876	30.209984
447.402725	25264.175859	30.215002
447.603510	25311.215874	30.220020
447.714702	25344.861596	30.225037
448.218312	25401.644681	30.230055
448.606484	25445.107282	30.235072
448.946659	25491.448833	30.240090
449.313540	25547.470348	30.245108
449.953005	25579.761032	30.250125
450.824294	25614.683951	30.255143
451.107914	25653.647680	30.260160
451.815692	25694.904734	30.265178
452.620731	25744.353408	30.270196
453.092249	25769.524972	30.275213
453.608921	25810.228298	30.280231
453.859310	25843.800660	30.285248
454.359528	25877.557407	30.290266
454.638259	25914.166078	30.295284
455.160925	25951.562687	30.300301
455.511410	25993.518907	30.305319
455.908602	26023.662632	30.310336
456.559851	26057.684074	30.315354
456.510529	26089.756193	30.320372
456.886677	26131.922865	30.325389
457.962336	26161.316485	30.330407
458.202451	26196.206775	30.335424
458.744482	26230.714161	30.340442
459.091967	26270.980668	30.345460
459.139447	26296.720942	30.350477
459.701035	26331.398683	30.355495
460.078430	26382.581816	30.360512
460.955048	26416.240409	30.365530
461.000602	26461.240658	30.370548
461.486941	26506.768040	30.375565
461.845931	26548.837711	30.380583
462.416829	26592.013182	30.385600
462.682480	26637.247475	30.390618
462.936611	26684.398787	30.395636
463.632153	26731.616550	30.400653
463.976240	26776.247825	30.405671
464.383557	26827.610112	30.410688
465.275727	26866.257753	30.415706
465.199196	26916.643209	30.420724
465.640026	26967.539567	30.425741
466.411785	27018.653834	30.430759
466.694089	27073.114196	30.435776
467.183416	27113.661205	30.440794
467.767913	27172.149271	30.445812
468.006177	27223.967594	30.450829
468.521471	27266.671572	30.455847
469.167231	27315.656695	30.460864
469.763629	27368.300591	30.465882
470.519937	27406.887530	30.470900
470.903735	27458.344037	30.475917
471.485855	27499.626903	30.480935
472.168366	27537.646277	30.485952
472.623908	27580.701990	30.490970
473.197376	27621.484997	30.495988
473.617878	27670.692699	30.501005
473.946749	27702.201338	30.506023
474.083257	27762.411858	30.511040
475.279517	27777.319026	30.516058
475.510911	27827.067517	30.521076
475.780950	27867.451934	30.526093
476.483994	27900.505839	30.531111
476.461260	27947.562868	30.536128
477.157482	27997.525604	30.541146
477.731936	28034.595997	30.546164
477.920228	28086.690452	30.551181
478.558770	28125.999566	30.556199
478.733705	28177.503439	30.561216
479.408877	28218.197842	30.566234
479.841137	28268.522083	30.571252
479.792249	28319.316983	30.576269
480.680408	28361.126809	30.581287
480.958463	28414.696034	30.586304
481.164526	28454.130471	30.591322
481.840302	28505.622050	30.596340
481.987535	28554.241731	30.601357
482.946416	28602.195568	30.606375
483.223596	28661.583672	30.611392
483.513890	28710.876547	30.616410
484.303879	28753.568629	30.621428
484.637610	28813.319857	30.626445
485.094081	28853.100359	30.631463
485.513939	28908.139163	30.636480
486.144387	28956.554103	30.641498
486.385628	29016.085230	30.646516
487.043441	29065.505432	30.651533
487.536076	29113.635212	30.656551
488.024597	29174.569573	30.661568
488.794981	29215.754801	30.666586
489.556257	29260.809964	30.671604
489.901089	29308.407132	30.676621
490.540217	29348.343612	30.681639
491.132051	29399.372596	30.686656
491.770232	29437.387906	30.691674
492.052011	29490.152021	30.696692
492.556260	29538.334609	30.701709
493.806424	29564.391052	30.706727
494.257559	29605.565636	30.711744
495.028371	29638.134756	30.716762
495.750570	29669.213510	30.721780
496.267094	29709.550450	30.726797
496.516284	29728.540439	30.731815
496.745084	29774.259262	30.736832
497.003905	29802.372792	30.741850
497.561753	29850.931996	30.746868
497.917526	29886.144267	30.751885
498.583295	29909.158667	30.756903
498.947469	29947.190475	30.761920
499.200725	29986.465639	30.766938
500.064946	30033.780133	30.771956
500.017397	30082.702445	30.776973
500.619918	30124.805214	30.781991
501.162841	30170.196719	30.787008
501.516239	30218.634196	30.792026
501.668358	30267.895140	30.797044
502.285089	30316.839955	30.802061
502.829567	30356.678184	30.807079
503.275852	30423.029282	30.812096
503.456394	30470.572530	30.817114
504.430507	30513.107951	30.822132
505.570578	30549.543986	30.827149
506.282939	30594.156551	30.832167
506.607195	30630.839827	30.837184
507.399199	30664.880803	30.842202
507.826127	30703.370488	30.847220
508.021326	30740.732441	30.852237
509.055478	30769.263705	30.857255
509.368663	30800.774258	30.862272
509.582011	30839.326078	30.867290
509.965053	30862.910821	30.872308
510.009874	30901.523208	30.877325
510.654821	30941.579043	30.882343
511.248551	30988.566932	30.887360
511.588693	31030.041531	30.892378
511.966414	31079.483799	30.897396
512.178936	31129.708683	30.902413
512.656236	31178.114925	30.907431
512.532283	31230.461473	30.912448
513.088659	31280.851909	30.917466
513.620934	31337.955361	30.922484
513.988490	31406.011848	30.927501
514.805976	31460.794804	30.932519
515.551244	31520.355264	30.937536
516.096840	31572.351419	30.942554
516.604646	31632.088633	30.947572
516.691581	31698.566017	30.952589
517.585675	31741.787089	30.957607
518.105987	31797.647585	30.962624
518.618160	31852.540862	30.967642
519.510281	31899.729324	30.972660
520.088394	31959.853203	30.977677
520.719284	32007.326543	30.982695
521.311215	32071.522425	30.987712
521.384554	32122.064274	30.992730
522.055299	32173.425373	30.997748
522.546947	32246.295205	31.002765
523.341731	32277.845767	31.007783
523.859493	32335.033790	31.012800
524.368767	32383.611389	31.017818
525.209478	32436.941717	31.022836
525.560333	32489.636621	31.027853
526.698241	32531.817453	31.032871
527.127971	32574.315385	31.037888
527.617099	32616.569712	31.042906
527.655619	32667.466203	31.047924
528.149444	32723.441427	31.052941
528.429091	32771.207353	31.057959
529.022211	32824.991517	31.062976
529.222220	32886.521368	31.067994
530.216145	32934.054886	31.073012
530.315258	32986.904840	31.078029
531.334127	33044.255422	31.083047
531.943762	33102.042390	31.088064
532.770983	33146.221930	31.093082
533.416983	33187.705934	31.098100
533.922811	33239.467589	31.103117
534.327111	33277.250309	31.108135
534.810470	33331.644955	31.113152
535.172687	33380.143150	31.118170
536.056879	33422.975496	31.123188
536.120705	33471.275745	31.128205
536.770697	33517.471657	31.133223
537.267645	33556.097508	31.138240
538.295992	33603.961438	31.143258
538.738797	33630.383126	31.148276
539.036506	33676.617716	31.153293
539.612114	33717.165054	31.158311
540.207739	33758.643229	31.163328
540.287833	33808.024100	31.168346
541.029348	33842.679436	31.173364
541.213215	33890.786661	31.178381
541.772137	33938.274290	31.183399
542.738419	33991.502512	31.188416
542.526300	34042.048173	31.193434
543.571160	34078.968528	31.198452
544.042773	34131.167833	31.203469
544.659543	34174.934646	31.208487
545.634191	34212.227097	31.213504
546.049302	34262.927860	31.218522
546.880281	34301.201406	31.223540
547.252768	34350.129682	31.228557
547.961576	34401.528508	31.233575
548.639903	34439.727509	31.238592
548.717431	34489.318986	31.243610
549.320319	34533.467782	31.248628
549.439767	34591.756973	31.253645
549.965749	34655.616742	31.258663
550.340933	34707.843705	31.263680
550.563695	34770.932076	31.268698
550.797766	34826.904689	31.273716
551.414256	34895.739724	31.278733
551.613640	34971.650114	31.283751
552.514535	35040.285471	31.288768
552.388680	35116.719314	31.293786
553.358248	35192.877415	31.298804
554.061056	35262.787960	31.303821
554.725170	35327.450212	31.308839
555.165836	35399.981718	31.313856
556.348101	35456.781729	31.318874
557.562968	35515.252330	31.323892
557.909287	35567.480401	31.328909
558.469614	35622.389548	31.333927
559.279940	35680.030442	31.338944
559.515044	35738.306654	31.343962
560.323986	35787.312376	31.348980
560.447927	35848.587582	31.353997
561.101825	35900.637656	31.359015
561.966299	35960.817355	31.364032
562.309695	36010.515782	31.369050
563.084090	36065.560034	31.374068
563.915684	36128.684529	31.379085
564.455235	36162.201578	31.384103
565.021156	36217.487177	31.389120
565.206061	36279.457269	31.394138
565.716753	36329.935951	31.399156
566.370193	36383.755095	31.404173
566.754818	36439.372292	31.409191
567.577730	36491.234118	31.414208
568.039117	36538.518006	31.419226
568.593811	36575.565324	31.424244
569.478643	36626.842446	31.429261
570.245678	36661.830244	31.434279
570.997830	36698.932363	31.439296
571.544530	36753.635771	31.444314
571.902438	36778.735081	31.449332
572.365991	36829.409458	31.454349
572.950868	36870.524128	31.459367
573.432764	36921.867961	31.464384
573.741697	36975.167072	31.469402
574.354171	37020.245142	31.474420
574.784057	37067.674687	31.479437
575.319123	37130.487294	31.484455
575.753281	37178.181547	31.489472
576.097555	37249.843613	31.494490
576.605340	37301.174604	31.499508
576.939435	37376.077591	31.504525
577.128539	37442.773216	31.509543
577.644682	37505.492495	31.514560
578.203014	37585.894679	31.519578
578.995593	37655.107709	31.524596
579.840469	37731.660804	31.529613
580.552724	37801.304831	31.534631
581.399061	37862.191536	31.539648
581.878311	37936.181747	31.544666
583.023579	37990.012898	31.549684
583.334249	38051.531808	31.554701
583.608791	38113.682152	31.559719
584.403119	38174.995496	31.564736
584.931799	38243.046918	31.569754
585.297425	38303.231410	31.574772
586.174123	38364.329240	31.579789
586.797785	38419.785221	31.584807
587.680594	38481.816808	31.589824
588.186593	38544.487706	31.594842
588.713386	38594.815187	31.599860
589.568514	38645.894704	31.604877
590.287240	38700.991149	31.609895
591.519248	38736.443074	31.614912
592.517347	38782.160228	31.619930
593.501113	38825.152414	31.624948
594.048728	38851.172278	31.629965
594.693008	38884.815274	31.634983
595.058743	38919.939283	31.640000
595.346247	38962.883765	31.645018
595.860056	38993.957502	31.650036
596.259637	39039.291677	31.655053
596.759383	39090.796361	31.660071
597.370264	39135.295869	31.665088
597.877818	39188.763097	31.670106
598.121785	39240.921311	31.675124
598.354540	39293.233126	31.680141
598.915967	39350.861928	31.685159
599.598052	39398.124842	31.690176
599.746474	39456.358260	31.695194
600.223184	39506.223261	31.700212
600.602365	39564.205965	31.705229
600.902787	39626.798950	31.710247
601.737519	39687.873630	31.715264
602.204160	39758.056472	31.720282
602.730806	39824.630268	31.725300
603.403097	39901.910184	31.730317
603.367543	39970.967560	31.735335
604.310994	40035.137629	31.740352
604.634921	40112.635960	31.745370
605.219312	40184.811309	31.750388
605.865778	40268.925996	31.755405
606.374073	40344.565735	31.760423
607.153571	40423.550091	31.765440
607.800582	40503.564615	31.770458
608.738142	40570.045426	31.775476
609.481672	40656.001651	31.780493
610.112551	40725.437013	31.785511
610.617232	40795.187876	31.790528
611.128657	40871.801642	31.795546
611.587732	40950.685271	31.800564
612.292150	41018.713630	31.805581
612.509564	41110.659825	31.810599
613.600111	41183.270120	31.815616
614.215703	41270.681344	31.820634
614.941775	41350.016613	31.825652
615.655899	41420.921078	31.830669
615.892638	41493.536780	31.835687
616.719352	41575.460558	31.840704
617.573886	41642.581418	31.845722
618.153220	41714.476239	31.850740
619.209590	41787.132629	31.855757
620.072219	41847.941247	31.860775
620.715624	41919.551188	31.865792
621.535052	41988.898957	31.870810
622.114009	42048.639105	31.875828
622.471069	42102.778290	31.880845
623.033393	42174.655692	31.885863
623.772784	42229.623297	31.890880
624.223091	42313.673452	31.895898
624.720197	42384.148286	31.900916
625.640878	42449.975617	31.905933
625.705702	42520.657637	31.910951
626.563514	42585.691053	31.915968
627.266433	42660.100653	31.920986
627.769427	42726.802525	31.926004
629.059077	42796.666339	31.931021
629.476361	42863.661245	31.936039
630.202440	42916.391279	31.941056
631.124414	42982.393922	31.946074
631.730101	43040.257047	31.951092
632.666571	43100.987613	31.956109
632.836397	43154.991397	31.961127
633.778078	43197.893553	31.966144
634.346395	43257.304662	31.971162
634.630901	43314.929997	31.976180
635.921657	43356.819107	31.981197
636.634917	43401.832273	31.986215
637.016974	43450.865144	31.991232
637.560415	43504.202809	31.996250
638.181602	43547.520644	32.001268
638.437066	43602.729900	32.006285
638.907059	43656.538443	32.011303
639.934454	43716.690193	32.016320
640.335614	43784.423721	32.021338
640.761545	43837.883508	32.026356
641.984456	43878.793882	32.031373
642.692877	43933.746516	32.036391
643.243773	43991.615633	32.041408
643.540476	44045.941266	32.046426
644.874567	44095.813720	32.051444
645.418607	44141.227101	32.056461
645.842827	44197.861759	32.061479
646.484323	44255.122499	32.066496
647.068937	44319.583466	32.071514
647.046306	44377.965692	32.076532
647.618377	44442.909214	32.081549
648.445882	44513.862762	32.086567
649.267000	44580.387216	32.091584
649.939652	44651.652015	32.096602
650.238084	44710.434991	32.101620
651.404630	44775.827279	32.106637
651.902236	44839.101768	32.111655
652.488661	44906.782307	32.116672
653.159585	44987.102357	32.121690
653.413151	45042.660346	32.126708
653.911690	45118.646238	32.131725
654.348909	45204.539942	32.136743
655.211285	45267.383886	32.141760
655.901558	45350.885378	32.146778
656.633384	45420.191296	32.151796
657.249596	45489.204632	32.156813
658.521616	45567.851476	32.161831
659.548945	45621.557484	32.166848
660.099469	45689.303803	32.171866
660.820951	45753.139845	32.176884
661.514570	45805.864549	32.181901
662.547123	45870.048765	32.186919
663.155367	45922.055747	32.191936
664.162930	45965.492929	32.196954
665.510017	46001.943218	32.201972
667.469718	46012.566046	32.206989
667.549894	46044.310009	32.212007
668.068379	46080.037085	32.217024
668.570917	46117.794458	32.222042
669.136308	46157.928666	32.227060
669.486254	46188.925555	32.232077
669.489997	46230.769927	32.237095
670.321375	46280.468977	32.242112
671.082545	46329.235902	32.247130
670.697822	46373.130441	32.252148
671.136535	46426.197395	32.257165
671.135770	46483.934903	32.262183
671.876497	46550.208416	32.267200
672.073453	46619.082907	32.272218
672.520413	46701.365561	32.277236
673.209976	46775.471466	32.282253
673.444405	46863.927622	32.287271
674.053234	46958.503873	32.292288
674.592128	47042.746139	32.297306
674.895956	47135.938509	32.302324
675.660815	47222.382063	32.307341
676.433154	47325.570006	32.312359
677.022283	47424.346142	32.317376
677.749774	47523.790756	32.322394
677.617702	47631.935937	32.327412
678.512122	47734.006051	32.332429
679.086082	47843.266386	32.337447
680.337950	47962.015902	32.342464
680.854183	48050.950371	32.347482
681.174296	48169.620744	32.352500
682.014740	48275.540469	32.357517
682.726826	48389.461059	32.362535
683.369239	48494.490477	32.367552
684.180823	48606.617072	32.372570
684.835976	48714.412353	32.377588
686.067086	48817.119072	32.382605
686.512937	48923.687956	32.387623
687.713711	49027.620193	32.392640
688.688431	49122.096989	32.397658
689.593154	49217.236909	32.402676
690.862468	49295.965824	32.407693
691.828745	49371.739955	32.412711
692.589427	49446.431442	32.417728
693.578406	49534.028280	32.422746
694.532485	49600.954842	32.427764
695.526021	49675.247233	32.432781
696.278259	49745.032728	32.437799
697.063399	49801.710544	32.442816
699.137476	49828.520098	32.447834
700.223154	49883.333573	32.452852
701.259245	49912.052032	32.457869
701.876217	49941.916298	32.462887
702.602558	49971.566032	32.467904
703.251082	50014.679032	32.472922
703.336317	50046.169692	32.477940
704.098615	50073.412781	32.482957
704.579393	50126.984942	32.487975
704.781252	50171.015033	32.492992
705.504183	50211.866686	32.498010
705.492725	50269.453068	32.503028
706.153735	50323.828813	32.508045
706.322750	50390.109201	32.513063
706.822331	50460.768150	32.518080
707.310891	50534.651239	32.523098
707.846171	50602.006777	32.528116
708.358628	50671.135408	32.533133
708.850349	50751.146926	32.538151
708.917880	50830.245870	32.543168
709.230250	50912.455754	32.548186
709.566003	51013.627980	32.553204
710.470649	51112.277230	32.558221
711.319781	51208.403027	32.563239
712.012994	51304.758178	32.568256
713.026156	51410.851768	32.573274
713.057502	51499.373312	32.578292
714.071596	51596.123500	32.583309
714.760761	51704.567606	32.588327
715.355340	51807.910893	32.593344
716.214396	51897.707684	32.598362
716.660682	52014.509695	32.603380
717.695760	52105.654631	32.608397
718.700041	52198.144717	32.613415
719.665791	52301.850334	32.618432
720.718043	52389.790315	32.623450
721.756597	52483.331016	32.628468
722.830648	52552.622800	32.633485
723.671074	52642.628366	32.638503
724.886066	52724.722797	32.643520
725.972594	52783.486903	32.648538
726.291446	52863.473448	32.653556
726.729877	52938.069184	32.658573
727.278545	53022.711584	32.663591
728.113442	53098.263596	32.668608
728.998171	53177.990198	32.673626
729.341602	53270.010896	32.678644
729.966394	53349.005536	32.683661
730.763942	53445.707122	32.688679
730.891703	53538.998133	32.693696
731.665371	53624.792461	32.698714
731.984917	53726.613243	32.703732
732.411075	53826.489084	32.708749
733.104141	53939.020345	32.713767
734.076931	54040.219018	32.718784
734.932250	54133.508246	32.723802
735.730234	54233.600465	32.728820
736.800400	54331.068471	32.733837
738.085643	54422.497175	32.738855
738.504764	54517.095103	32.743872
739.425226	54611.133681	32.748890
740.124011	54707.826730	32.753908
740.695905	54794.823360	32.758925
741.688027	54881.969551	32.763943
742.277931	54979.560912	32.768960
742.761336	55067.768191	32.773978
743.258714	55172.681208	32.778996
744.083944	55267.263678	32.784013
744.757070	55371.332461	32.789031
745.332227	55467.696489	32.794048
746.035367	55555.103651	32.799066
746.760758	55650.128421	32.804084
747.539699	55738.483928	32.809101
749.114485	55827.461819	32.814119
750.174783	55919.397222	32.819136
750.713696	55995.118356	32.824154
751.207524	56086.753438	32.829172
752.176124	56159.166051	32.834189
753.438282	56243.712549	32.839207
753.633048	56330.129543	32.844224
754.335406	56406.342427	32.849242
754.776452	56498.045301	32.854260
755.302319	56589.544475	32.859277
756.326893	56679.258669	32.864295
757.379281	56769.530946	32.869312
759.141186	56823.344142	32.874330
760.491855	56893.595838	32.879348
761.316728	56956.278392	32.884365
762.695855	57017.223080	32.889383
763.289250	57077.550496	32.894400
763.810528	57135.842852	32.899418
764.560691	57195.063092	32.904436
765.367865	57253.616484	32.909453
766.222493	57311.055954	32.914471
766.585828	57381.882943	32.919488
767.282100	57431.772429	32.924506
768.114827	57516.151359	32.929524
768.286405	57593.837380	32.934541
769.401488	57654.399473	32.939559
769.511852	57744.344521	32.944576
769.962285	57812.743887	32.949594
770.156716	57903.958191	32.954612
771.163108	57999.135507	32.959629
771.865199	58093.366828	32.964647
772.223882	58192.530178	32.969664
772.883700	58287.818773	32.974682
773.586609	58388.687425	32.979700
774.371364	58489.384553	32.984717
775.115892	58585.791343	32.989735
775.451678	58705.375329	32.994752
776.489061	58812.155080	32.999770
777.486628	58911.054490	33.004788
778.285643	59019.228698	33.009805
779.162465	59116.664514	33.014823
779.814931	59233.492242	33.019840
780.860917	59320.218602	33.024858
781.244142	59431.430489	33.029876
781.878821	59542.397654	33.034893
783.452535	59637.681392	33.039911
783.936072	59748.125677	33.044928
784.820704	59849.665686	33.049946
785.357854	59953.123976	33.054964
786.160556	60056.979748	33.059981
787.204481	60154.278115	33.064999
787.858082	60253.868687	33.070016
789.475992	60322.891869	33.075034
790.631075	60392.019843	33.080052
791.422123	60473.200900	33.085069
792.748789	60531.592575	33.090087
793.128869	60610.537482	33.095104
794.152100	60683.955573	33.100122
794.632692	60760.146916	33.105140
795.334549	60840.769506	33.110157
796.079334	60921.770634	33.115175
796.901625	61009.193515	33.120192
797.717933	61075.587966	33.125210
798.300094	61156.668440	33.130228
798.744547	61241.723448	33.135245
799.993715	61321.065824	33.140263
800.213812	61417.689547	33.145280
800.617852	61514.781580	33.150298
800.985536	61617.354386	33.155316
801.899769	61719.625488	33.160333
802.918150	61825.362228	33.165351
803.140966	61942.114591	33.170368
804.157315	62045.084108	33.175386
804.538545	62157.328783	33.180404
805.360672	62274.928560	33.185421
806.354735	62387.044224	33.190439
806.735482	62509.582054	33.195456
807.590742	62618.498833	33.200474
808.313059	62737.806147	33.205492
809.105863	62856.760711	33.210509
810.333937	62970.356601	33.215527
811.167081	63097.561555	33.220544
812.516573	63212.004022	33.225562
813.251584	63315.084917	33.230580
813.868362	63443.346823	33.235597
814.912696	63537.576067	33.240615
816.234191	63628.660616	33.245632
817.613380	63729.559696	33.250650
818.484856	63831.418633	33.255668
819.358973	63928.801764	33.260685
820.729943	64008.639303	33.265703
821.716521	64107.116647	33.270720
822.368403	64187.463669	33.275738
822.962394	64282.715371	33.280756
823.439408	64368.561506	33.285773
824.312908	64461.623005	33.290791
824.873254	64556.805851	33.295808
825.512396	64667.312905	33.300826
826.310503	64765.926778	33.305844
827.065621	64874.929372	33.310861
827.651893	64964.805378	33.315879
828.523935	65076.810972	33.320896
828.908716	65191.644453	33.325914
830.035402	65298.208450	33.330932
830.474534	65417.162269	33.335949
830.853483	65525.828034	33.340967
831.831940	65636.067095	33.345984
832.785723	65746.930550	33.351002
833.038220	65862.549021	33.356020
833.487666	65979.297718	33.361037
834.633401	66096.471533	33.366055
835.130362	66226.174524	33.371072
835.849149	66347.500874	33.376090
836.684974	66472.064003	33.381108
837.389243	66597.895951	33.386125
838.534787	66728.812355	33.391143
839.242756	66862.219784	33.396160
839.776261	67008.113729	33.401178
840.724117	67131.567701	33.406196
841.438038	67261.834193	33.411213
843.022198	67390.118804	33.416231
843.944665	67519.554473	33.421248
845.054485	67628.156401	33.426266
846.723569	67732.679631	33.431284
847.601665	67849.649712	33.436301
848.908363	67948.153349	33.441319
849.910018	68072.235855	33.446336
850.579951	68171.342780	33.451354
851.588885	68270.442687	33.456372
852.117623	68384.446755	33.461389
853.040361	68493.401280	33.466407
853.637357	68599.301129	33.471424
854.294155	68717.129545	33.476442
855.112269	68825.161510	33.481460
855.360215	68956.416034	33.486477
856.597077	69068.329575	33.491495
857.743902	69190.857115	33.496512
858.358694	69316.714067	33.501530
859.514499	69427.340734	33.506548
860.029640	69548.340722	33.511565
861.020342	69658.939944	33.516583
862.154503	69793.557338	33.521600
863.001090	69906.933264	33.526618
863.997551	70017.185538	33.531636
864.449202	70141.020056	33.536653
865.191980	70262.105201	33.541671
866.193528	70389.483088	33.546688
867.114161	70509.546328	33.551706
868.278627	70617.989585	33.556724
869.205786	70743.921496	33.561741
870.289779	70848.003588	33.566759
871.364565	70956.893922	33.571776
872.457243	71058.920271	33.576794
873.807435	71159.853217	33.581812
874.778572	71273.486890	33.586829
875.811200	71363.022417	33.591847
877.328204	71450.559170	33.596864
878.400330	71532.632583	33.601882
879.366178	71615.616204	33.606900
879.916245	71703.800211	33.611917
879.995928	71795.271477	33.616935
880.489384	71888.044605	33.621952
881.212441	71977.294170	33.626970
882.081021	72059.594153	33.631988
882.830745	72157.036079	33.637005
883.983738	72251.797446	33.642023
884.488293	72343.836990	33.647040
885.284333	72443.397225	33.652058
886.013500	72543.500612	33.657076
886.356675	72661.062642	33.662093
887.782240	72764.500890	33.667111
888.326318	72874.174720	33.672128
889.195907	72984.881160	33.677146
890.568514	73084.111552	33.682164
891.038926	73196.032158	33.687181
891.794799	73314.500983	33.692199
892.340290	73440.849002	33.697216
893.528883	73557.271743	33.702234
893.915347	73682.358152	33.707252
894.756740	73806.279504	33.712269
895.680869	73933.431984	33.717287
896.979865	74064.689037	33.722304
897.555894	74195.716495	33.727322
898.569224	74316.727138	33.732340
899.015469	74445.387500	33.737357
899.846882	74566.563486	33.742375
901.116440	74705.931633	33.747392
901.723560	74849.392544	33.752410
902.449527	74989.001040	33.757428
902.727431	75139.180492	33.762445
904.199085	75273.331003	33.767463
904.966605	75412.726310	33.772480
905.819056	75555.087122	33.777498
907.258274	75690.074304	33.782516
907.827917	75849.475083	33.787533
908.907198	75995.803777	33.792551
909.891273	76128.404672	33.797568
910.879142	76274.301742	33.802586
911.599787	76413.047148	33.807604
912.561767	76559.393290	33.812621
913.588912	76704.122539	33.817639
914.761687	76845.083034	33.822656
915.512890	76986.875686	33.827674
916.589743	77121.142852	33.832692
917.289278	77273.680814	33.837709
918.226757	77413.268208	33.842727
918.890071	77556.199153	33.847744
919.840581	77699.031213	33.852762
921.185629	77844.200438	33.857780
922.030749	77975.077431	33.862797
923.741980	78110.551310	33.867815
924.751918	78244.678476	33.872832
925.733714	78377.274034	33.877850
927.124563	78492.485919	33.882868
927.871618	78615.033027	33.887885
928.631387	78738.084708	33.892903
929.536546	78851.800068	33.897920
930.381274	78979.405985	33.902938
930.969812	79092.569458	33.907956
931.710138	79213.855705	33.912973
932.160159	79339.367659	33.917991
933.148348	79476.567746	33.923008
933.915590	79612.035115	33.928026
934.732300	79746.223212	33.933044
935.739697	79890.818056	33.938061
936.831203	80025.593377	33.943079
937.828641	80151.718285	33.948096
938.825451	80304.592631	33.953114
939.881936	80432.935922	33.958132
940.421047	80563.285500	33.963149
941.832612	80694.144379	33.968167
943.127803	80816.571476	33.973184
943.922982	80955.420460	33.978202
944.747837	81084.338505	33.983220
945.702133	81218.226951	33.988237
946.840140	81346.200756	33.993255
948.065654	81474.963800	33.998272
948.824012	81601.915819	34.003290
950.061469	81743.699092	34.008308
950.844490	81882.144489	34.013325
952.057916	82013.323186	34.018343
953.426703	82122.185822	34.023360
954.236254	82259.989904	34.028378
954.846434	82383.289224	34.033396
956.195504	82511.739510	34.038413
956.279658	82645.019645	34.043431
957.219147	82780.925393	34.048448
957.884278	82924.066692	34.053466
958.784295	83061.100763	34.058484
959.390578	83212.871703	34.063501
960.120159	83374.917174	34.068519
961.112916	83526.604990	34.073536
962.033517	83686.354691	34.078554
963.091645	83835.711137	34.083572
963.865371	83994.051746	34.088589
964.847702	84157.476730	34.093607
965.893075	84320.525055	34.098624
966.766555	84482.737055	34.103642
967.664124	84643.370446	34.108660
968.437152	84805.095654	34.113677
969.100026	84977.889209	34.118695
970.177703	85146.556835	34.123712
971.214707	85324.553647	34.128730
972.125617	85494.543213	34.133748
972.906770	85656.570283	34.138765
973.963243	85842.420713	34.143783
975.144130	86005.223348	34.148800
976.183637	86183.618537	34.153818
977.419478	86347.875916	34.158836
978.227086	86520.807830	34.163853
979.029385	86690.539802	34.168871
980.271561	86843.104864	34.173888
981.237647	87004.875320	34.178906
982.377882	87156.997880	34.183924
983.393347	87304.921706	34.188941
984.665620	87469.193239	34.193959
985.752764	87613.322268	34.198976
986.767940	87758.141645	34.203994
987.790149	87906.941382	34.209012
989.131608	88045.555227	34.214029
990.179326	88185.340348	34.219047
991.465328	88318.731457	34.224064
992.855514	88455.004031	34.229082
993.494502	88593.526156	34.234100
994.389235	88736.403811	34.239117
995.356921	88877.966077	34.244135
996.543046	89023.440998	34.249152
997.053338	89179.260081	34.254170
998.368316	89312.189721	34.259188
999.547115	89467.794926	34.264205
1000.300606	89609.353855	34.269223
1001.224955	89754.915981	34.274240
1002.139580	89922.373089	34.279258
1002.889642	90060.789664	34.284276
1004.335366	90203.803159	34.289293
1004.920198	90359.882893	34.294311
1006.181611	90512.752753	34.299328
1006.989491	90665.061973	34.304346
1007.840293	90822.225744	34.309364
1008.999219	90984.103806	34.314381
1009.733960	91137.428544	34.319399
1010.672489	91300.574354	34.324416
1011.415150	91470.685626	34.329434
1012.067436	91648.016608	34.334452
1013.002533	91814.014733	34.339469
1013.727759	92003.368399	34.344487
1015.026648	92165.072055	34.349504
1016.233234	92347.092096	34.354522
1017.404288	92512.516504	34.359540
1018.643995	92692.083791	34.364557
1019.972281	92870.314271	34.369575
1021.681057	93035.289304	34.374592
1022.265468	93196.697965	34.379610
1022.935275	93353.548106	34.384628
1024.025962	93520.898359	34.389645
1025.097198	93684.455014	34.394663
1026.317794	93855.216190	34.399680
1027.139497	94030.034859	34.404698
1028.257858	94198.302814	34.409716
1029.569927	94359.315899	34.414733
1030.412865	94534.501626	34.419751
1031.839093	94681.887078	34.424768
1032.762737	94844.007979	34.429786
1034.101895	94995.664215	34.434804
1035.008883	95160.898262	34.439821
1035.489099	95314.235479	34.444839
1036.711462	95475.574978	34.449856
1037.752463	95625.918682	34.454874
1038.847688	95777.754360	34.459892
1039.491046	95928.978285	34.464909
1039.914580	96100.055863	34.469927
1041.047372	96252.109542	34.474944
1042.325430	96417.516212	34.479962
1043.147785	96579.747951	34.484980
1044.287992	96744.559945	34.489997
1045.098773	96914.057316	34.495015
1046.658640	97086.219504	34.500032
1047.508593	97264.955706	34.505050
1048.046245	97434.313389	34.510068
1048.985386	97609.364737	34.515085
1049.902332	97795.785466	34.520103
1050.540315	97978.260351	34.525120
1051.719061	98170.140780	34.530138
1052.718140	98357.190998	34.535156
1054.095979	98541.873131	34.540173
1055.659364	98741.485835	34.545191
1056.492009	98923.737859	34.550208
1057.328795	99120.020973	34.555226
1058.421236	99306.441646	34.560244
1059.648704	99491.764186	34.565261
1060.764274	99674.802520	34.570279
1062.185640	99847.108320	34.575296
1063.468843	100034.134757	34.580314
1064.115080	100225.463215	34.585332
1065.514795	100400.594032	34.590349
1066.181198	100587.432484	34.595367
1067.916238	100767.219234	34.600384
1068.913385	100949.045811	34.605402
1069.767514	101134.197092	34.610420
1071.096135	101311.720708	34.615437
1072.000877	101497.993002	34.620455
1072.986823	101684.771951	34.625472
1074.524394	101873.863993	34.630490
1075.435049	102058.847517	34.635508
1076.311161	102240.862118	34.640525
1077.556192	102431.717976	34.645543
1078.681935	102614.540949	34.650560
1079.883866	102795.110497	34.655578
1080.651143	102977.921384	34.660596
1081.747032	103162.235053	34.665613
1082.295151	103365.831229	34.670631
1083.131798	103559.019542	34.675648
1084.198022	103760.288326	34.680666
1085.132245	103961.517913	34.685684
1086.601694	104153.728310	34.690701
1087.717902	104352.953909	34.695719
1089.957429	104520.198178	34.700736
1091.623675	104683.931960	34.705754
1093.239508	104846.801449	34.710772
1094.935421	105000.817525	34.715789
1096.031087	105159.775611	34.720807
1097.237065	105299.362259	34.725824
1098.351202	105445.918975	34.730842
1099.289376	105587.060227	34.735860
1099.942411	105728.821016	34.740877
1100.754705	105873.823157	34.745895
1101.801113	106033.618161	34.750912
1102.793473	106179.781748	34.755930
1103.451544	106337.175113	34.760948
1104.349317	106497.884968	34.765965
1104.862976	106673.177398	34.770983
1105.719701	106848.285560	34.776000
1106.703031	107030.124533	34.781018
1107.324383	107217.410090	34.786036
1108.561707	107403.286787	34.791053
1109.446665	107605.413478	34.796071
1110.295254	107795.425515	34.801088
1111.507158	107991.748250	34.806106
1112.552421	108203.415637	34.811124
1114.156539	108385.334726	34.816141
1115.337654	108580.425569	34.821159
1116.415775	108778.296956	34.826176
1117.946282	108963.158688	34.831194
1119.251701	109153.760667	34.836212
1120.230230	109340.480256	34.841229
1121.304678	109540.713973	34.846247
1122.641141	109726.589490	34.851264
1123.701696	109914.122340	34.856282
1124.345124	110124.011128	34.861300
1125.568084	110323.984403	34.866317
1126.412640	110528.977224	34.871335
1127.612627	110742.069166	34.876352
1128.914022	110947.784973	34.881370
1129.647120	111145.225651	34.886388
1131.052593	111340.943686	34.891405
1131.895550	111561.197494	34.896423
1133.887926	111751.585714	34.901440
1135.654449	111943.065426	34.906458
1136.648286	112146.650995	34.911476
1137.790431	112334.984337	34.916493
1138.838722	112534.509270	34.921511
1139.870131	112735.052055	34.926528
1140.884948	112932.875184	34.931546
1141.727664	113127.764502	34.936564
1143.400859	113330.241428	34.941581
1144.502590	113535.085516	34.946599
1145.435424	113723.248578	34.951616
1146.882748	113914.859690	34.956634
1147.663933	114129.632765	34.961652
1148.918890	114324.814491	34.966669
1150.411200	114536.073315	34.971687
1151.479355	114730.212838	34.976704
1152.192500	114921.867730	34.981722
1153.427429	115130.159481	34.986740
1154.341014	115337.278726	34.991757
1155.482691	115540.647937	34.996775
1156.491590	115730.027574	35.001792
1157.787318	115916.077630	35.006810
1158.986761	116110.875566	35.011828
1160.584615	116294.380187	35.016845
1161.567915	116490.421425	35.021863
1162.418145	116675.057467	35.026880
1163.695589	116868.998196	35.031898
1164.639226	117063.706961	35.036916
1166.187630	117252.598726	35.041933
1166.980182	117452.366473	35.046951
1168.196430	117647.437957	35.051968
1169.131326	117852.518773	35.056986
1169.567834	118064.034859	35.062004
1170.693342	118279.793601	35.067021
1171.564733	118496.889965	35.072039
1172.546700	118726.260799	35.077056
1173.890069	118951.883980	35.082074
1175.205754	119174.700412	35.087092
1176.368318	119398.178353	35.092109
1177.566404	119640.457662	35.097127
1178.549354	119886.564849	35.102144
1179.756875	120084.948827	35.107162
1180.899206	120341.854851	35.112180
1181.845151	120576.163177	35.117197
1183.380733	120814.541764	35.122215
1184.311152	121051.238972	35.127232
1185.660300	121297.295116	35.132250
1186.715671	121536.826206	35.137268
1188.286174	121766.360532	35.142285
1189.690169	122006.570731	35.147303
1190.854791	122243.642788	35.152320
1192.727923	122468.023252	35.157338
1193.651344	122711.033468	35.162356
1195.007699	122942.539797	35.167373
1195.822254	123179.742484	35.172391
1196.782159	123412.524280	35.177408
1197.999881	123650.054502	35.182426
1199.591627	123902.199197	35.187444
1200.727540	124129.785281	35.192461
1201.825932	124371.067761	35.197479
1202.978245	124625.270834	35.202496
1204.313297	124857.885329	35.207514
1204.965559	125109.212163	35.212532
1206.141145	125354.101407	35.217549
1207.957245	125591.316059	35.222567
1209.125678	125832.838811	35.227584
1210.331464	126074.509147	35.232602
1211.472049	126326.269257	35.237620
1212.902649	126559.742089	35.242637
1214.485505	126809.427701	35.247655
1215.684847	127037.391898	35.252672
1218.179244	127238.872392	35.257690
1220.053405	127453.997894	35.262708
1221.313407	127669.065225	35.267725
1222.621370	127862.260126	35.272743
1223.322747	128055.724839	35.277760
1224.649903	128257.487741	35.282778
1225.458631	128466.527972	35.287796
1226.253600	128667.509950	35.292813
1227.066105	128880.076211	35.297831
1227.869578	129095.510272	35.302848
1228.985445	129308.559866	35.307866
1229.989347	129543.851824	35.312884
1231.055846	129773.620511	35.317901
1232.164481	130005.754161	35.322919
1233.011087	130238.593536	35.327936
1234.136057	130462.982231	35.332954
1235.671383	130707.116213	35.337972
1237.645567	130928.586541	35.342989
1239.509070	131147.732081	35.348007
1240.917766	131365.245550	35.353024
1242.786165	131582.263435	35.358042
1244.254583	131795.231117	35.363060
1245.849456	131995.843443	35.368077
1246.802554	132210.499410	35.373095
1247.924634	132415.239368	35.378112
1248.801016	132630.392974	35.383130
1249.866927	132856.253580	35.388148
1251.073873	133072.735374	35.393165
1252.044423	133297.423624	35.398183
1253.012705	133520.427625	35.403200
1254.452478	133757.894166	35.408218
1255.525408	133976.826352	35.413236
1256.895739	134208.932483	35.418253
1258.418472	134445.984056	35.423271
1259.318950	134681.495645	35.428288
1260.840370	134913.732976	35.433306
1261.620319	135153.655298	35.438324
1262.846386	135389.712044	35.443341
1264.019318	135632.638771	35.448359
1264.849566	135888.685162	35.453376
1265.896262	136133.057150	35.458394
1266.876266	136389.398686	35.463412
1268.158941	136653.576796	35.468429
1269.521202	136904.911929	35.473447
1270.647889	137174.725038	35.478464
1272.616224	137423.956927	35.483482
1273.805003	137687.322308	35.488500
1275.462512	137934.696525	35.493517
1276.909778	138177.226823	35.498535
1277.787368	138435.794895	35.503552
1279.219543	138688.868331	35.508570
1280.128290	138952.468881	35.513588
1281.413436	139211.543612	35.518605
1282.942869	139475.751992	35.523623
1284.425811	139723.600070	35.528640
1285.300024	139982.801626	35.533658
1286.397695	140247.178542	35.538676
1287.517015	140517.298061	35.543693
1289.220778	140769.858319	35.548711
1290.622422	141027.759995	35.553728
1292.158093	141263.068685	35.558746
1293.683066	141485.306728	35.563764
1295.484829	141707.866543	35.568781
1297.042919	141928.110786	35.573799
1298.716238	142161.664596	35.578816
1300.042511	142378.933202	35.583834
1301.214491	142616.697230	35.588852
1302.008460	142837.128634	35.593869
1303.271468	143073.307627	35.598887
1303.911671	143319.296204	35.603904
1304.793612	143563.634514	35.608922
1305.910472	143810.001401	35.613940
1306.656975	144073.794828	35.618957
1307.921919	144345.440341	35.623975
1308.546886	144620.799140	35.628992
1309.951690	144892.348719	35.634010
1311.131454	145178.371237	35.639028
1312.122240	145470.591966	35.644045
1312.968712	145755.851703	35.649063
1314.306120	146058.671046	35.654080
1315.611768	146352.214620	35.659098
1316.774280	146666.762307	35.664116
1317.997576	146973.413524	35.669133
1319.251526	147269.991755	35.674151
1320.339223	147591.954266	35.679168
1322.401943	147894.677160	35.684186
1323.953536	148210.870859	35.689204
1325.407280	148521.401815	35.694221
1326.709622	148813.658975	35.699239
1328.042180	149121.539408	35.704256
1329.493457	149422.882609	35.709274
1331.063956	149733.492335	35.714292
1332.490658	150037.736527	35.719309
1334.744096	150325.606126	35.724327
1336.274095	150615.922911	35.729344
1338.005301	150894.436534	35.734362
1339.534055	151188.372852	35.739380
1340.505059	151483.878266	35.744397
1342.099565	151759.136283	35.749415
1343.340067	152053.166568	35.754432
1344.633225	152340.467198	35.759450
1346.315168	152615.754371	35.764468
1347.517004	152902.909869	35.769485
1349.448222	153172.627706	35.774503
1350.730969	153443.752261	35.779520
1352.569755	153710.635483	35.784538
1354.176993	153988.748472	35.789556
1355.262752	154245.324286	35.794573
1357.371305	154500.508903	35.799591
1358.436464	154762.850732	35.804608
1359.859323	155021.771400	35.809626
1361.082090	155274.588163	35.814644
1362.535964	155524.994744	35.819661
1363.913304	155790.220257	35.824679
1365.302874	156037.659880	35.829696
1366.658362	156268.386825	35.834714
1367.570230	156514.490306	35.839732
1369.064042	156770.771381	35.844749
1370.560490	157007.174440	35.849767
1370.921468	157266.684513	35.854784
1372.094404	157522.289427	35.859802
1373.526237	157783.382880	35.864820
1374.497583	158052.841063	35.869837
1375.898803	158313.080435	35.874855
1376.687593	158581.355402	35.879872
1378.428544	158855.672933	35.884890
1379.678806	159135.239782	35.889908
1380.667117	159424.431929	35.894925
1382.070483	159708.898920	35.899943
1383.247290	160005.662307	35.904960
1384.024246	160304.411980	35.909978
1385.726206	160616.200170	35.914996
1386.873055	160924.127219	35.920013
1387.763435	161228.611354	35.925031
1388.574071	161556.253332	35.930048
1389.823276	161883.822755	35.935066
1391.218731	162220.796613	35.940084
1391.910177	162563.679242	35.945101
1393.307896	162902.573894	35.950119
1394.930710	163251.215123	35.955136
1396.506350	163605.944823	35.960154
1397.883617	163949.393463	35.965172
1399.249743	164306.702338	35.970189
1401.042979	164648.346943	35.975207
1402.787918	164991.258617	35.980224
1404.693319	165325.783683	35.985242
1406.567378	165660.824173	35.990260
1407.862071	165982.884182	35.995277
1409.753561	166305.351916	36.000295
1411.412862	166641.756132	36.005312
1412.902270	166962.635124	36.010330
1415.099872	167270.832912	36.015348
1416.987712	167572.322437	36.020365
1419.242036	167866.074190	36.025383
1420.977662	168153.851067	36.030400
1422.740205	168437.234579	36.035418
1424.543863	168720.194040	36.040436
1425.899114	169001.569634	36.045453
1427.230710	169277.672061	36.050471
1428.255655	169554.780342	36.055488
1429.794244	169832.728717	36.060506
1431.172095	170102.901940	36.065524
1432.432317	170389.822279	36.070541
1434.096299	170669.264252	36.075559
1434.995447	170954.155948	36.080576
1436.541136	171246.958933	36.085594
1437.639102	171534.345435	36.090612
1438.466865	171821.830667	36.095629
1439.841811	172113.031116	36.100647
1441.003840	172395.297550	36.105664
1442.192382	172678.284461	36.110682
1444.463341	172948.612830	36.115700
1445.947038	173224.813659	36.120717
1447.184723	173489.852153	36.125735
1448.953822	173766.134108	36.130752
1450.019376	174038.489603	36.135770
1451.816111	174310.404194	36.140788
1453.076479	174601.410670	36.145805
1454.259945	174870.742777	36.150823
1456.015923	175168.000655	36.155840
1457.319898	175448.559716	36.160858
1459.079969	175722.645826	36.165876
1459.884389	176020.274670	36.170893
1461.462452	176316.249881	36.175911
1462.859186	176618.514825	36.180928
1463.361717	176909.245542	36.185946
1464.939730	177220.849506	36.190964
1466.043806	177544.834878	36.195981
1467.030774	177862.534440	36.200999
1468.534345	178196.583700	36.206016
1470.304256	178509.685654	36.211034
1472.422364	178834.025931	36.216052
1474.129471	179158.451249	36.221069
1476.095210	179447.029273	36.226087
1477.719596	179753.969718	36.231104
1478.914819	180079.389464	36.236122
1480.875809	180380.678554	36.241140
1483.034577	180669.471356	36.246157
1485.315752	180969.680873	36.251175
1486.261456	181256.488598	36.256192
1487.919761	181550.372722	36.261210
1489.372675	181839.305285	36.266228
1490.404807	182147.147734	36.271245
1492.202013	182434.222131	36.276263
1493.221286	182733.248426	36.281280
1494.763252	183042.265264	36.286298
1496.130209	183352.354623	36.291316
1496.928645	183665.157824	36.296333
1498.439944	183975.720992	36.301351
1499.680719	184314.092745	36.306368
1501.083784	184633.753892	36.311386
1502.314090	184963.157009	36.316404
1503.199515	185301.938209	36.321421
1504.667630	185634.744500	36.326439
1505.862563	185981.880020	36.331456
1507.326310	186352.988487	36.336474
1508.912853	186690.794701	36.341492
1510.624324	187046.124678	36.346509
1512.574085	187373.755531	36.351527
1513.782233	187793.522720	36.356544
1515.458346	188147.976809	36.361562
1517.195423	188493.853883	36.366580
1518.315697	188838.543677	36.371597
1520.080868	189172.867928	36.376615
1521.450611	189508.378822	36.381632
1522.823520	189846.328402	36.386650
1524.520389	190160.828055	36.391668
1526.032211	190507.770770	36.396685
1527.078529	190827.120316	36.401703
1528.484726	191179.581752	36.406720
1530.227492	191521.717340	36.411738
1531.737259	191865.659286	36.416756
1533.386707	192208.385869	36.421773
1535.034261	192543.167440	36.426791
1536.518613	192885.621254	36.431808
1537.606987	193246.959152	36.436826
1539.581318	193586.171727	36.441844
1541.003740	193947.824560	36.446861
1542.602223	194293.833760	36.451879
1544.448572	194652.929640	36.456896
1545.136114	195014.066652	36.461914
1546.542277	195368.874444	36.466932
1547.890311	195738.560881	36.471949
1549.075262	196107.528210	36.476967
1551.440033	196487.480815	36.481984
1552.523499	196869.787742	36.487002
1554.122665	197241.331145	36.492020
1556.229989	197607.914277	36.497037
1558.066364	197980.576436	36.502055
1560.251561	198342.960382	36.507072
1561.921192	198702.463480	36.512090
1563.450003	199068.226463	36.517108
1564.770709	199435.296596	36.522125
1566.050404	199809.726952	36.527143
1567.710461	200174.203502	36.532160
1569.131259	200554.885729	36.537178
1570.765788	200922.531894	36.542196
1572.397829	201287.806028	36.547213
1573.827702	201679.208678	36.552231
1575.444049	202058.113074	36.557248
1577.181524	202439.499982	36.562266
1578.687709	202819.112719	36.567284
1580.111329	203195.694173	36.572301
1581.639947	203592.702033	36.577319
1583.088658	203969.905168	36.582336
1584.050497	204373.248394	36.587354
1585.631711	204771.611921	36.592372
1587.102454	205164.980870	36.597389
1588.458138	205579.258907	36.602407
1590.002143	205989.354756	36.607424
1591.424053	206402.825772	36.612442
1592.913668	206817.061873	36.617460
1594.792770	207236.579200	36.622477
1596.325395	207652.450173	36.627495
1598.186175	208064.991012	36.632512
1599.760653	208485.988935	36.637530
1601.280785	208897.322341	36.642548
1603.270068	209296.311084	36.647565
1605.042150	209705.929113	36.652583
1607.064032	210094.808229	36.657600
1608.815505	210478.935393	36.662618
1610.553873	210851.612577	36.667636
1612.057639	211236.293343	36.672653
1613.924458	211607.529485	36.677671
1616.136626	211968.727048	36.682688
1617.478405	212343.611613	36.687706
1619.509586	212705.554171	36.692724
1621.253659	213072.525136	36.697741
1622.535360	213429.925650	36.702759
1624.679233	213799.802547	36.707776
1625.914476	214178.268346	36.712794
1627.774031	214531.739099	36.717812
1629.169799	214911.196220	36.722829
1630.490978	215277.308301	36.727847
1632.306773	215657.839350	36.732864
1633.759116	216034.141772	36.737882
1635.356091	216419.005436	36.742900
1636.835722	216803.306481	36.747917
1638.413054	217192.773517	36.752935
1639.472569	217567.040759	36.757952
1640.891567	217974.215134	36.762970
1642.968377	218374.065321	36.767988
1644.886110	218775.595147	36.773005
1646.132218	219173.990337	36.778023
1647.757323	219575.471607	36.783040
1649.164487	219983.722371	36.788058
1651.146745	220378.389317	36.793076
1653.207595	220782.797493	36.798093
1654.930280	221175.098715	36.803111
1657.046287	221570.534303	36.808128
1659.088719	221973.400466	36.813146
1661.194412	222353.930998	36.818164
1663.246490	222726.979037	36.823181
1664.921510	223107.839655	36.828199
1666.925746	223481.634805	36.833216
1668.059070	223851.338327	36.838234
1670.187327	224231.769291	36.843252
1672.123281	224597.324510	36.848269
1673.741157	224971.799828	36.853287
1675.252527	225338.166413	36.858304
1676.991870	225703.250416	36.863322
1678.978325	226071.391990	36.868340
1680.627470	226442.792737	36.873357
1681.423075	226825.745331	36.878375
1682.880059	227206.528404	36.883392
1684.239056	227595.940082	36.888410
1685.981864	227985.236376	36.893428
1687.276291	228382.865680	36.898445
1688.276081	228785.067830	36.903463
1690.043757	229188.739964	36.908480
1691.695547	229611.458314	36.913498
1693.374801	230024.876389	36.918516
1694.565430	230427.990148	36.923533
1696.547438	230840.774393	36.928551
1697.989959	231236.048994	36.933568
1699.798574	231648.661795	36.938586
1701.141089	232037.478150	36.943604
1702.630669	232458.301391	36.948621
1703.971833	232866.399555	36.953639
1705.516266	233288.587149	36.958656
1706.865456	233715.000427	36.963674
1708.352559	234134.507296	36.968692
1709.653881	234580.058244	36.973709
1711.360692	235029.224149	36.978727
1713.275673	235472.894125	36.983744
1714.999815	235920.408055	36.988762
1716.657820	236366.537216	36.993780
1718.133356	236818.668051	36.998797
1719.803673	237286.642828	37.003815
1721.890594	237742.252767	37.008832
1723.202069	238212.018316	37.013850
1724.634545	238678.080847	37.018868
1726.719839	239143.854839	37.023885
1728.540987	239619.099209	37.028903
1730.635168	240079.488248	37.033920
1732.327362	240560.726081	37.038938
1733.632399	241040.811749	37.043956
1735.404275	241521.504303	37.048973
1736.791087	242013.847150	37.053991
1738.866447	242496.242278	37.059008
1740.945996	242977.341969	37.064026
1742.441673	243474.368184	37.069044
1744.590968	243952.002733	37.074061
1746.136835	244447.726367	37.079079
1748.213605	244925.450961	37.084096
1750.256828	245419.414350	37.089114
1751.746383	245897.215314	37.094132
1754.449324	246383.649507	37.099149
1756.173218	246872.538050	37.104167
1758.389772	247337.235508	37.109184
1759.781855	247822.447680	37.114202
1761.582210	248296.438612	37.119220
1763.581519	248773.342723	37.124237
1764.935250	249252.313751	37.129255
1767.409423	249731.347556	37.134272
1769.047951	250209.813423	37.139290
1770.799783	250675.711145	37.144308
1772.608782	251158.060626	37.149325
1774.489631	251622.184093	37.154343
1776.719353	252084.647751	37.159360
1778.572160	252561.706735	37.164378
1780.057317	253029.048627	37.169396
1782.006176	253495.904943	37.174413
1783.666071	253962.455220	37.179431
1785.824164	254410.757139	37.184448
1788.020434	254867.080053	37.189466
1790.125505	255334.037202	37.194484
1791.954497	255791.566259	37.199501
1793.551749	256240.472515	37.204519
1795.238997	256673.460992	37.209536
1796.548141	257112.991971	37.214554
1798.428785	257551.993315	37.219572
1800.111082	257989.910810	37.224589
1801.655328	258440.045396	37.229607
1803.128121	258888.388496	37.234624
1804.497250	259337.866962	37.239642
1805.740765	259791.609119	37.244660
1807.600570	260255.025919	37.249677
1809.234224	260739.438825	37.254695
1810.818748	261214.079695	37.259712
1812.303888	261697.018740	37.264730
1813.575269	262188.859755	37.269748
1815.399920	262694.475895	37.274765
1816.369322	263205.242368	37.279783
1818.180657	263717.769637	37.284800
1820.099978	264234.723517	37.289818
1821.456627	264764.855705	37.294836
1823.529049	265297.887857	37.299853
1825.194947	265826.721257	37.304871
1827.650674	266360.423306	37.309888
1830.159095	266869.601884	37.314906
1832.783767	267374.847896	37.319924
1835.410277	267864.292374	37.324941
1837.663892	268360.760350	37.329959
1840.099323	268860.422674	37.334976
1842.415373	269350.781884	37.339994
1844.047360	269835.694177	37.345012
1846.252328	270318.424690	37.350029
1848.200669	270801.935002	37.355047
1850.290559	271263.294676	37.360064
1852.184561	271748.514652	37.365082
1853.852128	272211.850172	37.370100
1855.817899	272679.858720	37.375117
1857.464805	273174.161602	37.380135
1859.212314	273657.777321	37.385152
1860.718614	274143.084477	37.390170
1861.692429	274635.035483	37.395188
1862.887691	275135.736695	37.400205
1864.307181	275659.082497	37.405223
1866.095421	276170.323392	37.410240
1867.696251	276692.543350	37.415258
1869.492799	277228.191508	37.420276
1871.201493	277769.568666	37.425293
1872.907482	278313.865981	37.430311
1874.388169	278851.316412	37.435328
1876.138169	279405.433475	37.440346
1877.940607	279964.975792	37.445364
1879.706403	280520.280556	37.450381
1881.525455	281090.764431	37.455399
1883.817426	281652.351234	37.460416
1885.963452	282212.259197	37.465434
1887.443590	282784.547832	37.470452
1889.560958	283332.289617	37.475469
1891.747136	283889.035005	37.480487
1893.998056	284424.024155	37.485504
1896.372584	284954.900706	37.490522
1898.372572	285478.422385	37.495540
1900.080959	286001.356999	37.500557
1901.504429	286536.352798	37.505575
1903.315241	287068.537020	37.510592
1905.135367	287615.983095	37.515610
1907.312367	288146.119170	37.520628
1909.564253	288657.317247	37.525645
1911.519451	289199.374148	37.530663
1913.363743	289732.760945	37.535680
1915.373736	290268.657073	37.540698
1916.805911	290813.107739	37.545716
1918.530953	291369.037206	37.550733
1920.261382	291917.648116	37.555751
1922.268360	292476.699019	37.560768
1924.055894	293033.346406	37.565786
1925.422119	293607.309008	37.570804
1927.220747	294171.543118	37.575821
1929.031418	294754.668897	37.580839
1930.426974	295342.231065	37.585856
1932.463357	295935.369616	37.590874
1934.433573	296515.969353	37.595892
1936.708717	297107.384061	37.600909
1938.617763	297695.886360	37.605927
1940.967771	298279.788952	37.610944
1943.689129	298868.805692	37.615962
1945.456204	299448.000832	37.620980
1947.875470	300026.572972	37.625997
1950.612379	300605.645976	37.631015
1952.278167	301186.143027	37.636032
1954.813638	301754.144773	37.641050
1956.160915	302329.355680	37.646068
1958.314454	302902.164703	37.651085
1960.351689	303482.685023	37.656103
1962.152486	304062.784790	37.661120
1964.681312	304649.130559	37.666138
1966.206037	305228.177627	37.671156
1967.943522	305795.019775	37.676173
1969.691934	306375.417418	37.681191
1971.771458	306961.900017	37.686208
1973.666294	307558.060140	37.691226
1975.630985	308152.477033	37.696244
1977.618762	308740.257486	37.701261
1979.591200	309329.331287	37.706279
1981.377557	309921.200434	37.711296
1983.806153	310504.219569	37.716314
1985.601615	311110.679612	37.721332
1988.025932	311683.151858	37.726349
1989.938627	312278.561450	37.731367
1991.299357	312870.759474	37.736384
1993.730222	313470.336837	37.741402
1995.675940	314070.500032	37.746420
1997.522939	314658.232592	37.751437
1999.170303	315255.110322	37.756455
2001.182245	315831.555933	37.761472
2003.361742	316408.983764	37.766490
2005.062384	316993.420609	37.771508
2007.319014	317570.038250	37.776525
2009.449334	318150.151170	37.781543
2011.455037	318724.313391	37.786560
2013.942583	319287.800137	37.791578
2016.306512	319847.875396	37.796596
2018.682610	320411.244500	37.801613
2020.735401	320973.140520	37.806631
2022.661347	321532.768148	37.811648
2025.400454	322087.351485	37.816666
2027.073064	322655.162588	37.821684
2029.948232	323198.719002	37.826701
2031.982704	323756.353067	37.831719
2033.866576	324309.843982	37.836736
2035.743192	324867.494825	37.841754
2036.799226	325428.885977	37.846772
2038.833669	325990.282225	37.851789
2040.795947	326568.695459	37.856807
2042.653512	327150.751329	37.861824
2044.690855	327728.835541	37.866842
2046.333392	328322.366145	37.871860
2048.045976	328914.304596	37.876877
2050.034987	329521.903970	37.881895
2052.091043	330128.672927	37.886912
2053.784002	330743.747862	37.891930
2055.753401	331358.464031	37.896948
2057.599929	331967.837937	37.901965
2059.512437	332603.315206	37.906983
2061.090091	333234.450620	37.912000
2063.008461	333875.039568	37.917018
2064.379400	334543.104131	37.922036
2066.462877	335204.616168	37.927053
2068.457505	335867.962611	37.932071
2070.250823	336544.483547	37.937088
2072.112946	337216.465578	37.942106
2073.876735	337908.685549	37.947124
2076.159354	338593.928641	37.952141
2078.062089	339286.384999	37.957159
2080.363316	339983.027630	37.962176
2082.997312	340671.811391	37.967194
2084.788211	341373.673834	37.972212
2086.584045	342076.997283	37.977229
2089.107994	342768.460227	37.982247
2091.070008	343473.663514	37.987264
2093.210868	344177.531291	37.992282
2094.979505	344895.385189	37.997300
2097.096078	345600.225338	38.002317
2099.318635	346324.653931	38.007335
2101.397789	347046.811507	38.012352
2103.536339	347766.739537	38.017370
2105.656140	348485.999397	38.022388
2107.681079	349211.481108	38.027405
2109.917519	349928.261429	38.032423
2111.718547	350641.907109	38.037440
2113.870505	351336.119639	38.042458
2115.772367	352038.204615	38.047476
2117.833026	352744.285465	38.052493
2119.817079	353446.231689	38.057511
2121.614039	354164.158268	38.062528
2124.226742	354870.743435	38.067546
2126.323422	355597.068749	38.072564
2128.093625	356325.086294	38.077581
2130.308459	357037.588735	38.082599
2132.141571	357770.085925	38.087616
2134.490910	358505.348466	38.092634
2136.591280	359245.764922	38.097652
2138.496907	359976.661742	38.102669
2140.980126	360711.429291	38.107687
2142.973881	361462.680562	38.112704
2145.565289	362191.160961	38.117722
2147.751880	362933.471738	38.122740
2150.287911	363668.453253	38.127757
2152.945443	364407.686859	38.132775
2154.739172	365164.582068	38.137792
2156.802521	365890.849728	38.142810
2159.446589	366640.644741	38.147828
2161.792207	367369.498646	38.152845
2164.588902	368114.519720	38.157863
2166.189446	368861.784621	38.162880
2168.617180	369594.790561	38.167898
2170.686159	370339.256330	38.172916
2173.078440	371065.390324	38.177933
2175.471781	371800.183144	38.182951
2177.608483	372545.504241	38.187968
2180.040411	373276.683727	38.192986
2182.066497	374011.290233	38.198004
2184.418358	374747.651404	38.203021
2186.961587	375486.550787	38.208039
2189.172667	376216.133631	38.213056
2192.124601	376939.412123	38.218074
2194.640106	377650.907722	38.223092
2196.633010	378372.011932	38.228109
2199.176627	379076.828904	38.233127
2201.317498	379795.696365	38.238144
2203.636147	380497.554939	38.243162
2205.700529	381227.814249	38.248180
2208.036598	381931.895723	38.253197
2210.351591	382650.645445	38.258215
2212.147511	383376.972504	38.263232
2214.605949	384076.067783	38.268250
2217.104866	384783.861995	38.273268
2219.279271	385494.636704	38.278285
2221.892282	386208.489312	38.283303
2223.892344	386918.577218	38.288320
2226.432745	387625.159715	38.293338
2228.548564	388338.769794	38.298356
2230.006689	389045.251448	38.303373
2232.483180	389733.849740	38.308391
2234.119291	390436.517372	38.313408
2236.366491	391119.547099	38.318426
2238.550762	391814.079445	38.323444
2240.362536	392514.083457	38.328461
2242.777798	393208.924223	38.333479
2244.447625	393907.525852	38.338496
2246.915654	394603.034638	38.343514
2249.082853	395312.846809	38.348532
2251.184933	396023.539932	38.353549
2253.969937	396718.614892	38.358567
2256.580835	397442.034886	38.363584
2258.507255	398142.214744	38.368602
2260.928032	398861.754415	38.373620
2262.875145	399575.554159	38.378637
2265.809218	400287.798949	38.383655
2268.207433	400998.951851	38.388672
2270.332236	401710.995017	38.393690
2272.577235	402435.870808	38.398708
2274.396576	403159.812397	38.403725
2276.604282	403870.823440	38.408743
2278.317033	404622.209013	38.413760
2280.464523	405368.179476	38.418778
2282.772920	406109.541987	38.423796
2284.969939	406862.885857	38.428813
2287.091868	407612.269734	38.433831
2289.551564	408379.433802	38.438848
2292.259952	409134.906485	38.443866
2294.215813	409893.855300	38.448884
2296.492892	410662.783265	38.453901
2298.692761	411424.154051	38.458919
2301.257925	412198.256250	38.463936
2303.624040	412965.176591	38.468954
2305.652050	413744.871300	38.473972
2307.686051	414529.150741	38.478989
2310.104512	415315.949008	38.484007
2312.159647	416117.093319	38.489024
2314.506173	416904.437363	38.494042
2317.056354	417699.926619	38.499060
2318.968817	418501.070562	38.504077
2321.236375	419296.431001	38.509095
2323.671829	420106.321767	38.514112
2325.867348	420902.377480	38.519130
2328.571181	421714.651053	38.524148
2330.699511	422540.515762	38.529165
2332.619416	423349.831056	38.534183
2334.721592	424187.391459	38.539200
2337.220625	425014.627782	38.544218
2339.693047	425850.649568	38.549236
2341.578109	426682.338091	38.554253
2344.149212	427507.552248	38.559271
2346.835687	428346.538061	38.564288
2349.103801	429177.466189	38.569306
2351.742660	430020.348974	38.574324
2354.001365	430852.535434	38.579341
2356.710232	431685.779344	38.584359
2358.998666	432500.287363	38.589376
2361.258847	433291.692263	38.594394
2364.036847	434090.927190	38.599412
2365.924240	434887.553509	38.604429
2368.798840	435679.985218	38.609447
2370.841728	436482.500554	38.614464
2372.731276	437300.498123	38.619482
2374.913638	438105.613638	38.624500
2376.834000	438921.927416	38.629517
2379.038349	439741.502116	38.634535
2381.388036	440576.807507	38.639552
2383.750260	441417.340828	38.644570
2386.165405	442256.062145	38.649588
2388.656477	443101.567882	38.654605
2390.964655	443935.183770	38.659623
2393.259964	444792.089876	38.664640
2395.777123	445654.538755	38.669658
2397.878555	446522.891462	38.674676
2400.047028	447401.920264	38.679693
2402.390992	448270.160162	38.684711
2403.916552	449152.513711	38.689728
2405.958799	450050.116256	38.694746
2408.603292	450953.190761	38.699764
2410.918650	451860.479581	38.704781
2413.560167	452768.380858	38.709799
2416.150002	453682.672700	38.714816
2418.636091	454592.239239	38.719834
2421.399885	455515.217358	38.724852
2424.017032	456432.313929	38.729869
2426.930227	457336.022222	38.734887
2429.469982	458245.516862	38.739904
2432.067515	459153.494384	38.744922
2434.598920	460068.821998	38.749940
2436.722591	460982.003630	38.754957
2439.333190	461894.251161	38.759975
2441.750871	462811.493003	38.764992
2444.198281	463746.527170	38.770010
2446.630879	464669.693430	38.775028
2448.630694	465594.557398	38.780045
2451.211119	466527.918838	38.785063
2453.433495	467473.322204	38.790080
2455.611737	468419.646454	38.795098
2457.947360	469366.654693	38.800116
2459.725248	470335.940627	38.805133
2462.546841	471285.750591	38.810151
2464.917672	472257.311797	38.815168
2467.341357	473227.045538	38.820186
2470.378434	474199.048505	38.825204
2472.623824	475175.328049	38.830221
2475.183615	476145.896042	38.835239
2477.913875	477115.373558	38.840256
2480.499839	478082.299305	38.845274
2483.396397	479041.697398	38.850292
2486.058641	480003.205559	38.855309
2488.748127	480949.156562	38.860327
2491.731725	481885.161920	38.865344
2494.342118	482800.734645	38.870362
2497.226336	483704.501006	38.875380
2499.318115	484611.688598	38.880397
2501.809095	485514.218211	38.885415
2503.974138	486432.203261	38.890432
2506.365295	487344.801764	38.895450
2508.998162	488246.409310	38.900468
2511.307913	489173.461824	38.905485
2514.128054	490087.104771	38.910503
2516.768887	490999.922523	38.915520
2519.408164	491924.752241	38.920538
2521.744872	492847.111197	38.925556
2524.027888	493755.150422	38.930573
2526.402921	494685.778726	38.935591
2528.797069	495617.210169	38.940608
2530.805052	496561.469697	38.945626
2533.475394	497507.832846	38.950644
2535.450540	498473.731614	38.955661
2537.858874	499445.603320	38.960679
2540.299076	500416.000336	38.965696
2542.377437	501406.474280	38.970714
2544.874377	502404.482245	38.975732
2546.915939	503399.229401	38.980749
2549.624346	504397.180199	38.985767
2552.387587	505414.219898	38.990784
2554.290891	506431.191242	38.995802
2557.244330	507452.355228	39.000820
2559.959415	508475.259181	39.005837
2562.035978	509510.858865	39.010855
2564.752051	510544.114343	39.015872
2566.964597	511597.800618	39.020890
2569.588517	512645.701569	39.025908
2571.879086	513708.405238	39.030925
2574.503950	514765.587645	39.035943
2577.466482	515828.233388	39.040960
2580.133139	516902.948759	39.045978
2583.097056	517954.766596	39.050996
2585.435652	519022.689310	39.056013
2588.248567	520097.810788	39.061031
2590.675223	521169.799387	39.066048
2593.511995	522245.318760	39.071066
2596.401403	523318.133617	39.076084
2598.788054	524393.677137	39.081101
2601.640137	525463.323322	39.086119
2604.267133	526539.829311	39.091136
2606.999943	527616.339799	39.096154
2609.725451	528685.171136	39.101172
2612.048727	529768.491602	39.106189
2614.582779	530837.601693	39.111207
2617.597487	531913.547612	39.116224
2619.755618	533002.796830	39.121242
2622.604483	534070.256433	39.126260
2625.198929	535159.419445	39.131277
2627.805512	536234.660337	39.136295
2630.754656	537287.019837	39.141312
2633.340711	538332.974186	39.146330
2636.486030	539361.098163	39.151348
2638.945799	540405.009368	39.156365
2641.569160	541444.388872	39.161383
2644.570806	542479.552757	39.166400
2646.655201	543522.290173	39.171418
2649.253592	544558.827074	39.176436
2651.822163	545617.567561	39.181453
2654.230930	546663.382398	39.186471
2657.362858	547713.871025	39.191488
2659.540732	548775.451905	39.196506
2661.989470	549837.758560	39.201524
2664.918171	550906.384428	39.206541
2667.016546	551985.823743	39.211559
2669.550349	553060.780270	39.216576
2672.081021	554158.265183	39.221594
2674.762003	555250.609643	39.226612
2677.796848	556362.550322	39.231629
2680.472560	557460.793987	39.236647
2683.636626	558561.676346	39.241664
2686.168278	559668.351550	39.246682
2689.052851	560758.398563	39.251700
2692.123114	561857.965994	39.256717
2694.826889	562957.854860	39.261735
2697.617806	564065.017324	39.266752
2700.015436	565182.043774	39.271770
2702.969136	566277.490544	39.276788
2705.034868	567397.192988	39.281805
2707.211559	568525.914472	39.286823
2710.030092	569657.789296	39.291840
2712.154542	570810.409701	39.296858
2714.932049	571957.343460	39.301876
2717.556856	573112.829766	39.306893
2719.390708	574285.002850	39.311911
2722.464199	575458.158681	39.316928
2725.037316	576642.175337	39.321946
2728.003141	577820.092968	39.326964
2730.498889	579010.216591	39.331981
2733.433125	580199.799177	39.336999
2737.047343	581383.383387	39.342016
2739.981060	582572.033377	39.347034
2742.692517	583748.021044	39.352052
2745.434672	584941.936593	39.357069
2747.686143	586130.604783	39.362087
2750.477367	587325.428683	39.367104
2753.259008	588534.869220	39.372122
2756.196178	589726.521496	39.377140
2758.610388	590936.432392	39.382157
2761.346833	592148.819981	39.387175
2764.766272	593348.542526	39.392192
2767.885950	594542.483449	39.397210
2771.285953	595723.482873	39.402228
2774.234032	596922.819466	39.407245
2777.060017	598085.397937	39.412263
2780.278826	599233.622607	39.417280
2782.822256	600368.280601	39.422298
2785.785380	601499.400837	39.427316
2788.678447	602629.820674	39.432333
2790.976095	603767.837994	39.437351
2794.073872	604890.290786	39.442368
2797.008535	606031.775850	39.447386
2799.641541	607162.589535	39.452404
2802.557422	608292.090593	39.457421
2805.098483	609425.193823	39.462439
2808.064729	610561.160824	39.467456
2810.546942	611710.448787	39.472474
2813.459407	612854.293212	39.477492
2816.337088	614017.777275	39.482509
2819.017543	615167.072342	39.487527
2821.893989	616310.514338	39.492544
2824.548101	617477.469808	39.497562
2827.283551	618641.587457	39.502580
2830.077562	619808.769095	39.507597
2832.429830	620987.844028	39.512615
2835.046282	622170.592599	39.517632
2837.148260	623384.025656	39.522650
2840.117852	624569.747206	39.527668
2842.795551	625801.091899	39.532685
2845.060877	627030.017228	39.537703
2848.098874	628264.261383	39.542720
2850.782227	629509.756813	39.547738
2853.457518	630757.153353	39.552756
2856.251487	632016.711886	39.557773
2858.781068	633283.750956	39.562791
2861.707656	634550.717848	39.567808
2864.383353	635837.883423	39.572826
2867.337769	637115.909696	39.577844
2870.330760	638410.733602	39.582861
2873.231436	639715.436658	39.587879
2875.983519	640997.204566	39.592896
2878.550519	642309.364181	39.597914
2881.195493	643619.595648	39.602932
2884.526442	644938.315321	39.607949
2887.170341	646261.765574	39.612967
2890.555852	647578.085926	39.617984
2893.187313	648911.805406	39.623002
2896.379542	650242.759050	39.628020
2899.370184	651567.290754	39.633037
2902.281290	652899.231155	39.638055
2905.581135	654218.771096	39.643072
2908.496863	655546.865464	39.648090
2911.283642	656872.311707	39.653108
2914.886167	658206.998426	39.658125
2917.607637	659533.039500	39.663143
2920.791926	660858.770103	39.668160
2923.904577	662181.891933	39.673178
2926.759202	663508.558229	39.678196
2929.872171	664828.826704	39.683213
2932.838059	666139.087034	39.688231
2935.917800	667411.342133	39.693248
2938.942834	668681.346799	39.698266
2942.430474	669951.151384	39.703284
2945.728754	671199.187126	39.708301
2948.636886	672458.906425	39.713319
2951.571889	673708.608727	39.718336
2954.495168	674970.322863	39.723354
2957.171427	676221.421712	39.728372
2960.082690	677469.329917	39.733389
2962.045166	678752.854492	39.738407
2964.905849	680026.160908	39.743424
2967.709989	681315.591706	39.748442
2970.324098	682603.383070	39.753460
2973.190000	683903.909346	39.758477
2975.968548	685220.697700	39.763495
2979.289739	686531.393615	39.768512
2981.866144	687855.873901	39.773530
2984.265280	689182.124575	39.778548
2987.182879	690523.968260	39.783565
2989.843122	691879.892505	39.788583
2992.391824	693236.621050	39.793600
2995.130347	694605.310034	39.798618
2997.945894	696005.510165	39.803636
3001.271925	697395.732047	39.808653
3003.655345	698798.188367	39.813671
3007.149727	700201.171485	39.818688
3010.015216	701630.647585	39.823706
3012.378999	703058.586395	39.828724
3015.490812	704479.027744	39.833741
3018.408330	705933.197132	39.838759
3021.491215	707367.431062	39.843776
3024.518777	708825.052402	39.848794
3027.007772	710292.318522	39.853812
3030.433851	711746.746996	39.858829
3033.648975	713225.953351	39.863847
3036.930239	714702.761029	39.868864
3040.052985	716177.950746	39.873882
3043.675127	717652.053034	39.878900
3046.693178	719117.788313	39.883917
3049.559610	720602.030607	39.888935
3052.924872	722072.721896	39.893952
3055.902706	723550.581720	39.898970
3058.909967	725043.243388	39.903988
3061.834037	726527.247410	39.909005
3065.220941	728018.757092	39.914023
3068.284353	729502.590122	39.919040
3071.259490	730996.536675	39.924058
3074.447925	732491.157668	39.929076
3078.012796	733966.628729	39.934093
3080.988292	735457.475564	39.939111
3084.498586	736933.198222	39.944128
3087.979915	738419.407469	39.949146
3090.692883	739905.814573	39.954164
3094.001570	741377.981844	39.959181
3097.140288	742863.512100	39.964199
3100.340851	744307.585185	39.969216
3103.110444	745743.825047	39.974234
3106.405196	747171.825415	39.979252
3109.531850	748588.505516	39.984269
3112.198741	750032.789515	39.989287
3115.020148	751463.281039	39.994304
3118.027116	752900.713771	39.999322
3120.766721	754352.742519	40.004340
3124.244583	755791.717921	40.009357
3127.694232	757245.240445	40.014375
3130.427198	758697.573476	40.019392
3133.917038	760163.126197	40.024410
3136.875991	761629.074782	40.029428
3140.216706	763093.098308	40.034445
3143.087007	764568.814764	40.039463
3145.815280	766040.871557	40.044480
3149.106635	767528.907620	40.049498
3152.049190	769022.896022	40.054516
3155.437169	770520.878678	40.059533
3158.058051	772027.381612	40.064551
3161.017476	773537.544332	40.069568
3163.785910	775059.555238	40.074586
3166.650218	776596.743938	40.079604
3169.618973	778141.343749	40.084621
3172.738687	779700.455621	40.089639
3175.807942	781253.695476	40.094656
3179.482138	782813.460875	40.099674
3182.780771	784388.691098	40.104692
3186.016818	785958.828793	40.109709
3188.914484	787539.215571	40.114727
3192.250524	789118.145934	40.119744
3195.572805	790708.287695	40.124762
3198.595819	792305.125455	40.129780
3202.025621	793878.661132	40.134797
3205.611915	795480.897243	40.139815
3208.883413	797070.973072	40.144832
3212.526661	798658.614626	40.149850
3215.671011	800262.660216	40.154868
3219.072849	801847.358853	40.159885
3222.160371	803444.215512	40.164903
3225.321192	805035.113453	40.169920
3228.754797	806639.915341	40.174938
3231.530129	808254.077590	40.179956
3235.245082	809849.862188	40.184973
3238.326177	811471.460637	40.189991
3241.743881	813079.083961	40.195008
3245.264950	814675.661007	40.200026
3248.623783	816279.205500	40.205044
3252.004549	817886.507732	40.210061
3255.363226	819490.253203	40.215079
3258.891941	821090.849240	40.220096
3262.426972	822693.444668	40.225114
3265.794107	824280.906285	40.230132
3269.241822	825857.295323	40.235149
3272.440933	827433.199604	40.240167
3275.907161	828963.566119	40.245184
3279.510179	830496.518727	40.250202
3283.257774	832019.295654	40.255220
3286.335740	833528.196097	40.260237
3289.433940	835034.937557	40.265255
3292.267479	836554.360958	40.270272
3295.742467	838066.113219	40.275290
3299.031625	839587.556392	40.280308
3302.248691	841101.596269	40.285325
3305.544472	842634.801494	40.290343
3308.809275	844160.931995	40.295360
3312.156166	845691.341819	40.300378
3315.367021	847226.743845	40.305396
3318.458408	848757.029087	40.310413
3321.592520	850307.516236	40.315431
3324.994957	851863.588568	40.320448
3328.448291	853412.175331	40.325466
3331.484914	854982.566519	40.330484
3335.036919	856542.767555	40.335501
3338.480832	858115.196566	40.340519
3341.578652	859679.716825	40.345536
3345.662493	861249.869664	40.350554
3348.821384	862821.324029	40.355572
3351.994321	864400.989476	40.360589
3355.155148	865989.346853	40.365607
3358.228380	867568.293902	40.370624
3361.941324	869171.012425	40.375642
3365.128756	870772.325393	40.380660
3368.183304	872381.937198	40.385677
3371.291272	873991.005947	40.390695
3374.562477	875610.341843	40.395712
3377.558000	877258.860396	40.400730
3380.568787	878901.018036	40.405748
3384.431356	880539.477503	40.410765
3387.825357	882185.766389	40.415783
3391.133817	883836.817683	40.420800
3394.491397	885486.038410	40.425818
3397.595037	887164.747903	40.430836
3401.231712	888842.104755	40.435853
3404.446148	890518.367824	40.440871
3407.498796	892185.971105	40.445888
3410.669347	893875.139812	40.450906
3414.236021	895580.505446	40.455924
3417.336598	897277.729897	40.460941
3421.027025	898989.462670	40.465959
3424.179152	900697.973958	40.470976
3427.926243	902412.311010	40.475994
3431.100137	904129.586952	40.481012
3434.906044	905841.319442	40.486029
3438.652846	907562.149207	40.491047
3441.974706	909279.631817	40.496064
3445.489606	910991.741073	40.501082
3448.286655	912712.661237	40.506100
3452.285954	914438.116888	40.511117
3455.724561	916140.903305	40.516122
3458.870846	917805.264503	40.521127
3462.463962	919396.027434	40.526132
3465.471680	920935.742211	40.531136
3468.494002	922409.254803	40.536141
3472.387747	923809.455708	40.541146
3475.222021	925124.238898	40.546151
3478.649546	926359.340744	40.551156
3481.470980	927519.630797	40.556160
3484.223330	928597.095382	40.561165
3487.196750	929608.152661	40.566170
3489.531999	930537.915925	40.571175
3492.070975	931399.049109	40.576180
3493.833711	932205.667451	40.581184
3496.219243	932923.878667	40.586189
3498.276825	933588.994400	40.591194
3500.083308	934187.687762	40.596199
3501.893970	934734.900877	40.601204
3503.394395	935221.784027	40.606208
3505.062586	935647.025699	40.611213
3506.725540	936049.123565	40.616218
3507.936718	936386.928079	40.621223
3509.737034	936662.479300	40.626228
3511.388556	936913.017532	40.631232
3512.309573	937107.678664	40.636237
3513.481198	937259.244033	40.641242
3514.534155	937383.023508	40.646247
3515.742432	937464.017102	40.651252
3516.743609	937516.956166	40.656256
3517.979396	937521.250929	40.661261
3518.970588	937505.839072	40.666266
3519.720366	937460.653869	40.671271
3520.843600	937377.153178	40.676276
3521.423922	937270.447385	40.681280
3522.029116	937126.057212	40.686285
3522.704173	936975.035703	40.691290
3523.077711	936797.215237	40.696295
3524.139807	936587.629935	40.701300
3524.136249	936371.122519	40.706304
3524.834205	936139.239730	40.711309
3525.456849	935884.919966	40.716314
3525.748231	935618.081426	40.721319
3526.315631	935334.494587	40.726324
3526.371974	935038.031635	40.731328
3526.772826	934722.885238	40.736333
3527.654127	934405.431678	40.741338
3527.664657	934070.648528	40.746343
3528.147503	933709.860880	40.751348
3528.112863	933365.255055	40.756352
3528.675367	932982.337228	40.761357
3529.150188	932611.113110	40.766362
3528.772697	932223.406807	40.771367
3529.480948	931823.010564	40.776372
3529.613306	931428.728803	40.781376
3529.711592	931010.427284	40.786381
3530.282526	930599.019396	40.791386
3530.271375	930170.686898	40.796391
3530.794679	929731.571626	40.801396
3530.826943	929296.728466	40.806400
3530.873077	928835.632732	40.811405
3530.830416	928395.447112	40.816410
3530.939432	927945.499044	40.821415
3530.976796	927478.044273	40.826420
3531.315652	927028.267489	40.831424
3531.281527	926553.539434	40.836429
3531.470248	926085.648355	40.841434
3531.556992	925620.327850	40.846439
3531.468249	925134.048950	40.851444
3531.459471	924656.937693	40.856448
3531.479686	924170.936962	40.861453
3531.923761	923684.531398	40.866458
3531.771453	923200.586622	40.871463
3532.062702	922707.678086	40.876468
3532.183317	922214.945703	40.881472
3532.012049	921704.718240	40.886477
3532.084677	921210.363521	40.891482
3531.978600	920704.838163	40.896487
3532.322953	920194.668055	40.901492
3532.072767	919696.286164	40.906496
3532.404341	919185.830492	40.911501
3532.892545	918672.509888	40.916506
3532.529147	918156.399481	40.921511
3532.730689	917626.190815	40.926516
3532.863384	917104.025732	40.931520
3532.576839	916578.224703	40.936525
3532.694854	916058.656398	40.941530
3532.545083	915543.704730	40.946535
3532.792958	915011.403901	40.951540
3532.415188	914485.319830	40.956544
3532.743918	913957.234890	40.961549
3532.742754	913432.910857	40.966554
3532.812872	912901.108588	40.971559
3532.661842	912361.875880	40.976564
3532.968331	911829.832861	40.981568
3532.796482	911294.640747	40.986573
3532.943647	910758.089472	40.991578
3532.847621	910214.107912	40.996583
3533.015085	909673.978534	41.001588
3532.805848	909137.811827	41.006592
3533.118957	908593.118365	41.011597
3533.143790	908052.661656	41.016602
3532.767144	907496.410463	41.021607
3532.781642	906948.038793	41.026612
3532.804010	906414.267630	41.031616
3532.879171	905868.285650	41.036621
3532.655843	905318.443224	41.041626
3532.521032	904775.282774	41.046631
3533.038000	904226.556213	41.051636
3532.911329	903676.631310	41.056640
3532.594321	903127.938825	41.061645
3532.869518	902580.442087	41.066650
3532.931961	902035.726416	41.071655
3532.717440	901490.232861	41.076660
3532.864152	900939.316009	41.081664
3532.699420	900388.784229	41.086669
3532.796228	899829.658563	41.091674
3532.503069	899283.480867	41.096679
3532.908320	898720.330276	41.101684
3533.004240	898172.047072	41.106688
3532.743448	897609.574980	41.111693
3532.927945	897057.401782	41.116698
3532.582770	896497.054551	41.121703
3532.521290	895937.762531	41.126708
3532.726385	895387.451245	41.131712
3532.709121	894826.979153	41.136717
3533.109144	894270.438917	41.141722
3532.544593	893713.428910	41.146727
3532.841655	893138.046921	41.151732
3533.052803	892582.823348	41.156736
3532.907792	892017.166127	41.161741
3533.396666	891447.477388	41.166746
3532.938231	890884.565012	41.171751
3532.998716	890308.454290	41.176756
3533.014682	889745.445427	41.181760
3533.064945	889182.858929	41.186765
3532.761337	888608.670366	41.191770
3532.600782	888045.621376	41.196775
3532.882514	887472.186594	41.201780
3532.522743	886910.414846	41.206784
3532.835120	886342.280560	41.211789
3532.903135	885768.519053	41.216794
3532.385559	885191.122643	41.221799
3532.902920	884628.688522	41.226804
3532.790020	884069.405014	41.231808
3532.915676	883498.021968	41.236813
3532.878960	882924.480225	41.241818
3532.446608	882352.208146	41.246823
3532.915360	881778.951133	41.251828
3532.785734	881213.584713	41.256832
3533.165465	880634.419120	41.261837
3533.068177	880049.852692	41.266842
3532.842658	879490.632109	41.271847
3532.942491	878900.104166	41.276852
3533.245365	878319.850156	41.281856
3533.112731	877730.891230	41.286861
3533.114910	877152.123478	41.291866
3533.216288	876569.404618	41.296871
3533.063628	875982.309163	41.301876
3533.041283	875398.138245	41.306880
3532.844913	874812.775625	41.311885
3532.902967	874224.984279	41.316890
3532.521966	873639.439823	41.321895
3532.644860	873053.266418	41.326900
3532.372378	872469.624336	41.331904
3532.836513	871887.642113	41.336909
3533.005545	871310.794946	41.341914
3532.420030	870733.923542	41.346919
3532.306487	870143.233924	41.351924
3532.388582	869568.464354	41.356928
3532.476924	868992.085468	41.361933
3532.675481	868408.158375	41.366938
3532.434359	867837.256767	41.371943
3532.589694	867243.516227	41.376948
3532.359176	866667.355955	41.381952
3532.262401	866077.135207	41.386957
3532.848961	865500.529212	41.391962
3532.471018	864917.914129	41.396967
3532.596645	864322.044453	41.401972
3532.774474	863751.848234	41.406976
3532.420480	863162.745409	41.411981
3532.387582	862566.437920	41.416986
3532.158272	861998.283051	41.421991
3532.215401	861412.243068	41.426996
3532.062535	860831.721733	41.432000
3531.520729	860244.990891	41.437005
3532.118987	859666.368156	41.442010
3531.776620	859096.988835	41.447015
3531.790160	858514.467947	41.452020
3531.777986	857939.479721	41.457024
3531.917690	857356.340556	41.462029
3531.923108	856786.783434	41.467034
3531.516219	856215.979323	41.472039
3531.834655	855628.851958	41.477044
3531.572264	855062.389993	41.482048
3531.663987	854482.876450	41.487053
3531.654384	853894.179934	41.492058
3531.501603	853321.409275	41.497063
3531.604264	852745.622397	41.502068
3531.868254	852166.347993	41.507072
3532.014276	851587.720715	41.512077
3531.822819	851005.787358	41.517082
3531.718111	850426.315551	41.522087
3531.738979	849844.820974	41.527092
3531.455223	849260.987101	41.532096
3531.610464	848690.656061	41.537101
3531.719079	848099.635075	41.542106
3531.569024	847531.587194	41.547111
3531.683036	846945.812532	41.552116
3531.507894	846364.708056	41.557120
3531.449453	845786.841951	41.562125
3531.630749	845199.625680	41.567130
3531.362718	844627.339304	41.572135
3531.535261	844034.071563	41.577140
3531.515156	843466.217074	41.582144
3531.483761	842880.769310	41.587149
3531.804859	842294.524603	41.592154
3530.965876	841714.564930	41.597159
3531.276784	841124.118833	41.602164
3530.923777	840559.471539	41.607168
3530.884510	839981.702559	41.612173
3531.062646	839396.334716	41.617178
3531.126173	838829.121560	41.622183
3531.291995	838238.187372	41.627188
3531.164096	837663.441168	41.632192
3531.163689	837086.377514	41.637197
3530.812560	836501.223620	41.642202
3530.847353	835927.463823	41.647207
3530.742132	835354.701000	41.652212
3530.724389	834783.287008	41.657216
3530.792165	834204.731457	41.662221
3531.080627	833626.037217	41.667226
3530.829920	833059.292125	41.672231
3530.867335	832467.162785	41.677236
3530.838201	831902.865024	41.682240
3531.063218	831318.164653	41.687245
3530.910980	830731.864417	41.692250
3530.847795	830157.947519	41.697255
3530.838314	829579.917216	41.702260
3530.783791	829001.061556	41.707264
3530.796278	828422.484658	41.712269
3530.742858	827845.235162	41.717274
3530.768172	827272.757302	41.722279
3531.058561	826684.598571	41.727284
3530.591861	826107.314244	41.732288
3530.622786	825540.741924	41.737293
3530.941743	824954.474603	41.742298
3530.817343	824366.275433	41.747303
3530.871693	823788.110690	41.752308
3530.900319	823209.312733	41.757312
3530.628634	822617.755489	41.762317
3530.736052	822044.952295	41.767322
3530.556495	821472.245996	41.772327
3531.056832	820872.381103	41.777332
3530.613032	820286.609459	41.782336
3530.435241	819708.614700	41.787341
3530.625193	819122.387077	41.792346
3530.467520	818552.211705	41.797351
3530.688979	817970.621708	41.802356
3530.513257	817396.044902	41.807360
3530.638077	816802.773705	41.812365
3530.548044	816225.047378	41.817370
3530.353718	815642.982137	41.822375
3530.459038	815056.018527	41.827380
3530.287491	814468.903729	41.832384
3530.552223	813895.075559	41.837389
3530.704542	813312.845980	41.842394
3530.386995	812731.233540	41.847399
3530.514734	812146.311989	41.852404
3530.094871	811562.608227	41.857408
3529.930495	810983.952303	41.862413
3530.327631	810407.550658	41.867418
3530.161253	809831.930657	41.872423
3530.320778	809251.552348	41.877428
3530.512028	808667.297623	41.882432
3530.354552	808082.121115	41.887437
3530.444959	807500.085609	41.892442
3530.358684	806918.324348	41.897447
3530.084163	806332.428875	41.902452
3529.837591	805764.415959	41.907456
3529.928594	805179.191981	41.912461
3529.999096	804596.225159	41.917466
3529.831930	804018.543605	41.922471
3529.912164	803443.418453	41.927476
3529.953861	802863.838755	41.932480
3530.026942	802286.460306	41.937485
3529.980006	801698.461247	41.942490
3529.593261	801129.106437	41.947495
3529.810838	800545.230372	41.952500
3529.643792	799978.832910	41.957504
3529.466134	799406.258764	41.962509
3529.623663	798830.881622	41.967514
3529.378357	798255.083789	41.972519
3529.381243	797675.073968	41.977524
3529.554879	797103.770374	41.982528
3529.408703	796539.148699	41.987533
3529.747842	795959.625170	41.992538
3529.128183	795383.800200	41.997543
3529.561673	794812.214865	42.002548
3529.471462	794249.214152	42.007552
3529.391522	793676.543432	42.012557
3529.647013	793105.928957	42.017562
3529.412369	792529.704655	42.022567
3529.325374	791952.671147	42.027572
3529.124943	791378.949200	42.032576
3529.071684	790803.829141	42.037581
3529.090624	790239.112380	42.042586
3528.955606	789676.587224	42.047591
3529.077474	789100.266586	42.052596
3529.412053	788539.437515	42.057600
3529.103750	787973.367025	42.062605
3529.482572	787390.672054	42.067610
3528.932622	786820.226342	42.072615
3529.102109	786245.729264	42.077620
3529.210866	785668.984280	42.082624
3528.975941	785099.427998	42.087629
3528.904691	784530.633961	42.092634
3528.681060	783965.901180	42.097639
3528.722930	783393.949111	42.102644
3528.663934	782836.375797	42.107648
3528.606981	782265.235486	42.112653
3528.619232	781697.578780	42.117658
3528.851745	781140.512342	42.122663
3528.481854	780565.994997	42.127668
3528.585895	780005.567065	42.132672
3528.345963	779446.236557	42.137677
3528.583095	778881.517001	42.142682
3528.645767	778320.276463	42.147687
3528.729545	777750.623720	42.152692
3528.744510	777189.008381	42.157696
3528.452989	776633.553602	42.162701
3528.418859	776062.213519	42.167706
3528.299142	775504.034518	42.172711
3528.415110	774938.634815	42.177716
3528.668756	774378.681413	42.182720
3528.614658	773810.761863	42.187725
3528.514443	773248.566741	42.192730
3528.509690	772682.471365	42.197735
3528.410731	772105.613060	42.202740
3528.684171	771554.944335	42.207744
3528.669871	770983.351422	42.212749
3528.518169	770417.352689	42.217754
3528.267599	769849.948058	42.222759
3528.643107	769281.112033	42.227764
3528.120405	768718.888772	42.232768
3528.088156	768158.460570	42.237773
3528.018695	767601.396224	42.242778
3527.824909	767046.479465	42.247783
3528.049455	766477.601576	42.252788
3527.881595	765918.752114	42.257792
3527.676258	765361.050007	42.262797
3528.006341	764805.728679	42.267802
3527.881669	764257.049393	42.272807
3527.410767	763695.570819	42.277812
3527.848528	763138.776047	42.282816
3527.757197	762590.313880	42.287821
3527.715498	762032.433970	42.292826
3527.305085	761480.444011	42.297831
3527.485580	760926.931703	42.302836
3527.264705	760380.352299	42.307840
3527.344296	759829.834538	42.312845
3527.400524	759267.589535	42.317850
3527.280403	758726.101973	42.322855
3527.344153	758172.752827	42.327860
3527.312441	757627.569999	42.332864
3527.466562	757084.240644	42.337869
3527.431215	756527.877094	42.342874
3527.083728	755987.910563	42.347879
3527.376142	755437.629496	42.352884
3527.061574	754892.298743	42.357888
3527.045499	754341.102768	42.362893
3527.180679	753783.275661	42.367898
3526.935905	753251.983626	42.372903
3526.858765	752703.642179	42.377908
3526.815631	752161.378272	42.382912
3526.769414	751610.040244	42.387917
3526.877307	751076.216525	42.392922
3526.749589	750542.988639	42.397927
3527.379322	750001.642879	42.402932
3527.389158	749447.522854	42.407936
3526.944638	748904.060869	42.412941
3527.149298	748363.364459	42.417946
3526.974155	747813.308535	42.422951
3527.124859	747260.440599	42.427956
3526.861784	746726.132786	42.432960
3527.129646	746189.819898	42.437965
3527.045317	745631.440772	42.442970
3526.740080	745091.641509	42.447975
3526.651411	744535.260318	42.452980
3526.580938	744002.363906	42.457984
3526.407246	743464.851760	42.462989
3526.296547	742915.674934	42.467994
3525.925198	742392.607248	42.472999
3526.179698	741847.742751	42.478004
3526.233614	741320.773622	42.483008
3526.245504	740794.320331	42.488013
3526.339009	740251.548587	42.493018
3526.077905	739721.806570	42.498023
3526.228003	739191.464273	42.503028
3526.462778	738654.889365	42.508032
3525.953401	738120.729994	42.513037
3526.144146	737584.436426	42.518042
3526.014302	737059.045008	42.523047
3526.415607	736524.424952	42.528052
3526.005530	735994.607905	42.533056
3525.848595	735465.108284	42.538061
3525.981834	734935.771431	42.543066
3525.736596	734413.095457	42.548071
3525.978799	733882.284658	42.553076
3526.063992	733353.098815	42.558080
3526.072344	732825.475108	42.563085
3526.278142	732285.358440	42.568090
3525.888994	731771.296536	42.573095
3525.866947	731230.504452	42.578100
3525.786720	730701.618011	42.583104
3525.711188	730177.399909	42.588109
3525.723197	729635.405909	42.593114
3525.539912	729117.376634	42.598119
3525.503267	728587.255109	42.603124
3525.666834	728066.623368	42.608128
3525.643878	727548.813303	42.613133
3525.720825	727025.256983	42.618138
3525.459871	726501.873316	42.623143
3525.176628	725978.558952	42.628148
3525.385583	725460.824378	42.633152
3525.568652	724939.444650	42.638157
3525.511447	724405.140596	42.643162
3525.329777	723900.058454	42.648167
3525.249320	723374.808758	42.653172
3525.403591	722849.287195	42.658176
3525.198316	722333.507426	42.663181
3525.413963	721809.891511	42.668186
3525.366837	721299.918230	42.673191
3525.373179	720773.397423	42.678196
3525.521848	720256.039480	42.683200
3525.491254	719733.127251	42.688205
3525.266137	719215.024492	42.693210
3525.304805	718693.522324	42.698215
3525.617233	718172.486157	42.703220
3525.518612	717638.445641	42.708224
3525.266592	717117.588630	42.713229
3525.587999	716597.345147	42.718234
3525.166914	716076.104877	42.723239
3525.266089	715553.900090	42.728244
3525.019688	715037.624694	42.733248
3525.091930	714522.850566	42.738253
3525.167405	713998.271050	42.743258
3525.076641	713486.041010	42.748263
3524.924414	712960.592258	42.753268
3524.728366	712454.420342	42.758272
3524.950440	711942.340836	42.763277
3524.815883	711421.209683	42.768282
3524.968989	710906.300197	42.773287
3525.008150	710394.207897	42.778292
3524.984167	709878.968484	42.783296
3524.841153	709368.036638	42.788301
3524.567207	708841.161749	42.793306
3524.759586	708337.755504	42.798311
3524.849304	707823.017614	42.803316
3524.714010	707314.791236	42.808321
3524.436297	706787.740568	42.813325
3524.914760	706286.399030	42.818330
3524.485732	705775.598990	42.823335
3524.880228	705262.740814	42.828340
3524.638695	704743.702884	42.833345
3524.582371	704238.210949	42.838349
3524.901116	703725.274098	42.843354
3524.280016	703213.957412	42.848359
3523.886141	702712.407582	42.853364
3524.324009	702211.382178	42.858369
3524.077574	701704.035633	42.863373
3524.130842	701207.886730	42.868378
3523.994029	700700.015601	42.873383
3524.148786	700200.611834	42.878388
3524.129857	699704.240377	42.883393
3523.763977	699203.476905	42.888397
3524.241021	698696.427779	42.893402
3523.991313	698191.759610	42.898407
3523.941500	697686.232921	42.903412
3524.033353	697190.196784	42.908417
3523.517518	696691.203993	42.913421
3524.057158	696188.124999	42.918426
3523.712778	695696.354326	42.923431
3523.613248	695205.956233	42.928436
3523.537139	694706.576929	42.933441
3523.471718	694219.797607	42.938445
3523.682267	693726.827895	42.943450
3523.492777	693239.568254	42.948455
3523.278411	692745.174260	42.953460
3523.499703	692254.905864	42.958465
3523.122476	691764.165469	42.963469
3523.222210	691271.575624	42.968474
3523.633608	690780.546872	42.973479
3523.940084	690296.672509	42.978484
3523.787547	689801.855691	42.983489
3523.722155	689307.842387	42.988493
3523.743921	688809.707038	42.993498
3523.701659	688319.914204	42.998503
3523.652248	687833.429792	43.003508
3523.669915	687337.253567	43.008513
3523.267425	686846.197807	43.013517
3523.282003	686349.470000	43.018522
3523.176133	685867.716516	43.023527
3523.497464	685378.348553	43.028532
3523.528055	684887.460671	43.033537
3523.204507	684396.556850	43.038541
3522.923094	683912.489144	43.043546
3523.037536	683432.957993	43.048551
3523.085918	682945.546447	43.053556
3523.099453	682456.621045	43.058561
3523.037802	681981.823301	43.063565
3522.950741	681489.576904	43.068570
3522.607462	681013.531986	43.073575
3522.933983	680528.732475	43.078580
3522.983017	680055.060732	43.083585
3522.549658	679577.761262	43.088589
3522.580535	679096.920949	43.093594
3522.340821	678627.558136	43.098599
3522.258692	678150.423423	43.103604
3522.452282	677673.017664	43.108609
3522.327228	677198.431431	43.113613
3522.730051	676735.438605	43.118618
3522.558801	676266.392335	43.123623
3522.432047	675788.495509	43.128628
3522.395228	675314.694460	43.133633
3522.370964	674850.334980	43.138637
3522.707777	674376.771118	43.143642
3522.558334	673911.987486	43.148647
3522.511460	673435.102223	43.153652
3522.473457	672963.424383	43.158657
3522.182754	672487.578998	43.163661
3522.184141	671998.101358	43.168666
3521.863399	671539.310124	43.173671
3521.774590	671084.744034	43.178676
3521.946676	670617.348878	43.183681
3521.739172	670168.242589	43.188685
3522.072806	669705.710288	43.193690
3521.997427	669247.812311	43.198695
3522.031202	668789.424701	43.203700
3521.623046	668326.003989	43.208705
3521.365832	667863.232944	43.213709
3522.094878	667403.911452	43.218714
3521.599488	666950.961000	43.223719
3521.618575	666479.497077	43.228724
3521.470376	666029.535673	43.233729
3521.405902	665579.987614	43.238733
3521.894113	665115.209577	43.243738
3521.649006	664670.088992	43.248743
3521.347887	664219.868719	43.253748
3521.303849	663772.077832	43.258753
3521.160958	663322.586547	43.263757
3521.237866	662866.251032	43.268762
3521.154864	662420.898378	43.273767
3521.309266	661971.143341	43.278772
3521.271723	661519.403996	43.283777
3521.187552	661083.021726	43.288781
3521.587869	660625.127379	43.293786
3521.232796	660180.765601	43.298791
3521.338009	659732.910894	43.303796
3521.193682	659282.332859	43.308801
3521.009737	658841.074764	43.313805
3521.412151	658380.328526	43.318810
3520.978705	657946.759662	43.323815
3520.985974	657491.579843	43.328820
3521.274436	657054.303500	43.333825
3521.184499	656609.982579	43.338829
3521.429982	656154.400102	43.343834
3521.413952	655711.623420	43.348839
3521.178828	655261.873425	43.353844
3521.008337	654818.233840	43.358849
3520.546111	654376.921137	43.363853
3521.143363	653928.815611	43.368858
3520.907499	653501.458137	43.373863
3520.779815	653053.486456	43.378868
3520.977551	652613.979779	43.383873
3520.419980	652182.024895	43.388877
3520.600702	651729.694791	43.393882
3520.523548	651300.366685	43.398887
3520.487140	650861.321601	43.403892
3520.606050	650430.673452	43.408897
3520.490481	649998.048253	43.413901
3520.432619	649565.993919	43.418906
3520.430159	649135.710087	43.423911
3520.217488	648699.397604	43.428916
3520.338168	648274.901689	43.433921
3520.295335	647838.072842	43.438925
3520.412902	647406.844487	43.443930
3520.084630	646982.770154	43.448935
3520.239286	646552.598150	43.453940
3520.199956	646125.839431	43.458945
3520.023346	645716.029762	43.463949
3520.271162	645283.088506	43.468954
3520.063973	644861.053232	43.473959
3520.007076	644428.527173	43.478964
3520.146925	644006.396901	43.483969
3519.952296	643576.457351	43.488973
3519.992539	643146.909383	43.493978
3519.735839	642730.542925	43.498983
3519.988102	642318.672325	43.503988
3519.928529	641895.438185	43.508993
3519.930268	641473.526026	43.513997
3519.748173	641051.427749	43.519002
3519.723526	640637.436179	43.524007
3519.840088	640221.803431	43.529012
3520.112754	639803.226508	43.534017
3519.824544	639383.577924	43.539021
3519.450745	638953.923801	43.544026
3519.378665	638547.357943	43.549031
3519.402383	638135.657713	43.554036
3519.887498	637720.360765	43.559041
3519.087829	637319.322804	43.564045
3519.126661	636906.970556	43.569050
3519.221455	636496.843470	43.574055
3519.048976	636087.996443	43.579060
3519.184553	635686.084943	43.584065
3519.098626	635274.989653	43.589069
3519.198834	634870.400806	43.594074
3519.114312	634477.786444	43.599079
3519.244412	634065.855806	43.604084
3519.365475	633664.018558	43.609089
3518.810338	633261.830863	43.614093
3518.997425	632849.592155	43.619098
3518.714487	632444.223699	43.624103
3518.776753	632031.373439	43.629108
3518.986186	631639.252569	43.634113
3518.841669	631241.371415	43.639117
3518.928887	630839.130958	43.644122
3518.934852	630439.291636	43.649127
3518.587767	630038.546276	43.654132
3518.630610	629633.864480	43.659137
3518.371571	629245.288428	43.664141
3518.530239	628855.174902	43.669146
3518.290404	628475.778877	43.674151
3518.313769	628084.909021	43.679156
3518.394812	627703.477885	43.684161
3518.504847	627311.813654	43.689165
3518.576018	626913.281655	43.694170
3518.506935	626530.982738	43.699175
3518.387800	626138.162618	43.704180
3518.795960	625750.145617	43.709185
3518.381283	625369.065821	43.714189
3518.597086	624969.584962	43.719194
3518.434832	624579.619490	43.724199
3518.444577	624189.109570	43.729204
3518.626963	623791.193106	43.734209
3518.177861	623411.902613	43.739213
3518.369571	623014.907430	43.744218
3517.977409	622645.848747	43.749223
3518.050191	622257.311510	43.754228
3518.353683	621867.919318	43.759233
3517.977861	621482.937459	43.764237
3518.113682	621103.565872	43.769242
3518.032359	620729.027770	43.774247
3517.972619	620347.959590	43.779252
3518.190173	619970.688731	43.784257
3517.848433	619591.646276	43.789261
3518.048407	619205.683332	43.794266
3517.928569	618833.240928	43.799271
3517.648876	618453.747270	43.804276
3517.985167	618072.230889	43.809281
3517.613097	617699.241486	43.814285
3517.631486	617321.812469	43.819290
3517.517484	616952.963339	43.824295
3517.538113	616580.319735	43.829300
3517.772797	616222.563325	43.834305
3517.272777	615852.740569	43.839309
3517.290289	615472.390854	43.844314
3517.284343	615111.882389	43.849319
3517.191858	614745.110759	43.854324
3517.236741	614387.076306	43.859329
3517.009934	614030.831229	43.864333
3517.097352	613659.380571	43.869338
3517.285333	613296.824376	43.874343
3517.035225	612931.072167	43.879348
3517.169581	612570.607082	43.884353
3517.011266	612223.768291	43.889357
3516.983884	611855.836650	43.894362
3517.018545	611502.173173	43.899367
3516.869770	611148.078451	43.904372
3517.159137	610786.626357	43.909377
3516.879219	610432.029775	43.914381
3516.888353	610072.558154	43.919386
3516.850529	609721.759214	43.924391
3516.627371	609367.520328	43.929396
3516.801352	609023.233380	43.934401
3516.572125	608681.462348	43.939405
3517.020622	608320.304550	43.944410
3516.691369	607967.193124	43.949415
3516.683650	607622.793888	43.954420
3516.657167	607269.207548	43.959425
3516.655193	606925.588590	43.964429
3516.860574	606577.559337	43.969434
3516.596630	606223.629569	43.974439
3516.418414	605871.630654	43.979444
3516.576829	605531.303176	43.984449
3516.180829	605188.401010	43.989453
3516.560550	604832.662145	43.994458
3516.242065	604500.864443	43.999463
3516.307592	604155.393669	44.004468
3516.048032	603816.089607	44.009473
3516.471151	603481.275377	44.014477
3516.445313	603131.624221	44.019482
3516.718879	602792.148450	44.024487
3517.038043	602443.772237	44.029492
3516.841080	602094.670554	44.034497
3516.128807	601753.425182	44.039501
3516.687211	601394.185943	44.044506
3516.670811	601060.329401	44.049511
3516.625632	600714.472280	44.054516
3516.465378	600365.361841	44.059521
3516.249777	600026.188779	44.064525
3516.186429	599677.442474	44.069530
3516.179450	599344.689016	44.074535
3515.879393	599009.516245	44.079540
3516.035630	598675.761853	44.084545
3516.006433	598342.983322	44.089549
3516.169908	598009.710494	44.094554
3515.999295	597679.246382	44.099559
3516.027400	597337.492729	44.104564
3516.048170	596994.424866	44.109569
3515.901068	596668.898537	44.114573
3515.975566	596329.467146	44.119578
3515.722432	596001.379506	44.124583
3515.843603	595668.096954	44.129588
3516.065184	595329.866683	44.134593
3515.834129	595004.308196	44.139597
3515.897473	594669.349886	44.144602
3515.944413	594345.834757	44.149607
3515.866149	594018.716196	44.154612
3515.882579	593684.189720	44.159617
3515.439033	593361.032501	44.164621
3515.455741	593038.842534	44.169626
3515.309517	592715.265232	44.174631
3515.408341	592390.331287	44.179636
3515.229460	592078.947357	44.184641
3515.178592	591763.967015	44.189645
3515.233900	591433.991155	44.194650
3515.256722	591126.415509	44.199655
3515.167176	590811.818273	44.204660
3515.332801	590489.684023	44.209665
3515.156921	590186.840055	44.214669
3515.159128	589853.262428	44.219674
3514.805577	589548.473226	44.224679
3514.887451	589237.120805	44.229684
3515.147392	588923.519189	44.234689
3514.976433	588613.550180	44.239693
3515.006308	588299.870961	44.244698
3514.613643	587995.149204	44.249703
3514.910800	587694.170950	44.254708
3515.006736	587377.541911	44.259713
3514.610500	587071.691777	44.264717
3514.835741	586764.220198	44.269722
3514.845477	586457.179559	44.274727
3514.646747	586147.101184	44.279732
3514.934898	585843.414596	44.284737
3514.676390	585549.010591	44.289741
3514.839448	585242.867663	44.294746
3514.697607	584938.176271	44.299751
3514.474811	584632.184248	44.304756
3514.634281	584326.571565	44.309761
3514.205545	584031.053857	44.314765
3514.472486	583721.889175	44.319770
3514.671128	583435.749709	44.324775
3514.566910	583145.684168	44.329780
3514.473076	582828.767053	44.334785
3514.390454	582533.455378	44.339789
3514.300072	582247.287007	44.344794
3514.158207	581951.468630	44.349799
3514.389438	581658.143270	44.354804
3514.579267	581355.919492	44.359809
3514.113491	581070.089238	44.364813
3514.425840	580772.254299	44.369818
3514.572446	580479.920638	44.374823
3514.322900	580186.340398	44.379828
3514.300868	579882.960020	44.384833
3514.339812	579596.757816	44.389837
3514.285875	579301.815719	44.394842
3514.171065	579011.452723	44.399847
3514.063983	578721.483835	44.404852
3514.002338	578424.158656	44.409857
3514.051602	578138.021348	44.414861
3514.116146	577847.047150	44.419866
3513.875783	577561.147081	44.424871
3513.585159	577279.121341	44.429876
3513.867513	576990.755202	44.434881
3514.041899	576714.219567	44.439885
3513.930222	576425.002280	44.444890
3513.967528	576141.939101	44.449895
3514.196444	575856.372252	44.454900
3513.873945	575572.603101	44.459905
3513.692956	575288.652425	44.464909
3513.866901	575004.936478	44.469914
3513.730261	574726.397777	44.474919
3513.503869	574448.119694	44.479924
3513.772484	574172.064834	44.484929
3513.699592	573886.554729	44.489933
3513.536865	573608.297397	44.494938
3513.133916	573338.174211	44.499943
3513.104747	573060.988667	44.504948
3513.594678	572793.015442	44.509953
3513.289288	572523.562389	44.514957
3513.102688	572253.680796	44.519962
3513.496662	571992.750393	44.524967
3512.883406	571720.112758	44.529972
3513.129758	571440.831979	44.534977
3512.689814	571180.329031	44.539981
3513.179188	570924.643319	44.544986
3513.300075	570657.543093	44.549991
3513.141052	570388.723891	44.554996
3513.237203	570125.742750	44.560001
3512.871642	569865.049070	44.565005
3513.166393	569592.562787	44.570010
3513.147575	569328.477691	44.575015
3513.160478	569066.696565	44.580020
3513.256864	568797.145856	44.585025
3512.954509	568533.897870	44.590029
3513.221346	568271.000204	44.595034
3513.100669	568009.824091	44.600039
3512.886619	567749.816133	44.605044
3513.103583	567482.028883	44.610049
3513.343152	567214.332832	44.615053
3513.296536	566948.542318	44.620058
3513.029512	566688.672843	44.625063
3512.917907	566429.123902	44.630068
3513.067884	566163.736566	44.635073
3512.746635	565911.461153	44.640077
3512.992404	565637.640544	44.645082
3512.998183	565382.731755	44.650087
3512.441727	565123.484108	44.655092
3512.759039	564866.196334	44.660097
3512.664760	564616.373798	44.665101
3512.786762	564358.052094	44.670106
3512.761585	564114.400091	44.675111
3512.533527	563855.675039	44.680116
3512.431558	563603.115688	44.685121
3512.732447	563353.050263	44.690125
3512.867117	563099.735871	44.695130
3513.029454	562848.979543	44.700135
3512.454986	562591.194678	44.705140
3512.889964	562334.843541	44.710145
3512.647134	562081.825523	44.715149
3512.459856	561822.801272	44.720154
3512.299513	561572.025097	44.725159
3511.773981	561325.787915	44.730164
3512.046004	561075.633336	44.735169
3511.991986	560843.305089	44.740173
3512.290294	560606.632284	44.745178
3511.941791	560361.001346	44.750183
3511.946288	560120.139914	44.755188
3512.419984	559867.913523	44.760193
3512.092837	559637.020589	44.765197
3512.279657	559392.337684	44.770202
3512.098072	559147.259873	44.775207
3511.796427	558912.723815	44.780212
3512.251400	558669.240761	44.785217
3512.080769	558446.156945	44.790221
3512.163906	558197.994416	44.795226
3512.335886	557947.344103	44.800231
3512.010379	557710.373163	44.805236
3512.231040	557476.226085	44.810241
3511.986609	557236.764781	44.815245
3512.031664	556993.975670	44.820250
3512.433402	556754.949412	44.825255
3511.860475	556518.402369	44.830260
3511.716967	556278.755429	44.835265
3511.643563	556048.663195	44.840269
3512.232933	555810.192402	44.845274
3511.934667	555578.065073	44.850279
3511.856356	555346.903672	44.855284
3511.846876	555097.792233	44.860289
3511.623267	554876.168780	44.865293
3511.676534	554638.272363	44.870298
3511.893373	554410.570895	44.875303
3511.842602	554185.430279	44.880308
3511.659132	553953.355886	44.885313
3511.586254	553723.122742	44.890317
3511.631540	553493.721989	44.895322
3511.505120	553277.244963	44.900327
3511.333056	553042.280978	44.905332
3511.923373	552818.066058	44.910337
3511.575276	552591.135590	44.915341
3511.734924	552354.591368	44.920346
3511.719752	552123.917901	44.925351
3511.479681	551895.193681	44.930356
3511.811908	551663.697199	44.935361
3511.427067	551448.948193	44.940365
3511.027256	551213.386542	44.945370
3511.307912	551000.834822	44.950375
3511.261214	550779.012884	44.955380
3511.487682	550560.265120	44.960385
3511.533360	550339.428108	44.965389
3511.489558	550117.796450	44.970394
3511.223037	549896.451187	44.975399
3511.292488	549672.625879	44.980404
3510.977433	549453.851975	44.985409
3511.146169	549245.071776	44.990413
3511.111022	549016.213635	44.995418
3511.171039	548802.758035	45.000423
3510.544074	548584.023431	45.005428
3511.323033	548370.589536	45.010433
3511.087622	548159.341628	45.015437
3511.187098	547948.234898	45.020442
3511.263781	547734.709383	45.025447
3511.061974	547518.657414	45.030452
3511.081911	547288.097585	45.035457
3511.277416	547080.943207	45.040461
3511.025821	546863.478031	45.045466
3511.134842	546652.299333	45.050471
3511.178851	546445.766159	45.055476
3511.247972	546211.651231	45.060481
3510.656994	546001.842331	45.065485
3510.728573	545796.706233	45.070490
3510.749509	545591.122021	45.075495
3510.457464	545388.512156	45.080500
3510.680469	545180.568328	45.085505
3510.371171	544969.435300	45.090509
3510.546026	544762.501709	45.095514
3510.671814	544569.084961	45.100519
3510.539154	544375.810476	45.105524
3510.567937	544162.590758	45.110529
3510.445046	543968.250159	45.115533
3510.327400	543765.637210	45.120538
3510.533997	543570.781027	45.125543
3510.286672	543369.092001	45.130548
3510.545670	543167.111921	45.135553
3510.184023	542980.361485	45.140557
3510.324359	542773.404185	45.145562
3510.251361	542579.993727	45.150567
3510.419825	542386.993182	45.155572
3510.076765	542190.396296	45.160577
3510.301251	542000.809745	45.165581
3510.380138	541798.336373	45.170586
3510.203316	541597.416544	45.175591
3509.802514	541401.322705	45.180596
3510.194459	541213.411453	45.185601
3509.664035	541026.008174	45.190605
3510.055771	540845.605960	45.195610
3510.098231	540658.755555	45.200615
3509.763679	540470.201953	45.205620
3510.110749	540272.451739	45.210625
3510.003519	540090.359929	45.215629
3510.088055	539907.123499	45.220634
3509.997437	539722.754619	45.225639
3510.024461	539528.225938	45.230644
3510.266737	539337.843938	45.235649
3509.747865	539155.507740	45.240653
3510.004378	538962.848654	45.245658
3509.885574	538788.811863	45.250663
3509.607151	538597.298315	45.255668
3509.753273	538411.661420	45.260673
3509.957573	538238.268841	45.265677
3509.635632	538049.579909	45.270682
3509.652711	537873.390219	45.275687
3509.502543	537685.070639	45.280692
3510.033506	537508.889577	45.285697
3509.994970	537330.634557	45.290701
3509.688620	537137.945931	45.295706
3509.790910	536966.724315	45.300711
3509.341355	536783.034279	45.305716
3509.722636	536598.846909	45.310721
3509.349245	536425.984898	45.315725
3509.518032	536250.152803	45.320730
3509.596404	536078.218373	45.325735
3509.613988	535907.805674	45.330740
3509.581956	535721.659688	45.335745
3509.791823	535547.678523	45.340749
3509.630243	535365.535461	45.345754
3509.594321	535193.458583	45.350759
3509.677819	535019.643941	45.355764
3509.303516	534836.067420	45.360769
3509.098075	534671.984492	45.365773
3509.445537	534485.404522	45.370778
3509.796865	534319.456686	45.375783
3509.286900	534143.916488	45.380788
3509.109120	533965.391099	45.385793
3508.813226	533811.808251	45.390797
3508.883526	533642.621060	45.395802
3509.466842	533479.651265	45.400807
3509.010667	533312.215133	45.405812
3509.172105	533145.882576	45.410817
3508.798628	532974.795519	45.415821
3509.022280	532818.186869	45.420826
3509.014394	532652.684885	45.425831
3508.834049	532494.072906	45.430836
3508.832096	532327.102876	45.435841
3508.916774	532173.084435	45.440845
3508.813601	532009.054726	45.445850
3509.197498	531846.403385	45.450855
3509.163948	531681.853482	45.455860
3508.996482	531521.714826	45.460865
3508.752618	531364.514311	45.465869
3508.804391	531195.604516	45.470874
3508.930892	531037.731675	45.475879
3508.626322	530884.220231	45.480884
3508.829173	530716.288386	45.485889
3508.747371	530573.181957	45.490893
3508.918053	530410.500535	45.495898
3508.947037	530257.480682	45.500903
3508.760567	530107.170790	45.505908
3508.717688	529940.735548	45.510913
3508.753358	529791.646188	45.515917
3508.576481	529629.419175	45.520922
3508.872843	529481.998105	45.525927
3508.443451	529332.529253	45.530932
3508.907341	529171.298113	45.535937
3508.688971	529027.140012	45.540941
3508.601893	528864.889216	45.545946
3509.046201	528715.668688	45.550951
3508.742941	528563.444975	45.555956
3508.816017	528396.921963	45.560961
3508.579636	528238.525725	45.565965
3508.327576	528091.133878	45.570970
3508.708744	527949.941799	45.575975
3508.445404	527806.233695	45.580980
3508.506991	527641.420275	45.585985
3508.662315	527502.988183	45.590989
3508.473282	527350.681973	45.595994
3508.530438	527193.890146	45.600999
3508.650325	527044.405251	45.606004
3508.494265	526901.326246	45.611009
3508.437593	526758.733679	45.616013
3508.559248	526606.568682	45.621018
3508.618698	526451.535389	45.626023
3508.506830	526298.397505	45.631028
3508.294158	526155.421930	45.636033
3508.171002	526009.905623	45.641037
3508.135815	525870.077332	45.646042
3508.690207	525726.057986	45.651047
3508.298104	525584.521065	45.656052
3508.429530	525431.938513	45.661057
3508.596265	525304.337900	45.666061
3508.521369	525149.465426	45.671066
3508.497666	525000.085457	45.676071
3508.277636	524855.180227	45.681076
3508.573672	524703.016483	45.686081
3508.146065	524574.400418	45.691085
3507.910421	524419.800253	45.696090
3507.791419	524285.323021	45.701095
3507.793176	524156.882491	45.706100
3507.865267	524013.433857	45.711105
3508.036434	523889.253606	45.716109
3508.029368	523743.442938	45.721114
3507.893803	523601.035597	45.726119
3507.904553	523476.626871	45.731124
3507.869995	523330.614926	45.736129
3507.950257	523202.253798	45.741133
3507.642623	523072.695520	45.746138
3507.934252	522948.133479	45.751143
3507.625687	522819.330553	45.756148
3508.202838	522676.136360	45.761153
3507.937284	522551.161242	45.766157
3507.983082	522409.620527	45.771162
3508.113332	522278.112382	45.776167
3507.987838	522142.354725	45.781172
3508.112372	522006.755137	45.786177
3508.167762	521881.416701	45.791181
3508.175784	521736.290950	45.796186
3508.298498	521598.870162	45.801191
3508.193611	521464.264308	45.806196
3508.222940	521317.918983	45.811201
3508.118326	521194.016093	45.816205
3508.233310	521048.360507	45.821210
3508.089138	520909.514584	45.826215
3508.045873	520786.506863	45.831220
3508.289289	520645.723886	45.836225
3507.925048	520505.800855	45.841229
3507.835200	520375.222759	45.846234
3508.228932	520245.065984	45.851239
3507.916257	520107.453516	45.856244
3507.637280	519973.066161	45.861249
3507.199682	519850.774715	45.866253
3507.486769	519716.086433	45.871258
3507.640142	519592.378943	45.876263
3507.276922	519478.707819	45.881268
3507.716453	519359.595892	45.886273
3507.548451	519227.102152	45.891277
3507.524374	519103.471500	45.896282
3507.725280	518975.104468	45.901287
3507.568460	518852.807584	45.906292
3507.762341	518713.176836	45.911297
3507.451840	518605.954966	45.916301
3507.498723	518477.812083	45.921306
3507.695766	518354.642691	45.926311
3507.488722	518240.430618	45.931316
3507.390980	518112.006325	45.936321
3507.442647	517996.233023	45.941325
3507.526100	517871.866950	45.946330
3507.375904	517752.287615	45.951335
3507.522854	517637.657049	45.956340
3507.485778	517504.620955	45.961345
3507.382561	517395.284322	45.966349
3506.979129	517268.319451	45.971354
3507.078639	517150.359649	45.976359
3506.816010	517038.623167	45.981364
3507.387438	516927.299097	45.986369
3507.192989	516824.742563	45.991373
3507.132413	516696.249583	45.996378
3506.954866	516581.818098	46.001383
3506.792436	516470.969624	46.006388
3507.305348	516350.862077	46.011393
3507.348494	516246.038527	46.016397
3507.150591	516133.021582	46.021402
3507.213524	516011.624341	46.026407
3506.928846	515902.560678	46.031412
3507.026373	515789.894904	46.036417
3506.921929	515683.072117	46.041421
3507.168142	515573.359815	46.046426
3506.953377	515459.734636	46.051431
3506.797225	515349.836868	46.056436
3506.928428	515242.061501	46.061441
3506.962297	515137.888756	46.066445
3506.823437	515025.661928	46.071450
3507.089673	514917.002444	46.076455
3506.811973	514808.485590	46.081460
3506.786416	514700.834269	46.086465
3506.525891	514607.822418	46.091469
3506.883576	514493.031515	46.096474
3506.743426	514386.357457	46.101479
3506.848991	514281.459450	46.106484
3506.989584	514177.767253	46.111489
3506.931475	514063.195737	46.116493
3506.753709	513967.084138	46.121498
3506.711218	513854.680844	46.126503
3506.404717	513758.741505	46.131508
3506.645503	513651.037453	46.136513
3506.483024	513551.384111	46.141517
3506.798272	513444.322715	46.146522
3507.074157	513342.622794	46.151527
3506.958704	513252.154777	46.156532
3507.242856	513139.892662	46.161537
3506.939637	513040.613762	46.166541
3506.909485	512928.807993	46.171546
3506.589723	512826.802221	46.176551
3506.547990	512718.483159	46.181556
3507.033263	512613.104915	46.186561
3506.646650	512514.948487	46.191565
3506.913191	512413.345180	46.196570
3506.748610	512307.722156	46.201575
3506.904154	512209.824938	46.206580
3507.251460	512104.871057	46.211585
3506.932802	512001.849182	46.216589
3506.548791	511894.846069	46.221594
3506.773620	511790.719452	46.226599
3506.684409	511693.517677	46.231604
3506.761352	511586.534820	46.236609
3506.459189	511487.296438	46.241613
3506.629626	511390.048457	46.246618
3506.536920	511285.063178	46.251623
3506.174948	511194.372739	46.256628
3506.721206	511089.125467	46.261633
3506.405138	511004.742435	46.266637
3506.468134	510904.831666	46.271642
3506.602291	510809.253831	46.276647
3506.245288	510717.902894	46.281652
3506.397762	510626.616035	46.286657
3506.650803	510539.253011	46.291661
3506.401920	510435.147796	46.296666
3506.481125	510345.337275	46.301671
3506.129114	510245.442662	46.306676
3506.260396	510151.933214	46.311681
3506.431473	510058.618556	46.316685
3506.498730	509967.291911	46.321690
3506.478241	509871.583214	46.326695
3506.500447	509783.446881	46.331700
3506.400316	509693.309539	46.336705
3506.351994	509600.534997	46.341709
3506.436898	509510.263952	46.346714
3506.430687	509404.038561	46.351719
3506.329131	509324.562476	46.356724
3506.250190	509228.152370	46.361729
3506.354192	509136.410378	46.366733
3506.300949	509052.073136	46.371738
3506.303930	508959.387164	46.376743
3506.180001	508872.938467	46.381748
3506.556562	508781.855423	46.386753
3506.378263	508689.502060	46.391757
3506.373681	508600.100280	46.396762
3506.474590	508499.965735	46.401767
3506.125988	508417.798199	46.406772
3506.271531	508320.990496	46.411777
3505.919817	508236.346120	46.416781
3506.043132	508160.464693	46.421786
3506.036622	508072.677566	46.426791
3506.048835	507991.507574	46.431796
3506.249135	507899.691482	46.436801
3506.070382	507815.874538	46.441805
3505.792288	507730.204086	46.446810
3506.137858	507643.567481	46.451815
3505.911791	507559.504563	46.456820
3506.155053	507474.855648	46.461825
3506.062303	507395.772783	46.466829
3505.880039	507314.986360	46.471834
3506.155865	507228.409961	46.476839
3505.786377	507138.000904	46.481844
3506.131556	507054.899210	46.486849
3505.931037	506982.807710	46.491853
3505.740916	506898.886819	46.496858
3506.036471	506816.095626	46.501863
3505.828997	506738.848702	46.506868
3505.809172	506657.829055	46.511873
3505.703994	506577.632293	46.516877
3506.105893	506503.413982	46.521882
3506.034380	506424.524884	46.526887
3505.860597	506351.162345	46.531892
3506.178099	506258.659753	46.536897
3505.769545	506185.589274	46.541901
3505.683197	506094.519442	46.546906
3505.777586	506017.015322	46.551911
3505.827687	505942.854494	46.556916
3505.940396	505857.865522	46.561921
3505.931530	505787.707282	46.566925
3505.851188	505714.022601	46.571930
3506.108717	505649.934551	46.576935
3505.749231	505569.877284	46.581940
3506.207042	505481.895615	46.586945
3505.946852	505407.684209	46.591949
3505.678268	505326.245398	46.596954
3506.016295	505238.282854	46.601959
3505.893096	505177.543634	46.606964
3506.091234	505089.654716	46.611969
3506.174077	505005.121303	46.616973
3506.193656	504918.677342	46.621978
3506.023952	504838.482945	46.626983
3505.644368	504752.257900	46.631988
3505.697329	504672.782925	46.636993
3505.812898	504608.310578	46.641997
3505.729174	504524.055849	46.647002
3506.042714	504446.708986	46.652007
3505.655418	504379.035727	46.657012
3505.768895	504294.190061	46.662017
3505.750672	504223.824426	46.667021
3505.819779	504147.023393	46.672026
3505.619055	504080.479743	46.677031
3505.522140	504009.671640	46.682036
3505.226632	503929.140352	46.687041
3505.332691	503869.267042	46.692045
3504.946062	503801.894582	46.697050
3505.488923	503730.217719	46.702055
3505.438969	503666.730419	46.707060
3505.325888	503600.473163	46.712065
3505.345296	503532.271942	46.717069
3505.211583	503474.713073	46.722074
3505.622127	503403.411247	46.727079
3505.281875	503334.107843	46.732084
3505.706750	503266.594607	46.737089
3505.492118	503194.640281	46.742093
3505.470569	503126.697134	46.747098
3505.535024	503062.176827	46.752103
3505.618839	502997.096841	46.757108
3505.655897	502918.829354	46.762113
3505.455119	502849.752857	46.767117
3505.560128	502786.892907	46.772122
3505.637497	502713.268781	46.777127
3505.225058	502645.440928	46.782132
3505.632045	502570.698177	46.787137
3505.709173	502509.864221	46.792141
3505.847127	502435.015113	46.797146
3505.655951	502359.564602	46.802151
3505.500318	502294.674376	46.807156
3505.747727	502220.412297	46.812161
3505.481422	502162.011940	46.817165
3505.578937	502081.404417	46.822170
3505.391721	502008.782917	46.827175
3505.566052	501943.885521	46.832180
3505.612696	501874.307621	46.837185
3505.506902	501804.856573	46.842189
3505.061611	501747.243694	46.847194
3505.331029	501679.851574	46.852199
3505.192199	501619.910710	46.857204
3505.382221	501544.644160	46.862209
3505.355182	501486.655588	46.867213
3505.479395	501420.854584	46.872218
3505.623582	501349.639851	46.877223
3505.388102	501293.253584	46.882228
3505.361654	501218.022498	46.887233
3505.590845	501151.090133	46.892237
3505.705207	501092.368160	46.897242
3505.793305	501023.740257	46.902247
3505.595771	500959.559773	46.907252
3505.365530	500890.985670	46.912257
3505.365971	500822.422457	46.917261
3505.446659	500760.772401	46.922266
3505.561578	500679.952776	46.927271
3505.309965	500628.067119	46.932276
3505.758746	500547.543785	46.937281
3505.741319	500485.454378	46.942285
3505.415067	500432.872956	46.947290
3505.786563	500358.277892	46.952295
3505.309493	500298.137140	46.957300
3505.516595	500224.783090	46.962305
3505.262705	500164.249789	46.967309
3505.109749	500100.210041	46.972314
3505.378180	500026.136725	46.977319
3505.243732	499977.869721	46.982324
3505.653440	499909.789055	46.987329
3505.713319	499850.566305	46.992333
3505.733377	499780.073906	46.997338
3505.783953	499708.463538	47.002343
3505.866481	499638.465533	47.007348
3505.526083	499553.369413	47.012353
3505.669244	499492.209622	47.017357
3505.401923	499418.022792	47.022362
3505.685897	499348.191433	47.027367
3505.330499	499289.745525	47.032372
3505.399842	499221.416739	47.037377
3505.568338	499169.606472	47.042381
3505.227348	499117.124512	47.047386
3505.485526	499046.487198	47.052391
3505.472488	498993.443168	47.057396
3505.438377	498918.051204	47.062401
3505.579920	498859.670637	47.067405
3505.206646	498791.365083	47.072410
3505.415554	498724.426355	47.077415
3505.375882	498668.250536	47.082420
3505.473174	498597.790492	47.087425
3505.964310	498531.561345	47.092429
3505.513959	498462.003349	47.097434
3505.742413	498388.991519	47.102439
3505.759831	498324.460683	47.107444
3505.808368	498252.996092	47.112449
3505.712262	498189.141534	47.117453
3505.526766	498117.514036	47.122458
3505.748324	498046.777585	47.127463
3505.225676	497991.288800	47.132468
3505.493237	497934.552330	47.137473
3505.745426	497863.506442	47.142477
3505.360589	497794.086182	47.147482
3506.000123	497728.941096	47.152487
3505.549617	497666.813934	47.157492
3505.492963	497592.228973	47.162497
3505.509668	497527.796318	47.167501
3505.402330	497462.322559	47.172506
3505.508260	497396.104102	47.177511
3505.229486	497337.638245	47.182516
3505.206673	497284.691587	47.187521
3505.958945	497216.136817	47.192525
3505.335269	497149.586793	47.197530
3505.722289	497080.891537	47.202535
3505.268496	497028.978567	47.207540
3505.194039	496961.423678	47.212545
3505.286195	496902.994116	47.217549
3505.021857	496842.602219	47.222554
3505.430151	496772.081363	47.227559
3505.267354	496719.359118	47.232564
3505.131733	496666.986095	47.237569
3505.088063	496611.309787	47.242573
3504.893563	496552.675070	47.247578
3505.405024	496489.974675	47.252583
3505.166838	496438.023058	47.257588
3505.319318	496367.645332	47.262593
3505.311131	496320.003653	47.267597
3504.910917	496262.768614	47.272602
3505.392473	496196.987049	47.277607
3505.110225	496145.750127	47.282612
3505.012354	496080.319923	47.287617
3505.190767	496023.946242	47.292621
3505.089396	495971.666355	47.297626
3504.873956	495905.850924	47.302631
3504.843813	495865.646647	47.307636
3505.238578	495804.177491	47.312641
3505.319568	495744.683663	47.317645
3504.982845	495695.224909	47.322650
3505.306295	495632.603998	47.327655
3505.025977	495580.404027	47.332660
3504.887234	495533.743409	47.337665
3505.025900	495473.834143	47.342669
3505.246574	495410.319530	47.347674
3505.244170	495356.857510	47.352679
3505.092451	495313.182686	47.357684
3505.156642	495253.639412	47.362689
3505.123992	495204.481356	47.367693
3504.950654	495148.114221	47.372698
3505.163116	495082.981214	47.377703
3505.213230	495032.341695	47.382708
3505.428300	494971.760055	47.387713
3505.194144	494912.721744	47.392717
3505.238380	494853.332207	47.397722
3505.281497	494795.965899	47.402727
3504.928482	494744.382724	47.407732
3504.868525	494685.920853	47.412737
3505.188905	494641.354377	47.417741
3504.665224	494586.461471	47.422746
3504.929391	494528.651859	47.427751
3505.043303	494487.610388	47.432756
3505.303451	494425.754542	47.437761
3505.236816	494364.004849	47.442765
3504.990915	494312.300901	47.447770
3505.354086	494251.944309	47.452775
3505.040084	494196.508507	47.457780
3505.345002	494135.807366	47.462785
3505.306053	494080.172471	47.467789
3504.954713	494038.804684	47.472794
3505.168002	493975.033023	47.477799
3504.994039	493918.307808	47.482804
3504.926634	493854.128365	47.487809
3505.301671	493808.488104	47.492813
3504.544249	493761.827057	47.497818
3504.880738	493702.332998	47.502823
3505.033768	493660.220571	47.507828
3504.885980	493609.610587	47.512833
3504.729060	493554.854051	47.517837
3504.966965	493510.349271	47.522842
3505.211009	493453.601716	47.527847
3504.920070	493406.708287	47.532852
3504.985743	493351.457821	47.537857
3504.954672	493302.850414	47.542861
3505.378358	493242.024629	47.547866
3504.987186	493184.828192	47.552871
3504.448040	493134.081268	47.557876
3505.002208	493092.000115	47.562881
3505.152752	493035.671821	47.567885
3504.874639	492995.503061	47.572890
3504.821462	492936.578722	47.577895
3504.635260	492899.378658	47.582900
3505.059077	492843.256003	47.587905
3504.971592	492795.769693	47.592909
3504.810623	492745.513497	47.597914
3505.066788	492692.960083	47.602919
3504.830698	492651.569237	47.607924
3504.570608	492595.866065	47.612929
3504.694496	492551.479423	47.617933
3504.842033	492504.609816	47.622938
3505.046803	492455.706782	47.627943
3504.861791	492411.473696	47.632948
3504.699285	492364.201346	47.637953
3504.791219	492314.608936	47.642957
3504.579197	492261.274127	47.647962
3504.999770	492220.528945	47.652967
3504.787391	492178.525836	47.657972
3504.902062	492121.947705	47.662977
3505.004363	492070.379840	47.667981
3505.089517	492022.558366	47.672986
3505.123660	491964.728729	47.677991
3505.063887	491921.029474	47.682996
3505.024532	491864.375610	47.688001
3505.062474	491816.156901	47.693005
3504.840371	491768.943670	47.698010
3505.053694	491710.677859	47.703015
3504.910330	491667.751085	47.708020
3505.093419	491614.751520	47.713025
3504.890644	491562.121219	47.718029
3504.712465	491515.709242	47.723034
3504.926765	491462.501513	47.728039
3504.994520	491424.040687	47.733044
3504.894531	491378.171490	47.738049
3505.089391	491329.570480	47.743053
3505.077300	491276.400828	47.748058
3505.233802	491216.928842	47.753063
3505.103098	491167.573492	47.758068
3505.040114	491117.295778	47.763073
3504.876010	491067.541106	47.768077
3505.003748	491019.608377	47.773082
3505.129716	490965.857675	47.778087
3504.677717	490915.494014	47.783092
3504.830132	490861.232542	47.788097
3505.177343	490812.300498	47.793101
3505.235582	490762.102233	47.798106
3505.335305	490707.899867	47.803111
3505.018735	490649.822118	47.808116
3504.934951	490599.344066	47.813121
3505.303156	490548.029786	47.818125
3505.009636	490501.128821	47.823130
3505.101811	490445.611476	47.828135
3505.378788	490408.276317	47.833140
3505.108708	490335.669030	47.838145
3505.113505	490286.338607	47.843149
3504.940000	490238.404543	47.848154
3505.344494	490178.532462	47.853159
3505.209256	490138.990334	47.858164
3505.195804	490090.826152	47.863169
3505.386369	490041.210333	47.868173
3505.334810	489986.373789	47.873178
3504.903104	489921.938217	47.878183
3505.107893	489877.581443	47.883188
3505.220195	489825.246196	47.888193
3505.085881	489765.667064	47.893197
3504.797785	489729.185860	47.898202
3505.244513	489669.405995	47.903207
3504.838243	489626.266030	47.908212
3504.835487	489572.684751	47.913217
3505.020665	489516.844958	47.918221
3504.821190	489466.737521	47.923226
3505.367666	489421.916462	47.928231
3505.196907	489368.515027	47.933236
3505.248431	489312.140824	47.938241
3505.336265	489263.855847	47.943245
3505.240645	489209.732726	47.948250
3505.385087	489153.493935	47.953255
3505.124852	489098.993792	47.958260
3505.257791	489042.200025	47.963265
3505.192319	488988.172260	47.968269
3504.586670	488949.922090	47.973274
3504.986915	488898.445647	47.978279
3504.587443	488849.584938	47.983284
3504.516092	488809.371075	47.988289
3504.801196	488765.604925	47.993293
3504.432522	488728.932972	47.998298
3504.907624	488668.335224	48.003303
3504.644154	488635.085861	48.008308
3504.908034	488580.646396	48.013313
3505.088250	488537.555375	48.018317
3505.020090	488487.928681	48.023322
3504.970361	488432.935102	48.028327
3504.420548	488393.459769	48.033332
3504.907947	488338.424780	48.038337
3504.994138	488298.840638	48.043341
3504.884431	488256.253825	48.048346
3505.034632	488192.269060	48.053351
3505.095640	488152.587684	48.058356
3505.017709	488092.588365	48.063361
3504.852203	488038.422921	48.068365
3504.671301	488006.929295	48.073370
3505.343299	487944.878576	48.078375
3505.129578	487908.836250	48.083380
3504.916716	487848.606121	48.088385
3505.058480	487802.635550	48.093389
3504.847116	487754.195055	48.098394
3505.172065	487705.966466	48.103399
3504.883444	487660.473821	48.108404
3505.070360	487615.405887	48.113409
3505.384872	487569.911231	48.118413
3505.139806	487517.933659	48.123418
3505.569217	487454.961168	48.128423
3504.836109	487412.681144	48.133428
3504.495767	487357.278361	48.138433
3504.949469	487310.139963	48.143437
3504.845876	487266.790637	48.148442
3504.616447	487219.566221	48.153447
3504.519027	487173.078192	48.158452
3504.975917	487129.936451	48.163457
3504.918152	487080.253367	48.168461
3504.579300	487038.613573	48.173466
3504.967334	486990.271029	48.178471
3504.941661	486948.526942	48.183476
3504.710984	486902.212758	48.188481
3505.077439	486844.714095	48.193485
3504.763134	486804.790108	48.198490
3504.920168	486755.626078	48.203495
3504.548144	486710.954875	48.208500
3504.633156	486667.926097	48.213505
3504.908486	486623.599586	48.218509
3504.729786	486590.078817	48.223514
3504.621620	486536.658000	48.228519
3505.007896	486496.208845	48.233524
3504.912651	486441.520393	48.238529
3505.034351	486394.233795	48.243533
3504.706767	486362.661035	48.248538
3504.900739	486309.187937	48.253543
3504.879064	486272.502168	48.258548
3505.011649	486218.533214	48.263553
3505.089609	486166.243436	48.268557
3504.692573	486124.813826	48.273562
3504.923369	486078.975344	48.278567
3504.605231	486035.052318	48.283572
3504.695867	485992.982455	48.288577
3504.895980	485940.013255	48.293581
3504.720191	485901.429951	48.298586
3504.909415	485860.709335	48.303591
3504.785958	485812.147235	48.308596
3504.663514	485763.686042	48.313601
3505.040041	485720.352128	48.318605
3504.564793	485672.203961	48.323610
3504.939148	485623.657558	48.328615
3504.610801	485584.087444	48.333620
3504.715770	485532.398467	48.338625
3504.872366	485485.204680	48.343629
3504.919064	485454.780983	48.348634
3504.753160	485406.123792	48.353639
3504.706327	485367.669124	48.358644
3504.596057	485318.091231	48.363649
3504.521876	485273.011248	48.368653
3504.593125	485238.736693	48.373658
3504.823520	485202.005651	48.378663
3504.285284	485147.287589	48.383668
3504.636473	485121.416788	48.388673
3504.886295	485079.773048	48.393677
3504.618265	485042.974949	48.398682
3504.851445	484995.159457	48.403687
3504.689084	484953.231526	48.408692
3504.369086	484914.417630	48.413697
3504.870842	484872.932827	48.418701
3504.742899	484830.188963	48.423706
3504.756138	484785.396469	48.428711
3504.747220	484743.441841	48.433716
3504.696162	484698.963770	48.438721
3504.811147	484650.408364	48.443725
3504.415078	484617.325834	48.448730
3504.616973	484563.289362	48.453735
3504.175132	484531.226708	48.458740
3504.494221	484491.543593	48.463745
3504.779468	484458.344434	48.468749
3504.583364	484427.656754	48.473754
3504.938716	484382.399933	48.478759
3504.982990	484327.529256	48.483764
3505.006518	484291.995716	48.488769
3505.193958	484237.302762	48.493773
3504.837993	484192.824866	48.498778
3504.904779	484142.099971	48.503783
3505.163950	484103.944589	48.508788
3504.996236	484052.146001	48.513793
3505.169625	483999.124927	48.518797
3504.491584	483955.814908	48.523802
3504.834718	483906.509927	48.528807
3504.984820	483868.828180	48.533812
3504.634550	483824.550839	48.538817
3504.697328	483787.744254	48.543821
3504.607868	483744.889970	48.548826
3504.727455	483699.823503	48.553831
3504.384307	483659.796077	48.558836
3504.398609	483627.451445	48.563841
3504.241015	483577.977979	48.568845
3504.199589	483545.389642	48.573850
3504.515170	483503.174213	48.578855
3504.844754	483466.878164	48.583860
3504.314585	483434.271844	48.588865
3504.531062	483395.413629	48.593869
3504.229212	483364.742162	48.598874
3504.485664	483321.878409	48.603879
3504.523100	483275.407681	48.608884
3504.520910	483249.088339	48.613889
3504.613520	483196.179889	48.618893
3504.458438	483173.632055	48.623898
3504.513881	483128.322015	48.628903
3504.600999	483094.850445	48.633908
3504.485885	483053.922257	48.638913
3504.238729	483008.714195	48.643917
3504.607841	482992.302343	48.648922
3504.732962	482937.869106	48.653927
3504.510669	482902.071061	48.658932
3504.444837	482858.400750	48.663937
3504.543572	482822.041571	48.668941
3504.500194	482792.084225	48.673946
3504.352841	482755.210150	48.678951
3504.580224	482708.654894	48.683956
3504.354191	482670.022500	48.688961
3504.395889	482640.961472	48.693965
3504.299618	482612.025187	48.698970
3504.531196	482566.633028	48.703975
3504.485823	482521.389276	48.708980
3504.421554	482489.410310	48.713985
3504.599314	482463.767721	48.718989
3504.478273	482427.242794	48.723994
3504.459228	482398.343594	48.728999
3504.726529	482349.502806	48.734004
3504.302310	482316.572639	48.739009
3504.415953	482276.261634	48.744013
3504.232525	482252.198942	48.749018
3504.465075	482212.525520	48.754023
3504.550292	482173.433964	48.759028
3504.432508	482152.245152	48.764033
3504.394593	482102.240969	48.769037
3504.512864	482078.784566	48.774042
3504.362628	482041.048997	48.779047
3504.176529	482000.434220	48.784052
3504.110579	481965.771824	48.789057
3504.197900	481927.742361	48.794061
3504.116206	481894.702314	48.799066
3504.208290	481869.073501	48.804071
3504.582556	481834.386306	48.809076
3504.124611	481796.652141	48.814081
3504.461094	481765.919548	48.819085
3504.343389	481737.744792	48.824090
3504.362918	481710.558946	48.829095
3504.394978	481667.982632	48.834100
3504.317798	481627.449650	48.839105
3504.545180	481597.241591	48.844109
3504.259235	481567.323608	48.849114
3504.705342	481526.447950	48.854119
3504.350926	481478.976436	48.859124
3504.495238	481444.833950	48.864129
3504.460978	481414.467778	48.869133
3504.359349	481376.975609	48.874138
3504.537199	481341.713556	48.879143
3504.467837	481301.431602	48.884148
3504.114597	481270.815928	48.889153
3504.359728	481243.793335	48.894157
3504.277607	481213.688098	48.899162
3504.315099	481182.499350	48.904167
3504.406165	481150.238364	48.909172
3504.090819	481112.883375	48.914177
3504.452536	481086.093744	48.919181
3504.058883	481057.205719	48.924186
3504.449570	481017.907622	48.929191
3504.297165	481006.999470	48.934196
3504.585398	480958.809395	48.939201
3504.570341	480933.349403	48.944205
3504.231723	480891.695103	48.949210
3504.275181	480858.986128	48.954215
3504.341981	480829.816631	48.959220
3504.544648	480783.108725	48.964225
3504.347175	480755.806619	48.969229
3504.065290	480720.065002	48.974234
3504.487223	480676.255460	48.979239
3504.450587	480654.392932	48.984244
3504.583926	480616.605945	48.989249
3504.722998	480581.247777	48.994253
3504.413165	480539.790236	48.999258
3504.351815	480509.275290	49.004263
3504.452493	480477.163323	49.009268
3504.255296	480439.634892	49.014273
3504.381080	480413.947626	49.019277
3504.446172	480376.576772	49.024282
3504.536102	480342.441478	49.029287
3504.598743	480303.552197	49.034292
3504.544560	480273.946847	49.039297
3504.768318	480229.613202	49.044301
3504.270972	480202.209586	49.049306
3504.307229	480165.045710	49.054311
3504.392633	480117.495499	49.059316
3504.390409	480096.132656	49.064321
3504.424995	480053.653335	49.069325
3504.122562	480029.101739	49.074330
3504.345289	480000.714260	49.079335
3504.366662	479957.983849	49.084340
3504.077283	479936.214228	49.089345
3504.423311	479897.883177	49.094349
3504.177374	479872.410482	49.099354
3504.284735	479842.270597	49.104359
3504.402564	479805.750172	49.109364
3504.220536	479777.279578	49.114369
3504.154876	479745.447833	49.119373
3503.892995	479729.748242	49.124378
3504.166218	479694.162931	49.129383
3504.117076	479673.921347	49.134388
3504.042812	479651.203403	49.139393
3504.278598	479612.181818	49.144397
3504.252732	479579.887361	49.149402
3504.052775	479551.773849	49.154407
3504.173022	479520.416219	49.159412
3503.950224	479488.003346	49.164417
3504.216094	479467.808996	49.169421
3504.165283	479453.693144	49.174426
3504.111992	479406.063492	49.179431
3503.663807	479381.991533	49.184436
3503.907753	479364.281475	49.189441
3504.037786	479335.098765	49.194445
3503.885990	479306.267885	49.199450
3504.114653	479279.346415	49.204455
3504.259244	479262.108858	49.209460
3504.354145	479238.095857	49.214465
3504.365019	479201.136838	49.219469
3504.148630	479172.418026	49.224474
3504.422167	479129.490722	49.229479
3504.304999	479104.754356	49.234484
3503.936069	479076.010810	49.239489
3504.152923	479038.864410	49.244493
3504.033891	479019.241549	49.249498
3503.793891	478995.892931	49.254503
3504.086781	478980.857368	49.259508
3504.116847	478943.590785	49.264513
3504.073257	478910.032483	49.269517
3504.323589	478897.687356	49.274522
3504.401190	478858.691159	49.279527
3504.232285	478820.800142	49.284532
3503.962954	478808.543684	49.289537
3504.335391	478763.219139	49.294541
3504.284256	478735.534596	49.299546
3504.276923	478713.411578	49.304551
3504.278819	478675.997373	49.309556
3503.959623	478647.750933	49.314561
3504.384185	478621.858225	49.319565
3504.321128	478590.985937	49.324570
3504.075175	478562.271206	49.329575
3504.068130	478535.135739	49.334580
3503.816075	478500.954108	49.339585
3504.070197	478463.901425	49.344589
3503.960175	478453.187005	49.349594
3504.161285	478433.356962	49.354599
3504.097538	478400.914986	49.359604
3503.851112	478374.225180	49.364609
3504.070198	478347.101450	49.369613
3504.276099	478340.282059	49.374618
3504.192451	478291.895233	49.379623
3504.292927	478276.436283	49.384628
3504.070807	478248.881451	49.389633
3504.282243	478209.810381	49.394637
3504.103234	478194.095307	49.399642
3504.104344	478169.641245	49.404647
3504.111301	478129.136669	49.409652
3503.855469	478104.928909	49.414657
3504.388932	478082.409009	49.419661
3504.222688	478063.046322	49.424666
3504.250782	478013.728346	49.429671
3504.199572	477995.966094	49.434676
3504.040646	477969.767050	49.439681
3504.395521	477935.683246	49.444685
3504.125759	477911.983906	49.449690
3504.183810	477891.165101	49.454695
3504.049990	477855.696320	49.459700
3504.327949	477826.992232	49.464705
3504.033039	477795.297468	49.469709
3504.143663	477767.077530	49.474714
3504.434916	477738.826706	49.479719
3504.331101	477717.073363	49.484724
3504.051410	477686.185898	49.489729
3504.388371	477664.205340	49.494733
3504.111245	477631.393382	49.499738
3504.309933	477595.614167	49.504743
3504.097629	477575.094317	49.509748
3503.982553	477554.709736	49.514753
3504.243131	477514.413644	49.519757
3504.245013	477495.983636	49.524762
3504.108363	477466.438415	49.529767
3504.482743	477432.552866	49.534772
3504.431577	477408.511759	49.539777
3504.496550	477376.552294	49.544781
3504.161624	477339.446010	49.549786
3504.080620	477313.536507	49.554791
3504.313650	477282.611446	49.559796
3504.086733	477251.866130	49.564801
3504.356320	477231.921827	49.569805
3504.177061	477197.624055	49.574810
3504.196576	477170.785813	49.579815
3504.267440	477150.824720	49.584820
3504.086025	477112.274066	49.589825
3504.399481	477082.094416	49.594829
3504.367515	477060.024229	49.599834
3504.281634	477017.963437	49.604839
3504.232063	476997.718946	49.609844
3504.013582	476973.807101	49.614849
3504.446371	476934.138549	49.619853
3504.200187	476917.218660	49.624858
3504.064057	476886.558493	49.629863
3504.113416	476856.676729	49.634868
3503.870339	476839.300541	49.639873
3504.071206	476821.797904	49.644877
3504.032603	476795.070299	49.649882
3504.292222	476757.861319	49.654887
3504.288357	476748.140432	49.659892
3504.070947	476726.202772	49.664897
3504.205433	476681.116220	49.669901
3504.077278	476668.125347	49.674906
3503.956686	476648.905264	49.679911
3504.360681	476607.418120	49.684916
3503.948194	476590.728858	49.689921
3504.200486	476558.735981	49.694925
3503.954672	476533.410484	49.699930
3504.379754	476502.147512	49.704935
3504.244434	476487.588085	49.709940
3504.146466	476457.629558	49.714945
3504.230892	476411.234409	49.719949
3503.882527	476407.243177	49.724954
3503.898305	476369.720605	49.729959
3503.912689	476335.945132	49.734964
3504.058563	476321.337561	49.739969
3504.176956	476289.518981	49.744973
3503.687284	476282.868226	49.749978
3503.610186	476240.905419	49.754983
3504.053702	476219.310013	49.759988
3503.892033	476205.767553	49.764993
3504.010385	476179.569233	49.769997
3503.966559	476170.563749	49.775002
3503.838035	476139.495956	49.780007
3504.182073	476112.347579	49.785012
3504.360851	476101.177387	49.790017
3504.242565	476059.828818	49.795021
3504.427604	476036.555741	49.800026
3504.126862	476003.238542	49.805031
3503.998222	475968.423474	49.810036
3503.688125	475948.627391	49.815041
3503.969403	475923.717407	49.820045
3504.170510	475919.581613	49.825050
3503.728031	475887.199842	49.830055
3504.181082	475856.386718	49.835060
3503.856341	475837.200642	49.840065
3503.786344	475822.730805	49.845069
3503.654973	475808.727157	49.850074
3503.789155	475784.044643	49.855079
3503.954709	475752.368989	49.860084
3503.626825	475742.196535	49.865089
3503.918451	475723.512730	49.870093
3503.944511	475710.950570	49.875098
3503.820729	475689.046319	49.880103
3503.964377	475655.905793	49.885108
3503.611112	475630.242943	49.890113
3504.246779	475611.753463	49.895117
3503.846458	475607.365836	49.900122
3503.659121	475576.155223	49.905127
3503.684215	475545.769106	49.910132
3504.025346	475530.216112	49.915137
3503.888295	475501.933704	49.920141
3503.802443	475499.062091	49.925146
3503.859941	475483.658760	49.930151
3503.939010	475440.148363	49.935156
3503.797930	475414.702166	49.940161
3503.932342	475401.766837	49.945165
3504.071568	475396.578119	49.950170
3504.355022	475367.717337	49.955175
3504.205351	475351.690989	49.960180
3504.047048	475335.666100	49.965185
3504.402684	475309.577939	49.970189
3504.129948	475283.850219	49.975194
3504.274785	475248.581997	49.980199
3504.104530	475202.277923	49.985204
3503.997564	475187.915174	49.990209
3504.215263	475163.217569	49.995213
3503.823499	475145.865165	50.000218
3503.989118	475114.745418	50.005223
3503.954165	475092.622740	50.010228
3504.050945	475075.895781	50.015233
3503.878052	475055.822120	50.020237
3503.747127	475034.931066	50.025242
3504.021561	475011.236328	50.030247
3503.721830	474990.120857	50.035252
3503.756018	474975.379375	50.040257
3504.394510	474948.685391	50.045261
3503.898193	474928.565539	50.050266
3503.830780	474896.776280	50.055271
3503.899165	474878.281652	50.060276
3503.683504	474878.217212	50.065281
3503.931020	474852.805165	50.070285
3504.150695	474816.611851	50.075290
3504.284630	474802.764693	50.080295
3504.047695	474782.296561	50.085300
3504.030190	474748.776816	50.090305
3503.971867	474722.505315	50.095309
3503.695520	474710.095386	50.100314
3504.043968	474699.148571	50.105319
3503.748229	474668.714513	50.110324
3503.592625	474646.966373	50.115329
3503.553757	474617.045399	50.120333
3503.599991	474603.668817	50.125338
3503.934128	474592.825660	50.130343
3504.294362	474574.483454	50.135348
3504.232981	474552.516559	50.140353
3504.619479	474514.977552	50.145357
3503.799439	474506.711461	50.150362
3504.057680	474477.144645	50.155367
3503.974037	474444.445871	50.160372
3503.656461	474434.676048	50.165377
3503.561822	474410.790362	50.170381
3503.677780	474400.642661	50.175386
3503.819274	474385.477270	50.180391
3503.933521	474345.553704	50.185396
3503.997535	474328.122708	50.190401
3503.716646	474318.346559	50.195405
3503.673545	474295.819200	50.200410
3503.680948	474287.006609	50.205415
3503.842914	474278.420821	50.210420
3504.053306	474239.290848	50.215425
3503.683760	474217.376173	50.220429
3503.576064	474214.254888	50.225434
3503.719520	474190.885306	50.230439
3503.887320	474184.577287	50.235444
3503.752378	474163.888495	50.240449
3503.721932	474125.457727	50.245453
3503.671571	474111.641520	50.250458
3503.674815	474097.360387	50.255463
3503.702566	474085.505800	50.260468
3503.738479	474075.017104	50.265473
3504.307942	474060.386061	50.270477
3504.454537	474029.318380	50.275482
3504.008191	474005.087098	50.280487
3503.866092	473985.108298	50.285492
3504.174920	473958.013413	50.290497
3504.461657	473922.870361	50.295501
3503.815150	473905.053876	50.300506
3503.856443	473897.855823	50.305511
3503.907648	473871.716338	50.310516
3503.592592	473859.109882	50.315521
3503.755939	473838.623001	50.320525
3503.650978	473829.069761	50.325530
3503.543035	473814.554188	50.330535
3503.769517	473804.336649	50.335540
3503.531156	473787.665751	50.340545
3503.534934	473750.342470	50.345549
3503.912957	473733.161148	50.350554
3503.589878	473725.518829	50.355559
3503.778325	473708.521778	50.360564
3503.866433	473704.607352	50.365569
3504.183867	473687.031201	50.370573
3503.967606	473650.606197	50.375578
3503.842864	473636.042712	50.380583
3503.975826	473617.130667	50.385588
3503.690765	473615.963951	50.390593
3503.901100	473574.958845	50.395597
3503.898291	473551.866643	50.400602
3503.513662	473539.727626	50.405607
3503.841162	473517.034759	50.410612
3503.709558	473511.233412	50.415617
3503.857718	473497.737346	50.420621
3503.886295	473475.804458	50.425626
3503.777205	473450.603308	50.430631
3503.652415	473439.382060	50.435636
3503.639924	473428.344200	50.440641
3503.492571	473410.442011	50.445645
3503.684534	473409.041905	50.450650
3503.758618	473389.430690	50.455655
3503.727601	473371.154102	50.460660
3503.620628	473336.532948	50.465665
3503.525982	473314.620909	50.470669
3503.597588	473307.265525	50.475674
3503.684305	473294.995225	50.480679
3503.695504	473283.700021	50.485684
3503.319302	473276.775584	50.490689
3503.730634	473257.511788	50.495693
3503.584371	473255.612351	50.500698
3503.699343	473243.033336	50.505703
3503.732189	473205.805285	50.510708
3503.682045	473191.988358	50.515713
3503.568138	473174.738588	50.520717
3503.776885	473169.486736	50.525722
3503.438180	473155.769694	50.530727
3503.653131	473125.752335	50.535732
3503.529044	473098.426260	50.540737
3503.801419	473037.962403	50.545741
3503.509857	472983.874428	50.550746
3503.486421	472915.205798	50.555751
3503.787590	472830.731254	50.560756
3503.439558	472739.277000	50.565761
3503.653250	472642.510017	50.570765
3503.438154	472525.203367	50.575770
3503.284759	472397.452569	50.580775
3503.639363	472261.764124	50.585780
3503.745783	472114.367247	50.590785
3503.639802	471945.835352	50.595789
3503.593099	471781.647436	50.600794
3503.340520	471592.321585	50.605799
3503.621223	471395.001721	50.610804
3503.655692	471177.462505	50.615809
3503.819102	470954.833865	50.620813
3503.580172	470722.597227	50.625818
3503.425830	470474.337820	50.630823
3503.639976	470218.971753	50.635828
3503.472866	469950.497915	50.640833
3503.588990	469645.856746	50.645837
3503.874358	469358.099963	50.650842
3503.663697	469036.282698	50.655847
3503.840240	468706.137113	50.660852
3503.497193	468365.538105	50.665857
3503.596502	468003.986882	50.670861
3503.591591	467644.726211	50.675866
3503.251767	467250.206817	50.680871
3503.610337	466862.652432	50.685876
3503.412807	466456.541976	50.690881
3503.294558	466027.408860	50.695885
3503.209630	465598.463156	50.700890
3503.036043	465146.926784	50.705895
3503.069122	464679.435615	50.710900
3503.218519	464202.438635	50.715905
3503.233405	463700.726906	50.720909
3502.831128	463200.441574	50.725914
3502.632435	462677.104163	50.730919
3502.955981	462135.016262	50.735924
3502.679956	461587.948432	50.740929
3502.497939	461015.157133	50.745933
3502.483940	460431.678476	50.750938
3502.488152	459823.550000	50.755943
3502.723296	459214.349903	50.760948
3502.321302	458579.291208	50.765953
3502.717422	457926.590486	50.770957
3502.635398	457267.361200	50.775962
3502.489859	456570.005111	50.780967
3502.723758	455857.100315	50.785972
3502.022010	455142.049187	50.790977
3502.223722	454400.763153	50.795981
3502.020353	453643.601624	50.800986
3501.848478	452873.378043	50.805991
3501.891750	452080.224400	50.810996
3501.681270	451279.580171	50.816001
3502.161261	450449.785998	50.821005
3501.533292	449606.965122	50.826010
3501.326024	448746.545112	50.831015
3501.632270	447862.575332	50.836020
3501.237897	446972.805917	50.841025
3501.163628	446057.335067	50.846029
3501.150043	445129.034655	50.851034
3501.195840	444173.854997	50.856039
3501.116027	443207.952872	50.861044
3500.913053	442226.964648	50.866049
3501.386006	441207.774421	50.871053
3501.261858	440181.892282	50.876058
3500.811445	439120.457748	50.881063
3500.770114	438053.119300	50.886068
3500.421629	436979.136242	50.891073
3500.518849	435862.712338	50.896077
3500.477200	434737.682272	50.901082
3500.337213	433598.862663	50.906087
3500.264255	432437.597251	50.911092
3499.652526	431263.019207	50.916097
3499.634674	430060.114993	50.921101
3499.446928	428864.892010	50.926106
3499.170840	427623.742217	50.931111
3499.220002	426378.157626	50.936116
3499.091391	425128.985312	50.941121
3498.844337	423850.732777	50.946125
3498.569614	422553.939400	50.951130
3498.607784	421240.372226	50.956135
3498.580129	419910.829969	50.961140
3497.963408	418562.505958	50.966145
3498.055941	417197.968694	50.971149
3497.968563	415818.713642	50.976154
3497.908465	414420.031849	50.981159
3497.470221	412990.589143	50.986164
3496.932457	411566.823567	50.991169
3497.171027	410127.484354	50.996173
3497.308641	408658.726351	51.001178
3497.003833	407173.911999	51.006183
3496.675871	405671.240734	51.011188
3496.565771	404159.457742	51.016193
3496.096490	402631.675485	51.021197
3495.912796	401083.031745	51.026202
3495.644406	399522.834416	51.031207
3495.759529	397948.970122	51.036212
3495.096047	396359.882933	51.041217
3495.142459	394757.121161	51.046221
3495.067724	393134.955809	51.051226
3494.750139	391505.221807	51.056231
3494.562666	389853.217582	51.061236
3494.522715	388192.762921	51.066241
3494.096303	386497.542104	51.071245
3493.715353	384804.051762	51.076250
3493.380900	383088.171333	51.081255
3493.165113	381356.901947	51.086260
3493.033231	379629.898732	51.091265
3493.043718	377865.639146	51.096269
3492.532485	376104.248773	51.101274
3492.614926	374324.461711	51.106279
3492.454659	372520.901842	51.111284
3492.029753	370711.446215	51.116289
3492.294924	368867.579245	51.121293
3491.161050	367030.036957	51.126298
3491.174196	365183.077372	51.131303
3491.355660	363303.978447	51.136308
3490.986331	361427.068390	51.141313
3490.867529	359509.150706	51.146317
3490.535665	357599.366979	51.151322
3490.435880	355671.621505	51.156327
3489.814941	353728.636879	51.161332
3489.135440	351775.065588	51.166337
3489.272255	349803.253507	51.171341
3488.836153	347816.871974	51.176346
3488.243020	345815.188401	51.181351
3488.174293	343810.096134	51.186356
3487.535374	341796.465531	51.191361
3487.453539	339762.908517	51.196365
3487.011874	337728.208896	51.201370
3486.485239	335671.962747	51.206375
3486.333461	333606.866803	51.211380
3486.075090	331551.023443	51.216385
3485.744574	329453.221409	51.221389
3485.246350	327352.391437	51.226394
3484.780202	325258.860902	51.231399
3484.555998	323140.550005	51.236404
3483.728078	321008.701353	51.241409
3483.909906	318879.383189	51.246413
3483.786738	316730.904301	51.251418
3482.732864	314576.202775	51.256423
3482.649421	312405.154327	51.261428
3482.041664	310232.297843	51.266433
3481.648753	308041.724318	51.271437
3481.459868	305840.998474	51.276442
3481.084423	303643.937870	51.281447
3480.945866	301422.541394	51.286452
3480.338171	299199.413856	51.291457
3479.866143	296955.026211	51.296461
3479.261769	294703.405074	51.301466
3478.792368	292456.729908	51.306471
3478.742738	290188.268220	51.311476
3478.534817	287923.127049	51.316481
3478.326857	285638.465281	51.321485
3477.743644	283335.647677	51.326490
3477.532338	281028.988165	51.331495
3476.811105	278695.236328	51.336500
3476.325488	276374.988521	51.341505
3475.746243	274035.579136	51.346509
3474.780857	271692.264710	51.351514
3474.643534	269346.496325	51.356519
3474.532650	266992.378097	51.361524
3473.609508	264623.714746	51.366529
3473.146825	262254.859676	51.371533
3472.546065	259884.874155	51.376538
3472.015632	257504.404483	51.381543
3471.683058	255110.656106	51.386548
3470.894525	252724.755246	51.391553
3470.402048	250318.561893	51.396557
3469.736507	247913.629226	51.401562
3469.179086	245510.523837	51.406567
3468.838467	243089.594986	51.411572
3468.149789	240666.911050	51.416577
3467.783861	238236.376215	51.421581
3467.615044	235807.387485	51.426586
3466.523316	233358.900501	51.431591
3466.578067	230914.911860	51.436596
3465.594441	228466.681314	51.441601
3465.016380	226001.055164	51.446605
3464.519750	223539.789365	51.451610
3463.589643	221074.291927	51.456615
3463.237365	218604.063044	51.461620
3462.602905	216142.061537	51.466625
3461.986518	213665.450275	51.471629
3461.037103	211186.923096	51.476634
3460.672574	208694.895099	51.481639
3460.125651	206217.330383	51.486644
3459.137119	203734.519058	51.491649
3458.680474	201235.530092	51.496653
3457.915716	198745.231895	51.501658
3457.178703	196273.027248	51.506663
3456.401659	193769.099448	51.511668
3455.386175	191267.599449	51.516673
3454.768882	188772.838343	51.521677
3454.387072	186283.472448	51.526682
3453.698396	183790.485767	51.531687
3452.871649	181287.300230	51.536692
3451.772087	178802.727373	51.541697
3451.207076	176299.158031	51.546701
3450.560320	173800.624158	51.551706
3449.414109	171308.841422	51.556711
3449.214670	168809.202325	51.561716
3448.392143	166326.010849	51.566721
3447.394504	163832.605265	51.571725
3446.731943	161352.346950	51.576730
3445.734313	158866.209366	51.581735
3445.397289	156375.375462	51.586740
3444.178563	153897.167745	51.591745
3443.334158	151412.463107	51.596749
3442.956549	148918.911008	51.601754
3441.483092	146388.339901	51.606759
3440.949500	143908.867396	51.611764
3440.088263	141446.910861	51.616769
3439.312585	138978.449283	51.621773
3438.530086	136518.732138	51.626778
3437.610376	134057.360688	51.631783
3436.711127	131598.989285	51.636788
3435.661421	129162.306728	51.641793
3434.891877	126711.872150	51.646797
3433.825529	124280.917738	51.651802
3432.522939	121840.704210	51.656807
3431.770775	119415.331160	51.661812
3431.213761	116998.888420	51.666817
3430.413269	114583.817878	51.671821
3429.067146	112183.663480	51.676826
3427.695939	109787.629441	51.681831
3427.034526	107393.090837	51.686836
3425.666091	105015.822741	51.691841
3424.883524	102634.221067	51.696845
3423.998192	100268.334419	51.701850
3422.633963	97924.034037	51.706855
3421.730153	95582.325690	51.711860
3420.858569	93251.566899	51.716865
3419.561114	90937.147375	51.721869
3418.434106	88617.162102	51.726874
3417.263827	86308.611083	51.731879
3416.395517	84020.735256	51.736884
3415.141754	81751.308394	51.741889
3413.989000	79483.595621	51.746893
3412.872179	77227.744993	51.751898
3411.520983	74988.291739	51.756903
3410.694305	72760.285245	51.761908
3409.057935	70546.057635	51.766913
3407.991421	68348.326082	51.771917
3406.844946	66170.628512	51.776922
3405.423215	64003.411517	51.781927
3404.515052	61847.864284	51.786932
3402.793743	59708.470692	51.791937
3401.373620	57589.904126	51.796941
3399.911584	55489.868648	51.801946
3398.568865	53403.924251	51.806951
3397.018721	51348.745610	51.811956
3395.759855	49305.549894	51.816961
3394.478196	47288.128373	51.821965
3392.980865	45285.914239	51.826970
3391.358035	43310.435034	51.831975
3390.273648	41348.962992	51.836980
3388.695615	39416.665164	51.841985
3387.140872	37508.198839	51.846989
3385.562364	35616.221721	51.851994
3383.533174	33751.017266	51.856999
3381.723616	31918.864873	51.862004
3379.445634	30119.841942	51.867009
3377.406157	28366.383489	51.872013
3375.120073	26634.946099	51.877018
3369.670409	25030.603433	51.882023
3360.813822	23579.645431	51.887028
3353.074802	22232.258751	51.892033
3345.626149	20991.542629	51.897037
3338.995688	19872.838371	51.902042
3332.965568	18868.478731	51.907047
3327.758123	17979.077453	51.912052
3322.550459	17214.526663	51.917057
3318.219418	16543.694227	51.922061
3314.311781	15968.598258	51.927066
3310.886176	15486.785079	51.932071
3308.583233	15071.713314	51.937076
3306.211150	14741.229259	51.942081
3303.962948	14460.842389	51.947085
3302.470046	14230.364875	51.952090
3301.195350	14047.266287	51.957095
3299.879536	13896.478873	51.962100
3298.543607	13786.294488	51.967105
3297.807066	13694.776991	51.972109
3297.147693	13633.092745	51.977114
3296.706060	13607.727971	51.982119
3296.310185	13572.387312	51.987124
3295.751146	13560.879184	51.992129
3295.259718	13560.746655	51.997133
3294.787521	13559.194954	52.002138
3294.558981	13578.169924	52.007143
3294.781152	13597.120070	52.012148
3294.677629	13624.297279	52.017153
3294.729433	13640.166671	52.022157
3294.826911	13650.423166	52.027162
3294.645336	13679.766086	52.032167
3294.617850	13675.218116	52.037172
3294.647523	13677.659275	52.042177
3294.110506	13682.035062	52.047181
3294.350015	13678.302714	52.052186
3293.826274	13683.107640	52.057191
3294.247782	13672.007138	52.062196
3294.027652	13654.107443	52.067201
3293.855798	13625.675138	52.072205
3293.697833	13601.635142	52.077210
3293.382266	13575.068448	52.082215
3293.731410	13530.446327	52.087220
3293.318438	13483.190705	52.092225
3293.181004	13433.588930	52.097229
3292.995410	13380.321534	52.102234
3292.611358	13323.491657	52.107239
3292.296620	13269.255890	52.112244
3291.788793	13201.695879	52.117249
3291.059935	13149.778288	52.122253
3290.672074	13071.334503	52.127258
3289.964896	13008.423477	52.132263
3289.926948	12930.377259	52.137268
3289.290125	12862.290775	52.142273
3288.637583	12780.521519	52.147277
3288.357983	12693.604043	52.152282
3287.713099	12621.108161	52.157287
3287.373551	12540.563382	52.162292
3286.705101	12463.997056	52.167297
3285.919068	12386.890230	52.172301
3285.347993	12312.795080	52.177306
3284.953278	12239.866276	52.182311
3284.501575	12160.020385	52.187316
3283.841673	12084.866972	52.192321
3283.042028	12004.273851	52.197325
3282.996073	11926.298543	52.202330
3282.306970	11835.397927	52.207335
3282.004050	11758.721883	52.212340
3281.018027	11662.165782	52.217345
3280.383283	11574.674971	52.222349
3280.128493	11474.970859	52.227354
3279.045540	11398.121649	52.232359
3278.770878	11305.053325	52.237364
3278.172192	11220.658235	52.242369
3277.596298	11122.927668	52.247373
3277.143732	11031.703545	52.252378
3276.107687	10944.787094	52.257383
3275.531519	10846.505232	52.262388
3275.138945	10758.628243	52.267393
3274.283963	10671.946166	52.272397
3273.911624	10577.870116	52.277402
3273.318518	10488.959212	52.282407
3272.595925	10383.973045	52.287412
3272.075748	10293.153260	52.292417
3271.305018	10207.961759	52.297421
3270.887743	10106.007625	52.302426
3270.013595	10022.637425	52.307431
3269.740406	9916.928159	52.312436
3268.896905	9828.540759	52.317441
3268.225327	9731.390989	52.322445
3267.901750	9636.493674	52.327450
3267.129447	9537.411152	52.332455
3266.073393	9437.862682	52.337460
3265.554586	9349.236001	52.342465
3264.972027	9251.563609	52.347469
3264.312098	9160.589184	52.352474
3263.592660	9075.663424	52.357479
3263.020538	8975.881878	52.362484
3262.232538	8880.727084	52.367489
3261.488922	8792.669497	52.372493
3261.020656	8694.979353	52.377498
3260.213409	8603.568772	52.382503
3259.535559	8509.128772	52.387508
3258.973656	8427.468526	52.392513
3258.291046	8328.509191	52.397517
3257.943824	8225.453833	52.402522
3256.990327	8154.489404	52.407527
3256.656834	8061.610022	52.412532
3255.887417	7973.230358	52.417537
3254.957853	7879.388353	52.422541
3254.650652	7784.825289	52.427546
3254.130135	7699.171403	52.432551
3253.628393	7600.396519	52.437556
3252.595441	7497.921841	52.442561
3252.277279	7412.149610	52.447565
3251.329458	7315.679174	52.452570
3250.475258	7230.273552	52.457575
3249.956039	7128.000957	52.462580
3249.579081	7044.598295	52.467585
3248.779591	6952.275634	52.472589
3248.085603	6850.732048	52.477594
3246.992460	6766.803970	52.482599
3246.052346	6670.762576	52.487604
3245.523329	6587.269007	52.492609
3244.686721	6501.007350	52.497613
3244.295058	6412.192640	52.502618
3243.294602	6337.180108	52.507623
3243.123019	6247.779823	52.512628
3242.391862	6169.333207	52.517633
3241.329094	6089.642905	52.522637
3240.722273	6000.823004	52.527642
3239.946521	5927.040765	52.532647
3239.902691	5842.296208	52.537652
3239.296988	5770.047750	52.542657
3238.457265	5692.138510	52.547661
3237.912457	5593.486786	52.552666
3237.200896	5516.354135	52.557671
3236.474209	5435.739403	52.562676
3235.406077	5348.255225	52.567681
3234.768841	5276.863331	52.572685
3234.190721	5189.581397	52.577690
3233.078435	5118.488539	52.582695
3232.864828	5041.271536	52.587700
3232.126155	4972.976588	52.592705
3231.381786	4897.993405	52.597709
3230.762571	4820.835709	52.602714
3230.052669	4762.750607	52.607719
3229.373296	4680.254526	52.612724
3228.720303	4610.604034	52.617729
3227.830750	4546.659402	52.622733
3227.620477	4473.203445	52.627738
3227.037565	4403.652441	52.632743
3226.593182	4319.803285	52.637748
3225.248190	4252.236484	52.642753
3225.271067	4176.614715	52.647757
3224.959559	4091.602216	52.652762
3223.732510	4027.250648	52.657767
3223.180443	3943.908298	52.662772
3222.598519	3867.992550	52.667777
3221.759560	3785.135930	52.672781
3221.798742	3707.302619	52.677786
3220.782232	3632.686967	52.682791
3219.814173	3552.145921	52.687796
3219.199528	3473.995109	52.692801
3218.246049	3404.624710	52.697805
3217.913656	3331.066981	52.702810
3216.808082	3262.672309	52.707815
3216.178683	3184.074581	52.712820
3215.331589	3122.064567	52.717825
3215.004240	3059.454340	52.722829
3214.624782	2978.984632	52.727834
3213.842486	2924.095984	52.732839
3212.839703	2835.921232	52.737844
3211.935443	2766.673932	52.742849
3211.476866	2706.674213	52.747853
3210.798040	2636.499897	52.752858
3209.777741	2576.519261	52.757863
3209.767348	2503.395174	52.762868
3208.795648	2445.737559	52.767873
3208.079412	2372.284612	52.772877
3207.628896	2309.540488	52.777882
3206.535114	2249.774990	52.782887
3205.967626	2187.600871	52.787892
3205.634848	2129.333101	52.792897
3204.979772	2057.758212	52.797901
3204.682467	1997.245699	52.802906
3203.204292	1939.409602	52.807911
3202.857115	1872.653668	52.812916
3202.346563	1813.539466	52.817921
3201.004240	1747.418329	52.822925
3200.953026	1685.952265	52.827930
3200.399812	1630.535534	52.832935
3199.908646	1565.853546	52.837940
3198.879476	1499.199528	52.842945
3198.546494	1433.439808	52.847949
3197.819249	1370.211019	52.852954
3196.909883	1313.054181	52.857959
3196.555258	1248.802170	52.862964
3195.665353	1183.026931	52.867969
3194.686416	1125.367510	52.872973
3194.305147	1068.247663	52.877978
3193.553060	1007.485068	52.882983
3192.998656	943.150016	52.887988
3192.121623	898.966131	52.892993
3191.023231	832.313751	52.897997
3190.272130	777.248458	52.903002
3189.345312	729.968104	52.908007
3188.686375	681.283426	52.913012
3188.397955	642.227272	52.918017
3187.581518	595.240313	52.923021
3187.102707	539.596834	52.928026
3186.095767	506.510640	52.933031
3185.742923	449.045564	52.938036
3185.109826	408.487700	52.943041
3184.098746	360.180369	52.948045
3183.694058	316.742428	52.953050
3182.748843	277.831764	52.958055
3181.697713	236.451702	52.963060
3180.944569	206.375633	52.968065
3179.947320	179.514555	52.973069
3179.141775	150.626208	52.978074
3177.811271	144.418280	52.983079
3175.905873	158.348538	52.988084
3175.095173	151.961802	52.993089
3174.472035	149.816747	52.998093
3174.229512	155.968986	53.003098
3173.530088	153.556706	53.008103
3173.484860	159.462875	53.013108
3172.888687	160.464330	53.018113
3171.658291	161.350332	53.023117
3171.022473	154.480963	53.028122
3171.276515	162.709505	53.033127
3170.659560	155.123638	53.038132
3169.378790	159.682511	53.043137
3168.728196	162.826773	53.048141
3168.124418	164.129127	53.053146
3167.168773	168.349830	53.058151
3167.062958	157.536961	53.063156
3166.498847	161.641427	53.068161
3165.373297	163.087005	53.073165
3164.769338	160.280265	53.078170
3163.834974	169.593279	53.083175
3163.476466	158.417803	53.088180
3163.505767	155.686814	53.093185
3162.474049	156.581898	53.098189
3162.091666	153.232052	53.103194
3160.539437	153.522528	53.108199
3160.686228	151.028436	53.113204
3159.991510	148.400623	53.118209
3159.262280	159.126052	53.123213
3158.614010	150.977920	53.128218
3157.609345	162.574604	53.133223
3157.216022	156.261819	53.138228
3156.727341	160.990095	53.143233
3155.509063	152.791722	53.148237
3155.016603	147.772431	53.153242
3154.436886	155.370144	53.158247
3154.299222	151.114822	53.163252
3153.341179	147.662808	53.168257
3152.644533	159.075024	53.173261
3152.184702	154.322124	53.178266
3151.441121	160.276951	53.183271
3150.704005	152.854906	53.188276
3150.018956	149.641639	53.193281
3149.459095	160.578127	53.198285
3149.109457	149.361276	53.203290
3148.055882	150.576669	53.208295
3147.355978	153.429362	53.213300
3147.018580	149.741444	53.218305
3146.155246	155.832385	53.223309
3145.901117	148.830312	53.228314
3144.754255	160.585102	53.233319
3144.577651	153.917142	53.238324
3143.978887	145.289647	53.243329
3142.745027	159.517272	53.248333
3141.952590	154.503840	53.253338
3141.335102	157.640078	53.258343
3140.920255	152.708972	53.263348
3140.487546	149.751402	53.268353
3140.018245	155.155693	53.273357
3139.729724	148.790272	53.278362
3138.343027	154.485117	53.283367
3137.485226	154.041572	53.288372
3136.744230	149.157113	53.293377
3136.484014	153.348995	53.298381
3135.703474	144.032970	53.303386
3134.768720	152.515140	53.308391
3134.510626	149.423134	53.313396
3134.335546	151.864850	53.318401
3133.475994	150.353469	53.323405
3132.737519	152.260669	53.328410
3131.417820	151.821439	53.333415
3131.119410	151.172979	53.338420
3131.112960	153.403914	53.343425
3129.944858	156.905013	53.348429
3129.308556	155.858372	53.353434
3128.804293	148.620360	53.358439
3127.751390	147.025177	53.363444
3127.767525	139.473655	53.368449
3126.973898	154.762087	53.373453
3126.405924	135.568388	53.378458
3125.402918	141.473984	53.383463
3124.566654	145.138642	53.388468
3123.961917	135.879033	53.393473
3122.909668	140.825170	53.398477
3123.203532	147.269829	53.403482
3122.449319	150.110487	53.408487
3121.311386	146.912237	53.413492
3120.566923	147.536016	53.418497
3119.506475	152.225801	53.423501
3119.690548	144.676766	53.428506
3118.751950	147.693004	53.433511
3118.390142	146.203554	53.438516
3117.673635	145.863762	53.443521
3116.198798	149.150829	53.448525
3116.416209	144.680899	53.453530
3116.127206	151.315539	53.458535
3115.569039	145.003694	53.463540
3114.573267	142.638901	53.468545
3113.623993	148.020990	53.473549
3112.801534	140.453675	53.478554
3112.309961	147.610808	53.483559
3111.489994	146.212666	53.488564
3110.514854	149.270674	53.493569
3109.644664	151.979180	53.498573
3109.606148	140.407218	53.503578
3108.626642	150.255688	53.508583
3107.915748	151.400694	53.513588
3107.921051	146.087156	53.518593
3107.432240	153.962620	53.523597
3106.854902	148.717448	53.528602
3105.965356	142.498146	53.533607
3105.236955	151.614123	53.538612
3104.453547	142.921083	53.543617
3103.647494	153.396351	53.548621
3103.103828	144.876290	53.553626
3102.212551	141.631560	53.558631
3101.221623	145.222386	53.563636
3100.950586	138.352682	53.568641
3100.734805	154.617225	53.573645
3100.414661	140.708041	53.578650
3099.512259	144.728205	53.583655
3098.587534	139.410948	53.588660
3098.115643	141.557595	53.593665
3096.880110	151.744674	53.598669
3096.066167	145.877578	53.603674
3095.442080	140.171461	53.608679
3094.414340	144.371327	53.613684
3094.824700	141.849570	53.618689
3094.584332	146.673571	53.623693
3093.881824	139.911931	53.628698
3093.214937	147.920053	53.633703
3091.421629	148.629099	53.638708
3091.501511	144.333060	53.643713
3090.666052	150.252271	53.648717
3090.285709	143.533082	53.653722
3089.117795	147.765584	53.658727
3089.041868	144.018392	53.663732
3088.511475	141.022259	53.668737
3087.630105	147.460486	53.673741
3086.940215	144.259504	53.678746
3086.185645	150.129369	53.683751
3085.192717	143.516823	53.688756
3084.443209	149.057015	53.693761
3083.617355	152.845424	53.698765
3082.691080	149.176027	53.703770
3082.090447	139.106531	53.708775
3081.865760	143.485362	53.713780
3081.150481	140.344376	53.718785
3080.497170	138.433828	53.723789
3080.090537	131.838739	53.728794
3079.647159	137.594245	53.733799
3079.232910	144.332385	53.738804
3078.012668	136.577659	53.743809
3077.370609	145.972558	53.748813
3077.523868	138.147748	53.753818
3076.094206	137.773898	53.758823
3075.093267	141.420910	53.763828
3075.068088	141.738244	53.768833
3074.605574	138.068161	53.773837
3074.116072	135.389115	53.778842
3072.766103	142.317137	53.783847
3072.154427	140.719994	53.788852
3071.701213	137.626993	53.793857
3071.102855	142.239009	53.798861
3070.681123	135.261642	53.803866
3069.416893	139.349948	53.808871
3068.600318	135.200771	53.813876
3068.404004	132.931488	53.818881
3067.673959	137.742447	53.823885
3067.704348	132.691465	53.828890
3066.792307	143.397596	53.833895
3064.871524	140.717589	53.838900
3064.894775	131.172670	53.843905
3064.076070	144.935412	53.848909
3063.668809	136.737442	53.853914
3063.157105	140.215994	53.858919
3062.287703	142.045310	53.863924
3061.796774	133.269547	53.868929
3060.938169	136.011997	53.873933
3060.542969	136.582814	53.878938
3059.709637	141.104721	53.883943
3058.966160	138.466309	53.888948
3058.573010	132.355619	53.893953
3057.519604	136.648292	53.898957
3057.070763	131.052370	53.903962
3056.391353	141.447967	53.908967
3055.448177	138.826310	53.913972
3055.381840	133.923301	53.918977
3054.335473	138.650946	53.923981
3053.946945	140.044421	53.928986
3053.143271	141.686064	53.933991
3052.577686	142.161263	53.938996
3052.624433	133.981638	53.944001
3051.235154	144.510375	53.949005
3050.350332	142.424656	53.954010
3049.978764	151.190722	53.959015
3049.263831	138.418721	53.964020
3048.617138	144.390545	53.969025
3047.904880	143.204924	53.974029
3047.246107	133.941144	53.979034
3046.615977	138.766216	53.984039
3045.563359	139.843701	53.989044
3045.544580	135.680969	53.994049
3044.499642	146.463494	53.999053
3043.775515	135.765388	54.004058
3043.713416	150.013443	54.009063
3042.819815	151.184939	54.014068
3042.432591	145.425726	54.019073
3041.474644	149.164869	54.024077
3040.863642	143.761254	54.029082
3040.000188	138.193152	54.034087
3039.568625	140.024234	54.039092
3039.161195	141.115026	54.044097
3038.261596	139.030256	54.049101
3037.284244	135.562621	54.054106
3036.744631	139.255938	54.059111
3035.915290	138.044931	54.064116
3035.413725	137.829866	54.069121
3034.585958	141.732680	54.074125
3034.253036	138.558736	54.079130
3033.493682	144.327975	54.084135
3032.595247	140.029769	54.089140
3031.848163	136.500289	54.094145
3031.488068	136.564201	54.099149
3031.079740	140.506263	54.104154
3029.930433	136.451842	54.109159
3029.625075	133.699495	54.114164
3028.863833	130.794921	54.119169
3027.848189	151.385367	54.124173
3027.694494	132.801818	54.129178
3026.528635	146.038895	54.134183
3026.231268	143.398862	54.139188
3025.736188	131.279290	54.144193
3024.350644	137.736565	54.149197
3024.422061	129.130372	54.154202
3023.827439	134.974088	54.159207
3022.578512	131.309316	54.164212
3022.119824	131.962825	54.169217
3021.285067	137.909943	54.174221
3021.060255	125.486437	54.179226
3020.387936	130.044776	54.184231
3019.465236	136.551250	54.189236
3018.690388	128.758331	54.194241
3018.156555	136.471352	54.199245
3017.949769	129.467528	54.204250
3017.245754	139.081822	54.209255
3016.326634	136.930130	54.214260
3015.841923	129.815511	54.219265
3014.858056	135.248911	54.224269
3014.716711	130.368985	54.229274
3013.784222	129.442049	54.234279
3013.060708	130.685535	54.239284
3012.484846	127.369165	54.244289
3011.921351	128.273078	54.249293
3011.494875	125.909315	54.254298
3009.876016	130.276117	54.259303
3009.253535	131.181031	54.264308
3009.193739	121.928596	54.269313
3008.483507	133.519952	54.274317
3007.803814	134.173333	54.279322
3006.702451	136.318996	54.284327
3006.243725	130.085707	54.289332
3006.242864	130.527172	54.294337
3005.078330	136.574852	54.299341
3004.410755	133.214155	54.304346
3003.515755	135.146534	54.309351
3002.478153	133.196272	54.314356
3002.791667	127.663899	54.319361
3001.725640	134.597486	54.324365
3000.732139	129.986727	54.329370
3000.639929	137.615600	54.334375
2999.857302	138.628405	54.339380
2999.680902	135.759289	54.344385
2998.765520	136.696098	54.349389
2998.200760	133.716113	54.354394
2997.823574	143.815337	54.359399
2996.411935	143.219353	54.364404
2995.490582	131.247627	54.369409
2995.201759	140.804394	54.374413
2995.074769	134.872830	54.379418
2994.048671	136.723800	54.384423
2993.255169	138.788834	54.389428
2992.507024	134.324828	54.394433
2991.783691	137.529290	54.399437
2991.216020	133.943107	54.404442
2990.623187	136.901065	54.409447
2989.806079	131.448211	54.414452
2989.432364	130.125803	54.419457
2988.310602	137.450618	54.424461
2988.133655	131.192864	54.429466
2987.487719	133.714643	54.434471
2986.894371	124.772457	54.439476
2986.501844	126.238063	54.444481
2985.194061	134.456749	54.449485
2984.332831	124.587732	54.454490
2983.890383	136.745946	54.459495
2982.876599	134.190447	54.464500
2982.324936	129.342352	54.469505
2982.158154	136.993440	54.474509
2981.822684	138.140226	54.479514
2980.738939	132.045323	54.484519
2980.014853	130.920547	54.489524
2979.610638	122.443795	54.494529
2978.781109	132.462024	54.499533
2978.247632	128.402644	54.504538
2977.774823	132.699531	54.509543
2977.050154	131.824323	54.514548
2975.840631	124.416740	54.519553
2974.937286	127.957482	54.524557
2974.695130	132.291926	54.529562
2974.370146	128.802430	54.534567
2973.312404	122.763877	54.539572
2972.897573	121.764673	54.544577
2972.077790	130.895468	54.549581
2971.793485	128.937667	54.554586
2971.317668	131.956153	54.559591
2970.793849	130.711501	54.564596
2969.629881	127.428531	54.569601
2968.724065	129.872750	54.574605
2968.018372	123.247473	54.579610
2967.415529	133.826160	54.584615
2966.396650	129.515396	54.589620
2966.020087	126.063925	54.594625
2965.112941	138.198131	54.599629
2964.883727	132.707187	54.604634
2964.511287	129.524609	54.609639
2963.584245	127.703090	54.614644
2963.102192	123.597821	54.619649
2962.715198	128.309506	54.624653
2961.947416	124.313458	54.629658
2961.253682	129.881619	54.634663
2960.036483	129.042818	54.639668
2959.323271	130.440072	54.644673
2958.455488	125.790472	54.649677
2958.211680	117.192764	54.654682
2957.461472	122.731891	54.659687
2956.650121	133.832513	54.664692
2957.081306	122.112426	54.669697
2955.970084	117.977706	54.674701
2955.343888	122.814737	54.679706
2954.879749	129.195879	54.684711
2953.804712	131.292843	54.689716
2952.858682	126.902925	54.694721
2951.765201	126.522972	54.699725
2951.215733	131.178740	54.704730
2951.538723	128.257446	54.709735
2950.106321	132.767263	54.714740
2949.808590	117.343681	54.719745
2949.002424	129.914560	54.724749
2948.413567	128.179722	54.729754
2948.057972	127.353551	54.734759
2947.464595	122.706007	54.739764
2946.961232	112.209814	54.744769
2945.399265	126.069554	54.749773
2944.360463	125.099221	54.754778
2944.378689	129.011414	54.759783
2944.005418	123.239969	54.764788
2943.269333	128.945234	54.769793
2942.647897	136.722961	54.774797
2941.754024	121.747821	54.779802
2941.638800	118.225248	54.784807
2941.154452	120.607707	54.789812
2940.031730	118.734372	54.794817
2938.897027	127.048611	54.799821
2938.316667	124.366557	54.804826
2937.549134	124.857724	54.809831
2936.727004	130.279280	54.814836
2936.581617	121.846723	54.819841
2935.831990	117.189964	54.824845
2935.200534	113.492329	54.829850
2934.651577	119.884014	54.834855
2933.762362	121.993829	54.839860
2933.611317	116.929656	54.844865
2933.000543	129.430434	54.849869
2932.145620	118.978924	54.854874
2930.781659	120.420283	54.859879
2929.926620	133.757787	54.864884
2930.229572	117.691177	54.869889
2929.095980	122.616893	54.874893
2928.627014	127.616921	54.879898
2927.856235	118.272846	54.884903
2927.249509	128.248656	54.889908
2926.951356	121.494533	54.894913
2926.435051	119.133895	54.899917
2925.493336	110.847299	54.904922
2924.627853	110.913508	54.909927
2923.545151	120.478825	54.914932
2923.195614	123.724409	54.919937
2922.434023	122.137906	54.924941
2922.345293	123.243712	54.929946
2921.697306	121.062284	54.934951
2920.920155	124.345024	54.939956
2920.988376	114.507452	54.944961
2919.587119	122.613433	54.949965
2918.497654	121.474136	54.954970
2918.107887	119.290422	54.959975
2917.076488	128.315675	54.964980
2917.170829	124.141909	54.969985
2916.512498	131.311350	54.974989
2915.708574	121.650054	54.979994
2914.886731	119.451366	54.984999
2913.562356	125.862676	54.990004
2913.024098	116.297690	54.995009
2912.662971	126.228370	55.000013
2911.976218	121.319297	55.005018
2911.320185	120.315135	55.010023
2910.515441	127.388020	55.015028
2910.193133	113.821892	55.020033
2909.794825	122.326462	55.025037
2909.463425	121.725100	55.030042
2909.141578	118.854402	55.035047
2907.132523	126.785975	55.040052
2906.860404	115.294637	55.045057
2906.121719	123.359231	55.050061
2905.447276	119.685523	55.055066
2904.622655	122.900195	55.060071
2903.911257	122.505086	55.065076
2903.648777	118.058363	55.070081
2902.761155	126.754711	55.075085
2902.643866	125.745321	55.080090
2901.551373	123.153162	55.085095
2900.551533	130.868058	55.090100
2900.116315	121.938735	55.095105
2899.207761	123.319247	55.100109
2898.979164	123.522138	55.105114
2898.475060	121.498882	55.110119
2897.833840	128.060678	55.115124
2897.502543	119.035046	55.120129
2896.776674	128.073611	55.125133
2895.501515	131.207785	55.130138
2894.970696	112.399406	55.135143
2893.686333	127.218658	55.140148
2893.611313	118.636717	55.145153
2892.699337	128.177601	55.150157
2892.132897	125.602119	55.155162
2892.126926	121.746674	55.160167
2891.059979	126.749031	55.165172
2890.708322	119.137238	55.170177
2889.601187	125.976414	55.175181
2888.522822	124.543129	55.180186
2888.388827	125.591146	55.185191
2887.707430	132.383619	55.190196
2887.131882	117.271997	55.195201
2886.532967	126.013740	55.200205
2885.796429	117.434725	55.205210
2885.686227	121.649118	55.210215
2884.122829	122.464194	55.215220
2883.631551	120.591901	55.220225
2882.546342	126.648537	55.225229
2881.925419	124.989448	55.230234
2882.137037	122.400994	55.235239
2881.357224	124.096604	55.240244
2880.680837	116.500443	55.245249
2879.925419	128.426744	55.250253
2879.771803	123.743134	55.255258
2878.831423	127.117720	55.260263
2877.949568	126.756482	55.265268
2877.487274	120.367119	55.270273
2876.374227	120.493011	55.275277
2875.835440	112.048359	55.280282
2875.368598	115.323859	55.285287
2874.043922	121.454575	55.290292
2873.254614	120.500431	55.295297
2873.333787	119.103003	55.300301
2872.528318	121.976520	55.305306
2872.356315	114.735465	55.310311
2870.952848	115.162432	55.315316
2870.568807	116.323049	55.320321
2870.131497	119.289168	55.325325
2869.630704	116.918386	55.330330
2868.545666	109.003659	55.335335
2867.559818	120.339352	55.340340
2867.134635	112.425140	55.345345
2866.576718	122.428920	55.350349
2866.090094	117.476575	55.355354
2865.968755	120.358300	55.360359
2865.172333	127.467265	55.365364
2863.735384	113.951119	55.370369
2863.053994	122.488277	55.375373
2862.287394	115.992245	55.380378
2861.747224	117.836764	55.385383
2861.411487	123.277827	55.390388
2861.002978	109.642368	55.395393
2860.322341	126.652986	55.400397
2859.593880	114.447036	55.405402
2858.764629	102.843700	55.410407
2857.473738	113.430623	55.415412
2857.361178	110.015362	55.420417
2856.894877	120.997798	55.425421
2856.188165	114.089307	55.430426
2855.517390	112.114278	55.435431
2854.997388	121.660800	55.440436
2853.774118	112.799462	55.445441
2852.977658	114.508182	55.450445
2852.175740	118.635138	55.455450
2851.946566	111.008737	55.460455
2851.529799	123.743582	55.465460
2851.151690	116.951031	55.470465
2850.574474	120.474338	55.475469
2849.974201	112.083224	55.480474
2848.796505	112.466085	55.485479
2847.945060	115.037600	55.490484
2846.928684	113.082165	55.495489
2846.443852	114.598683	55.500493
2846.229544	118.783894	55.505498
2846.017554	118.480672	55.510503
2845.035409	124.214969	55.515508
2844.745462	113.514958	55.520513
2843.189027	123.145852	55.525517
2842.250986	122.103846	55.530522
2841.962592	115.077287	55.535527
2841.191245	118.175889	55.540532
2841.199070	110.990551	55.545537
2840.624429	124.482620	55.550541
2839.821745	117.809211	55.555546
2839.230591	118.587606	55.560551
2837.857355	121.395139	55.565556
2837.595417	116.425713	55.570561
2837.020851	120.385529	55.575565
2836.117526	116.565430	55.580570
2835.978007	120.994036	55.585575
2835.043240	119.109126	55.590580
2833.903060	114.026517	55.595585
2833.168018	121.865892	55.600589
2832.621118	126.871348	55.605594
2832.391142	124.562044	55.610599
2831.867585	132.917896	55.615604
2831.605595	117.302316	55.620609
2830.842582	117.596150	55.625613
2829.453118	122.470087	55.630618
2829.089332	116.651645	55.635623
2828.504448	118.389732	55.640628
2827.726130	114.401037	55.645633
2827.026232	117.824526	55.650637
2826.525011	123.751359	55.655642
2825.678802	118.373778	55.660647
2824.707357	123.989804	55.665652
2824.212189	114.087086	55.670657
2823.484526	115.353801	55.675661
2822.833333	114.459741	55.680666
2822.433904	122.814505	55.685671
2821.686633	118.992209	55.690676
2821.449802	115.215304	55.695681
2821.069410	112.458434	55.700685
2819.472877	119.530071	55.705690
2818.883407	119.150053	55.710695
2818.059434	128.928526	55.715700
2817.550799	114.407446	55.720705
2817.108252	129.714786	55.725709
2816.814761	120.382713	55.730714
2816.440550	112.991888	55.735719
2814.783782	121.602595	55.740724
2814.011721	116.674174	55.745729
2813.874664	122.925204	55.750733
2813.273492	113.954003	55.755738
2812.731525	109.617425	55.760743
2811.932995	105.607322	55.765748
2811.487507	113.678250	55.770753
2810.245007	115.825172	55.775757
2809.647594	116.626350	55.780762
2809.036837	109.509239	55.785767
2808.726022	126.771637	55.790772
2808.710695	110.423140	55.795777
2806.676533	104.278762	55.800781
2805.800720	109.405954	55.805786
2806.209196	104.600234	55.810791
2805.787944	120.861135	55.815796
2805.485083	112.740899	55.820801
2803.881912	116.562711	55.825805
2802.512904	114.640317	55.830810
2802.306713	109.690184	55.835815
2801.729304	116.650403	55.840820
2801.168441	110.091198	55.845825
2800.675195	118.509360	55.850829
2799.919953	114.692773	55.855834
2800.032255	110.383318	55.860839
2799.225848	117.898188	55.865844
2798.276939	107.620674	55.870849
2797.288042	111.097900	55.875853
2796.651205	109.077606	55.880858
2796.033603	109.466195	55.885863
2795.228486	113.589360	55.890868
2794.570472	114.227611	55.895873
2793.764384	109.747500	55.900877
2793.104882	123.706425	55.905882
2792.866969	111.376786	55.910887
2792.024147	124.019846	55.915892
2791.265535	112.024326	55.920897
2791.027879	112.318767	55.925901
2790.006963	110.534641	55.930906
2788.946140	103.358279	55.935911
2788.037927	117.526282	55.940916
2787.929995	111.064135	55.945921
2787.724516	112.050161	55.950925
2786.974427	119.366728	55.955930
2786.676309	109.311135	55.960935
2785.838696	113.452092	55.965940
2784.777663	109.391335	55.970945
2784.060013	119.129131	55.975949
2783.178415	112.195285	55.980954
2783.156915	108.131719	55.985959
2782.227519	114.268307	55.990964
2781.240681	104.828181	55.995969
2780.135653	113.312615	56.000973
2780.106637	108.278125	56.005978
2779.214816	106.778639	56.010983
2778.347869	103.212855	56.015988
2777.987813	110.264998	56.020993
2777.588937	118.892419	56.025997
2777.028233	110.896782	56.031002
2776.823765	111.995528	56.036007
2775.725616	120.503265	56.041012
2774.575270	117.851550	56.046017
2774.126603	117.045642	56.051021
2773.463576	117.419102	56.056026
2772.925641	114.134179	56.061031
2772.615800	113.740715	56.066036
2772.082150	113.074065	56.071041
2770.733689	107.515509	56.076045
2769.581053	111.630970	56.081050
2769.538541	108.184005	56.086055
2769.060881	112.622640	56.091060
2768.658202	104.598815	56.096065
2768.295586	109.377776	56.101069
2766.765801	109.144273	56.106074
2766.329385	105.575956	56.111079
2765.395612	111.309883	56.116084
2765.134317	110.067751	56.121089
2764.668700	107.819255	56.126093
2763.397381	106.113065	56.131098
2762.631321	101.181659	56.136103
2761.832041	110.814985	56.141108
2761.352011	108.139492	56.146113
2761.100011	99.490329	56.151117
2760.305976	109.965891	56.156122
2760.306859	104.841427	56.161127
2759.823584	106.111770	56.166132
2758.931764	104.915437	56.171137
2758.112860	107.880862	56.176141
2756.759340	102.329098	56.181146
2755.895112	100.160183	56.186151
2755.272877	99.309735	56.191156
2755.080069	101.148965	56.196161
2753.943897	109.890954	56.201165
2752.912773	102.403219	56.206170
2753.462879	106.092255	56.211175
2752.270926	108.795795	56.216180
2751.686882	104.080378	56.221185
2751.453222	113.678607	56.226189
2751.039368	111.748098	56.231194
2750.338731	96.869879	56.236199
2748.802184	107.419459	56.241204
2748.234235	98.658911	56.246209
2747.866355	103.177856	56.251213
2747.339377	109.251190	56.256218
2746.495950	99.530387	56.261223
2745.479593	97.695757	56.266228
2744.778077	98.812751	56.271233
2744.321912	96.787637	56.276237
2743.629682	109.693490	56.281242
2743.168084	100.947131	56.286247
2742.889053	107.275312	56.291252
2742.260152	105.205118	56.296257
2741.390482	113.981688	56.301261
2740.281823	109.120684	56.306266
2739.722867	107.420630	56.311271
2739.525907	108.746639	56.316276
2738.817226	108.720945	56.321281
2738.500355	105.404559	56.326285
2737.049305	105.569699	56.331290
2736.408515	96.178597	56.336295
2735.753385	104.291668	56.341300
2735.162557	102.126156	56.346305
2734.947791	106.538802	56.351309
2733.956570	101.828251	56.356314
2733.263182	100.935890	56.361319
2732.367213	103.933042	56.366324
2732.041864	100.309431	56.371329
2731.639076	94.844244	56.376333
2730.799137	99.290328	56.381338
2729.581696	97.575727	56.386343
2728.382506	106.425590	56.391348
2728.616496	100.743405	56.396353
2728.026315	99.418942	56.401357
2727.043250	108.418175	56.406362
2727.206479	99.394499	56.411367
2726.369642	99.493340	56.416372
2725.822682	102.602149	56.421377
2724.846155	103.335902	56.426381
2724.012940	107.067176	56.431386
2723.817036	101.126507	56.436391
2722.718461	98.699242	56.441396
2722.218557	102.546038	56.446401
2721.621258	97.405012	56.451405
2720.320318	101.336623	56.456410
2720.019071	97.967044	56.461415
2719.489509	98.802420	56.466420
2719.126828	100.564901	56.471425
2717.661841	102.880918	56.476429
2716.624283	102.670658	56.481434
2716.292749	96.428316	56.486439
2715.826705	97.117445	56.491444
2715.793659	95.767226	56.496449
2715.546310	100.645295	56.501453
2714.822262	102.414282	56.506458
2713.745214	93.456166	56.511463
2712.906633	96.612058	56.516468
2712.196254	101.580719	56.521473
2711.432909	105.847535	56.526477
2710.914076	105.905838	56.531482
2709.964945	98.408048	56.536487
2708.915780	101.053637	56.541492
2708.504939	106.727393	56.546497
2708.216839	94.844901	56.551501
2707.395391	99.060859	56.556506
2707.192052	101.322667	56.561511
2706.536477	112.534017	56.566516
2705.621134	109.146251	56.571521
2704.496368	113.556160	56.576525
2703.896970	113.953883	56.581530
2703.541912	106.487175	56.586535
2702.859635	108.918083	56.591540
2702.269458	101.529855	56.596545
2702.182352	109.428208	56.601549
2700.701602	105.422241	56.606554
2700.490793	104.871332	56.611559
2699.439024	106.987252	56.616564
2699.189613	109.981652	56.621569
2698.794524	108.887522	56.626573
2697.220584	107.945948	56.631578
2696.691007	98.657814	56.636583
2695.734414	112.649351	56.641588
2695.488832	105.622996	56.646593
2695.058248	96.062555	56.651597
2694.412219	110.751378	56.656602
2694.280779	99.025654	56.661607
2693.277697	103.499629	56.666612
2692.442691	97.631893	56.671617
2691.964207	97.912241	56.676621
2691.023420	99.857222	56.681626
2690.766692	99.000750	56.686631
2689.072071	103.994762	56.691636
2688.477926	103.493984	56.696641
2688.212088	95.475995	56.701645
2687.444713	99.815341	56.706650
2687.125356	101.856198	56.711655
2686.493282	106.981210	56.716660
2686.373845	104.385006	56.721665
2685.214060	105.784413	56.726669
2684.013420	109.928619	56.731674
2683.767255	101.045975	56.736679
2683.225850	107.295059	56.741684
2682.456713	99.380073	56.746689
2681.997336	101.630781	56.751693
2681.032796	102.579591	56.756698
2680.088224	101.074535	56.761703
2679.526627	105.263053	56.766708
2679.302906	103.180055	56.771713
2678.822110	98.724494	56.776717
2677.990912	111.074645	56.781722
2677.197338	103.969864	56.786727
2675.961133	110.715073	56.791732
2675.885978	107.023832	56.796737
2675.424639	108.209119	56.801741
2674.594812	107.613632	56.806746
2674.296237	101.603284	56.811751
2672.877390	101.811092	56.816756
2672.387333	100.195583	56.821761
2671.832574	94.545598	56.826765
2671.050425	105.602137	56.831770
2671.289147	103.049708	56.836775
2670.289019	105.664422	56.841780
2669.191774	110.780926	56.846785
2668.800422	113.056323	56.851789
2667.910660	107.097294	56.856794
2667.750678	100.288016	56.861799
2666.271005	107.076027	56.866804
2665.448130	101.532660	56.871809
2664.971267	100.108705	56.876813
2664.251142	109.220887	56.881818
2663.999227	104.699361	56.886823
2663.674726	105.165752	56.891828
2662.988586	102.936412	56.896833
2662.256570	97.407909	56.901837
2661.474782	106.348662	56.906842
2660.818744	99.964433	56.911847
2660.134930	107.227437	56.916852
2659.187252	105.542920	56.921857
2658.114500	100.135423	56.926861
2657.487251	116.131920	56.931866
2657.476512	97.901024	56.936871
2656.883027	109.386749	56.941876
2656.199056	98.217703	56.946881
2655.917584	101.604808	56.951885
2654.773869	103.633824	56.956890
2653.974199	101.196925	56.961895
2652.924788	101.096463	56.966900
2652.658341	101.227283	56.971905
2652.508407	97.578827	56.976909
2651.387977	102.710347	56.981914
2650.605097	100.696092	56.986919
2649.842725	104.342240	56.991924
2649.199592	100.241265	56.996929
2648.861981	98.831797	57.001933
2647.909524	100.572732	57.006938
2647.550954	97.772285	57.011943
2646.884735	103.634164	57.016948
2646.104619	97.134969	57.021953
2645.547955	89.284726	57.026957
2644.505995	97.790753	57.031962
2644.519682	102.518808	57.036967
2643.813745	104.873638	57.041972
2642.823313	93.661462	57.046977
2642.036871	98.233800	57.051981
2641.237304	109.209242	57.056986
2641.116377	99.651138	57.061991
2640.674367	100.923908	57.066996
2639.559710	97.412339	57.072001
2638.718442	93.258792	57.077005
2637.914511	99.979844	57.082010
2637.789502	95.472155	57.087015
2637.039492	98.175560	57.092020
2635.984145	99.571333	57.097025
2635.318828	94.702073	57.102029
2634.323109	105.541707	57.107034
2633.931260	100.225446	57.112039
2633.643719	99.369508	57.117044
2633.104250	102.083501	57.122049
2633.131007	91.395717	57.127053
2631.692628	96.789214	57.132058
2630.904003	99.536720	57.137063
2630.437337	101.154354	57.142068
2629.675587	99.265960	57.147073
2629.353816	91.782132	57.152077
2627.881329	98.361688	57.157082
2627.743943	94.905293	57.162087
2626.937921	105.350538	57.167092
2626.684051	98.341401	57.172097
2626.116022	99.672029	57.177101
2624.420739	104.572621	57.182106
2623.967281	98.712700	57.187111
2623.185319	103.274407	57.192116
2622.557985	96.332666	57.197121
2622.626551	97.203957	57.202125
2622.114552	98.966310	57.207130
2621.675470	97.657477	57.212135
2620.442000	108.103559	57.217140
2619.793377	102.232001	57.222145
2619.448020	93.789866	57.227149
2617.879596	98.627326	57.232154
2617.778232	95.848832	57.237159
2616.872656	107.382774	57.242164
2616.103258	100.912145	57.247169
2615.737559	97.140317	57.252173
2615.078905	105.192023	57.257178
2615.024989	95.518656	57.262183
2613.794349	100.442054	57.267188
2612.876651	100.148563	57.272193
2612.208046	96.644431	57.277197
2611.615423	109.956398	57.282202
2611.057755	90.780890	57.287207
2610.675298	102.177246	57.292212
2610.348912	101.898721	57.297217
2609.217924	98.373767	57.302221
2608.250571	103.805957	57.307226
2608.093767	96.158144	57.312231
2607.492064	97.087965	57.317236
2606.250281	98.167862	57.322241
2605.511340	94.196559	57.327245
2604.624531	97.203607	57.332250
2604.500087	100.647551	57.337255
2603.641016	98.027795	57.342260
2603.533885	93.438898	57.347265
2603.097338	100.862914	57.352269
2602.134033	99.070162	57.357274
2601.403439	99.698343	57.362279
2601.022962	106.173727	57.367284
2600.138314	111.949404	57.372289
2599.181009	97.677588	57.377293
2598.340065	104.996664	57.382298
2597.994669	102.033710	57.387303
2596.900461	98.292872	57.392308
2596.934844	94.565150	57.397313
2596.234966	96.774083	57.402317
2595.040065	108.328276	57.407322
2594.810104	104.637057	57.412327
2594.441697	108.279019	57.417332
2592.994008	104.005731	57.422337
2592.467417	99.888790	57.427341
2591.486041	103.137000	57.432346
2591.275837	101.687204	57.437351
2590.973055	104.035880	57.442356
2590.168314	101.071717	57.447361
2589.677488	103.376753	57.452365
2588.358886	109.410161	57.457370
2587.706932	98.028033	57.462375
2587.036453	102.370955	57.467380
2586.359583	105.676054	57.472385
2586.447655	106.378621	57.477389
2585.753857	112.105489	57.482394
2585.051740	107.370020	57.487399
2584.146353	113.811198	57.492404
2583.201609	111.007148	57.497409
2583.115239	104.384630	57.502413
2581.902091	108.453229	57.507418
2580.711679	99.205064	57.512423
2580.255173	105.918438	57.517428
2580.143460	112.838916	57.522433
2579.196569	104.221730	57.527437
2578.680196	110.997839	57.532442
2578.412570	107.708179	57.537447
2577.889662	107.818899	57.542452
2577.012485	116.730575	57.547457
2576.400017	106.336006	57.552461
2575.021869	120.040418	57.557466
2574.790423	103.203144	57.562471
2574.751599	108.858304	57.567476
2573.563861	107.321812	57.572481
2572.951278	110.765525	57.577485
2571.908635	107.085742	57.582490
2571.768114	100.804841	57.587495
2570.955980	102.504433	57.592500
2569.576881	110.398261	57.597505
2568.850621	105.619555	57.602509
2568.457396	106.165198	57.607514
2568.104500	99.375885	57.612519
2567.228113	104.394647	57.617524
2566.847500	101.918886	57.622529
2566.728027	105.988408	57.627533
2566.580193	106.732487	57.632538
2565.461178	106.572101	57.637543
2564.472550	98.761374	57.642548
2563.301939	106.458116	57.647553
2562.581090	93.517562	57.652557
2561.632395	113.916497	57.657562
2561.508135	94.542567	57.662567
2560.988341	94.553286	57.667572
2560.237615	102.690204	57.672577
2560.328710	89.048759	57.677581
2559.413095	101.252288	57.682586
2558.085552	105.388999	57.687591
2557.154332	103.242229	57.692596
2556.633383	105.994113	57.697601
2556.424793	98.095429	57.702605
2555.844308	103.828581	57.707610
2555.549090	94.800008	57.712615
2554.257257	101.561056	57.717620
2553.202687	102.299495	57.722625
2553.015866	97.157794	57.727629
2552.498468	107.216210	57.732634
2551.915938	95.112905	57.737639
2550.858945	98.892320	57.742644
2549.970397	106.050201	57.747649
2549.621374	103.677590	57.752653
2548.974863	107.638272	57.757658
2548.282560	97.658404	57.762663
2548.111733	102.238003	57.767668
2547.015716	98.579589	57.772673
2546.730760	87.993658	57.777677
2545.735654	99.726449	57.782682
2545.304373	101.316329	57.787687
2544.813956	97.326233	57.792692
2543.800541	97.670414	57.797697
2543.293187	90.111355	57.802701
2542.592596	107.175866	57.807706
2542.346926	87.101545	57.812711
2540.705211	92.022205	57.817716
2539.772224	104.049502	57.822721
2539.790949	91.223695	57.827725
2538.580174	105.101188	57.832730
2538.402918	96.533223	57.837735
2537.987268	98.015830	57.842740
2537.369320	100.337864	57.847745
2536.802680	92.164882	57.852749
2535.620987	101.313342	57.857754
2534.860862	91.356918	57.862759
2534.583729	92.656374	57.867764
2534.155646	94.798322	57.872769
2533.778840	99.321164	57.877773
2532.233205	96.343154	57.882778
2531.838532	95.134103	57.887783
2531.372729	107.011666	57.892788
2530.606263	98.566932	57.897793
2530.366709	92.962159	57.902797
2528.737488	99.732735	57.907802
2528.352124	102.459072	57.912807
2527.721331	99.439920	57.917812
2527.072291	100.197452	57.922817
2527.057821	98.037640	57.927821
2526.028277	105.257521	57.932826
2525.202736	101.088674	57.937831
2524.355446	105.515117	57.942836
2523.776155	98.540706	57.947841
2523.431573	103.155143	57.952845
2522.784097	110.171949	57.957850
2522.032437	104.681170	57.962855
2521.629077	105.461041	57.967860
2520.741194	103.042403	57.972865
2519.754033	93.682936	57.977869
2519.169093	110.230719	57.982874
2519.209502	98.327621	57.987879
2517.836261	97.740986	57.992884
2517.013100	100.087448	57.997889
2516.627294	102.218617	58.002893
2516.142521	101.643109	58.007898
2515.669547	103.654974	58.012903
2514.671256	97.394416	58.017908
2513.818218	103.454816	58.022913
2513.502074	98.137076	58.027917
2512.663410	108.572512	58.032922
2512.541466	98.572902	58.037927
2511.318881	97.798280	58.042932
2510.370959	104.735401	58.047937
2509.867862	98.006512	58.052941
2509.620899	101.880334	58.057946
2509.402165	92.215424	58.062951
2508.514992	95.953575	58.067956
2507.309582	99.887840	58.072961
2506.957410	97.369329	58.077965
2505.870502	96.179947	58.082970
2505.669386	100.913140	58.087975
2504.415028	103.200697	58.092980
2503.442112	107.623752	58.097985
2503.118314	97.201563	58.102989
2502.443270	100.783453	58.107994
2502.563957	98.618296	58.112999
2502.284366	100.951562	58.118004
2501.518993	104.019571	58.123009
2500.826015	93.534980	58.128013
2499.619105	94.455390	58.133018
2499.038761	92.276275	58.138023
2497.774873	95.102680	58.143028
2496.649669	98.591802	58.148033
2496.267184	99.000617	58.153037
2495.861748	95.698213	58.158042
2495.673993	84.101759	58.163047
2495.356872	91.512853	58.168052
2494.754135	100.709961	58.173057
2493.720898	93.976585	58.178061
2492.566297	99.659082	58.183066
2492.217181	90.278958	58.188071
2491.697908	88.808196	58.193076
2491.178946	91.903152	58.198081
2490.438473	86.699806	58.203085
2489.439379	93.383181	58.208090
2489.115340	94.730526	58.213095
2488.575695	89.552447	58.218100
2487.719967	93.205490	58.223105
2486.891437	92.676125	58.228109
2485.789486	89.932528	58.233114
2485.679035	96.970011	58.238119
2485.292051	84.418048	58.243124
2484.580035	97.673836	58.248129
2484.059397	93.430766	58.253133
2482.703820	92.440081	58.258138
2482.227041	88.324905	58.263143
2481.861690	89.933120	58.268148
2481.412386	92.904856	58.273153
2480.232773	91.457390	58.278157
2479.243294	92.095506	58.283162
2478.881380	88.666458	58.288167
2478.465218	89.819166	58.293172
2477.781033	92.767903	58.298177
2477.522513	82.715870	58.303181
2476.357544	82.335604	58.308186
2475.485201	81.530321	58.313191
2474.852226	94.746146	58.318196
2474.171769	91.579579	58.323201
2473.818221	84.257125	58.328205
2473.537978	93.325279	58.333210
2472.509401	91.392534	58.338215
2471.864600	95.426740	58.343220
2470.983204	91.808228	58.348225
2470.701980	89.704683	58.353229
2470.262902	96.705196	58.358234
2469.173972	92.236406	58.363239
2468.518471	96.099947	58.368244
2467.454649	94.842681	58.373249
2467.771052	88.840899	58.378253
2466.724880	84.878337	58.383258
2465.400241	88.989697	58.388263
2465.245890	85.437930	58.393268
2464.223911	90.461459	58.398273
2463.757089	84.156235	58.403277
2463.199753	98.098843	58.408282
2462.953270	94.029949	58.413287
2461.826031	97.985987	58.418292
2461.073788	90.006985	58.423297
2460.704999	77.402582	58.428301
2460.013149	90.274007	58.433306
2459.204150	86.148927	58.438311
2458.450026	85.419351	58.443316
2457.760754	93.584839	58.448321
2457.316603	80.879243	58.453325
2456.597576	88.189318	58.458330
2456.216150	78.671446	58.463335
2454.904216	81.987635	58.468340
2454.081279	86.024666	58.473345
2453.801840	80.605535	58.478349
2453.119160	75.237192	58.483354
2452.803204	83.424502	58.488359
2452.582088	81.202528	58.493364
2451.279978	91.263656	58.498369
2450.370541	80.922669	58.503373
2449.880206	84.319037	58.508378
2449.303718	82.693463	58.513383
2449.023288	87.715335	58.518388
2447.957888	86.253086	58.523393
2447.230103	81.235469	58.528397
2446.331497	85.682530	58.533402
2446.069680	86.860559	58.538407
2445.759181	82.088559	58.543412
2444.923884	91.923826	58.548417
2444.202156	78.396512	58.553421
2443.019993	86.677453	58.558426
2442.796751	88.345054	58.563431
2442.324970	79.568135	58.568436
2441.500734	91.174213	58.573441
2440.980089	87.606525	58.578445
2439.759258	85.026155	58.583450
2439.154353	88.352905	58.588455
2439.114904	90.122104	58.593460
2438.135509	92.198061	58.598465
2437.068127	81.655538	58.603469
2436.493244	90.156323	58.608474
2435.915153	85.339289	58.613479
2435.509442	88.005161	58.618484
2435.044178	95.030677	58.623489
2435.057160	84.566320	58.628493
2433.824389	88.283044	58.633498
2432.634056	87.287408	58.638503
2432.345907	87.156694	58.643508
2431.430137	87.684324	58.648513
2430.675988	90.566083	58.653517
2429.839052	87.725479	58.658522
2429.446847	81.635259	58.663527
2429.250689	80.923573	58.668532
2428.654236	84.643207	58.673537
2427.555862	82.343077	58.678541
2426.597936	90.775150	58.683546
2426.400172	86.007164	58.688551
2426.129408	82.275968	58.693556
2424.830309	89.344185	58.698561
2423.566417	76.194964	58.703565
2422.805303	91.461966	58.708570
2422.223486	81.153389	58.713575
2422.478504	80.394166	58.718580
2421.974442	80.347342	58.723585
2421.474049	82.374161	58.728589
2420.555898	85.288303	58.733594
2419.317459	84.099192	58.738599
2418.655853	79.938262	58.743604
2417.970901	86.156234	58.748609
2417.710587	77.810910	58.753613
2417.454091	83.970228	58.758618
2416.674025	84.000200	58.763623
2415.860752	77.537914	58.768628
2414.964934	83.338797	58.773633
2414.727804	76.555378	58.778637
2413.137536	81.459376	58.783642
2412.346099	86.409151	58.788647
2411.997199	76.602710	58.793652
2411.423560	86.739014	58.798657
2411.118439	80.722326	58.803661
2410.433277	86.649028	58.808666
2409.966310	85.470506	58.813671
2409.771184	76.896151	58.818676
2408.456938	78.350834	58.823681
2407.951136	83.270323	58.828685
2407.286249	83.165343	58.833690
2406.193145	82.967008	58.838695
2405.346386	80.077170	58.843700
2404.895969	85.977945	58.848705
2404.552893	79.539867	58.853709
2403.936157	87.976363	58.858714
2403.331496	81.365518	58.863719
2402.487435	84.145420	58.868724
2401.546117	83.507857	58.873729
2401.313413	81.406285	58.878733
2400.873406	87.942364	58.883738
2399.694453	84.945121	58.888743
2399.062609	88.703966	58.893748
2397.840421	90.368695	58.898753
2397.957306	78.284398	58.903757
2397.311108	80.104447	58.908762
2396.765562	81.500327	58.913767
2395.745981	68.996167	58.918772
2394.835455	80.831328	58.923777
2394.359631	72.194055	58.928781
2393.838302	84.140297	58.933786
2393.393058	77.375097	58.938791
2393.310354	80.588877	58.943796
2391.786083	77.787256	58.948801
2391.097361	72.983623	58.953805
2390.718385	85.434849	58.958810
2390.171064	78.188173	58.963815
2389.053634	76.205116	58.968820
2388.105635	87.250927	58.973825
2388.367143	82.108375	58.978829
2387.472794	79.547192	58.983834
2386.857389	78.584310	58.988839
2385.466257	77.649071	58.993844
2384.408166	97.456439	58.998849
2384.574207	82.614486	59.003853
2383.747939	85.013597	59.008858
2383.675003	83.980459	59.013863
2383.343460	83.984269	59.018868
2381.692880	88.482945	59.023873
2381.118018	85.353599	59.028877
2380.234044	88.709520	59.033882
2380.038049	87.177967	59.038887
2379.818736	80.243484	59.043892
2378.975943	88.236281	59.048897
2377.953240	92.129064	59.053901
2377.498831	91.029710	59.058906
2376.845372	86.916338	59.063911
2376.344935	89.025272	59.068916
2375.311047	101.284950	59.073921
2374.603814	91.675167	59.078925
2374.080114	83.762895	59.083930
2373.833130	94.096367	59.088935
2372.802503	88.453593	59.093940
2371.784706	92.753288	59.098945
2371.385410	78.438650	59.103949
2370.673339	89.164264	59.108954
2370.105422	92.925207	59.113959
2369.916937	86.035580	59.118964
2368.583921	91.677945	59.123969
2367.951013	81.462982	59.128973
2367.484225	87.634179	59.133978
2366.991677	90.484240	59.138983
2366.399762	80.642781	59.143988
2364.969126	91.915986	59.148993
2364.651324	79.911546	59.153997
2363.927434	91.542703	59.159002
2363.430796	90.379916	59.164007
2363.446260	84.102764	59.169012
2361.971527	99.749155	59.174017
2361.307058	90.166010	59.179021
2360.746143	85.470783	59.184026
2360.319454	85.111535	59.189031
2359.916043	79.990708	59.194036
2358.545649	91.905301	59.199041
2358.107937	80.668971	59.204045
2357.489324	92.335415	59.209050
2356.643944	92.875099	59.214055
2356.585225	88.817529	59.219060
2355.757489	91.999632	59.224065
2354.486742	86.036751	59.229069
2354.033379	92.524196	59.234074
2353.371605	93.990480	59.239079
2353.178922	84.724944	59.244084
2352.321340	91.287034	59.249089
2351.651377	84.238563	59.254093
2350.771488	85.666355	59.259098
2350.474755	85.261202	59.264103
2349.911696	87.107302	59.269108
2349.218360	87.414944	59.274113
2348.212927	82.743232	59.279117
2347.172054	83.910009	59.284122
2347.001136	91.975417	59.289127
2346.875770	86.355483	59.294132
2345.607977	87.363306	59.299137
2344.364413	92.401058	59.304141
2343.905711	94.358389	59.309146
2343.654154	92.533192	59.314151
2343.217647	91.205393	59.319156
2342.682318	94.229344	59.324161
2342.213035	82.207783	59.329165
2341.482101	91.983369	59.334170
2340.135475	94.693694	59.339175
2339.708566	81.594794	59.344180
2338.728237	87.313824	59.349185
2337.870818	79.773220	59.354189
2337.286294	91.320549	59.359194
2336.763086	83.792266	59.364199
2336.619723	86.629590	59.369204
2335.957767	96.251283	59.374209
2335.642278	88.279730	59.379213
2334.956605	91.169526	59.384218
2333.814347	103.767859	59.389223
2333.263785	90.322215	59.394228
2332.605859	105.049759	59.399233
2331.342502	101.428300	59.404237
2330.743574	100.434580	59.409242
2330.093997	94.737314	59.414247
2330.114747	94.725490	59.419252
2328.990488	96.482431	59.424257
2328.852986	96.125838	59.429261
2328.114934	94.372778	59.434266
2327.006292	93.253463	59.439271
2326.728475	94.095560	59.444276
2326.134978	97.063540	59.449281
2325.310853	102.112468	59.454285
2324.734966	93.168633	59.459290
2323.730458	96.700300	59.464295
2323.442694	90.556707	59.469300
2322.393972	91.165113	59.474305
2321.415435	89.760272	59.479309
2320.783304	92.559206	59.484314
2320.197294	88.103926	59.489319
2319.847344	89.718200	59.494324
2319.381161	100.017710	59.499329
2319.200693	86.573521	59.504333
2317.956786	94.660968	59.509338
2316.975522	89.796845	59.514343
2316.522488	88.944753	59.519348
2315.973322	87.412809	59.524353
2315.620049	87.260870	59.529357
2314.508041	84.536402	59.534362
2313.629140	82.130086	59.539367
2313.746806	83.389670	59.544372
2312.817422	78.473261	59.549377
2311.781784	79.300081	59.554381
2310.959038	83.000790	59.559386
2310.122164	80.860042	59.564391
2309.689927	86.482193	59.569396
2309.354920	81.545853	59.574401
2309.430572	77.187820	59.579405
2308.884452	90.864426	59.584410
2307.360668	91.103298	59.589415
2306.677554	86.699360	59.594420
2306.155094	85.953481	59.599425
2305.564609	81.046618	59.604429
2304.075090	83.267061	59.609434
2303.617509	90.808743	59.614439
2303.101327	83.483337	59.619444
2302.678207	85.697471	59.624449
2302.316662	77.837221	59.629453
2301.688569	83.535888	59.634458
2300.524682	92.867634	59.639463
2299.957041	89.387735	59.644468
2299.285815	93.615938	59.649473
2299.429354	86.321002	59.654477
2298.454077	87.293419	59.659482
2297.604545	88.515903	59.664487
2296.652279	85.295981	59.669492
2296.344725	85.030440	59.674497
2295.191957	83.239755	59.679501
2294.489607	79.174231	59.684506
2293.899859	88.130306	59.689511
2293.660575	80.300069	59.694516
2292.828891	86.631162	59.699521
2292.394536	81.247224	59.704525
2291.533240	79.572876	59.709530
2290.389503	80.041226	59.714535
2289.786399	68.699390	59.719540
2289.326095	85.447255	59.724545
2289.289820	73.530871	59.729549
2288.757527	86.296061	59.734554
2287.442737	84.317171	59.739559
2286.815650	79.481700	59.744564
2285.991672	88.294678	59.749569
2285.816324	88.555195	59.754573
2285.215606	80.594535	59.759578
2284.011357	78.076499	59.764583
2283.304547	76.614938	59.769588
2282.968228	82.170161	59.774593
2282.175474	79.871089	59.779597
2282.017871	87.313316	59.784602
2280.726580	90.027217	59.789607
2280.215831	77.159769	59.794612
2279.135829	86.267966	59.799617
2278.929041	84.216441	59.804621
2278.534732	85.516997	59.809626
2277.691696	83.196920	59.814631
2276.811908	78.661629	59.819636
2275.960585	82.582352	59.824641
2275.851559	77.741183	59.829645
2275.429416	80.188827	59.834650
2274.741727	89.378748	59.839655
2273.781334	80.478975	59.844660
2272.714257	83.035329	59.849665
2272.253142	84.447964	59.854669
2271.806288	74.636195	59.859674
2270.776067	86.730245	59.864679
2270.097709	83.268495	59.869684
2269.382479	93.992680	59.874689
2269.198767	87.405001	59.879693
2268.773489	82.216874	59.884698
2268.097835	85.939801	59.889703
2267.413820	74.924817	59.894708
2266.472720	85.263690	59.899713
2265.888548	84.927038	59.904718
2264.766709	90.239634	59.909722
2263.844038	85.568787	59.914727
2263.417037	79.035742	59.919732
2262.670686	83.510864	59.924737
2262.565302	76.083245	59.929742
2262.436938	83.929796	59.934746
2261.295148	89.739603	59.939751
2260.371619	76.501054	59.944756
2259.576934	84.243666	59.949761
2259.415156	83.848597	59.954766
2258.926638	84.498973	59.959770
2257.566987	81.957388	59.964775
2257.228332	79.687635	59.969780
2256.638656	84.895411	59.974785
2256.074329	78.863465	59.979790
2255.328251	80.454302	59.984794
2254.120750	87.366360	59.989799
2253.907487	84.057568	59.994804
2253.394524	86.331278	59.999809
2252.942537	84.120377	60.004814
2251.616687	88.732100	60.009818
2250.891029	99.953450	60.014823
2250.127223	81.809993	60.019828
2249.613893	88.628603	60.024833
2249.464260	78.681537	60.029838
2248.762861	76.107121	60.034842
2247.930620	89.902519	60.039847
2247.653288	84.508311	60.044852
2246.560558	91.855070	60.049857
2245.874386	87.632450	60.054862
2245.423515	83.433141	60.059866
2244.174481	94.338216	60.064871
2243.535849	84.346487	60.069876
2243.272742	79.626403	60.074881
2242.571209	80.857531	60.079886
2242.698061	80.619543	60.084890
2241.565983	87.785142	60.089895
2240.816020	83.752242	60.094900
2240.145896	84.356311	60.099905
2238.994205	85.098785	60.104910
2238.372164	80.967433	60.109914
2237.277891	92.110900	60.114919
2237.143500	82.437532	60.119924
2236.450264	82.888849	60.124929
2236.164618	79.413628	60.129934
2235.632307	83.264012	60.134938
2235.030740	85.508271	60.139943
2234.353985	83.135293	60.144948
2233.054488	87.662779	60.149953
2232.074149	82.952856	60.154958
2232.121256	79.800453	60.159962
2231.634725	79.330664	60.164967
2231.264365	78.548124	60.169972
2229.832176	82.510164	60.174977
2229.347654	83.221042	60.179982
2229.002609	86.330479	60.184986
2227.934428	87.614838	60.189991
2227.158796	86.151632	60.194996
2226.186269	86.272570	60.200001
2225.641632	88.734060	60.205006
2224.866975	88.240522	60.210010
2224.984986	97.893430	60.215015
2225.218330	84.983602	60.220020
2224.086556	92.008632	60.225025
2222.678717	92.561634	60.230030
2222.118881	87.582438	60.235034
2221.703988	85.952939	60.240039
2221.000807	79.586338	60.245044
2219.849919	84.799700	60.250049
2219.355414	73.353256	60.255054
2219.039572	75.294056	60.260058
2218.123481	76.557143	60.265063
2217.822490	78.213572	60.270068
2216.729260	78.630274	60.275073
2216.027828	80.422683	60.280078
2215.625779	77.757606	60.285082
2215.190270	85.741548	60.290087
2214.636161	77.223874	60.295092
2213.537638	84.633991	60.300097
2212.862016	80.173530	60.305102
2212.363287	74.505756	60.310106
2211.598903	79.121723	60.315111
2210.583996	75.961084	60.320116
2209.788998	72.493242	60.325121
2209.267974	75.972630	60.330126
2209.064127	83.929978	60.335130
2208.318253	87.110333	60.340135
2208.070008	82.403105	60.345140
2207.007042	86.583839	60.350145
2205.946593	84.527527	60.355150
2205.871561	76.966834	60.360154
2205.105552	82.460942	60.365159
2204.090727	79.473178	60.370164
2203.479925	81.672442	60.375169
2202.593550	78.640607	60.380174
2202.492500	75.317761	60.385178
2201.668418	85.647678	60.390183
2201.487981	83.521391	60.395188
2200.143003	84.096015	60.400193
2198.897494	82.001094	60.405198
2198.871467	76.558785	60.410202
2198.516445	83.680702	60.415207
2198.355895	73.154087	60.420212
2197.310138	84.335436	60.425217
2196.312522	85.411951	60.430222
2195.540436	78.852673	60.435226
2195.104947	87.603557	60.440231
2194.923219	79.902827	60.445236
2193.561998	80.758510	60.450241
2192.797880	84.921688	60.455246
2192.451219	78.745163	60.460250
2191.539079	83.942566	60.465255
2191.517055	83.622673	60.470260
2190.538041	80.716811	60.475265
2189.545756	90.792087	60.480270
2189.160515	85.767249	60.485274
2188.326789	85.423549	60.490279
2188.362994	78.347104	60.495284
2187.006495	80.223522	60.500289
2186.441298	84.499122	60.505294
2185.760349	77.637692	60.510298
2185.349595	79.261580	60.515303
2184.743261	71.134938	60.520308
2183.738383	78.774952	60.525313
2182.860772	75.085594	60.530318
2182.682045	75.746151	60.535322
2181.833770	76.493979	60.540327
2181.609746	71.132112	60.545332
2180.202085	70.110154	60.550337
2179.396692	83.719382	60.555342
2179.189089	74.961673	60.560346
2178.771737	84.495740	60.565351
2178.374967	68.764855	60.570356
2177.351488	82.428353	60.575361
2176.432352	80.745366	60.580366
2176.051950	75.076308	60.585370
2175.143276	83.166038	60.590375
2174.833969	69.642482	60.595380
2173.565637	81.466216	60.600385
2172.767803	77.504673	60.605390
2172.414381	80.653831	60.610394
2171.812292	86.828831	60.615399
2171.802595	68.159353	60.620404
2171.287179	82.346595	60.625409
2170.032741	82.152612	60.630414
2169.220963	76.320892	60.635418
2168.367553	75.945038	60.640423
2168.160558	73.417917	60.645428
2167.099655	81.293691	60.650433
2166.065093	82.095487	60.655438
2165.937526	73.023709	60.660442
2165.444709	80.632989	60.665447
2164.813484	79.030233	60.670452
2164.725184	82.196020	60.675457
2163.612939	73.791577	60.680462
2162.801241	76.796489	60.685466
2161.915887	91.552253	60.690471
2161.605534	72.271060	60.695476
2160.604904	81.195960	60.700481
2159.866864	80.251317	60.705486
2159.518204	79.545200	60.710490
2158.798483	85.053896	60.715495
2158.612849	78.300777	60.720500
2157.700394	82.195259	60.725505
2157.005275	80.750268	60.730510
2156.449784	77.992234	60.735514
2154.935253	84.131847	60.740519
2154.500462	74.538292	60.745524
2153.693022	85.414817	60.750529
2153.087057	84.016154	60.755534
2153.018835	79.866279	60.760538
2152.483195	77.197610	60.765543
2151.806893	71.747710	60.770548
2150.483067	78.653623	60.775553
2149.822908	77.364490	60.780558
2149.487987	78.886992	60.785562
2149.160942	84.685753	60.790567
2148.317647	73.334897	60.795572
2147.124704	77.287614	60.800577
2146.552941	79.695330	60.805582
2146.353221	77.609054	60.810586
2145.765931	81.015704	60.815591
2145.037951	78.531505	60.820596
2143.782448	79.890547	60.825601
2143.094310	84.235333	60.830606
2142.771579	79.705055	60.835610
2142.189982	86.255089	60.840615
2141.874033	76.233067	60.845620
2141.506382	78.579427	60.850625
2140.160828	80.102682	60.855630
2139.750452	75.143334	60.860634
2139.005942	84.773221	60.865639
2138.536342	78.217877	60.870644
2137.166691	91.241538	60.875649
2136.837771	85.974582	60.880654
2136.089679	80.788398	60.885658
2135.679120	80.171419	60.890663
2135.320818	83.201813	60.895668
2133.831623	80.220200	60.900673
2133.102410	90.452584	60.905678
2132.739158	86.808283	60.910682
2132.225038	87.439365	60.915687
2131.727337	77.132652	60.920692
2131.447289	89.971929	60.925697
2130.662704	78.116841	60.930702
2129.967122	77.038630	60.935706
2129.229635	79.730470	60.940711
2128.256520	74.613960	60.945716
2127.226584	80.395574	60.950721
2126.640786	76.850520	60.955726
2126.433777	83.571346	60.960730
2125.847482	82.565624	60.965735
2125.256432	81.312435	60.970740
2124.873051	84.041210	60.975745
2123.878336	85.025665	60.980750
2123.096912	80.665417	60.985754
2122.425072	86.116587	60.990759
2121.983135	80.416218	60.995764
2120.960546	75.360273	61.000769
2119.927520	78.996313	61.005774
2119.675713	77.514189	61.010778
2118.857150	88.773131	61.015783
2118.614749	77.254772	61.020788
2118.128258	83.404870	61.025793
2117.244515	81.202702	61.030798
2116.620420	78.683767	61.035802
2115.705058	93.851623	61.040807
2115.396096	83.521312	61.045812
2114.502192	94.141458	61.050817
2113.434898	89.220653	61.055822
2113.284896	77.977796	61.060826
2112.468148	84.341874	61.065831
2112.200901	75.799630	61.070836
2111.186078	85.311548	61.075841
2110.014809	81.087057	61.080846
2109.775398	82.963081	61.085850
2108.869241	84.070939	61.090855
2109.017432	77.945178	61.095860
2108.346014	77.403211	61.100865
2106.911162	84.372332	61.105870
2106.693019	81.092411	61.110874
2105.867503	86.279351	61.115879
2105.583167	79.094715	61.120884
2104.314279	77.955492	61.125889
2103.511830	74.136457	61.130894
2103.297308	67.645648	61.135898
2102.471890	85.183810	61.140903
2102.241259	76.525966	61.145908
2101.542521	74.958449	61.150913
2100.611113	81.732124	61.155918
2099.663691	72.345467	61.160922
2099.125100	80.859385	61.165927
2099.148562	78.727044	61.170932
2098.471040	82.869104	61.175937
2097.009899	81.978283	61.180942
2096.902784	78.939101	61.185946
2096.293143	86.546262	61.190951
2095.394094	83.787789	61.195956
2094.399862	76.334591	61.200961
2093.568602	76.612172	61.205966
2093.601991	70.536443	61.210970
2093.060193	80.695321	61.215975
2092.065250	73.769989	61.220980
2090.804862	78.524881	61.225985
2090.074694	84.051157	61.230990
2089.849386	74.076797	61.235994
2089.455939	83.495461	61.240999
2089.209077	75.796807	61.246004
2088.726367	79.248334	61.251009
2087.483194	85.660483	61.256014
2087.295312	83.557975	61.261018
2086.078962	86.450539	61.266023
2085.080172	86.707041	61.271028
2084.437944	87.436220	61.276033
2083.753528	88.655361	61.281038
2083.630232	76.522580	61.286042
2082.955980	77.657880	61.291047
2082.680663	78.409957	61.296052
2081.347692	65.957136	61.301057
2080.586956	75.562954	61.306062
2080.510660	72.913225	61.311066
2079.837114	81.258391	61.316071
2078.743566	83.280115	61.321076
2077.646898	76.184693	61.326081
2076.949063	75.492913	61.331086
2077.010166	74.411595	61.336090
2076.291281	82.366638	61.341095
2075.583078	85.725688	61.346100
2074.676574	85.013943	61.351105
2073.842722	93.645079	61.356110
2072.962743	92.372239	61.361114
2072.589006	86.643631	61.366119
2072.320724	86.157447	61.371124
2071.970703	86.947960	61.376129
2071.289020	94.868226	61.381134
2070.702975	80.781775	61.386138
2070.077750	90.739016	61.391143
2068.879134	80.459047	61.396148
2068.082023	86.440443	61.401153
2067.387522	88.689166	61.406158
2066.803538	85.513664	61.411162
2066.297704	87.065405	61.416167
2066.006438	87.555353	61.421172
2064.854924	91.169435	61.426177
2063.750017	88.092113	61.431182
2063.054742	81.007770	61.436186
2063.050030	90.853348	61.441191
2062.621504	79.627350	61.446196
2062.013814	80.311942	61.451201
2060.909502	96.124728	61.456206
2060.408253	83.463325	61.461210
2060.146050	92.263120	61.466215
2059.033306	78.419916	61.471220
2057.931549	85.852316	61.476225
2057.358003	84.725215	61.481230
2057.051099	83.657108	61.486234
2056.255156	98.150883	61.491239
2055.841999	86.990144	61.496244
2055.509826	92.539136	61.501249
2054.347738	88.534921	61.506254
2054.459311	79.827627	61.511258
2053.347256	87.674668	61.516263
2052.169645	77.563213	61.521268
2051.515389	78.462210	61.526273
2050.694107	82.618600	61.531278
2050.556534	80.245789	61.536282
2049.818208	79.736589	61.541287
2049.558983	78.294026	61.546292
2048.579326	81.605960	61.551297
2047.610036	85.904506	61.556302
2047.545450	73.715114	61.561306
2046.220473	79.821141	61.566311
2045.308954	81.657004	61.571316
2044.964034	84.837869	61.576321
2044.427965	78.019183	61.581326
2043.691648	71.910911	61.586330
2043.273896	87.517835	61.591335
2043.091775	74.079517	61.596340
2041.592158	84.588144	61.601345
2040.689647	80.099815	61.606350
2040.747662	74.688928	61.611354
2040.044941	91.489294	61.616359
2039.241027	84.147626	61.621364
2038.014689	83.282182	61.626369
2037.322455	88.663034	61.631374
2037.400702	76.004752	61.636378
2036.535138	84.250930	61.641383
2035.995078	79.709288	61.646388
2035.647224	81.529655	61.651393
2034.549256	86.260724	61.656398
2034.085517	78.106560	61.661402
2033.401169	85.411118	61.666407
2032.623572	87.241444	61.671412
2031.769140	84.243650	61.676417
2030.818262	82.319024	61.681422
2030.277010	87.140780	61.686426
2029.576767	85.745629	61.691431
2029.567373	87.540075	61.696436
2029.079024	86.968383	61.701441
2028.152332	90.859398	61.706446
2027.588067	76.132946	61.711450
2026.708791	82.058927	61.716455
2026.374934	80.841491	61.721460
2024.877545	81.289077	61.726465
2024.009791	84.760683	61.731470
2023.818462	85.304194	61.736474
2022.783756	90.828887	61.741479
2022.605491	86.400615	61.746484
2022.748148	91.070258	61.751489
2021.780726	85.935822	61.756494
2021.091900	85.351057	61.761498
2020.425498	88.859273	61.766503
2019.348788	82.168988	61.771508
2018.574766	79.884914	61.776513
2017.627549	89.117262	61.781518
2017.248808	77.612374	61.786522
2016.785147	94.674995	61.791527
2016.480455	86.143111	61.796532
2015.422800	84.467665	61.801537
2014.310887	95.684824	61.806542
2014.113555	86.386184	61.811546
2013.267596	88.252678	61.816551
2012.928595	90.733481	61.821556
2012.579419	84.822267	61.826561
2011.245562	90.013279	61.831566
2010.907746	82.524393	61.836570
2010.170398	82.308310	61.841575
2009.854016	88.265899	61.846580
2008.878503	82.776023	61.851585
2007.610587	91.271024	61.856590
2007.242401	76.276967	61.861594
2006.817557	90.521737	61.866599
2006.654399	88.656573	61.871604
2005.909302	86.032829	61.876609
2004.705299	94.657816	61.881614
2004.699595	81.062615	61.886618
2003.940451	88.803113	61.891623
2002.937692	91.762574	61.896628
2002.525827	83.844662	61.901633
2001.626004	92.249858	61.906638
2000.515421	81.410137	61.911642
1999.674266	85.402571	61.916647
1998.933503	87.024503	61.921652
1998.503470	81.462636	61.926657
1997.571752	84.775063	61.931662
1997.464888	82.010963	61.936666
1996.983194	92.941115	61.941671
1996.921796	87.124353	61.946676
1996.459291	82.505900	61.951681
1994.880165	88.442659	61.956686
1994.750870	84.764668	61.961690
1993.717830	86.954077	61.966695
1992.468135	90.427078	61.971700
1992.018393	92.561313	61.976705
1991.231139	84.178294	61.981710
1991.257673	79.478161	61.986714
1990.875365	89.816990	61.991719
1989.916048	87.470278	61.996724
1988.989831	89.799304	62.001729
1988.153674	90.830868	62.006734
1987.925064	82.324264	62.011738
1987.046530	87.729093	62.016743
1986.154883	84.748725	62.021748
1985.368171	83.436659	62.026753
1984.697963	81.081151	62.031758
1984.514776	75.016028	62.036762
1984.005814	82.045859	62.041767
1983.345286	85.030856	62.046772
1982.547384	78.503671	62.051777
1981.310970	89.173727	62.056782
1981.171465	78.306448	62.061786
1980.620226	86.085589	62.066791
1979.599111	86.113044	62.071796
1979.184997	77.147932	62.076801
1978.077299	84.404522	62.081806
1978.152540	84.446136	62.086810
1977.478319	84.161234	62.091815
1976.692785	82.575820	62.096820
1975.604761	83.285748	62.101825
1974.746409	95.040171	62.106830
1974.764810	77.234701	62.111834
1973.684896	84.863102	62.116839
1972.782314	81.461862	62.121844
1972.013710	77.250630	62.126849
1971.360063	79.185281	62.131854
1971.107773	84.484167	62.136858
1970.486971	86.940548	62.141863
1970.141956	83.508269	62.146868
1970.023240	79.130209	62.151873
1968.642526	84.682914	62.156878
1968.223083	80.023942	62.161882
1967.179681	84.530564	62.166887
1966.115319	79.430489	62.171892
1965.592008	78.802812	62.176897
1965.107316	83.063075	62.181902
1964.588410	82.243600	62.186906
1964.248690	85.865667	62.191911
1963.336293	78.619548	62.196916
1962.632924	80.719805	62.201921
1962.152693	87.946821	62.206926
1961.305342	82.801728	62.211930
1960.574233	82.169338	62.216935
1959.466247	83.309772	62.221940
1958.918033	77.207625	62.226945
1958.051684	89.291426	62.231950
1958.039803	81.257337	62.236954
1957.660018	83.907743	62.241959
1957.347858	79.226868	62.246964
1956.144318	78.470830	62.251969
1955.442438	82.483257	62.256974
1954.832163	78.945968	62.261978
1953.512247	88.730347	62.266983
1952.752113	77.310846	62.271988
1952.453869	77.952382	62.276993
1951.746673	81.459291	62.281998
1951.291574	80.038005	62.287002
1951.005591	80.808491	62.292007
1950.651609	84.216295	62.297012
1950.102931	81.367521	62.302017
1949.327905	85.407462	62.307022
1948.000030	79.055810	62.312026
1947.038045	86.912322	62.317031
1946.246368	82.926874	62.322036
1946.037566	84.237951	62.327041
1945.189404	81.564747	62.332046
1945.030602	82.249137	62.337050
1944.657098	86.269731	62.342055
1943.153664	82.936548	62.347060
1942.515938	76.687486	62.352065
1942.232325	84.977006	62.357070
1941.578364	82.282028	62.362074
1940.462185	84.023449	62.367079
1939.692763	81.332829	62.372084
1939.485933	76.590124	62.377089
1938.733534	88.348917	62.382094
1938.723203	76.187756	62.387098
1937.731121	85.109242	62.392103
1936.511880	84.127350	62.397108
1936.312192	76.179077	62.402113
1935.705012	85.854950	62.407118
1935.192749	78.817481	62.412122
1933.820217	86.930535	62.417127
1932.807121	88.712348	62.422132
1932.932568	81.385004	62.427137
1932.562929	88.572576	62.432142
1932.201697	81.969910	62.437146
1930.748421	77.833578	62.442151
1929.870336	84.904057	62.447156
1929.775288	87.609962	62.452161
1929.222850	89.173634	62.457166
1928.461280	80.161789	62.462170
1927.605168	83.502342	62.467175
1926.795476	87.590451	62.472180
1926.559954	74.858366	62.477185
1925.320000	83.107022	62.482190
1924.308616	79.451259	62.487194
1923.735922	82.993186	62.492199
1923.010327	79.733383	62.497204
1922.650923	77.755750	62.502209
1922.240959	75.161530	62.507214
1922.185396	68.719334	62.512218
1921.455562	78.043568	62.517223
1920.644497	87.813135	62.522228
1919.941205	77.409405	62.527233
1918.997808	80.225701	62.532238
1918.660550	73.198956	62.537242
1917.520976	86.876804	62.542247
1916.481549	82.547708	62.547252
1916.379904	78.664080	62.552257
1915.670746	83.244971	62.557262
1915.422052	83.530282	62.562266
1914.353615	79.868097	62.567271
1913.373223	83.737919	62.572276
1913.279499	79.755046	62.577281
1912.509544	80.712535	62.582286
1912.195063	83.711756	62.587290
1910.991744	83.139631	62.592295
1909.952198	80.017614	62.597300
1909.508466	73.506039	62.602305
1909.125253	78.665090	62.607310
1908.888598	72.055724	62.612314
1907.471660	72.142619	62.617319
1906.443341	77.858855	62.622324
1905.814345	75.003698	62.627329
1905.615125	78.051092	62.632334
1905.632898	71.149527	62.637338
1904.982050	77.286299	62.642343
1903.752908	69.044429	62.647348
1903.110402	72.831973	62.652353
1902.152895	83.313800	62.657358
1902.323816	75.451333	62.662362
1901.153902	78.508875	62.667367
1899.858121	81.270596	62.672372
1899.678644	72.058132	62.677377
1899.035739	78.170652	62.682382
1899.012443	73.680752	62.687386
1898.474533	79.107837	62.692391
1897.548684	71.605497	62.697396
1896.749832	80.103944	62.702401
1896.174182	78.296724	62.707406
1895.384703	71.307481	62.712410
1894.699989	78.953539	62.717415
1893.637417	72.655596	62.722420
1893.450971	73.121698	62.727425
1892.430659	68.846576	62.732430
1891.662903	72.834752	62.737434
1891.346470	82.242997	62.742439
1890.795544	78.530966	62.747444
1890.223110	73.578456	62.752449
1888.715741	82.292059	62.757454
1887.898749	69.205534	62.762458
1887.253702	81.213182	62.767463
1886.679352	76.266526	62.772468
1886.815056	69.621881	62.777473
1886.228410	81.850056	62.782478
1886.261653	72.629622	62.787482
1885.124880	80.334862	62.792487
1884.125528	79.657588	62.797492
1883.510029	77.669694	62.802497
1882.115354	76.767169	62.807502
1881.466450	73.203346	62.812506
1880.837102	69.955506	62.817511
1880.325460	74.668783	62.822516
1880.183807	73.893721	62.827521
1879.322343	73.779413	62.832526
1879.216340	71.837772	62.837530
1878.655903	77.087140	62.842535
1877.394346	75.896590	62.847540
1877.246279	71.811706	62.852545
1876.459927	82.137942	62.857550
1875.703505	70.589153	62.862554
1874.990098	73.504260	62.867559
1873.770010	76.282639	62.872564
1872.987658	74.339477	62.877569
1872.292460	74.766702	62.882574
1871.704449	72.866474	62.887578
1871.360882	77.794935	62.892583
1870.927146	71.250079	62.897588
1870.809157	67.242943	62.902593
1869.786710	78.285724	62.907598
1868.693697	78.832718	62.912602
1868.049948	70.765829	62.917607
1867.537001	80.988844	62.922612
1867.294242	74.807615	62.927617
1865.650511	71.671744	62.932622
1865.096095	78.460677	62.937626
1864.692657	82.920192	62.942631
1864.322681	78.680254	62.947636
1863.712373	84.542870	62.952641
1862.339750	80.151586	62.957646
1861.783163	78.510839	62.962650
1861.261325	78.601709	62.967655
1860.566956	87.064523	62.972660
1860.602789	76.018061	62.977665
1860.123441	81.328161	62.982670
1859.321519	81.689571	62.987674
1858.245933	77.287732	62.992679
1857.507251	83.640844	62.997684
1857.377685	74.125779	63.002689
1855.951178	78.295343	63.007694
1855.377414	76.410440	63.012698
1854.696887	75.261406	63.017703
1854.474452	82.816538	63.022708
1853.917408	79.314761	63.027713
1852.649185	78.604154	63.032718
1852.121223	77.250605	63.037722
1851.646274	74.310682	63.042727
1851.070135	76.852980	63.047732
1850.798030	69.125523	63.052737
1849.476626	75.391230	63.057742
1848.586307	74.707150	63.062746
1848.248406	79.124664	63.067751
1847.554582	84.083053	63.072756
1847.537240	81.344302	63.077761
1846.633060	81.933200	63.082766
1845.663309	81.623880	63.087770
1845.210127	83.272021	63.092775
1844.540013	85.416336	63.097780
1843.232091	82.568794	63.102785
1842.256423	89.471250	63.107790
1842.042061	73.003870	63.112794
1841.748163	84.964864	63.117799
1841.185638	84.889809	63.122804
1841.203382	75.758078	63.127809
1839.533729	83.440026	63.132814
1838.866274	75.276543	63.137818
1838.238491	79.989563	63.142823
1837.738155	82.960587	63.147828
1837.600745	75.481257	63.152833
1836.374606	79.544311	63.157838
1835.660739	80.874304	63.162842
1835.094698	75.149424	63.167847
1834.487899	84.578136	63.172852
1834.457008	78.419474	63.177857
1833.019452	76.291981	63.182862
1832.249698	69.192409	63.187866
1831.556423	76.482712	63.192871
1831.192565	85.565926	63.197876
1830.901689	74.122621	63.202881
1829.826495	80.540806	63.207886
1829.523377	80.691360	63.212890
1828.733900	71.618006	63.217895
1827.659611	74.903138	63.222900
1826.648548	70.508822	63.227905
1825.890124	75.894299	63.232910
1825.787660	71.790564	63.237914
1825.273403	80.854509	63.242919
1824.309064	76.923100	63.247924
1824.704510	78.643935	63.252929
1823.473924	80.187856	63.257934
1822.828881	77.473214	63.262938
1822.162832	81.429393	63.267943
1820.929785	86.483594	63.272948
1820.429473	78.079946	63.277953
1819.631229	84.776395	63.282958
1819.054842	79.309855	63.287962
1818.531804	84.150609	63.292967
1818.562668	84.587429	63.297972
1817.561263	83.593163	63.302977
1816.383177	89.761338	63.307982
1815.661253	79.629625	63.312986
1815.448341	78.973331	63.317991
1814.601865	85.765661	63.322996
1814.126985	83.715035	63.328001
1812.826688	82.661782	63.333006
1812.342860	87.945021	63.338010
1812.172066	81.363077	63.343015
1811.507189	82.466805	63.348020
1810.713668	79.395478	63.353025
1809.216929	90.523762	63.358030
1808.943242	82.010686	63.363034
1808.852917	80.765020	63.368039
1808.290391	89.983670	63.373044
1808.138218	81.567035	63.378049
1806.770263	82.288577	63.383054
1806.213724	79.329856	63.388058
1805.307869	77.217186	63.393063
1804.652488	82.738582	63.398068
1804.068599	78.474858	63.403073
1802.895932	77.207542	63.408078
1802.800873	80.024362	63.413082
1802.288803	82.350448	63.418087
1801.931966	92.975822	63.423092
1800.555806	83.871009	63.428097
1799.848158	88.442574	63.433102
1799.180145	79.601457	63.438106
1798.876667	81.383454	63.443111
1798.345018	85.725572	63.448116
1797.967182	80.611890	63.453121
1796.576874	79.680616	63.458126
1795.862145	80.402891	63.463130
1795.651055	75.848026	63.468135
1795.046062	84.915656	63.473140
1794.404327	78.592310	63.478145
1793.386701	79.197075	63.483150
1793.067699	78.628799	63.488154
1792.599210	80.770595	63.493159
1791.064656	75.114330	63.498164
1790.579380	75.638670	63.503169
1790.165306	78.902029	63.508174
1789.658057	67.828506	63.513178
1789.368079	72.072037	63.518183
1787.968580	83.101185	63.523188
1787.677628	74.911188	63.528193
1786.628765	88.685231	63.533198
1786.391045	87.001382	63.538202
1785.731188	77.684814	63.543207
1784.519692	81.917077	63.548212
1783.958953	73.935866	63.553217
1783.195288	77.169438	63.558222
1782.923517	68.199353	63.563226
1782.483911	77.939310	63.568231
1781.858747	83.459091	63.573236
1781.044805	75.685800	63.578241
1780.150129	81.814960	63.583246
1779.684620	79.449327	63.588250
1779.311270	75.644170	63.593255
1778.060101	79.262720	63.598260
1777.502443	77.200606	63.603265
1776.925868	78.160156	63.608270
1776.584608	76.457710	63.613274
1776.021654	77.046261	63.618279
1774.722625	81.874136	63.623284
1774.028837	77.847896	63.628289
1773.599397	80.708113	63.633294
1773.206936	78.013417	63.638298
1772.668408	74.568877	63.643303
1771.567712	83.815265	63.648308
1771.219405	79.702283	63.653313
1770.349467	89.103393	63.658318
1770.094044	79.373038	63.663322
1769.310958	78.228933	63.668327
1767.957966	87.081930	63.673332
1767.204907	82.715319	63.678337
1766.766586	81.383546	63.683342
1766.386551	87.059536	63.688346
1766.453710	77.056103	63.693351
1765.059708	86.850815	63.698356
1764.185578	80.163044	63.703361
1763.786098	87.566106	63.708366
1763.093954	86.651168	63.713370
1762.988054	79.477492	63.718375
1761.683301	88.465127	63.723380
1760.929784	79.937057	63.728385
1760.066704	75.582564	63.733390
1759.746777	86.491341	63.738394
1759.472159	73.880052	63.743399
1758.653376	80.951845	63.748404
1757.836860	72.178781	63.753409
1757.223314	81.369447	63.758414
1756.798462	77.944141	63.763418
1755.673081	78.957729	63.768423
1754.646330	80.565863	63.773428
1754.275011	80.512572	63.778433
1753.692383	77.327807	63.783438
1753.235805	79.323494	63.788442
1753.241850	78.002133	63.793447
1752.051122	86.832895	63.798452
1751.290884	81.592815	63.803457
1750.939231	82.000746	63.808462
1750.361373	84.745839	63.813466
1749.186365	75.608211	63.818471
1748.481498	79.697348	63.823476
1748.294118	83.497029	63.828481
1747.084209	79.140701	63.833486
1745.521220	80.865457	63.838490
1745.740919	68.880486	63.843495
1745.513064	72.022381	63.848500
1744.542035	67.165729	63.853505
1744.392164	75.197100	63.858510
1743.376783	78.233362	63.863514
1742.695042	76.306952	63.868519
1742.068589	81.676962	63.873524
1741.923763	74.141677	63.878529
1741.173189	76.683043	63.883534
1739.841782	77.238485	63.888538
1739.332499	65.938753	63.893543
1738.646385	80.365956	63.898548
1738.215451	69.603055	63.903553
1736.997189	75.292211	63.908558
1736.442408	82.237521	63.913562
1735.939528	73.664997	63.918567
1735.120638	74.827848	63.923572
1735.212730	69.123002	63.928577
1734.513029	73.145731	63.933582
1733.352234	57.546093	63.938586
1733.144805	72.621218	63.943591
1732.077193	74.100958	63.948596
1731.240879	71.647997	63.953601
1730.719791	77.058790	63.958606
1729.992161	73.450043	63.963610
1729.722321	68.466704	63.968615
1729.157202	72.629820	63.973620
1727.934809	66.555446	63.978625
1727.189180	65.814659	63.983630
1726.478920	63.240267	63.988634
1726.442873	65.815680	63.993639
1725.349823	69.994132	63.998644
1724.029949	67.962584	64.003649
1723.630842	72.788449	64.008654
1723.855156	73.058356	64.013658
1722.860141	64.488735	64.018663
1722.479698	72.211019	64.023668
1721.900244	62.750064	64.028673
1720.837802	59.810822	64.033678
1719.815431	71.851448	64.038682
1719.471372	72.608988	64.043687
1719.086248	74.334698	64.048692
1718.868784	70.756285	64.053697
1717.663763	71.088800	64.058702
1716.906935	72.379186	64.063706
1716.303263	68.752390	64.068711
1715.006159	80.712144	64.073716
1714.400491	70.253872	64.078721
1713.851515	74.325810	64.083726
1712.847177	76.203657	64.088730
1713.022105	81.542327	64.093735
1712.343223	77.758669	64.098740
1712.198163	69.724898	64.103745
1711.668242	71.658534	64.108750
1710.058625	69.286191	64.113754
1709.745048	64.272446	64.118759
1709.424991	71.181142	64.123764
1708.560854	67.173013	64.128769
1707.187746	70.987697	64.133774
1706.223679	65.550809	64.138778
1706.031575	69.172092	64.143783
1705.648271	71.377075	64.148788
1705.431983	68.021480	64.153793
1704.102686	67.909889	64.158798
1703.557529	69.759294	64.163802
1703.009102	68.318479	64.168807
1702.418408	77.437341	64.173812
1702.034068	70.145539	64.178817
1700.817976	74.643064	64.183822
1699.731695	74.614227	64.188826
1699.668178	64.363575	64.193831
1699.035235	67.575575	64.198836
1698.677283	64.376453	64.203841
1698.386932	67.698772	64.208846
1697.231312	69.828287	64.213850
1696.698721	62.895789	64.218855
1695.739839	79.073669	64.223860
1694.582631	72.315152	64.228865
1693.896497	70.080831	64.233870
1693.288585	67.736420	64.238874
1693.101530	62.111712	64.243879
1692.525579	71.335017	64.248884
1692.406619	66.387046	64.253889
1691.473222	71.553405	64.258894
1690.194461	67.583072	64.263898
1690.217703	71.653801	64.268903
1689.412724	76.054535	64.273908
1688.295662	68.880616	64.278913
1687.835048	72.341407	64.283918
1686.668091	77.639309	64.288922
1686.510975	69.552344	64.293927
1686.002825	79.841637	64.298932
1685.521128	69.457682	64.303937
1684.484093	73.650239	64.308942
1683.730209	72.544176	64.313946
1683.343201	72.343977	64.318951
1682.621584	74.176608	64.323956
1681.824497	65.942588	64.328961
1680.859501	69.670864	64.333966
1680.230441	74.047811	64.338970
1680.134227	69.694343	64.343975
1679.573662	75.432406	64.348980
1679.031359	72.540344	64.353985
1677.925122	79.375160	64.358990
1676.998305	72.863395	64.363994
1676.836815	73.719165	64.368999
1675.737710	81.611400	64.374004
1675.010095	73.496536	64.379009
1674.101959	79.202501	64.384014
1673.718022	76.281366	64.389018
1673.005276	74.994588	64.394023
1672.481365	74.661507	64.399028
1672.305722	64.551224	64.404033
1671.665447	72.950311	64.409038
1670.946304	77.771735	64.414042
1670.631170	67.456382	64.419047
1669.283817	70.546304	64.424052
1668.396743	80.314280	64.429057
1667.752791	77.126995	64.434062
1667.171125	75.806735	64.439066
1666.918766	73.294515	64.444071
1666.139676	81.708282	64.449076
1665.477170	76.978054	64.454081
1664.376349	77.223280	64.459086
1664.096461	69.582834	64.464090
1663.570564	74.277641	64.469095
1663.036422	82.211353	64.474100
1661.641472	80.827377	64.479105
1660.945922	77.241177	64.484110
1660.574166	74.981879	64.489114
1660.610336	72.634224	64.494119
1659.596498	78.065001	64.499124
1658.995477	61.932644	64.504129
1657.954544	75.207189	64.509134
1656.836004	79.532905	64.514138
1656.893280	70.141810	64.519143
1656.626180	80.771943	64.524148
1655.396591	83.374370	64.529153
1654.605205	77.592954	64.534158
1653.818811	80.337425	64.539162
1653.765200	78.182758	64.544167
1653.244261	75.407827	64.549172
1652.113340	75.498345	64.554177
1651.532988	76.060676	64.559182
1650.722861	84.191216	64.564186
1650.641459	76.292602	64.569191
1649.474392	79.725084	64.574196
1648.573608	81.229580	64.579201
1648.012322	78.786014	64.584206
1647.692078	86.176305	64.589210
1647.480712	73.649341	64.594215
1645.643269	78.154526	64.599220
1645.390081	72.700602	64.604225
1644.853245	74.326362	64.609230
1644.325613	73.568808	64.614234
1644.120719	68.820670	64.619239
1642.747896	79.389766	64.624244
1642.309242	71.532159	64.629249
1641.668649	78.384397	64.634254
1640.830862	79.427738	64.639258
1640.526735	69.003143	64.644263
1639.571049	80.289507	64.649268
1639.238432	72.056928	64.654273
1638.304090	75.016973	64.659278
1637.038210	81.547550	64.664282
1636.421092	70.398917	64.669287
1635.720923	83.493188	64.674292
1635.820152	69.609713	64.679297
1635.146915	76.493588	64.684302
1634.635334	83.503744	64.689306
1634.496251	74.147434	64.694311
1633.158518	81.645925	64.699316
1632.479619	77.765971	64.704321
1631.723778	71.094308	64.709326
1630.765620	87.325360	64.714330
1630.059052	79.231769	64.719335
1629.263182	78.105663	64.724340
1628.951696	71.426245	64.729345
1628.292524	74.575245	64.734350
1627.731041	84.402766	64.739354
1627.555960	71.042660	64.744359
1626.469761	80.712484	64.749364
1625.698143	66.947251	64.754369
1625.307956	78.132894	64.759374
1624.450681	80.447413	64.764378
1623.511789	69.805407	64.769383
1622.966312	75.568915	64.774388
1622.179816	70.711106	64.779393
1622.027679	72.137224	64.784398
1621.567435	79.326085	64.789402
1620.469592	65.999165	64.794407
1619.579004	72.270921	64.799412
1619.135278	73.232619	64.804417
1618.757431	78.349311	64.809422
1617.705817	81.436398	64.814426
1617.310799	69.013894	64.819431
1616.425433	80.569266	64.824436
1615.851404	71.963154	64.829441
1615.526658	73.488676	64.834446
1614.102141	71.582430	64.839450
1613.764036	75.655391	64.844455
1612.852344	82.677573	64.849460
1612.542186	75.077442	64.854465
1612.238024	70.032097	64.859470
1611.125392	77.783371	64.864474
1610.424476	71.787546	64.869479
1609.628984	80.317012	64.874484
1609.444396	73.792319	64.879489
1608.920215	70.544287	64.884494
1607.715128	77.432342	64.889498
1607.284933	66.177918	64.894503
1606.585882	79.116080	64.899508
1605.958225	74.433976	64.904513
1605.542778	69.811080	64.909518
1604.214157	66.810053	64.914522
1603.686176	66.917393	64.919527
1603.066473	75.168890	64.924532
1603.124522	65.392818	64.929537
1602.632224	72.653080	64.934542
1600.985946	73.624795	64.939546
1600.885756	63.196887	64.944551
1600.338278	72.072705	64.949556
1599.344725	75.569050	64.954561
1598.244202	70.746039	64.959566
1597.170668	72.634958	64.964570
1596.736640	65.247077	64.969575
1596.328669	76.721538	64.974580
1596.021565	75.487716	64.979585
1595.903004	67.424952	64.984590
1595.198011	72.097913	64.989594
1594.239545	63.685489	64.994599
1593.233266	79.138881	64.999604
1592.748274	79.127161	65.004609
1592.220552	76.324979	65.009614
1590.955402	70.084681	65.014618
1590.537604	74.812306	65.019623
1589.449557	74.961813	65.024628
1589.182957	83.645101	65.029633
1589.078607	77.612314	65.034638
1588.861219	72.677641	65.039642
1588.034385	72.757184	65.044647
1587.315183	74.884664	65.049652
1586.461053	71.971773	65.054657
1585.354850	77.730590	65.059662
1584.869558	76.749095	65.064666
1584.322858	70.679122	65.069671
1583.030402	78.237763	65.074676
1582.417059	72.089989	65.079681
1582.102755	73.294793	65.084686
1581.456950	77.935918	65.089690
1580.878438	71.560351	65.094695
1580.215874	71.340215	65.099700
1579.320606	74.410813	65.104705
1578.594629	63.099258	65.109710
1578.006605	68.846364	65.114714
1577.640351	72.926511	65.119719
1577.099590	73.727590	65.124724
1576.204545	80.885867	65.129729
1575.480941	72.381146	65.134734
1574.616520	77.790706	65.139738
1574.405005	65.902838	65.144743
1573.849271	72.497802	65.149748
1572.880106	71.453861	65.154753
1572.080345	70.133045	65.159758
1571.368437	79.561589	65.164762
1571.082062	68.677277	65.169767
1570.516039	65.889155	65.174772
1569.633659	75.195299	65.179777
1568.703076	68.023843	65.184782
1567.555735	79.028813	65.189786
1567.765246	72.942710	65.194791
1567.249632	79.980002	65.199796
1566.494074	69.891612	65.204801
1565.835191	74.594973	65.209806
1565.111496	72.106981	65.214810
1565.056372	69.396417	65.219815
1563.703653	78.160584	65.224820
1562.860663	75.238290	65.229825
1562.414027	67.281807	65.234830
1561.699822	70.249186	65.239834
1561.471337	75.492677	65.244839
1559.825142	70.873585	65.249844
1559.158892	74.433521	65.254849
1558.810197	72.769076	65.259854
1558.951590	78.098076	65.264858
1557.909617	70.020462	65.269863
1556.751238	74.058157	65.274868
1555.961397	68.739113	65.279873
1555.617667	67.618136	65.284878
1554.853370	78.580052	65.289882
1555.126905	64.170994	65.294887
1553.766144	66.325778	65.299892
1552.987100	66.822655	65.304897
1552.097300	71.361071	65.309902
1551.317075	71.838808	65.314906
1551.034118	63.317104	65.319911
1550.745036	66.134756	65.324916
1549.838445	74.156286	65.329921
1549.387726	71.646841	65.334926
1548.477588	75.215756	65.339930
1547.936277	70.919921	65.344935
1546.675805	68.917333	65.349940
1545.546319	76.422036	65.354945
1545.598505	71.284134	65.359950
1544.759401	74.152502	65.364954
1544.621918	62.074348	65.369959
1544.356765	70.760933	65.374964
1543.936273	73.043733	65.379969
1543.070619	79.091374	65.384974
1542.024015	74.752154	65.389978
1541.232645	69.826120	65.394983
1540.046788	71.064434	65.399988
1539.475177	71.334768	65.404993
1538.686715	69.652435	65.409998
1538.336773	67.673219	65.415002
1538.169600	65.428261	65.420007
1537.684096	72.629731	65.425012
1536.778362	69.694499	65.430017
1536.385930	64.970969	65.435022
1535.320058	72.537808	65.440026
1534.848849	68.796005	65.445031
1533.532528	69.475623	65.450036
1532.993727	76.651087	65.455041
1532.942855	65.411098	65.460046
1532.579247	69.756044	65.465050
1531.906360	70.655920	65.470055
1530.771629	68.595897	65.475060
1529.775649	72.194505	65.480065
1528.536323	64.935381	65.485070
1528.195365	78.029350	65.490074
1527.492871	69.451164	65.495079
1527.141985	72.124271	65.500084
1526.971689	69.558546	65.505089
1526.531491	64.883848	65.510094
1525.623743	72.333629	65.515098
1524.928749	63.452203	65.520103
1523.976049	70.443514	65.525108
1523.489464	68.557157	65.530113
1523.006981	65.019777	65.535118
1521.372418	73.546804	65.540122
1520.878679	65.446029	65.545127
1519.759550	69.048347	65.550132
1519.456267	68.195175	65.555137
1519.115607	59.133904	65.560142
1518.830394	71.814924	65.565146
1518.535012	59.598808	65.570151
1517.975055	63.313045	65.575156
1517.473830	70.789957	65.580161
1516.304876	71.203184	65.585166
1515.659576	68.943351	65.590170
1514.713022	59.971569	65.595175
1513.733481	66.901555	65.600180
1513.245347	67.805339	65.605185
1512.770680	55.072042	65.610190
1512.001560	74.072046	65.615194
1511.625486	60.980439	65.620199
1510.648930	69.267748	65.625204
1509.964598	67.680883	65.630209
1509.441491	63.679558	65.635214
1509.065275	70.497209	65.640218
1508.573132	64.490543	65.645223
1507.533648	67.532940	65.650228
1506.578557	69.842900	65.655233
1506.089954	67.569276	65.660238
1505.702703	66.726135	65.665242
1504.962301	56.634387	65.670247
1504.298350	69.952567	65.675252
1503.286410	61.846940	65.680257
1502.763752	63.593437	65.685262
1502.224074	69.102940	65.690266
1501.910863	61.408622	65.695271
1500.660614	68.621379	65.700276
1500.278692	69.776183	65.705281
1499.639924	62.471122	65.710286
1498.989062	69.594319	65.715290
1498.407313	69.002352	65.720295
1497.917227	71.998482	65.725300
1497.000148	67.427906	65.730305
1496.861494	55.626269	65.735310
1495.250097	70.814161	65.740314
1495.007755	76.682891	65.745319
1494.301426	69.563856	65.750324
1493.911788	67.105935	65.755329
1493.205168	64.755948	65.760334
1492.365375	72.278571	65.765338
1491.614952	61.723559	65.770343
1490.986002	62.139100	65.775348
1489.876032	59.467378	65.780353
1489.269047	60.521762	65.785358
1488.556455	71.809942	65.790362
1488.253757	62.234963	65.795367
1487.504211	63.912930	65.800372
1487.428451	67.630742	65.805377
1487.031503	69.324147	65.810382
1486.026958	70.398421	65.815386
1485.453499	72.602015	65.820391
1484.754479	69.931795	65.825396
1483.622236	75.704952	65.830401
1482.686004	70.665572	65.835406
1481.591473	75.404426	65.840410
1481.434873	73.794342	65.845415
1480.776415	74.000208	65.850420
1480.698409	73.907787	65.855425
1480.387119	71.434878	65.860430
1478.904515	77.748375	65.865434
1478.431274	72.337265	65.870439
1477.963401	73.221400	65.875444
1477.305654	68.220801	65.880449
1476.386264	66.429052	65.885454
1475.262452	63.928642	65.890458
1475.022415	64.273278	65.895463
1474.296543	59.557883	65.900468
1473.997795	66.958298	65.905473
1473.580549	68.875826	65.910478
1471.838241	75.146541	65.915482
1471.654611	72.833747	65.920487
1471.378618	62.437132	65.925492
1470.917272	71.719373	65.930497
1470.213507	69.931375	65.935502
1468.876547	77.125826	65.940506
1468.517030	67.164670	65.945511
1467.873887	71.761926	65.950516
1467.286408	73.662805	65.955521
1466.984592	68.154466	65.960526
1465.353325	74.779186	65.965530
1464.883169	76.234477	65.970535
1464.599170	68.496478	65.975540
1464.038850	64.569816	65.980545
1463.920037	64.139396	65.985550
1462.377943	71.856434	65.990554
1462.020171	58.787364	65.995559
1461.497212	64.508338	66.000564
1460.606526	68.401156	66.005569
1459.996539	71.050722	66.010574
1458.648289	70.712711	66.015578
1458.825351	68.692641	66.020583
1458.163876	67.789076	66.025588
1457.544788	72.310773	66.030593
1456.445315	61.367903	66.035598
1455.661009	70.166630	66.040602
1455.411079	68.160041	66.045607
1454.589150	75.429754	66.050612
1454.009845	66.543936	66.055617
1453.611798	69.033284	66.060622
1452.561554	78.450666	66.065626
1452.499054	61.917131	66.070631
1451.503457	72.004466	66.075636
1450.536168	78.268056	66.080641
1450.075175	71.417287	66.085646
1449.205711	73.143811	66.090650
1448.949059	66.004265	66.095655
1448.660160	63.234646	66.100660
1447.030826	64.724142	66.105665
1446.776514	71.776705	66.110670
1445.700446	72.823362	66.115674
1445.629669	70.036538	66.120679
1445.129860	68.304025	66.125684
1443.855429	75.307391	66.130689
1443.395961	70.551136	66.135694
1442.253917	71.334757	66.140698
1442.004255	66.699691	66.145703
1441.639288	64.704109	66.150708
1440.493836	74.794204	66.155713
1440.182836	64.657783	66.160718
1439.285056	72.512032	66.165722
1438.861076	66.674886	66.170727
1438.648497	66.191045	66.175732
1437.482071	69.123742	66.180737
1437.052222	68.795901	66.185742
1435.751709	63.013266	66.190746
1435.685042	64.781582	66.195751
1435.245088	66.369067	66.200756
1434.162456	68.471538	66.205761
1433.947659	61.658369	66.210766
1433.092057	78.040404	66.215770
1432.613625	72.970042	66.220775
1431.229758	71.907906	66.225780
1430.411606	78.367013	66.230785
1430.074476	74.680822	66.235790
1429.522465	80.976356	66.240794
1429.201079	67.455813	66.245799
1428.034340	75.514779	66.250804
1427.189874	74.919238	66.255809
1427.094217	62.938938	66.260814
1426.436270	69.174051	66.265818
1425.833407	68.598338	66.270823
1424.741417	70.922665	66.275828
1423.879495	72.780922	66.280833
1423.356671	70.674210	66.285838
1423.008586	72.810814	66.290842
1422.832261	65.660680	66.295847
1422.068116	69.290671	66.300852
1421.064037	70.746175	66.305857
1420.941880	65.061045	66.310862
1419.535186	75.245987	66.315866
1418.366495	73.923612	66.320871
1418.039032	75.886958	66.325876
1417.160823	74.210139	66.330881
1417.061734	73.458596	66.335886
1416.542483	74.076017	66.340890
1416.174081	71.050414	66.345895
1414.928697	60.914866	66.350900
1413.899743	77.302100	66.355905
1413.864913	71.037177	66.360910
1413.015345	72.191906	66.365914
1412.758951	73.008270	66.370919
1411.673981	76.503714	66.375924
1410.840498	80.640555	66.380929
1410.478193	65.306579	66.385934
1410.133662	74.036745	66.390938
1409.088021	77.460329	66.395943
1408.267228	64.275134	66.400948
1407.259811	70.963207	66.405953
1407.332866	65.797664	66.410958
1406.627367	65.015716	66.415962
1405.990698	68.016021	66.420967
1404.935074	69.507192	66.425972
1403.970756	72.194521	66.430977
1403.935904	56.007174	66.435982
1403.270674	72.666865	66.440986
1402.905286	67.459533	66.445991
1401.764678	68.714210	66.450996
1400.938196	74.824629	66.456001
1400.529992	64.498416	66.461006
1400.094384	74.681737	66.466010
1399.562744	68.227132	66.471015
1398.719361	64.549449	66.476020
1397.860604	69.844377	66.481025
1397.604098	66.250965	66.486030
1396.262395	72.377736	66.491034
1395.336477	73.485934	66.496039
1394.853617	71.213314	66.501044
1394.619681	67.709587	66.506049
1394.282542	67.211150	66.511054
1393.800867	68.655787	66.516058
1392.441705	68.699777	66.521063
1391.903697	66.997886	66.526068
1391.091950	74.475852	66.531073
1390.971615	65.032691	66.536078
1389.582064	59.453594	66.541082
1388.783894	65.149841	66.546087
1388.445953	65.105863	66.551092
1387.732381	67.113986	66.556097
1387.677023	71.500114	66.561102
1387.255933	71.032232	66.566106
1386.248331	67.846850	66.571111
1385.486862	64.298826	66.576116
1384.470954	74.621740	66.581121
1384.490715	68.697197	66.586126
1383.074443	68.668864	66.591130
1382.518768	68.241782	66.596135
1382.192074	65.803491	66.601140
1381.491014	81.630152	66.606145
1380.717339	63.634358	66.611150
1379.778351	66.080128	66.616154
1379.302321	69.068727	66.621159
1378.536834	66.073603	66.626164
1378.257795	73.019481	66.631169
1377.702778	68.984954	66.636174
1376.514074	64.378407	66.641178
1375.666636	67.319667	66.646183
1375.679323	63.202963	66.651188
1374.833107	68.372199	66.656193
1374.225599	66.415773	66.661198
1373.075769	69.810620	66.666202
1372.582126	62.093524	66.671207
1372.187896	61.819984	66.676212
1371.507117	75.373931	66.681217
1370.906253	66.998639	66.686222
1369.787912	75.477598	66.691226
1369.160637	64.060785	66.696231
1368.713701	71.726161	66.701236
1367.953631	65.925636	66.706241
1368.094395	60.319052	66.711246
1366.624609	73.680443	66.716250
1365.958934	69.788012	66.721255
1365.792352	66.452750	66.726260
1365.158163	65.199150	66.731265
1364.784877	68.837631	66.736270
1363.345777	72.464357	66.741274
1362.859606	64.239559	66.746279
1362.743654	62.268067	66.751284
1361.494174	73.277118	66.756289
1360.604352	65.546134	66.761294
1359.397856	70.281674	66.766298
1359.395388	64.996435	66.771303
1359.288691	66.820154	66.776308
1358.337157	68.597054	66.781313
1357.558042	61.961017	66.786318
1356.711534	65.520249	66.791322
1356.464080	62.943270	66.796327
1356.046224	64.744862	66.801332
1355.025771	61.782731	66.806337
1354.099786	66.989307	66.811342
1353.085960	58.441568	66.816346
1352.497214	66.609615	66.821351
1352.116419	65.089624	66.826356
1351.794320	65.506731	66.831361
1351.592830	59.429813	66.836366
1350.261657	68.479651	66.841370
1349.652002	67.488682	66.846375
1349.228169	61.080369	66.851380
1348.408985	62.013600	66.856385
1347.555125	58.297067	66.861390
1346.686848	65.758263	66.866394
1346.099732	65.294727	66.871399
1345.875473	53.498296	66.876404
1345.430425	70.210286	66.881409
1344.286024	65.703132	66.886414
1343.292173	66.391935	66.891418
1343.217034	62.195535	66.896423
1342.632497	66.576330	66.901428
1341.947595	67.488155	66.906433
1341.413347	57.088408	66.911438
1340.260623	68.377329	66.916442
1339.628368	70.087341	66.921447
1339.143154	59.702092	66.926452
1338.220588	74.495398	66.931457
1337.379649	61.380384	66.936462
1336.999049	61.690670	66.941466
1336.394109	66.048512	66.946471
1336.159941	65.453509	66.951476
1334.929731	60.610144	66.956481
1334.564332	56.092399	66.961486
1333.527456	56.831593	66.966490
1332.906167	62.154950	66.971495
1332.897838	58.065136	66.976500
1332.027671	66.799623	66.981505
1331.332817	64.877497	66.986510
1330.820774	63.444315	66.991514
1330.186583	67.976105	66.996519
1329.333281	65.075755	67.001524
1328.423328	77.131903	67.006529
1328.089972	66.345279	67.011534
1327.350615	62.703880	67.016538
1325.755857	60.506748	67.021543
1325.502315	70.204181	67.026548
1324.662285	70.606931	67.031553
1324.415643	63.981191	67.036558
1323.994139	65.409217	67.041562
1323.660785	64.396215	67.046567
1323.219611	63.173917	67.051572
1322.005523	74.141391	67.056577
1321.388577	65.601503	67.061582
1320.831100	66.141797	67.066586
1319.444773	58.926065	67.071591
1319.134348	57.454818	67.076596
1318.173456	70.619760	67.081601
1318.249818	63.514799	67.086606
1317.610507	69.676863	67.091610
1316.895563	63.319572	67.096615
1316.072515	61.975552	67.101620
1314.976201	71.341623	67.106625
1314.597377	61.770626	67.111630
1314.237900	59.033627	67.116634
1313.153673	68.215267	67.121639
1312.499100	61.926982	67.126644
1311.703628	69.620444	67.131649
1311.632718	63.594988	67.136654
1310.692778	74.301200	67.141658
1309.973648	68.619988	67.146663
1309.113507	66.119084	67.151668
1308.342196	72.867404	67.156673
1308.004594	62.278084	67.161678
1307.438517	65.281707	67.166682
1307.129889	57.125210	67.171687
1306.477677	51.689511	67.176692
1305.337301	55.957443	67.181697
1305.050495	49.535157	67.186702
1304.033724	53.063148	67.191706
1302.959781	57.343787	67.196711
1302.263490	53.529635	67.201716
1302.043111	60.203372	67.206721
1301.776892	57.187132	67.211726
1301.143604	53.886776	67.216730
1299.925083	66.158758	67.221735
1299.155532	60.053178	67.226740
1298.345521	61.363776	67.231745
1298.208336	63.148111	67.236750
1297.934304	60.058212	67.241754
1296.859757	65.286675	67.246759
1296.218726	49.663369	67.251764
1295.509967	60.220264	67.256769
1294.909055	58.017207	67.261774
1294.220096	59.457864	67.266778
1292.780865	60.846577	67.271783
1292.304828	54.273931	67.276788
1291.846078	59.731299	67.281793
1291.832900	54.480663	67.286798
1291.230047	63.748045	67.291802
1290.569043	61.555670	67.296807
1290.023986	50.358485	67.301812
1289.185513	65.046207	67.306817
1288.507830	53.971194	67.311822
1287.182805	64.201773	67.316826
1286.375880	66.058924	67.321831
1286.270747	55.171274	67.326836
1285.377932	62.819035	67.331841
1285.012090	55.453877	67.336846
1284.686765	57.406992	67.341850
1283.752510	60.777185	67.346855
1283.361438	60.466008	67.351860
1282.245371	65.508958	67.356865
1281.388516	65.348965	67.361870
1280.238486	58.121609	67.366874
1280.016058	62.292002	67.371879
1279.334694	53.358572	67.376884
1278.834846	61.257595	67.381889
1278.861465	60.285202	67.386894
1278.056520	61.437838	67.391898
1276.941992	63.713949	67.396903
1276.508365	57.762434	67.401908
1275.716341	66.436576	67.406913
1275.012641	67.453070	67.411918
1273.958801	61.557603	67.416922
1273.073260	65.513904	67.421927
1272.824531	58.607885	67.426932
1272.157351	62.162873	67.431937
1271.732423	53.455136	67.436942
1271.499660	63.217685	67.441946
1270.829361	65.234202	67.446951
1269.946557	58.795929	67.451956
1268.922518	61.955321	67.456961
1268.430920	60.382864	67.461966
1268.069806	64.095839	67.466970
1266.962784	67.069712	67.471975
1266.589839	62.437614	67.476980
1265.755398	71.239015	67.481985
1265.450086	59.779743	67.486990
1264.192942	66.381907	67.491994
1263.321596	62.351820	67.496999
1262.577569	58.884910	67.502004
1261.759125	68.640761	67.507009
1261.922602	65.744767	67.512014
1261.798165	66.987340	67.517018
1261.116314	61.437121	67.522023
1260.281352	57.936834	67.527028
1259.494388	69.091702	67.532033
1258.248550	61.146579	67.537038
1257.399117	64.005699	67.542042
1256.917597	60.417668	67.547047
1256.876797	66.778439	67.552052
1256.078319	71.264154	67.557057
1255.307713	64.275383	67.562062
1254.238973	61.247336	67.567066
1253.473365	54.078118	67.572071
1253.613668	56.480045	67.577076
1252.803472	63.437908	67.582081
1251.747209	58.504001	67.587086
1250.937939	63.728501	67.592090
1250.221808	69.851223	67.597095
1250.044096	63.006070	67.602100
1249.187889	72.435247	67.607105
1248.986511	61.786302	67.612110
1247.726512	54.739224	67.617114
1246.706952	61.927921	67.622119
1246.667951	57.319177	67.627124
1246.258180	70.921849	67.632129
1245.913270	59.727111	67.637134
1244.911487	65.986758	67.642138
1243.892106	73.169903	67.647143
1243.563672	53.026463	67.652148
1242.138570	65.692223	67.657153
1241.480104	59.380147	67.662158
1241.003842	58.898830	67.667162
1240.599919	59.365871	67.672167
1240.356104	54.942186	67.677172
1239.605188	71.490622	67.682177
1239.248042	58.389520	67.687182
1238.251431	61.787368	67.692186
1237.206313	57.839141	67.697191
1236.914549	59.416663	67.702196
1235.934147	62.488857	67.707201
1235.024218	55.549210	67.712206
1234.525711	61.336660	67.717210
1234.136964	57.280008	67.722215
1233.930710	60.759244	67.727220
1232.819247	61.178875	67.732225
1231.850559	61.476963	67.737230
1230.847869	62.492153	67.742234
1230.798727	57.044793	67.747239
1230.294189	57.168683	67.752244
1230.052139	60.333931	67.757249
1228.891971	55.613996	67.762254
1228.557093	61.829726	67.767258
1227.662957	60.654200	67.772263
1226.729581	62.449723	67.777268
1225.711778	67.939259	67.782273
1225.326268	58.219827	67.787278
1224.995676	53.274580	67.792282
1224.163571	61.080495	67.797287
1223.587608	59.456175	67.802292
1222.425394	63.663524	67.807297
1222.284182	61.937535	67.812302
1221.809119	58.001447	67.817306
1220.861180	58.964635	67.822311
1220.185054	56.302779	67.827316
1218.978515	66.779518	67.832321
1218.471964	58.632446	67.837326
1217.961718	60.683537	67.842330
1217.434016	65.032900	67.847335
1217.418476	58.453263	67.852340
1216.287049	68.570187	67.857345
1215.615029	57.254233	67.862350
1214.975246	60.559020	67.867354
1214.135337	68.122341	67.872359
1213.786427	56.450293	67.877364
1212.757920	65.284131	67.882369
1212.004947	60.847755	67.887374
1211.594321	55.763455	67.892378
1211.160240	62.550748	67.897383
1210.823699	56.336713	67.902388
1209.524792	62.115549	67.907393
1208.964218	57.686101	67.912398
1208.480368	64.738087	67.917402
1207.538429	65.302771	67.922407
1206.919178	55.079837	67.927412
1206.144225	64.873241	67.932417
1205.550057	61.647512	67.937422
1205.169659	62.633135	67.942426
1204.641256	63.868297	67.947431
1203.919820	56.089188	67.952436
1202.952816	54.753257	67.957441
1202.355049	61.270168	67.962446
1201.702098	56.779567	67.967450
1200.669366	63.087937	67.972455
1200.414675	56.376756	67.977460
1199.358421	61.446582	67.982465
1199.044240	59.043665	67.987470
1198.539240	60.201797	67.992474
1197.941676	58.572100	67.997479
1197.167176	54.068761	68.002484
1196.217870	57.499961	68.007489
1195.710666	53.383073	68.012494
1195.326736	61.887483	68.017498
1194.574202	67.659617	68.022503
1193.761523	63.133208	68.027508
1192.911725	62.404813	68.032513
1192.470604	63.679503	68.037518
1192.160027	61.154396	68.042522
1190.817048	64.569715	68.047527
1190.111992	52.857210	68.052532
1189.764428	61.308816	68.057537
1189.140597	57.312155	68.062542
1188.821471	58.799236	68.067546
1187.910238	64.836950	68.072551
1187.077133	59.779199	68.077556
1186.320494	66.662376	68.082561
1185.780794	62.400664	68.087566
1185.490256	54.807113	68.092570
1184.509926	69.538469	68.097575
1183.842088	54.443572	68.102580
1183.141101	61.439975	68.107585
1182.480719	59.685647	68.112590
1182.148069	52.898611	68.117594
1181.103756	59.466715	68.122599
1180.515801	53.321388	68.127604
1179.827351	61.175734	68.132609
1179.452105	59.314563	68.137614
1179.147075	53.779973	68.142618
1177.475743	58.211466	68.147623
1177.223833	57.698058	68.152628
1176.624706	61.203115	68.157633
1176.407324	58.118922	68.162638
1174.967634	61.712637	68.167642
1174.009230	59.632381	68.172647
1173.368463	49.654710	68.177652
1173.098192	63.627413	68.182657
1172.902656	58.487739	68.187662
1172.634090	60.888619	68.192666
1171.542422	60.362684	68.197671
1170.992280	58.161215	68.202676
1170.201894	62.465166	68.207681
1169.537791	60.414649	68.212686
1168.375326	54.198751	68.217690
1167.400614	63.336392	68.222695
1167.305808	63.032127	68.227700
1167.017875	62.542650	68.232705
1166.438487	61.705990	68.237710
1165.184063	64.171856	68.242714
1164.537584	66.725070	68.247719
1164.055433	62.955194	68.252724
1163.308871	69.266281	68.257729
1163.118588	67.028064	68.262734
1161.903343	64.138407	68.267738
1161.084758	67.211329	68.272743
1161.014371	66.431984	68.277748
1160.303443	64.842227	68.282753
1159.870115	56.967221	68.287758
1158.599367	64.323669	68.292762
1157.762039	71.150406	68.297767
1157.400340	62.333968	68.302772
1156.995882	63.611857	68.307777
1156.339242	57.863537	68.312782
1155.466479	55.436665	68.317786
1154.426199	65.819027	68.322791
1154.279501	58.136907	68.327796
1153.801829	66.244101	68.332801
1153.063964	54.644190	68.337806
1152.289477	62.141445	68.342810
1151.247182	64.702040	68.347815
1151.205857	56.734260	68.352820
1149.891658	66.415535	68.357825
1149.035347	65.991405	68.362830
1149.015539	54.966409	68.367834
1148.277347	60.377685	68.372839
1148.173466	55.378629	68.377844
1146.644668	61.844176	68.382849
1145.929877	58.654899	68.387854
1145.140620	59.438176	68.392858
1144.691876	59.701725	68.397863
1144.495685	55.359890	68.402868
1143.893432	62.192556	68.407873
1142.644200	50.982167	68.412878
1142.254287	58.886445	68.417882
1141.146714	63.954411	68.422887
1141.131792	62.777564	68.427892
1140.555311	68.544030	68.432897
1139.396400	60.328681	68.437902
1139.039663	60.413853	68.442906
1138.303024	65.346863	68.447911
1138.331436	54.695699	68.452916
1137.021204	69.348550	68.457921
1136.123025	73.449922	68.462926
1135.372778	64.761987	68.467930
1134.844090	74.432316	68.472935
1134.669256	61.083319	68.477940
1133.542793	66.269778	68.482945
1132.556923	67.205927	68.487950
1131.991596	61.674464	68.492954
1131.697216	66.925677	68.497959
1131.580242	58.405616	68.502964
1130.243989	66.333389	68.507969
1129.369047	64.575940	68.512974
1128.989716	62.615215	68.517978
1128.222796	75.324610	68.522983
1128.068871	63.151053	68.527988
1127.635578	69.486658	68.532993
1126.578141	59.174961	68.537998
1126.196709	59.720656	68.543002
1125.119669	66.268718	68.548007
1124.393126	59.938323	68.553012
1123.336165	63.806369	68.558017
1122.914692	62.486382	68.563022
1122.621258	61.007110	68.568026
1121.802122	68.205320	68.573031
1120.875458	65.125742	68.578036
1120.314368	64.594228	68.583041
1119.563510	59.027829	68.588046
1119.299505	59.069100	68.593050
1118.483899	56.105501	68.598055
1118.061905	52.448485	68.603060
1117.218423	68.315694	68.608065
1116.467350	60.394843	68.613070
1116.033180	65.603284	68.618074
1115.474325	65.214276	68.623079
1114.225705	64.455899	68.628084
1113.512399	67.875519	68.633089
1112.819307	65.656693	68.638094
1112.781331	65.525058	68.643098
1112.572538	60.988418	68.648103
1111.258136	61.768467	68.653108
1110.518125	57.755004	68.658113
1109.915607	65.480963	68.663118
1109.575115	58.530680	68.668122
1108.152072	65.306534	68.673127
1108.143629	61.692383	68.678132
1107.584144	53.752547	68.683137
1106.438353	57.610543	68.688142
1105.470476	63.139702	68.693146
1104.527747	65.992715	68.698151
1104.662035	64.962021	68.703156
1104.085946	68.132762	68.708161
1103.323628	64.316924	68.713166
1103.470326	64.911129	68.718170
1102.074413	70.060843	68.723175
1101.221470	60.523704	68.728180
1100.905764	66.129077	68.733185
1099.940332	69.569371	68.738190
1099.003652	52.704047	68.743194
1097.939154	68.174911	68.748199
1097.760992	59.601781	68.753204
1096.940546	61.661790	68.758209
1096.417083	62.053000	68.763214
1096.177015	64.034550	68.768218
1095.759663	70.265984	68.773223
1095.269750	64.151247	68.778228
1094.020283	54.815030	68.783233
1093.760562	59.783215	68.788238
1092.649198	60.970191	68.793242
1091.828395	60.622882	68.798247
1091.415894	57.102393	68.803252
1091.009336	63.274347	68.808257
1090.126181	63.290593	68.813262
1089.628681	58.942727	68.818266
1088.795370	60.767715	68.823271
1088.513417	57.126982	68.828276
1087.159172	64.709703	68.833281
1086.030851	61.835576	68.838286
1085.827714	62.436003	68.843290
1085.102874	70.606442	68.848295
1084.865669	58.038625	68.853300
1084.239659	66.676457	68.858305
1083.337207	61.088262	68.863310
1083.612428	65.920640	68.868314
1082.340208	70.350528	68.873319
1081.939669	64.250093	68.878324
1081.137839	68.509438	68.883329
1079.677123	64.131124	68.888334
1079.212525	56.026236	68.893338
1078.580042	64.671097	68.898343
1078.107779	63.229949	68.903348
1077.712155	69.598576	68.908353
1077.456776	64.197196	68.913358
1076.702190	60.398987	68.918362
1075.935364	69.027777	68.923367
1074.528448	68.287439	68.928372
1073.480089	67.175454	68.933377
1072.881616	66.459304	68.938382
1072.970081	65.164101	68.943386
1072.365031	69.139107	68.948391
1071.934268	61.810358	68.953396
1071.612627	63.511813	68.958401
1070.218249	64.049001	68.963406
1069.565767	63.357889	68.968410
1068.619043	66.464211	68.973415
1068.610261	57.766560	68.978420
1067.483580	67.609939	68.983425
1066.492168	64.999727	68.988430
1066.434449	61.237708	68.993434
1065.699622	69.308416	68.998439
1065.308464	66.252408	69.003444
1064.423656	69.648114	69.008449
1063.498291	65.972698	69.013454
1063.160132	65.893650	69.018458
1062.261446	67.772861	69.023463
1061.711230	65.583654	69.028468
1060.323652	64.353717	69.033473
1059.548408	69.123223	69.038478
1059.405580	63.754280	69.043482
1058.994403	73.890778	69.048487
1058.772108	56.994708	69.053492
1057.859792	67.995398	69.058497
1057.866108	66.959382	69.063502
1056.701741	66.124227	69.068506
1055.704672	76.081595	69.073511
1055.160828	66.244048	69.078516
1054.355695	64.165596	69.083521
1053.285310	65.101233	69.088526
1052.674096	58.897150	69.093530
1052.001142	65.552859	69.098535
1052.037060	61.560475	69.103540
1051.779479	65.432562	69.108545
1050.734856	76.019752	69.113550
1049.754288	64.490633	69.118554
1048.971417	72.062753	69.123559
1048.914024	60.483703	69.128564
1048.171789	67.156409	69.133569
1047.176988	65.813033	69.138574
1046.760400	63.362932	69.143578
1045.091387	64.999471	69.148583
1044.790703	66.399722	69.153588
1043.993810	65.078112	69.158593
1043.599057	62.707558	69.163598
1043.400923	63.896046	69.168602
1042.635117	68.977344	69.173607
1042.351438	68.705424	69.178612
1041.378272	64.559802	69.183617
1040.165050	66.247760	69.188622
1039.878089	58.267188	69.193626
1039.024410	75.308063	69.198631
1038.607080	60.717778	69.203636
1038.040920	67.047322	69.208641
1037.163347	74.665266	69.213646
1036.556535	74.078832	69.218650
1036.071757	74.809986	69.223655
1035.068398	62.285746	69.228660
1034.063675	68.631974	69.233665
1033.272284	60.054528	69.238670
1033.152468	58.639474	69.243674
1032.572366	64.086844	69.248679
1032.513156	52.894147	69.253684
1032.245186	55.711748	69.258689
1030.562613	70.443372	69.263694
1030.020463	61.417081	69.268698
1029.340703	70.094909	69.273703
1029.157626	62.026682	69.278708
1027.854234	61.945569	69.283713
1027.230430	62.864732	69.288718
1026.861962	61.807638	69.293722
1025.628202	63.265443	69.298727
1025.186604	59.272337	69.303732
1024.842667	69.708749	69.308737
1024.181005	69.722995	69.313742
1023.885806	54.003835	69.318746
1022.686918	61.701666	69.323751
1021.646832	58.742582	69.328756
1021.227820	61.423032	69.333761
1020.565062	70.408986	69.338766
1020.658286	59.971326	69.343770
1019.113463	61.814358	69.348775
1018.402404	60.945793	69.353780
1017.525048	59.237331	69.358785
1016.957169	73.305595	69.363790
1017.375435	60.731324	69.368794
1017.020706	68.611818	69.373799
1015.477801	71.944975	69.378804
1014.739952	58.002452	69.383809
1014.329113	63.147298	69.388814
1013.637556	60.910070	69.393818
1012.451902	66.662842	69.398823
1011.653978	64.865386	69.403828
1011.327255	65.447113	69.408833
1010.605523	69.279087	69.413838
1010.473573	60.618321	69.418842
1009.696845	64.897453	69.423847
1008.896726	55.369059	69.428852
1008.170584	54.942399	69.433857
1007.282851	68.508883	69.438862
1007.265940	55.663763	69.443866
1005.835639	66.155560	69.448871
1005.332802	64.410198	69.453876
1004.861751	68.148325	69.458881
1004.113407	61.757745	69.463886
1004.365630	61.419711	69.468890
1002.754488	67.627042	69.473895
1001.991873	62.091099	69.478900
1001.670298	60.457584	69.483905
1001.123556	59.366683	69.488910
1000.387923	55.488274	69.493914
999.410974	58.101650	69.498919
998.999643	59.653080	69.503924
998.289149	61.835187	69.508929
997.389357	55.649354	69.513934
996.705271	59.146081	69.518938
996.025829	58.509725	69.523943
995.266478	62.972583	69.528948
995.306781	55.983947	69.533953
994.862382	53.611638	69.538958
993.893797	52.375490	69.543962
992.690187	63.583164	69.548967
992.399842	56.215386	69.553972
991.753746	58.235683	69.558977
990.845110	61.633505	69.563982
990.189582	56.610516	69.568986
989.223084	61.755000	69.573991
988.614558	60.588238	69.578996
988.688775	58.348550	69.584001
987.908114	59.870472	69.589006
987.567523	58.978730	69.594010
986.220512	60.891706	69.599015
985.693932	56.626990	69.604020
985.231163	59.974112	69.609025
984.434631	66.559415	69.614030
983.529991	56.307649	69.619034
982.838108	66.704570	69.624039
982.241395	68.448795	69.629044
982.024685	58.099347	69.634049
981.369289	57.837804	69.639054
980.224124	62.200165	69.644058
979.408304	65.346054	69.649063
978.608084	60.563756	69.654068
978.217551	58.299059	69.659073
978.078100	65.711259	69.664078
977.798734	52.777678	69.669082
976.631161	61.811399	69.674087
975.955992	59.648341	69.679092
975.547495	57.872617	69.684097
973.888961	63.152591	69.689102
973.808507	60.584936	69.694106
972.947676	68.835905	69.699111
972.689225	68.598351	69.704116
972.268491	72.893098	69.709121
970.789429	72.200669	69.714126
970.413395	60.234512	69.719130
969.582148	70.795428	69.724135
969.173329	65.342578	69.729140
968.935078	58.908068	69.734145
968.339244	66.557103	69.739150
967.707947	61.908501	69.744154
966.318983	65.202675	69.749159
965.783126	63.887294	69.754164
965.013491	66.407938	69.759169
963.989724	64.876130	69.764174
963.947674	57.113745	69.769178
963.140956	69.287612	69.774183
962.491470	67.504216	69.779188
962.648515	62.715867	69.784193
961.296428	66.966047	69.789198
961.063479	62.257119	69.794202
960.458371	74.173053	69.799207
959.001028	68.018766	69.804212
958.130990	66.572337	69.809217
957.319356	71.015735	69.814222
957.068449	62.359559	69.819226
956.784499	69.950446	69.824231
956.402621	63.099635	69.829236
955.828836	62.526502	69.834241
954.813785	68.158888	69.839246
954.369684	61.540566	69.844250
953.448474	71.310484	69.849255
952.478780	64.604551	69.854260
951.385017	62.462266	69.859265
950.763197	63.513724	69.864270
950.743814	56.198620	69.869274
950.217251	66.719984	69.874279
949.862983	63.390449	69.879284
948.803814	59.986647	69.884289
947.744049	67.320026	69.889294
947.304880	55.671384	69.894298
946.726273	65.186845	69.899303
946.534024	61.080786	69.904308
945.648311	63.024896	69.909313
944.424016	64.510703	69.914318
944.324461	64.253438	69.919322
943.490683	62.887245	69.924327
942.844550	58.706954	69.929332
941.736067	56.412860	69.934337
940.891539	61.369101	69.939342
940.873972	57.343253	69.944346
940.339926	65.074859	69.949351
939.931124	63.644173	69.954356
938.584418	49.450711	69.959361
938.055279	61.190606	69.964366
937.608429	53.002974	69.969370
937.373301	61.788195	69.974375
936.325559	69.122674	69.979380
935.651378	57.398631	69.984385
935.098094	69.341210	69.989390
934.831165	59.488634	69.994394
933.119505	69.663126	69.999399
932.077015	58.529108	70.004404
931.616694	64.979074	70.009409
931.311241	63.503848	70.014414
931.115691	50.496717	70.019418
930.921002	59.213040	70.024423
929.541155	65.626684	70.029428
928.771160	59.588759	70.034433
927.969518	71.877017	70.039438
927.633278	59.494339	70.044442
927.147207	69.469587	70.049447
926.512972	55.644341	70.054452
925.941896	56.908941	70.059457
924.856777	60.754213	70.064462
924.280306	58.365848	70.069466
923.469063	68.647038	70.074471
922.515469	67.420573	70.079476
922.308114	70.382922	70.084481
921.703684	70.759992	70.089486
921.422306	64.472997	70.094490
920.632846	69.785714	70.099495
920.042986	66.369432	70.104500
919.288413	64.559832	70.109505
918.226383	68.100379	70.114510
917.267124	66.805810	70.119514
916.404937	67.456357	70.124519
916.263088	60.780354	70.129524
916.133681	70.192438	70.134529
915.561641	68.057907	70.139534
914.580654	65.490942	70.144538
913.625322	75.342101	70.149543
912.805999	77.328528	70.154548
912.406068	63.355787	70.159553
911.688645	61.418253	70.164558
910.662573	68.345624	70.169562
910.043385	70.131204	70.174567
909.625763	79.188466	70.179572
909.276077	70.164362	70.184577
909.104166	78.697592	70.189582
908.229555	65.225732	70.194586
906.824850	72.052567	70.199591
906.353178	66.978762	70.204596
906.098519	71.766882	70.209601
904.920318	75.627708	70.214606
904.418157	66.282371	70.219610
903.482510	83.902131	70.224615
903.125309	82.902324	70.229620
902.866931	68.055117	70.234625
901.702569	75.451022	70.239630
901.096006	67.895054	70.244634
900.308326	66.780697	70.249639
899.610760	69.766613	70.254644
899.664672	61.611237	70.259649
898.753133	67.856265	70.264654
897.823968	65.475812	70.269658
897.133170	73.596620	70.274663
896.399958	65.004900	70.279668
896.327430	74.229227	70.284673
895.175712	70.984175	70.289678
894.108138	63.659529	70.294682
893.861161	69.794684	70.299687
893.647742	74.830729	70.304692
892.893085	74.523437	70.309697
891.520038	75.424109	70.314702
891.197270	75.093370	70.319706
890.540332	74.771711	70.324711
889.860518	67.419334	70.329716
889.647183	69.114484	70.334721
888.309844	73.421363	70.339726
887.946168	69.963189	70.344730
887.310542	72.140776	70.349735
886.481606	72.052250	70.354740
886.282580	72.518566	70.359745
885.390310	79.050810	70.364750
884.521845	67.631219	70.369754
883.935892	69.342034	70.374759
882.801808	71.052787	70.379764
882.669674	76.020045	70.384769
881.953660	69.230024	70.389774
881.025683	73.310879	70.394778
880.342220	74.037394	70.399783
879.983061	72.130077	70.404788
879.839487	69.803750	70.409793
879.125806	71.488286	70.414798
878.386163	66.797075	70.419802
877.265436	74.481942	70.424807
876.760693	76.652509	70.429812
876.501547	56.991488	70.434817
875.049001	68.428517	70.439822
874.556340	66.709847	70.444826
874.001738	69.502736	70.449831
873.419800	70.816569	70.454836
873.245635	66.475719	70.459841
871.859619	73.329755	70.464846
871.418232	74.342029	70.469850
870.945265	74.267927	70.474855
870.303081	67.640124	70.479860
869.325559	68.569762	70.484865
868.289224	70.648230	70.489870
868.200991	68.833845	70.494874
867.789092	64.053345	70.499879
867.181023	73.683589	70.504884
866.656697	66.935343	70.509889
865.302978	72.094857	70.514894
864.947749	66.772572	70.519898
864.352213	60.405191	70.524903
863.039793	63.458529	70.529908
862.335793	61.924473	70.534913
861.920797	73.044462	70.539918
861.412837	69.531665	70.544922
861.105209	65.658916	70.549927
860.577860	69.555501	70.554932
859.378999	62.758985	70.559937
858.332286	70.346312	70.564942
858.000016	65.430207	70.569946
857.520590	61.112830	70.574951
857.132569	59.545969	70.579956
856.958029	58.695660	70.584961
855.494479	69.418169	70.589966
854.940769	59.682222	70.594970
854.524933	62.925398	70.599975
853.698082	57.653110	70.604980
852.617541	62.627288	70.609985
851.818190	65.756952	70.614990
851.355825	64.990283	70.619994
851.153631	67.659264	70.624999
850.838376	62.815637	70.630004
850.166728	62.795698	70.635009
848.695577	65.161397	70.640014
848.652709	61.339612	70.645018
847.822274	58.079412	70.650023
846.710873	65.602033	70.655028
846.162594	56.933262	70.660033
845.192204	65.362075	70.665038
845.010537	59.715214	70.670042
844.725584	61.444736	70.675047
843.898220	69.733402	70.680052
842.770306	61.995577	70.685057
841.655112	66.943327	70.690062
841.490882	63.289953	70.695066
841.327285	58.837962	70.700071
840.630287	64.044458	70.705076
840.253843	55.857414	70.710081
839.144838	58.291735	70.715086
838.755043	55.208682	70.720090
837.858740	64.748167	70.725095
836.594992	56.230761	70.730100
835.886386	62.960481	70.735105
835.350048	67.069780	70.740110
834.913835	64.321500	70.745114
834.543586	58.915352	70.750119
833.705421	64.890858	70.755124
833.956901	64.029156	70.760129
832.737483	69.338558	70.765134
832.182822	69.116619	70.770138
831.405219	66.712984	70.775143
830.656670	63.664143	70.780148
829.938451	64.234390	70.785153
828.966721	63.963501	70.790158
828.809799	59.472474	70.795162
827.548647	58.465676	70.800167
826.448531	61.874216	70.805172
825.995889	56.451000	70.810177
825.463717	64.270704	70.815182
825.339983	55.124635	70.820186
824.912181	53.508542	70.825191
824.539909	60.454190	70.830196
823.631094	56.953223	70.835201
822.693755	59.503005	70.840206
822.022610	64.110238	70.845210
820.886639	59.616788	70.850215
820.360804	59.547405	70.855220
820.000140	56.000309	70.860225
819.043648	76.172311	70.865230
818.835892	63.990658	70.870234
818.224900	69.124403	70.875239
817.422437	63.765843	70.880244
816.926263	54.013343	70.885249
816.341939	69.923394	70.890254
815.162078	60.457331	70.895258
814.263798	60.376748	70.900263
813.345320	59.123372	70.905268
813.222368	65.058868	70.910273
812.644518	69.892084	70.915278
812.378009	57.431569	70.920282
811.722543	64.651109	70.925287
810.375206	64.711390	70.930292
810.122078	63.440752	70.935297
809.218731	72.283593	70.940302
808.831663	68.063290	70.945306
807.726037	63.662930	70.950311
806.800905	62.727256	70.955316
806.799881	59.887465	70.960321
805.798222	72.408924	70.965326
805.586903	66.936083	70.970330
805.340685	61.321992	70.975335
804.375948	74.955754	70.980340
803.688442	53.366526	70.985345
802.860549	65.880321	70.990350
802.090229	58.508341	70.995354
801.089856	63.810225	71.000359
800.427726	66.306160	71.005364
800.272299	62.324852	71.010369
799.647488	63.149483	71.015374
799.319043	55.419594	71.020378
798.014321	65.150219	71.025383
797.370154	64.823228	71.030388
797.464113	58.459722	71.035393
796.248528	63.244290	71.040398
795.354552	55.579300	71.045402
794.577868	61.117985	71.050407
793.993810	58.794094	71.055412
793.759332	56.413480	71.060417
792.441453	67.636018	71.065422
791.871665	59.470652	71.070426
791.401026	66.163561	71.075431
790.574909	67.223192	71.080436
790.504552	57.850494	71.085441
789.898839	66.396048	71.090446
789.472825	64.050216	71.095450
788.492506	63.851856	71.100455
787.953835	64.872512	71.105460
786.540836	58.500707	71.110465
785.638563	66.779314	71.115470
785.038646	66.325146	71.120474
784.599010	61.790186	71.125479
784.313783	63.677643	71.130484
784.215984	55.505242	71.135489
782.766646	54.200709	71.140494
781.870738	53.829610	71.145498
781.225312	53.646908	71.150503
780.580790	70.119475	71.155508
780.411419	67.503115	71.160513
779.952503	60.502906	71.165518
779.475345	64.249985	71.170522
778.147063	60.663784	71.175527
777.462647	64.394657	71.180532
777.128269	61.292249	71.185537
776.706101	70.862624	71.190542
775.756043	53.880902	71.195546
774.832820	61.324326	71.200551
774.387760	65.930729	71.205556
774.298837	63.623861	71.210561
773.048417	68.818986	71.215566
772.298490	64.609533	71.220570
771.802905	63.487398	71.225575
771.171255	64.609241	71.230580
770.245407	55.314017	71.235585
769.696062	65.671132	71.240590
769.103253	55.816385	71.245594
768.529424	57.266200	71.250599
767.907750	67.180205	71.255604
766.731693	64.825101	71.260609
765.675987	71.251543	71.265614
765.326956	68.667143	71.270618
764.898824	60.449097	71.275623
764.506490	66.045493	71.280628
764.092455	58.994971	71.285633
763.705123	65.540985	71.290638
762.843105	58.046177	71.295642
762.164382	59.351339	71.300647
761.045384	67.446033	71.305652
760.075049	51.471555	71.310657
759.396937	58.063036	71.315662
759.430387	64.120940	71.320666
759.105375	61.117187	71.325671
758.053175	65.356697	71.330676
757.200650	64.030459	71.335681
756.513933	68.553134	71.340686
755.855259	56.008634	71.345690
755.774923	59.928907	71.350695
754.309810	57.538460	71.355700
753.484805	62.560849	71.360705
752.667718	63.073442	71.365710
752.239752	58.913442	71.370714
752.180322	53.360122	71.375719
751.557649	62.300532	71.380724
750.452442	55.550376	71.385729
749.683218	62.626388	71.390734
748.792445	63.977349	71.395738
748.543271	55.320517	71.400743
748.147990	68.170316	71.405748
747.549198	56.712474	71.410753
746.215443	63.227597	71.415758
745.711133	60.554938	71.420762
745.477609	60.364835	71.425767
744.989371	70.824375	71.430772
743.946229	70.794672	71.435777
743.220873	68.310659	71.440782
742.791483	60.713325	71.445786
742.338492	61.531423	71.450791
741.106832	66.147845	71.455796
740.471648	59.679128	71.460801
739.442046	65.875717	71.465806
739.207540	59.545588	71.470810
739.031595	57.459277	71.475815
738.601525	64.258915	71.480820
737.613203	60.123070	71.485825
736.578069	60.573155	71.490830
736.378739	62.878902	71.495834
735.907838	61.503082	71.500839
734.541188	68.368826	71.505844
734.530945	50.868910	71.510849
733.938080	61.945940	71.515854
732.523965	62.258458	71.520858
731.822289	59.591586	71.525863
730.821241	63.214872	71.530868
730.732886	59.918752	71.535873
729.823198	60.155122	71.540878
729.441800	56.936834	71.545882
728.782140	57.699552	71.550887
727.675269	68.805827	71.555892
727.236816	56.019145	71.560897
726.409009	61.455285	71.565902
726.292993	56.164277	71.570906
725.824890	53.726590	71.575911
724.763077	55.940099	71.580916
724.113093	49.467609	71.585921
722.996183	54.034375	71.590926
723.036813	58.370875	71.595930
722.625269	63.535981	71.600935
721.796969	64.765329	71.605940
721.157939	54.337097	71.610945
720.491294	56.079906	71.615950
719.612787	64.076568	71.620954
718.795816	58.535396	71.625959
717.899017	64.504775	71.630964
717.696799	56.019498	71.635969
717.346243	61.999900	71.640974
716.060319	63.934848	71.645978
715.089152	60.371959	71.650983
714.684347	60.500921	71.655988
714.230493	59.840171	71.660993
713.906103	64.543924	71.665998
712.924178	62.583450	71.671002
712.363488	59.838748	71.676007
711.275504	70.787061	71.681012
711.360361	61.663292	71.686017
710.507603	58.859289	71.691022
709.124166	61.218289	71.696026
708.640838	57.230797	71.701031
707.711274	69.578866	71.706036
707.444176	54.799521	71.711041
707.241343	58.520922	71.716046
706.976278	69.448253	71.721050
706.052304	60.073385	71.726055
704.955352	66.735046	71.731060
704.614104	60.660036	71.736065
703.537610	68.101703	71.741070
702.520626	61.694057	71.746074
702.271338	63.683907	71.751079
701.466032	69.215271	71.756084
701.167073	63.403396	71.761089
700.544835	63.590528	71.766094
700.030196	59.396438	71.771098
699.397357	57.317352	71.776103
698.450285	63.781241	71.781108
697.953506	60.277606	71.786113
696.793956	60.548103	71.791118
695.875610	63.953159	71.796122
695.448996	57.872645	71.801127
694.633695	69.268428	71.806132
694.788823	63.498361	71.811137
694.374991	57.433025	71.816142
693.185435	56.406893	71.821146
692.752724	64.479941	71.826151
691.537321	71.274392	71.831156
691.555807	66.375582	71.836161
690.230678	67.690839	71.841166
689.557935	63.490679	71.846170
689.194178	52.972273	71.851175
688.685012	58.225545	71.856180
688.349816	59.591858	71.861185
687.047133	63.517469	71.866190
685.845361	63.867435	71.871194
685.517647	57.041335	71.876199
685.169451	67.017827	71.881204
684.893434	55.513783	71.886209
683.785338	66.875651	71.891214
682.954257	59.166365	71.896218
682.465900	61.218091	71.901223
681.659347	67.326744	71.906228
681.766875	57.923980	71.911233
680.729926	68.127013	71.916238
679.648856	56.992586	71.921242
679.344979	60.215800	71.926247
678.622789	58.720809	71.931252
678.359430	58.763572	71.936257
677.126475	60.946019	71.941262
676.600669	58.418755	71.946266
676.135470	54.916030	71.951271
675.029253	66.327311	71.956276
674.724018	54.495925	71.961281
673.349744	62.688833	71.966286
673.198130	61.864209	71.971290
673.095762	61.194166	71.976295
672.244022	66.450476	71.981300
671.768204	62.332629	71.986305
670.751884	59.134310	71.991310
669.934644	59.327223	71.996314
669.401621	52.493672	72.001319
668.316211	60.821029	72.006324
667.445638	59.274886	72.011329
666.941522	63.561034	72.016334
666.280026	61.428050	72.021338
666.608532	58.867710	72.026343
665.893812	53.206803	72.031348
664.889185	54.533075	72.036353
664.136851	59.968922	72.041358
663.503521	55.773859	72.046362
663.252349	57.404052	72.051367
661.778177	63.223288	72.056372
661.161150	47.121222	72.061377
660.810927	53.566933	72.066382
660.196668	58.438760	72.071386
659.609443	53.946473	72.076391
658.536494	57.632611	72.081396
657.777648	60.676812	72.086401
657.417258	56.330784	72.091406
656.856219	58.721788	72.096410
656.739576	52.523049	72.101415
655.383625	64.193814	72.106420
654.841496	62.460358	72.111425
654.218454	61.939909	72.116430
653.683475	64.251060	72.121434
652.849123	58.737748	72.126439
651.473865	62.567254	72.131444
651.321844	59.816491	72.136449
650.675570	61.635552	72.141454
650.525331	65.349128	72.146458
650.109831	56.021765	72.151463
648.482603	63.282674	72.156468
648.213050	57.667864	72.161473
647.462679	62.245661	72.166478
647.259455	65.939895	72.171482
646.299801	59.008920	72.176487
645.350849	60.709321	72.181492
644.713914	54.039621	72.186497
644.274429	63.630718	72.191502
643.702045	61.328137	72.196506
642.964082	54.129065	72.201511
641.712941	61.890775	72.206516
641.533503	58.894855	72.211521
641.067233	61.654472	72.216526
640.687981	60.057315	72.221530
639.663959	62.128190	72.226535
638.304251	59.994443	72.231540
638.162401	52.781266	72.236545
638.127304	51.012654	72.241550
637.104469	65.534610	72.246554
636.357015	48.482318	72.251559
635.232291	56.718919	72.256564
634.983319	52.906407	72.261569
634.559020	56.322743	72.266574
634.094856	53.348370	72.271578
633.327223	47.357872	72.276583
632.460214	50.396923	72.281588
631.906709	50.815827	72.286593
630.686351	56.101742	72.291598
629.961980	57.245802	72.296602
629.370366	56.098297	72.301607
628.606853	58.446234	72.306612
628.140717	51.408610	72.311617
627.688701	62.283887	72.316622
627.491307	58.947248	72.321626
626.888544	50.913484	72.326631
625.851969	62.640449	72.331636
625.484193	56.885373	72.336641
624.151043	60.652412	72.341646
623.231293	60.161092	72.346650
622.944843	56.094095	72.351655
622.318992	59.758900	72.356660
622.079938	54.288071	72.361665
621.694501	53.121820	72.366670
620.245987	54.020890	72.371674
619.868166	53.295811	72.376679
618.890356	63.170180	72.381684
618.606034	57.175030	72.386689
618.001833	54.501347	72.391694
616.839694	57.637937	72.396698
616.564485	53.913995	72.401703
615.936446	54.899456	72.406708
615.540940	55.105381	72.411713
614.595877	51.081756	72.416718
613.689498	59.340554	72.421722
613.299455	52.000570	72.426727
612.622172	51.746775	72.431732
611.952646	49.550049	72.436737
610.947341	50.998414	72.441742
609.968718	45.542596	72.446746
609.938291	37.510252	72.451751
609.362902	50.779681	72.456756
608.825918	43.152658	72.461761
607.658856	53.115496	72.466766
606.894895	47.843151	72.471770
606.853874	40.996369	72.476775
606.026479	55.815998	72.481780
605.679240	46.814040	72.486785
604.711384	40.919431	72.491790
603.559437	51.086115	72.496794
603.279193	44.094014	72.501799
602.857813	54.855095	72.506804
602.224285	48.801761	72.511809
601.114534	49.463989	72.516814
600.466470	52.345934	72.521818
599.884658	45.658513	72.526823
599.358968	55.518571	72.531828
598.861189	51.862764	72.536833
598.031761	56.799090	72.541838
597.033443	59.113056	72.546842
596.797829	45.428419	72.551847
596.169270	55.184135	72.556852
595.511950	44.391199	72.561857
594.466204	46.101482	72.566862
594.200451	54.784172	72.571866
593.560395	42.515601	72.576871
592.506415	47.797881	72.581876
591.501951	44.202444	72.586881
591.139145	42.356569	72.591886
590.473538	51.541952	72.596890
590.365171	49.587749	72.601895
589.735350	64.503396	72.606900
589.169875	53.447234	72.611905
588.264297	56.749465	72.616910
587.362410	61.779915	72.621914
586.963530	43.408782	72.626919
586.021211	58.360993	72.631924
585.074382	48.334068	72.636929
584.501130	49.647231	72.641934
583.991286	53.807264	72.646938
583.766134	57.568014	72.651943
583.413026	56.801994	72.656948
582.456491	44.787374	72.661953
581.412431	45.024296	72.666958
580.521674	48.832379	72.671962
580.530119	43.703999	72.676967
579.404388	50.626379	72.681972
578.928532	43.650824	72.686977
578.662201	50.349776	72.691982
577.675614	53.937057	72.696986
576.773760	43.491139	72.701991
575.796705	47.113889	72.706996
575.398118	44.088424	72.712001
574.937148	40.528152	72.717006
574.482154	51.458006	72.722010
573.485058	45.933131	72.727015
572.606233	52.855047	72.732020
572.013132	38.583552	72.737025
572.022147	44.724959	72.742030
571.069087	44.171861	72.747034
569.998769	44.602353	72.752039
568.776259	48.007043	72.757044
568.673470	45.495733	72.762049
568.490073	48.691200	72.767054
567.953001	56.492010	72.772058
567.914030	44.225053	72.777063
566.626602	47.584817	72.782068
565.754866	42.451337	72.787073
564.631291	35.401648	72.792078
563.670883	48.373511	72.797082
563.466880	48.811481	72.802087
562.746128	49.307599	72.807092
562.050685	44.162859	72.812097
562.043327	51.488058	72.817102
561.458624	48.089506	72.822106
560.524352	46.152086	72.827111
559.338144	52.018708	72.832116
559.219982	52.159750	72.837121
559.041277	47.939703	72.842126
557.677000	53.506855	72.847130
557.286634	39.291411	72.852135
556.484550	48.406630	72.857140
555.892723	39.278840	72.862145
554.611291	48.711442	72.867150
553.471870	51.557588	72.872154
553.517512	41.328259	72.877159
552.729056	54.565517	72.882164
552.465687	47.837751	72.887169
552.116801	45.992652	72.892174
551.181351	50.253240	72.897178
550.408480	44.070645	72.902183
549.717382	48.483960	72.907188
549.088301	48.594919	72.912193
548.816530	46.251503	72.917198
548.255884	49.690415	72.922202
547.690844	41.795070	72.927207
546.717067	47.926066	72.932212
545.285984	45.437101	72.937217
544.367536	46.325496	72.942222
543.665348	58.419093	72.947226
544.070068	47.533399	72.952231
543.214007	46.937636	72.957236
542.847694	39.870298	72.962241
542.768045	43.855177	72.967246
541.176719	49.786481	72.972250
540.499172	40.470102	72.977255
539.703505	38.530648	72.982260
539.234329	40.315033	72.987265
538.301789	42.679706	72.992270
537.216150	47.264434	72.997274
537.023253	35.981834	73.002279
536.672033	45.432276	73.007284
536.209917	44.242860	73.012289
535.968027	41.642498	73.017294
534.787001	46.333170	73.022298
534.169367	43.801533	73.027303
533.281687	44.593873	73.032308
532.330236	46.418662	73.037313
531.564651	42.817043	73.042318
530.656083	49.569991	73.047322
530.643336	41.685009	73.052327
529.966629	44.332670	73.057332
529.664048	42.766991	73.062337
529.348980	41.161612	73.067342
528.079624	42.228157	73.072346
527.165805	43.468241	73.077351
526.641015	53.896138	73.082356
526.020235	42.358450	73.087361
525.186833	39.694059	73.092366
524.059720	48.759980	73.097370
523.792495	36.052175	73.102375
523.404497	47.445781	73.107380
522.964639	46.001908	73.112385
522.393153	52.976557	73.117390
521.444367	48.924385	73.122394
520.866002	40.302291	73.127399
520.434662	52.309608	73.132404
519.203178	48.462973	73.137409
518.379699	43.826074	73.142414
517.759289	46.874199	73.147418
517.787971	44.175373	73.152423
517.257549	48.558791	73.157428
516.201227	44.422816	73.162433
515.827113	48.297899	73.167438
514.757710	48.572334	73.172442
514.550410	48.708520	73.177447
513.282285	52.889548	73.182452
512.483196	55.358459	73.187457
511.954435	54.838847	73.192462
511.603652	49.401781	73.197466
511.483470	44.136770	73.202471
510.272106	49.580236	73.207476
509.552333	47.716987	73.212481
509.206330	49.183050	73.217486
507.576444	49.095263	73.222490
507.300160	40.353520	73.227495
506.537724	49.495895	73.232500
506.051572	42.113589	73.237505
505.498039	49.599868	73.242510
505.095083	55.764501	73.247514
504.538912	46.368912	73.252519
503.512039	50.417028	73.257524
502.653101	33.113523	73.262529
502.120935	41.491742	73.267534
501.741053	50.618301	73.272538
500.980424	46.617177	73.277543
499.806947	51.308538	73.282548
499.257462	50.441974	73.287553
499.334490	41.151428	73.292558
498.836736	47.845430	73.297562
497.925518	40.554910	73.302567
496.885374	41.960322	73.307572
496.553663	37.550987	73.312577
495.322316	40.817478	73.317582
494.377453	41.643701	73.322586
493.950847	38.703964	73.327591
493.415315	42.905899	73.332596
492.967925	42.869292	73.337601
492.801690	41.381694	73.342606
492.058650	46.931217	73.347610
491.050684	40.272241	73.352615
490.349928	50.835677	73.357620
489.498108	45.813663	73.362625
489.102750	39.557711	73.367630
487.373062	46.405974	73.372634
487.156409	32.975080	73.377639
487.024558	37.866875	73.382644
485.848320	46.961744	73.387649
485.350852	35.771999	73.392654
484.679775	45.893003	73.397658
484.695785	45.683442	73.402663
484.174204	48.385444	73.407668
483.502392	45.652321	73.412673
482.629846	42.691110	73.417678
481.825291	44.977813	73.422682
481.540229	43.333745	73.427687
479.896105	49.786845	73.432692
479.711666	52.933942	73.437697
479.011429	40.933069	73.442702
478.457880	48.891823	73.447706
478.282881	43.198076	73.452711
477.289755	43.888108	73.457716
476.423469	41.608287	73.462721
476.092505	38.535328	73.467726
474.930995	50.239103	73.472730
474.227784	39.241316	73.477735
473.526106	49.052584	73.482740
472.670233	39.535873	73.487745
472.729568	46.115861	73.492750
472.147069	41.593591	73.497754
471.632443	47.465928	73.502759
470.434930	53.857895	73.507764
469.832283	50.804255	73.512769
469.210473	51.894449	73.517774
468.645477	45.122072	73.522778
467.635443	48.705888	73.527783
467.131512	43.854384	73.532788
466.547795	44.578466	73.537793
466.163870	43.402893	73.542798
465.245314	56.964010	73.547802
464.481397	44.371717	73.552807
463.421715	50.303116	73.557812
462.979159	55.263159	73.562817
462.951668	40.820167	73.567822
462.631544	54.926065	73.572826
461.676888	45.481541	73.577831
460.739915	46.029725	73.582836
460.039991	51.980393	73.587841
459.013362	35.333233	73.592846
458.255199	53.893936	73.597850
457.892105	44.950770	73.602855
457.056837	44.639207	73.607860
456.763625	49.784038	73.612865
456.589454	48.329773	73.617870
455.214589	54.915941	73.622874
454.831901	44.998427	73.627879
454.170436	45.547950	73.632884
453.106586	47.930798	73.637889
452.243958	43.179051	73.642894
451.139842	51.347412	73.647898
451.184968	44.915722	73.652903
450.382541	50.136763	73.657908
449.933858	49.655539	73.662913
449.735822	47.595136	73.667918
449.163634	48.924315	73.672922
448.684295	48.483868	73.677927
447.315240	42.667131	73.682932
446.500994	56.188269	73.687937
446.252801	39.397451	73.692942
445.340102	57.407962	73.697946
444.258234	45.741688	73.702951
444.164467	40.832532	73.707956
443.648767	48.937160	73.712961
443.064720	43.213257	73.717966
441.790174	51.317672	73.722970
441.195625	47.865171	73.727975
440.744571	49.405290	73.732980
439.839093	51.058016	73.737985
439.898049	43.581124	73.742990
439.029266	46.327234	73.747994
438.277470	48.784497	73.752999
437.670160	53.767247	73.758004
437.213523	54.144706	73.763009
436.246720	46.935562	73.768014
435.080685	53.527787	73.773018
434.726299	50.574100	73.778023
434.494790	44.017329	73.783028
433.895133	47.218607	73.788033
433.166852	44.430042	73.793038
432.132391	48.561176	73.798042
431.506057	53.817566	73.803047
431.030697	57.538304	73.808052
429.954306	49.910992	73.813057
429.474981	41.821782	73.818062
428.307204	52.084749	73.823066
428.236741	44.475308	73.828071
427.970540	52.121155	73.833076
427.149303	50.355829	73.838081
426.196575	45.187316	73.843086
425.584701	54.417180	73.848090
425.404607	44.320883	73.853095
424.486176	44.204356	73.858100
423.309719	46.634532	73.863105
422.798207	39.653671	73.868110
422.128594	55.461466	73.873114
421.839254	44.871552	73.878119
421.284174	45.143126	73.883124
420.231460	53.593982	73.888129
419.528050	48.691410	73.893134
419.078743	44.136850	73.898138
418.709546	47.134040	73.903143
417.639352	49.661264	73.908148
416.721937	53.363026	73.913153
416.441199	39.869705	73.918158
415.826896	48.816973	73.923162
415.140772	40.228369	73.928167
414.384010	52.774184	73.933172
413.503617	55.800563	73.938177
413.160454	47.307515	73.943182
412.684461	56.717766	73.948186
412.086304	45.878030	73.953191
410.861718	51.997164	73.958196
409.958106	53.785752	73.963201
409.724597	38.750482	73.968206
408.947723	56.756268	73.973210
408.599748	41.279586	73.978215
407.710148	51.075697	73.983220
406.753617	54.558783	73.988225
406.444965	44.370842	73.993230
406.120167	59.128028	73.998234
405.605539	51.487342	74.003239
404.349812	51.716369	74.008244
403.451242	50.893062	74.013249
403.409251	50.250177	74.018254
402.739734	57.513591	74.023258
401.695704	56.988355	74.028263
400.730623	57.741882	74.033268
399.653621	62.239900	74.038273
399.743688	59.302016	74.043278
399.028908	60.352102	74.048282
398.751397	53.251799	74.053287
398.558509	50.382933	74.058292
397.176585	55.185823	74.063297
396.462103	54.517274	74.068302
395.958358	64.624615	74.073306
395.195143	58.493287	74.078311
394.040734	50.932643	74.083316
393.437439	62.262498	74.088321
392.924200	57.067617	74.093326
392.533495	64.161286	74.098330
392.410271	57.532275	74.103335
391.910564	51.264613	74.108340
390.419582	60.208192	74.113345
389.746462	49.888118	74.118350
388.931277	56.241419	74.123354
389.094925	50.008486	74.128359
388.049818	48.187198	74.133364
387.216383	53.789329	74.138369
386.631403	50.889375	74.143374
386.182084	64.780588	74.148378
385.641703	51.139141	74.153383
384.364417	50.859529	74.158388
383.587429	52.350911	74.163393
383.424707	51.959625	74.168398
383.123951	57.802027	74.173402
382.228811	51.144662	74.178407
381.021795	56.800555	74.183412
380.114886	59.162838	74.188417
379.845931	50.701284	74.193422
379.500550	57.870467	74.198426
379.141842	61.153610	74.203431
378.011853	54.155988	74.208436
376.933837	57.831995	74.213441
377.227905	51.259360	74.218446
376.258000	59.527096	74.223450
375.410878	53.525805	74.228455
374.592087	52.601206	74.233460
373.774557	51.537056	74.238465
373.687682	54.061547	74.243470
372.885204	60.054668	74.248474
372.116781	51.534249	74.253479
371.469290	52.892524	74.258484
370.636671	54.647243	74.263489
370.500340	45.428007	74.268494
369.713157	52.988280	74.273498
368.751711	59.096667	74.278503
368.068676	49.639564	74.283508
367.420622	48.823459	74.288513
367.215734	52.150103	74.293518
365.953524	52.986926	74.298522
365.220358	38.124136	74.303527
364.567799	45.914346	74.308532
364.023079	59.816771	74.313537
363.945290	54.360173	74.318542
363.061532	53.719061	74.323546
361.988715	42.915691	74.328551
361.449913	43.530251	74.333556
360.844360	54.596030	74.338561
360.664844	52.236424	74.343566
359.503810	57.947200	74.348570
358.918911	49.607293	74.353575
358.435690	49.646310	74.358580
357.499251	53.267662	74.363585
357.436245	51.901712	74.368590
356.107521	64.063223	74.373594
355.353899	59.552139	74.378599
354.939471	57.612901	74.383604
354.153227	53.262532	74.388609
353.673115	45.399246	74.393614
352.464830	56.486620	74.398618
351.785038	42.533971	74.403623
351.473510	57.397816	74.408628
351.093296	56.116229	74.413633
350.921106	53.905358	74.418638
349.663166	55.995064	74.423642
348.960883	59.926004	74.428647
348.377433	48.482613	74.433652
347.885120	56.080769	74.438657
347.426470	46.380755	74.443662
346.325810	52.229992	74.448666
345.983444	55.090359	74.453671
345.457322	52.455439	74.458676
344.040277	53.166445	74.463681
343.461627	51.647305	74.468686
342.667376	53.247830	74.473690
342.293546	56.125826	74.478695
341.920306	52.012948	74.483700
340.870211	62.669030	74.488705
340.278038	49.558284	74.493710
339.333963	52.057593	74.498714
339.053850	55.304373	74.503719
338.655642	46.662097	74.508724
337.881388	50.897459	74.513729
337.332982	45.953340	74.518734
335.841834	51.516235	74.523738
335.432680	51.446644	74.528743
335.189498	43.520651	74.533748
334.642649	56.452443	74.538753
334.352831	47.132024	74.543758
333.138872	56.103920	74.548762
332.451906	59.715281	74.553767
332.289016	48.738598	74.558772
331.052932	50.814300	74.563777
329.755046	52.820862	74.568782
329.718502	53.099491	74.573786
329.266424	49.724032	74.578791
328.922816	51.787685	74.583796
328.139123	51.453885	74.588801
327.199643	43.559211	74.593806
326.705513	54.320516	74.598810
325.939778	49.097875	74.603815
324.654545	54.137617	74.608820
323.987579	60.394869	74.613825
323.537761	51.690389	74.618830
323.234313	55.508767	74.623834
322.563579	48.707174	74.628839
322.105404	49.622901	74.633844
321.517624	58.195785	74.638849
320.834497	45.469300	74.643854
319.844803	59.156295	74.648858
319.461844	56.363034	74.653863
318.875651	50.669516	74.658868
317.652484	66.533117	74.663873
317.211862	47.131510	74.668878
316.765633	61.740959	74.673882
315.911713	57.972163	74.678887
315.458759	48.756675	74.683892
314.597847	53.024656	74.688897
313.937180	57.017147	74.693902
313.134370	56.544134	74.698906
312.739146	54.704235	74.703911
312.378633	51.461102	74.708916
311.471204	64.775209	74.713921
310.858220	54.946921	74.718926
310.252360	60.642287	74.723930
309.425578	53.994932	74.728935
308.721853	49.122436	74.733940
307.726869	63.226369	74.738945
307.195533	56.310495	74.743950
306.822107	54.359104	74.748954
305.910811	51.270765	74.753959
305.310369	52.795843	74.758964
304.666970	57.472966	74.763969
304.115870	51.314779	74.768974
303.598139	53.324993	74.773978
302.730376	48.808225	74.778983
301.850366	51.940733	74.783988
301.232943	56.431441	74.788993
301.065274	55.147769	74.793998
300.441635	56.224482	74.799002
299.727123	55.717392	74.804007
298.671906	45.955437	74.809012
298.108832	53.154429	74.814017
297.672214	45.732488	74.819022
296.551189	50.179255	74.824026
295.397401	45.233121	74.829031
295.084308	47.371672	74.834036
294.208954	52.173414	74.839041
294.252918	44.079402	74.844046
294.057352	51.219746	74.849050
293.607726	47.317719	74.854055
292.385590	48.728711	74.859060
291.449335	51.964407	74.864065
291.250048	51.110078	74.869070
290.051609	55.949830	74.874074
289.031592	49.420072	74.879079
288.768208	47.174708	74.884084
287.955266	50.195859	74.889089
287.491063	41.129143	74.894094
286.926762	42.218975	74.899098
286.604460	51.756030	74.904103
285.613793	46.191054	74.909108
285.073152	43.849536	74.914113
284.549268	42.113400	74.919118
283.531198	44.716185	74.924122
282.397244	45.946679	74.929127
282.237182	46.480543	74.934132
281.153600	43.439503	74.939137
281.150432	43.381247	74.944142
280.651072	48.302875	74.949146
279.908788	43.471729	74.954151
278.958205	43.009842	74.959156
278.236489	48.577441	74.964161
277.903401	33.248634	74.969166
277.296848	41.450935	74.974170
276.491231	42.278200	74.979175
275.689081	34.327640	74.984180
275.162548	43.065272	74.989185
274.691617	41.196121	74.994190
273.483111	49.267537	74.999194
272.850295	47.232329	75.004199
272.306087	37.039795	75.009204
272.149728	38.075099	75.014209
270.881254	48.319426	75.019214
269.936558	51.043051	75.024218
269.173371	50.198540	75.029223
268.619446	43.196161	75.034228
268.504356	57.587012	75.039233
268.064412	41.361964	75.044238
267.373871	44.681066	75.049242
266.437731	43.453725	75.054247
265.890728	41.859704	75.059252
265.306909	51.933790	75.064257
264.685769	48.934665	75.069262
263.572069	45.971813	75.074266
262.544263	51.640034	75.079271
262.306693	44.832495	75.084276
262.135660	51.430639	75.089281
261.896804	41.280103	75.094286
260.150101	48.738023	75.099290
259.271407	45.710814	75.104295
259.332907	49.694387	75.109300
258.870677	50.909218	75.114305
258.631025	45.500900	75.119310
257.606241	47.114505	75.124314
256.286882	52.323522	75.129319
255.267235	44.731934	75.134324
254.545198	48.688371	75.139329
254.204579	44.840688	75.144334
253.784929	51.339350	75.149338
252.988743	47.344767	75.154343
252.554804	43.255727	75.159348
252.088204	58.336395	75.164353
251.869877	44.852538	75.169358
250.567148	48.191317	75.174362
250.029256	52.435910	75.179367
249.618839	40.950653	75.184372
248.260428	52.808989	75.189377
247.595797	52.278358	75.194382
247.030856	51.646171	75.199386
246.366530	56.273600	75.204391
246.359546	46.277911	75.209396
245.607519	54.987495	75.214401
244.802667	52.952570	75.219406
244.318292	44.308504	75.224410
243.429095	52.825690	75.229415
242.318881	47.512914	75.234420
241.227235	54.499372	75.239425
241.295330	54.576523	75.244430
240.450505	51.223399	75.249434
239.819167	46.488105	75.254439
239.557155	46.767489	75.259444
238.995536	56.539370	75.264449
238.762610	49.161071	75.269454
237.718891	56.224573	75.274458
236.537586	55.547652	75.279463
236.007321	44.293321	75.284468
235.023767	54.853139	75.289473
234.625430	53.988329	75.294478
234.139163	50.019964	75.299482
233.578700	57.104047	75.304487
233.031750	47.565629	75.309492
231.596958	56.658679	75.314497
231.304324	52.191361	75.319502
230.623197	50.930184	75.324506
230.103672	52.941107	75.329511
230.188895	52.401148	75.334516
228.826554	56.007900	75.339521
227.682099	53.639240	75.344526
227.284473	46.590341	75.349530
226.711029	50.602228	75.354535
226.328278	46.841501	75.359540
225.405407	53.750087	75.364545
224.668203	48.154706	75.369550
224.296404	46.572102	75.374554
223.488799	49.499195	75.379559
223.025264	49.787467	75.384564
221.576796	56.631026	75.389569
221.092002	49.684695	75.394574
220.695680	53.993833	75.399578
220.398168	61.595706	75.404583
220.366052	56.323120	75.409588
218.803581	59.035420	75.414593
218.065940	53.184339	75.419598
217.837005	54.877047	75.424602
217.190389	56.095070	75.429607
216.321138	46.786367	75.434612
215.204903	56.954878	75.439617
214.814806	47.041836	75.444622
214.689569	49.272130	75.449626
213.651836	54.057904	75.454631
212.919267	48.251744	75.459636
212.081937	52.996062	75.464641
211.791112	52.091116	75.469646
211.237135	50.417775	75.474650
210.115417	61.726371	75.479655
209.584925	50.457082	75.484660
208.912623	55.678740	75.489665
208.589069	52.092198	75.494670
207.741469	53.504532	75.499674
206.745701	59.557644	75.504679
205.904249	59.365205	75.509684
205.346201	59.078005	75.514689
205.351565	62.131389	75.519694
204.512599	60.748858	75.524698
203.734057	63.077326	75.529703
202.863056	57.806048	75.534708
202.267892	64.699122	75.539713
202.224673	51.077496	75.544718
201.474382	56.962221	75.549722
200.473623	62.933301	75.554727
199.901713	55.292209	75.559732
199.204893	58.109928	75.564737
198.111751	60.072349	75.569742
197.209571	46.922028	75.574746
196.550318	56.980236	75.579751
196.074336	49.455722	75.584756
195.863641	63.806909	75.589761
195.587299	63.288274	75.594766
194.935332	54.779118	75.599770
193.319179	62.042985	75.604775
193.104771	54.764140	75.609780
192.217835	61.049242	75.614785
191.765489	64.875781	75.619790
191.670153	54.858135	75.624794
190.643010	66.254729	75.629799
189.952826	45.926132	75.634804
189.088408	50.348273	75.639809
188.353959	53.480318	75.644814
187.524585	56.771523	75.649818
186.717673	59.546934	75.654823
186.168285	54.890753	75.659828
185.517403	58.900525	75.664833
185.385699	55.086505	75.669838
185.057399	52.664788	75.674842
184.065112	48.186761	75.679847
183.450287	48.888579	75.684852
182.497399	58.487944	75.689857
182.043550	50.999504	75.694862
180.660726	55.585509	75.699866
180.075382	60.060467	75.704871
179.746588	49.581955	75.709876
179.123209	55.570839	75.714881
179.120897	53.576764	75.719886
178.425396	53.719684	75.724890
177.354866	58.657922	75.729895
176.696709	50.813346	75.734900
175.903199	57.730551	75.739905
175.445162	52.766230	75.744910
174.264756	56.339045	75.749914
173.384136	54.642366	75.754919
173.112691	42.752009	75.759924
172.454682	50.419620	75.764929
172.351541	49.519212	75.769934
171.754176	54.132405	75.774938
170.993319	60.190251	75.779943
170.609987	57.657580	75.784948
169.325802	62.676654	75.789953
168.373726	57.695187	75.794958
167.832364	61.167929	75.799962
167.169049	51.894589	75.804967
166.677108	51.037937	75.809972
165.935172	58.762964	75.814977
165.150288	52.844998	75.819982
164.579874	50.168359	75.824986
163.961048	50.943887	75.829991
163.456673	51.303898	75.834996
162.769103	55.558368	75.840001
162.513987	50.215864	75.845006
161.106972	48.080510	75.850010
160.745564	49.396875	75.855015
160.358045	40.416507	75.860020
159.536908	51.308860	75.865025
158.690982	51.187061	75.870030
157.821816	47.166327	75.875034
157.478468	51.271004	75.880039
157.309720	48.304865	75.885044
156.424000	54.307146	75.890049
155.362469	49.822840	75.895054
154.469568	55.017586	75.900058
153.886104	54.851584	75.905063
153.755052	45.598710	75.910068
153.192906	51.131862	75.915073
151.995400	46.534692	75.920078
151.506515	52.015420	75.925082
150.619747	55.320809	75.930087
150.889347	50.623705	75.935092
149.504599	57.857781	75.940097
148.352224	52.571205	75.945102
148.257892	56.301636	75.950106
147.744220	65.045366	75.955111
147.446512	55.335560	75.960116
146.066759	66.103832	75.965121
144.935671	58.096006	75.970126
144.937212	56.035749	75.975130
144.464893	53.920550	75.980135
143.857650	54.086632	75.985140
142.901106	61.056263	75.990145
142.248629	60.193584	75.995150
141.913068	55.750606	76.000154
140.689621	51.141308	76.005159
139.771686	53.020024	76.010164
139.133314	50.842509	76.015169
138.249060	42.578839	76.020174
138.140233	47.279588	76.025178
137.813301	57.668040	76.030183
137.701447	54.450978	76.035188
136.860103	54.282611	76.040193
135.797752	44.811259	76.045198
135.162228	49.080095	76.050202
134.156061	53.562859	76.055207
133.333556	48.439593	76.060212
132.678637	54.378233	76.065217
132.185314	51.756273	76.070222
132.053156	46.447954	76.075226
131.853190	56.677674	76.080231
130.693317	43.533269	76.085236
129.721513	50.170402	76.090241
128.961585	50.289639	76.095246
128.215492	38.748279	76.100250
127.293174	48.009265	76.105255
126.891410	43.575669	76.110260
125.919173	49.938552	76.115265
125.659729	50.114086	76.120270
125.510730	47.888992	76.125274
124.612750	50.270312	76.130279
123.681831	38.611437	76.135284
122.797694	48.884631	76.140289
121.920425	48.757949	76.145294
121.603285	47.721345	76.150298
121.229404	51.551406	76.155303
121.035315	43.917798	76.160308
119.953150	50.992248	76.165313
119.282115	49.848167	76.170318
118.997791	44.298322	76.175322
117.473416	53.820410	76.180327
117.010071	40.624099	76.185332
116.089542	58.002833	76.190337
115.683476	50.029402	76.195342
115.360644	43.849883	76.200346
114.380430	51.817852	76.205351
113.513369	46.228180	76.210356
113.056658	46.878823	76.215361
112.499140	40.150234	76.220366
111.749383	42.763890	76.225370
111.439338	53.123787	76.230375
111.097438	42.990940	76.235380
110.116289	50.648430	76.240385
109.554787	45.002429	76.245390
109.106226	45.982049	76.250394
107.795596	45.278784	76.255399
107.361743	44.977409	76.260404
106.908721	48.076216	76.265409
105.996903	51.375644	76.270414
105.240846	42.421758	76.275418
104.323628	47.664490	76.280423
103.864063	47.067148	76.285428
103.593291	52.757574	76.290433
102.438681	52.762912	76.295438
101.717004	52.002887	76.300442
101.033524	56.038781	76.305447
100.564415	47.476593	76.310452
100.150173	53.388183	76.315457
99.813549	44.912619	76.320462
98.934574	40.174812	76.325466
97.887322	51.292237	76.330471
97.483044	44.681053	76.335476
96.526961	52.940132	76.340481
95.113265	56.611377	76.345486
95.013601	46.987625	76.350490
94.354290	51.304752	76.355495
93.958483	49.019741	76.360500
93.659158	50.074824	76.365505
93.552409	43.335269	76.370510
92.585807	42.884456	76.375514
91.363935	49.718798	76.380519
90.882006	49.243705	76.385524
89.461399	49.832642	76.390529
89.112810	53.266814	76.395534
88.434928	51.460794	76.400538
87.968186	55.551105	76.405543
87.687116	47.393234	76.410548
87.187092	48.067488	76.415553
86.377583	45.067137	76.420558
85.668446	45.600411	76.425562
84.463478	53.819272	76.430567
84.513860	51.954710	76.435572
83.355274	51.767720	76.440577
82.363905	49.988211	76.445582
81.935164	47.165724	76.450586
81.431150	55.352829	76.455591
81.046138	49.255415	76.460596
80.812053	51.494108	76.465601
79.392475	45.361711	76.470606
78.609717	49.158063	76.475610
78.061334	56.480066	76.480615
77.970772	37.247857	76.485620
76.564243	38.942340	76.490625
75.646039	49.754634	76.495630
75.163229	45.392963	76.500634
74.789410	53.766153	76.505639
74.335889	53.744847	76.510644
74.035769	50.928334	76.515649
73.177792	60.724583	76.520654
72.236693	52.572903	76.525658
71.352315	56.074462	76.530663
71.232071	47.368790	76.535668
70.507600	54.724929	76.540673
69.320483	59.450689	76.545678
68.994534	52.518201	76.550682
68.311153	59.162736	76.555687
68.188679	40.699370	76.560692
66.806345	54.567765	76.565697
65.633881	58.441987	76.570702
65.589998	49.894922	76.575706
65.064427	55.083541	76.580711
64.717495	46.467259	76.585716
63.394689	52.222007	76.590721
62.796648	49.451442	76.595726
62.350857	49.302504	76.600730
61.644524	60.477535	76.605735
61.479325	51.957979	76.610740
60.348355	54.706867	76.615745
59.309304	46.058467	76.620750
59.191040	46.222432	76.625754
58.485697	55.597403	76.630759
57.937457	45.334161	76.635764
56.907281	57.389267	76.640769
56.088527	47.621981	76.645774
55.898469	46.332688	76.650778
55.327336	55.867007	76.655783
54.444475	44.863028	76.660788
53.301929	49.679035	76.665793
52.947896	54.901793	76.670798
52.539821	45.230667	76.675802
51.835407	54.521406	76.680807
51.152548	41.729828	76.685812
50.254764	47.763002	76.690817
49.358965	52.075287	76.695822
49.017449	43.473079	76.700826
48.671313	57.091591	76.705831
48.269011	49.104896	76.710836
47.051729	45.130848	76.715841
46.056484	53.705707	76.720846
46.004816	49.431951	76.725850
45.437203	55.925989	76.730855
45.248369	55.201714	76.735860
43.910954	45.186273	76.740865
43.033853	56.465971	76.745870
42.787740	42.559052	76.750874
41.374757	50.941865	76.755879
40.843852	46.217415	76.760884
40.149468	55.442886	76.765889
39.693371	52.411949	76.770894
39.667794	49.303647	76.775898
38.858992	58.707807	76.780903
38.012808	52.019246	76.785908
36.931078	56.813779	76.790913
36.557975	54.773945	76.795918
36.371719	55.126004	76.800922
35.297267	53.073400	76.805927
34.053557	51.792665	76.810932
33.842702	53.694240	76.815937
33.447942	50.192948	76.820942
33.169175	49.576061	76.825946
32.228618	55.994314	76.830951
31.690843	51.310512	76.835956
30.635400	51.739364	76.840961
29.611277	58.072873	76.845966
28.771713	47.671307	76.850970
27.930900	45.738112	76.855975
27.880709	50.450119	76.860980
27.396978	51.691945	76.865985
26.763743	55.656078	76.870990
26.690101	51.685281	76.875994
25.345345	58.776747	76.880999
24.716613	50.163788	76.886004
23.982359	53.252007	76.891009
23.203191	55.511138	76.896014
23.353275	53.784209	76.901018
22.225791	58.195430	76.906023
21.515080	50.459368	76.911028
21.003831	47.124884	76.916033
19.666647	60.432559	76.921038
19.219753	50.749146	76.926042
18.376475	57.747132	76.931047
17.806746	54.768047	76.936052
17.408215	56.074997	76.941057
16.760645	52.660866	76.946062
16.661603	54.982190	76.951066
15.352638	57.141514	76.956071
14.665026	49.851860	76.961076
13.914840	54.877691	76.966081
13.652642	56.758072	76.971086
12.837318	49.153626	76.976090
11.992238	56.365855	76.981095
11.299191	48.361127	76.986100
10.590492	56.547015	76.991105
10.628431	53.640967	76.996110
9.881586	55.233020	77.001114
8.408659	55.851872	77.006119
7.635823	46.542093	77.011124
7.542172	39.262705	77.016129
6.975898	53.367742	77.021134
6.765618	48.680685	77.026139
5.658461	55.614580	77.031143
5.232646	52.011649	77.036148
4.222887	49.944410	77.041153
3.308007	51.171352	77.046158