Tue Jun 08 17:45:47 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.366802	95.407035	0.000000
-1.523735	75.757092	0.005005
-2.595644	52.490207	0.010010
-3.662130	3.077112	0.015014
-7.505870	-22.995630	0.020019
-13.054693	-20.660343	0.025024
-17.990007	-26.409717	0.030029
-22.782161	-22.563742	0.035034
-27.090757	-20.756074	0.040038
-30.857331	-13.698139	0.045043
-34.420859	-22.870792	0.050048
-37.633960	-26.105897	0.055053
-41.699192	-27.367374	0.060058
-45.127747	-27.731507	0.065062
-49.015854	-26.965724	0.070067
-52.715235	-21.074615	0.075072
-56.527475	-33.003488	0.080077
-60.608753	-21.925916	0.085082
-63.958553	-31.369249	0.090086
-67.921886	-21.169601	0.095091
-71.741366	-28.661857	0.100096
-75.288153	-33.576044	0.105101
-79.197168	-27.475693	0.110106
-82.988763	-29.129032	0.115110
-86.856371	-26.588167	0.120115
-90.627251	-23.673517	0.125120
-94.541650	-20.092453	0.130125
-97.710670	-24.702350	0.135130
-101.251456	-31.173098	0.140134
-105.391022	-20.934517	0.145139
-109.519955	-30.019219	0.150144
-112.840685	-26.676911	0.155149
-116.998140	-30.688634	0.160154
-120.883496	-26.506650	0.165158
-124.601238	-25.504773	0.170163
-128.344585	-17.276487	0.175168
-131.776375	-30.446768	0.180173
-135.711516	-23.945206	0.185178
-139.082111	-28.464454	0.190182
-143.339527	-23.609609	0.195187
-146.846703	-26.923665	0.200192
-150.728065	-26.488930	0.205197
-154.865642	-25.780136	0.210202
-158.433115	-21.390548	0.215206
-162.375783	-18.399803	0.220211
-166.320799	-18.117154	0.225216
-169.552301	-30.693371	0.230221
-173.271892	-22.571753	0.235226
-177.034652	-31.163432	0.240230
-180.727926	-21.868508	0.245235
-184.752395	-17.200012	0.250240
-187.950746	-18.518850	0.255245
-191.950660	-14.319133	0.260250
-195.747629	-13.332423	0.265254
-199.755085	-25.584895	0.270259
-203.682276	-14.847823	0.275264
-206.789518	-23.452437	0.280269
-210.626280	-17.184381	0.285274
-214.056411	-19.484958	0.290278
-218.533184	-24.495300	0.295283
-222.335986	-20.175428	0.300288
-226.262549	-26.558593	0.305293
-230.039262	-19.597844	0.310298
-233.642139	-27.172097	0.315302
-236.988408	-27.235614	0.320307
-240.726539	-21.591516	0.325312
-244.723120	-16.731977	0.330317
-248.711675	-11.576198	0.335322
-252.423226	-28.863762	0.340326
-256.258328	-26.438062	0.345331
-259.565441	-27.902391	0.350336
-263.177452	-29.647558	0.355341
-267.526314	-20.371168	0.360346
-271.088173	-34.201069	0.365350
-274.673966	-21.087147	0.370355
-278.953725	-22.521203	0.375360
-282.776179	-26.682984	0.380365
-286.448762	-23.693069	0.385370
-290.254633	-15.627610	0.390374
-293.793835	-28.686960	0.395379
-297.366644	-25.090115	0.400384
-300.923695	-33.265809	0.405389
-305.086888	-26.285290	0.410394
-308.450251	-32.219095	0.415398
-312.285171	-22.244168	0.420403
-316.292414	-21.231948	0.425408
-320.165780	-23.560220	0.430413
-324.089391	-22.527209	0.435418
-327.847546	-29.692664	0.440422
-331.202307	-22.238994	0.445427
-335.040092	-20.094589	0.450432
-338.460992	-19.958531	0.455437
-342.605723	-24.696117	0.460442
-346.281735	-25.263871	0.465446
-350.065962	-20.954187	0.470451
-354.284112	-22.391634	0.475456
-357.528529	-26.934325	0.480461
-361.424070	-21.092618	0.485466
-365.464962	-25.998377	0.490470
-368.786170	-21.270772	0.495475
-372.348110	-25.044165	0.500480
-376.364876	-24.558379	0.505485
-380.671748	-23.543646	0.510490
-384.230560	-31.038881	0.515494
-387.645311	-26.892018	0.520499
-391.433733	-28.252762	0.525504
-395.180008	-35.495973	0.530509
-399.630481	-24.556499	0.535514
-402.429742	-23.458556	0.540518
-406.486578	-29.570138	0.545523
-410.526579	-26.848651	0.550528
-413.711829	-31.206461	0.555533
-417.912686	-27.366792	0.560538
-421.663078	-39.946918	0.565542
-425.199982	-30.439454	0.570547
-429.401799	-27.589539	0.575552
-433.047448	-30.092555	0.580557
-436.832774	-28.534525	0.585562
-440.443144	-23.859493	0.590566
-444.137612	-28.077818	0.595571
-448.157546	-17.975921	0.600576
-451.750305	-23.323980	0.605581
-455.395396	-22.427842	0.610586
-459.182693	-23.515977	0.615590
-462.795218	-27.312981	0.620595
-466.704452	-10.796698	0.625600
-470.407233	-28.383944	0.630605
-474.470800	-27.576247	0.635610
-478.192897	-29.692715	0.640614
-481.705209	-31.061280	0.645619
-485.824315	-28.424437	0.650624
-488.968688	-32.833804	0.655629
-493.271270	-15.772819	0.660634
-496.786932	-15.741951	0.665638
-500.593686	-22.356187	0.670643
-504.498063	-23.055932	0.675648
-507.991527	-27.240798	0.680653
-512.084301	-25.522989	0.685658
-515.609349	-23.132901	0.690662
-519.320701	-22.908977	0.695667
-523.535575	-20.044893	0.700672
-526.658338	-23.556822	0.705677
-530.906936	-27.119904	0.710682
-534.495968	-29.055880	0.715686
-537.954260	-28.428945	0.720691
-542.015264	-21.056045	0.725696
-545.649705	-30.469865	0.730701
-549.182600	-21.832145	0.735706
-553.142050	-22.956971	0.740710
-557.005574	-24.641371	0.745715
-561.517013	-26.631407	0.750720
-564.642155	-30.579445	0.755725
-568.329945	-19.721346	0.760730
-571.737002	-28.303431	0.765734
-575.652934	-27.514658	0.770739
-579.653480	-22.255501	0.775744
-583.001502	-29.271636	0.780749
-587.161631	-23.936542	0.785754
-591.073050	-25.612298	0.790758
-595.008119	-35.049083	0.795763
-598.565422	-20.102469	0.800768
-602.006828	-26.146976	0.805773
-606.100220	-21.945866	0.810778
-609.198124	-20.581432	0.815782
-613.446546	-16.463046	0.820787
-617.293280	-21.697911	0.825792
-620.851947	-29.824494	0.830797
-624.945920	-21.813941	0.835802
-628.576230	-20.403525	0.840806
-632.639939	-22.853973	0.845811
-636.295109	-20.546850	0.850816
-640.006863	-31.635874	0.855821
-643.851079	-24.444160	0.860826
-647.416684	-23.756885	0.865830
-651.087701	-29.819969	0.870835
-655.007657	-21.088123	0.875840
-658.401904	-28.860812	0.880845
-662.290497	-19.844626	0.885850
-666.091702	-26.631749	0.890854
-669.815212	-21.779635	0.895859
-674.110640	-21.650334	0.900864
-677.196816	-30.728676	0.905869
-681.019663	-27.821994	0.910874
-684.966246	-30.330778	0.915878
-688.397926	-32.150348	0.920883
-692.541025	-26.010511	0.925888
-696.132290	-29.220479	0.930893
-700.234176	-27.173326	0.935898
-703.639176	-27.470340	0.940902
-707.572155	-30.642573	0.945907
-711.421820	-23.693798	0.950912
-715.048123	-28.066861	0.955917
-718.734881	-24.937600	0.960922
-722.391166	-29.257355	0.965926
-726.199506	-34.327400	0.970931
-730.430635	-28.951575	0.975936
-733.963702	-25.652114	0.980941
-737.273507	-17.958400	0.985946
-741.230830	-27.060064	0.990950
-744.806154	-27.959740	0.995955
-748.759003	-19.011793	1.000960
-752.764506	-28.371208	1.005965
-756.861566	-23.557143	1.010970
-760.312588	-19.665471	1.015974
-764.132299	-19.587336	1.020979
-767.632479	-14.970037	1.025984
-771.164891	-25.501210	1.030989
-775.054425	-16.512796	1.035994
-779.132939	-21.114877	1.040998
-782.698026	-28.322518	1.046003
-786.414137	-12.253205	1.051008
-790.383406	-24.762254	1.056013
-794.166205	-14.842477	1.061018
-797.702301	-18.300232	1.066022
-801.369724	-18.425426	1.071027
-805.739193	-14.170040	1.076032
-808.840571	-19.158476	1.081037
-812.715125	-15.277747	1.086042
-816.573652	-21.199165	1.091046
-820.205264	-18.207565	1.096051
-824.253417	-13.896795	1.101056
-828.285181	-22.155132	1.106061
-831.879549	-13.683483	1.111066
-835.278706	-15.256696	1.116070
-839.050203	-17.412525	1.121075
-843.169906	-13.648362	1.126080
-846.385850	-22.490366	1.131085
-849.992808	-14.114036	1.136090
-854.146412	-16.581998	1.141094
-857.873537	-26.992041	1.146099
-862.034263	-20.602334	1.151104
-865.166648	-21.956071	1.156109
-869.046161	-17.179247	1.161114
-873.086583	-22.780461	1.166118
-877.284298	-21.276389	1.171123
-881.370375	-14.122694	1.176128
-884.404021	-24.950941	1.181133
-888.080592	-23.295941	1.186138
-891.646664	-26.423229	1.191142
-895.351686	-27.302489	1.196147
-898.830439	-22.610618	1.201152
-902.856393	-26.092735	1.206157
-906.921738	-23.270539	1.211162
-910.564436	-17.060892	1.216166
-914.060228	-22.391244	1.221171
-917.881437	-11.508008	1.226176
-921.916811	-17.856827	1.231181
-926.022291	-20.421787	1.236186
-929.943105	-19.727379	1.241190
-933.342553	-16.859220	1.246195
-937.025573	-16.211548	1.251200
-940.563796	-24.897100	1.256205
-944.621758	-20.075368	1.261210
-948.324350	-17.424742	1.266214
-952.011009	-20.314978	1.271219
-955.842901	-14.537384	1.276224
-959.325282	-27.271144	1.281229
-963.195317	-16.000970	1.286234
-967.151778	-24.619432	1.291238
-970.816013	-29.635441	1.296243
-974.977221	-28.734339	1.301248
-977.816739	-26.613542	1.306253
-981.849850	-25.893887	1.311258
-985.812687	-27.039439	1.316262
-989.697317	-25.519148	1.321267
-993.890459	-21.051898	1.326272
-996.821457	-33.009953	1.331277
-1000.899754	-30.952362	1.336282
-1004.790754	-32.298109	1.341286
-1008.438551	-29.748808	1.346291
-1012.559003	-16.561932	1.351296
-1015.742595	-19.757939	1.356301
-1019.712777	-17.776519	1.361306
-1023.347392	-31.833972	1.366310
-1027.034887	-29.965418	1.371315
-1031.006760	-22.143624	1.376320
-1034.889083	-26.965039	1.381325
-1038.611828	-17.459566	1.386330
-1042.136994	-15.565583	1.391334
-1046.081426	-28.396361	1.396339
-1049.998130	-30.887432	1.401344
-1053.387988	-39.126276	1.406349
-1057.423175	-28.960092	1.411354
-1061.244447	-26.974994	1.416358
-1064.510386	-33.217371	1.421363
-1068.567130	-25.309138	1.426368
-1072.377362	-33.611569	1.431373
-1076.130473	-31.563957	1.436378
-1080.246997	-28.771101	1.441382
-1083.444020	-23.002553	1.446387
-1087.718146	-18.897859	1.451392
-1090.821985	-30.925626	1.456397
-1094.559849	-29.381893	1.461402
-1098.728895	-22.057855	1.466406
-1102.720927	-27.859366	1.471411
-1106.299324	-21.519698	1.476416
-1110.137074	-24.990510	1.481421
-1113.907279	-17.058811	1.486426
-1117.471288	-21.649828	1.491430
-1121.195823	-20.926190	1.496435
-1124.965683	-15.678540	1.501440
-1128.829022	-27.128658	1.506445
-1132.558867	-17.332179	1.511450
-1136.554599	-20.735185	1.516454
-1140.016514	-20.498698	1.521459
-1144.168086	-16.268164	1.526464
-1147.757381	-16.548571	1.531469
-1151.153055	-17.372183	1.536474
-1154.920948	-24.562817	1.541478
-1158.669207	-34.009793	1.546483
-1162.577666	-22.656691	1.551488
-1166.172345	-24.348809	1.556493
-1170.328289	-13.128444	1.561498
-1174.346485	-17.045805	1.566502
-1177.457484	-23.373115	1.571507
-1181.755890	-17.898874	1.576512
-1184.888042	-25.362850	1.581517
-1189.184087	-21.898849	1.586522
-1193.156465	-15.972599	1.591526
-1196.395204	-24.458706	1.596531
-1200.378974	-14.366349	1.601536
-1203.962162	-25.850291	1.606541
-1207.548842	-26.200564	1.611546
-1211.239068	-17.431141	1.616550
-1215.181773	-23.849648	1.621555
-1219.439864	-19.762581	1.626560
-1222.564110	-24.116024	1.631565
-1226.429310	-19.713560	1.636570
-1230.220490	-20.791658	1.641574
-1233.714658	-25.927417	1.646579
-1238.185611	-15.305343	1.651584
-1241.886422	-28.881115	1.656589
-1245.756310	-23.360813	1.661594
-1249.296103	-18.958956	1.666598
-1252.640751	-25.223578	1.671603
-1256.917597	-22.399073	1.676608
-1259.975000	-29.016549	1.681613
-1263.975102	-26.489416	1.686618
-1267.884277	-21.375603	1.691622
-1271.469444	-23.798679	1.696627
-1275.462763	-19.995433	1.701632
-1279.005144	-23.411824	1.706637
-1283.238299	-15.803469	1.711642
-1287.031627	-13.854547	1.716646
-1290.653962	-24.491748	1.721651
-1294.129912	-15.850240	1.726656
-1297.692289	-20.142584	1.731661
-1301.891622	-19.816016	1.736666
-1305.836285	-25.033007	1.741670
-1309.421625	-19.890707	1.746675
-1313.285925	-20.094529	1.751680
-1316.859813	-25.380718	1.756685
-1320.072840	-21.110319	1.761690
-1324.060345	-25.582624	1.766694
-1328.086814	-20.450190	1.771699
-1332.089686	-17.868837	1.776704
-1335.460460	-20.743517	1.781709
-1339.870251	-18.806678	1.786714
-1343.888809	-7.271890	1.791718
-1346.948864	-19.471161	1.796723
-1350.681475	-20.201607	1.801728
-1354.239952	-29.163137	1.806733
-1357.908716	-25.649231	1.811738
-1361.923443	-12.573372	1.816742
-1365.922486	-28.194067	1.821747
-1369.846844	-12.574459	1.826752
-1373.146931	-26.046839	1.831757
-1376.665155	-16.456243	1.836762
-1380.348862	-17.176512	1.841766
-1383.952630	-15.621220	1.846771
-1388.298351	-13.778226	1.851776
-1392.215872	-16.914174	1.856781
-1396.101931	-15.477341	1.861786
-1399.917616	-13.471588	1.866790
-1403.171423	-24.661418	1.871795
-1407.090298	-18.213688	1.876800
-1410.498962	-21.672668	1.881805
-1415.282745	-24.927788	1.886810
-1418.522720	-11.185694	1.891814
-1422.289233	-23.805468	1.896819
-1426.252065	-19.296853	1.901824
-1429.630746	-19.933698	1.906829
-1433.331993	-23.380683	1.911834
-1436.987597	-13.597902	1.916838
-1440.794027	-18.758381	1.921843
-1445.033992	-26.849657	1.926848
-1448.384712	-26.384144	1.931853
-1452.213594	-14.903958	1.936858
-1456.233400	-24.581866	1.941862
-1459.699538	-25.132614	1.946867
-1463.726605	-20.668979	1.951872
-1467.173456	-24.796688	1.956877
-1471.211976	-21.432698	1.961882
-1474.813036	-18.380287	1.966886
-1478.442929	-22.956896	1.971891
-1482.353826	-16.950566	1.976896
-1486.208460	-22.069563	1.981901
-1489.622034	-22.867718	1.986906
-1493.595692	-24.224462	1.991910
-1496.836921	-25.263387	1.996915
-1501.570745	-17.400661	2.006912
-1502.346998	-28.599905	2.016909
-1499.728233	-21.095407	2.026906
-1496.888263	-24.439078	2.036902
-1494.406453	-25.458244	2.046899
-1492.928569	-22.957508	2.056896
-1491.178993	-23.273472	2.066893
-1489.356194	-26.098554	2.076890
-1487.375239	-22.781980	2.086886
-1485.092632	-25.680523	2.096883
-1483.364994	-29.188775	2.106880
-1481.476203	-28.227622	2.116877
-1479.589203	-28.652556	2.126874
-1477.853834	-24.391522	2.136870
-1475.824777	-29.521327	2.146867
-1473.692045	-27.325552	2.156864
-1472.270523	-24.981904	2.166861
-1470.374193	-20.305488	2.176858
-1468.083908	-23.345246	2.186854
-1466.343904	-26.237508	2.196851
-1464.212527	-23.070069	2.206848
-1462.725845	-24.260116	2.216845
-1460.567050	-20.273767	2.226842
-1458.668391	-20.507042	2.236838
-1457.247274	-16.077794	2.246835
-1455.319876	-14.962806	2.256832
-1452.837069	-23.522329	2.266829
-1451.004486	-23.028524	2.276826
-1449.502261	-22.781881	2.286822
-1447.672187	-29.561084	2.296819
-1445.864020	-21.876983	2.306816
-1443.703045	-21.171242	2.316813
-1441.700888	-22.418612	2.326810
-1439.629760	-28.915151	2.336806
-1438.089932	-25.062352	2.346803
-1436.122504	-21.287355	2.356800
-1434.362904	-26.002123	2.366797
-1432.661514	-27.081629	2.376794
-1430.665867	-18.578443	2.386790
-1428.609892	-23.208566	2.396787
-1426.707434	-22.905388	2.406784
-1424.882125	-27.481260	2.416781
-1423.002583	-25.466838	2.426778
-1421.334117	-24.186418	2.436774
-1419.007714	-22.698902	2.446771
-1417.383539	-19.447864	2.456768
-1415.407654	-18.245940	2.466765
-1413.623702	-21.987530	2.476762
-1412.054398	-21.708924	2.486758
-1409.774417	-23.156161	2.496755
-1408.025635	-21.541748	2.506752
-1406.481274	-21.875778	2.516749
-1404.096353	-21.896151	2.526746
-1402.301544	-23.768676	2.536742
-1400.392435	-22.897131	2.546739
-1398.347634	-23.377591	2.556736
-1396.657649	-19.326878	2.566733
-1394.569211	-18.735908	2.576730
-1393.070757	-23.117298	2.586726
-1391.426549	-24.058918	2.596723
-1389.353274	-25.520433	2.606720
-1387.352541	-29.003632	2.616717
-1384.999221	-26.842934	2.626714
-1383.634854	-24.838801	2.636710
-1381.899122	-31.655917	2.646707
-1379.982330	-28.381621	2.656704
-1377.643886	-26.743598	2.666701
-1376.107553	-26.564046	2.676698
-1374.172506	-32.393778	2.686694
-1372.413313	-35.475442	2.696691
-1370.439871	-25.605333	2.706688
-1368.469731	-29.785161	2.716685
-1366.978877	-32.466227	2.726682
-1364.713592	-26.595578	2.736678
-1362.738811	-27.838604	2.746675
-1361.024243	-22.932122	2.756672
-1359.134784	-27.822114	2.766669
-1357.359745	-23.804174	2.776666
-1355.237705	-26.588122	2.786662
-1353.521729	-25.603944	2.796659
-1351.416444	-22.334345	2.806656
-1350.027425	-26.391426	2.816653
-1347.932777	-21.572354	2.826650
-1346.070807	-23.082129	2.836646
-1343.899273	-24.906704	2.846643
-1342.195639	-29.540685	2.856640
-1340.546291	-26.037054	2.866637
-1338.619461	-25.140859	2.876634
-1336.608518	-24.054788	2.886630
-1334.504242	-24.652929	2.896627
-1333.064284	-25.481192	2.906624
-1331.018336	-19.097012	2.916621
-1329.232228	-17.065705	2.926618
-1326.921692	-17.222251	2.936614
-1325.221655	-13.274800	2.946611
-1323.413090	-18.758719	2.956608
-1321.730197	-21.557333	2.966605
-1319.853987	-19.367210	2.976602
-1317.579493	-25.497490	2.986598
-1316.102488	-19.219508	2.996595
-1314.345146	-23.000752	3.006592
-1312.158325	-22.203740	3.016589
-1309.974515	-19.983056	3.026586
-1308.482290	-25.839856	3.036582
-1306.595762	-27.275580	3.046579
-1304.656515	-24.216144	3.056576
-1303.166056	-29.233211	3.066573
-1300.744627	-20.208686	3.076570
-1298.800242	-25.146819	3.086566
-1297.279811	-27.752715	3.096563
-1295.387453	-18.092715	3.106560
-1293.612632	-22.236990	3.116557
-1291.703219	-16.072786	3.126554
-1289.545415	-19.230788	3.136550
-1287.642486	-19.401485	3.146547
-1286.039382	-17.247038	3.156544
-1284.239266	-18.821648	3.166541
-1281.681479	-24.350446	3.176538
-1280.474509	-22.240596	3.186534
-1278.841240	-21.437415	3.196531
-1276.531360	-23.020136	3.206528
-1274.711935	-15.173864	3.216525
-1272.717471	-17.528797	3.226522
-1270.894778	-14.889194	3.236518
-1268.897375	-17.486894	3.246515
-1267.043609	-17.931714	3.256512
-1265.435478	-20.539621	3.266509
-1263.700303	-23.335336	3.276506
-1261.710163	-21.799461	3.286502
-1259.313741	-23.932547	3.296499
-1257.656106	-24.389127	3.306496
-1255.839835	-25.452725	3.316493
-1254.136530	-21.829088	3.326490
-1252.088130	-25.614451	3.336486
-1250.317344	-21.342400	3.346483
-1248.623533	-22.985684	3.356480
-1246.271371	-23.354054	3.366477
-1244.698394	-22.374122	3.376474
-1242.681888	-25.732709	3.386470
-1240.837572	-28.283157	3.396467
-1239.056335	-22.466436	3.406464
-1237.016516	-18.059180	3.416461
-1235.437961	-21.256790	3.426458
-1233.227087	-22.823670	3.436454
-1231.478695	-17.424179	3.446451
-1229.875522	-24.407392	3.456448
-1227.909864	-16.039633	3.466445
-1225.402843	-17.189440	3.476442
-1223.787077	-19.282894	3.486438
-1222.136770	-19.553243	3.496435
-1220.358371	-21.864326	3.506432
-1218.512568	-18.326007	3.516429
-1216.826467	-26.258526	3.526426
-1214.551980	-23.199708	3.536422
-1212.755362	-23.695157	3.546419
-1210.782105	-28.119695	3.556416
-1209.168689	-21.019739	3.566413
-1206.930949	-29.317314	3.576410
-1205.164917	-24.742089	3.586406
-1203.478846	-24.459350	3.596403
-1201.365601	-23.306600	3.606400
-1199.568048	-24.361428	3.616397
-1197.369280	-23.094129	3.626394
-1195.684408	-24.693965	3.636390
-1194.198334	-25.066914	3.646387
-1192.132467	-25.517694	3.656384
-1190.536418	-19.531613	3.666381
-1188.306572	-17.712794	3.676378
-1186.475680	-17.468354	3.686374
-1184.498814	-19.238869	3.696371
-1182.573391	-25.839513	3.706368
-1180.862783	-22.568045	3.716365
-1178.953970	-22.092347	3.726362
-1176.992032	-18.943870	3.736358
-1175.163177	-21.474248	3.746355
-1173.279732	-24.824972	3.756352
-1171.111267	-22.339158	3.766349
-1169.770477	-22.668180	3.776346
-1167.792761	-23.509692	3.786342
-1166.059099	-28.814698	3.796339
-1163.930889	-29.217284	3.806336
-1161.943472	-22.989739	3.816333
-1160.284669	-27.225885	3.826330
-1158.512134	-28.236878	3.836326
-1156.310931	-29.504464	3.846323
-1154.265962	-23.689123	3.856320
-1152.610279	-30.088510	3.866317
-1150.887320	-24.668017	3.876314
-1148.809054	-29.060764	3.886310
-1146.801521	-33.601818	3.896307
-1145.245841	-26.309334	3.906304
-1143.619892	-21.926206	3.916301
-1140.926675	-29.573195	3.926298
-1139.377744	-27.581701	3.936294
-1137.967989	-21.778602	3.946291
-1135.821074	-26.394570	3.956288
-1134.111165	-32.476028	3.966285
-1132.184256	-28.645704	3.976282
-1130.269566	-27.932286	3.986278
-1128.234265	-34.057364	3.996275
-1126.397318	-24.766371	4.006272
-1124.549384	-25.399038	4.016269
-1122.717111	-19.476412	4.026266
-1120.587501	-26.565796	4.036262
-1118.941248	-27.084787	4.046259
-1116.710201	-27.840147	4.056256
-1115.169315	-25.740949	4.066253
-1113.364927	-24.249778	4.076250
-1111.763665	-24.998958	4.086246
-1109.388824	-29.346181	4.096243
-1107.514652	-24.514808	4.106240
-1105.807235	-27.967279	4.116237
-1104.166525	-25.599876	4.126234
-1101.897653	-30.782555	4.136230
-1100.132857	-30.904551	4.146227
-1098.279222	-27.299545	4.156224
-1096.160913	-26.665338	4.166221
-1094.699540	-27.762386	4.176218
-1092.437780	-30.896250	4.186214
-1090.507730	-33.632879	4.196211
-1088.816517	-29.157390	4.206208
-1087.003536	-27.180783	4.216205
-1085.660084	-23.491331	4.226202
-1083.275693	-28.034229	4.236198
-1081.210924	-25.662168	4.246195
-1079.543446	-26.191902	4.256192
-1077.305558	-26.940512	4.266189
-1075.707925	-29.308236	4.276186
-1074.348980	-26.325312	4.286182
-1071.833795	-27.682336	4.296179
-1069.864126	-33.030992	4.306176
-1068.182307	-34.717597	4.316173
-1066.628266	-34.646888	4.326170
-1064.389368	-28.056195	4.336166
-1062.565454	-33.949321	4.346163
-1060.925453	-26.027873	4.356160
-1058.713696	-28.876487	4.366157
-1056.924489	-37.551077	4.376154
-1055.245081	-29.963629	4.386150
-1053.045225	-28.051851	4.396147
-1051.066835	-28.104979	4.406144
-1049.793870	-29.694899	4.416141
-1047.795655	-27.212985	4.426138
-1045.428487	-22.044536	4.436134
-1043.688728	-21.246504	4.446131
-1042.179644	-28.259349	4.456128
-1040.244039	-25.450907	4.466125
-1038.240372	-23.403867	4.476122
-1036.466887	-25.135839	4.486118
-1034.334019	-23.359173	4.496115
-1032.537878	-22.054670	4.506112
-1030.734353	-21.071556	4.516109
-1028.778978	-25.377942	4.526106
-1026.944901	-16.426675	4.536102
-1024.865793	-20.999335	4.546099
-1022.996846	-16.673287	4.556096
-1021.376249	-16.693031	4.566093
-1019.567164	-16.615507	4.576090
-1017.611586	-22.941851	4.586086
-1015.448371	-17.996043	4.596083
-1013.942119	-22.241518	4.606080
-1011.807739	-22.952167	4.616077
-1010.194392	-25.211513	4.626074
-1008.375309	-23.835453	4.636070
-1006.389990	-20.820930	4.646067
-1004.285168	-27.613947	4.656064
-1002.486053	-24.263536	4.666061
-1000.830027	-26.959801	4.676058
-998.566670	-23.864960	4.686054
-996.902958	-20.929194	4.696051
-995.121059	-25.489545	4.706048
-993.170321	-16.712422	4.716045
-990.722132	-21.825848	4.726042
-989.439743	-27.741382	4.736038
-987.926056	-26.948778	4.746035
-985.741977	-23.686978	4.756032
-983.874024	-18.139536	4.766029
-982.161482	-17.213894	4.776026
-979.680974	-22.897226	4.786022
-978.172237	-19.889001	4.796019
-976.036343	-17.729468	4.806016
-974.555305	-24.366376	4.816013
-972.600468	-16.327410	4.826010
-970.713615	-22.288619	4.836006
-969.106123	-17.620064	4.846003
-966.882717	-18.076045	4.856000
-964.662867	-20.432779	4.865997
-963.282349	-21.320273	4.875994
-961.254288	-13.674459	4.885990
-959.283562	-21.817011	4.895987
-957.702012	-18.815745	4.905984
-955.816474	-17.743527	4.915981
-953.710433	-16.479940	4.925978
-952.050589	-22.627441	4.935974
-949.826150	-20.153883	4.945971
-947.825413	-21.890055	4.955968
-946.221693	-18.186346	4.965965
-944.648449	-19.636504	4.975962
-942.717158	-19.083145	4.985958
-940.525175	-19.235728	4.995955
-938.604116	-14.271622	5.005952
-936.955870	-18.565954	5.015949
-934.856361	-18.843749	5.025946
-932.980391	-29.355521	5.035942
-931.300229	-24.185257	5.045939
-929.751717	-23.674073	5.055936
-927.559392	-25.362503	5.065933
-925.572416	-26.576993	5.075930
-924.001413	-25.291101	5.085926
-921.428456	-25.536740	5.095923
-919.824392	-26.751100	5.105920
-918.037919	-21.672983	5.115917
-916.200300	-25.470626	5.125914
-914.295370	-17.653075	5.135910
-912.559981	-20.262549	5.145907
-910.629621	-17.732558	5.155904
-908.726835	-25.391148	5.165901
-906.627721	-23.890803	5.175898
-905.133035	-24.744523	5.185894
-903.392405	-26.218657	5.195891
-901.407452	-23.609112	5.205888
-899.026596	-24.513778	5.215885
-897.394164	-26.584286	5.225882
-895.649260	-28.668569	5.235878
-893.612025	-26.326463	5.245875
-891.852162	-29.317953	5.255872
-889.936456	-26.872385	5.265869
-888.159059	-16.487760	5.275866
-886.198806	-27.549499	5.285862
-884.360910	-27.404144	5.295859
-882.531684	-24.302693	5.305856
-880.624356	-25.273874	5.315853
-878.918633	-26.755839	5.325850
-876.783438	-26.063558	5.335846
-874.940084	-31.157278	5.345843
-872.958326	-28.615938	5.355840
-871.206201	-20.190384	5.365837
-869.158022	-21.529967	5.375834
-867.388148	-23.661603	5.385830
-865.423201	-23.594564	5.395827
-863.590642	-21.716068	5.405824
-861.841718	-19.777369	5.415821
-859.802466	-20.501256	5.425818
-858.093102	-24.623463	5.435814
-856.524951	-28.259820	5.445811
-854.401882	-30.777337	5.455808
-852.671937	-25.469355	5.465805
-850.505188	-24.520055	5.475802
-848.552285	-20.583392	5.485798
-847.112622	-30.150776	5.495795
-844.784866	-27.932420	5.505792
-843.034849	-22.882789	5.515789
-841.333486	-20.685749	5.525786
-839.294426	-26.161233	5.535782
-837.395799	-21.814502	5.545779
-835.529682	-23.714453	5.555776
-833.573774	-31.085722	5.565773
-831.694914	-24.458383	5.575770
-829.889314	-21.704195	5.585766
-827.980600	-30.563242	5.595763
-826.438387	-24.154369	5.605760
-824.499354	-25.585857	5.615757
-822.359014	-22.371789	5.625754
-820.317516	-24.805732	5.635750
-818.825237	-16.688473	5.645747
-816.674368	-28.358732	5.655744
-814.711470	-30.343657	5.665741
-813.225355	-25.897656	5.675738
-811.132495	-26.817261	5.685734
-809.106863	-22.561478	5.695731
-807.280851	-23.548706	5.705728
-805.589082	-24.455981	5.715725
-803.506196	-25.441847	5.725722
-801.799977	-25.201532	5.735718
-800.087659	-26.512286	5.745715
-798.103542	-24.277604	5.755712
-796.190230	-22.951218	5.765709
-793.907108	-22.579509	5.775706
-792.600810	-23.472390	5.785702
-790.315425	-17.835647	5.795699
-788.669703	-17.356510	5.805696
-786.845637	-16.971612	5.815693
-785.016377	-20.594667	5.825690
-783.028642	-18.779918	5.835686
-780.950018	-23.736141	5.845683
-779.146872	-20.900096	5.855680
-777.457710	-13.593993	5.865677
-775.465258	-17.513009	5.875674
-773.555318	-18.346267	5.885670
-771.823964	-18.047415	5.895667
-770.138259	-18.161629	5.905664
-768.168746	-15.290502	5.915661
-766.085400	-12.752711	5.925658
-764.111028	-10.145232	5.935654
-762.100835	-13.241688	5.945651
-760.691036	-18.583058	5.955648
-758.522872	-18.284079	5.965645
-756.690978	-13.931387	5.975642
-754.949799	-15.799981	5.985638
-753.089571	-19.512125	5.995635
-751.026873	-17.976205	6.005632
-749.194781	-22.740317	6.015629
-747.401866	-20.806749	6.025626
-745.680638	-12.099571	6.035622
-743.725732	-18.912994	6.045619
-741.720068	-16.691071	6.055616
-739.739759	-25.197991	6.065613
-737.723400	-20.265951	6.075610
-736.097714	-20.579314	6.085606
-734.187706	-23.708754	6.095603
-732.364404	-22.859327	6.105600
-730.539290	-16.422686	6.115597
-728.514084	-13.548847	6.125594
-726.730920	-15.348360	6.135590
-724.763862	-18.201059	6.145587
-722.415507	-18.091863	6.155584
-721.051069	-16.160233	6.165581
-719.323365	-9.185975	6.175578
-717.559838	-17.814167	6.185574
-715.619162	-15.345531	6.195571
-713.496787	-18.245036	6.205568
-712.070197	-17.743676	6.215565
-709.675788	-11.761602	6.225562
-707.852528	-12.679945	6.235558
-706.194911	-12.701182	6.245555
-704.096687	-14.283245	6.255552
-702.239062	-15.431174	6.265549
-700.710167	-12.311293	6.275546
-698.415561	-15.222960	6.285542
-696.704894	-17.217507	6.295539
-694.320033	-17.837801	6.305536
-693.249578	-16.713718	6.315533
-691.209219	-20.141371	6.325530
-689.083262	-18.735631	6.335526
-687.594687	-20.151013	6.345523
-685.344917	-20.665519	6.355520
-683.385370	-16.192818	6.365517
-681.776268	-19.649608	6.375514
-679.955244	-12.566066	6.385510
-678.011149	-15.255929	6.395507
-676.057885	-15.509293	6.405504
-674.043988	-19.101549	6.415501
-671.928210	-14.401925	6.425498
-670.552405	-21.400890	6.435494
-668.679588	-13.371790	6.445491
-666.711416	-20.713490	6.455488
-665.044823	-16.782931	6.465485
-662.618990	-12.342811	6.475482
-660.894448	-12.121788	6.485478
-659.376296	-16.754533	6.495475
-657.448582	-12.473566	6.505472
-655.155039	-11.279947	6.515469
-653.269892	-17.198459	6.525466
-651.751207	-11.669957	6.535462
-649.806115	-6.428041	6.545459
-647.715423	-18.214782	6.555456
-646.134985	-18.943226	6.565453
-644.209477	-19.717446	6.575450
-642.228247	-14.134733	6.585446
-640.355446	-15.507351	6.595443
-638.811438	-19.092072	6.605440
-636.862271	-15.960897	6.615437
-634.418123	-9.253005	6.625434
-632.925715	-10.306617	6.635430
-631.255861	-13.365166	6.645427
-628.816463	-21.385277	6.655424
-626.917196	-19.169149	6.665421
-625.792111	-18.353600	6.675418
-623.765980	-14.000978	6.685414
-621.666878	-19.824981	6.695411
-619.524741	-23.381518	6.705408
-617.878282	-15.398126	6.715405
-615.885801	-17.443373	6.725402
-614.253087	-12.868708	6.735398
-612.295328	-18.488236	6.745395
-610.764360	-9.276062	6.755392
-608.163320	-15.660053	6.765389
-606.634189	-7.441917	6.775386
-604.726995	-14.937542	6.785382
-602.597002	-15.108168	6.795379
-600.456905	-21.917351	6.805376
-599.675646	-17.675971	6.815373
-597.535687	-16.228323	6.825370
-595.327558	-13.188990	6.835366
-593.655271	-21.285337	6.845363
-591.457504	-21.966346	6.855360
-589.446695	-16.785082	6.865357
-587.883873	-14.284352	6.875354
-586.298067	-16.537640	6.885350
-584.379015	-22.474195	6.895347
-582.054419	-16.309728	6.905344
-580.182096	-12.105376	6.915341
-578.479477	-9.351584	6.925338
-576.530797	-19.445734	6.935334
-574.685926	-21.184242	6.945331
-572.907311	-15.851677	6.955328
-571.172171	-18.782291	6.965325
-569.032352	-22.967983	6.975322
-567.106615	-24.347677	6.985318
-565.033659	-22.414656	6.995315
-563.714679	-14.880527	7.005312
-561.156860	-23.732694	7.015309
-559.435822	-17.262699	7.025306
-558.291463	-21.628136	7.035302
-556.269411	-25.526054	7.045299
-554.534068	-14.758190	7.055296
-552.010533	-18.451672	7.065293
-550.252230	-18.426496	7.075290
-548.615100	-15.739313	7.085286
-546.513931	-14.322529	7.095283
-544.657154	-12.821919	7.105280
-542.645922	-15.744170	7.115277
-540.934719	-13.270066	7.125274
-538.802819	-17.025580	7.135270
-537.001007	-17.805801	7.145267
-535.524936	-14.859778	7.155264
-533.338603	-19.130107	7.165261
-531.673238	-17.406552	7.175258
-530.027530	-14.651275	7.185254
-527.987851	-10.530152	7.195251
-525.702025	-16.708649	7.205248
-524.049896	-18.477697	7.215245
-522.023150	-19.913039	7.225242
-520.409281	-23.456355	7.235238
-518.397213	-18.254719	7.245235
-516.488671	-20.525811	7.255232
-514.619125	-19.002876	7.265229
-512.659549	-16.987932	7.275226
-511.230081	-15.700917	7.285222
-509.111683	-16.339023	7.295219
-506.939461	-16.938542	7.305216
-505.335954	-20.233462	7.315213
-503.602666	-17.387284	7.325210
-501.770888	-19.826603	7.335206
-499.678293	-17.646353	7.345203
-497.757211	-17.170084	7.355200
-495.573508	-16.074123	7.365197
-493.891385	-18.387378	7.375194
-492.290637	-14.756482	7.385190
-490.484330	-15.837819	7.395187
-487.979352	-21.627065	7.405184
-486.660869	-18.819583	7.415181
-484.864043	-17.279020	7.425178
-482.876570	-18.626192	7.435174
-480.798079	-19.670437	7.445171
-479.132822	-20.196006	7.455168
-477.218958	-19.622453	7.465165
-475.184720	-8.207875	7.475162
-473.307405	-16.801766	7.485158
-471.387828	-17.749184	7.495155
-469.787507	-13.466893	7.505152
-467.685545	-17.202221	7.515149
-465.636112	-11.361581	7.525146
-464.137307	-15.363744	7.535142
-462.192023	-20.555033	7.545139
-460.280884	-16.522880	7.555136
-458.215759	-22.486820	7.565133
-456.587686	-18.797365	7.575130
-454.573067	-19.184859	7.585126
-452.640495	-18.065948	7.595123
-451.161033	-20.418324	7.605120
-449.109755	-19.948562	7.615117
-447.018823	-16.499362	7.625114
-445.213537	-20.099997	7.635110
-443.303796	-18.136148	7.645107
-441.312519	-18.109795	7.655104
-439.236995	-17.403502	7.665101
-437.750163	-20.187527	7.675098
-435.950788	-15.322442	7.685094
-434.204880	-18.358795	7.695091
-431.950480	-18.194199	7.705088
-430.264187	-21.068166	7.715085
-428.517977	-21.595747	7.725082
-426.594539	-20.902089	7.735078
-424.448849	-19.689305	7.745075
-422.449629	-26.241858	7.755072
-420.833022	-30.895767	7.765069
-419.037629	-25.803537	7.775066
-417.122877	-25.225367	7.785062
-415.227366	-21.379425	7.795059
-413.441724	-21.261662	7.805056
-411.379113	-16.471761	7.815053
-409.572358	-27.162386	7.825050
-407.878144	-15.460613	7.835046
-406.218462	-20.210833	7.845043
-403.793906	-19.058130	7.855040
-402.058876	-14.712368	7.865037
-399.757157	-19.034049	7.875034
-398.565645	-22.486296	7.885030
-396.592663	-16.823396	7.895027
-394.737544	-19.271420	7.905024
-392.785866	-21.422998	7.915021
-390.677421	-22.972682	7.925018
-388.943348	-21.453326	7.935014
-387.048448	-19.724825	7.945011
-385.017257	-14.526006	7.955008
-383.431910	-25.039527	7.965005
-381.434184	-27.636896	7.975002
-379.755187	-21.256436	7.984998
-377.714915	-25.202856	7.994995
-375.526205	-29.344680	8.004992
-373.750658	-22.898576	8.014989
-371.889436	-22.693377	8.024986
-370.079476	-27.044506	8.034982
-368.256355	-26.339937	8.044979
-366.825766	-22.981352	8.054976
-364.610103	-24.539536	8.064973
-362.510628	-30.212916	8.074970
-360.727728	-26.698583	8.084966
-359.001721	-28.177906	8.094963
-357.057498	-31.696422	8.104960
-355.337544	-27.468993	8.114957
-353.634492	-17.451534	8.124954
-351.384326	-16.449895	8.134950
-349.598120	-20.808406	8.144947
-347.543628	-16.623733	8.154944
-345.775902	-26.692691	8.164941
-343.606285	-22.090264	8.174938
-342.101257	-21.244567	8.184934
-340.551301	-11.943444	8.194931
-338.392522	-20.269794	8.204928
-336.190667	-17.150994	8.214925
-334.635715	-20.779786	8.224922
-332.644841	-21.409767	8.234918
-330.802384	-19.622448	8.244915
-328.917269	-23.213415	8.254912
-327.003022	-20.009313	8.264909
-325.080375	-24.216532	8.274906
-323.339396	-16.138954	8.284902
-321.562705	-23.402627	8.294899
-319.504875	-20.239749	8.304896
-317.367323	-23.052756	8.314893
-315.741802	-20.007006	8.324890
-314.212796	-17.338729	8.334886
-311.942668	-25.301201	8.344883
-310.054274	-18.016015	8.354880
-308.323129	-25.539431	8.364877
-306.568019	-20.199947	8.374874
-304.543745	-16.347978	8.384870
-302.151358	-18.845835	8.394867
-300.854467	-15.550054	8.404864
-298.797338	-18.948009	8.414861
-297.175332	-14.471365	8.424858
-295.104604	-21.757405	8.434854
-293.248202	-17.747797	8.444851
-291.312063	-19.246539	8.454848
-289.238633	-20.432106	8.464845
-287.611642	-19.367809	8.474842
-286.095170	-18.138721	8.484838
-284.002242	-10.824971	8.494835
-282.012444	-17.091699	8.504832
-279.909034	-23.341947	8.514829
-278.480753	-21.443254	8.524826
-276.304676	-18.920333	8.534822
-274.535623	-19.315029	8.544819
-272.615716	-20.716918	8.554816
-270.802959	-20.980388	8.564813
-269.022012	-19.454796	8.574810
-266.434835	-15.936091	8.584807
-265.123998	-22.949902	8.594803
-263.596078	-19.868025	8.604800
-261.192942	-20.006294	8.614797
-259.570611	-24.286077	8.624794
-257.677591	-19.123567	8.634791
-255.860503	-22.025835	8.644787
-253.784439	-14.057863	8.654784
-251.919881	-15.157001	8.664781
-249.527204	-16.334862	8.674778
-248.538854	-19.610742	8.684775
-246.568524	-22.180040	8.694771
-244.520535	-20.027583	8.704768
-242.473690	-22.350345	8.714765
-240.929740	-25.632593	8.724762
-238.779288	-18.951547	8.734759
-236.906295	-20.731500	8.744755
-235.121670	-17.835522	8.754752
-232.816635	-28.085525	8.764749
-230.655534	-28.897606	8.774746
-229.635959	-23.421660	8.784743
-228.039792	-25.243054	8.794739
-225.731618	-24.249324	8.804736
-223.769218	-22.573036	8.814733
-221.878822	-25.326616	8.824730
-219.708422	-19.995479	8.834727
-218.346359	-27.199072	8.844723
-216.641632	-22.280506	8.854720
-214.397128	-32.062063	8.864717
-212.521382	-21.270288	8.874714
-210.362381	-22.514759	8.884711
-208.788308	-21.022429	8.894707
-206.908738	-19.774173	8.904704
-205.198122	-17.838905	8.914701
-203.507640	-22.213750	8.924698
-201.410018	-26.720072	8.934695
-199.465496	-27.168151	8.944691
-197.417510	-26.076429	8.954688
-195.827931	-32.359452	8.964685
-193.835126	-24.327771	8.974682
-192.044104	-34.126397	8.984679
-190.039587	-29.035149	8.994675
-187.992217	-26.679024	9.004672
-186.267009	-24.457745	9.014669
-184.582297	-27.497740	9.024666
-182.561204	-30.727426	9.034663
-180.557080	-30.798802	9.044659
-178.884911	-27.085182	9.054656
-176.856413	-26.052553	9.064653
-175.280143	-28.221863	9.074650
-173.388605	-27.568073	9.084647
-171.352490	-28.044889	9.094643
-169.465614	-29.072730	9.104640
-167.466186	-26.764494	9.114637
-165.455900	-30.297030	9.124634
-163.782719	-25.488830	9.134631
-162.071235	-23.573851	9.144627
-159.882795	-27.600921	9.154624
-158.104082	-32.152523	9.164621
-156.263778	-30.653664	9.174618
-154.522536	-29.648829	9.184615
-152.348592	-28.071231	9.194611
-150.433328	-30.133468	9.204608
-148.929264	-29.409662	9.214605
-147.291045	-26.345473	9.224602
-144.931303	-24.437321	9.234599
-142.837334	-24.726439	9.244595
-141.287132	-19.614558	9.254592
-139.345387	-26.038190	9.264589
-137.341620	-29.129722	9.274586
-135.740011	-27.316826	9.284583
-133.694841	-23.046664	9.294579
-131.949766	-17.887179	9.304576
-129.842477	-24.175972	9.314573
-128.221455	-19.137490	9.324570
-126.370010	-22.494172	9.334567
-124.753880	-21.693932	9.344563
-122.521441	-18.264488	9.354560
-120.622828	-20.875976	9.364557
-118.822883	-23.325893	9.374554
-116.823687	-19.289709	9.384551
-115.067436	-15.577436	9.394547
-113.412310	-18.085908	9.404544
-111.232639	-22.311038	9.414541
-109.427494	-19.829156	9.424538
-107.068636	-22.042932	9.434535
-105.774628	-13.734070	9.444531
-103.963330	-14.557245	9.454528
-101.891025	-14.122940	9.464525
-99.952744	-21.354182	9.474522
-98.053751	-19.034618	9.484519
-96.088700	-18.515522	9.494515
-94.381913	-18.397151	9.504512
-92.599400	-20.948012	9.514509
-90.942653	-19.493924	9.524506
-88.728384	-18.162709	9.534503
-87.070872	-19.896168	9.544499
-84.945224	-15.978874	9.554496
-82.940235	-20.121475	9.564493
-80.997441	-17.037557	9.574490
-79.476275	-14.532258	9.584487
-77.565235	-13.772296	9.594483
-75.796220	-14.683061	9.604480
-73.486692	-17.118773	9.614477
-71.533769	-14.150804	9.624474
-70.034095	-12.780434	9.634471
-68.287632	-13.711832	9.644467
-66.264078	-13.466364	9.654464
-64.570914	-12.618053	9.664461
-62.520914	-14.700594	9.674458
-60.555807	-16.536981	9.684455
-58.814142	-16.785410	9.694451
-56.825289	-17.661539	9.704448
-55.096783	-19.237612	9.714445
-52.950736	-15.166899	9.724442
-51.231050	-18.713192	9.734439
-49.259021	-15.129976	9.744435
-47.439734	-14.969224	9.754432
-45.661244	-18.543778	9.764429
-43.839312	-15.280242	9.774426
-41.933205	-20.393516	9.784423
-39.847254	-21.544759	9.794419
-38.117532	-16.526853	9.804416
-36.128746	-11.168425	9.814413
-34.424066	-7.757122	9.824410
-32.558315	-12.499482	9.834407
-30.734292	-7.061420	9.844403
-28.684450	-8.936432	9.854400
-26.313165	-12.908247	9.864397
-24.809571	-14.315719	9.874394
-23.149445	-12.982725	9.884391
-21.669272	-9.168928	9.894387
-19.331326	-13.953911	9.904384
-17.437315	-14.443444	9.914381
-15.570362	-11.748425	9.924378
-13.476803	-18.009133	9.934375
-11.686908	-12.995208	9.944371
-10.096301	-15.990160	9.954368
-7.686665	-19.306553	9.964365
-5.827980	-17.236532	9.974362
-5.000287	-10.552243	9.984359
-3.836812	23.819896	9.994355
-2.512795	74.602907	10.004352
-0.991407	144.219662	10.014349
0.000000	205.227913	10.019354
0.719591	247.313226	10.024359
1.140202	287.353960	10.029363
1.975527	318.430264	10.034368
2.072814	345.738865	10.039373
2.685309	375.034618	10.044378
3.004435	393.139060	10.049383
3.043765	425.613194	10.054387
3.402928	421.657298	10.059392
3.411975	428.578003	10.064397
3.335225	437.033499	10.069402
3.648797	460.191024	10.074407
3.774010	469.696607	10.079411
4.210081	469.668035	10.084416
4.113355	481.480154	10.089421
4.211256	484.796429	10.094426
4.541851	489.052116	10.099431
4.240180	495.521275	10.104435
4.275636	488.537282	10.109440
4.421574	502.199325	10.114445
4.643268	507.598259	10.119450
4.662010	512.803052	10.124455
4.605297	525.656337	10.129459
4.643892	519.362560	10.134464
4.765300	526.784685	10.139469
4.551513	529.357461	10.144474
4.848121	527.126160	10.149479
4.663964	537.983079	10.154483
5.078879	532.532641	10.159488
4.807210	545.440561	10.164493
5.286204	543.810335	10.169498
5.550017	543.057373	10.174503
4.886502	541.642778	10.179507
5.026588	540.308680	10.184512
5.360099	547.515243	10.189517
5.158181	542.356479	10.194522
5.491715	546.326292	10.199527
5.319233	554.549588	10.204531
5.345530	537.254550	10.209536
5.157203	540.174663	10.214541
5.232390	555.961848	10.219546
5.554885	551.028551	10.224551
5.333969	564.403034	10.229555
5.433027	562.603088	10.234560
5.293421	561.698250	10.239565
5.149820	567.488644	10.244570
5.606312	562.633023	10.249575
5.258791	570.816473	10.254579
5.386046	556.406129	10.259584
5.326257	570.396392	10.264589
5.806604	585.780991	10.269594
6.103033	602.083300	10.274599
5.484469	609.283007	10.279603
6.081382	604.705263	10.284608
6.030089	611.427979	10.289613
5.696993	608.325713	10.294618
5.980700	610.906753	10.299623
5.929431	620.958201	10.304627
6.174587	611.153004	10.309632
5.758515	615.400568	10.314637
5.752449	622.473552	10.319642
6.245806	628.399092	10.324647
6.231013	638.924286	10.329651
6.542735	635.581194	10.334656
6.321697	645.614399	10.339661
6.048783	644.868199	10.344666
6.044230	647.886687	10.349671
6.222882	662.121144	10.354675
6.406944	649.899214	10.359680
6.187968	671.864710	10.364685
6.551916	681.492117	10.369690
6.841322	687.936587	10.374695
6.724590	693.058486	10.379699
7.177701	691.250319	10.384704
7.149358	703.884548	10.389709
6.849687	700.269305	10.394714
7.032864	693.393705	10.399719
7.105247	701.417991	10.404723
7.184191	699.341221	10.409728
6.952926	706.287859	10.414733
7.291235	692.776710	10.419738
7.171111	703.196852	10.424743
7.017395	707.170909	10.429747
7.134893	699.698290	10.434752
7.102341	701.091753	10.439757
7.153155	707.839240	10.444762
7.454371	706.641314	10.449767
7.754813	713.504289	10.454771
7.467801	704.643684	10.459776
7.483268	709.364376	10.464781
7.566574	713.653841	10.469786
7.658132	715.049710	10.474791
7.379805	713.531948	10.479795
7.291242	713.615436	10.484800
7.460895	720.663862	10.489805
7.455773	741.684121	10.494810
8.007036	745.735862	10.499815
7.805148	757.823979	10.504819
7.885913	742.577106	10.509824
7.817696	746.590591	10.514829
7.527787	753.971640	10.519834
7.880810	751.965894	10.524839
8.125121	756.101057	10.529843
8.241062	757.394855	10.534848
7.956292	755.546226	10.539853
8.193075	755.549456	10.544858
8.045131	750.295712	10.549863
8.218021	772.784282	10.554867
8.568277	781.379904	10.559872
8.775478	781.355444	10.564877
8.802552	773.616851	10.569882
9.008832	758.808697	10.574887
8.610047	765.525535	10.579891
8.578551	758.269879	10.584896
8.464213	758.000555	10.589901
8.430274	756.370230	10.594906
8.525388	757.665626	10.599911
8.523329	781.092874	10.604915
9.026337	777.853926	10.609920
8.741403	791.148396	10.614925
8.642893	792.044762	10.619930
8.985424	789.442002	10.624935
9.019706	796.409464	10.629939
8.941241	792.243120	10.634944
9.206227	787.638948	10.639949
8.872372	791.603650	10.644954
9.444684	791.160541	10.649959
9.158267	802.696747	10.654963
9.355839	791.794742	10.659968
9.084368	803.430226	10.664973
9.010274	793.762152	10.669978
8.942722	794.365451	10.674983
8.862944	801.639047	10.679987
9.859339	813.301886	10.684992
9.604942	815.566675	10.689997
9.843855	810.423026	10.695002
9.786081	797.331010	10.700007
9.644516	795.384797	10.705011
9.502724	792.823237	10.710016
9.587843	806.219268	10.715021
9.919651	826.594117	10.720026
10.294169	815.733992	10.725031
9.981899	819.987891	10.730035
9.482948	799.224902	10.735040
9.721038	816.793080	10.740045
10.211950	827.241562	10.745050
10.138112	824.232166	10.750055
9.833221	829.639790	10.755059
10.144678	825.267241	10.760064
10.185446	829.777187	10.765069
10.253692	829.495503	10.770074
10.602494	832.131340	10.775079
9.983083	828.896542	10.780083
10.240327	828.816134	10.785088
10.374801	834.390003	10.790093
10.505755	822.549277	10.795098
10.548355	834.215407	10.800103
10.417678	837.556738	10.805107
10.748018	836.930908	10.810112
10.433728	843.442636	10.815117
10.108381	842.519891	10.820122
10.499846	840.743988	10.825127
10.171540	840.620689	10.830131
10.602850	860.005899	10.835136
10.754828	865.327307	10.840141
10.928374	874.491300	10.845146
11.025512	875.925305	10.850151
11.115934	876.963359	10.855155
11.091394	867.498320	10.860160
11.282849	874.836365	10.865165
11.132298	880.417673	10.870170
11.786138	869.708170	10.875175
11.062310	853.278760	10.880179
11.318535	852.343140	10.885184
11.152872	856.633491	10.890189
11.251681	865.147537	10.895194
11.479699	866.903308	10.900199
11.338482	884.131601	10.905203
11.377386	871.923729	10.910208
11.383534	879.232365	10.915213
11.165678	873.060574	10.920218
11.755296	877.324456	10.925223
11.493227	881.757264	10.930227
11.593244	877.549637	10.935232
11.457575	875.317405	10.940237
11.531061	880.711880	10.945242
11.619522	876.072028	10.950247
11.599198	888.249904	10.955251
11.561428	886.976667	10.960256
11.767437	891.005934	10.965261
12.060130	905.777635	10.970266
12.504541	908.042620	10.975271
12.155667	899.512640	10.980275
12.122971	900.802725	10.985280
11.950500	896.825364	10.990285
12.454813	902.195715	10.995290
12.419434	896.658544	11.000295
12.029712	896.037752	11.005299
12.665609	889.933122	11.010304
12.465126	894.920632	11.015309
12.187123	892.899906	11.020314
11.959612	889.822505	11.025319
12.222765	908.985952	11.030323
12.224904	913.399520	11.035328
12.571067	912.992026	11.040333
12.166350	918.111271	11.045338
12.520337	911.776680	11.050343
12.176129	918.762908	11.055347
12.564056	930.042271	11.060352
13.077129	931.434176	11.065357
13.273824	935.643077	11.070362
13.212769	924.317168	11.075367
13.212537	916.304108	11.080371
13.103421	903.631724	11.085376
13.199751	909.977155	11.090381
13.075863	910.717222	11.095386
13.439215	899.486720	11.100391
13.243540	907.117339	11.105395
13.809773	896.045474	11.110400
13.812741	899.362324	11.115405
13.716262	904.065955	11.120410
13.979413	905.136369	11.125415
13.548507	894.347181	11.130419
13.585184	881.990868	11.135424
13.454238	882.851748	11.140429
13.360878	882.349484	11.145434
13.763227	876.907004	11.150439
13.293180	887.780420	11.155443
13.449557	890.925309	11.160448
13.295608	905.977273	11.165453
13.128538	916.560737	11.170458
13.518085	913.215690	11.175463
13.179263	916.682331	11.180467
13.571564	922.619785	11.185472
13.642268	927.746334	11.190477
13.709810	943.110488	11.195482
14.067178	937.905040	11.200487
14.069379	944.306887	11.205491
14.229152	934.138761	11.210496
14.576003	937.019686	11.215501
14.398260	944.231198	11.220506
14.356378	939.254466	11.225511
14.245965	942.963396	11.230515
14.217291	938.479793	11.235520
14.327234	948.707100	11.240525
14.146832	950.817512	11.245530
14.567563	944.277255	11.250535
14.400789	947.683614	11.255539
14.472157	941.391547	11.260544
14.633592	948.088593	11.265549
14.611508	944.992537	11.270554
14.756101	940.683698	11.275559
14.633866	958.140528	11.280563
14.941197	948.017751	11.285568
14.827355	950.675301	11.290573
14.696401	952.828550	11.295578
14.845772	942.883253	11.300583
14.700393	954.719861	11.305587
14.305795	950.105969	11.310592
14.457310	954.051438	11.315597
14.499462	965.276823	11.320602
14.952210	974.622742	11.325607
14.987372	985.866313	11.330611
15.152785	975.804167	11.335616
15.551572	979.450273	11.340621
15.337972	981.398223	11.345626
15.531916	975.041706	11.350631
15.447098	980.656779	11.355635
15.282048	984.813244	11.360640
15.512630	979.650047	11.365645
15.552909	981.859204	11.370650
15.569899	978.188416	11.375655
15.344409	983.094979	11.380659
15.369904	981.112599	11.385664
15.158783	980.428023	11.390669
15.286932	985.658426	11.395674
15.695745	979.720197	11.400679
15.611194	999.827582	11.405683
15.939805	1000.876516	11.410688
16.653585	1008.463357	11.415693
16.387464	999.801895	11.420698
16.844498	990.646581	11.425703
16.651786	986.735430	11.430707
16.566464	975.492591	11.435712
16.447812	973.581901	11.440717
15.896017	956.287622	11.445722
16.228506	950.660911	11.450727
15.915055	966.297252	11.455731
16.646003	973.022188	11.460736
16.314587	982.719271	11.465741
16.236903	989.217333	11.470746
16.829280	978.113691	11.475751
16.526766	971.412429	11.480755
16.360774	957.130547	11.485760
16.577957	975.956171	11.490765
16.141489	978.069438	11.495770
16.431695	983.646264	11.500775
16.473315	989.750450	11.505779
16.465670	985.440859	11.510784
16.454681	983.153287	11.515789
16.435221	989.056367	11.520794
16.634296	987.581460	11.525799
16.361247	994.543284	11.530803
16.601284	1010.138060	11.535808
16.904864	1013.713261	11.540813
16.848135	1017.295373	11.545818
17.068504	1020.241816	11.550823
16.458741	1027.021386	11.555827
16.556048	1018.753523	11.560832
16.800643	1021.674497	11.565837
16.762111	1035.650085	11.570842
17.155436	1037.486481	11.575847
16.869024	1044.509433	11.580851
17.372194	1038.980137	11.585856
17.282855	1040.071129	11.590861
17.395620	1042.662210	11.595866
17.449590	1038.225592	11.600871
16.942800	1043.882643	11.605875
17.797005	1053.203197	11.610880
17.947783	1055.707631	11.615885
17.832480	1045.837649	11.620890
17.902617	1034.364823	11.625895
17.751707	1042.883888	11.630899
17.826676	1037.706300	11.635904
17.848119	1031.933942	11.640909
17.579633	1039.828163	11.645914
17.923574	1043.926584	11.650919
17.799175	1068.021031	11.655923
17.824662	1067.014434	11.660928
18.575831	1073.228313	11.665933
18.422039	1074.419175	11.670938
18.458135	1062.624137	11.675943
18.496797	1051.425117	11.680947
18.248673	1044.965946	11.685952
18.331452	1038.208067	11.690957
18.207305	1042.218192	11.695962
18.331404	1037.570603	11.700967
18.359817	1051.031831	11.705971
18.230743	1050.813580	11.710976
18.219614	1059.310266	11.715981
18.303557	1065.045251	11.720986
18.557299	1068.850064	11.725991
18.464357	1078.441581	11.730995
18.415530	1075.336269	11.736000
18.479833	1076.228814	11.741005
17.994355	1073.138369	11.746010
18.440177	1078.575258	11.751015
18.662972	1097.071643	11.756019
19.078190	1096.659016	11.761024
19.121720	1093.462864	11.766029
19.072338	1095.203855	11.771034
19.376714	1089.570072	11.776039
19.352940	1090.795485	11.781043
19.227352	1094.586000	11.786048
19.568510	1087.206297	11.791053
19.393239	1085.057404	11.796058
19.582579	1067.581060	11.801063
19.004370	1068.348109	11.806067
19.183731	1059.584180	11.811072
19.136903	1066.905935	11.816077
19.381354	1081.425152	11.821082
19.724272	1090.281153	11.826087
19.273024	1096.195149	11.831091
19.353117	1092.385619	11.836096
19.697213	1093.049798	11.841101
19.709139	1090.963545	11.846106
19.696915	1093.270931	11.851111
19.576753	1101.654886	11.856115
19.383928	1098.549785	11.861120
19.856662	1095.574913	11.866125
19.785517	1094.246592	11.871130
19.820430	1084.082802	11.876135
19.603924	1098.116988	11.881139
19.612628	1099.150121	11.886144
19.438481	1108.913476	11.891149
19.743443	1123.539201	11.896154
20.087185	1128.425185	11.901159
20.206695	1124.645206	11.906163
19.939553	1126.013401	11.911168
20.186436	1117.145889	11.916173
20.151482	1127.621580	11.921178
20.608222	1126.456169	11.926183
20.335209	1128.869064	11.931187
20.380297	1124.274470	11.936192
20.393052	1126.379419	11.941197
20.506493	1127.469202	11.946202
20.860539	1119.308452	11.951207
20.746077	1128.025789	11.956211
20.410601	1120.314053	11.961216
20.609790	1121.398212	11.966221
20.525343	1129.009474	11.971226
21.118998	1128.486120	11.976231
20.752213	1133.611168	11.981235
20.823121	1128.021743	11.986240
21.185124	1140.484398	11.991245
21.088692	1139.824361	11.996250
21.254765	1131.974125	12.001255
20.796261	1128.531277	12.006259
21.010333	1127.889056	12.011264
21.262996	1140.062166	12.016269
20.800446	1149.797626	12.021274
21.333999	1143.584920	12.026279
21.234330	1149.911159	12.031283
21.265201	1149.557719	12.036288
21.490435	1145.460394	12.041293
21.185633	1133.402038	12.046298
21.466402	1121.572506	12.051303
21.257422	1125.161009	12.056307
21.632228	1121.270153	12.061312
21.189633	1125.279240	12.066317
21.132179	1121.627893	12.071322
21.171264	1121.162913	12.076327
21.225905	1123.399233	12.081331
21.296462	1126.031512	12.086336
21.184316	1127.873663	12.091341
21.033110	1131.390683	12.096346
21.198355	1125.275475	12.101351
20.852560	1125.828203	12.106355
21.346060	1121.992391	12.111360
21.319495	1125.364090	12.116365
21.258823	1126.106750	12.121370
21.258532	1120.906116	12.126375
21.132720	1123.431931	12.131379
21.466556	1125.550118	12.136384
21.593950	1124.884075	12.141389
21.193646	1131.294615	12.146394
21.448323	1115.426634	12.151399
21.436765	1126.655423	12.156403
21.425920	1129.596135	12.161408
21.535234	1134.537710	12.166413
21.179914	1126.295291	12.171418
21.573247	1099.300312	12.176423
21.171658	1097.886146	12.181427
21.031442	1090.197394	12.186432
21.178629	1094.782724	12.191437
20.977164	1095.635180	12.196442
21.155728	1091.284949	12.201447
21.240226	1107.555837	12.206451
21.258338	1090.169220	12.211456
21.138227	1090.624831	12.216461
21.087874	1100.884064	12.221466
21.028016	1099.913809	12.226471
21.124121	1111.412287	12.231475
21.347255	1124.433216	12.236480
21.255144	1114.342897	12.241485
21.072538	1107.125224	12.246490
21.366633	1098.011600	12.251495
21.217119	1098.964097	12.256499
21.133322	1099.184138	12.261504
21.211826	1105.633364	12.266509
21.284599	1107.309595	12.271514
21.285038	1103.724906	12.276519
20.929605	1108.629314	12.281523
21.174985	1099.799174	12.286528
21.231962	1103.302599	12.291533
21.331687	1107.233698	12.296538
21.348063	1095.042540	12.301543
21.222695	1103.141203	12.306547
20.854689	1110.116201	12.311552
20.908132	1107.119269	12.316557
21.097032	1119.628560	12.321562
21.325685	1135.982130	12.326567
21.376111	1128.907257	12.331571
21.272607	1121.340486	12.336576
21.274481	1119.106741	12.341581
20.954457	1119.378732	12.346586
21.245454	1114.798426	12.351591
21.273423	1122.046592	12.356595
21.242241	1111.907933	12.361600
21.061025	1113.958900	12.366605
20.956011	1122.936721	12.371610
20.979055	1116.820634	12.376615
21.111520	1134.260833	12.381619
21.473422	1143.514271	12.386624
21.253989	1121.932391	12.391629
20.892713	1126.718594	12.396634
21.522123	1132.735478	12.401639
21.285308	1130.600683	12.406643
21.196203	1127.008841	12.411648
20.991084	1112.893395	12.416653
21.255578	1125.561047	12.421658
21.138860	1114.467965	12.426663
20.940221	1123.854210	12.431667
21.237125	1135.474595	12.436672
21.437723	1138.108264	12.441677
20.967536	1137.948893	12.446682
21.440465	1124.752978	12.451687
21.207093	1119.644809	12.456691
21.318054	1121.610155	12.461696
21.426200	1111.501292	12.466701
20.959657	1121.518079	12.471706
21.570333	1110.908184	12.476711
21.428978	1119.521178	12.481715
21.384344	1106.377702	12.486720
21.376060	1110.724428	12.491725
21.144848	1116.279781	12.496730
21.081973	1110.268429	12.501735
21.372690	1118.449313	12.506739
21.182132	1115.589742	12.511744
21.170099	1122.253052	12.516749
21.233440	1116.113872	12.521754
21.514970	1118.509844	12.526759
21.619230	1118.133953	12.531763
21.557564	1127.591453	12.536768
21.915715	1106.807413	12.541773
21.298039	1098.318672	12.546778
21.266162	1092.436618	12.551783
21.362940	1092.343460	12.556787
21.157196	1086.222401	12.561792
21.447406	1073.704440	12.566797
21.278222	1091.805788	12.571802
21.207866	1085.916518	12.576807
20.836327	1094.718966	12.581811
20.817793	1092.490303	12.586816
20.902959	1091.087418	12.591821
20.758246	1093.737654	12.596826
20.972204	1087.021605	12.601831
21.209062	1104.079133	12.606835
21.319631	1114.326968	12.611840
21.204311	1105.921435	12.616845
21.042915	1099.726451	12.621850
21.387058	1103.529194	12.626855
21.202664	1098.539346	12.631859
21.234394	1089.195578	12.636864
21.496429	1089.090664	12.641869
21.334197	1092.493512	12.646874
21.378289	1086.364355	12.651879
21.537074	1086.672672	12.656883
21.421056	1095.343678	12.661888
21.506511	1087.416892	12.666893
21.560747	1095.393572	12.671898
21.819474	1093.734349	12.676903
21.071431	1080.610445	12.681907
21.020737	1061.590386	12.686912
21.379009	1072.818491	12.691917
21.289268	1073.554684	12.696922
21.077563	1057.242513	12.701927
20.960851	1065.363751	12.706931
20.746174	1085.113424	12.711936
21.268810	1085.668832	12.716941
21.155068	1099.381056	12.721946
21.651454	1086.527338	12.726951
21.267850	1096.148965	12.731955
21.116198	1100.021320	12.736960
21.175390	1091.838111	12.741965
20.975113	1097.618286	12.746970
21.487128	1096.487217	12.751975
21.242013	1087.544208	12.756979
21.166997	1071.575298	12.761984
21.412846	1062.675230	12.766989
20.766722	1068.137889	12.771994
20.675708	1078.490921	12.776999
20.986974	1089.655255	12.782003
21.053304	1099.971850	12.787008
21.004556	1100.591278	12.792013
21.110404	1104.215404	12.797018
21.072710	1103.784510	12.802023
21.067209	1104.715078	12.807027
20.952320	1101.902931	12.812032
21.342702	1097.159536	12.817037
20.929695	1100.071301	12.822042
21.488155	1105.619546	12.827047
21.195793	1110.594851	12.832051
21.084473	1101.735474	12.837056
21.010974	1097.565038	12.842061
21.221433	1107.844295	12.847066
21.331929	1099.621892	12.852071
21.418583	1106.056694	12.857075
20.770077	1116.889418	12.862080
20.911081	1102.648714	12.867085
21.075509	1108.023334	12.872090
21.079621	1106.083289	12.877095
21.322630	1109.175868	12.882099
20.707226	1112.304707	12.887104
20.914590	1106.768868	12.892109
21.099815	1122.442628	12.897114
21.514561	1127.240648	12.902119
21.257424	1122.255764	12.907123
21.347975	1114.617040	12.912128
21.534867	1111.587358	12.917133
21.434886	1113.098998	12.922138
21.317194	1112.291423	12.927143
21.384284	1120.656704	12.932147
21.296454	1119.457557	12.937152
21.328112	1117.270812	12.942157
21.306934	1118.406571	12.947162
21.235970	1115.200440	12.952167
21.427465	1110.000875	12.957171
21.322470	1119.271193	12.962176
21.289128	1109.842252	12.967181
20.828921	1112.343293	12.972186
21.394319	1103.535257	12.977191
21.318477	1111.244509	12.982195
21.209488	1111.667818	12.987200
21.205104	1098.251393	12.992205
20.875928	1110.629241	12.997210
21.219152	1111.818968	13.002215
21.190409	1110.319558	13.007219
21.634937	1117.409458	13.012224
21.441965	1107.155646	13.017229
21.287335	1101.441873	13.022234
21.276543	1078.991773	13.027239
21.491528	1075.366358	13.032243
21.403479	1075.140678	13.037248
21.416799	1068.219827	13.042253
21.091756	1083.945510	13.047258
21.431798	1075.540078	13.052263
21.307096	1075.742263	13.057267
21.349278	1079.876643	13.062272
21.311514	1071.541121	13.067277
21.258581	1084.267506	13.072282
21.455551	1077.821218	13.077287
21.537010	1075.306991	13.082291
21.175240	1081.963932	13.087296
21.624427	1077.828621	13.092301
21.146569	1068.145525	13.097306
21.146723	1057.785211	13.102311
21.533946	1057.828571	13.107315
21.231440	1055.587023	13.112320
21.137612	1059.471559	13.117325
21.533609	1064.161457	13.122330
21.651322	1060.062063	13.127335
21.457603	1055.424355	13.132339
21.432822	1069.228274	13.137344
21.548449	1065.084631	13.142349
21.030206	1067.573510	13.147354
21.144270	1063.235530	13.152359
21.422891	1064.271724	13.157363
21.067862	1062.315497	13.162368
21.303523	1059.080884	13.167373
20.674174	1065.878434	13.172378
20.881073	1058.963870	13.177383
20.954111	1062.802033	13.182387
20.852437	1063.515403	13.187392
21.094578	1067.922602	13.192397
21.401095	1072.186527	13.197402
21.361278	1067.283217	13.202407
21.174920	1067.992159	13.207411
21.105541	1073.118301	13.212416
21.264402	1066.423550	13.217421
21.049079	1069.850496	13.222426
20.871753	1062.324043	13.227431
20.996344	1063.019934	13.232435
21.052091	1070.788710	13.237440
21.238748	1070.357246	13.242445
21.132727	1071.569916	13.247450
21.202455	1060.239642	13.252455
21.403122	1072.540036	13.257459
21.139677	1074.551807	13.262464
21.445952	1066.366906	13.267469
21.198760	1068.740627	13.272474
21.305227	1071.107792	13.277479
21.762300	1071.205097	13.282483
21.396117	1070.128285	13.287488
21.515318	1064.414944	13.292493
21.247912	1075.310588	13.297498
21.207277	1062.995414	13.302503
21.089984	1075.359800	13.307507
21.184523	1073.533334	13.312512
21.256865	1065.450122	13.317517
21.249270	1073.558182	13.322522
21.109039	1069.896961	13.327527
21.196956	1074.579290	13.332531
20.801880	1074.511252	13.337536
20.907524	1075.401446	13.342541
21.017866	1077.183339	13.347546
20.959925	1079.555799	13.352551
20.940995	1074.722326	13.357555
20.829145	1077.880084	13.362560
21.171093	1076.195935	13.367565
21.019586	1076.804166	13.372570
20.983293	1076.013426	13.377575
21.243052	1074.871134	13.382579
21.546824	1082.334100	13.387584
21.481759	1078.198934	13.392589
21.172535	1079.248287	13.397594
21.558607	1079.272502	13.402599
21.449534	1080.144248	13.407603
21.027048	1072.267848	13.412608
21.365283	1073.806982	13.417613
21.179379	1080.717981	13.422618
21.057046	1076.690530	13.427623
21.372525	1076.986192	13.432627
21.196756	1086.001781	13.437632
21.186758	1080.450324	13.442637
20.881590	1083.525176	13.447642
21.200038	1079.162806	13.452647
20.949080	1081.316517	13.457651
20.867658	1088.029999	13.462656
21.366372	1086.545551	13.467661
20.988049	1083.840943	13.472666
20.981410	1082.171561	13.477671
21.109698	1083.033005	13.482675
20.650978	1088.087352	13.487680
20.960406	1083.454158	13.492685
20.795521	1105.134276	13.497690
21.320628	1101.145023	13.502695
21.201773	1111.551009	13.507699
20.941237	1111.878327	13.512704
21.097537	1108.422046	13.517709
21.030869	1111.043113	13.522714
21.252494	1115.297132	13.527719
21.229661	1110.932083	13.532723
21.307531	1115.457856	13.537728
21.131014	1114.712867	13.542733
21.393013	1117.225478	13.547738
21.729486	1107.499841	13.552743
21.452735	1113.972480	13.557747
21.285705	1104.781203	13.562752
21.377399	1091.565023	13.567757
21.077300	1093.045051	13.572762
20.912134	1095.447740	13.577767
20.908857	1094.130282	13.582771
21.119731	1105.542367	13.587776
21.108195	1105.206068	13.592781
20.957957	1112.541626	13.597786
21.140630	1112.538742	13.602791
21.384162	1115.960841	13.607795
21.015224	1122.424026	13.612800
21.153235	1120.407731	13.617805
21.227330	1126.648510	13.622810
21.083436	1116.522857	13.627815
21.469634	1123.566312	13.632819
21.260897	1124.222647	13.637824
21.213303	1114.923253	13.642829
20.958419	1129.432603	13.647834
21.323256	1122.545801	13.652839
21.483958	1124.594988	13.657843
21.318450	1114.538964	13.662848
21.487099	1107.591857	13.667853
21.288002	1108.060221	13.672858
20.945055	1099.171874	13.677863
21.119726	1097.997196	13.682867
21.316812	1097.463285	13.687872
21.489259	1087.004332	13.692877
21.455073	1103.043325	13.697882
21.326797	1100.171105	13.702887
21.468191	1093.510127	13.707891
21.291651	1098.246490	13.712896
21.501543	1093.206014	13.717901
21.558801	1097.245445	13.722906
21.379569	1091.963791	13.727911
21.373646	1093.534698	13.732915
21.151749	1090.103001	13.737920
21.138624	1087.526436	13.742925
21.015612	1096.382985	13.747930
21.242872	1097.546015	13.752935
21.232239	1101.126558	13.757939
21.183790	1101.131721	13.762944
21.646121	1087.975549	13.767949
20.938004	1076.672445	13.772954
20.907168	1071.617592	13.777959
21.242814	1086.531312	13.782963
21.141677	1104.532191	13.787968
21.311502	1088.273783	13.792973
21.241008	1102.618861	13.797978
21.339359	1089.889834	13.802983
20.983594	1077.835522	13.807987
21.006053	1085.101194	13.812992
21.447467	1095.466372	13.817997
21.384805	1086.729713	13.823002
21.311822	1071.845197	13.828007
21.423014	1056.321220	13.833011
21.304391	1063.812783	13.838016
21.703561	1060.491714	13.843021
21.432255	1058.553106	13.848026
21.338467	1055.649323	13.853031
21.297584	1061.490972	13.858035
20.978291	1065.302455	13.863040
20.996425	1063.901986	13.868045
20.849375	1066.087616	13.873050
20.939754	1068.480433	13.878055
20.823235	1064.615015	13.883059
20.429060	1075.518184	13.888064
21.024369	1079.376542	13.893069
20.810139	1096.686668	13.898074
20.867493	1105.065847	13.903079
21.074342	1096.625607	13.908083
21.217846	1103.748165	13.913088
21.215771	1101.090756	13.918093
21.201730	1108.552962	13.923098
21.453640	1095.595494	13.928103
21.109903	1098.157485	13.933107
21.446874	1105.778192	13.938112
21.604233	1097.674466	13.943117
21.569026	1108.693348	13.948122
21.444602	1091.813935	13.953127
21.495052	1076.532854	13.958131
21.333851	1074.047996	13.963136
21.387747	1066.360711	13.968141
21.633009	1064.758273	13.973146
21.387537	1063.885371	13.978151
21.491202	1066.012620	13.983155
21.317891	1073.064746	13.988160
21.757617	1059.717473	13.993165
21.254552	1049.621866	13.998170
20.636397	1048.268916	14.003175
21.130317	1052.605309	14.008179
20.984006	1066.165983	14.013184
20.958266	1066.364621	14.018189
21.061945	1070.429475	14.023207
21.630871	1068.173901	14.028224
21.363235	1069.719920	14.033242
21.415780	1074.755807	14.038259
21.498363	1064.958616	14.043277
21.233104	1063.382331	14.048295
20.970369	1064.691270	14.053312
21.020240	1068.827150	14.058330
21.217831	1068.844472	14.063347
21.289371	1070.346117	14.068365
21.183766	1065.903655	14.073383
21.179790	1069.017979	14.078400
21.385770	1070.225687	14.083418
21.036397	1086.163621	14.088435
21.436600	1069.837049	14.093453
21.221870	1071.431875	14.098471
21.172895	1075.617385	14.103488
21.447793	1067.156224	14.108506
21.226472	1063.717143	14.113523
21.373423	1079.745577	14.118541
21.313841	1095.369247	14.123559
21.420805	1111.425437	14.128576
21.702087	1109.108931	14.133594
21.465265	1113.018365	14.138611
21.919813	1109.264164	14.143629
21.697331	1107.425008	14.148647
21.362837	1112.163065	14.153664
21.436654	1106.220418	14.158682
21.651562	1113.873180	14.163699
21.733276	1110.346303	14.168717
21.393777	1120.910100	14.173735
21.463770	1115.170090	14.178752
21.544020	1104.594078	14.183770
21.319701	1115.764158	14.188787
21.383292	1110.296135	14.193805
21.506585	1117.270457	14.198823
21.584982	1129.954126	14.203840
21.882867	1135.236968	14.208858
21.598126	1139.370784	14.213875
22.045299	1133.208982	14.218893
22.009164	1139.669660	14.223911
21.972532	1134.899577	14.228928
21.879637	1145.393155	14.233946
21.723286	1146.733864	14.238963
21.596965	1138.846616	14.243981
21.790056	1140.730217	14.248999
21.604039	1136.368456	14.254016
21.729111	1140.167813	14.259034
22.036772	1139.268944	14.264051
21.895818	1141.408655	14.269069
22.123003	1148.197053	14.274087
21.710700	1152.107842	14.279104
22.133306	1163.197354	14.284122
22.184726	1176.968455	14.289139
22.527729	1172.694735	14.294157
22.472611	1168.770797	14.299175
22.557159	1156.157227	14.304192
22.404910	1150.163552	14.309210
22.239458	1149.954513	14.314227
22.200720	1140.067830	14.319245
22.004542	1140.874773	14.324263
21.966196	1140.300211	14.329280
22.274632	1139.664617	14.334298
22.363204	1160.740174	14.339315
22.281395	1146.925110	14.344333
22.187093	1151.400718	14.349351
22.198517	1172.565115	14.354368
22.342044	1167.577897	14.359386
22.146943	1173.623287	14.364403
22.279509	1173.579704	14.369421
22.596749	1175.744018	14.374439
22.551724	1170.270186	14.379456
22.851326	1169.758557	14.384474
22.591645	1173.148259	14.389491
22.726743	1173.103454	14.394509
22.745948	1168.417891	14.399527
22.400484	1168.842522	14.404544
22.471800	1161.417481	14.409562
22.584842	1166.667060	14.414579
22.730745	1161.755427	14.419597
22.826750	1167.414655	14.424615
22.564493	1179.021242	14.429632
22.755341	1174.718093	14.434650
22.384704	1186.599195	14.439667
22.547521	1168.522518	14.444685
22.776757	1168.371015	14.449703
23.033504	1171.116220	14.454720
22.844986	1173.258577	14.459738
23.010898	1169.826708	14.464755
23.050588	1167.019681	14.469773
23.083165	1172.431496	14.474791
22.675965	1162.055959	14.479808
22.827023	1150.451154	14.484826
22.621416	1167.940637	14.489843
22.828766	1166.276617	14.494861
23.313955	1169.789415	14.499879
22.800827	1170.192789	14.504896
22.961670	1172.523692	14.509914
22.959031	1166.581532	14.514931
22.684403	1170.247835	14.519949
22.968954	1162.663388	14.524967
22.712547	1164.927236	14.529984
23.167899	1162.036343	14.535002
22.801936	1166.036049	14.540019
23.359605	1161.351479	14.545037
23.038195	1162.878772	14.550055
23.185170	1161.615687	14.555072
23.262756	1159.231728	14.560090
22.933226	1158.201537	14.565107
23.334951	1160.665956	14.570125
23.416440	1155.405103	14.575143
22.915879	1164.568867	14.580160
23.532454	1151.005348	14.585178
23.463835	1164.661575	14.590195
22.914476	1148.695383	14.595213
23.019716	1155.542098	14.600231
23.196531	1166.430034	14.605248
23.521255	1155.339590	14.610266
23.181937	1166.902683	14.615283
23.572686	1162.031754	14.620301
23.573358	1166.890723	14.625319
23.227865	1162.403529	14.630336
23.507789	1164.387215	14.635354
23.474265	1161.938440	14.640371
23.647343	1160.592921	14.645389
23.391698	1153.710598	14.650407
23.385137	1165.534774	14.655424
23.390729	1161.501601	14.660442
23.452781	1171.468981	14.665459
23.300574	1181.549094	14.670477
23.868766	1178.021869	14.675495
23.602255	1188.562173	14.680512
24.177979	1174.741836	14.685530
24.118006	1175.456917	14.690547
24.080722	1162.407499	14.695565
24.171212	1147.982528	14.700583
24.115688	1153.940982	14.705600
24.182279	1143.768499	14.710618
24.258794	1149.079458	14.715635
23.996298	1134.999690	14.720653
24.388788	1123.180267	14.725671
23.878327	1123.213074	14.730688
23.775277	1116.333740	14.735706
23.924195	1115.004573	14.740723
23.807428	1110.693549	14.745741
24.011743	1116.186538	14.750759
23.647918	1117.103725	14.755776
23.634279	1113.927475	14.760794
23.759138	1134.509728	14.765811
23.735691	1144.116522	14.770829
24.325141	1150.085660	14.775847
23.945385	1150.851631	14.780864
24.204868	1146.259140	14.785882
24.304237	1152.734389	14.790899
24.275604	1149.905218	14.795917
24.417704	1148.999693	14.800935
24.102465	1151.399621	14.805952
24.262422	1145.647719	14.810970
23.993135	1151.126244	14.815987
23.879989	1149.797514	14.821005
24.392761	1159.617130	14.826023
23.637627	1159.505651	14.831040
23.741075	1149.894215	14.836058
23.993378	1151.704668	14.841075
23.944206	1149.796025	14.846093
24.009305	1145.240406	14.851111
24.022408	1168.016454	14.856128
24.352723	1175.460861	14.861146
24.837075	1188.396656	14.866163
24.556642	1183.438812	14.871181
24.357966	1163.419619	14.876199
23.951294	1159.749282	14.881216
24.473662	1173.085273	14.886234
24.869742	1179.475799	14.891251
25.178645	1174.946092	14.896269
24.852511	1159.496781	14.901287
23.942010	1160.222638	14.906304
24.557875	1148.860609	14.911322
24.414156	1160.458670	14.916339
24.561899	1179.924762	14.921357
25.102982	1176.412817	14.926375
24.425636	1173.322001	14.931392
24.391402	1174.824862	14.936410
24.339040	1184.140944	14.941427
24.883667	1192.194732	14.946445
24.492386	1190.449474	14.951463
24.545128	1196.946516	14.956480
24.761921	1178.581414	14.961498
24.652237	1179.516454	14.966515
24.512509	1188.104148	14.971533
24.818420	1185.549529	14.976551
24.536694	1189.421009	14.981568
24.513242	1189.607737	14.986586
25.286205	1195.557634	14.991603
24.827792	1193.902632	14.996621
24.753420	1192.306992	15.001639
24.990143	1205.901453	15.006656
24.948026	1220.627293	15.011674
25.074320	1222.098698	15.016691
24.895820	1223.920025	15.021709
25.310432	1219.010733	15.026727
25.264988	1223.117323	15.031744
25.008972	1218.552167	15.036762
25.006440	1222.833306	15.041779
24.984050	1227.961231	15.046797
25.026559	1217.527845	15.051815
25.534533	1222.477820	15.056832
25.626373	1213.838105	15.061850
25.686748	1210.368412	15.066867
25.239105	1197.506261	15.071885
25.140657	1182.535651	15.076903
25.196766	1186.966975	15.081920
25.078642	1196.536880	15.086938
25.246044	1207.467801	15.091955
25.273928	1211.203910	15.096973
25.670461	1210.837879	15.101991
25.055868	1219.241237	15.107008
25.271056	1207.143463	15.112026
25.313150	1212.037867	15.117043
25.166645	1223.543137	15.122061
25.684807	1206.507162	15.127079
25.615457	1215.996269	15.132096
25.555144	1220.421971	15.137114
25.764650	1211.981788	15.142131
25.362197	1221.248064	15.147149
25.412703	1212.118937	15.152167
25.393538	1219.391770	15.157184
25.154257	1209.122462	15.162202
25.660515	1212.360768	15.167219
25.374096	1215.829873	15.172237
25.647065	1229.474444	15.177255
25.930542	1246.054496	15.182272
25.687399	1238.599861	15.187290
26.308724	1228.081796	15.192307
25.695381	1222.282908	15.197325
25.874822	1201.873217	15.202343
25.861013	1219.086938	15.207360
26.124637	1199.914894	15.212378
26.011178	1209.763559	15.217395
25.780250	1209.847265	15.222413
25.887959	1203.847978	15.227431
25.924718	1201.965543	15.232448
25.753427	1202.449690	15.237466
26.113142	1213.610263	15.242483
26.044650	1228.510727	15.247501
26.278616	1227.590234	15.252519
26.236037	1218.247516	15.257536
26.191561	1215.136379	15.262554
26.108121	1204.269045	15.267571
25.814584	1220.919652	15.272589
26.176226	1220.371792	15.277607
26.190365	1231.670376	15.282624
26.354407	1237.468764	15.287642
26.535115	1230.319449	15.292659
26.340055	1218.240426	15.297677
26.700465	1207.258403	15.302695
26.319092	1207.110795	15.307712
26.418533	1209.963694	15.312730
26.801422	1203.431357	15.317747
26.386554	1210.892514	15.322765
26.275977	1210.142523	15.327783
26.333347	1212.345885	15.332800
26.033614	1208.343000	15.337818
26.153328	1207.322796	15.342835
26.056931	1214.650210	15.347853
26.091178	1220.729137	15.352871
26.171865	1242.729466	15.357888
26.449120	1243.171357	15.362906
26.463312	1231.700992	15.367923
26.447114	1232.719621	15.372941
26.499126	1226.103836	15.377959
26.493349	1232.106551	15.382976
26.590596	1241.160380	15.387994
26.619263	1234.921068	15.393011
26.514950	1240.019733	15.398029
26.705106	1245.879794	15.403047
26.797912	1268.213938	15.408064
26.927805	1264.235418	15.413082
27.013201	1248.742234	15.418099
26.625945	1241.688325	15.423117
26.818357	1235.980829	15.428135
27.053373	1229.157272	15.433152
27.121732	1242.354217	15.438170
27.162673	1233.816927	15.443187
27.146208	1237.957138	15.448205
27.081620	1236.075539	15.453223
26.960111	1238.946246	15.458240
26.818380	1241.618433	15.463258
27.122902	1232.546145	15.468275
27.084954	1232.004979	15.473293
27.271082	1225.272884	15.478311
27.123524	1232.298815	15.483328
26.936477	1238.757846	15.488346
27.040220	1232.696231	15.493363
26.598660	1235.538339	15.498381
26.979781	1248.622997	15.503399
26.983620	1257.791286	15.508416
27.278521	1271.286451	15.513434
27.469541	1267.688824	15.518451
27.062650	1273.286662	15.523469
27.342197	1271.217303	15.528487
27.367345	1271.587449	15.533504
27.026310	1276.154220	15.538522
27.389260	1272.349538	15.543539
27.084845	1262.656374	15.548557
27.312204	1273.187262	15.553575
27.355700	1275.318596	15.558592
27.331366	1271.887431	15.563610
27.481336	1273.603229	15.568627
27.459487	1275.353998	15.573645
27.247749	1283.750135	15.578663
27.135806	1293.858459	15.583680
27.496224	1303.158175	15.588698
27.318372	1300.318731	15.593715
27.420401	1302.126618	15.598733
27.691855	1296.341764	15.603751
27.696285	1303.816121	15.608768
27.601862	1301.280513	15.613786
28.100355	1296.958839	15.618803
28.017803	1305.038716	15.623821
27.923432	1303.062205	15.628839
27.924565	1305.466579	15.633856
27.688112	1303.371109	15.638874
28.171335	1299.497370	15.643891
27.980033	1301.854809	15.648909
27.861314	1298.420133	15.653927
28.033806	1298.447664	15.658944
27.814990	1305.581917	15.663962
28.156219	1294.744474	15.668979
27.684000	1299.933799	15.673997
27.674220	1300.496960	15.679015
27.465466	1301.334021	15.684032
27.874377	1307.149906	15.689050
28.241648	1319.172726	15.694067
28.270594	1328.969488	15.699085
28.565978	1315.530196	15.704103
28.512787	1305.008819	15.709120
28.217454	1299.925922	15.714138
28.316786	1297.034230	15.719155
28.065367	1300.197719	15.724173
28.031048	1290.482246	15.729191
28.222695	1292.487779	15.734208
28.392766	1291.550282	15.739226
28.312215	1302.990361	15.744243
28.467110	1316.737938	15.749261
28.529412	1305.875863	15.754279
28.614676	1292.821467	15.759296
28.716749	1302.393844	15.764314
28.786883	1286.377206	15.769331
28.664151	1288.222841	15.774349
28.353613	1287.643363	15.779367
28.774660	1293.289430	15.784384
28.272783	1294.835864	15.789402
28.372489	1285.944344	15.794419
28.285163	1297.900589	15.799437
28.402070	1306.569160	15.804455
28.829246	1322.424984	15.809472
28.439628	1331.567460	15.814490
28.733285	1333.208624	15.819507
28.606210	1328.052377	15.824525
28.812753	1331.298391	15.829543
28.966765	1326.090801	15.834560
28.462994	1334.661456	15.839578
28.487271	1334.116312	15.844595
28.359770	1335.997418	15.849613
28.727938	1331.803208	15.854631
29.185186	1328.459949	15.859648
28.677442	1330.425936	15.864666
29.173520	1345.588409	15.869683
29.509778	1343.405371	15.874701
29.290611	1343.558721	15.879719
29.518470	1330.646003	15.884736
28.870750	1337.767579	15.889754
29.001312	1332.139164	15.894771
28.918652	1330.952843	15.899789
28.917825	1335.687306	15.904807
29.122878	1336.875901	15.909824
28.975341	1348.981892	15.914842
29.040585	1360.827372	15.919859
29.596247	1364.808101	15.924877
29.270339	1359.708770	15.929895
29.480382	1360.209044	15.934912
29.391996	1361.786568	15.939930
29.625702	1357.433498	15.944947
29.651189	1360.007737	15.949965
29.410363	1342.324900	15.954983
29.633839	1331.738352	15.960000
29.130011	1324.733528	15.965018
29.239420	1329.423890	15.970035
29.769545	1344.773850	15.975053
29.545780	1345.981633	15.980071
29.916595	1343.851730	15.985088
29.780921	1343.253687	15.990106
29.617859	1330.943871	15.995123
29.907089	1326.512779	16.000141
29.614352	1330.915758	16.005159
29.989377	1324.164621	16.010176
29.762066	1320.198113	16.015194
29.643152	1317.377304	16.020211
29.806806	1317.855606	16.025229
29.488580	1321.890476	16.030247
29.510675	1322.254847	16.035264
29.821203	1350.267673	16.040282
30.050307	1346.656411	16.045299
30.222063	1352.116873	16.050317
29.927618	1348.880835	16.055335
30.199498	1348.527906	16.060352
29.871349	1360.724327	16.065370
30.017778	1359.179403	16.070387
29.817835	1351.136543	16.075405
29.558402	1355.892121	16.080423
29.964547	1354.560961	16.085440
29.817247	1361.672741	16.090458
29.652044	1362.512575	16.095475
29.735084	1359.539011	16.100493
29.811175	1363.898843	16.105511
30.111049	1369.866136	16.110528
30.081875	1389.746718	16.115546
29.890169	1388.398757	16.120563
30.105743	1386.910486	16.125581
30.122798	1390.437451	16.130599
30.325976	1396.066180	16.135616
30.278686	1392.102651	16.140634
30.755278	1391.415380	16.145651
30.800577	1387.781680	16.150669
30.450112	1389.686846	16.155687
30.891889	1383.267186	16.160704
30.417461	1381.723974	16.165722
30.154366	1392.027585	16.170739
30.455997	1390.700167	16.175757
30.322377	1389.226487	16.180775
30.736115	1383.584938	16.185792
30.286459	1390.528864	16.190810
30.751577	1400.356410	16.195827
30.994102	1417.477576	16.200845
30.571805	1421.957524	16.205863
31.134140	1418.232807	16.210880
30.501347	1408.479700	16.215898
30.625995	1421.720693	16.220915
31.027859	1420.967486	16.225933
30.795005	1427.314751	16.230951
30.833241	1419.682246	16.235968
30.973547	1420.384261	16.240986
31.142759	1419.794184	16.246003
31.017654	1417.881989	16.251021
30.999491	1427.630979	16.256039
31.022948	1421.937422	16.261056
31.388910	1426.526340	16.266074
31.234098	1424.083357	16.271091
31.594485	1418.265098	16.276109
31.428820	1408.777605	16.281127
31.599776	1384.933354	16.286144
31.039368	1392.697923	16.291162
30.962713	1381.294604	16.296179
31.063079	1387.703237	16.301197
30.912788	1401.901679	16.306215
31.002149	1406.928212	16.311232
31.126331	1413.526099	16.316250
31.006986	1415.829874	16.321267
31.187939	1422.537728	16.326285
30.811565	1424.068956	16.331303
31.078958	1425.563831	16.336320
31.053190	1438.525873	16.341338
31.528890	1449.100137	16.346355
31.570099	1448.467825	16.351373
31.505282	1452.843178	16.356391
31.720459	1445.887482	16.361408
31.410746	1442.610730	16.366426
31.427909	1448.370201	16.371443
31.573497	1443.147873	16.376461
31.651816	1448.127882	16.381479
31.464265	1441.600722	16.386496
31.811804	1439.110194	16.391514
31.655721	1446.742861	16.396531
31.891619	1447.860422	16.401549
31.669653	1451.771330	16.406567
31.726590	1437.854259	16.411584
32.089982	1444.741101	16.416602
31.984644	1452.986000	16.421619
31.951279	1448.536555	16.426637
31.945356	1445.173068	16.431655
32.074533	1451.393698	16.436672
31.852537	1470.528229	16.441690
32.110985	1469.918912	16.446707
32.260026	1464.418398	16.451725
32.196361	1475.677343	16.456743
32.591879	1468.085929	16.461760
32.672376	1453.626560	16.466778
32.113774	1455.135485	16.471795
32.376920	1444.212105	16.476813
32.192474	1444.483925	16.481831
32.349943	1435.162295	16.486848
32.210126	1435.085877	16.491866
32.398025	1442.778082	16.496883
32.581410	1428.704679	16.501901
32.222488	1439.742934	16.506919
32.371009	1445.737782	16.511936
32.560986	1457.469815	16.516954
32.703670	1465.118203	16.521971
32.905292	1452.816638	16.526989
32.454440	1437.755795	16.532007
32.731940	1427.455225	16.537024
32.961774	1440.320289	16.542042
32.475370	1437.740043	16.547059
32.591433	1435.067132	16.552077
32.384592	1441.786754	16.557095
32.914851	1448.959980	16.562112
32.744000	1455.636425	16.567130
33.059043	1464.675486	16.572147
32.887371	1456.456840	16.577165
32.787386	1447.803031	16.582183
33.061114	1440.022254	16.587200
32.665943	1430.399276	16.592218
32.946221	1458.395039	16.597235
33.108798	1456.995778	16.602253
33.173983	1467.974332	16.607271
33.197464	1464.320730	16.612288
33.190987	1445.337624	16.617306
33.192017	1447.417988	16.622323
33.600442	1441.207193	16.627341
33.608839	1439.156347	16.632359
32.966322	1438.052226	16.637376
32.946914	1429.552345	16.642394
32.610449	1438.042397	16.647411
33.046834	1450.987029	16.652429
33.063143	1460.277327	16.657447
32.538620	1461.282721	16.662464
32.603496	1463.940785	16.667482
32.887658	1467.036104	16.672499
33.088387	1482.613954	16.677517
33.427603	1490.821240	16.682535
33.712929	1496.309924	16.687552
33.689312	1499.941141	16.692570
33.378313	1502.600658	16.697587
33.499486	1484.678016	16.702605
33.854168	1492.303063	16.707623
33.959310	1490.840804	16.712640
33.947486	1483.473964	16.717658
34.075794	1488.616693	16.722675
34.319759	1477.037848	16.727693
34.136515	1463.340692	16.732711
33.936243	1456.428659	16.737728
34.125906	1452.660339	16.742746
34.008120	1448.605327	16.747763
33.903156	1451.807128	16.752781
34.243529	1447.558198	16.757799
33.573222	1447.009685	16.762816
33.758288	1445.412455	16.767834
33.556530	1453.696330	16.772851
33.922357	1456.259482	16.777869
34.045959	1458.945276	16.782887
33.897348	1456.691795	16.787904
34.057628	1465.645175	16.792922
34.082019	1480.108257	16.797939
34.223121	1477.851169	16.802957
34.253215	1491.664003	16.807975
33.843213	1491.564611	16.812992
34.241503	1483.134832	16.818010
34.004872	1499.831889	16.823027
34.339758	1488.876097	16.828045
34.303839	1499.959418	16.833063
34.149954	1490.197779	16.838080
34.246271	1482.769086	16.843098
34.429520	1486.963321	16.848115
34.304351	1489.299211	16.853133
34.262826	1491.779439	16.858151
33.896778	1490.278663	16.863168
34.242388	1501.905297	16.868186
34.499600	1523.786377	16.873203
34.407197	1519.142681	16.878221
34.485082	1521.904441	16.883239
34.728884	1530.388371	16.888256
34.796107	1521.981078	16.893274
34.726721	1525.608336	16.898291
34.962098	1521.449837	16.903309
34.584374	1518.941898	16.908327
34.475714	1525.985703	16.913344
34.644480	1515.850978	16.918362
34.562763	1526.974457	16.923379
34.843848	1533.138757	16.928397
35.297613	1543.249079	16.933415
35.344301	1550.615117	16.938432
35.482711	1539.814642	16.943450
35.201993	1529.508127	16.948467
35.013465	1520.139065	16.953485
35.326182	1519.605884	16.958503
35.097429	1519.410448	16.963520
35.186542	1515.229779	16.968538
35.187088	1521.718581	16.973555
35.277322	1511.363833	16.978573
35.397126	1522.841776	16.983591
35.235860	1534.647476	16.988608
35.618080	1533.792109	16.993626
35.354664	1539.935975	16.998643
35.245181	1544.711181	17.003661
35.718431	1546.071944	17.008679
35.308531	1552.843752	17.013696
35.592053	1545.890468	17.018714
35.494094	1551.422050	17.023731
35.562571	1543.351969	17.028749
35.823598	1546.992668	17.033767
35.936112	1544.906632	17.038784
36.226521	1543.819341	17.043802
35.586427	1527.362748	17.048819
35.870055	1519.930667	17.053837
35.955145	1506.184317	17.058855
35.832780	1513.059581	17.063872
36.032117	1501.188731	17.068890
35.847059	1511.810966	17.073907
35.478535	1508.942358	17.078925
36.426901	1515.587582	17.083943
36.027947	1517.437290	17.088960
36.406523	1512.838055	17.093978
35.814777	1506.221097	17.098995
35.901844	1512.489921	17.104013
36.297846	1503.858927	17.109031
36.057804	1509.580620	17.114048
36.021010	1505.531788	17.119066
35.997214	1518.220695	17.124083
36.419211	1529.008180	17.129101
36.337240	1539.717888	17.134119
36.356604	1546.137719	17.139136
36.563691	1535.310116	17.144154
36.295570	1531.161948	17.149171
36.171648	1531.128085	17.154189
36.287050	1533.616063	17.159207
35.989791	1547.890234	17.164224
36.011077	1535.579362	17.169242
36.189086	1546.117322	17.174259
36.366886	1544.667013	17.179277
35.972411	1539.730576	17.184295
35.989636	1559.139195	17.189312
36.343187	1559.379412	17.194330
36.285845	1571.442154	17.199347
36.536533	1575.088176	17.204365
36.096877	1568.777041	17.209383
35.994026	1582.359178	17.214400
36.882489	1591.082651	17.219418
37.125594	1593.757429	17.224435
37.800117	1577.803423	17.229453
37.866178	1565.246635	17.234471
37.786029	1551.779391	17.239488
37.765092	1537.766121	17.244506
37.744830	1537.591244	17.249523
37.645099	1539.413276	17.254541
37.800341	1517.334307	17.259559
37.391081	1511.783419	17.264576
37.230037	1513.662423	17.269594
37.479468	1518.417033	17.274611
37.455268	1509.346608	17.279629
37.408290	1507.943504	17.284647
37.366544	1519.546397	17.289664
37.388595	1513.426625	17.294682
37.388927	1525.353446	17.299699
37.168970	1522.373526	17.304717
37.459290	1514.713110	17.309735
37.612266	1513.165474	17.314752
37.729996	1513.726074	17.319770
37.656662	1514.063893	17.324787
37.510877	1519.827309	17.329805
37.755907	1520.864168	17.334823
37.457350	1528.951664	17.339840
37.908406	1521.284161	17.344858
37.501331	1513.700397	17.349875
37.537533	1519.538528	17.354893
37.451447	1520.182109	17.359911
37.317160	1510.442296	17.364928
37.420856	1517.085870	17.369946
37.574357	1518.737698	17.374963
37.556052	1528.860438	17.379981
37.951279	1534.831922	17.384999
37.533689	1542.540578	17.390016
37.867690	1538.208849	17.395034
37.641096	1537.773646	17.400051
37.627757	1544.846003	17.405069
37.943919	1534.306820	17.410087
37.655661	1548.681034	17.415104
37.844625	1569.309569	17.420122
37.909868	1578.284821	17.425139
38.063861	1576.635025	17.430157
38.392785	1567.693414	17.435175
38.025130	1570.691038	17.440192
38.013120	1568.879526	17.445210
38.406240	1570.854884	17.450227
38.152177	1585.831210	17.455245
38.283805	1580.354902	17.460263
38.346431	1593.777167	17.465280
38.511137	1597.148928	17.470298
38.514784	1605.171656	17.475315
38.690315	1607.003202	17.480333
39.004344	1602.414220	17.485351
38.609395	1603.460799	17.490368
38.990200	1607.157757	17.495386
38.911257	1603.049584	17.500403
38.573351	1610.348897	17.505421
38.839560	1601.191223	17.510439
39.010539	1607.683520	17.515456
38.934522	1597.545036	17.520474
39.002233	1597.349169	17.525491
38.759800	1608.446318	17.530509
39.045943	1593.375512	17.535527
39.124242	1601.266135	17.540544
39.193956	1591.325135	17.545562
39.316358	1597.112291	17.550579
38.983639	1607.099203	17.555597
39.009559	1593.839746	17.560615
39.212876	1591.764123	17.565632
39.302535	1599.542942	17.570650
39.525348	1600.048122	17.575667
39.187430	1598.416121	17.580685
39.446931	1593.830585	17.585703
39.311708	1598.449965	17.590720
39.369159	1599.579233	17.595738
39.331191	1596.826787	17.600755
38.860001	1604.086344	17.605773
39.183722	1599.513421	17.610791
39.236751	1601.908549	17.615808
39.411076	1614.197776	17.620826
39.579944	1624.849574	17.625843
39.607663	1639.225608	17.630861
39.748325	1636.841787	17.635879
39.752850	1638.101799	17.640896
40.062917	1634.724650	17.645914
40.337067	1632.874306	17.650931
40.199021	1625.631807	17.655949
40.086146	1601.024775	17.660967
39.726664	1599.944563	17.665984
39.856614	1601.805972	17.671002
40.109013	1591.682453	17.676019
39.794721	1602.031597	17.681037
40.163829	1606.996450	17.686055
40.266216	1616.744577	17.691072
40.377767	1605.416318	17.696090
40.250033	1590.218815	17.701107
40.136229	1598.980261	17.706125
40.021664	1586.202823	17.711143
39.965028	1599.590416	17.716160
40.387032	1614.697342	17.721178
39.999650	1616.258036	17.726195
40.118734	1625.476081	17.731213
40.362033	1617.955188	17.736231
40.534609	1622.829318	17.741248
40.618716	1624.639529	17.746266
40.828927	1616.595508	17.751283
40.474131	1621.835679	17.756301
40.679288	1613.619279	17.761319
40.643213	1616.788040	17.766336
40.584597	1615.758223	17.771354
40.536253	1618.979881	17.776371
40.384537	1622.062159	17.781389
40.769787	1613.117952	17.786407
40.747082	1628.308618	17.791424
40.592106	1649.114352	17.796442
41.110383	1651.468701	17.801459
40.870938	1652.121650	17.806477
40.919846	1655.007707	17.811495
41.366579	1646.872326	17.816512
41.084139	1649.866380	17.821530
41.446670	1648.021355	17.826547
40.876318	1649.551999	17.831565
41.314367	1641.469690	17.836583
41.201718	1639.849461	17.841600
41.195378	1652.458309	17.846618
41.552987	1640.492494	17.851635
41.295620	1644.648916	17.856653
41.308169	1639.982465	17.861671
41.656875	1640.228239	17.866688
41.400506	1638.397978	17.871706
41.479114	1642.307011	17.876723
41.249526	1637.452522	17.881741
41.571577	1640.850864	17.886759
41.138382	1636.714433	17.891776
41.210188	1633.671475	17.896794
41.398411	1636.891164	17.901811
41.286957	1644.967115	17.906829
41.506262	1659.420963	17.911847
41.787156	1671.965618	17.916864
41.780632	1668.552574	17.921882
42.041663	1672.360251	17.926899
42.096510	1668.327559	17.931917
42.381911	1670.368254	17.936935
42.337384	1669.403742	17.941952
41.826839	1657.176870	17.946970
42.098810	1650.962613	17.951987
42.152063	1666.122968	17.957005
41.844809	1664.204960	17.962023
42.106815	1669.572887	17.967040
42.088897	1676.072400	17.972058
42.167889	1673.168376	17.977075
41.903899	1674.254324	17.982093
42.197321	1666.219243	17.987111
41.965731	1668.550568	17.992128
41.886646	1674.244331	17.997146
42.120870	1681.915325	18.002163
42.375176	1691.598865	18.007181
42.252116	1702.717351	18.012199
42.125142	1709.856516	18.017216
42.204333	1703.296112	18.022234
42.414643	1699.419850	18.027251
42.201602	1703.530101	18.032269
42.550955	1719.577254	18.037287
42.767977	1727.424862	18.042304
42.686469	1731.994910	18.047322
43.138387	1726.877467	18.052339
42.722266	1731.063493	18.057357
43.349623	1736.587333	18.062375
43.299375	1723.835767	18.067392
43.092531	1720.152689	18.072410
43.037202	1699.119136	18.077427
42.686802	1703.444693	18.082445
43.021459	1726.898795	18.087463
43.204087	1730.929403	18.092480
42.994701	1732.217436	18.097498
43.102566	1727.434210	18.102515
43.131766	1729.820844	18.107533
43.005579	1724.900561	18.112551
42.996266	1730.667431	18.117568
42.815208	1727.705609	18.122586
43.164272	1739.718489	18.127603
43.396672	1757.027615	18.132621
43.553699	1759.737654	18.137639
43.756739	1756.172112	18.142656
43.201689	1761.512418	18.147674
43.486654	1761.181257	18.152691
43.510609	1759.529325	18.157709
43.342943	1750.657001	18.162727
43.634537	1753.706217	18.167744
43.729642	1759.629626	18.172762
43.792381	1746.674789	18.177779
43.570673	1751.609079	18.182797
43.445048	1763.256065	18.187815
44.111902	1768.546739	18.192832
44.297139	1774.218845	18.197850
44.495723	1765.900724	18.202867
44.059444	1759.234557	18.207885
44.177438	1750.613293	18.212903
44.425815	1740.041888	18.217920
44.216597	1757.371998	18.222938
44.230533	1743.732926	18.227955
44.306587	1747.997979	18.232973
44.003473	1751.468094	18.237991
44.521700	1754.873777	18.243008
44.460941	1767.954310	18.248026
44.175833	1771.628061	18.253043
44.574948	1777.004804	18.258061
44.527799	1779.534079	18.263079
44.818844	1776.864579	18.268096
44.502794	1784.431913	18.273114
44.614941	1775.239914	18.278131
44.894635	1780.181959	18.283149
44.998913	1778.600517	18.288167
44.947507	1785.180628	18.293184
44.613331	1786.173093	18.298202
44.721351	1780.838181	18.303219
44.666211	1788.122171	18.308237
44.618192	1786.534945	18.313255
44.895250	1780.609172	18.318272
44.699030	1783.996786	18.323290
45.012402	1776.584683	18.328307
45.158742	1782.865110	18.333325
44.630504	1773.302532	18.338343
44.877573	1773.661417	18.343360
44.772002	1806.699769	18.348378
45.118614	1802.937532	18.353395
45.032806	1811.144621	18.358413
44.815266	1809.760495	18.363431
45.488882	1807.212429	18.368448
45.248583	1814.742771	18.373466
45.327986	1805.785137	18.378483
45.697030	1803.833847	18.383501
45.346712	1801.154211	18.388519
45.865506	1815.533231	18.393536
45.637556	1824.007642	18.398554
45.752773	1822.790113	18.403571
45.859596	1813.037911	18.408589
45.633450	1818.141114	18.413607
46.208421	1819.476588	18.418624
46.309024	1820.426404	18.423642
46.396861	1803.803763	18.428659
46.123246	1805.400489	18.433677
45.780677	1799.608900	18.438695
45.977503	1794.755671	18.443712
45.758192	1796.053679	18.448730
45.854850	1802.501313	18.453747
45.783962	1804.402693	18.458765
45.849324	1826.308034	18.463783
46.717474	1827.853906	18.468800
46.314366	1835.640941	18.473818
46.856179	1830.488364	18.478835
46.203013	1809.486287	18.483853
46.231488	1830.230883	18.488871
46.447568	1824.811280	18.493888
46.264074	1829.370492	18.498906
46.031635	1832.500119	18.503923
46.270187	1833.303435	18.508941
46.168388	1831.858906	18.513959
46.515317	1827.941471	18.518976
46.568246	1835.444780	18.523994
46.373677	1831.694208	18.529011
46.520459	1843.058693	18.534029
46.810169	1867.667316	18.539047
47.149726	1858.301222	18.544064
47.062729	1860.638104	18.549082
46.962147	1868.055528	18.554099
47.139492	1870.829042	18.559117
46.925583	1861.541694	18.564135
47.408735	1853.863409	18.569152
47.074869	1863.487248	18.574170
47.083323	1853.679829	18.579187
47.337719	1852.371498	18.584205
46.980590	1860.966120	18.589223
47.562980	1860.337475	18.594240
47.383944	1852.067120	18.599258
47.588825	1858.663960	18.604275
47.658765	1850.142625	18.609293
47.843979	1865.443955	18.614311
48.115187	1859.919994	18.619328
47.548982	1865.040172	18.624346
47.719694	1863.001209	18.629363
47.808173	1852.598500	18.634381
47.541287	1859.176999	18.639399
47.966047	1857.992628	18.644416
47.539562	1861.083474	18.649434
47.377909	1849.806998	18.654451
47.248957	1847.473702	18.659469
47.548563	1855.332810	18.664487
47.781811	1853.628054	18.669504
47.495803	1873.837180	18.674522
47.561448	1877.577213	18.679539
48.045549	1880.288291	18.684557
47.810556	1892.557746	18.689575
47.906652	1888.832139	18.694592
47.761605	1890.269804	18.699610
48.020095	1911.206991	18.704627
48.361236	1917.023308	18.709645
48.115603	1924.957819	18.714663
48.404208	1912.093272	18.719680
48.478317	1915.792881	18.724698
48.434897	1914.267460	18.729715
48.423077	1914.243907	18.734733
48.385316	1918.367080	18.739751
48.428278	1910.450024	18.744768
48.375552	1919.029500	18.749786
47.986209	1918.419800	18.754803
48.615085	1930.142696	18.759821
48.632566	1945.331898	18.764839
48.590827	1941.098343	18.769856
48.601352	1949.089356	18.774874
48.680324	1950.375217	18.779891
48.872702	1948.750696	18.784909
48.840599	1945.100213	18.789927
49.117347	1942.849728	18.794944
48.965419	1955.670814	18.799962
49.120618	1970.267454	18.804979
49.627282	1961.810965	18.809997
49.387078	1958.162688	18.815015
49.416373	1957.368597	18.820032
49.413599	1962.657202	18.825050
49.517185	1966.760879	18.830067
49.714139	1964.438234	18.835085
49.666500	1965.149267	18.840103
49.487837	1955.191951	18.845120
49.499927	1945.628766	18.850138
49.852920	1961.299115	18.855155
49.693639	1961.767443	18.860173
49.449318	1967.072261	18.865191
49.597456	1955.291748	18.870208
50.048600	1969.432869	18.875226
49.718874	1962.069513	18.880243
49.896550	1960.988530	18.885261
49.867370	1966.012335	18.890279
50.195200	1959.082774	18.895296
50.444665	1956.303428	18.900314
49.940218	1957.971638	18.905331
50.640516	1956.737657	18.910349
50.337568	1963.293639	18.915367
50.307384	1952.899789	18.920384
50.453693	1953.000326	18.925402
50.301403	1969.084523	18.930419
50.388645	1953.686794	18.935437
50.375294	1963.333311	18.940455
50.131246	1964.229220	18.945472
49.786898	1959.681351	18.950490
50.341243	1969.597125	18.955507
50.530824	1977.486971	18.960525
50.343041	1991.575429	18.965543
50.225695	1992.268883	18.970560
50.386126	1996.061994	18.975578
50.441420	1992.953284	18.980595
50.553411	1997.428414	18.985613
50.988507	2021.186255	18.990631
51.051200	2020.450223	18.995648
51.119315	2020.129461	19.000666
51.262647	2020.108051	19.005683
51.649838	2005.862162	19.010701
51.167772	2006.695717	19.015719
51.452594	1980.393301	19.020736
51.836575	1975.006286	19.025754
50.976390	1979.341749	19.030771
51.185045	1979.268583	19.035789
51.068821	1983.534772	19.040807
51.140842	1974.579488	19.045824
51.122801	1991.332517	19.050842
51.072618	2005.966767	19.055859
51.619016	1995.168086	19.060877
51.583529	2005.592546	19.065895
51.445987	2006.840326	19.070912
51.795449	2007.411221	19.075930
51.494745	2011.523981	19.080947
51.180830	1996.020556	19.085965
51.499014	2022.086552	19.090983
51.742164	2031.915543	19.096000
51.737087	2036.057951	19.101018
51.749404	2044.849211	19.106035
52.091714	2033.082992	19.111053
51.977943	2041.783254	19.116071
52.160473	2045.817504	19.121088
52.057561	2035.186427	19.126106
51.804659	2045.658033	19.131123
52.061264	2048.684169	19.136141
52.197848	2063.842041	19.141159
52.457503	2063.847938	19.146176
52.508424	2063.369470	19.151194
52.267457	2069.180119	19.156211
53.022840	2050.501153	19.161229
52.459882	2054.832141	19.166247
52.891881	2055.801937	19.171264
53.092185	2048.728823	19.176282
53.160721	2051.446605	19.181299
53.271786	2049.496990	19.186317
53.082238	2043.400295	19.191335
53.276643	2030.562827	19.196352
53.547016	2018.486073	19.201370
53.170534	2020.105575	19.206387
53.053237	2021.362485	19.211405
53.180382	2018.860435	19.216423
52.764391	2022.492107	19.221440
53.038544	2015.713476	19.226458
53.044403	2025.500458	19.231475
53.299885	2042.377143	19.236493
53.284756	2055.357166	19.241511
53.097921	2056.178694	19.246528
53.373956	2054.220483	19.251546
53.207608	2068.107275	19.256563
53.185602	2049.957318	19.261581
53.089508	2054.405534	19.266599
53.393223	2053.497056	19.271616
53.625251	2062.762540	19.276634
53.429671	2082.904455	19.281651
53.193315	2084.923228	19.286669
53.565015	2086.484943	19.291687
53.766057	2087.564034	19.296704
54.016241	2087.858211	19.301722
53.604046	2097.561772	19.306739
53.687485	2089.366780	19.311757
53.393131	2103.828780	19.316775
53.780038	2121.184663	19.321792
53.842936	2119.021613	19.326810
53.676684	2122.853833	19.331827
54.093152	2120.991633	19.336845
54.176203	2134.959759	19.341863
54.205719	2151.093298	19.346880
54.739832	2152.850043	19.351898
54.441266	2150.199274	19.356915
55.342541	2152.284465	19.361933
55.215416	2137.104832	19.366951
54.884312	2118.228936	19.371968
55.356948	2104.942859	19.376986
55.024549	2111.999298	19.382003
55.061391	2109.682426	19.387021
54.977705	2101.722410	19.392039
55.071275	2103.108158	19.397056
55.198152	2103.572316	19.402074
54.909144	2101.779883	19.407091
54.986510	2098.791402	19.412109
55.134613	2110.084190	19.417127
55.055724	2110.357610	19.422144
55.287558	2091.953029	19.427162
55.484840	2102.886150	19.432179
55.214322	2106.640165	19.437197
55.442433	2098.510928	19.442215
55.561186	2107.287912	19.447232
55.501974	2105.554520	19.452250
55.102675	2111.215927	19.457267
55.144567	2111.154420	19.462285
55.577456	2110.786473	19.467303
55.554261	2134.708899	19.472320
55.662893	2133.572015	19.477338
55.577627	2142.068203	19.482355
55.725433	2145.341785	19.487373
55.882193	2137.925652	19.492391
55.920242	2140.332094	19.497408
56.006528	2140.288964	19.502426
55.928963	2146.707153	19.507443
55.752978	2141.631866	19.512461
56.069313	2139.987649	19.517479
55.796712	2152.488984	19.522496
55.906651	2158.960082	19.527514
56.018326	2168.873915	19.532531
56.367727	2171.948348	19.537549
56.705065	2173.643542	19.542567
56.420658	2169.831902	19.547584
56.827871	2173.691030	19.552602
56.277308	2173.126284	19.557619
56.785331	2169.196109	19.562637
56.746893	2173.544303	19.567655
56.513143	2174.643605	19.572672
56.274162	2171.524281	19.577690
56.729123	2176.871508	19.582707
56.545025	2179.134126	19.587725
56.838577	2184.524780	19.592743
56.969798	2197.745223	19.597760
57.308076	2190.986236	19.602778
57.123881	2194.832574	19.607795
57.241579	2201.694545	19.612813
57.288440	2196.024257	19.617831
57.147734	2204.456745	19.622848
57.504263	2189.063412	19.627866
57.366840	2188.845219	19.632883
57.646202	2184.254139	19.637901
57.664102	2185.545765	19.642919
57.871105	2192.462510	19.647936
58.087482	2183.578435	19.652954
57.903664	2189.728989	19.657971
57.725760	2168.220077	19.662989
58.013088	2162.906271	19.668007
57.725090	2166.449880	19.673024
57.762903	2159.625080	19.678042
58.086678	2179.796992	19.683059
57.726885	2195.430310	19.688077
57.856531	2188.665355	19.693095
58.121840	2195.299623	19.698112
58.037181	2185.293755	19.703130
57.791504	2193.115794	19.708147
57.892693	2188.714339	19.713165
58.013615	2182.861254	19.718183
58.217339	2193.628742	19.723200
58.371998	2205.859199	19.728218
58.132719	2219.169958	19.733235
58.250869	2217.516397	19.738253
58.497982	2212.406349	19.743271
58.272440	2220.243850	19.748288
58.368907	2215.326583	19.753306
58.239551	2223.820137	19.758323
58.437472	2229.316192	19.763341
58.888409	2240.451627	19.768359
58.533110	2248.793351	19.773376
58.925385	2244.929466	19.778394
58.657498	2249.802133	19.783411
58.834580	2246.279125	19.788429
58.529864	2241.588137	19.793447
58.588491	2264.117781	19.798464
59.188403	2267.844667	19.803482
59.267061	2265.459176	19.808499
59.275280	2275.346712	19.813517
59.010519	2267.491684	19.818535
59.141871	2268.849706	19.823552
59.370441	2262.909622	19.828570
59.251272	2277.544139	19.833587
59.608374	2286.380374	19.838605
59.760382	2299.275242	19.843623
59.788140	2304.969028	19.848640
60.207211	2292.472415	19.853658
60.099623	2290.197603	19.858675
60.222873	2290.248939	19.863693
60.726677	2273.230812	19.868711
60.013868	2269.637500	19.873728
60.400821	2264.891709	19.878746
60.569675	2252.101754	19.883763
60.389085	2256.075068	19.888781
60.140413	2253.086541	19.893799
60.122902	2258.168292	19.898816
59.976265	2257.203530	19.903834
60.223038	2252.772372	19.908851
59.911431	2276.097906	19.913869
60.283889	2284.844093	19.918887
60.103162	2287.906273	19.923904
60.039678	2285.611300	19.928922
60.267692	2297.295311	19.933939
60.623304	2307.913983	19.938957
60.795340	2314.597369	19.943975
61.299753	2328.142978	19.948992
61.378022	2317.078220	19.954010
61.035884	2323.212655	19.959027
61.132491	2322.080182	19.964045
61.261877	2316.670549	19.969063
61.235315	2320.124480	19.974080
61.314752	2314.801377	19.979098
61.074590	2319.214121	19.984115
61.097980	2316.983003	19.989133
61.154524	2314.382363	19.994151
60.981367	2324.510508	19.999168
61.026804	2319.400352	20.004186
61.577907	2320.699802	20.009203
61.474713	2337.657200	20.014221
61.630142	2338.497633	20.019239
61.752052	2344.737586	20.024256
61.669405	2350.380227	20.029274
61.825451	2347.089974	20.034291
61.798761	2346.421229	20.039309
62.009768	2344.721809	20.044327
61.948244	2349.845786	20.049344
61.984523	2338.314121	20.054362
61.894306	2338.005142	20.059379
61.930836	2344.314072	20.064397
62.118431	2354.914330	20.069415
62.171940	2360.747052	20.074432
62.559151	2362.490419	20.079450
62.756952	2363.701603	20.084467
62.674761	2368.173905	20.089485
62.836466	2365.580429	20.094503
62.596423	2367.891254	20.099520
63.012830	2361.040047	20.104538
62.573462	2358.981976	20.109555
62.429846	2360.947869	20.114573
62.782412	2352.694786	20.119591
62.687846	2363.290662	20.124608
62.672517	2359.152482	20.129626
63.073280	2356.347128	20.134643
62.901487	2358.971499	20.139661
62.893975	2359.451618	20.144679
62.848513	2375.878604	20.149696
62.927701	2388.993150	20.154714
62.935690	2389.639932	20.159731
63.231784	2396.470615	20.164749
62.999623	2401.861698	20.169767
63.117648	2402.480951	20.174784
63.251500	2416.039765	20.179802
63.338328	2423.332392	20.184819
63.470656	2427.054430	20.189837
63.510103	2424.147991	20.194855
63.745192	2427.357841	20.199872
63.672898	2430.418784	20.204890
64.179804	2419.904191	20.209907
63.826898	2424.923793	20.214925
63.925050	2412.663237	20.219943
64.096031	2436.292160	20.224960
64.130238	2440.527168	20.229978
64.455857	2445.457221	20.234995
64.432368	2450.006899	20.240013
64.807830	2445.266963	20.245031
64.497292	2453.376674	20.250048
64.921453	2443.893743	20.255066
64.756882	2429.659772	20.260083
64.505387	2424.227200	20.265101
64.933797	2431.640037	20.270119
64.634705	2442.384436	20.275136
64.468932	2443.398861	20.280154
64.884508	2439.411230	20.285171
65.007744	2435.813934	20.290189
65.008747	2429.624566	20.295207
64.798852	2441.392425	20.300224
65.045692	2444.380543	20.305242
65.480404	2445.124273	20.310259
65.034381	2449.143143	20.315277
64.986522	2440.752332	20.320295
65.128286	2438.969483	20.325312
65.290559	2446.705954	20.330330
65.265885	2460.563685	20.335347
65.686408	2474.655388	20.340365
65.958819	2474.223594	20.345383
65.515214	2465.466688	20.350400
65.804616	2465.980959	20.355418
65.917227	2465.057579	20.360435
66.061519	2465.837714	20.365453
65.871242	2467.057950	20.370471
66.067344	2467.332269	20.375488
66.517088	2466.241621	20.380506
66.438696	2462.397738	20.385523
66.347266	2475.751093	20.390541
66.508667	2457.321934	20.395559
66.611859	2446.216586	20.400576
66.097488	2441.591407	20.405594
66.277437	2427.344048	20.410611
66.255358	2446.537634	20.415629
66.427136	2456.816999	20.420647
66.549834	2461.708607	20.425664
66.589919	2461.672610	20.430682
66.488463	2463.684839	20.435699
66.210628	2468.589992	20.440717
66.350861	2467.689440	20.445735
66.671914	2472.352523	20.450752
66.488875	2500.802092	20.455770
67.061718	2497.797891	20.460787
66.741604	2498.355235	20.465805
66.790780	2498.929594	20.470823
67.031443	2506.806225	20.475840
67.025885	2506.403186	20.480858
67.236613	2511.849106	20.485875
67.073381	2529.946331	20.490893
67.383521	2526.214591	20.495911
67.707017	2527.179002	20.500928
67.513459	2524.417235	20.505946
67.618039	2510.890718	20.510963
67.655195	2513.854946	20.515981
67.538826	2519.922398	20.520999
67.819880	2518.546441	20.526016
67.543184	2519.802761	20.531034
68.104710	2537.627682	20.536051
68.066186	2541.941340	20.541069
68.103775	2542.810651	20.546087
68.272985	2545.317525	20.551104
68.344873	2553.034893	20.556122
68.903543	2540.667720	20.561139
68.469532	2548.048913	20.566157
68.349197	2542.064587	20.571175
68.578516	2543.959477	20.576192
68.602467	2546.154189	20.581210
68.649376	2539.774986	20.586227
68.517441	2550.406533	20.591245
68.272391	2545.109845	20.596263
68.382224	2541.204533	20.601280
68.541640	2567.180921	20.606298
68.705389	2560.539904	20.611315
69.320503	2574.852711	20.616333
69.483684	2576.106862	20.621351
68.812264	2572.238617	20.626368
69.157365	2564.765579	20.631386
69.084612	2566.600430	20.636403
69.248820	2570.613151	20.641421
68.888241	2572.858829	20.646439
69.046847	2582.322281	20.651456
68.977383	2597.714062	20.656474
69.315536	2595.973917	20.661491
69.312012	2600.001226	20.666509
69.155427	2609.143076	20.671527
69.432569	2618.013685	20.676544
69.676181	2630.219773	20.681562
70.263664	2626.305791	20.686579
70.036749	2629.169619	20.691597
70.006302	2632.751867	20.696615
70.243491	2625.442997	20.701632
70.292463	2634.958354	20.706650
70.492206	2636.277120	20.711667
70.519866	2633.811324	20.716685
70.164818	2634.225816	20.721703
70.009046	2632.864888	20.726720
70.006281	2640.855775	20.731738
70.661434	2650.609008	20.736755
70.619440	2662.098595	20.741773
70.671710	2664.379823	20.746791
70.591483	2663.472954	20.751808
70.451700	2661.060275	20.756826
71.036438	2651.880458	20.761843
71.130466	2650.189249	20.766861
70.975390	2650.489127	20.771879
71.305143	2650.615317	20.776896
71.442850	2648.433068	20.781914
71.409511	2647.127540	20.786931
71.582155	2643.316965	20.791949
71.807567	2641.227574	20.796967
72.127733	2641.976778	20.801984
71.703986	2652.494615	20.807002
71.798617	2644.136757	20.812019
71.791426	2646.687278	20.817037
71.704804	2645.559419	20.822055
71.955196	2636.948048	20.827072
71.425473	2646.128690	20.832090
72.004263	2660.351724	20.837107
72.003247	2669.688237	20.842125
71.960937	2674.782249	20.847143
72.651087	2672.599001	20.852160
72.068151	2680.410585	20.857178
72.429935	2669.088274	20.862195
72.391389	2675.192846	20.867213
72.284017	2671.619282	20.872231
72.170253	2670.858345	20.877248
72.350365	2680.346521	20.882266
72.462924	2679.348321	20.887283
72.133305	2702.762628	20.892301
72.443145	2711.646586	20.897319
72.989693	2717.346084	20.902336
72.700887	2707.050414	20.907354
72.962069	2697.755933	20.912371
72.881871	2699.520409	20.917389
73.074878	2717.123624	20.922407
73.437851	2718.548295	20.927424
73.291938	2725.739994	20.932442
73.600805	2726.191872	20.937459
73.779220	2729.463480	20.942477
73.689295	2706.485723	20.947495
73.772716	2689.061968	20.952512
73.711298	2696.574662	20.957530
73.848439	2687.581819	20.962547
73.936403	2678.138275	20.967565
73.857340	2684.096226	20.972583
73.855792	2691.842792	20.977600
73.754688	2720.807154	20.982618
74.032709	2713.172287	20.987635
73.977025	2716.313917	20.992653
73.830900	2717.592756	20.997671
74.330098	2715.925006	21.002688
73.885561	2718.934842	21.007706
73.578820	2725.103528	21.012723
74.365723	2746.235544	21.017741
74.235742	2749.905762	21.022759
74.376879	2750.361983	21.027776
74.395552	2754.640692	21.032794
74.453708	2748.484715	21.037811
74.833514	2763.568882	21.042829
74.626095	2773.963869	21.047847
74.624300	2775.369965	21.052864
74.755449	2775.137219	21.057882
74.939005	2772.220185	21.062899
74.944882	2767.436410	21.067917
74.929428	2786.982098	21.072935
75.499202	2789.949570	21.077952
75.393679	2803.870292	21.082970
75.409674	2798.780778	21.087987
75.598528	2799.984080	21.093005
75.554607	2803.204041	21.098023
75.314988	2799.091598	21.103040
75.469430	2798.729638	21.108058
75.242031	2805.032024	21.113075
75.664790	2819.930895	21.118093
76.122209	2834.261526	21.123111
76.257558	2832.942026	21.128128
75.986876	2830.659657	21.133146
76.281306	2829.496382	21.138163
76.432824	2832.768685	21.143181
75.942576	2837.900956	21.148199
76.653130	2823.206298	21.153216
76.314991	2821.956949	21.158234
76.473984	2847.946475	21.163251
77.032940	2851.968772	21.168269
76.688315	2862.303071	21.173287
76.635390	2854.868997	21.178304
76.683732	2862.944954	21.183322
77.104395	2870.475887	21.188339
77.029615	2861.630323	21.193357
77.089921	2861.968884	21.198375
77.018903	2852.857274	21.203392
76.921917	2863.592511	21.208410
77.153590	2860.499463	21.213427
77.319739	2863.660582	21.218445
77.292037	2868.997081	21.223463
77.561150	2878.385850	21.228480
77.527761	2882.748337	21.233498
77.504757	2886.400246	21.238515
77.505261	2881.287373	21.243533
77.652805	2894.258313	21.248551
77.685172	2890.096853	21.253568
77.801156	2892.225431	21.258586
77.836841	2890.229965	21.263603
78.137962	2901.950722	21.268621
78.118797	2910.814807	21.273639
78.200404	2913.563575	21.278656
78.033032	2908.667699	21.283674
78.188764	2919.623478	21.288691
78.353788	2908.986037	21.293709
78.149952	2916.343690	21.298727
78.459141	2916.801032	21.303744
78.234428	2938.846258	21.308762
78.579627	2945.160790	21.313779
79.012068	2943.164238	21.318797
79.175361	2937.709989	21.323815
79.380024	2935.586315	21.328832
79.091585	2941.180180	21.333850
79.256664	2936.055612	21.338867
79.192078	2928.866069	21.343885
79.125861	2938.853416	21.348903
79.452014	2929.753213	21.353920
79.882296	2928.633583	21.358938
79.508212	2935.483319	21.363955
79.636149	2931.970948	21.368973
79.698274	2948.734487	21.373991
80.037656	2959.871449	21.379008
80.039045	2970.678887	21.384026
79.763386	2970.494619	21.389043
80.096423	2962.953369	21.394061
79.888272	2967.255273	21.399079
80.417228	2959.686736	21.404096
80.243146	2965.435055	21.409114
80.217753	2971.108268	21.414131
80.333607	2965.924399	21.419149
80.866642	2962.887561	21.424167
80.754937	2958.358579	21.429184
80.990686	2952.773769	21.434202
80.677974	2965.091247	21.439219
80.631436	2956.769239	21.444237
80.631866	2961.038531	21.449255
80.630476	2966.146886	21.454272
81.012601	2980.775656	21.459290
81.138171	2993.637825	21.464307
81.111195	2987.643624	21.469325
80.909359	2994.044085	21.474343
81.255854	2987.374708	21.479360
81.502931	2987.003163	21.484378
81.521061	2986.832319	21.489395
81.716206	2979.633664	21.494413
81.338653	2977.027007	21.499431
81.533793	2979.745297	21.504448
81.944127	2982.165224	21.509466
81.755561	3007.459332	21.514483
82.015659	3015.332888	21.519501
81.967059	3014.289840	21.524519
82.038967	3012.236169	21.529536
82.080522	3013.656119	21.534554
82.063585	3015.627939	21.539571
82.221534	3014.117897	21.544589
82.004685	3018.488248	21.549607
82.289458	3012.631967	21.554624
82.031241	3032.848053	21.559642
82.347530	3046.213110	21.564659
82.483819	3045.395108	21.569677
82.414212	3051.884756	21.574695
82.151065	3060.389097	21.579712
82.773124	3065.852110	21.584730
82.479400	3070.334888	21.589747
82.567586	3074.307217	21.594765
82.802064	3085.996222	21.599783
82.960468	3092.109719	21.604800
83.140623	3100.272671	21.609818
83.272079	3096.707681	21.614835
83.469742	3093.849601	21.619853
83.472809	3099.077732	21.624871
83.538674	3116.571669	21.629888
84.051598	3123.720690	21.634906
83.897873	3125.632493	21.639923
84.527236	3125.471841	21.644941
84.488772	3130.969362	21.649959
84.640485	3122.447101	21.654976
84.677736	3106.891819	21.659994
84.680788	3100.794768	21.665011
84.637548	3094.666278	21.670029
84.484415	3097.119032	21.675047
84.597379	3092.961815	21.680064
84.625121	3099.326109	21.685082
84.503496	3091.761939	21.690099
84.734802	3110.019796	21.695117
84.968636	3128.283541	21.700135
84.893897	3125.283927	21.705152
84.967768	3126.812544	21.710170
84.922741	3129.145961	21.715187
84.720899	3120.842616	21.720205
84.866927	3117.898088	21.725223
84.876168	3132.155404	21.730240
85.345312	3144.263372	21.735258
85.162064	3154.941140	21.740275
85.538945	3153.073798	21.745293
85.603695	3152.118418	21.750311
85.772697	3155.125532	21.755328
85.999494	3144.732514	21.760346
85.733802	3150.051630	21.765363
85.942807	3149.353468	21.770381
85.687159	3154.318820	21.775399
85.996503	3174.862283	21.780416
86.347017	3184.335727	21.785434
86.023617	3189.336333	21.790451
85.940812	3183.693433	21.795469
86.363780	3188.246328	21.800487
86.140880	3185.792687	21.805504
86.181474	3188.188615	21.810522
85.931461	3204.597192	21.815539
86.181839	3209.945988	21.820557
86.217865	3220.861856	21.825575
86.274756	3238.208617	21.830592
86.756010	3240.445523	21.835610
86.947821	3244.541106	21.840627
87.262001	3235.542802	21.845645
87.239268	3241.339305	21.850663
87.220495	3255.843320	21.855680
87.652368	3262.413258	21.860698
87.596427	3267.535789	21.865715
87.971834	3262.475078	21.870733
87.559962	3261.815624	21.875751
87.653931	3263.265202	21.880768
88.135217	3259.225936	21.885786
87.601429	3271.613845	21.890803
87.738340	3255.792457	21.895821
87.837476	3267.953717	21.900839
87.842061	3291.184014	21.905856
88.420840	3290.324005	21.910874
88.311528	3296.067639	21.915891
88.179699	3302.201836	21.920909
88.271249	3303.159597	21.925927
88.141806	3314.629999	21.930944
88.568598	3321.709608	21.935962
88.814485	3326.355120	21.940979
88.784497	3331.955218	21.945997
89.141116	3325.476134	21.951015
88.878579	3324.408312	21.956032
89.301269	3321.721895	21.961050
88.826093	3330.015431	21.966067
88.870839	3347.221842	21.971085
89.507647	3361.705708	21.976103
89.218893	3356.561938	21.981120
89.450278	3349.934196	21.986138
89.304032	3361.446104	21.991155
89.532655	3375.947195	21.996173
89.733346	3376.504274	22.001191
89.982057	3385.024996	22.006208
90.205385	3385.651439	22.011226
89.912277	3386.783838	22.016243
89.814750	3382.503540	22.021261
89.961829	3385.005681	22.026279
90.131522	3407.113894	22.031296
90.815301	3403.666004	22.036314
90.333225	3408.022076	22.041331
90.360819	3406.939950	22.046349
90.524624	3405.840772	22.051367
91.017212	3408.986203	22.056384
91.008812	3401.379633	22.061402
91.212768	3399.867968	22.066419
90.894305	3397.214880	22.071437
90.796585	3408.411347	22.076455
90.981937	3421.180921	22.081472
91.448647	3425.975262	22.086490
91.349330	3436.074134	22.091507
91.564374	3435.186692	22.096525
91.709724	3432.000435	22.101543
91.501937	3434.450010	22.106560
91.975763	3436.136124	22.111578
91.553411	3428.323280	22.116595
91.701565	3431.437195	22.121613
91.792308	3448.486977	22.126631
91.682436	3464.667814	22.131648
91.865977	3462.759551	22.136666
92.037800	3462.462330	22.141683
92.052645	3463.112705	22.146701
92.609349	3481.654655	22.151719
92.332188	3488.350972	22.156736
92.800858	3493.856186	22.161754
92.710941	3496.906180	22.166771
92.660962	3496.509157	22.171789
93.034355	3496.915344	22.176807
92.721729	3501.877184	22.181824
93.042928	3493.287863	22.186842
93.014533	3514.058215	22.191859
93.312639	3529.428843	22.196877
94.287658	3500.979498	22.201895
94.776665	3479.836455	22.206912
95.267326	3454.430760	22.211930
95.137116	3450.110366	22.216947
94.991925	3420.853770	22.221965
95.239942	3405.342393	22.226983
94.856329	3392.531242	22.232000
94.683366	3365.869858	22.237018
94.722917	3369.689935	22.242035
95.134171	3364.051266	22.247053
95.125350	3358.520056	22.252071
94.750580	3347.016381	22.257088
94.767134	3330.372056	22.262106
94.485758	3332.260088	22.267123
94.673476	3332.658724	22.272141
94.848787	3344.664434	22.277159
95.105214	3370.599530	22.282176
94.935451	3360.828812	22.287194
95.059246	3368.085613	22.292211
95.062869	3363.681656	22.297229
95.182137	3364.529134	22.302247
95.167624	3371.778145	22.307264
95.432700	3366.867056	22.312282
95.251765	3367.789628	22.317299
95.176274	3374.074860	22.322317
95.111268	3382.218558	22.327335
95.192031	3404.162447	22.332352
95.404260	3396.357387	22.337370
95.648834	3403.966812	22.342387
95.507345	3415.297588	22.347405
95.957398	3427.604370	22.352423
95.860465	3440.162453	22.357440
95.993392	3433.263301	22.362458
96.030518	3442.996976	22.367475
96.000205	3459.638293	22.372493
95.934982	3475.623255	22.377511
95.737612	3481.304870	22.382528
95.660540	3490.625768	22.387546
96.019270	3504.465942	22.392563
96.059138	3516.918724	22.397581
96.374599	3525.665142	22.402599
96.613881	3542.894334	22.407616
97.004077	3556.058922	22.412634
96.934587	3568.117796	22.417651
97.113220	3576.212737	22.422669
97.397594	3562.367025	22.427687
97.057167	3575.071708	22.432704
97.364046	3593.627481	22.437722
97.719533	3602.956197	22.442739
97.806166	3606.098020	22.447757
97.704080	3607.278019	22.452775
97.797613	3605.080373	22.457792
97.962352	3613.127309	22.462810
98.125463	3625.239286	22.467827
98.228536	3621.534915	22.472845
98.421208	3613.636228	22.477863
98.218292	3630.593999	22.482880
98.401338	3633.762617	22.487898
98.861198	3648.166034	22.492915
98.998019	3656.152408	22.497933
99.176682	3653.814146	22.502951
98.896664	3652.833570	22.507968
99.136686	3656.638251	22.512986
99.009618	3664.497387	22.518003
99.144455	3658.065640	22.523021
99.244145	3655.012394	22.528039
99.421790	3676.117804	22.533056
99.400418	3672.977409	22.538074
99.788073	3680.571101	22.543091
99.558037	3689.701752	22.548109
99.937755	3677.031224	22.553127
99.560662	3679.261770	22.558144
99.552689	3695.304084	22.563162
99.932530	3709.303063	22.568179
100.203676	3711.509903	22.573197
100.339690	3714.966984	22.578215
100.212287	3719.656133	22.583232
100.098633	3723.655355	22.588250
100.408077	3740.091439	22.593267
100.230498	3751.586949	22.598285
100.917047	3743.043547	22.603303
100.834808	3743.885425	22.608320
101.232860	3743.084732	22.613338
101.305500	3752.723511	22.618355
101.242353	3772.113200	22.623373
101.480075	3768.536931	22.628391
101.417341	3785.223528	22.633408
101.345461	3771.008681	22.638426
101.892811	3768.441011	22.643443
101.475708	3778.053502	22.648461
101.692405	3764.290888	22.653479
101.731370	3772.679233	22.658496
102.029932	3780.350468	22.663514
102.088217	3789.039522	22.668531
102.123356	3803.064601	22.673549
102.245620	3794.425737	22.678567
102.415731	3802.493114	22.683584
102.662787	3806.677036	22.688602
103.146039	3792.689914	22.693619
103.057328	3805.413848	22.698637
103.314342	3791.793942	22.703655
103.182864	3792.741925	22.708672
102.630211	3793.517171	22.713690
102.816741	3790.456100	22.718707
102.762473	3809.660803	22.723725
103.112767	3816.484392	22.728743
102.965704	3832.735777	22.733760
103.176670	3839.328868	22.738778
103.531246	3839.346067	22.743795
103.464095	3856.810073	22.748813
103.669796	3854.755409	22.753831
103.955738	3857.893830	22.758848
103.683167	3853.771004	22.763866
103.765163	3863.623262	22.768883
103.775624	3884.986019	22.773901
104.261215	3887.922459	22.778919
104.707904	3888.416907	22.783936
104.456110	3880.467481	22.788954
104.869117	3873.326372	22.793971
105.067572	3872.981260	22.798989
105.338101	3875.976621	22.804007
105.294715	3881.250780	22.809024
105.010568	3881.715362	22.814042
104.984376	3879.162517	22.819059
104.943832	3898.356311	22.824077
105.122538	3899.797722	22.829095
105.463224	3906.959305	22.834112
105.420155	3911.434001	22.839130
105.675110	3907.334139	22.844147
105.517634	3913.299695	22.849165
105.887195	3928.667916	22.854183
106.036016	3942.460976	22.859200
105.557958	3944.660823	22.864218
106.143993	3943.768036	22.869235
106.114454	3948.524748	22.874253
106.260368	3945.460371	22.879271
106.054737	3940.940906	22.884288
106.034670	3954.525861	22.889306
106.451050	3967.218466	22.894323
105.959943	3970.963478	22.899341
106.431185	3975.827310	22.904359
106.780961	3998.154365	22.909376
106.466747	4005.165205	22.914394
107.049906	4006.077324	22.919411
106.961898	4012.937547	22.924429
107.445094	4023.192903	22.929447
107.913227	4025.580247	22.934464
107.883117	4029.282471	22.939482
107.958083	4029.965881	22.944499
108.054224	4032.297283	22.949517
108.053822	4031.114374	22.954535
108.335696	4026.198627	22.959552
107.776657	4025.433622	22.964570
108.234628	4025.794610	22.969587
108.372974	4027.164978	22.974605
108.375442	4018.755246	22.979623
108.241285	4027.434893	22.984640
108.252324	4055.436557	22.989658
108.435894	4061.504374	22.994675
108.499732	4068.497688	22.999693
108.594360	4066.409269	23.004711
108.910817	4066.169154	23.009728
108.815789	4077.267968	23.014746
109.216836	4072.118333	23.019763
109.409881	4079.179289	23.024781
109.900913	4077.093795	23.029799
109.822012	4067.914311	23.034816
109.774548	4081.283540	23.039834
110.276062	4084.579591	23.044851
110.112092	4087.591198	23.049869
110.356238	4092.364831	23.054887
110.567352	4096.189539	23.059904
110.508064	4091.664633	23.064922
110.666776	4081.365374	23.069939
110.636549	4086.363255	23.074957
110.473762	4081.666280	23.079975
110.536932	4075.285245	23.084992
110.801740	4087.760560	23.090010
111.377413	4090.287002	23.095027
111.411248	4082.311347	23.100045
111.432989	4080.830071	23.105063
111.516751	4077.780261	23.110080
111.517277	4087.660015	23.115098
111.325742	4074.563341	23.120115
111.432232	4082.958390	23.125133
111.569941	4093.452597	23.130151
111.617914	4105.301141	23.135168
111.704113	4111.509326	23.140186
111.719236	4105.986352	23.145203
111.905363	4111.863935	23.150221
112.013470	4110.616736	23.155239
112.043542	4125.768473	23.160256
111.867685	4151.423748	23.165274
112.349777	4142.430013	23.170291
112.264253	4154.634642	23.175309
112.114899	4156.759261	23.180327
112.259371	4169.637266	23.185344
112.462652	4179.578408	23.190362
112.205062	4183.750493	23.195379
112.481654	4203.955150	23.200397
112.533184	4211.375165	23.205415
112.926785	4226.311877	23.210432
113.299322	4237.675625	23.215450
114.205204	4218.389019	23.220467
114.225036	4225.555346	23.225485
114.258960	4218.724809	23.230503
114.338766	4222.791018	23.235520
114.365762	4219.103489	23.240538
114.387915	4219.555738	23.245555
114.364657	4221.507526	23.250573
114.613354	4222.113116	23.255591
114.875215	4217.641809	23.260608
114.596455	4224.947539	23.265626
115.101649	4217.254103	23.270643
114.709340	4222.823692	23.275661
114.891493	4232.648771	23.280679
115.255836	4224.298973	23.285696
114.658009	4241.502313	23.290714
115.133638	4245.351809	23.295731
114.957006	4262.264006	23.300749
115.606116	4259.058169	23.305767
115.437285	4265.429855	23.310784
115.227585	4281.126137	23.315802
115.467508	4288.313834	23.320819
115.893283	4281.850861	23.325837
115.805342	4296.916664	23.330855
116.282552	4303.970749	23.335872
116.081546	4324.717411	23.340890
116.101350	4322.974164	23.345907
116.316176	4320.227917	23.350925
115.961819	4324.725377	23.355943
116.068657	4346.507004	23.360960
115.740018	4354.404189	23.365978
116.238637	4368.828403	23.370995
116.523693	4385.493029	23.376013
116.503508	4399.574591	23.381031
116.753797	4408.483900	23.386048
116.748751	4424.568983	23.391066
117.245213	4430.914895	23.396083
117.148748	4446.742366	23.401101
117.734620	4448.877241	23.406119
117.633355	4443.840381	23.411136
117.367493	4468.527845	23.416154
117.981630	4475.798762	23.421171
117.964004	4485.204570	23.426189
118.307202	4475.010477	23.431207
118.520908	4461.973181	23.436224
118.205284	4480.839138	23.441242
118.782629	4498.616322	23.446259
118.965713	4508.956527	23.451277
118.433599	4503.634348	23.456295
119.069075	4502.560567	23.461312
118.869863	4509.235284	23.466330
119.181837	4507.663254	23.471347
119.388238	4528.878294	23.476365
118.948670	4532.335776	23.481383
119.208018	4530.721570	23.486400
119.743550	4540.234215	23.491418
119.422156	4542.099316	23.496435
119.740813	4556.782182	23.501453
119.960053	4559.185500	23.506471
120.309802	4555.218873	23.511488
119.722870	4566.599267	23.516506
119.873260	4576.275628	23.521523
120.261506	4586.723274	23.526541
120.361040	4597.195218	23.531559
120.570838	4588.644884	23.536576
120.713496	4611.156389	23.541594
120.879748	4621.902824	23.546611
121.362671	4623.520566	23.551629
121.011469	4622.262277	23.556647
121.564677	4611.715462	23.561664
121.378484	4619.282753	23.566682
122.053777	4634.158959	23.571699
122.369423	4633.586593	23.576717
122.099020	4631.889913	23.581735
122.783977	4615.820411	23.586752
123.192007	4603.176587	23.591770
122.949127	4597.826845	23.596787
123.140143	4593.277000	23.601805
123.261206	4597.511088	23.606823
123.293570	4596.404434	23.611840
122.854825	4596.201627	23.616858
123.082133	4593.261009	23.621875
123.295200	4598.467813	23.626893
122.244039	4599.356907	23.631911
123.021872	4590.613888	23.636928
123.030057	4590.488051	23.641946
122.678808	4596.170452	23.646963
123.022262	4615.340242	23.651981
123.301954	4629.117767	23.656999
123.595749	4640.393700	23.662016
123.176215	4657.925300	23.667034
123.170016	4658.490329	23.672051
123.916403	4665.583497	23.677069
123.740790	4681.258577	23.682087
124.102805	4689.736166	23.687104
123.864299	4700.618994	23.692122
124.394421	4711.794601	23.697139
124.787850	4732.952648	23.702157
124.621900	4734.145253	23.707175
124.833387	4724.643080	23.712192
124.482852	4737.230700	23.717210
124.690122	4747.547223	23.722227
124.650013	4749.768190	23.727245
124.324351	4772.794991	23.732263
124.909353	4777.564747	23.737280
125.049817	4796.532474	23.742298
125.318866	4815.727865	23.747315
125.744399	4814.946043	23.752333
125.533469	4826.413392	23.757351
125.956652	4832.549912	23.762368
126.030978	4842.688437	23.767386
126.167052	4846.566364	23.772403
126.728445	4846.506369	23.777421
126.604446	4846.967938	23.782439
127.050490	4853.325028	23.787456
126.969846	4863.401128	23.792474
127.285013	4877.159398	23.797491
127.430143	4874.671540	23.802509
127.421294	4877.332189	23.807527
127.660857	4863.347311	23.812544
127.792310	4867.672634	23.817562
128.009125	4865.611211	23.822579
128.216771	4861.774415	23.827597
127.941070	4871.288495	23.832615
127.980817	4865.551519	23.837632
127.966518	4877.268750	23.842650
128.068842	4889.275546	23.847667
128.288177	4890.272149	23.852685
128.220230	4898.057172	23.857703
128.491218	4896.577199	23.862720
128.847588	4911.704468	23.867738
128.797675	4924.140667	23.872755
129.183047	4930.981571	23.877773
128.824277	4929.813559	23.882791
128.889010	4937.701881	23.887808
128.956376	4950.554357	23.892826
128.810324	4962.682553	23.897843
129.239376	4962.017483	23.902861
129.245021	4988.764619	23.907879
129.549935	4979.692093	23.912896
129.409417	4986.633416	23.917914
129.634189	5011.851199	23.922931
129.837800	5017.327567	23.927949
129.760439	5029.623625	23.932967
130.055536	5037.823801	23.937984
130.653550	5051.367537	23.943002
130.499571	5045.606996	23.948019
131.033170	5060.659915	23.953037
131.132378	5080.589702	23.958055
131.457202	5083.883964	23.963072
131.327150	5081.839444	23.968090
131.625140	5082.464976	23.973107
131.854043	5077.445353	23.978125
131.927430	5087.732276	23.983143
131.856338	5082.532506	23.988160
132.019146	5084.923525	23.993178
131.713420	5085.078347	23.998195
132.305218	5089.023138	24.003213
132.145392	5108.745313	24.008231
132.286217	5112.627217	24.013248
132.425207	5106.336741	24.018266
132.493474	5110.152316	24.023283
132.872194	5120.848489	24.028301
132.877685	5134.878255	24.033319
132.688056	5136.282104	24.038336
133.062452	5134.184181	24.043354
133.065385	5136.580561	24.048371
133.388254	5148.120466	24.053389
133.442916	5161.996895	24.058407
133.682116	5165.843043	24.063424
133.478548	5160.702979	24.068442
133.422469	5189.196265	24.073459
133.857574	5198.405945	24.078477
134.063008	5202.248439	24.083495
134.097582	5209.628505	24.088512
134.495282	5231.065321	24.093530
134.775620	5230.621866	24.098547
135.077312	5220.370612	24.103565
135.006019	5231.462225	24.108583
135.110927	5215.738102	24.113600
134.898950	5233.090608	24.118618
135.080976	5250.336993	24.123635
135.327205	5247.053526	24.128653
135.363037	5261.161695	24.133671
135.175146	5270.159998	24.138688
135.702472	5279.871417	24.143706
135.465858	5284.985400	24.148723
135.538797	5291.475945	24.153741
136.256849	5312.645281	24.158759
136.617848	5305.274574	24.163776
137.021477	5309.104384	24.168794
137.201420	5314.480152	24.173811
136.988008	5308.261037	24.178829
136.964796	5311.097509	24.183847
137.164604	5318.832898	24.188864
137.414737	5332.983160	24.193882
137.696270	5344.329438	24.198899
138.135170	5331.975913	24.203917
137.758496	5338.398622	24.208935
137.568938	5342.723969	24.213952
138.051451	5334.802311	24.218970
137.728885	5343.027402	24.223987
138.073535	5347.641618	24.229005
137.778323	5370.864133	24.234023
137.937551	5372.611490	24.239040
138.270039	5376.466903	24.244058
138.111177	5390.563665	24.249075
138.046318	5402.458514	24.254093
138.135979	5422.150123	24.259111
138.481708	5439.680571	24.264128
139.229937	5448.085271	24.269146
138.961165	5448.511023	24.274163
139.324508	5457.425174	24.279181
139.786834	5464.907682	24.284199
139.903774	5474.128745	24.289216
139.903464	5465.130323	24.294234
140.200814	5472.343374	24.299251
140.212888	5467.285969	24.304269
140.169822	5467.746284	24.309287
140.212014	5479.734690	24.314304
140.324396	5489.785185	24.319322
140.341696	5489.122155	24.324339
140.855699	5494.100437	24.329357
141.147027	5508.201259	24.334375
140.750566	5519.171586	24.339392
140.872985	5525.048015	24.344410
140.778921	5537.221298	24.349427
140.973535	5545.638249	24.354445
140.830531	5558.569816	24.359463
141.233525	5581.123926	24.364480
142.411802	5581.222058	24.369498
142.217131	5591.208677	24.374515
142.568659	5582.058503	24.379533
142.431493	5584.863359	24.384551
142.565976	5584.774941	24.389568
142.749572	5603.013927	24.394586
142.957196	5620.343759	24.399603
142.948059	5608.570162	24.404621
143.194193	5618.080298	24.409639
143.139457	5608.398746	24.414656
143.724083	5603.603908	24.419674
143.538939	5612.903619	24.424691
143.487839	5629.372757	24.429709
143.545369	5643.865877	24.434727
143.369210	5641.631478	24.439744
143.852494	5660.549345	24.444762
143.329465	5671.402052	24.449779
143.617544	5680.838868	24.454797
143.875231	5695.231556	24.459815
143.870195	5716.738069	24.464832
144.553342	5732.964865	24.469850
144.638569	5738.434208	24.474867
144.901327	5741.947202	24.479885
145.007568	5751.235637	24.484903
145.111724	5773.594701	24.489920
145.391686	5767.352267	24.494938
145.517553	5779.683382	24.499955
145.744011	5783.673651	24.504973
145.985943	5802.114756	24.509991
146.570949	5803.953799	24.515008
146.803724	5798.855305	24.520026
146.882983	5802.335178	24.525043
147.051438	5797.150823	24.530061
146.898961	5800.123758	24.535079
146.933653	5791.657151	24.540096
147.244426	5788.145893	24.545114
146.947610	5786.432345	24.550131
147.378524	5791.651823	24.555149
147.557082	5783.312583	24.560167
147.287568	5790.281094	24.565184
147.542431	5792.331121	24.570202
147.420293	5791.388717	24.575219
147.467155	5813.573338	24.580237
147.641838	5826.137944	24.585255
147.743285	5836.934910	24.590272
148.170249	5849.899763	24.595290
148.059353	5857.988005	24.600307
148.493647	5864.006446	24.605325
148.739485	5869.820097	24.610343
148.591829	5889.951545	24.615360
148.918337	5891.385134	24.620378
148.893829	5897.303430	24.625395
149.177824	5914.701624	24.630413
149.170583	5925.798494	24.635431
148.953976	5933.671736	24.640448
149.553392	5939.117594	24.645466
149.596940	5949.855244	24.650483
149.448514	5950.523471	24.655501
149.532785	5960.163174	24.660519
149.691437	5977.352125	24.665536
149.977225	5990.276702	24.670554
150.447564	6005.331914	24.675571
150.654104	6018.082624	24.680589
151.109078	6024.280330	24.685607
151.105765	6043.976831	24.690624
151.328503	6040.821689	24.695642
151.131491	6052.100843	24.700659
151.357782	6054.596921	24.705677
151.850904	6070.316269	24.710695
151.681587	6068.416201	24.715712
151.738008	6067.165896	24.720730
152.005792	6080.830931	24.725747
152.094515	6088.844109	24.730765
152.369396	6097.193241	24.735783
152.396190	6098.616787	24.740800
152.931594	6111.202491	24.745818
153.452263	6126.767507	24.750835
153.360354	6120.473679	24.755853
153.737037	6122.655683	24.760871
153.494759	6122.882343	24.765888
153.388373	6124.930536	24.770906
153.603127	6122.523501	24.775923
153.661190	6137.815722	24.780941
154.032136	6142.933742	24.785959
153.893514	6157.365641	24.790976
154.178314	6144.294304	24.795994
154.155069	6152.295988	24.801011
153.747196	6180.191246	24.806029
154.334952	6175.826586	24.811047
154.264333	6194.361899	24.816064
154.366129	6207.834938	24.821082
154.735514	6222.197139	24.826099
154.754293	6224.891875	24.831117
155.026089	6237.601641	24.836135
155.134429	6252.993272	24.841152
155.583427	6269.063039	24.846170
156.002185	6280.421910	24.851187
155.850513	6280.403812	24.856205
156.503056	6289.024662	24.861223
156.403082	6293.508206	24.866240
156.323106	6305.752130	24.871258
156.884107	6318.751105	24.876275
156.973240	6313.673921	24.881293
156.973898	6320.318280	24.886311
156.810419	6325.075819	24.891328
157.552951	6339.516738	24.896346
157.333236	6347.604977	24.901363
157.287585	6351.174915	24.906381
157.710684	6346.367376	24.911399
157.070992	6373.688285	24.916416
157.782117	6372.392680	24.921434
157.919671	6391.016995	24.926451
157.782543	6403.500020	24.931469
158.475590	6406.253288	24.936487
158.213519	6415.190116	24.941504
158.684849	6427.180504	24.946522
158.771037	6441.597753	24.951539
158.852545	6454.311166	24.956557
159.561911	6460.489854	24.961575
158.980428	6463.890146	24.966592
159.419140	6473.011726	24.971610
159.506931	6485.002524	24.976627
159.480369	6493.709967	24.981645
160.023047	6497.867563	24.986663
160.007180	6519.955211	24.991680
160.182239	6521.416397	24.996698
160.684317	6526.805888	25.001715
160.522309	6531.247354	25.006733
161.416024	6532.053625	25.011751
161.368140	6540.924659	25.016768
161.621238	6545.840871	25.021786
162.288766	6545.226242	25.026803
162.270033	6538.553407	25.031821
162.244028	6532.664042	25.036839
162.328743	6540.841983	25.041856
162.751057	6533.884006	25.046874
162.694669	6532.931074	25.051891
162.640143	6537.953584	25.056909
162.476060	6532.263554	25.061927
162.751342	6532.835539	25.066944
163.058077	6530.047954	25.071962
163.169914	6532.793747	25.076979
162.943650	6529.684759	25.081997
163.456911	6551.404462	25.087015
163.147197	6561.992757	25.092032
163.443609	6565.734124	25.097050
163.230983	6569.305951	25.102067
163.225606	6581.416775	25.107085
163.527408	6594.421023	25.112103
163.752290	6605.792880	25.117120
164.041313	6625.047690	25.122138
164.465011	6629.273769	25.127155
164.425595	6632.829310	25.132173
164.710379	6646.674673	25.137191
164.703532	6663.891161	25.142208
164.883103	6658.842478	25.147226
164.977310	6682.385346	25.152243
164.870682	6699.182566	25.157261
165.320875	6694.931154	25.162279
165.402250	6726.242649	25.167296
165.557275	6719.525773	25.172314
165.706433	6739.609772	25.177331
165.871540	6759.995920	25.182349
166.355071	6751.772475	25.187367
166.719956	6776.191531	25.192384
167.000609	6779.511843	25.197402
167.336473	6777.379355	25.202419
167.156061	6786.667906	25.207437
167.270324	6788.300240	25.212455
167.414942	6800.073568	25.217472
167.029738	6814.364783	25.222490
167.461604	6820.458842	25.227507
167.939651	6838.783472	25.232525
167.945319	6843.914710	25.237543
168.083161	6853.960126	25.242560
167.910328	6873.354277	25.247578
168.474344	6877.526435	25.252595
168.241579	6887.774048	25.257613
168.740673	6889.885548	25.262631
169.238709	6889.443335	25.267648
169.460624	6892.528749	25.272666
169.686986	6901.351395	25.277683
169.667072	6913.737524	25.282701
170.214424	6925.096870	25.287719
169.907127	6929.926507	25.292736
170.225369	6924.436459	25.297754
170.502043	6928.356178	25.302771
170.260431	6956.162839	25.307789
170.457423	6957.992128	25.312807
170.626359	6960.909391	25.317824
170.737148	6976.445458	25.322842
170.928981	6986.891337	25.327859
170.839286	6998.337882	25.332877
171.518188	7001.334738	25.337895
171.536268	7017.565785	25.342912
171.804165	7025.991440	25.347930
171.983862	7015.485815	25.352947
171.545490	7032.436359	25.357965
171.980898	7042.616008	25.362983
172.236617	7060.379520	25.368000
172.001691	7056.141475	25.373018
172.238946	7082.688564	25.378035
172.314879	7093.945293	25.383053
172.763524	7114.619664	25.388071
173.113145	7132.921745	25.393088
172.960029	7142.744653	25.398106
173.334787	7152.227356	25.403123
172.958627	7173.107001	25.408141
173.316706	7186.430583	25.413159
173.465963	7197.739413	25.418176
174.129086	7217.623257	25.423194
174.229686	7228.609586	25.428211
174.372162	7232.442097	25.433229
174.690007	7245.000611	25.438247
175.140732	7257.415040	25.443264
175.003416	7264.724688	25.448282
175.125225	7261.169880	25.453299
175.413009	7285.052279	25.458317
175.473147	7281.380419	25.463335
175.395586	7296.668637	25.468352
175.876926	7313.396433	25.473370
176.249904	7322.228053	25.478387
176.082407	7340.082543	25.483405
176.448193	7349.735485	25.488423
176.261991	7352.269393	25.493440
176.696456	7373.014278	25.498458
177.190314	7391.732297	25.503475
177.142895	7403.252237	25.508493
177.978687	7380.322513	25.513511
178.313996	7372.666941	25.518528
178.344446	7370.158182	25.523546
178.560898	7373.543193	25.528563
179.225518	7372.796693	25.533581
179.314795	7354.244242	25.538599
179.630661	7353.821431	25.543616
179.376538	7350.987263	25.548634
179.649176	7344.572165	25.553651
179.819413	7347.772088	25.558669
180.276157	7338.771465	25.563687
179.899795	7340.742411	25.568704
179.762851	7342.527366	25.573722
180.012492	7336.250923	25.578739
180.107746	7340.628817	25.583757
180.490293	7345.052785	25.588775
180.792385	7357.345458	25.593792
180.582556	7372.321618	25.598810
181.025348	7368.310784	25.603827
180.548772	7372.421970	25.608845
180.565158	7373.948250	25.613863
181.159832	7388.190957	25.618880
180.912495	7399.380424	25.623898
180.938554	7399.847062	25.628915
181.211947	7422.038410	25.633933
181.622365	7438.454718	25.638951
181.577813	7435.231685	25.643968
181.417823	7459.936342	25.648986
181.981815	7466.933645	25.654003
181.967982	7491.376174	25.659021
181.767134	7503.778019	25.664039
182.255892	7515.052510	25.669056
182.055900	7540.708701	25.674074
182.512369	7555.486521	25.679092
182.878595	7567.213760	25.684109
182.999020	7590.713291	25.689127
183.336291	7604.890025	25.694144
183.185642	7625.836375	25.699162
183.793554	7630.431344	25.704180
184.165621	7646.747300	25.709197
184.237347	7658.628290	25.714215
184.902943	7670.352342	25.719232
185.193105	7683.620233	25.724250
185.612116	7688.632042	25.729268
185.460094	7699.658060	25.734285
185.588687	7693.832364	25.739303
186.242422	7680.832037	25.744320
186.259783	7683.921946	25.749338
186.719700	7687.734026	25.754356
186.909013	7680.594918	25.759373
186.723061	7675.215467	25.764391
186.906798	7683.722071	25.769408
186.938177	7705.396754	25.774426
187.142803	7707.844027	25.779444
187.189461	7711.488252	25.784461
187.009965	7709.600759	25.789479
187.359917	7724.089755	25.794496
187.262774	7745.209857	25.799514
187.848603	7747.778498	25.804532
187.870090	7773.406548	25.809549
187.943906	7776.846032	25.814567
187.782664	7788.405455	25.819584
188.189998	7814.317210	25.824602
188.373727	7819.959454	25.829620
188.442563	7837.502193	25.834637
188.237563	7855.063531	25.839655
188.963272	7865.616993	25.844672
188.664748	7886.691445	25.849690
188.868737	7899.063587	25.854708
188.967173	7922.780080	25.859725
189.225341	7943.911225	25.864743
189.633886	7969.273136	25.869760
189.560703	7990.554103	25.874778
189.993120	7998.940253	25.879796
189.949748	8025.755231	25.884813
190.066186	8043.149016	25.889831
190.849206	8064.766240	25.894848
190.912734	8081.397082	25.899866
191.152684	8086.630362	25.904884
191.520420	8106.335120	25.909901
192.037414	8114.858093	25.914919
191.977516	8114.409868	25.919936
192.433004	8121.918443	25.924954
192.896947	8123.815553	25.929972
192.909291	8133.228612	25.934989
192.837348	8125.759092	25.940007
193.313131	8130.509997	25.945024
193.395586	8148.695173	25.950042
193.826570	8159.747618	25.955060
193.912556	8163.625488	25.960077
193.958502	8160.994201	25.965095
193.921478	8162.674670	25.970112
194.017217	8178.327139	25.975130
194.214944	8197.158314	25.980148
194.150945	8198.124133	25.985165
194.441897	8222.056229	25.990183
194.680635	8216.339090	25.995200
195.055792	8236.647780	26.000218
195.642228	8249.055475	26.005236
195.509814	8254.512568	26.010253
195.780254	8254.825470	26.015271
195.921895	8268.588057	26.020288
196.017379	8289.107045	26.025306
196.422365	8292.537141	26.030324
196.911914	8298.200399	26.035341
196.829297	8326.413110	26.040359
197.175328	8321.442519	26.045376
196.956772	8328.818571	26.050394
196.922451	8333.920111	26.055412
197.122195	8356.899020	26.060429
197.204801	8374.538462	26.065447
197.550153	8382.753024	26.070464
197.602307	8396.787892	26.075482
197.956938	8413.339240	26.080500
197.906727	8429.240714	26.085517
198.120669	8452.301622	26.090535
198.791053	8446.779061	26.095552
198.755728	8467.637407	26.100570
199.220283	8473.271135	26.105588
199.643256	8485.768485	26.110605
199.733521	8505.080898	26.115623
199.766326	8510.846160	26.120640
200.313766	8510.545134	26.125658
200.738085	8488.056235	26.130676
201.568369	8501.318091	26.135693
201.574219	8498.498241	26.140711
201.623711	8494.176393	26.145728
201.769334	8481.918789	26.150746
201.742831	8484.131637	26.155764
201.865619	8500.715727	26.160781
201.927876	8513.520735	26.165799
202.469825	8511.953028	26.170816
202.552178	8506.466643	26.175834
202.487962	8511.116421	26.180852
203.350693	8502.581288	26.185869
202.980522	8507.411139	26.190887
203.492927	8511.423199	26.195904
203.728863	8507.570449	26.200922
203.597160	8505.703030	26.205940
203.831027	8503.865123	26.210957
203.626232	8506.532389	26.215975
203.782062	8508.884945	26.220992
203.421159	8528.141580	26.226010
203.601534	8535.372923	26.231028
203.816290	8562.010615	26.236045
203.571877	8584.876905	26.241063
203.896940	8602.419888	26.246080
204.421000	8627.326576	26.251098
204.213729	8656.938374	26.256116
204.311884	8676.937425	26.261133
204.666681	8698.855809	26.266151
204.789871	8720.112744	26.271168
204.806361	8751.237621	26.276186
204.935048	8777.123061	26.281204
205.371006	8793.961818	26.286221
205.256566	8829.598437	26.291239
205.911568	8850.783292	26.296256
206.262479	8872.196778	26.301274
206.439161	8890.786563	26.306292
207.093682	8901.510487	26.311309
207.745730	8919.662712	26.316327
208.041493	8933.624775	26.321344
208.111155	8945.770999	26.326362
208.391854	8938.728335	26.331380
208.592468	8940.257062	26.336397
208.671286	8962.525648	26.341415
209.042777	8974.681609	26.346432
209.448101	8967.888592	26.351450
209.308900	8985.372911	26.356468
209.332591	9004.469644	26.361485
209.465730	9015.776215	26.366503
209.958647	9021.033408	26.371520
209.914530	9035.535988	26.376538
209.856031	9047.994189	26.381556
210.308282	9061.920085	26.386573
210.311604	9092.844609	26.391591
210.550996	9104.084182	26.396608
210.746815	9122.478715	26.401626
210.857110	9139.926737	26.406644
211.209227	9149.612261	26.411661
211.490734	9166.307705	26.416679
212.575161	9158.503187	26.421696
212.845178	9167.336146	26.426714
212.969926	9164.647068	26.431732
213.394140	9170.198142	26.436749
213.528445	9186.143580	26.441767
213.465670	9181.244379	26.446784
213.828211	9182.983308	26.451802
213.797493	9185.021280	26.456820
213.912878	9181.322186	26.461837
214.215340	9188.350111	26.466855
214.599930	9179.398658	26.471872
214.428202	9182.333755	26.476890
215.019175	9202.687035	26.481908
214.757656	9211.456708	26.486925
214.659345	9223.608299	26.491943
214.960315	9216.421800	26.496960
215.265431	9235.747895	26.501978
215.329613	9248.044982	26.506996
215.657215	9242.740063	26.512013
215.809425	9254.752614	26.517031
216.580510	9256.724064	26.522048
216.457048	9263.790365	26.527066
216.537438	9289.922843	26.532084
217.328904	9295.253435	26.537101
217.165572	9315.057011	26.542119
217.188905	9299.985777	26.547136
217.480972	9326.770629	26.552154
217.772670	9345.957340	26.557172
218.069551	9343.534968	26.562189
217.865121	9361.941656	26.567207
217.970769	9360.522721	26.572224
218.180517	9377.181835	26.577242
218.068293	9400.013223	26.582260
218.574382	9417.984608	26.587277
218.188072	9431.859171	26.592295
218.317796	9458.270252	26.597312
218.752575	9475.188712	26.602330
219.094484	9503.566285	26.607348
219.833683	9525.717722	26.612365
220.198707	9542.911363	26.617383
220.612927	9557.233421	26.622400
220.925244	9558.306574	26.627418
221.199271	9569.083562	26.632436
221.782384	9582.186988	26.637453
221.589722	9589.314141	26.642471
221.874450	9584.519131	26.647488
222.084704	9583.463583	26.652506
222.302946	9602.778221	26.657524
222.341494	9611.206733	26.662541
222.214067	9622.194390	26.667559
222.544964	9639.272649	26.672576
222.878235	9644.276926	26.677594
222.688425	9657.958846	26.682612
223.359221	9674.514026	26.687629
223.545527	9683.990353	26.692647
223.644497	9709.332434	26.697664
223.956501	9712.328104	26.702682
223.971610	9734.993165	26.707700
224.484246	9745.152634	26.712717
224.689654	9759.602061	26.717735
224.775680	9770.802204	26.722752
225.291916	9772.951348	26.727770
224.871359	9783.180981	26.732788
225.017835	9793.497792	26.737805
225.217590	9808.674670	26.742823
225.760457	9830.146347	26.747840
226.263019	9843.418221	26.752858
225.982154	9856.677845	26.757876
226.472291	9870.380487	26.762893
226.713276	9873.963528	26.767911
226.509823	9900.791722	26.772928
227.067148	9901.643261	26.777946
227.034186	9931.874376	26.782964
227.269432	9939.514532	26.787981
227.637461	9962.579552	26.792999
228.149467	9968.270284	26.798016
228.012989	9984.486689	26.803034
227.875470	9998.281269	26.808052
228.337267	10022.936051	26.813069
228.568014	10050.834106	26.818087
228.764805	10065.069396	26.823104
229.314089	10092.834132	26.828122
228.926226	10120.223773	26.833140
229.191314	10138.486251	26.838157
229.083976	10151.664368	26.843175
229.718949	10183.822153	26.848192
230.318568	10204.118487	26.853210
230.510983	10225.627122	26.858228
230.890557	10239.210356	26.863245
231.367502	10256.123984	26.868263
231.668474	10285.455445	26.873280
232.566699	10282.241220	26.878298
232.335314	10287.708079	26.883316
232.685391	10295.914933	26.888333
232.877379	10304.156768	26.893351
232.789279	10324.178750	26.898368
233.171623	10323.174026	26.903386
233.040403	10352.215670	26.908404
233.172241	10355.924685	26.913421
233.150810	10382.441972	26.918439
233.010524	10393.703400	26.923456
233.634126	10417.035701	26.928474
233.330934	10440.908252	26.933492
234.079714	10469.439971	26.938509
233.757185	10492.693450	26.943527
234.295740	10519.781563	26.948544
234.633833	10548.711596	26.953562
234.677942	10578.155376	26.958580
235.158121	10594.027156	26.963597
235.433617	10608.054024	26.968615
235.872217	10624.851691	26.973632
236.536472	10648.200995	26.978650
236.526194	10659.739738	26.983668
236.368347	10678.245512	26.988685
236.797960	10696.346468	26.993703
237.224831	10724.520934	26.998720
237.820548	10732.852949	27.003738
237.812473	10740.892917	27.008756
238.003393	10750.763047	27.013773
238.378777	10770.239671	27.018791
238.284306	10771.434640	27.023808
238.935755	10788.441832	27.028826
239.371534	10805.528558	27.033844
239.479671	10808.039337	27.038861
239.777060	10811.144880	27.043879
239.919681	10832.122324	27.048896
240.318130	10831.538725	27.053914
239.933997	10844.120307	27.058932
240.210333	10859.127453	27.063949
240.705257	10867.081265	27.068967
241.207656	10891.708347	27.073984
242.033930	10895.993425	27.079002
241.679161	10904.077140	27.084020
241.556878	10911.090372	27.089037
241.995601	10913.327028	27.094055
241.652290	10934.447780	27.099072
241.893420	10945.204535	27.104090
242.710719	10953.974606	27.109108
242.829173	10958.614259	27.114125
243.282232	10980.093401	27.119143
243.387573	10992.764547	27.124160
243.290442	11003.264139	27.129178
243.278012	11018.863041	27.134196
243.624703	11045.674465	27.139213
243.938417	11055.734906	27.144231
244.043975	11086.956158	27.149248
244.338624	11094.865616	27.154266
244.863174	11116.028531	27.159284
245.242544	11131.730583	27.164301
245.350251	11153.297516	27.169319
245.304722	11175.847328	27.174336
245.762308	11189.038190	27.179354
245.864166	11206.828705	27.184372
246.222554	11221.525847	27.189389
246.655055	11233.208154	27.194407
247.044733	11247.378324	27.199424
247.727689	11254.780042	27.204442
248.017678	11266.720038	27.209460
248.427334	11268.704851	27.214477
248.510512	11273.200927	27.219495
248.497897	11278.999386	27.224512
248.695126	11291.169627	27.229530
249.118882	11308.271552	27.234548
249.078519	11310.034078	27.239565
249.653018	11318.098973	27.244583
249.728983	11340.243659	27.249600
249.919026	11338.824272	27.254618
250.105920	11350.495181	27.259636
250.198707	11369.552908	27.264653
250.567030	11377.531825	27.269671
250.536046	11395.643169	27.274688
250.911299	11406.563201	27.279706
250.740275	11420.854845	27.284724
251.208766	11444.585561	27.289741
251.258219	11453.942969	27.294759
251.483505	11476.246631	27.299776
252.003179	11491.712229	27.304794
251.808714	11515.759980	27.309812
252.173653	11524.390419	27.314829
252.538559	11543.313453	27.319847
252.403811	11562.960417	27.324864
252.864581	11581.436826	27.329882
253.089115	11609.524584	27.334900
252.987945	11628.215563	27.339917
253.348778	11651.712878	27.344935
253.443701	11684.497306	27.349952
253.859647	11697.772942	27.354970
254.124365	11721.458614	27.359988
254.511094	11749.882862	27.365005
255.179200	11760.470836	27.370023
254.994014	11800.855606	27.375040
255.446650	11810.545987	27.380058
255.722222	11831.711535	27.385076
255.587606	11860.434942	27.390093
255.974200	11877.230213	27.395111
256.035686	11909.637857	27.400128
256.756341	11930.859628	27.405146
257.079602	11950.333991	27.410164
257.500123	11982.932400	27.415181
257.855169	11982.890470	27.420199
257.856412	12013.934374	27.425216
258.324892	12023.472446	27.430234
258.407274	12037.823633	27.435252
258.455948	12066.924171	27.440269
259.208345	12070.468900	27.445287
259.501116	12087.505839	27.450304
259.587726	12103.131352	27.455322
259.866070	12123.146313	27.460340
260.138698	12137.742358	27.465357
260.593604	12152.017185	27.470375
260.577937	12167.720179	27.475392
260.869918	12180.836215	27.480410
261.481018	12195.111101	27.485428
261.653193	12200.301389	27.490445
262.203889	12219.215427	27.495463
262.345935	12233.255538	27.500480
263.087449	12227.073367	27.505498
263.737498	12236.269966	27.510516
263.852250	12258.064098	27.515533
264.388707	12252.479706	27.520551
264.076727	12256.944495	27.525568
264.312136	12257.857656	27.530586
264.630412	12255.946557	27.535604
264.393595	12259.496976	27.540621
264.980809	12268.378126	27.545639
264.559717	12288.231065	27.550656
264.884167	12292.165978	27.555674
264.833435	12305.632423	27.560692
264.901021	12329.765686	27.565709
265.460761	12331.631923	27.570727
265.554798	12360.491955	27.575744
265.846315	12389.367047	27.580762
266.234663	12397.940353	27.585780
266.051496	12424.208141	27.590797
266.482912	12439.535317	27.595815
266.328511	12471.182021	27.600832
266.544533	12487.394074	27.605850
266.879750	12522.386440	27.610868
266.919784	12554.341982	27.615885
267.228803	12568.383706	27.620903
267.547337	12607.853542	27.625920
267.649566	12637.744978	27.630938
268.117653	12670.643938	27.635956
268.124602	12702.324898	27.640973
268.758592	12728.363274	27.645991
268.866723	12768.354989	27.651008
269.194009	12796.329455	27.656026
270.322567	12811.193903	27.661044
270.308708	12829.437862	27.666061
270.867094	12844.425286	27.671079
271.451903	12859.064608	27.676096
271.789241	12877.577828	27.681114
272.273134	12883.826046	27.686132
272.320073	12913.963874	27.691149
272.764099	12913.249466	27.696167
272.997821	12925.219235	27.701184
273.204929	12941.028209	27.706202
273.704726	12951.029559	27.711220
273.858041	12949.130895	27.716237
274.372958	12950.467441	27.721255
274.669674	12973.088729	27.726272
274.453778	12977.724798	27.731290
274.613793	12980.238054	27.736308
274.627463	13007.016789	27.741325
274.728812	13017.127451	27.746343
275.186183	13045.169883	27.751360
275.463329	13062.401224	27.756378
275.611120	13084.236497	27.761396
275.403228	13101.385523	27.766413
275.895243	13121.428126	27.771431
276.640250	13130.527001	27.776448
276.703403	13161.065987	27.781466
276.955298	13176.073150	27.786484
276.963911	13205.715301	27.791501
277.681127	13217.882963	27.796519
277.592068	13248.769730	27.801536
277.855444	13272.148955	27.806554
278.700376	13290.685969	27.811572
278.668998	13313.710710	27.816589
279.251215	13318.876781	27.821607
279.217963	13349.221439	27.826624
279.214005	13371.827038	27.831642
279.824951	13378.595861	27.836660
279.599498	13389.219845	27.841677
279.925542	13409.667944	27.846695
280.075427	13442.419671	27.851712
280.725678	13460.533165	27.856730
281.212623	13475.319058	27.861748
281.291175	13501.732844	27.866765
281.716854	13516.690041	27.871783
282.067264	13542.314931	27.876800
282.164884	13560.482276	27.881818
282.041991	13580.217882	27.886836
282.506620	13597.135518	27.891853
282.867847	13633.897395	27.896871
283.123169	13651.408922	27.901888
283.587172	13678.401576	27.906906
284.147399	13691.628887	27.911924
284.243800	13711.164718	27.916941
284.587660	13729.438204	27.921959
284.914647	13745.432308	27.926976
284.958172	13772.749372	27.931994
285.415721	13784.883156	27.937012
285.860669	13801.869000	27.942029
285.949986	13823.018606	27.947047
286.358218	13843.464191	27.952064
286.534413	13865.489503	27.957082
286.981414	13869.287157	27.962100
287.044477	13899.009489	27.967117
287.634358	13913.734001	27.972135
287.762875	13937.744118	27.977152
287.835558	13950.490927	27.982170
288.228679	13962.473537	27.987188
288.208778	13993.712369	27.992205
288.670219	14017.087077	27.997223
288.869736	14050.189300	28.002240
288.915252	14073.052181	28.007258
289.303624	14090.954337	28.012276
289.360816	14129.894153	28.017293
289.673596	14153.344972	28.022311
290.290142	14176.493143	28.027328
290.551173	14200.897051	28.032346
291.018807	14221.780570	28.037364
291.237763	14247.039761	28.042381
291.379672	14269.969933	28.047399
291.745620	14300.410269	28.052416
291.838854	14326.353143	28.057434
292.468116	14349.772065	28.062452
292.841014	14367.606244	28.067469
293.965433	14375.701355	28.072487
294.523495	14381.059478	28.077504
294.929417	14386.473627	28.082522
295.119939	14370.000901	28.087540
295.645553	14392.679483	28.092557
296.150264	14391.815910	28.097575
296.105602	14374.628474	28.102592
296.323981	14384.128831	28.107610
296.675693	14391.503648	28.112628
296.846400	14393.532963	28.117645
296.811872	14399.881654	28.122663
297.123015	14394.306798	28.127680
296.783459	14400.931595	28.132698
297.285955	14419.114033	28.137716
296.993732	14434.363769	28.142733
297.268436	14464.954028	28.147751
297.516616	14479.397148	28.152768
297.372969	14508.317445	28.157786
297.869388	14529.467535	28.162804
298.074085	14568.985230	28.167821
298.045113	14588.360743	28.172839
298.570014	14627.658190	28.177856
298.745414	14663.551018	28.182874
299.149263	14693.088692	28.187892
299.545879	14723.023300	28.192909
299.883528	14745.955261	28.197927
300.305528	14773.762381	28.202944
300.197717	14805.039879	28.207962
301.055621	14821.541439	28.212980
301.370195	14854.953420	28.217997
301.700464	14873.867320	28.223015
302.444054	14889.291452	28.228032
302.890921	14918.964021	28.233050
303.290658	14933.939566	28.238068
303.226885	14950.025458	28.243085
303.744292	14956.530394	28.248103
304.286185	14978.433036	28.253120
304.428171	14995.021220	28.258138
304.871239	15002.929202	28.263156
305.026614	15026.762907	28.268173
305.190942	15047.753052	28.273191
305.532220	15063.604120	28.278208
305.507364	15091.627076	28.283226
305.948506	15108.859248	28.288244
306.161255	15136.032914	28.293261
306.170570	15150.054127	28.298279
306.656930	15182.006041	28.303296
306.482872	15208.817366	28.308314
306.972772	15231.884691	28.313332
307.803981	15270.320942	28.318349
307.702749	15296.583980	28.323367
308.169071	15309.926422	28.328384
308.378486	15336.394797	28.333402
308.864280	15359.450393	28.338420
309.031621	15387.887008	28.343437
309.314907	15411.269004	28.348455
309.785137	15429.579463	28.353472
309.798757	15460.287243	28.358490
310.737501	15480.344430	28.363508
310.837755	15495.989737	28.368525
310.884006	15521.912586	28.373543
311.658380	15537.492837	28.378560
312.362851	15546.311542	28.383578
312.608142	15546.920544	28.388596
312.881639	15573.778705	28.393613
313.093925	15578.140337	28.398631
313.570830	15590.035685	28.403648
313.710304	15613.644387	28.408666
314.054273	15610.880435	28.413684
314.072617	15624.347203	28.418701
314.215381	15643.773331	28.423719
314.779131	15666.704073	28.428736
314.913740	15689.202388	28.433754
315.031011	15705.158671	28.438772
314.995441	15733.088387	28.443789
315.207496	15761.653546	28.448807
315.483149	15786.692560	28.453824
315.521115	15824.690680	28.458842
316.076113	15859.769110	28.463860
316.172801	15882.584730	28.468877
316.303598	15926.226354	28.473895
316.773548	15958.117944	28.478912
316.750803	15993.186904	28.483930
317.135090	16029.702661	28.488948
317.783266	16064.467615	28.493965
317.463691	16107.021948	28.498983
318.347709	16136.434182	28.504000
318.666751	16182.977890	28.509018
318.893253	16219.432828	28.514036
319.779039	16243.617590	28.519053
320.219495	16276.995094	28.524071
320.712498	16303.908245	28.529088
320.850890	16338.130578	28.534106
321.521382	16357.514384	28.539124
321.731056	16386.177183	28.544141
321.752043	16401.725002	28.549159
322.516636	16424.999135	28.554176
322.577019	16455.768522	28.559194
323.110250	16477.283677	28.564212
323.393866	16499.883663	28.569229
323.474477	16526.096978	28.574247
323.817777	16557.990932	28.579264
324.025673	16581.830474	28.584282
324.787677	16591.115966	28.589300
325.106248	16606.217285	28.594317
325.473987	16642.387252	28.599335
326.307470	16650.788752	28.604352
326.803800	16669.168625	28.609370
328.039378	16665.900143	28.614388
328.901432	16654.401993	28.619405
329.073837	16664.474331	28.624423
329.516969	16652.056396	28.629440
329.694882	16636.335556	28.634458
329.869664	16612.873356	28.639476
330.159993	16611.552999	28.644493
329.974958	16611.422352	28.649511
330.313481	16598.390232	28.654528
330.206594	16617.518196	28.659546
330.545089	16610.772927	28.664564
330.464720	16612.771456	28.669581
330.525867	16640.627789	28.674599
330.890202	16650.758658	28.679616
330.804583	16668.396447	28.684634
330.813311	16684.750619	28.689652
330.854773	16715.700292	28.694669
331.007009	16746.410332	28.699687
331.353573	16777.864318	28.704704
331.651690	16810.211060	28.709722
331.689322	16841.841077	28.714740
332.720533	16868.615607	28.719757
332.903881	16914.779464	28.724775
333.372468	16928.639908	28.729792
333.148651	16965.493680	28.734810
333.366635	17007.203041	28.739828
333.953781	17044.892264	28.744845
334.051125	17084.018143	28.749863
334.646651	17111.575578	28.754880
334.943987	17163.203615	28.759898
335.021326	17195.663037	28.764916
335.675392	17229.297491	28.769933
335.534941	17273.982322	28.774951
336.273218	17311.293106	28.779968
336.320568	17351.413496	28.784986
336.897163	17386.215550	28.790004
337.415968	17427.098756	28.795021
337.532123	17466.222303	28.800039
337.759481	17508.306518	28.805056
337.920288	17547.972811	28.810074
338.463318	17592.177171	28.815092
338.770943	17628.228722	28.820109
338.905367	17665.927567	28.825127
339.408885	17708.051663	28.830144
339.755450	17748.659323	28.835162
340.635786	17785.593672	28.840180
341.098884	17812.287359	28.845197
342.242486	17837.276868	28.850215
343.270968	17835.951306	28.855232
343.857769	17862.051582	28.860250
344.343606	17864.870779	28.865268
345.027576	17862.536927	28.870285
344.839221	17865.011315	28.875303
345.075054	17863.213046	28.880320
345.525471	17877.280770	28.885338
345.457820	17893.780067	28.890356
345.672110	17904.452951	28.895373
345.529144	17929.245307	28.900391
345.943274	17947.546084	28.905408
346.212208	17968.119954	28.910426
346.346073	17987.145155	28.915444
346.550188	18015.958323	28.920461
346.705901	18046.707989	28.925479
346.937558	18075.254826	28.930496
347.027838	18103.967834	28.935514
346.970055	18124.244735	28.940532
347.641902	18163.348771	28.945549
347.864041	18195.433731	28.950567
348.476425	18223.139886	28.955584
349.024076	18248.550621	28.960602
348.928206	18286.991915	28.965620
349.221418	18314.812833	28.970637
349.620176	18364.424901	28.975655
350.261943	18383.483327	28.980672
350.455981	18413.003647	28.985690
350.718555	18452.990455	28.990708
351.112072	18484.133735	28.995725
351.315026	18524.160886	29.000743
352.037077	18554.147508	29.005760
352.835634	18573.724793	29.010778
353.374022	18605.187173	29.015796
353.504919	18628.240322	29.020813
353.697872	18654.928044	29.025831
354.050600	18682.403548	29.030848
354.404719	18708.251766	29.035866
354.689869	18738.058179	29.040884
355.296946	18756.873867	29.045901
355.740784	18797.604561	29.050919
355.852799	18824.773112	29.055936
356.365894	18837.899102	29.060954
356.557762	18876.483201	29.065972
356.596808	18894.937587	29.070989
356.904766	18928.295789	29.076007
357.736449	18966.721566	29.081024
358.395069	18994.715907	29.086042
358.310339	19022.675295	29.091060
358.648652	19035.982755	29.096077
359.254789	19059.927852	29.101095
359.920837	19096.048837	29.106112
360.278998	19114.191775	29.111130
360.921512	19136.344371	29.116148
361.395992	19147.962033	29.121165
361.474598	19160.754379	29.126183
362.332712	19172.936984	29.131200
362.931685	19177.977486	29.136218
362.404198	19192.802012	29.141236
363.063482	19209.890675	29.146253
363.588596	19231.417077	29.151271
364.082003	19251.514152	29.156288
364.469036	19263.711336	29.161306
364.861591	19296.041957	29.166324
364.920689	19297.086651	29.171341
365.257546	19317.104996	29.176359
365.203736	19338.719714	29.181376
365.366742	19362.611898	29.186394
365.593093	19392.995582	29.191412
365.901541	19419.874425	29.196429
365.941074	19447.201457	29.201447
366.396160	19489.507028	29.206464
366.644520	19514.086435	29.211482
366.624212	19551.226328	29.216500
367.200924	19584.254383	29.221517
366.980556	19627.508567	29.226535
367.167497	19658.047694	29.231552
367.836026	19706.149545	29.236570
367.906592	19762.351223	29.241588
368.806308	19797.372521	29.246605
368.938072	19839.305504	29.251623
369.431099	19872.652776	29.256640
371.120108	19879.665252	29.261658
371.964690	19899.456943	29.266676
372.428829	19905.014298	29.271693
372.768856	19926.018291	29.276711
373.072619	19936.639291	29.281728
373.565903	19946.718526	29.286746
373.198527	19980.531971	29.291764
373.930237	19997.311017	29.296781
374.227403	20019.692676	29.301799
374.388292	20042.802533	29.306816
374.661727	20057.108974	29.311834
374.893505	20083.454874	29.316852
375.084686	20108.065442	29.321869
375.336061	20137.705094	29.326887
375.750906	20171.370673	29.331904
376.321278	20199.642310	29.336922
376.244245	20242.509262	29.341940
376.861310	20266.648148	29.346957
377.314712	20302.905921	29.351975
377.303643	20340.777590	29.356992
377.889257	20364.218756	29.362010
378.077667	20407.124202	29.367028
378.447427	20434.493995	29.372045
378.646468	20485.631870	29.377063
378.968931	20522.057618	29.382080
379.204734	20557.526980	29.387098
379.186176	20606.747264	29.392116
380.103460	20646.467803	29.397133
380.360257	20702.492458	29.402151
380.378323	20752.744439	29.407168
381.045188	20787.919651	29.412186
381.260326	20843.816304	29.417204
382.357284	20888.820564	29.422221
382.352149	20938.518867	29.427239
382.561175	20979.820148	29.432256
383.205147	21003.419344	29.437274
383.819433	21049.903842	29.442292
384.475905	21088.839110	29.447309
385.163353	21125.679815	29.452327
385.363053	21150.853374	29.457344
385.896268	21180.711460	29.462362
386.142631	21214.929926	29.467380
386.566780	21242.867259	29.472397
386.403850	21266.795906	29.477415
387.075798	21297.030948	29.482432
387.395974	21320.455851	29.487450
388.006879	21361.358041	29.492468
388.564903	21382.304403	29.497485
388.838910	21405.388843	29.502503
388.902301	21436.933169	29.507520
389.386272	21455.269939	29.512538
389.956153	21488.843755	29.517556
390.845435	21511.034447	29.522573
391.276934	21536.823267	29.527591
391.720815	21563.549838	29.532608
392.420020	21577.499176	29.537626
392.782606	21602.178725	29.542644
392.848299	21609.419683	29.547661
393.348451	21628.718936	29.552679
393.123153	21650.894247	29.557696
393.797227	21670.422356	29.562714
394.552831	21706.864720	29.567732
394.390326	21727.575451	29.572749
394.917762	21750.222698	29.577767
394.956766	21780.928186	29.582784
395.823739	21813.100304	29.587802
395.640622	21848.065414	29.592820
396.056381	21878.826360	29.597837
396.460376	21907.555128	29.602855
396.591296	21950.005964	29.607872
397.209318	21983.861085	29.612890
397.464166	22027.028884	29.617908
397.706347	22054.479918	29.622925
397.545043	22104.594732	29.627943
397.878736	22143.923622	29.632960
398.603299	22183.387469	29.637978
398.541922	22239.515855	29.642996
398.777208	22284.463320	29.648013
399.762838	22332.578193	29.653031
400.521230	22374.127754	29.658048
400.901938	22417.338047	29.663066
401.112943	22456.001115	29.668084
401.438144	22505.005530	29.673101
401.917977	22545.843135	29.678119
402.312242	22591.098483	29.683136
402.982475	22624.192122	29.688154
403.459533	22671.483597	29.693172
403.734693	22711.278000	29.698189
404.359749	22749.091729	29.703207
405.164588	22780.834758	29.708224
405.627202	22812.548180	29.713242
405.681935	22833.200939	29.718260
406.245883	22862.399086	29.723277
406.597966	22903.038652	29.728295
407.106551	22946.140052	29.733312
407.719341	22971.169805	29.738330
408.430405	23008.092537	29.743348
409.049713	23022.772731	29.748365
409.760765	23046.590360	29.753383
409.978806	23070.126636	29.758400
410.472508	23077.498307	29.763418
410.554797	23101.726556	29.768436
410.538739	23118.013909	29.773453
410.723089	23131.100219	29.778471
411.036636	23156.954280	29.783488
411.810965	23175.238412	29.788506
411.945900	23211.307774	29.793524
412.255665	23246.738506	29.798541
412.607397	23268.712934	29.803559
412.952800	23302.040181	29.808576
413.350832	23330.258238	29.813594
413.893123	23368.607953	29.818612
413.969372	23395.424047	29.823629
414.316285	23435.434932	29.828647
414.493776	23478.780504	29.833664
415.126999	23511.970519	29.838682
415.468241	23555.773965	29.843700
415.318346	23603.635960	29.848717
415.905036	23628.538671	29.853735
416.490109	23690.967177	29.858752
416.844572	23737.967180	29.863770
417.231794	23790.427958	29.868788
417.360618	23837.687696	29.873805
417.677224	23885.032090	29.878823
418.202471	23943.462729	29.883840
418.460579	23981.745803	29.888858
418.975788	24039.853601	29.893876
419.250538	24096.968200	29.898893
419.837504	24145.658013	29.903911
420.089193	24207.445269	29.908928
420.942694	24248.062019	29.913946
421.226673	24301.289612	29.918964
421.892655	24360.962427	29.923981
422.118773	24405.122118	29.928999
422.719710	24451.719080	29.934016
423.591460	24489.052759	29.939034
424.791091	24524.677450	29.944052
425.069241	24559.999589	29.949069
426.189192	24581.828276	29.954087
426.103072	24612.172274	29.959104
426.461005	24634.087450	29.964122
426.931744	24672.963340	29.969140
427.082741	24699.935834	29.974157
427.561522	24729.031883	29.979175
427.522005	24766.128024	29.984192
427.917480	24799.077367	29.989210
428.979529	24834.666344	29.994228
429.123340	24882.459466	29.999245
430.034597	24905.633411	30.004263
429.868174	24936.878132	30.009280
430.532123	24974.380959	30.014298
430.695595	25016.732838	30.019316
430.860510	25052.734667	30.024333
431.409228	25085.122039	30.029351
431.524504	25135.469548	30.034368
432.099065	25170.029230	30.039386
432.416872	25205.349046	30.044404
432.729198	25246.893669	30.049421
433.101237	25278.532522	30.054439
433.175736	25324.193686	30.059456
433.723360	25364.657285	30.064474
434.252707	25416.638086	30.069492
434.833750	25463.815308	30.074509
435.134685	25505.807291	30.079527
435.360797	25564.903496	30.084544
435.760458	25600.670653	30.089562
436.550635	25648.459221	30.094580
436.882843	25701.859509	30.099597
437.609005	25739.649862	30.104615
437.829078	25785.956063	30.109632
437.963198	25831.788155	30.114650
438.727000	25876.146522	30.119668
438.028996	25929.686195	30.124685
438.965056	25972.381202	30.129703
439.791253	26022.003767	30.134720
440.188165	26072.204780	30.139738
440.986296	26125.756816	30.144756
441.795153	26161.940823	30.149773
443.170991	26184.200892	30.154791
444.010337	26211.048314	30.159808
444.778834	26229.434494	30.164826
445.503571	26245.730340	30.169844
445.774702	26253.299256	30.174861
446.718839	26259.793829	30.179879
446.632677	26287.948266	30.184896
447.086865	26296.886507	30.189914
447.644064	26306.895464	30.194932
447.545941	26321.934867	30.199949
447.973161	26331.051255	30.204967
448.392105	26360.396899	30.209984
448.447621	26387.738548	30.215002
448.882728	26418.387563	30.220020
448.651466	26451.573633	30.225037
449.132854	26482.265305	30.230055
449.341877	26520.830549	30.235072
449.754416	26562.288586	30.240090
450.272671	26601.201668	30.245108
450.542119	26647.375511	30.250125
450.687060	26690.447613	30.255143
451.098993	26747.086835	30.260160
451.549705	26789.826012	30.265178
452.043974	26834.974384	30.270196
452.384777	26886.616471	30.275213
452.980162	26939.877660	30.280231
453.108411	27005.680525	30.285248
453.552391	27046.134251	30.290266
454.092424	27082.186416	30.295284
455.343669	27118.924417	30.300301
455.629132	27161.831634	30.305319
455.939217	27207.324860	30.310336
456.435437	27250.177249	30.315354
457.098466	27290.682342	30.320372
457.444961	27332.756103	30.325389
457.724474	27355.208705	30.330407
458.614953	27392.965030	30.335424
459.238436	27431.243576	30.340442
459.919313	27464.748494	30.345460
460.336988	27491.417762	30.350477
460.650683	27525.206558	30.355495
460.726024	27564.812890	30.360512
460.593581	27597.558285	30.365530
461.269632	27641.106446	30.370548
461.546400	27682.628266	30.375565
462.323889	27719.874633	30.380583
462.679879	27769.207314	30.385600
462.912736	27820.712908	30.390618
463.725799	27853.893046	30.395636
463.911588	27904.463620	30.400653
464.538858	27948.569869	30.405671
465.022780	27999.685919	30.410688
465.410100	28048.979313	30.415706
465.777776	28083.820013	30.420724
466.216380	28136.477555	30.425741
466.573029	28188.991549	30.430759
467.023718	28240.644038	30.435776
467.498733	28291.008413	30.440794
467.822922	28328.624014	30.445812
468.422933	28383.617765	30.450829
469.488332	28422.059380	30.455847
470.177978	28462.209256	30.460864
470.809648	28511.383200	30.465882
471.727382	28542.559012	30.470900
471.825167	28590.143004	30.475917
472.307867	28619.913764	30.480935
472.721379	28659.508786	30.485952
473.118493	28688.865235	30.490970
474.025742	28719.125022	30.495988
474.371182	28751.800141	30.501005
475.208376	28791.603667	30.506023
474.806597	28826.915288	30.511040
475.281849	28870.065502	30.516058
475.927012	28907.557928	30.521076
476.099894	28950.151208	30.526093
476.189056	28997.829277	30.531111
476.730528	29034.860158	30.536128
476.948467	29088.173620	30.541146
477.240172	29140.912979	30.546164
477.383015	29202.266446	30.551181
478.255098	29261.971202	30.556199
478.795428	29324.295045	30.561216
478.863361	29380.108783	30.566234
479.620804	29434.397309	30.571252
479.869444	29500.804152	30.576269
480.482131	29540.505854	30.581287
481.580697	29578.644570	30.586304
482.157890	29627.111563	30.591322
482.626145	29664.875716	30.596340
483.257615	29712.986564	30.601357
483.532718	29746.035280	30.606375
484.038644	29789.696799	30.611392
484.440828	29837.209903	30.616410
485.110299	29873.737850	30.621428
485.851794	29909.294313	30.626445
486.549328	29944.489207	30.631463
486.973259	29981.015276	30.636480
487.412439	30018.630555	30.641498
487.903045	30059.565995	30.646516
488.632226	30099.378363	30.651533
489.162105	30137.215004	30.656551
489.684154	30163.365583	30.661568
490.132713	30195.113803	30.666586
490.712498	30215.666400	30.671604
490.948070	30267.292267	30.676621
491.727790	30288.555362	30.681639
492.231235	30314.223421	30.686656
492.372523	30361.132626	30.691674
493.011457	30394.145453	30.696692
493.426784	30439.086263	30.701709
493.620725	30479.606507	30.706727
493.768210	30517.610459	30.711744
493.855009	30569.048126	30.716762
494.207993	30620.323580	30.721780
494.583986	30685.608632	30.726797
495.224286	30740.120034	30.731815
495.778344	30794.072083	30.736832
496.013286	30853.714682	30.741850
496.657854	30901.608786	30.746868
496.855162	30967.319928	30.751885
497.178557	31036.035853	30.756903
498.101002	31096.353497	30.761920
498.194635	31165.002000	30.766938
498.675212	31218.459885	30.771956
499.413098	31279.289417	30.776973
500.289794	31338.918343	30.781991
501.280100	31379.607114	30.787008
501.732643	31437.096984	30.792026
502.338317	31480.821307	30.797044
502.952039	31529.501821	30.802061
503.064284	31583.898020	30.807079
503.593416	31631.432038	30.812096
504.005261	31701.561716	30.817114
504.792202	31749.316948	30.822132
505.020691	31806.420386	30.827149
505.335067	31863.190567	30.832167
505.932832	31912.831029	30.837184
506.295878	31967.971186	30.842202
506.955761	32021.889886	30.847220
507.259138	32084.434425	30.852237
507.986390	32129.228225	30.857255
509.183475	32174.459171	30.862272
509.645115	32217.559901	30.867290
510.014715	32258.618964	30.872308
510.484555	32304.041121	30.877325
510.696647	32342.735311	30.882343
511.472090	32391.134848	30.887360
511.397276	32437.310222	30.892378
512.033239	32478.466159	30.897396
512.407491	32532.195502	30.902413
512.804503	32589.259939	30.907431
513.261565	32645.724132	30.912448
513.620894	32701.716097	30.917466
514.468509	32742.227302	30.922484
515.061149	32800.164611	30.927501
515.696395	32848.037135	30.932519
516.373048	32890.869112	30.937536
516.866186	32952.784555	30.942554
517.358290	33001.685581	30.947572
517.564589	33060.870225	30.952589
518.131928	33109.083293	30.957607
518.234729	33163.706817	30.962624
518.764931	33231.013453	30.967642
519.338967	33288.157079	30.972660
519.883246	33349.364512	30.977677
520.450503	33408.131829	30.982695
520.979122	33466.789189	30.987712
521.680439	33529.658761	30.992730
522.033948	33593.377141	30.997748
522.648559	33660.219616	31.002765
523.217372	33720.489935	31.007783
523.948911	33771.879981	31.012800
524.406912	33835.625497	31.017818
524.846804	33892.355341	31.022836
525.006736	33953.378200	31.027853
525.079528	34023.508768	31.032871
526.059878	34080.156066	31.037888
526.428509	34151.429429	31.042906
526.958018	34222.713381	31.047924
527.618380	34298.475786	31.052941
528.047883	34366.473008	31.057959
528.674013	34423.109486	31.062976
529.063444	34499.900710	31.067994
529.540072	34561.411055	31.073012
530.678122	34617.319731	31.078029
531.219656	34680.343782	31.083047
532.220322	34731.428487	31.088064
532.618831	34791.753656	31.093082
533.518319	34841.650348	31.098100
534.078735	34879.766377	31.103117
534.476110	34945.823908	31.108135
535.341774	34986.722136	31.113152
535.664315	35046.284740	31.118170
535.729903	35089.517020	31.123188
536.846414	35144.951273	31.128205
537.078845	35193.915359	31.133223
537.225789	35242.423942	31.138240
537.832438	35289.847038	31.143258
538.676898	35326.996866	31.148276
539.770449	35371.890638	31.153293
540.221911	35419.331195	31.158311
540.612181	35454.185575	31.163328
540.831916	35498.995817	31.168346
541.386627	35539.702382	31.173364
541.890922	35588.523105	31.178381
541.996703	35645.713387	31.183399
542.892977	35681.646191	31.188416
543.618360	35728.554546	31.193434
544.347007	35775.172078	31.198452
545.024458	35818.822055	31.203469
545.196830	35876.661333	31.208487
545.889909	35907.377201	31.213504
546.397094	35959.452649	31.218522
546.940854	36013.415815	31.223540
547.391378	36061.587336	31.228557
547.382162	36105.330403	31.233575
548.307889	36161.756847	31.238592
548.279146	36222.743912	31.243610
549.029019	36275.381560	31.248628
549.534191	36334.288960	31.253645
549.741526	36401.514351	31.258663
550.586912	36455.708072	31.263680
551.166775	36519.028643	31.268698
551.676688	36579.179676	31.273716
552.844214	36628.653423	31.278733
553.650846	36690.136529	31.283751
553.777434	36737.857141	31.288768
553.966906	36797.132622	31.293786
554.358211	36863.731608	31.298804
554.747356	36927.834374	31.303821
555.186548	36996.095452	31.308839
556.033568	37054.911883	31.313856
557.042400	37107.482310	31.318874
557.696458	37157.004433	31.323892
558.417655	37215.167428	31.328909
558.994676	37273.459478	31.333927
559.520038	37323.708027	31.338944
559.736172	37386.920310	31.343962
560.432856	37451.862388	31.348980
560.807409	37501.550128	31.353997
561.344691	37570.295291	31.359015
562.077867	37619.871400	31.364032
562.447844	37682.670073	31.369050
562.975437	37753.358941	31.374068
563.316670	37808.015542	31.379085
563.772158	37878.474180	31.384103
564.214518	37940.854117	31.389120
564.580967	38020.388359	31.394138
565.214461	38086.287373	31.399156
565.963816	38151.292350	31.404173
565.914430	38231.776332	31.409191
566.828565	38295.591893	31.414208
567.471904	38358.450210	31.419226
567.647615	38429.388217	31.424244
568.185124	38503.355036	31.429261
568.692069	38563.361557	31.434279
569.719658	38619.696053	31.439296
570.538011	38685.994873	31.444314
571.242667	38749.993116	31.449332
571.580059	38807.532403	31.454349
572.299703	38868.466321	31.459367
573.229967	38927.858516	31.464384
573.923889	38980.485111	31.469402
574.664419	39042.413608	31.474420
575.799091	39097.992503	31.479437
576.653072	39134.965350	31.484455
577.196710	39184.224575	31.489472
577.815802	39225.692288	31.494490
578.035396	39269.037476	31.499508
578.805365	39306.669079	31.504525
578.789082	39360.002475	31.509543
579.639413	39414.232505	31.514560
579.786596	39465.173620	31.519578
579.910497	39529.507685	31.524596
580.735838	39587.382523	31.529613
580.874644	39648.854200	31.534631
581.547092	39716.431897	31.539648
582.318357	39782.026075	31.544666
582.670554	39829.596075	31.549684
583.510745	39889.922341	31.554701
583.890407	39969.952057	31.559719
584.391615	40023.015586	31.564736
584.979197	40097.437981	31.569754
585.175955	40178.364976	31.574772
586.151103	40247.300817	31.579789
586.206867	40324.299890	31.584807
586.801652	40395.435670	31.589824
587.791161	40473.809755	31.594842
588.103766	40551.166721	31.599860
588.528537	40616.655883	31.604877
589.380856	40702.183354	31.609895
590.095717	40776.820294	31.614912
590.694523	40842.046798	31.619930
591.194049	40923.266136	31.624948
592.197927	40993.058588	31.629965
592.914152	41050.337863	31.634983
593.905891	41114.329815	31.640000
594.545559	41176.266932	31.645018
594.957719	41239.326183	31.650036
595.315690	41300.639474	31.655053
595.817617	41372.230600	31.660071
596.564108	41433.139929	31.665088
597.115203	41501.508975	31.670106
597.436325	41573.447583	31.675124
598.385389	41644.581107	31.680141
599.340898	41702.591783	31.685159
599.941803	41767.094967	31.690176
600.468370	41816.288316	31.695194
600.529307	41879.210984	31.700212
601.221315	41924.416900	31.705229
601.105529	41999.365226	31.710247
601.748019	42064.446431	31.715264
602.355918	42134.803553	31.720282
602.638650	42217.625431	31.725300
603.274107	42279.503774	31.730317
604.339470	42355.264703	31.735335
604.935488	42432.334612	31.740352
605.301353	42507.859203	31.745370
605.590476	42579.324054	31.750388
606.295454	42648.125602	31.755405
606.800186	42730.033912	31.760423
607.525862	42804.923379	31.765440
608.546869	42882.913795	31.770458
608.861572	42970.548798	31.775476
609.136748	43047.202558	31.780493
609.750303	43134.610297	31.785511
610.484986	43212.790070	31.790528
611.076507	43293.984972	31.795546
611.440770	43389.198063	31.800564
612.126816	43472.373173	31.805581
612.863421	43563.854150	31.810599
613.500346	43644.578603	31.815616
614.301097	43721.378727	31.820634
615.149297	43811.919738	31.825652
615.642066	43893.478328	31.830669
616.143067	43969.383495	31.835687
616.565094	44060.718677	31.840704
617.590237	44135.258976	31.845722
618.559709	44216.386774	31.850740
619.701699	44279.713276	31.855757
620.484861	44347.932911	31.860775
620.887904	44414.572692	31.865792
621.466787	44487.716134	31.870810
622.320222	44559.641260	31.875828
622.671521	44625.150664	31.880845
623.331151	44698.795817	31.885863
624.021249	44769.739206	31.890880
624.619090	44843.843926	31.895898
625.338572	44910.765972	31.900916
625.985941	44969.891092	31.905933
626.958084	45037.108194	31.910951
627.792505	45107.096532	31.915968
628.267638	45159.553773	31.920986
628.928408	45226.616467	31.926004
629.453217	45280.306606	31.931021
629.999331	45344.215605	31.936039
630.294773	45406.503506	31.941056
631.202111	45466.507764	31.946074
632.045895	45548.003854	31.951092
632.954228	45602.668181	31.956109
633.330910	45656.296334	31.961127
634.421252	45704.541089	31.966144
634.946329	45748.549975	31.971162
635.297968	45804.608210	31.976180
635.789079	45856.385653	31.981197
636.290868	45913.716447	31.986215
636.729397	45966.665366	31.991232
637.183938	46024.222494	31.996250
637.853004	46090.320433	32.001268
638.418726	46160.327095	32.006285
638.526717	46224.159354	32.011303
638.923529	46301.275974	32.016320
639.614978	46364.904527	32.021338
640.198636	46454.897086	32.026356
640.856724	46535.481759	32.031373
641.493545	46607.158021	32.036391
641.609224	46700.402722	32.041408
642.370109	46776.719864	32.046426
642.940031	46854.904954	32.051444
644.010233	46941.942463	32.056461
644.760548	47024.430441	32.061479
645.083788	47109.840693	32.066496
646.323070	47181.289559	32.071514
647.271172	47256.092145	32.076532
648.061003	47330.615783	32.081549
648.969348	47385.961087	32.086567
650.156245	47451.902370	32.091584
651.052314	47506.138395	32.096602
651.811845	47558.193445	32.101620
652.785631	47610.249831	32.106637
653.332824	47661.340341	32.111655
654.018354	47714.946613	32.116672
654.286074	47770.071146	32.121690
654.764704	47836.359331	32.126708
655.033866	47897.560713	32.131725
655.410605	47958.964947	32.136743
656.034416	48020.371268	32.141760
656.632759	48092.378664	32.146778
656.917376	48176.363179	32.151796
657.517378	48259.415980	32.156813
658.479577	48324.830228	32.161831
658.631750	48405.231462	32.166848
659.326364	48476.949011	32.171866
659.689885	48563.448481	32.176884
660.469564	48645.347731	32.181901
661.183129	48739.930678	32.186919
661.265731	48829.511652	32.191936
662.169142	48919.072449	32.196954
662.469515	49019.621421	32.201972
663.219465	49110.978197	32.206989
663.914260	49202.742837	32.212007
664.143606	49295.907952	32.217024
665.084686	49377.422563	32.222042
666.199988	49476.476079	32.227060
666.921869	49563.392413	32.232077
667.768775	49650.477238	32.237095
668.278728	49742.996274	32.242112
669.283338	49816.112352	32.247130
669.413758	49899.979125	32.252148
670.186467	49984.254260	32.257165
670.925283	50060.537619	32.262183
671.057263	50150.545805	32.267200
671.602513	50242.454684	32.272218
672.545072	50334.308566	32.277236
672.981337	50416.191983	32.282253
673.735801	50509.689904	32.287271
674.345924	50607.749086	32.292288
675.264739	50699.431859	32.297306
675.802839	50785.595414	32.302324
677.170902	50860.314708	32.307341
678.535277	50926.600693	32.312359
679.212709	51012.374948	32.317376
679.675493	51087.553450	32.322394
680.515459	51164.645111	32.327412
681.038533	51256.360384	32.332429
681.976257	51320.977063	32.337447
682.458338	51400.215868	32.342464
683.159802	51477.837922	32.347482
683.564523	51565.291345	32.352500
684.038588	51642.807694	32.357517
685.010050	51721.945007	32.362535
685.703789	51812.332127	32.367552
686.225741	51879.384825	32.372570
687.010263	51971.475641	32.377588
687.866392	52047.961467	32.382605
688.573366	52132.111793	32.387623
688.917509	52219.932320	32.392640
689.642691	52294.470262	32.397658
690.499605	52384.787830	32.402676
690.739140	52478.869852	32.407693
691.612244	52561.590897	32.412711
692.060522	52664.180381	32.417728
692.630300	52752.893420	32.422746
693.239930	52844.594946	32.427764
693.891703	52938.545352	32.432781
694.487582	53030.395419	32.437799
695.447779	53130.068961	32.442816
696.239214	53225.153085	32.447834
697.485092	53319.540600	32.452852
697.611672	53418.499076	32.457869
698.489427	53499.687839	32.462887
698.802579	53604.339929	32.467904
699.864178	53690.312775	32.472922
700.464170	53785.192272	32.477940
701.522665	53879.254388	32.482957
702.174425	53961.406287	32.487975
703.073032	54052.432024	32.492992
703.857625	54139.332577	32.498010
704.409934	54220.889662	32.503028
704.901509	54301.256903	32.508045
706.080130	54391.522195	32.513063
706.678303	54475.157695	32.518080
707.032080	54559.517856	32.523098
707.695663	54631.572846	32.528116
708.102204	54718.780810	32.533133
709.334175	54792.988575	32.538151
709.749802	54876.783410	32.543168
710.668481	54950.299783	32.548186
711.047183	55038.385941	32.553204
711.375434	55125.899771	32.558221
712.571239	55214.029985	32.563239
712.929295	55313.590131	32.568256
713.507677	55407.678517	32.573274
714.412335	55500.466565	32.578292
714.804289	55604.749135	32.583309
715.473693	55697.559437	32.588327
716.136432	55802.074695	32.593344
717.113048	55889.190103	32.598362
717.683165	55986.037856	32.603380
718.214307	56099.102051	32.608397
719.326519	56193.146911	32.613415
719.833900	56303.391532	32.618432
720.391264	56391.579416	32.623450
721.495145	56494.259563	32.628468
722.335088	56596.682108	32.633485
723.029135	56698.896341	32.638503
723.552494	56798.189060	32.643520
724.686125	56891.930175	32.648538
725.620171	57000.222261	32.653556
725.858552	57097.915830	32.658573
727.159647	57185.297255	32.663591
727.702367	57277.422411	32.668608
728.320556	57378.035211	32.673626
728.971481	57477.031343	32.678644
729.662889	57582.088110	32.683661
730.709800	57669.211816	32.688679
731.247352	57771.433002	32.693696
731.835510	57876.009704	32.698714
732.642548	57971.891046	32.703732
732.983772	58068.870159	32.708749
734.002604	58169.367699	32.713767
734.980939	58268.008245	32.718784
735.598597	58374.206725	32.723802
736.369047	58476.530608	32.728820
737.048019	58572.721131	32.733837
738.036000	58673.144285	32.738855
738.870384	58775.300714	32.743872
738.981312	58868.682624	32.748890
740.086321	58967.045730	32.753908
741.021733	59068.516370	32.758925
741.789947	59161.913438	32.763943
742.274468	59260.940443	32.768960
743.126110	59360.012488	32.773978
744.345556	59447.272273	32.778996
744.802078	59541.874793	32.784013
745.712747	59638.593178	32.789031
746.624779	59736.221945	32.794048
746.986663	59815.432448	32.799066
748.016771	59897.619567	32.804084
748.617465	59985.550172	32.809101
749.023198	60066.694567	32.814119
749.952497	60158.652768	32.819136
750.555313	60254.775766	32.824154
750.910127	60345.916709	32.829172
751.806909	60449.606753	32.834189
752.085586	60550.432422	32.839207
752.858392	60650.598748	32.844224
753.419153	60749.474503	32.849242
754.764387	60844.550241	32.854260
755.407331	60952.040908	32.859277
755.903701	61050.113737	32.864295
756.673042	61156.041504	32.869312
757.113120	61271.444534	32.874330
758.026692	61382.171695	32.879348
758.746228	61496.491460	32.884365
759.355364	61604.598140	32.889383
759.974266	61723.993299	32.894400
760.553797	61848.155750	32.899418
761.804510	61963.278396	32.904436
762.150976	62076.179778	32.909453
762.900555	62192.356691	32.914471
763.917021	62315.998289	32.919488
764.508991	62439.795514	32.924506
765.422911	62561.939011	32.929524
766.061985	62688.125463	32.934541
766.688284	62806.868154	32.939559
767.433734	62931.343700	32.944576
768.321432	63051.756146	32.949594
769.500599	63164.552410	32.954612
770.076716	63295.070973	32.959629
770.903757	63413.757449	32.964647
771.989079	63525.604526	32.969664
772.847641	63643.496697	32.974682
773.648592	63751.739728	32.979700
774.443064	63875.984928	32.984717
775.288035	63982.950932	32.989735
776.800654	64096.441093	32.994752
777.623847	64200.870546	32.999770
778.480741	64303.360234	33.004788
779.017329	64406.828295	33.009805
779.969322	64495.255215	33.014823
780.498987	64607.456132	33.019840
780.808374	64721.794304	33.024858
782.007013	64831.877736	33.029876
782.262504	64938.715666	33.034893
783.255071	65046.837728	33.039911
784.326377	65154.611783	33.044928
785.235341	65270.241116	33.049946
785.986690	65374.201894	33.054964
786.395277	65492.194167	33.059981
787.213864	65601.834617	33.064999
787.859913	65700.984781	33.070016
788.707606	65809.236726	33.075034
789.418446	65920.907809	33.080052
790.191471	66026.891262	33.085069
790.878953	66118.101604	33.090087
791.874900	66226.323967	33.095104
792.449075	66341.219868	33.100122
793.275643	66448.852770	33.105140
793.836619	66555.020605	33.110157
794.800807	66666.525770	33.115175
795.922017	66775.861236	33.120192
796.662910	66883.947284	33.125210
797.268040	66975.567426	33.130228
798.617833	67082.127570	33.135245
799.569683	67166.860558	33.140263
800.649857	67265.621216	33.145280
801.307175	67368.975602	33.150298
802.523031	67459.873582	33.155316
802.905063	67561.745917	33.160333
803.363590	67669.163502	33.165351
804.395584	67767.359350	33.170368
804.908594	67878.442304	33.175386
805.967250	67982.331603	33.180404
806.399035	68100.340701	33.185421
807.263087	68205.073767	33.190439
808.191156	68314.039204	33.195456
808.280850	68431.836827	33.200474
809.542920	68544.223969	33.205492
809.955900	68668.670113	33.210509
810.419298	68781.745419	33.215527
811.230490	68913.383892	33.220544
812.139957	69043.507704	33.225562
812.779718	69163.586374	33.230580
813.348982	69289.982239	33.235597
814.446775	69416.781548	33.240615
815.336490	69534.157296	33.245632
816.400903	69663.790377	33.250650
817.306762	69776.871003	33.255668
818.388594	69902.449130	33.260685
819.232283	70013.575004	33.265703
820.466822	70135.783130	33.270720
821.169513	70261.074154	33.275738
822.301633	70359.467053	33.280756
823.433814	70466.049664	33.285773
824.342713	70575.149971	33.290791
825.154143	70682.458907	33.295808
825.711990	70789.059267	33.300826
826.305330	70899.764599	33.305844
827.507583	71002.979861	33.310861
828.298313	71121.930532	33.315879
829.139105	71219.947203	33.320896
829.736691	71345.275132	33.325914
830.747227	71446.545918	33.330932
831.392597	71564.189526	33.335949
831.838436	71671.622874	33.340967
832.695856	71762.619372	33.345984
832.935826	71884.938118	33.351002
833.910437	71991.542544	33.356020
834.735893	72112.200203	33.361037
835.845834	72217.454462	33.366055
836.866919	72319.100620	33.371072
837.218092	72433.510657	33.376090
838.206662	72540.279799	33.381108
838.637528	72660.476814	33.386125
839.710019	72776.029974	33.391143
840.273141	72892.063100	33.396160
841.129328	73019.120848	33.401178
841.859656	73144.196007	33.406196
842.854377	73264.894259	33.411213
844.047984	73383.408743	33.416231
844.705111	73497.620123	33.421248
845.596124	73621.728101	33.426266
846.711548	73739.827815	33.431284
847.551478	73855.040664	33.436301
848.347357	73977.351734	33.441319
849.989709	74087.640508	33.446336
850.495782	74191.654134	33.451354
851.909503	74301.369624	33.456372
852.699309	74404.412224	33.461389
853.393171	74522.676871	33.466407
853.990145	74632.704662	33.471424
854.910408	74760.109325	33.476442
855.459142	74872.739818	33.481460
856.608164	74987.254140	33.486477
857.031970	75115.663005	33.491495
858.028717	75229.989604	33.496512
858.708194	75357.963919	33.501530
859.829994	75478.911810	33.506548
860.820945	75589.762387	33.511565
861.342764	75707.474551	33.516583
861.910010	75822.364796	33.521600
862.925862	75949.064106	33.526618
864.133636	76064.978131	33.531636
865.139197	76188.100400	33.536653
865.836574	76311.326732	33.541671
866.926529	76417.970695	33.546688
868.492765	76540.935625	33.551706
868.938929	76663.068325	33.556724
870.038051	76773.039642	33.561741
870.338852	76894.521660	33.566759
871.093130	77003.680234	33.571776
871.951325	77125.232501	33.576794
872.766439	77248.627257	33.581812
873.436706	77367.132398	33.586829
873.943456	77503.409961	33.591847
875.165406	77622.789805	33.596864
875.731415	77754.491501	33.601882
876.815842	77887.364028	33.606900
877.636595	78024.419647	33.611917
877.888013	78160.283109	33.616935
878.779641	78288.895688	33.621952
879.525911	78421.095448	33.626970
880.391538	78552.902299	33.631988
881.236075	78678.766989	33.637005
881.751242	78811.008600	33.642023
882.773291	78950.603755	33.647040
883.868859	79097.753334	33.652058
884.777268	79225.489000	33.657076
886.374733	79342.687973	33.662093
887.401973	79470.290788	33.667111
888.356634	79584.115289	33.672128
889.207112	79712.610117	33.677146
890.002619	79842.405674	33.682164
890.782185	79980.138083	33.687181
891.066721	80115.254684	33.692199
892.492925	80242.110221	33.697216
893.217662	80367.448014	33.702234
893.406996	80512.857617	33.707252
894.744688	80653.870574	33.712269
895.372395	80803.281302	33.717287
896.079337	80949.016252	33.722304
896.718254	81102.495091	33.727322
897.335352	81257.231399	33.732340
898.601022	81408.555049	33.737357
899.164391	81567.288559	33.742375
900.194383	81711.093910	33.747392
901.233087	81872.550945	33.752410
901.593726	82043.470256	33.757428
902.919764	82193.656171	33.762445
903.842220	82359.559135	33.767463
904.685280	82517.099720	33.772480
905.867788	82669.464533	33.777498
906.577872	82832.446115	33.782516
907.877338	82997.498162	33.787533
908.450160	83160.119581	33.792551
909.731243	83312.408449	33.797568
910.745183	83459.922572	33.802586
912.130358	83612.676459	33.807604
913.057486	83751.829742	33.812621
914.167559	83913.320360	33.817639
914.984253	84052.747447	33.822656
915.785917	84203.225953	33.827674
916.961960	84350.338273	33.832692
917.633973	84500.562474	33.837709
918.396834	84656.441730	33.842727
919.216431	84800.662860	33.847744
920.410135	84953.426638	33.852762
921.091591	85111.860306	33.857780
921.953487	85268.403733	33.862797
922.456963	85426.218217	33.867815
923.479344	85585.735710	33.872832
924.818892	85743.858420	33.877850
925.299275	85904.306181	33.882868
926.648700	86061.625657	33.887885
927.434793	86217.802333	33.892903
928.560862	86358.835394	33.897920
929.664841	86495.917931	33.902938
930.532556	86633.199928	33.907956
931.823542	86764.259119	33.912973
932.890609	86906.134541	33.917991
934.187585	87045.338830	33.923008
934.751365	87179.733332	33.928026
935.470138	87314.424799	33.933044
936.600365	87446.597439	33.938061
937.212091	87596.244050	33.943079
938.072375	87732.641325	33.948096
939.101552	87856.157082	33.953114
940.123378	87997.648032	33.958132
941.000662	88132.494158	33.963149
941.972206	88275.318048	33.968167
943.117230	88414.948710	33.973184
943.983884	88557.570734	33.978202
944.750671	88705.140852	33.983220
945.584380	88858.731811	33.988237
946.278934	88999.430307	33.993255
947.077705	89161.142814	33.998272
947.902511	89321.415267	34.003290
948.765461	89471.460889	34.008308
950.282214	89625.262530	34.013325
951.517452	89773.233629	34.018343
952.335381	89922.834063	34.023360
953.525945	90065.770280	34.028378
954.313456	90225.561424	34.033396
955.375745	90366.521347	34.038413
956.137701	90525.318815	34.043431
957.165407	90673.906907	34.048448
958.123795	90829.913134	34.053466
958.873717	90989.975233	34.058484
959.676539	91143.003632	34.063501
960.242516	91310.257936	34.068519
960.581274	91473.653299	34.073536
961.686741	91654.432398	34.078554
962.763219	91811.817171	34.083572
964.463634	91975.033330	34.088589
965.370655	92149.526726	34.093607
966.330127	92316.347046	34.098624
967.425863	92478.549732	34.103642
968.290370	92649.711821	34.108660
969.166283	92806.333411	34.113677
969.872083	92966.643818	34.118695
971.178690	93142.113914	34.123712
971.898968	93313.045765	34.128730
972.309218	93488.735113	34.133748
973.556232	93663.573442	34.138765
974.582789	93845.502531	34.143783
975.095579	94021.121112	34.148800
976.415933	94192.063864	34.153818
976.840454	94381.348078	34.158836
978.055769	94559.958317	34.163853
978.964221	94737.717140	34.168871
980.234723	94910.078690	34.173888
981.160997	95077.087834	34.178906
981.670718	95259.001781	34.183924
982.835192	95418.679676	34.188941
983.781591	95601.546874	34.193959
984.655562	95776.641129	34.198976
985.957607	95948.573928	34.203994
986.881481	96130.644832	34.209012
987.438169	96315.040010	34.214029
988.113918	96497.960059	34.219047
989.151297	96685.668941	34.224064
990.248092	96875.135363	34.229082
991.091641	97064.602251	34.234100
992.325452	97263.101372	34.239117
993.035588	97452.138164	34.244135
993.950076	97650.872263	34.249152
995.249450	97829.548248	34.254170
995.923507	98028.712664	34.259188
996.963866	98231.962870	34.264205
997.904821	98427.881084	34.269223
998.974829	98628.261287	34.274240
1000.136201	98835.800877	34.279258
1001.143641	99038.265362	34.284276
1002.750742	99212.042090	34.289293
1004.721043	99399.313603	34.294311
1005.922412	99575.251669	34.299328
1007.114624	99746.234848	34.304346
1008.156836	99925.741931	34.309364
1009.146809	100095.400746	34.314381
1010.388716	100266.955047	34.319399
1011.040245	100436.471436	34.324416
1011.956718	100605.930901	34.329434
1013.145922	100786.406544	34.334452
1014.190643	100952.332121	34.339469
1015.169246	101122.803755	34.344487
1015.853832	101309.017533	34.349504
1016.750537	101488.743967	34.354522
1017.765445	101675.606654	34.359540
1018.520648	101855.271190	34.364557
1019.728067	102046.447402	34.369575
1020.812822	102228.704919	34.374592
1021.754596	102408.911203	34.379610
1022.601165	102597.544328	34.384628
1023.467961	102784.592254	34.389645
1024.464860	102976.229217	34.394663
1025.188382	103174.170838	34.399680
1026.510135	103364.767135	34.404698
1027.620878	103562.784678	34.409716
1028.440747	103763.310553	34.414733
1029.152142	103964.185815	34.419751
1029.794489	104169.051345	34.424768
1031.360939	104365.818972	34.429786
1032.285723	104571.753802	34.434804
1032.979232	104774.360760	34.439821
1033.837704	104974.521850	34.444839
1034.651321	105187.269305	34.449856
1035.890021	105380.769422	34.454874
1036.844734	105586.136975	34.459892
1037.663827	105783.904309	34.464909
1038.631819	105983.598202	34.469927
1039.766702	106199.123236	34.474944
1041.164759	106386.726139	34.479962
1042.396904	106599.083780	34.484980
1043.537619	106790.381510	34.489997
1044.961819	106984.127392	34.495015
1045.653954	107182.522053	34.500032
1046.830300	107378.555216	34.505050
1047.662878	107579.854782	34.510068
1048.863264	107784.424297	34.515085
1049.888890	107981.399643	34.520103
1050.654936	108187.427274	34.525120
1051.919643	108383.731224	34.530138
1052.491936	108605.110004	34.535156
1053.459329	108812.779972	34.540173
1054.784557	109026.635389	34.545191
1055.693376	109241.640530	34.550208
1056.712901	109450.788522	34.555226
1057.644005	109674.496032	34.560244
1058.703087	109896.485925	34.565261
1059.850569	110115.954173	34.570279
1060.876466	110334.748227	34.575296
1062.175292	110546.542357	34.580314
1063.206315	110771.584471	34.585332
1064.216977	111001.559957	34.590349
1065.506627	111210.700325	34.595367
1066.639336	111435.591040	34.600384
1068.117131	111633.693230	34.605402
1069.585981	111849.952928	34.610420
1070.674712	112063.897604	34.615437
1071.749769	112277.630879	34.620455
1072.873287	112494.892194	34.625472
1073.865735	112693.997163	34.630490
1075.425931	112884.986599	34.635508
1076.240208	113087.418897	34.640525
1077.966434	113283.450399	34.645543
1079.281523	113480.199809	34.650560
1081.011527	113655.923785	34.655578
1082.123763	113837.722111	34.660596
1083.848482	114014.627509	34.665613
1084.907439	114190.786443	34.670631
1085.641620	114374.490081	34.675648
1086.832658	114534.879646	34.680666
1088.666475	114705.410254	34.685684
1088.962918	114887.785751	34.690701
1089.995552	115049.206280	34.695719
1090.402722	115234.808640	34.700736
1091.780201	115417.040422	34.705754
1092.942168	115585.005154	34.710772
1094.091707	115770.445856	34.715789
1095.268193	115935.736637	34.720807
1095.887051	116118.052068	34.725824
1096.770588	116282.748784	34.730842
1097.927686	116456.662085	34.735860
1098.538043	116638.285348	34.740877
1099.494174	116818.862198	34.745895
1100.237992	117002.897752	34.750912
1101.335935	117201.103709	34.755930
1102.446209	117381.885751	34.760948
1103.298565	117569.682378	34.765965
1104.396866	117766.295516	34.770983
1105.002006	117975.450634	34.776000
1106.203630	118167.803783	34.781018
1107.508796	118373.534569	34.786036
1108.006048	118582.687148	34.791053
1109.545428	118785.605575	34.796071
1110.265246	119005.684327	34.801088
1111.342344	119214.399968	34.806106
1112.644374	119425.232858	34.811124
1113.592964	119649.104259	34.816141
1115.058833	119863.245050	34.821159
1116.290598	120070.774385	34.826176
1117.530542	120284.906211	34.831194
1118.820950	120501.730227	34.836212
1119.586102	120720.711419	34.841229
1120.943677	120935.119252	34.846247
1121.944995	121153.416862	34.851264
1122.895518	121368.543815	34.856282
1124.302581	121592.946954	34.861300
1125.249921	121811.271265	34.866317
1126.486335	122031.993628	34.871335
1127.188168	122264.139210	34.876352
1128.316586	122475.074042	34.881370
1129.577914	122713.704860	34.886388
1130.332102	122956.226511	34.891405
1131.898479	123177.306297	34.896423
1132.579141	123412.214519	34.901440
1133.882528	123642.594694	34.906458
1134.842249	123881.590490	34.911476
1135.756040	124125.602343	34.916493
1136.990886	124364.884339	34.921511
1138.487833	124606.290657	34.926528
1139.993508	124836.949370	34.931546
1141.233144	125063.117842	34.936564
1142.256013	125290.567207	34.941581
1144.045399	125504.375665	34.946599
1145.405834	125724.406365	34.951616
1146.820021	125945.342024	34.956634
1147.765179	126172.633721	34.961652
1148.947759	126388.542151	34.966669
1149.918140	126604.868664	34.971687
1151.248850	126830.362638	34.976704
1152.349608	127049.547212	34.981722
1153.668178	127267.327073	34.986740
1154.333322	127490.442668	34.991757
1155.727871	127706.171791	34.996775
1156.927613	127914.457030	35.001792
1158.109112	128120.211595	35.006810
1158.853373	128326.676154	35.011828
1160.569793	128536.765757	35.016845
1161.559925	128725.558465	35.021863
1162.748597	128934.600207	35.026880
1163.635111	129142.630247	35.031898
1165.682303	129333.907615	35.036916
1166.961383	129535.255956	35.041933
1168.615951	129721.342150	35.046951
1169.511042	129921.237482	35.051968
1170.462212	130117.245402	35.056986
1171.389021	130309.265516	35.062004
1172.388050	130509.729849	35.067021
1173.949781	130706.739719	35.072039
1174.597061	130920.590246	35.077056
1175.799310	131133.054117	35.082074
1177.055382	131333.593655	35.087092
1178.548718	131552.526497	35.092109
1179.811159	131759.380837	35.097127
1180.863631	131967.578212	35.102144
1181.627763	132176.764413	35.107162
1182.717960	132386.073618	35.112180
1183.444059	132619.432582	35.117197
1184.304331	132835.579240	35.122215
1185.393358	133073.544705	35.127232
1186.435173	133311.570687	35.132250
1187.539482	133543.464218	35.137268
1188.150833	133793.408621	35.142285
1189.192156	134034.546033	35.147303
1190.210369	134284.982333	35.152320
1191.521920	134542.901259	35.157338
1192.997486	134786.467432	35.162356
1194.194468	135046.451106	35.167373
1195.271721	135297.404732	35.172391
1196.617434	135556.314578	35.177408
1197.817822	135812.309806	35.182426
1199.605412	136056.516464	35.187444
1200.323015	136323.527487	35.192461
1201.436554	136582.015845	35.197479
1202.610109	136834.473263	35.202496
1203.765825	137086.415761	35.207514
1205.252070	137341.511439	35.212532
1206.420262	137596.270411	35.217549
1208.046502	137851.244502	35.222567
1209.992061	138103.934201	35.227584
1210.748957	138349.196010	35.232602
1212.270032	138587.215329	35.237620
1213.482001	138836.726554	35.242637
1214.897954	139080.523991	35.247655
1216.023517	139332.234562	35.252672
1216.682572	139574.224986	35.257690
1217.977532	139814.776799	35.262708
1219.296978	140068.019196	35.267725
1220.967041	140294.231944	35.272743
1222.239803	140521.718830	35.277760
1223.396868	140754.476803	35.282778
1224.830895	140985.058539	35.287796
1225.914807	141215.676363	35.292813
1227.043915	141441.405803	35.297831
1228.095260	141667.251447	35.302848
1229.903480	141887.592185	35.307866
1230.903338	142103.215789	35.312884
1232.308388	142333.266004	35.317901
1233.657615	142554.742006	35.322919
1234.600551	142779.383199	35.327936
1235.514297	143017.181507	35.332954
1236.894718	143247.292562	35.337972
1237.641744	143489.370872	35.342989
1239.423362	143733.290103	35.348007
1240.235642	143981.029291	35.353024
1241.477969	144205.970572	35.358042
1243.041705	144444.884515	35.363060
1243.952782	144689.808927	35.368077
1245.449425	144923.994415	35.373095
1246.841873	145162.384389	35.378112
1247.655632	145411.490093	35.383130
1249.417825	145651.379894	35.388148
1250.562885	145899.278106	35.393165
1251.787605	146147.570198	35.398183
1252.855535	146392.149419	35.403200
1254.078669	146642.854829	35.408218
1255.470136	146881.306868	35.413236
1256.561838	147138.607846	35.418253
1257.890714	147397.112942	35.423271
1259.202778	147643.459621	35.428288
1259.797998	147906.976835	35.433306
1261.096923	148171.326690	35.438324
1262.377177	148433.474700	35.443341
1263.800168	148695.080084	35.448359
1264.809429	148967.475700	35.453376
1265.496829	149246.422397	35.458394
1267.156997	149510.491507	35.463412
1268.352803	149785.765650	35.468429
1269.576321	150057.866063	35.473447
1271.039632	150341.647385	35.478464
1272.391356	150609.391853	35.483482
1273.977858	150873.318116	35.488500
1275.283122	151157.259371	35.493517
1276.605242	151421.285386	35.498535
1277.879668	151686.348808	35.503552
1279.340893	151960.375402	35.508570
1280.799503	152222.506202	35.513588
1281.719889	152500.802422	35.518605
1282.627524	152771.086015	35.523623
1284.277642	153049.248540	35.528640
1285.113534	153328.985815	35.533658
1286.234088	153607.623488	35.538676
1287.447514	153889.697594	35.543693
1288.549861	154173.860419	35.548711
1290.122268	154436.316318	35.553728
1291.307019	154708.189459	35.558746
1292.457774	154975.782570	35.563764
1293.441030	155249.457169	35.568781
1294.419190	155528.348319	35.573799
1295.790520	155804.624263	35.578816
1297.138010	156096.230692	35.583834
1298.319340	156372.390812	35.588852
1299.410896	156662.218347	35.593869
1300.533732	156958.106559	35.598887
1301.850354	157250.931740	35.603904
1303.265572	157560.082105	35.608922
1304.929938	157847.587206	35.613940
1306.496137	158142.773759	35.618957
1307.974593	158426.496086	35.623975
1309.272416	158714.019216	35.628992
1310.391875	159003.668181	35.634010
1311.814791	159288.129046	35.639028
1313.481316	159589.436452	35.644045
1314.624601	159873.644674	35.649063
1316.299622	160166.923890	35.654080
1317.561247	160442.666086	35.659098
1319.169216	160732.332172	35.664116
1320.629583	161020.629892	35.669133
1321.800880	161313.546525	35.674151
1323.688104	161593.617030	35.679168
1324.605286	161879.222269	35.684186
1326.045015	162160.971717	35.689204
1327.602768	162441.560908	35.694221
1329.027019	162714.384425	35.699239
1330.378151	162994.213232	35.704256
1331.791251	163281.481106	35.709274
1333.719307	163555.061080	35.714292
1334.940647	163831.758144	35.719309
1336.037406	164116.306939	35.724327
1337.353358	164384.414023	35.729344
1338.503503	164675.732871	35.734362
1339.973480	164941.634564	35.739380
1341.946753	165219.708876	35.744397
1343.175858	165491.593347	35.749415
1344.657680	165758.474921	35.754432
1345.769706	166032.400230	35.759450
1347.591628	166282.502858	35.764468
1349.317970	166551.555162	35.769485
1350.490497	166819.650671	35.774503
1352.134470	167080.091675	35.779520
1353.202785	167354.260885	35.784538
1354.605336	167610.000490	35.789556
1355.869552	167875.345646	35.794573
1357.067070	168146.020614	35.799591
1358.701285	168403.235032	35.804608
1359.372018	168674.295127	35.809626
1360.528295	168952.227617	35.814644
1361.612766	169232.635864	35.819661
1362.777090	169504.809156	35.824679
1363.880818	169768.479516	35.829696
1365.137811	170051.731057	35.834714
1366.406237	170326.759228	35.839732
1367.746878	170597.309738	35.844749
1368.716012	170879.498793	35.849767
1369.893506	171152.478834	35.854784
1371.424742	171433.077522	35.859802
1372.603925	171714.778725	35.864820
1374.147446	172003.741611	35.869837
1375.153112	172301.795871	35.874855
1376.509902	172599.487299	35.879872
1377.617498	172908.594057	35.884890
1378.937720	173210.394582	35.889908
1380.663617	173513.751968	35.894925
1382.176566	173806.804584	35.899943
1383.793792	174107.760280	35.904960
1385.243205	174412.756912	35.909978
1386.281434	174719.831001	35.914996
1387.975523	175027.086632	35.920013
1389.034876	175328.589411	35.925031
1390.740070	175627.990921	35.930048
1391.879080	175946.731368	35.935066
1392.975517	176260.226818	35.940084
1394.740906	176566.273961	35.945101
1396.525468	176871.380482	35.950119
1398.070512	177170.145863	35.955136
1399.316506	177487.887704	35.960154
1401.051800	177793.223910	35.965172
1402.598655	178097.375742	35.970189
1403.801142	178414.331135	35.975207
1405.007879	178718.900195	35.980224
1406.544920	179033.657120	35.985242
1407.730939	179349.834087	35.990260
1409.196751	179679.038211	35.995277
1409.879819	179997.577069	36.000295
1411.586127	180314.457686	36.005312
1413.035614	180638.365072	36.010330
1414.606795	180960.083140	36.015348
1416.050838	181284.109588	36.020365
1417.113266	181618.509872	36.025383
1418.538201	181942.099277	36.030400
1419.680844	182278.431903	36.035418
1421.132658	182614.675602	36.040436
1422.536206	182960.779497	36.045453
1423.300927	183308.606930	36.050471
1425.265106	183649.643435	36.055488
1426.684039	184009.345760	36.060506
1428.216167	184340.991161	36.065524
1430.104275	184685.766175	36.070541
1431.176265	185023.739557	36.075559
1432.491111	185358.829997	36.080576
1434.374157	185719.174606	36.085594
1436.066575	186050.472508	36.090612
1437.278049	186380.750251	36.095629
1439.124419	186711.987514	36.100647
1440.527757	187028.247334	36.105664
1442.065991	187336.907387	36.110682
1443.413139	187654.640026	36.115700
1445.506130	187946.337760	36.120717
1446.670801	188332.019546	36.125735
1448.268236	188643.113593	36.130752
1450.259125	188947.413855	36.135770
1451.496526	189246.474824	36.140788
1452.617079	189554.545039	36.145805
1453.740981	189872.302266	36.150823
1455.641911	190179.277299	36.155840
1456.371057	190498.768347	36.160858
1457.604145	190818.733382	36.165876
1459.117455	191131.809555	36.170893
1460.554221	191472.715112	36.175911
1462.190030	191794.749007	36.180928
1463.390233	192126.215402	36.185946
1464.614458	192466.070943	36.190964
1465.859748	192797.863213	36.195981
1467.091920	193150.759075	36.200999
1468.757442	193491.522096	36.206016
1470.055450	193844.829446	36.211034
1471.083230	194204.596206	36.216052
1472.698590	194552.178186	36.221069
1473.890696	194913.202976	36.226087
1475.308825	195280.869017	36.231104
1476.908727	195648.239374	36.236122
1478.796119	196000.149763	36.241140
1480.648118	196360.282326	36.246157
1482.071596	196724.603650	36.251175
1483.734902	197077.535592	36.256192
1485.819200	197430.994030	36.261210
1486.975165	197787.444405	36.266228
1488.813566	198135.209847	36.271245
1490.405618	198501.949419	36.276263
1491.845666	198841.114951	36.281280
1493.144173	199194.081996	36.286298
1494.852406	199535.084039	36.291316
1497.165673	199875.755637	36.296333
1498.570517	200222.132743	36.301351
1500.626624	200555.424033	36.306368
1502.125907	200891.618125	36.311386
1503.397171	201238.200690	36.316404
1505.142508	201566.217110	36.321421
1506.280799	201908.826067	36.326439
1507.565004	202245.494833	36.331456
1509.116495	202593.153108	36.336474
1510.133051	202942.897973	36.341492
1512.031240	203276.025358	36.346509
1513.170755	203643.350672	36.351527
1514.382965	203996.368158	36.356544
1515.838377	204348.063206	36.361562
1516.980075	204712.980728	36.366580
1518.700553	205060.494269	36.371597
1520.024060	205427.364793	36.376615
1521.586137	205767.620169	36.381632
1523.205820	206112.654137	36.386650
1524.635619	206465.645427	36.391668
1526.541870	206799.345052	36.396685
1527.824120	207141.482565	36.401703
1529.741485	207463.082004	36.406720
1531.077957	207808.374763	36.411738
1532.572849	208153.933895	36.416756
1534.018675	208496.455327	36.421773
1535.341742	208845.551341	36.426791
1537.125180	209190.532014	36.431808
1538.811246	209536.851342	36.436826
1540.855682	209875.745782	36.441844
1542.678300	210207.466897	36.446861
1544.671457	210549.547287	36.451879
1546.499788	210884.012806	36.456896
1547.738732	211205.882052	36.461914
1548.925999	211552.040696	36.466932
1550.665390	211886.880732	36.471949
1552.009929	212234.970637	36.476967
1553.497836	212582.377005	36.481984
1554.863291	212924.624593	36.487002
1556.286650	213267.904821	36.492020
1557.969369	213617.821449	36.497037
1558.735570	213981.306094	36.502055
1559.660866	214339.786963	36.507072
1561.408859	214713.367024	36.512090
1562.389548	215091.295855	36.517108
1563.506134	215472.809394	36.522125
1564.932745	215879.770965	36.527143
1566.394821	216280.480186	36.532160
1567.747697	216681.463665	36.537178
1568.896638	217098.382969	36.542196
1570.501643	217516.927616	36.547213
1571.952396	217939.564105	36.552231
1573.152704	218363.921455	36.557248
1574.991947	218793.835086	36.562266
1576.330493	219229.246062	36.567284
1578.305133	219658.250999	36.572301
1580.390611	220092.724835	36.577319
1581.840129	220523.931099	36.582336
1583.423469	220948.029728	36.587354
1584.791765	221384.307607	36.592372
1586.493007	221811.259375	36.597389
1588.115060	222248.208260	36.602407
1589.881304	222675.380636	36.607424
1591.822903	223109.890442	36.612442
1592.842171	223550.274573	36.617460
1594.919411	223977.677714	36.622477
1596.624741	224405.603158	36.627495
1598.441804	224840.114945	36.632512
1600.293231	225263.573270	36.637530
1601.885430	225679.939872	36.642548
1603.793062	226101.918086	36.647565
1605.606856	226519.341625	36.652583
1607.249451	226923.333509	36.657600
1609.180521	227305.229574	36.662618
1610.738647	227708.399994	36.667636
1612.410684	228082.798532	36.672653
1614.290026	228477.025951	36.677671
1615.865035	228864.422902	36.682688
1617.620627	229250.951751	36.687706
1619.574804	229638.184254	36.692724
1620.748023	230019.785351	36.697741
1622.569244	230406.077325	36.702759
1623.825849	230795.057782	36.707776
1625.696470	231181.470227	36.712794
1626.651467	231576.448080	36.717812
1628.228529	231973.454169	36.722829
1629.859786	232371.595001	36.727847
1631.551498	232783.290797	36.732864
1633.512613	233182.088341	36.737882
1634.867012	233588.407860	36.742900
1636.758149	233985.872929	36.747917
1637.830323	234402.200021	36.752935
1639.411368	234820.879559	36.757952
1641.205329	235229.921738	36.762970
1642.272594	235653.542773	36.767988
1644.421555	236073.067770	36.773005
1646.655217	236482.672411	36.778023
1648.129589	236898.326459	36.783040
1649.921060	237312.682392	36.788058
1651.450860	237727.033107	36.793076
1653.156899	238144.453528	36.798093
1654.969597	238570.035997	36.803111
1656.782609	238988.481191	36.808128
1658.744376	239393.921133	36.813146
1660.847207	239795.552694	36.818164
1662.563382	240206.624547	36.823181
1664.347438	240617.685471	36.828199
1665.702127	241026.458096	36.833216
1667.587208	241428.840803	36.838234
1669.221679	241839.192579	36.843252
1670.973396	242234.054754	36.848269
1672.358770	242640.538338	36.853287
1674.553599	243047.900108	36.858304
1676.298296	243436.592286	36.863322
1678.142799	243856.563995	36.868340
1679.271450	244259.105451	36.873357
1680.808893	244668.385401	36.878375
1682.146169	245089.385373	36.883392
1683.623246	245503.985825	36.888410
1684.744114	245938.004659	36.893428
1686.500130	246369.222622	36.898445
1687.824761	246806.001886	36.903463
1689.227532	247247.569399	36.908480
1690.953787	247700.564156	36.913498
1692.141142	248144.760522	36.918516
1694.233996	248596.118450	36.923533
1695.573301	249034.675565	36.928551
1696.919681	249485.374487	36.933568
1698.445375	249920.674238	36.938586
1700.204306	250376.561704	36.943604
1701.373578	250816.648034	36.948621
1702.936375	251264.821718	36.953639
1704.800557	251717.110223	36.958656
1706.533618	252169.700847	36.963674
1708.038338	252639.528699	36.968692
1709.530968	253109.943114	36.973709
1711.109641	253581.105100	36.978727
1712.685725	254063.241875	36.983744
1714.628958	254536.577293	36.988762
1716.311744	255027.917449	36.993780
1718.404388	255496.858173	36.998797
1720.195558	255972.099728	37.003815
1721.635904	256462.770283	37.008832
1723.548250	256934.256894	37.013850
1725.494752	257427.330374	37.018868
1727.003025	257919.310238	37.023885
1728.861712	258403.913962	37.028903
1730.338407	258894.552690	37.033920
1732.777730	259387.516120	37.038938
1734.798420	259877.451823	37.043956
1736.285217	260352.643228	37.048973
1738.473915	260827.638146	37.053991
1740.094635	261320.867847	37.059008
1741.891464	261795.802300	37.064026
1744.130129	262281.609627	37.069044
1745.708411	262761.331253	37.074061
1747.744634	263243.844745	37.079079
1749.183175	263729.152837	37.084096
1751.310066	264200.726743	37.089114
1752.889103	264691.141385	37.094132
1755.011144	265172.571622	37.099149
1756.903547	265640.983544	37.104167
1758.776461	266120.956655	37.109184
1761.213945	266588.944098	37.114202
1763.179757	267055.182693	37.119220
1765.220918	267520.264722	37.124237
1766.676766	267981.737497	37.129255
1768.249783	268445.856934	37.134272
1770.527575	268910.160022	37.139290
1772.469375	269379.549680	37.144308
1774.073400	269837.971680	37.149325
1775.855444	270286.963577	37.154343
1778.000406	270748.644825	37.159360
1780.123462	271194.223870	37.164378
1781.813913	271650.799296	37.169396
1783.135735	272105.811263	37.174413
1784.589558	272561.765162	37.179431
1786.458415	273031.415348	37.184448
1788.074054	273487.593929	37.189466
1789.351783	273955.158879	37.194484
1790.723601	274433.629773	37.199501
1792.623089	274890.595372	37.204519
1794.051387	275355.743925	37.209536
1796.046044	275822.598156	37.214554
1797.686233	276275.515492	37.219572
1798.707383	276744.718790	37.224589
1800.855043	277207.530243	37.229607
1802.158929	277693.245009	37.234624
1803.307755	278162.169113	37.239642
1805.127371	278655.693184	37.244660
1806.766715	279156.181434	37.249677
1808.247797	279651.437255	37.254695
1809.965465	280167.632869	37.259712
1811.357742	280677.633865	37.264730
1813.021146	281199.296978	37.269748
1814.829796	281734.193075	37.274765
1816.725284	282260.410764	37.279783
1818.087293	282802.009436	37.284800
1819.539501	283345.089466	37.289818
1821.123456	283890.278715	37.294836
1822.742661	284458.422297	37.299853
1824.706558	285014.286982	37.304871
1826.291011	285594.522824	37.309888
1828.098570	286164.634121	37.314906
1830.000399	286743.413889	37.319924
1831.358167	287327.770724	37.324941
1833.398677	287912.998822	37.329959
1835.325300	288509.343616	37.334976
1837.298659	289097.448066	37.339994
1839.163874	289695.474206	37.345012
1840.778004	290296.943969	37.350029
1843.196053	290889.205598	37.355047
1845.220613	291494.028129	37.360064
1846.629889	292091.002804	37.365082
1848.741429	292689.022635	37.370100
1851.264377	293282.447915	37.375117
1853.447153	293874.683681	37.380135
1855.762227	294457.115098	37.385152
1857.915260	295029.970409	37.390170
1860.196936	295609.226461	37.395188
1862.225175	296195.050048	37.400205
1864.387921	296754.636345	37.405223
1866.536638	297328.419502	37.410240
1868.610891	297886.363809	37.415258
1870.635234	298444.669084	37.420276
1872.327699	299006.024863	37.425293
1874.149271	299555.139099	37.430311
1876.726149	300110.216347	37.435328
1878.854200	300663.487697	37.440346
1880.786168	301215.646424	37.445364
1882.489569	301759.256772	37.450381
1884.604396	302291.568125	37.455399
1886.317057	302834.637073	37.460416
1888.253361	303386.451606	37.465434
1890.182658	303934.378227	37.470452
1892.063002	304471.262439	37.475469
1894.206405	305009.393481	37.480487
1895.982190	305534.428951	37.485504
1897.865723	306043.570419	37.490522
1900.097746	306540.586293	37.495540
1901.796854	307046.223135	37.500557
1904.214202	307538.045978	37.505575
1906.178250	308041.421891	37.510592
1907.914586	308541.684603	37.515610
1910.116181	309037.115755	37.520628
1911.514224	309539.791667	37.525645
1913.343733	310056.027290	37.530663
1914.746862	310562.123892	37.535680
1916.745641	311065.804383	37.540698
1919.093499	311586.435674	37.545716
1921.059364	312090.775128	37.550733
1923.377891	312603.659213	37.555751
1925.444940	313119.833052	37.560768
1926.812723	313633.202596	37.565786
1928.692351	314149.147185	37.570804
1930.155323	314674.833936	37.575821
1931.885527	315211.288296	37.580839
1933.251490	315749.832219	37.585856
1935.350558	316287.078526	37.590874
1937.280093	316825.720782	37.595892
1938.694847	317373.689415	37.600909
1940.787002	317922.426436	37.605927
1942.908003	318493.549179	37.610944
1944.304735	319047.093240	37.615962
1946.436770	319619.448485	37.620980
1947.948242	320192.006379	37.625997
1949.845165	320760.532341	37.631015
1951.621552	321346.973958	37.636032
1953.448282	321925.809912	37.641050
1955.797788	322496.223265	37.646068
1957.570531	323098.898533	37.651085
1959.862532	323681.523125	37.656103
1961.853539	324271.632609	37.661120
1963.848613	324862.497295	37.666138
1966.370655	325448.670705	37.671156
1968.140616	326033.545207	37.676173
1969.856900	326625.480948	37.681191
1972.116369	327214.855177	37.686208
1974.277103	327814.573001	37.691226
1976.313049	328391.254292	37.696244
1978.208543	328996.920299	37.701261
1979.951938	329577.574533	37.706279
1982.009027	330180.407618	37.711296
1984.085383	330776.655850	37.716314
1985.863136	331369.978547	37.721332
1988.163379	331974.958982	37.726349
1989.868188	332566.732587	37.731367
1991.796005	333172.321776	37.736384
1994.015792	333764.476396	37.741402
1996.007597	334359.811055	37.746420
1997.750612	334979.651859	37.751437
1999.740873	335574.744503	37.756455
2001.467383	336161.041920	37.761472
2003.041117	336756.547522	37.766490
2005.302209	337337.511074	37.771508
2006.673959	337931.412929	37.776525
2008.948367	338528.199283	37.781543
2010.249670	339130.399000	37.786560
2012.109079	339737.546923	37.791578
2014.035277	340343.178413	37.796596
2015.603604	340982.214403	37.801613
2017.254105	341608.385219	37.806631
2019.283913	342252.223955	37.811648
2021.296939	342898.163415	37.816666
2023.301495	343526.735741	37.821684
2025.428539	344182.561597	37.826701
2028.275816	344819.905991	37.831719
2030.338112	345465.167113	37.836736
2032.093237	346121.079855	37.841754
2034.138177	346766.198713	37.846772
2035.909327	347421.531629	37.851789
2037.998565	348090.783462	37.856807
2040.176304	348750.722187	37.861824
2042.127158	349418.632720	37.866842
2044.151023	350090.504672	37.871860
2046.332200	350754.853548	37.876877
2048.306079	351420.699460	37.881895
2050.696759	352086.362296	37.886912
2051.995916	352771.206939	37.891930
2054.275465	353446.636703	37.896948
2056.400235	354149.384207	37.901965
2057.990458	354835.338091	37.906983
2060.370749	355538.043860	37.912000
2062.227259	356227.532079	37.917018
2064.882694	356913.117017	37.922036
2067.488012	357604.813512	37.927053
2069.653886	358292.209470	37.932071
2071.888511	358967.074141	37.937088
2074.349366	359659.089732	37.942106
2076.356670	360319.762942	37.947124
2078.468932	361014.985585	37.952141
2080.749077	361696.188864	37.957159
2082.794542	362372.980829	37.962176
2084.663192	363056.868832	37.967194
2086.594388	363740.860770	37.972212
2088.746461	364446.897410	37.977229
2090.918606	365127.753717	37.982247
2093.566944	365804.229371	37.987264
2095.260893	366496.227595	37.992282
2097.530394	367176.522574	37.997300
2099.392706	367864.839169	38.002317
2101.562443	368555.601333	38.007335
2103.979030	369239.941861	38.012352
2105.703228	369926.137911	38.017370
2107.487460	370612.691048	38.022388
2110.078884	371319.408231	38.027405
2111.766895	372008.284272	38.032423
2114.198236	372667.803464	38.037440
2116.374326	373338.791680	38.042458
2117.976001	374004.362005	38.047476
2120.238649	374674.269897	38.052493
2121.796583	375349.864356	38.057511
2123.939312	376020.121581	38.062528
2125.677139	376706.968567	38.067546
2128.221284	377392.624100	38.072564
2130.134200	378069.701393	38.077581
2132.329742	378756.783373	38.082599
2134.541478	379447.550453	38.087616
2136.167839	380145.680350	38.092634
2138.302804	380849.590926	38.097652
2140.391442	381549.767161	38.102669
2142.894083	382267.326594	38.107687
2144.965646	382968.717529	38.112704
2146.014567	383697.902884	38.117722
2148.127640	384416.292363	38.122740
2150.501998	385147.778599	38.127757
2152.872577	385894.281906	38.132775
2155.177932	386626.835781	38.137792
2156.983839	387361.916872	38.142810
2159.173606	388092.276014	38.147828
2161.190307	388847.565481	38.152845
2163.513906	389606.129911	38.157863
2166.038918	390353.766960	38.162880
2167.847876	391104.220197	38.167898
2169.947778	391855.416161	38.172916
2172.590239	392615.371612	38.177933
2175.100494	393369.602366	38.182951
2177.383356	394124.689239	38.187968
2179.697470	394877.014364	38.192986
2181.925567	395633.592606	38.198004
2184.245844	396381.721811	38.203021
2186.362309	397142.233449	38.208039
2188.956226	397892.354950	38.213056
2190.837113	398648.331108	38.218074
2193.161894	399401.373348	38.223092
2195.943443	400152.898583	38.228109
2197.960513	400908.842125	38.233127
2200.192909	401658.090061	38.238144
2202.449016	402419.729113	38.243162
2204.898785	403168.164629	38.248180
2207.138236	403908.685807	38.253197
2209.429447	404674.488010	38.258215
2211.413788	405429.655544	38.263232
2213.542129	406190.832323	38.268250
2215.359054	406945.327785	38.273268
2217.658234	407711.752555	38.278285
2219.377331	408485.322147	38.283303
2221.353441	409249.478375	38.288320
2223.328014	410035.447428	38.293338
2225.518285	410822.470764	38.298356
2227.515252	411612.998969	38.303373
2229.521133	412385.696386	38.308391
2231.970457	413162.474049	38.313408
2234.057154	413929.615815	38.318426
2236.317146	414692.273191	38.323444
2238.812466	415456.083277	38.328461
2241.232898	416217.452235	38.333479
2243.092877	416982.338179	38.338496
2244.946962	417758.951648	38.343514
2247.006501	418531.606513	38.348532
2249.743944	419308.097049	38.353549
2251.788177	420098.228177	38.358567
2253.696276	420877.925884	38.363584
2256.450453	421661.834438	38.368602
2258.668874	422456.645551	38.373620
2260.653928	423254.204959	38.378637
2262.752704	424055.769363	38.383655
2265.075459	424850.788273	38.388672
2267.459996	425667.287587	38.393690
2269.680617	426477.205638	38.398708
2272.466635	427286.442681	38.403725
2274.220807	428106.560734	38.408743
2276.522112	428923.215781	38.413760
2278.252681	429749.051645	38.418778
2280.455542	430578.877721	38.423796
2283.122937	431413.302152	38.428813
2285.220111	432251.893811	38.433831
2287.733930	433081.779624	38.438848
2289.986786	433915.830149	38.443866
2292.313473	434765.273348	38.448884
2294.898981	435600.015142	38.453901
2297.041783	436449.173707	38.458919
2299.821882	437299.861230	38.463936
2302.587491	438145.205810	38.468954
2305.138816	438981.649494	38.473972
2307.663621	439811.842712	38.478989
2309.827229	440658.004120	38.484007
2312.449042	441488.825967	38.489024
2315.049636	442313.144178	38.494042
2317.270946	443140.784400	38.499060
2319.836413	443961.100158	38.504077
2322.678253	444811.992631	38.509095
2325.227883	445619.348573	38.514112
2327.327872	446439.345885	38.519130
2329.442027	447259.815041	38.524148
2331.889834	448079.183887	38.529165
2334.043917	448897.458498	38.534183
2336.998642	449713.440306	38.539200
2339.211661	450530.073411	38.544218
2341.726116	451348.746974	38.549236
2344.626724	452150.533571	38.554253
2347.121869	452955.341809	38.559271
2350.163865	453745.209743	38.564288
2353.026975	454535.027270	38.569306
2355.373704	455323.739631	38.574324
2358.207022	456091.912568	38.579341
2360.120000	456876.088499	38.584359
2362.541756	457618.590998	38.589376
2364.639906	458370.170365	38.594394
2366.283842	459125.084991	38.599412
2368.742954	459872.603202	38.604429
2370.389149	460639.743466	38.609447
2372.702110	461389.150313	38.614464
2374.917939	462152.849047	38.619482
2377.213127	462932.222880	38.624500
2379.688608	463694.806369	38.629517
2381.547506	464487.332964	38.634535
2383.897251	465262.207620	38.639552
2386.115528	466053.294870	38.644570
2387.997592	466854.159625	38.649588
2390.035219	467652.842179	38.654605
2392.089111	468474.276197	38.659623
2394.527452	469295.508042	38.664640
2396.928129	470123.935487	38.669658
2398.772970	470973.993729	38.674676
2401.455859	471809.018103	38.679693
2403.790865	472658.663753	38.684711
2405.633401	473509.617755	38.689728
2408.554740	474370.955731	38.694746
2410.673442	475227.137949	38.699764
2413.379689	476096.059096	38.704781
2415.807832	476974.380387	38.709799
2418.149239	477849.593763	38.714816
2420.465940	478722.900871	38.719834
2422.987840	479601.433021	38.724852
2426.056166	480480.334017	38.729869
2428.421350	481360.675554	38.734887
2430.903150	482228.028732	38.739904
2433.266351	483112.323566	38.744922
2435.580819	484000.621500	38.749940
2438.660940	484881.878540	38.754957
2441.636720	485758.818677	38.759975
2443.940797	486635.678431	38.764992
2446.526152	487517.695490	38.770010
2448.880388	488406.117310	38.775028
2451.160065	489291.276430	38.780045
2453.095634	490186.946059	38.785063
2455.786826	491074.819994	38.790080
2458.066144	491972.558290	38.795098
2460.044396	492881.098989	38.800116
2462.469429	493775.538663	38.805133
2464.891581	494688.851522	38.810151
2467.656650	495593.479876	38.815168
2470.322458	496507.459799	38.820186
2472.575641	497418.433732	38.825204
2475.661687	498320.892703	38.830221
2478.177648	499238.128390	38.835239
2480.944338	500132.775800	38.840256
2483.703189	501031.763790	38.845274
2485.948156	501935.430103	38.850292
2488.573118	502842.108170	38.855309
2490.876787	503727.864242	38.860327
2493.355518	504606.079585	38.865344
2495.627512	505473.442356	38.870362
2497.975269	506343.216014	38.875380
2500.298890	507223.180903	38.880397
2502.389647	508108.329672	38.885415
2504.670878	508992.287822	38.890432
2507.435778	509869.410177	38.895450
2509.234312	510773.362887	38.900468
2511.600667	511663.861120	38.905485
2514.170953	512580.027226	38.910503
2516.408739	513488.435854	38.915520
2518.595705	514416.301873	38.920538
2520.848382	515356.144191	38.925556
2523.382883	516290.792439	38.930573
2525.452967	517244.054581	38.935591
2527.739236	518196.968825	38.940608
2530.299848	519171.136381	38.945626
2532.116073	520142.296254	38.950644
2534.751422	521129.624243	38.955661
2537.559468	522118.117528	38.960679
2540.061262	523116.469527	38.965696
2541.914470	524115.571101	38.970714
2544.112405	525126.682948	38.975732
2546.628553	526149.101939	38.980749
2548.900379	527183.425080	38.985767
2550.726547	528234.919945	38.990784
2553.450174	529283.216257	38.995802
2555.887024	530352.880512	39.000820
2558.147260	531425.164422	39.005837
2560.779784	532502.187844	39.010855
2563.520822	533575.086552	39.015872
2566.445669	534668.406076	39.020890
2568.926914	535760.158384	39.025908
2571.663374	536835.884105	39.030925
2574.555885	537928.004344	39.035943
2576.905987	539033.817091	39.040960
2579.609742	540127.711848	39.045978
2582.192241	541225.063426	39.050996
2584.773551	542322.027637	39.056013
2588.022702	543431.565868	39.061031
2590.562543	544535.052004	39.066048
2593.461682	545621.694569	39.071066
2596.057534	546731.080419	39.076084
2599.266208	547823.479839	39.081101
2602.142849	548913.988825	39.086119
2604.703749	550005.821871	39.091136
2607.496253	551088.429848	39.096154
2610.215515	552181.116339	39.101172
2612.852064	553265.586979	39.106189
2615.582041	554359.753272	39.111207
2618.628380	555436.139066	39.116224
2621.393905	556525.348374	39.121242
2623.588394	557612.757326	39.126260
2626.554301	558686.431753	39.131277
2629.683073	559750.848771	39.136295
2632.453879	560777.218451	39.141312
2635.765565	561799.849338	39.146330
2638.455196	562814.621819	39.151348
2641.509289	563816.096231	39.156365
2644.397850	564820.986108	39.161383
2646.855761	565822.206142	39.166400
2649.501801	566815.032410	39.171418
2651.693456	567821.764908	39.176436
2654.367040	568827.582793	39.181453
2656.627583	569837.106030	39.186471
2659.195727	570847.249224	39.191488
2662.077510	571857.007216	39.196506
2664.413085	572873.903227	39.201524
2666.996957	573892.781888	39.206541
2669.807007	574924.433188	39.211559
2672.411076	575952.673114	39.216576
2675.256428	576983.646100	39.221594
2677.417830	578028.644661	39.226612
2679.702078	579067.715791	39.231629
2682.615795	580117.675001	39.236647
2684.773037	581189.487344	39.241664
2687.502430	582240.800327	39.246682
2689.958850	583320.798188	39.251700
2692.098364	584398.397819	39.256717
2694.556461	585490.785399	39.261735
2696.975720	586603.431028	39.266752
2699.944431	587701.294885	39.271770
2702.661841	588820.500011	39.276788
2705.187243	589929.510611	39.281805
2707.669622	591050.500465	39.286823
2710.762572	592171.229740	39.291840
2713.224178	593298.522957	39.296858
2716.047121	594439.922281	39.301876
2718.572343	595576.603204	39.306893
2721.506677	596730.581871	39.311911
2724.261225	597873.860538	39.316928
2726.986876	599026.244439	39.321946
2729.790806	600184.908407	39.326964
2732.636530	601327.629144	39.331981
2735.720802	602486.163132	39.336999
2738.035171	603644.110502	39.342016
2740.894233	604806.401176	39.347034
2743.542958	605975.314113	39.352052
2745.920452	607136.496989	39.357069
2749.207064	608313.164389	39.362087
2752.097916	609482.122092	39.367104
2755.408847	610646.233899	39.372122
2758.374138	611820.286023	39.377140
2760.849652	612978.694653	39.382157
2763.732072	614143.613006	39.387175
2766.243735	615318.121358	39.392192
2769.201380	616488.878364	39.397210
2771.902383	617664.202861	39.402228
2774.556486	618829.412130	39.407245
2777.214392	619988.948311	39.412263
2779.867560	621128.772048	39.417280
2782.702082	622259.500338	39.422298
2785.642630	623403.281548	39.427316
2788.304993	624532.051289	39.432333
2791.471733	625654.521580	39.437351
2793.722014	626793.712040	39.442368
2796.756301	627924.605899	39.447386
2799.661907	629068.184237	39.452404
2802.034140	630220.517286	39.457421
2804.800485	631374.354089	39.462439
2807.701532	632533.581740	39.467456
2810.439954	633694.804794	39.472474
2812.799202	634867.791088	39.477492
2815.006548	636040.471056	39.482509
2817.786709	637222.599962	39.487527
2819.873318	638427.162293	39.492544
2822.684547	639632.956038	39.497562
2825.283672	640855.851937	39.502580
2828.154183	642079.651980	39.507597
2831.212745	643304.469266	39.512615
2833.513410	644551.904392	39.517632
2836.441311	645795.388950	39.522650
2839.104718	647050.130196	39.527668
2841.995071	648303.230128	39.532685
2844.648974	649558.904275	39.537703
2847.458100	650838.361140	39.542720
2850.201991	652128.624951	39.547738
2853.145478	653407.328123	39.552756
2855.940020	654695.852509	39.557773
2859.204491	655988.011972	39.562791
2861.800615	657287.584191	39.567808
2864.562654	658580.780767	39.572826
2867.766992	659894.140442	39.577844
2870.108270	661206.722525	39.582861
2873.322190	662519.126074	39.587879
2876.280259	663844.580965	39.592896
2879.267144	665160.642540	39.597914
2882.474331	666477.430025	39.602932
2884.656210	667801.024734	39.607949
2887.655417	669137.772889	39.612967
2890.494570	670482.265625	39.617984
2893.221149	671826.634984	39.623002
2896.068072	673166.068049	39.628020
2898.628684	674522.009323	39.633037
2902.323387	675877.509463	39.638055
2904.837768	677233.758255	39.643072
2907.964086	678587.566879	39.648090
2911.388878	679949.321969	39.653108
2914.158894	681304.430216	39.658125
2917.249464	682643.788083	39.663143
2920.185804	684007.405391	39.668160
2923.252759	685362.603577	39.673178
2926.376622	686722.155712	39.678196
2928.960843	688086.955090	39.683213
2932.020939	689426.206619	39.688231
2935.372391	690742.929571	39.693248
2937.977683	692034.780293	39.698266
2940.979601	693350.581749	39.703284
2943.936310	694657.218576	39.708301
2947.154618	695949.335800	39.713319
2949.739842	697271.665363	39.718336
2952.471012	698585.144771	39.723354
2955.310348	699898.209999	39.728372
2957.775253	701227.049501	39.733389
2961.087276	702558.365288	39.738407
2963.383828	703909.764156	39.743424
2965.873990	705249.425946	39.748442
2968.468317	706611.990504	39.753460
2971.007665	707978.853956	39.758477
2973.853591	709363.022785	39.763495
2976.568533	710752.087590	39.768512
2979.658329	712146.503207	39.773530
2983.005256	713547.919315	39.778548
2985.931282	714962.533263	39.783565
2988.807188	716380.281203	39.788583
2991.712880	717801.839495	39.793600
2994.550677	719225.787834	39.798618
2997.285227	720676.061502	39.803636
2999.828873	722123.345099	39.808653
3003.165891	723576.120978	39.813671
3005.401374	725051.017011	39.818688
3008.442274	726529.462525	39.823706
3011.535453	728005.655069	39.828724
3014.396322	729505.771650	39.833741
3017.539141	730989.364732	39.838759
3020.507765	732498.685140	39.843776
3023.506330	733999.226478	39.848794
3026.819583	735508.563626	39.853812
3029.739516	737025.923204	39.858829
3033.271532	738539.780606	39.863847
3036.240171	740054.579520	39.868864
3039.273839	741579.729209	39.873882
3042.577345	743092.456875	39.878900
3045.792089	744619.647867	39.883917
3049.185998	746133.103312	39.888935
3052.256929	747661.251061	39.893952
3055.837554	749188.764357	39.898970
3058.760018	750703.083733	39.903988
3061.857737	752228.156565	39.909005
3065.022155	753730.461664	39.914023
3068.378044	755249.915598	39.919040
3071.476721	756777.182593	39.924058
3074.521598	758287.075694	39.929076
3077.721163	759810.909243	39.934093
3080.881398	761318.897421	39.939111
3084.089778	762834.197776	39.944128
3087.200619	764349.208195	39.949146
3090.399127	765858.881730	39.954164
3093.328831	767384.416131	39.959181
3096.250864	768889.441148	39.964199
3099.838207	770369.677146	39.969216
3102.621158	771838.749799	39.974234
3105.809696	773299.011983	39.979252
3108.286975	774758.416639	39.984269
3111.484971	776231.298921	39.989287
3114.420894	777711.093233	39.994304
3117.414679	779183.803436	39.999322
3120.176025	780675.190465	40.004340
3122.907260	782173.532999	40.009357
3126.103704	783665.990427	40.014375
3128.859321	785181.696957	40.019392
3131.452158	786705.638176	40.024410
3134.633850	788227.975456	40.029428
3137.443569	789766.953169	40.034445
3140.282541	791313.525990	40.039463
3143.760435	792871.011953	40.044480
3146.521007	794432.338133	40.049498
3149.675269	796005.339655	40.054516
3152.825915	797590.466660	40.059533
3155.988918	799167.106189	40.064551
3159.215123	800762.503246	40.069568
3161.990983	802368.709927	40.074586
3164.925416	803969.085681	40.079604
3168.362626	805587.040129	40.084621
3171.586900	807201.860683	40.089639
3174.913550	808830.205656	40.094656
3178.020371	810456.388610	40.099674
3181.328126	812101.583146	40.104692
3184.278767	813747.265716	40.109709
3187.681401	815384.900003	40.114727
3190.858743	817038.080630	40.119744
3193.438576	818701.295832	40.124762
3197.006606	820362.558791	40.129780
3199.999822	822030.426537	40.134797
3203.110365	823702.872914	40.139815
3206.299770	825387.990513	40.144832
3209.337625	827078.254192	40.149850
3212.931319	828765.596706	40.154868
3215.669071	830464.529874	40.159885
3219.294704	832150.399733	40.164903
3222.500016	833847.971962	40.169920
3225.435940	835556.090559	40.174938
3229.129641	837251.119631	40.179956
3232.390886	838961.530454	40.184973
3235.446623	840663.929667	40.189991
3239.004432	842371.326706	40.195008
3241.783279	844079.754840	40.200026
3245.078735	845796.278323	40.205044
3248.328082	847521.179011	40.210061
3251.409538	849240.386661	40.215079
3254.929584	850970.209240	40.220096
3257.670413	852698.710772	40.225114
3261.381219	854432.966826	40.230132
3264.801684	856161.835519	40.235149
3267.674337	857879.156631	40.240167
3271.167041	859571.261845	40.245184
3274.045171	861263.582744	40.250202
3277.432215	862924.626222	40.255220
3280.317549	864610.195597	40.260237
3283.791508	866299.647538	40.265255
3287.184565	867991.154824	40.270272
3290.215380	869692.505454	40.275290
3293.678212	871384.587600	40.280308
3296.687202	873091.549610	40.285325
3299.573849	874797.749993	40.290343
3302.762809	876513.460043	40.295360
3306.013508	878241.126943	40.300378
3309.356947	879970.973832	40.305396
3312.334945	881708.581030	40.310413
3315.779368	883452.735437	40.315431
3319.116094	885198.410622	40.320448
3322.196222	886967.632547	40.325466
3325.598134	888717.924762	40.330484
3329.027282	890489.089849	40.335501
3331.903678	892258.450538	40.340519
3335.680343	894038.770926	40.345536
3338.771258	895826.936675	40.350554
3342.254254	897623.813886	40.355572
3345.188302	899436.871178	40.360589
3348.322880	901237.275665	40.365607
3351.394966	903049.622017	40.370624
3354.120327	904883.949964	40.375642
3357.573999	906725.337814	40.380660
3360.850082	908581.429475	40.385677
3363.952503	910438.752184	40.390695
3367.432120	912301.339361	40.395712
3370.723051	914175.522315	40.400730
3373.801828	916052.457917	40.405748
3377.393039	917947.468897	40.410765
3380.357568	919829.067760	40.415783
3384.046988	921726.382795	40.420800
3387.281575	923636.432186	40.425818
3390.653487	925531.784645	40.430836
3394.043036	927450.507869	40.435853
3397.284223	929369.617525	40.440871
3400.981450	931294.464101	40.445888
3404.035909	933236.327117	40.450906
3407.543461	935157.401943	40.455924
3410.913757	937103.806845	40.460941
3414.336610	939042.881059	40.465959
3418.063983	940980.033574	40.470976
3421.292109	942935.364742	40.475994
3424.566977	944883.358808	40.481012
3427.989437	946840.325623	40.486029
3431.130224	948809.282893	40.491047
3434.592661	950783.045097	40.496064
3437.378595	952811.976933	40.501082
3440.972701	954829.789702	40.506100
3444.238815	956881.755059	40.511117
3447.436031	958912.751530	40.516122
3451.297933	960874.383381	40.521127
3454.351877	962809.538674	40.526132
3457.761410	964655.208329	40.531136
3461.136411	966430.918017	40.536141
3464.420108	968145.740896	40.541146
3467.830241	969775.539906	40.546151
3470.918155	971321.734554	40.551156
3474.520258	972777.505455	40.556160
3477.346839	974146.952205	40.561165
3479.887933	975451.056861	40.566170
3483.059075	976661.089885	40.571175
3485.099593	977812.273208	40.576180
3486.957164	978874.311799	40.581184
3489.624763	979868.854401	40.586189
3491.805333	980785.421415	40.591194
3493.986372	981639.776221	40.596199
3495.765843	982432.991079	40.601204
3497.992138	983151.093082	40.606208
3499.692021	983813.493944	40.611213
3501.305582	984420.723217	40.616218
3503.088329	984957.637841	40.621223
3504.783328	985462.822492	40.626228
3506.215729	985884.535867	40.631232
3507.624282	986271.997110	40.636237
3508.932608	986602.410953	40.641242
3510.445364	986887.044959	40.646247
3511.657448	987151.437700	40.651252
3512.714391	987344.385803	40.656256
3513.912100	987518.586082	40.661261
3515.034250	987646.489404	40.666266
3516.274422	987717.732736	40.671271
3517.053511	987774.334206	40.676276
3518.263585	987795.573533	40.681280
3519.181864	987779.819825	40.686285
3519.833723	987735.451906	40.691290
3520.698524	987660.242652	40.696295
3521.335655	987563.527131	40.701300
3522.012864	987436.874654	40.706304
3522.855469	987284.941341	40.711309
3522.667648	987114.753776	40.716314
3523.916828	986914.677100	40.721319
3524.326954	986720.781583	40.726324
3524.980900	986482.668932	40.731328
3525.788573	986240.229747	40.736333
3525.920192	985975.760412	40.741338
3526.674755	985682.795021	40.746343
3526.985148	985392.425948	40.751348
3527.447016	985082.803326	40.756352
3527.376079	984757.454478	40.761357
3527.986828	984421.046337	40.766362
3528.735602	984067.426897	40.771367
3528.746365	983699.181269	40.776372
3529.004240	983328.235595	40.781376
3529.322166	982934.425522	40.786381
3529.603617	982544.790008	40.791386
3530.016109	982136.077818	40.796391
3529.892464	981736.991153	40.801396
3530.296433	981313.681302	40.806400
3530.802537	980888.565807	40.811405
3530.468850	980454.679766	40.816410
3530.990779	980010.169935	40.821415
3531.460303	979564.170094	40.826420
3531.507887	979099.853026	40.831424
3531.725941	978638.593491	40.836429
3531.797867	978156.718350	40.841434
3532.163896	977672.994559	40.846439
3532.176159	977194.075648	40.851444
3532.294187	976711.777721	40.856448
3532.539775	976220.919227	40.861453
3532.402915	975724.613347	40.866458
3532.696176	975214.904261	40.871463
3532.631673	974715.079004	40.876468
3532.710739	974209.615879	40.881472
3532.496977	973707.676061	40.886477
3532.757952	973203.656550	40.891482
3532.895177	972681.141013	40.896487
3533.265287	972162.741211	40.901492
3533.244625	971628.915499	40.906496
3533.223283	971101.688266	40.911501
3533.095576	970574.821755	40.916506
3533.310928	970050.195058	40.921511
3533.121829	969515.810014	40.926516
3533.253617	968979.266510	40.931520
3533.496036	968451.946038	40.936525
3533.474450	967913.959670	40.941530
3533.722143	967363.256776	40.946535
3533.608578	966816.280600	40.951540
3533.534016	966274.725170	40.956544
3533.692171	965724.760972	40.961549
3533.851815	965176.799067	40.966554
3533.912084	964622.537716	40.971559
3533.990565	964066.555708	40.976564
3534.001514	963494.672257	40.981568
3533.891662	962940.767199	40.986573
3534.012683	962383.538161	40.991578
3534.192997	961809.499862	40.996583
3533.503600	961251.124333	41.001588
3533.782674	960689.884792	41.006592
3534.003674	960126.249552	41.011597
3534.163773	959561.883781	41.016602
3534.238988	958991.206922	41.021607
3534.192226	958413.439584	41.026612
3534.389679	957834.396702	41.031616
3534.270505	957263.189875	41.036621
3534.180707	956694.959793	41.041626
3534.457731	956112.593980	41.046631
3534.343123	955540.039381	41.051636
3534.352560	954947.210225	41.056640
3534.094442	954363.190478	41.061645
3534.359180	953787.651785	41.066650
3534.196980	953196.829478	41.071655
3534.252076	952619.641009	41.076660
3534.167157	952038.789395	41.081664
3534.618177	951457.395499	41.086669
3534.470450	950869.864345	41.091674
3534.769790	950282.834503	41.096679
3534.423006	949713.970331	41.101684
3534.185553	949134.024285	41.106688
3534.292700	948551.657630	41.111693
3534.123507	947987.162280	41.116698
3534.402523	947396.215558	41.121703
3534.480339	946830.784996	41.126708
3534.487072	946245.015035	41.131712
3534.960058	945653.260006	41.136717
3534.423173	945072.809086	41.141722
3534.436552	944480.901788	41.146727
3534.186335	943899.024898	41.151732
3534.300640	943328.415280	41.156736
3534.261629	942746.468015	41.161741
3534.289413	942156.972959	41.166746
3534.297598	941567.701404	41.171751
3534.245858	940990.635565	41.176756
3534.267250	940403.624335	41.181760
3534.499865	939816.510622	41.186765
3534.121010	939233.076597	41.191770
3534.618676	938630.450230	41.196775
3534.596187	938054.586623	41.201780
3534.579110	937467.250383	41.206784
3534.709425	936866.495934	41.211789
3534.625887	936269.832080	41.216794
3534.414221	935673.122003	41.221799
3534.556191	935075.995801	41.226804
3534.405950	934478.563679	41.231808
3534.466894	933886.975246	41.236813
3534.291636	933295.360500	41.241818
3534.626276	932700.041873	41.246823
3534.523359	932100.988017	41.251828
3534.566624	931489.364314	41.256832
3534.582306	930893.992124	41.261837
3534.593867	930294.713651	41.266842
3534.596779	929683.655752	41.271847
3534.507470	929098.372219	41.276852
3534.308358	928488.555228	41.281856
3534.499924	927884.075804	41.286861
3534.450644	927289.558103	41.291866
3534.434124	926681.423557	41.296871
3534.677152	926083.455123	41.301876
3534.733916	925472.672226	41.306880
3534.754857	924859.519272	41.311885
3534.447261	924254.617195	41.316890
3534.601581	923643.704727	41.321895
3534.266170	923048.859569	41.326900
3534.332377	922430.325876	41.331904
3534.503696	921820.837237	41.336909
3534.346459	921215.374336	41.341914
3534.531764	920602.379637	41.346919
3534.495166	920003.395725	41.351924
3534.026114	919389.701578	41.356928
3534.541546	918777.501313	41.361933
3534.480426	918167.543119	41.366938
3534.447510	917550.871803	41.371943
3534.042372	916943.817546	41.376948
3534.102119	916326.895011	41.381952
3534.098029	915716.651424	41.386957
3534.348758	915122.084015	41.391962
3534.488129	914501.090077	41.396967
3534.059423	913890.136632	41.401972
3533.977874	913279.055540	41.406976
3534.142316	912666.901013	41.411981
3533.954992	912060.228467	41.416986
3534.274288	911442.323884	41.421991
3534.330061	910836.341410	41.426996
3533.938075	910221.503833	41.432000
3534.211084	909618.722441	41.437005
3534.207538	909000.791161	41.442010
3534.458267	908385.927980	41.447015
3534.310911	907765.858751	41.452020
3534.072154	907147.085251	41.457024
3534.104655	906532.824365	41.462029
3534.037678	905922.273111	41.467034
3534.242512	905292.802229	41.472039
3534.087580	904677.017576	41.477044
3534.005369	904055.171603	41.482048
3534.442021	903433.649940	41.487053
3534.133116	902829.167420	41.492058
3534.234000	902207.566409	41.497063
3534.050695	901581.408979	41.502068
3534.329064	900955.778239	41.507072
3534.079701	900333.449602	41.512077
3533.917766	899716.829202	41.517082
3534.114868	899093.514490	41.522087
3533.918388	898473.577394	41.527092
3533.953987	897842.523431	41.532096
3534.233065	897216.475986	41.537101
3534.071394	896608.303639	41.542106
3533.935656	895954.948390	41.547111
3533.841479	895330.301209	41.552116
3534.115335	894705.618907	41.557120
3533.736998	894077.693543	41.562125
3533.392805	893460.903645	41.567130
3533.775252	892840.636478	41.572135
3533.914024	892221.889948	41.577140
3533.877396	891601.075957	41.582144
3533.831047	890972.074365	41.587149
3533.663210	890348.052490	41.592154
3533.737120	889721.503540	41.597159
3533.748324	889099.926083	41.602164
3533.667194	888472.880161	41.607168
3533.549754	887849.448024	41.612173
3533.467056	887233.295305	41.617178
3533.708696	886605.700274	41.622183
3533.725234	885988.816863	41.627188
3533.498306	885357.101502	41.632192
3533.541720	884721.108823	41.637197
3533.429387	884107.627748	41.642202
3533.519437	883477.588958	41.647207
3533.347374	882866.213301	41.652212
3533.215762	882249.537330	41.657216
3533.305834	881618.812576	41.662221
3533.091129	880990.202267	41.667226
3533.307904	880363.290890	41.672231
3533.421990	879750.860909	41.677236
3533.283743	879125.911600	41.682240
3533.482208	878507.426906	41.687245
3533.364358	877883.988681	41.692250
3533.515842	877255.495448	41.697255
3533.479278	876627.742427	41.702260
3533.457929	876002.149293	41.707264
3533.277303	875368.082427	41.712269
3533.291281	874753.790378	41.717274
3533.274426	874122.373327	41.722279
3533.260851	873492.536837	41.727284
3533.031666	872864.609835	41.732288
3533.196690	872232.959991	41.737293
3533.094624	871607.885054	41.742298
3533.236662	870979.306954	41.747303
3532.954256	870361.311031	41.752308
3532.651967	869732.191822	41.757312
3532.922412	869108.440245	41.762317
3532.697377	868500.431705	41.767322
3533.139590	867869.824299	41.772327
3532.500810	867247.683819	41.777332
3532.554182	866629.049949	41.782336
3533.174781	865997.923730	41.787341
3532.891114	865383.491382	41.792346
3532.754533	864758.676391	41.797351
3532.898082	864134.040105	41.802356
3532.489454	863505.644867	41.807360
3532.800065	862883.570474	41.812365
3532.552379	862265.705235	41.817370
3532.860138	861628.636686	41.822375
3532.669861	861015.784099	41.827380
3532.768228	860388.241773	41.832384
3532.500284	859768.667554	41.837389
3532.895412	859144.250915	41.842394
3533.071215	858514.946676	41.847399
3533.200890	857890.057942	41.852404
3532.793899	857255.278340	41.857408
3532.798740	856613.943961	41.862413
3532.519572	855998.948446	41.867418
3532.258822	855358.014163	41.872423
3532.737649	854738.385645	41.877428
3532.263129	854118.857383	41.882432
3532.710242	853490.644286	41.887437
3532.577262	852865.969304	41.892442
3532.646398	852238.860865	41.897447
3532.794163	851603.596952	41.902452
3532.546518	850977.193180	41.907456
3532.588604	850339.676062	41.912461
3532.000148	849720.601959	41.917466
3532.427252	849085.713662	41.922471
3532.414179	848464.663498	41.927476
3532.011456	847838.845817	41.932480
3532.371392	847210.789708	41.937485
3532.348650	846592.281728	41.942490
3532.380168	845966.202065	41.947495
3532.348220	845343.967680	41.952500
3532.044395	844713.338265	41.957504
3532.921480	844077.571474	41.962509
3532.508578	843451.803723	41.967514
3532.479012	842822.691839	41.972519
3532.820932	842193.453677	41.977524
3532.473694	841549.062482	41.982528
3532.601667	840910.081672	41.987533
3532.439075	840279.568909	41.992538
3532.343579	839640.693026	41.997543
3532.388890	839008.457976	42.002548
3532.300647	838379.547706	42.007552
3532.486282	837745.846277	42.012557
3532.248849	837120.055889	42.017562
3532.406232	836469.257709	42.022567
3532.314852	835842.487687	42.027572
3532.180906	835213.760548	42.032576
3532.348083	834569.402843	42.037581
3531.960367	833946.108540	42.042586
3532.385453	833307.728969	42.047591
3532.203376	832671.732538	42.052596
3531.884015	832048.974586	42.057600
3532.195774	831404.225785	42.062605
3532.169970	830776.314992	42.067610
3532.113854	830140.974921	42.072615
3532.295886	829503.578351	42.077620
3532.106166	828879.173912	42.082624
3531.982594	828241.949574	42.087629
3532.091738	827610.240637	42.092634
3532.491374	826967.868203	42.097639
3532.185655	826331.660170	42.102644
3531.953713	825702.169489	42.107648
3532.216634	825052.204288	42.112653
3531.684248	824426.209297	42.117658
3532.114126	823784.495800	42.122663
3531.871163	823152.073183	42.127668
3531.697850	822512.977890	42.132672
3531.328713	821884.170120	42.137677
3531.349738	821263.890380	42.142682
3531.510390	820631.400828	42.147687
3531.367345	820017.486815	42.152692
3531.057601	819390.680682	42.157696
3531.673837	818766.445238	42.162701
3531.355540	818143.435661	42.167706
3531.115934	817517.076164	42.172711
3531.273439	816895.580558	42.177716
3531.196041	816266.335434	42.182720
3531.466166	815642.452607	42.187725
3531.180467	815018.508401	42.192730
3531.370309	814385.663084	42.197735
3531.283305	813767.050189	42.202740
3531.075853	813142.721712	42.207744
3531.243722	812515.676059	42.212749
3531.165339	811892.188364	42.217754
3531.154828	811268.974030	42.222759
3531.392660	810644.924962	42.227764
3530.915711	810012.907505	42.232768
3530.658283	809386.083632	42.237773
3530.891660	808768.131698	42.242778
3530.884478	808153.299941	42.247783
3530.898074	807521.063756	42.252788
3530.770065	806907.315566	42.257792
3531.008377	806288.107695	42.262797
3531.019405	805669.911488	42.267802
3531.123560	805043.506737	42.272807
3531.156151	804415.880199	42.277812
3531.131627	803779.871593	42.282816
3531.114006	803146.499253	42.287821
3530.290908	802540.811615	42.292826
3530.575409	801912.176939	42.297831
3530.385189	801301.711364	42.302836
3530.355343	800683.267723	42.307840
3530.498395	800063.071284	42.312845
3530.185041	799450.647711	42.317850
3530.280820	798830.397591	42.322855
3530.787871	798224.937083	42.327860
3530.401037	797600.783053	42.332864
3530.581717	796984.131285	42.337869
3530.138338	796373.322367	42.342874
3530.343331	795755.183186	42.347879
3530.292680	795141.106870	42.352884
3530.378024	794525.873245	42.357888
3530.282974	793907.719605	42.362893
3530.134835	793294.724811	42.367898
3530.229600	792682.567803	42.372903
3530.300280	792061.080136	42.377908
3529.776886	791449.117392	42.382912
3530.261646	790824.404651	42.387917
3530.292744	790220.344430	42.392922
3529.888245	789597.786829	42.397927
3530.173856	788998.245280	42.402932
3529.732794	788390.178634	42.407936
3530.141066	787772.038126	42.412941
3529.857169	787167.721467	42.417946
3529.528487	786552.057445	42.422951
3529.773929	785946.612673	42.427956
3529.660404	785336.508002	42.432960
3529.863153	784726.690332	42.437965
3529.604388	784120.635654	42.442970
3529.698920	783507.536713	42.447975
3529.929918	782891.903359	42.452980
3529.354544	782290.664697	42.457984
3529.709877	781692.511725	42.462989
3529.378474	781086.556829	42.467994
3529.243383	780491.141821	42.472999
3529.451999	779883.566965	42.478004
3529.472235	779283.549193	42.483008
3529.645887	778676.911785	42.488013
3529.460070	778070.973685	42.493018
3529.725795	777460.331418	42.498023
3529.553466	776845.086540	42.503028
3529.225276	776248.026148	42.508032
3529.531478	775637.912662	42.513037
3529.362143	775033.194682	42.518042
3529.085821	774416.137625	42.523047
3529.176292	773821.317425	42.528052
3529.221283	773217.840148	42.533056
3529.631713	772608.538781	42.538061
3528.931023	772011.983121	42.543066
3528.787509	771414.298842	42.548071
3529.368545	770806.690177	42.553076
3529.179894	770204.088433	42.558080
3529.416452	769605.896809	42.563085
3529.118553	769005.186143	42.568090
3528.889397	768399.487986	42.573095
3528.892187	767799.416296	42.578100
3529.052193	767198.086505	42.583104
3529.362182	766585.840542	42.588109
3529.200735	765995.704289	42.593114
3529.350402	765387.132617	42.598119
3528.861356	764780.197632	42.603124
3528.566845	764184.518333	42.608128
3528.823270	763588.303054	42.613133
3528.469860	762996.779003	42.618138
3528.740682	762396.423325	42.623143
3528.545755	761805.320558	42.628148
3528.243012	761210.342972	42.633152
3528.920576	760614.213861	42.638157
3528.606356	760020.919715	42.643162
3528.739165	759425.134808	42.648167
3528.695767	758825.682396	42.653172
3528.660640	758233.334758	42.658176
3528.827774	757633.653286	42.663181
3528.835662	757042.241315	42.668186
3528.896617	756428.024956	42.673191
3529.092564	755840.978008	42.678196
3528.953361	755237.458317	42.683200
3528.772689	754620.521532	42.688205
3528.201741	754033.663757	42.693210
3528.544567	753424.685948	42.698215
3528.456967	752836.913333	42.703220
3528.472825	752240.634907	42.708224
3528.475039	751641.794184	42.713229
3528.150887	751057.036507	42.718234
3528.366848	750462.906986	42.723239
3528.029702	749869.369387	42.728244
3527.966192	749283.395454	42.733248
3528.330828	748689.153419	42.738253
3528.380694	748103.861134	42.743258
3528.087553	747505.836714	42.748263
3528.099336	746919.671085	42.753268
3528.119820	746321.304276	42.758272
3527.786672	745727.942885	42.763277
3527.645826	745146.907918	42.768282
3527.647005	744565.360629	42.773287
3527.648657	743983.423991	42.778292
3527.656263	743404.903235	42.783296
3527.642367	742818.384452	42.788301
3527.607493	742241.070389	42.793306
3527.878095	741663.315667	42.798311
3527.764635	741073.519351	42.803316
3527.380157	740493.812821	42.808321
3527.827146	739909.619336	42.813325
3527.769914	739333.134522	42.818330
3527.720347	738754.529064	42.823335
3527.504577	738163.988930	42.828340
3527.498542	737588.802899	42.833345
3527.658209	736999.150844	42.838349
3527.496225	736423.659784	42.843354
3527.751588	735835.290489	42.848359
3527.783270	735244.194480	42.853364
3527.307536	734665.661232	42.858369
3527.335729	734079.527234	42.863373
3527.303955	733509.643725	42.868378
3527.531920	732923.193112	42.873383
3527.350415	732347.511085	42.878388
3527.329096	731774.879227	42.883393
3527.385066	731194.767418	42.888397
3527.327587	730622.604456	42.893402
3527.594252	730044.602000	42.898407
3527.315453	729468.433999	42.903412
3527.261801	728880.004370	42.908417
3527.148230	728300.555785	42.913421
3527.128335	727736.898892	42.918426
3526.906514	727147.381885	42.923431
3526.965599	726574.665777	42.928436
3526.659872	726005.934830	42.933441
3526.965170	725438.447143	42.938445
3526.427766	724880.428051	42.943450
3527.015353	724293.935976	42.948455
3526.728962	723734.854598	42.953460
3526.650872	723168.414891	42.958465
3526.588594	722597.324458	42.963469
3526.567782	722029.508043	42.968474
3526.679778	721456.474985	42.973479
3526.760339	720887.224388	42.978484
3526.351589	720334.228477	42.983489
3526.629172	719758.670009	42.988493
3526.685594	719198.181578	42.993498
3526.741499	718636.514997	42.998503
3526.588483	718059.920645	43.003508
3526.286800	717505.379199	43.008513
3526.464823	716937.675998	43.013517
3525.953084	716372.878956	43.018522
3526.191392	715809.056502	43.023527
3526.248965	715260.901513	43.028532
3525.939030	714700.223031	43.033537
3525.981078	714144.507195	43.038541
3525.980092	713587.571264	43.043546
3526.003718	713035.555907	43.048551
3526.237637	712476.422545	43.053556
3526.002921	711925.470284	43.058561
3526.413287	711359.781951	43.063565
3525.976925	710808.741754	43.068570
3526.216406	710250.998863	43.073575
3526.133988	709688.856700	43.078580
3525.673160	709137.265437	43.083585
3525.785673	708583.753421	43.088589
3525.673562	708032.577147	43.093594
3525.799231	707475.168252	43.098599
3525.733038	706927.388227	43.103604
3525.836169	706381.878023	43.108609
3525.478212	705824.295213	43.113613
3525.572773	705277.375450	43.118618
3525.571983	704727.357959	43.123623
3525.470251	704171.263081	43.128628
3525.582694	703631.934204	43.133633
3525.398285	703084.624784	43.138637
3525.097253	702552.054719	43.143642
3525.474050	702002.544243	43.148647
3525.501352	701458.722498	43.153652
3525.396987	700911.858272	43.158657
3525.352726	700361.620160	43.163661
3525.392096	699816.202865	43.168666
3524.937752	699282.315450	43.173671
3525.402598	698737.801673	43.178676
3525.232948	698199.227121	43.183681
3525.378705	697655.893293	43.188685
3525.115659	697112.247604	43.193690
3525.144989	696563.398050	43.198695
3524.927387	696028.774651	43.203700
3524.670077	695497.058855	43.208705
3524.956989	694953.185738	43.213709
3525.038450	694419.258841	43.218714
3524.772079	693886.552484	43.223719
3524.950372	693354.782442	43.228724
3524.680468	692815.000356	43.233729
3524.704822	692281.551039	43.238733
3524.508041	691755.966083	43.243738
3524.759100	691219.628981	43.248743
3524.896319	690692.183237	43.253748
3524.558044	690166.677867	43.258753
3524.773457	689620.549986	43.263757
3524.569685	689094.112819	43.268762
3524.841151	688576.917695	43.273767
3525.116281	688027.995673	43.278772
3525.024370	687504.829711	43.283777
3524.704735	686957.635742	43.288781
3524.774775	686414.522495	43.293786
3524.754395	685877.862191	43.298791
3524.795590	685357.186648	43.303796
3524.454412	684833.808682	43.308801
3524.667633	684291.986918	43.313805
3524.483626	683771.607088	43.318810
3524.037673	683248.304809	43.323815
3524.159244	682718.403037	43.328820
3524.127271	682204.877911	43.333825
3524.260437	681680.639767	43.338829
3523.959261	681166.355223	43.343834
3523.910656	680639.100528	43.348839
3523.965248	680120.712479	43.353844
3523.750313	679600.747355	43.358849
3524.048759	679081.611477	43.363853
3524.405495	678564.129897	43.368858
3523.940985	678043.770607	43.373863
3524.345455	677523.980819	43.378868
3524.025398	677001.346111	43.383873
3523.809118	676475.575149	43.388877
3523.713014	675964.352494	43.393882
3523.489150	675440.915663	43.398887
3523.869960	674928.508096	43.403892
3523.555322	674420.576323	43.408897
3523.498893	673905.844884	43.413901
3523.673060	673388.852733	43.418906
3523.675505	672891.249557	43.423911
3523.905805	672368.708782	43.428916
3523.378788	671861.620949	43.433921
3523.693318	671352.467702	43.438925
3523.489650	670846.864945	43.443930
3523.717423	670327.501055	43.448935
3523.735468	669817.716973	43.453940
3523.263018	669307.789593	43.458945
3523.612049	668796.746989	43.463949
3523.053368	668290.868144	43.468954
3523.011474	667784.225709	43.473959
3523.212523	667282.451926	43.478964
3523.104744	666780.105833	43.483969
3523.109323	666279.609277	43.488973
3523.064321	665782.586365	43.493978
3523.182684	665289.300609	43.498983
3523.605198	664769.648448	43.503988
3522.771638	664275.574869	43.508993
3523.198190	663767.141900	43.513997
3523.042436	663276.642705	43.519002
3522.493098	662772.664160	43.524007
3522.780839	662279.892801	43.529012
3522.588204	661782.138315	43.534017
3522.848773	661287.025336	43.539021
3523.003329	660788.960632	43.544026
3523.002725	660303.523302	43.549031
3523.334347	659794.646981	43.554036
3522.971542	659304.130484	43.559041
3522.818775	658802.571954	43.564045
3522.606467	658299.300453	43.569050
3522.463264	657817.606565	43.574055
3522.710681	657322.792299	43.579060
3522.652993	656838.139823	43.584065
3522.432805	656336.016283	43.589069
3522.683029	655850.363491	43.594074
3522.402875	655366.474849	43.599079
3522.736206	654872.021086	43.604084
3522.300875	654388.360312	43.609089
3522.391383	653886.257859	43.614093
3522.407913	653398.426045	43.619098
3522.141908	652923.204494	43.624103
3522.421612	652430.834721	43.629108
3522.210053	651954.907911	43.634113
3522.242357	651455.938378	43.639117
3522.053148	650981.809178	43.644122
3521.911958	650500.355317	43.649127
3522.443594	650014.916324	43.654132
3522.085362	649539.098385	43.659137
3522.476787	649060.981225	43.664141
3522.803914	648579.854087	43.669146
3522.347189	648091.991758	43.674151
3522.314950	647587.442433	43.679156
3521.893313	647118.066190	43.684161
3521.781595	646627.624799	43.689165
3521.561890	646161.767634	43.694170
3521.789481	645680.967996	43.699175
3522.189006	645189.269514	43.704180
3521.727198	644722.537301	43.709185
3521.736737	644236.807308	43.714189
3521.726551	643760.355662	43.719194
3521.632972	643289.545061	43.724199
3521.556270	642815.409974	43.729204
3521.708292	642357.513018	43.734209
3521.772161	641876.160337	43.739213
3521.596294	641406.376415	43.744218
3521.530912	640935.701866	43.749223
3521.490303	640463.151089	43.754228
3521.987274	639997.838065	43.759233
3521.831016	639516.011452	43.764237
3521.671868	639054.268359	43.769242
3521.518139	638569.595998	43.774247
3521.490695	638097.383899	43.779252
3521.600360	637636.281397	43.784257
3521.592267	637165.173676	43.789261
3521.478352	636694.112508	43.794266
3521.199727	636242.969046	43.799271
3521.619740	635761.768621	43.804276
3521.384939	635296.567928	43.809281
3521.203302	634834.889726	43.814285
3521.541813	634360.392803	43.819290
3521.177006	633895.902042	43.824295
3521.390728	633435.795487	43.829300
3521.057722	632970.557417	43.834305
3520.998139	632509.105437	43.839309
3521.044242	632052.719918	43.844314
3520.712594	631596.879475	43.849319
3521.000108	631135.207506	43.854324
3520.819056	630684.757374	43.859329
3520.920502	630222.376245	43.864333
3520.668241	629777.105248	43.869338
3520.545780	629327.187641	43.874343
3520.800540	628870.327775	43.879348
3520.466343	628426.866053	43.884353
3520.880716	627966.635541	43.889357
3520.654953	627517.860101	43.894362
3520.394872	627073.978532	43.899367
3520.607165	626613.423318	43.904372
3520.367979	626181.718878	43.909377
3520.397084	625721.657063	43.914381
3520.077096	625282.518393	43.919386
3520.008425	624840.413966	43.924391
3520.268111	624398.335343	43.929396
3520.011100	623960.934599	43.934401
3520.221494	623522.885211	43.939405
3520.136218	623087.623376	43.944410
3520.165729	622648.867916	43.949415
3520.483563	622208.642677	43.954420
3520.121176	621769.968364	43.959425
3520.307516	621326.823932	43.964429
3520.300117	620881.189348	43.969434
3520.186900	620441.817283	43.974439
3520.368453	620002.326941	43.979444
3520.274002	619570.832858	43.984449
3520.270045	619114.752877	43.989453
3520.401143	618675.167269	43.994458
3520.162983	618238.984496	43.999463
3520.147130	617791.771139	44.004468
3519.579521	617358.215323	44.009473
3519.546729	616920.641700	44.014477
3519.652742	616499.767230	44.019482
3519.570963	616075.249679	44.024487
3519.633679	615646.380289	44.029492
3519.445962	615222.750068	44.034497
3519.552170	614795.694714	44.039501
3519.431756	614371.168003	44.044506
3519.233765	613955.912675	44.049511
3519.510530	613524.266996	44.054516
3519.353598	613101.101395	44.059521
3519.652454	612674.582798	44.064525
3519.237339	612253.685086	44.069530
3519.120558	611833.472586	44.074535
3519.670761	611419.949877	44.079540
3519.196480	611002.675327	44.084545
3519.220939	610576.825017	44.089549
3519.220612	610157.783010	44.094554
3519.264551	609751.155264	44.099559
3519.386221	609319.974485	44.104564
3519.106734	608912.418533	44.109569
3519.198840	608492.997403	44.114573
3519.121831	608071.081513	44.119578
3518.884630	607656.701237	44.124583
3518.985017	607234.874139	44.129588
3518.890383	606843.263548	44.134593
3519.062048	606425.958948	44.139597
3518.671939	606015.607861	44.144602
3518.353323	605597.352981	44.149607
3518.895970	605194.940384	44.154612
3518.675226	604791.941402	44.159617
3518.477441	604387.519269	44.164621
3518.698456	603985.720792	44.169626
3518.705695	603588.259996	44.174631
3518.919077	603170.878600	44.179636
3518.684269	602769.566650	44.184641
3518.547512	602370.482133	44.189645
3518.642462	601954.280885	44.194650
3518.171899	601558.236166	44.199655
3518.447713	601153.216966	44.204660
3518.331959	600756.983603	44.209665
3518.241576	600361.234164	44.214669
3518.254822	599968.414899	44.219674
3518.618461	599573.263568	44.224679
3518.753129	599161.321397	44.229684
3518.370011	598767.223713	44.234689
3518.265932	598366.388123	44.239693
3518.625519	597969.525959	44.244698
3518.555876	597583.567783	44.249703
3518.522658	597172.185910	44.254708
3518.341947	596775.274718	44.259713
3517.990094	596381.241179	44.264717
3518.135391	595985.904334	44.269722
3517.948074	595594.427107	44.274727
3518.136234	595196.947231	44.279732
3517.998029	594806.941680	44.284737
3517.859717	594417.425332	44.289741
3518.276157	594034.832166	44.294746
3517.631128	593634.629156	44.299751
3517.757705	593251.959515	44.304756
3518.174428	592877.113256	44.309761
3517.467594	592484.214517	44.314765
3517.851229	592105.532105	44.319770
3517.432992	591722.805344	44.324775
3517.963553	591345.881777	44.329780
3517.522918	590967.002214	44.334785
3517.791771	590579.399203	44.339789
3517.593859	590193.521027	44.344794
3517.629989	589814.121328	44.349799
3517.766784	589435.596652	44.354804
3517.484861	589059.593258	44.359809
3517.451623	588670.824036	44.364813
3517.472064	588295.900524	44.369818
3517.581482	587926.477142	44.374823
3517.441006	587538.292321	44.379828
3517.417914	587166.204953	44.384833
3517.661020	586792.754062	44.389837
3517.413382	586415.505891	44.394842
3517.691542	586038.658646	44.399847
3517.521688	585659.664837	44.404852
3517.466839	585293.505336	44.409857
3517.774662	584913.250587	44.414861
3517.502765	584528.609664	44.419866
3517.557603	584153.249455	44.424871
3517.606878	583765.061341	44.429876
3517.302225	583405.522102	44.434881
3517.286356	583023.152113	44.439885
3517.561063	582644.993281	44.444890
3517.218431	582272.357236	44.449895
3517.336488	581896.061866	44.454900
3517.121351	581533.687085	44.459905
3517.094997	581156.740024	44.464909
3517.169307	580789.165750	44.469914
3516.792480	580427.791303	44.474919
3517.023186	580055.140555	44.479924
3516.680716	579690.772058	44.484929
3516.733924	579338.493408	44.489933
3517.004678	578975.155479	44.494938
3516.937268	578617.245040	44.499943
3516.871423	578250.423271	44.504948
3516.905754	577878.997305	44.509953
3516.963460	577515.652760	44.514957
3517.186061	577165.093528	44.519962
3517.092396	576793.003031	44.524967
3517.250642	576432.677379	44.529972
3517.088275	576062.638749	44.534977
3516.915919	575690.075975	44.539981
3517.260045	575337.231335	44.544986
3516.875048	574977.459256	44.549991
3517.348813	574611.343155	44.554996
3517.298593	574248.323937	44.560001
3516.671864	573869.546857	44.565005
3517.091961	573496.767164	44.570010
3516.738039	573138.647258	44.575015
3516.832955	572780.742350	44.580020
3516.621960	572421.269564	44.585025
3516.428875	572062.135629	44.590029
3516.331000	571707.553651	44.595034
3516.328217	571350.178194	44.600039
3516.888249	570996.923034	44.605044
3516.534596	570654.430868	44.610049
3516.817654	570298.939252	44.615053
3516.721058	569937.514442	44.620058
3516.462262	569594.222626	44.625063
3516.088929	569226.937265	44.630068
3515.630681	568876.463988	44.635073
3515.661230	568532.037291	44.640077
3516.198524	568196.875521	44.645082
3516.338899	567849.895328	44.650087
3516.021312	567499.863485	44.655092
3516.047001	567168.687788	44.660097
3515.904684	566818.657721	44.665101
3515.954965	566471.806550	44.670106
3515.813505	566134.542342	44.675111
3515.692542	565802.198711	44.680116
3515.651293	565464.849492	44.685121
3515.514354	565119.755624	44.690125
3515.760009	564790.847013	44.695130
3515.466871	564456.434138	44.700135
3515.920493	564112.320024	44.705140
3515.474511	563786.121751	44.710145
3515.610026	563459.262183	44.715149
3515.630573	563126.070362	44.720154
3515.176243	562796.827843	44.725159
3515.459248	562469.213308	44.730164
3515.143184	562144.361372	44.735169
3515.350544	561820.821809	44.740173
3515.254100	561491.887998	44.745178
3515.207289	561173.763534	44.750183
3515.462595	560835.790142	44.755188
3515.331472	560521.138715	44.760193
3515.429961	560197.728646	44.765197
3515.466459	559859.666724	44.770202
3515.175029	559544.918531	44.775207
3515.687970	559216.881128	44.780212
3515.381890	558898.493942	44.785217
3515.353349	558565.446133	44.790221
3514.934107	558239.306293	44.795226
3514.890775	557917.224263	44.800231
3515.162991	557600.721690	44.805236
3514.867351	557285.164774	44.810241
3514.793282	556963.870696	44.815245
3515.020844	556648.964860	44.820250
3515.061529	556345.115028	44.825255
3514.971528	556011.660878	44.830260
3514.770957	555702.497948	44.835265
3514.708080	555394.009599	44.840269
3514.539273	555079.235053	44.845274
3514.633211	554764.357849	44.850279
3514.910350	554456.746986	44.855284
3514.480334	554156.756514	44.860289
3514.751634	553852.105219	44.865293
3514.796061	553536.048806	44.870298
3514.413252	553235.173145	44.875303
3514.753170	552921.067179	44.880308
3514.533184	552617.126772	44.885313
3514.770673	552306.147911	44.890317
3515.224875	551995.477602	44.895322
3514.689186	551686.531244	44.900327
3515.136466	551366.071998	44.905332
3514.983538	551062.891407	44.910337
3514.975352	550750.356542	44.915341
3514.344651	550431.671831	44.920346
3514.162221	550138.856896	44.925351
3514.271841	549828.346910	44.930356
3514.539160	549531.359962	44.935361
3514.420778	549232.416433	44.940365
3514.713154	548928.860205	44.945370
3513.927687	548620.995541	44.950375
3514.437909	548315.372433	44.955380
3514.340972	548024.816007	44.960385
3514.136721	547723.535565	44.965389
3514.269730	547421.081992	44.970394
3513.754433	547137.181325	44.975399
3514.123181	546836.942941	44.980404
3513.935694	546543.295727	44.985409
3513.637459	546262.767749	44.990413
3513.991705	545964.226750	44.995418
3513.613639	545676.138809	45.000423
3513.713562	545379.342595	45.005428
3513.718201	545103.629423	45.010433
3513.706512	544811.780677	45.015437
3513.856574	544527.964773	45.020442
3513.480180	544247.812576	45.025447
3513.793038	543952.461960	45.030452
3513.827990	543671.370791	45.035457
3513.732125	543388.027360	45.040461
3513.779929	543101.527505	45.045466
3513.178100	542824.813792	45.050471
3513.612547	542533.597391	45.055476
3513.362759	542263.064948	45.060481
3513.459643	541987.879363	45.065485
3513.348379	541703.344584	45.070490
3513.249588	541430.652357	45.075495
3513.021173	541157.825674	45.080500
3513.212165	540894.402811	45.085505
3513.078470	540619.330603	45.090509
3513.339192	540332.989906	45.095514
3512.883038	540069.056905	45.100519
3513.090261	539798.045900	45.105524
3513.233202	539534.504939	45.110529
3512.787451	539261.678623	45.115533
3513.008326	538984.698325	45.120538
3513.118811	538734.362278	45.125543
3512.912569	538460.319564	45.130548
3512.991210	538201.657259	45.135553
3512.895834	537921.179446	45.140557
3513.190792	537666.354340	45.145562
3512.674875	537398.800447	45.150567
3512.915278	537134.088518	45.155572
3512.792923	536870.291153	45.160577
3512.532299	536614.230548	45.165581
3512.285941	536348.326030	45.170586
3512.588964	536087.165629	45.175591
3512.773481	535820.471479	45.180596
3512.666312	535578.794089	45.185601
3512.770322	535322.900354	45.190605
3512.949098	535050.845253	45.195610
3512.803635	534799.172139	45.200615
3512.691183	534539.013058	45.205620
3512.709880	534282.560392	45.210625
3512.498614	534028.564202	45.215629
3512.700378	533769.094373	45.220634
3512.730670	533522.868502	45.225639
3512.744736	533254.793587	45.230644
3512.673881	533002.571806	45.235649
3512.265338	532745.660215	45.240653
3512.436423	532491.470811	45.245658
3512.042740	532246.708472	45.250663
3512.232423	531994.424662	45.255668
3512.378169	531745.272600	45.260673
3512.329794	531502.810468	45.265677
3512.544931	531254.142774	45.270682
3512.180732	531002.642826	45.275687
3512.565597	530745.005294	45.280692
3512.430473	530506.124421	45.285697
3512.420980	530255.762225	45.290701
3512.582674	529996.181390	45.295706
3512.138909	529745.884616	45.300711
3512.308654	529497.649001	45.305716
3512.405578	529258.052039	45.310721
3512.484707	529017.949494	45.315725
3512.577220	528762.800102	45.320730
3511.813279	528511.376085	45.325735
3512.346196	528258.313084	45.330740
3512.176718	528025.706904	45.335745
3511.988190	527782.399541	45.340749
3511.999419	527538.902633	45.345754
3511.924994	527302.886931	45.350759
3512.056953	527057.948134	45.355764
3511.771734	526824.787554	45.360769
3511.991405	526583.308956	45.365773
3512.140738	526338.860104	45.370778
3511.802591	526108.069864	45.375783
3511.826792	525863.230701	45.380788
3511.887672	525633.122186	45.385793
3511.899780	525400.393303	45.390797
3511.988137	525158.409151	45.395802
3511.915330	524923.869895	45.400807
3511.727260	524685.105822	45.405812
3511.793756	524458.259803	45.410817
3511.347850	524225.287881	45.415821
3511.633715	523996.327420	45.420826
3511.681554	523763.415475	45.425831
3511.743172	523518.783933	45.430836
3511.677234	523286.590869	45.435841
3511.121643	523069.069812	45.440845
3511.862054	522841.680347	45.445850
3511.473851	522613.167334	45.450855
3511.696428	522382.981268	45.455860
3511.580941	522151.637545	45.460865
3511.534413	521925.025044	45.465869
3511.499701	521695.225884	45.470874
3511.394092	521480.634825	45.475879
3511.807429	521250.802910	45.480884
3511.794226	521020.131370	45.485889
3511.750360	520796.026414	45.490893
3511.971352	520562.681987	45.495898
3511.795782	520331.472202	45.500903
3511.893904	520096.929591	45.505908
3511.359726	519862.996342	45.510913
3511.242320	519639.795928	45.515917
3510.804894	519418.515513	45.520922
3510.867683	519207.752359	45.525927
3510.962418	518990.768742	45.530932
3510.909421	518774.615357	45.535937
3510.927128	518555.972035	45.540941
3511.199273	518349.757383	45.545946
3510.523937	518138.095374	45.550951
3510.743675	517918.095253	45.555956
3510.946609	517705.570201	45.560961
3510.933903	517495.402478	45.565965
3510.740198	517279.252034	45.570970
3510.606058	517078.140723	45.575975
3510.920167	516860.988500	45.580980
3510.754236	516659.978180	45.585985
3510.561938	516448.564017	45.590989
3510.899930	516236.096651	45.595994
3510.659630	516033.979569	45.600999
3510.686961	515826.914168	45.606004
3510.692628	515631.417844	45.611009
3510.680945	515419.049477	45.616013
3510.773215	515205.801656	45.621018
3510.413595	515012.481621	45.626023
3510.991980	514796.114096	45.631028
3510.828471	514596.996279	45.636033
3510.607134	514393.288470	45.641037
3510.899956	514179.285041	45.646042
3510.520844	513966.454347	45.651047
3510.283907	513774.613618	45.656052
3510.566556	513572.425728	45.661057
3510.313211	513372.095052	45.666061
3510.379708	513167.160044	45.671066
3510.182751	512977.525750	45.676071
3510.498137	512778.707152	45.681076
3510.479931	512580.801927	45.686081
3510.269559	512381.411222	45.691085
3510.668950	512184.793915	45.696090
3510.148390	511989.442830	45.701095
3510.266798	511790.544289	45.706100
3510.323550	511590.238949	45.711105
3510.346588	511394.585543	45.716109
3510.543364	511200.870723	45.721114
3509.744705	511013.589310	45.726119
3510.118567	510818.374161	45.731124
3510.291610	510623.342485	45.736129
3509.755063	510428.025296	45.741133
3510.082205	510240.491959	45.746138
3510.019617	510062.422250	45.751143
3510.199328	509871.675550	45.756148
3509.850878	509685.969173	45.761153
3509.665861	509494.926469	45.766157
3510.062370	509313.788360	45.771162
3509.739669	509129.940922	45.776167
3509.943587	508935.540188	45.781172
3510.172860	508757.001704	45.786177
3510.107400	508577.399692	45.791181
3510.157443	508386.606772	45.796186
3510.010658	508200.090521	45.801191
3510.050161	508004.341929	45.806196
3509.966745	507824.481804	45.811201
3509.905740	507634.861305	45.816205
3510.243685	507444.361766	45.821210
3510.001475	507275.237520	45.826215
3510.377397	507072.647361	45.831220
3510.050481	506884.074242	45.836225
3509.692425	506699.851054	45.841229
3509.446175	506513.635402	45.846234
3509.802253	506334.896604	45.851239
3509.830525	506151.915360	45.856244
3509.795854	505976.019338	45.861249
3509.624296	505807.423586	45.866253
3510.026661	505614.465082	45.871258
3509.532150	505440.158164	45.876263
3509.745422	505257.741765	45.881268
3509.798437	505085.662792	45.886273
3509.688767	504904.712937	45.891277
3509.601603	504726.284752	45.896282
3509.559174	504555.277999	45.901287
3509.699382	504364.219735	45.906292
3509.791757	504194.955480	45.911297
3509.469681	504022.272073	45.916301
3509.890509	503837.630470	45.921306
3509.682258	503659.565100	45.926311
3509.668262	503487.986155	45.931316
3509.685866	503319.534423	45.936321
3509.558831	503137.758953	45.941325
3510.017285	502957.903738	45.946330
3509.853279	502786.696916	45.951335
3509.750476	502608.096481	45.956340
3509.481485	502426.590113	45.961345
3509.590970	502253.308688	45.966349
3509.675826	502078.108393	45.971354
3509.521867	501913.261133	45.976359
3509.792910	501733.879491	45.981364
3509.576507	501556.399295	45.986369
3509.549643	501384.699342	45.991373
3509.740834	501205.982859	45.996378
3509.448350	501052.880900	46.001383
3509.643421	500871.227513	46.006388
3509.819695	500701.053178	46.011393
3509.692192	500521.625228	46.016397
3509.695598	500336.105257	46.021402
3509.500374	500177.871559	46.026407
3509.270383	499996.786758	46.031412
3509.263246	499837.051284	46.036417
3509.047052	499661.219295	46.041421
3509.178318	499493.517948	46.046426
3509.072938	499328.636515	46.051431
3509.380845	499161.407319	46.056436
3509.367121	498997.265458	46.061441
3509.162655	498840.284753	46.066445
3509.267268	498666.865311	46.071450
3509.100248	498512.656432	46.076455
3509.204171	498347.476662	46.081460
3509.062770	498188.456215	46.086465
3509.105929	498024.446744	46.091469
3509.349642	497858.024537	46.096474
3509.292970	497696.506905	46.101479
3509.388395	497527.527530	46.106484
3509.478423	497359.204820	46.111489
3509.166544	497196.916754	46.116493
3509.555907	497016.452324	46.121498
3509.381226	496853.581181	46.126503
3509.766098	496690.056585	46.131508
3509.430924	496515.981819	46.136513
3509.335599	496344.696573	46.141517
3509.355550	496183.808746	46.146522
3509.081219	496020.541907	46.151527
3509.339608	495853.136291	46.156532
3509.132189	495692.788362	46.161537
3508.968399	495537.287028	46.166541
3508.803180	495368.583288	46.171546
3508.893690	495217.840625	46.176551
3508.796585	495050.234825	46.181556
3508.848904	494897.523186	46.186561
3508.495713	494752.061940	46.191565
3508.819144	494595.962923	46.196570
3508.780355	494453.126252	46.201575
3508.507743	494291.511578	46.206580
3508.579072	494130.595382	46.211585
3508.513766	493985.432469	46.216589
3508.846631	493820.270238	46.221594
3508.279221	493685.509623	46.226599
3508.684182	493534.698271	46.231604
3508.956895	493385.476306	46.236609
3508.996077	493232.397802	46.241613
3509.231533	493071.291783	46.246618
3508.428008	492927.763461	46.251623
3508.645114	492768.630591	46.256628
3508.570155	492614.554277	46.261633
3508.327232	492476.946358	46.266637
3508.677763	492326.538305	46.271642
3508.942999	492185.047135	46.276647
3508.634589	492029.285375	46.281652
3508.661574	491881.609883	46.286657
3508.743423	491734.834373	46.291661
3508.923911	491576.253140	46.296666
3508.599063	491422.512288	46.301671
3508.398412	491267.939386	46.306676
3508.512877	491127.982971	46.311681
3508.494889	490986.327888	46.316685
3508.553965	490840.054531	46.321690
3508.583737	490698.945445	46.326695
3508.378163	490543.658557	46.331700
3508.468651	490401.777761	46.336705
3508.013608	490253.057487	46.341709
3508.395413	490114.767396	46.346714
3508.165092	489972.128317	46.351719
3508.089040	489835.077853	46.356724
3508.021033	489691.396824	46.361729
3507.873601	489558.201661	46.366733
3508.090559	489424.791464	46.371738
3508.194934	489290.640499	46.376743
3508.147264	489147.204461	46.381748
3508.584432	489010.363417	46.386753
3508.205142	488876.342424	46.391757
3508.489971	488733.605169	46.396762
3508.060649	488603.790328	46.401767
3508.266790	488461.266666	46.406772
3508.423250	488326.340350	46.411777
3508.056060	488198.181674	46.416781
3508.155465	488046.058720	46.421786
3508.125222	487914.146543	46.426791
3508.248721	487777.501150	46.431796
3507.906477	487643.261909	46.436801
3507.869968	487513.979085	46.441805
3508.164509	487372.544672	46.446810
3507.995434	487249.911515	46.451815
3507.941308	487113.645472	46.456820
3508.171447	486974.647812	46.461825
3507.784921	486852.251407	46.466829
3508.076379	486718.757131	46.471834
3507.941715	486580.931937	46.476839
3508.086234	486449.383697	46.481844
3508.290297	486314.585517	46.486849
3507.641534	486179.527064	46.491853
3507.921293	486050.027600	46.496858
3507.806393	485931.626926	46.501863
3508.016047	485785.740763	46.506868
3508.098290	485665.179115	46.511873
3507.703943	485540.902396	46.516877
3507.887643	485401.647160	46.521882
3507.801423	485281.314080	46.526887
3507.710839	485144.381048	46.531892
3508.017042	485019.930427	46.536897
3507.680690	484898.675858	46.541901
3507.767584	484761.911992	46.546906
3507.738516	484643.589223	46.551911
3507.570513	484514.104309	46.556916
3507.965498	484394.087906	46.561921
3507.724129	484266.891227	46.566925
3507.932903	484135.415956	46.571930
3508.035976	484013.371710	46.576935
3507.723609	483881.932926	46.581940
3507.652869	483761.688079	46.586945
3507.674300	483636.162854	46.591949
3507.998692	483506.384044	46.596954
3507.762614	483389.809122	46.601959
3507.947598	483263.645966	46.606964
3507.877618	483140.612970	46.611969
3507.748930	483015.969453	46.616973
3507.414125	482893.030578	46.621978
3507.540926	482774.921806	46.626983
3507.794057	482644.895799	46.631988
3507.922666	482523.393744	46.636993
3507.562382	482400.152116	46.641997
3507.662473	482266.606276	46.647002
3507.540748	482149.396296	46.652007
3507.507218	482025.083929	46.657012
3507.476772	481917.676791	46.662017
3507.222451	481802.916872	46.667021
3507.145088	481680.938067	46.672026
3507.003609	481568.485863	46.677031
3507.681276	481452.045976	46.682036
3507.598255	481337.658786	46.687041
3507.356485	481219.248326	46.692045
3507.490504	481103.607691	46.697050
3507.468796	480983.943202	46.702055
3507.309890	480871.084632	46.707060
3507.542790	480757.652235	46.712065
3507.658914	480642.315419	46.717069
3507.464457	480520.551209	46.722074
3507.189148	480408.823308	46.727079
3507.423285	480293.514730	46.732084
3507.350202	480177.802258	46.737089
3507.243106	480073.738329	46.742093
3507.302103	479956.685668	46.747098
3507.172155	479847.359425	46.752103
3506.863682	479731.937407	46.757108
3507.067225	479624.729738	46.762113
3506.972969	479523.444822	46.767117
3507.249691	479411.616489	46.772122
3507.210187	479305.511567	46.777127
3506.988535	479186.375546	46.782132
3507.157553	479082.765028	46.787137
3506.889507	478978.671649	46.792141
3507.241408	478871.940462	46.797146
3507.334142	478766.214819	46.802151
3506.834428	478653.501832	46.807156
3507.518502	478546.306991	46.812161
3507.122480	478439.954109	46.817165
3507.556647	478326.927754	46.822170
3507.449790	478231.004410	46.827175
3507.450139	478115.519366	46.832180
3507.722694	477997.253115	46.837185
3507.281405	477883.310264	46.842189
3507.435805	477767.847343	46.847194
3507.113014	477652.870213	46.852199
3506.940199	477551.283926	46.857204
3507.006942	477437.859116	46.862209
3506.821403	477330.704347	46.867213
3506.958306	477223.443262	46.872218
3506.853641	477124.526448	46.877223
3506.938432	477022.336282	46.882228
3507.130469	476917.848768	46.887233
3506.694123	476825.518572	46.892237
3507.014013	476721.514435	46.897242
3507.046195	476620.242405	46.902247
3506.868694	476516.929635	46.907252
3507.018789	476411.585623	46.912257
3506.970694	476298.882239	46.917261
3507.062463	476195.926760	46.922266
3506.881152	476102.637953	46.927271
3506.732533	475992.836041	46.932276
3507.031604	475886.045793	46.937281
3506.573085	475797.562500	46.942285
3506.610371	475695.423691	46.947290
3506.704646	475604.363919	46.952295
3506.744805	475505.717466	46.957300
3506.663042	475398.584325	46.962305
3506.424116	475305.301313	46.967309
3506.665947	475214.619517	46.972314
3506.361139	475120.789810	46.977319
3506.560588	475023.379518	46.982324
3506.272923	474927.115283	46.987329
3506.331819	474841.273506	46.992333
3506.351820	474744.398766	46.997338
3506.409298	474660.379380	47.002343
3506.210204	474565.921137	47.007348
3506.257149	474476.281777	47.012353
3506.026524	474394.943621	47.017357
3506.424194	474301.243006	47.022362
3506.347173	474222.561775	47.027367
3506.186011	474135.690860	47.032372
3506.254815	474047.261058	47.037377
3506.089496	473965.707305	47.042381
3506.521573	473869.567881	47.047386
3506.471996	473782.980108	47.052391
3506.487063	473691.620597	47.057396
3506.331588	473591.883232	47.062401
3506.105289	473520.010501	47.067405
3506.654878	473431.191823	47.072410
3506.121782	473344.228784	47.077415
3505.803321	473250.493219	47.082420
3506.335404	473167.601463	47.087425
3506.080524	473091.629883	47.092429
3506.284621	473006.463831	47.097434
3506.520052	472915.670606	47.102439
3505.791267	472828.029558	47.107444
3505.987673	472755.170111	47.112449
3505.760429	472683.750109	47.117453
3505.979988	472597.060222	47.122458
3506.041631	472525.691579	47.127463
3505.736169	472447.244424	47.132468
3506.303324	472365.153436	47.137473
3506.094700	472284.156809	47.142477
3506.325388	472192.702492	47.147482
3506.248188	472111.024284	47.152487
3505.871143	472033.803115	47.157492
3505.981867	471952.801172	47.162497
3505.822720	471870.072335	47.167501
3505.950112	471792.257576	47.172506
3505.636143	471723.431691	47.177511
3505.674469	471643.909532	47.182516
3506.158884	471567.197760	47.187521
3505.714774	471490.897454	47.192525
3505.871717	471412.772191	47.197530
3505.639031	471348.945167	47.202535
3505.621644	471270.798432	47.207540
3505.611186	471194.574821	47.212545
3505.729882	471134.840227	47.217549
3506.144021	471056.720218	47.222554
3505.767744	470983.242588	47.227559
3505.554755	470910.496524	47.232564
3506.016454	470831.911621	47.237569
3505.702984	470760.043169	47.242573
3505.592967	470682.973446	47.247578
3505.553656	470618.756380	47.252583
3505.841241	470543.745490	47.257588
3505.735723	470477.513248	47.262593
3505.775482	470419.360019	47.267597
3505.841540	470334.762563	47.272602
3505.918394	470263.230775	47.277607
3505.819293	470184.333725	47.282612
3505.774485	470106.541401	47.287617
3505.752058	470041.914281	47.292621
3505.642649	469966.867582	47.297626
3505.933889	469905.934652	47.302631
3505.764138	469834.696607	47.307636
3506.061291	469766.113784	47.312641
3505.981485	469696.885946	47.317645
3505.886410	469609.273623	47.322650
3505.995228	469539.658436	47.327655
3505.916155	469466.377417	47.332660
3505.778357	469378.112834	47.337665
3505.905910	469324.246760	47.342669
3505.858770	469245.083658	47.347674
3505.878878	469175.836857	47.352679
3506.038932	469108.034868	47.357684
3506.342265	469024.201506	47.362689
3505.871912	468953.669980	47.367693
3505.794324	468882.716548	47.372698
3505.664670	468806.959554	47.377703
3505.669546	468736.599351	47.382708
3505.691778	468668.059504	47.387713
3505.857130	468599.748250	47.392717
3505.477617	468528.237185	47.397722
3505.488068	468469.373805	47.402727
3505.477271	468399.876178	47.407732
3505.727637	468333.525025	47.412737
3505.424914	468269.243664	47.417741
3505.405578	468197.973798	47.422746
3505.443927	468143.916990	47.427751
3505.370289	468084.306933	47.432756
3505.729569	468010.185608	47.437761
3505.442505	467951.928654	47.442765
3505.300073	467879.513508	47.447770
3505.566964	467822.124057	47.452775
3505.276539	467758.497419	47.457780
3505.402758	467692.266552	47.462785
3504.950565	467633.783534	47.467789
3505.216271	467577.862626	47.472794
3505.250789	467519.802735	47.477799
3505.378938	467459.801669	47.482804
3505.466789	467391.549984	47.487809
3505.025351	467347.501884	47.492813
3505.315093	467284.585144	47.497818
3505.444932	467221.695501	47.502823
3504.717203	467174.656356	47.507828
3505.321294	467110.469557	47.512833
3504.745243	467061.479189	47.517837
3505.418122	466986.895085	47.522842
3505.710321	466948.698614	47.527847
3505.396164	466888.011388	47.532852
3505.350209	466826.670258	47.537857
3505.374014	466777.323441	47.542861
3505.236266	466708.601247	47.547866
3505.303872	466649.773169	47.552871
3504.960941	466594.763885	47.557876
3505.534200	466539.040740	47.562881
3505.456444	466487.633436	47.567885
3505.237895	466424.952652	47.572890
3505.318958	466360.447369	47.577895
3505.312053	466301.073676	47.582900
3505.282070	466242.666307	47.587905
3505.176085	466189.895169	47.592909
3505.097433	466138.537746	47.597914
3505.070311	466079.065497	47.602919
3505.064227	466035.446667	47.607924
3505.335657	465966.601295	47.612929
3505.293549	465920.353925	47.617933
3505.044958	465857.423113	47.622938
3505.205804	465812.610041	47.627943
3505.161553	465756.534111	47.632948
3506.061130	465689.252366	47.637953
3505.751827	465634.943877	47.642957
3505.785461	465561.223352	47.647962
3505.824915	465509.742763	47.652967
3505.328785	465445.586291	47.657972
3505.826411	465381.209262	47.662977
3505.667499	465320.034613	47.667981
3505.478433	465250.606689	47.672986
3505.221931	465197.047913	47.677991
3504.812463	465133.990220	47.682996
3504.895665	465084.223615	47.688001
3505.120416	465043.602998	47.693005
3504.981625	464971.885586	47.698010
3505.123749	464930.265545	47.703015
3505.267303	464881.248087	47.708020
3505.214530	464816.507176	47.713025
3505.103047	464778.932658	47.718029
3505.294131	464728.842730	47.723034
3505.389192	464670.915915	47.728039
3505.088027	464609.509983	47.733044
3505.394735	464547.037415	47.738049
3505.265576	464495.380257	47.743053
3505.145730	464440.073412	47.748058
3505.135104	464388.953060	47.753063
3504.892005	464337.973600	47.758068
3505.291336	464289.468306	47.763073
3505.416188	464236.095093	47.768077
3505.086951	464175.705916	47.773082
3505.167759	464130.547955	47.778087
3505.046047	464076.760403	47.783092
3505.184945	464019.432166	47.788097
3504.968261	463984.660771	47.793101
3505.168655	463931.577829	47.798106
3505.143147	463879.141325	47.803111
3504.983723	463832.148990	47.808116
3504.921858	463770.395542	47.813121
3504.951909	463731.528136	47.818125
3505.241065	463684.205512	47.823130
3504.951690	463636.322868	47.828135
3504.958718	463587.224125	47.833140
3504.991076	463534.726145	47.838145
3504.985601	463493.128233	47.843149
3504.681790	463434.100466	47.848154
3505.022046	463385.197661	47.853159
3504.659154	463354.554283	47.858164
3505.111607	463298.133099	47.863169
3504.974534	463256.506483	47.868173
3505.099431	463201.103663	47.873178
3505.251638	463161.859580	47.878183
3505.022543	463102.412698	47.883188
3505.105273	463054.667769	47.888193
3504.827202	463000.447919	47.893197
3504.787629	462963.110969	47.898202
3504.967405	462903.999029	47.903207
3504.770908	462875.910664	47.908212
3504.782000	462817.384638	47.913217
3504.681732	462781.780496	47.918221
3504.591614	462731.125407	47.923226
3505.022604	462684.992242	47.928231
3504.765410	462655.697828	47.933236
3504.758666	462592.157769	47.938241
3504.630776	462563.753216	47.943245
3504.677338	462512.618186	47.948250
3504.953756	462466.612242	47.953255
3504.637193	462439.658519	47.958260
3504.647376	462393.951221	47.963265
3504.427845	462368.399632	47.968269
3504.448850	462326.237332	47.973274
3504.331645	462281.970328	47.978279
3504.386188	462251.760663	47.983284
3504.673344	462216.292031	47.988289
3504.440553	462169.966963	47.993293
3504.463563	462131.959008	47.998298
3504.311418	462101.074993	48.003303
3504.425720	462070.550813	48.008308
3504.575549	462015.292402	48.013313
3504.520547	461990.218952	48.018317
3504.607723	461960.256630	48.023322
3504.768503	461916.194700	48.028327
3504.260407	461885.219105	48.033332
3504.259480	461847.518724	48.038337
3504.196126	461812.869305	48.043341
3504.008833	461770.183977	48.048346
3504.550735	461741.359831	48.053351
3504.568400	461723.874599	48.058356
3505.007751	461678.801783	48.063361
3504.359325	461641.414259	48.068365
3504.296631	461604.129345	48.073370
3504.837116	461563.396915	48.078375
3504.814194	461526.003715	48.083380
3504.875333	461488.089354	48.088385
3504.653203	461447.841615	48.093389
3504.898002	461411.821355	48.098394
3504.917582	461362.664227	48.103399
3504.441440	461328.388483	48.108404
3504.551556	461285.245929	48.113409
3504.406029	461252.180458	48.118413
3504.514221	461208.683345	48.123418
3504.339581	461185.402905	48.128423
3504.327071	461150.540942	48.133428
3504.684978	461100.717299	48.138433
3504.380641	461082.374332	48.143437
3504.485862	461045.667790	48.148442
3504.403118	461001.493374	48.153447
3504.170558	460982.935359	48.158452
3504.100868	460947.424026	48.163457
3504.292824	460932.948842	48.168461
3504.446288	460891.470308	48.173466
3504.766303	460854.270657	48.178471
3504.597310	460823.742245	48.183476
3504.593432	460782.341023	48.188481
3504.325551	460739.819251	48.193485
3504.479167	460718.053158	48.198490
3504.862999	460668.832110	48.203495
3504.211143	460637.625719	48.208500
3504.518298	460609.448120	48.213505
3504.488463	460580.567879	48.218509
3504.829512	460539.614016	48.223514
3504.972482	460515.670442	48.228519
3504.333297	460476.708165	48.233524
3504.448003	460431.839970	48.238529
3504.493098	460412.676570	48.243533
3504.322246	460372.215179	48.248538
3504.539009	460332.903762	48.253543
3504.260267	460308.474499	48.258548
3504.374597	460279.214466	48.263553
3504.554716	460238.540844	48.268557
3504.273646	460204.888642	48.273562
3504.347783	460180.297614	48.278567
3504.453966	460157.170722	48.283572
3504.361577	460113.553421	48.288577
3504.193947	460082.922279	48.293581
3503.987394	460058.632414	48.298586
3504.411630	460038.745110	48.303591
3504.115831	460009.757418	48.308596
3504.369005	459975.101409	48.313601
3504.708014	459950.312838	48.318605
3504.727165	459917.825152	48.323610
3504.447421	459868.107289	48.328615
3504.445722	459845.961336	48.333620
3504.988067	459811.559736	48.338625
3504.408997	459774.359544	48.343629
3504.088584	459745.071599	48.348634
3504.476825	459720.223657	48.353639
3504.314376	459685.992860	48.358644
3504.520485	459649.418543	48.363649
3504.647685	459632.368867	48.368653
3504.401656	459592.374828	48.373658
3504.560915	459557.480736	48.378663
3504.473238	459537.781697	48.383668
3504.608346	459495.999310	48.388673
3504.183702	459461.508822	48.393677
3504.270968	459430.427720	48.398682
3504.065154	459407.961377	48.403687
3503.824558	459386.869285	48.408692
3504.224308	459364.198138	48.413697
3504.153485	459333.346594	48.418701
3504.334176	459291.150560	48.423706
3504.256295	459270.993470	48.428711
3504.093527	459254.246379	48.433716
3504.472410	459228.537872	48.438721
3504.090392	459194.191681	48.443725
3503.923700	459168.677611	48.448730
3504.075126	459143.362590	48.453735
3504.192575	459121.144807	48.458740
3504.276654	459096.854822	48.463745
3504.230274	459064.275573	48.468749
3503.894410	459031.593659	48.473754
3504.163698	459004.231135	48.478759
3504.135584	458986.801986	48.483764
3504.096281	458972.922346	48.488769
3504.433213	458954.873357	48.493773
3504.147501	458917.469430	48.498778
3504.388147	458878.911271	48.503783
3504.034139	458866.200260	48.508788
3504.194663	458843.772092	48.513793
3503.809870	458826.707788	48.518797
3503.776954	458816.881392	48.523802
3504.006141	458798.952021	48.528807
3503.491243	458759.661067	48.533812
3504.289057	458725.568743	48.538817
3504.042256	458710.609371	48.543821
3504.088192	458682.980460	48.548826
3504.292747	458665.105856	48.553831
3503.957126	458659.841674	48.558836
3504.329487	458627.342256	48.563841
3504.143192	458605.378488	48.568845
3503.895073	458575.417624	48.573850
3504.295496	458547.474592	48.578855
3504.071997	458539.707852	48.583860
3503.998697	458526.340519	48.588865
3504.150408	458503.862793	48.593869
3504.111686	458473.409891	48.598874
3503.999118	458436.178225	48.603879
3503.989638	458416.667454	48.608884
3504.306213	458393.502594	48.613889
3504.324209	458386.302739	48.618893
3504.092328	458365.410805	48.623898
3504.096379	458319.188343	48.628903
3504.075919	458304.544793	48.633908
3503.770720	458270.842760	48.638913
3503.955342	458255.708020	48.643917
3503.925345	458243.093334	48.648922
3503.826407	458221.823776	48.653927
3503.828160	458209.811833	48.658932
3503.914953	458193.832154	48.663937
3503.532239	458179.503777	48.668941
3503.747219	458161.525580	48.673946
3504.036350	458149.211120	48.678951
3503.775788	458141.045095	48.683956
3504.348194	458116.011670	48.688961
3503.790470	458076.878733	48.693965
3503.583147	458058.009583	48.698970
3503.844981	458027.555366	48.703975
3503.600791	458015.179840	48.708980
3503.947378	457998.192677	48.713985
3503.631770	457991.049642	48.718989
3503.712529	457970.154596	48.723994
3503.966944	457949.635339	48.728999
3503.789719	457932.889608	48.734004
3504.198618	457925.774892	48.739009
3504.060633	457915.611214	48.744013
3504.036293	457893.771059	48.749018
3503.845990	457886.707958	48.754023
3503.497038	457875.820037	48.759028
3503.742354	457852.413306	48.764033
3503.697585	457842.892554	48.769037
3503.622206	457843.462953	48.774042
3503.913224	457819.136084	48.779047
3503.836532	457813.523368	48.784052
3504.078046	457777.243682	48.789057
3503.753765	457742.378305	48.794061
3503.702437	457720.238470	48.799066
3504.179095	457705.915069	48.804071
3503.669790	457703.265142	48.809076
3504.035141	457684.652642	48.814081
3503.783782	457672.024710	48.819085
3504.136178	457658.330694	48.824090
3503.627753	457639.309828	48.829095
3503.862793	457635.721860	48.834100
3503.725719	457616.333464	48.839105
3503.639181	457601.447266	48.844109
3503.606768	457590.859928	48.849114
3503.753276	457572.994263	48.854119
3503.539658	457567.911695	48.859124
3504.010814	457541.982538	48.864129
3503.585145	457533.895140	48.869133
3503.514332	457527.875870	48.874138
3503.486876	457508.468652	48.879143
3503.321208	457497.751967	48.884148
3503.330041	457477.628948	48.889153
3503.686193	457469.357347	48.894157
3503.265909	457456.707438	48.899162
3503.655737	457445.794508	48.904167
3503.518223	457437.860606	48.909172
3503.703430	457425.107292	48.914177
3503.727569	457411.215737	48.919181
3503.699997	457404.732889	48.924186
3503.962473	457382.133627	48.929191
3503.846565	457378.402801	48.934196
3504.056499	457366.760281	48.939201
3503.666960	457353.294110	48.944205
3503.710166	457346.799158	48.949210
3503.997613	457329.517424	48.954215
3503.580425	457324.925712	48.959220
3503.410712	457306.606961	48.964225
3503.461643	457295.599762	48.969229
3503.299287	457279.864636	48.974234
3503.754280	457266.000783	48.979239
3503.456035	457262.301068	48.984244
3503.435938	457248.416954	48.989249
3503.442362	457245.020007	48.994253
3503.530426	457253.266564	48.999258
3503.794080	457243.591497	49.004263
3503.621704	457246.307225	49.009268
3503.611889	457230.900807	49.014273
3503.665030	457226.026027	49.019277
3503.676497	457213.352929	49.024282
3503.805519	457200.406328	49.029287
3503.677315	457189.480343	49.034292
3503.722634	457175.534324	49.039297
3503.881036	457162.531998	49.044301
3503.647510	457149.039051	49.049306
3503.839144	457125.894066	49.054311
3503.436865	457101.329916	49.059316
3503.789412	457093.616310	49.064321
3503.515818	457082.968516	49.069325
3503.617231	457084.066284	49.074330
3503.837258	457085.245168	49.079335
3503.834803	457078.301761	49.084340
3503.988640	457058.812470	49.089345
3503.818913	457033.650995	49.094349
3503.683450	457014.109688	49.099354
3504.100823	456995.132874	49.104359
3503.905848	456996.129198	49.109364
3503.741002	456977.302465	49.114369
3503.782853	456963.052780	49.119373
3503.611775	456965.109415	49.124378
3503.560820	456941.752214	49.129383
3503.534453	456933.444337	49.134388
3503.822357	456917.429306	49.139393
3503.607450	456908.089218	49.144397
3503.467849	456899.395179	49.149402
3503.617614	456884.113304	49.154407
3503.359480	456882.079290	49.159412
3503.382557	456871.431414	49.164417
3503.906369	456857.251417	49.169421
3503.686642	456849.331320	49.174426
3503.764773	456832.743814	49.179431
3503.665492	456840.110188	49.184436
3503.739241	456810.547902	49.189441
3503.438691	456809.686893	49.194445
3503.547188	456798.416165	49.199450
3503.802938	456799.082110	49.204455
3503.565237	456797.145970	49.209460
3503.675260	456802.195764	49.214465
3503.704076	456795.601721	49.219469
3503.567864	456792.887966	49.224474
3503.587329	456764.500652	49.229479
3503.535147	456763.597232	49.234484
3503.525163	456758.581060	49.239489
3503.795839	456751.996392	49.244493
3503.508258	456743.580981	49.249498
3503.890231	456730.185402	49.254503
3503.603286	456727.345317	49.259508
3503.711702	456718.811595	49.264513
3503.751899	456706.741504	49.269517
3503.292864	456692.982641	49.274522
3503.666953	456679.436317	49.279527
3503.762961	456675.973291	49.284532
3503.687908	456658.398078	49.289537
3503.343790	456653.590990	49.294541
3503.236261	456641.089909	49.299546
3503.868796	456636.420173	49.304551
3503.555604	456627.907715	49.309556
3503.958071	456612.227684	49.314561
3503.607003	456606.509421	49.319565
3503.571776	456594.300083	49.324570
3503.464874	456585.752383	49.329575
3503.269537	456576.510173	49.334580
3503.514170	456563.289992	49.339585
3503.710830	456560.316624	49.344589
3503.564230	456550.457844	49.349594
3503.720462	456536.492447	49.354599
3503.702730	456534.062544	49.359604
3503.647774	456514.152202	49.364609
3503.815855	456513.616653	49.369613
3503.842873	456504.843307	49.374618
3503.750921	456493.910754	49.379623
3503.372222	456480.695579	49.384628
3503.372327	456473.143290	49.389633
3503.763485	456468.058552	49.394637
3503.500318	456460.247092	49.399642
3504.052570	456461.166541	49.404647
3503.651635	456449.931917	49.409652
3503.433603	456425.386169	49.414657
3503.641165	456432.700299	49.419661
3503.458727	456436.279525	49.424666
3503.853782	456435.096980	49.429671
3503.509609	456444.431404	49.434676
3503.377869	456427.423220	49.439681
3503.179130	456421.374775	49.444685
3503.249601	456419.335292	49.449690
3503.456524	456405.715955	49.454695
3503.190586	456404.392837	49.459700
3503.147092	456392.286162	49.464705
3503.323523	456401.328967	49.469709
3503.215962	456404.895413	49.474714
3503.597449	456398.443769	49.479719
3503.443074	456402.981256	49.484724
3503.366493	456385.760873	49.489729
3503.692777	456378.609035	49.494733
3503.326061	456385.159564	49.499738
3503.367861	456364.776374	49.504743
3503.407990	456359.346052	49.509748
3503.342678	456348.915740	49.514753
3503.457838	456365.470667	49.519757
3503.420685	456369.582652	49.524762
3503.453913	456356.955988	49.529767
3503.283911	456366.210022	49.534772
3503.463007	456347.678781	49.539777
3503.654262	456340.144491	49.544781
3503.464604	456340.278262	49.549786
3503.739060	456327.965199	49.554791
3503.615386	456317.696896	49.559796
3503.419877	456306.427116	49.564801
3503.592125	456305.789477	49.569805
3503.655787	456301.318172	49.574810
3503.904296	456293.013785	49.579815
3503.400102	456284.584481	49.584820
3503.456633	456275.552561	49.589825
3503.804325	456275.848017	49.594829
3503.595702	456271.372511	49.599834
3503.465958	456259.838040	49.604839
3503.518615	456268.445855	49.609844
3503.580761	456268.232510	49.614849
3503.500656	456264.850172	49.619853
3503.217819	456260.691458	49.624858
3503.502544	456242.953078	49.629863
3503.342132	456249.772548	49.634868
3503.295674	456239.541708	49.639873
3503.830621	456225.815554	49.644877
3503.512699	456220.547705	49.649882
3503.623088	456206.083036	49.654887
3503.547411	456203.510926	49.659892
3503.385932	456198.216360	49.664897
3503.519263	456202.603392	49.669901
3503.130233	456216.811546	49.674906
3503.364587	456204.454569	49.679911
3503.293034	456213.286364	49.684916
3503.371911	456206.683581	49.689921
3503.551514	456192.612581	49.694925
3503.251257	456186.733461	49.699930
3503.360971	456177.540356	49.704935
3503.353419	456190.416211	49.709940
3503.331434	456201.621847	49.714945
3503.319003	456198.025194	49.719949
3503.174739	456192.474250	49.724954
3503.670863	456191.477184	49.729959
3503.404846	456189.292383	49.734964
3503.292668	456180.238540	49.739969
3503.340132	456168.927196	49.744973
3503.289538	456181.962468	49.749978
3503.119884	456194.612563	49.754983
3503.199343	456204.128199	49.759988
3503.400054	456187.823356	49.764993
3503.239750	456180.095598	49.769997
3503.468563	456180.056543	49.775002
3503.638195	456171.613513	49.780007
3503.511436	456167.326754	49.785012
3503.255540	456182.171135	49.790017
3503.351556	456180.330015	49.795021
3503.341574	456178.253557	49.800026
3503.294181	456172.381944	49.805031
3503.302539	456167.362493	49.810036
3503.441837	456163.689240	49.815041
3503.510469	456151.360527	49.820045
3503.226305	456150.192566	49.825050
3503.492751	456159.169422	49.830055
3503.380811	456178.196269	49.835060
3503.184041	456173.414594	49.840065
3503.575398	456171.624419	49.845069
3503.154592	456173.825148	49.850074
3503.220314	456165.906730	49.855079
3503.118741	456153.860516	49.860084
3503.436750	456167.745230	49.865089
3503.240154	456174.469529	49.870093
3503.282533	456180.342026	49.875098
3503.358589	456163.957074	49.880103
3503.541556	456164.077909	49.885108
3503.253594	456158.855616	49.890113
3503.415816	456151.833086	49.895117
3503.557451	456148.869053	49.900122
3503.625019	456149.921963	49.905127
3503.352098	456163.755518	49.910132
3503.577328	456163.260890	49.915137
3503.554522	456162.960674	49.920141
3503.359493	456171.560135	49.925146
3503.746814	456157.250895	49.930151
3503.937359	456149.159095	49.935156
3503.173765	456149.644301	49.940161
3503.383901	456140.636781	49.945165
3503.246965	456133.462576	49.950170
3503.626443	456127.112564	49.955175
3503.263329	456127.225266	49.960180
3503.115942	456118.887031	49.965185
3503.355568	456136.789453	49.970189
3503.042964	456140.137519	49.975194
3503.438601	456135.457433	49.980199
3503.332954	456121.739213	49.985204
3503.363091	456116.411907	49.990209
3503.283314	456120.379159	49.995213
3503.309233	456131.576653	50.000218
3503.566019	456137.209804	50.005223
3503.515798	456145.429739	50.010228
3503.445114	456143.465017	50.015233
3503.516437	456140.462301	50.020237
3503.342669	456133.193010	50.025242
3504.006521	456119.647523	50.030247
3503.149542	456113.863440	50.035252
3503.192233	456110.764234	50.040257
3503.070986	456103.029778	50.045261
3503.210186	456111.927007	50.050266
3503.444753	456122.784756	50.055271
3503.230117	456131.995830	50.060276
3503.223802	456126.978875	50.065281
3503.538102	456113.138258	50.070285
3503.441708	456107.629805	50.075290
3503.749075	456102.660658	50.080295
3504.164162	456102.184298	50.085300
3503.990937	456095.725899	50.090305
3503.944520	456090.665095	50.095309
3503.659085	456087.824661	50.100314
3503.861247	456076.841664	50.105319
3503.729445	456075.292871	50.110324
3503.475741	456063.931517	50.115329
3503.821596	456059.817476	50.120333
3503.797898	456058.909161	50.125338
3503.800607	456045.121701	50.130343
3503.950904	456042.764424	50.135348
3503.785884	456038.585547	50.140353
3503.697298	456038.245874	50.145357
3503.757333	456035.346445	50.150362
3504.055354	456021.001669	50.155367
3503.848591	456016.323038	50.160372
3503.209049	455985.766211	50.165377
3503.534508	455987.383348	50.170381
3503.037318	456002.015622	50.175386
3503.490916	455991.243085	50.180391
3503.344233	455984.780119	50.185396
3503.101637	455982.743359	50.190401
3503.251078	455975.469512	50.195405
3503.190002	455990.331455	50.200410
3503.469642	455996.315557	50.205415
3503.008720	455998.168341	50.210420
3503.399488	456004.133465	50.215425
3503.702844	455991.511138	50.220429
3503.445950	455997.079974	50.225434
3503.104054	455983.351312	50.230439
3503.192171	455994.132761	50.235444
3503.127717	456003.977189	50.240449
3503.363547	456004.747939	50.245453
3503.047574	456004.700529	50.250458
3503.423652	455991.406845	50.255463
3503.487165	455986.834121	50.260468
3503.367926	455992.075328	50.265473
3503.326869	455993.602983	50.270477
3503.358067	456011.186291	50.275482
3503.267940	456016.777334	50.280487
3503.359827	456007.789946	50.285492
3503.216646	456004.519710	50.290497
3503.411275	455996.123026	50.295501
3503.296483	455995.280950	50.300506
3503.347277	456007.690770	50.305511
3503.320467	456018.035641	50.310516
3503.347288	456024.924592	50.315521
3503.456835	456009.446174	50.320525
3503.329335	456010.532399	50.325530
3503.250901	456001.675465	50.330535
3503.483509	456002.750891	50.335540
3503.360577	456003.126709	50.340545
3503.459913	456010.966348	50.345549
3503.336908	456028.778721	50.350554
3503.564962	456021.390092	50.355559
3503.317766	456032.532900	50.360564
3503.075136	456037.085537	50.365569
3503.438070	456016.900602	50.370573
3503.042674	456016.562628	50.375578
3503.360417	456011.236874	50.380583
3503.519914	456024.033624	50.385588
3503.577791	456021.134562	50.390593
3503.348333	456020.768254	50.395597
3503.319490	456022.750010	50.400602
3503.611799	456015.096970	50.405607
3503.247605	456005.731267	50.410612
3503.390534	456009.305699	50.415617
3503.283353	456000.200235	50.420621
3503.504398	456000.162507	50.425626
3503.178342	456020.949441	50.430631
3503.133700	456032.159039	50.435636
3503.487371	456028.297095	50.440641
3503.308570	456015.250233	50.445645
3503.278108	456022.301029	50.450650
3503.271369	456009.427535	50.455655
3503.372021	456009.714489	50.460660
3503.209312	456034.072342	50.465665
3503.509223	456036.150026	50.470669
3502.977098	456043.235784	50.475674
3503.220029	456034.881556	50.480679
3503.145649	456028.710383	50.485684
3503.173084	456035.649913	50.490689
3503.392102	456052.085989	50.495693
3503.473409	456053.896872	50.500698
3503.631823	456051.335460	50.505703
3503.394816	456059.790073	50.510708
3503.145057	456062.721921	50.515713
3503.244366	456040.199709	50.520717
3503.242616	456035.131264	50.525722
3503.495839	456029.816531	50.530727
3503.338320	456026.041871	50.535732
3503.418669	456017.208520	50.540737
3503.411514	455985.023085	50.545741
3503.069570	455941.946198	50.550746
3503.425786	455894.999102	50.555751
3503.027372	455832.872952	50.560756
3502.783243	455764.181483	50.565761
3503.362639	455676.239617	50.570765
3503.324729	455585.716273	50.575770
3502.937209	455477.663154	50.580775
3502.917357	455371.219426	50.585780
3503.169017	455234.568501	50.590785
3503.606621	455080.650328	50.595789
3503.373865	454921.827111	50.600794
3503.451367	454751.240112	50.605799
3503.689669	454559.638059	50.610804
3503.724556	454381.046023	50.615809
3503.624310	454158.423976	50.620813
3503.330898	453944.399574	50.625818
3503.479272	453708.600750	50.630823
3503.617281	453468.238530	50.635828
3503.049213	453207.462754	50.640833
3502.792625	452955.299370	50.645837
3502.480038	452684.030115	50.650842
3502.983043	452395.381193	50.655847
3503.025331	452106.198538	50.660852
3503.294045	451787.771098	50.665857
3503.245578	451460.875512	50.670861
3502.857905	451131.751210	50.675866
3503.106438	450764.791861	50.680871
3503.066251	450409.333879	50.685876
3503.336276	450025.829178	50.690881
3503.637837	449624.616597	50.695885
3503.205828	449228.642729	50.700890
3503.044437	448803.155404	50.705895
3503.214243	448367.512357	50.710900
3503.111908	447919.889117	50.715905
3502.974125	447454.058084	50.720909
3503.008441	446978.856844	50.725914
3502.960424	446484.896016	50.730919
3502.615860	445981.288368	50.735924
3502.289387	445458.445417	50.740929
3502.513385	444922.715641	50.745933
3502.464686	444381.085319	50.750938
3502.468942	443819.044045	50.755943
3502.446191	443250.196489	50.760948
3502.396224	442655.572962	50.765953
3502.425676	442039.667391	50.770957
3501.945986	441411.962248	50.775962
3502.060998	440762.529030	50.780967
3502.107227	440104.211358	50.785972
3501.977936	439433.323635	50.790977
3502.027792	438737.477102	50.795981
3501.705437	438028.634597	50.800986
3501.676940	437305.717321	50.805991
3501.857555	436554.279326	50.810996
3501.486812	435795.198580	50.816001
3501.663816	435002.816593	50.821005
3501.610595	434219.630052	50.826010
3501.549753	433400.594845	50.831015
3501.758493	432558.497858	50.836020
3501.296258	431705.320822	50.841025
3501.752669	430821.710511	50.846029
3501.391457	429921.712973	50.851034
3501.572147	429005.754096	50.856039
3501.467921	428070.725232	50.861044
3501.118785	427110.932964	50.866049
3501.121877	426127.389189	50.871053
3501.035368	425144.936960	50.876058
3500.832179	424116.678199	50.881063
3501.138643	423080.115874	50.886068
3500.464620	422027.838097	50.891073
3500.820048	420947.163404	50.896077
3500.301905	419857.782011	50.901082
3500.355186	418736.116592	50.906087
3500.281668	417604.902361	50.911092
3500.046221	416450.358527	50.916097
3500.069811	415280.865102	50.921101
3499.926915	414090.373942	50.926106
3499.726298	412867.716947	50.931111
3499.823161	411641.802864	50.936116
3499.390953	410385.347034	50.941121
3499.779520	409114.266614	50.946125
3499.371502	407827.058432	50.951130
3499.121889	406514.922305	50.956135
3499.215007	405182.598739	50.961140
3498.980569	403836.372133	50.966145
3498.949263	402472.289371	50.971149
3498.347097	401082.834329	50.976154
3498.394305	399664.848638	50.981159
3498.314039	398252.733398	50.986164
3498.462058	396804.254245	50.991169
3498.494769	395335.040266	50.996173
3498.133608	393853.064389	51.001178
3497.756960	392353.712383	51.006183
3497.852542	390837.636129	51.011188
3497.426010	389291.001117	51.016193
3497.666377	387725.519956	51.021197
3497.119659	386166.549773	51.026202
3496.573253	384561.370244	51.031207
3496.382552	382961.742607	51.036212
3496.052037	381346.502591	51.041217
3496.340862	379698.487321	51.046221
3495.518610	378046.588338	51.051226
3495.453216	376375.131493	51.056231
3495.438759	374696.769929	51.061236
3495.195097	373003.923888	51.066241
3495.151790	371267.659359	51.071245
3494.477000	369549.293849	51.076250
3494.506549	367793.192141	51.081255
3494.256439	366025.203229	51.086260
3493.877520	364250.107649	51.091265
3493.899889	362452.631658	51.096269
3493.472096	360637.242773	51.101274
3493.317545	358816.356139	51.106279
3493.452482	356976.132163	51.111284
3492.876638	355119.436952	51.116289
3493.071822	353227.166507	51.121293
3492.022963	351337.567579	51.126298
3492.054371	349427.144620	51.131303
3492.244108	347502.643626	51.136308
3491.679804	345578.239654	51.141313
3491.453194	343637.260002	51.146317
3491.135841	341669.421215	51.151322
3490.696984	339693.888361	51.156327
3490.598928	337698.037779	51.161332
3490.298135	335713.009109	51.166337
3489.912926	333678.800662	51.171341
3489.086312	331659.248856	51.176346
3489.257843	329616.392431	51.181351
3489.588232	327551.774109	51.186356
3488.736031	325493.621415	51.191361
3488.904426	323409.157728	51.196365
3488.005427	321312.510300	51.201370
3487.887324	319200.157074	51.206375
3487.982184	317088.946333	51.211380
3487.157342	314945.699114	51.216385
3487.026563	312792.491627	51.221389
3486.684330	310634.266353	51.226394
3486.495604	308460.422657	51.231399
3486.098533	306269.343138	51.236404
3485.764370	304080.664080	51.241409
3485.448807	301866.438806	51.246413
3485.016720	299653.019208	51.251418
3484.871057	297414.035961	51.256423
3484.169604	295160.226694	51.261428
3484.047327	292903.825863	51.266433
3483.977414	290631.811850	51.271437
3483.129104	288360.804332	51.276442
3482.638771	286073.754046	51.281447
3482.152512	283763.898676	51.286452
3481.360642	281464.984849	51.291457
3481.018956	279150.121582	51.296461
3480.677682	276830.415234	51.301466
3480.602816	274497.138951	51.306471
3480.065127	272165.063687	51.311476
3479.837892	269812.463976	51.316481
3479.328243	267447.109542	51.321485
3478.476970	265077.061329	51.326490
3477.992586	262694.077208	51.331495
3478.040238	260315.450445	51.336500
3477.061993	257922.298351	51.341505
3476.942077	255516.034272	51.346509
3475.963026	253111.446275	51.351514
3475.391857	250687.972385	51.356519
3475.479240	248269.844402	51.361524
3474.903863	245852.477940	51.366529
3474.760518	243405.408435	51.371533
3473.682093	240964.095027	51.376538
3473.357453	238513.812824	51.381543
3472.980216	236055.059929	51.386548
3472.135082	233591.603846	51.391553
3471.645455	231108.868467	51.396557
3471.107365	228641.458961	51.401562
3470.793454	226152.865346	51.406567
3470.172210	223663.886196	51.411572
3469.617969	221173.366416	51.416577
3469.461918	218665.160231	51.421581
3468.656282	216167.282830	51.426586
3467.882761	213655.737061	51.431591
3467.588413	211134.754541	51.436596
3466.963343	208612.931344	51.441601
3466.320983	206076.520307	51.446605
3465.443971	203551.468903	51.451610
3464.895024	201009.463000	51.456615
3464.424314	198470.764434	51.461620
3463.352965	195941.156940	51.466625
3463.105536	193384.265677	51.471629
3462.356239	190839.982871	51.476634
3461.618241	188279.931593	51.481639
3461.299728	185724.384878	51.486644
3460.428724	183170.661659	51.491649
3459.827731	180605.938358	51.496653
3459.099129	178061.209172	51.501658
3458.527337	175493.139990	51.506663
3457.561149	172936.223528	51.511668
3456.968406	170371.247206	51.516673
3456.238203	167801.687727	51.521677
3455.722445	165237.043511	51.526682
3454.946417	162671.369478	51.531687
3454.044540	160098.554314	51.536692
3453.350819	157540.829915	51.541697
3452.450348	154966.307992	51.546701
3451.486817	152416.531354	51.551706
3451.033515	149842.392377	51.556711
3450.580367	147260.873460	51.561716
3449.562541	144658.332312	51.566721
3448.969739	142093.574985	51.571725
3447.891462	139537.348342	51.576730
3446.832677	136976.131997	51.581735
3446.329556	134423.847074	51.586740
3445.192016	131878.894100	51.591745
3444.567763	129322.181305	51.596749
3443.307593	126793.052230	51.601754
3442.581384	124259.346714	51.606759
3441.436779	121718.462687	51.611764
3440.742138	119200.024956	51.616769
3440.275101	116683.134154	51.621773
3438.949727	114173.098454	51.626778
3437.872153	111657.855294	51.631783
3436.578462	109156.742896	51.636788
3435.773163	106670.733177	51.641793
3435.108566	104185.066700	51.646797
3433.872694	101715.663607	51.651802
3432.672463	99243.566554	51.656807
3431.939060	96776.443662	51.661812
3430.546784	94336.594586	51.666817
3429.502495	91884.948846	51.671821
3428.515780	89463.626259	51.676826
3427.337238	87042.184163	51.681831
3426.293137	84646.225729	51.686836
3425.253699	82258.920835	51.691841
3424.099405	79864.224536	51.696845
3422.828066	77492.223421	51.701850
3421.539567	75144.976718	51.706855
3420.360510	72798.743943	51.711860
3419.131007	70481.350219	51.716865
3418.051501	68153.121409	51.721869
3416.809640	65853.259059	51.726874
3415.383431	63569.078483	51.731879
3414.554775	61304.766150	51.736884
3412.950272	59047.068715	51.741889
3412.114985	56803.015755	51.746893
3410.208441	54586.357023	51.751898
3409.134119	52386.733608	51.756903
3407.846105	50195.707156	51.761908
3406.627906	48032.095506	51.766913
3405.163513	45873.475442	51.771917
3403.346966	43754.126951	51.776922
3402.067583	41649.456073	51.781927
3400.384877	39576.101904	51.786932
3398.346330	37514.679591	51.791937
3396.670603	35486.041872	51.796941
3394.396016	33488.113571	51.801946
3392.653055	31527.236231	51.806951
3390.553691	29592.881117	51.811956
3387.871849	27706.238004	51.816961
3385.415140	25855.431123	51.821965
3381.463057	24096.950523	51.826970
3375.866131	22433.302824	51.831975
3369.723612	20871.442040	51.836980
3363.454327	19404.175278	51.841985
3358.098435	18020.323589	51.846989
3352.857389	16749.486881	51.851994
3347.750614	15581.125355	51.856999
3343.273689	14513.568797	51.862004
3338.093482	13560.029599	51.867009
3333.926145	12691.483825	51.872013
3329.528874	11930.463323	51.877018
3325.072056	11277.134344	51.882023
3321.534236	10687.447767	51.887028
3317.922651	10207.032975	51.892033
3315.318340	9773.150107	51.897037
3312.897083	9420.711553	51.902042
3310.432471	9119.340990	51.907047
3308.635791	8880.230060	51.912052
3306.842018	8689.249611	51.917057
3305.523827	8537.881333	51.922061
3304.291907	8420.498822	51.927066
3303.469848	8329.450721	51.932071
3302.842939	8249.592134	51.937076
3302.413690	8211.358856	51.942081
3302.281799	8170.653171	51.947085
3301.861304	8154.052728	51.952090
3301.084049	8142.861357	51.957095
3301.221680	8132.725343	51.962100
3300.978698	8137.727155	51.967105
3300.932174	8133.338783	51.972109
3300.724167	8148.285221	51.977114
3300.686479	8146.489222	51.982119
3300.434541	8151.037612	51.987124
3300.190238	8160.323835	51.992129
3300.099643	8150.643052	51.997133
3300.275453	8160.271393	52.002138
3300.036540	8146.716429	52.007143
3300.186796	8139.300888	52.012148
3299.661788	8130.725878	52.017153
3299.563431	8109.978212	52.022157
3299.317119	8088.396489	52.027162
3299.204744	8068.995600	52.032167
3299.645190	8042.239990	52.037172
3298.865846	8012.380170	52.042177
3298.866085	7958.009392	52.047181
3298.416470	7925.213628	52.052186
3297.790923	7886.363823	52.057191
3297.455983	7837.978480	52.062196
3297.261997	7801.358332	52.067201
3296.910525	7748.023005	52.072205
3296.209376	7705.357426	52.077210
3295.784410	7640.767240	52.082215
3295.229511	7589.782182	52.087220
3294.413041	7540.221795	52.092225
3294.335490	7476.868232	52.097229
3294.176118	7429.549608	52.102234
3293.540080	7355.094646	52.107239
3293.141098	7299.081174	52.112244
3292.418881	7227.054410	52.117249
3292.156220	7161.780506	52.122253
3291.309143	7103.834202	52.127258
3291.088799	7034.771210	52.132263
3290.956174	6962.909493	52.137268
3290.033554	6887.041370	52.142273
3289.773516	6823.341661	52.147277
3289.060535	6748.104176	52.152282
3288.707285	6669.443484	52.157287
3288.292739	6577.030168	52.162292
3287.575453	6506.041984	52.167297
3286.784847	6420.282119	52.172301
3286.396489	6340.043968	52.177306
3285.550779	6267.350771	52.182311
3285.270455	6183.858495	52.187316
3284.529913	6107.365900	52.192321
3284.158655	6012.638406	52.197325
3283.461918	5929.126983	52.202330
3282.563390	5857.574797	52.207335
3282.571884	5756.465210	52.212340
3281.326905	5686.505068	52.217345
3280.953071	5593.085139	52.222349
3280.483776	5509.637348	52.227354
3279.550562	5415.341864	52.232359
3278.974134	5328.256123	52.237364
3278.451893	5259.173381	52.242369
3277.773464	5165.565544	52.247373
3277.212101	5079.140365	52.252378
3276.475196	4990.668729	52.257383
3275.948130	4897.606771	52.262388
3275.211024	4812.383390	52.267393
3274.550525	4722.929657	52.272397
3274.176452	4642.284582	52.277402
3273.132021	4555.155875	52.282407
3272.477315	4473.566179	52.287412
3271.611772	4401.682443	52.292417
3271.603743	4305.397914	52.297421
3270.657762	4218.780940	52.302426
3269.927818	4144.585972	52.307431
3269.416401	4055.232924	52.312436
3268.831308	3973.177486	52.317441
3268.125376	3882.826566	52.322445
3267.544179	3812.807863	52.327450
3266.410670	3725.724196	52.332455
3265.944060	3633.054130	52.337460
3265.209151	3564.781814	52.342465
3264.736444	3481.680832	52.347469
3263.991707	3396.029693	52.352474
3263.499889	3313.525073	52.357479
3262.859327	3236.970763	52.362484
3262.252920	3155.291950	52.367489
3261.511046	3074.122309	52.372493
3260.631261	2996.186373	52.377498
3260.242103	2917.254232	52.382503
3259.742081	2834.156578	52.387508
3259.285510	2754.669837	52.392513
3258.063760	2674.866520	52.397517
3257.210933	2590.995826	52.402522
3256.485118	2518.454844	52.407527
3255.987114	2437.206547	52.412532
3255.515536	2368.736499	52.417537
3254.588311	2292.304433	52.422541
3254.055864	2218.911436	52.427546
3253.171118	2145.289197	52.432551
3252.860456	2063.187313	52.437556
3251.957744	2001.147644	52.442561
3251.326281	1929.454656	52.447565
3250.630513	1858.044584	52.452570
3249.981268	1792.763202	52.457575
3249.466113	1717.968940	52.462580
3248.677532	1648.641896	52.467585
3248.038370	1580.481822	52.472589
3247.242585	1508.386559	52.477594
3246.500427	1433.939161	52.482599
3246.023470	1359.314170	52.487604
3245.225963	1301.904431	52.492609
3244.518655	1236.606068	52.497613
3243.823375	1170.365617	52.502618
3243.143947	1104.888164	52.507623
3242.845724	1039.177301	52.512628
3242.048814	976.972418	52.517633
3241.369424	902.646297	52.522637
3240.681752	837.284663	52.527642
3240.118604	768.421563	52.532647
3239.459614	701.338063	52.537652
3238.409052	649.563117	52.542657
3237.657714	578.974426	52.547661
3237.332594	518.499071	52.552666
3236.549490	459.210612	52.557671
3235.983702	403.821557	52.562676
3234.872260	344.567521	52.567681
3233.999485	294.352188	52.572685
3233.191402	255.981735	52.577690
3231.481611	206.566910	52.582695
3230.873402	167.883453	52.587700
3230.107723	151.342479	52.592705
3228.885668	115.981856	52.597709
3227.197494	117.321441	52.602714
3225.245354	135.942346	52.607719
3224.655409	130.897857	52.612724
3224.250364	136.142359	52.617729
3224.744566	133.947328	52.622733
3224.059548	128.551589	52.627738
3223.200618	132.406426	52.632743
3223.030388	125.444482	52.637748
3222.375393	141.064108	52.642753
3221.608171	136.690549	52.647757
3220.897229	130.495966	52.652762
3219.793547	142.739161	52.657767
3219.359650	130.432631	52.662772
3219.186720	137.345865	52.667777
3218.043860	136.274443	52.672781
3217.873761	133.684492	52.677786
3217.310556	138.681679	52.682791
3216.460893	133.754980	52.687796
3215.644243	145.309285	52.692801
3214.997362	136.285786	52.697805
3214.563498	133.073015	52.702810
3213.559468	132.909831	52.707815
3213.048512	130.468901	52.712820
3212.428572	139.308993	52.717825
3211.871905	131.164540	52.722829
3211.618882	128.082714	52.727834
3210.708421	136.106008	52.732839
3210.169325	133.940669	52.737844
3209.282399	134.672461	52.742849
3208.528147	131.258249	52.747853
3208.055252	134.401360	52.752858
3207.426714	138.366047	52.757863
3207.117532	131.400999	52.762868
3206.168126	138.489520	52.767873
3205.459445	135.472514	52.772877
3205.181699	132.052682	52.777882
3203.871492	132.060227	52.782887
3204.086888	133.067105	52.787892
3202.943664	138.545088	52.792897
3202.884192	135.562824	52.797901
3201.714666	134.294254	52.802906
3200.457091	141.613844	52.807911
3200.331634	140.177558	52.812916
3199.755420	138.560919	52.817921
3199.210991	143.215828	52.822925
3198.144393	128.784811	52.827930
3198.155012	138.568731	52.832935
3197.243935	127.085428	52.837940
3196.474680	132.784119	52.842945
3196.212063	137.099176	52.847949
3195.453184	130.667661	52.852954
3194.048006	136.802623	52.857959
3194.029740	131.684942	52.862964
3193.088934	133.334606	52.867969
3192.926087	134.455841	52.872973
3192.408589	129.297140	52.877978
3191.115913	131.875323	52.882983
3190.837085	134.689627	52.887988
3189.831272	126.653889	52.892993
3189.012455	124.383189	52.897997
3188.815739	130.872202	52.903002
3187.895135	136.170051	52.908007
3187.264857	127.875553	52.913012
3186.582069	141.784436	52.918017
3185.995835	131.616527	52.923021
3185.648125	132.237646	52.928026
3185.250381	134.687012	52.933031
3184.665334	127.942386	52.938036
3183.755193	131.755451	52.943041
3182.641139	129.715188	52.948045
3182.568442	129.180528	52.953050
3181.439566	132.660709	52.958055
3180.605983	120.877208	52.963060
3180.183332	125.231445	52.968065
3179.845609	124.258917	52.973069
3178.844510	128.068575	52.978074
3178.264662	127.977396	52.983079
3177.753469	122.123295	52.988084
3177.167877	130.739229	52.993089
3176.438751	131.318147	52.998093
3175.783359	128.704533	53.003098
3175.299898	127.769537	53.008103
3174.664002	128.699623	53.013108
3173.668197	126.645476	53.018113
3172.747220	129.192130	53.023117
3172.642017	119.419275	53.028122
3171.950791	130.383338	53.033127
3171.365258	119.709278	53.038132
3170.209833	130.434499	53.043137
3170.063703	130.695132	53.048141
3169.734900	124.544612	53.053146
3168.938705	125.272749	53.058151
3167.963771	122.761494	53.063156
3166.916844	123.427472	53.068161
3165.903953	123.856323	53.073165
3165.855492	127.018102	53.078170
3164.991204	131.224379	53.083175
3164.760087	118.668887	53.088180
3164.306009	133.216435	53.093185
3163.902821	121.981496	53.098189
3163.423357	127.417917	53.103194
3162.387490	128.145163	53.108199
3161.673348	119.136728	53.113204
3160.603709	129.662559	53.118209
3159.626557	130.735818	53.123213
3159.240072	121.093125	53.128218
3158.544935	125.180898	53.133223
3158.531473	127.780130	53.138228
3157.355248	136.894865	53.143233
3156.793982	122.431609	53.148237
3156.108787	115.704893	53.153242
3155.123603	130.121736	53.158247
3155.188649	122.116597	53.163252
3154.506674	128.930485	53.168257
3153.904817	125.961947	53.173261
3153.051110	132.137296	53.178266
3152.044476	132.479030	53.183271
3151.544858	117.988273	53.188276
3150.361826	124.771322	53.193281
3150.247735	124.247683	53.198285
3149.612585	124.168719	53.203290
3148.850801	131.371630	53.208295
3148.244283	123.597281	53.213300
3147.590146	130.301416	53.218305
3146.773467	138.577502	53.223309
3146.677572	126.127585	53.228314
3145.989393	136.682588	53.233319
3145.595043	126.453092	53.238324
3144.877420	125.581789	53.243329
3142.927630	126.544132	53.248333
3142.598164	123.910363	53.253338
3141.810180	132.891266	53.258343
3141.511600	126.473880	53.263348
3141.099572	126.588106	53.268353
3140.742281	124.573684	53.273357
3140.091172	122.329206	53.278362
3138.898151	131.317338	53.283367
3138.000420	120.066640	53.288372
3137.598485	130.150767	53.293377
3136.867680	125.510484	53.298381
3137.120151	129.695691	53.303386
3136.366372	122.724515	53.308391
3135.359213	123.339099	53.313396
3134.209554	125.480366	53.318401
3133.525210	124.262729	53.323405
3132.986440	122.246157	53.328410
3132.253628	130.610146	53.333415
3131.635334	122.185327	53.338420
3131.335122	118.914997	53.343425
3131.261924	123.078084	53.348429
3130.484494	115.321103	53.353434
3128.827558	120.609763	53.358439
3128.374899	115.860383	53.363444
3128.213379	122.217853	53.368449
3127.678794	119.910048	53.373453
3127.028045	115.230828	53.378458
3126.089671	118.562415	53.383463
3125.205504	115.194496	53.388468
3124.836869	122.430888	53.393473
3123.549467	123.059409	53.398477
3123.263754	117.388629	53.403482
3122.241534	123.656716	53.408487
3122.105596	121.398428	53.413492
3121.946272	120.689890	53.418497
3120.465706	120.474330	53.423501
3120.481238	118.732913	53.428506
3119.565815	129.201609	53.433511
3119.157151	116.631857	53.438516
3117.859760	120.723061	53.443521
3117.582201	123.560832	53.448525
3117.286888	123.163287	53.453530
3115.938035	128.521679	53.458535
3115.561870	117.382396	53.463540
3114.471413	123.336492	53.468545
3113.703985	130.985228	53.473549
3113.329498	124.967254	53.478554
3112.465443	126.233560	53.483559
3112.075616	122.773679	53.488564
3111.840753	125.927043	53.493569
3111.207274	120.732911	53.498573
3110.279488	122.959033	53.503578
3109.264237	124.796292	53.508583
3109.044727	115.607045	53.513588
3108.913859	119.199733	53.518593
3107.607766	122.079822	53.523597
3106.652110	118.181369	53.528602
3105.818841	123.342724	53.533607
3105.652566	124.063896	53.538612
3104.790909	121.097124	53.543617
3104.112882	128.542693	53.548621
3103.593253	118.984732	53.553626
3102.842578	124.932878	53.558631
3102.268020	111.136245	53.563636
3101.517383	119.314989	53.568641
3100.825050	119.785394	53.573645
3100.757863	114.857657	53.578650
3099.763273	119.017914	53.583655
3098.882620	114.900995	53.588660
3098.325133	115.000605	53.593665
3098.049419	115.247066	53.598669
3097.383191	112.179802	53.603674
3096.149540	116.171699	53.608679
3095.678463	108.657246	53.613684
3095.184786	108.513853	53.618689
3094.819331	110.851915	53.623693
3093.853895	110.626501	53.628698
3092.322282	115.431134	53.633703
3092.854531	116.334131	53.638708
3092.751727	111.952864	53.643713
3091.321622	115.094533	53.648717
3090.304472	113.929819	53.653722
3089.320657	118.619934	53.658727
3089.469736	107.535783	53.663732
3088.856682	113.851587	53.668737
3087.432278	115.239691	53.673741
3087.125425	114.478996	53.678746
3086.850555	111.190132	53.683751
3086.011773	102.843663	53.688756
3084.976458	113.280336	53.693761
3084.540608	113.020882	53.698765
3084.316510	112.128419	53.703770
3083.014147	121.165628	53.708775
3082.336141	109.310581	53.713780
3082.464491	109.592999	53.718785
3081.075709	118.153932	53.723789
3080.548629	118.675444	53.728794
3080.084157	118.636796	53.733799
3079.066344	115.632371	53.738804
3078.967343	114.457618	53.743809
3077.661071	113.510068	53.748813
3077.576094	117.308856	53.753818
3076.873176	123.032927	53.758823
3075.754932	113.755675	53.763828
3075.193494	117.170886	53.768833
3074.885979	114.512059	53.773837
3074.440467	103.355828	53.778842
3073.020463	115.823977	53.783847
3072.508658	109.519222	53.788852
3072.594808	113.310874	53.793857
3071.536410	118.602669	53.798861
3070.367445	110.166963	53.803866
3069.700689	114.229364	53.808871
3069.707222	102.176046	53.813876
3068.983555	107.948656	53.818881
3067.842307	113.889722	53.823885
3067.693731	111.293342	53.828890
3066.568293	120.488213	53.833895
3066.028614	111.331576	53.838900
3065.642278	112.004693	53.843905
3064.821309	113.120357	53.848909
3064.440596	114.233425	53.853914
3063.081385	116.124726	53.858919
3062.551837	106.452425	53.863924
3062.381899	110.500592	53.868929
3061.653167	116.821164	53.873933
3060.944686	108.584667	53.878938
3059.924640	110.253414	53.883943
3059.492007	107.808201	53.888948
3058.810021	113.180938	53.893953
3058.380691	119.903105	53.898957
3058.140958	104.801147	53.903962
3057.340602	112.024460	53.908967
3056.655969	109.205079	53.913972
3056.428835	109.539949	53.918977
3054.766140	116.349310	53.923981
3053.817817	104.333230	53.928986
3053.391853	111.183105	53.933991
3053.092373	113.987516	53.938996
3052.664307	115.555902	53.944001
3051.315175	125.096492	53.949005
3051.069930	108.914709	53.954010
3050.002691	117.842667	53.959015
3049.418744	111.995100	53.964020
3049.393932	110.306367	53.969025
3048.451148	114.852110	53.974029
3047.661987	108.429755	53.979034
3046.495209	118.063916	53.984039
3046.323976	113.021334	53.989044
3046.131935	115.079115	53.994049
3044.700312	120.544421	53.999053
3044.025700	110.750070	54.004058
3043.935050	112.417509	54.009063
3043.472317	104.176131	54.014068
3042.687758	109.211140	54.019073
3041.295324	114.771588	54.024077
3041.039614	106.974824	54.029082
3040.502300	118.278491	54.034087
3039.830680	113.579168	54.039092
3039.143302	114.847662	54.044097
3038.691815	115.800329	54.049101
3038.288425	108.524577	54.054106
3037.565235	109.187362	54.059111
3036.688652	109.257426	54.064116
3035.242133	113.623198	54.069121
3035.315848	116.689885	54.074125
3034.779826	109.450612	54.079130
3033.478459	114.215519	54.084135
3032.553621	116.434831	54.089140
3032.887091	115.740774	54.094145
3031.778052	112.436166	54.099149
3031.114996	106.855930	54.104154
3030.251291	118.719436	54.109159
3030.249524	109.635493	54.114164
3029.533455	112.254516	54.119169
3028.555964	117.751564	54.124173
3028.319086	105.382218	54.129178
3027.422731	116.585002	54.134183
3026.729896	106.161023	54.139188
3026.247183	108.715698	54.144193
3025.377726	114.673090	54.149197
3024.791641	105.988593	54.154202
3023.340854	113.206212	54.159207
3023.124308	110.744998	54.164212
3022.871881	106.478118	54.169217
3021.789556	112.441884	54.174221
3020.987268	110.766006	54.179226
3020.715970	119.790851	54.184231
3020.481209	112.531678	54.189236
3018.979554	111.555556	54.194241
3018.106117	110.728658	54.199245
3018.101402	104.483708	54.204250
3017.476289	111.983387	54.209255
3016.311993	106.566961	54.214260
3015.783249	109.707778	54.219265
3015.360437	117.928399	54.224269
3014.729132	105.842765	54.229274
3014.273125	106.400688	54.234279
3013.591446	108.938837	54.239284
3013.217490	98.009600	54.244289
3012.799449	112.034655	54.249293
3012.027753	102.160593	54.254298
3010.351297	112.312099	54.259303
3009.637881	99.136055	54.264308
3009.220314	101.546180	54.269313
3009.004255	97.069015	54.274317
3008.629450	101.440337	54.279322
3007.142396	104.852667	54.284327
3007.183442	100.257360	54.289332
3006.449116	104.942742	54.294337
3005.522903	109.274082	54.299341
3005.140376	102.400552	54.304346
3004.533099	108.009202	54.309351
3003.492134	104.205482	54.314356
3002.448648	102.604376	54.319361
3001.948747	104.428980	54.324365
3002.273373	98.170781	54.329370
3001.359707	108.104707	54.334375
3000.608553	103.153728	54.339380
2999.684585	103.799118	54.344385
2998.882962	108.741916	54.349389
2998.355317	98.729448	54.354394
2997.179792	112.125670	54.359399
2996.744139	105.187009	54.364404
2996.544311	101.208374	54.369409
2995.025570	113.861161	54.374413
2994.886382	108.358778	54.379418
2994.328643	109.609465	54.384423
2993.380752	102.918597	54.389428
2992.647817	106.387194	54.394433
2992.250186	106.808042	54.399437
2991.861437	102.401833	54.404442
2990.909558	98.026328	54.409447
2990.301323	103.198573	54.414452
2989.861237	104.464286	54.419457
2989.171310	106.277549	54.424461
2989.041777	105.687081	54.429466
2988.167985	109.343956	54.434471
2987.569235	103.250648	54.439476
2986.298064	107.338576	54.444481
2985.545648	105.690497	54.449485
2985.066536	102.452333	54.454490
2984.531244	103.269722	54.459495
2983.726418	105.180775	54.464500
2983.222551	107.551572	54.469505
2982.290572	110.364990	54.474509
2982.238996	97.476111	54.479514
2980.506720	102.892539	54.484519
2979.899363	109.062901	54.489524
2979.913254	105.232083	54.494529
2979.266460	115.323695	54.499533
2978.021540	107.391249	54.504538
2977.467936	110.263165	54.509543
2977.172406	112.466128	54.514548
2976.619096	113.592905	54.519553
2975.676189	109.408889	54.524557
2975.347330	105.955186	54.529562
2974.406395	111.164156	54.534567
2974.116709	114.611090	54.539572
2973.699187	103.393256	54.544577
2972.893885	110.488737	54.549581
2971.814153	100.729296	54.554586
2970.886583	111.595579	54.559591
2970.095069	107.907918	54.564596
2969.758028	111.331365	54.569601
2968.785831	106.812891	54.574605
2969.009198	111.306203	54.579610
2968.199382	109.480045	54.584615
2967.401031	106.564850	54.589620
2967.362151	98.863280	54.594625
2966.335493	99.888582	54.599629
2965.276610	103.682084	54.604634
2964.231704	104.213543	54.609639
2963.391146	103.907997	54.614644
2962.971297	104.064229	54.619649
2962.401919	98.184193	54.624653
2962.026680	99.928682	54.629658
2961.643603	102.157262	54.634663
2961.135577	102.450138	54.639668
2960.583715	97.709053	54.644673
2959.434966	102.941298	54.649677
2958.498223	104.190835	54.654682
2957.825833	101.247408	54.659687
2957.129711	94.060776	54.664692
2956.686646	87.420626	54.669697
2955.737054	103.927363	54.674701
2955.646236	97.609899	54.679706
2954.843647	95.497122	54.684711
2954.335065	98.449368	54.689716
2953.999711	96.915546	54.694721
2952.978850	100.656369	54.699725
2951.835649	98.361805	54.704730
2951.396574	97.087676	54.709735
2951.061647	95.727856	54.714740
2950.175952	92.120637	54.719745
2949.755581	103.038789	54.724749
2949.118506	97.900568	54.729754
2948.105839	101.471049	54.734759
2947.124826	102.986304	54.739764
2946.559596	101.308612	54.744769
2945.487716	99.402904	54.749773
2945.568260	98.745355	54.754778
2944.970676	100.034827	54.759783
2944.205035	100.597512	54.764788
2943.600267	94.873918	54.769793
2942.960841	106.838428	54.774797
2942.318917	95.246859	54.779802
2941.895990	97.531195	54.784807
2941.280348	93.972957	54.789812
2939.702828	96.398945	54.794817
2938.797551	100.731055	54.799821
2939.071329	92.752250	54.804826
2938.310574	97.338733	54.809831
2937.116875	103.006547	54.814836
2937.143668	101.271500	54.819841
2936.035532	103.763720	54.824845
2935.968251	99.555207	54.829850
2935.141109	105.634842	54.834855
2934.806847	100.705395	54.839860
2934.216047	98.112756	54.844865
2932.933437	101.989099	54.849869
2932.070091	100.284988	54.854874
2931.806402	93.567212	54.859879
2931.286874	99.036923	54.864884
2930.735272	106.723376	54.869889
2929.183805	98.606894	54.874893
2928.165026	96.296599	54.879898
2928.111787	103.528026	54.884903
2928.123261	103.193719	54.889908
2926.939536	106.861724	54.894913
2925.572754	105.548770	54.899917
2925.078246	97.380345	54.904922
2924.769646	106.323133	54.909927
2924.930334	100.905297	54.914932
2924.122570	95.431918	54.919937
2923.422585	104.858420	54.924941
2923.075742	97.378427	54.929946
2921.926881	106.852825	54.934951
2920.555430	106.970766	54.939956
2920.041819	91.965389	54.944961
2919.424447	107.243806	54.949965
2918.822806	103.572259	54.954970
2918.435817	96.394777	54.959975
2918.339194	103.456780	54.964980
2918.272778	100.063232	54.969985
2916.356441	103.362238	54.974989
2915.451994	102.204745	54.979994
2914.525116	105.262425	54.984999
2913.850485	97.642270	54.990004
2914.114042	100.054023	54.995009
2913.228384	103.804903	55.000013
2912.995782	98.191392	55.005018
2912.300772	98.676881	55.010023
2911.695865	102.101500	55.015028
2910.564003	93.405306	55.020033
2909.394037	99.168932	55.025037
2908.964996	97.643624	55.030042
2908.246736	88.789516	55.035047
2907.625388	99.243865	55.040052
2907.271392	91.090906	55.045057
2906.775531	101.480391	55.050061
2906.174194	88.782586	55.055066
2905.592890	94.387981	55.060071
2904.524633	95.468558	55.065076
2903.469669	90.737280	55.070081
2902.678452	96.613411	55.075085
2902.806759	88.811835	55.080090
2901.894491	95.532447	55.085095
2901.154933	93.277464	55.090100
2900.963337	94.225197	55.095105
2900.300971	88.595533	55.100109
2899.793729	78.829473	55.105114
2898.829452	87.407867	55.110119
2897.695966	83.238681	55.115124
2897.485947	77.119623	55.120129
2896.774021	85.256217	55.125133
2896.238348	82.295359	55.130138
2895.763618	84.790253	55.135143
2894.782277	79.388785	55.140148
2893.530279	88.851591	55.145153
2892.616875	98.660739	55.150157
2892.275349	93.621621	55.155162
2891.987146	89.144956	55.160167
2891.614237	83.983314	55.165172
2891.391381	84.145358	55.170177
2890.601160	91.677589	55.175181
2889.662441	90.399646	55.180186
2888.440631	91.433443	55.185191
2887.678602	85.554769	55.190196
2887.337579	83.183524	55.195201
2886.502863	91.936748	55.200205
2886.327673	86.758289	55.205210
2885.767366	88.135340	55.210215
2885.121696	93.570951	55.215220
2884.760699	94.298168	55.220225
2883.518215	85.701416	55.225229
2882.949614	84.526796	55.230234
2882.122478	91.421538	55.235239
2881.361748	94.677004	55.240244
2881.185407	97.269718	55.245249
2879.566370	93.856918	55.250253
2879.250500	91.630580	55.255258
2878.782197	87.704156	55.260263
2878.000394	95.900460	55.265268
2877.742161	89.812927	55.270273
2876.799739	98.306280	55.275277
2876.886071	91.927367	55.280282
2876.142080	98.485017	55.285287
2874.321537	87.583962	55.290292
2873.960871	91.418802	55.295297
2873.051726	95.237251	55.300301
2872.528881	92.623928	55.305306
2872.103366	93.362172	55.310311
2871.607249	92.557655	55.315316
2871.477311	83.262364	55.320321
2870.541287	94.959009	55.325325
2870.343542	90.788194	55.330330
2868.830677	87.059235	55.335335
2868.296078	88.444131	55.340340
2867.912804	86.203657	55.345345
2867.179658	91.836977	55.350349
2866.651843	88.645047	55.355354
2865.380285	91.247309	55.360359
2864.300946	90.742593	55.365364
2863.981017	82.990786	55.370369
2863.323141	86.041573	55.375373
2863.005793	83.654837	55.380378
2862.752909	88.690960	55.385383
2862.101624	91.522734	55.390388
2861.642688	86.481583	55.395393
2860.013574	88.983510	55.400397
2859.374030	76.643562	55.405402
2858.751426	88.907147	55.410407
2858.377782	83.654847	55.415412
2857.703920	83.299119	55.420417
2857.178745	92.739159	55.425421
2856.540143	88.746714	55.430426
2856.292128	91.461411	55.435431
2855.206657	93.002821	55.440436
2854.396165	88.032411	55.445441
2853.430960	94.122617	55.450445
2853.488217	84.117591	55.455450
2852.890151	88.838507	55.460455
2852.088390	91.964807	55.465460
2850.854707	84.501399	55.470465
2850.205369	94.203838	55.475469
2849.387845	87.231395	55.480474
2849.059616	89.001801	55.485479
2848.668605	92.034613	55.490484
2848.065691	86.065597	55.495489
2846.977161	96.377557	55.500493
2846.699004	89.634635	55.505498
2846.159267	94.991751	55.510503
2844.971719	103.249510	55.515508
2844.292876	89.199606	55.520513
2843.206257	94.208884	55.525517
2843.053648	89.362480	55.530522
2842.799196	99.741098	55.535527
2842.293523	93.681252	55.540532
2841.912610	88.428616	55.545537
2840.477474	94.631112	55.550541
2839.754195	92.627165	55.555546
2839.111735	94.728374	55.560551
2838.632342	90.995686	55.565556
2838.042583	87.429094	55.570561
2837.242507	89.884468	55.575565
2836.983139	87.715186	55.580570
2835.619629	91.177883	55.585575
2834.629082	101.159294	55.590580
2834.488463	94.748118	55.595585
2833.794143	98.837348	55.600589
2833.925724	84.382504	55.605594
2833.506366	90.070351	55.610599
2832.336428	92.906298	55.615604
2831.459660	92.041318	55.620609
2830.416698	90.543576	55.625613
2830.229288	80.045912	55.630618
2829.792575	82.924696	55.635623
2828.964453	85.309076	55.640628
2827.894867	85.132691	55.645633
2826.526050	97.871570	55.650637
2826.144950	88.557236	55.655642
2825.861759	90.137977	55.660647
2825.050987	91.469421	55.665652
2824.953084	84.597411	55.670657
2824.618522	92.608728	55.675661
2823.934239	83.984486	55.680666
2823.160474	90.089342	55.685671
2821.998318	85.783762	55.690676
2821.833176	89.054280	55.695681
2821.140939	97.212780	55.700685
2820.161149	81.571079	55.705690
2819.165975	87.131161	55.710695
2818.212793	89.418893	55.715700
2817.853422	85.428466	55.720705
2817.187119	99.530266	55.725709
2816.928946	90.385970	55.730714
2816.444276	89.690815	55.735719
2816.019385	89.179253	55.740724
2815.377059	87.616989	55.745729
2813.706634	90.840443	55.750733
2813.020842	85.535316	55.755738
2812.339528	87.435936	55.760743
2811.907982	90.841588	55.765748
2811.595695	83.678992	55.770753
2810.963902	89.438277	55.775757
2810.620301	95.729740	55.780762
2809.917347	90.910296	55.785767
2808.446402	94.473464	55.790772
2808.224749	79.456517	55.795777
2807.143542	86.324819	55.800781
2807.143014	90.665330	55.805786
2806.397587	91.830481	55.810791
2805.949578	88.647024	55.815796
2804.895114	87.543611	55.820801
2803.871691	98.452721	55.825805
2803.649314	92.348015	55.830810
2803.257409	91.668189	55.835815
2802.585945	98.862772	55.840820
2802.519195	92.947778	55.845825
2800.697398	94.095586	55.850829
2799.806529	82.609369	55.855834
2799.113348	85.320416	55.860839
2798.378451	91.719413	55.865844
2798.320011	94.681966	55.870849
2797.566707	92.219749	55.875853
2797.382301	89.256100	55.880858
2796.979090	85.071069	55.885863
2795.707985	89.787418	55.890868
2795.215004	82.409793	55.895873
2794.136831	89.343894	55.900877
2793.948769	84.606184	55.905882
2793.272422	90.630052	55.910887
2792.441064	95.548342	55.915892
2791.421349	86.627761	55.920897
2790.730278	96.758113	55.925901
2790.169384	82.363212	55.930906
2789.440946	87.158122	55.935911
2788.801500	84.781050	55.940916
2788.774178	89.711912	55.945921
2788.293192	90.207807	55.950925
2787.741219	84.586532	55.955930
2786.803692	88.917852	55.960935
2785.867853	96.227487	55.965940
2785.666934	81.546857	55.970945
2784.001213	92.500613	55.975949
2783.182380	90.535112	55.980954
2782.694920	92.240764	55.985959
2781.627260	90.669887	55.990964
2782.288949	86.717310	55.995969
2781.570250	89.483640	56.000973
2780.737537	80.757282	56.005978
2780.250296	87.018820	56.010983
2779.312422	85.263135	56.015988
2778.445171	80.909531	56.020993
2777.538904	94.534064	56.025997
2776.839310	96.999902	56.031002
2776.590837	87.552780	56.036007
2775.855518	91.140614	56.041012
2775.730984	84.166188	56.046017
2774.761805	91.173239	56.051021
2774.196035	87.001389	56.056026
2773.771429	86.848588	56.061031
2772.637885	89.883582	56.066036
2771.211880	82.694247	56.071041
2771.178015	80.631293	56.076045
2770.443185	87.411977	56.081050
2769.605500	92.632131	56.086055
2768.788249	91.614098	56.091060
2768.434215	80.653093	56.096065
2768.093767	89.921430	56.101069
2767.967688	81.231793	56.106074
2767.207025	81.477868	56.111079
2766.147709	84.466624	56.116084
2765.369803	81.255087	56.121089
2764.649509	87.184233	56.126093
2764.466777	82.218253	56.131098
2763.300519	80.918832	56.136103
2762.060815	83.593034	56.141108
2761.702758	84.273967	56.146113
2760.859432	91.593841	56.151117
2760.629874	80.997603	56.156122
2760.169688	95.287187	56.161127
2759.339221	87.523183	56.166132
2759.195309	84.235257	56.171137
2758.626816	90.763309	56.176141
2757.232768	93.193508	56.181146
2756.888184	85.670922	56.186151
2756.108991	89.507038	56.191156
2755.835346	82.792964	56.196161
2754.585937	95.040531	56.201165
2753.879257	84.790309	56.206170
2753.630272	81.855071	56.211175
2752.575161	85.085865	56.216180
2752.508714	84.267524	56.221185
2751.952005	93.780846	56.226189
2750.796889	92.946877	56.231194
2750.106163	86.187646	56.236199
2749.112550	87.808897	56.241204
2748.984484	82.635818	56.246209
2748.123381	94.860829	56.251213
2747.452111	86.926332	56.256218
2746.520025	85.582152	56.261223
2745.608439	84.564458	56.266228
2745.080077	86.438941	56.271233
2744.387632	87.518072	56.276237
2743.955267	89.138523	56.281242
2743.375636	83.829869	56.286247
2742.997150	92.592749	56.291252
2743.019438	86.913194	56.296257
2742.089239	92.333894	56.301261
2741.178904	87.825822	56.306266
2740.268738	81.442383	56.311271
2739.702446	93.171753	56.316276
2739.480380	86.383338	56.321281
2738.157849	91.544660	56.326285
2737.312430	81.703804	56.331290
2736.750898	84.934708	56.336295
2736.242078	88.451462	56.341300
2735.887735	84.391503	56.346305
2735.298883	83.823501	56.351309
2734.289482	81.191523	56.356314
2733.195687	80.763118	56.361319
2732.637108	89.454544	56.366324
2732.215644	81.426041	56.371329
2731.635909	86.409479	56.376333
2731.172747	85.311588	56.381338
2730.599591	82.443997	56.386343
2729.407218	85.414844	56.391348
2728.792425	87.765141	56.396353
2728.607512	87.132834	56.401357
2728.330738	84.405236	56.406362
2727.473003	79.309906	56.411367
2725.708214	84.557084	56.416372
2725.485994	80.953740	56.421377
2724.610595	84.431707	56.426381
2724.122251	89.000459	56.431386
2723.558557	80.932322	56.436391
2723.353782	86.339945	56.441396
2723.455345	75.969743	56.446401
2722.140082	77.111124	56.451405
2721.435963	82.832643	56.456410
2720.754538	86.360349	56.461415
2719.317368	88.536223	56.466420
2718.443773	86.722194	56.471425
2718.079453	88.399698	56.476429
2718.036012	81.189977	56.481434
2717.122954	80.978175	56.486439
2716.354069	87.806130	56.491444
2716.044356	82.342795	56.496449
2715.298159	88.613862	56.501453
2714.801228	83.306866	56.506458
2713.766753	77.211122	56.511463
2712.717386	81.657089	56.516468
2712.541292	74.838325	56.521473
2711.804135	78.488053	56.526477
2711.450317	74.512085	56.531482
2710.298439	78.077574	56.536487
2709.259907	81.090020	56.541492
2708.748204	76.730920	56.546497
2708.546518	83.983749	56.551501
2707.953676	85.848336	56.556506
2707.922423	74.318241	56.561511
2707.143311	80.441384	56.566516
2706.255417	79.242416	56.571521
2705.083738	85.709364	56.576525
2704.676407	77.166098	56.581530
2704.040001	79.708769	56.586535
2703.266722	88.557285	56.591540
2702.105546	78.811859	56.596545
2701.381971	85.351025	56.601549
2701.046787	83.729566	56.606554
2700.555770	80.246378	56.611559
2700.048725	88.532296	56.616564
2699.717544	81.824906	56.621569
2699.101398	84.416219	56.626573
2697.760693	86.157594	56.631578
2697.501849	81.363705	56.636583
2696.316112	80.925760	56.641588
2696.088456	73.905818	56.646593
2695.389544	80.496028	56.651597
2694.708979	84.322001	56.656602
2693.764777	76.037079	56.661607
2692.956268	80.460035	56.666612
2692.574444	71.832285	56.671617
2691.920032	75.059329	56.676621
2691.555716	82.655736	56.681626
2691.391374	73.502535	56.686631
2690.152636	75.730151	56.691636
2689.632811	70.587335	56.696641
2688.788735	83.089288	56.701645
2688.261264	82.547510	56.706650
2687.755508	86.979111	56.711655
2686.282369	89.409028	56.716660
2685.816860	77.890796	56.721665
2685.011296	84.729363	56.726669
2684.625199	80.486159	56.731674
2684.585392	77.209654	56.736679
2683.924823	85.091958	56.741684
2683.652344	76.117499	56.746689
2682.218318	85.647362	56.751693
2681.360420	80.944427	56.756698
2681.008017	76.372185	56.761703
2679.582252	87.231256	56.766708
2679.383743	78.013238	56.771713
2678.091540	81.724295	56.776717
2678.002969	79.520699	56.781722
2677.483904	71.325346	56.786727
2676.613332	83.419341	56.791732
2676.757448	69.977227	56.796737
2675.993382	81.445534	56.801741
2674.917266	91.948008	56.806746
2674.317498	85.282189	56.811751
2673.330903	87.908012	56.816756
2673.106248	89.384807	56.821761
2672.873665	86.947677	56.826765
2671.666855	86.973589	56.831770
2670.857951	85.308769	56.836775
2669.651463	85.353573	56.841780
2669.484700	78.759395	56.846785
2669.073768	83.101367	56.851789
2668.103001	89.413983	56.856794
2667.402029	80.097913	56.861799
2666.358235	81.192113	56.866804
2666.294344	77.356847	56.871809
2665.264385	79.276420	56.876813
2665.068706	84.320129	56.881818
2664.945511	85.343409	56.886823
2663.726719	89.620983	56.891828
2662.762578	82.034586	56.896833
2662.301514	78.008273	56.901837
2661.912731	78.227898	56.906842
2661.552239	73.127321	56.911847
2660.528935	77.839620	56.916852
2659.891420	77.242052	56.921857
2659.206293	75.492527	56.926861
2658.131181	84.125408	56.931866
2657.928772	78.575846	56.936871
2656.556676	80.204574	56.941876
2655.589854	70.071482	56.946881
2655.998633	81.062997	56.951885
2655.346232	76.227048	56.956890
2654.897366	75.684863	56.961895
2653.883803	80.642201	56.966900
2653.200279	72.758377	56.971905
2652.012395	88.009550	56.976909
2651.585681	83.978154	56.981914
2650.920490	81.318537	56.986919
2650.347845	89.900662	56.991924
2650.114616	79.382042	56.996929
2649.043811	79.453392	57.001933
2648.206880	77.981257	57.006938
2647.571384	76.987042	57.011943
2647.113633	79.694567	57.016948
2646.707159	75.240516	57.021953
2646.128085	82.692849	57.026957
2645.609551	88.774219	57.031962
2644.385818	82.522953	57.036967
2643.423184	86.611483	57.041972
2643.256361	76.405978	57.046977
2642.551876	83.438052	57.051981
2642.016397	79.945499	57.056986
2640.844988	77.162819	57.061991
2639.914352	76.671016	57.066996
2639.990228	75.096134	57.072001
2639.280867	80.595534	57.077005
2638.973383	80.067865	57.082010
2638.400041	79.683138	57.087015
2637.070493	76.529215	57.092020
2636.316122	70.130619	57.097025
2636.033591	77.465155	57.102029
2635.718576	79.744478	57.107034
2634.738715	81.400500	57.112039
2633.523270	83.007191	57.117044
2632.644923	85.728196	57.122049
2632.229249	83.235528	57.127053
2631.689154	85.153471	57.132058
2631.568104	81.821384	57.137063
2630.634357	87.085205	57.142068
2630.479224	74.784083	57.147073
2629.505404	81.952590	57.152077
2628.498419	80.068620	57.157082
2628.093285	82.254799	57.162087
2627.543147	87.383574	57.167092
2627.536671	79.610192	57.172097
2626.042287	86.811243	57.177101
2624.856440	87.364487	57.182106
2624.459667	80.955679	57.187111
2623.720090	84.714774	57.192116
2623.850496	78.989904	57.197121
2623.004946	84.731661	57.202125
2621.569977	92.140446	57.207130
2621.287384	85.626858	57.212135
2620.482804	85.366529	57.217140
2620.007285	87.470007	57.222145
2619.382003	93.074642	57.227149
2618.810586	80.599950	57.232154
2618.180027	77.308385	57.237159
2617.210639	93.127326	57.242164
2616.826641	86.071748	57.247169
2616.332297	86.166136	57.252173
2615.938251	83.777532	57.257178
2615.002136	81.208443	57.262183
2613.922154	85.403482	57.267188
2613.539573	81.085871	57.272193
2613.144905	85.171652	57.277197
2612.303016	84.462189	57.282202
2611.019606	85.274080	57.287207
2610.437720	87.398900	57.292212
2610.042425	74.573196	57.297217
2609.395990	82.706103	57.302221
2608.930491	83.316203	57.307226
2608.791826	76.636704	57.312231
2607.481761	86.188809	57.317236
2606.770221	78.109655	57.322241
2605.790187	77.001453	57.327245
2605.765540	80.350973	57.332250
2605.737523	76.296033	57.337255
2604.179307	82.984988	57.342260
2603.752404	80.375035	57.347265
2602.770280	80.831486	57.352269
2602.123311	84.773693	57.357274
2601.994109	79.359248	57.362279
2600.376236	83.876365	57.367284
2599.842027	77.824204	57.372289
2598.838749	77.380352	57.377293
2598.517434	80.848085	57.382298
2598.353614	74.277096	57.387303
2597.619516	89.055578	57.392308
2597.281324	82.354531	57.397313
2596.827078	83.017970	57.402317
2595.941431	85.030118	57.407322
2594.967158	81.122729	57.412327
2594.204210	86.996021	57.417332
2593.911167	79.317813	57.422337
2592.677387	77.576039	57.427341
2591.740699	85.792513	57.432346
2591.428311	76.239513	57.437351
2590.885044	82.812595	57.442356
2591.182917	78.215248	57.447361
2590.241931	69.074045	57.452365
2588.898064	69.272611	57.457370
2588.514536	76.862824	57.462375
2587.753302	77.739790	57.467380
2587.085199	73.650595	57.472385
2586.646899	81.056758	57.477389
2585.386380	76.523722	57.482394
2584.875746	78.515576	57.487399
2584.267251	84.360885	57.492404
2583.575228	84.204868	57.497409
2583.162320	88.079038	57.502413
2582.562451	80.051059	57.507418
2581.619388	73.470000	57.512423
2580.175084	79.567530	57.517428
2580.077031	75.392726	57.522433
2579.502653	73.430864	57.527437
2579.037565	72.390157	57.532442
2578.902640	80.871396	57.537447
2578.452079	83.976763	57.542452
2578.088394	77.290737	57.547457
2576.872929	80.603837	57.552461
2575.913752	79.311686	57.557466
2575.236406	70.610138	57.562471
2574.516949	84.291146	57.567476
2573.783732	76.589905	57.572481
2573.298669	80.657193	57.577485
2572.243143	82.100773	57.582490
2571.963957	79.470702	57.587495
2570.904931	77.617745	57.592500
2570.560957	71.627804	57.597505
2569.930012	79.880033	57.602509
2569.412248	68.696018	57.607514
2568.923348	69.982732	57.612519
2567.549600	82.866543	57.617524
2566.674271	80.329703	57.622529
2566.129038	78.128393	57.627533
2565.682643	82.275910	57.632538
2565.921594	77.719425	57.637543
2565.073521	82.141263	57.642548
2564.168771	71.570098	57.647553
2563.161890	75.241476	57.652557
2562.265943	76.199895	57.657562
2562.036689	70.219159	57.662567
2561.321269	75.421977	57.667572
2560.662127	71.214811	57.672577
2559.677730	69.924607	57.677581
2558.827441	79.857571	57.682586
2558.171628	66.233290	57.687591
2557.571777	73.402603	57.692596
2557.811942	72.189228	57.697601
2557.407474	76.026033	57.702605
2556.879944	83.912437	57.707610
2555.377903	73.326941	57.712615
2554.315029	72.571191	57.717620
2554.445184	72.192912	57.722625
2552.821153	80.305847	57.727629
2552.017220	77.384579	57.732634
2551.888623	72.082140	57.737639
2550.915985	79.678727	57.742644
2550.909360	68.239181	57.747649
2550.531734	69.274380	57.752653
2550.046131	71.811808	57.757658
2549.248302	75.088645	57.762663
2548.042038	75.943412	57.767668
2547.939199	76.770982	57.772673
2546.643786	72.539966	57.777677
2545.493504	70.294471	57.782682
2544.791427	66.905018	57.787687
2544.179551	83.260442	57.792692
2543.923029	69.417115	57.797697
2543.149483	82.230686	57.802701
2542.806064	81.808636	57.807706
2542.949115	71.948844	57.812711
2541.963173	89.214908	57.817716
2541.142080	81.828291	57.822721
2540.353090	73.880812	57.827725
2539.556828	75.331387	57.832730
2538.712522	71.784676	57.837735
2537.593300	76.147874	57.842740
2536.876506	62.130225	57.847745
2536.679649	71.750560	57.852749
2536.334502	82.086231	57.857754
2536.148254	68.649695	57.862759
2535.412032	75.468519	57.867764
2534.610806	73.915302	57.872769
2533.505698	81.454410	57.877773
2533.027872	83.315926	57.882778
2532.295011	74.178232	57.887783
2531.496762	76.742665	57.892788
2530.722074	69.434567	57.897793
2529.960169	67.126626	57.902797
2529.299128	79.439397	57.907802
2529.413073	70.139962	57.912807
2528.881128	79.634436	57.917812
2527.660728	75.788877	57.922817
2526.912655	73.328576	57.927821
2526.301629	80.848345	57.932826
2525.656503	77.672965	57.937831
2525.012568	82.605416	57.942836
2523.966009	77.519123	57.947841
2523.240924	74.841740	57.952845
2522.231593	75.889811	57.957850
2521.839826	74.562636	57.962855
2521.654248	83.032006	57.967860
2521.303024	71.434277	57.972865
2521.033324	77.604548	57.977869
2519.829851	74.333974	57.982874
2518.985722	76.658760	57.987879
2518.209072	69.477312	57.992884
2518.217787	73.449525	57.997889
2517.184003	72.288558	58.002893
2516.019695	66.063886	58.007898
2515.419732	63.694315	58.012903
2514.739534	69.056897	58.017908
2514.526792	70.949275	58.022913
2514.287778	70.589112	58.027917
2513.491480	70.633294	58.032922
2512.492072	68.741738	58.037927
2511.640972	72.095578	58.042932
2511.591726	71.485873	58.047937
2510.194457	72.878550	58.052941
2509.081466	80.067703	58.057946
2508.593668	70.498131	58.062951
2508.343463	72.002585	58.067956
2507.831283	67.224795	58.072961
2507.666725	75.856351	58.077965
2506.537460	73.136365	58.082970
2506.345481	65.993906	58.087975
2505.357298	79.302839	58.092980
2504.446150	76.417278	58.097985
2504.180577	70.199212	58.102989
2502.633107	70.449186	58.107994
2502.018852	61.542273	58.112999
2501.241889	71.015871	58.118004
2501.319181	66.725835	58.123009
2500.703922	60.482693	58.128013
2499.875785	71.668274	58.133018
2499.908431	74.130522	58.138023
2498.254082	75.125458	58.143028
2497.626835	68.874494	58.148033
2497.328470	64.127648	58.153037
2496.588783	72.034925	58.158042
2496.450153	77.606489	58.163047
2495.347065	71.860022	58.168052
2494.344907	69.404878	58.173057
2493.963045	74.102266	58.178061
2493.200701	76.251236	58.183066
2493.228025	66.477947	58.188071
2491.958167	80.917372	58.193076
2491.032503	71.056755	58.198081
2490.481163	65.279511	58.203085
2489.599028	76.997337	58.208090
2489.198717	75.238614	58.213095
2488.848685	77.838128	58.218100
2488.131979	71.596144	58.223105
2487.205441	74.128438	58.228109
2486.221432	79.150611	58.233114
2486.332679	65.621383	58.238119
2485.841398	76.843320	58.243124
2484.679545	69.624715	58.248129
2483.522411	76.048547	58.253133
2483.053439	77.347649	58.258138
2482.808083	67.983337	58.263143
2482.056495	74.684005	58.268148
2481.779971	72.766360	58.273153
2481.359787	67.207870	58.278157
2480.380494	77.468013	58.283162
2479.886834	68.612718	58.288167
2478.336788	71.274113	58.293172
2477.381035	71.221619	58.298177
2476.774199	66.782901	58.303181
2476.286114	70.601636	58.308186
2475.972098	63.965557	58.313191
2475.463413	67.663475	58.318196
2475.286860	68.043795	58.323201
2474.614077	66.281134	58.328205
2473.601014	66.063181	58.333210
2473.153984	69.060976	58.338215
2472.280338	78.588609	58.343220
2471.525906	70.827075	58.348225
2470.367595	69.251633	58.353229
2469.565053	78.056999	58.358234
2469.285500	74.748075	58.363239
2468.892291	74.145470	58.368244
2468.513827	76.043685	58.373249
2468.299186	77.643899	58.378253
2467.120751	75.415076	58.383258
2466.266360	70.258051	58.388263
2465.571660	73.825938	58.393268
2465.010221	70.311402	58.398273
2463.975154	62.596276	58.403277
2463.218591	71.751398	58.408282
2462.751820	72.064500	58.413287
2461.902001	68.127970	58.418292
2461.498964	61.170020	58.423297
2461.103158	74.430563	58.428301
2460.395525	70.022105	58.433306
2459.794466	59.997851	58.438311
2458.788302	66.004700	58.443316
2458.361033	68.334796	58.448321
2457.977733	69.149531	58.453325
2457.212923	69.731477	58.458330
2455.916213	63.683008	58.463335
2455.672989	68.674838	58.468340
2454.783185	69.361048	58.473345
2455.008910	72.786961	58.478349
2453.788642	68.639831	58.483354
2453.109417	64.738082	58.488359
2452.433692	75.180790	58.493364
2451.998973	72.912443	58.498369
2450.412060	65.051679	58.503373
2449.367764	72.900122	58.508378
2449.651327	72.775077	58.513383
2449.349221	69.590008	58.518388
2448.674879	67.405262	58.523393
2448.486034	67.616769	58.528397
2446.619070	75.677709	58.533402
2446.046170	71.754228	58.538407
2445.289513	78.723785	58.543412
2445.164188	68.573585	58.548417
2444.632708	65.372868	58.553421
2444.092323	74.044598	58.558426
2442.830496	66.414824	58.563431
2442.006792	74.502648	58.568436
2441.611851	70.764655	58.573441
2441.562445	68.477008	58.578445
2440.621714	81.814541	58.583450
2440.265024	75.317990	58.588455
2438.890294	75.648576	58.593460
2438.114366	69.976052	58.598465
2437.770324	66.075020	58.603469
2436.826345	74.784968	58.608474
2436.894640	62.337138	58.613479
2435.447299	66.557115	58.618484
2434.990563	66.377071	58.623489
2433.993080	65.108471	58.628493
2433.603823	73.561341	58.633498
2433.516260	68.704250	58.638503
2433.544267	64.379225	58.643508
2432.046610	62.736291	58.648513
2431.373504	61.530252	58.653517
2430.296541	70.334380	58.658522
2430.119136	67.037206	58.663527
2428.638461	66.489490	58.668532
2428.378431	75.894050	58.673537
2427.464707	70.810333	58.678541
2427.046846	68.569106	58.683546
2426.817691	67.719778	58.688551
2426.223828	75.357793	58.693556
2425.416468	74.374044	58.698561
2424.508732	68.516830	58.703565
2423.755215	68.419898	58.708570
2423.730142	64.169868	58.713575
2422.921833	69.508966	58.718580
2421.773844	69.455009	58.723585
2420.801907	67.079580	58.728589
2420.203216	77.028739	58.733594
2419.984785	68.709402	58.738599
2419.534639	73.045452	58.743604
2418.963043	68.081261	58.748609
2418.346783	64.405981	58.753613
2416.836655	74.534660	58.758618
2416.806490	63.717297	58.763623
2415.837337	73.067845	58.768628
2415.356007	66.560245	58.773633
2415.005282	68.627002	58.778637
2413.533902	69.915534	58.783642
2413.594104	66.311296	58.788647
2412.454418	64.961228	58.793652
2412.503311	65.342869	58.798657
2411.884258	68.042065	58.803661
2410.374088	77.500119	58.808666
2410.099010	68.839955	58.813671
2409.268379	73.840647	58.818676
2408.725596	70.550290	58.823681
2407.521135	69.356162	58.828685
2407.171407	78.536067	58.833690
2406.320931	69.963234	58.838695
2406.073168	69.267083	58.843700
2405.376453	74.430004	58.848705
2405.190082	69.497050	58.853709
2404.618018	68.229133	58.858714
2403.915546	62.647477	58.863719
2402.988541	71.532938	58.868724
2402.207290	71.876132	58.873729
2401.620021	67.527630	58.878733
2400.337842	73.955091	58.883738
2400.027129	75.165167	58.888743
2399.627481	79.015364	58.893748
2399.138949	66.277494	58.898753
2398.595222	59.592285	58.903757
2397.254317	74.855016	58.908762
2396.820185	69.126822	58.913767
2395.950020	64.651040	58.918772
2395.686719	71.287959	58.923777
2395.220107	67.225527	58.928781
2393.958966	70.079906	58.933786
2393.165074	61.230178	58.938791
2392.427732	72.517075	58.943796
2392.023195	73.735695	58.948801
2392.067686	67.796195	58.953805
2391.179905	74.789358	58.958810
2390.135792	69.214409	58.963815
2389.614185	67.354465	58.968820
2388.659463	78.091582	58.973825
2388.611466	67.359766	58.978829
2387.839039	78.765164	58.983834
2387.165148	66.162803	58.988839
2386.343279	76.211698	58.993844
2385.692021	70.383662	58.998849
2385.558298	66.042872	59.003853
2383.798272	76.097054	59.008858
2383.043498	70.520395	59.013863
2382.366799	77.290763	59.018868
2382.126777	72.863940	59.023873
2381.975686	71.310894	59.028877
2381.416254	76.324427	59.033882
2380.830758	62.733172	59.038887
2379.520017	72.237652	59.043892
2378.937170	67.301443	59.048897
2378.726936	64.322507	59.053901
2377.854503	67.302653	59.058906
2377.010288	70.213636	59.063911
2376.009516	68.706406	59.068916
2375.934044	78.026119	59.073921
2375.656370	67.858560	59.078925
2374.114441	68.421428	59.083930
2373.676336	65.710789	59.088935
2372.829914	70.208149	59.093940
2372.099508	67.045797	59.098945
2371.915302	55.474417	59.103949
2371.355068	70.672736	59.108954
2370.126787	58.379910	59.113959
2369.376953	65.521187	59.118964
2368.576859	70.118385	59.123969
2368.388569	61.007616	59.128973
2367.882958	59.502956	59.133978
2367.386343	51.510271	59.138983
2367.220276	62.442120	59.143988
2366.065987	60.269193	59.148993
2365.302543	57.062759	59.153997
2364.483932	58.910321	59.159002
2363.410267	62.795637	59.164007
2362.319244	56.805183	59.169012
2362.010337	61.862713	59.174017
2361.492796	60.610742	59.179021
2360.917524	62.128943	59.184026
2360.904936	60.556558	59.189031
2360.119146	64.141607	59.194036
2359.858893	64.772681	59.199041
2358.910755	62.026103	59.204045
2358.007895	64.349898	59.209050
2357.732696	63.292139	59.214055
2356.701637	63.366223	59.219060
2355.653496	61.745523	59.224065
2354.994793	62.813795	59.229069
2354.138696	67.005321	59.234074
2354.288132	58.465206	59.239079
2353.487306	64.428666	59.244084
2352.315043	68.032828	59.249089
2351.889122	54.400881	59.254093
2351.235136	63.919371	59.259098
2350.627028	57.633983	59.264103
2350.164524	62.605282	59.269108
2348.750871	57.822590	59.274113
2348.540180	59.805405	59.279117
2347.659586	70.978250	59.284122
2347.713347	59.904187	59.289127
2347.214087	66.708156	59.294132
2346.224721	65.190694	59.299137
2345.648115	59.876070	59.304141
2344.580159	70.685439	59.309146
2344.487068	59.502282	59.314151
2343.382082	62.501277	59.319156
2342.292088	59.830274	59.324161
2342.242413	57.502416	59.329165
2341.809715	48.982115	59.334170
2340.799780	55.795248	59.339175
2339.841347	59.703098	59.344180
2339.433223	59.711718	59.349185
2338.995325	56.808425	59.354189
2337.907758	60.881641	59.359194
2337.482256	54.776209	59.364199
2336.564770	60.106350	59.369204
2335.829436	56.996953	59.374209
2335.329025	51.151822	59.379213
2334.702761	48.278373	59.384218
2334.393939	55.382919	59.389223
2333.198643	56.748600	59.394228
2331.959704	61.301633	59.399233
2331.997493	57.223617	59.404237
2331.431261	51.830648	59.409242
2331.177770	56.391218	59.414247
2330.360537	56.857018	59.419252
2329.527445	60.105169	59.424257
2328.795675	54.069477	59.429261
2327.810716	61.756996	59.434266
2327.507330	58.208619	59.439271
2327.267768	56.597287	59.444276
2326.470195	48.554237	59.449281
2325.481490	52.687914	59.454285
2324.640161	67.149584	59.459290
2324.107309	56.964493	59.464295
2323.668621	54.662105	59.469300
2323.090384	63.278331	59.474305
2322.286083	55.398659	59.479309
2321.206905	53.068826	59.484314
2320.997615	58.167346	59.489319
2320.641949	61.978442	59.494324
2319.774454	68.260006	59.499329
2319.256017	64.969052	59.504333
2318.229787	63.232512	59.509338
2317.540026	62.560239	59.514343
2316.895957	61.445958	59.519348
2315.725535	68.766130	59.524353
2315.213572	67.524657	59.529357
2314.219275	65.131758	59.534362
2313.814002	60.740703	59.539367
2313.706052	69.338879	59.544372
2313.240028	66.312111	59.549377
2313.047883	60.370453	59.554381
2311.826323	63.772270	59.559386
2311.433798	57.755934	59.564391
2310.661837	56.753126	59.569396
2309.475801	58.264854	59.574401
2309.191470	61.577454	59.579405
2308.276605	64.601574	59.584410
2307.509203	58.982884	59.589415
2306.689416	52.766860	59.594420
2306.410418	59.848151	59.599425
2306.133647	59.500770	59.604429
2304.862540	61.633737	59.609434
2304.002509	58.985389	59.614439
2303.687779	58.731339	59.619444
2303.143242	58.554480	59.624449
2302.821704	52.397329	59.629453
2301.696211	61.687378	59.634458
2300.932721	55.534357	59.639463
2300.405230	62.795900	59.644468
2299.850933	65.741785	59.649473
2299.520286	57.172853	59.654477
2298.127211	65.902369	59.659482
2297.735635	58.328690	59.664487
2296.708551	59.034846	59.669492
2296.460451	58.090479	59.674497
2296.309766	59.756335	59.679501
2294.985563	61.819833	59.684506
2294.637591	53.721613	59.689511
2293.811307	57.594635	59.694516
2293.013721	59.192698	59.699521
2293.139061	56.110597	59.704525
2292.182670	65.559227	59.709530
2291.107723	55.455397	59.714535
2290.968483	52.437488	59.719540
2289.716868	53.415717	59.724545
2289.132352	64.239123	59.729549
2287.919440	68.554434	59.734554
2287.726544	62.005427	59.739559
2287.271002	65.577429	59.744564
2286.283128	71.515648	59.749569
2286.095941	60.698709	59.754573
2285.232969	64.257097	59.759578
2284.550934	66.008686	59.764583
2283.826151	67.653510	59.769588
2283.674251	65.821538	59.774593
2282.989875	60.261284	59.779597
2281.531955	61.020593	59.784602
2281.220594	51.338803	59.789607
2280.598811	61.087040	59.794612
2280.172762	55.357090	59.799617
2279.680457	65.430939	59.804621
2278.047025	58.289095	59.809626
2277.687700	60.547583	59.814631
2277.357787	59.197617	59.819636
2276.785687	72.593683	59.824641
2276.352044	57.296945	59.829645
2275.038782	70.728967	59.834650
2274.254919	61.221523	59.839655
2274.050305	58.824245	59.844660
2273.598905	61.442283	59.849665
2273.336959	58.409832	59.854669
2271.971292	62.880341	59.859674
2271.522756	61.002786	59.864679
2270.853527	61.022510	59.869684
2270.074633	65.341363	59.874689
2269.221402	59.034751	59.879693
2268.051248	69.551745	59.884698
2267.840259	52.009253	59.889703
2267.166532	62.350957	59.894708
2266.739513	69.571244	59.899713
2267.009489	59.374395	59.904718
2265.500961	71.557356	59.909722
2264.705186	58.101565	59.914727
2264.307729	60.760508	59.919732
2263.789506	67.755216	59.924737
2262.694728	58.912371	59.929742
2261.822634	64.529618	59.934746
2261.174609	60.208107	59.939751
2261.136939	68.997543	59.944756
2260.439471	60.286485	59.949761
2259.040512	54.926198	59.954766
2258.486580	61.229929	59.959770
2257.976019	59.721390	59.964775
2257.376997	61.854297	59.969780
2256.869621	64.443621	59.974785
2256.389780	57.100957	59.979790
2255.491111	69.944993	59.984794
2254.420042	49.091422	59.989799
2253.977882	62.753010	59.994804
2253.080553	56.230926	59.999809
2252.897767	58.257127	60.004814
2252.207095	58.674849	60.009818
2252.151325	55.563328	60.014823
2250.799454	60.279761	60.019828
2249.979277	66.944409	60.024833
2249.882627	56.040946	60.029838
2249.238118	62.670814	60.034842
2248.335511	60.529872	60.039847
2247.164766	54.621369	60.044852
2246.654314	66.696012	60.049857
2246.019373	63.871424	60.054862
2245.523085	56.760119	60.059866
2245.432274	58.500206	60.064871
2244.467499	57.173552	60.069876
2243.812708	63.192964	60.074881
2243.576366	53.781761	60.079886
2242.489844	64.228401	60.084890
2240.940723	55.747070	60.089895
2240.298605	64.960385	60.094900
2240.026738	62.680001	60.099905
2239.804981	58.015607	60.104910
2239.080430	67.999310	60.109914
2238.854195	62.175195	60.114919
2238.408026	56.181859	60.119924
2236.818471	66.365987	60.124929
2237.008237	60.720195	60.129934
2235.939215	63.924235	60.134938
2234.897325	64.865427	60.139943
2233.936235	64.846255	60.144948
2233.312774	63.583202	60.149953
2233.074834	58.721846	60.154958
2232.674366	66.772035	60.159962
2232.218048	60.934771	60.164967
2231.370388	60.714629	60.169972
2230.593910	55.859323	60.174977
2229.987846	62.226837	60.179982
2228.593421	68.255114	60.184986
2227.927586	62.062510	60.189991
2227.191363	65.394763	60.194996
2226.813873	68.403966	60.200001
2226.983986	63.251386	60.205006
2226.480894	67.742544	60.210010
2225.213246	65.681795	60.215015
2224.164987	65.416226	60.220020
2223.309542	65.613850	60.225025
2223.163197	68.898118	60.230030
2222.541877	65.580562	60.235034
2222.063459	60.024964	60.240039
2221.316923	57.288936	60.245044
2220.112834	64.942102	60.250049
2219.901350	53.665534	60.255054
2219.334715	62.443981	60.260058
2218.799030	58.705218	60.265063
2217.771017	58.948933	60.270068
2216.635870	66.031383	60.275073
2216.540431	65.724441	60.280078
2215.934279	66.048373	60.285082
2215.879698	55.316529	60.290087
2214.534432	61.763883	60.295092
2213.452520	60.044388	60.300097
2213.624504	50.013511	60.305102
2212.729770	62.628720	60.310106
2211.874518	64.234288	60.315111
2210.990849	65.689985	60.320116
2210.001554	65.460517	60.325121
2210.028411	61.131752	60.330126
2209.399855	57.655180	60.335130
2209.295382	59.205374	60.340135
2207.979395	60.273969	60.345140
2207.096063	63.516913	60.350145
2206.921956	53.433122	60.355150
2205.891767	54.477708	60.360154
2205.646460	53.860093	60.365159
2204.173577	54.515801	60.370164
2203.656802	57.130023	60.375169
2203.416552	55.014756	60.380174
2202.740204	51.185979	60.385178
2202.275117	51.206719	60.390183
2201.773876	54.449445	60.395188
2200.600795	63.945795	60.400193
2200.435358	52.570964	60.405198
2199.390865	62.695431	60.410202
2198.366323	56.298533	60.415207
2197.774314	62.843639	60.420212
2196.801843	55.953117	60.425217
2196.623324	52.487606	60.430222
2196.006789	53.805253	60.435226
2195.790475	50.538436	60.440231
2195.278493	57.760617	60.445236
2194.147681	58.233488	60.450241
2193.746455	53.044813	60.455246
2192.907886	58.439628	60.460250
2191.931659	53.306266	60.465255
2191.050546	51.759270	60.470260
2190.470958	60.756633	60.475265
2190.003350	60.021912	60.480270
2189.389611	53.568971	60.485274
2189.190351	54.060547	60.490279
2188.544237	56.378743	60.495284
2187.227922	53.054929	60.500289
2186.591765	46.294785	60.505294
2186.101651	58.761058	60.510298
2185.816920	54.123229	60.515303
2184.946842	55.111227	60.520308
2183.855536	66.257350	60.525313
2183.489107	60.255910	60.530318
2182.301780	59.004433	60.535322
2182.227583	57.502587	60.540327
2182.097663	52.320406	60.545332
2180.766991	58.901843	60.550337
2180.027801	56.224564	60.555342
2179.401082	59.438228	60.560346
2179.253785	59.108578	60.565351
2178.780442	58.593120	60.570356
2177.264543	56.086965	60.575361
2176.482390	55.870234	60.580366
2175.818949	63.109242	60.585370
2175.581687	57.087687	60.590375
2175.052472	63.834415	60.595380
2174.489631	61.471568	60.600385
2174.425585	58.292389	60.605390
2172.888006	65.344595	60.610394
2172.414798	58.812755	60.615399
2171.665296	56.247368	60.620404
2170.312524	59.952298	60.625409
2169.865705	56.809769	60.630414
2169.416115	66.864469	60.635418
2168.967107	67.609936	60.640423
2168.695705	56.267835	60.645428
2168.073099	64.977306	60.650433
2167.141172	54.270392	60.655438
2166.110767	60.346153	60.660442
2165.986956	61.729924	60.665447
2165.484356	55.829932	60.670452
2164.180448	57.210276	60.675457
2163.440046	49.821803	60.680462
2162.470852	55.010811	60.685466
2162.152104	53.743415	60.690471
2162.147473	48.080353	60.695476
2161.566604	54.205540	60.700481
2160.442025	51.212086	60.705486
2159.406105	62.456890	60.710490
2158.931005	55.196324	60.715495
2159.150724	61.028281	60.720500
2158.159458	64.517445	60.725505
2157.359367	56.506439	60.730510
2156.147011	53.468789	60.735514
2155.657473	54.238161	60.740519
2155.148264	60.501485	60.745524
2154.400425	62.813795	60.750529
2153.400955	48.460154	60.755534
2152.890936	54.662431	60.760538
2152.444073	49.461437	60.765543
2152.443104	50.648941	60.770548
2150.923443	60.321408	60.775553
2150.467145	49.081199	60.780558
2149.669658	57.921231	60.785562
2149.109642	56.417610	60.790567
2148.950976	50.170258	60.795572
2147.906686	53.848483	60.800577
2147.007310	48.596994	60.805582
2145.628580	55.186260	60.810586
2145.463720	50.304917	60.815591
2145.341394	51.891320	60.820596
2144.913360	61.707865	60.825601
2144.369691	56.769338	60.830606
2142.920899	58.922071	60.835610
2142.205031	53.062506	60.840615
2142.078768	63.452284	60.845620
2141.318098	60.567508	60.850625
2141.142253	55.238059	60.855630
2140.083170	58.865134	60.860634
2139.347314	49.838187	60.865639
2138.831295	55.220074	60.870644
2137.776673	57.294735	60.875649
2137.006169	54.910965	60.880654
2136.258470	62.628579	60.885658
2135.839779	59.129546	60.890663
2135.512159	57.920904	60.895668
2134.706783	60.251740	60.900673
2134.591296	54.320675	60.905678
2133.315600	56.714189	60.910682
2132.597419	59.276814	60.915687
2132.163857	59.764255	60.920692
2131.547870	57.651680	60.925697
2130.569413	57.267221	60.930702
2130.394646	60.043603	60.935706
2129.930937	59.946487	60.940711
2128.557712	61.947356	60.945716
2127.417332	62.365432	60.950721
2127.235486	59.747567	60.955726
2126.344418	68.068368	60.960730
2126.083604	65.819259	60.965735
2125.639461	59.023517	60.970740
2125.413135	61.568332	60.975745
2124.694048	61.333716	60.980750
2123.692456	63.239447	60.985754
2122.525848	60.008856	60.990759
2121.193128	59.628545	60.995764
2121.075584	68.902928	61.000769
2120.566102	55.785043	61.005774
2119.409742	57.880660	61.010778
2119.073021	59.970690	61.015783
2118.860776	57.317369	61.020788
2118.163822	60.048463	61.025793
2117.984692	54.382091	61.030798
2117.499550	53.339729	61.035802
2116.498438	60.084672	61.040807
2116.066168	52.674689	61.045812
2114.381013	58.055235	61.050817
2113.668358	50.974647	61.055822
2113.265952	58.448867	61.060826
2112.854588	56.647073	61.065831
2112.672377	55.007788	61.070836
2111.830408	63.502551	61.075841
2110.983277	56.083396	61.080846
2110.080994	64.091521	61.085850
2109.423596	63.980562	61.090855
2109.227537	53.187277	61.095860
2108.689483	57.723494	61.100865
2107.380006	52.496761	61.105870
2106.590086	59.543070	61.110874
2106.237587	53.649388	61.115879
2105.934221	55.228073	61.120884
2104.919039	61.425971	61.125889
2104.366938	50.318205	61.130894
2103.435977	57.505474	61.135898
2102.810721	62.043581	61.140903
2102.507193	56.502298	61.145908
2101.489410	56.947172	61.150913
2100.963893	52.000813	61.155918
2100.105392	62.451094	61.160922
2099.511988	58.282104	61.165927
2098.958822	55.861168	61.170932
2098.511263	64.061508	61.175937
2097.571918	48.345679	61.180942
2096.681046	59.335554	61.185946
2096.414748	59.379931	61.190951
2095.720380	54.674023	61.195956
2095.484447	60.890212	61.200961
2094.437942	50.060820	61.205966
2093.670657	56.920105	61.210970
2092.936673	57.240653	61.215975
2092.670277	57.767003	61.220980
2091.519163	57.521027	61.225985
2090.667116	53.880603	61.230990
2090.096719	53.868840	61.235994
2089.394328	53.898601	61.240999
2089.112112	53.610977	61.246004
2088.608583	62.069169	61.251009
2088.701405	52.233808	61.256014
2087.468507	54.819346	61.261018
2086.006317	58.487353	61.266023
2085.999813	49.266987	61.271028
2084.683809	56.111973	61.276033
2083.858871	54.625253	61.281038
2083.352004	58.682076	61.286042
2083.115637	57.560063	61.291047
2083.117699	48.323233	61.296052
2082.216414	59.149106	61.301057
2081.141180	53.883895	61.306062
2080.121994	63.838655	61.311066
2079.509104	52.915757	61.316071
2079.227074	50.909483	61.321076
2078.502543	60.811080	61.326081
2078.221649	56.437858	61.331086
2077.420179	55.406187	61.336090
2076.710033	53.243411	61.341095
2076.180042	53.642750	61.346100
2074.774103	63.917468	61.351105
2074.322764	45.851291	61.356110
2073.560767	56.324929	61.361114
2073.103913	45.971773	61.366119
2072.849470	46.413977	61.371124
2072.229962	57.542955	61.376129
2071.396881	53.248000	61.381134
2070.426373	54.576865	61.386138
2069.770171	56.508787	61.391143
2069.711680	61.412173	61.396148
2068.559227	54.900220	61.401153
2068.318352	48.484182	61.406158
2067.262710	51.402153	61.411162
2066.334269	56.262110	61.416167
2066.307353	55.531361	61.421172
2065.434292	62.922672	61.426177
2064.908058	57.434485	61.431182
2064.162705	62.998494	61.436186
2063.098550	61.596509	61.441191
2062.399282	51.700852	61.446196
2061.419329	54.045374	61.451201
2060.638483	46.579373	61.456206
2060.421224	63.207100	61.461210
2060.278288	51.953964	61.466215
2059.722152	49.103691	61.471220
2058.984480	56.833406	61.476225
2058.278776	56.307969	61.481230
2057.319790	56.967786	61.486234
2056.424845	61.775833	61.491239
2056.072820	52.552202	61.496244
2055.560746	57.321601	61.501249
2054.771927	51.279934	61.506254
2053.762121	45.129628	61.511258
2053.181666	50.887262	61.516263
2052.863255	48.416705	61.521268
2052.266161	58.164271	61.526273
2051.783864	60.276836	61.531278
2050.495212	50.420420	61.536282
2049.914741	55.649526	61.541287
2049.708572	48.200882	61.546292
2049.137504	60.246803	61.551297
2047.971107	50.105408	61.556302
2047.047117	56.381656	61.561306
2046.746669	52.144410	61.566311
2046.204541	53.483291	61.571316
2045.457321	61.016097	61.576321
2045.415149	51.816045	61.581326
2044.065560	52.466100	61.586330
2043.714752	50.749083	61.591335
2043.173208	48.705495	61.596340
2041.941520	59.788403	61.601345
2041.448141	48.924019	61.606350
2040.374180	42.406153	61.611354
2039.796312	50.784296	61.616359
2039.600218	47.366012	61.621364
2039.020663	57.412539	61.626369
2038.389107	54.727530	61.631374
2037.414899	54.386177	61.636378
2036.571486	58.608723	61.641383
2036.158211	44.728387	61.646388
2035.610848	52.263319	61.651393
2035.564533	47.238160	61.656398
2034.219413	55.883329	61.661402
2033.454998	54.713884	61.666407
2032.852510	53.371484	61.671412
2032.278011	58.136957	61.676417
2032.105510	54.133211	61.681422
2030.801362	51.438520	61.686426
2029.983590	45.769299	61.691431
2029.468434	51.993378	61.696436
2028.723931	59.558877	61.701441
2028.805627	51.638247	61.706446
2027.755612	57.057009	61.711450
2026.830712	57.572058	61.716455
2026.552600	51.208970	61.721460
2025.767954	59.277106	61.726465
2025.420093	53.389351	61.731470
2024.979905	58.943397	61.736474
2024.047127	60.159242	61.741479
2022.880288	50.032140	61.746484
2021.375999	57.907201	61.751489
2020.987648	57.903778	61.756494
2021.196523	53.031144	61.761498
2020.695309	54.931823	61.766503
2020.114542	51.595523	61.771508
2019.169426	51.862199	61.776513
2018.705716	53.392924	61.781518
2017.722317	56.199472	61.786522
2017.211980	54.685791	61.791527
2016.920568	48.573654	61.796532
2015.345590	53.645653	61.801537
2014.623995	51.611157	61.806542
2014.044362	47.961255	61.811546
2013.478628	55.973787	61.816551
2013.467407	48.076553	61.821556
2012.673518	52.899289	61.826561
2012.114524	52.163639	61.831566
2011.304896	57.601676	61.836570
2010.457090	61.528936	61.841575
2010.557030	49.278643	61.846580
2008.489706	58.043012	61.851585
2007.560712	55.106530	61.856590
2007.249044	49.015622	61.861594
2007.008343	56.465732	61.866599
2006.535479	49.400595	61.871604
2005.900092	60.296642	61.876609
2005.719390	49.483380	61.881614
2004.928654	55.653158	61.886618
2003.702563	58.550958	61.891623
2003.771596	52.876487	61.896628
2002.712870	51.297146	61.901633
2001.931671	54.939865	61.906638
2001.339283	55.694081	61.911642
2000.654621	55.438594	61.916647
2000.684857	50.321003	61.921652
1999.386137	55.442062	61.926657
1998.469250	53.341110	61.931662
1997.820781	57.376372	61.936666
1997.130591	52.721081	61.941671
1996.376607	45.772716	61.946676
1995.078048	49.480644	61.951681
1994.927277	40.542329	61.956686
1994.029501	46.280826	61.961690
1993.465738	51.234323	61.966695
1993.606256	48.181998	61.971700
1992.998153	50.842644	61.976705
1992.728848	54.854887	61.981710
1992.023867	51.181432	61.986714
1990.997351	48.267952	61.991719
1990.171247	46.903022	61.996724
1988.536613	52.576919	62.001729
1988.181757	54.073631	62.006734
1987.703650	33.161788	62.011738
1987.026736	50.715587	62.016743
1987.227405	48.421889	62.021748
1986.450944	56.562044	62.026753
1986.060658	46.726050	62.031758
1984.750474	52.039722	62.036762
1983.852182	54.747246	62.041767
1983.896822	48.287903	62.046772
1982.153863	53.721789	62.051777
1981.660887	46.859826	62.056782
1981.229957	44.532072	62.061786
1980.353113	52.580453	62.066791
1980.474809	45.481508	62.071796
1980.079152	55.704199	62.076801
1979.118419	49.896818	62.081806
1978.029303	53.198279	62.086810
1977.452404	55.455316	62.091815
1977.262663	51.578072	62.096820
1975.671537	52.227226	62.101825
1975.111171	44.991940	62.106830
1974.666912	51.465987	62.111834
1974.062111	53.508331	62.116839
1973.530612	46.588620	62.121844
1972.852019	59.313301	62.126849
1972.663945	42.391418	62.131854
1971.496729	50.000411	62.136858
1971.129947	52.773719	62.141863
1970.503249	41.373236	62.146868
1968.925240	43.448644	62.151873
1968.515704	50.446862	62.156878
1968.184575	42.283846	62.161882
1967.393316	53.530618	62.166887
1967.216657	47.903707	62.171892
1966.314959	44.967302	62.176897
1965.567132	45.639168	62.181902
1964.341888	45.131570	62.186906
1963.751725	51.033758	62.191911
1963.712686	51.043213	62.196916
1962.988850	48.008885	62.201921
1962.836050	44.371236	62.206926
1962.052059	50.226847	62.211930
1961.041230	47.273192	62.216935
1960.697687	53.810140	62.221940
1959.134240	59.124118	62.226945
1958.533550	50.073697	62.231950
1957.934015	49.396301	62.236954
1957.323374	53.809158	62.241959
1957.292252	43.282940	62.246964
1956.494469	48.858684	62.251969
1955.897608	48.268460	62.256974
1954.931419	44.844557	62.261978
1954.084402	43.911484	62.266983
1953.823438	47.514157	62.271988
1953.351037	50.395924	62.276993
1952.722269	45.946444	62.281998
1951.763848	45.024534	62.287002
1950.908018	50.666655	62.292007
1950.653383	44.362718	62.297012
1949.349623	38.454562	62.302017
1948.591562	46.880896	62.307022
1948.096978	46.800524	62.312026
1947.526457	44.228637	62.317031
1947.345682	40.008826	62.322036
1946.570911	55.631420	62.327041
1946.085648	47.912387	62.332046
1944.960198	43.408933	62.337050
1944.856757	49.606001	62.342055
1944.459002	44.498870	62.347060
1942.803105	42.514089	62.352065
1942.210755	44.787980	62.357070
1941.767822	51.798227	62.362074
1940.834560	52.508924	62.367079
1941.045643	35.011161	62.372084
1939.947515	44.689700	62.377089
1938.615722	42.510534	62.382094
1938.178280	39.756416	62.387098
1937.509200	52.425781	62.392103
1937.260038	43.525224	62.397108
1936.504218	48.143698	62.402113
1936.491767	42.524226	62.407118
1935.368468	37.843573	62.412122
1934.620119	41.678036	62.417127
1933.894699	45.261088	62.422132
1932.525461	42.894127	62.427137
1931.785538	39.645067	62.432142
1932.101652	42.133795	62.437146
1931.119658	47.380674	62.442151
1930.698170	38.937872	62.447156
1930.665506	48.807156	62.452161
1929.413556	30.582748	62.457166
1928.418068	39.216268	62.462170
1927.688567	39.385288	62.467175
1927.343339	41.929523	62.472180
1926.660413	41.556123	62.477185
1925.975915	44.133925	62.482190
1925.142888	47.539605	62.487194
1924.214543	46.834389	62.492199
1924.012299	38.266454	62.497204
1923.410530	39.522393	62.502209
1923.303060	43.342349	62.507214
1922.344551	46.666474	62.512218
1921.439444	49.708711	62.517223
1920.615684	42.988608	62.522228
1919.325518	48.367942	62.527233
1918.737634	42.773099	62.532238
1918.576786	50.980433	62.537242
1917.988518	55.603009	62.542247
1917.538429	45.858177	62.547252
1917.153927	47.552982	62.552257
1916.427876	47.256037	62.557262
1915.522507	45.880998	62.562266
1914.937213	47.307403	62.567271
1913.851465	35.059059	62.572276
1912.875635	47.379466	62.577281
1912.623581	44.287727	62.582286
1911.855803	43.133482	62.587290
1910.766861	45.627325	62.592295
1911.075171	38.681190	62.597300
1910.568689	47.954584	62.602305
1909.658720	37.647405	62.607310
1908.969909	35.765603	62.612314
1908.331880	49.378167	62.617319
1908.017099	42.184562	62.622324
1906.884343	48.126288	62.627329
1905.723057	35.629959	62.632334
1905.487569	38.046083	62.637338
1904.950038	47.684773	62.642343
1904.062511	38.705150	62.647348
1903.088208	46.603635	62.652353
1902.362019	39.555806	62.657358
1901.886332	48.824721	62.662362
1901.238199	44.598422	62.667367
1901.371770	44.928071	62.672372
1900.321749	46.006103	62.677377
1899.424829	45.786548	62.682382
1898.757441	45.333918	62.687386
1898.400989	53.148022	62.692391
1898.239074	46.324169	62.697396
1896.794678	43.300629	62.702401
1896.126392	42.361857	62.707406
1895.561763	46.076477	62.712410
1894.850398	41.216024	62.717415
1894.544732	40.723221	62.722420
1893.086301	45.250724	62.727425
1892.234671	48.735772	62.732430
1891.995191	40.634060	62.737434
1891.331088	45.523809	62.742439
1890.976133	45.099831	62.747444
1890.673467	47.356535	62.752449
1890.229449	44.699464	62.757454
1889.447488	40.491327	62.762458
1888.551100	39.383561	62.767463
1887.718858	38.937426	62.772468
1886.663095	43.488801	62.777473
1886.258642	44.269690	62.782478
1886.292991	40.664764	62.787482
1885.084677	46.447716	62.792487
1883.862767	44.759351	62.797492
1883.057484	43.637973	62.802497
1882.825726	47.728261	62.807502
1883.038700	36.901360	62.812506
1882.157189	45.023961	62.817511
1880.907992	37.852070	62.822516
1880.068205	45.408609	62.827521
1879.197359	43.460851	62.832526
1878.900952	40.631693	62.837530
1878.437360	41.940968	62.842535
1878.189087	40.069061	62.847540
1877.338304	47.795240	62.852545
1876.506653	39.406829	62.857550
1876.246313	48.538248	62.862554
1874.822867	49.717276	62.867559
1873.913511	45.381730	62.872564
1873.241017	49.567157	62.877569
1873.020751	47.351393	62.882574
1872.883387	40.184281	62.887578
1872.056830	46.765572	62.892583
1871.234675	42.313271	62.897588
1870.106711	45.780863	62.902593
1869.871369	48.285776	62.907598
1869.174058	42.592825	62.912602
1868.733995	48.021724	62.917607
1868.057217	44.562931	62.922612
1867.105711	44.098126	62.927617
1866.774348	40.448798	62.932622
1865.669905	44.975349	62.937626
1864.410536	51.602664	62.942631
1864.443692	43.730616	62.947636
1863.798373	45.392285	62.952641
1863.164658	44.848639	62.957646
1862.882258	41.308167	62.962650
1862.079817	43.703268	62.967655
1861.145118	40.961997	62.972660
1860.029561	54.286014	62.977665
1859.367684	55.002398	62.982670
1859.276059	54.125624	62.987674
1858.552429	51.391266	62.992679
1858.585099	52.265918	62.997684
1857.473746	51.880170	63.002689
1856.306735	43.912280	63.007694
1856.419788	45.988919	63.012698
1855.511485	50.954792	63.017703
1854.742198	41.681015	63.022708
1853.844677	51.685231	63.027713
1853.387312	56.358834	63.032718
1852.839570	45.118546	63.037722
1851.351664	57.573150	63.042727
1850.788100	45.312452	63.047732
1849.972222	42.011667	63.052737
1849.605490	46.200438	63.057742
1849.350206	30.816479	63.062746
1848.423761	49.242659	63.067751
1848.837302	43.397159	63.072756
1848.221215	56.192849	63.077761
1847.391493	51.148186	63.082766
1846.555685	46.265611	63.087770
1844.942905	51.465692	63.092775
1844.007700	39.182139	63.097780
1843.512008	56.003906	63.102785
1843.021824	51.617966	63.107790
1842.703418	43.046624	63.112794
1842.281375	49.017945	63.117799
1841.862123	39.111546	63.122804
1840.633106	45.869059	63.127809
1840.210108	46.255246	63.132814
1839.431310	45.582089	63.137818
1838.914702	41.845646	63.142823
1838.093620	39.225857	63.147828
1837.137108	42.934504	63.152833
1836.521554	48.993009	63.157838
1836.058601	49.168935	63.162842
1835.684500	49.435051	63.167847
1835.424625	44.434207	63.172852
1833.980850	48.082543	63.177857
1833.372095	48.142499	63.182862
1833.192500	34.295658	63.187866
1832.324331	46.989212	63.192871
1831.107255	41.654000	63.197876
1830.428917	53.185785	63.202881
1829.731769	43.302064	63.207886
1829.543609	45.917322	63.212890
1829.159837	46.454292	63.217895
1828.725945	41.217576	63.222900
1827.396150	43.278581	63.227905
1826.617214	41.439051	63.232910
1826.247724	44.050991	63.237914
1825.787140	48.362395	63.242919
1825.305292	40.680302	63.247924
1824.146327	49.184313	63.252929
1823.728309	45.924405	63.257934
1823.328881	42.653422	63.262938
1822.202961	46.817354	63.267943
1821.644112	41.786352	63.272948
1820.950867	44.566180	63.277953
1819.829564	39.491285	63.282958
1819.648465	41.453256	63.287962
1818.480174	43.712806	63.292967
1818.096785	36.221888	63.297972
1817.399536	39.464223	63.302977
1816.824466	44.107438	63.307982
1816.638177	43.218837	63.312986
1815.999867	47.047117	63.317991
1815.004642	40.860829	63.322996
1814.732320	47.563212	63.328001
1813.861839	46.657465	63.333006
1813.020491	40.002369	63.338010
1812.179748	44.935765	63.343015
1811.765193	42.982186	63.348020
1810.876906	49.336818	63.353025
1810.780990	49.700597	63.358030
1809.761970	43.326545	63.363034
1808.963804	46.060776	63.368039
1808.404632	47.728238	63.373044
1807.567495	44.600038	63.378049
1807.191756	47.515010	63.383054
1806.316139	43.927229	63.388058
1805.262003	50.914160	63.393063
1805.042858	46.232390	63.398068
1804.625426	50.280239	63.403073
1803.962074	54.660679	63.408078
1803.101555	44.156784	63.413082
1801.784741	48.665605	63.418087
1801.159996	42.575399	63.423092
1800.559012	41.014492	63.428097
1800.473685	41.398958	63.433102
1800.134291	40.350245	63.438106
1799.615686	45.831660	63.443111
1798.520669	43.510578	63.448116
1797.909985	46.628374	63.453121
1797.363894	52.590921	63.458126
1796.902874	35.991693	63.463130
1795.659479	50.217020	63.468135
1795.031479	41.283806	63.473140
1795.088620	49.878159	63.478145
1793.723679	54.793491	63.483150
1793.269046	40.947527	63.488154
1792.490644	50.486515	63.493159
1791.950338	48.152627	63.498164
1791.649110	45.720994	63.503169
1790.269325	37.128772	63.508174
1789.062853	36.851678	63.513178
1788.399793	45.361235	63.518183
1788.527080	36.566418	63.523188
1787.907770	42.975682	63.528193
1787.224056	41.412354	63.533198
1787.027058	33.174318	63.538202
1786.243935	48.814119	63.543207
1785.312657	37.459876	63.548212
1784.793906	46.984830	63.553217
1784.282821	49.548766	63.558222
1782.968498	42.638694	63.563226
1782.189966	45.079449	63.568231
1781.820095	47.106876	63.573236
1781.113009	43.741306	63.578241
1780.783466	39.022774	63.583246
1780.472541	37.237381	63.588250
1779.214706	45.398723	63.593255
1778.299037	44.581632	63.598260
1777.523725	32.870329	63.603265
1777.102271	37.119381	63.608270
1777.248258	41.917108	63.613274
1776.691711	39.103654	63.618279
1775.490901	45.261508	63.623284
1775.233582	50.630722	63.628289
1773.826761	41.454206	63.633294
1773.051951	38.837959	63.638298
1772.109720	46.485453	63.643303
1772.098308	45.299312	63.648308
1771.360559	44.855579	63.653313
1770.802489	38.470563	63.658318
1770.403732	42.444167	63.663322
1768.864851	43.428639	63.668327
1768.558432	40.830141	63.673332
1767.943136	40.165334	63.678337
1767.667278	45.129972	63.683342
1767.368481	40.853793	63.688346
1765.694127	46.562959	63.693351
1765.077162	32.629131	63.698356
1764.699402	43.871070	63.703361
1764.258585	41.672920	63.708366
1763.816817	41.442219	63.713370
1762.514071	47.863428	63.718375
1762.025925	47.264494	63.723380
1761.337980	48.089951	63.728385
1760.885651	49.880446	63.733390
1760.485701	45.180277	63.738394
1759.369814	46.967076	63.743399
1759.109902	50.272741	63.748404
1758.472531	47.355886	63.753409
1757.507692	43.514182	63.758414
1757.033719	40.222805	63.763418
1755.937755	48.855777	63.768423
1755.319848	39.390736	63.773428
1754.761971	40.835359	63.778433
1754.400975	56.065058	63.783438
1753.719237	47.002892	63.788442
1752.768396	50.455593	63.793447
1751.842444	44.510482	63.798452
1751.675305	46.689530	63.803457
1750.978274	36.714237	63.808462
1750.577923	42.803419	63.813466
1749.501604	46.190356	63.818471
1748.964861	44.064671	63.823476
1748.304631	48.016308	63.828481
1747.465195	49.832384	63.833486
1747.123554	47.442010	63.838490
1745.664950	53.242157	63.843495
1745.694254	46.894396	63.848500
1744.352371	44.067301	63.853505
1744.416732	45.294540	63.858510
1744.491282	38.483534	63.863514
1743.296673	47.043388	63.868519
1742.883326	38.436996	63.873524
1741.364371	43.499078	63.878529
1740.704827	46.774837	63.883534
1739.891444	33.873660	63.888538
1739.075620	42.465406	63.893543
1738.517586	40.906237	63.898548
1738.169680	43.100822	63.903553
1737.837599	40.160153	63.908558
1737.719220	39.600974	63.913562
1736.965894	42.991064	63.918567
1735.834515	38.261323	63.923572
1735.447873	43.156894	63.928577
1734.457244	41.089928	63.933582
1733.490867	35.401206	63.938586
1732.487378	53.360987	63.943591
1732.089322	32.096466	63.948596
1731.831954	48.262461	63.953601
1731.534996	46.625069	63.958606
1730.989889	36.873248	63.963610
1729.637393	43.818479	63.968615
1729.220439	42.179120	63.973620
1728.519784	37.015696	63.978625
1727.766910	32.742223	63.983630
1726.920066	41.111524	63.988634
1725.912402	33.268382	63.993639
1725.487203	39.446284	63.998644
1725.709170	45.658709	64.003649
1724.933336	39.319251	64.008654
1724.014021	41.923833	64.013658
1723.103925	50.215150	64.018663
1722.496948	38.953060	64.023668
1722.215725	45.273689	64.028673
1721.458470	45.697344	64.033678
1720.165641	34.950491	64.038682
1719.573804	39.292645	64.043687
1719.008966	45.057094	64.048692
1718.629447	43.011874	64.053697
1718.033177	47.366631	64.058702
1717.336466	37.907584	64.063706
1716.386030	45.637405	64.068711
1715.839305	42.528606	64.073716
1714.925395	42.430012	64.078721
1714.832598	44.125044	64.083726
1714.466682	31.912672	64.088730
1713.333663	46.248978	64.093735
1712.901946	36.552361	64.098740
1711.370927	46.113558	64.103745
1710.632793	46.335003	64.108750
1710.712398	39.122493	64.113754
1709.674986	51.501607	64.118759
1709.323860	49.520211	64.123764
1709.155399	43.449836	64.128769
1708.440053	45.015351	64.133774
1707.448976	39.682556	64.138778
1706.517471	48.921706	64.143783
1706.428616	39.111950	64.148788
1705.318931	39.553677	64.153793
1704.181272	41.155141	64.158798
1703.418668	41.505901	64.163802
1702.946247	41.328212	64.168807
1703.129701	42.709537	64.173812
1702.250195	46.122013	64.178817
1701.515872	41.957074	64.183822
1700.559896	39.039880	64.188826
1699.598210	47.814084	64.193831
1699.234987	37.025006	64.198836
1698.852986	35.851755	64.203841
1698.376039	40.244906	64.208846
1697.622324	39.735630	64.213850
1696.541020	44.872827	64.218855
1696.387211	43.907624	64.223860
1695.757549	40.794469	64.228865
1695.023859	47.837100	64.233870
1693.985246	40.986059	64.238874
1693.227965	53.344871	64.243879
1692.846420	46.283108	64.248884
1692.278742	42.609501	64.253889
1691.074716	42.334775	64.258894
1690.293474	34.627364	64.263898
1689.556386	48.467257	64.268903
1689.298114	45.190687	64.273908
1688.963894	39.965355	64.278913
1688.380927	40.516684	64.283918
1688.133546	39.819324	64.288922
1687.068901	39.850340	64.293927
1686.598701	34.348292	64.298932
1686.009998	44.490714	64.303937
1684.415541	48.481829	64.308942
1684.069663	33.931659	64.313946
1683.218429	42.461182	64.318951
1682.951713	37.965979	64.323956
1682.484987	38.373871	64.328961
1681.264982	40.257051	64.333966
1680.576278	31.650820	64.338970
1679.807458	43.344128	64.343975
1679.627097	35.743494	64.348980
1679.296222	39.907185	64.353985
1678.489652	39.000790	64.358990
1677.747293	34.624479	64.363994
1676.686515	36.808030	64.368999
1676.382887	36.316077	64.374004
1675.711819	39.252774	64.379009
1675.118351	34.476002	64.384014
1674.260523	31.312294	64.389018
1673.442781	37.868407	64.394023
1673.002797	41.810780	64.399028
1672.341538	31.317042	64.404033
1671.745359	42.143607	64.409038
1670.906266	32.039100	64.414042
1670.011525	36.657290	64.419047
1669.864495	33.698384	64.424052
1669.474091	33.869015	64.429057
1668.176124	30.854438	64.434062
1667.496448	36.652352	64.439066
1666.860268	41.824694	64.444071
1666.181410	37.094901	64.449076
1666.011472	43.468325	64.454081
1665.335137	46.964849	64.459086
1664.409659	37.810609	64.464090
1663.875890	40.848545	64.469095
1663.123997	35.244710	64.474100
1662.808963	36.871591	64.479105
1661.089969	39.172517	64.484110
1660.570787	32.530616	64.489114
1660.203157	42.076679	64.494119
1660.236113	24.802469	64.499124
1659.473162	35.572309	64.504129
1658.465564	35.581331	64.509134
1658.126210	34.622619	64.514138
1657.339410	43.913584	64.519143
1656.807947	36.778410	64.524148
1655.337878	34.305238	64.529153
1654.630759	36.651290	64.534158
1654.451870	31.183474	64.539162
1653.396349	41.526167	64.544167
1653.452077	33.637647	64.549172
1653.170651	33.269786	64.554177
1651.697365	40.281091	64.559182
1651.514329	33.057482	64.564186
1650.500203	39.911270	64.569191
1649.656010	35.660939	64.574196
1648.439162	37.694368	64.579201
1648.051822	39.716106	64.584206
1647.485693	36.610244	64.589210
1647.165417	45.694672	64.594215
1647.163146	43.682793	64.599220
1646.597575	34.361976	64.604225
1645.264415	46.762096	64.609230
1644.894752	45.570949	64.614234
1643.812938	40.024364	64.619239
1643.355277	40.990025	64.624244
1642.480029	37.205646	64.629249
1641.607648	42.258549	64.634254
1641.262802	34.675409	64.639258
1640.682101	45.153159	64.644263
1640.554742	42.128915	64.649268
1639.375559	40.245020	64.654273
1638.469354	45.770665	64.659278
1637.866865	36.983116	64.664282
1637.746783	48.233453	64.669287
1637.027112	42.381750	64.674292
1635.829749	37.889896	64.679297
1635.058856	47.184063	64.684302
1635.061133	36.707039	64.689306
1633.854026	44.654073	64.694311
1632.863561	33.017521	64.699316
1632.595199	33.714352	64.704321
1631.719504	35.614802	64.709326
1631.668031	28.909053	64.714330
1630.900090	39.252269	64.719335
1630.045146	36.030841	64.724340
1629.279388	35.520873	64.729345
1628.110683	45.063108	64.734350
1628.027654	36.550599	64.739354
1627.573437	46.379100	64.744359
1626.888551	35.322991	64.749364
1626.057331	34.652918	64.754369
1624.856492	46.526340	64.759374
1624.871189	41.111443	64.764378
1624.187018	44.261169	64.769383
1623.808027	42.640192	64.774388
1623.008071	33.978805	64.779393
1622.057087	41.487684	64.784398
1621.615323	33.197218	64.789402
1621.090677	38.316530	64.794407
1620.370753	38.967484	64.799412
1619.552663	30.772209	64.804417
1618.655575	40.369797	64.809422
1618.334952	32.758834	64.814426
1617.268209	35.967318	64.819431
1616.545934	40.930591	64.824436
1616.313159	34.695190	64.829441
1615.741097	46.464168	64.834446
1615.077896	40.236901	64.839450
1613.949085	47.492017	64.844455
1613.049089	41.858275	64.849460
1612.433265	39.421288	64.854465
1611.904537	52.097419	64.859470
1611.945506	47.807713	64.864474
1610.947950	48.306452	64.869479
1610.768816	39.476062	64.874484
1609.841233	45.563502	64.879489
1608.830896	53.525816	64.884494
1608.457639	38.698909	64.889498
1607.072540	47.802542	64.894503
1606.450207	51.156022	64.899508
1606.287428	46.360024	64.904513
1605.296504	53.584442	64.909518
1605.017271	44.327516	64.914522
1604.815815	47.023205	64.919527
1603.813720	46.357115	64.924532
1603.044914	42.851357	64.929537
1602.297376	53.084911	64.934542
1602.144523	37.255988	64.939546
1601.206549	43.636510	64.944551
1599.805840	53.182142	64.949556
1599.502486	44.425112	64.954561
1598.681570	47.864679	64.959566
1598.482460	41.218929	64.964570
1597.766795	47.589827	64.969575
1596.935293	47.705694	64.974580
1596.874445	44.960189	64.979585
1596.073458	44.985574	64.984590
1595.170855	41.779018	64.989594
1594.343054	50.889910	64.994599
1593.646133	42.298520	64.999604
1593.034000	43.435878	65.004609
1592.393393	53.439958	65.009614
1591.270127	40.098848	65.014618
1590.325326	43.474356	65.019623
1589.950895	44.100135	65.024628
1589.185694	39.703670	65.029633
1588.686344	42.610200	65.034638
1588.722188	47.572809	65.039642
1588.434218	46.643201	65.044647
1587.768333	46.712569	65.049652
1586.873247	41.893088	65.054657
1585.991030	43.539674	65.059662
1585.435461	44.720639	65.064666
1584.067768	46.759373	65.069671
1583.588475	36.669493	65.074676
1583.462753	44.012277	65.079681
1582.562089	42.283616	65.084686
1582.609753	34.707520	65.089690
1581.455943	44.063272	65.094695
1580.406650	35.858626	65.099700
1579.559152	36.576811	65.104705
1578.457068	45.212821	65.109710
1578.487190	35.915198	65.114714
1577.883355	42.634441	65.119719
1577.297655	34.523740	65.124724
1577.122487	29.935124	65.129729
1576.237087	40.372651	65.134734
1574.609703	34.964058	65.139738
1574.146696	49.500302	65.144743
1573.492322	49.717300	65.149748
1573.094033	47.559653	65.154753
1572.703337	48.886475	65.159758
1572.530436	44.889546	65.164762
1571.478302	44.580959	65.169767
1570.774506	37.367535	65.174772
1570.215721	42.924515	65.179777
1569.124350	45.431072	65.184782
1568.275913	43.407699	65.189786
1567.344723	56.614530	65.194791
1567.046433	45.560159	65.199796
1566.539614	48.664541	65.204801
1566.214532	50.411957	65.209806
1565.869213	46.145733	65.214810
1564.741869	49.268289	65.219815
1563.819011	55.654522	65.224820
1563.488080	41.913752	65.229825
1562.789052	50.992345	65.234830
1561.636959	44.218784	65.239834
1560.947989	56.003039	65.244839
1560.234371	50.906200	65.249844
1560.098727	45.514667	65.254849
1559.149450	42.683985	65.259854
1559.347217	50.377969	65.264858
1558.548112	56.362908	65.269863
1557.334832	46.826519	65.274868
1556.959643	47.367565	65.279873
1556.106136	49.475405	65.284878
1555.548536	37.934128	65.289882
1554.731542	51.559156	65.294887
1554.100559	46.958155	65.299892
1553.938336	46.459771	65.304897
1552.619082	51.921914	65.309902
1552.206054	49.726135	65.314906
1551.502035	47.062681	65.319911
1551.037518	45.210438	65.324916
1550.111580	49.034679	65.329921
1549.022270	45.346950	65.334926
1548.218208	45.338528	65.339930
1547.904380	54.218178	65.344935
1547.402814	47.302499	65.349940
1547.074596	48.581920	65.354945
1546.638623	43.264288	65.359950
1545.489331	41.245043	65.364954
1544.755063	55.451152	65.369959
1544.385189	54.603061	65.374964
1543.717528	50.312667	65.379969
1542.524270	51.262131	65.384974
1542.001694	52.067997	65.389978
1541.397293	47.344032	65.394983
1540.727394	46.218883	65.399988
1540.590163	48.746878	65.404993
1539.519496	58.114464	65.409998
1538.650660	52.308437	65.415002
1538.165474	47.108169	65.420007
1537.760150	59.137553	65.425012
1537.458260	50.742631	65.430017
1536.336846	49.586604	65.435022
1535.463562	48.159962	65.440026
1535.073815	51.903096	65.445031
1534.394454	43.441340	65.450036
1533.059077	34.932002	65.455041
1532.416656	48.439522	65.460046
1531.523702	35.184937	65.465050
1531.424666	44.714631	65.470055
1531.222021	44.990501	65.475060
1531.245522	34.670509	65.480065
1529.894715	46.486321	65.485070
1529.412005	36.053237	65.490074
1528.439226	38.498058	65.495079
1527.687162	33.082958	65.500084
1526.576568	33.534351	65.505089
1525.827664	42.343989	65.510094
1525.440087	40.084257	65.515098
1524.899027	47.099852	65.520103
1524.742717	47.193720	65.525108
1524.365525	29.828286	65.530113
1523.029132	51.240412	65.535118
1522.296630	45.741042	65.540122
1521.697649	50.510732	65.545127
1521.325994	45.484844	65.550132
1520.617975	44.091892	65.555137
1519.341447	53.590233	65.560142
1518.975080	41.609277	65.565146
1518.473576	41.968268	65.570151
1518.255902	46.986104	65.575156
1517.252913	41.156863	65.580161
1516.224699	49.567882	65.585166
1515.820229	40.950142	65.590170
1515.604106	47.256864	65.595175
1514.461046	42.753381	65.600180
1513.615700	49.128719	65.605185
1512.864880	52.055796	65.610190
1512.421767	40.455855	65.615194
1511.953370	47.316521	65.620199
1511.312508	44.236099	65.625204
1510.282017	44.031183	65.630209
1509.401938	46.122263	65.635214
1508.785969	46.709259	65.640218
1508.590052	48.279841	65.645223
1507.772342	50.256436	65.650228
1507.745238	43.837823	65.655233
1506.183472	51.237712	65.660238
1505.737031	42.200069	65.665242
1505.461283	51.277664	65.670247
1504.783534	52.956370	65.675252
1504.485952	49.041571	65.680257
1503.811577	38.303415	65.685262
1502.430748	39.234071	65.690266
1501.115960	44.079696	65.695271
1500.432108	46.186532	65.700276
1501.074893	40.590726	65.705281
1500.393913	49.329141	65.710286
1499.447227	43.766177	65.715290
1498.747444	40.562032	65.720295
1497.572827	43.650455	65.725300
1497.277007	38.658170	65.730305
1496.663045	44.969433	65.735310
1496.028353	39.283207	65.740314
1495.412478	40.443320	65.745319
1494.415887	42.461189	65.750324
1493.861676	36.823161	65.755329
1492.844862	49.811365	65.760334
1492.789722	40.488869	65.765338
1492.591622	33.852039	65.770343
1491.453125	46.475428	65.775348
1490.928035	34.441521	65.780353
1490.040778	50.938707	65.785358
1489.566077	42.826784	65.790362
1488.375159	43.345221	65.795367
1487.588556	46.447759	65.800372
1487.137003	34.968872	65.805377
1486.963317	51.050256	65.810382
1486.553840	34.139149	65.815386
1485.422818	32.947676	65.820391
1484.413012	41.707238	65.825396
1484.212665	43.132532	65.830401
1483.552802	46.164433	65.835406
1483.012928	27.644673	65.840410
1481.989824	40.401063	65.845415
1480.843380	42.149333	65.850420
1480.495706	32.931777	65.855425
1479.701406	43.648969	65.860430
1479.597727	36.421269	65.865434
1479.204663	41.563064	65.870439
1478.255349	40.126949	65.875444
1477.661587	36.478366	65.880449
1476.756864	37.513847	65.885454
1476.411683	35.474222	65.890458
1475.130634	39.526612	65.895463
1474.098450	40.607988	65.900468
1473.881083	34.145766	65.905473
1473.270303	39.830855	65.910478
1472.923652	39.039187	65.915482
1472.740091	37.962643	65.920487
1471.986204	40.066075	65.925492
1471.435533	40.876361	65.930497
1470.307928	40.109023	65.935502
1469.627508	36.815127	65.940506
1468.418472	36.678673	65.945511
1467.356974	36.923922	65.950516
1467.024563	33.166269	65.955521
1466.469898	43.784028	65.960526
1466.142853	30.765749	65.965530
1466.228274	38.291059	65.970535
1465.717958	38.513018	65.975540
1464.847261	36.257434	65.980545
1463.792785	45.808557	65.985550
1463.497584	41.092472	65.990554
1461.879990	42.859023	65.995559
1461.013530	44.951726	66.000564
1460.935107	31.215530	66.005569
1459.998974	39.595395	66.010574
1459.634353	32.094218	66.015578
1459.313560	39.135265	66.020583
1458.061190	43.495763	66.025588
1457.618029	37.318099	66.030593
1456.927001	47.009112	66.035598
1456.641530	34.612503	66.040602
1455.692903	45.403084	66.045607
1454.620905	42.047928	66.050612
1454.457347	36.226600	66.055617
1453.827501	43.837629	66.060622
1453.834430	36.532580	66.065626
1452.744551	38.093946	66.070631
1451.947131	45.229996	66.075636
1451.344026	44.361047	66.080641
1449.824850	45.480785	66.085646
1448.935811	38.330671	66.090650
1448.118110	36.334428	66.095655
1448.293546	41.547857	66.100660
1448.429638	36.049434	66.105665
1447.369290	42.932081	66.110670
1446.777150	43.950379	66.115674
1445.936743	41.151611	66.120679
1444.827236	47.867419	66.125684
1444.430580	43.759201	66.130689
1443.953197	43.624225	66.135694
1443.370255	41.279524	66.140698
1442.482205	38.946786	66.145703
1441.740967	39.682329	66.150708
1441.332044	39.153943	66.155713
1440.154133	41.024444	66.160718
1439.205153	37.970722	66.165722
1438.586348	40.547198	66.170727
1438.335681	48.495546	66.175732
1438.316868	33.720511	66.180737
1437.563083	43.582520	66.185742
1437.020262	42.191303	66.190746
1435.966267	43.125638	66.195751
1434.988726	42.657870	66.200756
1434.591357	40.126283	66.205761
1433.850310	43.769293	66.210766
1432.987890	40.858643	66.215770
1432.383947	46.824001	66.220775
1431.672469	49.072541	66.225780
1431.503856	45.750647	66.230785
1431.052952	48.601530	66.235790
1430.192430	34.656589	66.240794
1429.112412	41.636548	66.245799
1428.064526	35.940933	66.250804
1427.721123	30.195785	66.255809
1427.678720	41.688578	66.260814
1426.736443	39.389992	66.265818
1425.686887	39.802540	66.270823
1425.027351	40.854086	66.275828
1424.863952	39.965532	66.280833
1424.218646	42.585228	66.285838
1423.387736	40.331130	66.290842
1422.572769	35.749017	66.295847
1421.661571	45.420876	66.300852
1421.429521	44.429999	66.305857
1420.970595	36.652481	66.310862
1419.923266	35.345650	66.315866
1419.375872	38.293570	66.320871
1418.826985	46.174152	66.325876
1418.319954	35.279487	66.330881
1416.951355	43.092359	66.335886
1416.594669	38.957568	66.340890
1416.118162	41.717706	66.345895
1415.003809	39.034912	66.350900
1414.961493	30.976097	66.355905
1414.326352	41.445004	66.360910
1413.057654	32.821275	66.365914
1412.104636	38.746518	66.370919
1411.982585	41.696236	66.375924
1411.456989	40.090505	66.380929
1411.068162	44.870015	66.385934
1410.439611	33.740376	66.390938
1409.721471	40.697076	66.395943
1408.676321	42.019094	66.400948
1408.317850	36.939653	66.405953
1407.587314	43.494679	66.410958
1406.553300	38.676917	66.415962
1406.264417	39.593576	66.420967
1405.249802	44.489282	66.425972
1405.119889	36.180998	66.430977
1403.811710	45.367810	66.435982
1403.182633	35.290187	66.440986
1402.557261	35.180546	66.445991
1401.984679	36.554695	66.450996
1401.751725	29.938843	66.456001
1401.387351	40.160491	66.461006
1400.571247	43.797011	66.466010
1399.350094	34.496494	66.471015
1399.125929	43.465385	66.476020
1398.544640	31.335733	66.481025
1397.109135	41.251673	66.486030
1396.623443	33.925564	66.491034
1396.228478	29.441294	66.496039
1395.830786	40.935691	66.501044
1395.145267	32.651071	66.506049
1394.070815	36.397336	66.511054
1393.552448	41.472954	66.516058
1393.334307	38.962795	66.521063
1392.329984	43.072829	66.526068
1391.300086	26.967791	66.531073
1390.354912	37.100179	66.536078
1390.136740	42.170199	66.541082
1389.658520	36.940346	66.546087
1388.990619	42.846392	66.551092
1389.166879	41.315515	66.556097
1387.890280	50.874672	66.561102
1386.905109	42.868699	66.566106
1386.641281	47.598790	66.571111
1385.648247	45.160485	66.576116
1384.484887	40.185667	66.581121
1383.684243	48.001982	66.586126
1383.362147	36.966330	66.591130
1383.187464	39.686251	66.596135
1382.639600	45.765558	66.601140
1382.456524	43.255318	66.606145
1381.291316	58.463573	66.611150
1380.416206	45.040980	66.616154
1379.540268	44.862923	66.621159
1378.610388	40.468243	66.626164
1377.918381	41.144055	66.631169
1377.117859	48.050918	66.636174
1376.597404	38.930054	66.641178
1376.437604	37.379338	66.646183
1376.037042	41.442865	66.651188
1375.760704	34.017373	66.656193
1374.773544	41.239984	66.661198
1373.741841	37.494680	66.666202
1373.494082	43.974173	66.671207
1372.626218	44.203269	66.676212
1371.729297	41.011182	66.681217
1371.045198	44.895492	66.686222
1370.574689	38.801861	66.691226
1369.668183	40.228832	66.696231
1369.026971	38.895912	66.701236
1368.028771	34.091372	66.706241
1367.130301	51.236236	66.711246
1366.454690	38.563810	66.716250
1366.239846	42.507523	66.721255
1365.785061	38.341769	66.726260
1365.705718	29.135932	66.731265
1365.364356	34.883059	66.736270
1364.592611	30.925899	66.741274
1363.535163	39.320618	66.746279
1362.447469	46.644517	66.751284
1361.757617	35.824578	66.756289
1360.882188	39.026805	66.761294
1360.212402	34.348803	66.766298
1359.953353	40.156049	66.771303
1359.417412	43.235824	66.776308
1358.807565	31.555917	66.781313
1357.931516	43.990317	66.786318
1357.247047	35.853938	66.791322
1356.862108	41.355117	66.796327
1355.988344	41.807452	66.801332
1354.965354	42.653604	66.806337
1353.938776	39.059394	66.811342
1353.622733	37.545293	66.816346
1353.241362	36.340782	66.821351
1352.652707	51.230478	66.826356
1352.686271	39.277014	66.831361
1351.910533	39.837695	66.836366
1350.577563	31.211965	66.841370
1350.272978	34.818950	66.846375
1348.800668	37.914942	66.851380
1348.228098	35.092055	66.856385
1347.579667	45.638238	66.861390
1346.929804	32.575380	66.866394
1346.866632	38.159629	66.871399
1346.073815	43.755103	66.876404
1345.927180	33.777268	66.881409
1345.195976	45.400596	66.886414
1343.929207	40.597431	66.891418
1343.643027	38.586005	66.896423
1342.745624	43.480996	66.901428
1341.814231	32.503869	66.906433
1340.804466	38.889998	66.911438
1339.985961	39.551550	66.916442
1339.977320	36.348326	66.921447
1339.596548	48.218363	66.926452
1339.438344	32.901180	66.931457
1338.370591	44.338973	66.936462
1337.030158	44.407009	66.941466
1336.795521	36.131264	66.946471
1336.368302	43.970494	66.951476
1335.886311	37.869361	66.956481
1334.756667	51.793032	66.961486
1333.625483	42.462132	66.966490
1333.682018	37.092589	66.971495
1333.199366	43.462694	66.976500
1332.305542	39.258422	66.981505
1331.008073	46.431139	66.986510
1330.799175	41.570038	66.991514
1330.523154	38.258251	66.996519
1329.848456	42.181216	67.001524
1328.807790	37.110020	67.006529
1327.826443	45.756181	67.011534
1327.425006	48.169543	67.016538
1327.142208	40.931073	67.021543
1326.250194	49.118675	67.026548
1325.227966	45.088351	67.031553
1324.429836	46.471121	67.036558
1323.844242	45.101055	67.041562
1323.846211	37.523721	67.046567
1323.366654	44.304987	67.051572
1322.813265	32.611871	67.056577
1321.894081	44.197118	67.061582
1321.114185	44.257618	67.066586
1320.310769	42.178429	67.071591
1319.170352	41.869219	67.076596
1318.769165	43.043518	67.081601
1317.889853	38.017330	67.086606
1317.809200	35.067213	67.091610
1317.302009	41.707163	67.096615
1316.560245	47.839008	67.101620
1315.345082	38.888397	67.106625
1314.920471	35.286669	67.111630
1314.574897	41.768695	67.116634
1313.940169	43.712413	67.121639
1313.082115	43.302764	67.126644
1312.331523	28.689341	67.131649
1311.553035	42.449476	67.136654
1311.206677	29.796888	67.141658
1310.533428	40.164561	67.146663
1309.183204	49.628575	67.151668
1308.529116	36.319749	67.156673
1308.278667	49.496491	67.161678
1308.039994	39.587306	67.166682
1307.688652	38.126223	67.171687
1306.273082	43.426093	67.176692
1305.823061	43.846946	67.181697
1304.932836	41.433296	67.186702
1304.469986	39.313966	67.191706
1303.863286	48.257951	67.196711
1302.290692	46.506616	67.201716
1301.987608	42.576203	67.206721
1301.792714	48.454175	67.211726
1301.096108	46.201975	67.216730
1301.229721	40.928968	67.221735
1300.075880	45.933784	67.226740
1299.335898	43.521649	67.231745
1298.513017	41.735520	67.236750
1297.841035	33.330978	67.241754
1296.904900	46.971664	67.246759
1296.339030	47.736414	67.251764
1295.724226	45.160752	67.256769
1295.563118	44.347991	67.261774
1294.906502	48.478251	67.266778
1293.707444	46.222072	67.271783
1292.823214	45.463240	67.276788
1292.627130	45.655894	67.281793
1291.804926	49.122165	67.286798
1291.656719	46.859370	67.291802
1290.787979	38.839415	67.296807
1289.802523	43.870270	67.301812
1289.213367	43.245652	67.306817
1288.505101	39.392896	67.311822
1287.368948	38.993757	67.316826
1287.013421	35.908733	67.321831
1286.516183	45.263825	67.326836
1286.173429	41.261657	67.331841
1285.499549	47.458853	67.336846
1284.882076	52.411321	67.341850
1283.981952	43.250477	67.346855
1282.863586	48.028969	67.351860
1282.793748	44.587155	67.356865
1281.974019	54.291132	67.361870
1281.262943	47.517940	67.366874
1280.040140	36.444672	67.371879
1279.349424	37.090671	67.376884
1279.270496	38.225986	67.381889
1278.730681	36.944796	67.386894
1278.318750	41.222630	67.391898
1278.239259	41.982665	67.396903
1276.841403	36.253851	67.401908
1275.946082	31.491719	67.406913
1275.586425	37.118038	67.411918
1274.505177	32.520362	67.416922
1273.989827	34.442856	67.421927
1273.479105	51.375293	67.426932
1272.906949	44.089265	67.431937
1272.092085	50.199683	67.436942
1271.132770	40.497556	67.441946
1270.845213	38.186386	67.446951
1269.949600	36.854403	67.451956
1269.716349	32.763233	67.456961
1269.078708	43.670708	67.461966
1267.450032	52.053507	67.466970
1267.088833	36.025071	67.471975
1266.651682	48.126193	67.476980
1266.392984	38.273335	67.481985
1265.873053	44.933232	67.486990
1264.755138	39.719363	67.491994
1263.813264	43.495847	67.496999
1263.279189	50.040146	67.502004
1262.903422	37.667715	67.507009
1262.585779	39.179408	67.512014
1261.273628	41.438438	67.517018
1261.008178	33.219689	67.522023
1260.172719	44.038668	67.527028
1260.129958	37.874983	67.532033
1258.800511	47.412811	67.537038
1257.687747	47.647539	67.542042
1257.402083	40.261156	67.547047
1256.894077	47.702922	67.552052
1256.544246	45.272945	67.557057
1254.764383	40.006624	67.562062
1254.093515	41.855487	67.567066
1254.577027	37.587135	67.572071
1253.736626	44.687140	67.577076
1253.263886	41.336410	67.582081
1252.492831	49.273979	67.587086
1251.402793	44.913852	67.592090
1251.311722	40.715053	67.597095
1250.550162	42.020918	67.602100
1250.184343	44.860007	67.607105
1248.962719	46.472388	67.612110
1248.193674	45.685556	67.617114
1247.895854	40.328132	67.622119
1246.899897	44.259134	67.627124
1245.946889	44.700976	67.632129
1244.945803	43.353899	67.637134
1244.584862	50.613785	67.642138
1244.618241	37.526342	67.647143
1244.092953	41.688591	67.652148
1243.266106	38.951486	67.657153
1242.528291	47.154140	67.662158
1241.552705	42.805999	67.667162
1241.301850	48.889725	67.672167
1240.248628	51.775452	67.677172
1239.333117	44.489797	67.682177
1238.926491	37.154125	67.687182
1238.459406	33.175618	67.692186
1238.258166	40.342635	67.697191
1236.902688	40.226572	67.702196
1235.958016	38.682348	67.707201
1235.512017	42.667215	67.712206
1234.748787	42.671588	67.717210
1234.542787	39.354926	67.722215
1233.758384	46.365615	67.727220
1233.299336	42.992806	67.732225
1232.149367	41.004938	67.737230
1231.254068	40.817196	67.742234
1230.912798	38.393652	67.747239
1230.089392	46.742796	67.752244
1229.986688	38.976952	67.757249
1229.910042	49.751677	67.762254
1228.387564	43.475424	67.767258
1228.007286	33.553791	67.772263
1227.693773	46.983677	67.777268
1226.004350	40.872580	67.782273
1225.350529	38.665961	67.787278
1224.591864	47.864506	67.792282
1224.424060	42.053398	67.797287
1223.720951	42.480090	67.802292
1223.777312	33.859293	67.807297
1222.763984	41.124689	67.812302
1221.757387	43.806656	67.817306
1221.369995	29.645001	67.822311
1220.887353	40.497913	67.827316
1220.062067	36.804934	67.832321
1219.126842	37.891074	67.837326
1218.482005	40.414399	67.842330
1217.779122	38.035005	67.847335
1217.248146	50.166005	67.852340
1216.284427	44.614316	67.857345
1215.471760	37.959978	67.862350
1214.867355	44.718413	67.867354
1214.601026	37.531611	67.872359
1213.626142	47.507666	67.877364
1213.500281	36.983554	67.882369
1213.158462	47.699866	67.887374
1212.048323	45.388224	67.892378
1211.350747	40.609616	67.897383
1210.516667	43.129818	67.902388
1210.230578	39.242293	67.907393
1209.217931	40.188934	67.912398
1208.493208	41.805456	67.917402
1208.367347	40.802726	67.922407
1207.145191	49.049625	67.927412
1206.519051	38.022641	67.932417
1205.869724	38.948524	67.937422
1204.898239	38.805014	67.942426
1204.864793	34.131377	67.947431
1204.157979	40.489733	67.952436
1203.736003	40.687909	67.957441
1202.921656	43.396961	67.962446
1201.935076	38.209964	67.967450
1201.762820	35.425923	67.972455
1200.866819	49.429989	67.977460
1199.642534	43.520304	67.982465
1198.758812	41.071221	67.987470
1198.343207	55.017909	67.992474
1198.478039	46.901542	67.997479
1198.155559	50.811978	68.002484
1197.424267	38.341359	68.007489
1196.426889	47.906419	68.012494
1195.402858	52.308794	68.017498
1194.559263	42.548588	68.022503
1193.455866	44.102451	68.027508
1193.532479	37.194026	68.032513
1193.154990	49.926347	68.037518
1192.760824	47.655539	68.042522
1191.943638	41.881015	68.047527
1190.792623	45.825154	68.052532
1190.478457	38.530498	68.057537
1189.470254	49.518791	68.062542
1188.411490	43.194342	68.067546
1187.989046	40.166572	68.072551
1187.069598	50.251949	68.077556
1186.546568	38.263546	68.082561
1186.002312	42.676534	68.087566
1185.797917	40.519677	68.092570
1184.642840	39.873945	68.097575
1184.066652	45.311168	68.102580
1183.408106	34.891290	68.107585
1182.907128	45.095665	68.112590
1182.587230	42.516105	68.117594
1181.916609	48.384345	68.122599
1180.844558	49.804167	68.127604
1180.277002	45.647482	68.132609
1179.957009	43.581466	68.137614
1178.581361	40.521120	68.142618
1177.972675	49.275195	68.147623
1177.070303	55.248641	68.152628
1176.683288	45.340793	68.157633
1176.262921	40.818663	68.162638
1175.843838	43.867391	68.167642
1175.534187	42.267345	68.172647
1174.041256	49.958666	68.177652
1173.622292	43.724009	68.182657
1173.247725	53.824249	68.187662
1172.612339	50.978589	68.192666
1171.637124	47.847315	68.197671
1170.571551	46.880356	68.202676
1170.093688	38.842847	68.207681
1169.668447	46.606743	68.212686
1169.081678	48.397009	68.217690
1168.799212	44.643465	68.222695
1167.604304	43.203675	68.227700
1166.764124	39.389711	68.232705
1166.256063	46.770701	68.237710
1165.904007	48.137509	68.242714
1164.921856	42.429919	68.247719
1164.451957	38.511505	68.252724
1163.512277	39.285012	68.257729
1163.092282	43.597387	68.262734
1162.318657	43.408166	68.267738
1162.266470	27.601974	68.272743
1160.892970	37.392475	68.277748
1160.103367	35.227666	68.282753
1159.850050	47.545584	68.287758
1158.917045	38.080159	68.292762
1159.052627	41.037471	68.297767
1157.373525	37.548718	68.302772
1157.141841	35.353906	68.307777
1156.706184	36.496619	68.312782
1155.739204	42.660326	68.317786
1155.536999	44.291990	68.322791
1154.155349	47.743940	68.327796
1153.691682	40.753952	68.332801
1153.191630	40.448816	68.337806
1152.627823	38.119432	68.342810
1152.026223	42.393037	68.347815
1150.850999	44.265114	68.352820
1150.407760	36.079979	68.357825
1149.939156	32.957887	68.362830
1149.240364	40.662043	68.367834
1148.832069	35.921545	68.372839
1147.380348	35.190043	68.377844
1147.053533	28.516086	68.382849
1146.849462	41.008320	68.387854
1146.172773	39.261922	68.392858
1145.030598	34.764312	68.397863
1144.479313	38.850890	68.402868
1143.977537	39.584156	68.407873
1143.540644	36.561630	68.412878
1143.094837	43.659209	68.417882
1142.412617	41.084852	68.422887
1141.059291	39.456283	68.427892
1140.789944	37.614088	68.432897
1140.099005	39.800332	68.437902
1138.655674	36.819875	68.442906
1138.398155	34.190957	68.447911
1137.829378	32.892244	68.452916
1137.451831	32.101157	68.457921
1136.830686	36.684014	68.462926
1135.988590	32.482773	68.467930
1135.473072	31.787543	68.472935
1134.537103	39.939659	68.477940
1134.139705	37.519419	68.482945
1133.453009	35.693030	68.487950
1132.439832	38.170490	68.492954
1131.976452	32.281327	68.497959
1131.341529	38.505411	68.502964
1131.135945	33.973747	68.507969
1130.084031	25.969811	68.512974
1128.940277	32.441273	68.517978
1128.784273	35.685733	68.522983
1128.432820	40.522005	68.527988
1127.804693	35.541665	68.532993
1126.589664	33.725219	68.537998
1125.448677	41.681137	68.543002
1125.256884	32.583391	68.548007
1124.316047	50.811111	68.553012
1124.102553	34.217053	68.558017
1123.460524	36.862663	68.563022
1123.362677	39.323126	68.568026
1122.551804	42.231320	68.573031
1121.658304	45.535750	68.578036
1120.927656	41.829349	68.583041
1120.093025	38.235880	68.588046
1119.310123	37.913261	68.593050
1118.677057	33.977401	68.598055
1117.910235	43.229449	68.603060
1117.643285	38.977490	68.608065
1117.385849	41.585273	68.613070
1115.680734	45.012886	68.618074
1115.377413	34.703509	68.623079
1115.158436	39.933128	68.628084
1114.480733	35.873471	68.633089
1113.450666	34.605987	68.638094
1112.364861	42.367336	68.643098
1112.129720	38.607275	68.648103
1111.403142	36.932184	68.653108
1111.322876	40.083945	68.658113
1110.477733	41.245069	68.663118
1108.987102	46.461921	68.668122
1108.877147	46.527339	68.673127
1108.259961	43.326486	68.678132
1107.889600	44.997996	68.683137
1106.639259	42.852881	68.688142
1105.797797	42.619629	68.693146
1105.401147	38.437246	68.698151
1104.701780	37.559957	68.703156
1104.666835	41.312611	68.708161
1104.624082	41.342840	68.713166
1102.868218	34.287168	68.718170
1102.414197	35.406188	68.723175
1101.694313	38.878644	68.728180
1100.936911	45.491186	68.733185
1099.771197	41.312997	68.738190
1098.837083	45.804194	68.743194
1098.456790	33.945709	68.748199
1098.108127	41.370453	68.753204
1097.425372	34.424702	68.758209
1097.768802	42.912327	68.763214
1096.996194	38.623014	68.768218
1096.442829	39.594054	68.773223
1095.102369	38.775229	68.778228
1094.666148	35.760093	68.783233
1093.751174	30.993080	68.788238
1092.701169	43.716211	68.793242
1092.757623	30.465772	68.798247
1091.973706	38.105169	68.803252
1090.944166	36.032377	68.808257
1090.314255	42.535066	68.813262
1089.574577	40.937613	68.818266
1089.652784	44.526425	68.823271
1088.238518	42.718448	68.828276
1086.959880	47.797957	68.833281
1086.473033	42.832112	68.838286
1085.995128	47.767404	68.843290
1085.949763	36.209972	68.848295
1085.531220	46.167742	68.853300
1085.390925	44.966182	68.858305
1084.033738	45.199383	68.863310
1083.195548	41.457723	68.868314
1082.535396	38.705132	68.873319
1082.150637	43.938667	68.878324
1080.883507	45.545458	68.883329
1080.013635	37.534042	68.888334
1079.470743	42.577956	68.893338
1079.407420	39.901579	68.898343
1078.512518	30.141120	68.903348
1078.072438	41.615130	68.908353
1077.205448	39.328989	68.913358
1076.640649	46.838111	68.918362
1076.497370	38.524259	68.923367
1075.166851	46.516194	68.928372
1074.280318	40.826595	68.933377
1073.586010	35.810626	68.938382
1072.974669	39.728686	68.943386
1072.967409	48.275571	68.948391
1072.257957	41.799371	68.953396
1071.125478	42.213560	68.958401
1070.716780	44.235829	68.963406
1069.754177	51.631503	68.968410
1069.487040	38.747115	68.973415
1068.635723	38.237281	68.978420
1067.739372	33.291041	68.983425
1066.987497	39.196883	68.988430
1066.621281	42.529444	68.993434
1066.373400	43.299368	68.998439
1065.341540	44.519709	69.003444
1064.281241	34.051426	69.008449
1063.929075	44.102823	69.013454
1063.230974	38.569635	69.018458
1063.410335	33.941273	69.023463
1062.042536	40.311383	69.028468
1061.169212	39.199429	69.033473
1060.868566	37.708371	69.038478
1059.960057	44.192062	69.043482
1059.923500	37.792078	69.048487
1058.563375	31.487698	69.053492
1057.865164	32.879446	69.058497
1057.285969	34.376335	69.063502
1057.154722	45.239332	69.068506
1056.552313	25.073000	69.073511
1055.485809	43.219208	69.078516
1054.570133	38.811515	69.083521
1054.412601	32.905515	69.088526
1053.005449	42.168142	69.093530
1051.924973	28.826624	69.098535
1051.185649	34.625322	69.103540
1051.169725	35.070541	69.108545
1050.908090	34.959444	69.113550
1050.103391	36.537184	69.118554
1050.023924	30.501770	69.123559
1049.328157	40.728839	69.128564
1047.917084	33.715196	69.133569
1047.427975	38.622407	69.138574
1046.809759	41.046064	69.143578
1046.669499	32.626312	69.148583
1044.827402	33.059397	69.153588
1044.500770	31.346619	69.158593
1044.122379	35.029798	69.163598
1043.555372	43.543064	69.168602
1043.198319	33.345922	69.173607
1042.762283	35.719040	69.178612
1041.685591	29.706772	69.183617
1041.100287	31.233916	69.188622
1040.203558	37.945315	69.193626
1039.565680	39.745924	69.198631
1038.580946	43.988836	69.203636
1038.263624	39.787351	69.208641
1037.745240	27.300853	69.213646
1037.230022	35.435791	69.218650
1036.292123	31.569909	69.223655
1035.649854	37.750258	69.228660
1035.146671	43.930475	69.233665
1034.634762	40.135714	69.238670
1032.998948	41.603951	69.243674
1032.659644	33.991536	69.248679
1032.226576	40.443546	69.253684
1031.783022	38.376993	69.258689
1031.460161	31.187269	69.263694
1030.213948	39.540936	69.268698
1029.204865	38.745511	69.273703
1028.421591	36.239397	69.278708
1027.797190	43.461504	69.283713
1027.639152	30.827249	69.288718
1026.883170	39.419845	69.293722
1026.964365	30.382729	69.298727
1026.051707	31.771733	69.303732
1024.962801	42.122572	69.308737
1024.828080	38.266773	69.313742
1023.781347	42.525436	69.318746
1022.812447	35.392267	69.323751
1022.186528	45.184637	69.328756
1021.602605	43.384873	69.333761
1021.251786	43.263394	69.338766
1020.597377	42.866290	69.343770
1019.470274	34.700399	69.348775
1018.601298	41.408233	69.353780
1018.403430	42.094993	69.358785
1018.009106	29.687116	69.363790
1017.195400	34.661361	69.368794
1016.365684	24.309132	69.373799
1015.444790	39.506342	69.378804
1015.058229	38.181572	69.383809
1014.982380	39.617529	69.388814
1014.266850	47.772172	69.393818
1013.111166	32.145503	69.398823
1012.402056	35.455867	69.403828
1011.699934	31.969198	69.408833
1011.609039	28.699157	69.413838
1010.561936	39.473078	69.418842
1009.699711	31.265779	69.423847
1009.284497	32.738142	69.428852
1008.740520	36.484021	69.433857
1008.102340	26.950396	69.438862
1006.740022	34.267686	69.443866
1006.330539	31.739800	69.448871
1005.763436	37.355070	69.453876
1005.327393	32.866831	69.458881
1004.890779	33.674999	69.463886
1003.731110	37.629337	69.468890
1003.093716	34.100007	69.473895
1002.803178	34.838162	69.478900
1001.921071	36.917035	69.483905
1001.078332	28.241821	69.488910
1000.338638	35.237762	69.493914
999.613821	28.637115	69.498919
999.200825	34.756887	69.503924
998.962844	40.600387	69.508929
998.112560	27.672999	69.513934
997.333733	36.957893	69.518938
996.794426	36.018080	69.523943
996.284503	41.781842	69.528948
995.183994	36.883211	69.533953
994.197802	41.446100	69.538958
993.057684	36.739770	69.543962
993.635156	36.141969	69.548967
992.784063	31.888224	69.553972
992.389529	34.784342	69.558977
992.254316	31.024943	69.563982
990.512532	39.088504	69.568986
990.084641	35.351596	69.573991
989.286904	36.293447	69.578996
988.843825	31.977329	69.584001
987.944885	29.624051	69.589006
987.233982	39.626751	69.594010
986.745638	34.078579	69.599015
986.304257	33.882616	69.604020
985.060802	37.561190	69.609025
984.788276	37.950489	69.614030
984.040773	41.336509	69.619034
983.531310	35.021467	69.624039
982.990871	39.000414	69.629044
981.634771	31.466223	69.634049
981.093014	29.800160	69.639054
980.249850	35.769007	69.644058
980.038779	33.331085	69.649063
979.530225	33.469111	69.654068
978.788055	30.498096	69.659073
978.816828	25.520545	69.664078
977.678450	36.043665	69.669082
977.282464	37.243936	69.674087
976.494310	29.871813	69.679092
974.898845	37.602045	69.684097
974.563575	37.251340	69.689102
973.756934	38.743375	69.694106
973.770966	38.141806	69.699111
973.291532	35.576168	69.704116
972.530925	38.032111	69.709121
971.949741	36.795542	69.714126
970.787651	42.161808	69.719130
969.835523	35.899289	69.724135
968.873052	37.344200	69.729140
968.211872	29.699294	69.734145
968.600594	30.546110	69.739150
967.318696	34.838739	69.744154
967.166926	31.876741	69.749159
966.553467	37.615604	69.754164
965.582417	35.739655	69.759169
965.105676	34.843208	69.764174
964.402878	39.627159	69.769178
963.813350	33.278467	69.774183
962.701667	34.337637	69.779188
962.024217	34.225920	69.784193
961.302863	33.483465	69.789198
960.559503	33.959716	69.794202
960.551317	39.000083	69.799207
960.471000	28.115731	69.804212
958.992200	29.922213	69.809217
958.568675	29.588991	69.814222
957.889955	26.996700	69.819226
956.924391	19.617472	69.824231
956.095698	22.592286	69.829236
955.169668	37.135935	69.834241
954.942950	24.713186	69.839246
954.325826	27.210081	69.844250
954.120688	18.807774	69.849255
952.749602	26.016841	69.854260
951.992051	30.897400	69.859265
951.699487	15.424912	69.864270
951.248134	27.650798	69.869274
950.759750	27.946811	69.874279
950.048302	27.401598	69.879284
949.275621	27.605781	69.884289
948.650766	24.454032	69.889294
947.156187	33.003790	69.894298
946.488513	30.087125	69.899303
946.139238	29.698559	69.904308
945.279248	34.838624	69.909313
944.744297	29.388438	69.914318
944.090062	31.966686	69.919322
943.902067	18.622755	69.924327
943.631329	28.716241	69.929332
943.163471	25.642204	69.934337
941.880138	17.327061	69.939342
940.994175	27.713796	69.944346
940.943323	31.055504	69.949351
939.927836	29.891346	69.954356
939.438231	32.487186	69.959361
938.937681	14.713601	69.964366
937.737107	31.048120	69.969370
936.615294	30.550296	69.974375
936.220433	27.766506	69.979380
935.275174	28.927436	69.984385
935.391961	26.409685	69.989390
934.556404	28.745054	69.994394
934.371106	27.835010	69.999399
933.322026	35.358787	70.004404
932.487804	32.866153	70.009409
932.141075	32.125065	70.014414
931.617519	30.158669	70.019418
930.287706	28.791781	70.024423
929.444684	29.832971	70.029428
929.176768	31.093807	70.034433
928.814338	29.595580	70.039438
928.152162	29.722028	70.044442
927.401179	25.048938	70.049447
926.700430	30.008976	70.054452
925.884971	29.004764	70.059457
925.492211	25.488417	70.064462
924.254310	30.806885	70.069466
923.453798	21.743168	70.074471
922.976899	28.904487	70.079476
922.216993	30.699561	70.084481
922.038761	29.489903	70.089486
921.461598	31.506297	70.094490
921.100848	27.406998	70.099495
920.404434	26.560021	70.104500
919.311194	33.571125	70.109505
918.900353	34.288443	70.114510
918.530943	33.092975	70.119514
917.396660	36.617873	70.124519
916.752623	33.232977	70.129524
916.100809	29.238788	70.134529
915.688359	26.206579	70.139534
914.497058	37.337160	70.144538
913.542319	24.374799	70.149543
913.273541	34.303355	70.154548
912.705278	29.721335	70.159553
912.759800	26.369555	70.164558
911.265924	38.974516	70.169562
910.357689	27.465429	70.174567
910.072378	29.766559	70.179572
909.400072	29.488581	70.184577
909.355081	28.069008	70.189582
907.821124	30.444263	70.194586
906.966905	25.426904	70.199591
906.371629	20.023373	70.204596
905.922660	27.037021	70.209601
906.183081	18.251054	70.214606
905.421156	33.357089	70.219610
904.215709	22.393097	70.224615
903.369939	27.380737	70.229620
902.713229	41.906290	70.234625
902.610558	31.689685	70.239630
900.941435	29.580040	70.244634
900.621280	25.291827	70.249639
899.795299	23.908126	70.254644
899.487784	36.453179	70.259649
899.013757	22.856679	70.264654
898.480216	30.129932	70.269658
897.767858	30.874815	70.274663
896.905808	22.823039	70.279668
896.177618	29.535582	70.284673
896.161510	30.321077	70.289678
894.840407	29.676616	70.294682
894.007171	26.123615	70.299687
893.503856	25.695913	70.304692
893.410497	29.952746	70.309697
892.527193	27.895611	70.314702
891.540974	36.007016	70.319706
890.996457	27.504953	70.324711
890.503932	24.746580	70.329716
888.983802	28.147313	70.334721
888.313761	17.795407	70.339726
887.642734	24.959186	70.344730
887.721950	21.127546	70.349735
887.206203	28.614844	70.354740
886.503353	22.989753	70.359745
886.214493	22.919248	70.364750
884.990529	29.182261	70.369754
884.294976	27.565050	70.374759
883.684406	30.077407	70.379764
883.318209	29.032963	70.384769
882.687011	28.919256	70.389774
881.509303	40.147772	70.394778
881.169167	26.025078	70.399783
880.671293	28.351958	70.404788
879.092349	34.792609	70.409793
878.588407	30.788888	70.414798
877.766816	27.413491	70.419802
877.405976	30.585671	70.424807
876.885246	27.720425	70.429812
876.971398	33.573137	70.434817
876.638668	29.651402	70.439822
875.500652	32.149500	70.444826
874.291960	26.490661	70.449831
874.080242	27.074409	70.454836
872.689189	36.564822	70.459841
872.048675	27.845534	70.464846
870.968529	32.846877	70.469850
871.034534	37.190094	70.474855
870.416342	35.785018	70.479860
870.002993	45.460460	70.484865
870.097206	28.391021	70.489870
868.749660	35.509635	70.494874
867.829378	24.554045	70.499879
867.531031	27.475139	70.504884
866.348443	31.519870	70.509889
865.622780	22.920164	70.514894
864.824176	35.829575	70.519898
864.472854	23.413977	70.524903
864.426024	27.615079	70.529908
863.248268	32.255399	70.534913
862.319081	22.846256	70.539918
861.186756	28.286777	70.544922
861.331036	23.878365	70.549927
860.953290	33.078384	70.554932
860.226141	24.349861	70.559937
859.271682	25.890913	70.564942
858.389494	31.815144	70.569946
858.039688	24.444152	70.574951
857.571150	23.705382	70.579956
856.852594	35.535745	70.584961
855.899691	27.181792	70.589966
855.184622	33.015823	70.594970
854.700466	27.624449	70.599975
853.607179	31.046814	70.604980
852.500877	29.733239	70.609985
852.147108	25.890502	70.614990
852.194885	35.629843	70.619994
852.060034	29.232110	70.624999
851.323228	28.831774	70.630004
849.736765	30.235171	70.635009
848.914414	23.062351	70.640014
847.889290	28.276497	70.645018
847.796204	32.879844	70.650023
847.890892	30.044184	70.655028
847.006360	33.647099	70.660033
846.373480	31.286961	70.665038
845.408342	36.728850	70.670042
844.769600	30.301773	70.675047
844.273263	33.915167	70.680052
843.104563	38.876030	70.685057
842.524170	22.914072	70.690062
841.946356	28.719068	70.695066
841.571540	29.356409	70.700071
841.256128	24.643466	70.705076
840.289585	24.610886	70.710081
839.447918	24.481132	70.715086
838.674063	31.612401	70.720090
838.192538	25.601665	70.725095
836.819737	24.918315	70.730100
836.102790	25.342299	70.735105
835.835004	15.995529	70.740110
835.101887	29.017264	70.745114
835.118586	27.578442	70.750119
834.411808	18.801837	70.755124
833.993481	23.993360	70.760129
833.398062	23.924054	70.765134
832.321290	33.982319	70.770138
831.711876	27.204847	70.775143
830.820345	33.569606	70.780148
829.875095	29.763055	70.785153
829.571869	23.274173	70.790158
828.679358	24.460428	70.795162
828.413329	27.756098	70.800167
827.193962	22.581052	70.805172
826.542951	33.877636	70.810177
826.419589	28.690505	70.815182
825.267157	30.822812	70.820186
825.558341	21.198727	70.825191
824.418580	24.096980	70.830196
823.245740	22.411146	70.835201
822.914085	23.529754	70.840206
822.242915	26.692725	70.845210
821.683554	19.279482	70.850215
821.090913	22.466105	70.855220
819.912742	30.179365	70.860225
819.567640	20.785446	70.865230
819.089787	29.163838	70.870234
818.192390	24.475589	70.875239
817.525381	20.395212	70.880244
816.437880	32.691774	70.885249
816.226882	18.770390	70.890254
815.557762	23.048871	70.895258
815.651065	30.008713	70.900263
815.026349	22.687976	70.905268
813.633543	26.757277	70.910273
813.370910	22.849201	70.915278
812.164600	33.125830	70.920282
811.170371	25.881016	70.925287
810.497005	28.414005	70.930292
809.718494	26.536294	70.935297
809.927522	28.635126	70.940302
809.410663	37.017441	70.945306
808.900193	25.986541	70.950311
808.056719	22.623197	70.955316
806.886248	26.119971	70.960321
806.611561	22.952473	70.965326
805.806581	25.403407	70.970330
804.717691	27.200772	70.975335
804.088563	20.267220	70.980340
803.555399	24.818846	70.985345
803.408781	18.205650	70.990350
802.516150	30.793683	70.995354
801.897357	23.820072	71.000359
801.025245	12.731136	71.005364
800.181497	27.216478	71.010369
800.035348	16.841168	71.015374
799.433324	22.928585	71.020378
798.221237	27.297312	71.025383
797.603946	30.058315	71.030388
796.646001	29.262075	71.035393
796.771913	26.862755	71.040398
796.145217	38.330036	71.045402
795.431017	31.380660	71.050407
794.447285	29.932426	71.055412
793.464668	34.364080	71.060417
793.304264	24.678803	71.065422
792.683574	24.972627	71.070426
792.126780	26.844631	71.075431
791.504175	28.518709	71.080436
790.087308	29.822815	71.085441
790.078123	19.086562	71.090446
789.341812	26.932152	71.095450
788.240574	24.743431	71.100455
787.964970	19.630145	71.105460
787.343350	24.820969	71.110465
786.896727	26.472797	71.115470
786.177328	31.800760	71.120474
785.210120	34.997080	71.125479
784.509193	26.425127	71.130484
784.075915	26.854604	71.135489
783.608759	14.098496	71.140494
782.356270	24.579996	71.145498
781.703290	22.775915	71.150503
781.496928	23.614524	71.155508
780.774693	26.033130	71.160513
779.984857	23.009137	71.165518
779.017480	29.085329	71.170522
778.405013	24.397227	71.175527
777.973098	19.564915	71.180532
777.299950	24.611811	71.185537
777.291204	21.256663	71.190542
775.951570	33.048949	71.195546
775.078462	21.730854	71.200551
774.863292	25.228986	71.205556
774.135737	29.474853	71.210561
773.487791	24.752568	71.215566
772.117481	31.988777	71.220570
771.816007	30.314736	71.225575
771.108191	32.663773	71.230580
770.617194	30.906940	71.235585
770.596606	24.419385	71.240590
769.323832	30.382507	71.245594
768.382378	30.488925	71.250599
767.875158	28.227663	71.255604
767.370133	27.630935	71.260609
767.165218	20.108436	71.265614
766.551244	26.290266	71.270618
765.152806	34.640052	71.275623
765.070338	31.502783	71.280628
764.272247	32.807868	71.285633
763.514163	35.836928	71.290638
762.123035	26.952182	71.295642
762.021801	24.984514	71.300647
761.498128	18.240527	71.305652
760.971293	35.352101	71.310657
760.841661	29.762256	71.315662
759.559663	23.664851	71.320666
758.815825	25.890197	71.325671
758.346633	25.733361	71.330676
757.850364	25.261048	71.335681
756.364351	21.305190	71.340686
755.977824	19.206798	71.345690
755.536385	18.995868	71.350695
755.087257	20.542738	71.355700
754.569393	31.089052	71.360705
753.457693	18.535723	71.365710
752.456979	23.062054	71.370714
752.054698	26.428827	71.375719
751.694870	16.384586	71.380724
751.172655	20.749611	71.385729
750.675566	18.897121	71.390734
749.394157	20.864442	71.395738
748.718539	21.130184	71.400743
748.865403	22.323526	71.405748
747.955489	25.315045	71.410753
747.031516	17.764945	71.415758
746.659432	21.321138	71.420762
745.432624	26.499985	71.425767
744.487601	28.344951	71.430772
743.571016	32.952396	71.435777
743.427419	22.885321	71.440782
742.690598	28.494941	71.445786
741.889316	23.364742	71.450791
741.898250	23.384935	71.455796
741.381016	30.460410	71.460801
740.674311	25.838980	71.465806
739.872523	25.511765	71.470810
739.130189	22.125584	71.475815
738.634455	24.220409	71.480820
737.544910	25.861988	71.485825
736.943360	22.782857	71.490830
736.380352	29.507376	71.495834
735.897835	21.722583	71.500839
735.298682	27.164154	71.505844
734.066686	25.121392	71.510849
733.306511	21.540516	71.515854
732.870791	17.332513	71.520858
732.822593	17.947066	71.525863
732.358789	16.967117	71.530868
731.295151	27.021560	71.535873
730.452902	15.201647	71.540878
729.877364	17.218569	71.545882
729.144213	18.881592	71.550887
728.106261	22.856969	71.555892
727.188201	24.358653	71.560897
726.754264	11.440169	71.565902
726.420967	13.307837	71.570906
725.996656	14.517712	71.575911
725.719683	12.511077	71.580916
724.461011	26.298989	71.585921
723.788831	19.649525	71.590926
723.391426	24.491697	71.595930
722.673956	27.283289	71.600935
721.654075	13.504839	71.605940
720.732405	26.959115	71.610945
720.289325	14.409282	71.615950
719.836181	22.175577	71.620954
719.356305	25.656296	71.625959
718.898862	21.525432	71.630964
717.484698	35.287492	71.635969
717.180217	18.690579	71.640974
716.572405	23.113294	71.645978
715.821970	28.208566	71.650983
715.775828	25.793723	71.655988
714.780723	22.221519	71.660993
714.084468	23.558110	71.665998
712.994271	23.037162	71.671002
712.776016	26.899355	71.676007
712.299766	26.844779	71.681012
710.806605	31.962690	71.686017
710.532527	22.791477	71.691022
709.913681	25.069229	71.696026
709.624941	22.435039	71.701031
709.116272	10.482205	71.706036
708.221272	20.613540	71.711041
707.456806	15.098908	71.716046
706.480834	17.987282	71.721050
705.566306	17.522684	71.726055
705.092009	12.124914	71.731060
704.383364	12.994706	71.736065
704.172580	12.387840	71.741070
703.884483	13.134275	71.746074
702.947548	20.587550	71.751079
701.905901	19.137023	71.756084
701.051634	19.628364	71.761089
700.921648	11.988836	71.766094
700.556443	14.191558	71.771098
698.975096	26.355634	71.776103
698.312846	17.833131	71.781108
697.504792	19.812131	71.786113
697.099637	19.278035	71.791118
696.828512	26.569885	71.796122
696.368560	15.473525	71.801127
695.686531	12.249514	71.806132
694.914602	19.008637	71.811137
694.277249	5.832135	71.816142
693.607959	21.270425	71.821146
692.973072	21.649979	71.826151
692.131641	28.889541	71.831156
690.744762	23.018537	71.836161
690.687814	19.459294	71.841166
690.294222	20.243539	71.846170
689.738733	20.621332	71.851175
688.801067	12.088388	71.856180
687.398397	20.374568	71.861185
687.090024	17.393238	71.866190
687.019064	15.770500	71.871194
686.433012	17.849225	71.876199
686.397514	13.310180	71.881204
685.231193	20.570267	71.886209
684.151002	13.036292	71.891214
683.648699	14.060991	71.896218
682.782337	18.942057	71.901223
681.934169	19.175398	71.906228
681.414979	22.962837	71.911233
681.159396	11.807393	71.916238
680.316377	12.451539	71.921242
679.618312	15.047189	71.926247
679.018876	18.307615	71.931252
678.252517	23.490481	71.936257
677.820316	23.081013	71.941262
677.366150	14.469186	71.946266
675.901370	24.301057	71.951271
675.266807	15.604484	71.956276
674.692896	19.606549	71.961281
674.211408	16.709348	71.966286
674.015877	15.314782	71.971290
672.679272	23.444788	71.976295
671.897167	17.716881	71.981300
671.401698	17.924929	71.986305
671.074720	23.881554	71.991310
670.166507	23.127739	71.996314
670.240521	17.469861	72.001319
669.059618	10.808493	72.006324
668.237733	21.964221	72.011329
667.885612	17.549679	72.016334
667.702438	16.816511	72.021338
666.351875	19.317119	72.026343
665.582912	22.417917	72.031348
665.083798	30.186171	72.036353
664.438605	19.326013	72.041358
663.717550	20.191622	72.046362
662.581994	17.961053	72.051367
662.266151	15.109288	72.056372
661.482821	21.756296	72.061377
661.125680	25.288619	72.066382
660.854038	19.056442	72.071386
659.942835	21.143509	72.076391
659.271860	26.304905	72.081396
658.484749	27.124204	72.086401
658.261731	22.226911	72.091406
656.670983	22.673918	72.096410
655.833045	18.690746	72.101415
655.659404	16.876401	72.106420
655.016336	18.685045	72.111425
654.875559	18.686284	72.116430
654.543019	20.494224	72.121434
653.473385	23.051305	72.126439
652.730461	19.339998	72.131444
651.831088	28.967646	72.136449
650.683101	20.045634	72.141454
650.080372	31.577880	72.146458
649.372253	24.588421	72.151463
649.336417	20.652953	72.156468
648.664973	25.298143	72.161473
648.362016	18.230984	72.166478
647.310744	21.801311	72.171482
646.446769	20.760464	72.176487
645.749651	15.611654	72.181492
645.176661	20.693898	72.186497
644.885603	19.802777	72.191502
644.165850	23.557478	72.196506
642.888048	18.408685	72.201511
642.804226	17.733889	72.206516
642.377572	18.936278	72.211521
641.627419	17.405431	72.216526
640.683197	24.338546	72.221530
639.730550	23.466435	72.226535
639.680035	14.928741	72.231540
638.265527	23.570625	72.236545
637.754579	24.226172	72.241550
637.449469	26.478995	72.246554
636.488206	26.149910	72.251559
636.248149	15.120489	72.256564
634.990538	16.600235	72.261569
634.476618	22.496129	72.266574
634.066653	20.144806	72.271578
633.272977	23.848230	72.276583
633.307668	21.726235	72.281588
632.047767	20.758749	72.286593
631.368730	15.707497	72.291598
630.663597	22.552283	72.296602
629.573714	17.589182	72.301607
629.354143	19.579073	72.306612
628.554985	28.485778	72.311617
628.166599	20.143724	72.316622
627.307895	26.770101	72.321626
626.685226	23.786968	72.326631
626.804744	15.061074	72.331636
625.527276	28.403823	72.336641
624.591069	16.651746	72.341646
623.831107	23.346068	72.346650
623.260335	29.433669	72.351655
622.845083	21.950382	72.356660
621.988764	23.876876	72.361665
620.961184	17.344375	72.366670
620.542886	21.074665	72.371674
619.706239	18.288055	72.376679
619.635966	19.844627	72.381684
619.782999	21.663162	72.386689
618.931313	18.602829	72.391694
618.144650	15.559775	72.396698
616.947836	29.594852	72.401703
616.052137	16.409338	72.406708
615.347846	24.640615	72.411713
614.955436	17.135655	72.416718
614.281461	20.026380	72.421722
613.202192	30.557568	72.426727
612.575048	20.606516	72.431732
612.081085	31.079659	72.436737
611.412147	21.693104	72.441742
610.953856	23.610218	72.446746
610.495711	30.291910	72.451751
609.898616	24.973608	72.456756
609.035675	32.527505	72.461761
608.159090	26.124650	72.466766
607.814267	25.539174	72.471770
606.168929	30.790547	72.476775
605.707256	26.360044	72.481780
605.164151	28.627988	72.486785
604.354687	26.632862	72.491790
604.226629	25.425280	72.496794
603.486135	23.969359	72.501799
603.295301	17.585984	72.506804
602.712957	25.957807	72.511809
602.192987	20.025932	72.516814
601.394165	22.659775	72.521818
600.242376	27.791063	72.526823
599.296428	23.849301	72.531828
598.239462	37.049287	72.536833
598.213996	19.345972	72.541838
597.607210	26.766774	72.546842
597.144488	33.762655	72.551847
597.158696	25.138086	72.556852
596.203182	23.902549	72.561857
595.657550	23.211750	72.566862
594.617334	20.386212	72.571866
592.798287	22.474502	72.576871
592.544263	18.636417	72.581876
591.794581	24.266014	72.586881
591.564225	19.767464	72.591886
591.210437	15.940552	72.596890
590.504449	28.338333	72.601895
590.137413	20.077887	72.606900
589.138056	24.419286	72.611905
588.316495	16.678009	72.616910
587.794706	20.718516	72.621914
587.206407	23.805737	72.626919
586.832335	11.833816	72.631924
585.415228	24.488033	72.636929
584.905220	11.817471	72.641934
584.843311	13.579045	72.646938
583.639843	23.972837	72.651943
583.595143	14.686168	72.656948
582.402913	27.993003	72.661953
581.891190	20.021808	72.666958
581.475696	26.876576	72.671962
580.470189	27.833563	72.676967
579.715287	14.531576	72.681972
578.804080	15.649239	72.686977
578.313367	15.635442	72.691982
578.043971	20.416213	72.696986
577.611879	30.577981	72.701991
577.088895	30.129212	72.706996
576.018667	29.473039	72.712001
575.537285	18.706409	72.717006
574.381410	22.891085	72.722010
573.330235	33.244186	72.727015
573.292127	25.222628	72.732020
572.579327	37.202792	72.737025
572.256304	26.671509	72.742030
572.078122	26.560351	72.747034
570.624750	30.945994	72.752039
570.185201	18.606364	72.757044
569.029093	24.802941	72.762049
567.950362	19.107329	72.767054
567.836358	22.275119	72.772058
567.257785	21.893899	72.777063
566.940970	16.033796	72.782068
566.463870	23.323436	72.787073
565.446418	17.601932	72.792078
564.677192	19.352075	72.797082
564.029586	27.731529	72.802087
563.589801	19.470922	72.807092
562.168441	26.717497	72.812097
561.311470	27.584700	72.817102
561.192335	17.483859	72.822106
560.490278	21.776296	72.827111
560.399185	19.000103	72.832116
559.311536	25.852020	72.837121
558.977464	18.120770	72.842126
558.116976	26.429337	72.847130
557.018740	29.418420	72.852135
556.798177	11.998799	72.857140
556.165907	23.377030	72.862145
555.671218	19.439272	72.867150
554.822361	23.807386	72.872154
553.949273	19.262659	72.877159
553.476892	16.241158	72.882164
553.040792	23.967433	72.887169
551.883754	19.210059	72.892174
551.068812	15.441247	72.897178
550.338961	18.203008	72.902183
549.940798	16.341487	72.907188
549.840014	31.471991	72.912193
549.243639	14.368195	72.917198
548.326156	11.415857	72.922202
547.576930	15.753083	72.927207
547.312677	15.222093	72.932212
546.166040	25.451031	72.937217
545.136003	21.301072	72.942222
544.582957	11.678774	72.947226
543.959093	15.687828	72.952231
543.349060	19.148228	72.957236
542.739358	26.448750	72.962241
542.381284	16.411352	72.967246
541.324697	23.443069	72.972250
540.588776	20.197925	72.977255
539.837011	21.683384	72.982260
539.592363	25.205909	72.987265
539.196692	24.426268	72.992270
538.568273	23.956887	72.997274
537.500899	27.925498	73.002279
537.269572	32.798823	73.007284
536.432404	32.764267	73.012289
535.411722	28.665598	73.017294
534.672399	26.756355	73.022298
534.153066	29.564149	73.027303
533.595719	23.135429	73.032308
533.086667	23.224246	73.037313
532.517464	24.642901	73.042318
531.718305	14.447415	73.047322
531.210236	27.995426	73.052327
530.578087	11.051314	73.057332
529.551791	29.807960	73.062337
528.374430	16.555086	73.067342
528.085019	21.252450	73.072346
527.548688	25.584385	73.077351
527.246674	12.429012	73.082356
527.013630	21.850524	73.087361
525.972772	25.430930	73.092366
525.334079	16.021456	73.097370
524.531834	24.688313	73.102375
523.386263	25.010139	73.107380
522.422201	29.378264	73.112385
521.859819	21.640352	73.117390
521.670870	22.577822	73.122394
520.969173	28.809829	73.127399
520.523043	14.261731	73.132404
520.221584	22.453195	73.137409
519.334421	23.590037	73.142414
518.181701	20.979178	73.147418
517.770590	27.761753	73.152423
517.557258	11.995150	73.157428
516.057801	22.465325	73.162433
515.111160	23.471446	73.167438
514.920167	21.411807	73.172442
514.590180	31.878561	73.177447
514.039220	16.027316	73.182452
513.441310	20.714387	73.187457
512.524012	25.957080	73.192462
511.741771	24.803970	73.197466
511.098901	30.636315	73.202471
510.939959	25.162035	73.207476
509.580317	29.653995	73.212481
508.567529	27.164020	73.217486
508.258435	31.370972	73.222490
507.512591	26.022522	73.227495
507.717506	22.164616	73.232500
507.210880	22.224207	73.237505
505.705730	24.586354	73.242510
505.246141	19.245695	73.247514
504.534645	25.484907	73.252519
504.242451	27.388962	73.257524
502.659828	33.445888	73.262529
502.251004	29.750380	73.267534
501.613317	19.589595	73.272538
501.370861	34.809103	73.277543
500.873270	25.543204	73.282548
500.185150	30.765181	73.287553
499.165605	35.061112	73.292558
498.819099	24.820036	73.297562
498.020958	29.378405	73.302567
497.946617	22.152099	73.307572
496.451547	26.549642	73.312577
495.435941	22.017508	73.317582
495.190225	16.166151	73.322586
494.230325	22.814617	73.327591
494.361536	8.210230	73.332596
493.153781	18.720812	73.337601
492.261752	29.444520	73.342606
491.879157	21.701858	73.347610
491.457035	24.862054	73.352615
491.461646	20.410482	73.357620
490.026925	23.560651	73.362625
489.410233	22.133269	73.367630
488.693258	17.173804	73.372634
488.271226	26.954919	73.377639
487.427376	21.334732	73.382644
486.400304	28.633755	73.387649
485.722893	25.102689	73.392654
485.234306	23.463893	73.397658
484.954629	25.403302	73.402663
484.613575	25.898707	73.407668
483.245141	27.957188	73.412673
482.884716	20.865164	73.417678
482.393014	18.176175	73.422682
481.170738	25.434045	73.427687
480.159504	28.064439	73.432692
479.635399	30.957129	73.437697
479.550106	30.699800	73.442702
479.195345	29.332924	73.447706
478.506320	25.934500	73.452711
478.010825	26.280723	73.457716
476.712430	33.117455	73.462721
476.179481	19.070134	73.467726
475.953153	22.110337	73.472730
474.527212	31.100381	73.477735
474.096898	21.839934	73.482740
473.851350	26.541625	73.487745
472.729988	24.408535	73.492750
471.698515	21.160369	73.497754
470.869688	21.967504	73.502759
470.711027	20.460848	73.507764
470.043855	25.597925	73.512769
469.493936	26.694353	73.517774
469.338325	20.085889	73.522778
468.399556	22.713340	73.527783
467.536776	14.923898	73.532788
466.725646	25.885966	73.537793
466.327148	23.053908	73.542798
466.204305	20.119354	73.547802
464.703549	34.823473	73.552807
464.243289	23.596165	73.557812
463.605455	29.126088	73.562817
463.304456	24.559527	73.567822
462.560038	21.836087	73.572826
461.181264	30.988962	73.577831
460.313600	23.909262	73.582836
460.256695	28.192202	73.587841
459.720813	28.782176	73.592846
459.395762	29.835334	73.597850
458.142702	34.193392	73.602855
457.647429	24.813821	73.607860
456.796134	33.910254	73.612865
456.183309	33.705828	73.617870
456.281626	26.826889	73.622874
455.072930	35.302897	73.627879
454.259465	25.479724	73.632884
453.600415	31.413130	73.637889
453.554689	26.467318	73.642894
452.189245	24.201991	73.647898
451.186450	31.158589	73.652903
451.115745	29.536208	73.657908
450.196376	34.069176	73.662913
449.848491	34.738639	73.667918
449.546678	23.412345	73.672922
448.126823	34.102176	73.677927
447.583173	18.737956	73.682932
446.818047	24.207197	73.687937
446.628872	29.301837	73.692942
446.206983	17.980730	73.697946
444.753914	35.197717	73.702951
444.119762	19.357193	73.707956
443.645221	23.107788	73.712961
443.241773	34.758640	73.717966
443.000537	17.897551	73.722970
441.832865	28.743889	73.727975
441.154578	26.479223	73.732980
440.188447	29.524634	73.737985
439.757100	23.885476	73.742990
439.435148	21.742895	73.747994
437.937125	23.176658	73.752999
437.802590	17.595975	73.758004
437.295203	22.003082	73.763009
436.912485	24.746815	73.768014
435.827675	21.059008	73.773018
434.867427	26.956009	73.778023
434.591883	30.462911	73.783028
433.999919	26.546180	73.788033
433.872417	24.123580	73.793038
432.475318	21.238458	73.798042
431.420381	35.113068	73.803047
430.778705	29.141686	73.808052
430.352085	26.973228	73.813057
429.742218	33.665927	73.818062
430.047066	26.141368	73.823066
428.228780	30.446697	73.828071
427.825897	30.215375	73.833076
427.387133	29.758901	73.838081
427.009830	26.900716	73.843086
426.214122	28.103213	73.848090
424.983090	40.867283	73.853095
424.649162	20.947255	73.858100
424.190976	30.663518	73.863105
423.354585	30.746868	73.868110
422.826391	19.057558	73.873114
422.018982	36.733080	73.878119
421.679998	21.270243	73.883124
420.828092	24.489096	73.888129
419.588599	27.010205	73.893134
419.091717	28.905923	73.898138
418.313762	32.163812	73.903143
417.853764	26.186955	73.908148
417.454378	31.610497	73.913153
416.944998	32.062126	73.918158
416.110714	31.093598	73.923162
414.997799	30.688711	73.928167
414.848062	26.814613	73.933172
414.261425	28.415862	73.938177
413.550180	17.166849	73.943182
413.319353	18.957371	73.948186
412.171882	26.624778	73.953191
411.538829	24.232768	73.958196
409.976230	24.008362	73.963201
409.243547	20.383368	73.968206
408.724795	20.300187	73.973210
408.786253	21.548016	73.978215
408.537111	21.235090	73.983220
407.788136	24.804968	73.988225
407.487395	24.168535	73.993230
406.272754	22.730356	73.998234
405.275979	27.864718	74.003239
404.792674	24.181593	74.008244
404.381298	26.946028	74.013249
402.956451	28.251611	74.018254
402.582000	15.853895	74.023258
401.850379	25.596489	74.028263
401.157689	29.335923	74.033268
401.081872	30.834239	74.038273
400.355755	36.582577	74.043278
399.990484	30.833421	74.048282
398.899277	32.690081	74.053287
398.584488	33.935289	74.058292
397.891397	27.386180	74.063297
396.332261	33.496737	74.068302
395.972367	23.626639	74.073306
395.604873	36.027599	74.078311
395.300277	21.196338	74.083316
394.416196	22.631077	74.088321
393.438824	26.561791	74.093326
393.065258	20.398428	74.098330
392.738855	28.501409	74.103335
391.820675	18.692256	74.108340
390.738743	25.194687	74.113345
389.747786	29.833083	74.118350
388.947620	27.452349	74.123354
388.306870	27.858208	74.128359
388.353597	24.607641	74.133364
388.007809	22.925833	74.138369
387.410807	29.451732	74.143374
386.471705	23.773687	74.148378
385.490442	27.085369	74.153383
385.383568	15.774233	74.158388
384.312461	27.122682	74.163393
383.282447	25.500903	74.168398
383.103999	27.768737	74.173402
382.577270	34.431007	74.178407
381.959487	26.881816	74.183412
380.804731	29.203292	74.188417
379.924946	25.202484	74.193422
379.779994	25.680471	74.198426
378.819331	33.954124	74.203431
379.200424	24.902772	74.208436
377.627540	23.843740	74.213441
376.772703	26.689704	74.218446
376.166597	27.001607	74.223450
375.437732	31.451808	74.228455
375.376025	28.923598	74.233460
374.826882	26.242098	74.238465
373.783156	27.181600	74.243470
373.056389	24.293318	74.248474
372.549522	23.378416	74.253479
372.384413	24.231679	74.258484
371.205773	29.611150	74.263489
370.583118	29.985886	74.268494
369.802873	17.617855	74.273498
368.941020	30.509694	74.278503
368.315760	28.906967	74.283508
367.393904	32.566082	74.288513
367.037608	35.632905	74.293518
366.818399	17.183283	74.298522
366.194573	37.333771	74.303527
365.191181	26.193252	74.308532
364.231073	17.694639	74.313537
363.517783	38.264647	74.318542
363.243672	25.322398	74.323546
362.558958	29.727535	74.328551
362.339910	26.771582	74.333556
361.249749	25.471545	74.338561
360.472594	28.227624	74.343566
360.142027	27.803530	74.348570
358.951764	31.335368	74.353575
358.339473	29.555560	74.358580
357.729734	32.741210	74.363585
357.215106	27.763272	74.368590
357.347504	24.218171	74.373594
355.789159	30.799101	74.378599
355.122291	32.442922	74.383604
354.547750	35.116912	74.388609
353.828393	34.123568	74.393614
353.624114	34.647248	74.398618
352.523915	30.824344	74.403623
351.929836	21.385157	74.408628
351.045521	23.183870	74.413633
350.285575	27.376914	74.418638
350.478493	22.645195	74.423642
349.436251	32.630100	74.428647
348.718610	28.104565	74.433652
347.811745	25.416092	74.438657
347.739394	26.994729	74.443662
347.300451	27.273645	74.448666
345.609723	27.860252	74.453671
345.163402	24.400520	74.458676
344.597737	24.750494	74.463681
344.046976	22.741473	74.468686
343.753919	22.985518	74.473690
342.369031	28.847158	74.478695
342.085255	21.292441	74.483700
341.508201	24.147639	74.488705
340.863707	32.736955	74.493710
340.814160	19.667811	74.498714
339.542142	35.574120	74.503719
338.935633	24.975817	74.508724
337.945209	29.892403	74.513729
336.724314	27.267227	74.518734
336.195521	18.650096	74.523738
335.970203	31.664540	74.528743
335.149092	17.579019	74.533748
334.608279	23.492561	74.538753
333.847572	23.489144	74.543758
334.003262	18.487902	74.548762
333.523996	24.229458	74.553767
332.574508	19.963520	74.558772
331.738169	22.396607	74.563777
330.912664	24.949408	74.568782
329.892793	21.593901	74.573786
329.127672	33.607112	74.578791
328.477002	29.637305	74.583796
328.071168	29.892391	74.588801
327.420707	32.190996	74.593806
327.493671	27.837050	74.598810
326.177769	26.934901	74.603815
325.617371	20.358727	74.608820
324.779711	29.979379	74.613825
324.150416	30.876676	74.618830
323.938484	25.557145	74.623834
322.675960	35.766904	74.628839
322.130170	20.875558	74.633844
321.707335	25.570136	74.638849
320.898377	31.685552	74.643854
320.402245	25.806872	74.648858
319.484722	30.665181	74.653863
318.882809	21.875859	74.658868
318.455020	27.508336	74.663873
317.702505	24.988799	74.668878
316.923027	19.680891	74.673882
315.965862	21.248558	74.678887
315.484091	30.538230	74.683892
314.968858	20.730296	74.688897
314.570379	25.934223	74.693902
313.902513	19.860783	74.698906
312.745180	29.172300	74.703911
312.404092	23.004170	74.708916
311.855777	17.764796	74.713921
311.256143	26.260768	74.718926
310.251346	16.285314	74.723930
309.236717	25.228970	74.728935
309.226942	22.192946	74.733940
308.490174	20.584868	74.738945
307.909910	24.620417	74.743950
307.083851	27.540007	74.748954
306.116392	29.382582	74.753959
306.048865	18.701385	74.758964
305.460917	21.555690	74.763969
304.420815	24.209615	74.768974
303.650019	14.502724	74.773978
303.143836	19.756291	74.778983
302.443781	17.755498	74.783988
301.977853	19.622631	74.788993
300.477841	19.109262	74.793998
300.367921	19.236662	74.799002
299.538293	24.408703	74.804007
299.169838	15.141638	74.809012
298.754559	23.552330	74.814017
298.049909	27.416580	74.819022
297.027633	17.086121	74.824026
296.236136	30.772304	74.829031
295.958105	15.750607	74.834036
295.527632	20.400708	74.839041
294.317110	25.612772	74.844046
293.927385	23.238283	74.849050
293.119044	23.801162	74.854055
292.476275	27.797298	74.859060
292.124644	23.225225	74.864065
290.628470	28.254555	74.869070
290.508784	23.935604	74.874074
289.673525	27.443317	74.879079
289.198121	20.296036	74.884084
288.832135	22.561674	74.889089
288.171287	23.653846	74.894094
287.689473	24.138261	74.899098
287.176312	26.879888	74.904103
285.891499	18.798904	74.909108
284.937136	23.757077	74.914113
284.004843	19.830025	74.919118
284.059374	21.238503	74.924122
283.335331	26.821502	74.929127
283.091469	20.063194	74.934132
281.894161	30.410190	74.939137
280.718496	26.907724	74.944142
280.642313	21.498225	74.949146
280.208104	29.620472	74.954151
279.624673	26.403711	74.959156
278.623292	29.498610	74.964161
277.555692	30.902460	74.969166
277.593156	26.883002	74.974170
276.790442	26.733251	74.979175
275.926117	20.316542	74.984180
274.990474	23.783834	74.989185
274.502311	20.309181	74.994190
274.362914	28.705350	74.999194
273.764928	32.813017	75.004199
273.194624	29.472040	75.009204
272.223659	33.219319	75.014209
271.012151	29.901409	75.019214
270.770079	23.346072	75.024218
270.304004	35.028571	75.029223
269.315076	24.789894	75.034228
268.998271	35.859080	75.039233
268.026821	29.628879	75.044238
267.726415	27.245792	75.049242
266.545136	25.174733	75.054247
265.659241	23.122909	75.059252
265.381238	26.584449	75.064257
264.782727	28.646802	75.069262
264.415138	26.360883	75.074266
263.383296	36.438749	75.079271
262.772212	24.996562	75.084276
262.051900	20.408745	75.089281
261.353002	25.406813	75.094286
261.114366	17.834899	75.099290
260.244925	26.185683	75.104295
259.294310	21.184606	75.109300
258.608818	26.419967	75.114305
258.156696	23.104918	75.119310
257.542209	21.338924	75.124314
256.788789	26.844861	75.129319
255.440004	18.666307	75.134324
255.241795	28.132755	75.139329
254.662814	31.614308	75.144334
254.434034	19.069686	75.149338
254.165677	28.153445	75.154343
253.611312	24.658959	75.159348
252.833213	24.435523	75.164353
251.856621	29.821830	75.169358
251.014713	26.841208	75.174362
249.785825	23.934813	75.179367
249.282831	23.628699	75.184372
248.664184	23.241362	75.189377
248.224386	22.948099	75.194382
248.194734	18.115593	75.199386
246.950018	25.748777	75.204391
245.956794	19.654152	75.209396
245.961542	20.605005	75.214401
244.890828	19.812423	75.219406
244.370626	25.551527	75.224410
243.416775	27.351125	75.229415
243.199125	23.147254	75.234420
242.295533	21.944339	75.239425
241.849072	22.627949	75.244430
241.182999	18.753165	75.249434
239.989512	21.979676	75.254439
238.966165	24.537589	75.259444
238.466885	27.152506	75.264449
238.189791	22.725944	75.269454
237.776553	19.278715	75.274458
237.309001	31.246051	75.279463
236.757344	24.853119	75.284468
235.766919	25.032770	75.289473
234.751599	28.135987	75.294478
234.862218	17.354400	75.299482
233.823234	21.676203	75.304487
232.714675	24.608307	75.309492
232.174326	26.125463	75.314497
231.967740	25.066743	75.319502
231.400853	22.690262	75.324506
230.442743	21.585899	75.329511
229.471313	26.399384	75.334516
229.063077	27.112757	75.339521
228.417807	38.624275	75.344526
228.464104	27.301109	75.349530
227.016424	31.211421	75.354535
226.314467	33.197174	75.359540
225.663765	30.019976	75.364545
225.180414	33.736572	75.369550
224.891066	30.426780	75.374554
223.657061	28.176098	75.379559
222.986866	27.606165	75.384564
222.424500	21.150340	75.389569
221.964568	24.360056	75.394574
221.635493	25.440363	75.399578
220.336389	23.549768	75.404583
219.716492	22.486506	75.409588
218.839291	19.811135	75.414593
218.269062	25.770776	75.419598
218.526773	18.551523	75.424602
217.702595	25.836722	75.429607
216.626115	21.213657	75.434612
216.300547	18.600824	75.439617
215.215087	26.473936	75.444622
214.224031	28.114927	75.449626
213.566343	20.356708	75.454631
213.000529	15.803600	75.459636
212.781469	21.011507	75.464641
212.170138	24.328486	75.469646
211.562380	23.677593	75.474650
210.473078	24.588629	75.479655
210.020473	23.478930	75.484660
209.262928	14.217003	75.489665
208.981077	18.511651	75.494670
207.974036	15.560926	75.499674
207.192464	16.737350	75.504679
206.731867	21.977583	75.509684
206.554699	19.369706	75.514689
205.007025	23.520965	75.519694
204.196085	23.032000	75.524698
203.665818	23.037258	75.529703
203.021936	22.643596	75.534708
203.107063	15.820618	75.539713
202.504692	25.015703	75.544718
201.627122	13.730924	75.549722
200.752323	20.062490	75.554727
200.149752	25.885974	75.559732
199.486921	14.936600	75.564737
198.477083	26.728879	75.569742
198.034161	18.533215	75.574746
197.261655	22.076759	75.579751
196.730692	29.582078	75.584756
196.572712	16.838633	75.589761
195.451768	32.320396	75.594766
194.592389	25.917462	75.599770
193.853200	20.855687	75.604775
193.356046	22.849754	75.609780
193.257537	22.145514	75.614785
191.909170	30.277633	75.619790
191.139175	16.908881	75.624794
190.441054	25.969206	75.629799
190.067798	24.010301	75.634804
189.833575	16.478296	75.639809
189.130990	28.301192	75.644814
188.190824	15.275016	75.649818
187.411078	25.525182	75.654823
186.739630	23.535687	75.659828
186.530843	26.856292	75.664833
185.198759	30.117627	75.669838
184.471671	23.937926	75.674842
183.723628	23.056890	75.679847
183.530511	22.842128	75.684852
183.337175	16.387392	75.689857
182.612158	24.878810	75.694862
181.356645	23.763074	75.699866
180.507739	24.848026	75.704871
180.277999	21.606965	75.709876
179.868916	14.800816	75.714881
179.216207	26.310838	75.719886
178.779981	16.702538	75.724890
177.599172	21.890190	75.729895
176.705044	18.569217	75.734900
176.777177	13.619012	75.739905
175.820387	19.468482	75.744910
175.082062	22.037149	75.749914
174.261611	34.406802	75.754919
173.599491	24.455535	75.759924
172.533028	25.591597	75.764929
171.407442	22.526605	75.769934
171.408728	18.940039	75.774938
170.897859	28.023921	75.779943
170.662765	26.661032	75.784948
170.462265	26.753440	75.789953
169.317920	27.921405	75.794958
168.719124	14.561997	75.799962
167.680946	13.769777	75.804967
166.986140	13.780747	75.809972
166.131291	19.006465	75.814977
165.363453	23.387582	75.819982
165.203486	25.723694	75.824986
164.958962	24.392025	75.829991
164.162754	23.668845	75.834996
163.284541	17.661495	75.840001
162.255428	16.650631	75.845006
161.863672	9.148402	75.850010
160.680073	18.095381	75.855015
159.746970	17.848799	75.860020
159.413030	8.844251	75.865025
158.736104	14.999408	75.870030
158.505206	11.151482	75.875034
158.165146	19.278899	75.880039
157.776506	17.648272	75.885044
156.672784	13.824847	75.890049
155.552529	17.426824	75.895054
155.517904	20.157475	75.900058
154.785600	15.336489	75.905063
153.634694	12.013755	75.910068
153.005227	14.748093	75.915073
152.305711	20.381368	75.920078
152.273886	13.418189	75.925082
150.932287	16.264740	75.930087
149.890056	16.325008	75.935092
149.315284	17.164430	75.940097
148.503655	26.930622	75.945102
148.524387	17.444900	75.950106
148.322628	19.644895	75.955111
147.836001	26.084783	75.960116
146.893222	21.686696	75.965121
145.742220	23.719835	75.970126
145.465888	15.156961	75.975130
144.792680	23.135056	75.980135
144.037115	24.773583	75.985140
143.174882	14.907553	75.990145
142.458534	25.903912	75.995150
142.185699	18.944944	76.000154
141.243404	25.082840	76.005159
140.235555	26.036372	76.010164
139.433382	25.546310	76.015169
139.007874	31.109723	76.020174
138.697173	22.381433	76.025178
138.384098	30.235825	76.030183
137.348651	29.428933	76.035188
136.948403	20.931903	76.040193
136.161432	24.201636	76.045198
135.878381	21.034846	76.050202
134.202946	24.636879	76.055207
133.521350	27.598039	76.060212
133.199368	19.948067	76.065217
132.544831	34.972140	76.070222
131.872759	23.031659	76.075226
131.741112	26.425087	76.080231
130.767288	23.193571	76.085236
130.086331	15.268057	76.090241
129.319562	18.910882	76.095246
129.119450	10.634534	76.100250
128.387663	17.061188	76.105255
127.318791	16.658689	76.110260
126.842997	15.268388	76.115265
126.107077	21.078817	76.120270
125.898296	17.768646	76.125274
124.780139	22.179037	76.130279
123.799670	28.274141	76.135284
123.464089	19.618800	76.140289
122.856239	22.943875	76.145294
122.222611	12.437119	76.150298
120.990486	16.458915	76.155303
120.479895	19.091568	76.160308
120.334937	20.387407	76.165313
118.962909	19.864787	76.170318
119.305247	23.968750	76.175322
118.521563	27.507116	76.180327
117.415069	22.172426	76.185332
117.206553	14.308414	76.190337
116.084659	29.754029	76.195342
115.539641	23.988365	76.200346
114.954592	32.235546	76.205351
113.835319	23.698770	76.210356
113.805410	21.058549	76.215361
112.951028	28.376172	76.220366
112.501567	24.330862	76.225370
111.162307	18.008248	76.230375
110.434802	19.021481	76.235380
110.494792	22.813476	76.240385
109.954748	27.167784	76.245390
109.212057	26.997905	76.250394
108.162677	21.442255	76.255399
106.968462	22.345249	76.260404
107.053825	26.476294	76.265409
106.309598	28.492596	76.270414
105.425954	26.191357	76.275418
104.584418	23.722645	76.280423
104.264079	23.763368	76.285428
103.717473	14.209533	76.290433
103.254586	19.645149	76.295438
102.754125	22.394876	76.300442
101.969349	23.534369	76.305447
100.901331	27.052409	76.310452
100.457186	14.199368	76.315457
98.983835	23.841390	76.320462
98.295946	16.833593	76.325466
97.903571	25.713619	76.330471
97.289776	28.086880	76.335476
96.985635	23.316044	76.340481
96.489380	30.138484	76.345486
95.993148	19.297142	76.350490
95.612928	27.558150	76.355495
94.730112	29.054300	76.360500
94.208137	22.130551	76.365505
93.282910	24.594307	76.370510
92.258854	21.038670	76.375514
91.240750	24.820900	76.380519
90.811939	22.586547	76.385524
90.672207	16.801931	76.390529
89.926600	27.105852	76.395534
89.204262	24.592236	76.400538
88.670383	29.641368	76.405543
87.864076	20.713467	76.410548
87.169611	22.934780	76.415553
85.880327	24.518379	76.420558
85.511559	20.908817	76.425562
85.013632	20.376867	76.430567
84.454253	24.339384	76.435572
84.401244	25.298165	76.440577
82.788477	27.485084	76.445582
82.853413	22.325732	76.450586
81.819432	24.447368	76.455591
81.165299	20.881205	76.460596
80.883947	21.527839	76.465601
79.552371	22.842786	76.470606
78.970182	20.049766	76.475610
78.257668	18.425730	76.480615
77.954114	24.194799	76.485620
77.642951	15.855788	76.490625
76.609198	25.050630	76.495630
75.727501	28.040972	76.500634
75.128271	23.847277	76.505639
74.494112	29.314630	76.510644
74.490904	25.326625	76.515649
73.293848	27.041248	76.520654
72.629133	28.340941	76.525658
72.290701	25.598888	76.530663
71.127576	33.771111	76.535668
70.465688	23.108164	76.540673
69.698530	32.225727	76.545678
69.295252	19.907624	76.550682
68.887065	27.366239	76.555687
68.209110	26.481101	76.560692
67.137055	18.002954	76.565697
66.280456	31.750432	76.570702
65.782736	18.010585	76.575706
65.180708	20.512086	76.580711
64.501050	18.543361	76.585716
64.505982	17.444440	76.590721
63.060142	28.484167	76.595726
62.696339	22.553637	76.600730
62.365645	25.903038	76.605735
61.772095	23.587991	76.610740
60.654836	19.412066	76.615745
59.704723	35.180323	76.620750
59.619921	22.153579	76.625754
58.598267	23.594201	76.630759
58.154504	26.191720	76.635764
57.166172	13.847228	76.640769
56.301774	30.032599	76.645774
56.278842	24.527150	76.650778
55.583048	17.738994	76.655783
54.682666	24.528884	76.660788
53.960583	16.567415	76.665793
53.126383	25.474246	76.670798
52.572727	16.754472	76.675802
52.592025	23.850075	76.680807
51.700847	24.247998	76.685812
50.699771	20.856185	76.690817
50.000813	25.784814	76.695822
49.728254	16.388860	76.700826
49.182280	24.726439	76.705831
48.031518	26.576807	76.710836
47.542123	31.546477	76.715841
46.517244	38.460739	76.720846
46.362348	28.310834	76.725850
46.014904	34.656608	76.730855
44.788543	25.798761	76.735860
44.220016	21.547705	76.740865
43.432429	26.546791	76.745870
42.800989	25.986818	76.750874
41.894123	18.190840	76.755879
40.718350	23.405287	76.760884
40.419330	19.839821	76.765889
39.924984	24.972960	76.770894
39.628688	21.769768	76.775898
39.425274	25.865852	76.780903
38.470304	16.804781	76.785908
37.724913	13.983307	76.790913
37.174371	25.933679	76.795918
36.698010	17.288282	76.800922
35.616249	17.246808	76.805927
34.474586	20.667362	76.810932
33.936358	19.742484	76.815937
33.544621	22.587646	76.820942
33.641911	11.634300	76.825946
32.780441	21.797438	76.830951
31.590755	22.234309	76.835956
31.126312	16.861402	76.840961
30.331775	20.786483	76.845966
29.741983	14.225276	76.850970
28.751456	14.106981	76.855975
27.970316	24.503043	76.860980
27.656599	23.534936	76.865985
26.954321	20.340172	76.870990
26.883155	21.441793	76.875994
25.163630	23.279164	76.880999
24.619346	22.924895	76.886004
23.881663	15.082154	76.891009
23.624826	21.335418	76.896014
23.387490	24.315546	76.901018
23.045501	22.145257	76.906023
22.136378	28.337084	76.911028
21.497582	15.332710	76.916033
20.362366	26.586406	76.921038
19.559992	20.675819	76.926042
18.791707	18.704141	76.931047
17.985528	28.021014	76.936052
17.776925	19.033677	76.941057
17.219081	20.197428	76.946062
16.796571	23.752824	76.951066
15.977379	18.839402	76.956071
15.054445	21.346196	76.961076
14.847829	22.167902	76.966081
13.825411	28.530725	76.971086
12.783232	24.637579	76.976090
12.653880	20.043220	76.981095
11.718614	24.763306	76.986100
11.697882	17.215245	76.991105
10.335067	22.459794	76.996110
9.490689	19.555039	77.001114
9.198069	18.709624	77.006119
8.428283	25.649618	77.011124
8.035100	21.162859	77.016129
7.318964	22.907139	77.021134
6.428990	23.277233	77.026139
5.705194	12.771364	77.031143
4.845152	20.340213	77.036148
4.460159	15.148281	77.041153
4.083719	13.498606	77.046158