Tue Jun 08 17:48:53 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.326954	95.308340	0.000000
-0.613292	71.491524	0.005005
-2.325411	44.197084	0.010010
-4.677664	1.065735	0.015014
-9.038799	7.358038	0.020019
-14.145968	7.601436	0.025024
-18.098208	6.787913	0.030029
-22.415767	7.461941	0.035034
-26.537208	4.842034	0.040038
-30.112316	1.837548	0.045043
-33.882777	9.266403	0.050048
-37.554611	4.130097	0.055053
-41.444844	7.856188	0.060058
-45.032550	2.153658	0.065062
-49.070008	9.204388	0.070067
-52.592887	13.914665	0.075072
-56.235875	-3.419184	0.080077
-60.234579	7.271639	0.085082
-63.959221	-1.051164	0.090086
-67.674161	2.465295	0.095091
-71.282058	7.211872	0.100096
-75.119587	-2.124520	0.105101
-79.223225	3.492546	0.110106
-82.851364	-4.746925	0.115110
-86.443379	-0.849716	0.120115
-90.596998	6.150708	0.125120
-93.903662	8.859856	0.130125
-98.114799	14.123558	0.135130
-101.266210	4.311919	0.140134
-105.643778	5.917176	0.145139
-109.440900	-2.334344	0.150144
-112.703649	-2.551597	0.155149
-116.567041	-6.348884	0.160154
-120.244769	-8.675739	0.165158
-124.217452	-2.027219	0.170163
-128.148859	-6.084392	0.175168
-131.771852	-0.544974	0.180173
-136.096192	8.008743	0.185178
-139.419156	-1.505039	0.190182
-143.243684	0.576950	0.195187
-146.954868	2.440175	0.200192
-150.436751	4.404991	0.205197
-154.382509	3.321285	0.210202
-157.983185	-2.192225	0.215206
-161.802553	0.859487	0.220211
-165.814292	5.260947	0.225216
-169.157804	2.795106	0.230221
-172.986202	9.026978	0.235226
-176.963948	2.639136	0.240230
-180.614967	5.967102	0.245235
-184.620653	-11.575176	0.250240
-187.971585	-1.439406	0.255245
-191.986168	12.839791	0.260250
-195.656308	5.787802	0.265254
-199.426119	8.775392	0.270259
-203.436059	9.067249	0.275264
-206.817055	6.444061	0.280269
-210.491444	13.672243	0.285274
-214.269738	2.975912	0.290278
-217.944271	6.186764	0.295283
-222.191497	7.404670	0.300288
-225.868459	2.877656	0.305293
-229.890212	7.773486	0.310298
-233.346816	7.261565	0.315302
-237.030986	-2.612915	0.320307
-240.773720	5.513527	0.325312
-244.092746	0.799619	0.330317
-248.361388	-0.851475	0.335322
-252.016367	6.149605	0.340326
-255.968947	2.643641	0.345331
-259.994714	8.299212	0.350336
-263.508024	-8.515519	0.355341
-267.326529	14.871970	0.360346
-270.947441	1.732680	0.365350
-274.672533	0.725697	0.370355
-278.382756	8.175585	0.375360
-282.073655	-2.019388	0.380365
-286.084262	3.184818	0.385370
-289.784989	-3.857098	0.390374
-293.275426	1.088164	0.395379
-297.412750	3.311560	0.400384
-300.950903	-2.187684	0.405389
-304.795198	5.265485	0.410394
-308.729733	6.652057	0.415398
-312.113095	-1.213174	0.420403
-316.278019	-3.157499	0.425408
-319.683334	-12.221631	0.430413
-323.711891	-4.054787	0.435418
-327.326372	-9.290667	0.440422
-330.908616	2.925522	0.445427
-335.026910	-4.394437	0.450432
-338.257392	-0.616683	0.455437
-342.141380	7.195800	0.460442
-346.222605	0.065662	0.465446
-349.877969	-4.834789	0.470451
-353.740975	1.955751	0.475456
-357.846047	-2.820973	0.480461
-361.639429	-1.517381	0.485466
-364.896104	1.799128	0.490470
-368.448179	-3.967650	0.495475
-372.137937	7.213929	0.500480
-376.205485	-2.605705	0.505485
-380.371013	3.860597	0.510490
-383.902706	0.301889	0.515494
-387.764673	-3.215944	0.520499
-391.680356	8.632390	0.525504
-394.962998	-2.161424	0.530509
-398.852135	2.633250	0.535514
-402.918438	-7.140781	0.540518
-406.168604	-8.649492	0.545523
-410.207852	-2.588093	0.550528
-414.033557	-7.734771	0.555533
-417.725369	7.740047	0.560538
-421.089736	2.352791	0.565542
-425.190143	0.328426	0.570547
-428.891451	11.068772	0.575552
-432.592964	3.708586	0.580557
-436.621208	5.235285	0.585562
-440.156875	3.406131	0.590566
-443.705969	4.781162	0.595571
-448.066075	11.456948	0.600576
-451.582762	6.153476	0.605581
-455.301322	3.972450	0.610586
-459.289249	-2.377059	0.615590
-462.617846	-0.970373	0.620595
-466.763158	3.320847	0.625600
-470.170524	0.674763	0.630605
-473.978073	8.407924	0.635610
-478.146991	-5.415506	0.640614
-481.291963	7.090475	0.645619
-485.072843	6.736222	0.650624
-489.156298	2.460748	0.655629
-493.196584	10.541335	0.660634
-496.790522	4.577782	0.665638
-500.559884	8.378640	0.670643
-504.237669	5.775426	0.675648
-507.713197	7.270114	0.680653
-511.619492	5.899318	0.685658
-515.326970	-3.721839	0.690662
-519.251093	-1.123931	0.695667
-523.387893	8.981517	0.700672
-526.730351	1.371930	0.705677
-530.108569	1.422672	0.710682
-533.855848	9.934562	0.715686
-537.982478	0.382580	0.720691
-541.718677	9.295177	0.725696
-545.493484	-3.634294	0.730701
-549.541850	9.152254	0.735706
-553.189046	7.480083	0.740710
-556.779443	4.158155	0.745715
-560.703920	4.924319	0.750720
-564.613976	-3.250950	0.755725
-568.338935	9.319079	0.760730
-571.932732	5.572646	0.765734
-575.891451	11.827594	0.770739
-579.486262	10.500115	0.775744
-582.918622	5.445161	0.780749
-586.673635	7.023786	0.785754
-590.743549	5.118285	0.790758
-594.540827	6.839949	0.795763
-598.433432	12.041146	0.800768
-601.673430	4.663495	0.805773
-605.991608	3.469641	0.810778
-609.570824	1.513899	0.815782
-613.104119	-2.878358	0.820787
-617.008674	12.143271	0.825792
-621.463449	-2.659954	0.830797
-625.236567	3.401747	0.835802
-628.625635	5.657687	0.840806
-631.727319	-5.518658	0.845811
-635.718723	1.652142	0.850816
-639.338192	-4.092573	0.855821
-643.316504	7.449748	0.860826
-646.939439	6.567646	0.865830
-650.882646	4.441919	0.870835
-654.771405	0.369231	0.875840
-658.342869	-4.096562	0.880845
-662.466872	1.689882	0.885850
-666.120294	-2.146491	0.890854
-669.663998	3.702599	0.895859
-673.589200	5.735999	0.900864
-677.127508	0.775487	0.905869
-680.945620	1.294178	0.910874
-684.555266	1.290421	0.915878
-688.399235	-1.824861	0.920883
-692.542971	8.502165	0.925888
-695.867182	5.470570	0.930893
-700.008760	10.894172	0.935898
-703.756774	2.331650	0.940902
-707.202932	1.624508	0.945907
-710.920390	11.763532	0.950912
-714.395910	6.007990	0.955917
-718.636426	9.566227	0.960922
-722.184750	10.064307	0.965926
-726.134641	9.270358	0.970931
-730.013827	11.526025	0.975936
-733.394770	6.597758	0.980941
-737.459756	9.325814	0.985946
-741.243052	3.192494	0.990950
-744.812886	13.408831	0.995955
-748.751572	16.221398	1.000960
-752.396280	1.722153	1.005965
-756.702729	6.506651	1.010970
-760.258551	-4.007474	1.015974
-763.670496	8.034925	1.020979
-767.622816	7.946379	1.025984
-771.069986	5.031073	1.030989
-774.898294	12.452664	1.035994
-778.776999	1.029700	1.040998
-782.667591	2.652681	1.046003
-786.669785	11.219965	1.051008
-790.046098	10.583000	1.056013
-794.127458	5.141894	1.061018
-797.733100	3.417408	1.066022
-801.137680	5.779160	1.071027
-805.275050	15.157894	1.076032
-808.541364	9.420598	1.081037
-812.166722	10.944399	1.086042
-816.573017	1.672011	1.091046
-819.786623	0.247331	1.096051
-823.868939	11.705025	1.101056
-827.808740	-0.725350	1.106061
-831.474242	0.103567	1.111066
-835.027357	4.486086	1.116070
-838.893461	-2.864807	1.121075
-843.037388	7.032936	1.126080
-846.927046	-1.000303	1.131085
-850.650922	-1.604004	1.136090
-854.084134	-2.342852	1.141094
-857.347418	-4.206573	1.146099
-861.320211	3.325537	1.151104
-865.070817	-0.267811	1.156109
-869.161031	5.400527	1.161114
-872.636195	1.564128	1.166118
-876.385912	3.385624	1.171123
-880.542596	7.898234	1.176128
-884.111104	0.548004	1.181133
-888.201350	11.434787	1.186138
-891.908317	-2.231057	1.191142
-895.472584	-4.802891	1.196147
-899.309163	8.333600	1.201152
-902.889146	2.734698	1.206157
-906.531096	8.622147	1.211162
-910.264317	-1.919012	1.216166
-913.983323	1.173330	1.221171
-918.153117	4.039534	1.226176
-921.676721	0.287672	1.231181
-925.404747	14.567963	1.236186
-929.346644	6.425358	1.241190
-932.907479	4.654615	1.246195
-936.753576	10.905137	1.251200
-940.248075	7.296703	1.256205
-944.255280	1.806311	1.261210
-948.331801	15.804237	1.266214
-952.090275	7.688581	1.271219
-956.052676	3.865249	1.276224
-959.422789	2.559906	1.281229
-963.067988	11.748496	1.286234
-966.374969	9.277801	1.291238
-970.219477	7.293706	1.296243
-973.845936	5.647150	1.301248
-977.837246	-1.673033	1.306253
-982.250568	-1.581190	1.311258
-985.591367	0.958028	1.316262
-989.684978	2.585261	1.321267
-993.453597	12.222136	1.326272
-997.386254	-1.089482	1.331277
-1000.789594	-0.767239	1.336282
-1003.964145	-9.145708	1.341286
-1007.884440	9.820446	1.346291
-1011.983782	10.779262	1.351296
-1016.057951	0.496860	1.356301
-1019.596502	0.588538	1.361306
-1023.203820	-1.034815	1.366310
-1027.081608	-1.210914	1.371315
-1031.278195	7.094315	1.376320
-1034.564109	2.155512	1.381325
-1038.519619	9.675334	1.386330
-1042.283193	4.443579	1.391334
-1045.526528	-7.374752	1.396339
-1049.380447	-1.855373	1.401344
-1053.284191	-9.201562	1.406349
-1057.216696	-0.522875	1.411354
-1061.311420	2.619894	1.416358
-1064.864861	4.781242	1.421363
-1068.783717	1.792057	1.426368
-1071.806732	-2.801095	1.431373
-1075.373740	1.481767	1.436378
-1079.656028	6.550560	1.441382
-1083.405979	1.518596	1.446387
-1087.425418	7.107481	1.451392
-1090.848959	-8.154859	1.456397
-1094.873965	0.098067	1.461402
-1098.562210	-3.065676	1.466406
-1102.285075	-6.157949	1.471411
-1106.160839	-3.077605	1.476416
-1109.775520	-4.034144	1.481421
-1113.681026	2.374739	1.486426
-1116.989897	-5.695989	1.491430
-1120.991913	-6.806646	1.496435
-1124.992817	0.729329	1.501440
-1128.364794	-4.926794	1.506445
-1132.384635	5.800874	1.511450
-1136.209052	-0.389344	1.516454
-1139.993866	-8.546071	1.521459
-1144.272940	-1.977890	1.526464
-1147.353740	-1.537641	1.531469
-1150.786326	7.393937	1.536474
-1154.872498	6.835352	1.541478
-1158.513339	-1.211884	1.546483
-1162.575577	-5.929637	1.551488
-1166.305230	-9.259877	1.556493
-1169.970629	5.654381	1.561498
-1173.694391	8.603692	1.566502
-1177.524068	1.665264	1.571507
-1181.441450	8.789085	1.576512
-1184.982135	0.331545	1.581517
-1188.754767	4.053806	1.586522
-1192.330438	3.999251	1.591526
-1196.212367	-1.982495	1.596531
-1199.833510	7.633554	1.601536
-1203.778232	-1.528202	1.606541
-1207.827965	8.948896	1.611546
-1211.425753	5.192264	1.616550
-1215.155246	-12.592070	1.621555
-1218.821751	-0.710508	1.626560
-1222.351981	3.886657	1.631565
-1226.383779	-3.847862	1.636570
-1230.550797	4.568114	1.641574
-1233.719188	1.862272	1.646579
-1237.678511	4.299506	1.651584
-1241.452011	-5.675499	1.656589
-1245.615634	-0.550752	1.661594
-1249.642629	-1.019152	1.666598
-1252.758177	2.616360	1.671603
-1256.693242	3.333266	1.676608
-1260.191386	-0.341758	1.681613
-1263.729649	8.242159	1.686618
-1267.740128	4.089917	1.691622
-1271.124571	-4.602778	1.696627
-1275.285965	1.152748	1.701632
-1278.657812	6.355862	1.706637
-1282.818124	5.992885	1.711642
-1286.949760	-2.371741	1.716646
-1290.130223	-6.105643	1.721651
-1293.893839	5.750426	1.726656
-1297.785231	-3.210407	1.731661
-1301.545747	2.944409	1.736666
-1305.978902	3.681392	1.741670
-1309.235657	-5.939047	1.746675
-1313.058684	1.572064	1.751680
-1316.421551	-6.601310	1.756685
-1320.443393	1.756260	1.761690
-1324.216600	0.919892	1.766694
-1327.696427	-0.980468	1.771699
-1331.682450	6.279997	1.776704
-1335.376570	-2.769546	1.781709
-1339.022215	7.015408	1.786714
-1342.758266	9.001131	1.791718
-1346.767218	5.168811	1.796723
-1350.801260	8.681135	1.801728
-1354.160744	-6.612081	1.806733
-1358.171488	3.818974	1.811738
-1362.049867	7.022356	1.816742
-1365.451895	2.849372	1.821747
-1369.363817	0.585544	1.826752
-1373.162801	-0.776045	1.831757
-1376.979705	5.769017	1.836762
-1380.986443	0.181100	1.841766
-1384.319662	5.130178	1.846771
-1387.925471	5.457515	1.851776
-1391.650131	1.420103	1.856781
-1395.340668	6.482276	1.861786
-1399.731083	6.055531	1.866790
-1403.151163	-13.085065	1.871795
-1407.048085	-6.204552	1.876800
-1410.462237	-2.645913	1.881805
-1414.532247	-1.317962	1.886810
-1417.978076	-5.109983	1.891814
-1421.730055	-5.455738	1.896819
-1425.931501	0.757168	1.901824
-1429.674800	-10.238801	1.906829
-1433.045764	1.648594	1.911834
-1437.130410	3.146435	1.916838
-1440.734379	2.465822	1.921843
-1444.755856	2.544907	1.926848
-1448.400774	4.465333	1.931853
-1451.971937	4.948209	1.936858
-1455.904608	-2.088685	1.941862
-1459.593344	-0.396755	1.946867
-1463.697919	7.226797	1.951872
-1467.426416	-0.103693	1.956877
-1470.743347	4.766867	1.961882
-1474.234497	0.972813	1.966886
-1477.831530	0.242492	1.971891
-1482.236041	7.100552	1.976896
-1486.033830	1.272783	1.981901
-1489.533807	4.685981	1.986906
-1493.550882	10.410999	1.991910
-1497.505231	-1.293454	1.996915
-1501.453197	1.077800	2.006912
-1502.049879	2.895542	2.016909
-1499.429738	-4.753741	2.026906
-1496.645273	-2.889316	2.036902
-1494.598135	-1.744354	2.046899
-1492.726551	5.726856	2.056896
-1490.682184	2.562139	2.066893
-1488.588922	3.234809	2.076890
-1487.161187	0.173269	2.086886
-1485.060851	1.959612	2.096883
-1483.620535	-0.090771	2.106880
-1481.054372	0.744895	2.116877
-1479.038761	-1.543438	2.126874
-1477.748170	-1.731951	2.136870
-1475.596974	-0.523444	2.146867
-1474.052308	-6.999523	2.156864
-1472.007089	1.937338	2.166861
-1469.574228	-0.987429	2.176858
-1467.770908	-6.006147	2.186854
-1466.139225	-8.141964	2.196851
-1464.436412	-0.708142	2.206848
-1462.442547	-6.931390	2.216845
-1460.598417	-2.127462	2.226842
-1458.599173	-6.573979	2.236838
-1456.639149	-3.382655	2.246835
-1454.903391	-8.513856	2.256832
-1452.929859	0.031822	2.266829
-1450.910618	3.584870	2.276826
-1449.275058	-1.940926	2.286822
-1447.133873	1.972552	2.296819
-1445.389870	-5.320676	2.306816
-1443.854297	1.779876	2.316813
-1441.417642	0.424641	2.326810
-1439.950265	-4.834342	2.336806
-1438.009193	-2.159848	2.346803
-1435.734399	-0.443761	2.356800
-1434.254798	-1.886325	2.366797
-1432.334142	-2.516622	2.376794
-1430.204320	-1.398874	2.386790
-1428.439967	-2.680498	2.396787
-1426.706420	-1.142539	2.406784
-1424.695219	-1.129572	2.416781
-1422.880459	-4.280106	2.426778
-1420.743266	-2.374385	2.436774
-1419.296974	-4.979462	2.446771
-1417.071964	-3.442143	2.456768
-1415.155565	-6.854768	2.466765
-1413.660157	-3.976840	2.476762
-1411.465829	-2.267864	2.486758
-1409.414912	4.961541	2.496755
-1407.890797	0.999779	2.506752
-1405.943872	-0.157881	2.516749
-1404.031159	-0.330728	2.526746
-1402.159987	-4.002346	2.536742
-1400.245218	2.637085	2.546739
-1398.564011	-0.668737	2.556736
-1396.830214	-3.795471	2.566733
-1394.578466	1.271631	2.576730
-1392.301523	-3.479845	2.586726
-1390.471499	0.689859	2.596723
-1389.371439	6.212088	2.606720
-1387.179125	0.020383	2.616717
-1385.264045	-0.223210	2.626714
-1383.584563	-3.861892	2.636710
-1381.829135	-5.485400	2.646707
-1379.593568	-3.259442	2.656704
-1377.585427	6.411429	2.666701
-1375.859872	-2.020370	2.676698
-1373.939125	-0.151347	2.686694
-1371.997365	2.044068	2.696691
-1370.430166	1.093137	2.706688
-1368.396447	1.448072	2.716685
-1366.442098	0.576472	2.726682
-1364.511681	2.597971	2.736678
-1362.539184	1.022943	2.746675
-1360.827050	0.759683	2.756672
-1359.048696	-0.231861	2.766669
-1356.984254	-0.398343	2.776666
-1355.196052	-2.886263	2.786662
-1353.181395	-1.675973	2.796659
-1351.423542	6.249580	2.806656
-1349.883984	7.711027	2.816653
-1348.066352	1.157662	2.826650
-1345.639717	-0.016766	2.836646
-1343.964777	0.665390	2.846643
-1342.017435	0.991701	2.856640
-1340.112510	2.623171	2.866637
-1338.315137	1.156882	2.876634
-1336.125478	3.849195	2.886630
-1334.217691	4.430892	2.896627
-1332.747028	-0.205378	2.906624
-1330.950567	6.516066	2.916621
-1328.768214	-0.892335	2.926618
-1326.903661	-4.995935	2.936614
-1325.036725	-2.177046	2.946611
-1323.418828	9.204570	2.956608
-1321.708184	4.823093	2.966605
-1319.593533	2.172012	2.976602
-1317.701334	6.617601	2.986598
-1315.887321	7.044683	2.996595
-1313.859916	4.317692	3.006592
-1312.035390	8.611687	3.016589
-1310.169466	8.767040	3.026586
-1308.124904	7.836893	3.036582
-1306.461101	2.112243	3.046579
-1304.408191	8.335162	3.056576
-1302.387993	5.604276	3.066573
-1300.809236	7.252661	3.076570
-1299.251318	9.627468	3.086566
-1296.978903	4.210490	3.096563
-1294.730774	1.265380	3.106560
-1293.462330	3.437368	3.116557
-1291.417720	4.663095	3.126554
-1289.346603	6.823291	3.136550
-1287.618136	-0.470378	3.146547
-1285.822230	1.482968	3.156544
-1283.870434	3.753769	3.166541
-1281.864996	2.448186	3.176538
-1280.114717	3.922472	3.186534
-1277.876468	6.433371	3.196531
-1276.521294	6.623900	3.206528
-1274.365255	5.811761	3.216525
-1272.919618	4.897553	3.226522
-1270.532106	10.265882	3.236518
-1268.690793	5.777406	3.246515
-1267.041688	6.058940	3.256512
-1265.210572	9.759010	3.266509
-1263.482536	5.733814	3.276506
-1260.977959	10.932653	3.286502
-1259.767334	4.970473	3.296499
-1257.436838	4.065937	3.306496
-1255.325532	5.834707	3.316493
-1253.925993	1.484162	3.326490
-1251.848503	-0.196585	3.336486
-1250.080916	6.103822	3.346483
-1248.548949	8.740783	3.356480
-1246.381577	-1.997822	3.366477
-1244.502530	1.061291	3.376474
-1242.592474	-0.168215	3.386470
-1240.542212	5.238687	3.396467
-1238.502961	1.899095	3.406464
-1236.838231	4.121605	3.416461
-1234.870438	0.871353	3.426458
-1233.411182	5.642299	3.436454
-1231.261559	3.316045	3.446451
-1229.638535	1.659217	3.456448
-1227.070319	5.785215	3.466445
-1225.448916	2.827633	3.476442
-1224.105358	-6.104848	3.486438
-1221.942242	-3.218608	3.496435
-1220.147788	4.896354	3.506432
-1218.111510	-5.016654	3.516429
-1216.508320	-5.398678	3.526426
-1214.482615	-3.044106	3.536422
-1212.099131	0.489194	3.546419
-1211.034131	2.691801	3.556416
-1208.979601	8.603464	3.566413
-1206.444719	6.727598	3.576410
-1204.746788	3.083835	3.586406
-1203.187399	1.754509	3.596403
-1201.457230	0.267806	3.606400
-1199.369126	-1.199744	3.616397
-1197.607352	4.899339	3.626394
-1196.016244	5.293616	3.636390
-1193.900693	3.107998	3.646387
-1191.789243	1.762910	3.656384
-1190.064830	5.677759	3.666381
-1187.871323	5.555986	3.676378
-1186.320327	-1.921376	3.686374
-1184.420070	-1.924415	3.696371
-1182.318762	3.684795	3.706368
-1180.705195	8.493682	3.716365
-1178.903627	-0.171637	3.726362
-1176.494847	-3.922051	3.736358
-1175.246831	1.928946	3.746355
-1173.298594	2.997389	3.756352
-1171.276035	-0.854266	3.766349
-1169.259299	9.249986	3.776346
-1167.245383	1.687597	3.786342
-1165.713603	-1.223747	3.796339
-1163.559473	-0.750671	3.806336
-1161.633676	2.674323	3.816333
-1159.828268	6.983530	3.826330
-1158.250392	5.365702	3.836326
-1156.435743	2.100286	3.846323
-1154.525123	-4.479250	3.856320
-1152.349248	4.361064	3.866317
-1150.250666	10.902276	3.876314
-1148.992181	9.477623	3.886310
-1147.156387	4.590979	3.896307
-1145.292259	5.544645	3.906304
-1143.084695	7.013578	3.916301
-1141.020160	7.660532	3.926298
-1138.928304	11.551037	3.936294
-1137.428745	4.659923	3.946291
-1135.740509	8.186193	3.956288
-1133.984371	4.748640	3.966285
-1132.183055	4.887503	3.976282
-1129.826765	6.520605	3.986278
-1127.819238	3.636656	3.996275
-1126.024796	6.964871	4.006272
-1124.097548	11.410468	4.016269
-1122.502735	12.051540	4.026266
-1120.601322	6.639467	4.036262
-1118.907588	9.426546	4.046259
-1116.687243	5.769382	4.056256
-1115.202733	12.107796	4.066253
-1113.219079	8.387732	4.076250
-1110.886271	10.964296	4.086246
-1109.476295	6.368942	4.096243
-1107.587703	7.228712	4.106240
-1105.630938	3.921128	4.116237
-1103.503132	6.601269	4.126234
-1101.708644	5.483358	4.136230
-1100.060303	4.055800	4.146227
-1098.025596	0.689386	4.156224
-1096.272089	1.849004	4.166221
-1094.265632	2.481450	4.176218
-1092.373108	7.206906	4.186214
-1090.590509	1.663092	4.196211
-1088.795206	2.072539	4.206208
-1086.216726	0.050143	4.216205
-1084.870323	1.277299	4.226202
-1083.048028	3.905969	4.236198
-1081.378789	1.373375	4.246195
-1079.488325	6.895541	4.256192
-1077.456002	8.482338	4.266189
-1075.425650	5.764828	4.276186
-1073.548171	5.888661	4.286182
-1071.805368	9.639556	4.296179
-1070.045307	5.435433	4.306176
-1067.931270	8.960944	4.316173
-1066.362087	6.873549	4.326170
-1064.481185	6.748211	4.336166
-1062.351132	4.599687	4.346163
-1060.578830	1.762875	4.356160
-1058.480500	6.958881	4.366157
-1056.848084	7.367855	4.376154
-1054.844249	2.184044	4.386150
-1053.009018	9.623396	4.396147
-1051.033709	0.876514	4.406144
-1049.268633	-0.709788	4.416141
-1047.600811	-0.576820	4.426138
-1045.534952	1.795447	4.436134
-1043.788191	-3.507044	4.446131
-1041.791344	1.179181	4.456128
-1039.825387	1.068495	4.466125
-1037.885603	-4.614922	4.476122
-1036.205730	0.383803	4.486118
-1034.038864	3.578162	4.496115
-1032.204320	-3.209980	4.506112
-1030.398434	3.487468	4.516109
-1028.479397	-1.514596	4.526106
-1026.972690	1.093195	4.536102
-1025.155722	1.608423	4.546099
-1022.776624	0.019461	4.556096
-1020.879762	1.012617	4.566093
-1019.214283	0.986729	4.576090
-1017.491864	4.295347	4.586086
-1015.703517	1.151485	4.596083
-1013.640331	10.729731	4.606080
-1011.978370	8.492053	4.616077
-1009.817401	2.294043	4.626074
-1007.850420	2.483952	4.636070
-1006.033989	2.219528	4.646067
-1004.401472	-2.157905	4.656064
-1002.227824	3.510519	4.666061
-1000.371438	4.975008	4.676058
-998.548760	1.427280	4.686054
-996.656933	2.500749	4.696051
-994.860180	7.686914	4.706048
-992.897250	3.125497	4.716045
-991.196097	5.592815	4.726042
-989.560203	-0.807887	4.736038
-987.285365	0.426679	4.746035
-985.396406	-1.291131	4.756032
-983.505642	7.361901	4.766029
-981.607072	9.960925	4.776026
-979.856753	9.219380	4.786022
-978.037475	4.788153	4.796019
-976.137403	1.379698	4.806016
-974.176632	-1.805211	4.816013
-972.340609	2.607905	4.826010
-970.434132	-0.839192	4.836006
-968.660387	2.329821	4.846003
-966.894995	0.643508	4.856000
-964.986763	9.940120	4.865997
-963.088493	5.342390	4.875994
-960.833775	5.405855	4.885990
-958.996949	3.086403	4.895987
-957.312029	3.890704	4.905984
-955.190538	6.604810	4.915981
-953.617454	4.697002	4.925978
-951.936934	6.827997	4.935974
-949.623702	6.488977	4.945971
-947.735431	3.593963	4.955968
-946.297487	11.997917	4.965965
-944.143033	2.936951	4.975962
-942.055010	4.310321	4.985958
-940.547921	-1.714143	4.995955
-938.801499	0.918133	5.005952
-936.853714	7.233602	5.015949
-934.536122	6.987507	5.025946
-932.907204	1.159101	5.035942
-931.010157	-2.623477	5.045939
-929.123917	-3.713595	5.055936
-927.300696	-2.110589	5.065933
-925.484768	6.426482	5.075930
-923.481787	2.078351	5.085926
-921.561067	-3.276093	5.095923
-919.790371	-3.625900	5.105920
-917.715428	6.228216	5.115917
-916.116040	7.749904	5.125914
-914.269500	-2.154134	5.135910
-912.563592	1.672721	5.145907
-910.406830	-1.289315	5.155904
-908.762868	-4.671560	5.165901
-906.650213	1.848400	5.175898
-904.338325	0.994278	5.185894
-902.952586	4.846855	5.195891
-901.015048	2.126782	5.205888
-899.417684	2.173101	5.215885
-897.203068	4.970054	5.225882
-895.201975	4.000535	5.235878
-893.542988	1.052820	5.245875
-891.477432	-0.532834	5.255872
-889.894356	-0.712096	5.265869
-887.803561	1.964236	5.275866
-886.375649	-1.718821	5.285862
-884.182551	2.677700	5.295859
-882.048913	0.534575	5.305856
-880.411516	1.144321	5.315853
-878.339524	-0.054334	5.325850
-876.606476	-3.604412	5.335846
-874.568728	-6.131027	5.345843
-872.930922	1.309105	5.355840
-871.423522	-3.598127	5.365837
-869.173500	1.322957	5.375834
-866.688441	1.175409	5.385830
-865.346317	7.131695	5.395827
-863.446644	-1.053975	5.405824
-861.429335	5.613194	5.415821
-860.007748	-0.587063	5.425818
-858.046113	-0.767272	5.435814
-855.959793	3.554324	5.445811
-854.078785	-0.442047	5.455808
-852.324219	-0.151184	5.465805
-850.775872	0.837850	5.475802
-848.320712	-5.289652	5.485798
-846.443992	-1.701552	5.495795
-844.656190	-3.774624	5.505792
-842.676383	2.935351	5.515789
-840.832529	-0.070953	5.525786
-839.029028	-1.264998	5.535782
-836.999575	-2.653937	5.545779
-835.804013	-5.653688	5.555776
-833.685340	-7.162671	5.565773
-831.764068	-5.717150	5.575770
-829.926818	-5.555478	5.585766
-827.755138	-7.152204	5.595763
-825.930562	-6.231128	5.605760
-824.011024	1.806445	5.615757
-822.424262	2.442689	5.625754
-820.392342	1.454475	5.635750
-818.470938	4.208134	5.645747
-816.256527	1.613280	5.655744
-814.795719	0.408114	5.665741
-812.810646	0.955441	5.675738
-810.768085	0.620668	5.685734
-808.356929	-2.421345	5.695731
-807.561354	4.334623	5.705728
-805.793378	6.758143	5.715725
-803.613128	4.784109	5.725722
-801.276809	-3.459886	5.735718
-799.808337	0.203052	5.745715
-797.881269	5.590238	5.755712
-796.104103	2.225083	5.765709
-794.027899	5.814539	5.775706
-791.996401	0.881791	5.785702
-790.443727	2.552242	5.795699
-788.518298	-6.014062	5.805696
-786.578777	0.496951	5.815693
-784.910086	-0.507550	5.825690
-782.547274	-2.204642	5.835686
-781.013791	-8.995558	5.845683
-779.031715	1.810044	5.855680
-777.226262	0.588418	5.865677
-775.042559	-0.305287	5.875674
-773.594035	-1.186233	5.885670
-771.722977	-0.510633	5.895667
-769.357471	2.615391	5.905664
-767.855590	5.254146	5.915661
-765.869515	4.492773	5.925658
-763.986567	4.208339	5.935654
-762.094368	1.431686	5.945651
-760.131816	0.015929	5.955648
-758.603080	8.071214	5.965645
-756.872166	2.299260	5.975642
-754.701795	-3.534283	5.985638
-752.846368	3.902543	5.995635
-750.741882	7.926249	6.005632
-748.634543	8.306788	6.015629
-747.165624	6.568295	6.025626
-745.643181	1.987729	6.035622
-743.552015	2.061199	6.045619
-741.394815	9.100823	6.055616
-739.718415	7.001462	6.065613
-737.804524	4.666896	6.075610
-735.880069	3.286538	6.085606
-733.770021	2.081025	6.095603
-732.004979	1.195961	6.105600
-730.308862	2.895564	6.115597
-728.534583	-0.433105	6.125594
-726.536431	1.017056	6.135590
-724.482199	0.887016	6.145587
-722.865359	2.736972	6.155584
-720.975950	3.936263	6.165581
-718.958671	-1.100721	6.175578
-717.134891	2.193003	6.185574
-715.373077	-0.242711	6.195571
-713.277188	0.595886	6.205568
-711.529642	5.785887	6.215565
-709.578666	-2.103428	6.225562
-707.834753	1.624119	6.235558
-705.704222	-3.887581	6.245555
-703.839298	-2.346964	6.255552
-702.037524	-0.914467	6.265549
-700.381338	0.741809	6.275546
-698.453473	7.622815	6.285542
-696.331828	1.700434	6.295539
-694.554062	-0.297347	6.305536
-693.135210	0.436924	6.315533
-691.013325	2.558280	6.325530
-688.803455	5.253801	6.335526
-687.049959	1.497536	6.345523
-685.399245	1.127708	6.355520
-683.413203	1.582845	6.365517
-681.505317	-1.218204	6.375514
-679.251168	1.980733	6.385510
-677.355247	1.728493	6.395507
-675.812714	6.003998	6.405504
-674.016999	2.378816	6.415501
-672.425856	8.123288	6.425498
-670.292520	0.322439	6.435494
-668.297698	-2.990306	6.445491
-666.481935	-2.045912	6.455488
-664.286307	4.188434	6.465485
-662.827109	5.201531	6.475482
-661.110167	2.292167	6.485478
-659.062818	4.223191	6.495475
-656.975801	1.682684	6.505472
-655.063437	-4.251978	6.515469
-653.136745	-2.468212	6.525466
-651.464220	7.115632	6.535462
-649.370521	-0.933713	6.545459
-647.640175	-1.578032	6.555456
-646.398601	-0.030406	6.565453
-644.296869	0.613173	6.575450
-641.835369	-2.533825	6.585446
-639.772650	-3.403145	6.595443
-638.285910	3.174581	6.605440
-636.618785	-3.438069	6.615437
-634.632079	1.360371	6.625434
-632.843889	0.218042	6.635430
-631.116858	1.658654	6.645427
-628.599905	4.578159	6.655424
-627.063476	1.208139	6.665421
-625.385295	3.257465	6.675418
-623.129826	0.489273	6.685414
-621.250751	0.198847	6.695411
-619.867120	-1.324992	6.705408
-617.800277	0.277051	6.715405
-615.860466	4.243325	6.725402
-614.012045	2.585585	6.735398
-611.735417	1.226260	6.745395
-610.047180	3.929922	6.755392
-608.266232	1.054648	6.765389
-606.555737	5.561804	6.775386
-604.484657	0.672138	6.785382
-602.790433	-7.501105	6.795379
-600.945668	-4.680444	6.805376
-598.816784	-1.166325	6.815373
-597.162750	-1.094840	6.825370
-595.023986	-1.930949	6.835366
-593.474346	0.717459	6.845363
-591.526814	2.999995	6.855360
-589.193681	3.746565	6.865357
-587.471231	5.138184	6.875354
-585.953100	-1.580885	6.885350
-583.891772	-0.260062	6.895347
-581.784133	2.208816	6.905344
-580.015459	5.599401	6.915341
-578.397048	2.388433	6.925338
-576.489893	2.824747	6.935334
-574.514237	6.586494	6.945331
-572.470797	-1.856920	6.955328
-570.581744	2.771373	6.965325
-568.888024	7.385365	6.975322
-567.155669	1.437358	6.985318
-565.547613	-1.559994	6.995315
-563.409537	-1.701579	7.005312
-561.388320	1.352431	7.015309
-559.423401	-2.643995	7.025306
-557.628434	2.502369	7.035302
-555.834606	3.011493	7.045299
-553.598220	4.037105	7.055296
-552.096953	9.265092	7.065293
-550.072913	10.805351	7.075290
-548.047217	5.077341	7.085286
-546.392660	2.876276	7.095283
-544.361431	0.021711	7.105280
-542.826060	3.576836	7.115277
-540.925415	-4.376106	7.125274
-539.039083	2.676120	7.135270
-537.079101	-1.438014	7.145267
-535.227788	6.622881	7.155264
-533.260409	3.197917	7.165261
-531.517939	-2.494924	7.175258
-529.345716	-0.964274	7.185254
-527.244630	-4.155287	7.195251
-525.831382	-3.337795	7.205248
-524.047443	0.837066	7.215245
-521.992421	3.588885	7.225242
-519.694341	-0.567050	7.235238
-518.324647	-3.690268	7.245235
-516.279684	-2.538918	7.255232
-514.603450	0.299238	7.265229
-512.805343	-2.422043	7.275226
-510.802901	0.261736	7.285222
-508.956754	-7.074399	7.295219
-507.152148	-2.604691	7.305216
-505.074243	-0.314053	7.315213
-503.065075	8.306669	7.325210
-501.501594	-0.097844	7.335206
-499.271720	-1.223817	7.345203
-497.582360	-4.585256	7.355200
-495.741679	0.415759	7.365197
-493.852049	-2.518035	7.375194
-491.959514	-0.866263	7.385190
-489.901955	-4.243052	7.395187
-488.206417	-7.229698	7.405184
-486.344588	-0.533283	7.415181
-484.889173	-2.959419	7.425178
-482.368177	-5.407131	7.435174
-480.524984	-1.080775	7.445171
-478.539359	-0.801344	7.455168
-477.146768	3.787285	7.465165
-475.104706	0.175637	7.475162
-473.172213	-3.063494	7.485158
-471.533268	-5.765356	7.495155
-469.037038	-4.612365	7.505152
-467.346558	2.303162	7.515149
-465.715601	-1.006749	7.525146
-463.705305	0.540651	7.535142
-461.844376	2.932167	7.545139
-460.076057	-1.146683	7.555136
-458.531088	0.547346	7.565133
-456.589701	0.431653	7.575130
-454.281689	-3.030377	7.585126
-452.202806	-0.275504	7.595123
-450.706347	-7.503409	7.605120
-448.822254	1.912627	7.615117
-447.061651	2.374536	7.625114
-445.005701	0.343351	7.635110
-443.263540	-1.583015	7.645107
-441.350104	6.368467	7.655104
-439.179856	1.455533	7.665101
-437.718165	-3.146925	7.675098
-435.886953	1.516649	7.685094
-433.901008	2.745746	7.695091
-431.450853	4.170273	7.705088
-430.152259	3.964497	7.715085
-428.301453	7.216961	7.725082
-426.004579	8.098285	7.735078
-424.564451	7.865858	7.745075
-422.686484	9.731205	7.755072
-420.479907	6.765196	7.765069
-418.657518	9.402053	7.775066
-417.117840	5.287352	7.785062
-414.938619	3.887531	7.795059
-412.862850	6.013383	7.805056
-411.340938	10.019833	7.815053
-409.332268	8.290814	7.825050
-407.630857	7.228672	7.835046
-405.304783	6.208362	7.845043
-403.830793	0.053376	7.855040
-402.219724	3.486490	7.865037
-400.191431	8.026954	7.875034
-398.207316	5.304631	7.885030
-396.193129	-0.067230	7.895027
-394.071751	6.901670	7.905024
-392.422014	5.326715	7.915021
-390.732359	12.093822	7.925018
-389.055097	4.065428	7.935014
-386.780354	6.963792	7.945011
-385.052528	4.463287	7.955008
-382.964730	4.600346	7.965005
-381.101291	4.536395	7.975002
-379.503230	1.763324	7.984998
-377.603639	5.866244	7.994995
-375.663660	1.929893	8.004992
-373.543884	1.475763	8.014989
-371.594271	3.175893	8.024986
-370.324021	9.485369	8.034982
-368.256437	7.560906	8.044979
-366.192122	3.586235	8.054976
-364.362390	12.625523	8.064973
-362.328660	12.175883	8.074970
-360.581690	11.931941	8.084966
-358.513396	7.830912	8.094963
-356.839050	3.100305	8.104960
-355.146009	1.435334	8.114957
-352.985382	8.930275	8.124954
-350.968005	-0.142907	8.134950
-349.571947	2.226834	8.144947
-347.710194	0.792186	8.154944
-345.523867	5.498432	8.164941
-343.796292	4.014479	8.174938
-342.141189	2.253265	8.184934
-339.822603	2.414780	8.194931
-337.957862	3.975746	8.204928
-336.094199	2.720203	8.214925
-334.417229	2.830930	8.224922
-332.385139	8.931086	8.234918
-330.418626	4.148393	8.244915
-328.651141	-2.832724	8.254912
-326.845896	-0.092898	8.264909
-325.111300	-2.483485	8.274906
-323.293641	5.833462	8.284902
-321.522524	6.105496	8.294899
-319.331750	-0.695292	8.304896
-317.571278	2.003608	8.314893
-315.399825	3.903631	8.324890
-313.435646	0.873729	8.334886
-311.572616	2.265058	8.344883
-310.345501	0.658289	8.354880
-308.068486	7.316380	8.364877
-306.224141	5.091538	8.374874
-304.454196	6.129312	8.384870
-302.121831	6.684093	8.394867
-300.665452	0.070544	8.404864
-298.854801	2.273149	8.414861
-296.530569	-0.742229	8.424858
-295.033910	0.204890	8.434854
-293.165830	-3.828964	8.444851
-291.003137	-3.711427	8.454848
-289.049788	-0.632205	8.464845
-287.339484	3.787779	8.474842
-286.125685	-0.433813	8.484838
-283.457856	-2.019347	8.494835
-282.007568	0.837110	8.504832
-279.905283	1.437296	8.514829
-277.938804	7.070128	8.524826
-275.971214	7.691048	8.534822
-273.995464	1.908085	8.544819
-272.776065	-2.808483	8.554816
-270.281457	-1.165822	8.564813
-268.722813	0.041396	8.574810
-266.985660	6.043178	8.584807
-265.219162	8.598000	8.594803
-262.806310	-0.218908	8.604800
-261.083427	3.956268	8.614797
-259.390035	5.284236	8.624794
-257.798255	3.512967	8.634791
-255.224212	3.946091	8.644787
-253.337759	3.159744	8.654784
-252.191048	3.915150	8.664781
-249.737803	10.878192	8.674778
-247.928358	0.677987	8.684775
-245.981711	-1.193271	8.694771
-244.232683	2.379467	8.704768
-242.453667	0.417212	8.714765
-240.880596	0.809404	8.724762
-238.728747	2.187586	8.734759
-236.782974	-0.601998	8.744755
-234.725595	-3.343932	8.754752
-232.988448	-3.854886	8.764749
-231.387631	0.272471	8.774746
-229.208350	-0.332889	8.784743
-227.156879	-9.040369	8.794739
-225.564636	-7.854707	8.804736
-223.588754	-1.743277	8.814733
-221.725117	-2.185022	8.824730
-219.990931	-4.735563	8.834727
-217.810174	-3.995464	8.844723
-216.236507	1.603595	8.854720
-214.304411	-4.740967	8.864717
-211.977142	-11.413353	8.874714
-210.321282	-8.699234	8.884711
-208.707180	-4.355989	8.894707
-206.887813	-6.990298	8.904704
-204.756362	-7.211989	8.914701
-202.949330	-9.193656	8.924698
-201.102287	-13.944737	8.934695
-199.153378	-12.828932	8.944691
-197.473747	-14.546084	8.954688
-195.288807	-6.573466	8.964685
-193.631764	-4.125127	8.974682
-191.751376	-5.582669	8.984679
-189.855429	-12.322952	8.994675
-188.165667	-6.827187	9.004672
-185.788235	-6.787531	9.014669
-184.351225	-1.295444	9.024666
-182.635885	-1.310595	9.034663
-180.669824	-5.676593	9.044659
-178.702690	-7.631565	9.054656
-176.654565	-5.865642	9.064653
-174.659901	-6.528632	9.074650
-172.917111	-3.129085	9.084647
-171.171755	-4.873705	9.094643
-169.212120	-6.033794	9.104640
-167.437156	-3.396600	9.114637
-165.695099	-9.830671	9.124634
-163.501945	-10.481062	9.134631
-161.213988	-11.819182	9.144627
-159.672477	-2.849725	9.154624
-158.302925	-4.885188	9.164621
-156.500376	-3.496857	9.174618
-154.312038	-6.925968	9.184615
-152.213026	-3.470520	9.194611
-150.269204	-0.212148	9.204608
-148.657713	-2.429006	9.214605
-147.085117	0.632190	9.224602
-144.782104	0.047938	9.234599
-142.768206	-5.798822	9.244595
-141.030334	-4.070969	9.254592
-139.053949	-4.769145	9.264589
-137.150656	-0.766739	9.274586
-135.697937	-9.001580	9.284583
-133.703877	0.146775	9.294579
-131.747452	-5.916978	9.304576
-129.718711	-9.183939	9.314573
-128.029297	0.144714	9.324570
-126.211061	-0.759907	9.334567
-124.222414	-2.792847	9.344563
-122.254579	-9.314236	9.354560
-120.245895	-0.130045	9.364557
-118.254696	-2.560612	9.374554
-116.676265	-1.185208	9.384551
-114.919493	-3.333699	9.394547
-113.125586	-9.313849	9.404544
-111.099756	0.016008	9.414541
-108.911325	-2.036564	9.424538
-107.264621	4.523827	9.434535
-105.408908	2.301856	9.444531
-103.529423	-2.251221	9.454528
-101.790622	-0.044510	9.464525
-99.984049	1.917007	9.474522
-98.109706	-1.486689	9.484519
-95.763325	-1.391073	9.494515
-94.178821	-3.455080	9.504512
-92.546402	0.762555	9.514509
-90.347801	1.290193	9.524506
-88.387102	4.405400	9.534503
-86.750453	6.303583	9.544499
-84.934208	2.506733	9.554496
-82.798010	11.337103	9.564493
-81.095151	2.920257	9.574490
-79.482626	4.930078	9.584487
-77.318459	3.063086	9.594483
-75.095923	-0.158834	9.604480
-73.570997	4.339666	9.614477
-71.945303	2.210901	9.624474
-69.886468	4.429933	9.634471
-67.951034	-1.750740	9.644467
-66.188548	1.183469	9.654464
-64.091014	5.949753	9.664461
-62.249319	9.321719	9.674458
-60.293641	8.186856	9.684455
-58.608093	5.816235	9.694451
-56.669028	6.510516	9.704448
-54.453635	1.207832	9.714445
-53.009815	3.345395	9.724442
-51.037021	1.125501	9.734439
-49.127874	5.434819	9.744435
-47.340759	5.653631	9.754432
-45.217994	3.642385	9.764429
-43.761599	0.631687	9.774426
-41.741316	3.735512	9.784423
-39.735820	2.185043	9.794419
-37.769740	2.993660	9.804416
-35.791042	0.269649	9.814413
-34.113089	0.309576	9.824410
-32.352279	0.537647	9.834407
-30.614707	2.171140	9.844403
-28.437102	-0.204801	9.854400
-26.592967	0.208963	9.864397
-24.708353	6.344446	9.874394
-22.957336	0.069732	9.884391
-20.737407	0.097356	9.894387
-19.040197	3.734406	9.904384
-17.454611	5.429534	9.914381
-15.759405	5.257441	9.924378
-13.708313	0.663904	9.934375
-11.476514	-3.963778	9.944371
-9.691430	-1.358683	9.954368
-7.657115	0.496240	9.964365
-5.864161	-4.593290	9.974362
-4.310408	8.635759	9.984359
-3.542558	39.272137	9.994355
-2.106422	95.393857	10.004352
-1.093962	164.675748	10.014349
0.000000	235.339515	10.019354
0.928937	274.511053	10.024359
1.862902	316.323287	10.029363
2.111821	343.658729	10.034368
2.751893	372.225780	10.039373
3.132517	396.532149	10.044378
3.045938	413.591057	10.049383
3.456241	431.850000	10.054387
3.505075	449.708725	10.059392
3.968468	452.877447	10.064397
4.107734	471.459610	10.069402
3.943604	475.164209	10.074407
4.085301	484.458146	10.079411
3.639145	491.680722	10.084416
3.848910	500.024740	10.089421
3.729657	515.496258	10.094426
4.059735	511.324280	10.099431
4.221322	526.677394	10.104435
4.175753	544.224003	10.109440
4.515105	554.030389	10.114445
4.363132	558.694473	10.119450
4.429868	555.996541	10.124455
4.947346	558.906940	10.129459
4.917065	568.504354	10.134464
4.774084	560.665956	10.139469
5.072846	571.430600	10.144474
5.057652	570.181935	10.149479
4.794466	579.822843	10.154483
4.811965	578.689752	10.159488
5.209698	574.679047	10.164493
5.273356	579.207877	10.169498
4.985754	578.111311	10.174503
5.524686	589.200698	10.179507
5.256205	589.404237	10.184512
5.300160	579.098318	10.189517
5.182766	594.476441	10.194522
5.572183	607.870624	10.199527
5.674646	611.583622	10.204531
5.650758	611.816273	10.209536
5.577912	597.174171	10.214541
5.019207	601.940375	10.219546
5.336620	618.402093	10.224551
5.761285	628.203372	10.229555
5.856492	620.168185	10.234560
5.785978	626.337229	10.239565
5.676067	639.185099	10.244570
5.897960	628.197734	10.249575
5.774546	631.713419	10.254579
6.095385	636.579475	10.259584
6.270323	637.153025	10.264589
5.714619	642.333585	10.269594
5.560644	639.780059	10.274599
5.700705	641.623505	10.279603
5.702996	647.357321	10.284608
6.172383	656.510308	10.289613
6.164077	681.503136	10.294618
6.417160	677.874830	10.299623
6.280994	688.058882	10.304627
5.773968	688.835812	10.309632
6.329648	684.805102	10.314637
6.160261	696.791262	10.319642
5.922013	680.175381	10.324647
6.318321	691.621262	10.329651
6.591931	711.029341	10.334656
6.943611	719.622296	10.339661
6.636659	729.741318	10.344666
6.984808	731.991587	10.349671
6.730525	711.480076	10.354675
6.941407	722.942379	10.359680
6.673399	710.574117	10.364685
6.856490	727.625813	10.369690
6.934605	731.073413	10.374695
7.238250	730.281240	10.379699
6.718015	740.978014	10.384704
7.209900	741.193281	10.389709
6.966920	736.549513	10.394714
7.118855	737.541872	10.399719
7.208581	742.777583	10.404723
7.148856	739.005928	10.409728
7.205172	744.248947	10.414733
7.050786	750.324265	10.419738
6.992814	743.416181	10.424743
7.127117	737.489587	10.429747
7.020906	748.414185	10.434752
7.780879	762.237587	10.439757
7.647918	779.895759	10.444762
7.806968	779.718894	10.449767
7.841580	777.644185	10.454771
7.746019	782.042087	10.459776
7.752253	759.057462	10.464781
7.574588	770.771551	10.469786
8.161436	783.271521	10.474791
7.631278	778.566457	10.479795
7.739718	781.875055	10.484800
7.860314	783.743961	10.489805
7.983453	794.091643	10.494810
8.087239	786.193451	10.499815
8.014891	787.131903	10.504819
7.721839	791.403015	10.509824
8.101114	797.591318	10.514829
7.723601	802.659272	10.519834
7.832256	795.550887	10.524839
8.230465	814.535105	10.529843
8.020680	823.019917	10.534848
8.156267	823.317989	10.539853
8.254299	833.906841	10.544858
7.959180	831.860242	10.549863
8.311070	838.056809	10.554867
8.350601	841.183423	10.559872
8.642129	833.447224	10.564877
8.349408	838.976697	10.569882
8.465123	858.012169	10.574887
8.960619	856.927361	10.579891
8.744154	871.529330	10.584896
8.801480	862.268554	10.589901
8.632408	871.373247	10.594906
8.875045	860.834131	10.599911
8.894849	875.270067	10.604915
8.664706	879.843045	10.609920
8.836955	877.128545	10.614925
8.860258	880.977942	10.619930
8.789310	882.357865	10.624935
8.599904	883.510208	10.629939
8.672973	890.119338	10.634944
9.203927	903.223457	10.639949
9.124112	905.225030	10.644954
9.236821	905.589788	10.649959
9.535007	910.512709	10.654963
8.801221	908.244475	10.659968
9.683499	907.831891	10.664973
9.197127	914.620638	10.669978
9.220608	919.480532	10.674983
9.217087	930.017389	10.679987
9.290464	934.557288	10.684992
9.599286	936.499727	10.689997
9.782113	945.788860	10.695002
10.022096	941.515771	10.700007
9.812416	940.870025	10.705011
9.789470	946.080518	10.710016
10.289597	943.110841	10.715021
9.810182	944.960674	10.720026
9.661270	946.743574	10.725031
9.647574	951.552222	10.730035
10.121816	960.733371	10.735040
10.498301	958.824624	10.740045
9.943034	957.554057	10.745050
10.033874	963.827015	10.750055
10.321067	966.988951	10.755059
10.413532	984.253439	10.760064
10.748072	972.378494	10.765069
10.281141	965.402276	10.770074
10.338481	976.303727	10.775079
10.659819	974.020751	10.780083
10.636368	987.844474	10.785088
10.607668	991.522025	10.790093
10.659838	995.360185	10.795098
10.679896	991.313869	10.800103
10.833741	981.888841	10.805107
10.439236	992.030938	10.810112
11.081230	991.308238	10.815117
11.006548	997.063670	10.820122
10.974409	988.172632	10.825127
10.917556	991.260144	10.830131
10.825365	995.033451	10.835136
10.957821	988.865500	10.840141
10.615364	996.548156	10.845146
10.579804	1001.490831	10.850151
10.924609	993.444630	10.855155
10.658977	1002.130956	10.860160
11.309971	1017.243533	10.865165
11.466721	1028.405870	10.870170
11.545069	1024.135209	10.875175
11.636398	1019.737982	10.880179
11.244688	1015.390815	10.885184
11.215569	1009.613323	10.890189
11.491827	1033.510292	10.895194
11.979317	1034.158557	10.900199
12.135130	1027.200665	10.905203
11.646071	1008.097571	10.910208
11.840762	1008.062223	10.915213
11.487748	1006.111580	10.920218
11.754371	1001.361406	10.925223
12.035168	1011.175359	10.930227
11.425441	1013.448594	10.935232
11.499618	1021.744299	10.940237
11.575705	1038.037839	10.945242
12.033215	1039.582166	10.950247
12.380296	1030.174897	10.955251
12.176310	1041.398306	10.960256
12.411853	1036.490426	10.965261
12.625821	1042.007697	10.970266
12.651886	1039.429945	10.975271
12.174658	1030.588752	10.980275
12.149361	1038.080073	10.985280
12.472274	1036.618661	10.990285
12.370451	1043.132711	10.995290
12.554394	1041.445653	11.000295
12.696189	1041.150954	11.005299
12.525910	1039.905158	11.010304
12.222198	1036.290530	11.015309
12.152223	1044.522936	11.020314
12.249858	1036.816725	11.025319
12.534826	1038.871426	11.030323
12.274716	1051.039992	11.035328
12.365111	1045.174890	11.040333
12.751773	1068.697324	11.045338
13.039894	1077.667297	11.050343
13.001197	1075.828541	11.055347
13.172435	1080.898809	11.060352
13.121753	1075.917624	11.065357
12.871846	1075.029296	11.070362
12.688540	1068.053348	11.075367
13.010716	1071.874835	11.080371
12.964366	1071.540553	11.085376
13.301897	1076.604807	11.090381
13.284125	1073.175222	11.095386
13.145798	1082.620161	11.100391
13.084857	1072.198877	11.105395
13.055770	1077.103360	11.110400
12.935828	1079.514863	11.115405
12.919143	1092.536594	11.120410
13.430410	1101.214108	11.125415
13.923450	1101.311159	11.130419
13.829516	1110.926925	11.135424
14.151443	1100.072473	11.140429
14.220767	1099.865989	11.145434
13.820135	1082.439886	11.150439
14.223664	1068.397770	11.155443
13.956502	1072.347149	11.160448
14.166600	1067.234016	11.165453
14.132115	1069.904812	11.170458
14.130509	1071.452073	11.175463
14.134767	1063.474886	11.180467
14.212830	1069.568892	11.185472
14.410260	1063.147008	11.190477
14.151188	1075.181204	11.195482
13.882233	1070.794816	11.200487
13.952430	1075.031352	11.205491
13.621613	1078.684147	11.210496
13.759622	1069.553098	11.215501
14.327452	1101.290200	11.220506
14.591178	1101.737623	11.225511
14.704490	1106.961517	11.230515
14.501404	1107.527271	11.235520
14.538963	1100.989887	11.240525
14.646983	1100.936638	11.245530
14.238422	1107.056464	11.250535
14.303457	1111.105605	11.255539
14.512227	1116.333267	11.260544
14.580274	1109.572756	11.265549
14.769476	1103.124240	11.270554
14.688081	1103.831366	11.275559
14.757724	1105.704311	11.280563
14.554072	1105.685553	11.285568
14.999438	1118.115316	11.290573
15.094075	1129.049953	11.295578
15.089724	1140.043413	11.300583
15.612962	1141.484111	11.305587
15.244714	1130.406527	11.310592
15.160573	1114.932187	11.315597
14.705054	1118.516372	11.320602
15.108250	1124.364387	11.325607
15.182172	1128.243850	11.330611
15.274255	1142.728036	11.335616
15.275930	1134.178882	11.340621
15.288370	1141.193253	11.345626
15.474729	1139.214453	11.350631
15.422246	1131.194064	11.355635
15.212611	1131.430545	11.360640
15.277223	1138.682681	11.365645
15.644934	1144.638631	11.370650
15.984224	1160.019532	11.375655
15.862138	1152.382912	11.380659
15.678565	1154.936390	11.385664
15.858983	1158.434440	11.390669
16.393111	1170.288889	11.395674
16.088463	1153.025856	11.400679
16.219038	1140.744437	11.405683
16.320895	1136.896034	11.410688
16.394197	1134.187798	11.415693
16.210671	1132.024523	11.420698
16.205512	1135.752151	11.425703
16.440769	1133.047331	11.430707
16.074104	1141.673293	11.435712
16.333743	1138.224944	11.440717
16.400462	1140.524713	11.445722
16.027876	1136.018311	11.450727
15.969928	1137.398396	11.455731
16.219234	1146.403091	11.460736
16.638526	1155.577989	11.465741
16.748476	1169.582291	11.470746
16.714703	1174.216421	11.475751
16.815933	1163.791744	11.480755
16.676969	1176.439771	11.485760
16.811355	1171.999986	11.490765
16.722671	1168.693461	11.495770
16.845492	1169.763472	11.500775
17.103948	1156.256551	11.505779
17.120202	1163.579360	11.510784
16.955830	1154.498135	11.515789
17.010009	1144.564304	11.520794
16.678113	1160.894374	11.525799
17.367886	1166.781691	11.530803
17.325949	1173.054999	11.535808
17.251792	1174.486419	11.540813
17.511908	1178.487524	11.545818
16.817930	1165.026268	11.550823
17.353875	1163.079104	11.555827
17.196284	1166.788665	11.560832
17.289419	1163.342806	11.565837
17.434980	1178.492862	11.570842
16.873834	1180.650026	11.575847
17.500783	1174.888273	11.580851
16.883935	1175.428657	11.585856
17.059645	1170.364807	11.590861
17.248957	1186.660011	11.595866
17.524414	1192.564692	11.600871
17.913626	1192.700073	11.605875
18.116319	1187.601197	11.610880
18.250463	1184.810283	11.615885
18.488155	1186.268762	11.620890
18.357525	1173.473545	11.625895
18.734005	1158.784269	11.630899
18.241496	1156.731996	11.635904
17.839472	1162.544010	11.640909
17.956174	1160.392412	11.645914
17.851231	1150.644546	11.650919
18.031928	1154.524656	11.655923
17.551039	1157.133454	11.660928
18.172751	1164.436530	11.665933
18.421280	1184.073713	11.670938
18.324431	1188.651557	11.675943
18.822267	1181.662979	11.680947
18.386742	1193.541598	11.685952
18.678793	1184.880260	11.690957
18.863269	1198.413515	11.695962
18.011002	1180.182493	11.700967
18.755684	1184.414334	11.705971
18.208176	1197.777040	11.710976
18.541933	1186.631154	11.715981
18.548716	1196.931948	11.720986
18.923674	1196.883061	11.725991
18.988587	1197.756554	11.730995
18.514529	1197.378761	11.736000
18.681910	1188.601032	11.741005
18.761633	1190.259493	11.746010
18.623061	1192.701445	11.751015
19.082522	1211.021955	11.756019
19.045929	1226.496977	11.761024
19.357411	1220.269818	11.766029
18.934658	1214.878694	11.771034
18.449121	1222.282436	11.776039
19.189886	1216.754577	11.781043
19.165766	1217.815050	11.786048
19.598281	1216.898520	11.791053
19.521440	1218.390406	11.796058
19.592822	1224.199431	11.801063
19.584117	1221.605505	11.806067
19.508570	1220.015816	11.811072
19.537751	1214.321016	11.816077
19.680466	1217.928177	11.821082
19.746655	1215.426412	11.826087
19.843896	1212.969456	11.831091
20.140487	1218.415386	11.836096
20.238728	1224.054804	11.841101
20.246384	1225.666020	11.846106
20.301629	1217.801196	11.851111
20.144364	1215.727355	11.856115
19.804613	1209.030802	11.861120
20.161085	1212.007619	11.866125
19.901526	1218.038782	11.871130
20.080736	1216.806864	11.876135
20.318812	1218.648575	11.881139
19.883435	1214.761212	11.886144
20.018668	1218.332156	11.891149
20.168789	1224.653476	11.896154
20.198792	1227.804695	11.901159
20.112285	1218.954821	11.906163
20.149930	1223.500931	11.911168
20.235016	1219.118534	11.916173
20.028496	1226.960365	11.921178
20.432063	1245.559319	11.926183
20.662105	1243.876177	11.931187
20.509441	1246.042654	11.936192
20.876855	1251.343425	11.941197
20.915801	1259.846221	11.946202
20.963961	1253.586828	11.951207
21.310892	1239.628870	11.956211
20.714967	1233.913347	11.961216
20.614927	1222.500758	11.966221
21.231969	1236.896996	11.971226
21.294755	1236.187941	11.976231
20.953864	1224.007821	11.981235
20.707003	1229.218511	11.986240
20.956205	1239.031709	11.991245
21.016737	1243.501268	11.996250
20.979935	1243.114423	12.001255
21.282551	1243.758475	12.006259
21.074107	1246.825055	12.011264
21.276261	1247.033169	12.016269
21.147253	1248.755847	12.021274
21.172294	1246.129684	12.026279
21.267308	1244.967069	12.031283
21.197077	1251.659740	12.036288
21.610311	1250.810857	12.041293
21.303335	1253.397352	12.046298
21.407828	1256.773440	12.051303
21.563453	1242.583803	12.056307
21.265414	1248.609338	12.061312
21.422131	1250.706190	12.066317
21.332039	1248.246611	12.071322
21.209548	1255.313380	12.076327
21.695251	1247.338024	12.081331
21.118411	1244.742427	12.086336
21.368476	1245.560097	12.091341
21.440198	1245.888865	12.096346
21.369042	1253.503418	12.101351
21.650355	1251.027527	12.106355
21.242418	1253.291064	12.111360
21.595973	1246.276275	12.116365
21.870691	1253.312438	12.121370
21.987517	1253.539129	12.126375
22.249693	1255.551978	12.131379
21.948107	1237.475550	12.136384
22.071272	1223.453340	12.141389
21.819504	1225.685360	12.146394
21.597096	1225.400604	12.151399
21.592586	1220.295796	12.156403
21.688588	1220.999353	12.161408
21.927077	1211.967442	12.166413
21.785467	1194.819697	12.171418
21.502486	1195.330073	12.176423
21.595232	1186.870671	12.181427
21.186292	1189.213715	12.186432
21.094070	1184.535278	12.191437
20.868764	1198.414719	12.196442
21.371166	1192.847606	12.201447
21.310517	1186.464395	12.206451
21.132417	1196.414386	12.211456
21.505298	1206.729784	12.216461
21.213207	1205.665126	12.221466
21.364707	1214.223994	12.226471
21.692825	1217.398703	12.231475
21.212360	1210.219033	12.236480
21.339301	1205.050243	12.241485
21.607629	1211.355238	12.246490
21.390149	1205.366809	12.251495
21.463205	1191.820592	12.256499
21.164461	1197.473199	12.261504
21.449836	1195.890313	12.266509
21.286837	1194.652730	12.271514
21.595986	1207.985799	12.276519
21.543923	1201.727822	12.281523
21.132009	1199.927385	12.286528
21.391095	1194.125672	12.291533
21.331106	1199.877080	12.296538
21.215303	1198.410744	12.301543
21.822457	1203.763551	12.306547
21.247250	1206.220764	12.311552
21.319949	1202.987614	12.316557
21.284474	1204.913332	12.321562
21.248988	1212.142797	12.326567
21.445921	1206.166997	12.331571
21.369604	1225.284792	12.336576
21.753152	1217.675524	12.341581
21.878076	1209.958627	12.346586
21.398962	1205.055597	12.351591
21.662302	1207.546271	12.356595
21.554159	1212.575274	12.361600
21.555174	1207.747816	12.366605
21.686512	1202.486299	12.371610
21.729245	1208.134439	12.376615
21.470018	1211.257088	12.381619
21.243262	1212.593886	12.386624
21.294029	1215.039298	12.391629
21.795957	1207.150787	12.396634
21.284590	1215.556861	12.401639
21.710992	1206.609182	12.406643
21.247063	1203.689097	12.411648
21.352629	1199.351747	12.416653
21.553778	1207.809729	12.421658
21.478119	1194.855857	12.426663
21.451546	1188.580488	12.431667
21.679506	1192.297371	12.436672
21.349393	1179.963856	12.441677
21.377229	1188.641810	12.446682
21.109092	1181.396931	12.451687
21.616370	1178.695594	12.456691
21.545627	1186.164384	12.461696
21.218939	1182.418659	12.466701
21.381438	1185.845182	12.471706
21.000276	1186.306075	12.476711
21.440881	1176.342283	12.481715
21.498190	1178.486564	12.486720
21.301074	1178.323395	12.491725
21.168612	1179.674813	12.496730
20.970152	1198.368645	12.501735
21.142208	1200.769574	12.506739
20.901588	1210.299630	12.511744
21.239330	1215.549028	12.516749
21.676828	1208.851840	12.521754
21.721132	1217.084481	12.526759
21.720180	1213.476715	12.531763
21.332660	1212.358154	12.536768
21.602552	1207.003010	12.541773
21.676315	1212.408986	12.546778
21.079883	1197.529249	12.551783
21.392988	1200.863241	12.556787
20.836338	1214.930168	12.561792
21.076046	1209.656383	12.566797
21.107116	1217.598395	12.571802
20.829570	1216.601900	12.576807
21.008321	1213.664383	12.581811
21.071929	1215.234425	12.586816
20.918086	1220.629298	12.591821
21.417033	1244.966442	12.596826
21.274535	1250.790043	12.601831
21.441013	1253.314307	12.606835
21.411330	1260.881093	12.611840
21.558796	1251.846608	12.616845
21.775944	1244.392965	12.621850
21.381841	1236.429122	12.626855
21.229723	1230.398687	12.631859
21.197652	1234.216612	12.636864
21.291545	1240.837320	12.641869
21.414313	1254.006200	12.646874
21.198210	1259.707028	12.651879
21.351768	1258.099368	12.656883
21.135930	1253.787901	12.661888
21.662868	1243.724394	12.666893
21.854753	1249.881851	12.671898
21.339322	1245.063194	12.676903
21.541727	1230.795676	12.681907
21.378210	1232.584271	12.686912
21.417300	1231.098084	12.691917
21.519257	1217.332940	12.696922
21.618679	1225.508370	12.701927
21.551761	1223.498380	12.706931
21.436621	1230.478219	12.711936
21.504641	1221.999747	12.716941
21.413183	1226.576284	12.721946
21.567579	1231.389355	12.726951
21.913857	1220.342747	12.731955
21.819157	1227.908429	12.736960
21.711519	1232.012472	12.741965
21.746609	1227.135349	12.746970
21.300365	1210.873515	12.751975
21.648874	1205.896869	12.756979
21.404638	1202.965564	12.761984
21.130714	1192.956510	12.766989
21.559906	1199.643659	12.771994
21.559334	1206.833188	12.776999
21.937604	1202.417105	12.782003
21.182244	1203.602166	12.787008
21.320301	1201.294531	12.792013
21.832675	1201.284451	12.797018
21.579657	1206.691981	12.802023
21.692011	1197.035514	12.807027
21.467355	1200.958689	12.812032
20.838938	1197.380749	12.817037
21.069302	1202.099864	12.822042
21.128228	1204.195318	12.827047
21.079086	1198.477637	12.832051
21.154708	1200.266673	12.837056
21.073138	1212.446594	12.842061
21.340480	1213.678148	12.847066
21.373783	1227.206559	12.852071
21.634251	1218.511142	12.857075
21.271778	1214.040878	12.862080
21.273027	1202.293170	12.867085
21.657847	1204.288930	12.872090
21.240974	1216.088973	12.877095
21.353044	1201.416572	12.882099
21.276879	1211.174618	12.887104
21.383048	1204.803061	12.892109
21.414961	1215.791145	12.897114
21.332149	1217.038920	12.902119
21.629483	1211.592621	12.907123
21.191817	1216.934313	12.912128
21.379155	1216.043638	12.917133
21.577135	1206.077612	12.922138
20.963458	1214.925574	12.927143
21.424172	1220.304680	12.932147
21.494972	1238.849366	12.937152
21.335169	1240.778247	12.942157
21.203342	1239.404656	12.947162
21.169662	1237.970815	12.952167
21.728615	1226.012594	12.957171
21.437758	1240.538057	12.962176
21.578679	1240.298374	12.967181
21.474096	1218.147610	12.972186
21.432741	1218.732611	12.977191
21.539770	1210.737332	12.982195
21.372223	1217.992996	12.987200
21.333353	1217.374398	12.992205
21.434842	1212.487474	12.997210
21.441920	1205.361977	13.002215
21.847452	1202.567948	13.007219
21.155192	1211.304250	13.012224
21.004689	1209.234776	13.017229
21.339246	1208.258069	13.022234
21.007320	1214.049398	13.027239
21.103389	1220.096560	13.032243
21.225750	1235.804078	13.037248
21.488262	1238.907933	13.042253
21.753759	1242.774709	13.047258
21.400253	1242.818751	13.052263
21.562054	1223.436423	13.057267
21.182722	1222.566329	13.062272
21.248102	1222.252755	13.067277
21.605250	1224.370501	13.072282
21.530531	1237.222697	13.077287
21.339071	1212.471671	13.082291
21.274919	1219.406051	13.087296
21.554398	1221.308953	13.092301
21.472255	1215.136261	13.097306
21.423334	1214.048066	13.102311
21.590403	1207.027374	13.107315
21.772902	1220.197431	13.112320
21.192059	1221.103883	13.117325
21.544561	1220.488444	13.122330
21.062955	1224.648711	13.127335
21.666261	1215.327270	13.132339
21.236837	1224.519440	13.137344
21.675504	1220.695767	13.142349
21.125137	1223.479911	13.147354
21.049430	1226.937417	13.152359
21.494231	1215.741682	13.157363
21.219016	1217.140079	13.162368
21.076860	1215.077069	13.167373
21.399786	1213.782220	13.172378
21.169226	1228.892998	13.177383
21.687585	1232.629177	13.182387
21.383322	1225.979822	13.187392
21.719188	1231.829555	13.192397
21.770397	1223.034224	13.197402
21.596980	1224.926359	13.202407
22.023843	1219.606665	13.207411
21.539440	1219.674335	13.212416
21.416716	1223.890306	13.217421
21.566978	1223.111383	13.222426
21.354951	1236.411468	13.227431
21.617085	1226.792855	13.232435
21.438151	1227.594079	13.237440
21.600148	1220.410433	13.242445
21.718102	1203.229623	13.247450
21.515783	1207.587133	13.252455
21.883195	1193.513202	13.257459
21.536814	1194.614323	13.262464
21.468295	1199.834688	13.267469
21.457188	1183.580774	13.272474
20.975834	1185.599125	13.277479
21.682653	1186.668875	13.282483
21.038173	1178.594832	13.287488
21.025283	1193.074959	13.292493
21.078375	1191.997300	13.297498
21.163024	1193.243992	13.302503
21.077860	1197.414832	13.307507
21.049813	1212.753768	13.312512
21.186291	1217.483854	13.317517
21.428756	1221.488786	13.322522
21.567720	1219.087833	13.327527
21.225584	1226.252250	13.332531
21.343351	1228.576833	13.337536
21.197348	1231.383227	13.342541
21.510235	1228.479551	13.347546
21.453713	1233.143258	13.352551
21.480888	1223.600065	13.357555
21.511790	1232.917788	13.362560
21.710447	1242.749129	13.367565
21.787346	1229.949468	13.372570
21.233540	1214.396476	13.377575
21.417026	1199.960518	13.382579
21.289320	1201.312701	13.387584
21.261072	1206.865641	13.392589
21.489401	1220.915219	13.397594
21.219966	1222.365521	13.402599
21.496266	1226.202414	13.407603
21.396381	1229.291430	13.412608
21.073377	1228.452731	13.417613
21.669850	1229.484956	13.422618
21.488997	1225.504607	13.427623
21.213022	1214.438773	13.432627
21.486429	1218.814982	13.437632
21.423430	1217.914334	13.442637
21.481677	1206.943569	13.447642
21.424206	1202.472724	13.452647
21.636348	1196.197870	13.457651
21.659620	1197.534429	13.462656
21.379051	1192.627360	13.467661
21.234717	1190.821307	13.472666
21.064968	1209.261938	13.477671
21.335991	1197.707980	13.482675
21.156430	1197.056269	13.487680
21.005311	1206.332948	13.492685
21.522626	1223.823282	13.497690
21.446560	1232.950133	13.502695
21.815798	1223.476580	13.507699
21.693132	1208.862183	13.512704
21.407782	1205.753188	13.517709
21.417605	1194.949420	13.522714
21.346476	1202.843420	13.527719
21.438874	1196.833837	13.532723
21.370660	1195.023811	13.537728
21.212278	1194.160046	13.542733
21.289213	1198.924414	13.547738
21.393483	1208.084673	13.552743
21.183889	1194.631918	13.557747
21.542603	1203.346306	13.562752
21.361481	1214.190520	13.567757
22.005690	1201.523349	13.572762
21.425172	1208.021650	13.577767
21.375051	1206.190758	13.582771
21.256592	1202.341034	13.587776
21.521153	1203.622011	13.592781
21.528634	1201.652952	13.597786
21.348767	1208.353744	13.602791
21.476181	1208.395065	13.607795
21.397186	1201.136694	13.612800
21.308208	1209.484158	13.617805
21.570904	1206.221588	13.622810
21.224592	1202.415274	13.627815
21.431734	1201.311596	13.632819
21.420251	1206.292445	13.637824
21.308650	1202.464440	13.642829
21.285227	1203.589925	13.647834
21.341997	1210.075668	13.652839
21.350790	1206.278336	13.657843
21.437421	1206.923893	13.662848
21.375716	1215.276157	13.667853
21.738673	1203.144320	13.672858
21.592134	1211.888107	13.677863
21.543524	1209.208656	13.682867
21.470529	1214.642954	13.687872
21.275851	1213.350010	13.692877
21.767283	1211.912189	13.697882
21.331683	1217.647479	13.702887
21.414802	1211.600007	13.707891
21.462900	1213.924691	13.712896
21.508017	1210.674557	13.717901
21.693519	1209.363008	13.722906
21.298277	1203.124792	13.727911
21.739863	1192.957136	13.732915
21.731615	1188.710357	13.737920
21.526105	1186.849267	13.742925
21.538326	1175.456938	13.747930
21.417773	1187.274047	13.752935
21.090859	1186.753787	13.757939
21.422900	1181.579050	13.762944
21.351725	1183.936022	13.767949
21.196577	1174.008063	13.772954
21.441144	1177.550382	13.777959
21.572724	1179.770746	13.782963
21.794343	1187.488227	13.787968
21.607750	1182.914393	13.792973
21.535735	1175.651680	13.797978
21.495047	1175.545769	13.802983
21.418112	1175.418047	13.807987
21.548990	1175.978252	13.812992
21.349698	1176.549673	13.817997
21.557709	1180.538001	13.823002
21.238506	1185.793845	13.828007
21.215132	1178.035680	13.833011
21.333445	1176.488546	13.838016
21.047076	1180.691511	13.843021
21.593572	1185.684051	13.848026
21.194521	1191.785306	13.853031
21.233709	1179.578342	13.858035
21.648845	1181.293767	13.863040
21.286612	1183.187481	13.868045
21.337575	1180.530831	13.873050
21.327746	1190.854207	13.878055
21.109562	1176.160691	13.883059
21.205949	1179.484073	13.888064
21.156487	1181.780084	13.893069
21.242805	1180.016197	13.898074
21.179599	1187.277246	13.903079
21.352775	1181.416056	13.908083
21.725544	1183.410722	13.913088
21.420410	1171.833992	13.918093
21.416662	1181.111835	13.923098
21.299716	1183.942055	13.928103
21.471728	1177.280137	13.933107
21.709546	1181.917835	13.938112
21.339852	1182.942425	13.943117
21.310029	1174.064305	13.948122
21.422798	1188.606567	13.953127
21.526231	1187.821464	13.958131
21.300577	1182.524848	13.963136
21.297288	1189.825362	13.968141
21.218795	1185.489969	13.973146
21.039093	1189.538067	13.978151
21.442685	1190.643624	13.983155
21.192736	1183.874052	13.988160
20.882850	1188.628162	13.993165
21.192875	1193.584670	13.998170
21.150441	1215.986416	14.003175
21.811088	1210.768747	14.008179
21.954853	1219.195522	14.013184
21.820447	1204.909593	14.018189
21.765700	1188.665578	14.023207
21.316473	1202.657173	14.028224
21.697853	1193.195719	14.033242
21.608847	1187.048266	14.038259
21.395010	1188.219680	14.043277
21.419871	1188.972182	14.048295
21.423082	1194.248462	14.053312
21.496916	1188.862918	14.058330
21.194325	1191.418563	14.063347
21.370713	1191.220204	14.068365
21.667066	1187.402941	14.073383
21.161111	1188.446080	14.078400
21.343773	1186.730770	14.083418
21.432448	1188.096005	14.088435
21.207813	1197.479805	14.093453
21.455857	1208.221271	14.098471
21.430512	1215.063611	14.103488
21.833964	1216.097294	14.108506
21.584156	1217.126834	14.113523
21.592440	1215.834760	14.118541
21.468697	1216.146956	14.123559
21.467563	1225.129427	14.128576
21.824597	1215.169729	14.133594
22.002737	1218.708398	14.138611
22.059797	1224.040028	14.143629
21.851649	1217.866923	14.148647
21.888956	1226.924702	14.153664
22.143197	1234.029376	14.158682
21.923325	1228.844584	14.163699
21.657508	1230.483221	14.168717
22.131980	1231.760262	14.173735
21.810656	1232.020107	14.178752
22.052881	1225.856006	14.183770
22.074949	1230.681782	14.188787
21.686743	1239.770398	14.193805
22.049232	1229.216003	14.198823
22.000433	1227.976239	14.203840
21.877893	1237.009064	14.208858
21.891852	1228.237808	14.213875
21.778416	1225.075495	14.218893
21.766981	1229.375080	14.223911
21.719719	1232.996498	14.228928
21.608122	1249.415105	14.233946
22.237210	1253.368631	14.238963
22.375801	1261.388107	14.243981
22.120993	1257.210566	14.248999
21.950661	1271.391037	14.254016
22.244229	1263.327792	14.259034
22.349971	1266.636737	14.264051
22.413965	1273.444885	14.269069
22.391078	1271.289570	14.274087
22.174397	1270.217577	14.279104
22.355075	1266.715431	14.284122
22.359358	1260.461394	14.289139
21.719473	1261.194007	14.294157
21.841027	1256.521975	14.299175
22.020709	1262.517299	14.304192
22.773230	1264.311679	14.309210
22.794627	1261.685739	14.314227
22.588989	1263.692048	14.319245
22.330792	1248.511754	14.324263
22.578659	1263.517442	14.329280
22.720835	1256.680659	14.334298
22.914719	1256.017053	14.339315
22.797054	1263.415449	14.344333
22.657467	1254.498443	14.349351
22.661667	1267.383913	14.354368
22.692207	1261.769525	14.359386
23.136689	1261.036178	14.364403
22.743110	1272.989373	14.369421
22.879018	1261.109905	14.374439
22.406870	1239.365327	14.379456
22.229627	1246.760937	14.384474
22.709013	1250.339701	14.389491
22.499743	1257.689622	14.394509
22.557043	1266.971575	14.399527
22.136458	1263.126026	14.404544
22.105397	1256.419743	14.409562
22.332320	1263.375951	14.414579
22.255068	1281.440818	14.419597
22.766679	1288.280108	14.424615
22.904586	1290.308231	14.429632
22.921403	1289.028469	14.434650
22.981397	1281.766750	14.439667
22.895665	1286.796083	14.444685
23.121811	1294.610390	14.449703
23.047281	1290.336568	14.454720
23.289596	1287.552655	14.459738
23.702880	1289.195737	14.464755
23.062068	1279.981944	14.469773
23.255082	1274.247953	14.474791
22.985710	1265.131520	14.479808
23.183582	1268.013215	14.484826
23.220306	1258.781699	14.489843
23.176418	1267.835705	14.494861
23.108673	1259.511549	14.499879
23.105180	1264.241710	14.504896
23.113297	1264.480899	14.509914
23.122640	1254.075629	14.514931
22.922152	1260.580664	14.519949
22.814811	1268.793113	14.524967
23.066263	1279.326938	14.529984
23.097360	1285.011890	14.535002
23.311251	1282.315930	14.540019
23.312144	1291.104375	14.545037
23.192028	1293.268873	14.550055
23.433678	1295.008319	14.555072
23.263352	1303.745018	14.560090
22.996409	1289.991510	14.565107
22.952379	1301.816677	14.570125
23.371405	1296.994801	14.575143
23.492344	1293.895447	14.580160
23.105330	1294.622503	14.585178
23.254809	1291.419428	14.590195
23.371529	1301.422776	14.595213
23.537040	1318.347930	14.600231
23.610473	1317.885306	14.605248
23.870401	1315.258226	14.610266
24.000618	1296.185739	14.615283
23.575275	1297.306804	14.620301
23.791958	1296.452263	14.625319
23.645371	1285.359469	14.630336
23.245954	1290.178785	14.635354
23.487852	1280.360058	14.640371
23.337970	1297.265638	14.645389
23.563604	1309.851735	14.650407
23.944895	1307.722398	14.655424
23.868069	1320.507621	14.660442
24.333226	1309.703264	14.665459
23.846470	1302.415585	14.670477
23.742142	1295.677354	14.675495
24.363382	1284.530475	14.680512
23.491194	1288.758351	14.685530
23.952097	1282.321279	14.690547
23.680656	1279.215577	14.695565
24.042996	1282.793156	14.700583
24.101654	1283.626884	14.705600
23.722532	1288.691167	14.710618
23.877894	1281.687529	14.715635
24.293779	1302.239359	14.720653
24.462985	1302.861596	14.725671
24.176444	1285.724136	14.730688
23.985720	1280.470149	14.735706
24.026180	1291.301994	14.740723
24.022212	1283.648842	14.745741
23.911250	1284.882946	14.750759
23.738828	1284.173869	14.755776
24.512086	1304.569930	14.760794
25.126420	1297.819904	14.765811
24.543525	1294.153371	14.770829
24.484612	1292.738549	14.775847
24.122223	1278.839984	14.780864
23.901225	1288.140137	14.785882
24.189277	1286.201609	14.790899
24.157379	1288.432485	14.795917
23.932824	1275.480062	14.800935
24.172517	1286.577770	14.805952
23.827739	1294.249001	14.810970
24.499054	1303.577679	14.815987
24.399961	1317.186083	14.821005
24.421059	1304.147813	14.826023
24.767571	1315.732391	14.831040
24.333730	1318.701541	14.836058
24.499861	1323.663684	14.841075
24.517441	1314.518889	14.846093
24.398399	1317.610064	14.851111
24.660601	1320.807541	14.856128
24.712519	1320.669895	14.861146
24.898438	1314.342563	14.866163
24.594349	1309.253294	14.871181
24.598534	1319.444862	14.876199
24.788690	1313.569995	14.881216
24.634161	1318.502463	14.886234
24.707301	1319.122667	14.891251
24.795563	1323.515036	14.896269
24.288010	1320.095840	14.901287
24.647535	1316.115732	14.906304
24.260342	1321.584596	14.911322
24.397909	1320.135295	14.916339
24.409464	1319.319468	14.921357
24.654197	1319.267278	14.926375
24.613312	1313.545422	14.931392
24.155723	1322.937740	14.936410
24.867226	1334.968066	14.941427
25.212528	1348.067977	14.946445
25.222721	1347.079531	14.951463
25.413851	1347.718091	14.956480
24.835947	1335.209312	14.961498
25.148669	1329.767010	14.966515
25.148746	1322.056841	14.971533
25.191535	1319.933963	14.976551
25.251140	1306.390617	14.981568
25.171442	1318.094341	14.986586
24.887834	1308.814954	14.991603
24.972688	1311.499086	14.996621
25.262127	1318.806444	15.001639
24.897613	1316.913260	15.006656
24.956169	1340.269968	15.011674
25.295832	1344.816895	15.016691
25.526074	1339.880116	15.021709
25.100251	1343.321562	15.026727
25.458462	1339.738562	15.031744
25.714386	1346.219318	15.036762
25.345170	1335.948986	15.041779
25.707506	1321.323310	15.046797
25.471180	1316.937052	15.051815
25.298785	1300.525348	15.056832
25.377158	1312.870531	15.061850
25.543239	1306.725360	15.066867
25.382999	1301.935080	15.071885
25.340252	1314.212834	15.076903
25.721142	1321.964399	15.081920
25.404797	1329.529974	15.086938
25.710003	1328.607099	15.091955
25.425159	1325.033957	15.096973
25.580884	1336.495736	15.101991
25.678074	1336.947628	15.107008
25.435563	1345.127383	15.112026
25.656721	1341.810423	15.117043
25.644112	1351.883227	15.122061
25.948195	1355.699180	15.127079
25.538057	1334.094244	15.132096
25.797277	1346.446245	15.137114
25.911397	1341.377786	15.142131
25.731924	1348.791939	15.147149
25.658610	1348.106814	15.152167
26.154341	1335.723033	15.157184
25.756762	1344.140418	15.162202
26.033928	1337.609619	15.167219
26.090399	1339.521778	15.172237
25.573379	1342.931219	15.177255
25.637684	1333.131490	15.182272
25.968037	1335.170328	15.187290
25.962215	1329.368825	15.192307
26.321287	1344.934713	15.197325
26.344079	1338.119151	15.202343
26.353856	1336.002719	15.207360
26.014625	1338.139039	15.212378
25.596322	1341.527616	15.217395
26.237656	1333.020813	15.222413
25.489299	1340.064742	15.227431
26.006505	1340.198926	15.232448
25.687816	1343.806666	15.237466
25.880358	1341.188380	15.242483
26.351588	1340.683929	15.247501
26.084890	1341.569902	15.252519
26.153137	1337.462550	15.257536
26.479141	1348.647875	15.262554
26.175330	1345.210670	15.267571
26.313266	1339.529017	15.272589
26.160554	1361.198196	15.277607
26.570375	1363.944347	15.282624
26.714648	1363.840871	15.287642
26.079526	1356.373073	15.292659
26.597078	1362.058907	15.297677
26.640526	1368.682806	15.302695
26.588599	1360.837033	15.307712
26.341569	1352.214403	15.312730
26.302490	1360.850670	15.317747
26.578987	1363.324376	15.322765
26.281808	1371.727711	15.327783
26.609598	1377.171650	15.332800
26.850469	1375.147098	15.337818
27.037055	1378.518985	15.342835
27.121328	1379.688910	15.347853
26.727961	1366.062927	15.352871
26.615387	1366.542912	15.357888
26.740700	1363.210095	15.362906
26.664713	1373.444187	15.367923
26.971230	1372.614794	15.372941
26.542332	1380.389869	15.377959
26.661790	1373.146654	15.382976
26.727369	1379.473035	15.387994
26.663677	1379.386317	15.393011
26.996406	1368.081741	15.398029
26.703348	1376.789519	15.403047
26.888536	1369.498419	15.408064
26.408728	1379.313124	15.413082
26.584665	1383.801119	15.418099
27.004260	1371.898125	15.423117
26.708684	1379.308968	15.428135
27.236789	1394.572669	15.433152
27.310516	1400.217674	15.438170
27.217235	1385.525555	15.443187
27.121140	1377.811768	15.448205
26.897282	1380.414185	15.453223
27.416526	1393.924511	15.458240
27.153890	1396.003213	15.463258
27.426278	1398.155158	15.468275
27.232433	1394.428194	15.473293
27.323273	1395.555258	15.478311
27.566718	1394.584302	15.483328
27.480911	1385.183937	15.488346
27.318383	1376.666895	15.493363
27.442123	1370.606132	15.498381
27.427085	1375.251683	15.503399
27.499567	1363.770451	15.508416
27.288947	1372.677893	15.513434
27.280902	1367.047246	15.518451
27.527574	1376.846454	15.523469
27.287540	1389.577032	15.528487
27.431819	1398.892186	15.533504
27.576909	1397.390402	15.538522
27.452103	1399.786451	15.543539
27.492720	1399.675154	15.548557
27.740581	1408.951293	15.553575
27.830763	1403.724305	15.558592
27.862441	1401.500161	15.563610
27.435980	1407.177776	15.568627
27.960593	1394.661031	15.573645
27.765973	1396.421349	15.578663
27.664938	1398.749142	15.583680
27.666276	1399.833279	15.588698
27.810620	1402.659210	15.593715
27.695033	1394.441226	15.598733
28.000405	1400.301656	15.603751
27.708550	1390.569259	15.608768
28.118417	1398.203678	15.613786
28.412121	1396.339766	15.618803
28.470271	1389.477957	15.623821
28.520309	1401.456379	15.628839
28.306225	1398.036064	15.633856
28.022095	1378.353746	15.638874
28.048954	1374.803533	15.643891
28.106285	1375.891849	15.648909
27.931732	1384.955727	15.653927
27.980419	1390.832996	15.658944
28.147708	1400.756471	15.663962
27.784020	1405.270060	15.668979
28.488494	1394.738815	15.673997
28.249500	1402.537251	15.679015
27.910309	1399.493933	15.684032
28.123015	1397.644696	15.689050
28.263627	1398.615968	15.694067
28.350953	1394.041898	15.699085
27.732147	1396.038348	15.704103
27.885153	1399.640429	15.709120
28.453154	1402.713830	15.714138
28.182641	1416.245796	15.719155
28.066455	1421.717445	15.724173
28.276439	1431.661181	15.729191
28.387747	1434.212440	15.734208
28.457064	1423.690857	15.739226
28.496941	1434.288626	15.744243
28.389883	1434.876732	15.749261
28.454741	1434.627407	15.754279
28.010955	1423.731944	15.759296
28.600161	1417.525600	15.764314
28.362557	1426.571570	15.769331
28.910850	1433.305413	15.774349
29.192123	1441.011119	15.779367
29.002605	1428.808149	15.784384
29.154606	1423.549293	15.789402
28.967402	1422.699029	15.794419
28.982641	1414.225116	15.799437
29.050222	1429.344168	15.804455
28.951973	1423.135207	15.809472
28.942360	1423.875520	15.814490
28.835043	1419.263550	15.819507
29.036584	1426.024163	15.824525
29.141914	1424.530375	15.829543
29.501097	1419.167880	15.834560
29.006477	1417.382039	15.839578
28.788357	1415.601156	15.844595
29.175264	1415.046589	15.849613
29.227958	1409.102334	15.854631
29.291537	1424.371688	15.859648
29.630617	1424.703361	15.864666
29.313850	1428.742723	15.869683
29.149819	1419.785320	15.874701
28.974563	1416.651680	15.879719
28.974325	1415.808733	15.884736
29.356672	1411.459692	15.889754
29.047937	1419.308286	15.894771
29.068553	1415.150807	15.899789
29.087225	1424.164253	15.904807
28.797705	1421.115958	15.909824
29.249574	1429.506652	15.914842
29.112245	1446.559074	15.919859
29.671459	1440.743729	15.924877
29.535016	1447.346533	15.929895
29.550669	1449.429894	15.934912
29.813052	1445.174255	15.939930
29.523909	1453.057700	15.944947
29.857454	1441.803330	15.949965
29.649068	1447.001003	15.954983
29.565940	1452.555193	15.960000
29.983151	1446.511806	15.965018
29.393464	1442.726704	15.970035
29.836000	1451.518657	15.975053
29.576058	1450.469030	15.980071
29.432708	1445.487208	15.985088
29.728202	1437.400313	15.990106
29.300461	1458.270636	15.995123
29.539308	1449.891055	16.000141
29.524545	1450.765336	16.005159
29.618679	1450.097958	16.010176
30.070734	1459.648596	16.015194
30.141408	1465.606384	16.020211
30.157947	1466.348121	16.025229
30.252633	1450.465721	16.030247
29.641887	1452.702158	16.035264
29.853831	1459.039700	16.040282
29.620494	1476.638198	16.045299
30.295012	1475.076737	16.050317
30.437974	1474.567145	16.055335
30.100147	1477.758468	16.060352
30.655144	1473.543211	16.065370
30.362839	1475.829393	16.070387
30.887216	1469.755023	16.075405
30.617753	1446.698894	16.080423
30.371757	1439.535633	16.085440
30.698159	1430.318527	16.090458
30.588650	1439.411839	16.095475
30.268926	1447.928934	16.100493
30.024183	1435.354681	16.105511
30.329890	1443.111716	16.110528
30.276944	1442.080147	16.115546
30.502755	1444.665717	16.120563
30.598475	1440.637100	16.125581
30.417157	1435.820469	16.130599
30.411080	1441.588238	16.135616
30.690941	1453.675735	16.140634
30.169555	1463.039701	16.145651
30.530265	1465.592301	16.150669
30.476642	1470.539409	16.155687
30.481475	1469.364847	16.160704
30.858073	1467.018950	16.165722
30.562177	1467.874499	16.170739
30.696269	1468.820906	16.175757
30.729948	1476.986842	16.180775
30.597645	1481.470622	16.185792
30.908693	1472.829017	16.190810
30.555137	1472.368333	16.195827
31.091844	1466.947035	16.200845
31.194246	1470.531034	16.205863
30.858481	1476.668761	16.210880
31.374271	1468.588178	16.215898
31.101738	1472.711315	16.220915
31.238153	1472.695415	16.225933
31.549037	1476.446446	16.230951
31.113187	1478.759604	16.235968
31.255363	1467.617957	16.240986
30.931027	1471.776750	16.246003
31.311135	1475.939971	16.251021
31.337413	1466.558926	16.256039
30.695250	1477.403994	16.261056
31.277282	1468.498977	16.266074
30.953937	1475.471274	16.271091
30.900496	1474.071246	16.276109
31.076280	1482.791225	16.281127
31.373805	1488.569168	16.286144
31.451854	1490.225258	16.291162
31.639724	1495.334531	16.296179
31.508115	1495.568151	16.301197
31.569304	1480.908125	16.306215
31.280080	1492.584119	16.311232
31.738002	1491.494091	16.316250
32.185673	1488.360727	16.321267
31.595617	1489.756528	16.326285
31.874343	1481.675635	16.331303
31.418354	1473.116721	16.336320
31.815943	1481.632904	16.341338
32.138920	1489.752000	16.346355
31.703733	1476.678028	16.351373
31.577063	1468.151244	16.356391
31.725605	1469.734216	16.361408
31.909395	1485.020030	16.366426
31.757928	1491.055684	16.371443
32.171348	1494.919861	16.376461
31.965002	1487.914758	16.381479
31.870926	1493.118047	16.386496
31.906760	1486.993563	16.391514
32.076373	1489.407261	16.396531
31.576107	1491.051867	16.401549
31.960288	1489.683902	16.406567
31.812347	1501.401827	16.411584
31.722848	1498.231023	16.416602
31.700656	1494.542721	16.421619
31.685349	1504.548362	16.426637
31.974395	1501.922953	16.431655
32.235423	1528.967663	16.436672
32.387097	1527.722639	16.441690
32.079521	1527.097359	16.446707
32.282097	1535.172155	16.451725
32.388517	1523.241633	16.456743
32.127838	1526.818600	16.461760
32.035504	1526.185159	16.466778
32.479204	1522.678808	16.471795
32.759075	1523.890412	16.476813
32.885275	1518.901330	16.481831
32.724635	1528.448783	16.486848
32.806618	1514.717542	16.491866
32.708614	1518.041395	16.496883
32.811435	1514.920692	16.501901
33.116740	1509.234299	16.506919
32.347422	1496.701902	16.511936
32.412217	1504.218749	16.516954
32.830611	1502.945714	16.521971
32.455979	1519.074630	16.526989
32.969852	1525.090718	16.532007
32.491756	1528.292321	16.537024
32.485907	1526.204528	16.542042
32.728033	1517.816080	16.547059
32.711440	1520.184931	16.552077
32.891905	1517.341496	16.557095
32.434802	1523.408305	16.562112
32.846578	1519.379814	16.567130
32.858169	1521.068564	16.572147
33.150579	1525.332277	16.577165
33.083756	1516.245147	16.582183
32.715169	1527.367392	16.587200
32.989907	1535.397922	16.592218
33.365551	1541.217220	16.597235
33.026018	1545.227835	16.602253
33.407674	1542.098693	16.607271
33.276513	1555.554518	16.612288
33.051089	1547.415135	16.617306
33.124534	1546.461112	16.622323
33.370653	1550.399662	16.627341
33.334000	1551.044606	16.632359
33.575119	1555.048983	16.637376
34.021795	1547.838176	16.642394
33.916785	1538.448098	16.647411
33.450460	1537.872481	16.652429
33.415155	1516.661339	16.657447
33.543288	1517.211879	16.662464
33.230171	1523.222107	16.667482
33.580877	1530.715538	16.672499
33.296611	1548.615400	16.677517
33.703334	1545.855621	16.682535
33.339820	1553.284494	16.687552
33.273004	1548.979748	16.692570
33.669248	1550.112733	16.697587
33.329144	1549.075663	16.702605
33.762085	1546.057424	16.707623
33.743709	1547.769821	16.712640
33.902460	1563.608884	16.717658
33.956327	1568.671071	16.722675
34.008185	1586.364116	16.727693
34.344359	1573.535801	16.732711
33.843892	1555.661803	16.737728
33.874276	1543.255274	16.742746
34.091545	1554.316068	16.747763
33.959497	1571.032646	16.752781
33.803251	1577.116402	16.757799
33.773684	1579.008299	16.762816
34.189130	1577.892081	16.767834
34.241726	1576.252579	16.772851
34.460844	1580.837963	16.777869
34.579107	1572.376618	16.782887
34.350285	1574.336541	16.787904
34.428045	1571.160275	16.792922
34.843075	1573.074772	16.797939
34.778837	1567.578898	16.802957
34.873847	1553.285093	16.807975
34.551696	1545.495402	16.812992
34.314590	1543.709097	16.818010
34.324396	1532.442052	16.823027
34.165530	1544.732022	16.828045
34.199638	1556.883392	16.833063
34.476840	1564.539852	16.838080
34.458961	1566.618741	16.843098
34.784353	1566.294032	16.848115
34.414261	1572.660147	16.853133
34.549605	1562.767378	16.858151
34.644813	1559.358570	16.863168
34.404969	1570.987569	16.868186
34.708936	1565.255317	16.873203
34.798988	1575.890253	16.878221
34.568735	1572.508109	16.883239
34.719578	1569.651632	16.888256
34.745690	1585.128771	16.893274
35.099635	1588.360186	16.898291
35.056103	1593.355214	16.903309
35.054528	1590.383906	16.908327
35.223755	1601.375797	16.913344
35.211112	1596.800304	16.918362
35.250868	1587.451918	16.923379
35.332590	1590.096080	16.928397
35.390031	1565.776505	16.933415
34.991496	1574.651313	16.938432
34.663123	1575.808530	16.943450
35.139921	1580.805688	16.948467
35.024681	1592.505868	16.953485
35.075419	1592.404254	16.958503
35.290608	1589.201665	16.963520
35.471490	1593.240792	16.968538
35.655809	1589.036692	16.973555
35.334362	1591.683044	16.978573
35.281609	1588.279125	16.983591
35.162158	1587.185319	16.988608
35.173484	1599.501669	16.993626
35.930207	1607.001121	16.998643
35.724425	1611.758196	17.003661
35.467924	1597.171825	17.008679
35.723141	1611.617867	17.013696
35.389298	1618.026216	17.018714
35.875028	1619.879773	17.023731
35.806449	1626.712775	17.028749
36.112684	1619.305124	17.033767
35.883850	1618.243458	17.038784
35.909185	1620.679552	17.043802
36.079958	1611.273646	17.048819
35.783979	1617.833788	17.053837
35.970145	1622.496102	17.058855
36.388891	1626.456260	17.063872
36.119983	1621.238400	17.068890
36.073329	1616.583683	17.073907
35.887770	1628.888927	17.078925
35.928783	1623.227727	17.083943
36.456390	1620.434215	17.088960
36.132978	1632.447314	17.093978
36.703201	1614.619224	17.098995
36.840421	1621.379926	17.104013
36.520607	1607.326900	17.109031
36.572619	1585.640407	17.114048
36.200797	1589.989676	17.119066
35.990943	1580.303735	17.124083
36.010650	1592.704479	17.129101
36.203192	1609.277639	17.134119
36.346338	1610.094930	17.139136
36.274858	1616.049588	17.144154
36.372122	1610.166913	17.149171
36.328206	1623.573188	17.154189
36.303791	1613.024631	17.159207
36.309156	1618.712936	17.164224
36.578881	1629.555319	17.169242
37.064931	1638.437566	17.174259
36.735169	1636.580907	17.179277
36.744419	1627.275134	17.184295
37.012743	1642.319024	17.189312
36.754789	1640.796155	17.194330
37.459543	1644.277704	17.199347
37.007579	1626.720542	17.204365
36.544600	1616.428694	17.209383
36.884887	1623.421539	17.214400
36.821273	1641.425816	17.219418
36.752999	1637.570558	17.224435
36.848153	1641.435793	17.229453
37.137398	1643.956184	17.234471
37.357350	1641.211087	17.239488
37.025041	1639.696635	17.244506
37.420719	1633.871460	17.249523
37.340139	1631.562976	17.254541
37.254364	1637.605929	17.259559
37.853075	1638.297862	17.264576
37.446204	1637.264358	17.269594
37.453357	1627.141530	17.274611
37.563265	1634.219554	17.279629
37.144471	1642.463943	17.284647
37.668477	1628.835181	17.289664
37.423779	1635.347950	17.294682
37.647598	1635.853739	17.299699
37.627158	1638.936734	17.304717
37.128849	1639.507669	17.309735
37.803433	1635.973519	17.314752
37.461610	1639.446694	17.319770
37.459022	1627.463909	17.324787
37.418172	1639.419903	17.329805
37.864656	1662.555839	17.334823
38.156445	1659.625961	17.339840
37.873226	1652.279987	17.344858
37.647832	1634.817448	17.349875
37.954620	1642.556286	17.354893
38.161948	1650.152714	17.359911
38.202907	1660.393323	17.364928
37.625767	1657.367127	17.369946
38.203202	1654.983618	17.374963
38.173887	1659.370255	17.379981
38.184697	1661.921063	17.384999
38.455029	1651.874763	17.390016
37.884189	1657.198044	17.395034
38.292362	1661.524633	17.400051
38.521502	1662.757547	17.405069
38.562675	1661.169213	17.410087
38.832984	1661.064994	17.415104
38.405727	1642.180593	17.420122
38.335240	1622.342029	17.425139
38.308679	1631.503918	17.430157
38.337936	1643.975120	17.435175
38.591383	1652.641717	17.440192
38.789148	1663.541742	17.445210
38.573849	1660.983092	17.450227
38.868134	1649.159256	17.455245
38.521045	1663.003811	17.460263
38.560578	1658.468571	17.465280
38.786062	1655.813872	17.470298
38.775777	1656.931913	17.475315
38.675323	1662.044609	17.480333
38.182562	1658.839359	17.485351
38.458883	1654.259584	17.490368
39.022981	1660.903013	17.495386
38.650783	1653.510082	17.500403
38.834223	1656.714440	17.505421
38.782230	1660.946286	17.510439
39.254628	1663.999909	17.515456
38.847886	1672.033168	17.520474
39.101571	1670.593063	17.525491
38.915026	1681.190841	17.530509
38.713762	1694.278446	17.535527
39.560645	1687.594696	17.540544
39.143565	1685.565185	17.545562
39.309378	1681.283515	17.550579
39.127593	1687.385867	17.555597
39.345375	1690.649706	17.560615
39.575944	1684.446081	17.565632
39.243411	1682.945838	17.570650
39.742191	1676.867510	17.575667
39.763106	1679.767417	17.580685
39.817931	1683.221418	17.585703
39.883336	1676.877197	17.590720
40.002994	1680.849670	17.595738
40.098865	1683.951712	17.600755
39.979561	1678.635339	17.605773
39.548010	1678.875894	17.610791
39.787701	1675.469851	17.615808
39.787291	1679.203038	17.620826
39.795024	1681.143677	17.625843
39.904173	1678.988110	17.630861
40.089997	1682.737404	17.635879
40.024147	1678.082415	17.640896
39.895804	1671.602106	17.645914
40.077979	1670.972385	17.650931
39.928881	1671.170418	17.655949
40.090821	1682.825110	17.660967
40.214769	1674.706082	17.665984
39.849406	1686.034209	17.671002
39.716772	1674.869446	17.676019
39.679987	1676.990179	17.681037
39.182445	1685.819418	17.686055
39.400854	1696.921069	17.691072
39.618397	1710.614124	17.696090
39.812808	1716.692936	17.701107
40.128264	1721.529592	17.706125
40.098768	1747.920868	17.711143
40.635629	1738.476529	17.716160
40.514219	1748.175677	17.721178
40.778986	1744.488515	17.726195
40.459009	1743.614140	17.731213
40.373397	1741.098604	17.736231
40.900486	1728.883963	17.741248
41.019576	1735.315894	17.746266
40.822410	1734.999666	17.751283
41.286752	1735.565806	17.756301
40.975534	1736.279096	17.761319
41.145097	1734.467930	17.766336
40.851501	1734.049324	17.771354
40.777386	1722.901662	17.776371
41.080376	1728.414553	17.781389
41.208190	1741.602487	17.786407
41.103113	1723.996369	17.791424
40.959277	1735.555479	17.796442
40.980275	1739.928393	17.801459
41.245104	1738.385573	17.806477
40.877734	1736.772385	17.811495
41.030849	1731.599072	17.816512
41.214238	1737.123023	17.821530
41.058576	1734.801016	17.826547
41.438261	1729.571532	17.831565
41.226302	1731.055298	17.836583
41.256932	1727.225979	17.841600
41.181464	1733.468407	17.846618
41.110539	1752.481272	17.851635
41.712643	1765.950942	17.856653
41.595138	1769.571927	17.861671
41.809891	1763.367833	17.866688
41.856564	1761.277698	17.871706
41.678704	1759.831646	17.876723
42.060787	1747.615865	17.881741
41.904390	1756.632350	17.886759
41.831982	1737.146770	17.891776
41.801360	1727.052797	17.896794
41.809903	1734.638068	17.901811
41.792585	1740.179501	17.906829
41.780070	1760.495510	17.911847
42.135342	1754.227165	17.916864
42.444248	1751.579410	17.921882
42.299074	1744.551102	17.926899
42.940556	1727.603686	17.931917
42.216256	1717.422725	17.936935
42.385037	1721.271418	17.941952
42.474879	1718.170225	17.946970
42.319270	1709.694733	17.951987
42.273973	1716.882092	17.957005
41.917060	1721.473358	17.962023
42.086724	1711.360805	17.967040
42.241313	1711.146885	17.972058
41.940079	1718.302528	17.977075
42.461294	1734.170179	17.982093
42.659526	1748.845830	17.987111
42.388437	1744.361067	17.992128
42.378390	1749.432697	17.997146
42.212446	1746.869115	18.002163
42.598104	1747.134929	18.007181
42.109160	1753.949105	18.012199
42.485193	1752.499041	18.017216
42.431084	1758.017651	18.022234
42.606301	1766.496519	18.027251
42.818022	1767.286311	18.032269
42.772092	1774.313550	18.037287
42.894691	1782.461643	18.042304
43.048111	1771.715145	18.047322
43.292345	1782.846685	18.052339
43.338591	1775.970211	18.057357
42.644633	1777.818154	18.062375
42.937087	1779.644232	18.067392
43.041404	1774.585977	18.072410
43.395697	1781.150850	18.077427
43.475658	1772.408134	18.082445
43.036399	1775.206622	18.087463
43.397392	1773.696922	18.092480
43.328178	1771.740449	18.097498
43.134906	1782.137060	18.102515
43.528292	1782.042846	18.107533
43.700830	1793.304811	18.112551
43.558492	1800.035167	18.117568
43.863777	1793.928151	18.122586
43.233877	1785.801686	18.127603
43.462558	1795.569987	18.132621
43.608802	1802.249290	18.137639
43.582603	1809.422786	18.142656
43.494697	1804.627036	18.147674
43.225847	1808.093642	18.152691
43.537106	1809.073088	18.157709
43.645012	1808.325372	18.162727
43.958997	1824.511358	18.167744
43.844392	1830.447109	18.172762
43.948425	1836.206382	18.177779
44.074277	1834.632650	18.182797
44.277043	1839.086252	18.187815
44.386803	1840.002992	18.192832
44.585072	1824.424540	18.197850
44.147461	1811.298726	18.202867
44.553513	1800.485268	18.207885
44.534509	1803.468430	18.212903
44.124758	1804.857359	18.217920
44.082530	1796.208030	18.222938
44.221598	1817.756152	18.227955
44.442000	1818.018015	18.232973
44.445273	1823.362222	18.237991
44.286349	1833.008397	18.243008
44.795105	1821.585115	18.248026
44.410331	1818.206966	18.253043
44.695031	1819.800491	18.258061
44.672385	1822.550394	18.263079
44.819848	1822.429438	18.268096
44.700709	1816.858233	18.273114
44.633718	1824.156855	18.278131
44.747803	1822.676491	18.283149
44.663982	1820.479572	18.288167
44.497092	1825.897450	18.293184
45.087839	1842.530158	18.298202
45.105094	1854.013304	18.303219
45.096257	1858.689042	18.308237
45.182699	1859.303050	18.313255
45.219421	1857.112233	18.318272
45.328404	1848.181799	18.323290
45.135592	1857.398705	18.328307
45.332486	1853.652674	18.333325
45.132738	1850.849170	18.338343
45.202149	1861.288208	18.343360
45.308886	1853.683521	18.348378
45.300440	1854.731960	18.353395
45.463220	1855.053710	18.358413
45.148918	1850.681457	18.363431
45.197007	1856.993705	18.368448
45.608129	1852.564405	18.373466
45.585717	1875.890909	18.378483
46.100665	1868.674551	18.383501
45.961007	1867.824378	18.388519
45.436622	1867.441006	18.393536
45.789866	1873.044951	18.398554
45.857495	1870.685427	18.403571
45.833795	1868.957388	18.408589
46.374099	1871.421778	18.413607
46.165720	1866.513577	18.418624
46.244457	1869.374074	18.423642
46.203913	1874.152509	18.428659
46.269759	1870.978226	18.433677
46.514286	1866.332178	18.438695
46.126293	1867.185031	18.443712
46.440682	1865.667564	18.448730
45.986128	1871.174153	18.453747
46.467485	1867.235233	18.458765
46.406477	1864.828071	18.463783
46.552732	1871.014819	18.468800
46.647707	1863.174711	18.473818
46.517849	1875.281204	18.478835
46.402988	1862.426823	18.483853
46.607126	1867.522405	18.488871
46.561360	1867.269598	18.493888
46.516151	1868.727936	18.498906
46.597512	1874.805324	18.503923
46.553093	1868.516475	18.508941
47.109651	1870.805615	18.513959
46.882982	1867.719679	18.518976
46.726926	1860.555372	18.523994
46.569655	1863.059825	18.529011
46.735491	1866.424746	18.534029
46.801043	1859.381912	18.539047
46.803096	1873.923973	18.544064
47.013915	1893.026909	18.549082
46.592601	1901.538435	18.554099
46.783601	1897.456746	18.559117
46.937580	1901.529310	18.564135
46.999572	1896.365660	18.569152
47.149507	1896.177736	18.574170
47.067403	1909.594742	18.579187
47.417180	1921.895448	18.584205
47.349775	1917.356812	18.589223
47.371262	1929.777993	18.594240
47.693155	1933.513467	18.599258
47.663475	1929.021516	18.604275
47.938732	1933.267415	18.609293
47.859706	1924.762137	18.614311
47.809180	1921.334138	18.619328
47.986891	1918.213903	18.624346
47.856916	1927.779179	18.629363
48.242581	1920.223105	18.634381
48.369098	1921.003102	18.639399
48.235013	1909.469473	18.644416
47.796710	1903.608426	18.649434
48.158649	1907.553198	18.654451
48.305149	1914.169899	18.659469
48.148580	1903.305571	18.664487
48.059238	1906.754414	18.669504
48.035651	1914.763447	18.674522
48.045943	1920.658131	18.679539
48.236409	1924.578363	18.684557
48.165556	1925.581200	18.689575
48.270757	1933.410266	18.694592
48.125122	1929.150429	18.699610
48.089634	1933.617739	18.704627
47.896376	1925.289547	18.709645
48.202156	1942.574058	18.714663
47.930263	1959.589079	18.719680
48.215777	1961.878242	18.724698
48.507309	1968.151158	18.729715
48.580689	1961.393983	18.734733
48.570369	1966.398792	18.739751
48.541609	1981.607347	18.744768
48.895054	1979.725645	18.749786
48.792968	1983.308991	18.754803
49.202735	1976.471690	18.759821
49.669744	1969.674979	18.764839
49.079958	1979.199421	18.769856
49.551716	1975.275902	18.774874
49.579642	1966.596731	18.779891
49.118582	1957.498187	18.784909
49.523470	1943.193028	18.789927
49.308498	1952.902437	18.794944
49.208934	1948.668164	18.799962
49.150132	1953.303278	18.804979
49.450958	1968.349393	18.809997
50.033071	1965.332670	18.815015
50.060229	1971.560353	18.820032
50.498410	1955.872123	18.825050
49.813739	1954.951195	18.830067
49.616273	1949.640255	18.835085
49.856490	1949.613646	18.840103
49.670611	1956.149932	18.845120
49.919703	1947.630516	18.850138
49.710528	1951.110546	18.855155
49.921763	1942.262934	18.860173
50.028175	1938.829679	18.865191
49.443466	1949.767594	18.870208
49.868024	1950.725262	18.875226
49.483910	1952.400004	18.880243
49.381895	1955.234807	18.885261
49.697614	1966.573149	18.890279
49.435092	1976.576590	18.895296
49.706592	1981.565766	18.900314
49.900631	1999.091969	18.905331
50.139020	2006.949423	18.910349
50.406634	1995.455929	18.915367
50.297768	2008.031035	18.920384
50.329515	1994.361537	18.925402
50.663242	1997.753220	18.930419
50.585518	1997.181042	18.935437
50.564243	2001.046247	18.940455
50.804387	2001.452781	18.945472
50.519453	1986.604347	18.950490
50.587846	2004.663191	18.955507
50.797369	2006.560610	18.960525
51.625461	2019.329854	18.965543
51.257751	2006.532487	18.970560
51.385842	1993.904884	18.975578
51.198546	1985.805590	18.980595
51.196498	1980.834806	18.985613
51.297304	1986.695883	18.990631
51.231059	1974.324480	18.995648
51.007459	1981.441730	19.000666
51.096852	1979.346998	19.005683
50.991169	1982.145029	19.010701
51.441622	1978.549221	19.015719
51.184484	1980.071075	19.020736
51.317773	1994.085167	19.025754
51.552752	2008.550010	19.030771
51.931811	2019.645216	19.035789
51.806565	2008.138743	19.040807
51.404272	2001.396168	19.045824
51.397270	2006.968215	19.050842
51.298397	2018.463517	19.055859
51.668155	2020.958354	19.060877
51.334850	2024.107666	19.065895
51.332950	2016.674697	19.070912
51.428793	2019.029464	19.075930
51.773559	2037.659549	19.080947
51.588200	2049.316179	19.085965
51.837320	2055.141221	19.090983
52.075404	2054.195953	19.096000
52.109015	2049.689178	19.101018
52.503287	2044.927628	19.106035
52.223814	2049.925453	19.111053
52.452757	2045.572617	19.116071
52.499081	2051.686794	19.121088
52.337088	2052.390262	19.126106
52.594022	2046.695432	19.131123
52.333861	2043.048589	19.136141
52.278501	2043.425857	19.141159
52.691206	2048.929896	19.146176
52.277409	2041.557298	19.151194
52.525452	2056.365663	19.156211
52.191057	2074.106584	19.161229
52.770646	2072.689712	19.166247
52.869894	2083.150558	19.171264
52.812470	2084.578329	19.176282
52.693360	2075.918796	19.181299
52.906610	2073.610662	19.186317
52.659203	2081.319918	19.191335
52.880321	2087.066690	19.196352
53.051685	2096.447707	19.201370
53.247604	2107.296777	19.206387
53.147341	2115.782904	19.211405
53.515269	2106.515364	19.216423
53.220204	2107.010120	19.221440
53.081934	2103.569562	19.226458
53.982816	2105.945393	19.231475
53.363932	2111.753114	19.236493
53.577861	2099.469027	19.241511
53.466743	2095.158338	19.246528
53.041827	2098.557657	19.251546
53.719670	2098.810003	19.256563
53.684679	2093.893264	19.261581
53.803561	2103.851475	19.266599
53.827962	2102.431350	19.271616
53.903740	2105.626697	19.276634
53.737703	2098.872318	19.281651
53.767025	2107.096030	19.286669
54.032615	2123.926149	19.291687
54.104442	2123.040489	19.296704
54.188495	2126.641567	19.301722
54.450779	2121.635263	19.306739
54.402538	2130.722015	19.311757
54.443046	2122.157940	19.316775
54.318081	2126.361078	19.321792
54.217790	2125.620693	19.326810
54.511058	2122.089604	19.331827
54.482660	2122.524464	19.336845
54.676542	2119.523876	19.341863
54.529412	2126.787159	19.346880
54.580728	2126.776794	19.351898
54.976229	2121.280653	19.356915
55.067868	2133.684062	19.361933
54.804300	2113.939012	19.366951
54.844805	2123.116858	19.371968
55.004069	2128.300547	19.376986
54.877655	2121.596852	19.382003
54.503755	2131.430091	19.387021
54.640083	2121.667528	19.392039
54.704409	2124.475810	19.397056
54.550302	2141.353493	19.402074
54.949020	2153.194745	19.407091
54.820239	2161.103024	19.412109
55.047017	2164.511112	19.417127
55.185684	2171.019012	19.422144
55.263239	2167.687914	19.427162
55.109589	2160.700641	19.432179
55.243688	2174.289889	19.437197
55.461696	2189.707556	19.442215
55.753591	2189.059004	19.447232
55.588773	2198.672157	19.452250
55.573975	2181.858040	19.457267
55.914514	2187.568231	19.462285
56.105035	2178.953992	19.467303
55.938038	2180.203285	19.472320
55.799160	2175.921746	19.477338
56.255760	2168.144700	19.482355
56.136736	2177.089262	19.487373
56.361000	2172.483219	19.492391
56.299340	2179.049095	19.497408
56.217698	2174.979823	19.502426
56.538926	2174.634162	19.507443
56.559469	2180.179497	19.512461
56.032650	2173.366451	19.517479
56.461865	2174.003998	19.522496
56.227330	2179.141819	19.527514
56.602227	2170.351070	19.532531
56.224987	2170.218878	19.537549
56.413984	2174.141394	19.542567
56.520971	2167.766221	19.547584
56.711329	2179.855847	19.552602
57.213881	2190.192491	19.557619
56.848712	2184.073880	19.562637
56.510703	2171.001561	19.567655
57.210848	2183.348718	19.572672
57.280326	2197.849987	19.577690
57.516703	2182.723770	19.582707
57.356237	2173.755477	19.587725
57.527949	2171.428070	19.592743
57.363274	2161.326481	19.597760
57.206792	2168.214954	19.602778
57.756481	2162.108025	19.607795
57.226230	2167.041388	19.612813
57.115705	2162.307682	19.617831
57.550885	2157.426076	19.622848
57.208574	2167.971348	19.627866
57.552581	2154.529316	19.632883
57.364244	2162.060349	19.637901
57.362443	2181.483992	19.642919
57.801900	2193.615184	19.647936
57.543672	2207.802515	19.652954
57.115639	2194.174661	19.657971
57.331113	2202.249167	19.662989
57.424219	2210.514762	19.668007
57.600374	2215.838912	19.673024
57.392186	2234.430160	19.678042
57.470040	2233.044172	19.683059
57.698052	2238.263362	19.688077
57.886075	2252.933362	19.693095
58.483486	2261.299162	19.698112
58.285666	2258.905945	19.703130
58.876049	2264.818247	19.708147
58.257081	2269.288039	19.713165
58.352330	2263.599984	19.718183
58.663859	2258.141031	19.723200
58.654688	2264.920811	19.728218
58.373240	2253.879195	19.733235
58.718884	2254.420033	19.738253
58.710589	2258.915062	19.743271
58.693371	2252.957272	19.748288
58.451293	2259.451737	19.753306
58.539679	2267.997742	19.758323
58.612244	2276.222792	19.763341
58.937160	2279.726695	19.768359
59.174110	2276.999051	19.773376
59.429390	2285.971639	19.778394
59.325813	2275.342886	19.783411
59.255633	2273.401872	19.788429
59.245478	2275.760676	19.793447
59.435336	2272.790675	19.798464
59.341306	2273.106851	19.803482
59.436483	2269.445888	19.808499
59.696592	2265.510154	19.813517
59.350435	2267.172119	19.818535
59.732199	2280.589057	19.823552
59.710989	2290.906890	19.828570
59.947578	2293.842386	19.833587
59.817524	2291.687978	19.838605
60.055531	2299.826398	19.843623
60.113126	2291.901921	19.848640
59.877690	2292.643979	19.853658
60.666354	2286.914992	19.858675
60.035273	2276.008120	19.863693
59.958392	2273.831210	19.868711
60.465446	2271.129709	19.873728
60.052737	2284.772642	19.878746
60.160619	2284.235964	19.883763
60.121930	2290.193917	19.888781
60.264039	2295.170334	19.893799
60.091626	2282.564094	19.898816
60.342110	2294.812030	19.903834
60.669754	2290.829272	19.908851
60.698319	2279.906165	19.913869
60.180454	2299.938988	19.918887
60.809345	2308.402582	19.923904
60.484714	2322.513198	19.928922
60.691034	2322.250238	19.933939
60.750729	2313.541015	19.938957
61.047908	2316.246407	19.943975
61.181459	2309.260228	19.948992
60.991261	2316.089181	19.954010
61.299994	2310.078635	19.959027
61.144885	2305.132810	19.964045
61.193288	2307.941494	19.969063
61.421627	2299.407333	19.974080
61.578911	2304.245697	19.979098
61.427742	2301.959454	19.984115
61.633880	2324.986771	19.989133
61.554759	2337.870083	19.994151
62.118743	2334.895777	19.999168
61.894929	2333.047248	20.004186
61.972952	2313.509563	20.009203
62.055300	2304.997279	20.014221
61.999094	2316.561480	20.019239
62.289155	2303.207324	20.024256
61.933859	2311.037961	20.029274
62.374829	2313.383214	20.034291
61.883652	2309.911763	20.039309
61.802541	2317.340221	20.044327
62.192821	2330.326540	20.049344
61.940602	2353.137163	20.054362
62.175632	2341.818714	20.059379
62.279579	2345.648752	20.064397
62.003464	2350.010957	20.069415
62.182534	2342.296372	20.074432
62.363802	2354.744441	20.079450
62.580970	2363.777161	20.084467
62.512912	2372.682382	20.089485
62.984192	2371.617179	20.094503
63.023414	2371.875072	20.099520
62.817489	2371.047257	20.104538
63.048557	2362.537008	20.109555
63.110057	2358.446296	20.114573
63.053179	2375.022476	20.119591
63.245506	2357.451282	20.124608
63.296886	2359.264818	20.129626
63.236797	2364.086131	20.134643
63.291325	2365.605380	20.139661
63.207850	2365.267676	20.144679
63.545761	2366.353238	20.149696
63.795551	2370.071650	20.154714
63.496412	2363.927471	20.159731
63.186053	2356.405471	20.164749
63.185098	2357.129380	20.169767
63.610986	2358.039991	20.174784
63.675147	2373.569269	20.179802
63.844968	2384.825433	20.184819
64.252654	2394.461041	20.189837
63.806529	2401.187430	20.194855
64.013581	2394.068907	20.199872
64.006466	2399.651350	20.204890
64.094824	2395.138634	20.209907
63.922890	2384.359296	20.214925
63.693796	2390.346783	20.219943
64.019765	2390.351543	20.224960
63.995956	2390.224117	20.229978
63.898404	2410.255894	20.234995
64.235103	2410.143835	20.240013
63.988980	2418.439350	20.245031
64.043502	2414.215153	20.250048
64.507483	2438.916819	20.255066
64.448625	2451.781000	20.260083
64.739194	2446.612237	20.265101
64.803770	2448.249477	20.270119
64.978775	2453.570756	20.275136
65.202474	2442.486499	20.280154
65.062980	2446.797743	20.285171
65.357942	2439.929525	20.290189
64.948141	2446.751297	20.295207
65.336465	2440.498671	20.300224
65.615959	2451.632913	20.305242
65.320944	2450.582534	20.310259
65.781051	2446.160422	20.315277
65.428200	2447.558943	20.320295
65.434267	2447.072792	20.325312
65.702555	2451.373187	20.330330
65.430343	2448.853302	20.335347
65.641185	2440.630777	20.340365
65.166825	2462.005387	20.345383
65.395025	2465.355807	20.350400
65.488868	2471.872306	20.355418
65.219940	2474.446401	20.360435
65.668945	2484.128532	20.365453
65.382627	2500.426018	20.370471
65.549152	2503.573600	20.375488
66.333913	2506.353724	20.380506
66.439373	2502.301115	20.385523
66.636712	2496.480492	20.390541
66.146435	2502.172586	20.395559
66.625938	2496.494957	20.400576
66.651630	2489.605943	20.405594
66.516801	2506.344470	20.410611
66.778892	2508.690496	20.415629
66.531664	2510.026811	20.420647
66.843168	2526.521090	20.425664
66.903988	2526.338988	20.430682
66.740159	2528.844671	20.435699
66.884995	2522.506179	20.440717
66.792927	2527.833896	20.445735
67.194287	2521.813689	20.450752
67.008304	2522.885918	20.455770
66.911396	2531.231513	20.460787
67.153808	2517.527803	20.465805
67.196687	2523.433271	20.470823
67.361233	2543.806173	20.475840
67.606337	2552.554637	20.480858
67.625433	2558.378355	20.485875
67.530943	2554.110365	20.490893
67.833728	2550.097940	20.495911
67.954287	2553.214824	20.500928
68.002534	2548.908975	20.505946
68.230020	2549.513398	20.510963
68.185413	2544.139033	20.515981
68.390859	2542.817771	20.520999
68.324561	2519.006991	20.526016
68.071595	2506.498648	20.531034
68.174626	2519.232749	20.536051
68.358113	2525.292881	20.541069
68.668954	2545.354827	20.546087
68.636073	2533.719908	20.551104
68.712087	2519.148511	20.556122
68.468396	2511.604768	20.561139
68.474817	2513.777270	20.566157
68.821101	2529.362288	20.571175
68.569425	2538.870835	20.576192
68.742958	2537.158915	20.581210
68.902394	2539.865912	20.586227
69.110112	2528.869388	20.591245
69.021234	2538.792619	20.596263
68.515012	2540.826207	20.601280
69.011148	2540.640349	20.606298
68.682120	2538.695641	20.611315
69.154710	2535.670816	20.616333
69.344584	2551.232269	20.621351
69.478034	2563.906063	20.626368
69.432532	2561.166945	20.631386
69.375253	2563.803997	20.636403
69.622520	2554.256831	20.641421
69.876094	2561.204327	20.646439
69.675386	2556.135509	20.651456
69.384533	2551.964189	20.656474
69.441674	2556.239387	20.661491
69.812294	2556.689326	20.666509
70.232469	2557.011851	20.671527
69.882669	2555.532199	20.676544
70.399530	2551.120805	20.681562
70.011315	2547.433187	20.686579
70.041911	2540.785872	20.691597
69.988942	2557.190678	20.696615
70.005497	2575.174408	20.701632
70.132975	2575.161223	20.706650
70.105473	2587.180624	20.711667
70.246748	2580.488327	20.716685
70.204461	2587.260536	20.721703
70.111996	2597.982195	20.726720
70.462236	2606.458289	20.731738
70.633787	2611.748712	20.736755
71.177452	2605.244941	20.741773
71.124062	2612.697136	20.746791
70.784295	2612.154505	20.751808
71.262879	2608.367088	20.756826
71.410648	2611.653364	20.761843
71.184614	2601.643127	20.766861
71.276622	2605.511503	20.771879
71.129403	2610.491949	20.776896
71.088987	2606.119382	20.781914
71.215164	2628.376465	20.786931
71.966686	2639.685076	20.791949
71.941704	2644.690252	20.796967
71.948964	2648.628296	20.801984
72.297847	2645.263179	20.807002
71.413881	2648.585384	20.812019
71.516859	2643.503848	20.817037
72.043918	2643.945870	20.822055
72.126074	2647.239465	20.827072
71.896724	2636.657232	20.832090
71.721053	2641.915843	20.837107
71.879523	2643.533067	20.842125
71.782983	2648.281174	20.847143
71.844692	2657.941611	20.852160
72.193465	2660.016848	20.857178
72.323890	2657.139657	20.862195
72.495499	2657.390608	20.867213
72.849653	2668.415337	20.872231
72.699436	2679.054810	20.877248
72.758527	2682.455535	20.882266
72.572341	2702.205189	20.887283
72.782635	2689.710203	20.892301
72.978350	2689.237208	20.897319
72.950072	2688.046574	20.902336
73.168098	2688.291142	20.907354
73.235243	2681.885577	20.912371
73.323156	2685.406581	20.917389
73.296455	2682.786287	20.922407
73.409830	2687.045578	20.927424
73.670960	2689.585533	20.932442
73.392930	2691.386281	20.937459
73.445143	2690.184997	20.942477
73.724325	2710.762125	20.947495
73.604384	2711.968739	20.952512
73.489834	2708.521617	20.957530
73.524853	2711.156257	20.962547
73.528256	2723.016892	20.967565
74.062053	2710.862561	20.972583
73.864654	2714.197012	20.977600
74.258696	2740.066473	20.982618
74.142803	2751.119872	20.987635
74.434764	2745.305773	20.992653
74.704448	2744.955552	20.997671
74.186934	2746.333501	21.002688
74.377152	2741.565383	21.007706
74.519972	2743.244367	21.012723
74.784961	2737.383705	21.017741
74.824863	2728.463433	21.022759
74.627236	2739.014995	21.027776
74.818326	2738.200208	21.032794
74.718297	2744.075920	21.037811
74.843654	2749.201838	21.042829
75.224690	2753.386118	21.047847
75.063066	2763.725973	21.052864
75.432671	2763.334994	21.057882
75.357642	2762.178359	21.062899
75.650142	2770.254130	21.067917
75.328723	2764.752312	21.072935
75.149800	2766.940089	21.077952
75.760090	2764.516138	21.082970
75.419463	2766.220519	21.087987
75.883343	2766.671803	21.093005
75.905716	2753.946733	21.098023
76.195007	2746.268969	21.103040
76.141973	2735.598161	21.108058
76.135201	2744.017408	21.113075
76.447833	2744.446582	21.118093
76.411390	2734.370677	21.123111
76.324990	2738.294876	21.128128
76.703288	2726.175856	21.133146
76.835011	2728.529304	21.138163
76.620155	2729.541130	21.143181
77.011773	2728.565957	21.148199
76.739703	2730.598801	21.153216
77.061010	2730.353136	21.158234
76.812166	2729.479106	21.163251
76.733862	2720.976027	21.168269
77.150877	2721.158916	21.173287
77.268210	2726.297228	21.178304
77.412624	2723.327058	21.183322
77.364144	2724.937245	21.188339
76.737799	2731.691521	21.193357
77.126578	2723.031969	21.198375
77.173454	2752.614395	21.203392
77.323119	2752.236710	21.208410
77.224139	2753.005008	21.213427
77.153723	2764.516847	21.218445
77.540389	2762.256456	21.223463
77.468717	2765.760736	21.228480
78.080847	2758.643478	21.233498
77.749357	2761.201569	21.238515
78.073949	2774.839797	21.243533
78.208887	2775.200207	21.248551
78.023656	2781.188984	21.253568
78.519517	2786.736521	21.258586
78.255577	2784.119082	21.263603
78.439113	2785.806053	21.268621
78.442609	2791.612843	21.273639
77.925498	2802.590944	21.278656
77.966154	2791.092073	21.283674
78.353528	2794.794086	21.288691
77.696416	2792.700832	21.293709
78.093975	2806.862899	21.298727
78.109156	2818.778290	21.303744
78.411515	2834.938179	21.308762
78.664624	2847.884657	21.313779
78.464237	2865.008104	21.318797
78.901190	2857.044291	21.323815
78.807334	2870.186519	21.328832
78.936761	2878.418676	21.333850
79.385558	2882.398423	21.338867
79.557445	2885.914526	21.343885
79.813282	2879.387536	21.348903
79.613510	2884.867723	21.353920
79.645048	2890.382285	21.358938
79.953605	2884.848810	21.363955
79.778579	2888.158197	21.368973
80.016988	2884.701713	21.373991
79.836027	2886.934746	21.379008
79.664244	2880.375538	21.384026
79.915653	2903.091948	21.389043
79.803099	2916.593395	21.394061
80.610921	2912.824278	21.399079
80.429215	2910.270687	21.404096
80.453676	2904.770161	21.409114
80.924696	2910.566143	21.414131
80.724491	2907.271485	21.419149
80.686312	2900.783081	21.424167
80.581098	2906.679431	21.429184
80.882417	2910.676596	21.434202
80.790408	2901.999357	21.439219
80.694458	2907.603512	21.444237
80.825445	2919.547953	21.449255
80.739134	2933.244167	21.454272
80.871136	2938.695843	21.459290
80.938323	2942.780410	21.464307
80.750989	2944.597926	21.469325
81.362909	2962.109873	21.474343
81.524265	2970.876868	21.479360
81.456901	2966.731699	21.484378
81.693819	2967.456594	21.489395
81.636413	2968.203598	21.494413
81.937191	2963.433784	21.499431
81.433696	2965.912714	21.504448
81.405507	2971.777769	21.509466
82.006381	2978.061064	21.514483
81.934604	2991.790276	21.519501
82.035889	2988.164328	21.524519
82.223261	3000.666993	21.529536
82.107574	2998.296595	21.534554
83.005247	2993.300790	21.539571
82.977032	3001.283605	21.544589
83.085236	2993.568252	21.549607
82.516018	2992.372680	21.554624
82.464082	2998.736403	21.559642
82.975891	2999.319663	21.564659
83.019359	2993.470897	21.569677
83.181985	2988.487707	21.574695
83.305596	2998.824492	21.579712
82.866549	2993.474283	21.584730
83.309985	3005.592825	21.589747
83.276174	3018.058608	21.594765
83.349263	3017.037222	21.599783
82.834675	3016.656857	21.604800
83.183458	3021.949324	21.609818
83.293098	3022.286512	21.614835
83.483925	3044.422056	21.619853
84.039407	3049.643654	21.624871
83.774565	3051.257103	21.629888
83.650867	3052.870769	21.634906
84.007659	3048.586702	21.639923
83.927773	3054.463014	21.644941
84.080917	3041.950771	21.649959
84.384190	3047.792891	21.654976
84.336783	3057.681773	21.659994
84.677865	3047.474000	21.665011
84.854196	3061.207203	21.670029
84.998474	3055.416736	21.675047
85.236438	3058.400183	21.680064
84.996796	3040.209234	21.685082
85.160715	3025.119046	21.690099
84.970044	3024.952492	21.695117
85.442965	3028.368186	21.700135
85.255815	3033.255591	21.705152
84.906781	3030.407767	21.710170
85.456850	3031.850786	21.715187
85.179997	3042.549231	21.720205
85.687203	3044.844652	21.725223
85.534586	3048.715700	21.730240
85.450315	3046.211536	21.735258
85.844920	3042.021009	21.740275
85.593610	3053.973604	21.745293
85.791524	3053.387601	21.750311
85.441953	3043.680208	21.755328
85.547179	3052.466322	21.760346
85.518439	3073.231391	21.765363
85.718305	3088.067107	21.770381
85.850120	3085.337662	21.775399
85.913851	3095.939948	21.780416
85.851202	3106.227618	21.785434
86.216094	3109.816215	21.790451
86.180534	3116.619001	21.795469
86.290929	3116.456746	21.800487
86.770570	3135.587960	21.805504
86.137622	3143.185449	21.810522
86.564500	3146.839033	21.815539
86.978044	3149.601017	21.820557
87.078464	3143.773146	21.825575
86.464931	3143.049823	21.830592
86.965777	3171.929878	21.835610
87.236585	3166.871379	21.840627
86.877410	3177.624195	21.845645
87.008468	3174.605039	21.850663
87.417665	3186.031020	21.855680
87.724410	3209.477125	21.860698
87.648751	3206.869074	21.865715
87.683458	3217.333868	21.870733
87.695689	3206.709043	21.875751
87.663110	3207.237583	21.880768
87.635317	3214.260387	21.885786
88.114903	3219.416298	21.890803
88.309950	3231.650058	21.895821
88.261088	3236.709921	21.900839
88.404354	3237.570597	21.905856
88.301769	3240.755803	21.910874
88.188778	3240.846065	21.915891
88.261688	3248.570671	21.920909
88.484870	3262.129838	21.925927
88.680657	3262.374293	21.930944
88.665542	3263.612593	21.935962
88.937468	3265.015901	21.940979
88.794024	3273.045387	21.945997
88.594597	3286.619538	21.951015
89.102308	3291.683230	21.956032
89.249983	3300.091259	21.961050
89.527271	3294.010126	21.966067
89.498021	3294.129347	21.971085
89.575702	3296.704004	21.976103
89.791289	3309.785671	21.981120
89.786037	3322.454717	21.986138
90.264642	3324.950404	21.991155
89.931851	3328.643702	21.996173
89.762642	3319.766823	22.001191
90.110689	3318.842403	22.006208
90.300954	3325.058411	22.011226
90.493223	3314.333341	22.016243
90.495055	3314.669329	22.021261
90.831277	3314.081657	22.026279
91.139262	3302.573596	22.031296
91.543977	3290.755982	22.036314
92.258689	3274.859945	22.041331
92.015829	3263.127386	22.046349
91.848730	3246.735963	22.051367
92.023227	3236.885046	22.056384
92.095879	3219.428705	22.061402
92.035306	3205.149439	22.066419
91.948488	3206.178721	22.071437
92.084965	3193.834604	22.076455
91.999503	3175.228006	22.081472
91.811326	3181.022122	22.086490
92.084878	3163.664498	22.091507
92.075179	3169.005088	22.096525
92.096453	3167.057733	22.101543
91.971704	3163.860342	22.106560
91.958083	3170.028550	22.111578
91.750534	3162.657072	22.116595
91.914904	3166.391896	22.121613
92.155646	3168.218740	22.126631
92.180372	3181.659076	22.131648
92.123635	3204.882393	22.136666
92.023884	3206.486455	22.141683
92.195178	3206.444495	22.146701
92.746369	3214.536788	22.151719
93.024863	3225.337037	22.156736
92.520896	3242.227840	22.161754
92.779522	3235.819937	22.166771
92.227170	3244.824433	22.171789
92.552819	3238.842139	22.176807
93.045730	3253.719129	22.181824
92.951425	3277.121472	22.186842
93.042805	3271.250212	22.191859
92.952285	3276.609419	22.196877
93.078505	3283.004931	22.201895
93.325240	3309.159700	22.206912
92.861048	3322.206708	22.211930
93.185188	3322.989124	22.216947
93.324418	3342.120672	22.221965
93.592214	3337.484776	22.226983
93.610318	3344.335166	22.232000
93.487069	3366.197379	22.237018
93.959910	3370.728373	22.242035
94.188580	3370.869533	22.247053
94.003569	3394.240345	22.252071
94.042611	3402.295316	22.257088
94.433967	3411.688629	22.262106
94.333573	3407.232399	22.267123
94.725093	3419.894931	22.272141
94.618511	3427.689777	22.277159
95.021743	3431.879888	22.282176
94.897134	3440.774931	22.287194
94.617205	3426.060523	22.292211
94.866409	3443.522572	22.297229
95.172164	3465.453924	22.302247
95.586726	3459.830405	22.307264
95.754567	3460.551416	22.312282
95.664591	3452.135789	22.317299
95.961779	3449.167646	22.322317
95.625485	3451.439201	22.327335
96.192093	3443.221319	22.332352
96.231015	3448.260686	22.337370
95.762225	3442.528718	22.342387
96.016288	3439.364773	22.347405
96.397564	3459.722184	22.352423
96.880980	3463.748129	22.357440
96.637561	3468.037300	22.362458
96.877266	3453.222753	22.367475
97.087552	3458.367421	22.372493
97.054835	3458.143065	22.377511
97.177097	3450.558967	22.382528
97.066874	3454.918234	22.387546
97.209927	3453.557191	22.392563
96.974278	3448.470446	22.397581
97.085493	3457.466044	22.402599
97.449456	3454.506141	22.407616
97.268961	3461.919098	22.412634
97.350448	3452.977897	22.417651
97.424934	3454.165410	22.422669
97.371220	3462.257579	22.427687
97.768364	3478.077397	22.432704
97.404535	3489.455775	22.437722
97.576773	3498.062107	22.442739
97.874301	3492.184563	22.447757
97.964080	3502.170704	22.452775
97.972744	3518.530504	22.457792
98.021366	3520.861304	22.462810
97.898404	3522.942715	22.467827
98.028503	3532.417909	22.472845
98.376494	3554.622524	22.477863
98.723350	3550.573941	22.482880
98.706968	3557.568164	22.487898
98.753694	3553.022088	22.492915
98.727710	3553.944877	22.497933
98.653930	3571.340366	22.502951
99.352313	3572.077536	22.507968
99.195154	3586.008562	22.512986
99.212501	3578.823583	22.518003
99.701835	3581.886111	22.523021
99.034399	3594.190837	22.528039
99.569581	3600.517940	22.533056
100.078917	3607.804034	22.538074
99.976540	3614.659446	22.543091
100.308253	3612.140580	22.548109
100.163353	3612.450537	22.553127
100.329393	3607.435064	22.558144
100.098473	3612.599506	22.563162
100.336473	3616.520286	22.568179
100.345129	3624.260819	22.573197
100.559313	3637.252426	22.578215
101.195380	3643.863897	22.583232
101.051429	3651.687313	22.588250
101.043061	3650.216748	22.593267
101.284438	3645.345865	22.598285
101.172727	3644.761731	22.603303
101.191875	3645.238100	22.608320
100.858412	3647.359555	22.613338
100.887587	3639.995311	22.618355
100.868802	3636.403977	22.623373
100.876821	3659.976002	22.628391
100.825300	3668.419954	22.633408
101.107997	3678.788981	22.638426
101.592916	3693.345634	22.643443
102.145243	3699.443798	22.648461
101.990447	3704.835435	22.653479
102.545169	3696.116188	22.658496
102.505156	3690.640619	22.663514
102.987784	3689.013414	22.668531
103.000311	3688.011819	22.673549
103.109544	3692.502860	22.678567
103.410950	3682.043939	22.683584
103.200218	3674.996467	22.688602
102.850209	3662.540066	22.693619
102.794602	3651.919483	22.698637
102.815936	3662.670399	22.703655
103.390572	3672.215956	22.708672
103.275572	3687.323595	22.713690
102.715934	3684.298318	22.718707
103.018080	3681.827828	22.723725
102.399674	3695.273324	22.728743
103.097076	3703.115553	22.733760
103.598184	3717.608809	22.738778
103.311719	3725.722113	22.743795
103.477735	3733.535746	22.748813
103.030912	3746.760483	22.753831
103.720228	3753.270723	22.758848
103.987550	3777.190691	22.763866
104.095248	3784.807997	22.768883
104.574261	3776.515963	22.773901
104.370315	3784.921526	22.778919
104.359187	3784.434344	22.783936
104.639745	3797.253246	22.788954
104.550594	3802.768341	22.793971
105.052907	3802.335689	22.798989
104.754950	3806.596496	22.804007
105.240467	3804.118965	22.809024
105.249658	3813.287416	22.814042
105.356243	3832.023480	22.819059
105.713710	3833.019951	22.824077
105.702382	3847.061672	22.829095
105.745216	3842.821770	22.834112
106.268928	3838.745157	22.839130
105.831986	3849.774817	22.844147
106.115398	3843.408889	22.849165
105.680958	3843.774003	22.854183
105.959524	3838.355604	22.859200
106.412288	3844.906439	22.864218
105.971635	3840.298131	22.869235
106.111910	3851.150073	22.874253
106.229327	3865.942376	22.879271
106.547488	3875.503675	22.884288
106.433496	3872.136536	22.889306
106.328530	3870.918792	22.894323
106.609912	3883.774642	22.899341
106.597238	3902.413094	22.904359
106.981358	3903.633406	22.909376
106.805894	3900.050758	22.914394
107.093451	3916.338740	22.919411
107.372511	3927.759220	22.924429
107.516768	3934.017224	22.929447
107.458552	3926.866306	22.934464
107.835707	3922.177626	22.939482
107.847531	3932.792524	22.944499
108.019784	3939.953840	22.949517
107.771489	3949.528812	22.954535
108.077801	3948.912380	22.959552
108.413937	3952.663625	22.964570
108.091846	3956.396975	22.969587
108.813705	3953.596153	22.974605
108.495446	3971.343524	22.979623
108.842242	3976.848524	22.984640
109.154233	3972.266302	22.989658
109.063941	3978.866977	22.994675
109.219658	3975.756805	22.999693
109.451140	3982.218829	23.004711
109.448625	3972.677403	23.009728
109.231498	3969.553180	23.014746
109.203730	3977.173325	23.019763
109.491029	3971.799065	23.024781
109.775939	3992.424934	23.029799
109.484121	4008.633553	23.034816
110.064832	3996.222103	23.039834
109.676393	4013.037210	23.044851
110.028882	4011.678020	23.049869
109.981448	4020.479821	23.054887
109.928289	4030.764103	23.059904
110.151656	4042.488781	23.064922
110.228869	4047.705289	23.069939
110.127325	4035.384783	23.074957
110.353802	4063.659799	23.079975
110.252776	4068.298835	23.084992
110.706940	4078.021241	23.090010
110.650870	4098.949080	23.095027
111.097365	4106.225703	23.100045
110.722054	4102.666244	23.105063
110.855576	4108.410271	23.110080
111.391371	4121.537743	23.115098
111.225344	4133.063820	23.120115
111.736410	4136.184956	23.125133
111.733300	4137.615020	23.130151
111.706353	4155.500107	23.135168
112.263753	4156.999478	23.140186
112.394813	4159.761242	23.145203
112.650215	4163.558671	23.150221
112.602598	4157.769984	23.155239
112.315311	4166.306604	23.160256
112.769657	4156.258279	23.165274
112.740513	4167.401760	23.170291
112.667541	4151.752522	23.175309
112.637516	4159.434576	23.180327
112.444883	4163.311967	23.185344
112.980055	4178.830798	23.190362
113.276640	4183.056725	23.195379
113.624285	4181.215541	23.200397
113.731457	4192.676709	23.205415
114.308651	4176.343383	23.210432
115.186520	4164.845688	23.215450
114.835033	4157.627589	23.220467
115.233782	4141.505255	23.225485
114.810069	4136.453678	23.230503
114.459583	4137.311628	23.235520
114.985925	4128.491472	23.240538
114.882687	4123.529090	23.245555
114.253966	4104.421458	23.250573
114.465773	4118.005368	23.255591
114.909755	4128.624282	23.260608
114.741734	4120.146855	23.265626
114.664854	4136.474704	23.270643
114.836680	4124.631026	23.275661
115.250740	4131.831311	23.280679
114.973650	4158.801113	23.285696
115.277814	4157.622684	23.290714
115.212406	4166.959289	23.295731
115.179523	4164.902954	23.300749
115.533223	4174.835611	23.305767
115.475417	4191.837598	23.310784
115.504379	4195.190258	23.315802
115.202804	4210.980956	23.320819
115.576796	4224.059068	23.325837
115.930707	4236.870479	23.330855
115.628424	4243.502094	23.335872
115.377859	4256.658952	23.340890
115.360822	4268.640821	23.345907
116.104288	4288.940362	23.350925
116.463143	4296.180904	23.355943
116.748781	4315.722513	23.360960
116.983666	4317.044056	23.365978
117.179596	4326.394235	23.370995
117.145953	4333.321661	23.376013
117.031997	4324.933309	23.381031
117.276350	4348.839178	23.386048
117.710834	4354.517521	23.391066
117.792501	4367.859315	23.396083
117.982308	4361.707709	23.401101
118.031772	4354.939827	23.406119
118.066417	4364.550817	23.411136
118.037566	4346.792433	23.416154
118.043816	4357.381005	23.421171
118.299703	4357.739622	23.426189
118.450130	4366.654192	23.431207
118.191242	4375.949266	23.436224
118.066501	4369.672792	23.441242
118.242005	4380.558441	23.446259
118.327212	4394.610878	23.451277
118.779582	4398.930662	23.456295
118.582110	4414.287846	23.461312
119.227704	4432.466726	23.466330
118.897043	4434.766594	23.471347
119.117049	4441.531649	23.476365
119.140898	4453.590925	23.481383
119.154379	4469.531076	23.486400
119.935351	4466.120646	23.491418
120.059457	4480.067248	23.496435
120.153363	4490.373086	23.501453
120.065072	4490.255121	23.506471
119.965764	4505.231678	23.511488
120.420916	4492.394780	23.516506
120.294504	4498.400111	23.521523
120.498916	4519.202721	23.526541
120.613590	4514.828240	23.531559
120.590033	4519.583298	23.536576
120.880689	4525.617167	23.541594
120.945506	4549.943212	23.546611
120.980633	4555.467980	23.551629
121.360101	4557.070359	23.556647
121.186101	4562.278120	23.561664
121.875619	4580.906471	23.566682
121.989154	4590.408769	23.571699
122.102452	4599.629926	23.576717
122.487372	4589.780690	23.581735
122.622332	4589.682735	23.586752
122.667609	4578.229817	23.591770
122.771125	4575.255288	23.596787
122.988652	4574.913976	23.601805
123.355348	4569.497549	23.606823
122.788153	4569.026123	23.611840
122.738314	4570.276779	23.616858
122.764139	4566.235721	23.621875
123.060997	4570.073401	23.626893
123.139211	4569.785115	23.631911
123.102775	4592.133499	23.636928
123.536700	4593.086984	23.641946
123.487512	4603.262262	23.646963
123.405750	4611.155040	23.651981
123.345356	4611.611994	23.656999
123.683083	4626.908348	23.662016
123.845166	4622.006654	23.667034
124.182122	4621.526721	23.672051
124.167593	4632.905104	23.677069
124.584188	4647.170326	23.682087
124.162359	4656.333606	23.687104
125.028735	4655.610894	23.692122
124.910308	4661.343181	23.697139
124.672116	4669.161988	23.702157
125.023852	4658.600068	23.707175
124.846686	4663.802892	23.712192
125.326893	4677.772110	23.717210
125.538654	4680.735945	23.722227
125.448168	4682.340141	23.727245
125.657773	4682.336509	23.732263
126.009309	4686.948548	23.737280
126.017153	4683.932115	23.742298
126.057423	4684.383628	23.747315
125.946412	4684.792551	23.752333
126.622036	4681.016557	23.757351
126.148110	4688.372483	23.762368
126.205419	4702.495350	23.767386
126.281326	4707.623296	23.772403
126.448453	4721.782489	23.777421
126.553511	4716.316350	23.782439
126.584502	4739.619034	23.787456
127.040592	4744.892116	23.792474
126.793133	4750.760765	23.797491
127.098292	4760.417774	23.802509
127.512343	4765.438934	23.807527
127.135586	4788.954158	23.812544
127.794535	4787.588838	23.817562
128.154941	4783.565191	23.822579
128.110025	4780.871269	23.827597
128.078695	4774.699918	23.832615
128.334463	4790.608306	23.837632
128.411497	4801.863992	23.842650
128.836165	4800.077274	23.847667
128.285060	4799.340005	23.852685
128.759290	4796.960355	23.857703
128.582320	4805.696582	23.862720
128.828394	4815.192047	23.867738
129.145691	4820.532270	23.872755
128.791369	4830.513471	23.877773
129.287010	4825.430870	23.882791
129.519536	4848.261230	23.887808
129.571799	4853.883983	23.892826
129.972102	4855.123654	23.897843
129.806994	4852.440873	23.902861
130.413525	4851.852494	23.907879
129.949169	4864.197418	23.912896
129.711291	4859.700547	23.917914
130.007064	4874.792455	23.922931
129.983420	4891.347462	23.927949
130.506441	4885.073943	23.932967
130.445341	4905.621696	23.937984
130.438837	4912.674685	23.943002
131.037233	4913.704754	23.948019
130.599316	4911.088423	23.953037
130.980601	4923.720053	23.958055
131.005430	4941.333286	23.963072
131.242228	4932.113364	23.968090
131.893824	4925.286120	23.973107
131.908053	4933.699782	23.978125
132.363983	4937.158987	23.983143
132.033384	4939.484908	23.988160
132.155663	4958.132185	23.993178
132.555508	4959.277424	23.998195
132.502873	4968.116875	24.003213
132.680406	4955.006624	24.008231
132.816769	4955.354241	24.013248
132.820099	4957.258231	24.018266
133.370196	4957.618411	24.023283
133.172698	4965.314600	24.028301
133.187226	4954.889848	24.033319
133.252081	4968.935257	24.038336
133.341592	4984.472213	24.043354
133.538256	4987.623006	24.048371
133.718038	4993.969860	24.053389
133.908315	4988.412616	24.058407
133.869456	4985.173348	24.063424
133.830785	4989.162384	24.068442
134.458535	4998.494857	24.073459
134.175874	5013.396992	24.078477
134.480609	5020.039861	24.083495
134.563534	5024.453088	24.088512
134.669523	5026.056717	24.093530
134.623956	5037.617147	24.098547
134.591430	5062.672712	24.103565
135.143699	5062.947455	24.108583
134.805423	5066.505825	24.113600
134.878743	5080.835802	24.118618
134.999366	5082.811068	24.123635
134.827911	5088.937767	24.128653
135.299047	5109.819091	24.133671
135.707010	5123.135513	24.138688
135.926592	5125.300975	24.143706
136.533781	5130.625476	24.148723
136.788160	5133.949143	24.153741
137.261965	5138.004742	24.158759
137.167992	5133.531957	24.163776
137.021777	5131.791875	24.168794
137.741890	5125.906662	24.173811
137.593122	5121.317248	24.178829
137.903420	5092.678956	24.183847
137.697020	5089.714928	24.188864
137.518689	5090.267729	24.193882
137.482692	5091.803550	24.198899
137.523169	5110.971499	24.203917
137.867370	5117.141347	24.208935
138.001437	5126.089083	24.213952
137.937487	5125.050885	24.218970
138.231113	5127.270606	24.223987
138.206663	5141.209389	24.229005
137.694514	5142.317225	24.234023
137.983340	5155.966015	24.239040
137.998518	5170.777853	24.244058
138.738678	5183.128409	24.249075
138.201033	5187.849711	24.254093
138.900931	5206.525859	24.259111
139.290309	5202.928784	24.264128
139.292278	5213.929825	24.269146
139.385575	5209.346935	24.274163
139.336330	5220.722238	24.279181
139.821813	5234.435841	24.284199
140.321145	5229.245358	24.289216
140.231293	5220.125378	24.294234
141.056504	5222.580863	24.299251
141.232600	5219.335417	24.304269
141.004337	5217.992985	24.309287
141.144814	5212.116530	24.314304
141.319111	5216.073839	24.319322
141.965171	5220.089690	24.324339
141.370164	5199.469711	24.329357
141.411381	5184.901035	24.334375
142.056913	5195.472729	24.339392
141.765689	5191.193640	24.344410
141.983507	5185.651297	24.349427
141.806475	5200.378753	24.354445
141.865745	5210.260143	24.359463
142.175177	5213.004117	24.364480
141.671848	5215.440030	24.369498
141.745639	5221.547579	24.374515
142.218479	5244.353853	24.379533
142.130560	5240.136781	24.384551
142.105386	5252.613870	24.389568
142.051041	5273.794230	24.394586
142.707827	5272.914450	24.399603
142.365547	5295.146906	24.404621
142.301877	5304.714670	24.409639
142.638486	5323.842349	24.414656
142.970124	5350.182860	24.419674
142.842608	5352.399194	24.424691
143.344774	5377.624312	24.429709
143.116528	5384.245281	24.434727
143.479581	5400.722710	24.439744
143.726342	5414.965756	24.444762
144.119385	5431.734243	24.449779
143.932419	5444.561380	24.454797
144.132906	5451.212064	24.459815
144.636897	5461.365525	24.464832
144.785159	5478.554900	24.469850
144.914944	5476.250744	24.474867
144.905535	5493.461652	24.479885
145.514464	5502.432954	24.484903
145.477074	5497.443098	24.489920
145.513140	5512.584864	24.494938
145.431565	5516.022920	24.499955
145.597821	5534.728713	24.504973
145.961868	5532.280415	24.509991
146.374084	5531.358269	24.515008
146.151209	5541.507998	24.520026
146.418441	5549.203566	24.525043
146.778961	5555.459798	24.530061
146.950702	5556.263736	24.535079
147.357565	5558.019851	24.540096
147.140462	5560.541440	24.545114
147.364775	5554.603226	24.550131
148.046357	5532.814013	24.555149
148.241121	5525.599312	24.560167
148.705938	5517.419090	24.565184
148.848725	5523.720512	24.570202
149.038422	5514.271237	24.575219
149.089629	5506.154050	24.580237
149.226085	5493.907397	24.585255
149.053780	5475.878536	24.590272
148.715671	5478.023077	24.595290
149.190079	5483.133371	24.600307
148.863382	5475.501608	24.605325
148.873310	5479.721890	24.610343
149.210601	5487.282540	24.615360
149.052551	5503.457933	24.620378
149.215319	5508.106515	24.625395
149.341805	5509.208077	24.630413
149.293202	5526.962941	24.635431
149.603868	5541.608679	24.640448
149.514816	5555.892092	24.645466
149.483485	5560.427454	24.650483
149.796413	5578.682806	24.655501
149.826930	5585.284704	24.660519
150.270597	5605.319902	24.665536
150.405159	5611.933118	24.670554
150.372071	5627.925738	24.675571
150.333340	5645.272594	24.680589
150.494039	5656.255394	24.685607
150.534340	5678.254230	24.690624
150.426207	5699.382149	24.695642
150.764128	5701.837756	24.700659
151.192016	5722.439007	24.705677
151.192763	5745.367107	24.710695
151.965253	5740.001239	24.715712
151.636313	5761.022945	24.720730
151.764337	5774.666751	24.725747
151.917761	5782.445748	24.730765
152.248237	5806.258707	24.735783
152.342041	5804.755460	24.740800
152.474279	5823.848672	24.745818
152.912431	5825.866484	24.750835
153.036118	5828.655013	24.755853
153.304134	5854.207752	24.760871
153.339325	5868.440213	24.765888
153.499975	5876.466142	24.770906
153.787353	5877.800877	24.775923
154.436292	5885.682450	24.780941
154.285319	5902.960605	24.785959
154.469602	5899.323705	24.790976
154.810886	5906.449059	24.795994
154.689931	5897.592389	24.801011
154.903455	5895.543212	24.806029
154.774885	5901.421045	24.811047
155.069320	5896.382843	24.816064
155.144249	5903.973704	24.821082
154.905714	5919.285814	24.826099
155.158412	5933.833148	24.831117
155.429909	5940.846812	24.836135
155.855437	5950.491004	24.841152
155.940926	5966.545557	24.846170
156.101439	5965.668901	24.851187
155.920663	5967.338329	24.856205
155.983762	5983.258889	24.861223
155.964135	5991.966428	24.866240
156.382162	5997.786827	24.871258
156.692847	6010.506261	24.876275
157.116819	6019.315791	24.881293
156.922209	6017.639046	24.886311
157.602323	6016.040782	24.891328
157.452233	6029.418188	24.896346
157.949236	6043.505469	24.901363
158.067849	6049.830149	24.906381
157.969700	6049.268016	24.911399
157.811643	6049.930803	24.916416
158.176181	6061.170391	24.921434
158.121388	6068.472423	24.926451
158.404524	6072.887066	24.931469
158.112240	6086.800909	24.936487
158.492372	6098.718434	24.941504
158.460289	6111.747204	24.946522
158.512545	6121.712285	24.951539
159.128084	6133.695821	24.956557
158.958113	6158.326099	24.961575
159.300971	6170.276062	24.966592
159.426717	6181.146271	24.971610
159.799497	6176.864151	24.976627
159.860533	6204.228448	24.981645
159.784751	6209.591629	24.986663
160.617391	6211.170850	24.991680
160.345010	6239.855079	24.996698
160.568257	6235.077107	25.001715
160.429897	6233.716812	25.006733
161.001324	6258.660481	25.011751
161.276671	6264.490472	25.016768
161.554087	6274.383177	25.021786
161.610159	6269.134439	25.026803
162.176502	6274.602610	25.031821
162.098325	6295.426848	25.036839
162.217178	6293.237094	25.041856
161.881509	6299.158452	25.046874
162.246665	6303.559100	25.051891
162.323556	6307.061535	25.056909
162.314403	6319.886461	25.061927
162.643269	6324.264190	25.066944
162.667287	6323.288817	25.071962
162.952611	6344.548645	25.076979
163.069685	6354.010431	25.081997
163.004214	6359.260038	25.087015
163.051411	6370.495955	25.092032
163.612020	6378.103823	25.097050
163.690963	6384.575653	25.102067
164.410330	6382.871373	25.107085
164.089610	6408.193507	25.112103
164.428106	6410.777528	25.117120
164.669007	6421.795946	25.122138
164.736089	6421.292912	25.127155
164.752959	6415.317471	25.132173
164.773107	6426.921208	25.137191
165.530381	6430.153425	25.142208
165.336965	6445.362200	25.147226
165.351286	6445.807184	25.152243
165.838683	6458.653442	25.157261
165.814411	6473.118776	25.162279
165.918110	6475.662709	25.167296
165.903505	6476.600259	25.172314
166.108964	6497.985841	25.177331
166.358176	6502.810527	25.182349
166.708580	6512.145757	25.187367
166.638591	6510.486194	25.192384
167.006753	6530.496116	25.197402
166.859110	6542.392592	25.202419
167.258475	6542.309958	25.207437
167.519487	6563.639628	25.212455
167.667339	6573.007254	25.217472
167.644223	6572.926150	25.222490
167.547432	6575.415455	25.227507
168.460956	6596.503334	25.232525
168.454252	6607.375271	25.237543
168.788440	6599.710019	25.242560
169.143753	6601.136366	25.247578
168.367020	6605.925846	25.252595
168.649687	6621.313126	25.257613
168.810093	6635.808391	25.262631
169.093727	6644.773880	25.267648
169.074255	6655.642524	25.272666
169.398350	6663.271381	25.277683
169.376408	6674.845490	25.282701
169.375204	6690.497342	25.287719
169.946406	6697.918429	25.292736
170.086589	6721.948136	25.297754
169.851540	6724.750267	25.302771
170.143719	6740.441677	25.307789
170.383465	6752.582270	25.312807
170.389707	6763.508811	25.317824
170.614100	6783.401115	25.322842
171.011670	6796.605715	25.327859
171.315950	6804.360138	25.332877
171.483567	6816.568288	25.337895
172.117437	6809.647189	25.342912
172.432285	6798.671892	25.347930
172.454356	6804.327294	25.352947
172.618244	6802.996274	25.357965
172.832244	6816.092141	25.362983
173.166820	6827.681654	25.368000
173.689852	6823.192425	25.373018
173.955914	6810.179700	25.378035
173.891842	6799.070060	25.383053
174.141693	6797.828286	25.388071
173.916557	6798.556168	25.393088
174.290806	6782.340845	25.398106
174.159132	6790.503213	25.403123
174.338633	6789.666585	25.408141
174.030673	6793.068887	25.413159
174.316042	6812.852306	25.418176
174.368260	6822.404264	25.423194
174.457945	6826.520639	25.428211
174.754210	6850.905842	25.433229
174.389823	6861.762856	25.438247
174.685532	6865.721034	25.443264
175.224773	6889.610899	25.448282
175.094100	6898.972896	25.453299
175.264903	6905.880572	25.458317
175.674461	6910.373823	25.463335
176.658312	6901.574556	25.468352
177.507794	6901.109901	25.473370
177.303319	6904.110062	25.478387
177.104606	6887.984977	25.483405
177.370259	6889.193546	25.488423
177.158397	6881.476034	25.493440
177.745647	6880.455279	25.498458
177.876322	6887.236697	25.503475
177.671692	6878.316626	25.508493
177.808845	6893.673973	25.513511
177.800231	6901.523045	25.518528
178.039173	6917.616845	25.523546
178.231566	6911.806491	25.528563
178.369984	6910.694885	25.533581
178.757045	6932.654913	25.538599
178.902165	6943.457725	25.543616
178.996051	6937.534270	25.548634
178.998407	6937.718997	25.553651
179.376196	6956.777774	25.558669
179.756706	6974.912069	25.563687
179.652203	6977.562673	25.568704
179.683687	6967.036805	25.573722
179.299998	6985.854333	25.578739
179.872405	6998.856612	25.583757
179.867346	7014.593732	25.588775
180.286357	7033.408419	25.593792
180.436578	7042.241814	25.598810
180.435326	7053.489668	25.603827
180.846483	7067.253838	25.608845
181.149763	7077.989453	25.613863
181.100007	7069.813156	25.618880
181.616301	7090.601904	25.623898
181.069127	7115.632327	25.628915
181.470203	7108.210604	25.633933
181.882329	7122.110151	25.638951
181.851818	7130.193115	25.643968
182.158696	7133.400283	25.648986
182.175224	7151.933551	25.654003
182.119370	7161.631067	25.659021
182.328938	7170.425212	25.664039
182.622477	7192.405568	25.669056
182.814524	7203.599909	25.674074
182.897757	7226.134714	25.679092
182.987602	7232.895705	25.684109
183.332683	7245.232102	25.689127
183.607149	7270.685171	25.694144
184.123561	7268.917127	25.699162
183.998343	7298.630483	25.704180
184.484004	7297.879207	25.709197
184.278505	7305.455785	25.714215
184.732031	7326.206758	25.719232
185.183866	7320.094970	25.724250
185.467414	7336.271350	25.729268
185.656095	7345.052629	25.734285
186.156906	7344.703670	25.739303
186.417233	7352.084613	25.744320
186.710698	7338.843036	25.749338
186.676430	7344.780857	25.754356
186.721448	7339.659707	25.759373
186.961241	7344.568194	25.764391
187.134022	7352.495104	25.769408
187.340578	7354.668624	25.774426
187.084958	7359.975575	25.779444
187.065367	7367.985100	25.784461
187.290394	7375.275997	25.789479
187.128724	7397.045554	25.794496
187.606368	7403.336010	25.799514
187.265090	7422.799057	25.804532
187.551943	7429.014304	25.809549
188.016064	7458.674984	25.814567
188.142717	7472.681281	25.819584
188.405216	7486.212116	25.824602
188.468849	7506.944294	25.829620
188.456765	7517.011868	25.834637
189.062691	7539.891580	25.839655
188.860674	7553.539915	25.844672
189.849081	7565.461407	25.849690
190.082602	7571.722877	25.854708
189.818093	7585.374862	25.859725
189.907455	7595.431398	25.864743
190.436033	7615.883916	25.869760
190.552341	7620.138522	25.874778
190.534526	7632.012761	25.879796
190.972773	7631.639072	25.884813
190.975345	7645.410759	25.889831
191.288082	7671.273069	25.894848
191.096609	7669.901270	25.899866
191.664333	7677.587326	25.904884
191.469825	7696.965671	25.909901
191.650604	7694.861224	25.914919
191.860723	7716.914108	25.919936
192.356895	7723.780543	25.924954
192.392645	7737.981483	25.929972
192.902511	7746.812701	25.934989
193.219417	7762.685221	25.940007
193.128136	7771.839297	25.945024
193.503138	7778.056901	25.950042
193.493680	7791.182420	25.955060
194.054748	7790.413471	25.960077
194.422800	7777.896913	25.965095
194.263819	7793.182202	25.970112
194.930584	7804.521684	25.975130
194.931721	7814.869211	25.980148
194.965132	7813.103553	25.985165
195.073820	7809.396465	25.990183
194.962057	7818.234233	25.995200
195.902421	7822.873092	26.000218
195.589522	7837.218181	26.005236
195.882868	7844.333718	26.010253
196.205690	7836.217634	26.015271
196.376795	7844.620119	26.020288
196.394696	7856.597117	26.025306
196.272651	7867.096568	26.030324
196.250793	7873.741477	26.035341
197.080237	7885.714095	26.040359
196.516632	7907.257817	26.045376
197.042530	7912.768947	26.050394
197.512317	7923.809040	26.055412
197.201233	7939.558560	26.060429
197.594981	7961.530672	26.065447
197.818795	7975.319862	26.070464
198.215516	7979.674603	26.075482
198.407903	7992.300092	26.080500
199.047536	7982.557166	26.085517
199.454655	7975.160009	26.090535
199.325450	7982.110125	26.095552
199.356990	7997.735582	26.100570
199.757655	8010.353743	26.105588
199.862612	8017.422871	26.110605
200.328536	8012.576778	26.115623
200.293883	8019.572939	26.120640
200.473198	8027.218604	26.125658
201.038273	8039.125576	26.130676
200.933336	8043.852303	26.135693
201.392131	8037.816259	26.140711
201.199029	8040.974604	26.145728
201.021975	8049.247016	26.150746
201.326766	8059.188921	26.155764
201.586495	8066.232327	26.160781
202.022596	8066.914664	26.165799
202.249924	8072.030342	26.170816
202.398773	8081.693323	26.175834
203.239188	8078.209740	26.180852
203.066997	8080.230061	26.185869
203.384556	8066.673360	26.190887
203.215227	8081.952032	26.195904
203.219038	8076.893646	26.200922
203.077380	8089.912082	26.205940
203.302274	8114.873155	26.210957
203.826310	8108.361879	26.215975
203.453135	8128.923153	26.220992
203.696489	8134.870398	26.226010
203.901099	8153.617590	26.231028
203.633737	8172.841192	26.236045
204.472336	8184.112887	26.241063
204.219468	8206.324592	26.246080
204.128800	8227.496178	26.251098
204.476113	8248.833785	26.256116
204.589200	8269.179528	26.261133
205.207755	8290.767702	26.266151
205.399484	8320.078033	26.271168
206.037331	8329.554922	26.276186
206.278215	8343.090187	26.281204
206.034591	8366.007204	26.286221
206.473925	8365.326853	26.291239
206.833451	8384.640990	26.296256
207.391160	8401.025130	26.301274
207.983471	8404.170235	26.306292
208.060471	8414.099413	26.311309
208.407753	8411.344736	26.316327
208.581998	8431.961455	26.321344
209.101768	8437.378492	26.326362
208.998333	8440.142598	26.331380
208.563410	8450.755149	26.336397
209.139681	8447.180476	26.341415
209.042090	8448.608214	26.346432
209.009606	8464.631922	26.351450
209.297731	8473.295931	26.356468
209.466536	8492.720887	26.361485
209.682927	8505.465567	26.366503
209.533335	8517.702603	26.371520
209.532147	8534.773559	26.376538
209.930555	8556.287957	26.381556
209.714174	8583.665265	26.386573
210.348725	8593.523401	26.391591
210.454513	8618.857046	26.396608
210.469702	8630.789391	26.401626
211.216086	8655.151390	26.406644
210.952237	8675.271547	26.411661
211.298491	8690.398598	26.416679
211.613306	8711.413073	26.421696
212.449695	8721.617216	26.426714
212.490694	8729.632001	26.431732
212.802872	8756.886697	26.436749
213.470730	8758.683530	26.441767
213.569048	8760.629991	26.446784
213.416385	8757.679696	26.451802
213.944309	8767.079572	26.456820
214.057846	8788.355549	26.461837
214.682729	8792.572134	26.466855
214.642742	8786.692220	26.471872
214.512804	8789.777643	26.476890
215.051831	8790.997802	26.481908
214.970726	8800.872384	26.486925
215.393091	8811.221614	26.491943
215.708377	8814.898816	26.496960
215.631317	8813.203983	26.501978
216.318542	8809.829234	26.506996
216.325760	8815.763637	26.512013
216.092515	8827.572478	26.517031
216.379604	8843.743471	26.522048
216.710882	8851.985880	26.527066
216.854115	8850.984405	26.532084
216.841645	8876.671988	26.537101
217.152904	8874.299213	26.542119
217.409845	8901.760585	26.547136
217.235102	8900.747434	26.552154
217.443153	8919.267240	26.557172
217.445213	8941.495344	26.562189
218.156052	8954.177682	26.567207
217.999398	8970.544621	26.572224
218.374707	8991.898900	26.577242
218.960259	8998.626085	26.582260
218.985110	9016.874870	26.587277
219.128302	9025.855529	26.592295
219.132087	9048.828797	26.597312
219.050996	9073.395516	26.602330
219.814059	9080.542963	26.607348
219.734828	9101.170110	26.612365
220.180585	9111.287045	26.617383
220.748216	9140.219287	26.622400
220.751944	9144.083908	26.627418
220.807584	9154.872821	26.632436
221.125583	9175.731359	26.637453
221.937563	9189.077261	26.642471
222.172926	9189.898848	26.647488
222.308048	9202.312927	26.652506
222.324878	9193.364634	26.657524
222.703789	9225.112116	26.662541
222.966619	9228.788952	26.667559
223.416822	9232.982024	26.672576
223.576901	9225.179928	26.677594
223.443018	9237.271423	26.682612
223.579416	9256.713097	26.687629
223.747910	9259.195945	26.692647
223.955162	9269.500407	26.697664
223.573077	9284.940380	26.702682
224.138765	9298.117443	26.707700
224.198212	9331.293940	26.712717
224.336752	9342.212160	26.717735
224.391534	9355.423272	26.722752
224.540612	9380.448938	26.727770
224.884730	9403.813459	26.732788
225.093791	9426.577168	26.737805
226.089927	9417.514459	26.742823
226.772084	9420.282735	26.747840
226.915211	9435.130156	26.752858
227.547809	9436.688874	26.757876
227.324216	9439.769989	26.762893
227.563187	9438.974248	26.767911
227.979919	9436.632163	26.772928
227.546513	9432.716658	26.777946
227.884900	9432.460117	26.782964
228.101669	9449.789344	26.787981
228.288444	9460.734044	26.792999
228.462949	9462.275167	26.798016
228.419418	9484.155712	26.803034
229.114006	9496.258237	26.808052
228.630363	9509.746133	26.813069
228.944942	9521.411148	26.818087
229.008105	9545.922342	26.823104
229.163464	9567.356055	26.828122
229.646716	9575.889515	26.833140
229.785097	9592.654027	26.838157
229.956797	9620.364446	26.843175
230.196683	9634.985887	26.848192
230.175068	9662.371815	26.853210
230.680479	9670.290126	26.858228
230.883078	9698.376720	26.863245
231.247983	9711.542842	26.868263
231.684662	9725.063829	26.873280
231.696890	9746.764986	26.878298
231.954319	9756.405632	26.883316
232.074721	9776.417954	26.888333
232.477541	9802.050001	26.893351
233.132235	9810.954449	26.898368
233.027099	9834.349328	26.903386
233.174839	9838.217793	26.908404
233.759503	9867.326485	26.913421
233.705497	9867.643031	26.918439
234.504448	9874.267825	26.923456
234.531507	9899.255328	26.928474
234.933177	9898.003061	26.933492
235.104864	9900.945595	26.938509
234.840296	9917.941821	26.943527
235.198030	9925.189069	26.948544
235.507306	9954.187543	26.953562
235.926757	9954.153471	26.958580
235.923944	9965.690420	26.963597
236.456030	9978.812346	26.968615
237.029277	9986.842099	26.973632
236.837417	9996.536266	26.978650
237.248887	10003.320506	26.983668
237.414848	10019.100579	26.988685
237.400022	10020.842822	26.993703
237.557413	10027.213640	26.998720
237.614356	10049.796294	27.003738
237.644673	10063.128787	27.008756
237.937660	10079.058908	27.013773
238.031278	10092.947869	27.018791
238.320491	10101.800093	27.023808
238.751076	10126.980363	27.028826
238.907868	10138.260007	27.033844
238.866744	10152.971056	27.038861
239.046837	10175.178215	27.043879
239.320241	10186.548211	27.048896
239.478376	10219.950712	27.053914
240.062908	10231.054672	27.058932
240.559987	10246.204606	27.063949
240.838632	10253.476590	27.068967
240.948921	10277.463938	27.073984
241.045832	10295.005291	27.079002
241.517161	10305.178477	27.084020
242.267547	10303.533906	27.089037
242.659560	10305.581492	27.094055
243.266025	10316.428041	27.099072
242.673916	10334.375922	27.104090
243.505872	10333.453283	27.109108
243.120637	10331.202841	27.114125
243.371877	10344.168346	27.119143
243.744244	10359.829850	27.124160
243.696129	10367.214627	27.129178
243.864293	10384.466515	27.134196
243.998248	10400.597556	27.139213
243.981824	10423.478533	27.144231
244.344910	10430.006505	27.149248
244.581928	10464.844195	27.154266
244.676774	10474.798368	27.159284
244.642731	10495.416389	27.164301
245.191667	10532.005111	27.169319
245.594688	10538.663381	27.174336
246.028440	10562.436543	27.179354
246.251100	10569.756087	27.184372
246.573748	10592.445233	27.189389
246.581957	10609.360754	27.194407
247.112203	10627.241065	27.199424
247.102218	10639.406917	27.204442
247.576793	10652.047578	27.209460
247.963684	10672.275345	27.214477
247.783979	10698.891151	27.219495
247.937404	10697.525367	27.224512
248.056681	10717.822701	27.229530
248.463782	10740.867910	27.234548
248.996699	10764.630673	27.239565
249.297358	10780.487679	27.244583
249.875858	10783.505623	27.249600
250.122365	10793.259073	27.254618
250.484719	10804.916827	27.259636
250.752296	10822.744673	27.264653
251.143324	10827.755165	27.269671
251.482118	10823.916547	27.274688
251.251100	10823.960882	27.279706
251.720850	10846.650383	27.284724
252.126322	10853.138168	27.289741
251.744665	10855.515427	27.294759
252.488167	10858.448372	27.299776
252.628196	10875.787551	27.304794
253.199465	10882.418701	27.309812
253.081361	10886.889276	27.314829
252.702828	10897.968092	27.319847
253.488507	10909.000220	27.324864
253.305982	10920.042302	27.329882
253.590853	10937.114031	27.334900
253.611743	10943.935676	27.339917
253.692335	10982.854502	27.344935
254.083401	10990.058695	27.349952
255.026828	11011.519977	27.354970
256.646084	10978.413199	27.359988
257.099732	10972.244587	27.365005
257.013205	10972.544665	27.370023
257.696715	10968.653230	27.375040
257.995408	10960.312800	27.380058
257.716294	10943.298384	27.385076
258.041117	10934.567394	27.390093
258.128878	10932.388651	27.395111
258.072403	10923.795515	27.400128
258.270527	10931.035906	27.405146
258.025293	10931.806015	27.410164
258.380632	10931.879067	27.415181
258.700819	10953.053127	27.420199
258.907420	10959.770455	27.425216
258.672080	10964.428192	27.430234
258.798608	10987.830723	27.435252
258.798726	10992.367738	27.440269
258.670603	11022.732187	27.445287
259.123505	11037.540585	27.450304
259.303426	11065.324555	27.455322
259.127062	11083.022340	27.460340
259.139079	11104.889241	27.465357
259.424419	11147.505131	27.470375
259.728533	11169.676633	27.475392
260.053639	11217.001044	27.480410
260.020284	11238.335359	27.485428
261.135134	11268.433627	27.490445
261.169585	11306.551107	27.495463
261.580219	11326.532926	27.500480
261.759764	11349.290210	27.505498
262.125196	11368.643150	27.510516
262.754989	11402.011360	27.515533
262.673287	11435.158038	27.520551
263.181294	11445.691277	27.525568
263.814529	11465.371929	27.530586
264.062650	11487.752030	27.535604
264.518193	11495.862602	27.540621
264.383305	11515.670249	27.545639
264.444642	11526.492857	27.550656
264.639277	11549.592967	27.555674
264.652699	11564.852254	27.560692
265.201696	11574.410912	27.565709
265.495598	11605.191076	27.570727
265.981073	11614.997041	27.575744
266.268034	11625.095497	27.580762
266.632649	11643.460774	27.585780
267.046152	11648.236004	27.590797
267.091810	11662.656171	27.595815
267.622818	11678.201927	27.600832
267.762448	11692.965334	27.605850
267.843611	11705.272379	27.610868
268.633843	11724.874429	27.615885
268.433092	11750.226896	27.620903
268.698929	11748.495043	27.625920
268.652757	11765.885998	27.630938
269.094919	11780.529861	27.635956
269.872819	11789.384348	27.640973
269.747583	11800.962493	27.645991
270.059692	11816.490743	27.651008
270.525884	11836.492034	27.656026
270.767128	11865.626931	27.661044
270.818382	11868.530581	27.666061
271.011544	11885.232908	27.671079
271.201325	11900.339353	27.676096
271.252222	11937.224635	27.681114
271.587646	11958.392662	27.686132
271.685175	11971.026486	27.691149
272.257364	12003.405043	27.696167
272.593611	12009.889399	27.701184
272.777458	12037.348119	27.706202
272.957228	12054.825157	27.711220
273.509601	12066.511136	27.716237
273.751756	12098.434249	27.721255
273.728061	12107.689503	27.726272
274.263713	12138.632541	27.731290
274.297078	12166.081021	27.736308
274.674321	12168.861079	27.741325
274.965244	12190.260829	27.746343
275.600595	12210.323417	27.751360
275.673781	12222.082188	27.756378
275.985529	12246.974060	27.761396
276.358172	12254.169367	27.766413
276.342994	12280.601944	27.771431
276.698408	12300.621216	27.776448
277.109622	12317.704258	27.781466
276.599388	12339.273045	27.786484
277.560069	12372.228767	27.791501
277.831029	12382.919873	27.796519
278.311372	12406.315799	27.801536
278.352021	12420.650810	27.806554
278.427997	12447.865509	27.811572
278.628856	12458.201462	27.816589
278.736454	12487.108205	27.821607
278.895962	12503.931984	27.826624
279.612164	12522.329399	27.831642
279.844944	12543.189535	27.836660
280.377608	12562.529413	27.841677
280.652209	12587.713437	27.846695
280.884488	12587.090491	27.851712
281.251467	12603.363440	27.856730
281.736851	12621.538905	27.861748
282.325793	12622.826476	27.866765
282.324615	12650.130386	27.871783
282.712935	12653.917311	27.876800
283.402864	12660.940210	27.881818
283.378802	12680.191253	27.886836
283.943534	12678.163783	27.891853
284.153328	12688.734761	27.896871
284.502843	12675.150635	27.901888
284.411798	12678.435010	27.906906
284.748951	12699.425606	27.911924
285.277570	12695.634401	27.916941
284.965363	12704.846455	27.921959
285.368075	12726.840837	27.926976
285.775756	12726.105866	27.931994
285.607776	12759.225881	27.937012
285.817126	12767.910425	27.942029
286.185308	12800.300313	27.947047
286.073670	12810.461520	27.952064
286.599329	12835.965393	27.957082
286.877289	12869.997398	27.962100
286.875936	12874.844099	27.967117
287.111416	12914.990809	27.972135
286.969493	12945.113738	27.977152
287.605954	12964.204616	27.982170
287.732974	13001.942944	27.987188
287.849128	13030.379502	27.992205
288.204767	13068.498040	27.997223
288.761562	13101.245490	28.002240
289.343222	13126.246894	28.007258
289.198162	13154.559795	28.012276
289.947197	13170.646463	28.017293
290.333890	13195.646716	28.022311
290.605445	13227.552804	28.027328
291.080537	13234.478806	28.032346
291.202335	13261.088073	28.037364
291.775271	13270.676728	28.042381
292.313729	13284.657651	28.047399
292.640761	13306.125172	28.052416
292.799645	13325.035116	28.057434
292.777262	13346.062946	28.062452
293.171199	13353.537218	28.067469
293.784860	13378.245090	28.072487
293.384256	13388.702059	28.077504
293.961957	13417.006587	28.082522
294.012672	13434.980058	28.087540
294.572801	13460.144853	28.092557
295.146822	13483.149565	28.097575
295.114875	13494.821665	28.102592
295.648367	13500.661265	28.107610
296.355041	13502.078467	28.112628
297.225257	13496.239438	28.117645
297.749052	13485.573742	28.122663
297.686689	13487.798921	28.127680
298.321991	13478.622487	28.132698
298.306173	13492.422767	28.137716
298.321042	13491.893795	28.142733
298.463119	13496.270046	28.147751
298.510882	13511.515802	28.152768
298.933305	13526.902254	28.157786
299.002836	13538.452966	28.162804
299.425598	13561.009294	28.167821
299.383822	13563.248292	28.172839
299.279748	13596.983193	28.177856
299.552753	13601.589216	28.182874
299.814736	13631.057841	28.187892
299.829161	13661.609216	28.192909
299.919671	13688.746247	28.197927
299.980000	13723.203481	28.202944
300.617213	13754.193635	28.207962
300.378156	13790.801781	28.212980
300.938751	13818.495227	28.217997
301.361552	13853.322477	28.223015
301.447929	13888.483295	28.228032
301.747139	13911.324501	28.233050
301.855845	13952.182686	28.238068
302.377657	13991.114989	28.243085
303.214353	14018.028518	28.248103
303.568331	14056.316706	28.253120
304.453663	14066.362974	28.258138
304.570324	14097.411473	28.263156
305.182545	14121.646275	28.268173
305.546906	14129.646119	28.273191
305.608664	14159.220936	28.278208
305.774676	14172.473622	28.283226
305.860625	14195.323403	28.288244
306.125571	14215.516564	28.293261
306.657912	14240.118304	28.298279
306.343180	14275.181615	28.303296
307.297791	14288.151066	28.308314
307.560786	14324.909200	28.313332
307.500386	14345.120454	28.318349
307.808485	14369.874310	28.323367
307.840704	14406.435746	28.328384
308.291638	14430.035053	28.333402
308.567112	14467.253201	28.338420
308.733400	14504.739193	28.343437
309.259261	14530.368609	28.348455
309.345792	14556.180550	28.353472
309.823158	14587.270600	28.358490
309.805240	14625.538732	28.363508
310.346829	14654.551435	28.368525
310.921901	14681.168844	28.373543
311.478609	14704.884397	28.378560
312.395252	14721.169269	28.383578
312.660128	14735.404812	28.388596
313.079038	14742.244933	28.393613
313.252344	14763.502687	28.398631
313.327314	14774.025606	28.403648
313.807314	14786.737903	28.408666
313.844000	14807.413843	28.413684
313.971093	14825.869109	28.418701
314.653637	14848.440995	28.423719
314.829740	14863.382271	28.428736
315.212644	14869.087395	28.433754
315.703037	14890.549474	28.438772
315.704573	14908.624401	28.443789
316.204823	14924.757013	28.448807
316.176340	14951.183540	28.453824
316.154858	14972.604203	28.458842
316.417683	15000.358553	28.463860
316.827801	15019.093393	28.468877
317.302205	15039.180728	28.473895
317.825579	15068.619728	28.478912
317.807769	15095.039926	28.483930
318.193106	15120.757396	28.488948
318.830493	15148.233419	28.493965
319.375908	15175.815100	28.498983
319.368372	15195.792919	28.504000
319.579399	15214.647225	28.509018
319.885736	15238.906147	28.514036
320.221168	15262.777074	28.519053
320.551860	15277.025448	28.524071
321.210476	15310.122391	28.529088
322.124492	15315.104538	28.534106
322.702039	15331.151788	28.539124
322.970319	15347.297774	28.544141
323.226888	15356.377555	28.549159
323.479312	15361.495177	28.554176
324.304876	15356.780780	28.559194
324.886387	15358.829647	28.564212
324.768916	15365.147197	28.569229
324.848014	15356.299940	28.574247
325.184671	15365.845202	28.579264
325.426964	15384.716411	28.584282
325.550852	15390.757731	28.589300
325.991485	15404.586986	28.594317
326.166987	15420.458901	28.599335
325.938871	15434.037091	28.604352
326.366341	15448.447152	28.609370
326.570957	15475.748835	28.614388
326.941377	15494.806286	28.619405
327.042579	15518.095075	28.624423
327.655083	15547.309998	28.629440
327.569952	15574.891650	28.634458
327.848098	15588.105760	28.639476
327.622571	15619.206302	28.644493
328.152222	15650.869487	28.649511
328.500855	15690.940498	28.654528
329.042158	15707.514523	28.659546
329.107742	15739.314164	28.664564
329.340751	15771.621133	28.669581
330.021584	15793.519924	28.674599
330.086180	15829.697467	28.679616
330.534523	15855.074242	28.684634
331.420181	15873.646576	28.689652
331.207174	15898.577156	28.694669
331.537840	15927.303510	28.699687
331.616264	15958.217022	28.704704
332.041001	15979.510483	28.709722
332.507789	16008.642424	28.714740
332.190890	16040.839235	28.719757
332.835099	16067.664569	28.724775
333.284233	16105.461964	28.729792
333.714362	16137.160475	28.734810
334.069712	16165.310778	28.739828
334.878081	16195.850553	28.744845
335.594994	16209.538545	28.749863
335.935725	16242.557839	28.754880
335.933264	16259.488874	28.759898
336.760244	16281.052709	28.764916
336.883533	16301.460286	28.769933
337.293891	16318.949616	28.774951
337.515493	16340.226334	28.779968
337.677266	16361.071938	28.784986
338.160407	16383.538220	28.790004
338.053056	16418.688736	28.795021
338.374944	16438.007815	28.800039
338.491870	16479.263344	28.805056
338.722664	16514.947267	28.810074
339.235545	16537.660890	28.815092
338.968969	16582.272419	28.820109
339.802730	16608.954212	28.825127
339.691422	16648.017036	28.830144
339.896467	16686.702559	28.835162
340.498117	16719.630786	28.840180
340.916997	16759.118500	28.845197
341.370183	16783.926762	28.850215
341.501041	16827.288485	28.855232
342.256854	16863.400249	28.860250
342.866834	16887.242220	28.865268
342.937937	16926.056877	28.870285
343.768954	16957.726076	28.875303
344.387202	16977.854167	28.880320
344.309462	16996.148312	28.885338
345.017340	17021.666833	28.890356
345.174428	17044.180431	28.895373
346.161231	17052.735561	28.900391
346.738797	17064.400294	28.905408
346.994920	17084.298928	28.910426
347.784719	17081.120959	28.915444
348.001710	17087.955676	28.920461
348.481114	17092.598247	28.925479
348.328218	17097.018126	28.930496
349.006593	17111.553738	28.935514
349.159898	17109.548980	28.940532
349.249225	17120.116642	28.945549
349.837364	17131.145862	28.950567
349.991218	17151.043186	28.955584
349.903153	17155.522912	28.960602
350.421729	17164.697511	28.965620
350.270107	17191.035186	28.970637
350.411499	17216.367327	28.975655
350.794582	17243.857300	28.980672
350.824873	17273.758349	28.985690
351.172284	17296.547086	28.990708
351.305315	17331.986234	28.995725
351.729299	17368.107093	29.000743
352.023065	17403.660731	29.005760
352.263969	17431.583698	29.010778
352.865057	17468.314485	29.015796
352.959889	17506.883639	29.020813
353.142838	17543.536485	29.025831
353.814893	17578.084472	29.030848
354.160965	17622.442422	29.035866
354.676718	17654.805477	29.040884
354.657594	17686.577622	29.045901
355.385768	17709.588595	29.050919
355.729435	17751.352308	29.055936
356.190029	17786.931769	29.060954
356.842675	17814.726475	29.065972
356.773531	17844.642430	29.070989
357.059323	17875.963806	29.076007
357.275660	17907.341288	29.081024
358.335889	17929.146340	29.086042
359.102919	17951.581848	29.091060
359.029924	17974.205498	29.096077
359.556773	17997.464209	29.101095
360.093805	18032.673211	29.106112
360.249103	18060.643429	29.111130
360.544671	18077.003376	29.116148
360.678125	18107.172012	29.121165
361.048648	18130.516033	29.126183
361.784724	18158.566608	29.131200
361.620060	18193.926164	29.136218
362.206709	18226.011729	29.141236
362.307283	18248.046309	29.146253
362.905118	18280.317675	29.151271
363.605328	18307.170126	29.156288
363.124112	18347.782307	29.161306
363.848344	18374.741111	29.166324
364.109818	18396.019918	29.171341
364.658570	18437.028102	29.176359
364.900811	18470.639410	29.181376
364.971717	18500.966098	29.186394
365.792640	18526.166411	29.191412
365.569287	18561.907303	29.196429
366.324417	18590.258047	29.201447
366.450429	18616.662313	29.206464
366.873696	18659.374809	29.211482
367.506968	18684.568106	29.216500
367.519935	18722.633789	29.221517
367.974121	18744.759774	29.226535
368.328328	18772.356531	29.231552
368.964023	18805.735529	29.236570
369.167016	18832.541598	29.241588
369.483611	18862.215089	29.246605
370.126547	18890.714855	29.251623
370.637241	18902.482207	29.256640
371.107208	18935.773194	29.261658
371.713377	18957.548620	29.266676
372.029899	18971.649647	29.271693
372.434231	18990.878713	29.276711
373.026052	19012.946777	29.281728
373.088042	19033.574730	29.286746
373.783052	19052.840766	29.291764
373.788523	19081.131619	29.296781
373.800311	19093.126510	29.301799
374.368421	19123.908329	29.306816
374.482103	19160.358990	29.311834
375.072163	19179.982145	29.316852
375.305648	19219.840108	29.321869
375.329100	19255.951685	29.326887
376.068197	19285.927188	29.331904
376.497373	19320.525120	29.336922
376.938645	19344.323828	29.341940
377.072500	19378.072197	29.346957
377.189615	19410.604710	29.351975
377.913596	19435.636955	29.356992
378.375849	19465.278662	29.362010
378.828874	19488.889508	29.367028
379.007777	19522.272531	29.372045
379.427862	19550.803725	29.377063
379.695158	19584.274208	29.382080
380.167255	19620.943516	29.387098
380.431809	19638.555909	29.392116
380.927606	19684.471937	29.397133
381.371490	19718.260879	29.402151
381.751224	19736.367649	29.407168
381.894370	19777.820720	29.412186
382.170465	19821.182616	29.417204
382.128564	19853.041583	29.422221
382.524224	19899.218173	29.427239
383.401592	19932.857569	29.432256
383.595178	19969.622668	29.437274
384.235690	20006.842619	29.442292
384.326231	20050.506527	29.447309
384.605725	20086.003629	29.452327
385.269065	20105.134391	29.457344
385.630198	20152.399252	29.462362
386.375033	20181.758848	29.467380
386.654171	20205.471451	29.472397
387.200122	20240.915329	29.477415
387.541785	20261.484234	29.482432
388.149959	20279.993936	29.487450
388.958165	20306.704930	29.492468
389.496252	20327.814203	29.497485
389.562982	20349.918822	29.502503
390.147834	20363.424727	29.507520
390.020472	20390.425488	29.512538
390.117206	20409.341495	29.517556
390.606464	20435.427755	29.522573
390.939853	20458.136456	29.527591
391.347384	20481.236142	29.532608
391.425698	20512.370913	29.537626
392.271394	20540.588009	29.542644
392.898221	20572.814648	29.547661
392.985749	20589.029780	29.552679
393.918695	20599.552809	29.557696
394.118952	20628.631230	29.562714
394.589182	20657.305495	29.567732
394.569275	20678.416225	29.572749
395.368953	20706.565798	29.577767
395.776720	20717.797021	29.582784
395.937001	20758.289267	29.587802
396.196238	20772.948777	29.592820
396.728222	20805.264647	29.597837
397.129625	20832.386786	29.602855
397.039615	20857.071823	29.607872
397.563892	20900.266222	29.612890
397.917191	20925.337398	29.617908
398.150770	20967.988896	29.622925
398.426728	21004.557629	29.627943
398.595317	21043.516430	29.632960
398.625824	21091.206398	29.637978
399.134160	21124.134018	29.642996
399.589512	21160.481541	29.648013
399.902276	21209.823330	29.653031
400.521044	21248.541455	29.658048
401.148947	21305.288126	29.663066
401.356028	21341.336401	29.668084
401.450894	21379.587970	29.673101
401.906877	21436.446539	29.678119
402.298599	21465.928800	29.683136
402.638980	21524.359137	29.688154
403.233174	21571.021896	29.693172
403.571892	21612.278773	29.698189
404.347402	21643.966316	29.703207
405.407421	21678.717988	29.708224
406.110877	21713.740567	29.713242
406.463071	21744.037465	29.718260
406.955882	21761.933061	29.723277
407.151003	21787.450500	29.728295
407.720989	21807.721958	29.733312
408.268750	21834.125188	29.738330
408.764811	21855.752915	29.743348
409.540846	21874.511558	29.748365
409.155180	21892.989921	29.753383
410.037067	21907.829129	29.758400
410.001370	21936.368330	29.763418
410.446966	21946.866918	29.768436
411.030940	21970.944480	29.773453
410.822677	22004.878121	29.778471
411.563999	22027.563164	29.783488
411.645193	22060.438065	29.788506
412.152166	22095.813646	29.793524
412.595981	22119.590585	29.798541
412.414291	22147.691535	29.803559
412.986128	22180.879976	29.808576
413.540518	22205.114327	29.813594
414.462105	22238.788572	29.818612
414.923070	22272.781522	29.823629
415.097016	22308.618321	29.828647
415.795756	22333.553523	29.833664
415.599631	22353.412867	29.838682
415.936519	22387.553467	29.843700
416.407098	22429.568750	29.848717
416.636335	22460.905146	29.853735
417.565370	22478.997982	29.858752
418.343399	22513.536330	29.863770
418.562193	22540.361316	29.868788
419.386261	22569.050706	29.873805
419.692594	22590.243512	29.878823
420.109460	22616.605731	29.883840
420.397207	22647.222791	29.888858
420.311935	22673.841467	29.893876
421.201254	22699.290189	29.898893
421.139288	22741.684518	29.903911
421.722194	22768.078441	29.908928
422.009248	22807.278017	29.913946
421.890390	22841.541782	29.918964
422.386637	22876.081842	29.923981
422.347289	22922.964105	29.928999
423.249037	22957.144664	29.934016
423.482891	23001.681013	29.939034
424.380794	23045.059677	29.944052
425.245197	23076.742538	29.949069
425.621348	23105.238339	29.954087
425.911746	23136.499254	29.959104
426.818428	23172.363685	29.964122
426.881791	23203.278828	29.969140
427.180356	23229.056674	29.974157
427.516430	23264.148548	29.979175
427.991559	23302.525341	29.984192
428.187712	23336.288221	29.989210
428.401342	23381.529238	29.994228
429.255924	23421.077692	29.999245
429.890542	23460.616620	30.004263
430.075024	23497.491813	30.009280
430.484959	23529.272319	30.014298
431.194388	23557.011532	30.019316
431.418960	23586.802086	30.024333
432.076382	23624.795092	30.029351
432.410040	23640.660251	30.034368
432.888186	23678.491693	30.039386
433.021925	23700.642783	30.044404
433.333827	23725.129021	30.049421
433.518129	23767.890568	30.054439
434.194333	23798.900474	30.059456
434.505503	23838.274906	30.064474
434.947278	23873.242666	30.069492
435.415989	23906.802246	30.074509
435.546945	23941.662544	30.079527
435.752356	23973.586164	30.084544
436.582574	24014.710978	30.089562
437.316497	24055.991179	30.094580
437.717822	24086.430474	30.099597
438.041742	24119.630461	30.104615
438.607136	24157.593102	30.109632
439.039347	24193.455813	30.114650
439.511116	24229.286586	30.119668
440.035847	24261.275881	30.124685
440.116128	24304.529730	30.129703
440.817943	24337.621217	30.134720
441.170462	24376.832078	30.139738
441.372658	24420.686726	30.144756
441.582271	24455.064586	30.149773
442.149257	24498.803296	30.154791
442.912733	24540.994356	30.159808
443.945984	24574.556278	30.164826
444.586225	24606.785078	30.169844
444.943598	24626.479636	30.174861
445.627022	24668.568015	30.179879
446.241548	24688.511934	30.184896
446.743860	24709.812564	30.189914
447.047047	24732.327084	30.194932
447.408164	24751.484898	30.199949
447.633277	24786.737683	30.204967
447.808578	24807.444667	30.209984
448.028144	24850.622388	30.215002
448.471627	24884.021011	30.220020
448.829186	24920.106217	30.225037
449.126102	24965.264563	30.230055
449.408007	25014.904900	30.235072
449.650805	25056.684892	30.240090
449.340177	25104.534359	30.245108
450.105912	25146.877927	30.250125
450.161378	25212.844130	30.255143
450.909131	25267.701723	30.260160
451.233315	25304.869129	30.265178
451.694339	25367.447897	30.270196
452.595941	25408.822473	30.275213
452.892196	25464.123982	30.280231
453.394521	25506.901576	30.285248
454.838586	25551.650360	30.290266
455.240098	25608.464243	30.295284
455.603929	25647.565635	30.300301
456.308924	25684.911499	30.305319
456.393063	25725.379602	30.310336
457.448122	25747.173539	30.315354
457.678122	25788.500074	30.320372
458.159590	25805.234643	30.325389
458.404242	25850.634534	30.330407
458.623553	25885.253319	30.335424
459.138029	25914.935114	30.340442
459.208683	25950.207268	30.345460
459.804279	25985.774401	30.350477
460.029243	26025.446189	30.355495
460.661829	26062.802121	30.360512
461.389541	26107.731885	30.365530
461.470130	26150.220552	30.370548
461.957617	26191.011794	30.375565
461.981138	26240.031125	30.380583
462.123963	26283.216094	30.385600
462.716095	26334.620976	30.390618
463.056690	26393.577269	30.395636
463.553298	26438.178391	30.400653
464.022851	26504.870362	30.405671
464.101490	26553.038819	30.410688
464.925765	26610.439708	30.415706
465.211215	26672.056364	30.420724
466.086231	26735.566009	30.425741
466.958625	26777.586114	30.430759
467.857032	26824.892405	30.435776
468.324582	26871.733190	30.440794
468.353846	26924.709546	30.445812
469.057381	26958.745875	30.450829
469.583127	27005.204781	30.455847
470.033087	27051.629476	30.460864
471.084693	27090.483748	30.465882
471.320500	27132.497068	30.470900
471.981892	27158.635029	30.475917
472.308556	27198.680102	30.480935
472.634362	27240.504743	30.485952
473.346316	27269.984648	30.490970
473.642555	27326.973606	30.495988
474.225322	27363.157793	30.501005
475.564725	27384.611668	30.506023
476.422544	27394.960926	30.511040
477.293557	27407.756109	30.516058
477.256876	27433.449383	30.521076
478.583105	27449.747376	30.526093
478.514863	27462.542652	30.531111
478.923185	27484.780868	30.536128
479.401734	27498.823299	30.541146
479.859284	27536.032557	30.546164
479.747963	27538.960454	30.551181
480.045575	27560.085131	30.556199
480.499088	27606.778859	30.561216
481.188508	27621.908401	30.566234
480.821208	27661.180611	30.571252
481.470089	27703.449476	30.576269
481.711291	27744.201371	30.581287
481.830418	27778.143839	30.586304
482.532806	27819.132374	30.591322
482.617615	27863.097839	30.596340
482.737400	27905.016162	30.601357
483.217972	27951.097263	30.606375
483.439008	28003.823173	30.611392
483.928111	28061.655401	30.616410
483.742158	28123.184419	30.621428
484.267443	28179.707820	30.626445
485.037643	28241.174368	30.631463
485.165333	28312.613862	30.636480
485.613582	28351.766790	30.641498
486.199875	28432.179998	30.646516
486.827795	28494.785548	30.651533
487.658002	28555.712862	30.656551
487.639892	28621.038811	30.661568
488.753073	28673.635938	30.666586
489.223031	28729.899250	30.671604
489.778216	28787.290291	30.676621
490.727566	28847.327387	30.681639
490.728844	28902.185495	30.686656
491.589000	28956.218242	30.691674
492.070194	29016.140516	30.696692
492.849449	29055.932428	30.701709
493.988561	29109.189000	30.706727
494.541886	29155.645723	30.711744
494.998656	29186.734401	30.716762
495.393157	29234.783522	30.721780
495.822702	29274.440231	30.726797
495.968998	29313.060172	30.731815
496.392136	29361.145747	30.736832
497.558209	29393.618288	30.741850
498.031639	29439.695046	30.746868
498.511640	29479.182652	30.751885
498.845888	29513.908810	30.756903
499.275644	29563.514633	30.761920
499.817370	29607.705905	30.766938
499.955246	29653.320100	30.771956
500.711443	29699.585729	30.776973
501.398234	29743.664135	30.781991
501.400225	29803.052758	30.787008
501.633645	29847.313235	30.792026
502.395509	29902.148240	30.797044
502.352333	29954.824286	30.802061
502.914137	29999.694647	30.807079
503.501369	30064.685553	30.812096
503.518920	30120.207272	30.817114
504.533213	30178.111060	30.822132
504.803547	30229.579335	30.827149
505.698251	30304.129710	30.832167
505.904520	30350.601713	30.837184
506.660470	30406.417467	30.842202
508.186371	30446.463224	30.847220
508.591338	30487.038778	30.852237
509.462208	30511.044329	30.857255
510.055248	30551.890726	30.862272
510.548891	30573.326213	30.867290
511.572995	30601.849460	30.872308
511.791775	30618.961816	30.877325
512.536402	30648.870937	30.882343
512.419470	30669.079564	30.887360
512.997115	30695.290785	30.892378
513.596934	30722.839318	30.897396
513.546210	30760.991301	30.902413
514.233118	30795.520702	30.907431
514.033221	30828.302526	30.912448
514.476681	30869.386703	30.917466
514.819110	30926.382530	30.922484
515.412426	30977.415815	30.927501
516.185420	31023.659938	30.932519
516.341615	31083.689077	30.937536
516.711249	31132.321912	30.942554
516.774544	31181.035772	30.947572
517.517496	31245.246988	30.952589
518.101844	31309.403567	30.957607
518.281754	31374.525863	30.962624
519.339300	31422.640858	30.967642
519.311091	31488.051677	30.972660
520.026018	31549.233105	30.977677
521.288952	31581.349115	30.982695
521.814509	31644.384109	30.987712
522.268476	31687.689935	30.992730
523.242792	31740.159048	30.997748
523.293096	31800.710491	31.002765
524.064198	31842.668534	31.007783
524.551921	31903.909045	31.012800
525.265221	31945.154585	31.017818
525.531043	31997.909953	31.022836
525.856599	32048.938541	31.027853
526.672284	32092.915492	31.032871
526.596450	32152.602986	31.037888
526.895907	32210.648509	31.042906
527.417556	32261.685128	31.047924
528.060546	32327.750851	31.052941
528.613894	32377.078264	31.057959
529.186373	32455.435590	31.062976
529.826750	32511.208321	31.067994
529.888334	32572.464179	31.073012
530.492545	32635.602798	31.078029
531.281223	32698.258751	31.083047
531.425342	32768.599343	31.088064
532.431683	32816.701628	31.093082
532.940643	32883.786455	31.098100
533.299564	32947.271163	31.103117
533.988383	33012.687763	31.108135
534.412680	33080.008741	31.113152
535.127165	33138.598394	31.118170
535.395567	33200.774034	31.123188
536.086988	33266.749709	31.128205
536.694863	33320.687474	31.133223
537.994915	33353.816530	31.138240
538.591368	33387.728952	31.143258
539.656572	33431.814769	31.148276
540.427489	33476.575997	31.153293
540.589934	33497.528930	31.158311
541.036985	33549.954837	31.163328
541.341741	33585.912183	31.168346
541.810469	33620.563335	31.173364
541.822701	33673.584841	31.178381
542.097926	33717.907712	31.183399
542.669297	33781.352650	31.188416
543.216444	33837.909230	31.193434
544.198206	33883.777821	31.198452
544.421364	33938.559741	31.203469
544.836733	33994.290420	31.208487
545.254184	34049.591691	31.213504
545.788327	34109.998578	31.218522
545.845218	34166.198342	31.223540
545.729329	34238.167259	31.228557
546.584401	34314.619019	31.233575
547.197521	34388.559270	31.238592
547.636392	34470.397890	31.243610
548.588486	34541.866252	31.248628
548.436473	34622.727407	31.253645
549.289830	34691.861950	31.258663
549.347252	34769.859956	31.263680
550.197783	34837.515294	31.268698
551.177390	34911.237075	31.273716
551.649785	34974.195012	31.278733
552.744009	35050.416378	31.283751
553.270310	35115.852674	31.288768
553.894403	35182.825324	31.293786
554.834585	35239.221101	31.298804
555.156915	35303.730367	31.303821
556.119930	35356.477109	31.308839
556.779383	35422.623954	31.313856
557.614686	35472.539633	31.318874
558.827963	35514.458894	31.323892
559.312723	35568.175119	31.328909
559.658692	35605.297255	31.333927
560.248935	35659.320777	31.338944
561.028528	35702.309025	31.343962
561.158841	35744.890983	31.348980
561.843111	35786.772106	31.353997
562.353379	35838.319503	31.359015
563.166818	35895.679635	31.364032
563.309063	35933.329740	31.369050
563.426865	35982.208212	31.374068
563.484802	36052.626844	31.379085
564.498886	36104.369590	31.384103
564.986518	36165.542520	31.389120
565.454264	36234.887898	31.394138
565.722698	36290.688688	31.399156
565.642890	36356.624700	31.404173
566.542546	36432.531683	31.409191
567.179740	36502.896992	31.414208
567.616370	36562.574354	31.419226
568.335160	36622.083618	31.424244
568.528891	36689.612184	31.429261
569.027619	36755.712499	31.434279
569.633681	36819.645066	31.439296
570.334986	36893.719288	31.444314
570.920892	36953.574368	31.449332
571.040908	37033.572594	31.454349
571.809864	37104.138602	31.459367
572.185770	37176.495725	31.464384
572.742791	37254.879624	31.469402
573.656019	37327.356771	31.474420
573.700539	37402.726160	31.479437
574.652004	37469.695315	31.484455
575.381835	37558.212133	31.489472
575.946962	37628.660409	31.494490
577.006479	37694.563859	31.499508
577.448533	37752.397512	31.504525
578.609338	37816.257450	31.509543
579.177784	37878.568144	31.514560
579.619912	37948.483141	31.519578
580.813012	38007.438979	31.524596
581.191351	38069.650311	31.529613
581.317204	38116.935787	31.534631
581.710185	38192.393920	31.539648
582.309213	38260.565941	31.544666
582.898174	38313.296935	31.549684
583.305772	38383.364713	31.554701
583.748953	38450.661295	31.559719
584.971576	38517.995045	31.564736
585.782837	38560.877263	31.569754
586.942281	38611.500469	31.574772
588.071331	38659.130019	31.579789
588.990328	38709.374831	31.584807
589.128328	38740.992369	31.589824
589.760683	38793.821482	31.594842
590.603555	38833.251621	31.599860
591.005451	38883.774920	31.604877
591.566838	38924.787729	31.609895
591.626771	38972.168772	31.614912
592.043503	39023.864279	31.619930
592.997831	39073.516847	31.624948
593.028872	39127.400174	31.629965
593.440254	39182.560188	31.634983
594.370330	39238.749056	31.640000
594.478358	39308.732770	31.645018
594.871651	39363.969035	31.650036
595.096499	39430.179560	31.655053
596.727213	39485.261002	31.660071
597.663946	39535.561854	31.665088
598.108152	39593.672419	31.670106
598.859735	39641.782752	31.675124
599.422352	39700.372172	31.680141
600.269118	39749.290459	31.685159
600.957073	39780.711368	31.690176
600.877542	39837.239201	31.695194
601.995577	39878.136655	31.700212
602.126500	39924.904976	31.705229
602.512266	39970.332197	31.710247
603.183325	40022.719360	31.715264
603.306175	40075.948827	31.720282
603.888443	40131.243401	31.725300
604.088095	40197.331542	31.730317
604.059327	40254.944306	31.735335
605.089285	40328.158340	31.740352
605.517651	40394.507922	31.745370
606.264938	40468.181367	31.750388
606.822692	40545.802462	31.755405
607.660633	40604.063419	31.760423
608.295724	40673.223194	31.765440
608.645115	40756.311230	31.770458
609.553767	40817.920005	31.775476
610.147559	40897.875889	31.780493
610.334007	40964.985643	31.785511
611.260815	41039.183107	31.790528
611.920105	41111.863855	31.795546
612.414145	41189.050216	31.800564
613.042080	41257.136753	31.805581
613.510866	41331.385437	31.810599
613.847485	41406.588467	31.815616
614.716553	41492.460741	31.820634
615.231876	41574.213698	31.825652
615.646889	41658.434305	31.830669
616.262537	41737.461776	31.835687
617.240075	41807.643747	31.840704
618.071539	41893.120160	31.845722
618.348474	41962.001916	31.850740
619.285696	42041.016621	31.855757
619.975406	42124.260821	31.860775
620.606387	42193.310104	31.865792
621.453949	42270.377208	31.870810
622.322912	42349.979568	31.875828
622.731759	42421.606356	31.880845
623.307955	42485.168924	31.885863
624.177505	42548.826692	31.890880
624.737707	42622.919588	31.895898
625.061042	42687.021891	31.900916
625.578199	42763.402450	31.905933
626.331712	42837.810403	31.910951
626.987887	42913.384681	31.915968
627.565683	42992.026069	31.920986
628.126552	43060.639020	31.926004
629.166131	43133.944499	31.931021
629.659316	43209.386852	31.936039
630.575334	43277.175603	31.941056
631.340940	43341.554858	31.946074
633.129217	43381.274739	31.951092
633.695710	43431.052741	31.956109
634.451406	43477.836574	31.961127
635.883255	43500.395905	31.966144
636.215356	43540.829781	31.971162
637.088146	43561.356697	31.976180
637.177038	43594.083425	31.981197
637.529501	43628.605984	31.986215
637.841559	43669.665634	31.991232
638.028789	43719.531479	31.996250
639.002559	43767.882785	32.001268
639.209804	43812.121568	32.006285
639.772400	43875.214345	32.011303
640.786792	43923.050695	32.016320
641.126904	43978.303389	32.021338
642.183685	44023.827580	32.026356
642.554563	44073.763945	32.031373
643.146036	44131.288659	32.036391
643.256590	44185.485540	32.041408
644.109975	44240.843689	32.046426
645.138049	44286.834471	32.051444
645.472778	44347.050059	32.056461
646.101489	44408.469126	32.061479
646.698743	44468.400130	32.066496
647.053976	44538.449442	32.071514
647.831421	44600.086802	32.076532
647.869136	44664.017385	32.081549
648.243175	44740.458882	32.086567
648.752712	44823.212188	32.091584
649.281183	44906.066820	32.096602
650.115457	44986.339937	32.101620
650.735382	45066.552219	32.106637
651.556361	45141.642958	32.111655
652.390345	45218.604430	32.116672
652.516542	45306.847715	32.121690
653.421690	45385.130329	32.126708
654.265542	45470.330293	32.131725
654.933607	45542.903473	32.136743
656.409357	45610.279416	32.141760
656.703534	45688.753218	32.146778
658.004161	45760.710415	32.151796
658.536468	45831.867888	32.156813
658.735079	45899.656297	32.161831
659.513109	45960.413710	32.166848
659.756977	46043.192566	32.171866
659.892625	46115.123302	32.176884
660.259595	46204.406396	32.181901
660.941649	46293.834889	32.186919
661.745624	46376.967686	32.191936
662.580009	46469.282708	32.196954
663.426375	46551.632095	32.201972
663.880233	46627.325309	32.206989
664.082543	46724.405008	32.212007
664.781598	46808.871464	32.217024
665.332708	46907.070345	32.222042
665.787977	47002.206858	32.227060
666.658607	47093.211163	32.232077
667.207634	47194.737517	32.237095
667.708340	47283.191044	32.242112
668.740083	47376.623082	32.247130
669.065076	47461.696563	32.252148
669.790952	47549.187350	32.257165
670.110433	47652.881005	32.262183
671.141322	47746.267609	32.267200
671.814264	47834.981576	32.272218
672.796932	47923.014369	32.277236
673.724148	48002.766242	32.282253
674.571998	48080.232712	32.287271
675.180485	48165.497613	32.292288
675.929956	48254.333053	32.297306
676.434637	48337.370840	32.302324
677.584119	48410.412491	32.307341
677.929048	48500.679670	32.312359
679.013293	48570.966269	32.317376
680.024771	48647.014083	32.322394
680.643237	48728.341094	32.327412
681.479862	48798.892040	32.332429
682.053194	48880.037907	32.337447
683.075695	48951.846258	32.342464
683.649264	49012.992633	32.347482
684.762736	49083.888854	32.352500
685.445132	49159.009580	32.357517
685.432274	49233.346341	32.362535
686.201506	49294.643284	32.367552
686.588891	49374.351159	32.372570
687.099080	49463.533210	32.377588
687.930745	49535.155309	32.382605
688.615454	49630.454977	32.387623
689.259248	49706.342515	32.392640
689.512008	49804.604072	32.397658
690.270730	49873.352861	32.402676
691.196542	49957.153020	32.407693
692.098415	50050.844498	32.412711
692.772483	50127.644527	32.417728
693.431191	50215.130439	32.422746
694.068475	50299.467950	32.427764
694.512593	50386.852407	32.432781
695.202606	50495.175954	32.437799
696.016591	50580.015087	32.442816
696.118356	50673.347527	32.447834
696.955933	50765.922588	32.452852
697.613659	50852.918743	32.457869
698.436766	50952.914198	32.462887
699.562902	51033.816395	32.467904
700.389098	51113.424613	32.472922
701.232893	51202.228933	32.477940
702.443667	51279.251120	32.482957
703.081496	51363.302503	32.487975
703.918722	51430.798700	32.492992
705.044440	51492.660643	32.498010
705.847832	51568.521758	32.503028
706.689315	51627.583414	32.508045
707.338457	51703.022896	32.513063
707.775870	51757.712601	32.518080
708.555907	51832.081362	32.523098
708.634407	51888.728333	32.528116
709.310309	51957.726092	32.533133
709.691921	52038.974798	32.538151
710.377058	52101.286906	32.543168
710.766406	52185.258010	32.548186
711.405892	52255.539321	32.553204
712.412696	52328.316836	32.558221
712.829526	52422.797757	32.563239
713.352503	52508.383772	32.568256
714.171359	52585.585634	32.573274
714.848451	52683.460372	32.578292
715.640270	52764.900849	32.583309
716.046258	52850.634755	32.588327
716.868448	52941.820025	32.593344
717.694980	53035.336477	32.598362
718.048861	53123.980658	32.603380
719.771975	53193.839577	32.608397
720.780892	53283.629643	32.613415
721.462455	53353.756012	32.618432
722.028931	53428.192650	32.623450
723.083555	53509.881831	32.628468
723.631656	53571.413275	32.633485
724.298594	53663.077086	32.638503
724.911069	53742.119632	32.643520
725.606977	53827.441618	32.648538
725.322414	53918.606142	32.653556
726.478357	54013.119688	32.658573
726.960525	54114.320638	32.663591
727.486923	54211.565267	32.668608
727.911109	54306.199239	32.673626
728.835072	54402.605797	32.678644
729.677569	54510.779947	32.683661
729.897308	54612.660275	32.688679
730.793198	54720.573658	32.693696
731.365358	54820.145118	32.698714
732.420937	54926.958032	32.703732
733.622201	55018.751400	32.708749
734.639447	55120.769425	32.713767
735.579957	55214.308199	32.718784
736.482634	55307.253573	32.723802
736.855782	55408.656698	32.728820
737.650546	55492.705038	32.733837
738.399508	55590.556498	32.738855
739.180254	55675.157780	32.743872
739.595736	55770.274121	32.748890
740.326000	55872.161877	32.753908
740.931832	55967.625707	32.758925
741.496927	56067.451036	32.763943
742.347031	56165.490194	32.768960
743.098921	56271.938903	32.773978
743.828153	56377.583161	32.778996
744.634159	56467.599266	32.784013
745.486128	56567.011400	32.789031
746.428723	56655.646244	32.794048
747.159217	56732.683406	32.799066
748.088474	56820.923127	32.804084
749.647891	56898.589927	32.809101
750.008881	56976.904694	32.814119
751.025367	57051.031266	32.819136
752.055413	57111.441973	32.824154
752.761776	57189.616248	32.829172
753.403012	57259.756907	32.834189
754.191913	57342.145563	32.839207
754.629704	57423.665685	32.844224
755.764981	57492.287923	32.849242
755.610792	57571.925615	32.854260
756.351894	57656.466176	32.859277
756.925684	57745.131062	32.864295
757.353973	57839.376500	32.869312
757.794083	57935.933466	32.874330
758.705368	58040.746281	32.879348
759.167669	58142.602924	32.884365
759.660659	58253.650540	32.889383
760.182342	58363.031657	32.894400
761.404711	58472.116372	32.899418
761.813367	58588.906323	32.904436
762.486812	58693.194428	32.909453
763.232395	58813.524159	32.914471
763.772902	58928.024495	32.919488
765.139132	59035.595999	32.924506
765.654163	59164.474454	32.929524
766.842075	59267.495462	32.934541
768.111913	59373.745338	32.939559
768.780617	59473.544419	32.944576
769.956903	59580.974364	32.949594
770.806847	59686.235949	32.954612
771.382024	59780.427279	32.959629
772.274753	59885.714164	32.964647
772.706019	59987.876081	32.969664
773.826228	60089.958418	32.974682
774.303618	60198.156026	32.979700
775.121695	60295.082894	32.984717
775.788925	60395.556715	32.989735
776.675301	60504.008235	32.994752
777.276068	60608.413364	32.999770
777.658872	60718.222755	33.004788
779.131456	60823.648997	33.009805
779.909908	60924.156916	33.014823
780.621844	61029.632335	33.019840
781.519027	61125.203206	33.024858
782.287417	61231.504356	33.029876
782.990469	61330.396353	33.034893
783.868229	61433.026251	33.039911
785.111432	61535.543493	33.044928
786.513964	61611.023797	33.049946
787.268247	61716.748320	33.054964
788.441415	61780.801970	33.059981
789.220534	61864.158706	33.064999
789.597311	61932.426412	33.070016
790.481366	62014.419359	33.075034
790.774359	62095.274907	33.080052
791.859831	62164.231106	33.085069
792.714892	62247.797624	33.090087
792.888263	62332.378875	33.095104
793.713510	62412.651425	33.100122
794.201318	62498.342622	33.105140
794.940192	62592.961258	33.110157
795.741535	62686.355906	33.115175
796.381433	62786.725929	33.120192
797.497363	62875.724689	33.125210
798.479526	62969.171816	33.130228
799.110687	63062.091580	33.135245
799.972299	63157.462990	33.140263
800.747995	63245.933705	33.145280
801.785389	63338.317319	33.150298
802.578945	63433.208560	33.155316
803.454537	63510.398070	33.160333
804.209059	63596.383152	33.165351
804.689387	63687.921796	33.170368
805.752216	63782.420806	33.175386
806.429919	63887.537308	33.180404
806.746425	63985.629424	33.185421
807.963929	64090.597588	33.190439
808.379894	64191.543761	33.195456
809.265603	64291.177183	33.200474
809.423993	64408.042891	33.205492
810.130154	64514.453666	33.210509
810.777044	64638.355553	33.215527
811.386644	64754.709682	33.220544
812.722957	64862.885619	33.225562
813.761586	64982.334895	33.230580
814.659944	65098.249492	33.235597
815.501997	65209.502261	33.240615
815.679230	65336.599229	33.245632
817.076505	65449.269179	33.250650
817.470176	65567.340186	33.255668
818.166441	65687.357885	33.260685
819.453563	65800.800939	33.265703
820.211573	65914.853670	33.270720
821.012802	66021.464411	33.275738
821.925570	66140.492909	33.280756
823.005787	66263.811677	33.285773
824.444381	66366.793344	33.290791
824.763597	66482.757832	33.295808
825.697256	66582.128319	33.300826
826.102306	66703.946701	33.305844
827.104126	66819.903597	33.310861
828.404776	66919.946238	33.315879
828.924215	67026.679848	33.320896
829.588725	67141.912254	33.325914
830.026237	67255.824758	33.330932
831.327803	67370.569917	33.335949
832.167293	67482.315594	33.340967
832.561385	67588.656177	33.345984
833.572370	67701.467493	33.351002
834.374854	67802.269840	33.356020
835.149217	67909.640763	33.361037
836.835458	67988.301201	33.366055
837.652467	68087.110649	33.371072
838.823381	68173.283312	33.376090
839.824923	68262.330734	33.381108
840.506868	68366.071342	33.386125
841.180576	68452.191180	33.391143
841.702310	68550.699245	33.396160
842.858115	68652.665461	33.401178
843.071954	68755.994919	33.406196
843.768354	68871.895128	33.411213
844.463480	68972.310356	33.416231
845.238136	69077.309509	33.421248
846.452049	69194.033379	33.426266
847.151233	69298.433169	33.431284
847.896339	69419.323486	33.436301
848.599561	69530.059809	33.441319
849.353904	69664.583360	33.446336
850.286054	69769.356557	33.451354
851.028986	69893.885950	33.456372
851.263061	70021.652383	33.461389
852.386380	70138.826890	33.466407
852.973036	70262.107789	33.471424
853.737197	70391.183148	33.476442
854.984209	70517.672359	33.481460
856.079165	70639.002828	33.486477
857.262544	70752.502559	33.491495
858.435872	70878.835755	33.496512
859.459732	70986.849612	33.501530
860.499020	71096.385433	33.506548
860.960695	71217.751714	33.511565
862.217390	71327.649875	33.516583
862.729796	71444.019084	33.521600
863.803446	71555.480164	33.526618
864.590019	71679.025766	33.531636
865.093768	71783.793526	33.536653
865.801599	71909.750770	33.541671
866.528307	72035.212217	33.546688
868.160652	72127.784971	33.551706
870.069513	72219.830116	33.556724
871.273496	72332.461804	33.561741
872.460609	72422.329373	33.566759
872.731418	72509.837157	33.571776
873.441767	72612.682521	33.576794
874.194291	72714.180369	33.581812
874.911147	72810.226804	33.586829
875.693396	72919.613412	33.591847
876.065958	73033.466260	33.596864
876.863713	73143.698810	33.601882
878.033151	73249.251322	33.606900
878.743760	73366.033188	33.611917
879.887023	73470.794345	33.616935
880.159205	73569.171821	33.621952
880.660075	73684.808587	33.626970
881.565436	73804.601596	33.631988
882.503465	73911.120321	33.637005
883.190309	74016.645316	33.642023
883.594941	74146.259782	33.647040
884.595305	74263.464805	33.652058
885.462190	74385.620397	33.657076
886.703974	74502.108573	33.662093
888.507763	74609.222399	33.667111
889.335420	74714.960629	33.672128
890.402058	74821.505984	33.677146
891.903951	74923.948254	33.682164
892.839695	75009.049743	33.687181
893.873597	75098.657188	33.692199
894.640048	75203.940173	33.697216
895.281731	75307.866142	33.702234
896.153122	75399.033317	33.707252
896.318422	75510.113368	33.712269
897.319455	75615.908417	33.717287
897.758328	75734.741752	33.722304
898.587412	75852.528467	33.727322
899.300336	75977.755321	33.732340
899.992972	76106.743626	33.737357
900.774787	76228.468477	33.742375
901.203707	76372.197414	33.747392
902.050119	76514.755134	33.752410
902.884567	76656.253119	33.757428
903.625184	76801.632992	33.762445
904.163135	76938.388750	33.767463
904.843227	77098.064142	33.772480
905.768657	77251.676580	33.777498
907.082625	77401.194026	33.782516
907.727388	77550.732188	33.787533
908.661844	77696.078312	33.792551
909.529317	77864.456679	33.797568
910.373622	78013.653763	33.802586
911.598296	78161.508846	33.807604
912.373899	78325.187213	33.812621
913.255291	78472.590713	33.817639
914.518818	78632.050502	33.822656
915.472649	78768.505718	33.827674
917.418636	78915.109807	33.832692
918.090912	79064.235721	33.837709
919.267655	79186.579468	33.842727
920.442165	79329.427718	33.847744
921.146443	79460.286783	33.852762
922.572016	79587.246236	33.857780
923.534747	79728.526365	33.862797
924.651055	79854.629272	33.867815
925.675554	79971.657477	33.872832
926.410653	80091.759907	33.877850
927.300025	80216.594093	33.882868
928.566550	80341.244163	33.887885
929.963961	80442.381866	33.892903
931.059860	80553.131171	33.897920
931.971393	80648.766593	33.902938
933.028860	80745.313769	33.907956
933.636150	80857.343963	33.912973
934.429444	80954.633198	33.917991
935.368902	81071.124831	33.923008
935.729757	81180.630137	33.928026
936.373845	81287.930012	33.933044
936.943487	81421.518556	33.938061
938.013584	81534.807751	33.943079
939.027808	81656.774952	33.948096
939.464559	81797.094965	33.953114
940.215828	81920.753602	33.958132
940.607633	82067.087265	33.963149
941.878079	82198.573593	33.968167
942.997445	82340.488304	33.973184
943.894986	82473.577543	33.978202
945.021832	82614.866265	33.983220
945.511638	82759.257720	33.988237
946.484712	82903.162363	33.993255
947.351623	83035.779196	33.998272
948.262526	83193.970670	34.003290
949.482453	83339.999689	34.008308
950.343486	83492.393195	34.013325
951.216114	83639.919892	34.018343
952.162902	83780.329039	34.023360
953.229821	83948.724147	34.028378
954.315706	84087.750896	34.033396
955.186787	84246.734609	34.038413
956.271980	84385.465845	34.043431
957.300354	84539.602928	34.048448
958.211237	84682.814148	34.053466
959.080811	84833.993662	34.058484
960.320738	84983.914766	34.063501
961.049572	85143.574343	34.068519
962.182434	85284.536456	34.073536
962.981279	85434.460027	34.078554
964.021833	85587.083173	34.083572
964.772419	85747.717619	34.088589
966.453359	85905.333543	34.093607
967.635082	86047.203081	34.098624
968.063061	86195.733194	34.103642
969.310141	86336.093498	34.108660
970.278609	86480.261308	34.113677
971.523340	86622.920855	34.118695
972.515592	86763.453889	34.123712
973.582590	86907.404911	34.128730
975.004890	87026.393819	34.133748
975.605199	87174.533486	34.138765
976.673461	87315.436464	34.143783
977.428762	87456.450824	34.148800
978.197679	87603.918774	34.153818
979.171077	87730.943021	34.158836
979.959277	87890.908333	34.163853
981.134000	88027.272328	34.168871
981.949402	88173.235936	34.173888
982.756104	88316.037566	34.178906
983.804004	88453.400322	34.183924
984.191614	88596.965223	34.188941
985.061869	88738.467406	34.193959
985.857264	88888.463909	34.198976
986.025296	89056.669432	34.203994
987.164130	89216.950591	34.209012
987.915928	89394.292425	34.214029
988.775954	89562.053853	34.219047
989.553210	89729.482518	34.224064
990.281828	89923.040966	34.229082
991.563212	90083.056611	34.234100
992.535642	90267.765852	34.239117
993.676638	90448.150057	34.244135
995.273131	90611.615306	34.249152
996.253032	90792.194210	34.254170
997.595386	90950.629112	34.259188
998.459960	91128.863062	34.264205
999.591594	91287.260279	34.269223
1001.037734	91447.876964	34.274240
1002.232521	91615.323041	34.279258
1003.520589	91761.182987	34.284276
1004.375300	91926.290503	34.289293
1005.452696	92088.822790	34.294311
1006.452904	92244.602889	34.299328
1007.651366	92406.907665	34.304346
1008.604877	92568.692104	34.309364
1009.922205	92727.357985	34.314381
1010.619507	92882.497702	34.319399
1011.610116	93045.241055	34.324416
1012.319549	93216.731016	34.329434
1013.419165	93371.038975	34.334452
1014.090794	93550.437581	34.339469
1014.639722	93713.634431	34.344487
1016.026352	93895.521095	34.349504
1016.376551	94067.344313	34.354522
1017.697156	94247.991481	34.359540
1018.753662	94429.786654	34.364557
1019.910519	94601.633678	34.369575
1020.737010	94776.171892	34.374592
1021.993887	94964.267018	34.379610
1022.992957	95141.753527	34.384628
1023.819876	95324.790979	34.389645
1024.710032	95506.217305	34.394663
1025.907598	95682.882331	34.399680
1026.850511	95874.367940	34.404698
1027.798073	96049.495688	34.409716
1029.184130	96237.337661	34.414733
1030.579255	96410.897225	34.419751
1031.675083	96583.888812	34.424768
1033.148366	96758.336357	34.429786
1034.273200	96920.360209	34.434804
1035.788823	97077.190109	34.439821
1036.892334	97216.896584	34.444839
1038.595609	97359.869230	34.449856
1039.466281	97498.211636	34.454874
1040.582158	97627.902524	34.459892
1041.479393	97775.086420	34.464909
1042.078122	97915.320017	34.469927
1043.039717	98058.923756	34.474944
1043.231805	98216.468489	34.479962
1044.221235	98371.604732	34.484980
1045.169459	98531.149234	34.489997
1046.263925	98687.035492	34.495015
1047.188921	98843.451897	34.500032
1047.961715	99019.446776	34.505050
1048.979860	99197.357273	34.510068
1049.755239	99366.636389	34.515085
1050.562551	99553.975096	34.520103
1052.139945	99722.156820	34.525120
1052.597948	99905.670288	34.530138
1053.533832	100096.454329	34.535156
1054.388731	100289.013868	34.540173
1055.611450	100468.563347	34.545191
1057.153253	100650.034963	34.550208
1058.122987	100837.526111	34.555226
1059.250779	101021.439337	34.560244
1060.771067	101195.611412	34.565261
1061.809723	101376.262450	34.570279
1063.026658	101546.740267	34.575296
1064.214665	101737.790791	34.580314
1065.154003	101906.773459	34.585332
1066.563474	102076.664537	34.590349
1067.839825	102249.745621	34.595367
1069.120291	102415.684354	34.600384
1070.104805	102594.567376	34.605402
1070.977225	102764.668850	34.610420
1072.275517	102946.970665	34.615437
1072.729474	103123.377178	34.620455
1073.741561	103299.511991	34.625472
1075.021970	103490.293472	34.630490
1075.906459	103662.374411	34.635508
1077.330367	103842.659812	34.640525
1078.109917	104023.981338	34.645543
1079.536354	104199.823218	34.650560
1080.367479	104388.762959	34.655578
1081.376365	104562.512939	34.660596
1082.407662	104744.644864	34.665613
1083.576804	104925.601849	34.670631
1085.205442	105098.501928	34.675648
1086.515226	105285.326867	34.680666
1087.914433	105442.968070	34.685684
1089.220201	105605.641952	34.690701
1090.130022	105785.217891	34.695719
1091.347448	105941.550543	34.700736
1092.566882	106108.080111	34.705754
1093.773349	106266.734458	34.710772
1094.887791	106413.917052	34.715789
1096.024745	106587.265575	34.720807
1097.365697	106738.021106	34.725824
1097.967635	106886.535354	34.730842
1098.903648	107023.453843	34.735860
1099.636372	107174.911287	34.740877
1100.452929	107340.871435	34.745895
1101.358333	107498.482545	34.750912
1101.771864	107667.021743	34.755930
1102.889100	107851.148684	34.760948
1103.653383	108029.079719	34.765965
1104.576396	108203.640580	34.770983
1105.632384	108394.482655	34.776000
1106.716441	108591.857652	34.781018
1108.012892	108780.431779	34.786036
1109.353646	108968.277565	34.791053
1110.234116	109160.231775	34.796071
1111.316770	109341.651115	34.801088
1112.848572	109533.179713	34.806106
1114.185156	109719.929246	34.811124
1115.575260	109905.619433	34.816141
1116.646377	110085.880188	34.821159
1117.848173	110256.808615	34.826176
1119.640122	110442.281587	34.831194
1120.498682	110612.320855	34.836212
1121.893693	110791.225904	34.841229
1122.181505	110975.439761	34.846247
1123.278871	111161.479862	34.851264
1123.906120	111353.315279	34.856282
1124.524684	111556.504736	34.861300
1125.596659	111759.972766	34.866317
1126.627357	111977.017819	34.871335
1127.296485	112177.441286	34.876352
1128.484456	112398.681475	34.881370
1129.111209	112638.351935	34.886388
1130.823124	112852.525214	34.891405
1132.349588	113063.019718	34.896423
1134.127387	113265.807675	34.901440
1135.347952	113477.637270	34.906458
1136.796070	113689.163424	34.911476
1138.004520	113879.370841	34.916493
1139.078141	114076.837142	34.921511
1140.522692	114265.270941	34.926528
1141.211519	114476.324795	34.931546
1142.235901	114687.145376	34.936564
1143.425366	114883.545806	34.941581
1144.436361	115092.635841	34.946599
1145.612120	115293.704130	34.951616
1146.964927	115503.853642	34.956634
1148.324201	115708.846632	34.961652
1149.709351	115901.115238	34.966669
1150.538121	116114.995435	34.971687
1151.901242	116301.340538	34.976704
1153.294244	116493.142922	34.981722
1154.114600	116695.954417	34.986740
1155.558250	116892.287021	34.991757
1156.267213	117097.920725	34.996775
1157.495324	117284.802119	35.001792
1158.475157	117476.428316	35.006810
1159.296892	117677.358380	35.011828
1160.227170	117870.566917	35.016845
1160.931271	118079.502988	35.021863
1162.087797	118278.301708	35.026880
1162.859890	118498.937841	35.031898
1163.963762	118709.165842	35.036916
1165.310072	118926.437510	35.041933
1166.207240	119151.010797	35.046951
1167.541975	119362.483822	35.051968
1168.738954	119590.886827	35.056986
1169.712639	119819.114392	35.062004
1171.160500	120027.315986	35.067021
1172.615780	120246.821736	35.072039
1174.272896	120458.678258	35.077056
1174.850834	120680.859282	35.082074
1176.197605	120911.299783	35.087092
1177.540738	121126.154912	35.092109
1178.553142	121347.937011	35.097127
1179.601514	121567.762925	35.102144
1181.258260	121803.125099	35.107162
1182.393541	122021.887573	35.112180
1183.953968	122241.453316	35.117197
1184.914142	122466.839192	35.122215
1186.079793	122683.674883	35.127232
1186.927421	122911.427959	35.132250
1188.355346	123137.739969	35.137268
1190.477171	123329.208348	35.142285
1192.891397	123527.573219	35.147303
1194.803071	123707.521285	35.152320
1197.039897	123886.223379	35.157338
1198.308498	124043.279972	35.162356
1200.088884	124205.458879	35.167373
1201.056661	124368.335435	35.172391
1202.067151	124518.480445	35.177408
1203.680928	124676.824680	35.182426
1204.244605	124839.544777	35.187444
1205.361792	124989.458355	35.192461
1206.426766	125163.742295	35.197479
1207.501950	125338.519787	35.202496
1208.536381	125500.529041	35.207514
1209.054074	125685.822624	35.212532
1210.595579	125847.975035	35.217549
1211.806529	126030.515606	35.222567
1212.643341	126208.748395	35.227584
1213.771439	126382.394630	35.232602
1214.487432	126578.572902	35.237620
1215.297432	126776.574235	35.242637
1216.368911	126975.026398	35.247655
1217.280106	127175.497310	35.252672
1218.090924	127383.769484	35.257690
1218.646563	127606.232753	35.262708
1220.114662	127822.000701	35.267725
1220.854315	128041.786314	35.272743
1221.986766	128251.441532	35.277760
1223.186113	128467.335957	35.282778
1223.929687	128692.753566	35.287796
1225.099913	128908.034849	35.292813
1226.238492	129132.576681	35.297831
1227.313351	129362.987482	35.302848
1228.366671	129594.341692	35.307866
1229.142683	129833.300269	35.312884
1230.303038	130077.645787	35.317901
1231.221703	130330.870229	35.322919
1232.359565	130579.406739	35.327936
1233.668328	130837.068659	35.332954
1234.820134	131091.628277	35.337972
1236.313919	131336.179801	35.342989
1238.162949	131583.917728	35.348007
1240.121867	131820.127723	35.353024
1242.058076	132049.738390	35.358042
1243.902350	132279.214285	35.363060
1245.564641	132496.463720	35.368077
1247.120858	132714.708938	35.373095
1248.406863	132931.822837	35.378112
1250.155352	133135.179616	35.383130
1251.463323	133346.308559	35.388148
1253.761270	133524.015017	35.393165
1255.603765	133701.546842	35.398183
1256.949751	133890.042448	35.403200
1258.381930	134060.014213	35.408218
1259.084194	134253.541225	35.413236
1260.017414	134426.744495	35.418253
1260.756823	134618.251419	35.423271
1261.469526	134820.185722	35.428288
1262.923631	135009.518635	35.433306
1263.633682	135225.186716	35.438324
1264.936618	135436.241071	35.443341
1265.747011	135657.587502	35.448359
1266.481051	135879.430259	35.453376
1267.741871	136102.097186	35.458394
1268.191337	136346.344751	35.463412
1269.732912	136579.984872	35.468429
1270.921912	136812.330285	35.473447
1271.839415	137056.452136	35.478464
1273.960536	137295.145783	35.483482
1275.023523	137528.810969	35.488500
1277.034839	137750.637524	35.493517
1278.512285	137977.159629	35.498535
1279.749358	138213.868179	35.503552
1280.973585	138441.058005	35.508570
1282.538015	138663.994044	35.513588
1284.377277	138871.478288	35.518605
1285.927045	139079.089419	35.523623
1287.756851	139279.324738	35.528640
1289.485880	139471.983021	35.533658
1290.271521	139679.830004	35.538676
1291.283650	139877.368366	35.543693
1292.679856	140079.724070	35.548711
1293.612197	140273.512249	35.553728
1295.065614	140454.937513	35.558746
1296.250572	140652.881824	35.563764
1297.682518	140831.916078	35.568781
1298.911924	141033.037785	35.573799
1299.999182	141220.413574	35.578816
1300.921146	141407.463590	35.583834
1301.766181	141627.054496	35.588852
1302.911202	141831.974145	35.593869
1304.126536	142048.727130	35.598887
1305.399568	142267.817589	35.603904
1306.386077	142487.719324	35.608922
1306.850386	142713.557921	35.613940
1307.425238	142955.357667	35.618957
1308.524987	143210.321421	35.623975
1309.081825	143473.179135	35.628992
1310.606139	143739.880593	35.634010
1311.502408	144013.108544	35.639028
1312.460851	144292.237701	35.644045
1313.851192	144579.170625	35.649063
1314.904083	144867.228881	35.654080
1316.385731	145145.704349	35.659098
1317.695164	145449.867788	35.664116
1318.947778	145734.601300	35.669133
1320.322918	146020.698447	35.674151
1321.630642	146331.946355	35.679168
1323.009119	146622.727507	35.684186
1324.294598	146925.613619	35.689204
1325.908576	147221.254744	35.694221
1327.050424	147527.353774	35.699239
1328.706146	147824.983791	35.704256
1330.583759	148115.437527	35.709274
1331.729334	148415.328401	35.714292
1333.304643	148701.855852	35.719309
1334.959648	148995.411211	35.724327
1336.698022	149281.623435	35.729344
1338.100298	149556.289733	35.734362
1339.575822	149844.923061	35.739380
1340.980276	150129.955824	35.744397
1342.346267	150406.042380	35.749415
1343.840116	150693.410587	35.754432
1345.489237	150962.007112	35.759450
1347.078980	151236.602664	35.764468
1348.564700	151514.084647	35.769485
1350.006891	151774.249083	35.774503
1351.395833	152060.021818	35.779520
1352.921377	152313.262514	35.784538
1354.570556	152589.087885	35.789556
1356.179169	152842.317797	35.794573
1357.577482	153093.657239	35.799591
1358.755188	153348.689324	35.804608
1360.432648	153603.586781	35.809626
1361.458347	153867.375564	35.814644
1363.043626	154117.344908	35.819661
1364.444070	154364.226880	35.824679
1366.090685	154610.484722	35.829696
1367.280666	154855.591757	35.834714
1368.478093	155086.199452	35.839732
1369.445012	155329.825308	35.844749
1370.774850	155568.214763	35.849767
1372.049888	155811.537087	35.854784
1373.518070	156065.230211	35.859802
1374.691074	156314.345089	35.864820
1376.060993	156561.131627	35.869837
1376.903095	156817.676797	35.874855
1377.766627	157086.512802	35.879872
1379.223758	157341.915733	35.884890
1380.138787	157621.034978	35.889908
1380.818195	157904.700124	35.894925
1382.103692	158194.162707	35.899943
1383.177217	158504.647227	35.904960
1384.630617	158785.572502	35.909978
1385.812141	159090.245102	35.914996
1386.998231	159393.130298	35.920013
1388.964579	159691.392955	35.925031
1390.412508	160011.263706	35.930048
1391.827277	160305.603334	35.935066
1393.657444	160605.989163	35.940084
1395.141367	160898.050065	35.945101
1396.811927	161183.724639	35.950119
1398.693525	161488.573876	35.955136
1400.020329	161779.665401	35.960154
1401.395116	162071.841828	35.965172
1402.652803	162366.577834	35.970189
1404.423206	162668.079534	35.975207
1405.365584	162972.097698	35.980224
1406.931528	163272.623562	35.985242
1408.096128	163568.424085	35.990260
1409.687072	163875.103551	35.995277
1411.187691	164174.098834	36.000295
1412.343157	164474.106850	36.005312
1414.066979	164779.640614	36.010330
1415.454679	165083.977850	36.015348
1416.841054	165377.697014	36.020365
1418.739206	165671.419344	36.025383
1420.686592	165961.899535	36.030400
1422.655785	166236.859386	36.035418
1424.660192	166526.863986	36.040436
1425.930178	166801.604353	36.045453
1427.791369	167074.075364	36.050471
1428.709911	167353.142761	36.055488
1430.451344	167623.962591	36.060506
1431.740230	167901.447245	36.065524
1432.509381	168176.573473	36.070541
1433.753044	168458.472457	36.075559
1435.070810	168747.276293	36.080576
1436.169606	169029.850722	36.085594
1437.698251	169315.563802	36.090612
1438.921371	169607.447408	36.095629
1440.883409	169886.541873	36.100647
1442.016570	170168.926968	36.105664
1442.935005	170442.340587	36.110682
1444.495409	170729.275088	36.115700
1445.327272	171014.127922	36.120717
1446.701334	171296.986130	36.125735
1448.143137	171597.347080	36.130752
1449.120092	171904.477320	36.135770
1450.560499	172201.936192	36.140788
1451.652747	172511.499839	36.145805
1453.128428	172819.997282	36.150823
1454.424545	173144.898470	36.155840
1455.582506	173455.713272	36.160858
1457.261821	173777.240779	36.165876
1458.343059	174102.159715	36.170893
1460.062206	174423.722703	36.175911
1461.022982	174762.207967	36.180928
1462.244656	175100.029014	36.185946
1464.060153	175435.060156	36.190964
1465.528060	175787.667178	36.195981
1467.106431	176128.784644	36.200999
1467.958821	176466.081573	36.206016
1469.582676	176818.694479	36.211034
1471.639011	177163.620751	36.216052
1472.892603	177518.929049	36.221069
1474.666934	177858.146153	36.226087
1476.354129	178200.071104	36.231104
1478.119216	178552.633650	36.236122
1479.628790	178895.888169	36.241140
1480.889998	179237.169371	36.246157
1482.406230	179569.575269	36.251175
1484.283509	179921.899354	36.256192
1486.010436	180273.007643	36.261210
1487.861025	180611.759877	36.266228
1489.259975	180961.063006	36.271245
1490.731259	181301.559942	36.276263
1492.210105	181643.136620	36.281280
1493.424883	181979.861172	36.286298
1495.089450	182323.339660	36.291316
1496.547232	182666.614522	36.296333
1498.451818	183002.871906	36.301351
1500.181116	183334.426759	36.306368
1501.890137	183659.132678	36.311386
1503.942438	183978.095109	36.316404
1505.794866	184314.305880	36.321421
1507.786080	184623.571945	36.326439
1509.123695	184934.474785	36.331456
1510.560337	185248.028050	36.336474
1512.500478	185553.398275	36.341492
1513.994886	185865.371020	36.346509
1515.408114	186174.934821	36.351527
1517.022153	186492.069582	36.356544
1517.982880	186817.835554	36.361562
1519.728474	187127.550662	36.366580
1520.999220	187454.650783	36.371597
1522.039609	187773.870954	36.376615
1523.197570	188118.600930	36.381632
1524.583836	188431.469087	36.386650
1525.766635	188734.890972	36.391668
1526.977276	189060.677306	36.396685
1528.302665	189383.691047	36.401703
1529.414178	189703.264785	36.406720
1530.870062	190035.907577	36.411738
1532.260228	190370.556502	36.416756
1532.993590	190719.753667	36.421773
1534.346954	191074.762529	36.426791
1535.455522	191448.781606	36.431808
1536.894439	191819.686882	36.436826
1538.031457	192189.693876	36.441844
1539.035140	192573.322415	36.446861
1540.515093	192960.439141	36.451879
1542.183841	193360.322825	36.456896
1543.696590	193756.414362	36.461914
1545.531833	194148.834912	36.466932
1546.834505	194555.606113	36.471949
1548.261404	194960.022573	36.476967
1550.411117	195371.935270	36.481984
1552.220216	195761.043621	36.487002
1553.818208	196159.496456	36.492020
1555.422928	196565.441124	36.497037
1557.238817	196951.939825	36.502055
1559.343099	197346.732717	36.507072
1561.190038	197729.320089	36.512090
1563.210260	198108.515418	36.517108
1564.920283	198499.573484	36.522125
1566.609863	198877.851955	36.527143
1568.364568	199258.647908	36.532160
1569.680295	199643.837845	36.537178
1571.346728	200020.704356	36.542196
1572.523108	200408.613925	36.547213
1574.145810	200800.664516	36.552231
1575.611757	201188.084309	36.557248
1577.137163	201578.822552	36.562266
1579.120273	201969.954325	36.567284
1580.527771	202358.837703	36.572301
1582.217685	202752.017169	36.577319
1584.530370	203126.528898	36.582336
1586.331794	203494.095708	36.587354
1588.847819	203851.066765	36.592372
1590.705171	204205.752391	36.597389
1592.607727	204563.238023	36.602407
1594.141742	204922.299346	36.607424
1595.393988	205286.337146	36.612442
1597.010488	205637.172327	36.617460
1598.084462	205999.237681	36.622477
1599.610277	206361.379720	36.627495
1601.713773	206726.522774	36.632512
1602.561171	207094.599718	36.637530
1603.920463	207452.838786	36.642548
1605.273739	207832.070037	36.647565
1607.146017	208195.316380	36.652583
1608.656889	208569.038492	36.657600
1609.920490	208926.322490	36.662618
1611.297119	209281.836304	36.667636
1612.595487	209649.072680	36.672653
1614.164750	210010.397686	36.677671
1615.929429	210372.985972	36.682688
1617.480385	210747.142394	36.687706
1619.527953	211112.682115	36.692724
1620.938040	211481.049870	36.697741
1621.987231	211858.293623	36.702759
1623.514686	212241.298427	36.707776
1624.879804	212626.237395	36.712794
1626.681129	213009.452505	36.717812
1628.151472	213403.926061	36.722829
1629.430269	213806.104083	36.727847
1631.348189	214198.167799	36.732864
1632.820805	214592.137946	36.737882
1634.826876	214989.828087	36.742900
1636.118741	215404.328468	36.747917
1637.674931	215806.111758	36.752935
1639.671953	216217.091546	36.757952
1640.918090	216635.643167	36.762970
1642.442812	217041.703667	36.767988
1643.950409	217467.122292	36.773005
1645.771937	217878.951534	36.778023
1647.549649	218295.768017	36.783040
1648.956076	218718.567563	36.788058
1651.165328	219143.212518	36.793076
1652.928869	219569.865714	36.798093
1654.164148	219970.043588	36.803111
1656.601307	220399.658014	36.808128
1657.954052	220820.874698	36.813146
1660.025075	221238.287148	36.818164
1661.814048	221645.335625	36.823181
1663.353890	222076.887844	36.828199
1665.287666	222484.676450	36.833216
1666.851055	222901.953094	36.838234
1668.335160	223323.435702	36.843252
1669.958399	223739.688995	36.848269
1671.643899	224154.713840	36.853287
1673.991165	224570.287235	36.858304
1675.246323	224996.158076	36.863322
1677.181796	225419.373913	36.868340
1678.833218	225835.045051	36.873357
1679.999185	226258.903258	36.878375
1682.303672	226672.280850	36.883392
1683.872229	227095.336193	36.888410
1685.734278	227505.667745	36.893428
1687.912768	227916.530577	36.898445
1689.834866	228318.472021	36.903463
1691.583840	228714.271824	36.908480
1693.007410	229132.735122	36.913498
1694.494155	229537.091290	36.918516
1696.444346	229940.505623	36.923533
1698.237884	230348.240603	36.928551
1699.970316	230738.917567	36.933568
1701.051122	231117.489028	36.938586
1702.721969	231509.042070	36.943604
1704.091882	231916.574157	36.948621
1705.440501	232317.328734	36.953639
1707.172748	232722.870308	36.958656
1708.434358	233134.361110	36.963674
1710.182671	233544.753561	36.968692
1711.680090	233969.541795	36.973709
1713.060742	234390.159739	36.978727
1714.700351	234813.122109	36.983744
1716.374891	235239.686514	36.988762
1718.530284	235662.283131	36.993780
1720.354310	236101.499390	36.998797
1722.099666	236520.230719	37.003815
1724.061772	236949.594670	37.008832
1725.434210	237380.025675	37.013850
1727.792785	237811.635157	37.018868
1729.775789	238228.906742	37.023885
1731.360259	238654.426805	37.028903
1733.270458	239082.152742	37.033920
1734.957953	239519.697452	37.038938
1736.469675	239951.481309	37.043956
1738.256036	240391.855754	37.048973
1739.631962	240829.735549	37.053991
1741.408734	241261.857362	37.059008
1743.040576	241721.718811	37.064026
1744.523022	242157.474176	37.069044
1746.606845	242612.865145	37.074061
1748.344811	243055.563883	37.079079
1750.156500	243506.557336	37.084096
1751.976685	243956.178249	37.089114
1753.705902	244409.168518	37.094132
1755.454551	244865.687068	37.099149
1756.649211	245317.957119	37.104167
1758.747823	245780.843898	37.109184
1760.442610	246248.347451	37.114202
1762.519017	246701.205018	37.119220
1764.230623	247165.658424	37.124237
1765.891686	247620.417056	37.129255
1768.346070	248074.837209	37.134272
1770.294631	248530.868514	37.139290
1772.369319	248975.244077	37.144308
1774.290545	249428.207095	37.149325
1776.290848	249872.900957	37.154343
1778.223064	250317.124141	37.159360
1779.543592	250770.851425	37.164378
1781.452480	251222.471511	37.169396
1783.200381	251664.669450	37.174413
1784.774275	252111.673191	37.179431
1786.610488	252560.791550	37.184448
1788.294530	253015.220007	37.189466
1790.430434	253452.678241	37.194484
1792.632344	253907.424905	37.199501
1794.115784	254341.768844	37.204519
1796.003559	254759.785681	37.209536
1797.734902	255184.307178	37.214554
1799.368349	255608.439040	37.219572
1801.170971	256024.031938	37.224589
1802.235235	256459.540274	37.229607
1804.224472	256877.590806	37.234624
1805.173534	257323.991426	37.239642
1807.152317	257761.096118	37.244660
1808.870472	258212.191703	37.249677
1810.029184	258672.756696	37.254695
1811.661316	259131.411573	37.259712
1813.908891	259613.738424	37.264730
1815.073260	260073.717796	37.269748
1817.206587	260548.646122	37.274765
1818.609446	261024.893143	37.279783
1820.560669	261496.371945	37.284800
1822.335586	261981.014060	37.289818
1824.073028	262466.983247	37.294836
1825.904072	262961.395318	37.299853
1827.133517	263460.812720	37.304871
1829.476752	263947.921932	37.309888
1831.242425	264456.036212	37.314906
1832.725011	264958.152516	37.319924
1834.353635	265466.721088	37.324941
1836.305036	265982.372121	37.329959
1838.433252	266492.759306	37.334976
1840.634082	267004.886247	37.339994
1842.265125	267523.587722	37.345012
1844.403475	268039.356593	37.350029
1845.895229	268560.442902	37.355047
1848.073089	269073.383798	37.360064
1849.691828	269595.437497	37.365082
1851.438867	270122.091674	37.370100
1853.777904	270635.967778	37.375117
1855.657081	271163.156379	37.380135
1857.466771	271692.184866	37.385152
1859.290256	272212.547730	37.390170
1861.044710	272733.327814	37.395188
1863.034636	273263.490834	37.400205
1864.658259	273796.763650	37.405223
1866.620375	274324.871527	37.410240
1868.130179	274862.301968	37.415258
1870.516378	275397.650657	37.420276
1872.312228	275927.434358	37.425293
1874.357295	276468.020765	37.430311
1876.788231	276984.788952	37.435328
1880.191017	277481.322105	37.440346
1882.514411	277982.052121	37.445364
1885.387483	278461.603369	37.450381
1887.358582	278953.271863	37.455399
1889.547922	279419.576313	37.460416
1892.302072	279876.867004	37.465434
1893.914389	280333.183351	37.470452
1895.823589	280796.483904	37.475469
1897.464944	281239.330126	37.480487
1899.524865	281670.774611	37.485504
1901.296597	282106.280643	37.490522
1903.157719	282540.601755	37.495540
1904.575505	282975.657934	37.500557
1905.972537	283400.810058	37.505575
1907.466014	283838.644969	37.510592
1908.942409	284293.093683	37.515610
1910.727734	284765.725914	37.520628
1912.207293	285218.748783	37.525645
1913.676162	285688.155437	37.530663
1915.186040	286167.942327	37.535680
1916.454787	286667.225525	37.540698
1917.693018	287167.832934	37.545716
1920.114469	287669.785510	37.550733
1921.523740	288190.756201	37.555751
1923.072146	288702.658594	37.560768
1924.739663	289239.151091	37.565786
1926.410667	289773.786515	37.570804
1927.989851	290319.560401	37.575821
1929.432965	290873.279783	37.580839
1931.298609	291421.996836	37.585856
1933.268919	291992.562267	37.590874
1935.246651	292566.069928	37.595892
1937.440099	293144.643024	37.600909
1939.202256	293718.664292	37.605927
1941.100112	294286.919234	37.610944
1943.196975	294870.935154	37.615962
1945.357386	295463.547126	37.620980
1947.688009	296042.741698	37.625997
1949.418767	296627.445469	37.631015
1951.593827	297207.066481	37.636032
1953.948598	297798.412685	37.641050
1955.506345	298387.199522	37.646068
1957.633531	298967.885168	37.651085
1959.251560	299563.537348	37.656103
1961.051004	300163.396137	37.661120
1963.130390	300755.609463	37.666138
1964.699979	301362.357103	37.671156
1966.679639	301976.497258	37.676173
1969.143169	302573.382326	37.681191
1971.055808	303184.884414	37.686208
1972.927104	303795.043313	37.691226
1974.867969	304408.893861	37.696244
1977.339964	305015.004987	37.701261
1978.837847	305627.830480	37.706279
1980.948081	306249.155852	37.711296
1983.022199	306857.099346	37.716314
1984.870344	307475.108056	37.721332
1987.332362	308089.578706	37.726349
1989.185740	308703.793171	37.731367
1991.320944	309307.746001	37.736384
1993.773739	309923.752954	37.741402
1995.136091	310551.978308	37.746420
1997.406158	311160.667602	37.751437
1999.755466	311769.744704	37.756455
2001.871260	312362.528666	37.761472
2004.125366	312931.287435	37.766490
2006.035079	313508.455009	37.771508
2008.566607	314071.469285	37.776525
2011.162746	314640.156041	37.781543
2013.588296	315185.252282	37.786560
2015.408848	315748.197011	37.791578
2017.596499	316312.851828	37.796596
2019.764106	316853.586187	37.801613
2021.833647	317413.732317	37.806631
2023.668021	317971.349454	37.811648
2025.828188	318518.648109	37.816666
2027.118986	319075.485624	37.821684
2029.996689	319638.927951	37.826701
2031.708945	320199.213124	37.831719
2033.762246	320763.294441	37.836736
2035.555110	321318.706453	37.841754
2036.856741	321904.005464	37.846772
2039.174100	322469.422839	37.851789
2041.000332	323048.553236	37.856807
2043.214499	323626.545490	37.861824
2045.660046	324202.360018	37.866842
2047.955620	324774.234054	37.871860
2050.261898	325352.270229	37.876877
2051.913773	325928.330852	37.881895
2053.790623	326500.589941	37.886912
2056.353765	327077.829018	37.891930
2058.290973	327664.689730	37.896948
2060.571068	328234.450932	37.901965
2062.753899	328815.342607	37.906983
2064.715154	329387.990118	37.912000
2067.342549	329959.096226	37.917018
2069.493620	330532.131131	37.922036
2071.676883	331104.976889	37.927053
2073.760922	331683.012323	37.932071
2075.179912	332264.049290	37.937088
2077.339661	332836.500062	37.942106
2079.498237	333421.459688	37.947124
2081.551577	333991.504704	37.952141
2084.084702	334568.391453	37.957159
2085.784634	335153.181862	37.962176
2088.168125	335733.457406	37.967194
2090.013085	336315.239995	37.972212
2091.856701	336905.570357	37.977229
2094.054117	337496.264877	37.982247
2095.651117	338088.831944	37.987264
2098.143058	338670.578392	37.992282
2100.229668	339266.855108	37.997300
2101.983700	339855.592365	38.002317
2104.122976	340463.749605	38.007335
2106.537853	341067.664242	38.012352
2108.755579	341658.203997	38.017370
2110.836722	342268.835790	38.022388
2112.937549	342858.593922	38.027405
2114.812477	343452.291828	38.032423
2116.091375	344035.424766	38.037440
2118.516986	344619.674056	38.042458
2120.317610	345220.722151	38.047476
2122.151253	345807.544781	38.052493
2124.309659	346401.283360	38.057511
2126.058324	347005.438421	38.062528
2127.977449	347594.278977	38.067546
2129.673644	348219.261668	38.072564
2131.536909	348832.127655	38.077581
2133.489236	349475.497820	38.082599
2134.911613	350105.347601	38.087616
2137.107843	350746.322794	38.092634
2139.128180	351407.517356	38.097652
2140.632658	352060.035616	38.102669
2142.777418	352726.212819	38.107687
2145.129821	353403.813179	38.112704
2146.953545	354062.361244	38.117722
2149.800737	354746.452515	38.122740
2152.394177	355414.971571	38.127757
2154.601144	356092.071048	38.132775
2156.603428	356763.384136	38.137792
2159.190248	357441.157472	38.142810
2161.167737	358135.413458	38.147828
2163.202919	358811.101532	38.152845
2165.540183	359496.316514	38.157863
2167.416927	360202.528576	38.162880
2169.370082	360895.319832	38.167898
2170.953027	361604.017748	38.172916
2172.664913	362315.369754	38.177933
2175.005294	363044.688609	38.182951
2176.615500	363775.818057	38.187968
2178.948771	364505.820510	38.192986
2181.165014	365259.724191	38.198004
2182.845897	365998.839749	38.203021
2185.209389	366747.336024	38.208039
2187.277414	367511.619374	38.213056
2189.613712	368265.821983	38.218074
2192.301100	369029.384383	38.223092
2194.697579	369782.074157	38.228109
2197.305731	370538.744713	38.233127
2199.289053	371296.951750	38.238144
2201.508210	372046.808967	38.243162
2203.306296	372808.413811	38.248180
2205.525410	373569.777965	38.253197
2208.032947	374335.919963	38.258215
2210.312732	375107.333382	38.263232
2212.502099	375875.575072	38.268250
2214.544349	376649.631729	38.273268
2217.130004	377409.732412	38.278285
2219.749089	378174.475992	38.283303
2221.831417	378950.653708	38.288320
2224.406642	379694.222465	38.293338
2226.773488	380454.646251	38.298356
2229.646169	381205.483197	38.303373
2232.648409	381923.674939	38.308391
2235.202742	382638.960978	38.313408
2237.734692	383328.957733	38.318426
2240.213099	384022.574271	38.323444
2242.167442	384710.713209	38.328461
2244.499207	385403.944466	38.333479
2246.734478	386092.005382	38.338496
2248.803434	386783.502003	38.343514
2250.824154	387479.782731	38.348532
2253.050523	388170.156990	38.353549
2255.679161	388847.950064	38.358567
2257.948179	389534.889742	38.363584
2260.198867	390230.384680	38.368602
2262.295367	390928.576894	38.373620
2264.435472	391621.980404	38.378637
2267.404684	392297.078468	38.383655
2269.440132	392985.247142	38.388672
2272.059681	393673.883012	38.393690
2274.415311	394366.729825	38.398708
2276.649231	395057.756444	38.403725
2278.962501	395744.926440	38.408743
2280.883387	396446.567226	38.413760
2282.995563	397149.045350	38.418778
2285.007455	397861.609372	38.423796
2287.006274	398564.705952	38.428813
2289.369421	399285.283588	38.433831
2290.916016	400013.331003	38.438848
2293.300588	400736.224752	38.443866
2295.849318	401473.565249	38.448884
2297.671290	402207.032655	38.453901
2300.556118	402945.771812	38.458919
2302.761519	403687.647789	38.463936
2305.223788	404427.939819	38.468954
2307.753219	405166.832364	38.473972
2309.673114	405907.734533	38.478989
2312.330270	406651.555821	38.484007
2314.109579	407400.927913	38.489024
2316.542073	408137.881562	38.494042
2319.038717	408895.018236	38.499060
2321.360652	409647.629143	38.504077
2324.259593	410385.023570	38.509095
2326.748406	411134.473462	38.514112
2329.621786	411867.499505	38.519130
2332.025119	412601.902393	38.524148
2334.650999	413343.211401	38.529165
2336.634500	414082.988140	38.534183
2338.784608	414831.933617	38.539200
2340.719395	415577.880415	38.544218
2343.162638	416330.555962	38.549236
2344.955702	417094.108026	38.554253
2347.294728	417848.579594	38.559271
2349.351747	418621.181710	38.564288
2351.460699	419377.545797	38.569306
2353.890428	420159.430679	38.574324
2355.426167	420942.608433	38.579341
2357.481236	421721.773540	38.584359
2359.720272	422500.376145	38.589376
2361.487841	423264.350796	38.594394
2363.704988	424039.920635	38.599412
2366.037537	424803.750287	38.604429
2368.854364	425576.889930	38.609447
2371.407090	426365.794871	38.614464
2373.506922	427148.524242	38.619482
2376.102824	427936.661052	38.624500
2378.222617	428722.170029	38.629517
2380.862501	429511.562929	38.634535
2383.019263	430313.312190	38.639552
2384.680885	431111.069194	38.644570
2387.211748	431927.732161	38.649588
2389.487338	432759.695162	38.654605
2391.582034	433582.599539	38.659623
2393.579739	434419.256775	38.664640
2395.664191	435261.030475	38.669658
2398.268294	436105.011986	38.674676
2400.201514	436982.475270	38.679693
2402.610155	437843.579770	38.684711
2404.188901	438726.146182	38.689728
2406.846449	439604.040555	38.694746
2409.731305	440485.048800	38.699764
2411.736141	441378.314782	38.704781
2414.187415	442265.953536	38.709799
2416.739525	443184.904609	38.714816
2419.075190	444082.961069	38.719834
2421.659621	444986.653829	38.724852
2424.019246	445900.918945	38.729869
2426.515355	446814.868738	38.734887
2428.909155	447736.838831	38.739904
2431.622609	448657.601452	38.744922
2434.181115	449578.097446	38.749940
2436.384938	450503.064025	38.754957
2439.224069	451427.425880	38.759975
2441.301383	452365.833527	38.764992
2443.932329	453288.276910	38.770010
2446.458901	454222.831943	38.775028
2448.811377	455173.452435	38.780045
2451.517644	456106.070343	38.785063
2454.125091	457042.706724	38.790080
2456.706586	457978.849059	38.795098
2459.834490	458895.644742	38.800116
2462.673891	459830.594843	38.805133
2465.715940	460741.608219	38.810151
2467.717993	461664.332123	38.815168
2470.294173	462576.503002	38.820186
2472.869595	463498.335237	38.825204
2475.168066	464421.080960	38.830221
2477.838394	465342.001128	38.835239
2480.252068	466267.620861	38.840256
2482.428658	467195.358902	38.845274
2484.835870	468121.496808	38.850292
2486.889434	469062.201496	38.855309
2489.197585	469978.464136	38.860327
2491.712028	470896.112229	38.865344
2493.773695	471802.982170	38.870362
2496.299562	472713.517580	38.875380
2498.297712	473633.039574	38.880397
2501.267165	474554.572541	38.885415
2503.432568	475481.500374	38.890432
2505.228371	476404.101297	38.895450
2508.170358	477335.045423	38.900468
2510.420255	478274.796928	38.905485
2513.260250	479209.248277	38.910503
2516.322709	480140.937151	38.915520
2518.576905	481073.422914	38.920538
2521.437422	482015.501152	38.925556
2523.548672	482960.283129	38.930573
2526.170265	483899.475437	38.935591
2528.609422	484852.481147	38.940608
2531.119218	485809.512123	38.945626
2534.093213	486767.320219	38.950644
2536.454197	487725.584438	38.955661
2539.221287	488689.581145	38.960679
2541.892715	489643.648943	38.965696
2544.503890	490599.844345	38.970714
2546.883814	491553.402085	38.975732
2549.306968	492540.353923	38.980749
2551.941042	493503.144896	38.985767
2554.573090	494477.687779	38.990784
2556.994220	495459.172745	38.995802
2559.903893	496441.172844	39.000820
2562.002352	497425.826757	39.005837
2564.392190	498405.933952	39.010855
2566.596869	499402.609380	39.015872
2568.655383	500406.260367	39.020890
2571.350195	501422.248809	39.025908
2573.797882	502442.553542	39.030925
2576.360366	503466.556950	39.035943
2579.152083	504480.422572	39.040960
2581.514942	505514.415607	39.045978
2584.301054	506548.471736	39.050996
2586.561630	507576.904836	39.056013
2589.433026	508620.693780	39.061031
2592.035060	509660.579049	39.066048
2594.518960	510711.051484	39.071066
2597.266021	511750.825068	39.076084
2599.863893	512811.066906	39.081101
2602.686513	513853.409711	39.086119
2605.379352	514911.325928	39.091136
2607.680666	515965.810705	39.096154
2610.648727	517005.750458	39.101172
2613.167730	518058.644308	39.106189
2616.560289	519100.586453	39.111207
2619.338962	520147.901922	39.116224
2621.884775	521196.645775	39.121242
2624.836383	522238.146088	39.126260
2627.253343	523286.817307	39.131277
2629.958769	524311.042704	39.136295
2632.616530	525332.889785	39.141312
2634.760790	526338.742608	39.146330
2637.034899	527339.017100	39.151348
2639.439468	528363.971492	39.156365
2642.090464	529378.844811	39.161383
2644.577212	530399.917939	39.166400
2647.052907	531431.642908	39.171418
2649.361805	532461.561684	39.176436
2651.549253	533506.526316	39.181453
2654.315871	534550.561539	39.186471
2656.805965	535606.242522	39.191488
2658.967988	536675.487223	39.196506
2661.510863	537749.265831	39.201524
2663.708028	538832.631384	39.206541
2666.337559	539922.882860	39.211559
2669.323845	541030.845912	39.216576
2671.620560	542137.531675	39.221594
2674.210543	543245.739450	39.226612
2676.853494	544368.785822	39.231629
2678.864738	545502.207901	39.236647
2681.669155	546635.753465	39.241664
2684.001930	547781.402867	39.246682
2686.840202	548934.159602	39.251700
2689.735278	550097.264987	39.256717
2691.975193	551250.832707	39.261735
2695.206379	552420.567531	39.266752
2698.001158	553583.742269	39.271770
2701.206784	554751.017312	39.276788
2704.001770	555929.515719	39.281805
2706.679750	557102.001285	39.286823
2709.465147	558277.027387	39.291840
2711.922095	559465.718571	39.296858
2714.702503	560644.753928	39.301876
2717.239852	561836.230342	39.306893
2719.703283	563032.732882	39.311911
2722.643062	564230.500034	39.316928
2725.633927	565414.490508	39.321946
2728.842824	566609.731457	39.326964
2731.511210	567811.730450	39.331981
2734.150746	569006.844900	39.336999
2737.496459	570194.147632	39.342016
2739.926703	571411.356326	39.347034
2743.335178	572597.870636	39.352052
2746.289846	573789.368161	39.357069
2749.358494	574973.357582	39.362087
2752.516026	576159.276277	39.367104
2754.819569	577349.240664	39.372122
2757.407251	578534.327301	39.377140
2759.788239	579715.323123	39.382157
2762.690715	580909.806627	39.387175
2765.763403	582099.832113	39.392192
2767.997961	583304.374431	39.397210
2770.590409	584502.018257	39.402228
2773.371731	585705.927557	39.407245
2776.167654	586893.825022	39.412263
2778.662838	588077.897390	39.417280
2780.661096	589260.734638	39.422298
2783.695561	590433.957243	39.427316
2785.992509	591622.521361	39.432333
2788.902221	592811.712915	39.437351
2791.882800	593996.514317	39.442368
2794.857115	595183.601305	39.447386
2797.476830	596365.369560	39.452404
2800.646527	597552.282197	39.457421
2803.732137	598759.116739	39.462439
2806.976603	599935.056710	39.467456
2809.655998	601133.100588	39.472474
2812.820202	602314.167389	39.477492
2816.301814	603499.812793	39.482509
2818.781346	604686.606917	39.487527
2822.284895	605860.391413	39.492544
2824.872494	607054.325006	39.497562
2827.852724	608224.700520	39.502580
2830.520444	609421.620976	39.507597
2833.132543	610618.372772	39.512615
2835.676584	611811.356542	39.517632
2838.255273	613019.559066	39.522650
2841.411207	614223.030623	39.527668
2844.241728	615435.826022	39.532685
2847.032848	616655.093234	39.537703
2849.960318	617871.102032	39.542720
2852.467051	619092.545017	39.547738
2855.578792	620317.345543	39.552756
2858.051785	621545.864311	39.557773
2860.969989	622775.665975	39.562791
2864.342957	624006.947746	39.567808
2867.091513	625250.433035	39.572826
2870.117453	626485.135001	39.577844
2873.113260	627732.433705	39.582861
2876.009184	628969.865073	39.587879
2879.191665	630200.911033	39.592896
2882.294989	631444.357214	39.597914
2885.070368	632681.971214	39.602932
2888.123992	633914.100234	39.607949
2891.065219	635163.769204	39.612967
2894.273020	636400.617205	39.617984
2897.650282	637643.973881	39.623002
2900.616661	638870.188752	39.628020
2903.436511	640104.811829	39.633037
2906.455645	641336.857614	39.638055
2909.390937	642565.277717	39.643072
2912.250636	643801.639955	39.648090
2914.653399	645033.292280	39.653108
2917.347042	646276.808490	39.658125
2920.081940	647530.132745	39.663143
2922.704825	648782.471876	39.668160
2925.404257	650051.982492	39.673178
2928.188510	651323.857565	39.678196
2930.505449	652593.656275	39.683213
2932.735113	653870.180766	39.688231
2935.521766	655130.555901	39.693248
2938.116780	656392.146251	39.698266
2940.638622	657657.320668	39.703284
2943.100296	658931.750761	39.708301
2945.849497	660236.231197	39.713319
2949.294950	661512.791767	39.718336
2952.196697	662802.414646	39.723354
2955.126680	664091.013420	39.728372
2958.234443	665398.663096	39.733389
2960.787382	666707.521497	39.738407
2963.848193	668011.685808	39.743424
2966.652086	669327.749787	39.748442
2969.950793	670645.932420	39.753460
2973.149732	671976.774809	39.758477
2975.898648	673308.449402	39.763495
2979.478261	674632.932651	39.768512
2982.111640	675978.460898	39.773530
2984.961233	677302.091436	39.778548
2988.070958	678646.653138	39.783565
2990.742278	680005.946494	39.788583
2993.964518	681360.573281	39.793600
2997.596902	682712.644637	39.798618
3000.835294	684071.385055	39.803636
3004.340363	685413.542455	39.808653
3007.247621	686765.828392	39.813671
3010.739840	688106.892271	39.818688
3013.776231	689457.113433	39.823706
3016.914376	690800.415032	39.828724
3020.343887	692148.028505	39.833741
3023.441903	693488.252177	39.838759
3026.908905	694822.952849	39.843776
3029.957659	696171.655368	39.848794
3033.247203	697509.846865	39.853812
3036.914769	698832.451604	39.858829
3040.113209	700155.283063	39.863847
3043.384500	701465.858618	39.868864
3046.566365	702770.751405	39.873882
3049.748938	704089.021682	39.878900
3053.451272	705398.729234	39.883917
3056.039921	706714.568608	39.888935
3058.864488	708021.450047	39.893952
3062.164717	709332.555679	39.898970
3065.166177	710652.321959	39.903988
3068.153833	711964.460677	39.909005
3071.020314	713288.046197	39.914023
3073.697392	714594.236701	39.919040
3076.856833	715931.359220	39.924058
3079.601690	717263.689152	39.929076
3082.692746	718587.092114	39.934093
3085.803741	719926.648772	39.939111
3088.736564	721267.601439	39.944128
3091.659371	722617.977618	39.949146
3094.493837	723963.896827	39.954164
3097.424078	725310.715524	39.959181
3100.425213	726667.478577	39.964199
3103.756354	727973.817672	39.969216
3106.749206	729288.648300	39.974234
3109.609413	730599.041074	39.979252
3113.174679	731896.608438	39.984269
3116.042877	733215.314327	39.989287
3119.380310	734524.147399	39.994304
3122.428296	735845.598107	39.999322
3125.453316	737147.885467	40.004340
3128.537960	738467.118408	40.009357
3130.768900	739807.537965	40.014375
3133.539665	741147.785916	40.019392
3136.077290	742509.739785	40.024410
3138.680013	743888.800765	40.029428
3141.772162	745275.372849	40.034445
3144.067369	746681.400628	40.039463
3146.976575	748097.121575	40.044480
3149.811546	749519.543158	40.049498
3152.499036	750950.495815	40.054516
3156.185236	752392.831537	40.059533
3158.929347	753854.210917	40.064551
3162.439532	755317.198576	40.069568
3165.210642	756791.007602	40.074586
3168.292579	758289.574822	40.079604
3171.031521	759785.296248	40.084621
3173.964215	761289.296357	40.089639
3177.163812	762805.786132	40.094656
3179.873141	764347.031310	40.099674
3182.806509	765889.788093	40.104692
3186.084796	767437.326753	40.109709
3188.843755	769002.124754	40.114727
3192.082277	770561.940301	40.119744
3195.403126	772140.223727	40.124762
3198.524313	773730.134851	40.129780
3202.267741	775308.841405	40.134797
3205.740553	776893.927639	40.139815
3209.028448	778480.024174	40.144832
3212.402534	780063.108467	40.149850
3215.865323	781652.746395	40.154868
3219.323229	783240.807018	40.159885
3222.823361	784844.247334	40.164903
3225.871258	786433.531008	40.169920
3229.533551	788028.872575	40.174938
3232.644375	789610.767759	40.179956
3236.157224	791201.400366	40.184973
3239.008839	792811.523774	40.189991
3242.160995	794409.424864	40.195008
3245.428818	796007.919440	40.200026
3248.590440	797614.238314	40.205044
3251.750611	799215.389744	40.210061
3254.988118	800840.666088	40.215079
3258.297547	802462.416102	40.220096
3261.894355	804061.974006	40.225114
3264.652911	805686.281467	40.230132
3268.214625	807293.984648	40.235149
3271.064033	808911.298854	40.240167
3274.210780	810494.272670	40.245184
3277.693760	812078.233612	40.250202
3280.246740	813670.280602	40.255220
3284.254380	815255.549678	40.260237
3287.192914	816848.335723	40.265255
3290.501224	818428.820231	40.270272
3293.549382	820013.264948	40.275290
3296.514890	821596.855911	40.280308
3300.123829	823181.418736	40.285325
3303.282623	824788.098968	40.290343
3306.032008	826399.814992	40.295360
3309.746507	828018.275878	40.300378
3312.303835	829634.874709	40.305396
3315.557719	831270.527296	40.310413
3318.711064	832922.968072	40.315431
3321.886075	834570.112964	40.320448
3325.518346	836227.801989	40.325466
3328.730251	837887.175357	40.330484
3331.935120	839552.779925	40.335501
3334.959580	841241.024305	40.340519
3338.508370	842927.950152	40.345536
3341.837198	844617.863056	40.350554
3345.145899	846311.016298	40.355572
3348.377077	848014.117883	40.360589
3351.665018	849726.940767	40.365607
3355.071730	851445.581135	40.370624
3358.567102	853163.146353	40.375642
3361.817303	854901.621383	40.380660
3365.258798	856622.499012	40.385677
3368.495805	858361.352904	40.390695
3372.087510	860089.858575	40.395712
3375.626054	861826.313578	40.400730
3378.578469	863578.842239	40.405748
3382.382936	865331.975554	40.410765
3385.634831	867089.146284	40.415783
3389.052479	868841.029672	40.420800
3392.769849	870585.669918	40.425818
3395.550505	872355.693814	40.430836
3399.349930	874110.120111	40.435853
3402.949138	875881.560635	40.440871
3405.828486	877649.304201	40.445888
3409.947310	879420.265253	40.450906
3413.082418	881192.403051	40.455924
3416.983900	882964.063773	40.460941
3420.342319	884724.849184	40.465959
3424.081225	886501.344573	40.470976
3427.744382	888254.727195	40.475994
3431.601077	890021.527458	40.481012
3435.036262	891778.596943	40.486029
3438.290687	893547.590957	40.491047
3441.336717	895319.442534	40.496064
3445.029359	897088.702427	40.501082
3448.100256	898862.328849	40.506100
3451.450905	900627.453294	40.511117
3454.618591	902384.215759	40.516122
3457.575560	904111.329595	40.521127
3461.281366	905758.511536	40.526132
3464.413237	907359.991590	40.531136
3467.427494	908884.503219	40.536141
3470.397384	910343.466045	40.541146
3473.765957	911718.263773	40.546151
3476.960387	913020.227926	40.551156
3479.898916	914246.535021	40.556160
3483.190923	915397.612615	40.561165
3485.760474	916463.681860	40.566170
3487.833328	917451.586019	40.571175
3490.797806	918367.576654	40.576180
3493.507228	919219.004184	40.581184
3495.928793	919989.745752	40.586189
3498.374626	920684.494841	40.591194
3500.489272	921313.438130	40.596199
3502.498351	921873.867906	40.601204
3504.255887	922388.231167	40.606208
3506.201230	922833.490549	40.611213
3507.713449	923218.708870	40.616218
3508.937506	923557.331034	40.621223
3510.453576	923850.324087	40.626228
3511.915704	924099.676748	40.631232
3513.078690	924303.995383	40.636237
3514.166552	924464.015740	40.641242
3515.169476	924591.659971	40.646247
3516.321311	924675.070292	40.651252
3517.420257	924720.433523	40.656256
3518.892580	924731.137407	40.661261
3519.562759	924712.091646	40.666266
3520.367004	924662.463417	40.671271
3521.348289	924575.421372	40.676276
3521.965586	924477.388248	40.681280
3522.688971	924338.778986	40.686285
3523.714725	924183.391762	40.691290
3524.263050	923994.730994	40.696295
3525.036095	923787.763392	40.701300
3525.631809	923575.435418	40.706304
3526.143094	923324.375865	40.711309
3526.800507	923059.821699	40.716314
3526.740141	922770.574682	40.721319
3527.237614	922479.870913	40.726324
3527.758525	922186.070814	40.731328
3527.701424	921852.259031	40.736333
3528.263080	921536.013520	40.741338
3528.272573	921191.668424	40.746343
3528.692977	920834.056167	40.751348
3528.753252	920477.924266	40.756352
3528.819551	920100.223302	40.761357
3529.191854	919736.583242	40.766362
3529.354848	919364.296957	40.771367
3529.965250	918966.992592	40.776372
3529.939741	918566.977553	40.781376
3529.961626	918154.416828	40.786381
3530.345833	917733.776307	40.791386
3530.643020	917320.239058	40.796391
3530.630176	916884.011039	40.801396
3530.676768	916463.810862	40.806400
3530.946155	916019.380574	40.811405
3530.976783	915586.698597	40.816410
3531.066851	915143.189952	40.821415
3531.156586	914687.418077	40.826420
3531.399244	914234.374262	40.831424
3531.345654	913773.447367	40.836429
3531.448788	913318.329190	40.841434
3531.501491	912845.653421	40.846439
3531.896909	912365.461832	40.851444
3531.790540	911899.377441	40.856448
3531.823827	911409.627601	40.861453
3532.098526	910946.672569	40.866458
3532.196536	910468.870596	40.871463
3532.309609	909968.572671	40.876468
3532.051075	909483.229831	40.881472
3532.481944	908993.196803	40.886477
3532.696867	908500.651056	40.891482
3532.481653	907998.784512	40.896487
3532.473534	907497.126213	40.901492
3532.330902	907003.158304	40.906496
3532.512209	906489.517612	40.911501
3532.529222	905978.268083	40.916506
3532.747345	905476.291617	40.921511
3532.783835	904962.051963	40.926516
3532.558969	904453.210872	40.931520
3532.841239	903931.310322	40.936525
3532.564465	903424.506245	40.941530
3532.660350	902909.005481	40.946535
3532.915725	902388.894736	40.951540
3532.872199	901877.375147	40.956544
3532.803121	901344.001899	40.961549
3533.292603	900824.091642	40.966554
3532.613213	900302.305579	40.971559
3532.729171	899771.453768	40.976564
3533.046730	899255.675065	40.981568
3532.965992	898717.709372	40.986573
3533.430171	898183.751468	40.991578
3533.136161	897653.638724	40.996583
3533.420948	897111.883983	41.001588
3533.150262	896579.831235	41.006592
3533.288557	896044.277513	41.011597
3533.251963	895510.152071	41.016602
3532.811860	894979.426770	41.021607
3532.976226	894433.184663	41.026612
3533.177526	893883.694604	41.031616
3532.791360	893348.845351	41.036621
3533.002029	892812.007414	41.041626
3532.906888	892276.234354	41.046631
3533.093322	891738.139326	41.051636
3532.869214	891200.353656	41.056640
3532.829036	890657.264524	41.061645
3532.977035	890116.509196	41.066650
3532.612987	889577.627669	41.071655
3533.057356	889028.498549	41.076660
3533.169039	888495.624133	41.081664
3533.176187	887950.238873	41.086669
3533.177649	887396.772774	41.091674
3533.021539	886849.279233	41.096679
3533.325382	886300.590688	41.101684
3533.132517	885752.805689	41.106688
3532.978001	885204.865351	41.111693
3533.339718	884650.009365	41.116698
3533.032668	884098.118402	41.121703
3533.201479	883550.062880	41.126708
3533.339079	883002.154510	41.131712
3532.991160	882445.078401	41.136717
3533.036465	881880.521908	41.141722
3532.638540	881329.157747	41.146727
3533.016504	880777.512050	41.151732
3533.238836	880229.231071	41.156736
3533.187160	879663.313822	41.161741
3532.974095	879104.248197	41.166746
3532.896655	878546.268705	41.171751
3532.911732	877987.251190	41.176756
3532.763235	877440.031731	41.181760
3532.773030	876884.108099	41.186765
3532.811169	876328.127013	41.191770
3532.708451	875774.734810	41.196775
3532.987890	875211.627284	41.201780
3532.769201	874658.149973	41.206784
3532.723740	874098.870026	41.211789
3532.978331	873541.328476	41.216794
3532.962018	872983.392662	41.221799
3533.357571	872417.865268	41.226804
3532.818755	871857.390690	41.231808
3532.918302	871287.925867	41.236813
3532.849846	870728.137506	41.241818
3532.468873	870162.915958	41.246823
3532.655053	869593.468156	41.251828
3532.643408	869033.704858	41.256832
3532.772990	868462.605932	41.261837
3532.841695	867905.829121	41.266842
3532.750052	867345.824259	41.271847
3533.069500	866770.551140	41.276852
3532.977421	866214.809596	41.281856
3532.771535	865632.137606	41.286861
3532.897070	865077.321814	41.291866
3532.909682	864512.567443	41.296871
3532.690316	863932.646855	41.301876
3532.787974	863371.947819	41.306880
3532.882735	862806.145298	41.311885
3532.620951	862234.521005	41.316890
3532.766103	861664.716636	41.321895
3532.712731	861091.588458	41.326900
3532.490982	860528.056521	41.331904
3532.442068	859954.723009	41.336909
3532.557990	859386.653650	41.341914
3532.796833	858824.829305	41.346919
3533.075667	858253.807207	41.351924
3532.988117	857678.126974	41.356928
3532.872675	857097.243340	41.361933
3532.963214	856519.186924	41.366938
3532.730537	855951.927120	41.371943
3533.143045	855377.403922	41.376948
3532.839316	854794.388589	41.381952
3532.734227	854215.175562	41.386957
3533.059370	853636.515625	41.391962
3532.983601	853062.637806	41.396967
3532.812805	852469.064881	41.401972
3532.561935	851905.814127	41.406976
3532.917042	851316.128279	41.411981
3532.758877	850742.048865	41.416986
3532.936464	850156.176589	41.421991
3533.240850	849568.377446	41.426996
3532.467360	848992.683326	41.432000
3532.402911	848412.140582	41.437005
3532.858266	847839.148701	41.442010
3532.368268	847262.759189	41.447015
3532.500040	846674.618805	41.452020
3532.665796	846103.075448	41.457024
3532.650269	845521.086306	41.462029
3532.557836	844935.158819	41.467034
3532.520550	844355.695862	41.472039
3532.835960	843781.966341	41.477044
3532.554663	843200.684328	41.482048
3532.352768	842611.050059	41.487053
3532.550589	842015.151139	41.492058
3532.293402	841436.626593	41.497063
3532.246239	840860.353124	41.502068
3532.148446	840275.357691	41.507072
3532.391236	839704.292271	41.512077
3532.227430	839116.860736	41.517082
3532.279189	838543.577869	41.522087
3532.662541	837949.068794	41.527092
3532.357256	837378.619315	41.532096
3532.504115	836795.456319	41.537101
3532.516284	836202.945147	41.542106
3532.295479	835619.395926	41.547111
3532.173320	835037.289176	41.552116
3531.984307	834456.312030	41.557120
3531.893238	833871.946922	41.562125
3531.702041	833291.010948	41.567130
3531.380082	832717.366405	41.572135
3531.744361	832148.483886	41.577140
3531.918592	831574.262207	41.582144
3531.591774	831004.713195	41.587149
3531.681435	830428.353328	41.592154
3531.581765	829855.392662	41.597159
3531.714430	829279.997408	41.602164
3531.590985	828706.401893	41.607168
3531.439319	828124.505528	41.612173
3531.492912	827552.389687	41.617178
3531.414641	826984.984877	41.622183
3531.878865	826402.145238	41.627188
3531.702239	825828.940033	41.632192
3531.601825	825254.498638	41.637197
3531.647754	824674.361507	41.642202
3531.404097	824106.490206	41.647207
3531.484265	823519.646625	41.652212
3531.464734	822950.317090	41.657216
3531.706479	822369.062492	41.662221
3531.781221	821789.789622	41.667226
3531.562826	821208.853289	41.672231
3531.322335	820624.739784	41.677236
3531.312212	820055.891720	41.682240
3531.287790	819479.905121	41.687245
3531.287664	818899.510811	41.692250
3531.378990	818325.556212	41.697255
3531.391102	817742.661451	41.702260
3531.523238	817171.682202	41.707264
3531.463524	816592.221498	41.712269
3531.575750	816009.842698	41.717274
3530.991561	815428.363855	41.722279
3531.191571	814845.868380	41.727284
3530.907635	814281.124095	41.732288
3530.907831	813713.346442	41.737293
3530.989634	813125.679174	41.742298
3531.143263	812560.764018	41.747303
3531.109143	811976.247264	41.752308
3531.124866	811397.057807	41.757312
3530.941564	810822.553944	41.762317
3531.215664	810245.963880	41.767322
3530.878678	809677.168016	41.772327
3531.013053	809087.424617	41.777332
3530.960245	808510.938172	41.782336
3530.698617	807940.562611	41.787341
3530.839693	807367.179375	41.792346
3530.690745	806797.913450	41.797351
3530.738609	806223.714541	41.802356
3530.744016	805647.072873	41.807360
3530.597412	805075.898051	41.812365
3530.909696	804507.244099	41.817370
3530.838837	803925.715037	41.822375
3531.210742	803339.060102	41.827380
3530.891399	802763.848303	41.832384
3530.934642	802192.400166	41.837389
3530.849484	801610.284680	41.842394
3530.455158	801036.755392	41.847399
3530.579240	800459.018781	41.852404
3530.551687	799888.470304	41.857408
3530.722986	799314.799189	41.862413
3531.009916	798736.448999	41.867418
3530.815437	798157.641979	41.872423
3530.862620	797582.523602	41.877428
3530.749642	797003.949760	41.882432
3530.859020	796425.584189	41.887437
3530.540439	795835.169622	41.892442
3530.280787	795267.077709	41.897447
3530.086658	794687.097813	41.902452
3530.180256	794114.973672	41.907456
3530.299247	793546.922499	41.912461
3530.593009	792974.916365	41.917466
3530.353132	792406.981235	41.922471
3530.265885	791828.710226	41.927476
3530.274448	791252.880000	41.932480
3530.248736	790678.580204	41.937485
3530.099169	790110.296596	41.942490
3529.910131	789547.819782	41.947495
3530.253120	788965.703053	41.952500
3530.216650	788403.452930	41.957504
3529.828113	787823.823710	41.962509
3530.428709	787251.988180	41.967514
3530.529379	786676.358587	41.972519
3530.153000	786100.567173	41.977524
3530.513401	785523.816891	41.982528
3530.478552	784948.316289	41.987533
3530.304653	784363.894822	41.992538
3530.101096	783789.066894	41.997543
3529.980029	783202.820612	42.002548
3529.790355	782633.797715	42.007552
3529.651354	782070.474651	42.012557
3529.876216	781496.176305	42.017562
3529.920276	780928.109356	42.022567
3529.976539	780343.517301	42.027572
3529.961304	779777.583146	42.032576
3529.744235	779204.259577	42.037581
3530.179964	778633.485045	42.042586
3529.799568	778067.085536	42.047591
3529.996578	777487.207761	42.052596
3530.157134	776919.691219	42.057600
3529.666654	776343.038091	42.062605
3529.830689	775766.325890	42.067610
3529.666249	775196.072339	42.072615
3529.615848	774617.976742	42.077620
3529.425525	774053.890133	42.082624
3529.573799	773485.024817	42.087629
3529.653338	772923.759013	42.092634
3529.511700	772353.328811	42.097639
3529.415329	771786.638474	42.102644
3528.915864	771216.427180	42.107648
3529.239253	770654.847649	42.112653
3529.490627	770075.406212	42.117658
3529.205523	769512.907590	42.122663
3529.322420	768947.735648	42.127668
3529.565717	768386.095550	42.132672
3529.477262	767820.182702	42.137677
3529.562683	767242.813993	42.142682
3529.160592	766680.859116	42.147687
3529.591096	766105.560652	42.152692
3529.706779	765541.903437	42.157696
3529.267094	764963.609379	42.162701
3528.986886	764387.165762	42.167706
3529.040956	763833.742012	42.172711
3529.146365	763269.619057	42.177716
3529.139524	762707.691553	42.182720
3529.180717	762139.747138	42.187725
3529.326766	761565.429605	42.192730
3528.537484	761012.878459	42.197735
3528.812427	760446.492265	42.202740
3528.996584	759884.468945	42.207744
3528.645940	759329.351778	42.212749
3529.136104	758762.161096	42.217754
3528.581841	758207.292254	42.222759
3528.717155	757641.064850	42.227764
3528.607088	757081.745157	42.232768
3528.626697	756513.134173	42.237773
3528.768144	755940.561125	42.242778
3528.499340	755394.321065	42.247783
3528.507238	754832.002570	42.252788
3528.648045	754277.419112	42.257792
3528.558097	753720.020971	42.262797
3528.687272	753150.992459	42.267802
3528.753024	752601.484078	42.272807
3528.592769	752037.063311	42.277812
3528.825597	751482.459296	42.282816
3528.769555	750909.691515	42.287821
3528.546687	750345.898059	42.292826
3528.486339	749781.294769	42.297831
3528.625103	749217.702869	42.302836
3528.758636	748669.235914	42.307840
3528.480613	748098.372144	42.312845
3528.526558	747536.995592	42.317850
3528.455459	746972.979762	42.322855
3528.179764	746417.901521	42.327860
3528.518119	745862.777682	42.332864
3528.407665	745307.344984	42.337869
3528.462872	744743.393177	42.342874
3528.269102	744186.906531	42.347879
3528.504655	743628.181518	42.352884
3528.097382	743064.681931	42.357888
3527.875622	742508.723453	42.362893
3527.945310	741953.269140	42.367898
3527.819650	741403.544421	42.372903
3528.176453	740853.847296	42.377908
3528.054510	740300.781485	42.382912
3527.953494	739751.679136	42.387917
3528.014154	739178.820829	42.392922
3528.065482	738635.154225	42.397927
3527.925088	738076.346906	42.402932
3527.654503	737521.084161	42.407936
3527.904321	736964.308565	42.412941
3527.798668	736417.004414	42.417946
3527.930066	735876.697590	42.422951
3527.760312	735307.409305	42.427956
3527.694727	734770.079601	42.432960
3527.598303	734218.614842	42.437965
3527.519748	733662.654782	42.442970
3527.600909	733118.953256	42.447975
3527.214847	732578.660590	42.452980
3527.583898	732020.876988	42.457984
3527.529794	731490.701511	42.462989
3527.904561	730938.980700	42.467994
3527.791803	730394.930276	42.472999
3527.829799	729839.082336	42.478004
3527.541057	729280.924615	42.483008
3527.206463	728734.324477	42.488013
3527.743383	728181.348035	42.493018
3527.381795	727642.603103	42.498023
3527.451699	727092.405956	42.503028
3527.463174	726540.101135	42.508032
3527.325322	725998.088503	42.513037
3527.226002	725447.759783	42.518042
3527.136813	724913.494582	42.523047
3527.209903	724360.437408	42.528052
3527.140690	723818.813762	42.533056
3527.314036	723275.824542	42.538061
3527.435032	722725.771082	42.543066
3527.234817	722188.274875	42.548071
3527.079261	721638.741235	42.553076
3526.904548	721096.312135	42.558080
3526.586443	720558.135079	42.563085
3526.924504	720020.802499	42.568090
3526.917563	719479.726054	42.573095
3527.011090	718931.705371	42.578100
3526.925376	718404.950929	42.583104
3526.719576	717864.150323	42.588109
3526.974620	717325.318754	42.593114
3526.619170	716786.804581	42.598119
3526.817892	716239.729528	42.603124
3526.981206	715711.621758	42.608128
3526.526506	715167.415402	42.613133
3526.490985	714635.950348	42.618138
3526.155724	714107.429820	42.623143
3526.547876	713570.268037	42.628148
3526.638817	713035.008835	42.633152
3526.665991	712507.367931	42.638157
3526.849337	711969.197031	42.643162
3526.267858	711439.757316	42.648167
3526.428779	710905.790396	42.653172
3526.658211	710372.721148	42.658176
3526.480717	709835.518548	42.663181
3526.598160	709290.537708	42.668186
3526.255813	708764.265617	42.673191
3526.068659	708225.672349	42.678196
3526.352222	707698.929774	42.683200
3526.121105	707171.001330	42.688205
3526.505535	706633.103788	42.693210
3526.211948	706112.469467	42.698215
3526.109093	705583.577116	42.703220
3526.212139	705053.872099	42.708224
3526.130812	704527.046553	42.713229
3526.167921	703996.145372	42.718234
3525.445314	703473.139702	42.723239
3525.488562	702951.263135	42.728244
3525.904927	702431.725585	42.733248
3525.695494	701903.023046	42.738253
3525.823793	701384.465491	42.743258
3525.912378	700864.244069	42.748263
3525.946633	700335.056601	42.753268
3525.651992	699815.384450	42.758272
3525.787693	699291.830946	42.763277
3525.783648	698771.599708	42.768282
3525.415047	698249.809273	42.773287
3525.723972	697735.029523	42.778292
3525.728213	697208.789068	42.783296
3525.344848	696693.668691	42.788301
3525.328469	696179.698280	42.793306
3525.514348	695655.371990	42.798311
3525.593068	695133.419312	42.803316
3525.984275	694626.149926	42.808321
3525.316093	694094.020475	42.813325
3525.483490	693578.723387	42.818330
3525.375860	693059.713429	42.823335
3525.453290	692540.044678	42.828340
3525.484461	692028.957885	42.833345
3525.329848	691512.103608	42.838349
3525.226697	690987.948094	42.843354
3525.497390	690478.422617	42.848359
3525.361710	689957.097304	42.853364
3525.308137	689434.384267	42.858369
3524.985171	688935.419431	42.863373
3525.504629	688424.241800	42.868378
3525.196701	687911.982067	42.873383
3525.600584	687381.905837	42.878388
3525.616871	686870.476887	42.883393
3524.975321	686358.235372	42.888397
3525.262664	685839.186591	42.893402
3525.153574	685325.352168	42.898407
3524.992491	684811.447643	42.903412
3525.202991	684293.667248	42.908417
3525.025133	683790.460096	42.913421
3525.493712	683276.211704	42.918426
3525.158533	682762.071450	42.923431
3525.173772	682244.058212	42.928436
3525.199922	681734.379028	42.933441
3524.834727	681218.613217	42.938445
3524.818479	680700.218951	42.943450
3524.707825	680199.889624	42.948455
3524.668233	679696.582360	42.953460
3524.612919	679194.196515	42.958465
3524.610424	678676.233356	42.963469
3524.676973	678168.490759	42.968474
3524.826442	677662.051051	42.973479
3524.390084	677158.921766	42.978484
3524.678772	676664.011259	42.983489
3524.266901	676160.424864	42.988493
3524.309253	675656.633878	42.993498
3524.383119	675152.859974	42.998503
3524.174172	674652.944094	43.003508
3524.403588	674156.564427	43.008513
3524.188531	673659.038085	43.013517
3524.539097	673147.582923	43.018522
3524.210144	672660.688557	43.023527
3524.237091	672166.829408	43.028532
3524.392933	671661.207918	43.033537
3523.960503	671164.582858	43.038541
3523.929245	670662.080034	43.043546
3523.784573	670176.022167	43.048551
3523.993891	669675.419783	43.053556
3523.994844	669185.945420	43.058561
3523.626911	668697.605642	43.063565
3523.913906	668205.588292	43.068570
3523.556774	667720.188148	43.073575
3523.814939	667231.615917	43.078580
3523.915558	666739.005621	43.083585
3523.492528	666249.751030	43.088589
3523.773266	665760.999536	43.093594
3523.642913	665284.663802	43.098599
3523.544175	664786.599236	43.103604
3523.722584	664305.023792	43.108609
3523.612549	663820.479976	43.113613
3523.650486	663328.302802	43.118618
3523.430786	662854.854733	43.123623
3523.581221	662367.249203	43.128628
3523.470254	661873.326334	43.133633
3523.220366	661395.570057	43.138637
3523.320804	660908.148627	43.143642
3523.202985	660433.116750	43.148647
3522.811443	659955.063770	43.153652
3523.287865	659475.042145	43.158657
3522.820755	659010.731072	43.163661
3522.942733	658522.736515	43.168666
3522.457582	658054.688925	43.173671
3522.678693	657588.894450	43.178676
3522.994386	657121.114509	43.183681
3523.080658	656653.201513	43.188685
3522.842783	656173.288596	43.193690
3522.879073	655715.025360	43.198695
3523.134434	655238.227864	43.203700
3523.094824	654759.859577	43.208705
3522.534006	654290.995303	43.213709
3522.773142	653821.772303	43.218714
3522.957394	653348.690670	43.223719
3522.649331	652873.722489	43.228724
3522.824163	652407.389873	43.233729
3522.405244	651938.788942	43.238733
3522.978396	651476.090643	43.243738
3522.543482	651011.444721	43.248743
3522.668924	650541.435825	43.253748
3522.897024	650070.288033	43.258753
3522.409404	649612.230231	43.263757
3522.526026	649143.155951	43.268762
3522.451895	648676.540525	43.273767
3522.503587	648214.578880	43.278772
3522.588914	647746.143827	43.283777
3522.367501	647286.784442	43.288781
3521.916858	646827.343168	43.293786
3522.574408	646368.591246	43.298791
3522.491381	645905.646488	43.303796
3522.710678	645438.680153	43.308801
3522.831113	644982.805739	43.313805
3522.755409	644509.748528	43.318810
3522.787360	644042.699529	43.323815
3522.455830	643572.241549	43.328820
3522.827917	643100.141734	43.333825
3522.360143	642642.462378	43.338829
3522.817812	642169.904675	43.343834
3522.893297	641709.190556	43.348839
3522.529329	641236.529747	43.353844
3522.697161	640768.706791	43.358849
3522.172230	640307.681751	43.363853
3521.711740	639829.821382	43.368858
3521.959589	639382.075456	43.373863
3522.020721	638927.739871	43.378868
3522.000578	638464.394950	43.383873
3521.945014	638007.287590	43.388877
3522.083902	637553.228045	43.393882
3521.566348	637103.612615	43.398887
3522.049037	636645.152303	43.403892
3522.257831	636188.869607	43.408897
3521.848808	635739.026106	43.413901
3521.891133	635276.227613	43.418906
3521.960807	634825.962517	43.423911
3521.688234	634370.882727	43.428916
3522.021108	633921.884484	43.433921
3521.518029	633466.053843	43.438925
3521.814460	633013.719922	43.443930
3521.604147	632568.659475	43.448935
3521.662649	632116.026994	43.453940
3521.914492	631668.447006	43.458945
3521.522688	631224.261212	43.463949
3521.478655	630781.098409	43.468954
3521.209141	630324.340071	43.473959
3521.297904	629876.561300	43.478964
3521.134676	629423.299831	43.483969
3520.912538	628980.792416	43.488973
3521.157362	628543.193198	43.493978
3521.488142	628108.815529	43.498983
3520.952353	627664.954738	43.503988
3521.519526	627229.599393	43.508993
3520.568622	626791.581125	43.513997
3520.898797	626350.922449	43.519002
3520.658424	625921.660377	43.524007
3520.606294	625494.702576	43.529012
3520.660552	625062.901711	43.534017
3520.676696	624627.684223	43.539021
3521.087637	624199.744143	43.544026
3520.778567	623776.117210	43.549031
3520.708648	623334.901446	43.554036
3520.808084	622901.052139	43.559041
3520.457407	622480.286422	43.564045
3520.771171	622055.333081	43.569050
3520.847087	621625.393854	43.574055
3521.010845	621192.216130	43.579060
3520.600056	620769.640386	43.584065
3520.270703	620339.468625	43.589069
3520.721799	619906.290515	43.594074
3520.615099	619481.558234	43.599079
3520.554413	619050.237166	43.604084
3520.906229	618623.889774	43.609089
3520.556365	618201.905089	43.614093
3520.540277	617772.029113	43.619098
3520.227430	617352.510967	43.624103
3520.346334	616921.225266	43.629108
3520.463970	616508.216906	43.634113
3519.932667	616083.123919	43.639117
3520.273424	615660.121164	43.644122
3520.253320	615249.745511	43.649127
3520.264467	614833.233516	43.654132
3520.545072	614404.879089	43.659137
3520.101628	613997.787493	43.664141
3520.143296	613566.433337	43.669146
3520.212745	613149.246140	43.674151
3520.361388	612724.910073	43.679156
3520.360232	612310.360622	43.684161
3520.340394	611898.606801	43.689165
3519.995380	611468.640898	43.694170
3520.201759	611050.047581	43.699175
3520.054030	610633.203995	43.704180
3519.837894	610218.613215	43.709185
3519.597781	609815.495755	43.714189
3519.635582	609402.436142	43.719194
3519.490506	608986.483509	43.724199
3519.517942	608578.009488	43.729204
3519.696805	608173.958847	43.734209
3519.814638	607773.415311	43.739213
3519.806517	607358.632943	43.744218
3519.406834	606956.894626	43.749223
3519.287823	606546.264876	43.754228
3519.449230	606141.191078	43.759233
3519.109776	605745.670288	43.764237
3519.682611	605340.296868	43.769242
3519.534212	604946.722380	43.774247
3519.119762	604536.621996	43.779252
3519.127423	604133.258732	43.784257
3519.195170	603744.171703	43.789261
3519.053626	603335.637262	43.794266
3519.114400	602946.323439	43.799271
3519.125857	602545.713464	43.804276
3519.070171	602148.714240	43.809281
3518.910708	601765.369808	43.814285
3518.936085	601379.320983	43.819290
3518.764428	600981.749015	43.824295
3518.977046	600593.935315	43.829300
3519.055305	600205.278173	43.834305
3519.124618	599814.149851	43.839309
3519.229635	599417.329870	43.844314
3519.119911	599025.351996	43.849319
3518.869770	598634.187998	43.854324
3519.205092	598231.514874	43.859329
3519.066402	597852.353968	43.864333
3519.173751	597451.349379	43.869338
3519.208171	597061.087778	43.874343
3519.269540	596661.720615	43.879348
3519.176178	596262.617214	43.884353
3518.950214	595882.252055	43.889357
3518.812955	595477.706314	43.894362
3518.866607	595091.342348	43.899367
3519.010880	594697.517939	43.904372
3519.010486	594305.060901	43.909377
3519.054862	593916.399869	43.914381
3518.843083	593521.742982	43.919386
3518.616946	593137.722838	43.924391
3518.778838	592748.601312	43.929396
3518.880871	592358.271689	43.934401
3518.433207	591981.534661	43.939405
3518.401351	591597.179990	43.944410
3518.737549	591212.800214	43.949415
3518.390804	590829.026900	43.954420
3518.450796	590434.371023	43.959425
3518.113768	590066.948226	43.964429
3518.405190	589677.150919	43.969434
3518.134582	589304.267392	43.974439
3518.065669	588934.201549	43.979444
3518.462971	588553.392956	43.984449
3517.973589	588183.626833	43.989453
3518.488444	587801.970290	43.994458
3517.998226	587425.950260	43.999463
3518.112210	587045.644511	44.004468
3518.001550	586678.329974	44.009473
3517.961071	586306.720701	44.014477
3517.834464	585934.461336	44.019482
3517.859781	585567.491678	44.024487
3517.838693	585201.172119	44.029492
3517.836505	584828.455281	44.034497
3517.853807	584460.548656	44.039501
3518.067964	584093.954314	44.044506
3518.004379	583727.597350	44.049511
3517.664333	583365.750134	44.054516
3517.679562	583005.892412	44.059521
3517.277088	582632.020202	44.064525
3517.528496	582267.525876	44.069530
3517.520768	581912.365097	44.074535
3517.355226	581557.572829	44.079540
3517.582661	581194.407891	44.084545
3517.600793	580840.619201	44.089549
3517.650375	580467.960935	44.094554
3517.493283	580117.700687	44.099559
3517.346042	579756.769349	44.104564
3517.831764	579397.328348	44.109569
3517.269716	579045.145661	44.114573
3517.719729	578674.074219	44.119578
3518.064993	578325.336534	44.124583
3517.314790	577965.209900	44.129588
3517.034964	577600.114416	44.134593
3517.085649	577251.296129	44.139597
3517.232153	576896.617799	44.144602
3517.351563	576542.436882	44.149607
3517.286776	576186.416403	44.154612
3517.343514	575827.447794	44.159617
3517.180839	575486.311652	44.164621
3517.323554	575118.405241	44.169626
3517.227613	574774.270568	44.174631
3517.406113	574422.131857	44.179636
3517.310365	574066.257302	44.184641
3517.048225	573718.198269	44.189645
3516.934608	573362.256450	44.194650
3517.134290	573017.922390	44.199655
3516.753543	572668.395554	44.204660
3517.069541	572327.695273	44.209665
3516.836029	571984.664635	44.214669
3516.691263	571624.251500	44.219674
3516.971229	571286.799585	44.224679
3516.730133	570944.144464	44.229684
3516.798397	570597.804400	44.234689
3516.771303	570260.880710	44.239693
3516.935109	569912.039980	44.244698
3516.914139	569573.688032	44.249703
3516.714789	569218.801388	44.254708
3517.079698	568881.824499	44.259713
3516.615593	568543.822758	44.264717
3516.780329	568181.799504	44.269722
3516.651259	567848.956125	44.274727
3516.532423	567514.995082	44.279732
3516.581307	567163.028617	44.284737
3516.378879	566829.164614	44.289741
3516.608164	566501.459545	44.294746
3516.388030	566169.242392	44.299751
3516.605954	565836.186818	44.304756
3516.857444	565496.422036	44.309761
3516.626354	565159.549652	44.314765
3516.267417	564814.283526	44.319770
3516.276378	564479.315652	44.324775
3516.346713	564150.118013	44.329780
3516.472832	563815.868093	44.334785
3516.346214	563484.874791	44.339789
3516.625586	563156.824508	44.344794
3516.369998	562819.794694	44.349799
3516.058673	562488.404745	44.354804
3516.249595	562153.093983	44.359809
3516.246974	561827.827598	44.364813
3516.326624	561493.022375	44.369818
3516.388893	561160.024286	44.374823
3516.196135	560833.103905	44.379828
3516.435570	560499.504847	44.384833
3516.210347	560170.760635	44.389837
3516.142674	559840.067637	44.394842
3515.945523	559513.266172	44.399847
3515.861806	559182.357921	44.404852
3515.809207	558858.587577	44.409857
3515.669649	558545.904240	44.414861
3515.907223	558219.046803	44.419866
3515.971252	557895.484741	44.424871
3515.811557	557576.032755	44.429876
3515.976022	557249.415678	44.434881
3515.465473	556930.813939	44.439885
3515.824679	556608.681157	44.444890
3515.983105	556295.793051	44.449895
3515.651219	555975.626713	44.454900
3515.932004	555650.663181	44.459905
3515.383683	555342.860485	44.464909
3515.724522	555015.856182	44.469914
3515.978747	554700.395394	44.474919
3515.494639	554388.176783	44.479924
3515.850747	554065.831976	44.484929
3515.465838	553757.662596	44.489933
3515.478120	553434.353672	44.494938
3515.642156	553123.103374	44.499943
3515.487940	552801.571119	44.504948
3515.744760	552482.833065	44.509953
3515.509320	552186.594265	44.514957
3515.213750	551869.296505	44.519962
3515.194418	551559.553089	44.524967
3515.053055	551247.001483	44.529972
3515.631485	550941.626718	44.534977
3515.334570	550628.986625	44.539981
3515.209587	550322.357382	44.544986
3515.414210	550016.975240	44.549991
3514.945921	549708.929280	44.554996
3515.272153	549395.549645	44.560001
3515.099441	549099.434272	44.565005
3514.921087	548804.674252	44.570010
3514.875469	548495.520691	44.575015
3514.878726	548195.373923	44.580020
3515.207312	547889.217349	44.585025
3515.179188	547596.724237	44.590029
3515.264206	547290.747102	44.595034
3515.157417	546988.929305	44.600039
3514.598521	546683.451845	44.605044
3515.341369	546380.417051	44.610049
3515.532309	546082.359666	44.615053
3515.182447	545766.895280	44.620058
3515.525795	545473.033309	44.625063
3514.480339	545168.361549	44.630068
3515.367732	544870.965744	44.635073
3514.597603	544569.006609	44.640077
3514.679413	544262.660380	44.645082
3514.711929	543969.525432	44.650087
3514.752072	543675.626708	44.655092
3514.783105	543380.160294	44.660097
3514.578619	543088.055651	44.665101
3514.852693	542798.434731	44.670106
3514.706651	542500.509203	44.675111
3514.248500	542205.252698	44.680116
3514.438078	541914.165561	44.685121
3514.331693	541630.384372	44.690125
3514.509300	541333.235989	44.695130
3514.506293	541051.089549	44.700135
3514.303743	540775.023103	44.705140
3514.257589	540484.349996	44.710145
3514.473833	540206.486236	44.715149
3514.050616	539913.243260	44.720154
3514.114680	539626.921317	44.725159
3513.836538	539341.458958	44.730164
3514.365082	539056.054842	44.735169
3514.220740	538778.123674	44.740173
3514.357518	538495.750944	44.745178
3514.365390	538215.109529	44.750183
3514.298509	537930.339246	44.755188
3514.566510	537640.108882	44.760193
3514.094514	537368.460749	44.765197
3514.216142	537082.228923	44.770202
3514.275344	536797.717109	44.775207
3513.981674	536527.939381	44.780212
3514.284958	536237.876228	44.785217
3513.824839	535965.896683	44.790221
3514.295049	535679.930373	44.795226
3514.100936	535406.784935	44.800231
3513.692287	535132.359226	44.805236
3513.776513	534851.134144	44.810241
3513.716021	534584.155703	44.815245
3513.721245	534300.663013	44.820250
3513.889832	534032.878444	44.825255
3513.610650	533769.605370	44.830260
3513.862640	533484.339038	44.835265
3513.556107	533220.001044	44.840269
3513.544540	532948.543794	44.845274
3513.511775	532693.837294	44.850279
3512.997369	532430.226786	44.855284
3513.503947	532152.913794	44.860289
3513.417743	531900.372282	44.865293
3513.251360	531635.577776	44.870298
3513.626383	531376.438798	44.875303
3513.568585	531105.055905	44.880308
3513.397202	530846.202650	44.885313
3513.234272	530587.948948	44.890317
3513.308138	530319.153180	44.895322
3513.379867	530057.519237	44.900327
3513.298277	529794.392741	44.905332
3513.522825	529539.587170	44.910337
3513.248295	529280.067711	44.915341
3513.230816	529010.052238	44.920346
3513.421458	528753.320906	44.925351
3513.629455	528495.471727	44.930356
3513.563559	528238.977118	44.935361
3513.100685	527974.469869	44.940365
3513.412885	527710.784575	44.945370
3513.529698	527452.125115	44.950375
3512.899709	527204.744146	44.955380
3513.195081	526941.704218	44.960385
3512.933102	526682.793116	44.965389
3513.264163	526432.054961	44.970394
3512.905411	526182.439970	44.975399
3512.812986	525930.503632	44.980404
3512.810510	525667.189085	44.985409
3512.912753	525429.951950	44.990413
3512.874148	525177.236423	44.995418
3513.021491	524924.636321	45.000423
3512.734055	524672.257639	45.005428
3512.592340	524427.321861	45.010433
3512.838685	524184.284832	45.015437
3512.679200	523930.306667	45.020442
3512.887602	523685.248483	45.025447
3512.832306	523443.109258	45.030452
3512.858569	523198.377165	45.035457
3512.753094	522947.907518	45.040461
3512.905603	522697.945072	45.045466
3512.796359	522456.455575	45.050471
3512.924328	522215.881097	45.055476
3513.053226	521956.568954	45.060481
3512.926897	521705.981241	45.065485
3512.768156	521451.860134	45.070490
3512.744604	521212.961956	45.075495
3512.685652	520963.612885	45.080500
3512.640202	520713.752416	45.085505
3512.514648	520477.688026	45.090509
3512.582960	520241.182860	45.095514
3512.467945	519995.362518	45.100519
3512.559383	519760.764997	45.105524
3512.540805	519512.698291	45.110529
3512.528759	519281.545284	45.115533
3512.261147	519042.957706	45.120538
3512.468048	518801.154034	45.125543
3512.210864	518564.425911	45.130548
3512.713741	518331.604923	45.135553
3512.203820	518092.639837	45.140557
3511.880443	517859.750728	45.145562
3512.179511	517630.994600	45.150567
3512.060125	517398.013148	45.155572
3512.424471	517164.844550	45.160577
3512.299311	516932.766236	45.165581
3512.140893	516703.013680	45.170586
3512.113754	516471.517834	45.175591
3511.955302	516238.222433	45.180596
3512.144062	516004.611651	45.185601
3511.771685	515789.076672	45.190605
3511.835879	515552.600950	45.195610
3512.173081	515325.572203	45.200615
3511.905251	515104.655047	45.205620
3512.084613	514869.917371	45.210625
3512.123972	514653.740603	45.215629
3511.731563	514417.881266	45.220634
3511.397972	514195.244729	45.225639
3511.528177	513980.710282	45.230644
3511.716271	513755.957540	45.235649
3511.766127	513535.974310	45.240653
3511.858318	513311.029448	45.245658
3511.543016	513100.247187	45.250663
3511.390366	512888.575390	45.255668
3511.561720	512668.912892	45.260673
3511.774843	512450.048606	45.265677
3511.703586	512224.913946	45.270682
3511.909855	512018.070237	45.275687
3511.564055	511795.300569	45.280692
3511.718717	511576.080391	45.285697
3511.695545	511356.887525	45.290701
3511.790046	511132.365812	45.295706
3511.763434	510910.539739	45.300711
3511.378418	510704.032388	45.305716
3511.303545	510483.724517	45.310721
3511.572614	510271.642312	45.315725
3511.560527	510052.985320	45.320730
3511.421640	509839.754172	45.325735
3511.078609	509631.760151	45.330740
3511.565228	509420.286370	45.335745
3511.414228	509212.658358	45.340749
3511.332237	509001.175013	45.345754
3511.492982	508787.777505	45.350759
3511.337750	508576.098865	45.355764
3511.558588	508365.161831	45.360769
3511.197052	508165.591867	45.365773
3511.229007	507937.750531	45.370778
3511.479482	507727.355959	45.375783
3511.206931	507518.513644	45.380788
3511.371713	507308.481991	45.385793
3510.878952	507104.372342	45.390797
3510.841609	506902.406269	45.395802
3510.974614	506699.650398	45.400807
3510.783809	506493.813451	45.405812
3511.162725	506292.830089	45.410817
3511.212052	506099.482471	45.415821
3511.067635	505883.520492	45.420826
3511.247674	505692.875222	45.425831
3510.973327	505491.336283	45.430836
3511.245140	505275.092894	45.435841
3511.110188	505081.410693	45.440845
3510.718428	504879.580870	45.445850
3511.094928	504674.735947	45.450855
3510.851022	504478.082621	45.455860
3510.942797	504269.135958	45.460865
3511.111066	504077.361513	45.465869
3511.050959	503869.345588	45.470874
3511.205411	503674.636646	45.475879
3510.793910	503472.641023	45.480884
3511.086675	503271.078751	45.485889
3510.948734	503077.676478	45.490893
3510.603559	502871.314262	45.495898
3510.791119	502672.543167	45.500903
3511.183896	502485.211230	45.505908
3511.001177	502280.532774	45.510913
3510.836798	502087.628874	45.515917
3510.886951	501885.838141	45.520922
3511.127139	501678.602529	45.525927
3510.646957	501483.571348	45.530932
3511.119412	501290.599894	45.535937
3511.031890	501101.564504	45.540941
3510.844288	500896.768485	45.545946
3510.812727	500699.123260	45.550951
3510.737831	500499.460507	45.555956
3510.888767	500306.481851	45.560961
3510.553138	500122.281206	45.565965
3510.489678	499924.581578	45.570970
3510.633099	499731.546920	45.575975
3509.885192	499543.617748	45.580980
3510.164033	499349.089068	45.585985
3510.583707	499166.771509	45.590989
3509.997077	498984.927178	45.595994
3510.475936	498802.190958	45.600999
3510.084435	498625.163996	45.606004
3510.311683	498436.550072	45.611009
3510.489731	498261.343654	45.616013
3510.235338	498065.879576	45.621018
3510.375781	497883.241617	45.626023
3510.486577	497714.463555	45.631028
3510.158717	497513.594299	45.636033
3510.207679	497330.611899	45.641037
3509.960612	497154.454968	45.646042
3509.927430	496973.657370	45.651047
3509.956441	496795.729984	45.656052
3510.114584	496614.390088	45.661057
3509.601287	496446.666728	45.666061
3509.679534	496269.989758	45.671066
3509.917233	496092.676776	45.676071
3509.705009	495933.697324	45.681076
3509.869028	495749.666461	45.686081
3509.966832	495574.091559	45.691085
3509.764703	495406.355259	45.696090
3509.713337	495235.455595	45.701095
3509.461452	495065.296561	45.706100
3510.078362	494901.917045	45.711105
3509.929964	494736.795114	45.716109
3509.705273	494548.973335	45.721114
3510.006405	494373.958211	45.726119
3509.701425	494202.838491	45.731124
3510.018998	494035.606834	45.736129
3509.815000	493864.820540	45.741133
3509.919445	493692.259989	45.746138
3509.681474	493524.561722	45.751143
3509.882412	493349.654305	45.756148
3510.018928	493173.946713	45.761153
3509.818740	493011.447289	45.766157
3509.400127	492839.877952	45.771162
3509.665118	492672.540688	45.776167
3509.546315	492508.353181	45.781172
3509.369730	492348.018682	45.786177
3509.085822	492179.960894	45.791181
3509.409803	492015.440098	45.796186
3509.612240	491854.935077	45.801191
3509.452271	491700.156552	45.806196
3509.519399	491544.578991	45.811201
3509.420823	491380.478379	45.816205
3509.347731	491211.767990	45.821210
3509.508388	491051.464944	45.826215
3509.358563	490893.743054	45.831220
3509.287242	490727.253683	45.836225
3509.359963	490573.335940	45.841229
3508.829877	490416.686474	45.846234
3509.422358	490261.209963	45.851239
3509.399132	490107.506817	45.856244
3509.384382	489938.672788	45.861249
3509.252492	489789.741347	45.866253
3509.147585	489634.580650	45.871258
3509.431555	489462.351593	45.876263
3509.257856	489325.111177	45.881268
3509.391133	489160.848631	45.886273
3509.444367	489013.245032	45.891277
3509.189250	488849.956624	45.896282
3509.384984	488688.816061	45.901287
3509.318071	488536.573791	45.906292
3509.404021	488369.478249	45.911297
3509.276146	488215.118363	45.916301
3508.676207	488063.620768	45.921306
3508.954293	487907.822610	45.926311
3509.004497	487772.656947	45.931316
3509.033431	487613.811988	45.936321
3508.875254	487466.787978	45.941325
3508.652001	487325.188382	45.946330
3508.975898	487171.905987	45.951335
3508.559141	487030.235831	45.956340
3508.986351	486874.402984	45.961345
3508.970490	486731.447448	45.966349
3508.968146	486591.878991	45.971354
3508.933457	486437.892313	45.976359
3508.699488	486291.934085	45.981364
3508.989003	486140.723386	45.986369
3508.578630	485994.286734	45.991373
3508.483196	485855.183772	45.996378
3508.901937	485709.564720	46.001383
3508.598885	485575.758211	46.006388
3508.629509	485425.142251	46.011393
3508.663242	485281.913397	46.016397
3508.500160	485152.786417	46.021402
3508.576312	485004.132851	46.026407
3508.707310	484863.920587	46.031412
3509.072946	484715.721267	46.036417
3508.860390	484572.629929	46.041421
3508.640976	484430.449611	46.046426
3508.820883	484289.364040	46.051431
3508.929126	484145.050392	46.056436
3509.041823	483999.874392	46.061441
3509.181107	483852.010165	46.066445
3509.002263	483702.630003	46.071450
3509.027999	483556.807247	46.076455
3508.558962	483414.914470	46.081460
3508.568623	483266.966273	46.086465
3508.572604	483127.622406	46.091469
3508.774474	482991.837369	46.096474
3509.010309	482855.589953	46.101479
3508.385293	482713.009583	46.106484
3508.808372	482573.235504	46.111489
3508.378394	482433.302284	46.116493
3508.635236	482287.783991	46.121498
3508.583995	482148.745606	46.126503
3508.639516	482019.254787	46.131508
3508.558382	481875.815584	46.136513
3508.545652	481745.119582	46.141517
3508.457030	481614.334346	46.146522
3508.931843	481473.327967	46.151527
3508.392443	481334.417227	46.156532
3508.557081	481200.447268	46.161537
3508.600789	481062.700376	46.166541
3508.643977	480918.877939	46.171546
3508.407807	480787.706897	46.176551
3508.077537	480659.841410	46.181556
3508.380374	480524.729127	46.186561
3508.338155	480389.674749	46.191565
3508.181334	480258.587547	46.196570
3508.599112	480122.592026	46.201575
3508.408372	480000.722257	46.206580
3508.522170	479855.512421	46.211585
3508.436851	479722.991633	46.216589
3508.135669	479595.518626	46.221594
3508.083441	479469.419728	46.226599
3508.404028	479349.584531	46.231604
3508.146788	479214.051814	46.236609
3508.159161	479081.610898	46.241613
3508.154185	478953.880288	46.246618
3508.197355	478824.469855	46.251623
3508.198356	478700.432237	46.256628
3507.993698	478563.366845	46.261633
3507.935521	478439.742575	46.266637
3508.042511	478312.038960	46.271642
3508.083690	478190.876844	46.276647
3507.763023	478076.256275	46.281652
3508.133029	477949.214017	46.286657
3507.997190	477828.839164	46.291661
3507.766903	477704.125422	46.296666
3507.805439	477576.833384	46.301671
3507.758241	477460.440799	46.306676
3507.989701	477343.240420	46.311681
3507.667007	477218.944192	46.316685
3507.526842	477101.856350	46.321690
3507.522604	476985.757198	46.326695
3507.594387	476885.897449	46.331700
3507.900304	476759.516087	46.336705
3507.755965	476640.907016	46.341709
3507.783464	476532.951555	46.346714
3508.174208	476409.793857	46.351719
3507.631912	476292.617603	46.356724
3507.707049	476170.676781	46.361729
3507.430011	476060.897056	46.366733
3507.535034	475937.481168	46.371738
3507.736949	475821.238176	46.376743
3507.769443	475714.542944	46.381748
3507.975336	475595.867322	46.386753
3507.792869	475482.067728	46.391757
3507.747624	475372.851959	46.396762
3507.827974	475247.916555	46.401767
3507.546017	475133.169686	46.406772
3507.502177	475018.229531	46.411777
3507.864017	474904.535986	46.416781
3507.910810	474785.983598	46.421786
3508.021073	474672.280943	46.426791
3507.451672	474553.680363	46.431796
3507.694163	474436.763415	46.436801
3507.685185	474332.751172	46.441805
3507.681389	474220.888251	46.446810
3507.798660	474103.433541	46.451815
3507.247839	473995.258129	46.456820
3507.192063	473878.135383	46.461825
3507.305358	473773.896564	46.466829
3507.433080	473661.855893	46.471834
3507.692164	473550.855596	46.476839
3507.203401	473455.883975	46.481844
3507.466421	473344.476638	46.486849
3507.542270	473232.898023	46.491853
3507.456264	473131.829488	46.496858
3507.669838	473012.629580	46.501863
3507.560023	472909.386239	46.506868
3507.665833	472802.104639	46.511873
3507.579038	472692.424387	46.516877
3507.197242	472579.552610	46.521882
3507.144382	472472.397497	46.526887
3507.300132	472374.119689	46.531892
3507.380340	472261.167103	46.536897
3507.428695	472162.805231	46.541901
3507.415936	472052.754064	46.546906
3507.548239	471938.676426	46.551911
3507.138679	471843.683074	46.556916
3507.060347	471742.757655	46.561921
3507.243230	471642.597445	46.566925
3507.501822	471546.070381	46.571930
3507.668345	471422.968537	46.576935
3507.408741	471324.705501	46.581940
3507.408763	471219.154927	46.586945
3507.468749	471111.668879	46.591949
3507.259808	471005.950194	46.596954
3507.568163	470895.482873	46.601959
3507.319938	470795.999554	46.606964
3507.235057	470690.612461	46.611969
3507.415920	470586.648251	46.616973
3507.211075	470489.435152	46.621978
3507.568312	470383.363049	46.626983
3507.203485	470279.439672	46.631988
3507.356069	470170.919435	46.636993
3507.734928	470070.008287	46.641997
3507.188033	469972.243113	46.647002
3507.471020	469860.001262	46.652007
3507.404843	469756.024013	46.657012
3507.332671	469652.958960	46.662017
3507.326472	469555.200613	46.667021
3507.413316	469445.269166	46.672026
3507.483087	469341.266428	46.677031
3507.012093	469242.268847	46.682036
3507.437455	469129.086595	46.687041
3507.377705	469035.640289	46.692045
3507.341942	468938.542317	46.697050
3507.647386	468827.252954	46.702055
3507.119749	468726.793373	46.707060
3507.332445	468621.343954	46.712065
3507.437814	468522.902729	46.717069
3507.114181	468418.354250	46.722074
3507.342503	468308.189450	46.727079
3507.168639	468221.901127	46.732084
3507.329809	468120.966143	46.737089
3507.163142	468015.274210	46.742093
3506.608402	467912.079493	46.747098
3507.110778	467814.276021	46.752103
3506.895792	467716.087962	46.757108
3506.935594	467621.857863	46.762113
3506.850221	467532.258557	46.767117
3506.638943	467439.894123	46.772122
3506.639291	467345.618742	46.777127
3507.055229	467264.037948	46.782132
3506.935916	467163.095143	46.787137
3506.658561	467070.486916	46.792141
3506.625671	466978.191115	46.797146
3507.101289	466884.642869	46.802151
3506.572283	466805.551824	46.807156
3506.624145	466713.645560	46.812161
3506.614959	466621.394658	46.817165
3506.424399	466536.216118	46.822170
3506.654818	466439.870577	46.827175
3506.471410	466369.027117	46.832180
3506.651698	466277.046178	46.837185
3506.758484	466178.744647	46.842189
3506.644163	466093.449807	46.847194
3506.371334	466006.408482	46.852199
3506.625127	465923.684464	46.857204
3506.507836	465831.448236	46.862209
3506.506747	465750.793500	46.867213
3506.588271	465676.710504	46.872218
3506.874294	465584.708210	46.877223
3506.325164	465505.057962	46.882228
3506.384759	465424.644819	46.887233
3506.236239	465337.883235	46.892237
3506.189653	465264.377836	46.897242
3506.573666	465184.414941	46.902247
3506.234297	465104.372575	46.907252
3506.489985	465021.391052	46.912257
3506.132697	464929.596818	46.917261
3506.239139	464865.487446	46.922266
3506.671404	464778.776184	46.927271
3506.613825	464703.294587	46.932276
3506.485276	464609.483826	46.937281
3506.589091	464529.414079	46.942285
3506.195943	464449.783520	46.947290
3506.395449	464369.544776	46.952295
3506.209381	464294.235528	46.957300
3506.202204	464206.786084	46.962305
3506.205892	464134.585157	46.967309
3505.946256	464070.383668	46.972314
3506.126576	463983.255874	46.977319
3506.319153	463918.419328	46.982324
3506.270118	463833.914073	46.987329
3506.440013	463760.619357	46.992333
3505.885286	463690.437515	46.997338
3506.280641	463609.959529	47.002343
3506.207342	463538.681570	47.007348
3506.421125	463448.252219	47.012353
3506.320599	463378.346380	47.017357
3506.212053	463305.553520	47.022362
3506.281474	463223.001489	47.027367
3506.080701	463144.802158	47.032372
3506.112411	463079.179580	47.037377
3506.195919	462997.840267	47.042381
3506.179290	462926.347719	47.047386
3506.309257	462848.496090	47.052391
3506.085843	462784.334856	47.057396
3506.231607	462707.392037	47.062401
3506.421935	462631.252042	47.067405
3506.057219	462563.465908	47.072410
3506.276528	462480.682471	47.077415
3506.393299	462413.016288	47.082420
3506.339138	462332.356450	47.087425
3506.433897	462258.815582	47.092429
3506.324153	462187.184223	47.097434
3506.297607	462097.701772	47.102439
3505.860504	462030.736913	47.107444
3505.854785	461952.195485	47.112449
3506.089751	461881.973660	47.117453
3505.672606	461810.596108	47.122458
3505.695471	461738.433741	47.127463
3505.765879	461688.711279	47.132468
3505.675964	461618.746683	47.137473
3506.020849	461550.987911	47.142477
3505.884132	461490.152106	47.147482
3506.210374	461416.315196	47.152487
3506.007291	461356.655813	47.157492
3506.080625	461286.155421	47.162497
3506.126371	461212.669690	47.167501
3505.565564	461145.824292	47.172506
3505.825688	461070.173089	47.177511
3506.049130	461017.737036	47.182516
3505.733425	460938.788426	47.187521
3505.764084	460885.219409	47.192525
3505.660822	460819.460313	47.197530
3506.402666	460750.110750	47.202535
3505.886976	460682.901351	47.207540
3505.788959	460620.637335	47.212545
3505.864693	460554.998826	47.217549
3506.080449	460483.153671	47.222554
3505.843045	460406.520681	47.227559
3505.743177	460352.617774	47.232564
3505.980550	460289.535300	47.237569
3505.809618	460223.988490	47.242573
3505.828593	460160.334771	47.247578
3505.516629	460084.220038	47.252583
3505.367738	460038.889131	47.257588
3505.663155	459982.333170	47.262593
3505.847375	459917.079448	47.267597
3505.333598	459866.590634	47.272602
3505.732553	459794.052891	47.277607
3505.740688	459740.940733	47.282612
3505.748188	459685.193264	47.287617
3505.851990	459613.313401	47.292621
3505.679652	459563.627053	47.297626
3506.042573	459484.556777	47.302631
3505.599163	459435.980653	47.307636
3505.776728	459364.137976	47.312641
3505.938194	459301.977558	47.317645
3505.753712	459238.000872	47.322650
3505.849861	459169.871005	47.327655
3505.688866	459112.478272	47.332660
3506.061320	459048.709962	47.337665
3505.768974	458993.214476	47.342669
3505.849966	458922.552343	47.347674
3505.794946	458856.271711	47.352679
3505.561664	458806.087076	47.357684
3505.646137	458739.630196	47.362689
3505.924623	458686.823835	47.367693
3505.565334	458635.342580	47.372698
3505.697718	458577.036636	47.377703
3505.832124	458515.993380	47.382708
3505.741757	458451.947425	47.387713
3505.817216	458385.744318	47.392717
3505.613704	458327.393637	47.397722
3505.841715	458264.762495	47.402727
3505.501154	458202.887109	47.407732
3505.330234	458155.629760	47.412737
3505.578046	458086.862121	47.417741
3505.294697	458035.062260	47.422746
3505.565115	457969.635411	47.427751
3505.714758	457925.059653	47.432756
3505.459535	457871.835447	47.437761
3505.759576	457810.559031	47.442765
3505.491275	457763.418752	47.447770
3505.720432	457697.744647	47.452775
3505.567105	457647.695507	47.457780
3505.545314	457588.602077	47.462785
3505.764882	457525.361867	47.467789
3505.525481	457471.373639	47.472794
3505.565130	457410.393886	47.477799
3505.601146	457358.841855	47.482804
3505.605582	457296.296555	47.487809
3505.669108	457240.329973	47.492813
3505.238025	457194.331216	47.497818
3505.311708	457125.590023	47.502823
3505.532489	457091.238620	47.507828
3505.258365	457031.020885	47.512833
3505.603706	456978.908214	47.517837
3505.025895	456927.054406	47.522842
3505.487419	456875.428483	47.527847
3505.382884	456836.773239	47.532852
3505.535329	456776.836708	47.537857
3505.355838	456721.974584	47.542861
3505.258730	456672.065478	47.547866
3505.541712	456619.962528	47.552871
3505.221884	456561.981389	47.557876
3504.896465	456519.663151	47.562881
3505.510727	456464.462049	47.567885
3505.164314	456428.128219	47.572890
3505.610448	456361.246922	47.577895
3505.499134	456314.228506	47.582900
3505.489056	456257.004594	47.587905
3505.822915	456201.039660	47.592909
3505.321489	456155.709480	47.597914
3505.470284	456099.015554	47.602919
3505.448047	456046.811184	47.607924
3505.257606	455994.483337	47.612929
3505.353789	455937.088314	47.617933
3505.316146	455901.359757	47.622938
3505.384955	455841.637490	47.627943
3505.253824	455801.109347	47.632948
3505.327233	455753.703272	47.637953
3505.416119	455708.017852	47.642957
3504.890629	455659.598673	47.647962
3505.265824	455611.937983	47.652967
3505.201446	455562.780885	47.657972
3505.094437	455511.856834	47.662977
3505.291533	455464.682410	47.667981
3505.237901	455427.029564	47.672986
3505.577950	455377.701584	47.677991
3506.019598	455331.346811	47.682996
3506.034252	455270.973153	47.688001
3505.990677	455211.217535	47.693005
3505.397876	455163.771771	47.698010
3505.500802	455099.428725	47.703015
3505.652473	455039.030983	47.708020
3505.364218	454994.016638	47.713025
3505.672667	454934.707002	47.718029
3505.482663	454888.256315	47.723034
3505.628515	454826.540985	47.728039
3505.568242	454779.662374	47.733044
3505.426411	454732.138600	47.738049
3505.879489	454664.540867	47.743053
3505.630852	454613.435989	47.748058
3505.650484	454559.902683	47.753063
3505.747757	454497.586357	47.758068
3505.829917	454456.208053	47.763073
3505.803208	454396.396476	47.768077
3505.445657	454341.963861	47.773082
3505.470843	454296.032693	47.778087
3505.597798	454245.623141	47.783092
3505.549389	454186.980574	47.788097
3505.922925	454136.275188	47.793101
3505.315147	454094.202881	47.798106
3505.613887	454015.933245	47.803111
3505.374966	453976.585810	47.808116
3505.625180	453925.748882	47.813121
3505.472712	453871.786926	47.818125
3505.200043	453824.080610	47.823130
3505.385932	453768.387733	47.828135
3505.201321	453732.072151	47.833140
3505.219888	453670.020213	47.838145
3505.464878	453627.750642	47.843149
3505.118296	453580.563316	47.848154
3505.162817	453532.143141	47.853159
3505.475809	453489.810981	47.858164
3505.340507	453444.817801	47.863169
3505.243096	453390.794485	47.868173
3505.469178	453342.849804	47.873178
3505.685830	453285.984398	47.878183
3505.524533	453244.746608	47.883188
3505.666385	453193.013868	47.888193
3504.969846	453141.272069	47.893197
3505.331449	453106.028094	47.898202
3505.067509	453055.885146	47.903207
3505.345343	453007.981544	47.908212
3505.341284	452965.499662	47.913217
3505.309221	452914.454956	47.918221
3505.102416	452875.809662	47.923226
3505.260920	452813.883332	47.928231
3505.243096	452778.855673	47.933236
3505.172616	452732.734561	47.938241
3505.285514	452691.854411	47.943245
3504.810090	452647.018954	47.948250
3504.997288	452595.226274	47.953255
3505.102278	452555.868090	47.958260
3505.030246	452517.655378	47.963265
3504.746836	452477.400133	47.968269
3504.966041	452433.662318	47.973274
3504.824782	452398.350910	47.978279
3505.363056	452359.222548	47.983284
3505.344850	452314.967356	47.988289
3505.198284	452256.640225	47.993293
3504.802229	452231.460739	47.998298
3505.293743	452180.476908	48.003303
3504.873702	452142.931291	48.008308
3505.361488	452100.211554	48.013313
3505.024691	452052.258592	48.018317
3504.606681	452020.137038	48.023322
3505.169726	451967.011169	48.028327
3505.268012	451936.829235	48.033332
3504.821197	451896.702156	48.038337
3504.877962	451843.459626	48.043341
3504.687093	451826.761875	48.048346
3505.284824	451780.575238	48.053351
3505.151499	451751.547942	48.058356
3505.167193	451696.791102	48.063361
3504.945215	451655.966085	48.068365
3504.778759	451617.970628	48.073370
3504.934962	451580.122801	48.078375
3504.987631	451548.122939	48.083380
3504.857281	451502.820486	48.088385
3504.677300	451467.666198	48.093389
3505.069548	451428.155423	48.098394
3505.122412	451390.629091	48.103399
3505.196203	451353.758206	48.108404
3504.938385	451311.012060	48.113409
3505.540217	451277.244934	48.118413
3505.022715	451233.731780	48.123418
3505.154796	451181.437982	48.128423
3505.150103	451136.975169	48.133428
3504.618530	451096.151215	48.138433
3505.082934	451040.149929	48.143437
3505.227639	451017.107428	48.148442
3504.845363	450970.072328	48.153447
3505.107562	450944.221176	48.158452
3504.936045	450909.317999	48.163457
3505.241268	450858.159932	48.168461
3505.355358	450827.568085	48.173466
3505.398416	450777.113690	48.178471
3505.536918	450734.704292	48.183476
3505.200342	450692.629432	48.188481
3505.344554	450637.645054	48.193485
3505.200436	450600.455137	48.198490
3505.130785	450552.098185	48.203495
3504.992867	450522.512243	48.208500
3504.914561	450466.348579	48.213505
3505.341131	450433.674744	48.218509
3504.854985	450390.053066	48.223514
3505.058777	450348.747169	48.228519
3505.349570	450311.279669	48.233524
3504.889367	450270.847522	48.238529
3505.038617	450229.804212	48.243533
3505.280061	450202.383926	48.248538
3504.895999	450160.671014	48.253543
3504.850387	450120.674805	48.258548
3505.118201	450084.681186	48.263553
3504.975299	450043.687396	48.268557
3504.753951	450003.873079	48.273562
3504.919075	449974.082507	48.278567
3504.737977	449927.872647	48.283572
3504.771127	449893.084930	48.288577
3504.795562	449864.636497	48.293581
3504.854021	449833.342854	48.298586
3504.981859	449792.707967	48.303591
3504.995253	449764.971126	48.308596
3504.775113	449722.671616	48.313601
3505.050784	449688.501289	48.318605
3504.741565	449643.225336	48.323610
3504.954426	449613.020474	48.328615
3504.737333	449581.469284	48.333620
3504.774630	449541.052183	48.338625
3504.922197	449507.461175	48.343629
3504.823866	449471.833246	48.348634
3504.908572	449430.190945	48.353639
3504.915161	449399.361846	48.358644
3504.595686	449366.357400	48.363649
3505.011776	449325.368163	48.368653
3505.026112	449313.855882	48.373658
3504.879060	449257.903529	48.378663
3504.799104	449225.162189	48.383668
3505.009014	449191.255804	48.388673
3505.092067	449142.311771	48.393677
3504.946034	449115.868909	48.398682
3504.798283	449072.744453	48.403687
3505.032223	449058.000135	48.408692
3504.754995	449014.593439	48.413697
3505.215232	448968.170545	48.418701
3504.910657	448939.067167	48.423706
3504.841137	448897.703670	48.428711
3504.923465	448863.260785	48.433716
3504.479125	448833.775484	48.438721
3504.752624	448786.877023	48.443725
3505.013548	448766.550295	48.448730
3504.942810	448732.589682	48.453735
3504.937690	448703.485550	48.458740
3504.783555	448674.609646	48.463745
3504.894793	448628.397714	48.468749
3504.748731	448598.404798	48.473754
3505.027910	448563.167221	48.478759
3505.021423	448526.000827	48.483764
3504.743502	448491.162492	48.488769
3504.894215	448443.979998	48.493773
3504.987560	448416.379845	48.498778
3504.751089	448377.579150	48.503783
3504.710410	448343.511364	48.508788
3504.601884	448324.312131	48.513793
3504.801112	448298.417766	48.518797
3504.585087	448257.078028	48.523802
3504.938728	448220.813031	48.528807
3504.844088	448199.532335	48.533812
3504.907650	448157.891129	48.538817
3505.217515	448126.501312	48.543821
3505.011897	448097.177044	48.548826
3505.064980	448056.703690	48.553831
3505.243492	448019.048450	48.558836
3505.157978	447980.018419	48.563841
3505.378074	447941.138963	48.568845
3505.142748	447896.353706	48.573850
3505.386880	447857.013623	48.578855
3505.458091	447815.877514	48.583860
3505.266688	447766.977154	48.588865
3505.486435	447728.300198	48.593869
3505.066443	447690.036656	48.598874
3505.288365	447651.004231	48.603879
3505.391561	447600.633355	48.608884
3505.092501	447565.137893	48.613889
3505.529422	447511.870153	48.618893
3505.242456	447474.394843	48.623898
3504.653150	447433.776444	48.628903
3504.637823	447404.773684	48.633908
3504.435830	447371.593926	48.638913
3504.750626	447336.652479	48.643917
3504.628392	447323.184784	48.648922
3504.792412	447292.122888	48.653927
3504.863554	447251.746331	48.658932
3504.373424	447228.554533	48.663937
3504.624332	447200.520218	48.668941
3504.709926	447163.741381	48.673946
3504.816087	447132.739841	48.678951
3504.464020	447114.798121	48.683956
3504.504436	447090.247844	48.688961
3504.591873	447035.314461	48.693965
3504.879809	447016.553441	48.698970
3504.828368	446993.235769	48.703975
3504.654733	446952.393341	48.708980
3504.363099	446928.203834	48.713985
3504.752629	446899.993323	48.718989
3504.615071	446875.422477	48.723994
3504.508648	446836.038939	48.728999
3504.690147	446816.738107	48.734004
3504.685480	446793.158678	48.739009
3504.693243	446760.550670	48.744013
3504.102311	446735.803525	48.749018
3504.649335	446701.379196	48.754023
3504.829567	446686.287427	48.759028
3504.468624	446646.490604	48.764033
3504.543290	446608.292778	48.769037
3504.413620	446594.978022	48.774042
3504.568207	446568.074956	48.779047
3504.919690	446528.866216	48.784052
3504.148109	446501.614102	48.789057
3504.384241	446480.275200	48.794061
3504.802357	446475.436984	48.799066
3504.822135	446428.221653	48.804071
3505.034167	446397.961632	48.809076
3504.924097	446369.987862	48.814081
3504.979335	446324.287582	48.819085
3505.084710	446306.571338	48.824090
3505.152918	446265.737009	48.829095
3505.232550	446226.878402	48.834100
3504.594259	446191.185010	48.839105
3504.737911	446154.698788	48.844109
3504.157059	446141.156518	48.849114
3504.074538	446116.879669	48.854119
3504.391215	446077.777468	48.859124
3504.272749	446046.508432	48.864129
3504.736663	446019.349009	48.869133
3504.501195	446010.413189	48.874138
3504.276968	445991.637297	48.879143
3504.499785	445962.034075	48.884148
3504.415959	445921.427897	48.889153
3504.327431	445905.925057	48.894157
3504.288068	445895.687896	48.899162
3504.379079	445873.257496	48.904167
3504.595773	445846.393629	48.909172
3504.489387	445815.781455	48.914177
3504.250182	445789.299636	48.919181
3504.217790	445773.077139	48.924186
3504.306778	445759.268111	48.929191
3504.422030	445744.237485	48.934196
3504.299476	445713.932202	48.939201
3504.613480	445678.227483	48.944205
3504.385973	445673.245765	48.949210
3504.298309	445660.683947	48.954215
3504.392051	445642.614148	48.959220
3504.229040	445604.962240	48.964225
3504.147660	445572.418353	48.969229
3504.366867	445556.457009	48.974234
3504.295562	445532.836853	48.979239
3504.477292	445519.721820	48.984244
3504.220646	445507.898751	48.989249
3504.200174	445464.136664	48.994253
3504.157418	445443.351483	48.999258
3504.326153	445424.102286	49.004263
3504.147934	445408.512974	49.009268
3503.979280	445398.044084	49.014273
3504.288062	445379.075215	49.019277
3504.287157	445362.542748	49.024282
3504.277682	445347.228860	49.029287
3504.330022	445324.550921	49.034292
3504.222915	445292.416710	49.039297
3504.227753	445269.797538	49.044301
3504.370095	445254.254805	49.049306
3504.206902	445240.742073	49.054311
3504.465314	445221.274527	49.059316
3504.422120	445207.690571	49.064321
3504.756847	445164.120791	49.069325
3504.505669	445150.876596	49.074330
3504.712864	445140.039118	49.079335
3504.555597	445093.358214	49.084340
3504.565811	445071.092914	49.089345
3504.570836	445044.923472	49.094349
3504.467425	445037.587555	49.099354
3504.584584	445007.899628	49.104359
3504.099233	444980.089549	49.109364
3504.184433	444955.022026	49.114369
3504.222835	444937.772517	49.119373
3504.370750	444928.821495	49.124378
3504.195897	444907.804778	49.129383
3504.361801	444884.346263	49.134388
3504.649054	444850.926900	49.139393
3504.425140	444826.774161	49.144397
3504.449968	444809.171863	49.149402
3504.543796	444799.469299	49.154407
3504.560058	444764.118191	49.159412
3504.149139	444734.672203	49.164417
3504.430013	444714.186061	49.169421
3504.471634	444706.115254	49.174426
3504.516750	444681.307833	49.179431
3504.492944	444652.404215	49.184436
3504.401079	444631.170195	49.189441
3504.391551	444604.495549	49.194445
3504.484033	444589.315857	49.199450
3504.166295	444565.128130	49.204455
3504.453566	444534.294762	49.209460
3504.334050	444510.174558	49.214465
3504.258175	444493.806371	49.219469
3504.262193	444484.524726	49.224474
3504.413110	444467.103481	49.229479
3504.146730	444456.955112	49.234484
3503.757823	444423.904121	49.239489
3504.386509	444397.475253	49.244493
3504.028990	444378.974287	49.249498
3504.137702	444364.045245	49.254503
3504.381014	444343.920177	49.259508
3504.227226	444334.462549	49.264513
3504.499445	444327.417262	49.269517
3504.075218	444321.403782	49.274522
3504.455562	444288.474812	49.279527
3504.454572	444260.631811	49.284532
3504.391059	444244.819203	49.289537
3504.491405	444230.145078	49.294541
3504.504477	444213.355760	49.299546
3504.522804	444179.778412	49.304551
3504.652308	444159.824755	49.309556
3504.473892	444135.054874	49.314561
3504.634953	444116.972299	49.319565
3504.611470	444077.772394	49.324570
3504.341853	444052.916558	49.329575
3504.297197	444036.644127	49.334580
3504.316914	444030.706910	49.339585
3504.527371	444009.369939	49.344589
3504.152266	443974.692964	49.349594
3504.469793	443947.048756	49.354599
3504.354880	443930.991109	49.359604
3504.305809	443926.637836	49.364609
3504.336894	443900.208969	49.369613
3504.364833	443896.197559	49.374618
3504.104426	443865.558189	49.379623
3504.288046	443844.022769	49.384628
3504.213050	443836.783025	49.389633
3504.189970	443814.623546	49.394637
3504.310052	443811.560015	49.399642
3504.077123	443794.203769	49.404647
3504.386077	443786.086971	49.409652
3504.356077	443754.799493	49.414657
3504.357445	443720.767871	49.419661
3504.365184	443711.079518	49.424666
3504.007539	443688.520580	49.429671
3504.102778	443676.027806	49.434676
3504.093025	443666.038115	49.439681
3504.155169	443656.289731	49.444685
3504.013070	443643.178134	49.449690
3504.186988	443629.150369	49.454695
3504.218742	443589.940147	49.459700
3504.093736	443574.137548	49.464705
3504.223500	443549.212937	49.469709
3503.909810	443552.563170	49.474714
3504.399008	443532.851823	49.479719
3504.022641	443522.316051	49.484724
3503.695243	443516.691553	49.489729
3503.963386	443499.148076	49.494733
3503.834289	443493.794020	49.499738
3503.862470	443488.108799	49.504743
3504.246330	443476.327398	49.509748
3504.090021	443466.768383	49.514753
3504.236585	443450.057115	49.519757
3504.061069	443438.219053	49.524762
3503.911465	443401.828955	49.529767
3504.147366	443374.299391	49.534772
3503.493677	443372.737314	49.539777
3504.135706	443358.122260	49.544781
3504.367330	443350.474969	49.549786
3504.486120	443334.985594	49.554791
3504.365285	443321.362988	49.559796
3504.378355	443314.057313	49.564801
3504.593413	443294.899745	49.569805
3504.069440	443267.753387	49.574810
3504.113270	443241.625851	49.579815
3504.508391	443222.589630	49.584820
3504.276293	443214.108536	49.589825
3504.620144	443204.108972	49.594829
3504.206190	443195.608205	49.599834
3504.340860	443157.038971	49.604839
3504.670046	443133.956426	49.609844
3504.306766	443113.071572	49.614849
3504.624491	443100.489757	49.619853
3504.533074	443079.558450	49.624858
3503.922451	443046.086737	49.629863
3504.058003	443030.695722	49.634868
3503.906966	443022.302150	49.639873
3503.985085	443011.232051	49.644877
3503.849515	442997.053847	49.649882
3504.109839	442991.683891	49.654887
3504.259204	442975.631129	49.659892
3504.334827	442968.669691	49.664897
3504.105768	442953.949510	49.669901
3504.000294	442941.896340	49.674906
3503.995028	442930.992596	49.679911
3504.267713	442920.294983	49.684916
3503.833378	442894.299396	49.689921
3504.009434	442865.917176	49.694925
3504.234547	442858.980897	49.699930
3504.083439	442833.697668	49.704935
3504.022029	442827.773975	49.709940
3503.872595	442823.488336	49.714945
3504.223625	442805.879427	49.719949
3504.207009	442800.404554	49.724954
3504.049599	442797.743300	49.729959
3504.282647	442781.726825	49.734964
3503.985694	442775.082542	49.739969
3503.924433	442754.551529	49.744973
3504.004929	442757.530257	49.749978
3503.968057	442744.501588	49.754983
3504.192824	442725.341861	49.759988
3503.975235	442707.627086	49.764993
3504.517044	442679.131450	49.769997
3504.169654	442666.206475	49.775002
3503.771341	442648.066031	49.780007
3504.020582	442641.835643	49.785012
3503.574627	442634.100918	49.790017
3504.289746	442619.878651	49.795021
3503.742705	442610.690297	49.800026
3504.085476	442600.690642	49.805031
3504.152587	442590.281570	49.810036
3503.798093	442589.429147	49.815041
3504.026714	442575.543521	49.820045
3503.876071	442567.859788	49.825050
3504.081323	442559.963122	49.830055
3504.302314	442548.158310	49.835060
3503.973299	442546.946493	49.840065
3504.276611	442532.338004	49.845069
3504.092201	442499.654915	49.850074
3503.751106	442471.309765	49.855079
3504.211907	442457.029376	49.860084
3504.094317	442445.028719	49.865089
3504.157979	442433.960796	49.870093
3504.267775	442427.196232	49.875098
3504.093271	442421.342459	49.880103
3504.314553	442414.000929	49.885108
3503.925522	442406.966490	49.890113
3504.040733	442393.302996	49.895117
3504.294074	442384.130041	49.900122
3504.318955	442363.178185	49.905127
3504.494067	442334.592552	49.910132
3504.449732	442320.449048	49.915137
3504.550190	442300.701525	49.920141
3504.030759	442298.710675	49.925146
3503.825015	442284.949755	49.930151
3504.345080	442280.245365	49.935156
3504.204861	442245.982004	49.940161
3504.265785	442220.103927	49.945165
3503.784910	442209.382475	49.950170
3503.858241	442199.682249	49.955175
3503.923823	442186.686473	49.960180
3503.743000	442186.159426	49.965185
3504.082672	442172.356024	49.970189
3503.840527	442156.217346	49.975194
3503.836641	442153.681962	49.980199
3503.964103	442139.762612	49.985204
3503.766737	442138.477571	49.990209
3503.892029	442120.653049	49.995213
3503.865187	442121.519901	50.000218
3503.781092	442106.165738	50.005223
3504.067318	442098.813013	50.010228
3503.726682	442098.211809	50.015233
3503.788101	442078.775079	50.020237
3503.608670	442078.755005	50.025242
3503.768045	442062.243369	50.030247
3503.962475	442054.399090	50.035252
3503.733422	442050.786271	50.040257
3503.943461	442053.286484	50.045261
3504.071485	442039.823466	50.050266
3503.491191	442023.488823	50.055271
3504.043680	442037.647211	50.060276
3503.941971	442031.983789	50.065281
3503.780671	442015.932645	50.070285
3503.828643	442026.677408	50.075290
3503.913104	442026.916601	50.080295
3503.659238	442020.366172	50.085300
3503.830198	442015.721337	50.090305
3503.849068	442004.204351	50.095309
3503.834133	442003.699695	50.100314
3503.591666	441994.915566	50.105319
3503.959215	441984.962120	50.110324
3503.781305	441971.196248	50.115329
3503.923892	441968.027173	50.120333
3503.924132	441963.817250	50.125338
3503.963157	441957.064625	50.130343
3504.108876	441942.939146	50.135348
3503.946222	441943.321979	50.140353
3503.882674	441922.334078	50.145357
3503.764794	441923.520813	50.150362
3503.688047	441915.012685	50.155367
3503.990939	441904.309417	50.160372
3503.817876	441908.041661	50.165377
3503.518376	441885.318754	50.170381
3503.843175	441889.473208	50.175386
3503.733182	441884.267657	50.180391
3503.712076	441868.598241	50.185396
3503.882463	441874.300718	50.190401
3504.064821	441849.770955	50.195405
3503.953582	441853.644817	50.200410
3503.899795	441846.958727	50.205415
3503.749034	441828.014501	50.210420
3503.801154	441830.186651	50.215425
3503.536314	441824.246698	50.220429
3503.895233	441817.236520	50.225434
3504.035078	441802.858344	50.230439
3503.893190	441796.948111	50.235444
3503.823001	441790.924191	50.240449
3503.916100	441772.191886	50.245453
3504.026922	441771.716473	50.250458
3503.921635	441767.879586	50.255463
3504.181705	441757.335725	50.260468
3503.615564	441753.881860	50.265473
3503.962140	441748.902649	50.270477
3503.928065	441743.075437	50.275482
3503.702044	441737.483887	50.280487
3504.084426	441728.592956	50.285492
3504.139569	441727.163330	50.290497
3504.082208	441712.818768	50.295501
3503.667881	441700.310425	50.300506
3503.571772	441696.624125	50.305511
3503.729421	441688.938162	50.310516
3503.763863	441691.417678	50.315521
3504.035417	441678.183541	50.320525
3503.900611	441667.098396	50.325530
3503.736257	441656.982013	50.330535
3503.904047	441655.178091	50.335540
3503.945234	441650.707505	50.340545
3503.603601	441635.599876	50.345549
3503.828022	441621.866530	50.350554
3503.669367	441619.458955	50.355559
3503.955499	441616.823265	50.360564
3503.757148	441613.763077	50.365569
3503.786296	441604.323743	50.370573
3503.674573	441590.952109	50.375578
3503.599452	441585.537643	50.380583
3503.682905	441587.958079	50.385588
3503.499546	441607.618974	50.390593
3503.922844	441600.800623	50.395597
3503.883521	441598.677005	50.400602
3503.422724	441600.683147	50.405607
3503.777588	441585.760889	50.410612
3503.663254	441591.055555	50.415617
3503.847040	441578.089956	50.420621
3503.924876	441573.004427	50.425626
3503.610367	441569.101785	50.430631
3504.063618	441557.104612	50.435636
3503.493464	441553.194896	50.440641
3503.499856	441538.027773	50.445645
3503.560022	441537.814618	50.450650
3503.404477	441540.174423	50.455655
3503.898932	441558.908063	50.460660
3503.739373	441560.812049	50.465665
3503.808485	441557.503293	50.470669
3503.900900	441560.074370	50.475674
3503.396207	441549.813161	50.480679
3503.771014	441541.937900	50.485684
3503.392382	441533.531893	50.490689
3503.852337	441518.895980	50.495693
3504.450802	441515.040327	50.500698
3504.094095	441512.311500	50.505703
3504.154901	441507.533199	50.510708
3503.849192	441502.716035	50.515713
3503.965081	441492.602447	50.520717
3503.584079	441492.363176	50.525722
3503.839692	441486.283540	50.530727
3503.982335	441455.571950	50.535732
3503.495521	441438.815123	50.540737
3503.942233	441394.559260	50.545741
3503.917560	441343.434747	50.550746
3503.709429	441282.298259	50.555751
3503.912769	441210.287276	50.560756
3503.580870	441135.324041	50.565761
3503.914777	441040.363176	50.570765
3503.984963	440938.345580	50.575770
3503.958299	440808.192109	50.580775
3503.968612	440672.350403	50.585780
3503.846706	440532.218821	50.590785
3503.771025	440382.846464	50.595789
3504.236518	440217.300676	50.600794
3503.863655	440035.410845	50.605799
3503.905551	439839.296011	50.610804
3503.640885	439643.181055	50.615809
3504.085675	439426.956625	50.620813
3503.849491	439199.128212	50.625818
3503.973795	438959.872724	50.630823
3504.009390	438708.911396	50.635828
3503.247467	438450.017402	50.640833
3503.256575	438179.371511	50.645837
3503.277152	437894.617188	50.650842
3502.970374	437607.378554	50.655847
3503.318763	437304.804690	50.660852
3503.342336	436994.266401	50.665857
3503.144255	436664.584336	50.670861
3503.112266	436325.787611	50.675866
3503.092104	435960.246295	50.680871
3503.476028	435588.795412	50.685876
3502.993909	435213.883990	50.690881
3503.101279	434815.932218	50.695885
3503.187677	434406.611583	50.700890
3502.958230	433979.984555	50.705895
3503.087445	433536.188708	50.710900
3503.093829	433093.166361	50.715905
3502.975822	432623.212344	50.720909
3503.127735	432141.430092	50.725914
3503.142744	431646.771975	50.730919
3503.128815	431118.818872	50.735924
3502.809353	430593.900021	50.740929
3503.149642	430038.509183	50.745933
3503.019360	429478.313544	50.750938
3502.480097	428908.582455	50.755943
3502.773622	428312.913315	50.760948
3502.893472	427709.747306	50.765953
3502.907031	427074.456363	50.770957
3502.900432	426431.792258	50.775962
3502.349426	425772.656873	50.780967
3502.903208	425086.310959	50.785972
3502.589049	424401.718017	50.790977
3502.567546	423681.623921	50.795981
3502.566302	422948.814150	50.800986
3502.456975	422206.863116	50.805991
3502.408074	421435.790059	50.810996
3502.138551	420648.281627	50.816001
3501.938787	419841.697518	50.821005
3501.776828	419025.231106	50.826010
3501.444068	418195.946946	50.831015
3501.712309	417340.180604	50.836020
3501.894301	416477.494364	50.841025
3501.916056	415585.329310	50.846029
3501.745024	414678.033495	50.851034
3501.551267	413742.093820	50.856039
3501.712103	412779.423513	50.861044
3501.613281	411816.660323	50.866049
3501.461926	410823.677365	50.871053
3501.587282	409804.300645	50.876058
3501.080907	408779.557888	50.881063
3501.267764	407718.644703	50.886068
3501.013529	406661.600036	50.891073
3500.944714	405576.264316	50.896077
3500.562147	404469.857078	50.901082
3500.598825	403347.254918	50.906087
3500.540818	402204.378055	50.911092
3500.300839	401053.534322	50.916097
3500.131132	399870.088917	50.921101
3500.319337	398681.985502	50.926106
3500.155404	397470.519183	50.931111
3500.103131	396219.627063	50.936116
3500.039250	394970.639626	50.941121
3499.929406	393691.293450	50.946125
3499.919724	392384.711072	50.951130
3499.707589	391070.482745	50.956135
3499.582502	389734.835677	50.961140
3499.332692	388389.468799	50.966145
3499.080815	387012.274811	50.971149
3498.917506	385629.006670	50.976154
3498.008053	384230.809041	50.981159
3498.385223	382808.411633	50.986164
3497.720386	381374.588929	50.991169
3497.693990	379928.036343	50.996173
3497.875161	378471.572089	51.001178
3497.252419	376986.428286	51.006183
3497.320453	375485.058716	51.011188
3496.973002	373969.761280	51.016193
3497.001773	372439.662439	51.021197
3497.092382	370887.771445	51.026202
3496.796097	369325.046381	51.031207
3496.734862	367736.580539	51.036212
3496.198803	366132.614188	51.041217
3496.120357	364519.268749	51.046221
3496.235432	362892.443596	51.051226
3495.864428	361234.831846	51.056231
3495.802516	359558.885226	51.061236
3495.515439	357878.709105	51.066241
3495.564737	356172.510291	51.071245
3495.387735	354456.612439	51.076250
3494.799201	352719.548641	51.081255
3494.736567	350966.983323	51.086260
3494.241666	349206.050479	51.091265
3494.116545	347428.268366	51.096269
3493.813769	345640.294236	51.101274
3493.057938	343818.613799	51.106279
3493.413524	341986.952414	51.111284
3492.930139	340150.172966	51.116289
3492.774818	338306.143095	51.121293
3492.745558	336443.649907	51.126298
3492.094083	334563.940492	51.131303
3492.044233	332674.186134	51.136308
3491.624770	330764.500141	51.141313
3491.993624	328856.929310	51.146317
3490.947334	326923.344816	51.151322
3490.605291	324962.416618	51.156327
3490.399440	323007.204293	51.161332
3490.055650	321046.022204	51.166337
3489.657368	319060.910926	51.171341
3489.255358	317061.865993	51.176346
3488.824885	315062.843034	51.181351
3488.691945	313045.280224	51.186356
3488.319597	311029.127643	51.191361
3488.060216	308983.953955	51.196365
3487.905908	306928.575400	51.201370
3487.421985	304871.138646	51.206375
3487.090646	302786.076371	51.211380
3486.622761	300703.407046	51.216385
3486.208839	298601.075328	51.221389
3486.041780	296497.815610	51.226394
3485.720353	294376.587025	51.231399
3485.317476	292243.540703	51.236404
3484.495370	290101.817240	51.241409
3484.341160	287953.040937	51.246413
3483.865162	285796.593443	51.251418
3483.401030	283642.122362	51.256423
3483.443952	281448.876089	51.261428
3482.902627	279268.000541	51.266433
3482.220652	277060.815215	51.271437
3481.970861	274847.266620	51.276442
3481.881755	272631.682092	51.281447
3481.427129	270397.625637	51.286452
3480.649626	268161.187863	51.291457
3480.612138	265906.985600	51.296461
3480.368312	263646.949178	51.301466
3479.697540	261380.202157	51.306471
3479.320041	259098.347171	51.311476
3478.888835	256806.106958	51.316481
3478.536393	254510.185410	51.321485
3477.985855	252194.333169	51.326490
3477.681425	249890.720064	51.331495
3477.427213	247554.813535	51.336500
3476.695743	245220.859507	51.341505
3476.362991	242873.685572	51.346509
3475.949082	240520.813598	51.351514
3475.098651	238172.545396	51.356519
3474.969809	235795.757571	51.361524
3474.121223	233428.110850	51.366529
3473.631681	231044.619848	51.371533
3473.167074	228656.041229	51.376538
3472.425882	226270.477105	51.381543
3471.992883	223867.713522	51.386548
3471.352562	221475.700886	51.391553
3471.000730	219065.634027	51.396557
3470.219698	216648.156413	51.401562
3469.523363	214230.084624	51.406567
3469.047986	211804.498695	51.411572
3468.423594	209385.265902	51.416577
3467.745382	206958.789730	51.421581
3467.507613	204522.392991	51.426586
3466.587501	202084.342371	51.431591
3466.265893	199644.410116	51.436596
3465.127410	197202.918059	51.441601
3464.975476	194741.742516	51.446605
3464.363540	192290.830006	51.451610
3463.588804	189837.468683	51.456615
3462.779763	187375.391724	51.461620
3462.254819	184915.570312	51.466625
3461.476838	182455.821667	51.471629
3461.363319	179980.048333	51.476634
3460.555874	177506.569567	51.481639
3459.876740	175029.738965	51.486644
3459.011239	172555.823383	51.491649
3458.398882	170082.384673	51.496653
3457.982971	167602.261067	51.501658
3457.028257	165127.489912	51.506663
3456.597578	162635.530113	51.511668
3455.773014	160157.593825	51.516673
3454.909731	157667.191847	51.521677
3453.982520	155185.217683	51.526682
3453.219441	152703.393791	51.531687
3452.223561	150232.511738	51.536692
3451.757900	147748.728084	51.541697
3450.556632	145264.942023	51.546701
3450.442983	142717.352472	51.551706
3448.951894	140250.665496	51.556711
3448.462275	137780.485069	51.561716
3447.902671	135307.990112	51.566721
3446.158000	132844.064687	51.571725
3445.391056	130385.151221	51.576730
3444.191115	127932.052348	51.581735
3443.594766	125484.072376	51.586740
3442.721157	123050.779594	51.591745
3441.808302	120617.585849	51.596749
3440.735832	118189.292086	51.601754
3439.683310	115773.263308	51.606759
3438.574325	113362.209279	51.611764
3437.619147	110962.332579	51.616769
3436.574728	108558.663904	51.621773
3435.842746	106169.641394	51.626778
3434.963359	103797.057339	51.631783
3433.743319	101420.375197	51.636788
3432.504274	99055.572550	51.641793
3431.448094	96697.397639	51.646797
3430.029799	94358.530237	51.651802
3429.194790	92031.559639	51.656807
3428.292531	89711.875803	51.661812
3427.096486	87402.633782	51.666817
3425.673138	85110.166499	51.671821
3424.811245	82822.811237	51.676826
3423.564480	80553.702396	51.681831
3422.478916	78292.355650	51.686836
3420.843729	76053.808619	51.691841
3419.709368	73829.628296	51.696845
3418.573657	71614.072101	51.701850
3417.400608	69424.136888	51.706855
3415.726106	67245.088692	51.711860
3414.182047	65076.343547	51.716865
3412.598786	62938.020771	51.721869
3411.033833	60812.163194	51.726874
3409.001417	58739.406241	51.731879
3407.588098	56666.202255	51.736884
3405.773134	54647.540571	51.741889
3403.181103	52648.611567	51.746893
3400.025435	50712.205433	51.751898
3396.099105	48841.425391	51.756903
3391.666629	47029.388714	51.761908
3386.373303	45309.505607	51.766913
3381.379230	43676.799405	51.771917
3376.794396	42126.719055	51.776922
3372.174041	40673.106219	51.781927
3367.661277	39300.405789	51.786932
3363.698174	38011.784884	51.791937
3359.382801	36808.864798	51.796941
3356.053383	35691.755033	51.801946
3352.650677	34663.956349	51.806951
3349.778251	33694.956033	51.811956
3346.339509	32799.951647	51.816961
3343.916332	31968.860595	51.821965
3341.231111	31199.889763	51.826970
3339.132897	30504.123286	51.831975
3337.320213	29855.581492	51.836980
3335.032165	29257.707633	51.841985
3333.252035	28702.129514	51.846989
3330.882684	28175.682043	51.851994
3329.053408	27705.084397	51.856999
3327.679323	27267.911426	51.862004
3326.290634	26877.348098	51.867009
3325.347662	26512.036063	51.872013
3324.047802	26171.190479	51.877018
3322.649225	25854.041561	51.882023
3321.822315	25555.565006	51.887028
3320.388392	25293.959821	51.892033
3319.652970	25038.216560	51.897037
3318.876035	24809.827613	51.902042
3317.727561	24598.766164	51.907047
3317.098346	24399.000356	51.912052
3316.790067	24214.232119	51.917057
3315.899309	24035.703606	51.922061
3315.034671	23867.829714	51.927066
3314.289934	23701.903954	51.932071
3313.855697	23545.581331	51.937076
3312.791934	23408.749408	51.942081
3312.424955	23278.693308	51.947085
3312.223609	23138.357864	51.952090
3311.743560	23022.432993	51.957095
3311.236132	22888.640770	51.962100
3310.354194	22765.933776	51.967105
3309.871924	22650.122466	51.972109
3309.778671	22536.794169	51.977114
3309.172275	22426.757507	51.982119
3308.879366	22307.434659	51.987124
3308.478678	22199.444974	51.992129
3307.529768	22092.140926	51.997133
3307.722108	21976.566740	52.002138
3306.866724	21860.290108	52.007143
3306.847650	21738.929198	52.012148
3306.285656	21622.616708	52.017153
3305.957326	21495.663064	52.022157
3305.535739	21370.435314	52.027162
3304.554891	21251.219945	52.032167
3304.629779	21121.849315	52.037172
3304.080777	21011.626964	52.042177
3303.286055	20895.104648	52.047181
3303.037866	20775.546111	52.052186
3302.570640	20656.870028	52.057191
3302.230446	20524.100018	52.062196
3301.783485	20406.029279	52.067201
3301.047693	20267.411634	52.072205
3300.811619	20132.766211	52.077210
3300.195853	20005.022257	52.082215
3300.061252	19865.005739	52.087220
3299.305251	19728.326127	52.092225
3299.245867	19587.175090	52.097229
3298.834873	19438.427967	52.102234
3297.832947	19292.841889	52.107239
3297.060637	19147.954470	52.112244
3296.754620	19005.487791	52.117249
3296.010081	18854.074410	52.122253
3295.819004	18707.679873	52.127258
3295.008624	18565.380514	52.132263
3294.776887	18408.202474	52.137268
3294.248029	18263.274720	52.142273
3293.736001	18107.849744	52.147277
3292.952363	17961.570803	52.152282
3292.259496	17797.762634	52.157287
3291.668594	17632.726307	52.162292
3291.246488	17476.394003	52.167297
3290.897596	17328.478336	52.172301
3289.864949	17163.322923	52.177306
3289.646903	17005.632455	52.182311
3288.990731	16840.053961	52.187316
3288.633189	16676.558215	52.192321
3287.766342	16521.399758	52.197325
3287.288297	16343.542033	52.202330
3286.560785	16181.075266	52.207335
3286.051190	16015.484622	52.212340
3285.404406	15837.662681	52.217345
3284.389448	15671.847266	52.222349
3284.212419	15499.306342	52.227354
3283.654687	15344.385738	52.232359
3282.859426	15173.082209	52.237364
3282.096899	15008.270164	52.242369
3281.319635	14838.078007	52.247373
3280.659549	14669.030702	52.252378
3280.059302	14498.336101	52.257383
3279.518876	14330.586624	52.262388
3279.131276	14166.373123	52.267393
3278.226742	13997.970179	52.272397
3277.584955	13827.953286	52.277402
3276.871031	13673.989907	52.282407
3276.044815	13509.864165	52.287412
3275.528167	13339.693430	52.292417
3274.935440	13173.614343	52.297421
3274.601868	13003.855084	52.302426
3273.332648	12836.703502	52.307431
3272.663644	12674.374813	52.312436
3271.921793	12523.309122	52.317441
3271.042146	12362.580661	52.322445
3270.472974	12209.419979	52.327450
3269.528667	12045.602344	52.332455
3268.645038	11897.124785	52.337460
3267.664162	11745.367602	52.342465
3267.420340	11602.994606	52.347469
3266.842244	11460.115881	52.352474
3265.551679	11313.007173	52.357479
3264.593491	11174.504576	52.362484
3264.003657	11053.012008	52.367489
3263.308803	10917.849355	52.372493
3262.140491	10782.143038	52.377498
3261.351520	10664.076405	52.382503
3260.714434	10537.253924	52.387508
3260.178924	10410.742121	52.392513
3259.410121	10296.689298	52.397517
3258.551644	10174.084764	52.402522
3257.807306	10057.858644	52.407527
3257.049897	9938.948205	52.412532
3256.275074	9830.778417	52.417537
3255.689365	9725.251747	52.422541
3254.954251	9606.480537	52.427546
3254.094842	9496.733354	52.432551
3253.872780	9397.064768	52.437556
3252.778035	9301.261620	52.442561
3252.206331	9193.442111	52.447565
3251.618568	9089.093722	52.452570
3250.568744	8988.494796	52.457575
3250.149938	8886.681265	52.462580
3249.650171	8790.828462	52.467585
3248.552675	8690.106833	52.472589
3247.824111	8584.931095	52.477594
3247.054214	8487.292147	52.482599
3246.645007	8396.377118	52.487604
3246.012679	8309.378940	52.492609
3245.141455	8212.713115	52.497613
3244.592728	8110.545162	52.502618
3244.445259	8032.187983	52.507623
3243.567379	7932.580418	52.512628
3242.558713	7839.783687	52.517633
3241.873003	7745.998732	52.522637
3241.385883	7652.211198	52.527642
3240.624138	7564.758928	52.532647
3240.198301	7461.577329	52.537652
3239.398816	7373.616001	52.542657
3238.106033	7283.973411	52.547661
3237.642935	7195.206059	52.552666
3236.557944	7107.923649	52.557671
3236.422334	7026.607570	52.562676
3235.947472	6944.914682	52.567681
3234.833195	6870.400872	52.572685
3234.704653	6778.052247	52.577690
3234.071793	6700.729844	52.582695
3233.496687	6610.878368	52.587700
3232.877961	6519.644055	52.592705
3232.185796	6436.026713	52.597709
3231.847323	6344.262178	52.602714
3230.907956	6268.809894	52.607719
3230.513397	6176.299311	52.612724
3229.639219	6082.272741	52.617729
3229.158897	5996.170110	52.622733
3228.506690	5908.425419	52.627738
3228.079972	5823.578150	52.632743
3227.353408	5730.502178	52.637748
3226.741224	5645.689907	52.642753
3225.822303	5555.923621	52.647757
3224.992777	5460.124095	52.652762
3224.312744	5381.315652	52.657767
3223.763387	5290.313412	52.662772
3223.036379	5205.435438	52.667777
3222.027761	5131.327070	52.672781
3222.048728	5040.310948	52.677786
3221.002741	4957.639936	52.682791
3220.456370	4868.648581	52.687796
3220.129658	4788.764790	52.692801
3218.923317	4706.567074	52.697805
3218.571499	4611.273032	52.702810
3217.943817	4540.211307	52.707815
3216.971110	4446.938502	52.712820
3216.446168	4366.569514	52.717825
3215.864964	4284.419585	52.722829
3215.470319	4199.267508	52.727834
3214.383189	4118.042705	52.732839
3213.973062	4028.974336	52.737844
3213.353195	3951.638552	52.742849
3212.947905	3863.393887	52.747853
3212.806946	3775.225367	52.752858
3211.663615	3699.326579	52.757863
3211.200342	3606.375183	52.762868
3210.188796	3519.207255	52.767873
3208.975340	3434.529237	52.772877
3208.505282	3349.588062	52.777882
3207.794250	3274.500248	52.782887
3207.395683	3191.081928	52.787892
3206.674490	3114.448186	52.792897
3206.119727	3032.051504	52.797901
3205.326195	2949.326513	52.802906
3204.530063	2873.479759	52.807911
3203.574606	2789.059590	52.812916
3203.314784	2709.566474	52.817921
3202.449913	2648.256978	52.822925
3201.750009	2562.538135	52.827930
3201.004662	2488.966434	52.832935
3200.328288	2411.603617	52.837940
3199.917467	2338.632387	52.842945
3199.104646	2267.251665	52.847949
3198.556527	2177.758556	52.852954
3197.676927	2116.963700	52.857959
3197.295012	2039.641622	52.862964
3196.759154	1966.778748	52.867969
3195.819001	1891.499799	52.872973
3195.435830	1816.085783	52.877978
3194.529788	1754.313870	52.882983
3194.021654	1673.353281	52.887988
3193.025588	1589.930239	52.892993
3192.330842	1525.785723	52.897997
3191.826674	1446.971555	52.903002
3190.565045	1395.062941	52.908007
3189.897231	1326.627153	52.913012
3189.388875	1264.274066	52.918017
3188.659139	1203.141735	52.923021
3187.920054	1135.483204	52.928026
3187.071939	1085.398995	52.933031
3186.355281	1020.433286	52.938036
3185.885179	977.534037	52.943041
3184.969442	921.888835	52.948045
3184.550113	864.147787	52.953050
3183.971974	809.783101	52.958055
3183.070702	745.596932	52.963060
3182.502855	681.023267	52.968065
3181.269833	645.341683	52.973069
3181.242815	595.432183	52.978074
3179.895133	542.686494	52.983079
3179.544294	494.108438	52.988084
3178.942780	438.850219	52.993089
3178.049737	385.859623	52.998093
3177.311709	342.737499	53.003098
3176.413101	302.591580	53.008103
3175.755979	253.881865	53.013108
3175.111122	212.988623	53.018113
3174.267129	184.122173	53.023117
3173.316468	152.641162	53.028122
3171.976802	134.761897	53.033127
3170.414180	130.311886	53.038132
3169.006742	134.496878	53.043137
3167.898192	141.714422	53.048141
3167.679944	139.277563	53.053146
3167.243552	149.324547	53.058151
3167.159914	149.690943	53.063156
3166.929960	151.467835	53.068161
3165.242480	152.962842	53.073165
3164.730588	146.255061	53.078170
3164.121031	155.229947	53.083175
3163.744765	144.571840	53.088180
3163.291925	151.366706	53.093185
3162.814697	154.381874	53.098189
3162.369806	152.231231	53.103194
3161.205302	151.904423	53.108199
3160.691042	154.013700	53.113204
3160.268109	154.117153	53.118209
3159.201017	157.082317	53.123213
3158.853575	149.525797	53.128218
3157.998205	159.835025	53.133223
3157.291782	152.034713	53.138228
3156.960463	148.727454	53.143233
3156.133052	153.669913	53.148237
3155.713010	143.380070	53.153242
3154.646458	153.872610	53.158247
3154.095983	146.689459	53.163252
3153.746788	139.195611	53.168257
3153.261167	145.676346	53.173261
3152.702653	140.414529	53.178266
3151.793267	138.115099	53.183271
3151.141546	148.148741	53.188276
3150.406992	144.884722	53.193281
3149.455474	153.327521	53.198285
3148.888875	139.153727	53.203290
3148.865513	156.216699	53.208295
3147.822806	140.248896	53.213300
3147.344404	144.772914	53.218305
3146.429578	140.652743	53.223309
3145.918904	141.947873	53.228314
3145.087874	143.646678	53.233319
3144.855416	146.161349	53.238324
3144.365391	139.308920	53.243329
3142.625033	150.184210	53.248333
3142.626473	145.145661	53.253338
3142.001980	151.764991	53.258343
3141.440015	143.636064	53.263348
3140.623657	142.681368	53.268353
3139.823854	142.060942	53.273357
3139.560537	141.491744	53.278362
3138.761250	151.663493	53.283367
3138.036629	154.923427	53.288372
3138.265044	150.365953	53.293377
3137.159597	147.438853	53.298381
3136.620894	142.693511	53.303386
3135.528564	149.064756	53.308391
3134.468661	150.298205	53.313396
3134.329731	147.960292	53.318401
3133.611303	147.075311	53.323405
3132.902133	148.130020	53.328410
3132.887663	136.410262	53.333415
3131.681837	140.473580	53.338420
3130.704792	134.786712	53.343425
3129.760411	151.128772	53.348429
3129.485764	140.216869	53.353434
3129.083459	139.791416	53.358439
3128.144659	141.497979	53.363444
3128.366492	140.217086	53.368449
3127.015669	140.684341	53.373453
3126.562573	134.472171	53.378458
3125.492518	145.785156	53.383463
3125.245518	137.625314	53.388468
3125.055236	141.592877	53.393473
3124.327428	149.267995	53.398477
3123.885799	136.768214	53.403482
3122.606394	136.418417	53.408487
3121.392139	134.615941	53.413492
3120.610246	133.039980	53.418497
3120.051733	142.089425	53.423501
3119.674370	129.151181	53.428506
3118.841109	134.558047	53.433511
3119.189159	137.329180	53.438516
3118.410497	131.848808	53.443521
3117.166119	141.355698	53.448525
3116.514788	138.101149	53.453530
3115.808167	141.088803	53.458535
3115.576009	137.172515	53.463540
3115.359904	127.016394	53.468545
3113.988094	140.358520	53.473549
3113.453360	137.350886	53.478554
3112.487757	141.340795	53.483559
3111.497540	142.723390	53.488564
3111.708945	136.039269	53.493569
3110.723323	140.566271	53.498573
3110.659398	133.578677	53.503578
3109.211121	141.156241	53.508583
3108.479439	132.963168	53.513588
3108.081184	137.869008	53.518593
3107.805211	134.875582	53.523597
3107.408573	137.495672	53.528602
3106.550139	131.933409	53.533607
3105.471182	132.464740	53.538612
3104.907561	134.495217	53.543617
3103.855413	141.653790	53.548621
3103.434946	134.133446	53.553626
3102.803247	137.849597	53.558631
3102.581433	130.988060	53.563636
3102.094546	125.243502	53.568641
3101.003032	142.719088	53.573645
3100.774295	132.670121	53.578650
3099.922920	139.746626	53.583655
3099.086338	136.468472	53.588660
3098.350077	129.895358	53.593665
3097.159634	138.170166	53.598669
3096.797364	123.440051	53.603674
3096.098363	123.945934	53.608679
3095.818321	127.958830	53.613684
3095.521888	127.816073	53.618689
3094.611003	131.769001	53.623693
3093.816404	131.364003	53.628698
3093.010150	133.964480	53.633703
3092.237291	134.506667	53.638708
3091.638471	132.922718	53.643713
3090.297544	139.133551	53.648717
3090.169265	134.548216	53.653722
3089.781717	132.407522	53.658727
3088.987860	133.837882	53.663732
3088.638580	128.277834	53.668737
3087.415110	136.355790	53.673741
3087.055630	125.083014	53.678746
3086.805053	135.445596	53.683751
3086.203835	136.380025	53.688756
3085.766051	122.419510	53.693761
3084.419024	134.187963	53.698765
3084.336393	127.706453	53.703770
3083.811782	125.443526	53.708775
3082.021716	132.472795	53.713780
3081.703572	132.685056	53.718785
3081.054002	132.964999	53.723789
3080.541029	136.206928	53.728794
3079.848141	136.983341	53.733799
3078.825948	139.182570	53.738804
3078.825987	131.870241	53.743809
3078.284138	134.088444	53.748813
3077.724142	131.068554	53.753818
3076.657355	142.711763	53.758823
3076.211593	142.826622	53.763828
3075.691446	132.529827	53.768833
3074.580120	137.574878	53.773837
3074.216779	123.229811	53.778842
3073.501191	139.379610	53.783847
3072.749965	137.550131	53.788852
3072.375041	132.292091	53.793857
3071.522404	135.439694	53.798861
3070.995347	131.235125	53.803866
3069.960128	144.608559	53.808871
3069.146347	137.753832	53.813876
3068.822358	141.152940	53.818881
3067.549671	139.632033	53.823885
3067.213931	133.481528	53.828890
3066.524352	133.223981	53.833895
3066.173733	136.103834	53.838900
3066.364168	141.904194	53.843905
3064.592485	142.163908	53.848909
3064.198841	128.165456	53.853914
3063.939864	131.106226	53.858919
3062.287854	139.136231	53.863924
3062.458697	124.624495	53.868929
3061.967875	142.741500	53.873933
3061.357219	135.942065	53.878938
3059.909876	137.440277	53.883943
3059.265404	135.640716	53.888948
3059.117067	131.515511	53.893953
3058.442260	139.695111	53.898957
3057.859846	135.553685	53.903962
3057.179166	137.819690	53.908967
3056.517181	141.400497	53.913972
3055.855305	136.026888	53.918977
3054.733234	142.539798	53.923981
3054.320669	145.514315	53.928986
3053.767835	136.307030	53.933991
3052.808268	142.663491	53.938996
3052.827511	135.565772	53.944001
3051.925101	143.910183	53.949005
3051.285059	131.529192	53.954010
3050.395027	136.436172	53.959015
3049.724035	146.044827	53.964020
3049.013810	132.707561	53.969025
3047.726147	134.043099	53.974029
3047.394091	134.250239	53.979034
3046.683330	134.438407	53.984039
3046.047010	136.473418	53.989044
3045.813299	136.340076	53.994049
3044.790107	137.714500	53.999053
3044.720936	141.477425	54.004058
3043.784335	141.598398	54.009063
3042.979633	140.364626	54.014068
3042.863984	133.789288	54.019073
3041.941535	133.159835	54.024077
3040.764527	129.079357	54.029082
3040.559547	129.386359	54.034087
3040.340377	133.282674	54.039092
3039.346284	127.897551	54.044097
3038.418102	133.210909	54.049101
3037.947757	137.650659	54.054106
3037.042047	134.000259	54.059111
3036.462809	134.912779	54.064116
3036.295226	134.900767	54.069121
3035.527236	134.588728	54.074125
3034.331770	134.762226	54.079130
3033.814681	139.376144	54.084135
3032.996386	134.540046	54.089140
3032.832054	127.489884	54.094145
3032.019545	132.127834	54.099149
3031.539765	132.161275	54.104154
3030.864603	129.624086	54.109159
3029.802643	134.822545	54.114164
3029.523637	121.450686	54.119169
3028.458047	127.601845	54.124173
3028.049316	127.293153	54.129178
3027.223579	132.466246	54.134183
3026.345455	133.822594	54.139188
3025.940965	128.071467	54.144193
3024.999916	129.042261	54.149197
3025.443647	130.027078	54.154202
3024.254948	133.716047	54.159207
3023.312274	138.139406	54.164212
3023.330674	133.780847	54.169217
3022.243502	135.398307	54.174221
3021.547406	124.413191	54.179226
3021.083523	131.333091	54.184231
3020.349838	134.812864	54.189236
3019.792193	135.157630	54.194241
3018.794918	137.844046	54.199245
3017.526812	137.034062	54.204250
3017.341081	136.540426	54.209255
3016.877145	136.065515	54.214260
3016.632006	128.879561	54.219265
3015.516354	137.887237	54.224269
3014.216692	131.198051	54.229274
3014.229627	128.606438	54.234279
3013.549321	129.067295	54.239284
3013.362760	130.976901	54.244289
3011.776917	133.493503	54.249293
3011.406829	124.828544	54.254298
3011.358753	137.836322	54.259303
3010.047760	131.425382	54.264308
3009.504667	115.298860	54.269313
3008.327068	127.548746	54.274317
3008.660689	127.140043	54.279322
3007.639192	123.470754	54.284327
3006.783906	123.890461	54.289332
3006.223364	131.287130	54.294337
3005.423760	133.794509	54.299341
3004.872646	125.446267	54.304346
3004.381316	125.823123	54.309351
3003.698131	129.558734	54.314356
3003.160359	124.444977	54.319361
3002.160001	127.697169	54.324365
3001.826727	124.981565	54.329370
3001.431729	123.157935	54.334375
3000.781488	133.483018	54.339380
3000.096372	128.767851	54.344385
2999.614616	131.750639	54.349389
2998.543119	126.584011	54.354394
2997.083918	126.397594	54.359399
2996.533468	134.171083	54.364404
2996.385589	120.308678	54.369409
2995.814485	124.543412	54.374413
2994.569899	128.041414	54.379418
2994.852558	118.208628	54.384423
2993.649931	128.628892	54.389428
2992.524155	120.942131	54.394433
2993.222520	131.576744	54.399437
2992.347936	126.007794	54.404442
2991.484950	119.963586	54.409447
2990.599914	129.591440	54.414452
2990.174926	120.824555	54.419457
2988.906768	125.909046	54.424461
2988.428292	120.707793	54.429466
2987.562001	126.044524	54.434471
2987.222056	132.497598	54.439476
2986.777241	130.506827	54.444481
2985.553404	128.535499	54.449485
2984.539493	130.320836	54.454490
2984.957121	128.394655	54.459495
2983.749164	132.982558	54.464500
2982.959855	124.588975	54.469505
2982.471793	127.746915	54.474509
2981.769645	122.727565	54.479514
2981.180586	121.186962	54.484519
2980.666527	123.373184	54.489524
2980.229341	121.077567	54.494529
2979.563996	130.789850	54.499533
2978.888859	119.368940	54.504538
2978.317950	128.592991	54.509543
2977.537254	128.504969	54.514548
2976.736681	120.612249	54.519553
2975.644296	134.587142	54.524557
2975.096899	135.708958	54.529562
2974.521792	127.709023	54.534567
2973.695120	131.707968	54.539572
2973.252457	120.316803	54.544577
2972.587673	126.610259	54.549581
2972.145961	121.759165	54.554586
2971.552644	125.410738	54.559591
2970.711577	125.521712	54.564596
2970.369408	118.785760	54.569601
2969.677750	125.283540	54.574605
2969.314612	128.998803	54.579610
2967.960319	128.720652	54.584615
2966.685338	128.245005	54.589620
2967.029929	122.500875	54.594625
2966.140967	127.012161	54.599629
2965.161017	127.133844	54.604634
2964.404875	126.054810	54.609639
2963.829025	121.832544	54.614644
2963.844826	116.521172	54.619649
2963.176660	125.708554	54.624653
2962.146388	128.531664	54.629658
2961.527928	121.333334	54.634663
2960.914297	126.517157	54.639668
2960.712268	118.896752	54.644673
2959.552382	128.185928	54.649677
2958.313209	125.293961	54.654682
2957.960166	127.417144	54.659687
2957.576991	129.460216	54.664692
2956.975641	118.006966	54.669697
2955.728085	123.123466	54.674701
2955.142363	120.550479	54.679706
2955.069914	120.699839	54.684711
2954.354628	125.320785	54.689716
2953.818621	125.387129	54.694721
2952.914752	120.837247	54.699725
2952.239146	120.032997	54.704730
2951.712163	123.036146	54.709735
2951.277752	123.631037	54.714740
2950.490981	125.424140	54.719745
2949.166871	134.457181	54.724749
2948.518274	122.044529	54.729754
2948.671896	119.649134	54.734759
2947.761728	125.818346	54.739764
2946.849199	119.458938	54.744769
2946.480833	131.159629	54.749773
2945.543000	125.229665	54.754778
2945.060195	118.121444	54.759783
2944.572614	120.693528	54.764788
2944.266546	126.054127	54.769793
2942.812379	131.218571	54.774797
2941.570898	126.451260	54.779802
2941.991114	127.463772	54.784807
2940.889150	132.482372	54.789812
2940.339555	122.434980	54.794817
2939.430230	130.640445	54.799821
2939.127941	128.658480	54.804826
2938.274742	119.696369	54.809831
2937.771741	125.315222	54.814836
2937.651444	122.948481	54.819841
2936.905296	126.741829	54.824845
2935.831287	122.320102	54.829850
2934.781642	121.026764	54.834855
2933.843954	124.888370	54.839860
2933.737892	121.787373	54.844865
2933.297497	124.512838	54.849869
2932.461877	121.175739	54.854874
2931.775499	117.432225	54.859879
2931.128635	133.074883	54.864884
2930.539612	122.921733	54.869889
2930.003687	121.824017	54.874893
2929.692521	119.809230	54.879898
2928.643238	131.197217	54.884903
2927.365500	126.009801	54.889908
2926.816793	116.953028	54.894913
2926.227140	133.160631	54.899917
2926.016951	123.150762	54.904922
2925.451326	117.927703	54.909927
2924.199835	121.658600	54.914932
2923.920557	119.183638	54.919937
2923.294364	123.725020	54.924941
2922.967463	127.015286	54.929946
2922.772788	123.122217	54.934951
2921.061496	123.986243	54.939956
2920.210685	111.037389	54.944961
2919.753038	121.232843	54.949965
2919.369149	119.101804	54.954970
2919.434043	121.905123	54.959975
2918.482330	120.603735	54.964980
2917.529919	119.065631	54.969985
2916.065126	124.843326	54.974989
2915.257078	125.892852	54.979994
2915.121916	116.291340	54.984999
2914.613699	126.810432	54.990004
2913.905421	119.895086	54.995009
2913.344374	131.383579	55.000013
2912.667132	128.382169	55.005018
2912.114504	123.213729	55.010023
2911.489355	124.438441	55.015028
2911.081443	118.701338	55.020033
2910.447952	125.899294	55.025037
2909.010730	125.293101	55.030042
2908.449197	118.500307	55.035047
2907.208539	124.043125	55.040052
2907.620666	114.582946	55.045057
2906.917744	119.280727	55.050061
2906.192304	122.789887	55.055066
2905.284925	119.335192	55.060071
2904.956458	122.928085	55.065076
2904.685390	116.029206	55.070081
2903.744251	117.689620	55.075085
2902.021997	114.588920	55.080090
2902.030381	112.862147	55.085095
2901.157238	118.418732	55.090100
2900.747363	115.199139	55.095105
2899.900544	117.000930	55.100109
2899.500408	125.876855	55.105114
2898.776886	117.735730	55.110119
2898.363849	118.990506	55.115124
2898.157894	108.632173	55.120129
2897.347410	115.924713	55.125133
2896.207660	114.304554	55.130138
2895.337868	113.195218	55.135143
2894.258615	114.135573	55.140148
2894.157326	114.738271	55.145153
2893.587669	115.437987	55.150157
2893.270646	121.571752	55.155162
2893.056460	117.022434	55.160167
2891.541837	125.036880	55.165172
2890.456178	118.957725	55.170177
2889.959318	110.574584	55.175181
2889.490434	113.171500	55.180186
2889.018171	118.286559	55.185191
2888.319578	119.127914	55.190196
2887.866878	115.269078	55.195201
2887.446202	118.859572	55.200205
2886.441333	112.915820	55.205210
2885.401434	112.224363	55.210215
2884.357068	112.451803	55.215220
2883.810853	107.286224	55.220225
2883.346762	117.123970	55.225229
2883.056472	116.292955	55.230234
2882.620266	118.048258	55.235239
2881.747285	115.353458	55.240244
2881.397422	109.774990	55.245249
2881.177926	113.943321	55.250253
2879.924182	109.800611	55.255258
2878.979908	115.903024	55.260263
2877.954290	116.248047	55.265268
2877.367551	116.544116	55.270273
2876.856383	112.971583	55.275277
2876.854472	115.617374	55.280282
2876.588303	106.073394	55.285287
2874.733453	115.356610	55.290292
2874.034541	107.972321	55.295297
2873.259810	108.748138	55.300301
2872.745957	106.006570	55.305306
2872.175814	106.398090	55.310311
2871.944672	112.282706	55.315316
2871.974121	106.946511	55.320321
2871.056022	114.931242	55.325325
2869.993072	116.752212	55.330330
2869.506175	115.316133	55.335335
2868.844075	119.047359	55.340340
2867.868611	116.850064	55.345345
2866.585989	113.483193	55.350349
2866.228727	120.945772	55.355354
2866.304434	111.242707	55.360359
2865.227863	122.027082	55.365364
2864.596615	116.776565	55.370369
2864.138809	112.278754	55.375373
2862.791957	116.305820	55.380378
2862.584294	117.216428	55.385383
2861.993514	123.543424	55.390388
2861.108925	112.710961	55.395393
2859.909285	119.513056	55.400397
2859.176315	117.777200	55.405402
2859.505083	115.553183	55.410407
2858.632200	110.100420	55.415412
2858.285431	117.628703	55.420417
2857.929220	110.833986	55.425421
2856.834736	113.041259	55.430426
2855.929754	106.952948	55.435431
2855.015318	115.358227	55.440436
2854.296133	110.818645	55.445441
2854.140669	113.013849	55.450445
2852.924830	119.210046	55.455450
2852.572802	112.924995	55.460455
2852.144856	120.974771	55.465460
2851.739436	112.626533	55.470465
2850.423680	112.609843	55.475469
2849.309029	112.090638	55.480474
2849.251853	112.583168	55.485479
2848.681544	110.076640	55.490484
2848.078457	111.200878	55.495489
2847.586245	120.666467	55.500493
2847.029228	110.878126	55.505498
2846.550721	109.178913	55.510503
2845.230323	124.545102	55.515508
2844.607775	109.626653	55.520513
2843.610077	111.534762	55.525517
2842.900407	109.884924	55.530522
2842.744287	103.814679	55.535527
2842.135856	117.620009	55.540532
2841.438777	107.311678	55.545537
2841.215697	119.741844	55.550541
2840.414036	112.718532	55.555546
2839.222363	113.334304	55.560551
2838.435596	121.982234	55.565556
2837.977034	109.612927	55.570561
2837.600907	109.465647	55.575565
2837.091730	108.726518	55.580570
2836.689853	109.210069	55.585575
2835.158333	110.626405	55.590580
2834.692531	116.559417	55.595585
2833.647497	110.402287	55.600589
2833.077778	110.160992	55.605594
2832.624619	116.463280	55.610599
2831.875491	120.170701	55.615604
2831.732812	117.008076	55.620609
2831.447859	113.899372	55.625613
2830.977830	112.263051	55.630618
2829.712149	109.618012	55.635623
2828.996200	111.539940	55.640628
2828.198642	111.714155	55.645633
2827.950476	110.940285	55.650637
2826.987723	115.492220	55.655642
2825.859409	114.080906	55.660647
2825.375885	113.393444	55.665652
2824.418863	107.817706	55.670657
2824.252828	125.576398	55.675661
2823.493319	116.272261	55.680666
2823.435065	114.993445	55.685671
2822.695912	114.700981	55.690676
2821.751542	120.551583	55.695681
2821.069563	118.378345	55.700685
2820.022778	112.380590	55.705690
2819.633826	108.784809	55.710695
2818.350851	116.840986	55.715700
2817.761447	117.054624	55.720705
2817.469259	117.782711	55.725709
2816.986345	113.438009	55.730714
2817.235255	108.497716	55.735719
2816.299298	107.821664	55.740724
2815.461898	111.355098	55.745729
2814.566841	119.956406	55.750733
2813.590431	113.587424	55.755738
2812.628589	114.424834	55.760743
2811.979458	116.200348	55.765748
2811.958504	115.009497	55.770753
2811.013927	116.047635	55.775757
2810.404621	119.615900	55.780762
2810.132553	112.481948	55.785767
2809.046607	113.378858	55.790772
2808.430145	111.535074	55.795777
2807.271940	118.332462	55.800781
2806.750074	116.774079	55.805786
2806.399958	114.710697	55.810791
2805.046242	116.565981	55.815796
2804.958862	109.011660	55.820801
2804.524879	112.377858	55.825805
2803.964807	121.555448	55.830810
2803.577414	115.320657	55.835815
2802.772016	122.814042	55.840820
2802.303170	112.821170	55.845825
2800.770864	118.765157	55.850829
2800.034419	114.823386	55.855834
2800.057545	106.530594	55.860839
2799.202298	111.839793	55.865844
2798.469441	107.025066	55.870849
2798.524545	106.222258	55.875853
2797.184254	113.676012	55.880858
2796.772139	109.630258	55.885863
2795.907312	114.351769	55.890868
2795.329194	112.205783	55.895873
2795.001886	109.604835	55.900877
2793.636033	116.794942	55.905882
2793.088996	110.173373	55.910887
2792.571623	112.271754	55.915892
2792.234130	108.033251	55.920897
2791.355081	104.738735	55.925901
2790.833773	108.252485	55.930906
2789.540260	105.892074	55.935911
2788.685252	108.144476	55.940916
2788.166675	108.344827	55.945921
2787.711886	112.719948	55.950925
2787.183031	109.471757	55.955930
2786.988136	102.865791	55.960935
2786.215965	117.847758	55.965940
2785.772322	106.967189	55.970945
2784.478807	107.913397	55.975949
2783.785486	100.843955	55.980954
2783.199772	103.756099	55.985959
2782.384324	115.545419	55.990964
2781.911181	111.163133	55.995969
2781.482103	104.247467	56.000973
2781.114039	110.423107	56.005978
2780.713933	105.469802	56.010983
2779.674152	116.833269	56.015988
2778.972632	110.830985	56.020993
2778.061446	109.487172	56.025997
2777.492958	114.294610	56.031002
2776.043139	114.091252	56.036007
2775.515849	109.170343	56.041012
2775.292565	106.409121	56.046017
2774.930974	114.989904	56.051021
2774.270868	107.077570	56.056026
2773.551340	101.071659	56.061031
2773.137916	108.027134	56.066036
2772.164834	105.385780	56.071041
2770.942458	103.395705	56.076045
2770.159280	111.897760	56.081050
2769.827331	105.010492	56.086055
2768.923918	113.256396	56.091060
2769.019310	103.430773	56.096065
2768.584229	100.939431	56.101069
2768.149279	109.469594	56.106074
2767.805997	102.036386	56.111079
2766.574361	111.192181	56.116084
2765.717918	115.282281	56.121089
2764.673021	108.990938	56.126093
2763.074393	116.197942	56.131098
2763.287519	104.237650	56.136103
2763.091518	108.450908	56.141108
2762.527612	102.640629	56.146113
2761.530769	106.001194	56.151117
2761.046011	111.814686	56.156122
2760.503114	102.472758	56.161127
2759.478050	107.309289	56.166132
2758.066014	105.180717	56.171137
2757.922197	100.900432	56.176141
2757.512133	111.921007	56.181146
2757.387341	102.389987	56.186151
2756.422607	109.004707	56.191156
2756.264038	111.143207	56.196161
2755.206728	107.802984	56.201165
2753.945504	110.042721	56.206170
2753.525348	112.953412	56.211175
2752.765837	113.666250	56.216180
2752.172513	109.552793	56.221185
2752.289101	114.912984	56.226189
2750.886703	120.372158	56.231194
2750.278432	114.200391	56.236199
2748.915073	119.875123	56.241204
2748.324107	111.392438	56.246209
2748.058277	108.760065	56.251213
2747.541134	118.820028	56.256218
2746.958215	107.419735	56.261223
2746.439177	113.688285	56.266228
2746.512931	110.945370	56.271233
2746.230393	105.017527	56.276237
2744.882873	114.048270	56.281242
2743.752494	105.268195	56.286247
2742.499520	118.207931	56.291252
2742.070899	117.235968	56.296257
2741.531501	116.493725	56.301261
2740.511548	119.588648	56.306266
2740.006411	114.413699	56.311271
2739.522125	117.968098	56.316276
2739.144211	109.270978	56.321281
2738.551299	110.286516	56.326285
2738.262697	115.027959	56.331290
2737.811841	118.821374	56.336295
2736.458012	125.144595	56.341300
2735.452192	116.946761	56.346305
2735.153469	121.747565	56.351309
2734.439924	115.349459	56.356314
2734.285679	115.027289	56.361319
2732.970439	125.672082	56.366324
2732.338248	112.746701	56.371329
2731.630166	96.299538	56.376333
2730.913048	111.592209	56.381338
2730.424735	106.812667	56.386343
2729.816200	123.736741	56.391348
2729.800782	116.934708	56.396353
2729.153683	110.194862	56.401357
2728.065820	120.857627	56.406362
2727.173374	113.101853	56.411367
2726.445935	118.046987	56.416372
2726.384059	120.024885	56.421377
2725.386670	109.536602	56.426381
2724.556177	113.110311	56.431386
2723.996077	107.393330	56.436391
2723.547465	114.177986	56.441396
2722.669936	108.074355	56.446401
2721.757279	110.172020	56.451405
2720.618362	115.021703	56.456410
2720.164797	107.213414	56.461415
2719.546120	114.678436	56.466420
2719.250343	106.112146	56.471425
2718.655852	109.936427	56.476429
2718.531107	118.580538	56.481434
2718.533363	113.775166	56.486439
2717.112874	113.687597	56.491444
2716.338119	106.338804	56.496449
2715.108486	109.861927	56.501453
2713.877786	111.273847	56.506458
2713.635941	99.843687	56.511463
2713.153135	114.908814	56.516468
2712.202097	110.693485	56.521473
2711.705490	116.765578	56.526477
2710.910877	111.577354	56.531482
2710.711921	101.490612	56.536487
2710.506041	105.959367	56.541492
2709.598723	115.009604	56.546497
2709.562979	103.571844	56.551501
2708.187538	104.413654	56.556506
2707.881217	106.160184	56.561511
2707.028147	101.465890	56.566516
2705.884970	106.560242	56.571521
2705.010116	109.692337	56.576525
2704.308921	107.670424	56.581530
2703.642109	106.057885	56.586535
2703.084682	110.687782	56.591540
2702.502775	104.133769	56.596545
2702.286871	110.312214	56.601549
2701.502373	115.215394	56.606554
2701.269672	109.947701	56.611559
2700.597487	113.891840	56.616564
2699.282926	104.832218	56.621569
2698.980555	114.107066	56.626573
2698.123738	111.086258	56.631578
2697.795580	104.983856	56.636583
2696.682365	115.800159	56.641588
2695.668011	113.856250	56.646593
2695.408649	113.560339	56.651597
2694.055786	110.413541	56.656602
2694.222142	100.940522	56.661607
2693.724030	112.936116	56.666612
2693.002128	113.906210	56.671617
2692.974113	110.918594	56.676621
2692.110066	116.942972	56.681626
2691.631922	109.744792	56.686631
2690.577965	108.845387	56.691636
2689.302443	111.766903	56.696641
2688.312272	106.885263	56.701645
2687.488989	112.613733	56.706650
2687.257581	102.000058	56.711655
2687.370538	110.688792	56.716660
2686.565560	108.680279	56.721665
2686.069959	99.346862	56.726669
2685.059840	105.860797	56.731674
2684.143164	106.514065	56.736679
2683.400844	102.556743	56.741684
2682.746156	104.299667	56.746689
2682.496396	105.410495	56.751693
2681.819581	111.266687	56.756698
2681.493566	102.771491	56.761703
2680.306143	104.433775	56.766708
2679.637157	106.078094	56.771713
2678.807622	99.719963	56.776717
2677.988430	101.098256	56.781722
2678.121849	93.565816	56.786727
2677.647268	100.198988	56.791732
2676.390799	107.860661	56.796737
2675.998923	104.904851	56.801741
2675.131404	109.315790	56.806746
2674.351496	103.366401	56.811751
2673.090650	118.178485	56.816756
2672.472398	108.486304	56.821761
2672.634928	103.483414	56.826765
2671.525261	113.691630	56.831770
2671.005892	106.463003	56.836775
2670.670458	109.504078	56.841780
2669.861880	115.329903	56.846785
2669.713450	110.176093	56.851789
2668.647151	109.793129	56.856794
2667.705681	103.763993	56.861799
2667.359388	111.240083	56.866804
2666.668094	108.561634	56.871809
2665.796777	107.413124	56.876813
2664.599929	104.812412	56.881818
2664.658486	105.221609	56.886823
2663.933038	109.615369	56.891828
2663.277947	109.143956	56.896833
2663.017828	114.773792	56.901837
2661.546902	110.305118	56.906842
2661.126284	98.778032	56.911847
2660.624009	105.020821	56.916852
2660.208670	107.761749	56.921857
2659.613502	100.533452	56.926861
2658.217160	104.328627	56.931866
2657.579355	110.195914	56.936871
2656.989918	108.109510	56.941876
2656.569410	103.095764	56.946881
2656.041061	99.784745	56.951885
2655.218645	110.256873	56.956890
2655.228718	109.206770	56.961895
2653.834959	113.198474	56.966900
2653.145004	110.351250	56.971905
2652.790429	104.414812	56.976909
2652.171929	107.059815	56.981914
2650.768070	104.123847	56.986919
2650.595805	102.118890	56.991924
2649.357070	96.173339	56.996929
2649.162004	104.342764	57.001933
2648.559317	107.096377	57.006938
2648.458643	93.470323	57.011943
2647.994414	102.403367	57.016948
2646.774811	100.321666	57.021953
2646.004321	100.262339	57.026957
2645.069692	106.621667	57.031962
2645.333203	106.366636	57.036967
2644.114948	101.617548	57.041972
2643.094435	103.247359	57.046977
2642.307383	107.668230	57.051981
2641.435291	102.986279	57.056986
2641.241466	103.597693	57.061991
2640.945469	105.785737	57.066996
2640.246899	106.637772	57.072001
2640.034682	107.007996	57.077005
2638.776197	104.279278	57.082010
2638.404791	101.460890	57.087015
2637.566044	99.741573	57.092020
2636.873544	110.263333	57.097025
2635.789156	100.513881	57.102029
2634.870675	108.803419	57.107034
2634.818227	98.328499	57.112039
2634.340480	108.292905	57.117044
2633.629040	107.070098	57.122049
2633.039450	109.875156	57.127053
2631.988728	111.381849	57.132058
2631.584994	96.795922	57.137063
2630.325574	101.253727	57.142068
2630.019740	99.036744	57.147073
2629.915293	101.379931	57.152077
2629.079126	107.180868	57.157082
2627.678252	111.187214	57.162087
2627.006771	103.726448	57.167092
2626.506033	98.347881	57.172097
2626.181451	96.274231	57.177101
2625.368415	110.597666	57.182106
2625.114838	103.304664	57.187111
2624.538423	98.210605	57.192116
2623.859692	98.989384	57.197121
2622.871698	97.003092	57.202125
2622.405067	98.455723	57.207130
2621.890171	89.688895	57.212135
2621.159327	102.823966	57.217140
2620.028939	99.378640	57.222145
2619.320439	97.030369	57.227149
2618.607845	104.950773	57.232154
2618.147444	96.492773	57.237159
2617.715291	96.251668	57.242164
2617.253636	100.420339	57.247169
2616.380101	98.420797	57.252173
2615.680773	107.703103	57.257178
2615.186914	95.521858	57.262183
2614.550646	97.649654	57.267188
2613.971982	105.921757	57.272193
2613.175128	98.566111	57.277197
2612.110935	103.749207	57.282202
2611.499200	103.814319	57.287207
2611.346477	109.457371	57.292212
2610.412951	106.437458	57.297217
2609.441856	100.396033	57.302221
2608.119512	102.282705	57.307226
2608.094420	103.172371	57.312231
2608.188501	102.694863	57.317236
2607.423454	107.619196	57.322241
2606.990095	97.382682	57.327245
2605.873716	108.091769	57.332250
2604.617968	100.902991	57.337255
2604.384554	96.894606	57.342260
2603.940541	95.986865	57.347265
2603.440436	90.716350	57.352269
2602.512524	105.729266	57.357274
2601.630689	94.148414	57.362279
2600.912345	102.593205	57.367284
2600.854560	98.108362	57.372289
2600.284879	91.368340	57.377293
2598.812053	98.948589	57.382298
2597.682189	98.318750	57.387303
2597.082544	102.066947	57.392308
2596.622228	98.593521	57.397313
2596.440209	102.018489	57.402317
2595.863395	111.629580	57.407322
2595.591549	96.174035	57.412327
2595.419288	97.648579	57.417332
2593.885399	97.408722	57.422337
2593.270339	98.212145	57.427341
2592.502981	102.828988	57.432346
2592.139833	102.091366	57.437351
2591.104349	102.614963	57.442356
2590.132162	104.710586	57.447361
2589.664312	96.759113	57.452365
2589.130944	107.665760	57.457370
2588.705557	102.145241	57.462375
2588.412515	96.240925	57.467380
2587.128834	103.605691	57.472385
2586.802317	98.391945	57.477389
2585.846053	108.071455	57.482394
2585.306828	100.252968	57.487399
2584.858959	103.793252	57.492404
2583.649644	111.092415	57.497409
2583.039719	97.830525	57.502413
2582.150983	105.451053	57.507418
2581.939975	106.684730	57.512423
2581.429420	114.246926	57.517428
2580.911525	102.556488	57.522433
2580.720337	95.527953	57.527437
2579.280610	103.376883	57.532442
2578.515797	100.485234	57.537447
2578.110031	103.282948	57.542452
2577.474977	106.029074	57.547457
2576.983834	100.929522	57.552461
2575.261880	107.114387	57.557466
2575.170571	95.769042	57.562471
2574.880893	105.590770	57.567476
2574.277988	103.826407	57.572481
2574.194420	91.960678	57.577485
2572.629230	107.402269	57.582490
2572.008875	101.386152	57.587495
2571.399980	111.310218	57.592500
2570.922249	99.068593	57.597505
2569.706607	99.356160	57.602509
2568.463914	111.077605	57.607514
2569.066177	102.243735	57.612519
2568.498894	106.146661	57.617524
2567.851665	105.459185	57.622529
2567.338671	104.916519	57.627533
2565.640695	108.036593	57.632538
2565.459186	108.619063	57.637543
2564.716147	101.894075	57.642548
2564.558705	106.783613	57.647553
2563.419831	101.753352	57.652557
2562.218114	99.368228	57.657562
2561.236882	90.050366	57.662567
2561.526466	92.347898	57.667572
2560.823449	104.107729	57.672577
2560.094162	92.978427	57.677581
2559.469688	100.250233	57.682586
2559.031878	96.760728	57.687591
2558.411536	103.461453	57.692596
2557.578492	101.423025	57.697601
2557.041701	96.532986	57.702605
2555.973038	108.306386	57.707610
2555.949008	96.876516	57.712615
2555.358240	98.739178	57.717620
2554.295018	92.049594	57.722625
2553.388450	93.429814	57.727629
2552.728510	95.512321	57.732634
2552.238796	96.626677	57.737639
2551.585195	93.332745	57.742644
2550.263989	95.394097	57.747649
2549.785442	88.853629	57.752653
2549.001646	95.899259	57.757658
2548.652760	97.876090	57.762663
2548.143059	94.207436	57.767668
2547.899222	91.640398	57.772673
2547.564294	83.354383	57.777677
2546.874560	94.553007	57.782682
2546.020315	94.018160	57.787687
2544.865451	93.404843	57.792692
2544.665450	86.142567	57.797697
2543.964171	89.026722	57.802701
2542.665368	97.176025	57.807706
2542.143187	99.446554	57.812711
2541.933516	98.396127	57.817716
2541.401701	95.290184	57.822721
2540.494154	89.963419	57.827725
2539.127962	90.626456	57.832730
2538.735485	86.081607	57.837735
2538.296129	82.245804	57.842740
2537.600688	86.549572	57.847745
2537.472682	91.208290	57.852749
2536.197765	93.764609	57.857754
2535.572290	92.600145	57.862759
2535.239578	89.109649	57.867764
2534.706084	99.132918	57.872769
2534.532439	82.647354	57.877773
2532.560196	90.072212	57.882778
2532.039696	80.256397	57.887783
2531.555830	86.392222	57.892788
2530.911146	94.379564	57.897793
2530.762192	90.347274	57.902797
2530.341189	83.415276	57.907802
2529.267721	89.374017	57.912807
2528.330682	89.842507	57.917812
2527.916835	96.599108	57.922817
2527.526202	86.697932	57.927821
2526.345775	92.991925	57.932826
2525.194632	80.587175	57.937831
2524.765796	89.276930	57.942836
2524.227602	95.096399	57.947841
2523.859861	90.632976	57.952845
2523.237713	97.641894	57.957850
2523.288374	96.959447	57.962855
2522.552522	100.378051	57.967860
2521.187827	93.119905	57.972865
2520.430631	90.077761	57.977869
2519.423077	101.966628	57.982874
2519.346329	92.800050	57.987879
2518.217918	96.031567	57.992884
2517.072305	87.986387	57.997889
2516.833481	90.388466	58.002893
2516.238840	90.019233	58.007898
2515.946181	88.086973	58.012903
2515.501249	97.650245	58.017908
2514.671044	90.454270	58.022913
2514.650165	89.200652	58.027917
2513.534676	93.356377	58.032922
2512.742878	96.021545	58.037927
2512.538488	93.350269	58.042932
2511.278271	96.453142	58.047937
2510.536732	94.429868	58.052941
2509.690772	92.465893	58.057946
2508.809463	99.247550	58.062951
2509.003325	101.290664	58.067956
2508.191849	99.048038	58.072961
2507.264003	91.101413	58.077965
2506.046190	107.301095	58.082970
2505.866712	102.457337	58.087975
2505.291317	95.711202	58.092980
2504.823857	98.524597	58.097985
2504.833880	96.078760	58.102989
2503.452877	101.055122	58.107994
2502.346825	95.393629	58.112999
2501.695449	89.635457	58.118004
2501.375153	102.333241	58.123009
2501.232467	88.189022	58.128013
2500.245397	103.452437	58.133018
2499.125489	94.781963	58.138023
2498.525141	86.905267	58.143028
2497.904995	99.284853	58.148033
2497.783568	92.227823	58.153037
2497.211403	93.613640	58.158042
2496.101368	93.068062	58.163047
2495.214900	87.950855	58.168052
2494.536697	97.710320	58.173057
2494.584640	92.528483	58.178061
2493.672129	95.219818	58.183066
2492.696609	90.282042	58.188071
2492.004416	86.179613	58.193076
2490.919427	91.082470	58.198081
2490.699310	91.004853	58.203085
2490.153722	94.694867	58.208090
2489.964321	86.884092	58.213095
2489.368531	88.868403	58.218100
2488.022845	92.133125	58.223105
2487.756582	90.377532	58.228109
2486.939495	94.336589	58.233114
2485.941364	92.861252	58.238119
2485.384702	96.302116	58.243124
2484.797345	100.630438	58.248129
2484.503292	89.030441	58.253133
2483.880420	95.704756	58.258138
2483.334776	95.449119	58.263143
2482.046683	96.916291	58.268148
2481.044271	97.419254	58.273153
2481.032039	92.810583	58.278157
2480.984710	100.628299	58.283162
2479.341070	98.067709	58.288167
2478.353094	103.508177	58.293172
2477.865002	99.526767	58.298177
2477.466244	101.118589	58.303181
2476.755329	94.131165	58.308186
2476.530906	98.655188	58.313191
2476.476631	89.071894	58.318196
2475.180072	97.267400	58.323201
2474.694717	91.099543	58.328205
2473.847299	93.692912	58.333210
2472.593645	96.002459	58.338215
2472.003362	90.535416	58.343220
2470.965494	95.808761	58.348225
2470.741177	89.142341	58.353229
2470.487128	95.379794	58.358234
2469.863193	97.724566	58.363239
2469.855589	93.248914	58.368244
2468.655836	101.111304	58.373249
2468.008323	83.341818	58.378253
2467.337134	96.092089	58.383258
2466.569116	100.354198	58.388263
2465.489326	94.673621	58.393268
2464.591871	97.327255	58.398273
2464.036641	83.430813	58.403277
2463.737951	93.355118	58.408282
2463.497537	96.967694	58.413287
2463.090184	96.204088	58.418292
2461.661741	90.392474	58.423297
2460.475360	86.835977	58.428301
2460.118232	92.128716	58.433306
2459.433106	92.268760	58.438311
2459.124925	87.851213	58.443316
2458.906471	89.042745	58.448321
2458.282702	79.829978	58.453325
2457.075373	93.273474	58.458330
2456.586214	90.503659	58.463335
2456.050075	88.463828	58.468340
2454.871529	86.077139	58.473345
2454.012711	83.998140	58.478349
2453.235182	92.523311	58.483354
2452.874515	89.236150	58.488359
2452.464242	89.359594	58.493364
2451.774033	84.906318	58.498369
2451.547685	88.494383	58.503373
2451.150969	89.345354	58.508378
2450.038738	87.659804	58.513383
2449.328983	91.569725	58.518388
2448.712801	88.603348	58.523393
2448.138707	85.341232	58.528397
2446.820829	90.412594	58.533402
2446.452734	88.821252	58.538407
2446.192115	90.451427	58.543412
2445.284426	87.482789	58.548417
2445.072073	86.596636	58.553421
2443.503328	91.145649	58.558426
2442.866658	85.811670	58.563431
2442.488008	83.991615	58.568436
2442.055593	89.613794	58.573441
2441.862194	93.291750	58.578445
2440.474061	89.626864	58.583450
2439.752622	88.241985	58.588455
2439.119573	86.205700	58.593460
2438.322143	94.294948	58.598465
2438.405383	88.854457	58.603469
2437.807949	90.487749	58.608474
2436.845411	91.307575	58.613479
2436.143953	84.181183	58.618484
2435.096993	92.810053	58.623489
2435.061575	90.061735	58.628493
2433.994992	95.317495	58.633498
2432.772013	86.280209	58.638503
2432.441593	82.346453	58.643508
2431.920056	86.365898	58.648513
2431.715060	88.640224	58.653517
2431.438742	90.063485	58.658522
2430.291166	85.455133	58.663527
2429.715034	92.669729	58.668532
2429.231421	93.614504	58.673537
2428.068512	88.559973	58.678541
2426.772624	91.361471	58.683546
2426.645227	89.201625	58.688551
2426.266253	89.869175	58.693556
2425.450667	87.405433	58.698561
2425.079225	79.584744	58.703565
2423.557491	94.308408	58.708570
2422.841115	90.056577	58.713575
2422.853221	85.098760	58.718580
2421.999377	92.417681	58.723585
2421.896664	85.323516	58.728589
2421.218643	83.995557	58.733594
2420.337054	88.079330	58.738599
2419.240006	88.006005	58.743604
2418.557564	91.766789	58.748609
2418.482544	77.451162	58.753613
2417.771022	88.758504	58.758618
2416.778884	91.082160	58.763623
2416.446175	85.951994	58.768628
2415.805207	90.512503	58.773633
2415.191590	91.938571	58.778637
2413.760962	91.437958	58.783642
2413.122632	85.360610	58.788647
2412.993664	83.484445	58.793652
2411.933140	84.777724	58.798657
2411.637413	90.819807	58.803661
2411.092774	96.169477	58.808666
2410.603588	97.352831	58.813671
2409.844195	79.312375	58.818676
2408.853497	90.065895	58.823681
2408.999389	86.083460	58.828685
2407.712727	84.514189	58.833690
2406.695104	86.417087	58.838695
2406.259660	87.662696	58.843700
2405.599937	92.938494	58.848705
2405.232852	87.988674	58.853709
2404.263565	90.032119	58.858714
2403.162722	81.727488	58.863719
2402.591545	87.074193	58.868724
2401.666356	93.892569	58.873729
2401.847280	78.857807	58.878733
2401.327378	85.717798	58.883738
2400.892171	83.701371	58.888743
2399.785350	86.918557	58.893748
2398.877389	90.861189	58.898753
2398.341732	88.336561	58.903757
2397.842813	86.139588	58.908762
2396.814778	96.107288	58.913767
2395.786999	89.305111	58.918772
2395.183585	88.676085	58.923777
2394.791214	82.472213	58.928781
2394.257798	87.442212	58.933786
2393.867145	90.322607	58.938791
2393.766824	93.909255	58.943796
2393.093038	90.534723	58.948801
2392.300955	79.613967	58.953805
2391.522277	76.947744	58.958810
2390.246405	91.340036	58.963815
2389.473733	91.434666	58.968820
2388.272527	88.623592	58.973825
2388.222494	79.309579	58.978829
2387.792208	83.838010	58.983834
2387.041052	93.214436	58.988839
2386.673713	86.108682	58.993844
2386.171998	88.681237	58.998849
2385.459484	85.929887	59.003853
2384.416852	89.554113	59.008858
2383.789641	84.790087	59.013863
2383.472019	85.288075	59.018868
2381.902760	90.566244	59.023873
2380.849125	80.220722	59.028877
2381.478176	90.932930	59.033882
2380.809553	85.967572	59.038887
2379.887514	88.173067	59.043892
2379.237762	90.160693	59.048897
2379.118704	85.474378	59.053901
2377.795310	84.529927	59.058906
2376.976500	80.772449	59.063911
2376.886784	78.852075	59.068916
2376.188782	88.567161	59.073921
2375.758175	80.153459	59.078925
2374.547358	97.877546	59.083930
2374.010520	92.864390	59.088935
2373.831568	79.947676	59.093940
2372.126133	89.651086	59.098945
2371.916904	78.475940	59.103949
2371.136020	90.637484	59.108954
2370.725800	90.459356	59.113959
2370.402742	82.348964	59.118964
2369.150275	84.532016	59.123969
2368.372936	75.112644	59.128973
2367.812579	81.745876	59.133978
2366.897010	86.574386	59.138983
2366.994383	77.037810	59.143988
2366.410725	84.256848	59.148993
2365.341191	78.659415	59.153997
2364.741735	80.779357	59.159002
2363.965610	77.984812	59.164007
2364.144902	80.300792	59.169012
2362.575503	80.837572	59.174017
2361.938957	73.776677	59.179021
2361.098614	75.814656	59.184026
2360.506954	71.982421	59.189031
2360.688571	68.335712	59.194036
2359.255531	76.975732	59.199041
2358.341068	80.514098	59.204045
2357.803877	78.375778	59.209050
2356.995241	80.913188	59.214055
2357.118509	75.943869	59.219060
2356.494933	82.033720	59.224065
2355.563292	77.708586	59.229069
2354.583446	75.850032	59.234074
2353.934413	74.768960	59.239079
2353.398701	73.491674	59.244084
2352.930512	80.401239	59.249089
2352.307138	77.282561	59.254093
2351.422581	71.578506	59.259098
2350.606537	77.269045	59.264103
2350.276898	67.176700	59.269108
2349.430104	75.658450	59.274113
2349.112613	71.176593	59.279117
2347.651801	75.786507	59.284122
2347.168933	83.703943	59.289127
2347.407921	75.532974	59.294132
2346.670131	82.743633	59.299137
2345.678709	79.672496	59.304141
2344.711188	80.143465	59.309146
2343.994564	73.633879	59.314151
2343.453635	71.541990	59.319156
2343.034490	84.165469	59.324161
2342.489919	79.484028	59.329165
2341.129919	74.357046	59.334170
2340.054296	72.684998	59.339175
2339.984090	67.026424	59.344180
2339.427726	73.411479	59.349185
2339.295136	70.448082	59.354189
2338.804898	76.260534	59.359194
2337.998851	76.132333	59.364199
2336.979650	76.768056	59.369204
2336.113227	73.709494	59.374209
2336.201431	67.335830	59.379213
2334.914608	75.025620	59.384218
2333.813586	75.874275	59.389223
2333.832029	73.152279	59.394228
2332.667853	75.439446	59.399233
2333.146252	69.197603	59.404237
2331.942489	79.719934	59.409242
2330.680897	81.022743	59.414247
2330.358043	75.953272	59.419252
2329.343239	81.506492	59.424257
2329.193691	76.830923	59.429261
2328.032845	72.493283	59.434266
2327.093771	77.208187	59.439271
2326.932401	81.361435	59.444276
2326.177027	84.509850	59.449281
2325.554381	78.798904	59.454285
2325.541027	82.722770	59.459290
2325.085829	83.517040	59.464295
2323.877819	78.001717	59.469300
2322.803814	81.972749	59.474305
2322.506682	81.266095	59.479309
2322.026469	82.172797	59.484314
2321.413595	77.411859	59.489319
2320.493089	69.129314	59.494324
2320.208342	78.050594	59.499329
2318.889875	83.234575	59.504333
2317.962095	89.723017	59.509338
2316.981065	80.053891	59.514343
2317.396081	81.215650	59.519348
2316.537647	84.518659	59.524353
2316.304455	80.870647	59.529357
2315.378237	78.846225	59.534362
2314.740773	81.203189	59.539367
2313.799166	80.607927	59.544372
2312.738056	80.376115	59.549377
2312.297010	77.617039	59.554381
2312.110988	78.424094	59.559386
2311.580707	78.992398	59.564391
2310.626666	80.874965	59.569396
2309.301842	78.272940	59.574401
2309.029109	71.287996	59.579405
2309.055844	71.570001	59.584410
2307.822092	90.288757	59.589415
2307.032624	82.432995	59.594420
2306.215781	90.755298	59.599425
2305.794258	72.551321	59.604429
2305.450106	79.215079	59.609434
2304.726146	85.828924	59.614439
2304.191733	79.873164	59.619444
2303.134960	78.828667	59.624449
2302.867548	78.716516	59.629453
2302.354485	86.325312	59.634458
2301.269525	86.478883	59.639463
2300.607139	75.735310	59.644468
2299.724925	79.010415	59.649473
2299.441777	82.796474	59.654477
2298.976114	78.454034	59.659482
2297.889460	80.877946	59.664487
2296.997058	76.089816	59.669492
2296.224340	84.772058	59.674497
2295.735139	72.796546	59.679501
2295.628465	74.893801	59.684506
2294.920120	78.827964	59.689511
2294.251242	72.601924	59.694516
2292.970605	81.239184	59.699521
2292.465084	73.568154	59.704525
2292.253074	85.396368	59.709530
2291.674101	83.426643	59.714535
2290.735940	75.025152	59.719540
2289.632259	78.016036	59.724545
2289.105805	75.313014	59.729549
2288.749272	72.802375	59.734554
2288.724550	79.842149	59.739559
2288.215541	80.797593	59.744564
2286.648159	80.278561	59.749569
2286.082954	74.748057	59.754573
2285.639956	73.093752	59.759578
2284.416135	80.641336	59.764583
2283.698502	74.949801	59.769588
2282.809435	73.886102	59.774593
2282.651357	68.486498	59.779597
2282.460174	70.750962	59.784602
2281.703802	77.785990	59.789607
2281.677606	62.570372	59.794612
2280.395291	73.309813	59.799617
2279.269929	74.695517	59.804621
2278.856786	74.866042	59.809626
2277.597767	72.312771	59.814631
2277.104788	75.948799	59.819636
2276.566768	82.307039	59.824641
2275.889309	74.339373	59.829645
2275.222045	69.256574	59.834650
2274.527164	82.341265	59.839655
2274.664991	63.991523	59.844660
2274.185865	77.625871	59.849665
2273.289054	74.575675	59.854669
2272.472263	75.414024	59.859674
2271.484046	72.531823	59.864679
2271.125650	71.840780	59.869684
2269.877299	83.042167	59.874689
2269.244666	77.011636	59.879693
2268.501416	70.974366	59.884698
2268.104813	78.716396	59.889703
2268.293850	74.966579	59.894708
2267.607906	81.198147	59.899713
2266.479152	81.919326	59.904718
2265.767983	78.375558	59.909722
2264.969369	81.075075	59.914727
2264.371476	75.950018	59.919732
2263.396323	85.610662	59.924737
2262.927142	72.136130	59.929742
2262.594702	79.658379	59.934746
2261.747303	85.344028	59.939751
2260.757104	79.386092	59.944756
2259.580428	86.611421	59.949761
2259.346621	79.948626	59.954766
2258.841618	81.358502	59.959770
2258.681483	80.078575	59.964775
2258.292500	78.981067	59.969780
2256.789525	78.791675	59.974785
2256.088034	77.506042	59.979790
2255.816026	78.701210	59.984794
2255.255444	72.791777	59.989799
2254.803032	69.537303	59.994804
2253.519119	71.862329	59.999809
2252.915418	73.808539	60.004814
2252.272636	71.321199	60.009818
2252.090870	82.472023	60.014823
2251.748657	66.964277	60.019828
2250.510077	64.203053	60.024833
2249.376115	70.940695	60.029838
2249.055415	73.114813	60.034842
2248.336690	80.309190	60.039847
2248.154092	72.699386	60.044852
2246.416656	75.097238	60.049857
2245.959933	78.648912	60.054862
2245.545639	72.563679	60.059866
2244.983843	66.189475	60.064871
2244.364851	66.452441	60.069876
2244.188464	71.005738	60.074881
2243.860220	77.894133	60.079886
2243.070250	72.824824	60.084890
2241.527088	72.330872	60.089895
2241.684451	60.832550	60.094900
2240.363529	78.340983	60.099905
2239.799136	71.385796	60.104910
2239.286549	71.473465	60.109914
2238.753648	77.857275	60.114919
2238.172334	64.519954	60.119924
2236.970813	70.764695	60.124929
2235.909555	72.134708	60.129934
2235.561910	65.228505	60.134938
2235.103627	72.317157	60.139943
2234.666357	68.651163	60.144948
2234.018407	71.817134	60.149953
2233.698881	69.090574	60.154958
2232.800349	66.263700	60.159962
2231.742310	64.494331	60.164967
2231.611377	61.972747	60.169972
2230.252732	64.100961	60.174977
2229.468752	66.823239	60.179982
2228.979218	69.237013	60.184986
2228.237730	70.335242	60.189991
2228.279956	67.559841	60.194996
2227.818006	59.965059	60.200001
2226.843740	70.750898	60.205006
2226.063078	72.359493	60.210010
2225.221775	84.943851	60.215015
2224.962022	79.149546	60.220020
2224.110437	69.866063	60.225025
2223.334566	64.880793	60.230030
2222.483205	69.376241	60.235034
2221.695115	71.159390	60.240039
2221.564142	64.005748	60.245044
2220.951466	75.893392	60.250049
2220.202421	76.573325	60.255054
2219.427704	70.350007	60.260058
2218.457156	77.351407	60.265063
2218.108583	70.034458	60.270068
2217.614027	72.885260	60.275073
2216.541417	74.189325	60.280078
2215.869771	72.739126	60.285082
2215.136601	72.904784	60.290087
2214.989912	71.410988	60.295092
2214.460586	73.453030	60.300097
2213.701217	74.248805	60.305102
2212.845030	70.231315	60.310106
2212.039070	82.046628	60.315111
2211.654624	78.921449	60.320116
2210.877388	62.381709	60.325121
2209.933802	63.454506	60.330126
2209.532599	70.324192	60.335130
2208.922222	79.353657	60.340135
2208.941586	65.734408	60.345140
2207.478869	74.935297	60.350145
2206.908847	70.170603	60.355150
2206.362228	69.266634	60.360154
2205.203863	81.842059	60.365159
2204.394693	64.199005	60.370164
2203.771790	74.965413	60.375169
2203.497720	81.263513	60.380174
2202.867670	73.518668	60.385178
2202.495433	75.188464	60.390183
2202.103790	69.135679	60.395188
2200.982329	76.578928	60.400193
2200.081959	77.096461	60.405198
2199.896073	65.055682	60.410202
2199.193667	73.174075	60.415207
2198.139125	78.062684	60.420212
2197.298555	78.941425	60.425217
2196.631525	74.895928	60.430222
2196.187821	66.197542	60.435226
2195.415833	73.415238	60.440231
2195.597691	73.545191	60.445236
2194.397660	77.372408	60.450241
2192.813554	75.396185	60.455246
2192.609477	72.530677	60.460250
2192.325138	76.659165	60.465255
2191.947944	68.037426	60.470260
2191.546225	77.121989	60.475265
2190.458717	72.447381	60.480270
2189.910666	72.729798	60.485274
2189.088858	69.472194	60.490279
2188.490218	70.381004	60.495284
2187.327269	70.938316	60.500289
2186.299360	69.048544	60.505294
2186.044668	75.525689	60.510298
2185.593416	72.790084	60.515303
2185.409140	71.139302	60.520308
2184.894765	72.943141	60.525313
2183.769268	74.415725	60.530318
2183.239036	70.343283	60.535322
2182.333182	74.919106	60.540327
2181.903402	65.114304	60.545332
2180.856679	63.972986	60.550337
2180.088955	74.389571	60.555342
2179.370661	70.056410	60.560346
2178.729144	78.917128	60.565351
2179.111576	63.015872	60.570356
2178.229080	73.242489	60.575361
2177.595884	71.042457	60.580366
2177.070911	59.270461	60.585370
2175.742146	75.152403	60.590375
2174.732857	72.864331	60.595380
2173.708988	71.846207	60.600385
2173.020698	75.013162	60.605390
2172.955803	73.561824	60.610394
2172.229943	77.086508	60.615399
2172.271652	74.103572	60.620404
2171.539438	75.750860	60.625409
2170.929135	64.022666	60.630414
2170.129728	69.173550	60.635418
2168.631719	76.132541	60.640423
2168.831803	69.680936	60.645428
2168.177187	69.670935	60.650433
2167.062264	75.614310	60.655438
2166.384981	68.381614	60.660442
2165.451014	75.394919	60.665447
2165.190419	70.596257	60.670452
2164.754059	76.008725	60.675457
2164.469480	64.111537	60.680462
2163.283153	66.921189	60.685466
2162.204114	70.001822	60.690471
2162.199446	64.264162	60.695476
2161.446133	64.061050	60.700481
2160.374349	68.078302	60.705486
2160.361642	68.200084	60.710490
2159.470146	65.045587	60.715495
2159.018777	65.905923	60.720500
2158.054751	68.271780	60.725505
2157.150465	66.034831	60.730510
2156.711569	72.478745	60.735514
2155.959133	69.684133	60.740519
2155.501414	66.968980	60.745524
2154.669849	69.076534	60.750529
2153.718480	79.366249	60.755534
2153.307417	69.747319	60.760538
2152.773088	77.035683	60.765543
2152.178556	71.084314	60.770548
2150.879110	75.221030	60.775553
2150.433542	69.672852	60.780558
2149.753647	64.867753	60.785562
2149.013270	78.365599	60.790567
2148.833400	68.228726	60.795572
2148.472145	72.624964	60.800577
2147.380354	77.083784	60.805582
2146.797618	73.300184	60.810586
2146.110330	75.582793	60.815591
2145.783468	73.986005	60.820596
2144.553295	77.443795	60.825601
2143.660418	79.735122	60.830606
2143.244936	75.708977	60.835610
2142.667228	68.865818	60.840615
2141.971441	68.895624	60.845620
2141.431936	71.027435	60.850625
2141.444738	72.450990	60.855630
2140.394819	71.791393	60.860634
2139.598265	74.841479	60.865639
2139.039465	68.861896	60.870644
2138.272361	67.815652	60.875649
2137.325292	76.494165	60.880654
2136.741894	71.817030	60.885658
2135.948192	73.404578	60.890663
2135.718568	69.066395	60.895668
2134.780788	76.574943	60.900673
2133.789447	74.568799	60.905678
2133.444278	74.567847	60.910682
2132.879906	79.410128	60.915687
2132.695547	70.831597	60.920692
2132.051884	75.159695	60.925697
2130.443568	73.706693	60.930702
2130.278969	77.086044	60.935706
2129.412708	73.588563	60.940711
2129.026276	69.596136	60.945716
2128.405654	75.008146	60.950721
2127.389461	82.266830	60.955726
2126.929983	76.729715	60.960730
2126.014763	74.187942	60.965735
2125.852856	79.651754	60.970740
2125.379140	80.460654	60.975745
2123.828011	74.445149	60.980750
2123.262466	76.083277	60.985754
2122.908223	80.301088	60.990759
2122.526324	72.051202	60.995764
2121.882423	83.030804	61.000769
2120.940011	82.832805	61.005774
2120.395947	78.351830	61.010778
2119.519129	83.141373	61.015783
2119.459496	81.281387	61.020788
2118.129867	74.204090	61.025793
2117.268472	75.736116	61.030798
2116.838866	81.532285	61.035802
2116.164106	79.337396	61.040807
2115.631016	76.481195	61.045812
2115.312711	68.398849	61.050817
2114.886777	70.177698	61.055822
2113.689974	76.123638	61.060826
2112.611830	78.518497	61.065831
2112.603350	67.296434	61.070836
2112.204145	71.933628	61.075841
2111.068781	78.880733	61.080846
2110.240801	73.826240	61.085850
2109.525519	76.431788	61.090855
2109.311503	74.501897	61.095860
2108.836140	77.788355	61.100865
2107.397076	78.726451	61.105870
2107.170385	80.286492	61.110874
2106.261872	77.854887	61.115879
2106.176058	74.107083	61.120884
2105.282583	80.251793	61.125889
2103.981782	85.144646	61.130894
2103.560671	81.436824	61.135898
2102.905052	81.830013	61.140903
2102.802968	78.591815	61.145908
2102.335189	83.535994	61.150913
2100.940036	83.157288	61.155918
2100.524312	79.479333	61.160922
2099.807944	89.132437	61.165927
2099.479159	82.307097	61.170932
2098.954579	77.725691	61.175937
2097.968210	82.162935	61.180942
2097.094694	79.999677	61.185946
2096.716181	85.253444	61.190951
2096.022507	89.708914	61.195956
2094.805922	85.785850	61.200961
2094.134714	76.386680	61.205966
2093.840731	81.171268	61.210970
2093.185183	90.985280	61.215975
2092.843940	82.394504	61.220980
2092.155217	90.308078	61.225985
2090.727842	78.021384	61.230990
2090.486158	80.292516	61.235994
2089.453246	87.913263	61.240999
2089.343099	82.807434	61.246004
2088.724402	83.961255	61.251009
2088.339944	84.393325	61.256014
2087.275054	87.826805	61.261018
2086.366677	84.036545	61.266023
2085.809351	78.251709	61.271028
2085.604599	77.475191	61.276033
2084.581032	77.782904	61.281038
2083.973263	76.335217	61.286042
2082.886998	87.887836	61.291047
2082.690823	82.060172	61.296052
2082.112380	78.393869	61.301057
2081.881245	84.464764	61.306062
2080.611502	83.048993	61.311066
2079.952584	86.293037	61.316071
2079.471813	84.274175	61.321076
2078.873949	82.588356	61.326081
2077.503999	85.678899	61.331086
2077.233024	83.750858	61.336090
2076.109136	91.692684	61.341095
2076.178832	76.895668	61.346100
2075.428311	90.964844	61.351105
2075.046341	82.809705	61.356110
2074.690395	80.992116	61.361114
2073.194143	86.671931	61.366119
2072.507647	83.864473	61.371124
2072.421309	78.909306	61.376129
2071.591433	78.362079	61.381134
2071.065801	82.217248	61.386138
2069.982398	87.601060	61.391143
2069.437635	77.517529	61.396148
2069.084327	82.817509	61.401153
2067.848965	83.630776	61.406158
2067.298193	83.389480	61.411162
2066.610603	89.724762	61.416167
2066.133319	87.173614	61.421172
2065.958657	93.489053	61.426177
2064.963629	83.927388	61.431182
2064.065973	83.902921	61.436186
2063.138447	86.210449	61.441191
2062.712941	82.901263	61.446196
2062.706207	78.275888	61.451201
2061.767349	80.024455	61.456206
2060.773340	75.269940	61.461210
2059.756858	79.869439	61.466215
2059.529675	87.444733	61.471220
2059.262055	77.638260	61.476225
2058.208535	93.089083	61.481230
2057.319086	83.027011	61.486234
2056.689422	86.780771	61.491239
2056.268026	83.502460	61.496244
2055.664590	86.885826	61.501249
2055.240021	86.556236	61.506254
2054.532393	80.146612	61.511258
2053.894128	86.254780	61.516263
2053.076886	84.588332	61.521268
2052.618794	82.978867	61.526273
2051.434406	89.338736	61.531278
2050.972868	83.561202	61.536282
2050.484196	79.856653	61.541287
2049.897749	78.586896	61.546292
2048.492300	77.951818	61.551297
2047.630357	82.250553	61.556302
2047.292834	77.868860	61.561306
2046.341342	81.382418	61.566311
2046.558219	80.559437	61.571316
2046.173089	80.034820	61.576321
2045.670843	83.227200	61.581326
2044.943426	74.539868	61.586330
2043.820984	83.252732	61.591335
2043.061418	75.744407	61.596340
2042.051897	80.712572	61.601345
2041.073518	83.453917	61.606350
2040.905211	81.148725	61.611354
2040.319046	85.084907	61.616359
2039.954645	78.927616	61.621364
2039.586923	79.017761	61.626369
2038.853814	80.691270	61.631374
2037.527647	78.787023	61.636378
2036.737637	81.161818	61.641383
2036.371987	85.248956	61.646388
2035.985817	78.556595	61.651393
2035.161295	78.401206	61.656398
2034.584296	73.660627	61.661402
2033.612402	75.543922	61.666407
2033.292279	79.824185	61.671412
2032.907804	78.672244	61.676417
2031.910567	76.449243	61.681422
2031.334179	78.652107	61.686426
2029.876735	85.495643	61.691431
2029.970452	76.232869	61.696436
2029.451191	83.647341	61.701441
2028.207434	90.203283	61.706446
2027.586894	89.268162	61.711450
2027.365724	86.820045	61.716455
2026.723163	86.373410	61.721460
2025.989984	84.098925	61.726465
2024.433269	78.715174	61.731470
2023.811356	78.098436	61.736474
2023.628545	85.887182	61.741479
2023.579821	81.636477	61.746484
2022.980987	77.072126	61.751489
2022.392202	76.963648	61.756494
2021.465915	77.137895	61.761498
2020.687956	81.356743	61.766503
2020.092416	80.319062	61.771508
2019.646562	84.097433	61.776513
2018.309620	83.419855	61.781518
2017.565626	83.407793	61.786522
2016.936983	87.191381	61.791527
2016.549409	85.036588	61.796532
2016.846913	88.249265	61.801537
2015.442768	86.820976	61.806542
2014.849026	80.896728	61.811546
2014.057680	95.318666	61.816551
2013.210078	87.358050	61.821556
2012.157095	90.801347	61.826561
2011.168494	92.421463	61.831566
2011.264032	78.038046	61.836570
2010.689394	85.297393	61.841575
2010.464099	84.836223	61.846580
2010.241130	83.038916	61.851585
2008.980696	95.537489	61.856590
2008.374684	85.724170	61.861594
2007.865862	96.604098	61.866599
2006.137343	86.233613	61.871604
2005.329704	86.123103	61.876609
2005.060045	87.703128	61.881614
2004.412487	87.089594	61.886618
2003.674871	86.891319	61.891623
2003.295594	82.409803	61.896628
2002.888603	84.209497	61.901633
2002.424424	78.160855	61.906638
2002.244208	82.047332	61.911642
2001.268691	81.332406	61.916647
2000.109347	86.671194	61.921652
1999.333167	86.303076	61.926657
1998.586128	86.646393	61.931662
1998.082684	83.101871	61.936666
1997.861624	80.457562	61.941671
1996.488643	79.475509	61.946676
1995.680579	83.065982	61.951681
1994.817776	85.066013	61.956686
1994.514204	82.181617	61.961690
1994.502355	88.145924	61.966695
1994.220427	87.043940	61.971700
1993.426299	79.089186	61.976705
1992.313556	86.686890	61.981710
1991.650466	80.522676	61.986714
1990.843863	86.142953	61.991719
1990.089907	90.863734	61.996724
1989.314396	84.767696	62.001729
1988.749677	79.608984	62.006734
1988.408843	81.216185	62.011738
1987.829295	93.590784	62.016743
1986.534807	80.587872	62.021748
1985.592239	79.707450	62.026753
1984.900429	91.590087	62.031758
1985.187445	78.311507	62.036762
1984.300861	89.533936	62.041767
1983.739030	80.590534	62.046772
1983.508787	72.695239	62.051777
1982.231809	81.626380	62.056782
1981.825859	71.554255	62.061786
1981.071503	80.579144	62.066791
1980.709688	83.471990	62.071796
1979.441680	73.820085	62.076801
1978.472855	82.171559	62.081806
1978.006164	75.891256	62.086810
1977.742799	76.010920	62.091815
1977.006520	77.184077	62.096820
1976.952220	78.486876	62.101825
1975.219947	81.522585	62.106830
1974.982369	73.746962	62.111834
1974.234232	83.107486	62.116839
1973.943292	75.707292	62.121844
1973.413053	76.751259	62.126849
1972.024313	83.401875	62.131854
1971.507402	82.557583	62.136858
1971.103979	75.977916	62.141863
1970.388497	75.959405	62.146868
1970.127765	69.270466	62.151873
1968.943576	82.669770	62.156878
1968.631083	73.692010	62.161882
1967.552582	82.739985	62.166887
1967.455032	85.861166	62.171892
1966.229771	83.145496	62.176897
1965.385692	83.857509	62.181902
1965.063795	74.322828	62.186906
1964.661930	84.106861	62.191911
1964.070910	84.098636	62.196916
1963.061956	79.698792	62.201921
1962.024525	76.841260	62.206926
1961.603810	80.301923	62.211930
1960.925741	82.669419	62.216935
1960.858550	83.837456	62.221940
1960.444322	72.859286	62.226945
1959.054506	83.550850	62.231950
1958.686219	76.478877	62.236954
1957.928883	82.953194	62.241959
1957.203965	75.043845	62.246964
1956.388714	78.283460	62.251969
1955.566526	81.110199	62.256974
1954.976175	74.546724	62.261978
1954.459129	74.140598	62.266983
1954.284597	77.984261	62.271988
1953.600789	72.410948	62.276993
1952.402066	87.910292	62.281998
1951.908776	73.701826	62.287002
1951.563343	81.486019	62.292007
1950.837246	82.362581	62.297012
1950.073778	71.461526	62.302017
1949.308920	83.072059	62.307022
1948.938879	78.524631	62.312026
1947.451963	83.223571	62.317031
1947.125426	75.261861	62.322036
1946.916933	79.329615	62.327041
1946.275927	83.663590	62.332046
1946.297386	81.095817	62.337050
1944.618616	81.936416	62.342055
1943.740134	86.189443	62.347060
1943.509168	81.975445	62.352065
1941.730619	85.087368	62.357070
1941.376077	77.398860	62.362074
1941.109259	81.289099	62.367079
1940.269939	77.794152	62.372084
1939.560850	76.118695	62.377089
1938.885851	83.021016	62.382094
1938.770953	72.704905	62.387098
1938.063082	76.720725	62.392103
1937.908541	80.896087	62.397108
1937.695036	77.193031	62.402113
1936.123860	80.988661	62.407118
1935.823258	71.158249	62.412122
1934.641621	84.496333	62.417127
1933.417773	81.826613	62.422132
1933.291934	73.764259	62.427137
1932.731332	86.827161	62.432142
1932.424437	78.447239	62.437146
1931.650673	78.079902	62.442151
1930.739005	82.197297	62.447156
1930.099699	80.961464	62.452161
1929.461584	80.435532	62.457166
1928.999276	77.655664	62.462170
1927.621728	78.123038	62.467175
1926.767396	74.883679	62.472180
1926.614342	75.362221	62.477185
1925.554408	74.934899	62.482190
1925.621562	66.668224	62.487194
1925.271660	78.220396	62.492199
1924.890770	71.973185	62.497204
1924.469880	75.500586	62.502209
1923.134402	84.394379	62.507214
1921.918804	75.327188	62.512218
1920.619732	66.725449	62.517223
1920.007308	69.166977	62.522228
1920.146650	68.805266	62.527233
1919.262406	71.601969	62.532238
1919.340951	68.574056	62.537242
1918.592603	70.734903	62.542247
1917.803188	76.523552	62.547252
1916.579591	71.293239	62.552257
1916.026244	78.942085	62.557262
1915.866998	69.796414	62.562266
1915.539661	80.370161	62.567271
1913.957220	78.933326	62.572276
1913.582056	76.588929	62.577281
1912.815184	77.876271	62.582286
1912.716982	74.661103	62.587290
1911.596821	72.609942	62.592295
1910.483720	78.727904	62.597300
1910.117848	76.318368	62.602305
1909.734099	83.675317	62.607310
1909.514151	69.225901	62.612314
1907.969962	83.234670	62.617319
1907.361228	78.529143	62.622324
1906.877823	72.915632	62.627329
1906.199757	82.862173	62.632334
1905.839752	78.778409	62.637338
1905.209584	80.336827	62.642343
1904.288879	76.569638	62.647348
1903.672201	72.021781	62.652353
1902.880043	77.608804	62.657358
1902.718992	74.291499	62.662362
1901.779878	80.548244	62.667367
1900.798027	80.104015	62.672372
1900.152938	72.570613	62.677377
1900.032969	78.959575	62.682382
1899.460256	74.910230	62.687386
1898.459321	82.439475	62.692391
1897.861960	80.134671	62.697396
1897.640253	75.656211	62.702401
1896.640360	75.064681	62.707406
1895.479378	70.506925	62.712410
1894.530241	83.023292	62.717415
1893.968928	77.346140	62.722420
1893.952030	81.094153	62.727425
1893.199720	80.750387	62.732430
1892.975225	72.493741	62.737434
1891.764418	76.212334	62.742439
1890.849381	78.442754	62.747444
1890.768970	75.078891	62.752449
1890.091060	80.504271	62.757454
1888.929496	69.203203	62.762458
1888.020205	69.869939	62.767463
1887.416548	74.079899	62.772468
1886.982196	62.767312	62.777473
1886.451990	75.624880	62.782478
1886.207342	74.850855	62.787482
1885.624292	79.892126	62.792487
1884.783520	72.097744	62.797492
1884.254133	71.259543	62.802497
1883.597520	82.731168	62.807502
1882.409549	68.531447	62.812506
1881.941553	73.818679	62.817511
1880.875840	66.991957	62.822516
1880.903210	75.365232	62.827521
1879.513738	76.711729	62.832526
1878.790687	73.638990	62.837530
1877.980093	74.545411	62.842535
1877.648692	81.178959	62.847540
1877.189656	66.112061	62.852545
1876.713515	74.130576	62.857550
1876.451782	65.194281	62.862554
1875.561605	82.713515	62.867559
1874.603945	80.700478	62.872564
1874.305047	67.389533	62.877569
1873.655668	81.707830	62.882574
1872.604411	73.279224	62.887578
1871.502854	74.800271	62.892583
1870.699586	67.485379	62.897588
1870.686147	75.462231	62.902593
1870.275556	66.723107	62.907598
1869.875096	61.653551	62.912602
1868.727001	67.276207	62.917607
1867.845970	82.320162	62.922612
1867.710990	74.098332	62.927617
1866.856903	81.340757	62.932622
1865.766655	77.428115	62.937626
1864.816777	82.797400	62.942631
1864.493160	71.441394	62.947636
1864.327747	68.957305	62.952641
1863.718865	77.233391	62.957646
1863.095157	64.688518	62.962650
1861.957333	67.838863	62.967655
1861.161195	69.123323	62.972660
1860.743975	69.975076	62.977665
1860.393994	76.163397	62.982670
1859.585373	75.172060	62.987674
1858.458946	76.297907	62.992679
1857.738174	72.403763	62.997684
1857.964795	68.705149	63.002689
1857.185298	72.554421	63.007694
1856.025296	68.017034	63.012698
1854.918699	76.349064	63.017703
1854.416589	69.346188	63.022708
1854.137266	75.459264	63.027713
1853.750241	84.392105	63.032718
1853.358861	69.176667	63.037722
1851.856397	64.678138	63.042727
1851.198023	72.757829	63.047732
1851.215821	73.618442	63.052737
1850.347788	71.924011	63.057742
1849.404236	68.797823	63.062746
1848.796649	69.035594	63.067751
1847.906553	66.725228	63.072756
1847.678097	63.420250	63.077761
1847.054900	72.999388	63.082766
1846.427556	64.429191	63.087770
1845.727998	65.194650	63.092775
1844.855882	73.042501	63.097780
1844.923266	64.631326	63.102785
1843.620506	78.287359	63.107790
1842.540390	67.238415	63.112794
1842.371539	66.271432	63.117799
1841.723311	68.736461	63.122804
1841.070788	82.891881	63.127809
1839.802430	82.164723	63.132814
1839.267888	73.231291	63.137818
1838.807138	77.290494	63.142823
1838.177866	87.824325	63.147828
1838.150154	73.011253	63.152833
1837.178928	78.372745	63.157838
1835.953169	80.090306	63.162842
1835.468222	68.195880	63.167847
1834.632536	79.129348	63.172852
1834.912802	74.162000	63.177857
1833.837695	79.548372	63.182862
1833.197597	77.021162	63.187866
1832.329248	78.401268	63.192871
1831.948667	79.941858	63.197876
1831.080016	69.854589	63.202881
1829.770237	76.573822	63.207886
1829.439513	71.832585	63.212890
1829.127621	73.428130	63.217895
1828.394514	79.536746	63.222900
1828.013221	69.709896	63.227905
1826.960701	79.442225	63.232910
1825.887857	72.083863	63.237914
1825.588810	74.491519	63.242919
1825.085309	73.599951	63.247924
1824.912072	75.985293	63.252929
1824.035936	85.701657	63.257934
1823.072918	81.771599	63.262938
1822.336096	70.083684	63.267943
1821.826959	70.261194	63.272948
1821.407489	67.496905	63.277953
1820.348852	82.669928	63.282958
1819.978502	70.243549	63.287962
1819.026837	69.650494	63.292967
1818.485868	70.100677	63.297972
1818.385638	70.724520	63.302977
1816.912886	69.482493	63.307982
1816.447610	72.270681	63.312986
1815.925551	67.540869	63.317991
1815.293523	71.930154	63.322996
1814.236475	74.475002	63.328001
1813.020573	77.784763	63.333006
1812.761393	68.597391	63.338010
1812.500226	67.072676	63.343015
1811.750542	66.158892	63.348020
1811.577513	62.707861	63.353025
1811.165660	70.923787	63.358030
1810.743384	66.259005	63.363034
1809.606244	76.054363	63.368039
1808.030072	72.947612	63.373044
1807.172733	70.278768	63.378049
1806.650776	73.440981	63.383054
1806.357415	73.184880	63.388058
1805.976218	65.425962	63.393063
1805.633802	71.912580	63.398068
1805.321471	67.559763	63.403073
1804.061724	74.579899	63.408078
1803.298747	70.037356	63.413082
1802.999294	68.260256	63.418087
1802.103360	73.305723	63.423092
1801.114180	65.224533	63.428097
1800.350406	66.072824	63.433102
1799.809550	63.522326	63.438106
1799.498265	64.475558	63.443111
1798.815809	75.751081	63.448116
1798.115666	62.628409	63.453121
1797.010159	72.211914	63.458126
1796.467006	66.159849	63.463130
1796.685121	63.227265	63.468135
1795.473054	78.655079	63.473140
1794.622024	65.058900	63.478145
1793.987639	71.308907	63.483150
1793.636717	74.863024	63.488154
1793.165126	68.824766	63.493159
1791.939758	77.140811	63.498164
1791.069769	69.647097	63.503169
1790.248654	73.845326	63.508174
1790.034573	65.854930	63.513178
1789.738404	70.862117	63.518183
1789.137057	74.922484	63.523188
1788.040667	66.486630	63.528193
1787.385492	76.325441	63.533198
1786.741671	64.839513	63.538202
1786.437875	61.999386	63.543207
1785.214722	73.537547	63.548212
1784.779849	70.739188	63.553217
1783.825110	73.821907	63.558222
1783.084964	63.890293	63.563226
1783.255783	65.786519	63.568231
1782.370999	76.041180	63.573236
1781.377465	64.240500	63.578241
1780.686733	66.318876	63.583246
1780.257120	69.315691	63.588250
1780.029586	70.767336	63.593255
1778.755273	79.287145	63.598260
1778.358624	75.252691	63.603265
1777.702797	77.112737	63.608270
1776.950472	72.568375	63.613274
1775.918091	76.685128	63.618279
1775.221342	66.153613	63.623284
1774.608503	67.800653	63.628289
1774.159797	76.697859	63.633294
1773.576817	69.059519	63.638298
1773.564585	64.375502	63.643303
1771.890256	79.757682	63.648308
1771.834471	72.076502	63.653313
1771.073093	77.928259	63.658318
1770.215943	76.443551	63.663322
1769.421857	74.806347	63.668327
1768.667784	76.155463	63.673332
1767.955880	66.468086	63.678337
1767.724843	73.896791	63.683342
1767.193738	70.261514	63.688346
1766.850089	68.734732	63.693351
1765.375675	70.589191	63.698356
1765.133669	71.066380	63.703361
1764.437002	65.526883	63.708366
1763.607324	63.670386	63.713370
1762.947512	61.618648	63.718375
1762.011787	67.883507	63.723380
1761.359064	59.305438	63.728385
1760.884406	68.348389	63.733390
1760.355148	63.240098	63.738394
1760.229485	62.130340	63.743399
1758.898802	64.234538	63.748404
1758.580241	67.094725	63.753409
1758.059492	68.793902	63.758414
1757.403685	65.475216	63.763418
1756.185244	62.801463	63.768423
1755.280638	71.500765	63.773428
1754.967108	70.709324	63.778433
1754.317915	68.950625	63.783438
1753.872435	62.439375	63.788442
1753.646820	63.254797	63.793447
1752.254304	65.875607	63.798452
1751.965713	69.884435	63.803457
1751.216958	72.744815	63.808462
1750.646269	67.334942	63.813466
1749.602562	65.947289	63.818471
1748.882313	67.073917	63.823476
1748.629086	62.630867	63.828481
1747.992750	71.384919	63.833486
1747.044893	60.444427	63.838490
1746.475667	67.554433	63.843495
1745.280223	70.496773	63.848500
1744.969759	59.668261	63.853505
1744.359364	60.067570	63.858510
1744.498969	62.626344	63.863514
1743.604253	60.389023	63.868519
1742.513175	71.563550	63.873524
1742.373228	68.340537	63.878529
1741.204651	69.226919	63.883534
1740.114103	73.635855	63.888538
1739.783209	70.002243	63.893543
1738.743854	80.469272	63.898548
1738.712966	63.867896	63.903553
1738.432198	68.790740	63.908558
1737.320346	68.346289	63.913562
1736.852403	67.590745	63.918567
1736.306313	71.108394	63.923572
1735.443407	61.243191	63.928577
1734.442543	69.866995	63.933582
1733.461049	66.211690	63.938586
1732.940582	69.045245	63.943591
1732.292666	67.449351	63.948596
1731.960465	70.789090	63.953601
1731.827986	73.123644	63.958606
1730.442032	69.890032	63.963610
1729.789819	71.743937	63.968615
1728.930954	73.350190	63.973620
1729.047991	75.679546	63.978625
1728.469228	80.747329	63.983630
1726.959862	73.354746	63.988634
1726.558491	74.013936	63.993639
1725.971581	81.451829	63.998644
1725.794362	67.490514	64.003649
1724.170633	80.227708	64.008654
1723.443644	71.906680	64.013658
1723.079817	77.587787	64.018663
1722.232878	78.271117	64.023668
1722.070940	66.469467	64.028673
1721.750494	74.827641	64.033678
1721.389553	70.884975	64.038682
1720.435582	63.876159	64.043687
1718.884825	81.013049	64.048692
1718.871915	67.094670	64.053697
1718.453547	67.783215	64.058702
1717.830152	64.037823	64.063706
1716.698323	64.296239	64.068711
1715.926971	72.703543	64.073716
1715.676923	66.423318	64.078721
1714.840386	71.285744	64.083726
1713.635966	71.116075	64.088730
1713.228619	68.139337	64.093735
1712.985460	76.935057	64.098740
1712.467185	65.216094	64.103745
1711.944398	71.532268	64.108750
1710.934381	69.837687	64.113754
1710.292128	65.113854	64.118759
1709.182580	69.559596	64.123764
1709.107273	70.508372	64.128769
1707.803317	67.271789	64.133774
1707.136787	75.900753	64.138778
1706.547209	70.696216	64.143783
1706.105183	76.266762	64.148788
1705.634304	60.919320	64.153793
1705.205879	69.048083	64.158798
1704.281792	78.451354	64.163802
1703.934371	70.850873	64.168807
1702.837148	76.042898	64.173812
1702.504919	67.701298	64.178817
1701.267522	76.953322	64.183822
1700.591350	82.803926	64.188826
1700.662507	75.111292	64.193831
1699.864829	79.002377	64.198836
1699.669286	60.547556	64.203841
1698.053841	70.334379	64.208846
1697.629041	74.694923	64.213850
1697.186408	72.485639	64.218855
1695.572673	69.244439	64.223860
1695.084599	69.966624	64.228865
1694.355299	76.596811	64.233870
1694.073001	73.388291	64.238874
1693.838286	75.165627	64.243879
1693.168798	75.135336	64.248884
1692.920680	65.047708	64.253889
1691.884866	70.786569	64.258894
1690.968666	67.369169	64.263898
1690.684143	67.295502	64.268903
1689.745195	70.464739	64.273908
1688.762706	71.706510	64.278913
1687.899508	73.414163	64.283918
1687.315663	72.388338	64.288922
1687.150812	65.856706	64.293927
1686.349213	72.947271	64.298932
1686.246377	69.664229	64.303937
1685.251242	70.451079	64.308942
1683.890436	63.632675	64.313946
1683.945774	64.943946	64.318951
1683.526448	67.688358	64.323956
1682.792644	66.863451	64.328961
1681.712067	66.422739	64.333966
1681.067818	65.886442	64.338970
1680.579105	62.339053	64.343975
1679.391719	74.083070	64.348980
1678.777641	69.597173	64.353985
1678.095667	72.519947	64.358990
1677.410504	73.731366	64.363994
1677.039477	65.721265	64.368999
1676.918861	73.137386	64.374004
1676.505780	72.141943	64.379009
1675.330830	70.902285	64.384014
1674.490167	77.764680	64.389018
1673.842641	66.832810	64.394023
1673.061789	76.483928	64.399028
1671.847998	68.613307	64.404033
1671.961843	74.148332	64.409038
1671.041174	69.972259	64.414042
1670.703971	67.355349	64.419047
1670.549849	69.205732	64.424052
1669.691723	66.871378	64.429057
1668.506638	73.576404	64.434062
1667.943923	72.718669	64.439066
1667.382195	70.328068	64.444071
1665.999380	78.869619	64.449076
1665.608927	67.470619	64.454081
1665.077317	68.358144	64.459086
1664.342835	67.943470	64.464090
1664.283353	67.413286	64.469095
1663.758833	68.113290	64.474100
1662.791487	69.695880	64.479105
1661.825901	74.276857	64.484110
1661.380534	65.711478	64.489114
1660.982393	72.118819	64.494119
1659.544946	68.414850	64.499124
1658.914473	68.258682	64.504129
1658.673021	73.804773	64.509134
1657.938359	66.104786	64.514138
1657.860528	62.381697	64.519143
1656.599349	69.479860	64.524148
1655.953614	59.082539	64.529153
1655.801422	67.118637	64.534158
1654.772847	66.484303	64.539162
1653.977635	62.250453	64.544167
1653.119210	69.497579	64.549172
1652.817879	68.549723	64.554177
1652.423444	69.450089	64.559182
1651.355749	71.864556	64.564186
1650.458667	64.920230	64.569191
1649.975665	73.008205	64.574196
1649.843944	68.180043	64.579201
1648.924193	70.256575	64.584206
1647.071852	65.762333	64.589210
1647.054144	62.722873	64.594215
1646.463067	72.729128	64.599220
1645.962792	75.201619	64.604225
1645.313772	71.291288	64.609230
1644.612021	72.240693	64.614234
1644.928285	70.211796	64.619239
1643.584761	76.208973	64.624244
1642.787457	59.982318	64.629249
1642.227322	69.840783	64.634254
1641.782452	68.392909	64.639258
1640.658477	61.170060	64.644263
1639.785776	74.866194	64.649268
1639.334839	64.799863	64.654273
1639.027669	65.379784	64.659278
1638.638068	67.971092	64.664282
1637.702602	67.878566	64.669287
1636.409632	64.315270	64.674292
1636.272036	63.472810	64.679297
1635.541361	70.596634	64.684302
1635.015328	71.852665	64.689306
1634.101308	66.932601	64.694311
1633.327442	73.281483	64.699316
1632.982103	69.074854	64.704321
1632.331122	69.258105	64.709326
1631.621139	69.863145	64.714330
1630.951935	61.659750	64.719335
1629.966123	72.691936	64.724340
1629.608422	69.042004	64.729345
1629.198354	62.347089	64.734350
1628.473652	71.452962	64.739354
1627.422787	61.304969	64.744359
1626.769926	77.981905	64.749364
1626.502247	65.588919	64.754369
1625.865397	66.657476	64.759374
1624.975057	67.788361	64.764378
1624.171711	68.677395	64.769383
1623.206373	75.006154	64.774388
1622.962230	72.617653	64.779393
1622.589059	72.588765	64.784398
1621.814392	67.778665	64.789402
1620.970281	64.554198	64.794407
1620.447668	77.216649	64.799412
1619.798143	71.784369	64.804417
1618.808308	64.838556	64.809422
1618.232624	71.777970	64.814426
1617.575471	63.106744	64.819431
1616.773106	63.669573	64.824436
1616.659689	62.356023	64.829441
1616.137230	64.420224	64.834446
1615.392526	63.687584	64.839450
1614.137728	59.755804	64.844455
1613.532664	68.849492	64.849460
1613.203514	61.948503	64.854465
1612.672182	62.764146	64.859470
1611.320352	71.114882	64.864474
1610.988968	53.625139	64.869479
1610.026753	66.597277	64.874484
1609.851837	63.402361	64.879489
1609.661232	71.212543	64.884494
1608.178634	67.112521	64.889498
1608.017120	66.623877	64.894503
1607.120141	62.590996	64.899508
1606.719261	63.567070	64.904513
1605.532375	60.053520	64.909518
1604.658270	66.429425	64.914522
1604.581561	67.100558	64.919527
1603.513867	68.799801	64.924532
1603.027738	58.841737	64.929537
1602.629092	58.585509	64.934542
1602.089552	62.207039	64.939546
1601.060632	64.770792	64.944551
1600.385070	62.471126	64.949556
1599.967800	61.234051	64.954561
1599.346356	62.309843	64.959566
1598.315791	59.591349	64.964570
1598.124079	56.187740	64.969575
1596.971525	64.916064	64.974580
1596.622617	56.383928	64.979585
1596.467950	62.888145	64.984590
1595.269314	60.169205	64.989594
1594.575969	65.554218	64.994599
1593.875430	63.927088	64.999604
1593.416738	57.056958	65.004609
1592.429433	60.793011	65.009614
1591.412277	59.651890	65.014618
1591.005361	53.200382	65.019623
1590.278402	65.425316	65.024628
1590.271937	61.580680	65.029633
1590.117025	59.173361	65.034638
1589.161525	64.477323	65.039642
1588.656880	58.715141	65.044647
1587.510987	67.113525	65.049652
1586.275601	56.114930	65.054657
1585.331717	64.955562	65.059662
1584.829912	66.398890	65.064666
1584.166677	55.349744	65.069671
1583.960973	65.533584	65.074676
1583.958248	67.012283	65.079681
1583.316903	52.349289	65.084686
1582.117435	59.282169	65.089690
1581.737932	54.327878	65.094695
1580.529981	68.695171	65.099700
1579.419241	57.942864	65.104705
1578.664193	57.270418	65.109710
1578.162199	59.370986	65.114714
1578.079777	58.213574	65.119719
1577.503599	63.831155	65.124724
1577.193059	62.419112	65.129729
1576.796399	69.319204	65.134734
1575.471302	63.028781	65.139738
1574.772559	57.901766	65.144743
1574.771767	67.357410	65.149748
1573.827433	61.214578	65.154753
1572.679998	64.879755	65.159758
1572.132870	68.212862	65.164762
1571.846987	53.129052	65.169767
1570.422124	64.631886	65.174772
1569.562712	62.104360	65.179777
1569.611844	53.518318	65.184782
1568.841366	63.278968	65.189786
1568.462874	54.978075	65.194791
1567.640519	64.984831	65.199796
1566.880226	53.832701	65.204801
1566.144433	56.076304	65.209806
1565.486196	61.508991	65.214810
1565.084949	57.340755	65.219815
1563.550875	68.744658	65.224820
1563.368541	60.983323	65.229825
1562.802763	56.060913	65.234830
1562.168894	64.154969	65.239834
1562.009364	51.573768	65.244839
1560.635168	66.399756	65.249844
1559.773076	55.821604	65.254849
1559.516690	58.499847	65.259854
1558.888964	56.272524	65.264858
1558.664430	52.900194	65.269863
1558.059288	58.285111	65.274868
1556.814781	56.862396	65.279873
1556.216559	64.959035	65.284878
1555.438000	66.347893	65.289882
1555.394953	58.033009	65.294887
1554.310202	64.377077	65.299892
1553.288839	63.628246	65.304897
1552.852149	59.098594	65.309902
1552.256518	63.046291	65.314906
1552.401204	54.837037	65.319911
1551.003564	65.063825	65.324916
1550.053036	57.101615	65.329921
1549.952725	61.943838	65.334926
1548.778544	67.177475	65.339930
1548.069148	55.283250	65.344935
1547.342603	62.166379	65.349940
1546.806677	59.183249	65.354945
1546.384205	59.507393	65.359950
1545.593671	64.241178	65.364954
1545.488472	56.822683	65.369959
1544.617630	57.067257	65.374964
1543.613533	56.853870	65.379969
1542.869417	69.384098	65.384974
1542.459600	61.090541	65.389978
1542.043773	55.825117	65.394983
1540.786641	64.081104	65.399988
1540.262976	58.139035	65.404993
1540.008976	62.573765	65.409998
1539.140788	62.733021	65.415002
1539.038272	58.060523	65.420007
1537.743375	54.426143	65.425012
1536.997190	65.442186	65.430017
1536.662783	63.707009	65.435022
1535.897484	63.626429	65.440026
1534.919383	55.457374	65.445031
1534.263376	61.979895	65.450036
1533.747374	62.003483	65.455041
1533.386698	63.912902	65.460046
1532.269463	71.369328	65.465050
1531.810169	57.061617	65.470055
1530.822074	70.085951	65.475060
1530.286678	60.455266	65.480065
1530.208765	55.103984	65.485070
1529.512243	64.742247	65.490074
1528.618147	52.093361	65.495079
1527.611063	60.920735	65.500084
1527.113066	53.398164	65.505089
1526.881299	51.939093	65.510094
1525.706153	61.038378	65.515098
1525.135510	53.547187	65.520103
1524.407827	67.541377	65.525108
1524.168577	59.856102	65.530113
1523.940731	58.416490	65.535118
1522.641080	58.249744	65.540122
1521.892459	52.916946	65.545127
1521.386443	59.122887	65.550132
1520.270189	59.669983	65.555137
1519.889410	57.328956	65.560142
1518.614222	60.926012	65.565146
1518.292438	54.592174	65.570151
1518.008258	59.994788	65.575156
1517.580537	65.101065	65.580161
1517.419461	58.375395	65.585166
1515.897074	72.558498	65.590170
1515.133945	60.941489	65.595175
1514.329636	64.659260	65.600180
1514.063637	62.290299	65.605185
1513.612795	57.235335	65.610190
1512.495696	63.576262	65.615194
1511.680079	58.075333	65.620199
1511.286028	65.249700	65.625204
1510.746391	57.085339	65.630209
1510.548880	52.088462	65.635214
1509.329317	59.814625	65.640218
1508.615315	56.281742	65.645223
1507.739695	59.204123	65.650228
1507.373983	57.433651	65.655233
1507.451152	54.821622	65.660238
1505.995275	65.326794	65.665242
1505.740943	55.132509	65.670247
1504.907655	59.138253	65.675252
1503.895230	58.283302	65.680257
1502.923491	53.301707	65.685262
1502.035358	63.281041	65.690266
1502.079887	56.446765	65.695271
1501.125356	61.344011	65.700276
1500.812460	63.304461	65.705281
1500.635065	59.461850	65.710286
1499.671486	65.077850	65.715290
1498.930692	59.577143	65.720295
1498.475046	61.938588	65.725300
1497.863883	57.442358	65.730305
1496.764876	68.827463	65.735310
1495.500875	63.740370	65.740314
1495.076480	61.050379	65.745319
1495.030202	62.359302	65.750324
1494.485841	57.467973	65.755329
1493.878977	59.662677	65.760334
1492.631118	59.119196	65.765338
1492.281142	61.128623	65.770343
1491.766548	63.870009	65.775348
1490.763850	63.820201	65.780353
1489.957906	58.608134	65.785358
1489.069885	63.495578	65.790362
1488.599887	55.540345	65.795367
1488.050418	68.157252	65.800372
1487.628676	64.722762	65.805377
1487.657673	62.885917	65.810382
1486.556616	66.061220	65.815386
1485.741950	53.036794	65.820391
1485.351736	63.614953	65.825396
1484.668615	61.784736	65.830401
1483.466588	59.218373	65.835406
1482.650103	70.428814	65.840410
1482.414690	52.563484	65.845415
1481.790927	58.902075	65.850420
1481.185575	52.984263	65.855425
1480.448356	55.502449	65.860430
1479.333521	60.685282	65.865434
1479.139698	56.733385	65.870439
1478.058986	61.218436	65.875444
1477.850520	64.396088	65.880449
1476.653189	66.551340	65.885454
1475.731174	65.003976	65.890458
1475.667255	59.216900	65.895463
1475.422155	55.891515	65.900468
1474.654640	56.637470	65.905473
1473.667847	55.340790	65.910478
1473.035166	56.302076	65.915482
1472.643621	49.841246	65.920487
1471.648214	54.678784	65.925492
1470.746412	57.344742	65.930497
1470.426635	53.802019	65.935502
1469.432269	55.776879	65.940506
1469.316814	55.106287	65.945511
1468.826445	59.461874	65.950516
1467.582550	61.567468	65.955521
1466.823527	57.812177	65.960526
1466.106936	52.478250	65.965530
1465.646707	45.212901	65.970535
1465.546846	55.202960	65.975540
1464.660903	54.465703	65.980545
1463.800360	56.275955	65.985550
1462.999690	63.124412	65.990554
1462.434327	57.862884	65.995559
1462.178868	59.005910	66.000564
1460.782669	57.978641	66.005569
1460.701817	55.047098	66.010574
1459.960048	61.202609	66.015578
1459.666173	52.747127	66.020583
1458.273997	56.683546	66.025588
1457.487666	51.562469	66.030593
1456.826353	50.421256	66.035598
1456.221815	46.050213	66.040602
1456.208730	49.520457	66.045607
1455.687802	52.332399	66.050612
1454.501610	55.117692	66.055617
1453.814592	55.448442	66.060622
1452.939991	62.982155	66.065626
1452.898391	59.006572	66.070631
1452.083613	56.299727	66.075636
1451.169901	58.548141	66.080641
1450.926377	50.189433	66.085646
1450.029611	53.085442	66.090650
1449.335814	54.573879	66.095655
1448.061093	54.256050	66.100660
1447.317358	62.710740	66.105665
1447.471525	54.559473	66.110670
1446.489940	68.178325	66.115674
1446.235270	52.992495	66.120679
1445.712131	55.599168	66.125684
1444.870447	55.217875	66.130689
1444.001776	48.322822	66.135694
1443.503611	61.745639	66.140698
1442.819614	58.671425	66.145703
1441.580076	63.185642	66.150708
1440.838174	60.960512	66.155713
1441.101198	52.779956	66.160718
1440.397281	59.028063	66.165722
1439.544072	57.492613	66.170727
1438.377919	61.627181	66.175732
1437.812887	62.058232	66.180737
1437.688527	50.090347	66.185742
1437.144063	59.065506	66.190746
1435.986415	56.356172	66.195751
1435.408911	66.326945	66.200756
1434.782835	65.103127	66.205761
1434.721875	61.187698	66.210766
1433.485260	66.679135	66.215770
1432.431046	70.002345	66.220775
1431.903108	65.757524	66.225780
1431.509753	68.146994	66.230785
1431.039529	67.591994	66.235790
1429.914708	63.881165	66.240794
1429.178203	60.342279	66.245799
1428.853986	64.514305	66.250804
1428.156939	65.008610	66.255809
1427.860258	55.066707	66.260814
1426.227913	65.926163	66.265818
1425.892302	68.400087	66.270823
1425.208719	65.201862	66.275828
1424.812298	67.122142	66.280833
1424.589030	61.345767	66.285838
1423.606941	71.022655	66.290842
1422.886242	57.941899	66.295847
1421.958326	65.549080	66.300852
1421.565806	71.155366	66.305857
1421.184218	63.171982	66.310862
1420.231165	67.603615	66.315866
1419.659587	55.688597	66.320871
1418.635193	58.367258	66.325876
1418.266832	61.425050	66.330881
1417.884369	64.030145	66.335886
1416.820400	65.827860	66.340890
1416.282970	60.029871	66.345895
1415.926194	66.494076	66.350900
1414.731321	70.867240	66.355905
1413.893351	56.179530	66.360910
1413.067706	64.842840	66.365914
1412.556757	62.865142	66.370919
1412.204445	56.214454	66.375924
1411.869183	55.211637	66.380929
1411.508368	58.802190	66.385934
1410.522778	63.895020	66.390938
1409.597169	57.460486	66.395943
1409.105467	60.888322	66.400948
1408.389333	60.108588	66.405953
1407.938304	53.321254	66.410958
1406.529551	63.242876	66.415962
1406.078098	60.526344	66.420967
1405.596686	59.041332	66.425972
1404.790726	65.983064	66.430977
1404.846344	62.837908	66.435982
1403.523322	73.687449	66.440986
1402.637086	67.268278	66.445991
1402.113806	61.372742	66.450996
1401.645985	61.347045	66.456001
1401.917187	56.633085	66.461006
1400.795504	68.592448	66.466010
1399.998119	58.377062	66.471015
1399.063070	57.963208	66.476020
1398.507317	59.374340	66.481025
1397.616089	57.760936	66.486030
1396.497703	61.697475	66.491034
1396.467054	60.399370	66.496039
1396.055910	52.699726	66.501044
1395.479056	58.301247	66.506049
1394.642264	62.026171	66.511054
1393.151949	61.488693	66.516058
1392.855671	67.108897	66.521063
1392.603415	60.641204	66.526068
1391.870745	64.077923	66.531073
1391.068765	58.009844	66.536078
1389.784306	58.593260	66.541082
1389.322466	59.881348	66.546087
1388.668201	70.267876	66.551092
1388.471486	65.438231	66.556097
1388.664774	55.927568	66.561102
1387.612364	60.011097	66.566106
1386.738234	56.723926	66.571111
1386.093704	59.425590	66.576116
1385.282422	60.588373	66.581121
1384.504053	54.158641	66.586126
1383.676754	63.237085	66.591130
1383.230807	57.659879	66.596135
1383.139400	64.418114	66.601140
1382.397200	56.344898	66.606145
1381.152923	55.213492	66.611150
1380.753197	63.072086	66.616154
1380.209804	59.832506	66.621159
1379.024563	61.066014	66.626164
1378.116199	65.384613	66.631169
1377.617930	54.173076	66.636174
1377.255513	67.576210	66.641178
1376.961234	63.830191	66.646183
1376.388602	60.846262	66.651188
1375.238547	62.291238	66.656193
1375.175531	54.869488	66.661198
1374.267672	58.189362	66.666202
1373.024337	52.920360	66.671207
1372.159836	61.336913	66.676212
1371.325849	64.745191	66.681217
1371.304888	60.384781	66.686222
1370.624892	68.182414	66.691226
1370.474868	59.014322	66.696231
1369.830264	62.801872	66.701236
1368.861484	54.101557	66.706241
1368.495583	51.544062	66.711246
1367.112944	53.375416	66.716250
1366.381638	52.126203	66.721255
1365.669884	63.300952	66.726260
1365.273922	61.694743	66.731265
1364.652937	53.064755	66.736270
1363.935899	60.192967	66.741274
1363.554000	62.057872	66.746279
1362.379696	58.989056	66.751284
1361.537909	61.834617	66.756289
1361.298569	54.896583	66.761294
1360.963738	58.788597	66.766298
1360.769730	53.030511	66.771303
1359.780726	55.214858	66.776308
1358.459797	63.544950	66.781313
1358.498544	52.079261	66.786318
1357.712767	57.420115	66.791322
1356.608647	64.549464	66.796327
1355.755168	63.283668	66.801332
1354.818121	64.472721	66.806337
1354.979198	55.087965	66.811342
1354.285946	68.758117	66.816346
1353.875792	61.034623	66.821351
1352.511704	62.460983	66.826356
1351.921369	57.549127	66.831361
1351.670233	58.558002	66.836366
1351.075608	55.711257	66.841370
1350.807550	48.571706	66.846375
1349.359578	61.377939	66.851380
1348.550275	55.987277	66.856385
1348.391787	63.705896	66.861390
1347.941171	64.396436	66.866394
1346.933419	52.365852	66.871399
1346.011988	58.064650	66.876404
1345.310265	62.309590	66.881409
1345.143303	60.400114	66.886414
1344.097637	67.069480	66.891418
1343.374969	56.038463	66.896423
1342.491539	59.619410	66.901428
1341.896026	62.298873	66.906433
1341.690396	53.645152	66.911438
1340.704763	59.450464	66.916442
1340.722039	66.997292	66.921447
1340.470706	60.582734	66.926452
1339.277266	67.205165	66.931457
1338.630823	57.530377	66.936462
1337.328208	59.280543	66.941466
1336.596716	58.999216	66.946471
1336.115901	57.058209	66.951476
1335.285237	57.071346	66.956481
1335.416182	53.658705	66.961486
1334.911612	64.235909	66.966490
1333.804528	54.702346	66.971495
1333.151761	56.288374	66.976500
1332.568536	64.459422	66.981505
1331.828475	50.664414	66.986510
1330.716178	64.711415	66.991514
1329.899587	58.869262	66.996519
1329.539441	65.581531	67.001524
1329.000440	68.646435	67.006529
1328.695623	57.084832	67.011534
1328.101427	64.593447	67.016538
1327.369074	56.533163	67.021543
1326.425096	57.372503	67.026548
1325.932005	65.076169	67.031553
1325.297585	56.917413	67.036558
1323.903273	59.138389	67.041562
1323.753413	70.356683	67.046567
1323.245063	60.023550	67.051572
1322.676471	63.094703	67.056577
1321.792875	52.878312	67.061582
1320.640928	64.424853	67.066586
1320.205955	62.271931	67.071591
1319.873930	57.103896	67.076596
1319.328075	63.859403	67.081601
1318.997685	53.595279	67.086606
1317.548221	64.644490	67.091610
1317.294285	61.255502	67.096615
1316.828272	61.409495	67.101620
1315.725680	59.697692	67.106625
1314.734051	64.373563	67.111630
1314.115923	65.614601	67.116634
1313.376398	57.938423	67.121639
1313.466559	58.957948	67.126644
1312.919788	60.394785	67.131649
1312.532413	59.886795	67.136654
1311.084897	62.013468	67.141658
1310.871960	58.999154	67.146663
1310.332456	63.614992	67.151668
1308.894793	58.118762	67.156673
1308.510238	53.553773	67.161678
1307.872369	61.825354	67.166682
1307.475487	55.067449	67.171687
1306.860731	61.986323	67.176692
1305.765400	59.933427	67.181697
1304.733537	51.472473	67.186702
1304.308867	60.307131	67.191706
1303.742186	55.326896	67.196711
1303.508966	57.323842	67.201716
1302.805755	60.077401	67.206721
1301.942066	50.621388	67.211726
1301.140026	60.822036	67.216730
1300.643839	60.008611	67.221735
1300.124433	62.957272	67.226740
1299.465227	59.033353	67.231745
1298.590779	56.263335	67.236750
1297.315402	63.641079	67.241754
1297.214667	60.797417	67.246759
1296.542733	60.200782	67.251764
1296.197570	67.422436	67.256769
1295.709525	56.067857	67.261774
1295.072021	66.414016	67.266778
1294.446622	63.990159	67.271783
1293.861301	61.566545	67.276788
1292.217768	70.313837	67.281793
1291.664316	59.463852	67.286798
1290.900064	66.644758	67.291802
1290.597977	66.129274	67.296807
1290.220627	63.289943	67.301812
1289.720557	70.401151	67.306817
1288.859115	56.324577	67.311822
1288.022050	64.062263	67.316826
1287.632732	53.350755	67.321831
1286.985850	55.263790	67.326836
1285.978933	60.389892	67.331841
1285.182159	62.354641	67.336846
1284.381652	69.032569	67.341850
1284.112540	59.629099	67.346855
1283.932400	59.380487	67.351860
1283.048825	66.034348	67.356865
1282.005650	67.085669	67.361870
1281.263989	65.769561	67.366874
1281.230775	65.574739	67.371879
1280.838843	59.007426	67.376884
1279.064092	76.429408	67.381889
1278.356500	66.804569	67.386894
1277.687096	66.392231	67.391898
1277.401432	72.121929	67.396903
1277.091907	66.292839	67.401908
1276.567605	69.603114	67.406913
1276.078550	66.897376	67.411918
1274.828762	70.121075	67.416922
1274.180250	64.267130	67.421927
1274.108325	61.428404	67.426932
1272.611402	62.269266	67.431937
1271.846793	65.756069	67.436942
1271.201243	66.763001	67.441946
1270.796507	66.885194	67.446951
1270.504632	66.293361	67.451956
1270.010862	67.408512	67.456961
1268.956220	64.329891	67.461966
1268.059770	70.922410	67.466970
1267.840203	63.069200	67.471975
1267.507668	61.824360	67.476980
1266.063093	69.087007	67.481985
1265.580235	63.164442	67.486990
1264.786798	72.991013	67.491994
1264.509128	65.992447	67.496999
1263.956287	65.414899	67.502004
1262.888549	64.529601	67.507009
1262.485850	58.368326	67.512014
1261.798920	63.346100	67.517018
1261.557725	64.522217	67.522023
1260.173534	64.526715	67.527028
1259.518092	63.525439	67.532033
1259.212780	55.757174	67.537038
1258.735630	57.061313	67.542042
1257.691610	60.449908	67.547047
1256.658356	62.455937	67.552052
1255.916341	67.135659	67.557057
1255.532875	61.735265	67.562062
1254.983545	62.090625	67.567066
1254.719654	63.916780	67.572071
1253.888388	60.604535	67.577076
1252.747352	60.941204	67.582081
1252.407091	57.068473	67.587086
1251.695575	54.759231	67.592090
1251.378280	60.811298	67.597095
1250.922420	54.143232	67.602100
1249.616397	56.278852	67.607105
1248.976985	61.411510	67.612110
1248.326375	56.357630	67.617114
1247.970689	54.054176	67.622119
1247.209566	58.886371	67.627124
1246.048271	61.737704	67.632129
1245.525187	59.928676	67.637134
1245.087103	65.101074	67.642138
1244.716517	61.269453	67.647143
1244.454908	57.805210	67.652148
1243.258188	63.813642	67.657153
1242.524630	53.260942	67.662158
1241.940310	58.808095	67.667162
1241.345884	66.403591	67.672167
1240.581771	60.144730	67.677172
1239.473092	66.258873	67.682177
1238.859840	65.699171	67.687182
1238.175080	64.460165	67.692186
1237.919047	63.851540	67.697191
1237.861705	60.691387	67.702196
1236.735215	70.431302	67.707201
1235.753599	63.366166	67.712206
1235.045356	58.452413	67.717210
1234.735046	58.843822	67.722215
1234.348711	58.102383	67.727220
1233.283800	67.509663	67.732225
1232.513751	61.990336	67.737230
1232.194913	63.778139	67.742234
1231.327785	66.694764	67.747239
1230.425037	67.464303	67.752244
1229.870558	68.014354	67.757249
1229.544926	64.982630	67.762254
1229.110258	66.770529	67.767258
1227.971504	64.854158	67.772263
1227.313971	60.524984	67.777268
1226.587524	65.100600	67.782273
1226.066955	66.823078	67.787278
1225.736994	69.877067	67.792282
1224.746833	65.850751	67.797287
1223.941122	60.917373	67.802292
1222.972719	72.118310	67.807297
1223.240001	56.607119	67.812302
1221.863644	66.772689	67.817306
1220.731281	66.248580	67.822311
1220.441874	67.459793	67.827316
1219.777723	65.983589	67.832321
1219.878758	62.066882	67.837326
1219.382305	65.942364	67.842330
1218.430126	61.467859	67.847335
1217.507504	64.669105	67.852340
1216.802160	63.494019	67.857345
1216.379254	56.658481	67.862350
1215.136028	58.784542	67.867354
1214.169226	64.122066	67.872359
1213.967758	57.731749	67.877364
1213.365893	64.640921	67.882369
1212.876559	59.652588	67.887374
1212.679185	66.051607	67.892378
1211.158785	67.086366	67.897383
1210.501465	65.429397	67.902388
1209.983388	64.978923	67.907393
1210.161717	55.371760	67.912398
1209.110300	71.437989	67.917402
1207.996729	65.781307	67.922407
1207.752928	61.136575	67.927412
1207.029456	66.321523	67.932417
1206.347824	59.758429	67.937422
1204.938100	62.580467	67.942426
1204.436282	67.028026	67.947431
1204.153827	63.954572	67.952436
1203.380832	73.768963	67.957441
1203.157908	62.576628	67.962446
1203.202452	64.338135	67.967450
1201.697625	59.555249	67.972455
1201.281566	61.587450	67.977460
1199.870591	67.775857	67.982465
1199.295821	52.810274	67.987470
1198.569248	67.178462	67.992474
1198.021342	73.436589	67.997479
1197.778846	65.746385	68.002484
1197.138644	64.630803	68.007489
1197.107074	58.401257	68.012494
1195.898448	62.158687	68.017498
1195.060098	60.232336	68.022503
1194.736407	61.974789	68.027508
1193.123859	60.556766	68.032513
1192.974432	57.587637	68.037518
1191.836752	66.400306	68.042522
1191.583621	70.926465	68.047527
1191.327743	59.057310	68.052532
1191.018501	63.021917	68.057537
1190.091449	56.093501	68.062542
1188.827933	66.741837	68.067546
1188.393644	65.682574	68.072551
1187.501917	60.960500	68.077556
1186.863778	61.974068	68.082561
1186.352660	61.560693	68.087566
1185.731084	60.139175	68.092570
1185.386615	63.318011	68.097575
1184.522992	54.289497	68.102580
1183.319317	67.601404	68.107585
1183.008357	56.655850	68.112590
1182.743769	56.229079	68.117594
1181.835059	57.568434	68.122599
1181.204605	59.867860	68.127604
1180.297620	58.122203	68.132609
1179.827411	43.439111	68.137614
1179.293954	55.096857	68.142618
1178.993332	55.988296	68.147623
1177.556705	59.102302	68.152628
1176.394089	53.563762	68.157633
1175.951327	53.779705	68.162638
1175.547180	59.336273	68.167642
1175.192680	64.842503	68.172647
1175.000909	52.090449	68.177652
1173.739964	53.438802	68.182657
1173.286847	55.166707	68.187662
1172.704810	58.918692	68.192666
1172.128423	65.883897	68.197671
1170.936551	56.095312	68.202676
1170.022130	56.424381	68.207681
1169.686043	54.485060	68.212686
1169.262899	58.535482	68.217690
1168.775929	51.758289	68.222695
1168.589019	48.902155	68.227700
1166.916717	60.302554	68.232705
1166.400982	56.370276	68.237710
1165.864759	67.966140	68.242714
1165.265524	69.760116	68.247719
1164.768107	63.874795	68.252724
1163.844185	65.950933	68.257729
1163.037272	59.379696	68.262734
1162.390182	62.478513	68.267738
1162.106150	60.724875	68.272743
1161.478685	52.996392	68.277748
1160.406919	64.164896	68.282753
1159.594021	54.069860	68.287758
1159.333270	65.171339	68.292762
1158.564341	65.243405	68.297767
1158.906109	51.358735	68.302772
1157.306066	65.010865	68.307777
1156.621736	53.670981	68.312782
1156.319183	54.159746	68.317786
1155.480583	49.262806	68.322791
1154.408826	61.276397	68.327796
1153.386841	64.385724	68.332801
1153.378566	60.313666	68.337806
1152.678820	55.589123	68.342810
1152.645497	57.026082	68.347815
1151.556332	54.252599	68.352820
1150.352975	62.131563	68.357825
1149.917976	55.114958	68.362830
1149.405040	58.904453	68.367834
1149.042117	60.848221	68.372839
1148.204364	54.436210	68.377844
1147.000385	62.083188	68.382849
1146.736702	54.561615	68.387854
1146.205761	52.597638	68.392858
1145.830173	61.086407	68.397863
1144.928694	53.886796	68.402868
1144.020776	66.000621	68.407873
1143.550267	57.276233	68.412878
1142.942028	55.012480	68.417882
1142.016909	52.299722	68.422887
1141.265324	58.321550	68.427892
1140.767210	65.402426	68.432897
1140.568590	59.497131	68.437902
1140.059814	63.471827	68.442906
1138.949448	66.579318	68.447911
1138.135988	55.106030	68.452916
1137.434940	61.471690	68.457921
1136.761376	53.237973	68.462926
1135.510457	57.246985	68.467930
1135.022349	58.296445	68.472935
1134.810899	50.524366	68.477940
1134.345783	63.244439	68.482945
1134.043992	62.392221	68.487950
1133.269746	57.545049	68.492954
1132.428106	64.024779	68.497959
1131.616307	55.882623	68.502964
1130.578105	61.473555	68.507969
1130.476402	53.730443	68.512974
1129.621279	63.975320	68.517978
1129.034076	61.099707	68.522983
1128.767706	55.150361	68.527988
1128.227555	55.294173	68.532993
1126.621668	52.054202	68.537998
1126.419249	54.671111	68.543002
1125.707372	58.652953	68.548007
1125.139971	55.490544	68.553012
1123.555142	58.224960	68.558017
1123.080811	60.329509	68.563022
1122.684240	54.261940	68.568026
1122.291156	55.845759	68.573031
1122.196491	53.727348	68.578036
1121.364155	55.858463	68.583041
1119.934807	55.040248	68.588046
1119.199693	57.762976	68.593050
1118.435695	57.792758	68.598055
1118.224195	53.430255	68.603060
1117.643316	66.573949	68.608065
1117.586019	56.556371	68.613070
1116.412618	59.722025	68.618074
1115.228588	58.736679	68.623079
1115.385415	53.971650	68.628084
1114.591237	56.156229	68.633089
1114.054113	55.162739	68.638094
1112.948943	52.209253	68.643098
1111.869738	61.180066	68.648103
1111.637990	57.488890	68.653108
1110.941683	57.913247	68.658113
1110.914835	55.875981	68.663118
1109.666019	54.833050	68.668122
1108.586086	55.184156	68.673127
1108.511228	49.739625	68.678132
1107.896260	57.768092	68.683137
1107.377632	60.972805	68.688142
1106.926720	59.812192	68.693146
1105.663153	59.886074	68.698151
1104.813722	51.610247	68.703156
1104.607894	55.802265	68.708161
1104.192567	50.655234	68.713166
1103.053543	60.771496	68.718170
1102.154940	65.735796	68.723175
1101.831852	57.989544	68.728180
1101.767326	63.849126	68.733185
1100.708068	64.090119	68.738190
1099.657669	61.232250	68.743194
1098.652550	65.442724	68.748199
1098.498265	51.177630	68.753204
1097.612260	65.129453	68.758209
1097.352883	55.828159	68.763214
1097.075770	54.019660	68.768218
1095.959554	55.955060	68.773223
1095.530772	45.319428	68.778228
1094.809397	46.511461	68.783233
1093.964377	53.627263	68.788238
1093.105954	52.170136	68.793242
1092.358086	59.231806	68.798247
1092.073294	53.036948	68.803252
1091.480590	64.723396	68.808257
1090.456339	58.305440	68.813262
1089.490821	59.881106	68.818266
1089.145940	56.344299	68.823271
1089.123131	63.744422	68.828276
1088.217394	64.312007	68.833281
1087.327726	61.811467	68.838286
1086.624450	61.898353	68.843290
1086.041249	63.805243	68.848295
1085.689596	66.308767	68.853300
1084.294869	67.246257	68.858305
1083.430329	67.190635	68.863310
1083.366029	66.713389	68.868314
1082.671855	66.446629	68.873319
1082.363564	60.466966	68.878324
1081.649408	63.289921	68.883329
1080.430624	57.254605	68.888334
1080.081661	55.617876	68.893338
1079.585815	64.187631	68.898343
1079.008568	63.674676	68.903348
1077.751000	67.403409	68.908353
1077.177843	56.592769	68.913358
1076.913873	63.682889	68.918362
1076.401506	63.699587	68.923367
1076.020834	53.397145	68.928372
1074.655436	66.286778	68.933377
1073.925150	53.551171	68.938382
1073.839115	57.892405	68.943386
1072.336214	54.521140	68.948391
1071.703154	50.225304	68.953396
1070.859265	51.319115	68.958401
1070.818220	59.684678	68.963406
1070.437671	56.425941	68.968410
1069.872363	51.362620	68.973415
1069.342848	44.400111	68.978420
1068.109344	54.026921	68.983425
1067.241646	48.319103	68.988430
1067.046559	52.171009	68.993434
1066.348921	62.484442	68.998439
1065.652124	60.289546	69.003444
1064.613838	54.735669	69.008449
1063.982931	55.598415	69.013454
1063.578224	50.736925	69.018458
1063.152779	62.796156	69.023463
1061.979925	59.947819	69.028468
1060.932961	65.359483	69.033473
1060.698132	54.110799	69.038478
1060.312142	64.969257	69.043482
1059.622581	61.110180	69.048487
1059.341710	53.886022	69.053492
1058.040158	59.209840	69.058497
1057.691339	52.304803	69.063502
1057.146323	58.732164	69.068506
1056.210942	57.530973	69.073511
1055.286167	47.114882	69.078516
1054.705257	63.186190	69.083521
1053.835236	57.672971	69.088526
1053.979137	57.913192	69.093530
1053.400770	68.323436	69.098535
1053.010647	63.031967	69.103540
1051.819951	67.338566	69.108545
1051.168048	64.513910	69.113550
1049.963883	53.357806	69.118554
1048.995192	61.195811	69.123559
1048.711777	60.429657	69.128564
1047.702169	59.825360	69.133569
1047.603742	59.035817	69.138574
1047.465426	58.949780	69.143578
1046.847478	64.073647	69.148583
1046.203258	55.837292	69.153588
1045.007043	61.566212	69.158593
1044.602402	60.495571	69.163598
1043.922247	68.616916	69.168602
1042.557334	63.294230	69.173607
1042.264354	62.334330	69.178612
1041.755638	64.378857	69.183617
1041.192128	58.903146	69.188622
1040.988264	57.407354	69.193626
1039.769537	55.932600	69.198631
1039.158890	57.725779	69.203636
1038.309334	61.957776	69.208641
1037.761334	52.734339	69.213646
1036.891215	60.018649	69.218650
1035.715233	63.618951	69.223655
1035.261500	48.837943	69.228660
1034.784629	54.416834	69.233665
1034.437976	57.913005	69.238670
1034.651482	54.202427	69.243674
1033.766633	56.843444	69.248679
1032.683345	49.473298	69.253684
1031.906149	57.890715	69.258689
1031.507747	62.836861	69.263694
1030.345866	51.649841	69.268698
1029.230451	55.129644	69.273703
1029.101535	57.940798	69.278708
1028.639629	54.441011	69.283713
1028.085116	52.633841	69.288718
1027.659479	57.537283	69.293722
1026.353162	65.149704	69.298727
1026.113470	50.545979	69.303732
1025.572620	59.784984	69.308737
1024.496237	53.626621	69.313742
1023.584357	57.709037	69.318746
1023.018911	60.973876	69.323751
1022.780507	51.997408	69.328756
1022.108443	58.494288	69.333761
1021.200874	52.398986	69.338766
1020.549944	54.954553	69.343770
1019.792836	63.741540	69.348775
1019.310187	49.100876	69.353780
1018.519659	62.703603	69.358785
1018.239644	54.602637	69.363790
1017.030763	55.800409	69.368794
1016.619523	59.588285	69.373799
1016.079988	47.707752	69.378804
1015.656359	61.572102	69.383809
1014.651358	63.812536	69.388814
1014.111713	57.263061	69.393818
1013.367440	60.176045	69.398823
1013.270325	56.862855	69.403828
1011.775340	60.624759	69.408833
1011.019305	61.157642	69.413838
1010.414902	59.315993	69.418842
1009.922784	63.892945	69.423847
1009.766530	51.122208	69.428852
1008.909122	63.996691	69.433857
1007.979204	53.609516	69.438862
1007.034725	53.935078	69.443866
1006.460565	58.640152	69.448871
1006.322082	46.976320	69.453876
1005.745217	61.664634	69.458881
1004.587702	57.967019	69.463886
1004.022624	51.339013	69.468890
1003.584519	57.057312	69.473895
1003.253702	53.884799	69.478900
1002.064369	52.675797	69.483905
1001.280044	57.155165	69.488910
1000.720503	56.571297	69.493914
1000.662667	59.794204	69.498919
999.424023	54.319655	69.503924
998.408193	52.085465	69.508929
997.763288	54.332913	69.513934
997.269315	58.309029	69.518938
996.715996	53.148935	69.523943
996.367126	51.577722	69.528948
995.603714	61.290610	69.533953
994.561303	51.768189	69.538958
993.916603	47.284108	69.543962
993.295450	57.137622	69.548967
992.904937	59.319401	69.553972
992.547242	58.003501	69.558977
991.901434	57.543743	69.563982
990.828149	56.177903	69.568986
990.163416	64.349893	69.573991
989.840187	54.308406	69.578996
988.992593	58.011942	69.584001
988.175829	64.293225	69.589006
987.442911	58.378797	69.594010
986.644738	55.185671	69.599015
986.440902	55.191379	69.604020
985.315570	60.498848	69.609025
984.393507	52.970848	69.614030
984.171042	54.470196	69.619034
983.531925	62.118746	69.624039
983.161688	54.548737	69.629044
982.945231	68.046049	69.634049
981.947322	62.152925	69.639054
981.295311	56.574758	69.644058
980.490586	56.504962	69.649063
979.729202	51.652070	69.654068
978.987644	51.552906	69.659073
978.535032	53.573618	69.664078
978.100935	55.084738	69.669082
976.642075	55.124208	69.674087
976.434166	63.974634	69.679092
975.915630	68.455066	69.684097
974.732149	56.802444	69.689102
974.609766	45.262959	69.694106
973.134718	67.537609	69.699111
972.562066	42.743292	69.704116
972.022315	53.939503	69.709121
971.467651	61.724372	69.714126
971.174913	55.863240	69.719130
970.772200	63.477225	69.724135
970.084453	47.284545	69.729140
969.269946	58.893323	69.734145
968.752540	56.619170	69.739150
967.991276	49.647817	69.744154
966.354548	53.911614	69.749159
965.710777	51.313728	69.754164
965.356940	54.863233	69.759169
964.765616	53.889701	69.764174
964.734737	52.760978	69.769178
964.438801	51.842641	69.774183
963.931814	53.290855	69.779188
962.811404	57.793841	69.784193
962.073038	63.913681	69.789198
961.177357	57.578737	69.794202
959.727550	63.353077	69.799207
959.346469	55.219300	69.804212
958.790718	66.802714	69.809217
958.317490	62.535966	69.814222
958.043530	48.708217	69.819226
957.659683	59.021197	69.824231
956.910562	54.897618	69.829236
955.980313	54.761698	69.834241
955.082488	53.734876	69.839246
954.948905	58.623431	69.844250
953.753305	55.476668	69.849255
953.116021	60.831997	69.854260
952.820867	52.719425	69.859265
952.202244	65.151194	69.864270
951.481197	52.180764	69.869274
949.929952	60.966007	69.874279
949.672877	48.304125	69.879284
949.664514	58.392936	69.884289
949.042527	60.399635	69.889294
947.726381	55.101393	69.894298
946.713952	59.831404	69.899303
946.483309	55.919408	69.904308
945.952053	52.912275	69.909313
945.914163	55.084581	69.914318
944.674704	58.100933	69.919322
943.828105	64.240496	69.924327
943.407362	53.695087	69.929332
943.041417	53.678037	69.934337
941.953671	54.938759	69.939342
941.114683	42.965068	69.944346
940.418678	52.180118	69.949351
939.987767	55.443631	69.954356
939.396670	50.145551	69.959361
938.949556	55.661721	69.964366
938.275140	52.547273	69.969370
937.500135	57.413848	69.974375
936.710946	60.912004	69.979380
936.271906	49.856206	69.984385
935.179237	60.249140	69.989390
934.381300	54.555850	69.994394
933.351036	51.402091	69.999399
933.475350	56.096088	70.004404
932.817565	60.016979	70.009409
932.398318	62.298019	70.014414
931.971651	53.685765	70.019418
930.493155	58.684275	70.024423
930.159847	55.788496	70.029428
929.547137	59.941654	70.034433
928.981434	53.977287	70.039438
928.364107	54.263016	70.044442
927.032646	63.384814	70.049447
926.537843	46.772676	70.054452
926.178341	48.394964	70.059457
925.783940	48.476337	70.064462
925.112279	50.762715	70.069466
924.320824	57.936462	70.074471
923.945664	48.031773	70.079476
923.108678	51.506932	70.084481
921.988564	55.464377	70.089486
921.873323	50.630298	70.094490
920.988080	56.236112	70.099495
920.206511	59.406534	70.104500
919.375560	52.477126	70.109505
918.729777	56.966721	70.114510
918.376816	55.384768	70.119514
917.407568	53.943497	70.124519
916.449378	57.491915	70.129524
915.767050	58.524530	70.134529
915.183867	59.468720	70.139534
915.015501	53.026982	70.144538
914.206160	66.117830	70.149543
913.685853	56.084848	70.154548
913.404233	52.439336	70.159553
912.331366	65.317569	70.164558
911.406889	66.605595	70.169562
910.825417	62.564619	70.174567
910.627814	51.405109	70.179572
909.814040	60.697176	70.184577
908.705029	64.699695	70.189582
908.393361	52.098086	70.194586
907.431443	71.589344	70.199591
907.342029	60.078552	70.204596
906.504591	59.043370	70.209601
905.546979	60.757050	70.214606
905.020821	51.577266	70.219610
904.361500	58.948636	70.224615
904.143964	46.932852	70.229620
902.988140	52.531724	70.234625
902.596625	61.760548	70.239630
902.372357	53.507954	70.244634
900.771037	52.678209	70.249639
900.152998	55.477221	70.254644
899.692447	60.571375	70.259649
898.671647	59.397478	70.264654
898.845687	49.241235	70.269658
897.832713	57.547078	70.274663
896.200266	59.913157	70.279668
896.122845	57.847061	70.284673
895.486347	58.054372	70.289678
895.374725	54.684860	70.294682
894.732587	61.187281	70.299687
894.043169	57.874893	70.304692
892.611474	59.643724	70.309697
892.510890	57.904868	70.314702
891.878242	50.525865	70.319706
891.595524	59.945252	70.324711
890.708195	53.966905	70.329716
889.766259	61.110775	70.334721
889.241162	62.952472	70.339726
888.532809	51.016018	70.344730
887.645409	60.218070	70.349735
886.768830	52.871770	70.354740
886.105436	58.063426	70.359745
885.591699	58.081168	70.364750
885.598859	47.549321	70.369754
885.209773	56.695624	70.374759
884.227173	59.337618	70.379764
883.147979	54.056442	70.384769
882.798349	61.538183	70.389774
882.255375	53.794893	70.394778
880.964605	64.877784	70.399783
880.376105	61.253259	70.404788
879.867592	59.577958	70.409793
879.338510	59.290450	70.414798
878.859628	54.010658	70.419802
877.540546	56.680287	70.424807
877.305695	49.702471	70.429812
876.613347	55.840879	70.434817
875.903648	55.677855	70.439822
875.505298	44.527478	70.444826
874.772498	56.676838	70.449831
874.098350	54.972675	70.454836
873.366367	55.109900	70.459841
872.656923	57.073958	70.464846
871.790920	40.977371	70.469850
870.567679	60.836252	70.474855
870.395492	51.877674	70.479860
869.732334	56.321699	70.484865
869.656289	56.936675	70.489870
869.543747	53.055376	70.494874
868.160525	56.680154	70.499879
867.187056	50.055024	70.504884
867.002634	60.768425	70.509889
865.881544	58.525454	70.514894
864.876722	43.654950	70.519898
864.217119	53.364663	70.524903
863.937228	50.196862	70.529908
863.355795	47.296225	70.534913
862.675040	55.346231	70.539918
862.731943	49.840468	70.544922
861.869625	55.995755	70.549927
860.827481	54.092929	70.554932
860.336988	55.213475	70.559937
859.558488	52.202916	70.564942
858.434198	49.891026	70.569946
857.503028	62.626182	70.574951
856.777639	47.644659	70.579956
856.964618	51.782419	70.584961
856.521169	61.550240	70.589966
856.351868	50.815342	70.594970
854.891266	55.153998	70.599975
854.521066	56.787202	70.604980
853.570258	58.751160	70.609985
852.413178	55.722162	70.614990
851.887208	58.325813	70.619994
850.935799	57.842635	70.624999
850.556878	55.721610	70.630004
850.538980	51.372152	70.635009
849.910171	50.635570	70.640014
849.361609	52.718513	70.645018
847.899761	54.847370	70.650023
847.450341	55.025800	70.655028
847.059494	51.594784	70.660033
846.169465	57.365234	70.665038
845.403480	47.394484	70.670042
844.799680	61.498094	70.675047
844.103587	57.487421	70.680052
843.949393	58.965212	70.685057
843.119528	62.998477	70.690062
842.312017	61.169537	70.695066
841.423625	54.759170	70.700071
841.114963	56.534194	70.705076
840.767396	51.918722	70.710081
839.653549	58.261956	70.715086
839.164927	51.809165	70.720090
838.238221	56.161764	70.725095
837.511032	60.682678	70.730100
836.788126	55.419824	70.735105
835.797175	59.048863	70.740110
835.166300	51.140649	70.745114
834.764493	59.447992	70.750119
834.631565	59.855223	70.755124
834.562904	50.914442	70.760129
833.259087	59.994416	70.765134
832.348961	58.020038	70.770138
831.732822	65.217843	70.775143
831.038674	52.141793	70.780148
830.317509	58.038839	70.785153
829.042661	62.136486	70.790158
828.797676	46.875720	70.795162
828.075874	58.177323	70.800167
827.929784	47.719494	70.805172
827.571337	48.606646	70.810177
826.670914	54.099025	70.815182
826.114430	55.581386	70.820186
825.483588	52.503701	70.825191
824.175808	52.562730	70.830196
823.605129	51.346088	70.835201
822.840461	57.067438	70.840206
822.525267	50.121547	70.845210
822.186834	57.388221	70.850215
821.440729	54.866304	70.855220
820.413855	45.066559	70.860225
819.374317	48.672738	70.865230
819.120043	38.657767	70.870234
818.649793	58.679754	70.875239
818.186234	55.613676	70.880244
817.540067	57.373492	70.885249
816.573294	54.458345	70.890254
816.058840	47.175951	70.895258
814.445608	52.449790	70.900263
814.002158	48.297960	70.905268
813.708377	45.215039	70.910273
813.159053	50.633462	70.915278
812.804406	43.714069	70.920282
812.254173	51.639487	70.925287
811.239834	53.983393	70.930292
810.519451	56.886387	70.935297
809.899194	61.425302	70.940302
809.883689	57.881839	70.945306
808.348171	58.523801	70.950311
807.370501	52.163471	70.955316
806.769250	52.540403	70.960321
806.704942	58.902799	70.965326
806.063252	46.219202	70.970330
805.633493	55.786526	70.975335
805.005024	54.853718	70.980340
804.031505	56.309628	70.985345
803.208567	56.402053	70.990350
802.886211	48.695591	70.995354
801.731058	54.026355	71.000359
800.882428	47.608794	71.005364
800.138558	48.512236	71.010369
799.650670	53.098339	71.015374
799.501213	49.468883	71.020378
799.301992	52.860468	71.025383
798.548965	48.179464	71.030388
797.432966	47.402008	71.035393
796.788652	52.822100	71.040398
795.893904	52.685655	71.045402
794.684539	61.951551	71.050407
794.076036	52.545119	71.055412
793.679350	42.291270	71.060417
793.314025	53.784424	71.065422
793.272428	52.208748	71.070426
792.867537	51.412503	71.075431
791.850511	53.006913	71.080436
791.064864	52.268785	71.085441
790.064157	48.939481	71.090446
788.956260	46.906234	71.095450
788.399470	53.937562	71.100455
787.639725	48.163164	71.105460
787.247843	51.727086	71.110465
786.911996	56.060580	71.115470
786.593813	49.959898	71.120474
786.215274	56.719126	71.125479
785.077675	54.115471	71.130484
784.616631	56.138826	71.135489
783.014977	57.252364	71.140494
782.236628	49.375346	71.145498
781.706190	50.053555	71.150503
781.156696	49.683112	71.155508
780.805719	53.550275	71.160513
780.130223	62.065941	71.165518
779.762838	49.532717	71.170522
778.959202	50.794145	71.175527
778.300200	44.545412	71.180532
777.799490	45.965726	71.185537
776.890987	55.714922	71.190542
776.744315	50.145753	71.195546
775.438047	58.911962	71.200551
775.006150	49.790266	71.205556
774.229607	43.574301	71.210561
773.856307	48.869025	71.215566
772.892543	49.315955	71.220570
771.736665	49.280297	71.225575
771.340871	46.678251	71.230580
771.039542	46.293323	71.235585
770.507085	52.090944	71.240590
769.895399	44.094992	71.245594
768.984153	56.291105	71.250599
768.314676	51.893804	71.255604
767.731316	48.285392	71.260609
766.187383	52.656107	71.265614
765.959076	52.236566	71.270618
765.192435	53.035367	71.275623
764.557306	47.047401	71.280628
764.399918	52.905502	71.285633
764.030531	56.082698	71.290638
763.727595	44.878896	71.295642
762.975509	57.419567	71.300647
761.804610	57.480427	71.305652
761.349700	54.804828	71.310657
760.008478	53.082726	71.315662
759.382247	51.737064	71.320666
758.918161	47.049990	71.325671
758.440030	57.772644	71.330676
758.138791	46.585918	71.335681
756.573124	53.049192	71.340686
755.933563	47.067513	71.345690
755.354640	59.478264	71.350695
754.813273	53.108730	71.355700
754.656407	52.800892	71.360705
753.895621	53.649215	71.365710
754.081446	52.533897	71.370714
752.637682	51.604979	71.375719
751.750795	57.024395	71.380724
751.366606	48.568312	71.385729
749.869503	59.083834	71.390734
749.574946	48.010431	71.395738
748.804380	57.435623	71.400743
748.497743	51.960171	71.405748
748.423979	51.046813	71.410753
747.349037	56.573046	71.415758
746.674994	57.128632	71.420762
746.051919	62.170901	71.425767
745.509766	58.001646	71.430772
744.177992	59.033439	71.435777
743.335010	63.215009	71.440782
742.839965	55.878775	71.445786
742.129469	62.473833	71.450791
742.264090	59.626984	71.455796
741.969972	52.733543	71.460801
740.669086	60.564151	71.465806
740.244776	57.204796	71.470810
739.041885	58.114254	71.475815
738.332269	53.266754	71.480820
737.291583	49.442234	71.485825
736.475367	59.760200	71.490830
736.493776	40.627967	71.495834
735.896820	49.495285	71.500839
735.363717	54.741207	71.505844
735.389018	47.440963	71.510849
734.032769	57.285419	71.515854
733.289998	52.281372	71.520858
733.158744	53.643924	71.525863
731.959813	53.612493	71.530868
730.855597	47.594768	71.535873
730.146230	57.777593	71.540878
729.969094	52.107467	71.545882
729.524695	57.352010	71.550887
728.841145	52.389920	71.555892
728.430508	45.887083	71.560897
727.017095	60.882896	71.565902
726.573773	52.444839	71.570906
726.142393	50.440177	71.575911
725.699266	53.047803	71.580916
724.756931	49.002369	71.585921
723.777655	54.536294	71.590926
723.474276	50.383373	71.595930
723.133092	53.333120	71.600935
722.536364	45.518948	71.605940
721.965747	55.396964	71.610945
721.110658	50.257828	71.615950
719.987401	48.104078	71.620954
719.028001	51.386300	71.625959
718.484333	53.738797	71.630964
718.484937	51.049507	71.635969
717.480097	56.853851	71.640974
716.538083	49.975097	71.645978
715.805720	54.319287	71.650983
715.331962	56.418636	71.655988
715.247185	54.120926	71.660993
714.371012	53.878688	71.665998
713.691459	56.699309	71.671002
712.589619	57.063332	71.676007
711.844225	53.275462	71.681012
711.778117	49.629364	71.686017
710.734512	57.218937	71.691022
710.071440	45.701467	71.696026
709.309915	54.229897	71.701031
709.083954	54.627017	71.706036
708.485414	48.101507	71.711041
707.327811	59.434354	71.716046
706.647049	49.654292	71.721050
705.792996	50.776744	71.726055
705.528844	53.809211	71.731060
705.531920	46.732239	71.736065
704.304891	55.142666	71.741070
703.590411	52.326026	71.746074
703.267643	57.180674	71.751079
702.344713	62.185111	71.756084
701.192224	53.446205	71.761089
700.508937	61.036418	71.766094
699.995563	50.296941	71.771098
699.596700	58.457339	71.776103
698.410328	59.839214	71.781108
698.295110	53.828501	71.786113
697.724060	58.931726	71.791118
697.574412	52.024198	71.796122
696.372347	46.732155	71.801127
695.481361	57.177398	71.806132
695.377723	57.663689	71.811137
694.075931	58.778775	71.816142
693.401317	49.249097	71.821146
692.794758	56.319743	71.826151
692.376511	54.882014	71.831156
691.921746	53.864203	71.836161
691.162741	56.278856	71.841166
690.411978	47.577707	71.846170
689.526741	52.492795	71.851175
688.896497	49.645150	71.856180
688.723943	50.442441	71.861185
687.657207	57.425356	71.866190
687.115226	51.014889	71.871194
686.585501	50.077023	71.876199
685.908093	54.952955	71.881204
685.054169	49.197083	71.886209
683.675839	53.200389	71.891214
683.490842	54.447419	71.896218
683.135702	54.381172	71.901223
682.674501	46.428926	71.906228
682.539565	51.898725	71.911233
681.113167	54.559157	71.916238
680.123135	52.877960	71.921242
679.350295	45.380531	71.926247
679.051662	49.987897	71.931252
678.869111	50.271404	71.936257
677.590032	59.201120	71.941262
676.718920	45.784012	71.946266
676.266780	48.809608	71.951271
675.734901	48.127493	71.956276
675.442143	44.486678	71.961281
674.713654	56.803846	71.966286
673.785864	51.146284	71.971290
673.238943	53.973789	71.976295
672.376460	53.320684	71.981300
672.390296	45.696770	71.986305
671.184944	61.320460	71.991310
670.288851	44.564791	71.996314
669.956790	56.032901	72.001319
669.187191	55.025612	72.006324
669.114166	44.521345	72.011329
667.706902	50.428979	72.016334
667.262406	44.398111	72.021338
666.673393	60.468808	72.026343
665.609024	53.053297	72.031348
665.170420	52.814256	72.036353
664.195194	62.595817	72.041358
663.709321	53.837447	72.046362
663.498480	49.983267	72.051367
662.996374	56.177909	72.056372
662.354488	45.951882	72.061377
661.102876	57.494249	72.066382
660.492455	47.834773	72.071386
660.201961	51.170947	72.076391
659.075862	46.191146	72.081396
658.076264	47.695759	72.086401
657.275596	53.168699	72.091406
657.079715	50.692275	72.096410
656.788089	55.592110	72.101415
656.363334	54.578240	72.106420
656.282795	45.821086	72.111425
654.839467	53.072196	72.116430
654.554803	50.803998	72.121434
653.677240	54.006688	72.126439
652.609281	56.248501	72.131444
651.791649	48.959266	72.136449
651.121598	53.337784	72.141454
650.998579	57.346675	72.146458
650.132676	42.508106	72.151463
648.969484	41.982706	72.156468
648.436048	41.051796	72.161473
647.897706	52.299073	72.166478
647.786338	44.766082	72.171482
647.353996	49.412934	72.176487
646.134949	49.952177	72.181492
645.660313	41.203339	72.186497
644.890807	46.566341	72.191502
643.934175	42.809941	72.196506
642.959419	46.911470	72.201511
642.203474	43.558821	72.206516
642.305563	41.506584	72.211521
641.346276	48.144269	72.216526
641.410402	38.024252	72.221530
640.621785	45.846443	72.226535
638.868118	46.644642	72.231540
638.676630	36.418430	72.236545
637.916479	44.611511	72.241550
637.754789	36.898473	72.246554
637.021521	39.889740	72.251559
635.984756	47.180926	72.256564
635.139796	34.157628	72.261569
634.715846	43.495408	72.266574
634.212982	36.573809	72.271578
634.097664	45.568596	72.276583
633.106441	53.724698	72.281588
632.303698	42.419065	72.286593
631.327366	45.628021	72.291598
631.386204	41.668039	72.296602
630.446973	46.939339	72.301607
629.200386	41.322202	72.306612
628.693567	45.882741	72.311617
627.910388	51.578465	72.316622
628.045438	42.006001	72.321626
627.359188	43.497983	72.326631
626.209525	46.729927	72.331636
625.561391	38.621050	72.336641
625.055100	50.273732	72.341646
624.502913	44.429865	72.346650
623.693817	48.596168	72.351655
622.463302	38.227073	72.356660
621.897836	36.523672	72.361665
621.410437	50.749025	72.366670
621.311762	37.672465	72.371674
620.382392	41.986471	72.376679
619.631734	46.602604	72.381684
619.332822	37.239094	72.386689
618.863539	40.902330	72.391694
618.078771	34.847279	72.396698
617.264139	47.847452	72.401703
616.256490	52.101851	72.406708
615.662277	40.542613	72.411713
614.646082	46.509168	72.416718
613.643505	45.513782	72.421722
613.572964	50.007862	72.426727
613.018998	53.503647	72.431732
612.927223	47.500375	72.436737
611.894285	46.391777	72.441742
611.089830	39.434228	72.446746
610.456465	40.051936	72.451751
609.397491	43.699768	72.456756
609.483603	43.324254	72.461761
608.622335	55.202355	72.466766
607.871624	50.974126	72.471770
606.852288	51.722304	72.476775
606.249484	48.084489	72.481780
606.517932	41.927531	72.486785
605.133418	45.937045	72.491790
604.399036	43.990629	72.496794
603.719422	44.244047	72.501799
603.100425	44.507209	72.506804
602.624045	43.479692	72.511809
601.804592	44.284013	72.516814
600.899030	44.420232	72.521818
600.619648	40.870681	72.526823
599.947735	46.754962	72.531828
599.589129	48.336854	72.536833
598.157665	44.254477	72.541838
597.816542	44.180309	72.546842
597.263741	45.021833	72.551847
596.952762	45.883105	72.556852
596.260654	40.844754	72.561857
594.977685	47.004644	72.566862
594.726028	48.709519	72.571866
594.056620	46.975775	72.576871
593.144037	51.301911	72.581876
592.747363	43.407308	72.586881
591.475322	56.350078	72.591886
591.053942	48.613250	72.596890
590.478195	42.228721	72.601895
589.697421	47.428274	72.606900
589.701878	43.403009	72.611905
588.813760	53.280956	72.616910
587.555866	46.840025	72.621914
587.521510	47.305368	72.626919
587.069246	54.074465	72.631924
586.180731	36.130631	72.636929
585.280528	49.480975	72.641934
584.454416	42.418596	72.646938
583.713559	43.020385	72.651943
583.240423	44.629401	72.656948
583.104210	39.772894	72.661953
581.965134	41.700475	72.666958
581.268837	42.535011	72.671962
580.756758	44.747114	72.676967
580.466107	47.875696	72.681972
579.733346	43.627032	72.686977
578.712734	52.821142	72.691982
578.041970	44.315515	72.696986
577.383163	38.827408	72.701991
576.190418	45.961391	72.706996
575.556680	41.949562	72.712001
574.861293	51.807512	72.717006
574.702989	41.706665	72.722010
574.304477	46.060765	72.727015
573.501623	50.838207	72.732020
573.645123	39.329806	72.737025
572.203159	52.841266	72.742030
571.348334	40.928426	72.747034
570.972526	37.568286	72.752039
570.499185	45.886693	72.757044
569.442939	41.424657	72.762049
568.622644	46.146669	72.767054
568.249550	47.038716	72.772058
567.908542	46.235098	72.777063
566.808020	56.498766	72.782068
565.845289	52.422524	72.787073
565.298907	56.381988	72.792078
564.941062	44.944882	72.797082
564.451630	52.923832	72.802087
563.256486	44.141369	72.807092
563.070177	39.371206	72.812097
562.554753	44.642524	72.817102
561.678577	43.300247	72.822106
560.460200	40.826147	72.827111
559.654628	51.421356	72.832116
559.345772	39.365632	72.837121
558.461274	51.942017	72.842126
558.446312	40.945082	72.847130
558.342653	44.798686	72.852135
557.177565	48.862978	72.857140
556.476700	41.744411	72.862145
555.662610	48.563268	72.867150
554.986263	45.275939	72.872154
554.172250	45.884347	72.877159
553.217591	51.372633	72.882164
552.626560	40.136927	72.887169
552.254590	41.143249	72.892174
551.691816	44.778696	72.897178
551.557633	49.094611	72.902183
550.518448	52.534208	72.907188
549.853255	42.659553	72.912193
549.148007	54.435533	72.917198
548.458833	51.661952	72.922202
547.203293	49.402631	72.927207
546.618693	49.981993	72.932212
546.694438	40.366413	72.937217
545.883370	43.639428	72.942222
545.335929	41.103259	72.947226
544.258465	46.364706	72.952231
543.539000	51.600731	72.957236
543.215508	45.536912	72.962241
542.722302	50.005524	72.967246
541.772106	39.827229	72.972250
540.864519	52.817679	72.977255
540.381415	49.380009	72.982260
539.629988	42.176957	72.987265
539.284717	47.757391	72.992270
538.315320	47.741543	72.997274
537.497273	46.384574	73.002279
536.781399	40.920463	73.007284
536.442704	42.327245	73.012289
536.116338	36.782973	73.017294
535.984634	42.502064	73.022298
535.008268	33.634368	73.027303
533.966774	37.344739	73.032308
532.663876	36.791600	73.037313
531.488326	53.751425	73.042318
530.849095	42.402410	73.047322
531.219321	45.726812	73.052327
530.622638	49.272157	73.057332
530.098542	41.318088	73.062337
529.443148	49.165616	73.067342
528.715202	44.529316	73.072346
527.808326	44.334215	73.077351
526.844070	58.472737	73.082356
526.554044	44.161153	73.087361
526.098388	50.440201	73.092366
525.074939	43.275080	73.097370
524.308237	49.677291	73.102375
523.759435	48.985069	73.107380
523.269971	45.776242	73.112385
522.568338	50.789357	73.117390
522.484982	44.634264	73.122394
521.314224	43.028675	73.127399
520.625943	45.653454	73.132404
520.337073	41.653983	73.137409
519.567784	44.939974	73.142414
518.696817	46.469148	73.147418
518.347964	43.080711	73.152423
517.574952	41.578668	73.157428
516.365576	46.489324	73.162433
515.433607	51.479939	73.167438
514.918126	44.676172	73.172442
514.558071	47.187080	73.177447
513.941157	55.770476	73.182452
513.992608	45.355419	73.187457
512.899146	47.676624	73.192462
511.891501	44.633168	73.197466
511.634015	45.308841	73.202471
510.854215	44.498317	73.207476
509.868200	44.519663	73.212481
509.037294	50.317124	73.217486
508.542525	41.717018	73.222490
508.368921	43.005913	73.227495
507.819278	47.677212	73.232500
506.788865	42.069254	73.237505
505.786389	46.506720	73.242510
505.251282	47.637311	73.247514
504.994511	42.907646	73.252519
503.965097	50.268641	73.257524
503.126987	41.886045	73.262529
502.481421	50.572632	73.267534
501.779334	56.076063	73.272538
501.606624	54.093019	73.277543
501.010885	47.203538	73.282548
500.495155	42.448384	73.287553
499.202423	44.214825	73.292558
498.771062	49.928822	73.297562
498.830864	43.559343	73.302567
497.564444	52.056679	73.307572
496.845136	42.563921	73.312577
495.947572	43.765702	73.317582
495.356166	46.403487	73.322586
495.299881	40.367699	73.327591
494.292009	55.488638	73.332596
493.434052	45.043509	73.337601
493.038123	51.061286	73.342606
492.317237	45.273192	73.347610
491.238940	42.167642	73.352615
490.290895	46.980234	73.357620
489.778771	41.949349	73.362625
488.986478	45.760703	73.367630
488.595603	41.725035	73.372634
488.587723	38.803931	73.377639
488.241197	51.734158	73.382644
487.346702	44.337356	73.387649
486.406514	41.935204	73.392654
486.064176	42.584763	73.397658
484.969529	39.255451	73.402663
483.684565	41.147662	73.407668
483.368307	43.244116	73.412673
482.603300	49.599859	73.417678
481.995799	36.379610	73.422682
481.920587	38.953806	73.427687
481.220842	48.902498	73.432692
480.474531	39.793299	73.437697
479.743116	40.722283	73.442702
479.332871	44.386463	73.447706
478.496821	42.617351	73.452711
477.206301	47.538762	73.457716
476.646175	46.559555	73.462721
476.381293	45.993543	73.467726
475.851706	45.801293	73.472730
475.640557	38.501331	73.477735
474.562531	46.701926	73.482740
473.900259	35.088079	73.487745
473.223576	41.779585	73.492750
471.981059	44.208837	73.497754
471.328378	39.436896	73.502759
470.675597	40.280568	73.507764
470.317874	45.496447	73.512769
469.997155	52.621140	73.517774
469.477730	47.983853	73.522778
468.740521	46.037156	73.527783
467.929287	51.227733	73.532788
467.130344	46.312313	73.537793
466.507342	55.375936	73.542798
465.117904	49.075212	73.547802
464.545187	46.194853	73.552807
464.035305	54.420453	73.557812
463.784622	44.091913	73.562817
463.467235	50.521732	73.567822
462.927183	51.151099	73.572826
461.948343	46.007576	73.577831
461.043454	55.686315	73.582836
460.793153	48.638572	73.587841
460.236957	52.061334	73.592846
458.964704	48.296700	73.597850
458.097463	39.977528	73.602855
457.105678	49.028165	73.607860
457.206533	45.955409	73.612865
456.703118	42.488078	73.617870
456.480333	50.444227	73.622874
455.363571	45.252898	73.627879
454.356792	47.659123	73.632884
454.102106	45.183712	73.637889
453.443075	48.688041	73.642894
452.456453	53.648954	73.647898
451.507048	48.152646	73.652903
450.560987	46.269372	73.657908
450.873398	46.049274	73.662913
450.241880	44.337479	73.667918
449.385870	49.736641	73.672922
448.454906	46.352841	73.677927
447.747295	49.471965	73.682932
447.564988	52.155299	73.687937
446.903273	52.376858	73.692942
445.673617	54.707207	73.697946
445.153834	47.349222	73.702951
444.419281	60.479757	73.707956
444.146486	49.176115	73.712961
443.961155	56.125248	73.717966
442.863461	62.787472	73.722970
442.157911	52.380969	73.727975
441.194022	56.871438	73.732980
440.941324	49.967784	73.737985
439.729551	55.452783	73.742990
438.498176	62.230675	73.747994
438.550313	50.586759	73.752999
437.685867	59.863068	73.758004
437.663947	53.331156	73.763009
437.107171	55.655137	73.768014
436.138519	58.734925	73.773018
435.513436	52.169808	73.778023
434.658299	64.704074	73.783028
434.232080	52.750578	73.788033
433.337072	52.167825	73.793038
432.314204	49.439610	73.798042
432.030400	48.581597	73.803047
431.575834	51.169492	73.808052
431.072314	48.134392	73.813057
430.259400	50.512135	73.818062
429.136217	48.238850	73.823066
428.829400	44.045502	73.828071
428.100204	50.286173	73.833076
427.880273	42.572086	73.838081
427.042323	52.884317	73.843086
425.531881	44.637487	73.848090
425.165538	44.107022	73.853095
424.522436	42.265383	73.858100
424.610509	47.291977	73.863105
424.455805	48.005300	73.868110
423.430529	47.397903	73.873114
422.567395	42.755980	73.878119
421.161393	52.607830	73.883124
420.182132	47.812922	73.888129
419.560154	47.547307	73.893134
419.297645	52.345448	73.898138
419.516051	37.619149	73.903143
418.427209	45.226376	73.908148
417.978503	41.556659	73.913153
417.154233	52.082454	73.918158
416.437157	50.307173	73.923162
416.063963	41.723749	73.928167
414.217359	48.328407	73.933172
413.818399	46.200996	73.938177
413.251529	43.706462	73.943182
412.519548	50.731118	73.948186
412.346706	40.092425	73.953191
412.141536	44.881131	73.958196
411.051802	49.896035	73.963201
410.296729	43.922382	73.968206
409.407605	50.023103	73.973210
409.532430	45.427381	73.978215
407.941222	42.912225	73.983220
407.320112	42.681198	73.988225
406.653034	38.736295	73.993230
406.231335	41.550649	73.998234
406.056675	38.490773	74.003239
405.673435	57.364178	74.008244
404.466951	43.482825	74.013249
403.509956	44.905585	74.018254
402.954759	45.483083	74.023258
402.533662	40.335566	74.028263
401.257969	48.195464	74.033268
400.435517	48.378659	74.038273
399.722516	45.991271	74.043278
399.205176	45.894426	74.048282
399.373713	48.901689	74.053287
398.477728	42.041979	74.058292
398.717751	39.473106	74.063297
397.535090	45.755574	74.068302
396.569943	51.078714	74.073306
396.193762	50.937547	74.078311
394.651207	47.286754	74.083316
394.219985	42.581473	74.088321
393.727611	44.330767	74.093326
393.419126	43.562246	74.098330
392.763128	36.073681	74.103335
391.461966	41.536902	74.108340
390.972044	40.387000	74.113345
390.477152	41.149941	74.118350
390.195602	49.982950	74.123354
389.998467	35.412341	74.128359
388.446202	46.395248	74.133364
388.050917	42.320482	74.138369
387.343030	37.878527	74.143374
385.755896	45.708518	74.148378
385.086820	42.830476	74.153383
384.538285	46.403895	74.158388
384.802382	39.753899	74.163393
383.854425	40.647776	74.168398
383.354019	50.757693	74.173402
383.193257	46.578790	74.178407
381.903810	48.203785	74.183412
380.871434	36.579975	74.188417
380.737383	33.827729	74.193422
380.369131	45.480427	74.198426
379.161312	38.061966	74.203431
378.544098	41.874115	74.208436
378.219989	38.816565	74.213441
377.704163	42.620417	74.218446
376.314347	47.430586	74.223450
375.605217	47.513052	74.228455
374.802853	53.073941	74.233460
374.443982	40.741841	74.238465
374.002307	50.184890	74.243470
373.475557	48.249899	74.248474
373.396122	42.844499	74.253479
371.897968	45.734799	74.258484
371.693548	42.717127	74.263489
370.507364	36.474761	74.268494
369.336255	35.492131	74.273498
369.016985	39.572540	74.278503
368.464234	39.820431	74.283508
367.871425	42.342028	74.288513
367.236915	33.096865	74.293518
367.282668	46.347062	74.298522
366.797112	45.262725	74.303527
365.476956	45.611748	74.308532
365.138414	42.630089	74.313537
363.800396	40.048268	74.318542
362.923170	39.228812	74.323546
362.535593	39.452737	74.328551
361.820070	43.688686	74.333556
361.254388	40.451107	74.338561
361.064944	40.279517	74.343566
360.335916	44.442786	74.348570
359.733834	41.476692	74.353575
358.806268	47.628610	74.358580
358.116354	39.567215	74.363585
357.817266	46.001000	74.368590
356.536625	48.368528	74.373594
355.986055	35.420382	74.378599
355.215778	46.264930	74.383604
354.879366	42.172578	74.388609
354.589008	41.968156	74.393614
353.319103	48.164538	74.398618
352.798687	51.652225	74.403623
351.997797	44.546110	74.408628
351.954375	45.577842	74.413633
350.992954	51.411505	74.418638
349.635715	45.537123	74.423642
349.420279	37.906748	74.428647
348.528423	41.550457	74.433652
348.684217	48.703996	74.438657
348.088358	42.307567	74.443662
346.688861	45.289511	74.448666
346.274655	34.882451	74.453671
345.523412	41.664108	74.458676
345.336721	40.717620	74.463681
344.481598	41.212721	74.468686
343.080986	42.719813	74.473690
342.892825	39.029135	74.478695
342.333964	48.337539	74.483700
341.956398	43.411897	74.488705
340.620778	38.588885	74.493710
340.001818	44.929081	74.498714
339.961467	38.262587	74.503719
338.966304	41.239965	74.508724
338.167399	35.235162	74.513729
337.536151	46.887543	74.518734
336.582018	42.601085	74.523738
336.353611	41.007706	74.528743
335.882710	49.303595	74.533748
335.317445	50.856189	74.538753
334.472346	45.224016	74.543758
333.757823	45.068217	74.548762
333.490296	37.123107	74.553767
331.804841	48.154511	74.558772
331.241989	56.343012	74.563777
330.725073	50.935625	74.568782
330.006470	52.653047	74.573786
329.761003	48.037113	74.578791
329.151955	45.835593	74.583796
328.577430	45.085438	74.588801
327.779702	39.937752	74.593806
327.155739	44.780870	74.598810
326.603699	37.251214	74.603815
325.698024	45.961467	74.608820
325.614020	42.700542	74.613825
324.571130	47.673486	74.618830
323.572721	55.382857	74.623834
323.409495	42.665939	74.628839
322.149532	53.556136	74.633844
321.163289	46.382723	74.638849
320.442668	53.142167	74.643854
319.902134	49.391101	74.648858
319.599137	39.220756	74.653863
319.318747	45.342671	74.658868
319.090711	47.553872	74.663873
318.412839	44.750371	74.668878
316.965347	39.623271	74.673882
316.713473	36.560847	74.678887
316.209810	41.944627	74.683892
315.403970	44.038954	74.688897
314.624173	52.889075	74.693902
313.877271	43.189921	74.698906
313.959785	42.914487	74.703911
312.521583	41.576622	74.708916
311.535511	49.789505	74.713921
311.073584	44.265731	74.718926
310.471175	45.583130	74.723930
310.029201	34.059457	74.728935
309.067573	37.025566	74.733940
308.179588	46.024876	74.738945
307.740345	45.293772	74.743950
307.175565	52.828562	74.748954
307.160338	46.293148	74.753959
306.153289	48.148822	74.758964
305.199552	41.598228	74.763969
304.720084	35.402506	74.768974
303.878941	48.227242	74.773978
303.610575	40.019006	74.778983
302.510203	47.732037	74.783988
301.734324	40.464158	74.788993
301.285332	42.014589	74.793998
300.815404	40.473267	74.799002
300.120635	46.374119	74.804007
298.991875	49.644784	74.809012
298.610504	43.567631	74.814017
298.362059	44.655424	74.819022
297.503922	38.513554	74.824026
296.822546	35.371206	74.829031
295.683824	47.992754	74.834036
294.931348	52.157288	74.839041
294.611447	50.661299	74.844046
294.175507	50.591564	74.849050
293.874580	44.253928	74.854055
292.913143	46.743195	74.859060
292.006751	50.225600	74.864065
291.383687	42.669441	74.869070
290.770144	44.433592	74.874074
289.817222	39.824063	74.879079
289.056236	44.888816	74.884084
288.668614	43.824017	74.889089
288.015811	48.297499	74.894094
287.457045	46.654965	74.899098
287.303549	36.255331	74.904103
286.108661	42.788583	74.909108
285.738267	35.523442	74.914113
285.052805	41.690313	74.919118
283.951149	48.158248	74.924122
283.143313	36.334548	74.929127
281.962332	40.288729	74.934132
282.133051	38.692070	74.939137
281.944213	39.817802	74.944142
281.515254	51.839304	74.949146
280.717807	42.581035	74.954151
279.281039	41.251619	74.959156
278.816302	44.286108	74.964161
278.521871	36.488110	74.969166
277.659696	48.163496	74.974170
276.879741	43.228287	74.979175
276.383097	50.984280	74.984180
275.350269	45.648362	74.989185
274.548706	43.953111	74.994190
273.647795	46.975132	74.999194
273.368513	47.517193	75.004199
272.889177	48.954413	75.009204
272.515599	41.263132	75.014209
272.380200	39.075956	75.019214
271.172474	47.409725	75.024218
270.185273	43.247365	75.029223
269.296266	47.836727	75.034228
269.089633	47.874917	75.039233
268.422509	49.293803	75.044238
267.224371	46.348186	75.049242
267.044957	38.833613	75.054247
266.011211	48.125529	75.059252
265.763347	42.789662	75.064257
265.344450	41.548263	75.069262
263.965885	54.079885	75.074266
263.177663	52.942446	75.079271
262.886826	52.410499	75.084276
262.591196	45.988674	75.089281
262.238408	54.150248	75.094286
261.029762	43.291251	75.099290
260.251905	44.274409	75.104295
259.798006	53.901911	75.109300
258.958685	52.581401	75.114305
258.040555	45.564480	75.119310
256.949029	53.943465	75.124314
256.637164	45.509018	75.129319
256.263806	51.491747	75.134324
255.707860	53.270898	75.139329
255.345713	50.612224	75.144334
254.821303	54.495316	75.149338
254.564485	50.238551	75.154343
253.521580	50.743358	75.159348
252.129200	45.853923	75.164353
251.392656	50.702136	75.169358
250.480619	50.233648	75.174362
250.012492	57.077311	75.179367
249.401369	58.121096	75.184372
249.117533	57.282047	75.189377
249.151303	53.988305	75.194382
248.592262	61.451465	75.199386
247.410238	50.658163	75.204391
246.730211	52.827246	75.209396
245.924188	59.210965	75.214401
244.828673	59.633614	75.219406
244.088653	55.362181	75.224410
243.830420	58.566134	75.229415
243.356649	56.987583	75.234420
242.942772	54.317252	75.239425
242.363378	42.770961	75.244430
241.048681	61.933087	75.249434
240.391176	48.136895	75.254439
240.317362	49.869321	75.259444
239.170695	49.261854	75.264449
238.319136	44.182226	75.269454
237.529610	55.139420	75.274458
237.268312	53.699702	75.279463
236.824931	55.019060	75.284468
236.412058	57.747840	75.289473
235.065135	42.728990	75.294478
234.431549	50.142164	75.299482
234.415681	48.438942	75.304487
233.533930	48.725088	75.309492
232.334710	55.803012	75.314497
231.987493	51.285051	75.319502
231.366039	55.888948	75.324506
231.028080	49.374520	75.329511
230.061025	47.589625	75.334516
228.925122	45.690393	75.339521
228.691704	48.054089	75.344526
227.827913	50.360062	75.349530
227.798684	47.732739	75.354535
226.730753	52.078848	75.359540
225.888445	44.300957	75.364545
225.424319	43.898580	75.369550
224.898959	55.612944	75.374554
224.439957	52.744310	75.379559
223.059707	51.156948	75.384564
222.117865	46.196609	75.389569
221.630485	43.678216	75.394574
221.080300	55.658135	75.399578
221.111320	51.391108	75.404583
220.251990	48.115865	75.409588
219.230380	52.428378	75.414593
218.885674	53.125332	75.419598
217.940148	57.469407	75.424602
217.828932	54.788642	75.429607
216.538324	59.698289	75.434612
215.807106	55.903745	75.439617
215.380364	47.488996	75.444622
214.868212	53.026600	75.449626
214.867334	47.055935	75.454631
213.714558	50.987931	75.459636
212.792426	53.123524	75.464641
212.408805	45.292665	75.469646
211.223779	52.410787	75.474650
210.361303	39.544168	75.479655
209.676641	51.359252	75.484660
209.374594	54.157451	75.489665
209.320178	52.977517	75.494670
208.276030	52.568787	75.499674
208.028805	55.529683	75.504679
206.737684	44.330786	75.509684
206.233430	53.013293	75.514689
205.560518	52.661313	75.519694
204.938968	52.422889	75.524698
204.180662	54.628289	75.529703
203.388907	50.595062	75.534708
202.869816	51.466376	75.539713
202.507704	46.355745	75.544718
201.681286	53.483839	75.549722
200.818262	56.753970	75.554727
199.957709	50.674503	75.559732
199.730682	50.630145	75.564737
199.345096	51.111095	75.569742
198.052064	59.261360	75.574746
197.560863	49.165528	75.579751
196.829485	51.025675	75.584756
196.325346	48.673173	75.589761
196.144506	45.037300	75.594766
194.983191	58.245335	75.599770
194.372086	50.415580	75.604775
193.696332	53.478356	75.609780
192.872897	53.104815	75.614785
192.529811	45.492786	75.619790
191.330176	52.022137	75.624794
190.860003	43.125790	75.629799
190.541766	55.271592	75.634804
190.003957	52.493441	75.639809
189.288357	43.964016	75.644814
187.774934	49.932589	75.649818
187.607778	49.625351	75.654823
187.178604	52.217594	75.659828
186.938545	56.070499	75.664833
185.950754	49.358809	75.669838
184.840892	59.105077	75.674842
184.372277	47.393369	75.679847
183.756655	53.038312	75.684852
183.183878	59.664273	75.689857
181.719291	50.078313	75.694862
181.039985	52.503843	75.699866
180.788271	53.025789	75.704871
180.426630	55.609219	75.709876
179.929277	56.354053	75.714881
179.635650	51.443644	75.719886
178.834001	50.707183	75.724890
177.746549	44.041396	75.729895
177.231500	47.722374	75.734900
176.306128	47.685239	75.739905
176.040009	51.124608	75.744910
174.885868	56.711485	75.749914
174.162076	44.016877	75.754919
173.764544	46.972752	75.759924
173.350711	57.634245	75.764929
173.174435	56.256531	75.769934
171.706167	49.330783	75.774938
171.102822	43.656022	75.779943
170.856837	46.581576	75.784948
169.926593	53.816282	75.789953
169.175689	49.686066	75.794958
168.301266	59.090021	75.799962
167.960283	52.374815	75.804967
167.209818	52.082317	75.809972
166.750174	46.889732	75.814977
166.229331	48.657742	75.819982
165.259199	52.884076	75.824986
164.663584	42.904438	75.829991
164.173484	47.318068	75.834996
163.223856	53.197497	75.840001
162.967734	55.307735	75.845006
161.747863	53.368839	75.850010
161.590264	54.811305	75.855015
160.223762	48.380849	75.860020
159.549474	54.391487	75.865025
158.880914	52.690428	75.870030
158.307706	54.802528	75.875034
158.007853	44.953360	75.880039
157.684669	52.981181	75.885044
157.187029	55.381886	75.890049
156.128254	44.747483	75.895054
155.247684	49.617240	75.900058
154.603257	46.802113	75.905063
154.131020	55.291645	75.910068
152.797252	49.365942	75.915073
152.526806	45.149418	75.920078
151.988165	51.026281	75.925082
151.737467	41.896540	75.930087
151.465701	49.140329	75.935092
150.429400	50.032818	75.940097
149.813239	43.210461	75.945102
148.929294	46.829952	75.950106
147.658250	47.717293	75.955111
146.907014	46.000018	75.960116
146.483314	51.349971	75.965121
146.134697	52.580857	75.970126
145.650725	48.268709	75.975130
145.095887	45.056144	75.980135
144.079246	42.826641	75.985140
142.873126	45.740753	75.990145
142.511276	41.706863	75.995150
142.054091	48.759031	76.000154
141.824446	41.413731	76.005159
141.152357	44.521670	76.010164
139.899423	38.092675	76.015169
139.771439	39.415992	76.020174
138.894689	44.392061	76.025178
138.621448	45.084268	76.030183
137.296691	39.793702	76.035188
136.542848	43.857045	76.040193
136.143361	38.685338	76.045198
135.890610	46.166244	76.050202
134.726083	41.606057	76.055207
133.731715	39.862576	76.060212
132.962788	45.326972	76.065217
132.302409	42.444721	76.070222
131.915419	46.562403	76.075226
131.936308	48.166890	76.080231
131.675372	41.291138	76.085236
130.764323	46.687142	76.090241
129.731781	49.123897	76.095246
129.021557	44.528455	76.100250
128.369443	41.808988	76.105255
127.671755	43.552454	76.110260
126.821573	48.595414	76.115265
126.748135	47.747540	76.120270
125.764125	48.810269	76.125274
124.776544	47.760715	76.130279
124.099037	54.690404	76.135284
123.835577	56.626254	76.140289
123.287324	39.213963	76.145294
121.934007	46.920652	76.150298
120.834969	40.402520	76.155303
120.283455	43.172046	76.160308
119.873434	45.845082	76.165313
119.766353	40.360368	76.170318
118.969055	49.157057	76.175322
118.691115	42.272775	76.180327
118.621166	47.359988	76.185332
117.248683	49.543596	76.190337
116.738427	44.150895	76.195342
115.843789	51.243327	76.200346
114.924248	47.515432	76.205351
113.977923	40.944675	76.210356
113.749646	55.143736	76.215361
113.665682	45.570966	76.220366
112.630152	52.369020	76.225370
111.895552	50.676923	76.230375
111.382566	37.583853	76.235380
110.509878	47.040399	76.240385
109.578939	49.405663	76.245390
108.766389	47.087497	76.250394
108.598573	45.012459	76.255399
107.833177	47.858915	76.260404
107.238711	54.550567	76.265409
106.419013	44.808689	76.270414
105.362917	51.581851	76.275418
104.553388	38.466205	76.280423
104.418141	39.453288	76.285428
104.355012	44.153697	76.290433
104.212435	38.298120	76.295438
102.757769	42.899619	76.300442
102.071951	51.493261	76.305447
100.743291	46.609928	76.310452
99.641996	45.157928	76.315457
99.479617	43.992560	76.320462
99.064549	46.853556	76.325466
98.129878	44.231087	76.330471
97.932826	43.681889	76.335476
97.277968	49.944183	76.340481
97.022812	46.411053	76.345486
96.170800	53.813529	76.350490
95.561958	39.721299	76.355495
94.734888	42.035995	76.360500
94.244983	51.899390	76.365505
93.433968	48.163946	76.370510
92.229743	43.292834	76.375514
91.541505	37.828028	76.380519
91.331617	42.156121	76.385524
90.614533	48.195020	76.390529
89.666239	43.687373	76.395534
89.000303	50.116952	76.400538
88.467811	42.325848	76.405543
88.196057	43.770914	76.410548
88.063057	48.744602	76.415553
87.414108	37.618017	76.420558
86.226743	47.805053	76.425562
85.410829	42.096495	76.430567
84.418080	45.058508	76.435572
83.847903	50.482915	76.440577
83.688390	41.793840	76.445582
82.855449	44.915942	76.450586
81.840445	41.402569	76.455591
81.003846	39.023800	76.460596
79.769740	39.179739	76.465601
79.419166	35.406409	76.470606
79.086724	42.938078	76.475610
78.686491	38.618691	76.480615
78.566509	48.876133	76.485620
77.969495	45.318726	76.490625
77.181971	42.000022	76.495630
76.312870	43.717229	76.500634
75.735897	42.654126	76.505639
74.446544	48.861795	76.510644
73.586170	49.234300	76.515649
73.327142	47.295290	76.520654
72.726162	49.613856	76.525658
72.421076	53.210690	76.530663
72.135290	48.393681	76.535668
70.767192	47.215575	76.540673
70.251987	48.086630	76.545678
69.410147	57.580132	76.550682
68.567973	44.033933	76.555687
67.658549	39.137152	76.560692
66.814312	49.237338	76.565697
66.662463	42.098169	76.570702
65.964813	51.691281	76.575706
65.408267	42.962916	76.580711
65.315600	46.934224	76.585716
64.738677	49.055653	76.590721
64.178565	46.216613	76.595726
63.035854	44.744093	76.600730
62.153778	47.641743	76.605735
61.174930	51.533688	76.610740
60.211603	55.789661	76.615745
60.001918	46.890517	76.620750
59.871921	46.225225	76.625754
59.292834	42.199777	76.630759
58.823053	43.031468	76.635764
57.210434	47.212458	76.640769
56.844548	37.228986	76.645774
56.368704	52.383849	76.650778
56.079213	44.089669	76.655783
54.849388	45.398230	76.660788
53.879432	46.614476	76.665793
53.545609	43.815188	76.670798
52.969035	50.914273	76.675802
52.318863	38.478647	76.680807
51.676485	37.787528	76.685812
50.755469	46.744766	76.690817
50.404153	38.898926	76.695822
49.710039	49.801085	76.700826
49.318272	45.894696	76.705831
48.137868	44.647313	76.710836
47.064555	48.886619	76.715841
47.058423	40.149147	76.720846
46.382658	49.542728	76.725850
46.096823	44.706787	76.730855
45.571316	42.876228	76.735860
44.089561	47.613827	76.740865
43.886511	41.507324	76.745870
43.034521	53.756866	76.750874
42.411096	37.057317	76.755879
41.337171	40.836099	76.760884
40.375235	47.797980	76.765889
40.497714	39.958137	76.770894
40.351988	45.845395	76.775898
39.718311	46.616379	76.780903
38.580758	45.261789	76.785908
37.765706	51.565765	76.790913
36.960977	48.801036	76.795918
37.010264	53.655449	76.800922
35.540786	48.073564	76.805927
35.095760	44.814558	76.810932
34.154784	48.265041	76.815937
34.067706	38.827416	76.820942
33.083232	48.922045	76.825946
32.153136	42.791789	76.830951
31.602863	47.312448	76.835956
30.392428	50.260878	76.840961
30.636453	45.030160	76.845966
30.536147	50.351903	76.850970
29.618656	48.532111	76.855975
28.674063	40.367628	76.860980
27.909167	55.004456	76.865985
27.572844	38.930246	76.870990
26.646981	51.261134	76.875994
25.692143	39.902424	76.880999
25.400158	35.626849	76.886004
24.464117	44.814018	76.891009
23.791278	39.174886	76.896014
22.564201	49.803320	76.901018
21.861497	49.539760	76.906023
22.120891	39.425794	76.911028
21.312257	41.406967	76.916033
21.002106	40.000115	76.921038
20.349036	33.581592	76.926042
19.519682	37.976822	76.931047
18.771166	39.710861	76.936052
17.863389	46.331900	76.941057
17.556996	32.832800	76.946062
16.362022	45.181801	76.951066
15.636453	44.042745	76.956071
15.120897	45.854859	76.961076
14.458853	48.421913	76.966081
14.611788	41.179969	76.971086
13.330624	44.959951	76.976090
12.455153	40.477731	76.981095
12.179151	34.283091	76.986100
11.497535	51.304695	76.991105
11.103884	45.740053	76.996110
9.833985	49.149445	77.001114
9.280187	42.781395	77.006119
8.939228	44.198464	77.011124
8.557825	47.794568	77.016129
7.500844	44.959027	77.021134
6.622147	43.165350	77.026139
6.189266	48.047174	77.031143
5.708410	40.730756	77.036148
4.631204	50.306850	77.041153
3.998292	41.468049	77.046158