Tue Jun 08 17:52:01 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.086713	96.569243	0.000000
-0.122701	89.613980	0.005005
-0.713119	58.839987	0.010010
-2.145866	18.533341	0.015014
-6.279338	7.778867	0.020019
-11.462597	8.954948	0.025024
-16.758858	3.975553	0.030029
-21.482724	6.370291	0.035034
-25.136461	-1.106636	0.040038
-29.537136	8.858506	0.045043
-33.041047	1.543382	0.050048
-36.611856	-3.104257	0.055053
-40.223768	0.034902	0.060058
-43.473812	-3.775687	0.065062
-47.678011	-1.453848	0.070067
-51.187094	3.310078	0.075072
-55.208103	0.549399	0.080077
-58.951470	1.554810	0.085082
-62.649888	-9.704429	0.090086
-66.235856	2.662974	0.095091
-69.959075	0.241613	0.100096
-73.693909	-0.150124	0.105101
-77.433652	1.576606	0.110106
-81.410176	2.625174	0.115110
-85.504609	6.688634	0.120115
-89.208539	-6.717653	0.125120
-92.826833	-1.681566	0.130125
-96.764446	12.344347	0.135130
-100.147021	-3.538588	0.140134
-104.059702	1.457996	0.145139
-107.521938	0.209595	0.150144
-111.476336	-0.159853	0.155149
-115.556678	11.808847	0.160154
-119.505973	0.627410	0.165158
-122.959529	15.349888	0.170163
-126.342074	2.126921	0.175168
-130.148262	-5.285480	0.180173
-133.712769	4.064281	0.185178
-137.700675	-5.755076	0.190182
-141.996896	-2.942536	0.195187
-145.930565	2.332006	0.200192
-149.456456	-3.763934	0.205197
-153.655256	9.188990	0.210202
-157.111646	-2.119567	0.215206
-160.875397	7.053214	0.220211
-164.554594	-0.873140	0.225216
-167.628801	-2.079100	0.230221
-171.840598	3.558535	0.235226
-175.196072	-4.573711	0.240230
-179.479704	-0.051042	0.245235
-183.109774	-4.207638	0.250240
-186.782067	-1.548636	0.255245
-190.921277	4.414043	0.260250
-193.978545	-7.502891	0.265254
-198.220558	4.264663	0.270259
-202.177011	1.863285	0.275264
-205.771460	-1.302758	0.280269
-209.793545	2.579858	0.285274
-213.039271	-3.381722	0.290278
-216.844453	3.882282	0.295283
-220.789888	5.595067	0.300288
-224.157877	3.006735	0.305293
-228.105527	3.053836	0.310298
-231.652833	-1.136650	0.315302
-235.700214	3.290290	0.320307
-239.692494	0.029098	0.325312
-243.641169	5.370237	0.330317
-247.168964	8.253171	0.335322
-250.481055	-2.912300	0.340326
-254.596935	2.505285	0.345331
-258.156664	0.060385	0.350336
-261.755097	-1.678447	0.355341
-266.123845	5.401225	0.360346
-270.039222	-2.640039	0.365350
-273.471147	0.211076	0.370355
-277.346246	7.192273	0.375360
-280.977727	0.334213	0.380365
-284.861435	6.386561	0.385370
-288.387810	-1.502740	0.390374
-292.160732	-0.601798	0.395379
-295.559971	4.884729	0.400384
-299.577502	-11.234078	0.405389
-303.627724	-0.220868	0.410394
-307.206876	-2.858566	0.415398
-311.045943	-1.186842	0.420403
-314.872548	-2.436523	0.425408
-318.582282	1.454578	0.430413
-322.556476	4.587417	0.435418
-326.086741	-1.019368	0.440422
-329.969015	1.221455	0.445427
-333.641940	7.067566	0.450432
-337.057935	3.550122	0.455437
-341.104363	2.332249	0.460442
-344.714147	-8.482881	0.465446
-348.517414	6.084202	0.470451
-352.406328	-4.172683	0.475456
-356.013254	-3.928540	0.480461
-359.980357	3.530312	0.485466
-363.605015	-7.153969	0.490470
-367.299925	3.058263	0.495475
-371.579781	-5.216015	0.500480
-375.417769	-10.325523	0.505485
-379.235041	2.849079	0.510490
-382.620975	-8.389258	0.515494
-385.709545	-2.490207	0.520499
-389.704680	-2.323115	0.525504
-393.541472	-7.984221	0.530509
-397.863352	-2.393817	0.535514
-401.495660	-4.412491	0.540518
-405.265560	2.746928	0.545523
-409.118311	1.347482	0.550528
-412.693268	0.038137	0.555533
-416.780514	10.674927	0.560538
-419.724761	5.589354	0.565542
-423.905051	2.164022	0.570547
-427.507593	3.501603	0.575552
-431.550857	5.873151	0.580557
-435.471043	-0.121352	0.585562
-438.388328	5.237596	0.590566
-442.409452	11.839006	0.595571
-446.252822	1.980156	0.600576
-450.327852	5.236976	0.605581
-454.249604	10.582355	0.610586
-457.813544	4.567803	0.615590
-461.590412	8.528164	0.620595
-465.397116	5.433487	0.625600
-468.772611	6.869902	0.630605
-472.883327	9.755128	0.635610
-476.014099	2.229536	0.640614
-480.213386	4.462511	0.645619
-483.814160	5.577219	0.650624
-487.878765	5.909860	0.655629
-491.388746	13.760098	0.660634
-495.290410	-1.584232	0.665638
-499.461827	-0.928935	0.670643
-503.041139	7.256471	0.675648
-506.812427	2.697701	0.680653
-510.280542	8.711687	0.685658
-513.764857	3.609510	0.690662
-517.922122	5.231407	0.695667
-522.198651	5.041927	0.700672
-525.560394	2.053314	0.705677
-529.753078	10.838157	0.710682
-533.050642	-0.069449	0.715686
-537.055552	5.814438	0.720691
-540.556382	-1.205928	0.725696
-543.602510	-0.324882	0.730701
-547.759093	4.890351	0.735706
-551.628516	0.470425	0.740710
-555.723047	4.561151	0.745715
-559.553007	6.078377	0.750720
-563.195494	6.553773	0.755725
-567.132540	5.200508	0.760730
-570.231805	0.483462	0.765734
-574.169980	-3.698477	0.770739
-578.124291	2.342934	0.775744
-582.146938	-7.968136	0.780749
-586.086025	-6.833187	0.785754
-589.539089	-0.402944	0.790758
-593.276974	0.355275	0.795763
-596.817913	-0.936862	0.800768
-600.581369	-0.771048	0.805773
-604.382818	6.017389	0.810778
-607.973058	-4.486663	0.815782
-611.940900	4.746734	0.820787
-615.705596	1.241593	0.825792
-619.081738	3.114779	0.830797
-623.104153	7.663288	0.835802
-626.901655	-5.118565	0.840806
-630.796250	-9.166621	0.845811
-635.034246	1.075055	0.850816
-638.705828	-0.394352	0.855821
-642.547483	5.113872	0.860826
-645.626936	-0.387644	0.865830
-649.301172	0.919791	0.870835
-653.349141	8.907066	0.875840
-656.816574	-1.321986	0.880845
-660.851783	11.537357	0.885850
-664.819460	3.268625	0.890854
-668.516152	6.373877	0.895859
-671.985990	8.240684	0.900864
-675.489986	-1.840376	0.905869
-679.704284	1.643822	0.910874
-683.377875	1.830204	0.915878
-687.612699	6.725461	0.920883
-691.383884	8.291130	0.925888
-694.898093	-1.650011	0.930893
-698.337771	-1.903599	0.935898
-701.530718	-6.151736	0.940902
-705.805395	-0.468893	0.945907
-709.726032	8.373223	0.950912
-713.528254	9.872796	0.955917
-717.578107	8.071693	0.960922
-721.097564	1.814494	0.965926
-724.643139	8.767125	0.970931
-729.011608	6.268797	0.975936
-732.336508	-3.843341	0.980941
-735.979367	3.838045	0.985946
-739.700428	2.553256	0.990950
-743.659161	7.171856	0.995955
-747.541784	4.411361	1.000960
-750.702544	-5.082795	1.005965
-754.818340	9.248500	1.010970
-758.613388	-3.989135	1.015974
-762.484075	6.943109	1.020979
-766.524584	6.179321	1.025984
-769.916447	2.359689	1.030989
-773.725169	5.579774	1.035994
-777.546238	3.085432	1.040998
-781.560705	-4.379812	1.046003
-785.041808	2.169456	1.051008
-788.446602	7.354153	1.056013
-793.054736	2.899807	1.061018
-796.516112	-0.310284	1.066022
-800.291190	4.184874	1.071027
-803.790302	4.180764	1.076032
-806.996119	1.449803	1.081037
-811.306415	0.155302	1.086042
-814.860867	3.058246	1.091046
-818.867538	3.954364	1.096051
-822.635170	3.990833	1.101056
-826.192655	2.293204	1.106061
-830.260111	8.359775	1.111066
-834.195332	8.981163	1.116070
-837.615617	6.008375	1.121075
-841.196418	9.205184	1.126080
-845.089372	5.462152	1.131085
-849.113351	6.594146	1.136090
-852.392258	-4.866207	1.141094
-856.374977	3.498429	1.146099
-860.542192	-0.068834	1.151104
-864.073229	-5.234130	1.156109
-868.152795	2.418510	1.161114
-871.685662	-4.827756	1.166118
-875.273039	7.214409	1.171123
-879.202936	5.208147	1.176128
-882.340271	-4.117038	1.181133
-886.685964	2.745707	1.186138
-890.118480	-1.404321	1.191142
-894.206921	1.547328	1.196147
-898.004981	7.897294	1.201152
-901.496899	-0.207755	1.206157
-905.402903	1.715556	1.211162
-909.051200	0.746822	1.216166
-912.949327	-1.666278	1.221171
-916.864410	9.006492	1.226176
-920.144779	4.981542	1.231181
-924.106536	6.347248	1.236186
-927.831151	-1.016830	1.241190
-931.671519	7.527891	1.246195
-935.786225	7.545889	1.251200
-939.373393	3.847155	1.256205
-943.342704	8.436957	1.261210
-946.618993	-1.294158	1.266214
-950.279856	-0.322295	1.271219
-954.683691	1.138672	1.276224
-957.728519	9.894972	1.281229
-961.806368	7.287393	1.286234
-965.545174	8.380010	1.291238
-969.512042	9.580068	1.296243
-973.214312	6.219652	1.301248
-976.485420	-2.182164	1.306253
-980.881057	7.342463	1.311258
-984.208906	8.709911	1.316262
-987.927288	12.745527	1.321267
-991.380006	4.490154	1.326272
-995.205147	3.023343	1.331277
-999.386164	7.192469	1.336282
-1003.424329	10.658180	1.341286
-1007.145214	6.085294	1.346291
-1011.082670	16.456088	1.351296
-1014.731004	7.294127	1.356301
-1018.292938	7.441888	1.361306
-1021.933443	7.673793	1.366310
-1025.676448	7.002845	1.371315
-1029.322081	6.972368	1.376320
-1033.142758	0.074849	1.381325
-1036.988416	2.190795	1.386330
-1040.701803	-0.179304	1.391334
-1044.612474	1.064064	1.396339
-1048.538654	9.074972	1.401344
-1052.020900	4.827443	1.406349
-1055.960110	6.107298	1.411354
-1059.460900	-3.228355	1.416358
-1063.246034	0.425654	1.421363
-1066.876395	9.075337	1.426368
-1070.809556	-4.638354	1.431373
-1074.767794	-1.537988	1.436378
-1078.491257	2.465813	1.441382
-1082.355022	-1.072414	1.446387
-1085.902141	-2.376501	1.451392
-1089.349093	-7.660633	1.456397
-1093.814682	0.378592	1.461402
-1097.378845	0.449044	1.466406
-1100.978912	3.162301	1.471411
-1104.637643	3.547001	1.476416
-1108.101320	-5.712880	1.481421
-1112.421926	-4.957963	1.486426
-1116.261702	-2.585609	1.491430
-1119.991286	5.752360	1.496435
-1123.582432	6.836731	1.501440
-1127.055957	-3.759890	1.506445
-1131.601251	5.366660	1.511450
-1135.051585	-5.428526	1.516454
-1138.730092	-6.064267	1.521459
-1142.301889	1.641144	1.526464
-1145.855232	-3.862678	1.531469
-1149.775613	5.382746	1.536474
-1153.676102	3.082769	1.541478
-1157.471533	-2.053444	1.546483
-1161.700343	-4.167568	1.551488
-1164.890337	-1.583490	1.556493
-1168.959307	-0.007717	1.561498
-1172.334372	7.087270	1.566502
-1175.919910	-1.770733	1.571507
-1179.665503	1.385178	1.576512
-1183.603702	-0.910267	1.581517
-1187.637133	-2.858591	1.586522
-1191.146644	-4.261803	1.591526
-1194.990245	-5.069654	1.596531
-1198.990390	-2.319977	1.601536
-1202.485155	-2.480021	1.606541
-1206.453010	0.918934	1.611546
-1209.730174	-11.622095	1.616550
-1213.412819	-4.402425	1.621555
-1217.697744	-4.212431	1.626560
-1221.668697	-6.374330	1.631565
-1225.413659	1.861765	1.636570
-1228.845199	-9.923321	1.641574
-1232.339801	-0.777401	1.646579
-1236.422385	0.753015	1.651584
-1239.807305	3.899136	1.656589
-1244.059043	0.640045	1.661594
-1247.571687	-7.535723	1.666598
-1251.706405	3.614735	1.671603
-1255.401849	5.587060	1.676608
-1258.648560	3.080564	1.681613
-1262.779038	7.913048	1.686618
-1266.186154	5.457395	1.691622
-1269.966624	5.773153	1.696627
-1273.760720	1.435310	1.701632
-1277.456577	0.656234	1.706637
-1281.592911	-1.130257	1.711642
-1285.698546	2.224940	1.716646
-1289.159528	1.371984	1.721651
-1293.055503	-1.458329	1.726656
-1296.582361	-4.933436	1.731661
-1300.572548	-2.060254	1.736666
-1304.142039	-5.216216	1.741670
-1307.915747	-1.416339	1.746675
-1311.785790	2.911231	1.751680
-1314.889215	-2.049240	1.756685
-1318.832589	8.439255	1.761690
-1322.706004	-4.296872	1.766694
-1326.633887	6.523281	1.771699
-1330.851548	6.866033	1.776704
-1334.194964	4.435809	1.781709
-1338.110723	10.334683	1.786714
-1341.539076	-7.763364	1.791718
-1345.440264	-7.785195	1.796723
-1349.340270	6.432150	1.801728
-1352.846220	-8.125471	1.806733
-1356.926919	1.794581	1.811738
-1360.729692	-6.978563	1.816742
-1364.210608	5.724554	1.821747
-1368.096461	-2.728418	1.826752
-1371.390447	-9.310315	1.831757
-1375.710542	-1.646307	1.836762
-1378.975076	-3.374048	1.841766
-1382.898730	-4.848050	1.846771
-1386.671271	-1.637600	1.851776
-1390.467600	-7.680464	1.856781
-1394.626179	1.589106	1.861786
-1398.231904	-3.891279	1.866790
-1401.885700	0.369620	1.871795
-1405.421574	-3.018192	1.876800
-1409.290521	-4.460912	1.881805
-1413.372380	-1.754231	1.886810
-1417.059697	5.533114	1.891814
-1420.426347	1.930338	1.896819
-1424.590898	-1.139871	1.901824
-1427.944385	-7.933717	1.906829
-1432.069949	-0.228473	1.911834
-1435.682064	0.153637	1.916838
-1439.400897	1.654914	1.921843
-1443.374685	13.572833	1.926848
-1446.953516	-3.066087	1.931853
-1450.840143	4.093301	1.936858
-1454.692338	6.222585	1.941862
-1458.420523	-1.578095	1.946867
-1462.162248	10.631523	1.951872
-1465.541416	2.014240	1.956877
-1469.964095	-0.015343	1.961882
-1473.151479	-6.536526	1.966886
-1476.658637	4.807079	1.971891
-1480.689073	-3.059273	1.976896
-1484.676032	-5.210271	1.981901
-1488.101434	0.424897	1.986906
-1491.969019	2.136498	1.991910
-1495.702260	5.522250	1.996915
-1500.060741	-0.009501	2.006912
-1500.517670	6.196317	2.016909
-1498.307319	4.526982	2.026906
-1495.431779	-2.370645	2.036902
-1493.228142	2.105502	2.046899
-1491.671988	-3.189724	2.056896
-1489.659582	-1.349572	2.066893
-1487.644833	-2.068804	2.076890
-1485.582382	2.223723	2.086886
-1483.675908	-6.348691	2.096883
-1482.035491	-2.478065	2.106880
-1480.243898	-1.284871	2.116877
-1478.174754	-2.220138	2.126874
-1475.989034	-9.662007	2.136870
-1474.249419	-6.230899	2.146867
-1472.362955	-1.453245	2.156864
-1470.859291	-7.667002	2.166861
-1468.482537	-2.369697	2.176858
-1466.696859	0.064292	2.186854
-1464.741607	-11.177835	2.196851
-1463.060893	-6.071981	2.206848
-1461.061795	-11.189960	2.216845
-1459.238743	-9.299480	2.226842
-1457.077615	-6.119808	2.236838
-1455.224049	-2.699572	2.246835
-1453.809489	-5.622518	2.256832
-1451.947954	-0.229577	2.266829
-1449.771383	-3.130484	2.276826
-1448.021679	-2.792823	2.286822
-1446.064106	-4.811542	2.296819
-1443.998567	-9.797863	2.306816
-1442.110183	-3.577614	2.316813
-1440.499914	-0.448341	2.326810
-1438.568863	-3.165580	2.336806
-1436.468611	-3.045032	2.346803
-1434.679558	-3.599000	2.356800
-1432.860280	-7.305609	2.366797
-1431.032895	0.266863	2.376794
-1429.049780	-6.429989	2.386790
-1427.244415	-9.631894	2.396787
-1425.368994	-9.233221	2.406784
-1423.439855	-8.460421	2.416781
-1421.589040	-3.150989	2.426778
-1419.548151	-2.439277	2.436774
-1417.741977	-7.977403	2.446771
-1415.632114	-5.791154	2.456768
-1414.207147	-3.285296	2.466765
-1412.145948	-0.446492	2.476762
-1410.130614	0.365256	2.486758
-1408.434682	-3.049832	2.496755
-1406.580603	-5.606816	2.506752
-1404.658903	-1.812535	2.516749
-1402.893453	-1.693739	2.526746
-1400.801694	-2.000913	2.536742
-1398.742399	-1.106603	2.546739
-1397.021917	-4.006203	2.556736
-1395.389761	0.355546	2.566733
-1393.319435	0.225160	2.576730
-1391.485406	-3.499381	2.586726
-1389.707189	-5.013409	2.596723
-1387.272439	-7.211292	2.606720
-1385.793606	-3.875252	2.616717
-1384.030195	1.553156	2.626714
-1382.326309	-5.548229	2.636710
-1380.182322	-5.060111	2.646707
-1377.995486	-0.104388	2.656704
-1376.408608	0.302375	2.666701
-1374.840998	7.659060	2.676698
-1372.637445	6.165641	2.686694
-1371.058585	-1.241499	2.696691
-1368.769051	-5.680958	2.706688
-1367.221266	-0.305217	2.716685
-1365.120905	-3.723364	2.726682
-1363.124845	-1.774820	2.736678
-1361.484197	-4.034680	2.746675
-1359.926081	-5.299847	2.756672
-1357.846555	2.951404	2.766669
-1355.475521	-1.885008	2.776666
-1353.990776	9.795690	2.786662
-1351.906300	4.616847	2.796659
-1350.174669	4.984924	2.806656
-1348.301864	3.697720	2.816653
-1346.521377	4.551815	2.826650
-1344.162368	4.822011	2.836646
-1342.686850	2.004819	2.846643
-1340.716629	3.111668	2.856640
-1338.944725	2.777658	2.866637
-1337.147543	4.582137	2.876634
-1335.091021	5.174620	2.886630
-1333.033604	-0.324034	2.896627
-1331.427143	3.216168	2.906624
-1329.384052	2.628096	2.916621
-1327.662814	12.106781	2.926618
-1325.812205	3.475248	2.936614
-1323.956796	4.785599	2.946611
-1321.761558	-0.567572	2.956608
-1320.245334	-2.699735	2.966605
-1318.344090	1.181099	2.976602
-1316.361133	0.622726	2.986598
-1314.279627	0.990400	2.996595
-1312.687511	-7.822784	3.006592
-1310.903541	-6.882326	3.016589
-1309.042079	-5.256051	3.026586
-1306.834285	-0.686845	3.036582
-1304.861249	-3.186363	3.046579
-1303.106408	-0.626858	3.056576
-1301.543350	-2.166734	3.066573
-1299.595225	-3.107608	3.076570
-1297.027197	1.675193	3.086566
-1295.443470	-0.538112	3.096563
-1294.029394	-6.985414	3.106560
-1292.041147	-5.880057	3.116557
-1289.710797	-0.137960	3.126554
-1288.121412	1.276589	3.136550
-1286.513929	-2.742954	3.146547
-1284.510265	0.286806	3.156544
-1282.577733	-0.272770	3.166541
-1280.788783	-5.105204	3.176538
-1279.233260	-2.541887	3.186534
-1276.675295	3.331856	3.196531
-1274.890036	0.371379	3.206528
-1273.215876	0.247046	3.216525
-1271.305191	7.207346	3.226522
-1269.292733	2.290287	3.236518
-1267.668899	-0.437743	3.246515
-1265.350795	2.738789	3.256512
-1263.626809	-2.378495	3.266509
-1262.172479	-2.229522	3.276506
-1260.289838	-2.878927	3.286502
-1258.070236	-3.101674	3.296499
-1256.618234	-5.717984	3.306496
-1254.817509	-5.357782	3.316493
-1252.273462	-2.009796	3.326490
-1250.634534	3.528978	3.336486
-1248.739377	-5.695482	3.346483
-1246.741831	1.259000	3.356480
-1244.977341	2.245910	3.366477
-1243.079614	4.826352	3.376474
-1241.361451	2.201880	3.386470
-1239.185451	6.985653	3.396467
-1237.461288	2.972961	3.406464
-1235.890895	7.511379	3.416461
-1233.821553	3.349694	3.426458
-1231.839088	3.821760	3.436454
-1229.957100	-4.542034	3.446451
-1228.285331	-3.209587	3.456448
-1226.169306	3.872763	3.466445
-1224.121625	2.469819	3.476442
-1222.534635	3.069485	3.486438
-1220.920851	-2.195637	3.496435
-1218.770987	1.524380	3.506432
-1216.511885	1.534369	3.516429
-1214.971927	4.726400	3.526426
-1213.422536	4.793459	3.536422
-1211.549482	-2.132204	3.546419
-1209.168359	0.391321	3.556416
-1207.444814	2.570517	3.566413
-1205.633455	3.882163	3.576410
-1203.224908	0.969993	3.586406
-1202.197308	3.307835	3.596403
-1200.320340	-4.576882	3.606400
-1198.032479	2.243986	3.616397
-1196.104989	0.364124	3.626394
-1194.297902	-1.534975	3.636390
-1192.354203	-3.065881	3.646387
-1190.709365	3.665838	3.656384
-1188.451270	2.923928	3.666381
-1186.977201	-1.617271	3.676378
-1185.136372	3.795171	3.686374
-1183.226160	0.934602	3.696371
-1181.217971	-0.013767	3.706368
-1179.223735	-0.804420	3.716365
-1177.422802	-2.333329	3.726362
-1175.506567	5.882839	3.736358
-1173.828798	3.108825	3.746355
-1172.052104	6.225441	3.756352
-1169.836347	6.637319	3.766349
-1167.977447	2.162435	3.776346
-1166.051636	0.176959	3.786342
-1164.347922	5.062033	3.796339
-1162.207544	6.445247	3.806336
-1160.529224	2.085556	3.816333
-1158.833244	-1.290719	3.826330
-1156.863301	1.054858	3.836326
-1154.932218	-9.357418	3.846323
-1153.095332	-4.432767	3.856320
-1151.276429	-5.358101	3.866317
-1149.152276	-1.751009	3.876314
-1147.573749	-1.243131	3.886310
-1145.746736	-2.258383	3.896307
-1143.618042	3.497092	3.906304
-1141.608268	-3.895845	3.916301
-1140.148295	0.178624	3.926298
-1138.049455	8.269792	3.936294
-1136.063068	4.875668	3.946291
-1134.447540	5.264562	3.956288
-1132.469882	1.781041	3.966285
-1130.384226	1.324078	3.976282
-1128.426572	3.054855	3.986278
-1126.982990	-0.354739	3.996275
-1124.764229	-1.342401	4.006272
-1123.211673	-1.911352	4.016269
-1121.224751	5.307445	4.026266
-1119.257377	4.902416	4.036262
-1117.304369	-2.694968	4.046259
-1115.407141	0.019596	4.056256
-1113.571260	-3.056612	4.066253
-1111.769150	3.963911	4.076250
-1110.038863	-0.286517	4.086246
-1108.304952	-1.397612	4.096243
-1105.871180	-0.535050	4.106240
-1104.168616	1.624476	4.116237
-1102.446536	4.193648	4.126234
-1100.544863	0.115353	4.136230
-1098.598873	2.213322	4.146227
-1096.686688	3.306936	4.156224
-1095.120431	5.962940	4.166221
-1093.105265	5.636663	4.176218
-1090.879340	1.180202	4.186214
-1089.086212	2.111675	4.196211
-1087.015556	0.677976	4.206208
-1085.503621	-0.262600	4.216205
-1083.552102	3.925492	4.226202
-1082.040579	2.062565	4.236198
-1079.998540	-4.317427	4.246195
-1077.798039	-3.128267	4.256192
-1076.067352	4.028239	4.266189
-1074.576242	2.283826	4.276186
-1072.470033	-0.473212	4.286182
-1070.447414	3.947314	4.296179
-1068.661238	3.001154	4.306176
-1066.587047	2.656060	4.316173
-1064.835467	2.240683	4.326170
-1063.082823	5.339741	4.336166
-1061.055690	0.545137	4.346163
-1059.115629	2.773773	4.356160
-1057.444658	0.625799	4.366157
-1055.684384	-0.385861	4.376154
-1053.405679	-3.402915	4.386150
-1051.448311	-3.674985	4.396147
-1050.260752	-7.657916	4.406144
-1048.021369	-6.765501	4.416141
-1045.717320	-5.947818	4.426138
-1044.454169	-9.648107	4.436134
-1042.662199	-3.964788	4.446131
-1040.195488	-4.996955	4.456128
-1038.763542	-8.410846	4.466125
-1036.691860	-1.515219	4.476122
-1034.703134	-2.774371	4.486118
-1033.132181	-1.875076	4.496115
-1031.238542	-5.001083	4.506112
-1029.000311	-3.247690	4.516109
-1027.321814	1.197558	4.526106
-1025.718277	0.016005	4.536102
-1023.762636	2.221432	4.546099
-1021.217803	3.122676	4.556096
-1019.678549	-0.676787	4.566093
-1018.152425	1.730040	4.576090
-1016.270709	4.814072	4.586086
-1014.007988	5.478809	4.596083
-1012.154478	5.460134	4.606080
-1010.319711	6.453655	4.616077
-1008.681872	3.605143	4.626074
-1006.889490	1.602727	4.636070
-1004.756114	3.950356	4.646067
-1003.030589	4.790718	4.656064
-1000.938319	4.769788	4.666061
-999.147815	2.552306	4.676058
-997.112369	6.758440	4.686054
-995.186141	-4.944504	4.696051
-993.441919	3.111591	4.706048
-991.709951	3.616107	4.716045
-990.042591	5.422479	4.726042
-988.094428	3.976262	4.736038
-985.976084	3.000773	4.746035
-984.415525	4.408534	4.756032
-982.261364	3.445867	4.766029
-980.467418	-3.999666	4.776026
-978.716445	7.138328	4.786022
-976.590539	3.816752	4.796019
-974.709030	0.917329	4.806016
-972.976971	-0.332114	4.816013
-970.874010	6.668053	4.826010
-969.468716	12.017448	4.836006
-966.817604	6.871912	4.846003
-965.660660	9.374944	4.856000
-963.292803	4.873229	4.865997
-961.158556	7.392649	4.875994
-960.152569	9.054897	4.885990
-958.178442	5.161430	4.895987
-956.022735	1.098072	4.905984
-954.409308	5.434379	4.915981
-952.134925	5.660833	4.925978
-950.545119	4.382071	4.935974
-948.450310	1.202985	4.945971
-946.676023	2.729387	4.955968
-944.825075	7.419345	4.965965
-942.826003	3.643327	4.975962
-940.995446	5.802687	4.985958
-939.018794	6.722479	4.995955
-937.410300	6.344760	5.005952
-935.235633	6.180086	5.015949
-933.340066	5.660211	5.025946
-931.817643	4.997303	5.035942
-929.613815	9.883578	5.045939
-928.046624	7.151953	5.055936
-925.938380	13.713742	5.065933
-924.148026	5.297804	5.075930
-922.239007	6.598343	5.085926
-920.485365	13.034863	5.095923
-918.397785	3.201654	5.105920
-916.236752	12.908576	5.115917
-914.532847	10.582291	5.125914
-912.829946	1.191364	5.135910
-911.130885	6.257965	5.145907
-909.530780	4.646262	5.155904
-907.379979	4.190476	5.165901
-905.259204	10.348193	5.175898
-903.363096	7.933984	5.185894
-901.459261	6.286348	5.195891
-899.799401	0.417043	5.205888
-898.228028	-3.756627	5.215885
-895.761110	3.907503	5.225882
-894.148714	6.549738	5.235878
-892.067842	5.786633	5.245875
-890.526472	5.385674	5.255872
-888.508120	3.061147	5.265869
-886.662345	1.898924	5.275866
-884.757164	3.926540	5.285862
-882.875291	-0.814598	5.295859
-880.910286	0.614279	5.305856
-879.070398	1.480114	5.315853
-876.915145	6.365271	5.325850
-875.402390	6.138776	5.335846
-873.647496	1.219856	5.345843
-871.721292	2.891735	5.355840
-869.764466	1.916757	5.365837
-867.636508	4.623451	5.375834
-865.876573	4.637501	5.385830
-864.225654	4.239089	5.395827
-862.325472	6.571492	5.405824
-859.938156	1.946740	5.415821
-858.403320	5.197888	5.425818
-856.669516	7.933515	5.435814
-854.621391	-0.901306	5.445811
-852.814702	3.794711	5.455808
-850.909864	3.420299	5.465805
-849.079022	-2.565284	5.475802
-847.464025	0.972073	5.485798
-845.452709	4.995097	5.495795
-843.397836	1.463666	5.505792
-841.389423	-0.571419	5.515789
-839.429768	7.154528	5.525786
-837.713395	7.559424	5.535782
-835.971073	2.503955	5.545779
-833.931151	-7.241993	5.555776
-832.127450	-3.420060	5.565773
-830.365934	0.192934	5.575770
-828.683550	-3.937720	5.585766
-826.326304	-4.083091	5.595763
-824.619729	-2.672668	5.605760
-822.830164	-7.284906	5.615757
-821.029326	-1.496689	5.625754
-819.088224	-0.406331	5.635750
-817.219716	-0.369399	5.645747
-815.548537	-1.685792	5.655744
-813.481669	0.788754	5.665741
-811.495505	-4.337014	5.675738
-809.591785	-5.811487	5.685734
-807.748623	3.101928	5.695731
-806.065532	-1.116183	5.705728
-804.130132	-1.016427	5.715725
-801.977549	-2.423743	5.725722
-800.350745	2.753717	5.735718
-798.360196	5.588368	5.745715
-796.366483	-1.763739	5.755712
-794.698164	-3.218748	5.765709
-792.783302	0.105917	5.775706
-790.932104	-3.512258	5.785702
-789.129671	-7.278961	5.795699
-786.960492	-7.997101	5.805696
-785.021198	-5.480885	5.815693
-783.568740	-0.238716	5.825690
-781.695964	4.789037	5.835686
-779.428340	-1.909363	5.845683
-777.771106	2.194623	5.855680
-776.081663	1.263999	5.865677
-774.126715	-4.419574	5.875674
-771.889469	1.539983	5.885670
-769.738820	0.821474	5.895667
-768.723750	2.934335	5.905664
-766.648952	4.493021	5.915661
-764.950720	5.103409	5.925658
-763.067433	3.783038	5.935654
-760.787450	3.968320	5.945651
-758.934012	4.198751	5.955648
-757.009199	-1.502171	5.965645
-755.369961	1.468676	5.975642
-753.097136	0.842238	5.985638
-751.543805	-1.040007	5.995635
-749.602177	-2.711059	6.005632
-747.574686	3.824374	6.015629
-746.018683	2.443198	6.025626
-744.065634	5.277988	6.035622
-742.150820	3.170878	6.045619
-740.240998	6.425296	6.055616
-738.404072	2.640043	6.065613
-736.164814	-1.066449	6.075610
-734.619286	1.768333	6.085606
-732.821539	0.593866	6.095603
-730.721967	1.379234	6.105600
-729.093704	2.209526	6.115597
-727.088228	-0.954128	6.125594
-725.420200	-5.707905	6.135590
-723.187062	1.719020	6.145587
-721.290572	6.977490	6.155584
-719.677688	2.502317	6.165581
-717.694793	4.979863	6.175578
-715.951775	3.642877	6.185574
-714.072059	3.459772	6.195571
-712.159656	5.207208	6.205568
-709.958362	6.214233	6.215565
-708.257227	1.063912	6.225562
-706.548779	-0.766686	6.235558
-704.721144	3.698163	6.245555
-702.579796	1.134452	6.255552
-700.903610	1.957716	6.265549
-699.213881	6.562429	6.275546
-696.975000	11.889412	6.285542
-695.280696	2.275146	6.295539
-693.061274	7.458449	6.305536
-691.374943	1.998455	6.315533
-689.377686	-1.122670	6.325530
-688.017510	7.523539	6.335526
-685.795094	7.357120	6.345523
-684.035973	2.250209	6.355520
-682.066907	3.320815	6.365517
-679.967815	6.440025	6.375514
-678.175373	3.970980	6.385510
-676.723620	-5.559363	6.395507
-675.090495	7.549788	6.405504
-672.508055	4.617541	6.415501
-670.307950	-0.727475	6.425498
-669.232123	2.257496	6.435494
-667.027456	1.886250	6.445491
-664.990934	5.844968	6.455488
-663.005719	0.998442	6.465485
-661.635831	-4.424625	6.475482
-659.640767	4.938638	6.485478
-657.583863	2.114766	6.495475
-655.662139	2.220887	6.505472
-654.346602	0.639137	6.515469
-651.930768	9.073378	6.525466
-650.038921	8.854625	6.535462
-648.089584	-3.991181	6.545459
-646.372662	5.594504	6.555456
-644.566301	7.184299	6.565453
-642.626166	-0.250641	6.575450
-640.828503	-4.272964	6.585446
-638.964256	8.756629	6.595443
-636.793143	4.227975	6.605440
-635.147007	-0.186480	6.615437
-633.471805	7.305418	6.625434
-631.310678	6.190360	6.635430
-629.588694	7.409702	6.645427
-627.694504	3.701611	6.655424
-625.826635	-3.552954	6.665421
-623.918363	-0.728999	6.675418
-622.077820	2.164676	6.685414
-620.267960	4.281886	6.695411
-618.346504	5.761042	6.705408
-616.368379	-2.209202	6.715405
-614.130050	3.717458	6.725402
-612.577035	1.710822	6.735398
-610.737023	6.875492	6.745395
-608.844506	7.304398	6.755392
-607.230586	-0.296662	6.765389
-605.303408	-0.549518	6.775386
-603.279753	4.226369	6.785382
-601.290690	-0.871752	6.795379
-599.429129	5.071748	6.805376
-597.646589	-0.268375	6.815373
-595.496819	3.739317	6.825370
-593.997711	-1.349424	6.835366
-591.850804	7.067766	6.845363
-590.163142	4.646771	6.855360
-588.337656	-1.047320	6.865357
-586.401170	-1.331011	6.875354
-584.476482	-1.924105	6.885350
-582.453100	-3.704360	6.895347
-580.942946	-2.018263	6.905344
-579.273499	-9.279865	6.915341
-576.701637	-1.301162	6.925338
-575.120958	0.053108	6.935334
-573.090277	3.686823	6.945331
-571.151486	-2.380024	6.955328
-569.373797	0.083401	6.965325
-567.791763	0.129679	6.975322
-565.783753	-2.991263	6.985318
-564.123798	0.201775	6.995315
-561.823231	-2.080134	7.005312
-559.989823	-4.286625	7.015309
-558.213932	-4.673959	7.025306
-556.373378	-5.819736	7.035302
-554.599764	-1.101307	7.045299
-552.638610	1.472528	7.055296
-550.611420	-5.179377	7.065293
-549.074122	5.687634	7.075290
-546.907592	5.065312	7.085286
-544.775012	0.934179	7.095283
-543.092310	5.145347	7.105280
-541.588948	-4.083184	7.115277
-539.232636	-0.836910	7.125274
-537.812833	1.169020	7.135270
-535.651799	0.459909	7.145267
-533.633004	-10.107116	7.155264
-532.050057	-4.861155	7.165261
-530.042192	-4.238987	7.175258
-528.388515	-4.109346	7.185254
-526.628513	-4.537414	7.195251
-524.559033	4.828570	7.205248
-522.164958	-3.694773	7.215245
-520.475473	-3.661777	7.225242
-518.908694	-3.149674	7.235238
-517.116016	-4.012942	7.245235
-514.961844	-0.637911	7.255232
-513.249878	-2.260368	7.265229
-511.294322	5.367258	7.275226
-509.067562	7.280590	7.285222
-507.921456	3.525819	7.295219
-505.950403	-2.959143	7.305216
-503.715251	-1.502140	7.315213
-501.456264	3.221566	7.325210
-500.069217	8.648965	7.335206
-498.259439	-0.549530	7.345203
-496.490671	-1.950131	7.355200
-494.320995	2.319783	7.365197
-492.549664	-2.582853	7.375194
-490.615860	3.827304	7.385190
-488.893368	5.499136	7.395187
-486.853604	1.745574	7.405184
-484.873793	-2.604355	7.415181
-482.967610	-5.384901	7.425178
-481.411756	-0.904542	7.435174
-479.554968	2.768935	7.445171
-477.310608	-4.717744	7.455168
-475.644638	0.279636	7.465165
-473.723551	-1.255378	7.475162
-472.292663	-2.094893	7.485158
-469.803310	1.593368	7.495155
-468.065634	2.973306	7.505152
-466.486786	0.649672	7.515149
-464.404562	2.384288	7.525146
-462.444105	-0.711853	7.535142
-460.667657	4.730957	7.545139
-458.951156	8.587389	7.555136
-456.854863	0.341620	7.565133
-454.655079	0.712344	7.575130
-453.227847	-2.340529	7.585126
-451.268000	3.681428	7.595123
-449.361810	0.503702	7.605120
-447.448542	0.391626	7.615117
-445.525765	-5.457824	7.625114
-443.802245	-0.806632	7.635110
-441.821747	3.522641	7.645107
-439.951175	-3.431566	7.655104
-438.240533	2.902686	7.665101
-436.186537	0.585679	7.675098
-434.296363	4.656172	7.685094
-432.159921	7.385744	7.695091
-430.825620	6.253754	7.705088
-428.950342	8.671253	7.715085
-426.972747	-0.573005	7.725082
-424.845343	0.631802	7.735078
-423.145437	4.908047	7.745075
-421.550850	-0.789452	7.755072
-419.166430	-0.474889	7.765069
-417.632170	-5.898823	7.775066
-415.668360	-2.056742	7.785062
-413.576609	-0.690494	7.795059
-412.078507	-4.048762	7.805056
-409.827949	0.266999	7.815053
-407.922313	-1.682683	7.825050
-405.869433	-2.713062	7.835046
-404.357523	4.150107	7.845043
-402.635461	-2.753317	7.855040
-400.746919	0.520719	7.865037
-398.779427	-4.759372	7.875034
-396.837991	-3.804832	7.885030
-394.886596	0.333824	7.895027
-393.140510	3.897491	7.905024
-391.267643	0.201055	7.915021
-389.484210	2.275472	7.925018
-387.624270	5.904977	7.935014
-385.597789	-0.516334	7.945011
-383.544638	6.134642	7.955008
-381.649197	0.876401	7.965005
-379.749910	-0.254877	7.975002
-378.117687	0.046862	7.984998
-376.344696	-3.928450	7.994995
-374.363255	1.129074	8.004992
-372.282686	-1.871442	8.014989
-370.326252	3.061534	8.024986
-368.749378	-3.850961	8.034982
-366.880605	2.103665	8.044979
-364.847962	1.123412	8.054976
-363.267180	4.049512	8.064973
-361.317974	0.888945	8.074970
-359.469234	-1.728751	8.084966
-357.415001	0.241920	8.094963
-355.306123	1.393423	8.104960
-353.733107	-2.343251	8.114957
-351.920370	2.021561	8.124954
-349.671121	3.611390	8.134950
-348.042601	5.001012	8.144947
-346.286201	1.191384	8.154944
-344.057968	-3.036693	8.164941
-342.790923	-1.085117	8.174938
-340.619270	-0.501233	8.184934
-338.359253	3.886061	8.194931
-337.374610	4.036081	8.204928
-334.955374	6.052441	8.214925
-332.913038	3.609429	8.224922
-330.850854	4.425117	8.234918
-329.456789	7.584819	8.244915
-327.344843	3.814594	8.254912
-325.849022	0.423149	8.264909
-323.683307	-0.071666	8.274906
-321.518038	4.312524	8.284902
-319.767201	4.863870	8.294899
-318.049943	5.577088	8.304896
-316.037269	1.802949	8.314893
-314.296911	13.034411	8.324890
-312.604693	6.468507	8.334886
-310.629359	11.503400	8.344883
-308.671695	14.371596	8.354880
-306.731700	5.304559	8.364877
-304.853093	8.119919	8.374874
-302.854582	0.427682	8.384870
-301.262326	8.456041	8.394867
-299.359072	2.994534	8.404864
-297.329723	-0.415697	8.414861
-295.457523	-1.982959	8.424858
-293.620727	-0.146879	8.434854
-291.596857	4.366707	8.444851
-289.643474	-1.476081	8.454848
-288.287967	1.221523	8.464845
-286.257903	-2.593131	8.474842
-284.241292	-0.555899	8.484838
-282.450195	1.377737	8.494835
-280.917736	-3.132112	8.504832
-278.446528	2.211770	8.514829
-276.480148	-1.479716	8.524826
-274.968999	-1.001062	8.534822
-273.024300	4.040684	8.544819
-271.235183	1.468027	8.554816
-269.145430	-1.368029	8.564813
-267.485157	-7.210330	8.574810
-265.399855	-1.633075	8.584807
-263.485521	0.103957	8.594803
-261.622939	-3.141306	8.604800
-260.093430	-1.617686	8.614797
-257.802852	-6.202624	8.624794
-255.838271	-8.410945	8.634791
-254.530151	0.358976	8.644787
-252.609700	-5.388435	8.654784
-250.299221	-1.541313	8.664781
-248.590165	-3.673002	8.674778
-247.115541	-3.846107	8.684775
-245.124685	-4.041752	8.694771
-242.861532	-0.560778	8.704768
-240.934488	-1.044259	8.714765
-238.946948	-5.072920	8.724762
-237.408978	-0.847076	8.734759
-235.816960	-3.858986	8.744755
-233.375251	1.848048	8.754752
-231.739366	-4.151308	8.764749
-229.721232	-1.842404	8.774746
-227.451517	-4.791117	8.784743
-226.112407	-8.050920	8.794739
-224.276480	-11.772967	8.804736
-222.290315	-6.860039	8.814733
-220.416996	-7.113372	8.824730
-218.286614	-7.300923	8.834727
-216.693204	-3.984090	8.844723
-214.713840	-4.007413	8.854720
-212.987099	-5.006274	8.864717
-211.232820	-6.057677	8.874714
-209.412771	-9.987646	8.884711
-207.161380	-0.300943	8.894707
-205.454998	-4.934265	8.904704
-203.660077	-3.215063	8.914701
-201.715382	-2.860932	8.924698
-199.874661	-15.853564	8.934695
-198.355020	-7.829313	8.944691
-196.301966	-9.134303	8.954688
-193.753497	-4.778223	8.964685
-192.486069	-6.997374	8.974682
-190.174316	-3.207349	8.984679
-188.808709	-8.525621	8.994675
-186.696824	-5.081118	9.004672
-184.772959	-8.117121	9.014669
-183.046778	-10.533116	9.024666
-180.980455	-6.672935	9.034663
-179.077094	-8.183050	9.044659
-177.294442	-8.601429	9.054656
-175.572583	-10.602099	9.064653
-173.478870	-7.732278	9.074650
-171.960372	-7.232323	9.084647
-169.644183	-6.858103	9.094643
-168.099849	-7.001640	9.104640
-165.894930	-9.547157	9.114637
-164.073424	-7.263784	9.124634
-162.541112	-9.944911	9.134631
-160.187142	-2.372389	9.144627
-158.641330	-4.625046	9.154624
-156.775726	-3.988981	9.164621
-154.853964	-6.694211	9.174618
-152.450315	-7.739578	9.184615
-150.849596	-8.157573	9.194611
-149.336524	-4.739989	9.204608
-147.486600	-4.066451	9.214605
-145.524340	-5.964084	9.224602
-143.881978	-8.970370	9.234599
-141.667713	-5.817287	9.244595
-139.740256	-6.158914	9.254592
-137.997727	-10.863623	9.264589
-136.195336	-6.409993	9.274586
-133.870024	-4.383343	9.284583
-132.041507	0.454307	9.294579
-130.540243	-3.144710	9.304576
-128.688042	-1.769257	9.314573
-126.964782	-1.625711	9.324570
-124.431480	6.122386	9.334567
-122.912948	0.660523	9.344563
-120.926807	2.908569	9.354560
-119.076831	5.089068	9.364557
-117.544832	5.896972	9.374554
-115.182847	3.705530	9.384551
-113.148918	2.117325	9.394547
-111.653709	3.455991	9.404544
-109.953769	4.893923	9.414541
-108.035756	-1.112675	9.424538
-106.306083	0.525276	9.434535
-104.187031	2.347813	9.444531
-102.045595	0.106460	9.454528
-100.232710	6.703146	9.464525
-98.611235	4.746196	9.474522
-96.859319	-2.968889	9.484519
-94.623472	3.026469	9.494515
-93.073951	4.543556	9.504512
-90.847428	3.583925	9.514509
-89.222342	0.296853	9.524506
-87.383929	-0.803710	9.534503
-85.483202	3.092031	9.544499
-83.364828	0.238895	9.554496
-81.722700	2.495759	9.564493
-79.772018	3.890705	9.574490
-78.067606	4.482911	9.584487
-75.815869	2.964081	9.594483
-74.151389	3.362761	9.604480
-72.245611	6.560088	9.614477
-70.277643	2.927693	9.624474
-68.329301	-1.072443	9.634471
-66.568922	8.030633	9.644467
-64.745237	5.406674	9.654464
-62.887395	8.449396	9.664461
-61.344815	6.489387	9.674458
-58.992441	4.961608	9.684455
-56.828796	2.787210	9.694451
-55.369310	4.808237	9.704448
-53.866264	4.974554	9.714445
-51.754742	0.910084	9.724442
-49.537412	6.351784	9.734439
-47.870050	2.610486	9.744435
-46.017870	5.689755	9.754432
-43.988559	6.408062	9.764429
-41.990022	-3.289806	9.774426
-40.190726	3.213595	9.784423
-38.977209	3.748502	9.794419
-36.609369	5.545012	9.804416
-34.961941	9.747426	9.814413
-32.948087	3.136732	9.824410
-30.949523	7.380903	9.834407
-28.835454	11.106509	9.844403
-27.237212	2.559777	9.854400
-25.477186	7.865697	9.864397
-23.256093	7.800219	9.874394
-21.378391	15.105916	9.884391
-19.773726	6.391697	9.894387
-17.909201	5.497728	9.904384
-15.997595	6.101067	9.914381
-13.815286	5.812227	9.924378
-12.179971	3.201221	9.934375
-10.189314	0.387800	9.944371
-8.374418	8.456762	9.954368
-6.559664	-1.191404	9.964365
-5.280582	8.606812	9.974362
-3.791357	23.481922	9.984359
-2.613491	69.921924	9.994355
-0.859246	130.556743	10.004352
0.000000	192.039143	10.009357
0.974373	230.650171	10.014362
1.395813	251.755650	10.019367
1.502929	284.627518	10.024371
2.069690	310.745553	10.029376
2.447005	341.212372	10.034381
2.320892	358.435477	10.039386
2.648773	372.346025	10.044391
3.152419	390.631532	10.049395
3.217150	399.792554	10.054400
3.561118	401.505471	10.059405
3.403203	411.493721	10.064410
3.338611	412.543694	10.069415
3.574070	435.633603	10.074419
3.835126	440.120242	10.079424
3.718882	451.520004	10.084429
3.748072	456.228369	10.089434
4.240730	458.334204	10.094439
3.601030	453.673264	10.099443
3.620825	461.245769	10.104448
3.522976	458.867362	10.109453
4.051425	479.459032	10.114458
4.138106	475.544298	10.119463
4.126272	489.876345	10.124467
4.497293	482.795727	10.129472
4.527574	489.696603	10.134477
4.369277	490.493447	10.139482
4.549594	495.425377	10.144487
4.318411	500.301554	10.149491
4.417990	499.108196	10.154496
4.734434	498.160276	10.159501
4.540350	507.050352	10.164506
4.692566	500.583145	10.169511
4.475352	499.029645	10.174515
4.447632	511.483183	10.179520
4.321597	511.447944	10.184525
4.601804	506.782413	10.189530
5.163849	506.588934	10.194535
5.254321	515.350096	10.199539
5.551322	507.985327	10.204544
5.464317	514.161875	10.209549
5.077071	513.959062	10.214554
5.416172	511.518753	10.219559
5.298055	523.671626	10.224563
5.421405	518.497346	10.229568
5.394402	522.976954	10.234573
5.195575	526.558422	10.239578
5.272474	519.847550	10.244583
5.109679	522.171959	10.249587
5.326127	525.697618	10.254592
5.404667	527.070809	10.259597
5.399560	531.530481	10.264602
5.580069	524.161600	10.269607
5.523964	534.454567	10.274611
5.190086	543.726649	10.279616
5.352537	537.609766	10.284621
5.273935	545.309705	10.289626
5.547792	551.069142	10.294631
5.733624	568.789634	10.299635
5.629013	570.889343	10.304640
5.849048	578.432308	10.309645
5.716459	578.555688	10.314650
5.738677	575.249203	10.319655
5.687617	583.665207	10.324659
5.968551	579.661880	10.329664
5.902546	584.132798	10.334669
5.696151	596.777299	10.339674
6.376250	608.644564	10.344679
6.215781	610.166504	10.349683
6.368194	619.099073	10.354688
6.263837	618.090668	10.359693
6.225872	627.006149	10.364698
6.408699	622.693587	10.369703
6.002251	616.183178	10.374707
6.221412	619.765628	10.379712
6.155219	620.996674	10.384717
6.291635	629.661605	10.389722
6.447831	628.378399	10.394727
6.469744	654.044919	10.399731
6.718556	659.312913	10.404736
7.130439	674.099044	10.409741
6.537028	664.475479	10.414746
7.044080	654.233771	10.419751
6.883710	672.262813	10.424755
6.836507	667.785606	10.429760
6.911403	673.720514	10.434765
7.002968	669.134647	10.439770
6.776398	661.892340	10.444775
6.679304	676.467329	10.449779
6.769723	669.133563	10.454784
6.885082	671.582008	10.459789
6.541348	673.039062	10.464794
7.099980	687.316503	10.469799
7.200288	701.678857	10.474803
7.003810	700.576113	10.479808
6.928136	698.875168	10.484813
7.012501	712.406599	10.489818
7.383768	716.655347	10.494823
7.455008	731.493229	10.499827
7.291618	735.356031	10.504832
7.868424	743.885122	10.509837
8.076771	751.202022	10.514842
8.162925	744.245129	10.519847
7.925842	733.386499	10.524851
7.391735	719.436366	10.529856
7.936327	731.765504	10.534861
8.085903	743.239110	10.539866
8.029212	739.362314	10.544871
7.637123	746.328223	10.549875
7.614532	751.970408	10.554880
8.182932	757.540079	10.559885
7.967849	759.318498	10.564890
8.419165	755.047495	10.569895
8.020014	763.101314	10.574899
8.096465	754.987942	10.579904
8.228953	752.467761	10.584909
7.901596	758.578644	10.589914
8.874518	757.656305	10.594919
8.624501	762.709079	10.599923
8.463408	757.965194	10.604928
8.352705	767.690581	10.609933
7.976185	771.247309	10.614938
8.236186	775.581860	10.619943
8.282099	794.999467	10.624947
8.399344	799.718102	10.629952
8.619191	804.026783	10.634957
8.537777	814.704400	10.639962
8.841022	801.252060	10.644967
8.725508	810.738301	10.649971
8.988099	811.791412	10.654976
8.970298	814.342447	10.659981
8.452085	812.024219	10.664986
8.719022	820.106357	10.669991
8.885736	846.136781	10.674995
9.215338	841.442945	10.680000
9.706866	846.727017	10.685005
9.471897	851.241982	10.690010
9.716602	824.296660	10.695015
9.493750	825.030379	10.700019
9.558585	818.339211	10.705024
9.623665	817.366083	10.710029
9.501071	824.604367	10.715034
9.483971	814.720054	10.720039
9.148088	825.896830	10.725043
9.516507	817.009427	10.730048
9.504231	825.443386	10.735053
9.537722	830.045734	10.740058
9.699750	838.671653	10.745063
9.654369	855.299232	10.750067
9.603215	855.846015	10.755072
9.978546	863.236967	10.760077
9.891773	866.976534	10.765082
9.951400	867.377614	10.770087
10.051620	865.697807	10.775091
9.779799	861.658922	10.780096
9.735920	860.473950	10.785101
9.471916	859.647243	10.790106
9.750778	851.908059	10.795111
10.049073	861.654165	10.800115
9.846739	869.260218	10.805120
10.214033	881.621454	10.810125
10.381929	885.201309	10.815130
10.423985	876.985614	10.820135
10.421265	885.676911	10.825139
10.274094	882.261247	10.830144
10.365453	886.800006	10.835149
10.042806	885.447700	10.840154
10.892758	880.573451	10.845159
10.590775	886.513060	10.850163
10.908520	884.252407	10.855168
10.704785	881.965511	10.860173
10.492808	897.291843	10.865178
10.404927	881.087705	10.870183
10.638930	888.458296	10.875187
10.603812	892.739271	10.880192
10.971195	897.280048	10.885197
10.586757	916.509096	10.890202
11.250040	915.762998	10.895207
11.104600	923.338005	10.900211
11.148101	916.777557	10.905216
10.942544	921.576444	10.910221
11.075835	923.929882	10.915226
11.080948	924.277547	10.920231
10.749732	927.096284	10.925235
10.855128	925.103744	10.930240
11.206741	925.988836	10.935245
11.118337	939.887980	10.940250
11.815297	943.539371	10.945255
11.142775	947.239654	10.950259
11.294648	949.469120	10.955264
11.339866	961.291962	10.960269
11.123192	969.638281	10.965274
11.477379	970.629119	10.970279
11.323464	961.410800	10.975283
11.399947	967.026997	10.980288
11.671651	969.655524	10.985293
11.263417	994.663727	10.990298
12.125203	994.933193	10.995303
11.952588	994.827782	11.000307
12.339760	994.217048	11.005312
12.259774	991.034972	11.010317
12.052485	993.329184	11.015322
12.552213	997.094142	11.020327
12.385611	978.105117	11.025331
12.593649	967.479476	11.030336
12.400632	966.568750	11.035341
12.159244	965.908685	11.040346
12.543309	962.638365	11.045351
12.404096	964.460639	11.050355
12.548657	960.952701	11.055360
12.435644	966.165206	11.060365
12.390723	966.558161	11.065370
12.200733	965.706916	11.070375
12.577923	978.619557	11.075379
12.198001	987.797163	11.080384
12.504973	1001.383440	11.085389
12.307350	1001.366000	11.090394
12.666141	997.626322	11.095399
12.664333	1003.014377	11.100403
12.596436	1002.979432	11.105408
12.798771	1004.678018	11.110413
12.229487	1006.360879	11.115418
12.758819	1012.523920	11.120423
12.694288	1037.021286	11.125427
13.012200	1037.717559	11.130432
13.411077	1030.267973	11.135437
13.295272	1025.614136	11.140442
13.368885	1033.818349	11.145447
13.549244	1033.576232	11.150451
13.534888	1030.585395	11.155456
13.560374	1019.766018	11.160461
13.415264	1032.284704	11.165466
13.821563	1025.283848	11.170471
13.628340	1033.493154	11.175475
13.741469	1029.077564	11.180480
13.607749	1011.523649	11.185485
13.549607	1010.162690	11.190490
13.324224	1007.354882	11.195495
13.369880	1027.162821	11.200499
13.625675	1028.433428	11.205504
13.821142	1031.089247	11.210509
13.566877	1036.320468	11.215514
13.780564	1040.203955	11.220519
13.835305	1041.280877	11.225523
13.801266	1037.199202	11.230528
14.176574	1038.713003	11.235533
13.890524	1035.718617	11.240538
14.100385	1046.361057	11.245543
13.622802	1045.727275	11.250547
14.130190	1046.061850	11.255552
14.083862	1049.706500	11.260557
14.567478	1063.154780	11.265562
14.672154	1060.335371	11.270567
14.504413	1052.840030	11.275571
13.952836	1050.271696	11.280576
14.507883	1056.083371	11.285581
14.267010	1064.087310	11.290586
14.443951	1069.505924	11.295591
14.388811	1077.692762	11.300595
14.778174	1073.290192	11.305600
14.298610	1071.011876	11.310605
14.171505	1078.513156	11.315610
14.940542	1073.089037	11.320615
14.997550	1074.257547	11.325619
14.859595	1072.408950	11.330624
14.658642	1065.419036	11.335629
14.511530	1074.881645	11.340634
14.370867	1070.729427	11.345639
14.741162	1078.239371	11.350643
15.158147	1094.136216	11.355648
15.506751	1089.021811	11.360653
14.971631	1096.752532	11.365658
15.302216	1094.270963	11.370663
15.572148	1100.555096	11.375667
15.353629	1099.836630	11.380672
15.331847	1092.559403	11.385677
15.931188	1086.048055	11.390682
15.869307	1072.890981	11.395687
15.729293	1068.555494	11.400691
15.549759	1062.749280	11.405696
15.570547	1065.616635	11.410701
15.238439	1072.656482	11.415706
15.574692	1061.748662	11.420711
15.398064	1070.600538	11.425715
15.318194	1072.528308	11.430720
15.694517	1080.196695	11.435725
15.631424	1098.830472	11.440730
15.758908	1101.179011	11.445735
15.667436	1104.345491	11.450739
15.814938	1107.278365	11.455744
15.810815	1111.207899	11.460749
15.760528	1106.434251	11.465754
16.032668	1101.366111	11.470759
15.955538	1106.187639	11.475763
15.994352	1110.095207	11.480768
15.874414	1116.345928	11.485773
16.000556	1127.776466	11.490778
16.292966	1133.322937	11.495783
16.596222	1140.056111	11.500787
16.563794	1137.376249	11.505792
16.670639	1131.752225	11.510797
16.310460	1133.267403	11.515802
16.805684	1128.497717	11.520807
16.567776	1124.957030	11.525811
16.501591	1113.516197	11.530816
16.642388	1114.754818	11.535821
16.639722	1132.975641	11.540826
17.020827	1128.118942	11.545831
16.557767	1133.340600	11.550835
16.969757	1139.513548	11.555840
16.774038	1144.771083	11.560845
16.417846	1146.172683	11.565850
16.863695	1146.693866	11.570855
16.730734	1146.887577	11.575859
16.749218	1145.557679	11.580864
17.040307	1144.777492	11.585869
16.662873	1154.014374	11.590874
16.976866	1137.913566	11.595879
16.628649	1143.889621	11.600883
16.948120	1158.252318	11.605888
17.487861	1166.287468	11.610893
17.172365	1172.660164	11.615898
17.389157	1173.126279	11.620903
17.181760	1175.255139	11.625907
17.460500	1168.520040	11.630912
17.798082	1168.098990	11.635917
17.395720	1176.659627	11.640922
17.876140	1165.010167	11.645927
17.759290	1170.425110	11.650931
17.985119	1167.932675	11.655936
17.857398	1164.510061	11.660941
17.392197	1163.682702	11.665946
18.013245	1171.705888	11.670951
17.774120	1166.963415	11.675955
17.606317	1170.451288	11.680960
17.703337	1171.064255	11.685965
17.788826	1178.256367	11.690970
17.823521	1172.386934	11.695975
17.797489	1171.388748	11.700979
17.727321	1188.887783	11.705984
18.385179	1193.200815	11.710989
18.085057	1209.594551	11.715994
18.485187	1205.229967	11.720999
18.143756	1208.608669	11.726003
18.222471	1204.440117	11.731008
18.483417	1205.606039	11.736013
18.283660	1208.169783	11.741018
18.599111	1199.314536	11.746023
18.116708	1205.966918	11.751027
18.463957	1208.521349	11.756032
18.929712	1200.676132	11.761037
18.507386	1205.201611	11.766042
18.834957	1198.807472	11.771047
18.740812	1200.094278	11.776051
19.113501	1201.108407	11.781056
19.545985	1207.954456	11.786061
18.735798	1221.403256	11.791066
18.985432	1202.866807	11.796071
18.877231	1205.428274	11.801075
18.988328	1210.022954	11.806080
19.021284	1204.225650	11.811085
18.730741	1210.110524	11.816090
18.842687	1206.210224	11.821095
18.970776	1214.532298	11.826099
19.225953	1214.349589	11.831104
19.205949	1210.304542	11.836109
18.650595	1222.084104	11.841114
19.384922	1220.747122	11.846119
19.504126	1235.325020	11.851123
19.627850	1233.281929	11.856128
19.706838	1233.826938	11.861133
19.778912	1231.232564	11.866138
19.794255	1224.570235	11.871143
19.794262	1221.120577	11.876147
19.759143	1208.099329	11.881152
19.572444	1205.614460	11.886157
19.714731	1209.405626	11.891162
19.827959	1214.936269	11.896167
19.849272	1215.728010	11.901171
20.020825	1231.241546	11.906176
19.717332	1231.435680	11.911181
19.577112	1230.449569	11.916186
20.040616	1242.519067	11.921191
19.988432	1232.768796	11.926195
20.268112	1221.090950	11.931200
20.519236	1224.808984	11.936205
20.262089	1230.387346	11.941210
20.524791	1227.295283	11.946215
20.442679	1221.562702	11.951219
20.366502	1229.904413	11.956224
20.568707	1220.920937	11.961229
20.252817	1211.224183	11.966234
20.434819	1220.036760	11.971239
20.326761	1226.864969	11.976243
20.385554	1226.132897	11.981248
20.552641	1225.987397	11.986253
20.459150	1229.967416	11.991258
20.762748	1218.894557	11.996263
20.740908	1227.721957	12.001267
20.631297	1225.209657	12.006272
20.861282	1223.313745	12.011277
20.514544	1228.477989	12.016282
21.048137	1223.258401	12.021287
20.691283	1233.497998	12.026291
20.623114	1225.861157	12.031296
21.028340	1220.672659	12.036301
20.563783	1231.830337	12.041306
20.832269	1222.858786	12.046311
20.893263	1229.362350	12.051315
20.778187	1230.805906	12.056320
20.867119	1242.715020	12.061325
20.644819	1240.987049	12.066330
20.811932	1234.395405	12.071335
20.924969	1238.936866	12.076339
20.610871	1234.692760	12.081344
21.208565	1230.865092	12.086349
20.664011	1235.721803	12.091354
21.261805	1235.586930	12.096359
20.899558	1231.570951	12.101363
21.105312	1236.114673	12.106368
20.875055	1235.549793	12.111373
20.649485	1242.780663	12.116378
20.914900	1238.942464	12.121383
21.270257	1242.356048	12.126387
20.788170	1222.727649	12.131392
21.044671	1214.454482	12.136397
20.767200	1212.861897	12.141402
21.021322	1210.918032	12.146407
20.838601	1209.930524	12.151411
20.698570	1206.736199	12.156416
20.901417	1204.951128	12.161421
20.792745	1207.583334	12.166426
21.110156	1206.337969	12.171431
20.874544	1209.400892	12.176435
20.928874	1214.789659	12.181440
21.042782	1200.389296	12.186445
20.833895	1204.930285	12.191450
20.740946	1201.359199	12.196455
20.753264	1208.570977	12.201459
20.698037	1205.834616	12.206464
21.052432	1204.617647	12.211469
20.412627	1214.273369	12.216474
20.611270	1204.121290	12.221479
20.562877	1211.051764	12.226483
20.778315	1206.689241	12.231488
21.056472	1200.684499	12.236493
20.656804	1218.607962	12.241498
20.875073	1206.911839	12.246503
21.142077	1215.723655	12.251507
20.819109	1212.424508	12.256512
20.962186	1222.548775	12.261517
20.678979	1214.269460	12.266522
21.221639	1218.058692	12.271527
20.806771	1218.163368	12.276531
20.607477	1223.546281	12.281536
20.870057	1211.990190	12.286541
20.407781	1210.561924	12.291546
20.803646	1215.551076	12.296551
21.062244	1223.804989	12.301555
20.794810	1216.775878	12.306560
21.247412	1215.893390	12.311565
20.926525	1215.366945	12.316570
21.368619	1217.752745	12.321575
21.356767	1210.646263	12.326579
20.840323	1201.585487	12.331584
21.245746	1190.972037	12.336589
20.472313	1196.456932	12.341594
20.711192	1183.807941	12.346599
20.485273	1191.246480	12.351603
20.553403	1189.823197	12.356608
20.430886	1191.007101	12.361613
20.293334	1215.772271	12.366618
21.189607	1218.481257	12.371623
21.111505	1228.136602	12.376627
20.827002	1226.306007	12.381632
21.094372	1219.346254	12.386637
20.881291	1215.504049	12.391642
20.900080	1193.207409	12.396647
20.595609	1199.046114	12.401651
20.473544	1191.055764	12.406656
21.038659	1206.313505	12.411661
20.549367	1208.495834	12.416666
21.275882	1210.196544	12.421671
20.606021	1204.841851	12.426675
20.896319	1192.616278	12.431680
21.148350	1190.636063	12.436685
20.601488	1192.583916	12.441690
21.141664	1188.762173	12.446695
20.777310	1194.666802	12.451699
21.057484	1198.422086	12.456704
20.960801	1186.413265	12.461709
20.451903	1194.113879	12.466714
20.692657	1191.759409	12.471719
20.672887	1197.610485	12.476723
20.458324	1190.087974	12.481728
20.553285	1183.731751	12.486733
20.599869	1204.540424	12.491738
20.832845	1219.096037	12.496743
20.962568	1219.659188	12.501747
20.882984	1216.663709	12.506752
21.103747	1201.669887	12.511757
20.657284	1206.396874	12.516762
21.258169	1199.496790	12.521767
20.652209	1195.675372	12.526771
20.305193	1195.014459	12.531776
20.714615	1196.441900	12.536781
20.715320	1221.889961	12.541786
20.857436	1230.105822	12.546791
20.843374	1233.396425	12.551795
21.013112	1226.832756	12.556800
20.850731	1204.639400	12.561805
20.363683	1201.499442	12.566810
21.077576	1209.509098	12.571815
20.689688	1210.224946	12.576819
20.522594	1218.879479	12.581824
20.860735	1218.102275	12.586829
20.890615	1230.420982	12.591834
21.103223	1226.821580	12.596839
20.827517	1217.428989	12.601843
20.751199	1210.125137	12.606848
20.540451	1211.238117	12.611853
20.367321	1224.714272	12.616858
20.964706	1236.570151	12.621863
20.736960	1232.360583	12.626867
20.761959	1239.101246	12.631872
20.942206	1231.991818	12.636877
21.372409	1241.821338	12.641882
21.491307	1223.385439	12.646887
21.291810	1212.255948	12.651891
20.568734	1210.641079	12.656896
20.995956	1208.485954	12.661901
21.235133	1211.405893	12.666906
21.362286	1207.212456	12.671911
21.111999	1204.318880	12.676915
21.100358	1202.818482	12.681920
21.101213	1185.751303	12.686925
20.583036	1185.884350	12.691930
20.762019	1182.613227	12.696935
20.693805	1184.174666	12.701939
20.601433	1184.376024	12.706944
20.594134	1179.822353	12.711949
20.566623	1193.558912	12.716954
20.973732	1201.215370	12.721959
20.605188	1205.139121	12.726963
20.748146	1202.788391	12.731968
20.917251	1206.955883	12.736973
20.718050	1209.795061	12.741978
20.788073	1208.386057	12.746983
20.711496	1210.605388	12.751987
20.601298	1205.778034	12.756992
20.911108	1208.520859	12.761997
20.370538	1210.706454	12.767002
20.604822	1208.224011	12.772007
20.721186	1214.610311	12.777011
20.503897	1224.192412	12.782016
21.055780	1211.124201	12.787021
20.758674	1219.418127	12.792026
21.037163	1214.031884	12.797031
20.819428	1214.197104	12.802035
20.871111	1203.253897	12.807040
20.902315	1204.915925	12.812045
20.706947	1212.359895	12.817050
20.630197	1205.230594	12.822055
20.938982	1208.244783	12.827059
20.842159	1208.622169	12.832064
21.309215	1209.706962	12.837069
20.609007	1213.008626	12.842074
20.803817	1210.587030	12.847079
20.881821	1207.977827	12.852083
20.613596	1211.278451	12.857088
21.152253	1215.846010	12.862093
20.996298	1216.914069	12.867098
20.846177	1214.750169	12.872103
20.914106	1212.829543	12.877107
21.084317	1208.593196	12.882112
21.120598	1195.195765	12.887117
20.989087	1193.346048	12.892122
21.510252	1188.697819	12.897127
21.224839	1200.099105	12.902131
20.919614	1189.298418	12.907136
21.060630	1187.167894	12.912141
20.952356	1195.603907	12.917146
21.014845	1194.077379	12.922151
21.207917	1188.841975	12.927155
20.868678	1165.023456	12.932160
20.358700	1160.744270	12.937165
20.332012	1176.276346	12.942170
20.731898	1182.861523	12.947175
20.878240	1196.368932	12.952179
20.720027	1191.087573	12.957184
20.918448	1188.799967	12.962189
20.749766	1190.090473	12.967194
20.616917	1187.224923	12.972199
20.322059	1189.873260	12.977203
20.511886	1192.755866	12.982208
20.802448	1192.945252	12.987213
20.354692	1196.429419	12.992218
20.818194	1193.287144	12.997223
20.738773	1197.572641	13.002227
20.648186	1198.914100	13.007232
20.632561	1192.878021	13.012237
20.616294	1191.820922	13.017242
20.917037	1200.772999	13.022247
20.443253	1196.117330	13.027251
20.624922	1193.581936	13.032256
20.794402	1198.941480	13.037261
20.644194	1220.616820	13.042266
21.283258	1218.021156	13.047271
21.340430	1207.250297	13.052275
20.785284	1191.153584	13.057280
20.979298	1189.615558	13.062285
20.979879	1190.903884	13.067290
20.689355	1186.662065	13.072295
20.650236	1197.162953	13.077299
20.554768	1195.327188	13.082304
20.793260	1196.880253	13.087309
20.772548	1205.601656	13.092314
21.017564	1196.308482	13.097319
21.017940	1199.989370	13.102323
20.753030	1196.985407	13.107328
21.001187	1202.317252	13.112333
20.537767	1205.025282	13.117338
21.136697	1201.565703	13.122343
20.898773	1204.128096	13.127347
21.034985	1203.349198	13.132352
21.057193	1203.905914	13.137357
20.956145	1204.116259	13.142362
20.977130	1194.352677	13.147367
20.762331	1202.403533	13.152371
20.712362	1208.358080	13.157376
20.799424	1198.113030	13.162381
20.702144	1200.944205	13.167386
20.923270	1197.734143	13.172391
20.641896	1195.968543	13.177395
20.583117	1196.850990	13.182400
21.124484	1201.798216	13.187405
20.571303	1201.465944	13.192410
20.571340	1204.698860	13.197415
20.858606	1213.246672	13.202419
20.843875	1203.453286	13.207424
20.952083	1200.094029	13.212429
20.787434	1207.286016	13.217434
20.632474	1205.726111	13.222439
20.687143	1199.067707	13.227443
20.664700	1195.514140	13.232448
20.877353	1190.244984	13.237453
20.792654	1203.167927	13.242458
20.832542	1206.410984	13.247463
20.664229	1201.535174	13.252467
20.725364	1205.583808	13.257472
20.825965	1206.059977	13.262477
20.894689	1209.662438	13.267482
20.999055	1202.992749	13.272487
20.906424	1203.265994	13.277491
20.809857	1207.900621	13.282496
21.136658	1207.165625	13.287501
20.995365	1207.002735	13.292506
20.682316	1205.814939	13.297511
20.579126	1214.077983	13.302515
20.451015	1210.442265	13.307520
21.166913	1209.486212	13.312525
20.940023	1217.115985	13.317530
21.089027	1209.449417	13.322535
21.043786	1219.133860	13.327539
20.353251	1205.378663	13.332544
20.711037	1203.828346	13.337549
20.354019	1211.273583	13.342554
20.872246	1210.433133	13.347559
20.698056	1204.370158	13.352563
20.772264	1214.720572	13.357568
20.974827	1207.119429	13.362573
20.574249	1218.091652	13.367578
20.796778	1206.026505	13.372583
21.394763	1216.817254	13.377587
20.831450	1218.059370	13.382592
21.136802	1209.775856	13.387597
20.403492	1218.541287	13.392602
20.551156	1212.905498	13.397607
20.843314	1216.603863	13.402611
20.986892	1213.154460	13.407616
21.022031	1210.136943	13.412621
20.753841	1218.029985	13.417626
20.742577	1215.638590	13.422631
20.839349	1211.825365	13.427635
20.877510	1222.170123	13.432640
21.191191	1214.241236	13.437645
20.749718	1196.349874	13.442650
20.719537	1185.939011	13.447655
20.766072	1191.765294	13.452659
20.603767	1198.610292	13.457664
21.042483	1213.001149	13.462669
20.627232	1214.807622	13.467674
20.836713	1212.101665	13.472679
21.005662	1215.064435	13.477683
20.775494	1201.870185	13.482688
21.011812	1191.660337	13.487693
20.717683	1194.001836	13.492698
20.640694	1181.948588	13.497703
21.054589	1186.691084	13.502707
20.977573	1186.211644	13.507712
21.167568	1178.750038	13.512717
20.649816	1188.010999	13.517722
20.876366	1176.102293	13.522727
20.557419	1174.880379	13.527731
20.279110	1179.684713	13.532736
20.467654	1190.759595	13.537741
20.830042	1209.307921	13.542746
20.783632	1209.871271	13.547751
20.873831	1213.774396	13.552755
20.833535	1217.566868	13.557760
21.172628	1217.430956	13.562765
20.686065	1200.900495	13.567770
20.460437	1185.472429	13.572775
20.907979	1196.901201	13.577779
20.678050	1212.819480	13.582784
20.921219	1216.898091	13.587789
21.419919	1216.651917	13.592794
20.568021	1203.902954	13.597799
21.002714	1186.903890	13.602803
20.582099	1181.461865	13.607808
20.717626	1184.924180	13.612813
20.539373	1199.595284	13.617818
20.718032	1206.585511	13.622823
20.894801	1219.964959	13.627827
20.546799	1232.009770	13.632832
20.630394	1218.046042	13.637837
20.296478	1225.569431	13.642842
20.446521	1217.769258	13.647847
20.686926	1234.364426	13.652851
20.982796	1225.551206	13.657856
20.896291	1216.541839	13.662861
20.807870	1230.940987	13.667866
21.009570	1222.563132	13.672871
21.309039	1229.762791	13.677875
21.227260	1226.727422	13.682880
20.815974	1216.440698	13.687885
20.540663	1207.891213	13.692890
20.752735	1213.592410	13.697895
20.479758	1221.370221	13.702899
20.639745	1230.702111	13.707904
20.894805	1219.806917	13.712909
21.047613	1226.080788	13.717914
21.273894	1218.264780	13.722919
21.192592	1214.347479	13.727923
20.643585	1200.322887	13.732928
20.964859	1188.097138	13.737933
20.836278	1198.149150	13.742938
20.888064	1193.936665	13.747943
21.024550	1186.335413	13.752947
20.635471	1190.456498	13.757952
20.865355	1188.392843	13.762957
20.391448	1195.458242	13.767962
20.622402	1193.214006	13.772967
20.786883	1199.262046	13.777971
20.684458	1189.064490	13.782976
20.562092	1200.913089	13.787981
20.574170	1222.904821	13.792986
20.811312	1225.062075	13.797991
21.072827	1223.128784	13.802995
20.857924	1234.701165	13.808000
21.104994	1221.816656	13.813005
20.321597	1216.768403	13.818010
20.594155	1217.964704	13.823015
20.815426	1228.951500	13.828019
20.751156	1228.862642	13.833024
21.132827	1233.893312	13.838029
20.763445	1234.440985	13.843034
21.059579	1230.514231	13.848039
20.951359	1219.165792	13.853043
20.774481	1205.481606	13.858048
20.850322	1200.383537	13.863053
20.766607	1197.400218	13.868058
20.827493	1190.773121	13.873063
20.585054	1198.413840	13.878067
20.381588	1203.070348	13.883072
21.022873	1211.844831	13.888077
20.620377	1222.999362	13.893082
21.080245	1226.806739	13.898087
21.519845	1222.718808	13.903091
21.241600	1213.327839	13.908096
21.518736	1199.740685	13.913101
20.923196	1204.478627	13.918106
20.757603	1192.278719	13.923111
20.770999	1197.055939	13.928115
20.913369	1200.241555	13.933120
20.819569	1191.553983	13.938125
20.697790	1198.667956	13.943130
20.837949	1198.636811	13.948135
20.876478	1198.332167	13.953139
20.676411	1198.157644	13.958144
20.979980	1191.775518	13.963149
20.867053	1192.043559	13.968154
20.895781	1198.420009	13.973159
20.917279	1198.449473	13.978163
20.542214	1196.716121	13.983168
20.695662	1191.607117	13.988173
20.747471	1200.976484	13.993178
20.993322	1197.306257	13.998183
20.618907	1196.349249	14.003187
20.534654	1199.947147	14.008192
20.843132	1200.612416	14.013210
20.900197	1205.148679	14.018227
20.571622	1209.204167	14.023245
20.912199	1202.151861	14.028263
21.106625	1197.326772	14.033280
20.932604	1203.200797	14.038298
20.858850	1207.344101	14.043315
20.841268	1198.917256	14.048333
21.134140	1197.679137	14.053351
20.724423	1213.153052	14.058368
21.235162	1197.531473	14.063386
21.132036	1205.754962	14.068403
20.849991	1201.622247	14.073421
20.993617	1204.425019	14.078439
20.926650	1200.521199	14.083456
21.085659	1202.864995	14.088474
20.663240	1208.025248	14.093491
20.944095	1197.671484	14.098509
20.868622	1203.941247	14.103527
20.633014	1204.704925	14.108544
20.927131	1209.409618	14.113562
20.593037	1227.258974	14.118579
20.706271	1233.768464	14.123597
20.950169	1234.513714	14.128615
21.045567	1243.761150	14.133632
21.047957	1237.348360	14.138650
21.208428	1239.233997	14.143667
21.128656	1235.080373	14.148685
21.040279	1233.099281	14.153703
21.072472	1235.215985	14.158720
21.240443	1229.252409	14.163738
21.104783	1248.742321	14.168755
21.150802	1256.912309	14.173773
21.616884	1264.058226	14.178791
21.392373	1272.773076	14.183808
21.851778	1261.116102	14.188826
21.607874	1275.727717	14.193843
21.118858	1251.891316	14.198861
21.666913	1254.189676	14.203879
21.240054	1268.471991	14.208896
21.552256	1264.788996	14.213914
21.673660	1267.708198	14.218931
21.791872	1265.558204	14.223949
22.150873	1269.100113	14.228967
21.718343	1259.058404	14.233984
22.121167	1243.337162	14.239002
21.788138	1257.973097	14.244019
21.821569	1253.740999	14.249037
21.799837	1243.932829	14.254055
21.806277	1245.443267	14.259072
21.864593	1241.533705	14.264090
21.483943	1239.007396	14.269107
21.783973	1244.500526	14.274125
21.781373	1242.453146	14.279143
21.594904	1234.750968	14.284160
21.866088	1239.372981	14.289178
21.959087	1242.828591	14.294195
21.435629	1250.725712	14.299213
21.959994	1243.701723	14.304231
21.902923	1254.363225	14.309248
21.654007	1243.813624	14.314266
21.775443	1246.204423	14.319283
21.840744	1247.209450	14.324301
21.920225	1250.057483	14.329319
21.540855	1261.728270	14.334336
22.021400	1245.683830	14.339354
21.953246	1252.686673	14.344371
21.754194	1256.219528	14.349389
21.926028	1262.459117	14.354407
21.735707	1273.695890	14.359424
21.962148	1269.256663	14.364442
21.926793	1269.224130	14.369459
22.044569	1284.831316	14.374477
22.514520	1278.448588	14.379495
21.815983	1286.861222	14.384512
22.172818	1282.181505	14.389530
21.794749	1279.420080	14.394547
21.761730	1277.285383	14.399565
22.081650	1279.965414	14.404583
21.659514	1282.615968	14.409600
21.805285	1290.157792	14.414618
21.860249	1302.511689	14.419635
21.853774	1312.885396	14.424653
22.349786	1308.718866	14.429671
22.212386	1316.942383	14.434688
22.532773	1311.567267	14.439706
22.368269	1309.248791	14.444723
22.019377	1314.844545	14.449741
22.600835	1302.646093	14.454759
22.193621	1308.569983	14.459776
22.598461	1301.779081	14.464794
22.314339	1309.099319	14.469811
22.580714	1302.475083	14.474829
22.801138	1300.124078	14.479847
22.499080	1311.930874	14.484864
22.669111	1306.363409	14.489882
22.532829	1303.146706	14.494899
22.368387	1310.642506	14.499917
22.711409	1305.482429	14.504935
22.315321	1314.360590	14.509952
22.329496	1310.384558	14.514970
22.781603	1312.025694	14.519987
22.815795	1307.279624	14.525005
23.065776	1306.482749	14.530023
22.495731	1313.698849	14.535040
23.053940	1302.216654	14.540058
23.051011	1309.774927	14.545075
22.900432	1311.763121	14.550093
22.950630	1305.293283	14.555111
22.836335	1312.861596	14.560128
22.574099	1307.472192	14.565146
23.322146	1312.416439	14.570163
22.925555	1310.711431	14.575181
23.190287	1306.418005	14.580199
22.919994	1307.961327	14.585216
23.069858	1299.237584	14.590234
22.861291	1303.444582	14.595251
22.442574	1310.499290	14.600269
22.657188	1307.684670	14.605287
22.706934	1311.167004	14.610304
22.645757	1308.237845	14.615322
23.134553	1317.882484	14.620339
22.689747	1332.988483	14.625357
23.346836	1332.427345	14.630375
23.048588	1346.927466	14.635392
23.164760	1341.478288	14.640410
23.144538	1341.205343	14.645427
23.293151	1345.401117	14.650445
23.703789	1337.979224	14.655463
23.657766	1331.419957	14.660480
23.073183	1313.207458	14.665498
23.038457	1308.385794	14.670515
23.077682	1313.909097	14.675533
23.439884	1319.955424	14.680551
23.220037	1321.601527	14.685568
22.884459	1323.477728	14.690586
23.389347	1335.266275	14.695603
23.453576	1338.216161	14.700621
23.823075	1338.800498	14.705639
23.144061	1335.361066	14.710656
23.309727	1333.051731	14.715674
23.495787	1337.711599	14.720691
23.374646	1337.118524	14.725709
23.563343	1332.030571	14.730727
23.109980	1342.045446	14.735744
23.642829	1334.158071	14.740762
23.826987	1336.906275	14.745779
23.532918	1344.435341	14.750797
23.419266	1339.045649	14.755815
23.669942	1347.262492	14.760832
23.565330	1340.958172	14.765850
23.623479	1337.142325	14.770867
23.437992	1337.694640	14.775885
23.685370	1342.760571	14.780903
23.703582	1347.366929	14.785920
23.585169	1338.325741	14.790938
23.333146	1329.442519	14.795955
23.282440	1336.052608	14.800973
23.745950	1344.068770	14.805991
23.611287	1367.797247	14.811008
23.867544	1370.913447	14.816026
24.116903	1369.942249	14.821043
23.905548	1375.016757	14.826061
24.109231	1373.747062	14.831079
23.840352	1372.826526	14.836096
24.036390	1376.589333	14.841114
24.004153	1369.915865	14.846131
24.097875	1376.112981	14.851149
23.954990	1364.364297	14.856167
23.861318	1359.699588	14.861184
24.004792	1369.126669	14.866202
23.907275	1365.652496	14.871219
24.077014	1372.674059	14.876237
24.587030	1365.352448	14.881255
24.211442	1372.244262	14.886272
24.303881	1366.165225	14.891290
24.617149	1346.016292	14.896307
24.198028	1343.131173	14.901325
24.567280	1336.421955	14.906343
24.273356	1334.942277	14.911360
23.822765	1334.362378	14.916378
24.111132	1333.566400	14.921395
23.868282	1340.184236	14.926413
24.432888	1355.445170	14.931431
24.186080	1365.022637	14.936448
23.926251	1363.493012	14.941466
24.089155	1362.495689	14.946483
23.850565	1369.209273	14.951501
24.148373	1363.534831	14.956519
24.147909	1364.962598	14.961536
23.841951	1364.779986	14.966554
24.514594	1382.360047	14.971571
24.078959	1399.702943	14.976589
24.497248	1399.864310	14.981607
24.676092	1400.279350	14.986624
24.440400	1394.612503	14.991642
24.708291	1400.395478	14.996659
24.356420	1402.509544	15.001677
24.527586	1395.703936	15.006695
24.677234	1394.659273	15.011712
24.704813	1391.624320	15.016730
24.622633	1396.388470	15.021747
24.727060	1395.634658	15.026765
24.779242	1389.994841	15.031783
24.571652	1393.677629	15.036800
24.769901	1394.730743	15.041818
24.991330	1390.542760	15.046835
25.157334	1401.305497	15.051853
25.337359	1393.701837	15.056871
25.476659	1392.519565	15.061888
25.340432	1390.494683	15.066906
25.359023	1390.532042	15.071923
25.422916	1377.055604	15.076941
25.150088	1359.266810	15.081959
25.108519	1355.546803	15.086976
25.256865	1356.954960	15.091994
25.158051	1352.249006	15.097011
24.927072	1357.814714	15.102029
25.250765	1359.740103	15.107047
25.284688	1361.314744	15.112064
25.325164	1359.670238	15.117082
25.819747	1355.126740	15.122099
25.952001	1367.655250	15.127117
25.782134	1337.029104	15.132135
25.344559	1334.777524	15.137152
25.498965	1332.117331	15.142170
25.337946	1328.348907	15.147187
24.660532	1325.511621	15.152205
24.996153	1316.394568	15.157223
24.653634	1316.161134	15.162240
24.769583	1337.255019	15.167258
25.037350	1355.369473	15.172275
25.189693	1358.232201	15.177293
25.128685	1356.002677	15.182311
25.025040	1357.338674	15.187328
25.416375	1355.361151	15.192346
25.598818	1359.753117	15.197363
25.419199	1356.205218	15.202381
25.521465	1358.087463	15.207399
25.387351	1363.246370	15.212416
25.148044	1360.657614	15.217434
25.442984	1363.168698	15.222451
25.579383	1379.163373	15.227469
25.414305	1384.422095	15.232487
25.758751	1383.186143	15.237504
25.867274	1388.209354	15.242522
25.864703	1382.443875	15.247539
25.689417	1384.314649	15.252557
25.554971	1387.259234	15.257575
26.033002	1390.860299	15.262592
25.678738	1387.966020	15.267610
25.599343	1378.443664	15.272627
25.594814	1386.828706	15.277645
25.773562	1387.391808	15.282663
25.591934	1385.130200	15.287680
25.590575	1386.955404	15.292698
25.679222	1383.746580	15.297715
25.777294	1395.019828	15.302733
25.646719	1389.862570	15.307751
25.830709	1399.419744	15.312768
25.923733	1416.424355	15.317786
25.795817	1410.273623	15.322803
25.936047	1423.979667	15.327821
25.933718	1418.646065	15.332839
26.024103	1415.200693	15.337856
26.024482	1423.819976	15.342874
25.879030	1420.591434	15.347891
26.188496	1419.629221	15.352909
26.204621	1420.687970	15.357927
26.903878	1416.972833	15.362944
26.543606	1424.617629	15.367962
26.844472	1415.756502	15.372979
26.596994	1426.824033	15.377997
26.244390	1411.345936	15.383015
26.598422	1389.676816	15.388032
26.007310	1393.483242	15.393050
26.925755	1395.444471	15.398067
26.728778	1391.510920	15.403085
26.224488	1390.795329	15.408103
26.264971	1381.950516	15.413120
26.169939	1391.167692	15.418138
26.367246	1384.542270	15.423155
26.324105	1404.135816	15.428173
26.537216	1415.269264	15.433191
26.747614	1412.618751	15.438208
26.565131	1419.160121	15.443226
26.672782	1420.553606	15.448243
26.721366	1429.633965	15.453261
26.712707	1420.149067	15.458279
27.059027	1411.444339	15.463296
26.729845	1401.862029	15.468314
26.499744	1384.523405	15.473331
26.389855	1392.922578	15.478349
26.569769	1414.888758	15.483367
26.409831	1407.403621	15.488384
26.125273	1422.725562	15.493402
26.582234	1422.940541	15.498419
26.513148	1412.816731	15.503437
26.213873	1420.238447	15.508455
26.292886	1438.177465	15.513472
26.423116	1451.857293	15.518490
26.814399	1451.081070	15.523507
26.769653	1452.653459	15.528525
26.766238	1447.686606	15.533543
27.170349	1429.873013	15.538560
27.324022	1436.474090	15.543578
27.608854	1443.280657	15.548595
27.920012	1434.646518	15.553613
27.544446	1439.894885	15.558631
27.955343	1427.780311	15.563648
27.467022	1420.120346	15.568666
27.843251	1407.805017	15.573683
27.516413	1408.569778	15.578701
27.255187	1410.746263	15.583719
27.595772	1398.747713	15.588736
27.336022	1403.960462	15.593754
27.333680	1404.718804	15.598771
27.454950	1400.816521	15.603789
27.416299	1407.533245	15.608807
27.676508	1406.588534	15.613824
27.271688	1402.795745	15.618842
27.326497	1401.485818	15.623859
27.171256	1405.418321	15.628877
27.379726	1403.772175	15.633895
27.584758	1397.428916	15.638912
27.122534	1406.632673	15.643930
27.285856	1407.722488	15.648947
27.599001	1399.432550	15.653965
27.631258	1421.585883	15.658983
27.732191	1402.960437	15.664000
27.634679	1409.063178	15.669018
27.434760	1411.821730	15.674035
27.682939	1420.636737	15.679053
27.557359	1444.819725	15.684071
27.894844	1439.915697	15.689088
27.413447	1443.495428	15.694106
27.648882	1445.893094	15.699123
27.518386	1439.975887	15.704141
27.650308	1444.701374	15.709159
27.814990	1437.818111	15.714176
27.472434	1439.390373	15.719194
27.499076	1444.965097	15.724211
27.757701	1448.178554	15.729229
27.762771	1457.677849	15.734247
28.347959	1458.711874	15.739264
28.321760	1463.020338	15.744282
28.413047	1451.499575	15.749299
28.139569	1448.429999	15.754317
28.075466	1445.297358	15.759335
27.888486	1439.476459	15.764352
27.875890	1450.815970	15.769370
28.237389	1451.393809	15.774387
28.182369	1450.156652	15.779405
27.757623	1458.016476	15.784423
28.186939	1470.245292	15.789440
28.000435	1477.445318	15.794458
28.107122	1471.511450	15.799475
28.376990	1475.426994	15.804493
28.171159	1479.153994	15.809511
28.812400	1468.122845	15.814528
28.504060	1480.644697	15.819546
28.615703	1482.541885	15.824563
28.864314	1474.404719	15.829581
28.117109	1479.183300	15.834599
28.149881	1477.388512	15.839616
28.593831	1479.749644	15.844634
28.723198	1478.120991	15.849651
28.574780	1481.939733	15.854669
28.253810	1476.367800	15.859687
28.466805	1472.022958	15.864704
28.859656	1478.145991	15.869722
28.749267	1476.435991	15.874739
28.881482	1474.326486	15.879757
28.262835	1476.059880	15.884775
28.564651	1471.836043	15.889792
28.608065	1478.683624	15.894810
28.651702	1474.647374	15.899827
28.809149	1487.836297	15.904845
29.188132	1502.989818	15.909863
28.948220	1485.491329	15.914880
28.722999	1494.150119	15.919898
28.862966	1503.623557	15.924915
28.925507	1507.536069	15.929933
29.023181	1513.023434	15.934951
28.705356	1495.334729	15.939968
28.720996	1502.881643	15.944986
29.117019	1504.838355	15.950003
28.858164	1496.867720	15.955021
28.621626	1512.127178	15.960039
28.864526	1499.701553	15.965056
29.158218	1509.864066	15.970074
28.913746	1503.109988	15.975091
29.515304	1500.759361	15.980109
29.344916	1504.310587	15.985127
29.239190	1496.810994	15.990144
29.373228	1500.090710	15.995162
29.384102	1503.513210	16.000179
29.573456	1492.965863	16.005197
29.245885	1500.908270	16.010215
29.747975	1494.754222	16.015232
30.119501	1503.953682	16.020250
29.321006	1500.310265	16.025267
29.679371	1501.006766	16.030285
29.289313	1497.048806	16.035303
29.381059	1504.007809	16.040320
29.734010	1502.841659	16.045338
29.585752	1512.488942	16.050355
29.538106	1500.397413	16.055373
29.295804	1507.451885	16.060391
29.370051	1501.936210	16.065408
29.513183	1505.338002	16.070426
29.526003	1524.826819	16.075443
29.615496	1522.576585	16.080461
29.767502	1542.572718	16.085479
29.875488	1534.354503	16.090496
29.736481	1538.932355	16.095514
29.826392	1533.491945	16.100531
29.795426	1529.523989	16.105549
29.532381	1533.013541	16.110567
30.062552	1530.333381	16.115584
29.816067	1532.058883	16.120602
29.615403	1526.676170	16.125619
30.166722	1529.823317	16.130637
29.818127	1533.666943	16.135655
29.929977	1534.931752	16.140672
29.878188	1525.123047	16.145690
29.869780	1530.438428	16.150707
30.233964	1532.384853	16.155725
30.180385	1556.128064	16.160743
30.294233	1550.531952	16.165760
30.130525	1545.718155	16.170778
30.511948	1557.178396	16.175795
30.646325	1549.399790	16.180813
30.354437	1541.302499	16.185831
30.299552	1532.510177	16.190848
30.173714	1532.794370	16.195866
30.224172	1535.041856	16.200883
30.735469	1541.468263	16.205901
30.501878	1549.701307	16.210919
30.479332	1540.964071	16.215936
30.390151	1540.514343	16.220954
30.181662	1549.861707	16.225971
30.686298	1550.081114	16.230989
30.805835	1555.680506	16.236007
30.845102	1556.508500	16.241024
30.428064	1557.794299	16.246042
30.512903	1545.020107	16.251059
30.885909	1553.575573	16.256077
30.821601	1560.018386	16.261095
30.980457	1548.705675	16.266112
30.663094	1547.888727	16.271130
30.745087	1551.890051	16.276147
30.881490	1550.149543	16.281165
30.913283	1542.807865	16.286183
30.996694	1553.130883	16.291200
30.823056	1545.944124	16.296218
30.666283	1557.945509	16.301235
30.949959	1559.161566	16.306253
30.363925	1556.689318	16.311271
30.734132	1556.223430	16.316288
30.916365	1555.829539	16.321306
30.713019	1561.538629	16.326323
31.013852	1557.212171	16.331341
30.662256	1564.960677	16.336359
30.825024	1582.393321	16.341376
31.345426	1576.305795	16.346394
31.332964	1590.478765	16.351411
31.448757	1589.925774	16.356429
31.115535	1593.801821	16.361447
31.077123	1588.331813	16.366464
31.322703	1588.307811	16.371482
31.198245	1596.887169	16.376499
31.309689	1586.784661	16.381517
31.408010	1597.684349	16.386535
31.587174	1589.957106	16.391552
31.748890	1593.647102	16.396570
31.608297	1590.559833	16.401587
31.582041	1580.731753	16.406605
31.144348	1583.909885	16.411623
31.353891	1589.432826	16.416640
31.627816	1581.777538	16.421658
31.432480	1591.327418	16.426675
31.496332	1582.869079	16.431693
31.403678	1585.921903	16.436711
31.310440	1594.493545	16.441728
31.602844	1607.253873	16.446746
31.678465	1617.555432	16.451763
31.919501	1608.759579	16.456781
32.189139	1619.583842	16.461799
32.327641	1606.195607	16.466816
32.502770	1597.233089	16.471834
31.948281	1592.975702	16.476851
32.201356	1582.876475	16.481869
32.578695	1572.569315	16.486887
32.439055	1572.831069	16.491904
32.503033	1566.580044	16.496922
32.586749	1567.331907	16.501939
32.972028	1556.980478	16.506957
32.376698	1535.825935	16.511975
32.209895	1533.941724	16.516992
32.444280	1524.038279	16.522010
32.227444	1528.453864	16.527027
32.493507	1527.117944	16.532045
32.231126	1528.157121	16.537063
32.486092	1529.894689	16.542080
32.322388	1530.024728	16.547098
32.047948	1539.109348	16.552115
32.639867	1531.404682	16.557133
32.717031	1534.416174	16.562151
32.609207	1535.366247	16.567168
32.838515	1530.280324	16.572186
32.102692	1532.007433	16.577203
32.464069	1532.782561	16.582221
32.324300	1532.759661	16.587239
32.526402	1533.101813	16.592256
32.851681	1530.409534	16.597274
32.869577	1533.898560	16.602291
32.864454	1527.844063	16.607309
32.673145	1530.492487	16.612327
32.550270	1533.793422	16.617344
32.665006	1527.173829	16.622362
32.112108	1533.288153	16.627379
32.363070	1537.896398	16.632397
32.703596	1547.414225	16.637415
32.811120	1557.156278	16.642432
33.016967	1559.813392	16.647450
32.712001	1569.608458	16.652467
32.762711	1567.161302	16.657485
32.534592	1569.655790	16.662503
32.484726	1576.267411	16.667520
32.944355	1562.878098	16.672538
32.790555	1578.362437	16.677555
33.022962	1589.833290	16.682573
33.149764	1601.682927	16.687591
32.719483	1590.588139	16.692608
33.657467	1591.282127	16.697626
33.240614	1598.828429	16.702643
33.477485	1592.191018	16.707661
33.664638	1603.201478	16.712679
33.506384	1597.630347	16.717696
33.910893	1593.458563	16.722714
33.600738	1590.658662	16.727731
32.980293	1567.606599	16.732749
33.235060	1580.513137	16.737767
33.362568	1593.210772	16.742784
33.280641	1591.515173	16.747802
33.138662	1594.679223	16.752819
33.241023	1598.660924	16.757837
33.470205	1596.963958	16.762855
33.362268	1594.888524	16.767872
33.605352	1593.219494	16.772890
33.534717	1595.026282	16.777907
33.703406	1606.849054	16.782925
33.585907	1623.256057	16.787943
33.530216	1624.790964	16.792960
34.011308	1617.714775	16.797978
33.769373	1626.280823	16.802995
34.215792	1628.916390	16.808013
33.922184	1623.255845	16.813031
33.936053	1617.347287	16.818048
34.176362	1614.451821	16.823066
34.012732	1629.967821	16.828083
33.901945	1621.344106	16.833101
34.176364	1619.816173	16.838119
34.499199	1617.316446	16.843136
34.288677	1612.799663	16.848154
33.849681	1606.595484	16.853171
34.321562	1610.761498	16.858189
34.088735	1617.350957	16.863207
33.984992	1626.817037	16.868224
34.657643	1620.799070	16.873242
34.302160	1628.672303	16.878259
34.262246	1623.400200	16.883277
34.573578	1618.514382	16.888295
34.769090	1622.295452	16.893312
34.566307	1620.752082	16.898330
34.264315	1630.990033	16.903347
34.417905	1618.872966	16.908365
34.802678	1620.637899	16.913383
34.546402	1623.767609	16.918400
34.661609	1615.636705	16.923418
34.811494	1617.282838	16.928435
34.755310	1611.574897	16.933453
34.784125	1622.967283	16.938471
34.779723	1619.494806	16.943488
34.380621	1614.203572	16.948506
34.412787	1621.957182	16.953523
34.602213	1621.855791	16.958541
35.031845	1616.374036	16.963559
34.598584	1621.131905	16.968576
34.640096	1625.910748	16.973594
34.696649	1632.028504	16.978611
34.743336	1612.028490	16.983629
35.075534	1627.941026	16.988647
34.934471	1649.529844	16.993664
35.435239	1649.240804	16.998682
34.883501	1642.078665	17.003699
35.313085	1641.625038	17.008717
35.544699	1644.714413	17.013735
34.816945	1636.115360	17.018752
35.306890	1640.240091	17.023770
35.340784	1655.602946	17.028787
35.694112	1648.929007	17.033805
35.204860	1631.618790	17.038823
35.024645	1643.340369	17.043840
35.343998	1646.758048	17.048858
35.627634	1650.921698	17.053875
35.566888	1645.574803	17.058893
35.914220	1648.306505	17.063911
35.405575	1639.285587	17.068928
35.596183	1639.312354	17.073946
36.019789	1640.728074	17.078963
36.064849	1622.235189	17.083981
35.703796	1618.091890	17.088999
35.380937	1619.037100	17.094016
35.775372	1607.125233	17.099034
35.531707	1604.246599	17.104051
35.227245	1611.353118	17.109069
36.049701	1630.036248	17.114087
35.887513	1641.766942	17.119104
35.931059	1643.143876	17.124122
35.947350	1647.468337	17.129139
35.679456	1645.186436	17.134157
36.263929	1643.510449	17.139175
35.979431	1650.887609	17.144192
35.891376	1635.144221	17.149210
35.863138	1644.617053	17.154227
35.666836	1643.320630	17.159245
35.698040	1637.511465	17.164263
35.646481	1638.696807	17.169280
35.801450	1650.537716	17.174298
35.871129	1663.933196	17.179315
35.998048	1675.130039	17.184333
36.213881	1666.498336	17.189351
36.267935	1679.919346	17.194368
36.234022	1670.827253	17.199386
36.203135	1675.525207	17.204403
35.997258	1682.184490	17.209421
36.467103	1678.257417	17.214439
36.457183	1689.057998	17.219456
36.339107	1689.079809	17.224474
37.053597	1698.141439	17.229491
37.064852	1687.565042	17.234509
37.106786	1686.112400	17.239527
36.818839	1676.341334	17.244544
36.858390	1676.901539	17.249562
36.775722	1669.453427	17.254579
36.637859	1672.929815	17.259597
36.715141	1670.491868	17.264615
36.890011	1671.195427	17.269632
36.609660	1670.689485	17.274650
36.659027	1665.803680	17.279667
36.624214	1682.043400	17.284685
36.932350	1684.405014	17.289703
36.605163	1692.223027	17.294720
36.857878	1690.988607	17.299738
36.889987	1689.241946	17.304755
36.858324	1692.079979	17.309773
37.483111	1693.245437	17.314791
37.216950	1696.804071	17.319808
37.109037	1691.973181	17.324826
37.420621	1695.022474	17.329843
36.916418	1700.518993	17.334861
37.365950	1695.894135	17.339879
37.044507	1699.482329	17.344896
37.312352	1693.221893	17.349914
37.176879	1699.308418	17.354931
36.966315	1714.664812	17.359949
37.388528	1717.078140	17.364967
37.520871	1724.373235	17.369984
37.217300	1733.638573	17.375002
37.392948	1718.944112	17.380019
37.322959	1724.403992	17.385037
38.373885	1726.108668	17.390055
37.492897	1731.067758	17.395072
37.721972	1726.186167	17.400090
37.439305	1721.356880	17.405107
37.550037	1723.045175	17.410125
38.371291	1720.876561	17.415143
37.629283	1724.267938	17.420160
37.683381	1725.798207	17.425178
37.943796	1727.600618	17.430195
37.562386	1727.448655	17.435213
37.905782	1744.459915	17.440231
37.603640	1754.596384	17.445248
38.434852	1741.653901	17.450266
38.041902	1741.888215	17.455283
38.202103	1748.041794	17.460301
38.433180	1744.761227	17.465319
38.184331	1741.581846	17.470336
38.105859	1742.956084	17.475354
38.374665	1750.423093	17.480371
38.197120	1743.392837	17.485389
38.613085	1741.374426	17.490407
38.346786	1740.666049	17.495424
38.694830	1740.409887	17.500442
38.795689	1738.522284	17.505459
38.405797	1748.504483	17.510477
38.612182	1741.728124	17.515495
38.200412	1742.832303	17.520512
38.506977	1742.464341	17.525530
38.554967	1737.110584	17.530547
38.469742	1735.773846	17.535565
38.720527	1728.038980	17.540583
38.640315	1743.395103	17.545600
38.774338	1738.558549	17.550618
39.226390	1740.670273	17.555635
38.608055	1745.708366	17.560653
38.995039	1737.107917	17.565671
38.812499	1744.676326	17.570688
38.650285	1744.297388	17.575706
39.054650	1761.455318	17.580723
39.060434	1770.034097	17.585741
39.320072	1762.631202	17.590759
39.467696	1754.605311	17.595776
39.306523	1749.293712	17.600794
39.229058	1739.392806	17.605811
39.022043	1739.621227	17.610829
39.104081	1739.565810	17.615847
38.881988	1751.932916	17.620864
38.992673	1758.968323	17.625882
39.127689	1763.334672	17.630899
38.854794	1769.581415	17.635917
38.935340	1762.678180	17.640935
38.976042	1774.918741	17.645952
39.064107	1786.983454	17.650970
39.512711	1796.877834	17.655987
39.145327	1805.350907	17.661005
39.394764	1800.779620	17.666023
39.377573	1796.071742	17.671040
39.377274	1803.799903	17.676058
39.582458	1796.129916	17.681075
39.333318	1799.619898	17.686093
39.660732	1812.409436	17.691111
39.867300	1821.178255	17.696128
40.189106	1826.166221	17.701146
40.348483	1820.788613	17.706163
40.165748	1803.242164	17.711181
40.579762	1778.140149	17.716199
40.399714	1788.482506	17.721216
40.576341	1781.417102	17.726234
40.417836	1782.447148	17.731251
40.340104	1785.094647	17.736269
40.491165	1780.332334	17.741287
40.370873	1780.350981	17.746304
40.252606	1791.524583	17.751322
40.526882	1783.996711	17.756339
40.289327	1788.148959	17.761357
40.236525	1778.751736	17.766375
40.405569	1781.417168	17.771392
40.398379	1785.364543	17.776410
40.596645	1774.435512	17.781427
40.355108	1780.786346	17.786445
40.804487	1779.444963	17.791463
40.424304	1792.923984	17.796480
40.496057	1785.762372	17.801498
40.735633	1783.831686	17.806515
40.703511	1789.440233	17.811533
40.530727	1781.584632	17.816551
40.647928	1786.898252	17.821568
40.687211	1784.829839	17.826586
40.928509	1781.408125	17.831603
40.702323	1788.948995	17.836621
40.575245	1784.547005	17.841639
40.742466	1782.145989	17.846656
40.377496	1791.432519	17.851674
40.838755	1807.723554	17.856691
40.712724	1816.278889	17.861709
40.439576	1823.864053	17.866727
40.681696	1824.310389	17.871744
40.712683	1833.054193	17.876762
40.955700	1841.090305	17.881779
40.812952	1848.766524	17.886797
41.386084	1857.429990	17.891815
41.378250	1854.682157	17.896832
41.063688	1850.869449	17.901850
41.681339	1842.896408	17.906867
41.534706	1850.385868	17.911885
41.730178	1843.692844	17.916903
41.796083	1847.148902	17.921920
41.567681	1851.493322	17.926938
42.156053	1834.353281	17.931955
42.104509	1832.475653	17.936973
42.526315	1823.700268	17.941991
42.451418	1808.469474	17.947008
42.250494	1807.771934	17.952026
42.075691	1804.730650	17.957043
41.821610	1805.635728	17.962061
42.018744	1801.856182	17.967079
41.852796	1803.456080	17.972096
42.105248	1807.586532	17.977114
41.953248	1795.722141	17.982131
42.022747	1792.775604	17.987149
42.030225	1798.627789	17.992167
42.083576	1804.007487	17.997184
41.917011	1804.144712	18.002202
42.090931	1801.182632	18.007219
41.923160	1799.632060	18.012237
41.859169	1803.032024	18.017255
41.972707	1798.876606	18.022272
42.012853	1804.608611	18.027290
42.116689	1807.801827	18.032307
41.943942	1835.363608	18.037325
41.881459	1835.679075	18.042343
42.464321	1836.317021	18.047360
42.043056	1838.370591	18.052378
42.506862	1827.958664	18.057395
42.493149	1838.114642	18.062413
42.648658	1853.620640	18.067431
42.526120	1863.752768	18.072448
42.430670	1870.073471	18.077466
42.458397	1871.613001	18.082483
42.698674	1868.943902	18.087501
43.089507	1870.823983	18.092519
42.873313	1867.854358	18.097536
42.501790	1876.995193	18.102554
42.659097	1870.922165	18.107571
42.596489	1868.391228	18.112589
42.689626	1878.367080	18.117607
43.020400	1892.787026	18.122624
42.930616	1906.982596	18.127642
43.308136	1898.513226	18.132659
43.256720	1901.875224	18.137677
43.570231	1903.462228	18.142695
43.804330	1894.334684	18.147712
43.230636	1896.588828	18.152730
43.446973	1895.198009	18.157747
43.364889	1903.478894	18.162765
43.687451	1893.748706	18.167783
43.482073	1895.642024	18.172800
43.350796	1898.879506	18.177818
43.530403	1891.457984	18.182835
43.489514	1899.323483	18.187853
43.407276	1895.214600	18.192871
43.561831	1892.353080	18.197888
43.035890	1894.803393	18.202906
43.554560	1888.838108	18.207923
43.614934	1892.847165	18.212941
43.639567	1891.084045	18.217959
43.587240	1904.295111	18.222976
43.715244	1918.651408	18.227994
43.991109	1921.668677	18.233011
43.945558	1923.175493	18.238029
43.855477	1932.546490	18.243047
44.225090	1928.551884	18.248064
43.797648	1930.848682	18.253082
44.218704	1924.973358	18.258099
44.025763	1925.921117	18.263117
44.362835	1928.084475	18.268135
44.424774	1919.015572	18.273152
43.991901	1921.871247	18.278170
44.282609	1921.574513	18.283187
44.299628	1914.570278	18.288205
44.357305	1925.701209	18.293223
44.780338	1923.703615	18.298240
44.404539	1931.327299	18.303258
44.424226	1943.610970	18.308275
44.544607	1952.898250	18.313293
44.596737	1953.099568	18.318311
45.166544	1955.154514	18.323328
44.933879	1964.032584	18.328346
45.011823	1946.055009	18.333363
44.869700	1944.789433	18.338381
44.944429	1943.189394	18.343399
45.141240	1937.987635	18.348416
44.708601	1940.964549	18.353434
44.774782	1949.758298	18.358451
45.087434	1949.295182	18.363469
44.807987	1956.985440	18.368487
45.342317	1948.875037	18.373504
44.841351	1952.946095	18.378522
44.996748	1949.608767	18.383539
45.097129	1955.803398	18.388557
45.319122	1951.438768	18.393575
45.622080	1961.509820	18.398592
45.149514	1951.791496	18.403610
45.151929	1952.851844	18.408627
45.378222	1955.077119	18.413645
45.398661	1969.097133	18.418663
45.735057	1977.403171	18.423680
45.762764	1990.478524	18.428698
45.683445	1980.986500	18.433715
45.491586	1969.584778	18.438733
45.571059	1986.204091	18.443751
45.835850	1982.513309	18.448768
45.709048	1978.647903	18.453786
45.892850	1981.492360	18.458803
45.918757	1984.192999	18.463821
45.574333	1985.502211	18.468839
45.909154	1987.406086	18.473856
45.845896	1992.569589	18.478874
45.821081	1978.638488	18.483891
45.796905	1983.392871	18.488909
45.732556	1982.858940	18.493927
46.055139	1973.423228	18.498944
46.139979	1997.890721	18.503962
46.083495	2004.296936	18.508979
46.610675	2002.231076	18.513997
46.506540	2007.327173	18.519015
46.703135	2010.126522	18.524032
46.695969	2000.294906	18.529050
46.677174	1991.622532	18.534067
46.837182	1976.188680	18.539085
46.795859	1978.639392	18.544103
46.973092	1966.669598	18.549120
46.523450	1977.505606	18.554138
46.416534	1969.396065	18.559155
46.725571	1971.057869	18.564173
46.540633	1975.375183	18.569191
46.657103	1988.993659	18.574208
46.589361	1994.558774	18.579226
46.686238	2002.547181	18.584243
47.160153	1994.416400	18.589261
47.018645	2003.082773	18.594279
47.542759	2002.950379	18.599296
46.979524	2006.437557	18.604314
46.938532	2001.993183	18.609331
46.937528	2000.563230	18.614349
47.014613	1996.992435	18.619367
47.238575	2002.751667	18.624384
46.984957	2000.706275	18.629402
46.882420	2000.664390	18.634419
47.155335	2022.700137	18.639437
47.160107	2036.967420	18.644455
46.948751	2028.258347	18.649472
47.056835	2037.163874	18.654490
47.193017	2041.052083	18.659507
47.815582	2059.863717	18.664525
47.443477	2069.391037	18.669543
47.994463	2073.130171	18.674560
47.876797	2068.203578	18.679578
47.736191	2073.105528	18.684595
48.265669	2060.853585	18.689613
48.349992	2058.782139	18.694631
48.431044	2044.247313	18.699648
48.524665	2032.880862	18.704666
48.448895	2027.437974	18.709683
48.424442	2022.383588	18.714701
47.916506	2018.624074	18.719719
48.277023	2017.078193	18.724736
48.404709	2028.247201	18.729754
48.454945	2019.653934	18.734771
48.653633	2023.919664	18.739789
48.423803	2012.994563	18.744807
48.496218	2025.449205	18.749824
48.468147	2013.413380	18.754842
48.398189	2020.257011	18.759859
48.648509	2008.137234	18.764877
48.296587	2019.520767	18.769895
48.464487	2017.380265	18.774912
48.731068	2025.206105	18.779930
48.434923	2023.191232	18.784947
48.509642	2016.175089	18.789965
48.311484	2023.421069	18.794983
48.389821	2028.181121	18.800000
48.783426	2043.620892	18.805018
48.501747	2049.890515	18.810035
48.713531	2055.886533	18.815053
48.788845	2054.521061	18.820071
48.929945	2048.562569	18.825088
49.211766	2046.082802	18.830106
49.001767	2053.530853	18.835123
49.045848	2046.592401	18.840141
48.742195	2073.691150	18.845159
49.374733	2076.282679	18.850176
49.602739	2083.271342	18.855194
49.599648	2081.008158	18.860211
49.681691	2082.710074	18.865229
49.566481	2083.649239	18.870247
49.686752	2086.558159	18.875264
49.631283	2084.232684	18.880282
49.465562	2082.919167	18.885299
49.844618	2072.945292	18.890317
49.453818	2079.310024	18.895335
49.565908	2074.318837	18.900352
49.676566	2086.678769	18.905370
49.515400	2076.067094	18.910387
49.595473	2077.239745	18.915405
49.453950	2072.023105	18.920423
50.020346	2082.786180	18.925440
50.190543	2090.751824	18.930458
50.076854	2100.411654	18.935475
50.614811	2097.856857	18.940493
50.362354	2100.916310	18.945511
50.444701	2103.916786	18.950528
50.327998	2096.568808	18.955546
50.455987	2099.770149	18.960563
50.634614	2090.968977	18.965581
50.138020	2087.912720	18.970599
50.537551	2089.265279	18.975616
50.534088	2093.318014	18.980634
50.406088	2098.133546	18.985651
50.527886	2097.611009	18.990669
50.642660	2096.705370	18.995687
50.280385	2092.447962	19.000704
50.538064	2096.347642	19.005722
50.497422	2095.847442	19.010739
50.882998	2089.580053	19.015757
50.508780	2096.866096	19.020775
50.687111	2098.260912	19.025792
50.840595	2114.289637	19.030810
51.097463	2115.585938	19.035827
51.537476	2114.893078	19.040845
51.419172	2114.765300	19.045863
51.307526	2110.460980	19.050880
51.309373	2102.794205	19.055898
51.589521	2098.700707	19.060915
51.740031	2081.524430	19.065933
51.616644	2082.544142	19.070951
51.656313	2083.890674	19.075968
51.384410	2075.979467	19.080986
50.919487	2081.505607	19.086003
51.237346	2084.034931	19.091021
51.437621	2104.918124	19.096039
51.435113	2111.839220	19.101056
51.699426	2111.125296	19.106074
51.545447	2117.426602	19.111091
51.445461	2112.396556	19.116109
51.207081	2113.621052	19.121127
51.956251	2130.799024	19.126144
51.830949	2140.473864	19.131162
51.385178	2151.977141	19.136179
52.018345	2141.004792	19.141197
52.245076	2138.585250	19.146215
52.461550	2140.679145	19.151232
52.259064	2141.052484	19.156250
52.221925	2144.353022	19.161267
52.255966	2133.290457	19.166285
52.426812	2137.079820	19.171303
52.459695	2140.397490	19.176320
52.658600	2128.841240	19.181338
52.459505	2143.252250	19.186355
52.370212	2140.397843	19.191373
52.763570	2140.883230	19.196391
52.421013	2136.468076	19.201408
52.405099	2135.415525	19.206426
52.194232	2148.007035	19.211443
52.648940	2158.454223	19.216461
52.706235	2175.122428	19.221479
52.600970	2165.944628	19.226496
53.122288	2167.997286	19.231514
52.777175	2171.606575	19.236531
52.857841	2167.888255	19.241549
52.786866	2160.289064	19.246567
52.731229	2179.631355	19.251584
52.876654	2180.707364	19.256602
52.906398	2194.055413	19.261619
53.069135	2189.037787	19.266637
53.470990	2199.025491	19.271655
53.188841	2197.045996	19.276672
53.585961	2189.757933	19.281690
53.650125	2188.828677	19.286707
53.814902	2187.114342	19.291725
53.461446	2192.016595	19.296743
53.684920	2199.647915	19.301760
53.801879	2184.886298	19.306778
53.453948	2184.614397	19.311795
53.957373	2183.898062	19.316813
53.947489	2193.524795	19.321831
53.993505	2190.047879	19.326848
54.270403	2191.844764	19.331866
53.818473	2193.492551	19.336883
54.284425	2194.420679	19.341901
54.196121	2198.056820	19.346919
53.972141	2190.720890	19.351936
53.890292	2189.370145	19.356954
53.999507	2213.349473	19.361971
54.272123	2217.799461	19.366989
54.558176	2220.587843	19.372007
54.408269	2225.191389	19.377024
54.830182	2225.248984	19.382042
54.236418	2228.929268	19.387059
54.167600	2227.011634	19.392077
54.351529	2230.317601	19.397095
54.618511	2228.761355	19.402112
54.526819	2219.151998	19.407130
54.293731	2231.527666	19.412147
54.808773	2233.989345	19.417165
54.970416	2248.689837	19.422183
55.092206	2250.901571	19.427200
55.266055	2245.669391	19.432218
55.352369	2242.344634	19.437235
55.227065	2237.156659	19.442253
55.379879	2221.128039	19.447271
55.032565	2217.198790	19.452288
55.321064	2218.200658	19.457306
55.020526	2224.742915	19.462323
55.478681	2235.252566	19.467341
55.375835	2241.103356	19.472359
55.219570	2247.987084	19.477376
55.590439	2239.728547	19.482394
55.726199	2245.384863	19.487411
55.447099	2251.405267	19.492429
55.657645	2240.433643	19.497447
55.380230	2242.303520	19.502464
55.899610	2238.995867	19.507482
55.451407	2243.140248	19.512499
55.725682	2236.929290	19.517517
55.942040	2240.644723	19.522535
55.758851	2260.835093	19.527552
56.331058	2263.784690	19.532570
56.044839	2269.723631	19.537587
56.440266	2267.246796	19.542605
56.159077	2269.079523	19.547623
55.978463	2260.757234	19.552640
56.533188	2269.421726	19.557658
56.289980	2272.356772	19.562675
56.405798	2268.596964	19.567693
56.327041	2263.837287	19.572711
56.241760	2283.345443	19.577728
56.488197	2262.263734	19.582746
56.182710	2277.738150	19.587763
56.012197	2269.933102	19.592781
56.112733	2274.943400	19.597799
56.063118	2295.707855	19.602816
56.331983	2297.055666	19.607834
56.510024	2300.337458	19.612851
56.706155	2300.341624	19.617869
56.998814	2309.427505	19.622887
57.353619	2320.080937	19.627904
57.454666	2310.095118	19.632922
57.463009	2296.420689	19.637939
57.393163	2283.592876	19.642957
57.711035	2282.766596	19.647975
57.534333	2285.613853	19.652992
57.600024	2269.429229	19.658010
57.204515	2278.107013	19.663027
57.377881	2282.241702	19.668045
57.768141	2279.768114	19.673063
57.521123	2285.118361	19.678080
57.668345	2277.404526	19.683098
57.754992	2283.484301	19.688115
57.463192	2284.291130	19.693133
57.716604	2288.600315	19.698151
58.148075	2311.265293	19.703168
58.346063	2311.334505	19.708186
58.145898	2301.468849	19.713203
58.297501	2300.063895	19.718221
58.502601	2281.687303	19.723239
57.920454	2276.535902	19.728256
58.150011	2274.960079	19.733274
57.968235	2280.381829	19.738291
57.957266	2297.724963	19.743309
58.235519	2311.382528	19.748327
58.150116	2310.139486	19.753344
58.648763	2304.377511	19.758362
58.187808	2308.334301	19.763379
58.606542	2310.984973	19.768397
58.899736	2300.247995	19.773415
58.443056	2311.791059	19.778432
58.362408	2307.978297	19.783450
58.434380	2315.997123	19.788467
58.800224	2321.276171	19.793485
59.592506	2306.585299	19.798503
59.601216	2311.052210	19.803520
59.784450	2289.531624	19.808538
59.716943	2285.144085	19.813555
59.246467	2281.948644	19.818573
59.759695	2274.394928	19.823591
59.637131	2279.434027	19.828608
59.757027	2278.927561	19.833626
59.746492	2259.815406	19.838643
59.453496	2250.282281	19.843661
59.778550	2243.054588	19.848679
59.539502	2245.754235	19.853696
59.819601	2237.759330	19.858714
59.422885	2237.552494	19.863731
59.458901	2235.006556	19.868749
59.566705	2254.098838	19.873767
59.670136	2279.816532	19.878784
59.847454	2274.930258	19.883802
59.955571	2276.928559	19.888819
59.904248	2281.580584	19.893837
59.721411	2274.702198	19.898855
59.728119	2283.960732	19.903872
59.907657	2273.153481	19.908890
59.849784	2272.707419	19.913907
59.825788	2294.287292	19.918925
60.132144	2303.084951	19.923943
59.859028	2314.250822	19.928960
59.823695	2306.662774	19.933978
60.191494	2305.946850	19.938995
59.954498	2321.837192	19.944013
60.333211	2335.270436	19.949031
60.021868	2351.137328	19.954048
60.600412	2352.498991	19.959066
60.611050	2353.725700	19.964083
60.231727	2352.412554	19.969101
60.498974	2364.852175	19.974119
60.894769	2383.089598	19.979136
60.782928	2380.030318	19.984154
61.519500	2376.249109	19.989171
61.232848	2376.597507	19.994189
61.785776	2377.302829	19.999207
61.108582	2377.744960	20.004224
61.594430	2381.001559	20.009242
61.388489	2375.086300	20.014259
61.065459	2386.123749	20.019277
61.601962	2372.081492	20.024295
61.407901	2375.493248	20.029312
61.407408	2380.480737	20.034330
61.524768	2374.868373	20.039347
61.306577	2379.202524	20.044365
61.890359	2393.570106	20.049383
61.599741	2402.803296	20.054400
61.946295	2407.274526	20.059418
61.858442	2406.064972	20.064435
61.733083	2416.455855	20.069453
62.179637	2406.533594	20.074471
61.968649	2410.022287	20.079488
62.275448	2405.530376	20.084506
62.745522	2396.412093	20.089523
62.359344	2401.162515	20.094541
62.289582	2405.944531	20.099559
62.528604	2401.223257	20.104576
62.337128	2401.037932	20.109594
62.525667	2400.888257	20.114611
62.181267	2410.261401	20.119629
62.545539	2400.035089	20.124647
62.514402	2421.567534	20.129664
62.810042	2438.618059	20.134682
63.127356	2435.456052	20.139699
62.946449	2438.593081	20.144717
63.085058	2434.187487	20.149735
62.889753	2441.241800	20.154752
62.915751	2433.739254	20.159770
63.367587	2424.609119	20.164787
63.420476	2422.389446	20.169805
63.913723	2412.367035	20.174823
63.884576	2411.864854	20.179840
63.747997	2396.421979	20.184858
63.837244	2390.096991	20.189875
63.431180	2379.905111	20.194893
63.477390	2376.778570	20.199911
63.459112	2390.014528	20.204928
63.689030	2384.705749	20.209946
63.560299	2381.984064	20.214963
63.825346	2413.268081	20.219981
63.878635	2418.593662	20.224999
63.746631	2420.030689	20.230016
63.395478	2417.258140	20.235034
63.560268	2411.861290	20.240051
63.606078	2420.527278	20.245069
63.651872	2422.026751	20.250087
63.776106	2442.919101	20.255104
63.849811	2452.471023	20.260122
63.908648	2446.033884	20.265139
63.612331	2457.025064	20.270157
63.835011	2464.122704	20.275175
63.951127	2477.657795	20.280192
64.095120	2480.917898	20.285210
64.602939	2488.295064	20.290227
64.735636	2503.078724	20.295245
64.936949	2504.834266	20.300263
65.086310	2505.397726	20.305280
64.634712	2503.462205	20.310298
65.391694	2500.584709	20.315315
64.874339	2502.388648	20.320333
65.072740	2499.607706	20.325351
65.373962	2499.897056	20.330368
65.466577	2496.460910	20.335386
65.269169	2496.627052	20.340403
65.229280	2504.890388	20.345421
65.674021	2507.957178	20.350439
65.208595	2492.291014	20.355456
65.174936	2493.670235	20.360474
65.236074	2487.264186	20.365491
65.377547	2503.134713	20.370509
65.322448	2506.313188	20.375527
65.443292	2521.956523	20.380544
65.489110	2521.502127	20.385562
65.762412	2526.378143	20.390579
66.043767	2518.575040	20.395597
66.375335	2505.330921	20.400615
66.146116	2511.023133	20.405632
66.226855	2514.874501	20.410650
66.693498	2506.815977	20.415667
66.348992	2513.300526	20.420685
66.507780	2505.334948	20.425703
66.679595	2503.203554	20.430720
66.415927	2502.756542	20.435738
66.502640	2495.797193	20.440755
66.469598	2507.269344	20.445773
66.756463	2502.146859	20.450791
67.176344	2492.703212	20.455808
67.420276	2494.616040	20.460826
67.546388	2485.818926	20.465843
67.400488	2492.804151	20.470861
67.812730	2473.521597	20.475879
67.849564	2466.701544	20.480896
67.686265	2456.737327	20.485914
67.673322	2459.971568	20.490931
67.508563	2464.845491	20.495949
67.608044	2447.972886	20.500967
67.450946	2445.873478	20.505984
67.283844	2450.941531	20.511002
67.415601	2448.293303	20.516019
67.061790	2458.646992	20.521037
67.444647	2448.565518	20.526055
67.285357	2453.464488	20.531072
67.280935	2449.700838	20.536090
67.804477	2457.401331	20.541107
67.336802	2476.938275	20.546125
67.652389	2489.828840	20.551143
67.704839	2482.364263	20.556160
67.561513	2479.696253	20.561178
68.023666	2484.518615	20.566195
68.157726	2494.844598	20.571213
68.303484	2508.542378	20.576231
68.277636	2520.141673	20.581248
68.226172	2515.413466	20.586266
68.363249	2513.496723	20.591283
68.156584	2524.328461	20.596301
68.132816	2520.309799	20.601319
68.172176	2525.806337	20.606336
68.141659	2531.853531	20.611354
68.537426	2540.411548	20.616371
68.475545	2552.746303	20.621389
68.183330	2552.875935	20.626407
68.526944	2566.297283	20.631424
68.499532	2575.311401	20.636442
68.822477	2582.493498	20.641459
68.924597	2587.992686	20.646477
68.797779	2583.164760	20.651495
69.063225	2596.915338	20.656512
69.205710	2608.221225	20.661530
69.419357	2603.924000	20.666547
69.477272	2609.276417	20.671565
69.498333	2608.934943	20.676583
69.867006	2609.804174	20.681600
69.385959	2616.190105	20.686618
69.966278	2608.676706	20.691635
69.712569	2616.946045	20.696653
69.700556	2612.378004	20.701671
70.312771	2602.887929	20.706688
69.883193	2610.240007	20.711706
70.160307	2612.229065	20.716723
70.196884	2621.462202	20.721741
69.964338	2613.807799	20.726759
70.541128	2628.266577	20.731776
70.199481	2642.074814	20.736794
70.471890	2641.923360	20.741811
70.525890	2646.654303	20.746829
70.297499	2642.292671	20.751847
70.907827	2636.943790	20.756864
70.492379	2648.617850	20.761882
70.668901	2645.592558	20.766899
70.439821	2644.992341	20.771917
70.145396	2639.354402	20.776935
70.648872	2656.375834	20.781952
70.494025	2672.279221	20.786970
70.962250	2669.833160	20.791987
70.616156	2674.075126	20.797005
70.765280	2692.426079	20.802023
71.209059	2687.702693	20.807040
71.488597	2703.442647	20.812058
71.511950	2694.835506	20.817075
71.484581	2699.628455	20.822093
71.214693	2700.922187	20.827111
71.236872	2687.860116	20.832128
71.703810	2708.464103	20.837146
71.926127	2717.885964	20.842163
72.320536	2724.680215	20.847181
72.099584	2713.039586	20.852199
72.177595	2715.273855	20.857216
72.325804	2725.102985	20.862234
72.354206	2711.243620	20.867251
72.238606	2710.351454	20.872269
72.194029	2719.641089	20.877287
72.338291	2718.031020	20.882304
72.245182	2720.141056	20.887322
72.996722	2716.610006	20.892339
72.540290	2719.410005	20.897357
72.422224	2721.455804	20.902375
72.879760	2712.838006	20.907392
72.555506	2720.265007	20.912410
72.535459	2709.968140	20.917427
72.626890	2712.326902	20.922445
72.629864	2715.738027	20.927463
72.995640	2725.640901	20.932480
73.241984	2738.456913	20.937498
73.805477	2735.202238	20.942515
73.492433	2727.558430	20.947533
73.570567	2715.703500	20.952551
73.411812	2700.283028	20.957568
73.509023	2705.074310	20.962586
73.482896	2707.824947	20.967603
73.416978	2712.209474	20.972621
73.641823	2727.233500	20.977639
74.056319	2725.495195	20.982656
73.805166	2731.801593	20.987674
73.883624	2728.564710	20.992691
73.892357	2729.322398	20.997709
73.997137	2736.070229	21.002727
74.324084	2729.053052	21.007744
73.853438	2736.121625	21.012762
74.098245	2731.131497	21.017779
74.281857	2737.187736	21.022797
74.072350	2736.332145	21.027815
74.584949	2743.704676	21.032832
74.194465	2764.049363	21.037850
74.338061	2765.367504	21.042867
74.241630	2765.477746	21.047885
74.501923	2769.628376	21.052903
74.954590	2760.084443	21.057920
74.792238	2757.146368	21.062938
74.828123	2758.000996	21.067955
74.958551	2765.366604	21.072973
74.934008	2774.347268	21.077991
75.156060	2774.427322	21.083008
75.161386	2786.421543	21.088026
75.517239	2784.997279	21.093043
75.485993	2779.521294	21.098061
75.207573	2784.781799	21.103079
75.257035	2781.686910	21.108096
75.107101	2788.222479	21.113114
75.585075	2797.556455	21.118131
75.784555	2806.744445	21.123149
76.029793	2814.369185	21.128167
76.327808	2813.954236	21.133184
76.240652	2816.312918	21.138202
76.204187	2813.628891	21.143219
76.235193	2814.683609	21.148237
76.139864	2807.848264	21.153255
76.531710	2806.233541	21.158272
76.854351	2816.616398	21.163290
76.842651	2808.855520	21.168307
76.595327	2801.841473	21.173325
76.490050	2804.803372	21.178343
76.154850	2808.027567	21.183360
76.437565	2814.491335	21.188378
76.519084	2808.536077	21.193395
76.556281	2804.366707	21.198413
76.355029	2814.814180	21.203431
76.792557	2832.529915	21.208448
76.361203	2845.426763	21.213466
76.429706	2846.087578	21.218483
77.014676	2838.276368	21.223501
76.837263	2850.483104	21.228519
77.214711	2855.821775	21.233536
76.802273	2865.628194	21.238554
77.108240	2866.591671	21.243571
77.331325	2863.032270	21.248589
77.114950	2887.122003	21.253607
77.831306	2884.987768	21.258624
77.591930	2895.657620	21.263642
77.929905	2894.956237	21.268659
77.954116	2895.597871	21.273677
78.061367	2891.094358	21.278695
78.003995	2889.879540	21.283712
77.874302	2897.708785	21.288730
77.881629	2891.487422	21.293747
78.062590	2904.445513	21.298765
78.048934	2918.028435	21.303783
78.289020	2911.887654	21.308800
78.050583	2916.178957	21.313818
78.330190	2928.794895	21.318835
79.107474	2924.179649	21.323853
79.269953	2932.536099	21.328871
79.449729	2916.443082	21.333888
79.279173	2908.186453	21.338906
79.374183	2903.051054	21.343923
79.362703	2891.280660	21.348941
79.335892	2896.665027	21.353959
79.448374	2900.859935	21.358976
79.044465	2894.857922	21.363994
79.255487	2906.863434	21.369011
79.453661	2910.685316	21.374029
79.577946	2940.470600	21.379047
79.685559	2926.947927	21.384064
79.685105	2942.105291	21.389082
79.605021	2940.298971	21.394099
79.864330	2939.559881	21.399117
79.761302	2941.829946	21.404135
80.081251	2933.763280	21.409152
79.741913	2938.130953	21.414170
79.740956	2936.948988	21.419187
80.136499	2953.880565	21.424205
79.985532	2968.847182	21.429223
80.248368	2962.605612	21.434240
80.343533	2965.387479	21.439258
80.392676	2969.809842	21.444275
80.324741	2967.496611	21.449293
80.654848	2989.753884	21.454311
80.624781	2994.957704	21.459328
80.678203	2992.258237	21.464346
80.892179	2998.832311	21.469363
81.116992	2989.785664	21.474381
80.747072	2991.897515	21.479399
81.074543	2988.420210	21.484416
81.030531	2995.092855	21.489434
81.058199	3012.714463	21.494451
81.322505	3017.993044	21.499469
81.174220	3017.866459	21.504487
81.957020	3011.786169	21.509504
82.205634	3009.194995	21.514522
82.218897	3003.250579	21.519539
82.603015	3002.977588	21.524557
82.370218	2986.566178	21.529575
82.624233	2977.071925	21.534592
82.488337	2977.511833	21.539610
82.444758	2971.380284	21.544627
82.568277	2965.087780	21.549645
82.550087	2980.266336	21.554663
82.539325	2966.448112	21.559680
82.613615	2966.017174	21.564698
82.461258	2969.661325	21.569715
82.454099	2973.080543	21.574733
82.399733	2978.178266	21.579751
82.521583	2975.693098	21.584768
82.492610	2969.648040	21.589786
82.285007	2986.190835	21.594803
82.539429	2995.899544	21.599821
82.463013	3009.472041	21.604839
82.860255	3016.966075	21.609856
83.283788	3030.180380	21.614874
82.965102	3044.166171	21.619891
82.930024	3044.333626	21.624909
82.970820	3048.138420	21.629927
83.009524	3042.166788	21.634944
83.078310	3068.616271	21.639962
83.044209	3078.972256	21.644979
83.190224	3072.960162	21.649997
82.871332	3093.810428	21.655015
83.335524	3105.518306	21.660032
83.905572	3117.796355	21.665050
83.465337	3131.972387	21.670067
83.878434	3127.595936	21.675085
84.362554	3136.125745	21.680103
84.414610	3140.613025	21.685120
84.315892	3140.025091	21.690138
84.346847	3143.236194	21.695155
84.739518	3149.830888	21.700173
84.793701	3159.726815	21.705191
85.149628	3160.458866	21.710208
85.509467	3160.858680	21.715226
85.025497	3147.311229	21.720243
85.485262	3126.575336	21.725261
85.174256	3121.245639	21.730279
85.013609	3122.101691	21.735296
85.527688	3129.359168	21.740314
85.391277	3148.798407	21.745331
85.488526	3155.300414	21.750349
85.414290	3158.214528	21.755367
85.569033	3160.720018	21.760384
85.392590	3150.664680	21.765402
85.747676	3156.508969	21.770419
86.183442	3154.235365	21.775437
85.784199	3162.079451	21.780455
85.693467	3159.777976	21.785472
85.943285	3147.539670	21.790490
85.829805	3164.520941	21.795507
86.164814	3163.704283	21.800525
86.306813	3181.523847	21.805543
86.102857	3185.820336	21.810560
86.153355	3182.759056	21.815578
85.860085	3191.472577	21.820595
86.127271	3196.076567	21.825613
86.299701	3218.456492	21.830631
86.715806	3217.684996	21.835648
86.694005	3208.444234	21.840666
86.409975	3222.017853	21.845683
86.728577	3236.470269	21.850701
86.966413	3244.786400	21.855719
86.973350	3252.262404	21.860736
87.010248	3253.184617	21.865754
86.903387	3258.058308	21.870771
87.332477	3262.708592	21.875789
87.545424	3279.166992	21.880807
87.848034	3273.257925	21.885824
88.248496	3277.172016	21.890842
88.128430	3279.834111	21.895859
87.895063	3274.024021	21.900877
88.398975	3279.437241	21.905895
88.279303	3273.191821	21.910912
88.755150	3277.812829	21.915930
88.443621	3281.577273	21.920947
88.727173	3271.460322	21.925965
88.744171	3275.840241	21.930983
88.437141	3276.625313	21.936000
88.781452	3270.353115	21.941018
88.500204	3285.780258	21.946035
88.700691	3273.966937	21.951053
88.725189	3278.331395	21.956071
88.597939	3273.976661	21.961088
88.915864	3284.187371	21.966106
88.798482	3297.806517	21.971123
88.766998	3292.847042	21.976141
88.654854	3301.887917	21.981159
88.547693	3313.767149	21.986176
88.881882	3326.188183	21.991194
89.292963	3328.722209	21.996211
89.320437	3335.291383	22.001229
89.508087	3344.368306	22.006247
89.472710	3349.622771	22.011264
89.792728	3343.716994	22.016282
89.569586	3355.658671	22.021299
89.679246	3351.192417	22.026317
90.116621	3377.346892	22.031335
89.912262	3383.206057	22.036352
90.535529	3380.577370	22.041370
90.228917	3385.199456	22.046387
90.404073	3380.440012	22.051405
90.276128	3389.122935	22.056423
90.303913	3393.783778	22.061440
90.353784	3390.554811	22.066458
90.763281	3412.436786	22.071475
90.852029	3405.769667	22.076493
91.210383	3407.639366	22.081511
91.168276	3416.056350	22.086528
91.581393	3415.834301	22.091546
91.099518	3417.785833	22.096563
91.089500	3409.232853	22.101581
91.205480	3410.697547	22.106599
91.523653	3431.409111	22.111616
92.051188	3437.171172	22.116634
91.455892	3444.414218	22.121651
91.981279	3446.398626	22.126669
91.292919	3436.083546	22.131687
91.457669	3438.619655	22.136704
91.791242	3448.147320	22.141722
91.755862	3466.832453	22.146739
92.026544	3473.665571	22.151757
92.294764	3480.553456	22.156775
92.159295	3480.495552	22.161792
92.130268	3487.636022	22.166810
92.419793	3504.122484	22.171827
92.872206	3501.909773	22.176845
92.770176	3508.409861	22.181863
92.920710	3508.191087	22.186880
92.913674	3494.799420	22.191898
92.961244	3497.615531	22.196915
93.020970	3501.356545	22.201933
92.849593	3517.019466	22.206951
93.257532	3528.484490	22.211968
93.635271	3524.168337	22.216986
93.711483	3532.180756	22.222003
93.792382	3530.215242	22.227021
93.541772	3519.829784	22.232039
93.429236	3528.818875	22.237056
94.083420	3533.874061	22.242074
94.340094	3554.424636	22.247091
94.235304	3550.398336	22.252109
94.359083	3543.087209	22.257127
94.603497	3554.240837	22.262144
94.705248	3549.773521	22.267162
94.428308	3552.104992	22.272179
94.639814	3547.582631	22.277197
94.810906	3555.381899	22.282215
94.137092	3562.012328	22.287232
94.257397	3547.654468	22.292250
94.554177	3550.597982	22.297267
94.548665	3573.259371	22.302285
95.024489	3580.500777	22.307303
94.569770	3591.005605	22.312320
94.904637	3584.834927	22.317338
95.089118	3587.691377	22.322355
95.769218	3596.489485	22.327373
95.760043	3607.918178	22.332391
95.367228	3621.172126	22.337408
95.512288	3611.509514	22.342426
95.432412	3614.969691	22.347443
95.952351	3611.640401	22.352461
95.795991	3621.330924	22.357479
95.931263	3622.820685	22.362496
96.168057	3626.343138	22.367514
95.919783	3640.065353	22.372531
95.712692	3647.816878	22.377549
96.088399	3643.708965	22.382567
96.265802	3658.252134	22.387584
96.281389	3672.604895	22.392602
96.514641	3681.173285	22.397619
96.862414	3677.832543	22.402637
96.746476	3679.826906	22.407655
96.607646	3682.616725	22.412672
97.089789	3701.711170	22.417690
97.025682	3706.216164	22.422707
97.063948	3710.023914	22.427725
97.275292	3706.391517	22.432743
97.329340	3708.185834	22.437760
97.608840	3705.668800	22.442778
97.590988	3714.739426	22.447795
97.897415	3723.374841	22.452813
97.771277	3730.112282	22.457831
98.474892	3723.757830	22.462848
98.744249	3718.708052	22.467866
98.269391	3726.622086	22.472883
98.346844	3724.125511	22.477901
98.866916	3723.964670	22.482919
99.148485	3725.189931	22.487936
98.924904	3718.597492	22.492954
98.848600	3723.038423	22.497971
98.719245	3723.618208	22.502989
99.210796	3724.471167	22.508007
99.050518	3721.072598	22.513024
99.091076	3728.121701	22.518042
99.365188	3733.292518	22.523059
98.803957	3722.452179	22.528077
99.017021	3713.979716	22.533095
99.013193	3730.094556	22.538112
98.969182	3733.721094	22.543130
99.046908	3743.599963	22.548147
98.879714	3753.237292	22.553165
99.144207	3758.756309	22.558183
98.996869	3782.745786	22.563200
99.438968	3790.430976	22.568218
99.567607	3809.329400	22.573235
99.672049	3821.571261	22.578253
99.840823	3820.899637	22.583271
99.909200	3843.507002	22.588288
99.771577	3852.456472	22.593306
100.412353	3855.485201	22.598323
100.350260	3848.943782	22.603341
100.976107	3845.661658	22.608359
101.329364	3863.917549	22.613376
101.393955	3852.618560	22.618394
101.517330	3836.015248	22.623411
101.650182	3833.186242	22.628429
101.929153	3821.570923	22.633447
101.570391	3826.847908	22.638464
102.205700	3825.541830	22.643482
102.294004	3820.195419	22.648499
102.074406	3826.582689	22.653517
102.213806	3819.109662	22.658535
102.055903	3824.575889	22.663552
102.215797	3815.783270	22.668570
102.478385	3825.473765	22.673587
102.090394	3827.560468	22.678605
102.369517	3821.949788	22.683623
102.360307	3820.643155	22.688640
102.142586	3824.186867	22.693658
102.272928	3829.798217	22.698675
102.176371	3828.955490	22.703693
102.171017	3837.473511	22.708711
101.890503	3852.555323	22.713728
101.993748	3860.217518	22.718746
102.394487	3877.190157	22.723763
102.266520	3891.488968	22.728781
102.752879	3905.179980	22.733799
102.544232	3922.150813	22.738816
102.933629	3931.533734	22.743834
103.061454	3945.594201	22.748851
103.080737	3948.593242	22.753869
103.447757	3947.442627	22.758887
103.435708	3969.460655	22.763904
103.870635	3979.239053	22.768922
103.957426	3973.147773	22.773939
104.026246	3986.134645	22.778957
104.355434	3975.648698	22.783975
103.995589	3986.876297	22.788992
104.575238	4004.055471	22.794010
104.829721	4006.690493	22.799027
104.870904	4003.843306	22.804045
105.142601	4005.814572	22.809063
105.135765	4008.903164	22.814080
105.232653	4002.861335	22.819098
105.583415	3998.856060	22.824115
105.065513	4004.180864	22.829133
105.034167	4004.441414	22.834151
105.377285	4005.304085	22.839168
105.224613	4003.319484	22.844186
105.490110	4003.335393	22.849203
105.187759	4016.006295	22.854221
105.525420	4026.736291	22.859239
105.656492	4034.281959	22.864256
105.671856	4034.906254	22.869274
106.026464	4032.588948	22.874291
105.937795	4042.651690	22.879309
106.059184	4052.880055	22.884327
106.310035	4057.665100	22.889344
106.345577	4055.531660	22.894362
106.533352	4057.894586	22.899379
106.608675	4064.705534	22.904397
107.144583	4056.575284	22.909415
106.837561	4058.895445	22.914432
106.918444	4076.465799	22.919450
107.543275	4087.549074	22.924467
107.221260	4090.844512	22.929485
107.177452	4081.851959	22.934503
107.311877	4083.200139	22.939520
107.344296	4082.762174	22.944538
107.290947	4082.630328	22.949555
107.214273	4094.820753	22.954573
107.724590	4107.883257	22.959591
107.612475	4122.935668	22.964608
107.773236	4118.591970	22.969626
107.934158	4114.963399	22.974643
107.988409	4144.432166	22.979661
108.280433	4136.713866	22.984679
108.658042	4128.648524	22.989696
109.093408	4121.155332	22.994714
109.502416	4110.598904	22.999731
109.584692	4126.221305	23.004749
109.861225	4126.151835	23.009767
109.950776	4115.724994	23.014784
109.999948	4092.941121	23.019802
110.120279	4083.677055	23.024819
109.948677	4079.354116	23.029837
110.044679	4080.413528	23.034855
109.969904	4080.612216	23.039872
109.937970	4074.729490	23.044890
110.279288	4076.255643	23.049907
109.916922	4080.413344	23.054925
110.173794	4078.321505	23.059943
110.339775	4077.581826	23.064960
109.769508	4075.421498	23.069978
109.819403	4078.558660	23.074995
109.589893	4086.522960	23.080013
109.580472	4102.001172	23.085031
110.355500	4114.288183	23.090048
110.062864	4124.378068	23.095066
110.027452	4142.468569	23.100083
110.210276	4146.743114	23.105101
110.263754	4154.363577	23.110119
110.655283	4170.134634	23.115136
110.552608	4179.354750	23.120154
111.158520	4187.630333	23.125171
111.019770	4205.787455	23.130189
111.321627	4206.359491	23.135207
111.468263	4208.074982	23.140224
111.459599	4230.718951	23.145242
111.767333	4235.974747	23.150259
111.712228	4239.141756	23.155277
112.022972	4233.762585	23.160295
111.944205	4243.205474	23.165312
112.206979	4257.914926	23.170330
112.486463	4254.659021	23.175347
112.657844	4265.564184	23.180365
112.875118	4260.489297	23.185383
113.058510	4251.598682	23.190400
113.422735	4249.601046	23.195418
113.475260	4245.717725	23.200435
113.291060	4252.324356	23.205453
113.697663	4248.305508	23.210471
113.678794	4253.159694	23.215488
113.731380	4246.466129	23.220506
113.750716	4246.989724	23.225523
113.791056	4253.096316	23.230541
113.717888	4247.660087	23.235559
113.888542	4245.920897	23.240576
113.947280	4255.005482	23.245594
113.996011	4246.000909	23.250611
113.611572	4262.648602	23.255629
113.760906	4272.270576	23.260647
114.313940	4276.432069	23.265664
114.131872	4280.128082	23.270682
114.555514	4296.175729	23.275699
114.893269	4304.713155	23.280717
115.313602	4309.311697	23.285735
115.146676	4307.806801	23.290752
115.300527	4314.423241	23.295770
115.227474	4313.129087	23.300787
115.345974	4314.795855	23.305805
115.250766	4311.899534	23.310823
115.586475	4328.015059	23.315840
115.430677	4341.943350	23.320858
115.887271	4340.041711	23.325875
115.517743	4349.757409	23.330893
115.654524	4348.506042	23.335911
115.997403	4363.031732	23.340928
115.798160	4371.964492	23.345946
116.089243	4370.807965	23.350963
115.779878	4384.966616	23.355981
116.131223	4390.821461	23.360999
116.779421	4398.685854	23.366016
116.252085	4392.513028	23.371034
116.557885	4407.427115	23.376051
116.772057	4422.087555	23.381069
116.552015	4426.561989	23.386087
117.467741	4435.148476	23.391104
117.090168	4448.094898	23.396122
117.702396	4455.629168	23.401139
117.437264	4456.641037	23.406157
117.575879	4462.524502	23.411175
117.864852	4447.943153	23.416192
117.601835	4451.663322	23.421210
117.781677	4455.353253	23.426227
117.968977	4474.760678	23.431245
118.151750	4477.686108	23.436263
118.164797	4482.942887	23.441280
118.395828	4493.005453	23.446298
118.587866	4481.095804	23.451315
118.406727	4503.999721	23.456333
118.674112	4513.176281	23.461351
118.805323	4504.220432	23.466368
118.440241	4508.789066	23.471386
118.933481	4517.562234	23.476403
119.040664	4530.625678	23.481421
119.270865	4537.470926	23.486439
119.627401	4530.836190	23.491456
119.445219	4546.846177	23.496474
119.755724	4555.758601	23.501491
120.136581	4565.032308	23.506509
120.244374	4565.183162	23.511527
120.475894	4564.277062	23.516544
120.338615	4557.654510	23.521562
120.397204	4555.617868	23.526579
120.737394	4551.210999	23.531597
120.637789	4554.650346	23.536615
120.592310	4548.343654	23.541632
120.888652	4570.726310	23.546650
120.994420	4577.462947	23.551667
121.206403	4576.583037	23.556685
121.480956	4584.818759	23.561703
121.998843	4577.044198	23.566720
121.665691	4588.060495	23.571738
121.916180	4576.002130	23.576755
121.826923	4577.991243	23.581773
121.811099	4579.350259	23.586791
121.821624	4574.039770	23.591808
121.832446	4580.109804	23.596826
121.903025	4594.280693	23.601843
122.331590	4603.378478	23.606861
121.947096	4610.329137	23.611879
122.484981	4596.557993	23.616896
122.079657	4616.683911	23.621914
122.303671	4633.069365	23.626931
122.594928	4640.298799	23.631949
122.284632	4651.055238	23.636967
122.644211	4663.799849	23.641984
122.705071	4679.586359	23.647002
123.329934	4683.356792	23.652019
123.718063	4699.370769	23.657037
123.456071	4708.399540	23.662055
123.745515	4701.591926	23.667072
123.430851	4711.928554	23.672090
123.796429	4700.719924	23.677107
123.977423	4709.387625	23.682125
123.963099	4722.702051	23.687143
124.401507	4723.929649	23.692160
124.199132	4726.242203	23.697178
124.717717	4723.659608	23.702195
124.542904	4723.539916	23.707213
124.517748	4736.638820	23.712231
124.951408	4746.661297	23.717248
125.038872	4749.640137	23.722266
124.745057	4759.558919	23.727283
125.139944	4759.742473	23.732301
124.976286	4760.786585	23.737319
124.820819	4771.163697	23.742336
125.365911	4784.856435	23.747354
125.744447	4777.842117	23.752371
125.751235	4802.175333	23.757389
125.446720	4817.752880	23.762407
125.874819	4811.904436	23.767424
125.826704	4823.817997	23.772442
126.213083	4833.858875	23.777459
126.364460	4840.082922	23.782477
126.498149	4839.692949	23.787495
126.632658	4842.216356	23.792512
126.854619	4854.527876	23.797530
127.522361	4863.699805	23.802547
127.593756	4871.360862	23.807565
127.527159	4880.101034	23.812583
127.870150	4882.024747	23.817600
127.718501	4873.343239	23.822618
127.582464	4868.025482	23.827635
127.829823	4874.152747	23.832653
127.739401	4863.673565	23.837671
127.891350	4861.519273	23.842688
128.177992	4878.153382	23.847706
128.087839	4883.094808	23.852723
128.674530	4876.622112	23.857741
128.101549	4886.473047	23.862759
128.403026	4882.390936	23.867776
128.529431	4904.390466	23.872794
128.923125	4911.032202	23.877811
129.307672	4909.470514	23.882829
129.536145	4916.397351	23.887847
129.670604	4914.843880	23.892864
129.907929	4920.990212	23.897882
129.748736	4914.303528	23.902899
129.858934	4911.777524	23.907917
129.888014	4921.362223	23.912935
130.023519	4919.822749	23.917952
129.672689	4920.188494	23.922970
129.724010	4940.201091	23.927987
129.976862	4938.809270	23.933005
130.187468	4950.585630	23.938023
130.517486	4958.422936	23.943040
130.253811	4974.303184	23.948058
130.660401	4974.361861	23.953075
130.677163	4970.633360	23.958093
130.656897	4992.150905	23.963111
131.116938	4996.760960	23.968128
131.447128	5005.778961	23.973146
131.580204	5006.003464	23.978163
131.378193	5001.197136	23.983181
131.248754	5008.581564	23.988199
131.577993	5024.478365	23.993216
131.983987	5026.244004	23.998234
131.772034	5024.508884	24.003251
132.387047	5032.220967	24.008269
132.313567	5037.796800	24.013287
132.554137	5031.837858	24.018304
132.571391	5037.116941	24.023322
132.886509	5036.201211	24.028339
133.636815	5036.386065	24.033357
133.110058	5036.770944	24.038375
133.682971	5027.218436	24.043392
133.517015	5043.243470	24.048410
133.760341	5028.634758	24.053427
134.594182	5029.685895	24.058445
134.086760	5026.192173	24.063463
133.915551	5012.922672	24.068480
133.920153	5024.101125	24.073498
133.847976	5031.700230	24.078515
133.796823	5022.951789	24.083533
133.748688	5033.614708	24.088551
134.170906	5056.212769	24.093568
133.990464	5067.326093	24.098586
134.025743	5075.032823	24.103603
134.396623	5090.518482	24.108621
134.233668	5097.199800	24.113639
134.383886	5106.949732	24.118656
134.609940	5131.622367	24.123674
134.720880	5142.687366	24.128691
134.975468	5154.825754	24.133709
134.887832	5175.452431	24.138727
135.604191	5185.036830	24.143744
135.963623	5198.847612	24.148762
135.845310	5204.239786	24.153779
136.102679	5198.735538	24.158797
136.116619	5211.435085	24.163815
136.216792	5220.907742	24.168832
136.540932	5234.152758	24.173850
136.822143	5231.858106	24.178867
137.046373	5230.200208	24.183885
136.874385	5232.177592	24.188903
137.069514	5242.315318	24.193920
137.452378	5260.280251	24.198938
137.441401	5259.409385	24.203955
138.523438	5232.508454	24.208973
138.469692	5228.326467	24.213991
138.459429	5226.374797	24.219008
138.731298	5207.861275	24.224026
138.469580	5194.695357	24.229043
139.074101	5198.036188	24.234061
138.630748	5189.703039	24.239079
138.718976	5195.692299	24.244096
138.927127	5189.141017	24.249114
138.457191	5191.986285	24.254131
138.707908	5184.096548	24.259149
138.873486	5211.190726	24.264167
139.045485	5218.964670	24.269184
138.800574	5222.382599	24.274202
139.143843	5225.357847	24.279219
139.002176	5228.078318	24.284237
139.123447	5253.552837	24.289255
139.161696	5261.878259	24.294272
139.416210	5278.935764	24.299290
139.638433	5296.633688	24.304307
139.739205	5290.971939	24.309325
139.861249	5308.720132	24.314343
139.922943	5330.769156	24.319360
140.218720	5340.150852	24.324378
140.214367	5354.506980	24.329395
140.367889	5369.492191	24.334413
139.883569	5377.815887	24.339431
140.545041	5396.405101	24.344448
140.658473	5404.500309	24.349466
140.504515	5430.476785	24.354483
141.187504	5437.574840	24.359501
141.609661	5459.017173	24.364519
141.450550	5461.461835	24.369536
141.791529	5461.359262	24.374554
142.115235	5474.317837	24.379571
142.696373	5486.885711	24.384589
142.490659	5494.224363	24.389607
142.806284	5487.611212	24.394624
143.306627	5488.769181	24.399642
143.470511	5492.056435	24.404659
143.550360	5487.559247	24.409677
143.700648	5492.580159	24.414695
143.724663	5492.253871	24.419712
143.402430	5492.898290	24.424730
143.415671	5500.262424	24.429747
143.087406	5485.582718	24.434765
143.400190	5502.782497	24.439783
143.426485	5510.353922	24.444800
143.738340	5519.208370	24.449818
143.610329	5538.486835	24.454835
143.947584	5546.112094	24.459853
143.594511	5561.983833	24.464871
143.681744	5575.399716	24.469888
144.169645	5596.852232	24.474906
144.086047	5616.791924	24.479923
144.670624	5627.998194	24.484941
145.205519	5642.050250	24.489959
145.324671	5645.479899	24.494976
145.452641	5640.986235	24.499994
145.559758	5650.818720	24.505011
145.972343	5661.517294	24.510029
146.092648	5670.875705	24.515047
146.114769	5674.699298	24.520064
146.728814	5674.045791	24.525082
146.324729	5676.858586	24.530099
146.608674	5669.648207	24.535117
147.036551	5671.889873	24.540135
147.131219	5669.247472	24.545152
147.233606	5663.704255	24.550170
147.038611	5677.978353	24.555187
147.231871	5674.017782	24.560205
147.352875	5686.795453	24.565223
147.600166	5690.033004	24.570240
147.668864	5693.000273	24.575258
147.175182	5698.688543	24.580275
147.843410	5701.171006	24.585293
148.014337	5718.737197	24.590311
148.155918	5724.162973	24.595328
148.425101	5722.694243	24.600346
148.167686	5734.005546	24.605363
148.365685	5742.214036	24.610381
148.788553	5753.492229	24.615399
148.371190	5754.349889	24.620416
148.694837	5762.940150	24.625434
149.010941	5784.720121	24.630451
149.117917	5788.374807	24.635469
149.377742	5803.804582	24.640487
149.465642	5808.700017	24.645504
149.803236	5814.389973	24.650522
149.582936	5831.184456	24.655539
149.707307	5846.060110	24.660557
149.459727	5853.339149	24.665575
149.654304	5872.650938	24.670592
150.171744	5883.432513	24.675610
150.544575	5900.816205	24.680627
150.995416	5910.813635	24.685645
150.881081	5913.679988	24.690663
151.086629	5931.082937	24.695680
151.546117	5921.584003	24.700698
151.540749	5938.597758	24.705715
151.799523	5938.196558	24.710733
152.129568	5936.944234	24.715751
151.947119	5941.955374	24.720768
152.019329	5939.604290	24.725786
152.021450	5954.225305	24.730803
152.374692	5963.077634	24.735821
152.303569	5968.268987	24.740839
152.367484	5977.206369	24.745856
152.790857	5978.940782	24.750874
152.641564	5999.913084	24.755891
152.752403	6008.272926	24.760909
153.156960	6007.975130	24.765927
153.095933	6024.091865	24.770944
153.433887	6028.608937	24.775962
153.359510	6036.011183	24.780979
153.833675	6039.783366	24.785997
154.420934	6056.410502	24.791015
153.897890	6062.264626	24.796032
154.500732	6067.913929	24.801050
154.239984	6069.710490	24.806067
154.044567	6065.904676	24.811085
154.370708	6076.968882	24.816103
154.917811	6078.647436	24.821120
155.419498	6074.146301	24.826138
155.079063	6080.428363	24.831155
155.759912	6079.185998	24.836173
156.422922	6089.945123	24.841191
156.456363	6083.176084	24.846208
156.834479	6062.669352	24.851226
156.856592	6070.504856	24.856243
156.738816	6072.183958	24.861261
156.607534	6062.184404	24.866279
156.591781	6059.433258	24.871296
156.855812	6065.631386	24.876314
156.725372	6067.628530	24.881331
157.226333	6081.344140	24.886349
157.308810	6084.547797	24.891367
157.298041	6093.914747	24.896384
157.525813	6089.968638	24.901402
157.552601	6097.437855	24.906419
157.258223	6100.771498	24.911437
157.750340	6108.700534	24.916455
157.693198	6126.605604	24.921472
157.796944	6122.369601	24.926490
157.573451	6141.587179	24.931507
157.977320	6157.861455	24.936525
158.107365	6167.187767	24.941543
158.137638	6191.923181	24.946560
158.365704	6196.170047	24.951578
158.340118	6220.629139	24.956595
158.548102	6225.720739	24.961613
159.051507	6250.773722	24.966631
159.022286	6258.993861	24.971648
159.471967	6266.786098	24.976666
159.809600	6271.008687	24.981683
160.144658	6267.301728	24.986701
160.307163	6272.383810	24.991719
160.459134	6286.069623	24.996736
161.040032	6302.936789	25.001754
160.996723	6305.157707	25.006771
160.669896	6300.718978	25.011789
161.235241	6295.417571	25.016807
161.388729	6305.367760	25.021824
161.398142	6298.225430	25.026842
161.239605	6312.245711	25.031859
161.184095	6317.121774	25.036877
161.894175	6330.314151	25.041895
161.401892	6346.133333	25.046912
161.835107	6351.220236	25.051930
162.531308	6359.859601	25.056947
162.285504	6366.019209	25.061965
162.264921	6371.544690	25.066983
162.144239	6395.690294	25.072000
162.617436	6393.930520	25.077018
162.590375	6396.956873	25.082035
162.915199	6419.958772	25.087053
163.052589	6429.036632	25.092071
162.692988	6433.630862	25.097088
163.169297	6443.789688	25.102106
163.525124	6460.434866	25.107123
163.551232	6468.776391	25.112141
163.860656	6488.087357	25.117159
164.557919	6497.690012	25.122176
164.643049	6496.239374	25.127194
164.367054	6497.767615	25.132211
164.574192	6514.866078	25.137229
164.622085	6513.866103	25.142247
164.850779	6530.927015	25.147264
165.412457	6538.398485	25.152282
165.417818	6544.753001	25.157299
165.502313	6545.865757	25.162317
166.255147	6535.884496	25.167335
165.883174	6549.620966	25.172352
165.931810	6550.055327	25.177370
166.406558	6567.229282	25.182387
166.051110	6567.279965	25.187405
166.774605	6576.489818	25.192423
166.674215	6606.506414	25.197440
167.135929	6601.855226	25.202458
167.402975	6605.428307	25.207475
167.475140	6603.315030	25.212493
167.709107	6601.519047	25.217511
167.451814	6624.276001	25.222528
167.636694	6626.170321	25.227546
167.434666	6640.032132	25.232563
167.511589	6650.380866	25.237581
167.789364	6651.291920	25.242599
167.856584	6680.178661	25.247616
168.182356	6695.523161	25.252634
168.085244	6702.020557	25.257651
168.556517	6715.195111	25.262669
168.961203	6737.309383	25.267687
169.069066	6736.600820	25.272704
168.954260	6752.315517	25.277722
169.578051	6764.047601	25.282739
169.454685	6773.702085	25.287757
169.988298	6781.183208	25.292775
169.627916	6797.173220	25.297792
169.747425	6797.370931	25.302810
170.466105	6814.220536	25.307827
170.603105	6827.895988	25.312845
170.936016	6826.993656	25.317863
170.782684	6841.750841	25.322880
171.072076	6854.814107	25.327898
171.170926	6862.647085	25.332915
171.220339	6867.822005	25.337933
171.326355	6862.398278	25.342951
171.219488	6884.793445	25.347968
171.359219	6893.853050	25.352986
171.720098	6910.227633	25.358003
171.587740	6930.946958	25.363021
171.703707	6932.674308	25.368039
171.824244	6951.466787	25.373056
172.046193	6959.251927	25.378074
172.069312	6982.839667	25.383091
172.350173	7001.795359	25.388109
172.706042	7013.450665	25.393127
172.184668	7031.560793	25.398144
173.067000	7049.145143	25.403162
173.484726	7069.749868	25.408179
173.893762	7083.051196	25.413197
173.922627	7089.937577	25.418215
173.652400	7099.172347	25.423232
173.930849	7114.590747	25.428250
174.458538	7125.151626	25.433267
174.045249	7141.010038	25.438285
175.098242	7143.434659	25.443303
174.917136	7163.005414	25.448320
175.032745	7171.676216	25.453338
175.423855	7194.874263	25.458355
175.305119	7200.865882	25.463373
175.507250	7209.101205	25.468391
175.529822	7225.681418	25.473408
175.949584	7236.973802	25.478426
175.727913	7243.799999	25.483443
176.079851	7260.144175	25.488461
176.711639	7267.315648	25.493479
176.908400	7292.166020	25.498496
176.871823	7286.579892	25.503514
177.317418	7306.233244	25.508531
177.872383	7314.025280	25.513549
177.824459	7318.594691	25.518567
178.100692	7325.066940	25.523584
178.348655	7325.595561	25.528602
178.891013	7312.192369	25.533619
178.208679	7327.067466	25.538637
178.825845	7326.340896	25.543655
178.248179	7340.474887	25.548672
178.089494	7352.138295	25.553690
178.673196	7371.248120	25.558707
178.609619	7392.336745	25.563725
178.970744	7400.686711	25.568743
179.399188	7410.512466	25.573760
179.586385	7414.513789	25.578778
180.036396	7412.134752	25.583795
180.357311	7424.799980	25.588813
180.608804	7422.223366	25.593831
180.808391	7431.124912	25.598848
180.925724	7431.752344	25.603866
181.069208	7424.263540	25.608883
180.815108	7426.479782	25.613901
181.341038	7438.299253	25.618919
181.628554	7438.879394	25.623936
181.249701	7450.195390	25.628954
181.644440	7449.044518	25.633971
181.645893	7460.842047	25.638989
181.955637	7461.969036	25.644007
182.623903	7477.398167	25.649024
182.359387	7487.876085	25.654042
182.498559	7481.484585	25.659059
182.307309	7496.582102	25.664077
183.109109	7505.444268	25.669095
182.989889	7519.996919	25.674112
182.918447	7520.375476	25.679130
183.031621	7530.664209	25.684148
183.001228	7556.968002	25.689165
183.111766	7560.537404	25.694183
183.444866	7583.216568	25.699200
183.665139	7598.524088	25.704218
184.028702	7610.233658	25.709236
183.822416	7634.836961	25.714253
184.075716	7646.003765	25.719271
183.964040	7665.279625	25.724288
183.892604	7693.315149	25.729306
184.627408	7710.457573	25.734324
184.606535	7736.570170	25.739341
184.876050	7758.515228	25.744359
184.934330	7775.692551	25.749376
185.121104	7794.419518	25.754394
185.494795	7813.498910	25.759412
185.813422	7839.722066	25.764429
186.203937	7840.990433	25.769447
186.442336	7866.904389	25.774464
186.425593	7872.844898	25.779482
187.054777	7884.343697	25.784500
187.195645	7907.855102	25.789517
187.542902	7909.097015	25.794535
187.387527	7916.211496	25.799552
187.724055	7926.833250	25.804570
187.886248	7941.066249	25.809588
187.892983	7953.816477	25.814605
188.421146	7972.682870	25.819623
188.599539	7973.726847	25.824640
188.534591	7978.815376	25.829658
188.809865	7981.809109	25.834676
189.015938	7996.411994	25.839693
188.971311	8011.814162	25.844711
189.837444	8020.333135	25.849728
189.531874	8030.781415	25.854746
189.403566	8037.186221	25.859764
189.927222	8056.971283	25.864781
189.790300	8069.870702	25.869799
190.206044	8088.586336	25.874816
189.965556	8111.740356	25.879834
190.267392	8110.158676	25.884852
190.322427	8134.975562	25.889869
190.430397	8148.520038	25.894887
190.831811	8171.836693	25.899904
190.565497	8186.299351	25.904922
191.078296	8201.588027	25.909940
191.054160	8228.325931	25.914957
191.277973	8237.806757	25.919975
191.372708	8262.448441	25.924992
191.412207	8286.653724	25.930010
191.997277	8315.758735	25.935028
191.983179	8326.648843	25.940045
192.331060	8349.512481	25.945063
192.746005	8363.849063	25.950080
193.111480	8380.850683	25.955098
193.319059	8396.218651	25.960116
193.479734	8422.995314	25.965133
193.943897	8420.344272	25.970151
194.325611	8433.055811	25.975168
194.256113	8454.312285	25.980186
194.491503	8458.252824	25.985204
194.677933	8457.525205	25.990221
194.990465	8483.574770	25.995239
195.427134	8485.320583	26.000256
195.358117	8485.054302	26.005274
195.433913	8487.054994	26.010292
195.779325	8517.350109	26.015309
196.299746	8517.275860	26.020327
196.542513	8516.761538	26.025344
196.440306	8524.239028	26.030362
196.788709	8536.728676	26.035380
196.801656	8548.225656	26.040397
197.057505	8558.281025	26.045415
196.942638	8556.149922	26.050432
197.328864	8578.191117	26.055450
197.251252	8579.430283	26.060468
197.220023	8597.881997	26.065485
197.433271	8617.943130	26.070503
197.880787	8626.615336	26.075520
197.796428	8651.192985	26.080538
198.285115	8657.945280	26.085556
198.046289	8675.846517	26.090573
197.956895	8689.819199	26.095591
198.325320	8711.323957	26.100608
198.620997	8734.133276	26.105626
199.140086	8760.243210	26.110644
198.988611	8779.506739	26.115661
199.104730	8799.907763	26.120679
199.307826	8809.924275	26.125696
199.333404	8822.917767	26.130714
200.042378	8845.711546	26.135732
200.866561	8853.259653	26.140749
200.897067	8868.382678	26.145767
201.094419	8882.307949	26.150784
201.022246	8888.578989	26.155802
201.371386	8888.451377	26.160820
201.688235	8911.978988	26.165837
201.967634	8918.993382	26.170855
202.008253	8916.715824	26.175872
202.151063	8929.468709	26.180890
202.194153	8929.045328	26.185908
203.001383	8945.339965	26.190925
202.667874	8944.342979	26.195943
203.074346	8955.722369	26.200960
203.339336	8971.456064	26.205978
203.490848	8973.424929	26.210996
204.106400	8978.003984	26.216013
203.889547	8977.636191	26.221031
204.331411	8978.263206	26.226048
204.126644	9005.488739	26.231066
204.643293	8997.414469	26.236084
204.864480	9007.062437	26.241101
204.874050	9017.919016	26.246119
204.419740	9035.677957	26.251136
205.030585	9049.313469	26.256154
205.371553	9059.501891	26.261172
205.374025	9069.916945	26.266189
205.704504	9070.564632	26.271207
206.940671	9068.316899	26.276224
207.278056	9076.260550	26.281242
207.177415	9071.597912	26.286260
207.998406	9074.756725	26.291277
207.541008	9064.871863	26.296295
207.726302	9060.768441	26.301312
207.904211	9077.451566	26.306330
208.219244	9073.519715	26.311348
208.318234	9073.496435	26.316365
207.785554	9080.260901	26.321383
208.033792	9075.161862	26.326400
208.177321	9088.433161	26.331418
208.223442	9103.892510	26.336436
208.478919	9110.380071	26.341453
208.138872	9131.748417	26.346471
208.596011	9149.556090	26.351488
208.532091	9179.148147	26.356506
208.695992	9193.385113	26.361524
208.838079	9207.881098	26.366541
209.278255	9243.237551	26.371559
209.937509	9258.732189	26.376576
209.882860	9288.032920	26.381594
209.799979	9296.447382	26.386612
209.917601	9309.945483	26.391629
210.606697	9337.814102	26.396647
210.888752	9337.467930	26.401664
211.040473	9366.322159	26.406682
210.994350	9375.187327	26.411700
211.437808	9402.540350	26.416717
211.585257	9416.755120	26.421735
212.068874	9428.370591	26.426752
211.901033	9455.779642	26.431770
211.873797	9465.300287	26.436788
212.354551	9482.855311	26.441805
212.788567	9502.444792	26.446823
212.514103	9526.005325	26.451840
212.678562	9540.362259	26.456858
212.827933	9551.666384	26.461876
213.497601	9570.919311	26.466893
213.656801	9591.646438	26.471911
214.079879	9611.018894	26.476928
214.321745	9630.464981	26.481946
214.269444	9633.012506	26.486964
214.521384	9652.551440	26.491981
214.449005	9672.082959	26.496999
214.813704	9688.414814	26.502016
214.995969	9705.868395	26.507034
215.220213	9728.021658	26.512052
215.410200	9751.372114	26.517069
215.614489	9766.970442	26.522087
215.894231	9781.500073	26.527104
215.944046	9801.604874	26.532122
216.000165	9827.034790	26.537140
216.465285	9840.302006	26.542157
216.702850	9866.750360	26.547175
217.499255	9872.680646	26.552192
217.841686	9907.245347	26.557210
218.265228	9905.456694	26.562228
218.834235	9905.136962	26.567245
218.584162	9911.404224	26.572263
218.748131	9935.630823	26.577280
218.674971	9943.386844	26.582298
218.517858	9957.570778	26.587316
218.886565	9966.083092	26.592333
218.884097	9990.703889	26.597351
219.265831	10006.353973	26.602368
219.488589	10028.047764	26.607386
219.479280	10045.917473	26.612404
220.073385	10058.606497	26.617421
220.159260	10080.706745	26.622439
220.346128	10090.076022	26.627456
220.874252	10103.721881	26.632474
220.524247	10112.946825	26.637492
221.061220	10136.540916	26.642509
221.252923	10162.422440	26.647527
221.959493	10169.646230	26.652544
222.004585	10191.473123	26.657562
222.096779	10208.638551	26.662580
222.437083	10210.928194	26.667597
222.447328	10237.561094	26.672615
223.138381	10238.069811	26.677632
223.378552	10247.147968	26.682650
223.644426	10265.911520	26.687668
223.771265	10267.859562	26.692685
224.114149	10280.481515	26.697703
224.531411	10293.990532	26.702720
224.265667	10305.591685	26.707738
224.388361	10308.700258	26.712756
224.410662	10304.911266	26.717773
224.544524	10334.131145	26.722791
224.786129	10332.720318	26.727808
225.182108	10354.162660	26.732826
225.182247	10365.555968	26.737844
225.757795	10377.438442	26.742861
225.297678	10405.190724	26.747879
225.913770	10420.273128	26.752896
225.854133	10436.010315	26.757914
225.910310	10455.599532	26.762932
225.975947	10469.334431	26.767949
226.291938	10503.514124	26.772967
226.746610	10519.539862	26.777984
227.158467	10545.407897	26.783002
227.121297	10561.656660	26.788020
227.596217	10576.282770	26.793037
227.820311	10614.047778	26.798055
228.406421	10615.540505	26.803072
228.442605	10643.827437	26.808090
228.255124	10665.617614	26.813108
228.716293	10679.005963	26.818125
228.665383	10698.957369	26.823143
228.947617	10721.582690	26.828160
229.504678	10736.539982	26.833178
229.655997	10762.514481	26.838196
229.636116	10787.442038	26.843213
229.903014	10800.512366	26.848231
229.983767	10821.582294	26.853248
230.726476	10848.976291	26.858266
230.724677	10866.185315	26.863284
231.336218	10876.194556	26.868301
231.574925	10893.907643	26.873319
232.149357	10910.234722	26.878336
232.330312	10918.826999	26.883354
232.829742	10922.254057	26.888372
233.434368	10920.996853	26.893389
233.382706	10944.804909	26.898407
233.644420	10950.059789	26.903424
233.697989	10941.929990	26.908442
234.254818	10956.302868	26.913460
234.901463	10953.779315	26.918477
234.373613	10953.578244	26.923495
234.649374	10967.948881	26.928512
235.265036	10979.895839	26.933530
234.831463	10982.909207	26.938548
235.318368	10982.449098	26.943565
235.030086	11004.496543	26.948583
235.119887	11014.901027	26.953600
235.182401	11024.894156	26.958618
235.199147	11065.359035	26.963636
235.620629	11076.355980	26.968653
235.710396	11090.653021	26.973671
235.358264	11131.690313	26.978688
236.161650	11147.017077	26.983706
235.784329	11172.944164	26.988724
236.452901	11192.081018	26.993741
236.514930	11219.289739	26.998759
236.334659	11237.500516	27.003776
237.309667	11251.653839	27.008794
237.461471	11278.664463	27.013812
237.930504	11302.254561	27.018829
238.281183	11326.150226	27.023847
238.492626	11331.112843	27.028864
239.120915	11341.388987	27.033882
239.301819	11357.908472	27.038900
239.273286	11371.947095	27.043917
239.110032	11407.567718	27.048935
239.701692	11415.270368	27.053952
239.756345	11436.857747	27.058970
240.004754	11465.007290	27.063988
240.255353	11480.561503	27.069005
240.877634	11497.549176	27.074023
240.841547	11518.074264	27.079040
241.046142	11534.698608	27.084058
241.090277	11554.305393	27.089076
241.748654	11569.723604	27.094093
242.255683	11589.519001	27.099111
242.278266	11601.623236	27.104128
242.849153	11611.059947	27.109146
243.092035	11632.232362	27.114164
243.328402	11632.239117	27.119181
243.469753	11657.337362	27.124199
243.391473	11667.556741	27.129216
243.804973	11685.719824	27.134234
243.838456	11704.509110	27.139252
243.832321	11720.449544	27.144269
244.228536	11748.804333	27.149287
244.267389	11763.296655	27.154304
244.672663	11787.527201	27.159322
244.343255	11820.986591	27.164340
244.970535	11836.183444	27.169357
245.213293	11856.910167	27.174375
245.434785	11892.098691	27.179392
245.978089	11911.985973	27.184410
246.292139	11931.888936	27.189428
246.915605	11951.597047	27.194445
246.808584	11970.322466	27.199463
247.161511	11994.040636	27.204480
247.352913	11997.388340	27.209498
247.681447	12028.949770	27.214516
248.288946	12034.139429	27.219533
248.484222	12051.137832	27.224551
248.423684	12066.470134	27.229568
249.014589	12081.287330	27.234586
248.638925	12104.823225	27.239604
249.641737	12095.516772	27.244621
250.549908	12102.739977	27.249639
250.437410	12104.962515	27.254656
250.959091	12104.518484	27.259674
250.451161	12107.656695	27.264692
251.278708	12100.246279	27.269709
251.198023	12106.425454	27.274727
251.262115	12102.518561	27.279744
251.594545	12121.148340	27.284762
251.365343	12137.316537	27.289780
251.866718	12138.844428	27.294797
251.681112	12155.996483	27.299815
251.665894	12176.099600	27.304832
252.410614	12185.237353	27.309850
252.366269	12215.391056	27.314868
252.745012	12229.133658	27.319885
252.904471	12255.769492	27.324903
252.481951	12275.565874	27.329920
253.381564	12289.060068	27.334938
253.693360	12324.079592	27.339956
253.790856	12330.042338	27.344973
254.484051	12345.102288	27.349991
254.618220	12359.499999	27.355008
254.974517	12363.577588	27.360026
254.661202	12392.464882	27.365044
255.131841	12410.497623	27.370061
255.604236	12433.070661	27.375079
255.464880	12452.780895	27.380096
256.182095	12472.738344	27.385114
256.106131	12497.679697	27.390132
256.309311	12515.197325	27.395149
256.276144	12540.095157	27.400167
256.710172	12565.926352	27.405184
257.298327	12580.474969	27.410202
257.299211	12603.860352	27.415220
257.248956	12624.089804	27.420237
258.180433	12654.304005	27.425255
258.260933	12667.141426	27.430272
258.816666	12687.941643	27.435290
258.667167	12709.256783	27.440308
259.422767	12737.157670	27.445325
259.524146	12743.001696	27.450343
259.683658	12760.768210	27.455360
260.435473	12775.050962	27.460378
260.428363	12796.308712	27.465396
260.769037	12809.676918	27.470413
261.183202	12818.099409	27.475431
261.154937	12839.089755	27.480448
261.280910	12842.872814	27.485466
261.478403	12865.816666	27.490484
262.080289	12872.227448	27.495501
262.848331	12886.260071	27.500519
262.413172	12896.369592	27.505536
262.949975	12902.351814	27.510554
263.069225	12917.603659	27.515572
263.278587	12929.448327	27.520589
263.651994	12952.592257	27.525607
264.045300	12974.870685	27.530624
264.326843	12978.797330	27.535642
264.056773	12988.218226	27.540660
264.515242	13009.530418	27.545677
264.275011	13013.423569	27.550695
264.444870	13043.360825	27.555712
264.414171	13062.118538	27.560730
264.538557	13095.991332	27.565748
264.525917	13117.787897	27.570765
264.590609	13147.541627	27.575783
264.470790	13188.202224	27.580800
265.330098	13222.381166	27.585818
265.526225	13266.444229	27.590836
265.732090	13292.392906	27.595853
266.590059	13324.769205	27.600871
266.448909	13358.387012	27.605888
267.230784	13379.494519	27.610906
267.587377	13404.607406	27.615924
268.084630	13430.536303	27.620941
268.606646	13437.189539	27.625959
268.406408	13473.604322	27.630976
269.030107	13493.566439	27.635994
268.881633	13506.755839	27.641012
268.818461	13538.070508	27.646029
269.500654	13561.096170	27.651047
270.020766	13586.482352	27.656064
270.039429	13603.254148	27.661082
270.173637	13632.814005	27.666100
270.281384	13657.662580	27.671117
270.821135	13685.138688	27.676135
270.926420	13718.839507	27.681152
271.293404	13739.421225	27.686170
271.551300	13767.834740	27.691188
271.680824	13801.933497	27.696205
272.436275	13823.273075	27.701223
272.418088	13854.754013	27.706240
272.666896	13870.377004	27.711258
273.202835	13895.480390	27.716276
273.227627	13924.730102	27.721293
273.708378	13944.483993	27.726311
273.642516	13973.952659	27.731328
273.967356	14002.712899	27.736346
274.805674	14023.486867	27.741364
275.061238	14053.682374	27.746381
275.590942	14067.922367	27.751399
275.083363	14091.058129	27.756416
275.257702	14114.546750	27.761434
275.519864	14138.266240	27.766452
275.927743	14163.150824	27.771469
277.122207	14184.393558	27.776487
277.062302	14198.113697	27.781504
277.489246	14217.320736	27.786522
277.759321	14234.978471	27.791540
278.005893	14262.803699	27.796557
278.135106	14273.539231	27.801575
278.192957	14300.066540	27.806592
278.627639	14307.554737	27.811610
279.275353	14336.316963	27.816628
278.965522	14342.897206	27.821645
279.570028	14357.597497	27.826663
279.668411	14374.080572	27.831680
280.067670	14390.118036	27.836698
280.320540	14406.967145	27.841716
280.484978	14430.264036	27.846733
280.866832	14433.470839	27.851751
281.176953	14454.310666	27.856768
281.567238	14466.828433	27.861786
282.057520	14472.819208	27.866804
282.001021	14506.021323	27.871821
282.284631	14510.703003	27.876839
282.266653	14539.306993	27.881856
282.676291	14551.630782	27.886874
282.910342	14581.156308	27.891892
282.986906	14594.536559	27.896909
283.698041	14617.648589	27.901927
283.820983	14641.893912	27.906944
283.714708	14650.335620	27.911962
284.149407	14681.343291	27.916980
284.076489	14713.016513	27.921997
284.256052	14734.046154	27.927015
284.237053	14772.360499	27.932032
284.720785	14793.089031	27.937050
285.005281	14830.361595	27.942068
285.241763	14873.172047	27.947085
286.206256	14885.292221	27.952103
286.799852	14923.284391	27.957120
287.682244	14916.905261	27.962138
288.134624	14925.620205	27.967156
287.994670	14956.761566	27.972173
288.440365	14960.244415	27.977191
288.775939	14969.747053	27.982208
289.121181	14979.005292	27.987226
289.290628	14988.165988	27.992244
289.145861	15015.075955	27.997261
289.745808	15026.497370	28.002279
289.591170	15043.557264	28.007296
289.797209	15066.572070	28.012314
290.540673	15082.513381	28.017332
290.640217	15101.889484	28.022349
291.506535	15106.293338	28.027367
291.391615	15133.267738	28.032384
291.482847	15133.392383	28.037402
291.837300	15147.266122	28.042420
291.837171	15183.234223	28.047437
292.453522	15192.061496	28.052455
292.634371	15217.558782	28.057472
292.893709	15237.919646	28.062490
293.120582	15250.497543	28.067508
293.510168	15279.482204	28.072525
293.955046	15292.546104	28.077543
293.846468	15324.472510	28.082560
294.159668	15337.804921	28.087578
294.343113	15354.091539	28.092596
294.430391	15388.216570	28.097613
295.078144	15393.009484	28.102631
295.087367	15421.209947	28.107648
297.354005	15390.864945	28.112666
298.755917	15360.493236	28.117684
298.678113	15349.149168	28.122701
299.117944	15334.513306	28.127719
299.308433	15318.369096	28.132736
299.437696	15308.249044	28.137754
299.430156	15284.228852	28.142772
299.175074	15285.741689	28.147789
299.492084	15272.510937	28.152807
299.454993	15271.178995	28.157824
299.338422	15276.482770	28.162842
299.493913	15278.476945	28.167860
299.517295	15312.592282	28.172877
299.932688	15305.698777	28.177895
299.610887	15338.840843	28.182912
299.908186	15355.796802	28.187930
300.303694	15377.111819	28.192948
300.156344	15407.282702	28.197965
300.591329	15431.042209	28.202983
300.745681	15465.173243	28.208000
300.876977	15493.105422	28.213018
301.281474	15519.690344	28.218036
301.395088	15554.249425	28.223053
301.387680	15588.605480	28.228071
301.697091	15630.585691	28.233088
302.315822	15664.029071	28.238106
302.825643	15692.683307	28.243124
302.867709	15734.823100	28.248141
303.519826	15767.622542	28.253159
303.837053	15798.887320	28.258176
303.605850	15827.747614	28.263194
303.628069	15858.506610	28.268212
303.813468	15900.016928	28.273229
304.343616	15943.013111	28.278247
304.357186	15989.597511	28.283264
305.023447	16034.906800	28.288282
305.393743	16065.792533	28.293300
305.337889	16105.851873	28.298317
305.666605	16131.240093	28.303335
306.484966	16179.134216	28.308352
306.985118	16218.136927	28.313370
307.938079	16234.636175	28.318388
308.681953	16252.322053	28.323405
308.994352	16275.392820	28.328423
309.359689	16290.599294	28.333440
309.473463	16306.200437	28.338458
310.055258	16325.069681	28.343476
310.182660	16345.151846	28.348493
310.220724	16366.950300	28.353511
310.529116	16383.933783	28.358528
310.782851	16400.184157	28.363546
311.128304	16415.594359	28.368564
311.057127	16441.095731	28.373581
311.767754	16456.519051	28.378599
311.629554	16470.732141	28.383616
312.133568	16496.385665	28.388634
312.334549	16520.385468	28.393652
312.593197	16542.321329	28.398669
313.094016	16568.818905	28.403687
313.266199	16584.916335	28.408704
313.244678	16623.850187	28.413722
313.737505	16646.455447	28.418740
314.266655	16669.406059	28.423757
314.670876	16695.660280	28.428775
314.785087	16722.930611	28.433792
314.754488	16747.288874	28.438810
315.325143	16768.340766	28.443828
315.410979	16790.907202	28.448845
315.925662	16828.903073	28.453863
316.161309	16849.364560	28.458880
316.617385	16883.650150	28.463898
316.891756	16908.342613	28.468916
317.338461	16936.021363	28.473933
317.675549	16959.005293	28.478951
317.552339	16985.232131	28.483968
317.685576	17017.930641	28.488986
318.643950	17042.488729	28.494004
318.534205	17073.602065	28.499021
319.024478	17105.383523	28.504039
319.108226	17132.716497	28.509056
319.244083	17176.652087	28.514074
319.887649	17202.181885	28.519092
319.982577	17247.310201	28.524109
320.495074	17278.236868	28.529127
321.193665	17310.678251	28.534144
321.103028	17350.934140	28.539162
321.663486	17370.183437	28.544180
321.673470	17402.840763	28.549197
322.008531	17430.189481	28.554215
323.112335	17450.365753	28.559232
323.436992	17488.681044	28.564250
323.831070	17492.403456	28.569268
324.439790	17525.458161	28.574285
324.924224	17543.224565	28.579303
325.194886	17566.515526	28.584320
325.051194	17579.590665	28.589338
325.430991	17601.915475	28.594356
325.666254	17627.941568	28.599373
325.457907	17651.261142	28.604391
325.552593	17673.072088	28.609408
325.953803	17715.458016	28.614426
326.361393	17754.899544	28.619444
326.656812	17782.943007	28.624461
326.502911	17817.886849	28.629479
326.958095	17851.007926	28.634496
327.091334	17896.041557	28.639514
327.696896	17931.180242	28.644532
327.616101	17965.482811	28.649549
327.629156	17987.405903	28.654567
328.317992	18022.830056	28.659584
328.575394	18061.259083	28.664602
329.277581	18090.707444	28.669620
329.847459	18122.939129	28.674637
330.598192	18145.588929	28.679655
331.407410	18171.834390	28.684672
331.926938	18196.005876	28.689690
332.157132	18219.323599	28.694708
332.491382	18230.007624	28.699725
332.098416	18253.391204	28.704743
333.036193	18267.184915	28.709760
332.929579	18298.186468	28.714778
333.706007	18311.541196	28.719796
333.498613	18334.041719	28.724813
333.702368	18359.484698	28.729831
334.427058	18387.845022	28.734848
334.561073	18421.629264	28.739866
334.851330	18455.276433	28.744884
334.766736	18483.006232	28.749901
334.675793	18518.274980	28.754919
335.327117	18539.506051	28.759936
335.707374	18581.661264	28.764954
335.994835	18614.744799	28.769972
336.508157	18648.182271	28.774989
336.746384	18683.670859	28.780007
337.654709	18710.273842	28.785024
337.887114	18741.779389	28.790042
338.096949	18762.179839	28.795060
339.027421	18793.498049	28.800077
339.578017	18797.047303	28.805095
340.407036	18799.120399	28.810112
341.020418	18823.606224	28.815130
341.101912	18821.238313	28.820148
340.970661	18835.292969	28.825165
341.598681	18859.855170	28.830183
342.205433	18862.696358	28.835200
341.940871	18902.005090	28.840218
342.298330	18905.087668	28.845236
342.613751	18923.841535	28.850253
342.053943	18944.169147	28.855271
342.979224	18970.739681	28.860288
343.046420	19002.362324	28.865306
342.913818	19022.304633	28.870324
343.417824	19061.086270	28.875341
343.907218	19092.073851	28.880359
344.123507	19115.833514	28.885376
344.651804	19153.676233	28.890394
344.790965	19176.476390	28.895412
345.249093	19218.022289	28.900429
345.216167	19244.303394	28.905447
345.434498	19270.896233	28.910464
345.811790	19311.978480	28.915482
346.374649	19353.492573	28.920500
346.736376	19381.180465	28.925517
346.998616	19405.604335	28.930535
347.606199	19421.623560	28.935552
347.894862	19454.681735	28.940570
347.942883	19484.944716	28.945588
349.003993	19504.755538	28.950605
349.102688	19546.929888	28.955623
349.465837	19573.272913	28.960640
349.619073	19601.969734	28.965658
350.174142	19624.730751	28.970676
350.170520	19658.479566	28.975693
350.765150	19698.465946	28.980711
351.063861	19719.028917	28.985728
351.222589	19762.300379	28.990746
351.534531	19789.393584	28.995764
351.974482	19816.406553	29.000781
352.592500	19853.306764	29.005799
352.498854	19882.252925	29.010816
352.848666	19921.772502	29.015834
353.202180	19949.599911	29.020852
353.658837	19987.489889	29.025869
354.111651	20035.366233	29.030887
354.966328	20054.867774	29.035904
354.875017	20087.959196	29.040922
355.698805	20108.320700	29.045940
356.022092	20133.287029	29.050957
355.955732	20162.033471	29.055975
356.623202	20186.787945	29.060992
356.789576	20221.845853	29.066010
357.409877	20250.350198	29.071028
357.583710	20281.312051	29.076045
357.998562	20307.316235	29.081063
358.280709	20325.780927	29.086080
358.794801	20360.240267	29.091098
358.982810	20405.428884	29.096116
359.485539	20422.208127	29.101133
359.497889	20452.571979	29.106151
360.006543	20489.033472	29.111168
360.495860	20513.490981	29.116186
360.569719	20548.961198	29.121204
361.206314	20578.097181	29.126221
361.324598	20616.702511	29.131239
362.120173	20638.553274	29.136256
362.308658	20667.176478	29.141274
362.426741	20701.283369	29.146292
363.331259	20731.469590	29.151309
363.074433	20759.972165	29.156327
363.658369	20786.135749	29.161344
364.112610	20828.531450	29.166362
364.379411	20854.574462	29.171380
364.926328	20880.156375	29.176397
365.544945	20911.421591	29.181415
365.732772	20922.955533	29.186432
366.001565	20949.985453	29.191450
366.086147	20989.868344	29.196468
366.858280	21000.199982	29.201485
366.985276	21034.898911	29.206503
367.797613	21054.129763	29.211520
368.328616	21074.222511	29.216538
368.473493	21098.481291	29.221556
368.480756	21113.980572	29.226573
368.578105	21153.093726	29.231591
369.320393	21167.995606	29.236608
369.378428	21196.708286	29.241626
369.952211	21235.087154	29.246644
370.490407	21257.739727	29.251661
370.311633	21292.212476	29.256679
370.521481	21322.264926	29.261696
370.465937	21356.234159	29.266714
371.188141	21404.460841	29.271732
371.995766	21435.026030	29.276749
371.569626	21476.355288	29.281767
371.869934	21513.931706	29.286784
372.475116	21546.700025	29.291802
372.807629	21593.604778	29.296820
373.528371	21631.415321	29.301837
373.821259	21675.917575	29.306855
374.220783	21713.199892	29.311872
374.788845	21745.063497	29.316890
375.003814	21773.931599	29.321908
375.742941	21816.403937	29.326925
375.873095	21858.498206	29.331943
376.173260	21884.456652	29.336960
376.901712	21910.767511	29.341978
377.451142	21950.219749	29.346996
378.120507	21975.118435	29.352013
378.303938	22003.904023	29.357031
378.401140	22030.600791	29.362048
379.065199	22064.025486	29.367066
379.264572	22082.107304	29.372084
379.893384	22100.090313	29.377101
380.133753	22146.367403	29.382119
380.875464	22167.986521	29.387136
381.061465	22186.638446	29.392154
381.342708	22220.144823	29.397172
382.054542	22243.967444	29.402189
382.142017	22274.198662	29.407207
382.074334	22303.658577	29.412224
382.560549	22344.765764	29.417242
382.595632	22381.843912	29.422260
383.396795	22411.877369	29.427277
383.532396	22454.697583	29.432295
384.408958	22485.787443	29.437312
384.573437	22512.555437	29.442330
384.678305	22555.185622	29.447348
384.891749	22589.748312	29.452365
385.762932	22636.044779	29.457383
385.990379	22658.679930	29.462400
385.933732	22693.834759	29.467418
386.255455	22727.029252	29.472436
387.001749	22758.879975	29.477453
386.957752	22798.085773	29.482471
387.633233	22826.107147	29.487488
388.235539	22865.565053	29.492506
387.965633	22898.618407	29.497524
388.583486	22934.538116	29.502541
388.948410	22976.424580	29.507559
389.395910	23016.335162	29.512576
389.708300	23059.517693	29.517594
389.905328	23099.748952	29.522612
390.397688	23138.948769	29.527629
390.442313	23184.792248	29.532647
391.065902	23230.451468	29.537664
391.517692	23254.263290	29.542682
392.035736	23303.716270	29.547700
392.674310	23332.445014	29.552717
392.934504	23373.855197	29.557735
393.229666	23408.563237	29.562752
394.161670	23447.325689	29.567770
393.923333	23484.257517	29.572788
394.618686	23524.010099	29.577805
394.939239	23571.494800	29.582823
395.117449	23613.506286	29.587840
395.949635	23656.680092	29.592858
395.512130	23700.090524	29.597876
396.358655	23740.757652	29.602893
396.439146	23785.268662	29.607911
397.127257	23833.287241	29.612928
397.274408	23876.402360	29.617946
397.829211	23915.028639	29.622964
398.986114	23952.567698	29.627981
399.187848	23994.014625	29.632999
399.816748	24023.992114	29.638016
400.138963	24052.801513	29.643034
400.480364	24097.221302	29.648052
401.042955	24122.942600	29.653069
401.398046	24153.989224	29.658087
401.609871	24196.485283	29.663104
402.366492	24231.374553	29.668122
402.405631	24272.887866	29.673140
402.929057	24299.988262	29.678157
403.428801	24338.952976	29.683175
403.729612	24378.904476	29.688192
404.122185	24405.055931	29.693210
404.316332	24462.172827	29.698228
404.897437	24488.528675	29.703245
405.266368	24532.408628	29.708263
405.539266	24566.936711	29.713280
405.710384	24604.819621	29.718298
405.905094	24655.161488	29.723316
406.696370	24685.298410	29.728333
406.890348	24734.669086	29.733351
407.158907	24774.172794	29.738368
407.515472	24808.292722	29.743386
407.867183	24864.021242	29.748404
408.549079	24897.028865	29.753421
409.130530	24938.419294	29.758439
409.199319	24963.838477	29.763456
410.020653	24986.731364	29.768474
410.459316	25037.881080	29.773492
411.001494	25066.878442	29.778509
411.164139	25103.836488	29.783527
411.710224	25129.640979	29.788544
412.513134	25152.442611	29.793562
412.689937	25188.291195	29.798580
413.442933	25208.893327	29.803597
413.610451	25245.999101	29.808615
414.249428	25268.961469	29.813632
414.970451	25302.303846	29.818650
414.987196	25323.461297	29.823668
415.421034	25356.159005	29.828685
415.428971	25390.342979	29.833703
416.068562	25417.989881	29.838720
416.612717	25452.668826	29.843738
416.910252	25486.412201	29.848756
417.498318	25520.547488	29.853773
417.725828	25555.009611	29.858791
417.910579	25591.797719	29.863808
418.609589	25623.444190	29.868826
418.529666	25656.858262	29.873844
419.743620	25682.814110	29.878861
419.652204	25715.864337	29.883879
419.977539	25762.429949	29.888896
420.468409	25790.096623	29.893914
421.079371	25826.556668	29.898932
421.437881	25863.703589	29.903949
421.929442	25906.184296	29.908967
422.369841	25932.333020	29.913984
423.116089	25967.391616	29.919002
422.924197	26013.816251	29.924020
423.614603	26038.991680	29.929037
423.755823	26075.119490	29.934055
424.091817	26123.807310	29.939072
424.863059	26158.164833	29.944090
424.731134	26205.500858	29.949108
425.109359	26232.808983	29.954125
425.467970	26283.430333	29.959143
425.809311	26325.303720	29.964160
426.852790	26358.498232	29.969178
426.726824	26409.777142	29.974196
427.362178	26453.682549	29.979213
427.753545	26495.203909	29.984231
428.059359	26540.942107	29.989248
428.575724	26576.624949	29.994266
428.946028	26631.646143	29.999284
429.200227	26672.144060	30.004301
429.826815	26719.736373	30.009319
430.021413	26776.545328	30.014336
430.637855	26797.712218	30.019354
431.103340	26854.919827	30.024372
431.349853	26893.936834	30.029389
432.048596	26942.252453	30.034407
432.091378	26986.112473	30.039424
432.706051	27014.775723	30.044442
433.324309	27064.118163	30.049460
433.585463	27099.536639	30.054477
433.862950	27141.763647	30.059495
434.367888	27190.144713	30.064512
434.823386	27235.594074	30.069530
435.252520	27285.751949	30.074548
435.846233	27322.965784	30.079565
436.392507	27366.708928	30.084583
436.644955	27411.322800	30.089600
437.053801	27454.427191	30.094618
437.486877	27497.660041	30.099636
437.772441	27547.682371	30.104653
438.321540	27580.588503	30.109671
438.310180	27637.609066	30.114688
439.242039	27676.986766	30.119706
439.847556	27729.014947	30.124724
440.090523	27771.984489	30.129741
440.833235	27815.568896	30.134759
441.040725	27865.681231	30.139776
441.674157	27907.461030	30.144794
441.711147	27948.409267	30.149812
442.154570	28003.696728	30.154829
442.979267	28050.419492	30.159847
443.007689	28092.817672	30.164864
443.766778	28140.921188	30.169882
443.939191	28191.968035	30.174900
444.231470	28241.284469	30.179917
445.418834	28285.232395	30.184935
445.577117	28338.310771	30.189952
445.808748	28385.173917	30.194970
446.172663	28432.800128	30.199988
446.288042	28492.417285	30.205005
446.984607	28541.091058	30.210023
447.277679	28593.380423	30.215040
447.670231	28640.390202	30.220058
448.186097	28695.670580	30.225076
448.913098	28759.913330	30.230093
449.210914	28807.422522	30.235111
449.400308	28860.623345	30.240128
450.302672	28903.460571	30.245146
450.544986	28961.382183	30.250164
451.238619	29007.637751	30.255181
452.029149	29055.101040	30.260199
452.481619	29098.328196	30.265216
453.230239	29126.801573	30.270234
454.036393	29166.784715	30.275252
454.609250	29204.788603	30.280269
455.236058	29242.269031	30.285287
455.581889	29275.519228	30.290304
456.277807	29292.393909	30.295322
456.484743	29315.186385	30.300340
456.866709	29350.878977	30.305357
457.204484	29383.203124	30.310375
457.698591	29405.337548	30.315392
458.242877	29435.868942	30.320410
458.107055	29465.690259	30.325428
458.551775	29506.748941	30.330445
459.131846	29539.293740	30.335463
459.209661	29578.790507	30.340480
459.718561	29617.768600	30.345498
459.840548	29666.913111	30.350516
460.531966	29715.303882	30.355533
460.638069	29756.156125	30.360551
460.324916	29811.638856	30.365568
460.765302	29863.278834	30.370586
461.190732	29924.125594	30.375604
461.336869	29991.148076	30.380621
462.311736	30052.232434	30.385639
463.155103	30116.804117	30.390656
463.840109	30168.365203	30.395674
464.163148	30213.908063	30.400692
464.196318	30268.988941	30.405709
464.971594	30316.912613	30.410727
465.322804	30384.977430	30.415744
466.050763	30430.268446	30.420762
466.901548	30480.426274	30.425780
467.337296	30534.637515	30.430797
468.286914	30566.426685	30.435815
468.910103	30613.156067	30.440832
469.468034	30661.360885	30.445850
469.916162	30706.277726	30.450868
470.247063	30736.563940	30.455885
470.726335	30773.706863	30.460903
471.025294	30818.428667	30.465920
471.298592	30860.217221	30.470938
471.707205	30911.184111	30.475956
472.642768	30949.407280	30.480973
473.543243	30979.441688	30.485991
473.830761	31022.282127	30.491008
474.317310	31071.005171	30.496026
474.792189	31100.724584	30.501044
474.942806	31142.238204	30.506061
475.343232	31183.513470	30.511079
475.687656	31236.104773	30.516096
476.571028	31277.660391	30.521114
476.948979	31321.432722	30.526132
477.157190	31360.920574	30.531149
477.651522	31407.800350	30.536167
477.976123	31445.734832	30.541184
478.224507	31492.126835	30.546202
478.656668	31542.207928	30.551220
478.869914	31595.138329	30.556237
480.202579	31651.954138	30.561255
480.144896	31694.416712	30.566272
480.545240	31742.405323	30.571290
481.221093	31781.192310	30.576308
481.682825	31825.415402	30.581325
482.042851	31857.273206	30.586343
482.631158	31909.673232	30.591360
483.023032	31955.123550	30.596378
483.789338	31989.057833	30.601396
484.300001	32029.170654	30.606413
485.028687	32066.440789	30.611431
485.132000	32105.941952	30.616448
485.703563	32155.208796	30.621466
485.856113	32198.617970	30.626484
486.465655	32249.787779	30.631501
486.950915	32294.115295	30.636519
487.363054	32348.613806	30.641536
487.431333	32391.690756	30.646554
488.358625	32445.788869	30.651572
488.413819	32502.763174	30.656589
489.036796	32556.825407	30.661607
489.432088	32615.707849	30.666624
489.742818	32662.840130	30.671642
490.424429	32716.034417	30.676660
490.876837	32776.990439	30.681677
491.523571	32828.398528	30.686695
492.162771	32885.457015	30.691712
492.531664	32937.885027	30.696730
492.884469	32991.458370	30.701748
493.507563	33042.325159	30.706765
494.325948	33099.334688	30.711783
494.530764	33146.246539	30.716800
494.927519	33193.800986	30.721818
496.201010	33231.037001	30.726836
496.737014	33276.077797	30.731853
497.455582	33320.591944	30.736871
498.342717	33354.542832	30.741888
499.128213	33389.155011	30.746906
499.516180	33411.587181	30.751924
499.566736	33459.895960	30.756941
500.622757	33490.829489	30.761959
500.999498	33526.269401	30.766976
501.490019	33555.163358	30.771994
502.597516	33588.079646	30.777012
502.428432	33621.621858	30.782029
502.714547	33645.198455	30.787047
503.090191	33697.210936	30.792064
503.378514	33729.942784	30.797082
503.964882	33771.460418	30.802100
504.120394	33826.755360	30.807117
504.449453	33864.590052	30.812135
504.587486	33923.615541	30.817152
505.024270	33977.540375	30.822170
505.666439	34025.376884	30.827188
505.601531	34089.676723	30.832205
505.929450	34151.356222	30.837223
506.271047	34216.669388	30.842240
506.616899	34274.574723	30.847258
507.343226	34338.487382	30.852276
508.137278	34397.218956	30.857293
508.594156	34449.879313	30.862311
509.082454	34508.777261	30.867328
509.281991	34565.480865	30.872346
510.384676	34625.160792	30.877364
510.462824	34685.354178	30.882381
510.661919	34749.140854	30.887399
511.247843	34809.642168	30.892416
511.814246	34869.916627	30.897434
512.685028	34922.835684	30.902452
513.047058	34997.916610	30.907469
513.836028	35056.540729	30.912487
514.040025	35116.433078	30.917504
514.682338	35180.454639	30.922522
515.429227	35233.941864	30.927540
515.911654	35293.594558	30.932557
516.504439	35347.575651	30.937575
517.277888	35409.871164	30.942592
517.493763	35473.730107	30.947610
518.084004	35529.170384	30.952628
518.282745	35594.471962	30.957645
519.183891	35651.759445	30.962663
519.842533	35711.263376	30.967680
520.461871	35765.260100	30.972698
521.218972	35814.533566	30.977716
521.650498	35872.331476	30.982733
522.069376	35926.056858	30.987751
522.968558	35971.929086	30.992768
523.782685	36020.075979	30.997786
524.243474	36079.861217	31.002804
524.394663	36133.569951	31.007821
525.235315	36182.243005	31.012839
525.565792	36219.921394	31.017856
525.500434	36282.013259	31.022874
526.484417	36329.080773	31.027892
526.953099	36388.136532	31.032909
527.879643	36441.473428	31.037927
528.071883	36488.601261	31.042944
529.029321	36531.838736	31.047962
529.836777	36568.823762	31.052980
530.064584	36618.158531	31.057997
530.415772	36669.827044	31.063015
531.555332	36710.237077	31.068032
531.466816	36759.976802	31.073050
532.148631	36805.443308	31.078068
532.270594	36873.477233	31.083085
532.674554	36918.597062	31.088103
533.333685	36966.867712	31.093120
533.739145	37022.861873	31.098138
534.709203	37076.679284	31.103156
534.740582	37133.555432	31.108173
535.384350	37184.442941	31.113191
536.826199	37236.967855	31.118208
536.764882	37289.087589	31.123226
537.023056	37324.482634	31.128244
537.638567	37378.450068	31.133261
537.733693	37422.724418	31.138279
538.550890	37475.789507	31.143296
539.455334	37519.919108	31.148314
539.767656	37564.955219	31.153332
540.166581	37616.933893	31.158349
540.594167	37670.363029	31.163367
541.392411	37716.907219	31.168384
541.530742	37766.244628	31.173402
542.142947	37816.593194	31.178420
542.520097	37876.730092	31.183437
542.787141	37933.479951	31.188455
543.407673	37987.887103	31.193472
543.849931	38054.522604	31.198490
544.515594	38114.124707	31.203508
544.996337	38186.565673	31.208525
545.481045	38249.314944	31.213543
546.297398	38311.893962	31.218560
546.237724	38379.314290	31.223578
546.727429	38442.994620	31.228596
547.354532	38519.847135	31.233613
547.744936	38591.658024	31.238631
548.764221	38659.494305	31.243648
548.880049	38739.974162	31.248666
550.013820	38785.907965	31.253684
551.127714	38847.061427	31.258701
551.767641	38902.667574	31.263719
552.609379	38961.696111	31.268736
552.790693	39020.140317	31.273754
553.424178	39074.456911	31.278772
553.672699	39134.297947	31.283789
554.257790	39190.536270	31.288807
554.559136	39253.771819	31.293824
554.945399	39322.028380	31.298842
555.758721	39378.054537	31.303860
556.250094	39447.748915	31.308877
556.780267	39517.484262	31.313895
557.629622	39575.190676	31.318912
557.447082	39647.078577	31.323930
558.455557	39720.088641	31.328948
559.108160	39780.178232	31.333965
559.269361	39846.025426	31.338983
559.640495	39907.969489	31.344000
560.318936	39986.464132	31.349018
561.101751	40043.551993	31.354036
561.829170	40117.173738	31.359053
562.006807	40201.163196	31.364071
562.731608	40263.530886	31.369088
563.223633	40333.635749	31.374106
564.019963	40401.365082	31.379124
564.598412	40478.546625	31.384141
564.733058	40540.318628	31.389159
565.526203	40608.718581	31.394176
565.803690	40683.534142	31.399194
566.716708	40749.612484	31.404212
567.403177	40811.982268	31.409229
567.481511	40876.524436	31.414247
568.124991	40940.395381	31.419264
568.357896	41020.410423	31.424282
568.892898	41088.584845	31.429300
569.457417	41154.039207	31.434317
569.736808	41226.943317	31.439335
570.357436	41300.685916	31.444352
571.258559	41386.751075	31.449370
572.321283	41446.873661	31.454388
573.142332	41516.576138	31.459405
573.639976	41579.580734	31.464423
574.531880	41630.668458	31.469440
575.134461	41699.401855	31.474458
575.638919	41758.664415	31.479476
576.026850	41813.656249	31.484493
576.794938	41884.600552	31.489511
577.317569	41935.332445	31.494528
577.760585	42011.552108	31.499546
578.395806	42066.199202	31.504564
578.893761	42134.768993	31.509581
579.487889	42210.243678	31.514599
580.375086	42271.879836	31.519616
580.739194	42338.537784	31.524634
580.990797	42408.290628	31.529652
581.643758	42470.867454	31.534669
581.756678	42539.533110	31.539687
582.897472	42607.400879	31.544704
583.458412	42684.288250	31.549722
584.088093	42752.654592	31.554740
584.767087	42821.817910	31.559757
585.290307	42889.413602	31.564775
586.060396	42949.780609	31.569792
587.266982	43000.575024	31.574810
588.144490	43049.221963	31.579828
588.998209	43095.040740	31.584845
589.662763	43150.443790	31.589863
590.239043	43192.742247	31.594880
590.927195	43243.900858	31.599898
591.140886	43286.552149	31.604916
591.764865	43342.442676	31.609933
592.270507	43401.195524	31.614951
592.948822	43451.961679	31.619968
592.934519	43510.112422	31.624986
593.358317	43568.144076	31.630004
594.319246	43627.605886	31.635021
594.835616	43692.161627	31.640039
595.272805	43749.392647	31.645056
595.700426	43811.662035	31.650074
595.951887	43872.291372	31.655092
596.661713	43938.106318	31.660109
596.966481	44008.234903	31.665127
597.926938	44080.070279	31.670144
598.013789	44145.689535	31.675162
598.394464	44222.503540	31.680180
599.459413	44278.084452	31.685197
600.256371	44339.130230	31.690215
601.249578	44393.040662	31.695232
602.042309	44439.419459	31.700250
602.931518	44484.970279	31.705268
603.742502	44524.790511	31.710285
604.448978	44573.527528	31.715303
605.327879	44606.657463	31.720320
605.853042	44649.770037	31.725338
606.257130	44694.987641	31.730356
606.637831	44744.377748	31.735373
606.965490	44796.931792	31.740391
607.598755	44842.533639	31.745408
607.803014	44900.875413	31.750426
607.997105	44964.363337	31.755444
608.698723	45021.852901	31.760461
608.920348	45104.072500	31.765479
609.172307	45165.905901	31.770496
609.534018	45239.749335	31.775514
610.248763	45322.978046	31.780532
610.842726	45412.837467	31.785549
611.370899	45491.504017	31.790567
612.040340	45573.958404	31.795584
612.621710	45658.856755	31.800602
613.093122	45736.065559	31.805620
613.555654	45819.115426	31.810637
614.139587	45916.975120	31.815655
615.011903	45995.038441	31.820672
615.531029	46092.085877	31.825690
615.864014	46180.294569	31.830708
616.639478	46258.880858	31.835725
617.079902	46358.848602	31.840743
617.836205	46446.351209	31.845760
618.409522	46539.636588	31.850778
619.120023	46623.026443	31.855796
620.022545	46711.809541	31.860813
620.516386	46799.409259	31.865831
621.147838	46878.310161	31.870848
621.868527	46981.078692	31.875866
622.421235	47073.703811	31.880884
623.512917	47154.930434	31.885901
623.913598	47233.847068	31.890919
624.624975	47306.084697	31.895936
625.555157	47397.187574	31.900954
625.813778	47486.817300	31.905972
626.905705	47555.841824	31.910989
627.562766	47635.268889	31.916007
628.577822	47715.105545	31.921024
629.397064	47788.716186	31.926042
629.898497	47856.440637	31.931060
630.813868	47917.433357	31.936077
631.322811	47991.906484	31.941095
631.584148	48064.448308	31.946112
632.318077	48140.096294	31.951130
632.521466	48213.122368	31.956148
633.199377	48274.065304	31.961165
633.712606	48354.246417	31.966183
634.288027	48410.280138	31.971200
634.921409	48485.059170	31.976218
635.417107	48559.577815	31.981236
636.351313	48636.422090	31.986253
636.615775	48705.927298	31.991271
637.035494	48780.428225	31.996288
637.835102	48866.936322	32.001306
638.487920	48953.425734	32.006324
639.602791	49017.568425	32.011341
640.536214	49103.334499	32.016359
641.186883	49180.027359	32.021376
641.823776	49247.525007	32.026394
641.831015	49322.844116	32.031412
642.163902	49392.933884	32.036429
642.948284	49475.448475	32.041447
643.177460	49565.159204	32.046464
643.965885	49648.773053	32.051482
644.570499	49730.555126	32.056500
646.051303	49804.126431	32.061517
646.906200	49877.179819	32.066535
647.663442	49946.162824	32.071552
648.589656	50022.957106	32.076570
649.335795	50086.162024	32.081588
650.554611	50130.693740	32.086605
651.267071	50199.230454	32.091623
651.572132	50261.955564	32.096640
652.481115	50324.956469	32.101658
652.900434	50399.811137	32.106676
653.570284	50452.492571	32.111693
654.086588	50519.699413	32.116711
654.480359	50591.728895	32.121728
654.844022	50666.556214	32.126746
655.055487	50733.411683	32.131764
656.198121	50817.734309	32.136781
656.536853	50895.618239	32.141799
657.476457	50968.244233	32.146816
658.120402	51043.764158	32.151834
658.406928	51132.909982	32.156852
659.062261	51208.504405	32.161869
659.631888	51288.776398	32.166887
659.652225	51369.199682	32.171904
660.806528	51454.818226	32.176922
661.251961	51548.765617	32.181940
661.863437	51639.102709	32.186957
662.359053	51733.446737	32.191975
663.075905	51818.510008	32.196992
663.798405	51903.439999	32.202010
664.503749	52008.275336	32.207028
665.029860	52091.154806	32.212045
665.955797	52177.188392	32.217063
667.026954	52261.099837	32.222080
667.808857	52330.238658	32.227098
668.481296	52404.116196	32.232116
669.503735	52466.750733	32.237133
669.931445	52551.020057	32.242151
670.129194	52624.177318	32.247168
671.327716	52686.384335	32.252186
671.900889	52758.947041	32.257204
672.482051	52833.764306	32.262221
672.864138	52913.948687	32.267239
673.537401	52988.535933	32.272256
674.450191	53067.296833	32.277274
675.384583	53144.613735	32.282292
675.915859	53217.317989	32.287309
676.101319	53299.565855	32.292327
676.347358	53382.580866	32.297344
677.466510	53463.336245	32.302362
677.389208	53557.768183	32.307380
678.462227	53641.704133	32.312397
679.300854	53728.208056	32.317415
680.050673	53815.574275	32.322432
681.484060	53890.104206	32.327450
682.129109	53972.206621	32.332468
682.982159	54050.040170	32.337485
683.485704	54130.796310	32.342503
683.726047	54207.143103	32.347520
684.923844	54279.023041	32.352538
685.446798	54372.250220	32.357556
686.037594	54442.414900	32.362573
686.718068	54526.055340	32.367591
687.434170	54613.791021	32.372608
687.606232	54700.400725	32.377626
688.402344	54784.982925	32.382644
689.225955	54871.620775	32.387661
689.431062	54962.870438	32.392679
690.088208	55060.785539	32.397696
690.575471	55159.829748	32.402714
691.000325	55253.412760	32.407732
691.559810	55367.523105	32.412749
692.332929	55471.252951	32.417767
692.218289	55581.107101	32.422784
693.330113	55691.187779	32.427802
693.965256	55817.092142	32.432820
694.860026	55921.012012	32.437837
695.557792	56036.107250	32.442855
695.905018	56146.744808	32.447872
696.566343	56267.648845	32.452890
697.337550	56376.243362	32.457908
698.119939	56504.957943	32.462925
699.007226	56615.120067	32.467943
699.397333	56728.180188	32.472960
700.154095	56841.677384	32.477978
700.916060	56960.691406	32.482996
702.300728	57063.281957	32.488013
703.504369	57163.426702	32.493031
704.230520	57271.673536	32.498048
705.770722	57355.639837	32.503066
705.808129	57448.414655	32.508084
706.604347	57525.601537	32.513101
707.661773	57603.546593	32.518119
708.151337	57689.489108	32.523136
708.868380	57769.856759	32.528154
709.832768	57854.423048	32.533172
710.553107	57921.866428	32.538189
711.413317	58005.616958	32.543207
711.540605	58092.090919	32.548224
712.281671	58183.655195	32.553242
712.706478	58271.551528	32.558260
712.921265	58367.365403	32.563277
713.689363	58467.319444	32.568295
713.978315	58573.183262	32.573312
715.005199	58674.857323	32.578330
715.246123	58792.606191	32.583348
715.936216	58906.638311	32.588365
717.026430	59014.503419	32.593383
717.638679	59123.108291	32.598400
718.389117	59233.971728	32.603418
718.903586	59347.296910	32.608436
719.833189	59454.098422	32.613453
720.898928	59558.494348	32.618471
721.979201	59670.163237	32.623488
722.375727	59763.247348	32.628506
722.949010	59864.177045	32.633524
723.861976	59967.501448	32.638541
724.667940	60064.321799	32.643559
725.312929	60164.766644	32.648576
726.295258	60271.165185	32.653594
727.181399	60374.167556	32.658612
727.429154	60486.817843	32.663629
728.261596	60586.309806	32.668647
728.794040	60690.423604	32.673664
729.750200	60801.045369	32.678682
730.178948	60914.419173	32.683700
730.675527	61034.374721	32.688717
731.561901	61144.845942	32.693735
732.044766	61269.141392	32.698752
732.799694	61376.602285	32.703770
733.123979	61501.684824	32.708788
733.974375	61623.365730	32.713805
734.505718	61742.579863	32.718823
735.226961	61878.873629	32.723840
735.791492	62000.043131	32.728858
736.154942	62133.593232	32.733876
737.033219	62257.586675	32.738893
738.114612	62398.784397	32.743911
738.681538	62540.652774	32.748928
739.196288	62659.521020	32.753946
740.141488	62794.954329	32.758964
740.795636	62934.743330	32.763981
741.759038	63062.431403	32.768999
741.972612	63201.400000	32.774016
743.026640	63329.554626	32.779034
743.785924	63459.707605	32.784052
744.578404	63580.170841	32.789069
745.599415	63710.236297	32.794087
746.141145	63833.999651	32.799104
746.950452	63945.757007	32.804122
748.041590	64058.256915	32.809140
748.977619	64179.988675	32.814157
749.476522	64289.866538	32.819175
750.055364	64410.782075	32.824192
751.801527	64531.536284	32.829210
752.185998	64649.995625	32.834228
752.653689	64775.243928	32.839245
753.964286	64877.784987	32.844263
754.431654	65004.817546	32.849280
755.481697	65120.364817	32.854298
756.362823	65226.331897	32.859316
757.148515	65344.182707	32.864333
758.044138	65448.422447	32.869351
758.249381	65571.412807	32.874368
759.185673	65677.676176	32.879386
759.974137	65803.305559	32.884404
759.765566	65926.659697	32.889421
760.791815	66055.847306	32.894439
761.476922	66193.408221	32.899456
762.530759	66316.763353	32.904474
763.963472	66415.845192	32.909492
765.258104	66525.067300	32.914509
765.855009	66639.815335	32.919527
766.479704	66752.346296	32.924544
767.535678	66866.896792	32.929562
768.471084	66973.305912	32.934580
768.911965	67087.659467	32.939597
769.584710	67191.926995	32.944615
770.137633	67317.649949	32.949632
770.870558	67434.667836	32.954650
771.815908	67556.537583	32.959668
771.976307	67677.050266	32.964685
772.844131	67793.288259	32.969703
773.811154	67924.229860	32.974720
774.719304	68030.263220	32.979738
775.718985	68149.540918	32.984756
776.305408	68271.008311	32.989773
777.449169	68386.917726	32.994791
777.701854	68510.707330	32.999808
778.517301	68632.441054	33.004826
779.287689	68749.099288	33.009844
779.760365	68874.478382	33.014861
780.894202	68985.239247	33.019879
781.356067	69129.174319	33.024896
782.055515	69252.860052	33.029914
782.883711	69377.144139	33.034932
783.767043	69513.800868	33.039949
784.840969	69626.858073	33.044967
786.008797	69756.720424	33.049984
786.374949	69876.116217	33.055002
786.970087	70000.096015	33.060020
787.237401	70108.171768	33.065037
787.853880	70235.538736	33.070055
788.485507	70359.862145	33.075072
789.626517	70482.005852	33.080090
790.687259	70601.697716	33.085108
791.097780	70734.870198	33.090125
792.275185	70855.352929	33.095143
792.880872	70981.043973	33.100160
793.625624	71107.122979	33.105178
794.610652	71231.295985	33.110196
795.323255	71353.125885	33.115213
796.535121	71469.843330	33.120231
797.158286	71589.868547	33.125248
797.896235	71712.081880	33.130266
799.177358	71822.218591	33.135284
799.759013	71948.969141	33.140301
800.884719	72069.144909	33.145319
801.641481	72187.442986	33.150336
802.370010	72309.193276	33.155354
803.082890	72434.994493	33.160372
803.505253	72564.489026	33.165389
805.035387	72686.382383	33.170407
805.547740	72804.915387	33.175424
806.294286	72920.025327	33.180442
807.269350	73037.266032	33.185460
808.216956	73165.295401	33.190477
808.972399	73285.648773	33.195495
810.045456	73401.736214	33.200512
810.458212	73522.301366	33.205530
811.396503	73630.039271	33.210548
812.393989	73753.572999	33.215565
813.802960	73861.870213	33.220583
814.478504	73986.529268	33.225600
814.770814	74101.128650	33.230618
815.398016	74221.819008	33.235636
816.183171	74352.356101	33.240653
816.789378	74473.399293	33.245671
817.606441	74605.051919	33.250688
818.356507	74739.404920	33.255706
819.473527	74857.858023	33.260724
820.119717	74991.711690	33.265741
820.904479	75126.737872	33.270759
821.275994	75251.316955	33.275776
821.979110	75378.085372	33.280794
823.422120	75517.707107	33.285812
823.900794	75663.206587	33.290829
824.856865	75803.938207	33.295847
825.430457	75939.372344	33.300864
826.306501	76075.577797	33.305882
827.655463	76209.324726	33.310900
828.033966	76349.115010	33.315917
828.955624	76468.090861	33.320935
829.414165	76609.203733	33.325952
830.051431	76745.409875	33.330970
831.149920	76877.299699	33.335988
831.660282	77011.998400	33.341005
832.587860	77139.301326	33.346023
833.215007	77273.760192	33.351040
833.960644	77400.817427	33.356058
835.488047	77536.218021	33.361076
836.177398	77671.421373	33.366093
837.489373	77788.363704	33.371111
838.276181	77916.416276	33.376128
839.261801	78038.931973	33.381146
840.601634	78154.568291	33.386164
841.453215	78276.431355	33.391181
842.435935	78387.796732	33.396199
843.133391	78495.194475	33.401216
843.820816	78625.583413	33.406234
845.090955	78736.641907	33.411252
846.312158	78842.699022	33.416269
847.288684	78947.919201	33.421287
848.083719	79067.518780	33.426304
848.360662	79177.414708	33.431322
849.502749	79290.496933	33.436340
850.423329	79414.195230	33.441357
850.862883	79524.368642	33.446375
851.525521	79641.305218	33.451392
852.088627	79760.113074	33.456410
853.010234	79880.353183	33.461428
853.705974	80011.621678	33.466445
854.823074	80135.967158	33.471463
855.804460	80275.577185	33.476480
856.313641	80382.332801	33.481498
858.067679	80501.231555	33.486516
859.029516	80623.442577	33.491533
860.178691	80735.860119	33.496551
861.305968	80842.606916	33.501568
861.619072	80960.546442	33.506586
862.545638	81064.367737	33.511604
863.663328	81182.936139	33.516621
864.509564	81285.633369	33.521639
865.477108	81402.229343	33.526656
865.834998	81510.060036	33.531674
866.952183	81625.094077	33.536692
867.731720	81750.828436	33.541709
868.017267	81870.637457	33.546727
868.975984	81995.823649	33.551744
869.738256	82133.761526	33.556762
870.229388	82257.017212	33.561780
870.808324	82400.372423	33.566797
871.525616	82528.184305	33.571815
872.180974	82669.781796	33.576832
872.562580	82820.000436	33.581850
873.608581	82959.773816	33.586868
874.407625	83119.926319	33.591885
875.050235	83268.413756	33.596903
875.623099	83423.247808	33.601920
876.355595	83574.233773	33.606938
877.370265	83723.938528	33.611956
877.793186	83888.431768	33.616973
878.543221	84039.683489	33.621991
879.445417	84194.238448	33.627008
880.437235	84358.523657	33.632026
880.881184	84509.160097	33.637044
881.576822	84691.943592	33.642061
882.322083	84863.469200	33.647079
883.648510	85038.452766	33.652096
884.074098	85203.435668	33.657114
884.790952	85377.387130	33.662132
885.674228	85565.808757	33.667149
886.312178	85738.782900	33.672167
887.485021	85922.867380	33.677184
888.479819	86106.654722	33.682202
889.563687	86280.056367	33.687220
890.434911	86456.507926	33.692237
891.559261	86648.263479	33.697255
892.345201	86826.257499	33.702272
892.824388	87016.645685	33.707290
894.054696	87199.274687	33.712308
894.366648	87391.523414	33.717325
895.764531	87570.443391	33.722343
897.031238	87757.791496	33.727360
898.213427	87938.048517	33.732378
899.305063	88102.842523	33.737396
900.305968	88290.752936	33.742413
900.942270	88467.291217	33.747431
902.330195	88637.537827	33.752448
903.038956	88816.426897	33.757466
904.330868	88988.249324	33.762484
904.963801	89165.103409	33.767501
905.987016	89331.398511	33.772519
907.258974	89500.563505	33.777536
908.138986	89670.290473	33.782554
909.410339	89832.369344	33.787572
910.305833	89991.830111	33.792589
911.887552	90152.592141	33.797607
912.738411	90305.087849	33.802624
913.905506	90456.194880	33.807642
914.910875	90603.438026	33.812660
915.602697	90766.400881	33.817677
916.474959	90921.118381	33.822695
917.254649	91073.131062	33.827712
918.101909	91228.797876	33.832730
919.316118	91373.807250	33.837748
920.227883	91527.021727	33.842765
921.470170	91695.219646	33.847783
922.137905	91827.976281	33.852800
923.010380	91985.403217	33.857818
923.738063	92123.411128	33.862836
924.982049	92281.447285	33.867853
926.065372	92438.973940	33.872871
927.067392	92585.071222	33.877888
927.767382	92724.663368	33.882906
928.631988	92866.994273	33.887924
930.012786	92995.729547	33.892941
930.601255	93135.944459	33.897959
931.556958	93269.684994	33.902976
931.973126	93415.279834	33.907994
933.242101	93544.233344	33.913012
934.136034	93693.590345	33.918029
934.762451	93837.385558	33.923047
936.603484	93963.109864	33.928064
937.488305	94108.147414	33.933082
938.722609	94233.869382	33.938100
939.235274	94366.805465	33.943117
940.233536	94502.982505	33.948135
941.481615	94644.017188	33.953152
941.890274	94787.620953	33.958170
942.765643	94912.964685	33.963188
943.705242	95057.245052	33.968205
944.903514	95193.290315	33.973223
945.806142	95339.781647	33.978240
946.550978	95487.320074	33.983258
947.548755	95630.492261	33.988276
948.340400	95775.409832	33.993293
948.511859	95930.816728	33.998311
949.701837	96086.075483	34.003328
950.221817	96252.256507	34.008346
951.011368	96403.743029	34.013364
951.873752	96576.882057	34.018381
952.758520	96754.114509	34.023399
953.512872	96923.203658	34.028416
954.339404	97102.803620	34.033434
955.306647	97283.001193	34.038452
956.153532	97453.673442	34.043469
957.476061	97639.738559	34.048487
958.466622	97816.814694	34.053504
959.102040	97995.504016	34.058522
960.552998	98164.861997	34.063540
961.515978	98333.665209	34.068557
962.876203	98506.073665	34.073575
964.333433	98665.740668	34.078592
964.927470	98840.802459	34.083610
965.474487	99006.604285	34.088628
966.918039	99179.522178	34.093645
968.243443	99347.877453	34.098663
969.761321	99504.918046	34.103680
970.649976	99672.691756	34.108698
971.621014	99830.391489	34.113716
972.414500	99994.694862	34.118733
973.460223	100153.992024	34.123751
974.771071	100298.086569	34.128768
975.483798	100470.878668	34.133786
976.538033	100625.067521	34.138804
977.330788	100782.645289	34.143821
978.409407	100947.114824	34.148839
979.164977	101091.663451	34.153856
979.966306	101259.373740	34.158874
981.102750	101406.208054	34.163892
981.859884	101563.112787	34.168909
982.327093	101719.080305	34.173927
983.594574	101875.000362	34.178944
984.348773	102032.997544	34.183962
985.175489	102187.880481	34.188980
986.460206	102347.131137	34.193997
986.823107	102518.812572	34.199015
987.943739	102687.997084	34.204032
988.385887	102856.855602	34.209050
989.388154	103035.561163	34.214068
990.236460	103209.608287	34.219085
991.477129	103397.052245	34.224103
992.993592	103566.313925	34.229120
993.717983	103744.919888	34.234138
994.507407	103926.454252	34.239156
995.495424	104107.727875	34.244173
996.644813	104279.969997	34.249191
997.550007	104457.371909	34.254208
998.483990	104645.409158	34.259226
1000.148221	104812.690319	34.264244
1001.804965	104980.974407	34.269261
1002.798413	105137.859911	34.274279
1004.167950	105294.314624	34.279296
1005.194395	105458.973218	34.284314
1006.249370	105618.346199	34.289332
1007.407152	105775.384623	34.294349
1008.567850	105941.479794	34.299367
1009.398524	106099.817415	34.304384
1009.905756	106268.585089	34.309402
1010.998504	106424.143810	34.314420
1012.257571	106598.801359	34.319437
1012.679047	106785.244056	34.324455
1013.653992	106941.864592	34.329472
1015.214996	107107.467731	34.334490
1016.317189	107272.403106	34.339508
1017.641286	107430.296696	34.344525
1018.403070	107600.422445	34.349543
1019.570412	107749.908535	34.354560
1020.489919	107926.697515	34.359578
1021.252454	108095.306174	34.364596
1022.525381	108253.314641	34.369613
1023.428386	108427.284889	34.374631
1024.504364	108597.350391	34.379648
1025.531928	108769.528047	34.384666
1026.752829	108933.959117	34.389684
1027.459158	109103.102982	34.394701
1028.414631	109274.181395	34.399719
1029.477989	109433.081292	34.404736
1030.244668	109610.756054	34.409754
1030.651165	109785.541997	34.414772
1031.963759	109971.385127	34.419789
1032.376948	110160.474543	34.424807
1033.576610	110350.140002	34.429824
1034.488937	110531.190828	34.434842
1035.297476	110710.030968	34.439860
1036.309602	110896.552506	34.444877
1037.522661	111076.858628	34.449895
1038.264871	111247.947753	34.454912
1039.217048	111436.750863	34.459930
1039.945790	111634.449012	34.464948
1040.938592	111815.050995	34.469965
1041.603644	112022.809234	34.474983
1042.748579	112206.402912	34.480000
1044.024192	112413.274014	34.485018
1045.000626	112615.864978	34.490036
1045.847524	112817.263323	34.495053
1047.359356	113010.605509	34.500071
1048.603855	113194.099897	34.505088
1050.218373	113393.318452	34.510106
1050.921194	113588.576866	34.515124
1052.619259	113770.375608	34.520141
1053.406440	113968.067457	34.525159
1054.633702	114141.295671	34.530176
1055.819031	114330.965144	34.535194
1056.888128	114520.339030	34.540212
1057.987127	114706.744227	34.545229
1059.043782	114889.749585	34.550247
1060.470264	115085.629231	34.555264
1061.029233	115280.252336	34.560282
1061.322011	115476.670873	34.565300
1062.858274	115666.998668	34.570317
1063.491477	115878.477714	34.575335
1064.541900	116074.365139	34.580352
1065.621159	116283.452022	34.585370
1066.480954	116487.889733	34.590388
1067.516474	116698.228861	34.595405
1068.929154	116901.155662	34.600423
1071.197713	117086.983209	34.605440
1072.761486	117277.228203	34.610458
1073.895566	117465.292504	34.615476
1075.304466	117635.925686	34.620493
1076.266741	117819.890789	34.625511
1077.311628	118008.062563	34.630528
1078.754243	118175.018347	34.635546
1079.945543	118352.155547	34.640564
1081.080370	118521.522960	34.645581
1081.725230	118701.721048	34.650599
1082.952601	118868.704964	34.655616
1084.186472	119037.031957	34.660634
1085.080772	119210.867082	34.665652
1086.071450	119389.122011	34.670669
1086.597099	119578.431863	34.675687
1087.753950	119756.660555	34.680704
1088.451629	119939.454993	34.685722
1089.440937	120133.010312	34.690740
1090.633366	120318.256882	34.695757
1091.216026	120531.412954	34.700775
1092.165318	120718.566534	34.705792
1093.576867	120917.529308	34.710810
1094.165204	121120.575650	34.715828
1095.043682	121309.392540	34.720845
1096.205648	121504.840823	34.725863
1097.060828	121698.581329	34.730880
1098.047575	121891.121940	34.735898
1099.910037	122079.141529	34.740916
1101.427589	122263.153168	34.745933
1102.468510	122448.641625	34.750951
1103.871975	122632.016022	34.755968
1104.975284	122808.485069	34.760986
1105.958892	123007.509587	34.766004
1107.479764	123182.160336	34.771021
1108.183266	123369.752689	34.776039
1109.497368	123561.626856	34.781056
1110.441559	123753.312085	34.786074
1111.106401	123941.320143	34.791092
1112.390002	124125.484518	34.796109
1113.687791	124319.774345	34.801127
1114.498903	124517.152560	34.806144
1115.692564	124710.892344	34.811162
1116.550825	124920.648039	34.816180
1117.981813	125113.830069	34.821197
1118.591921	125316.545822	34.826215
1119.772258	125518.138614	34.831232
1121.049726	125732.619126	34.836250
1122.188409	125938.645325	34.841268
1123.521413	126139.303421	34.846285
1124.333750	126340.863166	34.851303
1125.906846	126525.980959	34.856320
1127.472628	126722.483516	34.861338
1128.690857	126913.862589	34.866356
1129.922199	127111.565637	34.871373
1131.319874	127305.147259	34.876391
1132.325434	127503.677319	34.881408
1134.142501	127686.706764	34.886426
1135.092203	127873.865963	34.891444
1136.487642	128053.775439	34.896461
1137.454649	128233.759293	34.901479
1138.651574	128412.094958	34.906496
1139.934671	128591.709833	34.911514
1141.763794	128766.542079	34.916532
1143.347424	128934.800352	34.921549
1144.266116	129104.162106	34.926567
1145.460033	129277.242509	34.931584
1146.274562	129442.732267	34.936602
1147.176528	129607.421975	34.941620
1148.502482	129776.426016	34.946637
1149.689643	129949.980255	34.951655
1150.450111	130128.641118	34.956672
1151.911781	130294.924534	34.961690
1152.826476	130475.411724	34.966708
1153.890213	130651.133263	34.971725
1155.068047	130829.713890	34.976743
1155.765259	131017.708066	34.981760
1156.907751	131189.489182	34.986778
1157.886035	131356.329885	34.991796
1159.289861	131523.846548	34.996813
1160.712280	131703.594461	35.001831
1161.388571	131867.421595	35.006848
1162.707840	132028.299736	35.011866
1163.749200	132215.126319	35.016884
1164.707282	132375.801785	35.021901
1165.747501	132554.504206	35.026919
1166.631527	132743.541294	35.031936
1167.858527	132923.620975	35.036954
1169.018850	133115.947156	35.041972
1169.816025	133297.091342	35.046989
1170.739187	133486.962749	35.052007
1171.485430	133689.480188	35.057024
1172.751766	133897.006433	35.062042
1173.349482	134107.247479	35.067060
1174.376509	134318.582762	35.072077
1175.631868	134535.015037	35.077095
1176.752441	134757.696914	35.082112
1177.522726	134980.655784	35.087130
1178.577830	135213.596171	35.092148
1179.820286	135431.291655	35.097165
1181.089762	135669.409461	35.102183
1182.322334	135908.105825	35.107200
1183.621860	136139.425936	35.112218
1184.682045	136379.841459	35.117236
1185.759420	136610.898536	35.122253
1187.015528	136845.514817	35.127271
1188.340345	137079.550389	35.132288
1189.538899	137310.769001	35.137306
1190.866029	137551.172489	35.142324
1191.900100	137792.135025	35.147341
1193.117919	138031.279967	35.152359
1194.306468	138271.724928	35.157376
1195.825042	138509.731261	35.162394
1196.995963	138750.588346	35.167412
1198.592055	138987.633719	35.172429
1199.852168	139225.321524	35.177447
1201.172877	139458.778080	35.182464
1202.422372	139679.961204	35.187482
1203.266701	139919.031015	35.192500
1204.585185	140151.199209	35.197517
1205.902792	140393.082393	35.202535
1206.628779	140630.845884	35.207552
1208.388951	140869.029936	35.212570
1209.567961	141109.876619	35.217588
1210.830611	141342.176396	35.222605
1212.390944	141578.890445	35.227623
1213.539003	141816.247307	35.232640
1215.586155	142028.723631	35.237658
1216.366396	142263.787770	35.242676
1217.820093	142485.080419	35.247693
1219.183537	142705.375385	35.252711
1220.083380	142932.269342	35.257728
1221.721422	143136.528653	35.262746
1222.885328	143356.646209	35.267764
1223.887851	143560.522150	35.272781
1225.325547	143763.880891	35.277799
1226.131604	143968.705865	35.282816
1227.427625	144173.777854	35.287834
1228.579674	144392.052216	35.292852
1229.389210	144608.192535	35.297869
1231.040507	144804.431308	35.302887
1231.757809	145040.006304	35.307904
1233.103744	145262.539290	35.312922
1234.586818	145475.183293	35.317940
1235.495057	145697.755814	35.322957
1236.891142	145913.562497	35.327975
1237.976934	146143.349033	35.332992
1239.149816	146370.065577	35.338010
1240.431138	146604.843852	35.343028
1241.178721	146835.199907	35.348045
1242.461440	147064.007255	35.353063
1243.536933	147318.597925	35.358080
1244.737187	147544.936490	35.363098
1245.685953	147793.007642	35.368116
1247.223657	148048.627610	35.373133
1248.236119	148298.428813	35.378151
1249.122688	148556.586222	35.383168
1250.367507	148806.224192	35.388186
1251.455416	149067.851280	35.393204
1252.427442	149333.774409	35.398221
1254.037020	149598.841924	35.403239
1255.079939	149871.250764	35.408256
1256.184116	150132.172112	35.413274
1257.693529	150404.365382	35.418292
1259.311719	150671.062435	35.423309
1260.910257	150919.347267	35.428327
1262.482557	151186.905600	35.433344
1264.083835	151443.082961	35.438362
1265.160983	151709.524665	35.443380
1266.945404	151960.130999	35.448397
1267.958074	152207.801384	35.453415
1269.094844	152464.267960	35.458432
1270.519488	152715.638404	35.463450
1272.083073	152968.001468	35.468468
1273.223029	153220.134234	35.473485
1274.891032	153465.036565	35.478503
1275.887308	153716.956094	35.483520
1277.477214	153959.008029	35.488538
1278.730237	154204.074775	35.493556
1279.792803	154461.899023	35.498573
1281.439120	154698.985852	35.503591
1282.311907	154946.532486	35.508608
1283.753945	155195.492793	35.513626
1284.765564	155453.484389	35.518644
1286.374221	155707.975668	35.523661
1287.795720	155948.355920	35.528679
1289.083408	156205.188724	35.533696
1289.993324	156436.576358	35.538714
1291.285143	156679.482284	35.543732
1292.378958	156924.491389	35.548749
1293.404903	157162.853338	35.553767
1294.788470	157414.095443	35.558784
1296.230146	157642.747469	35.563802
1297.753517	157880.825468	35.568820
1299.192890	158123.435608	35.573837
1300.385207	158358.515593	35.578855
1301.293275	158604.035913	35.583872
1302.160283	158839.719837	35.588890
1303.345703	159102.855516	35.593908
1304.628982	159356.093044	35.598925
1305.948300	159612.281993	35.603943
1307.222979	159873.237778	35.608960
1308.679341	160124.509210	35.613978
1310.183982	160386.405720	35.618996
1311.723541	160644.187211	35.624013
1312.714835	160902.076805	35.629031
1313.902998	161169.881184	35.634048
1315.198169	161425.641204	35.639066
1316.653731	161710.861177	35.644084
1317.397099	161975.892043	35.649101
1318.858042	162240.357646	35.654119
1319.892487	162522.787668	35.659136
1320.782444	162800.816196	35.664154
1321.927594	163090.183927	35.669172
1323.468627	163377.100469	35.674189
1324.880760	163661.211509	35.679207
1326.558058	163971.150279	35.684224
1327.708237	164250.018987	35.689242
1329.165423	164547.907552	35.694260
1330.492635	164848.586459	35.699277
1331.767132	165136.740136	35.704295
1332.904918	165427.431430	35.709312
1334.119628	165727.881767	35.714330
1335.037358	166022.928767	35.719348
1336.532047	166328.613750	35.724365
1337.797734	166640.608361	35.729383
1338.921128	166951.297127	35.734400
1340.110524	167268.790799	35.739418
1341.576631	167579.501335	35.744436
1342.554333	167904.877620	35.749453
1343.993902	168227.296660	35.754471
1345.672971	168548.420704	35.759488
1346.600933	168872.124634	35.764506
1348.318838	169194.401267	35.769524
1349.353174	169519.525434	35.774541
1351.136596	169836.351380	35.779559
1352.587094	170161.332637	35.784576
1354.381096	170466.828905	35.789594
1356.466487	170773.749330	35.794612
1357.915503	171082.100446	35.799629
1359.620568	171373.557053	35.804647
1360.725840	171671.310991	35.809664
1362.185330	171971.518858	35.814682
1363.437812	172238.045361	35.819700
1365.034448	172531.215399	35.824717
1367.071521	172796.633523	35.829735
1369.416549	173064.716205	35.834752
1370.746974	173305.193898	35.839770
1373.114444	173539.670184	35.844788
1374.102558	173793.889598	35.849805
1375.371230	174029.000474	35.854823
1376.935062	174277.933248	35.859840
1377.875539	174527.113569	35.864858
1378.535469	174780.112434	35.869876
1379.317504	175045.440248	35.874893
1380.228287	175304.274877	35.879911
1381.497519	175593.254934	35.884928
1382.583548	175869.449660	35.889946
1383.633433	176158.825868	35.894964
1384.632026	176473.075320	35.899981
1385.570270	176771.980135	35.904999
1386.634790	177094.306728	35.910016
1387.866005	177405.666472	35.915034
1389.323487	177722.218438	35.920052
1390.497038	178044.938474	35.925069
1391.559470	178368.758363	35.930087
1392.946989	178711.943594	35.935104
1394.231902	179041.098356	35.940122
1395.806287	179375.460250	35.945140
1397.027293	179724.366752	35.950157
1398.383425	180061.397666	35.955175
1399.926545	180412.005121	35.960192
1400.938641	180768.823609	35.965210
1402.559994	181111.552827	35.970228
1404.129318	181470.704910	35.975245
1405.744211	181811.294590	35.980263
1407.243605	182166.845780	35.985280
1408.562489	182509.064406	35.990298
1410.163579	182844.077950	35.995316
1411.554437	183195.440262	36.000333
1412.993667	183549.309790	36.005351
1415.069722	183896.789365	36.010368
1416.028403	184247.039101	36.015386
1417.937985	184591.949321	36.020404
1419.598850	184946.817907	36.025421
1421.306763	185276.255247	36.030439
1422.838210	185608.453844	36.035456
1424.344048	185946.180557	36.040474
1426.024472	186269.916099	36.045492
1427.104669	186616.097541	36.050509
1428.447216	186955.647941	36.055527
1430.154085	187288.460863	36.060544
1431.338187	187626.734778	36.065562
1432.756465	188013.627634	36.070580
1433.983158	188363.691440	36.075597
1435.453132	188710.072370	36.080615
1436.788419	189051.743311	36.085632
1438.408034	189385.928522	36.090650
1440.253351	189702.812271	36.095668
1441.916005	190017.355027	36.100685
1443.304651	190332.263665	36.105703
1445.093003	190647.714863	36.110720
1446.450074	190956.640149	36.115738
1447.932951	191264.428290	36.120756
1448.954007	191584.141425	36.125773
1450.723985	191898.243754	36.130791
1451.754918	192223.493505	36.135808
1452.967740	192541.909176	36.140826
1453.494702	192866.169382	36.145844
1454.899836	193214.237027	36.150861
1456.019392	193545.305515	36.155879
1457.317204	193891.414707	36.160896
1458.242472	194251.846583	36.165914
1460.108691	194612.017853	36.170932
1461.032321	194981.912252	36.175949
1462.331795	195347.237412	36.180967
1464.062426	195718.534002	36.185984
1465.659134	196089.233475	36.191002
1467.211775	196454.394402	36.196020
1468.668351	196838.033758	36.201037
1470.503051	197212.520161	36.206055
1472.012986	197571.663744	36.211072
1473.678434	197945.446729	36.216090
1474.915331	198313.502860	36.221108
1476.714328	198689.857033	36.226125
1478.054931	199062.774757	36.231143
1480.134828	199429.372039	36.236160
1481.715378	199806.112344	36.241178
1483.418543	200156.716681	36.246196
1485.679232	200508.687433	36.251213
1487.360462	200859.184661	36.256231
1489.448098	201199.786694	36.261248
1491.305872	201527.745475	36.266266
1493.852117	201844.033699	36.271284
1495.724520	202167.764739	36.276301
1497.367033	202475.690632	36.281319
1499.147233	202772.928681	36.286336
1500.833075	203080.557599	36.291354
1502.509368	203368.584956	36.296372
1503.992700	203663.147398	36.301389
1505.303862	203968.329959	36.306407
1506.812612	204253.164195	36.311424
1508.338073	204552.001814	36.316442
1509.876085	204845.149985	36.321460
1511.352902	205131.478487	36.326477
1512.711586	205430.424171	36.331495
1514.261078	205719.066003	36.336512
1515.310445	206019.565141	36.341530
1517.140515	206315.741578	36.346548
1518.312435	206615.853733	36.351565
1519.642160	206916.409807	36.356583
1521.061001	207218.373887	36.361600
1522.148742	207514.262677	36.366618
1523.734714	207802.207276	36.371636
1524.792118	208107.207750	36.376653
1525.803143	208405.817489	36.381671
1527.365240	208699.762699	36.386688
1528.627446	209016.642151	36.391706
1530.113939	209322.868779	36.396724
1531.534261	209632.383943	36.401741
1532.756261	209950.695909	36.406759
1534.059534	210268.639578	36.411776
1535.103150	210605.498495	36.416794
1536.747002	210929.811608	36.421812
1538.026031	211287.610492	36.426829
1539.269987	211624.185010	36.431847
1540.797488	211967.950399	36.436864
1541.901137	212327.865960	36.441882
1543.524498	212681.370103	36.446900
1545.236247	213041.285979	36.451917
1546.529236	213414.583123	36.456935
1548.213852	213771.153991	36.461952
1549.431673	214147.590778	36.466970
1551.044747	214520.685111	36.471988
1552.242559	214899.617234	36.477005
1553.766962	215281.314107	36.482023
1555.394569	215662.664627	36.487040
1556.869643	216054.684499	36.492058
1558.370558	216444.669628	36.497076
1560.443277	216840.374616	36.502093
1561.684451	217229.823040	36.507111
1563.356513	217625.167836	36.512128
1564.834068	218026.541470	36.517146
1566.649188	218417.166043	36.522164
1567.975253	218817.476454	36.527181
1568.999699	219217.941559	36.532199
1571.083034	219625.541840	36.537216
1572.394242	220044.883104	36.542234
1574.088036	220454.839009	36.547252
1575.824546	220855.873978	36.552269
1577.636516	221273.102200	36.557287
1579.216840	221672.845996	36.562304
1580.868268	222076.871508	36.567322
1582.832990	222472.818540	36.572340
1585.357767	222861.990953	36.577357
1587.199302	223250.900537	36.582375
1589.223034	223630.077464	36.587392
1590.880152	224016.785854	36.592410
1592.290485	224396.247882	36.597428
1593.999209	224781.324201	36.602445
1595.302740	225164.362804	36.607463
1597.316669	225541.667547	36.612480
1599.157312	225919.942840	36.617498
1600.461391	226290.690925	36.622516
1602.303254	226667.139308	36.627533
1604.020613	227036.574111	36.632551
1605.505399	227408.742157	36.637568
1607.186300	227778.058177	36.642586
1608.755479	228120.901389	36.647604
1610.452470	228470.454748	36.652621
1612.114755	228822.326363	36.657639
1613.806686	229165.125652	36.662656
1615.112670	229529.811148	36.667674
1616.578582	229870.009038	36.672692
1618.154024	230221.390799	36.677709
1619.017083	230590.726810	36.682727
1620.597146	230941.804600	36.687744
1622.037068	231320.340440	36.692762
1623.709985	231689.184829	36.697780
1625.107898	232068.898067	36.702797
1626.549509	232445.632738	36.707815
1628.355160	232828.529318	36.712832
1629.749902	233214.088015	36.717850
1631.515657	233600.777961	36.722868
1632.991319	233988.509052	36.727885
1634.532126	234393.655369	36.732903
1636.222528	234784.399622	36.737920
1637.216033	235192.918159	36.742938
1638.495050	235599.127963	36.747956
1640.364049	236012.223193	36.752973
1641.621505	236441.223920	36.757991
1643.681146	236861.197619	36.763008
1645.552675	237279.197602	36.768026
1646.954436	237691.182295	36.773044
1648.390772	238125.922171	36.778061
1649.790007	238563.768322	36.783079
1651.333289	239000.193560	36.788096
1652.700227	239452.729437	36.793114
1654.317936	239894.122460	36.798132
1655.976204	240338.887863	36.803149
1657.637527	240798.742574	36.808167
1659.346129	241237.023332	36.813184
1660.727476	241692.507500	36.818202
1662.254945	242151.066543	36.823220
1664.355643	242607.623069	36.828237
1665.417807	243075.738377	36.833255
1667.262227	243544.381052	36.838272
1668.747634	244025.025131	36.843290
1670.589809	244490.037010	36.848308
1672.728689	244960.714399	36.853325
1674.960861	245435.872765	36.858343
1677.285318	245879.922891	36.863360
1678.662922	246330.308435	36.868378
1680.615615	246769.418831	36.873396
1683.133760	247225.605334	36.878413
1684.101307	247685.639426	36.883431
1685.789227	248111.612366	36.888448
1687.553279	248570.926801	36.893466
1689.541016	249028.958641	36.898484
1691.609741	249458.347794	36.903501
1693.358138	249904.608906	36.908519
1695.980980	250332.608353	36.913536
1697.909904	250748.609531	36.918554
1699.793977	251153.669897	36.923572
1701.449957	251539.539346	36.928589
1702.835782	251935.794281	36.933607
1704.835301	252315.762604	36.938624
1706.380177	252703.302798	36.943642
1708.345445	253096.334512	36.948660
1710.913071	253471.658913	36.953677
1712.941785	253842.426844	36.958695
1714.866730	254218.064635	36.963712
1716.167889	254582.250778	36.968730
1718.095723	254961.647909	36.973748
1720.266670	255328.555943	36.978765
1721.702182	255696.631374	36.983783
1723.332640	256066.985180	36.988800
1724.869575	256423.916713	36.993818
1726.168926	256813.023958	36.998836
1727.661187	257189.498209	37.003853
1729.142333	257580.657397	37.008871
1730.759003	257973.165143	37.013888
1732.001290	258372.773577	37.018906
1733.450764	258767.189655	37.023924
1735.370250	259174.684099	37.028941
1736.668726	259590.540719	37.033959
1738.048983	260000.616708	37.038976
1739.774441	260413.732694	37.043994
1740.845052	260842.608898	37.049012
1742.441688	261285.138028	37.054029
1743.934561	261732.485884	37.059047
1745.866628	262174.423707	37.064064
1747.410215	262634.768767	37.069082
1748.704317	263085.045776	37.074100
1750.548626	263536.523901	37.079117
1752.206947	264012.039380	37.084135
1753.504850	264477.785147	37.089152
1755.437271	264960.568978	37.094170
1756.968976	265445.707159	37.099188
1758.875760	265924.455341	37.104205
1760.347328	266413.972089	37.109223
1762.450904	266890.627903	37.114240
1764.281677	267381.225184	37.119258
1766.375818	267861.285420	37.124276
1768.442719	268321.941957	37.129293
1770.445682	268815.810232	37.134311
1772.572017	269269.596597	37.139328
1774.759779	269732.669204	37.144346
1777.220903	270193.357324	37.149364
1779.742335	270632.823253	37.154381
1782.152261	271071.799550	37.159399
1784.194789	271504.639803	37.164416
1785.850050	271932.515935	37.169434
1787.407102	272365.641091	37.174452
1789.345980	272800.021138	37.179469
1791.045952	273248.031575	37.184487
1792.431414	273673.436138	37.189504
1794.374090	274101.361066	37.194522
1795.656640	274523.403215	37.199540
1797.218873	274946.184213	37.204557
1799.109334	275370.864231	37.209575
1800.623223	275784.735755	37.214592
1802.182930	276218.132803	37.219610
1803.529494	276650.879563	37.224628
1805.660114	277081.636950	37.229645
1806.805510	277522.824299	37.234663
1808.606913	277963.669825	37.239680
1810.283542	278415.509241	37.244698
1811.705644	278870.185299	37.249716
1813.168880	279336.868168	37.254733
1814.515751	279801.385204	37.259751
1816.133167	280284.093010	37.264768
1817.893859	280768.070437	37.269786
1819.050508	281268.787690	37.274804
1820.996645	281752.857570	37.279821
1823.236434	282255.926674	37.284839
1825.031594	282743.473976	37.289856
1827.492877	283235.198595	37.294874
1829.165668	283741.916072	37.299892
1831.087278	284234.847428	37.304909
1833.032843	284739.101795	37.309927
1834.885096	285235.013557	37.314944
1837.284519	285719.907752	37.319962
1839.357620	286235.920916	37.324980
1840.848647	286731.482791	37.329997
1842.596327	287239.699122	37.335015
1843.964109	287747.800706	37.340032
1846.119361	288260.515454	37.345050
1847.337930	288775.902997	37.350068
1849.169340	289294.968218	37.355085
1850.589575	289823.880548	37.360103
1852.045559	290361.344196	37.365120
1854.367519	290895.787189	37.370138
1855.821110	291444.295235	37.375156
1857.664390	291981.990146	37.380173
1859.466415	292545.876222	37.385191
1861.362854	293088.179526	37.390208
1863.541677	293643.969567	37.395226
1865.360477	294195.729183	37.400244
1867.253792	294744.831796	37.405261
1868.868059	295293.801544	37.410279
1871.264682	295840.221775	37.415296
1873.593418	296387.996871	37.420314
1875.504482	296939.066064	37.425332
1877.616325	297491.317033	37.430349
1879.334101	298032.000120	37.435367
1880.988009	298587.472676	37.440384
1882.815295	299139.585328	37.445402
1884.790794	299696.901345	37.450420
1886.902800	300245.327080	37.455437
1889.195954	300799.737757	37.460455
1891.142474	301334.191552	37.465472
1893.022790	301864.590052	37.470490
1894.667714	302393.451107	37.475508
1896.766769	302906.536275	37.480525
1898.357410	303437.711495	37.485543
1899.803695	303971.219241	37.490560
1901.664584	304498.024396	37.495578
1903.671088	305035.289930	37.500596
1905.574359	305564.392261	37.505613
1907.735401	306086.691916	37.510631
1910.018973	306614.605112	37.515648
1912.175418	307139.286048	37.520666
1913.898243	307663.301291	37.525684
1916.266032	308189.361370	37.530701
1918.350868	308719.961239	37.535719
1920.290068	309244.640086	37.540736
1921.941727	309767.688538	37.545754
1923.775739	310295.019278	37.550772
1925.877337	310827.633369	37.555789
1927.866725	311356.047500	37.560807
1929.517155	311885.709374	37.565824
1931.324331	312419.505197	37.570842
1932.872816	312970.812026	37.575860
1934.644096	313514.204675	37.580877
1936.473235	314076.424923	37.585895
1937.982765	314641.260067	37.590912
1940.002277	315210.472558	37.595930
1941.682589	315770.673344	37.600948
1943.900721	316343.295947	37.605965
1945.391668	316916.292051	37.610983
1947.918147	317484.205605	37.616000
1950.324676	318051.474694	37.621018
1952.205331	318624.973583	37.626036
1954.379763	319187.752986	37.631053
1956.707509	319764.694815	37.636071
1958.126181	320324.622909	37.641088
1960.254411	320897.805515	37.646106
1962.361268	321479.086080	37.651124
1964.310904	322050.029075	37.656141
1966.447505	322624.337099	37.661159
1968.021104	323201.452760	37.666176
1970.669892	323773.935998	37.671194
1972.379031	324368.993035	37.676212
1973.585325	324943.336823	37.681229
1975.703154	325536.205140	37.686247
1977.516223	326132.851724	37.691264
1979.333437	326712.989356	37.696282
1981.613232	327307.360786	37.701300
1983.642042	327895.498324	37.706317
1986.077459	328490.287901	37.711335
1987.547815	329086.175619	37.716352
1989.267218	329669.498820	37.721370
1990.776314	330280.573857	37.726388
1992.855503	330879.841668	37.731405
1995.021879	331495.842695	37.736423
1996.843832	332105.879297	37.741440
1998.985011	332699.912483	37.746458
2000.831032	333304.295880	37.751476
2002.882772	333890.969489	37.756493
2005.058285	334471.294701	37.761511
2006.694205	335057.087211	37.766528
2008.933974	335641.881431	37.771546
2010.605618	336240.904837	37.776564
2012.589382	336828.902303	37.781581
2014.767431	337429.805068	37.786599
2016.533423	338039.325114	37.791616
2018.800075	338632.482046	37.796634
2020.586251	339243.126166	37.801652
2022.702526	339840.609318	37.806669
2024.957218	340447.757229	37.811687
2026.237553	341078.617858	37.816704
2028.531150	341699.296959	37.821722
2030.185760	342327.589915	37.826740
2032.229994	342960.452514	37.831757
2034.378513	343586.766214	37.836775
2035.708230	344226.510394	37.841792
2037.844629	344866.666185	37.846810
2039.925226	345532.861208	37.851828
2041.305828	346190.156964	37.856845
2043.291707	346857.186385	37.861863
2045.190790	347530.235301	37.866880
2047.671170	348181.527970	37.871898
2049.745002	348852.065529	37.876916
2052.162941	349526.340550	37.881933
2054.765996	350193.696656	37.886951
2056.779504	350867.791788	37.891968
2059.254208	351529.135302	37.896986
2061.551621	352181.211755	37.902004
2064.092713	352843.056507	37.907021
2066.436817	353491.171855	37.912039
2068.353255	354157.771668	37.917056
2070.550000	354805.663555	37.922074
2072.463982	355463.133904	37.927092
2074.238521	356126.757769	37.932109
2076.574071	356791.340588	37.937127
2078.215667	357460.369782	37.942144
2080.219877	358126.611184	37.947162
2081.987681	358809.829669	37.952180
2083.920371	359484.686784	37.957197
2086.363782	360158.278064	37.962215
2087.994939	360846.558815	37.967232
2090.367218	361522.371369	37.972250
2092.313867	362209.280304	37.977268
2094.266230	362903.761125	37.982285
2096.408576	363593.630705	37.987303
2098.197666	364289.610974	37.992320
2100.360695	364990.156630	37.997338
2102.484229	365682.629515	38.002356
2104.824229	366373.758902	38.007373
2107.228495	367057.559216	38.012391
2109.590689	367764.385365	38.017408
2111.876732	368431.287359	38.022426
2113.807706	369105.542680	38.027444
2115.940604	369766.029292	38.032461
2117.987603	370427.888084	38.037479
2120.363014	371095.232882	38.042496
2122.219266	371752.280859	38.047514
2124.546574	372415.094622	38.052532
2126.484601	373076.846573	38.057549
2128.807778	373724.343559	38.062567
2130.813542	374398.967414	38.067584
2133.277140	375052.172358	38.072602
2135.629533	375712.230889	38.077620
2137.498499	376376.568884	38.082637
2139.560716	377041.291952	38.087655
2141.689074	377719.810586	38.092672
2143.855315	378385.174041	38.097690
2145.846240	379056.893404	38.102708
2148.206109	379753.714769	38.107725
2150.202805	380424.239074	38.112743
2152.015963	381117.930290	38.117760
2153.832513	381797.458380	38.122778
2156.378473	382494.874264	38.127796
2158.096200	383186.458659	38.132813
2160.267057	383890.246876	38.137831
2162.256086	384592.098568	38.142848
2164.663338	385303.218077	38.147866
2166.517136	386016.114762	38.152884
2168.293001	386728.298801	38.157901
2170.615214	387452.997541	38.162919
2173.094860	388190.986292	38.167936
2175.657897	388910.362474	38.172954
2177.807812	389632.884954	38.177972
2180.073709	390366.092597	38.182989
2182.414416	391086.722996	38.188007
2184.476379	391815.570791	38.193024
2186.754629	392544.972255	38.198042
2188.403246	393281.509562	38.203060
2190.577177	394025.288756	38.208077
2192.848531	394748.301275	38.213095
2194.979887	395498.893492	38.218112
2196.862921	396244.440403	38.223130
2199.487834	396994.478978	38.228148
2201.117732	397760.126463	38.233165
2203.352804	398515.235133	38.238183
2205.254867	399281.859855	38.243200
2207.203704	400047.619766	38.248218
2209.800690	400819.557492	38.253236
2211.697603	401596.889396	38.258253
2214.501504	402352.305364	38.263271
2216.576653	403138.406638	38.268288
2218.888731	403916.692383	38.273306
2221.673472	404682.739864	38.278324
2223.590139	405452.765201	38.283341
2225.934489	406212.790246	38.288359
2228.062144	406999.633327	38.293376
2230.652789	407761.878103	38.298394
2233.186621	408495.283723	38.303412
2235.088752	409232.044909	38.308429
2237.767135	409954.696096	38.313447
2239.907684	410681.320252	38.318464
2242.036914	411421.907777	38.323482
2244.159144	412148.697157	38.328500
2246.193621	412885.232327	38.333517
2248.351263	413636.060412	38.338535
2250.039942	414382.818764	38.343552
2252.342168	415140.492305	38.348570
2254.205716	415907.157921	38.353588
2256.054256	416685.755769	38.358605
2257.877080	417452.331117	38.363623
2259.876029	418248.707721	38.368640
2262.129714	419045.370023	38.373658
2263.981239	419844.253233	38.378676
2266.072614	420664.363516	38.383693
2267.999184	421477.132367	38.388711
2270.240215	422292.706864	38.393728
2272.684516	423127.612280	38.398746
2274.810792	423959.708052	38.403764
2276.622452	424814.916562	38.408781
2279.480340	425652.145224	38.413799
2281.537647	426507.099705	38.418816
2283.827842	427363.907514	38.423834
2286.439622	428213.440940	38.428852
2288.914502	429075.723831	38.433869
2291.185835	429928.746515	38.438887
2293.749558	430789.584479	38.443904
2296.197842	431646.361074	38.448922
2299.220490	432497.743934	38.453940
2301.299578	433363.782310	38.458957
2303.662843	434220.123472	38.463975
2305.900952	435081.109857	38.468992
2308.215840	435938.609242	38.474010
2310.609173	436803.552133	38.479028
2312.861680	437668.840046	38.484045
2315.138111	438545.424921	38.489063
2317.074190	439428.257086	38.494080
2319.596398	440288.286666	38.499098
2321.560833	441165.377806	38.504116
2323.806999	442054.679698	38.509133
2326.416328	442934.928802	38.514151
2328.718592	443816.510038	38.519168
2331.030377	444706.096928	38.524186
2333.853591	445579.676200	38.529204
2335.531041	446477.037539	38.534221
2338.344564	447362.533527	38.539239
2341.107855	448248.051719	38.544256
2343.663567	449131.949836	38.549274
2346.400833	450003.743228	38.554292
2348.328323	450889.495301	38.559309
2350.871035	451763.321885	38.564327
2353.054429	452651.281299	38.569344
2355.549543	453522.159373	38.574362
2358.192505	454371.233193	38.579380
2360.306992	455213.688059	38.584397
2362.821383	456062.056203	38.589415
2364.898332	456915.468721	38.594432
2367.384143	457762.860395	38.599450
2369.688467	458601.451248	38.604468
2371.876912	459456.809442	38.609485
2374.169013	460299.779476	38.614503
2376.723577	461146.864141	38.619520
2379.229896	462008.275144	38.624538
2381.991661	462853.330395	38.629556
2383.985184	463710.256165	38.634573
2386.552938	464555.321532	38.639591
2388.881086	465410.548600	38.644608
2391.512851	466275.994615	38.649626
2394.096296	467130.748093	38.654644
2396.498676	467996.610608	38.659661
2399.236451	468854.241887	38.664679
2401.787641	469701.509056	38.669696
2403.873838	470579.029519	38.674714
2406.426641	471431.776186	38.679732
2408.233868	472312.294677	38.684749
2410.435992	473183.460137	38.689767
2412.661790	474079.786208	38.694784
2414.844573	474977.945172	38.699802
2417.468192	475878.106409	38.704820
2419.053375	476799.208882	38.709837
2421.156088	477708.106660	38.714855
2423.316904	478637.350921	38.719872
2425.300985	479577.889091	38.724890
2427.714582	480514.265414	38.729908
2429.812851	481467.914971	38.734925
2432.441517	482407.942675	38.739943
2434.954099	483368.084612	38.744960
2436.985934	484325.278333	38.749978
2439.975944	485290.383863	38.754996
2441.851264	486263.955854	38.760013
2444.644975	487232.774108	38.765031
2446.955102	488213.128893	38.770048
2449.275731	489204.075607	38.775066
2451.590910	490190.374103	38.780084
2453.955333	491195.228724	38.785101
2456.679004	492180.233091	38.790119
2459.296886	493184.170762	38.795136
2461.610996	494181.138385	38.800154
2464.327665	495184.789477	38.805172
2466.832907	496188.669212	38.810189
2469.267200	497197.444710	38.815207
2471.975169	498197.335585	38.820224
2474.378610	499197.369763	38.825242
2477.359848	500197.698783	38.830260
2479.479759	501209.108830	38.835277
2482.361397	502192.135983	38.840295
2485.256375	503197.390606	38.845312
2487.885747	504182.559845	38.850330
2491.134470	505122.184464	38.855348
2493.735953	506073.864603	38.860365
2496.335301	507015.557064	38.865383
2499.498595	507942.478291	38.870400
2501.983959	508864.622295	38.875418
2504.764924	509787.418451	38.880436
2506.903590	510718.083216	38.885453
2508.949409	511642.156956	38.890471
2511.286893	512579.985924	38.895488
2513.619877	513527.132940	38.900506
2516.116608	514458.119660	38.905524
2518.964462	515394.432617	38.910541
2520.984229	516336.221767	38.915559
2523.708717	517283.878923	38.920576
2525.947078	518229.192957	38.925594
2528.458458	519193.041160	38.930612
2530.953072	520149.426574	38.935629
2533.443768	521104.845867	38.940647
2536.313882	522063.514630	38.945664
2538.596097	523040.101929	38.950682
2541.289505	524007.994348	38.955700
2543.703974	524984.281470	38.960717
2546.248679	525965.366752	38.965735
2548.657361	526947.971393	38.970752
2550.964015	527943.064608	38.975770
2553.125620	528944.408411	38.980788
2555.533846	529951.934334	38.985805
2557.844794	530963.283451	38.990823
2560.417768	531975.020998	38.995840
2562.867097	533003.267550	39.000858
2565.883025	534021.681701	39.005876
2568.490370	535049.604606	39.010893
2570.917980	536076.427969	39.015911
2573.718614	537103.667358	39.020928
2576.036897	538137.707148	39.025946
2578.964861	539168.448377	39.030964
2582.018960	540212.876179	39.035981
2584.511939	541229.858560	39.040999
2587.662244	542261.995364	39.046016
2589.539950	543289.948263	39.051034
2592.589189	544317.122232	39.056052
2595.265569	545353.636954	39.061069
2597.613656	546391.035137	39.066087
2600.563616	547432.224284	39.071104
2602.893924	548464.893746	39.076122
2605.978961	549509.421066	39.081140
2608.959758	550535.840498	39.086157
2611.746595	551564.477241	39.091175
2614.462896	552584.151990	39.096192
2616.505132	553614.820299	39.101210
2618.917812	554648.009479	39.106228
2621.837715	555694.247139	39.111245
2624.427962	556736.540012	39.116263
2626.641211	557773.037974	39.121280
2629.320457	558810.379800	39.126298
2631.781312	559820.652858	39.131316
2634.218275	560835.372758	39.136333
2636.578045	561856.054001	39.141351
2639.228525	562867.967913	39.146368
2641.540125	563900.399149	39.151386
2643.840002	564918.992087	39.156404
2646.658805	565943.089429	39.161421
2649.625222	566984.299838	39.166439
2652.766879	567999.643296	39.171456
2655.251580	569029.876165	39.176474
2658.005161	570061.736385	39.181492
2660.542728	571098.919600	39.186509
2662.863270	572148.299483	39.191527
2665.872659	573196.922248	39.196544
2668.263561	574245.262001	39.201562
2671.092100	575292.134652	39.206580
2674.460213	576333.208505	39.211597
2676.956047	577378.256754	39.216615
2680.146198	578425.405379	39.221632
2682.725577	579486.010616	39.226650
2684.879295	580529.546273	39.231668
2687.617732	581598.166218	39.236685
2689.748890	582671.309008	39.241703
2692.286031	583741.480124	39.246720
2694.865972	584836.715531	39.251738
2697.044349	585934.526833	39.256756
2699.499212	587030.336224	39.261773
2701.854034	588152.224091	39.266791
2704.639727	589272.479728	39.271808
2707.228079	590404.439126	39.276826
2709.678350	591538.719072	39.281844
2711.839352	592686.516340	39.286861
2713.940036	593847.136243	39.291879
2716.773876	595018.184992	39.296896
2719.241018	596193.987114	39.301914
2721.948733	597374.837611	39.306932
2724.571201	598564.545652	39.311949
2726.971226	599768.038171	39.316967
2730.024874	600968.689996	39.321984
2732.791216	602177.424674	39.327002
2735.406474	603387.358720	39.332020
2738.238884	604608.137476	39.337037
2740.528378	605837.835089	39.342055
2743.663512	607063.902037	39.347072
2746.334628	608301.371782	39.352090
2748.968622	609524.654310	39.357108
2752.470686	610765.011461	39.362125
2754.856413	612003.720669	39.367143
2757.617807	613248.778491	39.372160
2760.415237	614490.689723	39.377178
2763.175171	615729.867427	39.382196
2765.942163	616981.201840	39.387213
2768.532353	618229.424036	39.392231
2772.280191	619465.060253	39.397248
2775.033309	620699.376324	39.402266
2778.172774	621895.509205	39.407284
2781.376902	623079.606916	39.412301
2784.445449	624264.446412	39.417319
2787.334238	625428.205383	39.422336
2789.784191	626603.849546	39.427354
2792.975774	627791.472497	39.432372
2796.285032	628972.250702	39.437389
2798.787333	630151.436815	39.442407
2802.040659	631305.999203	39.447424
2804.999902	632482.299187	39.452442
2807.109326	633658.462095	39.457460
2809.996885	634841.795397	39.462477
2812.513407	636024.258637	39.467495
2815.214604	637209.548834	39.472512
2817.307649	638401.392085	39.477530
2820.272781	639602.176663	39.482548
2823.324323	640809.040383	39.487565
2825.832273	642031.264789	39.492583
2828.384072	643242.413892	39.497600
2831.408198	644471.287325	39.502618
2834.152808	645691.932556	39.507636
2837.223175	646919.901123	39.512653
2839.738236	648161.720129	39.517671
2842.767572	649399.060821	39.522688
2845.535195	650649.298020	39.527706
2848.380696	651893.186205	39.532724
2851.371398	653146.457995	39.537741
2854.336176	654396.187616	39.542759
2857.154366	655648.920875	39.547776
2860.104372	656919.946345	39.552794
2862.805863	658179.595643	39.557812
2865.877135	659451.514558	39.562829
2868.329282	660715.108886	39.567847
2871.415835	661988.483354	39.572864
2874.433279	663262.596772	39.577882
2877.374837	664545.112266	39.582900
2880.637550	665820.932875	39.587917
2883.513881	667103.612803	39.592935
2886.588588	668378.922992	39.597952
2889.228936	669667.065619	39.602970
2891.921856	670951.442906	39.607988
2894.827953	672239.535806	39.613005
2897.809807	673530.719369	39.618023
2900.884713	674816.688049	39.623040
2903.524365	676117.760582	39.628058
2906.372291	677418.614737	39.633076
2909.931038	678715.239088	39.638093
2912.423554	680016.035569	39.643111
2915.397535	681314.926116	39.648128
2918.536556	682623.834238	39.653146
2921.355018	683920.741284	39.658164
2924.449710	685224.813346	39.663181
2926.990252	686535.642440	39.668199
2929.904867	687829.688915	39.673216
2932.701757	689134.635798	39.678234
2935.411737	690411.918101	39.683252
2938.462296	691685.784179	39.688269
2940.734674	692959.203849	39.693287
2943.655716	694242.398233	39.698304
2946.505487	695530.526281	39.703322
2949.012572	696821.846543	39.708340
2951.660872	698118.306961	39.713357
2954.155663	699441.120828	39.718375
2957.121818	700758.003530	39.723392
2959.470214	702093.870379	39.728410
2962.235586	703423.564019	39.733428
2964.882026	704785.471218	39.738445
2967.673694	706152.982613	39.743463
2970.555987	707520.309942	39.748480
2973.835507	708884.775869	39.753498
2976.017644	710267.379476	39.758516
2979.796253	711654.138037	39.763533
2982.661508	713058.146734	39.768551
2986.312748	714445.161378	39.773568
2989.429778	715840.646623	39.778586
2992.304237	717241.480780	39.783604
2995.355325	718646.945793	39.788621
2998.519078	720065.752338	39.793639
3001.638308	721458.713452	39.798656
3004.711069	722876.954342	39.803674
3007.618614	724288.455118	39.808692
3010.925033	725706.464045	39.813709
3013.977265	727129.803805	39.818727
3016.967140	728556.906648	39.823744
3019.960015	729981.535548	39.828762
3022.773623	731413.844948	39.833780
3026.267868	732829.540444	39.838797
3029.704643	734254.967486	39.843815
3033.167380	735677.668591	39.848832
3035.996826	737104.369129	39.853850
3038.857065	738535.643382	39.858868
3041.820344	739962.646057	39.863885
3044.763591	741404.485702	39.868903
3048.054288	742842.648887	39.873920
3051.337936	744272.415093	39.878938
3054.292514	745710.799125	39.883956
3057.620021	747146.340575	39.888973
3060.651702	748579.844078	39.893991
3063.423746	750029.728280	39.899008
3066.767477	751467.125778	39.904026
3069.592865	752925.321462	39.909044
3072.597156	754370.506292	39.914061
3075.631926	755818.809050	39.919079
3078.745255	757269.037565	39.924096
3082.651263	758725.447261	39.929114
3085.605642	760161.420049	39.934132
3089.013892	761591.237406	39.939149
3092.399634	763046.507199	39.944167
3095.538465	764468.199094	39.949184
3098.803796	765886.304737	39.954202
3101.528362	767278.231302	39.959220
3104.837890	768661.540774	39.964237
3107.963914	770053.613976	39.969255
3111.170968	771421.094069	39.974272
3114.536634	772808.674986	39.979290
3117.165744	774186.150339	39.984308
3120.136866	775561.245315	39.989325
3123.193542	776955.062333	39.994343
3126.060287	778345.503022	39.999360
3129.187761	779738.821231	40.004378
3132.036684	781145.408675	40.009396
3135.313900	782549.930972	40.014413
3137.846679	783964.603155	40.019431
3140.782498	785392.017038	40.024448
3143.931018	786822.784814	40.029466
3146.261342	788273.399546	40.034484
3149.301172	789723.742671	40.039501
3151.863531	791187.928802	40.044519
3154.733626	792670.173305	40.049536
3157.818680	794161.175547	40.054554
3160.686115	795662.667223	40.059572
3163.928747	797176.839716	40.064589
3167.152420	798693.474268	40.069607
3170.230764	800215.671967	40.074624
3173.536462	801759.506069	40.079642
3176.338800	803299.606931	40.084660
3179.809651	804831.717712	40.089677
3183.076409	806381.507564	40.094695
3186.390639	807932.841985	40.099712
3189.869254	809485.894115	40.104730
3193.124515	811039.506498	40.109748
3196.636476	812602.630233	40.114765
3199.922016	814168.016126	40.119783
3203.416721	815719.771371	40.124800
3207.126178	817262.490616	40.129818
3210.326629	818827.821287	40.134836
3213.751302	820372.695306	40.139853
3217.127908	821912.631639	40.144871
3220.881454	823463.503262	40.149888
3224.574599	824990.328232	40.154906
3227.828759	826532.368599	40.159924
3231.201570	828066.910193	40.164941
3234.380435	829603.655091	40.169959
3237.454309	831141.806115	40.174976
3241.100024	832664.302276	40.179994
3244.410791	834198.858686	40.185012
3247.846509	835727.478604	40.190029
3251.260263	837245.178900	40.195047
3255.142716	838765.015393	40.200064
3258.146495	840278.121658	40.205082
3261.342459	841802.112577	40.210100
3264.521291	843314.364470	40.215117
3267.976988	844842.921751	40.220135
3270.819838	846348.280095	40.225152
3274.249495	847844.821472	40.230170
3277.684632	849332.553097	40.235188
3281.078830	850785.272355	40.240205
3284.141238	852236.639595	40.245223
3287.304618	853700.167765	40.250240
3290.620711	855164.001026	40.255258
3293.432149	856638.532581	40.260276
3296.623011	858108.085936	40.265293
3299.494487	859585.484075	40.270311
3302.154948	861061.105337	40.275328
3305.458173	862556.802415	40.280346
3308.381994	864068.083210	40.285364
3311.519098	865584.469606	40.290381
3314.210757	867113.718907	40.295399
3317.196276	868656.468288	40.300416
3320.362612	870194.819957	40.305434
3323.354461	871762.799413	40.310452
3326.600966	873335.544663	40.315469
3329.739357	874925.104198	40.320487
3332.446487	876521.946647	40.325504
3335.772830	878121.245828	40.330522
3338.407476	879761.583550	40.335540
3341.685875	881393.332660	40.340557
3345.004595	883034.274765	40.345575
3348.200329	884693.020947	40.350592
3351.480282	886348.284757	40.355610
3354.620304	888032.333666	40.360628
3357.678711	889714.552238	40.365645
3361.032212	891406.930205	40.370663
3364.093320	893115.341253	40.375680
3367.676374	894823.053492	40.380698
3371.095005	896551.957061	40.385716
3374.457766	898274.947100	40.390733
3378.276446	899993.576601	40.395751
3381.295598	901728.083488	40.400768
3384.953460	903460.307285	40.405786
3388.294220	905195.702071	40.410804
3392.023026	906935.969717	40.415821
3395.853224	908681.729297	40.420839
3399.465870	910418.515885	40.425856
3403.433036	912142.491327	40.430874
3406.987169	913879.825211	40.435892
3410.422101	915607.312967	40.440909
3414.082048	917331.526173	40.445927
3417.249606	919064.582682	40.450944
3420.665232	920787.832390	40.455962
3423.846422	922538.379634	40.460980
3427.471024	924273.038352	40.465997
3430.694044	926020.236032	40.471015
3433.870437	927761.504403	40.476032
3437.441071	929504.624852	40.481050
3440.803329	931266.545705	40.486068
3443.575619	933016.877514	40.491085
3446.742239	934777.753253	40.496103
3450.101221	936559.427915	40.501120
3453.478649	938315.072291	40.506125
3456.530198	940033.455697	40.511130
3459.766321	941694.244627	40.516135
3463.012008	943303.363720	40.521140
3465.694708	944847.076395	40.526144
3469.297190	946306.716234	40.531149
3472.082351	947705.229842	40.536154
3475.314412	949021.885244	40.541159
3478.308685	950266.807018	40.546164
3481.032675	951452.215083	40.551168
3483.899040	952571.936859	40.556173
3486.372854	953621.588756	40.561178
3488.885091	954593.781716	40.566183
3491.632634	955497.638228	40.571188
3493.487131	956328.481990	40.576192
3495.924331	957077.664147	40.581197
3497.816861	957784.508605	40.586202
3499.905547	958401.774650	40.591207
3502.415392	958961.490190	40.596212
3504.136815	959461.135410	40.601216
3505.941009	959906.454736	40.606221
3507.665649	960296.508960	40.611226
3509.083406	960625.373450	40.616231
3510.511038	960907.206062	40.621236
3511.531427	961156.775405	40.626240
3513.071230	961342.686859	40.631245
3514.103446	961485.295701	40.636250
3515.359185	961598.680083	40.641255
3516.748129	961664.152961	40.646260
3517.711516	961696.598394	40.651264
3518.636726	961692.915074	40.656269
3519.664491	961663.850988	40.661274
3520.815165	961584.136598	40.666279
3521.596142	961481.372553	40.671284
3522.214375	961352.094633	40.676288
3523.223341	961190.428359	40.681293
3524.035116	961015.471540	40.686298
3524.204447	960814.174707	40.691303
3524.888181	960582.713613	40.696308
3525.550917	960342.137430	40.701312
3525.879969	960068.793332	40.706317
3526.181295	959793.579759	40.711322
3527.040848	959488.280582	40.716327
3527.889653	959173.072085	40.721332
3527.657820	958846.077775	40.726336
3528.107951	958502.585583	40.731341
3528.854526	958145.793996	40.736346
3529.113128	957774.854512	40.741351
3529.856749	957389.794308	40.746356
3529.512976	956996.955426	40.751360
3529.798185	956578.498733	40.756365
3530.143796	956181.173961	40.761370
3530.259544	955751.609809	40.766375
3530.828881	955318.210888	40.771380
3530.765882	954881.455847	40.776384
3531.383653	954426.412157	40.781389
3531.437156	953966.722107	40.786394
3531.359067	953506.331447	40.791399
3531.712502	953041.809368	40.796404
3531.878891	952565.315809	40.801408
3532.324867	952079.122339	40.806413
3532.540495	951591.553900	40.811418
3532.529956	951090.051681	40.816423
3532.819119	950597.164668	40.821428
3532.698540	950104.226814	40.826432
3533.182633	949606.451613	40.831437
3533.009722	949110.939927	40.836442
3532.911206	948599.966166	40.841447
3533.266726	948091.351188	40.846452
3533.222492	947582.945213	40.851456
3533.410819	947056.842293	40.856461
3533.222317	946545.008762	40.861466
3533.324891	946028.001916	40.866471
3533.665864	945499.511870	40.871476
3533.268794	944974.922561	40.876480
3533.983869	944444.154159	40.881485
3534.034702	943919.093537	40.886490
3533.783181	943383.880758	40.891495
3533.543866	942838.363245	40.896500
3533.657313	942302.592955	40.901504
3533.881909	941755.924185	40.906509
3533.944310	941221.200040	40.911514
3534.100134	940667.722291	40.916519
3534.281293	940119.738573	40.921524
3533.962420	939568.045071	40.926528
3534.188108	939012.845691	40.931533
3534.466290	938463.904086	40.936538
3533.984875	937909.953778	40.941543
3534.370685	937352.824622	40.946548
3533.855190	936799.433238	40.951552
3534.007646	936234.362497	40.956557
3534.217299	935684.468946	40.961562
3534.308799	935120.726836	40.966567
3534.735241	934550.823949	40.971572
3534.009181	933985.756480	40.976576
3534.521578	933411.686177	40.981581
3534.246648	932850.736964	40.986586
3534.294223	932277.581765	40.991591
3534.663535	931710.739418	40.996596
3534.156095	931142.546092	41.001600
3534.435212	930549.295227	41.006605
3534.305313	929987.344736	41.011610
3534.232778	929417.067623	41.016615
3534.776858	928837.885692	41.021620
3534.796514	928265.452459	41.026624
3534.403493	927679.773770	41.031629
3534.401154	927102.032505	41.036634
3534.380425	926518.755903	41.041639
3534.531925	925928.948920	41.046644
3534.369433	925361.710746	41.051648
3534.334022	924770.558521	41.056653
3534.417601	924194.601757	41.061658
3534.617340	923611.931031	41.066663
3534.571872	923018.664640	41.071668
3534.321647	922428.828596	41.076672
3534.371528	921843.684020	41.081677
3534.373465	921265.695957	41.086682
3534.463005	920677.436785	41.091687
3534.697995	920074.757551	41.096692
3534.136503	919497.156851	41.101696
3534.255631	918910.238975	41.106701
3534.444520	918319.781827	41.111706
3534.260825	917716.911072	41.116711
3534.573596	917133.905145	41.121716
3534.465956	916538.589087	41.126720
3534.432328	915947.045333	41.131725
3534.127110	915364.917567	41.136730
3534.329428	914773.109641	41.141735
3534.652450	914174.573121	41.146740
3534.242208	913583.607255	41.151744
3534.337990	912976.407788	41.156749
3534.455847	912376.360980	41.161754
3534.028841	911798.689545	41.166759
3534.309275	911192.320325	41.171764
3533.880057	910602.288244	41.176768
3533.957038	910002.952245	41.181773
3533.956229	909411.466555	41.186778
3534.092477	908810.737827	41.191783
3534.354065	908215.898483	41.196788
3534.159985	907633.701353	41.201792
3534.264789	907024.300318	41.206797
3534.365541	906419.075429	41.211802
3534.136031	905822.133985	41.216807
3534.177258	905218.041745	41.221812
3534.342311	904618.203047	41.226816
3533.976184	904016.750421	41.231821
3534.174905	903411.084455	41.236826
3534.138288	902806.743623	41.241831
3534.484840	902195.806744	41.246836
3534.536697	901596.241028	41.251840
3534.535929	900987.354482	41.256845
3534.268107	900371.207810	41.261850
3534.125276	899768.680346	41.266855
3534.139900	899157.758232	41.271860
3534.001605	898556.548155	41.276864
3534.071230	897949.057966	41.281869
3534.044026	897342.581153	41.286874
3534.351943	896731.249047	41.291879
3534.116477	896119.460517	41.296884
3533.985015	895516.089691	41.301888
3534.511378	894904.136285	41.306893
3533.732709	894287.701297	41.311898
3534.147808	893670.802247	41.316903
3534.286004	893056.009823	41.321908
3534.555212	892449.634851	41.326912
3533.902688	891825.758254	41.331917
3533.963909	891223.155167	41.336922
3534.232312	890609.816850	41.341927
3534.375300	889991.695645	41.346932
3534.034919	889382.391164	41.351936
3533.801552	888757.624416	41.356941
3534.116000	888142.950008	41.361946
3533.880155	887531.109368	41.366951
3534.251527	886912.036808	41.371956
3533.806274	886295.649770	41.376960
3534.090794	885676.556045	41.381965
3533.939686	885057.470280	41.386970
3533.712154	884432.716993	41.391975
3533.805656	883812.972235	41.396980
3533.780076	883207.994623	41.401984
3533.960516	882587.813588	41.406989
3533.820376	881964.231704	41.411994
3533.651126	881342.524877	41.416999
3533.871645	880720.878833	41.422004
3533.722892	880113.953659	41.427008
3533.671107	879495.323287	41.432013
3533.662705	878875.457333	41.437018
3533.982261	878253.047219	41.442023
3534.146185	877626.139670	41.447028
3534.024546	877013.170426	41.452032
3534.220981	876387.094183	41.457037
3534.302454	875758.741257	41.462042
3534.049329	875131.541798	41.467047
3534.033758	874500.938339	41.472052
3534.175722	873872.277023	41.477056
3533.889541	873245.076653	41.482061
3534.244268	872617.506398	41.487066
3533.916967	871990.083099	41.492071
3533.968789	871354.282575	41.497076
3533.543176	870732.757965	41.502080
3533.765277	870095.629443	41.507085
3533.634917	869473.631811	41.512090
3533.983400	868847.993592	41.517095
3534.061507	868209.038132	41.522100
3533.931505	867585.193571	41.527104
3533.881845	866949.620070	41.532109
3534.063101	866324.620214	41.537114
3533.732808	865689.640733	41.542119
3533.805856	865054.428160	41.547124
3533.568659	864424.737647	41.552128
3533.837831	863791.592234	41.557133
3533.784129	863162.807054	41.562138
3533.637652	862529.891671	41.567143
3533.669104	861896.490992	41.572148
3533.398289	861256.856335	41.577152
3533.422507	860629.835301	41.582157
3533.357877	860013.359108	41.587162
3532.957632	859386.184944	41.592167
3533.229192	858759.900831	41.597172
3533.043941	858146.464241	41.602176
3532.939253	857507.865207	41.607181
3532.912360	856889.218940	41.612186
3533.007712	856264.751105	41.617191
3532.877462	855642.300702	41.622196
3532.861500	855023.464093	41.627200
3532.830252	854389.488388	41.632205
3533.013226	853768.448409	41.637210
3533.063413	853147.271140	41.642215
3533.257881	852512.090497	41.647220
3533.060177	851887.422609	41.652224
3532.809295	851259.196568	41.657229
3532.688061	850633.902308	41.662234
3533.099716	850006.506864	41.667239
3532.883665	849381.491893	41.672244
3532.817096	848763.399487	41.677248
3532.905453	848141.031676	41.682253
3533.022470	847512.558335	41.687258
3532.909925	846884.255649	41.692263
3533.037020	846253.608304	41.697268
3532.829789	845633.573590	41.702272
3532.758399	845003.808372	41.707277
3532.783446	844366.070516	41.712282
3532.585891	843745.457585	41.717287
3532.872817	843119.145290	41.722292
3532.836252	842492.923357	41.727296
3532.528076	841866.100654	41.732301
3532.419073	841238.011762	41.737306
3532.261216	840619.131376	41.742311
3532.663203	839990.343782	41.747316
3532.638157	839372.537724	41.752320
3532.696490	838735.443827	41.757325
3532.755348	838104.430936	41.762330
3532.629107	837478.898568	41.767335
3533.144837	836842.756323	41.772340
3532.761844	836216.704840	41.777344
3532.822012	835577.489574	41.782349
3532.833517	834944.903486	41.787354
3532.621439	834311.951451	41.792359
3532.603243	833671.339218	41.797364
3532.554480	833045.945345	41.802368
3532.621742	832408.755599	41.807373
3532.762450	831786.965571	41.812378
3532.088740	831154.269426	41.817383
3532.749903	830519.379061	41.822388
3532.365269	829898.131426	41.827392
3532.367968	829262.204531	41.832397
3532.191485	828633.279028	41.837402
3532.054839	827999.645298	41.842407
3532.212232	827365.020222	41.847412
3532.168473	826752.352816	41.852416
3532.000038	826118.443492	41.857421
3532.060009	825503.442213	41.862426
3531.837096	824867.954728	41.867431
3532.130314	824232.121857	41.872436
3531.731637	823620.394092	41.877440
3531.820870	822990.194398	41.882445
3532.003544	822366.371573	41.887450
3531.975480	821743.356705	41.892455
3531.886423	821109.975766	41.897460
3531.387024	820484.917472	41.902464
3531.420547	819864.501903	41.907469
3531.676638	819247.609569	41.912474
3531.479364	818620.758142	41.917479
3531.969149	817996.420774	41.922484
3531.580713	817384.259233	41.927488
3531.903007	816757.730165	41.932493
3531.846173	816138.057691	41.937498
3531.412499	815517.853553	41.942503
3531.630107	814889.551617	41.947508
3531.373512	814266.509021	41.952512
3531.621125	813639.552899	41.957517
3531.465229	813023.671402	41.962522
3531.297922	812396.278117	41.967527
3531.457403	811780.767269	41.972532
3531.202164	811158.953575	41.977536
3531.252425	810539.381118	41.982541
3531.423485	809911.894244	41.987546
3531.245118	809298.320376	41.992551
3531.328202	808677.787672	41.997556
3531.245263	808061.684843	42.002560
3531.395316	807435.588584	42.007565
3531.315287	806805.259597	42.012570
3531.437197	806192.676308	42.017575
3531.291836	805561.508066	42.022580
3531.167141	804944.198429	42.027584
3531.297178	804320.612846	42.032589
3531.317028	803699.342359	42.037594
3531.287763	803076.552945	42.042599
3531.653320	802453.541439	42.047604
3531.201174	801829.632173	42.052608
3531.368635	801203.353514	42.057613
3531.125507	800579.589340	42.062618
3531.074142	799962.799391	42.067623
3531.398951	799330.829797	42.072628
3531.424093	798705.476735	42.077632
3531.365835	798074.586060	42.082637
3531.357274	797447.604063	42.087642
3531.352586	796818.356379	42.092647
3531.458215	796184.959321	42.097652
3531.199366	795563.101290	42.102656
3531.112891	794923.585002	42.107661
3530.801989	794305.648791	42.112666
3530.422858	793687.669529	42.117671
3530.906673	793060.257424	42.122676
3530.903396	792448.192983	42.127680
3530.668315	791824.377587	42.132685
3530.738921	791208.705642	42.137690
3530.668957	790588.042874	42.142695
3530.414254	789963.525387	42.147700
3530.577520	789349.836420	42.152704
3530.970668	788727.899154	42.157709
3531.238602	788111.087735	42.162714
3531.000792	787481.925779	42.167719
3530.914715	786847.718539	42.172724
3530.675266	786232.501144	42.177728
3530.507370	785606.404752	42.182733
3530.330872	784992.691389	42.187738
3530.487032	784372.428306	42.192743
3530.813731	783743.822451	42.197748
3530.398022	783137.119307	42.202752
3530.472335	782509.628128	42.207757
3530.956115	781887.175799	42.212762
3530.774012	781263.307700	42.217767
3530.777738	780626.909507	42.222772
3530.508860	780015.392160	42.227776
3530.603552	779381.573881	42.232781
3530.731201	778773.425573	42.237786
3530.263032	778148.697032	42.242791
3530.401026	777524.549181	42.247796
3530.193010	776906.902624	42.252800
3529.961360	776285.467098	42.257805
3529.947420	775673.883763	42.262810
3530.021725	775059.182045	42.267815
3530.107973	774441.768091	42.272820
3529.947007	773827.790394	42.277824
3529.647430	773203.248062	42.282829
3530.105521	772596.151389	42.287834
3530.216957	771983.449660	42.292839
3530.442825	771359.694641	42.297844
3530.177755	770751.928609	42.302848
3530.251618	770135.286672	42.307853
3530.304478	769511.847865	42.312858
3529.948756	768883.696608	42.317863
3529.973230	768259.417913	42.322868
3529.979998	767650.512383	42.327872
3529.932736	767025.944848	42.332877
3529.818437	766409.024236	42.337882
3529.617341	765797.291580	42.342887
3529.744113	765177.073275	42.347892
3529.623330	764575.873305	42.352896
3529.577264	763960.956454	42.357901
3529.765353	763349.942535	42.362906
3529.642811	762737.994930	42.367911
3529.670373	762117.884773	42.372916
3529.417333	761507.634217	42.377920
3529.273769	760895.145383	42.382925
3529.609106	760285.533621	42.387930
3529.460992	759677.977476	42.392935
3529.544692	759065.103785	42.397940
3529.269262	758463.588663	42.402944
3529.095480	757848.785631	42.407949
3529.286150	757246.304822	42.412954
3529.341758	756646.217214	42.417959
3529.604651	756028.231346	42.422964
3529.358771	755424.496216	42.427968
3529.039699	754817.122587	42.432973
3529.132881	754208.544259	42.437978
3528.908573	753607.475316	42.442983
3529.142842	752996.209389	42.447988
3528.777905	752402.376616	42.452992
3528.899072	751787.725624	42.457997
3528.816044	751189.899489	42.463002
3528.852200	750597.043878	42.468007
3528.925860	749986.306717	42.473012
3528.580005	749390.410803	42.478016
3528.725395	748796.657327	42.483021
3528.540359	748187.155850	42.488026
3528.471132	747601.152679	42.493031
3528.931533	746999.055938	42.498036
3528.921965	746410.037606	42.503040
3528.566642	745806.900756	42.508045
3528.567402	745201.580794	42.513050
3528.345596	744607.223915	42.518055
3528.534491	744009.736643	42.523060
3528.172798	743412.989785	42.528064
3528.538659	742818.001231	42.533069
3528.663978	742227.507551	42.538074
3528.251165	741630.337214	42.543079
3528.329787	741031.405934	42.548084
3528.177674	740445.671625	42.553088
3528.298925	739841.054840	42.558093
3528.400022	739240.796942	42.563098
3528.134673	738655.493301	42.568103
3528.092477	738062.589704	42.573108
3527.893626	737469.470680	42.578112
3528.152851	736878.653313	42.583117
3527.869414	736289.022673	42.588122
3527.940868	735705.868568	42.593127
3527.853671	735112.109582	42.598132
3527.494629	734534.287579	42.603136
3527.794753	733950.224028	42.608141
3527.826672	733367.747504	42.613146
3527.428067	732778.867541	42.618151
3527.770509	732197.441064	42.623156
3527.533155	731615.229990	42.628160
3527.671041	731035.487211	42.633165
3527.956796	730451.271003	42.638170
3527.319875	729869.101179	42.643175
3527.502284	729284.075569	42.648180
3527.420058	728707.669802	42.653184
3527.557846	728114.990556	42.658189
3527.653647	727537.827531	42.663194
3527.251467	726954.715093	42.668199
3527.613069	726373.709215	42.673204
3527.372444	725793.854673	42.678208
3527.357626	725220.361099	42.683213
3527.710351	724643.643127	42.688218
3527.275078	724059.636070	42.693223
3527.470072	723476.817806	42.698228
3527.377476	722898.467495	42.703232
3526.920935	722320.188230	42.708237
3527.040940	721739.737806	42.713242
3526.914049	721175.398302	42.718247
3527.143889	720607.191939	42.723252
3527.406892	720031.603843	42.728256
3527.530813	719436.713571	42.733261
3527.278423	718862.272616	42.738266
3526.894730	718283.252528	42.743271
3527.263850	717701.980907	42.748276
3526.775236	717133.709130	42.753280
3526.873314	716563.909819	42.758285
3527.064790	715989.046239	42.763290
3526.816088	715410.994179	42.768295
3527.370810	714831.872186	42.773300
3526.670520	714275.447009	42.778304
3526.948914	713697.484601	42.783309
3526.829817	713120.046531	42.788314
3526.401930	712551.404208	42.793319
3526.534514	711980.047515	42.798324
3526.562032	711419.984827	42.803329
3526.570734	710849.168411	42.808333
3526.468793	710281.409657	42.813338
3526.718364	709708.837517	42.818343
3526.390035	709145.111596	42.823348
3526.295903	708583.194762	42.828353
3526.426554	708023.933019	42.833357
3526.522908	707459.377713	42.838362
3526.382261	706894.974540	42.843367
3526.169254	706326.673379	42.848372
3525.887386	705774.038444	42.853377
3526.023763	705209.377669	42.858381
3526.176761	704650.289133	42.863386
3526.291404	704087.147698	42.868391
3526.236890	703521.167072	42.873396
3526.004378	702970.976330	42.878401
3525.934970	702411.532291	42.883405
3525.809000	701857.626050	42.888410
3526.035508	701303.972028	42.893415
3526.222380	700736.426632	42.898420
3526.004894	700180.491182	42.903425
3525.978234	699616.486915	42.908429
3525.891053	699065.328063	42.913434
3525.437286	698520.906532	42.918439
3525.505658	697958.518429	42.923444
3525.534360	697411.410602	42.928449
3525.478624	696860.057726	42.933453
3525.793766	696299.062044	42.938458
3525.817355	695761.993716	42.943463
3526.181393	695203.803377	42.948468
3525.806118	694648.438637	42.953473
3525.721286	694089.806949	42.958477
3525.753577	693540.866736	42.963482
3525.451479	692988.169981	42.968487
3525.830990	692430.746817	42.973492
3525.562713	691882.103353	42.978497
3525.400747	691324.852464	42.983501
3525.390563	690784.652674	42.988506
3525.170627	690230.825319	42.993511
3525.490420	689691.249201	42.998516
3525.201949	689136.569718	43.003521
3524.966634	688595.579458	43.008525
3525.252585	688053.621659	43.013530
3525.055750	687505.045463	43.018535
3525.228148	686960.752083	43.023540
3525.267686	686431.926340	43.028545
3525.037760	685887.686594	43.033549
3525.182040	685335.286767	43.038554
3524.865284	684796.321922	43.043559
3525.155336	684255.678216	43.048564
3524.987946	683713.537104	43.053569
3525.423606	683174.098462	43.058573
3525.185806	682622.494738	43.063578
3525.014388	682088.422791	43.068583
3525.045652	681532.225864	43.073588
3524.523297	681002.482416	43.078593
3524.659253	680465.972397	43.083597
3525.120805	679921.655803	43.088602
3524.468683	679395.178353	43.093607
3524.643125	678853.686402	43.098612
3524.539934	678328.797462	43.103617
3524.580343	677787.215831	43.108621
3524.486006	677263.310808	43.113626
3524.328170	676730.269683	43.118631
3524.474557	676193.010520	43.123636
3524.241446	675672.277589	43.128641
3524.137545	675138.986172	43.133645
3524.503984	674614.453975	43.138650
3524.448871	674090.014000	43.143655
3524.411872	673558.414580	43.148660
3524.390938	673028.975103	43.153665
3524.227909	672501.523609	43.158669
3524.533253	671969.775305	43.163674
3524.160578	671447.534060	43.168679
3524.409130	670909.902964	43.173684
3524.145557	670385.938891	43.178689
3524.569123	669859.584719	43.183693
3524.094676	669338.440202	43.188698
3523.974399	668805.438715	43.193703
3523.987374	668284.501815	43.198708
3523.902943	667763.602718	43.203713
3524.181416	667238.872656	43.208717
3524.236513	666713.004595	43.213722
3524.015527	666199.773404	43.218727
3523.911014	665665.794590	43.223732
3523.800651	665144.606614	43.228737
3523.516408	664626.462831	43.233741
3524.035210	664098.774921	43.238746
3523.735400	663584.917566	43.243751
3523.493087	663065.734137	43.248756
3523.478954	662553.818341	43.253761
3523.387870	662036.798742	43.258765
3523.383331	661528.668892	43.263770
3523.600752	661029.706545	43.268775
3523.820591	660502.870174	43.273780
3523.687732	659993.533499	43.278785
3523.136294	659480.148690	43.283789
3523.102827	658971.689583	43.288794
3523.145599	658458.947851	43.293799
3523.287686	657957.993052	43.298804
3523.046581	657450.737747	43.303809
3523.028990	656930.986566	43.308813
3522.966077	656427.891207	43.313818
3522.537304	655934.768462	43.318823
3522.957604	655420.554144	43.323828
3522.798359	654934.525265	43.328833
3522.647300	654428.246164	43.333837
3522.940588	653937.995777	43.338842
3522.629120	653437.585950	43.343847
3522.907721	652933.603724	43.348852
3523.173806	652444.332468	43.353857
3523.157059	651940.649638	43.358861
3523.227028	651428.584219	43.363866
3523.010426	650948.013116	43.368871
3523.394501	650429.797862	43.373876
3523.050700	649929.315869	43.378881
3522.794622	649412.056108	43.383885
3522.846703	648916.301972	43.388890
3522.871014	648417.479880	43.393895
3523.212665	647912.182464	43.398900
3523.238597	647418.757019	43.403905
3523.003983	646904.312055	43.408909
3522.712095	646399.446260	43.413914
3522.333935	645901.317177	43.418919
3522.884470	645409.602611	43.423924
3522.691083	644912.192735	43.428929
3522.398092	644419.474183	43.433933
3522.343414	643921.591878	43.438938
3522.119924	643441.011373	43.443943
3522.460697	642936.064065	43.448948
3522.190466	642459.244600	43.453953
3522.044698	641968.531501	43.458957
3522.301329	641480.176130	43.463962
3521.675072	640996.498501	43.468967
3522.206430	640509.299806	43.473972
3521.970344	640027.859965	43.478977
3522.110898	639538.731337	43.483981
3521.793331	639054.809022	43.488986
3521.613831	638564.838287	43.493991
3521.711790	638082.349662	43.498996
3521.507787	637603.991692	43.504001
3521.668591	637124.748826	43.509005
3521.796836	636653.293285	43.514010
3521.268742	636177.926005	43.519015
3521.188857	635708.113780	43.524020
3521.504696	635239.963811	43.529025
3521.393004	634762.409061	43.534029
3521.428858	634299.768307	43.539034
3521.136051	633825.453807	43.544039
3521.401097	633359.679680	43.549044
3521.503343	632891.310235	43.554049
3521.201721	632414.981302	43.559053
3521.256666	631939.120304	43.564058
3521.074583	631487.102334	43.569063
3521.177679	631017.447566	43.574068
3520.788474	630551.159467	43.579073
3520.841114	630097.439763	43.584077
3521.279362	629638.778871	43.589082
3520.720085	629185.174366	43.594087
3521.065377	628710.669427	43.599092
3520.840499	628256.116799	43.604097
3520.588718	627793.588355	43.609101
3520.994460	627329.875962	43.614106
3520.666221	626886.698260	43.619111
3520.724741	626420.802220	43.624116
3520.632530	625964.125664	43.629121
3520.769406	625513.950767	43.634125
3520.694799	625058.734760	43.639130
3520.622034	624614.467275	43.644135
3520.543124	624150.398615	43.649140
3520.364128	623702.555308	43.654145
3520.406191	623249.496301	43.659149
3520.741386	622799.774362	43.664154
3520.661465	622362.427565	43.669159
3520.678390	621910.167968	43.674164
3520.610118	621455.499221	43.679169
3520.374272	620998.284808	43.684173
3520.147920	620556.781528	43.689178
3520.325440	620112.084804	43.694183
3520.834195	619655.838912	43.699188
3520.284693	619212.983141	43.704193
3520.276711	618753.981482	43.709197
3520.406128	618307.916162	43.714202
3519.999009	617867.837699	43.719207
3520.207288	617426.583950	43.724212
3520.028381	617000.865134	43.729217
3519.964788	616546.641528	43.734221
3519.955348	616103.918057	43.739226
3520.034988	615666.875713	43.744231
3520.045711	615221.406439	43.749236
3520.107195	614786.688123	43.754241
3520.205004	614348.286887	43.759245
3520.407161	613912.056232	43.764250
3520.044796	613472.545685	43.769255
3519.711421	613024.439316	43.774260
3519.962695	612596.872129	43.779265
3519.782213	612158.832618	43.784269
3520.090487	611722.096352	43.789274
3519.639146	611281.009732	43.794279
3519.895879	610846.153338	43.799284
3519.855422	610410.528326	43.804289
3519.429407	609974.250011	43.809293
3519.893770	609545.676563	43.814298
3519.648942	609119.113633	43.819303
3519.952010	608681.105584	43.824308
3519.882643	608251.018851	43.829313
3519.783264	607815.052019	43.834317
3519.854132	607381.497150	43.839322
3519.502021	606951.659766	43.844327
3519.345550	606517.157311	43.849332
3519.396570	606090.127876	43.854337
3519.203440	605665.381622	43.859341
3519.719933	605233.373891	43.864346
3519.677172	604808.118252	43.869351
3519.527054	604382.313068	43.874356
3519.236332	603957.268580	43.879361
3519.337138	603529.381501	43.884365
3519.290432	603101.603891	43.889370
3519.254520	602686.253751	43.894375
3519.502960	602245.647196	43.899380
3519.297268	601825.878496	43.904385
3519.265792	601402.501270	43.909389
3519.445336	600976.663239	43.914394
3519.126344	600564.044888	43.919399
3519.312184	600136.518288	43.924404
3519.178212	599720.274289	43.929409
3519.300951	599304.623992	43.934413
3519.294101	598870.758416	43.939418
3519.063139	598452.326644	43.944423
3518.980153	598030.139432	43.949428
3518.794174	597615.836603	43.954433
3519.164047	597189.776087	43.959437
3519.017923	596782.465660	43.964442
3518.806884	596369.177010	43.969447
3518.976963	595949.833369	43.974452
3519.124853	595533.692130	43.979457
3518.791378	595115.559395	43.984461
3519.121902	594702.018787	43.989466
3518.576042	594280.578099	43.994471
3518.986504	593872.167139	43.999476
3518.697014	593466.874846	44.004481
3518.649303	593052.737984	44.009485
3518.541926	592631.866392	44.014490
3518.589473	592229.738652	44.019495
3518.309681	591817.607116	44.024500
3518.388135	591414.441726	44.029505
3518.335847	591004.955516	44.034509
3518.292956	590600.527283	44.039514
3518.291961	590199.996570	44.044519
3518.407681	589792.700465	44.049524
3518.145655	589399.120225	44.054529
3518.576640	588994.606658	44.059533
3518.775619	588587.405826	44.064538
3518.244759	588175.642897	44.069543
3518.483638	587776.346351	44.074548
3518.240198	587371.289986	44.079553
3518.171412	586976.993928	44.084557
3518.228073	586573.165866	44.089562
3518.040973	586184.793721	44.094567
3518.245678	585775.787722	44.099572
3518.202984	585381.535378	44.104577
3517.857228	584981.391367	44.109581
3518.280644	584587.686867	44.114586
3517.853108	584193.712740	44.119591
3518.049210	583790.220020	44.124596
3517.573013	583409.146414	44.129601
3517.532764	583014.464641	44.134605
3517.687466	582619.736762	44.139610
3517.860102	582238.716741	44.144615
3518.265194	581846.937262	44.149620
3518.303010	581449.426484	44.154625
3518.025517	581052.157702	44.159629
3517.727028	580656.287338	44.164634
3517.658136	580276.554530	44.169639
3518.014677	579881.804260	44.174644
3517.618096	579499.488801	44.179649
3517.250013	579101.468324	44.184653
3517.227104	578720.422483	44.189658
3517.066725	578347.182659	44.194663
3517.069738	577969.377770	44.199668
3517.033803	577594.987633	44.204673
3517.100982	577221.674949	44.209677
3517.049071	576846.963168	44.214682
3517.385330	576469.860282	44.219687
3517.332518	576085.720757	44.224692
3517.436675	575708.382912	44.229697
3516.988562	575324.035869	44.234701
3516.999445	574958.511309	44.239706
3516.777174	574585.520970	44.244711
3516.801869	574204.630099	44.249716
3516.694609	573837.583830	44.254721
3516.857201	573479.636365	44.259725
3516.590872	573103.741959	44.264730
3516.388087	572746.037175	44.269735
3516.869792	572374.219146	44.274740
3516.838075	572010.125153	44.279745
3516.676776	571643.527114	44.284749
3516.657245	571276.340756	44.289754
3516.618925	570930.430555	44.294759
3516.439265	570565.162878	44.299764
3516.166605	570212.278947	44.304769
3516.192305	569840.011315	44.309773
3516.493047	569481.725542	44.314778
3516.147709	569136.271695	44.319783
3516.225735	568778.909958	44.324788
3516.760797	568428.606427	44.329793
3516.564847	568072.982754	44.334797
3516.598377	567698.336112	44.339802
3516.423581	567337.152194	44.344807
3516.148480	566977.183165	44.349812
3516.360898	566628.445681	44.354817
3516.148993	566273.781396	44.359821
3516.227338	565919.208770	44.364826
3515.831311	565568.482637	44.369831
3516.103434	565217.582535	44.374836
3515.716968	564871.013866	44.379841
3515.776820	564528.437314	44.384845
3516.097331	564182.383896	44.389850
3515.726476	563838.654391	44.394855
3515.956202	563491.490447	44.399860
3515.997250	563146.665363	44.404865
3516.249161	562790.416523	44.409869
3516.187057	562440.001692	44.414874
3516.059909	562106.707696	44.419879
3516.608606	561744.891376	44.424884
3515.870861	561398.491338	44.429889
3515.515650	561060.174226	44.434893
3515.883523	560723.134866	44.439898
3515.812405	560376.896081	44.444903
3515.651279	560031.972839	44.449908
3515.756894	559695.606505	44.454913
3515.869144	559353.438912	44.459917
3515.980026	559004.514099	44.464922
3515.833194	558674.560785	44.469927
3516.028895	558317.796949	44.474932
3515.779761	557981.296316	44.479937
3515.919507	557637.367056	44.484941
3515.870182	557289.834581	44.489946
3515.593814	556960.918356	44.494951
3515.622824	556616.024462	44.499956
3515.347467	556284.925340	44.504961
3515.412984	555942.929365	44.509965
3515.395899	555602.147717	44.514970
3515.281517	555280.265177	44.519975
3515.355118	554942.373027	44.524980
3515.336281	554611.440425	44.529985
3515.522595	554285.905679	44.534989
3515.639148	553952.263512	44.539994
3515.273479	553618.040399	44.544999
3515.371409	553289.725509	44.550004
3515.550694	552956.199028	44.555009
3515.266623	552620.979867	44.560013
3515.364541	552287.450714	44.565018
3515.270962	551973.950428	44.570023
3515.235436	551629.392618	44.575028
3514.973359	551291.264425	44.580033
3514.835562	550978.706046	44.585037
3515.082809	550649.797511	44.590042
3514.850908	550322.525059	44.595047
3515.111455	550002.568893	44.600052
3514.840200	549687.181370	44.605057
3514.799448	549360.357097	44.610061
3515.142844	549029.981810	44.615066
3514.809705	548728.241014	44.620071
3514.998084	548405.790042	44.625076
3515.179418	548077.989916	44.630081
3514.567005	547769.370380	44.635085
3514.818656	547437.712187	44.640090
3514.529385	547130.988934	44.645095
3514.707417	546804.267883	44.650100
3514.516866	546486.625255	44.655105
3514.695871	546172.491338	44.660109
3514.778391	545861.643486	44.665114
3514.583189	545556.280614	44.670119
3514.313438	545227.834218	44.675124
3514.328931	544925.345437	44.680129
3514.304742	544624.117224	44.685133
3514.610123	544304.575196	44.690138
3514.359682	544003.775481	44.695143
3514.609953	543690.883954	44.700148
3514.279496	543386.403926	44.705153
3514.088212	543074.784032	44.710157
3514.464686	542762.303894	44.715162
3514.154820	542466.523392	44.720167
3514.153353	542162.918539	44.725172
3514.406136	541854.069808	44.730177
3513.916353	541555.880319	44.735181
3514.191641	541248.577643	44.740186
3514.014392	540955.263987	44.745191
3514.050795	540646.929920	44.750196
3513.977446	540352.829500	44.755201
3513.931215	540049.035272	44.760205
3514.281009	539750.815442	44.765210
3513.834971	539456.659093	44.770215
3514.280772	539150.643267	44.775220
3513.725755	538858.107010	44.780225
3513.930413	538562.005232	44.785229
3513.983474	538262.442872	44.790234
3513.555920	537970.370918	44.795239
3513.483822	537667.185696	44.800244
3513.624579	537386.807903	44.805249
3513.507423	537104.804008	44.810253
3513.427859	536815.221516	44.815258
3513.314811	536525.033524	44.820263
3513.604805	536231.088260	44.825268
3513.680055	535946.304543	44.830273
3513.779886	535658.938113	44.835277
3514.004726	535372.805804	44.840282
3513.716407	535087.562608	44.845287
3513.797549	534794.178487	44.850292
3513.550558	534512.044778	44.855297
3513.345928	534220.665384	44.860301
3513.372411	533925.406121	44.865306
3513.372796	533648.107308	44.870311
3513.493492	533362.810563	44.875316
3513.266924	533090.938611	44.880321
3513.438680	532806.429487	44.885325
3513.360017	532511.562963	44.890330
3513.261122	532240.157834	44.895335
3513.328675	531945.456680	44.900340
3513.457482	531675.011335	44.905345
3513.242955	531396.343660	44.910349
3513.375035	531103.935740	44.915354
3513.062649	530837.183571	44.920359
3513.182250	530552.891583	44.925364
3513.194229	530270.782515	44.930369
3513.101797	529995.801794	44.935373
3513.311604	529723.943836	44.940378
3512.823916	529454.016835	44.945383
3512.883096	529171.676661	44.950388
3512.986096	528896.843847	44.955393
3512.681567	528627.677927	44.960397
3512.823779	528357.522285	44.965402
3512.742782	528088.762608	44.970407
3512.799711	527826.182942	44.975412
3512.761336	527559.223452	44.980417
3512.618111	527295.154235	44.985421
3512.679407	527022.363170	44.990426
3512.354642	526763.262301	44.995431
3512.722763	526491.216734	45.000436
3512.863178	526226.726687	45.005441
3512.381765	525958.097646	45.010445
3512.665282	525695.542497	45.015450
3512.488410	525431.445855	45.020455
3512.411689	525174.849591	45.025460
3512.277730	524916.037339	45.030465
3512.315413	524657.443724	45.035469
3512.487256	524402.558758	45.040474
3512.419805	524142.055679	45.045479
3512.628949	523878.067614	45.050484
3512.590944	523622.649830	45.055489
3512.332179	523373.425215	45.060493
3512.473891	523109.586617	45.065498
3512.114391	522845.576506	45.070503
3512.174518	522591.235262	45.075508
3512.210452	522339.216572	45.080513
3512.397543	522091.964855	45.085517
3512.458527	521823.573002	45.090522
3512.035211	521577.780468	45.095527
3512.371064	521319.633993	45.100532
3512.339554	521061.899330	45.105537
3511.940911	520806.192426	45.110541
3511.867046	520558.354223	45.115546
3512.133731	520318.028915	45.120551
3512.022732	520063.674410	45.125556
3512.485167	519809.924776	45.130561
3512.032801	519565.973197	45.135565
3512.827440	519305.239523	45.140570
3512.333122	519062.398138	45.145575
3512.266609	518804.075654	45.150580
3512.229453	518545.743795	45.155585
3511.738087	518295.818826	45.160589
3512.079743	518046.858726	45.165594
3512.062593	517804.319968	45.170599
3512.162051	517552.514198	45.175604
3512.139338	517299.765462	45.180609
3511.698873	517056.428498	45.185613
3511.958547	516800.239085	45.190618
3511.566224	516579.111698	45.195623
3511.606059	516334.266963	45.200628
3511.874739	516089.934933	45.205633
3511.875057	515848.069597	45.210637
3511.931746	515604.826921	45.215642
3511.640552	515374.673170	45.220647
3511.637191	515121.380307	45.225652
3511.523387	514883.055629	45.230657
3511.382517	514647.156836	45.235661
3511.854780	514411.857056	45.240666
3511.783368	514173.716347	45.245671
3511.588956	513934.582567	45.250676
3511.783610	513698.106894	45.255681
3511.607564	513453.708290	45.260685
3511.444696	513211.577185	45.265690
3511.405431	512987.509033	45.270695
3511.859597	512758.048267	45.275700
3511.718672	512514.386872	45.280705
3511.450538	512284.941456	45.285709
3511.845256	512038.958042	45.290714
3511.572297	511809.304390	45.295719
3511.306203	511566.306524	45.300724
3511.594510	511336.701730	45.305729
3511.399048	511104.397007	45.310733
3511.183321	510876.640144	45.315738
3511.307804	510648.063926	45.320743
3511.504033	510411.487966	45.325748
3511.675196	510180.521976	45.330753
3511.317076	509944.539022	45.335757
3511.948830	509713.133837	45.340762
3511.625147	509487.750564	45.345767
3511.284839	509244.072705	45.350772
3511.369041	509016.692714	45.355777
3511.344189	508783.869989	45.360781
3511.348370	508547.602266	45.365786
3511.224860	508330.204073	45.370791
3511.254716	508097.867380	45.375796
3511.320615	507866.178186	45.380801
3511.240933	507640.575488	45.385805
3511.429947	507411.335223	45.390810
3511.141833	507197.133890	45.395815
3510.994168	506957.482204	45.400820
3511.334844	506738.770077	45.405825
3511.129966	506512.566343	45.410829
3511.174668	506274.084698	45.415834
3511.287053	506063.186433	45.420839
3511.194922	505832.253048	45.425844
3511.019089	505606.183257	45.430849
3510.891893	505387.835951	45.435853
3511.064670	505159.981732	45.440858
3510.991209	504949.151187	45.445863
3511.000496	504727.384798	45.450868
3510.698817	504496.468095	45.455873
3510.664153	504287.998238	45.460877
3510.911630	504060.419108	45.465882
3510.650789	503852.639463	45.470887
3510.750392	503637.566372	45.475892
3510.680568	503425.805431	45.480897
3510.591763	503206.512205	45.485901
3511.027726	502988.592559	45.490906
3510.674641	502780.966654	45.495911
3510.268084	502558.887791	45.500916
3510.749196	502354.299153	45.505921
3510.506032	502157.668233	45.510925
3510.230803	501938.996523	45.515930
3510.112904	501741.226905	45.520935
3510.030325	501531.465990	45.525940
3510.233054	501322.968275	45.530945
3509.938849	501131.743827	45.535949
3510.161845	500929.810713	45.540954
3509.932881	500720.822881	45.545959
3510.296139	500515.624695	45.550964
3510.565542	500317.923517	45.555969
3510.202154	500116.434508	45.560973
3510.594271	499915.572526	45.565978
3510.184566	499714.946142	45.570983
3510.059871	499500.666161	45.575988
3510.395706	499306.936335	45.580993
3509.937705	499109.193201	45.585997
3509.976053	498900.288404	45.591002
3510.025770	498711.758491	45.596007
3509.708920	498518.232036	45.601012
3509.920059	498323.146631	45.606017
3509.996440	498125.603964	45.611021
3510.478310	497926.725427	45.616026
3510.210877	497740.716676	45.621031
3510.161421	497539.951927	45.626036
3509.931912	497339.316653	45.631041
3509.841014	497141.184007	45.636045
3509.719910	496936.833481	45.641050
3509.634336	496750.580354	45.646055
3509.861307	496556.027927	45.651060
3509.729927	496380.652317	45.656065
3509.512659	496190.571646	45.661069
3509.316070	495993.353857	45.666074
3509.339211	495815.012456	45.671079
3509.815871	495632.848909	45.676084
3509.774606	495430.793030	45.681089
3509.909681	495255.157866	45.686093
3510.045546	495059.035700	45.691098
3509.859147	494878.747530	45.696103
3509.092395	494681.611731	45.701108
3509.503005	494495.552407	45.706113
3509.110434	494313.775949	45.711117
3509.726152	494131.471297	45.716122
3509.429664	493951.242618	45.721127
3509.235448	493777.570508	45.726132
3509.391534	493588.408461	45.731137
3508.885761	493418.276218	45.736141
3509.171464	493243.606168	45.741146
3509.364711	493075.627503	45.746151
3509.168869	492890.362336	45.751156
3509.273813	492710.355472	45.756161
3508.913445	492524.912073	45.761165
3509.403397	492349.085044	45.766170
3509.038266	492185.897676	45.771175
3509.073211	492001.443460	45.776180
3509.296269	491827.528447	45.781185
3508.804619	491658.236253	45.786189
3509.278115	491476.281613	45.791194
3509.244696	491315.305898	45.796199
3509.203663	491140.366580	45.801204
3508.925080	490964.403596	45.806209
3509.156763	490802.922479	45.811213
3509.288418	490613.832857	45.816218
3508.992975	490450.009937	45.821223
3508.796631	490275.644871	45.826228
3509.061267	490106.410623	45.831233
3508.916437	489944.884556	45.836237
3509.233115	489776.245330	45.841242
3508.808429	489603.582125	45.846247
3508.921548	489431.786711	45.851252
3508.761804	489268.991943	45.856257
3508.680952	489105.018419	45.861261
3508.813719	488936.149414	45.866266
3508.956699	488775.018662	45.871271
3508.631238	488611.891820	45.876276
3508.641851	488449.920460	45.881281
3508.663471	488283.695278	45.886285
3508.972451	488112.005147	45.891290
3508.697380	487960.805392	45.896295
3508.710588	487781.825311	45.901300
3508.631726	487620.721738	45.906305
3508.115554	487461.462442	45.911309
3508.370497	487308.547241	45.916314
3508.618290	487150.116121	45.921319
3508.692570	486993.686753	45.926324
3509.032183	486830.834503	45.931329
3508.748549	486668.745019	45.936333
3508.726663	486504.686331	45.941338
3508.681381	486358.747048	45.946343
3508.404799	486185.974029	45.951348
3508.625970	486036.494723	45.956353
3508.411668	485886.076352	45.961357
3508.730619	485723.470383	45.966362
3508.503473	485576.492885	45.971367
3508.436146	485411.318358	45.976372
3508.246787	485259.726370	45.981377
3508.828084	485119.742908	45.986381
3508.672699	484957.868784	45.991386
3508.766845	484801.416498	45.996391
3509.070647	484642.801371	46.001396
3508.818048	484466.059725	46.006401
3508.670005	484316.274588	46.011405
3508.851696	484149.780441	46.016410
3508.682812	483990.379763	46.021415
3508.602984	483828.128104	46.026420
3508.817824	483674.833883	46.031425
3508.375741	483522.662786	46.036429
3508.944842	483362.573704	46.041434
3508.538860	483203.763202	46.046439
3508.273464	483049.685129	46.051444
3508.206700	482893.142244	46.056449
3508.355963	482742.432591	46.061453
3508.389804	482592.348772	46.066458
3508.541031	482449.127583	46.071463
3508.104420	482300.437681	46.076468
3508.127657	482146.150661	46.081473
3507.877786	482000.919023	46.086477
3508.430867	481850.385982	46.091482
3508.067267	481697.983424	46.096487
3508.006623	481552.766457	46.101492
3507.983964	481406.883766	46.106497
3507.736389	481277.135609	46.111501
3508.194680	481120.487546	46.116506
3507.948864	480983.498173	46.121511
3508.073368	480837.281997	46.126516
3508.137750	480698.465726	46.131521
3508.042685	480548.842392	46.136525
3508.194083	480398.821371	46.141530
3508.388062	480260.131461	46.146535
3508.296648	480119.363017	46.151540
3508.194601	479968.875455	46.156545
3507.712346	479831.158320	46.161549
3507.974270	479688.908700	46.166554
3507.705341	479547.710483	46.171559
3507.744802	479407.420395	46.176564
3507.856358	479271.015121	46.181569
3507.646655	479130.967939	46.186573
3507.821085	478992.474145	46.191578
3507.633522	478869.229278	46.196583
3507.760849	478733.121026	46.201588
3507.926013	478591.993122	46.206593
3507.625493	478452.563744	46.211597
3507.603813	478318.604221	46.216602
3507.872729	478188.644424	46.221607
3507.788203	478054.440540	46.226612
3507.875453	477905.169260	46.231617
3508.053303	477771.627312	46.236621
3507.920722	477633.732524	46.241626
3508.074111	477506.521645	46.246631
3507.551836	477360.792892	46.251636
3507.563831	477225.503167	46.256641
3507.290814	477092.792715	46.261645
3507.337666	476969.748126	46.266650
3507.406881	476838.648268	46.271655
3507.341913	476705.545053	46.276660
3507.090203	476586.650160	46.281665
3506.932064	476468.194224	46.286669
3507.421909	476331.398555	46.291674
3506.964456	476214.308577	46.296679
3506.891727	476087.734064	46.301684
3507.477915	475970.717512	46.306689
3507.094970	475848.295775	46.311693
3507.427195	475721.143240	46.316698
3507.493407	475609.631222	46.321703
3507.363559	475483.619305	46.326708
3507.205973	475350.268903	46.331713
3506.807606	475236.504650	46.336717
3507.338250	475101.313269	46.341722
3507.253095	474989.316968	46.346727
3507.313645	474878.864896	46.351732
3507.283342	474746.855634	46.356737
3507.338024	474631.237945	46.361741
3507.400411	474500.021318	46.366746
3507.358985	474383.557623	46.371751
3507.131129	474252.388800	46.376756
3507.334360	474129.754297	46.381761
3507.134562	474020.151800	46.386765
3507.220330	473883.913398	46.391770
3507.035237	473767.723571	46.396775
3506.890435	473661.755741	46.401780
3507.255713	473546.635314	46.406785
3506.760784	473439.257382	46.411789
3507.095398	473321.558046	46.416794
3507.066141	473202.350169	46.421799
3507.031241	473083.193135	46.426804
3507.191826	472969.268883	46.431809
3506.801430	472857.818270	46.436813
3507.125778	472731.153010	46.441818
3507.002149	472620.567025	46.446823
3506.916361	472504.301714	46.451828
3507.132371	472394.669295	46.456833
3506.820037	472281.328046	46.461837
3507.065517	472163.332756	46.466842
3506.737748	472049.840803	46.471847
3507.166410	471930.546621	46.476852
3506.821879	471816.296419	46.481857
3506.445682	471723.221323	46.486861
3507.371160	471605.055766	46.491866
3506.849353	471493.619462	46.496871
3507.207745	471386.641152	46.501876
3507.337046	471251.135831	46.506881
3507.035319	471135.456029	46.511885
3506.777706	471028.783457	46.516890
3506.483610	470921.812616	46.521895
3506.708120	470809.434439	46.526900
3506.839764	470699.148084	46.531905
3506.811406	470607.021059	46.536909
3506.822852	470483.027847	46.541914
3506.966071	470379.068916	46.546919
3506.407734	470268.391349	46.551924
3506.530989	470160.028004	46.556929
3506.517626	470063.489125	46.561933
3506.602945	469953.105019	46.566938
3506.493969	469849.743405	46.571943
3506.231321	469745.799640	46.576948
3506.241384	469637.959154	46.581953
3506.253107	469548.200789	46.586957
3506.483685	469441.993075	46.591962
3506.301324	469349.784914	46.596967
3506.229701	469253.251852	46.601972
3506.489636	469155.851227	46.606977
3506.594388	469057.868752	46.611981
3506.615496	468949.313310	46.616986
3506.440185	468858.519880	46.621991
3506.570033	468757.492300	46.626996
3506.460276	468652.047449	46.632001
3506.404144	468555.254922	46.637005
3506.436210	468453.634561	46.642010
3506.539349	468367.248936	46.647015
3506.299800	468255.441414	46.652020
3506.495400	468154.500722	46.657025
3506.321344	468065.729554	46.662029
3506.321794	467966.898113	46.667034
3506.751401	467867.739599	46.672039
3506.340077	467761.530800	46.677044
3506.489991	467661.811085	46.682049
3506.190549	467565.561659	46.687053
3506.275272	467460.330307	46.692058
3506.408844	467369.679683	46.697063
3506.502785	467266.826642	46.702068
3506.823420	467171.279899	46.707073
3506.405426	467075.504184	46.712077
3506.789274	466968.851259	46.717082
3506.444316	466873.568660	46.722087
3506.754118	466773.513065	46.727092
3506.665299	466675.247464	46.732097
3506.793268	466565.950997	46.737101
3506.475414	466464.582468	46.742106
3506.317511	466366.377744	46.747111
3506.262971	466264.557912	46.752116
3506.616005	466166.670221	46.757121
3505.917389	466068.151007	46.762125
3506.286908	465969.803544	46.767130
3506.196341	465876.803031	46.772135
3506.008090	465797.446998	46.777140
3506.306514	465702.859348	46.782145
3506.085273	465618.239273	46.787149
3506.444055	465519.486046	46.792154
3506.080490	465432.457617	46.797159
3505.879333	465338.004147	46.802164
3505.964444	465243.298681	46.807169
3505.824232	465160.790658	46.812173
3506.047476	465063.730170	46.817178
3505.713209	464987.232957	46.822183
3505.727413	464905.812106	46.827188
3506.086935	464808.879069	46.832193
3505.958605	464723.732565	46.837197
3505.807513	464632.864354	46.842202
3505.929888	464549.042250	46.847207
3505.702917	464466.242090	46.852212
3506.088663	464390.379575	46.857217
3505.986601	464310.546735	46.862221
3506.034340	464214.930633	46.867226
3505.839628	464134.251554	46.872231
3505.855035	464048.064207	46.877236
3506.093914	463958.696942	46.882241
3505.848678	463881.014818	46.887245
3505.873151	463787.629966	46.892250
3505.740238	463717.274851	46.897255
3505.484679	463629.409205	46.902260
3505.726651	463542.218238	46.907265
3505.672084	463462.019131	46.912269
3506.170819	463372.858157	46.917274
3505.764370	463299.812118	46.922279
3505.645309	463217.950940	46.927284
3506.011448	463129.622206	46.932289
3505.862635	463059.166095	46.937293
3505.873299	462972.974811	46.942298
3505.447636	462888.833787	46.947303
3505.863166	462808.703743	46.952308
3505.944149	462734.964322	46.957313
3505.891674	462658.460517	46.962317
3505.879788	462564.265297	46.967322
3505.688898	462487.277748	46.972327
3505.311441	462406.268036	46.977332
3505.449670	462326.538072	46.982337
3505.390306	462260.472249	46.987341
3505.570590	462178.808976	46.992346
3505.504212	462114.872087	46.997351
3505.441705	462033.300337	47.002356
3505.542910	461958.997152	47.007361
3505.342547	461878.056368	47.012365
3505.571305	461795.521789	47.017370
3505.358090	461732.419497	47.022375
3505.448245	461667.339616	47.027380
3505.653274	461583.490694	47.032385
3505.406414	461517.099674	47.037389
3505.519288	461439.498743	47.042394
3505.459376	461367.399817	47.047399
3505.506447	461294.370222	47.052404
3505.502606	461218.713976	47.057409
3505.267718	461148.569758	47.062413
3505.460851	461067.051708	47.067418
3505.275664	461009.212504	47.072423
3505.482242	460931.188177	47.077428
3505.392334	460859.751297	47.082433
3505.535840	460787.716872	47.087437
3505.545917	460704.049532	47.092442
3505.587466	460637.099550	47.097447
3505.530397	460574.422979	47.102452
3505.319664	460490.234999	47.107457
3504.991190	460424.259653	47.112461
3505.339150	460354.317158	47.117466
3505.374893	460283.414188	47.122471
3505.412935	460224.064944	47.127476
3505.140298	460158.484596	47.132481
3505.099713	460098.945694	47.137485
3505.091194	460020.245025	47.142490
3505.007154	459964.108535	47.147495
3505.423639	459892.987128	47.152500
3505.331906	459825.296996	47.157505
3505.522016	459764.704141	47.162509
3505.259962	459684.068980	47.167514
3505.278277	459619.957528	47.172519
3505.398141	459556.284638	47.177524
3505.459500	459478.279396	47.182529
3505.049516	459424.984381	47.187533
3505.325352	459352.516724	47.192538
3505.457037	459298.064617	47.197543
3505.101729	459215.213586	47.202548
3505.358663	459138.694009	47.207553
3504.980422	459084.379067	47.212557
3505.103118	459015.433250	47.217562
3505.069098	458954.774843	47.222567
3505.056043	458900.599766	47.227572
3505.173792	458838.496040	47.232577
3505.067129	458772.832106	47.237581
3505.122121	458707.089673	47.242586
3504.950341	458654.765545	47.247591
3505.061512	458590.533567	47.252596
3505.636746	458523.079901	47.257601
3504.747510	458463.985109	47.262605
3505.045571	458401.646513	47.267610
3505.073781	458337.579934	47.272615
3504.852629	458277.356880	47.277620
3504.851155	458214.460662	47.282625
3505.093906	458159.428987	47.287629
3504.927815	458091.948403	47.292634
3504.877077	458035.699439	47.297639
3504.927099	457974.871664	47.302644
3505.339227	457899.233142	47.307649
3504.816836	457850.514585	47.312653
3505.208778	457788.462153	47.317658
3505.361800	457723.257271	47.322663
3505.170789	457666.727124	47.327668
3504.780346	457604.098144	47.332673
3504.729398	457556.666836	47.337677
3505.103472	457483.111283	47.342682
3504.716836	457448.712139	47.347687
3504.851109	457378.897089	47.352692
3505.099568	457311.292416	47.357697
3505.058328	457271.055966	47.362701
3504.877768	457206.210474	47.367706
3504.618432	457157.749429	47.372711
3505.006040	457096.050397	47.377716
3505.189291	457037.021698	47.382721
3504.767666	456989.601661	47.387725
3505.092720	456920.360671	47.392730
3505.135713	456874.432279	47.397735
3505.230387	456810.349487	47.402740
3505.384279	456747.422155	47.407745
3505.389229	456681.985758	47.412749
3504.985691	456622.853297	47.417754
3505.115723	456558.155434	47.422759
3505.044404	456502.361878	47.427764
3505.018266	456443.164450	47.432769
3504.914702	456392.748878	47.437773
3504.983714	456328.973063	47.442778
3504.777452	456275.939016	47.447783
3504.782480	456214.961553	47.452788
3505.105328	456152.003520	47.457793
3504.854459	456103.791936	47.462797
3504.983891	456042.944776	47.467802
3505.132260	455989.038424	47.472807
3505.073430	455938.512707	47.477812
3505.115855	455883.965223	47.482817
3505.013125	455832.939859	47.487821
3505.164711	455753.890998	47.492826
3505.506176	455695.743763	47.497831
3504.737033	455632.210245	47.502836
3505.248216	455574.185750	47.507841
3504.723982	455520.747821	47.512845
3504.870942	455466.688256	47.517850
3504.918705	455410.263093	47.522855
3504.849614	455357.304600	47.527860
3504.922958	455300.367871	47.532865
3504.695764	455261.071587	47.537869
3504.936533	455201.520825	47.542874
3504.848781	455155.915003	47.547879
3504.722601	455091.712421	47.552884
3504.665565	455038.142760	47.557889
3504.743883	454988.706447	47.562893
3504.851155	454934.956388	47.567898
3505.083639	454882.401381	47.572903
3504.949983	454829.199086	47.577908
3505.019464	454774.846771	47.582913
3504.752966	454719.588551	47.587917
3505.049599	454658.100410	47.592922
3505.171287	454609.314757	47.597927
3504.873658	454549.245727	47.602932
3504.668509	454503.354342	47.607937
3504.775740	454464.050110	47.612941
3504.922140	454402.992385	47.617946
3504.737078	454350.203154	47.622951
3505.217759	454287.719328	47.627956
3505.022458	454240.963908	47.632961
3505.032951	454195.896778	47.637965
3505.268669	454127.979532	47.642970
3505.068960	454064.039735	47.647975
3504.838718	454011.054572	47.652980
3504.799965	453956.262327	47.657985
3504.647001	453907.471204	47.662989
3504.796317	453850.821619	47.667994
3504.994059	453808.408397	47.672999
3504.697179	453761.263680	47.678004
3504.488024	453704.117272	47.683009
3504.852246	453661.827401	47.688013
3504.906418	453596.017826	47.693018
3505.199443	453558.302332	47.698023
3504.748452	453497.850851	47.703028
3504.876787	453444.549528	47.708033
3504.596541	453394.106012	47.713037
3504.377116	453329.964515	47.718042
3504.291699	453298.802039	47.723047
3504.233785	453245.582696	47.728052
3504.499398	453199.709397	47.733057
3504.555109	453163.605234	47.738061
3504.738707	453112.220015	47.743066
3504.560104	453081.681460	47.748071
3504.673955	453033.653821	47.753076
3504.711908	452984.574430	47.758081
3504.293143	452938.716016	47.763085
3504.364746	452891.607775	47.768090
3504.361426	452841.318400	47.773095
3504.263777	452800.575794	47.778100
3504.530883	452764.536228	47.783105
3504.371920	452723.854636	47.788109
3504.224973	452680.331939	47.793114
3504.762362	452632.281743	47.798119
3504.615125	452599.658578	47.803124
3504.756587	452537.582230	47.808129
3504.500032	452502.239975	47.813133
3504.682339	452440.714022	47.818138
3504.594407	452405.190720	47.823143
3504.485402	452358.771158	47.828148
3504.562428	452312.928089	47.833153
3504.205048	452282.266784	47.838157
3504.560482	452238.251798	47.843162
3504.591031	452195.813107	47.848167
3504.445422	452147.320736	47.853172
3504.305420	452108.966769	47.858177
3504.534091	452059.244245	47.863181
3504.479055	452017.681659	47.868186
3504.217274	451969.664986	47.873191
3504.088899	451932.981731	47.878196
3504.303869	451897.152347	47.883201
3503.748216	451858.970283	47.888205
3504.346308	451813.087834	47.893210
3504.283996	451791.703863	47.898215
3504.631721	451745.965412	47.903220
3504.538433	451703.191968	47.908225
3504.629799	451660.792494	47.913229
3504.648767	451617.594118	47.918234
3504.625841	451571.512982	47.923239
3504.669392	451537.486700	47.928244
3504.857419	451486.907865	47.933249
3504.191927	451453.661599	47.938253
3504.186574	451405.143542	47.943258
3504.107865	451367.741018	47.948263
3504.116758	451340.463320	47.953268
3504.328731	451297.079224	47.958273
3504.219624	451260.949182	47.963277
3504.261324	451216.326506	47.968282
3504.209861	451174.254624	47.973287
3503.848609	451148.155266	47.978292
3504.290301	451114.009609	47.983297
3504.100200	451077.031181	47.988301
3504.080828	451030.796138	47.993306
3504.421550	451003.512038	47.998311
3504.032807	450959.570709	48.003316
3504.037869	450922.406582	48.008321
3503.998318	450900.206602	48.013325
3504.231469	450863.307625	48.018330
3504.129787	450823.119522	48.023335
3503.883439	450791.930047	48.028340
3504.419967	450755.638186	48.033345
3504.058100	450711.184736	48.038349
3504.239175	450685.194998	48.043354
3504.240713	450658.272567	48.048359
3504.669727	450614.241579	48.053364
3504.511449	450573.504947	48.058369
3504.680499	450533.371461	48.063373
3504.764932	450493.303047	48.068378
3504.810828	450446.244342	48.073383
3504.697461	450403.167444	48.078388
3504.680218	450346.840916	48.083393
3504.347778	450312.065604	48.088397
3504.401620	450250.352292	48.093402
3504.583753	450228.316553	48.098407
3504.266678	450191.510339	48.103412
3504.510292	450147.256514	48.108417
3504.269364	450114.391928	48.113421
3504.354528	450077.466129	48.118426
3504.432244	450042.671038	48.123431
3504.057816	449997.964700	48.128436
3504.155985	449962.253337	48.133441
3504.030448	449935.655887	48.138445
3504.134210	449890.816968	48.143450
3503.941313	449874.422195	48.148455
3503.936154	449855.358805	48.153460
3503.918594	449805.723647	48.158465
3504.010831	449774.424135	48.163469
3503.780799	449746.627414	48.168474
3504.409981	449715.743162	48.173479
3504.117912	449683.545773	48.178484
3504.191354	449634.959441	48.183489
3503.828233	449617.579464	48.188493
3504.180949	449578.984593	48.193498
3504.267877	449544.288507	48.198503
3504.127971	449513.636686	48.203508
3504.027812	449480.949884	48.208513
3503.363943	449446.888871	48.213517
3503.730352	449420.561695	48.218522
3504.020777	449397.238994	48.223527
3503.726109	449376.500667	48.228532
3503.745033	449351.348225	48.233537
3503.322496	449314.811996	48.238541
3503.517683	449278.880086	48.243546
3503.668897	449262.172556	48.248551
3503.543116	449237.906659	48.253556
3504.032010	449210.037175	48.258561
3504.141856	449204.035290	48.263565
3504.120943	449176.151401	48.268570
3504.333170	449132.052906	48.273575
3503.624773	449106.618723	48.278580
3503.809222	449082.705313	48.283585
3504.000715	449048.446896	48.288589
3503.731664	449008.182474	48.293594
3503.720105	448984.758765	48.298599
3503.813797	448966.945313	48.303604
3504.308337	448941.964695	48.308609
3503.976750	448909.823570	48.313613
3503.846204	448876.431143	48.318618
3504.452348	448854.625794	48.323623
3504.161334	448824.100178	48.328628
3504.030582	448782.848309	48.333633
3504.098806	448763.416459	48.338637
3504.214908	448729.626746	48.343642
3504.150629	448685.726647	48.348647
3504.032740	448666.174369	48.353652
3504.197935	448630.246474	48.358657
3503.947742	448592.462620	48.363661
3503.828155	448564.696181	48.368666
3504.057433	448538.239200	48.373671
3504.134119	448516.118258	48.378676
3504.196062	448476.455481	48.383681
3504.467424	448451.613803	48.388685
3504.096980	448404.469489	48.393690
3504.026742	448379.077578	48.398695
3503.563732	448362.677038	48.403700
3503.813754	448336.824740	48.408705
3503.677811	448316.514623	48.413709
3503.600169	448267.038210	48.418714
3503.540650	448245.345895	48.423719
3503.305520	448230.833197	48.428724
3503.560684	448205.689756	48.433729
3503.756764	448185.728475	48.438733
3503.844128	448168.676032	48.443738
3503.679045	448147.407296	48.448743
3503.891222	448124.958568	48.453748
3503.978556	448088.992339	48.458753
3503.535988	448064.829888	48.463757
3503.610443	448047.069651	48.468762
3503.448635	448033.913393	48.473767
3503.555654	448016.502521	48.478772
3503.597009	447996.263236	48.483777
3503.171074	447984.166193	48.488781
3503.664890	447960.604347	48.493786
3503.458837	447928.186751	48.498791
3503.321478	447911.983792	48.503796
3503.334823	447884.498005	48.508801
3503.427140	447872.363115	48.513805
3503.603563	447853.419029	48.518810
3503.776670	447830.672414	48.523815
3503.393443	447821.204786	48.528820
3503.444522	447807.809206	48.533825
3503.271705	447804.796239	48.538829
3503.355934	447775.168479	48.543834
3503.490264	447762.468566	48.548839
3503.440406	447755.885043	48.553844
3503.576593	447728.276663	48.558849
3503.415559	447713.294586	48.563853
3503.550268	447698.059168	48.568858
3503.768913	447673.326995	48.573863
3503.812648	447640.004269	48.578868
3503.502570	447605.677030	48.583873
3503.431088	447601.784690	48.588877
3503.305424	447574.727902	48.593882
3503.273971	447568.698971	48.598887
3503.330867	447550.738483	48.603892
3503.491922	447534.484282	48.608897
3503.300849	447525.135836	48.613901
3503.309869	447508.451198	48.618906
3503.337879	447494.704400	48.623911
3503.237512	447488.484378	48.628916
3503.596537	447467.784679	48.633921
3503.380107	447454.688096	48.638925
3503.409699	447433.638944	48.643930
3503.406274	447425.678256	48.648935
3503.118668	447410.261198	48.653940
3503.428587	447394.336432	48.658945
3503.207332	447386.260798	48.663949
3503.483714	447375.057661	48.668954
3503.457595	447361.928525	48.673959
3503.316885	447345.573578	48.678964
3503.366526	447324.875857	48.683969
3503.280208	447323.521446	48.688973
3503.100149	447306.311136	48.693978
3503.687464	447297.336771	48.698983
3503.452574	447287.691448	48.703988
3503.332819	447266.718340	48.708993
3503.404143	447256.970009	48.713997
3503.501787	447241.994138	48.719002
3503.502202	447217.755079	48.724007
3503.719682	447184.655516	48.729012
3503.944882	447157.183322	48.734017
3503.893649	447153.338151	48.739021
3503.904330	447121.389407	48.744026
3503.306856	447103.438854	48.749031
3503.243416	447094.879776	48.754036
3503.477697	447082.415937	48.759041
3503.230510	447063.289930	48.764045
3503.385235	447057.279773	48.769050
3503.428696	447031.562573	48.774055
3503.671982	447014.279740	48.779060
3503.607933	446986.704585	48.784065
3503.481804	446978.004036	48.789069
3503.580504	446958.159647	48.794074
3503.637951	446942.632621	48.799079
3503.194008	446933.631350	48.804084
3503.134316	446910.568530	48.809089
3503.255414	446904.513363	48.814093
3503.401696	446891.354498	48.819098
3503.915013	446886.297264	48.824103
3503.704396	446869.294657	48.829108
3503.367461	446857.029640	48.834113
3503.253295	446840.010540	48.839117
3503.587885	446835.085232	48.844122
3503.338022	446807.592282	48.849127
3503.127853	446790.893796	48.854132
3503.426507	446776.998901	48.859137
3503.337714	446769.914618	48.864141
3503.214350	446741.335067	48.869146
3503.430023	446738.103482	48.874151
3503.518617	446724.092289	48.879156
3503.537227	446699.088875	48.884161
3503.497145	446701.884784	48.889165
3503.384280	446677.664451	48.894170
3503.722719	446669.847950	48.899175
3503.476520	446658.378693	48.904180
3503.659777	446637.251804	48.909185
3503.330716	446635.938797	48.914189
3503.386686	446620.361078	48.919194
3503.420268	446601.440267	48.924199
3503.359426	446597.444504	48.929204
3503.727530	446585.870317	48.934209
3503.625582	446574.528516	48.939213
3503.330288	446544.608868	48.944218
3503.489786	446515.676452	48.949223
3503.410050	446497.484849	48.954228
3503.129439	446480.950280	48.959233
3503.289659	446480.669360	48.964237
3503.301210	446462.766406	48.969242
3503.425800	446449.458840	48.974247
3502.983298	446438.276538	48.979252
3503.523586	446417.849135	48.984257
3503.318274	446414.385117	48.989261
3503.613962	446396.484303	48.994266
3503.751149	446386.318638	48.999271
3503.505130	446378.500403	49.004276
3503.252172	446364.851561	49.009281
3503.024192	446357.486639	49.014285
3502.947220	446334.781125	49.019290
3503.241530	446329.101908	49.024295
3503.283602	446311.700730	49.029300
3503.419711	446304.476468	49.034305
3503.039984	446295.920363	49.039309
3503.095833	446290.332565	49.044314
3503.549632	446281.634131	49.049319
3503.035554	446274.622300	49.054324
3503.616016	446258.701203	49.059329
3503.259523	446253.843051	49.064333
3503.613075	446235.222261	49.069338
3503.452599	446230.837750	49.074343
3503.043761	446218.990334	49.079348
3503.190950	446197.919880	49.084353
3503.416251	446194.483723	49.089357
3503.343777	446193.076164	49.094362
3503.619065	446184.509594	49.099367
3503.460486	446176.270662	49.104372
3503.613084	446158.444793	49.109377
3503.329398	446148.857995	49.114381
3503.160480	446137.324550	49.119386
3503.265610	446128.330606	49.124391
3502.908852	446117.336341	49.129396
3503.553423	446096.789402	49.134401
3503.236711	446098.669099	49.139405
3503.199688	446085.388901	49.144410
3503.387347	446072.628162	49.149415
3503.273290	446062.961650	49.154420
3503.424748	446050.460639	49.159425
3503.113072	446047.978250	49.164429
3503.466038	446042.339654	49.169434
3503.531845	446027.875487	49.174439
3503.538402	446018.847616	49.179444
3503.304895	445996.320606	49.184449
3503.304389	445997.994183	49.189453
3502.976946	445986.386300	49.194458
3503.357984	445976.787348	49.199463
3503.281454	445973.351981	49.204468
3503.639043	445957.113731	49.209473
3503.681188	445956.599404	49.214477
3503.390120	445940.218338	49.219482
3503.378775	445932.816279	49.224487
3503.087241	445931.851805	49.229492
3503.152180	445909.223031	49.234497
3502.971400	445905.856165	49.239501
3503.015325	445892.511314	49.244506
3503.472723	445880.972212	49.249511
3503.412473	445878.041173	49.254516
3503.385744	445864.201244	49.259521
3503.418219	445856.436689	49.264525
3503.573130	445849.817613	49.269530
3503.675887	445840.823954	49.274535
3503.255011	445832.832525	49.279540
3503.546213	445815.844816	49.284545
3503.722445	445810.591326	49.289549
3503.447368	445780.768578	49.294554
3503.805603	445758.647404	49.299559
3503.028710	445750.057469	49.304564
3503.506068	445724.619595	49.309569
3503.403200	445720.884408	49.314573
3503.449628	445705.054087	49.319578
3503.543836	445696.264678	49.324583
3503.112419	445691.824892	49.329588
3503.418268	445679.449441	49.334593
3503.412247	445675.748422	49.339597
3503.286513	445664.815902	49.344602
3503.400833	445659.877223	49.349607
3503.416761	445654.955343	49.354612
3503.427582	445633.907619	49.359617
3503.147627	445640.243819	49.364621
3503.310784	445625.052775	49.369626
3503.348568	445617.743645	49.374631
3503.072237	445604.859001	49.379636
3503.324440	445589.754154	49.384641
3503.342449	445592.793855	49.389645
3503.251253	445579.218314	49.394650
3503.527780	445574.657624	49.399655
3503.234299	445562.587292	49.404660
3503.410335	445547.495421	49.409665
3503.163414	445543.987653	49.414669
3502.902296	445535.512415	49.419674
3503.022868	445528.290544	49.424679
3503.125952	445520.108106	49.429684
3503.391919	445498.205271	49.434689
3503.113418	445502.664871	49.439693
3502.958555	445485.854493	49.444698
3503.013686	445481.027306	49.449703
3502.984074	445487.574371	49.454708
3502.980234	445488.741424	49.459713
3503.346225	445495.728072	49.464717
3503.359199	445487.763860	49.469722
3503.054280	445482.237452	49.474727
3502.912893	445480.638759	49.479732
3503.013387	445463.632621	49.484737
3502.933966	445457.712709	49.489741
3502.936821	445448.735944	49.494746
3503.074225	445450.335303	49.499751
3503.240325	445440.164251	49.504756
3503.498603	445422.066158	49.509761
3503.297801	445416.674095	49.514765
3503.487495	445410.961787	49.519770
3503.647926	445399.574561	49.524775
3502.864607	445406.605340	49.529780
3503.071263	445388.921740	49.534785
3503.480398	445391.996112	49.539789
3503.341909	445367.372959	49.544794
3502.871826	445367.909639	49.549799
3502.893305	445388.901379	49.554804
3502.919263	445391.990464	49.559809
3503.145192	445388.909067	49.564813
3503.350734	445380.759794	49.569818
3503.062057	445373.506323	49.574823
3503.164151	445364.208296	49.579828
3503.291286	445355.869547	49.584833
3503.092385	445348.905021	49.589837
3503.242318	445344.923748	49.594842
3503.084676	445329.381562	49.599847
3503.152352	445328.102156	49.604852
3503.125895	445316.138232	49.609857
3503.198267	445318.205128	49.614861
3503.191114	445303.144365	49.619866
3503.243350	445293.550538	49.624871
3502.981798	445294.558751	49.629876
3502.920430	445298.879890	49.634881
3502.789127	445313.710712	49.639885
3503.055055	445310.825329	49.644890
3503.258260	445301.966433	49.649895
3502.915816	445299.032785	49.654900
3503.268532	445290.503353	49.659905
3503.080992	445284.956851	49.664909
3503.271549	445276.302960	49.669914
3503.634320	445259.404019	49.674919
3503.181838	445249.287785	49.679924
3503.098713	445244.078441	49.684929
3503.394544	445242.303648	49.689933
3503.420707	445235.604938	49.694938
3503.608343	445226.799384	49.699943
3503.380442	445217.354784	49.704948
3503.353237	445202.601657	49.709953
3503.532422	445197.448941	49.714957
3503.134380	445193.764062	49.719962
3503.533936	445181.930178	49.724967
3503.412951	445182.762252	49.729972
3503.581536	445173.402075	49.734977
3503.424695	445166.126022	49.739981
3503.830841	445160.325975	49.744986
3503.392634	445153.097961	49.749991
3503.314079	445134.752854	49.754996
3502.871092	445112.869251	49.760001
3502.834377	445119.062643	49.765005
3502.687359	445124.362011	49.770010
3502.953004	445118.636657	49.775015
3503.355135	445112.380854	49.780020
3503.117837	445103.444950	49.785025
3502.879481	445102.978499	49.790029
3502.938257	445093.282037	49.795034
3503.154477	445099.026531	49.800039
3502.948198	445117.623143	49.805044
3502.884943	445112.055375	49.810049
3503.065927	445105.482332	49.815053
3502.928757	445115.800727	49.820058
3503.295110	445102.298901	49.825063
3503.000538	445101.689905	49.830068
3502.869695	445075.290114	49.835073
3502.886820	445094.051457	49.840077
3503.156933	445111.958160	49.845082
3503.205650	445105.407701	49.850087
3503.240675	445110.777417	49.855092
3503.227005	445100.687616	49.860097
3503.107766	445109.988668	49.865101
3502.814301	445095.280931	49.870106
3503.101740	445074.185425	49.875111
3502.946344	445072.893379	49.880116
3503.291258	445064.415904	49.885121
3503.040674	445069.073684	49.890125
3503.263027	445061.276420	49.895130
3503.270427	445043.778702	49.900135
3502.924840	445047.894850	49.905140
3503.014979	445045.597305	49.910145
3503.330618	445057.613414	49.915149
3502.781241	445065.517215	49.920154
3502.923142	445067.166550	49.925159
3503.006837	445065.478678	49.930164
3502.923645	445057.429299	49.935169
3502.884028	445057.233198	49.940173
3502.820437	445049.231183	49.945178
3503.034471	445039.001043	49.950183
3502.817598	445061.555232	49.955188
3503.096118	445053.646947	49.960193
3502.972008	445052.349557	49.965197
3502.756278	445054.212101	49.970202
3503.060351	445038.641581	49.975207
3502.874311	445035.072618	49.980212
3502.893888	445030.504973	49.985217
3503.371711	445059.279844	49.990221
3503.212824	445055.756962	49.995226
3503.317307	445049.704108	50.000231
3502.890599	445055.456965	50.005236
3502.960183	445048.345068	50.010241
3503.044370	445050.815687	50.015245
3503.188166	445030.961810	50.020250
3503.201074	445031.923171	50.025255
3503.087332	445025.704714	50.030260
3503.079789	445018.098832	50.035265
3503.150470	445010.631735	50.040269
3503.169814	445006.419125	50.045274
3503.510420	444999.565222	50.050279
3503.353568	444991.325537	50.055284
3503.580040	444989.055422	50.060289
3503.604825	444976.271127	50.065293
3503.201017	444976.745785	50.070298
3503.343845	444973.069943	50.075303
3503.056392	444969.518286	50.080308
3503.566623	444954.419649	50.085313
3503.530246	444947.680814	50.090317
3503.229494	444944.993571	50.095322
3503.339412	444937.570463	50.100327
3502.785343	444938.527209	50.105332
3502.996084	444920.538240	50.110337
3503.283895	444928.299142	50.115341
3503.208694	444924.812665	50.120346
3503.414424	444909.512417	50.125351
3503.120235	444908.649777	50.130356
3503.222317	444889.563612	50.135361
3503.155150	444898.095143	50.140365
3502.934355	444891.286350	50.145370
3503.216639	444902.192518	50.150375
3502.958700	444910.148042	50.155380
3502.921509	444909.545808	50.160385
3502.874935	444909.756611	50.165389
3503.072132	444906.730765	50.170394
3503.614369	444896.748806	50.175399
3503.074867	444898.514502	50.180404
3502.921909	444876.530420	50.185409
3502.731752	444882.141503	50.190413
3503.023748	444889.445272	50.195418
3503.246435	444902.390204	50.200423
3503.268052	444904.212234	50.205428
3503.532243	444903.304965	50.210433
3503.493283	444892.306519	50.215437
3503.318396	444885.895603	50.220442
3503.276941	444857.755980	50.225447
3502.911485	444856.347644	50.230452
3503.450805	444857.320558	50.235457
3502.871972	444870.300939	50.240461
3502.825279	444868.077454	50.245466
3502.835566	444853.723404	50.250471
3502.784685	444858.499274	50.255476
3502.732745	444841.670817	50.260481
3502.691366	444856.892318	50.265485
3502.847971	444867.972107	50.270490
3502.817632	444873.657333	50.275495
3502.971184	444863.538866	50.280500
3502.827330	444854.891191	50.285505
3502.844655	444864.524035	50.290509
3502.507657	444879.491708	50.295514
3502.688319	444880.272288	50.300519
3502.715093	444888.990642	50.305524
3502.618140	444884.138574	50.310529
3502.610693	444898.289243	50.315533
3502.621735	444912.538175	50.320538
3502.979126	444907.709963	50.325543
3502.574441	444901.997580	50.330548
3502.688892	444915.163845	50.335553
3502.628980	444935.257062	50.340557
3502.480095	444936.195339	50.345562
3502.781538	444930.818825	50.350567
3502.516835	444949.679131	50.355572
3502.667482	444951.479124	50.360577
3502.733857	444960.342831	50.365581
3502.831310	444959.058319	50.370586
3503.190386	444949.716233	50.375591
3502.701456	444964.101215	50.380596
3502.969111	444972.981262	50.385601
3502.732416	444984.381719	50.390605
3502.859071	444978.730775	50.395610
3502.857614	444969.095256	50.400615
3502.543795	444970.518124	50.405620
3502.989528	444991.032096	50.410625
3502.947941	445001.993514	50.415629
3503.112598	445000.545386	50.420634
3503.329484	445002.993352	50.425639
3502.843031	444992.375653	50.430644
3502.728936	444989.960831	50.435649
3502.980989	444996.003522	50.440653
3502.877821	445001.549006	50.445658
3503.007621	445012.379725	50.450663
3502.941309	445019.288201	50.455668
3502.834278	445014.995742	50.460673
3502.905380	445009.506435	50.465677
3502.495955	445005.417751	50.470682
3502.975296	445017.507359	50.475687
3502.693896	445039.109016	50.480692
3503.025660	445034.538780	50.485697
3503.382651	445030.319237	50.490701
3503.096452	445028.136663	50.495706
3503.294252	445018.315001	50.500711
3503.074288	445017.439692	50.505716
3503.517389	445006.967566	50.510721
3502.770692	445009.833635	50.515725
3502.879327	445006.315781	50.520730
3502.841317	445000.743673	50.525735
3502.786126	444995.377355	50.530740
3502.879337	444956.716970	50.535745
3503.121750	444923.102504	50.540749
3502.855150	444864.420383	50.545754
3502.954730	444793.554709	50.550759
3502.881880	444722.109662	50.555764
3502.898598	444631.326552	50.560769
3502.914825	444533.442967	50.565773
3502.789219	444424.577825	50.570778
3502.909876	444297.260142	50.575783
3502.579606	444173.568852	50.580788
3502.783630	444022.905756	50.585793
3503.010149	443880.656809	50.590797
3503.130056	443706.422409	50.595802
3503.366840	443521.160860	50.600807
3503.189753	443337.642102	50.605812
3503.529232	443119.037590	50.610817
3503.386100	442898.129472	50.615821
3503.256111	442659.921368	50.620826
3503.681934	442405.943110	50.625831
3503.280876	442147.284575	50.630836
3503.385530	441871.291224	50.635841
3503.168008	441587.233810	50.640845
3502.683509	441304.638541	50.645850
3502.910984	440994.882284	50.650855
3502.470577	440676.866150	50.655860
3502.776321	440342.333741	50.660865
3502.603465	440010.870815	50.665869
3502.536771	439664.673997	50.670874
3502.852928	439304.557733	50.675879
3502.729404	438933.654789	50.680884
3502.862666	438532.923632	50.685889
3502.756230	438127.305345	50.690893
3502.584887	437698.760205	50.695898
3502.866007	437276.014545	50.700903
3502.432445	436837.807827	50.705908
3502.621691	436364.022921	50.710913
3502.507343	435882.466636	50.715917
3502.321715	435401.368888	50.720922
3502.576105	434888.373287	50.725927
3502.231017	434380.846785	50.730932
3502.334403	433840.048456	50.735937
3502.362398	433307.571766	50.740941
3502.403781	432724.084288	50.745946
3502.517552	432141.077091	50.750951
3502.174160	431540.118736	50.755956
3501.857025	430921.937271	50.760961
3501.518449	430294.405435	50.765965
3501.333671	429653.178931	50.770970
3501.616275	428991.859330	50.775975
3501.293220	428329.051236	50.780980
3501.570911	427636.278891	50.785985
3501.371598	426926.869345	50.790989
3501.401860	426193.543860	50.795994
3501.392386	425455.380643	50.800999
3501.438160	424698.556475	50.806004
3501.404498	423904.869352	50.811009
3501.788722	423110.831075	50.816013
3501.154451	422286.126606	50.821018
3501.070770	421442.719783	50.826023
3500.835600	420584.028662	50.831028
3500.773921	419721.673435	50.836033
3500.859114	418829.307825	50.841037
3500.815839	417919.136124	50.846042
3501.026415	416984.211201	50.851047
3500.415876	416023.901627	50.856052
3500.806781	415047.820914	50.861057
3500.596208	414056.774415	50.866061
3500.203148	413047.083463	50.871066
3500.289200	412017.465096	50.876071
3499.806095	410975.892104	50.881076
3500.143382	409895.410781	50.886081
3500.150265	408807.297672	50.891085
3499.653632	407705.511868	50.896090
3499.921559	406574.876109	50.901095
3499.723403	405424.842519	50.906100
3499.611987	404258.438818	50.911105
3499.530916	403068.941638	50.916109
3499.252150	401872.416185	50.921114
3499.522234	400637.208932	50.926119
3499.261132	399392.689456	50.931124
3499.143430	398114.911343	50.936129
3498.720289	396835.172216	50.941133
3498.836956	395533.382817	50.946138
3498.553442	394209.116850	50.951143
3498.313571	392867.759254	50.956148
3498.118043	391501.710206	50.961153
3498.242424	390127.793813	50.966157
3497.653888	388728.752260	50.971162
3498.069439	387315.014632	50.976167
3497.674829	385880.027122	50.981172
3497.575961	384424.107028	50.986177
3497.086758	382951.410900	50.991181
3496.978653	381469.634680	50.996186
3497.190951	379961.248063	51.001191
3496.697854	378443.506859	51.006196
3496.251009	376903.418266	51.011201
3496.382377	375337.279055	51.016205
3496.115776	373772.814322	51.021210
3496.187124	372180.633738	51.026215
3495.818241	370568.877104	51.031220
3495.717648	368945.075851	51.036225
3495.348626	367305.125132	51.041229
3494.958193	365649.592022	51.046234
3495.133087	363958.741730	51.051239
3494.895176	362274.422928	51.056244
3494.627537	360553.791561	51.061249
3494.324204	358836.931499	51.066253
3494.290966	357099.067871	51.071258
3494.004349	355340.568460	51.076263
3493.668821	353572.539223	51.081268
3493.613744	351782.840130	51.086273
3492.932356	349979.765798	51.091277
3492.471747	348154.266641	51.096282
3492.116442	346313.994008	51.101287
3492.140923	344469.816253	51.106292
3491.969170	342623.334079	51.111297
3491.620587	340752.992648	51.116301
3491.516714	338866.429244	51.121306
3491.261368	336965.950725	51.126311
3490.966472	335049.934801	51.131316
3490.553625	333117.580454	51.136321
3490.098762	331187.479220	51.141325
3489.654458	329237.481169	51.146330
3489.384095	327263.460260	51.151335
3489.219606	325296.658868	51.156340
3488.765423	323294.383984	51.161345
3488.832695	321296.663665	51.166349
3488.264260	319281.627665	51.171354
3488.003915	317245.143940	51.176359
3487.505877	315214.978019	51.181364
3487.440732	313160.493663	51.186369
3487.034568	311099.313300	51.191373
3486.328155	309025.219412	51.196378
3486.384189	306931.921195	51.201383
3486.312902	304840.092813	51.206388
3485.777518	302725.834844	51.211393
3485.306899	300597.765684	51.216397
3485.050475	298465.027769	51.221402
3484.501382	296312.813726	51.226407
3483.758860	294160.001894	51.231412
3483.988732	291998.145178	51.236417
3483.468640	289820.689647	51.241421
3482.870411	287628.362588	51.246426
3482.755456	285424.176734	51.251431
3482.507205	283220.081088	51.256436
3482.039597	280990.652132	51.261441
3481.614460	278766.483159	51.266445
3481.239235	276534.664059	51.271450
3480.858214	274282.906145	51.276455
3480.415883	272016.594691	51.281460
3480.261789	269729.432875	51.286465
3479.782390	267446.817426	51.291469
3478.959843	265157.905044	51.296474
3478.926362	262845.518013	51.301479
3478.345523	260543.887231	51.306484
3478.088464	258223.069248	51.311489
3477.756709	255888.712601	51.316493
3476.927943	253554.186882	51.321498
3476.730887	251188.919008	51.326503
3476.024765	248849.926352	51.331508
3475.548126	246471.938807	51.336513
3474.978380	244112.241283	51.341517
3474.070297	241738.687586	51.346522
3473.779833	239355.040016	51.351527
3473.286104	236971.068876	51.356532
3472.195331	234586.360869	51.361537
3471.686391	232183.375433	51.366541
3471.578689	229789.778116	51.371546
3471.409181	227383.699616	51.376551
3470.383574	224975.210989	51.381556
3470.024986	222542.792728	51.386561
3469.635414	220124.688664	51.391565
3468.808474	217689.981672	51.396570
3468.483175	215255.881739	51.401575
3467.625234	212812.053064	51.406580
3467.352755	210367.220572	51.411585
3466.730146	207919.612668	51.416589
3466.053200	205467.502302	51.421594
3465.322021	202997.998341	51.426599
3464.448642	200541.518535	51.431604
3463.937209	198074.532707	51.436609
3463.437968	195610.661021	51.441613
3462.647550	193131.146851	51.446618
3461.991065	190659.048711	51.451623
3461.349528	188192.098928	51.456628
3460.604239	185708.991547	51.461633
3460.003982	183232.799844	51.466637
3459.304026	180753.579175	51.471642
3458.725230	178270.417986	51.476647
3457.917802	175791.829043	51.481652
3457.089563	173300.081790	51.486657
3456.458633	170813.745305	51.491661
3455.687610	168341.187629	51.496666
3455.141418	165853.228892	51.501671
3454.277407	163373.081411	51.506676
3453.583076	160881.749936	51.511681
3452.607675	158402.644061	51.516685
3451.986387	155914.022991	51.521690
3451.385661	153429.874949	51.526695
3450.470621	150954.787253	51.531700
3449.637996	148488.083821	51.536705
3449.418526	145936.690646	51.541709
3448.254670	143442.709154	51.546714
3448.085237	140957.260839	51.551719
3446.872114	138481.216986	51.556724
3446.248738	136008.160771	51.561729
3445.385306	133525.386623	51.566733
3444.573896	131051.330380	51.571738
3443.752155	128578.608063	51.576743
3442.589103	126114.129066	51.581748
3441.848229	123652.821922	51.586753
3440.647056	121191.041321	51.591757
3439.914046	118740.435059	51.596762
3439.360521	116290.496743	51.601767
3438.184757	113849.458227	51.606772
3437.010294	111407.485206	51.611777
3436.147235	108976.200079	51.616781
3435.324035	106552.462534	51.621786
3434.444676	104127.033738	51.626791
3432.818911	101730.279325	51.631796
3432.260170	99323.468337	51.636801
3431.290369	96932.400628	51.641805
3430.072912	94553.664596	51.646810
3429.181638	92164.811504	51.651815
3427.767187	89807.555055	51.656820
3426.914237	87458.000099	51.661825
3425.999521	85108.400022	51.666829
3424.578137	82770.309533	51.671834
3423.406068	80440.307375	51.676839
3422.133143	78143.068365	51.681844
3420.920333	75840.965157	51.686849
3420.157016	73565.742038	51.691853
3418.758778	71302.863109	51.696858
3417.703017	69037.103931	51.701863
3416.260180	66792.966328	51.706868
3415.296893	64566.362300	51.711873
3414.136425	62344.203376	51.716877
3412.556399	60151.464922	51.721882
3411.325569	57962.277277	51.726887
3409.934779	55798.827573	51.731892
3408.924250	53651.882897	51.736897
3407.688409	51526.573301	51.741901
3406.114509	49407.744618	51.746906
3404.913639	47313.748809	51.751911
3402.962469	45236.100075	51.756916
3401.708070	43173.725192	51.761921
3400.165557	41155.734272	51.766925
3398.308258	39156.321101	51.771930
3396.883216	37174.844656	51.776935
3394.282477	35235.723431	51.781940
3389.346942	33390.522361	51.786945
3383.342093	31652.931726	51.791949
3377.246009	29992.302922	51.796954
3371.758944	28407.578737	51.801959
3366.184112	26922.555606	51.806964
3361.288810	25523.586058	51.811969
3357.109706	24223.515058	51.816973
3353.024238	23043.699685	51.821978
3348.985679	21918.897237	51.826983
3345.577662	20902.252451	51.831988
3342.352539	19955.345250	51.836993
3339.454681	19074.359996	51.841997
3336.309549	18272.618171	51.847002
3334.069054	17529.544162	51.852007
3331.685505	16857.809793	51.857012
3329.395039	16228.397526	51.862017
3327.250849	15663.767295	51.867021
3325.236351	15152.832185	51.872026
3323.382526	14672.453748	51.877031
3321.658061	14240.711716	51.882036
3320.239025	13847.494926	51.887041
3318.886190	13497.165015	51.892045
3317.355188	13174.818684	51.897050
3316.745295	12877.804626	51.902055
3314.681334	12605.748202	51.907060
3314.080622	12359.088432	51.912065
3313.568908	12137.060306	51.917069
3312.273557	11927.684815	51.922074
3311.877678	11727.460129	51.927079
3310.720067	11558.561126	51.932084
3310.138157	11400.188022	51.937089
3309.271224	11243.855949	51.942093
3308.747707	11109.201124	51.947098
3308.332744	10973.127418	51.952103
3307.674364	10849.431258	51.957108
3306.900217	10731.895534	51.962113
3306.464114	10621.990943	51.967117
3306.398261	10523.745413	51.972122
3306.255011	10406.131118	51.977127
3305.143210	10311.045290	51.982132
3304.341011	10218.746229	51.987137
3304.188117	10116.399193	51.992141
3303.630445	10012.324031	51.997146
3303.032464	9929.867620	52.002151
3302.393049	9856.713110	52.007156
3301.944181	9767.800375	52.012161
3301.707363	9684.349810	52.017165
3301.148686	9618.007573	52.022170
3300.939018	9521.794321	52.027175
3300.299939	9438.034575	52.032180
3299.927493	9348.450707	52.037185
3299.734584	9271.195580	52.042189
3299.254563	9189.059277	52.047194
3299.135427	9092.314924	52.052199
3298.290868	9010.763131	52.057204
3297.679315	8915.964945	52.062209
3297.296924	8827.763221	52.067213
3296.730637	8750.147819	52.072218
3296.176391	8645.486836	52.077223
3295.640088	8551.467807	52.082228
3295.215967	8461.283144	52.087233
3295.175620	8376.905286	52.092237
3294.502943	8287.021552	52.097242
3293.939574	8182.499398	52.102247
3293.362640	8072.446540	52.107252
3293.208628	7965.945206	52.112257
3292.316387	7866.033952	52.117261
3291.989362	7780.050305	52.122266
3291.668047	7655.415736	52.127271
3291.340645	7553.375323	52.132276
3290.804682	7435.714579	52.137281
3290.130805	7333.001796	52.142285
3289.288972	7219.673309	52.147290
3289.135346	7102.160566	52.152295
3288.392841	6998.445165	52.157300
3287.923395	6875.230401	52.162305
3287.695165	6763.153222	52.167309
3286.844555	6638.361051	52.172314
3286.136221	6517.449401	52.177319
3285.651652	6397.269671	52.182324
3284.728512	6276.741660	52.187329
3284.432830	6148.509905	52.192333
3283.814978	6041.164680	52.197338
3283.450976	5913.087844	52.202343
3282.142378	5786.759195	52.207348
3281.389550	5671.997007	52.212353
3281.041223	5565.175959	52.217357
3280.163776	5452.405427	52.222362
3279.900622	5325.769154	52.227367
3279.064530	5225.667317	52.232372
3277.922705	5102.983006	52.237377
3277.756473	4990.572010	52.242381
3276.690915	4880.482360	52.247386
3276.507477	4762.517255	52.252391
3275.483362	4662.030963	52.257396
3275.102262	4535.764620	52.262401
3274.127187	4426.850324	52.267405
3273.582212	4324.239854	52.272410
3273.258518	4217.945589	52.277415
3271.947271	4102.922110	52.282420
3271.461006	4001.029390	52.287425
3270.884724	3896.307610	52.292429
3269.885790	3801.083080	52.297434
3269.501519	3686.490175	52.302439
3268.617823	3593.387907	52.307444
3268.007777	3495.172411	52.312449
3267.315910	3392.473034	52.317453
3266.484263	3304.968294	52.322458
3265.567319	3210.426593	52.327463
3264.618280	3127.025182	52.332468
3263.903873	3035.024837	52.337473
3263.319721	2946.180907	52.342477
3261.986703	2869.475130	52.347482
3261.475881	2785.924857	52.352487
3260.909819	2715.002048	52.357492
3260.358721	2643.251097	52.362497
3259.965731	2561.793225	52.367501
3258.600595	2491.731974	52.372506
3258.279682	2418.763885	52.377511
3257.194938	2347.707888	52.382516
3256.535153	2260.041407	52.387521
3256.196503	2202.217240	52.392525
3255.219113	2138.377016	52.397530
3254.878451	2065.349193	52.402535
3254.200561	1994.042112	52.407540
3253.426254	1937.117635	52.412545
3252.678665	1858.297902	52.417549
3252.099567	1797.388918	52.422554
3251.621695	1736.661051	52.427559
3250.711533	1676.949973	52.432564
3250.424974	1605.745970	52.437569
3249.701557	1541.503575	52.442573
3248.710335	1484.004335	52.447578
3248.260099	1412.061359	52.452583
3247.535211	1355.278980	52.457588
3246.829943	1293.874396	52.462593
3246.127348	1222.230811	52.467597
3245.495277	1166.638053	52.472602
3244.945489	1099.171876	52.477607
3244.036689	1038.752048	52.482612
3243.337324	980.486350	52.487617
3242.991152	929.210735	52.492621
3241.911706	873.413597	52.497626
3241.465111	805.760524	52.502631
3241.081217	763.398142	52.507636
3240.582395	706.097118	52.512641
3239.536512	645.106564	52.517645
3238.805731	593.068405	52.522650
3238.569537	536.209456	52.527655
3237.309167	481.403843	52.532660
3236.764188	422.012140	52.537665
3236.320612	382.403215	52.542669
3234.917245	332.072007	52.547674
3234.159622	275.094671	52.552679
3233.285467	244.083896	52.557684
3232.495009	212.417843	52.562689
3231.963299	187.707785	52.567693
3230.445051	166.755579	52.572698
3228.736711	161.655031	52.577703
3226.805853	164.826153	52.582708
3226.459094	165.990232	52.587713
3226.023747	160.239188	52.592717
3225.814282	173.409972	52.597722
3225.081313	167.144124	52.602727
3224.761544	164.579323	52.607732
3224.124549	168.386752	52.612737
3224.066802	163.234342	52.617741
3222.831198	165.905773	52.622746
3222.347402	167.402732	52.627751
3221.790982	171.047584	52.632756
3221.106015	167.368091	52.637761
3220.452766	169.092549	52.642765
3219.533600	182.579979	52.647770
3219.206963	175.767876	52.652775
3218.483848	177.097305	52.657780
3217.923896	173.723290	52.662785
3217.355835	175.467931	52.667789
3216.445364	183.624636	52.672794
3216.462739	177.106255	52.677799
3215.412423	178.446190	52.682804
3214.595519	180.441368	52.687809
3214.240669	169.778372	52.692813
3213.428946	176.968879	52.697818
3213.151090	166.012474	52.702823
3212.172092	175.681643	52.707828
3211.308995	172.068109	52.712833
3210.722771	167.463477	52.717837
3210.191062	172.502238	52.722842
3209.940355	167.678446	52.727847
3209.306405	180.633208	52.732852
3208.370063	171.332691	52.737857
3207.612124	171.054812	52.742861
3207.034305	175.568568	52.747866
3206.878217	166.236987	52.752871
3205.790322	169.508832	52.757876
3204.968540	170.805777	52.762881
3204.675908	171.826008	52.767885
3203.932762	172.297956	52.772890
3203.324781	167.772040	52.777895
3202.561636	167.263346	52.782900
3201.998010	170.502069	52.787905
3201.172852	156.405556	52.792909
3200.461564	169.249577	52.797914
3200.011766	159.406086	52.802919
3199.634581	165.674867	52.807924
3198.289824	175.561654	52.812929
3198.154355	167.266268	52.817933
3197.185229	179.688173	52.822938
3197.042630	163.294163	52.827943
3196.508993	174.242348	52.832948
3195.507534	168.201583	52.837953
3195.137514	168.517418	52.842957
3194.427483	170.036846	52.847962
3193.499759	154.954459	52.852967
3192.925564	159.578510	52.857972
3192.394461	168.334724	52.862977
3191.779489	164.677225	52.867981
3190.977463	164.809109	52.872986
3190.813560	158.213158	52.877991
3189.625397	163.948270	52.882996
3188.580231	164.542475	52.888001
3187.808199	162.594146	52.893005
3187.249827	174.229437	52.898010
3187.029353	163.403758	52.903015
3186.459020	166.440737	52.908020
3185.620578	158.882814	52.913025
3185.321664	154.147789	52.918029
3184.292531	165.681928	52.923034
3183.684926	153.506505	52.928039
3183.318223	159.909675	52.933044
3182.602549	157.496990	52.938049
3181.807439	155.352873	52.943053
3181.126657	160.860775	52.948058
3180.566726	158.102542	52.953063
3179.809816	165.063423	52.958068
3179.029517	152.881191	52.963073
3179.141267	153.275371	52.968077
3178.400221	155.923102	52.973082
3177.507476	154.763540	52.978087
3176.682347	154.792797	52.983092
3175.592184	162.075476	52.988097
3175.338960	152.171568	52.993101
3174.544843	153.456290	52.998106
3174.078282	151.177885	53.003111
3173.416885	158.637960	53.008116
3173.418554	159.781196	53.013121
3172.890166	152.444249	53.018125
3171.774460	164.080413	53.023130
3170.843394	163.673437	53.028135
3170.001272	162.281021	53.033140
3168.340118	154.906691	53.038145
3168.554290	151.312008	53.043149
3168.010353	160.546453	53.048154
3167.768571	155.316546	53.053159
3167.363742	159.245360	53.058164
3166.381150	161.990019	53.063169
3165.877107	159.179213	53.068173
3164.712606	157.638987	53.073178
3163.917708	151.697942	53.078183
3163.869848	162.224050	53.083188
3163.587894	165.080315	53.088193
3162.870268	154.001698	53.093197
3161.565276	155.173183	53.098202
3161.212466	151.341035	53.103207
3160.002331	157.559892	53.108212
3159.206801	160.100489	53.113217
3159.235142	157.978709	53.118221
3158.716251	161.074793	53.123226
3157.792751	158.094869	53.128231
3156.701166	163.615725	53.133236
3155.673165	154.105897	53.138241
3155.478094	157.633749	53.143245
3155.015487	164.095542	53.148250
3154.392102	157.230738	53.153255
3153.732577	147.290861	53.158260
3153.499465	149.805233	53.163265
3153.295477	148.109193	53.168269
3151.941478	162.534565	53.173274
3151.095346	159.518134	53.178279
3150.434066	155.675138	53.183284
3149.687352	161.371541	53.188289
3149.197257	154.109763	53.193293
3148.693551	156.718920	53.198298
3147.696881	156.497232	53.203303
3147.159185	161.574514	53.208308
3146.816246	156.022031	53.213313
3146.805293	154.132355	53.218317
3145.270744	158.710494	53.223322
3144.711376	150.039531	53.228327
3143.615739	150.079485	53.233332
3142.945199	162.258525	53.238337
3142.592765	160.839683	53.243341
3142.076936	164.737729	53.248346
3141.828316	160.142136	53.253351
3141.046905	159.157765	53.258356
3140.465003	161.841467	53.263361
3139.916256	155.997313	53.268365
3138.201527	165.504822	53.273370
3137.548085	161.743775	53.278375
3136.925204	151.430936	53.283380
3136.500065	157.879220	53.288385
3136.166976	148.996707	53.293389
3135.611051	151.928990	53.298394
3135.354718	151.865411	53.303399
3134.109657	153.570993	53.308404
3133.480155	147.605249	53.313409
3132.621775	148.279259	53.318413
3131.983622	156.893891	53.323418
3131.161890	142.124998	53.328423
3130.400269	151.456629	53.333428
3130.286649	151.344194	53.338433
3130.126021	147.195010	53.343437
3129.045985	145.058138	53.348442
3128.310677	147.441213	53.353447
3127.523795	149.777444	53.358452
3126.842752	154.168311	53.363457
3126.155694	151.059972	53.368461
3125.468767	157.042995	53.373466
3124.885219	150.234155	53.378471
3123.883744	151.772201	53.383476
3123.713836	157.455708	53.388481
3123.524553	146.558012	53.393485
3122.066710	153.776807	53.398490
3121.970332	151.167138	53.403495
3120.849727	153.227239	53.408500
3120.310448	150.060889	53.413505
3119.976442	145.868305	53.418509
3119.165583	151.026598	53.423514
3118.417296	144.460641	53.428519
3117.813014	149.062597	53.433524
3116.939965	146.165246	53.438529
3116.251332	149.080731	53.443533
3115.294211	148.312303	53.448538
3114.674884	147.055511	53.453543
3114.584006	151.103179	53.458548
3114.157282	144.878193	53.463553
3113.544234	140.791707	53.468557
3112.208106	150.047818	53.473562
3111.543334	145.014532	53.478567
3111.297444	143.997876	53.483572
3111.135441	148.144141	53.488577
3110.162376	140.134784	53.493581
3108.827035	148.721300	53.498586
3108.664981	138.615522	53.503591
3108.243972	146.390171	53.508596
3107.321880	151.571418	53.513601
3106.349755	142.489818	53.518605
3105.300200	145.350131	53.523610
3105.289729	145.666905	53.528615
3104.778553	149.500997	53.533620
3103.750458	151.457270	53.538625
3103.426504	143.314504	53.543629
3102.438749	147.684357	53.548634
3101.863377	143.087368	53.553639
3101.049179	142.993586	53.558644
3099.936225	149.926880	53.563649
3100.543395	142.509212	53.568653
3099.266404	150.087494	53.573658
3098.402785	144.591224	53.578663
3098.557084	145.110365	53.583668
3097.541322	151.069049	53.588673
3096.705100	143.815505	53.593677
3095.641845	148.291020	53.598682
3095.620884	147.073304	53.603687
3095.182494	145.719285	53.608692
3093.686260	143.828398	53.613697
3093.696791	136.103344	53.618701
3092.432119	154.401519	53.623706
3092.419944	139.384977	53.628711
3091.532782	142.566879	53.633716
3090.405200	153.505218	53.638721
3090.186123	150.176795	53.643725
3089.833890	145.989301	53.648730
3089.171020	154.800783	53.653735
3087.945731	146.370719	53.658740
3086.753317	148.727299	53.663745
3086.951471	144.513263	53.668749
3086.699435	150.249087	53.673754
3085.787699	139.075775	53.678759
3084.653858	143.421643	53.683764
3084.022431	149.894908	53.688769
3084.022548	144.431054	53.693773
3082.846085	155.228539	53.698778
3081.633911	136.921327	53.703783
3081.482516	141.805497	53.708788
3080.982081	141.510873	53.713793
3080.868404	144.459959	53.718797
3079.478099	148.353873	53.723802
3078.656163	142.207473	53.728807
3078.494251	139.742029	53.733812
3077.738672	143.318282	53.738817
3076.731873	142.046782	53.743821
3075.861041	143.881848	53.748826
3075.998318	139.060466	53.753831
3075.383759	147.703036	53.758836
3073.970879	147.425770	53.763841
3073.671608	135.345725	53.768845
3072.870984	147.594347	53.773850
3072.712386	143.696658	53.778855
3071.618304	139.052124	53.783860
3070.386095	147.786809	53.788865
3070.714933	141.455623	53.793869
3070.258027	143.974288	53.798874
3069.108722	148.108860	53.803879
3068.240581	145.755008	53.808884
3067.327495	155.646985	53.813889
3067.159278	141.578404	53.818893
3065.920830	141.079892	53.823898
3065.944377	140.828365	53.828903
3065.337665	139.095357	53.833908
3064.398400	151.869765	53.838913
3063.801474	145.575186	53.843917
3062.709088	144.135553	53.848922
3062.832050	140.143572	53.853927
3061.990789	147.913847	53.858932
3060.986580	141.536102	53.863937
3060.526696	144.040276	53.868941
3059.843380	152.385525	53.873946
3058.945728	144.163560	53.878951
3058.908874	147.654507	53.883956
3057.877799	143.576301	53.888961
3057.573678	140.511487	53.893965
3056.558621	152.232292	53.898970
3056.568183	137.506511	53.903975
3055.651786	144.354513	53.908980
3054.778315	141.861841	53.913985
3053.448225	132.962213	53.918989
3052.864581	145.512434	53.923994
3052.768136	137.030811	53.928999
3052.226893	142.985782	53.934004
3051.164149	149.816952	53.939009
3049.991992	142.985944	53.944013
3050.291033	141.042118	53.949018
3049.080456	140.322142	53.954023
3048.494882	142.790163	53.959028
3047.597577	142.424412	53.964033
3047.954203	138.388558	53.969037
3046.881237	143.805979	53.974042
3045.465062	134.337654	53.979047
3044.897574	130.748254	53.984052
3044.380688	141.354084	53.989057
3044.555037	132.599224	53.994061
3043.274434	140.008788	53.999066
3042.954897	135.911240	54.004071
3042.413800	136.148950	54.009076
3041.234125	143.881920	54.014081
3040.838005	136.630952	54.019085
3039.894280	142.172339	54.024090
3039.849265	136.051086	54.029095
3039.293287	141.426746	54.034100
3038.007601	141.609717	54.039105
3037.464071	137.738334	54.044109
3035.815389	137.416898	54.049114
3036.046091	131.844967	54.054119
3035.794406	139.100427	54.059124
3035.214057	141.526110	54.064129
3034.252810	134.251317	54.069133
3033.041579	137.604256	54.074138
3032.368528	131.679134	54.079143
3032.795992	133.271438	54.084148
3032.104487	145.375100	54.089153
3030.887635	127.955672	54.094157
3029.841196	139.074345	54.099162
3029.137545	136.871207	54.104167
3028.664300	135.797486	54.109172
3028.280636	145.533864	54.114177
3027.774853	134.170812	54.119181
3027.257222	143.692059	54.124186
3026.491659	138.105631	54.129191
3025.825479	131.410802	54.134196
3024.546601	140.135701	54.139201
3023.940085	129.016834	54.144205
3023.613802	139.421150	54.149210
3023.141958	137.220637	54.154215
3022.350741	138.129495	54.159220
3020.935995	133.925812	54.164225
3020.591982	136.034012	54.169229
3020.676442	137.100335	54.174234
3019.821656	133.395429	54.179239
3019.120427	131.483977	54.184244
3018.214756	131.786749	54.189249
3017.762809	128.927986	54.194253
3017.143394	135.431563	54.199258
3016.905949	132.869296	54.204263
3016.130284	141.184926	54.209268
3014.840560	138.271560	54.214273
3013.815245	134.769474	54.219277
3013.568028	127.645040	54.224282
3013.254758	131.056902	54.229287
3012.235704	136.640766	54.234292
3011.246891	132.392725	54.239297
3010.938623	130.185184	54.244301
3010.470675	136.129602	54.249306
3009.644977	137.587498	54.254311
3009.102646	137.064782	54.259316
3008.197009	138.198846	54.264321
3007.951002	126.483527	54.269325
3007.245467	137.346978	54.274330
3007.013551	137.169894	54.279335
3006.488207	133.551192	54.284340
3005.281226	138.047723	54.289345
3004.569200	130.759168	54.294349
3002.999630	130.808293	54.299354
3002.977101	135.076374	54.304359
3002.458917	132.345375	54.309364
3001.421103	135.344613	54.314369
3001.549004	135.045651	54.319373
3000.251659	134.219726	54.324378
2999.659255	131.788377	54.329383
2999.465406	138.415019	54.334388
2998.439500	133.325444	54.339393
2998.404037	131.306545	54.344397
2997.839964	135.446512	54.349402
2996.767098	131.031656	54.354407
2995.748699	121.589330	54.359412
2994.561471	129.628714	54.364417
2995.041323	128.233056	54.369421
2993.724083	126.847651	54.374426
2992.774888	122.294433	54.379431
2992.303189	123.080011	54.384436
2991.851133	134.478027	54.389441
2991.852516	125.470501	54.394445
2990.964378	130.000968	54.399450
2990.380514	127.858680	54.404455
2990.110518	122.898091	54.409460
2988.768486	127.382569	54.414465
2987.998030	124.879414	54.419469
2986.564755	130.405381	54.424474
2985.919072	131.276348	54.429479
2986.126841	130.412698	54.434484
2985.006188	127.200062	54.439489
2984.605407	121.162113	54.444493
2983.857468	136.983082	54.449498
2983.287723	134.967458	54.454503
2983.028397	129.483214	54.459508
2982.182753	133.662219	54.464513
2981.605803	123.199087	54.469517
2981.260076	136.797694	54.474522
2980.571849	125.487546	54.479527
2979.425108	129.294065	54.484532
2978.339956	134.367003	54.489537
2977.770450	128.433672	54.494541
2977.176494	137.083374	54.499546
2976.754546	132.050856	54.504551
2976.281686	136.933115	54.509556
2975.413593	128.615735	54.514561
2975.595276	123.633618	54.519565
2974.604577	130.499055	54.524570
2973.557918	126.611820	54.529575
2972.566337	132.713217	54.534580
2971.180175	131.482881	54.539585
2971.946243	128.176779	54.544589
2971.241006	133.573208	54.549594
2970.439830	129.539816	54.554599
2970.017850	126.367655	54.559604
2969.244451	129.412106	54.564609
2968.383339	126.354065	54.569613
2966.692119	141.878742	54.574618
2966.297734	134.345260	54.579623
2966.439403	124.709437	54.584628
2965.520561	137.195353	54.589633
2964.659255	124.689552	54.594637
2963.753976	128.357708	54.599642
2963.487081	130.473652	54.604647
2963.271094	131.631578	54.609652
2962.789775	139.286267	54.614657
2962.258160	131.513743	54.619661
2961.278973	132.268813	54.624666
2959.768319	123.164425	54.629671
2959.464634	126.342550	54.634676
2958.702231	135.249978	54.639681
2958.418466	131.036987	54.644685
2957.479458	137.349661	54.649690
2957.078889	128.310171	54.654695
2956.785063	129.902177	54.659700
2955.837137	129.883372	54.664705
2955.492748	129.476043	54.669709
2954.385633	127.337522	54.674714
2953.273472	131.875881	54.679719
2952.577963	125.889089	54.684724
2951.771238	121.915465	54.689729
2952.302735	122.513824	54.694733
2951.450908	127.796358	54.699738
2950.742268	113.883331	54.704743
2950.006233	123.905297	54.709748
2949.189006	124.791767	54.714753
2948.587524	119.260214	54.719757
2946.744064	131.995710	54.724762
2946.891111	120.537307	54.729767
2946.830594	130.615545	54.734772
2945.678547	127.948664	54.739777
2945.614638	120.706866	54.744781
2944.258504	117.234491	54.749786
2944.049426	122.929014	54.754791
2943.067185	121.612293	54.759796
2942.705215	126.232053	54.764801
2941.538810	119.153003	54.769805
2940.516773	123.470308	54.774810
2940.687380	126.923425	54.779815
2939.780637	124.351202	54.784820
2938.836850	125.344562	54.789825
2938.473363	127.554774	54.794829
2937.564403	123.474679	54.799834
2937.246521	125.756042	54.804839
2936.777339	125.533062	54.809844
2936.272183	133.599576	54.814849
2936.170511	120.761082	54.819853
2934.372598	132.361851	54.824858
2933.892564	125.970749	54.829863
2933.111196	125.518890	54.834868
2932.474175	126.876264	54.839873
2932.317889	119.813276	54.844877
2931.244807	126.846342	54.849882
2930.787983	127.448598	54.854887
2929.743091	130.839836	54.859892
2928.680287	131.759197	54.864897
2928.667778	124.599401	54.869901
2927.504288	128.365766	54.874906
2927.238297	128.697785	54.879911
2926.618024	125.864245	54.884916
2925.978539	133.753193	54.889921
2925.532541	123.830970	54.894925
2924.941803	122.635632	54.899930
2924.472010	126.637124	54.904935
2923.700583	129.568350	54.909940
2922.110442	126.124522	54.914945
2921.755461	122.816184	54.919949
2921.194294	124.512692	54.924954
2920.866442	120.622629	54.929959
2921.021321	125.259849	54.934964
2920.087136	118.189672	54.939969
2918.902795	116.196986	54.944973
2917.946050	123.306089	54.949978
2916.994584	117.868694	54.954983
2916.273172	118.290384	54.959988
2915.445650	121.482241	54.964993
2915.538421	118.350012	54.969997
2914.610604	124.449988	54.975002
2914.613686	123.448426	54.980007
2914.031435	119.857227	54.985012
2912.785214	116.972377	54.990017
2911.881498	115.867237	54.995021
2911.031782	116.100860	55.000026
2910.339356	117.224157	55.005031
2910.066166	119.549592	55.010036
2909.573890	118.129014	55.015041
2908.994359	114.020260	55.020045
2908.465103	120.956047	55.025050
2907.969239	123.025465	55.030055
2907.306801	123.964827	55.035060
2906.267133	116.375459	55.040065
2905.606935	115.555142	55.045069
2905.331383	125.049216	55.050074
2904.472779	124.799239	55.055079
2903.155425	126.134334	55.060084
2902.033171	134.363148	55.065089
2902.592267	126.459500	55.070093
2901.487345	125.518217	55.075098
2900.855891	122.988558	55.080103
2900.205415	121.135160	55.085108
2899.676082	129.688553	55.090113
2899.333936	123.755065	55.095117
2898.736880	129.322478	55.100122
2898.017498	117.495456	55.105127
2897.015830	117.000331	55.110132
2895.878810	123.086326	55.115137
2895.505468	120.823207	55.120141
2894.822542	124.556000	55.125146
2894.292110	127.963135	55.130151
2893.814273	116.277594	55.135156
2892.956037	124.170765	55.140161
2892.426426	118.368788	55.145165
2891.288254	118.917756	55.150170
2890.888465	122.570977	55.155175
2890.361306	117.455011	55.160180
2889.582507	123.948722	55.165185
2889.134793	111.708183	55.170189
2888.502694	120.468603	55.175194
2887.972275	118.674818	55.180199
2887.069999	117.188130	55.185204
2885.599060	119.391032	55.190209
2885.522081	115.551649	55.195213
2884.688741	114.737241	55.200218
2884.573598	120.238477	55.205223
2884.132138	113.835269	55.210228
2883.258542	118.217999	55.215233
2883.092447	112.248509	55.220237
2882.248727	117.416769	55.225242
2880.983459	116.852227	55.230247
2880.549655	120.336397	55.235252
2879.616259	116.267202	55.240257
2879.398819	121.880655	55.245261
2878.915184	127.333950	55.250266
2877.728511	117.538717	55.255271
2876.654974	117.412712	55.260276
2875.914364	122.418488	55.265281
2875.213848	115.650223	55.270285
2875.102262	119.998644	55.275290
2874.482349	127.933191	55.280295
2874.062827	120.863092	55.285300
2873.795651	134.001037	55.290305
2873.005370	117.481390	55.295309
2872.001932	124.253882	55.300314
2871.286523	120.874519	55.305319
2870.500386	116.311619	55.310324
2869.621321	122.565500	55.315329
2869.248152	108.728585	55.320333
2868.978678	124.055276	55.325338
2868.292623	117.703344	55.330343
2866.853854	110.583238	55.335348
2865.977694	119.944696	55.340353
2866.296846	119.481996	55.345357
2865.473781	124.209768	55.350362
2864.691018	118.149884	55.355367
2864.555269	115.683142	55.360372
2863.359242	119.052849	55.365377
2862.530640	113.317766	55.370381
2861.621971	118.115428	55.375386
2861.068152	119.350434	55.380391
2860.730664	116.386079	55.385396
2859.727446	110.558475	55.390401
2859.544949	112.552630	55.395405
2859.303115	124.738497	55.400410
2858.185321	115.526747	55.405415
2857.452608	115.341313	55.410420
2856.121467	123.890819	55.415425
2856.088929	114.552014	55.420429
2855.375219	112.427595	55.425434
2854.987939	112.855739	55.430439
2854.512927	112.817310	55.435444
2853.022199	119.182043	55.440449
2852.429817	114.464062	55.445453
2851.742914	112.412034	55.450458
2850.848096	117.446929	55.455463
2850.779150	112.194635	55.460468
2850.051926	114.634377	55.465473
2849.919588	114.008056	55.470477
2849.162328	123.734449	55.475482
2848.633448	115.215058	55.480487
2847.720383	109.202713	55.485492
2846.965457	113.453061	55.490497
2846.383119	110.298851	55.495501
2844.782090	115.032479	55.500506
2844.745143	116.444405	55.505511
2843.794141	108.078477	55.510516
2842.858294	116.447530	55.515521
2843.127452	103.023860	55.520525
2842.484428	115.545910	55.525530
2842.092597	112.333878	55.530535
2841.170761	112.499312	55.535540
2840.019118	118.944644	55.540545
2839.087612	104.661598	55.545549
2838.549720	116.019791	55.550554
2838.211807	116.686992	55.555559
2837.416410	115.133100	55.560564
2837.076847	125.946628	55.565569
2836.554891	119.025091	55.570573
2835.900143	122.991882	55.575578
2834.781615	118.184620	55.580583
2833.932717	108.739824	55.585588
2833.040235	122.231724	55.590593
2832.869080	117.651355	55.595597
2832.446219	113.337814	55.600602
2832.134188	121.488154	55.605607
2832.056068	108.187779	55.610612
2830.625440	114.512243	55.615617
2830.131562	109.316787	55.620621
2828.751852	116.914225	55.625626
2827.580950	116.866842	55.630631
2827.536892	122.551711	55.635636
2827.069513	122.597241	55.640641
2825.906278	115.827938	55.645645
2825.435574	113.923695	55.650650
2824.993263	113.241013	55.655655
2824.287677	114.920765	55.660660
2823.854990	117.227673	55.665665
2823.146493	111.937454	55.670669
2822.808416	121.188793	55.675674
2821.978422	113.106914	55.680679
2820.977797	122.843717	55.685684
2820.072542	117.393709	55.690689
2819.551390	111.273335	55.695693
2819.078764	114.257314	55.700698
2818.831854	115.176981	55.705703
2818.329542	109.468641	55.710708
2816.580409	114.336532	55.715713
2816.443102	111.514806	55.720717
2815.688345	111.137756	55.725722
2815.291422	108.077778	55.730727
2814.691714	99.834185	55.735732
2813.744847	111.935279	55.740737
2813.164455	102.731568	55.745741
2812.164791	112.381756	55.750746
2811.339359	107.541383	55.755751
2811.309658	107.741445	55.760756
2810.591038	109.402110	55.765761
2810.666509	107.035847	55.770765
2808.685136	105.919521	55.775770
2807.950724	110.704377	55.780775
2807.325302	109.578138	55.785780
2806.924643	113.019146	55.790785
2806.812025	109.231648	55.795789
2806.218411	112.447879	55.800794
2806.054664	105.949459	55.805799
2805.442892	106.431763	55.810804
2803.771941	105.883682	55.815809
2803.249184	101.775507	55.820813
2802.686683	108.120541	55.825818
2801.760027	105.136499	55.830823
2800.824377	98.224501	55.835828
2799.842395	108.012582	55.840833
2800.020979	103.745065	55.845837
2799.346896	105.316410	55.850842
2798.352863	108.980015	55.855847
2798.418599	106.069905	55.860852
2797.697953	108.268533	55.865857
2797.195187	99.590755	55.870861
2795.754552	106.827565	55.875866
2795.180667	100.692528	55.880871
2794.664253	104.409101	55.885876
2794.077942	113.691020	55.890881
2793.639056	98.983544	55.895885
2792.460953	102.035601	55.900890
2791.274665	115.383112	55.905895
2790.924699	103.050106	55.910900
2790.569898	111.866151	55.915905
2789.920856	101.891042	55.920909
2789.234172	104.392937	55.925914
2788.665516	102.724513	55.930919
2788.859744	104.986638	55.935924
2788.120388	114.121035	55.940929
2786.839381	110.844280	55.945933
2785.836302	109.283263	55.950938
2785.057531	105.141085	55.955943
2784.876389	101.934892	55.960948
2784.562698	118.403566	55.965953
2783.528122	106.205334	55.970957
2782.399315	103.605969	55.975962
2781.830437	108.158855	55.980967
2781.577251	105.000501	55.985972
2780.739030	108.675370	55.990977
2780.475528	106.351255	55.995981
2779.618679	111.426638	56.000986
2778.554359	111.324338	56.005991
2777.815030	106.329917	56.010996
2777.307775	108.271424	56.016001
2776.844324	106.613835	56.021005
2775.866670	115.229242	56.026010
2775.803640	120.242764	56.031015
2775.410642	111.522537	56.036020
2773.985045	116.705395	56.041025
2773.346040	109.168371	56.046029
2772.500372	112.310451	56.051034
2772.152475	115.106144	56.056039
2771.911949	103.842301	56.061044
2771.225108	113.996773	56.066049
2770.182665	102.605528	56.071053
2769.223454	111.783423	56.076058
2768.570552	110.691884	56.081063
2768.618372	103.854159	56.086068
2767.659055	114.667422	56.091073
2767.527414	103.640751	56.096077
2766.216981	106.452938	56.101082
2765.437542	105.229875	56.106087
2764.980574	100.784022	56.111092
2764.398733	107.003682	56.116097
2763.747122	99.102908	56.121101
2762.815138	110.327143	56.126106
2761.991939	114.779031	56.131111
2761.450528	110.160904	56.136116
2760.844355	117.492722	56.141121
2760.712624	113.437712	56.146125
2760.013065	112.515197	56.151130
2759.558333	112.504888	56.156135
2758.076287	112.013346	56.161140
2757.396905	107.035918	56.166145
2756.825409	112.087793	56.171149
2756.585069	110.326546	56.176154
2755.962578	109.399149	56.181159
2755.363034	103.297713	56.186164
2753.859732	115.062090	56.191169
2753.503990	110.771429	56.196173
2752.566970	114.578450	56.201178
2752.348168	106.531068	56.206183
2751.999375	107.974189	56.211188
2751.243093	113.049360	56.216193
2751.043646	103.644762	56.221197
2749.622018	114.138767	56.226202
2748.786702	119.799012	56.231207
2748.577476	107.168411	56.236212
2747.840438	112.695805	56.241217
2747.460771	109.227106	56.246221
2745.787566	114.474001	56.251226
2745.380012	110.178382	56.256231
2744.811951	108.615252	56.261236
2743.982989	116.385008	56.266241
2744.096624	114.199321	56.271245
2743.671682	109.429846	56.276250
2742.781070	111.928314	56.281255
2742.697732	105.943510	56.286260
2741.056894	113.097318	56.291265
2740.546625	104.955289	56.296269
2739.604852	115.082285	56.301274
2738.986210	105.316720	56.306279
2739.135019	102.506883	56.311284
2737.653775	105.100778	56.316289
2737.012591	93.406103	56.321293
2736.604366	107.226128	56.326298
2735.771280	106.990763	56.331303
2736.242232	97.473952	56.336308
2735.009526	114.198380	56.341313
2733.661772	100.241908	56.346317
2733.196960	104.054266	56.351322
2732.391949	105.035778	56.356327
2731.911500	97.755079	56.361332
2731.206329	110.368267	56.366337
2730.524215	101.220644	56.371341
2729.469956	106.926203	56.376346
2729.156402	104.298814	56.381351
2728.685163	103.720950	56.386356
2728.368763	104.756311	56.391361
2727.891459	103.130699	56.396365
2726.255027	110.300334	56.401370
2725.287647	104.870049	56.406375
2725.210420	98.740920	56.411380
2724.395956	113.444311	56.416385
2724.177384	102.172777	56.421389
2723.890176	104.671131	56.426394
2723.000860	104.041970	56.431399
2722.059485	102.800804	56.436404
2720.947720	98.980419	56.441409
2720.518978	99.232900	56.446413
2719.865141	100.294360	56.451418
2719.465521	111.047085	56.456423
2719.441891	100.281033	56.461428
2717.962010	106.401571	56.466433
2717.253177	100.254484	56.471437
2716.505600	108.111770	56.476442
2716.392230	103.430750	56.481447
2715.657784	95.299022	56.486452
2715.126585	106.453171	56.491457
2714.077486	103.329028	56.496461
2713.114072	109.701147	56.501466
2712.643018	109.065624	56.506471
2712.246864	98.332855	56.511476
2712.114595	109.286584	56.516481
2711.537198	106.084971	56.521485
2710.178572	101.371284	56.526490
2709.459764	113.146436	56.531495
2708.925817	99.554539	56.536500
2707.169125	106.306588	56.541505
2706.940065	107.705167	56.546509
2707.241531	99.671889	56.551514
2705.991064	110.583864	56.556519
2705.402246	101.632661	56.561524
2704.873668	114.385794	56.566529
2704.622097	104.218819	56.571533
2704.096369	100.625887	56.576538
2702.667829	103.580244	56.581543
2702.822697	103.903491	56.586548
2701.868272	103.241253	56.591553
2700.986239	105.220774	56.596557
2700.036088	105.086343	56.601562
2699.239724	105.526003	56.606567
2698.537386	108.985818	56.611572
2697.773182	110.773099	56.616577
2697.651335	99.447539	56.621581
2697.158702	101.818381	56.626586
2696.537947	112.852451	56.631591
2695.786636	100.803984	56.636596
2694.453322	115.609880	56.641601
2693.787372	104.272720	56.646605
2693.362540	105.029783	56.651610
2692.812759	109.320865	56.656615
2692.944423	110.168720	56.661620
2691.911467	110.400145	56.666625
2691.232441	108.160484	56.671629
2690.411135	109.387148	56.676634
2689.839707	102.278711	56.681639
2689.176717	97.046662	56.686644
2688.502807	111.126438	56.691649
2687.465397	102.212839	56.696653
2686.868290	104.768114	56.701658
2686.026862	109.043130	56.706663
2685.858459	100.329532	56.711668
2685.421232	107.540498	56.716673
2684.469812	103.592057	56.721677
2683.554790	109.028303	56.726682
2682.875356	109.076540	56.731687
2682.259416	103.294096	56.736692
2681.709631	112.515693	56.741697
2681.389487	102.598858	56.746701
2680.651083	104.727509	56.751706
2679.566657	105.677450	56.756711
2679.087327	104.214817	56.761716
2678.202697	110.773599	56.766721
2677.899776	99.637673	56.771725
2677.502918	106.983840	56.776730
2676.495843	108.756588	56.781735
2675.294279	101.293248	56.786740
2674.524545	103.145422	56.791745
2674.347428	105.536936	56.796749
2674.024585	108.830439	56.801754
2673.212280	107.742872	56.806759
2673.257923	99.621091	56.811764
2671.719237	103.382549	56.816769
2671.208957	94.559638	56.821773
2670.542654	106.958159	56.826778
2670.055645	112.125066	56.831783
2669.790499	102.606977	56.836788
2668.457325	112.104980	56.841793
2667.630794	110.343286	56.846797
2667.020635	106.600584	56.851802
2666.525976	99.482978	56.856807
2666.253100	102.495183	56.861812
2665.346362	107.048988	56.866817
2663.975106	103.109161	56.871821
2663.701498	106.099782	56.876826
2662.893431	102.720903	56.881831
2662.441623	100.087154	56.886836
2661.962999	107.694395	56.891841
2661.275297	108.358241	56.896845
2661.127517	104.996752	56.901850
2659.961435	114.286200	56.906855
2659.307866	95.260454	56.911860
2658.246383	106.643796	56.916865
2658.203554	103.205948	56.921869
2657.833031	102.726135	56.926874
2656.981731	107.847157	56.931879
2656.082256	105.848073	56.936884
2655.265415	107.360155	56.941889
2655.062159	99.817748	56.946893
2654.073916	101.997794	56.951898
2652.518582	110.899056	56.956903
2652.542451	99.036242	56.961908
2651.603922	108.788880	56.966913
2651.469122	101.211482	56.971917
2650.688041	103.497428	56.976922
2650.603687	110.652417	56.981927
2649.959234	102.076645	56.986932
2648.558230	107.462551	56.991937
2648.031956	106.228991	56.996941
2647.264898	107.764931	57.001946
2646.847209	109.715215	57.006951
2646.523416	97.291324	57.011956
2645.120656	105.863355	57.016961
2644.401537	104.493818	57.021965
2644.269504	95.656384	57.026970
2643.149814	96.069612	57.031975
2642.849286	101.380291	57.036980
2642.042539	111.407238	57.041985
2641.966701	112.814758	57.046989
2640.453453	104.082773	57.051994
2639.893935	108.077899	57.056999
2639.588004	101.756956	57.062004
2638.754604	106.363751	57.067009
2638.608575	100.538881	57.072013
2637.803122	109.606423	57.077018
2636.747336	109.773079	57.082023
2636.469561	102.235517	57.087028
2635.851791	114.725218	57.092033
2634.798126	105.032461	57.097037
2633.940250	103.694540	57.102042
2633.034804	108.143131	57.107047
2632.622541	101.757079	57.112052
2632.163648	107.039570	57.117057
2632.048311	107.203747	57.122061
2631.522144	106.363712	57.127066
2630.311588	111.484968	57.132071
2629.495747	99.947667	57.137076
2628.832938	110.840508	57.142081
2628.502562	108.438233	57.147085
2627.658928	109.937135	57.152090
2626.483176	103.470420	57.157095
2626.235149	99.790555	57.162100
2625.218033	107.755498	57.167105
2625.063101	102.274772	57.172109
2624.551696	105.256309	57.177114
2623.876798	110.769931	57.182119
2623.032770	106.559203	57.187124
2621.994381	109.411360	57.192129
2621.542102	105.360237	57.197133
2621.070537	111.035674	57.202138
2620.891156	108.481275	57.207143
2620.119769	110.565837	57.212148
2618.811836	112.718042	57.217153
2618.260728	108.776969	57.222157
2617.685405	107.894418	57.227162
2617.050032	110.587289	57.232167
2616.726336	100.853831	57.237172
2615.316404	112.493714	57.242177
2614.819877	104.508827	57.247181
2614.080709	98.755355	57.252186
2613.941229	105.620167	57.257191
2613.694209	100.113738	57.262196
2612.327496	97.807706	57.267201
2611.490989	97.714651	57.272205
2611.081454	96.688501	57.277210
2610.470518	93.581846	57.282215
2609.972483	96.836614	57.287220
2609.435822	102.887902	57.292225
2608.122163	96.441612	57.297229
2607.313258	101.669465	57.302234
2606.964670	106.119572	57.307239
2606.605686	91.554406	57.312244
2605.747993	110.275189	57.317249
2605.715498	93.797816	57.322253
2604.764197	109.272596	57.327258
2603.764029	109.761713	57.332263
2603.349462	107.286993	57.337268
2602.493129	104.798585	57.342273
2601.780747	101.423096	57.347277
2600.703904	102.272679	57.352282
2599.896211	94.989921	57.357287
2599.726171	96.671693	57.362292
2599.235948	105.677057	57.367297
2598.728382	105.869208	57.372301
2598.433160	97.394007	57.377306
2597.482950	97.946030	57.382311
2596.696940	92.922129	57.387316
2596.067092	100.343646	57.392321
2595.881679	99.491940	57.397325
2594.219308	99.557043	57.402330
2593.368934	99.310445	57.407335
2593.242836	97.292450	57.412340
2592.036027	96.774822	57.417345
2592.000289	97.887731	57.422349
2591.712330	91.419257	57.427354
2591.076284	95.260102	57.432359
2590.046786	94.160337	57.437364
2589.212313	96.490547	57.442369
2588.710454	100.422529	57.447373
2588.060288	96.106041	57.452378
2587.188989	100.962469	57.457383
2586.341420	87.739612	57.462388
2585.206030	95.878321	57.467393
2585.355186	95.452958	57.472397
2584.907740	96.069030	57.477402
2584.217852	98.022823	57.482407
2584.093739	94.144548	57.487412
2583.030502	97.923033	57.492417
2581.937603	86.058920	57.497421
2581.315353	96.335758	57.502426
2580.906484	95.209631	57.507431
2580.504606	89.341669	57.512436
2579.149532	102.407389	57.517441
2578.538226	94.329638	57.522445
2577.865808	96.164002	57.527450
2577.550360	98.240489	57.532455
2576.981423	96.638059	57.537460
2575.989593	103.556609	57.542465
2575.453596	93.961295	57.547469
2574.795473	100.956608	57.552474
2574.137524	103.791889	57.557479
2573.640259	98.710734	57.562484
2572.504341	103.212151	57.567489
2571.716244	97.931249	57.572493
2571.164079	97.906429	57.577498
2570.637596	96.172403	57.582503
2570.337653	98.327948	57.587508
2569.853132	100.592019	57.592513
2569.392509	104.983123	57.597517
2568.016106	98.827826	57.602522
2567.290743	102.968540	57.607527
2567.016995	95.981338	57.612532
2565.856345	102.116406	57.617537
2565.785060	95.370110	57.622541
2565.316456	96.600834	57.627546
2564.078415	105.332607	57.632551
2563.647696	91.238384	57.637556
2562.841871	93.054899	57.642561
2562.156017	94.050404	57.647565
2561.221946	101.120523	57.652570
2560.023751	93.863087	57.657575
2560.899290	86.145350	57.662580
2559.417031	98.020613	57.667585
2558.753235	87.216403	57.672589
2558.772638	105.660132	57.677594
2557.822022	102.086963	57.682599
2556.825788	93.574118	57.687604
2555.949400	96.770023	57.692609
2555.758089	93.868339	57.697613
2555.626141	93.768524	57.702618
2553.980059	95.015421	57.707623
2553.343935	93.964068	57.712628
2552.456552	96.789234	57.717633
2551.999728	96.461546	57.722637
2551.642626	93.496235	57.727642
2551.141485	90.640020	57.732647
2551.090899	89.085552	57.737652
2549.998311	90.830702	57.742657
2549.169678	96.431393	57.747661
2548.619356	101.184005	57.752666
2547.898282	102.022512	57.757671
2546.730523	93.116244	57.762676
2545.917460	102.919669	57.767681
2545.461790	101.679577	57.772685
2544.644968	95.098632	57.777690
2544.104497	101.511351	57.782695
2544.026536	98.234247	57.787700
2543.554108	99.979163	57.792705
2542.850814	96.643972	57.797709
2542.406718	99.804263	57.802714
2541.494161	101.380878	57.807719
2540.142616	88.398137	57.812724
2538.849513	101.381821	57.817729
2538.520841	94.519272	57.822733
2539.016177	96.064793	57.827738
2538.136253	92.560464	57.832743
2537.759111	92.062449	57.837748
2536.279248	104.147699	57.842753
2535.462747	96.652519	57.847757
2534.905106	95.500911	57.852762
2533.949178	106.001769	57.857767
2534.171137	96.714630	57.862772
2533.525134	96.763881	57.867777
2532.906705	95.476617	57.872781
2531.892554	100.988243	57.877786
2530.840737	102.513276	57.882791
2530.860979	90.119409	57.887796
2529.903307	100.532538	57.892801
2529.433957	95.880025	57.897805
2528.433874	94.881819	57.902810
2527.535889	99.326776	57.907815
2527.246714	98.097693	57.912820
2526.345217	95.043093	57.917825
2526.173172	103.109481	57.922829
2525.231917	95.502610	57.927834
2524.450983	88.756464	57.932839
2524.038482	94.778235	57.937844
2523.475822	102.904694	57.942849
2522.786257	98.204569	57.947853
2521.782781	98.990309	57.952858
2520.955293	102.226411	57.957863
2521.217710	93.003408	57.962868
2520.028159	95.276309	57.967873
2519.582173	100.241604	57.972877
2518.508888	97.695174	57.977882
2517.475711	97.232743	57.982887
2517.201852	90.197808	57.987892
2516.472238	99.117388	57.992897
2516.108819	99.815807	57.997901
2516.102746	97.574408	58.002906
2514.746550	94.508734	58.007911
2514.166746	84.968294	58.012916
2513.047601	92.516488	58.017921
2512.931930	91.345767	58.022925
2512.252336	93.518063	58.027930
2511.550372	97.273082	58.032935
2510.589013	90.357265	58.037940
2509.780214	91.657206	58.042945
2509.594760	98.300140	58.047949
2508.696975	95.268592	58.052954
2507.399084	100.071254	58.057959
2507.005099	90.922582	58.062964
2506.538831	96.786183	58.067969
2506.172063	94.628161	58.072973
2505.773019	101.754441	58.077978
2505.087433	109.958365	58.082983
2504.609547	99.494600	58.087988
2503.474743	100.973038	58.092993
2502.336396	95.815188	58.097997
2502.330544	91.291852	58.103002
2501.509564	92.262703	58.108007
2501.270369	90.711272	58.113012
2499.779888	101.930737	58.118017
2498.983540	104.567852	58.123021
2498.570477	101.618822	58.128026
2498.303914	109.875051	58.133031
2498.307287	94.134832	58.138036
2496.723612	100.453545	58.143041
2496.020893	97.968499	58.148045
2495.662261	96.180522	58.153050
2494.885101	102.408321	58.158055
2494.644018	101.130756	58.163060
2493.193191	112.261741	58.168065
2492.607585	105.604564	58.173069
2491.679171	101.361714	58.178074
2491.309366	110.830819	58.183079
2491.156211	97.141902	58.188084
2490.768587	102.760752	58.193089
2489.645422	100.529952	58.198093
2488.636240	102.266775	58.203098
2488.042938	106.477678	58.208103
2487.700630	105.472017	58.213108
2487.022627	100.334146	58.218113
2486.771794	102.641161	58.223117
2485.816874	98.822436	58.228122
2484.681103	100.473143	58.233127
2484.354732	93.674943	58.238132
2483.997349	102.042613	58.243137
2483.009327	104.723552	58.248141
2482.300069	105.078483	58.253146
2481.362519	106.310445	58.258151
2481.145298	101.376416	58.263156
2480.583584	107.609224	58.268161
2479.802861	101.953274	58.273165
2478.863887	99.355865	58.278170
2477.995387	110.294135	58.283175
2477.876398	101.030158	58.288180
2477.039972	102.346275	58.293185
2476.598329	101.368256	58.298189
2475.302386	102.248612	58.303194
2474.724543	107.129483	58.308199
2474.382005	102.122937	58.313204
2473.719556	112.294161	58.318209
2473.235134	100.161835	58.323213
2472.918380	103.664688	58.328218
2471.591924	106.166263	58.333223
2471.190861	102.658229	58.338228
2470.467232	105.695401	58.343233
2470.299191	99.973385	58.348237
2469.345207	105.251319	58.353242
2468.522557	102.958881	58.358247
2467.932348	93.486932	58.363252
2467.137413	101.812177	58.368257
2466.356086	99.915294	58.373261
2465.509928	90.888148	58.378266
2464.768738	102.056480	58.383271
2464.505232	92.761562	58.388276
2464.251154	96.457771	58.393281
2463.737809	100.910785	58.398285
2462.743986	94.355385	58.403290
2462.191330	103.828117	58.408295
2461.314234	86.993094	58.413300
2459.695271	107.463576	58.418305
2459.104381	105.558605	58.423309
2458.902775	95.186954	58.428314
2458.755507	104.600638	58.433319
2458.365337	105.407841	58.438324
2457.345873	108.359416	58.443329
2456.801383	95.417920	58.448333
2455.670797	103.920156	58.453338
2454.837825	103.394692	58.458343
2454.558280	102.026603	58.463348
2454.146977	105.808904	58.468353
2453.749725	102.749811	58.473357
2452.935634	98.954382	58.478362
2451.535084	98.992919	58.483367
2451.210784	100.345816	58.488372
2450.559804	104.135149	58.493377
2450.187098	106.106172	58.498381
2449.180796	99.408833	58.503386
2448.091016	99.559626	58.508391
2447.686065	95.522541	58.513396
2446.887912	105.441445	58.518401
2446.523823	101.021989	58.523405
2446.446514	104.123915	58.528410
2445.782536	102.958131	58.533415
2444.947259	97.061657	58.538420
2444.239725	103.945034	58.543425
2443.748672	99.700440	58.548429
2442.818046	90.240915	58.553434
2441.486237	106.361784	58.558439
2440.881246	96.200020	58.563444
2440.233446	102.530043	58.568449
2439.783375	91.724447	58.573453
2439.469865	97.537064	58.578458
2438.818538	104.672138	58.583463
2438.512868	104.125991	58.588468
2437.557488	104.289727	58.593473
2436.654130	99.985765	58.598477
2436.088359	92.755625	58.603482
2435.698235	94.375953	58.608487
2435.480482	87.243412	58.613492
2433.928702	99.746744	58.618497
2433.697290	92.534434	58.623501
2433.083779	94.833988	58.628506
2431.641231	95.257462	58.633511
2431.020737	98.568309	58.638516
2430.537309	97.432839	58.643521
2429.701984	85.378689	58.648525
2429.322365	91.553911	58.653530
2428.871532	92.494247	58.658535
2428.686513	85.932408	58.663540
2427.911306	92.693540	58.668545
2426.827028	90.047173	58.673549
2426.297320	85.519073	58.678554
2425.679756	87.177104	58.683559
2424.907100	86.357526	58.688564
2424.081667	97.497629	58.693569
2423.177093	96.104967	58.698573
2422.826902	91.634590	58.703578
2421.852284	101.425775	58.708583
2421.739975	94.107447	58.713588
2421.185215	94.447021	58.718593
2420.712740	101.586250	58.723597
2419.970536	89.716697	58.728602
2418.687538	92.499394	58.733607
2418.492602	95.136314	58.738612
2417.340871	102.906010	58.743617
2416.671132	93.092024	58.748621
2416.312245	90.940163	58.753626
2415.280033	90.822181	58.758631
2414.973439	93.681080	58.763636
2414.922124	92.637907	58.768641
2413.925648	92.594733	58.773645
2413.080639	92.403691	58.778650
2412.399875	93.961219	58.783655
2412.132563	91.842645	58.788660
2411.015975	99.171740	58.793665
2410.125374	89.685250	58.798669
2409.738508	92.939967	58.803674
2409.095645	98.439436	58.808679
2408.387222	91.611839	58.813684
2407.262294	97.652403	58.818689
2406.970940	99.349394	58.823693
2406.508298	98.461021	58.828698
2405.727425	98.359274	58.833703
2405.705881	93.436797	58.838708
2404.262223	92.607614	58.843713
2403.521556	93.761714	58.848717
2403.204217	90.045960	58.853722
2402.304807	98.020004	58.858727
2401.600293	92.124077	58.863732
2400.646650	99.671619	58.868737
2399.835977	89.903053	58.873741
2399.521251	91.163528	58.878746
2398.856590	96.470941	58.883751
2398.630574	95.594609	58.888756
2397.969584	101.024550	58.893761
2397.543558	98.246690	58.898765
2396.922050	91.737381	58.903770
2396.022890	96.293864	58.908775
2395.305423	86.850800	58.913780
2394.478817	86.814899	58.918785
2393.347684	93.615577	58.923789
2392.603037	85.285151	58.928794
2391.987209	91.779831	58.933799
2391.977112	88.501791	58.938804
2391.098280	95.561688	58.943809
2391.000553	88.410998	58.948813
2390.832289	80.051887	58.953818
2389.394805	87.889780	58.958823
2388.887107	93.501528	58.963828
2387.954370	86.182968	58.968833
2386.561788	86.552516	58.973837
2385.836124	86.662772	58.978842
2385.152611	84.092359	58.983847
2385.372812	79.812212	58.988852
2384.699325	93.861101	58.993857
2384.163898	94.442891	58.998861
2383.987342	87.622249	59.003866
2382.751940	91.192971	59.008871
2382.204577	92.990972	59.013876
2381.661989	93.884634	59.018881
2380.240117	93.913020	59.023885
2379.681796	90.091636	59.028890
2379.120086	95.790776	59.033895
2378.392710	87.015703	59.038900
2377.855818	94.062526	59.043905
2377.490224	95.692872	59.048909
2377.135478	90.300810	59.053914
2375.638290	94.635484	59.058919
2375.143643	90.749925	59.063924
2374.893054	92.906904	59.068929
2373.886129	89.051311	59.073933
2374.026521	91.596947	59.078938
2372.501069	88.163953	59.083943
2372.034857	90.376353	59.088948
2371.705409	98.595167	59.093953
2371.182282	99.093936	59.098957
2369.930435	94.116181	59.103962
2369.130517	90.806225	59.108967
2368.644303	87.312766	59.113972
2368.258969	88.697022	59.118977
2367.389486	92.790160	59.123981
2366.254503	85.057782	59.128986
2365.343951	90.377636	59.133991
2365.167126	95.836891	59.138996
2364.218000	94.541856	59.144001
2363.965395	91.824739	59.149005
2363.533564	87.084523	59.154010
2363.258635	95.961490	59.159015
2362.973765	87.936912	59.164020
2361.760947	92.867152	59.169025
2360.810940	95.854229	59.174029
2360.636178	90.729803	59.179034
2359.488012	93.621295	59.184039
2358.868525	88.294635	59.189044
2358.105092	93.055669	59.194049
2357.921222	91.188086	59.199053
2356.881512	87.492834	59.204058
2355.641561	91.080918	59.209063
2355.526019	85.802295	59.214068
2355.184351	89.700578	59.219073
2354.437038	86.608597	59.224077
2353.952656	83.804803	59.229082
2352.253754	89.650238	59.234087
2352.433520	85.408581	59.239092
2351.552029	90.281378	59.244097
2350.873767	90.811413	59.249101
2349.704220	92.600152	59.254106
2348.975190	88.125487	59.259111
2348.917845	88.456984	59.264116
2348.096982	90.892655	59.269121
2347.575000	87.320054	59.274125
2347.371404	90.370151	59.279130
2346.493727	86.901397	59.284135
2345.818316	90.441106	59.289140
2344.583989	91.944485	59.294145
2343.846723	80.831195	59.299149
2343.843472	85.844332	59.304154
2343.440448	89.283782	59.309159
2342.353398	88.804940	59.314164
2341.301304	91.508302	59.319169
2340.839490	91.227668	59.324173
2340.735661	90.767404	59.329178
2339.869827	97.631670	59.334183
2338.847947	90.918474	59.339188
2338.116610	91.786786	59.344193
2337.287191	90.382868	59.349197
2337.445808	88.311860	59.354202
2336.643762	92.002693	59.359207
2335.826490	91.996387	59.364212
2335.180925	95.798222	59.369217
2334.350985	88.064610	59.374221
2334.385606	91.668426	59.379226
2332.891634	98.449846	59.384231
2332.374712	91.004933	59.389236
2331.435969	92.395800	59.394241
2331.258937	93.023280	59.399245
2330.723813	84.935320	59.404250
2329.777604	97.488662	59.409255
2329.166940	85.106397	59.414260
2328.267542	86.285280	59.419265
2327.618764	87.855898	59.424269
2327.884404	87.959671	59.429274
2326.001265	90.206742	59.434279
2325.304264	85.847389	59.439284
2324.580113	81.583073	59.444289
2323.898614	92.516595	59.449293
2324.091885	84.484471	59.454298
2323.375508	96.351954	59.459303
2323.217172	83.588802	59.464308
2321.718346	90.393155	59.469313
2320.901430	87.835695	59.474317
2320.692335	91.959196	59.479322
2319.468492	90.152612	59.484327
2319.730475	85.398362	59.489332
2318.352731	87.396781	59.494337
2317.629535	98.435329	59.499341
2316.975111	87.686809	59.504346
2316.389378	87.883274	59.509351
2316.208297	83.473200	59.514356
2315.494282	90.183613	59.519361
2314.323904	96.641289	59.524365
2314.439712	94.191955	59.529370
2313.328717	99.583198	59.534375
2312.257145	87.265936	59.539380
2311.543519	87.246253	59.544385
2310.879753	84.034996	59.549389
2310.429019	93.843175	59.554394
2309.873024	93.458259	59.559399
2309.428429	91.212120	59.564404
2309.207373	86.548365	59.569409
2308.872035	93.957025	59.574413
2307.890654	91.345588	59.579418
2306.915592	92.632147	59.584423
2305.953913	87.599267	59.589428
2304.961087	94.563800	59.594433
2303.897828	97.463677	59.599437
2303.596711	90.345011	59.604442
2303.422631	87.674469	59.609447
2302.646599	87.850979	59.614452
2302.359271	95.693125	59.619457
2301.279205	93.907353	59.624461
2300.944029	84.383939	59.629466
2300.276960	98.723433	59.634471
2299.614008	91.903870	59.639476
2298.498641	92.369716	59.644481
2297.426645	90.880975	59.649485
2296.996900	89.535819	59.654490
2296.380968	96.325381	59.659495
2296.278424	89.413936	59.664500
2295.640183	93.998442	59.669505
2294.761542	85.215310	59.674509
2294.025355	92.713831	59.679514
2293.317606	96.544461	59.684519
2293.323292	95.476937	59.689524
2292.520149	95.593350	59.694529
2291.599756	92.348613	59.699533
2290.840404	91.817691	59.704538
2290.214140	98.234823	59.709543
2289.623828	89.919866	59.714548
2288.501749	92.859013	59.719553
2287.586092	97.227284	59.724557
2287.013108	91.380727	59.729562
2286.584899	88.555493	59.734567
2286.668093	93.809233	59.739572
2286.251937	91.376266	59.744577
2285.302449	93.170806	59.749581
2284.213681	85.657119	59.754586
2283.616842	92.857085	59.759591
2283.210696	90.350567	59.764596
2282.091364	86.103310	59.769601
2280.803951	87.078958	59.774605
2280.813272	85.289260	59.779610
2280.037631	91.257872	59.784615
2279.994914	85.676680	59.789620
2279.128013	92.544683	59.794625
2277.816414	87.296921	59.799629
2277.342672	82.046403	59.804634
2276.922039	93.482402	59.809639
2276.735691	86.325169	59.814644
2276.038651	89.109135	59.819649
2274.729545	92.525120	59.824653
2274.245121	85.954500	59.829658
2273.303274	86.155422	59.834663
2272.998191	80.823564	59.839668
2272.979557	94.870593	59.844673
2271.690108	94.808864	59.849677
2270.806900	91.328044	59.854682
2269.939270	89.634235	59.859687
2269.790008	85.735415	59.864692
2269.410415	81.804146	59.869697
2268.269102	86.170349	59.874701
2267.204041	79.215492	59.879706
2266.372470	92.080400	59.884711
2266.525874	82.493967	59.889716
2265.896962	88.258678	59.894721
2265.636915	80.633674	59.899725
2264.333363	84.094497	59.904730
2263.540320	89.850961	59.909735
2263.077870	82.062024	59.914740
2262.687775	86.763957	59.919745
2261.942541	89.100656	59.924750
2260.801276	82.352639	59.929754
2259.943238	85.572676	59.934759
2259.721653	88.691374	59.939764
2259.059720	88.166296	59.944769
2258.419072	82.882352	59.949774
2257.557737	87.141864	59.954778
2256.576661	92.576814	59.959783
2256.266584	93.879526	59.964788
2255.688225	97.861315	59.969793
2255.650734	91.100585	59.974798
2255.259209	88.099744	59.979802
2254.504072	98.672851	59.984807
2253.291130	87.237518	59.989812
2252.417372	90.569979	59.994817
2251.469158	90.687523	59.999822
2250.729433	81.337509	60.004826
2250.045156	91.767446	60.009831
2250.023271	89.742698	60.014836
2249.633621	88.378454	60.019841
2249.322235	92.492212	60.024846
2248.281925	88.980634	60.029850
2247.048202	91.091410	60.034855
2246.930948	97.102954	60.039860
2245.553998	99.829520	60.044865
2244.779931	93.168703	60.049870
2244.443717	94.534698	60.054874
2243.577218	86.685786	60.059879
2243.356583	84.664635	60.064884
2243.129606	87.142829	60.069889
2241.365981	89.492248	60.074894
2241.246924	86.646122	60.079898
2240.347058	91.107220	60.084903
2239.651239	88.756819	60.089908
2239.260058	89.340401	60.094913
2238.896969	88.953686	60.099918
2238.472449	86.297952	60.104922
2237.011970	83.436502	60.109927
2236.652903	88.637980	60.114932
2236.401291	88.969938	60.119937
2235.154908	81.109420	60.124942
2234.553751	89.245222	60.129946
2233.641773	97.268399	60.134951
2233.378889	87.929599	60.139956
2232.824787	93.611653	60.144961
2232.268667	90.680015	60.149966
2231.361974	88.846846	60.154970
2230.304232	96.735878	60.159975
2229.697402	87.869568	60.164980
2229.311119	86.575800	60.169985
2228.793697	86.804011	60.174990
2228.788428	85.876121	60.179994
2227.558146	86.611098	60.184999
2226.605377	78.739843	60.190004
2226.264770	85.755071	60.195009
2225.623345	91.464690	60.200014
2224.399098	78.789509	60.205018
2223.464997	87.815114	60.210023
2223.220239	78.841892	60.215028
2222.621298	81.245151	60.220033
2222.060043	86.462654	60.225038
2222.003934	79.060533	60.230042
2220.921012	89.913500	60.235047
2220.221135	78.333996	60.240052
2219.789378	83.868814	60.245057
2218.884681	86.316864	60.250062
2217.930848	81.178063	60.255066
2216.936367	88.422744	60.260071
2216.536828	86.986776	60.265076
2215.911276	97.312334	60.270081
2215.469132	92.089180	60.275086
2215.369030	87.870125	60.280090
2214.136191	88.476862	60.285095
2213.185554	84.124987	60.290100
2212.839226	86.143611	60.295105
2212.017539	87.064494	60.300110
2212.389426	83.702977	60.305114
2211.020219	84.155017	60.310119
2210.197044	80.046204	60.315124
2209.543763	85.317733	60.320129
2209.342028	84.794088	60.325134
2208.577635	90.615523	60.330138
2207.126894	88.912506	60.335143
2206.678394	85.326173	60.340148
2206.138221	90.855062	60.345153
2205.312433	88.304271	60.350158
2205.644844	86.368138	60.355162
2204.346582	89.729389	60.360167
2203.598420	83.634134	60.365172
2202.631528	92.885212	60.370177
2202.499757	93.776130	60.375182
2201.859508	87.448873	60.380186
2200.467289	91.429725	60.385191
2199.788305	85.841304	60.390196
2199.434852	79.562105	60.395201
2198.944821	81.780956	60.400206
2198.743113	76.451561	60.405210
2197.993531	86.321104	60.410215
2197.141932	78.998193	60.415220
2196.183316	86.054774	60.420225
2195.909498	87.039850	60.425230
2195.447329	85.479995	60.430234
2194.244199	88.445649	60.435239
2193.497801	84.762639	60.440244
2193.231314	87.941120	60.445249
2192.444722	85.829270	60.450254
2192.153666	84.002922	60.455258
2191.052315	94.015523	60.460263
2190.582593	84.138574	60.465268
2189.675095	89.906330	60.470273
2189.058003	87.384584	60.475278
2188.021277	86.805197	60.480282
2187.160236	88.749619	60.485287
2186.894452	87.877336	60.490292
2186.029598	87.662883	60.495297
2185.864001	93.620326	60.500302
2185.556434	87.079471	60.505306
2184.929306	95.001831	60.510311
2184.332051	81.658136	60.515316
2183.547926	83.645059	60.520321
2182.583139	91.319651	60.525326
2181.656010	92.115287	60.530330
2180.395866	90.980054	60.535335
2180.101893	86.631928	60.540340
2179.783075	90.099217	60.545345
2179.292693	93.817683	60.550350
2178.971909	81.056683	60.555354
2177.763005	87.335445	60.560359
2177.197177	86.551582	60.565364
2176.337069	87.317599	60.570369
2175.879555	82.423912	60.575374
2175.825509	80.429536	60.580378
2174.439055	84.797812	60.585383
2173.885266	84.997513	60.590388
2173.355597	89.744239	60.595393
2172.802977	88.420110	60.600398
2172.411089	88.255818	60.605402
2171.157357	97.031372	60.610407
2170.677642	78.622628	60.615412
2170.070214	82.463343	60.620417
2169.325473	86.140840	60.625422
2168.266526	86.244969	60.630426
2167.608407	96.145849	60.635431
2167.518344	83.238815	60.640436
2167.094711	83.290339	60.645441
2165.908798	79.811184	60.650446
2164.770604	73.095436	60.655450
2164.042237	79.308195	60.660455
2164.278469	88.287192	60.665460
2163.486480	78.244323	60.670465
2162.791635	86.515355	60.675470
2162.056163	80.569907	60.680474
2161.102811	79.348263	60.685479
2160.806228	81.268779	60.690484
2160.169960	78.605850	60.695489
2159.478196	82.633879	60.700494
2158.732150	76.680374	60.705498
2158.009192	87.699139	60.710503
2157.499100	78.169355	60.715508
2156.866611	80.576778	60.720513
2156.143271	88.538485	60.725518
2154.921189	82.910334	60.730522
2154.346991	88.426885	60.735527
2153.855723	83.457267	60.740532
2153.573489	82.292547	60.745537
2152.607207	85.006524	60.750542
2152.719031	85.851833	60.755546
2151.781459	90.292153	60.760551
2150.755611	83.184572	60.765556
2150.190845	90.069593	60.770561
2149.476122	89.632897	60.775566
2149.007282	79.387926	60.780570
2147.619672	82.725391	60.785575
2147.592728	80.361657	60.790580
2146.970912	77.830464	60.795585
2146.101872	82.370769	60.800590
2145.207512	68.228862	60.805594
2144.581879	75.869916	60.810599
2144.082613	82.083756	60.815604
2143.761916	83.627489	60.820609
2142.965136	85.268832	60.825614
2142.424109	80.857180	60.830618
2141.430890	82.735007	60.835623
2140.830049	79.167240	60.840628
2140.801622	86.507218	60.845633
2139.801157	87.059229	60.850638
2139.216462	79.619631	60.855642
2138.141118	80.672720	60.860647
2137.677420	79.778634	60.865652
2136.528455	87.046982	60.870657
2135.224116	86.149837	60.875662
2135.476863	72.157907	60.880666
2134.759194	84.047706	60.885671
2134.281344	80.299042	60.890676
2133.570971	81.140899	60.895681
2132.891852	78.634508	60.900686
2132.944460	85.800369	60.905690
2131.459196	89.309272	60.910695
2130.692442	88.888188	60.915700
2130.355365	79.468154	60.920705
2129.698395	84.664927	60.925710
2129.623605	79.763813	60.930714
2128.157939	99.724949	60.935719
2127.313121	85.116681	60.940724
2126.692043	86.754421	60.945729
2126.494472	87.835797	60.950734
2126.133268	85.163326	60.955738
2124.850950	88.931587	60.960743
2124.348151	86.558455	60.965748
2123.039694	86.516986	60.970753
2122.549656	84.829672	60.975758
2122.883480	87.421550	60.980762
2122.105632	91.060111	60.985767
2121.068956	89.095252	60.990772
2120.440072	83.549987	60.995777
2119.656849	87.650108	61.000782
2119.599269	80.661917	61.005786
2118.276887	92.532392	61.010791
2117.707111	79.929252	61.015796
2117.027044	82.024697	61.020801
2116.590327	83.191974	61.025806
2116.459231	84.447895	61.030810
2114.697609	86.594516	61.035815
2114.254829	89.014495	61.040820
2113.750845	87.021684	61.045825
2113.487464	88.821659	61.050830
2112.784121	76.700429	61.055834
2111.023668	91.955182	61.060839
2110.764729	80.953553	61.065844
2110.145946	74.658962	61.070849
2109.870576	83.693480	61.075854
2109.870222	79.455400	61.080858
2108.692891	78.019453	61.085863
2107.392973	79.628044	61.090868
2106.932158	81.690726	61.095873
2106.266250	89.858132	61.100878
2106.222245	83.131688	61.105882
2105.645776	87.206710	61.110887
2104.569590	77.265754	61.115892
2103.803366	74.343625	61.120897
2103.059174	77.339742	61.125902
2103.010375	80.308495	61.130906
2101.793360	84.539258	61.135911
2100.766962	81.187962	61.140916
2100.397991	86.712043	61.145921
2100.153423	86.530058	61.150926
2099.881963	78.480729	61.155930
2098.454169	84.184727	61.160935
2097.599331	80.424366	61.165940
2097.183350	82.324649	61.170945
2096.672616	83.740631	61.175950
2096.561828	83.412611	61.180954
2095.109210	87.230138	61.185959
2094.597326	90.073238	61.190964
2093.840974	94.453362	61.195969
2093.033693	97.254624	61.200974
2093.105412	74.959886	61.205978
2092.098448	82.741956	61.210983
2091.403365	78.967297	61.215988
2090.777643	80.690305	61.220993
2090.046558	89.261607	61.225998
2089.711923	87.432853	61.231002
2088.372318	89.094420	61.236007
2088.015888	82.944817	61.241012
2087.791779	88.243998	61.246017
2086.756119	91.507070	61.251022
2085.862578	81.658030	61.256026
2084.859712	81.912051	61.261031
2084.532861	81.994394	61.266036
2084.075061	85.163758	61.271041
2083.502304	84.850810	61.276046
2083.436231	92.612473	61.281050
2081.812954	95.350420	61.286055
2081.182258	85.620625	61.291060
2080.673815	88.977855	61.296065
2080.413931	100.617268	61.301070
2080.109422	85.167414	61.306074
2078.643281	89.492897	61.311079
2078.086189	82.319762	61.316084
2077.626299	84.790826	61.321089
2076.734446	96.022427	61.326094
2076.328787	93.694261	61.331098
2075.140944	92.705365	61.336103
2074.736644	91.726128	61.341108
2074.804532	95.073989	61.346113
2073.795289	97.788618	61.351118
2072.968099	84.628746	61.356122
2071.718308	91.179773	61.361127
2071.499025	93.407190	61.366132
2070.906223	94.037506	61.371137
2069.648581	100.108712	61.376142
2068.923696	92.200093	61.381146
2068.439799	87.739600	61.386151
2068.255527	82.209082	61.391156
2067.806875	89.642249	61.396161
2066.894154	87.603703	61.401166
2066.495180	83.359599	61.406170
2065.383102	87.476108	61.411175
2064.635244	90.260498	61.416180
2064.122808	91.795586	61.421185
2063.412992	94.865564	61.426190
2063.176214	87.488042	61.431194
2062.874985	85.663443	61.436199
2062.095826	84.127823	61.441204
2061.007316	84.408339	61.446209
2060.728309	87.718037	61.451214
2059.457803	86.976566	61.456218
2058.693201	90.784572	61.461223
2058.051737	84.932402	61.466228
2057.618288	85.323101	61.471233
2056.857620	87.798641	61.476238
2056.921221	91.233283	61.481242
2055.187880	96.487076	61.486247
2054.478480	91.119797	61.491252
2053.945811	92.492563	61.496257
2053.454615	100.040377	61.501262
2053.491047	91.827466	61.506266
2052.733645	96.102778	61.511271
2052.307626	87.764110	61.516276
2051.617187	92.404137	61.521281
2050.421221	92.456334	61.526286
2049.245054	90.304570	61.531290
2048.243507	98.574785	61.536295
2048.144652	90.741056	61.541300
2047.355425	97.909599	61.546305
2046.949518	96.456577	61.551310
2046.822848	89.702435	61.556314
2046.106522	98.765807	61.561319
2045.374354	97.330698	61.566324
2044.465860	96.747168	61.571329
2043.992190	100.295421	61.576334
2043.283654	91.010378	61.581338
2042.499374	95.978683	61.586343
2041.607310	86.477939	61.591348
2041.131177	87.937348	61.596353
2040.214261	87.671432	61.601358
2040.585455	87.119659	61.606362
2039.084485	94.869797	61.611367
2038.212060	86.495390	61.616372
2037.737083	82.327445	61.621377
2037.059616	88.370463	61.626382
2037.172470	79.290310	61.631386
2035.610247	86.180560	61.636391
2035.181737	90.098836	61.641396
2035.070820	89.779918	61.646401
2033.982718	91.216117	61.651406
2033.228817	79.937601	61.656410
2032.494611	84.827078	61.661415
2031.796958	90.057265	61.666420
2031.407952	92.610546	61.671425
2030.270890	91.564029	61.676430
2029.764432	90.662268	61.681434
2029.023325	96.632099	61.686439
2028.896866	86.741462	61.691444
2028.204951	85.645643	61.696449
2027.604109	89.593002	61.701454
2026.837480	89.538609	61.706458
2025.624527	94.024867	61.711463
2025.041824	90.098762	61.716468
2024.715046	85.612190	61.721473
2023.688176	95.434443	61.726478
2022.826816	85.063617	61.731482
2022.158888	96.735715	61.736487
2021.349623	91.100930	61.741492
2021.240715	90.502995	61.746497
2020.763659	95.138892	61.751502
2020.244335	88.665068	61.756506
2020.069707	91.837312	61.761511
2019.229648	90.032652	61.766516
2018.281754	80.580546	61.771521
2017.542529	98.911562	61.776526
2016.570879	84.974342	61.781530
2015.556794	89.828016	61.786535
2015.225831	83.688277	61.791540
2015.165908	80.221809	61.796545
2014.466596	83.042108	61.801550
2013.807722	78.693265	61.806554
2012.690529	89.246990	61.811559
2011.801829	80.856430	61.816564
2011.518831	84.006553	61.821569
2010.672125	90.387590	61.826574
2009.836402	84.263933	61.831578
2009.058125	94.032216	61.836583
2008.437363	87.842973	61.841588
2008.248909	82.827498	61.846593
2007.823181	85.945592	61.851598
2006.943245	84.071575	61.856602
2005.817077	97.352395	61.861607
2005.248783	78.813200	61.866612
2004.818248	81.693703	61.871617
2004.415855	83.963890	61.876622
2004.025051	79.447224	61.881626
2002.416112	82.953234	61.886631
2001.662976	83.098239	61.891636
2001.536907	86.089287	61.896641
2000.822743	82.822756	61.901646
2000.505379	78.548518	61.906650
1999.275258	90.111524	61.911655
1998.879652	77.015613	61.916660
1997.931123	83.095525	61.921665
1997.553737	84.018592	61.926670
1997.307418	80.292705	61.931674
1996.126046	82.805087	61.936679
1995.398245	86.952974	61.941684
1994.567015	83.516214	61.946689
1993.992017	86.686289	61.951694
1993.746557	85.068069	61.956698
1993.541028	86.431851	61.961703
1992.817214	87.468255	61.966708
1992.138696	87.977457	61.971713
1990.493706	92.736170	61.976718
1989.759347	83.532137	61.981722
1988.672970	94.493476	61.986727
1988.802902	85.972880	61.991732
1988.593485	87.405615	61.996737
1987.986051	88.008048	62.001742
1987.870696	82.389962	62.006746
1986.401759	85.396389	62.011751
1985.602945	82.702477	62.016756
1985.819276	89.990708	62.021761
1984.077830	89.321920	62.026766
1983.391231	81.962149	62.031770
1982.697766	79.014964	62.036775
1982.294970	86.016354	62.041780
1981.917793	82.298248	62.046785
1981.235766	90.935767	62.051790
1980.512163	87.027851	62.056794
1979.261212	88.082195	62.061799
1978.894003	85.301427	62.066804
1978.367696	82.539587	62.071809
1978.300457	83.780638	62.076814
1977.337438	80.069990	62.081818
1976.409504	87.334100	62.086823
1975.774045	96.451531	62.091828
1975.738648	82.563767	62.096833
1974.242159	90.294991	62.101838
1973.704868	84.601063	62.106842
1973.072009	87.039750	62.111847
1972.643464	78.433517	62.116852
1971.698774	85.941274	62.121857
1970.454186	87.077424	62.126862
1970.243774	84.786525	62.131866
1969.344635	86.041206	62.136871
1969.340480	90.642389	62.141876
1968.598202	89.758081	62.146881
1967.997830	97.893364	62.151886
1967.249298	87.628378	62.156890
1966.120231	86.147104	62.161895
1965.422437	84.594028	62.166900
1965.462774	84.610013	62.171905
1964.502026	90.107439	62.176910
1964.364302	92.738917	62.181914
1962.982939	83.238218	62.186919
1962.529442	81.626773	62.191924
1962.102863	81.898283	62.196929
1961.209250	88.279453	62.201934
1960.350838	83.997513	62.206938
1959.194691	94.301341	62.211943
1958.849203	85.710897	62.216948
1958.206817	83.957693	62.221953
1957.899012	94.051270	62.226958
1957.987508	84.001508	62.231962
1957.111781	88.084313	62.236967
1956.212256	90.181398	62.241972
1955.755857	85.057823	62.246977
1954.609223	88.278323	62.251982
1953.574757	81.285160	62.256986
1952.803703	86.206999	62.261991
1952.347406	93.813180	62.266996
1952.348438	89.745783	62.272001
1951.695574	92.003955	62.277006
1950.926224	82.292779	62.282010
1949.860846	88.650836	62.287015
1949.076669	91.377901	62.292020
1948.975467	85.968967	62.297025
1948.248751	84.941874	62.302030
1947.469489	81.528205	62.307034
1946.270168	96.084257	62.312039
1945.955678	90.916274	62.317044
1945.440666	85.428925	62.322049
1944.951043	87.537203	62.327054
1944.276708	93.707977	62.332058
1943.076002	94.122180	62.337063
1943.247791	89.570062	62.342068
1942.518596	83.590033	62.347073
1941.380412	91.451805	62.352078
1940.604923	86.978847	62.357082
1939.614423	89.580952	62.362087
1939.409831	82.652661	62.367092
1939.154315	83.832372	62.372097
1937.936780	79.195047	62.377102
1937.321107	83.462304	62.382106
1936.478722	80.318374	62.387111
1936.030496	85.388664	62.392116
1935.685756	81.558045	62.397121
1934.908847	77.896487	62.402126
1934.328016	72.613423	62.407130
1933.196683	84.821874	62.412135
1932.757795	80.369887	62.417140
1932.585771	79.961956	62.422145
1931.294338	84.310476	62.427150
1930.536271	77.060046	62.432154
1930.088614	80.642139	62.437159
1929.553793	78.035703	62.442164
1929.531221	80.916285	62.447169
1928.266326	82.079601	62.452174
1927.355691	79.443512	62.457178
1926.463622	87.457383	62.462183
1926.379214	79.042934	62.467188
1926.129046	82.911362	62.472193
1924.669100	83.303999	62.477198
1923.937140	82.432142	62.482202
1923.348865	86.374990	62.487207
1922.868370	83.481771	62.492212
1922.759388	83.407647	62.497217
1922.014795	83.314369	62.502222
1921.445520	74.261320	62.507226
1920.633245	85.583908	62.512231
1919.158073	76.410712	62.517236
1918.715657	85.124471	62.522241
1918.029321	95.049917	62.527246
1917.615584	77.878861	62.532250
1917.042548	83.288648	62.537255
1916.546992	80.009601	62.542260
1915.660604	89.691384	62.547265
1914.401454	82.373131	62.552270
1914.173064	80.301620	62.557274
1913.638798	86.151205	62.562279
1912.995617	87.942347	62.567284
1912.894809	83.341344	62.572289
1911.386662	88.609935	62.577294
1910.634937	80.208995	62.582298
1910.192704	82.524685	62.587303
1909.703433	82.862579	62.592308
1909.134690	88.278344	62.597313
1908.877785	82.557775	62.602318
1908.120035	81.601521	62.607322
1907.365330	85.182067	62.612327
1906.581879	83.759702	62.617332
1905.637932	88.779411	62.622337
1904.537544	97.256805	62.627342
1904.320570	80.011827	62.632346
1904.057414	84.662841	62.637351
1903.492833	84.770472	62.642356
1902.304034	80.731375	62.647361
1901.204987	85.588151	62.652366
1901.103780	77.069215	62.657370
1900.548012	86.092880	62.662375
1900.396558	86.532450	62.667380
1898.882276	76.724136	62.672385
1898.188754	83.483957	62.677390
1897.966724	79.980494	62.682394
1896.718582	83.034429	62.687399
1896.333877	77.548876	62.692404
1895.985152	71.936386	62.697409
1894.762302	87.756013	62.702414
1894.201621	74.549820	62.707418
1893.695367	89.999760	62.712423
1893.213804	83.498185	62.717428
1893.134694	91.198119	62.722433
1892.270299	89.008845	62.727438
1891.172762	77.098790	62.732442
1890.216644	85.057308	62.737447
1890.076127	87.064813	62.742452
1889.760065	79.405234	62.747457
1888.711272	85.518101	62.752462
1887.854619	88.138762	62.757466
1887.116828	78.757719	62.762471
1886.725461	80.160007	62.767476
1885.535226	79.834697	62.772481
1884.463527	80.063823	62.777486
1884.149173	80.674151	62.782490
1884.030207	83.135056	62.787495
1883.652229	81.255315	62.792500
1883.283172	68.610403	62.797505
1882.089344	78.779760	62.802510
1881.462316	65.404937	62.807514
1880.506984	78.397191	62.812519
1880.254204	77.979789	62.817524
1879.503839	73.372686	62.822529
1878.283965	80.232424	62.827534
1878.195733	73.034379	62.832538
1877.369833	78.656762	62.837543
1876.971582	84.449922	62.842548
1875.889248	75.132961	62.847553
1874.881090	80.325887	62.852558
1874.488391	83.784111	62.857562
1873.763071	85.286953	62.862567
1873.720756	87.258711	62.867572
1873.325234	82.374198	62.872577
1872.112513	80.236626	62.877582
1871.667600	79.305406	62.882586
1870.890175	84.515699	62.887591
1869.580910	85.936084	62.892596
1868.786685	86.673509	62.897601
1868.097894	85.380607	62.902606
1867.747041	82.748625	62.907610
1867.788745	86.164504	62.912615
1866.989354	79.446926	62.917620
1866.659174	79.157235	62.922625
1865.949849	83.499333	62.927630
1865.426638	76.769242	62.932634
1864.217875	74.619549	62.937639
1863.131750	75.447965	62.942644
1862.388663	78.610491	62.947649
1861.868136	79.481874	62.952654
1861.582015	87.784435	62.957658
1861.129671	87.225919	62.962663
1860.122057	92.603093	62.967668
1859.589075	82.578749	62.972673
1858.537771	89.837137	62.977678
1858.446151	79.857280	62.982682
1858.079630	93.387076	62.987687
1856.643566	95.132303	62.992692
1856.164096	86.333491	62.997697
1855.260833	90.699298	63.002702
1855.285863	80.210424	63.007706
1854.578227	91.444067	63.012711
1853.750671	82.660601	63.017716
1852.935334	85.873778	63.022721
1851.903902	89.457467	63.027726
1851.868351	80.701521	63.032730
1850.662811	85.938090	63.037735
1849.535860	80.129943	63.042740
1849.217193	77.734816	63.047745
1848.665750	86.424597	63.052750
1848.396349	87.709315	63.057754
1847.746069	88.458825	63.062759
1847.402279	92.094598	63.067764
1846.637150	82.304967	63.072769
1845.601253	93.111239	63.077774
1845.281933	79.418909	63.082778
1844.427262	93.252079	63.087783
1843.600451	89.638545	63.092788
1842.660421	84.590624	63.097793
1842.093003	95.910407	63.102798
1842.148835	84.463405	63.107802
1841.406802	83.485526	63.112807
1839.723600	83.250093	63.117812
1839.861761	78.861623	63.122817
1839.004122	84.526151	63.127822
1838.362059	83.716292	63.132826
1838.023986	80.091378	63.137831
1837.397615	84.313895	63.142836
1837.009160	85.424779	63.147841
1835.580246	84.996243	63.152846
1834.974585	82.812053	63.157850
1834.030435	87.388929	63.162855
1833.772285	83.067867	63.167860
1833.581839	82.715194	63.172865
1832.014904	73.451948	63.177870
1831.581065	79.186856	63.182874
1830.525178	74.534538	63.187879
1829.628052	81.802468	63.192884
1829.638228	79.496732	63.197889
1828.964097	80.844774	63.202894
1829.002748	76.412938	63.207898
1828.298488	74.509293	63.212903
1827.678269	71.563023	63.217908
1827.058199	73.330088	63.222913
1825.940760	77.230849	63.227918
1824.724460	75.197714	63.232922
1824.218353	72.663351	63.237927
1823.485356	68.374986	63.242932
1823.230301	67.597596	63.247937
1822.702814	76.631417	63.252942
1822.500692	70.203623	63.257946
1821.522920	79.503162	63.262951
1820.369327	74.808750	63.267956
1820.142709	72.532082	63.272961
1819.002809	73.437204	63.277966
1818.028693	72.531798	63.282970
1817.334629	83.476152	63.287975
1816.742149	75.526391	63.292980
1816.332732	73.596776	63.297985
1815.966641	78.870112	63.302990
1815.823839	76.860540	63.307994
1815.237730	76.253471	63.312999
1814.011571	75.956034	63.318004
1813.636721	75.861877	63.323009
1812.689195	78.314548	63.328014
1811.577269	80.061562	63.333018
1810.766709	78.537672	63.338023
1810.183659	79.064902	63.343028
1809.897087	69.319326	63.348033
1809.188364	76.511601	63.353038
1809.042260	71.706394	63.358042
1808.730046	74.120233	63.363047
1807.895273	75.974558	63.368052
1806.833422	74.049208	63.373057
1805.451187	73.378625	63.378062
1804.757126	68.532571	63.383066
1804.162604	79.876321	63.388071
1803.965189	77.510187	63.393076
1803.323049	76.838499	63.398081
1802.749553	72.792441	63.403086
1802.596083	74.343102	63.408090
1801.692553	76.631543	63.413095
1800.716452	75.717796	63.418100
1800.544354	72.611572	63.423105
1799.566218	74.830677	63.428110
1798.669571	73.791236	63.433114
1797.581561	79.951874	63.438119
1796.772775	86.227365	63.443124
1796.880107	74.832351	63.448129
1796.099064	85.224769	63.453134
1795.859538	73.592271	63.458138
1794.792616	75.491450	63.463143
1793.779983	78.093416	63.468148
1793.660228	76.902105	63.473153
1793.150675	78.947489	63.478158
1792.147914	71.418051	63.483162
1790.868100	77.866101	63.488167
1790.402237	77.990799	63.493172
1789.978533	83.155183	63.498177
1789.460395	83.380400	63.503182
1789.148426	70.508247	63.508186
1788.892505	83.570703	63.513191
1787.892248	78.349162	63.518196
1787.619369	72.256358	63.523201
1785.960177	74.837509	63.528206
1785.384114	72.578793	63.533210
1784.577823	77.619959	63.538215
1784.060273	75.036639	63.543220
1784.004128	74.010885	63.548225
1782.570713	70.500762	63.553230
1781.576673	71.076211	63.558234
1781.035945	75.274998	63.563239
1780.970005	76.352017	63.568244
1780.120010	74.198590	63.573249
1779.670147	80.170311	63.578254
1779.556638	73.208695	63.583258
1778.654807	74.264532	63.588263
1777.537753	69.002588	63.593268
1777.426182	77.143439	63.598273
1776.170880	89.591398	63.603278
1775.475763	76.927293	63.608282
1774.759024	80.608721	63.613287
1774.156663	84.603328	63.618292
1774.284321	72.195934	63.623297
1773.395126	77.882444	63.628302
1772.031663	80.444972	63.633306
1771.346229	83.058061	63.638311
1770.990553	81.135833	63.643316
1770.615471	75.699965	63.648321
1769.395020	76.256921	63.653326
1768.607117	73.154227	63.658330
1768.135025	78.879103	63.663335
1767.320267	82.143110	63.668340
1767.439938	74.349393	63.673345
1767.010534	85.316356	63.678350
1766.039039	72.359692	63.683354
1765.409027	77.813575	63.688359
1764.380448	83.021457	63.693364
1763.463483	83.665824	63.698369
1762.259832	85.607746	63.703374
1762.225746	78.786876	63.708378
1761.594257	82.493190	63.713383
1761.018436	76.746684	63.718388
1760.612150	68.641928	63.723393
1760.366436	74.585032	63.728398
1759.422263	75.804031	63.733402
1758.541670	67.675041	63.738407
1757.829379	72.561183	63.743412
1757.476514	74.869089	63.748417
1755.567839	78.596574	63.753422
1755.245961	78.440070	63.758426
1754.640232	80.273370	63.763431
1754.273068	69.522030	63.768436
1754.201130	77.880693	63.773441
1753.303974	71.069745	63.778446
1753.061251	74.354685	63.783450
1751.717765	75.825160	63.788455
1751.029014	73.670990	63.793460
1750.744123	70.941291	63.798465
1750.434914	71.334834	63.803470
1749.301298	67.648298	63.808474
1748.686156	66.304526	63.813479
1748.018786	71.516915	63.818484
1747.513373	64.891169	63.823489
1746.140630	79.495049	63.828494
1745.577732	70.738567	63.833498
1744.956994	74.050689	63.838503
1744.545547	71.150022	63.843508
1744.425006	64.606837	63.848513
1743.216594	74.756599	63.853518
1742.306871	62.847232	63.858522
1741.779875	65.819642	63.863527
1741.471638	64.237444	63.868532
1741.247158	58.949494	63.873537
1740.344192	64.148512	63.878542
1739.300242	64.632644	63.883546
1738.950547	67.569191	63.888551
1737.827079	70.890759	63.893556
1736.729169	69.825769	63.898561
1736.162844	77.260909	63.903566
1735.900370	67.365966	63.908570
1735.295038	79.002078	63.913575
1735.055945	76.580320	63.918580
1734.608359	72.471282	63.923585
1732.914268	75.396695	63.928590
1732.709304	69.624633	63.933594
1732.303945	74.118010	63.938599
1731.609488	74.449978	63.943604
1730.812339	68.376235	63.948609
1729.459727	73.042353	63.953614
1729.233373	72.676882	63.958618
1728.604684	71.260039	63.963623
1727.747415	78.106305	63.968628
1727.718444	63.707914	63.973633
1726.810219	72.284665	63.978638
1726.338368	73.072339	63.983642
1725.421738	79.516281	63.988647
1725.065881	87.543018	63.993652
1724.175003	74.222060	63.998657
1722.961822	79.506533	64.003662
1722.787190	73.235091	64.008666
1722.415202	78.379178	64.013671
1721.584818	79.463850	64.018676
1721.006131	68.910151	64.023681
1719.697821	72.698727	64.028686
1719.280335	71.027860	64.033690
1718.716776	83.569815	64.038695
1718.280421	74.551298	64.043700
1718.089274	69.619601	64.048705
1716.654895	78.932151	64.053710
1716.175393	75.019227	64.058714
1715.642434	74.280712	64.063719
1715.168005	77.723717	64.068724
1714.088637	75.772570	64.073729
1713.074802	80.049553	64.078734
1712.633494	70.389678	64.083738
1712.148282	74.618836	64.088743
1711.759718	74.995961	64.093748
1711.391985	67.743527	64.098753
1710.017377	75.023303	64.103758
1709.237740	72.189589	64.108762
1708.838576	73.639009	64.113767
1708.275203	74.101701	64.118772
1708.107632	72.758319	64.123777
1706.724370	78.431487	64.128782
1706.230449	77.121844	64.133786
1705.631308	73.537669	64.138791
1705.246586	78.826431	64.143796
1704.305049	66.611477	64.148801
1702.942129	86.943444	64.153806
1702.611895	79.333289	64.158810
1702.405966	78.308694	64.163815
1702.126407	81.479549	64.168820
1701.677441	74.447848	64.173825
1700.286109	82.840838	64.178830
1699.519618	82.666080	64.183834
1699.190363	76.008614	64.188839
1698.577773	75.091498	64.193844
1697.842260	69.303651	64.198849
1696.712396	79.012498	64.203854
1696.204344	71.424486	64.208858
1696.076367	75.873163	64.213863
1695.088109	74.369832	64.218868
1694.313848	74.398895	64.223873
1693.464127	86.863114	64.228878
1693.394471	77.973291	64.233882
1692.492651	74.590906	64.238887
1691.136149	76.437029	64.243892
1690.714559	78.493420	64.248897
1689.867431	75.129701	64.253902
1689.528891	71.813950	64.258906
1689.198800	73.725215	64.263911
1689.145460	79.891969	64.268916
1688.392825	68.978849	64.273921
1686.976999	79.265950	64.278926
1686.420535	73.887973	64.283930
1685.947710	74.204915	64.288935
1684.929874	76.450568	64.293940
1684.088532	69.895339	64.298945
1683.449084	73.208300	64.303950
1682.830693	77.440513	64.308954
1682.296016	82.118252	64.313959
1682.241244	79.463650	64.318964
1681.999902	76.188500	64.323969
1680.749368	75.874346	64.328974
1680.203740	73.871741	64.333978
1679.615809	73.478938	64.338983
1678.268987	75.026183	64.343988
1677.633555	75.801591	64.348993
1676.830342	82.218632	64.353998
1676.721485	74.531523	64.359002
1676.359420	72.338830	64.364007
1675.172522	79.053226	64.369012
1674.460590	72.559140	64.374017
1673.812381	75.009559	64.379022
1673.357080	68.062235	64.384026
1672.866699	74.819671	64.389031
1671.907779	86.121969	64.394036
1671.233749	73.024042	64.399041
1670.660092	80.147822	64.404046
1670.241038	76.411262	64.409050
1669.002286	84.677495	64.414055
1667.875297	83.019100	64.419060
1667.795367	77.708784	64.424065
1667.230401	80.975056	64.429070
1666.737956	78.720993	64.434074
1666.376994	81.312514	64.439079
1665.984853	84.141072	64.444084
1665.105410	75.308514	64.449089
1664.578212	81.259130	64.454094
1663.403488	74.775163	64.459098
1662.316827	74.508363	64.464103
1661.651267	79.507697	64.469108
1661.633117	81.146909	64.474113
1660.837387	90.274402	64.479118
1660.016306	78.609605	64.484122
1659.022496	79.100173	64.489127
1658.206353	79.162065	64.494132
1657.902274	74.157333	64.499137
1657.399651	82.551404	64.504142
1656.975782	78.599757	64.509146
1655.787233	77.172548	64.514151
1654.692206	81.929600	64.519156
1654.459471	75.569031	64.524161
1653.794151	75.357231	64.529166
1653.587222	82.396152	64.534170
1653.316559	80.725033	64.539175
1652.556994	80.414102	64.544180
1651.591534	77.453124	64.549185
1650.718574	78.421149	64.554190
1650.559626	82.558956	64.559194
1649.540909	78.592266	64.564199
1648.633139	82.366788	64.569204
1647.920772	75.151627	64.574209
1647.376942	77.966671	64.579214
1647.494477	73.378455	64.584218
1645.878941	74.625127	64.589223
1645.434272	79.800600	64.594228
1645.107467	67.961237	64.599233
1644.534527	78.080027	64.604238
1643.283674	76.650853	64.609242
1642.649246	72.247368	64.614247
1641.675327	81.656391	64.619252
1641.617276	70.449559	64.624257
1640.941314	74.228621	64.629262
1640.573606	63.435953	64.634266
1639.194493	72.675505	64.639271
1638.757625	72.438822	64.644276
1638.341946	70.690684	64.649281
1638.009567	74.306744	64.654286
1637.391118	73.076836	64.659290
1635.928430	71.345245	64.664295
1634.996434	74.872477	64.669300
1634.706116	69.806186	64.674305
1634.139803	75.184835	64.679310
1634.121852	74.426484	64.684314
1633.168714	71.772468	64.689319
1632.226321	72.525414	64.694324
1631.820560	80.139125	64.699329
1631.100875	80.270959	64.704334
1630.392544	77.427029	64.709338
1629.443016	88.365371	64.714343
1628.735314	79.082658	64.719348
1628.528539	75.018474	64.724353
1628.053787	75.327462	64.729358
1627.273462	71.553658	64.734362
1626.317007	69.937141	64.739367
1625.137875	78.662497	64.744372
1625.481124	74.958905	64.749377
1624.826081	76.465933	64.754382
1623.047293	74.317144	64.759386
1622.766895	80.715374	64.764391
1621.919169	80.910172	64.769396
1621.591796	71.409624	64.774401
1621.152513	74.895958	64.779406
1620.960421	67.791895	64.784410
1619.817001	73.249569	64.789415
1618.966234	78.475592	64.794420
1618.799920	67.713195	64.799425
1617.984553	72.403839	64.804430
1617.118585	72.996874	64.809434
1616.325089	68.681797	64.814439
1615.244358	79.082084	64.819444
1615.061620	69.936112	64.824449
1614.842661	74.821128	64.829454
1614.373315	66.667586	64.834458
1613.654521	71.571825	64.839463
1612.439914	72.834365	64.844468
1611.827421	67.901366	64.849473
1610.352407	73.960897	64.854478
1609.716062	67.136536	64.859482
1609.965012	67.338650	64.864487
1608.969365	71.645691	64.869492
1608.626705	67.322540	64.874497
1608.112701	81.767637	64.879502
1607.725766	78.410045	64.884506
1606.723741	73.004125	64.889511
1605.921868	74.156563	64.894516
1605.448118	72.368236	64.899521
1604.083308	71.884981	64.904526
1603.343499	70.531380	64.909530
1602.774488	71.396083	64.914535
1602.226513	79.156889	64.919540
1601.751061	60.183551	64.924545
1601.245575	69.588191	64.929550
1601.267395	63.643525	64.934554
1600.645118	69.914739	64.939559
1599.604520	71.621167	64.944564
1599.269256	62.743662	64.949569
1597.982682	77.701477	64.954574
1597.202123	65.444405	64.959578
1596.624222	66.858895	64.964583
1596.030883	76.476724	64.969588
1595.649121	69.621823	64.974593
1594.609476	74.431375	64.979598
1593.967828	75.685073	64.984602
1593.696021	78.222262	64.989607
1592.601862	72.987632	64.994612
1591.446366	76.141032	64.999617
1590.929542	78.142677	65.004622
1590.055946	70.406462	65.009626
1589.466130	71.161443	65.014631
1588.870848	73.960033	65.019636
1588.730640	75.195414	65.024641
1588.167280	76.716361	65.029646
1587.795239	73.580424	65.034650
1586.851118	71.644449	65.039655
1586.339419	72.627630	65.044660
1586.344330	69.554679	65.049665
1584.615869	74.993670	65.054670
1583.999086	80.438985	65.059674
1583.044837	66.588948	65.064679
1582.723819	73.663570	65.069684
1582.461105	66.730669	65.074689
1581.128938	76.916236	65.079694
1580.570071	68.997879	65.084698
1579.893924	62.928725	65.089703
1579.224393	74.290437	65.094708
1579.369497	71.092050	65.099713
1578.738021	80.303137	65.104718
1577.750961	77.043121	65.109722
1576.917977	79.493200	65.114727
1576.351866	81.276713	65.119732
1575.471947	72.521627	65.124737
1574.532821	75.797072	65.129742
1573.819826	72.572652	65.134746
1573.726957	69.398808	65.139751
1572.889332	75.977659	65.144756
1572.453722	69.245656	65.149761
1570.963111	82.222170	65.154766
1570.541509	72.915774	65.159770
1570.277492	76.224491	65.164775
1569.612576	73.131969	65.169780
1569.625062	71.347665	65.174785
1568.439992	73.637352	65.179790
1567.822778	76.321677	65.184794
1567.547268	77.782705	65.189799
1566.222250	74.207916	65.194804
1565.335380	71.694541	65.199809
1564.832532	75.231229	65.204814
1564.192322	79.047204	65.209818
1564.297532	70.596795	65.214823
1562.652068	76.864710	65.219828
1561.966131	70.379620	65.224833
1561.538954	69.288691	65.229838
1561.056035	67.791664	65.234842
1560.648260	66.672548	65.239847
1559.319210	72.533036	65.244852
1559.198935	69.573085	65.249857
1557.926554	75.845438	65.254862
1557.737388	66.590843	65.259866
1556.982346	74.318404	65.264871
1556.068042	71.613156	65.269876
1555.283802	65.750392	65.274881
1554.399371	75.071870	65.279886
1554.089912	68.624583	65.284890
1554.169040	72.902817	65.289895
1553.418185	66.514100	65.294900
1552.904142	66.140245	65.299905
1551.648353	77.712025	65.304910
1551.076019	69.614406	65.309914
1550.713837	67.246096	65.314919
1549.558240	75.248253	65.319924
1549.111524	71.290664	65.324929
1548.469574	73.948831	65.329934
1548.167344	71.043309	65.334938
1547.225752	68.087744	65.339943
1545.904211	73.419211	65.344948
1545.816140	63.159731	65.349953
1545.022642	73.510467	65.354958
1544.695378	70.153329	65.359962
1544.265858	73.076311	65.364967
1542.473294	79.828466	65.369972
1542.287103	62.395569	65.374977
1541.617834	73.724473	65.379982
1541.211435	65.013486	65.384986
1540.818195	67.282128	65.389991
1539.661647	74.173315	65.394996
1538.773199	64.430931	65.400001
1538.371403	69.736034	65.405006
1537.979594	63.585069	65.410010
1537.865658	66.186814	65.415015
1537.000777	67.155053	65.420020
1535.648545	67.525416	65.425025
1535.262189	77.939495	65.430030
1534.879003	68.124451	65.435034
1533.813970	70.479649	65.440039
1532.953655	72.898096	65.445044
1532.321958	58.267385	65.450049
1531.548668	70.962846	65.455054
1531.325722	70.384837	65.460058
1531.030936	75.083496	65.465063
1529.183672	77.855587	65.470068
1529.323605	67.793916	65.475073
1528.310207	77.419298	65.480078
1527.883304	67.367801	65.485082
1528.135384	66.840330	65.490087
1526.424053	68.855767	65.495092
1526.344694	65.725007	65.500097
1525.347467	73.831504	65.505102
1525.242645	72.531073	65.510106
1524.003866	62.613006	65.515111
1522.869537	72.405524	65.520116
1522.892084	66.781643	65.525121
1521.964846	73.914626	65.530126
1520.796645	75.258452	65.535130
1520.207102	66.202250	65.540135
1519.517678	69.562460	65.545140
1519.163217	63.443394	65.550145
1518.517311	71.545417	65.555150
1518.147876	68.450094	65.560154
1517.789280	70.519001	65.565159
1517.341263	73.878946	65.570164
1516.365976	67.173006	65.575169
1515.521165	75.117241	65.580174
1515.056255	73.835415	65.585178
1513.696370	73.343052	65.590183
1513.068064	75.644034	65.595188
1512.846424	75.201192	65.600193
1511.983254	77.551845	65.605198
1511.194871	71.506648	65.610202
1511.124214	75.270934	65.615207
1509.861194	83.750941	65.620212
1509.481491	67.042714	65.625217
1508.731468	80.548506	65.630222
1508.458047	70.214175	65.635226
1507.286734	75.150876	65.640231
1506.379028	74.512442	65.645236
1506.241847	76.747131	65.650241
1505.252270	71.105433	65.655246
1505.220837	71.651964	65.660250
1504.707595	78.464237	65.665255
1502.847537	81.113007	65.670260
1502.548907	73.351823	65.675265
1502.352033	76.873250	65.680270
1502.196982	67.484541	65.685274
1501.037578	67.278381	65.690279
1499.871612	84.606778	65.695284
1499.550235	72.593228	65.700289
1498.848654	86.352828	65.705294
1498.338478	72.970337	65.710298
1497.333576	72.382882	65.715303
1496.563740	80.769399	65.720308
1496.227637	71.908628	65.725313
1495.741240	77.958050	65.730318
1495.171252	73.516326	65.735322
1494.858406	70.486316	65.740327
1493.262793	79.432966	65.745332
1493.036569	74.190332	65.750337
1492.343591	77.052229	65.755342
1491.748586	66.266914	65.760346
1490.730463	72.510364	65.765351
1489.612972	79.772622	65.770356
1489.843583	79.634858	65.775361
1489.544047	77.154386	65.780366
1488.556528	67.501599	65.785370
1487.603816	66.703907	65.790375
1486.779845	71.900094	65.795380
1486.574979	65.026381	65.800385
1486.125506	70.516480	65.805390
1485.043410	73.914693	65.810394
1484.381545	73.187215	65.815399
1483.343752	68.827930	65.820404
1483.250089	62.606603	65.825409
1481.959836	67.285781	65.830414
1481.120247	60.289008	65.835418
1480.718055	64.897895	65.840423
1480.174272	72.513120	65.845428
1479.998945	64.934910	65.850433
1479.750503	67.207981	65.855438
1479.004722	69.985368	65.860442
1477.800180	66.250256	65.865447
1476.843848	80.016744	65.870452
1476.336225	72.821049	65.875457
1475.372843	72.994615	65.880462
1474.789262	74.942961	65.885466
1474.246210	73.633463	65.890471
1473.305620	76.969566	65.895476
1473.415657	68.822273	65.900481
1472.934112	72.889769	65.905486
1471.986615	69.016719	65.910490
1470.954867	71.048878	65.915495
1470.745768	74.703839	65.920500
1470.616836	60.977440	65.925505
1469.305868	71.941330	65.930510
1468.260460	68.491601	65.935514
1467.467903	68.530145	65.940519
1467.235351	70.665109	65.945524
1466.843225	69.051898	65.950529
1465.818129	79.335708	65.955534
1464.986666	69.979885	65.960538
1464.666996	67.092751	65.965543
1463.955479	70.722394	65.970548
1463.478453	73.449836	65.975553
1462.218060	75.293379	65.980558
1461.737533	68.770389	65.985562
1461.353274	65.529195	65.990567
1460.809930	71.505867	65.995572
1459.777910	71.813547	66.000577
1459.054618	71.138427	66.005582
1458.631938	67.854864	66.010586
1458.164822	65.178091	66.015591
1457.368315	75.142917	66.020596
1456.655587	69.225699	66.025601
1455.706117	81.518712	66.030606
1454.924649	74.548305	66.035610
1454.849427	74.723796	66.040615
1454.434442	74.510620	66.045620
1453.614782	67.585436	66.050625
1452.433899	73.833067	66.055630
1451.862450	70.911663	66.060634
1451.267124	70.733697	66.065639
1450.817837	75.787207	66.070644
1449.720596	74.501125	66.075649
1448.764711	68.654343	66.080654
1448.326514	74.767354	66.085658
1448.074372	69.107603	66.090663
1447.370991	78.702429	66.095668
1447.530935	80.850342	66.100673
1445.918602	69.790764	66.105678
1445.342263	71.805764	66.110682
1444.858907	67.909327	66.115687
1444.457126	74.043736	66.120692
1443.416024	68.672178	66.125697
1442.436783	69.183581	66.130702
1441.566761	65.711339	66.135706
1441.551961	67.640881	66.140711
1441.037276	68.949439	66.145716
1440.330104	58.297414	66.150721
1439.162091	62.845156	66.155726
1438.810374	68.607852	66.160730
1438.446975	70.810605	66.165735
1437.457037	78.547199	66.170740
1436.446207	71.040951	66.175745
1435.886740	80.404708	66.180750
1435.395674	66.904498	66.185754
1434.897870	73.334014	66.190759
1434.447035	76.183285	66.195764
1433.824121	75.300338	66.200769
1432.910808	78.287189	66.205774
1432.082595	75.642621	66.210778
1431.774857	69.929232	66.215783
1430.458316	78.286967	66.220788
1429.765972	69.843221	66.225793
1429.010560	70.238160	66.230798
1428.514898	68.609123	66.235802
1428.474186	67.272460	66.240807
1427.788327	64.341830	66.245812
1427.562001	65.604979	66.250817
1426.431441	75.999996	66.255822
1425.831437	74.972608	66.260826
1424.923074	79.521306	66.265831
1423.777877	71.246254	66.270836
1423.242515	67.198071	66.275841
1422.770492	78.407958	66.280846
1422.281552	75.601903	66.285850
1421.811040	78.885576	66.290855
1420.854022	68.719190	66.295860
1420.096737	65.185815	66.300865
1419.344371	73.992482	66.305870
1419.011931	67.536910	66.310874
1418.581939	59.626529	66.315879
1417.777830	75.353972	66.320884
1417.000114	65.435569	66.325889
1416.073667	73.566276	66.330894
1415.542269	70.226331	66.335898
1415.514767	73.598771	66.340903
1414.569373	74.204645	66.345908
1414.004708	61.323332	66.350913
1413.413713	70.473805	66.355918
1412.764860	79.245784	66.360922
1411.703111	67.506611	66.365927
1410.553036	79.240700	66.370932
1410.315213	69.212515	66.375937
1409.525205	71.041472	66.380942
1409.306550	66.405025	66.385946
1408.622824	69.896897	66.390951
1406.802742	66.009811	66.395956
1406.848962	71.552426	66.400961
1406.144997	69.274605	66.405966
1405.934616	77.394450	66.410970
1406.135622	69.768802	66.415975
1404.283846	75.240399	66.420980
1404.088774	65.695930	66.425985
1403.513156	74.172752	66.430990
1402.540787	75.767279	66.435994
1401.947735	77.915797	66.440999
1401.154277	77.937928	66.446004
1400.444175	72.741817	66.451009
1399.212181	72.842566	66.456014
1398.309819	67.287016	66.461018
1398.383642	71.648249	66.466023
1397.392131	74.815456	66.471028
1397.476576	71.345624	66.476033
1396.945289	65.331444	66.481038
1396.207251	70.373200	66.486042
1395.249687	61.409627	66.491047
1394.625072	75.457212	66.496052
1393.933265	65.967774	66.501057
1393.610016	72.272284	66.506062
1392.403470	74.412927	66.511066
1391.814044	70.096910	66.516071
1390.800583	65.369948	66.521076
1390.637740	66.410662	66.526081
1389.910210	71.349178	66.531086
1389.145397	62.764699	66.536090
1388.217799	64.012895	66.541095
1387.581458	77.098980	66.546100
1387.221961	72.078504	66.551105
1386.477011	64.649518	66.556110
1386.156152	78.491959	66.561114
1385.453504	71.290982	66.566119
1384.228966	73.169850	66.571124
1384.217380	69.180824	66.576129
1383.438156	70.270209	66.581134
1382.916356	68.073705	66.586138
1382.189194	76.525155	66.591143
1381.018164	73.835074	66.596148
1380.585700	74.712741	66.601153
1379.916006	73.807020	66.606158
1379.729868	76.099824	66.611162
1378.595915	73.185906	66.616167
1377.477883	77.271575	66.621172
1377.433019	72.718271	66.626177
1376.971963	72.713899	66.631182
1376.288574	71.544088	66.636186
1375.303966	68.335015	66.641191
1374.492114	77.132133	66.646196
1374.327160	62.599585	66.651201
1373.434765	62.476032	66.656206
1372.429465	72.645146	66.661210
1371.995998	60.810285	66.666215
1371.208140	75.967341	66.671220
1370.654930	69.531014	66.676225
1370.057299	75.846969	66.681230
1369.765080	73.634455	66.686234
1369.305699	73.714267	66.691239
1368.111932	74.871852	66.696244
1367.623968	67.746231	66.701249
1366.561251	69.104794	66.706254
1365.749429	65.245649	66.711258
1365.441161	62.767475	66.716263
1364.600362	61.885126	66.721268
1364.306210	64.652713	66.726273
1363.804784	70.373540	66.731278
1363.078371	72.519628	66.736282
1362.299993	65.078213	66.741287
1361.430344	70.022112	66.746292
1361.550869	61.038205	66.751297
1360.356676	72.923919	66.756302
1358.930340	68.551443	66.761306
1358.529390	67.313551	66.766311
1358.351082	78.786170	66.771316
1357.630301	74.045427	66.776321
1356.327013	75.043350	66.781326
1355.940905	71.360004	66.786330
1355.671428	66.316229	66.791335
1355.115892	71.101758	66.796340
1354.861319	77.432802	66.801345
1353.513574	71.378003	66.806350
1352.324595	68.805076	66.811354
1352.222621	66.829985	66.816359
1351.829559	76.863117	66.821364
1351.318441	70.931933	66.826369
1350.294556	77.972142	66.831374
1349.624325	78.673418	66.836378
1349.286916	67.373930	66.841383
1347.723061	77.769711	66.846388
1347.004859	75.761166	66.851393
1346.753361	69.258196	66.856398
1346.639707	78.812072	66.861402
1346.221138	67.191756	66.866407
1345.247556	71.206125	66.871412
1343.829930	63.053130	66.876417
1343.147440	76.696956	66.881422
1342.885951	79.731310	66.886426
1342.474168	70.230260	66.891431
1341.965085	69.425729	66.896436
1341.822314	71.580062	66.901441
1340.368889	69.234767	66.906446
1339.706407	78.602738	66.911450
1339.046281	70.789783	66.916455
1338.543339	76.713364	66.921460
1337.384761	68.772196	66.926465
1336.921549	74.739104	66.931470
1336.229726	76.942429	66.936474
1336.151521	74.450134	66.941479
1335.222664	75.752238	66.946484
1334.168462	71.837883	66.951489
1333.685247	65.844299	66.956494
1333.307881	65.307339	66.961498
1333.254036	72.644891	66.966503
1331.681069	69.041175	66.971508
1330.786121	63.337538	66.976513
1330.177183	73.324731	66.981518
1329.341699	68.529029	66.986522
1329.045921	68.942795	66.991527
1328.658865	74.691018	66.996532
1328.016016	79.046256	67.001537
1326.596497	67.469799	67.006542
1326.194043	71.562445	67.011546
1325.920912	67.868052	67.016551
1325.438583	71.175067	67.021556
1324.439707	69.042872	67.026561
1323.289080	67.766748	67.031566
1322.733854	69.689334	67.036570
1322.553209	72.027774	67.041575
1321.698017	71.507879	67.046580
1321.691393	71.263490	67.051585
1320.927377	79.644679	67.056590
1319.893717	75.571291	67.061594
1319.266345	70.784173	67.066599
1318.583551	80.889404	67.071604
1318.095193	74.542636	67.076609
1317.316220	64.099106	67.081614
1316.560354	78.111925	67.086618
1316.192975	69.233250	67.091623
1315.215076	74.764871	67.096628
1314.440418	65.325555	67.101633
1313.606424	71.168840	67.106638
1313.322112	71.575118	67.111642
1313.132724	72.246974	67.116647
1311.974622	77.907336	67.121652
1310.958582	74.664975	67.126657
1310.232898	83.323802	67.131662
1309.703894	75.669581	67.136666
1309.508526	82.382840	67.141671
1309.109848	85.188061	67.146676
1308.446605	73.130051	67.151681
1307.533105	82.740725	67.156686
1306.791102	83.453108	67.161690
1306.152186	82.570154	67.166695
1304.976974	84.694401	67.171700
1304.215329	75.874930	67.176705
1303.823664	84.832219	67.181710
1303.457586	90.983812	67.186714
1303.340594	77.679312	67.191719
1302.232563	77.148234	67.196724
1301.301001	72.282936	67.201729
1300.503681	78.414012	67.206734
1299.969783	79.225369	67.211738
1300.117855	75.718200	67.216743
1298.498428	87.676728	67.221748
1297.712616	76.993587	67.226753
1297.679092	76.246194	67.231758
1296.797756	79.676386	67.236762
1296.489809	76.788048	67.241767
1294.915380	78.011606	67.246772
1294.462580	73.668662	67.251777
1294.213378	84.368321	67.256782
1293.609217	85.627478	67.261786
1293.093202	79.097166	67.266791
1291.980840	83.650017	67.271796
1291.184425	77.842678	67.276801
1290.601629	78.749246	67.281806
1290.331088	75.204799	67.286810
1289.850432	74.929066	67.291815
1288.760343	80.068603	67.296820
1288.332032	87.225144	67.301825
1287.688247	79.216382	67.306830
1286.911159	77.127142	67.311834
1285.932777	74.472391	67.316839
1284.928085	80.955535	67.321844
1285.129105	77.991906	67.326849
1284.703881	83.005386	67.331854
1283.908533	79.926161	67.336858
1283.065764	77.070965	67.341863
1281.601832	85.365150	67.346868
1281.603354	76.328195	67.351873
1281.063531	88.136638	67.356878
1280.091631	82.948263	67.361882
1279.840136	75.554024	67.366887
1278.501968	87.852414	67.371892
1278.156097	73.423475	67.376897
1277.727656	71.336521	67.381902
1277.532934	73.392385	67.386906
1276.263399	73.901414	67.391911
1275.301966	83.524244	67.396916
1275.175171	82.157322	67.401921
1274.186613	76.767338	67.406926
1273.866188	82.577970	67.411930
1273.024145	75.930987	67.416935
1272.045427	92.792365	67.421940
1271.230725	75.161208	67.426945
1271.249379	82.695944	67.431950
1270.709847	81.586384	67.436954
1269.745525	77.319963	67.441959
1268.736746	80.128585	67.446964
1268.540048	73.214024	67.451969
1267.905086	77.129779	67.456974
1266.670051	76.826494	67.461978
1266.296937	74.815723	67.466983
1264.732151	78.660148	67.471988
1264.804640	80.401068	67.476993
1264.344186	79.178503	67.481998
1264.046301	79.920249	67.487002
1263.963786	73.056795	67.492007
1262.722030	85.095138	67.497012
1261.969599	81.517144	67.502017
1261.615096	81.568354	67.507022
1260.291436	79.809128	67.512026
1259.645438	74.013939	67.517031
1258.956167	81.585401	67.522036
1258.609861	74.688558	67.527041
1258.371885	76.538286	67.532046
1257.023977	78.183316	67.537050
1256.684941	70.621315	67.542055
1255.610339	74.431556	67.547060
1255.311106	68.425037	67.552065
1254.616255	74.030965	67.557070
1253.771094	79.705258	67.562074
1253.359869	70.512799	67.567079
1252.649844	77.042203	67.572084
1252.167575	80.893926	67.577089
1250.738169	83.501814	67.582094
1250.521549	78.675961	67.587098
1250.120064	70.847165	67.592103
1249.481782	81.260947	67.597108
1248.424456	76.016947	67.602113
1247.682998	79.714500	67.607118
1247.008614	76.431029	67.612122
1246.484303	74.486801	67.617127
1246.204081	76.172848	67.622132
1245.425995	75.339385	67.627137
1244.189605	73.327603	67.632142
1243.523284	70.368396	67.637146
1242.965604	67.766361	67.642151
1242.491900	80.856180	67.647156
1242.255990	76.300855	67.652161
1241.673009	75.971202	67.657166
1240.203516	80.570994	67.662170
1239.510400	70.631046	67.667175
1239.077991	77.375410	67.672180
1238.929175	66.691388	67.677185
1238.300983	71.492915	67.682190
1237.211784	74.197685	67.687194
1236.694004	68.770532	67.692199
1235.804374	77.249017	67.697204
1235.806203	73.275462	67.702209
1234.761247	64.126380	67.707214
1233.671602	73.787341	67.712218
1233.234854	67.975281	67.717223
1233.217655	71.500286	67.722228
1232.512115	74.417648	67.727233
1231.703099	70.780275	67.732238
1230.379854	66.605314	67.737242
1230.368806	73.592127	67.742247
1229.000628	73.563477	67.747252
1228.249433	73.868912	67.752257
1227.523308	68.330596	67.757262
1227.328716	71.377575	67.762266
1226.792273	67.337502	67.767271
1226.199075	74.901987	67.772276
1225.769860	72.864116	67.777281
1225.133216	72.879557	67.782286
1223.704861	71.394044	67.787290
1223.697015	73.449492	67.792295
1222.528986	72.430965	67.797300
1222.542696	68.235125	67.802305
1221.623979	71.741985	67.807310
1220.333692	75.475875	67.812314
1220.143511	72.054249	67.817319
1219.835904	75.680288	67.822324
1219.030822	64.998897	67.827329
1217.575057	67.661828	67.832334
1217.137145	69.801169	67.837338
1216.852738	63.119519	67.842343
1215.878824	72.569229	67.847348
1216.326752	72.316092	67.852353
1215.494579	59.486552	67.857358
1214.503976	71.372948	67.862362
1213.610234	67.338394	67.867367
1211.950065	78.846824	67.872372
1212.079676	71.879956	67.877377
1211.311476	75.600642	67.882382
1210.288741	77.950238	67.887386
1210.097537	62.707776	67.892391
1209.537018	72.728520	67.897396
1209.528961	71.153388	67.902401
1208.738681	72.826900	67.907406
1207.715004	78.802538	67.912410
1207.356437	72.390149	67.917415
1206.542343	70.328575	67.922420
1205.402498	59.145191	67.927425
1204.708774	71.413370	67.932430
1203.989965	67.269134	67.937434
1204.259820	58.647286	67.942439
1203.321277	61.532703	67.947444
1202.379299	58.785298	67.952449
1201.778822	64.316256	67.957454
1201.005566	67.781241	67.962458
1200.265291	59.374968	67.967463
1198.862145	65.868314	67.972468
1198.175662	64.903918	67.977473
1198.202109	64.386249	67.982478
1197.802957	65.435849	67.987482
1197.332712	66.002250	67.992487
1196.930486	73.323654	67.997492
1196.038071	63.175882	68.002497
1195.066635	66.379154	68.007502
1194.310676	66.536601	68.012506
1194.016113	58.366241	68.017511
1192.774269	65.673113	68.022516
1191.878177	62.619052	68.027521
1191.294268	58.941570	68.032526
1190.671365	63.394447	68.037530
1190.630469	63.767343	68.042535
1190.055163	67.014894	68.047540
1189.484512	60.633298	68.052545
1188.429790	64.792627	68.057550
1187.692572	71.061439	68.062554
1187.512651	58.636524	68.067559
1186.826573	69.660032	68.072564
1185.771091	54.315310	68.077569
1185.288402	59.594006	68.082574
1184.461815	72.941988	68.087578
1183.946183	65.094067	68.092583
1182.763143	66.123153	68.097588
1182.310910	65.659021	68.102593
1181.609565	73.845547	68.107598
1181.429679	63.795246	68.112602
1181.031441	65.248092	68.117607
1179.659692	65.911612	68.122612
1178.919818	57.072273	68.127617
1178.567149	58.498764	68.132622
1177.610665	64.744330	68.137626
1177.495430	65.616642	68.142631
1176.678672	64.005509	68.147636
1175.990540	56.033979	68.152641
1175.246794	65.094560	68.157646
1174.306093	65.551654	68.162650
1174.538748	55.103900	68.167655
1173.173156	58.283086	68.172660
1172.525890	48.996470	68.177665
1171.907680	59.374830	68.182670
1171.226662	62.497987	68.187674
1171.010558	61.187019	68.192679
1169.467910	57.578172	68.197684
1168.850948	64.226242	68.202689
1168.430473	61.284163	68.207694
1167.793072	64.766151	68.212698
1168.023282	58.857672	68.217703
1166.704167	57.552411	68.222708
1165.934704	61.541724	68.227713
1165.567891	56.665026	68.232718
1164.993336	69.878673	68.237722
1164.224638	58.129282	68.242727
1163.413668	68.998524	68.247732
1162.734589	64.557377	68.252737
1162.338221	54.975577	68.257742
1161.379382	59.275195	68.262746
1160.580025	50.433023	68.267751
1159.673244	59.139824	68.272756
1159.232565	59.353420	68.277761
1158.900308	64.169805	68.282766
1158.020503	64.019267	68.287770
1157.637828	54.140270	68.292775
1156.828958	64.049592	68.297780
1156.407671	62.339172	68.302785
1155.559488	62.013887	68.307790
1154.587740	67.064498	68.312794
1154.324311	64.095531	68.317799
1152.935307	67.388858	68.322804
1152.536161	61.929568	68.327809
1152.374353	65.843258	68.332814
1151.271649	63.631385	68.337818
1150.531288	55.142251	68.342823
1149.902266	62.185919	68.347828
1149.212070	60.036041	68.352833
1148.809008	61.327486	68.357838
1148.495004	64.632135	68.362842
1148.274245	51.311506	68.367847
1146.796378	63.333434	68.372852
1146.223144	59.661630	68.377857
1145.731793	59.119336	68.382862
1144.556910	66.706053	68.387866
1144.153137	65.019871	68.392871
1143.355725	71.642793	68.397876
1142.922153	64.171206	68.402881
1142.500174	67.386192	68.407886
1141.342548	73.843829	68.412890
1140.680917	65.982233	68.417895
1140.321547	69.814889	68.422900
1139.292942	59.499017	68.427905
1139.299095	67.027585	68.432910
1138.245647	67.439257	68.437914
1137.530121	62.629374	68.442919
1136.723610	65.833626	68.447924
1136.329903	65.890373	68.452929
1135.896210	69.467347	68.457934
1134.641490	67.707011	68.462938
1134.505908	62.576392	68.467943
1133.773003	72.070496	68.472948
1133.256108	69.015857	68.477953
1132.520621	68.325507	68.482958
1131.320142	70.333726	68.487962
1130.810911	64.583434	68.492967
1130.160988	76.962138	68.497972
1129.819500	57.844435	68.502977
1128.658746	66.060283	68.507982
1127.410443	64.362795	68.512986
1127.761146	65.012044	68.517991
1127.357653	67.754546	68.522996
1126.726460	61.967115	68.528001
1126.242467	64.340919	68.533006
1125.032741	66.156522	68.538010
1124.695050	60.963805	68.543015
1123.888668	71.917919	68.548020
1122.896012	63.811444	68.553025
1121.680250	63.603576	68.558030
1121.060570	63.251802	68.563034
1121.090532	55.336529	68.568039
1120.479371	72.099426	68.573044
1120.189771	69.772016	68.578049
1119.593967	68.671716	68.583054
1118.608647	74.832630	68.588058
1118.162947	64.309194	68.593063
1117.419727	59.310252	68.598068
1116.010317	62.359200	68.603073
1115.496760	68.104612	68.608078
1115.053338	73.442509	68.613082
1114.471391	63.502114	68.618087
1114.269613	73.548664	68.623092
1113.144661	71.468892	68.628097
1112.277100	62.975492	68.633102
1111.742708	72.302191	68.638106
1111.318774	65.976797	68.643111
1110.729080	70.733455	68.648116
1109.976461	68.014825	68.653121
1109.310771	61.803458	68.658126
1108.185931	71.044952	68.663130
1108.221092	64.677262	68.668135
1107.042911	70.374251	68.673140
1105.863373	69.154049	68.678145
1105.695951	65.721036	68.683150
1104.867490	66.778236	68.688154
1104.911629	60.104684	68.693159
1104.135652	67.105233	68.698164
1103.192600	63.865820	68.703169
1102.403414	66.516084	68.708174
1101.972945	69.923964	68.713178
1101.618545	64.288473	68.718183
1100.876782	66.452615	68.723188
1100.184587	69.790053	68.728193
1099.327413	69.142648	68.733198
1098.515743	64.827239	68.738202
1098.378864	56.224519	68.743207
1097.099614	67.890754	68.748212
1096.048251	53.186383	68.753217
1095.586330	61.000347	68.758222
1095.048855	65.199800	68.763226
1094.889855	62.438340	68.768231
1094.443672	69.094276	68.773236
1093.884390	66.009403	68.778241
1092.741192	67.915853	68.783246
1092.017866	69.637519	68.788250
1091.386311	67.448399	68.793255
1090.140707	71.158087	68.798260
1089.438153	64.507793	68.803265
1089.215236	71.371013	68.808270
1088.828298	75.026428	68.813274
1088.362445	70.210904	68.818279
1088.110546	73.529000	68.823284
1086.835708	70.117861	68.828289
1086.371673	70.572688	68.833294
1085.276309	70.137380	68.838298
1084.341287	59.834710	68.843303
1083.514903	61.560602	68.848308
1083.142711	62.469810	68.853313
1083.233378	59.300881	68.858318
1082.311458	67.074017	68.863322
1082.322238	51.270453	68.868327
1081.249028	64.722631	68.873332
1080.266607	66.161444	68.878337
1078.989373	65.376378	68.883342
1077.899078	76.423322	68.888346
1078.119349	70.417467	68.893351
1077.254320	70.227311	68.898356
1076.590629	64.676758	68.903361
1076.136157	54.107473	68.908366
1075.396756	59.377635	68.913370
1075.356654	66.602686	68.918375
1074.413154	65.276945	68.923380
1073.655383	62.777879	68.928385
1073.205026	70.761570	68.933390
1072.280804	69.328323	68.938394
1071.084144	61.440341	68.943399
1070.453453	71.870582	68.948404
1070.095198	64.153227	68.953409
1070.014069	62.722841	68.958414
1069.413334	70.753202	68.963418
1068.466433	63.751616	68.968423
1067.171394	71.377869	68.973428
1066.699588	69.947280	68.978433
1066.452970	66.557041	68.983438
1065.679754	67.852274	68.988442
1064.849429	62.503934	68.993447
1063.868285	70.118670	68.998452
1062.744776	68.503246	69.003457
1062.874425	66.679547	69.008462
1062.167981	71.120690	69.013466
1062.243649	64.437398	69.018471
1061.322025	66.888121	69.023476
1060.593464	60.254919	69.028481
1059.875455	54.961162	69.033486
1059.135588	64.179760	69.038490
1058.188229	56.986031	69.043495
1057.343943	64.021964	69.048500
1056.699539	70.366467	69.053505
1056.607643	61.411063	69.058510
1056.043983	65.338700	69.063514
1055.266867	61.371840	69.068519
1054.384566	68.584802	69.073524
1054.141035	72.385783	69.078529
1053.483309	68.802667	69.083534
1052.106813	70.709999	69.088538
1051.816815	64.317472	69.093543
1050.809950	70.164729	69.098548
1050.742846	67.758569	69.103553
1049.527752	67.918086	69.108558
1048.721599	74.556329	69.113562
1048.114268	63.282993	69.118567
1047.503228	79.304199	69.123572
1047.316103	74.791064	69.128577
1046.759720	68.824659	69.133582
1045.357574	69.756697	69.138586
1044.754173	63.421786	69.143591
1044.105391	62.168735	69.148596
1043.840706	63.683189	69.153601
1043.711699	65.695041	69.158606
1042.775323	70.984336	69.163610
1041.642672	64.688742	69.168615
1041.290308	70.729828	69.173620
1040.609645	71.117550	69.178625
1040.244452	65.423919	69.183630
1038.285050	70.924715	69.188634
1038.161037	62.152041	69.193639
1037.486393	71.401710	69.198644
1037.177397	73.410045	69.203649
1037.144734	64.542388	69.208654
1036.234466	75.597584	69.213658
1035.188779	68.301095	69.218663
1034.923255	71.872959	69.223668
1034.219790	64.151966	69.228673
1032.993220	65.314060	69.233678
1031.959004	76.068787	69.238682
1031.824817	61.292234	69.243687
1030.898113	66.277519	69.248692
1030.662742	61.628579	69.253697
1030.477324	65.390793	69.258702
1029.666583	73.791840	69.263706
1028.983478	60.868543	69.268711
1027.982056	70.461920	69.273716
1027.127922	69.392845	69.278721
1026.328025	67.628859	69.283726
1025.368489	70.690392	69.288730
1025.073615	65.952172	69.293735
1024.685393	68.979418	69.298740
1024.375625	71.225111	69.303745
1023.807727	65.535011	69.308750
1022.589895	69.191802	69.313754
1022.036272	66.610813	69.318759
1021.432213	76.212327	69.323764
1020.647368	70.811603	69.328769
1019.777303	67.834432	69.333774
1018.901074	71.787970	69.338778
1018.878962	61.963295	69.343783
1018.158293	66.509503	69.348788
1017.880428	67.511899	69.353793
1016.638256	66.545986	69.358798
1015.697236	71.835291	69.363802
1015.269954	67.141851	69.368807
1014.839501	69.026519	69.373812
1014.708731	76.034214	69.378817
1013.538657	69.644777	69.383822
1012.481141	72.416002	69.388826
1012.092928	70.557439	69.393831
1011.597704	72.892520	69.398836
1011.019152	69.633730	69.403841
1010.041426	70.254688	69.408846
1009.420534	78.400606	69.413850
1009.213758	69.934590	69.418855
1007.905739	70.284890	69.423860
1006.895920	71.795905	69.428865
1006.408063	67.580185	69.433870
1005.445948	76.721596	69.438874
1006.001679	63.882188	69.443879
1005.547184	68.722667	69.448884
1004.465506	65.085459	69.453889
1004.147379	63.698029	69.458894
1003.371465	68.679205	69.463898
1001.895387	64.953626	69.468903
1001.164288	73.486292	69.473908
1000.790919	69.550161	69.478913
1000.459204	59.846400	69.483918
999.657241	68.480405	69.488922
998.516769	66.434897	69.493927
997.725799	70.908679	69.498932
997.431299	75.055478	69.503937
996.935902	63.699831	69.508942
996.536408	73.347228	69.513946
996.224279	72.154945	69.518951
994.752627	64.631828	69.523956
994.223795	65.127363	69.528961
993.878127	66.356492	69.533966
992.560146	64.653211	69.538970
991.764710	71.503165	69.543975
991.163485	69.998041	69.548980
990.893775	76.143390	69.553985
990.365294	73.789008	69.558990
989.779321	75.918196	69.563994
989.464464	73.239482	69.568999
988.373167	77.800223	69.574004
987.397178	74.929615	69.579009
986.973481	72.637416	69.584014
986.454411	68.201661	69.589018
986.113106	63.728753	69.594023
984.822514	67.724442	69.599028
983.872764	65.391684	69.604033
983.736346	63.594604	69.609038
983.036766	72.719474	69.614042
982.423786	64.668801	69.619047
981.658482	68.048770	69.624052
981.097157	69.758494	69.629057
980.252584	62.472580	69.634062
979.906385	67.041499	69.639066
979.586397	63.949609	69.644071
978.102432	68.363659	69.649076
977.469000	62.254157	69.654081
977.285242	66.804336	69.659086
976.548493	67.700593	69.664090
975.840886	62.374281	69.669095
974.527178	68.649869	69.674100
973.981659	73.582119	69.679105
973.716417	65.105203	69.684110
972.975980	65.169240	69.689114
972.822944	70.205187	69.694119
972.193492	65.743340	69.699124
970.845884	64.478538	69.704129
970.494203	56.042877	69.709134
970.028300	69.525264	69.714138
969.279270	62.580998	69.719143
968.446902	66.599658	69.724148
967.425077	71.981356	69.729153
967.291066	58.746947	69.734158
966.529568	67.409943	69.739162
966.218468	69.406798	69.744167
964.965264	67.698747	69.749172
964.580608	66.727299	69.754177
964.069087	66.090193	69.759182
963.643654	75.289293	69.764186
962.575592	64.610382	69.769191
962.017606	66.021131	69.774196
961.176139	66.968086	69.779201
960.604792	62.942321	69.784206
959.415251	71.121681	69.789210
958.756973	69.020442	69.794215
957.986226	64.695686	69.799220
957.469484	68.617269	69.804225
957.689370	72.356254	69.809230
957.061909	72.205955	69.814234
956.987398	66.581756	69.819239
955.690211	66.956661	69.824244
954.882894	73.614452	69.829249
954.676559	63.129395	69.834254
953.187196	62.264646	69.839258
953.204512	63.651075	69.844263
951.976545	70.543530	69.849268
951.065934	57.963942	69.854273
949.924413	54.915258	69.859278
949.523804	55.618168	69.864282
949.107412	62.765161	69.869287
948.629404	74.622997	69.874292
947.867337	62.767533	69.879297
947.921002	54.732168	69.884302
946.747074	66.676422	69.889306
946.168626	60.276472	69.894311
945.337262	64.787569	69.899316
944.643734	61.584401	69.904321
944.189677	57.541316	69.909326
942.936679	76.203379	69.914330
942.461375	62.491397	69.919335
941.897660	64.625854	69.924340
941.009630	64.287695	69.929345
941.125675	59.314909	69.934350
940.526912	65.928692	69.939354
939.656326	69.683916	69.944359
939.031866	68.946161	69.949364
938.215502	67.284480	69.954369
937.210379	67.103343	69.959374
936.290622	65.356743	69.964378
935.888277	63.664812	69.969383
935.321213	64.543461	69.974388
934.811410	68.434253	69.979393
934.756164	65.195583	69.984398
933.631201	74.331339	69.989402
932.958013	50.280895	69.994407
932.342543	66.953728	69.999412
931.383430	63.931831	70.004417
930.923116	67.244966	70.009422
929.899332	74.306526	70.014426
929.549199	63.325863	70.019431
928.909169	65.784429	70.024436
928.585507	67.028345	70.029441
927.716957	63.357418	70.034446
926.722544	73.041575	70.039450
926.164925	65.290101	70.044455
925.682148	76.815614	70.049460
924.884265	66.082153	70.054465
924.089970	61.189493	70.059470
923.261605	71.535570	70.064474
922.628116	67.819648	70.069479
922.048930	67.969359	70.074484
921.656966	67.581373	70.079489
921.615425	61.134470	70.084494
920.267226	71.966268	70.089498
919.929833	67.955305	70.094503
919.109973	69.146054	70.099508
917.734368	69.446772	70.104513
917.277655	63.573053	70.109518
916.471648	75.751525	70.114522
916.110695	65.668724	70.119527
915.370645	69.289495	70.124532
915.292756	67.442921	70.129537
914.957257	68.384934	70.134542
913.674062	76.193521	70.139546
912.886457	63.816283	70.144551
912.388569	64.963335	70.149556
912.135493	62.182080	70.154561
910.910823	57.902317	70.159566
910.076521	66.145175	70.164570
909.592742	65.488325	70.169575
909.198721	70.594358	70.174580
908.855381	70.956296	70.179585
908.000636	60.360471	70.184590
906.752208	64.508420	70.189594
906.348130	63.449124	70.194599
905.975738	65.498320	70.199604
904.782361	64.015290	70.204609
904.455760	56.095186	70.209614
903.600135	64.813777	70.214618
903.451772	69.135273	70.219623
903.102330	68.215033	70.224628
901.923486	74.928568	70.229633
901.416240	67.119526	70.234638
900.095814	68.135103	70.239642
900.102310	64.819153	70.244647
898.788576	69.232882	70.249652
897.942252	64.223224	70.254657
897.533851	65.799006	70.259662
897.107890	71.929274	70.264666
896.718564	65.373787	70.269671
896.191391	66.690848	70.274676
895.303703	66.659728	70.279681
894.202831	58.982757	70.284686
893.520906	72.627661	70.289690
893.430059	68.536581	70.294695
893.103100	72.538949	70.299700
892.184291	68.813087	70.304705
891.443740	68.753215	70.309710
890.803964	71.031751	70.314714
890.064881	62.237737	70.319719
889.066128	66.978816	70.324724
888.393048	69.908023	70.329729
887.700414	63.190156	70.334734
887.154030	75.705458	70.339738
886.434169	69.119352	70.344743
885.407202	70.358999	70.349748
884.965651	75.524487	70.354753
885.060812	70.830394	70.359758
883.973245	74.641342	70.364762
883.859442	64.692260	70.369767
882.909741	70.339497	70.374772
881.726046	75.186068	70.379777
881.372789	68.037066	70.384782
880.651576	75.767956	70.389786
880.015493	72.348523	70.394791
879.060191	75.243968	70.399796
878.210752	78.635994	70.404801
878.169706	68.799574	70.409806
877.800429	72.816294	70.414810
876.960076	71.626077	70.419815
875.952347	71.566971	70.424820
875.497567	76.931296	70.429825
875.028112	57.770849	70.434830
873.681053	69.012567	70.439834
872.750624	65.016741	70.444839
872.460515	73.764394	70.449844
871.965842	69.889711	70.454849
871.463591	74.761270	70.459854
870.907245	73.471886	70.464858
870.399276	67.938119	70.469863
869.410197	72.674388	70.474868
868.137016	76.504895	70.479873
868.037325	61.046710	70.484878
867.510358	70.145176	70.489882
867.225862	72.251947	70.494887
866.224914	66.105155	70.499892
865.324265	63.724541	70.504897
864.763605	55.963737	70.509902
864.105813	71.679529	70.514906
863.827344	71.342368	70.519911
862.391357	73.154945	70.524916
861.967975	73.086935	70.529921
861.586549	63.773007	70.534926
860.800665	72.717674	70.539930
860.585896	65.764419	70.544935
859.620484	62.486262	70.549940
858.697561	63.404556	70.554945
858.170563	70.258671	70.559950
857.644715	66.439065	70.564954
857.152223	66.966283	70.569959
855.867362	71.565725	70.574964
855.318717	72.040591	70.579969
854.716015	69.522898	70.584974
854.325212	67.599272	70.589978
853.799905	61.529297	70.594983
852.681353	68.474472	70.599988
852.018543	63.373394	70.604993
851.618110	64.221538	70.609998
851.004027	64.239084	70.615002
850.836670	63.927100	70.620007
849.845822	67.965816	70.625012
848.965175	63.649249	70.630017
848.567166	62.605102	70.635022
847.443475	65.395980	70.640026
846.809489	69.118190	70.645031
846.258156	70.085728	70.650036
845.248288	69.344531	70.655041
845.513099	60.488704	70.660046
844.412378	70.108580	70.665050
843.521324	69.450448	70.670055
842.833815	68.669824	70.675060
842.157983	67.260392	70.680065
842.208239	67.645702	70.685070
840.819239	76.743017	70.690074
840.131465	68.332176	70.695079
839.355659	70.596914	70.700084
838.733956	72.166608	70.705089
838.479784	66.618584	70.710094
837.923589	70.807446	70.715098
837.486602	69.715901	70.720103
836.255332	69.931922	70.725108
835.806143	72.287156	70.730113
835.588923	67.727093	70.735118
834.194772	78.670196	70.740122
833.305610	74.820853	70.745127
832.791966	76.520058	70.750132
832.424681	74.198083	70.755137
832.484209	69.059724	70.760142
831.176102	74.389038	70.765146
830.335858	71.031028	70.770151
829.681474	75.335389	70.775156
829.261097	69.545059	70.780161
828.963419	73.209667	70.785166
827.869559	73.231242	70.790170
827.115487	77.163883	70.795175
826.459935	69.737870	70.800180
825.529678	71.807630	70.805185
825.424051	62.566462	70.810190
824.331693	77.079392	70.815194
823.581881	65.247915	70.820199
823.085007	66.682944	70.825204
822.566470	68.356935	70.830209
822.167470	66.811276	70.835214
821.179962	76.167043	70.840218
820.187082	69.772971	70.845223
820.031687	67.634562	70.850228
819.504912	70.137290	70.855233
818.960463	70.618151	70.860238
817.455040	73.427451	70.865242
817.306633	74.703324	70.870247
816.621308	68.593661	70.875252
816.141063	71.172889	70.880257
815.203798	67.288372	70.885262
813.753844	76.854793	70.890266
813.729042	72.521101	70.895271
813.152167	68.013567	70.900276
812.500694	68.966685	70.905281
812.488718	62.659586	70.910286
811.583064	72.536960	70.915290
810.945053	71.929037	70.920295
810.124490	70.353752	70.925300
809.520281	68.418925	70.930305
808.716723	64.179158	70.935310
807.828413	74.837469	70.940314
807.013120	73.747967	70.945319
806.930338	65.066541	70.950324
806.240521	69.445258	70.955329
805.245602	65.784952	70.960334
804.532376	65.978556	70.965338
804.026649	71.334635	70.970343
803.664884	68.624503	70.975348
802.612853	73.241704	70.980353
801.788605	72.882777	70.985358
800.926392	69.072246	70.990362
800.415888	66.395486	70.995367
800.086516	68.516657	71.000372
799.858337	75.156572	71.005377
799.440443	64.825797	71.010382
798.338601	69.491002	71.015386
797.870459	75.527450	71.020391
796.766325	72.659101	71.025396
795.814919	72.575364	71.030401
795.757192	73.485592	71.035406
795.009957	70.803596	71.040410
794.273121	62.908384	71.045415
793.079575	67.717974	71.050420
792.565987	72.966064	71.055425
792.408174	61.736182	71.060430
791.479406	70.909790	71.065434
791.048434	65.140229	71.070439
790.188245	68.960004	71.075444
789.273857	67.303300	71.080449
789.125509	62.812363	71.085454
787.968717	81.168239	71.090458
788.003606	67.327452	71.095463
786.674304	72.360026	71.100468
785.938868	83.873954	71.105473
785.979696	66.343131	71.110478
784.699883	71.306047	71.115482
783.768328	61.836514	71.120487
782.793631	66.339422	71.125492
782.073352	82.100265	71.130497
782.002504	68.469422	71.135502
781.470953	79.021629	71.140506
781.271651	71.626412	71.145511
780.523535	68.440517	71.150516
780.274347	75.014166	71.155521
779.048446	66.325672	71.160526
778.307450	71.992829	71.165530
777.782436	66.383054	71.170535
777.128945	70.348600	71.175540
775.982735	71.983674	71.180545
775.592534	62.652319	71.185550
775.022579	73.747915	71.190554
774.546101	66.041779	71.195559
773.626385	71.694157	71.200564
772.647908	71.148114	71.205569
772.528880	65.531161	71.210574
771.676907	61.621389	71.215578
771.228299	60.768276	71.220583
770.483330	68.563236	71.225588
769.627937	60.601502	71.230593
769.169132	53.246406	71.235598
768.593306	58.949604	71.240602
767.370446	51.004641	71.245607
766.700255	64.163605	71.250612
766.053001	62.681398	71.255617
766.038942	63.961493	71.260622
765.233476	72.159166	71.265626
764.648833	62.124976	71.270631
763.676794	65.813527	71.275636
762.708592	68.281355	71.280641
762.356764	63.430955	71.285646
761.772407	62.871477	71.290650
761.393544	65.365449	71.295655
760.331411	65.638170	71.300660
759.529609	65.507104	71.305665
759.028546	62.702030	71.310670
758.450694	70.559149	71.315674
758.169013	68.179495	71.320679
757.111577	67.074643	71.325684
756.307996	76.740338	71.330689
755.712041	61.610331	71.335694
754.963702	71.875212	71.340698
754.849847	63.746193	71.345703
753.956852	63.166169	71.350708
753.151462	70.365987	71.355713
753.081105	68.716672	71.360718
751.786552	75.942659	71.365722
751.063820	69.067747	71.370727
750.109610	59.608422	71.375732
749.852288	66.988286	71.380737
749.190575	69.651101	71.385742
748.919252	75.405953	71.390746
748.077660	63.501015	71.395751
747.621021	66.861687	71.400756
746.726450	65.830380	71.405761
746.057416	58.613925	71.410766
745.071907	69.434537	71.415770
744.344723	67.576835	71.420775
744.151330	64.321579	71.425780
743.238252	69.401670	71.430785
742.967243	59.976092	71.435790
741.784680	68.688339	71.440794
741.369863	70.071427	71.445799
740.704981	68.013589	71.450804
739.780839	69.697468	71.455809
738.850319	67.542249	71.460814
738.419685	67.486149	71.465818
737.852550	65.077243	71.470823
737.530374	79.790991	71.475828
736.954745	72.000402	71.480833
736.624111	68.490775	71.485838
735.014858	77.032582	71.490842
734.501972	73.668249	71.495847
734.265935	70.946453	71.500852
733.499797	74.537374	71.505857
732.052274	68.153320	71.510862
731.306531	68.279088	71.515866
730.548592	64.212697	71.520871
730.574055	68.982414	71.525876
730.087381	71.759317	71.530881
730.104473	65.329223	71.535886
729.512627	73.059670	71.540890
728.543419	70.899633	71.545895
727.813159	68.255792	71.550900
726.761480	72.372840	71.555905
725.384182	64.611833	71.560910
724.946596	77.711619	71.565914
724.513343	69.532716	71.570919
724.478574	66.088454	71.575924
723.572070	74.547768	71.580929
723.397723	66.030451	71.585934
722.092713	67.472095	71.590938
721.308725	68.113205	71.595943
720.949262	72.624802	71.600948
720.703040	73.622186	71.605953
719.481471	69.769029	71.610958
718.326210	74.340774	71.615962
717.825724	71.800459	71.620967
717.458586	63.826932	71.625972
716.985286	70.841186	71.630977
716.132262	65.711934	71.635982
715.126365	68.914083	71.640986
715.060726	69.789747	71.645991
714.368931	65.879782	71.650996
713.739605	70.893111	71.656001
712.751528	63.118717	71.661006
711.934928	71.822748	71.666010
711.625462	69.438779	71.671015
711.081093	69.654389	71.676020
710.537689	77.333910	71.681025
709.537639	62.157884	71.686030
708.641979	71.186099	71.691034
707.934942	79.634930	71.696039
707.917288	73.985220	71.701044
707.233198	72.433545	71.706049
706.097843	65.377504	71.711054
705.340850	70.572959	71.716058
704.899668	66.761370	71.721063
704.489251	69.646784	71.726068
703.888630	77.292688	71.731073
703.320253	73.716035	71.736078
702.165010	72.789784	71.741082
701.768512	67.943095	71.746087
701.432261	71.193152	71.751092
699.691625	74.492756	71.756097
699.189200	72.880752	71.761102
698.748063	70.551709	71.766106
698.596016	70.174743	71.771111
698.564391	61.251686	71.776116
697.391411	64.090904	71.781121
696.944075	66.337676	71.786126
696.273783	74.979542	71.791130
694.605977	70.840094	71.796135
694.164076	73.305399	71.801140
693.351509	73.615507	71.806145
692.840701	70.983811	71.811150
692.571777	72.347039	71.816154
691.933370	62.773236	71.821159
690.679952	73.066231	71.826164
690.008054	71.956526	71.831169
689.507473	66.949654	71.836174
689.389355	73.063896	71.841178
689.009130	67.723000	71.846183
688.086454	67.834485	71.851188
686.797284	72.439438	71.856193
686.457307	61.119208	71.861198
686.359522	70.596888	71.866202
685.346601	71.994423	71.871207
684.327352	69.561537	71.876212
683.724224	74.836814	71.881217
683.346721	59.602698	71.886222
682.320046	75.272741	71.891226
681.273150	74.076105	71.896231
680.678391	71.671150	71.901236
679.896563	68.914580	71.906241
679.579750	64.321466	71.911246
679.402087	74.000717	71.916250
678.964081	69.253506	71.921255
678.691900	66.498831	71.926260
677.211300	78.026739	71.931265
676.829588	64.448779	71.936270
676.293626	68.245785	71.941274
675.246597	63.203856	71.946279
674.581681	65.351334	71.951284
673.590911	67.375042	71.956289
673.466468	61.141297	71.961294
672.239479	65.109186	71.966298
671.372842	71.204828	71.971303
671.140153	73.265233	71.976308
670.259437	75.057336	71.981313
670.022307	65.760955	71.986318
669.601563	64.237194	71.991322
669.214328	60.820558	71.996327
668.163269	67.415137	72.001332
667.295833	61.728660	72.006337
667.172016	59.216186	72.011342
665.797215	63.085064	72.016346
664.573969	72.232560	72.021351
664.422054	66.394289	72.026356
663.561724	69.744790	72.031361
663.814531	57.295566	72.036366
663.139456	76.185458	72.041370
662.070979	66.942694	72.046375
661.402347	68.203491	72.051380
660.721995	68.334251	72.056385
660.264125	62.324595	72.061390
659.253872	68.263667	72.066394
658.451487	71.798047	72.071399
658.189484	59.217164	72.076404
657.540129	66.420649	72.081409
657.299269	64.007960	72.086414
656.066319	68.334881	72.091418
655.208917	70.845716	72.096423
654.253671	74.913495	72.101428
653.904742	75.323379	72.106433
653.675584	66.280621	72.111438
652.990158	71.492634	72.116442
652.154336	66.570043	72.121447
651.597076	62.959919	72.126452
650.820422	70.403099	72.131457
650.266705	67.218659	72.136462
649.099433	74.108270	72.141466
648.436840	69.830570	72.146471
648.224225	65.233423	72.151476
647.485511	71.318598	72.156481
647.516866	74.135434	72.161486
646.494336	68.483425	72.166490
645.649443	72.528351	72.171495
645.295727	64.702924	72.176500
643.799530	66.443775	72.181505
643.106583	63.977890	72.186510
642.610858	65.800744	72.191514
642.149532	58.828579	72.196519
641.813657	64.973807	72.201524
641.255484	67.056425	72.206529
640.411485	61.023326	72.211534
639.476274	61.058419	72.216538
639.010625	61.452776	72.221543
638.763658	66.242321	72.226548
637.240083	71.449914	72.231553
636.467255	55.910142	72.236558
635.803632	59.694285	72.241562
635.449389	67.807949	72.246567
635.462897	64.948282	72.251572
634.516075	69.594061	72.256577
633.555659	64.142194	72.261582
632.582081	64.896322	72.266586
632.425453	67.285519	72.271591
631.999768	64.301767	72.276596
630.932306	68.353644	72.281601
630.149745	63.905855	72.286606
629.425048	63.010852	72.291610
628.976780	64.114694	72.296615
628.538038	52.314456	72.301620
627.855437	67.940544	72.306625
626.983073	63.590242	72.311630
626.190880	63.876740	72.316634
625.658196	67.278078	72.321639
625.292705	64.255199	72.326644
624.195165	77.532388	72.331649
623.440622	62.343541	72.336654
622.910592	66.878836	72.341658
622.312618	60.802801	72.346663
622.227630	68.301549	72.351668
621.472943	62.665235	72.356673
620.621957	59.808428	72.361678
619.898369	64.606214	72.366682
619.146344	66.042741	72.371687
618.101089	66.461804	72.376692
617.187225	74.192166	72.381697
616.799293	63.245276	72.386702
616.201562	69.690751	72.391706
615.848106	63.731104	72.396711
615.775477	71.796520	72.401716
614.710665	71.579495	72.406721
614.049830	67.242687	72.411726
613.025029	67.093804	72.416730
612.382052	55.962471	72.421735
611.900654	60.155109	72.426740
610.876756	59.218220	72.431745
610.313181	54.202421	72.436750
609.596970	60.504781	72.441754
609.385739	65.133473	72.446759
609.126807	65.210195	72.451764
607.745607	66.516509	72.456769
607.080291	53.499900	72.461774
606.371542	66.837173	72.466778
606.212680	64.048484	72.471783
605.306358	60.122405	72.476788
604.211646	64.801815	72.481793
603.811219	63.106825	72.486798
603.045823	61.602650	72.491802
602.946372	62.340826	72.496807
602.281699	53.038378	72.501812
601.072027	63.092581	72.506817
600.741728	59.461342	72.511822
600.058348	59.872877	72.516826
599.565962	58.584412	72.521831
598.398238	58.949861	72.526836
597.051747	60.426668	72.531841
596.967149	54.415436	72.536846
596.437160	62.383559	72.541850
596.108538	54.455167	72.546855
595.920833	58.497622	72.551860
595.005211	66.492743	72.556865
594.549689	64.255383	72.561870
593.617823	63.446010	72.566874
592.597809	65.462902	72.571879
592.014238	51.781013	72.576884
591.534876	60.123335	72.581889
590.643096	49.626714	72.586894
589.657651	64.378684	72.591898
588.981845	64.066990	72.596903
588.424470	53.861604	72.601908
587.551139	55.450754	72.606913
587.439466	51.176962	72.611918
586.993552	61.168592	72.616922
586.458022	62.791044	72.621927
586.032742	55.103807	72.626932
584.730083	59.010866	72.631937
584.256603	55.096284	72.636942
583.068151	54.639544	72.641946
582.088041	65.710676	72.646951
582.026788	59.370987	72.651956
581.138042	63.151870	72.656961
580.948661	52.563716	72.661966
581.041938	61.734714	72.666970
580.143367	67.795181	72.671975
579.158143	60.284799	72.676980
578.174113	64.069771	72.681985
577.105758	55.421857	72.686990
576.387418	62.740580	72.691994
575.752678	59.338733	72.696999
575.381779	61.131125	72.702004
574.620247	67.938596	72.707009
574.008997	52.819560	72.712014
573.401577	56.565660	72.717018
573.012076	61.321996	72.722023
572.013519	55.834842	72.727028
571.134547	60.469398	72.732033
570.914510	58.101303	72.737038
570.486349	59.655231	72.742042
570.124553	68.642114	72.747047
569.383646	61.668130	72.752052
568.270813	60.475319	72.757057
567.763586	62.446588	72.762062
566.643893	63.627979	72.767066
565.329258	72.239338	72.772071
565.268516	57.984738	72.777076
564.589989	72.058111	72.782081
564.470796	61.364775	72.787086
564.078184	59.375179	72.792090
563.207918	60.599486	72.797095
562.877379	61.134113	72.802100
561.732324	65.440467	72.807105
561.220885	66.429618	72.812110
560.377671	61.073341	72.817114
559.526180	62.960316	72.822119
559.109597	57.298848	72.827124
558.539598	61.545352	72.832129
557.805167	64.757064	72.837134
556.644748	62.505495	72.842138
555.475469	64.048655	72.847143
555.308885	62.023093	72.852148
554.564784	70.106457	72.857153
554.989864	67.550067	72.862158
554.447232	63.129075	72.867162
553.220595	63.229512	72.872167
552.530361	61.209206	72.877172
552.081984	68.877971	72.882177
551.345803	62.571433	72.887182
550.114072	68.976737	72.892186
549.664826	70.098910	72.897191
549.265538	61.081769	72.902196
548.284770	59.533590	72.907201
547.246916	56.602245	72.912206
546.887294	67.668900	72.917210
546.150176	65.224809	72.922215
545.892483	63.402743	72.927220
545.636619	73.272216	72.932225
545.084698	67.062783	72.937230
543.985522	64.689414	72.942234
543.235563	58.262879	72.947239
542.477911	63.978300	72.952244
541.085085	62.319159	72.957249
540.957471	61.678290	72.962254
540.233661	68.831782	72.967258
539.641077	64.813276	72.972263
539.390721	58.959521	72.977268
538.975960	67.156969	72.982273
537.851226	59.544984	72.987278
537.157713	61.939732	72.992282
536.622096	70.109341	72.997287
536.284484	59.104508	73.002292
535.069500	68.410072	73.007297
534.395931	62.613438	73.012302
533.808634	54.632279	73.017306
533.598062	66.912008	73.022311
532.931731	61.243997	73.027316
531.693767	63.310086	73.032321
531.306262	63.814610	73.037326
530.615292	56.451970	73.042330
530.003300	64.057589	73.047335
528.959443	59.298958	73.052340
527.890846	73.881250	73.057345
527.487420	61.892618	73.062350
526.977782	72.673157	73.067354
526.653521	70.546726	73.072359
526.605211	59.649025	73.077364
525.660068	69.055186	73.082369
524.811083	62.580100	73.087374
524.273707	62.868739	73.092378
523.460276	59.242533	73.097383
522.498678	58.103157	73.102388
521.505789	57.957904	73.107393
521.275234	60.535022	73.112398
520.424708	69.600516	73.117402
520.233306	68.280617	73.122407
519.837098	53.574723	73.127412
518.262338	67.282612	73.132417
517.894229	59.004963	73.137422
517.260326	65.337436	73.142426
517.061451	61.529746	73.147431
516.778540	62.802620	73.152436
515.496172	66.135463	73.157441
514.866286	54.346292	73.162446
514.064969	63.113631	73.167450
513.195911	67.538877	73.172455
512.516558	56.659711	73.177460
511.396892	66.361420	73.182465
510.834372	59.187551	73.187470
510.435182	58.832022	73.192474
510.215606	64.234205	73.197479
510.232522	57.645090	73.202484
509.481948	57.669095	73.207489
508.525094	56.847839	73.212494
507.758286	62.685614	73.217498
506.217637	63.102356	73.222503
505.734577	64.224405	73.227508
505.459399	70.513964	73.232513
504.721108	59.508326	73.237518
504.380716	62.447667	73.242522
503.902285	64.755830	73.247527
502.687206	57.514187	73.252532
501.536176	62.307469	73.257537
500.952401	55.743528	73.262542
500.398292	64.787832	73.267546
499.906966	63.199609	73.272551
499.842227	58.092430	73.277556
499.549262	60.343945	73.282561
498.355896	61.370222	73.287566
497.761897	58.586635	73.292570
497.254929	61.434527	73.297575
496.547882	60.724801	73.302580
495.842922	64.005282	73.307585
495.233517	58.556459	73.312590
494.352278	64.070048	73.317594
493.486225	64.411459	73.322599
492.689134	62.906419	73.327604
492.023564	69.811922	73.332609
491.510965	57.604390	73.337614
491.173675	59.899025	73.342618
489.790379	60.153816	73.347623
489.297631	54.340815	73.352628
488.236775	64.301644	73.357633
488.169036	54.430381	73.362638
487.676540	60.930455	73.367642
487.339235	61.972269	73.372647
487.103958	61.975869	73.377652
485.510372	57.909048	73.382657
485.075984	61.181452	73.387662
484.649374	56.362850	73.392666
483.522358	58.196399	73.397671
482.879523	56.725714	73.402676
481.951389	61.273185	73.407681
481.532961	54.830511	73.412686
481.210566	60.764230	73.417690
480.569980	61.680788	73.422695
479.895509	57.569754	73.427700
478.752087	64.229131	73.432705
478.807527	58.210094	73.437710
477.653506	75.158344	73.442714
477.198575	70.396694	73.447719
476.346806	65.925272	73.452724
475.567256	60.123919	73.457729
475.165358	61.262851	73.462734
474.448236	59.009943	73.467738
473.754560	62.350462	73.472743
473.182189	59.364237	73.477748
471.933218	61.558141	73.482753
471.601897	54.705038	73.487758
471.186178	62.022829	73.492762
470.835392	65.229990	73.497767
470.324078	59.040457	73.502772
469.026461	65.754679	73.507777
468.491023	60.793289	73.512782
468.167801	65.123821	73.517786
466.984882	65.898856	73.522791
466.472723	61.008473	73.527796
465.741568	62.243693	73.532801
465.222344	60.514211	73.537806
464.868232	68.779420	73.542810
463.637110	67.627036	73.547815
463.129899	59.267054	73.552820
462.031047	64.885434	73.557825
461.923761	64.847367	73.562830
461.490228	55.990841	73.567834
460.658246	62.605141	73.572839
459.726718	56.574062	73.577844
458.902484	66.717361	73.582849
458.457710	64.305685	73.587854
457.983747	59.229952	73.592858
457.556212	62.819719	73.597863
456.916681	59.860004	73.602868
456.116583	63.482037	73.607873
455.428154	56.895382	73.612878
454.973480	58.576223	73.617882
453.831094	58.292007	73.622887
453.090995	53.728435	73.627892
452.687399	51.414700	73.632897
452.170601	56.505465	73.637902
451.397106	57.751101	73.642906
450.054259	65.279874	73.647911
449.921691	63.093367	73.652916
449.034352	63.097005	73.657921
449.096269	56.564521	73.662926
448.536565	60.681381	73.667930
447.175969	63.021123	73.672935
446.763225	64.953318	73.677940
445.926822	64.240505	73.682945
445.614268	67.083111	73.687950
444.473302	67.628343	73.692954
443.601871	66.374064	73.697959
443.208623	49.538201	73.702964
442.693377	61.311213	73.707969
442.258001	57.569321	73.712974
441.965231	60.311830	73.717978
440.810431	63.067071	73.722983
440.668322	58.325635	73.727988
439.700255	63.016921	73.732993
438.566769	62.242527	73.737998
437.409495	63.482489	73.743002
436.907757	58.186138	73.748007
436.918638	59.287886	73.753012
436.444398	61.463107	73.758017
435.987771	59.916311	73.763022
434.854904	67.714613	73.768026
433.832913	71.145742	73.773031
433.813485	54.103718	73.778036
432.944695	68.194692	73.783041
432.090391	60.824144	73.788046
431.093918	61.742490	73.793050
430.773295	61.276798	73.798055
430.488594	58.083396	73.803060
429.704033	62.110904	73.808065
428.992932	71.086202	73.813070
428.058807	74.061378	73.818074
427.576947	76.258433	73.823079
427.347612	64.168543	73.828084
425.936373	71.074738	73.833089
424.908637	63.379458	73.838094
424.643228	70.950953	73.843098
424.078857	64.435405	73.848103
424.291026	62.560852	73.853108
423.227202	70.382850	73.858113
422.136497	65.318081	73.863118
421.724111	63.266760	73.868122
420.994945	59.041564	73.873127
420.471310	60.502134	73.878132
419.315690	64.713621	73.883137
418.619328	55.916750	73.888142
417.805110	58.880061	73.893146
417.227202	66.807458	73.898151
417.188583	61.507923	73.903156
416.923634	60.532984	73.908161
416.044281	64.744098	73.913166
415.422835	62.547825	73.918170
414.488140	61.197426	73.923175
413.652539	59.340995	73.928180
412.420751	64.075902	73.933185
411.994788	57.583611	73.938190
411.360321	65.504517	73.943194
411.054101	59.485492	73.948199
410.886753	59.788884	73.953204
409.971685	63.253399	73.958209
409.297626	66.154406	73.963214
408.304938	56.715990	73.968218
407.488358	60.120603	73.973223
407.317315	55.592538	73.978228
406.189763	62.679841	73.983233
405.250510	67.988266	73.988238
405.011053	61.969246	73.993242
404.438384	67.320236	73.998247
404.336338	60.679281	74.003252
403.181217	65.419603	74.008257
402.178454	63.754443	74.013262
401.643075	60.620581	74.018266
401.269134	59.628007	74.023271
400.892817	54.852901	74.028276
399.849935	59.733846	74.033281
398.941870	57.652219	74.038286
398.295061	69.092935	74.043290
398.085935	64.649153	74.048295
397.434166	66.433642	74.053300
395.760922	63.575305	74.058305
395.583989	52.256406	74.063310
394.987898	60.394931	74.068314
394.479524	59.559205	74.073319
394.557775	53.452585	74.078324
393.308138	56.057519	74.083329
392.847388	60.125453	74.088334
391.982744	61.655519	74.093338
391.422378	67.371880	74.098343
390.496861	54.716881	74.103348
389.523006	64.102317	74.108353
389.066018	62.003383	74.113358
388.945485	71.508620	74.118362
388.205682	63.862684	74.123367
387.055381	64.027446	74.128372
386.336011	62.355168	74.133377
385.959391	58.408225	74.138382
385.627140	65.251082	74.143386
384.610244	67.977571	74.148391
383.640213	61.343670	74.153396
382.994995	70.138346	74.158401
382.906567	65.035232	74.163406
382.098192	73.682224	74.168410
381.058633	62.140520	74.173415
380.275874	53.497011	74.178420
379.257692	53.562558	74.183425
379.100929	62.754674	74.188430
378.748357	64.772082	74.193434
378.765594	64.904902	74.198439
378.611980	50.385615	74.203444
377.254577	62.349927	74.208449
376.094315	56.850279	74.213454
374.857746	60.719220	74.218458
373.756677	62.986084	74.223463
373.556177	59.964561	74.228468
373.160712	67.920295	74.233473
372.495570	54.633343	74.238478
372.164998	60.254666	74.243482
371.738848	61.578541	74.248487
371.566482	56.540735	74.253492
370.152678	63.356594	74.258497
369.763149	59.602117	74.263502
369.146179	54.402497	74.268506
367.925189	60.262469	74.273511
367.360217	53.491265	74.278516
366.637713	62.308656	74.283521
366.172696	63.797473	74.288526
364.957090	53.665872	74.293530
364.417501	64.145238	74.298535
363.861124	54.159589	74.303540
363.497092	60.104391	74.308545
363.170107	63.204852	74.313550
362.662640	62.098200	74.318554
361.923513	62.103294	74.323559
361.066955	58.355838	74.328564
360.008500	72.743782	74.333569
359.566385	52.239946	74.338574
358.552408	53.179462	74.343578
357.513635	56.066010	74.348583
357.443364	57.177323	74.353588
356.876195	61.490458	74.358593
357.072323	57.637584	74.363598
355.886093	59.908784	74.368602
354.554256	59.883232	74.373607
354.411549	55.673980	74.378612
353.620601	63.472110	74.383617
352.793127	68.840723	74.388622
351.929512	66.865164	74.393626
351.257352	65.299268	74.398631
350.755229	63.690019	74.403636
349.688144	62.200097	74.408641
349.650136	62.258705	74.413646
349.600638	65.282795	74.418650
348.812138	68.119743	74.423655
348.247652	62.472996	74.428660
346.992368	65.625588	74.433665
345.766041	64.397813	74.438670
345.228914	57.433956	74.443674
344.741264	61.847141	74.448679
344.412991	56.038736	74.453684
343.423058	66.898822	74.458689
343.112138	63.689395	74.463694
342.783481	58.306557	74.468698
341.716930	63.945473	74.473703
341.129668	55.770938	74.478708
340.646145	63.256659	74.483713
339.464595	55.073459	74.488718
338.707880	57.483404	74.493722
338.331349	66.235582	74.498727
338.316932	56.070610	74.503732
337.393721	58.001489	74.508737
336.457602	63.131369	74.513742
335.413831	64.803060	74.518746
334.677498	63.477099	74.523751
334.968248	61.450532	74.528756
333.337862	63.401963	74.533761
332.876977	60.851757	74.538766
332.520819	51.592020	74.543770
331.725461	59.480900	74.548775
331.734254	59.402810	74.553780
330.457585	63.203244	74.558785
329.672052	51.406067	74.563790
328.930539	55.077281	74.568794
328.230086	58.643570	74.573799
328.099542	52.405776	74.578804
327.258154	57.697040	74.583809
326.778645	54.022331	74.588814
326.142604	61.743389	74.593818
325.452000	55.378176	74.598823
324.335863	48.531326	74.603828
323.238773	60.012897	74.608833
323.095560	59.017494	74.613838
322.507464	57.497586	74.618842
322.032035	56.808187	74.623847
321.582948	54.398452	74.628852
319.800813	60.051470	74.633857
319.552542	59.864290	74.638862
319.499533	55.542173	74.643866
318.618557	58.940468	74.648871
318.274422	54.776400	74.653876
317.161570	51.364971	74.658881
316.549533	54.860056	74.663886
315.803162	54.744433	74.668890
315.340789	57.086566	74.673895
314.795636	58.092966	74.678900
313.824882	67.423805	74.683905
313.190751	62.211740	74.688910
312.683784	59.122756	74.693914
311.982992	57.202584	74.698919
311.957595	60.790534	74.703924
310.345306	60.036661	74.708929
309.644888	55.799061	74.713934
309.366087	60.814705	74.718938
308.781940	62.848914	74.723943
307.589141	48.772607	74.728948
306.968779	64.449589	74.733953
306.551514	58.488293	74.738958
306.004799	59.336682	74.743962
305.478830	64.854137	74.748967
305.193333	51.947374	74.753972
303.977981	58.762389	74.758977
303.390722	53.023246	74.763982
302.969413	57.373749	74.768986
302.124323	60.113040	74.773991
300.835169	54.757474	74.778996
300.108731	57.753516	74.784001
299.758959	54.805345	74.789006
299.609507	57.837881	74.794010
299.072933	62.604828	74.799015
298.819381	54.580331	74.804020
297.489682	60.155810	74.809025
297.022357	55.472496	74.814030
296.355684	61.957432	74.819034
295.060016	68.142440	74.824039
294.647052	63.728474	74.829044
293.133615	61.203951	74.834049
293.096315	50.421630	74.839054
292.844627	55.628007	74.844058
292.255812	58.240089	74.849063
292.096500	48.305213	74.854068
290.941025	63.682750	74.859073
290.373559	52.728814	74.864078
289.800177	62.130876	74.869082
288.848576	61.422049	74.874087
287.786447	55.722856	74.879092
287.418657	64.390645	74.884097
286.890274	56.963879	74.889102
286.842655	60.215000	74.894106
285.589987	69.215237	74.899111
284.838887	59.780448	74.904116
283.936599	64.129320	74.909121
283.826195	61.759427	74.914126
283.515110	59.602737	74.919130
281.977166	59.061908	74.924135
281.477528	53.027505	74.929140
280.610418	68.433381	74.934145
280.344181	63.464956	74.939150
279.820138	54.149535	74.944154
278.744949	63.669975	74.949159
278.290141	57.423031	74.954164
277.238528	65.888705	74.959169
276.663636	58.392549	74.964174
276.668693	59.638574	74.969178
275.667025	67.521380	74.974183
275.020602	66.866425	74.979188
273.874248	69.558285	74.984193
273.700782	65.052353	74.989198
273.491320	59.261090	74.994202
272.480071	64.361623	74.999207
271.302436	58.488427	75.004212
270.959325	59.331130	75.009217
270.181226	62.987704	75.014222
269.932692	55.606128	75.019226
269.035088	61.475424	75.024231
268.324227	53.421165	75.029236
267.848446	67.123483	75.034241
267.383735	58.440485	75.039246
266.570885	52.052821	75.044250
265.532943	65.094039	75.049255
264.954663	60.385539	75.054260
264.351400	63.533753	75.059265
263.957445	58.502360	75.064270
262.965937	61.207152	75.069274
262.156424	61.182486	75.074279
261.646161	57.698967	75.079284
261.042755	62.044766	75.084289
260.657371	63.127597	75.089294
260.125416	56.424565	75.094298
258.997711	58.597339	75.099303
258.409173	55.669179	75.104308
258.134668	59.751772	75.109313
257.294598	60.025223	75.114318
256.562902	54.419393	75.119322
255.409277	53.072610	75.124327
255.277792	60.375628	75.129332
254.676259	62.879374	75.134337
253.922589	61.712310	75.139342
252.971697	57.820005	75.144346
252.357392	67.977858	75.149351
251.845374	57.572548	75.154356
251.244315	55.205844	75.159361
250.754762	59.688435	75.164366
249.829941	60.429545	75.169370
248.753306	64.721075	75.174375
248.765748	60.068813	75.179380
248.018066	63.983451	75.184385
247.193612	58.793365	75.189390
246.375228	57.886855	75.194394
245.704638	66.105654	75.199399
245.300118	55.974798	75.204404
244.799091	58.299879	75.209409
244.015255	64.890951	75.214414
243.222012	64.086309	75.219418
242.439773	68.909581	75.224423
242.257482	58.417361	75.229428
241.497978	56.866849	75.234433
240.739397	60.982291	75.239438
240.062633	52.926930	75.244442
239.373611	60.561159	75.249447
238.876032	59.452037	75.254452
238.074722	65.452850	75.259457
237.369517	63.456873	75.264462
236.559430	63.039965	75.269466
236.083306	64.398862	75.274471
235.327144	55.902401	75.279476
233.997466	63.460142	75.284481
233.717652	55.918548	75.289486
232.932613	55.424720	75.294490
232.456526	62.678261	75.299495
232.556366	55.512879	75.304500
232.150075	55.329108	75.309505
231.184570	62.370505	75.314510
230.146722	60.029335	75.319514
229.332732	58.680390	75.324519
228.550584	52.072354	75.329524
227.791759	60.331143	75.334529
227.099684	58.871701	75.339534
226.734818	55.281164	75.344538
226.079394	62.284803	75.349543
226.234440	55.345998	75.354548
224.689945	61.806551	75.359553
223.941763	56.691024	75.364558
223.522900	61.152027	75.369562
223.039540	63.105025	75.374567
222.123283	52.054586	75.379572
220.722005	55.189603	75.384577
220.236932	56.061380	75.389582
220.103916	56.422047	75.394586
219.510755	60.376116	75.399591
219.421365	57.502918	75.404596
218.614265	71.771211	75.409601
217.793097	62.616459	75.414606
216.871899	60.538307	75.419610
216.163396	57.093906	75.424615
214.949391	52.381107	75.429620
214.445942	55.942452	75.434625
214.243574	57.312842	75.439630
213.832103	54.137245	75.444634
213.171544	60.816522	75.449639
212.855854	63.744535	75.454644
211.264562	58.703669	75.459649
210.555953	60.585548	75.464654
210.127309	58.428097	75.469658
209.597793	66.225635	75.474663
209.233542	52.779003	75.479668
207.967388	58.519256	75.484673
207.499305	59.520745	75.489678
207.336807	56.298128	75.494682
206.352611	61.399164	75.499687
205.407089	60.829436	75.504692
204.507066	60.761878	75.509697
203.827298	53.785398	75.514702
203.847177	52.293124	75.519706
203.293298	55.663390	75.524711
202.819904	53.665575	75.529716
201.610084	58.787920	75.534721
201.003907	46.158773	75.539726
200.710240	50.708437	75.544730
199.455663	58.724991	75.549735
198.789420	52.932702	75.554740
198.232376	55.028587	75.559745
197.880735	55.544355	75.564750
197.357912	56.304191	75.569754
196.533991	62.057451	75.574759
195.314079	56.560585	75.579764
194.856230	60.866834	75.584769
194.499644	59.104376	75.589774
194.057496	59.027407	75.594778
192.913202	58.119540	75.599783
192.314127	50.329937	75.604788
191.636755	59.517735	75.609793
191.158957	53.658014	75.614798
190.832420	55.603077	75.619802
189.268468	61.554638	75.624807
188.978174	53.486721	75.629812
188.042938	60.403336	75.634817
187.761002	53.304192	75.639822
187.434919	58.900669	75.644826
186.637796	59.075986	75.649831
186.062403	51.993597	75.654836
185.326906	61.581337	75.659841
184.875198	56.782869	75.664846
184.402663	59.813160	75.669850
182.847361	53.709095	75.674855
182.228434	52.642098	75.679860
181.630220	60.598637	75.684865
181.175715	61.335712	75.689870
181.030243	56.083721	75.694874
179.344114	67.553795	75.699879
179.220000	60.246816	75.704884
178.460835	53.308818	75.709889
178.125786	59.530084	75.714894
177.096911	51.929418	75.719898
175.828952	58.514278	75.724903
175.714500	59.337920	75.729908
175.310145	56.260575	75.734913
174.649771	62.880221	75.739918
174.474079	61.098202	75.744922
173.408446	62.891299	75.749927
172.502310	64.962562	75.754932
172.227022	68.350598	75.759937
171.473579	62.731144	75.764942
170.478952	60.375475	75.769946
169.512936	64.058355	75.774951
169.238823	52.206316	75.779956
168.385810	66.005267	75.784961
168.388538	59.071653	75.789966
167.552808	58.556134	75.794970
166.769895	56.415606	75.799975
166.068136	50.919921	75.804980
165.612217	53.701457	75.809985
164.526745	64.792660	75.814990
163.936966	57.496042	75.819994
163.298732	65.423921	75.824999
163.020072	54.224333	75.830004
162.185846	53.713293	75.835009
161.121294	53.821177	75.840014
161.004808	53.413663	75.845018
160.229999	63.728495	75.850023
159.504203	49.804283	75.855028
158.090712	60.343462	75.860033
157.414004	56.219847	75.865038
157.397972	59.916312	75.870042
156.799675	59.471401	75.875047
156.683560	51.932150	75.880052
155.681900	63.086348	75.885057
154.411086	61.726919	75.890062
154.133038	53.791901	75.895066
153.649051	58.428665	75.900071
153.302967	56.592573	75.905076
151.934585	55.448017	75.910081
151.125049	59.287221	75.915086
150.924192	49.984317	75.920090
150.199199	57.024752	75.925095
149.587045	51.483317	75.930100
148.301600	59.856862	75.935105
147.587077	58.905329	75.940110
147.341300	50.982938	75.945114
146.325410	52.839349	75.950119
146.542939	50.350488	75.955124
146.017072	59.162600	75.960129
145.077850	50.025746	75.965134
144.175769	52.267622	75.970138
143.551357	60.362068	75.975143
143.349282	50.191399	75.980148
141.861729	46.989904	75.985153
140.816217	54.986021	75.990158
140.313104	53.553406	75.995162
139.524953	61.139113	76.000167
139.472275	51.595293	76.005172
139.247425	56.224736	76.010177
139.104830	52.598079	76.015182
138.019005	49.567701	76.020186
137.349421	57.853036	76.025191
136.922625	49.963258	76.030196
135.493116	56.515824	76.035201
134.668897	61.881534	76.040206
134.413113	52.959866	76.045210
134.040819	62.362588	76.050215
133.332431	54.608708	76.055220
131.838943	60.849370	76.060225
131.442291	61.644817	76.065230
131.073514	53.867847	76.070234
130.320523	57.932608	76.075239
129.949129	45.628734	76.080244
128.939470	50.381666	76.085249
128.105720	51.641233	76.090254
127.779654	49.845921	76.095258
127.193086	56.467914	76.100263
126.478979	55.337509	76.105268
125.303356	61.060287	76.110273
124.677768	56.933835	76.115278
124.358146	53.238060	76.120282
123.969643	63.511140	76.125287
123.760121	58.089355	76.130292
122.748799	53.394730	76.135297
121.647790	49.803704	76.140302
121.047364	48.763542	76.145306
119.548956	69.031567	76.150311
119.033749	49.312007	76.155316
119.006199	55.238202	76.160321
118.466047	55.848658	76.165326
117.933403	55.022257	76.170330
117.311531	55.563044	76.175335
116.885218	47.016385	76.180340
115.639857	62.657225	76.185345
114.859259	59.449006	76.190350
114.443728	57.655216	76.195354
113.979098	65.023631	76.200359
113.486316	54.306391	76.205364
112.268354	56.518354	76.210369
111.867343	55.492161	76.215374
111.504846	57.334847	76.220378
110.387938	60.793752	76.225383
109.699403	58.686788	76.230388
108.733924	55.816168	76.235393
108.414096	58.729106	76.240398
108.099632	58.642885	76.245402
107.568786	58.665599	76.250407
107.072833	50.056674	76.255412
105.851179	55.687482	76.260417
105.290006	53.111870	76.265422
104.596916	55.212537	76.270426
103.651982	55.872654	76.275431
103.082235	51.874389	76.280436
102.351412	63.723037	76.285441
101.987684	55.120650	76.290446
101.823458	50.662887	76.295450
100.391126	60.006960	76.300455
99.828330	54.469307	76.305460
99.290804	52.472238	76.310465
98.665128	48.780782	76.315470
98.233159	49.515579	76.320474
97.321631	56.505503	76.325479
96.659995	48.175628	76.330484
95.963733	47.922774	76.335489
95.447503	49.415655	76.340494
94.376832	41.947308	76.345498
93.297197	50.796727	76.350503
92.773945	45.472549	76.355508
92.426340	59.746919	76.360513
92.042195	54.868992	76.365518
91.586334	51.606290	76.370522
91.542142	56.792883	76.375527
90.848971	50.285672	76.380532
89.818489	54.401958	76.385537
88.747327	53.178836	76.390542
87.908488	43.051432	76.395546
86.962270	59.576454	76.400551
86.628560	44.803912	76.405556
86.223472	46.358261	76.410561
85.390126	49.720794	76.415566
84.601532	43.291522	76.420570
83.790033	54.424961	76.425575
83.463255	47.906250	76.430580
82.813012	61.014423	76.435585
82.198734	56.169637	76.440590
81.519753	54.018411	76.445594
80.300468	61.618832	76.450599
80.190469	48.580589	76.455604
79.424526	49.368304	76.460609
78.736627	56.739864	76.465614
78.506374	44.195108	76.470618
77.145157	57.286627	76.475623
76.419129	55.303327	76.480628
76.181731	57.915177	76.485633
75.527190	49.694610	76.490638
75.512033	54.799649	76.495642
74.110771	56.814903	76.500647
73.451855	50.108019	76.505652
72.607979	57.179105	76.510657
72.264484	54.551179	76.515662
71.761374	46.365438	76.520666
70.644158	61.093840	76.525671
70.251279	51.738215	76.530676
69.555508	60.996274	76.535681
69.057846	55.944403	76.540686
68.317860	52.570163	76.545690
67.364317	53.755942	76.550695
66.503106	44.677578	76.555700
66.387091	55.508633	76.560705
65.694836	53.054179	76.565710
65.039936	55.373289	76.570714
63.984081	55.064071	76.575719
63.949075	54.193013	76.580724
63.393247	54.139494	76.585729
62.357128	49.259675	76.590734
61.258430	49.640656	76.595738
60.335512	54.152164	76.600743
60.525858	53.432721	76.605748
59.726650	55.087011	76.610753
59.329105	55.722362	76.615758
58.723245	47.061244	76.620762
57.280991	52.430691	76.625767
56.814190	39.607966	76.630772
56.424338	46.542000	76.635777
55.849491	47.944678	76.640782
55.216091	43.377899	76.645786
53.902243	45.375802	76.650791
53.661880	39.388959	76.655796
53.117507	47.183119	76.660801
52.565632	45.038526	76.665806
51.892922	41.252124	76.670810
50.752792	52.760440	76.675815
50.384840	46.080252	76.680820
49.778016	47.738661	76.685825
49.430508	50.458594	76.690830
48.992248	48.895669	76.695834
47.850136	51.740392	76.700839
47.240695	45.843272	76.705844
46.095820	52.892154	76.710849
45.156582	47.968890	76.715854
44.984186	50.044233	76.720858
44.407052	52.406851	76.725863
44.207402	47.234028	76.730868
43.734491	55.898911	76.735873
42.553117	59.648733	76.740878
42.210313	57.505792	76.745882
41.242234	51.616085	76.750887
40.316754	47.194906	76.755892
39.427384	52.951113	76.760897
38.851558	55.443368	76.765902
38.698939	56.559722	76.770906
37.863036	52.447243	76.775911
37.205939	51.845861	76.780916
36.128486	61.289356	76.785921
35.522490	54.241453	76.790926
35.341253	46.176574	76.795930
34.893628	62.702557	76.800935
34.554279	52.944627	76.805940
33.804307	60.598791	76.810945
32.725108	68.395850	76.815950
32.390316	54.143334	76.820954
30.839579	54.086332	76.825959
30.489500	41.055321	76.830964
29.723293	53.150804	76.835969
29.104527	51.226881	76.840974
28.509361	50.073732	76.845978
28.255190	57.852875	76.850983
27.327025	45.912495	76.855988
26.331613	50.325916	76.860993
25.750926	49.355011	76.865998
25.744958	54.478207	76.871002
24.609866	54.608084	76.876007
23.613811	46.404640	76.881012
23.020068	50.652490	76.886017
22.521232	49.827409	76.891022
22.403450	44.474773	76.896026
21.676361	47.813570	76.901031
20.554461	52.023300	76.906036
20.000543	55.855796	76.911041
19.451790	53.465950	76.916046
18.996892	48.714238	76.921050
17.737852	56.826716	76.926055
16.868329	51.589155	76.931060
16.412065	48.277193	76.936065
15.944645	50.817174	76.941070
15.792801	41.179464	76.946074
15.456518	52.622585	76.951079
14.511420	44.979583	76.956084
13.665755	54.874752	76.961089
12.677982	49.275386	76.966094
11.546753	46.085865	76.971098
10.760519	56.775663	76.976103
10.234945	50.865747	76.981108
9.469087	51.514915	76.986113
9.082088	54.606731	76.991118
8.762644	46.482663	76.996122
8.822858	59.768607	77.001127
8.183621	54.377490	77.006132
7.032910	49.996910	77.011137
6.153013	46.464710	77.016142
5.896249	50.854902	77.021147
4.846087	56.563689	77.026151
3.898166	49.761120	77.031156
3.133385	50.262481	77.036161