Tue Jun 08 17:55:07 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.358427	99.404106	0.000000
-0.417558	98.593610	0.005005
-0.968560	69.890603	0.010010
-2.290247	22.349959	0.015014
-6.444746	21.710780	0.020019
-11.808361	15.995321	0.025024
-16.879252	12.087189	0.030029
-21.374561	12.827954	0.035034
-25.268653	12.295316	0.040038
-29.136117	18.475307	0.045043
-32.671556	13.513307	0.050048
-36.149411	25.984899	0.055053
-39.953044	17.169145	0.060058
-43.612422	15.859351	0.065062
-47.655955	25.860353	0.070067
-51.181860	11.514454	0.075072
-55.202328	16.461179	0.080077
-58.868770	14.655668	0.085082
-62.535714	15.331004	0.090086
-66.365702	26.038249	0.095091
-70.113172	21.998761	0.100096
-73.833890	21.098958	0.105101
-77.310224	17.312965	0.110106
-81.315405	13.150324	0.115110
-85.175412	19.863124	0.120115
-89.055081	17.755145	0.125120
-92.758514	25.225788	0.130125
-96.337238	21.555650	0.135130
-99.918941	17.069766	0.140134
-104.043061	23.115814	0.145139
-107.453710	16.297466	0.150144
-111.425103	8.584954	0.155149
-115.125529	15.271594	0.160154
-119.229475	11.950081	0.165158
-122.869399	17.814433	0.170163
-126.418775	15.284739	0.175168
-130.038092	18.805324	0.180173
-134.041335	12.610035	0.185178
-137.328518	7.840404	0.190182
-141.611445	4.758409	0.195187
-145.146063	0.781958	0.200192
-149.024603	11.501527	0.205197
-153.866389	21.863700	0.210202
-157.167433	18.508338	0.215206
-161.288748	11.825332	0.220211
-164.349265	12.616603	0.225216
-168.125634	-1.198359	0.230221
-171.466715	10.921452	0.235226
-174.999062	4.917009	0.240230
-179.089096	18.853055	0.245235
-183.088125	6.250550	0.250240
-187.092586	12.580860	0.255245
-190.763061	16.036059	0.260250
-193.916093	6.926914	0.265254
-198.311364	18.461806	0.270259
-201.862574	14.201289	0.275264
-205.278006	9.423708	0.280269
-209.424683	17.649748	0.285274
-213.016716	3.763346	0.290278
-216.976714	10.814293	0.295283
-220.637696	9.175733	0.300288
-224.149515	5.122019	0.305293
-228.300457	13.784565	0.310298
-231.999860	12.505080	0.315302
-236.017637	19.150325	0.320307
-239.578606	9.591349	0.325312
-243.005562	18.780612	0.330317
-246.895718	9.029435	0.335322
-250.522872	7.331023	0.340326
-254.651098	13.252777	0.345331
-257.988432	8.816293	0.350336
-261.943481	13.625266	0.355341
-265.695628	11.802656	0.360346
-269.323231	9.950794	0.365350
-273.596270	14.650120	0.370355
-277.211363	12.967422	0.375360
-280.780867	11.568204	0.380365
-284.765555	16.832250	0.385370
-288.309398	10.372799	0.390374
-291.937427	7.816472	0.395379
-295.878737	10.749036	0.400384
-299.599709	12.392185	0.405389
-303.648502	15.360164	0.410394
-306.968971	8.890834	0.415398
-310.947303	21.118859	0.420403
-314.738530	17.793229	0.425408
-318.177500	15.654857	0.430413
-322.307300	12.373495	0.435418
-325.685249	11.374847	0.440422
-329.925526	15.575217	0.445427
-333.321426	16.585963	0.450432
-337.008780	17.448560	0.455437
-341.138883	17.558613	0.460442
-345.048862	17.105947	0.465446
-348.502441	13.894916	0.470451
-351.941970	19.872685	0.475456
-356.076967	14.201886	0.480461
-359.716767	17.605774	0.485466
-363.174319	8.079692	0.490470
-367.386749	7.307113	0.495475
-371.282036	11.401369	0.500480
-374.832251	13.814968	0.505485
-379.113526	18.384365	0.510490
-382.341024	9.927574	0.515494
-385.961913	13.977929	0.520499
-389.415309	4.399848	0.525504
-393.143297	14.980492	0.530509
-397.911975	21.418396	0.535514
-401.527525	10.851366	0.540518
-405.098035	17.170567	0.545523
-408.868813	12.572128	0.550528
-413.042648	5.213170	0.555533
-416.441363	11.730258	0.560538
-419.788331	9.928660	0.565542
-423.854196	18.655322	0.570547
-427.286307	14.748747	0.575552
-431.208544	10.953495	0.580557
-434.806974	12.272200	0.585562
-438.542765	10.624948	0.590566
-442.697045	16.284510	0.595571
-446.478123	20.892490	0.600576
-450.248200	6.404928	0.605581
-453.764586	12.146101	0.610586
-457.560945	7.055158	0.615590
-461.798356	15.100410	0.620595
-465.411631	1.881007	0.625600
-468.586623	2.940790	0.630605
-472.900310	15.483029	0.635610
-476.102246	7.745827	0.640614
-480.050627	13.334572	0.645619
-484.226308	11.437194	0.650624
-487.417898	4.641187	0.655629
-491.884719	10.363492	0.660634
-495.196745	3.558551	0.665638
-499.308082	14.295827	0.670643
-502.886033	13.930797	0.675648
-506.386346	10.392017	0.680653
-510.483402	16.190626	0.685658
-513.981171	15.104531	0.690662
-517.650239	12.422813	0.695667
-521.297058	15.753036	0.700672
-525.479732	18.333290	0.705677
-529.253007	17.117252	0.710682
-532.601218	10.366703	0.715686
-536.659769	19.144700	0.720691
-540.605508	16.489157	0.725696
-543.956317	10.503614	0.730701
-547.898612	21.728602	0.735706
-551.448070	16.795496	0.740710
-555.649618	19.410198	0.745715
-559.414293	12.894142	0.750720
-563.058722	13.333538	0.755725
-567.032503	17.067244	0.760730
-570.123507	8.709942	0.765734
-574.045604	16.118993	0.770739
-577.607254	19.000469	0.775744
-581.867300	15.143328	0.780749
-585.794666	14.987128	0.785754
-589.092370	14.822352	0.790758
-593.109363	8.344890	0.795763
-596.460865	8.187773	0.800768
-600.564671	8.379207	0.805773
-604.466807	17.902074	0.810778
-608.320339	5.948418	0.815782
-612.477781	8.046430	0.820787
-615.798980	16.823481	0.825792
-619.237035	11.564235	0.830797
-623.333193	16.010912	0.835802
-626.633416	6.097700	0.840806
-630.552848	16.252324	0.845811
-634.346538	8.051574	0.850816
-638.105518	8.027171	0.855821
-642.232132	11.127215	0.860826
-645.715416	12.348573	0.865830
-649.663058	15.180298	0.870835
-653.250599	12.169729	0.875840
-656.273780	10.360907	0.880845
-660.638250	11.067621	0.885850
-664.193706	1.601241	0.890854
-668.357423	8.284518	0.895859
-672.075538	10.356925	0.900864
-676.192570	7.224496	0.905869
-680.037835	13.964443	0.910874
-683.155439	2.484134	0.915878
-686.776150	9.980095	0.920883
-691.200065	12.307055	0.925888
-694.955320	13.995094	0.930893
-698.572715	24.509623	0.935898
-701.972112	14.296935	0.940902
-705.930732	17.583717	0.945907
-709.394747	13.309457	0.950912
-713.316318	12.088639	0.955917
-717.455857	18.119309	0.960922
-720.911817	13.166751	0.965926
-724.806710	21.376463	0.970931
-728.419295	11.863497	0.975936
-732.204020	13.855814	0.980941
-736.014491	18.944695	0.985946
-739.631192	19.225937	0.990950
-743.453602	20.334666	0.995955
-747.586115	22.910464	1.000960
-751.140277	14.926457	1.005965
-754.971747	23.782497	1.010970
-758.574053	13.718755	1.015974
-762.288445	11.275933	1.020979
-765.860334	15.957206	1.025984
-769.529442	15.304905	1.030989
-773.547875	19.483001	1.035994
-777.517845	12.243362	1.040998
-781.362047	18.667445	1.046003
-784.973129	15.432494	1.051008
-788.749789	18.307620	1.056013
-792.467953	22.597210	1.061018
-796.230367	20.406193	1.066022
-800.136671	16.998127	1.071027
-803.712138	20.038851	1.076032
-807.406611	18.908603	1.081037
-811.274264	18.230026	1.086042
-814.693238	11.513568	1.091046
-818.501756	9.802557	1.096051
-822.265335	24.932318	1.101056
-826.100734	19.263061	1.106061
-830.558986	12.582909	1.111066
-833.900824	12.639432	1.116070
-837.620647	9.814743	1.121075
-841.463808	19.630021	1.126080
-845.091885	11.926795	1.131085
-848.827293	26.080761	1.136090
-852.276380	15.801346	1.141094
-856.220635	14.837560	1.146099
-860.499222	17.318545	1.151104
-864.234188	16.028731	1.156109
-867.553412	17.906130	1.161114
-871.509023	16.851157	1.166118
-875.289066	19.540635	1.171123
-878.777114	18.774065	1.176128
-882.289945	11.052274	1.181133
-886.296214	19.407541	1.186138
-890.214109	4.265726	1.191142
-894.168266	14.891483	1.196147
-897.844362	17.003837	1.201152
-901.249138	11.552422	1.206157
-905.402426	12.345487	1.211162
-909.000663	9.662609	1.216166
-912.964355	15.019498	1.221171
-916.682048	13.881096	1.226176
-920.446481	14.869114	1.231181
-924.019076	16.522045	1.236186
-927.718282	22.794262	1.241190
-931.698210	17.110052	1.246195
-935.577567	21.347700	1.251200
-938.765873	17.850845	1.256205
-942.802217	14.266700	1.261210
-946.583290	11.103308	1.266214
-950.088226	19.085216	1.271219
-953.956057	16.385505	1.276224
-957.703012	18.612302	1.281229
-961.650058	9.113953	1.286234
-965.470030	3.111818	1.291238
-969.075720	14.973239	1.296243
-973.350965	13.297497	1.301248
-976.832373	6.554798	1.306253
-980.413300	15.350238	1.311258
-984.028684	14.683767	1.316262
-988.061938	14.462828	1.321267
-992.091267	17.678324	1.326272
-995.358660	12.418518	1.331277
-999.138286	12.068394	1.336282
-1002.951446	3.427301	1.341286
-1007.051782	13.834712	1.346291
-1011.171029	14.201278	1.351296
-1014.518812	17.319912	1.356301
-1018.416817	23.459372	1.361306
-1021.953331	20.456148	1.366310
-1025.227783	26.150293	1.371315
-1029.261072	26.232533	1.376320
-1033.142117	17.708503	1.381325
-1036.682066	29.940377	1.386330
-1040.604437	22.849918	1.391334
-1044.499180	19.249454	1.396339
-1048.274709	19.491914	1.401344
-1051.567161	12.182009	1.406349
-1056.118793	19.301685	1.411354
-1059.750155	19.254949	1.416358
-1063.554269	23.863837	1.421363
-1067.402325	22.606251	1.426368
-1070.831814	19.469044	1.431373
-1074.429452	21.337566	1.436378
-1078.084783	16.202458	1.441382
-1081.904885	15.757524	1.446387
-1086.127055	22.124004	1.451392
-1089.431631	13.326196	1.456397
-1093.191847	11.342291	1.461402
-1096.988368	14.847488	1.466406
-1100.915989	12.481446	1.471411
-1104.768507	19.946091	1.476416
-1108.292220	12.769884	1.481421
-1112.489205	21.782910	1.486426
-1115.881369	8.067919	1.491430
-1119.562019	15.008890	1.496435
-1123.199555	20.392451	1.501440
-1126.741065	17.233083	1.506445
-1130.944570	21.881007	1.511450
-1134.720938	13.990373	1.516454
-1138.478870	12.344380	1.521459
-1142.547921	16.090215	1.526464
-1146.025069	12.133953	1.531469
-1150.168367	18.574967	1.536474
-1153.181873	10.727419	1.541478
-1157.052295	7.405105	1.546483
-1160.758317	18.235951	1.551488
-1164.488167	15.665099	1.556493
-1168.905251	22.484700	1.561498
-1172.422176	11.565968	1.566502
-1176.088086	14.950916	1.571507
-1179.936247	22.619333	1.576512
-1183.487019	11.493283	1.581517
-1187.641387	18.962862	1.586522
-1191.119734	15.092101	1.591526
-1195.018209	16.509924	1.596531
-1198.720684	20.400869	1.601536
-1202.261641	15.377672	1.606541
-1206.141277	16.643071	1.611546
-1209.887704	11.176785	1.616550
-1214.067159	25.232022	1.621555
-1217.281459	18.726665	1.626560
-1220.846923	9.146081	1.631565
-1225.381001	16.488681	1.636570
-1228.695716	13.953560	1.641574
-1232.634702	14.189916	1.646579
-1236.284294	14.290135	1.651584
-1239.964245	20.129460	1.656589
-1243.494952	20.008362	1.661594
-1247.850064	9.927154	1.666598
-1251.304430	16.495446	1.671603
-1255.340995	21.369401	1.676608
-1258.874005	16.657496	1.681613
-1262.715428	18.335167	1.686618
-1265.881870	16.756637	1.691622
-1270.006597	14.912071	1.696627
-1274.357868	19.476964	1.701632
-1277.677967	13.572811	1.706637
-1281.297232	14.074013	1.711642
-1285.005326	9.091833	1.716646
-1289.084319	12.754649	1.721651
-1292.593524	19.811959	1.726656
-1296.067382	10.299785	1.731661
-1300.246852	14.042626	1.736666
-1303.963695	11.209954	1.741670
-1307.632405	16.629804	1.746675
-1311.847669	21.021386	1.751680
-1315.220375	9.527802	1.756685
-1318.928871	19.674775	1.761690
-1322.586975	12.396332	1.766694
-1326.534565	14.482264	1.771699
-1330.323663	12.709573	1.776704
-1333.755838	15.629803	1.781709
-1337.848350	15.881971	1.786714
-1341.645342	20.748799	1.791718
-1345.524967	15.574708	1.796723
-1349.248134	15.310720	1.801728
-1352.523693	20.816617	1.806733
-1356.933087	17.326170	1.811738
-1360.116956	12.515704	1.816742
-1363.932909	11.945588	1.821747
-1367.962209	15.755061	1.826752
-1371.998759	6.869703	1.831757
-1375.395101	16.243946	1.836762
-1379.465516	11.929175	1.841766
-1382.935304	10.820837	1.846771
-1386.672772	13.825127	1.851776
-1390.119044	14.172373	1.856781
-1394.429105	15.483463	1.861786
-1398.512077	15.669320	1.866790
-1401.565326	6.378261	1.871795
-1405.539986	13.629681	1.876800
-1408.842897	10.518779	1.881805
-1412.668230	7.788521	1.886810
-1416.754204	8.135951	1.891814
-1420.669903	13.648449	1.896819
-1424.573838	20.854189	1.901824
-1427.924078	1.108711	1.906829
-1431.893977	12.605566	1.911834
-1435.688446	12.212994	1.916838
-1439.094564	9.514158	1.921843
-1443.201639	15.845804	1.926848
-1446.688795	12.312279	1.931853
-1450.733455	19.958630	1.936858
-1454.638665	7.962627	1.941862
-1458.234893	18.905880	1.946867
-1462.064455	15.459611	1.951872
-1465.631430	15.988300	1.956877
-1469.346906	22.535701	1.961882
-1473.370928	16.279002	1.966886
-1476.719013	11.314490	1.971891
-1480.936510	18.431264	1.976896
-1484.276838	20.049887	1.981901
-1488.085806	19.673274	1.986906
-1492.030226	23.053052	1.991910
-1495.489165	4.396753	1.996915
-1499.743837	21.905155	2.006912
-1500.918962	20.200106	2.016909
-1498.260413	16.406550	2.026906
-1495.184012	12.498921	2.036902
-1493.147031	17.263719	2.046899
-1491.407246	14.267067	2.056896
-1489.426147	21.753004	2.066893
-1487.631466	20.205247	2.076890
-1485.388044	19.747847	2.086886
-1483.365988	15.839565	2.096883
-1481.739058	16.450022	2.106880
-1480.127737	6.398423	2.116877
-1478.001405	13.734525	2.126874
-1476.231189	12.884174	2.136870
-1474.434474	9.428791	2.146867
-1472.230562	15.699916	2.156864
-1470.290032	14.427865	2.166861
-1468.518950	12.711464	2.176858
-1466.761894	13.835080	2.186854
-1464.723790	10.764663	2.196851
-1462.693748	11.046221	2.206848
-1461.017925	10.067051	2.216845
-1459.146232	8.051981	2.226842
-1457.117200	0.747663	2.236838
-1455.437243	2.178565	2.246835
-1453.310084	5.892044	2.256832
-1451.727224	12.044997	2.266829
-1449.502671	8.815694	2.276826
-1447.744831	8.746045	2.286822
-1446.135914	9.525203	2.296819
-1444.250541	11.528655	2.306816
-1442.053191	12.147841	2.316813
-1440.105773	15.933704	2.326810
-1438.499707	17.333045	2.336806
-1436.636757	12.420619	2.346803
-1434.413041	17.769502	2.356800
-1432.602719	16.981442	2.366797
-1430.791935	12.023441	2.376794
-1429.073391	17.101049	2.386790
-1426.767179	10.513856	2.396787
-1425.253023	14.617209	2.406784
-1423.568773	16.088095	2.416781
-1421.404085	11.279949	2.426778
-1419.550883	11.895033	2.436774
-1417.562464	8.037219	2.446771
-1415.739664	12.480790	2.456768
-1413.876916	9.544064	2.466765
-1412.248911	14.989760	2.476762
-1410.278893	11.794715	2.486758
-1408.246043	8.538292	2.496755
-1406.418431	8.712771	2.506752
-1404.355293	7.348156	2.516749
-1402.664800	4.459996	2.526746
-1400.606608	3.664544	2.536742
-1399.061710	6.090096	2.546739
-1396.964330	6.425724	2.556736
-1394.985587	2.060553	2.566733
-1393.219334	13.361258	2.576730
-1391.209848	13.380801	2.586726
-1389.435198	4.069462	2.596723
-1387.568672	4.135300	2.606720
-1385.727965	9.953116	2.616717
-1384.086408	8.337250	2.626714
-1381.859679	10.533053	2.636710
-1379.773751	11.696252	2.646707
-1378.319774	10.616898	2.656704
-1376.431894	11.926357	2.666701
-1374.638140	18.450584	2.676698
-1372.235015	13.494401	2.686694
-1370.634031	11.204958	2.696691
-1368.757846	11.597566	2.706688
-1367.115092	15.428290	2.716685
-1365.017242	15.357973	2.726682
-1363.185454	15.987827	2.736678
-1361.611586	10.376163	2.746675
-1359.070070	14.923554	2.756672
-1357.350304	13.576444	2.766669
-1355.732080	17.203902	2.776666
-1353.842305	11.903942	2.786662
-1352.036226	9.041791	2.796659
-1350.140571	10.805604	2.806656
-1348.350641	16.247623	2.816653
-1345.922612	14.872922	2.826650
-1344.485751	8.367909	2.836646
-1342.331741	10.834297	2.846643
-1340.679575	10.355227	2.856640
-1338.961807	12.966501	2.866637
-1336.992225	9.867600	2.876634
-1334.724010	5.235368	2.886630
-1333.108665	12.293754	2.896627
-1331.326356	11.428740	2.906624
-1329.337813	12.201230	2.916621
-1327.495422	8.511999	2.926618
-1325.368535	14.547064	2.936614
-1323.856694	12.136600	2.946611
-1322.046058	11.148162	2.956608
-1319.788588	15.473647	2.966605
-1317.994971	9.469354	2.976602
-1316.422865	12.599275	2.986598
-1314.406068	18.575400	2.996595
-1312.680602	15.035491	3.006592
-1310.727629	11.804291	3.016589
-1309.035745	15.285141	3.026586
-1306.713698	14.655458	3.036582
-1304.781723	15.341639	3.046579
-1302.824348	15.450403	3.056576
-1301.664941	11.690763	3.066573
-1299.265909	15.204292	3.076570
-1297.252691	15.149731	3.086566
-1295.733251	17.535040	3.096563
-1293.675783	20.205367	3.106560
-1291.893455	13.918074	3.116557
-1290.106631	17.399225	3.126554
-1288.034251	17.317512	3.136550
-1286.059028	12.972750	3.146547
-1284.184045	15.391453	3.156544
-1282.810351	12.151075	3.166541
-1280.426796	18.843979	3.176538
-1278.466045	13.646074	3.186534
-1276.845264	14.908580	3.196531
-1274.863484	19.295275	3.206528
-1273.117105	16.216556	3.216525
-1271.437227	17.471682	3.226522
-1269.008212	16.340304	3.236518
-1267.361701	9.320704	3.246515
-1265.815922	15.835406	3.256512
-1263.899525	16.663396	3.266509
-1261.872944	14.850634	3.276506
-1259.847615	17.202031	3.286502
-1257.885178	14.916944	3.296499
-1256.121131	12.085762	3.306496
-1254.340637	9.834297	3.316493
-1252.211945	13.629039	3.326490
-1250.576903	12.781051	3.336486
-1248.650197	18.000838	3.346483
-1246.982961	21.916334	3.356480
-1244.980409	19.578124	3.366477
-1242.679247	14.405159	3.376474
-1241.284197	17.224453	3.386470
-1239.407614	12.269056	3.396467
-1237.625099	9.140277	3.406464
-1235.534354	15.357865	3.416461
-1233.757436	16.316926	3.426458
-1231.548109	15.519312	3.436454
-1229.715154	16.975016	3.446451
-1228.209036	19.165429	3.456448
-1226.234291	19.504816	3.466445
-1224.243184	8.780622	3.476442
-1222.470103	15.421504	3.486438
-1220.526194	15.776860	3.496435
-1218.200776	17.361409	3.506432
-1216.844247	12.627334	3.516429
-1215.059618	17.495692	3.526426
-1213.302262	17.223481	3.536422
-1210.960916	12.026243	3.546419
-1209.135568	19.307489	3.556416
-1207.040908	14.413851	3.566413
-1205.533916	13.048408	3.576410
-1203.669176	9.143160	3.586406
-1201.860536	17.339820	3.596403
-1199.680532	16.082490	3.606400
-1198.071576	19.885896	3.616397
-1196.046648	20.221421	3.626394
-1194.296396	13.187584	3.636390
-1192.020191	17.923714	3.646387
-1190.832569	12.415978	3.656384
-1188.698677	23.598734	3.666381
-1186.910531	21.374830	3.676378
-1184.811207	18.446577	3.686374
-1183.003844	17.109786	3.696371
-1180.875626	20.800710	3.706368
-1179.292476	15.253508	3.716365
-1177.474529	21.223546	3.726362
-1175.649320	19.727190	3.736358
-1173.252640	21.648104	3.746355
-1171.416816	11.465159	3.756352
-1169.842692	15.589145	3.766349
-1168.265339	15.481445	3.776346
-1166.004205	13.340340	3.786342
-1164.054097	7.549914	3.796339
-1162.461522	15.043466	3.806336
-1160.670752	16.922208	3.816333
-1158.455915	15.005238	3.826330
-1156.707811	12.151933	3.836326
-1154.983766	11.691813	3.846323
-1152.788823	16.459705	3.856320
-1150.860162	9.634746	3.866317
-1149.417525	14.493490	3.876314
-1147.216303	7.630818	3.886310
-1145.460142	14.094427	3.896307
-1143.490792	13.289456	3.906304
-1141.507580	12.542968	3.916301
-1139.828972	11.399433	3.926298
-1138.074374	9.201071	3.936294
-1136.248260	14.962239	3.946291
-1134.249615	15.815687	3.956288
-1132.295457	15.610890	3.966285
-1130.414250	15.098894	3.976282
-1128.333473	10.779942	3.986278
-1126.414452	6.249270	3.996275
-1125.047852	8.115892	4.006272
-1123.023867	5.512823	4.016269
-1120.949687	9.737501	4.026266
-1119.335382	7.565609	4.036262
-1117.421180	3.486705	4.046259
-1114.956704	4.028578	4.056256
-1113.574822	8.694628	4.066253
-1111.977312	5.313905	4.076250
-1109.910201	9.626749	4.086246
-1107.856908	6.554281	4.096243
-1105.765067	12.670974	4.106240
-1104.005380	10.005007	4.116237
-1102.442335	12.459574	4.126234
-1100.299240	9.536887	4.136230
-1098.393585	11.732649	4.146227
-1096.676452	8.335342	4.156224
-1094.964530	10.628000	4.166221
-1092.777132	11.155415	4.176218
-1091.227236	10.430001	4.186214
-1088.996426	10.269410	4.196211
-1087.194652	6.570254	4.206208
-1085.422148	13.468585	4.216205
-1083.601293	15.339033	4.226202
-1081.565295	13.153634	4.236198
-1079.795149	5.869019	4.246195
-1077.865124	7.835336	4.256192
-1075.772608	14.464520	4.266189
-1074.211557	10.785755	4.276186
-1072.483181	12.725440	4.286182
-1070.532600	13.317637	4.296179
-1068.158320	6.245861	4.306176
-1066.745060	6.358051	4.316173
-1064.715134	8.590192	4.326170
-1062.733310	10.431430	4.336166
-1061.159468	6.364748	4.346163
-1059.188316	3.722168	4.356160
-1057.159320	9.417316	4.366157
-1055.611975	12.747224	4.376154
-1053.414695	12.801080	4.386150
-1051.426336	9.090848	4.396147
-1049.712016	7.827394	4.406144
-1048.055575	4.712827	4.416141
-1045.948997	6.549252	4.426138
-1044.073533	2.209470	4.436134
-1042.045145	7.194930	4.446131
-1040.404232	14.972301	4.456128
-1038.365937	11.710760	4.466125
-1036.672857	13.505550	4.476122
-1035.016661	13.829767	4.486118
-1032.834386	15.356398	4.496115
-1030.852191	17.217744	4.506112
-1029.176990	17.208303	4.516109
-1027.253127	18.889174	4.526106
-1025.380236	12.393563	4.536102
-1023.255212	13.182683	4.546099
-1021.634219	10.938144	4.556096
-1019.760623	17.178513	4.566093
-1017.740781	18.668622	4.576090
-1016.159239	13.788470	4.586086
-1013.974768	13.324051	4.596083
-1011.959427	10.582215	4.606080
-1010.357527	16.389844	4.616077
-1008.716394	17.618532	4.626074
-1006.842363	10.349697	4.636070
-1004.578830	5.705387	4.646067
-1002.646950	8.108919	4.656064
-1000.763617	12.998372	4.666061
-999.181434	12.494694	4.676058
-997.440293	10.317668	4.686054
-995.288483	9.332444	4.696051
-993.332303	7.289233	4.706048
-991.510421	15.203918	4.716045
-989.861060	6.482923	4.726042
-987.805168	14.813509	4.736038
-985.845709	13.038481	4.746035
-984.272386	11.825343	4.756032
-982.144959	19.025598	4.766029
-980.215115	15.982679	4.776026
-978.331871	18.843931	4.786022
-976.582088	13.792236	4.796019
-974.727249	12.554879	4.806016
-972.880550	9.331398	4.816013
-970.920449	11.317896	4.826010
-968.962477	13.055381	4.836006
-966.982601	12.577896	4.846003
-965.337509	12.606846	4.856000
-963.576860	5.651137	4.865997
-961.528527	10.304400	4.875994
-959.393872	16.883339	4.885990
-958.097292	12.442596	4.895987
-955.946428	13.667581	4.905984
-953.950589	12.840759	4.915981
-952.046447	4.905192	4.925978
-950.292720	5.142746	4.935974
-948.645904	10.147522	4.945971
-946.669345	11.554196	4.955968
-944.429835	6.278537	4.965965
-942.835841	14.852852	4.975962
-940.888754	9.345213	4.985958
-938.466275	8.302485	4.995955
-937.151048	7.116677	5.005952
-935.134626	8.621244	5.015949
-933.535676	13.649264	5.025946
-931.606578	12.916509	5.035942
-929.907810	17.323512	5.045939
-927.989105	13.579048	5.055936
-925.893757	17.208566	5.065933
-924.094073	12.992497	5.075930
-921.967841	13.288631	5.085926
-920.164955	15.132992	5.095923
-918.323686	6.064090	5.105920
-916.639532	13.360631	5.115917
-914.964322	10.626639	5.125914
-912.611756	8.892844	5.135910
-910.813085	15.362707	5.145907
-908.680745	9.533588	5.155904
-906.815435	6.664606	5.165901
-905.241900	10.098366	5.175898
-903.815936	11.260881	5.185894
-901.600570	13.134825	5.195891
-899.486915	13.461980	5.205888
-897.814779	9.904109	5.215885
-895.566299	11.500862	5.225882
-893.987112	10.998526	5.235878
-892.290823	12.728010	5.245875
-890.168789	8.834839	5.255872
-888.505114	9.624970	5.265869
-886.297702	10.457322	5.275866
-884.124621	9.747126	5.285862
-882.707774	3.620335	5.295859
-880.581510	15.520712	5.305856
-879.248500	8.509203	5.315853
-877.494762	12.770443	5.325850
-875.414967	12.214984	5.335846
-873.403569	4.919458	5.345843
-871.017398	9.962552	5.355840
-869.383104	5.779639	5.365837
-868.120176	10.949941	5.375834
-865.712178	18.778310	5.385830
-863.839848	7.600376	5.395827
-862.387104	4.470252	5.405824
-860.348754	11.467312	5.415821
-858.321357	9.248711	5.425818
-856.493934	14.217390	5.435814
-854.206751	10.999760	5.445811
-852.572589	20.031600	5.455808
-851.199164	7.975383	5.465805
-849.034984	11.871354	5.475802
-846.952459	7.719796	5.485798
-845.446809	11.143891	5.495795
-843.358292	11.384490	5.505792
-841.442128	19.069655	5.515789
-839.415162	20.407657	5.525786
-837.641150	13.420447	5.535782
-835.816451	11.371812	5.545779
-834.026658	19.790055	5.555776
-832.069237	15.559592	5.565773
-830.092939	6.381780	5.575770
-828.431369	11.910896	5.585766
-826.493675	18.518185	5.595763
-824.572797	9.780273	5.605760
-823.000353	12.857772	5.615757
-820.700977	19.314061	5.625754
-818.337295	19.679359	5.635750
-817.056022	19.349517	5.645747
-815.202422	16.948141	5.655744
-813.368415	13.619008	5.665741
-811.193165	14.897978	5.675738
-809.725539	17.049311	5.685734
-807.835442	13.422838	5.695731
-805.608166	13.237311	5.705728
-803.808367	18.163728	5.715725
-802.042294	11.965552	5.725722
-800.316407	20.713719	5.735718
-798.422958	9.297818	5.745715
-796.548688	14.201179	5.755712
-794.663538	18.296836	5.765709
-792.607150	19.019996	5.775706
-791.033576	18.607189	5.785702
-789.046448	17.063440	5.795699
-786.845743	14.098208	5.805696
-784.892993	20.019217	5.815693
-783.359227	20.327791	5.825690
-781.076614	18.851103	5.835686
-779.484057	12.830922	5.845683
-777.780682	12.619136	5.855680
-775.919974	14.158806	5.865677
-773.877131	17.873692	5.875674
-772.085711	15.899956	5.885670
-770.144078	21.045892	5.895667
-768.249842	16.936958	5.905664
-766.401278	18.198512	5.915661
-764.801067	18.035660	5.925658
-762.693481	19.019187	5.935654
-760.725112	12.241702	5.945651
-758.592158	19.572743	5.955648
-756.889841	22.564746	5.965645
-755.014587	15.511180	5.975642
-753.215981	17.325126	5.985638
-751.426596	15.577809	5.995635
-749.588086	13.513401	6.005632
-747.533471	13.294303	6.015629
-746.067911	13.678225	6.025626
-744.131036	14.357105	6.035622
-741.980897	19.285077	6.045619
-740.080827	10.333793	6.055616
-738.190967	10.816419	6.065613
-736.364825	16.535095	6.075610
-734.154321	18.617056	6.085606
-732.900700	10.384953	6.095603
-730.734312	11.671413	6.105600
-728.865587	18.147918	6.115597
-727.143884	18.737662	6.125594
-724.965553	12.581000	6.135590
-723.036169	16.358856	6.145587
-721.505847	16.997651	6.155584
-719.636371	18.341002	6.165581
-717.748465	22.774922	6.175578
-715.625939	23.740100	6.185574
-713.764709	22.025917	6.195571
-711.970010	15.421716	6.205568
-710.081449	14.202790	6.215565
-708.212533	20.740136	6.225562
-706.110990	15.991368	6.235558
-704.489084	16.734201	6.245555
-702.553161	19.906665	6.255552
-701.024205	17.150422	6.265549
-698.959183	17.081324	6.275546
-696.875373	17.014535	6.285542
-694.987371	14.984337	6.295539
-693.039705	20.975429	6.305536
-691.239738	20.462152	6.315533
-689.819122	18.133157	6.325530
-687.866453	17.914193	6.335526
-685.439910	13.740816	6.345523
-683.685809	12.561970	6.355520
-681.791757	20.118223	6.365517
-680.120407	13.713443	6.375514
-678.491957	16.104784	6.385510
-676.185780	20.391457	6.395507
-674.399368	15.770687	6.405504
-672.742209	20.754447	6.415501
-670.563139	12.634261	6.425498
-668.545825	12.894277	6.435494
-666.702608	13.385335	6.445491
-665.032896	9.690031	6.455488
-663.582171	14.796166	6.465485
-661.444508	15.595945	6.475482
-659.720053	18.178701	6.485478
-657.443100	11.222226	6.495475
-655.533459	16.059119	6.505472
-653.679590	26.829444	6.515469
-651.982547	18.345390	6.525466
-650.114598	21.582503	6.535462
-648.070340	17.817791	6.545459
-646.193441	17.145892	6.555456
-644.448057	18.933449	6.565453
-642.722987	21.489233	6.575450
-640.619686	18.515095	6.585446
-638.875845	9.307682	6.595443
-637.010337	11.991128	6.605440
-635.141378	12.671041	6.615437
-633.344429	13.518631	6.625434
-631.312448	16.202759	6.635430
-629.020513	13.973249	6.645427
-627.301530	14.487222	6.655424
-625.876211	10.007873	6.665421
-623.538359	16.297220	6.675418
-621.930768	17.250423	6.685414
-619.679140	16.843050	6.695411
-618.057876	17.589978	6.705408
-616.276103	14.863495	6.715405
-614.803106	17.226206	6.725402
-612.439828	18.463923	6.735398
-610.586534	17.727718	6.745395
-608.678983	16.632834	6.755392
-607.157861	15.856406	6.765389
-604.833557	13.345494	6.775386
-603.514447	20.813113	6.785382
-601.338938	19.448166	6.795379
-599.098600	14.190700	6.805376
-597.513397	7.548189	6.815373
-595.865580	6.105037	6.825370
-593.809582	9.845025	6.835366
-591.794823	2.909465	6.845363
-589.776525	5.671446	6.855360
-588.044599	2.846821	6.865357
-586.134759	5.064629	6.875354
-584.500986	6.849625	6.885350
-582.644175	5.405396	6.895347
-580.579262	6.433089	6.905344
-578.880453	6.298836	6.915341
-577.077253	1.464576	6.925338
-575.216222	5.258972	6.935334
-572.778280	8.019304	6.945331
-570.961358	2.953071	6.955328
-569.412342	0.711557	6.965325
-567.550817	5.484421	6.975322
-565.637368	4.186589	6.985318
-563.721699	7.549133	6.995315
-561.931226	2.104085	7.005312
-559.972381	4.053841	7.015309
-558.379895	6.437171	7.025306
-556.264628	5.793968	7.035302
-554.070580	6.360039	7.045299
-552.283697	7.787587	7.055296
-550.660586	10.237990	7.065293
-548.705385	8.316468	7.075290
-547.128756	6.751175	7.085286
-544.974893	12.429915	7.095283
-542.886797	7.808413	7.105280
-540.973642	9.939123	7.115277
-539.594556	13.946651	7.125274
-537.581872	9.217155	7.135270
-535.605418	6.660440	7.145267
-533.553090	2.369552	7.155264
-531.529283	7.437084	7.165261
-529.979514	10.677860	7.175258
-528.143909	7.742197	7.185254
-526.233943	7.602165	7.195251
-524.087723	1.285114	7.205248
-523.049118	0.789901	7.215245
-520.742285	-0.031988	7.225242
-518.509029	6.105027	7.235238
-516.614551	5.613941	7.245235
-515.023439	2.706004	7.255232
-513.183268	7.806634	7.265229
-510.983800	5.807254	7.275226
-509.489166	7.807831	7.285222
-507.382774	7.469697	7.295219
-505.936771	4.529354	7.305216
-503.742516	4.495480	7.315213
-501.567338	15.818591	7.325210
-499.998897	8.458113	7.335206
-497.972600	11.002585	7.345203
-496.117362	11.788459	7.355200
-494.300416	14.652615	7.365197
-492.278247	15.241094	7.375194
-490.682243	7.827278	7.385190
-488.818833	6.906403	7.395187
-486.814222	8.609238	7.405184
-484.581285	11.113521	7.415181
-482.674611	12.232436	7.425178
-481.655409	4.740529	7.435174
-479.484547	3.525038	7.445171
-477.142565	4.085133	7.455168
-475.716681	7.070534	7.465165
-473.766803	8.132638	7.475162
-471.901890	11.935903	7.485158
-469.838209	6.650314	7.495155
-468.010159	4.316301	7.505152
-466.161211	8.732517	7.515149
-464.460853	9.280182	7.525146
-462.030031	7.024161	7.535142
-460.618753	3.542417	7.545139
-458.487807	5.953946	7.555136
-456.652421	1.646955	7.565133
-454.867058	5.342939	7.575130
-453.273161	9.973256	7.585126
-450.884183	7.058483	7.595123
-449.522932	5.616330	7.605120
-447.099115	3.743691	7.615117
-445.500681	7.368598	7.625114
-443.923313	2.944233	7.635110
-441.776850	9.037692	7.645107
-440.076467	7.038601	7.655104
-437.866041	6.835205	7.665101
-436.158938	6.231650	7.675098
-434.384674	7.236558	7.685094
-432.115996	3.669778	7.695091
-430.514543	6.135799	7.705088
-428.614712	7.029059	7.715085
-426.830341	8.197830	7.725082
-425.001592	4.227921	7.735078
-423.124512	5.129432	7.745075
-421.198038	-1.264095	7.755072
-418.873231	3.825762	7.765069
-417.403606	1.116150	7.775066
-415.776645	5.142455	7.785062
-413.603724	2.408624	7.795059
-411.766240	10.698353	7.805056
-409.559636	8.846002	7.815053
-408.011768	16.026256	7.825050
-406.223509	11.953823	7.835046
-404.213738	9.243242	7.845043
-402.226589	6.604519	7.855040
-400.406993	1.223694	7.865037
-398.692512	5.214045	7.875034
-396.831166	10.877441	7.885030
-394.824164	2.290104	7.895027
-392.993368	2.143160	7.905024
-390.972531	-0.775614	7.915021
-389.251407	-2.705129	7.925018
-387.331618	0.652047	7.935014
-385.545975	2.473115	7.945011
-383.303242	5.284829	7.955008
-381.807389	5.868398	7.965005
-380.070615	6.931532	7.975002
-378.080349	9.279893	7.984998
-375.834261	5.557348	7.994995
-374.144925	6.894996	8.004992
-372.327336	8.213411	8.014989
-370.287180	15.124667	8.024986
-368.909185	5.296766	8.034982
-366.968453	7.998652	8.044979
-364.778975	5.451311	8.054976
-362.671396	9.567902	8.064973
-361.290499	15.122054	8.074970
-359.267963	10.041174	8.084966
-357.300335	9.929660	8.094963
-355.205794	10.254825	8.104960
-353.618023	7.985390	8.114957
-351.872197	10.334988	8.124954
-349.740431	14.698794	8.134950
-347.768737	7.314635	8.144947
-345.898419	10.475202	8.154944
-344.299845	5.252453	8.164941
-342.218540	13.712230	8.174938
-340.742904	10.264138	8.184934
-338.781083	10.152837	8.194931
-336.818162	11.929291	8.204928
-334.856037	11.586739	8.214925
-332.821622	12.353408	8.224922
-331.139572	14.815921	8.234918
-329.101984	15.164700	8.244915
-327.045930	10.781567	8.254912
-325.205705	5.139152	8.264909
-323.486939	9.553263	8.274906
-321.882060	11.744856	8.284902
-319.932565	8.707926	8.294899
-317.955640	6.086801	8.304896
-315.919447	10.067850	8.314893
-314.299771	13.161160	8.324890
-312.446016	10.279771	8.334886
-310.363234	16.451810	8.344883
-308.487651	9.378189	8.354880
-306.483030	8.218961	8.364877
-304.816498	14.417741	8.374874
-302.936098	13.744989	8.384870
-301.056604	17.839084	8.394867
-298.921421	11.590410	8.404864
-297.409126	13.683676	8.414861
-295.261450	11.630047	8.424858
-293.851874	13.148111	8.434854
-291.633868	7.227096	8.444851
-289.735926	6.775824	8.454848
-287.670912	4.266861	8.464845
-286.144311	5.331699	8.474842
-284.338918	6.700063	8.484838
-282.176722	13.156487	8.494835
-279.957589	5.918823	8.504832
-278.564290	9.875394	8.514829
-276.697882	15.950981	8.524826
-274.862362	13.616154	8.534822
-272.957916	4.714074	8.544819
-270.983109	5.647105	8.554816
-269.173168	4.851289	8.564813
-267.164793	14.237354	8.574810
-265.383102	8.748857	8.584807
-263.588206	6.179132	8.594803
-261.469865	5.019784	8.604800
-259.606132	4.544355	8.614797
-258.040662	7.790051	8.624794
-256.099671	10.897435	8.634791
-254.054207	9.161324	8.644787
-252.173753	11.179209	8.654784
-250.301793	8.961054	8.664781
-248.616870	14.073025	8.674778
-246.385008	8.228696	8.684775
-244.769857	6.048662	8.694771
-242.860843	7.549059	8.704768
-240.971439	10.445953	8.714765
-238.977860	9.923364	8.724762
-237.131595	8.419428	8.734759
-235.660535	11.521659	8.744755
-233.370983	13.178114	8.754752
-231.342230	6.744188	8.764749
-229.505963	5.618610	8.774746
-228.139068	5.199556	8.784743
-226.161932	6.432572	8.794739
-224.026312	-0.661507	8.804736
-221.997568	-0.668436	8.814733
-220.668064	0.397030	8.824730
-218.194979	6.024753	8.834727
-216.648342	4.585257	8.844723
-214.810153	5.752394	8.854720
-212.703401	2.886935	8.864717
-210.791271	-1.553668	8.874714
-208.796936	5.961908	8.884711
-207.503857	-0.739863	8.894707
-205.522996	2.099862	8.904704
-203.853941	3.090500	8.914701
-201.563472	8.010106	8.924698
-199.588557	2.182203	8.934695
-198.091141	7.171426	8.944691
-195.933965	7.994962	8.954688
-194.075721	6.988146	8.964685
-192.104241	7.296157	8.974682
-190.116828	7.207408	8.984679
-188.501456	9.182650	8.994675
-186.631739	14.465305	9.004672
-184.638377	14.911054	9.014669
-182.731793	3.167433	9.024666
-181.138105	11.508970	9.034663
-179.011731	9.341272	9.044659
-177.159001	4.310534	9.054656
-175.554337	10.679252	9.064653
-173.528766	12.828000	9.074650
-171.450998	10.907747	9.084647
-169.789818	14.882045	9.094643
-168.048511	6.426905	9.104640
-165.804369	13.530140	9.114637
-164.004890	12.170605	9.124634
-162.206616	12.505173	9.134631
-160.160682	8.393380	9.144627
-158.531664	4.703645	9.154624
-156.695002	2.882845	9.164621
-154.624267	7.761513	9.174618
-152.651843	12.776398	9.184615
-150.900362	7.276522	9.194611
-148.889880	3.725303	9.204608
-147.334949	5.248523	9.214605
-145.463666	7.879426	9.224602
-143.528513	4.626472	9.234599
-141.536172	3.213717	9.244595
-139.595839	0.672847	9.254592
-137.684509	7.654927	9.264589
-135.839216	14.729355	9.274586
-134.489241	8.389342	9.284583
-132.099507	8.064052	9.294579
-130.169733	7.419659	9.304576
-128.345283	4.529139	9.314573
-126.442226	8.371865	9.324570
-124.975241	16.367608	9.334567
-122.901266	15.797688	9.344563
-120.750721	16.245362	9.354560
-118.982118	13.342684	9.364557
-117.163857	11.515568	9.374554
-115.265311	17.250974	9.384551
-113.427419	12.665838	9.394547
-111.761337	15.836242	9.404544
-109.483595	10.494327	9.414541
-108.019912	17.303415	9.424538
-105.804011	12.932877	9.434535
-103.880228	10.754108	9.444531
-102.010133	18.468504	9.454528
-100.099392	18.003654	9.464525
-98.558410	20.495588	9.474522
-96.468554	21.192787	9.484519
-94.625727	19.693843	9.494515
-93.083861	18.355589	9.504512
-90.936143	16.118664	9.514509
-89.033242	16.338491	9.524506
-87.228231	15.671642	9.534503
-85.418271	15.389675	9.544499
-83.148740	21.734535	9.554496
-81.296605	18.050431	9.564493
-79.674689	15.192286	9.574490
-77.860114	19.741048	9.584487
-75.929756	22.182822	9.594483
-73.985693	17.037256	9.604480
-71.792202	12.817991	9.614477
-70.573894	18.528181	9.624474
-68.635328	24.849179	9.634471
-66.269455	14.771706	9.644467
-64.619364	13.526750	9.654464
-62.957432	8.634291	9.664461
-60.377434	17.171542	9.674458
-58.997339	9.379494	9.684455
-57.226819	10.144906	9.694451
-55.376959	15.460274	9.704448
-53.306169	13.455112	9.714445
-51.408567	18.486040	9.724442
-50.123752	19.686878	9.734439
-47.925778	19.077155	9.744435
-45.570483	14.714357	9.754432
-43.872149	10.902902	9.764429
-42.100262	20.577446	9.774426
-40.289896	21.682637	9.784423
-38.534242	16.563857	9.794419
-36.496894	17.109629	9.804416
-34.590186	16.162939	9.814413
-32.662267	16.941683	9.824410
-31.072605	16.505832	9.834407
-28.845103	23.799732	9.844403
-26.997618	13.774407	9.854400
-25.084589	15.595917	9.864397
-23.233053	19.698886	9.874394
-21.359304	12.785342	9.884391
-19.790817	10.113040	9.894387
-17.905787	10.860018	9.904384
-15.793223	13.274132	9.914381
-13.937986	17.693829	9.924378
-12.039610	17.560746	9.934375
-10.058771	14.235194	9.944371
-8.454893	13.424620	9.954368
-6.535388	16.330292	9.964365
-4.583198	14.810656	9.974362
-2.885445	28.367500	9.984359
-1.938107	61.117914	9.994355
-0.763286	108.129588	10.004352
0.000000	157.146333	10.009357
0.860296	193.452714	10.014362
1.307526	231.744774	10.019367
1.942875	252.821051	10.024371
1.860093	291.047431	10.029376
2.407243	310.254131	10.034381
2.671589	336.052602	10.039386
2.696243	353.892824	10.044391
3.172178	362.954877	10.049395
3.363627	375.067560	10.054400
3.656871	383.993194	10.059405
3.956847	390.246210	10.064410
3.917121	395.751059	10.069415
3.872761	399.467436	10.074419
3.913362	405.959922	10.079424
4.174694	408.777211	10.084429
4.537214	417.977948	10.089434
4.200371	412.669838	10.094439
4.615151	404.036012	10.099443
4.054600	411.717846	10.104448
3.959464	399.464627	10.109453
4.061111	401.722344	10.114458
4.038868	418.379018	10.119463
3.764659	423.248714	10.124467
4.046670	426.447708	10.129472
4.227935	423.879728	10.134477
4.445163	432.495146	10.139482
3.985171	438.702835	10.144487
4.583010	446.151333	10.149491
4.636731	466.241746	10.154496
4.625016	456.695790	10.159501
4.795666	470.853223	10.164506
4.807597	478.979282	10.169511
4.655748	478.172032	10.174515
4.801871	475.029038	10.179520
4.732611	478.510500	10.184525
4.813865	477.548419	10.189530
4.616423	486.715344	10.194535
4.925588	473.603300	10.199539
4.877264	478.200606	10.204544
4.584503	484.265564	10.209549
4.917400	483.890708	10.214554
5.099190	508.879834	10.219559
5.504153	508.394730	10.224563
5.092822	513.751369	10.229568
5.459923	513.610245	10.234573
5.470968	513.628457	10.239578
5.392898	525.491821	10.244583
5.578258	516.080191	10.249587
5.312959	517.697048	10.254592
5.364656	524.037292	10.259597
5.432065	523.549671	10.264602
5.251378	526.711182	10.269607
5.565345	524.105039	10.274611
5.439268	531.020090	10.279616
5.699164	543.386029	10.284621
6.145724	551.156954	10.289626
5.682519	545.247194	10.294631
6.061483	549.399823	10.299635
5.824107	550.835455	10.304640
6.376779	561.374553	10.309645
6.004837	551.255981	10.314650
5.692670	556.770100	10.319655
6.174993	561.452494	10.324659
6.172398	569.163471	10.329664
6.107812	580.618787	10.334669
6.574255	574.445412	10.339674
6.194477	580.203230	10.344679
6.580854	573.285711	10.349683
6.372963	579.059845	10.354688
6.587718	576.369655	10.359693
6.681931	585.085985	10.364698
6.109894	585.974281	10.369703
6.200054	576.485387	10.374707
6.235309	590.438387	10.379712
6.513016	584.788801	10.384717
6.491926	582.079049	10.389722
6.436061	589.130110	10.394727
6.506538	588.961295	10.399731
6.656312	605.117767	10.404736
6.885459	609.453595	10.409741
7.039069	615.313388	10.414746
6.632600	620.344765	10.419751
6.749910	614.729775	10.424755
6.936048	615.193610	10.429760
6.826052	613.599593	10.434765
7.188408	615.207525	10.439770
6.833289	621.565062	10.444775
6.706022	618.108134	10.449779
7.104276	638.206404	10.454784
7.410845	644.732333	10.459789
7.885816	641.981726	10.464794
7.316952	645.423364	10.469799
7.391189	636.834773	10.474803
7.612506	655.278314	10.479808
7.523223	648.090222	10.484813
7.685888	645.036328	10.489818
7.337319	656.683678	10.494823
7.830403	654.040092	10.499827
7.645324	660.328227	10.504832
7.702954	660.083063	10.509837
8.152443	660.381749	10.514842
7.798597	664.486376	10.519847
8.098619	663.153229	10.524851
8.395734	664.784983	10.529856
7.807607	659.286984	10.534861
7.968481	650.778660	10.539866
7.812850	666.108897	10.544871
8.338231	667.071529	10.549875
8.199622	672.788425	10.554880
8.085710	674.884594	10.559885
8.616775	670.119937	10.564890
8.380859	673.821855	10.569895
8.722343	667.334744	10.574899
8.583206	653.027603	10.579904
8.130356	649.518732	10.584909
8.190282	651.882321	10.589914
8.534316	672.444657	10.594919
8.614600	670.873271	10.599923
8.158534	676.241583	10.604928
8.054928	673.453596	10.609933
8.106349	677.329665	10.614938
8.036426	681.653241	10.619943
8.279065	689.257099	10.624947
8.727996	703.379266	10.629952
8.884671	710.684855	10.634957
8.690985	703.421876	10.639962
8.617722	712.165019	10.644967
9.034153	710.176790	10.649971
8.829644	718.350741	10.654976
9.090616	708.590512	10.659981
9.297332	706.712845	10.664986
9.088561	716.057501	10.669991
8.923480	708.703169	10.674995
9.381851	712.528418	10.680000
9.130780	712.762095	10.685005
9.309639	714.808465	10.690010
8.823335	730.427562	10.695015
9.622251	744.314894	10.700019
9.609364	751.441157	10.705024
9.426352	748.185992	10.710029
9.764451	745.710672	10.715034
9.802517	756.206297	10.720039
9.992031	744.512280	10.725043
9.863691	728.741535	10.730048
9.642083	724.218412	10.735053
9.630308	724.854735	10.740058
9.815963	742.874239	10.745063
9.662580	748.227782	10.750067
9.962215	752.612354	10.755072
10.089507	750.297518	10.760077
10.272627	749.893470	10.765082
9.836250	764.507349	10.770087
10.159288	757.300219	10.775091
10.362297	757.837349	10.780096
10.047091	756.889939	10.785101
10.178882	759.613452	10.790106
9.787435	758.210175	10.795111
10.048044	755.730772	10.800115
9.954712	756.115427	10.805120
10.270765	759.172867	10.810125
10.360657	760.503457	10.815130
9.996985	762.188521	10.820135
10.121562	760.464271	10.825139
10.485032	774.330765	10.830144
11.059200	777.954996	10.835149
11.062349	779.045465	10.840154
10.805951	775.971821	10.845159
10.626083	767.792642	10.850163
10.618876	767.273203	10.855168
10.795215	777.946052	10.860173
10.948635	787.782852	10.865178
10.817613	784.565343	10.870183
10.885135	789.194982	10.875187
11.242388	788.136613	10.880192
11.391623	792.301855	10.885197
11.255671	792.708028	10.890202
11.207268	793.097217	10.895207
11.565385	781.279529	10.900211
11.053443	779.992434	10.905216
11.453266	775.783923	10.910221
11.641062	760.609062	10.915226
11.433205	766.642992	10.920231
10.999384	767.128263	10.925235
11.176828	779.811679	10.930240
11.029026	789.361448	10.935245
11.511194	794.463144	10.940250
10.898070	793.506813	10.945255
11.176551	795.505324	10.950259
11.426738	800.170751	10.955264
11.506513	793.444650	10.960269
12.114275	799.515193	10.965274
11.805096	803.046547	10.970279
11.891088	798.755263	10.975283
11.716615	796.175587	10.980288
11.773113	809.981064	10.985293
12.415058	806.709175	10.990298
12.201995	808.776573	10.995303
12.056756	794.579688	11.000307
12.449315	791.930421	11.005312
12.118001	797.443171	11.010317
12.452501	791.137599	11.015322
11.990590	801.981871	11.020327
12.241118	800.204048	11.025331
12.192471	798.398180	11.030336
12.049350	807.584005	11.035341
12.621549	819.645173	11.040346
12.458791	826.865062	11.045351
12.799067	822.060441	11.050355
12.698902	827.029891	11.055360
12.333452	812.339834	11.060365
12.501752	817.735349	11.065370
12.765190	827.473969	11.070375
12.678624	827.057740	11.075379
12.363652	822.225337	11.080384
12.733231	829.085535	11.085389
13.008459	828.811349	11.090394
12.772597	830.821080	11.095399
13.132941	832.452670	11.100403
13.025251	827.679461	11.105408
12.801761	825.040290	11.110413
12.980911	822.166297	11.115418
12.973964	839.353685	11.120423
13.116027	832.763333	11.125427
13.261450	830.853135	11.130432
13.261108	831.946180	11.135437
13.231025	826.521779	11.140442
12.716325	837.414599	11.145447
12.803071	831.340962	11.150451
13.134386	847.643004	11.155456
13.324463	860.250111	11.160461
13.216168	846.622364	11.165466
13.610935	865.941142	11.170471
13.847513	861.116000	11.175475
13.789493	849.162771	11.180480
13.574073	854.958824	11.185485
13.779792	862.929489	11.190490
13.349343	864.863247	11.195495
13.941381	858.245073	11.200499
14.044694	859.749027	11.205504
13.585638	860.334152	11.210509
14.050335	855.555557	11.215514
13.951893	859.355919	11.220519
14.023580	857.357704	11.225523
14.513450	856.408828	11.230528
14.239655	857.582707	11.235533
14.288395	852.548199	11.240538
14.171697	862.063074	11.245543
14.141323	862.525751	11.250547
14.371703	860.843349	11.255552
14.042095	864.245984	11.260557
14.224427	855.911895	11.265562
14.245212	867.604228	11.270567
14.301104	870.156435	11.275571
14.544998	883.561561	11.280576
14.470364	891.975043	11.285581
14.792986	883.809119	11.290586
14.802440	895.370392	11.295591
14.707338	891.385656	11.300595
15.177519	888.875431	11.305600
14.794687	872.640548	11.310605
14.849265	855.236881	11.315610
15.038296	862.544099	11.320615
14.622520	860.503542	11.325619
14.839699	875.460594	11.330624
14.743338	896.130709	11.335629
15.115129	896.604169	11.340634
15.189054	904.992976	11.345639
15.014908	894.543031	11.350643
14.986559	896.102720	11.355648
14.946897	887.089841	11.360653
15.149477	894.052517	11.365658
15.208855	900.131862	11.370663
15.453266	892.092633	11.375667
14.983807	900.103687	11.380672
15.329510	897.336123	11.385677
15.409923	892.849586	11.390682
15.387988	905.996366	11.395687
15.445710	897.605462	11.400691
15.452620	902.928416	11.405696
15.764008	922.679978	11.410701
16.027367	924.537021	11.415706
15.716008	918.226085	11.420711
15.730052	909.856874	11.425715
16.072491	920.527000	11.430720
15.892493	926.151217	11.435725
15.889663	908.107602	11.440730
15.721103	923.153732	11.445735
15.638271	927.488273	11.450739
15.898494	926.407848	11.455744
16.027805	934.015863	11.460749
15.875283	927.003088	11.465754
15.607468	929.685411	11.470759
16.097224	922.988827	11.475763
16.407574	928.936732	11.480768
16.383176	920.985025	11.485773
16.418716	924.259145	11.490778
16.265045	927.476893	11.495783
16.191515	923.804632	11.500787
16.329858	937.431585	11.505792
16.246413	947.180414	11.510797
16.975377	936.235336	11.515802
17.171146	942.788283	11.520807
17.264429	930.176290	11.525811
17.042178	913.476860	11.530816
16.796747	920.364784	11.535821
17.173658	912.287827	11.540826
17.096586	912.860354	11.545831
16.472225	905.030075	11.550835
17.111798	906.500114	11.555840
16.804764	904.526169	11.560845
17.209128	906.434822	11.565850
17.318470	912.582184	11.570855
17.502711	905.526284	11.575859
17.422937	915.158017	11.580864
17.397981	910.614543	11.585869
17.577080	902.059143	11.590874
17.521527	918.243645	11.595879
17.424006	907.989762	11.600883
17.557597	902.066354	11.605888
17.425365	889.940292	11.610893
17.471911	888.873611	11.615898
17.433884	891.319557	11.620903
17.748264	900.295154	11.625907
17.927173	896.833036	11.630912
17.407844	895.655748	11.635917
17.531458	888.828932	11.640922
17.251297	904.286148	11.645927
17.529006	897.058306	11.650931
17.859182	905.650675	11.655936
17.730909	913.796262	11.660941
17.541824	909.477901	11.665946
17.611412	924.598857	11.670951
17.496545	923.808137	11.675955
17.484949	925.293116	11.680960
17.301270	937.133453	11.685965
18.020204	938.666466	11.690970
18.131767	945.936480	11.695975
17.765935	942.378279	11.700979
18.098689	944.982501	11.705984
17.997102	945.214629	11.710989
18.143804	942.493413	11.715994
18.457087	964.827847	11.720999
18.211293	958.166180	11.726003
18.501547	967.176347	11.731008
18.852573	961.960895	11.736013
18.879115	958.524493	11.741018
18.538716	946.865919	11.746023
18.545747	941.272878	11.751027
18.764460	953.753572	11.756032
18.484973	961.297877	11.761037
18.754045	950.981111	11.766042
18.887619	966.551003	11.771047
18.755661	962.498357	11.776051
19.177894	963.290012	11.781056
19.142883	969.335832	11.786061
19.380928	962.298706	11.791066
18.966459	959.222917	11.796071
18.816962	953.870656	11.801075
19.275334	960.939109	11.806080
19.105535	966.004227	11.811085
19.665558	958.904793	11.816090
19.456598	959.227172	11.821095
19.152249	946.929656	11.826099
19.033589	944.033677	11.831104
19.106327	958.548208	11.836109
19.271890	966.499759	11.841114
19.355699	960.714732	11.846119
19.627232	962.210380	11.851123
19.511985	963.753792	11.856128
19.462018	963.945490	11.861133
19.375162	963.162597	11.866138
19.417366	965.951244	11.871143
19.572110	970.270721	11.876147
19.607525	963.321232	11.881152
19.464144	973.692589	11.886157
19.773246	985.544787	11.891162
19.987220	992.393055	11.896167
20.260121	1001.589769	11.901171
20.213529	1001.151680	11.906176
20.316254	987.853155	11.911181
20.083386	966.248924	11.916186
20.029918	967.259904	11.921191
20.140815	963.364960	11.926195
20.291966	965.760719	11.931200
20.245202	981.122731	11.936205
20.525719	984.386835	11.941210
20.258122	982.560854	11.946215
20.620166	982.284018	11.951219
20.369729	966.633044	11.956224
20.526081	973.323815	11.961229
20.444114	979.387557	11.966234
20.431016	988.915142	11.971239
20.559672	986.948195	11.976243
20.795035	987.182551	11.981248
20.675792	990.935196	11.986253
20.882905	988.316115	11.991258
20.728235	985.032750	11.996263
20.534136	986.224948	12.001267
20.753810	991.807110	12.006272
20.374804	992.662723	12.011277
20.621888	995.321116	12.016282
20.671802	996.841344	12.021287
20.670877	992.409383	12.026291
20.660371	990.000902	12.031296
20.877086	994.940549	12.036301
20.963327	991.238904	12.041306
20.758471	997.354908	12.046311
20.679165	1005.474384	12.051315
21.434182	1010.189503	12.056320
21.446246	996.971646	12.061325
21.573103	986.998975	12.066330
21.281718	977.321047	12.071335
21.152440	980.418176	12.076339
21.344005	982.775824	12.081344
21.148208	990.702897	12.086349
21.371568	970.999248	12.091354
21.157483	960.019661	12.096359
21.102410	953.208848	12.101363
21.147649	949.958320	12.106368
21.040158	951.762899	12.111373
21.217220	949.182529	12.116378
20.962350	954.183676	12.121383
21.118319	959.852933	12.126387
21.329216	954.225328	12.131392
20.840128	959.434793	12.136397
21.226327	955.400281	12.141402
21.058948	963.523389	12.146407
21.017588	955.959043	12.151411
21.030899	941.493261	12.156416
20.811584	931.069193	12.161421
20.879493	924.708225	12.166426
20.908320	928.702704	12.171431
20.841659	922.148495	12.176435
21.300088	926.416286	12.181440
20.971913	923.622548	12.186445
21.052855	921.543396	12.191450
20.618090	925.984067	12.196455
20.837757	921.485094	12.201459
20.913035	919.977304	12.206464
20.680714	923.654190	12.211469
21.200006	924.611964	12.216474
20.866456	930.923295	12.221479
21.050957	930.206772	12.226483
21.118715	921.831108	12.231488
20.895269	924.074772	12.236493
21.358718	931.469182	12.241498
20.955893	923.399200	12.246503
21.049962	932.026934	12.251507
21.145592	928.998690	12.256512
20.972677	937.019313	12.261517
21.229859	933.189690	12.266522
20.732702	930.600185	12.271527
21.075349	939.690169	12.276531
21.316416	934.005293	12.281536
20.795697	939.082412	12.286541
21.180738	934.238504	12.291546
21.145503	937.098449	12.296551
21.028845	931.487935	12.301555
21.038780	913.004364	12.306560
20.645322	910.125901	12.311565
20.881810	915.543312	12.316570
21.128631	930.455862	12.321575
20.696795	926.773981	12.326579
20.869737	923.386301	12.331584
20.716248	937.536577	12.336589
21.089767	936.053045	12.341594
20.786761	942.862825	12.346599
20.976815	927.805045	12.351603
21.090393	930.101847	12.356608
20.727694	934.444112	12.361613
20.923279	941.603008	12.366618
21.077741	935.458115	12.371623
20.908177	928.149447	12.376627
21.007908	921.149871	12.381632
20.495344	927.328474	12.386637
20.767234	933.572316	12.391642
21.062230	934.443416	12.396647
21.013934	941.713206	12.401651
21.021409	939.453623	12.406656
20.888138	948.600342	12.411661
21.151120	942.229999	12.416666
20.830350	932.702794	12.421671
20.776781	932.103273	12.426675
20.809754	931.419046	12.431680
21.188892	942.886970	12.436685
21.148175	921.694326	12.441690
20.855092	921.158371	12.446695
20.600812	916.456452	12.451699
21.018726	920.273691	12.456704
20.736528	937.367068	12.461709
20.775281	935.773171	12.466714
20.774115	948.528007	12.471719
20.688577	948.309754	12.476723
21.120428	951.035144	12.481728
21.421606	946.705345	12.486733
21.362978	941.436981	12.491738
20.979982	926.869820	12.496743
21.273427	919.518086	12.501747
21.537676	914.593448	12.506752
21.175307	916.190673	12.511757
20.981953	914.971308	12.516762
21.095197	915.851860	12.521767
21.011993	914.819660	12.526771
21.107249	919.886291	12.531776
20.802355	924.430615	12.536781
20.892949	915.736435	12.541786
20.710166	917.882733	12.546791
20.631309	914.910066	12.551795
20.713647	918.404713	12.556800
20.852398	919.244575	12.561805
20.956591	919.901680	12.566810
21.049911	922.296295	12.571815
20.894840	918.979460	12.576819
21.129596	919.011421	12.581824
20.934721	932.590504	12.586829
21.118041	926.615534	12.591834
20.728428	925.279425	12.596839
20.799962	927.682512	12.601843
20.945297	917.746191	12.606848
20.971317	920.867997	12.611853
21.023606	919.589542	12.616858
20.827070	925.755012	12.621863
20.955739	922.007031	12.626867
21.081124	922.593398	12.631872
21.355397	932.115886	12.636877
21.316079	924.021473	12.641882
20.603014	907.515543	12.646887
20.468670	906.274614	12.651891
20.951235	910.975627	12.656896
20.815025	930.504341	12.661901
20.988586	927.461156	12.666906
21.105595	922.316631	12.671911
20.875451	928.941809	12.676915
20.924799	929.716475	12.681920
21.043442	929.305320	12.686925
20.988093	922.112861	12.691930
20.749907	921.058287	12.696935
20.762246	922.001139	12.701939
21.058981	923.920749	12.706944
20.864435	926.750770	12.711949
21.028566	933.829793	12.716954
20.749087	932.866377	12.721959
20.996748	930.806007	12.726963
21.159202	932.897456	12.731968
20.875605	925.517552	12.736973
20.863485	911.936809	12.741978
20.532811	915.493585	12.746983
20.620148	928.073363	12.751987
21.206862	932.763631	12.756992
21.068178	935.055922	12.761997
21.119164	937.354772	12.767002
21.024720	931.085189	12.772007
20.471269	916.234241	12.777011
20.834233	924.014557	12.782016
20.936815	932.558728	12.787021
21.029405	927.890095	12.792026
20.936828	931.607760	12.797031
20.887125	933.321113	12.802035
20.999677	934.449283	12.807040
20.637938	934.291412	12.812045
21.062810	942.465726	12.817050
21.090167	938.435508	12.822055
21.098857	932.412715	12.827059
21.125395	910.720663	12.832064
20.513106	917.095175	12.837069
20.679067	922.523102	12.842074
20.949172	928.267120	12.847079
21.042516	938.794049	12.852083
20.957244	940.254161	12.857088
20.897315	943.045316	12.862093
20.838995	935.547045	12.867098
20.948002	945.089588	12.872103
20.955034	940.938118	12.877107
21.118567	941.714523	12.882112
20.694236	937.394646	12.887117
20.789634	929.590946	12.892122
21.174091	937.647056	12.897127
20.798622	935.705761	12.902131
20.997887	932.163567	12.907136
20.798614	938.631088	12.912141
21.019634	936.566601	12.917146
21.198882	933.398099	12.922151
20.916203	922.703850	12.927155
20.650986	915.829611	12.932160
20.956761	925.999190	12.937165
20.941198	922.121597	12.942170
20.731327	915.491289	12.947175
20.624949	932.590830	12.952179
21.242291	946.622372	12.957184
20.964195	944.042674	12.962189
20.866792	927.039192	12.967194
20.933182	927.464360	12.972199
21.020526	934.106946	12.977203
21.116460	916.201123	12.982208
20.661036	923.749918	12.987213
20.983304	924.147003	12.992218
21.287843	919.530058	12.997223
20.990662	922.479518	13.002227
20.815359	916.497356	13.007232
20.449382	919.559268	13.012237
20.836049	919.779128	13.017242
20.697530	929.509363	13.022247
20.812524	945.359523	13.027251
21.264860	940.918152	13.032256
21.177431	945.325722	13.037261
20.993184	929.827646	13.042266
20.807714	926.274050	13.047271
20.871566	918.529842	13.052275
21.103839	923.285615	13.057280
21.025941	927.990755	13.062285
21.264045	920.548247	13.067290
21.175210	925.803942	13.072295
20.802788	929.178800	13.077299
21.039936	922.542107	13.082304
20.702465	929.668842	13.087309
21.046324	923.785557	13.092314
20.651408	921.675100	13.097319
20.758469	928.399566	13.102323
20.715814	927.121994	13.107328
20.750603	928.491258	13.112333
20.736644	917.857911	13.117338
20.815141	925.409109	13.122343
20.690435	930.550957	13.127347
21.500582	939.841441	13.132352
21.150709	941.408895	13.137357
21.506742	933.742082	13.142362
21.239616	927.995921	13.147367
21.574859	924.436335	13.152371
21.499874	930.494915	13.157376
21.261393	919.634407	13.162381
20.696323	897.876835	13.167386
20.586762	900.256495	13.172391
20.569069	907.935098	13.177395
20.754188	911.727512	13.182400
20.554945	926.801012	13.187405
21.048859	926.321962	13.192410
20.704432	927.807955	13.197415
20.825298	929.955086	13.202419
20.860527	927.293644	13.207424
20.807687	928.794378	13.212429
21.111584	929.633557	13.217434
21.252825	928.783926	13.222439
21.371704	936.025839	13.227443
21.306347	919.164897	13.232448
20.739109	909.503518	13.237453
20.769148	898.526328	13.242458
21.074613	914.612219	13.247463
20.824228	914.259600	13.252467
20.740409	913.679082	13.257472
20.732561	930.629886	13.262477
20.662394	925.864028	13.267482
20.683541	922.753820	13.272487
20.945777	937.537418	13.277491
21.007294	924.040355	13.282496
20.389118	933.728097	13.287501
20.373643	932.600996	13.292506
20.210786	935.954924	13.297511
20.409993	937.464944	13.302515
20.920516	944.019189	13.307520
20.868198	963.150667	13.312525
20.953585	960.423777	13.317530
21.134890	961.025426	13.322535
21.091777	967.651316	13.327539
20.765352	952.755091	13.332544
20.695819	947.829645	13.337549
21.094818	959.002862	13.342554
20.971844	960.879175	13.347559
20.750487	958.675798	13.352563
21.001155	957.186090	13.357568
20.853800	972.775734	13.362573
20.950297	966.350638	13.367578
21.152731	957.045551	13.372583
20.958035	950.490389	13.377587
21.137659	942.105007	13.382592
20.797704	951.392954	13.387597
20.835985	939.782352	13.392602
20.897103	942.748540	13.397607
20.847542	933.032730	13.402611
20.919625	936.206246	13.407616
20.530115	941.283763	13.412621
21.113831	941.064446	13.417626
21.284166	948.355964	13.422631
21.018493	942.812442	13.427635
21.015860	936.484090	13.432640
20.872729	936.542947	13.437645
21.107214	941.952027	13.442650
21.657474	944.529219	13.447655
21.131256	939.995102	13.452659
21.430374	942.950878	13.457664
21.330958	943.254081	13.462669
21.325639	930.102023	13.467674
21.163337	915.953741	13.472679
20.978304	906.291569	13.477683
21.067579	905.683347	13.482688
21.123063	907.094060	13.487693
21.052227	904.463043	13.492698
20.924841	904.054599	13.497703
20.970071	907.384686	13.502707
21.378725	900.564650	13.507712
21.148677	907.044541	13.512717
21.055090	908.447260	13.517722
21.112016	905.591840	13.522727
20.744175	906.349614	13.527731
21.366064	900.517352	13.532736
20.747146	904.120388	13.537741
20.805994	899.472153	13.542746
20.626041	901.497175	13.547751
20.565657	908.821522	13.552755
20.633026	906.320755	13.557760
20.815974	913.564304	13.562765
20.788474	910.951514	13.567770
20.925793	904.510365	13.572775
20.596724	904.352814	13.577779
20.605187	905.723037	13.582784
20.926111	911.521098	13.587789
20.711394	906.145693	13.592794
20.756457	913.413278	13.597799
20.486698	908.136126	13.602803
21.059696	928.481126	13.607808
21.073117	932.109170	13.612813
20.528884	917.069141	13.617818
20.676187	920.489492	13.622823
21.313970	933.506210	13.627827
21.406603	927.169817	13.632832
21.061309	933.813951	13.637837
20.521768	914.385649	13.642842
20.383729	918.424129	13.647847
20.798742	936.890058	13.652851
21.014728	949.021482	13.657856
20.953620	946.229318	13.662861
20.857851	948.055966	13.667866
20.927655	943.307946	13.672871
20.953090	945.233811	13.677875
21.310177	940.613377	13.682880
20.909214	935.648445	13.687885
20.803764	920.264762	13.692890
20.957808	925.967495	13.697895
20.631442	931.807862	13.702899
21.035801	938.702409	13.707904
20.971513	945.374157	13.712909
20.954188	936.636891	13.717914
21.033397	929.973590	13.722919
20.808937	923.021703	13.727923
20.856057	928.934610	13.732928
20.521175	943.512306	13.737933
20.408725	945.623259	13.742938
20.610252	949.065504	13.747943
20.667423	953.205917	13.752947
20.871875	942.926288	13.757952
20.837055	956.851763	13.762957
20.582996	952.935712	13.767962
20.806099	953.963613	13.772967
20.831628	952.701980	13.777971
21.084300	953.623364	13.782976
20.764718	959.755866	13.787981
20.748568	952.281541	13.792986
20.822173	947.702210	13.797991
20.790073	963.914712	13.802995
20.944641	953.604550	13.808000
21.145977	954.773946	13.813005
20.997077	958.766930	13.818010
20.923922	951.639089	13.823015
21.070810	952.646110	13.828019
21.015358	941.923941	13.833024
20.746338	958.433636	13.838029
20.744785	952.550749	13.843034
20.917054	959.475626	13.848039
20.877256	952.908904	13.853043
21.022322	949.787311	13.858048
21.002883	954.504542	13.863053
20.802572	954.695965	13.868058
20.891609	945.956641	13.873063
20.863563	952.823098	13.878067
21.199053	951.451084	13.883072
20.725270	963.266576	13.888077
20.853633	961.103104	13.893082
20.796528	958.652881	13.898087
20.875843	966.567510	13.903091
21.127502	954.285183	13.908096
21.013774	962.177645	13.913101
20.940653	960.445428	13.918106
21.031896	959.898444	13.923111
20.939729	961.873291	13.928115
21.189738	953.213337	13.933120
20.799560	963.627002	13.938125
21.114753	966.094897	13.943130
21.125389	964.810948	13.948135
20.947917	969.483832	13.953139
21.041248	959.847320	13.958144
21.194755	961.237679	13.963149
20.964289	956.494954	13.968154
21.133257	958.488974	13.973159
21.051094	959.083691	13.978163
21.190388	957.178871	13.983168
21.103185	957.560506	13.988173
20.789204	938.226131	13.993178
20.916104	930.911631	13.998183
20.664845	937.971088	14.003187
21.215198	955.943706	14.008192
20.777980	950.166003	14.013210
20.322705	940.854420	14.018227
20.547332	956.283080	14.023245
20.496569	962.824493	14.028263
20.895320	960.817382	14.033280
20.995569	966.724989	14.038298
21.023878	966.108650	14.043315
20.925189	962.336699	14.048333
20.794419	971.382557	14.053351
21.011208	970.086219	14.058368
20.980559	967.723567	14.063386
21.196301	971.048596	14.068403
21.168008	967.992184	14.073421
20.909370	971.524936	14.078439
20.945682	969.009848	14.083456
21.055460	972.464077	14.088474
21.207329	987.562306	14.093491
21.464549	987.802057	14.098509
21.066982	985.963368	14.103527
21.193999	986.626259	14.108544
21.360716	997.922864	14.113562
21.339049	1006.078714	14.118579
21.298871	982.681546	14.123597
21.125482	991.266973	14.128615
21.611204	994.742188	14.133632
21.422023	1011.117899	14.138650
21.358252	1002.375814	14.143667
21.516839	993.075100	14.148685
21.127877	1003.602749	14.153703
21.317009	1011.615758	14.158720
21.315981	1011.828523	14.163738
21.296639	1017.899971	14.168755
21.385426	1010.814917	14.173773
21.567624	1008.083458	14.178791
21.654010	998.565575	14.183808
21.482599	1008.787798	14.188826
21.515246	1011.027219	14.193843
21.537349	1007.829078	14.198861
21.235822	1012.909855	14.203879
21.209418	1009.069197	14.208896
21.485607	1011.567277	14.213914
21.319915	1011.366115	14.218931
21.763151	1011.147565	14.223949
21.483184	1015.677756	14.228967
21.662240	1002.526397	14.233984
21.569837	1015.435272	14.239002
21.534945	1025.412035	14.244019
21.835038	1031.959467	14.249037
21.786856	1038.105951	14.254055
22.308612	1034.124053	14.259072
22.212214	1020.968722	14.264090
21.939442	1020.508342	14.269107
21.918174	1011.920787	14.274125
21.693020	1011.694779	14.279143
21.823587	1005.540822	14.284160
21.872598	1017.658861	14.289178
21.638676	1015.539337	14.294195
21.975247	1004.525694	14.299213
21.711549	1007.734889	14.304231
22.095178	1010.107059	14.309248
21.833171	1022.417021	14.314266
22.023446	1036.369652	14.319283
22.101779	1037.136569	14.324301
22.056191	1048.299520	14.329319
22.155924	1037.094948	14.334336
21.925660	1038.539231	14.339354
21.958007	1044.269125	14.344371
22.464401	1037.357752	14.349389
22.243571	1049.594135	14.354407
22.395520	1032.456156	14.359424
22.116631	1023.047741	14.364442
22.041516	1020.147783	14.369459
22.135371	1025.358819	14.374477
22.047634	1042.064045	14.379495
22.294357	1036.958744	14.384512
22.193726	1042.680726	14.389530
22.107320	1046.502885	14.394547
22.611958	1037.779474	14.399565
22.548961	1044.961649	14.404583
22.595872	1041.247399	14.409600
22.615811	1028.385917	14.414618
22.223853	1019.163045	14.419635
22.506113	1006.074703	14.424653
22.320087	1015.910432	14.429671
22.107187	1015.811466	14.434688
22.282531	1033.372429	14.439706
22.332806	1039.261858	14.444723
22.620058	1026.279344	14.449741
22.473864	1032.486334	14.454759
22.602122	1036.064190	14.459776
22.948621	1036.375649	14.464794
22.878576	1035.541901	14.469811
22.836917	1030.365959	14.474829
22.521013	1022.872299	14.479847
22.688497	1025.179161	14.484864
22.417079	1029.856327	14.489882
22.431246	1035.966528	14.494899
22.369417	1031.631506	14.499917
22.658996	1043.725250	14.504935
22.825978	1043.117418	14.509952
22.850091	1040.550862	14.514970
22.900592	1041.943070	14.519987
22.667036	1040.065230	14.525005
22.366017	1045.172703	14.530023
22.644730	1044.648084	14.535040
22.467429	1041.422703	14.540058
22.433991	1044.244368	14.545075
23.022163	1039.660880	14.550093
22.792928	1053.446854	14.555111
23.074444	1060.180961	14.560128
23.301521	1044.259314	14.565146
23.147176	1041.884786	14.570163
23.254955	1034.149174	14.575181
22.881124	1048.750545	14.580199
23.127657	1037.862954	14.585216
23.147748	1030.524690	14.590234
22.598252	1036.772876	14.595251
22.894287	1031.894571	14.600269
22.933026	1038.006860	14.605287
23.175100	1042.184540	14.610304
23.174378	1054.397756	14.615322
23.233759	1052.082258	14.620339
23.089343	1043.930792	14.625357
23.096651	1050.846959	14.630375
23.283699	1066.335719	14.635392
23.448464	1062.377618	14.640410
22.943554	1063.065782	14.645427
23.324207	1062.282327	14.650445
23.038760	1066.962696	14.655463
23.572381	1071.854629	14.660480
23.828201	1064.794066	14.665498
23.267756	1062.542316	14.670515
23.619003	1046.074535	14.675533
23.290948	1045.803566	14.680551
23.367324	1049.216686	14.685568
23.529365	1055.618494	14.690586
23.110827	1070.046827	14.695603
23.350985	1065.624190	14.700621
23.286805	1069.165358	14.705639
23.149233	1069.338537	14.710656
23.540275	1064.640011	14.715674
23.091478	1065.795363	14.720691
23.376577	1066.142154	14.725709
23.265288	1070.914721	14.730727
23.382522	1080.969776	14.735744
23.512670	1077.850347	14.740762
23.312952	1095.806027	14.745779
23.933993	1100.068759	14.750797
23.981862	1100.016428	14.755815
23.868982	1095.054659	14.760832
23.808002	1090.710027	14.765850
23.955044	1086.601009	14.770867
23.599050	1075.292643	14.775885
24.120051	1081.891597	14.780903
23.621257	1074.429270	14.785920
23.737858	1083.207565	14.790938
23.621309	1086.520296	14.795955
23.828083	1097.687655	14.800973
23.864542	1094.950064	14.805991
23.952807	1091.695677	14.811008
24.135860	1095.342110	14.816026
23.956946	1103.185968	14.821043
24.316229	1097.874719	14.826061
24.166723	1099.670544	14.831079
24.043728	1097.571756	14.836096
24.384685	1096.058040	14.841114
24.007591	1094.028412	14.846131
24.008903	1087.658770	14.851149
23.842088	1088.677974	14.856167
24.065772	1088.605342	14.861184
24.261982	1097.563318	14.866202
24.106305	1105.993397	14.871219
24.412641	1094.619885	14.876237
24.207365	1089.356613	14.881255
24.092121	1103.156553	14.886272
24.237612	1100.918417	14.891290
24.486606	1104.042877	14.896307
24.015019	1101.854632	14.901325
24.113675	1094.519404	14.906343
24.107030	1099.567368	14.911360
24.540818	1093.061758	14.916378
24.590097	1096.466934	14.921395
24.520612	1097.817509	14.926413
24.463683	1102.516193	14.931431
24.411559	1108.561405	14.936448
24.490408	1093.528576	14.941466
24.361984	1100.132972	14.946483
24.260694	1102.536720	14.951501
24.251836	1092.083068	14.956519
24.572871	1089.756169	14.961536
24.689844	1089.981776	14.966554
24.099380	1099.013604	14.971571
24.353806	1098.541576	14.976589
24.594017	1103.629112	14.981607
24.375371	1107.758234	14.986624
24.735145	1104.580925	14.991642
24.804460	1113.419711	14.996659
24.722156	1109.107471	15.001677
24.812494	1115.335756	15.006695
24.832017	1116.687609	15.011712
24.760861	1113.060913	15.016730
25.167269	1115.604405	15.021747
25.081171	1108.571735	15.026765
24.934314	1098.363804	15.031783
24.735364	1098.535696	15.036800
24.721239	1092.865997	15.041818
24.890779	1107.560494	15.046835
24.938051	1109.052875	15.051853
24.969579	1112.508740	15.056871
25.076326	1110.332368	15.061888
25.365243	1109.694570	15.066906
25.074142	1107.756110	15.071923
24.854043	1102.740670	15.076941
25.106495	1098.070227	15.081959
24.858845	1117.063363	15.086976
24.973813	1108.183084	15.091994
25.216892	1110.844744	15.097011
25.060183	1115.243979	15.102029
25.340522	1105.871138	15.107047
25.250275	1113.912414	15.112064
25.551261	1108.410353	15.117082
25.491901	1117.750376	15.122099
25.005605	1111.158397	15.127117
24.922864	1108.626295	15.132135
25.010371	1117.226906	15.137152
25.307313	1112.259438	15.142170
25.289068	1124.815898	15.147187
25.248173	1120.559159	15.152205
25.328391	1120.069357	15.157223
25.114114	1124.129619	15.162240
25.246798	1113.015020	15.167258
25.258276	1118.887113	15.172275
24.923563	1117.354586	15.177293
25.382119	1128.770554	15.182311
25.554450	1147.226721	15.187328
25.689811	1140.846280	15.192346
25.804226	1152.778394	15.197363
25.799488	1141.514094	15.202381
25.769362	1140.435681	15.207399
25.503540	1131.831718	15.212416
25.715934	1134.806935	15.217434
25.603942	1150.389180	15.222451
25.857674	1147.615508	15.227469
25.946240	1135.437504	15.232487
25.670772	1130.264211	15.237504
25.792234	1117.937656	15.242522
25.708876	1128.323220	15.247539
25.706194	1137.273585	15.252557
26.074271	1141.174156	15.257575
25.588133	1141.372451	15.262592
25.892873	1133.858158	15.267610
26.010151	1144.968449	15.272627
25.653650	1152.477790	15.277645
26.172985	1141.476026	15.282663
25.565204	1143.662659	15.287680
25.742866	1143.974326	15.292698
25.774012	1141.138023	15.297715
25.733706	1145.097196	15.302733
25.852781	1143.417959	15.307751
25.679642	1148.581893	15.312768
26.178234	1156.705711	15.317786
26.204674	1167.232331	15.322803
25.931039	1176.058688	15.327821
26.368527	1169.706362	15.332839
26.464280	1183.230806	15.337856
26.573375	1168.389980	15.342874
26.427301	1153.159418	15.347891
25.728006	1144.757338	15.352909
26.282481	1150.501302	15.357927
26.401129	1170.242395	15.362944
26.829605	1170.355535	15.367962
26.592448	1162.581354	15.372979
26.507911	1155.258608	15.377997
26.304009	1139.282008	15.383015
26.227071	1143.775456	15.388032
26.027451	1148.476570	15.393050
26.254667	1165.905944	15.398067
26.264150	1172.563504	15.403085
26.628237	1166.211952	15.408103
26.702635	1179.334903	15.413120
26.918279	1167.641033	15.418138
26.970098	1178.864155	15.423155
26.907366	1173.176775	15.428173
27.232020	1144.123043	15.433191
26.932939	1142.286349	15.438208
26.757757	1139.998849	15.443226
27.117622	1146.277793	15.448243
26.949014	1150.167619	15.453261
26.981893	1140.551729	15.458279
26.357018	1147.700750	15.463296
26.409726	1137.441252	15.468314
26.536696	1141.858004	15.473331
26.398373	1146.680508	15.478349
26.588762	1153.917328	15.483367
26.669383	1169.595318	15.488384
26.987602	1171.223154	15.493402
26.996424	1172.330369	15.498419
26.855720	1177.725386	15.503437
26.998558	1178.552122	15.508455
26.909849	1171.637597	15.513472
27.080631	1169.434095	15.518490
27.193806	1162.473936	15.523507
26.795780	1172.815048	15.528525
26.866390	1165.951563	15.533543
27.196524	1172.696283	15.538560
27.091592	1166.874790	15.543578
27.141307	1164.347136	15.548595
26.969405	1172.268573	15.553613
27.171334	1163.139475	15.558631
26.950026	1174.493288	15.563648
27.088294	1174.733357	15.568666
27.206282	1187.806318	15.573683
27.078660	1201.981334	15.578701
27.535423	1191.834822	15.583719
27.521578	1195.648121	15.588736
27.809483	1203.101728	15.593754
27.763098	1186.548026	15.598771
27.696073	1177.778839	15.603789
27.709428	1167.544968	15.608807
27.355055	1164.952727	15.613824
27.229030	1161.687425	15.618842
27.408016	1165.590105	15.623859
27.280991	1187.968045	15.628877
27.321414	1194.885292	15.633895
27.415095	1195.889763	15.638912
27.588915	1202.825090	15.643930
27.654018	1199.353767	15.648947
27.708291	1201.904495	15.653965
27.731996	1198.677298	15.658983
27.497555	1203.404085	15.664000
28.026270	1193.858280	15.669018
28.420022	1187.626841	15.674035
27.872546	1199.576797	15.679053
28.159740	1195.644133	15.684071
28.212510	1201.590680	15.689088
28.004106	1187.159421	15.694106
27.836180	1177.070415	15.699123
28.370197	1190.812268	15.704141
27.905868	1169.781829	15.709159
27.748550	1178.935123	15.714176
28.131061	1170.239665	15.719194
27.895280	1176.036447	15.724211
27.998988	1196.683754	15.729229
27.916084	1197.752756	15.734247
28.058233	1195.309650	15.739264
27.934070	1201.047143	15.744282
28.223776	1195.545411	15.749299
27.898855	1201.379535	15.754317
28.218644	1200.630921	15.759335
28.700614	1195.441530	15.764352
28.401411	1196.342481	15.769370
28.673692	1197.749044	15.774387
28.193942	1202.318267	15.779405
28.322569	1192.401653	15.784423
28.273063	1203.586255	15.789440
28.142518	1199.819315	15.794458
28.736605	1192.695185	15.799475
28.269645	1192.266518	15.804493
28.539826	1183.752924	15.809511
28.632122	1192.449614	15.814528
28.560398	1191.119254	15.819546
28.630140	1181.097772	15.824563
28.506821	1186.674472	15.829581
29.184735	1176.541239	15.834599
28.904735	1190.530147	15.839616
28.788680	1182.224521	15.844634
28.553207	1168.696813	15.849651
28.770519	1183.241841	15.854669
28.946508	1170.435384	15.859687
28.695511	1165.727213	15.864704
28.364382	1164.987439	15.869722
28.860169	1173.697229	15.874739
28.381015	1181.038227	15.879757
28.766699	1184.794834	15.884775
29.022488	1189.139902	15.889792
28.914949	1201.965298	15.894810
28.705880	1187.421545	15.899827
28.524088	1193.068908	15.904845
28.850521	1190.725320	15.909863
28.451770	1192.570976	15.914880
28.513613	1191.482698	15.919898
28.446460	1198.725897	15.924915
28.781323	1208.217692	15.929933
29.031538	1216.213247	15.934951
29.121263	1221.295912	15.939968
29.019120	1213.483989	15.944986
29.147795	1218.993083	15.950003
29.031273	1225.775822	15.955021
29.148082	1212.992076	15.960039
28.992650	1214.653091	15.965056
28.694980	1222.339402	15.970074
29.314939	1226.512978	15.975091
29.145006	1242.634034	15.980109
29.238699	1248.255839	15.985127
29.391206	1251.054716	15.990144
29.394860	1244.971642	15.995162
29.349124	1240.857445	16.000179
29.120409	1254.002505	16.005197
29.596236	1251.732909	16.010215
29.547162	1248.520542	16.015232
29.222454	1251.949713	16.020250
29.707585	1243.573264	16.025267
29.804655	1252.068758	16.030285
29.990852	1254.796106	16.035303
29.736087	1240.456612	16.040320
29.846322	1244.504970	16.045338
29.466158	1248.066888	16.050355
29.739066	1258.433191	16.055373
29.814609	1250.648663	16.060391
29.838278	1245.241350	16.065408
29.593736	1256.798042	16.070426
29.671401	1254.907370	16.075443
29.717336	1256.189346	16.080461
29.780401	1257.085281	16.085479
29.874736	1246.553984	16.090496
29.834938	1253.098363	16.095514
29.725427	1243.184748	16.100531
29.813835	1253.299585	16.105549
30.124068	1260.164695	16.110567
29.961659	1250.024691	16.115584
29.761597	1269.129942	16.120602
29.976901	1279.209653	16.125619
29.885410	1277.946459	16.130637
30.005227	1280.739528	16.135655
30.149263	1277.040069	16.140672
30.118818	1275.803026	16.145690
30.679971	1271.611147	16.150707
30.707170	1290.894802	16.155725
30.666274	1272.735198	16.160743
31.166378	1270.121250	16.165760
30.792506	1264.146207	16.170778
30.558880	1247.337116	16.175795
30.180154	1242.485847	16.180813
30.327143	1242.779545	16.185831
30.278002	1246.060671	16.190848
30.214374	1250.839295	16.195866
30.431733	1236.392477	16.200883
30.018300	1256.004809	16.205901
30.542190	1270.400495	16.210919
30.536386	1270.339648	16.215936
30.232663	1279.361395	16.220954
30.400724	1273.456045	16.225971
30.342102	1273.204630	16.230989
30.270312	1270.695429	16.236007
30.919180	1281.092571	16.241024
30.431334	1278.263723	16.246042
30.744458	1274.199416	16.251059
30.611605	1286.548471	16.256077
31.148939	1292.241878	16.261095
31.056314	1274.480152	16.266112
31.017481	1280.679465	16.271130
30.898062	1271.395146	16.276147
30.647734	1275.098209	16.281165
30.846119	1273.103758	16.286183
31.009630	1285.596898	16.291200
31.109634	1303.551432	16.296218
31.399828	1302.751584	16.301235
31.187321	1292.772123	16.306253
30.866628	1282.602932	16.311271
31.314134	1276.590609	16.316288
30.821247	1285.074269	16.321306
31.009932	1295.538903	16.326323
31.025150	1303.574400	16.331341
31.332198	1302.326346	16.336359
30.964835	1304.863153	16.341376
30.986309	1315.245042	16.346394
31.231852	1305.716222	16.351411
31.482339	1309.151126	16.356429
31.583331	1311.387141	16.361447
31.663533	1301.658304	16.366464
31.462815	1310.569487	16.371482
31.560796	1308.898574	16.376499
31.419341	1308.712545	16.381517
31.197309	1310.928346	16.386535
31.292027	1309.407219	16.391552
31.157968	1309.999915	16.396570
31.237373	1301.319737	16.401587
31.511211	1315.553987	16.406605
31.352659	1336.800039	16.411623
31.561336	1326.402643	16.416640
31.775157	1337.294137	16.421658
31.632385	1332.552005	16.426675
31.844086	1337.388971	16.431693
31.312434	1334.613690	16.436711
31.846637	1334.508293	16.441728
31.727501	1338.378659	16.446746
31.626279	1336.038288	16.451763
31.944430	1336.664486	16.456781
31.902402	1339.075434	16.461799
32.063244	1330.367102	16.466816
31.711657	1341.437044	16.471834
31.934989	1358.691693	16.476851
32.337987	1367.708080	16.481869
32.387900	1363.284904	16.486887
32.622058	1351.513307	16.491904
32.402940	1340.204116	16.496922
32.435762	1333.232459	16.501939
32.415363	1331.315280	16.506957
32.374310	1338.159937	16.511975
32.351359	1326.367868	16.516992
32.035695	1326.472363	16.522010
32.096080	1325.198481	16.527027
32.406478	1323.031262	16.532045
32.164315	1329.060712	16.537063
32.158102	1323.226566	16.542080
32.456341	1329.415747	16.547098
32.178412	1326.676895	16.552115
32.341148	1340.506556	16.557133
32.167338	1354.986901	16.562151
32.650392	1351.527751	16.567168
32.874292	1355.938970	16.572186
32.789797	1357.817387	16.577203
33.176685	1355.131095	16.582221
32.998854	1343.743950	16.587239
32.931038	1328.978584	16.592256
32.600809	1335.010929	16.597274
32.991781	1316.867787	16.602291
32.966174	1326.836064	16.607309
32.709248	1326.788742	16.612327
33.017264	1319.125754	16.617344
32.868502	1329.849862	16.622362
32.726075	1316.274968	16.627379
32.887350	1317.777747	16.632397
32.557816	1331.386655	16.637415
32.850450	1340.955463	16.642432
32.980407	1358.749793	16.647450
33.200852	1353.376034	16.652467
33.370101	1356.859527	16.657485
32.874784	1353.036182	16.662503
33.449489	1357.887301	16.667520
33.273798	1365.947294	16.672538
33.039649	1366.543766	16.677555
33.252661	1353.896575	16.682573
33.008432	1358.419949	16.687591
33.526308	1351.260386	16.692608
33.917528	1356.875316	16.697626
33.640855	1357.182200	16.702643
33.826614	1343.003325	16.707661
33.551288	1335.517912	16.712679
33.576557	1328.644411	16.717696
33.095502	1325.741942	16.722714
33.132607	1333.054738	16.727731
33.493171	1341.810644	16.732749
33.141861	1352.297027	16.737767
33.592931	1348.404738	16.742784
33.306771	1360.691545	16.747802
33.352656	1356.138734	16.752819
33.579698	1350.837868	16.757837
32.958654	1357.896947	16.762855
33.246468	1369.337642	16.767872
33.482655	1380.382040	16.772890
33.581473	1380.000076	16.777907
33.874025	1377.712275	16.782925
33.624506	1384.975803	16.787943
34.127370	1377.395139	16.792960
34.083197	1388.167502	16.797978
33.834109	1375.762530	16.802995
34.185192	1373.639514	16.808013
33.881849	1380.638620	16.813031
33.943623	1371.347981	16.818048
34.456836	1380.206489	16.823066
34.483849	1382.036654	16.828083
34.301986	1381.070863	16.833101
34.033530	1376.597928	16.838119
34.156530	1369.779707	16.843136
33.817197	1379.694709	16.848154
34.243314	1375.740150	16.853171
34.499216	1372.256551	16.858189
34.604869	1382.612239	16.863207
34.110980	1377.259756	16.868224
34.467338	1374.654688	16.873242
34.141161	1376.938752	16.878259
34.388692	1377.508156	16.883277
34.463067	1375.491643	16.888295
34.337085	1373.112988	16.893312
34.216169	1386.547187	16.898330
34.504692	1396.437237	16.903347
34.901629	1399.944700	16.908365
34.713240	1407.426913	16.913383
34.701339	1398.228031	16.918400
34.972949	1401.305363	16.923418
34.808020	1394.655407	16.928435
35.128682	1396.121417	16.933453
34.795116	1393.619672	16.938471
34.703148	1389.719682	16.943488
35.048344	1394.281391	16.948506
35.117018	1399.145261	16.953523
34.966984	1374.401247	16.958541
34.780614	1390.171697	16.963559
34.919283	1387.897285	16.968576
35.156294	1391.304594	16.973594
34.930409	1392.797769	16.978611
35.213972	1391.508848	16.983629
35.029432	1388.046030	16.988647
35.135930	1386.257495	16.993664
35.138163	1390.318109	16.998682
35.090658	1402.143910	17.003699
35.496541	1394.176677	17.008717
34.791067	1398.435804	17.013735
35.076273	1389.702179	17.018752
35.232687	1393.780457	17.023770
35.203984	1401.408141	17.028787
35.408024	1393.889334	17.033805
35.361627	1401.640535	17.038823
35.633244	1395.121658	17.043840
35.424492	1400.217757	17.048858
35.197755	1399.167524	17.053875
35.587521	1397.563121	17.058893
35.808050	1422.747834	17.063911
35.680204	1418.237785	17.068928
35.625996	1405.064265	17.073946
35.574426	1402.275171	17.078963
35.508518	1410.984539	17.083981
35.601076	1431.116301	17.088999
35.932079	1428.580932	17.094016
35.772881	1430.025271	17.099034
35.765898	1435.904586	17.104051
35.944030	1429.129254	17.109069
35.699417	1430.074013	17.114087
35.624289	1435.974856	17.119104
35.759985	1436.128748	17.124122
35.877592	1430.291838	17.129139
35.778426	1423.393956	17.134157
35.474397	1437.340743	17.139175
35.884426	1448.979856	17.144192
36.281952	1453.197538	17.149210
35.865846	1466.131966	17.154227
36.513165	1454.619409	17.159245
36.159539	1456.620761	17.164263
36.080207	1453.710026	17.169280
36.538338	1453.992119	17.174298
36.330912	1449.887083	17.179315
36.399082	1440.015327	17.184333
36.142711	1452.541610	17.189351
36.323962	1455.104471	17.194368
36.582285	1446.676635	17.199386
36.517425	1453.319105	17.204403
37.000648	1448.183359	17.209421
37.031766	1451.145619	17.214439
37.126745	1450.991500	17.219456
36.910271	1456.440158	17.224474
37.353281	1450.711246	17.229491
37.099863	1424.085475	17.234509
36.806230	1415.405799	17.239527
37.157101	1411.855509	17.244544
37.154761	1410.858937	17.249562
36.684752	1413.097187	17.254579
37.099852	1409.866233	17.259597
37.146753	1414.003455	17.264615
37.076708	1416.675149	17.269632
37.256678	1421.659722	17.274650
36.759590	1413.630345	17.279667
37.241408	1415.099437	17.284685
37.040889	1417.945879	17.289703
37.321647	1418.194990	17.294720
37.232470	1416.936900	17.299738
36.728910	1424.625930	17.304755
37.151523	1413.048376	17.309773
37.155730	1413.798490	17.314791
37.314644	1412.492746	17.319808
37.236328	1412.195487	17.324826
36.969582	1416.151029	17.329843
37.191019	1431.974054	17.334861
37.019060	1444.600831	17.339879
37.235938	1448.314784	17.344896
37.326879	1440.697224	17.349914
37.296408	1455.157023	17.354931
37.409316	1451.010059	17.359949
37.231188	1454.127892	17.364967
37.299420	1452.631373	17.369984
37.240667	1455.132223	17.375002
37.421326	1475.692289	17.380019
37.415545	1467.605816	17.385037
37.677544	1467.834520	17.390055
37.892602	1476.224859	17.395072
38.228976	1456.928987	17.400090
38.141799	1467.978490	17.405107
38.405873	1466.344051	17.410125
38.536407	1469.049087	17.415143
38.120704	1455.795363	17.420160
38.141477	1441.353318	17.425178
37.751456	1432.816942	17.430195
38.029451	1456.429104	17.435213
38.192698	1473.009467	17.440231
38.291778	1472.555008	17.445248
38.254745	1459.884848	17.450266
38.219839	1467.802633	17.455283
38.019629	1461.390610	17.460301
38.231308	1461.798038	17.465319
38.046307	1471.172412	17.470336
38.497401	1467.263553	17.475354
37.981253	1463.019693	17.480371
38.675825	1460.622791	17.485389
38.374499	1460.719315	17.490407
38.285884	1463.081571	17.495424
38.780247	1464.725307	17.500442
38.507925	1467.857718	17.505459
38.758155	1463.229286	17.510477
38.851391	1461.881643	17.515495
38.487670	1467.345314	17.520512
38.618697	1466.107346	17.525530
38.290814	1467.930251	17.530547
38.545067	1464.715839	17.535565
38.296669	1476.344227	17.540583
38.262607	1488.574524	17.545600
38.655395	1482.242337	17.550618
38.497902	1496.600318	17.555635
39.174762	1492.439337	17.560653
39.079993	1489.263498	17.565671
39.216233	1494.669808	17.570688
39.285285	1486.818946	17.575706
39.152881	1489.050904	17.580723
39.162836	1492.438103	17.585741
39.334680	1482.729666	17.590759
39.199435	1492.621561	17.595776
39.665349	1481.124337	17.600794
39.294529	1489.512367	17.605811
39.266995	1495.048341	17.610829
38.949156	1485.804213	17.615847
39.421384	1485.993330	17.620864
39.341385	1482.651557	17.625882
39.306227	1496.863354	17.630899
39.542007	1487.443589	17.635917
39.469510	1491.591065	17.640935
39.926834	1500.460800	17.645952
40.077671	1489.984227	17.650970
39.884190	1489.033414	17.655987
40.005083	1490.846708	17.661005
40.062016	1491.451552	17.666023
39.792588	1490.194436	17.671040
40.209030	1479.028957	17.676058
40.142455	1492.581896	17.681075
39.963834	1488.452224	17.686093
39.859985	1480.976714	17.691111
39.646406	1488.105768	17.696128
40.055494	1488.402176	17.701146
39.989717	1489.080032	17.706163
40.296274	1485.084128	17.711181
40.309157	1483.874289	17.716199
39.920484	1495.180643	17.721216
40.328152	1490.118474	17.726234
39.934017	1499.951207	17.731251
39.668616	1491.634402	17.736269
39.701726	1487.104612	17.741287
39.825488	1497.354506	17.746304
40.323195	1508.321083	17.751322
40.066801	1511.286187	17.756339
40.172632	1519.142463	17.761357
40.345628	1511.207225	17.766375
40.051396	1516.849963	17.771392
40.092571	1515.121438	17.776410
40.309381	1522.939001	17.781427
40.629841	1540.867036	17.786445
40.845647	1543.175535	17.791463
40.431623	1552.619937	17.796480
40.770667	1535.357980	17.801498
40.719659	1545.618577	17.806515
40.305508	1543.429081	17.811533
40.610120	1543.340999	17.816551
40.228299	1547.618304	17.821568
40.350108	1542.770501	17.826586
40.515847	1556.058443	17.831603
40.536056	1571.874768	17.836621
40.885372	1570.211922	17.841639
40.821124	1584.232702	17.846656
41.235183	1568.691501	17.851674
41.181013	1566.004802	17.856691
40.970900	1566.123093	17.861709
41.517950	1562.418650	17.866727
41.219259	1566.185196	17.871744
41.187072	1568.064120	17.876762
41.490365	1573.811935	17.881779
41.143962	1567.890338	17.886797
41.477813	1560.895711	17.891815
41.457135	1570.586497	17.896832
41.566885	1566.752675	17.901850
41.665502	1568.280396	17.906867
41.347480	1564.581341	17.911885
41.493479	1559.677412	17.916903
41.319396	1575.357742	17.921920
41.901270	1572.906518	17.926938
41.941700	1580.616934	17.931955
41.875256	1576.871593	17.936973
41.825224	1555.129766	17.941991
41.636508	1558.143124	17.947008
42.168914	1569.280193	17.952026
42.167573	1570.126158	17.957043
41.813861	1556.259292	17.962061
42.060715	1546.046563	17.967079
42.041965	1556.331167	17.972096
42.111166	1555.446349	17.977114
42.054932	1557.324669	17.982131
41.969564	1570.266657	17.987149
42.437948	1572.136538	17.992167
42.150346	1581.951844	17.997184
42.462209	1582.707098	18.002202
42.666142	1590.704482	18.007219
42.322814	1568.453019	18.012237
42.561258	1561.714539	18.017255
42.855922	1563.281096	18.022272
42.181974	1550.249932	18.027290
42.293491	1552.368811	18.032307
42.491909	1558.814202	18.037325
42.579356	1571.195009	18.042343
42.145474	1587.548309	18.047360
42.196504	1583.354038	18.052378
42.277738	1585.013496	18.057395
42.241747	1582.428019	18.062413
42.313254	1585.241239	18.067431
42.302067	1594.614236	18.072448
42.588389	1601.787961	18.077466
42.646349	1612.183086	18.082483
42.429264	1620.623970	18.087501
42.913348	1617.406740	18.092519
43.166043	1621.677650	18.097536
43.308892	1625.064930	18.102554
43.202815	1616.646325	18.107571
43.071250	1613.767747	18.112589
43.366281	1615.257860	18.117607
43.163149	1620.294793	18.122624
43.019686	1613.548926	18.127642
42.746050	1615.465314	18.132659
42.812876	1631.124872	18.137677
43.428760	1639.314672	18.142695
43.365607	1647.520887	18.147712
43.824224	1650.771742	18.152730
43.645732	1649.797481	18.157747
43.351570	1655.166210	18.162765
43.837139	1645.705886	18.167783
43.787911	1651.031044	18.172800
43.881033	1642.030966	18.177818
44.025847	1637.808788	18.182835
43.364736	1629.291221	18.187853
43.585536	1625.477326	18.192871
43.646767	1637.788656	18.197888
43.700944	1642.729900	18.202906
43.826480	1635.914672	18.207923
43.735273	1641.400979	18.212941
43.994801	1629.566943	18.217959
43.671659	1648.161416	18.222976
43.653353	1642.272524	18.227994
43.733707	1645.264573	18.233011
43.809114	1644.088889	18.238029
44.364941	1650.591163	18.243047
44.109378	1662.036250	18.248064
44.237522	1667.410540	18.253082
44.451422	1663.665150	18.258099
44.710825	1668.003434	18.263117
44.703893	1639.126908	18.268135
44.792522	1631.980965	18.273152
44.938733	1618.611073	18.278170
45.256530	1624.286333	18.283187
44.745871	1630.231996	18.288205
44.867425	1619.543009	18.293223
45.170862	1622.685016	18.298240
44.661932	1619.618352	18.303258
44.890521	1613.913544	18.308275
44.894300	1622.344124	18.313293
44.579061	1598.437224	18.318311
44.687452	1612.006729	18.323328
44.300806	1622.302872	18.328346
44.645208	1616.272268	18.333363
44.346707	1623.417911	18.338381
44.422956	1623.521755	18.343399
44.672098	1634.937777	18.348416
44.643448	1639.926295	18.353434
45.165379	1645.694532	18.358451
44.642962	1657.149931	18.363469
44.775549	1648.761657	18.368487
44.798645	1654.291370	18.373504
45.035548	1670.668348	18.378522
45.326307	1678.317781	18.383539
45.493025	1684.375700	18.388557
45.551608	1678.328320	18.393575
45.484351	1684.920506	18.398592
45.666452	1683.971830	18.403610
46.034811	1680.639374	18.408627
45.846902	1681.303922	18.413645
46.104841	1660.376570	18.418663
46.039946	1647.729540	18.423680
45.697654	1643.235718	18.428698
46.104865	1643.361173	18.433715
45.690209	1657.738587	18.438733
46.450250	1642.491578	18.443751
46.032843	1640.740077	18.448768
45.753572	1640.479630	18.453786
45.744473	1642.372322	18.458803
45.724877	1653.140654	18.463821
45.761821	1650.793478	18.468839
46.006067	1653.488501	18.473856
45.957469	1652.584893	18.478874
45.955476	1656.337210	18.483891
46.022334	1676.903665	18.488909
46.025066	1676.533050	18.493927
46.125667	1679.214512	18.498944
45.906434	1686.588748	18.503962
46.357332	1679.972078	18.508979
46.318623	1685.978594	18.513997
46.352903	1676.641300	18.519015
46.395509	1678.021531	18.524032
46.253688	1683.005841	18.529050
46.513302	1679.678249	18.534067
46.364010	1698.379210	18.539085
46.792716	1712.124227	18.544103
46.779410	1701.216152	18.549120
46.667830	1713.597726	18.554138
46.888024	1702.558267	18.559155
46.891699	1703.474647	18.564173
47.011284	1706.159947	18.569191
46.754567	1708.480186	18.574208
46.327771	1705.451003	18.579226
46.550987	1695.266249	18.584243
46.716749	1709.807220	18.589261
46.823524	1726.785376	18.594279
47.223760	1733.968376	18.599296
47.150632	1738.747990	18.604314
47.172014	1733.452331	18.609331
47.348310	1735.708571	18.614349
47.233882	1727.154314	18.619367
47.229012	1737.184659	18.624384
47.251943	1737.530743	18.629402
47.635585	1736.458130	18.634419
47.305581	1738.590914	18.639437
47.415910	1728.291619	18.644455
47.718148	1725.266195	18.649472
47.773545	1730.119845	18.654490
48.113861	1722.618860	18.659507
47.406341	1731.656548	18.664525
47.341754	1731.325035	18.669543
47.594486	1750.573347	18.674560
47.506659	1761.322739	18.679578
48.010272	1749.312890	18.684595
48.090664	1760.242127	18.689613
48.162059	1756.357348	18.694631
48.480158	1754.073383	18.699648
48.207486	1757.392153	18.704666
48.598882	1749.207514	18.709683
48.497063	1756.545901	18.714701
48.272287	1745.945344	18.719719
48.788781	1746.864366	18.724736
48.344517	1730.341290	18.729754
48.317406	1710.784553	18.734771
48.141668	1722.729838	18.739789
48.356055	1737.270373	18.744807
48.437332	1741.426988	18.749824
48.156133	1743.121826	18.754842
48.511901	1747.049470	18.759859
48.361894	1759.321119	18.764877
48.152739	1752.219876	18.769895
48.604662	1750.930806	18.774912
48.357577	1753.036776	18.779930
48.689258	1766.450796	18.784947
48.656767	1780.135557	18.789965
48.599390	1790.454106	18.794983
48.740742	1788.127203	18.800000
48.664132	1793.546878	18.805018
48.927925	1791.723849	18.810035
48.886355	1787.681637	18.815053
49.068221	1785.016250	18.820071
48.956190	1786.573415	18.825088
48.986284	1803.874288	18.830106
49.109394	1807.772930	18.835123
49.056568	1819.186522	18.840141
49.631960	1817.167135	18.845159
49.570076	1814.178529	18.850176
49.428795	1818.980877	18.855194
49.448752	1815.524246	18.860211
49.397310	1821.004979	18.865229
49.464433	1820.717820	18.870247
49.890360	1813.755333	18.875264
49.496341	1818.584869	18.880282
49.800100	1809.426125	18.885299
49.854837	1807.608617	18.890317
49.482906	1815.728080	18.895335
49.976348	1812.743882	18.900352
49.470880	1817.834682	18.905370
50.233203	1830.798105	18.910387
50.197789	1847.472777	18.915405
49.949044	1849.372719	18.920423
49.981588	1839.950969	18.925440
49.758796	1844.079812	18.930458
50.218192	1842.022822	18.935475
50.470419	1846.380106	18.940493
50.308839	1844.700481	18.945511
50.092216	1836.764942	18.950528
50.525281	1845.998529	18.955546
50.977653	1842.759129	18.960563
51.180210	1840.871780	18.965581
51.066046	1846.936182	18.970599
51.112458	1836.797400	18.975616
50.650666	1824.449800	18.980634
50.601247	1813.440738	18.985651
50.505571	1810.671732	18.990669
49.895701	1830.433434	18.995687
50.350318	1832.899877	19.000704
50.382813	1844.008272	19.005722
50.738359	1832.615946	19.010739
50.835435	1837.286084	19.015757
50.936982	1857.876362	19.020775
51.061354	1860.824286	19.025792
50.865345	1877.428873	19.030810
50.923632	1868.156256	19.035827
51.023545	1870.445299	19.040845
50.684659	1878.833967	19.045863
50.688614	1868.939481	19.050880
51.137956	1873.808322	19.055898
51.369747	1884.520325	19.060915
51.493102	1895.560809	19.065933
51.525021	1898.752574	19.070951
52.086169	1887.164309	19.075968
51.891392	1883.521615	19.080986
51.606469	1871.513386	19.086003
51.547177	1870.829343	19.091021
51.712922	1883.325730	19.096039
51.920129	1888.936967	19.101056
51.964810	1893.088871	19.106074
52.222316	1894.724440	19.111091
52.042060	1870.040341	19.116109
51.640238	1875.337827	19.121127
51.898960	1871.135433	19.126144
51.674901	1886.930562	19.131162
52.131660	1886.797494	19.136179
52.328024	1889.500768	19.141197
52.065865	1893.022515	19.146215
52.510333	1890.738915	19.151232
51.926898	1902.718798	19.156250
52.226498	1892.357414	19.161267
52.221720	1900.009195	19.166285
52.479594	1896.933857	19.171303
52.615737	1892.754442	19.176320
52.418429	1892.787851	19.181338
52.331778	1899.195238	19.186355
52.519548	1904.692082	19.191373
52.570260	1908.814606	19.196391
53.165387	1910.473011	19.201408
52.927474	1912.414810	19.206426
53.310148	1910.430028	19.211443
52.977070	1909.213715	19.216461
53.085787	1911.270123	19.221479
53.511152	1906.131944	19.226496
53.158151	1910.168547	19.231514
52.957195	1911.731914	19.236531
53.313956	1901.384742	19.241549
53.044190	1907.960160	19.246567
53.416994	1900.953192	19.251584
53.330118	1918.888106	19.256602
53.425697	1914.801478	19.261619
53.393340	1903.671301	19.266637
53.154827	1906.682632	19.271655
53.587636	1898.894805	19.276672
53.601067	1903.089082	19.281690
53.346444	1909.254765	19.286707
53.688738	1902.767661	19.291725
53.356671	1908.807233	19.296743
53.155574	1902.113648	19.301760
53.373633	1916.535201	19.306778
53.789686	1933.657433	19.311795
53.991749	1929.646651	19.316813
54.047316	1939.838440	19.321831
53.980680	1937.335728	19.326848
54.312861	1935.945504	19.331866
54.184045	1937.677238	19.336883
54.412253	1930.971068	19.341901
54.128518	1929.942382	19.346919
54.482415	1922.339748	19.351936
54.293158	1935.740459	19.356954
54.359661	1929.842432	19.361971
54.248650	1930.645793	19.366989
54.041875	1926.800395	19.372007
54.624931	1920.386194	19.377024
54.290641	1925.476817	19.382042
54.224941	1930.023689	19.387059
54.622204	1934.226193	19.392077
54.830576	1948.305690	19.397095
54.512537	1957.060559	19.402112
54.847567	1955.191829	19.407130
55.185533	1953.509234	19.412147
55.386500	1941.732648	19.417165
55.305547	1950.053112	19.422183
55.131325	1936.037795	19.427200
54.984864	1930.781477	19.432218
54.893019	1940.262616	19.437235
55.233486	1939.905753	19.442253
55.417378	1940.894807	19.447271
55.698279	1935.859744	19.452288
55.474744	1939.984802	19.457306
55.183238	1943.855337	19.462323
55.540134	1940.821289	19.467341
55.309333	1951.161802	19.472359
55.910520	1937.580152	19.477376
56.096939	1939.375965	19.482394
55.867047	1935.551459	19.487411
56.233644	1934.122653	19.492429
55.613463	1939.111489	19.497447
55.594284	1937.418859	19.502464
55.882513	1939.021997	19.507482
55.801048	1938.368134	19.512499
55.788873	1938.848605	19.517517
55.441106	1939.583883	19.522535
55.398722	1933.895492	19.527552
55.767808	1952.985898	19.532570
55.419209	1968.246089	19.537587
56.070849	1972.832607	19.542605
55.961906	1964.589525	19.547623
56.505165	1967.980682	19.552640
56.498447	1968.823259	19.557658
56.475226	1973.733777	19.562675
56.533155	1960.212172	19.567693
56.187665	1957.175299	19.572711
56.664297	1972.658625	19.577728
56.686852	1975.975256	19.582746
56.939159	1989.655474	19.587763
56.760782	1991.841046	19.592781
56.454128	1997.723125	19.597799
56.951367	1991.255882	19.602816
56.879949	1993.597550	19.607834
56.719264	1992.471768	19.612851
57.171229	1978.207696	19.617869
56.922565	1989.719565	19.622887
56.947188	1988.623438	19.627904
56.991387	1993.667304	19.632922
56.764733	1990.369073	19.637939
57.228225	1997.637427	19.642957
57.276519	2021.886758	19.647975
57.113112	2023.764609	19.652992
57.314648	2022.635392	19.658010
57.254366	2027.763333	19.663027
57.839170	2017.758930	19.668045
57.234207	2025.890890	19.673063
57.623089	2013.075989	19.678080
57.871549	2011.331558	19.683098
58.197791	2015.754951	19.688115
58.236439	2005.555964	19.693133
57.797012	2008.037905	19.698151
58.048542	2009.153574	19.703168
58.023606	2010.429650	19.708186
58.132392	2011.428435	19.713203
58.120047	1991.709344	19.718221
58.178995	1997.580717	19.723239
58.139883	1999.718395	19.728256
58.761807	2014.504320	19.733274
58.535594	2017.726191	19.738291
58.622585	2003.004521	19.743309
58.571837	1998.159781	19.748327
58.478429	1999.937820	19.753344
58.566550	1997.407779	19.758362
58.973660	2017.870672	19.763379
59.326778	2012.901561	19.768397
59.033110	2007.730699	19.773415
59.116726	1998.281591	19.778432
58.692367	1993.750941	19.783450
58.845515	1997.697244	19.788467
58.924558	1997.254081	19.793485
58.714333	1993.033616	19.798503
59.051223	2002.103447	19.803520
59.448092	2011.234269	19.808538
59.294328	2026.628458	19.813555
59.360649	2004.227387	19.818573
59.299832	2000.734950	19.823591
58.724195	2008.695315	19.828608
58.876393	2012.483102	19.833626
59.352194	2019.488297	19.838643
59.963311	2020.288739	19.843661
59.755381	2025.694390	19.848679
59.440848	2019.054065	19.853696
59.707489	2023.807408	19.858714
59.480953	2019.686596	19.863731
59.737409	2009.345919	19.868749
59.561064	2014.523287	19.873767
59.624188	2015.824822	19.878784
59.769406	2033.864191	19.883802
60.088252	2048.061471	19.888819
59.857272	2057.225937	19.893837
59.618600	2055.189770	19.898855
59.594043	2051.897039	19.903872
59.882946	2052.488122	19.908890
59.966108	2064.343210	19.913907
60.275286	2077.847590	19.918925
60.311555	2084.199328	19.923943
60.220740	2078.371530	19.928960
60.555073	2071.182867	19.933978
60.560991	2072.856865	19.938995
60.663878	2063.777694	19.944013
61.019046	2073.767396	19.949031
61.470145	2076.495937	19.954048
61.155325	2065.330990	19.959066
61.120135	2070.476694	19.964083
61.052811	2062.777289	19.969101
60.916968	2067.796134	19.974119
60.951587	2060.986860	19.979136
61.005497	2059.468326	19.984154
61.274453	2075.423248	19.989171
61.485248	2068.902708	19.994189
61.020994	2066.474445	19.999207
60.744856	2078.370276	20.004224
61.272373	2075.271512	20.009242
61.428180	2093.730453	20.014259
61.627109	2095.120539	20.019277
61.312975	2098.579184	20.024295
61.306283	2101.300378	20.029312
61.380590	2091.732320	20.034330
61.736349	2101.628225	20.039347
61.819544	2092.658728	20.044365
61.625887	2094.335444	20.049383
62.055060	2104.235302	20.054400
62.234453	2105.978788	20.059418
62.013863	2115.858932	20.064435
61.947081	2115.008815	20.069453
62.301678	2130.024962	20.074471
61.974234	2129.033681	20.079488
61.973110	2123.158200	20.084506
61.909057	2131.600290	20.089523
62.012440	2126.244764	20.094541
62.228917	2124.701896	20.099559
62.265052	2124.545259	20.104576
62.500365	2129.945043	20.109594
62.487710	2153.846709	20.114611
62.695197	2154.099341	20.119629
63.256272	2155.303310	20.124647
62.895702	2152.078798	20.129664
63.234530	2147.675956	20.134682
63.247439	2150.426085	20.139699
63.018709	2151.219715	20.144717
63.036442	2151.934864	20.149735
62.968538	2160.137437	20.154752
62.904498	2150.658820	20.159770
63.261079	2157.076555	20.164787
63.225129	2149.147681	20.169805
63.358055	2146.978885	20.174823
63.302983	2151.721272	20.179840
63.250093	2142.608518	20.184858
62.965247	2145.318344	20.189875
63.287856	2149.349428	20.194893
63.787652	2160.932342	20.199911
63.482271	2172.698985	20.204928
64.093514	2161.184620	20.209946
64.060436	2179.271656	20.214963
63.994688	2178.612725	20.219981
64.268356	2183.598017	20.224999
64.630122	2171.296373	20.230016
64.516259	2161.868818	20.235034
64.097718	2157.291840	20.240051
64.199513	2142.677753	20.245069
63.926863	2160.309706	20.250087
63.642250	2172.734303	20.255104
64.056519	2172.300207	20.260122
64.305529	2168.457720	20.265139
64.240034	2160.862299	20.270157
64.127805	2177.886368	20.275175
64.362207	2196.656806	20.280192
64.641449	2204.226572	20.285210
64.421710	2200.184873	20.290227
64.883447	2200.393916	20.295245
65.008964	2199.543902	20.300263
65.015518	2209.205607	20.305280
65.101380	2201.633043	20.310298
64.518466	2199.333387	20.315315
64.574210	2207.664415	20.320333
65.310893	2225.058817	20.325351
64.961561	2234.687051	20.330368
65.430437	2233.671852	20.335386
65.282548	2230.725868	20.340403
65.335046	2234.545764	20.345421
65.670967	2226.884641	20.350439
65.641193	2235.168918	20.355456
66.004831	2224.030867	20.360474
65.700684	2234.881460	20.365491
65.576689	2234.409705	20.370509
66.009972	2221.796503	20.375527
65.876980	2226.805066	20.380544
65.705764	2216.528913	20.385562
65.854188	2224.284921	20.390579
65.956801	2229.850031	20.395597
66.081174	2241.283952	20.400615
66.341260	2255.665931	20.405632
66.499051	2249.230006	20.410650
66.290777	2264.094715	20.415667
66.296772	2256.543693	20.420685
66.419635	2255.880773	20.425703
65.962310	2263.551649	20.430720
66.149343	2254.524487	20.435738
65.752415	2258.590759	20.440755
66.222052	2275.123776	20.445773
66.119747	2270.398045	20.450791
66.108811	2283.385350	20.455808
66.205483	2285.963637	20.460826
66.772150	2302.847035	20.465843
66.692340	2311.026527	20.470861
66.766468	2303.011763	20.475879
66.844336	2304.675025	20.480896
67.298202	2302.114911	20.485914
67.369976	2306.778108	20.490931
67.237662	2302.767071	20.495949
67.765253	2310.773125	20.500967
67.446216	2322.123258	20.505984
67.290659	2327.434980	20.511002
67.569786	2328.954274	20.516019
68.012852	2336.687386	20.521037
68.405592	2327.014583	20.526055
68.043629	2320.129859	20.531072
67.839651	2305.467242	20.536090
67.685710	2308.810659	20.541107
67.979493	2323.127072	20.546125
68.193958	2319.688958	20.551143
68.221368	2336.269508	20.556160
68.287545	2331.992900	20.561178
68.272185	2336.978968	20.566195
68.173019	2338.681248	20.571213
68.516738	2331.839338	20.576231
67.964807	2331.485837	20.581248
68.435644	2323.197504	20.586266
68.283814	2329.254374	20.591283
68.028302	2326.983619	20.596301
68.158829	2333.570125	20.601319
68.283582	2353.700706	20.606336
68.317871	2355.063522	20.611354
68.547513	2356.602328	20.616371
68.640366	2380.153914	20.621389
68.919290	2377.508015	20.626407
69.411686	2389.460144	20.631424
69.718009	2377.747465	20.636442
69.534216	2391.316552	20.641459
69.109651	2384.659890	20.646477
69.555093	2380.489139	20.651495
69.162547	2381.420332	20.656512
69.525192	2384.584633	20.661530
69.233730	2372.208969	20.666547
69.310828	2376.479086	20.671565
69.836131	2380.609359	20.676583
69.553118	2377.648713	20.681600
69.906406	2369.578178	20.686618
69.915730	2373.763836	20.691635
69.887909	2379.888455	20.696653
69.779824	2374.647065	20.701671
69.399474	2393.379018	20.706688
70.098263	2402.049580	20.711706
69.843326	2407.534298	20.716723
70.104518	2416.414560	20.721741
70.319403	2411.225677	20.726759
70.261477	2415.493753	20.731776
70.359968	2414.362488	20.736794
70.526670	2425.119099	20.741811
70.379558	2435.053785	20.746829
71.185659	2432.977445	20.751847
71.630329	2426.307982	20.756864
71.861321	2400.553163	20.761882
71.659587	2387.599021	20.766899
71.717979	2391.602227	20.771917
71.786123	2383.547496	20.776935
71.734201	2371.526103	20.781952
71.834832	2359.800663	20.786970
71.890127	2348.837455	20.791987
71.706820	2348.718439	20.797005
71.919351	2342.144724	20.802023
71.821128	2345.133661	20.807040
71.812366	2344.916992	20.812058
71.739411	2332.318042	20.817075
71.253442	2327.265095	20.822093
71.102226	2336.545990	20.827111
71.444958	2342.715744	20.832128
71.526552	2338.256147	20.837146
71.312323	2351.906021	20.842163
71.333906	2380.193409	20.847181
71.276225	2376.738152	20.852199
71.776080	2392.743196	20.857216
72.041697	2392.685031	20.862234
72.504862	2403.549094	20.867251
72.360786	2417.831983	20.872269
72.619541	2419.701292	20.877287
72.282167	2423.176986	20.882304
72.287432	2422.805131	20.887322
72.178032	2424.827337	20.892339
72.047684	2424.066067	20.897357
72.358223	2420.357088	20.902375
72.475233	2447.909223	20.907392
72.345343	2456.201331	20.912410
72.600385	2453.627242	20.917427
72.301283	2458.892741	20.922445
72.732547	2463.269906	20.927463
72.578019	2482.201083	20.932480
72.618011	2488.670083	20.937498
72.825663	2488.532077	20.942515
72.809843	2499.807515	20.947533
73.282546	2509.489503	20.952551
73.316571	2513.812719	20.957568
73.674958	2511.933621	20.962586
74.011412	2510.041745	20.967603
73.734815	2512.053251	20.972621
74.217577	2509.215664	20.977639
73.776603	2512.379950	20.982656
74.074744	2515.633303	20.987674
73.857195	2508.894631	20.992691
73.828257	2509.676863	20.997709
74.275965	2497.776049	21.002727
74.106138	2505.521394	21.007744
73.854011	2511.853053	21.012762
74.360441	2522.704268	21.017779
74.178007	2530.369882	21.022797
74.493667	2521.945031	21.027815
74.870704	2530.492846	21.032832
74.879479	2529.438381	21.037850
74.977051	2532.420561	21.042867
74.852565	2530.605346	21.047885
75.123134	2528.166402	21.052903
74.865399	2530.206964	21.057920
74.826294	2527.373792	21.062938
74.590689	2536.963023	21.067955
74.811989	2530.373551	21.072973
74.792032	2528.259266	21.077991
75.243225	2554.076844	21.083008
75.135817	2565.384569	21.088026
75.340464	2561.172363	21.093043
75.159479	2575.592454	21.098061
75.183362	2566.511181	21.103079
75.509948	2574.621136	21.108096
75.238380	2595.382276	21.113114
75.988928	2595.836352	21.118131
75.596296	2596.394277	21.123149
76.147388	2592.649530	21.128167
76.320963	2594.439747	21.133184
76.189228	2597.692001	21.138202
76.229377	2590.338936	21.143219
76.068353	2585.542059	21.148237
76.131300	2583.445841	21.153255
76.073139	2590.944485	21.158272
75.668993	2601.436818	21.163290
76.311144	2611.248902	21.168307
76.287178	2611.211246	21.173325
76.407578	2607.419054	21.178343
76.227675	2621.954770	21.183360
76.442790	2644.561220	21.188378
76.685713	2637.021373	21.193395
76.944178	2642.856813	21.198413
77.195661	2641.050369	21.203431
77.435249	2638.886058	21.208448
77.219436	2637.660605	21.213466
77.823415	2635.789003	21.218483
77.734943	2641.420884	21.223501
77.841068	2634.323463	21.228519
77.893230	2643.134948	21.233536
77.883243	2641.736387	21.238554
77.996060	2621.942674	21.243571
77.217280	2622.880243	21.248589
77.597519	2631.859136	21.253607
77.445882	2636.974193	21.258624
77.200798	2642.697503	21.263642
77.616294	2644.451763	21.268659
78.093139	2658.107853	21.273677
78.062627	2666.229462	21.278695
77.925198	2667.557955	21.283712
77.998508	2670.860125	21.288730
78.290897	2675.647843	21.293747
78.150159	2681.190257	21.298765
77.951851	2685.088702	21.303783
78.616476	2687.557084	21.308800
78.515108	2699.619911	21.313818
78.650096	2697.382170	21.318835
78.741570	2697.300308	21.323853
78.696151	2691.245561	21.328871
78.960641	2689.554225	21.333888
78.903251	2700.199811	21.338906
79.245189	2690.174802	21.343923
79.336790	2695.174147	21.348941
79.343965	2709.170693	21.353959
80.088068	2697.679627	21.358976
79.720163	2687.930675	21.363994
79.692422	2681.943780	21.369011
79.585376	2677.675512	21.374029
79.510042	2674.748507	21.379047
79.607787	2693.935167	21.384064
79.681309	2704.749685	21.389082
80.649212	2707.417302	21.394099
79.984060	2712.316429	21.399117
79.707431	2713.403388	21.404135
80.185257	2711.675475	21.409152
80.081561	2711.281342	21.414170
80.330844	2707.700143	21.419187
80.324755	2715.260798	21.424205
79.962291	2706.698519	21.429223
80.370594	2716.643691	21.434240
80.439782	2734.983962	21.439258
80.834498	2740.421995	21.444275
80.939471	2746.421610	21.449293
80.923113	2743.967246	21.454311
80.572655	2739.109868	21.459328
80.667637	2748.578760	21.464346
80.719670	2742.721498	21.469363
80.986027	2743.641339	21.474381
81.122147	2731.540179	21.479399
81.172772	2757.067646	21.484416
81.194290	2770.751495	21.489434
81.340363	2776.496784	21.494451
81.706268	2770.605390	21.499469
81.275226	2768.922246	21.504487
81.464425	2774.220690	21.509504
81.659317	2786.239092	21.514522
81.979859	2766.122130	21.519539
81.703816	2770.311927	21.524557
81.215172	2770.388588	21.529575
81.824890	2784.937926	21.534592
81.581075	2800.077787	21.539610
82.095707	2798.856250	21.544627
82.224357	2799.353162	21.549645
81.979496	2809.842739	21.554663
82.060431	2819.017963	21.559680
82.159263	2820.736752	21.564698
82.530682	2825.833863	21.569715
82.736797	2821.489028	21.574733
82.961750	2823.608322	21.579751
83.386858	2822.968379	21.584768
82.761874	2822.614786	21.589786
83.599837	2814.871245	21.594803
83.701816	2809.584244	21.599821
83.628101	2811.234959	21.604839
83.756720	2813.539303	21.609856
83.905398	2812.943602	21.614874
83.885632	2807.819233	21.619891
83.785368	2806.537728	21.624909
83.975315	2810.067222	21.629927
83.958670	2805.649537	21.634944
84.002723	2816.680248	21.639962
83.872378	2808.067092	21.644979
84.373438	2810.795864	21.649997
83.781433	2807.463619	21.655015
84.015099	2798.461229	21.660032
84.073313	2810.254217	21.665050
84.320964	2807.875075	21.670067
84.155568	2809.052440	21.675085
83.929427	2807.318411	21.680103
84.092789	2807.332906	21.685120
84.157429	2826.173369	21.690138
84.351440	2828.182199	21.695155
84.600825	2832.767850	21.700173
84.429207	2843.211027	21.705191
84.571788	2840.824693	21.710208
84.806906	2859.194940	21.715226
84.930681	2865.002364	21.720243
84.885749	2881.384828	21.725261
84.828423	2878.502737	21.730279
84.917215	2864.586406	21.735296
85.171527	2891.758232	21.740314
85.332979	2899.623387	21.745331
85.779866	2900.040542	21.750349
85.409770	2903.663709	21.755367
85.645259	2901.652851	21.760384
85.424212	2904.505439	21.765402
85.297958	2896.086847	21.770419
85.774801	2904.983182	21.775437
85.824986	2923.508068	21.780455
85.742001	2917.942445	21.785472
85.830336	2924.060750	21.790490
85.900778	2932.191966	21.795507
86.101794	2920.393771	21.800525
86.200495	2934.622905	21.805543
86.858279	2946.705407	21.810560
86.876214	2949.675331	21.815578
87.034287	2933.571043	21.820595
87.474728	2939.125741	21.825613
87.032216	2928.422311	21.830631
86.934302	2909.351113	21.835648
87.133543	2917.347620	21.840666
87.447688	2922.123809	21.845683
87.074630	2913.445886	21.850701
86.859760	2930.595475	21.855719
87.225910	2940.655125	21.860736
87.043404	2944.572976	21.865754
87.142746	2939.608494	21.870771
87.280448	2947.496646	21.875789
87.280956	2974.793246	21.880807
87.829735	2964.539651	21.885824
87.599727	2974.571582	21.890842
87.731473	2971.023076	21.895859
88.111181	2969.015837	21.900877
87.871262	2963.693681	21.905895
88.501300	2977.703390	21.910912
88.475421	2990.152790	21.915930
88.527009	2979.378004	21.920947
88.527028	2985.837524	21.925965
88.659153	2994.662274	21.930983
89.046496	2983.487336	21.936000
89.124696	2989.778305	21.941018
89.195089	2994.790832	21.946035
89.103044	2993.199180	21.951053
88.916213	2987.522176	21.956071
89.144594	2986.378841	21.961088
88.972159	2981.428650	21.966106
89.162653	2977.585762	21.971123
89.910716	2975.982393	21.976141
89.772476	2989.395336	21.981159
89.589671	2976.657977	21.986176
89.697682	2987.015507	21.991194
89.713815	2981.845548	21.996211
89.862073	2973.742915	22.001229
89.563184	2971.606297	22.006247
89.612379	2971.171769	22.011264
89.604259	2987.245611	22.016282
89.632201	2993.276640	22.021299
90.172452	2999.951483	22.026317
89.854738	3014.827786	22.031335
90.482550	3012.879602	22.036352
90.541337	3009.901187	22.041370
90.038515	3000.409863	22.046387
90.387460	3027.116791	22.051405
90.675650	3043.254874	22.056423
90.431529	3030.227923	22.061440
90.439648	3036.401765	22.066458
90.530354	3034.614966	22.071475
91.061985	3049.719781	22.076493
91.042882	3070.603651	22.081511
90.768092	3071.593448	22.086528
91.223604	3073.032174	22.091546
90.872082	3073.750815	22.096563
91.129252	3073.588566	22.101581
91.248429	3089.567444	22.106599
91.486414	3092.898176	22.111616
91.616143	3099.443401	22.116634
91.499697	3097.736212	22.121651
91.489626	3093.907205	22.126669
91.294771	3115.569451	22.131687
91.940031	3113.409559	22.136704
92.141319	3120.871063	22.141722
92.154824	3121.122318	22.146739
92.605367	3120.025155	22.151757
92.580149	3138.345853	22.156775
93.001494	3134.650791	22.161792
92.804395	3133.015705	22.166810
92.881926	3137.925459	22.171827
93.592674	3135.499166	22.176845
93.340802	3119.661861	22.181863
93.612241	3103.481260	22.186880
93.705070	3101.516100	22.191898
93.357748	3097.622837	22.196915
93.606375	3095.384460	22.201933
93.179430	3093.999850	22.206951
93.705691	3093.755240	22.211968
93.383535	3101.604961	22.216986
93.184266	3108.213681	22.222003
93.564220	3111.925673	22.227021
93.517911	3136.946646	22.232039
93.457590	3130.764336	22.237056
93.670698	3133.588212	22.242074
93.945514	3149.056903	22.247091
94.145339	3156.661225	22.252109
93.893063	3163.334973	22.257127
94.369876	3165.600151	22.262144
94.583812	3161.895750	22.267162
94.385232	3164.579931	22.272179
94.641720	3169.935492	22.277197
94.390555	3182.118878	22.282215
94.724966	3173.793637	22.287232
94.952995	3187.421180	22.292250
94.390797	3188.426391	22.297267
95.067386	3188.849855	22.302285
95.121580	3199.706618	22.307303
94.718876	3198.193407	22.312320
95.415589	3212.248602	22.317338
95.014743	3223.905595	22.322355
95.212623	3223.908660	22.327373
95.238156	3234.550629	22.332391
95.365273	3241.380674	22.337408
96.147491	3249.134855	22.342426
95.893793	3250.126559	22.347443
96.006192	3244.408400	22.352461
96.577116	3253.397491	22.357479
96.450634	3245.469406	22.362496
96.881847	3251.456601	22.367514
96.312789	3242.864076	22.372531
96.608384	3241.562711	22.377549
96.532257	3244.301519	22.382567
96.584962	3239.990747	22.387584
96.756829	3239.765939	22.392602
96.765751	3239.288691	22.397619
97.017278	3241.775221	22.402637
97.127375	3250.897656	22.407655
97.010125	3263.830753	22.412672
96.847788	3261.631306	22.417690
97.099591	3276.329885	22.422707
97.418068	3266.577884	22.427725
96.824641	3273.484218	22.432743
97.662659	3282.705548	22.437760
97.987525	3290.452313	22.442778
97.861040	3295.794816	22.447795
98.014005	3286.965074	22.452813
97.943932	3295.875063	22.457831
98.092405	3288.096713	22.462848
98.474789	3283.187558	22.467866
98.062153	3294.474102	22.472883
98.359926	3291.796470	22.477901
98.261490	3298.123358	22.482919
98.549187	3310.712207	22.487936
99.056724	3313.445473	22.492954
98.674512	3308.845384	22.497971
99.067373	3316.041016	22.502989
99.094598	3318.205303	22.508007
98.962034	3318.371343	22.513024
98.942711	3315.130611	22.518042
99.027474	3316.920387	22.523059
99.132874	3312.699007	22.528077
99.103915	3342.121447	22.533095
99.319638	3347.388761	22.538112
99.732371	3342.060908	22.543130
99.558551	3349.743557	22.548147
99.429746	3342.134791	22.553165
99.960178	3361.177992	22.558183
99.959953	3365.928668	22.563200
99.824512	3374.768788	22.568218
100.144564	3380.862511	22.573235
100.401335	3376.689983	22.578253
100.508239	3376.105362	22.583271
100.622979	3378.995764	22.588288
100.636691	3376.856690	22.593306
100.379158	3379.012311	22.598323
100.414438	3373.289213	22.603341
100.490520	3399.902578	22.608359
100.464533	3409.476878	22.613376
101.213833	3394.884511	22.618394
101.450338	3393.766532	22.623411
101.543844	3384.068779	22.628429
101.641897	3385.705857	22.633447
101.269019	3390.455058	22.638464
101.626491	3397.085801	22.643482
101.248196	3401.569733	22.648499
101.826900	3414.623065	22.653517
101.918513	3423.619606	22.658535
101.924659	3427.190202	22.663552
102.133117	3420.449772	22.668570
102.396834	3434.372266	22.673587
101.961493	3434.006617	22.678605
102.380114	3429.040013	22.683623
102.027890	3431.426883	22.688640
102.073376	3445.889277	22.693658
102.465857	3457.028458	22.698675
102.525219	3456.703223	22.703693
102.493018	3459.225828	22.708711
102.618278	3478.149614	22.713728
102.788600	3479.475818	22.718746
102.801538	3491.778769	22.723763
103.075419	3479.273804	22.728781
102.984312	3493.194174	22.733799
103.010325	3511.583706	22.738816
103.523366	3508.236703	22.743834
103.002527	3512.875842	22.748851
103.700198	3522.812876	22.753869
103.525216	3542.801046	22.758887
103.706213	3543.300823	22.763904
104.126665	3537.324187	22.768922
103.946208	3548.022947	22.773939
104.066860	3543.877650	22.778957
104.774055	3555.537885	22.783975
105.201391	3551.923610	22.788992
105.399786	3529.422904	22.794010
105.658928	3513.677164	22.799027
105.787961	3520.974039	22.804045
105.598586	3515.607588	22.809063
105.680342	3511.566628	22.814080
105.587543	3492.240243	22.819098
105.412857	3488.276331	22.824115
105.373983	3478.687849	22.829133
105.358391	3482.103092	22.834151
105.531970	3496.881445	22.839168
105.801114	3502.271968	22.844186
106.056361	3503.938028	22.849203
106.161195	3510.492418	22.854221
106.122260	3510.428185	22.859239
106.117333	3519.105821	22.864256
106.279548	3505.703230	22.869274
106.533166	3514.954793	22.874291
106.265815	3510.390870	22.879309
106.639328	3501.686228	22.884327
106.313608	3518.894837	22.889344
106.382046	3502.580874	22.894362
106.597598	3507.641138	22.899379
106.317407	3503.826836	22.904397
106.074712	3517.219544	22.909415
106.386308	3525.432588	22.914432
106.866151	3538.347818	22.919450
106.385924	3551.459942	22.924467
106.603730	3561.896688	22.929485
106.937930	3577.747840	22.934503
106.818714	3595.248766	22.939520
107.092614	3600.628268	22.944538
107.059834	3615.538197	22.949555
107.354843	3630.180870	22.954573
107.809949	3628.784396	22.959591
108.319977	3628.426002	22.964608
108.888215	3620.604667	22.969626
108.689560	3625.455597	22.974643
108.778526	3628.557600	22.979661
108.614623	3624.557151	22.984679
108.328998	3629.132371	22.989696
108.894005	3618.213211	22.994714
108.929913	3631.044744	22.999731
108.521789	3631.779412	23.004749
109.052716	3640.364462	23.009767
108.837139	3642.718486	23.014784
109.115027	3647.816151	23.019802
108.952055	3662.868158	23.024819
108.991842	3674.939035	23.029837
109.318464	3686.932394	23.034855
109.314816	3692.552471	23.039872
109.561755	3685.233539	23.044890
109.664906	3697.217961	23.049907
109.603825	3707.526195	23.054925
109.876198	3709.312206	23.059943
109.905013	3713.386978	23.064960
110.052707	3715.436155	23.069978
110.128279	3738.674552	23.074995
110.716131	3749.584336	23.080013
110.919527	3743.174639	23.085031
110.494350	3754.073799	23.090048
110.978890	3741.026877	23.095066
110.583381	3731.912868	23.100083
110.889514	3752.252788	23.105101
110.978614	3758.991126	23.110119
111.207176	3772.964840	23.115136
111.581688	3761.003958	23.120154
111.499963	3767.897601	23.125171
111.450969	3768.204474	23.130189
111.626168	3759.755791	23.135207
111.518643	3771.529082	23.140224
111.849390	3784.792203	23.145242
112.068537	3795.447040	23.150259
112.117619	3793.115972	23.155277
112.183260	3795.590354	23.160295
111.851510	3795.702334	23.165312
112.146144	3791.583065	23.170330
112.474164	3806.102890	23.175347
112.255462	3820.699130	23.180365
112.487190	3823.003275	23.185383
112.927791	3829.217487	23.190400
112.947183	3819.113169	23.195418
112.563424	3832.796536	23.200435
112.987605	3846.784035	23.205453
113.056647	3853.858220	23.210471
113.290164	3863.525350	23.215488
113.559661	3861.684179	23.220506
113.793868	3874.624470	23.225523
113.839272	3881.864178	23.230541
114.177827	3874.032476	23.235559
114.653333	3873.729615	23.240576
114.949046	3861.745937	23.245594
114.803106	3851.944028	23.250611
115.084911	3834.975664	23.255629
115.023125	3820.289615	23.260647
115.150819	3824.671168	23.265664
115.344742	3816.795768	23.270682
115.457917	3819.514036	23.275699
115.257319	3820.263540	23.280717
115.345483	3820.269665	23.285735
115.226430	3820.408190	23.290752
115.212093	3817.444522	23.295770
114.924530	3817.903347	23.300787
114.913049	3823.242064	23.305805
115.470331	3836.051328	23.310823
115.231025	3847.166781	23.315840
114.893204	3855.508658	23.320858
115.503499	3870.009293	23.325875
115.744988	3882.632514	23.330893
115.834012	3889.489849	23.335911
116.053210	3893.200449	23.340928
116.274285	3918.687977	23.345946
116.283833	3915.186988	23.350963
116.226656	3915.100677	23.355981
116.282504	3915.629010	23.360999
116.327228	3938.127915	23.366016
116.651822	3951.296144	23.371034
116.699191	3948.205308	23.376051
116.897388	3952.722092	23.381069
117.369109	3966.798425	23.386087
117.256110	3984.301078	23.391104
117.480945	3977.237049	23.396122
117.612020	3973.620700	23.401139
118.007550	3977.957167	23.406157
118.238647	3964.762909	23.411175
117.918467	3967.150665	23.416192
118.245559	3975.581031	23.421210
118.288843	3966.848474	23.426227
117.970406	3963.238305	23.431245
118.438062	3980.280686	23.436263
118.487360	3988.816178	23.441280
118.664090	3995.485250	23.446298
118.393512	3992.263824	23.451315
118.402152	3995.734095	23.456333
118.601809	3998.840823	23.461351
119.192030	4012.601529	23.466368
119.331673	4018.387758	23.471386
119.295257	4017.700091	23.476403
119.205924	4023.325523	23.481421
119.281574	4010.799778	23.486439
119.702808	4030.236628	23.491456
119.573795	4038.586910	23.496474
120.112262	4041.236245	23.501491
119.878225	4051.554663	23.506509
119.998265	4047.392800	23.511527
119.911133	4054.479672	23.516544
120.220316	4062.711527	23.521562
120.898602	4069.352929	23.526579
120.696637	4064.809139	23.531597
121.391456	4057.756653	23.536615
121.274709	4061.588682	23.541632
121.654105	4065.283673	23.546650
121.983561	4062.308278	23.551667
121.905766	4047.893338	23.556685
122.150013	4027.093180	23.561703
121.695232	4026.846623	23.566720
121.688112	4025.256846	23.571738
121.867624	4019.242576	23.576755
121.802890	4030.282548	23.581773
122.093409	4043.455121	23.586791
121.526872	4054.574835	23.591808
121.744562	4055.785854	23.596826
122.250179	4056.897105	23.601843
121.937753	4079.820529	23.606861
122.431896	4087.605617	23.611879
122.687538	4088.073714	23.616896
122.329919	4089.138415	23.621914
122.307236	4100.416175	23.626931
122.650423	4120.765971	23.631949
122.891875	4119.231235	23.636967
122.871222	4121.678718	23.641984
122.891806	4139.346883	23.647002
123.231097	4155.689217	23.652019
123.128825	4153.576223	23.657037
123.308881	4159.531214	23.662055
123.525011	4184.853045	23.667072
123.682001	4182.586909	23.672090
123.907653	4175.256436	23.677107
123.721959	4184.105623	23.682125
124.489005	4196.021505	23.687143
124.802689	4197.924935	23.692160
124.990494	4192.780283	23.697178
125.268533	4188.577908	23.702195
125.430253	4189.861542	23.707213
125.880187	4177.507785	23.712231
125.677024	4165.657446	23.717248
125.640029	4166.963330	23.722266
125.652770	4157.345897	23.727283
125.785781	4156.240096	23.732301
125.676338	4156.837731	23.737319
125.522161	4160.619491	23.742336
125.408241	4159.685979	23.747354
125.856446	4175.054284	23.752371
125.400022	4187.835201	23.757389
125.953335	4188.003384	23.762407
126.262052	4197.277409	23.767424
126.291237	4204.154591	23.772442
126.078002	4209.160995	23.777459
126.210103	4207.677290	23.782477
126.377672	4208.733089	23.787495
126.912990	4225.140343	23.792512
126.825855	4229.508430	23.797530
127.759896	4221.856440	23.802547
127.843475	4223.062897	23.807565
127.934516	4213.602919	23.812583
127.830569	4218.021930	23.817600
127.646821	4218.480295	23.822618
128.053560	4212.905082	23.827635
128.122507	4218.694840	23.832653
128.047687	4214.635649	23.837671
128.299798	4218.706139	23.842688
128.256166	4214.079241	23.847706
128.462853	4231.175298	23.852723
128.381978	4247.482643	23.857741
128.754968	4250.674700	23.862759
128.648759	4251.804215	23.867776
128.426129	4252.015632	23.872794
129.052886	4255.720247	23.877811
128.896447	4281.952010	23.882829
129.139946	4278.767627	23.887847
129.027060	4276.902961	23.892864
129.210208	4289.533360	23.897882
129.400002	4299.290955	23.902899
129.286152	4310.557714	23.907917
129.559303	4304.977016	23.912935
129.973652	4322.414056	23.917952
129.688960	4337.032322	23.922970
130.021250	4336.661857	23.927987
130.253252	4349.142156	23.933005
130.544199	4357.530879	23.938023
130.281390	4368.412075	23.943040
130.339429	4374.901598	23.948058
130.787435	4371.245005	23.953075
130.680246	4393.364185	23.958093
130.774202	4397.876915	23.963111
130.910218	4397.981168	23.968128
131.015818	4402.440707	23.973146
131.470336	4420.257694	23.978163
131.137572	4426.646470	23.983181
131.372548	4428.546094	23.988199
131.614503	4433.781711	23.993216
131.957313	4459.369751	23.998234
132.393297	4463.701782	24.003251
131.956932	4465.570000	24.008269
131.813474	4467.332084	24.013287
132.696156	4476.619721	24.018304
132.213640	4488.613781	24.023322
132.928885	4493.053898	24.028339
132.992785	4490.503589	24.033357
133.009578	4490.896077	24.038375
133.419172	4502.919155	24.043392
133.387859	4518.477906	24.048410
133.737282	4514.864172	24.053427
133.693643	4519.039001	24.058445
133.732586	4530.640459	24.063463
133.931197	4520.330903	24.068480
133.937908	4522.086939	24.073498
134.094676	4533.763505	24.078515
134.234030	4552.799584	24.083533
134.003604	4552.659479	24.088551
134.416732	4556.295246	24.093568
134.042551	4575.699787	24.098586
134.620281	4580.488798	24.103603
134.504955	4589.030782	24.108621
134.623055	4591.821590	24.113639
134.880016	4597.994341	24.118656
134.741854	4619.230690	24.123674
135.192102	4618.270534	24.128691
135.237391	4635.606572	24.133709
135.656580	4646.211938	24.138727
136.063072	4653.351504	24.143744
135.937162	4651.227530	24.148762
136.199165	4656.318009	24.153779
135.928556	4678.843670	24.158797
136.027779	4678.579314	24.163815
136.851126	4669.232969	24.168832
136.389531	4673.494454	24.173850
136.698280	4688.665052	24.178867
136.984970	4696.007121	24.183885
136.989325	4699.095485	24.188903
137.528952	4699.112434	24.193920
137.182294	4701.430797	24.198938
137.490937	4699.175610	24.203955
137.559118	4715.086902	24.208973
137.622650	4718.213959	24.213991
138.251992	4713.575516	24.219008
138.179892	4721.378440	24.224026
138.578049	4716.852091	24.229043
138.603855	4713.342625	24.234061
138.219375	4718.598299	24.239079
138.790272	4710.097029	24.244096
138.657454	4709.321889	24.249114
138.763627	4727.949566	24.254131
139.059853	4744.673238	24.259149
138.896677	4753.438541	24.264167
139.318293	4745.829255	24.269184
139.069699	4745.064509	24.274202
139.494792	4748.978672	24.279219
139.325082	4757.248880	24.284237
139.292164	4770.122279	24.289255
139.488371	4773.537724	24.294272
139.312157	4787.825900	24.299290
139.718246	4799.107841	24.304307
139.676705	4806.817352	24.309325
139.725551	4830.119432	24.314343
140.096993	4829.298799	24.319360
139.992851	4845.354760	24.324378
140.130609	4865.855730	24.329395
140.419599	4876.118889	24.334413
140.746457	4894.243427	24.339431
141.059168	4897.987857	24.344448
141.032928	4911.135116	24.349466
141.135594	4914.293311	24.354483
141.616466	4929.800105	24.359501
141.412163	4931.797939	24.364519
142.002183	4945.186937	24.369536
142.303672	4945.789770	24.374554
142.403224	4941.994294	24.379571
142.558834	4951.760515	24.384589
142.763162	4948.314912	24.389607
143.264461	4943.271445	24.394624
143.090914	4952.393868	24.399642
143.147952	4939.939106	24.404659
143.306123	4934.633100	24.409677
143.126491	4947.218307	24.414695
143.278837	4968.488025	24.419712
143.204235	4981.197032	24.424730
143.268343	4979.777685	24.429747
143.629683	4991.717253	24.434765
143.779866	5006.669591	24.439783
143.858779	5006.004644	24.444800
143.937002	5015.177673	24.449818
144.019409	5031.605123	24.454835
144.277439	5035.539334	24.459853
144.014288	5045.147403	24.464871
144.591629	5058.092855	24.469888
144.756037	5080.276705	24.474906
145.172045	5074.950870	24.479923
145.282000	5079.380710	24.484941
144.970889	5081.062116	24.489959
146.210593	5085.507017	24.494976
147.133724	5064.323679	24.499994
146.944278	5044.281015	24.505011
147.294074	5031.990237	24.510029
147.229137	5023.176405	24.515047
147.309848	5010.994785	24.520064
147.130692	5007.181697	24.525082
147.103775	4998.168384	24.530099
147.389960	4997.828653	24.535117
147.429355	4994.357753	24.540135
147.423547	4978.147154	24.545152
147.287130	4973.219302	24.550170
147.059241	4991.756477	24.555187
147.507292	4988.738529	24.560205
147.539709	4992.963457	24.565223
147.823599	4988.905586	24.570240
147.571536	4997.056134	24.575258
147.688331	4996.082233	24.580275
148.075203	5018.601211	24.585293
147.651844	5029.964859	24.590311
147.993749	5027.072222	24.595328
147.237382	5045.851287	24.600346
147.893494	5064.829326	24.605363
148.085982	5086.206532	24.610381
148.044825	5102.126716	24.615399
148.626514	5125.296140	24.620416
148.442392	5129.964660	24.625434
148.998594	5149.856290	24.630451
149.073379	5161.206314	24.635469
148.989800	5171.362610	24.640487
149.455722	5178.852980	24.645504
149.826841	5188.149973	24.650522
149.905912	5195.084410	24.655539
149.985681	5199.842403	24.660557
150.471369	5214.166362	24.665575
150.362520	5216.078553	24.670592
150.063153	5234.012306	24.675610
150.511228	5243.762440	24.680627
150.672100	5254.043082	24.685645
150.513453	5264.404498	24.690663
151.059452	5275.140570	24.695680
150.833560	5282.488078	24.700698
150.997378	5303.496347	24.705715
151.516632	5313.341446	24.710733
151.700622	5321.058228	24.715751
151.843623	5333.791652	24.720768
151.902141	5344.364009	24.725786
152.074143	5344.659808	24.730803
152.172231	5365.797578	24.735821
152.388037	5378.078246	24.740839
152.534414	5375.943728	24.745856
152.722428	5386.198536	24.750874
152.803657	5402.818765	24.755891
153.357788	5407.801121	24.760909
153.200869	5411.863273	24.765927
153.379697	5424.205453	24.770944
153.649429	5440.653988	24.775962
153.811113	5439.314758	24.780979
154.060344	5441.571246	24.785997
153.482347	5445.908812	24.791015
154.512745	5455.592334	24.796032
154.515071	5458.396842	24.801050
154.228203	5471.774348	24.806067
154.917481	5459.252544	24.811085
154.580863	5469.171206	24.816103
154.732122	5484.588541	24.821120
154.790272	5500.518094	24.826138
154.984295	5496.874856	24.831155
155.379751	5498.420214	24.836173
154.748851	5524.699129	24.841191
155.395600	5529.603420	24.846208
155.554885	5545.973325	24.851226
156.023749	5567.265203	24.856243
156.330237	5557.932119	24.861261
156.316548	5560.697643	24.866279
156.761141	5573.510314	24.871296
156.880573	5581.183940	24.876314
156.898985	5584.082597	24.881331
157.086910	5585.526483	24.886349
157.036047	5588.325165	24.891367
157.729021	5591.648540	24.896384
158.028949	5602.654661	24.901402
157.672699	5619.282370	24.906419
158.422117	5624.242347	24.911437
158.205009	5624.982945	24.916455
158.270798	5615.587903	24.921472
158.582472	5617.913269	24.926490
158.305594	5616.623999	24.931507
158.821666	5608.456971	24.936525
158.712163	5632.779861	24.941543
158.891872	5641.876779	24.946560
159.174666	5651.981603	24.951578
159.093627	5651.727655	24.956595
159.365028	5649.349540	24.961613
159.083985	5663.005051	24.966631
159.053754	5676.920051	24.971648
159.274569	5684.503091	24.976666
159.481008	5691.162274	24.981683
160.005833	5691.327492	24.986701
159.958979	5711.876957	24.991719
160.328791	5718.872059	24.996736
160.630528	5728.104859	25.001754
160.438425	5735.091531	25.006771
160.979917	5749.188218	25.011789
160.949097	5751.840920	25.016807
161.496033	5760.729230	25.021824
161.333479	5749.170067	25.026842
161.122063	5777.102539	25.031859
161.743499	5780.257837	25.036877
161.516054	5784.981235	25.041895
161.856182	5805.612569	25.046912
162.348574	5804.395425	25.051930
162.391162	5811.125282	25.056947
162.566388	5809.110219	25.061965
162.684836	5806.606275	25.066983
162.959570	5811.502748	25.072000
163.047510	5829.476327	25.077018
163.035117	5841.470365	25.082035
162.981983	5838.913122	25.087053
163.061040	5847.798191	25.092071
163.235577	5853.704355	25.097088
163.604353	5871.234413	25.102106
163.483248	5888.824050	25.107123
164.057580	5894.597891	25.112141
164.198910	5905.402188	25.117159
164.427936	5909.829967	25.122176
164.303322	5911.147075	25.127194
164.456867	5922.154881	25.132211
165.165797	5917.980591	25.137229
164.981065	5924.026352	25.142247
165.387510	5929.906181	25.147264
165.974367	5933.024114	25.152282
165.808457	5948.131563	25.157299
165.849344	5950.883860	25.162317
166.281215	5960.141749	25.167335
166.009551	5953.652700	25.172352
165.903232	5956.192345	25.177370
166.161822	5970.684316	25.182387
166.672511	5978.225684	25.187405
166.182783	5984.210321	25.192423
166.003170	5996.251258	25.197440
166.894473	6012.901041	25.202458
166.796880	6026.526989	25.207475
166.673052	6033.685623	25.212493
166.907017	6057.663556	25.217511
167.149447	6072.814554	25.222528
167.425168	6090.619175	25.227546
167.440232	6104.989958	25.232563
168.004773	6108.506397	25.237581
168.257618	6114.436257	25.242599
168.499699	6137.794564	25.247616
168.962250	6146.157973	25.252634
168.907374	6144.476919	25.257651
169.241443	6142.648055	25.262669
169.431854	6147.861570	25.267687
169.216704	6147.053208	25.272704
169.602563	6159.510923	25.277722
170.004564	6180.778064	25.282739
170.264158	6170.728752	25.287757
170.645142	6173.626018	25.292775
170.554885	6172.136139	25.297792
170.754144	6172.742369	25.302810
170.677440	6167.510090	25.307827
170.547340	6180.648631	25.312845
170.680786	6199.730234	25.317863
171.130955	6197.915334	25.322880
171.591537	6192.640570	25.327898
171.557726	6196.143806	25.332915
171.762260	6200.434863	25.337933
171.373062	6228.238693	25.342951
171.378027	6232.643529	25.347968
171.833392	6229.676877	25.352986
171.992833	6249.353537	25.358003
172.326526	6248.422728	25.363021
172.692892	6255.882627	25.368039
172.353989	6251.619263	25.373056
172.894746	6254.094508	25.378074
172.932728	6276.122886	25.383091
173.289320	6276.483164	25.388109
173.396652	6273.561986	25.393127
173.332127	6279.142212	25.398144
173.739607	6297.717714	25.403162
173.507817	6309.478737	25.408179
173.691302	6307.603199	25.413197
173.800228	6331.532083	25.418215
173.849357	6338.112950	25.423232
174.184376	6355.329513	25.428250
174.180498	6378.571215	25.433267
174.531124	6380.297648	25.438285
174.782261	6411.380828	25.443303
175.158125	6424.929105	25.448320
175.245484	6423.162983	25.453338
175.156933	6449.312631	25.458355
175.175939	6449.715816	25.463373
175.581474	6453.973274	25.468391
175.838857	6468.877889	25.473408
176.260295	6479.110719	25.478426
176.309666	6502.437214	25.483443
176.677861	6506.659337	25.488461
176.772632	6499.742528	25.493479
177.428589	6515.613156	25.498496
177.753971	6518.015868	25.503514
177.852372	6526.869642	25.508531
177.786565	6525.913560	25.513549
178.183162	6532.687805	25.518567
177.718237	6537.666396	25.523584
177.995459	6527.155378	25.528602
177.456562	6544.893764	25.533619
178.020832	6556.549228	25.538637
178.616479	6572.164784	25.543655
178.800949	6588.795336	25.548672
179.097677	6584.238591	25.553690
179.285986	6598.410757	25.558707
179.371364	6591.814553	25.563725
179.468084	6612.813207	25.568743
179.561221	6622.128763	25.573760
180.197969	6610.664340	25.578778
180.158057	6614.293175	25.583795
180.492560	6623.514578	25.588813
180.648844	6629.276853	25.593831
180.727092	6641.960193	25.598848
181.063355	6629.804428	25.603866
181.039637	6631.288629	25.608883
181.084026	6629.858338	25.613901
181.346080	6635.779726	25.618919
181.250492	6658.672046	25.623936
181.491295	6654.729065	25.628954
181.862323	6667.151122	25.633971
181.729892	6667.977293	25.638989
181.992818	6674.336530	25.644007
181.833311	6694.756112	25.649024
181.867214	6698.498351	25.654042
181.932946	6718.150691	25.659059
182.722682	6732.079661	25.664077
183.038896	6745.189423	25.669095
182.546917	6756.431349	25.674112
183.225943	6768.732154	25.679130
182.854232	6775.281359	25.684148
183.013185	6797.793877	25.689165
183.502133	6812.764677	25.694183
183.220396	6839.247422	25.699200
183.411855	6852.653582	25.704218
183.739949	6866.638172	25.709236
184.058496	6887.732292	25.714253
184.969312	6877.520490	25.719271
185.767761	6868.512732	25.724288
186.242695	6861.544780	25.729306
186.061998	6868.800188	25.734324
186.106926	6857.121153	25.739341
186.602811	6859.994912	25.744359
186.358069	6861.605251	25.749376
186.686119	6858.552389	25.754394
186.358650	6858.193354	25.759412
186.686050	6883.314505	25.764429
186.804476	6885.988289	25.769447
186.984458	6895.997306	25.774464
187.232844	6890.334093	25.779482
187.029807	6897.848575	25.784500
187.417348	6911.019508	25.789517
188.167243	6910.179595	25.794535
188.059604	6913.100102	25.799552
188.447429	6902.653381	25.804570
189.029732	6895.358998	25.809588
189.754950	6887.453245	25.814605
189.769024	6876.778352	25.819623
189.682344	6885.368645	25.824640
189.910998	6879.697002	25.829658
189.978441	6873.890719	25.834676
189.966692	6874.192841	25.839693
190.167059	6870.274857	25.844711
190.485284	6869.642072	25.849728
190.255590	6858.681274	25.854746
190.401852	6875.164277	25.859764
190.296144	6882.833010	25.864781
190.964548	6870.328660	25.869799
190.578624	6874.714814	25.874816
190.888975	6861.063438	25.879834
191.093634	6874.955761	25.884852
190.739904	6897.899764	25.889869
191.181978	6902.834062	25.894887
190.988465	6915.584687	25.899904
190.942792	6926.659635	25.904922
191.070502	6948.059111	25.909940
191.244208	6970.944317	25.914957
191.427534	6979.893282	25.919975
191.255185	7001.842916	25.924992
191.587150	7021.981728	25.930010
191.578494	7045.587588	25.935028
192.167692	7063.209582	25.940045
192.946505	7071.048188	25.945063
192.869334	7090.180351	25.950080
193.398201	7099.893363	25.955098
193.376484	7115.616858	25.960116
193.625676	7124.739738	25.965133
193.889690	7147.874404	25.970151
194.548448	7160.244374	25.975168
194.243069	7152.304035	25.980186
194.297711	7163.336742	25.985204
194.684872	7183.507260	25.990221
194.960870	7190.726279	25.995239
194.934027	7217.095844	26.000256
195.073187	7219.393515	26.005274
195.431321	7228.044026	26.010292
195.065876	7245.692792	26.015309
195.629656	7263.618717	26.020327
195.825604	7287.200101	26.025344
196.214366	7293.274900	26.030362
196.488120	7307.417294	26.035380
196.128835	7326.283776	26.040397
196.629555	7332.914473	26.045415
197.055882	7352.452998	26.050432
197.270110	7358.419092	26.055450
197.566460	7392.070090	26.060468
197.730038	7394.642474	26.065485
197.965456	7393.775717	26.070503
197.818011	7416.689825	26.075520
198.239171	7421.670411	26.080538
198.416035	7434.823534	26.085556
198.397865	7450.131589	26.090573
198.460116	7458.434328	26.095591
198.738253	7484.335317	26.100608
198.926007	7495.066560	26.105626
199.217626	7512.537601	26.110644
199.282825	7534.449605	26.115661
199.779809	7546.595516	26.120679
199.931066	7554.882260	26.125696
200.403451	7560.953856	26.130714
201.078654	7571.960036	26.135732
200.946229	7579.151557	26.140749
201.224231	7567.673902	26.145767
201.205145	7586.609206	26.150784
201.278286	7597.289264	26.155802
201.786158	7599.023543	26.160820
201.519839	7610.259679	26.165837
201.748324	7607.908333	26.170855
202.059060	7633.852030	26.175872
202.218327	7637.845575	26.180890
202.411025	7641.251215	26.185908
202.197234	7670.951253	26.190925
202.791661	7677.669232	26.195943
202.728332	7687.978848	26.200960
202.825902	7704.834222	26.205978
202.668594	7715.654698	26.210996
203.094608	7742.090875	26.216013
203.343966	7751.785236	26.221031
203.537224	7772.739715	26.226048
204.080478	7782.300209	26.231066
204.203145	7791.203306	26.236084
204.200931	7807.607941	26.241101
205.147775	7814.954892	26.246119
205.215346	7822.878765	26.251136
205.530261	7821.067970	26.256154
205.638029	7832.551316	26.261172
205.612827	7854.034147	26.266189
205.946611	7852.905499	26.271207
206.120065	7869.320263	26.276224
206.042151	7887.490023	26.281242
206.990771	7890.081541	26.286260
206.753770	7896.554535	26.291277
207.404279	7920.541066	26.296295
207.234973	7925.540307	26.301312
207.370964	7922.097121	26.306330
207.625129	7923.077670	26.311348
207.597438	7945.132206	26.316365
207.775384	7946.904960	26.321383
207.905821	7974.113027	26.326400
207.724233	7980.283492	26.331418
208.237980	7999.221695	26.336436
208.316414	8024.601598	26.341453
208.638151	8041.414172	26.346471
208.816319	8057.888982	26.351488
208.682213	8074.177056	26.356506
208.912998	8088.671778	26.361524
209.323022	8111.045415	26.366541
209.669392	8129.570502	26.371559
209.840015	8145.800897	26.376576
209.891513	8158.726367	26.381594
210.497713	8182.041789	26.386612
210.696622	8192.688079	26.391629
210.658034	8219.735671	26.396647
211.011236	8234.311957	26.401664
211.309857	8250.006073	26.406682
211.715358	8265.644855	26.411700
211.585471	8265.299970	26.416717
212.039348	8281.867981	26.421735
212.408365	8295.521439	26.426752
212.188787	8307.258979	26.431770
212.910018	8322.822426	26.436788
213.159701	8325.647273	26.441805
213.977099	8301.247750	26.446823
214.276875	8294.403748	26.451840
214.410667	8302.939673	26.456858
214.760299	8294.943210	26.461876
214.334850	8293.866682	26.466893
215.023107	8295.576424	26.471911
215.019923	8300.013950	26.476928
214.998035	8294.239012	26.481946
215.137668	8300.644456	26.486964
215.562376	8306.232911	26.491981
215.807683	8306.896724	26.496999
216.141456	8309.655158	26.502016
216.243574	8314.514243	26.507034
216.477298	8302.013974	26.512052
216.147729	8308.109877	26.517069
216.428922	8316.310141	26.522087
216.841146	8329.301542	26.527104
216.499649	8340.670033	26.532122
216.880172	8349.062848	26.537140
217.110426	8362.298180	26.542157
217.176419	8369.742809	26.547175
217.803177	8400.822188	26.552192
217.607530	8411.962470	26.557210
217.861011	8409.524791	26.562228
217.741172	8430.102067	26.567245
217.986474	8448.375410	26.572263
218.105479	8459.803706	26.577280
218.093625	8494.333913	26.582298
218.609878	8501.365019	26.587316
218.827436	8526.001787	26.592333
219.282914	8540.815291	26.597351
219.527701	8554.752613	26.602368
219.578685	8571.341139	26.607386
220.358989	8584.954282	26.612404
220.287885	8598.716529	26.617421
220.466823	8610.363919	26.622439
220.608952	8634.590715	26.627456
220.572747	8641.228122	26.632474
220.975235	8658.749161	26.637492
221.245005	8691.307615	26.642509
221.667278	8704.929445	26.647527
221.945915	8717.176703	26.652544
221.723304	8737.969736	26.657562
221.871047	8748.413235	26.662580
222.038700	8777.162815	26.667597
221.730658	8787.098310	26.672615
221.815232	8808.785768	26.677632
222.222552	8844.265131	26.682650
223.103339	8867.385580	26.687668
223.893854	8872.111077	26.692685
224.632832	8875.899991	26.697703
224.879334	8875.733232	26.702720
224.847397	8885.342562	26.707738
225.535520	8878.682284	26.712756
225.526943	8883.771659	26.717773
225.405510	8884.999433	26.722791
225.746784	8878.981618	26.727808
225.735088	8888.637903	26.732826
225.901807	8879.933503	26.737844
225.923503	8914.666063	26.742861
226.456732	8918.409894	26.747879
226.062078	8924.701540	26.752896
226.508030	8938.779616	26.757914
226.712249	8943.808898	26.762932
226.774187	8956.123420	26.767949
227.090978	8969.448416	26.772967
227.307153	8975.241452	26.777984
227.476079	8992.792649	26.783002
227.767311	8996.689855	26.788020
228.320635	9017.350244	26.793037
228.635595	9031.691938	26.798055
229.223319	9032.872226	26.803072
228.898507	9039.720777	26.808090
229.356087	9034.912025	26.813108
229.593958	9055.352361	26.818125
229.378328	9054.673921	26.823143
230.128199	9067.431565	26.828160
230.595123	9073.588191	26.833178
231.398980	9060.231691	26.838196
231.767292	9058.860689	26.843213
232.132568	9065.929743	26.848231
232.260822	9040.801863	26.853248
232.348488	9026.137405	26.858266
232.611008	9016.756287	26.863284
232.407247	9017.927276	26.868301
231.974747	9016.748694	26.873319
232.289515	9033.951917	26.878336
232.021372	9048.362062	26.883354
232.325611	9056.721054	26.888372
232.333284	9071.906467	26.893389
232.347624	9096.828693	26.898407
232.551064	9117.128468	26.903424
232.884744	9145.995213	26.908442
233.174789	9150.105384	26.913460
233.555025	9178.669547	26.918477
233.798198	9192.686485	26.923495
234.370242	9214.289357	26.928512
234.472243	9232.462094	26.933530
234.489663	9251.278068	26.938548
234.912532	9255.887066	26.943565
235.531451	9281.988596	26.948583
235.413773	9285.516334	26.953600
235.321483	9303.531790	26.958618
235.884141	9316.807051	26.963636
235.943390	9326.002350	26.968653
235.825672	9351.027966	26.973671
236.365914	9361.792219	26.978688
236.222363	9387.720495	26.983706
236.293523	9406.226470	26.988724
236.857085	9428.056414	26.993741
237.163656	9454.334670	26.998759
237.746469	9455.000562	27.003776
237.518417	9484.967955	27.008794
238.046009	9490.109010	27.013812
237.751882	9500.356131	27.018829
238.293633	9522.443639	27.023847
239.084732	9529.591181	27.028864
239.333272	9539.488460	27.033882
239.897797	9528.515762	27.038900
240.095078	9543.283054	27.043917
240.288732	9557.945406	27.048935
241.100083	9557.142912	27.053952
240.839086	9561.503642	27.058970
240.994214	9563.505036	27.063988
241.502058	9562.103774	27.069005
241.210078	9596.128894	27.074023
241.389894	9599.282674	27.079040
241.680832	9608.301328	27.084058
241.912603	9618.173167	27.089076
242.069644	9630.235536	27.094093
242.318398	9644.934220	27.099111
242.815340	9661.337909	27.104128
242.692048	9674.483646	27.109146
242.997338	9688.640067	27.114164
242.919044	9695.525426	27.119181
242.995561	9733.759606	27.124199
243.373993	9741.093009	27.129216
243.943332	9772.444884	27.134234
243.753511	9782.073929	27.139252
243.914288	9802.878250	27.144269
243.775696	9831.844506	27.149287
244.220125	9844.623609	27.154304
243.907480	9884.992289	27.159322
244.414507	9911.403963	27.164340
245.066230	9931.534949	27.169357
245.124739	9959.457559	27.174375
245.519214	9982.489634	27.179392
245.753428	10010.587070	27.184410
245.897672	10036.605723	27.189428
246.800927	10056.753632	27.194445
246.356374	10086.418868	27.199463
246.882983	10095.972572	27.204480
247.069577	10118.944349	27.209498
247.392467	10140.848027	27.214516
247.758327	10156.045547	27.219533
248.068028	10178.893878	27.224551
248.548932	10196.424423	27.229568
249.014841	10203.235628	27.234586
249.654583	10197.229204	27.239604
249.783844	10216.833951	27.244621
249.843930	10239.329621	27.249639
250.192565	10236.313580	27.254656
250.336543	10261.300470	27.259674
250.504779	10262.814348	27.264692
251.146875	10271.008904	27.269709
250.987688	10281.091561	27.274727
251.255912	10286.951789	27.279744
251.387538	10311.775412	27.284762
251.474519	10314.322789	27.289780
251.998445	10325.404077	27.294797
251.953178	10340.163244	27.299815
252.327580	10345.953291	27.304832
252.343077	10377.287809	27.309850
252.339405	10383.104853	27.314868
252.701429	10398.531756	27.319885
252.835054	10419.368312	27.324903
253.469399	10439.800746	27.329920
253.718012	10450.420311	27.334938
253.899598	10471.393690	27.339956
254.225712	10478.351890	27.344973
254.261582	10510.018828	27.349991
254.553164	10522.258935	27.355008
255.036868	10546.935897	27.360026
255.893484	10551.901135	27.365044
255.763601	10566.058849	27.370061
255.543939	10580.559743	27.375079
255.932620	10583.769316	27.380096
256.750459	10579.969954	27.385114
257.209695	10570.686598	27.390132
257.582020	10586.362477	27.395149
257.512683	10610.548109	27.400167
257.814458	10610.070874	27.405184
257.861645	10614.193107	27.410202
258.127725	10634.359554	27.415220
258.437296	10644.793876	27.420237
258.433253	10661.733576	27.425255
258.741095	10669.509716	27.430272
258.868509	10691.124590	27.435290
259.237188	10708.329810	27.440308
259.519963	10720.484903	27.445325
259.455550	10747.928809	27.450343
259.627721	10747.974915	27.455360
259.904821	10779.290581	27.460378
260.120429	10794.489241	27.465396
260.292872	10816.364463	27.470413
260.640645	10837.729017	27.475431
260.483636	10864.019680	27.480448
261.073867	10888.291234	27.485466
261.329563	10913.479028	27.490484
261.977857	10921.466412	27.495501
262.151429	10950.275567	27.500519
262.008717	10964.022939	27.505536
262.595125	10991.696097	27.510554
262.257175	11008.113457	27.515572
262.937073	11028.866616	27.520589
263.274473	11052.195234	27.525607
263.379288	11068.853521	27.530624
263.719068	11096.898496	27.535642
264.398593	11098.384702	27.540660
264.641197	11105.812926	27.545677
265.155260	11116.699459	27.550695
265.618913	11122.041112	27.555712
265.595256	11128.695508	27.560730
265.622953	11149.549579	27.565748
266.596730	11148.779070	27.570765
266.654668	11159.018890	27.575783
266.767906	11175.400057	27.580800
266.932954	11187.849890	27.585818
266.716540	11193.087502	27.590836
267.226896	11200.160995	27.595853
267.322180	11218.463182	27.600871
267.581042	11230.227198	27.605888
267.724239	11255.622340	27.610906
267.673896	11288.148689	27.615924
268.134779	11299.137441	27.620941
267.803665	11326.142645	27.625959
268.156003	11357.738076	27.630976
268.478558	11397.333428	27.635994
268.799957	11412.760379	27.641012
269.708498	11423.968764	27.646029
270.204181	11451.847370	27.651047
271.670504	11413.251677	27.656064
272.610040	11401.204849	27.661082
272.620147	11413.668804	27.666100
272.812871	11399.876183	27.671117
272.789604	11402.737330	27.676135
273.171490	11404.941207	27.681152
273.256081	11411.605531	27.686170
273.237670	11417.671319	27.691188
273.583542	11403.553016	27.696205
273.602485	11410.950374	27.701223
273.532393	11410.987577	27.706240
273.929258	11419.941810	27.711258
273.239867	11440.575607	27.716276
273.748981	11452.440303	27.721293
273.987255	11466.768935	27.726311
274.350462	11501.278290	27.731328
274.285202	11516.237366	27.736346
274.451895	11554.851206	27.741364
274.700659	11570.090611	27.746381
274.818951	11594.825495	27.751399
274.809169	11623.342619	27.756416
275.800320	11640.815640	27.761434
275.630121	11670.589594	27.766452
276.059129	11694.700872	27.771469
276.003417	11725.276384	27.776487
276.397421	11745.296205	27.781504
277.035718	11776.521936	27.786522
277.276940	11812.795890	27.791540
277.980219	11826.383225	27.796557
278.319380	11848.850619	27.801575
278.760586	11856.412201	27.806592
278.933310	11876.613525	27.811610
279.163781	11902.937156	27.816628
279.446515	11909.285620	27.821645
279.583975	11928.988735	27.826663
279.660147	11938.173156	27.831680
280.149952	11945.398643	27.836698
281.905177	11914.088520	27.841716
282.785345	11906.141203	27.846733
282.973157	11906.369025	27.851751
283.137567	11894.845541	27.856768
283.284141	11874.978685	27.861786
283.182345	11880.958073	27.866804
283.251388	11862.218745	27.871821
283.449243	11862.433813	27.876839
283.467608	11866.228770	27.881856
283.489971	11874.527217	27.886874
283.557635	11900.606105	27.891892
283.949048	11893.532137	27.896909
283.687926	11912.386323	27.901927
283.863558	11937.312050	27.906944
284.280379	11947.594870	27.911962
284.006032	11978.643305	27.916980
284.408067	12005.728848	27.921997
284.577244	12034.674633	27.927015
284.508415	12059.997047	27.932032
284.950817	12084.174375	27.937050
284.881518	12127.173496	27.942068
285.553353	12151.322631	27.947085
285.747306	12182.579597	27.952103
286.180011	12221.775098	27.957120
286.443871	12238.813933	27.962138
287.134488	12275.645451	27.967156
287.186107	12294.831024	27.972173
287.709274	12327.237501	27.977191
287.922630	12359.027329	27.982208
288.508597	12372.466594	27.987226
288.910529	12395.403097	27.992244
289.113893	12417.048217	27.997261
289.477136	12424.349196	28.002279
289.910910	12450.736579	28.007296
290.536197	12455.182573	28.012314
290.583235	12479.070487	28.017332
290.901261	12488.949778	28.022349
291.440009	12504.649418	28.027367
291.844514	12520.498165	28.032384
292.080765	12521.928102	28.037402
291.870248	12548.752315	28.042420
292.262078	12566.842852	28.047437
292.486695	12578.539638	28.052455
292.514039	12603.460274	28.057472
292.594079	12624.398666	28.062490
292.796476	12638.074107	28.067508
293.195369	12648.987716	28.072525
293.320696	12686.131392	28.077543
293.963397	12714.305324	28.082560
294.323736	12723.461970	28.087578
294.499585	12745.676473	28.092596
295.382938	12762.450493	28.097613
295.260141	12774.791688	28.102631
295.059785	12794.695592	28.107648
295.509767	12819.276184	28.112666
295.870604	12832.004201	28.117684
296.815294	12853.481859	28.122701
297.378393	12862.725189	28.127719
297.506281	12874.869037	28.132736
298.378590	12865.828811	28.137754
298.679396	12880.694869	28.142772
298.703155	12882.881530	28.147789
298.796161	12874.576932	28.152807
298.733882	12899.891639	28.157824
299.092129	12905.031300	28.162842
299.064095	12922.313160	28.167860
299.647071	12939.862272	28.172877
300.008439	12965.082403	28.177895
299.960644	12987.177956	28.182912
300.133890	12997.821558	28.187930
300.181968	13031.341626	28.192948
300.558328	13056.256717	28.197965
300.778886	13080.043264	28.202983
300.443233	13098.470274	28.208000
300.828663	13137.171714	28.213018
300.997768	13173.937028	28.218036
301.302616	13201.093219	28.223053
302.191111	13231.738244	28.228071
302.344848	13261.541521	28.233088
302.884672	13293.594005	28.238106
302.804065	13324.269754	28.243124
303.222322	13349.253762	28.248141
303.920241	13368.567813	28.253159
304.099998	13396.562204	28.258176
304.515297	13419.311867	28.263194
304.925287	13458.429107	28.268212
305.402295	13475.393293	28.273229
305.851936	13497.812494	28.278247
305.906331	13525.286396	28.283264
306.423235	13529.182277	28.288282
307.035126	13550.177274	28.293300
307.114313	13568.579415	28.298317
307.657090	13585.456788	28.303335
307.871693	13600.834762	28.308352
308.390775	13616.326060	28.313370
308.596281	13620.358871	28.318388
308.664574	13645.344993	28.323405
308.599137	13652.231387	28.328423
308.956695	13685.977149	28.333440
309.365904	13695.885674	28.338458
309.586690	13721.584997	28.343476
309.655407	13740.167230	28.348493
310.161104	13760.580179	28.353511
310.842117	13784.425954	28.358528
311.192429	13786.901948	28.363546
311.599672	13789.393404	28.368564
312.245253	13788.021793	28.373581
312.571315	13804.356504	28.378599
312.689264	13821.013764	28.383616
313.003814	13811.896823	28.388634
313.123712	13830.722575	28.393652
313.434945	13845.198404	28.398669
313.623266	13855.272556	28.403687
313.639008	13884.974518	28.408704
313.819466	13895.277011	28.413722
314.099473	13923.773681	28.418740
313.952384	13948.893325	28.423757
314.643263	13966.456569	28.428775
314.503670	14006.307662	28.433792
314.999527	14028.207403	28.438810
314.907597	14055.224951	28.443828
315.371845	14094.447890	28.448845
316.324394	14117.632892	28.453863
316.302898	14144.534485	28.458880
316.870768	14171.458054	28.463898
316.512843	14194.131678	28.468916
317.239588	14228.117907	28.473933
317.706858	14246.605607	28.478951
318.186041	14279.698101	28.483968
318.724779	14305.473090	28.488986
318.923495	14334.860781	28.494004
319.293648	14350.679357	28.499021
319.891479	14365.837894	28.504039
319.741769	14391.719977	28.509056
320.319361	14409.854792	28.514074
320.750784	14436.728098	28.519092
321.016540	14460.906105	28.524109
321.263257	14477.114798	28.529127
321.258504	14506.019083	28.534144
322.004631	14529.240046	28.539162
322.277636	14540.996140	28.544180
322.346301	14559.825199	28.549197
323.361375	14563.571324	28.554215
324.139820	14569.694003	28.559232
324.474682	14582.334832	28.564250
324.786017	14602.131148	28.569268
324.993669	14606.945654	28.574285
325.388333	14607.577842	28.579303
325.601103	14627.208236	28.584320
325.466773	14637.625042	28.589338
325.778820	14650.581933	28.594356
326.050712	14671.877805	28.599373
326.216936	14691.282966	28.604391
326.151779	14723.668906	28.609408
326.618269	14745.136434	28.614426
326.719880	14771.518272	28.619444
326.996222	14800.961267	28.624461
327.153220	14817.217196	28.629479
326.972224	14851.595153	28.634496
327.670428	14885.035933	28.639514
327.916672	14917.665221	28.644532
328.188152	14946.633272	28.649549
328.610784	14979.336485	28.654567
328.437745	15011.580694	28.659584
328.643882	15039.987915	28.664602
329.505223	15077.904591	28.669620
329.374995	15108.833327	28.674637
330.169632	15135.446906	28.679655
330.788504	15169.050030	28.684672
330.869182	15198.339686	28.689690
331.500110	15231.608270	28.694708
332.194875	15262.607125	28.699725
333.161850	15286.812756	28.704743
332.448795	15305.639500	28.709760
332.982268	15329.058821	28.714778
333.335435	15356.735194	28.719796
333.631775	15388.872893	28.724813
333.593955	15405.128109	28.729831
333.983242	15430.746039	28.734848
334.426643	15465.781195	28.739866
334.581177	15493.947400	28.744884
334.593629	15529.281965	28.749901
335.179632	15559.724653	28.754919
335.364938	15609.303533	28.759936
335.289594	15635.989780	28.764954
335.975242	15674.262662	28.769972
336.189509	15721.582730	28.774989
336.792587	15754.018516	28.780007
337.198665	15799.832037	28.785024
337.955122	15825.602035	28.790042
338.298019	15850.605899	28.795060
338.320763	15884.435599	28.800077
339.033126	15908.665286	28.805095
339.606986	15935.759376	28.810112
339.979593	15954.014568	28.815130
340.652060	15969.224845	28.820148
341.240232	15988.731033	28.825165
341.604909	16000.757779	28.830183
341.815088	16020.666133	28.835200
341.787125	16040.394631	28.840218
342.325648	16058.129670	28.845236
342.166584	16085.991208	28.850253
342.418328	16107.438981	28.855271
342.415087	16135.976968	28.860288
342.854273	16168.150018	28.865306
343.044482	16195.105352	28.870324
343.258694	16238.523732	28.875341
343.931442	16262.133317	28.880359
344.058838	16295.731524	28.885376
344.534750	16324.294909	28.890394
344.792900	16357.016415	28.895412
345.640592	16392.050444	28.900429
345.988139	16411.153819	28.905447
346.531094	16437.563552	28.910464
346.683623	16457.740843	28.915482
347.214396	16491.404308	28.920500
347.593697	16522.117499	28.925517
348.133858	16514.505321	28.930535
348.585783	16541.328081	28.935552
348.768722	16542.488487	28.940570
349.183733	16557.363508	28.945588
348.920232	16582.396731	28.950605
349.500248	16605.499320	28.955623
349.970931	16625.519819	28.960640
350.340241	16642.562474	28.965658
350.696427	16662.522242	28.970676
350.709756	16683.404687	28.975693
351.056403	16705.809634	28.980711
351.607717	16725.343500	28.985728
352.078819	16748.581612	28.990746
352.439581	16767.856541	28.995764
352.590754	16791.696573	29.000781
353.042398	16805.354820	29.005799
353.905454	16838.468609	29.010816
353.763330	16855.536074	29.015834
354.051471	16869.255501	29.020852
354.251898	16905.085728	29.025869
354.600550	16931.510629	29.030887
355.023776	16957.495566	29.035904
355.014592	16985.593034	29.040922
355.391916	17019.488808	29.045940
355.576247	17049.290497	29.050957
355.822935	17080.033749	29.055975
356.330531	17118.600591	29.060992
356.578257	17146.811949	29.066010
357.273505	17171.317570	29.071028
357.735989	17208.117219	29.076045
358.116238	17228.786118	29.081063
358.539544	17250.180735	29.086080
359.324514	17283.652470	29.091098
359.331871	17304.940298	29.096116
359.316392	17339.214611	29.101133
359.942605	17362.504245	29.106151
360.600237	17385.745961	29.111168
360.672211	17416.081502	29.116186
360.956353	17438.441391	29.121204
360.786072	17475.908162	29.126221
361.413513	17508.234412	29.131239
362.384594	17536.407590	29.136256
363.110044	17558.580074	29.141274
363.566099	17577.767088	29.146292
364.139524	17597.006530	29.151309
364.581761	17599.669151	29.156327
365.509324	17602.702640	29.161344
365.685105	17610.733306	29.166362
366.088410	17609.305190	29.171380
366.209113	17630.659140	29.176397
366.236017	17633.539565	29.181415
366.590473	17640.961036	29.186432
367.223713	17660.532409	29.191450
367.477406	17666.919609	29.196468
367.903185	17672.115409	29.201485
368.294794	17666.640739	29.206503
368.650983	17689.535676	29.211520
369.081884	17696.263005	29.216538
369.960445	17675.428191	29.221556
370.031841	17678.625766	29.226573
370.752721	17675.107905	29.231591
370.849431	17689.587600	29.236608
370.854293	17709.534734	29.241626
371.140337	17711.907258	29.246644
371.282387	17718.535904	29.251661
371.247749	17730.600806	29.256679
371.448022	17751.968077	29.261696
371.575396	17777.311314	29.266714
372.280325	17807.898545	29.271732
371.715824	17833.726200	29.276749
371.928066	17866.581503	29.281767
372.345818	17902.370316	29.286784
372.316604	17945.927867	29.291802
373.077582	17988.307997	29.296820
372.904636	18030.919234	29.301837
372.935661	18073.030532	29.306855
373.449383	18130.419853	29.311872
374.030930	18171.510019	29.316890
374.685745	18219.119546	29.321908
374.574764	18278.164644	29.326925
375.304260	18307.577166	29.331943
376.206211	18343.422679	29.336960
377.292510	18359.198021	29.341978
377.832925	18387.693973	29.346996
378.648085	18414.632496	29.352013
379.002609	18440.885347	29.357031
379.243657	18465.978380	29.362048
379.486182	18490.916688	29.367066
379.850624	18497.181170	29.372084
380.321550	18534.899882	29.377101
380.551466	18552.684162	29.382119
380.902605	18572.864652	29.387136
381.103556	18596.746020	29.392154
381.704019	18627.152419	29.397172
381.471622	18653.343795	29.402189
382.010316	18687.349303	29.407207
382.767484	18721.322169	29.412224
382.593606	18753.001409	29.417242
382.850281	18775.402475	29.422260
383.225765	18814.429441	29.427277
383.488166	18850.734082	29.432295
384.216704	18884.540329	29.437312
383.914147	18934.564263	29.442330
383.832146	18975.795339	29.447348
384.329027	19014.078274	29.452365
384.901451	19058.163108	29.457383
385.035527	19102.031494	29.462400
385.304638	19161.643639	29.467418
386.153646	19199.485093	29.472436
386.668299	19241.437594	29.477453
387.317579	19271.891976	29.482471
388.320945	19292.533892	29.487488
388.779877	19320.920832	29.492506
388.735133	19339.167683	29.497524
389.431271	19375.181537	29.502541
389.798113	19404.587180	29.507559
390.124690	19421.978981	29.512576
390.094223	19460.708064	29.517594
390.665367	19486.266359	29.522612
391.030633	19512.139054	29.527629
390.825670	19558.878007	29.532647
391.508462	19592.228384	29.537664
391.908319	19630.707516	29.542682
392.690655	19666.811285	29.547700
393.140524	19703.024139	29.552717
393.308407	19736.518230	29.557735
394.085817	19758.957501	29.562752
394.309103	19796.746703	29.567770
394.998270	19814.213947	29.572788
395.678091	19849.848463	29.577805
395.852141	19876.405681	29.582823
396.252393	19899.731259	29.587840
396.550861	19928.345390	29.592858
396.854771	19954.319152	29.597876
397.283783	19988.521102	29.602893
397.798063	20023.566266	29.607911
398.278007	20048.023120	29.612928
398.451782	20077.083021	29.617946
398.617563	20101.119184	29.622964
399.056502	20135.501059	29.627981
398.729618	20171.261472	29.632999
399.392764	20209.766179	29.638016
399.549119	20254.972420	29.643034
400.059970	20291.541897	29.648052
400.971076	20336.784575	29.653069
401.106150	20371.799262	29.658087
402.103250	20406.067111	29.663104
402.458227	20452.051888	29.668122
402.628547	20479.627725	29.673140
403.203450	20506.284376	29.678157
403.284213	20546.400232	29.683175
403.813414	20567.995374	29.688192
404.022561	20605.929139	29.693210
404.497263	20650.848511	29.698228
404.940804	20675.238399	29.703245
405.740371	20702.948018	29.708263
406.466114	20734.574554	29.713280
407.000956	20759.169673	29.718298
407.561182	20777.978242	29.723316
408.412958	20812.923052	29.728333
408.157352	20817.534915	29.733351
408.481447	20841.466156	29.738368
408.679898	20867.908789	29.743386
409.215412	20896.781955	29.748404
409.294895	20921.226703	29.753421
409.211002	20950.896766	29.758439
409.695829	20980.658641	29.763456
410.185224	21021.758926	29.768474
410.229508	21048.926806	29.773492
410.717297	21084.615753	29.778509
410.702216	21125.656094	29.783527
411.169854	21163.531037	29.788544
411.175370	21219.650798	29.793562
411.623820	21258.573130	29.798580
411.967063	21308.597457	29.803597
412.392525	21361.693803	29.808615
413.136883	21402.158405	29.813632
413.066051	21447.912931	29.818650
414.321572	21493.703624	29.823668
414.931530	21529.930791	29.828685
415.398172	21569.014712	29.833703
416.127493	21607.777750	29.838720
416.896517	21639.244018	29.843738
417.256628	21665.811570	29.848756
417.502541	21701.562185	29.853773
417.702255	21733.476265	29.858791
418.080954	21753.023483	29.863808
418.329633	21795.475731	29.868826
418.608645	21828.486554	29.873844
419.187699	21860.471480	29.878861
419.396961	21913.638133	29.883879
419.840064	21957.334782	29.888896
420.295245	21990.101264	29.893914
420.264922	22039.982020	29.898932
421.059598	22080.180993	29.903949
421.458241	22123.658606	29.908967
422.146042	22163.229538	29.913984
422.314198	22208.531981	29.919002
422.619616	22249.275668	29.924020
423.362433	22290.704596	29.929037
423.230702	22331.025068	29.934055
423.871991	22372.367511	29.939072
424.125745	22429.568358	29.944090
424.819453	22475.103148	29.949108
425.289746	22518.629412	29.954125
425.119417	22571.781155	29.959143
425.887071	22615.960048	29.964160
426.551291	22661.336380	29.969178
426.790435	22716.175182	29.974196
427.528513	22748.957719	29.979213
427.853632	22794.783614	29.984231
428.563720	22833.784554	29.989248
429.272420	22871.688213	29.994266
429.866232	22897.228839	29.999284
430.988354	22923.013298	30.004301
431.597096	22946.763090	30.009319
432.221591	22960.745237	30.014336
432.528880	22974.015316	30.019354
432.532941	22993.904136	30.024372
432.966475	23005.544031	30.029389
433.619821	23016.985408	30.034407
434.061785	23044.208163	30.039424
434.363645	23052.413786	30.044442
434.398416	23069.181201	30.049460
434.985887	23087.538202	30.054477
435.671004	23122.292374	30.059495
435.938969	23137.969583	30.064512
436.210206	23167.111093	30.069530
436.034399	23199.237345	30.074548
436.490683	23219.509432	30.079565
436.483346	23261.955568	30.084583
436.937972	23309.088528	30.089600
437.162160	23346.568453	30.094618
437.288391	23389.266423	30.099636
437.872709	23424.751318	30.104653
438.098356	23485.010560	30.109671
438.692416	23521.115354	30.114688
439.498381	23573.979881	30.119706
439.472872	23618.171113	30.124724
440.087947	23658.483428	30.129741
440.299070	23714.484652	30.134759
440.732008	23763.420468	30.139776
441.239332	23820.591958	30.144794
441.416025	23880.545550	30.149812
441.960917	23914.439017	30.154829
442.056521	23976.797752	30.159847
442.685824	24028.407015	30.164864
443.390536	24092.951782	30.169882
443.647571	24148.116973	30.174900
444.453242	24188.170760	30.179917
445.000426	24245.677492	30.184935
445.350407	24298.101923	30.189952
445.622173	24348.574777	30.194970
445.729269	24407.141608	30.199988
446.598487	24451.206883	30.205005
446.995550	24517.843659	30.210023
447.609829	24558.445262	30.215040
448.231714	24616.842575	30.220058
448.220678	24673.865987	30.225076
449.238211	24723.909321	30.230093
449.514341	24774.187098	30.235111
450.135365	24814.677745	30.240128
450.203798	24869.836551	30.245146
450.366096	24920.061706	30.250164
451.098198	24972.476326	30.255181
451.689008	25024.312818	30.260199
451.657748	25082.022397	30.265216
452.557121	25133.632847	30.270234
453.088149	25189.230730	30.275252
454.037344	25218.549741	30.280269
454.603320	25258.369494	30.285287
455.479438	25289.650619	30.290304
456.382021	25320.889412	30.295322
456.715277	25344.547774	30.300340
457.316950	25367.781632	30.305357
457.534367	25402.431282	30.310375
458.068560	25418.654839	30.315392
458.587152	25450.669433	30.320410
458.396027	25477.777395	30.325428
459.059470	25501.628598	30.330445
459.828997	25541.451976	30.335463
460.028785	25569.496236	30.340480
460.182407	25596.037426	30.345498
460.149439	25631.664185	30.350516
460.718332	25673.184694	30.355533
460.935699	25725.538380	30.360551
461.068654	25775.865678	30.365568
461.589880	25819.284295	30.370586
461.526827	25882.711779	30.375604
462.159854	25933.603688	30.380621
462.435896	25991.260473	30.385639
463.561903	26035.689575	30.390656
464.120783	26068.688958	30.395674
464.728908	26113.588714	30.400692
465.243703	26156.996658	30.405709
465.514882	26214.020932	30.410727
466.197989	26247.693391	30.415744
466.799522	26306.920097	30.420762
466.829035	26358.102791	30.425780
467.612916	26388.411139	30.430797
468.080374	26444.118574	30.435815
468.257672	26495.039744	30.440832
468.561379	26535.629796	30.445850
469.055726	26598.342889	30.450868
469.609407	26647.420743	30.455885
469.606218	26700.569134	30.460903
470.331785	26748.441100	30.465920
471.207167	26804.357403	30.470938
471.506946	26868.691654	30.475956
471.974876	26908.481513	30.480973
473.890248	26929.381806	30.485991
474.424077	26958.576191	30.491008
475.654963	26992.424385	30.496026
476.123397	27013.844035	30.501044
476.323837	27026.671785	30.506061
476.404342	27055.874607	30.511079
476.574119	27087.444064	30.516096
477.333006	27127.175101	30.521114
477.153050	27158.479669	30.526132
477.912442	27189.758987	30.531149
477.841918	27226.531176	30.536167
478.303008	27259.407606	30.541184
478.700952	27298.399553	30.546202
479.782100	27339.829951	30.551220
480.455344	27378.923182	30.556237
480.657227	27418.573656	30.561255
481.173977	27439.711077	30.566272
482.330021	27467.506196	30.571290
482.517115	27505.212840	30.576308
482.663595	27517.135279	30.581325
482.866027	27557.880721	30.586343
482.786560	27589.935479	30.591360
483.348461	27633.039311	30.596378
483.434374	27674.883971	30.601396
484.103414	27715.404699	30.606413
484.493334	27768.337535	30.611431
484.717235	27814.692526	30.616448
485.658361	27845.140524	30.621466
485.635905	27905.375580	30.626484
485.861304	27945.938156	30.631501
486.513045	27988.970679	30.636519
487.160948	28041.828585	30.641536
487.560245	28101.556657	30.646554
487.922695	28159.754759	30.651572
489.232238	28200.681123	30.656589
490.016866	28237.873646	30.661607
490.567397	28272.765331	30.666624
491.740026	28293.318144	30.671642
492.619212	28326.822200	30.676660
493.086314	28349.852785	30.681677
493.528197	28386.902432	30.686695
493.543726	28411.537519	30.691712
493.962732	28435.980457	30.696730
493.977598	28477.804498	30.701748
494.433793	28512.561382	30.706765
494.688359	28555.899985	30.711783
494.825673	28606.884626	30.716800
495.549131	28646.104596	30.721818
495.493149	28708.906929	30.726836
496.131106	28760.225856	30.731853
496.065221	28819.446071	30.736871
496.960787	28879.123299	30.741888
497.280182	28939.454764	30.746906
497.772884	28990.218704	30.751924
498.409814	29040.222925	30.756941
499.054373	29099.663102	30.761959
499.135779	29157.325796	30.766976
500.234455	29220.156114	30.771994
500.947653	29265.986205	30.777012
501.448223	29312.537530	30.782029
502.270280	29356.405593	30.787047
502.697669	29407.762487	30.792064
503.287349	29451.348771	30.797082
503.488501	29506.095579	30.802100
503.791152	29547.910706	30.807117
504.396633	29604.579502	30.812135
505.053501	29658.387307	30.817152
505.430173	29702.310460	30.822170
505.854279	29749.040112	30.827188
506.127943	29806.899162	30.832205
506.726684	29861.774573	30.837223
507.133164	29919.993027	30.842240
508.451649	29958.501831	30.847258
508.403641	30006.496307	30.852276
508.609306	30051.531908	30.857293
509.049673	30096.713574	30.862311
509.692262	30149.269489	30.867328
509.996524	30206.771202	30.872346
510.323884	30261.167404	30.877364
511.125600	30315.892693	30.882381
511.839634	30365.177490	30.887399
511.947317	30425.348353	30.892416
512.052927	30473.595444	30.897434
512.660908	30540.786976	30.902452
513.233599	30600.235045	30.907469
513.787150	30657.597684	30.912487
513.540423	30725.113070	30.917504
514.375363	30787.697538	30.922522
514.714684	30871.742418	30.927540
515.324983	30927.745655	30.932557
516.138810	30990.441742	30.937575
516.586160	31058.729318	30.942592
517.323961	31123.004037	30.947610
517.839532	31183.126505	30.952628
518.543094	31256.176831	30.957645
520.021914	31282.991804	30.962663
520.793358	31332.534517	30.967680
521.698299	31370.688101	30.972698
522.412187	31419.303711	30.977716
522.822709	31460.243385	30.982733
523.255451	31494.120270	30.987751
523.648474	31540.421335	30.992768
523.890031	31563.482136	30.997786
523.886824	31621.321953	31.002804
524.281184	31675.054628	31.007821
525.229880	31716.177217	31.012839
525.850693	31762.401960	31.017856
527.310206	31789.880542	31.022874
528.222679	31823.887284	31.027892
528.465731	31843.249760	31.032909
529.225266	31879.485465	31.037927
529.536530	31921.951616	31.042944
530.234464	31955.206451	31.047962
530.383547	31990.818016	31.052980
530.313641	32025.990666	31.057997
531.247374	32061.467928	31.063015
531.203517	32113.427769	31.068032
531.661037	32165.251362	31.073050
531.941405	32209.661101	31.078068
532.222046	32254.298116	31.083085
532.183791	32315.399745	31.088103
532.509969	32378.231606	31.093120
533.099308	32448.627151	31.098138
533.407813	32514.037623	31.103156
533.782394	32582.390832	31.108173
534.656181	32658.399953	31.113191
534.843431	32729.471410	31.118208
535.816048	32796.309159	31.123226
536.095824	32856.212570	31.128244
536.180702	32918.112513	31.133261
537.078474	32984.086460	31.138279
537.071244	33063.574531	31.143296
537.781094	33124.023696	31.148314
538.637356	33200.656670	31.153332
539.008022	33277.685610	31.158349
539.440599	33335.923363	31.163367
540.005540	33416.400592	31.168384
540.563554	33485.577910	31.173402
541.248539	33557.760306	31.178420
542.010727	33614.913642	31.183437
542.763419	33682.451971	31.188455
543.309984	33750.720191	31.193472
544.275277	33796.357795	31.198490
545.324691	33865.455533	31.203508
545.544605	33926.407935	31.208525
546.146145	33974.386968	31.213543
546.576258	34031.740548	31.218560
547.406556	34085.513054	31.223578
547.981569	34127.453197	31.228596
548.602120	34170.603878	31.233613
549.424817	34230.220003	31.238631
549.828511	34286.581599	31.243648
550.222375	34333.634564	31.248666
550.939343	34391.404084	31.253684
550.831570	34453.086660	31.258701
551.345562	34508.476901	31.263719
551.543979	34576.448097	31.268736
552.583415	34634.851182	31.273754
552.968372	34707.913342	31.278772
553.280750	34776.257126	31.283789
554.113915	34838.963362	31.288807
554.132009	34908.459575	31.293824
555.224774	34961.425920	31.298842
556.002372	35026.588387	31.303860
556.005056	35085.372560	31.308877
557.013541	35162.262379	31.313895
557.298900	35226.111688	31.318912
557.843032	35292.694396	31.323930
558.138581	35365.793463	31.328948
558.725977	35433.032091	31.333965
559.494682	35498.071525	31.338983
559.676549	35574.306176	31.344000
560.366520	35648.200473	31.349018
560.821124	35716.756997	31.354036
561.384740	35795.035599	31.359053
562.187603	35860.758563	31.364071
562.641857	35937.468866	31.369088
563.268550	36009.876195	31.374106
564.068741	36079.662681	31.379124
564.480207	36159.575528	31.384141
564.958082	36213.651467	31.389159
565.501465	36288.785547	31.394176
566.493729	36351.150947	31.399194
567.332673	36408.413586	31.404212
567.597980	36475.985864	31.409229
568.637681	36518.435869	31.414247
568.734658	36578.954237	31.419264
569.341140	36642.826091	31.424282
569.879347	36702.019296	31.429300
569.837248	36760.368319	31.434317
570.402708	36822.357075	31.439335
570.759321	36901.165154	31.444352
571.183717	36968.008084	31.449370
572.035598	37046.908701	31.454388
572.520636	37122.150902	31.459405
573.041996	37190.133339	31.464423
573.489275	37260.070032	31.469440
574.229396	37343.921694	31.474458
574.558301	37418.955118	31.479476
574.904553	37503.777791	31.484493
575.783417	37572.928331	31.489511
575.979919	37663.655098	31.494528
576.404132	37757.250609	31.499546
576.772280	37832.711466	31.504564
576.984536	37933.478339	31.509581
578.143157	38024.212505	31.514599
578.668101	38117.738929	31.519616
579.308295	38205.219812	31.524634
580.107702	38291.231184	31.529652
580.656274	38376.540930	31.534669
581.856713	38458.225856	31.539687
582.278021	38546.790769	31.544704
582.616296	38623.768949	31.549722
583.845286	38699.171102	31.554740
584.272912	38776.409257	31.559757
585.373403	38847.963721	31.564775
585.945100	38918.387346	31.569792
586.636553	38988.052007	31.574810
587.157709	39060.186401	31.579828
587.724682	39134.731432	31.584845
588.181589	39201.529555	31.589863
588.773147	39280.433848	31.594880
589.157958	39350.657525	31.599898
590.043732	39427.415815	31.604916
590.409610	39502.040977	31.609933
591.385813	39568.858793	31.614951
591.675750	39635.576595	31.619968
592.161132	39710.314716	31.624986
592.895195	39789.534565	31.630004
593.140209	39865.880386	31.635021
593.960537	39947.239237	31.640039
594.331882	40025.780330	31.645056
594.966785	40100.055570	31.650074
596.817935	40154.864415	31.655092
597.874682	40216.991951	31.660109
598.738995	40266.855685	31.665127
599.507686	40306.803619	31.670144
600.426924	40344.651611	31.675162
601.442821	40377.153873	31.680180
601.433182	40419.511695	31.685197
601.997844	40448.653261	31.690215
602.184319	40484.325520	31.695232
602.298297	40532.354771	31.700250
602.851811	40580.236227	31.705268
603.425226	40636.689298	31.710285
603.913062	40684.115011	31.715303
604.181025	40746.565735	31.720320
604.515668	40804.752482	31.725338
605.385053	40855.965059	31.730356
605.689069	40935.386608	31.735373
605.953746	40990.633911	31.740391
606.430982	41058.543426	31.745408
606.814570	41129.004514	31.750426
607.573770	41194.615087	31.755444
607.870075	41287.732563	31.760461
608.836141	41359.970161	31.765479
609.721468	41416.166929	31.770496
610.611806	41488.190672	31.775514
611.086444	41556.370815	31.780532
611.252887	41628.825382	31.785549
611.707324	41704.524017	31.790567
612.134002	41794.224357	31.795584
612.340984	41874.610575	31.800602
613.069591	41962.722346	31.805620
613.277072	42052.376225	31.810637
614.133140	42151.502231	31.815655
614.259870	42240.037322	31.820672
615.167590	42332.909999	31.825690
616.828609	42401.376211	31.830708
617.451535	42481.270665	31.835725
618.289025	42565.684979	31.840743
618.906295	42645.900010	31.845760
619.448007	42717.846121	31.850778
620.084989	42802.838949	31.855796
620.451548	42889.855122	31.860813
621.148347	42957.667595	31.865831
622.082410	43041.315998	31.870848
622.835327	43119.845764	31.875866
623.097066	43195.308710	31.880884
623.412297	43276.879112	31.885901
624.187068	43343.877581	31.890919
624.821839	43431.368156	31.895936
625.304186	43518.645268	31.900954
626.075304	43600.413682	31.905972
626.342744	43684.807527	31.910989
626.843739	43770.778481	31.916007
627.663685	43865.975731	31.921024
628.181191	43958.288576	31.926042
628.822475	44039.064340	31.931060
629.447588	44128.069201	31.936077
629.936517	44219.349310	31.941095
630.986452	44307.609626	31.946112
631.174362	44402.264190	31.951130
632.043627	44477.536593	31.956148
632.479707	44571.606339	31.961165
633.069239	44656.890368	31.966183
633.779801	44724.785773	31.971200
634.451662	44810.267965	31.976218
635.579474	44878.806119	31.981236
636.428866	44950.629071	31.986253
637.726516	45009.238575	31.991271
638.526411	45067.706164	31.996288
638.698836	45136.844721	32.001306
639.780400	45198.040282	32.006324
640.199285	45267.437095	32.011341
640.949663	45333.590980	32.016359
641.612735	45402.125379	32.021376
642.032912	45470.373205	32.026394
642.514780	45538.414911	32.031412
642.852638	45618.807259	32.036429
643.347375	45685.476707	32.041447
644.072673	45754.128032	32.046464
645.107892	45831.227978	32.051482
645.946833	45897.873939	32.056500
646.564947	45962.786287	32.061517
647.496359	46025.421892	32.066535
648.245274	46092.721890	32.071552
648.834524	46156.553457	32.076570
649.883446	46226.411124	32.081588
650.116477	46288.349285	32.086605
650.702027	46357.958371	32.091623
651.486259	46424.138664	32.096640
651.838113	46496.668522	32.101658
652.471273	46562.638313	32.106676
652.858734	46633.267685	32.111693
653.573625	46700.272465	32.116711
654.492739	46776.871860	32.121728
654.408749	46852.418020	32.126746
655.261052	46927.361923	32.131764
656.111332	47015.482659	32.136781
656.817979	47082.651258	32.141799
657.545768	47151.313490	32.146816
657.920368	47238.562944	32.151834
658.655096	47312.277814	32.156852
658.999363	47395.847450	32.161869
660.255748	47467.932295	32.166887
660.625848	47543.245460	32.171904
661.411560	47629.794593	32.176922
662.519013	47699.875007	32.181940
662.182178	47785.508564	32.186957
662.690108	47867.732011	32.191975
663.669296	47953.241927	32.196992
663.870610	48045.385498	32.202010
664.580465	48134.293435	32.207028
664.925682	48229.761167	32.212045
664.763029	48334.583296	32.217063
665.399653	48435.968457	32.222080
666.110758	48546.172541	32.227098
666.870247	48630.311245	32.232116
668.005528	48728.144468	32.237133
668.639718	48819.923827	32.242151
669.603909	48911.211207	32.247168
669.783194	49016.215336	32.252186
670.588631	49102.786640	32.257204
671.450582	49199.260339	32.262221
671.991141	49288.638467	32.267239
672.599071	49380.690302	32.272256
673.006043	49476.700038	32.277274
673.798758	49574.874182	32.282292
674.342569	49683.881510	32.287309
674.728111	49790.793918	32.292327
675.641106	49886.801115	32.297344
675.747855	49997.616048	32.302362
676.891100	50097.438492	32.307380
677.718088	50206.356010	32.312397
678.454509	50310.936849	32.317415
679.470336	50408.059844	32.322432
680.627569	50508.867545	32.327450
681.371981	50592.379246	32.332468
682.341960	50680.230817	32.337485
682.614995	50787.035283	32.342503
683.327913	50878.494975	32.347520
683.576388	50968.935365	32.352538
684.489125	51068.221028	32.357556
684.981870	51167.313793	32.362573
685.598468	51277.675882	32.367591
686.682660	51374.438164	32.372608
687.094529	51462.287768	32.377626
688.538607	51552.652391	32.382644
689.774873	51636.968805	32.387661
690.350407	51733.857906	32.392679
691.553697	51801.823326	32.397696
692.268116	51879.040244	32.402714
692.919012	51947.107114	32.407732
693.806572	52027.188640	32.412749
694.188170	52110.238240	32.417767
694.718050	52183.355901	32.422784
695.102320	52278.321817	32.427802
695.818749	52365.112369	32.432820
696.760036	52433.042718	32.437837
697.877439	52521.395377	32.442855
698.654102	52584.805295	32.447872
699.526923	52652.053116	32.452890
700.645508	52714.899415	32.457908
701.445759	52790.721489	32.462925
701.942784	52847.798613	32.467943
703.097755	52924.287050	32.472960
703.932016	52993.280203	32.477978
704.577260	53053.940353	32.482996
705.377808	53106.960338	32.488013
705.357962	53175.550733	32.493031
706.348961	53238.597474	32.498048
706.896871	53299.060221	32.503066
707.073171	53366.316060	32.508084
707.653276	53427.500317	32.513101
708.068111	53493.938544	32.518119
708.983986	53551.223965	32.523136
709.434754	53623.229478	32.528154
710.192315	53708.767797	32.533172
710.671920	53771.903842	32.538189
710.942771	53858.600356	32.543207
711.668689	53936.499451	32.548224
712.081465	54015.861575	32.553242
712.393452	54091.418422	32.558260
713.471766	54192.233231	32.563277
713.740372	54292.207837	32.568295
714.044456	54391.778778	32.573312
714.805470	54500.680790	32.578330
715.169083	54601.196733	32.583348
716.155531	54694.579798	32.588365
716.815213	54813.908218	32.593383
717.697988	54911.796553	32.598400
718.242498	55029.218682	32.603418
718.678451	55137.194075	32.608436
719.673002	55247.134401	32.613453
720.053002	55366.084324	32.618471
721.133905	55469.717181	32.623488
721.464321	55594.402159	32.628506
722.460994	55699.712597	32.633524
723.360353	55816.408712	32.638541
724.753620	55926.252870	32.643559
726.459705	56003.259082	32.648576
727.898476	56082.308314	32.653594
729.120677	56154.702683	32.658612
730.161157	56218.584549	32.663629
731.020053	56280.557648	32.668647
732.027213	56342.789918	32.673664
732.429391	56414.226103	32.678682
732.727083	56483.266379	32.683700
733.764005	56546.075578	32.688717
734.187623	56610.708954	32.693735
734.877988	56685.193323	32.698752
735.507899	56755.157160	32.703770
736.521761	56820.758118	32.708788
737.073698	56890.767380	32.713805
737.565351	56969.716921	32.718823
738.263861	57040.870738	32.723840
738.658163	57124.185515	32.728858
739.116750	57212.482232	32.733876
739.928328	57291.580461	32.738893
740.153455	57387.065606	32.743911
741.082775	57471.200219	32.748928
741.710509	57561.833106	32.753946
742.167770	57655.604989	32.758964
742.739418	57749.781146	32.763981
743.289698	57853.308616	32.768999
743.779625	57957.933990	32.774016
744.359297	58066.039504	32.779034
744.927543	58164.180822	32.784052
745.403050	58269.480198	32.789069
745.942107	58376.867512	32.794087
746.520642	58487.111660	32.799104
747.466809	58600.504088	32.804122
748.057454	58708.617458	32.809140
748.926166	58820.703454	32.814157
749.510233	58930.367590	32.819175
750.129140	59042.213181	32.824192
751.231871	59158.508208	32.829210
751.576047	59279.952230	32.834228
752.840249	59392.100029	32.839245
753.655924	59505.064769	32.844263
755.002864	59598.042193	32.849280
756.048563	59707.637749	32.854298
756.992464	59810.109092	32.859316
758.248489	59890.898419	32.864333
758.787808	59985.362231	32.869351
759.765904	60080.023107	32.874368
761.135828	60154.062476	32.879386
761.700935	60246.304519	32.884404
763.588124	60306.539928	32.889421
765.544268	60349.723010	32.894439
766.583239	60404.213083	32.899456
767.456852	60456.304451	32.904474
768.149367	60506.088285	32.909492
768.638626	60551.583633	32.914509
768.890659	60611.512197	32.919527
769.602016	60664.617934	32.924544
770.534914	60722.167339	32.929562
770.854371	60787.482868	32.934580
771.520175	60851.437176	32.939597
771.650720	60919.452896	32.944615
772.136131	61000.890593	32.949632
772.862332	61082.407464	32.954650
773.183397	61168.165901	32.959668
773.817777	61255.350142	32.964685
774.004943	61342.472292	32.969703
774.660005	61450.652301	32.974720
775.231594	61554.175882	32.979738
775.428082	61666.019629	32.984756
776.292242	61776.889937	32.989773
776.939016	61887.772791	32.994791
777.770377	61988.801424	32.999808
778.592629	62107.891964	33.004826
779.122911	62220.655005	33.009844
780.285575	62327.513674	33.014861
781.318586	62447.600442	33.019879
782.104443	62553.646149	33.024896
783.060617	62653.651539	33.029914
783.737505	62758.680242	33.034932
784.711502	62864.682667	33.039949
785.187489	62982.295087	33.044967
786.028126	63089.642701	33.049984
786.804695	63200.086783	33.055002
786.900656	63315.471434	33.060020
787.840323	63416.937295	33.065037
788.521185	63528.657520	33.070055
789.634720	63625.947583	33.075072
791.210874	63721.875543	33.080090
791.977235	63828.082797	33.085108
792.693801	63914.549760	33.090125
793.424639	64005.161764	33.095143
794.765576	64092.413897	33.100160
795.474313	64187.632799	33.105178
796.329322	64278.186785	33.110196
797.474880	64365.245933	33.115213
798.052726	64470.900797	33.120231
798.443166	64571.549646	33.125248
799.340803	64659.828377	33.130266
799.993326	64759.744136	33.135284
800.533547	64859.091649	33.140301
801.259646	64960.070514	33.145319
802.136306	65061.453982	33.150336
802.651627	65171.169257	33.155354
803.391081	65283.394569	33.160372
804.280113	65390.935354	33.165389
804.861888	65515.321327	33.170407
805.534017	65633.970845	33.175424
806.375804	65743.759625	33.180442
806.595899	65871.446694	33.185460
807.665397	65988.455862	33.190477
808.229213	66119.202513	33.195495
808.898779	66236.863223	33.200512
809.891861	66366.930917	33.205530
810.789277	66497.869344	33.210548
811.944296	66616.188752	33.215565
812.750686	66744.425563	33.220583
813.206860	66866.432047	33.225600
814.329370	66995.665796	33.230618
815.147822	67129.327772	33.235636
816.047159	67245.924103	33.240653
817.267241	67365.987961	33.245671
818.370485	67479.743303	33.250688
819.233824	67589.980543	33.255706
820.367255	67695.910426	33.260724
821.853289	67781.458407	33.265741
823.131925	67888.894537	33.270759
823.994774	67989.238429	33.275776
825.158756	68073.173461	33.280794
825.325604	68176.906463	33.285812
826.061867	68274.548124	33.290829
826.852832	68367.906415	33.295847
827.440634	68470.613943	33.300864
828.311749	68572.679057	33.305882
828.631566	68684.285994	33.310900
829.424144	68791.196551	33.315917
829.864831	68909.455004	33.320935
830.445489	69025.413731	33.325952
831.170079	69133.956411	33.330970
831.984932	69246.075871	33.335988
833.245675	69341.330833	33.341005
834.169118	69453.837476	33.346023
834.888194	69547.238498	33.351040
835.630890	69655.034531	33.356058
835.945738	69770.903679	33.361076
836.988620	69870.744933	33.366093
838.033531	69993.775003	33.371111
838.416148	70110.380550	33.376128
839.208743	70230.109967	33.381146
839.831063	70347.953122	33.386164
840.940286	70459.958905	33.391181
842.032179	70578.563948	33.396199
842.632726	70694.167769	33.401216
843.624231	70803.596398	33.406234
844.508440	70930.523189	33.411252
845.777037	71039.722158	33.416269
846.162677	71157.882175	33.421287
847.051653	71271.586746	33.426304
848.112400	71388.070359	33.431322
849.383264	71516.199149	33.436340
850.082915	71640.828113	33.441357
850.798790	71761.515074	33.446375
851.378993	71882.143725	33.451392
852.250237	71998.833809	33.456410
852.900088	72130.127155	33.461428
853.214782	72247.337610	33.466445
854.336717	72375.718299	33.471463
854.860511	72520.974364	33.476480
856.131395	72647.313666	33.481498
857.434754	72773.844191	33.486516
858.205043	72882.638094	33.491533
859.887122	72989.979853	33.496551
860.363199	73109.924750	33.501568
861.705891	73223.726197	33.506586
862.704351	73345.366434	33.511604
863.272512	73467.852645	33.516621
864.029652	73582.161009	33.521639
864.450720	73704.774921	33.526656
865.269010	73829.946245	33.531674
866.502846	73937.306150	33.536692
868.682091	74038.047050	33.541709
870.521978	74115.957031	33.546727
872.176356	74205.397610	33.551744
872.967428	74273.418640	33.556762
874.184545	74355.768657	33.561780
875.168780	74416.692157	33.566797
877.405085	74456.282509	33.571815
878.420883	74498.320988	33.576832
879.444502	74544.899509	33.581850
880.236353	74598.785187	33.586868
880.741378	74641.562887	33.591885
881.182899	74688.772701	33.596903
881.622494	74745.407180	33.601920
881.962366	74792.527100	33.606938
882.262080	74857.528503	33.611956
883.135633	74921.755038	33.616973
883.548623	74997.186419	33.621991
883.657403	75075.231815	33.627008
884.269551	75150.465155	33.632026
884.214314	75239.310873	33.637044
885.020848	75335.150457	33.642061
885.329010	75437.394667	33.647079
885.578338	75565.740952	33.652096
886.546224	75682.699627	33.657114
886.770366	75811.785369	33.662132
887.344911	75951.723039	33.667149
888.105740	76091.541126	33.672167
888.504116	76252.903269	33.677184
889.216703	76396.197849	33.682202
889.752012	76559.056852	33.687220
890.814072	76710.535721	33.692237
891.492387	76871.803765	33.697255
892.432486	77042.889802	33.702272
893.400732	77201.776397	33.707290
894.603119	77365.153236	33.712308
896.147391	77520.685679	33.717325
897.019589	77678.643220	33.722343
897.689582	77845.979796	33.727360
898.572179	78001.287274	33.732378
899.337891	78163.675600	33.737396
900.494980	78306.767034	33.742413
902.403792	78465.444504	33.747431
903.328770	78620.755299	33.752448
904.618188	78756.798638	33.757466
905.113969	78908.800435	33.762484
906.161676	79046.209070	33.767501
907.249154	79188.027439	33.772519
908.129548	79341.459248	33.777536
909.180051	79486.309770	33.782554
909.800354	79637.535943	33.787572
910.734112	79772.545477	33.792589
911.328914	79927.883774	33.797607
911.796992	80079.006082	33.802624
912.967423	80229.015838	33.807642
913.812202	80394.614077	33.812660
914.505429	80557.632900	33.817677
915.587643	80714.265928	33.822695
916.724084	80873.731428	33.827712
917.778205	81017.610377	33.832730
918.914418	81173.028876	33.837748
919.775410	81333.392524	33.842765
920.755456	81481.500726	33.847783
921.663356	81646.477133	33.852800
922.632905	81799.745612	33.857818
923.225124	81954.174298	33.862836
924.182432	82112.590798	33.867853
925.513009	82257.069161	33.872871
926.286411	82422.643571	33.877888
927.420493	82567.410604	33.882906
928.292483	82707.092061	33.887924
929.044388	82847.263138	33.892941
930.407279	82991.202723	33.897959
930.831681	83137.429898	33.902976
932.171357	83272.225891	33.907994
933.269154	83415.644035	33.913012
933.662523	83547.933519	33.918029
935.080959	83688.912990	33.923047
936.346721	83821.200152	33.928064
937.484782	83960.052613	33.933082
938.617371	84086.561726	33.938100
939.551398	84210.270756	33.943117
940.619016	84330.407753	33.948135
941.288409	84468.280444	33.953152
941.702913	84602.483223	33.958170
942.496853	84740.766467	33.963188
942.678709	84893.272653	33.968205
943.817815	85044.673047	33.973223
944.506576	85187.045723	33.978240
945.582884	85348.779591	33.983258
946.622552	85505.464801	33.988276
947.474520	85667.941676	33.993293
948.701107	85819.249795	33.998311
949.698180	85984.026384	34.003328
950.499514	86132.624971	34.008346
951.525604	86294.671327	34.013364
952.636962	86452.021310	34.018381
954.017230	86605.744493	34.023399
955.034670	86753.455643	34.028416
956.169670	86904.469952	34.033434
957.340018	87055.770271	34.038452
958.139111	87198.104484	34.043469
959.498916	87339.198075	34.048487
960.819668	87476.932435	34.053504
961.692827	87612.326744	34.058522
962.609465	87751.271022	34.063540
963.323924	87898.028572	34.068557
964.282462	88038.663406	34.073575
965.123576	88184.356794	34.078592
965.648563	88332.737945	34.083610
966.161490	88487.140718	34.088628
967.099570	88645.705636	34.093645
967.932350	88805.175668	34.098663
968.829320	88977.635277	34.103680
969.670807	89134.574444	34.108698
970.681253	89278.340447	34.113716
971.687127	89459.658050	34.118733
972.568459	89619.568174	34.123751
973.781771	89785.112356	34.128768
975.001513	89949.726186	34.133786
976.351162	90110.534039	34.138804
976.972959	90270.714422	34.143821
977.857313	90432.281310	34.148839
978.713946	90601.626400	34.153856
979.589281	90752.848551	34.158874
980.721033	90910.312807	34.163892
981.388865	91071.484281	34.168909
982.106538	91220.426087	34.173927
983.280328	91388.836202	34.178944
984.141601	91548.749770	34.183962
984.773380	91712.862221	34.188980
985.455980	91885.720950	34.193997
986.487551	92039.108018	34.199015
987.596387	92224.099751	34.204032
988.420142	92389.228247	34.209050
989.888613	92556.418571	34.214068
990.788034	92734.734075	34.219085
991.776719	92895.818265	34.224103
993.126831	93073.229820	34.229120
994.504055	93226.698016	34.234138
995.847683	93383.673418	34.239156
996.980871	93548.066699	34.244173
999.028970	93687.325831	34.249191
1000.263880	93817.615939	34.254208
1001.860917	93949.142404	34.259226
1002.823141	94073.156715	34.264244
1003.505688	94210.702921	34.269261
1004.598302	94334.512631	34.274279
1005.982410	94473.161892	34.279296
1007.144824	94600.822453	34.284314
1008.127172	94720.835776	34.289332
1008.957233	94851.548790	34.294349
1009.768485	94978.296533	34.299367
1010.612814	95114.167772	34.304384
1011.314542	95243.645048	34.309402
1012.478019	95387.274943	34.314420
1013.064759	95525.344898	34.319437
1014.309616	95670.228590	34.324455
1014.872354	95815.141292	34.329472
1015.513076	95965.068027	34.334490
1017.199821	96093.925206	34.339508
1018.488185	96238.684438	34.344525
1019.932981	96363.292185	34.349543
1021.183102	96505.065041	34.354560
1022.324210	96625.554083	34.359578
1023.690500	96747.714476	34.364596
1024.491138	96871.896911	34.369613
1025.559589	96998.902008	34.374631
1026.890706	97118.012373	34.379648
1028.175842	97228.919879	34.384666
1029.249975	97348.360225	34.389684
1029.751352	97479.548338	34.394701
1030.711013	97602.485227	34.399719
1031.459874	97743.844360	34.404736
1031.924539	97875.047127	34.409754
1032.783737	98009.234642	34.414772
1032.648173	98157.217975	34.419789
1033.406287	98322.593051	34.424807
1034.284266	98489.911374	34.429824
1035.125983	98653.742099	34.434842
1035.932880	98807.601579	34.439860
1036.463129	98983.783286	34.444877
1037.546385	99142.744899	34.449895
1038.798966	99301.507551	34.454912
1039.651496	99479.340642	34.459930
1040.976635	99637.637073	34.464948
1041.513734	99807.409350	34.469965
1042.836501	99989.781196	34.474983
1044.146071	100155.269913	34.480000
1045.426410	100320.410117	34.485018
1047.225140	100460.186116	34.490036
1048.111425	100619.747752	34.495053
1049.560029	100767.538133	34.500071
1050.660345	100919.162802	34.505088
1052.012304	101080.737060	34.510106
1053.009430	101224.820851	34.515124
1053.958976	101391.404879	34.520141
1054.927344	101532.012687	34.525159
1055.470567	101692.386821	34.530176
1056.752869	101858.916855	34.535194
1057.787161	102011.331700	34.540212
1058.752992	102188.138126	34.545229
1059.393804	102358.808461	34.550247
1060.098589	102535.016033	34.555264
1061.477436	102711.451314	34.560282
1062.207303	102895.496431	34.565300
1063.159463	103069.385569	34.570317
1064.503142	103235.635198	34.575335
1065.460123	103422.342729	34.580352
1066.499371	103599.981954	34.585370
1067.861307	103771.335857	34.590388
1068.692290	103959.322601	34.595405
1069.583413	104145.679215	34.600423
1070.930328	104322.510681	34.605440
1071.990941	104507.916237	34.610458
1073.077621	104684.389371	34.615476
1073.869833	104879.912627	34.620493
1074.969699	105071.483574	34.625511
1076.251311	105263.392086	34.630528
1077.127813	105454.928030	34.635546
1078.409630	105645.990630	34.640564
1080.128369	105810.254225	34.645581
1081.848157	105969.781484	34.650599
1082.798079	106147.414972	34.655616
1083.788047	106326.334745	34.660634
1085.081639	106496.185201	34.665652
1086.230128	106670.254195	34.670669
1086.947748	106833.428795	34.675687
1088.019859	107014.011054	34.680704
1088.277395	107199.256030	34.685722
1089.541462	107380.289201	34.690740
1090.319065	107577.582576	34.695757
1091.514010	107758.440097	34.700775
1092.804465	107938.370435	34.705792
1093.527297	108139.072047	34.710810
1094.721145	108311.940414	34.715828
1095.541576	108496.451802	34.720845
1096.814161	108671.348411	34.725863
1097.731646	108856.744999	34.730880
1098.335842	109045.895433	34.735898
1099.407299	109243.277195	34.740916
1100.173224	109440.053960	34.745933
1101.253533	109634.257389	34.750951
1102.371064	109837.412090	34.755968
1103.315300	110033.275797	34.760986
1104.280833	110240.183904	34.766004
1105.435520	110447.187853	34.771021
1106.831045	110644.220106	34.776039
1108.346109	110856.891516	34.781056
1109.303173	111059.031166	34.786074
1111.180468	111246.433109	34.791092
1112.221368	111434.486266	34.796109
1113.864817	111615.849741	34.801127
1115.585814	111793.818521	34.806144
1116.340920	111982.874468	34.811162
1119.560210	112107.429725	34.816180
1121.710653	112253.997398	34.821197
1122.859513	112396.163752	34.826215
1124.478389	112537.756254	34.831232
1125.548943	112676.592757	34.836250
1126.586880	112802.930879	34.841268
1127.632494	112924.605911	34.846285
1128.611152	113053.438509	34.851303
1129.397983	113195.734233	34.856320
1130.392481	113343.975167	34.861338
1130.892877	113488.297860	34.866356
1131.721937	113627.915231	34.871373
1132.652712	113779.995613	34.876391
1133.240062	113945.236241	34.881408
1133.950619	114122.265118	34.886426
1134.584917	114295.887247	34.891444
1135.328278	114481.173590	34.896461
1136.234542	114674.529493	34.901479
1137.407091	114867.232942	34.906496
1137.871965	115069.840366	34.911514
1138.808088	115269.657063	34.916532
1139.791868	115481.972815	34.921549
1140.673215	115705.483176	34.926567
1141.639159	115922.201944	34.931584
1142.475081	116149.043256	34.936602
1143.273158	116379.263298	34.941620
1144.171367	116614.663153	34.946637
1145.230236	116855.435322	34.951655
1146.500852	117092.751998	34.956672
1147.425791	117351.671098	34.961690
1148.336063	117594.616288	34.966708
1149.218108	117833.323357	34.971725
1150.411705	118086.842910	34.976743
1151.545881	118336.497265	34.981760
1152.426237	118594.687370	34.986778
1153.721833	118838.375236	34.991796
1154.827815	119095.073823	34.996813
1156.274286	119336.598392	35.001831
1157.924697	119569.232070	35.006848
1159.844051	119805.205069	35.011866
1161.317434	120012.160214	35.016884
1162.986862	120237.864028	35.021901
1164.143653	120457.827882	35.026919
1165.935239	120656.204311	35.031936
1166.981758	120873.782286	35.036954
1168.777286	121066.800147	35.041972
1169.734221	121260.976668	35.046989
1171.288068	121460.881888	35.052007
1172.694045	121648.495405	35.057024
1173.526563	121860.870481	35.062042
1174.722953	122056.962839	35.067060
1175.730257	122256.941575	35.072077
1176.881980	122465.248774	35.077095
1178.415962	122664.328933	35.082112
1179.216713	122869.555943	35.087130
1180.873717	123060.759946	35.092148
1182.035218	123262.860798	35.097165
1182.988135	123473.274799	35.102183
1184.876923	123671.337599	35.107200
1185.832360	123875.264832	35.112218
1186.700704	124068.916876	35.117236
1187.904156	124264.768799	35.122253
1188.750169	124474.815093	35.127271
1190.284535	124678.002165	35.132288
1191.263485	124872.628954	35.137306
1192.902502	125068.132592	35.142324
1194.580238	125270.652628	35.147341
1195.719335	125474.356238	35.152359
1196.979893	125673.185920	35.157376
1198.240549	125867.580630	35.162394
1199.745690	126049.031527	35.167412
1201.064650	126235.040368	35.172429
1202.068469	126432.790785	35.177447
1203.484136	126614.805334	35.182464
1204.379822	126808.368460	35.187482
1205.811733	126994.007584	35.192500
1207.389455	127177.366613	35.197517
1208.502414	127372.683276	35.202535
1209.669139	127555.709260	35.207552
1210.690345	127744.946966	35.212570
1212.365676	127927.647207	35.217588
1213.342625	128113.015912	35.222605
1214.359352	128302.942231	35.227623
1215.334613	128480.226134	35.232640
1216.801648	128675.148000	35.237658
1217.770115	128869.953598	35.242676
1219.090656	129052.898542	35.247693
1219.970002	129248.330174	35.252711
1221.654845	129424.978149	35.257728
1223.227521	129609.087383	35.262746
1224.175712	129787.257882	35.267764
1225.353674	129948.454113	35.272781
1226.334939	130129.828034	35.277799
1228.019492	130289.113817	35.282816
1228.967490	130472.612382	35.287834
1230.186035	130651.704838	35.292852
1231.023235	130833.475020	35.297869
1231.593460	131032.963682	35.302887
1232.832955	131214.147380	35.307904
1233.785546	131414.637815	35.312922
1234.344940	131609.187786	35.317940
1234.996188	131826.795921	35.322957
1235.320901	132044.207860	35.327975
1236.682669	132278.723146	35.332992
1237.606828	132533.675247	35.338010
1238.605045	132777.840614	35.343028
1239.658425	133016.242642	35.348045
1240.925300	133278.723183	35.353063
1241.920740	133521.639441	35.358080
1243.360325	133788.607839	35.363098
1244.690929	134055.546336	35.368116
1245.836425	134317.067010	35.373133
1246.775929	134572.653487	35.378151
1249.260839	134812.598386	35.383168
1250.518117	135073.991768	35.388186
1252.146260	135321.871643	35.393204
1253.758175	135571.746697	35.398221
1255.171472	135821.695650	35.403239
1256.200588	136066.158848	35.408256
1257.371000	136312.425413	35.413274
1258.845468	136557.741508	35.418292
1259.824811	136804.754401	35.423309
1260.783083	137063.057293	35.428327
1262.168959	137310.143745	35.433344
1263.378251	137567.545298	35.438362
1264.635025	137832.890777	35.443380
1266.199689	138084.757807	35.448397
1267.041303	138355.148844	35.453415
1268.648673	138611.615200	35.458432
1269.807138	138868.794310	35.463450
1270.704507	139131.979671	35.468468
1272.071431	139403.620419	35.473485
1272.848998	139680.246092	35.478503
1273.996899	139954.692948	35.483520
1275.019207	140236.923923	35.488538
1275.744040	140532.941182	35.493556
1277.366009	140824.381808	35.498573
1278.077266	141124.679783	35.503591
1279.145722	141425.971690	35.508608
1280.456437	141723.965678	35.513626
1281.750573	142029.218623	35.518644
1283.283906	142328.257485	35.523661
1284.475834	142631.466061	35.528679
1286.511013	142924.552567	35.533696
1288.618475	143196.273373	35.538714
1291.594009	143422.422031	35.543732
1293.673585	143648.319670	35.548749
1295.522207	143875.399624	35.553767
1297.257512	144082.260154	35.558784
1298.570087	144301.914212	35.563802
1300.218599	144495.095475	35.568820
1302.063838	144692.074081	35.573837
1303.282827	144891.786158	35.578855
1304.495991	145091.487648	35.583872
1305.262325	145292.471534	35.588890
1306.084782	145500.270027	35.593908
1307.534803	145699.591878	35.598925
1308.542720	145922.491156	35.603943
1309.549203	146129.107608	35.608960
1310.523866	146359.358438	35.613978
1311.788527	146571.183796	35.618996
1312.768286	146795.602424	35.624013
1313.840474	147033.196787	35.629031
1315.201048	147263.196948	35.634048
1316.308004	147503.692769	35.639066
1317.532083	147745.603289	35.644084
1318.550228	147987.778924	35.649101
1320.159312	148236.272720	35.654119
1321.838521	148465.312553	35.659136
1323.937103	148698.163135	35.664154
1325.428231	148921.149886	35.669172
1326.630649	149146.407003	35.674189
1327.804763	149383.149032	35.679207
1329.241772	149611.260640	35.684224
1330.586435	149839.516263	35.689242
1331.810618	150086.109441	35.694260
1332.875888	150319.895215	35.699277
1334.111821	150552.486273	35.704295
1335.464350	150788.394715	35.709312
1336.737261	151030.647661	35.714330
1337.799382	151268.917288	35.719348
1339.445034	151509.435117	35.724365
1340.956439	151752.869478	35.729383
1342.167898	151996.356709	35.734400
1343.688007	152232.283343	35.739418
1344.446328	152481.445087	35.744436
1345.958048	152732.483662	35.749453
1347.019177	152984.742610	35.754471
1348.349268	153240.115695	35.759488
1349.732436	153503.536345	35.764506
1350.641458	153755.445721	35.769524
1352.405701	154011.104674	35.774541
1353.693101	154273.468607	35.779559
1354.629966	154532.963954	35.784576
1355.924891	154793.351114	35.789594
1357.026360	155063.502881	35.794612
1358.677657	155340.158879	35.799629
1360.131005	155612.550215	35.804647
1361.414446	155880.989139	35.809664
1362.941886	156149.299284	35.814682
1363.642387	156406.677914	35.819700
1365.222137	156652.439516	35.824717
1366.821257	156918.966442	35.829735
1367.881225	157164.705927	35.834752
1369.792568	157413.104833	35.839770
1370.690888	157671.764272	35.844788
1371.931189	157929.986213	35.849805
1372.828306	158195.081162	35.854823
1374.083589	158469.758313	35.859840
1375.355039	158749.699485	35.864858
1376.212337	159038.340424	35.869876
1378.043073	159312.163445	35.874893
1378.965771	159614.549713	35.879911
1379.984026	159907.964768	35.884928
1381.140452	160202.601556	35.889946
1382.230766	160510.306848	35.894964
1384.149062	160818.405530	35.899981
1385.310128	161141.036240	35.904999
1386.494790	161455.139364	35.910016
1387.533550	161759.449582	35.915034
1389.068144	162078.775420	35.920052
1390.575849	162388.097587	35.925069
1392.287885	162715.517941	35.930087
1393.556350	163023.654880	35.935104
1396.089229	163326.768830	35.940122
1397.384687	163639.777717	35.945140
1399.356775	163924.162625	35.950157
1401.550135	164218.129232	35.955175
1403.265227	164510.720497	35.960192
1404.867480	164791.469306	35.965210
1405.920908	165082.426591	35.970228
1407.725833	165366.176911	35.975245
1409.073321	165650.502188	35.980263
1410.520251	165930.929487	35.985280
1412.231936	166211.034072	35.990298
1413.167941	166498.290142	35.995316
1414.293605	166785.096842	36.000333
1415.617324	167084.281405	36.005351
1416.774134	167378.776125	36.010368
1418.223082	167670.342286	36.015386
1419.393396	167969.749253	36.020404
1421.345494	168262.324354	36.025421
1422.292751	168561.291152	36.030439
1423.538008	168868.723601	36.035456
1424.501055	169175.356179	36.040474
1425.991777	169485.009460	36.045492
1427.587461	169790.053106	36.050509
1429.146907	170102.046333	36.055527
1430.311807	170417.713120	36.060544
1431.970840	170725.835671	36.065562
1433.502676	171030.542955	36.070580
1435.671203	171335.460485	36.075597
1437.542394	171639.263341	36.080615
1438.973762	171928.815912	36.085632
1440.603504	172210.595077	36.090650
1441.300304	172497.662545	36.095668
1443.110486	172774.084078	36.100685
1444.135229	173060.578439	36.105703
1445.488641	173343.401361	36.110720
1447.285578	173626.048489	36.115738
1447.930005	173912.422569	36.120756
1449.346989	174199.732143	36.125773
1450.914215	174503.135359	36.130791
1451.730840	174802.747319	36.135808
1453.155220	175103.970391	36.140826
1454.179240	175413.132416	36.145844
1455.777442	175721.906180	36.150861
1456.955659	176041.351101	36.155879
1458.121902	176373.935855	36.160896
1459.610624	176700.832512	36.165914
1460.388066	177038.983639	36.170932
1461.565674	177389.493801	36.175949
1462.342839	177737.917263	36.180967
1463.171401	178103.049627	36.185984
1464.896138	178468.551568	36.191002
1466.602139	178839.301148	36.196020
1467.776210	179205.613250	36.201037
1470.061993	179582.944994	36.206055
1471.259038	179960.351524	36.211072
1473.194160	180329.549284	36.216090
1474.130423	180710.496206	36.221108
1475.850998	181076.423066	36.226125
1477.345382	181452.659589	36.231143
1478.736788	181836.100519	36.236160
1480.644347	182213.502816	36.241178
1482.512597	182587.512706	36.246196
1483.952309	182967.462710	36.251213
1485.396194	183338.212020	36.256231
1486.665022	183712.700210	36.261248
1487.833725	184104.623391	36.266266
1489.597948	184487.536565	36.271284
1491.302531	184869.155107	36.276301
1493.361895	185251.477121	36.281319
1494.592235	185626.962012	36.286336
1496.798173	185992.101960	36.291354
1498.349334	186385.638298	36.296372
1500.438710	186751.983531	36.301389
1502.076929	187106.056946	36.306407
1503.780049	187468.918439	36.311424
1505.659549	187820.961896	36.316442
1506.745346	188157.491210	36.321460
1508.083824	188587.016252	36.326477
1509.971753	188944.917030	36.331495
1511.648490	189300.253699	36.336512
1512.699230	189647.892398	36.341530
1514.389747	190015.290778	36.346548
1515.403932	190364.133116	36.351565
1516.986246	190732.836485	36.356583
1518.136988	191096.068232	36.361600
1519.506716	191456.814498	36.366618
1521.162146	191804.983940	36.371636
1522.521646	192152.329991	36.376653
1524.260216	192492.897330	36.381671
1525.985586	192840.514623	36.386688
1527.548593	193166.896926	36.391706
1529.074035	193527.564870	36.396724
1530.736856	193870.386893	36.401741
1532.462916	194200.428209	36.406759
1533.968739	194555.747717	36.411776
1535.746511	194885.263121	36.416794
1536.796262	195231.142580	36.421812
1538.367378	195574.484339	36.426829
1540.178828	195929.009876	36.431847
1541.645900	196285.678348	36.436864
1542.706123	196636.565475	36.441882
1544.233130	196996.363346	36.446900
1545.633861	197350.928528	36.451917
1547.262891	197717.505155	36.456935
1548.553026	198089.220221	36.461952
1549.839910	198443.785097	36.466970
1551.448943	198829.809080	36.471988
1552.988806	199201.601587	36.477005
1554.872874	199574.962300	36.482023
1556.010417	199961.873007	36.487040
1557.552119	200333.861547	36.492058
1559.284242	200717.906698	36.497076
1560.922565	201097.983132	36.502093
1562.551484	201471.409994	36.507111
1563.891825	201870.459726	36.512128
1565.484270	202249.889701	36.517146
1566.721926	202651.424395	36.522164
1568.060221	203036.704386	36.527181
1569.649666	203429.180751	36.532199
1571.075034	203836.733448	36.537216
1573.006464	204235.719896	36.542234
1574.410849	204623.662971	36.547252
1576.283949	205022.625334	36.552269
1577.744106	205423.945926	36.557287
1579.289631	205844.224114	36.562304
1580.904529	206242.449529	36.567322
1582.858967	206648.072359	36.572340
1584.413212	207042.604350	36.577357
1587.190000	207426.656508	36.582375
1588.650240	207815.164119	36.587392
1591.156197	208200.269332	36.592410
1592.685603	208580.870543	36.597428
1593.919230	208939.531044	36.602445
1596.246439	209312.405585	36.607463
1597.458630	209681.612289	36.612480
1599.130932	210043.148304	36.617498
1600.724178	210418.464264	36.622516
1602.200956	210801.166780	36.627533
1603.708747	211171.751386	36.632551
1605.087965	211546.194451	36.637568
1606.245384	211923.978624	36.642586
1607.995507	212286.704077	36.647604
1609.519535	212644.237833	36.652621
1611.001001	213010.542309	36.657639
1612.395925	213384.736214	36.662656
1614.158850	213750.081117	36.667674
1615.621970	214121.955102	36.672692
1616.795657	214482.247927	36.677709
1618.408195	214849.375195	36.682727
1619.742821	215244.819208	36.687744
1621.460051	215626.255868	36.692762
1622.958373	216013.522206	36.697780
1624.500582	216397.607762	36.702797
1626.560509	216789.886023	36.707815
1628.349607	217187.926758	36.712832
1629.962969	217570.988618	36.717850
1631.410166	217958.245677	36.722868
1632.626626	218364.389422	36.727885
1634.103912	218750.958470	36.732903
1635.383879	219174.797337	36.737920
1637.491084	219580.920266	36.742938
1638.701234	220004.698101	36.747956
1640.038777	220425.560256	36.752973
1641.474323	220842.495740	36.757991
1642.701066	221287.382308	36.763008
1644.814562	221714.720286	36.768026
1646.523238	222150.129934	36.773044
1647.423491	222582.098166	36.778061
1649.418341	223042.099716	36.783079
1651.090428	223486.156380	36.788096
1652.641723	223928.406528	36.793114
1654.395279	224382.383819	36.798132
1655.586562	224830.794736	36.803149
1657.196202	225285.587279	36.808167
1658.354819	225758.518141	36.813184
1660.302598	226224.762398	36.818202
1661.771149	226692.487295	36.823220
1663.085853	227180.027105	36.828237
1664.870924	227645.008647	36.833255
1666.555563	228126.062132	36.838272
1668.463704	228609.974684	36.843290
1670.193254	229096.281683	36.848308
1672.003696	229583.770286	36.853325
1674.593072	230046.462836	36.858343
1677.143715	230500.120635	36.863360
1679.794164	230939.411039	36.868378
1681.678824	231385.412595	36.873396
1683.971959	231822.023232	36.878413
1685.726904	232248.922194	36.883431
1687.498329	232678.969204	36.888448
1689.359040	233097.088739	36.893466
1691.027944	233519.915984	36.898484
1692.524841	233949.886120	36.903501
1694.297830	234365.991554	36.908519
1695.440887	234800.342530	36.913536
1696.776655	235218.912453	36.918554
1698.556869	235639.007577	36.923572
1700.150007	236056.138197	36.928589
1701.444030	236465.954312	36.933607
1703.178917	236879.836360	36.938624
1704.699955	237291.596655	36.943642
1706.314961	237712.105400	36.948660
1707.634608	238129.439429	36.953677
1709.090327	238563.160780	36.958695
1710.195266	239019.144529	36.963712
1711.277710	239470.484412	36.968730
1712.976669	239914.454616	36.973748
1714.090984	240389.948391	36.978765
1715.764791	240868.370241	36.983783
1717.155872	241353.268175	36.988800
1718.459229	241832.263217	36.993818
1720.494208	242320.202644	36.998836
1722.170960	242821.489760	37.003853
1724.292462	243304.589558	37.008871
1725.685717	243815.960890	37.013888
1727.604339	244318.504631	37.018906
1729.386413	244817.363698	37.023924
1730.888458	245326.813562	37.028941
1732.559574	245828.284139	37.033959
1734.902610	246332.231531	37.038976
1736.716247	246834.517338	37.043994
1738.590778	247342.585210	37.049012
1740.207249	247851.510718	37.054029
1742.171671	248356.261981	37.059047
1744.134978	248869.041310	37.064064
1745.974626	249377.803219	37.069082
1748.235277	249867.644502	37.074100
1749.894818	250376.082466	37.079117
1751.833781	250880.459342	37.084135
1753.597815	251381.462492	37.089152
1755.982145	251879.006642	37.094170
1757.889853	252370.637482	37.099188
1759.545255	252867.036732	37.104205
1761.605469	253346.245227	37.109223
1763.733640	253840.582583	37.114240
1765.477437	254322.258872	37.119258
1767.278032	254800.597764	37.124276
1769.037273	255291.645439	37.129293
1770.814864	255780.200547	37.134311
1772.658644	256261.123428	37.139328
1773.972022	256747.674970	37.144346
1775.923715	257231.424577	37.149364
1777.531313	257720.085033	37.154381
1779.469632	258199.950155	37.159399
1781.526513	258706.138027	37.164416
1783.066317	259206.368272	37.169434
1784.755246	259699.282144	37.174452
1785.830531	260199.921765	37.179469
1787.633514	260702.189508	37.184487
1789.188698	261206.684067	37.189504
1790.886475	261709.248721	37.194522
1792.826152	262190.255251	37.199540
1794.368022	262682.227451	37.204557
1795.913635	263161.370106	37.209575
1797.947734	263652.546097	37.214592
1799.375028	264141.259775	37.219610
1801.690509	264629.135205	37.224628
1803.302135	265124.446640	37.229645
1805.220568	265606.165310	37.234663
1807.129931	266104.574756	37.239680
1809.089716	266597.056132	37.244698
1811.461130	267062.133017	37.249716
1813.954614	267548.196628	37.254733
1816.504242	268017.103113	37.259751
1818.785375	268470.610031	37.264768
1820.140637	268943.199782	37.269786
1822.040564	269405.407600	37.274804
1823.822467	269867.965180	37.279821
1825.702668	270334.772901	37.284839
1827.411269	270812.989611	37.289856
1828.972995	271279.926524	37.294874
1830.941213	271760.256457	37.299892
1832.077291	272245.249523	37.304909
1833.970364	272721.322973	37.309927
1835.210155	273224.027352	37.314944
1836.738216	273726.198758	37.319962
1839.029958	274212.920925	37.324980
1840.758527	274715.589386	37.329997
1842.001752	275222.886740	37.335015
1844.416195	275740.981694	37.340032
1845.647009	276251.708059	37.345050
1847.687844	276769.330966	37.350068
1848.696324	277302.471890	37.355085
1850.772371	277824.658402	37.360103
1852.334959	278356.228377	37.365120
1854.302137	278899.564836	37.370138
1855.899008	279445.020565	37.375156
1857.541154	279996.156839	37.380173
1859.063946	280545.330487	37.385191
1860.819503	281108.661926	37.390208
1862.889987	281673.334675	37.395226
1864.692967	282228.881406	37.400244
1866.499386	282807.210408	37.405261
1868.306068	283371.363472	37.410279
1870.248715	283940.672991	37.415296
1871.995016	284517.126163	37.420314
1874.236226	285084.856184	37.425332
1875.890349	285665.308489	37.430349
1877.377547	286246.929983	37.435367
1879.239499	286833.260209	37.440384
1881.484452	287420.309802	37.445402
1883.527449	287985.420202	37.450420
1885.524919	288574.386603	37.455437
1887.710944	289158.111063	37.460455
1889.965312	289725.692241	37.465472
1891.766640	290302.568400	37.470490
1893.676732	290859.662344	37.475508
1894.974524	291412.769110	37.480525
1896.951390	291966.061922	37.485543
1898.919280	292522.249142	37.490560
1901.011853	293076.812183	37.495578
1902.638425	293635.363636	37.500596
1904.379340	294205.525386	37.505613
1906.389311	294768.755084	37.510631
1908.421897	295335.990936	37.515648
1909.840563	295904.116104	37.520666
1911.948928	296471.866230	37.525684
1913.909333	297048.781864	37.530701
1915.746362	297621.854818	37.535719
1917.802701	298201.972979	37.540736
1919.510780	298791.239671	37.545754
1920.921707	299360.210166	37.550772
1922.523953	299963.761226	37.555789
1924.644392	300557.492660	37.560807
1926.724651	301154.198641	37.565824
1928.784674	301762.053455	37.570842
1930.277490	302365.455192	37.575860
1932.019083	302972.822970	37.580877
1934.107029	303592.089033	37.585895
1936.205254	304203.349134	37.590912
1937.895675	304844.641943	37.595930
1940.288730	305452.820557	37.600948
1942.157137	306079.394748	37.605965
1944.310331	306705.534558	37.610983
1946.298391	307327.939316	37.616000
1947.920333	307954.846027	37.621018
1950.147171	308580.298427	37.626036
1952.085975	309219.101919	37.631053
1953.699735	309850.515188	37.636071
1955.676935	310495.980306	37.641088
1957.380818	311144.762510	37.646106
1959.244624	311790.489895	37.651124
1961.013057	312444.379304	37.656141
1962.811079	313092.442746	37.661159
1964.645100	313747.121836	37.666176
1966.524561	314420.552502	37.671194
1968.825355	315077.374103	37.676212
1971.188392	315734.382033	37.681229
1973.476009	316385.175547	37.686247
1976.029749	317032.870330	37.691264
1978.218895	317684.455411	37.696282
1980.191964	318332.059264	37.701300
1982.079159	318977.056186	37.706317
1984.045456	319627.086029	37.711335
1986.578049	320268.151174	37.716352
1988.494337	320911.092650	37.721370
1990.639856	321556.400489	37.726388
1993.297106	322200.903283	37.731405
1995.698098	322826.121730	37.736423
1997.993393	323437.286208	37.741440
1999.697695	324057.914239	37.746458
2002.178766	324650.196045	37.751476
2003.846213	325239.412189	37.756493
2005.601124	325819.543900	37.761511
2007.692785	326399.688489	37.766528
2009.516602	327000.361146	37.771546
2011.526536	327587.971923	37.776564
2013.049309	328187.439743	37.781581
2015.048324	328788.038408	37.786599
2017.145447	329383.181149	37.791616
2018.687122	329999.889576	37.796634
2020.826918	330609.964625	37.801652
2023.008762	331215.989376	37.806669
2024.468750	331838.250775	37.811687
2026.244592	332461.745688	37.816704
2028.176321	333097.467725	37.821722
2029.452424	333725.628113	37.826740
2031.186963	334377.437144	37.831757
2032.558022	335043.439222	37.836775
2034.536737	335713.187214	37.841792
2035.875205	336403.393565	37.846810
2037.658963	337086.001058	37.851828
2040.263005	337789.069925	37.856845
2042.153449	338486.539953	37.861863
2044.483678	339176.386548	37.866880
2046.634145	339888.793232	37.871898
2048.160621	340592.108228	37.876916
2050.664153	341301.768886	37.881933
2053.002752	342006.828034	37.886951
2055.554404	342699.937026	37.891968
2057.688749	343404.934267	37.896986
2059.864517	344091.716773	37.902004
2062.195434	344797.496973	37.907021
2064.416724	345502.143120	37.912039
2067.252724	346184.619573	37.917056
2069.480270	346875.869111	37.922074
2071.986498	347555.589772	37.927092
2074.988542	348230.723594	37.932109
2077.228027	348893.720586	37.937127
2079.576964	349547.248895	37.942144
2081.652236	350221.140486	37.947162
2083.654864	350876.991999	37.952180
2085.615851	351544.361069	37.957197
2088.161651	352200.175711	37.962215
2089.995937	352853.133132	37.967232
2091.984151	353513.539534	37.972250
2093.998658	354173.804216	37.977268
2096.004865	354836.495731	37.982285
2098.003786	355506.713665	37.987303
2099.785590	356161.886594	37.992320
2101.657363	356849.738245	37.997338
2103.467371	357524.725424	38.002356
2105.601227	358211.748018	38.007373
2107.198090	358893.370597	38.012391
2108.836209	359587.126858	38.017408
2111.360770	360262.199387	38.022426
2113.779727	360928.703518	38.027444
2115.558951	361592.819512	38.032461
2117.118367	362258.382382	38.037479
2119.513793	362928.813721	38.042496
2121.127725	363610.909269	38.047514
2123.246365	364284.687328	38.052532
2125.708432	364969.074093	38.057549
2127.067704	365660.003922	38.062567
2128.998105	366343.162845	38.067584
2131.088427	367051.951620	38.072602
2132.526600	367752.924455	38.077620
2134.769947	368476.472713	38.082637
2136.044248	369204.205156	38.087655
2138.254105	369939.904647	38.092672
2140.027286	370686.392232	38.097690
2141.891157	371438.124075	38.102708
2144.021063	372193.294434	38.107725
2145.794025	372967.276939	38.112743
2148.014194	373739.415996	38.117760
2149.935973	374521.124320	38.122778
2152.449260	375300.761147	38.127796
2154.873243	376082.221379	38.132813
2157.694058	376868.616800	38.137831
2159.955306	377640.508943	38.142848
2162.037770	378439.850387	38.147866
2164.179222	379227.422564	38.152884
2166.220537	380010.860176	38.157901
2168.287705	380808.930156	38.162919
2170.842889	381607.226886	38.167936
2173.098728	382396.250288	38.172954
2175.306269	383191.322200	38.177972
2177.818007	383991.697252	38.182989
2179.957384	384801.927227	38.188007
2182.122878	385583.814390	38.193024
2184.564258	386388.983217	38.198042
2186.676451	387180.016862	38.203060
2189.039280	387985.158025	38.208077
2191.334837	388785.904399	38.213095
2193.741815	389586.788340	38.218112
2196.139574	390380.656954	38.223130
2198.450791	391171.148502	38.228148
2201.172543	391963.627594	38.233165
2202.846158	392756.771911	38.238183
2205.119394	393546.371095	38.243200
2207.176630	394347.999420	38.248218
2209.154625	395150.709315	38.253236
2211.751366	395941.354975	38.258253
2213.853704	396759.027862	38.263271
2215.694834	397570.716442	38.268288
2217.870407	398384.098869	38.273306
2220.340466	399185.396700	38.278324
2222.096573	399990.823040	38.283341
2224.147318	400817.942009	38.288359
2226.640864	401632.266743	38.293376
2228.936580	402439.963317	38.298394
2231.057119	403224.027566	38.303412
2233.421340	404008.712048	38.308429
2235.947444	404791.471738	38.313447
2238.699679	405565.354104	38.318464
2240.358242	406350.522924	38.323482
2242.571013	407129.089087	38.328500
2245.377921	407902.794124	38.333517
2246.927204	408689.585532	38.338535
2249.248043	409473.055547	38.343552
2251.342568	410259.631400	38.348570
2253.410891	411070.732211	38.353588
2255.804141	411864.706522	38.358605
2257.806813	412666.853648	38.363623
2260.004702	413480.744939	38.368640
2262.692497	414279.964479	38.373658
2264.781699	415096.330702	38.378676
2267.262606	415903.132651	38.383693
2269.116651	416733.263227	38.388711
2271.190529	417547.578336	38.393728
2273.850396	418370.021915	38.398746
2275.734374	419197.888600	38.403764
2277.825579	420028.730837	38.408781
2279.876939	420870.743242	38.413799
2281.925462	421723.589062	38.418816
2284.169408	422584.676049	38.423834
2285.788879	423455.156003	38.428852
2287.912799	424319.493421	38.433869
2289.923387	425206.855843	38.438887
2293.047870	426088.628579	38.443904
2295.674367	426961.999424	38.448922
2297.697806	427834.783213	38.453940
2300.486379	428711.301959	38.458957
2302.914012	429596.151533	38.463975
2305.390803	430456.662464	38.468992
2307.910025	431354.236312	38.474010
2310.216930	432227.111829	38.479028
2312.540140	433102.735252	38.484045
2314.374437	433994.806744	38.489063
2316.829183	434880.310046	38.494080
2319.083275	435773.657205	38.499098
2321.592854	436666.166339	38.504116
2323.838217	437562.986476	38.509133
2326.287375	438456.750418	38.514151
2328.354138	439356.565114	38.519168
2330.817761	440258.046329	38.524186
2332.983829	441166.675390	38.529204
2335.271221	442065.127615	38.534221
2337.954662	442983.205395	38.539239
2340.128660	443887.470311	38.544256
2342.212820	444802.942870	38.549274
2344.628150	445708.152506	38.554292
2347.363754	446621.412780	38.559309
2349.949076	447536.176976	38.564327
2352.980041	448424.677004	38.569344
2355.726346	449310.153749	38.574362
2358.197146	450180.013133	38.579380
2360.703989	451025.808871	38.584397
2363.018102	451864.118949	38.589415
2365.756988	452719.818694	38.594432
2368.398844	453557.751225	38.599450
2370.314496	454404.875017	38.604468
2372.738102	455246.315203	38.609485
2375.213266	456090.441964	38.614503
2377.502650	456932.088054	38.619520
2379.922455	457783.383209	38.624538
2381.443022	458642.985481	38.629556
2383.679173	459495.098748	38.634573
2385.505684	460362.056136	38.639591
2387.577432	461241.418505	38.644608
2390.068310	462128.655937	38.649626
2391.759905	463026.047630	38.654644
2394.154102	463931.162139	38.659661
2396.485645	464842.259145	38.664679
2398.614207	465759.866940	38.669696
2400.844096	466686.155779	38.674714
2402.880881	467628.299131	38.679732
2405.280418	468563.108796	38.684749
2407.546085	469507.697145	38.689767
2409.922314	470465.961409	38.694784
2412.481657	471418.790713	38.699802
2414.457476	472384.856216	38.704820
2417.119474	473351.916358	38.709837
2420.005712	474324.393647	38.714855
2422.366829	475305.597107	38.719872
2424.802083	476275.573931	38.724890
2427.243472	477255.952609	38.729908
2430.534928	478217.953270	38.734925
2433.049719	479192.054266	38.739943
2435.699612	480167.342164	38.744960
2438.396291	481139.135845	38.749978
2440.870559	482111.621788	38.754996
2443.561715	483062.106479	38.760013
2446.236055	484021.125575	38.765031
2448.977856	484978.415346	38.770048
2452.011429	485931.817401	38.775066
2454.709809	486873.817439	38.780084
2457.233181	487817.159432	38.785101
2459.756462	488771.907141	38.790119
2462.123929	489720.471874	38.795136
2464.501697	490656.416994	38.800154
2466.716787	491617.166360	38.805172
2468.940380	492560.552854	38.810189
2471.330307	493521.266237	38.815207
2473.402882	494480.112742	38.820224
2476.302943	495430.489550	38.825242
2478.479213	496391.984529	38.830260
2481.331976	497348.819183	38.835277
2484.004314	498310.623635	38.840295
2486.638213	499266.830745	38.845312
2489.195918	500217.699887	38.850330
2491.641670	501141.148026	38.855348
2493.928133	502049.997055	38.860365
2496.894034	502975.623281	38.865383
2498.798989	503888.620778	38.870400
2501.210248	504812.371639	38.875418
2503.295754	505745.755530	38.880436
2505.607584	506675.719242	38.885453
2508.044144	507609.691280	38.890471
2510.204064	508557.720579	38.895488
2512.410839	509502.156968	38.900506
2514.816526	510467.370584	38.905524
2517.578604	511425.559409	38.910541
2519.968618	512394.387542	38.915559
2522.716942	513352.814029	38.920576
2525.303652	514322.194801	38.925594
2528.108068	515289.764787	38.930612
2530.987320	516255.850809	38.935629
2533.731576	517231.018704	38.940647
2536.186882	518192.269493	38.945664
2539.187927	519156.993818	38.950682
2541.775578	520122.533801	38.955700
2544.389853	521090.173845	38.960717
2547.120898	522061.610365	38.965735
2549.136105	523041.517366	38.970752
2551.674951	524027.918549	38.975770
2553.592876	525013.001269	38.980788
2555.911784	526008.977814	38.985805
2558.408892	527005.108933	38.990823
2560.769530	528015.746491	38.995840
2564.112464	529013.259142	39.000858
2566.737071	530028.445664	39.005876
2569.643279	531028.211497	39.010893
2572.376667	532038.155831	39.015911
2574.781086	533036.107837	39.020928
2578.120644	534031.314939	39.025946
2580.142442	535044.240950	39.030964
2582.936189	536051.227303	39.035981
2585.999529	537041.392108	39.040999
2588.385255	538050.370139	39.046016
2591.646660	539035.934864	39.051034
2594.428047	540026.794931	39.056052
2597.307084	541010.224725	39.061069
2600.021499	541995.424503	39.066087
2602.992425	542973.922593	39.071104
2606.192342	543954.475376	39.076122
2608.217063	544935.763220	39.081140
2610.490121	545918.497881	39.086157
2613.367990	546896.282629	39.091175
2615.490463	547887.148425	39.096192
2617.863987	548872.771876	39.101210
2620.230180	549888.084528	39.106228
2622.309652	550889.245934	39.111245
2624.786740	551920.321666	39.116263
2626.683464	552936.089351	39.121280
2629.213967	553945.641637	39.126298
2631.593538	554952.882453	39.131316
2634.030940	555955.063089	39.136333
2636.644680	556963.770126	39.141351
2638.544957	557972.019989	39.146368
2641.130937	558989.318950	39.151386
2643.145780	560022.710735	39.156404
2645.256104	561060.575476	39.161421
2648.265855	562109.504256	39.166439
2650.162047	563159.643673	39.171456
2653.070599	564215.751772	39.176474
2655.488665	565296.611125	39.181492
2657.651716	566393.790566	39.186509
2660.178452	567484.739721	39.191527
2662.588432	568600.162299	39.196544
2665.156174	569710.190046	39.201562
2668.114635	570832.199603	39.206580
2670.706466	571951.060860	39.211597
2673.625903	573083.666531	39.216615
2675.867608	574223.159783	39.221632
2679.358219	575362.335822	39.226650
2682.080906	576501.288058	39.231668
2684.796115	577638.180767	39.236685
2687.464673	578777.133645	39.241703
2689.884375	579924.148346	39.246720
2692.966896	581063.119633	39.251738
2695.578115	582232.200961	39.256756
2698.256497	583388.473785	39.261773
2700.911446	584551.909693	39.266791
2704.263626	585712.758480	39.271808
2707.385575	586862.708079	39.276826
2710.281718	588025.416335	39.281844
2713.138873	589179.548972	39.286861
2715.997834	590328.608693	39.291879
2718.701231	591498.026045	39.296896
2721.773270	592640.461869	39.301914
2724.549580	593803.426014	39.306932
2727.277749	594959.320769	39.311949
2729.932590	596111.207229	39.316967
2732.221589	597284.676443	39.321984
2735.612144	598443.067017	39.327002
2737.815497	599613.711131	39.332020
2740.781395	600784.756879	39.337037
2743.751950	601940.564647	39.342055
2746.281328	603114.900910	39.347072
2749.425754	604275.447976	39.352090
2752.187147	605452.706402	39.357108
2755.150063	606621.801830	39.362125
2757.932390	607787.204522	39.367143
2760.618170	608953.853580	39.372160
2763.330235	610111.972793	39.377178
2766.363916	611288.673335	39.382196
2768.690268	612462.869563	39.387213
2771.682215	613626.126192	39.392231
2774.547206	614801.432263	39.397248
2777.261727	615960.039758	39.402266
2780.004099	617098.323717	39.407284
2782.933539	618222.761013	39.412301
2785.860008	619353.430214	39.417319
2788.438170	620473.896095	39.422336
2791.302622	621600.543199	39.427354
2794.210516	622726.815288	39.432372
2797.003004	623857.685224	39.437389
2800.509288	624955.343807	39.442407
2803.468506	626083.501987	39.447424
2806.289560	627194.483263	39.452442
2809.159025	628318.373880	39.457460
2811.546770	629439.031528	39.462477
2814.254566	630558.666511	39.467495
2816.654001	631695.258448	39.472512
2819.479988	632838.892093	39.477530
2822.259754	633977.866272	39.482548
2824.707280	635134.189730	39.487565
2827.574051	636294.354500	39.492583
2830.104413	637467.768382	39.497600
2832.714283	638637.542679	39.502618
2835.758648	639817.036209	39.507636
2838.632530	641000.313264	39.512653
2841.923463	642175.551773	39.517671
2844.356332	643368.353766	39.522688
2847.541726	644549.568381	39.527706
2850.275551	645746.425983	39.532724
2853.027791	646927.834497	39.537741
2856.401639	648112.984973	39.542759
2859.302036	649324.788141	39.547776
2862.491321	650522.142921	39.552794
2864.886546	651728.058671	39.557812
2867.584476	652932.729493	39.562829
2870.685950	654134.643721	39.567847
2873.467246	655344.285165	39.572864
2876.298645	656562.682818	39.577882
2878.832373	657782.323636	39.582900
2881.666270	659011.767541	39.587917
2884.655456	660243.169581	39.592935
2887.401636	661475.600998	39.597952
2890.027025	662717.102464	39.602970
2892.658452	663969.389916	39.607988
2895.370170	665219.509485	39.613005
2898.468831	666475.219624	39.618023
2900.952326	667741.115747	39.623040
2903.739942	669011.217140	39.628058
2906.485588	670291.001037	39.633076
2909.277560	671571.945351	39.638093
2912.569283	672853.225805	39.643111
2915.246430	674137.219116	39.648128
2918.657584	675423.245906	39.653146
2921.630570	676704.647038	39.658164
2924.515573	677999.400619	39.663181
2927.801716	679281.284872	39.668199
2930.626313	680574.394597	39.673216
2933.625420	681841.067816	39.678234
2936.798460	683081.215680	39.683252
2939.792796	684324.104789	39.688269
2942.693267	685552.144143	39.693287
2945.480980	686797.856450	39.698304
2948.100520	688030.967345	39.703322
2950.889654	689266.907070	39.708340
2953.722188	690534.821771	39.713357
2956.910887	691786.520368	39.718375
2959.199921	693056.351777	39.723392
2962.121544	694311.956233	39.728410
2964.981102	695593.031180	39.733428
2967.847974	696879.075150	39.738445
2971.002705	698153.826024	39.743463
2973.887342	699449.950124	39.748480
2976.752886	700731.165067	39.753498
2979.570282	702045.400577	39.758516
2982.820729	703351.683029	39.763533
2985.843473	704635.266455	39.768551
2988.842948	705948.034658	39.773568
2991.740090	707261.015621	39.778586
2994.959143	708568.144625	39.783604
2998.032611	709886.336474	39.788621
3001.618505	711205.968764	39.793639
3004.764145	712533.884385	39.798656
3007.449935	713863.599512	39.803674
3010.507452	715197.642364	39.808692
3013.005640	716527.907709	39.813709
3015.812572	717873.291185	39.818727
3018.472550	719229.807340	39.823744
3021.245582	720584.104713	39.828762
3024.291924	721957.760395	39.833780
3027.129793	723337.104923	39.838797
3029.986696	724708.554497	39.843815
3033.083327	726088.084236	39.848832
3036.698110	727477.815443	39.853850
3040.195707	728864.859495	39.858868
3043.195755	730255.652854	39.863885
3046.202516	731625.318571	39.868903
3049.381055	733015.210760	39.873920
3051.927419	734407.932023	39.878938
3055.179183	735797.181229	39.883956
3058.093617	737199.075622	39.888973
3061.326979	738608.315372	39.893991
3064.357906	740015.661931	39.899008
3067.420410	741420.878213	39.904026
3070.708501	742836.160027	39.909044
3073.211115	744258.764985	39.914061
3076.799107	745668.060744	39.919079
3079.969742	747085.156631	39.924096
3082.850433	748509.138839	39.929114
3085.734818	749925.025476	39.934132
3088.761536	751348.164039	39.939149
3091.815014	752777.781381	39.944167
3094.915215	754214.903510	39.949184
3097.926355	755638.872883	39.954202
3100.759676	757029.433081	39.959220
3103.516444	758429.888752	39.964237
3106.622937	759820.480595	39.969255
3109.854958	761218.419225	39.974272
3111.894783	762634.646382	39.979290
3115.368175	764039.788962	39.984308
3118.417343	765464.601637	39.989325
3121.667248	766884.142787	39.994343
3125.094443	768317.339141	39.999360
3127.829002	769748.410651	40.004378
3130.676701	771177.907819	40.009396
3133.865166	772624.897773	40.014413
3136.716036	774072.297904	40.019431
3140.116158	775515.880572	40.024448
3143.145537	776978.482070	40.029466
3146.443650	778439.712157	40.034484
3149.107042	779912.580325	40.039501
3152.495862	781389.782076	40.044519
3155.464757	782868.909740	40.049536
3158.582096	784360.799095	40.054554
3162.044508	785846.826690	40.059572
3164.886923	787353.383184	40.064589
3168.160398	788854.155314	40.069607
3171.575175	790368.449951	40.074624
3174.803064	791871.429399	40.079642
3178.413506	793374.070595	40.084660
3181.240391	794899.878071	40.089677
3184.293655	796414.592433	40.094695
3187.648836	797944.586304	40.099712
3190.983795	799458.098469	40.104730
3194.928978	800971.565892	40.109748
3197.611710	802505.506603	40.114765
3201.597178	804015.948492	40.119783
3205.122922	805537.281311	40.124800
3208.520350	807057.269832	40.129818
3211.847529	808572.678739	40.134836
3214.909625	810092.483577	40.139853
3218.196305	811614.105585	40.144871
3221.495071	813144.610449	40.149888
3224.201239	814675.940991	40.154906
3227.467905	816197.306823	40.159924
3230.708664	817730.675501	40.164941
3233.796129	819262.349969	40.169959
3236.937468	820794.684839	40.174976
3240.148831	822342.012483	40.179994
3243.075482	823876.446036	40.185012
3246.373523	825438.775666	40.190029
3249.708736	826991.222684	40.195047
3253.255343	828534.591309	40.200064
3256.698970	830085.452007	40.205082
3260.274508	831625.399945	40.210100
3263.269113	833184.162918	40.215117
3266.606894	834724.626508	40.220135
3270.046936	836277.256196	40.225152
3273.082546	837810.798971	40.230170
3276.309736	839322.587885	40.235188
3279.284281	840829.537344	40.240205
3282.296161	842324.065025	40.245223
3285.422454	843829.299932	40.250240
3288.138939	845354.166058	40.255258
3291.593067	846869.110755	40.260276
3294.441857	848401.177878	40.265293
3297.273284	849935.201377	40.270311
3301.016918	851478.980737	40.275328
3303.670757	853019.745922	40.280346
3306.972008	854584.662543	40.285364
3309.820312	856151.974188	40.290381
3313.038243	857733.466505	40.295399
3316.450268	859312.964590	40.300416
3319.442567	860906.470728	40.305434
3322.565777	862503.024611	40.310452
3325.946908	864118.005173	40.315469
3329.365136	865735.645986	40.320487
3332.742012	867346.273595	40.325504
3336.515806	868973.244219	40.330522
3340.154508	870591.374456	40.335540
3343.464501	872212.119836	40.340557
3346.724471	873847.132955	40.345575
3350.636318	875473.749691	40.350592
3353.349632	877123.903059	40.355610
3356.931138	878753.438821	40.360628
3360.665135	880407.905163	40.365645
3363.762386	882060.465294	40.370663
3367.125478	883698.025710	40.375680
3370.431802	885364.962363	40.380698
3374.103203	887019.291983	40.385716
3377.275674	888679.502343	40.390733
3380.975308	890340.974743	40.395751
3384.679931	892003.216884	40.400768
3387.741753	893661.806359	40.405786
3391.309502	895314.717637	40.410804
3395.109950	896981.075690	40.415821
3398.900858	898656.188983	40.420839
3402.321208	900308.047726	40.425856
3405.645290	901969.157701	40.430874
3408.862696	903626.231691	40.435892
3412.349707	905290.462276	40.440909
3415.789079	906953.913502	40.445927
3419.417393	908620.773995	40.450944
3422.308128	910299.077952	40.455962
3425.804203	911958.991441	40.460980
3429.541620	913642.181326	40.465997
3432.560726	915319.309778	40.471015
3436.018729	916996.230553	40.476032
3439.275985	918675.162271	40.481050
3442.861585	920357.545820	40.486068
3446.064595	922053.662951	40.491085
3449.433040	923741.834331	40.496103
3453.074454	925441.982046	40.501120
3456.189272	927127.570227	40.506125
3459.599386	928759.292929	40.511130
3462.822471	930334.099439	40.516135
3466.199568	931835.761872	40.521140
3469.706292	933269.814194	40.526144
3472.763673	934640.725605	40.531149
3475.736173	935934.769378	40.536154
3478.309140	937152.342935	40.541159
3481.302047	938305.340599	40.546164
3483.873475	939370.565249	40.551168
3486.293939	940385.008169	40.556173
3488.888492	941313.198835	40.561178
3491.394411	942181.280289	40.566183
3493.460623	942978.329479	40.571188
3495.705405	943709.827165	40.576192
3497.973891	944383.199410	40.581197
3500.225745	944983.925158	40.586202
3501.636548	945537.535706	40.591207
3503.568875	946021.322222	40.596212
3505.120224	946463.211578	40.601216
3506.633977	946840.285348	40.606221
3508.292354	947169.176289	40.611226
3509.651955	947455.040487	40.616231
3510.885698	947702.735171	40.621236
3512.421023	947895.928459	40.626240
3513.443305	948051.794961	40.631245
3514.724460	948159.587145	40.636250
3515.724445	948249.057040	40.641255
3516.597401	948296.549869	40.646260
3517.868235	948293.941271	40.651264
3518.692920	948274.762909	40.656269
3519.868551	948226.824481	40.661274
3520.593405	948140.503817	40.666279
3521.519286	948030.229713	40.671284
3522.065875	947891.794375	40.676288
3522.608214	947740.152704	40.681293
3523.441850	947559.752988	40.686298
3523.819402	947355.216899	40.691303
3524.387664	947138.105032	40.696308
3524.956210	946908.448302	40.701312
3525.362541	946658.999834	40.706317
3526.208155	946386.783022	40.711322
3526.830771	946104.349216	40.716327
3526.824824	945801.716157	40.721332
3527.621141	945474.520133	40.726336
3527.622796	945150.214948	40.731341
3528.046617	944802.554637	40.736346
3528.697876	944452.821529	40.741351
3528.902807	944079.874987	40.746356
3529.329491	943697.096938	40.751360
3529.139962	943319.279357	40.756365
3529.790650	942921.945978	40.761370
3529.926864	942524.095213	40.766375
3530.391410	942109.491888	40.771380
3530.480781	941682.083660	40.776384
3530.515512	941261.163648	40.781389
3531.052260	940822.304053	40.786394
3530.893010	940390.424654	40.791399
3530.811875	939934.828155	40.796404
3531.606573	939479.425497	40.801408
3531.406260	939026.261235	40.806413
3531.329459	938561.151435	40.811418
3531.696206	938093.336279	40.816423
3531.310625	937625.511685	40.821428
3532.023521	937153.239224	40.826432
3531.833431	936692.775681	40.831437
3531.891132	936203.654131	40.836442
3532.059443	935714.276157	40.841447
3532.071319	935225.166861	40.846452
3532.435213	934729.909055	40.851456
3532.030913	934246.246719	40.856461
3532.654340	933737.613195	40.861466
3532.192988	933243.795080	40.866471
3532.259625	932738.517985	40.871476
3532.461581	932234.512771	40.876480
3532.415626	931737.411626	40.881485
3532.628047	931216.896203	40.886490
3532.642611	930712.585601	40.891495
3532.574729	930208.432946	40.896500
3532.929143	929681.694138	40.901504
3532.803658	929160.361889	40.906509
3533.102482	928636.313185	40.911514
3533.174392	928113.884099	40.916519
3532.992256	927594.232345	40.921524
3533.480027	927054.051534	40.926528
3533.020127	926526.946584	40.931533
3533.037758	925988.851428	40.936538
3533.384639	925459.773871	40.941543
3532.984634	924926.735405	40.946548
3533.206537	924377.776479	40.951552
3533.235521	923844.749127	40.956557
3533.120274	923292.853066	40.961562
3533.196668	922761.343957	40.966567
3532.960609	922219.932798	40.971572
3533.187244	921678.868851	40.976576
3532.997855	921135.513585	40.981581
3533.163347	920584.926136	40.986586
3533.190116	920049.695263	40.991591
3533.061856	919509.339597	40.996596
3533.214646	918961.955390	41.001600
3533.079309	918415.623268	41.006605
3533.111974	917867.860219	41.011610
3533.022027	917323.815707	41.016615
3533.339150	916772.044154	41.021620
3532.956559	916216.582220	41.026624
3533.084069	915677.051817	41.031629
3533.326087	915123.489318	41.036634
3533.364212	914571.060719	41.041639
3533.088189	914017.859462	41.046644
3533.284536	913455.565707	41.051648
3533.269833	912905.577632	41.056653
3533.070502	912342.273839	41.061658
3533.408847	911795.677756	41.066663
3533.319042	911242.260287	41.071668
3533.534512	910671.295969	41.076672
3533.717676	910104.421219	41.081677
3533.768173	909535.872444	41.086682
3533.674789	908970.855496	41.091687
3533.332171	908400.039921	41.096692
3533.508523	907833.992974	41.101696
3533.847714	907263.521908	41.106701
3533.527977	906687.512279	41.111706
3533.363109	906124.723254	41.116711
3533.358588	905558.667288	41.121716
3533.662380	904982.566913	41.126720
3533.336629	904415.677680	41.131725
3533.473868	903836.207399	41.136730
3533.567550	903258.227881	41.141735
3533.256136	902688.941405	41.146740
3533.511597	902122.877461	41.151744
3533.536194	901548.399517	41.156749
3533.338117	900974.383159	41.161754
3533.625641	900391.827263	41.166759
3533.454669	899820.294246	41.171764
3533.512544	899244.512470	41.176768
3533.150955	898664.494821	41.181773
3533.147858	898083.197362	41.186778
3533.381344	897508.849562	41.191783
3533.117967	896937.522228	41.196788
3533.483988	896356.853034	41.201792
3533.195474	895782.032238	41.206797
3533.702266	895196.969266	41.211802
3533.332956	894619.822075	41.216807
3533.157156	894042.196549	41.221812
3533.376236	893443.182898	41.226816
3533.180071	892877.426398	41.231821
3533.161762	892290.703691	41.236826
3533.353092	891718.675997	41.241831
3533.138369	891128.000139	41.246836
3533.660619	890546.033260	41.251840
3533.414230	889965.685618	41.256845
3533.325819	889378.772296	41.261850
3533.125490	888790.850707	41.266855
3533.073253	888208.067204	41.271860
3533.266383	887626.440338	41.276864
3532.820416	887045.637755	41.281869
3533.171161	886456.028615	41.286874
3533.422467	885870.730929	41.291879
3533.099970	885282.277976	41.296884
3532.986023	884695.762113	41.301888
3532.881263	884114.315731	41.306893
3533.160673	883531.293185	41.311898
3532.963124	882947.034732	41.316903
3532.646628	882365.545873	41.321908
3532.923214	881766.175539	41.326912
3532.901028	881195.171956	41.331917
3533.039221	880594.639245	41.336922
3532.764514	880020.560960	41.341927
3532.365439	879428.330778	41.346932
3532.772772	878837.453158	41.351936
3532.828875	878255.878246	41.356941
3532.848227	877668.437283	41.361946
3533.109683	877078.570082	41.366951
3532.812800	876489.320513	41.371956
3533.261578	875892.614157	41.376960
3532.872307	875308.787612	41.381965
3532.603532	874709.369293	41.386970
3532.863561	874118.720877	41.391975
3532.456220	873542.964930	41.396980
3532.795637	872949.567730	41.401984
3532.651287	872365.602357	41.406989
3532.483805	871778.382180	41.411994
3532.552855	871184.078345	41.416999
3532.168251	870600.077250	41.422004
3532.618706	870020.145817	41.427008
3532.576562	869431.605026	41.432013
3532.252366	868830.728363	41.437018
3532.291266	868249.045009	41.442023
3532.027540	867665.900601	41.447028
3532.384920	867075.409187	41.452032
3532.177248	866495.733315	41.457037
3532.430481	865902.619766	41.462042
3532.199186	865323.708643	41.467047
3532.004671	864739.490968	41.472052
3532.048639	864149.153794	41.477056
3531.798848	863566.191568	41.482061
3532.159120	862982.777426	41.487066
3532.272028	862397.988957	41.492071
3532.135942	861819.210864	41.497076
3532.362217	861220.782951	41.502080
3532.204600	860639.272031	41.507085
3531.975055	860050.525159	41.512090
3532.130366	859463.696865	41.517095
3532.097651	858874.316484	41.522100
3532.223492	858280.088018	41.527104
3531.973230	857694.908610	41.532109
3531.856227	857109.164154	41.537114
3532.475415	856510.595080	41.542119
3532.100018	855918.264782	41.547124
3532.570015	855324.760200	41.552128
3532.349541	854731.121530	41.557133
3532.394528	854136.309984	41.562138
3532.530448	853545.803882	41.567143
3532.007223	852949.612453	41.572148
3531.935367	852345.890108	41.577152
3531.848121	851763.523482	41.582157
3531.809516	851170.970640	41.587162
3532.117617	850577.231067	41.592167
3531.703144	849982.584398	41.597172
3531.975111	849386.303066	41.602176
3531.041300	848802.342117	41.607181
3531.610884	848211.155450	41.612186
3531.472504	847634.252836	41.617191
3531.651491	847054.125808	41.622196
3531.732081	846457.109611	41.627200
3531.422119	845874.034109	41.632205
3531.554635	845291.315873	41.637210
3531.236500	844688.548095	41.642215
3531.030479	844104.802961	41.647220
3531.339503	843519.161419	41.652224
3531.077773	842945.843415	41.657229
3531.570915	842348.365617	41.662234
3531.458614	841766.336974	41.667239
3531.304522	841180.849535	41.672244
3531.479635	840587.939007	41.677248
3531.351721	840000.436491	41.682253
3531.563596	839415.990866	41.687258
3531.036528	838825.034320	41.692263
3530.906027	838244.732996	41.697268
3531.311402	837655.508003	41.702272
3530.634749	837074.168865	41.707277
3531.052946	836482.540607	41.712282
3531.291326	835891.327277	41.717287
3530.827982	835318.085456	41.722292
3530.984409	834723.704269	41.727296
3530.915080	834136.821704	41.732301
3531.045652	833553.462842	41.737306
3530.935910	832973.801489	41.742311
3531.099179	832392.625655	41.747316
3531.125126	831806.734251	41.752320
3530.734398	831221.690678	41.757325
3530.854043	830635.579199	41.762330
3530.911140	830053.234051	41.767335
3530.531048	829465.832181	41.772340
3530.629425	828884.449183	41.777344
3530.966303	828308.004310	41.782349
3530.705044	827717.981539	41.787354
3530.565784	827134.284139	41.792359
3530.608277	826560.323719	41.797364
3530.964617	825966.176905	41.802368
3530.741733	825388.396228	41.807373
3530.835457	824795.409332	41.812378
3530.881191	824204.429611	41.817383
3530.745078	823614.991732	41.822388
3530.892152	823026.283531	41.827392
3530.672456	822443.353958	41.832397
3530.618111	821853.108329	41.837402
3530.802760	821268.685493	41.842407
3530.399136	820682.599688	41.847412
3530.880925	820093.474117	41.852416
3530.560030	819507.416545	41.857421
3530.542781	818922.184561	41.862426
3530.369304	818335.362114	41.867431
3530.274587	817749.012422	41.872436
3530.665819	817158.956274	41.877440
3530.355719	816575.866840	41.882445
3530.261122	815985.740600	41.887450
3530.387681	815400.956710	41.892455
3529.976761	814821.695102	41.897460
3530.496273	814227.784497	41.902464
3530.085734	813647.295200	41.907469
3530.260457	813065.480680	41.912474
3530.490243	812482.724961	41.917479
3530.132514	811906.678309	41.922484
3530.433245	811317.247938	41.927488
3530.119567	810736.000583	41.932493
3530.183191	810143.471536	41.937498
3530.127406	809561.001319	41.942503
3529.882348	808981.844307	41.947508
3530.057249	808403.692802	41.952512
3530.022965	807812.543834	41.957517
3530.070709	807228.042296	41.962522
3530.174122	806652.154635	41.967527
3529.696068	806066.956893	41.972532
3529.954019	805492.267866	41.977536
3529.866792	804913.913070	41.982541
3529.900509	804329.066897	41.987546
3529.854142	803741.831131	41.992551
3529.513778	803175.187316	41.997556
3529.804682	802581.665820	42.002560
3529.773411	802006.586000	42.007565
3529.481273	801427.432106	42.012570
3529.479005	800846.708564	42.017575
3529.188201	800272.410787	42.022580
3529.226315	799692.367817	42.027584
3529.058488	799132.719298	42.032589
3529.295909	798552.154062	42.037594
3529.644418	797983.296971	42.042599
3529.123424	797409.192976	42.047604
3529.205874	796837.588424	42.052608
3529.035362	796274.814044	42.057613
3529.044686	795695.520931	42.062618
3529.305364	795131.107960	42.067623
3528.845806	794556.561508	42.072628
3528.944628	793982.412456	42.077632
3529.034245	793421.228797	42.082637
3529.083913	792842.673916	42.087642
3528.892634	792268.826573	42.092647
3528.876653	791706.934326	42.097652
3529.213478	791130.251790	42.102656
3529.072674	790559.792380	42.107661
3529.360808	789991.424010	42.112666
3529.203749	789410.902557	42.117671
3529.128749	788842.208822	42.122676
3528.886353	788260.723045	42.127680
3528.907315	787698.504910	42.132685
3528.720859	787124.237795	42.137690
3528.741704	786554.999972	42.142695
3528.639597	785984.508770	42.147700
3528.919616	785412.726876	42.152704
3528.546831	784851.087846	42.157709
3528.822994	784285.803308	42.162714
3528.714569	783718.671377	42.167719
3528.596401	783150.266871	42.172724
3528.767915	782575.965313	42.177728
3528.490128	782012.120003	42.182733
3528.461204	781450.548580	42.187738
3528.653955	780879.747019	42.192743
3528.290382	780318.242631	42.197748
3528.642740	779744.864385	42.202752
3528.690060	779180.692389	42.207757
3528.512172	778613.759531	42.212762
3528.432434	778050.308159	42.217767
3528.306045	777483.573154	42.222772
3528.540195	776917.470459	42.227776
3528.064702	776355.037500	42.232781
3528.339647	775781.456918	42.237786
3528.363106	775212.205719	42.242791
3527.929040	774657.707091	42.247796
3528.105520	774101.092832	42.252800
3528.343201	773536.843553	42.257805
3528.128443	772976.370104	42.262810
3527.892933	772405.122454	42.267815
3528.014826	771844.160215	42.272820
3527.935005	771278.560048	42.277824
3527.709774	770731.017269	42.282829
3527.929103	770166.758132	42.287834
3527.672605	769619.138005	42.292839
3527.758259	769063.339396	42.297844
3527.797862	768493.859454	42.302848
3527.632916	767941.714422	42.307853
3527.610309	767392.854678	42.312858
3527.493717	766838.795996	42.317863
3527.683743	766292.430361	42.322868
3527.820634	765731.986890	42.327872
3527.326973	765182.403494	42.332877
3527.322981	764623.675123	42.337882
3527.643388	764069.582131	42.342887
3527.405446	763516.775904	42.347892
3527.716400	762959.989310	42.352896
3527.470716	762414.005677	42.357901
3527.331404	761862.638389	42.362906
3527.258528	761310.430211	42.367911
3527.251721	760753.682101	42.372916
3527.176840	760203.859019	42.377920
3527.152307	759661.534238	42.382925
3526.991656	759108.143709	42.387930
3527.018955	758559.613963	42.392935
3527.186786	758016.447590	42.397940
3527.108628	757469.633024	42.402944
3527.073049	756917.541227	42.407949
3526.953570	756369.519522	42.412954
3526.976022	755827.356303	42.417959
3526.935768	755282.351927	42.422964
3527.069049	754730.664873	42.427968
3526.734155	754197.479401	42.432973
3526.883426	753647.093492	42.437978
3526.803576	753104.161892	42.442983
3526.709579	752567.612700	42.447988
3526.879416	752014.538615	42.452992
3526.594365	751476.859512	42.457997
3526.740173	750933.686475	42.463002
3526.682585	750390.411073	42.468007
3526.496429	749855.071168	42.473012
3526.828699	749304.935699	42.478016
3526.670815	748772.578358	42.483021
3526.151410	748228.044161	42.488026
3526.507321	747693.795920	42.493031
3526.437521	747157.903720	42.498036
3526.275269	746617.444532	42.503040
3526.523177	746081.572124	42.508045
3526.350397	745549.539826	42.513050
3526.202889	745001.800427	42.518055
3526.278054	744474.693460	42.523060
3526.508066	743938.775793	42.528064
3526.297917	743409.372066	42.533069
3526.276189	742860.868089	42.538074
3526.472148	742326.477329	42.543079
3526.302954	741794.584631	42.548084
3526.452680	741251.377567	42.553088
3526.350225	740731.268358	42.558093
3525.885691	740184.136755	42.563098
3525.640141	739654.387403	42.568103
3525.549376	739128.681146	42.573108
3525.967380	738599.835979	42.578112
3525.621811	738073.064474	42.583117
3525.677849	737549.751126	42.588122
3525.685201	737024.284364	42.593127
3525.460525	736502.186768	42.598132
3525.822020	735974.858679	42.603136
3525.596713	735450.119435	42.608141
3525.651370	734917.776310	42.613146
3525.679631	734399.902085	42.618151
3525.603069	733877.558095	42.623156
3525.679136	733341.246210	42.628160
3525.651352	732824.517120	42.633165
3525.589182	732301.969129	42.638170
3525.698114	731766.586050	42.643175
3525.558360	731243.784607	42.648180
3525.476033	730720.691922	42.653184
3525.316832	730195.944539	42.658189
3525.198636	729671.898848	42.663194
3525.430031	729156.475022	42.668199
3525.354577	728633.444296	42.673204
3525.519638	728108.902551	42.678208
3525.539317	727596.189256	42.683213
3525.346509	727077.536052	42.688218
3525.547496	726557.791890	42.693223
3525.489693	726036.820331	42.698228
3525.452643	725507.637594	42.703232
3525.203877	724997.531587	42.708237
3525.615239	724456.164877	42.713242
3525.679780	723933.403428	42.718247
3525.312959	723410.087677	42.723252
3525.400926	722889.138846	42.728256
3525.140521	722368.860805	42.733261
3525.022087	721847.484831	42.738266
3525.357754	721320.347740	42.743271
3525.304752	720804.545386	42.748276
3525.372447	720274.066131	42.753280
3525.028207	719760.727117	42.758285
3524.731619	719235.399514	42.763290
3524.943553	718718.380916	42.768295
3524.492557	718209.079546	42.773300
3524.838546	717691.825515	42.778304
3524.824675	717182.188376	42.783309
3524.670936	716664.906384	42.788314
3524.738386	716153.456760	42.793319
3524.442923	715638.218554	42.798324
3524.706458	715135.948673	42.803329
3524.341711	714624.578695	42.808333
3524.617810	714118.326825	42.813338
3524.619045	713600.531583	42.818343
3524.441739	713109.477987	42.823348
3524.545304	712590.759742	42.828353
3524.259414	712092.768453	42.833357
3524.359741	711587.138907	42.838362
3524.273490	711077.888168	42.843367
3523.774098	710581.085040	42.848372
3524.227542	710068.554795	42.853377
3524.250712	709571.851548	42.858381
3524.148775	709072.956508	42.863386
3524.143207	708567.115477	42.868391
3524.009842	708069.705968	42.873396
3524.325483	707563.750605	42.878401
3524.235893	707063.494716	42.883405
3523.925503	706557.487392	42.888410
3523.858763	706056.970174	42.893415
3523.714494	705567.908430	42.898420
3524.023431	705062.948705	42.903425
3523.528654	704580.446091	42.908429
3523.563637	704089.084350	42.913434
3523.666818	703582.086172	42.918439
3523.678559	703095.837643	42.923444
3523.983922	702604.146518	42.928449
3523.485266	702115.098388	42.933453
3523.548717	701613.655074	42.938458
3523.477237	701127.856734	42.943463
3523.318081	700633.549499	42.948468
3523.855163	700133.678973	42.953473
3523.701936	699655.912003	42.958477
3523.484004	699166.898462	42.963482
3523.427837	698671.319279	42.968487
3523.373996	698189.230597	42.973492
3523.567396	697690.819619	42.978497
3523.459765	697202.870321	42.983501
3522.936812	696722.520778	42.988506
3522.994066	696231.456979	42.993511
3522.894395	695755.009053	42.998516
3522.980989	695265.626400	43.003521
3522.655637	694792.148046	43.008525
3522.814922	694311.401280	43.013530
3523.291377	693831.071481	43.018535
3523.189925	693353.400206	43.023540
3523.226048	692865.235922	43.028545
3522.655254	692387.045633	43.033549
3522.965116	691898.681976	43.038554
3522.854964	691425.036602	43.043559
3522.608407	690960.442519	43.048564
3522.762221	690480.135769	43.053569
3522.422015	690008.891933	43.058573
3522.278298	689525.251480	43.063578
3522.479837	689065.556874	43.068583
3522.434772	688593.093477	43.073588
3522.498390	688120.536872	43.078593
3522.408126	687665.845951	43.083597
3522.331142	687188.089130	43.088602
3522.249127	686719.265765	43.093607
3522.144528	686253.905690	43.098612
3522.492480	685784.064448	43.103617
3522.213296	685323.115860	43.108621
3522.366123	684859.033640	43.113626
3522.107000	684392.558779	43.118631
3522.139016	683928.300167	43.123636
3522.790812	683456.145637	43.128641
3522.588232	682995.613224	43.133645
3522.485238	682520.302813	43.138650
3522.471079	682048.139124	43.143655
3522.445358	681583.023802	43.148660
3522.547909	681113.978710	43.153665
3522.058481	680648.994594	43.158669
3521.797111	680176.776390	43.163674
3522.300511	679718.099607	43.168679
3521.821402	679253.192308	43.173684
3521.825059	678793.956990	43.178689
3521.725424	678342.686336	43.183693
3521.622359	677878.292886	43.188698
3521.783677	677418.364275	43.193703
3521.540675	676969.691200	43.198708
3521.800571	676520.063509	43.203713
3521.826655	676059.243377	43.208717
3521.392577	675615.768838	43.213722
3521.532098	675154.186768	43.218727
3521.265295	674706.903028	43.223732
3521.761420	674249.102000	43.228737
3521.766433	673811.047782	43.233741
3521.785429	673349.845292	43.238746
3521.648403	672893.730475	43.243751
3521.468411	672446.771999	43.248756
3521.688473	671982.576735	43.253761
3521.559034	671536.563084	43.258765
3520.962218	671088.414555	43.263770
3521.293076	670636.945477	43.268775
3521.079504	670192.776764	43.273780
3521.082022	669746.406285	43.278785
3520.673053	669314.644182	43.283789
3521.116891	668873.242781	43.288794
3521.088400	668431.652064	43.293799
3520.953524	667989.959146	43.298804
3521.264733	667547.321669	43.303809
3521.539667	667092.251540	43.308813
3521.308838	666645.774487	43.313818
3521.029850	666201.928141	43.318823
3520.502646	665765.784848	43.323828
3520.783211	665323.448005	43.328833
3520.610418	664899.625030	43.333837
3520.414740	664457.478985	43.338842
3520.629785	664018.884205	43.343847
3520.317896	663595.126883	43.348852
3520.458464	663156.505304	43.353857
3520.866137	662725.402111	43.358861
3520.363869	662284.205964	43.363866
3520.616084	661850.146091	43.368871
3520.731594	661426.918671	43.373876
3520.539105	660982.565937	43.378881
3520.591398	660561.556999	43.383885
3520.377546	660127.000041	43.388890
3520.825591	659690.014651	43.393895
3520.313494	659267.648217	43.398900
3520.360111	658835.284785	43.403905
3520.368342	658410.046821	43.408909
3520.595311	657973.670754	43.413914
3520.650878	657545.741155	43.418919
3520.310844	657123.751313	43.423924
3520.596916	656683.213556	43.428929
3520.382324	656261.564398	43.433933
3520.384120	655826.778296	43.438938
3520.491661	655398.945403	43.443943
3520.393902	654974.324705	43.448948
3520.350949	654538.640159	43.453953
3520.273922	654112.380625	43.458957
3519.960453	653680.249873	43.463962
3519.939022	653255.142281	43.468967
3519.821910	652840.221620	43.473972
3519.992108	652424.435284	43.478977
3519.772945	652009.397214	43.483981
3519.598141	651593.235197	43.488986
3520.238278	651167.475205	43.493991
3519.642286	650762.340093	43.498996
3519.738759	650333.290029	43.504001
3519.867171	649931.744212	43.509005
3519.797960	649495.941621	43.514010
3519.819625	649077.841924	43.519015
3519.430493	648671.387113	43.524020
3519.851071	648257.032335	43.529025
3519.663631	647850.209839	43.534029
3519.669516	647425.597392	43.539034
3519.581289	647013.376820	43.544039
3519.478607	646604.740111	43.549044
3519.179095	646191.072473	43.554049
3519.313762	645788.559434	43.559053
3519.139153	645378.985481	43.564058
3519.296597	644968.788338	43.569063
3519.001152	644580.696174	43.574068
3519.433545	644165.120773	43.579073
3519.140633	643766.649120	43.584077
3519.159235	643358.759863	43.589082
3518.939290	642950.494942	43.594087
3518.895251	642555.732776	43.599092
3519.002943	642153.529485	43.604097
3518.994494	641760.130291	43.609101
3519.065552	641358.801835	43.614106
3518.854434	640962.356221	43.619111
3518.908835	640568.600236	43.624116
3519.323402	640170.216769	43.629121
3519.096471	639762.075164	43.634125
3518.872408	639369.870864	43.639130
3519.111296	638973.671359	43.644135
3519.141026	638578.042437	43.649140
3519.095391	638170.656769	43.654145
3518.922122	637771.830257	43.659149
3518.629224	637365.505330	43.664154
3519.271307	636965.557951	43.669159
3519.174336	636573.475331	43.674164
3519.275331	636164.084257	43.679169
3518.917760	635769.063919	43.684173
3518.929044	635375.216327	43.689178
3519.139349	634961.806481	43.694183
3518.782261	634558.534287	43.699188
3518.709051	634152.045563	43.704193
3518.624008	633758.253118	43.709197
3518.805541	633363.249296	43.714202
3518.890051	632972.951175	43.719207
3518.540723	632582.462291	43.724212
3518.852741	632174.579501	43.729217
3518.799055	631793.469633	43.734221
3518.058267	631392.893160	43.739226
3518.389792	631001.578340	43.744231
3517.712502	630617.328749	43.749236
3518.252286	630232.356735	43.754241
3518.154921	629857.240840	43.759245
3518.068619	629474.850928	43.764250
3518.531629	629090.400926	43.769255
3518.126940	628707.586980	43.774260
3518.766662	628313.816673	43.779265
3518.614827	627932.583651	43.784269
3518.347347	627545.348294	43.789274
3518.469589	627154.477175	43.794279
3518.158683	626763.365165	43.799284
3518.593796	626391.740803	43.804289
3518.117270	626001.981065	43.809293
3518.275332	625618.007989	43.814298
3518.532873	625232.802163	43.819303
3518.027869	624856.426928	43.824308
3518.087588	624463.464364	43.829313
3517.935030	624085.298931	43.834317
3517.801735	623702.809311	43.839322
3517.793806	623322.388388	43.844327
3517.844560	622950.860181	43.849332
3517.511766	622567.412401	43.854337
3517.422342	622207.103217	43.859341
3517.599810	621838.871286	43.864346
3517.740582	621460.162545	43.869351
3517.284107	621094.017326	43.874356
3517.440367	620728.807207	43.879361
3517.390672	620359.661763	43.884365
3517.016302	619992.112408	43.889370
3517.453431	619628.220133	43.894375
3517.379885	619272.971346	43.899380
3517.485414	618896.634207	43.904385
3517.100538	618542.717546	43.909389
3517.136915	618180.548995	43.914394
3517.142892	617813.412216	43.919399
3517.045316	617462.518524	43.924404
3516.904652	617100.695146	43.929409
3516.993639	616748.443586	43.934413
3516.764932	616392.776543	43.939418
3517.098784	616036.199932	43.944423
3516.753924	615677.271491	43.949428
3517.084093	615322.677304	43.954433
3516.913297	614972.167438	43.959437
3517.054056	614616.379735	43.964442
3517.297389	614256.953579	43.969447
3516.815607	613901.048532	43.974452
3517.226517	613540.567760	43.979457
3517.090097	613193.254179	43.984461
3516.760269	612834.782019	43.989466
3517.171499	612480.684258	43.994471
3516.580532	612127.648823	43.999476
3516.394759	611769.418437	44.004481
3516.164977	611437.309038	44.009485
3515.962052	611095.256323	44.014490
3516.497473	610744.993357	44.019495
3516.572575	610412.149393	44.024500
3516.435510	610064.186383	44.029505
3516.401484	609728.231334	44.034509
3516.371882	609383.940001	44.039514
3516.307400	609035.581490	44.044519
3516.221338	608703.566769	44.049524
3516.296632	608356.367021	44.054529
3516.256437	608015.696958	44.059533
3516.138700	607679.995722	44.064538
3516.301522	607331.996951	44.069543
3516.171289	607002.146613	44.074548
3516.129809	606661.134760	44.079553
3516.093585	606328.188561	44.084557
3515.852972	605995.167101	44.089562
3516.062980	605663.664324	44.094567
3515.695694	605330.243544	44.099572
3516.044792	604991.121461	44.104577
3516.058412	604668.353135	44.109581
3515.891075	604334.868935	44.114586
3515.648896	603995.065399	44.119591
3515.520555	603671.841396	44.124596
3515.667668	603342.740301	44.129601
3515.881953	603024.708337	44.134605
3515.824686	602696.175467	44.139610
3515.972304	602360.421800	44.144615
3515.504829	602046.995588	44.149620
3515.602573	601712.887550	44.154625
3515.413798	601393.574139	44.159629
3515.428377	601075.572243	44.164634
3515.580453	600754.325809	44.169639
3515.380545	600430.620845	44.174644
3515.444352	600112.935240	44.179649
3515.521524	599799.204034	44.184653
3515.585147	599473.620116	44.189658
3515.605828	599147.030368	44.194663
3515.332754	598839.005253	44.199668
3515.261173	598521.700520	44.204673
3515.472689	598192.490951	44.209677
3515.390477	597877.228664	44.214682
3515.838662	597557.398975	44.219687
3515.649433	597235.510409	44.224692
3515.370112	596912.423306	44.229697
3515.350327	596590.889613	44.234701
3515.272977	596274.478369	44.239706
3515.252544	595955.889686	44.244711
3515.151805	595650.713027	44.249716
3514.981811	595327.814359	44.254721
3515.002897	595020.893130	44.259725
3514.739690	594716.573477	44.264730
3514.975691	594399.656181	44.269735
3514.849195	594098.511133	44.274740
3514.925035	593787.128840	44.279745
3514.863445	593480.532923	44.284749
3514.698238	593167.065985	44.289754
3515.000548	592864.811608	44.294759
3514.901019	592565.983270	44.299764
3514.868565	592260.706715	44.304769
3515.104592	591957.486054	44.309773
3514.719942	591652.052966	44.314778
3514.947935	591343.342774	44.319783
3514.804988	591043.579139	44.324788
3514.687652	590726.924744	44.329793
3514.528709	590428.504609	44.334797
3514.574736	590129.589838	44.339802
3514.682276	589826.437019	44.344807
3514.586375	589530.947628	44.349812
3514.618022	589234.524786	44.354817
3514.747636	588919.839938	44.359821
3514.411501	588628.237812	44.364826
3514.530072	588319.166265	44.369831
3514.362011	588028.023228	44.374836
3514.531766	587726.765986	44.379841
3514.743850	587435.945613	44.384845
3514.241979	587135.441391	44.389850
3514.561018	586840.869841	44.394855
3514.102204	586559.841186	44.399860
3514.055639	586251.749530	44.404865
3514.032201	585968.471815	44.409869
3513.953526	585676.653382	44.414874
3514.021100	585390.230666	44.419879
3513.816479	585107.064141	44.424884
3514.003316	584821.461948	44.429889
3513.862341	584536.713141	44.434893
3513.859413	584261.936136	44.439898
3513.935927	583974.724406	44.444903
3513.730419	583695.847585	44.449908
3513.882931	583402.728432	44.454913
3514.005610	583118.504453	44.459917
3514.026749	582841.278355	44.464922
3513.787923	582550.417223	44.469927
3513.521977	582276.444466	44.474932
3513.513688	582002.924264	44.479937
3513.508456	581723.465288	44.484941
3513.334077	581451.067054	44.489946
3513.814379	581170.858980	44.494951
3513.297402	580903.081996	44.499956
3513.705691	580626.342758	44.504961
3513.624238	580344.301154	44.509965
3513.449628	580064.079010	44.514970
3513.769786	579795.933781	44.519975
3513.676661	579526.344823	44.524980
3514.143242	579249.262891	44.529985
3513.921522	578973.700174	44.534989
3513.841820	578687.698128	44.539994
3513.951905	578408.495907	44.544999
3513.708249	578143.277227	44.550004
3513.916798	577855.848936	44.555009
3514.012566	577581.659265	44.560013
3513.955370	577290.994421	44.565018
3514.001723	577009.910746	44.570023
3513.778394	576732.538098	44.575028
3513.842691	576450.432824	44.580033
3513.711887	576181.682582	44.585037
3513.572715	575898.794801	44.590042
3513.626645	575616.370587	44.595047
3513.392950	575362.558439	44.600052
3513.713120	575078.366436	44.605057
3513.779552	574802.510846	44.610061
3513.685423	574532.813354	44.615066
3513.673350	574260.782113	44.620071
3513.355560	573978.384291	44.625076
3513.668859	573702.311365	44.630081
3513.719288	573431.408441	44.635085
3513.320340	573154.891699	44.640090
3513.451981	572882.604771	44.645095
3513.245941	572616.004223	44.650100
3513.459673	572343.289125	44.655105
3512.963300	572075.720490	44.660109
3513.021293	571816.906497	44.665114
3513.065289	571546.265932	44.670119
3512.872339	571290.905304	44.675124
3512.843294	571025.297486	44.680129
3512.826674	570766.374067	44.685133
3512.779602	570513.035797	44.690138
3513.080146	570242.222880	44.695143
3513.154802	569993.482751	44.700148
3513.430993	569730.462604	44.705153
3513.213508	569474.666974	44.710157
3513.444571	569207.416684	44.715162
3513.185132	568938.332222	44.720167
3512.731841	568669.275169	44.725172
3512.884253	568401.165862	44.730177
3513.321806	568144.174817	44.735181
3513.323824	567888.410505	44.740186
3513.077740	567619.044286	44.745191
3512.847183	567370.305042	44.750196
3513.125849	567109.092603	44.755201
3513.349570	566843.807328	44.760205
3512.895996	566578.128873	44.765210
3513.038191	566312.745870	44.770215
3512.769062	566059.004693	44.775220
3513.021326	565793.642514	44.780225
3513.155192	565538.916221	44.785229
3512.543648	565290.201719	44.790234
3512.957708	565034.461191	44.795239
3512.633587	564769.528707	44.800244
3512.692957	564515.499682	44.805249
3512.870046	564265.926015	44.810253
3512.425195	564007.643678	44.815258
3512.570874	563755.296656	44.820263
3511.838602	563511.602931	44.825268
3512.342436	563254.905691	44.830273
3512.182064	563012.011165	44.835277
3512.005604	562772.236414	44.840282
3512.200792	562536.119601	44.845287
3512.148084	562290.021230	44.850292
3512.074936	562050.366588	44.855297
3512.228622	561807.144198	44.860301
3512.253666	561571.441769	44.865306
3512.258560	561321.790612	44.870311
3512.384475	561078.458684	44.875316
3512.292380	560836.116205	44.880321
3512.069818	560596.863248	44.885325
3512.062064	560361.799250	44.890330
3512.402798	560116.750990	44.895335
3511.985899	559875.000132	44.900340
3512.016681	559633.873427	44.905345
3512.018522	559397.027917	44.910349
3511.929251	559160.546232	44.915354
3512.138284	558918.822008	44.920359
3511.758589	558690.691319	44.925364
3511.817951	558444.199405	44.930369
3511.893276	558219.306935	44.935373
3511.820554	557990.456979	44.940378
3511.782167	557749.156509	44.945383
3511.255693	557529.542873	44.950388
3511.479172	557291.765483	44.955393
3511.511367	557070.739262	44.960397
3511.472178	556850.930439	44.965402
3511.803302	556610.956533	44.970407
3511.687291	556384.907044	44.975412
3511.865626	556158.299723	44.980417
3512.008959	555931.744895	44.985421
3511.603062	555710.619728	44.990426
3511.752773	555468.187818	44.995431
3511.557355	555241.124951	45.000436
3511.693263	555011.432397	45.005441
3511.463659	554787.440683	45.010445
3511.578891	554565.854922	45.015450
3511.607387	554337.680510	45.020455
3511.240203	554112.844528	45.025460
3511.358804	553883.538615	45.030465
3511.686671	553664.521497	45.035469
3511.353958	553449.593883	45.040474
3511.326651	553211.786604	45.045479
3511.294090	553000.579384	45.050484
3511.690570	552771.458973	45.055489
3511.547348	552554.922741	45.060493
3511.113511	552337.878383	45.065498
3511.504132	552112.073344	45.070503
3511.431718	551898.789734	45.075508
3511.399903	551670.429197	45.080513
3511.221791	551453.780472	45.085517
3511.066653	551229.464814	45.090522
3511.667828	551010.357920	45.095527
3511.709951	550794.568110	45.100532
3511.690863	550571.125406	45.105537
3511.693917	550343.240481	45.110541
3511.634481	550123.375342	45.115546
3511.973597	549886.001347	45.120551
3511.834439	549672.794900	45.125556
3511.358622	549445.127877	45.130561
3511.752217	549215.796631	45.135565
3511.555338	548996.843952	45.140570
3511.500491	548771.008996	45.145575
3511.063840	548557.583898	45.150580
3511.335525	548334.407663	45.155585
3510.923832	548111.294062	45.160589
3510.769475	547906.731985	45.165594
3511.156868	547696.277806	45.170599
3510.845795	547482.915318	45.175604
3510.600940	547273.217869	45.180609
3511.067443	547061.933955	45.185613
3511.236186	546845.606436	45.190618
3510.891869	546641.410790	45.195623
3510.757029	546431.480082	45.200628
3510.981550	546217.300771	45.205633
3510.659972	546012.991104	45.210637
3510.712094	545810.832720	45.215642
3510.675121	545594.218209	45.220647
3510.582081	545400.094182	45.225652
3510.662159	545194.493909	45.230657
3510.652639	544990.569565	45.235661
3510.600085	544785.137101	45.240666
3510.713798	544588.092705	45.245671
3510.680166	544390.616915	45.250676
3510.762600	544181.774534	45.255681
3510.852330	543980.843453	45.260685
3510.184747	543774.290991	45.265690
3510.845280	543567.912060	45.270695
3510.284735	543371.520148	45.275700
3510.428855	543168.954598	45.280705
3510.740858	542981.484045	45.285709
3510.418562	542782.522054	45.290714
3510.444283	542579.161391	45.295719
3510.267062	542381.126956	45.300724
3510.751993	542179.194794	45.305729
3510.594932	541981.352955	45.310733
3510.157307	541787.741604	45.315738
3510.560619	541583.898596	45.320743
3510.167585	541397.283590	45.325748
3510.452636	541199.960366	45.330753
3510.618982	541004.268369	45.335757
3510.480920	540812.306996	45.340762
3510.466318	540616.085762	45.345767
3510.092288	540420.629195	45.350772
3510.255443	540220.942780	45.355777
3510.271892	540028.036555	45.360781
3510.032267	539839.206075	45.365786
3510.331858	539643.068945	45.370791
3509.984522	539456.874306	45.375796
3510.200284	539259.233122	45.380801
3510.085203	539077.583447	45.385805
3509.994002	538884.276494	45.390810
3510.241927	538699.382476	45.395815
3510.076728	538514.859211	45.400820
3510.096107	538316.532269	45.405825
3509.922486	538136.595441	45.410829
3509.904459	537949.164648	45.415834
3510.081891	537754.333669	45.420839
3509.939166	537570.096932	45.425844
3509.996191	537384.058234	45.430849
3509.790040	537210.571817	45.435853
3509.863984	537026.694595	45.440858
3509.921111	536832.325533	45.445863
3509.760001	536664.827615	45.450868
3509.811115	536474.338936	45.455873
3509.561953	536290.810072	45.460877
3510.021670	536111.698006	45.465882
3509.758822	535932.555727	45.470887
3509.575679	535751.026552	45.475892
3509.246418	535573.101861	45.480897
3509.674355	535397.013191	45.485901
3509.442109	535221.539576	45.490906
3509.525525	535033.447799	45.495911
3509.346725	534869.211166	45.500916
3509.598375	534698.290019	45.505921
3509.751459	534513.862507	45.510925
3509.444456	534354.535741	45.515930
3509.514152	534164.669102	45.520935
3509.256440	534001.949645	45.525940
3509.424827	533814.281515	45.530945
3509.536103	533650.687822	45.535949
3509.319982	533481.850323	45.540954
3509.644951	533300.556660	45.545959
3509.361172	533140.707960	45.550964
3509.323530	532971.228541	45.555969
3509.156615	532800.760048	45.560973
3509.134762	532633.191386	45.565978
3509.815795	532455.560295	45.570983
3509.973653	532292.346972	45.575988
3509.864005	532115.553159	45.580993
3509.512424	531940.716024	45.585997
3509.791692	531752.800408	45.591002
3510.021175	531577.203688	45.596007
3509.344208	531415.334150	45.601012
3509.621924	531233.366718	45.606017
3509.675440	531068.996821	45.611021
3509.106342	530895.748657	45.616026
3509.187893	530720.621056	45.621031
3509.284444	530550.888649	45.626036
3509.481217	530388.555733	45.631041
3509.559617	530221.800126	45.636045
3509.308208	530053.786771	45.641050
3509.417479	529877.534052	45.646055
3509.030682	529713.224085	45.651060
3509.231937	529545.733240	45.656065
3509.451583	529381.770240	45.661069
3508.988423	529221.000690	45.666074
3509.385700	529054.732537	45.671079
3509.182435	528894.217863	45.676084
3509.157380	528724.636486	45.681089
3509.279388	528552.302515	45.686093
3508.913657	528394.989917	45.691098
3509.330251	528227.901553	45.696103
3508.916712	528074.682083	45.701108
3509.246286	527901.446996	45.706113
3508.970188	527743.052162	45.711117
3509.069730	527590.042910	45.716122
3508.930519	527421.425081	45.721127
3508.548797	527269.706123	45.726132
3508.892184	527106.605273	45.731137
3508.897890	526960.722892	45.736141
3508.353023	526796.558809	45.741146
3508.837758	526632.822865	45.746151
3509.012508	526499.930754	45.751156
3508.711317	526334.760836	45.756161
3508.797507	526180.073449	45.761165
3508.132298	526027.229112	45.766170
3508.486744	525866.990190	45.771175
3508.641984	525722.130226	45.776180
3508.432228	525573.746883	45.781185
3508.767082	525429.459201	45.786189
3508.515725	525279.363592	45.791194
3508.855090	525123.662805	45.796199
3508.568455	524979.931247	45.801204
3508.692067	524822.497182	45.806209
3509.068960	524666.179392	45.811213
3508.715187	524514.629483	45.816218
3508.750669	524358.619203	45.821223
3508.280390	524209.307521	45.826228
3508.415667	524064.283418	45.831233
3508.358042	523915.605184	45.836237
3508.083254	523772.566836	45.841242
3508.416295	523626.444462	45.846247
3508.292955	523486.103959	45.851252
3508.201491	523347.170434	45.856257
3507.926975	523203.066311	45.861261
3507.784835	523059.493610	45.866266
3508.262508	522920.509459	45.871271
3508.297221	522792.152556	45.876276
3508.090784	522653.787671	45.881281
3508.131371	522513.915032	45.886285
3507.668355	522382.054594	45.891290
3507.930444	522235.526878	45.896295
3507.907493	522102.982932	45.901300
3507.793409	521970.200908	45.906305
3508.047781	521837.001337	45.911309
3507.821270	521695.045901	45.916314
3508.062268	521565.431437	45.921319
3507.937396	521439.514106	45.926324
3508.067800	521297.948475	45.931329
3507.992887	521165.657671	45.936333
3507.836725	521037.772928	45.941338
3507.845616	520902.435625	45.946343
3508.239519	520764.809419	45.951348
3507.771023	520624.905231	45.956353
3507.829846	520494.353222	45.961357
3507.782366	520368.565282	45.966362
3508.277779	520231.472417	45.971367
3507.673716	520102.090738	45.976372
3507.537732	519968.486894	45.981377
3507.820861	519845.011758	45.986381
3507.577270	519720.110476	45.991386
3508.057697	519581.852764	45.996391
3507.699907	519459.291982	46.001396
3507.815302	519329.023341	46.006401
3507.711058	519205.205133	46.011405
3507.433496	519082.728636	46.016410
3507.660413	518946.326621	46.021415
3507.667158	518830.264213	46.026420
3507.565643	518699.370666	46.031425
3507.771733	518572.615508	46.036429
3507.438275	518449.486898	46.041434
3507.335881	518318.943795	46.046439
3507.655112	518195.701705	46.051444
3507.629701	518073.426612	46.056449
3507.619285	517956.552384	46.061453
3507.266101	517835.846613	46.066458
3507.349714	517710.569995	46.071463
3507.498469	517600.383601	46.076468
3507.211017	517473.602610	46.081473
3507.729065	517357.795325	46.086477
3507.402364	517231.625164	46.091482
3507.624883	517110.714380	46.096487
3507.352927	516983.017498	46.101492
3507.435191	516866.977859	46.106497
3507.295332	516743.499442	46.111501
3507.070372	516631.248400	46.116506
3507.218394	516505.496363	46.121511
3507.176140	516395.990638	46.126516
3507.372278	516276.138598	46.131521
3507.510495	516166.549918	46.136525
3507.073009	516048.016637	46.141530
3507.289455	515927.804827	46.146535
3507.628601	515817.219579	46.151540
3507.563988	515694.831270	46.156545
3507.728657	515566.745030	46.161549
3507.542400	515461.904769	46.166554
3507.582785	515333.130586	46.171559
3507.480267	515218.474083	46.176564
3507.216479	515095.407803	46.181569
3507.741184	514982.915767	46.186573
3507.125771	514866.171952	46.191578
3507.465155	514737.240737	46.196583
3507.467766	514622.864999	46.201588
3507.058153	514503.304757	46.206593
3507.156342	514390.275021	46.211597
3506.927446	514283.665883	46.216602
3507.402385	514168.751478	46.221607
3507.101519	514061.647900	46.226612
3507.275318	513948.501007	46.231617
3507.210818	513837.061201	46.236621
3506.785857	513728.006166	46.241626
3507.204197	513614.158307	46.246631
3506.878943	513507.711881	46.251636
3507.035980	513387.591621	46.256641
3507.003859	513287.257484	46.261645
3507.044389	513181.807380	46.266650
3507.381257	513052.761624	46.271655
3507.117108	512961.963598	46.276660
3507.095779	512844.951631	46.281665
3507.207818	512739.385286	46.286669
3506.915396	512637.474615	46.291674
3507.018163	512517.508523	46.296679
3506.974024	512417.726653	46.301684
3507.032033	512297.564415	46.306689
3507.186503	512188.854458	46.311693
3506.959072	512090.162872	46.316698
3507.097421	511975.795114	46.321703
3506.993189	511863.084846	46.326708
3507.118286	511761.602482	46.331713
3507.032087	511653.940489	46.336717
3506.414902	511550.360229	46.341722
3506.927709	511444.767287	46.346727
3506.776608	511344.542102	46.351732
3507.008164	511236.418761	46.356737
3507.251874	511128.191544	46.361741
3506.956810	511035.518027	46.366746
3507.227083	510916.471213	46.371751
3506.909466	510809.904123	46.376756
3506.992345	510709.281230	46.381761
3506.905384	510608.332970	46.386765
3506.827088	510502.430394	46.391770
3506.803335	510395.305006	46.396775
3506.779343	510296.062119	46.401780
3506.886019	510188.811997	46.406785
3506.793070	510097.917680	46.411789
3506.521102	510000.989307	46.416794
3506.730727	509888.817760	46.421799
3506.710821	509789.924746	46.426804
3506.703792	509687.541991	46.431809
3506.918462	509587.344283	46.436813
3506.433232	509493.430812	46.441818
3506.966449	509382.413295	46.446823
3506.967680	509294.328316	46.451828
3507.175952	509185.841193	46.456833
3507.340810	509082.970362	46.461837
3506.948611	508975.948833	46.466842
3507.162808	508863.061740	46.471847
3506.958949	508765.608817	46.476852
3506.925872	508664.436834	46.481857
3507.142494	508562.918342	46.486861
3506.557167	508455.218744	46.491866
3506.712718	508345.521960	46.496871
3506.435302	508257.832598	46.501876
3506.286673	508157.789002	46.506881
3506.680842	508065.839636	46.511885
3506.504119	507972.723700	46.516890
3506.810962	507885.892809	46.521895
3506.621932	507789.189501	46.526900
3506.498114	507693.080972	46.531905
3506.633213	507583.635157	46.536909
3506.813664	507497.682952	46.541914
3507.038977	507394.437120	46.546919
3506.940961	507297.816387	46.551924
3507.014591	507191.916383	46.556929
3506.707696	507087.748584	46.561933
3506.882774	506994.566889	46.566938
3506.985521	506884.768020	46.571943
3506.471245	506788.114199	46.576948
3506.266849	506690.497083	46.581953
3506.359124	506600.814822	46.586957
3506.563292	506507.372609	46.591962
3506.481649	506416.354293	46.596967
3506.547542	506311.713442	46.601972
3506.602963	506221.630992	46.606977
3506.722617	506126.431882	46.611981
3505.814791	506041.769720	46.616986
3506.200476	505946.321935	46.621991
3506.374304	505856.015035	46.626996
3506.514569	505769.150595	46.632001
3506.413203	505668.780119	46.637005
3506.104129	505579.362887	46.642010
3506.318610	505496.123771	46.647015
3506.204759	505411.727118	46.652020
3506.283357	505322.495014	46.657025
3506.480482	505241.683900	46.662029
3505.949942	505151.695522	46.667034
3506.053176	505063.064373	46.672039
3505.992578	504976.128863	46.677044
3506.065503	504896.146029	46.682049
3506.426926	504819.146574	46.687053
3506.220481	504726.926821	46.692058
3506.538064	504627.742118	46.697063
3506.370718	504550.831670	46.702068
3506.159701	504455.729725	46.707073
3506.310487	504356.521291	46.712077
3506.346464	504284.781717	46.717082
3506.354272	504186.405489	46.722087
3506.167348	504111.366742	46.727092
3506.255132	504032.084846	46.732097
3506.259586	503939.116861	46.737101
3506.061928	503856.799097	46.742106
3506.438071	503767.305413	46.747111
3506.573651	503688.519219	46.752116
3506.172907	503600.016680	46.757121
3506.294238	503507.835143	46.762125
3506.245568	503414.923786	46.767130
3506.239211	503334.087360	46.772135
3506.172451	503244.716981	46.777140
3506.199702	503157.099510	46.782145
3506.239867	503070.187146	46.787149
3506.146144	502991.588401	46.792154
3506.307620	502904.300547	46.797159
3505.863923	502833.799275	46.802164
3505.641608	502748.952284	46.807169
3505.935434	502671.701422	46.812173
3505.700657	502600.506227	46.817178
3505.748818	502520.768725	46.822183
3505.801393	502452.001145	46.827188
3505.597545	502365.986180	46.832193
3505.920090	502289.689215	46.837197
3505.814605	502219.430894	46.842202
3506.171158	502130.841637	46.847207
3505.964651	502065.858027	46.852212
3505.811212	501983.573816	46.857217
3505.909493	501904.734823	46.862221
3505.982054	501822.360655	46.867226
3505.870342	501737.995132	46.872231
3505.699581	501658.088568	46.877236
3505.845028	501584.296014	46.882241
3505.755775	501516.256570	46.887245
3505.719816	501447.247085	46.892250
3506.146772	501360.866333	46.897255
3505.515850	501294.485854	46.902260
3505.634603	501215.690617	46.907265
3505.890210	501145.012106	46.912269
3505.592350	501069.674950	46.917274
3505.937431	500991.598428	46.922279
3505.753142	500921.398564	46.927284
3505.716274	500847.229329	46.932289
3506.287510	500777.000975	46.937293
3506.038796	500695.535585	46.942298
3505.950812	500606.609505	46.947303
3505.917869	500535.320319	46.952308
3505.572880	500454.881451	46.957313
3505.770777	500380.417210	46.962317
3505.324119	500315.063162	46.967322
3505.684253	500243.604471	46.972327
3505.507315	500170.770789	46.977332
3505.517761	500116.462183	46.982337
3505.324236	500034.427885	46.987341
3505.521869	499969.518679	46.992346
3505.815489	499900.749834	46.997351
3505.878966	499835.407917	47.002356
3505.505875	499754.717604	47.007361
3505.655488	499682.786771	47.012365
3505.588915	499620.601326	47.017370
3505.621833	499549.246070	47.022375
3505.491100	499480.952470	47.027380
3505.577236	499407.109732	47.032385
3505.682624	499334.830968	47.037389
3505.760469	499267.663927	47.042394
3505.590578	499198.212790	47.047399
3505.579307	499135.611538	47.052404
3505.459031	499063.572394	47.057409
3505.571984	498992.909033	47.062413
3505.402113	498932.255696	47.067418
3505.890993	498861.578159	47.072423
3505.482129	498800.105473	47.077428
3505.546459	498728.893031	47.082433
3505.671945	498659.186927	47.087437
3505.562379	498600.999989	47.092442
3505.563667	498522.313108	47.097447
3505.522538	498453.291998	47.102452
3505.227025	498389.118219	47.107457
3505.582911	498318.208228	47.112461
3505.616615	498255.798263	47.117466
3505.922086	498188.689135	47.122471
3505.447003	498117.363891	47.127476
3505.631910	498041.981083	47.132481
3505.672429	497972.842897	47.137485
3505.587147	497906.962500	47.142490
3505.726023	497830.372872	47.147495
3505.902054	497772.690567	47.152500
3505.598274	497694.557584	47.157505
3505.328780	497639.024357	47.162509
3505.520634	497580.580097	47.167514
3505.880803	497505.468378	47.172519
3505.520414	497431.693108	47.177524
3505.786355	497361.047274	47.182529
3505.536556	497294.636240	47.187533
3505.614687	497228.017229	47.192538
3506.392501	497152.782043	47.197543
3505.798617	497092.093251	47.202548
3505.770532	497002.328443	47.207553
3505.998703	496941.498745	47.212557
3505.893328	496877.944156	47.217562
3506.023860	496795.686819	47.222567
3506.192607	496732.691776	47.227572
3506.060591	496653.917695	47.232577
3506.075238	496564.800729	47.237581
3505.668228	496497.907616	47.242586
3505.758365	496426.175181	47.247591
3505.298450	496358.683630	47.252596
3505.163016	496284.763740	47.257601
3505.247473	496237.004810	47.262605
3505.074501	496173.206206	47.267610
3505.420713	496102.237897	47.272615
3505.446496	496046.598390	47.277620
3505.075801	495987.789427	47.282625
3505.276038	495925.797532	47.287629
3505.312028	495866.463506	47.292634
3505.364976	495800.399481	47.297639
3504.913607	495748.734976	47.302644
3505.219262	495682.323869	47.307649
3504.830038	495629.029873	47.312653
3504.982577	495567.702325	47.317658
3505.130433	495506.931723	47.322663
3505.183489	495461.957802	47.327668
3505.229030	495401.558344	47.332673
3505.646325	495345.495615	47.337677
3505.429387	495279.323887	47.342682
3505.094098	495217.876041	47.347687
3505.182900	495153.725394	47.352692
3505.031968	495092.498512	47.357697
3504.982905	495048.906593	47.362701
3504.953789	494997.976974	47.367706
3505.382347	494944.794084	47.372711
3505.040867	494883.244913	47.377716
3505.005607	494814.814782	47.382721
3505.418951	494768.007155	47.387725
3505.209585	494715.539440	47.392730
3505.181373	494654.087690	47.397735
3505.356543	494601.301055	47.402740
3505.119230	494537.557822	47.407745
3505.122586	494477.971574	47.412749
3504.683151	494423.923607	47.417754
3505.056214	494365.234901	47.422759
3505.059112	494312.881441	47.427764
3505.071754	494261.133149	47.432769
3505.282402	494199.386049	47.437773
3504.935174	494144.259203	47.442778
3504.945058	494088.514786	47.447783
3504.946812	494036.261833	47.452788
3505.199521	493985.331628	47.457793
3505.222807	493932.821762	47.462797
3504.871175	493879.465237	47.467802
3505.148085	493820.639311	47.472807
3505.289403	493773.369544	47.477812
3504.917144	493713.338897	47.482817
3505.261585	493659.761662	47.487821
3504.921958	493610.449006	47.492826
3504.856282	493552.793511	47.497831
3504.943728	493501.485393	47.502836
3504.873009	493447.219598	47.507841
3504.993533	493398.434781	47.512845
3504.669426	493354.379607	47.517850
3504.735382	493309.802448	47.522855
3504.398170	493263.371751	47.527860
3504.729351	493222.037150	47.532865
3504.760544	493168.663611	47.537869
3504.753486	493124.857224	47.542874
3504.928281	493066.754332	47.547879
3504.500030	493028.786456	47.552884
3504.715923	492963.341156	47.557889
3504.902740	492926.583286	47.562893
3504.537544	492887.896114	47.567898
3505.013484	492838.441965	47.572903
3504.768098	492782.028629	47.577908
3504.871073	492738.253048	47.582913
3504.955501	492686.285352	47.587917
3504.977445	492638.425764	47.592922
3504.679984	492581.464192	47.597927
3504.843036	492547.036599	47.602932
3505.057023	492490.037983	47.607937
3505.250546	492431.676789	47.612941
3504.892444	492391.722573	47.617946
3505.048486	492331.950964	47.622951
3504.548041	492284.685463	47.627956
3504.643263	492245.462920	47.632961
3505.015741	492206.294126	47.637965
3504.843124	492166.155944	47.642970
3504.598660	492112.269686	47.647975
3504.597313	492068.965503	47.652980
3504.723780	492029.484184	47.657985
3504.968745	491981.129369	47.662989
3504.632310	491932.216023	47.667994
3504.701420	491883.840370	47.672999
3504.830456	491836.870868	47.678004
3504.606510	491796.689992	47.683009
3504.894314	491741.952833	47.688013
3504.880658	491700.622840	47.693018
3504.979824	491650.521323	47.698023
3504.618850	491615.574243	47.703028
3504.770057	491561.821054	47.708033
3504.837366	491502.769971	47.713037
3504.639968	491461.926093	47.718042
3504.804054	491418.086106	47.723047
3504.906972	491376.684837	47.728052
3504.592450	491323.668108	47.733057
3504.803284	491266.868324	47.738061
3505.196699	491235.535444	47.743066
3505.043701	491179.404593	47.748071
3505.053367	491134.780778	47.753076
3505.212365	491080.012909	47.758081
3505.311978	491021.713537	47.763085
3504.835381	490972.973158	47.768090
3504.840664	490924.200956	47.773095
3505.222437	490881.081320	47.778100
3504.760460	490834.058205	47.783105
3505.084012	490786.951432	47.788109
3504.814094	490739.591707	47.793114
3505.231756	490684.272479	47.798119
3504.507633	490632.942542	47.803124
3504.538298	490593.120120	47.808129
3504.858132	490541.510473	47.813133
3504.464921	490515.521756	47.818138
3504.356419	490462.922537	47.823143
3504.638463	490425.738291	47.828148
3504.424107	490392.281507	47.833153
3504.508653	490341.116188	47.838157
3504.245036	490313.637800	47.843162
3504.649399	490262.771803	47.848167
3504.245702	490239.921326	47.853172
3504.429217	490199.009406	47.858177
3504.860056	490153.147451	47.863181
3504.254815	490123.753887	47.868186
3504.600464	490076.186042	47.873191
3504.503804	490039.976338	47.878196
3504.559648	490005.814930	47.883201
3504.487944	489951.082860	47.888205
3504.209840	489922.341432	47.893210
3504.575891	489870.671292	47.898215
3504.601096	489847.949444	47.903220
3504.265100	489803.280005	47.908225
3504.504651	489751.681704	47.913229
3504.486206	489734.937502	47.918234
3504.450220	489690.823701	47.923239
3504.520337	489657.924075	47.928244
3504.524258	489614.157440	47.933249
3504.329691	489563.796420	47.938253
3504.250983	489547.467100	47.943258
3504.410400	489500.890807	47.948263
3504.428714	489461.472657	47.953268
3504.256978	489427.197171	47.958273
3504.511956	489379.035725	47.963277
3504.361336	489349.057242	47.968282
3504.408482	489310.746965	47.973287
3504.534333	489285.274933	47.978292
3504.868055	489248.585306	47.983297
3504.824863	489196.426454	47.988301
3504.279957	489170.107422	47.993306
3504.498268	489112.439101	47.998311
3504.367524	489085.695039	48.003316
3504.289255	489050.390887	48.008321
3504.574612	489006.878251	48.013325
3504.430231	488977.910025	48.018330
3504.312779	488935.275560	48.023335
3504.326773	488909.923272	48.028340
3504.356758	488875.055666	48.033345
3504.517057	488828.123223	48.038349
3504.289848	488796.487099	48.043354
3504.750452	488763.721497	48.048359
3504.538424	488717.257118	48.053364
3503.903928	488690.345463	48.058369
3504.557603	488648.185818	48.063373
3504.248784	488616.613899	48.068378
3504.437498	488579.593420	48.073383
3504.504248	488541.986491	48.078388
3504.604297	488513.431151	48.083393
3505.058453	488469.837749	48.088397
3504.543123	488433.038368	48.093402
3504.688331	488382.160499	48.098407
3504.758712	488350.169148	48.103412
3504.668564	488304.745459	48.108417
3504.621993	488268.169293	48.113421
3504.106528	488232.229717	48.118426
3504.584307	488188.479775	48.123431
3504.543419	488163.236969	48.128436
3504.456676	488117.559206	48.133441
3504.803072	488070.491740	48.138445
3504.524011	488032.740351	48.143450
3504.683910	488003.414938	48.148455
3504.565325	487953.997691	48.153460
3504.540477	487919.491739	48.158465
3504.408046	487895.630414	48.163469
3504.257691	487862.309614	48.168474
3504.717082	487829.744869	48.173479
3504.164345	487782.273527	48.178484
3504.195734	487753.779266	48.183489
3504.273953	487725.276962	48.188493
3504.117315	487690.034028	48.193498
3504.208509	487650.700526	48.198503
3504.375126	487631.139572	48.203508
3503.774187	487603.410860	48.208513
3504.140350	487561.702499	48.213517
3503.995624	487536.527116	48.218522
3504.278499	487507.888309	48.223527
3503.959311	487488.106526	48.228532
3503.982381	487447.367321	48.233537
3503.856185	487413.080082	48.238541
3504.232511	487395.861396	48.243546
3503.770696	487370.183281	48.248551
3503.905586	487351.285270	48.253556
3503.493499	487311.075475	48.258561
3503.785815	487283.497356	48.263565
3503.469654	487270.900479	48.268570
3503.769948	487232.542399	48.273575
3503.628633	487230.643570	48.278580
3503.770347	487220.043220	48.283585
3503.880452	487196.847976	48.288589
3503.873770	487182.224654	48.293594
3503.923342	487144.162208	48.298599
3503.855551	487117.505576	48.303604
3503.765465	487095.204643	48.308609
3503.741583	487076.890087	48.313613
3503.761156	487060.086212	48.318618
3504.121028	487039.024082	48.323623
3504.140607	487008.152231	48.328628
3504.031399	486972.646728	48.333633
3504.371623	486949.968512	48.338637
3504.105394	486925.470849	48.343642
3504.353204	486881.301459	48.348647
3504.214663	486862.449607	48.353652
3504.210731	486832.542946	48.358657
3504.265760	486804.194913	48.363661
3504.097784	486781.552646	48.368666
3504.292146	486752.320458	48.373671
3503.756534	486720.429587	48.378676
3503.736839	486688.906014	48.383681
3503.840900	486662.118136	48.388685
3503.754679	486652.922698	48.393690
3503.618523	486635.689559	48.398695
3503.768288	486616.484583	48.403700
3503.825032	486599.269077	48.408705
3504.224717	486568.888208	48.413709
3503.888629	486537.114752	48.418714
3504.237326	486512.713937	48.423719
3504.216201	486498.396143	48.428724
3503.901669	486464.695862	48.433729
3504.247250	486430.629777	48.438733
3503.991147	486410.734789	48.443738
3503.591099	486395.115251	48.448743
3503.432901	486389.373165	48.453748
3503.674268	486366.407438	48.458753
3504.048590	486330.969891	48.463757
3503.934969	486299.208624	48.468762
3503.770228	486265.128140	48.473767
3504.001492	486248.641584	48.478772
3503.689831	486240.344730	48.483777
3503.925186	486217.987112	48.488781
3503.524824	486185.515502	48.493786
3503.420810	486150.968968	48.498791
3503.641058	486137.115732	48.503796
3503.857845	486116.734814	48.508801
3503.614504	486098.102459	48.513805
3503.565356	486096.491409	48.518810
3503.749474	486080.164566	48.523815
3503.460637	486055.922579	48.528820
3503.455548	486050.002418	48.533825
3503.400778	486030.426870	48.538829
3503.496426	486019.327590	48.543834
3503.456686	486002.482221	48.548839
3503.344727	485999.262462	48.553844
3503.549873	485984.095901	48.558849
3503.673816	485967.070728	48.563853
3503.539646	485955.656398	48.568858
3503.694501	485933.970057	48.573863
3503.752331	485906.935883	48.578868
3503.203113	485878.335273	48.583873
3503.437572	485851.776930	48.588877
3503.706511	485845.556874	48.593882
3503.638917	485819.910383	48.598887
3503.485635	485813.914231	48.603892
3503.451583	485794.334882	48.608897
3503.352636	485779.574320	48.613901
3503.409435	485781.892549	48.618906
3503.644387	485752.297512	48.623911
3503.608832	485751.342010	48.628916
3503.866540	485739.253335	48.633921
3503.795007	485718.921185	48.638925
3503.731601	485717.008888	48.643930
3503.752975	485702.379541	48.648935
3503.494635	485690.125905	48.653940
3503.390261	485666.914651	48.658945
3503.711881	485642.669077	48.663949
3503.627824	485636.408004	48.668954
3504.009865	485617.718967	48.673959
3503.875925	485606.608019	48.678964
3503.598738	485595.774564	48.683969
3503.641484	485575.574560	48.688973
3503.358349	485570.157187	48.693978
3503.485236	485551.612862	48.698983
3503.552343	485541.580928	48.703988
3503.333353	485532.154531	48.708993
3503.737134	485523.026661	48.713997
3503.479105	485516.187949	48.719002
3503.497151	485491.234873	48.724007
3503.488927	485476.661001	48.729012
3503.518093	485464.611160	48.734017
3503.596568	485426.894313	48.739021
3503.559229	485411.313183	48.744026
3503.887420	485391.823362	48.749031
3503.632228	485381.340280	48.754036
3503.413060	485370.547388	48.759041
3503.656917	485347.731734	48.764045
3503.655770	485335.838808	48.769050
3503.545955	485328.063755	48.774055
3503.549643	485319.307747	48.779060
3503.546538	485311.362639	48.784065
3503.764349	485300.545702	48.789069
3503.613000	485288.678390	48.794074
3503.743929	485268.260541	48.799079
3503.413685	485233.194130	48.804084
3503.085395	485211.842440	48.809089
3503.098635	485217.710831	48.814093
3503.044746	485226.880284	48.819098
3503.356059	485214.326614	48.824103
3503.624926	485205.272226	48.829108
3503.342454	485200.158280	48.834113
3503.648555	485183.404904	48.839117
3503.681449	485173.226774	48.844122
3503.555934	485152.295874	48.849127
3503.702209	485146.552002	48.854132
3503.343739	485104.556654	48.859137
3503.423197	485090.524197	48.864141
3503.415999	485084.857119	48.869146
3502.987605	485068.380873	48.874151
3503.380777	485079.903335	48.879156
3503.649985	485076.871373	48.884161
3503.543986	485069.854699	48.889165
3503.359850	485054.045270	48.894170
3503.761898	485038.388789	48.899175
3503.654598	485012.089972	48.904180
3503.293835	484987.302083	48.909185
3503.750325	484973.508816	48.914189
3503.452396	484977.102358	48.919194
3503.867592	484953.295350	48.924199
3503.886586	484948.484127	48.929204
3503.712867	484938.796631	48.934209
3503.946756	484930.102345	48.939213
3503.493750	484919.855204	48.944218
3503.952678	484873.923980	48.949223
3503.899273	484857.839002	48.954228
3503.682080	484839.150236	48.959233
3503.847306	484826.924898	48.964237
3503.583911	484817.100815	48.969242
3503.746731	484796.423923	48.974247
3503.584490	484793.212528	48.979252
3503.573779	484777.828734	48.984257
3503.813863	484764.325307	48.989261
3503.518707	484743.119222	48.994266
3503.637825	484712.479395	48.999271
3503.541571	484717.506266	49.004276
3503.072441	484700.631745	49.009281
3503.262361	484690.224083	49.014285
3503.151551	484678.400048	49.019290
3503.433254	484664.282109	49.024295
3503.154060	484669.896949	49.029300
3503.193575	484672.572551	49.034305
3503.217438	484666.596371	49.039309
3503.231905	484668.972586	49.044314
3503.445233	484654.157761	49.049319
3503.282247	484654.691673	49.054324
3503.376491	484633.621413	49.059329
3503.593372	484622.905442	49.064333
3503.423575	484624.604571	49.069338
3503.308376	484614.198350	49.074343
3503.411096	484607.095243	49.079348
3503.517448	484592.855354	49.084353
3503.311364	484581.857300	49.089357
3503.294589	484588.085303	49.094362
3503.289215	484570.827807	49.099367
3503.351049	484567.476889	49.104372
3503.283850	484555.291048	49.109377
3502.941367	484534.194015	49.114381
3503.045355	484537.921465	49.119386
3503.281212	484522.647183	49.124391
3503.397012	484511.745959	49.129396
3503.435278	484507.488050	49.134401
3503.317785	484493.691192	49.139405
3503.324725	484493.740593	49.144410
3503.296452	484473.905733	49.149415
3503.615831	484465.803960	49.154420
3503.191552	484453.881464	49.159425
3503.560309	484447.795710	49.164429
3503.181699	484439.914325	49.169434
3503.088508	484442.916290	49.174439
3503.142041	484460.317471	49.179444
3503.039410	484458.006842	49.184449
3503.371523	484449.244938	49.189453
3502.834617	484452.018994	49.194458
3503.145094	484440.730206	49.199463
3503.102670	484439.067245	49.204468
3502.877647	484423.416066	49.209473
3503.155038	484428.581667	49.214477
3503.024862	484447.735020	49.219482
3503.469685	484432.981707	49.224487
3503.137819	484434.050576	49.229492
3503.197479	484418.300173	49.234497
3503.491402	484416.073664	49.239501
3502.949079	484407.764714	49.244506
3503.343189	484396.613453	49.249511
3503.313005	484393.733718	49.254516
3503.004282	484390.142366	49.259521
3503.340003	484384.416513	49.264525
3503.150103	484377.666947	49.269530
3503.601683	484367.062584	49.274535
3503.992510	484359.252233	49.279540
3503.693914	484339.007872	49.284545
3503.469027	484326.747575	49.289549
3503.106292	484329.795581	49.294554
3503.486567	484320.316825	49.299559
3503.465645	484317.789779	49.304564
3503.280699	484309.419762	49.309569
3503.336786	484290.582531	49.314573
3502.998885	484298.181376	49.319578
3503.462677	484288.688343	49.324583
3503.281370	484275.458941	49.329588
3503.383149	484275.340314	49.334593
3503.400404	484257.471305	49.339597
3502.990414	484254.960069	49.344602
3502.812086	484264.353716	49.349607
3503.173113	484268.998964	49.354612
3503.037499	484265.985374	49.359617
3503.245302	484258.560513	49.364621
3503.054541	484259.655911	49.369626
3503.310682	484252.880751	49.374631
3503.459323	484249.110055	49.379636
3502.878668	484245.261432	49.384641
3503.004334	484233.143662	49.389645
3503.265700	484247.877737	49.394650
3503.237955	484237.051465	49.399655
3503.216094	484236.599664	49.404660
3503.511608	484230.981850	49.409665
3503.611088	484228.788519	49.414669
3503.273558	484222.418385	49.419674
3503.457911	484197.232637	49.424679
3503.545310	484197.976871	49.429684
3503.199063	484196.315151	49.434689
3503.830939	484186.186017	49.439693
3503.047596	484185.054437	49.444698
3503.310608	484174.735217	49.449703
3503.341643	484164.759273	49.454708
3503.421015	484155.433031	49.459713
3503.401719	484148.806085	49.464717
3503.195055	484149.802980	49.469722
3503.705624	484125.016941	49.474727
3503.820194	484131.020229	49.479732
3503.882871	484116.584965	49.484737
3503.615546	484093.753749	49.489741
3503.885872	484085.103441	49.494746
3504.070908	484067.711719	49.499751
3503.791488	484067.455727	49.504756
3503.727577	484059.115538	49.509761
3503.581062	484042.539589	49.514765
3503.453469	484050.912434	49.519770
3503.707121	484031.889356	49.524775
3503.749314	484029.199655	49.529780
3503.508903	483997.304048	49.534785
3503.636328	483965.193738	49.539789
3503.579873	483964.191095	49.544794
3503.701311	483955.211855	49.549799
3503.523662	483944.613452	49.554804
3503.620241	483941.256482	49.559809
3504.121882	483924.114239	49.564813
3503.600844	483927.037504	49.569818
3503.819676	483914.346867	49.574823
3503.647059	483895.143360	49.579828
3503.311418	483873.487626	49.584833
3503.523461	483848.195427	49.589837
3503.080673	483836.528740	49.594842
3503.059433	483859.004601	49.599847
3503.610112	483865.642101	49.604852
3503.299022	483860.735103	49.609857
3503.575134	483849.856713	49.614861
3503.262015	483853.908592	49.619866
3503.030722	483833.044802	49.624871
3503.132421	483832.065761	49.629876
3503.124175	483831.257331	49.634881
3503.450645	483814.043664	49.639885
3503.347641	483813.605706	49.644890
3503.088019	483802.970601	49.649895
3503.260791	483800.562249	49.654900
3503.262177	483794.640226	49.659905
3503.417137	483792.083074	49.664909
3503.025270	483795.136146	49.669914
3503.163726	483777.043505	49.674919
3503.247300	483775.409581	49.679924
3503.143234	483795.217155	49.684929
3502.848332	483801.745989	49.689933
3502.833940	483801.748421	49.694938
3503.087744	483790.013377	49.699943
3503.338082	483781.568787	49.704948
3503.099621	483776.143231	49.709953
3503.167065	483769.197652	49.714957
3503.097943	483776.598987	49.719962
3503.143516	483779.577371	49.724967
3503.401668	483780.545535	49.729972
3503.076981	483779.892361	49.734977
3503.458795	483767.426857	49.739981
3503.237031	483762.858874	49.744986
3503.573344	483758.195601	49.749991
3503.388004	483756.961885	49.754996
3503.137755	483748.147231	49.760001
3503.526062	483731.074766	49.765005
3503.144629	483739.896007	49.770010
3503.287153	483729.698328	49.775015
3503.243353	483723.581542	49.780020
3503.161873	483724.860768	49.785025
3503.246415	483713.913777	49.790029
3502.932395	483715.080867	49.795034
3503.359246	483698.457312	49.800039
3503.293704	483703.377998	49.805044
3503.069088	483714.247634	49.810049
3503.447144	483711.399311	49.815053
3503.417791	483712.163501	49.820058
3503.433388	483702.038092	49.825063
3503.393366	483701.639992	49.830068
3503.487945	483692.159069	49.835073
3503.290236	483687.435118	49.840077
3503.354085	483682.666506	49.845082
3503.161412	483676.524509	49.850087
3503.304512	483675.589004	49.855092
3503.311597	483668.552465	49.860097
3503.538641	483656.821902	49.865101
3503.188590	483663.866341	49.870106
3503.485332	483654.097811	49.875111
3503.509479	483643.768454	49.880116
3503.412217	483639.533477	49.885121
3503.569122	483628.472851	49.890125
3503.764638	483629.856629	49.895130
3503.804652	483616.082807	49.900135
3503.182938	483609.710360	49.905140
3503.003016	483603.211864	49.910145
3503.314450	483605.183218	49.915149
3502.887104	483605.104318	49.920154
3503.012092	483592.378860	49.925159
3503.191556	483593.562927	49.930164
3503.085120	483587.861700	49.935169
3503.471155	483578.482794	49.940173
3503.308683	483574.967532	49.945178
3503.571306	483558.371887	49.950183
3503.413667	483566.497019	49.955188
3503.398488	483560.172834	49.960193
3503.704336	483544.126549	49.965197
3503.552428	483547.492989	49.970202
3503.704511	483530.005139	49.975207
3503.623051	483530.272093	49.980212
3503.470807	483530.551133	49.985217
3503.721642	483518.411504	49.990221
3503.591036	483512.714380	49.995226
3503.623751	483501.826722	50.000231
3503.594943	483499.149063	50.005236
3503.721599	483488.802113	50.010241
3503.330797	483478.796582	50.015245
3503.023006	483487.200459	50.020250
3503.213796	483479.069579	50.025255
3503.372174	483472.968801	50.030260
3503.101074	483460.108421	50.035265
3503.033584	483454.248658	50.040269
3502.958980	483450.667754	50.045274
3503.273098	483445.957576	50.050279
3503.405798	483439.203183	50.055284
3503.031267	483440.836152	50.060289
3503.636735	483425.599047	50.065293
3503.218043	483428.100001	50.070298
3503.054545	483419.928358	50.075303
3503.297070	483434.109569	50.080308
3503.153433	483444.560628	50.085313
3502.999105	483447.016442	50.090317
3502.835153	483452.611987	50.095322
3503.104032	483440.266766	50.100327
3503.189522	483428.863909	50.105332
3503.010235	483433.500405	50.110337
3503.184969	483422.234149	50.115341
3502.855984	483445.421067	50.120346
3503.055406	483453.637128	50.125351
3503.384088	483451.708252	50.130356
3503.425403	483444.463322	50.135361
3503.591350	483438.664925	50.140365
3503.329425	483435.116001	50.145370
3503.679825	483428.071362	50.150375
3503.382557	483424.781543	50.155380
3503.089941	483424.578408	50.160385
3503.786502	483411.907072	50.165389
3503.448658	483413.533779	50.170394
3503.323473	483405.507430	50.175399
3503.297843	483397.362851	50.180404
3503.483181	483390.953754	50.185409
3503.341396	483391.079167	50.190413
3503.080272	483390.566967	50.195418
3503.275296	483386.484482	50.200423
3503.370542	483380.242607	50.205428
3503.227121	483378.596790	50.210433
3503.477152	483364.078310	50.215437
3503.314174	483362.638289	50.220442
3503.244914	483355.209744	50.225447
3503.560002	483356.876816	50.230452
3503.477538	483347.223480	50.235457
3503.723565	483337.463436	50.240461
3503.121359	483346.980557	50.245466
3503.414382	483329.114141	50.250471
3503.325934	483329.179833	50.255476
3503.457824	483325.614260	50.260481
3503.406642	483314.335895	50.265485
3503.078530	483314.948654	50.270490
3503.225219	483305.306783	50.275495
3502.979963	483305.601708	50.280500
3502.758963	483309.030604	50.285505
3503.020076	483320.222463	50.290509
3502.704886	483331.664559	50.295514
3503.177285	483311.742912	50.300519
3503.060999	483311.813356	50.305524
3502.735463	483319.967269	50.310529
3503.332106	483335.100390	50.315533
3503.249840	483345.743486	50.320538
3503.402523	483347.944435	50.325543
3503.641688	483351.851514	50.330548
3503.371878	483348.152075	50.335553
3503.773588	483333.658286	50.340557
3503.458197	483333.307195	50.345562
3503.639115	483307.766468	50.350567
3503.414929	483278.751838	50.355572
3503.382899	483268.533084	50.360577
3504.011191	483253.696854	50.365581
3503.648467	483258.364716	50.370586
3504.039935	483251.869759	50.375591
3503.640997	483254.519210	50.380596
3503.562605	483251.445060	50.385601
3503.873208	483241.927013	50.390605
3503.495612	483241.991460	50.395610
3503.391394	483221.813862	50.400615
3503.000302	483218.135104	50.405620
3503.045609	483217.266888	50.410625
3503.220699	483208.075650	50.415629
3503.251156	483209.437030	50.420634
3503.049439	483206.535775	50.425639
3503.301376	483200.570773	50.430644
3503.183564	483188.240789	50.435649
3503.234274	483197.494662	50.440653
3503.152289	483192.345899	50.445658
3503.342906	483177.938642	50.450663
3503.466417	483177.259531	50.455668
3503.085594	483183.195881	50.460673
3503.211463	483194.309681	50.465677
3503.327537	483201.629019	50.470682
3503.197518	483206.813927	50.475687
3503.251281	483200.325997	50.480692
3502.950173	483202.199525	50.485697
3503.306401	483190.902134	50.490701
3503.088637	483186.485163	50.495706
3503.459286	483184.397249	50.500711
3503.572594	483174.001780	50.505716
3503.193309	483185.454913	50.510721
3503.408657	483167.905290	50.515725
3503.107700	483173.473700	50.520730
3503.462603	483157.317461	50.525735
3503.614354	483131.832078	50.530740
3503.252006	483101.929674	50.535745
3503.455175	483042.674931	50.540749
3503.496797	482989.521451	50.545754
3503.013666	482926.840408	50.550759
3502.918226	482847.592124	50.555764
3502.933971	482765.641840	50.560769
3503.650185	482652.897945	50.565773
3503.190669	482544.302206	50.570778
3503.465638	482412.549548	50.575783
3503.132789	482275.179903	50.580788
3502.762835	482130.931478	50.585793
3503.231041	481965.987659	50.590797
3502.947436	481795.855690	50.595802
3502.732362	481613.106139	50.600807
3503.066418	481417.656562	50.605812
3502.660155	481212.358990	50.610817
3503.330703	480989.309625	50.615821
3502.820468	480774.153636	50.620826
3503.126400	480529.444009	50.625831
3502.728965	480272.195326	50.630836
3502.729806	480019.279258	50.635841
3502.842337	479738.699444	50.640845
3502.790616	479453.283259	50.645850
3502.689895	479148.278504	50.650855
3503.000126	478837.224420	50.655860
3502.849459	478513.738530	50.660865
3502.780694	478168.816755	50.665869
3502.697503	477833.004332	50.670874
3502.779269	477459.437372	50.675879
3502.823373	477074.932640	50.680884
3502.650653	476690.051781	50.685889
3502.887358	476280.180806	50.690893
3503.077603	475863.219635	50.695898
3502.925512	475419.621891	50.700903
3503.014304	474970.351520	50.705908
3502.683112	474505.190559	50.710913
3502.813141	474014.365646	50.715917
3502.887821	473526.322512	50.720922
3502.898331	473013.563578	50.725927
3502.979840	472476.924721	50.730932
3502.579421	471946.329005	50.735937
3502.727075	471375.511660	50.740941
3502.618192	470811.862336	50.745946
3502.447135	470223.742394	50.750951
3502.322700	469614.676700	50.755956
3502.178461	469005.544155	50.760961
3502.453133	468359.645739	50.765965
3501.926865	467718.978618	50.770970
3502.147911	467039.256066	50.775975
3502.073269	466356.064305	50.780980
3502.063255	465671.722678	50.785985
3501.995095	464938.829828	50.790989
3501.700748	464214.206578	50.795994
3502.113603	463455.386210	50.800999
3502.249886	462678.848824	50.806004
3502.200973	461879.205505	50.811009
3502.006607	461052.798177	50.816013
3501.843219	460223.918500	50.821018
3501.702755	459370.116792	50.826023
3501.853080	458490.584042	50.831028
3501.500282	457610.997194	50.836033
3501.915016	456692.415366	50.841037
3501.510304	455777.074373	50.846042
3501.413582	454826.612287	50.851047
3501.121422	453863.668794	50.856052
3500.854239	452876.291281	50.861057
3501.127904	451873.970305	50.866061
3500.646385	450855.353541	50.871066
3500.844248	449818.165775	50.876071
3500.697367	448752.489010	50.881076
3500.494725	447679.770112	50.886081
3500.555776	446578.553856	50.891085
3500.388610	445464.844154	50.896090
3500.401235	444325.535707	50.901095
3500.054398	443172.534378	50.906100
3499.915739	442005.842876	50.911105
3499.989342	440810.444338	50.916109
3499.979524	439608.400528	50.921114
3499.972333	438372.961496	50.926119
3499.490034	437125.156323	50.931124
3499.027685	435852.367211	50.936129
3499.210127	434570.212667	50.941133
3498.946312	433268.273022	50.946138
3498.703854	431950.981830	50.951143
3498.655026	430614.247849	50.956148
3498.276592	429272.875186	50.961153
3498.177398	427884.330190	50.966157
3497.730830	426507.944490	50.971162
3498.198506	425106.146879	50.976167
3497.802010	423681.369287	50.981172
3497.440516	422237.566777	50.986177
3497.465686	420783.535689	50.991181
3497.245820	419308.213252	50.996186
3497.060684	417809.695450	51.001191
3496.913854	416303.160688	51.006196
3496.219744	414778.298478	51.011201
3496.420483	413239.049768	51.016205
3495.848359	411691.512698	51.021210
3496.052834	410123.410501	51.026215
3495.819806	408535.074784	51.031220
3495.488031	406932.616682	51.036225
3495.338121	405309.560809	51.041229
3495.186344	403675.943767	51.046234
3495.035806	402016.929392	51.051239
3494.956433	400353.053885	51.056244
3494.416197	398672.340946	51.061249
3494.549410	396969.107239	51.066253
3494.030169	395261.844875	51.071258
3493.712944	393519.789877	51.076263
3493.710657	391779.052745	51.081268
3493.382772	390024.090263	51.086273
3493.272800	388248.150006	51.091277
3492.921090	386462.643543	51.096282
3493.013606	384654.135016	51.101287
3492.600021	382831.680674	51.106292
3491.860463	380997.231617	51.111297
3492.153035	379149.386054	51.116301
3491.844297	377288.066332	51.121306
3491.254210	375410.878136	51.126311
3491.714837	373519.550774	51.131316
3490.940321	371615.618167	51.136321
3491.002663	369691.809653	51.141325
3490.572874	367763.328771	51.146330
3490.445965	365809.950356	51.151335
3490.304302	363840.704144	51.156340
3489.803096	361858.725872	51.161345
3489.416161	359866.376322	51.166349
3488.934412	357867.710483	51.171354
3488.681963	355848.429079	51.176359
3488.615554	353819.171826	51.181364
3488.043318	351781.863703	51.186369
3487.892349	349728.155283	51.191373
3487.224013	347658.410199	51.196378
3487.269669	345576.412731	51.201383
3486.914950	343480.521708	51.206388
3486.233334	341380.979587	51.211393
3486.150746	339267.222294	51.216397
3485.682939	337146.034844	51.221402
3485.669924	335016.104537	51.226407
3485.138968	332866.477128	51.231412
3484.462651	330704.800677	51.236417
3484.210464	328533.447820	51.241421
3483.733118	326361.490274	51.246426
3483.580201	324173.411569	51.251431
3483.073417	321978.797523	51.256436
3482.851111	319777.617386	51.261441
3482.650718	317546.523356	51.266445
3482.307146	315323.933063	51.271450
3481.589863	313072.949556	51.276455
3481.374851	310821.275461	51.281460
3480.992881	308553.370069	51.286465
3480.764555	306273.559249	51.291469
3479.979921	303996.020683	51.296474
3479.713262	301698.218524	51.301479
3479.458589	299390.120002	51.306484
3479.023684	297081.996328	51.311489
3478.608332	294749.829667	51.316493
3478.031717	292432.357897	51.321498
3477.492580	290083.943854	51.326503
3476.946440	287734.085079	51.331508
3476.652978	285390.176268	51.336513
3476.106601	283023.097740	51.341517
3475.443399	280651.749886	51.346522
3475.206127	278271.790154	51.351527
3474.850749	275881.659046	51.356532
3474.105766	273500.710093	51.361537
3473.950580	271085.968741	51.366541
3473.333569	268673.220944	51.371546
3472.792231	266250.714103	51.376551
3472.341862	263830.546194	51.381556
3471.821188	261392.475646	51.386561
3471.671775	258942.007925	51.391565
3470.765091	256503.177484	51.396570
3470.348966	254055.425736	51.401575
3469.788355	251588.499211	51.406580
3469.179673	249124.542413	51.411585
3468.969502	246654.237857	51.416589
3468.435874	244179.520826	51.421594
3467.830399	241682.066476	51.426599
3467.491621	239189.173194	51.431604
3466.857572	236685.762289	51.436609
3466.193679	234171.105029	51.441613
3465.808817	231663.539633	51.446618
3465.321173	229136.344766	51.451623
3464.603023	226615.496388	51.456628
3463.930921	224079.789503	51.461633
3463.357452	221543.938396	51.466637
3462.868751	219010.979626	51.471642
3462.054775	216467.287794	51.476647
3461.436509	213920.392038	51.481652
3460.867885	211368.208259	51.486657
3460.550730	208819.439656	51.491661
3459.454662	206267.671724	51.496666
3458.900011	203707.171347	51.501671
3458.193670	201147.290609	51.506676
3457.338264	198583.730751	51.511681
3457.177177	196024.002038	51.516685
3456.093597	193450.947023	51.521690
3455.834501	190874.544114	51.526695
3455.162472	188298.801832	51.531700
3454.434932	185710.224281	51.536705
3453.692792	183133.689216	51.541709
3453.058362	180562.497619	51.546714
3452.254978	177974.025091	51.551719
3451.834498	175393.530120	51.556724
3450.803277	172814.353056	51.561729
3450.133081	170219.156573	51.566733
3449.179218	167644.340261	51.571738
3448.687092	165058.929008	51.576743
3448.090989	162476.979703	51.581748
3446.954447	159897.642000	51.586753
3446.613639	157307.718313	51.591757
3445.701814	154734.423132	51.596762
3444.834993	152156.656291	51.601767
3444.280254	149591.913070	51.606772
3443.157527	146923.668562	51.611777
3442.190242	144341.882034	51.616781
3441.124435	141766.754100	51.621786
3440.537496	139207.227669	51.626791
3439.484103	136638.206706	51.631796
3438.827295	134092.890498	51.636801
3438.110043	131532.768879	51.641805
3436.673500	128996.304379	51.646810
3435.754138	126441.844302	51.651815
3434.996225	123900.386023	51.656820
3434.300166	121379.837654	51.661825
3433.462225	118851.342536	51.666829
3432.190324	116331.445745	51.671834
3431.382106	113821.672478	51.676839
3430.211713	111313.921947	51.681844
3428.895403	108815.793409	51.686849
3428.542806	106319.606270	51.691853
3427.274841	103845.937750	51.696858
3426.439541	101371.891786	51.701863
3425.095051	98905.593137	51.706868
3423.687935	96454.278966	51.711873
3422.882130	94002.940095	51.716877
3421.745908	91576.716603	51.721882
3420.553570	89150.386376	51.726887
3420.012828	86746.691714	51.731892
3418.620901	84360.132019	51.736897
3417.595998	81959.332870	51.741901
3416.322983	79593.448515	51.746906
3414.726556	77220.582875	51.751911
3413.572687	74881.543954	51.756916
3412.020565	72543.838948	51.761921
3411.002336	70233.400540	51.766925
3409.119090	67939.659935	51.771930
3407.878585	65668.163600	51.776935
3406.766324	63405.723555	51.781940
3405.170970	61171.386389	51.786945
3404.074342	58946.069805	51.791949
3402.031288	56742.762029	51.796954
3400.834635	54572.524225	51.801959
3399.009786	52419.250658	51.806964
3397.202426	50296.008907	51.811969
3395.765944	48195.650853	51.816973
3393.705210	46137.984877	51.821978
3391.435407	44095.027433	51.826983
3389.391826	42105.850404	51.831988
3385.901689	40172.326197	51.836993
3381.164552	38316.892358	51.841997
3375.879273	36550.648634	51.847002
3370.964115	34854.576618	51.852007
3365.795108	33265.765173	51.857012
3360.528964	31758.849952	51.862017
3355.626700	30352.691707	51.867021
3350.957459	29059.231281	51.872026
3346.126769	27847.845657	51.877031
3341.343834	26746.034773	51.882036
3336.301010	25755.747542	51.887041
3331.672293	24845.749468	51.892045
3327.240812	24045.156270	51.897050
3323.391222	23325.274828	51.902055
3320.118695	22703.472109	51.907060
3316.892146	22143.872337	51.912065
3314.335266	21655.788805	51.917069
3311.265513	21257.340698	51.922074
3309.453019	20895.531997	51.927079
3307.947567	20605.359220	51.932084
3305.760962	20358.098680	51.937089
3304.875883	20131.192560	51.942093
3303.205176	19953.845170	51.947098
3302.185603	19803.550006	51.952103
3301.249974	19677.723773	51.957108
3300.513555	19582.716852	51.962113
3300.009090	19495.655408	51.967117
3299.226662	19438.406462	51.972122
3298.849591	19377.806767	51.977127
3298.484182	19336.716793	51.982132
3297.540930	19317.045506	51.987137
3297.356212	19281.014892	51.992141
3297.517871	19261.850460	51.997146
3297.161884	19245.621439	52.002151
3297.189638	19231.064140	52.007156
3296.841999	19220.124539	52.012161
3296.257582	19191.930271	52.017165
3296.103635	19186.894946	52.022170
3295.998936	19172.135857	52.027175
3295.831765	19143.437265	52.032180
3295.559520	19130.777626	52.037185
3295.387065	19095.736445	52.042189
3295.011069	19076.567643	52.047194
3294.986007	19046.156698	52.052199
3295.113352	19017.671993	52.057204
3294.523838	18983.837264	52.062209
3294.497403	18938.223175	52.067213
3294.188272	18903.188353	52.072218
3293.721331	18840.501977	52.077223
3293.835357	18789.148381	52.082228
3293.291415	18741.712131	52.087233
3293.262688	18679.025788	52.092237
3292.497130	18620.067982	52.097242
3292.036252	18552.767551	52.102247
3291.530369	18492.676727	52.107252
3290.917334	18429.931474	52.112257
3290.585059	18357.902555	52.117261
3290.117269	18291.952668	52.122266
3289.684409	18219.061088	52.127271
3289.154514	18157.533989	52.132276
3288.871811	18087.688557	52.137281
3288.795439	17998.061095	52.142285
3287.759499	17911.828862	52.147290
3287.275408	17838.957161	52.152295
3287.031515	17760.860283	52.157300
3286.513225	17674.588256	52.162305
3286.218194	17575.820156	52.167309
3285.456861	17498.116368	52.172314
3284.934060	17414.122517	52.177319
3284.128513	17310.808880	52.182324
3283.652296	17232.545505	52.187329
3283.162033	17140.021829	52.192333
3282.341185	17051.098755	52.197338
3281.715275	16947.909980	52.202343
3281.323484	16857.500043	52.207348
3280.463787	16768.431792	52.212353
3280.242620	16682.330639	52.217357
3279.625853	16584.214451	52.222362
3279.051795	16495.084634	52.227367
3277.932350	16398.511056	52.232372
3277.606034	16296.952022	52.237377
3277.032404	16205.881250	52.242381
3276.576498	16117.417611	52.247386
3276.160908	16014.174955	52.252391
3275.713090	15917.046896	52.257396
3274.627387	15827.097704	52.262401
3274.406548	15720.296041	52.267405
3273.765596	15621.032760	52.272410
3272.969845	15516.652259	52.277415
3272.371137	15413.714851	52.282420
3271.790605	15318.455704	52.287425
3271.082156	15215.829059	52.292429
3270.472404	15123.439682	52.297434
3270.134608	15016.474441	52.302439
3269.607224	14908.522945	52.307444
3268.556526	14815.156509	52.312449
3268.203866	14702.026146	52.317453
3267.327033	14601.526008	52.322458
3266.683969	14493.766064	52.327463
3266.051812	14401.111136	52.332468
3265.352538	14299.618505	52.337473
3264.830790	14196.193498	52.342477
3263.956916	14091.236367	52.347482
3263.415967	13990.500822	52.352487
3262.753194	13887.519025	52.357492
3261.700335	13796.186177	52.362497
3261.454618	13682.115313	52.367501
3261.002530	13585.000032	52.372506
3260.216673	13485.284404	52.377511
3259.269881	13374.446889	52.382516
3258.653777	13286.529776	52.387521
3257.929177	13176.507363	52.392525
3257.413013	13093.351132	52.397530
3256.614213	12988.165377	52.402535
3255.919248	12886.073902	52.407540
3255.398656	12803.441345	52.412545
3254.925942	12697.825659	52.417549
3254.085831	12610.584059	52.422554
3253.237854	12514.075221	52.427559
3252.984383	12417.969444	52.432564
3252.234262	12317.962454	52.437569
3251.640364	12212.089328	52.442573
3250.708197	12121.549419	52.447578
3250.270773	12024.105850	52.452583
3249.632937	11926.458506	52.457588
3248.982462	11837.531118	52.462593
3248.209017	11733.113813	52.467597
3247.397840	11638.272374	52.472602
3246.676274	11540.028577	52.477607
3246.364671	11441.385107	52.482612
3245.521930	11351.346104	52.487617
3245.230437	11257.119619	52.492621
3244.373735	11164.116775	52.497626
3243.710004	11064.333352	52.502631
3243.105099	10963.123246	52.507636
3241.956470	10872.652503	52.512641
3241.699461	10766.288774	52.517645
3241.036130	10679.608680	52.522650
3240.227614	10580.135762	52.527655
3240.136713	10489.102520	52.532660
3238.977170	10394.008668	52.537665
3238.528642	10290.617837	52.542669
3237.992859	10201.090448	52.547674
3237.051831	10097.682285	52.552679
3236.414607	9999.185304	52.557684
3235.498445	9912.882679	52.562689
3235.464679	9818.092789	52.567693
3234.939870	9723.690673	52.572698
3234.055104	9616.563284	52.577703
3233.541017	9530.372523	52.582708
3232.605064	9430.397575	52.587713
3232.246106	9326.610507	52.592717
3231.547459	9229.601077	52.597722
3230.192906	9130.146580	52.602727
3229.675390	9031.892520	52.607732
3228.943457	8944.582518	52.612737
3228.330160	8849.976271	52.617741
3227.552030	8753.454043	52.622746
3226.686780	8670.278849	52.627751
3226.481820	8580.609090	52.632756
3225.699725	8509.992167	52.637761
3225.126303	8406.494069	52.642765
3224.793908	8330.292578	52.647770
3223.753058	8231.546703	52.652775
3223.254546	8144.299086	52.657780
3222.565709	8052.042059	52.662785
3221.779991	7953.692664	52.667789
3221.011567	7868.914309	52.672794
3220.297501	7773.497507	52.677799
3219.727718	7695.806494	52.682804
3219.080204	7594.745512	52.687809
3218.811125	7505.427559	52.692813
3217.650143	7413.708205	52.697818
3217.031629	7324.461221	52.702823
3217.142639	7230.360724	52.707828
3215.854159	7142.447094	52.712833
3215.424891	7053.327244	52.717837
3214.504342	6962.759616	52.722842
3214.120924	6869.694240	52.727847
3213.227653	6780.508274	52.732852
3212.141416	6688.051321	52.737857
3211.966212	6593.748344	52.742861
3211.202293	6506.449905	52.747866
3210.796340	6414.945288	52.752871
3209.926565	6322.455832	52.757876
3208.989750	6243.212371	52.762881
3208.392999	6147.442424	52.767885
3208.072088	6073.451493	52.772890
3207.192972	5979.816523	52.777895
3206.016854	5886.374206	52.782900
3205.486611	5815.667652	52.787905
3205.075508	5725.470135	52.792909
3204.511950	5651.137220	52.797914
3203.506948	5564.756179	52.802919
3203.298624	5480.234337	52.807924
3202.608842	5406.155516	52.812929
3201.878667	5315.381470	52.817933
3201.407325	5235.633879	52.822938
3200.726251	5150.327447	52.827943
3200.375390	5061.439826	52.832948
3199.050827	4975.580917	52.837953
3198.701454	4888.030178	52.842957
3198.440509	4811.540204	52.847962
3197.370252	4717.828422	52.852967
3196.454242	4628.025816	52.857972
3196.007220	4551.216686	52.862977
3195.440610	4459.716758	52.867981
3194.420986	4382.532466	52.872986
3193.881719	4303.717161	52.877991
3193.492544	4221.407625	52.882996
3191.966977	4142.932980	52.888001
3191.873264	4054.265268	52.893005
3191.357127	3982.135961	52.898010
3190.780209	3902.693411	52.903015
3190.031015	3814.086909	52.908020
3189.303644	3740.657138	52.913025
3188.798708	3648.308018	52.918029
3187.824744	3571.747629	52.923034
3187.061718	3488.147608	52.928039
3186.726345	3402.238763	52.933044
3185.820177	3326.616311	52.938049
3185.359227	3249.117052	52.943053
3184.567960	3174.755657	52.948058
3184.108480	3090.145715	52.953063
3183.227020	3014.586862	52.958068
3182.356699	2942.690196	52.963073
3182.215575	2861.012555	52.968077
3181.154149	2786.335932	52.973082
3180.975117	2701.804910	52.978087
3179.685232	2623.265175	52.983092
3178.895846	2553.913906	52.988097
3178.470634	2470.529220	52.993101
3177.673733	2402.469274	52.998106
3176.931768	2328.090813	53.003111
3176.258554	2247.645806	53.008116
3175.463661	2185.682662	53.013121
3174.849418	2114.642962	53.018125
3174.143720	2041.061060	53.023130
3173.688862	1979.312240	53.028135
3173.123111	1904.713024	53.033140
3172.352489	1843.313187	53.038145
3171.723002	1765.242064	53.043149
3171.025319	1696.643968	53.048154
3170.544532	1620.585157	53.053159
3169.692907	1547.504609	53.058164
3168.672250	1486.776164	53.063169
3168.312253	1411.023410	53.068173
3167.375569	1348.866332	53.073178
3166.755986	1279.931827	53.078183
3166.248251	1221.257939	53.083188
3165.247534	1156.742059	53.088193
3164.496453	1096.093419	53.093197
3163.474050	1028.930617	53.098202
3163.039421	977.309212	53.103207
3162.542620	920.007521	53.108212
3161.510084	869.844187	53.113217
3161.136428	811.062083	53.118221
3160.258886	756.788206	53.123226
3159.588508	707.174188	53.128231
3159.175402	642.997803	53.133236
3158.205447	602.158678	53.138241
3157.333344	542.108394	53.143245
3156.576861	503.054379	53.148250
3155.731088	455.099025	53.153255
3155.447143	415.846862	53.158260
3154.426716	372.162636	53.163265
3153.316535	327.614008	53.168269
3152.683479	294.484499	53.173274
3151.647850	281.512506	53.178279
3150.843592	238.955785	53.183284
3149.847139	207.861016	53.188289
3149.420594	187.218467	53.193293
3148.731975	164.487214	53.198298
3146.953546	146.138942	53.203303
3146.393210	142.974198	53.208308
3145.123593	147.491260	53.213313
3144.770852	138.372497	53.218317
3143.798428	154.171821	53.223322
3143.037810	155.027656	53.228327
3142.716927	146.684612	53.233332
3142.092577	153.039807	53.238337
3141.552192	151.924635	53.243341
3141.083980	149.149143	53.248346
3140.639200	155.023273	53.253351
3139.836935	156.112009	53.258356
3138.659349	159.243249	53.263361
3138.568138	156.129796	53.268365
3137.771337	154.653048	53.273370
3137.049051	153.509352	53.278375
3136.803201	148.304209	53.283380
3135.801750	161.061199	53.288385
3135.332217	149.717170	53.293389
3134.681733	159.863855	53.298394
3133.835790	160.047048	53.303399
3133.497703	157.917202	53.308404
3132.412517	155.183177	53.313409
3132.578907	152.596489	53.318413
3131.532254	156.000616	53.323418
3130.414046	157.213201	53.328423
3130.373221	159.216686	53.333428
3129.266806	161.794991	53.338433
3129.159074	157.326889	53.343437
3128.125768	157.639988	53.348442
3127.317096	157.597739	53.353447
3127.096707	150.489603	53.358452
3126.207271	158.137039	53.363457
3126.413211	160.781638	53.368461
3125.268271	161.324596	53.373466
3123.903247	155.678712	53.378471
3123.504291	155.062787	53.383476
3122.840114	166.953358	53.388481
3121.946913	152.966379	53.393485
3121.631082	157.709292	53.398490
3121.003664	163.437398	53.403495
3120.971104	158.296862	53.408500
3120.117950	154.997023	53.413505
3119.425585	153.737692	53.418509
3118.710004	155.242268	53.423514
3117.510606	154.632846	53.428519
3117.328683	156.863330	53.433524
3116.660130	158.799598	53.438529
3115.624033	163.115327	53.443533
3115.192685	155.566403	53.448538
3114.408794	160.573233	53.453543
3113.909574	154.052727	53.458548
3113.369775	160.963467	53.463553
3113.371198	157.440643	53.468557
3112.257199	159.271446	53.473562
3111.481040	160.562563	53.478567
3110.835868	149.746696	53.483572
3109.585647	151.283807	53.488577
3109.577339	148.985120	53.493581
3108.720668	156.136311	53.498586
3107.736283	153.836638	53.503591
3107.997934	156.256589	53.508596
3106.391366	165.247454	53.513601
3105.947172	155.038678	53.518605
3105.593864	152.586575	53.523610
3105.082689	150.205260	53.528615
3104.527261	146.950869	53.533620
3103.484238	158.923531	53.538625
3102.666879	151.998711	53.543629
3102.461281	154.610994	53.548634
3101.721882	156.133457	53.553639
3101.337886	153.767911	53.558644
3100.262357	153.610213	53.563649
3099.499247	151.978508	53.568653
3099.008451	148.713863	53.573658
3098.544105	143.491586	53.578663
3097.810194	153.172533	53.583668
3097.005455	153.385400	53.588673
3096.183510	149.377618	53.593677
3095.390130	150.632205	53.598682
3095.327800	155.260754	53.603687
3094.762588	146.999331	53.608692
3094.087232	156.263705	53.613697
3093.278629	147.368884	53.618701
3092.391479	156.341821	53.623706
3091.636138	156.667036	53.628711
3091.182178	148.927776	53.633716
3090.106936	149.232257	53.638721
3089.759078	153.225527	53.643725
3088.875632	147.487899	53.648730
3087.774276	154.640242	53.653735
3087.874874	153.957121	53.658740
3087.096193	156.281675	53.663745
3086.698390	155.823053	53.668749
3085.771187	152.232326	53.673754
3085.257204	151.577244	53.678759
3085.599064	157.836429	53.683764
3083.642063	156.833447	53.688769
3083.988300	154.665625	53.693773
3082.906169	148.365906	53.698778
3081.872145	162.184756	53.703783
3081.303583	152.870770	53.708788
3080.382072	158.283608	53.713793
3079.739479	152.834819	53.718797
3078.736973	150.195230	53.723802
3078.549180	153.066965	53.728807
3078.627347	147.111744	53.733812
3077.774001	155.942330	53.738817
3076.852686	149.193960	53.743821
3076.492314	148.404872	53.748826
3075.380063	150.018676	53.753831
3074.321473	141.508806	53.758836
3073.269046	149.566582	53.763841
3073.435010	139.896973	53.768845
3073.310366	144.325380	53.773850
3072.290225	154.611012	53.778855
3071.961590	153.954655	53.783860
3070.796005	157.103198	53.788865
3069.962451	150.654431	53.793869
3069.144878	150.451478	53.798874
3068.271381	142.483128	53.803879
3068.610959	149.224266	53.808884
3067.961556	152.360002	53.813889
3066.684198	144.775256	53.818893
3066.243422	142.878485	53.823898
3065.863311	147.107786	53.828903
3065.497006	146.381289	53.833908
3064.585138	151.137626	53.838913
3064.098162	149.221513	53.843917
3062.867969	148.055272	53.848922
3062.585055	152.573486	53.853927
3061.795299	146.099477	53.858932
3060.853343	152.662098	53.863937
3060.350941	147.912106	53.868941
3059.278308	142.725879	53.873946
3058.641721	152.384276	53.878951
3057.947190	147.405409	53.883956
3057.480673	152.295250	53.888961
3057.523805	142.738601	53.893965
3056.966734	156.507133	53.898970
3055.288958	149.596715	53.903975
3055.435213	147.619375	53.908980
3054.702034	158.712142	53.913985
3053.919918	148.525596	53.918989
3053.439869	156.509259	53.923994
3052.474296	150.874879	53.928999
3052.199711	150.124816	53.934004
3050.987801	152.310641	53.939009
3050.340239	148.022813	53.944013
3049.733628	144.385210	53.949018
3049.147263	153.881082	53.954023
3048.672198	147.815925	53.959028
3047.547301	141.632865	53.964033
3046.916482	141.956149	53.969037
3045.989190	143.017708	53.974042
3045.474573	147.225388	53.979047
3045.388466	147.028502	53.984052
3045.176424	146.630113	53.989057
3044.185962	151.248306	53.994061
3043.019321	141.425096	53.999066
3043.080952	146.825071	54.004071
3042.227530	141.508631	54.009076
3040.668810	143.455697	54.014081
3040.760959	146.255518	54.019085
3040.265317	148.763812	54.024090
3039.578823	147.990583	54.029095
3038.672052	144.390851	54.034100
3037.351471	151.125930	54.039105
3037.631586	143.830052	54.044109
3036.928364	142.198387	54.049114
3036.232039	147.380515	54.054119
3035.838924	139.484428	54.059124
3034.622268	150.642435	54.064129
3033.805076	144.548507	54.069133
3033.599794	151.349585	54.074138
3032.701951	144.359986	54.079143
3032.246464	140.605776	54.084148
3031.222362	147.606372	54.089153
3030.772078	141.347910	54.094157
3030.268113	145.758634	54.099162
3029.369693	148.296280	54.104167
3028.758007	147.561585	54.109172
3027.853896	152.382520	54.114177
3027.247832	144.113487	54.119181
3026.573005	141.363051	54.124186
3025.765008	151.184549	54.129191
3025.249912	142.194200	54.134196
3024.632399	148.842301	54.139201
3024.392010	141.766414	54.144205
3023.720639	148.772658	54.149210
3022.495722	145.205187	54.154215
3022.550311	135.375409	54.159220
3021.295434	140.741004	54.164225
3021.181599	133.400344	54.169229
3020.010148	138.725235	54.174234
3019.770705	145.202551	54.179239
3019.330103	137.504051	54.184244
3018.386619	149.944033	54.189249
3017.862867	138.141154	54.194253
3016.981600	144.407228	54.199258
3016.450014	146.271943	54.204263
3015.848163	130.046074	54.209268
3014.835001	137.694123	54.214273
3014.065367	139.121500	54.219277
3013.641036	138.048879	54.224282
3012.952283	139.535460	54.229287
3012.490900	138.434434	54.234292
3011.508546	139.806978	54.239297
3010.986493	139.298148	54.244301
3010.757972	140.640956	54.249306
3009.772075	146.418475	54.254311
3008.712041	137.213757	54.259316
3008.131138	144.639925	54.264321
3007.414798	141.389755	54.269325
3007.095547	136.448613	54.274330
3005.921094	137.981875	54.279335
3005.884506	138.161782	54.284340
3005.366978	142.541666	54.289345
3004.559259	138.396870	54.294349
3003.923516	138.086279	54.299354
3003.101681	135.150578	54.304359
3002.578613	133.119065	54.309364
3001.402340	142.172193	54.314369
3000.987648	131.420398	54.319373
3000.124863	132.590937	54.324378
2999.674180	135.836794	54.329383
2999.397752	126.919357	54.334388
2998.930458	140.684768	54.339393
2998.087254	127.665467	54.344397
2997.212555	134.533164	54.349402
2996.930594	134.980784	54.354407
2996.301105	138.092594	54.359412
2995.367572	135.457817	54.364417
2994.968368	134.307879	54.369421
2993.858897	135.497679	54.374426
2992.604684	133.945570	54.379431
2992.619593	123.176817	54.384436
2992.473345	137.134858	54.389441
2991.308301	132.521008	54.394445
2989.913015	131.152870	54.399450
2989.996206	141.141016	54.404455
2990.003536	131.924832	54.409460
2988.277666	132.816552	54.414465
2987.764085	133.564666	54.419469
2986.924795	136.015240	54.424474
2986.956913	137.102330	54.429479
2986.654762	131.535391	54.434484
2985.251306	134.130922	54.439489
2985.016462	128.657085	54.444493
2984.330168	131.942019	54.449498
2983.659914	135.995114	54.454503
2983.038651	130.452707	54.459508
2981.573878	136.132061	54.464513
2981.277109	137.398508	54.469517
2980.687993	134.437648	54.474522
2980.266461	135.256479	54.479527
2979.389923	127.122497	54.484532
2978.425142	142.979317	54.489537
2978.305844	132.234679	54.494541
2977.143222	132.054388	54.499546
2976.193127	129.255870	54.504551
2976.340656	124.609172	54.509556
2975.494915	134.302509	54.514561
2974.992981	133.243547	54.519565
2973.864374	131.530640	54.524570
2972.966059	131.367551	54.529575
2973.326464	135.275313	54.534580
2972.257833	142.650223	54.539585
2971.679630	125.311936	54.544589
2970.733002	123.811479	54.549594
2969.971339	130.514207	54.554599
2969.805196	130.362577	54.559604
2969.001736	133.822662	54.564609
2968.623720	132.229775	54.569613
2968.389050	140.522016	54.574618
2966.908857	135.383355	54.579623
2965.757553	133.945900	54.584628
2965.026233	136.536706	54.589633
2965.135812	133.707498	54.594637
2964.090704	130.251026	54.599642
2963.174115	138.798344	54.604647
2963.568180	140.023710	54.609652
2962.118794	133.351008	54.614657
2961.578752	130.020591	54.619661
2960.624313	132.128485	54.624666
2960.079709	131.484964	54.629671
2959.793447	131.205049	54.634676
2959.015316	140.459348	54.639681
2958.571351	133.180241	54.644685
2958.020172	136.322486	54.649690
2957.090222	132.277139	54.654695
2956.901423	130.173115	54.659700
2955.609597	144.137057	54.664705
2954.661610	134.559533	54.669709
2953.780952	128.609891	54.674714
2953.645247	142.259032	54.679719
2953.459551	134.319226	54.684724
2952.320553	141.700637	54.689729
2951.052201	135.930531	54.694733
2951.219539	138.515397	54.699738
2950.617826	132.803473	54.704743
2949.577994	134.978066	54.709748
2948.487646	145.992917	54.714753
2948.528951	138.034449	54.719757
2947.951963	129.215748	54.724762
2947.244133	135.214955	54.729767
2946.615266	131.275655	54.734772
2946.150857	140.530420	54.739777
2945.952186	136.797465	54.744781
2944.514189	135.201775	54.749786
2943.116930	138.140853	54.754791
2943.023046	129.124335	54.759796
2942.819804	128.254722	54.764801
2941.819654	142.468023	54.769805
2940.956366	134.214154	54.774810
2939.900471	137.205025	54.779815
2939.717213	134.216656	54.784820
2938.816756	137.047547	54.789825
2939.221200	132.237341	54.794829
2938.379593	139.487012	54.799834
2937.400135	144.354776	54.804839
2936.820580	127.758420	54.809844
2936.040829	138.626638	54.814849
2935.618388	138.689725	54.819853
2934.268457	132.347791	54.824858
2933.497993	134.042944	54.829863
2932.878519	127.332243	54.834868
2932.450568	134.289386	54.839873
2932.012064	139.495747	54.844877
2931.431379	133.911677	54.849882
2930.366987	135.207466	54.854887
2930.061789	127.554529	54.859892
2929.374257	140.814822	54.864897
2929.011374	131.543887	54.869901
2928.779244	131.989704	54.874906
2927.513462	137.202838	54.879911
2926.337521	130.479867	54.884916
2925.256576	135.902591	54.889921
2925.591854	123.881102	54.894925
2924.993515	129.776731	54.899930
2923.807590	124.046234	54.904935
2923.212167	124.554925	54.909940
2922.546001	131.680667	54.914945
2921.999445	126.667859	54.919949
2921.340995	130.733545	54.924954
2920.819834	130.210361	54.929959
2920.265542	123.419449	54.934964
2919.673968	135.201272	54.939969
2919.435131	127.434761	54.944973
2918.363545	132.731942	54.949978
2917.910014	137.971264	54.954983
2917.005945	133.406384	54.959988
2916.377826	135.805484	54.964993
2915.623895	129.481307	54.969997
2914.184463	133.976110	54.975002
2913.713409	135.024060	54.980007
2914.181991	122.949003	54.985012
2912.594239	123.550306	54.990017
2911.738093	128.428178	54.995021
2911.440486	121.684979	55.000026
2910.389220	130.106499	55.005031
2910.412106	127.588944	55.010036
2909.135938	129.678407	55.015041
2909.122740	123.575796	55.020045
2908.539348	125.450949	55.025050
2907.915651	132.906531	55.030055
2907.572889	126.244860	55.035060
2906.295098	129.355759	55.040065
2905.237020	124.383399	55.045069
2904.640303	129.216937	55.050074
2903.728092	134.314388	55.055079
2903.546663	124.213920	55.060084
2902.753619	132.803282	55.065089
2902.486249	130.875315	55.070093
2902.209561	127.769893	55.075098
2901.246748	129.656995	55.080103
2900.920755	120.874359	55.085108
2899.060443	136.917372	55.090113
2898.459924	127.361406	55.095117
2897.904709	131.178142	55.100122
2897.977777	136.261946	55.105127
2897.410797	129.917666	55.110132
2896.354705	136.164283	55.115137
2895.702612	134.307985	55.120141
2895.496062	129.736798	55.125146
2894.433688	132.011565	55.130151
2893.451656	133.626434	55.135156
2892.554496	136.499793	55.140161
2892.402227	133.489157	55.145165
2891.370917	132.004370	55.150170
2891.024700	134.037145	55.155175
2890.621218	132.531904	55.160180
2890.183318	132.245145	55.165185
2889.775713	131.781108	55.170189
2888.456777	126.143218	55.175194
2887.623659	136.965689	55.180199
2886.748411	129.623330	55.185204
2886.027888	141.192332	55.190209
2885.689774	132.753201	55.195213
2885.267403	128.479024	55.200218
2884.334077	132.187884	55.205223
2884.193292	143.840175	55.210228
2883.281639	130.826681	55.215233
2882.937029	130.771473	55.220237
2882.260758	138.281832	55.225242
2880.787435	133.318467	55.230247
2880.285553	128.806833	55.235252
2879.500727	133.221349	55.240257
2879.036828	130.224499	55.245261
2878.453217	125.733543	55.250266
2877.803395	136.633239	55.255271
2877.817960	123.613433	55.260276
2877.105624	138.936066	55.265281
2876.115577	123.863268	55.270285
2875.181189	128.595441	55.275290
2874.291410	135.543486	55.280295
2873.912852	132.608234	55.285300
2873.133353	128.665480	55.290305
2872.614525	131.311161	55.295309
2871.917732	128.967914	55.300314
2871.287269	142.456474	55.305319
2871.032102	131.216005	55.310324
2869.744255	136.745542	55.315329
2868.856588	133.371522	55.320333
2868.572138	124.040619	55.325338
2867.986157	129.857562	55.330343
2867.710202	124.576285	55.335348
2866.891691	136.015586	55.340353
2866.417773	122.214024	55.345357
2865.447458	129.715423	55.350362
2864.209926	130.813450	55.355367
2863.200245	131.271763	55.360372
2863.418077	131.260957	55.365377
2862.960368	133.911588	55.370381
2862.030092	126.976919	55.375386
2861.527408	132.212010	55.380391
2860.961290	126.186134	55.385396
2860.099496	131.177869	55.390401
2859.879270	130.141036	55.395405
2858.496202	130.383697	55.400410
2857.570366	136.438720	55.405415
2857.366398	124.764782	55.410420
2856.698243	128.569638	55.415425
2856.069917	124.413951	55.420429
2855.832548	128.046897	55.425434
2855.246147	133.420241	55.430439
2854.748262	122.136397	55.435444
2853.335644	131.580049	55.440449
2852.450398	125.302802	55.445453
2851.642351	127.489900	55.450458
2850.922862	125.484474	55.455463
2850.724636	117.809718	55.460468
2850.244158	126.533944	55.465473
2849.670266	116.069916	55.470477
2849.453656	131.046115	55.475482
2848.304921	135.056262	55.480487
2847.375419	131.609661	55.485492
2846.360529	123.662775	55.490497
2845.880650	120.596428	55.495501
2845.453800	128.935316	55.500506
2845.111396	123.523692	55.505511
2844.919000	112.067256	55.510516
2844.227840	122.161266	55.515521
2843.192542	117.994613	55.520525
2842.142204	121.982809	55.525530
2841.455206	126.272846	55.530535
2840.706336	122.642619	55.535540
2840.280737	126.499177	55.540545
2840.061038	122.420889	55.545549
2839.096543	126.017847	55.550554
2838.202851	126.289767	55.555559
2837.360944	123.911723	55.560564
2836.550559	127.295243	55.565569
2835.861588	120.941036	55.570573
2835.468012	122.166008	55.575578
2834.633481	126.522312	55.580583
2834.362854	121.048688	55.585588
2833.997965	124.847897	55.590593
2833.613670	121.124969	55.595597
2832.346122	119.694385	55.600602
2831.304460	126.078273	55.605607
2830.908159	112.902524	55.610612
2830.146395	126.755737	55.615617
2830.131094	119.945353	55.620621
2829.397329	121.472406	55.625626
2828.604549	113.684933	55.630631
2828.149158	122.867883	55.635636
2826.913128	126.276388	55.640641
2826.430996	119.702497	55.645645
2826.039469	110.042550	55.650650
2825.190693	121.566353	55.655655
2824.740713	117.683737	55.660660
2823.211435	117.480092	55.665665
2822.327398	116.246853	55.670669
2822.789032	124.784799	55.675674
2821.786623	122.357219	55.680679
2821.348852	121.132969	55.685684
2820.670295	130.310250	55.690689
2820.165936	124.743945	55.695693
2819.413498	116.720636	55.700698
2818.308939	117.987388	55.705703
2817.624286	116.737440	55.710708
2816.512175	124.256760	55.715713
2816.230690	119.170246	55.720717
2815.879548	120.407702	55.725722
2815.438744	120.709588	55.730727
2815.264764	113.112798	55.735732
2813.922403	127.951401	55.740737
2812.694209	123.199975	55.745741
2812.032547	125.366400	55.750746
2811.681202	131.152322	55.755751
2811.158761	123.579163	55.760756
2810.496034	121.837588	55.765761
2809.839614	114.609034	55.770765
2809.487562	115.453893	55.775770
2808.885668	113.606003	55.780775
2808.766096	122.796292	55.785780
2807.440218	129.317573	55.790785
2806.354600	122.154872	55.795789
2805.948769	120.080845	55.800794
2805.107238	132.144193	55.805799
2805.065313	117.371604	55.810804
2803.702546	127.940789	55.815809
2802.801457	122.751759	55.820813
2802.410114	124.596860	55.825818
2801.618360	123.390482	55.830823
2801.292174	118.408318	55.835828
2800.597105	117.254098	55.840833
2799.797265	123.757311	55.845837
2799.735616	116.752753	55.850842
2798.964639	122.465133	55.855847
2798.984113	115.178297	55.860852
2797.544647	117.929226	55.865857
2796.424731	121.508148	55.870861
2796.108333	117.647308	55.875866
2795.782873	121.336360	55.880871
2794.931530	113.364698	55.885876
2793.535824	119.791731	55.890881
2792.744570	119.832998	55.895885
2792.284121	123.143686	55.900890
2791.808043	128.832508	55.905895
2791.903702	115.725046	55.910900
2791.151173	124.758261	55.915905
2790.739220	112.817531	55.920909
2789.699245	115.352950	55.925914
2788.610136	115.256841	55.930919
2788.227230	119.648455	55.935924
2787.475502	121.146216	55.940929
2787.021804	116.685966	55.945933
2786.321639	115.036449	55.950938
2785.210451	119.637404	55.955943
2784.051320	113.785925	55.960948
2783.786507	118.638131	55.965953
2783.844807	118.058552	55.970957
2782.820723	120.640992	55.975962
2782.224216	120.352141	55.980967
2782.026545	110.967744	55.985972
2781.046337	111.648002	55.990977
2780.465293	114.770096	55.995981
2779.419521	117.389794	56.000986
2778.506581	125.449008	56.005991
2778.170401	113.551775	56.010996
2777.300227	109.022583	56.016001
2777.043814	116.934450	56.021005
2776.776999	116.541093	56.026010
2775.714680	115.640693	56.031015
2774.705948	101.532697	56.036020
2774.159895	115.412186	56.041025
2773.546817	108.885556	56.046029
2773.034631	111.948120	56.051034
2772.230017	116.422074	56.056039
2772.053162	115.517960	56.061044
2770.784043	114.471728	56.066049
2770.030766	114.027705	56.071053
2769.433877	111.122679	56.076058
2768.390988	114.180032	56.081063
2768.413538	106.456899	56.086068
2767.716285	114.642265	56.091073
2767.354294	113.587431	56.096077
2767.021009	110.505118	56.101082
2765.602252	112.969496	56.106087
2765.053590	113.277584	56.111092
2764.455509	108.301243	56.116097
2763.936189	118.631531	56.121101
2763.327994	108.819555	56.126106
2761.921747	116.273101	56.131111
2761.226243	104.445978	56.136116
2760.593121	107.536316	56.141121
2760.313266	108.722512	56.146125
2760.075295	106.774928	56.151130
2759.193139	112.066981	56.156135
2759.152009	115.460337	56.161140
2757.760933	111.029655	56.166145
2757.060931	115.469941	56.171149
2756.611632	115.510001	56.176154
2756.124950	111.541301	56.181159
2755.631828	112.618296	56.186164
2754.619154	119.924050	56.191169
2753.574059	109.371644	56.196173
2753.377566	113.370221	56.201178
2752.118380	117.293470	56.206183
2752.249660	110.838163	56.211188
2751.516766	114.089632	56.216193
2749.339381	113.352196	56.221197
2749.717083	114.815596	56.226202
2749.240860	116.976776	56.231207
2748.335952	107.713269	56.236212
2747.809621	120.275744	56.241217
2746.985553	114.221351	56.246221
2746.743989	113.351983	56.251226
2746.227750	122.823613	56.256231
2745.427049	113.569527	56.261236
2744.192114	119.524628	56.266241
2743.595311	117.911527	56.271245
2743.021744	111.011448	56.276250
2742.255454	114.511776	56.281255
2742.240371	108.036095	56.286260
2741.849814	124.482358	56.291265
2740.974782	113.739836	56.296269
2740.136695	110.760781	56.301274
2738.936544	109.262650	56.306279
2738.759452	106.812834	56.311284
2737.920764	111.588264	56.316289
2737.372808	109.969973	56.321293
2736.485663	115.335116	56.326298
2735.344332	119.212173	56.331303
2735.305079	114.889507	56.336308
2734.308575	124.682431	56.341313
2733.796187	112.922690	56.346317
2733.322828	116.006250	56.351322
2733.160098	120.256420	56.356327
2732.844934	109.153741	56.361332
2731.638069	113.994076	56.366337
2730.555170	114.084017	56.371341
2730.051302	116.420446	56.376346
2729.537098	110.519536	56.381351
2728.797756	109.361842	56.386356
2727.616125	122.667491	56.391361
2726.685977	110.829164	56.396365
2726.436781	118.309545	56.401370
2726.113705	123.440519	56.406375
2725.567836	115.458500	56.411380
2724.747521	124.183181	56.416385
2724.309520	118.597656	56.421389
2724.198716	114.577738	56.426394
2722.767842	118.151797	56.431399
2722.273491	110.487019	56.436404
2721.421063	111.640036	56.441409
2720.760612	108.700094	56.446413
2720.435872	110.349082	56.451418
2718.688347	120.172087	56.456423
2718.561509	112.975397	56.461428
2717.765078	115.958658	56.466433
2717.332793	112.302367	56.471437
2717.105581	108.114854	56.476442
2716.438086	116.520129	56.481447
2716.278925	106.767198	56.486452
2715.157186	113.162018	56.491457
2714.019953	114.919490	56.496461
2713.269483	117.708586	56.501466
2712.372970	115.974223	56.506471
2712.548999	110.767681	56.511476
2711.981982	111.803626	56.516481
2710.904145	107.965189	56.521485
2709.984961	112.474520	56.526490
2708.945007	114.817717	56.531495
2708.800795	101.118139	56.536500
2708.022653	107.987106	56.541505
2707.836006	108.677780	56.546509
2707.484397	112.056311	56.551514
2706.418013	114.961772	56.556519
2705.520779	111.442586	56.561524
2704.934573	114.761746	56.566529
2704.514111	118.595324	56.571533
2704.063396	113.973528	56.576538
2703.011131	119.085855	56.581543
2702.154259	106.453852	56.586548
2701.100119	122.876172	56.591553
2700.774365	120.259535	56.596557
2700.311702	114.899277	56.601562
2699.794585	111.092098	56.606567
2699.393704	107.058216	56.611572
2698.570704	114.001957	56.616577
2697.606394	114.960950	56.621581
2697.077786	109.071192	56.626586
2696.154850	116.925674	56.631591
2695.979727	111.551398	56.636596
2695.302113	126.296119	56.641601
2694.035469	113.478373	56.646605
2693.675779	110.607811	56.651610
2692.592153	120.733776	56.656615
2692.297828	105.791998	56.661620
2691.947290	111.003844	56.666625
2691.478937	119.822305	56.671629
2690.994092	109.742162	56.676634
2689.555196	115.925154	56.681639
2689.109077	106.668896	56.686644
2688.469319	120.818210	56.691649
2688.058130	116.345576	56.696653
2687.281041	114.265945	56.701658
2685.858055	115.727673	56.706663
2685.382184	112.876970	56.711668
2684.700822	111.898444	56.716673
2684.385223	112.467876	56.721677
2683.980548	117.317936	56.726682
2683.271138	121.134987	56.731687
2683.384339	111.119982	56.736692
2681.820756	116.136166	56.741697
2680.934656	114.773439	56.746701
2680.477305	114.114244	56.751706
2679.877336	107.841962	56.756711
2679.792613	110.504629	56.761716
2678.972841	113.821480	56.766721
2678.070092	107.798316	56.771725
2676.995157	113.663709	56.776730
2676.198462	109.664331	56.781735
2676.240642	108.430684	56.786740
2674.924717	112.283121	56.791745
2674.000242	106.537612	56.796749
2673.960293	113.693282	56.801754
2673.155158	118.924418	56.806759
2672.621852	105.300432	56.811764
2672.407441	114.789540	56.816769
2671.259319	105.468157	56.821773
2670.902123	111.886238	56.826778
2669.655132	112.279757	56.831783
2669.136330	107.737499	56.836788
2668.152133	113.369889	56.841793
2667.617257	106.533472	56.846797
2667.722656	109.140352	56.851802
2667.079963	115.165538	56.856807
2666.309110	101.652423	56.861812
2665.203909	109.104652	56.866817
2664.486147	109.752698	56.871821
2664.354874	106.893224	56.876826
2663.724817	107.766665	56.881831
2663.027870	104.351407	56.886836
2661.575755	109.260120	56.891841
2660.835374	103.893661	56.896845
2660.610612	110.396073	56.901850
2660.028396	112.259991	56.906855
2659.742652	110.723594	56.911860
2659.094255	104.626959	56.916865
2657.854170	99.548414	56.921869
2657.221795	108.679108	56.926874
2656.437822	116.404052	56.931879
2656.579605	108.078721	56.936884
2655.816554	115.475231	56.941889
2655.130549	110.799717	56.946893
2654.092663	105.414642	56.951898
2653.269523	112.861684	56.956903
2653.145990	100.724062	56.961908
2652.200367	107.352853	56.966913
2650.873819	102.358166	56.971917
2650.161020	104.829389	56.976922
2650.024283	103.926318	56.981927
2649.450120	103.062890	56.986932
2648.736181	112.631858	56.991937
2648.226574	105.781652	56.996941
2647.855954	102.536791	57.001946
2647.368440	112.269943	57.006951
2646.485686	106.076006	57.011956
2645.112055	109.912655	57.016961
2644.803746	114.160076	57.021965
2644.257864	111.422395	57.026970
2643.568560	109.370396	57.031975
2643.324925	106.634339	57.036980
2641.943929	114.676464	57.041985
2641.090826	104.870462	57.046989
2640.574365	102.910099	57.051994
2640.057165	102.721783	57.056999
2640.201334	104.577977	57.062004
2639.328671	113.695672	57.067009
2638.390515	106.997669	57.072013
2637.759765	108.561606	57.077018
2636.983929	107.976593	57.082023
2636.573479	109.537607	57.087028
2635.592408	106.294865	57.092033
2634.502118	101.006383	57.097037
2633.524103	99.975552	57.102042
2633.022735	109.953037	57.107047
2632.836037	103.517753	57.112052
2632.526875	111.359683	57.117057
2632.039146	102.139366	57.122061
2631.926089	102.100642	57.127066
2630.285151	107.625833	57.132071
2629.628581	103.825531	57.137076
2628.801277	104.087713	57.142081
2628.483986	108.007862	57.147085
2628.221608	96.649485	57.152090
2626.967839	110.815726	57.157095
2626.351038	100.886838	57.162100
2625.433097	103.141297	57.167105
2625.090714	115.515217	57.172109
2624.702888	101.196134	57.177114
2623.836634	106.882178	57.182119
2622.922580	103.754295	57.187124
2622.458422	105.977760	57.192129
2621.729855	99.187491	57.197133
2621.454041	103.001472	57.202138
2620.969611	111.247168	57.207143
2619.741449	99.847444	57.212148
2618.848306	106.173592	57.217153
2618.133930	100.650728	57.222157
2617.623346	96.541272	57.227162
2617.117653	104.682444	57.232167
2616.649326	101.545075	57.237172
2615.634589	104.619742	57.242177
2614.886001	109.517144	57.247181
2614.786940	106.487567	57.252186
2613.995719	107.743026	57.257191
2613.757685	100.475363	57.262196
2612.745951	109.096584	57.267201
2611.546252	105.994638	57.272205
2610.896180	104.468817	57.277210
2610.199443	117.434218	57.282215
2610.126957	102.576113	57.287220
2609.462369	107.617441	57.292225
2608.583200	104.378205	57.297229
2607.648147	102.305067	57.302234
2606.864279	108.548986	57.307239
2606.842546	101.606704	57.312244
2606.234813	108.257868	57.317249
2605.724667	107.918353	57.322253
2604.898219	108.013425	57.327258
2603.817598	111.895516	57.332263
2603.334418	108.727925	57.337268
2602.686364	114.909947	57.342273
2601.304481	110.760363	57.347277
2600.828598	109.869087	57.352282
2600.102070	121.557913	57.357287
2600.213490	109.136187	57.362292
2598.949319	113.990682	57.367297
2598.633783	115.486527	57.372301
2598.370330	114.919715	57.377306
2597.781787	110.081503	57.382311
2597.301822	113.763023	57.387316
2595.871582	104.955272	57.392321
2595.289885	106.976207	57.397325
2595.255062	106.710959	57.402330
2593.688261	114.589861	57.407335
2593.385204	111.163722	57.412340
2592.193688	116.964980	57.417345
2591.375014	117.551341	57.422349
2591.452875	109.504564	57.427354
2590.655870	110.083668	57.432359
2590.631347	105.422978	57.437364
2589.621507	111.680662	57.442369
2588.609945	108.208675	57.447373
2587.939295	109.711149	57.452378
2587.278078	111.222275	57.457383
2587.130457	106.406976	57.462388
2586.618642	112.084932	57.467393
2584.944677	107.796213	57.472397
2584.524571	112.943771	57.477402
2583.449722	108.902753	57.482407
2583.460686	104.410860	57.487412
2582.857039	112.617333	57.492417
2582.191122	106.003459	57.497421
2581.930852	110.880936	57.502426
2580.821311	111.664255	57.507431
2580.162689	109.440446	57.512436
2579.308895	110.844761	57.517441
2579.117976	106.499482	57.522445
2578.932933	100.236023	57.527450
2577.419855	109.927790	57.532455
2577.079899	104.615652	57.537460
2576.240149	116.602505	57.542465
2575.462014	106.227931	57.547469
2574.291771	104.981691	57.552474
2573.413495	114.277976	57.557479
2573.926387	103.539809	57.562484
2572.711214	109.626549	57.567489
2572.125513	116.521839	57.572493
2572.033858	110.262937	57.577498
2571.291964	106.247895	57.582503
2570.081600	99.063175	57.587508
2569.241839	111.110418	57.592513
2568.526261	110.935891	57.597517
2568.088231	104.145698	57.602522
2567.553958	109.814073	57.607527
2567.614902	103.181334	57.612532
2566.756769	105.557809	57.617537
2565.740443	103.475283	57.622541
2565.159052	107.445319	57.627546
2564.296168	111.838466	57.632551
2563.706216	107.343516	57.637556
2562.351741	107.734909	57.642561
2562.038984	113.232393	57.647565
2561.797744	102.800381	57.652570
2560.862761	117.857105	57.657575
2561.036233	104.299814	57.662580
2560.355623	105.932279	57.667585
2559.429296	105.285377	57.672589
2558.349102	96.882787	57.677594
2557.663624	105.579678	57.682599
2556.729672	101.561948	57.687604
2555.714663	108.772199	57.692609
2555.251890	105.729016	57.697613
2555.234192	102.106077	57.702618
2554.204122	110.057433	57.707623
2554.043431	102.993652	57.712628
2553.061672	110.362030	57.717633
2552.655921	111.407130	57.722637
2551.885605	106.873545	57.727642
2550.877343	106.498012	57.732647
2550.639478	102.994420	57.737652
2549.828704	115.592089	57.742657
2549.424059	115.459142	57.747661
2548.667970	109.367515	57.752666
2547.152958	115.851301	57.757671
2547.062137	106.073684	57.762676
2546.597177	109.950003	57.767681
2545.528182	110.028128	57.772685
2545.751410	108.285914	57.777690
2544.122035	104.378786	57.782695
2543.503252	106.627900	57.787700
2542.930668	110.186313	57.792705
2542.250032	109.517541	57.797709
2542.289850	100.286393	57.802714
2541.742454	109.215067	57.807719
2541.185847	103.029737	57.812724
2539.841274	95.640215	57.817729
2538.898513	103.962289	57.822733
2538.418062	106.814972	57.827738
2538.220966	110.102751	57.832743
2536.972877	97.861754	57.837748
2536.386933	105.286406	57.842753
2535.277331	111.266686	57.847757
2535.318976	102.351794	57.852762
2534.483986	105.287194	57.857767
2534.204988	93.161175	57.862772
2533.723553	100.282572	57.867777
2532.764815	96.638153	57.872781
2531.847279	98.950974	57.877786
2531.237444	103.456777	57.882791
2530.938953	96.836152	57.887796
2529.756299	102.457879	57.892801
2528.668623	101.910800	57.897805
2528.415453	103.935179	57.902810
2527.719555	109.414483	57.907815
2527.400065	100.186344	57.912820
2527.365676	102.042666	57.917825
2526.748572	107.350608	57.922829
2525.607938	100.666726	57.927834
2524.455991	106.424911	57.932839
2524.140883	102.583617	57.937844
2523.584326	103.707393	57.942849
2522.354210	105.954844	57.947853
2521.447242	109.058072	57.952858
2520.849832	107.941272	57.957863
2520.353836	99.659467	57.962868
2520.195852	100.719839	57.967873
2519.877343	100.580852	57.972877
2519.595439	97.923976	57.977882
2518.612610	105.067545	57.982887
2518.144928	105.538648	57.987892
2516.594289	107.898922	57.992897
2515.551919	107.676064	57.997901
2515.099952	101.397852	58.002906
2513.811677	108.860871	58.007911
2513.641071	104.529888	58.012916
2513.278537	112.000030	58.017921
2512.843579	112.276861	58.022925
2512.636597	109.958874	58.027930
2512.290065	111.699620	58.032935
2511.197860	101.598621	58.037940
2510.380649	109.258598	58.042945
2509.471420	104.342205	58.047949
2509.173140	107.846223	58.052954
2508.104015	108.109504	58.057959
2507.321245	104.042254	58.062964
2506.347662	115.619765	58.067969
2506.333823	109.892680	58.072973
2505.832225	103.984916	58.077978
2504.936049	113.913060	58.082983
2504.114142	106.804833	58.087988
2503.240014	114.843611	58.092993
2502.798641	107.174552	58.097997
2502.834876	105.148922	58.103002
2501.918217	109.919547	58.108007
2501.156683	103.431375	58.113012
2499.949625	111.230238	58.118017
2499.317027	112.702533	58.123021
2499.083645	112.246635	58.128026
2498.418713	114.649297	58.133031
2497.577496	109.071956	58.138036
2496.363587	109.097896	58.143041
2496.106308	107.343887	58.148045
2496.025415	101.400119	58.153050
2495.159249	112.045082	58.158055
2494.744239	115.773132	58.163060
2493.461856	104.770338	58.168065
2492.697668	107.549959	58.173069
2492.638314	94.629313	58.178074
2491.916119	113.191511	58.183079
2491.074713	105.347303	58.188084
2489.853459	107.146417	58.193089
2489.250203	114.386540	58.198093
2488.801450	106.744403	58.203098
2488.355020	116.530133	58.208103
2488.044398	108.580966	58.213108
2487.343956	105.414615	58.218113
2486.399629	106.429039	58.223117
2485.623710	102.831133	58.228122
2484.904140	110.147586	58.233127
2484.540266	102.678828	58.238132
2483.995666	112.000960	58.243137
2483.013691	113.901662	58.248141
2481.988409	109.008273	58.253146
2481.285989	111.308797	58.258151
2481.123809	110.330742	58.263156
2480.890544	114.437838	58.268161
2480.205876	114.689076	58.273165
2479.630501	118.375073	58.278170
2478.456963	115.856825	58.283175
2478.202359	108.787002	58.288180
2476.887957	117.402356	58.293185
2475.733382	111.018489	58.298189
2475.550702	112.045192	58.303194
2475.175879	114.211157	58.308199
2474.547342	111.765121	58.313204
2473.716850	104.872705	58.318209
2473.409136	107.978481	58.323213
2473.205504	105.357567	58.328218
2471.721025	114.369881	58.333223
2471.149331	103.587025	58.338228
2470.161245	109.487724	58.343233
2469.898882	107.858925	58.348237
2469.742926	98.115353	58.353242
2468.206723	107.767671	58.358247
2467.643277	101.712993	58.363252
2466.839306	106.962102	58.368257
2466.264026	112.676175	58.373261
2466.098361	104.171326	58.378266
2465.415011	107.699735	58.383271
2464.930512	104.459758	58.388276
2464.092038	109.075313	58.393281
2463.191604	109.836718	58.398285
2462.914157	109.806763	58.403290
2462.161880	119.563472	58.408295
2461.175073	104.113715	58.413300
2460.428478	100.399883	58.418305
2459.508966	116.617607	58.423309
2459.613732	95.817839	58.428314
2458.625364	103.697336	58.433319
2458.583563	106.573707	58.438324
2457.076793	103.909552	58.443329
2456.429187	103.820915	58.448333
2456.159257	101.021475	58.453338
2455.728455	112.081856	58.458343
2454.820556	93.528324	58.463348
2453.621629	104.381752	58.468353
2452.970410	101.991702	58.473357
2452.453815	105.056615	58.478362
2452.032151	106.504297	58.483367
2451.696401	94.021692	58.488372
2451.350086	112.481332	58.493377
2450.258548	105.792627	58.498381
2449.685088	101.193433	58.503386
2448.674305	114.213707	58.508391
2448.229752	102.462965	58.513396
2447.255050	99.463904	58.518401
2446.633898	96.032171	58.523405
2446.572939	91.900337	58.528410
2445.666973	102.953140	58.533415
2444.474905	94.246039	58.538420
2443.942332	99.314143	58.543425
2443.083157	103.938370	58.548429
2442.990246	98.869791	58.553434
2442.220513	107.755955	58.558439
2442.074033	88.396481	58.563444
2441.098445	97.664798	58.568449
2440.162887	101.320406	58.573453
2439.706021	102.898050	58.578458
2438.461582	103.955899	58.583463
2438.159476	101.247618	58.588468
2436.927481	107.490407	58.593473
2436.229318	98.231111	58.598477
2435.743260	92.756875	58.603482
2435.344985	111.255000	58.608487
2435.091379	91.560957	58.613492
2434.636608	92.742729	58.618497
2434.089201	102.633738	58.623501
2433.235089	100.789154	58.628506
2432.115207	105.710976	58.633511
2431.677798	102.512687	58.638516
2431.307367	98.801648	58.643521
2429.918157	100.473179	58.648525
2429.456023	101.143466	58.653530
2428.932723	104.560831	58.658535
2428.369891	98.401454	58.663540
2427.910542	100.212410	58.668545
2426.678697	97.725857	58.673549
2426.104334	104.827226	58.678554
2424.983104	106.334918	58.683559
2424.850465	95.893442	58.688564
2424.249714	98.995244	58.693569
2423.799025	110.263885	58.698573
2423.548994	102.707384	58.703578
2422.278846	102.457570	58.708583
2421.600422	97.459895	58.713588
2421.182281	105.846616	58.718593
2420.640284	101.915841	58.723597
2420.498867	94.228672	58.728602
2419.131148	99.654301	58.733607
2418.391449	96.452439	58.738612
2417.667198	107.182871	58.743617
2416.983490	104.372079	58.748621
2416.098959	103.284648	58.753626
2415.626018	100.575974	58.758631
2415.121065	91.672059	58.763636
2414.609396	96.191871	58.768641
2413.505653	99.385992	58.773645
2412.529139	88.038056	58.778650
2411.649968	103.532445	58.783655
2411.845889	97.807794	58.788660
2410.946465	95.460584	58.793665
2410.119215	98.519801	58.798669
2410.232436	86.299512	58.803674
2409.564291	97.605324	58.808679
2408.898818	90.906549	58.813684
2407.725216	100.989095	58.818689
2407.044790	94.069461	58.823693
2406.858733	92.032897	58.828698
2405.589948	87.776806	58.833703
2404.826251	91.637497	58.838708
2404.481129	95.430172	58.843713
2403.590116	93.052317	58.848717
2403.046469	90.723222	58.853722
2402.608176	92.697547	58.858727
2402.379769	87.640301	58.863732
2400.883117	95.147250	58.868737
2400.428448	96.298219	58.873741
2399.906170	93.255363	58.878746
2399.422518	92.066235	58.883751
2398.952166	97.020679	58.888756
2397.595872	97.538339	58.893761
2396.960307	91.519297	58.898765
2396.604535	90.045813	58.903770
2395.943272	103.166970	58.908775
2395.743450	93.438411	58.913780
2394.286583	95.437692	58.918785
2393.434243	98.805533	58.923789
2393.276650	97.807357	58.928794
2392.640119	99.926496	58.933799
2392.711996	90.608573	58.938804
2391.305211	99.857074	58.943809
2390.322343	94.413715	58.948813
2390.022408	88.692538	58.953818
2389.714855	100.356287	58.958823
2389.153087	94.221999	58.963828
2387.854969	94.012501	58.968833
2386.933263	93.302473	58.973837
2386.656690	97.471046	58.978842
2386.137640	98.520923	58.983847
2385.695891	94.754192	58.988852
2384.337365	98.147403	58.993857
2383.716523	102.668912	58.998861
2383.421981	99.178973	59.003866
2382.484763	104.963223	59.008871
2382.588457	89.951103	59.013876
2381.279806	96.194768	59.018881
2380.300403	107.163426	59.023885
2379.787845	94.832247	59.028890
2379.330788	99.675870	59.033895
2378.966525	97.809904	59.038900
2378.402773	103.653844	59.043905
2377.956206	97.639196	59.048909
2376.756326	104.329646	59.053914
2376.126468	113.785958	59.058919
2375.662974	96.588522	59.063924
2374.852276	99.628729	59.068929
2373.390054	97.161056	59.073933
2373.292024	94.870634	59.078938
2372.637107	104.663582	59.083943
2372.217077	97.732980	59.088948
2371.679595	100.317538	59.093953
2371.032537	91.394906	59.098957
2370.063401	95.812948	59.103962
2369.628676	94.928867	59.108967
2369.051179	89.508566	59.113972
2368.527450	92.527335	59.118977
2367.359207	94.048996	59.123981
2366.516028	95.402183	59.128986
2365.995926	98.613353	59.133991
2365.570850	99.352305	59.138996
2365.315589	96.266164	59.144001
2364.555707	93.941286	59.149005
2363.709020	97.219351	59.154010
2362.990416	97.594034	59.159015
2362.159660	98.651819	59.164020
2361.844364	92.904455	59.169025
2360.425969	97.529182	59.174029
2359.947999	95.671610	59.179034
2359.046667	99.830963	59.184039
2358.611893	92.081862	59.189044
2358.410130	100.445001	59.194049
2358.296020	98.513369	59.199053
2357.270148	91.145595	59.204058
2355.937504	100.574839	59.209063
2355.731205	90.664638	59.214068
2355.098003	101.559887	59.219073
2354.214745	100.761187	59.224077
2353.207337	87.029685	59.229082
2352.350870	96.926564	59.234087
2352.611377	91.098902	59.239092
2351.834726	89.268720	59.244097
2351.022593	98.853688	59.249101
2350.989716	93.921689	59.254106
2349.400231	96.008788	59.259111
2348.864624	94.062785	59.264116
2348.275365	104.613034	59.269121
2347.952321	99.283428	59.274125
2347.273320	99.291748	59.279130
2346.045007	101.323405	59.284135
2345.453873	91.038104	59.289140
2344.670932	96.347964	59.294145
2344.216824	96.850311	59.299149
2344.208859	96.036543	59.304154
2343.454730	89.502541	59.309159
2342.775072	90.691591	59.314164
2341.745545	91.583242	59.319169
2340.974051	102.937519	59.324173
2341.119808	88.739238	59.329178
2339.633270	94.948593	59.334183
2339.017101	84.172596	59.339188
2338.549461	89.784184	59.344193
2337.861863	89.563852	59.349197
2337.531474	88.412074	59.354202
2336.319273	97.279557	59.359207
2335.715025	97.823367	59.364212
2335.172453	99.350939	59.369217
2334.658651	89.576610	59.374221
2333.852348	87.842287	59.379226
2332.979908	99.355923	59.384231
2332.746861	96.912938	59.389236
2331.889125	90.861243	59.394241
2331.417596	89.411900	59.399245
2330.331781	85.959383	59.404250
2329.273133	94.733111	59.409255
2328.581881	85.497534	59.414260
2328.018827	88.723548	59.419265
2327.541225	89.512930	59.424269
2327.500150	84.192351	59.429274
2326.736630	93.609141	59.434279
2326.584032	88.694460	59.439284
2325.530600	87.972626	59.444289
2324.476230	99.876570	59.449293
2324.101252	84.227525	59.454298
2322.991470	100.928146	59.459303
2321.979483	94.872829	59.464308
2322.119840	96.948731	59.469313
2321.332392	94.143459	59.474317
2320.615445	88.842535	59.479322
2319.680186	93.257552	59.484327
2319.739000	92.823537	59.489332
2318.737427	98.433276	59.494337
2317.873904	100.921227	59.499341
2317.171210	96.917292	59.504346
2316.564225	105.918520	59.509351
2316.438795	91.000851	59.514356
2315.650290	98.432118	59.519361
2314.747637	102.311844	59.524365
2314.270672	95.535852	59.529370
2313.615274	97.274554	59.534375
2312.590681	87.197195	59.539380
2311.534707	89.958046	59.544385
2310.921927	91.706038	59.549389
2310.374375	89.853265	59.554394
2310.156104	92.318900	59.559399
2310.171203	86.249399	59.564404
2308.613284	86.119872	59.569409
2308.370127	89.955899	59.574413
2307.737919	85.627689	59.579418
2306.852926	97.035711	59.584423
2305.716046	92.164612	59.589428
2304.837495	94.149887	59.594433
2304.503562	92.453605	59.599437
2304.365204	81.889190	59.604442
2303.735086	94.529370	59.609447
2303.561826	86.883188	59.614452
2302.176576	88.335790	59.619457
2301.424686	88.070800	59.624461
2301.213399	82.889063	59.629466
2300.064465	91.789544	59.634471
2299.226820	88.775368	59.639476
2298.507081	89.776284	59.644481
2297.786526	92.666484	59.649485
2297.412112	83.218845	59.654490
2296.999340	91.174785	59.659495
2296.716281	82.817933	59.664500
2295.698406	90.599857	59.669505
2294.990493	93.007517	59.674509
2294.943939	83.994454	59.679514
2292.981680	90.990142	59.684519
2292.122256	91.336021	59.689524
2291.908173	90.568554	59.694529
2291.147433	91.607270	59.699533
2290.660638	88.785328	59.704538
2289.945213	94.815067	59.709543
2289.719145	91.773282	59.714548
2289.335380	95.220474	59.719553
2288.839183	94.646902	59.724557
2287.865565	87.342448	59.729562
2286.753024	98.481894	59.734567
2286.561867	88.292415	59.739572
2285.728026	86.091511	59.744577
2284.310554	86.602686	59.749581
2284.080439	83.538306	59.754586
2283.351729	94.974863	59.759591
2283.117510	85.478384	59.764596
2282.487071	89.303667	59.769601
2282.016881	92.173554	59.774605
2281.226183	86.919590	59.779610
2280.434522	92.539224	59.784615
2279.827447	85.468923	59.789620
2279.367904	87.139399	59.794625
2277.980615	92.433404	59.799629
2277.725216	86.329639	59.804634
2276.664025	94.528696	59.809639
2276.624399	89.464046	59.814644
2275.869178	91.477576	59.819649
2275.104533	100.150906	59.824653
2274.462177	99.039060	59.829658
2273.249752	95.142826	59.834663
2273.148449	96.836119	59.839668
2272.695095	95.884577	59.844673
2271.818047	98.011701	59.849677
2271.213389	96.810122	59.854682
2270.130384	95.782709	59.859687
2269.893314	86.739861	59.864692
2269.458984	82.764254	59.869697
2268.387716	95.352774	59.874701
2267.953450	94.611514	59.879706
2267.090409	100.202306	59.884711
2266.551321	84.662652	59.889716
2265.979146	90.548688	59.894721
2264.659050	96.766700	59.899725
2263.798692	86.799029	59.904730
2263.400521	93.907371	59.909735
2263.108025	86.870116	59.914740
2262.552613	81.807229	59.919745
2262.253088	91.179409	59.924750
2261.903862	85.764299	59.929754
2260.386159	101.930360	59.934759
2260.506354	91.343045	59.939764
2259.310699	88.689300	59.944769
2257.776244	90.046248	59.949774
2257.626321	81.488220	59.954778
2257.012895	92.423500	59.959783
2256.776864	85.643028	59.964788
2256.440129	83.697370	59.969793
2255.475312	91.610351	59.974798
2254.489646	80.033516	59.979802
2253.732365	95.760858	59.984807
2253.539899	92.472548	59.989812
2252.716572	96.940273	59.994817
2251.666437	99.464487	59.999822
2250.966428	89.330848	60.004826
2249.728208	88.091571	60.009831
2249.742033	93.921211	60.014836
2249.256489	96.012965	60.019841
2248.490577	92.738250	60.024846
2248.468347	93.840934	60.029850
2248.028114	101.559215	60.034855
2246.916577	97.905068	60.039860
2246.151149	96.993871	60.044865
2245.352326	96.168120	60.049870
2244.226778	83.765763	60.054874
2243.533840	99.934457	60.059879
2242.869721	90.442818	60.064884
2242.457853	98.665438	60.069889
2242.000519	94.611663	60.074894
2241.942433	91.742068	60.079898
2241.278634	96.127252	60.084903
2240.557182	100.539664	60.089908
2239.853607	98.790945	60.094913
2238.556306	103.338940	60.099918
2237.494268	87.447817	60.104922
2236.374536	95.086910	60.109927
2236.815417	89.542603	60.114932
2236.078695	94.415899	60.119937
2235.468233	94.719606	60.124942
2234.951384	92.243849	60.129946
2234.275913	98.537936	60.134951
2233.793222	94.906904	60.139956
2233.097049	95.277768	60.144961
2232.300302	99.011502	60.149966
2231.610109	93.574180	60.154970
2230.103973	106.602593	60.159975
2229.389330	95.818192	60.164980
2229.253513	97.380022	60.169985
2228.264761	96.118613	60.174990
2228.354363	95.939060	60.179994
2227.586211	99.996709	60.184999
2227.484416	100.200401	60.190004
2226.903207	103.492685	60.195009
2225.781621	97.738757	60.200014
2225.569559	94.023552	60.205018
2223.824478	98.804436	60.210023
2223.084926	96.688859	60.215028
2222.444295	94.851620	60.220033
2222.062190	93.637249	60.225038
2222.016013	90.326292	60.230042
2221.068741	99.079407	60.235047
2220.275473	88.943568	60.240052
2219.164892	98.517609	60.245057
2218.754965	100.146054	60.250062
2218.694790	98.344937	60.255066
2217.730393	98.612862	60.260071
2217.026394	89.851576	60.265076
2216.065720	95.597617	60.270081
2215.583272	90.371472	60.275086
2215.211477	88.960347	60.280090
2214.145835	89.753596	60.285095
2213.602662	89.065701	60.290100
2212.659109	95.975220	60.295105
2211.852955	94.959287	60.300110
2211.836299	92.323388	60.305114
2211.438149	94.617295	60.310119
2210.491748	95.723693	60.315124
2209.954668	88.819059	60.320129
2209.006733	89.262585	60.325134
2208.932904	89.670303	60.330138
2207.644169	101.501446	60.335143
2206.984087	93.625118	60.340148
2206.510277	93.666651	60.345153
2205.774647	92.522215	60.350158
2205.223512	88.287126	60.355162
2203.676595	96.052569	60.360167
2203.320392	85.158724	60.365172
2202.627342	87.370438	60.370177
2202.240426	92.695472	60.375182
2201.761632	83.363592	60.380186
2201.653938	95.039326	60.385191
2200.978847	90.234931	60.390196
2199.839568	87.687608	60.395201
2199.054007	98.031037	60.400206
2198.784894	87.494126	60.405210
2197.664022	95.826553	60.410215
2196.645371	97.880013	60.415220
2196.092957	89.300037	60.420225
2195.608071	90.439609	60.425230
2195.490274	93.432386	60.430234
2194.537006	85.932641	60.435239
2193.854931	87.696047	60.440244
2193.259384	94.789594	60.445249
2192.132843	95.872726	60.450254
2191.737517	88.274402	60.455258
2191.473716	92.241456	60.460263
2190.961443	87.390272	60.465268
2189.881855	90.145708	60.470273
2189.126070	91.913037	60.475278
2189.164858	87.391147	60.480282
2187.789204	89.181202	60.485287
2186.962490	84.619445	60.490292
2186.031223	86.975318	60.495297
2185.375752	90.626475	60.500302
2185.837402	84.482586	60.505306
2184.864995	87.899404	60.510311
2184.147767	88.017699	60.515316
2183.272546	87.021873	60.520321
2182.694899	86.741310	60.525326
2182.298963	87.473712	60.530330
2180.827257	91.805630	60.535335
2180.188281	87.269396	60.540340
2179.603953	85.698445	60.545345
2179.038338	92.493988	60.550350
2179.287548	83.003265	60.555354
2178.522374	85.441255	60.560359
2177.091383	89.162680	60.565364
2176.005943	89.799459	60.570369
2175.744862	94.461154	60.575374
2175.354064	81.837244	60.580378
2174.786815	94.288650	60.585383
2174.229188	90.788070	60.590388
2173.629915	95.837199	60.595393
2172.706792	97.462630	60.600398
2172.779459	89.912554	60.605402
2171.165759	90.812569	60.610407
2170.268536	95.361227	60.615412
2169.392215	82.997585	60.620417
2169.162438	91.224979	60.625422
2168.760502	87.067796	60.630426
2168.310738	90.538121	60.635431
2167.906322	88.844826	60.640436
2166.995439	86.799219	60.645441
2166.013191	89.871551	60.650446
2165.558970	76.030119	60.655450
2165.136353	84.984411	60.660455
2163.790893	82.301445	60.665460
2162.956187	83.117968	60.670465
2162.238246	90.765322	60.675470
2162.297625	95.319317	60.680474
2161.747346	92.410751	60.685479
2161.039306	89.601005	60.690484
2160.124034	87.690356	60.695489
2158.980973	80.869637	60.700494
2158.682711	83.626839	60.705498
2158.206965	90.755946	60.710503
2157.768773	91.642413	60.715508
2157.116931	90.915086	60.720513
2155.775662	88.776122	60.725518
2155.905462	91.504717	60.730522
2154.995168	91.002770	60.735527
2154.137207	88.535629	60.740532
2153.402984	90.346642	60.745537
2152.195687	93.790613	60.750542
2152.188718	82.647189	60.755546
2151.776870	100.371561	60.760551
2151.310558	87.073750	60.765556
2150.223770	88.274428	60.770561
2149.295329	87.674538	60.775566
2148.985861	88.710694	60.780570
2148.484451	91.808156	60.785575
2147.688287	91.708649	60.790580
2146.544956	86.708438	60.795585
2146.069821	86.150225	60.800590
2145.737424	90.167693	60.805594
2144.911438	88.427690	60.810599
2144.885552	89.980587	60.815604
2143.831091	92.665026	60.820609
2143.007145	98.787939	60.825614
2142.569425	87.099261	60.830618
2141.600784	94.138992	60.835623
2140.459512	95.152420	60.840628
2139.689417	86.400089	60.845633
2138.935511	94.213065	60.850638
2138.909320	89.423221	60.855642
2138.498033	93.698122	60.860647
2137.834746	89.179078	60.865652
2137.749924	83.673764	60.870657
2136.633904	93.868850	60.875662
2135.874900	85.355405	60.880666
2135.337140	91.310558	60.885671
2134.319146	91.496484	60.890676
2133.486538	93.869833	60.895681
2132.645159	93.491493	60.900686
2132.563956	87.612152	60.905690
2131.747335	85.789631	60.910695
2131.479166	90.259913	60.915700
2130.257367	93.683869	60.920705
2129.616060	98.207315	60.925710
2128.885894	82.103955	60.930714
2128.295453	95.463240	60.935719
2128.051449	88.041933	60.940724
2127.324440	99.335314	60.945729
2125.774193	99.409783	60.950734
2125.816499	86.784828	60.955738
2125.092543	92.735908	60.960743
2125.169336	87.822271	60.965748
2124.211331	90.874675	60.970753
2123.069284	91.922184	60.975758
2122.701664	94.670725	60.980762
2122.148108	90.338172	60.985767
2121.206636	95.023083	60.990772
2120.236541	96.002896	60.995777
2119.194445	89.720685	61.000782
2119.160221	91.191328	61.005786
2118.861218	97.352744	61.010791
2118.111827	83.862579	61.015796
2117.025569	88.843032	61.020801
2116.047332	95.628234	61.025806
2115.674209	98.145620	61.030810
2115.041862	97.270101	61.035815
2115.201964	94.072282	61.040820
2113.962503	88.437229	61.045825
2113.192241	99.875767	61.050830
2112.426439	97.915482	61.055834
2112.131872	95.264358	61.060839
2111.515637	96.248778	61.065844
2110.551500	89.087611	61.070849
2109.846880	93.378342	61.075854
2109.567720	87.889689	61.080858
2109.374062	97.407567	61.085863
2108.051945	86.532111	61.090868
2107.188287	102.416986	61.095873
2106.363362	107.021971	61.100878
2105.583497	94.812361	61.105882
2105.108465	99.114745	61.110887
2105.014269	99.491212	61.115892
2103.826145	99.225865	61.120897
2102.766999	99.306735	61.125902
2102.475465	96.457337	61.130906
2101.716428	99.952145	61.135911
2101.566556	104.230887	61.140916
2101.094458	99.728092	61.145921
2100.276918	101.285345	61.150926
2099.765379	97.724789	61.155930
2098.741917	92.548171	61.160935
2097.797133	101.940322	61.165940
2096.951059	90.604905	61.170945
2096.553840	96.306690	61.175950
2095.939077	98.216484	61.180954
2095.305778	91.835544	61.185959
2095.337438	89.254541	61.190964
2094.513474	96.532418	61.195969
2093.288509	102.520646	61.200974
2092.928343	94.953820	61.205978
2092.216425	95.655803	61.210983
2091.658495	93.388004	61.215988
2090.855082	94.343259	61.220993
2089.778354	103.430360	61.225998
2089.738845	89.095648	61.231002
2089.131689	97.823756	61.236007
2088.217415	98.734818	61.241012
2087.109653	95.965428	61.246017
2086.010779	99.912295	61.251022
2086.087568	94.576306	61.256026
2085.476788	94.715485	61.261031
2085.163677	92.112534	61.266036
2084.568818	97.947200	61.271041
2083.295990	102.097500	61.276046
2082.600728	90.824315	61.281050
2081.913545	96.642404	61.286055
2081.727927	91.425901	61.291060
2081.390020	102.501949	61.296065
2080.181059	100.654967	61.301070
2079.531790	95.136860	61.306074
2079.066127	101.545854	61.311079
2078.192729	95.686755	61.316084
2077.163003	103.744277	61.321089
2076.618540	103.741065	61.326094
2076.332382	94.186393	61.331098
2075.620196	105.434614	61.336103
2075.387379	96.318431	61.341108
2074.821496	98.721953	61.346113
2073.147278	104.600718	61.351118
2073.021351	87.862328	61.356122
2072.162984	93.783510	61.361127
2071.786807	88.744071	61.366132
2070.852657	93.568257	61.371137
2069.645869	102.950358	61.376142
2069.353146	88.856717	61.381146
2069.002096	94.281009	61.386151
2068.680611	89.825088	61.391156
2068.101777	90.252873	61.396161
2066.879387	106.936058	61.401166
2066.660162	92.958916	61.406170
2065.624402	99.964746	61.411175
2065.397311	91.995045	61.416180
2064.460892	94.309188	61.421185
2063.512108	99.165879	61.426190
2063.271283	92.808600	61.431194
2062.653232	96.867036	61.436199
2061.867176	98.605613	61.441204
2060.969186	93.431226	61.446209
2060.231451	104.431984	61.451214
2060.456055	94.404306	61.456218
2059.091674	95.675772	61.461223
2058.155539	105.707872	61.466228
2057.493656	98.680534	61.471233
2056.992131	99.157857	61.476238
2056.737271	94.476995	61.481242
2055.795628	101.937237	61.486247
2054.726180	99.564706	61.491252
2054.013619	103.646416	61.496257
2053.292207	110.449673	61.501262
2053.092467	99.213306	61.506266
2052.513689	101.329310	61.511271
2052.251429	92.963799	61.516276
2052.140053	93.489647	61.521281
2050.486290	98.162593	61.526286
2049.748753	96.289060	61.531290
2049.166105	99.017545	61.536295
2048.532739	98.403119	61.541300
2047.683848	90.457678	61.546305
2046.682578	99.714630	61.551310
2046.415407	90.136586	61.556314
2046.167801	102.998302	61.561319
2045.490536	90.908526	61.566324
2044.730776	90.012180	61.571329
2043.854554	92.966136	61.576334
2043.788905	93.793625	61.581338
2042.274142	95.004768	61.586343
2041.307686	93.919576	61.591348
2040.830467	93.597772	61.596353
2039.871408	85.527501	61.601358
2039.837726	81.984688	61.606362
2039.249810	103.271926	61.611367
2039.047668	95.698998	61.616372
2038.443478	88.432072	61.621377
2037.681055	92.180085	61.626382
2037.131177	92.128859	61.631386
2036.352262	94.792235	61.636391
2035.431639	86.675128	61.641396
2034.538732	92.376045	61.646401
2033.607074	91.597522	61.651406
2033.749732	84.920058	61.656410
2032.514619	95.782475	61.661415
2031.495626	89.004908	61.666420
2030.922645	85.029758	61.671425
2030.452193	90.289348	61.676430
2030.125065	84.440241	61.681434
2029.411910	85.188231	61.686439
2029.028027	81.586905	61.691444
2028.433927	93.827380	61.696449
2026.928801	92.773149	61.701454
2026.436034	92.413745	61.706458
2026.373383	95.755100	61.711463
2025.715754	91.442731	61.716468
2024.850253	86.627125	61.721473
2023.817525	89.305497	61.726478
2023.597555	84.877217	61.731482
2022.963510	92.954685	61.736487
2022.079186	95.702011	61.741492
2021.465851	91.927178	61.746497
2020.734164	92.617551	61.751502
2020.240904	88.171283	61.756506
2019.642578	97.056559	61.761511
2018.618588	94.554292	61.766516
2017.916232	88.725555	61.771521
2017.100068	89.390118	61.776526
2016.252055	88.024154	61.781530
2016.086709	90.500081	61.786535
2015.872802	88.966442	61.791540
2014.997094	85.513980	61.796545
2013.990308	88.243967	61.801550
2013.620289	90.087430	61.806554
2013.357492	92.418586	61.811559
2012.402824	87.221145	61.816564
2011.088244	86.368395	61.821569
2010.389937	96.555198	61.826574
2010.291506	89.328075	61.831578
2009.801663	93.998902	61.836583
2009.284238	100.942521	61.841588
2007.705863	93.189368	61.846593
2007.270946	96.686371	61.851598
2006.983613	91.908837	61.856602
2006.121849	93.387618	61.861607
2005.830368	95.868939	61.866612
2005.350925	91.521751	61.871617
2004.084166	94.572121	61.876622
2004.079499	89.999647	61.881626
2003.250214	94.277766	61.886631
2002.003162	91.703927	61.891636
2001.280063	88.971386	61.896641
2000.331373	103.315208	61.901646
2000.212660	92.732864	61.906650
1999.327610	93.583680	61.911655
1999.308356	90.058531	61.916660
1998.979741	94.481524	61.921665
1997.698997	98.946603	61.926670
1997.412549	93.255532	61.931674
1996.403034	98.319190	61.936679
1995.447170	91.987131	61.941684
1995.030981	90.958208	61.946689
1994.213238	98.458442	61.951694
1994.074314	90.001189	61.956698
1993.309784	89.437627	61.961703
1992.393349	81.206138	61.966708
1991.199708	87.052445	61.971713
1990.379112	95.904693	61.976718
1990.071534	90.907606	61.981722
1989.527916	94.619380	61.986727
1989.097528	87.593118	61.991732
1989.097741	87.288331	61.996737
1987.756997	89.802696	62.001742
1987.530504	81.234116	62.006746
1986.481054	80.971916	62.011751
1985.861741	86.187500	62.016756
1984.708810	83.452309	62.021761
1984.080350	87.555159	62.026766
1983.898225	83.348558	62.031770
1983.137390	90.771162	62.036775
1982.836491	82.475037	62.041780
1982.159120	81.827492	62.046785
1980.956412	86.771834	62.051790
1980.636274	80.181042	62.056794
1980.212387	82.282395	62.061799
1978.846103	81.971767	62.066804
1978.035962	76.763825	62.071809
1977.218015	78.934165	62.076814
1976.986402	79.437557	62.081818
1976.542209	92.318676	62.086823
1976.249463	86.260017	62.091828
1975.785460	79.118331	62.096833
1974.988860	88.635523	62.101838
1974.243100	88.412951	62.106842
1973.239690	85.063656	62.111847
1972.216465	82.432591	62.116852
1971.733453	78.441667	62.121857
1970.790132	88.759585	62.126862
1970.651913	88.410981	62.131866
1970.042319	85.293913	62.136871
1969.354620	91.538000	62.141876
1968.548315	93.454519	62.146881
1967.762722	92.897722	62.151886
1967.829849	84.967705	62.156890
1966.830172	86.943354	62.161895
1966.224688	87.253739	62.166900
1965.245227	82.739473	62.171905
1965.140815	84.044101	62.176910
1964.355161	88.136739	62.181914
1963.143863	82.222978	62.186919
1962.409482	84.667173	62.191924
1962.006909	85.221520	62.196929
1961.320603	88.185629	62.201934
1960.770652	81.135223	62.206938
1959.943345	89.585606	62.211943
1959.355144	85.522680	62.216948
1958.665382	77.139141	62.221953
1957.616080	85.640918	62.226958
1957.654499	79.748631	62.231962
1956.362451	82.982932	62.236967
1955.390568	89.329316	62.241972
1954.785136	71.967627	62.246977
1954.311345	84.757490	62.251982
1954.367184	80.482948	62.256986
1953.590928	86.677055	62.261991
1953.282187	78.918704	62.266996
1952.768049	80.710642	62.272001
1951.237587	83.013926	62.277006
1951.053601	76.980877	62.282010
1950.054226	82.520415	62.287015
1949.041486	75.771015	62.292020
1948.773645	89.200228	62.297025
1948.086344	86.377892	62.302030
1947.819927	81.296407	62.307034
1947.008212	80.862498	62.312039
1946.369953	81.948988	62.317044
1945.506653	79.049003	62.322049
1944.390372	83.901200	62.327054
1944.426662	82.931057	62.332058
1943.351475	87.784120	62.337063
1942.509645	79.333444	62.342068
1942.146338	80.448685	62.347073
1941.506093	87.320155	62.352078
1941.269998	76.062017	62.357082
1940.283894	82.863578	62.362087
1939.499886	88.422327	62.367092
1939.013705	80.618546	62.372097
1937.899427	80.226135	62.377102
1937.871249	78.736516	62.382106
1936.946933	87.634136	62.387111
1936.125466	79.217081	62.392116
1935.601924	84.722587	62.397121
1934.698084	87.789041	62.402126
1934.569026	78.457384	62.407130
1932.989552	86.112398	62.412135
1932.434190	84.229430	62.417140
1932.003763	78.351431	62.422145
1931.485444	86.484888	62.427150
1931.198378	88.119172	62.432154
1930.574513	77.513926	62.437159
1929.913501	78.592468	62.442164
1929.071620	84.801750	62.447169
1928.035598	82.821411	62.452174
1927.902897	81.930702	62.457178
1927.458904	76.791181	62.462183
1926.525233	83.183526	62.467188
1925.693883	84.629090	62.472193
1924.538599	85.938630	62.477198
1924.444369	78.569097	62.482202
1923.803147	83.451340	62.487207
1922.970435	77.507957	62.492212
1922.126730	79.646397	62.497217
1921.138242	88.189090	62.502222
1921.152486	83.622466	62.507226
1920.680918	87.423755	62.512231
1919.901934	82.337593	62.517236
1918.744997	81.427900	62.522241
1918.079624	85.616409	62.527246
1918.115664	93.355835	62.532250
1917.325574	84.795261	62.537255
1916.389209	84.175454	62.542260
1915.522383	86.422846	62.547265
1914.753296	86.447027	62.552270
1914.527641	82.086832	62.557274
1914.120363	82.398050	62.562279
1913.417806	81.190372	62.567284
1912.797399	70.940977	62.572289
1911.860449	87.026260	62.577294
1911.303804	77.549474	62.582298
1910.182320	85.006147	62.587303
1909.594561	85.690465	62.592308
1909.319631	86.307450	62.597313
1908.556205	84.349163	62.602318
1908.636570	76.080982	62.607322
1907.194011	85.284753	62.612327
1906.744170	82.119444	62.617332
1906.263157	77.459529	62.622337
1905.085548	82.502612	62.627342
1904.687903	84.438434	62.632346
1903.760996	86.255992	62.637351
1903.028257	75.151112	62.642356
1902.748263	81.513733	62.647361
1901.293042	82.287245	62.652366
1900.918940	81.585855	62.657370
1900.290616	81.049531	62.662375
1899.623952	82.111281	62.667380
1899.084696	81.794578	62.672385
1898.931170	81.569775	62.677390
1898.507362	72.418414	62.682394
1897.051868	70.823254	62.687399
1896.265964	82.684047	62.692404
1896.194041	78.931477	62.697409
1895.175800	78.288971	62.702414
1895.577328	72.173919	62.707418
1894.327049	83.503919	62.712423
1892.941154	79.534447	62.717428
1892.359158	70.840002	62.722433
1891.560916	83.214070	62.727438
1891.331378	77.658143	62.732442
1889.855811	83.009560	62.737447
1889.548240	82.543095	62.742452
1888.670875	76.342107	62.747457
1888.408660	90.195073	62.752462
1888.140931	84.237931	62.757466
1887.762876	83.576690	62.762471
1887.322079	76.086854	62.767476
1886.567110	78.527868	62.772481
1885.464602	81.736468	62.777486
1885.082856	73.806679	62.782490
1883.952068	84.105358	62.787495
1882.909915	81.432554	62.792500
1882.615111	75.721617	62.797505
1881.897315	86.207790	62.802510
1881.654437	79.678396	62.807514
1881.206765	80.683736	62.812519
1880.045482	80.814096	62.817524
1879.280847	73.909379	62.822529
1878.702216	84.702125	62.827534
1878.408630	78.288376	62.832538
1877.270933	80.826051	62.837543
1876.368762	82.435311	62.842548
1876.270249	81.512703	62.847553
1875.592579	78.177174	62.852558
1875.791369	66.798077	62.857562
1874.389998	77.907223	62.862567
1873.422106	80.141518	62.867572
1873.089216	75.916117	62.872577
1871.928395	81.815640	62.877582
1871.297886	75.672289	62.882586
1870.395691	79.545277	62.887591
1869.953344	83.611558	62.892596
1870.009105	84.274597	62.897601
1869.065144	91.717486	62.902606
1868.396678	78.926419	62.907610
1867.447406	89.493643	62.912615
1866.775549	85.732399	62.917620
1866.442699	70.943868	62.922625
1865.449042	85.574042	62.927630
1864.417159	80.848909	62.932634
1863.490045	81.825359	62.937639
1863.047447	78.931964	62.942644
1862.842925	83.189653	62.947649
1862.283388	82.525122	62.952654
1862.092480	78.213855	62.957658
1861.852683	73.205587	62.962663
1860.362167	72.506524	62.967668
1859.829455	75.635802	62.972673
1858.935797	81.791581	62.977678
1858.490586	78.908107	62.982682
1857.447161	79.267772	62.987687
1856.891306	75.719967	62.992692
1856.775585	84.620168	62.997697
1855.565052	87.259122	63.002702
1854.719097	77.973155	63.007706
1853.659874	83.365451	63.012711
1853.384250	79.009075	63.017716
1853.106503	82.562083	63.022721
1852.650484	84.180277	63.027726
1852.076622	79.051142	63.032730
1851.094200	76.043271	63.037735
1849.994594	76.060459	63.042740
1849.868686	74.428094	63.047745
1849.313840	78.044299	63.052750
1848.748377	77.277367	63.057754
1847.406878	86.982521	63.062759
1846.825749	85.201468	63.067764
1846.600345	78.239238	63.072769
1845.965258	79.161781	63.077774
1845.404586	73.902898	63.082778
1844.485822	80.494008	63.087783
1843.882028	82.239717	63.092788
1843.448134	74.239123	63.097793
1841.692812	83.203925	63.102798
1841.130063	74.071213	63.107802
1840.402644	77.611947	63.112807
1840.046267	80.823554	63.117812
1839.867212	81.242963	63.122817
1839.271479	80.748831	63.127822
1839.067053	72.114926	63.132826
1838.868736	91.363048	63.137831
1837.876379	81.346241	63.142836
1836.927917	79.103452	63.147841
1835.818509	83.740947	63.152846
1834.898913	66.987633	63.157850
1834.025884	82.601731	63.162855
1833.817942	80.597365	63.167860
1833.293428	77.974162	63.172865
1832.136653	83.373283	63.177870
1831.335820	76.028340	63.182874
1830.691410	87.515603	63.187879
1829.978826	74.787754	63.192884
1829.854489	73.547869	63.197889
1829.356814	88.771320	63.202894
1829.415690	85.586087	63.207898
1828.597979	90.077366	63.212903
1827.812595	84.751932	63.217908
1827.015607	75.735479	63.222913
1825.301970	85.851660	63.227918
1824.876768	82.020594	63.232922
1824.149671	87.434226	63.237927
1823.436444	82.313940	63.242932
1823.478551	81.799100	63.247937
1822.734127	79.857707	63.252942
1822.606491	69.748621	63.257946
1821.432360	80.429704	63.262951
1820.776937	82.803565	63.267956
1820.447931	79.390235	63.272961
1819.031827	97.305725	63.277966
1818.081180	83.593117	63.282970
1817.413885	83.991064	63.287975
1817.080177	79.982510	63.292980
1816.833450	86.978493	63.297985
1816.359455	85.588440	63.302990
1816.176204	79.657905	63.307994
1814.983030	81.997461	63.312999
1813.886596	79.511189	63.318004
1813.552450	76.339519	63.323009
1812.143117	82.536954	63.328014
1811.308456	75.975009	63.333018
1811.404020	83.127549	63.338023
1811.092126	84.350049	63.343028
1810.434836	77.311722	63.348033
1809.621069	88.936115	63.353038
1808.495572	73.701787	63.358042
1807.909604	87.323567	63.363047
1807.102013	79.737820	63.368052
1807.079821	76.245946	63.373057
1806.102084	92.468076	63.378062
1805.729021	83.320674	63.383066
1804.962736	75.212358	63.388071
1804.109286	84.830463	63.393076
1804.065625	79.892453	63.398081
1802.718253	89.070089	63.403086
1802.356653	87.845931	63.408090
1801.781868	82.974320	63.413095
1801.078544	79.480962	63.418100
1800.060980	81.953494	63.423105
1798.682367	89.284842	63.428110
1798.389926	82.744990	63.433114
1797.780243	82.394165	63.438119
1797.410134	83.074017	63.443124
1796.914535	91.397793	63.448129
1796.207607	82.392381	63.453134
1796.129135	77.660451	63.458138
1795.133755	80.982180	63.463143
1794.289269	91.282017	63.468148
1793.944003	80.985567	63.473153
1792.859528	86.938355	63.478158
1791.905551	80.335250	63.483162
1791.196538	87.379145	63.488167
1790.390798	86.239663	63.493172
1790.290690	86.547675	63.498177
1789.806098	87.807619	63.503182
1789.394500	83.912652	63.508186
1788.508583	83.699088	63.513191
1787.875786	80.359448	63.518196
1787.442970	77.233477	63.523201
1786.120515	83.257376	63.528206
1785.556153	83.092606	63.533210
1784.899236	78.659770	63.538215
1784.517953	82.154314	63.543220
1783.895978	83.266850	63.548225
1782.890998	87.966615	63.553230
1782.192632	76.544449	63.558234
1781.728275	82.644941	63.563239
1781.293518	83.655184	63.568244
1780.840362	81.119643	63.573249
1779.531144	89.239614	63.578254
1779.147804	86.525160	63.583258
1778.271177	84.199042	63.588263
1777.945992	83.359824	63.593268
1776.816117	85.118976	63.598273
1775.515686	86.439566	63.603278
1775.372538	83.301927	63.608282
1775.372312	87.785571	63.613287
1774.756793	80.618529	63.618292
1774.021362	72.908346	63.623297
1773.000949	80.607468	63.628302
1772.198060	82.587372	63.633306
1771.606793	82.609964	63.638311
1771.155005	81.677544	63.643316
1770.982890	80.011248	63.648321
1769.596288	82.342858	63.653326
1769.090678	73.389851	63.658330
1768.409336	79.239717	63.663335
1767.893498	78.510486	63.668340
1767.384339	74.051584	63.673345
1765.995470	78.482310	63.678350
1765.214329	80.069694	63.683354
1764.702768	87.754383	63.688359
1764.371989	79.493404	63.693364
1764.420098	80.582075	63.698369
1763.694072	82.139109	63.703374
1762.588118	72.090058	63.708378
1761.979567	77.963783	63.713383
1761.195531	81.051601	63.718388
1760.739322	71.812656	63.723393
1759.499590	78.749996	63.728398
1758.821689	79.965257	63.733402
1758.175719	88.609222	63.738407
1757.745786	86.962961	63.743412
1757.530182	81.453214	63.748417
1757.099755	80.961991	63.753422
1756.161672	76.354647	63.758426
1755.363749	72.618154	63.763431
1754.553341	80.969343	63.768436
1754.667293	77.724559	63.773441
1753.725503	84.777101	63.778446
1752.846533	83.513582	63.783450
1751.617828	85.307806	63.788455
1750.396121	87.791200	63.793460
1750.797000	81.343899	63.798465
1749.709094	92.022875	63.803470
1749.309679	82.622240	63.808474
1748.835842	89.340121	63.813479
1748.223342	78.176023	63.818484
1747.533980	86.710574	63.823489
1746.323374	84.425030	63.828494
1745.984029	80.660595	63.833498
1745.415395	85.455434	63.838503
1745.020033	83.633925	63.843508
1744.350297	88.085289	63.848513
1743.090846	86.247426	63.853518
1742.699849	82.389597	63.858522
1742.243822	84.305419	63.863527
1741.602162	80.521269	63.868532
1740.466928	81.798601	63.873537
1739.535009	90.096774	63.878542
1739.459502	85.721955	63.883546
1739.067152	86.878097	63.888551
1738.225349	90.703668	63.893556
1737.318136	84.349143	63.898561
1736.374579	83.415217	63.903566
1736.125704	82.624126	63.908570
1735.374727	81.840005	63.913575
1735.239600	87.016965	63.918580
1734.364587	78.799378	63.923585
1733.507837	84.682815	63.928590
1732.952882	85.710076	63.933594
1732.315133	85.550764	63.938599
1731.025355	87.250053	63.943604
1730.530600	85.218588	63.948609
1729.541139	77.795422	63.953614
1729.138885	78.665507	63.958618
1729.171415	82.805268	63.963623
1728.823097	80.190218	63.968628
1727.943582	84.661294	63.973633
1726.653590	94.130299	63.978638
1726.390118	83.697106	63.983642
1725.771892	77.198405	63.988647
1724.921512	80.809136	63.993652
1724.051778	80.150727	63.998657
1723.351364	85.309154	64.003662
1723.037284	75.389473	64.008666
1722.502650	84.568573	64.013671
1721.621991	76.061443	64.018676
1720.548189	77.473130	64.023681
1719.886735	88.793975	64.028686
1719.790967	81.735368	64.033690
1719.348053	81.051688	64.038695
1718.266976	78.830037	64.043700
1717.294609	77.182655	64.048705
1716.600122	72.952832	64.053710
1716.227279	67.023176	64.058714
1715.756381	80.572759	64.063719
1715.225837	79.180551	64.068724
1714.229923	75.997395	64.073729
1713.336088	88.039289	64.078734
1713.007538	74.924063	64.083738
1712.215340	77.267261	64.088743
1712.197491	81.810361	64.093748
1711.355139	76.624566	64.098753
1710.218643	80.052556	64.103758
1709.865479	71.534509	64.108762
1709.181389	80.419062	64.113767
1707.815492	74.511308	64.118772
1707.265385	77.890274	64.123777
1706.672344	80.952126	64.128782
1706.465246	73.237603	64.133786
1705.675091	83.160658	64.138791
1705.822942	77.990946	64.143796
1704.858063	74.474074	64.148801
1703.602371	75.956360	64.153806
1703.202921	73.673339	64.158810
1702.693392	78.777393	64.163815
1701.334871	79.634276	64.168820
1700.993779	72.820145	64.173825
1699.907194	79.470774	64.178830
1699.823186	68.153108	64.183834
1699.675461	80.448626	64.188839
1698.582062	81.870381	64.193844
1697.886663	72.620667	64.198849
1696.901130	78.592060	64.203854
1696.345479	77.563741	64.208858
1696.119666	81.284305	64.213863
1695.013596	75.176180	64.218868
1694.507113	71.857967	64.223873
1693.672530	79.844627	64.228878
1693.387183	74.653126	64.233882
1692.982407	86.293584	64.238887
1691.741354	86.696572	64.243892
1691.046626	76.753219	64.248897
1690.291463	80.647649	64.253902
1689.952654	68.019694	64.258906
1689.693295	75.001645	64.263911
1688.423863	81.571465	64.268916
1687.885247	77.974157	64.273921
1687.009987	79.766727	64.278926
1686.943551	72.717714	64.283930
1686.049725	78.434214	64.288935
1684.643353	78.206705	64.293940
1684.382066	77.933640	64.298945
1683.224828	79.205277	64.303950
1683.308566	73.368802	64.308954
1683.242063	75.356125	64.313959
1682.065792	77.747286	64.318964
1681.536087	72.076175	64.323969
1680.653713	78.103335	64.328974
1680.378903	75.006785	64.333978
1679.144977	71.003876	64.338983
1678.214830	76.755407	64.343988
1677.888273	67.831385	64.348993
1677.256363	76.369917	64.353998
1676.921563	66.275383	64.359002
1676.382563	71.757489	64.364007
1675.397700	73.570394	64.369012
1675.031024	70.105108	64.374017
1674.051394	78.753273	64.379022
1673.079140	73.161049	64.384026
1672.611153	75.955594	64.389031
1671.269156	81.978516	64.394036
1671.195384	83.062779	64.399041
1670.409082	81.268308	64.404046
1670.101460	73.141931	64.409050
1669.633305	85.376629	64.414055
1668.993959	80.284781	64.419060
1668.193507	77.795657	64.424065
1666.957897	83.297107	64.429070
1666.917778	81.654412	64.434074
1666.581822	83.040108	64.439079
1665.458402	78.912507	64.444084
1664.511774	83.223766	64.449089
1664.149522	72.239097	64.454094
1664.024026	67.102744	64.459098
1662.544114	73.385306	64.464103
1661.433212	80.762045	64.469108
1661.281454	76.578300	64.474113
1660.638877	81.599339	64.479118
1660.841889	80.747898	64.484122
1660.062395	84.387559	64.489127
1659.200070	81.693901	64.494132
1657.874500	76.393052	64.499137
1656.899417	77.236434	64.504142
1656.790416	67.969673	64.509146
1656.161270	81.036355	64.514151
1655.669295	85.887157	64.519156
1654.646693	72.338104	64.524161
1654.107856	78.237799	64.529166
1654.098510	72.853026	64.534170
1653.680518	72.515994	64.539175
1652.322209	76.746917	64.544180
1651.647193	72.281679	64.549185
1650.786435	81.863939	64.554190
1650.330443	68.629229	64.559194
1649.672030	72.482632	64.564199
1648.946548	72.882663	64.569204
1648.716119	71.842511	64.574209
1647.322867	75.119456	64.579214
1646.798268	71.763694	64.584218
1646.284712	72.935845	64.589223
1645.793267	74.193814	64.594228
1645.357036	63.247472	64.599233
1643.509132	75.271447	64.604238
1642.772046	79.265020	64.609242
1642.776289	77.137518	64.614247
1642.542323	83.609096	64.619252
1641.999461	63.774147	64.624257
1641.198658	70.157597	64.629262
1640.488851	71.306492	64.634266
1639.666004	80.708192	64.639271
1638.982605	72.487448	64.644276
1638.753703	67.333662	64.649281
1637.871045	82.100364	64.654286
1636.580764	74.157149	64.659290
1635.881819	86.113986	64.664295
1635.393618	89.488680	64.669300
1635.500205	85.089417	64.674305
1634.668468	91.102395	64.679310
1634.117468	84.078674	64.684314
1632.970895	84.576029	64.689319
1632.231496	85.227117	64.694324
1632.109323	76.867306	64.699329
1630.799792	83.282163	64.704334
1630.214599	80.681607	64.709338
1629.457910	76.390210	64.714343
1628.719035	82.210065	64.719348
1628.498775	81.842354	64.724353
1628.005665	80.723213	64.729358
1627.481728	74.468122	64.734362
1626.509187	77.561372	64.739367
1625.881912	74.451331	64.744372
1625.456187	75.984621	64.749377
1624.360376	76.024495	64.754382
1623.619507	74.148051	64.759386
1623.139578	83.747244	64.764391
1622.231622	85.757384	64.769396
1622.443891	81.444244	64.774401
1621.174267	74.571531	64.779406
1620.095506	67.404856	64.784410
1619.274069	70.685396	64.789415
1619.057369	78.842233	64.794420
1618.707820	72.749530	64.799425
1618.418349	84.933121	64.804430
1618.145453	73.580684	64.809434
1616.742477	70.441555	64.814439
1615.623598	68.580067	64.819444
1615.453981	71.026331	64.824449
1614.336306	77.008110	64.829454
1613.585847	76.669952	64.834458
1613.421463	76.685821	64.839463
1612.599256	87.885366	64.844468
1612.295440	72.643915	64.849473
1610.952604	83.910054	64.854478
1610.348836	84.578196	64.859482
1609.986107	75.408144	64.864487
1609.352921	77.701250	64.869492
1609.223325	73.420564	64.874497
1607.937652	86.922087	64.879502
1607.292079	75.831182	64.884506
1606.314760	74.849773	64.889511
1605.867102	83.702554	64.894516
1605.598110	75.635887	64.899521
1604.144036	85.655988	64.904526
1603.762961	73.353029	64.909530
1603.608198	80.016305	64.914535
1602.888677	76.222609	64.919540
1602.572179	68.323148	64.924545
1601.222832	81.035863	64.929550
1600.362868	72.674429	64.934554
1599.831905	76.013417	64.939559
1599.598496	72.328761	64.944564
1599.243697	67.034690	64.949569
1597.959611	75.528129	64.954574
1597.436342	72.430687	64.959578
1597.065275	72.701391	64.964583
1596.396498	78.018615	64.969588
1595.059807	73.178748	64.974593
1594.432571	85.322646	64.979598
1594.003568	75.932238	64.984602
1593.369167	69.846842	64.989607
1592.828281	71.461813	64.994612
1592.612121	74.098798	64.999617
1591.414598	66.712860	65.004622
1590.778673	62.040824	65.009626
1590.226532	80.155416	65.014631
1589.577745	81.199932	65.019636
1588.803611	75.009770	65.024641
1587.540599	75.095238	65.029646
1587.504282	72.888630	65.034650
1586.811247	64.774151	65.039655
1586.641632	73.075287	65.044660
1585.634446	78.302010	65.049665
1584.614119	78.420944	65.054670
1584.263714	74.432247	65.059674
1583.874732	77.767858	65.064679
1582.762337	70.947196	65.069684
1582.208574	74.808747	65.074689
1581.340279	78.921882	65.079694
1580.902144	77.880965	65.084698
1580.211640	82.654039	65.089703
1579.555010	76.809278	65.094708
1578.860590	75.767619	65.099713
1577.854669	87.182149	65.104718
1577.550953	72.564741	65.109722
1577.226349	70.287081	65.114727
1576.697952	73.674970	65.119732
1575.678278	70.818004	65.124737
1574.762480	79.305656	65.129742
1574.702780	73.811089	65.134746
1574.151222	74.812126	65.139751
1572.600563	77.973535	65.144756
1572.172527	72.832519	65.149761
1571.413719	76.556275	65.154766
1571.134507	69.750520	65.159770
1570.826530	69.080865	65.164775
1569.594880	74.290349	65.169780
1568.701513	76.730218	65.174785
1567.988811	78.363150	65.179790
1567.482689	79.368254	65.184794
1567.290615	75.894412	65.189799
1566.304192	80.321437	65.194804
1565.857879	81.202231	65.199809
1564.632753	81.443451	65.204814
1564.642881	71.830273	65.209818
1564.010052	71.170821	65.214823
1562.926744	78.469432	65.219828
1562.546355	70.489335	65.224833
1561.352005	81.777828	65.229838
1561.067141	75.500780	65.234842
1560.604714	80.213506	65.239847
1559.516147	79.150097	65.244852
1558.925764	71.809465	65.249857
1557.655301	80.807007	65.254862
1557.886135	84.688621	65.259866
1557.508137	77.828326	65.264871
1556.764410	74.889403	65.269876
1555.864690	73.396982	65.274881
1554.785114	81.778067	65.279886
1554.546548	72.501912	65.284890
1554.453717	76.760612	65.289895
1553.267519	73.697687	65.294900
1552.756863	66.808393	65.299905
1551.793110	77.114040	65.304910
1551.373801	71.649443	65.309914
1550.212898	75.145977	65.314919
1548.957336	73.470521	65.319924
1548.875283	73.441119	65.324929
1547.845642	81.939969	65.329934
1547.899497	75.326675	65.334938
1547.359257	74.771374	65.339943
1547.152277	73.878391	65.344948
1546.651798	76.638638	65.349953
1545.553966	80.649752	65.354958
1545.338885	72.747545	65.359962
1544.040911	76.371745	65.364967
1542.956975	76.155010	65.369972
1542.778062	74.610280	65.374977
1541.842578	74.031442	65.379982
1541.045512	72.153183	65.384986
1539.994569	74.641339	65.389991
1539.508369	75.528173	65.394996
1539.256596	71.268007	65.400001
1538.579129	83.221955	65.405006
1538.370945	74.615967	65.410010
1537.671780	78.573851	65.415015
1536.616655	80.381044	65.420020
1536.111450	77.340120	65.425025
1535.615195	79.541907	65.430030
1534.749746	68.971397	65.435034
1533.481774	73.052286	65.440039
1532.833123	76.555097	65.445044
1532.971408	75.699336	65.450049
1532.226851	83.841122	65.455054
1531.740851	77.528634	65.460058
1530.472442	75.073048	65.465063
1529.580438	77.733338	65.470068
1529.391915	77.279678	65.475073
1528.734714	82.127184	65.480078
1528.405730	75.690724	65.485082
1527.672541	81.540007	65.490087
1526.557726	84.757093	65.495092
1526.076572	82.897791	65.500097
1526.026221	78.852220	65.505102
1525.027910	79.086997	65.510106
1524.263048	75.980783	65.515111
1523.574784	82.686813	65.520116
1522.399832	72.132961	65.525121
1521.131927	79.652242	65.530126
1521.726246	73.971932	65.535130
1520.998222	73.510349	65.540135
1520.429803	77.502696	65.545140
1519.947916	77.001356	65.550145
1518.629293	82.820973	65.555150
1517.901236	78.004852	65.560154
1517.421346	67.741764	65.565159
1516.440043	80.805559	65.570164
1516.365422	66.184880	65.575169
1515.444562	80.927728	65.580174
1514.717396	71.912827	65.585178
1513.850540	78.102341	65.590183
1513.261220	78.600660	65.595188
1513.228524	63.400072	65.600193
1512.397162	73.267026	65.605198
1511.526799	76.628583	65.610202
1510.507595	75.805934	65.615207
1509.842689	77.628052	65.620212
1509.609802	65.492380	65.625217
1509.116856	72.217476	65.630222
1508.676424	66.919915	65.635226
1507.613701	81.277324	65.640231
1506.632459	80.456467	65.645236
1506.063845	73.584993	65.650241
1505.644451	77.472892	65.655246
1505.201055	72.398064	65.660250
1504.035326	72.460193	65.665255
1503.348856	71.352450	65.670260
1503.035429	75.496542	65.675265
1502.689217	74.213726	65.680270
1501.662232	75.180094	65.685274
1501.084756	76.106631	65.690279
1500.176473	78.569983	65.695284
1499.892016	77.655923	65.700289
1498.956340	76.607016	65.705294
1498.509782	75.055598	65.710298
1497.490674	78.478140	65.715303
1496.380414	80.439244	65.720308
1496.683005	72.780401	65.725313
1496.180636	76.632767	65.730318
1495.089886	73.598519	65.735322
1494.370023	70.500399	65.740327
1493.762144	79.729530	65.745332
1493.352857	70.869036	65.750337
1492.158628	77.803368	65.755342
1491.391896	70.003086	65.760346
1490.846707	74.128427	65.765351
1490.359831	78.242604	65.770356
1490.140559	73.983985	65.775361
1489.450427	78.331494	65.780366
1488.548511	71.426679	65.785370
1488.012970	75.876012	65.790375
1487.273304	66.331574	65.795380
1486.496764	58.937565	65.800385
1485.285872	71.683429	65.805390
1485.198368	72.445188	65.810394
1484.614234	70.999026	65.815399
1484.127618	74.280301	65.820404
1483.747556	72.069375	65.825409
1481.981840	73.829260	65.830414
1481.740044	74.662031	65.835418
1481.531266	66.834148	65.840423
1480.005258	71.293143	65.845428
1479.220282	64.644228	65.850433
1478.318020	69.816691	65.855438
1478.360487	71.961010	65.860442
1478.001183	75.797180	65.865447
1476.753020	76.375901	65.870452
1476.753299	68.641309	65.875457
1476.006055	73.765927	65.880462
1475.959011	64.479902	65.885466
1474.722415	66.409740	65.890471
1473.826784	73.176129	65.895476
1473.796649	70.481383	65.900481
1472.224751	76.332516	65.905486
1471.774861	74.305246	65.910490
1471.299751	73.136069	65.915495
1470.711864	73.658225	65.920500
1470.240665	65.698031	65.925505
1469.010747	76.574611	65.930510
1468.452427	77.235779	65.935514
1468.033331	74.542478	65.940519
1467.526199	75.544211	65.945524
1466.801711	69.666487	65.950529
1465.825695	78.121429	65.955534
1465.251604	61.643841	65.960538
1465.194693	61.981962	65.965543
1463.801803	67.800481	65.970548
1463.348471	60.019199	65.975553
1462.132780	68.605944	65.980558
1461.692877	63.436585	65.985562
1461.304973	63.144548	65.990567
1461.021543	76.965959	65.995572
1460.373555	64.850032	66.000577
1459.100198	75.067367	66.005582
1458.552568	69.469227	66.010586
1458.256614	74.697385	66.015591
1457.462134	71.427709	66.020596
1456.810563	64.789910	66.025601
1455.816940	70.743373	66.030606
1455.260354	60.956041	66.035610
1454.786971	69.043514	66.040615
1454.323461	68.450618	66.045620
1453.710747	61.858273	66.050625
1452.240561	74.184334	66.055630
1451.845330	65.384204	66.060634
1451.687601	64.386091	66.065639
1451.168899	70.290239	66.070644
1450.127404	67.868070	66.075649
1448.810828	69.302022	66.080654
1448.680088	64.275132	66.085658
1448.133262	71.755864	66.090663
1448.000267	60.213739	66.095668
1447.286418	56.620018	66.100673
1446.123010	71.857510	66.105678
1445.355842	64.232967	66.110682
1445.308312	68.080111	66.115687
1444.166976	78.029732	66.120692
1443.631338	71.154600	66.125697
1442.836734	74.364652	66.130702
1442.284043	63.923394	66.135706
1441.312759	67.252103	66.140711
1440.333598	71.825920	66.145716
1439.802186	62.692278	66.150721
1439.267281	76.826323	66.155726
1438.947109	63.721965	66.160730
1438.607633	66.737673	66.165735
1438.270864	68.346929	66.170740
1437.239715	62.218164	66.175745
1436.278182	64.246581	66.180750
1436.112600	68.324710	66.185754
1434.899436	64.231481	66.190759
1434.068768	63.300398	66.195764
1433.809308	63.858706	66.200769
1433.123533	79.065371	66.205774
1431.753520	70.680763	66.210778
1431.356606	74.348511	66.215783
1430.328720	71.575481	66.220788
1430.156287	69.389413	66.225793
1429.685099	71.861245	66.230798
1429.150766	68.219430	66.235802
1429.030266	66.462217	66.240807
1427.242059	74.575019	66.245812
1426.704636	66.892603	66.250817
1426.048986	76.288982	66.255822
1425.976251	67.441550	66.260826
1425.319805	72.039074	66.265831
1424.151456	70.372802	66.270836
1423.667830	65.645516	66.275841
1422.978708	67.624149	66.280846
1422.785150	62.617488	66.285850
1421.572604	60.380519	66.290855
1420.520197	72.026022	66.295860
1420.310541	63.543856	66.300865
1419.471994	64.291676	66.305870
1419.357706	66.341251	66.310874
1418.877972	68.835861	66.315879
1417.658612	76.069360	66.320884
1417.164173	64.946325	66.325889
1416.739325	68.613722	66.330894
1416.180625	60.863114	66.335898
1414.997754	65.300099	66.340903
1414.155675	70.946588	66.345908
1413.641633	66.225694	66.350913
1413.183965	73.824976	66.355918
1412.680830	68.702759	66.360922
1411.526144	76.223991	66.365927
1410.736939	65.652310	66.370932
1410.374489	63.433642	66.375937
1409.955045	71.005855	66.380942
1409.579269	71.177119	66.385946
1408.527049	72.774637	66.390951
1407.654936	70.674390	66.395956
1407.039588	58.866695	66.400961
1406.529883	70.075504	66.405966
1406.337884	62.405806	66.410970
1405.161431	67.045764	66.415975
1404.301499	69.959121	66.420980
1404.070845	65.743906	66.425985
1403.689601	71.866095	66.430990
1402.622757	69.071320	66.435994
1401.792193	69.838303	66.440999
1400.833985	66.972041	66.446004
1400.836592	63.436471	66.451009
1400.447710	66.119599	66.456014
1399.426543	67.337610	66.461018
1398.650556	78.901069	66.466023
1397.681887	62.494198	66.471028
1397.569993	62.798313	66.476033
1396.105480	70.182324	66.481038
1395.444057	70.136839	66.486042
1394.742521	71.686568	66.491047
1394.493083	68.692275	66.496052
1394.344531	65.456513	66.501057
1393.545574	70.297503	66.506062
1392.916333	63.520507	66.511066
1392.060113	63.710462	66.516071
1391.446451	71.424073	66.521076
1390.955902	62.340286	66.526081
1390.189667	75.760013	66.531086
1389.210221	71.460612	66.536090
1388.565054	66.365870	66.541095
1388.094505	72.847540	66.546100
1387.783362	63.575550	66.551105
1386.438103	70.917836	66.556110
1385.844509	61.822479	66.561114
1385.268849	69.888383	66.566119
1384.628962	72.907361	66.571124
1384.420523	55.585669	66.576129
1383.387881	79.007375	66.581134
1382.109323	63.331681	66.586138
1381.907719	64.170996	66.591143
1381.139306	66.127287	66.596148
1381.099275	63.800144	66.601153
1380.426380	71.170621	66.606158
1379.700161	67.337854	66.611162
1378.967323	66.313853	66.616167
1377.840650	70.890824	66.621172
1377.959460	67.507460	66.626177
1376.249596	74.577440	66.631182
1375.849612	66.329953	66.636186
1375.444248	62.865798	66.641191
1374.535708	67.049789	66.646196
1374.536653	63.920274	66.651201
1373.950198	66.301319	66.656206
1372.991206	61.560681	66.661210
1371.913665	61.310916	66.666215
1371.343959	66.848419	66.671220
1370.981128	61.916526	66.676225
1370.187525	58.951046	66.681230
1369.671952	67.309808	66.686234
1368.888978	69.503056	66.691239
1368.151834	69.268835	66.696244
1367.771343	66.540125	66.701249
1366.816497	72.916811	66.706254
1365.805432	70.239596	66.711258
1365.248632	60.640206	66.716263
1364.733750	66.911974	66.721268
1364.777829	65.835900	66.726273
1363.560242	68.019076	66.731278
1362.647145	57.861761	66.736282
1362.260482	59.738890	66.741287
1361.503133	69.963428	66.746292
1361.269740	62.822639	66.751297
1360.406012	62.516145	66.756302
1359.870143	64.564862	66.761306
1358.880849	66.143328	66.766311
1358.360464	63.420409	66.771316
1357.815647	57.307097	66.776321
1356.525601	65.303455	66.781326
1356.239793	65.543004	66.786330
1356.071955	70.009132	66.791335
1355.203145	64.973205	66.796340
1354.210234	68.377073	66.801345
1353.426141	74.484938	66.806350
1352.670204	64.466106	66.811354
1352.006281	56.522745	66.816359
1351.809491	63.968818	66.821364
1351.555985	67.165987	66.826369
1350.680238	64.885987	66.831374
1349.318843	60.600274	66.836378
1348.971733	61.703697	66.841383
1348.507198	59.214760	66.846388
1348.282949	55.656451	66.851393
1347.026639	61.823832	66.856398
1346.032565	52.006424	66.861402
1345.728513	56.834535	66.866407
1345.025795	57.294654	66.871412
1344.601265	58.724342	66.876417
1344.037551	68.090770	66.881422
1342.987067	63.799991	66.886426
1342.213015	63.339603	66.891431
1341.780093	63.332375	66.896436
1341.554264	67.747249	66.901441
1340.663625	67.909948	66.906446
1340.368982	69.428318	66.911450
1339.369398	57.404588	66.916455
1338.572110	71.557093	66.921460
1337.840390	65.024218	66.926465
1336.844850	60.450496	66.931470
1336.564014	67.848592	66.936474
1336.064824	64.275377	66.941479
1335.160678	72.959989	66.946484
1334.383232	66.194954	66.951489
1333.471615	57.344701	66.956494
1333.046839	62.314262	66.961498
1333.152571	64.702339	66.966503
1331.761940	68.259159	66.971508
1331.216199	58.158172	66.976513
1330.288594	60.607093	66.981518
1329.638111	58.082099	66.986522
1329.212919	59.902671	66.991527
1328.653709	70.161577	66.996532
1327.708841	56.927752	67.001537
1326.797148	72.289127	67.006542
1326.784235	66.878541	67.011546
1326.161833	63.582197	67.016551
1325.573091	63.510464	67.021556
1324.681217	60.295381	67.026561
1323.715341	65.670979	67.031566
1323.161397	66.368122	67.036570
1322.653449	66.922002	67.041575
1322.648353	67.962141	67.046580
1321.889945	70.152375	67.051585
1320.828642	65.423342	67.056590
1320.119516	64.804613	67.061594
1319.090872	63.616533	67.066599
1318.073182	64.538320	67.071604
1317.885694	64.156331	67.076609
1317.158547	66.977498	67.081614
1317.092031	68.836930	67.086618
1316.429556	64.201064	67.091623
1315.302866	72.179730	67.096628
1314.327063	65.642463	67.101633
1313.832841	64.841295	67.106638
1313.327913	69.531305	67.111642
1313.169703	68.828530	67.116647
1312.175858	73.750257	67.121652
1311.455781	64.058045	67.126657
1310.854986	68.766440	67.131662
1310.340901	65.621679	67.136666
1309.150068	68.096325	67.141671
1308.235730	66.142661	67.146676
1307.926796	58.734957	67.151681
1307.408656	65.417001	67.156686
1307.050220	65.244663	67.161690
1306.357073	56.289522	67.166695
1304.870225	65.194669	67.171700
1304.737831	69.518156	67.176705
1304.217384	67.889808	67.181710
1303.914114	72.180972	67.186714
1302.923543	61.528143	67.191719
1301.555163	73.388793	67.196724
1301.380280	65.429611	67.201729
1300.695352	70.253852	67.206734
1300.214875	62.437772	67.211738
1300.203745	66.953647	67.216743
1298.978284	70.081561	67.221748
1298.129064	60.018323	67.226753
1297.132543	66.032299	67.231758
1296.997026	62.651030	67.236762
1296.674239	58.009515	67.241767
1295.775549	68.584287	67.246772
1295.046712	63.187717	67.251777
1294.052082	70.173956	67.256782
1293.532637	63.281083	67.261786
1292.483640	68.513029	67.266791
1291.491915	62.648331	67.271796
1291.764845	62.740522	67.276801
1290.842653	64.590526	67.281806
1290.523617	59.687855	67.286810
1290.287549	59.219846	67.291815
1288.802857	69.935990	67.296820
1288.041142	68.717613	67.301825
1287.647651	73.615906	67.306830
1287.496275	69.771979	67.311834
1286.748219	77.955030	67.316839
1285.470849	75.649460	67.321844
1284.952416	70.548038	67.326849
1284.191724	70.849941	67.331854
1283.563334	65.633141	67.336858
1282.767848	68.929411	67.341863
1281.553068	72.566266	67.346868
1281.636604	65.018745	67.351873
1280.681071	66.217253	67.356878
1280.420192	63.773982	67.361882
1280.188392	62.386339	67.366887
1279.316291	69.417521	67.371892
1278.488604	61.918637	67.376897
1277.695699	66.922804	67.381902
1277.092241	64.197144	67.386906
1276.914047	68.733331	67.391911
1275.512235	73.381896	67.396916
1274.895664	62.080470	67.401921
1274.043381	70.381620	67.406926
1274.180404	68.158373	67.411930
1273.734548	69.560534	67.416935
1272.374876	77.268452	67.421940
1271.945651	68.238920	67.426945
1271.126112	76.959184	67.431950
1270.575437	66.184476	67.436954
1269.461787	73.383323	67.441959
1268.499448	70.653580	67.446964
1268.477879	69.915572	67.451969
1267.641389	77.199991	67.456974
1267.305681	72.533451	67.461978
1267.399274	70.165673	67.466983
1265.855065	65.070138	67.471988
1265.642378	68.305318	67.476993
1264.871455	66.927083	67.481998
1263.682337	67.575480	67.487002
1262.645016	64.952124	67.492007
1262.320161	72.792341	67.497012
1262.134644	72.373702	67.502017
1261.437994	70.519747	67.507022
1260.091321	67.421220	67.512026
1259.625782	70.910863	67.517031
1259.171962	76.629052	67.522036
1258.707993	67.057208	67.527041
1258.288609	74.885978	67.532046
1257.495814	66.930750	67.537050
1256.511047	77.913801	67.542055
1255.708694	78.040086	67.547060
1255.498486	63.038478	67.552065
1254.662274	70.415212	67.557070
1253.603699	66.480691	67.562074
1252.838626	74.787045	67.567079
1252.312128	75.332266	67.572084
1252.146313	61.712073	67.577089
1251.681665	65.858768	67.582094
1250.799504	62.852027	67.587098
1249.806725	62.114510	67.592103
1249.018121	70.448179	67.597108
1249.191405	67.395342	67.602113
1248.337260	72.024754	67.607118
1247.496955	65.569302	67.612122
1246.900219	66.601394	67.617127
1245.829175	63.904477	67.622132
1245.587100	56.031412	67.627137
1244.648800	68.688394	67.632142
1243.914064	63.023647	67.637146
1242.918071	64.893398	67.642151
1242.242023	80.890196	67.647156
1242.246831	64.043575	67.652161
1241.951461	66.399664	67.657166
1241.125156	75.292395	67.662170
1240.302726	64.244104	67.667175
1239.613319	71.301247	67.672180
1238.569319	66.405465	67.677185
1237.459543	66.617542	67.682190
1237.279530	60.136677	67.687194
1236.689024	68.535899	67.692199
1236.202840	71.539233	67.697204
1235.910224	67.802776	67.702209
1234.625339	75.769857	67.707214
1233.999957	74.684062	67.712218
1233.627920	70.235315	67.717223
1233.153092	69.715427	67.722228
1232.482987	57.769133	67.727233
1231.347378	66.594820	67.732238
1230.594692	68.550807	67.737242
1230.280092	63.761851	67.742247
1229.619811	66.604737	67.747252
1228.802307	63.898758	67.752257
1227.840641	61.402583	67.757262
1227.242100	63.795183	67.762266
1226.855084	56.701635	67.767271
1226.424080	70.532494	67.772276
1226.108919	65.414439	67.777281
1224.821442	66.970562	67.782286
1224.376831	71.103172	67.787290
1223.959059	64.612884	67.792295
1222.719987	73.733381	67.797300
1221.685995	63.538778	67.802305
1220.814867	67.703754	67.807310
1220.674474	67.987094	67.812314
1220.392027	66.298272	67.817319
1220.090504	77.385391	67.822324
1219.439456	65.226632	67.827329
1218.019652	69.297265	67.832334
1217.148704	66.280716	67.837338
1217.137643	72.330450	67.842343
1216.369019	79.111043	67.847348
1215.980958	73.272871	67.852353
1214.573035	82.204399	67.857358
1213.856282	75.280582	67.862362
1213.808440	80.089702	67.867367
1213.521541	76.051096	67.872372
1212.835707	69.783141	67.877377
1211.801951	69.555913	67.882382
1211.135481	66.172794	67.887386
1210.957074	70.561786	67.892391
1209.185169	72.192958	67.897396
1208.252405	62.670995	67.902401
1207.689782	71.942509	67.907406
1207.559487	73.310778	67.912410
1207.186865	73.944522	67.917415
1206.809882	79.170766	67.922420
1206.355628	65.484309	67.927425
1205.324882	72.365038	67.932430
1204.309961	68.218197	67.937434
1203.749559	69.989300	67.942439
1202.451698	72.802014	67.947444
1202.179874	68.769515	67.952449
1201.874714	74.363573	67.957454
1201.440645	76.075155	67.962458
1200.947903	73.514883	67.967463
1199.541860	73.967156	67.972468
1198.496301	70.289355	67.977473
1197.982398	75.130507	67.982478
1197.511536	66.526125	67.987482
1197.537868	59.179056	67.992487
1197.074443	74.663808	67.997492
1196.168590	71.833230	68.002497
1195.106222	80.591919	68.007502
1194.464194	68.367280	68.012506
1194.437547	66.024826	68.017511
1193.074029	65.858797	68.022516
1192.568677	68.490828	68.027521
1191.833280	68.661710	68.032526
1191.321078	66.559881	68.037530
1190.579239	69.325161	68.042535
1189.562589	70.180087	68.047540
1188.971992	68.506924	68.052545
1188.718253	65.886788	68.057550
1188.330756	68.436275	68.062554
1187.653130	60.880933	68.067559
1186.230999	75.222920	68.072564
1185.944012	70.254379	68.077569
1185.058334	78.221011	68.082574
1184.540319	70.966742	68.087578
1184.230717	72.049544	68.092583
1183.137834	72.766346	68.097588
1182.582131	77.837278	68.102593
1181.913821	88.530513	68.107598
1181.645622	66.554705	68.112602
1180.379077	61.985582	68.117607
1179.536108	72.359385	68.122612
1179.191960	67.910608	68.127617
1178.371218	67.995846	68.132622
1178.135570	60.520746	68.137626
1177.900731	66.776939	68.142631
1176.762791	69.629380	68.147636
1176.164146	64.372772	68.152641
1175.341086	73.391655	68.157646
1174.782881	74.470051	68.162650
1173.961634	72.326405	68.167655
1172.810139	74.068854	68.172660
1172.726850	67.983518	68.177665
1171.721928	78.307295	68.182670
1171.303415	74.655948	68.187674
1171.110893	67.195172	68.192679
1170.072908	74.621856	68.197684
1169.113029	64.971921	68.202689
1168.465779	73.659139	68.207694
1168.220912	65.902999	68.212698
1167.898503	64.947699	68.217703
1167.059124	74.040821	68.222708
1166.069741	60.020891	68.227713
1165.642467	68.091787	68.232718
1164.728167	52.984587	68.237722
1164.167777	58.631024	68.242727
1163.083910	72.876412	68.247732
1162.599511	64.968268	68.252737
1162.156100	79.483327	68.257742
1161.941435	69.432257	68.262746
1160.877868	53.624730	68.267751
1160.178087	59.399634	68.272756
1159.625854	63.430283	68.277761
1159.178024	62.765260	68.282766
1157.838511	59.357265	68.287770
1157.157496	68.356563	68.292775
1156.711422	73.545296	68.297780
1156.252152	63.299676	68.302785
1155.870192	72.678013	68.307790
1155.164977	67.591227	68.312794
1154.356739	66.589644	68.317799
1153.722300	73.880132	68.322804
1153.262154	61.185442	68.327809
1152.219341	71.769113	68.332814
1151.514030	71.260672	68.337818
1150.847144	66.385208	68.342823
1150.546865	66.931177	68.347828
1150.029264	61.095069	68.352833
1148.665320	74.693712	68.357838
1148.167987	67.257104	68.362842
1147.897649	63.152123	68.367847
1146.582706	69.273927	68.372852
1146.032357	65.515297	68.377857
1144.658888	69.086986	68.382862
1144.673002	67.264502	68.387866
1144.056163	70.389681	68.392871
1143.461472	69.582841	68.397876
1143.217504	58.784466	68.402881
1142.353374	66.254405	68.407886
1142.345199	70.193085	68.412890
1141.331595	54.871196	68.417895
1140.305067	62.445909	68.422900
1140.011787	58.176315	68.427905
1138.644826	68.682072	68.432910
1138.133406	64.938093	68.437914
1137.549438	60.407233	68.442919
1137.029111	70.365023	68.447924
1136.860724	66.130486	68.452929
1135.753348	63.767039	68.457934
1135.249523	66.180533	68.462938
1134.661647	62.506485	68.467943
1134.319000	70.542761	68.472948
1132.835673	62.530152	68.477953
1132.388718	81.594935	68.482958
1131.571792	66.183707	68.487962
1131.262519	67.589333	68.492967
1130.413884	71.819150	68.497972
1129.634489	73.225146	68.502977
1128.863282	72.588261	68.507982
1128.183164	79.182793	68.512986
1127.711923	66.069236	68.517991
1127.582143	72.425462	68.522996
1126.714107	70.369964	68.528001
1125.856614	77.897191	68.533006
1125.401134	65.172891	68.538010
1124.888766	70.456655	68.543015
1123.939234	71.890599	68.548020
1123.129344	64.534750	68.553025
1122.087586	71.765121	68.558030
1121.827519	73.958468	68.563034
1121.393034	66.232038	68.568039
1120.520208	73.776889	68.573044
1119.696047	67.071609	68.578049
1118.828141	72.331782	68.583054
1118.289045	65.875704	68.588058
1118.231990	65.697958	68.593063
1117.426245	72.815684	68.598068
1116.461742	69.669130	68.603073
1115.604669	75.785960	68.608078
1115.081205	58.795755	68.613082
1114.792346	67.354503	68.618087
1113.979987	74.601646	68.623092
1113.059717	73.371371	68.628097
1112.167782	68.947717	68.633102
1111.663460	68.625119	68.638106
1111.583180	69.388803	68.643111
1111.393514	78.854210	68.648116
1110.316757	78.167020	68.653121
1109.329239	77.511522	68.658126
1108.899778	79.504544	68.663130
1107.396837	69.410007	68.668135
1106.613724	71.763964	68.673140
1106.598960	67.756929	68.678145
1105.679651	80.195948	68.683150
1105.279534	73.001239	68.688154
1105.194140	72.329816	68.693159
1104.418179	73.492476	68.698164
1103.553078	72.798650	68.703169
1102.786079	71.917903	68.708174
1102.239485	70.407735	68.713178
1101.557446	74.260495	68.718183
1100.248398	77.601308	68.723188
1099.726895	61.093509	68.728193
1099.524824	69.063872	68.733198
1098.914467	68.361162	68.738202
1098.729211	66.489927	68.743207
1097.206997	72.389088	68.748212
1096.824841	66.656103	68.753217
1096.070678	71.834437	68.758222
1095.711497	70.942673	68.763226
1094.550337	71.036086	68.768231
1093.297201	73.344613	68.773236
1093.236210	62.662932	68.778241
1092.616358	75.412627	68.783246
1092.022762	73.242251	68.788250
1091.764827	70.981244	68.793255
1090.957378	77.311411	68.798260
1090.376057	69.001080	68.803265
1089.221677	67.858263	68.808270
1089.076719	73.199506	68.813274
1088.280374	69.169206	68.818279
1087.338515	77.357429	68.823284
1086.783231	70.912415	68.828289
1086.238293	75.145497	68.833294
1085.774083	79.347388	68.838298
1085.260602	70.532833	68.843303
1083.941670	71.218105	68.848308
1083.591772	69.392825	68.853313
1083.034823	71.773581	68.858318
1082.279698	80.390466	68.863322
1081.073651	66.030706	68.868327
1080.567036	68.871372	68.873332
1080.431793	68.809246	68.878337
1079.536841	70.409896	68.883342
1079.463406	77.301972	68.888346
1078.473235	76.770876	68.893351
1077.257682	76.893737	68.898356
1076.622851	64.395150	68.903361
1076.089465	73.209708	68.908366
1075.661935	61.920565	68.913370
1075.373481	68.307510	68.918375
1073.966562	72.124537	68.923380
1073.717479	69.785835	68.928385
1072.992967	66.401232	68.933390
1072.392169	75.483901	68.938394
1071.882674	68.866453	68.943399
1070.590336	72.472423	68.948404
1070.432309	65.527175	68.953409
1069.677685	72.092231	68.958414
1069.542701	70.562503	68.963418
1068.299235	76.125402	68.968423
1067.248894	75.001089	68.973428
1066.980026	70.465226	68.978433
1066.538806	70.524571	68.983438
1065.867362	70.573604	68.988442
1065.340305	71.014735	68.993447
1064.542275	70.543103	68.998452
1064.195300	66.277973	69.003457
1063.115503	67.318596	69.008462
1062.321462	63.598551	69.013466
1061.797942	76.742651	69.018471
1061.078023	75.456369	69.023476
1060.369798	74.623193	69.028481
1058.724094	79.302521	69.033486
1058.763704	78.642061	69.038490
1058.121295	77.524471	69.043495
1057.290627	76.841335	69.048500
1057.539149	71.770055	69.053505
1056.526422	73.933613	69.058510
1056.431116	70.590865	69.063514
1055.595641	68.702297	69.068519
1054.509479	75.718451	69.073524
1054.104024	65.343642	69.078529
1052.975940	72.243032	69.083534
1051.900061	71.517813	69.088538
1051.272069	66.882011	69.093543
1050.601597	73.841981	69.098548
1050.462879	69.531716	69.103553
1050.084438	75.077931	69.108558
1050.105822	81.606815	69.113562
1048.827327	78.735084	69.118567
1048.458123	76.696017	69.123572
1047.779753	77.309895	69.128577
1046.528727	81.221414	69.133582
1045.432330	72.609312	69.138586
1045.244393	78.388552	69.143591
1044.492360	77.238422	69.148596
1044.003108	68.911545	69.153601
1042.818770	75.784258	69.158606
1041.895648	76.200455	69.163610
1041.811535	71.257581	69.168615
1041.645369	74.870042	69.173620
1040.599876	71.468571	69.178625
1040.153251	75.103796	69.183630
1039.379020	71.246552	69.188634
1038.744842	79.674578	69.193639
1037.579231	80.984496	69.198644
1037.573642	76.417760	69.203649
1036.588492	74.064192	69.208654
1035.534140	76.074627	69.213658
1035.312817	74.894405	69.218663
1034.522588	71.502904	69.223668
1034.227958	72.482891	69.228673
1033.844010	74.863630	69.233678
1032.725554	74.778832	69.238682
1032.194640	74.563422	69.243687
1031.542649	73.969293	69.248692
1031.071080	66.090948	69.253697
1029.750971	72.864155	69.258702
1028.985874	68.003557	69.263706
1029.024337	65.728113	69.268711
1028.145859	74.372042	69.273716
1027.468453	70.901226	69.278721
1026.520246	71.583419	69.283726
1026.091577	67.558850	69.288730
1025.615057	69.821632	69.293735
1024.662138	72.582818	69.298740
1024.089847	73.995992	69.303745
1022.730024	73.676622	69.308750
1022.405042	76.005819	69.313754
1022.243880	68.559426	69.318759
1021.473761	76.713114	69.323764
1021.594991	74.088775	69.328769
1020.411190	78.920319	69.333774
1019.814499	79.424692	69.338778
1018.724133	74.405859	69.343783
1017.458651	72.894868	69.348788
1017.122948	65.827691	69.353793
1016.109444	75.069453	69.358798
1015.718465	74.306686	69.363802
1015.689219	66.881912	69.368807
1015.114168	70.586102	69.373812
1014.689480	62.987877	69.378817
1014.049778	61.912460	69.383822
1013.038124	72.927760	69.388826
1012.349283	66.693914	69.393831
1011.578228	76.692669	69.398836
1011.009789	75.552550	69.403841
1009.949895	79.661466	69.408846
1009.436610	75.148913	69.413850
1009.047325	74.702025	69.418855
1008.244628	70.521652	69.423860
1007.303951	68.083112	69.428865
1006.591699	73.067577	69.433870
1006.173941	69.659663	69.438874
1006.106063	66.200911	69.443879
1005.479386	78.501010	69.448884
1004.508658	66.723482	69.453889
1003.422445	73.676892	69.458894
1003.235585	70.075892	69.463898
1002.734428	61.835535	69.468903
1001.064572	65.926148	69.473908
1000.356546	67.806230	69.478913
999.837826	73.059511	69.483918
999.914004	63.567711	69.488922
999.764469	66.645638	69.493927
998.243952	71.876672	69.498932
997.517166	68.533522	69.503937
996.610253	80.057839	69.508942
995.884800	75.106383	69.513946
995.679718	69.245987	69.518951
995.218248	70.250995	69.523956
994.761784	63.028854	69.528961
993.460064	72.341683	69.533966
993.349215	73.593341	69.538970
992.761638	72.221646	69.543975
991.590759	75.479219	69.548980
990.745359	63.272099	69.553985
990.039110	73.394748	69.558990
989.811413	71.688279	69.563994
989.442137	67.930240	69.568999
988.882102	70.754010	69.574004
988.085549	66.865470	69.579009
987.074225	72.686640	69.584014
986.609127	63.597784	69.589018
985.657654	73.136803	69.594023
984.971348	71.434666	69.599028
984.061294	65.104111	69.604033
983.620320	69.567670	69.609038
983.461095	67.778426	69.614042
983.051890	63.491991	69.619047
981.656414	76.870279	69.624052
980.867234	68.542676	69.629057
980.641441	73.391337	69.634062
979.948858	74.786434	69.639066
979.348522	74.693045	69.644071
977.904329	77.932694	69.649076
977.806039	73.698401	69.654081
977.194782	81.063479	69.659086
976.987023	82.593827	69.664090
976.165017	73.541223	69.669095
974.723791	75.785678	69.674100
974.556499	74.312405	69.679105
973.844235	71.899093	69.684110
973.492312	70.002726	69.689114
972.335881	70.323109	69.694119
971.261281	67.863698	69.699124
970.875269	72.448102	69.704129
970.724549	74.538258	69.709134
970.124356	73.550812	69.714138
969.605965	71.833340	69.719143
968.697691	74.277826	69.724148
968.280332	70.235933	69.729153
967.525908	71.264273	69.734158
966.521917	69.532076	69.739162
965.678054	69.268431	69.744167
964.616707	69.096504	69.749172
964.986433	67.617706	69.754177
963.941154	76.524670	69.759182
963.920053	73.884840	69.764186
962.674570	71.845860	69.769191
961.668327	76.708187	69.774196
961.239144	71.119056	69.779201
960.903139	76.870364	69.784206
960.414639	67.267256	69.789210
959.491987	69.502242	69.794215
958.460303	72.272191	69.799220
958.046710	67.312728	69.804225
957.613199	74.013054	69.809230
956.873718	73.001309	69.814234
955.829565	76.970965	69.819239
954.914853	77.840452	69.824244
954.309451	69.767156	69.829249
954.250720	73.737381	69.834254
953.723426	70.118507	69.839258
953.088755	68.310827	69.844263
951.947269	75.656191	69.849268
951.540421	71.047265	69.854273
950.899308	66.774105	69.859278
950.069878	66.573909	69.864282
949.228674	72.141750	69.869287
948.230550	74.879507	69.874292
948.030750	66.575311	69.879297
947.635712	70.175259	69.884302
947.340876	74.538797	69.889306
946.189244	69.854541	69.894311
944.752075	73.884007	69.899316
944.495313	67.669329	69.904321
944.322354	72.006467	69.909326
943.768087	74.032715	69.914330
943.493704	64.084668	69.919335
942.249132	58.786367	69.924340
941.821481	63.268169	69.929345
941.212889	65.651466	69.934350
939.755389	67.855692	69.939354
939.072240	71.942330	69.944359
938.305912	69.453420	69.949364
938.197500	66.016218	69.954369
937.658265	74.442590	69.959374
937.328827	69.824751	69.964378
936.888635	62.487734	69.969383
935.956623	77.556562	69.974388
935.002424	64.014213	69.979393
933.875101	73.179559	69.984398
932.817184	80.815732	69.989402
932.463777	63.496466	69.994407
931.963599	75.811606	69.999412
931.906926	67.254753	70.004417
931.287278	68.888009	70.009422
931.046654	69.249704	70.014426
930.203399	64.210682	70.019431
929.481068	76.351512	70.024436
928.762733	75.438381	70.029441
927.520997	69.299243	70.034446
926.710690	75.070207	70.039450
926.283315	72.987828	70.044455
925.595893	79.681515	70.049460
925.210694	78.270431	70.054465
924.462972	74.649841	70.059470
923.638991	78.212339	70.064474
923.330755	63.972814	70.069479
922.074096	72.692573	70.074484
921.420069	74.378296	70.079489
920.640871	82.003444	70.084494
919.973892	74.579746	70.089498
919.699112	68.267898	70.094503
919.450619	76.468432	70.099508
918.892176	75.518840	70.104513
918.059911	74.846660	70.109518
916.955583	68.895560	70.114522
916.585107	72.254079	70.119527
915.742676	78.789191	70.124532
914.563555	71.301638	70.129537
913.768332	71.371891	70.134542
913.587075	67.716653	70.139546
913.130754	63.653812	70.144551
912.827937	77.779265	70.149556
912.632121	64.384522	70.154561
911.396987	76.508974	70.159566
910.455765	72.885214	70.164570
910.065068	60.693791	70.169575
908.923222	72.055065	70.174580
908.260747	64.957822	70.179585
907.593569	72.236956	70.184590
907.184600	66.486487	70.189594
906.581497	67.008943	70.194599
906.102482	76.105888	70.199604
905.698041	65.432923	70.204609
904.543934	75.288484	70.209614
903.527207	72.617477	70.214618
903.354458	58.904201	70.219623
902.245880	75.789359	70.224628
901.771873	62.100837	70.229633
901.018596	69.299589	70.234638
900.313753	67.113955	70.239642
900.442896	63.285562	70.244647
899.477080	73.347282	70.249652
898.561991	64.676548	70.254657
897.661316	67.741816	70.259662
897.075289	78.019924	70.264666
896.940724	68.846841	70.269671
896.473240	75.160245	70.274676
895.396817	66.009933	70.279681
894.784706	68.086353	70.284686
894.121570	73.098335	70.289690
892.868457	65.726485	70.294695
892.075540	69.772719	70.299700
891.555400	56.718125	70.304705
891.283058	72.617337	70.309710
890.589775	76.318105	70.314714
890.640679	72.456139	70.319719
889.603093	78.407342	70.324724
888.890658	62.436752	70.329729
887.799674	77.590438	70.334734
887.466206	74.953586	70.339738
886.907973	61.038322	70.344743
885.838794	68.285655	70.349748
885.386230	66.686783	70.354753
884.386528	71.868114	70.359758
884.080066	74.766484	70.364762
883.704719	65.001520	70.369767
882.997797	75.406511	70.374772
882.131280	69.172335	70.379777
881.703183	66.495248	70.384782
880.862328	74.188980	70.389786
879.681507	61.174126	70.394791
878.764038	78.962429	70.399796
878.934288	69.732404	70.404801
878.171117	71.541425	70.409806
877.857864	76.131922	70.414810
877.326531	67.303101	70.419815
876.024335	72.259943	70.424820
875.631820	70.424219	70.429825
874.759890	72.284630	70.434830
874.290532	75.408652	70.439834
873.138978	73.329532	70.444839
872.473364	82.779740	70.449844
871.988505	76.962931	70.454849
871.693699	72.693623	70.459854
871.193578	72.216786	70.464858
870.494460	65.157405	70.469863
869.309196	71.856233	70.474868
868.880669	81.546476	70.479873
868.568399	72.519089	70.484878
867.340074	74.621719	70.489882
866.554752	69.100706	70.494887
865.892376	73.280894	70.499892
865.600891	70.514097	70.504897
865.351825	74.866244	70.509902
864.569905	71.850703	70.514906
863.559569	69.337288	70.519911
862.846976	74.287879	70.524916
862.569064	67.463444	70.529921
862.108003	74.722672	70.534926
860.925978	72.332211	70.539930
860.165399	72.904934	70.544935
859.196009	71.405243	70.549940
859.326037	70.940864	70.554945
858.340627	73.841845	70.559950
857.156284	81.599546	70.564954
856.664826	75.141273	70.569959
856.195258	80.182471	70.574964
855.740342	72.765094	70.579969
855.247731	74.417257	70.584974
854.353210	74.843194	70.589978
853.719197	67.904499	70.594983
853.100975	81.547554	70.599988
853.117938	71.312391	70.604993
851.543052	73.640164	70.609998
850.398918	72.530781	70.615002
849.953598	71.197104	70.620007
849.369437	74.455654	70.625012
849.085702	70.287868	70.630017
848.888449	77.450205	70.635022
847.797523	77.590064	70.640026
847.165149	73.112538	70.645031
846.725048	74.829125	70.650036
845.978684	66.590139	70.655041
845.260714	69.331636	70.660046
843.877066	67.525950	70.665050
843.540227	66.418812	70.670055
842.824727	70.342455	70.675060
842.770810	67.956527	70.680065
842.136133	70.375485	70.685070
840.851870	71.964702	70.690074
840.502871	68.771204	70.695079
839.600363	78.915242	70.700084
839.500894	71.193841	70.705089
838.815035	73.604988	70.710094
837.407561	75.384644	70.715098
837.007553	67.970894	70.720103
836.161525	73.438133	70.725108
836.048636	73.902683	70.730113
835.503295	77.153401	70.735118
834.693279	77.717228	70.740122
834.046381	77.453026	70.745127
833.241230	79.667908	70.750132
832.813565	64.282077	70.755137
831.702853	65.823018	70.760142
830.747500	71.049259	70.765146
830.324756	67.610249	70.770151
829.711091	71.250413	70.775156
829.618077	68.564093	70.780161
829.245032	72.948132	70.785166
828.262483	76.431230	70.790170
827.671865	66.888665	70.795175
826.193894	71.251579	70.800180
825.556441	60.664728	70.805185
825.057279	74.057262	70.810190
824.123697	71.456503	70.815194
823.968895	64.468100	70.820199
823.395109	74.341499	70.825204
822.849216	71.004105	70.830209
822.313560	73.802399	70.835214
821.072187	67.831778	70.840218
820.992993	71.005809	70.845223
820.289569	76.079959	70.850228
819.691307	70.434157	70.855233
818.605241	67.021536	70.860238
817.593935	77.634581	70.865242
817.642909	66.931334	70.870247
817.048712	64.794653	70.875252
815.752422	68.708446	70.880257
815.483389	72.599431	70.885262
814.844039	75.728498	70.890266
814.573809	72.022193	70.895271
813.236038	83.375600	70.900276
812.099949	77.607590	70.905281
811.862826	73.228939	70.910286
811.251296	64.718592	70.915290
811.257133	60.395033	70.920295
810.367314	72.778092	70.925300
809.380700	64.956828	70.930305
808.561127	67.950588	70.935310
808.227241	69.147299	70.940314
807.691771	61.754392	70.945319
806.081959	72.467979	70.950324
805.820118	61.623382	70.955329
805.265041	74.534468	70.960334
804.838710	68.414769	70.965338
804.557295	78.702277	70.970343
803.608860	71.655220	70.975348
803.006003	65.654571	70.980353
802.031396	69.230649	70.985358
801.495443	65.815377	70.990362
801.386236	66.526389	70.995367
800.044039	76.125644	71.000372
799.422998	66.318311	71.005377
798.851368	65.802813	71.010382
798.330854	65.881290	71.015386
797.928920	73.185256	71.020391
796.280750	73.846476	71.025396
795.830491	65.236274	71.030401
795.350397	69.652860	71.035406
794.997623	72.635739	71.040410
794.829530	58.308692	71.045415
793.315615	70.399201	71.050420
792.974690	72.008018	71.055425
792.257764	71.719503	71.060430
791.697067	70.040089	71.065434
791.560354	65.695161	71.070439
790.114128	69.955546	71.075444
789.144539	68.769309	71.080449
788.831873	67.635930	71.085454
788.394027	75.805345	71.090458
788.261334	58.696593	71.095463
786.651951	75.057310	71.100468
786.074032	66.676202	71.105473
785.658996	79.311474	71.110478
785.036802	77.924816	71.115482
784.521237	73.863454	71.120487
783.033667	79.312311	71.125492
782.673367	64.774250	71.130497
782.279175	78.902318	71.135502
781.635130	82.002984	71.140506
781.296042	68.149672	71.145511
780.160436	72.980504	71.150516
779.718666	67.257776	71.155521
779.223824	70.675495	71.160526
778.332293	67.872158	71.165530
778.250168	65.137795	71.170535
777.376092	71.209811	71.175540
777.185698	64.797480	71.180545
776.028474	67.590544	71.185550
774.592996	80.934271	71.190554
774.070145	71.870344	71.195559
773.158391	77.946450	71.200564
772.980665	71.814168	71.205569
772.559084	67.303313	71.210574
772.228842	77.720359	71.215578
771.244005	69.701047	71.220583
770.121387	73.450898	71.225588
770.022821	66.674697	71.230593
769.857070	83.588618	71.235598
768.441170	82.546727	71.240602
767.702786	70.114902	71.245607
767.446035	78.753797	71.250612
766.598702	68.597228	71.255617
765.704669	73.540226	71.260622
764.844267	68.236560	71.265626
764.783789	75.184815	71.270631
763.734448	78.650551	71.275636
763.219872	69.565475	71.280641
762.483810	71.505255	71.285646
761.431022	75.468924	71.290650
761.058552	72.037493	71.295655
759.853493	66.871418	71.300660
759.647262	67.269858	71.305665
759.159345	65.105901	71.310670
759.065001	80.014271	71.315674
758.556159	75.371924	71.320679
757.132854	75.390328	71.325684
757.074526	81.094861	71.330689
756.295541	70.572131	71.335694
755.291935	67.958120	71.340698
754.924656	61.668062	71.345703
753.868790	67.386768	71.350708
753.310938	62.946626	71.355713
752.225794	61.001812	71.360718
751.566133	65.888083	71.365722
751.340911	62.581424	71.370727
750.829250	74.147774	71.375732
750.296837	63.752540	71.380737
749.238591	63.467240	71.385742
747.947718	57.261586	71.390746
747.855458	58.324151	71.395751
747.278221	63.658514	71.400756
746.907029	65.011215	71.405761
746.543740	72.488157	71.410766
745.293176	69.661861	71.415770
744.510881	63.829323	71.420775
743.826010	69.958137	71.425780
743.337769	63.123174	71.430785
742.969710	72.770684	71.435790
741.631118	71.698981	71.440794
741.081525	68.635772	71.445799
740.400322	70.676283	71.450804
740.228644	60.576870	71.455809
739.783957	70.925889	71.460814
739.034678	69.313917	71.465818
738.347284	67.073219	71.470823
737.710062	79.376701	71.475828
737.047560	68.864416	71.480833
736.144313	71.264264	71.485838
735.454712	72.706247	71.490842
735.150936	72.721157	71.495847
734.020552	70.566608	71.500852
733.532716	63.479748	71.505857
732.562283	62.831665	71.510862
731.239630	70.219147	71.515866
731.209703	66.038684	71.520871
730.897866	74.741088	71.525876
730.779147	66.364613	71.530881
729.344382	63.816970	71.535886
728.570395	69.389503	71.540890
728.188085	62.072605	71.545895
727.428089	68.085217	71.550900
727.159745	63.896258	71.555905
726.358563	69.591075	71.560910
725.739928	74.545714	71.565914
725.394649	68.710943	71.570919
724.323938	69.602852	71.575924
723.467010	62.716189	71.580929
722.726144	66.233290	71.585934
722.366816	71.320339	71.590938
722.377404	63.897848	71.595943
721.198677	69.974693	71.600948
720.042484	64.838547	71.605953
719.721649	68.466843	71.610958
718.963974	66.675138	71.615962
718.078129	65.121300	71.620967
716.996759	65.745446	71.625972
716.813504	61.562831	71.630977
716.286441	62.678567	71.635982
715.703459	68.266141	71.640986
715.599572	52.391883	71.645991
714.474142	66.320352	71.650996
714.045167	68.800000	71.656001
713.285435	70.162821	71.661006
711.508467	67.250275	71.666010
710.997793	70.414146	71.671015
710.249722	70.372545	71.676020
710.257441	65.848942	71.681025
709.565795	63.222551	71.686030
708.757282	68.969150	71.691034
708.582450	66.269617	71.696039
707.996983	71.721046	71.701044
707.491237	70.973627	71.706049
706.229704	64.998603	71.711054
705.776998	67.522183	71.716058
705.550523	64.513752	71.721063
704.587426	69.064399	71.726068
703.693134	71.814410	71.731073
703.149697	63.702530	71.736078
702.175729	67.857562	71.741082
702.237599	61.133618	71.746087
700.818309	70.707017	71.751092
700.322797	70.161912	71.756097
699.689546	64.914082	71.761102
698.825134	68.341042	71.766106
699.027730	55.604371	71.771111
697.571164	61.387780	71.776116
696.906462	69.876304	71.781121
696.001097	66.224348	71.786126
695.681653	66.522192	71.791130
695.528268	65.117600	71.796135
695.026650	68.943043	71.801140
694.262145	66.082044	71.806145
693.587728	64.703953	71.811150
692.514797	62.816269	71.816154
691.616185	60.544268	71.821159
690.437567	68.532311	71.826164
690.200071	60.945493	71.831169
689.999833	56.970254	71.836174
689.451269	64.409856	71.841178
689.276393	58.992324	71.846183
687.659651	67.990505	71.851188
686.723110	53.756447	71.856193
686.441979	59.708338	71.861198
686.145213	73.350388	71.866202
685.852656	64.775554	71.871207
684.513431	70.459531	71.876212
683.959175	62.590681	71.881217
683.002006	69.027449	71.886222
682.244647	67.799745	71.891226
682.532330	62.715052	71.896231
680.780583	72.706576	71.901236
680.023991	65.344863	71.906241
680.125135	66.317456	71.911246
679.568465	66.950004	71.916250
679.208678	64.822920	71.921255
677.796850	66.180230	71.926260
677.604464	63.755271	71.931265
676.899630	64.982777	71.936270
676.513978	68.769407	71.941274
675.697220	59.175628	71.946279
674.621253	64.945549	71.951284
674.045799	62.871991	71.956289
672.949279	56.786216	71.961294
672.437779	63.299388	71.966298
671.674933	63.056651	71.971303
670.989102	70.660686	71.976308
670.632900	62.565682	71.981313
670.654398	63.453241	71.986318
669.800175	60.658931	71.991322
669.327468	59.217868	71.996327
668.074437	68.428859	72.001332
667.255882	58.480147	72.006337
666.258612	61.016501	72.011342
665.128361	65.272912	72.016346
665.929133	52.578628	72.021351
664.910628	59.163659	72.026356
664.157322	55.688546	72.031361
663.756626	60.605058	72.036366
662.767467	61.010930	72.041370
662.216211	63.089184	72.046375
661.282751	61.999016	72.051380
660.965973	56.502383	72.056385
660.381844	57.912884	72.061390
659.022852	69.156657	72.066394
658.301697	55.753687	72.071399
657.619077	66.850399	72.076404
657.707672	60.610931	72.081409
657.108872	64.087123	72.086414
656.549403	63.363518	72.091418
655.668421	65.283142	72.096423
655.022095	64.170229	72.101428
654.792171	57.403128	72.106433
653.721759	61.941378	72.111438
652.275518	71.935434	72.116442
652.001705	58.278992	72.121447
651.426157	66.748294	72.126452
650.648258	63.565538	72.131457
650.290236	65.124004	72.136462
649.919431	65.713266	72.141466
649.155172	59.317956	72.146471
648.003748	68.005124	72.151476
647.627917	59.738629	72.156481
647.418282	68.305497	72.161486
646.141056	68.588629	72.166490
645.906404	59.276819	72.171495
644.627082	61.788082	72.176500
644.543538	57.119865	72.181505
643.647583	57.782520	72.186510
642.620349	58.412802	72.191514
642.335233	57.646142	72.196519
641.408432	67.603307	72.201524
641.826082	57.692271	72.206529
640.611993	66.469907	72.211534
639.373840	65.579963	72.216538
639.193041	58.201322	72.221543
638.616287	67.274351	72.226548
637.557712	62.224526	72.231553
636.473853	59.482592	72.236558
636.035008	62.412331	72.241562
635.613709	56.520736	72.246567
635.332667	70.094956	72.251572
634.909673	61.630896	72.256577
633.462087	61.758097	72.261582
632.554597	63.182162	72.266586
632.550389	62.420268	72.271591
631.724155	66.769461	72.276596
631.544638	58.263295	72.281601
630.643169	60.788768	72.286606
629.356419	64.593604	72.291610
629.451663	57.180302	72.296615
628.745223	70.857403	72.301620
627.655704	61.180111	72.306625
626.790479	65.645320	72.311630
625.973682	63.291030	72.316634
625.583567	57.046350	72.321639
625.173375	63.380728	72.326644
625.181654	63.310604	72.331649
624.305914	67.007921	72.336654
623.353411	63.244066	72.341658
623.082104	62.979487	72.346663
621.686835	67.089876	72.351668
620.856886	65.087952	72.356673
620.516294	72.557057	72.361678
619.990434	61.833117	72.366682
619.487003	57.474064	72.371687
618.371492	65.646294	72.376692
617.718177	65.764911	72.381697
617.348223	69.186111	72.386702
616.860337	65.639085	72.391706
615.963070	57.731130	72.396711
614.768698	72.904909	72.401716
614.043138	62.836466	72.406721
613.588331	61.583383	72.411726
613.282282	65.679253	72.416730
613.280337	61.087052	72.421735
612.280930	66.436916	72.426740
611.483919	61.770156	72.431745
610.423122	60.173293	72.436750
609.956170	69.701169	72.441754
609.438982	60.752753	72.446759
608.231611	72.624602	72.451764
607.673285	68.231929	72.456769
607.241777	70.758594	72.461774
606.640142	70.350492	72.466778
606.312335	64.837990	72.471783
605.294957	61.310242	72.476788
604.307374	64.563329	72.481793
603.911425	67.070876	72.486798
603.379317	76.096000	72.491802
603.362305	60.740526	72.496807
602.174868	74.373731	72.501812
601.294531	66.563527	72.506817
600.785979	65.625559	72.511822
600.021183	66.152072	72.516826
599.619249	59.258930	72.521831
598.769917	69.986336	72.526836
597.853412	63.801847	72.531841
597.341726	61.277662	72.536846
596.619828	73.173302	72.541850
596.491227	60.144454	72.546855
595.218382	65.354469	72.551860
594.564315	65.777148	72.556865
594.226487	61.338807	72.561870
593.928879	63.706353	72.566874
592.973357	57.452373	72.571879
592.021680	70.451926	72.576884
591.134270	60.738834	72.581889
591.204356	62.806158	72.586894
590.114086	65.547134	72.591898
589.161154	58.935889	72.596903
588.478228	65.350548	72.601908
588.186500	61.474277	72.606913
587.992808	65.355513	72.611918
586.873239	58.277846	72.616922
585.855731	67.171013	72.621927
585.345211	58.995497	72.626932
584.977111	61.719312	72.631937
584.310739	62.200545	72.636942
583.896526	63.761538	72.641946
583.037677	62.342831	72.646951
581.973862	67.425066	72.651956
581.562778	64.332624	72.656961
581.268326	58.092085	72.661966
580.065382	72.142398	72.666970
579.201948	59.460498	72.671975
578.363874	67.016810	72.676980
578.055154	66.654045	72.681985
577.674025	60.776889	72.686990
577.247942	65.400535	72.691994
576.827004	59.658483	72.696999
575.573885	62.194087	72.702004
574.884257	58.030356	72.707009
574.307272	63.507968	72.712014
573.498380	68.907691	72.717018
572.948182	61.044484	72.722023
572.359454	64.558035	72.727028
571.928263	52.915179	72.732033
571.304444	59.784288	72.737038
569.729134	66.604467	72.742042
569.621275	66.050190	72.747047
568.396617	66.357492	72.752052
568.181058	61.619140	72.757057
568.191585	67.860910	72.762062
567.565485	70.734717	72.767066
566.833880	56.300201	72.772071
565.886673	65.068434	72.777076
564.863216	66.042671	72.782081
564.360240	65.170458	72.787086
563.541223	67.260260	72.792090
563.082563	64.649234	72.797095
562.033645	72.407457	72.802100
561.634995	71.679202	72.807105
561.344185	68.006053	72.812110
560.192286	75.299975	72.817114
559.722565	69.617989	72.822119
559.010354	75.902284	72.827124
558.532676	67.657198	72.832129
557.974457	68.483831	72.837134
556.538404	71.450236	72.842138
556.147383	64.323137	72.847143
555.103968	68.385491	72.852148
554.597661	68.665628	72.857153
554.920216	63.058277	72.862158
554.233790	66.137805	72.867162
553.785846	61.226521	72.872167
552.474393	63.454775	72.877172
551.965132	69.186034	72.882177
551.525898	72.297810	72.887182
550.494922	72.176031	72.892186
550.012782	58.998570	72.897191
549.187055	70.068099	72.902196
548.807097	61.146706	72.907201
547.764488	63.893339	72.912206
546.895526	66.895992	72.917210
546.787630	58.386249	72.922215
546.021010	62.510117	72.927220
545.499641	62.835465	72.932225
544.745389	63.172296	72.937230
543.554668	65.262636	72.942234
543.219475	60.032841	72.947239
542.781779	67.434506	72.952244
541.939498	58.327084	72.957249
540.693801	64.853569	72.962254
539.840178	68.286992	72.967258
539.651506	67.130808	72.972263
539.022997	63.202122	72.977268
538.709659	61.505227	72.982273
538.700064	65.856206	72.987278
537.536445	66.789731	72.992282
537.032778	56.237265	72.997287
536.232399	62.572189	73.002292
535.326119	61.471864	73.007297
534.330470	63.077227	73.012302
533.045536	74.346226	73.017306
533.089929	58.271732	73.022311
532.382857	64.161220	73.027316
532.609042	58.143697	73.032321
531.898461	59.714030	73.037326
531.293297	65.763678	73.042330
530.149827	63.876279	73.047335
529.495438	63.223030	73.052340
528.620118	62.501064	73.057345
527.855284	64.681449	73.062350
526.905125	62.009786	73.067354
526.824906	56.568157	73.072359
526.176452	58.348885	73.077364
525.716650	59.945323	73.082369
525.033902	60.996970	73.087374
523.655376	63.157386	73.092378
523.462099	60.810744	73.097383
522.778574	65.141813	73.102388
522.547837	56.094996	73.107393
521.781303	56.874436	73.112398
520.819091	63.358270	73.117402
520.589065	63.199118	73.122407
519.511666	57.058010	73.127412
518.625144	61.014147	73.132417
518.352078	58.918402	73.137422
517.800724	64.958041	73.142426
516.260284	62.396603	73.147431
515.337746	65.362654	73.152436
515.047728	53.939159	73.157441
514.709355	52.324709	73.162446
514.124676	58.269404	73.167450
514.482699	52.308236	73.172455
513.269645	56.255197	73.177460
512.421379	53.699887	73.182465
511.582420	66.609868	73.187470
510.936990	59.715834	73.192474
510.035014	53.737292	73.197479
509.103802	67.965638	73.202484
508.234015	60.940321	73.207489
508.051936	62.536538	73.212494
507.569329	71.610807	73.217498
507.634319	60.945509	73.222503
506.363417	64.742527	73.227508
505.607069	55.496057	73.232513
504.969358	61.838635	73.237518
504.313368	68.250659	73.242522
504.275824	57.280452	73.247527
502.586333	64.356251	73.252532
501.748574	63.629827	73.257537
501.469881	64.638687	73.262542
500.862260	67.821947	73.267546
500.673184	63.646664	73.272551
499.579308	58.720947	73.277556
498.862585	53.092353	73.282561
498.372054	58.465948	73.287566
497.947138	64.822193	73.292570
497.549829	51.518116	73.297575
496.148942	59.131401	73.302580
495.608498	53.402342	73.307585
495.430248	56.123233	73.312590
494.485627	56.409802	73.317594
493.470534	62.123139	73.322599
492.625796	59.507232	73.327604
492.121583	56.404314	73.332609
491.810068	56.889880	73.337614
491.556771	56.870894	73.342618
490.807616	51.440480	73.347623
489.625369	60.033875	73.352628
488.991494	60.972947	73.357633
488.635577	61.763737	73.362638
487.204176	56.045647	73.367642
487.020092	58.624257	73.372647
486.283220	62.238590	73.377652
485.767242	60.444982	73.382657
485.534516	64.285541	73.387662
484.733331	66.412560	73.392666
483.814243	58.296024	73.397671
482.888446	65.652257	73.402676
482.415413	55.984634	73.407681
482.037328	68.056607	73.412686
480.815618	64.735605	73.417690
480.216468	55.833631	73.422695
479.455335	64.931151	73.427700
479.034273	55.074635	73.432705
478.589343	60.825658	73.437710
478.067134	69.149255	73.442714
477.975230	59.925109	73.447719
476.220987	64.304271	73.452724
475.708532	61.392625	73.457729
475.456804	66.900951	73.462734
474.637732	60.381660	73.467738
473.844131	61.369813	73.472743
473.027307	67.357057	73.477748
472.584475	56.781549	73.482753
472.371405	68.609731	73.487758
471.573212	70.308369	73.492762
470.495256	65.947135	73.497767
469.623299	64.749368	73.502772
469.461423	65.667952	73.507777
468.842132	65.178030	73.512782
467.540911	71.166971	73.517786
467.013235	67.586918	73.522791
466.343526	70.265720	73.527796
465.961387	62.672929	73.532801
465.535980	64.751345	73.537806
464.706695	70.403640	73.542810
463.856905	58.305986	73.547815
463.361534	66.343157	73.552820
462.642188	60.094527	73.557825
462.338566	64.760345	73.562830
461.103294	76.254123	73.567834
460.540386	60.239499	73.572839
459.747365	73.614088	73.577844
459.520142	69.650990	73.582849
458.848149	65.393078	73.587854
457.904757	74.072258	73.592858
457.413225	70.696000	73.597863
456.591295	69.919112	73.602868
456.378047	58.598119	73.607873
455.744972	58.987221	73.612878
454.381307	62.737387	73.617882
453.967227	66.645337	73.622887
453.324276	67.719777	73.627892
452.735477	72.825235	73.632897
452.360966	64.320532	73.637902
451.220412	76.455674	73.642906
450.818729	64.481744	73.647911
449.921795	72.689568	73.652916
449.677230	69.647154	73.657921
449.251877	70.096576	73.662926
447.997247	74.604070	73.667930
447.183432	65.614154	73.672935
446.454266	64.710062	73.677940
446.330443	63.406594	73.682945
446.289111	59.804779	73.687950
445.147967	68.879009	73.692954
444.727126	63.631931	73.697959
443.473730	59.091967	73.702964
442.392290	62.199332	73.707969
441.859367	59.618812	73.712974
441.347530	66.040476	73.717978
441.245252	60.680786	73.722983
440.533946	65.352920	73.727988
439.385395	69.968939	73.732993
438.701876	71.409523	73.737998
438.267927	67.419093	73.743002
437.888448	64.401774	73.748007
436.756104	62.632487	73.753012
435.977806	62.050219	73.758017
435.357831	60.848749	73.763022
434.414917	66.422629	73.768026
434.172615	58.539845	73.773031
433.297180	69.628161	73.778036
433.271417	65.242143	73.783041
432.693233	68.014599	73.788046
431.724024	71.061291	73.793050
430.984029	58.723002	73.798055
430.335762	67.656325	73.803060
429.710575	58.003340	73.808065
428.811430	64.264811	73.813070
427.802454	67.382655	73.818074
427.881443	59.873471	73.823079
426.921798	70.948984	73.828084
426.774674	63.384211	73.833089
425.793467	55.916591	73.838094
425.227502	62.690932	73.843098
424.754153	64.016952	73.848103
423.264187	64.088720	73.853108
422.307099	61.854033	73.858113
422.167410	62.297527	73.863118
421.178105	66.496281	73.868122
421.022099	58.106501	73.873127
420.797251	62.661721	73.878132
420.266331	65.816056	73.883137
419.499462	66.814242	73.888142
418.332814	65.820924	73.893146
418.477672	59.980357	73.898151
417.055426	73.449752	73.903156
416.322137	67.742303	73.908161
415.899228	68.142365	73.913166
415.299683	73.824766	73.918170
414.178708	65.647322	73.923175
413.235735	66.665820	73.928180
412.802881	69.782826	73.933185
412.372965	63.472764	73.938190
411.964718	70.090219	73.943194
411.696083	63.299386	73.948199
410.689727	69.019135	73.953204
409.930758	57.949164	73.958209
409.309845	66.334278	73.963214
408.642193	69.438630	73.968218
407.541712	69.449576	73.973223
406.614971	75.147790	73.978228
406.033147	63.659453	73.983233
405.730356	62.075623	73.988238
405.162982	68.834815	73.993242
405.123552	62.044570	73.998247
404.328550	66.594480	74.003252
403.074457	58.411832	74.008257
402.868244	64.307465	74.013262
402.154977	67.528576	74.018266
400.986853	70.713171	74.023271
400.268036	71.758385	74.028276
399.559709	67.990235	74.033281
399.294063	66.814094	74.038286
398.648243	70.130220	74.043290
398.377502	62.547163	74.048295
397.241827	68.941144	74.053300
396.430099	55.541933	74.058305
396.265871	59.322992	74.063310
395.447608	61.610836	74.068314
394.498839	56.953949	74.073319
393.799446	66.175492	74.078324
393.118339	64.871616	74.083329
392.861147	64.225312	74.088334
392.023832	67.310192	74.093338
391.247380	65.033898	74.098343
390.591507	60.830866	74.103348
389.953170	61.364554	74.108353
389.404043	64.312418	74.113358
388.925088	67.535214	74.118362
388.070185	67.438161	74.123367
386.780612	68.079904	74.128372
386.780239	65.691133	74.133377
386.493877	66.715522	74.138382
385.579400	70.533980	74.143386
384.642925	65.310151	74.148391
384.088568	69.626597	74.153396
383.655311	71.536243	74.158401
383.044774	65.785267	74.163406
381.810692	62.186957	74.168410
381.118964	57.943496	74.173415
380.485478	64.181943	74.178420
380.175286	66.012870	74.183425
380.024490	55.565350	74.188430
378.409977	67.058208	74.193434
378.335884	63.518455	74.198439
377.448494	69.219399	74.203444
376.501558	62.575606	74.208449
376.226838	60.754481	74.213454
375.074577	61.193495	74.218458
374.666360	60.189808	74.223463
374.247226	63.851931	74.228468
373.702466	58.651364	74.233473
373.363891	53.904513	74.238478
372.177497	63.070184	74.243482
371.672176	67.948983	74.248487
370.808427	68.219349	74.253492
370.428420	64.939643	74.258497
369.229675	60.103774	74.263502
368.427994	63.621471	74.268506
368.277839	55.428843	74.273511
367.482978	50.385610	74.278516
367.138392	58.295495	74.283521
366.798920	66.805262	74.288526
365.796334	60.619010	74.293530
365.224291	53.780718	74.298535
363.775926	53.863927	74.303540
362.707475	53.923075	74.308545
363.030571	61.414603	74.313550
362.291011	63.467134	74.318554
361.910620	59.191238	74.323559
361.349421	63.549118	74.328564
360.349037	62.581792	74.333569
359.654333	55.593216	74.338574
358.862574	64.367591	74.343578
358.456656	59.938185	74.348583
358.017704	70.572775	74.353588
356.878118	58.729282	74.358593
356.135372	57.943579	74.363598
355.099614	73.702792	74.368602
355.157668	60.471084	74.373607
354.507776	65.545966	74.378612
353.661512	73.156992	74.383617
352.944904	57.506621	74.388622
352.143782	63.820771	74.393626
351.664814	59.674659	74.398631
351.038840	64.000223	74.403636
350.565017	75.013796	74.408641
349.514450	61.579349	74.413646
348.657958	66.910286	74.418650
348.539882	63.423464	74.423655
347.784228	65.718347	74.428660
347.639810	61.859878	74.433665
346.505542	53.617246	74.438670
345.685553	57.267548	74.443674
345.375191	54.632715	74.448679
344.257801	62.888985	74.453684
343.524526	56.822364	74.458689
342.752974	60.287140	74.463694
341.906934	64.435302	74.468698
342.100304	62.192922	74.473703
341.508773	61.729442	74.478708
340.721709	56.451600	74.483713
339.839555	58.198592	74.488718
338.691396	68.672509	74.493722
338.444171	61.713816	74.498727
338.292840	61.761436	74.503732
337.464690	62.106228	74.508737
336.599305	62.383986	74.513742
335.633672	64.504870	74.518746
335.604162	56.512214	74.523751
334.308507	59.250943	74.528756
333.443465	65.450137	74.533761
333.299380	65.599141	74.538766
332.398462	68.231536	74.543770
332.156035	62.199599	74.548775
331.316224	64.208925	74.553780
330.217161	65.694692	74.558785
329.508521	62.189095	74.563790
328.987336	69.786246	74.568794
328.562588	58.527181	74.573799
328.329877	70.680411	74.578804
327.597824	65.271569	74.583809
326.765205	62.032339	74.588814
326.051970	65.672244	74.593818
325.658955	63.151834	74.598823
324.273745	70.583669	74.603828
323.506128	64.844233	74.608833
323.120587	65.452227	74.613838
322.970170	73.604351	74.618842
322.491862	64.406581	74.623847
321.303715	69.204267	74.628852
320.515471	62.643810	74.633857
320.314143	63.689547	74.638862
319.660742	61.119035	74.643866
318.637765	59.600623	74.648871
317.666564	72.073044	74.653876
317.190950	58.655721	74.658881
317.004456	62.906358	74.663886
316.223586	62.532171	74.668890
315.236158	60.617690	74.673895
314.659734	69.976048	74.678900
313.994802	64.208753	74.683905
313.979271	59.594029	74.688910
312.770012	67.744480	74.693914
311.925885	61.991715	74.698919
311.114640	66.276409	74.703924
310.709942	63.055808	74.708929
310.412041	59.608099	74.713934
309.483761	61.993754	74.718938
308.631987	59.669206	74.723943
307.578625	62.246816	74.728948
307.369294	63.244980	74.733953
307.587063	58.797890	74.738958
306.198432	66.332939	74.743962
305.270786	62.177292	74.748967
304.661130	63.209335	74.753972
304.125459	63.342171	74.758977
303.876241	55.466118	74.763982
303.012717	66.652261	74.768986
302.044595	63.518361	74.773991
301.034219	64.405152	74.778996
301.090695	64.611355	74.784001
300.466995	63.678158	74.789006
298.817222	66.644555	74.794010
298.473717	54.827660	74.799015
298.000883	69.207964	74.804020
297.498286	66.591872	74.809025
297.342785	68.198143	74.814030
296.296591	70.928072	74.819034
295.745481	62.724044	74.824039
294.520591	71.001909	74.829044
294.481683	62.499709	74.834049
294.076099	62.445260	74.839054
292.537928	73.059055	74.844058
292.068052	60.839103	74.849063
291.350302	66.238235	74.854068
291.238491	66.957990	74.859073
290.557984	64.546856	74.864078
289.109697	65.608174	74.869082
288.602932	62.125218	74.874087
287.886955	64.058461	74.879092
287.515126	67.592883	74.884097
287.392132	57.984507	74.889102
286.582421	63.164545	74.894106
286.169244	63.252310	74.899111
285.082316	66.033430	74.904116
284.284013	61.164871	74.909121
283.880937	62.640691	74.914126
282.744066	69.238569	74.919130
282.279497	61.052473	74.924135
281.576572	71.163919	74.929140
281.399532	63.071427	74.934145
280.602815	61.280178	74.939150
279.415244	63.069266	74.944154
279.099723	58.645297	74.949159
278.559508	67.866009	74.954164
277.638955	68.426375	74.959169
277.126458	65.819877	74.964174
276.140091	69.691724	74.969178
275.723334	61.762682	74.974183
275.122552	61.057258	74.979188
274.824129	62.502510	74.984193
273.919253	59.875247	74.989198
272.902694	70.696859	74.994202
272.420380	62.003836	74.999207
271.923537	69.549846	75.004212
271.176633	71.119335	75.009217
269.923740	60.322340	75.014222
269.211678	60.931046	75.019226
269.035226	59.988296	75.024231
268.874681	56.763350	75.029236
268.225390	58.843840	75.034241
267.135511	61.934134	75.039246
266.397204	63.342291	75.044250
266.225824	60.655223	75.049255
265.516530	61.743426	75.054260
263.823888	57.975082	75.059265
263.590615	64.528601	75.064270
262.743317	68.754354	75.069274
262.678625	56.820204	75.074279
262.184633	62.657008	75.079284
261.709832	60.752168	75.084289
261.166684	54.446148	75.089294
260.254547	59.880573	75.094298
259.444968	52.537918	75.099303
258.422853	63.081811	75.104308
257.338315	58.332580	75.109313
257.286550	54.245882	75.114318
256.674719	64.601432	75.119322
256.259612	59.539706	75.124327
255.386008	64.536501	75.129332
254.649744	69.018733	75.134337
254.038130	64.462765	75.139342
253.404395	71.609896	75.144346
251.778879	62.556678	75.149351
251.212963	63.204674	75.154356
251.336542	60.366791	75.159361
250.662815	58.507497	75.164366
249.830109	67.505597	75.169370
249.689292	55.910926	75.174375
249.193853	56.454874	75.179380
248.065761	62.765477	75.184385
247.498961	60.279996	75.189390
246.672845	64.129115	75.194394
246.082779	59.206715	75.199399
244.813934	59.541014	75.204404
244.047295	65.843739	75.209409
243.985748	64.075290	75.214414
243.004528	68.612142	75.219418
242.715441	58.881855	75.224423
242.402526	68.414902	75.229428
241.582462	64.895264	75.234433
241.173597	58.609648	75.239438
240.224554	63.980933	75.244442
240.080261	56.862120	75.249447
238.438742	58.611404	75.254452
237.762040	64.382823	75.259457
237.380672	60.075928	75.264462
236.775152	65.945667	75.269466
236.485061	59.677979	75.274471
235.555010	60.530490	75.279476
234.683084	58.650305	75.284481
234.098663	55.342897	75.289486
233.142806	61.792127	75.294490
233.038658	59.777970	75.299495
232.209518	57.407324	75.304500
231.350880	63.968568	75.309505
230.780924	54.958626	75.314510
229.984829	70.699655	75.319514
230.228418	54.572520	75.324519
229.064448	64.746414	75.329524
228.485342	62.396063	75.334529
227.824859	67.547768	75.339534
226.053168	68.788085	75.344538
225.292309	60.363464	75.349543
225.227693	58.282534	75.354548
224.944588	66.318453	75.359553
224.408306	57.803236	75.364558
223.792227	64.502893	75.369562
223.461954	59.489784	75.374567
222.267866	58.269130	75.379572
221.529908	59.435274	75.384577
221.055132	54.453252	75.389582
220.134442	65.784980	75.394586
219.782422	60.212342	75.399591
218.864405	65.579497	75.404596
218.216227	60.162224	75.409601
217.812840	56.887335	75.414606
217.120544	54.490077	75.419610
216.492290	59.789799	75.424615
215.703261	58.026059	75.429620
215.064222	57.702573	75.434625
214.730647	57.557634	75.439630
213.193181	59.336851	75.444634
212.722948	52.316937	75.449639
212.183631	66.580744	75.454644
211.798919	63.416330	75.459649
211.532945	58.359834	75.464654
210.176156	69.960518	75.469658
209.317793	62.798723	75.474663
208.779186	68.303726	75.479668
208.388565	66.567214	75.484673
208.238061	57.194077	75.489678
206.983894	66.817419	75.494682
206.275521	56.772193	75.499687
205.929974	65.008671	75.504692
205.209441	65.215046	75.509697
204.869896	53.457094	75.514702
203.218406	66.645700	75.519706
202.938431	58.286276	75.524711
202.534628	56.497950	75.529716
201.710774	60.287874	75.534721
201.234344	58.697907	75.539726
199.457424	57.205348	75.544730
199.631361	62.842402	75.549735
199.017115	65.614746	75.554740
198.567286	64.460324	75.559745
198.551458	56.786236	75.564750
197.307387	61.961404	75.569754
196.449102	65.040039	75.574759
195.912933	68.034249	75.579764
195.247609	66.275358	75.584769
194.988224	60.413703	75.589774
193.322877	65.875811	75.594778
192.739902	56.098024	75.599783
192.537467	60.967934	75.604788
192.357848	64.621375	75.609793
191.613659	69.487845	75.614798
190.490794	64.590868	75.619802
189.841023	57.418980	75.624807
188.977497	62.078944	75.629812
188.531462	58.905311	75.634817
187.901671	56.587338	75.639822
186.449002	59.002908	75.644826
186.599591	53.655549	75.649831
186.115815	60.532252	75.654836
185.659989	58.573645	75.659841
185.289392	53.354704	75.664846
184.063510	51.958734	75.669850
183.835219	55.452369	75.674855
182.660741	46.096888	75.679860
181.619850	51.453134	75.684865
180.920851	49.650681	75.689870
180.382103	60.952854	75.694874
180.320353	49.263729	75.699879
179.531967	56.074628	75.704884
178.272503	54.313385	75.709889
177.979454	48.668679	75.714894
177.368126	54.029838	75.719898
176.922349	54.197802	75.724903
176.190165	60.374633	75.729908
174.791169	61.624497	75.734913
174.467426	52.631175	75.739918
173.852108	56.360093	75.744922
173.609079	53.823464	75.749927
173.120226	53.855926	75.754932
172.169750	55.704258	75.759937
171.670529	54.296612	75.764942
170.639244	62.193168	75.769946
170.230294	54.527268	75.774951
168.792559	56.504915	75.779956
168.025502	54.165874	75.784961
167.722510	53.351394	75.789966
167.282320	56.956744	75.794970
166.844918	48.641685	75.799975
166.406121	53.987479	75.804980
165.727447	60.602742	75.809985
164.975311	54.594261	75.814990
164.005731	62.207494	75.819994
163.860589	50.061774	75.824999
163.155155	56.193363	75.830004
161.915607	57.783770	75.835009
161.541814	50.911929	75.840014
160.750408	56.654466	75.845018
160.685463	47.252465	75.850023
159.354246	51.167655	75.855028
158.706656	60.587155	75.860033
158.132954	64.030669	75.865038
157.574667	71.537482	75.870042
157.125374	62.359640	75.875047
156.135263	54.973752	75.880052
154.710852	58.262723	75.885057
154.650878	51.112889	75.890062
154.133876	59.246922	75.895066
154.016487	54.281798	75.900071
152.897571	58.521364	75.905076
151.974766	61.735400	75.910081
151.756326	57.901082	75.915086
150.724653	67.045003	75.920090
150.658583	55.025849	75.925095
149.897122	64.528421	75.930100
148.648056	61.445878	75.935105
147.906281	54.599228	75.940110
147.084117	66.641133	75.945114
147.095462	61.890765	75.950119
146.899093	60.053069	75.955124
145.694479	57.142502	75.960129
144.895030	59.791083	75.965134
144.269347	60.465915	75.970138
143.873290	56.765067	75.975143
142.887774	62.732319	75.980148
141.781823	65.069520	75.985153
141.597995	58.186033	75.990158
140.672988	62.904699	75.995162
140.824704	57.233087	76.000167
140.251778	54.781434	76.005172
139.061522	62.085548	76.010177
138.275118	56.396348	76.015182
137.873267	63.900812	76.020186
137.303022	52.752783	76.025191
135.703978	62.946803	76.030196
135.327095	57.797231	76.035201
135.104971	50.119047	76.040206
134.277710	55.386973	76.045210
134.145635	56.182831	76.050215
133.448898	61.821911	76.055220
132.470436	56.550089	76.060225
131.790801	47.507663	76.065230
131.228285	58.022115	76.070234
130.415533	51.752867	76.075239
129.426234	51.866390	76.080244
128.792440	62.830801	76.085249
128.623121	52.900806	76.090254
127.710613	57.860077	76.095258
127.490639	52.228110	76.100263
126.450350	54.446299	76.105268
125.546837	57.496383	76.110273
125.109065	60.643850	76.115278
124.592142	54.524401	76.120282
124.356558	49.308375	76.125287
122.918738	64.813248	76.130292
122.298546	58.890701	76.135297
122.218368	56.725212	76.140302
121.640757	50.885758	76.145306
120.440719	58.137475	76.150311
119.655146	57.569930	76.155316
119.021693	57.172478	76.160321
118.749063	53.921762	76.165326
117.928940	60.512728	76.170330
117.293182	58.328018	76.175335
116.350767	56.278375	76.180340
115.929660	57.451790	76.185345
115.650079	52.079107	76.190350
115.000460	63.214379	76.195354
114.282601	53.048840	76.200359
113.582850	59.528386	76.205364
112.329441	59.896388	76.210369
112.070278	66.551442	76.215374
111.001044	63.559652	76.220378
110.941442	61.801926	76.225383
110.078528	61.799845	76.230388
108.725513	58.297399	76.235393
107.816739	56.956815	76.240398
107.285221	67.100060	76.245402
107.582046	59.656178	76.250407
106.784208	55.641344	76.255412
106.055554	57.877160	76.260417
105.926333	52.778682	76.265422
105.009174	62.241636	76.270426
104.163282	55.886896	76.275431
103.834862	51.457661	76.280436
102.721638	62.146260	76.285441
102.042119	56.792407	76.290446
101.006906	57.320756	76.295450
101.049835	53.273094	76.300455
100.180496	61.639628	76.305460
98.882192	61.422077	76.310465
98.394149	63.430340	76.315470
97.670015	64.000485	76.320474
97.250886	53.749791	76.325479
97.316250	53.371871	76.330484
96.664081	58.537947	76.335489
95.865595	59.748037	76.340494
94.587186	60.846996	76.345498
94.369478	60.501818	76.350503
93.027266	60.850710	76.355508
92.526559	60.115918	76.360513
91.666250	60.152470	76.365518
90.976942	65.050590	76.370522
90.624670	56.092959	76.375527
90.260863	61.890084	76.380532
89.770833	63.099395	76.385537
89.472891	53.879441	76.390542
88.295262	68.219915	76.395546
87.573347	56.034937	76.400551
87.022875	64.059455	76.405556
85.426151	60.540776	76.410561
84.879146	55.791012	76.415566
84.321368	59.514022	76.420570
83.880901	64.657621	76.425575
83.508644	64.690233	76.430580
82.981492	63.040691	76.435585
83.007815	61.552427	76.440590
82.016583	55.869544	76.445594
80.894645	61.062479	76.450599
80.426217	68.682564	76.455604
79.556235	68.563286	76.460609
78.688836	60.209859	76.465614
77.781050	61.456059	76.470618
77.531120	57.723062	76.475623
77.315727	59.511698	76.480628
76.693558	60.839185	76.485633
75.590541	59.849654	76.490638
74.710109	62.621464	76.495642
74.276069	59.987335	76.500647
73.811419	66.235539	76.505652
72.958250	58.960794	76.510657
72.022141	54.451811	76.515662
71.117505	62.996494	76.520666
71.177660	54.632460	76.525671
70.513625	60.940108	76.530676
70.115398	54.374425	76.535681
69.566797	56.442411	76.540686
68.665651	58.116131	76.545690
67.961247	48.849034	76.550695
66.920103	54.025750	76.555700
65.986869	55.466170	76.560705
65.651027	56.464323	76.565710
64.742246	53.553584	76.570714
64.390636	58.417490	76.575719
64.148460	60.271110	76.580724
62.831765	59.806475	76.585729
62.489062	54.705130	76.590734
61.956119	73.304548	76.595738
61.114145	55.564844	76.600743
60.160941	59.750362	76.605748
59.279950	60.603179	76.610753
58.888768	52.697031	76.615758
58.307336	66.748591	76.620762
57.994159	57.783078	76.625767
57.580399	62.299637	76.630772
56.416759	57.853350	76.635777
56.033493	53.984937	76.640782
55.187914	60.980118	76.645786
54.983113	57.816455	76.650791
53.932368	61.635038	76.655796
53.149598	60.480481	76.660801
52.529940	53.970921	76.665806
51.633635	59.979334	76.670810
50.813103	58.697050	76.675815
49.873888	58.917259	76.680820
49.608041	60.135504	76.685825
49.081633	55.753245	76.690830
48.494521	63.720892	76.695834
48.364200	60.034887	76.700839
47.778708	64.430505	76.705844
46.588829	66.514105	76.710849
46.472104	60.175669	76.715854
45.395565	72.872999	76.720858
44.395691	58.340966	76.725863
43.713929	66.507200	76.730868
43.142406	68.665562	76.735873
42.705932	54.139958	76.740878
41.909409	65.089248	76.745882
40.790537	57.216686	76.750887
40.021291	57.611032	76.755892
39.447149	66.479954	76.760897
39.202132	66.923360	76.765902
38.658619	67.038230	76.770906
38.824791	56.794557	76.775911
37.729628	63.015872	76.780916
36.808990	64.835431	76.785921
36.240524	62.076337	76.790926
35.083057	70.922518	76.795930
34.218828	66.438321	76.800935
33.370146	67.880435	76.805940
33.112225	62.896388	76.810945
32.773033	70.989286	76.815950
31.762220	68.497469	76.820954
32.019783	74.210167	76.825959
31.151449	65.554956	76.830964
30.130507	62.563591	76.835969
29.563340	61.074065	76.840974
28.696208	69.679427	76.845978
27.758394	56.583778	76.850983
26.988352	66.442281	76.855988
26.380953	61.846951	76.860993
25.773842	62.103376	76.865998
25.664397	64.621040	76.871002
25.111480	57.100629	76.876007
24.319012	63.470563	76.881012
23.406817	61.735476	76.886017
23.281778	53.601740	76.891022
22.120488	66.288731	76.896026
21.323464	61.319360	76.901031
20.537803	64.610161	76.906036
19.901857	68.217903	76.911041
19.513448	65.538458	76.916046
18.833167	59.754911	76.921050
18.394770	55.284545	76.926055
17.304432	59.517265	76.931060
16.371678	64.802112	76.936065
16.086586	48.642111	76.941070
15.705004	60.139952	76.946074
15.634547	58.219101	76.951079
14.410087	61.293050	76.956084
13.746870	62.204057	76.961089
13.089725	55.680012	76.966094
11.553640	62.077188	76.971098
11.237800	62.242624	76.976103
10.918671	61.626305	76.981108
10.389941	57.898488	76.986113
10.288625	52.118303	76.991118
8.766752	63.930862	76.996122
8.381274	56.207284	77.001127
7.932917	63.505393	77.006132
6.971534	61.624806	77.011137
5.897089	59.025493	77.016142
4.767330	61.917428	77.021147
4.838573	58.664994	77.026151
3.983908	62.183535	77.031156
3.658619	66.435865	77.036161