Tue Jun 08 17:58:11 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.167065	97.386980	0.000000
-1.244272	88.401159	0.005005
-2.133661	68.551188	0.010010
-3.803266	19.696993	0.015014
-8.567761	5.383448	0.020019
-13.867395	10.660006	0.025024
-18.390211	6.508322	0.030029
-23.424947	13.220033	0.035034
-27.188373	9.463907	0.040038
-30.959466	8.160649	0.045043
-34.538033	4.197188	0.050048
-38.380203	2.406026	0.055053
-42.241217	15.685008	0.060058
-45.472702	6.346467	0.065062
-49.441300	12.159391	0.070067
-52.846171	14.155111	0.075072
-56.636578	4.373242	0.080077
-60.700692	15.982702	0.085082
-64.473040	3.601730	0.090086
-68.189888	11.174934	0.095091
-71.908791	7.413186	0.100096
-75.556743	10.594476	0.105101
-79.532064	12.753555	0.110106
-83.237539	13.193974	0.115110
-87.383984	8.643503	0.120115
-90.963299	13.034271	0.125120
-94.198929	11.205855	0.130125
-98.212575	13.649003	0.135130
-101.658648	6.210735	0.140134
-105.909625	12.473153	0.145139
-109.643928	8.466594	0.150144
-113.404231	11.641918	0.155149
-117.483022	18.383998	0.160154
-120.698127	8.464062	0.165158
-124.652512	11.056138	0.170163
-128.663649	2.773409	0.175168
-132.112389	7.984917	0.180173
-136.163546	13.385781	0.185178
-139.677028	3.759384	0.190182
-143.042560	13.357654	0.195187
-147.202014	16.941696	0.200192
-150.761237	3.021595	0.205197
-154.894082	12.984733	0.210202
-158.362798	0.289301	0.215206
-162.157244	5.121197	0.220211
-166.116245	9.433853	0.225216
-169.715504	8.920663	0.230221
-174.307151	17.178015	0.235226
-177.765199	11.159663	0.240230
-180.890427	7.915497	0.245235
-184.494071	9.236896	0.250240
-188.464854	5.619887	0.255245
-192.763904	16.291646	0.260250
-196.491269	16.000566	0.265254
-200.025302	12.670218	0.270259
-203.852431	16.579000	0.275264
-207.199644	-1.590938	0.280269
-211.210244	11.282396	0.285274
-214.874264	8.896792	0.290278
-218.591747	12.922167	0.295283
-222.540688	3.008577	0.300288
-226.201895	-2.151126	0.305293
-230.123157	2.894401	0.310298
-233.755072	9.589140	0.315302
-237.529900	8.023032	0.320307
-241.133191	5.018392	0.325312
-244.573252	3.548812	0.330317
-248.763057	14.305689	0.335322
-252.546685	1.142152	0.340326
-256.431848	13.029336	0.345331
-260.352773	2.300244	0.350336
-264.129820	0.348119	0.355341
-268.002391	5.870820	0.360346
-271.449648	1.570056	0.365350
-274.933200	4.547656	0.370355
-279.143139	7.277636	0.375360
-282.503025	-1.761597	0.380365
-286.448677	16.288328	0.385370
-290.339469	6.367987	0.390374
-294.232790	12.406603	0.395379
-297.815177	23.680615	0.400384
-301.386484	10.443992	0.405389
-305.478929	13.313701	0.410394
-309.017149	12.070203	0.415398
-312.961786	9.843728	0.420403
-316.295008	9.223449	0.425408
-319.975641	14.003978	0.430413
-324.016126	17.486460	0.435418
-327.525060	11.146984	0.440422
-331.861772	14.951844	0.445427
-335.948602	14.419007	0.450432
-339.170492	6.948012	0.455437
-343.252422	8.050019	0.460442
-346.652716	9.878996	0.465446
-350.559096	6.161489	0.470451
-354.306887	4.957135	0.475456
-357.498486	1.672777	0.480461
-361.920629	2.921574	0.485466
-365.342214	1.769818	0.490470
-368.946897	10.246046	0.495475
-372.883987	5.564421	0.500480
-376.391028	11.792219	0.505485
-380.947117	17.263328	0.510490
-384.448005	8.346647	0.515494
-388.249326	11.065838	0.520499
-392.002143	12.663631	0.525504
-395.124451	2.955753	0.530509
-399.518684	13.263119	0.535514
-402.665118	-0.911092	0.540518
-406.717520	5.067277	0.545523
-411.129484	6.579226	0.550528
-414.074519	-3.044577	0.555533
-418.376022	0.776029	0.560538
-421.989099	0.984970	0.565542
-425.732629	3.702960	0.570547
-429.449955	4.553826	0.575552
-432.693382	2.686344	0.580557
-437.139204	8.588163	0.585562
-440.511550	4.794518	0.590566
-444.343961	11.787475	0.595571
-448.679564	7.726091	0.600576
-451.729382	0.327899	0.605581
-455.912098	1.992392	0.610586
-459.291470	8.132823	0.615590
-463.105617	-0.081535	0.620595
-466.961841	2.231906	0.625600
-470.979924	1.991326	0.630605
-474.767857	9.731359	0.635610
-478.216834	0.181035	0.640614
-482.313563	9.608147	0.645619
-485.987308	12.118834	0.650624
-489.574106	3.449471	0.655629
-493.525840	5.399610	0.660634
-497.271892	8.586612	0.665638
-501.063610	5.382824	0.670643
-504.463594	10.578733	0.675648
-508.029076	4.065973	0.680653
-512.086220	1.564530	0.685658
-515.815029	0.649142	0.690662
-519.771961	5.016998	0.695667
-523.770952	-0.208823	0.700672
-527.560993	1.017732	0.705677
-530.997754	8.130754	0.710682
-534.509048	3.721596	0.715686
-538.138931	7.284987	0.720691
-541.834059	8.267128	0.725696
-545.621712	1.381235	0.730701
-549.935845	7.371477	0.735706
-553.571079	1.022689	0.740710
-557.356965	4.633386	0.745715
-561.357171	4.834658	0.750720
-564.533621	2.716985	0.755725
-568.508650	4.944719	0.760730
-572.367922	5.625073	0.765734
-576.397290	1.699159	0.770739
-580.112653	8.110073	0.775744
-583.522881	-3.560469	0.780749
-587.390277	1.968312	0.785754
-590.867164	-0.430135	0.790758
-594.803570	-2.464356	0.795763
-598.988780	7.073947	0.800768
-602.865910	0.435155	0.805773
-606.622022	10.092849	0.810778
-609.764669	6.577271	0.815782
-613.280092	5.808496	0.820787
-617.431417	9.710486	0.825792
-621.393690	-0.708405	0.830797
-625.784537	13.054249	0.835802
-628.987608	4.917940	0.840806
-632.622001	3.079016	0.845811
-636.427610	7.667698	0.850816
-639.705940	3.433375	0.855821
-643.380063	15.863671	0.860826
-647.525654	0.714894	0.865830
-651.211963	13.995514	0.870835
-655.303904	7.213643	0.875840
-659.089060	-7.238335	0.880845
-662.946821	6.110390	0.885850
-666.246271	2.749649	0.890854
-669.841052	9.130863	0.895859
-674.005744	5.089721	0.900864
-677.570930	1.343176	0.905869
-681.775383	4.230073	0.910874
-685.510634	5.692079	0.915878
-688.986374	-1.107084	0.920883
-692.883248	8.731134	0.925888
-696.213545	3.865953	0.930893
-700.180424	5.482976	0.935898
-703.961419	-0.972495	0.940902
-707.784602	1.428631	0.945907
-711.826315	6.141177	0.950912
-715.259257	0.088189	0.955917
-719.406797	-0.154812	0.960922
-722.715041	0.650170	0.965926
-726.435570	-0.307507	0.970931
-730.505643	3.078177	0.975936
-733.754201	4.056464	0.980941
-737.883736	1.789881	0.985946
-741.622555	2.900861	0.990950
-745.386145	4.348440	0.995955
-749.256564	1.607167	1.000960
-752.626101	5.271297	1.005965
-756.663482	9.207144	1.010970
-760.336218	-4.970364	1.015974
-764.205661	9.195908	1.020979
-768.344299	1.770113	1.025984
-771.866835	-1.358059	1.030989
-775.634323	5.116028	1.035994
-778.837522	9.177519	1.040998
-782.667416	5.525439	1.046003
-786.979201	11.763375	1.051008
-790.463192	-0.699525	1.056013
-794.600231	6.066145	1.061018
-798.015197	5.331591	1.066022
-801.888622	10.908161	1.071027
-805.673822	16.548140	1.076032
-809.114218	15.148928	1.081037
-813.245786	11.137368	1.086042
-816.786960	3.890106	1.091046
-820.666008	9.082027	1.096051
-824.739314	10.961358	1.101056
-828.285712	2.753496	1.106061
-831.983620	10.301921	1.111066
-835.123358	9.114790	1.116070
-839.161862	10.126120	1.121075
-843.337905	3.859367	1.126080
-846.902311	6.643268	1.131085
-850.838896	17.513093	1.136090
-854.424914	6.108606	1.141094
-858.065560	6.190410	1.146099
-862.170029	10.774529	1.151104
-865.783073	5.945783	1.156109
-869.548943	11.908128	1.161114
-873.350045	6.043197	1.166118
-877.133001	7.236469	1.171123
-881.208763	13.020325	1.176128
-884.683870	4.115852	1.181133
-888.538798	15.952537	1.186138
-891.797627	8.156779	1.191142
-895.407557	3.413573	1.196147
-900.032492	6.703618	1.201152
-903.050323	-2.612067	1.206157
-907.220446	14.222442	1.211162
-911.066427	8.515633	1.216166
-914.503613	1.734915	1.221171
-918.556031	6.995755	1.226176
-922.308525	-2.629162	1.231181
-925.764425	11.650964	1.236186
-929.526815	8.345825	1.241190
-933.668699	-0.667146	1.246195
-937.547992	6.476345	1.251200
-940.639495	13.605386	1.256205
-944.543622	14.976216	1.261210
-948.385609	10.584710	1.266214
-952.398089	3.098372	1.271219
-956.384728	12.994445	1.276224
-959.552548	2.808566	1.281229
-963.504454	17.042040	1.286234
-967.229266	10.022605	1.291238
-970.820978	14.887848	1.296243
-975.101788	15.666185	1.301248
-978.433303	8.783306	1.306253
-982.824597	10.675930	1.311258
-986.090159	8.252582	1.316262
-989.878584	12.710722	1.321267
-994.186447	18.282309	1.326272
-997.131685	7.956411	1.331277
-1001.198306	6.586321	1.336282
-1004.808587	-0.380109	1.341286
-1008.459858	8.701380	1.346291
-1012.362389	7.532059	1.351296
-1015.981864	-3.923359	1.356301
-1020.417439	11.800716	1.361306
-1023.897303	4.664684	1.366310
-1027.270887	6.652210	1.371315
-1031.528144	25.226262	1.376320
-1035.088292	13.358062	1.381325
-1039.101986	10.267472	1.386330
-1042.615740	17.505784	1.391334
-1046.074509	12.549270	1.396339
-1050.061104	14.652721	1.401344
-1053.637011	1.799697	1.406349
-1057.134856	16.920340	1.411354
-1061.469957	18.663276	1.416358
-1064.979563	7.921608	1.421363
-1069.049844	13.039609	1.426368
-1072.689105	0.026971	1.431373
-1076.453194	10.414231	1.436378
-1079.856631	12.467708	1.441382
-1084.169853	15.390240	1.446387
-1088.170957	17.317415	1.451392
-1091.003964	4.695262	1.456397
-1095.096960	14.329076	1.461402
-1099.259005	10.648275	1.466406
-1102.758824	11.446576	1.471411
-1106.712347	9.441426	1.476416
-1110.102708	5.997580	1.481421
-1113.979397	10.695568	1.486426
-1117.871757	8.721371	1.491430
-1121.569996	6.510177	1.496435
-1125.078616	12.451846	1.501440
-1128.986673	-1.300046	1.506445
-1132.824673	8.460919	1.511450
-1136.589801	3.729579	1.516454
-1139.977891	3.188828	1.521459
-1144.299488	21.506402	1.526464
-1147.858427	6.100750	1.531469
-1151.871480	7.479025	1.536474
-1155.445405	7.711060	1.541478
-1159.294149	8.595768	1.546483
-1162.989894	13.245360	1.551488
-1166.589831	11.257307	1.556493
-1170.343891	4.294009	1.561498
-1174.209045	11.801164	1.566502
-1177.869013	12.062992	1.571507
-1181.915049	10.446403	1.576512
-1185.650358	9.008151	1.581517
-1189.442804	5.196086	1.586522
-1192.621880	4.869727	1.591526
-1196.647742	7.911955	1.596531
-1200.555866	7.665014	1.601536
-1204.147895	-1.554189	1.606541
-1208.172331	10.569985	1.611546
-1212.136326	4.423902	1.616550
-1215.704299	6.534160	1.621555
-1219.513603	1.648262	1.626560
-1222.890187	3.445811	1.631565
-1226.769187	4.865866	1.636570
-1230.335322	7.217380	1.641574
-1234.132173	-0.435950	1.646579
-1238.355261	7.853854	1.651584
-1241.550246	0.633572	1.656589
-1245.950843	3.090516	1.661594
-1249.580016	8.413954	1.666598
-1253.360400	-2.524952	1.671603
-1257.249287	12.108415	1.676608
-1260.764410	2.090591	1.681613
-1264.128946	9.181869	1.686618
-1268.169584	6.434001	1.691622
-1271.690774	6.282502	1.696627
-1275.537497	4.110763	1.701632
-1279.453998	2.245068	1.706637
-1283.585858	10.158880	1.711642
-1287.096567	6.711776	1.716646
-1290.696052	0.865509	1.721651
-1294.863537	8.189444	1.726656
-1298.628113	-0.948722	1.731661
-1302.197419	5.723841	1.736666
-1305.658549	6.600919	1.741670
-1309.338483	0.565214	1.746675
-1313.760183	8.835915	1.751680
-1317.129360	5.858699	1.756685
-1321.198889	9.141024	1.761690
-1324.760512	5.555077	1.766694
-1328.116186	2.169401	1.771699
-1332.174363	9.645898	1.776704
-1335.786126	7.701469	1.781709
-1339.400612	10.641595	1.786714
-1343.454509	9.833688	1.791718
-1346.966149	2.442506	1.796723
-1350.887478	14.306348	1.801728
-1354.824845	9.298506	1.806733
-1358.878156	4.053237	1.811738
-1362.556281	8.223162	1.816742
-1365.975435	7.821340	1.821747
-1369.560834	14.099254	1.826752
-1373.558880	3.845171	1.831757
-1377.468705	10.369459	1.836762
-1381.182030	6.865668	1.841766
-1384.777307	1.928166	1.846771
-1388.761596	4.758974	1.851776
-1391.826317	11.798450	1.856781
-1395.710320	15.446841	1.861786
-1400.049824	21.869711	1.866790
-1403.799619	6.100031	1.871795
-1407.526464	12.239258	1.876800
-1410.820611	3.996104	1.881805
-1414.482706	1.224012	1.886810
-1418.682713	2.580183	1.891814
-1422.263312	-0.148274	1.896819
-1426.365073	8.942637	1.901824
-1430.558960	1.808851	1.906829
-1433.829348	2.428287	1.911834
-1437.563743	0.723287	1.916838
-1441.192096	3.644171	1.921843
-1444.884798	2.866282	1.926848
-1448.521102	-3.515046	1.931853
-1452.540231	-2.058478	1.936858
-1456.412806	-1.772909	1.941862
-1460.277376	-5.535617	1.946867
-1464.008938	0.506577	1.951872
-1467.609384	4.278013	1.956877
-1471.121098	5.519941	1.961882
-1475.194158	1.575580	1.966886
-1478.900308	2.977617	1.971891
-1482.646119	5.218903	1.976896
-1486.336335	-3.291242	1.981901
-1490.268213	1.704687	1.986906
-1493.672083	8.577512	1.991910
-1497.542680	2.911819	1.996915
-1501.901041	-1.375979	2.006912
-1502.578106	4.182008	2.016909
-1500.053011	5.865360	2.026906
-1496.959920	-0.002525	2.036902
-1495.087046	5.086560	2.046899
-1493.091717	3.665657	2.056896
-1491.050305	4.948374	2.066893
-1489.634549	5.187726	2.076890
-1487.566504	3.382440	2.086886
-1485.361982	0.864464	2.096883
-1483.659000	5.712419	2.106880
-1481.812412	1.261311	2.116877
-1480.124285	2.918522	2.126874
-1478.211433	3.055090	2.136870
-1475.947136	8.412871	2.146867
-1474.238213	5.999010	2.156864
-1472.237754	1.328610	2.166861
-1470.529540	2.274158	2.176858
-1468.389078	2.092216	2.186854
-1466.498007	4.914031	2.196851
-1464.608913	4.723896	2.206848
-1463.006223	3.501274	2.216845
-1461.190039	3.816493	2.226842
-1458.978891	0.706553	2.236838
-1457.157697	2.403357	2.246835
-1455.402664	6.746395	2.256832
-1453.492578	0.068842	2.266829
-1451.123183	-0.323545	2.276826
-1449.880918	-4.141638	2.286822
-1448.166016	2.292633	2.296819
-1445.910680	5.327739	2.306816
-1443.728854	-1.380682	2.316813
-1442.054508	-7.182256	2.326810
-1440.396377	-5.880307	2.336806
-1438.161582	2.360875	2.346803
-1436.400823	1.204774	2.356800
-1434.694485	-0.796027	2.366797
-1432.931463	3.580821	2.376794
-1430.796515	-1.488904	2.386790
-1428.404953	6.063381	2.396787
-1427.140704	1.323048	2.406784
-1425.410001	3.902108	2.416781
-1423.440859	8.471196	2.426778
-1421.236344	10.466159	2.436774
-1419.518853	9.620623	2.446771
-1417.642819	9.054932	2.456768
-1415.733998	9.419468	2.466765
-1413.918513	3.643846	2.476762
-1412.203012	4.977845	2.486758
-1410.339797	7.421515	2.496755
-1408.253166	9.207908	2.506752
-1406.309426	6.456539	2.516749
-1404.176411	11.207740	2.526746
-1402.548540	3.911568	2.536742
-1400.923655	5.934576	2.546739
-1399.043957	8.732690	2.556736
-1397.142432	-0.194489	2.566733
-1394.875680	2.525284	2.576730
-1393.010167	-1.074200	2.586726
-1391.153749	-1.359467	2.596723
-1389.453685	2.413269	2.606720
-1387.790917	5.774676	2.616717
-1386.287693	4.972282	2.626714
-1383.792222	3.065566	2.636710
-1381.642818	2.523677	2.646707
-1380.055077	8.329309	2.656704
-1378.538225	11.167233	2.666701
-1376.073919	3.528999	2.676698
-1374.388090	1.745553	2.686694
-1372.687313	4.704436	2.696691
-1370.725085	7.674532	2.706688
-1368.733373	3.870003	2.716685
-1367.006090	-2.697469	2.726682
-1365.171741	7.359771	2.736678
-1362.790995	0.631050	2.746675
-1361.430980	0.475325	2.756672
-1359.480161	5.664121	2.766669
-1357.480164	-1.891977	2.776666
-1355.772788	-2.618767	2.786662
-1353.791088	7.114785	2.796659
-1351.963538	2.562663	2.806656
-1349.923698	1.281990	2.816653
-1348.442652	4.064817	2.826650
-1346.256545	3.671168	2.836646
-1344.325330	4.153220	2.846643
-1342.320094	0.713926	2.856640
-1340.366667	10.573675	2.866637
-1339.024436	10.597275	2.876634
-1336.854339	4.101167	2.886630
-1335.308728	7.574408	2.896627
-1333.291890	11.547674	2.906624
-1331.281221	5.492736	2.916621
-1329.532375	6.318335	2.926618
-1327.614590	10.582497	2.936614
-1325.262083	7.369695	2.946611
-1323.653805	10.903317	2.956608
-1321.865892	7.082829	2.966605
-1320.031891	9.529979	2.976602
-1317.899028	8.589429	2.986598
-1316.670820	9.467306	2.996595
-1314.919689	12.797761	3.006592
-1312.192797	3.750585	3.016589
-1310.261360	8.009644	3.026586
-1308.751315	1.458951	3.036582
-1306.931970	-1.676099	3.046579
-1305.064512	5.716905	3.056576
-1303.132042	6.947290	3.066573
-1301.169369	8.605244	3.076570
-1299.553322	9.003915	3.086566
-1297.243003	8.572754	3.096563
-1295.666875	11.579560	3.106560
-1293.961609	12.803128	3.116557
-1291.691964	7.907935	3.126554
-1289.834670	9.319202	3.136550
-1288.139560	4.695790	3.146547
-1285.974236	5.819400	3.156544
-1284.323324	7.419062	3.166541
-1282.573762	4.102747	3.176538
-1280.718541	9.130555	3.186534
-1278.610748	10.344277	3.196531
-1276.866933	9.142540	3.206528
-1275.192714	4.857859	3.216525
-1273.088292	6.829783	3.226522
-1270.867289	1.576200	3.236518
-1269.342316	-1.254949	3.246515
-1267.554122	4.951828	3.256512
-1265.594729	6.496937	3.266509
-1263.528413	-0.148883	3.276506
-1261.536811	3.927160	3.286502
-1259.960283	6.214627	3.296499
-1258.072727	3.075785	3.306496
-1256.339103	6.821476	3.316493
-1254.015308	5.684945	3.326490
-1252.394307	10.428128	3.336486
-1250.922227	5.851332	3.346483
-1248.744007	11.428357	3.356480
-1246.759719	9.664839	3.366477
-1245.007880	9.876593	3.376474
-1242.952605	11.117928	3.386470
-1240.734419	8.205677	3.396467
-1239.395184	12.417877	3.406464
-1237.665054	14.752880	3.416461
-1235.399863	12.058224	3.426458
-1233.472364	8.695956	3.436454
-1231.956274	11.890944	3.446451
-1230.167707	9.237833	3.456448
-1227.917593	9.163255	3.466445
-1226.126649	13.165095	3.476442
-1224.249326	15.613150	3.486438
-1222.535122	10.794012	3.496435
-1220.575612	13.297511	3.506432
-1218.431869	8.987546	3.516429
-1216.878409	14.053376	3.526426
-1214.906970	12.281014	3.536422
-1212.942968	8.117320	3.546419
-1211.090073	0.671511	3.556416
-1208.998945	7.793771	3.566413
-1207.627775	6.055730	3.576410
-1205.580013	4.741752	3.586406
-1203.722371	9.657733	3.596403
-1201.472422	5.925517	3.606400
-1199.983319	11.601941	3.616397
-1197.937417	7.836790	3.626394
-1196.208618	11.260451	3.636390
-1194.226420	10.126098	3.646387
-1192.404606	11.551407	3.656384
-1190.450175	7.328504	3.666381
-1188.471666	9.340274	3.676378
-1186.776951	3.399331	3.686374
-1184.907679	3.122222	3.696371
-1182.815255	10.381020	3.706368
-1181.113450	12.262070	3.716365
-1179.480195	6.862452	3.726362
-1177.524318	5.776890	3.736358
-1175.301301	3.893763	3.746355
-1173.642004	5.950870	3.756352
-1171.919728	8.178566	3.766349
-1169.999121	8.424999	3.776346
-1167.888893	8.111658	3.786342
-1166.129503	7.080393	3.796339
-1164.126055	9.024264	3.806336
-1162.021255	18.641946	3.816333
-1160.551288	9.255416	3.826330
-1158.766394	13.348040	3.836326
-1156.615141	14.811646	3.846323
-1154.906176	12.946057	3.856320
-1153.101213	10.937123	3.866317
-1151.077210	9.377872	3.876314
-1148.985920	8.814462	3.886310
-1147.249936	10.737873	3.896307
-1145.524749	14.391005	3.906304
-1143.598829	13.109440	3.916301
-1141.940181	12.494252	3.926298
-1139.690537	14.010528	3.936294
-1137.706525	10.525960	3.946291
-1136.125625	12.774787	3.956288
-1134.253676	9.315392	3.966285
-1132.220473	6.914350	3.976282
-1130.285263	6.450074	3.986278
-1128.621329	10.456379	3.996275
-1126.830527	5.805525	4.006272
-1124.950439	14.391975	4.016269
-1122.987960	10.342401	4.026266
-1120.548425	5.276633	4.036262
-1119.362919	6.182848	4.046259
-1117.366438	13.173607	4.056256
-1115.529374	8.083242	4.066253
-1113.484134	11.375933	4.076250
-1111.779034	5.849389	4.086246
-1109.696437	8.698563	4.096243
-1107.959052	7.215816	4.106240
-1106.002366	7.470705	4.116237
-1104.327060	12.147324	4.126234
-1102.124147	7.806306	4.136230
-1100.339296	5.915853	4.146227
-1098.600727	5.974628	4.156224
-1096.781509	8.481329	4.166221
-1094.690025	9.627203	4.176218
-1092.941137	5.935229	4.186214
-1090.851160	6.252210	4.196211
-1089.386478	9.020557	4.206208
-1087.268803	11.422269	4.216205
-1085.197744	9.913855	4.226202
-1083.271811	7.769962	4.236198
-1081.565055	6.901901	4.246195
-1079.841498	3.232856	4.256192
-1078.061557	3.091672	4.266189
-1076.256454	-1.358872	4.276186
-1074.039427	-0.061046	4.286182
-1072.237133	-1.145484	4.296179
-1070.147349	2.093340	4.306176
-1068.541896	3.508427	4.316173
-1066.763852	4.194751	4.326170
-1064.689243	-3.259827	4.336166
-1062.837633	2.695873	4.346163
-1061.284948	1.926202	4.356160
-1058.976147	3.147416	4.366157
-1057.282842	1.681743	4.376154
-1055.361713	-1.933476	4.386150
-1053.361185	-1.807025	4.396147
-1051.838297	-1.287929	4.406144
-1050.106702	1.189573	4.416141
-1047.626436	4.585847	4.426138
-1045.789028	1.107125	4.436134
-1044.242905	1.916273	4.446131
-1042.367595	0.366003	4.456128
-1040.048864	5.115556	4.466125
-1038.539065	5.250783	4.476122
-1036.517093	3.482866	4.486118
-1034.964254	10.507945	4.496115
-1032.867885	6.717603	4.506112
-1030.704505	4.736500	4.516109
-1029.062126	8.814130	4.526106
-1027.279951	10.261731	4.536102
-1025.499382	-6.232618	4.546099
-1023.624505	5.630290	4.556096
-1021.655689	5.923843	4.566093
-1019.749667	3.505562	4.576090
-1017.664739	-0.514402	4.586086
-1015.965563	-1.623400	4.596083
-1014.090830	3.287761	4.606080
-1012.349736	3.133909	4.616077
-1010.658094	10.013837	4.626074
-1008.264755	4.118605	4.636070
-1006.446200	9.140591	4.646067
-1004.538751	8.652682	4.656064
-1003.193028	11.062477	4.666061
-1000.749529	9.371597	4.676058
-999.166819	4.495282	4.686054
-997.221562	6.165462	4.696051
-995.349835	6.069417	4.706048
-993.575784	9.854527	4.716045
-991.557368	6.654202	4.726042
-989.537145	7.769285	4.736038
-987.489514	13.638415	4.746035
-986.198504	9.859494	4.756032
-984.269979	16.062478	4.766029
-982.112049	11.822904	4.776026
-980.000389	4.377804	4.786022
-978.474817	7.916283	4.796019
-976.615026	10.917994	4.806016
-974.813752	5.973337	4.816013
-972.877938	8.989267	4.826010
-970.906957	8.194452	4.836006
-969.104037	4.996748	4.846003
-966.969487	14.152967	4.856000
-965.444098	14.323484	4.865997
-963.189945	9.153273	4.875994
-961.437708	10.151549	4.885990
-959.664534	16.454330	4.895987
-958.241696	10.070465	4.905984
-956.001988	10.984663	4.915981
-953.878707	3.341949	4.925978
-952.050524	4.253681	4.935974
-950.268676	6.499700	4.945971
-948.252990	1.536821	4.955968
-946.720272	9.047155	4.965965
-944.905766	9.747824	4.975962
-943.022016	10.514462	4.985958
-940.693755	12.190849	4.995955
-939.088215	10.278678	5.005952
-936.855325	12.027560	5.015949
-935.377399	8.286912	5.025946
-933.529451	10.506574	5.035942
-931.510015	7.826595	5.045939
-929.505482	12.771244	5.055936
-927.831047	7.450003	5.065933
-925.970780	9.635541	5.075930
-923.893412	8.968318	5.085926
-922.110889	14.161336	5.095923
-920.424203	14.957071	5.105920
-918.523029	11.121640	5.115917
-916.594409	9.446079	5.125914
-914.404585	11.816920	5.135910
-912.499101	4.109646	5.145907
-911.178219	12.108090	5.155904
-908.932483	8.044364	5.165901
-907.328373	10.040313	5.175898
-905.140898	10.093640	5.185894
-903.239106	9.416255	5.195891
-901.431034	5.590885	5.205888
-899.178297	9.944783	5.215885
-897.561987	9.553928	5.225882
-895.845210	10.126745	5.235878
-894.198368	4.688527	5.245875
-892.020134	10.070914	5.255872
-890.651763	6.356200	5.265869
-888.476366	3.662906	5.275866
-886.640551	4.314491	5.285862
-884.556182	10.062758	5.295859
-882.393508	10.491460	5.305856
-881.135579	5.737722	5.315853
-879.079959	10.151946	5.325850
-877.083761	6.666188	5.335846
-875.097813	3.108287	5.345843
-873.341540	7.062492	5.355840
-871.299480	1.531544	5.365837
-869.756999	5.860750	5.375834
-867.778878	-1.661368	5.385830
-866.205002	4.618753	5.395827
-864.024696	2.311936	5.405824
-861.803908	5.736660	5.415821
-860.522762	-2.043248	5.425818
-858.177911	1.145976	5.435814
-856.254337	-1.079619	5.445811
-854.653656	1.457984	5.455808
-852.708518	1.410658	5.465805
-850.948690	8.316502	5.475802
-848.731788	7.678718	5.485798
-846.987827	2.301307	5.495795
-845.451297	4.180830	5.505792
-843.154739	11.279896	5.515789
-841.711646	9.550566	5.525786
-839.562040	10.834797	5.535782
-837.675100	9.857651	5.545779
-835.868088	10.949727	5.555776
-834.055401	12.413517	5.565773
-832.043084	10.859579	5.575770
-829.424650	2.354938	5.585766
-828.334599	6.766560	5.595763
-826.755615	10.342567	5.605760
-824.620538	9.352081	5.615757
-822.524302	12.664625	5.625754
-820.635355	11.173760	5.635750
-819.159793	5.237355	5.645747
-817.362267	4.726898	5.655744
-815.455594	6.156778	5.665741
-813.290760	4.676265	5.675738
-811.151512	7.204442	5.685734
-809.617341	2.305295	5.695731
-807.715213	0.220935	5.705728
-805.679441	1.603763	5.715725
-804.042979	2.704574	5.725722
-802.262537	2.465405	5.735718
-799.925918	3.727042	5.745715
-798.351740	4.458351	5.755712
-796.503513	9.844079	5.765709
-794.502366	7.382295	5.775706
-792.618636	7.891325	5.785702
-790.854065	6.977489	5.795699
-788.949034	4.012104	5.805696
-787.213998	4.801964	5.815693
-785.137973	5.284712	5.825690
-783.280666	7.032532	5.835686
-781.426872	7.429722	5.845683
-779.336153	5.236334	5.855680
-777.695662	8.289213	5.865677
-775.759323	7.609905	5.875674
-774.000065	8.949308	5.885670
-772.001817	2.348568	5.895667
-769.943408	5.539976	5.905664
-768.309983	8.581424	5.915661
-766.425969	4.317427	5.925658
-764.400731	5.819462	5.935654
-762.618653	8.213334	5.945651
-760.865581	5.722607	5.955648
-759.300335	10.006850	5.965645
-756.923703	7.762821	5.975642
-754.975346	2.013246	5.985638
-753.413561	6.835178	5.995635
-751.374540	2.064006	6.005632
-749.702978	6.680954	6.015629
-747.794866	5.826681	6.025626
-745.439415	7.817447	6.035622
-743.785290	5.089191	6.045619
-742.009366	3.406317	6.055616
-740.139956	9.583211	6.065613
-738.271818	5.260691	6.075610
-736.310847	6.280147	6.085606
-734.510298	6.693214	6.095603
-732.781327	6.032520	6.105600
-730.671634	6.355778	6.115597
-729.057530	8.590371	6.125594
-727.012487	9.200190	6.135590
-724.880816	5.401160	6.145587
-723.003284	5.311351	6.155584
-721.260683	6.539417	6.165581
-719.491730	3.642863	6.175578
-717.766894	11.398164	6.185574
-715.815503	6.852692	6.195571
-713.762006	0.327860	6.205568
-711.943632	4.129598	6.215565
-710.099191	8.078231	6.225562
-708.422150	6.298518	6.235558
-706.553532	0.506921	6.245555
-704.254823	4.694954	6.255552
-702.203300	6.167214	6.265549
-700.671087	3.831000	6.275546
-698.930630	1.631362	6.285542
-697.123194	4.040276	6.295539
-695.224860	6.449400	6.305536
-693.332154	1.124769	6.315533
-691.411980	2.136624	6.325530
-689.191575	5.153648	6.335526
-687.638110	0.830215	6.345523
-685.686154	3.626935	6.355520
-683.772544	3.854236	6.365517
-682.133236	8.205633	6.375514
-680.222989	8.477381	6.385510
-678.316654	8.638746	6.395507
-676.241519	0.699304	6.405504
-674.297592	2.124040	6.415501
-672.685654	3.033085	6.425498
-670.805943	2.444955	6.435494
-668.451742	3.498532	6.445491
-667.296219	4.247983	6.455488
-664.626267	8.186186	6.465485
-663.180221	10.069449	6.475482
-661.431310	-0.514896	6.485478
-659.643819	7.801948	6.495475
-657.300800	6.544264	6.505472
-655.569529	5.203042	6.515469
-654.011921	2.742341	6.525466
-652.276496	3.467375	6.535462
-649.984082	-0.531517	6.545459
-647.901696	-1.671751	6.555456
-646.420770	-4.802219	6.565453
-644.367890	-0.157391	6.575450
-642.549099	4.793588	6.585446
-640.564887	-3.733332	6.595443
-638.823031	3.437722	6.605440
-637.191024	-2.533380	6.615437
-635.017036	-3.522942	6.625434
-633.175447	-4.835264	6.635430
-631.113607	-4.571723	6.645427
-629.102551	-4.029141	6.655424
-627.742945	-6.223866	6.665421
-625.714675	-8.372083	6.675418
-623.663000	-4.393763	6.685414
-621.818955	-4.125253	6.695411
-620.209268	-4.154830	6.705408
-618.348065	-6.174783	6.715405
-616.479580	-1.615677	6.725402
-614.390965	-2.934811	6.735398
-612.394910	-2.693171	6.745395
-610.549130	-4.546065	6.755392
-608.893786	2.164406	6.765389
-606.865366	-4.020146	6.775386
-604.967338	-1.197931	6.785382
-603.180724	1.371101	6.795379
-601.266897	-1.460949	6.805376
-599.714504	0.268528	6.815373
-597.555929	-2.205165	6.825370
-595.730607	3.209486	6.835366
-593.404793	0.280267	6.845363
-592.039134	-2.977030	6.855360
-589.899277	-3.155269	6.865357
-588.033108	1.237073	6.875354
-586.462318	-2.665236	6.885350
-584.354339	-6.224983	6.895347
-582.444196	-0.913409	6.905344
-580.687621	0.537589	6.915341
-578.696355	2.565643	6.925338
-576.873380	7.692992	6.935334
-575.153681	7.556422	6.945331
-573.242435	5.282077	6.955328
-571.182829	4.608187	6.965325
-569.257301	2.823040	6.975322
-567.407712	-0.567873	6.985318
-565.844289	0.588640	6.995315
-563.611127	1.822709	7.005312
-561.875734	4.011657	7.015309
-560.083541	2.337919	7.025306
-557.886441	3.012232	7.035302
-556.213261	5.229247	7.045299
-554.560956	9.043348	7.055296
-552.322268	2.772149	7.065293
-550.661934	0.553907	7.075290
-548.804645	0.834009	7.085286
-546.724826	-0.593849	7.095283
-545.322906	0.935799	7.105280
-542.938822	6.383050	7.115277
-541.173708	4.793008	7.125274
-539.361304	0.011799	7.135270
-537.835875	-1.308683	7.145267
-535.321618	5.331521	7.155264
-533.612344	2.765399	7.165261
-531.651671	3.703586	7.175258
-530.170965	-1.061811	7.185254
-527.856993	2.209968	7.195251
-526.260392	-2.855124	7.205248
-524.363001	-0.246968	7.215245
-522.532005	5.770633	7.225242
-520.660211	3.412179	7.235238
-518.862142	0.854540	7.245235
-516.724918	4.475193	7.255232
-514.930983	3.448535	7.265229
-513.116653	4.809029	7.275226
-511.117947	6.051338	7.285222
-509.392235	3.258713	7.295219
-507.440178	0.407099	7.305216
-505.501408	3.328684	7.315213
-503.741659	3.103857	7.325210
-501.846076	5.316329	7.335206
-499.942826	6.499535	7.345203
-497.729000	4.449168	7.355200
-496.230953	1.687308	7.365197
-494.469447	5.983830	7.375194
-492.469225	2.384908	7.385190
-490.840174	-0.162693	7.395187
-488.774204	-1.596053	7.405184
-486.555843	1.219871	7.415181
-485.078577	1.624481	7.425178
-482.904539	0.656325	7.435174
-480.987079	-1.454244	7.445171
-479.351079	5.150527	7.455168
-476.998891	6.597792	7.465165
-475.446818	1.588570	7.475162
-473.810764	-4.282001	7.485158
-471.692621	-3.516242	7.495155
-469.905047	-12.096309	7.505152
-468.003008	-8.852632	7.515149
-466.407280	-5.980467	7.525146
-464.320228	-9.472941	7.535142
-462.657868	-7.372203	7.545139
-460.271861	-9.466319	7.555136
-458.587585	-6.917609	7.565133
-457.035734	-3.335617	7.575130
-454.870287	-0.339471	7.585126
-453.183142	-3.657022	7.595123
-451.185496	-6.133075	7.605120
-449.224928	-4.545496	7.615117
-447.446122	-7.801702	7.625114
-445.283577	-3.420618	7.635110
-443.806370	1.778756	7.645107
-441.665154	-3.049341	7.655104
-439.631468	-0.411965	7.665101
-438.461499	-5.733842	7.675098
-436.341452	-9.420877	7.685094
-434.287787	-8.481606	7.695091
-432.146705	-6.204907	7.705088
-430.580485	2.211661	7.715085
-428.698412	4.699183	7.725082
-426.706875	4.555953	7.735078
-424.913422	-1.014369	7.745075
-422.847171	3.785181	7.755072
-420.915821	0.221026	7.765069
-419.368450	6.314207	7.775066
-417.374383	0.584189	7.785062
-415.430240	0.609947	7.795059
-413.313675	-4.405588	7.805056
-412.043582	1.731998	7.815053
-410.206246	5.751151	7.825050
-408.003339	4.102656	7.835046
-405.634641	3.797908	7.845043
-404.137843	-4.479719	7.855040
-402.482977	6.352621	7.865037
-400.425756	6.045187	7.875034
-398.705801	2.483711	7.885030
-397.101653	2.868955	7.895027
-394.732158	0.308586	7.905024
-393.021859	4.101738	7.915021
-391.121378	4.934912	7.925018
-389.136153	6.703250	7.935014
-387.330753	6.035506	7.945011
-385.321070	10.182007	7.955008
-383.883525	4.254217	7.965005
-381.885012	8.101876	7.975002
-379.645760	4.433936	7.984998
-377.886810	-1.239926	7.994995
-375.927656	2.174612	8.004992
-374.267338	7.884445	8.014989
-372.293207	0.834684	8.024986
-370.563382	8.195263	8.034982
-368.624605	1.639658	8.044979
-366.596593	4.438502	8.054976
-364.884616	0.198636	8.064973
-362.741210	2.683647	8.074970
-361.504300	3.175373	8.084966
-359.160623	-3.211763	8.094963
-357.156241	-0.131817	8.104960
-355.814225	5.711271	8.114957
-353.661212	6.458459	8.124954
-351.672908	8.227078	8.134950
-350.066969	7.054094	8.144947
-348.111940	7.281550	8.154944
-345.824144	8.048306	8.164941
-344.142944	5.616302	8.174938
-342.253068	6.698326	8.184934
-340.371599	5.663044	8.194931
-338.565887	7.550331	8.204928
-337.006088	8.920177	8.214925
-334.728105	4.452022	8.224922
-332.674065	4.926505	8.234918
-330.841611	4.358479	8.244915
-329.388547	7.149254	8.254912
-327.497622	12.014104	8.264909
-325.477220	6.755836	8.274906
-323.133363	-0.592478	8.284902
-321.779309	-0.574147	8.294899
-319.883064	-3.642964	8.304896
-317.588814	2.649386	8.314893
-316.109319	2.548189	8.324890
-314.251215	-0.750027	8.334886
-312.070356	-0.571172	8.344883
-310.581177	2.978945	8.354880
-308.914588	3.840021	8.364877
-306.963249	3.808867	8.374874
-304.420034	1.875593	8.384870
-303.024891	-4.897379	8.394867
-301.261139	0.803041	8.404864
-299.095880	2.615236	8.414861
-297.225856	-2.932211	8.424858
-295.395289	-5.186281	8.434854
-293.570232	-5.628925	8.444851
-291.694514	-7.222033	8.454848
-289.489139	-1.958583	8.464845
-288.096530	-1.025213	8.474842
-286.160948	2.202917	8.484838
-284.211406	4.490809	8.494835
-282.204290	0.763136	8.504832
-280.377940	-1.263351	8.514829
-278.512308	4.318431	8.524826
-276.510199	0.592014	8.534822
-274.782173	0.469545	8.544819
-273.039605	0.757583	8.554816
-271.160856	3.720794	8.564813
-269.336623	-0.362422	8.574810
-267.122590	2.150835	8.584807
-265.232122	1.548778	8.594803
-263.216546	-4.247708	8.604800
-261.676127	3.508213	8.614797
-260.035461	-1.272687	8.624794
-257.773225	-1.944037	8.634791
-255.739844	0.487573	8.644787
-254.115629	-8.429986	8.654784
-252.490685	-5.295188	8.664781
-250.367390	-3.826327	8.674778
-248.258368	-4.716033	8.684775
-246.313706	-8.152376	8.694771
-244.694536	-7.849882	8.704768
-242.683611	-6.234091	8.714765
-241.088522	-8.792775	8.724762
-239.214136	-4.451083	8.734759
-237.187123	-6.932083	8.744755
-235.178720	-3.282473	8.754752
-233.662985	2.375543	8.764749
-231.595771	-0.209178	8.774746
-229.903393	1.670323	8.784743
-227.929998	8.354874	8.794739
-225.818394	-3.556243	8.804736
-224.048365	-1.348988	8.814733
-222.224417	-1.035761	8.824730
-220.537294	-7.392829	8.834727
-218.821321	-5.536738	8.844723
-216.611969	-2.787500	8.854720
-214.538569	-1.616751	8.864717
-212.979418	-10.200249	8.874714
-211.012230	-6.950236	8.884711
-209.114497	-13.132770	8.894707
-207.012428	-9.446253	8.904704
-205.356111	-7.188267	8.914701
-203.500293	-3.596259	8.924698
-201.805427	-2.983445	8.934695
-199.652729	-10.666071	8.944691
-197.822527	-11.585003	8.954688
-195.732875	-8.099096	8.964685
-194.028755	-9.053710	8.974682
-192.570942	-7.844170	8.984679
-190.556643	-6.566053	8.994675
-188.285689	-2.712461	9.004672
-186.505035	-2.235685	9.014669
-184.720413	-1.975377	9.024666
-183.056653	-2.816752	9.034663
-181.092699	-6.963418	9.044659
-178.941790	-12.342018	9.054656
-177.002394	-9.812048	9.064653
-175.389826	-6.683002	9.074650
-173.598190	-5.016134	9.084647
-171.270298	-14.345619	9.094643
-169.797135	-7.578420	9.104640
-167.862380	-5.710426	9.114637
-166.037155	-6.264894	9.124634
-164.372536	-3.486630	9.134631
-162.298875	-6.079540	9.144627
-160.426680	-1.755615	9.154624
-158.392685	-6.991641	9.164621
-156.562785	-7.426762	9.174618
-154.745593	-8.608635	9.184615
-152.442878	-3.601699	9.194611
-150.784155	-6.752630	9.204608
-149.170060	-4.602388	9.214605
-147.303706	-1.466659	9.224602
-145.187076	1.342387	9.234599
-143.397631	0.235229	9.244595
-141.759263	-0.148465	9.254592
-139.517719	1.969272	9.264589
-137.606868	0.667402	9.274586
-136.104789	2.845158	9.284583
-133.984750	-0.262360	9.294579
-132.523126	4.279797	9.304576
-130.257051	-1.418504	9.314573
-128.302215	0.191151	9.324570
-126.584299	8.838338	9.334567
-124.719352	5.182929	9.344563
-122.763220	4.442015	9.354560
-120.859819	11.826302	9.364557
-119.022094	5.431181	9.374554
-117.231779	4.702501	9.384551
-115.350134	2.988300	9.394547
-113.240475	5.255136	9.404544
-111.559895	4.983965	9.414541
-110.070012	2.744517	9.424538
-107.972199	-0.824348	9.434535
-105.858551	7.076797	9.444531
-103.966605	1.004368	9.454528
-102.008267	2.088587	9.464525
-100.293570	6.236014	9.474522
-98.297940	1.535781	9.484519
-96.399553	5.386916	9.494515
-94.601243	1.557588	9.504512
-92.611262	2.311123	9.514509
-90.711589	-1.142344	9.524506
-89.142058	5.102888	9.534503
-87.332325	1.073601	9.544499
-85.327865	-3.470843	9.554496
-83.654120	8.308516	9.564493
-81.570624	-0.173977	9.574490
-79.505896	1.542140	9.584487
-77.895373	1.303941	9.594483
-75.953952	-0.388482	9.604480
-74.157062	-3.024796	9.614477
-72.014716	4.834296	9.624474
-70.324001	-0.724218	9.634471
-68.223389	-2.508750	9.644467
-66.644111	3.227361	9.654464
-64.641710	5.213830	9.664461
-62.708921	4.161166	9.674458
-60.986199	-2.135169	9.684455
-59.035860	1.870297	9.694451
-57.164961	3.452484	9.704448
-55.096365	-0.569404	9.714445
-53.598214	6.088831	9.724442
-51.651649	1.507690	9.734439
-49.554771	4.923271	9.744435
-47.567017	1.662206	9.754432
-46.093393	-2.203120	9.764429
-44.005541	-3.128625	9.774426
-42.091138	-4.355579	9.784423
-40.266356	5.962477	9.794419
-38.319065	2.434469	9.804416
-36.323155	2.887438	9.814413
-34.332004	-0.799062	9.824410
-32.831324	2.140948	9.834407
-31.105815	2.818921	9.844403
-29.020872	2.727433	9.854400
-26.970193	-3.144541	9.864397
-25.208827	-6.992406	9.874394
-23.453960	-3.531213	9.884391
-21.210101	-1.300781	9.894387
-19.795476	-5.561870	9.904384
-17.670663	0.218257	9.914381
-15.847271	-2.680260	9.924378
-13.814463	-0.804506	9.934375
-12.082551	-2.161801	9.944371
-10.400179	-3.972215	9.954368
-8.296861	-1.374631	9.964365
-6.454421	-3.152810	9.974362
-5.007641	15.582981	9.984359
-3.972161	41.782253	9.994355
-2.426944	83.662986	10.004352
-1.241009	148.977156	10.014349
0.000000	210.887852	10.019354
0.965932	250.343923	10.024359
1.256524	290.080485	10.029363
1.878644	312.398584	10.034368
2.265052	337.516219	10.039373
2.578103	358.447440	10.044378
2.755569	368.392787	10.049383
3.101907	392.714126	10.054387
3.455776	399.697656	10.059392
3.693535	401.591035	10.064397
3.566059	415.585250	10.069402
3.480295	410.271226	10.074407
3.568919	424.912055	10.079411
3.860121	439.702498	10.084416
4.042824	445.400972	10.089421
4.053729	453.648416	10.094426
4.148163	459.166641	10.099431
3.688688	466.298733	10.104435
3.650707	472.045316	10.109440
3.969594	472.443005	10.114445
3.613354	469.412626	10.119450
3.896699	466.954668	10.124455
4.452945	484.490402	10.129459
4.447075	502.458049	10.134464
4.522533	499.723503	10.139469
4.465371	505.537333	10.144474
4.426772	502.287886	10.149479
4.250311	506.719323	10.154483
4.422719	510.554910	10.159488
4.701484	507.188287	10.164493
4.290318	511.767332	10.169498
4.722822	509.983244	10.174503
4.903502	516.024316	10.179507
4.698553	519.565801	10.184512
4.982622	518.896601	10.189517
5.065551	525.347187	10.194522
5.170424	520.016229	10.199527
4.698954	521.767945	10.204531
4.841776	527.339869	10.209536
5.333814	525.544783	10.214541
4.829671	536.593125	10.219546
4.878079	539.281990	10.224551
5.177679	532.862542	10.229555
4.771771	540.045085	10.234560
5.281966	551.267276	10.239565
5.458900	566.989642	10.244570
5.409556	557.272874	10.249575
5.571219	572.104995	10.254579
5.406495	570.124887	10.259584
5.576250	568.850829	10.264589
5.146541	578.774497	10.269594
5.647025	576.677965	10.274599
5.442267	577.527008	10.279603
5.380526	579.704254	10.284608
5.841689	579.357968	10.289613
5.522384	588.762200	10.294618
5.497192	584.742301	10.299623
5.662066	587.660673	10.304627
5.434427	594.021645	10.309632
5.987661	597.385391	10.314637
5.994352	612.180571	10.319642
6.253778	611.206916	10.324647
6.253559	615.003839	10.329651
6.178916	620.231777	10.334656
6.116699	616.081642	10.339661
6.049196	620.422984	10.344666
6.297851	616.866506	10.349671
6.419712	624.081753	10.354675
6.254249	627.065454	10.359680
6.706694	622.629713	10.364685
6.286256	624.909912	10.369690
6.308770	621.496019	10.374695
6.743797	625.030430	10.379699
6.461030	629.692491	10.384704
6.649202	627.268194	10.389709
6.615456	637.970304	10.394714
6.587610	637.011956	10.399719
6.845187	635.316266	10.404723
6.337090	643.378856	10.409728
7.180125	638.259183	10.414733
6.966499	643.248069	10.419738
6.675366	638.960340	10.424743
6.765902	640.294006	10.429747
6.466090	643.389164	10.434752
6.560793	636.327847	10.439757
6.643995	657.583477	10.444762
7.325101	673.060037	10.449767
7.346341	673.980071	10.454771
7.121305	690.811195	10.459776
7.478874	681.149317	10.464781
7.175069	689.651762	10.469786
7.295455	688.530629	10.474791
7.204555	695.161086	10.479795
7.057624	692.011094	10.484800
7.628662	688.111568	10.489805
7.368636	692.436992	10.494810
7.326703	686.549319	10.499815
7.570086	693.706659	10.504819
7.695789	690.137298	10.509824
7.643293	688.238983	10.514829
7.543739	685.073763	10.519834
7.458612	684.396411	10.524839
7.997276	699.114279	10.529843
7.921077	707.498369	10.534848
8.163842	704.700365	10.539853
8.135402	708.004397	10.544858
8.000705	698.972030	10.549863
8.164470	705.656720	10.554867
8.021880	709.384921	10.559872
8.008864	700.052617	10.564877
8.134145	713.462193	10.569882
8.270201	717.436299	10.574887
8.107019	729.936156	10.579891
8.154316	724.856574	10.584896
8.263980	724.123323	10.589901
8.001408	727.338820	10.594906
8.203086	726.239668	10.599911
8.140574	730.547027	10.604915
8.150839	731.596049	10.609920
8.517230	733.721621	10.614925
8.449665	749.207808	10.619930
8.473817	747.318053	10.624935
8.801571	756.241977	10.629939
8.777609	755.003487	10.634944
8.933604	755.360825	10.639949
8.907799	761.719627	10.644954
9.387607	750.919661	10.649959
9.292084	749.333052	10.654963
9.160476	744.911364	10.659968
8.969940	724.204163	10.664973
8.944397	731.608546	10.669978
8.967142	727.045533	10.674983
8.904806	738.934433	10.679987
9.463972	759.921100	10.684992
9.135400	752.919277	10.689997
8.913915	765.327318	10.695002
9.279674	765.049096	10.700007
9.324226	762.206516	10.705011
9.268059	768.113429	10.710016
9.482015	762.350403	10.715021
9.260822	768.067720	10.720026
9.612422	771.621995	10.725031
9.384025	766.948479	10.730035
9.678679	771.559737	10.735040
9.890779	766.526885	10.740045
9.550597	774.070892	10.745050
9.663544	766.923100	10.750055
9.724977	767.179021	10.755059
9.412423	777.077201	10.760064
9.994605	788.184197	10.765069
9.969016	801.585769	10.770074
10.204163	797.199078	10.775079
10.104281	787.478990	10.780083
10.024662	791.431278	10.785088
10.631010	789.795772	10.790093
9.714661	785.386254	10.795098
9.744108	793.576226	10.800103
10.318522	804.281150	10.805107
10.053884	803.893909	10.810112
10.399710	805.145530	10.815117
10.483951	803.845064	10.820122
10.346980	808.668493	10.825127
10.678042	814.668503	10.830131
10.403658	809.984307	10.835136
10.698517	809.481796	10.840141
10.848978	818.064711	10.845146
10.656322	812.902297	10.850151
10.352596	811.504140	10.855155
10.421659	813.817279	10.860160
10.763336	813.185953	10.865165
10.447978	820.601385	10.870170
11.039596	813.252688	10.875175
11.039057	820.419145	10.880179
10.819436	819.265906	10.885184
11.214848	810.268898	10.890189
11.175481	824.681787	10.895194
11.124041	823.104980	10.900199
11.198322	816.550367	10.905203
11.051326	817.339387	10.910208
11.170535	817.845927	10.915213
11.250977	822.943133	10.920218
11.301887	823.764536	10.925223
10.739193	828.022288	10.930227
10.862754	847.086415	10.935232
11.410792	847.297197	10.940237
11.272989	852.098283	10.945242
11.493781	858.730236	10.950247
11.264485	863.904245	10.955251
11.402097	856.233110	10.960256
11.723014	853.096421	10.965261
11.579952	854.330817	10.970266
11.842020	846.484797	10.975271
11.891092	847.848485	10.980275
11.736255	848.981479	10.985280
12.418648	844.437173	10.990285
11.664975	857.861786	10.995290
12.321379	854.405473	11.000295
12.101045	850.326596	11.005299
12.013579	854.152352	11.010304
12.095251	847.294094	11.015309
12.345276	854.650499	11.020314
12.358362	844.057594	11.025319
12.626314	858.214930	11.030323
12.128981	859.233359	11.035328
12.551457	850.887340	11.040333
12.059893	851.015053	11.045338
12.059262	848.068494	11.050343
12.197851	852.533247	11.055347
12.095456	852.065294	11.060352
12.544790	861.018565	11.065357
12.064455	873.608045	11.070362
12.647453	873.560993	11.075367
13.351983	876.492681	11.080371
13.088404	884.265578	11.085376
13.139418	857.857097	11.090381
12.978709	860.356874	11.095386
12.723833	862.153988	11.100391
12.853380	855.808960	11.105395
12.969610	860.350179	11.110400
13.100158	858.897691	11.115405
12.966400	854.524893	11.120410
13.095634	849.776219	11.125415
12.672987	859.864246	11.130419
12.467045	877.070451	11.135424
12.923082	879.233569	11.140429
12.955512	885.949539	11.145434
12.997017	891.730806	11.150439
13.281591	899.127887	11.155443
13.325704	889.583966	11.160448
13.404621	897.473803	11.165453
13.178733	891.393778	11.170458
13.285460	891.431148	11.175463
13.489169	902.803247	11.180467
13.381892	916.459317	11.185472
13.676384	920.845649	11.190477
13.942652	924.743009	11.195482
13.465214	931.496682	11.200487
13.861877	921.254404	11.205491
13.835125	922.160970	11.210496
13.823903	918.599244	11.215501
13.388042	928.040638	11.220506
13.505070	925.926518	11.225511
13.717392	925.850652	11.230515
14.040322	928.002257	11.235520
14.268025	922.887338	11.240525
13.879221	927.350563	11.245530
13.802660	920.900321	11.250535
13.650968	923.192905	11.255539
14.002992	940.856932	11.260544
14.654962	936.123607	11.265549
14.847678	946.052104	11.270554
14.602826	938.744528	11.275559
14.578035	923.701904	11.280563
14.292482	928.079927	11.285568
14.697707	930.661103	11.290573
14.334508	925.645522	11.295578
14.498754	933.212065	11.300583
14.761465	933.208876	11.305587
14.441591	950.339170	11.310592
15.172400	942.300630	11.315597
15.081453	947.392920	11.320602
15.067895	940.803974	11.325607
14.713569	923.943253	11.330611
14.823548	926.905443	11.335616
15.150196	935.922029	11.340621
14.955403	935.271363	11.345626
14.842580	928.812729	11.350631
14.824868	943.094120	11.355635
15.077376	948.137787	11.360640
14.960685	947.540046	11.365645
15.126608	954.650393	11.370650
15.216162	955.236231	11.375655
15.061746	952.042469	11.380659
15.329122	956.026094	11.385664
15.252540	949.125056	11.390669
15.110379	944.664463	11.395674
14.897460	947.446362	11.400679
15.177411	963.136466	11.405683
15.452523	978.468205	11.410688
15.806136	970.661296	11.415693
16.009659	978.955730	11.420698
16.000497	972.112991	11.425703
16.074863	953.257954	11.430707
15.651023	957.934431	11.435712
15.973442	946.606318	11.440717
15.961374	942.885259	11.445722
15.928577	947.502187	11.450727
15.970882	940.698400	11.455731
15.717994	942.840970	11.460736
15.881610	949.602370	11.465741
16.158730	965.418487	11.470746
16.129799	974.911718	11.475751
16.261872	973.073695	11.480755
15.867055	972.223639	11.485760
16.228200	978.798817	11.490765
16.271099	989.196711	11.495770
16.240601	977.353955	11.500775
16.225999	977.472522	11.505779
16.157259	983.360751	11.510784
16.417483	984.085092	11.515789
16.012860	987.038418	11.520794
15.904179	985.836935	11.525799
16.711365	994.575376	11.530803
16.322714	1010.332793	11.535808
16.811724	1009.010673	11.540813
16.842142	1008.523102	11.545818
16.916894	1002.060304	11.550823
17.192066	1007.693788	11.555827
16.638794	1012.864972	11.560832
17.155347	1006.338660	11.565837
17.056463	1007.115099	11.570842
17.028566	1010.395417	11.575847
17.414495	1004.574002	11.580851
17.508068	1001.156132	11.585856
17.401715	987.614796	11.590861
17.128400	985.299963	11.595866
16.798400	976.433551	11.600871
17.188258	988.849847	11.605875
17.183437	1004.426187	11.610880
17.553544	1001.111694	11.615885
17.628396	1012.760176	11.620890
17.508212	1003.835670	11.625895
17.366877	996.037819	11.630899
17.206076	1006.680255	11.635904
17.416221	1008.628972	11.640909
17.372895	1016.702855	11.645914
17.635028	1011.974372	11.650919
17.519501	1012.173401	11.655923
17.284983	1013.393884	11.660928
17.431889	1014.877392	11.665933
17.332277	1020.440533	11.670938
17.865553	1039.204913	11.675943
18.281211	1043.454059	11.680947
18.168517	1043.364839	11.685952
18.205629	1041.866380	11.690957
17.944942	1028.426076	11.695962
18.027068	1032.418193	11.700967
18.619570	1037.707939	11.705971
17.881399	1027.925031	11.710976
18.518849	1023.745617	11.715981
18.655648	1011.225598	11.720986
18.722571	1009.095584	11.725991
18.595356	995.122030	11.730995
18.584135	999.890800	11.736000
18.679995	988.201239	11.741005
18.614151	997.070418	11.746010
18.401202	1004.056273	11.751015
18.811857	995.862203	11.756019
18.519647	1002.946121	11.761024
18.812768	994.844835	11.766029
18.680793	1006.346801	11.771034
18.457295	1002.403031	11.776039
18.419134	999.446300	11.781043
18.147122	1006.207414	11.786048
18.789651	1018.525150	11.791053
18.559934	1031.853761	11.796058
18.708783	1037.764309	11.801063
19.029334	1026.391459	11.806067
18.708869	1034.952999	11.811072
18.926544	1033.345820	11.816077
18.958375	1030.077477	11.821082
18.785573	1031.665933	11.826087
19.148704	1042.129353	11.831091
19.394045	1057.240090	11.836096
19.620154	1056.474228	11.841101
19.499216	1057.979978	11.846106
19.294853	1058.365556	11.851111
19.760507	1048.707420	11.856115
19.689547	1049.946837	11.861120
19.585233	1033.475370	11.866125
19.374114	1037.207503	11.871130
19.648353	1045.381690	11.876135
20.194333	1056.443376	11.881139
19.556647	1044.993620	11.886144
19.868831	1026.916405	11.891149
20.090714	1037.199566	11.896154
19.885044	1037.159051	11.901159
19.872828	1033.341679	11.906163
19.462084	1036.905144	11.911168
20.046173	1046.777656	11.916173
19.865324	1058.634620	11.921178
20.254602	1064.571062	11.926183
20.356210	1058.593111	11.931187
20.029529	1068.558633	11.936192
20.629391	1052.934705	11.941197
20.472912	1053.979573	11.946202
20.112617	1035.251857	11.951207
20.477138	1038.488584	11.956211
20.516977	1054.006790	11.961216
20.814533	1040.152209	11.966221
20.415270	1027.277639	11.971226
20.103376	1027.013757	11.976231
20.375416	1037.240949	11.981235
20.262484	1045.359939	11.986240
20.419247	1045.850179	11.991245
20.429807	1050.299046	11.996250
20.533040	1053.552943	12.001255
20.726728	1057.694098	12.006259
20.632186	1057.335712	12.011264
21.107110	1051.420074	12.016269
20.936376	1063.970835	12.021274
20.569194	1063.366694	12.026279
20.651205	1054.238938	12.031283
20.570188	1061.584305	12.036288
21.167216	1075.568576	12.041293
20.658899	1070.121906	12.046298
20.870535	1076.066704	12.051303
21.434434	1071.840283	12.056307
21.049498	1060.966919	12.061312
21.164474	1052.357330	12.066317
21.409810	1050.498695	12.071322
21.199449	1048.111085	12.076327
21.297544	1042.009795	12.081331
21.367263	1045.417463	12.086336
21.267954	1042.989893	12.091341
21.239229	1031.822975	12.096346
20.979341	1023.411489	12.101351
21.081621	1013.051861	12.106355
20.868036	1025.963623	12.111360
21.108079	1014.661821	12.116365
20.927000	1021.898404	12.121370
21.119388	1030.733986	12.126375
21.137457	1023.964712	12.131379
20.623880	1024.725015	12.136384
20.791842	1021.705702	12.141389
21.050215	1019.157599	12.146394
20.562821	1026.706440	12.151399
20.802116	1017.498449	12.156403
21.148560	1016.244984	12.161408
21.050303	1024.877762	12.166413
20.975832	1016.538305	12.171418
21.038632	1022.419391	12.176423
21.136910	1019.723868	12.181427
20.784518	1023.306141	12.186432
21.080625	1021.260384	12.191437
21.052862	1020.811997	12.196442
21.179585	1026.284625	12.201447
21.255876	1023.740898	12.206451
21.299668	1030.545772	12.211456
21.138428	1008.045010	12.216461
21.172688	999.814420	12.221466
20.807565	995.769802	12.226471
21.047093	984.766530	12.231475
20.842302	991.564271	12.236480
20.739680	987.106360	12.241485
20.714944	989.762054	12.246490
20.360134	991.079344	12.251495
20.766118	1001.504600	12.256499
20.732963	1023.644758	12.261504
20.946084	1019.329282	12.266509
20.875848	1034.210683	12.271514
21.154572	1030.787115	12.276519
20.903628	1025.646465	12.281523
20.892282	1034.929085	12.286528
21.173278	1028.062625	12.291533
20.912073	1022.928472	12.296538
21.041711	1017.096520	12.301543
20.888191	997.797343	12.306547
20.438229	1009.512121	12.311552
20.772293	1023.329852	12.316557
21.196270	1032.929018	12.321562
21.118931	1028.773472	12.326567
21.270600	1008.624587	12.331571
20.622722	1006.364497	12.336576
20.894662	997.838157	12.341581
20.924684	1001.316174	12.346586
20.925079	997.455202	12.351591
20.875353	1004.651494	12.356595
21.008893	1005.883871	12.361600
21.047868	1006.529305	12.366605
20.961976	998.992341	12.371610
20.955759	999.702365	12.376615
21.018382	998.321510	12.381619
20.895524	1002.095739	12.386624
21.157377	1003.887169	12.391629
21.335729	1001.627525	12.396634
20.872810	1005.094533	12.401639
20.810378	1005.428932	12.406643
20.711962	1008.856735	12.411648
21.209046	1004.773235	12.416653
20.881517	1008.490978	12.421658
21.019482	1010.549175	12.426663
21.273935	1008.013589	12.431667
20.850788	1016.264698	12.436672
20.709016	1011.688360	12.441677
21.020215	1014.011331	12.446682
21.132521	1018.419059	12.451687
21.162746	1010.214813	12.456691
20.876027	1020.188454	12.461696
21.001792	1011.092300	12.466701
20.933944	1008.256710	12.471706
20.679360	1017.283787	12.476711
20.897903	1005.072652	12.481715
20.542224	1013.794560	12.486720
20.849611	1011.159108	12.491725
21.136851	1016.300658	12.496730
21.005322	1012.705459	12.501735
20.875574	1015.382320	12.506739
20.900345	1019.286768	12.511744
20.872545	1004.795633	12.516749
20.955361	1012.712097	12.521754
20.856250	1021.037915	12.526759
21.040585	1010.993825	12.531763
21.142545	1020.663984	12.536768
21.064123	1007.736394	12.541773
21.078992	1009.660565	12.546778
20.738408	1022.585414	12.551783
21.266823	1014.928513	12.556787
21.079156	1002.828078	12.561792
20.924544	993.515138	12.566797
20.860919	988.447384	12.571802
21.271728	985.794204	12.576807
21.057891	989.636528	12.581811
20.540345	990.804482	12.586816
20.657147	987.276843	12.591821
20.756978	984.632376	12.596826
20.648016	987.859089	12.601831
21.019592	1001.875238	12.606835
20.950294	1014.053305	12.611840
20.773346	1010.224709	12.616845
20.654661	1009.117702	12.621850
20.720244	1019.754096	12.626855
20.822924	1010.229664	12.631859
20.801339	1020.446399	12.636864
20.755146	1020.848278	12.641869
20.760929	1019.556509	12.646874
20.794665	1024.456131	12.651879
21.044464	1017.437130	12.656883
20.848875	1025.672123	12.661888
21.113145	1019.796167	12.666893
21.148670	1019.580877	12.671898
20.804309	1027.976379	12.676903
21.065719	1021.787885	12.681907
20.754882	1024.406980	12.686912
20.930646	1025.106725	12.691917
20.797156	1019.676729	12.696922
20.754189	1024.482134	12.701927
20.825174	1017.961554	12.706931
20.898280	1025.049952	12.711936
20.794685	1028.474305	12.716941
21.120980	1025.547056	12.721946
21.012451	1021.547648	12.726951
21.287233	1021.373837	12.731955
21.305620	1021.812801	12.736960
20.800921	1020.014871	12.741965
20.717281	1013.712646	12.746970
20.930017	1021.994866	12.751975
21.088251	1020.577484	12.756979
20.780982	1028.205180	12.761984
20.862089	1019.964968	12.766989
21.066213	1024.156035	12.771994
20.709629	1023.353499	12.776999
20.953976	1016.583722	12.782003
20.943932	1026.137693	12.787008
21.093070	1023.121213	12.792013
21.266123	1006.460903	12.797018
20.954514	1002.077897	12.802023
20.678579	993.150495	12.807027
20.823196	1006.596483	12.812032
20.789280	997.848241	12.817037
21.175423	996.842181	12.822042
20.560544	1005.943261	12.827047
20.991006	996.902638	12.832051
20.844436	1002.640798	12.837056
21.070009	1001.406083	12.842061
21.249280	990.224061	12.847066
20.799387	998.788430	12.852071
20.753333	993.211215	12.857075
20.834734	1006.154094	12.862080
20.863649	1000.734944	12.867085
20.780154	1004.786635	12.872090
20.896226	1012.618844	12.877095
21.174638	1004.542181	12.882099
20.945444	1009.862667	12.887104
21.030051	1007.055412	12.892109
21.304684	1013.674648	12.897114
21.094908	1010.882733	12.902119
21.138915	1002.462576	12.907123
21.309694	1018.885928	12.912128
20.620625	1008.703823	12.917133
20.952993	1008.910928	12.922138
20.400746	1010.748386	12.927143
20.974780	1013.593134	12.932147
20.692867	1009.716219	12.937152
20.484431	1005.536971	12.942157
20.832180	1015.280249	12.947162
20.831079	1009.521242	12.952167
21.164032	1005.317460	12.957171
20.862367	1014.386950	12.962176
20.846309	1012.544716	12.967181
20.616156	1005.541693	12.972186
20.704299	1007.629748	12.977191
20.854716	1002.034634	12.982195
20.816351	1018.770949	12.987200
20.994574	1042.659892	12.992205
21.071255	1030.872929	12.997210
20.885768	1022.361055	13.002215
20.878199	1011.501183	13.007219
20.791908	1022.511776	13.012224
20.889238	1022.534968	13.017229
21.151098	1009.256535	13.022234
20.957129	1018.722825	13.027239
20.745320	1006.515211	13.032243
21.042270	1015.206936	13.037248
21.121113	1012.001194	13.042253
21.140623	1012.820886	13.047258
20.827614	1019.372325	13.052263
20.946914	1017.188725	13.057267
20.813329	1011.902432	13.062272
20.594626	1016.548886	13.067277
20.965075	1011.924990	13.072282
21.342725	1013.534725	13.077287
21.232873	1007.856338	13.082291
21.150880	1009.310407	13.087296
21.196268	1016.100791	13.092301
21.104966	1020.604613	13.097306
21.074786	1023.817826	13.102311
21.316662	1007.175320	13.107315
21.007064	1014.326172	13.112320
20.993804	1007.443856	13.117325
20.819901	1000.603691	13.122330
20.931933	1004.304884	13.127335
20.810801	991.685420	13.132339
21.234935	1006.013087	13.137344
20.956923	994.783937	13.142349
20.910965	993.386962	13.147354
20.686858	984.752257	13.152359
20.695914	982.988615	13.157363
20.643379	993.159323	13.162368
20.448688	1005.802171	13.167373
21.137779	1019.677055	13.172378
20.944038	1023.830152	13.177383
21.098480	1017.425527	13.182387
21.101698	1025.147618	13.187392
21.191166	1018.979527	13.192397
20.943745	1000.650525	13.197402
20.656243	1003.641405	13.202407
21.110970	996.127015	13.207411
20.551492	993.058745	13.212416
21.283238	1008.473277	13.217421
21.752057	1004.121070	13.222426
21.443742	991.061594	13.227431
21.466744	990.276085	13.232435
21.357901	989.637127	13.237440
21.175442	987.909873	13.242445
21.216698	976.289287	13.247450
20.732030	969.774785	13.252455
20.712209	954.569041	13.257459
20.470073	968.767356	13.262464
20.693167	976.576462	13.267469
21.058530	985.586834	13.272474
20.680638	988.232814	13.277479
20.621978	988.298936	13.282483
20.907673	995.139688	13.287488
21.317531	999.375212	13.292493
21.231036	989.066913	13.297498
21.154694	989.808696	13.302503
21.233171	970.015041	13.307507
20.965980	957.609330	13.312512
20.853492	954.002590	13.317517
21.169157	953.564403	13.322522
20.662962	953.393440	13.327527
20.867346	948.216591	13.332531
20.938872	950.969853	13.337536
20.601203	953.391037	13.342541
20.560226	959.026999	13.347546
20.767605	976.707184	13.352551
20.750777	978.274418	13.357555
20.937507	985.588449	13.362560
20.694657	990.614824	13.367565
20.883118	990.338971	13.372570
20.730677	988.469597	13.377575
21.240047	983.073867	13.382579
20.896589	991.221300	13.387584
20.954388	990.100614	13.392589
21.494218	990.140702	13.397594
20.747934	984.301047	13.402599
20.806116	964.176538	13.407603
20.709329	971.704961	13.412608
20.719496	978.830971	13.417613
21.105217	989.198510	13.422618
20.934821	990.982732	13.427623
20.848993	985.751418	13.432627
21.235461	993.385679	13.437632
20.558155	974.993439	13.442637
20.998938	977.230634	13.447642
20.588732	989.748183	13.452647
21.100612	988.718197	13.457651
20.895430	1001.074682	13.462656
20.802462	998.490900	13.467661
20.943301	996.834925	13.472666
20.973083	995.228780	13.477671
20.996827	991.717490	13.482675
21.082183	998.507329	13.487680
20.381738	987.780085	13.492685
20.678151	990.237034	13.497690
20.675402	1000.110263	13.502695
21.020876	990.073296	13.507699
20.716592	993.657576	13.512704
20.613735	1003.974287	13.517709
20.966193	999.215717	13.522714
20.765029	1005.162975	13.527719
21.075851	995.881549	13.532723
21.022614	994.298717	13.537728
21.195468	996.844352	13.542733
20.968449	996.786970	13.547738
20.743025	1005.528778	13.552743
20.902347	995.893986	13.557747
21.156527	1001.782910	13.562752
20.910652	1004.020995	13.567757
20.810460	1006.616209	13.572762
20.568834	1004.179492	13.577767
20.838935	998.119781	13.582771
21.030425	1004.309585	13.587776
20.858410	1003.741458	13.592781
21.535122	999.046898	13.597786
20.676161	999.716417	13.602791
21.289223	996.938164	13.607795
21.178162	995.654192	13.612800
20.991164	988.469700	13.617805
20.960125	987.537140	13.622810
20.911887	985.910031	13.627815
20.823025	973.260970	13.632819
20.464953	979.841434	13.637824
20.642883	993.119067	13.642829
21.143023	996.418586	13.647834
20.982534	1004.821235	13.652839
20.870236	1001.566951	13.657843
21.138388	1007.111244	13.662848
20.922284	1000.771341	13.667853
20.967544	976.994957	13.672858
20.675788	974.414867	13.677863
20.976894	990.267950	13.682867
21.163204	997.577322	13.687872
20.529876	986.247651	13.692877
20.843138	981.919357	13.697882
20.940767	1000.714963	13.702887
21.115818	996.886809	13.707891
21.025884	986.021734	13.712896
21.075061	987.231075	13.717901
21.237972	979.048306	13.722906
20.947214	967.745572	13.727911
20.992486	975.832269	13.732915
20.995675	974.627790	13.737920
20.705041	980.760904	13.742925
21.000266	965.792450	13.747930
20.650223	972.863770	13.752935
20.847217	971.035143	13.757939
20.750575	973.216849	13.762944
20.871938	970.949612	13.767949
21.004502	970.136635	13.772954
21.178333	978.731027	13.777959
21.281086	966.853985	13.782963
20.964614	969.519037	13.787968
20.723292	966.783064	13.792973
20.951643	973.675876	13.797978
20.847135	977.041559	13.802983
21.015787	976.180157	13.807987
21.119979	979.745321	13.812992
20.895092	972.613121	13.817997
20.910567	974.582184	13.823002
20.630348	979.353647	13.828007
20.689621	971.833650	13.833011
20.965131	980.649031	13.838016
20.609487	979.386074	13.843021
21.133888	980.211963	13.848026
20.883617	979.979359	13.853031
21.364396	977.370236	13.858035
21.245633	985.512299	13.863040
21.063445	981.773425	13.868045
21.374214	980.102132	13.873050
21.092099	987.586548	13.878055
21.106279	979.820463	13.883059
21.114563	966.409884	13.888064
20.655886	967.617086	13.893069
21.034611	959.587193	13.898074
20.922623	953.298931	13.903079
20.707573	944.560854	13.908083
20.706056	961.218948	13.913088
20.801832	971.927501	13.918093
20.812823	978.286399	13.923098
21.035536	983.789528	13.928103
20.669946	969.878576	13.933107
20.789358	983.385707	13.938112
20.935037	980.964695	13.943117
21.203909	981.573080	13.948122
21.127923	980.173754	13.953127
21.067149	979.757476	13.958131
20.766266	967.455823	13.963136
20.763281	974.483824	13.968141
20.769476	971.287783	13.973146
20.976252	983.313888	13.978151
20.915465	981.474589	13.983155
21.329555	978.017165	13.988160
20.787845	970.137578	13.993165
21.125253	949.891792	13.998170
20.565856	944.778791	14.003175
20.962127	955.982126	14.008179
21.009065	955.617644	14.013184
20.861113	951.913959	14.018189
21.079420	950.277963	14.023207
20.844103	952.487368	14.028224
21.104849	951.583953	14.033242
20.908841	945.848668	14.038259
20.726040	943.753102	14.043277
20.792401	952.291540	14.048295
20.946139	966.027179	14.053312
21.117087	974.461077	14.058330
21.284702	976.280119	14.063347
21.128611	970.309224	14.068365
20.937325	952.943963	14.073383
20.705887	974.364683	14.078400
21.099024	977.251043	14.083418
20.845540	977.103163	14.088435
21.031251	985.062062	14.093453
21.270246	981.001518	14.098471
20.945877	987.100883	14.103488
20.986515	986.034796	14.108506
21.656125	993.014212	14.113523
20.945918	991.179944	14.118541
21.333318	983.904356	14.123559
21.131505	989.361799	14.128576
21.434836	990.573280	14.133594
21.410180	992.398122	14.138611
21.225291	1000.495377	14.143629
21.533210	992.199480	14.148647
21.107482	991.434628	14.153664
21.014546	988.049935	14.158682
21.408525	984.709329	14.163699
20.837257	988.731583	14.168717
21.183525	979.537715	14.173735
20.999771	1006.370375	14.178752
21.709091	1016.305414	14.183770
21.271580	1013.257374	14.188787
21.227044	1017.397608	14.193805
21.706384	1011.124824	14.198823
21.766400	1017.452019	14.203840
21.307961	1020.226105	14.208858
21.693203	1024.211153	14.213875
21.559910	1032.914978	14.218893
21.845845	1019.896106	14.223911
21.661601	1030.371787	14.228928
21.423611	1028.320321	14.233946
21.761663	1025.823215	14.238963
21.180009	1028.801119	14.243981
21.559429	1022.430887	14.248999
21.347618	1028.014869	14.254016
21.521606	1034.879264	14.259034
21.239585	1030.028445	14.264051
21.433604	1042.338241	14.269069
21.943107	1049.809735	14.274087
21.944183	1059.468170	14.279104
21.990211	1058.705114	14.284122
21.778718	1059.811153	14.289139
21.888339	1062.888276	14.294157
22.240447	1060.669879	14.299175
22.081453	1051.264543	14.304192
21.627113	1039.197442	14.309210
21.492494	1042.718828	14.314227
21.770780	1059.985825	14.319245
21.934460	1050.829127	14.324263
22.121302	1059.632815	14.329280
22.259142	1060.224989	14.334298
21.866877	1061.010420	14.339315
22.007549	1060.667391	14.344333
22.417266	1063.206804	14.349351
22.164810	1063.415467	14.354368
22.093758	1067.142906	14.359386
22.777037	1063.964509	14.364403
22.520524	1049.386521	14.369421
22.775158	1043.525901	14.374439
22.522882	1032.754575	14.379456
22.303269	1034.018316	14.384474
22.178055	1033.196819	14.389491
21.897202	1031.847242	14.394509
22.118392	1023.604783	14.399527
22.095400	1024.664720	14.404544
22.022299	1030.377295	14.409562
22.007116	1025.839021	14.414579
21.606773	1042.221095	14.419597
21.845122	1047.769245	14.424615
22.039201	1056.153549	14.429632
22.103004	1060.418144	14.434650
22.553326	1056.407183	14.439667
22.202026	1074.544402	14.444685
22.178773	1066.413522	14.449703
22.535480	1064.736897	14.454720
22.280035	1071.232776	14.459738
22.705965	1076.055415	14.464755
22.307117	1074.988289	14.469773
22.767297	1085.445259	14.474791
22.984881	1089.857525	14.479808
22.648851	1080.702227	14.484826
22.657941	1073.104423	14.489843
22.432840	1069.259264	14.494861
22.453687	1069.095847	14.499879
22.459892	1073.059273	14.504896
22.587582	1087.433392	14.509914
23.093880	1090.977590	14.514931
22.588600	1089.609788	14.519949
22.831689	1094.211793	14.524967
22.837609	1091.575937	14.529984
22.801448	1093.094472	14.535002
23.301243	1091.790193	14.540019
22.917954	1083.446208	14.545037
22.731907	1069.486484	14.550055
22.644467	1067.361952	14.555072
22.613096	1081.117224	14.560090
23.143451	1075.538478	14.565107
22.967806	1085.927283	14.570125
23.052405	1090.164303	14.575143
23.243547	1074.876025	14.580160
22.655811	1076.833642	14.585178
22.746947	1076.599507	14.590195
23.063691	1093.128395	14.595213
23.127980	1097.136597	14.600231
23.235546	1095.020757	14.605248
23.160032	1101.033401	14.610266
23.296110	1084.799361	14.615283
22.919432	1077.305888	14.620301
23.001207	1082.945861	14.625319
23.501530	1084.998053	14.630336
23.192129	1085.511778	14.635354
23.218443	1071.791647	14.640371
23.098169	1071.953236	14.645389
23.163237	1080.373846	14.650407
23.227366	1086.703120	14.655424
23.144588	1090.457774	14.660442
23.547510	1093.709043	14.665459
22.937904	1096.681908	14.670477
23.182370	1088.490547	14.675495
22.772124	1086.953290	14.680512
22.857485	1095.788573	14.685530
23.153352	1081.946621	14.690547
23.105357	1093.725073	14.695565
23.419338	1095.583607	14.700583
23.371162	1093.093650	14.705600
23.512932	1105.152198	14.710618
23.503914	1108.530401	14.715635
23.567149	1108.382946	14.720653
23.359177	1107.667374	14.725671
23.906142	1109.043409	14.730688
23.549012	1104.688159	14.735706
23.644903	1096.291935	14.740723
23.625636	1097.141773	14.745741
23.622753	1109.922030	14.750759
23.964156	1103.153920	14.755776
23.704495	1104.367441	14.760794
23.895772	1086.160395	14.765811
23.555443	1091.344748	14.770829
23.515983	1091.310183	14.775847
24.066345	1095.530740	14.780864
23.611070	1099.413833	14.785882
23.758836	1094.877131	14.790899
23.872263	1110.887310	14.795917
23.661253	1117.648445	14.800935
24.166228	1117.609126	14.805952
24.211251	1116.611181	14.810970
24.050542	1092.862848	14.815987
24.025997	1092.921403	14.821005
23.255354	1096.349864	14.826023
23.839734	1102.559629	14.831040
23.797087	1116.303084	14.836058
23.837881	1113.402957	14.841075
24.049838	1125.065204	14.846093
23.821365	1123.928702	14.851111
23.787290	1119.729888	14.856128
23.779412	1129.530857	14.861146
23.954243	1119.302435	14.866163
24.010388	1117.272974	14.871181
23.676445	1116.617585	14.876199
23.785275	1118.979443	14.881216
23.983953	1139.734078	14.886234
24.359515	1147.369541	14.891251
24.619053	1152.619583	14.896269
24.462726	1146.841196	14.901287
24.836036	1131.043639	14.906304
24.564085	1124.988210	14.911322
24.267896	1114.270818	14.916339
24.351949	1112.624398	14.921357
24.502159	1109.498409	14.926375
24.320316	1106.744337	14.931392
24.351917	1114.576562	14.936410
24.413924	1109.100547	14.941427
24.356822	1104.632434	14.946445
24.222913	1111.870545	14.951463
24.706375	1107.673559	14.956480
24.123470	1113.170003	14.961498
24.559218	1113.670942	14.966515
24.343490	1118.952454	14.971533
24.607318	1142.790659	14.976551
24.976369	1134.723989	14.981568
24.587913	1134.843756	14.986586
24.726469	1124.924330	14.991603
24.544488	1118.863715	14.996621
24.675471	1129.528350	15.001639
24.663534	1132.696806	15.006656
24.853229	1145.330679	15.011674
24.635158	1143.294682	15.016691
25.375177	1143.652501	15.021709
24.632229	1131.956096	15.026727
24.863165	1119.499371	15.031744
24.316175	1125.551124	15.036762
24.510195	1139.303239	15.041779
24.925600	1139.945866	15.046797
24.844919	1148.991945	15.051815
25.260432	1136.687040	15.056832
25.106160	1147.290743	15.061850
24.839167	1137.397924	15.066867
25.451721	1141.200318	15.071885
25.097940	1147.106345	15.076903
25.002085	1140.311605	15.081920
24.955188	1140.358243	15.086938
25.101353	1140.804492	15.091955
25.456263	1143.297799	15.096973
24.808802	1134.262799	15.101991
25.160597	1132.526375	15.107008
24.903137	1144.146273	15.112026
25.043667	1139.069023	15.117043
25.345257	1151.877433	15.122061
25.138078	1148.358344	15.127079
25.149498	1141.225499	15.132096
25.023352	1145.807747	15.137114
25.135135	1150.726794	15.142131
25.150760	1147.929015	15.147149
25.086765	1151.508796	15.152167
25.270462	1142.549415	15.157184
25.305263	1148.730974	15.162202
25.383119	1155.037055	15.167219
25.359575	1143.029881	15.172237
25.464787	1150.235280	15.177255
25.396826	1145.920211	15.182272
25.156499	1145.963396	15.187290
25.293977	1142.792729	15.192307
25.311639	1155.445475	15.197325
25.189988	1172.714232	15.202343
25.649609	1166.930635	15.207360
25.545419	1171.484715	15.212378
25.614955	1172.818192	15.217395
26.068470	1172.293166	15.222413
25.667220	1179.648410	15.227431
25.917999	1185.228733	15.232448
25.856710	1177.835480	15.237466
25.887144	1165.544602	15.242483
25.620344	1147.687699	15.247501
25.385311	1160.962562	15.252519
25.742466	1163.253108	15.257536
25.744644	1174.756461	15.262554
25.523533	1176.845341	15.267571
25.818053	1179.113162	15.272589
25.868666	1178.595398	15.277607
25.854311	1174.879842	15.282624
25.619754	1177.044656	15.287642
25.862252	1186.702333	15.292659
25.867202	1170.196567	15.297677
25.638190	1174.667316	15.302695
25.951820	1171.792847	15.307712
26.096030	1179.036852	15.312730
26.276916	1171.463881	15.317747
26.647137	1163.866719	15.322765
26.575943	1176.115784	15.327783
26.399383	1169.829004	15.332800
26.321807	1173.690275	15.337818
26.598429	1172.236049	15.342835
26.412845	1170.353152	15.347853
26.288964	1179.492096	15.352871
26.337763	1167.501637	15.357888
26.076553	1180.964878	15.362906
26.088609	1182.776361	15.367923
26.447598	1169.345594	15.372941
26.452803	1181.376035	15.377959
26.524104	1177.159532	15.382976
26.364727	1178.077495	15.387994
26.308362	1171.852396	15.393011
26.231156	1171.798316	15.398029
26.252499	1179.193714	15.403047
26.325499	1175.598231	15.408064
26.291270	1177.384182	15.413082
26.111538	1180.218000	15.418099
26.425022	1178.365295	15.423117
26.371129	1182.457960	15.428135
26.841536	1188.143161	15.433152
26.761844	1173.157543	15.438170
26.596670	1174.227693	15.443187
26.496304	1170.909988	15.448205
26.337502	1174.790698	15.453223
26.582193	1181.767457	15.458240
26.673072	1193.910001	15.463258
26.716871	1199.562040	15.468275
27.005819	1197.172942	15.473293
26.664071	1202.261109	15.478311
27.064621	1197.453853	15.483328
27.367297	1197.436225	15.488346
26.765019	1192.002020	15.493363
26.744835	1183.533909	15.498381
26.607227	1183.748081	15.503399
27.127707	1199.062524	15.508416
27.279455	1200.001955	15.513434
26.841852	1198.829643	15.518451
27.398384	1196.913609	15.523469
27.151974	1193.224449	15.528487
26.943400	1172.639586	15.533504
27.001415	1181.361879	15.538522
26.924544	1205.088500	15.543539
27.156786	1193.533932	15.548557
26.851566	1204.482873	15.553575
27.394145	1207.727546	15.558592
27.554396	1202.974874	15.563610
27.484790	1210.260672	15.568627
27.541485	1190.620548	15.573645
27.095792	1178.693599	15.578663
27.370499	1171.514025	15.583680
27.382119	1172.067996	15.588698
27.096456	1171.921299	15.593715
27.106958	1181.040353	15.598733
27.196995	1201.812517	15.603751
27.255554	1198.523862	15.608768
27.455793	1203.817951	15.613786
27.258374	1203.244277	15.618803
27.422124	1194.469799	15.623821
27.666140	1204.547735	15.628839
27.230255	1194.698010	15.633856
27.205667	1200.893710	15.638874
26.974888	1203.085047	15.643891
27.337807	1206.394385	15.648909
27.210861	1228.167647	15.653927
28.016201	1225.934124	15.658944
27.930149	1229.052703	15.663962
27.857762	1229.047014	15.668979
27.662386	1224.738413	15.673997
27.692144	1234.725926	15.679015
27.844956	1225.743838	15.684032
27.975470	1229.452113	15.689050
27.887290	1234.837003	15.694067
28.394768	1218.080053	15.699085
27.981997	1221.787764	15.704103
27.878060	1214.929016	15.709120
27.609400	1198.926863	15.714138
27.460177	1215.619637	15.719155
27.848657	1221.592148	15.724173
27.632165	1223.549523	15.729191
27.923601	1221.387573	15.734208
28.137507	1218.119922	15.739226
27.706896	1231.440976	15.744243
28.163826	1228.626582	15.749261
28.249038	1233.057253	15.754279
28.115122	1225.438220	15.759296
28.195328	1228.825170	15.764314
27.967929	1236.279778	15.769331
27.815788	1222.557038	15.774349
28.108763	1234.043256	15.779367
28.122454	1231.619843	15.784384
28.347691	1237.392770	15.789402
28.408288	1253.229853	15.794419
28.455524	1246.963338	15.799437
28.425364	1248.975390	15.804455
28.449614	1252.446355	15.809472
28.905253	1246.477962	15.814490
28.370061	1245.820454	15.819507
28.384106	1224.003549	15.824525
28.771847	1224.067409	15.829543
28.236457	1225.627451	15.834560
28.321965	1233.925732	15.839578
28.606182	1248.136536	15.844595
28.862331	1250.701129	15.849613
28.608773	1258.318515	15.854631
28.569876	1260.623825	15.859648
29.150309	1253.186660	15.864666
29.185052	1247.310510	15.869683
29.254355	1234.138034	15.874701
29.188940	1225.643794	15.879719
29.067813	1228.051395	15.884736
29.180116	1222.598215	15.889754
29.222516	1228.612741	15.894771
29.302532	1227.014250	15.899789
29.201563	1216.776746	15.904807
28.878057	1206.364787	15.909824
29.022827	1190.553593	15.914842
28.185395	1203.574263	15.919859
28.654463	1210.176709	15.924877
28.934109	1219.328782	15.929895
28.835984	1220.443350	15.934912
28.826541	1217.594340	15.939930
28.631661	1224.199987	15.944947
28.808975	1222.041854	15.949965
28.792179	1226.817601	15.954983
28.626843	1248.585662	15.960000
29.338336	1247.445881	15.965018
29.308313	1252.445577	15.970035
29.733575	1252.874296	15.975053
29.352744	1248.293520	15.980071
29.354937	1252.104517	15.985088
29.403261	1248.185661	15.990106
29.002360	1255.318419	15.995123
29.269272	1251.645181	16.000141
29.907868	1246.536838	16.005159
29.358022	1252.735992	16.010176
29.508152	1248.778025	16.015194
29.356243	1250.840876	16.020211
29.617529	1240.670000	16.025229
29.613299	1238.231940	16.030247
29.372022	1247.375301	16.035264
29.795741	1240.713108	16.040282
29.397098	1244.744415	16.045299
29.822456	1242.469336	16.050317
29.717006	1239.661194	16.055335
29.613807	1243.989121	16.060352
29.924370	1233.785783	16.065370
29.743852	1242.759261	16.070387
29.915014	1245.128957	16.075405
29.495535	1239.179493	16.080423
29.724393	1242.664986	16.085440
29.936239	1242.681437	16.090458
29.703468	1239.096629	16.095475
29.928107	1242.582846	16.100493
29.741873	1241.358771	16.105511
29.401906	1246.298209	16.110528
29.540459	1246.297696	16.115546
29.627794	1249.591294	16.120563
29.944740	1265.513584	16.125581
29.926949	1274.834018	16.130599
29.545285	1274.552191	16.135616
29.958751	1278.150935	16.140634
30.002242	1276.121261	16.145651
30.409219	1275.810923	16.150669
30.923744	1264.368156	16.155687
30.704544	1269.782216	16.160704
30.840995	1265.139521	16.165722
30.898006	1240.227155	16.170739
30.698086	1227.935955	16.175757
30.667347	1226.830510	16.180775
30.504248	1227.948344	16.185792
30.705362	1228.724575	16.190810
30.491650	1229.181736	16.195827
30.454237	1235.311138	16.200845
30.618725	1227.818123	16.205863
30.427793	1228.119004	16.210880
30.477809	1230.905172	16.215898
30.320336	1234.524622	16.220915
29.923289	1235.815649	16.225933
30.186301	1239.011797	16.230951
30.083996	1239.906591	16.235968
30.597173	1246.805848	16.240986
30.316884	1263.438854	16.246003
30.559839	1266.341175	16.251021
30.811906	1262.629924	16.256039
30.360938	1270.027989	16.261056
30.593865	1274.382161	16.266074
30.778298	1272.466524	16.271091
30.727558	1268.585515	16.276109
30.761641	1274.737717	16.281127
30.800387	1269.988927	16.286144
30.980498	1266.312850	16.291162
30.911206	1273.280090	16.296179
30.935574	1269.381086	16.301197
31.351534	1265.372026	16.306215
30.551393	1259.428758	16.311232
30.978252	1270.706600	16.316250
30.997384	1279.535624	16.321267
30.700458	1287.494740	16.326285
31.340627	1299.347504	16.331303
31.261940	1297.537612	16.336320
31.194444	1285.963099	16.341338
31.114618	1294.348032	16.346355
31.109094	1287.798000	16.351373
30.982346	1280.662006	16.356391
31.013217	1294.876129	16.361408
30.840034	1296.250444	16.366426
31.027468	1291.707278	16.371443
31.297912	1300.424715	16.376461
31.415083	1308.533339	16.381479
31.917486	1328.725081	16.386496
31.573557	1296.512569	16.391514
32.058127	1298.179268	16.396531
31.265812	1289.163105	16.401549
31.411909	1285.567271	16.406567
31.599276	1286.238766	16.411584
31.728401	1287.742762	16.416602
31.903935	1287.805994	16.421619
31.701275	1292.291157	16.426637
31.781285	1283.350654	16.431655
31.839141	1285.766164	16.436672
31.593980	1284.967974	16.441690
31.591146	1297.673961	16.446707
31.824496	1312.097107	16.451725
32.253908	1306.566299	16.456743
31.794247	1314.185580	16.461760
31.708159	1316.717120	16.466778
32.175527	1311.686543	16.471795
31.710432	1324.343841	16.476813
32.060040	1322.108119	16.481831
31.671295	1321.041998	16.486848
31.987846	1316.794040	16.491866
32.452296	1318.584674	16.496883
31.977175	1311.911976	16.501901
32.104521	1314.992016	16.506919
31.703866	1327.496523	16.511936
32.346099	1322.963570	16.516954
32.328093	1321.741751	16.521971
32.258098	1324.020904	16.526989
32.259532	1313.481108	16.532007
31.887990	1315.274508	16.537024
31.927574	1314.529869	16.542042
32.242147	1310.244059	16.547059
31.994118	1320.023325	16.552077
32.391669	1327.769291	16.557095
32.594360	1349.173578	16.562112
32.805224	1337.418219	16.567130
32.710761	1334.899149	16.572147
32.300813	1335.752590	16.577165
32.869368	1337.702560	16.582183
32.797784	1338.392861	16.587200
32.504408	1323.870153	16.592218
32.643405	1326.237108	16.597235
32.733944	1334.586553	16.602253
32.684177	1332.585066	16.607271
32.786598	1340.191069	16.612288
32.833652	1331.165630	16.617306
33.159202	1332.782424	16.622323
32.944953	1327.655693	16.627341
32.768474	1311.007639	16.632359
32.767384	1311.962651	16.637376
32.930601	1331.808577	16.642394
33.294229	1336.620324	16.647411
32.823962	1340.968688	16.652429
33.225777	1340.818305	16.657447
32.962742	1338.972684	16.662464
32.969652	1335.158160	16.667482
32.970187	1342.439474	16.672499
32.882030	1342.031726	16.677517
33.243609	1337.482708	16.682535
32.901744	1340.333721	16.687552
33.027703	1337.206726	16.692570
33.267724	1336.569861	16.697587
33.144513	1337.655270	16.702605
33.396386	1335.521744	16.707623
33.385471	1343.053864	16.712640
33.268051	1339.199232	16.717658
33.512476	1333.010303	16.722675
33.235374	1338.733947	16.727693
33.501549	1330.912396	16.732711
33.283970	1337.702708	16.737728
32.959678	1342.853288	16.742746
33.513432	1365.951905	16.747763
33.386216	1365.913880	16.752781
33.448271	1372.993698	16.757799
33.387654	1372.889524	16.762816
33.696274	1370.115495	16.767834
33.571106	1369.051429	16.772851
33.820908	1377.249170	16.777869
34.211351	1357.256311	16.782887
34.241653	1363.704500	16.787904
34.042657	1361.195473	16.792922
34.473927	1363.085511	16.797939
34.345999	1370.037648	16.802957
34.409273	1342.670266	16.807975
34.314696	1338.883772	16.812992
33.739403	1334.875732	16.818010
34.166645	1325.448861	16.823027
34.036413	1328.541566	16.828045
33.943210	1329.226124	16.833063
34.156224	1338.188097	16.838080
34.114047	1333.795713	16.843098
34.121094	1331.530525	16.848115
34.138401	1336.093746	16.853133
34.025550	1324.997497	16.858151
34.075453	1338.824109	16.863168
34.074883	1351.454941	16.868186
34.159928	1355.665183	16.873203
34.154049	1363.555933	16.878221
33.948327	1361.169330	16.883239
33.807781	1361.350540	16.888256
34.076255	1365.229701	16.893274
34.308025	1361.755000	16.898291
34.421088	1379.925567	16.903309
34.797906	1379.140825	16.908327
34.879673	1377.290026	16.913344
34.914827	1375.588177	16.918362
34.776702	1360.115500	16.923379
34.511332	1361.165829	16.928397
34.476912	1356.206307	16.933415
34.658520	1369.285493	16.938432
34.572644	1386.835782	16.943450
34.659937	1375.972532	16.948467
34.472221	1391.210140	16.953485
34.776723	1391.642244	16.958503
34.979485	1391.049958	16.963520
35.034162	1397.962138	16.968538
34.930485	1391.662378	16.973555
34.892878	1389.934022	16.978573
35.002668	1391.810277	16.983591
35.050499	1388.320252	16.988608
34.849631	1389.924541	16.993626
35.144699	1378.920931	16.998643
35.574389	1383.848544	17.003661
35.714541	1375.361503	17.008679
35.825960	1381.162266	17.013696
35.632281	1375.546906	17.018714
35.591301	1376.372132	17.023731
35.547943	1372.649296	17.028749
35.686484	1359.411689	17.033767
35.276343	1353.195592	17.038784
35.360040	1348.101244	17.043802
35.417099	1342.934292	17.048819
34.993488	1345.782390	17.053837
34.913226	1370.326457	17.058855
35.467274	1371.416631	17.063872
35.528516	1373.176786	17.068890
35.431604	1372.768175	17.073907
35.296798	1375.598657	17.078925
35.401769	1377.584802	17.083943
35.565378	1368.554713	17.088960
35.492006	1380.423173	17.093978
35.720907	1373.786845	17.098995
35.459223	1375.801598	17.104013
35.663258	1395.494924	17.109031
35.716832	1402.482105	17.114048
35.718311	1402.580692	17.119066
36.098309	1406.570283	17.124083
36.022700	1412.239328	17.129101
35.957889	1408.099254	17.134119
36.127665	1402.830271	17.139136
35.733848	1411.033250	17.144154
35.998229	1401.780333	17.149171
36.451365	1397.556185	17.154189
36.175325	1402.303198	17.159207
36.379124	1410.530106	17.164224
35.958140	1406.036096	17.169242
36.368414	1403.947458	17.174259
36.514206	1406.253805	17.179277
36.412084	1408.304203	17.184295
36.490291	1405.616133	17.189312
36.135911	1413.515079	17.194330
36.256677	1402.756317	17.199347
36.325131	1404.457753	17.204365
36.308727	1407.200217	17.209383
36.438686	1404.408777	17.214400
36.238631	1410.690948	17.219418
36.424224	1416.297887	17.224435
36.623537	1418.216283	17.229453
36.512657	1427.462602	17.234471
36.964120	1431.369073	17.239488
36.717463	1446.252237	17.244506
36.965767	1435.631446	17.249523
37.331625	1423.332862	17.254541
36.866476	1416.074492	17.259559
36.687489	1405.296248	17.264576
36.727217	1400.340537	17.269594
36.949592	1398.321126	17.274611
36.806955	1408.219792	17.279629
36.858649	1420.772421	17.284647
37.213521	1425.280156	17.289664
37.409671	1437.425316	17.294682
37.397472	1424.207986	17.299699
37.045848	1407.472917	17.304717
36.439887	1413.319119	17.309735
37.287226	1418.794885	17.314752
36.794777	1430.366299	17.319770
37.637274	1429.915535	17.324787
37.681090	1432.190547	17.329805
37.415643	1434.787900	17.334823
37.686227	1425.889453	17.339840
37.026151	1429.503771	17.344858
37.251704	1430.979436	17.349875
37.687788	1435.977238	17.354893
37.047636	1431.936980	17.359911
37.625738	1435.586284	17.364928
37.385106	1435.424382	17.369946
37.226643	1431.906324	17.374963
37.661569	1432.105024	17.379981
37.418141	1440.655106	17.384999
37.516347	1423.168026	17.390016
37.307034	1439.480751	17.395034
37.012739	1435.926526	17.400051
37.425406	1447.954644	17.405069
37.543638	1459.256795	17.410087
38.127493	1460.104439	17.415104
38.003251	1462.268097	17.420122
37.900366	1451.889020	17.425139
37.984772	1468.256940	17.430157
37.950912	1468.041474	17.435175
38.563036	1453.069273	17.440192
38.086667	1452.417025	17.445210
38.645521	1454.870300	17.450227
38.446201	1447.409236	17.455245
38.277640	1452.475665	17.460263
38.732788	1455.440865	17.465280
38.444738	1438.105827	17.470298
38.531211	1417.780321	17.475315
38.369766	1413.822971	17.480333
38.239094	1418.537584	17.485351
38.505366	1405.626104	17.490368
38.222215	1413.630565	17.495386
38.245539	1434.008925	17.500403
38.195478	1443.638172	17.505421
38.601476	1451.712708	17.510439
38.653446	1445.149208	17.515456
38.563249	1447.668874	17.520474
38.658532	1443.880909	17.525491
38.522377	1447.792058	17.530509
38.831480	1442.222769	17.535527
38.623511	1445.468997	17.540544
38.616590	1451.421979	17.545562
38.683689	1451.981411	17.550579
38.837539	1447.994407	17.555597
38.653948	1449.463836	17.560615
38.649182	1446.558859	17.565632
38.859640	1451.731977	17.570650
38.660895	1450.750605	17.575667
38.875106	1467.976281	17.580685
38.850137	1473.307892	17.585703
39.444692	1468.018821	17.590720
39.599180	1473.453930	17.595738
39.351661	1473.655056	17.600755
39.282542	1468.210059	17.605773
39.149967	1475.326048	17.610791
39.688609	1461.423633	17.615808
39.157395	1450.851825	17.620826
39.412426	1454.494706	17.625843
39.610531	1449.299206	17.630861
39.528195	1450.615040	17.635879
39.756667	1439.842119	17.640896
39.508090	1446.442103	17.645914
39.345466	1441.072207	17.650931
39.126823	1445.627877	17.655949
39.446269	1459.549343	17.660967
39.438202	1463.083775	17.665984
39.303189	1471.816488	17.671002
39.383544	1472.587449	17.676019
39.534964	1469.726170	17.681037
39.329007	1469.603208	17.686055
39.668281	1467.865746	17.691072
39.566229	1477.956731	17.696090
39.622569	1489.864458	17.701107
40.185185	1500.529368	17.706125
39.822809	1502.152696	17.711143
39.773683	1507.807391	17.716160
40.103352	1505.921556	17.721178
40.075031	1501.788588	17.726195
40.420978	1499.531420	17.731213
40.266927	1504.185886	17.736231
40.263273	1501.673663	17.741248
40.400989	1499.758133	17.746266
40.185305	1499.668732	17.751283
40.405374	1494.597417	17.756301
40.054670	1501.389755	17.761319
40.300709	1496.284456	17.766336
40.532565	1497.966550	17.771354
40.526770	1498.698340	17.776371
40.723411	1496.041923	17.781389
40.318275	1501.082386	17.786407
40.473153	1498.096086	17.791424
40.291028	1505.971451	17.796442
40.225176	1503.087567	17.801459
40.580019	1498.699517	17.806477
40.368614	1516.738058	17.811495
40.841280	1518.100886	17.816512
40.979437	1524.308579	17.821530
40.945242	1530.672610	17.826547
41.176232	1518.326201	17.831565
40.837747	1521.625139	17.836583
40.815465	1524.322957	17.841600
40.890035	1526.189517	17.846618
40.913289	1525.418137	17.851635
40.894921	1523.306113	17.856653
41.064108	1527.086971	17.861671
40.995362	1519.477882	17.866688
40.652985	1523.559461	17.871706
40.868447	1519.077573	17.876723
41.131810	1515.374171	17.881741
40.841029	1522.468088	17.886759
41.296805	1532.802088	17.891776
41.776009	1539.285210	17.896794
41.769399	1531.822172	17.901811
41.774558	1525.386756	17.906829
41.638678	1516.252007	17.911847
41.633296	1517.316440	17.916864
41.561487	1509.553140	17.921882
41.329597	1517.713056	17.926899
41.807807	1510.840206	17.931917
41.609344	1521.413152	17.936935
41.207453	1520.734743	17.941952
41.586759	1525.631273	17.946970
41.694754	1544.457695	17.951987
41.916043	1550.645634	17.957005
41.708755	1556.530635	17.962023
41.897331	1556.987345	17.967040
41.936944	1549.969572	17.972058
41.733991	1551.044649	17.977075
41.970183	1541.045615	17.982093
42.292366	1550.188622	17.987111
42.146213	1541.753726	17.992128
42.031438	1542.194327	17.997146
41.895445	1542.979153	18.002163
42.314589	1539.300224	18.007181
42.165358	1541.763090	18.012199
42.105963	1546.035553	18.017216
42.036210	1543.944936	18.022234
42.062747	1540.278981	18.027251
42.159541	1533.725478	18.032269
42.228352	1553.747733	18.037287
42.181083	1562.180383	18.042304
42.868639	1572.621538	18.047322
42.604794	1579.013936	18.052339
42.583734	1569.152701	18.057357
42.678994	1571.475218	18.062375
42.704767	1580.632837	18.067392
42.741974	1571.028963	18.072410
42.650456	1572.669645	18.077427
42.627190	1568.867719	18.082445
42.553523	1566.475374	18.087463
42.735248	1569.801682	18.092480
42.756944	1571.711962	18.097498
42.563700	1569.900415	18.102515
42.913570	1564.743824	18.107533
42.830180	1570.691063	18.112551
43.279436	1587.075697	18.117568
43.067145	1594.944466	18.122586
43.195568	1602.478809	18.127603
43.066065	1607.174378	18.132621
43.187180	1601.648682	18.137639
43.136317	1607.376160	18.142656
43.368891	1600.465061	18.147674
43.123376	1600.178389	18.152691
43.247669	1603.901601	18.157709
43.601813	1598.504083	18.162727
43.406867	1592.398255	18.167744
43.420035	1597.641078	18.172762
43.427959	1588.614324	18.177779
43.606285	1600.287812	18.182797
43.610400	1601.347866	18.187815
43.129355	1602.964380	18.192832
43.503458	1594.654456	18.197850
43.320002	1601.345714	18.202867
43.484156	1609.720486	18.207885
44.286418	1616.423086	18.212903
44.572316	1611.666862	18.217920
44.567859	1595.508361	18.222938
44.271146	1585.849510	18.227955
44.486632	1575.903615	18.232973
44.230205	1583.516925	18.237991
44.222251	1581.128274	18.243008
44.740831	1578.465865	18.248026
44.340979	1579.640851	18.253043
44.365290	1581.745194	18.258061
44.309493	1582.002436	18.263079
44.407738	1580.604350	18.268096
44.562822	1574.433793	18.273114
44.124562	1564.761424	18.278131
44.595725	1571.293974	18.283149
44.413301	1578.177980	18.288167
44.540351	1585.076654	18.293184
44.791128	1577.596634	18.298202
44.585454	1567.285896	18.303219
44.843110	1560.092137	18.308237
44.575232	1552.453386	18.313255
44.284386	1556.119795	18.318272
44.494090	1566.282597	18.323290
44.495447	1586.862582	18.328307
44.939242	1581.642633	18.333325
44.574230	1581.810749	18.338343
44.408788	1580.544494	18.343360
44.642129	1577.748686	18.348378
44.842350	1579.264934	18.353395
44.935451	1587.896785	18.358413
44.630931	1606.687696	18.363431
44.669249	1614.259937	18.368448
44.695397	1607.666147	18.373466
44.773039	1615.430093	18.378483
45.019147	1610.549968	18.383501
45.148872	1620.908428	18.388519
45.071792	1640.945570	18.393536
45.531745	1632.663432	18.398554
45.547308	1635.875313	18.403571
45.554147	1635.044530	18.408589
45.626927	1633.234223	18.413607
45.561603	1649.683915	18.418624
45.637847	1641.024989	18.423642
45.531420	1651.828334	18.428659
45.511433	1647.852578	18.433677
45.532881	1636.393280	18.438695
45.508382	1640.851934	18.443712
45.838715	1643.090453	18.448730
45.601064	1640.632894	18.453747
45.966102	1644.628656	18.458765
45.871352	1639.975484	18.463783
45.734630	1640.581680	18.468800
45.846526	1645.830823	18.473818
45.483736	1642.150875	18.478835
45.686591	1644.951470	18.483853
45.885978	1654.445944	18.488871
45.561777	1663.098982	18.493888
46.068021	1660.434738	18.498906
45.999794	1667.058624	18.503923
46.348213	1667.787574	18.508941
46.508206	1665.051182	18.513959
46.196263	1660.562027	18.518976
46.156174	1652.681000	18.523994
46.017631	1665.955497	18.529011
46.414339	1683.499375	18.534029
46.705008	1693.255420	18.539047
46.501792	1697.757725	18.544064
46.854620	1689.729778	18.549082
46.741136	1689.327543	18.554099
47.250916	1686.905237	18.559117
47.243138	1685.847403	18.564135
46.992620	1675.711624	18.569152
47.067553	1650.661658	18.574170
46.659832	1652.882211	18.579187
46.877346	1655.212131	18.584205
46.896804	1655.878174	18.589223
46.949474	1684.697681	18.594240
47.483513	1681.482148	18.599258
46.922189	1687.405452	18.604275
47.414871	1689.474396	18.609293
47.531052	1686.474614	18.614311
47.471889	1680.962473	18.619328
47.400583	1657.728720	18.624346
47.158761	1661.907280	18.629363
46.959925	1672.717427	18.634381
47.208950	1681.482851	18.639399
47.627369	1688.989961	18.644416
47.406667	1692.013987	18.649434
47.571704	1684.353711	18.654451
47.254789	1680.682820	18.659469
47.203632	1689.092580	18.664487
47.136129	1685.508470	18.669504
47.528527	1700.635503	18.674522
47.675476	1711.751002	18.679539
47.572840	1724.159449	18.684557
47.858039	1715.516631	18.689575
47.866809	1717.354333	18.694592
47.785084	1712.463839	18.699610
48.016653	1703.408519	18.704627
47.771299	1712.297702	18.709645
47.889334	1709.046780	18.714663
47.963075	1718.407698	18.719680
48.131735	1714.847667	18.724698
47.814386	1724.459126	18.729715
47.921456	1744.373085	18.734733
48.357508	1733.478142	18.739751
48.609763	1743.266398	18.744768
48.283269	1741.800156	18.749786
48.836322	1729.918899	18.754803
49.049343	1737.781365	18.759821
49.149859	1728.789843	18.764839
48.618704	1719.202603	18.769856
48.423384	1713.333828	18.774874
48.499758	1713.750717	18.779891
48.867678	1731.609858	18.784909
48.688596	1724.472396	18.789927
48.624446	1741.859891	18.794944
48.731308	1736.357853	18.799962
48.904627	1732.772213	18.804979
48.933146	1736.972956	18.809997
48.981756	1730.550482	18.815015
48.821323	1732.076603	18.820032
48.860767	1737.783527	18.825050
48.807676	1743.848092	18.830067
48.919160	1738.855558	18.835085
48.920086	1738.673893	18.840103
49.077679	1752.363496	18.845120
49.269230	1766.225264	18.850138
49.178991	1765.761948	18.855155
49.084428	1768.015452	18.860173
49.408262	1759.334487	18.865191
49.382599	1769.071576	18.870208
49.511400	1760.537841	18.875226
49.488019	1762.183399	18.880243
49.677961	1766.175744	18.885261
49.964623	1760.116430	18.890279
49.718463	1758.236365	18.895296
49.889930	1756.498898	18.900314
49.943313	1753.873300	18.905331
50.229280	1757.657424	18.910349
50.118560	1753.704284	18.915367
50.209957	1759.809052	18.920384
50.037514	1756.196061	18.925402
50.148148	1759.365286	18.930419
50.135157	1762.528538	18.935437
50.169071	1753.760257	18.940455
50.020358	1751.911916	18.945472
49.603608	1755.815337	18.950490
49.697829	1761.637303	18.955507
49.742276	1775.746768	18.960525
50.101254	1787.818217	18.965543
49.880593	1794.291892	18.970560
50.209398	1797.899763	18.975578
50.354246	1808.845199	18.980595
50.105543	1818.648908	18.985613
50.692799	1824.958094	18.990631
50.752897	1828.620310	18.995648
50.863999	1821.811052	19.000666
50.846705	1818.548660	19.005683
51.039595	1813.603572	19.010701
51.155004	1809.059218	19.015719
51.158640	1813.880860	19.020736
51.174342	1819.281216	19.025754
51.345168	1813.243316	19.030771
51.078265	1815.458255	19.035789
51.582117	1809.410511	19.040807
51.157728	1802.189070	19.045824
51.154150	1793.807163	19.050842
51.260003	1792.234898	19.055859
51.307777	1812.331178	19.060877
51.135623	1811.156617	19.065895
51.278007	1813.529760	19.070912
51.237520	1821.114037	19.075930
51.476386	1821.307771	19.080947
51.447740	1822.298644	19.085965
51.534581	1821.403342	19.090983
51.393673	1820.193499	19.096000
51.310770	1820.122280	19.101018
51.803772	1809.897528	19.106035
51.361101	1825.418669	19.111053
52.015635	1827.453190	19.116071
51.498744	1831.082422	19.121088
51.477149	1844.246458	19.126106
51.894843	1847.274069	19.131123
51.945062	1852.000323	19.136141
51.819343	1852.230577	19.141159
51.708996	1848.508087	19.146176
51.642965	1856.916156	19.151194
51.590479	1855.830145	19.156211
52.000815	1874.322022	19.161229
52.036736	1881.372295	19.166247
52.187235	1874.967730	19.171264
52.064371	1879.183441	19.176282
52.446423	1869.727768	19.181299
52.219884	1881.267704	19.186317
52.507409	1886.852219	19.191335
52.806542	1893.070261	19.196352
53.182806	1905.812941	19.201370
52.995529	1886.153134	19.206387
52.526279	1884.881059	19.211405
53.207695	1880.235708	19.216423
53.039273	1877.718204	19.221440
52.828298	1880.378346	19.226458
53.041927	1869.905745	19.231475
53.296093	1875.051429	19.236493
53.336885	1864.812427	19.241511
53.361788	1869.697771	19.246528
53.122704	1868.436637	19.251546
53.476306	1859.575294	19.256563
53.299415	1871.648118	19.261581
53.115655	1866.158061	19.266599
53.096526	1864.555635	19.271616
53.231556	1882.389908	19.276634
53.587339	1887.806008	19.281651
53.575345	1898.409450	19.286669
53.719552	1904.416232	19.291687
53.429372	1898.899915	19.296704
53.414386	1895.816661	19.301722
53.885441	1899.673826	19.306739
53.605207	1902.102901	19.311757
53.773488	1901.683066	19.316775
53.896762	1897.212545	19.321792
53.576056	1901.186160	19.326810
53.732357	1903.254136	19.331827
53.839831	1900.186899	19.336845
53.698857	1899.073924	19.341863
53.777670	1905.389201	19.346880
53.564821	1922.555507	19.351898
53.942506	1926.433806	19.356915
53.889151	1932.096860	19.361933
54.291062	1926.921780	19.366951
54.547495	1926.878616	19.371968
54.439884	1929.716740	19.376986
54.145498	1918.903981	19.382003
54.516629	1914.174791	19.387021
54.953206	1918.650944	19.392039
54.866434	1911.012861	19.397056
54.849070	1916.166918	19.402074
55.000978	1902.836784	19.407091
54.713300	1914.143493	19.412109
54.739985	1911.534258	19.417127
55.066805	1905.856637	19.422144
54.794681	1911.978113	19.427162
55.012899	1907.022746	19.432179
54.762281	1914.921477	19.437197
54.901237	1939.596592	19.442215
55.252052	1940.398383	19.447232
55.108004	1953.851650	19.452250
55.287798	1945.738657	19.457267
55.348100	1942.542080	19.462285
55.644536	1943.743404	19.467303
55.715065	1941.354236	19.472320
55.098723	1945.567943	19.477338
55.564950	1937.728330	19.482355
55.421038	1946.020648	19.487373
55.207760	1938.260521	19.492391
55.496663	1946.720399	19.497408
55.193075	1945.850683	19.502426
55.551660	1952.462941	19.507443
55.510455	1970.083008	19.512461
55.789375	1975.289451	19.517479
55.785571	1967.889512	19.522496
55.559665	1975.426114	19.527514
56.122651	1968.349137	19.532531
56.545789	1972.096409	19.537549
56.234648	1970.680275	19.542567
56.224715	1965.693917	19.547584
55.920412	1971.499236	19.552602
56.151678	1968.353668	19.557619
56.239909	1969.671016	19.562637
56.332229	1965.112463	19.567655
56.307535	1965.388398	19.572672
56.343040	1982.979971	19.577690
56.387132	1985.963380	19.582707
56.516891	2002.358341	19.587725
56.716742	1999.661914	19.592743
56.737644	1994.785237	19.597760
56.581229	1994.528562	19.602778
56.870091	1990.428105	19.607795
57.038071	1986.632664	19.612813
56.973189	1993.936523	19.617831
56.998963	1989.989847	19.622848
56.807512	1994.707571	19.627866
57.068777	1991.344228	19.632883
56.785046	1989.792667	19.637901
57.297257	1994.921320	19.642919
57.349663	1995.376977	19.647936
57.214995	1995.255963	19.652954
57.397982	1990.459780	19.657971
57.531105	1994.406013	19.662989
57.463547	2005.764431	19.668007
58.203601	2008.363529	19.673024
58.203907	2013.915825	19.678042
57.908465	1991.745734	19.683059
58.229774	1998.262814	19.688077
58.120017	1988.047967	19.693095
58.039418	1987.038035	19.698112
58.033675	1991.206527	19.703130
58.070824	1990.004731	19.708147
58.057028	1986.875187	19.713165
57.746514	1992.496907	19.718183
58.259870	1983.747101	19.723200
57.785445	1998.287502	19.728218
57.792385	1991.710231	19.733235
57.927679	1988.210985	19.738253
57.571255	1989.871139	19.743271
57.929736	2001.443166	19.748288
57.939157	2012.844305	19.753306
58.326097	2008.150178	19.758323
57.851369	2014.037888	19.763341
57.873106	2040.023986	19.768359
58.556403	2047.265355	19.773376
58.435477	2044.381757	19.778394
58.608731	2048.901912	19.783411
58.834565	2042.643047	19.788429
58.924195	2040.564019	19.793447
59.167382	2040.141182	19.798464
58.978761	2045.362837	19.803482
59.040074	2038.877026	19.808499
59.179592	2036.173218	19.813517
59.319572	2038.842519	19.818535
59.317740	2031.011443	19.823552
59.262762	2041.049831	19.828570
59.278114	2041.226763	19.833587
59.483477	2038.014747	19.838605
59.118646	2034.665022	19.843623
59.335590	2032.127493	19.848640
59.330925	2042.335628	19.853658
59.432225	2053.423759	19.858675
59.264915	2053.846998	19.863693
58.993831	2066.212931	19.868711
59.367031	2057.086269	19.873728
59.567602	2062.094728	19.878746
60.100883	2068.878689	19.883763
59.817290	2062.314185	19.888781
59.585753	2057.916261	19.893799
60.222230	2075.529333	19.898816
60.050145	2096.933143	19.903834
59.959663	2089.797254	19.908851
60.060325	2088.105754	19.913869
59.781381	2092.720380	19.918887
60.189992	2086.525845	19.923904
60.009625	2094.423253	19.928922
60.083051	2090.843239	19.933939
60.172541	2098.088785	19.938957
60.424520	2113.436778	19.943975
61.108785	2101.965093	19.948992
61.279536	2110.600851	19.954010
60.853134	2107.030137	19.959027
61.039227	2087.785266	19.964045
60.949435	2086.316996	19.969063
61.092347	2072.877614	19.974080
60.866549	2081.839254	19.979098
60.719497	2079.217251	19.984115
61.227651	2098.662447	19.989133
61.344657	2102.738260	19.994151
61.592005	2103.688921	19.999168
61.265312	2092.255900	20.004186
61.000963	2087.061117	20.009203
61.328393	2087.830307	20.014221
60.936648	2107.512092	20.019239
61.268970	2098.471166	20.024256
61.411273	2098.901964	20.029274
61.551496	2105.681271	20.034291
61.546024	2100.649217	20.039309
61.362050	2107.455755	20.044327
61.770307	2109.315184	20.049344
61.770482	2127.374461	20.054362
61.871327	2133.079271	20.059379
62.100348	2134.626076	20.064397
62.046597	2144.242999	20.069415
61.894202	2129.575665	20.074432
61.840458	2135.344780	20.079450
61.915351	2135.776898	20.084467
62.062445	2136.143087	20.089485
61.788640	2139.040849	20.094503
62.212930	2126.998666	20.099520
62.355479	2134.570615	20.104538
62.377755	2155.744698	20.109555
62.482603	2162.738786	20.114573
62.611650	2163.436464	20.119591
62.830897	2165.089687	20.124608
62.623741	2157.629625	20.129626
62.441570	2157.067869	20.134643
62.772479	2158.964190	20.139661
62.659911	2166.908287	20.144679
62.452715	2160.148334	20.149696
62.584669	2156.760663	20.154714
62.672288	2163.486800	20.159731
63.319437	2169.104264	20.164749
62.982683	2181.860735	20.169767
63.042550	2180.445551	20.174784
63.717794	2178.502754	20.179802
63.441257	2182.657083	20.184819
63.670231	2184.277928	20.189837
63.092604	2185.253477	20.194855
63.551887	2188.928061	20.199872
63.574972	2182.183745	20.204890
63.339192	2176.694227	20.209907
63.593626	2172.826431	20.214925
63.698117	2180.041881	20.219943
63.482438	2185.174900	20.224960
63.421201	2192.705425	20.229978
63.814775	2200.835246	20.234995
64.290014	2204.313368	20.240013
64.131778	2208.882920	20.245031
64.215793	2203.486620	20.250048
64.129483	2206.330986	20.255066
64.294595	2209.928430	20.260083
64.615482	2204.476557	20.265101
64.290810	2208.515505	20.270119
64.228335	2206.573179	20.275136
64.774035	2200.796107	20.280154
64.398842	2201.460532	20.285171
64.626231	2203.087163	20.290189
64.411448	2212.774262	20.295207
64.647772	2203.900150	20.300224
64.936891	2232.676191	20.305242
64.978239	2235.665631	20.310259
65.157708	2238.291182	20.315277
64.965969	2234.320309	20.320295
65.276865	2236.336625	20.325312
65.007858	2230.036913	20.330330
65.093837	2233.655017	20.335347
65.306116	2236.759269	20.340365
65.193926	2236.934443	20.345383
65.466788	2233.282404	20.350400
65.656884	2232.114220	20.355418
65.314911	2234.231440	20.360435
65.606844	2231.892866	20.365453
65.547431	2234.901943	20.370471
65.297281	2236.154473	20.375488
65.604312	2236.195561	20.380506
65.404427	2233.857041	20.385523
65.734215	2244.493475	20.390541
65.467664	2249.018607	20.395559
65.694954	2251.116197	20.400576
66.368384	2246.343352	20.405594
66.085861	2258.762979	20.410611
66.310209	2242.622072	20.415629
66.395544	2247.376683	20.420647
66.250325	2249.642878	20.425664
66.601425	2246.053024	20.430682
66.268563	2252.584318	20.435699
66.743614	2242.290306	20.440717
66.409523	2250.523643	20.445735
66.312495	2247.067319	20.450752
66.438448	2248.141967	20.455770
66.818142	2267.560966	20.460787
66.755026	2262.593869	20.465805
66.754551	2273.485399	20.470823
66.949245	2277.821997	20.475840
67.058809	2274.156993	20.480858
66.814493	2275.838513	20.485875
67.267343	2275.368701	20.490893
66.979923	2274.426497	20.495911
66.940501	2274.477368	20.500928
67.076651	2276.407095	20.505946
66.781461	2288.836006	20.510963
67.408920	2298.735510	20.515981
67.462345	2307.082782	20.520999
67.297697	2316.887354	20.526016
67.519558	2316.505968	20.531034
67.362512	2314.792474	20.536051
67.633958	2315.208225	20.541069
67.252028	2326.230554	20.546087
67.979467	2336.499616	20.551104
68.653005	2328.378955	20.556122
68.483151	2337.758381	20.561139
69.139533	2320.788875	20.566157
68.953438	2302.825063	20.571175
68.491030	2293.359559	20.576192
68.607950	2288.780550	20.581210
68.877955	2281.633173	20.586227
68.911242	2282.290572	20.591245
68.971200	2279.941361	20.596263
68.578001	2280.699441	20.601280
68.850508	2274.235996	20.606298
68.790349	2281.249763	20.611315
68.940334	2273.088948	20.616333
69.012375	2276.567698	20.621351
68.599386	2271.506227	20.626368
69.004377	2276.901427	20.631386
68.803793	2285.047316	20.636403
69.330196	2283.594665	20.641421
69.317102	2283.874917	20.646439
68.892193	2284.884141	20.651456
69.182333	2283.194787	20.656474
69.196070	2290.614853	20.661491
69.304938	2282.573698	20.666509
69.427695	2281.939970	20.671527
69.298103	2283.223024	20.676544
69.335004	2273.289981	20.681562
69.282269	2293.831342	20.686579
69.709253	2311.463273	20.691597
69.794740	2307.677172	20.696615
69.784256	2318.229451	20.701632
69.693186	2312.775715	20.706650
69.767375	2317.955947	20.711667
69.735642	2309.393916	20.716685
69.830854	2307.177261	20.721703
69.913773	2327.743449	20.726720
70.106472	2332.870292	20.731738
70.014360	2342.101725	20.736755
69.916689	2338.656517	20.741773
70.287080	2332.064438	20.746791
70.112190	2349.231003	20.751808
70.292463	2359.437958	20.756826
70.225997	2372.331739	20.761843
70.649156	2375.940109	20.766861
70.444727	2376.002731	20.771879
70.861369	2375.739944	20.776896
70.963379	2369.300177	20.781914
70.930640	2379.204240	20.786931
71.541660	2392.136244	20.791949
71.130494	2378.228904	20.796967
70.854302	2393.991397	20.801984
71.085101	2394.781895	20.807002
71.281800	2398.963827	20.812019
71.358458	2405.039873	20.817037
71.182062	2402.269672	20.822055
71.652188	2394.821749	20.827072
71.920467	2390.295516	20.832090
71.943889	2393.912569	20.837107
71.950821	2389.426416	20.842125
71.562968	2394.542556	20.847143
71.614965	2398.342931	20.852160
72.012294	2415.997389	20.857178
71.733344	2425.866513	20.862195
72.085432	2434.064209	20.867213
72.513016	2430.815591	20.872231
72.169268	2432.244839	20.877248
72.193363	2431.965084	20.882266
72.125962	2438.440705	20.887283
72.065591	2428.191902	20.892301
72.385334	2426.732929	20.897319
72.501862	2444.332393	20.902336
72.350682	2443.795239	20.907354
72.725149	2456.449688	20.912371
73.125628	2457.826162	20.917389
72.716314	2448.140403	20.922407
72.625600	2449.818446	20.927424
72.870679	2450.234784	20.932442
72.565742	2450.722579	20.937459
72.533175	2457.169397	20.942477
72.833483	2471.732163	20.947495
73.055574	2479.006342	20.952512
73.113874	2472.936293	20.957530
73.066600	2477.530213	20.962547
73.332354	2477.151537	20.967565
73.156058	2483.337133	20.972583
73.371329	2498.387022	20.977600
73.197413	2499.048452	20.982618
73.704157	2509.817749	20.987635
73.620044	2502.452983	20.992653
73.818262	2499.862675	20.997671
73.543315	2506.858239	21.002688
74.285762	2519.685914	21.007706
74.539363	2533.249487	21.012723
74.936483	2529.811550	21.017741
74.871836	2512.132240	21.022759
74.613754	2501.884996	21.027776
74.414819	2497.612089	21.032794
74.602816	2499.799929	21.037811
74.986797	2493.892183	21.042829
74.975953	2480.372102	21.047847
74.558643	2498.460066	21.052864
74.848325	2498.597847	21.057882
74.848361	2493.050463	21.062899
74.616355	2494.125857	21.067917
74.990451	2490.406789	21.072935
75.019801	2509.660130	21.077952
75.081396	2515.543492	21.082970
75.113815	2525.350635	21.087987
75.428067	2527.584562	21.093005
75.510429	2520.225110	21.098023
75.179524	2525.843427	21.103040
75.351857	2523.472551	21.108058
75.376309	2519.614960	21.113075
75.324973	2523.328339	21.118093
75.308811	2523.462640	21.123111
75.226711	2544.374779	21.128128
75.258395	2550.980728	21.133146
75.169600	2558.379122	21.138163
75.633813	2568.380814	21.143181
76.000439	2576.782428	21.148199
76.170618	2594.620150	21.153216
76.026832	2586.071666	21.158234
76.099703	2581.744261	21.163251
76.230913	2583.816630	21.168269
76.236070	2585.375083	21.173287
76.541614	2602.565877	21.178304
76.503056	2602.262996	21.183322
76.672673	2605.768405	21.188339
76.498512	2612.869594	21.193357
76.858896	2603.236852	21.198375
76.916219	2601.686609	21.203392
76.972293	2599.152157	21.208410
77.541287	2592.190430	21.213427
77.341424	2599.069207	21.218445
77.823642	2588.192539	21.223463
77.415024	2599.815013	21.228480
77.594702	2595.749658	21.233498
77.713171	2593.310039	21.238515
77.584559	2597.254832	21.243533
78.050001	2590.697540	21.248551
77.654070	2588.530395	21.253568
77.374225	2587.593173	21.258586
78.020082	2590.778308	21.263603
77.480503	2598.451675	21.268621
77.716267	2603.242033	21.273639
77.696281	2601.654641	21.278656
77.614935	2596.646461	21.283674
77.863132	2604.178474	21.288691
77.556606	2625.123684	21.293709
77.869670	2632.522521	21.298727
77.838451	2641.721640	21.303744
78.027764	2631.051091	21.308762
78.463573	2640.620615	21.313779
78.268135	2657.737486	21.318797
78.980865	2655.517296	21.323815
79.324989	2666.212200	21.328832
79.261525	2658.247651	21.333850
79.259602	2658.385024	21.338867
79.038323	2662.861560	21.343885
79.202282	2654.641449	21.348903
79.182669	2651.530882	21.353920
79.613117	2657.877140	21.358938
79.814499	2652.102233	21.363955
79.260183	2655.720739	21.368973
79.046167	2651.588982	21.373991
79.165485	2649.943839	21.379008
79.459968	2654.646967	21.384026
79.436559	2656.168586	21.389043
79.236311	2658.032388	21.394061
79.700305	2672.378268	21.399079
79.546702	2687.650663	21.404096
79.687680	2691.871366	21.409114
80.012430	2678.692077	21.414131
79.929961	2683.696102	21.419149
79.751368	2678.006017	21.424167
79.871464	2695.642166	21.429184
79.847374	2714.660781	21.434202
79.991876	2710.185604	21.439219
79.965223	2722.217572	21.444237
80.087203	2735.881065	21.449255
80.333631	2748.017446	21.454272
80.762554	2750.764128	21.459290
81.115422	2750.615439	21.464307
81.231219	2745.033944	21.469325
81.444741	2739.091539	21.474343
80.911380	2731.891889	21.479360
81.276542	2736.454555	21.484378
81.392642	2738.568125	21.489395
81.420597	2737.236328	21.494413
81.549929	2732.090393	21.499431
81.400882	2741.735833	21.504448
81.461791	2733.954684	21.509466
81.676406	2740.264737	21.514483
81.383892	2733.096249	21.519501
81.818822	2735.378034	21.524519
81.368908	2736.341168	21.529536
81.498029	2756.770840	21.534554
82.145929	2759.441392	21.539571
81.682405	2768.875359	21.544589
82.083220	2763.860856	21.549607
82.134780	2777.439590	21.554624
81.793827	2780.198557	21.559642
82.345939	2777.419163	21.564659
82.227951	2796.753244	21.569677
82.138935	2800.806281	21.574695
82.310036	2803.190010	21.579712
82.377336	2807.786436	21.584730
82.890972	2796.966455	21.589747
82.252330	2804.447416	21.594765
82.592190	2821.454581	21.599783
82.760742	2839.849658	21.604800
82.483310	2837.321153	21.609818
83.483877	2829.986853	21.614835
82.998136	2838.388252	21.619853
83.160589	2851.638531	21.624871
83.262143	2862.684664	21.629888
83.062761	2860.512136	21.634906
83.615537	2858.971434	21.639923
83.651126	2872.609692	21.644941
83.778904	2861.986552	21.649959
83.842611	2857.642529	21.654976
83.838876	2853.332909	21.659994
83.689330	2856.378033	21.665011
84.252037	2872.404348	21.670029
84.164498	2883.648300	21.675047
84.073661	2888.060008	21.680064
84.117298	2884.070668	21.685082
84.401226	2874.247681	21.690099
84.601331	2879.687668	21.695117
84.311820	2875.474288	21.700135
84.630039	2869.325661	21.705152
84.145321	2885.604014	21.710170
84.696647	2895.217682	21.715187
84.621506	2906.220895	21.720205
84.888363	2901.001712	21.725223
84.815179	2907.441502	21.730240
84.727894	2908.229857	21.735258
85.078732	2909.729867	21.740275
85.054830	2936.454943	21.745293
85.163351	2936.147317	21.750311
85.600565	2931.786493	21.755328
85.575567	2941.948689	21.760346
85.867341	2931.432059	21.765363
85.779994	2932.632317	21.770381
85.557448	2921.910109	21.775399
85.772167	2932.546263	21.780416
85.630398	2936.914738	21.785434
85.514725	2931.316944	21.790451
85.728403	2958.237593	21.795469
85.889951	2965.989401	21.800487
86.350651	2964.253410	21.805504
86.010599	2967.232770	21.810522
86.356840	2963.232485	21.815539
86.293335	2978.825214	21.820557
86.281065	2989.845272	21.825575
86.484046	2994.927255	21.830592
86.542331	2998.480192	21.835610
87.436613	2978.130735	21.840627
87.279981	2975.761848	21.845645
87.479678	2970.474612	21.850663
87.980366	2972.582136	21.855680
88.073470	2974.373631	21.860698
87.770661	2952.892160	21.865715
87.858703	2943.810726	21.870733
87.729420	2936.291263	21.875751
87.422985	2940.287103	21.880768
87.336752	2943.156789	21.885786
87.847848	2932.849851	21.890803
87.626449	2940.847648	21.895821
87.798360	2956.240123	21.900839
87.914906	2956.565104	21.905856
87.850127	2959.540586	21.910874
88.213368	2962.239500	21.915891
88.181895	2965.106891	21.920909
88.232568	2967.084436	21.925927
88.339909	2972.404111	21.930944
88.201537	2962.829880	21.935962
88.289833	2976.222925	21.940979
88.358938	2988.000838	21.945997
88.342293	2995.417782	21.951015
88.241502	2986.453752	21.956032
88.763028	2999.034602	21.961050
88.613919	3018.836588	21.966067
88.965154	3023.904190	21.971085
89.128714	3023.176807	21.976103
89.015721	3031.419898	21.981120
88.838739	3030.946999	21.986138
89.565214	3034.345226	21.991155
89.251459	3051.024447	21.996173
89.710673	3049.476142	22.001191
89.841080	3044.307870	22.006208
90.043514	3048.786692	22.011226
90.220966	3039.801708	22.016243
90.174077	3049.719644	22.021261
90.219313	3046.347437	22.026279
90.679504	3040.284663	22.031296
90.344933	3042.299910	22.036314
90.455688	3031.738641	22.041331
89.984060	3032.474758	22.046349
90.219947	3040.941565	22.051367
90.569226	3042.903367	22.056384
90.347341	3042.360197	22.061402
90.334783	3043.584657	22.066419
90.386403	3044.606737	22.071437
90.623230	3064.119736	22.076455
90.858486	3070.507502	22.081472
90.447054	3079.151459	22.086490
90.724651	3071.262903	22.091507
90.825384	3081.320939	22.096525
90.612258	3095.962857	22.101543
90.916949	3096.421762	22.106560
90.861994	3099.536561	22.111578
91.390606	3122.016768	22.116595
91.284150	3134.580951	22.121613
91.259582	3138.815191	22.126631
91.658127	3134.076611	22.131648
91.492794	3143.925917	22.136666
91.756786	3158.092313	22.141683
92.063045	3158.096526	22.146701
91.830264	3161.750591	22.151719
92.332113	3162.437170	22.156736
92.346777	3168.457197	22.161754
92.202831	3152.295804	22.166771
92.444986	3177.009122	22.171789
92.639442	3187.345709	22.176807
93.513300	3177.207180	22.181824
93.313401	3184.432747	22.186842
93.521619	3184.790059	22.191859
93.473270	3158.072246	22.196877
93.615741	3146.299698	22.201895
93.638495	3140.862387	22.206912
93.661992	3138.935134	22.211930
93.612716	3135.523194	22.216947
94.013443	3134.200701	22.221965
93.680461	3132.520427	22.226983
94.031463	3131.881403	22.232000
93.599757	3139.579852	22.237018
93.754944	3133.000709	22.242035
93.882168	3127.703794	22.247053
93.913802	3136.308052	22.252071
94.109549	3143.413006	22.257088
94.391756	3164.838438	22.262106
94.675442	3158.604262	22.267123
94.266776	3167.999920	22.272141
94.210530	3179.463962	22.277159
94.687991	3164.197811	22.282176
94.561681	3167.672961	22.287194
94.379019	3167.643644	22.292211
94.429994	3172.683226	22.297229
94.423816	3188.060780	22.302247
94.540685	3190.621619	22.307264
94.853986	3202.025474	22.312282
95.323793	3190.524405	22.317299
95.367220	3195.808647	22.322317
95.061870	3196.382377	22.327335
95.166856	3200.640103	22.332352
95.451322	3222.641727	22.337370
95.030218	3221.304968	22.342387
95.884345	3223.015642	22.347405
95.825275	3219.413195	22.352423
95.696065	3219.288870	22.357440
96.159685	3230.753609	22.362458
96.102087	3237.071151	22.367475
96.473385	3240.860307	22.372493
96.547087	3243.440368	22.377511
96.891430	3240.430317	22.382528
96.933098	3233.353160	22.387546
96.669560	3214.213922	22.392563
97.062111	3203.709763	22.397581
96.898777	3206.205231	22.402599
97.124684	3201.191438	22.407616
96.621663	3205.340756	22.412634
96.801278	3226.501122	22.417651
96.903314	3225.958332	22.422669
96.882844	3231.976530	22.427687
97.188211	3226.311962	22.432704
97.452663	3235.637942	22.437722
97.332002	3250.215322	22.442739
97.872475	3246.281690	22.447757
97.578049	3258.433219	22.452775
97.698346	3260.919449	22.457792
97.622180	3271.548997	22.462810
97.697777	3256.869086	22.467827
98.066473	3259.330847	22.472845
98.260247	3284.299926	22.477863
98.129781	3291.350612	22.482880
98.437162	3294.468700	22.487898
98.237329	3297.748563	22.492915
98.740530	3286.183419	22.497933
98.350881	3290.412557	22.502951
98.926094	3287.884291	22.507968
98.759047	3295.043634	22.512986
98.571536	3303.474483	22.518003
99.093591	3308.908257	22.523021
99.173634	3319.147985	22.528039
99.666468	3316.100649	22.533056
99.161942	3329.554672	22.538074
99.107356	3316.598187	22.543091
99.577715	3312.272534	22.548109
99.777556	3321.177263	22.553127
99.529353	3319.565129	22.558144
99.686442	3333.133340	22.563162
99.823624	3343.131741	22.568179
99.899791	3346.935290	22.573197
99.761246	3354.874200	22.578215
99.757833	3348.475735	22.583232
99.966256	3357.169518	22.588250
100.170274	3381.009972	22.593267
100.258326	3366.485340	22.598285
100.291819	3378.671315	22.603303
100.302099	3372.149993	22.608320
100.600882	3376.629719	22.613338
100.854679	3394.275235	22.618355
101.113117	3395.936050	22.623373
101.069491	3402.504863	22.628391
101.155465	3397.844993	22.633408
100.776394	3393.551528	22.638426
100.936957	3402.337812	22.643443
101.315687	3403.835453	22.648461
101.569090	3426.714539	22.653479
101.307693	3425.104657	22.658496
101.775298	3425.919983	22.663514
101.877806	3438.895931	22.668531
102.007970	3423.716635	22.673549
102.266147	3434.888323	22.678567
102.297209	3431.413716	22.683584
102.111286	3431.516483	22.688602
101.685148	3438.100481	22.693619
102.329020	3453.226663	22.698637
102.488021	3464.062538	22.703655
102.233487	3459.405894	22.708672
102.318755	3465.888842	22.713690
102.298097	3483.701222	22.718707
102.628828	3487.424148	22.723725
102.368403	3488.015388	22.728743
102.990197	3509.898153	22.733760
103.223409	3515.412233	22.738778
103.199184	3517.524763	22.743795
103.503433	3517.727793	22.748813
103.753795	3508.129117	22.753831
103.467807	3507.641024	22.758848
103.817874	3510.527376	22.763866
104.088028	3511.550614	22.768883
103.824043	3520.889385	22.773901
104.086797	3528.968296	22.778919
103.933202	3536.362505	22.783936
104.084867	3536.573580	22.788954
104.046351	3541.794015	22.793971
104.269215	3535.649664	22.798989
104.495587	3549.610216	22.804007
104.617312	3573.920294	22.809024
104.927063	3567.709843	22.814042
104.558231	3572.351332	22.819059
104.744700	3566.354188	22.824077
104.738123	3575.302324	22.829095
104.858038	3584.448517	22.834112
105.463292	3590.797481	22.839130
105.151322	3601.373165	22.844147
105.243533	3588.065229	22.849165
105.379365	3605.551635	22.854183
105.367114	3606.949355	22.859200
105.624624	3610.984935	22.864218
105.932547	3620.496652	22.869235
105.849968	3627.728299	22.874253
106.020363	3631.377935	22.879271
106.213447	3637.903115	22.884288
106.708690	3622.922522	22.889306
106.028706	3631.514368	22.894323
106.327968	3628.728561	22.899341
106.667872	3633.752625	22.904359
106.843228	3646.355538	22.909376
106.944166	3647.325097	22.914394
106.820248	3650.680228	22.919411
107.303904	3650.222431	22.924429
107.477831	3650.120955	22.929447
107.156877	3647.123284	22.934464
107.463124	3642.071164	22.939482
107.500276	3656.709286	22.944499
107.387246	3637.012895	22.949517
107.296647	3658.152433	22.954535
107.439329	3673.737280	22.959552
107.674949	3679.928335	22.964570
107.152198	3691.221481	22.969587
107.322869	3685.821633	22.974605
107.626079	3699.439930	22.979623
107.607896	3704.389151	22.984640
108.226546	3712.040125	22.989658
107.941534	3741.237908	22.994675
108.270323	3736.888368	22.999693
108.736694	3739.122385	23.004711
108.690475	3733.788056	23.009728
109.192295	3739.551515	23.014746
109.128877	3755.480514	23.019763
108.913318	3757.147017	23.024781
109.489343	3761.757323	23.029799
109.328254	3764.992047	23.034816
109.729732	3756.352598	23.039834
109.759955	3759.586028	23.044851
109.759906	3749.050364	23.049869
109.809593	3748.375551	23.054887
109.679478	3754.081954	23.059904
109.655724	3756.919812	23.064922
109.994373	3769.610607	23.069939
110.002947	3786.781150	23.074957
110.448474	3784.309697	23.079975
110.662941	3789.301759	23.084992
111.088013	3782.812334	23.090010
110.600861	3786.197472	23.095027
110.515814	3789.970484	23.100045
110.702390	3784.139422	23.105063
110.654030	3795.000834	23.110080
111.186320	3797.293656	23.115098
111.326017	3798.220351	23.120115
111.890855	3789.094497	23.125133
112.084842	3790.745139	23.130151
111.840292	3797.000442	23.135168
112.218620	3788.111339	23.140186
111.858159	3768.374503	23.145203
111.980178	3759.951507	23.150221
112.275614	3766.337117	23.155239
111.896689	3768.979896	23.160256
112.244734	3778.793568	23.165274
112.508590	3783.143933	23.170291
112.558393	3781.813816	23.175309
112.643597	3782.804984	23.180327
112.808606	3786.791885	23.185344
112.784612	3780.718900	23.190362
112.723805	3783.416622	23.195379
112.853412	3789.239971	23.200397
112.817608	3776.598866	23.205415
112.727478	3781.195787	23.210432
113.290205	3791.425534	23.215450
112.829010	3811.433234	23.220467
113.299448	3818.715869	23.225485
113.389289	3810.923717	23.230503
113.215828	3817.548828	23.235520
113.904220	3827.002533	23.240538
113.916352	3839.741485	23.245555
113.895807	3846.829493	23.250573
113.897398	3847.558551	23.255591
114.246515	3838.967414	23.260608
114.205225	3828.242654	23.265626
113.924563	3846.837211	23.270643
114.307487	3860.571150	23.275661
114.924724	3865.762761	23.280679
114.917323	3868.444253	23.285696
114.949147	3862.219112	23.290714
114.818796	3871.794302	23.295731
114.778928	3870.586664	23.300749
114.943054	3879.912113	23.305767
115.585499	3896.797687	23.310784
115.866596	3894.539493	23.315802
115.710131	3904.028604	23.320819
115.740959	3899.792321	23.325837
115.930855	3897.414293	23.330855
115.756432	3897.657647	23.335872
115.616358	3905.016630	23.340890
115.699083	3921.118431	23.345907
116.349555	3927.766161	23.350925
116.733255	3928.660485	23.355943
116.445939	3933.668518	23.360960
116.514283	3921.515085	23.365978
116.218284	3927.687897	23.370995
116.686533	3943.898479	23.376013
117.114040	3946.052553	23.381031
116.418270	3957.395238	23.386048
116.930468	3954.342890	23.391066
117.144636	3977.548484	23.396083
116.816294	3986.036130	23.401101
117.241608	3984.798357	23.406119
117.565324	3974.571701	23.411136
117.948149	3975.516586	23.416154
117.991631	3967.617313	23.421171
117.935430	3975.325038	23.426189
118.920611	3979.147757	23.431207
117.992814	3977.963949	23.436224
118.449644	3984.781157	23.441242
118.713428	3991.013188	23.446259
118.808239	3999.039221	23.451277
119.028041	3997.882359	23.456295
118.820923	4006.727287	23.461312
118.687323	3999.635727	23.466330
118.641217	3997.005939	23.471347
118.801453	3997.679453	23.476365
118.839583	4001.566868	23.481383
118.828142	4013.249091	23.486400
118.504549	4023.170180	23.491418
118.940838	4040.325959	23.496435
118.809003	4066.696551	23.501453
119.267545	4063.888877	23.506471
119.021071	4093.030295	23.511488
119.773665	4099.741717	23.516506
119.769957	4106.260660	23.521523
119.530272	4131.670056	23.526541
120.097062	4130.342647	23.531559
119.687911	4137.183145	23.536576
119.888282	4149.959386	23.541594
120.277663	4162.724501	23.546611
120.378475	4172.531972	23.551629
120.569740	4185.197173	23.556647
120.663148	4192.791143	23.561664
120.804038	4196.239613	23.566682
120.824193	4208.974336	23.571699
120.970541	4224.778057	23.576717
121.681834	4222.449220	23.581735
121.671452	4230.446146	23.586752
121.873547	4223.185882	23.591770
122.702524	4231.068847	23.596787
122.921857	4227.591720	23.601805
122.696696	4211.161982	23.606823
122.827464	4207.562207	23.611840
122.872827	4204.170041	23.616858
122.798191	4214.705446	23.621875
122.695063	4211.326133	23.626893
122.840893	4214.806053	23.631911
122.800476	4211.069436	23.636928
122.841013	4232.258146	23.641946
123.180982	4236.914575	23.646963
123.053317	4239.054386	23.651981
123.148782	4243.054112	23.656999
123.591492	4243.305880	23.662016
123.615134	4235.887961	23.667034
123.873829	4254.321223	23.672051
123.672089	4269.559290	23.677069
123.942106	4271.156781	23.682087
123.778276	4274.685861	23.687104
123.735048	4279.044113	23.692122
123.608674	4281.946127	23.697139
123.740939	4297.505809	23.702157
124.481193	4300.401033	23.707175
124.747444	4304.509331	23.712192
124.938970	4309.269992	23.717210
125.227607	4315.438820	23.722227
125.016963	4326.735619	23.727245
124.899413	4324.900137	23.732263
124.945016	4333.776747	23.737280
124.911724	4338.591710	23.742298
125.123632	4338.853117	23.747315
125.186491	4352.124884	23.752333
126.505525	4324.112116	23.757351
126.489042	4328.561886	23.762368
126.621861	4333.851664	23.767386
126.983663	4323.988440	23.772403
127.161232	4323.996604	23.777421
126.981547	4309.810001	23.782439
126.771296	4288.849572	23.787456
127.219274	4293.763958	23.792474
127.380928	4288.305592	23.797491
126.880816	4283.753811	23.802509
127.211584	4277.580438	23.807527
127.372847	4286.144986	23.812544
127.077796	4297.728752	23.817562
127.185437	4305.351053	23.822579
127.159511	4313.075018	23.827597
127.421482	4320.635427	23.832615
127.411190	4324.819493	23.837632
127.599920	4346.932829	23.842650
127.562930	4346.316169	23.847667
127.718848	4356.584520	23.852685
128.078143	4366.193425	23.857703
128.040372	4384.188545	23.862720
128.230940	4384.809619	23.867738
128.517081	4390.610294	23.872755
128.411319	4421.439711	23.877773
128.304634	4423.764981	23.882791
128.155489	4425.025564	23.887808
128.877146	4445.092779	23.892826
129.330473	4436.795359	23.897843
129.064125	4450.137822	23.902861
129.621249	4450.550349	23.907879
129.604121	4476.603446	23.912896
129.954439	4479.991660	23.917914
129.877024	4479.381925	23.922931
129.888960	4470.194516	23.927949
130.161640	4466.653845	23.932967
130.750230	4467.205903	23.937984
130.200069	4474.671682	23.943002
130.302785	4485.760499	23.948019
130.082813	4498.231017	23.953037
130.467020	4495.366702	23.958055
130.469433	4502.525893	23.963072
130.538552	4531.421044	23.968090
130.671374	4528.076040	23.973107
130.693658	4539.028244	23.978125
131.324010	4553.381199	23.983143
131.435892	4549.785373	23.988160
131.217437	4562.673130	23.993178
131.492343	4557.680441	23.998195
131.679663	4575.701777	24.003213
131.787389	4587.678263	24.008231
132.206524	4592.821378	24.013248
131.993366	4591.285804	24.018266
132.139515	4590.456582	24.023283
131.951513	4625.800274	24.028301
132.038439	4624.678749	24.033319
132.149779	4636.455379	24.038336
132.256132	4658.825865	24.043354
132.473622	4651.924295	24.048371
132.548339	4681.932486	24.053389
132.953223	4683.566761	24.058407
133.057084	4684.769815	24.063424
133.276568	4715.303815	24.068442
133.598021	4709.190946	24.073459
133.857023	4720.946263	24.078477
133.923662	4719.061044	24.083495
134.085865	4735.646265	24.088512
133.986685	4751.861222	24.093530
134.500244	4740.911553	24.098547
134.636511	4749.302629	24.103565
134.838115	4743.287482	24.108583
135.162592	4753.225527	24.113600
135.122691	4768.049594	24.118618
135.474183	4768.079142	24.123635
135.434736	4780.136925	24.128653
135.171401	4780.103315	24.133671
135.344912	4779.077995	24.138688
135.290925	4779.266057	24.143706
135.911975	4781.034994	24.148723
136.071068	4794.341044	24.153741
136.216435	4797.421047	24.158759
136.104090	4797.281212	24.163776
136.169457	4803.560971	24.168794
136.055153	4793.438022	24.173811
136.479943	4802.821726	24.178829
136.362821	4822.073067	24.183847
136.709499	4829.717656	24.188864
136.751651	4837.272675	24.193882
137.541623	4830.327237	24.198899
136.986106	4842.035602	24.203917
136.837337	4858.065406	24.208935
137.659512	4854.938487	24.213952
137.677335	4864.335281	24.218970
138.045045	4853.230953	24.223987
137.878946	4850.742892	24.229005
138.008921	4867.711061	24.234023
138.302810	4871.233484	24.239040
138.050415	4889.957528	24.244058
138.265840	4892.112650	24.249075
138.500113	4882.660831	24.254093
138.484407	4880.814914	24.259111
138.764298	4882.199685	24.264128
138.637151	4894.570322	24.269146
139.087976	4897.938248	24.274163
139.285799	4901.819775	24.279181
139.139788	4909.189692	24.284199
139.544859	4905.767220	24.289216
139.645150	4906.788167	24.294234
139.695032	4913.825984	24.299251
140.071554	4931.593173	24.304269
140.143784	4938.991067	24.309287
139.860328	4932.654145	24.314304
139.976600	4934.887708	24.319322
140.380034	4945.781155	24.324339
140.428826	4964.864025	24.329357
140.339738	4964.823385	24.334375
140.899520	4966.542197	24.339392
140.689202	4971.560196	24.344410
140.627883	4986.693750	24.349427
141.031177	4998.441079	24.354445
140.814046	5001.309159	24.359463
141.235756	5016.017305	24.364480
141.275111	5024.933181	24.369498
141.587359	5025.753181	24.374515
141.464565	5053.594424	24.379533
141.558375	5055.961030	24.384551
142.016243	5061.143344	24.389568
141.829413	5076.467059	24.394586
142.663684	5078.395608	24.399603
142.740427	5077.358502	24.404621
142.686371	5082.764846	24.409639
143.369709	5085.350188	24.414656
143.421626	5112.973334	24.419674
143.714862	5106.144438	24.424691
143.842041	5101.131221	24.429709
143.869123	5099.539447	24.434727
144.287198	5097.539589	24.439744
144.260635	5109.422915	24.444762
144.523392	5101.602064	24.449779
144.490692	5105.193915	24.454797
144.077897	5100.676547	24.459815
144.573694	5088.699422	24.464832
144.277934	5093.317794	24.469850
144.537612	5091.761764	24.474867
144.907639	5102.275092	24.479885
144.998109	5120.579881	24.484903
145.308645	5118.566949	24.489920
145.286977	5124.634120	24.494938
145.611254	5125.949867	24.499955
145.150710	5117.815058	24.504973
144.939494	5131.862263	24.509991
145.431406	5138.728310	24.515008
145.093032	5154.339583	24.520026
145.345574	5168.714545	24.525043
145.988605	5175.775250	24.530061
146.132089	5180.921703	24.535079
146.130453	5180.303676	24.540096
146.285258	5206.037847	24.545114
146.654574	5204.202293	24.550131
146.667731	5210.116233	24.555149
146.587073	5223.683503	24.560167
147.034079	5232.390984	24.565184
147.278356	5248.099386	24.570202
147.401297	5248.870720	24.575219
147.546274	5246.960194	24.580237
147.342139	5264.027021	24.585255
147.656784	5276.745201	24.590272
148.159138	5282.833663	24.595290
147.789404	5281.024758	24.600307
148.240352	5293.359619	24.605325
148.212405	5309.899271	24.610343
148.456382	5305.434668	24.615360
148.447722	5322.975312	24.620378
148.769359	5338.535061	24.625395
148.722681	5339.956953	24.630413
148.589898	5348.222755	24.635431
149.189107	5362.049318	24.640448
149.378901	5371.876149	24.645466
149.487060	5374.738155	24.650483
149.730969	5386.051517	24.655501
149.746010	5400.625726	24.660519
150.352106	5399.226107	24.665536
150.038943	5402.529765	24.670554
150.090579	5414.592107	24.675571
150.388554	5421.868822	24.680589
150.363382	5434.523291	24.685607
150.186779	5436.098218	24.690624
150.886492	5447.821062	24.695642
151.043529	5460.905111	24.700659
150.808403	5461.273892	24.705677
151.261237	5482.117117	24.710695
151.504065	5485.316817	24.715712
151.465834	5486.412748	24.720730
151.411908	5506.811191	24.725747
151.571198	5511.204379	24.730765
151.557916	5523.434682	24.735783
151.465561	5540.169144	24.740800
152.117781	5548.536000	24.745818
152.817280	5567.311912	24.750835
153.256150	5570.781283	24.755853
153.510339	5579.161250	24.760871
153.748681	5570.292004	24.765888
154.097683	5566.794722	24.770906
153.643069	5572.028865	24.775923
153.882128	5569.750865	24.780941
153.755379	5575.744849	24.785959
154.252866	5574.683635	24.790976
154.152752	5573.745343	24.795994
153.804686	5570.430569	24.801011
154.398791	5569.630059	24.806029
154.162287	5575.597172	24.811047
154.338879	5587.844600	24.816064
154.347446	5598.955061	24.821082
154.062708	5605.238439	24.826099
154.687858	5618.972560	24.831117
154.911971	5630.545489	24.836135
155.021487	5637.912899	24.841152
154.965188	5657.747168	24.846170
154.950827	5671.612229	24.851187
155.233954	5679.650943	24.856205
155.221588	5703.126329	24.861223
155.682404	5709.816787	24.866240
155.681370	5723.800127	24.871258
155.558734	5736.993785	24.876275
156.181380	5744.455239	24.881293
156.910588	5759.185409	24.886311
157.172952	5758.866327	24.891328
157.483201	5753.802619	24.896346
157.123727	5756.728316	24.901363
157.589946	5746.603706	24.906381
157.087678	5762.614673	24.911399
157.833779	5769.347625	24.916416
158.048104	5776.565587	24.921434
157.788587	5781.409526	24.926451
157.741628	5780.694481	24.931469
158.250492	5802.873911	24.936487
158.195231	5809.140087	24.941504
158.437287	5819.601786	24.946522
158.446114	5832.238139	24.951539
158.875854	5836.767804	24.956557
158.714499	5850.410881	24.961575
158.771727	5851.444786	24.966592
158.844792	5868.465529	24.971610
159.071479	5891.980559	24.976627
159.689553	5891.034140	24.981645
159.880041	5901.587442	24.986663
160.102117	5900.104737	24.991680
160.298519	5902.497207	24.996698
160.376087	5908.858808	25.001715
160.894618	5918.484687	25.006733
161.031121	5927.031524	25.011751
160.563653	5940.197814	25.016768
161.101089	5928.536673	25.021786
161.118422	5937.081888	25.026803
161.182220	5926.083267	25.031821
161.671615	5937.476247	25.036839
161.852469	5948.075343	25.041856
162.212240	5949.237777	25.046874
162.304483	5950.798963	25.051891
162.401155	5948.366509	25.056909
162.341311	5956.616972	25.061927
162.566301	5948.964449	25.066944
162.614090	5948.308774	25.071962
162.111402	5952.780116	25.076979
162.333053	5963.460451	25.081997
162.922070	5992.484970	25.087015
162.452833	5992.170776	25.092032
163.033570	6007.032182	25.097050
162.652165	6014.220826	25.102067
163.055378	6034.808614	25.107085
163.165996	6052.670692	25.112103
163.222563	6051.990665	25.117120
163.638568	6077.189151	25.122138
163.675638	6090.056393	25.127155
163.830975	6107.014449	25.132173
164.210109	6123.307138	25.137191
164.140410	6127.456175	25.142208
164.540149	6145.796564	25.147226
164.743180	6149.989442	25.152243
164.824132	6157.302910	25.157261
165.139034	6173.520801	25.162279
165.652313	6178.650664	25.167296
165.966113	6165.992626	25.172314
166.184317	6188.461099	25.177331
166.530315	6185.395869	25.182349
166.857469	6182.894725	25.187367
166.915193	6174.545279	25.192384
167.248367	6177.957284	25.197402
167.260378	6183.532275	25.202419
167.280691	6177.167200	25.207437
167.281738	6177.122132	25.212455
167.402826	6176.726433	25.217472
167.379081	6173.780515	25.222490
167.475229	6179.984647	25.227507
167.838955	6192.926738	25.232525
168.063947	6207.832772	25.237543
167.826782	6215.413483	25.242560
168.238521	6209.668188	25.247578
167.999281	6222.949979	25.252595
168.494160	6229.582831	25.257613
168.312643	6248.490096	25.262631
168.223321	6259.016767	25.267648
168.632607	6268.344922	25.272666
169.032776	6285.730682	25.277683
168.972876	6298.699789	25.282701
169.184130	6308.514855	25.287719
169.554362	6317.202226	25.292736
170.332287	6327.941056	25.297754
169.901961	6338.693231	25.302771
170.702526	6328.887476	25.307789
170.720391	6336.787668	25.312807
170.690904	6336.464253	25.317824
171.188498	6331.317835	25.322842
171.274951	6332.061606	25.327859
171.116649	6335.622487	25.332877
171.450450	6351.212654	25.337895
171.298355	6358.644937	25.342912
171.868252	6358.948997	25.347930
171.444379	6365.196655	25.352947
172.322950	6357.965979	25.357965
172.260306	6358.777059	25.362983
171.830380	6372.754927	25.368000
172.326065	6381.702046	25.373018
172.519170	6396.309660	25.378035
172.190647	6402.671750	25.383053
172.494062	6409.764447	25.388071
171.948780	6423.067357	25.393088
172.400850	6433.322523	25.398106
172.759072	6454.139918	25.403123
172.610035	6463.974304	25.408141
173.032592	6492.717117	25.413159
173.030724	6509.084178	25.418176
173.466746	6523.025595	25.423194
173.592615	6543.222028	25.428211
174.258899	6553.761947	25.433229
174.263660	6554.007704	25.438247
174.093984	6588.553053	25.443264
174.480518	6582.474007	25.448282
174.529492	6605.299774	25.453299
174.895291	6624.400400	25.458317
175.300255	6624.149025	25.463335
175.625758	6631.211252	25.468352
176.284183	6628.079780	25.473370
176.800448	6637.533972	25.478387
176.828794	6625.878457	25.483405
177.248570	6619.024866	25.488423
176.947287	6621.687877	25.493440
177.181123	6618.256589	25.498458
177.526129	6618.647259	25.503475
176.963370	6620.499608	25.508493
177.603639	6618.012469	25.513511
177.462280	6618.607036	25.518528
177.576315	6629.067581	25.523546
177.584622	6648.732882	25.528563
178.008909	6650.882379	25.533581
178.033432	6652.055859	25.538599
178.363900	6669.198758	25.543616
178.722152	6672.715281	25.548634
178.355134	6690.042359	25.553651
178.242517	6691.072349	25.558669
178.584317	6697.444112	25.563687
178.856651	6706.380862	25.568704
179.405560	6712.452448	25.573722
179.558516	6736.560356	25.578739
179.811159	6739.027603	25.583757
179.722019	6737.752568	25.588775
179.824883	6745.148415	25.593792
180.168136	6757.320910	25.598810
180.170681	6768.281970	25.603827
180.531498	6774.637114	25.608845
180.659815	6775.937756	25.613863
180.813208	6797.947125	25.618880
180.749849	6800.957741	25.623898
181.065215	6805.961035	25.628915
181.104314	6810.962848	25.633933
181.089401	6827.102449	25.638951
181.422054	6846.382327	25.643968
181.509819	6848.345335	25.648986
181.776693	6861.084003	25.654003
182.002044	6872.756093	25.659021
182.919563	6877.295401	25.664039
182.273363	6897.738852	25.669056
182.453566	6897.683553	25.674074
182.699211	6908.200496	25.679092
183.064117	6930.121011	25.684109
183.120186	6921.246815	25.689127
183.203914	6938.606394	25.694144
183.461231	6938.477219	25.699162
183.596026	6950.921134	25.704180
183.860017	6972.511605	25.709197
184.417181	6976.176858	25.714215
184.235063	6986.372513	25.719232
184.572625	6991.506768	25.724250
184.524312	7002.909186	25.729268
184.778850	7013.232461	25.734285
185.296907	7017.612622	25.739303
185.104925	7050.909468	25.744320
185.295113	7051.565381	25.749338
185.735041	7066.355023	25.754356
186.128719	7073.165493	25.759373
186.144285	7080.234571	25.764391
186.302039	7089.725279	25.769408
186.311359	7088.342746	25.774426
187.123173	7106.075566	25.779444
186.875757	7104.354975	25.784461
186.977686	7109.974746	25.789479
187.053502	7116.290651	25.794496
187.551908	7127.101574	25.799514
187.743538	7144.612249	25.804532
187.655253	7144.755012	25.809549
188.066106	7136.586377	25.814567
187.931052	7163.924504	25.819584
188.123761	7171.642311	25.824602
188.516767	7172.759755	25.829620
188.674574	7184.093883	25.834637
189.286575	7183.715633	25.839655
189.298777	7196.841690	25.844672
189.331994	7185.805694	25.849690
189.756406	7195.487874	25.854708
189.739958	7214.593284	25.859725
189.862650	7208.430825	25.864743
189.956070	7220.228194	25.869760
189.896274	7225.191945	25.874778
190.213075	7240.525933	25.879796
190.255588	7248.515307	25.884813
190.553036	7264.698701	25.889831
190.756371	7283.833480	25.894848
190.907066	7282.592917	25.899866
191.407664	7292.340086	25.904884
191.116260	7308.949812	25.909901
191.540062	7314.445157	25.914919
191.425864	7316.416846	25.919936
191.726836	7332.863609	25.924954
192.106763	7354.611184	25.929972
192.257519	7346.561079	25.934989
193.166863	7362.290700	25.940007
192.765176	7377.552611	25.945024
192.667134	7379.839012	25.950042
192.995630	7373.460023	25.955060
193.011992	7398.679473	25.960077
193.272478	7411.528389	25.965095
193.128906	7415.295744	25.970112
193.430594	7432.580682	25.975130
193.735776	7449.852436	25.980148
193.417868	7472.061686	25.985165
194.063213	7480.696234	25.990183
194.311698	7503.092040	25.995200
194.511830	7510.132034	26.000218
195.318687	7524.719767	26.005236
195.301422	7542.502232	26.010253
195.682615	7532.271336	26.015271
195.667658	7545.917545	26.020288
196.003880	7562.873713	26.025306
196.469521	7568.981962	26.030324
196.488586	7568.510761	26.035341
196.630012	7562.926340	26.040359
196.600849	7578.420793	26.045376
197.019682	7594.664855	26.050394
196.983167	7588.986457	26.055412
197.071895	7601.980772	26.060429
197.450682	7612.677031	26.065447
197.521152	7613.982932	26.070464
197.456474	7624.260484	26.075482
198.032694	7643.431825	26.080500
198.141060	7656.586678	26.085517
198.380169	7663.605090	26.090535
198.388627	7684.324911	26.095552
198.832415	7688.359547	26.100570
199.019639	7691.450271	26.105588
198.617086	7721.761058	26.110605
199.108837	7724.471079	26.115623
199.551892	7738.578580	26.120640
199.561007	7762.943513	26.125658
200.079330	7753.711530	26.130676
199.847776	7777.038459	26.135693
199.980084	7783.192899	26.140711
200.083378	7802.753525	26.145728
200.209376	7818.468980	26.150746
200.414080	7836.669069	26.155764
200.740447	7862.493920	26.160781
200.966729	7869.276705	26.165799
201.180864	7879.586984	26.170816
201.369908	7888.401596	26.175834
201.773465	7901.416241	26.180852
201.890508	7920.303446	26.185869
202.011726	7915.907223	26.190887
202.470164	7933.914246	26.195904
202.594289	7948.311367	26.200922
203.299398	7940.993137	26.205940
203.320473	7946.116564	26.210957
203.671373	7942.938299	26.215975
203.721962	7957.253496	26.220992
203.876218	7979.750415	26.226010
203.854992	7970.419358	26.231028
203.917532	7981.826315	26.236045
204.172940	7991.196041	26.241063
204.348363	7993.779136	26.246080
205.150416	7992.362269	26.251098
205.753552	8008.066238	26.256116
205.780744	8018.319628	26.261133
206.213003	8004.178459	26.266151
206.263800	8009.702532	26.271168
206.188666	8005.262737	26.276186
206.610097	8008.329921	26.281204
206.461091	8007.994659	26.286221
206.652979	8012.190727	26.291239
206.624975	8016.649015	26.296256
206.495224	8030.172718	26.301274
207.306192	8035.259253	26.306292
207.261024	8046.207306	26.311309
206.786977	8053.953958	26.316327
207.571310	8078.122675	26.321344
207.011321	8090.183946	26.326362
207.202077	8106.813473	26.331380
207.392751	8131.887599	26.336397
207.512917	8147.329429	26.341415
208.029645	8178.145262	26.346432
207.772449	8198.073833	26.351450
208.538080	8211.392214	26.356468
208.376976	8235.464034	26.361485
208.677793	8258.111905	26.366503
209.331911	8277.859155	26.371520
208.953623	8288.966890	26.376538
209.528264	8318.429830	26.381556
209.624495	8338.944008	26.386573
209.987536	8353.064191	26.391591
210.769812	8373.174049	26.396608
210.517575	8380.944285	26.401626
210.890316	8379.251971	26.406644
210.909350	8402.827558	26.411661
211.368556	8405.470010	26.416679
211.740288	8421.305437	26.421696
212.018059	8443.205144	26.426714
212.743042	8440.390452	26.431732
212.643911	8450.069384	26.436749
212.532479	8457.907698	26.441767
212.935311	8465.501876	26.446784
212.896600	8476.582257	26.451802
213.213086	8474.862548	26.456820
213.254399	8492.038845	26.461837
213.544327	8508.801477	26.466855
213.699328	8496.268099	26.471872
214.047955	8502.165143	26.476890
214.558037	8517.164697	26.481908
214.519236	8526.622195	26.486925
214.669333	8523.599564	26.491943
214.779794	8532.796706	26.496960
214.908488	8557.723765	26.501978
215.597552	8555.595900	26.506996
215.582888	8562.877224	26.512013
215.674010	8568.101503	26.517031
216.049845	8583.814274	26.522048
216.093295	8595.195788	26.527066
216.319188	8603.718493	26.532084
216.219669	8618.301874	26.537101
216.683686	8616.876723	26.542119
217.037768	8634.514806	26.547136
217.220926	8654.675716	26.552154
217.274350	8659.425117	26.557172
217.440043	8678.530983	26.562189
217.751208	8685.205812	26.567207
218.199454	8694.083584	26.572224
217.802158	8729.481660	26.577242
218.235976	8733.341796	26.582260
218.069675	8757.115905	26.587277
218.397460	8766.129390	26.592295
219.105318	8779.702381	26.597312
219.125831	8794.961014	26.602330
219.221228	8812.748417	26.607348
219.285322	8825.008942	26.612365
219.895920	8841.644474	26.617383
220.439493	8850.085282	26.622400
220.338353	8866.160561	26.627418
220.426563	8873.080101	26.632436
220.364762	8887.785679	26.637453
220.227605	8903.556755	26.642471
220.817105	8916.806647	26.647488
221.069586	8942.972070	26.652506
221.832127	8943.626077	26.657524
223.244407	8940.889671	26.662541
223.794175	8941.879533	26.667559
223.912484	8926.236154	26.672576
224.056844	8903.119496	26.677594
224.446852	8897.068143	26.682612
224.454445	8895.424973	26.687629
223.949388	8893.127519	26.692647
224.685037	8890.388924	26.697664
224.517020	8894.035543	26.702682
225.057119	8892.562664	26.707700
225.537272	8895.203185	26.712717
224.830083	8889.098820	26.717735
225.120163	8881.183216	26.722752
224.939372	8892.344962	26.727770
225.277562	8882.252947	26.732788
225.229944	8893.065697	26.737805
224.944002	8916.034880	26.742823
225.396666	8917.926930	26.747840
225.480505	8941.552863	26.752858
225.344234	8949.736813	26.757876
225.966711	8970.645335	26.762893
225.778745	8990.756829	26.767911
226.254964	9016.001623	26.772928
226.052912	9041.455685	26.777946
226.523759	9053.720723	26.782964
227.268823	9076.571714	26.787981
226.876462	9100.142414	26.792999
227.070810	9116.006569	26.798016
227.365892	9136.037021	26.803034
227.714814	9161.688340	26.808052
228.192270	9193.867977	26.813069
228.147622	9204.659941	26.818087
228.490852	9216.218990	26.823104
228.792692	9232.094773	26.828122
229.199179	9266.528988	26.833140
229.595392	9278.293300	26.838157
229.838773	9294.108256	26.843175
230.588228	9285.529116	26.848192
230.854216	9301.330750	26.853210
231.382539	9307.812619	26.858228
231.588430	9307.633947	26.863245
231.511839	9319.304424	26.868263
231.922737	9308.027330	26.873280
231.758161	9312.848956	26.878298
232.154143	9323.532382	26.883316
232.806362	9329.816541	26.888333
232.434877	9340.299045	26.893351
232.686699	9335.169391	26.898368
232.934434	9362.633146	26.903386
232.894283	9363.571306	26.908404
233.094014	9375.608882	26.913421
232.990143	9407.012471	26.918439
233.753714	9403.945979	26.923456
233.626694	9432.662204	26.928474
233.630795	9435.190597	26.933492
234.226527	9447.710287	26.938509
233.992317	9478.354781	26.943527
234.364738	9494.664665	26.948544
234.300659	9511.536293	26.953562
234.769316	9524.276370	26.958580
235.082214	9546.453618	26.963597
235.068056	9560.327515	26.968615
235.632298	9585.365871	26.973632
235.863314	9618.809817	26.978650
235.988064	9625.739174	26.983668
235.845522	9650.131375	26.988685
235.969598	9673.762511	26.993703
236.713170	9695.418622	26.998720
237.171469	9711.222361	27.003738
237.211611	9739.625261	27.008756
237.181836	9743.560380	27.013773
237.522408	9771.175948	27.018791
237.635987	9781.433773	27.023808
237.736235	9814.928901	27.028826
238.048773	9835.261355	27.033844
238.496266	9848.243261	27.038861
238.290517	9875.278210	27.043879
239.624634	9885.415139	27.048896
240.037193	9907.011663	27.053914
239.839702	9910.171912	27.058932
240.571783	9913.744844	27.063949
240.290898	9930.613098	27.068967
240.486158	9941.438494	27.073984
240.869426	9961.177512	27.079002
240.901051	9975.926369	27.084020
241.050624	9979.972626	27.089037
240.917031	10006.640869	27.094055
241.727487	10014.514956	27.099072
242.276023	10029.944256	27.104090
242.143784	10043.039870	27.109108
242.335306	10059.371875	27.114125
242.231098	10071.118537	27.119143
242.692423	10082.200980	27.124160
243.251041	10103.960254	27.129178
243.482178	10130.676491	27.134196
243.689500	10132.353885	27.139213
244.300908	10158.618913	27.144231
244.499575	10160.289914	27.149248
245.103586	10159.844442	27.154266
245.163909	10179.594958	27.159284
245.036744	10189.799755	27.164301
244.758021	10202.101175	27.169319
245.125917	10223.704201	27.174336
245.948830	10241.697826	27.179354
245.923827	10257.763009	27.184372
245.902350	10274.565094	27.189389
246.117599	10295.277244	27.194407
245.988913	10304.744883	27.199424
246.580303	10330.150061	27.204442
246.732761	10349.355509	27.209460
247.348511	10370.178754	27.214477
247.399234	10391.836369	27.219495
247.446989	10399.269343	27.224512
247.824922	10416.874559	27.229530
247.918510	10438.071044	27.234548
248.781095	10449.422194	27.239565
249.405436	10460.760609	27.244583
249.808570	10456.192463	27.249600
249.922964	10459.627136	27.254618
250.059246	10485.903220	27.259636
250.566754	10485.130747	27.264653
250.550014	10483.553045	27.269671
250.987770	10478.536143	27.274688
251.405460	10478.160421	27.279706
251.121755	10484.714190	27.284724
251.389419	10496.428937	27.289741
251.263201	10511.591419	27.294759
251.440931	10513.634797	27.299776
251.595417	10534.414398	27.304794
251.622025	10551.006817	27.309812
252.053830	10570.851722	27.314829
252.464600	10585.285584	27.319847
252.426844	10609.951223	27.324864
252.820465	10627.007153	27.329882
252.469626	10658.947163	27.334900
252.810608	10680.389945	27.339917
252.833156	10702.175721	27.344935
253.157996	10722.954730	27.349952
253.903161	10746.635408	27.354970
253.727467	10773.072589	27.359988
253.874586	10800.857020	27.365005
254.076638	10827.659760	27.370023
254.875926	10855.274194	27.375040
255.466672	10867.143425	27.380058
255.848938	10893.573416	27.385076
256.151846	10906.306750	27.390093
256.635523	10915.586261	27.395111
257.003968	10928.076722	27.400128
257.379269	10918.180380	27.405146
257.389053	10932.262515	27.410164
257.396923	10950.204370	27.415181
257.816827	10958.500444	27.420199
258.007804	10980.328638	27.425216
258.292937	10992.314956	27.430234
258.309992	11006.901775	27.435252
258.490899	11017.585367	27.440269
258.991610	11032.109796	27.445287
259.040905	11046.175802	27.450304
259.657515	11049.444150	27.455322
259.879639	11073.530138	27.460340
260.101593	11085.713312	27.465357
260.133941	11106.894374	27.470375
260.798348	11121.762743	27.475392
261.126430	11124.692884	27.480410
260.947806	11155.717107	27.485428
261.092753	11157.039686	27.490445
261.263077	11181.840725	27.495463
261.512528	11192.211683	27.500480
262.233998	11207.683384	27.505498
262.565413	11229.090708	27.510516
262.689489	11233.552967	27.515533
262.383266	11258.353854	27.520551
262.586709	11272.344781	27.525568
262.959308	11297.765338	27.530586
262.927264	11321.294826	27.535604
263.913936	11330.385927	27.540621
264.425062	11341.317288	27.545639
265.170738	11331.814238	27.550656
265.637035	11315.937139	27.555674
266.127315	11320.052987	27.560692
266.592210	11315.745080	27.565709
266.925023	11325.285500	27.570727
267.073398	11322.060929	27.575744
267.460987	11307.502203	27.580762
267.063176	11294.545301	27.585780
266.995110	11290.716429	27.590797
267.154861	11303.542377	27.595815
267.000582	11321.357992	27.600832
267.136517	11316.337411	27.605850
267.611592	11342.698645	27.610868
267.488264	11351.225136	27.615885
267.670390	11374.158534	27.620903
267.785493	11389.821018	27.625920
267.863345	11409.273745	27.630938
267.782496	11438.255081	27.635956
268.116462	11463.015893	27.640973
268.387871	11483.661622	27.645991
268.323607	11527.521995	27.651008
268.929974	11549.561852	27.656026
269.530324	11587.444332	27.661044
269.943356	11604.118156	27.666061
270.185564	11631.563058	27.671079
270.760035	11646.409501	27.676096
271.351183	11663.355442	27.681114
271.630205	11686.077251	27.686132
271.475308	11693.619621	27.691149
271.950041	11710.435847	27.696167
272.040951	11728.671640	27.701184
272.553553	11752.288060	27.706202
272.614789	11767.473161	27.711220
273.316059	11788.018807	27.716237
273.805649	11795.294739	27.721255
273.757601	11819.866260	27.726272
274.517415	11821.652439	27.731290
274.541557	11839.269406	27.736308
274.597017	11848.482586	27.741325
274.940117	11852.544998	27.746343
275.213572	11880.350592	27.751360
275.569319	11887.657386	27.756378
275.847268	11913.775956	27.761396
275.739677	11925.017061	27.766413
276.150947	11933.821010	27.771431
276.187879	11957.506647	27.776448
276.848213	11974.482032	27.781466
276.644597	11994.538449	27.786484
276.740303	12002.791337	27.791501
276.943429	12029.772382	27.796519
277.019941	12063.586678	27.801536
277.699182	12088.249860	27.806554
277.705814	12116.552326	27.811572
277.665339	12139.409903	27.816589
278.011268	12171.203496	27.821607
277.870790	12202.664449	27.826624
278.539071	12227.295048	27.831642
279.270046	12254.724993	27.836660
279.444445	12274.663377	27.841677
279.864652	12290.747239	27.846695
279.660503	12310.646531	27.851712
280.716686	12326.438605	27.856730
281.123564	12343.517705	27.861748
282.216704	12347.180611	27.866765
282.747224	12328.333312	27.871783
283.048156	12339.493650	27.876800
283.511437	12338.501733	27.881818
284.058865	12339.334627	27.886836
283.678143	12339.477118	27.891853
284.348151	12332.237044	27.896871
284.283360	12331.917193	27.901888
284.470237	12332.317008	27.906906
284.338931	12337.389138	27.911924
284.447010	12342.746479	27.916941
284.685307	12356.466013	27.921959
284.354538	12379.189282	27.926976
284.470177	12394.378250	27.931994
284.834545	12411.699537	27.937012
284.950541	12442.994063	27.942029
285.296977	12454.676232	27.947047
285.989986	12490.700957	27.952064
286.217938	12508.573704	27.957082
286.084844	12533.157719	27.962100
286.240059	12556.086356	27.967117
286.744774	12580.036297	27.972135
286.592507	12608.863307	27.977152
286.600386	12631.117529	27.982170
287.297274	12663.354691	27.987188
287.405856	12700.762962	27.992205
288.059732	12724.069731	27.997223
288.447550	12760.932241	28.002240
288.250952	12785.540125	28.007258
289.407932	12816.748358	28.012276
289.182837	12840.678766	28.017293
289.722025	12863.467946	28.022311
289.870784	12906.267890	28.027328
290.311094	12925.223718	28.032346
291.172842	12945.697614	28.037364
290.839397	12975.016536	28.042381
291.147775	12989.964976	28.047399
291.531010	13015.695300	28.052416
291.566128	13035.094238	28.057434
291.843967	13064.782957	28.062452
292.493249	13076.992095	28.067469
293.151360	13100.316011	28.072487
293.296646	13122.613546	28.077504
293.593161	13135.374936	28.082522
294.152965	13158.321756	28.087540
294.280110	13168.412320	28.092557
294.941864	13170.541722	28.097575
295.272238	13193.948737	28.102592
295.458596	13194.674921	28.107610
295.685406	13202.294410	28.112628
295.728145	13217.989959	28.117645
296.202107	13227.597142	28.122663
295.988561	13251.143170	28.127680
296.516129	13257.319422	28.132698
296.854507	13275.486152	28.137716
296.594257	13306.090268	28.142733
297.292104	13305.726374	28.147751
297.671051	13335.576356	28.152768
297.850265	13349.371469	28.157786
297.981177	13365.122972	28.162804
298.012386	13393.968770	28.167821
298.868555	13412.072124	28.172839
298.587894	13446.866220	28.177856
298.760689	13465.105671	28.182874
299.465632	13486.016918	28.187892
299.480980	13508.323060	28.192909
300.265032	13530.064043	28.197927
300.486613	13547.217138	28.202944
300.649613	13577.739760	28.207962
301.461929	13588.679331	28.212980
300.842308	13606.911322	28.217997
301.542475	13629.469078	28.223015
301.659308	13657.914503	28.228032
302.293756	13678.090977	28.233050
302.707767	13707.973453	28.238068
302.363024	13734.370297	28.243085
303.107026	13754.868541	28.248103
303.483568	13780.859704	28.253120
304.101049	13801.304034	28.258138
303.858722	13820.102064	28.263156
304.082430	13848.926699	28.268173
304.496404	13863.184808	28.273191
304.450276	13897.162599	28.278208
304.800575	13916.182285	28.283226
305.351602	13940.479343	28.288244
305.270610	13978.941227	28.293261
305.477577	14005.442545	28.298279
306.195948	14043.348309	28.303296
306.653542	14061.954149	28.308314
306.971997	14100.415631	28.313332
307.113689	14124.337051	28.318349
307.421932	14140.976254	28.323367
307.379892	14177.884090	28.328384
307.474588	14207.064041	28.333402
308.278164	14235.938132	28.338420
308.383833	14267.220556	28.343437
308.492780	14286.173276	28.348455
308.966703	14322.948871	28.353472
309.212296	14361.365128	28.358490
309.819671	14384.828816	28.363508
310.089329	14422.320572	28.368525
310.599827	14437.782642	28.373543
311.054703	14469.650280	28.378560
311.186039	14488.779086	28.383578
311.509853	14508.089295	28.388596
311.687388	14527.333174	28.393613
312.487860	14547.015693	28.398631
312.736937	14565.274812	28.403648
313.299823	14580.450618	28.408666
314.221077	14581.380350	28.413684
314.021878	14593.559503	28.418701
314.634863	14609.030965	28.423719
314.914490	14620.544860	28.428736
315.469789	14633.460093	28.433754
315.776884	14642.258140	28.438772
315.703410	14653.315563	28.443789
316.209388	14657.722762	28.448807
316.623657	14660.214766	28.453824
316.621585	14674.182345	28.458842
316.744321	14674.172355	28.463860
316.898674	14699.254139	28.468877
317.352414	14706.777113	28.473895
317.412655	14738.066639	28.478912
317.654179	14749.371206	28.483930
318.000168	14774.803293	28.488948
317.694393	14803.422425	28.493965
318.393506	14827.206768	28.498983
319.100018	14860.915681	28.504000
319.091481	14887.720163	28.509018
319.477318	14906.569394	28.514036
319.359572	14938.919113	28.519053
319.523458	14953.243098	28.524071
320.186748	14987.774616	28.529088
320.259288	15021.721766	28.534106
320.501107	15049.235492	28.539124
320.580631	15082.845820	28.544141
321.088337	15119.235933	28.549159
321.797261	15149.789269	28.554176
321.801046	15176.973572	28.559194
322.423665	15211.668582	28.564212
322.687717	15238.318147	28.569229
323.414356	15259.970377	28.574247
323.822399	15288.893610	28.579264
323.832852	15311.097409	28.584282
324.285672	15333.651028	28.589300
324.519820	15360.149859	28.594317
324.865528	15378.986012	28.599335
325.069535	15410.171773	28.604352
325.790145	15437.293550	28.609370
325.845941	15460.114003	28.614388
325.915172	15496.679403	28.619405
326.349565	15513.061918	28.624423
327.506948	15524.695564	28.629440
328.953004	15529.761581	28.634458
329.685963	15529.230855	28.639476
329.540906	15538.597114	28.644493
329.838483	15538.962279	28.649511
330.229113	15527.373880	28.654528
330.275677	15539.692884	28.659546
330.513483	15522.399108	28.664564
330.818230	15530.635280	28.669581
330.884644	15525.526029	28.674599
330.894009	15525.046805	28.679616
330.778472	15540.911980	28.684634
331.071128	15558.663452	28.689652
331.754990	15576.984738	28.694669
331.687327	15593.155450	28.699687
331.983023	15604.701958	28.704704
332.329953	15624.912757	28.709722
332.959395	15643.407384	28.714740
332.989133	15656.405613	28.719757
333.073691	15680.960156	28.724775
333.548405	15702.719198	28.729792
333.476458	15731.463793	28.734810
333.660696	15758.198809	28.739828
334.018252	15794.973976	28.744845
333.986223	15819.752056	28.749863
334.326831	15849.067729	28.754880
334.695302	15889.159490	28.759898
335.515746	15920.374555	28.764916
335.142193	15961.988754	28.769933
335.461354	15994.825264	28.774951
335.925985	16028.190219	28.779968
335.870306	16075.191908	28.784986
336.289551	16101.757936	28.790004
337.292138	16140.065920	28.795021
337.903805	16172.873144	28.800039
339.283405	16178.863496	28.805056
340.414919	16183.556428	28.810074
340.743649	16187.663377	28.815092
341.360552	16194.785463	28.820109
341.917907	16199.756511	28.825127
342.046249	16198.325223	28.830144
342.089448	16192.373220	28.835162
342.212745	16207.231762	28.840180
342.539954	16207.722708	28.845197
342.386663	16204.892549	28.850215
342.593932	16218.682097	28.855232
342.509653	16237.769477	28.860250
342.743703	16251.809840	28.865268
342.859064	16271.968106	28.870285
343.205755	16307.466225	28.875303
344.038378	16321.892751	28.880320
343.768652	16350.101647	28.885338
344.038484	16375.892902	28.890356
344.620466	16396.237763	28.895373
344.390009	16430.589683	28.900391
344.800114	16455.827343	28.905408
345.225829	16491.358026	28.910426
346.000991	16511.848058	28.915444
345.702383	16559.476026	28.920461
345.889710	16592.601151	28.925479
346.651955	16613.935341	28.930496
346.639165	16647.506323	28.935514
346.792771	16672.964832	28.940532
347.435569	16710.374162	28.945549
347.316847	16742.096970	28.950567
347.866409	16777.638567	28.955584
348.216011	16819.630704	28.960602
348.626515	16847.961906	28.965620
348.884977	16877.383327	28.970637
348.853991	16925.395269	28.975655
349.561483	16958.299549	28.980672
349.768230	17005.397611	28.985690
350.336454	17038.455189	28.990708
350.698595	17083.231482	28.995725
351.002125	17111.780101	29.000743
351.266677	17148.952552	29.005760
351.691316	17187.741934	29.010778
352.225065	17226.131194	29.015796
352.788822	17253.159855	29.020813
352.571811	17295.783151	29.025831
353.370085	17328.863361	29.030848
353.562487	17376.729533	29.035866
353.949776	17406.791943	29.040884
354.272635	17444.171039	29.045901
354.725572	17481.247305	29.050919
355.716812	17494.648155	29.055936
356.439955	17513.171376	29.060954
357.284772	17522.354912	29.065972
357.935974	17543.411362	29.070989
357.915853	17565.353814	29.076007
358.577519	17563.514129	29.081024
358.963387	17589.183320	29.086042
359.202103	17590.104106	29.091060
359.286390	17601.322477	29.096077
359.604033	17625.166754	29.101095
359.910132	17628.232696	29.106112
360.503203	17656.841408	29.111130
360.706032	17671.790098	29.116148
360.746344	17691.354393	29.121165
360.945416	17705.431929	29.126183
361.703432	17723.671937	29.131200
361.819710	17740.221526	29.136218
362.394949	17750.865553	29.141236
363.311156	17769.456873	29.146253
363.829384	17791.069300	29.151271
364.062995	17782.763414	29.156288
363.959254	17799.940400	29.161306
364.367335	17816.630820	29.166324
364.868007	17830.740332	29.171341
364.768944	17856.841460	29.176359
364.970470	17876.335775	29.181376
365.197898	17895.814638	29.186394
365.206265	17933.037464	29.191412
365.801946	17951.636622	29.196429
365.961067	17986.863022	29.201447
365.963043	18002.546427	29.206464
366.078930	18038.108271	29.211482
366.448883	18065.020109	29.216500
366.949565	18109.228331	29.221517
367.073182	18135.961777	29.226535
367.840509	18155.670039	29.231552
368.338833	18190.327921	29.236570
368.780491	18226.617900	29.241588
369.460183	18254.377195	29.246605
369.599204	18288.198195	29.251623
369.243679	18310.077701	29.256640
370.213731	18351.388737	29.261658
370.374019	18373.165737	29.266676
371.139878	18405.049108	29.271693
371.303994	18444.245515	29.276711
372.121886	18464.393234	29.281728
372.177419	18500.292759	29.286746
372.268692	18529.441447	29.291764
372.784565	18558.187905	29.296781
373.283993	18594.878701	29.301799
373.363366	18628.767367	29.306816
373.508880	18656.760769	29.311834
374.008598	18684.209489	29.316852
374.992290	18714.824765	29.321869
375.236620	18757.397928	29.326887
375.685145	18770.662630	29.331904
375.796968	18804.066787	29.336922
376.183764	18837.200003	29.341940
377.059719	18858.124996	29.346957
377.360813	18899.410125	29.351975
377.540980	18912.057157	29.356992
378.043010	18948.191719	29.362010
378.246063	18975.485212	29.367028
379.463538	18993.179600	29.372045
379.204714	19021.443138	29.377063
379.476228	19041.254757	29.382080
379.954947	19078.929271	29.387098
379.962521	19112.553718	29.392116
380.426836	19140.346659	29.397133
380.292217	19183.476187	29.402151
380.840029	19210.950635	29.407168
381.185416	19258.321364	29.412186
381.390227	19290.644707	29.417204
382.404085	19315.657076	29.422221
382.446164	19349.850000	29.427239
383.212616	19387.166860	29.432256
383.378030	19421.215809	29.437274
383.841560	19456.137688	29.442292
383.847721	19485.179630	29.447309
384.044473	19519.630198	29.452327
384.879131	19553.386554	29.457344
384.922188	19597.468983	29.462362
385.479483	19637.824319	29.467380
386.290440	19670.348819	29.472397
386.406440	19707.686408	29.477415
386.850552	19731.687016	29.482432
387.084572	19760.764489	29.487450
387.402327	19793.810504	29.492468
387.614928	19825.714122	29.497485
387.906591	19852.172364	29.502503
388.352425	19889.264620	29.507520
389.088862	19927.420342	29.512538
389.031039	19960.042252	29.517556
389.533991	19993.233516	29.522573
389.753109	20036.887997	29.527591
389.822499	20081.593146	29.532608
390.632471	20118.845826	29.537626
391.334532	20162.657537	29.542644
391.402218	20202.100026	29.547661
391.770279	20243.017456	29.552679
392.205240	20282.346734	29.557696
392.656056	20321.037942	29.562714
392.973663	20352.084128	29.567732
393.902426	20373.691018	29.572749
393.959548	20413.444860	29.577767
394.299560	20454.749192	29.582784
394.388231	20488.663642	29.587802
395.069855	20536.399757	29.592820
395.959735	20567.289925	29.597837
395.959399	20610.502561	29.602855
396.316523	20646.227232	29.607872
396.745656	20682.554599	29.612890
396.743137	20724.269917	29.617908
397.299803	20755.712655	29.622925
397.420749	20812.317530	29.627943
397.704522	20857.164587	29.632960
399.019232	20896.078041	29.637978
399.210189	20926.847382	29.642996
399.631485	20953.920597	29.648013
400.131389	20987.615769	29.653031
400.692354	21020.729723	29.658048
401.525604	21048.421578	29.663066
401.402792	21089.016761	29.668084
402.074854	21104.039461	29.673101
402.256982	21145.788821	29.678119
402.625474	21176.643301	29.683136
403.393690	21205.827237	29.688154
403.672943	21248.891085	29.693172
403.982591	21278.256226	29.698189
405.631371	21271.070123	29.703207
407.317779	21257.347735	29.708224
408.243454	21260.210409	29.713242
407.936741	21271.917672	29.718260
408.534624	21260.986818	29.723277
408.830203	21266.676005	29.728295
408.561126	21269.568389	29.733312
409.140236	21263.700948	29.738330
409.250601	21269.563794	29.743348
409.277751	21262.004340	29.748365
409.315898	21286.955044	29.753383
409.535234	21297.328020	29.758400
410.231865	21309.930916	29.763418
409.987992	21339.018876	29.768436
410.309161	21348.223308	29.773453
410.636047	21375.833748	29.778471
410.950067	21408.525597	29.783488
411.322887	21429.968925	29.788506
411.532831	21464.987286	29.793524
411.433945	21486.940436	29.798541
411.827858	21524.478812	29.803559
412.216389	21563.924669	29.808576
412.731919	21592.263200	29.813594
412.860593	21654.319340	29.818612
413.062758	21683.509640	29.823629
413.481663	21733.479746	29.828647
413.690927	21778.182730	29.833664
414.338832	21817.389187	29.838682
414.702313	21874.457491	29.843700
415.937182	21887.826434	29.848717
416.361354	21931.911105	29.853735
417.037153	21961.864378	29.858752
418.146876	21983.395011	29.863770
418.270582	22015.505630	29.868788
418.812647	22037.625615	29.873805
419.252928	22056.192859	29.878823
419.697229	22090.295560	29.883840
419.766740	22108.254615	29.888858
419.917983	22153.424264	29.893876
420.055618	22171.800645	29.898893
420.307662	22218.814004	29.903911
420.800326	22264.218753	29.908928
421.437151	22298.951205	29.913946
421.298108	22341.856101	29.918964
422.407952	22365.970286	29.923981
423.368569	22399.471031	29.928999
423.416565	22428.567596	29.934016
423.911932	22455.953790	29.939034
424.186172	22492.414067	29.944052
424.960939	22522.556375	29.949069
425.892967	22554.706112	29.954087
426.092727	22577.153546	29.959104
426.059635	22600.003621	29.964122
426.119654	22634.271033	29.969140
426.848901	22666.761669	29.974157
427.181325	22686.193356	29.979175
427.501425	22718.372567	29.984192
427.914897	22743.155419	29.989210
428.720552	22786.593428	29.994228
429.336912	22820.343235	29.999245
429.356432	22851.741538	30.004263
429.410000	22888.417099	30.009280
430.082541	22919.224207	30.014298
430.460709	22963.067095	30.019316
430.906517	22993.011126	30.024333
432.362145	23008.156723	30.029351
432.471530	23035.392357	30.034368
433.058519	23040.458162	30.039386
433.140035	23066.348675	30.044404
433.342345	23073.893283	30.049421
433.814778	23109.163361	30.054439
433.791250	23147.316185	30.059456
434.247929	23166.730280	30.064474
434.334638	23205.898889	30.069492
434.767153	23242.702670	30.074509
435.277521	23274.005016	30.079527
435.374698	23316.537532	30.084544
436.598905	23348.856332	30.089562
436.508653	23399.839561	30.094580
437.235901	23424.695797	30.099597
437.772975	23462.163428	30.104615
437.550887	23502.562128	30.109632
438.080569	23551.871955	30.114650
438.418854	23597.221529	30.119668
438.611786	23635.486588	30.124685
439.222688	23678.364089	30.129703
439.396698	23735.368546	30.134720
439.778552	23783.912665	30.139738
440.233478	23838.368032	30.144756
440.671296	23888.309639	30.149773
441.460984	23925.119915	30.154791
441.607762	23979.814634	30.159808
442.485819	24013.301147	30.164826
443.000587	24066.169852	30.169844
443.295455	24105.229133	30.174861
444.356442	24138.552064	30.179879
445.100643	24175.421140	30.184896
445.984123	24203.604740	30.189914
446.553285	24228.864592	30.194932
447.124516	24257.401446	30.199949
447.294218	24277.692401	30.204967
447.762868	24319.876696	30.209984
448.859415	24333.807517	30.215002
449.068721	24360.580212	30.220020
448.614466	24387.299476	30.225037
449.275579	24407.345506	30.230055
449.465481	24445.095571	30.235072
450.356316	24464.092916	30.240090
450.458473	24503.100954	30.245108
451.154422	24529.654884	30.250125
451.273613	24565.124116	30.255143
451.626669	24603.196703	30.260160
451.934756	24634.107194	30.265178
452.206204	24681.922020	30.270196
452.159541	24730.135316	30.275213
452.843454	24772.053559	30.280231
452.981414	24824.907143	30.285248
453.334830	24869.970419	30.290266
453.710880	24922.073758	30.295284
454.286869	24980.448704	30.300301
454.773806	25022.675743	30.305319
454.856383	25083.025095	30.310336
455.862907	25121.437933	30.315354
456.147153	25166.375037	30.320372
456.117507	25212.356549	30.325389
456.681350	25264.955537	30.330407
457.155169	25310.406255	30.335424
457.719486	25362.453422	30.340442
458.208149	25413.135187	30.345460
458.727711	25460.102089	30.350477
459.289262	25504.251237	30.355495
459.494950	25566.328782	30.360512
459.801584	25615.966633	30.365530
460.621234	25660.232834	30.370548
460.528451	25714.879446	30.375565
461.224884	25773.930430	30.380583
461.743382	25830.053101	30.385600
462.401009	25877.413879	30.390618
463.196337	25930.353770	30.395636
463.374729	25988.775003	30.400653
464.565523	26025.413771	30.405671
465.066394	26068.366531	30.410688
465.503983	26103.699173	30.415706
467.057432	26125.707902	30.420724
467.807502	26144.551409	30.425741
468.784460	26161.068939	30.430759
469.392061	26179.321741	30.435776
469.271460	26197.601548	30.440794
469.752671	26204.030310	30.445812
469.887108	26233.247812	30.450829
470.713480	26245.775344	30.455847
470.724666	26278.758627	30.460864
471.037873	26303.730977	30.465882
471.078383	26335.867045	30.470900
471.334058	26364.852630	30.475917
472.043627	26397.662838	30.480935
472.083773	26430.830728	30.485952
472.137496	26484.927817	30.490970
473.056046	26531.176224	30.495988
472.902920	26582.709576	30.501005
473.876935	26610.941535	30.506023
473.938294	26666.608935	30.511040
474.604534	26719.261030	30.516058
475.542455	26765.983109	30.521076
475.465097	26816.478871	30.526093
475.701432	26861.479040	30.531111
476.204180	26915.901179	30.536128
476.870267	26951.653832	30.541146
477.368876	26999.694802	30.546164
477.414114	27061.363494	30.551181
478.407594	27119.431166	30.556199
478.537578	27172.873734	30.561216
479.049586	27223.695584	30.566234
479.792728	27274.910191	30.571252
479.707078	27343.896318	30.576269
480.415686	27394.722835	30.581287
480.713447	27443.288444	30.586304
481.176376	27494.293008	30.591322
482.011970	27526.746175	30.596340
481.963506	27586.978367	30.601357
482.519988	27631.323072	30.606375
483.103894	27693.406473	30.611392
483.622229	27736.587504	30.616410
484.343140	27787.387815	30.621428
484.493085	27854.019851	30.626445
484.999133	27898.358099	30.631463
485.892738	27947.261546	30.636480
486.495627	28001.755086	30.641498
486.466058	28041.370976	30.646516
486.722380	28104.988499	30.651533
487.408751	28153.981667	30.656551
487.730335	28208.135984	30.661568
488.442060	28273.524924	30.666586
489.111549	28320.546403	30.671604
489.441936	28387.007564	30.676621
489.727142	28441.802999	30.681639
490.047577	28493.219800	30.686656
490.639883	28561.368872	30.691674
491.085400	28625.820352	30.696692
491.463600	28685.705549	30.701709
492.028071	28747.322741	30.706727
492.882159	28800.554687	30.711744
493.317287	28849.829480	30.716762
494.140112	28901.883916	30.721780
495.600908	28935.043438	30.726797
496.342194	28973.645899	30.731815
497.256900	29007.659523	30.736832
497.591608	29043.242901	30.741850
498.361768	29075.448273	30.746868
498.612502	29110.225831	30.751885
499.103335	29138.424777	30.756903
499.148282	29173.307134	30.761920
499.416113	29213.433168	30.766938
500.058063	29268.435083	30.771956
500.564040	29306.387603	30.776973
500.911502	29348.137854	30.781991
501.319278	29387.606105	30.787008
501.582739	29436.441824	30.792026
502.157069	29485.098201	30.797044
502.079957	29542.101548	30.802061
502.588889	29589.046648	30.807079
503.330202	29633.585602	30.812096
505.150074	29660.323947	30.817114
505.911403	29688.013599	30.822132
506.524222	29716.198879	30.827149
506.829482	29750.435112	30.832167
507.149678	29777.588364	30.837184
507.459111	29812.395111	30.842202
508.278107	29850.487641	30.847220
508.590644	29885.723123	30.852237
508.621495	29911.039279	30.857255
509.464793	29950.623483	30.862272
509.785476	29986.340534	30.867290
510.070305	30013.560160	30.872308
510.154164	30053.438798	30.877325
510.482070	30091.035409	30.882343
510.665437	30128.710507	30.887360
511.085649	30187.839470	30.892378
511.539647	30231.037643	30.897396
511.438584	30300.126321	30.902413
511.726999	30366.952372	30.907431
512.403822	30425.126245	30.912448
512.566009	30501.787767	30.917466
513.445148	30557.456710	30.922484
513.999302	30621.041729	30.927501
514.594281	30685.279471	30.932519
514.948168	30746.671501	30.937536
515.319611	30817.527176	30.942554
515.950456	30878.395728	30.947572
516.459735	30953.573442	30.952589
517.394271	31013.648877	30.957607
518.056403	31074.086744	30.962624
518.462795	31138.800211	30.967642
518.937058	31205.979391	30.972660
519.778208	31259.959361	30.977677
520.129566	31324.241153	30.982695
520.401795	31385.968091	30.987712
520.873238	31446.370471	30.992730
521.602205	31504.614677	30.997748
522.380073	31572.276514	31.002765
522.444871	31639.284503	31.007783
523.763567	31691.950108	31.012800
523.955087	31745.345462	31.017818
525.081820	31806.791751	31.022836
524.829228	31866.486517	31.027853
525.586321	31915.642083	31.032871
526.174961	31973.523716	31.037888
526.632862	32048.541286	31.042906
526.993668	32112.477170	31.047924
527.872798	32162.350942	31.052941
529.267432	32222.241171	31.057959
530.241235	32251.305880	31.062976
530.562655	32292.224928	31.067994
532.077819	32317.552107	31.073012
532.923941	32333.567730	31.078029
533.252866	32368.092120	31.083047
533.727662	32391.417034	31.088064
534.046442	32423.762640	31.093082
534.826522	32442.803434	31.098100
534.753566	32472.738969	31.103117
535.045195	32505.834138	31.108135
535.177497	32542.705740	31.113152
535.737447	32583.922256	31.118170
535.819171	32630.027090	31.123188
536.340844	32676.346997	31.128205
536.369644	32723.537271	31.133223
537.142438	32767.898806	31.138240
537.443045	32828.672802	31.143258
537.602764	32886.760270	31.148276
538.624082	32925.335974	31.153293
539.121874	32980.765399	31.158311
539.615004	33026.188523	31.163328
539.831930	33087.126057	31.168346
540.579693	33130.729056	31.173364
541.028482	33190.926608	31.178381
541.266512	33250.428301	31.183399
541.883134	33301.748296	31.188416
542.186450	33370.293535	31.193434
542.806270	33426.953177	31.198452
543.452275	33492.912258	31.203469
543.607361	33567.167515	31.208487
544.492536	33626.212413	31.213504
544.715628	33699.380374	31.218522
544.940164	33768.357215	31.223540
545.550298	33829.289853	31.228557
546.348523	33901.072438	31.233575
546.934281	33967.927268	31.238592
547.576039	34031.370531	31.243610
548.879993	34086.564244	31.248628
549.635097	34150.768054	31.253645
550.089062	34212.060131	31.258663
550.710457	34257.322362	31.263680
550.994992	34323.494752	31.268698
551.742100	34380.833082	31.273716
552.344383	34434.143953	31.278733
552.545586	34489.038642	31.283751
553.031960	34543.720518	31.288768
553.586221	34608.720996	31.293786
553.952270	34679.801158	31.298804
554.692015	34736.775765	31.303821
555.539945	34806.498768	31.308839
556.322606	34854.808989	31.313856
556.737026	34912.404847	31.318874
557.444996	34960.873333	31.323892
558.142567	35021.574078	31.328909
558.909135	35075.770840	31.333927
559.390814	35107.537860	31.338944
559.620664	35180.202500	31.343962
560.301406	35226.419646	31.348980
561.056649	35286.729491	31.353997
561.246164	35349.412141	31.359015
562.150454	35390.064763	31.364032
562.457044	35445.057917	31.369050
562.680512	35501.268029	31.374068
563.422542	35561.413767	31.379085
563.787027	35622.075745	31.384103
564.410421	35686.755769	31.389120
564.558429	35749.970862	31.394138
565.017265	35823.028101	31.399156
565.669655	35885.466005	31.404173
566.235830	35951.883309	31.409191
566.569251	36014.811886	31.414208
567.032468	36093.184823	31.419226
567.317743	36162.532820	31.424244
568.041927	36222.819530	31.429261
568.615979	36300.322132	31.434279
568.981837	36364.373208	31.439296
569.350399	36431.864591	31.444314
569.894478	36505.809553	31.449332
570.891405	36584.216261	31.454349
571.105347	36658.969651	31.459367
572.531791	36723.575741	31.464384
573.194543	36789.038906	31.469402
573.257049	36851.874742	31.474420
574.059972	36924.208252	31.479437
574.605592	36991.355710	31.484455
575.501415	37050.242643	31.489472
575.810355	37127.450110	31.494490
576.159756	37190.089592	31.499508
577.019471	37250.710014	31.504525
577.402740	37327.773012	31.509543
578.022450	37395.313306	31.514560
578.918660	37479.296780	31.519578
579.534288	37553.350514	31.524596
579.726142	37618.060808	31.529613
580.005743	37689.069656	31.534631
580.705793	37762.683619	31.539648
581.271205	37832.586561	31.544666
581.957047	37909.057207	31.549684
583.177124	37967.661096	31.554701
583.771972	38037.471387	31.559719
584.587331	38081.826013	31.564736
585.671878	38151.237163	31.569754
586.122184	38204.768197	31.574772
586.905855	38265.805915	31.579789
587.203034	38324.954191	31.584807
587.844072	38372.022655	31.589824
587.980426	38439.308667	31.594842
588.638459	38501.037933	31.599860
589.922219	38544.682064	31.604877
590.427916	38608.666511	31.609895
591.302851	38664.383271	31.614912
592.599405	38682.660285	31.619930
593.843862	38712.380372	31.624948
594.660949	38743.850021	31.629965
594.946871	38773.898587	31.634983
596.069366	38804.356328	31.640000
596.186807	38834.648525	31.645018
596.582763	38857.689053	31.650036
597.336370	38888.270114	31.655053
597.481035	38931.914596	31.660071
597.833307	38962.700286	31.665088
598.316815	39003.739269	31.670106
598.916989	39043.037838	31.675124
599.926911	39082.307331	31.680141
599.990550	39125.252688	31.685159
600.560791	39161.567029	31.690176
600.461614	39208.590819	31.695194
601.009914	39259.790937	31.700212
601.754340	39308.962397	31.705229
601.693472	39353.343932	31.710247
601.743436	39417.971204	31.715264
602.123748	39481.812841	31.720282
602.294079	39552.964398	31.725300
602.936828	39618.778868	31.730317
603.104423	39702.174356	31.735335
603.525074	39788.926996	31.740352
603.958557	39869.711011	31.745370
604.192152	39966.479131	31.750388
604.812150	40069.344189	31.755405
605.286746	40163.448507	31.760423
605.916908	40254.928340	31.765440
606.401538	40355.964947	31.770458
607.016663	40458.128949	31.775476
607.871902	40543.986640	31.780493
608.816833	40646.136215	31.785511
609.414553	40748.626826	31.790528
610.298374	40832.491915	31.795546
611.432757	40914.619022	31.800564
613.135467	40969.067461	31.805581
614.046849	41036.460595	31.810599
614.989485	41105.259914	31.815616
615.711665	41161.136651	31.820634
616.486626	41218.273740	31.825652
617.258521	41268.594938	31.830669
617.290731	41337.364810	31.835687
617.797290	41395.129367	31.840704
618.515512	41462.715000	31.845722
619.039796	41517.846850	31.850740
619.908877	41570.321300	31.855757
620.425937	41634.238456	31.860775
620.653712	41694.564953	31.865792
621.371690	41748.268745	31.870810
621.932154	41814.509222	31.875828
622.544410	41879.980128	31.880845
623.018508	41957.845646	31.885863
623.288488	42022.952598	31.890880
624.283702	42095.406006	31.895898
624.345749	42179.032723	31.900916
625.277241	42249.492667	31.905933
625.586877	42324.044136	31.910951
626.049028	42404.149041	31.915968
626.750172	42484.598558	31.920986
627.231641	42571.044273	31.926004
628.059261	42651.204448	31.931021
628.661476	42740.105753	31.936039
629.246154	42813.241670	31.941056
629.884005	42891.859765	31.946074
630.280719	42983.885524	31.951092
630.657360	43057.891634	31.956109
631.401468	43143.363494	31.961127
631.582318	43236.324227	31.966144
632.353256	43314.431853	31.971162
632.758531	43396.704232	31.976180
633.961103	43479.528748	31.981197
634.613820	43559.069117	31.986215
635.472731	43636.626202	31.991232
636.478161	43709.516686	31.996250
637.368861	43777.576862	32.001268
638.137378	43830.605358	32.006285
639.076334	43898.701912	32.011303
639.775155	43962.472694	32.016320
640.575899	44019.778099	32.021338
640.789588	44084.977607	32.026356
641.531725	44143.837574	32.031373
641.805681	44211.954449	32.036391
642.326707	44287.058495	32.041408
643.434924	44350.956234	32.046426
643.295858	44424.225540	32.051444
644.255411	44497.411128	32.056461
644.836000	44569.534570	32.061479
645.136695	44648.956673	32.066496
645.838116	44725.029432	32.071514
646.321917	44807.954487	32.076532
646.948218	44885.174436	32.081549
647.696205	44965.209655	32.086567
648.365834	45053.058704	32.091584
648.945645	45133.202389	32.096602
649.402950	45220.760161	32.101620
650.064102	45306.227579	32.106637
650.769018	45388.185683	32.111655
651.145081	45480.631330	32.116672
652.034607	45567.519789	32.121690
652.784187	45655.525296	32.126708
653.623627	45739.315625	32.131725
654.182679	45828.166184	32.136743
654.888477	45916.597258	32.141760
656.141705	45988.048709	32.146778
656.391967	46068.129616	32.151796
657.162635	46152.527262	32.156813
658.177077	46228.252382	32.161831
658.696930	46308.025985	32.166848
659.627412	46392.116238	32.171866
659.750094	46467.322389	32.176884
660.743584	46540.251049	32.181901
661.556086	46620.569557	32.186919
661.681167	46706.741448	32.191936
662.804533	46784.866133	32.196954
663.268832	46865.422177	32.201972
663.766246	46941.845073	32.206989
664.636761	47025.885216	32.212007
664.873912	47111.736534	32.217024
665.476274	47191.736549	32.222042
665.685060	47285.517618	32.227060
666.543977	47371.667842	32.232077
667.313535	47456.620966	32.237095
667.672728	47545.737965	32.242112
668.115116	47630.400486	32.247130
668.780158	47714.428306	32.252148
669.694942	47796.809254	32.257165
670.969245	47869.874890	32.262183
672.118060	47934.406199	32.267200
673.116323	48002.466190	32.272218
674.141125	48065.057810	32.277236
675.018385	48121.639151	32.282253
675.244555	48190.147915	32.287271
675.731685	48256.303390	32.292288
676.330767	48318.236001	32.297306
676.861513	48394.996909	32.302324
677.618725	48457.664071	32.307341
678.346941	48529.458135	32.312359
678.802518	48603.971268	32.317376
679.386353	48679.397638	32.322394
679.922920	48755.375667	32.327412
680.272606	48842.099793	32.332429
680.994144	48920.662059	32.337447
681.832948	49000.354276	32.342464
682.824832	49070.311110	32.347482
683.869405	49142.508091	32.352500
684.920072	49199.302936	32.357517
685.945992	49264.245096	32.362535
686.803854	49324.004531	32.367552
687.741312	49376.599370	32.372570
688.359659	49445.591835	32.377588
688.659097	49501.467587	32.382605
689.431697	49570.105570	32.387623
689.663303	49636.429561	32.392640
690.492239	49697.610189	32.397658
691.039451	49766.262206	32.402676
691.223075	49836.461341	32.407693
692.178812	49907.766681	32.412711
692.646588	49994.102992	32.417728
693.264164	50061.404693	32.422746
693.572893	50146.379077	32.427764
694.412772	50230.719533	32.432781
695.282779	50308.326983	32.437799
695.687463	50395.850948	32.442816
696.539875	50478.307684	32.447834
697.253224	50560.567474	32.452852
697.731594	50651.573622	32.457869
698.127954	50736.478702	32.462887
698.718117	50826.815791	32.467904
699.840681	50904.868814	32.472922
700.555964	50991.280853	32.477940
701.282873	51083.990147	32.482957
702.538077	51163.348223	32.487975
703.420066	51243.888816	32.492992
703.909638	51320.921034	32.498010
704.410278	51393.541751	32.503028
704.925693	51488.304602	32.508045
705.661157	51569.446566	32.513063
706.044470	51648.077764	32.518080
706.642051	51731.796490	32.523098
707.175282	51820.998031	32.528116
707.439596	51907.687219	32.533133
708.119151	51986.591245	32.538151
708.320182	52090.944882	32.543168
709.183256	52183.667633	32.548186
709.445754	52285.952048	32.553204
710.314256	52384.260107	32.558221
711.271642	52479.078383	32.563239
712.520136	52573.537652	32.568256
713.852597	52655.681213	32.573274
714.387445	52750.092981	32.578292
715.044209	52831.563228	32.583309
715.999246	52910.809185	32.588327
716.652100	53005.675840	32.593344
717.737805	53096.924145	32.598362
719.520721	53152.372946	32.603380
719.977790	53230.271192	32.608397
720.713301	53299.737358	32.613415
721.503803	53379.360899	32.618432
722.283181	53442.627872	32.623450
722.639040	53526.976930	32.628468
723.198523	53597.270437	32.633485
723.834863	53672.030948	32.638503
724.342351	53759.008851	32.643520
724.744705	53841.601008	32.648538
725.429258	53937.439774	32.653556
725.717026	54028.683725	32.658573
726.468241	54110.022993	32.663591
727.043701	54209.407640	32.668608
727.216658	54315.742957	32.673626
728.041541	54431.748805	32.678644
728.938546	54543.837878	32.683661
729.922200	54640.513443	32.688679
730.634971	54751.807462	32.693696
731.074627	54843.623110	32.698714
731.811310	54946.459273	32.703732
732.413617	55062.570105	32.708749
732.957793	55170.072286	32.713767
733.878583	55280.752258	32.718784
734.636321	55385.166860	32.723802
735.469882	55490.333645	32.728820
736.320257	55598.916819	32.733837
737.484318	55691.212598	32.738855
738.047712	55796.427268	32.743872
739.110972	55892.861439	32.748890
740.201830	55986.327558	32.753908
741.222428	56072.955912	32.758925
742.421684	56152.343566	32.763943
743.235519	56237.548260	32.768960
744.054321	56311.061422	32.773978
745.590925	56384.015854	32.778996
746.471763	56466.909745	32.784013
747.424572	56523.660307	32.789031
747.804900	56584.591530	32.794048
748.733412	56621.913875	32.799066
749.921266	56667.382057	32.804084
750.369378	56725.287650	32.809101
751.063417	56766.081976	32.814119
751.659286	56830.433857	32.819136
752.447702	56895.479723	32.824154
753.148046	56942.624589	32.829172
753.343154	57007.431182	32.834189
753.730971	57062.093427	32.839207
754.192064	57140.714027	32.844224
754.921250	57222.012830	32.849242
755.352883	57292.309618	32.854260
755.798587	57387.352627	32.859277
756.488709	57475.686780	32.864295
757.244451	57562.430110	32.869312
757.793933	57649.992810	32.874330
758.489001	57736.627201	32.879348
759.016656	57831.506580	32.884365
760.019149	57917.741489	32.889383
760.583115	58028.959053	32.894400
761.249257	58125.250728	32.899418
762.192653	58224.484765	32.904436
762.178523	58330.904943	32.909453
763.333161	58428.536406	32.914471
764.387341	58535.615244	32.919488
765.292793	58629.770021	32.924506
766.113922	58738.855432	32.929524
766.633272	58845.717820	32.934541
767.487216	58947.871714	32.939559
768.298533	59048.004594	32.944576
768.850073	59150.489396	32.949594
769.502968	59257.918862	32.954612
769.943016	59382.867671	32.959629
771.044115	59494.127638	32.964647
771.649148	59602.098031	32.969664
772.585761	59715.479464	32.974682
773.527032	59816.434483	32.979700
774.095618	59931.485575	32.984717
775.358223	60032.045304	32.989735
775.724040	60155.361854	32.994752
775.794020	60269.590068	32.999770
776.980884	60395.599104	33.004788
777.489238	60512.199709	33.009805
778.034393	60636.531356	33.014823
778.710547	60762.718611	33.019840
779.595766	60893.839058	33.024858
780.485318	61012.222903	33.029876
780.812687	61147.422705	33.034893
781.745742	61262.911851	33.039911
782.892598	61395.672064	33.044928
783.713944	61520.707619	33.049946
784.842691	61637.985819	33.054964
785.488285	61757.389178	33.059981
786.759497	61865.036097	33.064999
787.920504	61967.582256	33.070016
788.942311	62059.191703	33.075034
790.125534	62148.409747	33.080052
790.594595	62247.156614	33.085069
791.305648	62332.594003	33.090087
791.737489	62433.800813	33.095104
792.437670	62539.172208	33.100122
793.011211	62637.517429	33.105140
793.806638	62749.251902	33.110157
794.593274	62854.003224	33.115175
795.129075	62963.950084	33.120192
796.094799	63069.164893	33.125210
797.105696	63169.839914	33.130228
797.556031	63283.829956	33.135245
798.499638	63399.379766	33.140263
799.587118	63506.459785	33.145280
800.391549	63611.749211	33.150298
801.280817	63716.297635	33.155316
802.299125	63833.088759	33.160333
802.901183	63934.362203	33.165351
803.806667	64039.168658	33.170368
804.330776	64139.830583	33.175386
805.733181	64246.892065	33.180404
806.295360	64353.219257	33.185421
807.216184	64450.306040	33.190439
808.099379	64560.745487	33.195456
809.168812	64665.969537	33.200474
809.983929	64764.776511	33.205492
810.531377	64864.868929	33.210509
811.109301	64966.796344	33.215527
812.176568	65072.364196	33.220544
813.199657	65173.590472	33.225562
814.718329	65258.345142	33.230580
815.158246	65361.069415	33.235597
816.421937	65453.019013	33.240615
817.652197	65543.052757	33.245632
818.801315	65616.352922	33.250650
819.659746	65689.589328	33.255668
820.765982	65767.910992	33.260685
821.397784	65855.620781	33.265703
822.216145	65917.977668	33.270720
823.191295	65991.662991	33.275738
823.898391	66066.462979	33.280756
824.522980	66150.027687	33.285773
824.843573	66230.230634	33.290791
825.750009	66316.927953	33.295808
826.290888	66411.003447	33.300826
826.940505	66501.380984	33.305844
827.611001	66587.987048	33.310861
828.245657	66691.164944	33.315879
829.051273	66792.316092	33.320896
829.845882	66870.328495	33.325914
831.657534	66948.015247	33.330932
832.978996	67026.576586	33.335949
833.531448	67109.417666	33.340967
834.590396	67174.828886	33.345984
835.113603	67250.284177	33.351002
835.894061	67316.382135	33.356020
836.976468	67394.283942	33.361037
837.366136	67462.845651	33.366055
837.968048	67536.290445	33.371072
838.621764	67628.240150	33.376090
839.079752	67710.277764	33.381108
839.251614	67807.520883	33.386125
839.680592	67900.838078	33.391143
840.640186	68005.882561	33.396160
840.710976	68123.144212	33.401178
842.165050	68235.990012	33.406196
842.554270	68354.229055	33.411213
842.994465	68478.100296	33.416231
844.022741	68589.275687	33.421248
844.102024	68723.624492	33.426266
844.960640	68858.295935	33.431284
845.950878	68993.483163	33.436301
846.496863	69135.899062	33.441319
847.419676	69275.380532	33.446336
847.893323	69422.863125	33.451354
848.907388	69561.243182	33.456372
849.681120	69715.606935	33.461389
850.636025	69857.723592	33.466407
851.534045	69998.434434	33.471424
852.077371	70138.410157	33.476442
853.632848	70284.151397	33.481460
854.476650	70438.944646	33.486477
855.351546	70577.949477	33.491495
856.658059	70704.916582	33.496512
857.326968	70855.556381	33.501530
858.396211	70988.402719	33.506548
859.384544	71123.881844	33.511565
860.733373	71256.327795	33.516583
861.862198	71373.052753	33.521600
862.778728	71494.734816	33.526618
863.843968	71613.868775	33.531636
864.707356	71745.015861	33.536653
865.394752	71871.476044	33.541671
866.761083	71994.026157	33.546688
867.419894	72117.153477	33.551706
868.098554	72237.033737	33.556724
868.808080	72357.453257	33.561741
869.227684	72489.762270	33.566759
870.210642	72617.510581	33.571776
870.574041	72757.407447	33.576794
871.720861	72891.067922	33.581812
872.914415	73022.836506	33.586829
873.555089	73151.000712	33.591847
874.662103	73287.263476	33.596864
875.293211	73418.289586	33.601882
876.402935	73544.282302	33.606900
878.089084	73664.592320	33.611917
878.970407	73784.914339	33.616935
880.151090	73889.044975	33.621952
880.871056	73997.347140	33.626970
882.169812	74105.632933	33.631988
882.509111	74199.213876	33.637005
883.590449	74306.772584	33.642023
884.388878	74405.202839	33.647040
885.351276	74513.731658	33.652058
886.339672	74607.696504	33.657076
887.162512	74714.940944	33.662093
888.481287	74813.214322	33.667111
889.614732	74904.612931	33.672128
890.166849	75002.816046	33.677146
891.787092	75092.607719	33.682164
892.767175	75194.489168	33.687181
893.396993	75294.976286	33.692199
894.152942	75380.900674	33.697216
894.595220	75482.907174	33.702234
895.466360	75588.439751	33.707252
896.355672	75693.273936	33.712269
896.788371	75801.210304	33.717287
897.680522	75911.712493	33.722304
898.124998	76036.188710	33.727322
898.844316	76147.208715	33.732340
899.494302	76276.293909	33.737357
900.385219	76409.013681	33.742375
901.570644	76522.909716	33.747392
902.895382	76651.527288	33.752410
903.484189	76774.939176	33.757428
904.851868	76899.243102	33.762445
905.014522	77033.634736	33.767463
906.186114	77157.379061	33.772480
906.627808	77288.681779	33.777498
907.562630	77415.668884	33.782516
908.882315	77534.348298	33.787533
909.795927	77666.179671	33.792551
910.593462	77790.510251	33.797568
911.719356	77926.203513	33.802586
912.394131	78056.857171	33.807604
913.446901	78186.327153	33.812621
914.032731	78320.179523	33.817639
914.809425	78453.708999	33.822656
915.247458	78607.711514	33.827674
916.242644	78746.943053	33.832692
917.360207	78886.647929	33.837709
918.361810	79031.440808	33.842727
919.103274	79165.606795	33.847744
920.087637	79311.555784	33.852762
920.897659	79462.115819	33.857780
921.751405	79599.453596	33.862797
922.972882	79749.027738	33.867815
924.298253	79894.719615	33.872832
925.033114	80036.686028	33.877850
925.642806	80181.452098	33.882868
927.123001	80320.584882	33.887885
927.694037	80458.381131	33.892903
928.734596	80578.155479	33.897920
929.680864	80705.038787	33.902938
930.558772	80833.800879	33.907956
931.347818	80957.745287	33.912973
932.268164	81092.518282	33.917991
933.895262	81212.581426	33.923008
935.113776	81333.853998	33.928026
935.738754	81462.593327	33.933044
936.866295	81579.283136	33.938061
937.314391	81711.559249	33.943079
938.358909	81829.049079	33.948096
939.653776	81959.416376	33.953114
940.313748	82079.232072	33.958132
941.578884	82194.895428	33.963149
942.840026	82309.516076	33.968167
944.436922	82409.824768	33.973184
946.220485	82518.934641	33.978202
946.966851	82628.007523	33.983220
947.986829	82727.498946	33.988237
948.634638	82835.627944	33.993255
949.273034	82944.043783	33.998272
949.841232	83059.115818	34.003290
950.249931	83174.335955	34.008308
951.719852	83294.677264	34.013325
951.882960	83428.448275	34.018343
952.671486	83558.531618	34.023360
953.419926	83699.221074	34.028378
953.908936	83836.235224	34.033396
954.850955	83981.645194	34.038413
955.393073	84137.470167	34.043431
956.013095	84293.295489	34.048448
956.787215	84455.283930	34.053466
957.351126	84613.335673	34.058484
958.429189	84773.534133	34.063501
959.134618	84952.882182	34.068519
960.189072	85119.623676	34.073536
961.222910	85296.519842	34.078554
961.852877	85475.163403	34.083572
963.303061	85634.057380	34.088589
964.068975	85820.432068	34.093607
965.599225	85976.928964	34.098624
966.680952	86137.009488	34.103642
967.396881	86305.854975	34.108660
968.947908	86458.522947	34.113677
969.907371	86629.075617	34.118695
970.841298	86788.869431	34.123712
972.720644	86950.223732	34.128730
973.059397	87105.875270	34.133748
974.629850	87254.026551	34.138765
975.262384	87413.604041	34.143783
976.202631	87563.390321	34.148800
977.438254	87718.550528	34.153818
978.112732	87874.383733	34.158836
979.430131	88020.298476	34.163853
980.266709	88165.473716	34.168871
981.218594	88318.287826	34.173888
982.212215	88460.311574	34.178906
982.700015	88610.283129	34.183924
983.742827	88750.477475	34.188941
984.475604	88908.471859	34.193959
985.215196	89065.187671	34.198976
986.588008	89213.346925	34.203994
987.468824	89370.072178	34.209012
988.660255	89524.542755	34.214029
989.510410	89677.313278	34.219047
990.684601	89822.890045	34.224064
991.804292	89975.350470	34.229082
993.174572	90121.648622	34.234100
994.635843	90257.723045	34.239117
996.071083	90391.587450	34.244135
997.268930	90528.721180	34.249152
998.273094	90659.350658	34.254170
999.126506	90783.962117	34.259188
1000.282254	90907.883174	34.264205
1001.221004	91050.653057	34.269223
1002.156392	91197.278993	34.274240
1002.966359	91333.217773	34.279258
1003.440622	91473.430261	34.284276
1004.307086	91620.747795	34.289293
1005.191528	91779.975461	34.294311
1006.156348	91935.253353	34.299328
1006.769113	92087.383357	34.304346
1007.481304	92253.637897	34.309364
1008.015235	92414.948879	34.314381
1008.887769	92596.433037	34.319399
1009.714223	92775.647667	34.324416
1010.925005	92945.632075	34.329434
1011.731884	93127.194672	34.334452
1013.096194	93298.883297	34.339469
1014.541265	93474.338321	34.344487
1015.822818	93640.276812	34.349504
1016.778865	93802.442422	34.354522
1017.581250	93974.909271	34.359540
1019.165541	94136.861873	34.364557
1020.089731	94300.023695	34.369575
1021.492707	94461.749917	34.374592
1023.338970	94608.164167	34.379610
1024.220490	94761.986416	34.384628
1025.408881	94909.641888	34.389645
1026.943236	95054.168727	34.394663
1027.636297	95195.181436	34.399680
1028.979240	95333.222266	34.404698
1029.880408	95485.538933	34.409716
1030.713982	95624.162365	34.414733
1031.779987	95773.204958	34.419751
1032.308309	95922.296187	34.424768
1033.158066	96071.630801	34.429786
1033.607887	96232.917581	34.434804
1035.030892	96389.164052	34.439821
1036.755429	96542.593291	34.444839
1037.329509	96696.100167	34.449856
1038.395030	96816.444909	34.454874
1039.208601	96973.590706	34.459892
1040.156611	97110.619975	34.464909
1041.046106	97259.663575	34.469927
1041.433817	97408.217845	34.474944
1042.364044	97568.031705	34.479962
1043.249136	97731.526344	34.484980
1044.212727	97898.446410	34.489997
1044.863536	98073.214832	34.495015
1045.272743	98252.888214	34.500032
1045.911604	98444.280743	34.505050
1046.861896	98635.520075	34.510068
1048.138578	98829.554072	34.515085
1049.034351	99031.144848	34.520103
1049.700453	99235.074860	34.525120
1051.133415	99423.495881	34.530138
1052.066191	99633.689597	34.535156
1053.070725	99832.488457	34.540173
1054.729668	100026.681302	34.545191
1055.649905	100225.478623	34.550208
1057.199102	100413.583046	34.555226
1058.340224	100608.451444	34.560244
1059.887020	100797.781107	34.565261
1061.229667	100983.493591	34.570279
1062.190990	101169.709598	34.575296
1063.472838	101350.850774	34.580314
1064.541082	101540.071485	34.585332
1065.403593	101725.884134	34.590349
1066.532572	101913.678762	34.595367
1067.312502	102096.912007	34.600384
1068.854132	102288.298670	34.605402
1069.701925	102471.484918	34.610420
1071.283786	102656.066512	34.615437
1072.770723	102825.974575	34.620455
1073.977168	102993.652097	34.625472
1075.882672	103152.383572	34.630490
1077.062063	103324.221910	34.635508
1078.014255	103492.908676	34.640525
1079.253585	103638.484178	34.645543
1079.810943	103808.747708	34.650560
1081.376658	103973.963553	34.655578
1082.591798	104131.666574	34.660596
1083.303858	104289.849296	34.665613
1084.664824	104450.252307	34.670631
1085.531716	104611.956774	34.675648
1086.934704	104757.409068	34.680666
1087.627423	104930.215061	34.685684
1088.233931	105086.812039	34.690701
1089.673601	105257.579723	34.695719
1090.701321	105419.628854	34.700736
1091.836674	105585.029703	34.705754
1092.919163	105754.063132	34.710772
1093.655958	105920.281587	34.715789
1094.540278	106086.019825	34.720807
1095.208385	106256.647315	34.725824
1096.526114	106417.221513	34.730842
1097.517564	106586.288423	34.735860
1098.954386	106743.449550	34.740877
1100.482038	106901.090040	34.745895
1101.320744	107050.033366	34.750912
1102.528950	107200.307595	34.755930
1103.354013	107361.655763	34.760948
1104.640896	107520.899110	34.765965
1105.670459	107690.485733	34.770983
1106.544477	107861.607429	34.776000
1107.750333	108025.719104	34.781018
1108.577643	108182.017549	34.786036
1109.462889	108363.337609	34.791053
1110.546841	108543.497450	34.796071
1111.151233	108729.187609	34.801088
1111.969851	108908.217199	34.806106
1112.525301	109108.194674	34.811124
1113.539913	109318.051857	34.816141
1114.782284	109514.228353	34.821159
1115.659703	109723.833424	34.826176
1116.442277	109933.950380	34.831194
1117.738956	110145.881135	34.836212
1118.897883	110353.327201	34.841229
1120.870079	110559.090044	34.846247
1121.557127	110767.886836	34.851264
1123.291003	110970.843137	34.856282
1124.339350	111171.929315	34.861300
1125.314806	111381.960866	34.866317
1126.937897	111578.099453	34.871335
1128.103680	111790.951976	34.876352
1129.616602	111981.727976	34.881370
1130.400661	112175.556619	34.886388
1131.339822	112390.935636	34.891405
1132.552779	112588.469110	34.896423
1133.555258	112791.627191	34.901440
1135.404187	112973.901946	34.906458
1136.960418	113163.677669	34.911476
1138.467774	113343.796129	34.916493
1140.435322	113517.362744	34.921511
1141.479947	113700.020612	34.926528
1142.967967	113868.134792	34.931546
1144.228332	114037.758653	34.936564
1145.210795	114205.441917	34.941581
1146.160240	114375.057671	34.946599
1146.962733	114543.065146	34.951616
1147.725965	114716.769255	34.956634
1149.051830	114907.875767	34.961652
1150.413479	115079.515734	34.966669
1151.377707	115252.365110	34.971687
1152.376355	115429.504942	34.976704
1153.254604	115607.794164	34.981722
1154.885705	115778.568594	34.986740
1155.678043	115963.602860	34.991757
1156.776490	116144.657947	34.996775
1157.557276	116324.184688	35.001792
1158.717718	116491.838179	35.006810
1159.665550	116673.201124	35.011828
1160.663305	116863.223726	35.016845
1161.423665	117037.449172	35.021863
1162.408605	117228.946223	35.026880
1163.142280	117426.823250	35.031898
1164.203531	117630.993954	35.036916
1165.005318	117839.645560	35.041933
1166.211487	118033.720366	35.046951
1167.050447	118246.828937	35.051968
1168.265166	118457.682497	35.056986
1169.861412	118659.728620	35.062004
1171.380622	118875.297698	35.067021
1173.186012	119068.389721	35.072039
1174.452134	119277.808413	35.077056
1175.532639	119476.907111	35.082074
1176.822992	119673.538128	35.087092
1177.749350	119872.893982	35.092109
1178.976299	120070.679010	35.097127
1180.144952	120276.953320	35.102144
1181.547515	120476.979388	35.107162
1182.183396	120688.492879	35.112180
1183.155497	120908.225706	35.117197
1184.215953	121123.357402	35.122215
1185.448031	121346.584704	35.127232
1186.704135	121569.834901	35.132250
1187.674434	121792.666775	35.137268
1188.706885	122021.395445	35.142285
1190.226921	122229.929606	35.147303
1191.378841	122467.145089	35.152320
1192.608952	122677.975195	35.157338
1194.171766	122894.313579	35.162356
1195.311571	123125.148731	35.167373
1196.924276	123340.670630	35.172391
1198.137962	123566.579007	35.177408
1198.971238	123783.035931	35.182426
1200.552767	124005.678039	35.187444
1201.280675	124224.589571	35.192461
1203.276264	124436.707652	35.197479
1204.838624	124648.508458	35.202496
1206.157409	124854.370038	35.207514
1207.502995	125057.706157	35.212532
1208.349370	125276.186633	35.217549
1209.190963	125468.686137	35.222567
1210.908732	125688.465278	35.227584
1212.305710	125894.472504	35.232602
1213.507782	126093.226311	35.237620
1214.812061	126310.862514	35.242637
1216.249137	126514.053103	35.247655
1217.440212	126714.929523	35.252672
1218.247132	126913.388623	35.257690
1219.554475	127116.706745	35.262708
1220.888666	127320.870852	35.267725
1222.105370	127516.855271	35.272743
1223.269078	127705.789618	35.277760
1224.580714	127889.109760	35.282778
1226.123873	128076.992668	35.287796
1227.281688	128254.903330	35.292813
1228.698209	128440.262218	35.297831
1229.732533	128628.590440	35.302848
1230.513578	128815.011011	35.307866
1231.720898	129016.659903	35.312884
1232.466890	129215.904490	35.317901
1233.432522	129415.493015	35.322919
1234.525777	129622.856966	35.327936
1235.326229	129844.723653	35.332954
1236.447546	130060.578928	35.337972
1237.613786	130280.015479	35.342989
1238.646952	130506.676738	35.348007
1239.741411	130734.812298	35.353024
1240.757566	130972.965025	35.358042
1242.151058	131212.386007	35.363060
1243.037440	131454.519746	35.368077
1244.148508	131696.236511	35.373095
1245.229191	131943.157998	35.378112
1246.214044	132187.727073	35.383130
1247.736748	132438.417919	35.388148
1249.083566	132701.007092	35.393165
1250.381710	132945.160551	35.398183
1251.859725	133207.300276	35.403200
1253.613673	133447.094321	35.408218
1254.990907	133695.296756	35.413236
1256.083971	133943.486309	35.418253
1257.365245	134184.254091	35.423271
1258.989762	134434.384866	35.428288
1259.776426	134673.998389	35.433306
1261.697737	134915.714220	35.438324
1262.797892	135170.999017	35.443341
1264.055361	135407.202738	35.448359
1265.322314	135645.828149	35.453376
1266.626036	135897.546253	35.458394
1267.991529	136150.853218	35.463412
1268.886195	136405.421836	35.468429
1270.311498	136654.107156	35.473447
1271.512249	136901.044965	35.478464
1273.017297	137154.310200	35.483482
1274.979540	137382.647341	35.488500
1276.514285	137615.623823	35.493517
1278.353661	137852.087364	35.498535
1279.689969	138077.886266	35.503552
1281.191404	138305.763235	35.508570
1282.983207	138521.305221	35.513588
1284.001857	138738.515178	35.518605
1285.687045	138943.059186	35.523623
1287.411818	139143.375160	35.528640
1288.743527	139343.607417	35.533658
1290.315078	139541.174967	35.538676
1291.376253	139753.261205	35.543693
1292.423899	139945.556961	35.548711
1294.334943	140131.898342	35.553728
1294.787190	140322.903247	35.558746
1296.092308	140501.057255	35.563764
1297.185479	140704.242029	35.568781
1298.251060	140890.757539	35.573799
1299.471480	141083.537212	35.578816
1300.317507	141286.995917	35.583834
1301.425004	141486.226329	35.588852
1302.374874	141700.664026	35.593869
1303.380496	141918.745637	35.598887
1304.885523	142138.569197	35.603904
1305.523759	142368.408507	35.608922
1306.644944	142595.364059	35.613940
1307.522053	142842.868698	35.618957
1308.485161	143082.307569	35.623975
1309.607763	143336.165085	35.628992
1310.833944	143594.838393	35.634010
1312.230720	143841.652257	35.639028
1313.001245	144107.597814	35.644045
1314.558538	144373.753071	35.649063
1315.908503	144641.239344	35.654080
1317.108328	144910.782433	35.659098
1318.346504	145181.944282	35.664116
1319.343650	145460.834904	35.669133
1320.177392	145739.400513	35.674151
1321.903096	146024.562676	35.679168
1323.355936	146310.357159	35.684186
1325.277962	146585.115668	35.689204
1326.766814	146860.559142	35.694221
1328.282546	147131.104457	35.699239
1330.018701	147401.918408	35.704256
1331.384994	147669.779059	35.709274
1333.223761	147931.866009	35.714292
1334.467995	148199.180606	35.719309
1336.134463	148448.604702	35.724327
1337.539961	148702.311396	35.729344
1339.071681	148971.319914	35.734362
1340.492017	149226.638407	35.739380
1341.622080	149481.957572	35.744397
1343.107834	149736.240921	35.749415
1344.609202	149986.540560	35.754432
1345.683664	150255.902814	35.759450
1347.071395	150506.707305	35.764468
1348.016771	150767.571571	35.769485
1349.344302	151039.470898	35.774503
1350.448428	151300.831662	35.779520
1351.373134	151584.118190	35.784538
1352.776327	151854.982873	35.789556
1354.143976	152132.172457	35.794573
1355.306473	152424.455845	35.799591
1356.667886	152702.944393	35.804608
1357.690250	152994.761325	35.809626
1359.356390	153280.762007	35.814644
1360.526857	153564.249171	35.819661
1361.772958	153852.888279	35.824679
1363.362136	154123.952465	35.829696
1364.287904	154395.335015	35.834714
1366.004246	154659.023605	35.839732
1367.375913	154922.734876	35.844749
1369.245252	155189.178904	35.849767
1370.847541	155429.030547	35.854784
1372.831311	155696.384412	35.859802
1374.480566	155947.267695	35.864820
1375.524308	156209.813018	35.869837
1376.850150	156471.284196	35.874855
1378.343878	156712.417957	35.879872
1379.563391	156972.248685	35.884890
1381.509966	157226.349324	35.889908
1382.961025	157469.588089	35.894925
1384.348669	157719.410684	35.899943
1386.251955	157946.729617	35.904960
1387.543724	158211.173691	35.909978
1388.720754	158450.798755	35.914996
1390.419603	158706.206907	35.920013
1391.163475	158958.253162	35.925031
1392.352822	159211.607561	35.930048
1393.394262	159480.479512	35.935066
1394.974908	159737.703067	35.940084
1396.325890	160015.672782	35.945101
1397.325760	160289.809472	35.950119
1398.857270	160554.011667	35.955136
1400.405390	160826.002672	35.960154
1401.583897	161094.125590	35.965172
1402.971714	161357.469263	35.970189
1404.403453	161644.964123	35.975207
1405.753271	161921.449385	35.980224
1406.950845	162199.383506	35.985242
1408.364110	162477.726577	35.990260
1409.783679	162757.960857	35.995277
1411.131388	163052.622766	36.000295
1412.715488	163329.356076	36.005312
1414.036521	163629.469625	36.010330
1414.887111	163913.843547	36.015348
1416.389729	164208.664379	36.020365
1417.398728	164513.506667	36.025383
1418.629650	164815.838827	36.030400
1420.315891	165124.515533	36.035418
1421.131748	165440.182523	36.040436
1422.599162	165761.450167	36.045453
1423.551138	166084.673587	36.050471
1425.024536	166408.901340	36.055488
1426.029595	166753.475932	36.060506
1427.188120	167081.492969	36.065524
1428.914406	167411.179004	36.070541
1429.690036	167755.546672	36.075559
1431.157515	168105.381856	36.080576
1432.358738	168455.823607	36.085594
1433.656704	168808.218346	36.090612
1435.525033	169149.592338	36.095629
1437.252557	169506.626735	36.100647
1438.993723	169831.238913	36.105664
1440.374439	170162.183863	36.110682
1441.849291	170491.389184	36.115700
1443.786803	170809.857912	36.120717
1445.028536	171124.958047	36.125735
1447.109582	171439.942009	36.130752
1448.144224	171764.510701	36.135770
1449.902505	172082.549061	36.140788
1451.677369	172413.734095	36.145805
1452.845095	172736.484505	36.150823
1454.543687	173044.082327	36.155840
1455.891847	173376.895230	36.160858
1457.370101	173689.281189	36.165876
1458.645250	174008.963128	36.170893
1459.839586	174340.971289	36.175911
1461.335161	174663.284863	36.180928
1462.891319	174990.425514	36.185946
1464.808053	175322.583126	36.190964
1466.787376	175642.218528	36.195981
1468.149460	175965.921330	36.200999
1469.786591	176285.809751	36.206016
1470.765601	176610.039129	36.211034
1472.017983	176943.184134	36.216052
1473.800549	177278.347418	36.221069
1475.464919	177599.902048	36.226087
1477.326880	177911.157087	36.231104
1479.168704	178244.171578	36.236122
1480.912684	178554.460695	36.241140
1482.685381	178854.199545	36.246157
1484.330732	179165.346854	36.251175
1486.093277	179465.535166	36.256192
1487.747888	179770.084458	36.261210
1489.627927	180076.348485	36.266228
1491.291587	180364.627897	36.271245
1492.596956	180659.202252	36.276263
1493.799639	180965.523834	36.281280
1495.110378	181263.806850	36.286298
1495.995127	181575.085704	36.291316
1497.456779	181877.763380	36.296333
1498.753117	182204.206878	36.301351
1500.086500	182504.206376	36.306368
1501.454359	182827.848880	36.311386
1502.771531	183150.918070	36.316404
1504.378944	183466.323518	36.321421
1505.649767	183789.239341	36.326439
1507.013660	184117.764282	36.331456
1508.655601	184451.067088	36.336474
1509.967231	184791.384459	36.341492
1511.549431	185118.265787	36.346509
1512.670477	185473.230229	36.351527
1514.402586	185823.560621	36.356544
1515.697530	186172.190816	36.361562
1517.026128	186516.006350	36.366580
1518.618348	186864.310572	36.371597
1520.064860	187201.851829	36.376615
1521.425821	187538.178334	36.381632
1523.135545	187854.377495	36.386650
1524.500521	188249.976758	36.391668
1526.211243	188582.618767	36.396685
1527.111298	188921.380437	36.401703
1528.658420	189265.821994	36.406720
1529.996580	189597.073496	36.411738
1530.865479	189958.569645	36.416756
1532.653790	190311.087751	36.421773
1534.046278	190664.868929	36.426791
1535.814231	191020.352474	36.431808
1537.244124	191382.014878	36.436826
1538.576844	191740.585721	36.441844
1540.947252	192091.033907	36.446861
1542.245061	192468.403637	36.451879
1543.765818	192813.047170	36.456896
1545.658190	193165.106522	36.461914
1547.081835	193522.034176	36.466932
1549.390823	193866.802400	36.471949
1551.493648	194221.421381	36.476967
1553.054707	194573.494310	36.481984
1554.524562	194917.776899	36.487002
1556.104493	195262.194798	36.492020
1557.925358	195602.434427	36.497037
1559.510474	195953.812316	36.502055
1560.839398	196306.683218	36.507072
1562.666019	196635.107190	36.512090
1563.953321	196995.923802	36.517108
1565.530740	197343.057040	36.522125
1567.151926	197688.826051	36.527143
1568.472389	198041.402655	36.532160
1570.191239	198394.903192	36.537178
1571.378023	198764.608266	36.542196
1572.848445	199115.057023	36.547213
1574.039483	199479.724624	36.552231
1575.596992	199851.631916	36.557248
1577.566305	200228.244609	36.562266
1578.363588	200604.336101	36.567284
1579.999860	200982.964997	36.572301
1581.689048	201358.958552	36.577319
1583.068080	201739.679558	36.582336
1585.315211	202123.732947	36.587354
1586.729804	202504.147050	36.592372
1588.472520	202884.659296	36.597389
1589.710140	203254.860903	36.602407
1591.658508	203641.766514	36.607424
1593.865571	204022.763661	36.612442
1594.594126	204401.349223	36.617460
1596.568063	204766.797567	36.622477
1598.411135	205144.751616	36.627495
1600.601467	205510.839352	36.632512
1602.138098	205883.084673	36.637530
1603.584358	206250.103057	36.642548
1605.691160	206618.597298	36.647565
1607.285521	206986.507908	36.652583
1608.551956	207330.693271	36.657600
1610.268579	207673.177713	36.662618
1611.447141	208026.028243	36.667636
1612.780020	208377.863414	36.672653
1614.383755	208740.243860	36.677671
1616.216173	209096.771003	36.682688
1617.828002	209453.159599	36.687706
1619.011647	209820.797331	36.692724
1620.841980	210162.218393	36.697741
1622.396551	210528.475023	36.702759
1623.824860	210881.624692	36.707776
1625.633403	211247.561475	36.712794
1626.799933	211628.365188	36.717812
1627.899083	212009.055046	36.722829
1629.254984	212395.797865	36.727847
1630.819317	212785.046368	36.732864
1632.344152	213175.065179	36.737882
1633.628908	213583.946179	36.742900
1635.540860	213984.899194	36.747917
1637.101595	214400.644616	36.752935
1638.452353	214823.640717	36.757952
1639.825092	215226.748371	36.762970
1641.078949	215650.323376	36.767988
1642.996963	216074.319911	36.773005
1644.882330	216505.460711	36.778023
1646.637137	216923.977335	36.783040
1648.562507	217349.247855	36.788058
1650.232808	217778.830708	36.793076
1651.865002	218202.757954	36.798093
1653.594803	218628.270314	36.803111
1654.985684	219047.416456	36.808128
1657.287445	219461.709579	36.813146
1659.315985	219895.100259	36.818164
1661.119070	220323.578386	36.823181
1662.785976	220742.556754	36.828199
1664.375003	221167.391828	36.833216
1666.018581	221598.695981	36.838234
1667.032431	222024.394595	36.843252
1668.625025	222451.570504	36.848269
1670.335110	222900.977936	36.853287
1671.802023	223349.082460	36.858304
1673.271928	223793.403537	36.863322
1674.480037	224241.301586	36.868340
1675.998425	224700.501954	36.873357
1677.921251	225151.430547	36.878375
1679.350055	225617.939354	36.883392
1681.276583	226079.792614	36.888410
1682.765549	226543.093956	36.893428
1684.806634	227001.908145	36.898445
1686.199401	227462.841427	36.903463
1687.943962	227942.918923	36.908480
1689.627576	228404.719955	36.913498
1691.545960	228867.752341	36.918516
1693.057241	229333.497529	36.923533
1694.752200	229794.107157	36.928551
1696.830042	230239.386661	36.933568
1699.093503	230656.516681	36.938586
1701.122373	231094.567705	36.943604
1703.119766	231528.611924	36.948621
1704.735355	231949.437746	36.953639
1705.933795	232387.329522	36.958656
1707.359586	232814.387937	36.963674
1709.132909	233256.222436	36.968692
1710.612703	233700.394416	36.973709
1713.030796	234132.595230	36.978727
1714.849583	234566.601520	36.983744
1716.614053	234988.171273	36.988762
1718.241555	235423.558581	36.993780
1720.207761	235850.734937	36.998797
1722.468825	236273.264039	37.003815
1724.558838	236702.249994	37.008832
1726.947138	237119.958134	37.013850
1728.742016	237539.114942	37.018868
1730.240771	237943.818630	37.023885
1732.255052	238357.579654	37.028903
1733.976955	238768.648030	37.033920
1735.463956	239173.000336	37.038938
1737.306796	239594.413617	37.043956
1738.438629	240013.866286	37.048973
1740.537127	240434.144997	37.053991
1742.325657	240859.227695	37.059008
1743.820816	241282.684720	37.064026
1745.388965	241711.921708	37.069044
1747.046298	242140.813884	37.074061
1749.062821	242561.389430	37.079079
1750.300077	243002.370192	37.084096
1752.682735	243437.262246	37.089114
1753.970639	243871.478504	37.094132
1755.780588	244294.327239	37.099149
1757.659486	244728.773785	37.104167
1759.206983	245175.572530	37.109184
1760.841115	245617.987733	37.114202
1762.271680	246070.828060	37.119220
1763.847852	246523.034345	37.124237
1765.574921	246980.245103	37.129255
1767.163053	247438.775678	37.134272
1769.306834	247898.405618	37.139290
1770.584137	248364.357167	37.144308
1772.129065	248830.619021	37.149325
1774.240513	249296.555755	37.154343
1775.209676	249767.946724	37.159360
1777.326416	250242.088518	37.164378
1779.162744	250725.652380	37.169396
1780.825932	251202.260348	37.174413
1782.550410	251684.802471	37.179431
1784.114340	252174.332806	37.184448
1785.755723	252661.055813	37.189466
1787.679643	253153.167002	37.194484
1789.096712	253647.168732	37.199501
1791.178389	254128.965040	37.204519
1792.599964	254604.244182	37.209536
1794.567923	255078.236025	37.214554
1796.363664	255548.294520	37.219572
1798.170732	256022.872912	37.224589
1800.022693	256489.314638	37.229607
1801.609460	256971.856568	37.234624
1803.933344	257439.513131	37.239642
1805.739498	257910.941683	37.244660
1807.722048	258401.392396	37.249677
1809.957070	258862.001879	37.254695
1811.580993	259337.856084	37.259712
1813.317192	259805.333293	37.264730
1815.542104	260287.130336	37.269748
1817.103296	260765.966930	37.274765
1818.799197	261228.776273	37.279783
1820.850486	261709.382991	37.284800
1823.140373	262180.879701	37.289818
1825.026329	262664.740310	37.294836
1826.545597	263131.897270	37.299853
1828.532118	263610.964207	37.304871
1830.240801	264085.073884	37.309888
1832.049202	264573.493401	37.314906
1833.550835	265059.170604	37.319924
1835.385332	265552.792323	37.324941
1837.434384	266035.301135	37.329959
1839.063060	266528.448934	37.334976
1841.480846	267028.853408	37.339994
1842.763669	267509.738780	37.345012
1844.859472	268013.677249	37.350029
1846.643400	268508.447155	37.355047
1848.431425	269007.305496	37.360064
1850.561856	269505.444050	37.365082
1852.251968	270002.539428	37.370100
1853.862668	270507.522397	37.375117
1855.843508	271008.961043	37.380135
1857.240388	271526.349871	37.385152
1859.024427	272038.006756	37.390170
1860.930352	272555.382759	37.395188
1862.016306	273085.345143	37.400205
1863.995559	273604.560840	37.405223
1866.151786	274149.630060	37.410240
1867.806899	274675.249432	37.415258
1869.703441	275217.617113	37.420276
1871.000814	275755.589779	37.425293
1872.935069	276298.176937	37.430311
1874.933475	276852.614423	37.435328
1876.693926	277390.351257	37.440346
1879.347713	277940.787145	37.445364
1880.792893	278492.698270	37.450381
1882.988559	279033.607498	37.455399
1884.593244	279582.135079	37.460416
1886.636059	280126.115374	37.465434
1888.395812	280671.285454	37.470452
1889.910086	281222.592101	37.475469
1892.117516	281767.072437	37.480487
1894.308944	282292.858428	37.485504
1896.440812	282815.757152	37.490522
1898.204194	283341.079450	37.495540
1900.109378	283858.882425	37.500557
1902.319056	284378.866812	37.505575
1903.564000	284905.948777	37.510592
1905.735353	285428.399861	37.515610
1907.790688	285959.225653	37.520628
1909.303397	286491.666264	37.525645
1911.579716	287024.863217	37.530663
1913.588407	287548.578741	37.535680
1915.648161	288074.340874	37.540698
1917.411780	288610.921155	37.545716
1919.155734	289157.611728	37.550733
1920.929452	289693.753909	37.555751
1923.015397	290231.084955	37.560768
1924.979737	290765.996070	37.565786
1926.629238	291307.460917	37.570804
1928.087801	291859.064889	37.575821
1930.123705	292412.243851	37.580839
1932.331095	292982.255827	37.585856
1934.307628	293529.292914	37.590874
1936.621192	294073.450388	37.595892
1938.500021	294635.560221	37.600909
1941.186101	295174.644910	37.605927
1942.885606	295736.043070	37.610944
1944.877941	296292.918031	37.615962
1946.894146	296845.925377	37.620980
1948.521405	297405.498144	37.625997
1950.619961	297947.157846	37.631015
1952.781547	298519.077963	37.636032
1954.725632	299082.904689	37.641050
1956.829326	299641.418145	37.646068
1958.376531	300201.445747	37.651085
1960.675961	300755.500010	37.656103
1962.911814	301321.371453	37.661120
1964.774199	301877.906430	37.666138
1966.972491	302430.367854	37.671156
1968.898484	302987.393017	37.676173
1971.555845	303536.823045	37.681191
1972.840541	304100.528484	37.686208
1974.430308	304673.574607	37.691226
1976.812487	305237.846752	37.696244
1978.244235	305811.699470	37.701261
1979.986221	306376.733710	37.706279
1981.749093	306955.600971	37.711296
1983.364400	307536.774913	37.716314
1985.499493	308126.744008	37.721332
1987.529956	308713.730027	37.726349
1989.719616	309300.608249	37.731367
1991.704175	309884.545965	37.736384
1993.610554	310465.038995	37.741402
1995.564611	311058.648152	37.746420
1997.468349	311647.512578	37.751437
1999.574589	312225.494628	37.756455
2001.880316	312799.273498	37.761472
2003.933851	313360.978401	37.766490
2006.086465	313920.198858	37.771508
2007.834625	314489.539664	37.776525
2009.976228	315041.922498	37.781543
2012.068611	315601.723981	37.786560
2013.681179	316169.830079	37.791578
2016.044197	316738.361764	37.796596
2017.352876	317318.596878	37.801613
2019.057826	317893.300039	37.806631
2021.082454	318474.773857	37.811648
2022.768062	319070.849651	37.816666
2024.553988	319676.805311	37.821684
2025.992434	320284.363560	37.826701
2028.062097	320889.243687	37.831719
2029.971418	321522.125438	37.836736
2031.900750	322150.452617	37.841754
2033.741332	322780.235853	37.846772
2035.845070	323421.189775	37.851789
2037.595731	324061.765747	37.856807
2039.120382	324713.417745	37.861824
2041.200760	325371.619438	37.866842
2043.379497	326022.561364	37.871860
2045.045863	326706.080340	37.876877
2047.051971	327371.634888	37.881895
2049.371980	328034.208536	37.886912
2051.209795	328711.683037	37.891930
2053.556060	329384.416710	37.896948
2055.891941	330068.415699	37.901965
2057.706914	330752.165335	37.906983
2060.035636	331439.194954	37.912000
2062.067905	332129.211345	37.917018
2064.611607	332800.321039	37.922036
2066.382908	333495.416212	37.927053
2068.796436	334173.435589	37.932071
2071.201031	334852.107754	37.937088
2073.092588	335543.779230	37.942106
2075.517858	336211.794256	37.947124
2077.488911	336903.180057	37.952141
2079.542839	337589.922608	37.957159
2081.874274	338270.186575	37.962176
2083.731296	338954.710474	37.967194
2086.403602	339642.765880	37.972212
2088.123417	340330.568428	37.977229
2089.755522	341019.086950	37.982247
2092.420303	341696.556127	37.987264
2095.387697	342388.151633	37.992282
2098.114806	343048.865301	37.997300
2099.966626	343713.627864	38.002317
2102.138747	344383.503612	38.007335
2104.042565	345054.862191	38.012352
2106.161970	345723.306362	38.017370
2108.289469	346388.440228	38.022388
2110.392034	347064.861764	38.027405
2112.598957	347713.670022	38.032423
2114.728760	348363.979318	38.037440
2116.497681	349014.543829	38.042458
2118.192530	349653.717443	38.047476
2120.285813	350315.474363	38.052493
2122.042966	350967.153844	38.057511
2124.173341	351627.514135	38.062528
2125.813200	352284.446421	38.067546
2128.399866	352948.286159	38.072564
2129.925539	353626.963087	38.077581
2131.419297	354301.904604	38.082599
2133.366049	354979.777169	38.087616
2135.069416	355693.481235	38.092634
2137.023351	356399.569140	38.097652
2138.735311	357118.625878	38.102669
2140.453914	357844.975709	38.107687
2142.065190	358575.821459	38.112704
2143.991105	359325.019028	38.117722
2146.420099	360078.556192	38.122740
2148.745544	360832.020548	38.127757
2150.486544	361590.542651	38.132775
2152.518627	362356.027253	38.137792
2154.388816	363131.138815	38.142810
2156.427012	363914.983105	38.147828
2158.544078	364710.517270	38.152845
2160.459865	365499.575273	38.157863
2162.931513	366290.474781	38.162880
2164.952572	367109.564640	38.167898
2167.736732	367902.456240	38.172916
2170.138811	368698.262156	38.177933
2172.515596	369500.725622	38.182951
2175.114669	370279.926017	38.187968
2177.574395	371094.488675	38.192986
2180.081648	371889.090077	38.198004
2182.337500	372681.560884	38.203021
2184.503985	373476.717328	38.208039
2186.797560	374269.475408	38.213056
2189.300370	375074.478993	38.218074
2191.876632	375850.364342	38.223092
2194.402843	376629.613305	38.228109
2196.682590	377418.649306	38.233127
2198.872824	378197.463154	38.238144
2201.183873	378983.566331	38.243162
2203.685284	379753.212989	38.248180
2206.027702	380525.277693	38.253197
2208.237773	381304.725171	38.258215
2211.101138	382069.514325	38.263232
2213.535666	382824.496170	38.268250
2216.593669	383575.221188	38.273268
2218.768020	384331.479794	38.278285
2220.420559	385079.291417	38.283303
2223.144616	385809.029496	38.288320
2225.612149	386557.909005	38.293338
2227.828382	387287.547451	38.298356
2230.268723	388022.200404	38.303373
2232.548988	388744.188810	38.308391
2235.068512	389445.333706	38.313408
2237.477257	390143.667885	38.318426
2239.960590	390823.165650	38.323444
2242.056290	391511.281632	38.328461
2243.979891	392188.715283	38.333479
2246.526609	392874.086990	38.338496
2248.715735	393553.801482	38.343514
2250.804178	394242.109373	38.348532
2252.532154	394940.422959	38.353549
2254.527425	395651.573930	38.358567
2256.602392	396351.695331	38.363584
2258.301701	397067.322683	38.368602
2260.463631	397784.981930	38.373620
2262.523501	398512.498256	38.378637
2263.987059	399241.669138	38.383655
2266.312243	399979.922932	38.388672
2268.346461	400736.729817	38.393690
2270.140289	401481.293911	38.398708
2272.505254	402244.338198	38.403725
2274.655624	403014.061837	38.408743
2276.768417	403782.123729	38.413760
2278.361599	404573.916150	38.418778
2280.794895	405378.994715	38.423796
2282.926902	406174.651596	38.428813
2285.247154	406981.982148	38.433831
2287.430301	407784.524237	38.438848
2289.565864	408606.074388	38.443866
2292.067958	409411.426351	38.448884
2294.510665	410224.515009	38.453901
2296.910378	411058.254535	38.458919
2298.888134	411876.893464	38.463936
2301.383778	412706.714297	38.468954
2303.988426	413539.655859	38.473972
2306.059719	414375.067739	38.478989
2308.014779	415213.410079	38.484007
2311.272820	416054.996963	38.489024
2313.501022	416886.704032	38.494042
2316.090792	417725.538897	38.499060
2318.855374	418558.238752	38.504077
2321.301786	419381.064886	38.509095
2323.810788	420207.018167	38.514112
2326.205180	421032.305241	38.519130
2328.400180	421861.067409	38.524148
2331.172942	422679.170788	38.529165
2333.476395	423520.567618	38.534183
2335.832559	424331.598093	38.539200
2338.285765	425150.938692	38.544218
2340.724621	425980.581961	38.549236
2343.142362	426802.251778	38.554253
2345.510141	427623.344934	38.559271
2348.167309	428446.283856	38.564288
2350.647209	429267.351404	38.569306
2352.678150	430082.240826	38.574324
2355.467773	430896.314124	38.579341
2357.383561	431707.319511	38.584359
2359.936560	432491.007889	38.589376
2362.365801	433271.805871	38.594394
2364.723155	434051.678578	38.599412
2367.446247	434823.465946	38.604429
2369.816301	435605.307660	38.609447
2372.166948	436370.577745	38.614464
2374.550919	437149.782746	38.619482
2376.390876	437930.217522	38.624500
2379.387502	438701.015713	38.629517
2381.292447	439500.308837	38.634535
2383.816590	440272.802940	38.639552
2386.177767	441058.654836	38.644570
2388.285614	441853.223878	38.649588
2391.050117	442637.735955	38.654605
2393.127590	443429.318494	38.659623
2395.852874	444222.329599	38.664640
2398.017606	445027.750221	38.669658
2399.767073	445842.367250	38.674676
2402.182653	446646.925408	38.679693
2404.384217	447471.620464	38.684711
2406.285892	448306.450239	38.689728
2408.610121	449141.933411	38.694746
2410.915721	449986.085217	38.699764
2413.243223	450835.711521	38.704781
2415.072234	451705.767869	38.709799
2417.249252	452568.648804	38.714816
2419.341893	453451.430777	38.719834
2421.370078	454332.517262	38.724852
2424.016565	455217.757780	38.729869
2425.911284	456128.468701	38.734887
2428.649817	457041.269505	38.739904
2430.657469	457947.379685	38.744922
2432.745029	458876.486879	38.749940
2435.768500	459795.685446	38.754957
2437.960803	460712.355145	38.759975
2440.815125	461642.465754	38.764992
2443.117611	462577.226116	38.770010
2445.581758	463522.729813	38.775028
2448.172445	464457.755404	38.780045
2450.562265	465404.595496	38.785063
2453.097781	466356.215446	38.790080
2455.396996	467295.145746	38.795098
2457.585776	468253.047222	38.800116
2459.895299	469217.852390	38.805133
2462.824414	470189.323137	38.810151
2465.442493	471132.859731	38.815168
2467.972817	472097.833775	38.820186
2470.895717	473064.560034	38.825204
2473.644699	474015.708215	38.830221
2476.345795	474967.472444	38.835239
2478.883391	475916.892270	38.840256
2481.830918	476866.142516	38.845274
2484.810601	477801.652142	38.850292
2488.009420	478716.573730	38.855309
2490.772337	479627.685964	38.860327
2493.652246	480511.213088	38.865344
2496.099463	481385.379378	38.870362
2498.413228	482253.164235	38.875380
2501.433662	483113.213162	38.880397
2503.740327	483992.223556	38.885415
2505.630912	484851.725061	38.890432
2508.328298	485721.849375	38.895450
2510.037318	486609.110166	38.900468
2512.100653	487487.735339	38.905485
2514.054356	488394.599031	38.910503
2516.576474	489292.183389	38.915520
2518.859300	490196.221752	38.920538
2520.873530	491122.866255	38.925556
2523.337877	492041.007322	38.930573
2525.663848	492978.044489	38.935591
2528.006965	493918.054467	38.940608
2531.007065	494863.500271	38.945626
2533.184192	495818.064245	38.950644
2535.513880	496766.141237	38.955661
2537.833269	497730.863222	38.960679
2540.155749	498689.022007	38.965696
2542.707986	499667.866687	38.970714
2544.514233	500669.073146	38.975732
2546.990416	501660.068343	38.980749
2549.749811	502670.471183	38.985767
2551.828142	503679.969814	38.990784
2554.792922	504694.548657	38.995802
2557.204568	505712.385289	39.000820
2560.521774	506721.180111	39.005837
2562.962244	507739.337347	39.010855
2565.736352	508756.868644	39.015872
2568.349105	509774.513712	39.020890
2570.964443	510808.776481	39.025908
2573.279819	511831.733200	39.030925
2576.011696	512861.002964	39.035943
2578.603562	513896.175403	39.040960
2581.472367	514934.708699	39.045978
2584.056653	515967.577867	39.050996
2586.623287	517005.520148	39.056013
2589.549620	518033.305437	39.061031
2592.680484	519064.462865	39.066048
2595.458516	520090.674413	39.071066
2597.529458	521123.133021	39.076084
2600.756687	522157.942730	39.081101
2603.032421	523200.096276	39.086119
2605.555918	524237.099308	39.091136
2608.305614	525264.625688	39.096154
2610.879784	526304.900691	39.101172
2613.628154	527347.439429	39.106189
2616.437036	528382.493602	39.111207
2618.596738	529420.505778	39.116224
2621.241176	530449.955248	39.121242
2623.866362	531521.163353	39.126260
2626.464910	532564.615317	39.131277
2628.700902	533596.277592	39.136295
2631.236778	534619.712840	39.141312
2634.374083	535631.449231	39.146330
2636.878290	536642.467613	39.151348
2639.422302	537650.741014	39.156365
2641.678880	538665.381330	39.161383
2644.237280	539693.580555	39.166400
2647.121819	540697.705405	39.171418
2650.273857	541731.388887	39.176436
2652.642800	542753.109479	39.181453
2654.792779	543773.233676	39.186471
2657.017798	544826.057490	39.191488
2659.393502	545865.349888	39.196506
2661.861724	546930.039940	39.201524
2664.184660	547994.370708	39.206541
2666.771657	549065.712218	39.211559
2669.764405	550141.374086	39.216576
2672.679199	551212.943021	39.221594
2674.934528	552304.492907	39.226612
2678.090477	553376.502399	39.231629
2680.905158	554470.746099	39.236647
2683.633880	555566.673663	39.241664
2686.299395	556659.205865	39.246682
2688.976731	557751.947592	39.251700
2691.708083	558843.836295	39.256717
2694.821985	559944.761401	39.261735
2697.480540	561052.753916	39.266752
2700.035297	562141.836912	39.271770
2702.749145	563262.238221	39.276788
2705.780291	564365.164847	39.281805
2708.525129	565474.222058	39.286823
2710.851948	566590.735752	39.291840
2714.148392	567694.436439	39.296858
2717.263593	568807.710488	39.301876
2720.516411	569901.389174	39.306893
2723.608929	571002.629488	39.311911
2726.403019	572106.384187	39.316928
2729.766185	573173.765857	39.321946
2733.120911	574260.074387	39.326964
2736.117938	575332.903968	39.331981
2738.992254	576403.103649	39.336999
2741.414789	577481.263969	39.342016
2744.240957	578542.859896	39.347034
2746.836510	579608.315732	39.352052
2749.648082	580701.474750	39.357069
2752.164557	581767.308117	39.362087
2754.862296	582846.555129	39.367104
2757.753904	583919.807348	39.372122
2760.056336	585011.162359	39.377140
2762.912086	586095.857864	39.382157
2765.656247	587179.071189	39.387175
2767.858450	588268.443621	39.392192
2770.553893	589362.092456	39.397210
2773.411173	590460.273184	39.402228
2776.176381	591561.524456	39.407245
2778.674955	592658.560467	39.412263
2780.813606	593734.065429	39.417280
2783.725223	594811.393461	39.422298
2785.690033	595888.733928	39.427316
2788.226979	596979.949644	39.432333
2790.913733	598071.187495	39.437351
2793.225994	599184.067087	39.442368
2796.092255	600298.046408	39.447386
2798.484160	601417.855960	39.452404
2800.895361	602551.418294	39.457421
2803.611860	603695.226537	39.462439
2805.518751	604848.166455	39.467456
2808.242243	606004.302451	39.472474
2811.327325	607186.877278	39.477492
2813.778740	608370.786921	39.482509
2816.891036	609546.154547	39.487527
2819.711687	610739.505470	39.492544
2822.165674	611937.342434	39.497562
2824.807347	613143.869581	39.502580
2827.620799	614347.435511	39.507597
2830.529964	615572.252644	39.512615
2833.394100	616806.539259	39.517632
2836.482506	618026.651987	39.522650
2839.908962	619257.616084	39.527668
2842.464573	620490.738255	39.532685
2845.460255	621722.895102	39.537703
2848.496822	622970.292892	39.542720
2851.274465	624205.849847	39.547738
2854.579562	625445.020291	39.552756
2857.296892	626693.137384	39.557773
2860.742652	627936.688459	39.562791
2863.181804	629194.396783	39.567808
2866.405039	630432.848256	39.572826
2869.370798	631684.227503	39.577844
2872.031429	632943.945161	39.582861
2875.040688	634189.476110	39.587879
2877.780436	635469.387874	39.592896
2880.520761	636729.980320	39.597914
2884.112440	637988.926190	39.602932
2887.262242	639246.745698	39.607949
2890.208981	640499.407509	39.612967
2892.951743	641758.035021	39.617984
2896.375222	643000.382903	39.623002
2899.298097	644263.506144	39.628020
2901.872796	645533.410888	39.633037
2904.675524	646778.042306	39.638055
2907.639330	648043.874321	39.643072
2910.848497	649307.660090	39.648090
2913.769626	650566.800072	39.653108
2916.818530	651829.295919	39.658125
2919.719757	653082.040977	39.663143
2922.335152	654352.458162	39.668160
2925.237495	655613.149255	39.673178
2928.308504	656878.379930	39.678196
2930.825133	658152.304464	39.683213
2934.113366	659406.215213	39.688231
2937.013947	660649.177982	39.693248
2939.507714	661876.670423	39.698266
2941.868008	663118.710050	39.703284
2944.341282	664360.818267	39.708301
2947.559045	665610.100826	39.713319
2949.470957	666868.844626	39.718336
2952.050477	668133.773667	39.723354
2954.990779	669412.248028	39.728372
2957.623342	670705.370288	39.733389
2961.108975	671989.020426	39.738407
2964.146772	673275.354920	39.743424
2967.352625	674570.480098	39.748442
2970.574173	675873.523083	39.753460
2972.897522	677173.157168	39.758477
2976.345091	678483.545740	39.763495
2978.968713	679809.487211	39.768512
2981.789303	681132.968159	39.773530
2984.622866	682456.751855	39.778548
2987.161756	683799.709638	39.783565
2990.194539	685145.412913	39.788583
2993.186964	686506.807992	39.793600
2996.258902	687853.639717	39.798618
2998.959688	689222.217963	39.803636
3002.005707	690594.547055	39.808653
3005.498771	691951.506906	39.813671
3008.684051	693338.371639	39.818688
3011.958543	694707.397555	39.823706
3015.154385	696080.141925	39.828724
3017.955359	697473.067193	39.833741
3021.195182	698839.323772	39.838759
3024.817162	700218.287150	39.843776
3028.132696	701592.525124	39.848794
3031.074105	702976.964848	39.853812
3033.550053	704368.643822	39.858829
3036.819081	705740.446644	39.863847
3039.651422	707138.402330	39.868864
3042.550519	708536.266666	39.873882
3045.585135	709937.641218	39.878900
3048.723325	711336.885847	39.883917
3051.524670	712738.282791	39.888935
3054.308055	714154.295057	39.893952
3057.496246	715576.480896	39.898970
3060.606171	716998.834344	39.903988
3063.061646	718435.548456	39.909005
3066.259163	719859.920861	39.914023
3069.128866	721306.254118	39.919040
3072.087336	722752.714411	39.924058
3075.518458	724195.132994	39.929076
3078.188679	725661.344688	39.934093
3080.935249	727116.855637	39.939111
3083.859341	728595.342237	39.944128
3087.213381	730056.694074	39.949146
3090.218335	731528.211070	39.954164
3092.996182	733013.321782	39.959181
3096.001914	734466.626557	39.964199
3098.984225	735917.746644	39.969216
3102.019349	737358.675653	39.974234
3105.105929	738805.156050	39.979252
3107.751497	740254.407084	39.984269
3110.686138	741700.679588	39.989287
3114.308978	743155.641144	39.994304
3117.467417	744608.735790	39.999322
3121.003586	746064.995136	40.004340
3123.585529	747532.035770	40.009357
3127.417471	748977.990669	40.014375
3130.764581	750444.841593	40.019392
3133.813251	751912.744796	40.024410
3137.256202	753362.375994	40.029428
3140.320693	754826.764004	40.034445
3143.478968	756292.873039	40.039463
3146.516012	757772.696721	40.044480
3149.319591	759241.741587	40.049498
3152.662791	760725.216048	40.054516
3155.723348	762218.332440	40.059533
3159.191394	763699.968479	40.064551
3162.204799	765195.695465	40.069568
3165.013101	766697.596470	40.074586
3168.084278	768205.095312	40.079604
3171.104135	769723.989886	40.084621
3174.552154	771238.273708	40.089639
3177.857000	772747.358401	40.094656
3180.882963	774270.420040	40.099674
3184.306444	775802.423845	40.104692
3187.056453	777345.558274	40.109709
3190.697505	778868.582654	40.114727
3193.891478	780409.760831	40.119744
3196.771604	781951.349345	40.124762
3200.368657	783493.563083	40.129780
3203.377380	785043.634703	40.134797
3206.467235	786599.335723	40.139815
3209.918054	788159.486187	40.144832
3212.725037	789721.558493	40.149850
3216.158462	791281.610176	40.154868
3219.120516	792846.293679	40.159885
3222.323768	794420.232720	40.164903
3226.065677	795993.528970	40.169920
3229.319452	797579.229071	40.174938
3232.720419	799148.099834	40.179956
3236.106403	800729.385298	40.184973
3239.004938	802296.206699	40.189991
3242.295711	803870.084835	40.195008
3245.510618	805453.733348	40.200026
3249.599570	807018.780196	40.205044
3253.015057	808606.303532	40.210061
3256.103599	810183.592930	40.215079
3260.019872	811746.989296	40.220096
3263.265592	813325.762324	40.225114
3266.649747	814890.909542	40.230132
3269.718878	816456.085241	40.235149
3272.948008	818016.376163	40.240167
3275.934547	819549.753495	40.245184
3278.565129	821067.179458	40.250202
3281.994798	822592.409197	40.255220
3284.967214	824119.166547	40.260237
3288.360516	825626.389861	40.265255
3292.338493	827148.076178	40.270272
3295.289134	828668.753633	40.275290
3298.654016	830199.572864	40.280308
3301.411149	831728.282846	40.285325
3304.828457	833268.980118	40.290343
3308.142320	834817.161356	40.295360
3310.909887	836363.358293	40.300378
3314.025034	837922.888332	40.305396
3316.493457	839507.290668	40.310413
3319.228216	841091.446009	40.315431
3322.175017	842704.139798	40.320448
3325.304235	844330.579974	40.325466
3328.179946	845945.855946	40.330484
3331.620251	847595.784929	40.335501
3334.651785	849237.188902	40.340519
3338.011723	850892.375842	40.345536
3341.277433	852568.782305	40.350554
3344.289957	854249.822575	40.355572
3347.344558	855948.149587	40.360589
3350.389869	857646.977306	40.365607
3353.505957	859361.706457	40.370624
3356.693156	861091.837072	40.375642
3359.780744	862833.700904	40.380660
3363.065497	864579.775807	40.385677
3366.730858	866338.644283	40.390695
3370.116862	868098.690624	40.395712
3373.346420	869874.022260	40.400730
3377.371637	871642.592910	40.405748
3380.584850	873414.934576	40.410765
3384.071257	875190.566570	40.415783
3387.607143	876969.715354	40.420800
3390.975244	878748.353649	40.425818
3394.555572	880526.414984	40.430836
3398.076094	882313.989134	40.435853
3401.585330	884099.566768	40.440871
3404.751409	885892.470775	40.445888
3407.846803	887702.198808	40.450906
3411.157967	889498.490242	40.455924
3414.579997	891314.643537	40.460941
3417.689149	893135.285189	40.465959
3421.502105	894940.478576	40.470976
3424.601390	896778.649344	40.475994
3427.860633	898600.495571	40.481012
3431.202676	900436.757168	40.486029
3434.417572	902271.572572	40.491047
3437.728051	904119.720122	40.496064
3440.814722	905970.850786	40.501082
3444.548705	907818.175995	40.506100
3448.182024	909670.956064	40.511117
3451.191514	911520.444138	40.516122
3454.835737	913306.121537	40.521127
3457.974665	915053.274870	40.526132
3461.501265	916713.377544	40.531136
3464.967238	918314.581947	40.536141
3468.133728	919835.433854	40.541146
3471.617451	921267.624691	40.546151
3474.659067	922636.156626	40.551156
3477.789294	923919.649750	40.556160
3480.793873	925118.296950	40.561165
3483.576559	926246.293464	40.566170
3486.462263	927279.519035	40.571175
3488.453723	928247.777382	40.576180
3491.016252	929137.603055	40.581184
3493.760075	929964.654333	40.586189
3495.453656	930717.459846	40.591194
3497.596650	931422.284968	40.596199
3499.298220	932058.284397	40.601204
3501.370490	932615.940712	40.606208
3503.039214	933130.527218	40.611213
3504.789139	933603.316895	40.616218
3506.279685	934002.530430	40.621223
3508.064903	934359.361178	40.626228
3509.550882	934656.174316	40.631232
3510.807083	934904.285990	40.636237
3511.998145	935112.594629	40.641242
3513.153832	935273.331454	40.646247
3514.386087	935412.375950	40.651252
3515.529721	935502.329971	40.656256
3516.224008	935562.533860	40.661261
3517.275316	935588.055958	40.666266
3518.535274	935584.963873	40.671271
3518.942302	935553.534661	40.676276
3519.978754	935482.390055	40.681280
3520.743599	935394.123960	40.686285
3521.224458	935282.599602	40.691290
3522.281283	935139.995977	40.696295
3522.461775	934979.602524	40.701300
3523.337268	934790.502762	40.706304
3524.185458	934592.672211	40.711309
3524.347053	934366.270401	40.716314
3524.866708	934124.257431	40.721319
3525.004842	933877.405893	40.726324
3525.776267	933599.734796	40.731328
3526.066821	933318.101540	40.736333
3526.514220	933019.539625	40.741338
3527.078863	932705.108433	40.746343
3527.060528	932389.798389	40.751348
3527.486766	932048.962760	40.756352
3528.015568	931708.279540	40.761357
3527.693364	931347.756123	40.766362
3528.475401	930983.276177	40.771367
3528.364143	930614.891927	40.776372
3528.699061	930227.398131	40.781376
3529.103465	929847.928573	40.786381
3529.177881	929451.685940	40.791386
3529.475358	929039.052177	40.796391
3529.648775	928635.914220	40.801396
3530.077953	928213.014801	40.806400
3530.002367	927786.326159	40.811405
3530.144857	927353.418790	40.816410
3530.406652	926920.840062	40.821415
3530.526236	926479.412353	40.826420
3530.594044	926022.777127	40.831424
3530.761656	925576.366632	40.836429
3531.074134	925123.648171	40.841434
3531.248270	924652.944412	40.846439
3531.218928	924198.764475	40.851444
3531.368585	923723.562175	40.856448
3531.529780	923250.526616	40.861453
3531.567116	922773.913545	40.866458
3531.523389	922290.445920	40.871463
3531.321400	921805.423385	40.876468
3531.303089	921325.037528	40.881472
3531.506395	920837.646887	40.886477
3531.662113	920350.316450	40.891482
3531.836717	919863.515856	40.896487
3531.845908	919381.413081	40.901492
3532.004026	918875.383644	40.906496
3531.973645	918378.575342	40.911501
3531.691818	917875.028925	40.916506
3532.173774	917368.225980	40.921511
3532.264554	916865.003277	40.926516
3532.377381	916349.987977	40.931520
3532.362789	915835.811923	40.936525
3532.241338	915329.306751	40.941530
3532.138710	914815.241822	40.946535
3532.257083	914297.720741	40.951540
3532.120992	913780.001418	40.956544
3532.387875	913266.690416	40.961549
3532.290070	912755.801244	40.966554
3532.487405	912221.793467	40.971559
3532.627021	911709.417637	40.976564
3532.839211	911175.498042	40.981568
3532.897612	910647.333648	40.986573
3532.877142	910113.254147	40.991578
3533.387075	909567.660960	40.996583
3532.698013	909042.939287	41.001588
3532.839485	908495.664436	41.006592
3532.607424	907956.689046	41.011597
3532.276170	907426.547188	41.016602
3532.809375	906885.312184	41.021607
3532.654573	906360.919316	41.026612
3532.615770	905810.420304	41.031616
3532.668669	905279.139370	41.036621
3532.823882	904742.485332	41.041626
3533.182260	904186.163321	41.046631
3532.988387	903644.350490	41.051636
3532.945847	903105.739416	41.056640
3532.931599	902551.440291	41.061645
3532.755016	902005.702194	41.066650
3533.015859	901454.721210	41.071655
3532.700506	900911.312669	41.076660
3532.875944	900359.080206	41.081664
3532.424462	899812.692535	41.086669
3532.234068	899271.517091	41.091674
3532.706238	898716.658726	41.096679
3532.280348	898175.707642	41.101684
3532.502592	897621.653062	41.106688
3532.719155	897078.169145	41.111693
3532.318667	896533.772287	41.116698
3532.712461	895975.856314	41.121703
3532.656353	895437.187753	41.126708
3532.495489	894882.060329	41.131712
3532.736347	894326.326797	41.136717
3532.652163	893779.775065	41.141722
3532.876674	893220.650344	41.146727
3532.661749	892663.285504	41.151732
3532.602563	892107.676182	41.156736
3532.822692	891544.714205	41.161741
3532.831571	890994.688765	41.166746
3532.732218	890433.798863	41.171751
3532.565102	889877.023836	41.176756
3532.488126	889319.889107	41.181760
3532.951911	888758.738918	41.186765
3532.643328	888205.114193	41.191770
3532.827824	887636.550202	41.196775
3532.876169	887076.177216	41.201780
3532.377013	886503.844602	41.206784
3532.675245	885946.318648	41.211789
3532.524566	885386.589476	41.216794
3532.727426	884833.424238	41.221799
3532.580895	884263.809752	41.226804
3532.492121	883690.837817	41.231808
3532.812379	883128.099029	41.236813
3532.585197	882567.722983	41.241818
3532.458345	881994.493152	41.246823
3532.485046	881441.712187	41.251828
3532.561554	880865.527831	41.256832
3532.735004	880304.865383	41.261837
3532.286585	879730.014534	41.266842
3532.533556	879165.355069	41.271847
3532.491354	878599.430816	41.276852
3532.439037	878031.806212	41.281856
3532.472475	877469.151457	41.286861
3532.438444	876902.965059	41.291866
3532.447256	876333.421093	41.296871
3532.380957	875761.120435	41.301876
3532.543289	875186.204397	41.306880
3532.633654	874622.104071	41.311885
3532.474037	874049.750115	41.316890
3532.476994	873455.686690	41.321895
3532.232088	872893.709055	41.326900
3532.092261	872322.154391	41.331904
3532.259444	871747.096967	41.336909
3531.762933	871179.664380	41.341914
3532.093872	870608.931528	41.346919
3531.971300	870035.795468	41.351924
3532.262178	869462.242536	41.356928
3532.588211	868904.836345	41.361933
3532.430825	868334.357207	41.366938
3532.872618	867749.548832	41.371943
3532.616671	867170.918537	41.376948
3532.510155	866596.381729	41.381952
3532.931175	866013.252120	41.386957
3532.487180	865430.116433	41.391962
3532.502413	864850.536289	41.396967
3532.779141	864265.027994	41.401972
3532.690797	863673.114031	41.406976
3532.711964	863091.420905	41.411981
3532.331528	862513.820882	41.416986
3532.447913	861921.117316	41.421991
3532.354947	861349.964390	41.426996
3532.339849	860764.944155	41.432000
3532.162810	860173.188778	41.437005
3532.450090	859600.834369	41.442010
3532.327598	859013.525344	41.447015
3532.224361	858426.836942	41.452020
3531.676597	857862.142190	41.457024
3531.959332	857283.250854	41.462029
3531.797989	856709.631958	41.467034
3531.845951	856120.751229	41.472039
3532.027512	855556.010760	41.477044
3531.704734	854981.771278	41.482048
3532.223405	854396.049290	41.487053
3531.898756	853821.701702	41.492058
3532.115135	853234.655912	41.497063
3532.031185	852647.897413	41.502068
3532.218885	852069.601139	41.507072
3531.996959	851493.169958	41.512077
3531.886989	850916.373909	41.517082
3532.030784	850317.187644	41.522087
3532.019656	849734.034235	41.527092
3531.669394	849159.549720	41.532096
3532.018921	848566.877788	41.537101
3531.819572	847999.466271	41.542106
3531.690624	847409.200475	41.547111
3531.601284	846830.950256	41.552116
3531.734140	846253.582693	41.557120
3531.592981	845662.179688	41.562125
3531.475102	845093.126194	41.567130
3531.830789	844500.944137	41.572135
3531.468903	843933.288654	41.577140
3531.541503	843344.748965	41.582144
3531.722534	842768.709068	41.587149
3531.302191	842178.974889	41.592154
3531.456969	841593.279261	41.597159
3531.447775	841023.253979	41.602164
3531.231474	840441.609688	41.607168
3531.447759	839859.301760	41.612173
3531.625237	839286.357782	41.617178
3531.610723	838687.402913	41.622183
3531.460356	838112.263235	41.627188
3531.040048	837532.971794	41.632192
3531.296519	836957.219279	41.637197
3531.285080	836379.801868	41.642202
3531.359260	835787.242235	41.647207
3531.140333	835206.973289	41.652212
3531.407874	834635.400815	41.657216
3531.096571	834062.509726	41.662221
3530.895784	833487.498762	41.667226
3531.201340	832896.633174	41.672231
3531.204662	832319.774510	41.677236
3530.915578	831742.035322	41.682240
3530.910020	831169.468782	41.687245
3530.790480	830595.113107	41.692250
3530.849658	830011.544368	41.697255
3531.157972	829428.612980	41.702260
3530.860160	828846.758232	41.707264
3530.896478	828267.382980	41.712269
3530.548958	827693.736863	41.717274
3530.663968	827123.136604	41.722279
3530.496771	826563.380839	41.727284
3530.222838	825983.659616	41.732288
3530.562028	825411.893965	41.737293
3530.405053	824841.238102	41.742298
3530.668932	824260.490163	41.747303
3530.368034	823692.495641	41.752308
3530.405867	823125.567256	41.757312
3530.498481	822545.038731	41.762317
3530.498171	821964.865906	41.767322
3530.749825	821395.111544	41.772327
3530.746048	820826.085004	41.777332
3530.775684	820247.027144	41.782336
3530.495980	819664.938953	41.787341
3530.745501	819087.942856	41.792346
3530.629888	818498.827278	41.797351
3530.596593	817917.570594	41.802356
3530.089904	817343.535913	41.807360
3530.554518	816770.949433	41.812365
3529.953418	816197.565839	41.817370
3530.369328	815620.533547	41.822375
3530.214154	815050.449750	41.827380
3530.037380	814468.573666	41.832384
3530.468617	813899.417315	41.837389
3530.263343	813327.334943	41.842394
3530.417661	812745.644168	41.847399
3530.223328	812170.082959	41.852404
3530.428975	811592.788200	41.857408
3530.327258	811012.753911	41.862413
3530.005551	810442.943286	41.867418
3530.166621	809851.352638	41.872423
3530.368486	809278.807309	41.877428
3529.897970	808693.542116	41.882432
3530.187233	808117.552302	41.887437
3530.041480	807546.634525	41.892442
3530.008049	806971.827402	41.897447
3530.093055	806394.011074	41.902452
3529.712570	805828.820642	41.907456
3529.567163	805255.749951	41.912461
3529.571213	804691.918989	41.917466
3529.999597	804119.880382	41.922471
3529.922279	803551.017906	41.927476
3529.573660	802981.418994	41.932480
3529.544971	802403.039028	41.937485
3529.489633	801842.121563	41.942490
3529.925094	801263.615399	41.947495
3529.745831	800693.405344	41.952500
3529.724947	800122.189064	41.957504
3530.182371	799547.066592	41.962509
3529.673091	798968.529000	41.967514
3529.436191	798394.655569	41.972519
3529.842805	797820.575622	41.977524
3529.823962	797253.145331	41.982528
3529.590854	796680.405102	41.987533
3529.575634	796095.703301	41.992538
3529.783702	795524.902944	41.997543
3529.634157	794953.871413	42.002548
3529.203706	794372.777356	42.007552
3529.395695	793800.807681	42.012557
3529.338928	793239.782811	42.017562
3529.367354	792669.810742	42.022567
3529.286007	792105.114629	42.027572
3529.231560	791533.050905	42.032576
3529.420484	790962.126928	42.037581
3528.807080	790402.934808	42.042586
3529.279333	789829.561998	42.047591
3529.240954	789261.633721	42.052596
3529.078017	788691.273600	42.057600
3529.381056	788119.952614	42.062605
3529.093005	787550.946812	42.067610
3529.105610	786984.989134	42.072615
3529.316190	786414.971630	42.077620
3528.984691	785856.158140	42.082624
3528.981978	785281.662618	42.087629
3528.962514	784726.000486	42.092634
3528.932643	784147.485498	42.097639
3528.917217	783588.981042	42.102644
3528.622450	783019.368184	42.107648
3529.209025	782451.821548	42.112653
3528.581410	781891.617239	42.117658
3528.741788	781324.349214	42.122663
3528.822682	780761.968545	42.127668
3528.663390	780195.600567	42.132672
3528.784965	779630.173169	42.137677
3528.657037	779065.383603	42.142682
3528.477639	778503.953523	42.147687
3528.607474	777950.890291	42.152692
3528.512081	777382.962255	42.157696
3528.739542	776815.525156	42.162701
3528.649929	776264.043916	42.167706
3528.584300	775709.612749	42.172711
3528.923263	775143.108880	42.177716
3528.510197	774575.360199	42.182720
3528.408359	774008.695746	42.187725
3528.518446	773445.299151	42.192730
3528.405456	772877.859631	42.197735
3528.599274	772320.812497	42.202740
3528.796273	771748.800768	42.207744
3528.968933	771186.500229	42.212749
3528.727170	770617.134813	42.217754
3528.700119	770045.176528	42.222759
3528.651061	769473.177610	42.227764
3528.354220	768914.281325	42.232768
3528.644170	768344.797470	42.237773
3528.327024	767786.558438	42.242778
3528.600774	767216.744213	42.247783
3528.591564	766657.037066	42.252788
3528.565963	766089.109322	42.257792
3528.654746	765515.450531	42.262797
3528.396721	764958.960354	42.267802
3528.408126	764387.988310	42.272807
3527.973624	763822.323755	42.277812
3527.854970	763253.998697	42.282816
3527.604063	762697.536012	42.287821
3527.669166	762147.980141	42.292826
3527.653207	761594.255476	42.297831
3527.603858	761046.611093	42.302836
3527.447129	760496.380462	42.307840
3527.452997	759935.772967	42.312845
3527.774910	759393.469395	42.317850
3528.107984	758841.455892	42.322855
3528.126821	758283.782128	42.327860
3528.100815	757716.157719	42.332864
3527.812613	757144.538767	42.337869
3527.381294	756602.558594	42.342874
3527.352456	756047.738691	42.347879
3527.468322	755493.939415	42.352884
3527.377188	754949.068917	42.357888
3527.383185	754393.184787	42.362893
3527.344477	753852.669564	42.367898
3527.306017	753296.071494	42.372903
3527.075706	752741.489954	42.377908
3527.441151	752205.232899	42.382912
3527.428036	751651.473619	42.387917
3526.843802	751111.450800	42.392922
3526.858072	750559.731672	42.397927
3526.977233	750012.400166	42.402932
3526.790213	749479.949282	42.407936
3527.357365	748932.958715	42.412941
3527.088478	748392.000148	42.417946
3526.733646	747846.423988	42.422951
3526.853646	747305.026741	42.427956
3526.871505	746762.275120	42.432960
3526.995485	746221.394615	42.437965
3526.816326	745690.461043	42.442970
3526.737121	745150.776304	42.447975
3526.703774	744605.758098	42.452980
3526.837576	744062.106726	42.457984
3526.677875	743521.334652	42.462989
3526.720011	742975.844012	42.467994
3526.924073	742439.631437	42.472999
3526.717116	741894.207028	42.478004
3526.524433	741360.213369	42.483008
3526.798132	740818.637321	42.488013
3526.431131	740283.018096	42.493018
3526.648823	739747.757249	42.498023
3526.953065	739208.340416	42.503028
3526.549993	738669.452719	42.508032
3526.983960	738123.955125	42.513037
3527.060547	737592.381444	42.518042
3526.822439	737043.115331	42.523047
3526.925325	736493.950973	42.528052
3526.867894	735942.895967	42.533056
3526.898027	735404.801492	42.538061
3526.452033	734854.380914	42.543066
3526.393176	734319.890432	42.548071
3526.798862	733783.206337	42.553076
3526.375159	733245.489538	42.558080
3526.567137	732697.484548	42.563085
3526.404429	732159.006984	42.568090
3526.667799	731614.430605	42.573095
3526.707485	731083.470271	42.578100
3526.126080	730540.896413	42.583104
3526.275738	730007.271954	42.588109
3526.170350	729473.259699	42.593114
3525.975208	728931.898459	42.598119
3526.025310	728400.215488	42.603124
3525.631338	727872.783351	42.608128
3526.019986	727336.713648	42.613133
3525.704219	726817.768569	42.618138
3525.567449	726281.570539	42.623143
3525.990758	725763.670657	42.628148
3525.976199	725238.331664	42.633152
3526.367898	724698.620161	42.638157
3525.926204	724161.691084	42.643162
3525.946740	723632.923326	42.648167
3526.168409	723093.283917	42.653172
3525.812270	722572.689061	42.658176
3526.006313	722045.127723	42.663181
3526.150210	721510.750678	42.668186
3526.054961	720976.776433	42.673191
3526.223332	720437.715895	42.678196
3525.786397	719914.538178	42.683200
3525.924861	719366.142409	42.688205
3525.907044	718847.387074	42.693210
3525.735308	718320.989556	42.698215
3526.167829	717780.620494	42.703220
3526.289248	717252.816121	42.708224
3526.045715	716721.321082	42.713229
3525.936892	716182.726363	42.718234
3525.985908	715643.871618	42.723239
3526.197573	715107.285834	42.728244
3525.675653	714589.195214	42.733248
3525.660556	714059.129267	42.738253
3525.557342	713519.568795	42.743258
3525.670800	712989.760838	42.748263
3525.443225	712454.718128	42.753268
3525.400241	711942.039476	42.758272
3525.291996	711399.962413	42.763277
3525.346416	710884.672131	42.768282
3525.408552	710360.961411	42.773287
3525.593492	709827.568213	42.778292
3525.517544	709319.352595	42.783296
3525.474565	708780.819932	42.788301
3525.338418	708260.736795	42.793306
3524.964711	707728.201043	42.798311
3525.192620	707202.679032	42.803316
3524.842916	706689.735991	42.808321
3524.857768	706170.592261	42.813325
3525.017273	705654.471287	42.818330
3524.774455	705141.566362	42.823335
3525.273866	704623.537599	42.828340
3524.869778	704111.194758	42.833345
3524.949329	703572.562143	42.838349
3525.267007	703068.428595	42.843354
3525.139352	702547.600465	42.848359
3525.007130	702032.057546	42.853364
3525.029030	701504.533681	42.858369
3525.116033	700994.207728	42.863373
3524.719012	700474.443819	42.868378
3524.644973	699958.121843	42.873383
3524.642383	699441.856451	42.878388
3524.641833	698936.245198	42.883393
3524.504756	698422.178849	42.888397
3524.398149	697911.357518	42.893402
3524.340602	697399.503874	42.898407
3524.333062	696890.743504	42.903412
3524.197210	696385.952540	42.908417
3524.541778	695869.218345	42.913421
3524.522313	695367.729709	42.918426
3524.254420	694855.216896	42.923431
3524.477367	694341.148523	42.928436
3523.972585	693843.982105	42.933441
3524.317511	693340.774600	42.938445
3523.958782	692837.957034	42.943450
3524.203456	692327.945553	42.948455
3524.225430	691821.921847	42.953460
3523.922631	691330.896764	42.958465
3524.423590	690826.873553	42.963469
3524.228470	690329.109235	42.968474
3524.350910	689825.641293	42.973479
3524.699969	689306.683192	42.978484
3524.344963	688807.070327	42.983489
3523.976882	688293.897765	42.988493
3523.661471	687793.525052	42.993498
3523.909004	687295.217942	42.998503
3523.846265	686796.488310	43.003508
3523.681919	686298.246097	43.008513
3523.858528	685799.420436	43.013517
3523.532722	685304.336286	43.018522
3523.458575	684809.480722	43.023527
3523.697924	684306.231394	43.028532
3523.295584	683824.370529	43.033537
3523.175121	683317.891952	43.038541
3523.184798	682829.535476	43.043546
3523.199216	682351.010481	43.048551
3523.302264	681873.988808	43.053556
3522.852332	681389.318285	43.058561
3523.099554	680898.029247	43.063565
3523.255066	680415.793252	43.068570
3523.162197	679928.046077	43.073575
3523.238730	679436.558379	43.078580
3523.082260	678962.068965	43.083585
3523.516373	678463.445127	43.088589
3523.282121	677982.144084	43.093594
3523.187005	677500.096716	43.098599
3523.161827	677014.823791	43.103604
3522.857763	676527.729581	43.108609
3523.239140	676030.477961	43.113613
3523.234603	675565.304433	43.118618
3523.375906	675076.463412	43.123623
3523.268801	674582.157510	43.128628
3523.420979	674102.033879	43.133633
3523.173371	673606.952636	43.138637
3523.025726	673126.630580	43.143642
3523.307996	672630.011508	43.148647
3523.362707	672142.476779	43.153652
3523.132519	671660.598119	43.158657
3522.678293	671169.709972	43.163661
3522.563535	670700.424304	43.168666
3522.721765	670223.241263	43.173671
3523.278957	669726.920079	43.178676
3522.970030	669245.579147	43.183681
3523.109599	668773.112477	43.188685
3522.756720	668295.221006	43.193690
3522.481701	667813.551960	43.198695
3522.510768	667334.449651	43.203700
3522.243890	666863.353395	43.208705
3522.173672	666380.579107	43.213709
3522.209464	665914.521333	43.218714
3522.462542	665446.757575	43.223719
3522.584483	664977.446868	43.228724
3522.467754	664506.906681	43.233729
3522.621195	664024.224254	43.238733
3522.695777	663558.942783	43.243738
3522.373587	663069.907429	43.248743
3522.499681	662598.234089	43.253748
3522.108834	662138.301978	43.258753
3522.356660	661663.118990	43.263757
3522.037305	661201.533069	43.268762
3521.858401	660732.614889	43.273767
3521.951815	660261.381585	43.278772
3521.908169	659807.068235	43.283777
3522.071146	659334.480225	43.288781
3521.590069	658873.858868	43.293786
3521.376118	658415.516138	43.298791
3521.625246	657952.430193	43.303796
3521.448157	657509.563432	43.308801
3521.403372	657046.185006	43.313805
3521.486879	656597.491001	43.318810
3521.324059	656149.367642	43.323815
3521.459293	655688.390464	43.328820
3521.731299	655237.754398	43.333825
3521.558775	654774.889283	43.338829
3521.660662	654326.487489	43.343834
3521.639254	653866.300327	43.348839
3521.599253	653412.037997	43.353844
3521.506317	652969.600728	43.358849
3521.200124	652506.751551	43.363853
3521.617098	652061.888939	43.368858
3521.101729	651613.668847	43.373863
3521.373063	651159.799180	43.378868
3521.097569	650714.894328	43.383873
3520.747680	650259.041266	43.388877
3521.036607	649823.991859	43.393882
3521.017537	649377.284636	43.398887
3521.165194	648940.022328	43.403892
3520.741770	648501.039506	43.408897
3520.599871	648052.644965	43.413901
3521.209163	647608.549567	43.418906
3520.779705	647173.807057	43.423911
3521.126929	646731.566555	43.428916
3520.397766	646288.640686	43.433921
3520.813839	645842.850773	43.438925
3521.415332	645408.605501	43.443930
3520.678359	644963.123417	43.448935
3520.828161	644523.268777	43.453940
3520.558621	644088.665469	43.458945
3520.646316	643643.784178	43.463949
3520.690931	643209.539374	43.468954
3520.381128	642778.036247	43.473959
3520.422770	642341.754936	43.478964
3520.198267	641923.000396	43.483969
3520.390092	641480.656451	43.488973
3520.408945	641059.274692	43.493978
3520.316626	640629.343377	43.498983
3520.450004	640191.804109	43.503988
3520.004210	639767.447808	43.508993
3519.997113	639333.696611	43.513997
3519.953211	638910.236410	43.519002
3519.788809	638483.528187	43.524007
3519.750989	638066.884468	43.529012
3519.754587	637648.666137	43.534017
3519.691753	637226.740440	43.539021
3519.878456	636815.060043	43.544026
3519.593623	636393.838510	43.549031
3520.020632	635978.581827	43.554036
3519.685137	635564.439274	43.559041
3519.803917	635141.496817	43.564045
3519.642047	634726.990938	43.569050
3519.600247	634314.749713	43.574055
3519.600605	633895.229248	43.579060
3519.449003	633489.379058	43.584065
3519.590128	633069.551075	43.589069
3519.595153	632658.337198	43.594074
3519.272738	632256.121458	43.599079
3519.146660	631845.298330	43.604084
3519.170419	631433.182214	43.609089
3519.508074	631009.033624	43.614093
3519.462566	630595.544973	43.619098
3519.533038	630188.878047	43.624103
3519.524134	629781.107648	43.629108
3519.232108	629368.513886	43.634113
3519.684325	628956.277535	43.639117
3519.390629	628548.508066	43.644122
3519.021588	628142.688316	43.649127
3519.281515	627725.079621	43.654132
3519.300973	627329.626708	43.659137
3519.001044	626922.146119	43.664141
3519.028836	626519.300923	43.669146
3518.874978	626128.990522	43.674151
3518.961061	625721.247749	43.679156
3518.785804	625323.449824	43.684161
3519.341587	624925.712579	43.689165
3518.580307	624520.121901	43.694170
3518.832043	624118.850583	43.699175
3518.762365	623719.422245	43.704180
3518.699719	623328.643270	43.709185
3518.798650	622926.952690	43.714189
3518.941172	622539.365879	43.719194
3518.327814	622135.062280	43.724199
3518.759107	621741.436130	43.729204
3518.415545	621350.032034	43.734209
3518.474764	620960.098081	43.739213
3518.595588	620582.815370	43.744218
3518.191620	620188.724089	43.749223
3518.654190	619790.562270	43.754228
3518.340616	619407.049530	43.759233
3518.304658	619011.499709	43.764237
3518.152951	618621.216920	43.769242
3517.948208	618256.336412	43.774247
3518.436469	617870.277250	43.779252
3518.141669	617482.533921	43.784257
3518.539050	617093.505922	43.789261
3518.201358	616714.814039	43.794266
3518.090586	616336.772004	43.799271
3518.850550	615945.335685	43.804276
3518.419840	615562.008460	43.809281
3518.626114	615177.606683	43.814285
3518.687189	614785.847332	43.819290
3518.107304	614403.156818	43.824295
3518.120631	614012.430835	43.829300
3517.895284	613634.616189	43.834305
3518.080995	613252.256359	43.839309
3518.261584	612877.655477	43.844314
3518.058403	612485.558743	43.849319
3518.051358	612106.401138	43.854324
3517.583073	611734.880847	43.859329
3517.857897	611349.331291	43.864333
3517.829143	610979.515894	43.869338
3517.779214	610599.913031	43.874343
3518.012546	610223.909780	43.879348
3517.875268	609852.019364	43.884353
3517.828545	609475.737817	43.889357
3517.899070	609103.034706	43.894362
3517.667146	608731.925659	43.899367
3517.969729	608347.170474	43.904372
3517.709218	607974.887621	43.909377
3517.577992	607603.974863	43.914381
3517.828555	607238.502589	43.919386
3518.022452	606864.349691	43.924391
3517.917264	606495.201873	43.929396
3517.563984	606122.823433	43.934401
3517.550179	605735.925977	43.939405
3517.913294	605378.852882	43.944410
3517.569011	604999.060758	43.949415
3517.658448	604622.894760	43.954420
3517.583061	604262.901091	43.959425
3517.808739	603893.260705	43.964429
3517.840583	603517.017747	43.969434
3517.320682	603143.917587	43.974439
3517.599441	602768.761922	43.979444
3517.325084	602400.463220	43.984449
3517.507397	602036.340465	43.989453
3517.852470	601671.927396	43.994458
3517.188603	601303.358741	43.999463
3517.289476	600941.925295	44.004468
3517.388375	600577.268512	44.009473
3517.250594	600208.123130	44.014477
3517.127005	599848.550784	44.019482
3517.160732	599500.535820	44.024487
3517.373437	599128.635567	44.029492
3517.323643	598775.342151	44.034497
3517.271740	598407.580253	44.039501
3517.340324	598037.828170	44.044506
3517.724785	597689.949816	44.049511
3517.581100	597316.997877	44.054516
3516.806929	596952.024232	44.059521
3516.980780	596594.509095	44.064525
3516.999562	596237.411137	44.069530
3516.978097	595883.723550	44.074535
3517.008880	595522.835712	44.079540
3516.730380	595172.283709	44.084545
3516.988400	594809.577495	44.089549
3517.060675	594446.992189	44.094554
3516.595552	594097.896193	44.099559
3516.876566	593749.415738	44.104564
3517.010192	593393.969089	44.109569
3516.671263	593041.103603	44.114573
3516.840362	592684.574737	44.119578
3516.408065	592336.776918	44.124583
3516.492211	591982.702480	44.129588
3516.204724	591648.722892	44.134593
3516.162854	591304.042739	44.139597
3516.489939	590965.568740	44.144602
3516.345189	590617.470283	44.149607
3516.490055	590275.089348	44.154612
3516.200450	589932.220099	44.159617
3516.441008	589587.793499	44.164621
3516.522033	589244.338741	44.169626
3516.243932	588907.919058	44.174631
3516.624764	588560.625244	44.179636
3516.595165	588218.616890	44.184641
3516.376222	587876.631073	44.189645
3516.687000	587526.555608	44.194650
3516.266160	587180.715276	44.199655
3516.415438	586833.611856	44.204660
3516.489394	586510.682616	44.209665
3516.318321	586154.066317	44.214669
3516.562887	585809.781516	44.219674
3516.221960	585474.029942	44.224679
3516.273280	585122.923611	44.229684
3516.298132	584789.352138	44.234689
3516.495640	584446.041635	44.239693
3516.490008	584107.631512	44.244698
3516.286906	583762.912419	44.249703
3516.220154	583425.197358	44.254708
3516.267127	583093.435193	44.259713
3516.026844	582747.487203	44.264717
3515.989676	582414.011748	44.269722
3515.966068	582082.234045	44.274727
3515.969992	581734.255011	44.279732
3515.674094	581405.521708	44.284737
3515.550548	581082.883653	44.289741
3515.682215	580750.037736	44.294746
3515.877729	580415.965211	44.299751
3515.581445	580092.727217	44.304756
3515.648930	579770.776161	44.309761
3515.729070	579436.847511	44.314765
3515.611340	579115.212589	44.319770
3514.933268	578788.887933	44.324775
3515.345219	578462.469100	44.329780
3515.567005	578145.176008	44.334785
3515.120339	577835.230370	44.339789
3515.433890	577513.329170	44.344794
3515.371480	577184.091056	44.349799
3515.377022	576866.047705	44.354804
3515.101155	576552.117995	44.359809
3515.241877	576233.683299	44.364813
3515.389066	575916.899100	44.369818
3514.765787	575607.330267	44.374823
3515.173891	575289.680803	44.379828
3514.788393	574974.724019	44.384833
3514.868562	574668.884840	44.389837
3515.161060	574353.042102	44.394842
3515.098397	574046.105420	44.399847
3515.067159	573728.843397	44.404852
3514.859824	573426.544254	44.409857
3514.819181	573113.393337	44.414861
3514.956410	572802.870584	44.419866
3514.711840	572493.210298	44.424871
3515.210106	572178.283857	44.429876
3514.932898	571884.059578	44.434881
3514.497575	571564.145352	44.439885
3515.093541	571269.958922	44.444890
3515.012064	570954.245559	44.449895
3515.196426	570646.227739	44.454900
3515.196187	570338.586171	44.459905
3515.187666	570028.120661	44.464909
3515.147363	569716.093038	44.469914
3514.622235	569407.310800	44.474919
3514.903077	569102.912531	44.479924
3514.732091	568797.225368	44.484929
3514.559983	568488.662505	44.489933
3514.333275	568178.440714	44.494938
3514.234214	567886.106327	44.499943
3514.216466	567593.550052	44.504948
3514.372066	567301.964092	44.509953
3514.711114	567001.280530	44.514957
3514.604501	566697.495054	44.519962
3514.868177	566406.021259	44.524967
3514.934219	566102.292886	44.529972
3514.620150	565792.632240	44.534977
3514.788017	565503.067104	44.539981
3514.849160	565192.371552	44.544986
3514.601915	564888.416338	44.549991
3514.410593	564578.554540	44.554996
3514.336415	564290.060661	44.560001
3514.500836	563992.306823	44.565005
3514.454473	563685.872565	44.570010
3514.312566	563406.130460	44.575015
3514.526742	563096.768111	44.580020
3514.324286	562799.855079	44.585025
3513.882779	562505.694917	44.590029
3514.289267	562218.281275	44.595034
3514.252560	561924.038860	44.600039
3514.089029	561635.853728	44.605044
3514.244602	561345.291497	44.610049
3514.122898	561053.914120	44.615053
3514.116765	560759.791316	44.620058
3513.794725	560473.017567	44.625063
3513.959614	560184.039377	44.630068
3513.696353	559900.113457	44.635073
3513.708815	559617.393321	44.640077
3513.982123	559332.255599	44.645082
3513.574868	559067.322390	44.650087
3513.702853	558764.268255	44.655092
3514.033770	558496.830472	44.660097
3514.020667	558206.076483	44.665101
3514.434158	557915.243262	44.670106
3514.025633	557641.769703	44.675111
3514.110011	557345.590822	44.680116
3514.009372	557060.568630	44.685121
3514.346124	556767.607782	44.690125
3514.285928	556485.084868	44.695130
3513.945603	556202.150417	44.700135
3514.071555	555900.542288	44.705140
3513.913805	555624.213764	44.710145
3513.942710	555333.591159	44.715149
3514.176782	555054.262104	44.720154
3513.742322	554770.708806	44.725159
3513.517661	554480.312439	44.730164
3513.497104	554200.202943	44.735169
3513.234213	553922.597663	44.740173
3513.515052	553642.072373	44.745178
3513.385620	553381.059370	44.750183
3513.067812	553099.667670	44.755188
3513.404027	552836.952289	44.760193
3513.064595	552568.048805	44.765197
3513.326438	552287.851222	44.770202
3512.990869	552033.700015	44.775207
3513.059905	551752.919579	44.780212
3513.055327	551492.755691	44.785217
3513.295028	551216.016615	44.790221
3513.037795	550955.028867	44.795226
3512.878028	550693.868269	44.800231
3513.432841	550416.202371	44.805236
3513.204316	550153.581669	44.810241
3512.814847	549894.107962	44.815245
3512.899155	549631.070978	44.820250
3512.991864	549373.621722	44.825255
3513.382270	549101.400109	44.830260
3513.340417	548837.210157	44.835265
3513.310792	548571.500960	44.840269
3513.452257	548295.122454	44.845274
3513.309579	548034.563184	44.850279
3513.507523	547762.549387	44.855284
3513.438463	547491.180647	44.860289
3513.183196	547226.895239	44.865293
3513.318565	546953.212669	44.870298
3513.035575	546687.762252	44.875303
3513.258497	546414.205235	44.880308
3512.739887	546155.489236	44.885313
3512.834189	545893.991934	44.890317
3512.811606	545632.005510	44.895322
3512.616090	545373.018025	44.900327
3512.680338	545117.157432	44.905332
3512.946119	544859.442756	44.910337
3512.514911	544601.086046	44.915341
3512.821734	544353.135663	44.920346
3512.750602	544101.917802	44.925351
3512.731267	543838.283527	44.930356
3512.612724	543581.064502	44.935361
3512.536269	543319.598198	44.940365
3512.675328	543068.124097	44.945370
3512.385203	542826.904086	44.950375
3512.396332	542568.787055	44.955380
3512.337215	542326.510488	44.960385
3512.302666	542069.904770	44.965389
3512.564332	541823.329000	44.970394
3512.341831	541577.436679	44.975399
3512.361020	541325.749999	44.980404
3512.362132	541093.275255	44.985409
3512.185033	540841.714268	44.990413
3512.148158	540597.790278	44.995418
3512.056994	540349.130777	45.000423
3512.150102	540101.544933	45.005428
3512.129350	539864.262547	45.010433
3511.943819	539620.901789	45.015437
3511.942541	539378.967990	45.020442
3511.828333	539147.893010	45.025447
3511.947678	538908.956716	45.030452
3512.091901	538669.608644	45.035457
3512.163130	538439.801820	45.040461
3511.883486	538193.507165	45.045466
3511.869217	537965.371744	45.050471
3511.820790	537719.332027	45.055476
3511.781489	537479.743025	45.060481
3511.695124	537244.092538	45.065485
3511.676255	537013.117855	45.070490
3511.408668	536786.166979	45.075495
3511.574141	536553.539170	45.080500
3511.778672	536321.254025	45.085505
3511.743419	536092.537304	45.090509
3511.902805	535860.302828	45.095514
3511.668631	535638.978133	45.100519
3511.860920	535395.480568	45.105524
3511.951251	535163.549289	45.110529
3511.430390	534928.237522	45.115533
3511.536001	534706.840436	45.120538
3511.629744	534484.130212	45.125543
3511.483814	534251.417320	45.130548
3511.235212	534030.373024	45.135553
3511.360822	533801.895082	45.140557
3511.672582	533587.660604	45.145562
3510.964883	533363.354422	45.150567
3511.255739	533141.548482	45.155572
3511.427571	532920.869532	45.160577
3511.404861	532700.624103	45.165581
3511.287214	532475.749290	45.170586
3510.912144	532259.594055	45.175591
3511.310862	532036.894976	45.180596
3511.195454	531817.459339	45.185601
3511.140437	531599.725795	45.190605
3511.173235	531379.097609	45.195610
3510.859170	531161.754984	45.200615
3511.126134	530957.834397	45.205620
3511.062033	530736.859783	45.210625
3511.211062	530513.776329	45.215629
3511.433454	530298.903026	45.220634
3511.135287	530091.483695	45.225639
3511.221940	529867.744960	45.230644
3511.548144	529655.822119	45.235649
3510.979454	529435.115869	45.240653
3511.220023	529211.340838	45.245658
3510.675588	529003.594864	45.250663
3510.705386	528784.896443	45.255668
3510.903262	528581.005042	45.260673
3510.718116	528370.766095	45.265677
3510.775564	528161.845529	45.270682
3510.560080	527946.558300	45.275687
3510.702964	527744.885614	45.280692
3510.600898	527542.848186	45.285697
3510.414799	527340.923298	45.290701
3510.926778	527130.396229	45.295706
3510.669443	526931.102746	45.300711
3510.987782	526713.434894	45.305716
3510.633046	526515.212506	45.310721
3510.696368	526308.839228	45.315725
3510.803997	526107.604591	45.320730
3510.689299	525903.780135	45.325735
3510.645102	525694.185845	45.330740
3510.585842	525486.812437	45.335745
3510.253324	525294.173604	45.340749
3510.387245	525093.980935	45.345754
3510.095994	524893.757202	45.350759
3510.180456	524699.827855	45.355764
3510.342529	524498.511707	45.360769
3510.497356	524308.503220	45.365773
3510.602411	524107.898373	45.370778
3510.266999	523916.050068	45.375783
3510.226526	523713.243289	45.380788
3510.201066	523516.792927	45.385793
3510.018404	523325.365394	45.390797
3510.112800	523120.962380	45.395802
3509.819008	522943.888449	45.400807
3510.069552	522754.702306	45.405812
3510.107855	522561.056142	45.410817
3509.840886	522376.043539	45.415821
3510.147007	522188.002149	45.420826
3509.961270	522002.870110	45.425831
3510.216539	521806.198012	45.430836
3510.119134	521630.135526	45.435841
3509.711420	521437.964999	45.440845
3509.925510	521236.646818	45.445850
3509.834667	521047.699571	45.450855
3509.891958	520876.954712	45.455860
3509.900248	520693.793477	45.460865
3509.783063	520510.095955	45.465869
3509.870558	520320.402203	45.470874
3509.534327	520139.616132	45.475879
3509.813546	519952.763624	45.480884
3509.695767	519769.966294	45.485889
3509.309363	519596.202159	45.490893
3509.464111	519413.505530	45.495898
3509.558218	519245.513767	45.500903
3509.416494	519066.297880	45.505908
3509.753925	518889.674859	45.510913
3509.188257	518715.123214	45.515917
3509.526571	518531.930150	45.520922
3509.325981	518363.423439	45.525927
3509.735069	518178.294796	45.530932
3509.826766	518008.067522	45.535937
3509.419396	517832.064554	45.540941
3509.956691	517658.373235	45.545946
3509.583336	517486.098183	45.550951
3509.590907	517303.047938	45.555956
3509.439007	517129.114739	45.560961
3509.388315	516959.455783	45.565965
3509.354877	516777.062937	45.570970
3509.251053	516614.329425	45.575975
3509.735544	516432.349201	45.580980
3509.638944	516257.689540	45.585985
3509.271720	516088.883275	45.590989
3509.275624	515915.313902	45.595994
3509.281142	515747.147475	45.600999
3509.333418	515578.769174	45.606004
3509.387398	515407.155683	45.611009
3508.988404	515243.649874	45.616013
3509.027346	515076.834431	45.621018
3509.222731	514916.608383	45.626023
3509.478342	514742.629275	45.631028
3509.398069	514577.243350	45.636033
3509.451270	514414.005234	45.641037
3509.379617	514236.539947	45.646042
3509.370831	514069.772369	45.651047
3509.344370	513900.682032	45.656052
3509.517419	513720.339877	45.661057
3509.312056	513550.568979	45.666061
3509.860324	513381.172795	45.671066
3509.303372	513219.592575	45.676071
3509.453753	513042.530514	45.681076
3509.249683	512881.593891	45.686081
3508.996521	512713.287285	45.691085
3509.359323	512540.073733	45.696090
3508.900697	512376.345926	45.701095
3509.067568	512211.903289	45.706100
3509.488096	512047.365095	45.711105
3509.121182	511887.254513	45.716109
3509.246293	511719.377942	45.721114
3508.950281	511552.885240	45.726119
3508.762075	511376.418016	45.731124
3508.736703	511222.356450	45.736129
3508.883330	511073.872920	45.741133
3508.928903	510915.652727	45.746138
3508.744392	510760.401071	45.751143
3508.549239	510605.250770	45.756148
3508.728619	510454.229212	45.761153
3508.720804	510300.054583	45.766157
3509.104890	510132.521180	45.771162
3508.880587	509988.184014	45.776167
3508.978212	509821.403710	45.781172
3508.847940	509665.070817	45.786177
3508.513200	509513.117363	45.791181
3508.621848	509347.947341	45.796186
3508.519184	509193.929760	45.801191
3508.313887	509048.266844	45.806196
3508.689862	508891.385066	45.811201
3508.447542	508740.014891	45.816205
3508.687107	508593.614863	45.821210
3508.486083	508452.595318	45.826215
3508.720251	508306.850586	45.831220
3509.070273	508146.781923	45.836225
3508.816747	507996.366862	45.841229
3508.775358	507837.473819	45.846234
3508.882050	507685.730805	45.851239
3508.636221	507522.674596	45.856244
3508.915991	507370.292536	45.861249
3508.516988	507226.768850	45.866253
3508.839114	507074.629462	45.871258
3508.695500	506922.163800	45.876263
3508.732428	506771.485461	45.881268
3509.015468	506615.456478	45.886273
3508.818207	506459.255260	45.891277
3508.750910	506305.608171	45.896282
3508.453609	506162.664154	45.901287
3508.355137	506013.417123	45.906292
3508.460598	505866.155779	45.911297
3508.231794	505726.683952	45.916301
3508.400542	505576.073008	45.921306
3508.436147	505431.650317	45.926311
3508.212367	505284.894818	45.931316
3508.228349	505140.119027	45.936321
3508.006222	505001.650786	45.941325
3508.108779	504855.846670	45.946330
3508.199097	504726.623994	45.951335
3508.277957	504587.949170	45.956340
3508.233198	504441.357656	45.961345
3508.122878	504309.082255	45.966349
3507.984329	504167.913354	45.971354
3508.158164	504028.560348	45.976359
3508.170428	503886.149976	45.981364
3508.334563	503748.413933	45.986369
3508.352046	503609.539014	45.991373
3508.314013	503459.297581	45.996378
3508.376442	503331.130210	46.001383
3507.957704	503185.147322	46.006388
3508.272655	503045.509026	46.011393
3508.009014	502908.142250	46.016397
3508.140110	502766.510700	46.021402
3508.028287	502634.879185	46.026407
3507.868328	502499.665231	46.031412
3507.946262	502368.605863	46.036417
3507.994669	502239.775061	46.041421
3507.854923	502098.133405	46.046426
3508.016763	501964.528528	46.051431
3507.805421	501829.671725	46.056436
3507.973948	501692.473746	46.061441
3507.773730	501573.134903	46.066445
3508.123848	501430.240943	46.071450
3507.847502	501302.317758	46.076455
3507.976433	501165.273818	46.081460
3507.881963	501040.705183	46.086465
3507.939731	500904.884715	46.091469
3508.208999	500781.162138	46.096474
3507.788440	500644.157113	46.101479
3507.658382	500513.017315	46.106484
3507.938006	500375.890510	46.111489
3507.590970	500253.381611	46.116493
3508.069476	500113.134224	46.121498
3507.945545	499992.658464	46.126503
3507.848367	499860.749386	46.131508
3508.010287	499731.272762	46.136513
3507.788227	499608.080377	46.141517
3507.969111	499468.181736	46.146522
3507.687290	499352.481567	46.151527
3508.058813	499216.391369	46.156532
3508.008942	499074.607229	46.161537
3507.670434	498951.278134	46.166541
3507.781434	498822.763908	46.171546
3507.630383	498706.430074	46.176551
3507.427308	498573.112883	46.181556
3507.585460	498449.998683	46.186561
3507.271571	498324.031079	46.191565
3507.545931	498204.688009	46.196570
3507.509742	498083.374259	46.201575
3507.323059	497959.556739	46.206580
3507.671822	497834.079146	46.211585
3507.256743	497708.073587	46.216589
3507.753287	497587.575572	46.221594
3507.585686	497467.544095	46.226599
3507.363658	497348.886532	46.231604
3507.494303	497230.825370	46.236609
3507.229469	497113.589511	46.241613
3507.587315	496984.159197	46.246618
3507.462959	496871.196491	46.251623
3507.574391	496750.201873	46.256628
3507.682760	496626.981576	46.261633
3507.263588	496505.873487	46.266637
3507.425892	496380.062790	46.271642
3507.369199	496280.335555	46.276647
3507.287051	496167.512628	46.281652
3507.203027	496045.433604	46.286657
3507.117952	495929.524357	46.291661
3507.194631	495815.407504	46.296666
3507.076865	495695.405400	46.301671
3507.030486	495586.264690	46.306676
3507.671804	495468.103932	46.311681
3507.450302	495363.038006	46.316685
3507.577964	495232.166691	46.321690
3507.822558	495115.740335	46.326695
3507.445593	494986.925905	46.331700
3507.659414	494868.075227	46.336705
3507.361932	494747.338343	46.341709
3507.620160	494621.042894	46.346714
3507.269527	494516.094905	46.351719
3507.472680	494396.079344	46.356724
3507.304695	494272.383181	46.361729
3507.149773	494163.555302	46.366733
3507.330044	494039.949728	46.371738
3507.116936	493939.173101	46.376743
3507.402101	493825.361290	46.381748
3507.329859	493708.321753	46.386753
3506.998970	493603.870583	46.391757
3506.975549	493479.891029	46.396762
3506.952648	493377.358697	46.401767
3507.130235	493271.554030	46.406772
3507.152778	493168.506822	46.411777
3507.067161	493045.900545	46.416781
3507.148649	492927.767071	46.421786
3507.101026	492830.648442	46.426791
3507.222362	492712.304323	46.431796
3507.193256	492609.363724	46.436801
3506.847665	492500.051868	46.441805
3507.387994	492387.755104	46.446810
3506.975669	492285.383864	46.451815
3506.815695	492171.788768	46.456820
3507.029845	492061.265574	46.461825
3506.698687	491951.340668	46.466829
3507.014768	491843.328142	46.471834
3507.192112	491737.564594	46.476839
3507.057934	491634.585472	46.481844
3507.353101	491525.562703	46.486849
3507.034484	491401.213718	46.491853
3507.002959	491298.670371	46.496858
3507.142534	491192.909910	46.501863
3507.095218	491091.076304	46.506868
3507.250289	490983.743553	46.511873
3506.799086	490873.579265	46.516877
3507.493528	490768.429752	46.521882
3507.240145	490657.724373	46.526887
3507.152818	490538.692552	46.531892
3507.159711	490428.295413	46.536897
3506.720431	490322.628432	46.541901
3506.750049	490213.440301	46.546906
3506.562617	490114.964091	46.551911
3506.682112	490016.738484	46.556916
3506.833392	489921.036671	46.561921
3506.626171	489813.960868	46.566925
3506.486078	489714.715351	46.571930
3506.643249	489615.317315	46.576935
3506.522420	489519.254963	46.581940
3506.717321	489413.372937	46.586945
3506.394399	489328.576579	46.591949
3506.495641	489220.078300	46.596954
3506.315890	489128.931811	46.601959
3506.350226	489033.194453	46.606964
3506.424742	488936.741326	46.611969
3506.656473	488846.990453	46.616973
3506.652642	488755.457772	46.621978
3506.318719	488665.751942	46.626983
3506.361178	488560.649722	46.631988
3506.313800	488465.125578	46.636993
3506.360642	488386.080453	46.641997
3506.568021	488282.871197	46.647002
3506.601615	488190.873746	46.652007
3506.299344	488099.641566	46.657012
3506.212455	487995.317026	46.662017
3506.399173	487907.390629	46.667021
3506.352280	487811.457999	46.672026
3506.243859	487724.390698	46.677031
3506.456662	487640.101842	46.682036
3506.763101	487547.345974	46.687041
3506.617180	487454.970466	46.692045
3506.694113	487357.799731	46.697050
3506.825701	487260.214296	46.702055
3506.581415	487163.198530	46.707060
3506.736440	487063.128414	46.712065
3506.358658	486970.233286	46.717069
3506.653331	486876.666199	46.722074
3506.699436	486779.446907	46.727079
3506.510977	486684.493745	46.732084
3506.881656	486578.109012	46.737089
3506.668177	486491.964401	46.742093
3506.793112	486394.324667	46.747098
3506.645317	486298.249139	46.752103
3506.237955	486209.302299	46.757108
3506.292654	486114.102103	46.762113
3506.065506	486025.781448	46.767117
3506.451125	485933.054114	46.772122
3506.193468	485855.972605	46.777127
3506.030998	485764.805579	46.782132
3506.574990	485674.732049	46.787137
3506.317320	485584.592502	46.792141
3506.236081	485490.019433	46.797146
3506.188102	485402.272354	46.802151
3505.969194	485321.740494	46.807156
3506.234331	485237.937240	46.812161
3506.202327	485149.528255	46.817165
3506.017010	485063.877927	46.822170
3506.279185	484981.946521	46.827175
3505.873965	484890.411534	46.832180
3506.292227	484801.519045	46.837185
3506.069272	484724.831541	46.842189
3506.103101	484639.344176	46.847194
3506.137227	484550.465401	46.852199
3506.279630	484474.422984	46.857204
3506.275889	484385.043729	46.862209
3505.747928	484303.244084	46.867213
3505.947352	484216.663554	46.872218
3506.360941	484125.693370	46.877223
3506.204052	484047.979401	46.882228
3506.302997	483958.327396	46.887233
3505.785178	483885.685012	46.892237
3506.239994	483794.048118	46.897242
3506.246120	483716.203634	46.902247
3505.965751	483629.398475	46.907252
3506.065626	483548.146123	46.912257
3505.816522	483468.572641	46.917261
3506.054729	483386.334260	46.922266
3506.130946	483309.538930	46.927271
3505.822559	483225.621617	46.932276
3505.886191	483136.831946	46.937281
3505.809812	483062.035594	46.942285
3506.029725	482983.645245	46.947290
3506.058164	482902.402140	46.952295
3505.692516	482823.503675	46.957300
3505.652066	482744.296254	46.962305
3505.574769	482671.219370	46.967309
3505.555203	482592.412640	46.972314
3505.969351	482511.709299	46.977319
3505.774069	482445.738010	46.982324
3505.986229	482371.901838	46.987329
3505.800424	482290.591291	46.992333
3505.814010	482216.484675	46.997338
3505.697821	482138.249233	47.002343
3505.832060	482066.399206	47.007348
3505.921946	481993.088528	47.012353
3506.049405	481910.912871	47.017357
3505.875274	481829.243900	47.022362
3506.117249	481748.161558	47.027367
3505.743498	481674.675642	47.032372
3506.186083	481595.026316	47.037377
3506.098402	481516.428950	47.042381
3506.331120	481445.774492	47.047386
3506.114804	481356.416329	47.052391
3506.006279	481276.049759	47.057396
3506.331846	481182.751053	47.062401
3506.112345	481112.931809	47.067405
3505.704947	481039.094684	47.072410
3505.758683	480964.317958	47.077415
3505.597278	480893.121163	47.082420
3505.975123	480820.009630	47.087425
3505.838273	480744.960802	47.092429
3505.775583	480661.850072	47.097434
3505.906449	480583.666907	47.102439
3505.407742	480510.197555	47.107444
3505.640851	480445.816303	47.112449
3505.763153	480371.126650	47.117453
3505.714802	480293.428431	47.122458
3506.117872	480226.891203	47.127463
3505.666168	480148.906866	47.132468
3506.249827	480075.554678	47.137473
3505.839404	480007.282455	47.142477
3505.836579	479925.018712	47.147482
3505.882262	479835.304511	47.152487
3505.857675	479772.281093	47.157492
3506.004971	479688.168151	47.162497
3505.762046	479619.511487	47.167501
3505.971381	479543.740423	47.172506
3505.914202	479465.685771	47.177511
3505.548904	479397.707290	47.182516
3505.926061	479315.173391	47.187521
3505.889890	479243.543691	47.192525
3506.089361	479180.429328	47.197530
3505.765188	479104.089373	47.202535
3505.736339	479020.712177	47.207540
3505.615982	478953.044591	47.212545
3505.566947	478885.212694	47.217549
3505.981011	478806.264706	47.222554
3505.882374	478729.884666	47.227559
3505.941234	478653.882436	47.232564
3506.078088	478574.474494	47.237569
3505.565026	478517.200450	47.242573
3505.739318	478449.075651	47.247578
3505.825863	478374.940778	47.252583
3505.665963	478295.582284	47.257588
3505.816087	478230.397264	47.262593
3505.558809	478165.180312	47.267597
3505.751266	478084.900042	47.272602
3505.552818	478017.191674	47.277607
3505.662607	477946.747047	47.282612
3505.496611	477876.298606	47.287617
3505.383941	477813.334051	47.292621
3505.259953	477749.206714	47.297626
3505.018432	477683.985348	47.302631
3505.080352	477611.522378	47.307636
3505.582297	477554.071996	47.312641
3505.438794	477495.972173	47.317645
3505.288138	477433.670997	47.322650
3505.407637	477363.880667	47.327655
3505.282075	477303.448124	47.332660
3505.034387	477236.454106	47.337665
3504.947875	477179.305548	47.342669
3505.442460	477119.272830	47.347674
3505.130641	477063.782607	47.352679
3505.177832	477011.673919	47.357684
3505.539592	476943.308959	47.362689
3505.309856	476871.348545	47.367693
3505.425792	476815.784534	47.372698
3505.452259	476753.552063	47.377703
3505.025328	476697.877852	47.382708
3505.385237	476631.334841	47.387713
3505.218586	476571.362596	47.392717
3505.416385	476504.239200	47.397722
3505.496579	476441.034453	47.402727
3505.205208	476387.260242	47.407732
3505.431550	476311.219662	47.412737
3505.069249	476259.634462	47.417741
3505.106038	476190.917109	47.422746
3505.302561	476134.881564	47.427751
3505.255468	476072.608709	47.432756
3505.365917	476008.030162	47.437761
3505.085678	475952.429910	47.442765
3505.145108	475884.720252	47.447770
3505.093832	475830.093246	47.452775
3504.975870	475790.516287	47.457780
3505.500098	475724.802746	47.462785
3504.990953	475670.759804	47.467789
3504.741463	475607.152756	47.472794
3505.357139	475550.993230	47.477799
3505.172364	475498.210944	47.482804
3505.036915	475433.469820	47.487809
3504.907773	475391.868444	47.492813
3505.050323	475332.598914	47.497818
3505.341644	475268.290713	47.502823
3504.712894	475220.545880	47.507828
3505.144610	475160.618778	47.512833
3504.878312	475106.785903	47.517837
3504.755521	475055.561532	47.522842
3505.310418	474996.017966	47.527847
3505.473751	474948.744841	47.532852
3505.281864	474878.947602	47.537857
3505.148301	474827.369969	47.542861
3505.075862	474772.439613	47.547866
3505.253890	474713.364594	47.552871
3505.101903	474657.333426	47.557876
3505.945198	474598.296368	47.562881
3505.679162	474533.928860	47.567885
3505.514773	474463.011292	47.572890
3505.829938	474405.734895	47.577895
3505.611066	474337.915162	47.582900
3505.541876	474273.158659	47.587905
3505.590102	474205.748598	47.592909
3505.680077	474143.091348	47.597914
3505.778614	474077.596560	47.602919
3505.120807	474012.737087	47.607924
3505.669578	473938.606668	47.612929
3505.237403	473880.747281	47.617933
3505.175156	473830.319437	47.622938
3505.318744	473762.283788	47.627943
3505.343362	473710.372190	47.632948
3505.179366	473641.477071	47.637953
3504.853977	473601.323141	47.642957
3504.916711	473538.415294	47.647962
3505.070780	473484.252717	47.652967
3504.743479	473441.110886	47.657972
3505.146705	473378.245644	47.662977
3504.907408	473331.239713	47.667981
3504.729001	473274.044101	47.672986
3505.217626	473222.051914	47.677991
3504.844565	473173.042712	47.682996
3505.397827	473126.761871	47.688001
3504.738293	473078.257119	47.693005
3505.032363	473016.320872	47.698010
3505.081720	472967.796082	47.703015
3504.733868	472917.211954	47.708020
3504.991398	472858.978406	47.713025
3504.808589	472810.087696	47.718029
3504.791156	472765.979802	47.723034
3504.923758	472719.820421	47.728039
3504.993815	472664.454348	47.733044
3504.681576	472613.204939	47.738049
3504.816200	472564.310030	47.743053
3504.650091	472515.618275	47.748058
3504.861229	472466.861981	47.753063
3504.586304	472420.872733	47.758068
3504.797249	472366.849136	47.763073
3504.751442	472323.555364	47.768077
3504.622136	472279.262842	47.773082
3504.681549	472228.252792	47.778087
3504.656178	472181.460664	47.783092
3504.781725	472131.603907	47.788097
3504.594553	472089.650520	47.793101
3504.320363	472050.396131	47.798106
3504.683513	471995.281910	47.803111
3504.427150	471971.522012	47.808116
3504.668702	471918.859343	47.813121
3504.572013	471886.614139	47.818125
3504.777559	471837.502637	47.823130
3504.642983	471798.578408	47.828135
3504.749396	471743.709870	47.833140
3504.849608	471697.908027	47.838145
3504.410017	471659.795293	47.843149
3504.687757	471611.481224	47.848154
3504.701130	471569.087252	47.853159
3504.619135	471532.888446	47.858164
3504.483192	471484.594037	47.863169
3504.728961	471439.273186	47.868173
3504.895825	471390.572300	47.873178
3504.796564	471343.588107	47.878183
3504.770930	471303.732589	47.883188
3504.863252	471251.903897	47.888193
3505.167503	471211.485378	47.893197
3505.000703	471147.494418	47.898202
3504.609761	471100.407474	47.903207
3504.295606	471070.375885	47.908212
3504.488154	471017.415165	47.913217
3504.229797	470976.079226	47.918221
3504.478719	470942.000680	47.923226
3504.572693	470899.439489	47.928231
3504.321951	470866.509750	47.933236
3504.408856	470808.501566	47.938241
3504.267219	470775.046546	47.943245
3504.326366	470750.268891	47.948250
3504.484884	470704.404025	47.953255
3504.367034	470664.005752	47.958260
3504.558341	470625.023450	47.963265
3504.433872	470583.866389	47.968269
3504.417486	470554.846782	47.973274
3504.400915	470508.454185	47.978279
3504.150241	470479.018613	47.983284
3504.462087	470440.167299	47.988289
3504.458963	470393.670823	47.993293
3504.416567	470356.652586	47.998298
3504.550520	470324.466624	48.003303
3504.294186	470283.989881	48.008308
3504.620604	470238.753675	48.013313
3504.577816	470196.771409	48.018317
3504.472178	470158.142751	48.023322
3504.864773	470126.418801	48.028327
3504.612995	470087.865602	48.033332
3504.821950	470041.433351	48.038337
3505.132400	470006.988054	48.043341
3504.511497	469953.909984	48.048346
3504.832204	469908.825920	48.053351
3504.497412	469861.675641	48.058356
3504.816451	469832.850913	48.063361
3504.623679	469789.576402	48.068365
3504.503044	469752.418385	48.073370
3504.813326	469707.436925	48.078375
3504.603511	469670.040711	48.083380
3504.717687	469613.543773	48.088385
3504.875261	469574.666372	48.093389
3504.646410	469529.168712	48.098394
3504.500786	469485.733498	48.103399
3504.664266	469447.715927	48.108404
3504.629975	469399.398823	48.113409
3504.794783	469357.733822	48.118413
3504.737620	469312.358287	48.123418
3504.579407	469273.939414	48.128423
3504.559290	469237.168450	48.133428
3504.835881	469193.863092	48.138433
3504.796350	469147.926963	48.143437
3504.610507	469110.829475	48.148442
3504.440984	469069.930081	48.153447
3504.581330	469033.941790	48.158452
3504.139965	468993.291263	48.163457
3504.008028	468955.930997	48.168461
3504.122068	468921.871846	48.173466
3504.469901	468891.267872	48.178471
3504.299665	468861.258850	48.183476
3504.434010	468830.437957	48.188481
3504.425685	468785.610024	48.193485
3504.151205	468753.339169	48.198490
3504.188982	468715.493560	48.203495
3503.980377	468682.806098	48.208500
3504.543047	468647.758066	48.213505
3504.247870	468625.266955	48.218509
3504.291504	468584.431432	48.223514
3504.308226	468547.754155	48.228519
3504.179298	468527.412722	48.233524
3504.304130	468478.964798	48.238529
3504.275002	468441.788590	48.243533
3504.019858	468428.611043	48.248538
3504.049979	468391.576589	48.253543
3504.094929	468364.113484	48.258548
3504.280872	468322.138673	48.263553
3503.887144	468294.649058	48.268557
3503.558041	468260.461764	48.273562
3504.239999	468226.456370	48.278567
3504.234689	468215.312922	48.283572
3504.293349	468188.657724	48.288577
3504.503548	468149.819082	48.293581
3503.920765	468112.230201	48.298586
3504.121393	468086.259811	48.303591
3503.565152	468070.904537	48.308596
3504.037140	468022.852090	48.313601
3504.152072	467993.654175	48.318605
3504.057830	467975.687100	48.323610
3504.102416	467948.122145	48.328615
3504.071067	467924.774648	48.333620
3504.188303	467881.949431	48.338625
3504.378052	467860.691703	48.343629
3504.302933	467835.983827	48.348634
3504.106831	467795.795437	48.353639
3504.205802	467779.010963	48.358644
3504.095411	467742.353842	48.363649
3503.970628	467705.597793	48.368653
3504.067733	467672.349824	48.373658
3504.485671	467645.379236	48.378663
3504.090503	467624.322432	48.383668
3504.297563	467578.796336	48.388673
3504.435414	467554.760945	48.393677
3504.377021	467527.922179	48.398682
3504.044644	467480.714924	48.403687
3503.933253	467459.305536	48.408692
3503.880304	467439.912476	48.413697
3503.625649	467414.880102	48.418701
3503.710237	467374.440266	48.423706
3504.176167	467347.663699	48.428711
3504.064502	467335.170117	48.433716
3504.005585	467307.165985	48.438721
3504.138296	467270.973039	48.443725
3503.798821	467240.078505	48.448730
3504.289575	467215.577162	48.453735
3504.218820	467198.314570	48.458740
3504.177940	467161.289855	48.463745
3504.349868	467138.261304	48.468749
3504.488211	467115.441095	48.473754
3504.385986	467072.296926	48.478759
3504.184062	467049.433418	48.483764
3503.809666	467009.983050	48.488769
3504.095686	466998.485194	48.493773
3503.827466	466966.868821	48.498778
3504.142729	466935.912664	48.503783
3503.890554	466920.200587	48.508788
3504.067615	466899.855834	48.513793
3504.345334	466860.395133	48.518797
3503.674398	466835.078460	48.523802
3504.328508	466809.586170	48.528807
3503.997890	466794.697943	48.533812
3504.050290	466750.716089	48.538817
3504.094978	466719.400502	48.543821
3504.108299	466707.493092	48.548826
3504.212076	466681.790638	48.553831
3504.045318	466647.167457	48.558836
3504.219389	466616.640178	48.563841
3503.942673	466591.357192	48.568845
3503.807678	466566.151297	48.573850
3503.971088	466525.949519	48.578855
3504.073131	466508.758124	48.583860
3504.004336	466488.201611	48.588865
3504.151331	466478.753614	48.593869
3503.710075	466441.542569	48.598874
3504.173503	466410.053659	48.603879
3503.820478	466394.459692	48.608884
3504.145488	466373.582512	48.613889
3504.167697	466353.111638	48.618893
3503.538477	466311.018301	48.623898
3504.001102	466280.745188	48.628903
3503.585544	466268.353460	48.633908
3503.908112	466251.174843	48.638913
3504.027940	466247.253465	48.643917
3503.935486	466209.577124	48.648922
3504.042799	466169.688150	48.653927
3504.279322	466142.949078	48.658932
3504.427000	466126.256168	48.663937
3504.247795	466094.471175	48.668941
3504.205782	466062.105424	48.673946
3504.401347	466032.688111	48.678951
3504.358644	465998.751850	48.683956
3504.251317	465971.513968	48.688961
3503.973024	465949.928745	48.693965
3503.910549	465916.198363	48.698970
3504.220405	465884.278857	48.703975
3504.121285	465880.242802	48.708980
3504.006329	465844.292109	48.713985
3504.500030	465807.477487	48.718989
3503.954536	465788.268185	48.723994
3504.220879	465767.349704	48.728999
3504.087808	465725.170371	48.734004
3503.747804	465698.022493	48.739009
3503.698402	465673.256780	48.744013
3503.621223	465659.844287	48.749018
3503.984802	465637.743815	48.754023
3503.670684	465630.552646	48.759028
3503.917669	465606.597513	48.764033
3504.093655	465578.398767	48.769037
3503.407307	465551.917778	48.774042
3503.935731	465529.839700	48.779047
3503.929219	465520.518772	48.784052
3503.931987	465504.002056	48.789057
3503.636156	465466.814959	48.794061
3503.586366	465440.022474	48.799066
3503.590746	465412.562076	48.804071
3503.501347	465413.742615	48.809076
3503.590092	465400.352275	48.814081
3503.808350	465374.476541	48.819085
3503.551984	465367.731386	48.824090
3503.785395	465352.897727	48.829095
3503.836438	465340.071084	48.834100
3503.871906	465324.359253	48.839105
3503.814453	465292.501487	48.844109
3503.950424	465262.485210	48.849114
3504.021748	465236.583716	48.854119
3503.652717	465236.089433	48.859124
3503.733533	465218.039224	48.864129
3503.775093	465195.385261	48.869133
3503.808160	465182.004277	48.874138
3504.007987	465150.051683	48.879143
3503.778726	465133.624933	48.884148
3503.642234	465116.574356	48.889153
3503.732310	465106.071455	48.894157
3503.851963	465086.393232	48.899162
3504.121957	465062.230840	48.904167
3503.735685	465046.337470	48.909172
3503.921025	465013.120509	48.914177
3503.862882	464986.886134	48.919181
3503.549174	464984.305143	48.924186
3503.746099	464965.576233	48.929191
3503.463251	464956.454210	48.934196
3503.525829	464936.937574	48.939201
3503.499635	464936.840729	48.944205
3503.062780	464914.217458	48.949210
3503.197573	464894.485790	48.954215
3503.179668	464886.078471	48.959220
3503.475159	464872.652465	48.964225
3503.519037	464861.853330	48.969229
3503.382449	464858.026118	48.974234
3503.626350	464840.049043	48.979239
3503.666109	464829.605249	48.984244
3503.761850	464811.501448	48.989249
3503.635563	464781.275880	48.994253
3503.406721	464760.947516	48.999258
3503.453904	464742.851942	49.004263
3503.315542	464735.174440	49.009268
3503.517147	464716.545822	49.014273
3503.911989	464703.964049	49.019277
3503.579180	464693.381134	49.024282
3503.808113	464681.081002	49.029287
3503.672412	464679.178893	49.034292
3503.816604	464658.938725	49.039297
3503.500216	464654.534185	49.044301
3503.357264	464648.580063	49.049306
3503.513882	464622.916514	49.054311
3503.411473	464622.883346	49.059316
3503.431681	464604.792249	49.064321
3503.979246	464589.347045	49.069325
3503.873371	464557.293675	49.074330
3503.847894	464535.511707	49.079335
3503.965109	464518.873279	49.084340
3503.818221	464506.130546	49.089345
3503.768318	464489.317963	49.094349
3503.676172	464481.581803	49.099354
3504.190823	464444.406356	49.104359
3503.837544	464420.045588	49.109364
3503.526510	464396.741569	49.114369
3503.624437	464386.439604	49.119373
3503.494315	464380.989872	49.124378
3503.658153	464369.561985	49.129383
3503.814064	464352.815475	49.134388
3503.730882	464327.901810	49.139393
3503.799449	464309.447517	49.144397
3503.738835	464286.303274	49.149402
3504.010606	464265.331581	49.154407
3503.747713	464256.053820	49.159412
3503.910279	464236.418075	49.164417
3504.182290	464220.968963	49.169421
3503.957022	464199.474065	49.174426
3503.971048	464175.708944	49.179431
3504.017030	464162.375718	49.184436
3503.842365	464143.658797	49.189441
3503.987972	464112.119089	49.194445
3503.980269	464084.658875	49.199450
3504.300650	464063.273329	49.204455
3504.175253	464062.433409	49.209460
3504.106555	464035.844882	49.214465
3504.131892	464003.768195	49.219469
3504.023039	463990.613291	49.224474
3504.235047	463969.955489	49.229479
3504.031046	463937.816517	49.234484
3503.726360	463909.798754	49.239489
3503.738436	463894.545768	49.244493
3503.894885	463883.524199	49.249498
3503.873641	463868.732890	49.254503
3503.817457	463825.472276	49.259508
3503.485219	463806.832602	49.264513
3503.751063	463786.013410	49.269517
3504.029360	463781.963142	49.274522
3504.363272	463767.212452	49.279527
3504.212253	463757.459340	49.284532
3503.863100	463717.693928	49.289537
3503.960944	463700.652764	49.294541
3503.820761	463678.078732	49.299546
3503.796201	463666.023915	49.304551
3503.902416	463651.666693	49.309556
3503.465224	463623.671142	49.314561
3503.871591	463609.971996	49.319565
3503.554667	463589.708113	49.324570
3503.793379	463573.706823	49.329575
3503.767168	463566.769735	49.334580
3503.658179	463550.878462	49.339585
3504.007693	463546.815986	49.344589
3503.646896	463522.404708	49.349594
3504.003466	463493.918762	49.354599
3504.180012	463470.429044	49.359604
3503.840199	463456.401178	49.364609
3504.057409	463441.264818	49.369613
3503.744770	463423.989488	49.374618
3503.740970	463396.172955	49.379623
3503.644091	463382.204894	49.384628
3503.696037	463368.008736	49.389633
3503.822362	463348.682299	49.394637
3503.855792	463342.596322	49.399642
3503.964535	463334.217378	49.404647
3503.878737	463308.036130	49.409652
3503.718426	463273.456485	49.414657
3503.602026	463258.984976	49.419661
3503.680359	463246.658986	49.424666
3503.794129	463235.238985	49.429671
3503.168390	463231.038947	49.434676
3503.696578	463219.446838	49.439681
3503.658853	463200.857637	49.444685
3503.300916	463196.307850	49.449690
3503.495110	463182.695302	49.454695
3503.565830	463175.690856	49.459700
3503.729535	463174.598857	49.464705
3504.075256	463155.032091	49.469709
3504.104168	463125.385486	49.474714
3504.216766	463112.800214	49.479719
3503.983608	463096.068387	49.484724
3503.357624	463073.931292	49.489729
3503.733037	463051.876537	49.494733
3503.659849	463034.053279	49.499738
3503.620414	463008.573091	49.504743
3503.443065	462999.482803	49.509748
3503.346608	462983.892948	49.514753
3503.447071	462971.056306	49.519757
3503.732056	462974.199866	49.524762
3503.886424	462957.503094	49.529767
3503.473031	462951.645297	49.534772
3503.331242	462942.295561	49.539777
3503.762446	462924.639432	49.544781
3503.507514	462920.629363	49.549786
3503.686674	462909.198007	49.554791
3503.613109	462904.042224	49.559796
3503.573872	462889.050565	49.564801
3503.863954	462850.795687	49.569805
3503.695526	462840.285034	49.574810
3504.029279	462810.079199	49.579815
3503.616611	462812.277827	49.584820
3503.883280	462802.959624	49.589825
3503.879731	462785.225589	49.594829
3503.600722	462768.653322	49.599834
3504.157269	462735.673125	49.604839
3503.853288	462716.723561	49.609844
3504.038691	462704.986996	49.614849
3503.924277	462692.085519	49.619853
3503.448738	462688.518435	49.624858
3503.623702	462665.788082	49.629863
3503.244284	462644.419131	49.634868
3503.596719	462623.178552	49.639873
3503.932425	462607.666620	49.644877
3503.361337	462596.515195	49.649882
3503.407073	462596.304713	49.654887
3503.436830	462587.938936	49.659892
3503.476397	462569.285267	49.664897
3503.794825	462563.606426	49.669901
3503.358663	462559.880581	49.674906
3503.431061	462538.890410	49.679911
3503.374183	462540.166910	49.684916
3503.321137	462524.518605	49.689921
3503.626811	462516.257700	49.694925
3503.043677	462510.935464	49.699930
3503.823239	462494.131549	49.704935
3503.795117	462480.607145	49.709940
3504.061462	462476.355966	49.714945
3504.203139	462464.829409	49.719949
3504.278288	462431.170827	49.724954
3504.086883	462400.547316	49.729959
3504.132076	462395.928508	49.734964
3504.066450	462369.590546	49.739969
3504.168630	462334.863082	49.744973
3503.738406	462325.410285	49.749978
3503.500065	462316.532780	49.754983
3503.757310	462309.394833	49.759988
3503.301719	462300.453072	49.764993
3503.903328	462282.564584	49.769997
3503.508873	462264.035403	49.775002
3503.703959	462230.761374	49.780007
3503.694442	462231.877792	49.785012
3503.366262	462212.323808	49.790017
3503.646280	462198.797268	49.795021
3503.722600	462200.963143	49.800026
3503.322544	462180.458633	49.805031
3503.697952	462179.989170	49.810036
3503.667578	462168.897192	49.815041
3503.723580	462163.921780	49.820045
3503.193163	462163.404292	49.825050
3503.919717	462136.677398	49.830055
3503.650902	462130.490635	49.835060
3503.349340	462109.513183	49.840065
3503.837690	462086.677980	49.845069
3503.671164	462070.998018	49.850074
3503.793075	462058.359807	49.855079
3503.703511	462062.732931	49.860084
3503.606839	462047.142367	49.865089
3503.893158	462025.051001	49.870093
3503.681156	462024.327124	49.875098
3503.656217	462015.463719	49.880103
3504.047305	461996.141416	49.885108
3503.675101	461959.264696	49.890113
3504.072435	461938.978492	49.895117
3503.745107	461938.730357	49.900122
3503.809182	461922.504176	49.905127
3503.876610	461916.563969	49.910132
3503.529861	461888.854528	49.915137
3503.657452	461865.320574	49.920141
3503.533026	461852.876310	49.925146
3503.880015	461838.577996	49.930151
3503.667728	461835.016478	49.935156
3503.411009	461823.253531	49.940161
3503.661762	461812.873446	49.945165
3503.677228	461800.658628	49.950170
3503.498586	461798.104818	49.955175
3503.782789	461797.853612	49.960180
3503.432131	461785.549279	49.965185
3503.797747	461763.950812	49.970189
3503.339541	461750.144627	49.975194
3503.604513	461713.969423	49.980199
3503.783821	461706.236488	49.985204
3503.906396	461696.841019	49.990209
3504.245528	461683.658746	49.995213
3503.683290	461679.042139	50.000218
3503.699588	461669.816823	50.005223
3503.848377	461660.264840	50.010228
3503.427250	461634.087939	50.015233
3503.754195	461610.925031	50.020237
3503.462328	461596.836970	50.025242
3503.403178	461587.168436	50.030247
3503.570628	461570.265558	50.035252
3503.612597	461573.146798	50.040257
3503.777340	461563.288003	50.045261
3503.474134	461556.245479	50.050266
3503.622927	461548.973755	50.055271
3503.528506	461541.743555	50.060276
3503.623559	461532.200686	50.065281
3503.551700	461524.459891	50.070285
3503.323642	461521.255725	50.075290
3503.424964	461506.137663	50.080295
3503.664106	461503.867197	50.085300
3503.442983	461481.000411	50.090305
3503.732731	461467.116992	50.095309
3503.576137	461447.178232	50.100314
3503.674890	461420.912281	50.105319
3503.636195	461417.523743	50.110324
3503.402579	461410.317262	50.115329
3503.581860	461397.719506	50.120333
3503.543065	461404.617809	50.125338
3503.803920	461385.469168	50.130343
3503.792862	461379.440853	50.135348
3503.675205	461377.991405	50.140353
3503.817495	461366.514775	50.145357
3503.290676	461350.084970	50.150362
3503.638332	461328.235722	50.155367
3503.472140	461305.511376	50.160372
3503.371466	461290.427638	50.165377
3503.513927	461278.038790	50.170381
3503.526375	461275.300262	50.175386
3503.660190	461265.547948	50.180391
3504.184303	461258.820127	50.185396
3504.106985	461254.120621	50.190401
3504.205631	461239.458881	50.195405
3503.946184	461211.885603	50.200410
3503.704709	461178.988386	50.205415
3503.364799	461175.245840	50.210420
3503.340318	461167.648839	50.215425
3503.708435	461150.762014	50.220429
3503.365717	461147.678713	50.225434
3503.317350	461146.521466	50.230439
3503.636833	461131.720590	50.235444
3503.497549	461126.423538	50.240449
3503.586434	461115.107905	50.245453
3503.383637	461116.460086	50.250458
3503.601521	461098.990772	50.255463
3503.550463	461101.583916	50.260468
3503.424300	461098.311607	50.265473
3503.586369	461071.578307	50.270477
3503.315847	461075.171749	50.275482
3503.271771	461065.551061	50.280487
3503.438354	461052.904579	50.285492
3503.180093	461047.729169	50.290497
3503.547320	461036.112591	50.295501
3503.467108	461032.528376	50.300506
3503.345228	461029.305999	50.305511
3503.423710	461023.617012	50.310516
3503.210328	461020.410257	50.315521
3503.340943	461009.948914	50.320525
3503.208718	461007.032350	50.325530
3503.344958	461000.472018	50.330535
3503.311552	460998.552082	50.335540
3503.365566	460982.529546	50.340545
3503.483162	460972.830532	50.345549
3503.294429	460973.470870	50.350554
3503.646995	460959.221644	50.355559
3503.598220	460956.392174	50.360564
3503.500417	460948.402207	50.365569
3503.590262	460941.191001	50.370573
3503.528916	460939.427854	50.375578
3503.689791	460922.677571	50.380583
3503.434687	460923.835996	50.385588
3503.394011	460918.217999	50.390593
3503.553130	460910.994953	50.395597
3503.335354	460909.866617	50.400602
3503.443851	460887.145562	50.405607
3503.407109	460868.047234	50.410612
3503.206029	460871.375479	50.415617
3503.329426	460866.945662	50.420621
3503.416199	460876.812557	50.425626
3503.228128	460867.621761	50.430631
3503.079970	460857.461313	50.435636
3502.984167	460851.345956	50.440641
3503.512003	460836.357259	50.445645
3503.147546	460845.287705	50.450650
3503.296233	460819.215130	50.455655
3503.626008	460824.783816	50.460660
3503.185889	460823.136008	50.465665
3503.344931	460804.257566	50.470669
3503.493990	460793.640933	50.475674
3503.502760	460792.879313	50.480679
3503.452250	460792.026464	50.485684
3503.413812	460783.671565	50.490689
3503.214475	460780.107644	50.495693
3503.349746	460771.419026	50.500698
3503.203387	460759.839302	50.505703
3503.495087	460754.113832	50.510708
3503.317838	460752.066405	50.515713
3503.211105	460743.875177	50.520717
3503.504306	460736.527822	50.525722
3503.179543	460735.012338	50.530727
3503.379153	460730.518802	50.535732
3503.258198	460701.046160	50.540737
3503.754112	460658.900522	50.545741
3503.046815	460622.331895	50.550746
3503.049540	460557.820761	50.555751
3503.159389	460486.297788	50.560756
3503.100182	460407.404645	50.565761
3503.214232	460305.322306	50.570765
3503.245242	460207.763881	50.575770
3503.575462	460092.670203	50.580775
3503.218392	459970.750366	50.585780
3503.079150	459825.784764	50.590785
3503.219045	459667.543371	50.595789
3503.508686	459507.349355	50.600794
3503.588358	459328.539920	50.605799
3503.623080	459132.505426	50.610804
3503.543280	458932.788896	50.615809
3503.466074	458712.138732	50.620813
3503.181021	458490.913444	50.625818
3503.071754	458245.936503	50.630823
3503.023429	458004.088488	50.635828
3502.832993	457751.973112	50.640833
3502.853775	457481.268175	50.645837
3502.839663	457204.584761	50.650842
3503.228431	456913.484788	50.655847
3503.577659	456599.578588	50.660852
3503.022869	456280.296986	50.665857
3503.277141	455938.620242	50.670861
3503.349449	455580.038774	50.675866
3503.225791	455215.959265	50.680871
3503.299318	454838.203806	50.685876
3503.038947	454442.604238	50.690881
3503.410299	454030.768904	50.695885
3502.962400	453617.544365	50.700890
3503.094310	453176.178342	50.705895
3503.015879	452723.634989	50.710900
3502.622576	452266.927620	50.715905
3502.804665	451782.227951	50.720909
3502.573812	451308.893400	50.725914
3502.619148	450805.486214	50.730919
3502.860516	450293.414090	50.735924
3502.702045	449751.280072	50.740929
3502.866966	449202.688046	50.745933
3502.453043	448639.273038	50.750938
3502.262831	448053.696443	50.755943
3502.387008	447447.512956	50.760948
3502.239922	446841.713426	50.765953
3502.310137	446205.483318	50.770957
3502.475349	445559.683960	50.775962
3502.778103	444895.432222	50.780967
3502.990002	444207.338820	50.785972
3502.448241	443508.752111	50.790977
3502.959373	442775.930217	50.795981
3502.529247	442034.723157	50.800986
3502.501864	441271.763384	50.805991
3502.462674	440489.097800	50.810996
3502.310501	439688.009866	50.816001
3502.372732	438868.391075	50.821005
3501.908559	438045.737370	50.826010
3501.452811	437188.097238	50.831015
3501.199575	436328.309617	50.836020
3501.232359	435437.592624	50.841025
3501.430620	434544.935033	50.846029
3500.903758	433636.839689	50.851034
3501.096712	432700.575546	50.856039
3500.945995	431756.415838	50.861044
3500.629380	430773.982912	50.866049
3500.810200	429786.805421	50.871053
3500.291593	428784.835665	50.876058
3500.448010	427758.143434	50.881063
3500.474306	426721.024052	50.886068
3500.203045	425658.785282	50.891073
3500.265801	424573.295872	50.896077
3499.833479	423483.121299	50.901082
3499.454152	422362.023886	50.906087
3499.850470	421235.995953	50.911092
3499.383577	420072.697740	50.916097
3499.771912	418904.832593	50.921101
3499.453057	417714.363000	50.926106
3499.394105	416499.496168	50.931111
3499.431298	415260.561675	50.936116
3498.999864	414019.387420	50.941121
3499.095241	412743.301828	50.946125
3499.098310	411465.214088	50.951130
3498.825324	410159.202624	50.956135
3498.586962	408827.217052	50.961140
3498.302203	407481.204513	50.966145
3498.486093	406115.818103	50.971149
3498.106812	404749.925841	50.976154
3498.101180	403349.407325	50.981159
3497.651654	401943.203664	50.986164
3497.411126	400516.494590	50.991169
3497.440606	399068.682981	50.996173
3497.181924	397610.989542	51.001178
3497.121180	396143.000233	51.006183
3497.526997	394636.871357	51.011188
3496.888682	393115.064167	51.016193
3496.878416	391578.790836	51.021197
3496.081244	390034.263616	51.026202
3496.160550	388466.890117	51.031207
3496.212028	386878.931687	51.036212
3495.655775	385297.909535	51.041217
3495.473786	383675.084738	51.046221
3495.088821	382046.365960	51.051226
3494.849447	380408.211277	51.056231
3495.289538	378751.174067	51.061236
3494.843771	377081.265488	51.066241
3494.315163	375383.932169	51.071245
3493.994319	373685.258871	51.076250
3493.925277	371962.965399	51.081255
3494.121961	370229.939083	51.086260
3493.737027	368485.586897	51.091265
3493.918378	366713.386238	51.096269
3493.504934	364935.454698	51.101274
3493.181133	363129.244303	51.106279
3493.208671	361311.672219	51.111284
3492.499302	359479.515851	51.116289
3492.573989	357630.403736	51.121293
3492.240895	355776.570528	51.126298
3491.748000	353897.547612	51.131303
3491.259638	352005.796052	51.136308
3491.070095	350126.680974	51.141313
3490.866433	348202.633108	51.146317
3490.539948	346259.466154	51.151322
3490.060543	344315.987797	51.156327
3489.998276	342369.914178	51.161332
3489.323605	340399.462506	51.166337
3489.314112	338428.690183	51.171341
3488.979383	336442.880964	51.176346
3488.593874	334439.265059	51.181351
3488.626908	332423.055879	51.186356
3487.934463	330407.760315	51.191361
3487.717298	328364.160069	51.196365
3487.275150	326317.368557	51.201370
3487.361752	324251.757434	51.206375
3487.243820	322173.535804	51.211380
3486.893448	320087.087708	51.216385
3486.542451	317979.061279	51.221389
3486.302474	315867.206783	51.226394
3486.230047	313740.696888	51.231399
3485.528328	311582.178553	51.236404
3484.750355	309437.282114	51.241409
3484.617835	307267.264885	51.246413
3484.179011	305098.361703	51.251418
3483.520646	302904.666034	51.256423
3483.189726	300717.072514	51.261428
3482.485819	298524.805743	51.266433
3482.727266	296312.364908	51.271437
3482.137316	294092.557445	51.276442
3481.630850	291866.528009	51.281447
3481.097372	289621.336237	51.286452
3480.470210	287374.362471	51.291457
3480.591080	285127.757560	51.296461
3480.193819	282862.488220	51.301466
3479.767028	280580.892303	51.306471
3479.396075	278292.150921	51.311476
3478.586337	276000.145779	51.316481
3478.526550	273693.140040	51.321485
3477.708412	271381.911884	51.326490
3477.120553	269061.583862	51.331495
3476.824744	266725.450222	51.336500
3476.068168	264391.622725	51.341505
3475.903037	262055.849934	51.346509
3475.318950	259698.569673	51.351514
3474.450782	257339.550719	51.356519
3474.619055	254976.304103	51.361524
3473.737334	252615.021553	51.366529
3473.464147	250230.107798	51.371533
3472.454114	247841.508306	51.376538
3472.388770	245463.506885	51.381543
3471.977071	243055.960921	51.386548
3471.397514	240659.413558	51.391553
3470.901635	238244.894237	51.396557
3470.198345	235827.813164	51.401562
3469.670272	233404.976156	51.406567
3469.117923	230974.205423	51.411572
3468.512102	228543.480589	51.416577
3468.059491	226099.502437	51.421581
3467.660151	223664.013802	51.426586
3467.040888	221207.704027	51.431591
3466.894904	218741.816472	51.436596
3465.865211	216279.013195	51.441601
3465.434556	213811.405672	51.446605
3464.607695	211332.064038	51.451610
3463.843217	208868.641831	51.456615
3463.509020	206379.756334	51.461620
3462.702966	203895.469937	51.466625
3461.784083	201412.020412	51.471629
3461.327994	198931.235199	51.476634
3460.965012	196446.905750	51.481639
3460.340839	193943.581260	51.486644
3459.429400	191455.229186	51.491649
3458.716256	188942.442202	51.496653
3457.876186	186449.901707	51.501658
3457.476877	183946.002643	51.506663
3456.695692	181448.909911	51.511668
3455.751238	178939.616500	51.516673
3455.437229	176437.536720	51.521677
3454.720057	173929.464769	51.526682
3453.988738	171429.156003	51.531687
3453.737405	168914.175840	51.536692
3452.590779	166409.037959	51.541697
3451.981282	163893.426660	51.546701
3450.875552	161382.597328	51.551706
3450.115642	158872.924166	51.556711
3449.469523	156360.355130	51.561716
3448.608633	153863.035353	51.566721
3447.735963	151351.936655	51.571725
3447.056495	148867.493104	51.576730
3446.607203	146301.757494	51.581735
3445.802107	143783.748394	51.586740
3444.783227	141278.537271	51.591745
3443.862329	138787.521324	51.596749
3443.003568	136284.686814	51.601754
3442.306021	133795.241239	51.606759
3441.703608	131320.696478	51.611764
3440.303746	128836.639394	51.616769
3439.550296	126353.999528	51.621773
3438.193565	123873.603681	51.626778
3437.179825	121404.441618	51.631783
3436.673976	118962.392385	51.636788
3435.413783	116504.031700	51.641793
3434.580838	114060.782107	51.646797
3433.411500	111636.596937	51.651802
3432.506347	109205.565265	51.656807
3431.625607	106779.378564	51.661812
3430.028849	104385.974304	51.666817
3429.330286	101970.157388	51.671821
3428.620923	99577.924239	51.676826
3427.681504	97195.135785	51.681831
3426.468380	94812.857787	51.686836
3425.039881	92449.144487	51.691841
3423.881688	90102.902061	51.696845
3422.425572	87755.698798	51.701850
3421.357636	85434.720333	51.706855
3420.227496	83116.973672	51.711860
3418.599944	80834.846545	51.716865
3417.561334	78547.282055	51.721869
3416.264029	76279.637961	51.726874
3414.779616	74037.701120	51.731879
3413.587415	71807.740139	51.736884
3412.357678	69605.983367	51.741889
3410.696939	67407.826466	51.746893
3409.007880	65230.132457	51.751898
3407.378949	63090.647644	51.756903
3406.219034	60951.092210	51.761908
3403.737516	58856.529703	51.766913
3402.126095	56782.764004	51.771917
3400.425809	54739.603434	51.776922
3398.403444	52734.162851	51.781927
3396.025556	50745.669417	51.786932
3393.611327	48830.616356	51.791937
3390.201657	46964.272517	51.796941
3385.304269	45190.069339	51.801946
3380.054456	43491.994604	51.806951
3374.965182	41866.506985	51.811956
3370.039469	40347.175189	51.816961
3365.399913	38898.625115	51.821965
3361.145383	37546.218560	51.826970
3356.843206	36269.138464	51.831975
3353.400275	35090.624884	51.836980
3349.810348	33996.313682	51.841985
3346.209138	32972.741878	51.846989
3343.329476	32021.664545	51.851994
3340.217129	31147.248128	51.856999
3337.395556	30335.393448	51.862004
3334.712437	29596.671296	51.867009
3332.021047	28914.268967	51.872013
3329.598201	28288.262449	51.877018
3327.114234	27725.240225	51.882023
3325.420220	27203.283199	51.887028
3323.274074	26730.010604	51.892033
3321.723344	26297.316705	51.897037
3319.824281	25902.497423	51.902042
3318.308171	25558.313275	51.907047
3316.863617	25232.944545	51.912052
3315.124040	24947.860331	51.917057
3313.765055	24692.177970	51.922061
3312.517431	24463.159156	51.927066
3311.779522	24256.405383	51.932071
3310.529757	24062.618898	51.937076
3309.479017	23911.072286	51.942081
3308.715000	23764.120382	51.947085
3307.995673	23628.720458	51.952090
3307.372488	23520.520120	51.957095
3306.701875	23404.599889	51.962100
3306.006968	23312.449157	51.967105
3305.580758	23216.967419	51.972109
3305.138643	23129.603267	51.977114
3304.546004	23051.132186	51.982119
3304.056735	22976.511206	51.987124
3303.477185	22919.962208	51.992129
3303.270444	22838.662400	51.997133
3302.969748	22773.170984	52.002138
3302.136123	22724.558854	52.007143
3302.065171	22652.128781	52.012148
3301.364318	22594.453709	52.017153
3301.511898	22538.916968	52.022157
3300.977605	22478.061177	52.027162
3300.472022	22422.955762	52.032167
3300.043040	22348.330371	52.037172
3299.547079	22296.262507	52.042177
3299.265522	22217.438530	52.047181
3298.886220	22153.648295	52.052186
3297.949144	22094.823154	52.057191
3297.646340	22029.606871	52.062196
3297.278166	21968.528463	52.067201
3297.110331	21907.220005	52.072205
3296.384755	21837.463273	52.077210
3296.527459	21771.697564	52.082215
3295.991366	21684.565506	52.087220
3295.647768	21627.025544	52.092225
3295.369817	21534.594946	52.097229
3295.165610	21455.018201	52.102234
3294.278418	21358.800272	52.107239
3293.756968	21262.866637	52.112244
3293.195138	21181.478823	52.117249
3292.746987	21097.441295	52.122253
3292.261995	21005.630709	52.127258
3291.565141	20922.064961	52.132263
3291.308469	20830.020283	52.137268
3290.502039	20732.460959	52.142273
3290.209239	20635.149603	52.147277
3289.306248	20550.190180	52.152282
3288.582449	20452.352755	52.157287
3288.503781	20352.818494	52.162292
3287.803099	20259.094819	52.167297
3287.537874	20155.233564	52.172301
3286.847061	20058.957810	52.177306
3285.883682	19963.119629	52.182311
3285.719898	19851.014662	52.187316
3284.851653	19771.495974	52.192321
3284.247507	19662.303463	52.197325
3283.858941	19558.466924	52.202330
3283.057584	19458.819487	52.207335
3282.531361	19341.473095	52.212340
3281.861589	19257.700659	52.217345
3281.458933	19147.827345	52.222349
3280.779131	19042.407633	52.227354
3280.152102	18945.082432	52.232359
3279.497562	18838.570545	52.237364
3278.857557	18733.519011	52.242369
3278.244209	18629.498942	52.247373
3277.843838	18526.940055	52.252378
3276.960760	18420.062026	52.257383
3276.780679	18309.839995	52.262388
3275.855355	18202.412581	52.267393
3275.434783	18093.293676	52.272397
3274.844825	17985.160707	52.277402
3273.723880	17883.588698	52.282407
3273.385547	17760.096210	52.287412
3272.699481	17655.087713	52.292417
3271.764725	17550.244063	52.297421
3271.371521	17437.503557	52.302426
3270.368085	17331.403784	52.307431
3270.614974	17225.154313	52.312436
3269.823910	17120.443694	52.317441
3268.822001	17006.175759	52.322445
3268.290768	16907.907111	52.327450
3267.334846	16793.757631	52.332455
3267.134686	16677.131160	52.337460
3266.354053	16580.444890	52.342465
3265.589553	16471.711370	52.347469
3264.875275	16356.998859	52.352474
3263.795042	16257.753074	52.357479
3263.296698	16148.807074	52.362484
3262.704250	16052.338264	52.367489
3262.394682	15946.604453	52.372493
3261.779601	15844.000635	52.377498
3260.606329	15748.800752	52.382503
3260.460040	15634.043590	52.387508
3259.587183	15534.968972	52.392513
3258.934582	15427.275696	52.397517
3258.207644	15326.244553	52.402522
3257.595930	15223.454331	52.407527
3256.903271	15122.339550	52.412532
3256.083212	15020.573910	52.417537
3255.465713	14912.865323	52.422541
3254.686385	14812.002709	52.427546
3253.900563	14717.396807	52.432551
3253.596582	14612.356376	52.437556
3253.054718	14521.466363	52.442561
3252.259260	14414.736440	52.447565
3251.799879	14311.044023	52.452570
3251.066098	14209.668432	52.457575
3250.569546	14099.046206	52.462580
3249.870331	14010.843908	52.467585
3249.430460	13914.119651	52.472589
3248.935418	13795.673722	52.477594
3248.028657	13696.543179	52.482599
3247.368826	13583.572442	52.487604
3246.788153	13483.045854	52.492609
3246.319053	13378.126785	52.497613
3245.662341	13267.938850	52.502618
3244.859848	13161.488428	52.507623
3244.133597	13047.445532	52.512628
3243.470624	12948.388447	52.517633
3242.884375	12842.963435	52.522637
3242.106872	12742.685144	52.527642
3241.537745	12638.712255	52.532647
3241.139418	12529.287828	52.537652
3240.113130	12420.917899	52.542657
3239.830478	12312.293656	52.547661
3239.282801	12205.502501	52.552666
3238.270107	12103.613919	52.557671
3237.681985	11991.273884	52.562676
3236.911001	11888.002280	52.567681
3235.875167	11781.417362	52.572685
3235.535001	11679.419684	52.577690
3234.418656	11581.051870	52.582695
3234.050809	11474.051467	52.587700
3233.400554	11382.519438	52.592705
3232.707199	11283.591343	52.597709
3232.178217	11175.898350	52.602714
3231.594826	11066.204030	52.607719
3230.979693	10963.202351	52.612724
3229.781266	10872.204480	52.617729
3229.327865	10767.702289	52.622733
3228.819400	10664.799605	52.627738
3227.675585	10574.212755	52.632743
3227.534895	10469.941856	52.637748
3226.740583	10382.851214	52.642753
3226.293244	10277.327334	52.647757
3225.462205	10172.539566	52.652762
3224.876549	10081.637335	52.657767
3224.061816	9977.257232	52.662772
3223.731727	9885.786331	52.667777
3223.237824	9783.017855	52.672781
3222.466493	9676.134498	52.677786
3221.590041	9577.263830	52.682791
3220.771456	9467.334495	52.687796
3220.336291	9378.925582	52.692801
3219.623139	9277.474260	52.697805
3219.252415	9169.020234	52.702810
3218.044820	9074.759048	52.707815
3217.570933	8971.354048	52.712820
3216.732093	8883.342235	52.717825
3216.074900	8791.993407	52.722829
3215.421522	8689.327029	52.727834
3214.546788	8592.473110	52.732839
3213.982535	8507.992987	52.737844
3213.409217	8404.652825	52.742849
3212.312362	8320.002438	52.747853
3212.169544	8223.545418	52.752858
3211.519724	8128.550724	52.757863
3210.870770	8032.573869	52.762868
3210.126745	7939.822173	52.767873
3209.819213	7842.580448	52.772877
3209.302173	7743.638254	52.777882
3208.001792	7652.175910	52.782887
3207.559461	7556.747112	52.787892
3206.639883	7476.069757	52.792897
3206.092333	7376.755124	52.797901
3205.278247	7284.571251	52.802906
3204.814980	7197.731045	52.807911
3204.346844	7094.148315	52.812916
3203.612998	7006.879904	52.817921
3202.657838	6911.367209	52.822925
3202.375285	6815.417939	52.827930
3201.399916	6730.650115	52.832935
3201.063942	6629.914717	52.837940
3200.209287	6545.778815	52.842945
3199.447128	6441.457590	52.847949
3199.300079	6356.648952	52.852954
3198.226697	6267.536073	52.857959
3197.690893	6164.158076	52.862964
3197.019294	6073.888559	52.867969
3196.595920	5973.904312	52.872973
3195.691548	5879.729289	52.877978
3194.652371	5791.628038	52.882983
3194.337404	5688.098505	52.887988
3193.378389	5607.630774	52.892993
3192.633286	5511.739110	52.897997
3192.278645	5425.301391	52.903002
3191.340624	5339.770107	52.908007
3191.241259	5242.376680	52.913012
3190.341102	5161.413893	52.918017
3189.196217	5069.574101	52.923021
3188.599817	4977.870937	52.928026
3187.919963	4899.838739	52.933031
3187.485175	4811.318241	52.938036
3186.872074	4734.172538	52.943041
3186.319968	4643.815672	52.948045
3186.021021	4547.003889	52.953050
3185.049712	4459.159002	52.958055
3184.503149	4366.280550	52.963060
3183.319942	4283.019749	52.968065
3182.624358	4197.889867	52.973069
3182.473156	4105.712151	52.978074
3181.219946	4017.068203	52.983079
3180.811729	3925.147862	52.988084
3179.999962	3856.686987	52.993089
3179.609931	3767.851953	52.998093
3179.028971	3685.073364	53.003098
3178.000077	3603.706999	53.008103
3177.271849	3512.988682	53.013108
3176.912330	3422.260797	53.018113
3176.095263	3351.102510	53.023117
3175.635518	3262.309856	53.028122
3174.761939	3187.157044	53.033127
3173.978715	3102.216996	53.038132
3173.208085	3022.970646	53.043137
3172.741865	2940.743280	53.048141
3172.095024	2860.697262	53.053146
3171.441130	2789.711024	53.058151
3171.038205	2691.438375	53.063156
3170.469569	2617.734017	53.068161
3169.435765	2538.670078	53.073165
3168.917386	2449.119803	53.078170
3167.917617	2381.400950	53.083175
3167.394713	2293.175652	53.088180
3166.908618	2226.094526	53.093185
3165.788657	2144.958105	53.098189
3164.934507	2065.861900	53.103194
3163.989907	2001.928270	53.108199
3163.483725	1932.706619	53.113204
3162.715217	1862.048908	53.118209
3161.925162	1805.792457	53.123213
3161.762761	1737.137459	53.128218
3160.967542	1675.676151	53.133223
3159.783469	1606.838614	53.138228
3159.528269	1538.331400	53.143233
3158.994388	1472.642930	53.148237
3157.902257	1408.728238	53.153242
3157.154761	1339.673988	53.158247
3156.620487	1279.642098	53.163252
3156.479511	1215.523845	53.168257
3155.107196	1152.498106	53.173261
3154.691310	1103.418061	53.178266
3153.940957	1042.461591	53.183271
3152.996089	975.438923	53.188276
3152.333439	922.063706	53.193281
3151.512423	860.647110	53.198285
3151.068252	801.805634	53.203290
3150.386183	752.935589	53.208295
3149.737564	708.298333	53.213300
3149.186665	659.641437	53.218305
3148.448662	606.403331	53.223309
3148.000306	539.739021	53.228314
3146.957002	489.929671	53.233319
3146.284139	434.467731	53.238324
3145.687407	384.067686	53.243329
3144.660414	336.447606	53.248333
3143.926044	289.301091	53.253338
3143.157340	247.418400	53.258343
3142.779009	194.271037	53.263348
3141.858750	155.873897	53.268353
3140.070126	136.256767	53.273357
3138.142684	147.772293	53.278362
3136.576567	147.560286	53.283367
3135.965296	150.192971	53.288372
3135.816914	152.067242	53.293377
3134.925858	152.892900	53.298381
3134.741568	146.122437	53.303386
3134.362955	146.706599	53.308391
3133.449479	147.622928	53.313396
3132.996627	153.650449	53.318401
3132.698443	156.036226	53.323405
3131.877608	152.640501	53.328410
3130.697604	152.540944	53.333415
3130.365252	154.240599	53.338420
3129.892923	158.345174	53.343425
3128.965980	158.029489	53.348429
3128.519422	153.395500	53.353434
3127.751509	157.493341	53.358439
3127.100887	157.391756	53.363444
3126.933519	152.689936	53.368449
3125.436537	162.882613	53.373453
3125.335833	148.736968	53.378458
3124.170614	163.601810	53.383463
3124.399645	158.326219	53.388468
3124.000770	159.172785	53.393473
3122.533872	156.889662	53.398477
3122.529349	143.480337	53.403482
3121.501639	163.605123	53.408487
3120.828448	157.652384	53.413492
3120.035258	157.897651	53.418497
3119.676468	163.190303	53.423501
3119.246152	154.832038	53.428506
3118.092962	160.159762	53.433511
3117.754712	147.530597	53.438516
3116.743701	145.161691	53.443521
3116.168926	160.034593	53.448525
3116.322364	165.667614	53.453530
3114.937939	151.570779	53.458535
3114.761832	157.193787	53.463540
3113.917028	157.482215	53.468545
3113.288347	158.579621	53.473549
3112.307023	145.637578	53.478554
3111.747801	147.553624	53.483559
3111.009234	154.038899	53.488564
3110.661783	160.258410	53.493569
3109.833956	153.747896	53.498573
3109.233599	144.693180	53.503578
3108.275858	154.695434	53.508583
3107.914462	151.912385	53.513588
3107.122755	153.736314	53.518593
3106.592769	163.669830	53.523597
3106.387485	153.724993	53.528602
3105.557636	152.097619	53.533607
3104.368609	154.339953	53.538612
3103.914378	156.204905	53.543617
3103.644044	157.347661	53.548621
3103.167410	162.695578	53.553626
3101.678599	162.244192	53.558631
3101.510973	149.985341	53.563636
3101.347296	158.131698	53.568641
3099.939118	156.401036	53.573645
3099.400545	151.029236	53.578650
3099.069242	153.499618	53.583655
3098.222999	151.834784	53.588660
3097.393622	154.267111	53.593665
3096.657947	150.588428	53.598669
3096.768335	142.746855	53.603674
3095.848302	153.697513	53.608679
3095.170122	147.781160	53.613684
3094.667258	146.151207	53.618689
3093.027527	151.952843	53.623693
3092.837651	140.349894	53.628698
3092.266040	147.764252	53.633703
3091.924902	149.352518	53.638708
3090.925849	145.028458	53.643713
3089.976872	152.147698	53.648717
3090.031646	146.630708	53.653722
3089.453794	153.902059	53.658727
3088.638075	150.520074	53.663732
3087.636648	149.327799	53.668737
3086.679955	150.732694	53.673741
3086.533843	141.243142	53.678746
3085.931206	152.527982	53.683751
3085.133521	142.367407	53.688756
3084.553867	143.919848	53.693761
3083.578439	150.278625	53.698765
3083.773914	141.698188	53.703770
3082.831484	145.300465	53.708775
3082.076127	143.020908	53.713780
3081.841828	141.080996	53.718785
3080.702809	148.069684	53.723789
3079.757972	143.289137	53.728794
3078.760387	145.629024	53.733799
3078.039895	143.155620	53.738804
3077.817390	148.275379	53.743809
3077.588026	140.658040	53.748813
3077.410310	147.952597	53.753818
3075.892904	154.147407	53.758823
3075.285685	150.761377	53.763828
3074.733883	145.664601	53.768833
3073.313490	154.258177	53.773837
3073.493631	148.698450	53.778842
3073.064482	157.621596	53.783847
3072.233323	153.956073	53.788852
3071.632898	148.923261	53.793857
3070.845930	159.585142	53.798861
3070.044527	143.423755	53.803866
3069.146418	148.217645	53.808871
3068.206787	139.214990	53.813876
3068.720901	146.051082	53.818881
3067.746888	148.428390	53.823885
3067.293056	144.603663	53.828890
3066.529763	156.066347	53.833895
3065.607717	144.218246	53.838900
3065.076840	144.918426	53.843905
3063.797429	146.524514	53.848909
3063.303769	141.983057	53.853914
3062.552095	142.867803	53.858919
3061.868077	146.132646	53.863924
3061.962507	147.948061	53.868929
3061.099589	146.869490	53.873933
3060.751971	138.489614	53.878938
3059.745765	146.382036	53.883943
3059.585721	148.748552	53.888948
3058.476720	145.301820	53.893953
3057.440624	140.845943	53.898957
3056.483723	132.363340	53.903962
3055.921773	144.676592	53.908967
3055.129918	142.316435	53.913972
3055.061554	133.301097	53.918977
3054.504937	144.868586	53.923981
3054.278139	143.502513	53.928986
3053.532506	145.220683	53.933991
3052.483140	148.370325	53.938996
3051.389176	133.436813	53.944001
3050.809920	142.679276	53.949005
3050.636420	138.410346	53.954010
3049.879640	144.498085	53.959015
3048.903922	143.574972	53.964020
3048.568363	143.011412	53.969025
3047.462280	142.403068	53.974029
3047.107862	139.965406	53.979034
3046.159013	146.881735	53.984039
3046.266634	140.912439	53.989044
3045.067623	147.094295	53.994049
3044.114203	142.874946	53.999053
3044.341741	121.809332	54.004058
3043.425812	136.028016	54.009063
3042.522494	139.124678	54.014068
3041.909273	140.753909	54.019073
3040.969869	141.864940	54.024077
3040.694085	143.089153	54.029082
3039.713117	133.578452	54.034087
3039.656989	146.418287	54.039092
3038.640483	137.834162	54.044097
3037.326309	143.353210	54.049101
3037.178811	138.627086	54.054106
3036.369617	142.785273	54.059111
3036.271597	141.420486	54.064116
3035.341629	138.534865	54.069121
3034.339063	136.873860	54.074125
3034.537167	137.426981	54.079130
3033.944496	148.017761	54.084135
3032.601331	140.514166	54.089140
3031.918399	140.011543	54.094145
3030.713477	144.696418	54.099149
3031.226510	137.877078	54.104154
3030.666173	136.293269	54.109159
3029.173594	137.980392	54.114164
3028.655316	137.326085	54.119169
3028.025589	140.418235	54.124173
3027.944978	147.531201	54.129178
3026.915201	134.883651	54.134183
3025.444537	140.699829	54.139188
3025.431816	132.881274	54.144193
3024.463782	130.594649	54.149197
3024.272402	130.329342	54.154202
3023.603244	138.636661	54.159207
3022.678294	131.169373	54.164212
3022.380075	128.647113	54.169217
3021.697573	138.131421	54.174221
3021.279103	133.482784	54.179226
3020.104450	137.345795	54.184231
3019.540558	142.499017	54.189236
3019.095197	139.848744	54.194241
3018.074642	145.213022	54.199245
3017.520237	133.231468	54.204250
3016.553994	139.688148	54.209255
3015.766672	137.699847	54.214260
3015.362309	136.936473	54.219265
3014.638400	143.573978	54.224269
3014.370982	140.970667	54.229274
3013.437595	138.863249	54.234279
3012.972914	140.267368	54.239284
3012.941993	139.186373	54.244289
3011.886340	139.324532	54.249293
3011.159969	132.613954	54.254298
3010.436219	132.195675	54.259303
3009.641856	126.422748	54.264308
3009.192295	136.031852	54.269313
3008.373138	135.430144	54.274317
3008.016738	127.146912	54.279322
3006.917073	135.555817	54.284327
3006.492177	131.411954	54.289332
3006.221434	132.235842	54.294337
3005.439079	134.834217	54.299341
3004.275341	130.280959	54.304346
3003.667248	133.436517	54.309351
3003.175741	134.492334	54.314356
3002.583495	124.552471	54.319361
3001.505534	134.802229	54.324365
3001.126063	130.559422	54.329370
3000.361172	133.917822	54.334375
2999.551814	130.573058	54.339380
2999.059930	121.143009	54.344385
2998.455767	134.488966	54.349389
2997.575043	129.061184	54.354394
2997.043618	131.194718	54.359399
2996.135454	129.093258	54.364404
2995.592787	132.308687	54.369409
2994.550904	131.587149	54.374413
2994.888113	126.294665	54.379418
2993.878000	133.937103	54.384423
2993.318244	136.192318	54.389428
2993.394672	124.204426	54.394433
2992.031978	131.080946	54.399437
2991.497651	125.749104	54.404442
2990.969824	130.594984	54.409447
2989.708869	128.897617	54.414452
2988.806929	129.300428	54.419457
2988.488503	134.517886	54.424461
2988.239658	121.412843	54.429466
2987.577615	127.913064	54.434471
2985.954119	126.578036	54.439476
2986.120620	134.239674	54.444481
2985.260654	132.611941	54.449485
2984.586152	131.305403	54.454490
2983.649545	137.220587	54.459495
2983.888953	133.887267	54.464500
2983.267588	129.572116	54.469505
2981.918915	135.986387	54.474509
2981.467400	128.625311	54.479514
2980.238229	127.213428	54.484519
2979.758997	137.596531	54.489524
2979.320992	126.215611	54.494529
2978.622458	127.979027	54.499533
2977.735720	133.102155	54.504538
2977.185753	128.570731	54.509543
2976.482015	124.718463	54.514548
2976.431741	124.479966	54.519553
2975.446287	138.043049	54.524557
2974.981615	130.128050	54.529562
2974.305226	130.757184	54.534567
2973.499131	132.074387	54.539572
2973.045600	127.960684	54.544577
2972.321735	140.789086	54.549581
2971.865089	137.003142	54.554586
2971.242292	135.077127	54.559591
2970.188093	128.629810	54.564596
2969.140292	129.101759	54.569601
2968.592453	140.917210	54.574605
2967.994146	130.715892	54.579610
2967.617697	124.269602	54.584615
2966.630598	128.672529	54.589620
2966.518624	133.201829	54.594625
2965.694948	132.716554	54.599629
2965.271901	124.767211	54.604634
2964.508112	131.386266	54.609639
2963.541356	125.499522	54.614644
2963.422467	129.927768	54.619649
2962.613312	140.506984	54.624653
2961.520173	136.154034	54.629658
2960.544994	127.749973	54.634663
2959.579316	134.910360	54.639668
2959.762386	131.433908	54.644673
2959.554500	134.297664	54.649677
2958.973645	125.856616	54.654682
2957.644578	130.488109	54.659687
2956.839503	134.106795	54.664692
2956.273080	127.252058	54.669697
2955.485241	137.970521	54.674701
2955.394714	138.336914	54.679706
2954.775799	137.771652	54.684711
2953.187209	139.299941	54.689716
2953.097401	124.743153	54.694721
2952.418921	132.399185	54.699725
2951.468829	128.700331	54.704730
2950.482796	132.585987	54.709735
2950.225057	132.868852	54.714740
2950.308897	130.951162	54.719745
2948.725892	135.792232	54.724749
2947.961838	129.888614	54.729754
2947.851100	136.305288	54.734759
2947.049686	133.622712	54.739764
2946.333625	128.584820	54.744769
2945.409469	128.768019	54.749773
2945.354439	126.306443	54.754778
2944.431469	127.466784	54.759783
2943.541358	124.909891	54.764788
2943.478679	126.225976	54.769793
2942.439800	132.438106	54.774797
2942.240847	129.770997	54.779802
2941.432497	133.563529	54.784807
2941.116633	134.851040	54.789812
2940.186422	127.969659	54.794817
2938.567744	130.505304	54.799821
2938.275989	124.242303	54.804826
2937.479303	126.826949	54.809831
2936.967013	137.810948	54.814836
2936.617012	129.144931	54.819841
2935.948440	135.219573	54.824845
2935.194236	126.674735	54.829850
2934.799472	121.871276	54.834855
2934.079964	138.237263	54.839860
2933.442781	128.992706	54.844865
2932.881150	123.931585	54.849869
2932.315520	132.418574	54.854874
2931.243521	129.168835	54.859879
2930.032849	131.616208	54.864884
2929.546798	125.332332	54.869889
2929.573153	130.261928	54.874893
2928.811929	121.485010	54.879898
2928.428208	139.519362	54.884903
2927.499798	130.162734	54.889908
2927.197323	133.007129	54.894913
2926.342811	131.967802	54.899917
2924.886205	129.009969	54.904922
2924.149303	138.583704	54.909927
2923.970814	133.745652	54.914932
2923.862441	124.554806	54.919937
2922.214061	132.260140	54.924941
2921.614882	135.150503	54.929946
2921.321291	126.501296	54.934951
2920.621716	129.502365	54.939956
2919.979371	121.798922	54.944961
2919.442181	133.959907	54.949965
2919.358178	124.953971	54.954970
2918.343284	126.754088	54.959975
2917.430863	131.002553	54.964980
2917.078850	125.113001	54.969985
2915.609936	135.537336	54.974989
2915.549081	132.637819	54.979994
2915.056394	130.443267	54.984999
2913.608226	130.938646	54.990004
2913.090674	127.855866	54.995009
2912.262939	131.581846	55.000013
2912.493955	125.861073	55.005018
2912.091356	127.953651	55.010023
2910.851184	133.124553	55.015028
2910.810535	127.115082	55.020033
2909.810483	134.323582	55.025037
2908.414368	127.615378	55.030042
2907.827485	133.745533	55.035047
2907.701590	130.775028	55.040052
2906.779268	129.106255	55.045057
2905.949336	129.203097	55.050061
2905.205198	127.225987	55.055066
2905.196529	132.813656	55.060071
2904.307521	126.415493	55.065076
2904.204081	124.412970	55.070081
2903.675324	131.184490	55.075085
2902.591676	132.641500	55.080090
2901.686848	131.027369	55.085095
2900.768536	139.923177	55.090100
2900.263516	132.223895	55.095105
2899.460693	136.528238	55.100109
2899.026223	131.784459	55.105114
2897.951394	125.613049	55.110119
2897.386821	131.998332	55.115124
2897.282193	129.198268	55.120129
2896.445315	133.533297	55.125133
2895.476444	131.848403	55.130138
2894.584066	136.644486	55.135143
2894.561131	128.698615	55.140148
2893.810720	124.249615	55.145153
2892.473711	125.307830	55.150157
2891.845653	118.066942	55.155162
2891.518446	125.433999	55.160167
2890.979895	127.243108	55.165172
2890.612680	127.211141	55.170177
2889.317061	130.842218	55.175181
2889.281629	131.906943	55.180186
2889.105443	132.739938	55.185191
2888.245775	137.161757	55.190196
2887.504715	124.927538	55.195201
2886.310931	125.787993	55.200205
2885.452555	116.065347	55.205210
2884.903125	130.153500	55.210215
2884.450226	127.996756	55.215220
2883.981453	119.952614	55.220225
2883.145748	125.524515	55.225229
2882.757627	125.949267	55.230234
2881.704355	130.045364	55.235239
2880.737804	129.999772	55.240244
2880.273269	121.080980	55.245249
2879.339221	123.868313	55.250253
2879.541207	121.396369	55.255258
2878.818381	122.751061	55.260263
2878.021291	125.661433	55.265268
2878.026629	119.464902	55.270273
2876.456726	132.183283	55.275277
2875.353706	119.774094	55.280282
2875.414882	120.745335	55.285287
2874.368055	125.387422	55.290292
2873.657790	120.268820	55.295297
2872.845392	135.665438	55.300301
2872.744567	127.937350	55.305306
2872.123066	130.707981	55.310311
2871.183008	131.920988	55.315316
2870.993171	123.524052	55.320321
2870.394030	125.617063	55.325325
2869.310635	126.316554	55.330330
2868.253242	123.587743	55.335335
2867.179225	129.947197	55.340340
2866.978415	117.844077	55.345345
2866.442583	124.909691	55.350349
2866.205883	124.232542	55.355354
2865.955285	117.116619	55.360359
2865.108970	127.654812	55.365364
2864.829629	123.089392	55.370369
2863.632239	123.602319	55.375373
2862.555910	118.535227	55.380378
2861.824988	122.489790	55.385383
2860.925656	118.367031	55.390388
2860.618776	112.908318	55.395393
2860.074474	127.789386	55.400397
2859.558797	124.683398	55.405402
2859.082340	126.258482	55.410407
2857.712286	123.401533	55.415412
2857.074236	119.592137	55.420417
2856.206303	126.660826	55.425421
2855.939618	124.741860	55.430426
2855.419206	119.388715	55.435431
2854.824211	126.172344	55.440436
2854.462156	113.869028	55.445441
2853.851598	127.968019	55.450445
2853.797666	126.484391	55.455450
2852.702143	134.962471	55.460455
2851.566288	128.905709	55.465460
2851.070794	119.006186	55.470465
2849.678666	126.740762	55.475469
2848.883344	122.270237	55.480474
2849.379264	127.163786	55.485479
2848.394946	126.459674	55.490484
2847.833995	123.179852	55.495489
2847.067531	122.175226	55.500493
2846.231939	128.465120	55.505498
2845.523080	118.931266	55.510503
2844.086560	125.332148	55.515508
2844.077485	112.340896	55.520513
2843.576538	123.260182	55.525517
2842.910721	122.221382	55.530522
2842.145024	123.338675	55.535527
2841.352592	131.617722	55.540532
2841.322905	117.644355	55.545537
2840.354097	127.665866	55.550541
2839.730452	129.284264	55.555546
2838.760845	121.331249	55.560551
2837.647048	131.106364	55.565556
2837.407478	127.997400	55.570561
2836.699544	129.637309	55.575565
2836.278635	120.989746	55.580570
2835.602906	121.505101	55.585575
2834.881207	124.489037	55.590580
2834.536689	121.623400	55.595585
2833.348132	119.933039	55.600589
2833.376677	113.063092	55.605594
2832.929981	115.841347	55.610599
2832.067296	119.999610	55.615604
2830.831121	117.602144	55.620609
2830.213506	118.103226	55.625613
2829.919487	125.929992	55.630618
2829.425400	122.115338	55.635623
2828.047328	121.474577	55.640628
2827.007749	121.536210	55.645633
2827.018167	127.163635	55.650637
2826.608452	125.824101	55.655642
2825.502025	119.006024	55.660647
2825.019918	133.170300	55.665652
2824.423917	128.604135	55.670657
2823.534555	127.041057	55.675661
2823.445164	121.548333	55.680666
2822.990354	127.383950	55.685671
2821.916190	122.464914	55.690676
2820.999089	124.232938	55.695681
2820.079209	126.476688	55.700685
2819.581006	121.455665	55.705690
2819.433183	121.052662	55.710695
2818.592966	124.116064	55.715700
2818.329246	116.317145	55.720705
2816.843888	120.077370	55.725709
2815.887320	119.379968	55.730714
2815.689772	113.642055	55.735719
2815.247948	131.710392	55.740724
2814.988801	124.959871	55.745729
2813.971356	126.073616	55.750733
2813.713556	120.376787	55.755738
2812.790006	127.743924	55.760743
2811.590403	122.171348	55.765748
2811.194274	111.844735	55.770753
2810.239248	123.655551	55.775757
2809.679269	119.068235	55.780762
2809.741145	117.971385	55.785767
2808.685490	128.710748	55.790772
2807.976814	116.668386	55.795777
2806.614400	122.785432	55.800781
2806.158150	118.337095	55.805786
2805.895342	115.524994	55.810791
2804.927859	124.128422	55.815796
2805.048088	115.129047	55.820801
2804.454523	120.300763	55.825805
2803.675290	124.099382	55.830810
2803.016441	118.890297	55.835815
2801.199859	128.596454	55.840820
2801.032497	121.709857	55.845825
2800.332522	115.230863	55.850829
2799.465305	120.779736	55.855834
2799.319970	115.980243	55.860839
2798.749360	113.072728	55.865844
2798.659095	110.874543	55.870849
2798.061771	114.452996	55.875853
2796.701875	114.093735	55.880858
2796.213083	107.427866	55.885863
2795.269427	120.661699	55.890868
2795.262997	104.971264	55.895873
2794.355410	112.681842	55.900877
2792.779655	118.036821	55.905882
2792.154179	123.309516	55.910887
2791.776674	122.559333	55.915892
2791.346338	112.405144	55.920897
2790.362775	115.389629	55.925901
2789.869662	117.408868	55.930906
2789.379981	116.019059	55.935911
2789.026284	123.768394	55.940916
2788.637237	117.419808	55.945921
2788.156853	118.049409	55.950925
2786.390321	112.630973	55.955930
2786.023852	117.945449	55.960935
2785.307234	116.272331	55.965940
2784.970933	112.638343	55.970945
2783.964913	115.056683	55.975949
2783.440938	114.093515	55.980954
2783.342924	109.497905	55.985959
2781.961804	119.334496	55.990964
2781.254325	106.114476	55.995969
2780.693588	112.559887	56.000973
2780.291283	118.518760	56.005978
2779.727888	110.456866	56.010983
2779.147945	117.385548	56.015988
2778.634186	109.094519	56.020993
2777.597585	112.523848	56.025997
2776.594881	115.667129	56.031002
2776.363528	111.931917	56.036007
2775.886158	115.196589	56.041012
2775.139370	111.641444	56.046017
2774.220650	117.496349	56.051021
2773.355694	113.777854	56.056026
2772.992968	110.693500	56.061031
2772.878789	113.198616	56.066036
2772.136608	110.323587	56.071041
2770.494639	115.284898	56.076045
2769.746935	120.142312	56.081050
2769.114164	117.226872	56.086055
2768.597451	119.631845	56.091060
2768.316416	118.982804	56.096065
2767.494979	118.968480	56.101069
2766.823080	117.131805	56.106074
2766.766841	113.815072	56.111079
2766.050772	125.728336	56.116084
2765.763510	120.207858	56.121089
2764.653879	118.281003	56.126093
2763.226812	114.833842	56.131098
2763.266173	120.020537	56.136103
2762.608748	126.847996	56.141108
2761.771391	123.508851	56.146113
2760.538859	122.769813	56.151117
2759.758780	124.050623	56.156122
2759.486280	116.668069	56.161127
2758.399060	116.289054	56.166132
2758.357887	122.509485	56.171137
2758.046491	122.840213	56.176141
2757.634304	120.099040	56.181146
2757.545254	112.674476	56.186151
2756.082846	120.088322	56.191156
2755.212098	113.071305	56.196161
2754.356676	111.783880	56.201165
2753.637157	116.796341	56.206170
2753.354551	120.186406	56.211175
2751.687881	116.792831	56.216180
2751.464396	117.443655	56.221185
2750.824924	117.942560	56.226189
2750.123657	115.646314	56.231194
2749.942524	108.880105	56.236199
2749.649197	111.773462	56.241204
2749.113883	112.845073	56.246209
2748.302036	112.732405	56.251213
2746.961688	109.623707	56.256218
2746.331309	110.676832	56.261223
2745.735485	115.150665	56.266228
2745.210491	107.757592	56.271233
2744.832415	119.066780	56.276237
2744.362529	112.897409	56.281242
2743.642994	110.347320	56.286247
2742.044984	118.496036	56.291252
2741.673612	112.504033	56.296257
2741.285402	113.161302	56.301261
2740.266093	115.081013	56.306266
2740.399876	117.682691	56.311271
2739.023111	118.613528	56.316276
2738.457973	109.959456	56.321281
2737.913650	108.305843	56.326285
2736.968173	115.129244	56.331290
2737.238946	109.999301	56.336295
2736.304337	116.621114	56.341300
2734.981219	108.668557	56.346305
2733.978140	113.686065	56.351309
2734.073276	113.864021	56.356314
2733.549375	108.115585	56.361319
2732.523173	113.547560	56.366324
2732.531564	105.975298	56.371329
2731.733822	114.351167	56.376333
2730.835930	119.361356	56.381338
2730.114866	102.294308	56.386343
2729.093135	108.621150	56.391348
2728.414641	111.773757	56.396353
2728.192491	119.546787	56.401357
2727.238501	114.951437	56.406362
2726.987936	103.670386	56.411367
2725.700941	116.197133	56.416372
2725.356038	107.217272	56.421377
2724.231924	107.421658	56.426381
2723.904392	109.847191	56.431386
2723.993641	108.368304	56.436391
2723.408864	109.214695	56.441396
2722.417842	106.460363	56.446401
2721.462062	110.310084	56.451405
2720.549353	113.291546	56.456410
2720.152797	113.488809	56.461415
2719.357063	119.874526	56.466420
2719.092800	111.316657	56.471425
2717.882298	115.003476	56.476429
2716.836492	120.835901	56.481434
2716.383415	107.183609	56.486439
2715.766195	119.989814	56.491444
2715.829851	110.298296	56.496449
2715.190408	113.205420	56.501453
2714.990034	112.719037	56.506458
2714.294758	116.335949	56.511463
2712.614886	113.130166	56.516468
2712.398561	112.592827	56.521473
2711.763333	108.642847	56.526477
2710.823661	110.764470	56.531482
2710.152764	109.493274	56.536487
2709.335659	114.992141	56.541492
2708.490933	115.362322	56.546497
2708.109409	115.744905	56.551501
2707.628262	119.457057	56.556506
2707.654991	105.883804	56.561511
2705.902051	119.671612	56.566516
2705.293055	110.636238	56.571521
2704.473380	106.728838	56.576525
2703.990545	117.239242	56.581530
2703.871828	111.397868	56.586535
2703.205182	112.825475	56.591540
2703.068768	111.527262	56.596545
2701.684236	113.408750	56.601549
2700.586309	113.484721	56.606554
2699.992744	111.820582	56.611559
2699.382280	113.165562	56.616564
2699.079382	113.931801	56.621569
2698.423127	111.670105	56.626573
2697.989671	120.214231	56.631578
2697.413797	112.240140	56.636583
2696.219345	117.660223	56.641588
2695.622119	112.296551	56.646593
2695.106607	116.590086	56.651597
2694.674113	115.722997	56.656602
2694.042039	107.895091	56.661607
2693.036563	108.736027	56.666612
2692.306473	108.812282	56.671617
2691.562665	106.105698	56.676621
2691.112768	115.523396	56.681626
2690.678366	107.806961	56.686631
2689.422679	114.223535	56.691636
2688.680211	114.867942	56.696641
2688.168900	110.061149	56.701645
2687.276775	110.538512	56.706650
2686.974944	106.951930	56.711655
2686.755140	107.826726	56.716660
2686.304896	111.609775	56.721665
2685.658425	106.457809	56.726669
2684.212018	106.695188	56.731674
2683.807297	100.521008	56.736679
2682.876052	104.870997	56.741684
2682.780186	97.913388	56.746689
2682.339405	101.677845	56.751693
2681.651985	108.035177	56.756698
2680.770881	104.212492	56.761703
2679.762103	105.770421	56.766708
2679.418871	111.289734	56.771713
2678.015030	110.010803	56.776717
2676.897252	113.708621	56.781722
2676.955487	102.296639	56.786727
2676.687323	104.616106	56.791732
2675.638869	102.929861	56.796737
2675.275878	104.749631	56.801741
2674.654001	107.738226	56.806746
2674.812549	99.894392	56.811751
2673.753398	117.193110	56.816756
2672.314949	105.183958	56.821761
2671.943524	105.326008	56.826765
2671.177338	101.209742	56.831770
2671.127651	99.061863	56.836775
2669.589209	110.015981	56.841780
2668.762840	107.540217	56.846785
2668.165052	108.521070	56.851789
2667.271658	107.808555	56.856794
2666.844966	102.957304	56.861799
2666.249976	110.759717	56.866804
2666.049392	104.654851	56.871809
2665.675153	109.565666	56.876813
2665.571962	114.207920	56.881818
2664.600140	104.264342	56.886823
2663.336278	112.595156	56.891828
2662.217066	106.564818	56.896833
2661.689462	99.406675	56.901837
2661.631632	108.625907	56.906842
2661.407583	101.998491	56.911847
2660.026839	105.253378	56.916852
2659.192520	107.409499	56.921857
2658.893204	105.279422	56.926861
2658.292205	111.333045	56.931866
2657.594594	104.004625	56.936871
2656.041625	113.888368	56.941876
2655.749046	105.785339	56.946881
2655.377349	110.938475	56.951885
2654.581670	106.912513	56.956890
2654.412541	105.338061	56.961895
2653.495874	111.541562	56.966900
2653.287285	108.645998	56.971905
2652.004137	111.365142	56.976909
2651.211523	112.304302	56.981914
2651.248890	101.621791	56.986919
2650.309510	112.519694	56.991924
2649.655425	103.319548	56.996929
2648.502595	106.089835	57.001933
2647.735956	106.538648	57.006938
2647.606706	107.772165	57.011943
2646.797364	112.794066	57.016948
2646.920310	110.264581	57.021953
2645.844404	98.732272	57.026957
2644.697534	105.020515	57.031962
2643.793704	97.206709	57.036967
2643.117050	108.909544	57.041972
2642.896328	104.748988	57.046977
2642.820331	101.684318	57.051981
2641.861295	114.309348	57.056986
2640.748637	106.175983	57.061991
2639.994180	101.863907	57.066996
2639.477089	104.060931	57.072001
2639.280513	109.638856	57.077005
2638.653503	109.202511	57.082010
2637.899002	107.570627	57.087015
2636.574377	113.970573	57.092020
2636.129335	106.797924	57.097025
2635.638818	108.724362	57.102029
2635.015414	101.867986	57.107034
2634.381956	101.471427	57.112039
2633.353889	104.994051	57.117044
2632.946861	105.726778	57.122049
2632.405093	102.112930	57.127053
2631.704237	97.729328	57.132058
2631.270215	99.391510	57.137063
2630.543379	106.588452	57.142068
2629.611352	100.483497	57.147073
2628.878446	97.062188	57.152077
2628.074812	113.379358	57.157082
2627.687852	102.898853	57.162087
2627.505718	103.351960	57.167092
2626.290343	101.795703	57.172097
2625.702921	100.592747	57.177101
2624.831828	105.550995	57.182106
2624.812747	104.500352	57.187111
2623.852616	107.867290	57.192116
2622.828552	104.108526	57.197121
2622.260064	104.622940	57.202125
2621.462896	110.371029	57.207130
2620.707361	99.357893	57.212135
2620.273589	103.114444	57.217140
2619.984829	99.220119	57.222145
2619.296236	101.999471	57.227149
2618.616661	110.781841	57.232154
2617.621874	100.893519	57.237159
2617.042856	103.084552	57.242164
2616.270917	98.914019	57.247169
2616.154725	97.456832	57.252173
2615.609431	103.155547	57.257178
2614.544236	100.848116	57.262183
2613.972148	109.777896	57.267188
2613.477412	96.568929	57.272193
2613.181607	90.038655	57.277197
2611.586492	99.158704	57.282202
2610.746015	95.847363	57.287207
2609.766974	105.222484	57.292212
2609.867712	98.932700	57.297217
2609.572410	94.575694	57.302221
2608.933149	106.347922	57.307226
2608.215095	101.014791	57.312231
2607.230995	106.376032	57.317236
2606.508109	98.948922	57.322241
2605.432016	93.568846	57.327245
2605.211788	94.575948	57.332250
2605.274109	89.945053	57.337255
2603.919643	93.310718	57.342260
2602.989443	98.281044	57.347265
2602.313234	94.248881	57.352269
2601.828663	94.607641	57.357274
2601.436932	89.649772	57.362279
2600.987449	98.753581	57.367284
2599.903722	89.387301	57.372289
2599.259059	93.792909	57.377293
2598.112650	99.961081	57.382298
2597.850066	92.852383	57.387303
2597.656274	96.875006	57.392308
2596.818044	98.537606	57.397313
2595.944253	93.968054	57.402317
2594.963203	97.726979	57.407322
2594.419205	94.566663	57.412327
2594.255174	98.020927	57.417332
2593.698538	101.987555	57.422337
2592.947128	95.450299	57.427341
2591.727251	105.431049	57.432346
2591.268316	97.207266	57.437351
2590.427906	94.253144	57.442356
2590.328472	91.310902	57.447361
2590.054747	93.950258	57.452365
2588.158468	100.192148	57.457370
2587.659161	89.948359	57.462375
2587.307481	97.951929	57.467380
2586.754881	92.583811	57.472385
2586.402900	86.098670	57.477389
2585.635565	91.222727	57.482394
2585.103160	93.281850	57.487399
2584.083716	96.645115	57.492404
2583.384005	100.864747	57.497409
2583.060124	97.304052	57.502413
2582.577913	104.881927	57.507418
2581.535241	99.429037	57.512423
2580.839080	94.224405	57.517428
2580.082873	96.493097	57.522433
2579.775021	94.160414	57.527437
2578.367127	100.278556	57.532442
2578.016625	88.163204	57.537447
2577.022599	96.122245	57.542452
2576.633244	101.450497	57.547457
2576.242467	96.911664	57.552461
2575.773064	97.780974	57.557466
2575.357303	95.846464	57.562471
2574.366763	94.807951	57.567476
2573.349396	95.758700	57.572481
2572.828487	92.311424	57.577485
2572.023905	96.928314	57.582490
2571.850991	85.601660	57.587495
2571.402257	93.187228	57.592500
2569.939483	88.647320	57.597505
2569.616879	93.745087	57.602509
2568.645743	98.116906	57.607514
2568.351619	88.008172	57.612519
2567.758938	92.929879	57.617524
2566.584955	95.345780	57.622529
2566.228038	101.592933	57.627533
2565.214193	104.906693	57.632538
2564.931367	96.533602	57.637543
2564.405293	98.996237	57.642548
2563.705762	97.203394	57.647553
2563.490480	103.622118	57.652557
2561.975160	100.649565	57.657562
2561.597128	100.076722	57.662567
2561.048804	100.039028	57.667572
2560.097598	102.057646	57.672577
2559.898127	92.485344	57.677581
2558.951523	97.287958	57.682586
2558.042536	89.610844	57.687591
2557.155603	100.184393	57.692596
2557.019717	101.490885	57.697601
2556.617049	98.948235	57.702605
2555.940799	104.159356	57.707610
2555.250186	98.323008	57.712615
2554.232964	100.343834	57.717620
2553.578415	103.551964	57.722625
2553.241596	94.814696	57.727629
2552.429176	101.359580	57.732634
2552.124199	101.236076	57.737639
2551.529002	110.692818	57.742644
2550.352556	102.858535	57.747649
2550.352207	90.005979	57.752653
2549.316047	94.444177	57.757658
2548.504733	90.890634	57.762663
2546.909224	106.446354	57.767668
2546.344764	106.068404	57.772673
2546.219977	95.930325	57.777677
2545.436115	103.107808	57.782682
2545.388856	102.204085	57.787687
2545.129043	101.241176	57.792692
2544.369621	100.634064	57.797697
2543.530742	96.805372	57.802701
2542.312330	96.103049	57.807706
2542.206529	93.586622	57.812711
2541.686061	98.694928	57.817716
2540.293077	95.635155	57.822721
2539.518554	89.998679	57.827725
2538.370233	100.410079	57.832730
2538.631138	101.208224	57.837735
2537.918078	102.837197	57.842740
2537.456737	102.191364	57.847745
2536.931341	98.217505	57.852749
2535.778268	110.491246	57.857754
2535.194979	103.606714	57.862759
2534.898304	107.025236	57.867764
2534.065265	106.431500	57.872769
2533.253848	95.172161	57.877773
2531.972088	108.199720	57.882778
2531.827948	97.837588	57.887783
2530.696949	106.110967	57.892788
2530.702884	108.102929	57.897793
2530.639242	103.767112	57.902797
2529.648682	115.124943	57.907802
2528.591339	101.800207	57.912807
2527.767132	103.783304	57.917812
2527.173202	97.465052	57.922817
2527.054545	101.610221	57.927821
2526.294313	105.098913	57.932826
2525.206622	97.016579	57.937831
2524.332001	100.856395	57.942836
2523.791538	106.934803	57.947841
2523.312562	94.727739	57.952845
2522.863427	100.326731	57.957850
2522.358955	96.381270	57.962855
2521.324047	103.696803	57.967860
2520.590151	107.271386	57.972865
2520.368955	100.144960	57.977869
2519.755861	114.940652	57.982874
2518.607420	100.049438	57.987879
2517.705585	105.863189	57.992884
2516.907008	100.915278	57.997889
2516.299684	97.077399	58.002893
2515.808445	97.957157	58.007898
2515.829168	90.373339	58.012903
2515.544976	94.574436	58.017908
2514.750881	101.365262	58.022913
2513.749994	90.003328	58.027917
2512.844477	108.250740	58.032922
2512.427952	98.745942	58.037927
2510.873613	91.674549	58.042932
2510.453293	91.824575	58.047937
2510.310477	97.021865	58.052941
2509.294328	99.398951	58.057946
2508.661223	100.554404	58.062951
2508.224609	102.986749	58.067956
2507.585185	108.849190	58.072961
2506.460346	100.532823	58.077965
2505.718283	96.914949	58.082970
2505.513428	102.572043	58.087975
2505.006744	108.056538	58.092980
2504.541246	107.493126	58.097985
2504.114272	98.257345	58.102989
2502.963479	102.825673	58.107994
2502.182963	93.666522	58.112999
2501.739784	98.111110	58.118004
2500.750368	103.737736	58.123009
2500.149242	102.278594	58.128013
2499.387395	100.903374	58.133018
2498.367653	102.803065	58.138023
2497.954051	104.019278	58.143028
2497.655630	97.991552	58.148033
2497.506233	100.343611	58.153037
2496.608323	108.804111	58.158042
2495.876539	98.602449	58.163047
2494.926166	97.246830	58.168052
2494.301611	98.184908	58.173057
2494.022421	89.171361	58.178061
2493.207432	103.557492	58.183066
2492.472251	98.196919	58.188071
2491.861400	96.894961	58.193076
2491.312495	99.663074	58.198081
2490.167763	87.529583	58.203085
2488.810925	101.394554	58.208090
2488.406354	96.104166	58.213095
2487.640326	99.672401	58.218100
2487.470984	101.566832	58.223105
2487.330014	91.487976	58.228109
2486.414722	91.443952	58.233114
2486.391110	92.894664	58.238119
2485.374506	95.664187	58.243124
2484.406468	98.580929	58.248129
2484.203649	86.571396	58.253133
2483.392808	91.486196	58.258138
2482.309569	93.428323	58.263143
2481.346757	90.235025	58.268148
2480.984037	97.879702	58.273153
2480.466534	88.350734	58.278157
2479.899077	94.106922	58.283162
2479.891441	95.061104	58.288167
2478.324974	94.585664	58.293172
2477.265968	98.175176	58.298177
2477.054505	96.351400	58.303181
2476.451993	102.463310	58.308186
2475.876362	93.341766	58.313191
2475.074739	96.034274	58.318196
2473.944213	98.734463	58.323201
2473.362355	97.272819	58.328205
2473.092507	106.465520	58.333210
2472.758651	94.593251	58.338215
2472.110909	96.186195	58.343220
2471.630976	101.539014	58.348225
2470.877479	97.264305	58.353229
2469.792727	103.390377	58.358234
2469.060983	93.444893	58.363239
2468.761890	95.809124	58.368244
2467.468423	94.744662	58.373249
2467.163182	93.600452	58.378253
2466.596146	95.530508	58.383258
2465.801461	96.211896	58.388263
2465.388435	95.363210	58.393268
2464.858522	96.422474	58.398273
2464.146375	92.371217	58.403277
2463.405218	96.234403	58.408282
2462.785098	103.109958	58.413287
2462.408628	97.542408	58.418292
2460.867559	96.956846	58.423297
2460.458180	89.623798	58.428301
2459.635226	95.345120	58.433306
2459.364682	94.742460	58.438311
2458.595786	97.797653	58.443316
2458.331323	99.997284	58.448321
2457.429403	91.266652	58.453325
2456.354837	93.439004	58.458330
2455.632846	95.259769	58.463335
2455.065743	88.736032	58.468340
2454.708911	94.515024	58.473345
2454.873112	95.050233	58.478349
2453.497586	97.987703	58.483354
2452.795092	89.118375	58.488359
2452.046780	94.796542	58.493364
2451.810395	100.576653	58.498369
2450.719865	95.487231	58.503373
2449.689811	107.069306	58.508378
2449.129283	99.702495	58.513383
2448.555169	96.363406	58.518388
2448.123590	98.191360	58.523393
2448.000072	90.616024	58.528397
2446.494959	106.026042	58.533402
2445.760896	98.593773	58.538407
2445.214619	100.337130	58.543412
2444.639051	103.439400	58.548417
2444.542710	99.498378	58.553421
2443.627935	100.764757	58.558426
2442.739726	101.723050	58.563431
2442.009790	106.242327	58.568436
2441.018934	101.688479	58.573441
2440.917914	95.586353	58.578445
2440.352388	99.403725	58.583450
2439.378522	82.106470	58.588455
2438.723678	101.611233	58.593460
2438.118016	101.961895	58.598465
2437.887827	92.373152	58.603469
2437.368630	96.304177	58.608474
2436.605480	95.170367	58.613479
2435.783474	89.704656	58.618484
2435.049434	98.372787	58.623489
2434.216884	89.087161	58.628493
2432.850943	100.292070	58.633498
2432.752820	94.027613	58.638503
2432.247809	93.856215	58.643508
2431.767446	96.763791	58.648513
2431.749183	98.562920	58.653517
2430.217992	99.778382	58.658522
2429.429965	99.366829	58.663527
2428.605916	92.984524	58.668532
2428.488162	107.052901	58.673537
2427.932058	93.889604	58.678541
2426.639874	99.576292	58.683546
2425.756924	96.743549	58.688551
2425.094744	90.583035	58.693556
2424.372218	97.125188	58.698561
2424.829759	92.609484	58.703565
2424.325266	102.885159	58.708570
2423.353933	94.375211	58.713575
2422.451089	101.092271	58.718580
2421.281939	95.900250	58.723585
2421.028138	93.385844	58.728589
2420.298353	88.061075	58.733594
2419.357654	91.120382	58.738599
2418.959969	96.236119	58.743604
2417.793582	97.928799	58.748609
2417.509403	92.264164	58.753613
2416.926038	94.806470	58.758618
2416.448772	88.371192	58.763623
2416.113678	94.273174	58.768628
2415.309831	98.113532	58.773633
2413.897911	85.199200	58.778637
2413.237635	102.023926	58.783642
2412.889428	98.583061	58.788647
2412.543225	94.867126	58.793652
2412.321461	93.339184	58.798657
2411.881806	88.048887	58.803661
2410.298990	98.574849	58.808666
2409.959937	89.226166	58.813671
2409.571426	95.080441	58.818676
2408.100761	101.113824	58.823681
2407.698238	93.467384	58.828685
2407.336857	104.646192	58.833690
2406.701730	96.873342	58.838695
2405.955078	90.405575	58.843700
2404.811260	93.408039	58.848705
2404.125874	91.514120	58.853709
2403.410802	95.646790	58.858714
2403.295368	92.748739	58.863719
2402.837863	85.641819	58.868724
2402.139274	92.725387	58.873729
2401.331818	85.404364	58.878733
2400.156588	90.269373	58.883738
2399.777265	97.165333	58.888743
2399.338007	96.187326	58.893748
2398.717788	93.945961	58.898753
2397.512822	89.028880	58.903757
2397.044002	100.872612	58.908762
2396.110888	93.421497	58.913767
2395.861621	96.911253	58.918772
2395.216483	99.333470	58.923777
2395.353694	98.810695	58.928781
2394.278808	96.312344	58.933786
2393.573693	101.968921	58.938791
2392.942608	105.508174	58.943796
2391.315227	95.821238	58.948801
2390.883483	96.795830	58.953805
2390.109572	100.398186	58.958810
2389.523772	93.283991	58.963815
2389.338673	95.972142	58.968820
2388.700175	97.779034	58.973825
2388.573998	98.675723	58.978829
2387.699816	108.467524	58.983834
2386.621051	99.576491	58.988839
2385.780503	98.511184	58.993844
2385.280582	96.981069	58.998849
2385.476953	96.077928	59.003853
2384.419319	93.816227	59.008858
2383.299148	94.780245	59.013863
2382.493085	98.127975	59.018868
2381.721556	97.035867	59.023873
2381.590007	90.983967	59.028877
2380.373293	92.669075	59.033882
2379.479714	90.845888	59.038887
2379.046798	94.772426	59.043892
2378.562809	99.155314	59.048897
2378.450009	90.666736	59.053901
2377.411748	98.225610	59.058906
2377.452995	89.226366	59.063911
2376.108775	93.283461	59.068916
2374.963516	93.545215	59.073921
2374.807064	89.851707	59.078925
2374.392821	89.684530	59.083930
2373.785395	95.123488	59.088935
2373.045612	94.672117	59.093940
2372.077053	87.709819	59.098945
2371.738322	84.794296	59.103949
2370.928832	91.948537	59.108954
2369.518232	93.435096	59.113959
2368.802245	86.651447	59.118964
2368.451145	93.398506	59.123969
2368.126600	83.765519	59.128973
2367.558353	95.599406	59.133978
2367.419932	90.887191	59.138983
2366.646977	88.314722	59.143988
2365.314734	94.463385	59.148993
2365.340165	85.244620	59.153997
2364.334941	91.863139	59.159002
2363.546021	90.779929	59.164007
2362.622038	93.759415	59.169012
2361.762186	91.755602	59.174017
2361.137033	80.947613	59.179021
2360.868399	84.314761	59.184026
2360.362517	86.235158	59.189031
2359.951499	79.443577	59.194036
2358.656049	89.795673	59.199041
2358.182321	79.682559	59.204045
2357.505276	85.527354	59.209050
2357.004688	93.559535	59.214055
2357.033205	79.825792	59.219060
2355.644599	88.062311	59.224065
2355.087593	82.920374	59.229069
2354.695112	91.548259	59.234074
2354.107862	86.959369	59.239079
2352.440520	89.638872	59.244084
2351.986573	88.522860	59.249089
2351.902168	84.582569	59.254093
2351.193226	90.269009	59.259098
2350.574738	90.187283	59.264103
2349.638937	87.314252	59.269108
2348.558854	94.701074	59.274113
2348.436775	82.125938	59.279117
2348.116969	86.461014	59.284122
2347.547109	92.064860	59.289127
2346.286314	89.629492	59.294132
2345.234603	91.217316	59.299137
2344.795794	78.388852	59.304141
2344.655861	87.026049	59.309146
2343.779792	88.945012	59.314151
2342.708486	82.597509	59.319156
2341.890823	89.176457	59.324161
2341.640446	85.041528	59.329165
2340.986652	85.600950	59.334170
2340.477649	90.708880	59.339175
2340.383758	83.786497	59.344180
2339.339780	90.419538	59.349185
2338.198445	87.826383	59.354189
2337.492846	94.690504	59.359194
2337.532652	94.030441	59.364199
2337.150820	88.200547	59.369204
2335.370287	94.341005	59.374209
2335.025531	94.161949	59.379213
2334.588944	88.387601	59.384218
2333.901224	87.977068	59.389223
2333.296466	86.160949	59.394228
2332.216179	96.430474	59.399233
2332.037599	85.428894	59.404237
2331.220740	92.968465	59.409242
2330.359217	91.924121	59.414247
2329.732355	85.485624	59.419252
2328.804860	97.440938	59.424257
2328.463912	88.266272	59.429261
2327.623116	87.962833	59.434266
2327.428235	89.172838	59.439271
2327.113451	85.466541	59.444276
2325.643765	96.650518	59.449281
2325.106786	85.959294	59.454285
2324.534343	91.035837	59.459290
2324.032796	81.504176	59.464295
2323.790746	82.475940	59.469300
2322.850203	87.960018	59.474305
2322.216022	87.779929	59.479309
2321.228732	89.633442	59.484314
2321.145732	93.482780	59.489319
2320.008710	86.141947	59.494324
2319.045090	93.521094	59.499329
2318.484178	82.614105	59.504333
2317.699266	87.425805	59.509338
2317.206228	85.148889	59.514343
2317.088407	82.053497	59.519348
2315.305681	90.988580	59.524353
2314.775329	85.551179	59.529357
2314.332785	88.223749	59.534362
2313.902660	79.219860	59.539367
2313.331793	84.068771	59.544372
2312.716150	92.515745	59.549377
2312.493780	83.158576	59.554381
2311.501690	90.574957	59.559386
2310.623996	92.751957	59.564391
2310.443892	83.768469	59.569396
2309.713851	82.230742	59.574401
2308.179232	81.193347	59.579405
2307.408830	85.174042	59.584410
2307.059584	87.819606	59.589415
2306.947670	81.137538	59.594420
2306.111513	87.252299	59.599425
2305.940757	80.659238	59.604429
2305.158525	86.841749	59.609434
2304.073564	86.423755	59.614439
2303.549490	77.200285	59.619444
2302.767452	78.236756	59.624449
2302.603732	85.646481	59.629453
2301.397246	88.817962	59.634458
2300.820821	85.758756	59.639463
2300.232937	75.080986	59.644468
2299.501916	81.738273	59.649473
2298.658089	80.704331	59.654477
2297.396328	73.895613	59.659482
2297.224359	86.349335	59.664487
2296.878404	81.440124	59.669492
2296.588910	86.536175	59.674497
2296.022105	77.035023	59.679501
2294.925796	90.483623	59.684506
2293.675705	80.629985	59.689511
2292.858237	77.171884	59.694516
2292.354813	81.317313	59.699521
2292.630602	81.769884	59.704525
2292.007173	82.484376	59.709530
2291.401902	86.511833	59.714535
2290.627812	74.769761	59.719540
2289.771788	79.460994	59.724545
2289.155452	79.987174	59.729549
2287.897843	85.637971	59.734554
2287.263903	78.292832	59.739559
2286.801256	76.969111	59.744564
2286.385392	84.736546	59.749569
2285.804421	75.980294	59.754573
2284.802190	81.452029	59.759578
2283.902895	85.885411	59.764583
2283.372148	76.474013	59.769588
2283.052101	80.527297	59.774593
2282.519751	77.119123	59.779597
2282.217393	84.219408	59.784602
2281.234539	89.235085	59.789607
2280.623736	79.310421	59.794612
2279.595804	90.511224	59.799617
2278.986343	83.103084	59.804621
2277.819387	79.486467	59.809626
2276.992622	79.996924	59.814631
2276.731367	79.337031	59.819636
2276.260517	90.641906	59.824641
2276.268568	84.223132	59.829645
2275.543993	87.253395	59.834650
2274.844001	89.212912	59.839655
2273.984032	83.442688	59.844660
2273.232721	84.497987	59.849665
2272.325818	78.804472	59.854669
2271.170806	89.592416	59.859674
2270.563694	89.535594	59.864679
2270.047085	82.929050	59.869684
2269.472100	84.158268	59.874689
2269.490347	82.240358	59.879693
2269.391501	80.611672	59.884698
2267.969339	78.527595	59.889703
2267.604682	81.598937	59.894708
2266.547252	78.881325	59.899713
2265.778784	90.404851	59.904718
2264.612118	84.199987	59.909722
2263.804414	86.248975	59.914727
2263.437612	88.688734	59.919732
2262.893501	84.367209	59.924737
2262.481301	87.796408	59.929742
2262.223678	84.745056	59.934746
2261.467864	94.152285	59.939751
2260.974947	83.963129	59.944756
2259.718566	89.980815	59.949761
2259.745446	82.523463	59.954766
2258.606226	86.610653	59.959770
2257.725277	87.195114	59.964775
2257.137520	79.123686	59.969780
2256.407559	92.045447	59.974785
2255.861878	85.186911	59.979790
2255.527011	84.678549	59.984794
2254.129049	87.605292	59.989799
2253.299396	81.132413	59.994804
2252.873287	90.583912	59.999809
2252.605982	87.948676	60.004814
2251.861118	89.661668	60.009818
2251.358685	90.442707	60.014823
2251.545489	86.957736	60.019828
2250.246228	95.838579	60.024833
2249.644604	87.081123	60.029838
2248.658361	87.995422	60.034842
2247.275139	83.019660	60.039847
2246.628866	82.647445	60.044852
2246.435656	85.424611	60.049857
2246.296578	78.923636	60.054862
2245.336699	77.547588	60.059866
2245.047138	78.077100	60.064871
2244.519213	74.612913	60.069876
2243.651099	85.769806	60.074881
2242.831784	74.325998	60.079886
2242.502794	79.137889	60.084890
2240.880708	79.106226	60.089895
2240.496404	76.099830	60.094900
2239.828704	91.361518	60.099905
2239.601467	89.916625	60.104910
2239.018527	88.741765	60.109914
2237.685307	87.090495	60.114919
2237.327812	80.370302	60.119924
2236.612952	90.392609	60.124929
2236.278836	83.283562	60.129934
2235.850486	84.428105	60.134938
2234.694813	91.686160	60.139943
2234.145535	86.884749	60.144948
2233.127236	92.787122	60.149953
2232.421164	82.139048	60.154958
2232.209531	89.013037	60.159962
2231.655590	83.422979	60.164967
2230.631059	84.839996	60.169972
2229.995562	90.360732	60.174977
2229.277891	87.412924	60.179982
2228.911930	83.085411	60.184986
2228.600985	87.025040	60.189991
2227.805491	84.589471	60.194996
2226.570759	91.298172	60.200001
2225.834283	83.617695	60.205006
2225.629393	93.744628	60.210010
2225.313023	83.048463	60.215015
2224.253074	82.394506	60.220020
2223.414679	84.257307	60.225025
2222.651062	83.745299	60.230030
2222.108935	78.946617	60.235034
2221.534807	84.527906	60.240039
2221.374227	82.580186	60.245044
2219.999632	76.023279	60.250049
2219.603605	82.006726	60.255054
2219.050206	80.677611	60.260058
2218.444144	89.741083	60.265063
2217.740379	83.382466	60.270068
2216.647500	84.121199	60.275073
2216.251184	79.687963	60.280078
2216.199371	75.432251	60.285082
2215.189835	89.524413	60.290087
2214.339925	74.030066	60.295092
2213.583414	82.832694	60.300097
2213.067810	74.047911	60.305102
2211.840786	80.653848	60.310106
2210.608434	83.344654	60.315111
2210.751252	77.450321	60.320116
2210.335566	86.898455	60.325121
2209.495269	84.276347	60.330126
2208.928092	79.545502	60.335130
2208.513909	90.209126	60.340135
2208.300603	78.496298	60.345140
2206.745326	81.942963	60.350145
2205.958197	83.024132	60.355150
2205.557279	83.326777	60.360154
2204.918105	92.519856	60.365159
2204.987628	83.113574	60.370164
2203.955308	91.441156	60.375169
2203.235419	88.516625	60.380174
2202.626154	84.103229	60.385178
2201.516004	84.631373	60.390183
2200.989201	82.811414	60.395188
2199.789606	91.429700	60.400193
2198.849999	89.447056	60.405198
2199.109893	88.238188	60.410202
2198.592731	87.873502	60.415207
2198.554737	80.117393	60.420212
2197.961562	84.101341	60.425217
2196.715100	80.661757	60.430222
2195.906784	81.155255	60.435226
2195.064090	87.287327	60.440231
2193.986197	79.541305	60.445236
2193.275274	79.709080	60.450241
2193.037279	83.865961	60.455246
2192.478205	81.526146	60.460250
2191.874953	85.484582	60.465255
2191.872982	87.762086	60.470260
2190.927607	88.497308	60.475265
2190.367983	78.810613	60.480270
2189.642661	85.169708	60.485274
2188.599099	91.767171	60.490279
2188.037506	85.643185	60.495284
2186.979673	86.800651	60.500289
2186.612345	90.827684	60.505294
2185.598811	86.570267	60.510298
2184.435336	85.761135	60.515303
2184.121166	80.915578	60.520308
2183.321634	83.988273	60.525313
2182.756442	87.312987	60.530318
2182.338856	85.220939	60.535322
2181.943417	92.781207	60.540327
2181.859586	79.901543	60.545332
2180.904907	90.350114	60.550337
2180.128447	87.020014	60.555342
2179.096137	90.428957	60.560346
2178.743299	89.143307	60.565351
2178.414308	86.421919	60.570356
2177.161679	90.736538	60.575361
2176.434440	88.160230	60.580366
2176.161280	92.532725	60.585370
2175.421436	87.740626	60.590375
2175.269043	81.392323	60.595380
2174.056174	93.019880	60.600385
2173.064917	83.724363	60.605390
2172.571611	86.554826	60.610394
2171.792452	88.907223	60.615399
2171.541974	77.324307	60.620404
2170.275282	79.913629	60.625409
2169.743699	81.982903	60.630414
2169.398825	76.438416	60.635418
2168.760987	89.705590	60.640423
2168.374473	83.542586	60.645428
2167.479809	91.272308	60.650433
2166.552565	89.117431	60.655438
2166.082332	80.765009	60.660442
2165.430581	95.188341	60.665447
2165.200432	80.458770	60.670452
2164.113484	84.340463	60.675457
2163.220340	85.014258	60.680462
2163.133526	87.610997	60.685466
2162.098929	89.030538	60.690471
2161.855505	81.775338	60.695476
2160.686230	78.708602	60.700481
2159.736481	76.011280	60.705486
2159.631023	79.624854	60.710490
2158.489726	89.709436	60.715495
2158.371628	83.538816	60.720500
2156.807594	81.092994	60.725505
2156.392051	77.694069	60.730510
2155.824313	72.192043	60.735514
2155.386139	80.796154	60.740519
2155.631344	80.355559	60.745524
2154.597204	88.846083	60.750529
2153.867851	83.929435	60.755534
2152.921173	78.333537	60.760538
2152.246180	85.812538	60.765543
2151.785633	77.507805	60.770548
2150.624043	85.098447	60.775553
2150.027536	83.252916	60.780558
2149.228265	73.422490	60.785562
2148.883404	84.287797	60.790567
2148.831434	84.026707	60.795572
2147.743532	77.823407	60.800577
2146.395531	80.491374	60.805582
2145.922112	76.798413	60.810586
2145.193603	85.243374	60.815591
2145.088076	74.868787	60.820596
2144.324633	77.326257	60.825601
2144.149143	82.913579	60.830606
2142.937430	80.365270	60.835610
2142.196338	77.255306	60.840615
2141.942364	75.001865	60.845620
2140.982717	87.525552	60.850625
2139.675081	78.139689	60.855630
2139.217860	73.513993	60.860634
2138.485203	77.340226	60.865639
2138.616573	84.659211	60.870644
2138.114820	77.812528	60.875649
2137.530251	79.819421	60.880654
2136.688080	77.851309	60.885658
2135.819440	79.361281	60.890663
2135.507900	72.842450	60.895668
2134.018818	81.683532	60.900673
2133.398114	75.815186	60.905678
2133.022478	83.428507	60.910682
2132.263670	89.794914	60.915687
2132.017813	81.017690	60.920692
2131.303816	86.194237	60.925697
2130.187252	83.780047	60.930702
2129.569471	79.172733	60.935706
2128.977956	89.556826	60.940711
2128.722402	88.753076	60.945716
2127.954376	82.206134	60.950721
2126.773698	81.983357	60.955726
2126.340451	83.384919	60.960730
2125.325070	87.600945	60.965735
2125.339947	77.399180	60.970740
2125.002529	81.994629	60.975745
2124.316964	85.056128	60.980750
2123.280284	79.500497	60.985754
2122.697555	87.055690	60.990759
2121.846225	81.072846	60.995764
2120.614017	84.834528	61.000769
2120.031015	80.902952	61.005774
2119.817328	84.915155	61.010778
2119.253583	89.088279	61.015783
2118.960497	82.689047	61.020788
2117.842541	84.195876	61.025793
2116.923015	84.167637	61.030798
2116.537434	82.263536	61.035802
2115.580527	82.239718	61.040807
2115.197068	75.178603	61.045812
2114.860828	92.683641	61.050817
2113.562450	86.886990	61.055822
2112.972449	70.985477	61.060826
2112.627927	87.511042	61.065831
2112.198703	74.924932	61.070836
2111.699996	82.774425	61.075841
2110.753264	79.768714	61.080846
2110.164613	78.444852	61.085850
2109.457158	81.856662	61.090855
2108.959101	81.924491	61.095860
2107.509326	70.988802	61.100865
2106.625107	79.450130	61.105870
2106.402070	77.636252	61.110874
2105.545996	84.220208	61.115879
2105.244123	72.611362	61.120884
2104.869286	80.071392	61.125889
2104.649612	75.920974	61.130894
2103.415204	78.240324	61.135898
2102.572520	80.114926	61.140903
2102.479168	78.803059	61.145908
2101.131260	73.065018	61.150913
2099.800356	72.288489	61.155918
2099.598781	75.485885	61.160922
2098.858803	80.345178	61.165927
2098.810423	77.016483	61.170932
2098.455531	79.230798	61.175937
2097.910547	74.845505	61.180942
2097.076785	70.774068	61.185946
2096.242375	75.711877	61.190951
2095.974580	76.424772	61.195956
2094.576220	77.841016	61.200961
2093.647436	82.935885	61.205966
2093.326964	79.117695	61.210970
2092.663357	76.309081	61.215975
2092.432631	71.100331	61.220980
2091.538383	76.794400	61.225985
2090.928938	73.522987	61.230990
2090.147613	74.073461	61.235994
2089.425814	78.668339	61.240999
2088.941075	65.443604	61.246004
2087.842904	74.755441	61.251009
2086.869334	67.788161	61.256014
2086.615978	72.408702	61.261018
2085.862992	78.660036	61.266023
2085.695620	68.625238	61.271028
2085.305363	73.902328	61.276033
2084.344675	79.764073	61.281038
2083.464202	65.778107	61.286042
2082.779112	80.825260	61.291047
2082.452258	70.987074	61.296052
2081.715276	72.380985	61.301057
2080.711932	73.870190	61.306062
2080.011132	66.553112	61.311066
2079.449658	76.456813	61.316071
2079.214271	73.230761	61.321076
2078.536941	82.538910	61.326081
2077.135445	74.155141	61.331086
2076.694993	71.738213	61.336090
2076.195165	83.693797	61.341095
2075.683923	71.951432	61.346100
2075.093476	76.107018	61.351105
2074.112864	80.476175	61.356110
2073.353303	74.647774	61.361114
2072.621639	78.407530	61.366119
2072.253893	68.575947	61.371124
2071.701586	77.911261	61.376129
2071.314255	81.309766	61.381134
2070.750124	72.916981	61.386138
2069.557423	77.273074	61.391143
2069.335197	64.657497	61.396148
2068.378877	73.907181	61.401153
2067.347385	76.671813	61.406158
2066.768991	71.518189	61.411162
2066.044140	67.585230	61.416167
2065.535216	66.711537	61.421172
2065.158581	68.181573	61.426177
2064.538161	67.977452	61.431182
2063.900024	72.504338	61.436186
2063.181016	80.718342	61.441191
2062.535213	69.646341	61.446196
2061.936365	85.783178	61.451201
2060.940292	79.008031	61.456206
2060.148928	81.019909	61.461210
2059.346001	85.733664	61.466215
2058.779000	67.890150	61.471220
2058.470469	78.069918	61.476225
2058.056065	74.164777	61.481230
2057.356011	77.268231	61.486234
2056.384502	83.133016	61.491239
2056.277444	79.210039	61.496244
2055.388335	86.447784	61.501249
2054.005688	79.173518	61.506254
2053.669063	79.194004	61.511258
2052.898884	79.291015	61.516263
2052.863870	75.170987	61.521268
2052.131981	83.845863	61.526273
2050.552993	74.037911	61.531278
2050.451935	75.125299	61.536282
2049.777857	77.472366	61.541287
2049.511872	74.732321	61.546292
2048.629499	72.137178	61.551297
2047.573197	77.336754	61.556302
2047.086124	81.827148	61.561306
2046.434448	86.947255	61.566311
2046.079559	77.478984	61.571316
2045.593449	80.841493	61.576321
2044.692566	87.931654	61.581326
2043.849994	77.394606	61.586330
2043.031233	76.879031	61.591335
2042.774766	72.043359	61.596340
2042.088080	74.499947	61.601345
2040.958932	83.689204	61.606350
2040.243062	72.455514	61.611354
2039.423503	80.786977	61.616359
2039.116466	67.688560	61.621364
2038.804272	71.397094	61.626369
2038.645789	71.367768	61.631374
2037.521892	67.366102	61.636378
2036.569661	71.311608	61.641383
2035.863980	74.312215	61.646388
2035.483466	75.593056	61.651393
2034.282527	67.739058	61.656398
2034.064320	67.647714	61.661402
2033.259716	76.931054	61.666407
2032.964547	78.753066	61.671412
2032.349792	74.905486	61.676417
2031.485164	76.325579	61.681422
2031.220994	68.849354	61.686426
2029.926673	73.167180	61.691431
2028.946198	75.495608	61.696436
2028.209151	80.784652	61.701441
2027.405448	81.937756	61.706446
2027.390239	78.921142	61.711450
2027.266173	75.926305	61.716455
2026.916856	68.762265	61.721460
2025.023509	71.623404	61.726465
2024.294598	69.631599	61.731470
2024.108082	68.195939	61.736474
2023.952210	75.083664	61.741479
2023.174130	75.266502	61.746484
2022.152987	70.499264	61.751489
2021.312625	77.908269	61.756494
2020.752671	69.489913	61.761498
2019.974563	79.859734	61.766503
2019.197988	74.627916	61.771508
2017.860290	77.892153	61.776513
2017.362444	79.786726	61.781518
2017.653037	72.916634	61.786522
2016.568689	76.487259	61.791527
2016.293839	76.719408	61.796532
2016.242409	74.561589	61.801537
2014.965405	82.198041	61.806542
2014.162501	77.204402	61.811546
2013.630164	82.615927	61.816551
2013.092662	70.585974	61.821556
2011.782523	67.877702	61.826561
2010.715446	72.705323	61.831566
2010.419124	71.549752	61.836570
2010.246326	80.936594	61.841575
2009.655440	78.453435	61.846580
2009.399370	80.457041	61.851585
2008.752242	73.861424	61.856590
2007.933354	75.145017	61.861594
2007.228320	76.274931	61.866599
2006.378218	77.240981	61.871604
2005.208707	76.879353	61.876609
2004.584479	70.676910	61.881614
2004.260775	65.912348	61.886618
2004.050465	82.172973	61.891623
2003.180091	76.459457	61.896628
2001.868198	74.083447	61.901633
2001.161895	78.223726	61.906638
2000.831619	80.428309	61.911642
2000.322226	77.049402	61.916647
1999.958943	69.662764	61.921652
1999.491713	76.586775	61.926657
1998.348435	76.225792	61.931662
1997.787046	72.435008	61.936666
1997.308022	88.086365	61.941671
1996.053676	78.349212	61.946676
1994.806915	74.706453	61.951681
1994.538753	77.083166	61.956686
1993.686254	75.208028	61.961690
1993.568519	81.524779	61.966695
1993.082642	80.849248	61.971700
1992.712823	81.038830	61.976705
1992.165754	86.106706	61.981710
1991.503781	68.323271	61.986714
1990.437110	86.476632	61.991719
1989.941596	72.639569	61.996724
1988.996638	77.994179	62.001729
1987.532602	76.217334	62.006734
1987.337675	74.542729	62.011738
1986.819060	85.030791	62.016743
1986.384340	77.406907	62.021748
1986.022718	76.369871	62.026753
1985.437351	82.080193	62.031758
1984.819312	76.235890	62.036762
1983.653110	79.565532	62.041767
1983.163850	82.841350	62.046772
1982.818160	64.316610	62.051777
1981.680075	77.618816	62.056782
1981.043530	70.438391	62.061786
1979.847505	77.367074	62.066791
1980.168714	68.236308	62.071796
1979.918742	72.478916	62.076801
1979.323043	70.792343	62.081806
1978.613391	75.112794	62.086810
1977.103587	79.481307	62.091815
1976.110969	72.525207	62.096820
1975.345231	79.813296	62.101825
1974.652237	80.861815	62.106830
1974.675081	78.985754	62.111834
1974.217849	77.414832	62.116839
1973.650414	77.387572	62.121844
1972.588629	70.879867	62.126849
1971.836723	82.253722	62.131854
1971.183524	74.687345	62.136858
1970.465171	73.452790	62.141863
1969.833994	75.282152	62.146868
1968.751580	74.636827	62.151873
1967.943139	83.109283	62.156878
1967.542904	76.096059	62.161882
1967.030705	79.453166	62.166887
1967.108002	78.067113	62.171892
1966.303666	77.901569	62.176897
1965.647975	78.918051	62.181902
1964.804633	72.434951	62.186906
1963.972163	86.409596	62.191911
1963.299234	76.391425	62.196916
1962.719175	76.836438	62.201921
1961.560578	81.724723	62.206926
1961.094160	77.765335	62.211930
1960.252816	88.205584	62.216935
1960.208406	81.183593	62.221940
1959.922906	83.670244	62.226945
1959.135938	85.330475	62.231950
1958.473962	77.043260	62.236954
1957.629587	76.950880	62.241959
1956.421544	81.667631	62.246964
1955.699203	83.807446	62.251969
1954.940570	78.189296	62.256974
1954.541613	74.382968	62.261978
1953.866222	78.105479	62.266983
1953.753608	72.083543	62.271988
1953.146247	72.646907	62.276993
1951.769047	81.334284	62.281998
1951.347051	76.820214	62.287002
1950.698591	82.990919	62.292007
1950.441826	75.400150	62.297012
1949.170923	72.764521	62.302017
1948.296601	80.867341	62.307022
1947.973358	80.330170	62.312026
1947.232496	84.024016	62.317031
1947.103704	81.794173	62.322036
1946.607013	74.044718	62.327041
1945.560101	80.534626	62.332046
1945.125729	72.043883	62.337050
1944.092924	77.736014	62.342055
1943.887640	72.148336	62.347060
1942.922770	74.664758	62.352065
1941.717181	78.153508	62.357070
1941.702278	69.018269	62.362074
1941.193697	75.743310	62.367079
1939.913885	75.042552	62.372084
1939.349909	74.870236	62.377089
1938.483459	76.376309	62.382094
1938.221796	75.018243	62.387098
1937.774464	82.950919	62.392103
1937.257152	76.366264	62.397108
1936.032634	76.692192	62.402113
1934.742712	78.167291	62.407118
1934.960880	78.346683	62.412122
1934.196037	71.983183	62.417127
1933.895706	75.626536	62.422132
1933.216055	75.148363	62.427137
1931.974436	79.404696	62.432142
1931.633504	81.099545	62.437146
1931.051000	78.111298	62.442151
1930.445641	72.110106	62.447156
1929.840188	73.700606	62.452161
1928.460926	80.749851	62.457166
1928.451768	71.574157	62.462170
1927.896031	78.479760	62.467175
1927.149630	81.538264	62.472180
1926.540724	75.262952	62.477185
1925.746414	84.778611	62.482190
1925.485276	79.009047	62.487194
1924.496653	78.395054	62.492199
1922.869098	79.926730	62.497204
1922.956270	80.148267	62.502209
1922.096947	83.842250	62.507214
1922.029253	74.713672	62.512218
1920.971239	75.321766	62.517223
1920.302633	76.392960	62.522228
1919.439629	77.020981	62.527233
1918.484971	78.988183	62.532238
1918.301462	61.983816	62.537242
1918.152870	71.895037	62.542247
1917.891724	69.715074	62.547252
1916.981878	75.680634	62.552257
1915.849254	76.532010	62.557262
1915.424652	78.195385	62.562266
1913.878428	77.233116	62.567271
1913.397267	78.548155	62.572276
1912.760855	77.751153	62.577281
1911.616802	80.011666	62.582286
1911.640959	72.491657	62.587290
1911.464183	79.700311	62.592295
1911.123157	80.864672	62.597300
1910.071460	80.899341	62.602305
1908.737171	79.442151	62.607310
1908.346858	74.912010	62.612314
1907.815413	71.651359	62.617319
1907.351072	77.295192	62.622324
1906.247175	77.366817	62.627329
1905.508805	75.509668	62.632334
1905.191682	70.992270	62.637338
1904.555861	81.402489	62.642343
1904.157033	72.626604	62.647348
1903.542447	66.086230	62.652353
1902.210818	71.433974	62.657358
1902.241426	70.165247	62.662362
1901.399449	73.461936	62.667367
1900.943981	65.685311	62.672372
1899.919894	62.905635	62.677377
1898.871449	72.353847	62.682382
1898.488198	62.335090	62.687386
1897.600568	74.605677	62.692391
1897.149758	67.879792	62.697396
1896.597210	66.045329	62.702401
1895.803151	76.665765	62.707406
1895.375062	62.960878	62.712410
1894.675074	68.658047	62.717415
1894.183840	68.877880	62.722420
1893.249446	66.318509	62.727425
1892.164824	68.797796	62.732430
1891.929189	64.685654	62.737434
1891.328120	70.345376	62.742439
1891.246556	70.514071	62.747444
1890.118968	80.158189	62.752449
1889.536295	75.678720	62.757454
1888.925134	63.536672	62.762458
1887.921092	73.463980	62.767463
1886.785055	69.634553	62.772468
1886.298310	80.326361	62.777473
1885.368406	76.606925	62.782478
1885.241122	69.162168	62.787482
1884.534539	77.543388	62.792487
1884.673681	78.556133	62.797492
1884.263452	74.169528	62.802497
1882.750247	75.852567	62.807502
1882.451539	70.684678	62.812506
1881.833423	75.833392	62.817511
1880.555246	77.316362	62.822516
1879.724521	76.174069	62.827521
1879.394548	77.190098	62.832526
1878.893755	64.356960	62.837530
1878.203025	73.682006	62.842535
1877.066086	75.437645	62.847540
1876.367786	65.164116	62.852545
1875.951323	83.442280	62.857550
1875.436377	70.781289	62.862554
1875.146697	72.834857	62.867559
1874.445259	76.472229	62.872564
1873.630026	74.559554	62.877569
1872.796474	75.806203	62.882574
1872.939007	69.481688	62.887578
1871.417474	75.908333	62.892583
1870.755972	69.074029	62.897588
1870.143474	66.253549	62.902593
1869.526518	70.757879	62.907598
1869.268856	68.824024	62.912602
1867.753554	69.497335	62.917607
1866.977873	74.146052	62.922612
1866.720025	73.713748	62.927617
1866.332304	82.060551	62.932622
1866.360822	72.376727	62.937626
1864.703912	79.495192	62.942631
1864.232251	67.093238	62.947636
1863.824127	66.545333	62.952641
1862.891469	73.642125	62.957646
1862.518529	64.461181	62.962650
1861.410277	69.752165	62.967655
1860.903620	72.999386	62.972660
1860.566117	76.086227	62.977665
1859.782547	73.958146	62.982670
1858.952882	74.263512	62.987674
1858.041414	74.459325	62.992679
1857.209334	81.104720	62.997684
1857.060619	71.039920	63.002689
1856.446646	80.882344	63.007694
1855.980488	68.671284	63.012698
1854.956049	71.573290	63.017703
1853.953476	74.126965	63.022708
1853.742248	68.714386	63.027713
1853.223528	74.246343	63.032718
1852.432314	68.693788	63.037722
1851.151631	67.479671	63.042727
1850.533665	69.804526	63.047732
1850.344743	69.039918	63.052737
1849.771321	78.568705	63.057742
1849.546750	72.583694	63.062746
1848.768781	70.616098	63.067751
1847.754342	74.286891	63.072756
1847.452415	59.436268	63.077761
1846.612330	67.519416	63.082766
1845.678812	67.391781	63.087770
1844.697004	70.925153	63.092775
1844.055339	74.799791	63.097780
1843.849747	70.009908	63.102785
1843.306906	73.369501	63.107790
1842.126828	63.772067	63.112794
1841.390752	79.053317	63.117799
1840.936386	73.389057	63.122804
1840.610368	65.118605	63.127809
1840.223974	75.014850	63.132814
1839.203617	65.711787	63.137818
1838.286944	61.721692	63.142823
1837.341636	62.769974	63.147828
1837.227143	60.351384	63.152833
1836.521032	75.006609	63.157838
1836.483153	73.592895	63.162842
1835.462199	72.023700	63.167847
1834.133088	69.593448	63.172852
1833.807855	64.035779	63.177857
1832.972242	69.076841	63.182862
1832.887850	65.397099	63.187866
1831.596928	81.193261	63.192871
1830.993143	70.140574	63.197876
1830.473950	68.635925	63.202881
1829.820153	70.332596	63.207886
1829.431142	60.277340	63.212890
1828.352158	65.371881	63.217895
1827.928263	78.318629	63.222900
1827.396781	70.525810	63.227905
1826.796775	79.740607	63.232910
1826.404177	68.900860	63.237914
1825.543835	70.922594	63.242919
1824.783161	73.000694	63.247924
1824.188880	66.999997	63.252929
1822.887884	77.518491	63.257934
1822.133491	69.043840	63.262938
1821.991518	75.103027	63.267943
1821.172653	73.296374	63.272948
1821.276157	71.515854	63.277953
1819.774345	72.888683	63.282958
1818.957676	69.711184	63.287962
1818.620336	70.562300	63.292967
1817.987570	77.916461	63.297972
1817.572261	72.550642	63.302977
1816.800158	78.077007	63.307982
1816.054203	66.888788	63.312986
1815.191039	63.630433	63.317991
1814.925389	68.493460	63.322996
1814.433190	63.616833	63.328001
1813.049775	72.333711	63.333006
1812.654158	72.260888	63.338010
1812.003511	74.982901	63.343015
1811.284970	74.227594	63.348020
1811.191690	65.097887	63.353025
1809.808456	76.772378	63.358030
1809.066999	68.803523	63.363034
1808.445600	73.425060	63.368039
1807.825289	80.407239	63.373044
1808.104785	75.020042	63.378049
1807.137363	76.067771	63.383054
1806.302380	65.448581	63.388058
1805.444462	78.985881	63.393063
1804.834595	76.307058	63.398068
1804.536571	79.436487	63.403073
1803.193680	79.166934	63.408078
1802.523559	74.634944	63.413082
1801.747604	73.189226	63.418087
1801.404060	79.442369	63.423092
1801.410624	72.916128	63.428097
1799.684826	69.429196	63.433102
1798.936441	68.619395	63.438106
1798.339846	76.604841	63.443111
1797.963588	77.058027	63.448116
1797.846899	70.967332	63.453121
1797.352139	81.607617	63.458126
1796.658608	69.254689	63.463130
1795.723594	62.709952	63.468135
1794.963466	73.529049	63.473140
1794.460943	77.012795	63.478145
1793.316869	71.174060	63.483150
1792.581959	73.042106	63.488154
1792.026622	73.031348	63.493159
1791.469595	74.085439	63.498164
1791.477684	73.823157	63.503169
1790.845814	78.098739	63.508174
1789.983309	79.965329	63.513178
1788.966282	83.305799	63.518183
1787.645857	76.671480	63.523188
1787.279017	67.740545	63.528193
1786.710599	74.872521	63.533198
1785.916668	81.185750	63.538202
1785.113760	72.550467	63.543207
1784.953287	77.277084	63.548212
1784.195738	76.650029	63.553217
1784.202831	73.892098	63.558222
1783.970287	79.946651	63.563226
1783.177673	74.008312	63.568231
1781.347152	73.406160	63.573236
1780.175108	70.795898	63.578241
1779.990175	71.982109	63.583246
1780.113078	73.657206	63.588250
1779.085105	70.933877	63.593255
1778.433192	67.337819	63.598260
1778.097706	57.887601	63.603265
1776.863738	82.600624	63.608270
1776.443503	73.025956	63.613274
1775.462900	73.141248	63.618279
1774.896874	75.368017	63.623284
1775.206356	77.457226	63.628289
1773.662766	75.067634	63.633294
1772.957117	72.313235	63.638298
1772.294797	67.288491	63.643303
1772.105183	69.470987	63.648308
1771.071992	62.587806	63.653313
1770.320984	74.135971	63.658318
1769.885172	67.115053	63.663322
1769.688455	65.222092	63.668327
1768.394356	69.177182	63.673332
1767.570070	65.626407	63.678337
1767.045605	70.073078	63.683342
1766.717208	59.457223	63.688346
1765.918355	65.428673	63.693351
1765.336985	74.609096	63.698356
1764.654954	71.788292	63.703361
1763.932620	75.196364	63.708366
1763.517893	69.696249	63.713370
1762.098373	59.436420	63.718375
1760.618820	70.509262	63.723380
1761.290797	61.325992	63.728385
1760.667984	73.223260	63.733390
1759.550756	66.131047	63.738394
1759.221881	63.620463	63.743399
1758.990344	76.284040	63.748404
1757.901537	67.475850	63.753409
1756.640807	70.779471	63.758414
1756.500690	75.192354	63.763418
1756.189015	69.478432	63.768423
1755.296377	74.901483	63.773428
1755.347506	70.369644	63.778433
1753.983225	70.005083	63.783438
1753.177831	66.194905	63.788442
1752.808114	63.063704	63.793447
1751.441346	58.610663	63.798452
1750.784833	63.747793	63.803457
1749.976071	70.844711	63.808462
1749.794181	77.089929	63.813466
1749.364334	64.703348	63.818471
1748.973885	79.165227	63.823476
1748.661021	70.095594	63.828481
1747.392667	74.126808	63.833486
1747.035515	79.957560	63.838490
1746.353726	72.747029	63.843495
1745.211067	77.991028	63.848500
1744.367243	68.007287	63.853505
1743.189455	71.945244	63.858510
1743.148627	67.185598	63.863514
1743.200398	78.578253	63.868519
1742.268958	72.444607	63.873524
1741.751009	62.675495	63.878529
1740.129901	73.060882	63.883534
1740.005785	68.735864	63.888538
1739.550194	71.937646	63.893543
1739.139751	77.174777	63.898548
1738.606303	62.637726	63.903553
1737.592559	70.607314	63.908558
1736.773901	75.922581	63.913562
1735.855471	72.607779	63.918567
1734.759260	75.021580	63.923572
1734.468402	75.063070	63.928577
1733.662216	73.187554	63.933582
1733.346761	66.871545	63.938586
1732.941149	73.867511	63.943591
1732.184360	77.382136	63.948596
1732.254764	71.294169	63.953601
1731.300075	77.298606	63.958606
1730.780478	74.159499	63.963610
1730.002602	70.536845	63.968615
1728.770020	72.638468	63.973620
1728.116188	72.702988	63.978625
1727.424076	74.648190	63.983630
1726.696627	69.647623	63.988634
1725.632570	64.909513	63.993639
1724.645564	79.417810	63.998644
1724.861186	72.530553	64.003649
1724.132605	74.112537	64.008654
1723.666517	66.954707	64.013658
1723.632467	70.773543	64.018663
1722.846092	80.235748	64.023668
1722.021954	67.791115	64.028673
1720.739387	83.925316	64.033678
1720.142870	75.672346	64.038682
1719.291091	72.739679	64.043687
1718.582577	78.803834	64.048692
1718.456182	72.292454	64.053697
1717.809493	77.034374	64.058702
1717.285854	74.334890	64.063706
1715.869452	78.321972	64.068711
1715.338911	79.739024	64.073716
1714.924438	69.613538	64.078721
1714.395996	80.955871	64.083726
1714.315793	76.146121	64.088730
1712.777557	76.597619	64.093735
1711.988939	81.723416	64.098740
1711.766537	74.405078	64.103745
1711.295329	71.454265	64.108750
1710.833415	73.020620	64.113754
1709.359281	69.502896	64.118759
1708.938638	72.789091	64.123764
1708.297077	69.123775	64.128769
1707.752111	70.194363	64.133774
1707.292572	72.379628	64.138778
1706.470418	75.875046	64.143783
1705.596500	78.441862	64.148788
1704.999719	70.380382	64.153793
1704.872739	76.535286	64.158798
1703.467508	68.510304	64.163802
1702.561398	73.786066	64.168807
1702.268280	67.948191	64.173812
1701.978951	63.163178	64.178817
1701.308623	71.464781	64.183822
1700.609765	70.237984	64.188826
1699.823571	68.372869	64.193831
1698.752460	77.468155	64.198836
1698.963608	68.987785	64.203841
1697.648811	81.396212	64.208846
1696.657636	71.392697	64.213850
1696.155849	68.218576	64.218855
1695.509539	65.832179	64.223860
1695.110109	60.270647	64.228865
1694.497184	82.057914	64.233870
1694.424606	75.330493	64.238874
1693.536200	69.048582	64.243879
1692.454562	77.532274	64.248884
1692.204188	65.251962	64.253889
1691.043632	72.888666	64.258894
1690.184552	71.397589	64.263898
1689.453980	62.456285	64.268903
1688.812830	68.983759	64.273908
1688.571790	69.006859	64.278913
1687.916079	77.305964	64.283918
1687.773935	73.184945	64.288922
1686.779280	71.889954	64.293927
1685.538129	74.674736	64.298932
1685.152738	62.954745	64.303937
1684.901256	74.117054	64.308942
1684.246929	72.092410	64.313946
1683.485089	67.914412	64.318951
1682.761809	73.513746	64.323956
1682.656360	74.153880	64.328961
1681.100962	76.507718	64.333966
1680.013374	69.213095	64.338970
1679.583934	65.999362	64.343975
1679.404936	72.613144	64.348980
1679.090489	63.212627	64.353985
1677.768753	65.850942	64.358990
1677.045730	68.063927	64.363994
1676.578574	68.241372	64.368999
1676.040157	68.220625	64.374004
1675.868878	60.516986	64.379009
1674.418707	67.153687	64.384014
1673.781968	62.750611	64.389018
1673.434490	67.960388	64.394023
1672.517730	64.489796	64.399028
1672.651302	62.584137	64.404033
1671.551781	66.614893	64.409038
1670.517543	71.584571	64.414042
1669.960535	54.364323	64.419047
1669.285341	72.151877	64.424052
1668.782633	64.058917	64.429057
1667.773258	75.521038	64.434062
1666.614407	71.062441	64.439066
1666.637213	66.845308	64.444071
1666.146870	73.536050	64.449076
1666.356276	65.861606	64.454081
1664.880761	72.934867	64.459086
1663.974414	66.080138	64.464090
1663.623386	63.518092	64.469095
1663.199273	72.096893	64.474100
1662.340173	60.523492	64.479105
1660.954087	76.081351	64.484110
1660.641712	69.692194	64.489114
1660.011070	68.087035	64.494119
1659.536144	73.514799	64.499124
1659.257521	62.393097	64.504129
1658.189414	73.067933	64.509134
1657.237553	64.125820	64.514138
1656.824331	70.411803	64.519143
1655.972295	68.713087	64.524148
1655.654400	61.970420	64.529153
1654.782248	68.810966	64.534158
1653.707337	70.594716	64.539162
1653.188638	73.173382	64.544167
1652.842519	74.563223	64.549172
1652.672633	68.499801	64.554177
1651.866611	69.418890	64.559182
1651.067898	62.907705	64.564186
1650.467901	62.371337	64.569191
1649.686199	73.987912	64.574196
1648.883965	57.467234	64.579201
1647.718707	68.917345	64.584206
1647.211381	66.858867	64.589210
1646.780293	60.680285	64.594215
1646.124418	61.043573	64.599220
1645.704667	60.607014	64.604225
1645.281277	70.011049	64.609230
1644.160960	67.157506	64.614234
1643.717475	68.900705	64.619239
1643.121730	70.767849	64.624244
1642.747837	64.918937	64.629249
1641.626171	63.204000	64.634254
1640.807866	70.722145	64.639258
1640.444257	67.769113	64.644263
1639.652814	65.392956	64.649268
1639.268341	60.510552	64.654273
1638.284656	62.226196	64.659278
1637.152896	64.529655	64.664282
1637.100160	65.158796	64.669287
1636.243314	71.088080	64.674292
1636.255867	65.062913	64.679297
1634.790340	70.376782	64.684302
1633.903998	60.592975	64.689306
1633.752760	63.564266	64.694311
1633.329513	64.505878	64.699316
1632.809353	63.968481	64.704321
1631.676063	68.034627	64.709326
1630.842737	61.035576	64.714330
1630.852008	64.226889	64.719335
1629.645984	65.436658	64.724340
1628.985502	56.019978	64.729345
1627.655020	60.124209	64.734350
1627.436508	65.496250	64.739354
1626.575559	57.502498	64.744359
1626.322498	75.659507	64.749364
1626.406704	62.908682	64.754369
1625.918407	68.235711	64.759374
1624.590818	73.162442	64.764378
1623.565141	64.746501	64.769383
1623.063622	75.935017	64.774388
1622.977902	66.978503	64.779393
1621.923572	68.491117	64.784398
1620.879810	63.414050	64.789402
1620.317543	57.423703	64.794407
1619.789938	70.807372	64.799412
1620.079371	57.257651	64.804417
1618.740632	59.178919	64.809422
1617.837366	70.951289	64.814426
1617.188626	58.032225	64.819431
1616.918835	70.603651	64.824436
1615.905760	60.656808	64.829441
1614.946660	66.083745	64.834446
1614.422532	61.372473	64.839450
1614.228152	70.170895	64.844455
1613.379864	64.463167	64.849460
1612.653045	52.763339	64.854465
1611.995686	70.105354	64.859470
1611.178004	68.915483	64.864474
1611.010829	67.452457	64.869479
1609.643962	69.862863	64.874484
1608.919017	66.013684	64.879489
1608.624275	70.421051	64.884494
1608.158626	73.951390	64.889498
1607.564870	72.129540	64.894503
1606.591986	73.857157	64.899508
1605.584290	63.040222	64.904513
1605.205705	67.285891	64.909518
1605.124551	67.952657	64.914522
1604.590477	68.695747	64.919527
1603.138951	73.983940	64.924532
1602.418016	66.198719	64.929537
1601.908560	66.626162	64.934542
1601.394226	72.589201	64.939546
1600.913853	67.301256	64.944551
1599.871020	76.716566	64.949556
1599.185252	69.245444	64.954561
1598.566607	67.316545	64.959566
1598.095786	71.892986	64.964570
1597.997245	68.361330	64.969575
1596.541481	69.926858	64.974580
1595.888468	63.313387	64.979585
1595.034186	70.816773	64.984590
1594.772420	73.739483	64.989594
1594.433552	58.569990	64.994599
1593.303682	73.364038	64.999604
1592.664339	66.582444	65.004609
1592.183811	69.727319	65.009614
1591.804081	73.203483	65.014618
1591.290268	76.317347	65.019623
1589.922938	79.447807	65.024628
1589.317756	72.237225	65.029633
1588.894146	73.177324	65.034638
1588.058023	64.688693	65.039642
1587.240241	67.447619	65.044647
1585.988777	69.694998	65.049652
1585.902326	61.147547	65.054657
1585.613595	69.956587	65.059662
1585.278861	69.861915	65.064666
1585.239663	63.113009	65.069671
1583.742457	68.167453	65.074676
1582.922234	60.291868	65.079681
1582.101818	58.954450	65.084686
1581.602179	58.128560	65.089690
1580.289247	56.355979	65.094695
1579.398462	59.641322	65.099700
1579.532403	55.561880	65.104705
1579.068831	64.277291	65.109710
1578.400721	56.269892	65.114714
1578.002999	61.414059	65.119719
1576.495146	71.781675	65.124724
1575.972225	61.205853	65.129729
1575.477155	68.510798	65.134734
1574.673959	61.453712	65.139738
1574.535285	67.824545	65.144743
1574.032969	66.013893	65.149748
1573.286574	65.322596	65.154753
1572.473215	70.427770	65.159758
1572.051652	71.131872	65.164762
1571.077211	67.117775	65.169767
1569.689291	68.807088	65.174772
1569.203281	62.571603	65.179777
1568.816084	61.473456	65.184782
1568.659507	66.270843	65.189786
1568.516509	58.978807	65.194791
1567.060324	64.280038	65.199796
1566.523623	57.171823	65.204801
1566.272042	69.023711	65.209806
1565.006355	64.653292	65.214810
1564.415568	62.461879	65.219815
1563.661601	66.899680	65.224820
1563.158093	66.919153	65.229825
1561.820001	60.605292	65.234830
1560.926880	61.423647	65.239834
1560.948098	59.312226	65.244839
1560.029224	63.808248	65.249844
1560.359521	66.294910	65.254849
1559.547106	59.775435	65.259854
1558.346073	58.569868	65.264858
1557.825661	61.723148	65.269863
1556.801014	63.055833	65.274868
1556.876101	54.806781	65.279873
1556.314910	57.621660	65.284878
1554.872988	62.867956	65.289882
1554.774761	65.722810	65.294887
1554.237802	70.230049	65.299892
1553.234264	64.090241	65.304897
1552.253797	67.722896	65.309902
1550.981480	64.454489	65.314906
1551.032960	57.229432	65.319911
1550.386555	63.451113	65.324916
1550.107467	60.074303	65.329921
1549.689145	66.206033	65.334926
1548.189786	61.383790	65.339930
1547.858153	57.927161	65.344935
1547.053279	60.484153	65.349940
1546.626624	56.507363	65.354945
1546.296507	58.593517	65.359950
1545.165932	64.254668	65.364954
1544.302523	58.712171	65.369959
1543.831731	63.574384	65.374964
1543.480083	56.360295	65.379969
1542.714067	56.238783	65.384974
1541.797209	60.544996	65.389978
1541.134860	51.749156	65.394983
1540.555966	55.647017	65.399988
1540.362860	51.863933	65.404993
1539.236248	57.492038	65.409998
1538.621601	60.129760	65.415002
1537.911357	59.896866	65.420007
1537.240213	68.810822	65.425012
1536.801816	62.526144	65.430017
1535.713290	61.092915	65.435022
1534.813327	63.480270	65.440026
1534.785961	63.886395	65.445031
1534.182677	70.193459	65.450036
1533.570214	62.014314	65.455041
1532.516285	62.497842	65.460046
1531.853488	59.601948	65.465050
1531.290636	59.696709	65.470055
1531.022982	62.810680	65.475060
1530.285240	54.966782	65.480065
1528.902570	61.504726	65.485070
1528.074152	63.184342	65.490074
1528.140782	61.148041	65.495079
1527.386603	66.048887	65.500084
1526.842983	61.218207	65.505089
1526.607254	65.652183	65.510094
1525.667464	59.485290	65.515098
1524.590109	65.115627	65.520103
1524.085476	70.819650	65.525108
1523.662479	63.078980	65.530113
1522.559163	61.008446	65.535118
1521.844016	59.128836	65.540122
1521.439017	47.755257	65.545127
1520.458048	59.794331	65.550132
1520.318572	56.694011	65.555137
1519.606732	63.893956	65.560142
1518.335575	57.797198	65.565146
1518.103138	67.598397	65.570151
1517.465231	63.377907	65.575156
1517.418721	59.068440	65.580161
1516.366777	65.387556	65.585166
1515.240368	63.437812	65.590170
1514.610119	62.695464	65.595175
1514.292922	64.112728	65.600180
1513.739311	61.756282	65.605185
1513.307188	59.943097	65.610190
1512.389480	67.432477	65.615194
1511.982377	61.256915	65.620199
1510.359244	68.086271	65.625204
1509.888906	63.303049	65.630209
1509.396411	65.680274	65.635214
1508.419108	70.362349	65.640218
1508.721806	64.425289	65.645223
1508.214060	71.820823	65.650228
1507.282470	56.240056	65.655233
1506.426888	67.358508	65.660238
1505.314940	62.065783	65.665242
1504.329093	56.363469	65.670247
1503.797833	69.620263	65.675252
1503.750972	63.949074	65.680257
1502.918491	61.273663	65.685262
1502.344883	68.409691	65.690266
1502.281743	53.744062	65.695271
1500.895552	59.874474	65.700276
1500.480917	71.207580	65.705281
1499.766305	60.571034	65.710286
1499.203146	71.071440	65.715290
1497.645038	66.091907	65.720295
1496.797557	64.479675	65.725300
1497.003133	60.486654	65.730305
1495.954812	55.797621	65.735310
1495.475927	68.038522	65.740314
1495.362410	56.207309	65.745319
1495.034243	66.804855	65.750324
1494.334796	58.827704	65.755329
1493.054758	62.815968	65.760334
1492.713729	70.534662	65.765338
1491.990060	63.207416	65.770343
1491.049935	67.831026	65.775348
1490.741156	55.243401	65.780353
1489.847616	60.064290	65.785358
1488.362581	62.869143	65.790362
1487.940528	59.477335	65.795367
1487.069907	64.038525	65.800372
1486.795873	57.209037	65.805377
1486.264207	56.375613	65.810382
1485.822864	54.275076	65.815386
1485.817590	62.629823	65.820391
1485.211735	62.472618	65.825396
1483.969075	58.361957	65.830401
1483.210137	67.939069	65.835406
1482.463554	66.070766	65.840410
1481.725722	63.021939	65.845415
1480.582446	67.746239	65.850420
1479.971284	63.925765	65.855425
1479.747952	62.466437	65.860430
1479.412316	63.584898	65.865434
1478.916731	57.501062	65.870439
1477.903228	59.149603	65.875444
1477.125302	62.605110	65.880449
1476.381549	56.829395	65.885454
1475.754625	66.968097	65.890458
1475.596338	66.479302	65.895463
1474.396132	73.449827	65.900468
1473.705734	66.810410	65.905473
1473.162531	68.423457	65.910478
1472.603107	72.225630	65.915482
1472.139139	68.225234	65.920487
1471.178594	66.055279	65.925492
1470.141375	67.724065	65.930497
1469.747024	67.463955	65.935502
1468.967428	68.727874	65.940506
1468.810608	66.539562	65.945511
1468.346899	68.671874	65.950516
1467.149934	66.311079	65.955521
1466.693347	67.802727	65.960526
1466.199018	70.831557	65.965530
1465.689884	60.033936	65.970535
1464.763914	74.857433	65.975540
1464.010174	60.598150	65.980545
1463.484950	68.616779	65.985550
1462.510586	69.930219	65.990554
1461.935155	65.380902	65.995559
1461.147575	73.189448	66.000564
1460.652763	68.249769	66.005569
1460.377604	68.586206	66.010574
1459.474835	64.356193	66.015578
1458.420869	57.189696	66.020583
1457.670129	62.800453	66.025588
1457.485580	64.303958	66.030593
1457.121595	64.760988	66.035598
1456.498685	64.908666	66.040602
1455.440308	58.627884	66.045607
1454.644701	64.337501	66.050612
1454.100021	55.343521	66.055617
1453.423030	61.351768	66.060622
1452.159328	66.242730	66.065626
1452.039015	64.114879	66.070631
1451.407001	62.105793	66.075636
1450.869641	58.013758	66.080641
1450.763209	58.958392	66.085646
1449.363921	62.354471	66.090650
1449.016348	58.712300	66.095655
1448.074244	61.548176	66.100660
1447.872136	58.945269	66.105665
1446.767928	61.155237	66.110670
1445.478926	73.039427	66.115674
1445.066689	55.681576	66.120679
1444.830868	69.888018	66.125684
1444.283764	64.146146	66.130689
1443.884897	59.278073	66.135694
1442.786469	67.461914	66.140698
1442.158197	57.569257	66.145703
1441.082008	66.884502	66.150708
1440.776558	69.478391	66.155713
1440.819006	60.604170	66.160718
1439.282539	68.034867	66.165722
1438.863435	62.636202	66.170727
1438.119438	70.899900	66.175732
1438.052835	67.888948	66.180737
1436.733203	72.275958	66.185742
1435.883104	76.235645	66.190746
1435.426178	63.866400	66.195751
1434.928915	63.937314	66.200756
1434.472169	60.179625	66.205761
1433.879029	55.556377	66.210766
1432.526670	65.622675	66.215770
1432.154698	56.548614	66.220775
1431.633374	71.157196	66.225780
1431.003199	70.746409	66.230785
1430.603545	64.035923	66.235790
1429.533557	68.770582	66.240794
1428.965820	55.707843	66.245799
1428.140709	59.283531	66.250804
1428.323279	59.333210	66.255809
1426.906192	62.454065	66.260814
1425.802288	64.303607	66.265818
1425.479862	60.119132	66.270823
1424.642425	65.458956	66.275828
1424.622299	67.807832	66.280833
1424.497952	64.776371	66.285838
1422.956881	74.170009	66.290842
1422.449682	63.097735	66.295847
1421.604047	65.651854	66.300852
1421.036892	64.682412	66.305857
1420.387977	61.162476	66.310862
1419.405677	62.735822	66.315866
1418.807042	66.987189	66.320871
1418.603082	66.069655	66.325876
1418.056322	64.765948	66.330881
1416.835461	58.952705	66.335886
1416.095416	68.001611	66.340890
1415.352587	63.407142	66.345895
1414.927162	62.880789	66.350900
1414.805685	60.532096	66.355905
1414.466446	58.585793	66.360910
1413.294185	75.414778	66.365914
1412.545128	57.527245	66.370919
1411.939920	62.517465	66.375924
1411.314164	65.065132	66.380929
1410.382134	62.092187	66.385934
1409.663312	70.610513	66.390938
1409.345471	60.258956	66.395943
1408.817328	64.397604	66.400948
1407.834149	58.823930	66.405953
1407.122247	63.345331	66.410958
1406.233878	67.816416	66.415962
1406.313271	70.544950	66.420967
1405.005891	63.903792	66.425972
1403.953068	66.206417	66.430977
1403.637666	65.101915	66.435982
1403.376922	71.164047	66.440986
1402.925408	66.429720	66.445991
1402.279522	68.609798	66.450996
1401.312878	72.385368	66.456001
1400.303392	72.347392	66.461006
1399.737126	76.442835	66.466010
1399.405000	67.475631	66.471015
1398.755364	74.377585	66.476020
1397.669113	67.620818	66.481025
1396.679685	65.702916	66.486030
1396.431738	69.407175	66.491034
1395.949030	67.181496	66.496039
1395.457420	71.655325	66.501044
1395.032997	71.134723	66.506049
1394.024579	67.022277	66.511054
1393.232404	69.709743	66.516058
1392.678601	62.708689	66.521063
1392.424343	71.633790	66.526068
1391.203152	73.603675	66.531073
1390.757847	63.911013	66.536078
1389.435664	68.274786	66.541082
1389.125245	65.534113	66.546087
1388.899204	74.542012	66.551092
1388.088879	71.581395	66.556097
1387.147172	68.712738	66.561102
1386.258499	67.357434	66.566106
1386.084563	58.837218	66.571111
1385.752682	70.603763	66.576116
1384.911810	67.296287	66.581121
1384.092136	62.262236	66.586126
1383.107911	63.206342	66.591130
1383.188047	63.190268	66.596135
1382.357475	64.464109	66.601140
1381.064160	68.558086	66.606145
1380.375097	70.087561	66.611150
1379.838425	64.975858	66.616154
1379.808584	63.112380	66.621159
1379.080498	68.705848	66.626164
1378.225502	69.016809	66.631169
1377.351953	64.754578	66.636174
1376.835188	72.586244	66.641178
1376.629585	59.922954	66.646183
1375.435736	69.183746	66.651188
1374.388391	69.950772	66.656193
1373.950349	59.482435	66.661198
1373.491008	60.997454	66.666202
1373.115483	56.792865	66.671207
1372.412354	60.569512	66.676212
1371.466048	60.660458	66.681217
1371.395862	63.247232	66.686222
1370.265503	67.325554	66.691226
1369.242397	63.403516	66.696231
1368.551210	70.649277	66.701236
1367.865809	66.871133	66.706241
1367.348532	65.905001	66.711246
1367.135929	61.482664	66.716250
1366.846739	65.735930	66.721255
1365.725992	70.819535	66.726260
1364.563553	72.467936	66.731265
1364.347730	65.705072	66.736270
1363.777824	69.716273	66.741274
1362.933258	60.859296	66.746279
1361.683629	66.595722	66.751284
1361.064351	67.512097	66.756289
1360.675544	66.461609	66.761294
1360.368065	71.595073	66.766298
1360.156467	65.943409	66.771303
1359.472728	72.518059	66.776308
1358.350318	80.806675	66.781313
1358.025899	68.260821	66.786318
1357.061423	73.386754	66.791322
1356.257875	62.857437	66.796327
1355.625122	65.907994	66.801332
1355.058742	67.423182	66.806337
1354.823145	68.776751	66.811342
1353.165245	71.423739	66.816346
1352.812122	71.433674	66.821351
1352.125403	80.072427	66.826356
1352.319992	72.582101	66.831361
1351.565115	64.746698	66.836366
1349.970029	75.646765	66.841370
1348.961830	63.292962	66.846375
1348.325585	74.698733	66.851380
1348.044596	72.713648	66.856385
1347.861385	62.216297	66.861390
1347.236524	65.558385	66.866394
1347.082130	67.550129	66.871399
1346.069782	71.615360	66.876404
1345.468322	71.913320	66.881409
1344.688757	68.390104	66.886414
1342.958488	72.484680	66.891418
1342.486574	78.267187	66.896423
1342.296468	72.475665	66.901428
1341.789008	71.049982	66.906433
1341.106601	61.667117	66.911438
1340.784739	67.780364	66.916442
1340.109715	59.887089	66.921447
1339.295753	72.584011	66.926452
1338.526192	62.155456	66.931457
1338.087651	61.876080	66.936462
1337.173647	71.062528	66.941466
1336.294854	66.610159	66.946471
1335.733889	65.135218	66.951476
1335.034743	70.072845	66.956481
1334.900111	62.958208	66.961486
1333.905158	66.994410	66.966490
1333.165093	59.964467	66.971495
1332.537034	67.521513	66.976500
1332.055948	71.446463	66.981505
1331.677825	61.512983	66.986510
1330.691952	70.580292	66.991514
1329.474082	64.973394	66.996519
1329.086055	61.319608	67.001524
1328.924493	62.756420	67.006529
1327.755020	59.165751	67.011534
1326.428943	67.748953	67.016538
1326.107669	60.179580	67.021543
1325.558726	61.416666	67.026548
1324.955905	72.068328	67.031553
1325.157638	67.317709	67.036558
1324.486846	69.360354	67.041562
1323.999444	59.263618	67.046567
1322.967249	64.987302	67.051572
1322.152857	55.351525	67.056577
1320.674408	61.364748	67.061582
1319.860630	62.796374	67.066586
1320.011507	54.683964	67.071591
1319.618904	69.270108	67.076596
1319.177998	63.525078	67.081601
1318.636054	58.183380	67.086606
1317.382723	61.724234	67.091610
1316.936831	56.985408	67.096615
1316.453121	63.817117	67.101620
1314.905585	67.502674	67.106625
1314.110992	66.249694	67.111630
1313.482880	66.663926	67.116634
1313.337730	62.034266	67.121639
1312.581217	66.213592	67.126644
1312.222239	60.418225	67.131649
1312.250295	51.999621	67.136654
1310.423686	61.568859	67.141658
1310.188650	64.398580	67.146663
1309.452553	65.647181	67.151668
1308.906291	61.707868	67.156673
1308.330106	61.876775	67.161678
1307.560696	69.350656	67.166682
1306.960645	59.152029	67.171687
1306.253914	71.815595	67.176692
1305.112759	65.498104	67.181697
1304.594802	64.217900	67.186702
1303.820821	66.819765	67.191706
1303.682896	66.484984	67.196711
1303.417906	60.049873	67.201716
1302.107392	66.175267	67.206721
1301.408796	61.156033	67.211726
1300.505225	66.349304	67.216730
1300.402022	60.586728	67.221735
1299.805927	65.590396	67.226740
1298.408907	69.721485	67.231745
1298.040023	64.535681	67.236750
1297.565233	71.420337	67.241754
1297.141509	70.260575	67.246759
1296.578728	66.111732	67.251764
1295.467333	71.028755	67.256769
1295.237617	63.448448	67.261774
1294.111222	72.567843	67.266778
1293.865676	67.251192	67.271783
1292.354911	70.191548	67.276788
1291.952897	74.620047	67.281793
1291.486759	68.802762	67.286798
1290.670166	64.592376	67.291802
1290.627703	62.332000	67.296807
1289.761276	67.417867	67.301812
1288.274752	68.028788	67.306817
1288.028201	65.920976	67.311822
1287.253878	65.598040	67.316826
1287.039106	59.492608	67.321831
1286.869389	71.686497	67.326836
1286.182876	60.649689	67.331841
1285.255523	55.218458	67.336846
1284.558980	62.010816	67.341850
1283.755573	66.587760	67.346855
1283.133933	63.505262	67.351860
1282.063450	59.560569	67.356865
1281.801612	58.342308	67.361870
1281.030279	72.446603	67.366874
1280.519336	66.289244	67.371879
1279.344771	66.124429	67.376884
1278.585563	67.075425	67.381889
1278.326679	79.478785	67.386894
1277.803858	72.654805	67.391898
1277.538790	64.500711	67.396903
1276.308779	67.963375	67.401908
1275.723967	71.498737	67.406913
1275.126790	68.965052	67.411918
1274.574722	73.555021	67.416922
1273.961511	56.759755	67.421927
1272.962451	64.314002	67.426932
1272.044234	68.958758	67.431937
1271.653264	61.541055	67.436942
1271.326380	67.218209	67.441946
1270.789502	64.157121	67.446951
1269.871001	68.524045	67.451956
1268.645024	63.754567	67.456961
1268.670085	61.540656	67.461966
1267.961348	70.992744	67.466970
1266.810690	66.710479	67.471975
1266.279978	65.217737	67.476980
1265.535021	70.675557	67.481985
1265.313244	55.922657	67.486990
1264.716633	69.220627	67.491994
1264.161308	69.374521	67.496999
1263.156473	71.159770	67.502004
1261.927487	71.723452	67.507009
1262.153394	66.118077	67.512014
1261.556930	70.455922	67.517018
1260.986607	62.616972	67.522023
1259.674385	69.854589	67.527028
1259.215793	64.810457	67.532033
1258.628167	65.351179	67.537038
1257.764193	67.877278	67.542042
1256.899674	66.797324	67.547047
1256.081753	66.749870	67.552052
1255.503171	62.576899	67.557057
1255.239078	58.781910	67.562062
1254.849107	66.118996	67.567066
1254.636656	60.224739	67.572071
1253.688155	68.931201	67.577076
1252.494006	72.021038	67.582081
1252.310536	69.487580	67.587086
1251.155614	71.152875	67.592090
1250.133147	65.116645	67.597095
1249.347422	64.002678	67.602100
1248.914276	62.245352	67.607105
1248.908317	61.253668	67.612110
1248.052390	69.765080	67.617114
1247.907111	64.101285	67.622119
1246.550409	72.976312	67.627124
1245.744532	71.064122	67.632129
1245.483290	61.903242	67.637134
1245.052902	66.284494	67.642138
1244.137592	58.551187	67.647143
1243.270222	66.809963	67.652148
1241.926150	73.117162	67.657153
1242.079616	72.923934	67.662158
1241.968993	68.112717	67.667162
1241.370755	63.422085	67.672167
1240.580353	63.604780	67.677172
1239.455031	67.857122	67.682177
1238.541589	62.135769	67.687182
1237.595717	68.273351	67.692186
1236.882314	58.320321	67.697191
1236.408532	59.985842	67.702196
1236.225625	64.386696	67.707201
1236.080440	62.446262	67.712206
1235.264867	68.801921	67.717210
1234.281193	59.371980	67.722215
1233.701412	69.723263	67.727220
1232.779852	63.441222	67.732225
1232.171329	62.664403	67.737230
1231.017789	62.871376	67.742234
1230.540856	59.212692	67.747239
1230.071040	62.756787	67.752244
1229.900104	68.044497	67.757249
1229.213823	64.626117	67.762254
1227.753035	58.504683	67.767258
1227.633647	66.341733	67.772263
1227.343716	61.332676	67.777268
1226.078499	61.893886	67.782273
1225.369121	54.075596	67.787278
1224.416570	69.005479	67.792282
1224.017634	65.748685	67.797287
1223.645489	61.095924	67.802292
1223.325516	69.797804	67.807297
1222.568378	57.200944	67.812302
1221.028483	61.056919	67.817306
1220.458651	58.130554	67.822311
1220.125961	61.450656	67.827316
1219.708717	63.326357	67.832321
1219.362129	56.658530	67.837326
1218.236738	63.390899	67.842330
1217.628929	65.276332	67.847335
1217.041290	70.052386	67.852340
1216.102551	69.624984	67.857345
1215.865504	58.809257	67.862350
1214.739392	71.768034	67.867354
1214.002675	67.961204	67.872359
1213.617341	65.217979	67.877364
1213.109071	73.262920	67.882369
1212.722724	68.024460	67.887374
1211.438911	67.218396	67.892378
1210.669421	67.968277	67.897383
1210.095068	66.275391	67.902388
1209.543125	73.331541	67.907393
1209.272255	63.980480	67.912398
1208.860815	67.704443	67.917402
1207.713155	61.684923	67.922407
1207.871576	70.735141	67.927412
1206.240435	73.200759	67.932417
1205.782098	61.584537	67.937422
1205.045481	61.148189	67.942426
1204.380749	58.285046	67.947431
1204.073787	59.116785	67.952436
1202.791853	69.305268	67.957441
1202.147390	64.330071	67.962446
1201.185670	65.172467	67.967450
1200.682439	62.488901	67.972455
1200.755292	59.012790	67.977460
1199.915963	63.559974	67.982465
1199.710941	52.798373	67.987470
1198.583543	73.258587	67.992474
1198.198028	68.057485	67.997479
1197.453056	59.644532	68.002484
1195.907467	68.619401	68.007489
1195.085359	60.493983	68.012494
1194.476898	58.746548	68.017498
1194.526135	59.559932	68.022503
1194.207833	59.134068	68.027508
1193.380992	66.739757	68.032513
1193.018713	62.433057	68.037518
1192.010618	69.064828	68.042522
1191.346394	65.423609	68.047527
1190.951366	61.678280	68.052532
1189.705447	73.154092	68.057537
1189.070697	65.426838	68.062542
1188.407664	68.585222	68.067546
1188.163452	70.415907	68.072551
1187.620253	70.208934	68.077556
1186.262778	74.805757	68.082561
1185.842939	62.911381	68.087566
1185.239430	69.954650	68.092570
1185.041427	58.543324	68.097575
1183.704267	57.263267	68.102580
1182.822838	64.358063	68.107585
1182.481766	57.947047	68.112590
1181.751281	73.035484	68.117594
1181.330706	65.133807	68.122599
1181.511622	65.866622	68.127604
1179.953997	66.513431	68.132609
1179.679180	58.453782	68.137614
1178.552919	58.266510	68.142618
1177.475759	56.220396	68.147623
1176.434345	61.058747	68.152628
1176.835474	57.691425	68.157633
1176.013957	52.874044	68.162638
1175.558030	67.596142	68.167642
1174.517936	60.653522	68.172647
1174.315250	69.537809	68.177652
1173.508862	71.041215	68.182657
1172.535325	57.444890	68.187662
1171.943728	65.413310	68.192666
1171.848904	64.142382	68.197671
1170.896147	60.434522	68.202676
1169.581047	65.031591	68.207681
1169.087341	53.492092	68.212686
1168.747650	65.426133	68.217690
1168.634839	60.129402	68.222695
1167.725976	59.841361	68.227700
1166.585482	67.787714	68.232705
1166.314584	63.132624	68.237710
1165.721334	66.421555	68.242714
1164.834392	66.520927	68.247719
1164.193107	61.530589	68.252724
1163.529039	66.797339	68.257729
1162.989003	55.701146	68.262734
1161.540849	62.083016	68.267738
1160.918015	67.328892	68.272743
1160.737988	61.333571	68.277748
1159.931133	69.157278	68.282753
1160.221245	64.197329	68.287758
1159.304476	74.098705	68.292762
1158.183251	67.682717	68.297767
1157.855372	70.134015	68.302772
1156.992240	64.649581	68.307777
1156.392112	66.834875	68.312782
1155.436824	73.454059	68.317786
1154.972903	66.868691	68.322791
1154.427552	71.121218	68.327796
1153.502791	70.520127	68.332801
1152.738680	64.942954	68.337806
1151.432091	68.855315	68.342810
1150.605200	70.097378	68.347815
1150.828917	68.086285	68.352820
1150.074470	67.473403	68.357825
1149.826183	62.738263	68.362830
1149.608367	73.909767	68.367834
1148.613990	72.857593	68.372839
1148.053331	66.998492	68.377844
1146.859282	65.665127	68.382849
1145.779204	60.666637	68.387854
1144.885793	61.807990	68.392858
1145.003997	73.623769	68.397863
1144.302676	64.701271	68.402868
1143.512519	63.136524	68.407873
1143.302522	56.425584	68.412878
1142.699101	67.015375	68.417882
1141.364306	65.950045	68.422887
1141.175095	63.540335	68.427892
1140.105197	67.957671	68.432897
1140.097641	58.065380	68.437902
1138.963963	65.700321	68.442906
1137.892045	61.831301	68.447911
1137.430923	65.422069	68.452916
1137.044908	70.205446	68.457921
1136.866577	65.263338	68.462926
1135.685545	73.096250	68.467930
1134.579508	65.977045	68.472935
1134.201657	59.971391	68.477940
1133.669885	63.171249	68.482945
1133.753126	59.554026	68.487950
1132.573490	60.748336	68.492954
1131.677627	61.066731	68.497959
1131.572943	55.262190	68.502964
1131.083689	63.816215	68.507969
1129.871747	47.364296	68.512974
1128.828240	62.918799	68.517978
1128.464174	49.063413	68.522983
1128.487899	54.609481	68.527988
1126.773324	57.816081	68.532993
1126.214935	60.388554	68.537998
1125.875143	65.501498	68.543002
1125.130422	57.764672	68.548007
1124.598723	54.606015	68.553012
1123.376928	65.842842	68.558017
1122.832761	53.009822	68.563022
1122.045390	55.827543	68.568026
1121.625775	56.235307	68.573031
1121.475563	66.343307	68.578036
1120.759214	67.837224	68.583041
1119.848357	59.891224	68.588046
1119.175844	53.654200	68.593050
1118.385702	50.499140	68.598055
1118.056108	54.568676	68.603060
1117.226399	56.240679	68.608065
1116.599211	49.976555	68.613070
1115.779904	63.502901	68.618074
1114.971781	53.077463	68.623079
1115.134013	58.321145	68.628084
1114.163582	61.654137	68.633089
1112.977418	60.519158	68.638094
1112.442981	62.329279	68.643098
1111.687441	61.962104	68.648103
1111.584899	59.415983	68.653108
1110.773685	62.448569	68.658113
1109.877250	62.266564	68.663118
1109.008941	54.655899	68.668122
1108.395579	55.735886	68.673127
1108.466290	59.560837	68.678132
1107.635008	65.375276	68.683137
1106.417549	58.448442	68.688142
1106.013446	62.930588	68.693146
1105.144574	61.360774	68.698151
1105.066665	51.761970	68.703156
1103.819999	55.586318	68.708161
1103.455927	55.277635	68.713166
1102.775898	64.187599	68.718170
1102.527411	59.413027	68.723175
1101.310729	52.770656	68.728180
1100.234424	61.246787	68.733185
1099.864750	54.164135	68.738190
1099.718408	57.789421	68.743194
1099.243476	56.418589	68.748199
1098.117664	58.886917	68.753204
1097.006388	63.198455	68.758209
1096.551485	54.338380	68.763214
1095.702406	52.183367	68.768218
1095.947241	57.483558	68.773223
1095.173739	56.389629	68.778228
1093.456536	55.231117	68.783233
1093.459585	54.178685	68.788238
1092.879993	63.969039	68.793242
1092.387770	61.101243	68.798247
1091.460227	58.144179	68.803252
1090.359854	65.418573	68.808257
1090.110284	66.821515	68.813262
1089.533146	63.037909	68.818266
1088.984223	70.098281	68.823271
1088.429358	63.437713	68.828276
1087.104893	63.021125	68.833281
1086.641900	54.167174	68.838286
1086.243269	61.385351	68.843290
1085.875103	62.216130	68.848295
1084.819585	62.382274	68.853300
1083.989213	68.311029	68.858305
1083.408046	60.385950	68.863310
1082.848433	66.626350	68.868314
1082.658579	68.549172	68.873319
1081.493863	60.695991	68.878324
1080.240811	63.077958	68.883329
1080.127609	59.831068	68.888334
1079.618574	64.155533	68.893338
1079.446194	66.360743	68.898343
1078.826526	59.941395	68.903348
1077.184603	69.698143	68.908353
1077.108474	58.833964	68.913358
1076.353703	64.776219	68.918362
1075.088497	62.098808	68.923367
1074.582185	61.271746	68.928372
1073.831661	65.066012	68.933377
1073.614203	60.599141	68.938382
1073.178386	61.147439	68.943386
1072.957771	61.020631	68.948391
1072.089543	59.562024	68.953396
1070.974683	63.098166	68.958401
1070.406970	55.480247	68.963406
1069.826439	56.086087	68.968410
1068.849410	62.531771	68.973415
1068.136731	58.658095	68.978420
1067.237853	67.977361	68.983425
1067.097416	53.670423	68.988430
1067.201002	63.823374	68.993434
1065.866117	63.314238	68.998439
1064.997784	54.773635	69.003444
1064.226220	64.963159	69.008449
1063.541994	50.842493	69.013454
1062.930213	59.670905	69.018458
1061.749468	66.787759	69.023463
1061.312454	60.853427	69.028468
1060.659217	68.407691	69.033473
1060.520300	62.361922	69.038478
1060.280276	64.391620	69.043482
1059.643214	63.436956	69.048487
1058.517381	59.581532	69.053492
1057.776055	68.717907	69.058497
1057.393198	65.183655	69.063502
1056.514751	66.268780	69.068506
1055.274514	62.993050	69.073511
1054.798050	60.334128	69.078516
1054.126944	67.036889	69.083521
1053.696493	61.782716	69.088526
1053.564816	59.963920	69.093530
1053.112814	58.438780	69.098535
1052.377729	58.837021	69.103540
1051.395155	67.983918	69.108545
1050.856964	57.425829	69.113550
1049.677870	56.480699	69.118554
1049.251414	56.953190	69.123559
1048.691954	55.386454	69.128564
1047.774532	52.742652	69.133569
1046.645725	56.124483	69.138574
1045.785364	54.861498	69.143578
1045.387488	57.364651	69.148583
1045.140272	60.411582	69.153588
1044.399901	59.240544	69.158593
1044.214045	57.783903	69.163598
1043.797153	52.123223	69.168602
1043.173363	63.293971	69.173607
1042.057312	59.155443	69.178612
1041.297018	71.632796	69.183617
1040.771438	54.743260	69.188622
1039.570002	63.781195	69.193626
1039.247421	63.643823	69.198631
1039.238114	60.284017	69.203636
1037.987415	68.246892	69.208641
1037.002246	52.520743	69.213646
1036.494702	62.703738	69.218650
1035.906919	60.363866	69.223655
1035.897550	53.996723	69.228660
1034.397074	67.915626	69.233665
1033.832122	57.458829	69.238670
1033.078984	63.375545	69.243674
1032.677730	54.483008	69.248679
1032.124501	58.012977	69.253684
1031.546524	58.400500	69.258689
1030.675067	56.374457	69.263694
1029.757065	48.626280	69.268698
1029.135865	63.397585	69.273703
1029.394963	67.815506	69.278708
1028.031622	60.090693	69.283713
1027.192595	52.256758	69.288718
1026.318358	55.039237	69.293722
1025.712129	54.918073	69.298727
1025.914925	54.286150	69.303732
1025.211069	55.709258	69.308737
1024.093165	49.390639	69.313742
1023.107020	55.801968	69.318746
1022.500939	58.092104	69.323751
1022.474142	55.535386	69.328756
1021.520556	62.855701	69.333761
1020.488574	59.951667	69.338766
1020.082161	58.074136	69.343770
1019.290015	55.954780	69.348775
1019.228069	52.519916	69.353780
1018.072981	64.251359	69.358785
1017.053748	58.736853	69.363790
1016.238714	65.860953	69.368794
1016.030656	54.385857	69.373799
1015.590700	56.502289	69.378804
1015.211685	67.946108	69.383809
1014.673068	52.923458	69.388814
1013.408725	52.936308	69.393818
1012.552466	55.928069	69.398823
1012.704996	50.154884	69.403828
1011.662989	52.206266	69.408833
1010.405574	50.816292	69.413838
1009.818635	50.226455	69.418842
1009.586837	58.502717	69.423847
1009.309272	57.100071	69.428852
1008.251551	60.435001	69.433857
1007.576994	50.193948	69.438862
1006.770145	54.325085	69.443866
1006.245589	61.333128	69.448871
1006.297069	55.287523	69.453876
1004.781520	51.453461	69.458881
1003.766933	52.947940	69.463886
1003.194465	57.047624	69.468890
1002.811818	55.022743	69.473895
1002.589140	50.137585	69.478900
1002.029433	58.026339	69.483905
1001.201443	56.408099	69.488910
1000.567661	58.652852	69.493914
1000.219589	60.474092	69.498919
999.434422	57.901594	69.503924
997.998654	57.156739	69.508929
997.545991	63.409220	69.513934
997.463002	51.797848	69.518938
996.011996	63.815615	69.523943
995.584489	53.869344	69.528948
994.844763	61.211457	69.533953
994.200338	63.183310	69.538958
993.748008	55.213296	69.543962
993.065732	56.226944	69.548967
992.217325	48.958676	69.553972
991.665569	63.574806	69.558977
991.112089	61.473396	69.563982
990.782721	58.340104	69.568986
989.576045	66.838183	69.573991
988.827691	55.797836	69.578996
987.832681	60.627876	69.584001
987.741395	60.830221	69.589006
987.255064	58.088134	69.594010
986.547689	62.050669	69.599015
986.123894	61.455395	69.604020
985.123956	60.646960	69.609025
984.629723	58.370808	69.614030
983.965783	67.496696	69.619034
982.590999	62.973039	69.624039
982.117694	62.424532	69.629044
981.404109	66.805742	69.634049
980.718865	61.354832	69.639054
980.486448	60.032082	69.644058
980.143720	63.962959	69.649063
979.926761	57.099686	69.654068
978.707310	63.882145	69.659073
977.721100	56.833256	69.664078
977.325714	57.279907	69.669082
976.621042	65.340325	69.674087
975.882587	52.430488	69.679092
975.106206	62.356774	69.684097
974.308558	56.832752	69.689102
973.798041	57.771990	69.694106
973.401334	57.091556	69.699111
972.986191	56.561904	69.704116
971.702709	59.520261	69.709121
971.052462	60.050820	69.714126
970.584588	60.498438	69.719130
970.281776	63.494105	69.724135
969.080079	56.441861	69.729140
968.193172	65.155955	69.734145
967.558964	59.282250	69.739150
967.494586	61.171744	69.744154
966.738885	62.530321	69.749159
966.253057	56.615812	69.754164
965.490685	57.941586	69.759169
965.148422	54.688144	69.764174
964.150981	59.614519	69.769178
962.810597	67.867883	69.774183
962.121459	55.940341	69.779188
961.718505	66.213973	69.784193
961.447090	58.625854	69.789198
961.147784	64.385912	69.794202
960.462646	65.172303	69.799207
959.251597	56.443327	69.804212
958.337327	63.846913	69.809217
957.964926	57.798117	69.814222
958.111073	62.995597	69.819226
956.438460	63.493228	69.824231
956.242604	57.798652	69.829236
955.098169	66.639743	69.834241
955.132410	61.084567	69.839246
953.998080	59.135924	69.844250
953.302075	63.222825	69.849255
953.207641	55.737813	69.854260
952.574798	65.673860	69.859265
951.308111	54.356391	69.864270
950.432478	62.710153	69.869274
949.912943	72.179980	69.874279
950.061734	62.893662	69.879284
949.265350	58.602919	69.884289
947.866949	57.411176	69.889294
946.919884	64.023052	69.894298
946.671199	57.781763	69.899303
946.329910	59.387907	69.904308
945.879678	63.077078	69.909313
944.619061	64.537129	69.914318
943.762630	62.848379	69.919322
943.035250	65.010095	69.924327
942.824867	50.508330	69.929332
942.616558	65.234579	69.934337
941.758866	60.317263	69.939342
940.521819	58.558706	69.944346
939.944439	59.009292	69.949351
939.454746	66.470424	69.954356
939.040204	60.880798	69.959361
938.635553	63.093422	69.964366
937.750730	61.709915	69.969370
937.076610	61.154754	69.974375
936.749230	52.986913	69.979380
934.947823	72.749837	69.984385
934.397602	67.023191	69.989390
933.707865	63.980831	69.994394
932.973060	78.581350	69.999399
932.987022	63.003047	70.004404
932.794880	73.298997	70.009409
932.134809	55.995968	70.014414
931.330770	59.881120	70.019418
929.794721	59.644093	70.024423
929.720744	59.832422	70.029428
929.453818	62.505777	70.034433
928.199150	67.364903	70.039438
927.256280	67.775065	70.044442
926.751577	66.468163	70.049447
926.551473	60.738003	70.054452
925.914441	67.338625	70.059457
924.888566	58.508081	70.064462
924.518601	55.316622	70.069466
923.952769	67.815931	70.074471
923.621901	55.549161	70.079476
922.311031	64.627564	70.084481
921.581065	61.256982	70.089486
921.463542	56.255932	70.094490
920.594854	67.910313	70.099495
918.904735	65.188883	70.104500
918.437329	57.725516	70.109505
917.829784	62.847215	70.114510
917.468632	59.768715	70.119514
916.468021	60.637955	70.124519
916.563106	63.765994	70.129524
916.153112	62.959952	70.134529
915.694427	55.660085	70.139534
915.037027	57.833500	70.144538
913.964069	61.906020	70.149543
913.503429	62.487397	70.154548
912.224129	61.924576	70.159553
911.572050	57.344271	70.164558
911.009944	60.315273	70.169562
910.453377	68.421379	70.174567
909.953517	62.020622	70.179572
909.192994	62.919398	70.184577
908.597156	62.586085	70.189582
907.514375	56.079517	70.194586
907.242955	57.398975	70.199591
906.900004	53.907248	70.204596
905.645118	63.118953	70.209601
905.112419	60.526126	70.214606
904.195278	54.179472	70.219610
903.618761	63.481431	70.224615
903.630331	59.981088	70.229620
902.924748	69.935913	70.234625
902.089752	63.041529	70.239630
901.425330	57.414974	70.244634
900.645525	60.371947	70.249639
899.783422	53.588390	70.254644
898.742456	65.436084	70.259649
898.411959	62.661792	70.264654
897.930974	61.525297	70.269658
897.724056	67.456628	70.274663
897.414118	55.834008	70.279668
896.101312	66.846070	70.284673
895.220466	63.054909	70.289678
895.020148	58.669589	70.294682
893.152265	74.326620	70.299687
893.024640	61.878602	70.304692
892.122988	62.989043	70.309697
892.154140	67.007459	70.314702
891.643447	58.423411	70.319706
891.183352	60.680268	70.324711
890.072720	56.522697	70.329716
889.240405	60.951879	70.334721
888.678528	60.138303	70.339726
888.322538	49.893243	70.344730
886.874561	59.009736	70.349735
886.442347	52.448592	70.354740
886.080959	53.687938	70.359745
885.290380	64.457012	70.364750
885.018953	57.387169	70.369754
884.243084	58.353311	70.374759
883.205750	50.504828	70.379764
882.780206	51.962782	70.384769
882.497674	58.907272	70.389774
881.539475	57.551738	70.394778
880.233511	68.754463	70.399783
879.873613	57.936546	70.404788
878.931241	61.839871	70.409793
878.683791	59.669879	70.414798
878.267513	52.256183	70.419802
877.834132	64.236644	70.424807
876.773544	51.672916	70.429812
876.296800	61.183168	70.434817
875.342508	62.328679	70.439822
875.243387	58.068126	70.444826
873.979704	65.970491	70.449831
873.666914	55.755134	70.454836
873.060908	56.115504	70.459841
872.039137	60.443329	70.464846
871.265546	60.135728	70.469850
870.145561	69.129741	70.474855
869.820418	59.531467	70.479860
869.111338	63.152481	70.484865
868.983197	68.818886	70.489870
868.681009	63.803679	70.494874
868.229370	65.651348	70.499879
867.160022	50.752798	70.504884
866.187326	64.563960	70.509889
865.666768	60.978715	70.514894
864.894072	59.195118	70.519898
863.840841	62.726664	70.524903
863.412115	57.886677	70.529908
862.774813	69.096847	70.534913
862.659029	67.395331	70.539918
862.133355	62.160653	70.544922
860.698553	64.834313	70.549927
860.402395	64.625720	70.554932
859.768901	75.314612	70.559937
859.142930	61.729911	70.564942
858.252029	56.948955	70.569946
857.379993	64.318082	70.574951
857.073076	54.906944	70.579956
856.504777	59.066712	70.584961
855.811690	57.772349	70.589966
854.601014	63.877968	70.594970
853.900800	65.747688	70.599975
853.375970	65.550238	70.604980
852.977271	64.991333	70.609985
852.445341	65.576638	70.614990
852.055381	57.413212	70.619994
851.039596	63.477161	70.624999
850.546822	58.424342	70.630004
849.969332	63.020268	70.635009
849.183514	69.874130	70.640014
848.732201	61.967909	70.645018
847.772629	63.046043	70.650023
847.575001	68.346999	70.655028
846.017522	67.299764	70.660033
845.521236	67.831203	70.665038
845.123851	65.548742	70.670042
844.322153	67.522684	70.675047
843.897194	65.497565	70.680052
843.044052	65.349639	70.685057
842.377378	61.054068	70.690062
841.909012	53.498912	70.695066
841.076205	63.759722	70.700071
840.723367	52.826533	70.705076
839.531158	64.503567	70.710081
838.697694	57.106071	70.715086
837.998953	56.997618	70.720090
837.574622	68.046184	70.725095
837.618179	60.578992	70.730100
836.949127	60.641102	70.735105
835.890325	69.239397	70.740110
835.487196	62.898264	70.745114
834.408810	65.531803	70.750119
834.282321	64.628660	70.755124
833.184011	64.788372	70.760129
832.369036	69.094995	70.765134
831.797846	57.876721	70.770138
830.919547	68.007175	70.775143
830.945424	56.343232	70.780148
829.817501	61.810634	70.785153
828.992853	70.173834	70.790158
828.383007	53.003943	70.795162
827.912119	64.375069	70.800167
827.393916	52.561570	70.805172
826.956825	60.852463	70.810177
825.584302	63.578619	70.815182
825.405175	59.393349	70.820186
824.327332	57.274019	70.825191
824.495879	56.125747	70.830196
823.492122	62.626959	70.835201
822.619533	63.766774	70.840206
822.374484	60.651029	70.845210
821.516993	63.787101	70.850215
820.220645	58.504840	70.855220
819.464052	61.910588	70.860225
818.832463	62.526386	70.865230
818.720374	58.972627	70.870234
818.218908	65.857123	70.875239
817.843881	59.564467	70.880244
816.584811	60.766140	70.885249
816.089476	64.083326	70.890254
815.853641	55.712333	70.895258
814.542256	69.092066	70.900263
813.941849	63.846513	70.905268
812.771885	67.435167	70.910273
812.337099	68.021204	70.915278
811.864834	60.863408	70.920282
811.620488	62.578474	70.925287
811.074980	56.724737	70.930292
810.205117	63.400375	70.935297
809.355557	62.170714	70.940302
808.793804	55.514539	70.945306
807.864673	61.888502	70.950311
807.742300	62.903765	70.955316
806.599305	65.680606	70.960321
805.795786	64.398061	70.965326
805.446003	56.266049	70.970330
805.003065	63.035920	70.975335
804.631294	54.990960	70.980340
803.646458	69.924413	70.985345
802.651182	68.901281	70.990350
802.263913	59.645617	70.995354
801.621542	64.941439	71.000359
800.654502	61.385315	71.005364
799.922575	58.520329	71.010369
799.078956	58.903646	71.015374
798.907671	65.003335	71.020378
798.455705	66.969875	71.025383
798.023221	56.799506	71.030388
797.161620	59.017386	71.035393
796.588207	63.972598	71.040398
796.051907	56.868799	71.045402
794.706008	60.084981	71.050407
794.161625	61.776840	71.055412
793.182529	54.423643	71.060417
792.728077	60.903001	71.065422
792.733874	57.370101	71.070426
791.136024	62.941687	71.075431
790.882225	60.357942	71.080436
790.110629	59.891731	71.085441
789.613629	59.647681	71.090446
789.582784	59.016299	71.095450
787.891893	63.198635	71.100455
787.748364	62.095528	71.105460
787.124908	63.028078	71.110465
786.261427	50.634294	71.115470
785.456507	57.648921	71.120474
783.937663	65.577246	71.125479
784.131811	62.993346	71.130484
783.601176	60.879367	71.135489
783.178362	60.971145	71.140494
782.891936	60.533139	71.145498
781.805411	63.268735	71.150503
781.155375	59.130186	71.155508
780.676546	66.710243	71.160513
780.036483	71.603063	71.165518
779.223891	69.125298	71.170522
778.311921	71.128006	71.175527
778.016581	60.073270	71.180532
777.342860	64.570428	71.185537
775.874192	66.247727	71.190542
775.372148	60.834553	71.195546
774.638464	67.466739	71.200551
774.453241	60.207284	71.205556
773.765172	58.548146	71.210561
773.835057	66.114734	71.215566
772.656918	62.294003	71.220570
771.972383	63.898561	71.225575
771.047912	54.089170	71.230580
770.712550	58.963739	71.235585
769.315245	63.854434	71.240590
768.383689	60.857078	71.245594
768.058247	60.363392	71.250599
767.583417	62.016499	71.255604
767.424896	63.462668	71.260609
767.258219	64.234086	71.265614
766.255393	50.664241	71.270618
765.290889	57.069923	71.275623
764.708078	57.193056	71.280628
763.850701	55.345434	71.285633
762.440366	65.820435	71.290638
761.949510	60.646517	71.295642
761.198586	63.961701	71.300647
761.163892	52.758516	71.305652
760.693503	62.914225	71.310657
760.400956	60.945771	71.315662
760.047120	56.759252	71.320666
758.775749	62.092563	71.325671
758.012217	58.869465	71.330676
756.752381	63.881476	71.335681
756.018354	65.357153	71.340686
755.420994	59.817027	71.345690
754.812464	71.285546	71.350695
754.655034	69.727740	71.355700
754.435583	64.970728	71.360705
753.789799	66.527995	71.365710
752.975108	57.114648	71.370714
752.123442	62.305412	71.375719
751.645527	65.961837	71.380724
750.884088	62.106835	71.385729
749.646033	73.687140	71.390734
749.142534	58.284747	71.395738
748.518366	69.427934	71.400743
748.489412	61.197552	71.405748
747.610128	59.440918	71.410753
746.333059	61.314734	71.415758
745.851459	62.615337	71.420762
745.376556	74.282009	71.425767
745.120808	62.201733	71.430772
744.040092	55.276462	71.435777
743.091192	66.614215	71.440782
742.865425	59.464730	71.445786
742.071930	60.240107	71.450791
741.374981	51.151974	71.455796
740.452789	57.675932	71.460801
739.881922	62.828463	71.465806
739.425367	54.760935	71.470810
738.729194	59.876118	71.475815
738.439852	56.805861	71.480820
737.332331	59.026800	71.485825
736.287654	68.829728	71.490830
736.100519	60.909851	71.495834
735.451277	59.039211	71.500839
735.125260	59.025205	71.505844
734.621148	54.588131	71.510849
733.389033	67.150652	71.515854
733.288813	55.105318	71.520858
731.922018	64.238331	71.525863
731.011832	59.320188	71.530868
730.384827	63.516863	71.535873
729.731889	62.693643	71.540878
729.698761	58.460477	71.545882
728.959840	61.646905	71.550887
728.946971	70.068015	71.555892
727.776098	66.786812	71.560897
727.028119	62.961877	71.565902
726.586756	58.065656	71.570906
725.029101	67.729104	71.575911
724.358930	57.660647	71.580916
723.684880	56.286469	71.585921
723.550069	70.764856	71.590926
723.174140	58.263093	71.595930
722.575483	60.807369	71.600935
721.826262	65.329701	71.605940
721.339659	57.582700	71.610945
720.231502	58.434482	71.615950
719.863393	50.581533	71.620954
718.315924	58.733050	71.625959
717.707442	53.269835	71.630964
717.380371	60.208532	71.635969
716.867420	58.784654	71.640974
716.463349	50.502494	71.645978
716.213538	56.835091	71.650983
715.074023	47.666079	71.655988
714.435021	43.345271	71.660993
713.464873	52.291129	71.665998
713.044461	55.992963	71.671002
711.796741	59.613113	71.676007
711.034091	56.003447	71.681012
710.832652	55.402475	71.686017
710.515833	56.317239	71.691022
710.002553	51.480709	71.696026
709.438742	53.969281	71.701031
708.712222	54.176641	71.706036
707.613183	48.972719	71.711041
707.155276	58.439876	71.716046
706.678274	57.115230	71.721050
705.596823	58.332289	71.726055
704.681590	49.847188	71.731060
704.318135	59.840503	71.736065
703.823638	58.900940	71.741070
703.573339	51.203064	71.746074
702.355598	58.312101	71.751079
701.485526	49.054700	71.756084
700.861136	49.205489	71.761089
700.047639	58.777375	71.766094
700.165139	53.820551	71.771098
699.217667	61.335634	71.776103
698.366934	63.891123	71.781108
697.741328	53.194943	71.786113
696.806831	50.800840	71.791118
697.126904	52.037134	71.796122
696.287826	53.595153	71.801127
695.367538	54.369365	71.806132
695.074366	52.223798	71.811137
693.541479	59.755884	71.816142
692.696734	46.766849	71.821146
692.401504	52.813162	71.826151
691.956094	53.375767	71.831156
691.346341	49.250466	71.836161
690.579150	59.649243	71.841166
689.570867	46.645597	71.846170
688.997738	56.433658	71.851175
688.427109	50.618194	71.856180
688.052995	59.362088	71.861185
687.556994	59.643244	71.866190
686.951279	51.193144	71.871194
685.910881	52.304101	71.876199
685.236016	53.028376	71.881204
684.623303	49.081995	71.886209
683.680603	58.335771	71.891214
682.975852	48.714151	71.896218
682.048992	52.555639	71.901223
681.697634	55.063078	71.906228
681.266911	55.685533	71.911233
681.231782	57.634746	71.916238
680.450752	54.813719	71.921242
679.495750	53.634514	71.926247
678.706945	55.047352	71.931252
678.309246	60.882682	71.936257
676.927054	55.064153	71.941262
676.662796	55.630460	71.946266
675.984681	64.147372	71.951271
675.687731	55.554381	71.956276
674.677709	59.464984	71.961281
673.493149	64.518587	71.966286
673.060875	59.721864	71.971290
672.569828	65.586213	71.976295
672.297700	64.336599	71.981300
672.021834	54.762286	71.986305
670.669216	59.926385	71.991310
670.179428	61.239844	71.996314
669.604101	68.342646	72.001319
668.756342	59.933616	72.006324
667.756110	58.718348	72.011329
666.880049	61.767628	72.016334
666.553982	54.462058	72.021338
666.363670	60.795909	72.026343
665.776285	60.540121	72.031348
665.362859	64.760209	72.036353
663.992753	64.179460	72.041358
663.832981	50.855596	72.046362
662.945377	54.541555	72.051367
661.574678	51.671166	72.056372
660.921399	52.390562	72.061377
660.208267	54.077791	72.066382
660.157770	56.807621	72.071386
659.372117	57.595088	72.076391
659.275391	52.704570	72.081396
658.716755	55.635131	72.086401
657.068604	58.761819	72.091406
656.755261	49.007233	72.096410
656.358935	54.443269	72.101415
655.685475	56.586703	72.106420
655.075205	55.443570	72.111425
654.063170	52.049921	72.116430
653.556902	48.253853	72.121434
653.180248	53.479688	72.126439
652.279362	49.392429	72.131444
651.028244	56.636264	72.136449
650.303454	59.567267	72.141454
650.010189	48.592335	72.146458
649.491891	47.847109	72.151463
649.053591	59.666566	72.156468
648.884531	54.408329	72.161473
647.656136	59.656146	72.166478
647.024560	58.680471	72.171482
646.385525	65.151196	72.176487
645.887443	57.667871	72.181492
645.055173	60.772806	72.186497
644.088426	62.803472	72.191502
643.676702	53.187312	72.196506
643.406786	58.944306	72.201511
642.439674	60.255468	72.206516
641.570923	64.637638	72.211521
640.725737	54.784704	72.216526
640.557688	57.493228	72.221530
639.455595	61.334352	72.226535
638.425500	52.400024	72.231540
637.737700	53.624653	72.236545
637.039454	64.569751	72.241550
637.229548	59.045915	72.246554
636.849746	59.606757	72.251559
636.360394	56.702611	72.256564
635.160778	51.594489	72.261569
634.165718	56.334199	72.266574
633.800035	51.107678	72.271578
633.436759	52.927199	72.276583
632.457211	53.871434	72.281588
631.850266	56.735673	72.286593
630.911405	65.899200	72.291598
630.680389	55.428311	72.296602
629.811974	62.603824	72.301607
628.797995	56.906954	72.306612
627.997432	55.578544	72.311617
627.514807	68.803288	72.316622
627.458875	56.791431	72.321626
627.121650	66.260809	72.326631
626.028945	62.193786	72.331636
625.180916	54.912124	72.336641
624.296060	63.246575	72.341646
624.320815	58.555496	72.346650
622.680131	60.818068	72.351655
621.834920	56.927318	72.356660
621.871308	58.402066	72.361665
620.815356	60.668665	72.366670
620.753451	55.942700	72.371674
620.357110	55.976275	72.376679
619.429607	56.944357	72.381684
618.670544	51.876413	72.386689
617.866363	60.600046	72.391694
617.581012	60.142131	72.396698
615.887288	60.799013	72.401703
615.379641	61.588591	72.406708
615.163942	55.028288	72.411713
614.539416	68.383915	72.416718
614.390956	60.497688	72.421722
613.302006	62.754943	72.426727
612.442920	61.469323	72.431732
612.034025	60.376953	72.436737
611.540670	64.124842	72.441742
611.208397	56.652983	72.446746
609.897201	57.384453	72.451751
608.841618	63.379865	72.456756
608.636651	60.583701	72.461761
607.824010	63.225830	72.466766
607.499136	52.268950	72.471770
606.274991	63.968850	72.476775
605.834290	53.382716	72.481780
605.338071	51.931118	72.486785
604.697187	59.581963	72.491790
604.291142	55.726890	72.496794
603.430174	59.850376	72.501799
602.710444	55.810243	72.506804
602.198487	58.927801	72.511809
601.645187	60.796064	72.516814
600.719178	54.987426	72.521818
599.878753	62.168014	72.526823
599.647456	55.160410	72.531828
599.307713	56.388959	72.536833
597.648183	52.917585	72.541838
597.042006	54.234018	72.546842
596.598257	65.099990	72.551847
596.299102	65.839245	72.556852
596.078691	59.702884	72.561857
594.728654	67.216695	72.566862
593.898605	54.700010	72.571866
593.457653	52.740025	72.576871
593.062751	59.284970	72.581876
592.284809	57.437981	72.586881
591.117407	62.319327	72.591886
590.596063	58.976614	72.596890
590.131388	53.754821	72.601895
589.451614	56.683644	72.606900
589.067119	59.125717	72.611905
587.254952	63.740975	72.616910
586.868398	46.728293	72.621914
586.499021	50.783342	72.626919
586.053779	51.896554	72.631924
586.216029	59.949372	72.636929
585.728360	55.430955	72.641934
584.708829	52.663835	72.646938
583.480654	53.105577	72.651943
582.713385	58.697140	72.656948
581.916854	64.191882	72.661953
580.725185	62.629321	72.666958
580.540808	53.919564	72.671962
580.069381	63.227206	72.676967
579.250528	57.800453	72.681972
579.316097	56.914937	72.686977
579.063950	65.145725	72.691982
577.894618	59.743102	72.696986
577.020599	60.289947	72.701991
576.362801	64.551907	72.706996
575.868485	54.797551	72.712001
575.031156	66.142250	72.717006
574.045454	57.776223	72.722010
573.664169	55.084478	72.727015
572.865548	56.814391	72.732020
571.756292	53.180460	72.737025
571.229760	62.124931	72.742030
570.833394	54.327764	72.747034
570.041436	54.982517	72.752039
569.602664	59.050642	72.757044
569.522997	41.569755	72.762049
568.838180	57.561344	72.767054
567.880289	53.795696	72.772058
567.043126	56.429006	72.777063
566.504075	49.970689	72.782068
565.806948	51.767287	72.787073
564.576913	61.816319	72.792078
564.333726	52.965860	72.797082
563.980381	61.086886	72.802087
563.339677	53.662750	72.807092
562.615799	51.896500	72.812097
561.562551	56.306342	72.817102
561.104510	49.505744	72.822106
560.602548	58.150757	72.827111
559.581788	55.297017	72.832116
558.944576	48.150166	72.837121
557.959234	60.587531	72.842126
557.622032	60.095875	72.847130
557.104925	63.099062	72.852135
556.829958	54.447853	72.857140
556.158590	49.092545	72.862145
554.672791	63.260831	72.867150
554.505502	49.270813	72.872154
554.297194	58.544026	72.877159
552.991463	51.473036	72.882164
552.379886	55.016591	72.887169
551.733578	61.771971	72.892174
551.241991	49.997004	72.897178
550.609414	52.988003	72.902183
549.719638	59.695498	72.907188
549.143972	50.304017	72.912193
548.135162	54.431525	72.917198
548.104739	48.405114	72.922202
547.527936	50.545815	72.927207
546.282799	59.081336	72.932212
545.849558	51.484297	72.937217
544.974336	51.682821	72.942222
544.779770	46.738028	72.947226
544.380149	55.534837	72.952231
543.581132	56.779323	72.957236
543.101433	55.629228	72.962241
542.371224	60.127795	72.967246
541.532305	52.749074	72.972250
540.531657	53.252099	72.977255
539.924838	55.918573	72.982260
539.498741	51.498950	72.987265
538.584019	57.604833	72.992270
537.692466	46.287987	72.997274
536.791023	52.695523	73.002279
536.185310	55.471538	73.007284
535.656689	49.261690	73.012289
535.162732	57.696922	73.017294
535.059929	57.060506	73.022298
533.886724	55.397300	73.027303
533.395880	55.586409	73.032308
533.035679	57.877488	73.037313
531.993869	60.085236	73.042318
531.110167	56.525951	73.047322
530.277531	59.793982	73.052327
529.605593	60.596720	73.057332
529.556834	55.525107	73.062337
529.040872	62.299205	73.067342
528.400941	56.871016	73.072346
527.109225	53.438483	73.077351
526.567101	66.443296	73.082356
526.432732	56.603196	73.087361
525.857396	57.110319	73.092366
524.693047	56.743026	73.097370
523.884303	53.901516	73.102375
523.091249	57.338808	73.107380
522.981133	53.010300	73.112385
522.451868	60.851223	73.117390
521.329079	54.262421	73.122394
520.378601	54.918687	73.127399
519.783623	57.581949	73.132404
519.723958	45.420765	73.137409
519.179184	62.314361	73.142414
518.596528	60.773380	73.147418
517.393203	58.320779	73.152423
516.682440	58.578359	73.157428
516.433331	52.618234	73.162433
514.806102	54.644074	73.167438
514.415880	52.353714	73.172442
513.882311	63.057846	73.177447
513.137275	65.943786	73.182452
512.783152	55.393358	73.187457
512.610876	66.856987	73.192462
512.333980	53.524797	73.197466
511.012878	56.236696	73.202471
510.203079	62.158825	73.207476
509.924549	57.573401	73.212481
508.635287	56.893587	73.217486
508.185845	55.990928	73.222490
507.118750	65.082498	73.227495
506.574444	59.635559	73.232500
506.502380	53.577602	73.237505
506.054977	62.606800	73.242510
504.652252	52.348152	73.247514
504.453664	52.762302	73.252519
503.644887	58.466768	73.257524
503.384296	55.793822	73.262529
502.149701	66.820566	73.267534
501.464160	65.744033	73.272538
500.845813	58.127404	73.277543
499.983539	62.017457	73.282548
499.891231	55.148672	73.287553
498.914723	68.109109	73.292558
498.496522	60.392267	73.297562
497.947599	64.069558	73.302567
497.102721	62.026041	73.307572
496.504011	44.278468	73.312577
495.287746	53.146133	73.317582
494.680853	61.619666	73.322586
494.115989	53.486273	73.327591
493.442551	51.950984	73.332596
493.349279	48.797421	73.337601
492.639616	55.888114	73.342606
491.649026	45.908573	73.347610
491.227770	53.288510	73.352615
490.562085	56.889102	73.357620
490.196829	50.907833	73.362625
488.912990	66.325926	73.367630
488.397356	60.893418	73.372634
487.795124	67.000235	73.377639
487.164189	66.000395	73.382644
486.343006	61.545850	73.387649
485.308323	64.936531	73.392654
484.936101	60.048234	73.397658
484.548034	61.178498	73.402663
484.334136	55.268787	73.407668
483.562192	57.188342	73.412673
482.244836	59.530547	73.417678
481.718506	61.983115	73.422682
481.455251	66.930989	73.427687
480.213737	65.379364	73.432692
479.452750	64.056040	73.437697
478.772168	61.864382	73.442702
478.416244	65.072048	73.447706
478.286537	49.671999	73.452711
477.436911	57.054293	73.457716
476.862347	55.348520	73.462721
475.957944	70.723704	73.467726
475.408676	58.486158	73.472730
474.542772	51.842301	73.477735
473.748334	61.324890	73.482740
473.293075	41.743768	73.487745
472.838293	55.331596	73.492750
472.285141	51.243605	73.497754
471.276146	49.568067	73.502759
470.400101	54.626469	73.507764
470.073725	51.316282	73.512769
468.994040	48.509371	73.517774
468.764359	48.232969	73.522778
467.873515	53.726908	73.527783
466.811393	57.417934	73.532788
466.517313	55.779355	73.537793
466.243437	62.075812	73.542798
465.456336	55.439372	73.547802
464.204578	54.964316	73.552807
463.242711	57.441389	73.557812
462.975970	49.884910	73.562817
462.485094	60.702902	73.567822
462.593116	61.119378	73.572826
461.756186	57.409602	73.577831
460.745213	56.895260	73.582836
460.030032	54.074833	73.587841
459.550876	51.001211	73.592846
459.024430	51.321553	73.597850
458.166302	51.488348	73.602855
457.191809	52.749497	73.607860
456.437803	53.848923	73.612865
456.025599	45.871346	73.617870
455.345367	49.230499	73.622874
454.323303	47.267090	73.627879
453.566242	54.298411	73.632884
453.058528	50.035279	73.637889
452.669604	61.563653	73.642894
452.097641	50.899393	73.647898
452.136691	52.543014	73.652903
451.142289	62.177890	73.657908
449.942391	53.785058	73.662913
449.603386	53.768561	73.667918
448.948383	46.400585	73.672922
448.005431	67.240086	73.677927
447.051245	58.856854	73.682932
446.646087	47.785483	73.687937
446.018296	62.962479	73.692942
445.694719	60.779513	73.697946
445.383119	50.408515	73.702951
444.112430	52.014879	73.707956
443.598518	49.794667	73.712961
443.028275	58.572954	73.717966
441.891144	52.964738	73.722970
441.537387	51.395200	73.727975
440.769095	63.159891	73.732980
440.366295	48.377406	73.737985
439.681133	52.392237	73.742990
439.186974	59.769277	73.747994
438.272274	50.888261	73.752999
436.888708	56.905562	73.758004
436.990142	63.427425	73.763009
436.294624	59.222921	73.768014
435.779439	62.179607	73.773018
434.794063	64.219424	73.778023
434.039022	70.564788	73.783028
433.791246	57.465634	73.788033
433.103548	61.827462	73.793038
432.009406	53.487957	73.798042
431.727653	57.348797	73.803047
430.740474	60.869102	73.808052
430.178789	54.654674	73.813057
429.759963	63.069141	73.818062
429.030731	61.655126	73.823066
427.959870	58.065966	73.828071
427.243913	60.959168	73.833076
427.128448	55.997672	73.838081
426.617191	72.312008	73.843086
426.106036	65.028714	73.848090
425.185795	58.384705	73.853095
424.194672	61.514130	73.858100
423.581837	54.148798	73.863105
422.912419	51.266855	73.868110
422.438504	54.537766	73.873114
421.364329	61.328584	73.878119
420.781483	60.727858	73.883124
420.402977	53.525648	73.888129
419.760292	49.659445	73.893134
419.489965	47.316578	73.898138
418.417170	54.934872	73.903143
417.694714	55.689443	73.908148
417.186665	50.325121	73.913153
416.609617	58.943531	73.918158
415.587725	56.420396	73.923162
415.084494	51.952038	73.928167
414.333067	54.877371	73.933172
414.327814	46.880191	73.938177
412.981331	52.874168	73.943182
412.035385	56.700417	73.948186
411.505633	48.757595	73.953191
410.858708	56.181733	73.958196
410.817765	59.069780	73.963201
410.178427	59.820371	73.968206
409.712787	60.718817	73.973210
408.817747	58.732465	73.978215
408.072495	57.960242	73.983220
407.116307	51.655145	73.988225
406.186056	58.081451	73.993230
405.625555	51.798145	73.998234
404.952533	55.124493	74.003239
404.286516	57.793625	74.008244
404.051441	65.495721	74.013249
402.925886	66.654882	74.018254
402.127636	60.964522	74.023258
401.673997	60.250477	74.028263
401.087216	59.608983	74.033268
401.182081	62.403498	74.038273
400.020929	59.884890	74.043278
399.298652	59.360164	74.048282
398.394407	57.111723	74.053287
397.349831	57.167990	74.058292
397.558181	55.308717	74.063297
396.890317	53.755909	74.068302
396.143870	59.688113	74.073306
395.343092	62.209430	74.078311
394.926784	59.708433	74.083316
394.548590	49.711599	74.088321
393.330204	51.615706	74.093326
392.461330	51.049792	74.098330
392.120108	49.904402	74.103335
391.262504	59.565179	74.108340
390.501939	48.392893	74.113345
389.857741	55.333830	74.118350
389.173004	55.307906	74.123354
388.641987	52.599213	74.128359
388.246794	54.252122	74.133364
387.696999	51.099832	74.138369
386.507543	59.493214	74.143374
386.054248	62.332724	74.148378
385.503521	56.108926	74.153383
384.829669	60.807840	74.158388
384.056021	48.470629	74.163393
383.130685	64.811315	74.168398
382.868443	60.097198	74.173402
382.742948	60.746312	74.178407
381.469005	61.866568	74.183412
380.719507	49.562716	74.188417
380.222144	55.301058	74.193422
379.055526	54.532766	74.198426
378.316685	50.820409	74.203431
377.686113	54.840891	74.208436
376.949919	56.117660	74.213441
376.474442	48.455659	74.218446
376.153035	61.802747	74.223450
376.516465	53.696991	74.228455
375.012692	61.981621	74.233460
374.167440	58.832600	74.238465
373.184219	56.523887	74.243470
372.776190	58.413063	74.248474
372.434355	58.576257	74.253479
371.663490	58.318795	74.258484
371.050270	54.707271	74.263489
370.606072	52.972855	74.268494
369.750221	50.665209	74.273498
368.678398	54.217792	74.278503
367.863555	57.050584	74.283508
367.564021	50.603753	74.288513
367.058262	55.474768	74.293518
366.332442	59.399082	74.298522
365.625937	46.263706	74.303527
364.673406	52.747909	74.308532
364.350949	59.851986	74.313537
363.768397	59.253191	74.318542
362.877676	61.029708	74.323546
362.028133	47.295198	74.328551
361.311189	55.460769	74.333556
360.857441	58.120763	74.338561
359.935389	59.074934	74.343566
359.679021	59.640694	74.348570
359.047872	46.659369	74.353575
357.705267	56.725747	74.358580
357.689214	51.134624	74.363585
356.958560	50.403326	74.368590
356.805318	59.091993	74.373594
355.819080	42.722517	74.378599
354.861585	53.116027	74.383604
354.263791	42.914486	74.388609
354.015748	49.978176	74.393614
353.275089	52.713392	74.398618
352.424253	48.070947	74.403623
351.302836	49.078628	74.408628
350.977907	54.346918	74.413633
350.265459	46.618962	74.418638
349.734934	47.676945	74.423642
348.477306	40.011639	74.428647
347.772312	47.007597	74.433652
347.502484	44.880164	74.438657
347.234994	47.235093	74.443662
346.569032	40.041906	74.448666
346.442377	48.104731	74.453671
345.468651	52.671892	74.458676
344.727140	48.565286	74.463681
343.944148	50.977382	74.468686
343.018430	47.028656	74.473690
342.046311	42.126755	74.478695
341.467434	55.493490	74.483700
341.030471	49.492165	74.488705
340.771732	53.850742	74.493710
340.026043	45.673776	74.498714
339.111455	39.979300	74.503719
338.460636	52.902073	74.508724
338.089894	49.456224	74.513729
337.421673	47.824940	74.518734
336.238031	45.355598	74.523738
335.501066	49.506810	74.528743
334.794273	47.912925	74.533748
334.740805	45.408169	74.538753
334.360782	42.876095	74.543758
333.078647	48.275673	74.548762
332.582487	41.319819	74.553767
331.549018	50.980342	74.558772
331.391533	48.474861	74.563777
331.071511	49.573343	74.568782
329.749220	48.765433	74.573786
328.979873	34.937467	74.578791
328.613434	47.150747	74.583796
327.995890	50.961775	74.588801
327.536546	50.676586	74.593806
326.261423	47.290612	74.598810
325.929769	45.646249	74.603815
325.361074	54.096659	74.608820
325.132807	41.850331	74.613825
323.718666	42.900687	74.618830
322.864416	45.255529	74.623834
322.458052	47.046138	74.628839
321.898419	48.682236	74.633844
321.977774	45.863023	74.638849
320.609652	54.097966	74.643854
319.376985	48.569317	74.648858
319.033080	46.409190	74.653863
318.320289	50.954527	74.658868
318.220430	46.049179	74.663873
317.775965	49.256630	74.668878
316.796116	43.763595	74.673882
316.272520	45.069063	74.678887
315.336952	55.783670	74.683892
315.115056	47.224848	74.688897
313.911437	51.501829	74.693902
312.884135	55.516107	74.698906
313.215674	54.611845	74.703911
312.551016	52.860750	74.708916
311.257699	50.088521	74.713921
310.056937	47.990783	74.718926
309.489813	53.977517	74.723930
309.028616	41.648752	74.728935
308.754864	46.680519	74.733940
308.170041	46.914177	74.738945
308.128133	49.533586	74.743950
306.857431	53.304597	74.748954
306.234515	40.979473	74.753959
306.014458	54.365229	74.758964
304.953247	48.045006	74.763969
303.832223	52.448351	74.768974
303.007054	51.324733	74.773978
303.068243	51.144925	74.778983
302.275303	50.296030	74.783988
301.659095	45.644173	74.788993
300.726643	52.237436	74.793998
299.843505	58.735808	74.799002
299.807739	47.398668	74.804007
299.104483	49.648692	74.809012
298.308797	41.916861	74.814017
297.355487	44.999169	74.819022
296.387765	46.016439	74.824026
296.260389	43.512116	74.829031
295.650133	50.893265	74.834036
295.289799	48.505048	74.839041
294.161721	48.125282	74.844046
293.324878	48.391479	74.849050
293.199156	44.345911	74.854055
292.101900	52.163009	74.859060
291.696397	48.584579	74.864065
290.601192	48.013269	74.869070
289.952198	47.369033	74.874074
289.970643	43.431775	74.879079
289.563237	43.708049	74.884084
288.390930	47.340627	74.889089
287.870772	46.291832	74.894094
286.890253	48.808445	74.899098
286.317074	38.890845	74.904103
285.201952	47.368202	74.909108
284.643937	41.439739	74.914113
284.219934	48.589634	74.919118
284.076843	46.161422	74.924122
283.617016	45.018608	74.929127
282.411607	51.693392	74.934132
281.669600	40.562960	74.939137
281.339740	41.783518	74.944142
279.972155	41.662293	74.949146
279.139006	40.284668	74.954151
278.622420	52.959053	74.959156
278.046672	47.778059	74.964161
277.677550	44.481142	74.969166
277.197265	47.726706	74.974170
276.940758	47.722133	74.979175
275.892603	48.202173	74.984180
275.342457	43.230727	74.989185
274.694173	42.238235	74.994190
273.861831	41.761998	74.999194
272.776848	46.247981	75.004199
271.723169	46.471615	75.009204
271.189056	43.379810	75.014209
270.978842	38.385232	75.019214
270.891783	42.847400	75.024218
270.609850	46.566963	75.029223
269.025122	48.770718	75.034228
268.423926	47.701080	75.039233
267.707944	49.531736	75.044238
267.193366	52.314655	75.049242
266.707105	37.063400	75.054247
265.483490	44.547309	75.059252
265.245446	41.461597	75.064257
264.567399	37.975279	75.069262
263.985175	36.900418	75.074266
263.300630	33.961498	75.079271
262.281236	44.571266	75.084276
261.943520	41.386988	75.089281
261.778028	39.558634	75.094286
260.501949	40.916114	75.099290
259.673253	40.473595	75.104295
258.994565	41.839992	75.109300
258.891342	40.481726	75.114305
258.208597	43.025852	75.119310
256.779321	45.048633	75.124314
256.248174	42.023423	75.129319
255.578588	41.491269	75.134324
255.174592	38.165204	75.139329
254.651556	41.467830	75.144334
253.907722	48.204415	75.149338
253.933998	44.268973	75.154343
252.582301	40.451702	75.159348
252.254645	40.341700	75.164353
251.694717	42.926746	75.169358
250.346770	37.465248	75.174362
249.769738	31.643865	75.179367
249.057036	46.104778	75.184372
248.634715	41.051826	75.189377
248.251317	39.586461	75.194382
247.270906	43.719808	75.199386
246.349665	36.491063	75.204391
245.806601	37.936445	75.209396
245.287981	35.712332	75.214401
244.985666	38.774243	75.219406
244.071109	37.157174	75.224410
243.124801	37.778833	75.229415
242.633113	43.526071	75.234420
242.102162	39.949416	75.239425
241.963883	44.560091	75.244430
240.893746	42.731676	75.249434
240.091915	46.959934	75.254439
239.305386	43.088027	75.259444
238.952264	45.990501	75.264449
238.393272	47.701493	75.269454
237.389868	50.985809	75.274458
236.891807	44.758937	75.279463
236.083206	43.233437	75.284468
235.756634	42.489342	75.289473
234.659789	45.737176	75.294478
233.541954	46.310085	75.299482
233.310622	42.264468	75.304487
232.940981	44.710722	75.309492
232.247989	42.242962	75.314497
231.157617	43.094568	75.319502
230.461891	44.780054	75.324506
230.381885	41.791986	75.329511
229.660113	47.818650	75.334516
229.212193	44.250657	75.339521
228.011091	43.202149	75.344526
227.092347	38.120220	75.349530
226.821961	40.329605	75.354535
226.437780	48.624843	75.359540
226.350327	38.960295	75.364545
225.005758	41.671154	75.369550
224.150832	45.778259	75.374554
224.143214	39.619684	75.379559
222.193568	49.070177	75.384564
221.786721	39.597342	75.389569
220.788189	38.209395	75.394574
220.202000	43.204326	75.399578
220.297631	36.025879	75.404583
220.188845	42.168509	75.409588
219.912091	38.644596	75.414593
218.527790	38.597697	75.419598
217.545638	44.497293	75.424602
217.557993	39.833626	75.429607
216.085005	48.124849	75.434612
215.579871	39.876291	75.439617
214.929664	45.985419	75.444622
214.004874	47.441767	75.449626
213.786400	44.162058	75.454631
213.179052	47.250997	75.459636
211.835295	39.100007	75.464641
211.276117	44.112413	75.469646
210.646988	43.167171	75.474650
210.487336	40.584706	75.479655
209.813043	44.562172	75.484660
209.223139	40.165940	75.489665
208.516614	37.817735	75.494670
207.312658	40.990387	75.499674
207.203046	43.263393	75.504679
206.857510	48.240759	75.509684
206.273337	33.091960	75.514689
205.218999	42.300572	75.519694
204.558769	34.945393	75.524698
203.596237	46.519572	75.529703
202.155589	42.072998	75.534708
201.816637	35.325077	75.539713
201.528157	39.670592	75.544718
200.745559	55.285004	75.549722
200.786698	44.695705	75.554727
200.230613	44.914187	75.559732
199.490018	45.649795	75.564737
198.369723	42.435468	75.569742
197.424520	48.813442	75.574746
197.426275	47.698878	75.579751
196.899015	42.588136	75.584756
195.750822	43.180073	75.589761
195.015985	45.964439	75.594766
194.475720	52.550485	75.599770
194.179630	39.899781	75.604775
193.185728	42.962619	75.609780
192.272530	44.669994	75.614785
192.118449	39.605015	75.619790
190.842050	45.106660	75.624794
190.648794	40.546524	75.629799
189.746839	53.303148	75.634804
188.874617	43.628265	75.639809
188.384384	51.571047	75.644814
187.638071	56.075569	75.649818
187.449608	41.371669	75.654823
186.697707	49.697968	75.659828
186.278994	46.945583	75.664833
185.427199	49.643426	75.669838
184.786464	51.832620	75.674842
184.134931	43.605608	75.679847
183.127684	50.617866	75.684852
182.202740	48.875492	75.689857
181.826728	53.439688	75.694862
181.569521	55.991797	75.699866
181.251329	48.800998	75.704871
180.200949	57.691199	75.709876
179.274765	45.984505	75.714881
178.947113	46.076996	75.719886
177.902496	55.718926	75.724890
177.089782	49.776117	75.729895
176.346598	45.442873	75.734900
175.727168	41.859291	75.739905
175.315628	48.963238	75.744910
175.100527	46.099771	75.749914
173.922028	37.989543	75.754919
173.164918	52.210984	75.759924
172.604878	47.973443	75.764929
172.318498	43.116265	75.769934
171.392877	46.975380	75.774938
170.456292	43.564974	75.779943
169.659088	48.808043	75.784948
169.685743	45.082132	75.789953
168.720909	46.323918	75.794958
168.354528	52.054024	75.799962
167.848645	42.265826	75.804967
166.526269	47.630104	75.809972
166.272970	42.531217	75.814977
165.686397	48.544579	75.819982
164.742949	50.126890	75.824986
164.331969	42.312173	75.829991
163.458114	47.971384	75.834996
163.038471	40.299066	75.840001
161.796859	43.119785	75.845006
160.712735	43.991256	75.850010
160.460879	41.529594	75.855015
159.467474	46.695778	75.860020
158.975818	42.488753	75.865025
158.974327	43.566980	75.870030
158.520284	43.139988	75.875034
158.252975	37.159743	75.880039
157.146207	41.590668	75.885044
156.575810	41.579519	75.890049
155.973703	40.715304	75.895054
154.516599	45.446667	75.900058
153.973048	36.518697	75.905063
153.403622	43.710099	75.910068
152.748604	47.837810	75.915073
152.643106	37.516800	75.920078
151.740275	49.010098	75.925082
150.909191	37.578021	75.930087
149.850002	41.655418	75.935092
149.832247	47.656134	75.940097
149.078805	45.255984	75.945102
147.984949	52.334408	75.950106
147.370590	45.070052	75.955111
146.965602	43.148163	75.960116
146.588230	44.437659	75.965121
145.822661	43.918817	75.970126
144.502979	44.652657	75.975130
144.003065	40.837026	75.980135
143.258535	54.470559	75.985140
142.966175	49.610854	75.990145
142.761658	45.040022	75.995150
141.941131	47.658306	76.000154
140.911064	47.771744	76.005159
140.351933	48.568616	76.010164
140.202905	40.566901	76.015169
139.148421	39.859577	76.020174
137.610757	48.713319	76.025178
137.350241	41.948406	76.030183
136.979298	42.987342	76.035188
136.564920	47.794943	76.040193
136.646487	43.903708	76.045198
135.318199	44.797700	76.050202
134.641946	41.285047	76.055207
133.871073	46.958974	76.060212
132.810118	39.921174	76.065217
132.180608	45.754409	76.070222
131.321463	47.967629	76.075226
131.371350	38.849909	76.080231
131.045409	40.655558	76.085236
130.223224	45.868179	76.090241
129.191639	45.342840	76.095246
128.208698	49.672813	76.100250
127.699357	36.487533	76.105255
126.735894	37.929211	76.110260
125.932166	43.581930	76.115265
125.548296	40.999622	76.120270
124.729476	45.321984	76.125274
124.803590	35.563837	76.130279
124.525304	45.012819	76.135284
123.587611	41.901017	76.140289
122.729591	39.907988	76.145294
121.951160	46.212779	76.150298
121.189360	38.224148	76.155303
119.582300	41.377509	76.160308
118.959074	48.822859	76.165313
119.114295	44.729536	76.170318
118.572509	56.220153	76.175322
118.263470	40.306619	76.180327
117.450717	57.127312	76.185332
116.479570	46.734057	76.190337
115.903613	39.321031	76.195342
115.107631	45.976573	76.200346
114.778380	38.095753	76.205351
114.678451	44.540395	76.210356
113.614410	42.677417	76.215361
112.837159	36.355942	76.220366
111.883297	43.732058	76.225370
111.003294	34.741390	76.230375
109.903509	50.205713	76.235380
109.187698	49.395337	76.240385
109.037946	42.214358	76.245390
108.460206	45.392961	76.250394
108.338688	41.756793	76.255399
108.033504	40.868129	76.260404
106.905276	46.400439	76.265409
106.008379	45.734392	76.270414
105.192460	46.923031	76.275418
104.769151	42.456418	76.280423
103.723824	48.715393	76.285428
103.076101	44.637756	76.290433
102.890110	38.196368	76.295438
102.321330	55.399155	76.300442
102.015274	41.101856	76.305447
100.933908	36.596884	76.310452
100.073961	38.334618	76.315457
99.595878	37.541118	76.320462
98.548846	44.347456	76.325466
98.045023	42.650135	76.330471
97.189616	51.314692	76.335476
96.813550	55.275385	76.340481
96.622140	42.950942	76.345486
95.035690	52.565382	76.350490
94.305468	48.039681	76.355495
93.948658	49.760235	76.360500
93.362466	39.056670	76.365505
93.021566	38.311490	76.370510
92.248332	45.919127	76.375514
91.568737	36.826216	76.380519
90.538987	47.492249	76.385524
90.299496	38.790042	76.390529
90.070148	32.832903	76.395534
88.643322	45.733979	76.400538
88.203544	37.114660	76.405543
87.382900	42.222422	76.410548
87.123013	40.871680	76.415553
85.886648	47.943755	76.420558
84.590383	54.434824	76.425562
84.937752	35.300011	76.430567
84.259727	44.064805	76.435572
83.556649	42.234683	76.440577
83.530254	41.140735	76.445582
81.945374	42.147017	76.450586
81.488743	41.298529	76.455591
80.777616	45.269297	76.460596
80.122115	48.778583	76.465601
80.007664	46.164300	76.470606
78.853465	48.371669	76.475610
78.030095	42.933972	76.480615
77.552537	50.090289	76.485620
76.709644	47.317486	76.490625
76.659481	38.808598	76.495630
76.029307	43.871077	76.500634
75.412406	37.000310	76.505639
74.621977	47.062061	76.510644
73.748401	43.525224	76.515649
72.819301	47.680986	76.520654
71.788288	52.095390	76.525658
71.527112	49.047210	76.530663
71.022927	39.364528	76.535668
70.435133	47.071815	76.540673
69.423287	39.611956	76.545678
68.540894	48.513232	76.550682
68.174647	47.787398	76.555687
67.404916	50.093846	76.560692
67.201544	45.688603	76.565697
66.735493	48.274545	76.570702
65.472888	50.934687	76.575706
64.752207	45.121778	76.580711
64.347454	43.459578	76.585716
63.818935	46.000181	76.590721
63.478112	41.700210	76.595726
62.292529	49.643004	76.600730
61.693276	49.438667	76.605735
60.998613	40.764371	76.610740
60.520834	43.839004	76.615745
60.098630	47.319347	76.620750
59.081573	56.501068	76.625754
58.278247	36.700696	76.630759
57.664650	38.700524	76.635764
57.377357	43.850263	76.640769
56.473789	46.789488	76.645774
55.362215	47.144274	76.650778
54.923965	41.145587	76.655783
54.411727	38.611741	76.660788
53.723973	44.351552	76.665793
53.482422	37.088037	76.670798
52.115975	45.968492	76.675802
51.949302	43.510391	76.680807
51.127658	48.630173	76.685812
50.584773	43.996974	76.690817
50.082950	45.570297	76.695822
49.123881	51.582008	76.700826
48.585441	29.647811	76.705831
48.168269	50.703826	76.710836
47.867169	45.231066	76.715841
46.570741	37.817242	76.720846
45.405885	53.465218	76.725850
45.106481	39.982663	76.730855
44.916595	40.339683	76.735860
44.148401	39.351601	76.740865
42.972307	36.481996	76.745870
42.365299	49.089379	76.750874
42.013604	40.818495	76.755879
41.459354	46.399243	76.760884
40.728293	44.770097	76.765889
39.864576	46.264161	76.770894
39.045906	55.135177	76.775898
38.616448	34.596942	76.780903
38.164380	37.742952	76.785908
36.940922	43.090298	76.790913
36.608590	44.272218	76.795918
35.723596	47.272205	76.800922
35.665298	40.533816	76.805927
35.122980	42.484718	76.810932
33.814467	44.715002	76.815937
33.268725	41.449580	76.820942
32.652093	59.877469	76.825946
32.229128	55.963006	76.830951
31.679447	51.781734	76.835956
30.137148	51.315167	76.840961
29.818878	45.790092	76.845966
29.154698	59.536162	76.850970
28.714111	46.926048	76.855975
28.339629	53.999568	76.860980
27.669199	55.115516	76.865985
26.839149	52.798782	76.870990
26.038211	57.006391	76.875994
25.881627	52.277753	76.880999
24.739333	53.495918	76.886004
23.797362	52.558158	76.891009
23.502569	47.207074	76.896014
22.810368	50.417942	76.901018
22.046071	51.363680	76.906023
20.932126	46.676036	76.911028
20.246857	52.215307	76.916033
20.226468	54.853125	76.921038
19.600338	53.777930	76.926042
19.095822	56.203509	76.931047
18.406009	53.579723	76.936052
17.416836	49.237769	76.941057
16.765970	53.296893	76.946062
16.373097	51.906591	76.951066
15.887718	47.299061	76.956071
14.816841	53.191009	76.961076
14.083832	51.960860	76.966081
13.870776	47.586096	76.971086
12.965632	54.058670	76.976090
11.981603	55.267465	76.981095
11.108342	63.909442	76.986100
10.703702	50.091267	76.991105
10.685190	55.012963	76.996110
9.853600	63.483990	77.001114
8.649939	49.071015	77.006119
8.215279	48.546378	77.011124
7.560357	52.075309	77.016129
7.191835	53.069238	77.021134
6.289740	60.901471	77.026139
5.133093	51.544203	77.031143
4.848025	55.375225	77.036148
4.039236	50.326599	77.041153
3.695802	54.328276	77.046158