Tue Jun 08 18:01:18 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.265939	107.633681	0.000000
-0.524733	98.133098	0.005005
-1.002784	69.849764	0.010010
-1.940282	17.263095	0.015014
-5.421367	-25.860236	0.020019
-10.467316	-33.493560	0.025024
-15.828742	-23.035296	0.030029
-21.130055	-23.168342	0.035034
-25.272526	-30.083860	0.040038
-29.209921	-23.279658	0.045043
-32.675292	-22.751769	0.050048
-36.100608	-19.713280	0.055053
-39.539365	-27.113373	0.060058
-43.503062	-21.757974	0.065062
-47.308780	-18.000608	0.070067
-51.038030	-14.047154	0.075072
-54.782560	-20.926284	0.080077
-58.546613	-24.199536	0.085082
-62.216602	-26.409774	0.090086
-65.961680	-22.161905	0.095091
-69.536767	-23.186912	0.100096
-73.577732	-21.390765	0.105101
-77.674964	-19.528916	0.110106
-80.988973	-24.167656	0.115110
-85.235769	-18.912483	0.120115
-88.453017	-27.778582	0.125120
-92.254075	-25.094409	0.130125
-96.223621	-15.920717	0.135130
-99.793499	-26.605950	0.140134
-104.041061	-22.688698	0.145139
-107.594864	-21.948233	0.150144
-110.946942	-24.853958	0.155149
-115.004160	-23.526666	0.160154
-118.907566	-31.019103	0.165158
-122.750930	-18.591330	0.170163
-126.557001	-17.403801	0.175168
-129.691590	-19.256619	0.180173
-132.962831	-18.992456	0.185178
-137.126477	-27.988303	0.190182
-141.505704	-23.546368	0.195187
-145.297406	-30.055373	0.200192
-149.218954	-27.258523	0.205197
-153.466922	-22.153080	0.210202
-157.080886	-23.121222	0.215206
-160.678551	-16.024673	0.220211
-163.950249	-18.812310	0.225216
-167.156901	-25.012711	0.230221
-171.502327	-18.939286	0.235226
-174.807773	-18.922236	0.240230
-179.206094	-13.211153	0.245235
-182.742014	-20.085684	0.250240
-186.750192	-25.849022	0.255245
-190.543534	-20.354968	0.260250
-194.051746	-16.538383	0.265254
-197.754237	-19.824442	0.270259
-201.579611	-23.979887	0.275264
-205.341689	-20.404737	0.280269
-209.427177	-16.369933	0.285274
-212.845849	-18.377640	0.290278
-216.753650	-14.548950	0.295283
-220.497806	-23.225108	0.300288
-224.029978	-17.845683	0.305293
-228.020838	-15.108716	0.310298
-231.499175	-30.280802	0.315302
-235.427374	-16.651900	0.320307
-239.249264	-22.089928	0.325312
-243.205396	-17.850718	0.330317
-246.753351	-19.674788	0.335322
-250.216079	-33.606589	0.340326
-254.351532	-20.213689	0.345331
-257.685482	-27.356461	0.350336
-261.518873	-23.407481	0.355341
-265.789283	-20.215588	0.360346
-269.248115	-29.387843	0.365350
-272.981065	-30.906231	0.370355
-276.938216	-21.378894	0.375360
-280.834098	-27.310999	0.380365
-284.504237	-22.553217	0.385370
-287.993006	-29.442055	0.390374
-291.868954	-28.418049	0.395379
-295.289809	-23.013459	0.400384
-299.198742	-27.561824	0.405389
-303.346986	-25.607742	0.410394
-306.778319	-26.362368	0.415398
-310.940271	-17.909007	0.420403
-314.716412	-22.626574	0.425408
-318.297567	-20.972631	0.430413
-321.832198	-17.272991	0.435418
-325.282621	-28.505839	0.440422
-329.708652	-16.183220	0.445427
-333.443449	-16.091616	0.450432
-336.782227	-25.400452	0.455437
-340.718573	-22.774180	0.460442
-344.109154	-16.676901	0.465446
-348.266235	-13.101373	0.470451
-352.176481	-22.124288	0.475456
-355.578292	-14.009293	0.480461
-359.755066	-19.810253	0.485466
-363.411451	-21.167633	0.490470
-367.511506	-16.973494	0.495475
-370.633242	-19.127928	0.500480
-374.435771	-23.725264	0.505485
-378.302654	-22.741815	0.510490
-382.263948	-19.532979	0.515494
-386.228488	-18.295944	0.520499
-389.939772	-30.852440	0.525504
-393.246565	-23.014626	0.530509
-397.737007	-17.805400	0.535514
-401.036562	-21.983769	0.540518
-405.074954	-16.203970	0.545523
-408.432629	-18.071209	0.550528
-411.830883	-21.308229	0.555533
-416.016020	-23.201654	0.560538
-419.609140	-22.709971	0.565542
-423.661100	-22.224827	0.570547
-426.992585	-18.160513	0.575552
-431.369617	-27.818086	0.580557
-435.253474	-17.360237	0.585562
-438.929240	-17.877841	0.590566
-442.126911	-23.120819	0.595571
-446.041080	-23.874207	0.600576
-449.866695	-25.751522	0.605581
-453.780385	-15.138156	0.610586
-457.538147	-29.784492	0.615590
-461.359551	-19.756126	0.620595
-464.714520	-23.391685	0.625600
-468.572456	-23.577637	0.630605
-472.043630	-21.196442	0.635610
-475.752980	-29.034837	0.640614
-480.150827	-22.807676	0.645619
-484.200599	-30.468061	0.650624
-487.790163	-24.863482	0.655629
-491.331082	-19.063970	0.660634
-494.824040	-26.090061	0.665638
-498.420043	-23.164835	0.670643
-502.584177	-23.927783	0.675648
-506.464608	-28.004036	0.680653
-510.379226	-14.958273	0.685658
-513.883940	-18.264966	0.690662
-517.632455	-13.272913	0.695667
-521.278756	-18.991450	0.700672
-524.993321	-16.326497	0.705677
-528.766014	-12.649403	0.710682
-532.351956	-20.997573	0.715686
-536.641252	-23.410209	0.720691
-540.536175	-22.541406	0.725696
-544.184644	-28.373617	0.730701
-547.615542	-20.161537	0.735706
-551.242648	-23.005518	0.740710
-555.308611	-14.400274	0.745715
-558.753910	-12.759979	0.750720
-562.539112	-13.568153	0.755725
-567.116369	-7.936921	0.760730
-570.316113	-24.872291	0.765734
-574.076866	-16.995144	0.770739
-577.751531	-12.044527	0.775744
-581.320040	-16.491583	0.780749
-585.443267	-3.024329	0.785754
-589.099502	-19.876623	0.790758
-593.029426	-13.297046	0.795763
-596.362617	-13.396098	0.800768
-600.350585	-15.974843	0.805773
-604.073471	-12.423856	0.810778
-607.951267	-15.031367	0.815782
-611.764327	-11.532001	0.820787
-615.469655	-25.584458	0.825792
-619.167632	-12.667359	0.830797
-622.424973	-20.621078	0.835802
-626.168169	-24.176469	0.840806
-630.425751	-26.013047	0.845811
-634.643879	-19.485817	0.850816
-637.915067	-16.214801	0.855821
-642.040260	-14.902607	0.860826
-645.150132	-23.188694	0.865830
-649.822629	-18.873575	0.870835
-652.994444	-18.290591	0.875840
-656.552573	-9.234814	0.880845
-660.429664	-12.985474	0.885850
-664.343117	-8.413385	0.890854
-668.291625	-15.043809	0.895859
-672.180891	-16.529110	0.900864
-675.319247	-15.906066	0.905869
-679.026033	-17.000734	0.910874
-682.863512	-27.976191	0.915878
-687.032896	-10.673855	0.920883
-690.944068	-16.910034	0.925888
-694.429378	-16.790288	0.930893
-698.009271	-13.306394	0.935898
-701.704013	-17.531565	0.940902
-705.666127	-16.565433	0.945907
-709.314084	-22.836107	0.950912
-713.003039	-16.311996	0.955917
-716.779528	-16.117393	0.960922
-720.880165	-30.884997	0.965926
-724.922969	-17.337901	0.970931
-728.332704	-11.676768	0.975936
-732.315824	-21.306098	0.980941
-735.648139	-13.431701	0.985946
-739.634376	-27.961177	0.990950
-743.138244	-15.088753	0.995955
-747.171492	-17.119233	1.000960
-750.606840	-16.931444	1.005965
-754.674215	-24.706555	1.010970
-758.676401	-22.033492	1.015974
-762.137630	-13.844868	1.020979
-765.864724	-17.606963	1.025984
-769.274382	-20.364534	1.030989
-772.921880	-11.829350	1.035994
-776.281479	-16.873762	1.040998
-780.720123	-12.173543	1.046003
-784.666995	-17.749868	1.051008
-788.787193	-24.898160	1.056013
-792.886513	-11.235130	1.061018
-795.883332	-22.672900	1.066022
-799.778739	-17.683828	1.071027
-803.389279	-18.224555	1.076032
-806.917825	-15.034367	1.081037
-811.406128	-11.966789	1.086042
-814.829320	-17.353122	1.091046
-818.613129	-12.775921	1.096051
-822.378429	-11.884910	1.101056
-825.845340	-22.095737	1.106061
-830.065934	-11.698984	1.111066
-833.532714	-11.345482	1.116070
-837.442625	-10.142289	1.121075
-841.196590	-10.161429	1.126080
-844.903120	-22.318066	1.131085
-848.639638	-13.135619	1.136090
-852.139480	-15.647924	1.141094
-856.028650	-12.059506	1.146099
-859.802665	-14.210950	1.151104
-863.489941	-25.269242	1.156109
-867.763649	-24.418808	1.161114
-871.425191	-26.714273	1.166118
-874.859436	-21.126981	1.171123
-878.799696	-11.027761	1.176128
-882.491811	-20.806751	1.181133
-886.602601	-15.271066	1.186138
-889.891832	-20.205891	1.191142
-893.566996	-27.252060	1.196147
-897.339643	-27.950392	1.201152
-901.182285	-19.969730	1.206157
-905.403004	-12.542271	1.211162
-908.597212	-27.383171	1.216166
-912.343460	-22.317775	1.221171
-916.599297	-12.548008	1.226176
-920.169691	-14.632517	1.231181
-924.353898	-10.501981	1.236186
-927.276440	-21.602685	1.241190
-930.973888	-19.113218	1.246195
-935.113212	-21.727236	1.251200
-938.438030	-21.933243	1.256205
-942.887372	-17.720468	1.261210
-946.322754	-14.223689	1.266214
-950.219730	-4.383266	1.271219
-953.963510	-15.330732	1.276224
-957.599888	-17.828981	1.281229
-961.943672	-11.919701	1.286234
-965.394182	-21.850210	1.291238
-968.843253	-10.918734	1.296243
-972.582862	-14.168138	1.301248
-976.317346	-19.640221	1.306253
-980.167104	-15.302203	1.311258
-984.129699	-8.018453	1.316262
-987.887449	-4.914288	1.321267
-991.775559	-16.897119	1.326272
-994.878350	-26.639025	1.331277
-998.992294	-19.105484	1.336282
-1002.907316	-23.034819	1.341286
-1006.875410	-11.688576	1.346291
-1010.803821	-8.420497	1.351296
-1013.675601	-14.508785	1.356301
-1018.057240	-10.783179	1.361306
-1021.888921	-16.758756	1.366310
-1025.736774	-13.380953	1.371315
-1029.227119	-14.101192	1.376320
-1032.649220	-14.955899	1.381325
-1036.262662	-10.100686	1.386330
-1040.171499	-17.284615	1.391334
-1044.174519	-12.153708	1.396339
-1048.160400	-10.876103	1.401344
-1051.665257	-20.088704	1.406349
-1055.731448	-16.870347	1.411354
-1059.131483	-10.531348	1.416358
-1062.928295	-18.868875	1.421363
-1066.865044	-14.632680	1.426368
-1070.628842	-19.244708	1.431373
-1074.817390	-4.038216	1.436378
-1078.032042	-24.303854	1.441382
-1081.806281	-12.390488	1.446387
-1085.461460	-13.959810	1.451392
-1089.110737	-20.530676	1.456397
-1092.878825	-15.325207	1.461402
-1096.840406	-13.435198	1.466406
-1100.714327	-20.418629	1.471411
-1104.405782	-14.442027	1.476416
-1108.166948	-16.329815	1.481421
-1112.146593	-14.197498	1.486426
-1115.740902	-20.416226	1.491430
-1119.707785	-15.067660	1.496435
-1123.257508	-18.583591	1.501440
-1126.822218	-24.732396	1.506445
-1131.005103	-14.986807	1.511450
-1134.364450	-21.804769	1.516454
-1138.344117	-15.495645	1.521459
-1141.707902	-21.406593	1.526464
-1145.753578	-18.854781	1.531469
-1149.439814	-11.299425	1.536474
-1153.303517	-26.156573	1.541478
-1156.979640	-16.805855	1.546483
-1160.711442	-13.955849	1.551488
-1164.498598	-23.818497	1.556493
-1168.477759	-13.670919	1.561498
-1172.193035	-22.421780	1.566502
-1175.821962	-20.636584	1.571507
-1180.079780	-16.979051	1.576512
-1183.242615	-23.555606	1.581517
-1187.257958	-16.425246	1.586522
-1191.062785	-17.985748	1.591526
-1194.618698	-19.323356	1.596531
-1198.254880	-18.196448	1.601536
-1202.389277	-22.230800	1.606541
-1205.898039	-21.484555	1.611546
-1209.470524	-23.939873	1.616550
-1213.183588	-19.046887	1.621555
-1217.353274	-19.287174	1.626560
-1221.078252	-28.191042	1.631565
-1224.921000	-16.578807	1.636570
-1228.463947	-18.638161	1.641574
-1232.177887	-16.852131	1.646579
-1235.912976	-17.873560	1.651584
-1239.705129	-15.616628	1.656589
-1243.642149	-8.363888	1.661594
-1247.475141	-15.501035	1.666598
-1250.960467	-19.546162	1.671603
-1255.059160	-10.793790	1.676608
-1258.754667	-22.667715	1.681613
-1262.269128	-18.766354	1.686618
-1266.278814	-18.542268	1.691622
-1270.035844	-13.115541	1.696627
-1274.083553	-6.811582	1.701632
-1277.321975	-10.232435	1.706637
-1280.956944	-14.515894	1.711642
-1284.532473	-15.593497	1.716646
-1288.635733	-9.770604	1.721651
-1292.102213	-9.249822	1.726656
-1296.115980	-9.042769	1.731661
-1300.034911	-16.647433	1.736666
-1304.007392	-15.127569	1.741670
-1307.379934	-15.316406	1.746675
-1311.272467	-13.878156	1.751680
-1315.071095	-21.405183	1.756685
-1318.904863	-14.331156	1.761690
-1322.167768	-20.623193	1.766694
-1326.000035	-17.159392	1.771699
-1330.202343	-17.949708	1.776704
-1333.876345	-18.825237	1.781709
-1338.019602	-17.890959	1.786714
-1341.497079	-20.724424	1.791718
-1344.935350	-14.207742	1.796723
-1348.700975	-15.575111	1.801728
-1352.415035	-19.627435	1.806733
-1356.319725	-17.838531	1.811738
-1360.144750	-17.457406	1.816742
-1363.879660	-22.885630	1.821747
-1367.951042	-15.312100	1.826752
-1371.465610	-28.968687	1.831757
-1375.337951	-18.311173	1.836762
-1378.977347	-18.922233	1.841766
-1382.727633	-22.001278	1.846771
-1386.758758	-17.521633	1.851776
-1390.185873	-26.777266	1.856781
-1393.950312	-9.290138	1.861786
-1397.779035	-24.200397	1.866790
-1401.535818	-12.646204	1.871795
-1405.316681	-7.996389	1.876800
-1408.726022	-17.857383	1.881805
-1412.729320	-16.763141	1.886810
-1416.591399	-14.130123	1.891814
-1419.959766	-20.915498	1.896819
-1424.093993	-17.315271	1.901824
-1427.964105	-22.744681	1.906829
-1431.812419	-5.163778	1.911834
-1435.083713	-21.981452	1.916838
-1438.530818	-19.408651	1.921843
-1443.083084	-17.185158	1.926848
-1446.676096	-19.397155	1.931853
-1451.103205	-17.187655	1.936858
-1454.477964	-23.680608	1.941862
-1457.925331	-23.259675	1.946867
-1461.694192	-15.114398	1.951872
-1465.277936	-16.770648	1.956877
-1469.316647	-11.662043	1.961882
-1472.609857	-16.348219	1.966886
-1476.517895	-16.535310	1.971891
-1480.740063	-12.127354	1.976896
-1484.635212	-21.702330	1.981901
-1488.432116	-20.290214	1.986906
-1492.113535	-26.402449	1.991910
-1495.393816	-26.798809	1.996915
-1499.598548	-18.384288	2.006912
-1500.192993	-22.967365	2.016909
-1497.962021	-16.137671	2.026906
-1495.467320	-25.158119	2.036902
-1492.731815	-22.271954	2.046899
-1491.019279	-27.065230	2.056896
-1489.058380	-23.794236	2.066893
-1487.308806	-19.475199	2.076890
-1485.470692	-18.936930	2.086886
-1483.435189	-16.379456	2.096883
-1481.554101	-19.845326	2.106880
-1479.631441	-19.504958	2.116877
-1477.744659	-16.907704	2.126874
-1475.613499	-15.750289	2.136870
-1473.813612	-17.180312	2.146867
-1471.952495	-19.786327	2.156864
-1470.324041	-16.393396	2.166861
-1468.334611	-21.951935	2.176858
-1466.311425	-16.300609	2.186854
-1464.737034	-17.707697	2.196851
-1462.651860	-23.243556	2.206848
-1460.763061	-12.909614	2.216845
-1459.085295	-19.195939	2.226842
-1457.229843	-15.188320	2.236838
-1454.840185	-19.273501	2.246835
-1453.449426	-17.325718	2.256832
-1451.366817	-23.205754	2.266829
-1449.191600	-17.365542	2.276826
-1447.335549	-15.365294	2.286822
-1445.661334	-18.924449	2.296819
-1443.836924	-14.394952	2.306816
-1442.023263	-18.668494	2.316813
-1439.938031	-25.756341	2.326810
-1437.990279	-27.703786	2.336806
-1436.799026	-23.133100	2.346803
-1434.126426	-23.923793	2.356800
-1432.458700	-21.260037	2.366797
-1430.577647	-24.094728	2.376794
-1428.553549	-21.335687	2.386790
-1426.972571	-23.899882	2.396787
-1425.071497	-20.400423	2.406784
-1423.073852	-24.843489	2.416781
-1421.050348	-22.950642	2.426778
-1419.275907	-23.070497	2.436774
-1417.467455	-27.305191	2.446771
-1415.591959	-23.366208	2.456768
-1413.786853	-17.379798	2.466765
-1412.119549	-17.895031	2.476762
-1409.845920	-22.010051	2.486758
-1407.738277	-18.216857	2.496755
-1406.186319	-11.490200	2.506752
-1404.568939	-13.215287	2.516749
-1402.239533	-17.392845	2.526746
-1400.651230	-18.260071	2.536742
-1398.650210	-14.956796	2.546739
-1396.924247	-17.912642	2.556736
-1394.629648	-21.669640	2.566733
-1393.146055	-13.592262	2.576730
-1391.009566	-14.688813	2.586726
-1389.406837	-18.162159	2.596723
-1387.456872	-14.590059	2.606720
-1385.636082	-18.214287	2.616717
-1383.515613	-18.427159	2.626714
-1381.687240	-19.158167	2.636710
-1379.822104	-13.526673	2.646707
-1377.711030	-13.386981	2.656704
-1376.157736	-11.429939	2.666701
-1374.151663	-16.277549	2.676698
-1372.600342	-14.460862	2.686694
-1370.437689	-21.384926	2.696691
-1368.229411	-16.586192	2.706688
-1366.983888	-13.294613	2.716685
-1365.039627	-18.806620	2.726682
-1362.838698	-21.851547	2.736678
-1360.908498	-17.755153	2.746675
-1359.330925	-17.660950	2.756672
-1357.286967	-22.009584	2.766669
-1355.451664	-17.522227	2.776666
-1353.554323	-18.231477	2.786662
-1351.619016	-18.207018	2.796659
-1349.858913	-19.634503	2.806656
-1348.001819	-14.627230	2.816653
-1345.628993	-17.500118	2.826650
-1343.806984	-20.988981	2.836646
-1342.708113	-11.897782	2.846643
-1340.793979	-13.643387	2.856640
-1338.743521	-13.487335	2.866637
-1336.521850	-14.010416	2.876634
-1334.492766	-19.890694	2.886630
-1333.029189	-17.246368	2.896627
-1331.205969	-14.719143	2.906624
-1329.117174	-13.597848	2.916621
-1327.260968	-11.341078	2.926618
-1325.464899	-7.673745	2.936614
-1323.477713	-20.191896	2.946611
-1321.635440	-19.638855	2.956608
-1319.508044	-11.898083	2.966605
-1317.917453	-14.053664	2.976602
-1316.324649	-13.810300	2.986598
-1314.411156	-12.840289	2.996595
-1312.057994	-16.367017	3.006592
-1310.252558	-19.317510	3.016589
-1308.436314	-16.018021	3.026586
-1306.445396	-20.828615	3.036582
-1304.734138	-15.299098	3.046579
-1303.134641	-14.816195	3.056576
-1300.901254	-20.896747	3.066573
-1299.159356	-17.780509	3.076570
-1297.364018	-23.038873	3.086566
-1295.016456	-18.024917	3.096563
-1293.457099	-24.055697	3.106560
-1292.075202	-15.815766	3.116557
-1289.880943	-9.806416	3.126554
-1287.305367	-18.121766	3.136550
-1286.061282	-23.487400	3.146547
-1284.206086	-18.955604	3.156544
-1281.991577	-22.460082	3.166541
-1280.312902	-21.602673	3.176538
-1278.832154	-22.591681	3.186534
-1276.565999	-16.063117	3.196531
-1274.440411	-20.923305	3.206528
-1272.965769	-16.717798	3.216525
-1271.028613	-16.450960	3.226522
-1269.030216	-17.258151	3.236518
-1267.289689	-16.961492	3.246515
-1265.468576	-19.038477	3.256512
-1263.642450	-21.041627	3.266509
-1261.699013	-15.798578	3.276506
-1259.471135	-16.494206	3.286502
-1257.385976	-13.881515	3.296499
-1255.899704	-15.282879	3.306496
-1254.306781	-9.845253	3.316493
-1252.393961	-11.210400	3.326490
-1250.308915	-15.929640	3.336486
-1248.511147	-15.461402	3.346483
-1246.452328	-20.165069	3.356480
-1244.328677	-14.810684	3.366477
-1242.844880	-19.606481	3.376474
-1241.255832	-13.514901	3.386470
-1239.110906	-13.229982	3.396467
-1237.298313	-17.843143	3.406464
-1235.362502	-17.126702	3.416461
-1233.313878	-18.231797	3.426458
-1231.298193	-20.018110	3.436454
-1229.852722	-18.783515	3.446451
-1228.149541	-18.899745	3.456448
-1225.742565	-16.742654	3.466445
-1223.907524	-21.073136	3.476442
-1222.184214	-21.663122	3.486438
-1220.031487	-19.444184	3.496435
-1218.876452	-19.029961	3.506432
-1216.617232	-16.970796	3.516429
-1214.203981	-15.465688	3.526426
-1212.824593	-14.185749	3.536422
-1211.032629	-25.951442	3.546419
-1208.925159	-21.177198	3.556416
-1207.012990	-21.069261	3.566413
-1205.433788	-23.416498	3.576410
-1203.143579	-19.622928	3.586406
-1201.898343	-17.802221	3.596403
-1199.749904	-18.553734	3.606400
-1197.802051	-18.529777	3.616397
-1195.739825	-20.741410	3.626394
-1193.818704	-12.307509	3.636390
-1192.261914	-11.715264	3.646387
-1190.550539	-20.470228	3.656384
-1188.217949	-12.416435	3.666381
-1186.693887	-22.668698	3.676378
-1184.752397	-22.641666	3.686374
-1182.810345	-16.424538	3.696371
-1180.613835	-17.331710	3.706368
-1178.832178	-17.408438	3.716365
-1177.198877	-14.357280	3.726362
-1175.144274	-12.589397	3.736358
-1173.250997	-16.704986	3.746355
-1171.579654	-16.743007	3.756352
-1169.622790	-12.981886	3.766349
-1167.956326	-17.675053	3.776346
-1165.958092	-16.327476	3.786342
-1163.844699	-17.417181	3.796339
-1161.999197	-14.249510	3.806336
-1160.164945	-16.621560	3.816333
-1158.374884	-10.299273	3.826330
-1156.511857	-14.478823	3.836326
-1154.646145	-16.323529	3.846323
-1152.949526	-15.186967	3.856320
-1150.562771	-15.437939	3.866317
-1149.149563	-10.432594	3.876314
-1147.246701	-18.422496	3.886310
-1145.056438	-14.557979	3.896307
-1143.051246	-17.594876	3.906304
-1141.747198	-17.218076	3.916301
-1139.793328	-11.884669	3.926298
-1137.475581	-20.068720	3.936294
-1135.825978	-11.783397	3.946291
-1133.901351	-13.329550	3.956288
-1132.183979	-11.453545	3.966285
-1130.117874	-10.008131	3.976282
-1128.251532	-12.352481	3.986278
-1126.467790	-14.725725	3.996275
-1124.108487	-12.626783	4.006272
-1122.544405	-14.751263	4.016269
-1121.072506	-15.462841	4.026266
-1119.042435	-8.596044	4.036262
-1116.914240	-13.354252	4.046259
-1115.204059	-16.242862	4.056256
-1113.703699	-12.820669	4.066253
-1111.844207	-9.601231	4.076250
-1109.602732	-13.788046	4.086246
-1107.328252	-16.633644	4.096243
-1105.640682	-11.242241	4.106240
-1104.202698	-9.091399	4.116237
-1101.913709	-10.863325	4.126234
-1099.848377	-7.670532	4.136230
-1098.362221	-11.830402	4.146227
-1096.520337	-16.404671	4.156224
-1094.572425	-15.249186	4.166221
-1092.702728	-10.592921	4.176218
-1090.861275	-10.911869	4.186214
-1089.185098	-12.541020	4.196211
-1087.195362	-11.841673	4.206208
-1084.929997	-11.243401	4.216205
-1083.401593	-11.011417	4.226202
-1081.356093	-18.209674	4.236198
-1079.155245	-14.709743	4.246195
-1077.696224	-23.046680	4.256192
-1075.978406	-15.855527	4.266189
-1073.972144	-15.094988	4.276186
-1071.640500	-16.479405	4.286182
-1070.323913	-19.260897	4.296179
-1068.045926	-16.080889	4.306176
-1066.345325	-4.323259	4.316173
-1064.745618	-10.827648	4.326170
-1062.650011	-14.867669	4.336166
-1060.670668	-20.885125	4.346163
-1058.841368	-15.635020	4.356160
-1057.303512	-13.419896	4.366157
-1055.328879	-14.752887	4.376154
-1053.045499	-9.547543	4.386150
-1051.313882	-14.266086	4.396147
-1049.953269	-14.656985	4.406144
-1047.608628	-5.574060	4.416141
-1045.656926	-10.557241	4.426138
-1043.882887	-15.999978	4.436134
-1041.776321	-10.104266	4.446131
-1040.073542	-14.622619	4.456128
-1038.281337	-17.215042	4.466125
-1036.610971	-18.154321	4.476122
-1034.500528	-17.035408	4.486118
-1032.492701	-14.692293	4.496115
-1030.748681	-17.792587	4.506112
-1028.981351	-10.595288	4.516109
-1026.836999	-7.785546	4.526106
-1025.052668	-14.168673	4.536102
-1023.350773	-15.492368	4.546099
-1021.431804	-6.791628	4.556096
-1019.355558	-15.734468	4.566093
-1017.678730	-13.102923	4.576090
-1015.620347	-15.632750	4.586086
-1013.690325	-11.425489	4.596083
-1012.147848	-16.530073	4.606080
-1010.505355	-7.676338	4.616077
-1008.001597	-9.581916	4.626074
-1006.291675	-13.873050	4.636070
-1004.511409	-16.949521	4.646067
-1002.473569	-13.932570	4.656064
-1000.485599	-11.202279	4.666061
-998.678090	-13.691793	4.676058
-997.047372	-9.752074	4.686054
-995.147426	-5.563351	4.696051
-993.487261	-6.647486	4.706048
-991.540545	-3.426366	4.716045
-989.466842	-9.223267	4.726042
-987.403717	-9.477077	4.736038
-985.620743	-9.014486	4.746035
-984.034885	-12.803340	4.756032
-982.140453	-8.004643	4.766029
-980.125369	-9.950405	4.776026
-978.321096	-14.216231	4.786022
-976.254933	-12.164099	4.796019
-974.449035	-10.217464	4.806016
-972.732780	-7.633769	4.816013
-970.788620	-12.606535	4.826010
-968.602895	-14.889062	4.836006
-966.918803	-12.275341	4.846003
-965.177245	-5.814211	4.856000
-963.085567	-9.642076	4.865997
-961.118571	-6.944918	4.875994
-959.519608	-12.693501	4.885990
-957.622520	-17.233325	4.895987
-955.905016	-21.062553	4.905984
-954.024344	-10.872762	4.915981
-951.727171	-17.102429	4.925978
-950.092089	-15.243838	4.935974
-948.090362	-12.308001	4.945971
-946.337809	-14.550538	4.955968
-944.478768	-13.524373	4.965965
-942.522600	-9.396655	4.975962
-940.638608	-14.214036	4.985958
-938.652641	-15.614130	4.995955
-936.838181	-16.448083	5.005952
-934.767931	-10.872523	5.015949
-933.556812	-4.675612	5.025946
-931.419593	-6.723339	5.035942
-929.396573	-13.378609	5.045939
-927.234631	-12.610340	5.055936
-925.699138	-8.783478	5.065933
-923.769986	-10.278939	5.075930
-921.802464	-11.817346	5.085926
-919.912549	-15.681297	5.095923
-918.698004	-9.726052	5.105920
-916.258771	0.510158	5.115917
-914.041005	-9.668267	5.125914
-912.403366	-8.249575	5.135910
-910.782654	-8.911933	5.145907
-908.723332	-5.107799	5.155904
-907.127236	-5.745774	5.165901
-905.113373	-6.692196	5.175898
-903.180973	-5.726426	5.185894
-901.286090	-11.055092	5.195891
-899.553649	-10.150241	5.205888
-897.149742	-5.942855	5.215885
-895.869952	-6.063339	5.225882
-893.843687	-9.321904	5.235878
-891.894083	-5.189475	5.245875
-889.656400	-8.040901	5.255872
-887.958070	-14.296978	5.265869
-886.146868	-16.373294	5.275866
-884.490017	-15.884663	5.285862
-882.543809	-15.693105	5.295859
-881.098363	-17.115396	5.305856
-878.727618	-10.439342	5.315853
-876.718123	-3.606422	5.325850
-875.138317	-12.601921	5.335846
-873.231964	-6.424343	5.345843
-871.185790	-12.304599	5.355840
-869.220215	-7.396728	5.365837
-867.584071	-8.784564	5.375834
-865.555736	-11.145547	5.385830
-863.671976	-13.968219	5.395827
-861.652266	-7.337419	5.405824
-860.067906	-6.422942	5.415821
-858.432612	-5.109743	5.425818
-856.110612	-9.293661	5.435814
-854.352437	-8.687642	5.445811
-852.807965	-11.696708	5.455808
-850.526590	-11.336210	5.465805
-848.597588	-14.790683	5.475802
-846.788325	-18.703995	5.485798
-845.094901	-18.459939	5.495795
-842.959366	-10.165405	5.505792
-841.309954	-4.775630	5.515789
-839.438000	-10.997074	5.525786
-837.315797	-9.522807	5.535782
-835.603089	-11.857265	5.545779
-833.575914	-9.954873	5.555776
-831.878284	-8.219211	5.565773
-829.816598	-9.063937	5.575770
-828.303300	-12.053812	5.585766
-826.190644	-13.133743	5.595763
-824.468783	-17.992411	5.605760
-822.454133	-5.525402	5.615757
-820.493706	-13.328255	5.625754
-818.830520	-13.146185	5.635750
-816.926359	-13.520043	5.645747
-814.466708	-13.113850	5.655744
-813.046503	-8.273984	5.665741
-811.266742	-12.868705	5.675738
-809.658102	-9.388306	5.685734
-807.387365	-10.528559	5.695731
-805.443295	-9.241068	5.705728
-803.785692	-1.968305	5.715725
-801.763525	-6.894321	5.725722
-800.067949	-8.896614	5.735718
-798.073536	-7.457304	5.745715
-796.265403	-4.996406	5.755712
-794.499127	-4.212721	5.765709
-792.502251	-10.236247	5.775706
-790.166660	-4.248886	5.785702
-788.518869	-9.015394	5.795699
-786.880792	-15.003417	5.805696
-785.047835	-12.296606	5.815693
-783.046922	-8.301375	5.825690
-781.047039	-9.414888	5.835686
-779.209591	-10.542017	5.845683
-777.421035	-6.204045	5.855680
-775.798209	-8.076859	5.865677
-773.806416	-13.723261	5.875674
-771.846698	-10.965481	5.885670
-769.660394	-6.324666	5.895667
-768.153923	-5.486500	5.905664
-766.251112	-7.086847	5.915661
-764.213308	-1.170086	5.925658
-762.476119	-6.890166	5.935654
-760.323944	-7.191164	5.945651
-758.317516	-13.017918	5.955648
-756.835106	-1.433323	5.965645
-755.056010	0.997009	5.975642
-753.158883	-1.027212	5.985638
-751.284358	-9.965369	5.995635
-749.097024	-2.005717	6.005632
-747.470965	-5.165496	6.015629
-745.835000	-0.638491	6.025626
-743.752467	-5.909195	6.035622
-741.735538	-7.225594	6.045619
-739.757701	-6.758797	6.055616
-738.038964	-9.366162	6.065613
-736.192043	-10.396887	6.075610
-734.230992	-8.349910	6.085606
-732.353744	-6.722099	6.095603
-730.275251	-5.616915	6.105600
-728.774300	-0.666775	6.115597
-726.634398	-3.110870	6.125594
-724.981333	-9.171005	6.135590
-722.710191	-10.136205	6.145587
-721.155592	-8.756145	6.155584
-719.465905	-7.620983	6.165581
-717.589070	-6.712778	6.175578
-715.089108	-8.949125	6.185574
-713.688366	-8.467852	6.195571
-711.943982	-12.157355	6.205568
-709.764665	-10.752107	6.215565
-708.290780	-13.064898	6.225562
-706.165605	-7.493105	6.235558
-703.952404	-10.358024	6.245555
-702.249696	-8.244565	6.255552
-700.450492	-12.720461	6.265549
-698.815436	-10.588672	6.275546
-696.523335	-12.105617	6.285542
-694.823158	-14.986429	6.295539
-693.338496	-14.581995	6.305536
-690.978239	-7.764118	6.315533
-689.273974	-13.239812	6.325530
-687.317533	-15.194350	6.335526
-685.462947	-16.126775	6.345523
-683.546745	-13.909251	6.355520
-681.796169	-17.241346	6.365517
-680.091576	-12.850192	6.375514
-678.115378	-12.629304	6.385510
-675.674573	-16.029261	6.395507
-674.170614	-17.448485	6.405504
-672.367405	-13.798677	6.415501
-670.566439	-15.986183	6.425498
-668.614101	-13.948352	6.435494
-666.870762	-16.302232	6.445491
-664.755550	-7.615609	6.455488
-662.954332	-9.741107	6.465485
-661.159262	-16.899385	6.475482
-659.118420	-20.349260	6.485478
-657.193352	-20.244872	6.495475
-655.481163	-20.594016	6.505472
-653.735783	-14.969274	6.515469
-651.950680	-11.989793	6.525466
-649.407148	-14.530386	6.535462
-647.801221	-16.076969	6.545459
-645.984033	-14.004079	6.555456
-644.466595	-15.312181	6.565453
-642.472585	-13.961256	6.575450
-640.720113	-21.753647	6.585446
-638.666118	-14.079321	6.595443
-636.542238	-13.831194	6.605440
-634.633074	-18.955510	6.615437
-632.733454	-16.936281	6.625434
-630.842667	-13.643738	6.635430
-629.445668	-18.566343	6.645427
-627.480372	-8.912575	6.655424
-625.486015	-7.781045	6.665421
-623.496335	-9.434970	6.675418
-621.636099	-12.426217	6.685414
-619.669808	-14.046090	6.695411
-617.743736	-15.096276	6.705408
-616.174365	-15.445006	6.715405
-614.348224	-12.995814	6.725402
-612.085789	-17.030274	6.735398
-610.508391	-15.079445	6.745395
-608.795023	-15.213382	6.755392
-606.569748	-16.527530	6.765389
-604.910312	-17.025688	6.775386
-603.007284	-19.020822	6.785382
-600.870565	-23.158591	6.795379
-599.245743	-18.750948	6.805376
-597.450863	-9.248534	6.815373
-595.358607	-13.994022	6.825370
-593.351451	-17.293836	6.835366
-591.613505	-19.242458	6.845363
-589.650826	-14.537091	6.855360
-587.926833	-13.187234	6.865357
-586.373163	-16.494597	6.875354
-584.161063	-19.771872	6.885350
-582.317449	-16.097734	6.895347
-580.443187	-17.274573	6.905344
-578.570071	-19.879912	6.915341
-576.402903	-22.692605	6.925338
-574.540772	-18.175885	6.935334
-572.713261	-19.672725	6.945331
-571.195033	-17.338251	6.955328
-569.227094	-15.127971	6.965325
-567.515387	-14.345897	6.975322
-565.354218	-15.844260	6.985318
-563.218994	-16.673817	6.995315
-561.394582	-10.413255	7.005312
-560.013510	-19.103846	7.015309
-558.242632	-13.841499	7.025306
-555.954417	-17.430208	7.035302
-554.177433	-21.991555	7.045299
-552.140778	-17.450230	7.055296
-550.258545	-15.807385	7.065293
-548.582194	-16.155082	7.075290
-546.371316	-18.426309	7.085286
-544.944845	-13.229750	7.095283
-543.060049	-11.192127	7.105280
-540.957034	-18.425729	7.115277
-539.074578	-17.889122	7.125274
-537.156234	-15.104371	7.135270
-535.469159	-13.916520	7.145267
-533.365806	-16.082741	7.155264
-531.679108	-16.184802	7.165261
-529.970613	-14.434282	7.175258
-527.834949	-14.291275	7.185254
-525.764179	-18.425996	7.195251
-524.065771	-19.208251	7.205248
-522.232992	-24.340759	7.215245
-520.409958	-22.671146	7.225242
-518.343604	-15.501192	7.235238
-516.594401	-11.587133	7.245235
-514.774185	-15.149671	7.255232
-512.816088	-20.370864	7.265229
-510.965468	-16.853215	7.275226
-509.006193	-17.398040	7.285222
-507.226066	-23.415483	7.295219
-505.474248	-17.532123	7.305216
-503.604897	-19.245973	7.315213
-501.338667	-18.143643	7.325210
-499.725366	-16.887790	7.335206
-497.715434	-18.510750	7.345203
-496.002711	-11.768990	7.355200
-494.022798	-15.494872	7.365197
-492.243393	-17.620512	7.375194
-490.537181	-21.080485	7.385190
-488.504094	-13.483903	7.395187
-486.264469	-16.859915	7.405184
-484.689540	-14.177863	7.415181
-482.590738	-14.885730	7.425178
-481.165491	-20.447856	7.435174
-479.398019	-13.564905	7.445171
-477.342634	-14.600067	7.455168
-475.161846	-14.007117	7.465165
-473.329443	-12.648938	7.475162
-471.497131	-18.478903	7.485158
-469.699677	-18.164416	7.495155
-467.708589	-12.444999	7.505152
-466.031302	-15.206004	7.515149
-464.195963	-15.267541	7.525146
-462.235694	-15.534679	7.535142
-460.315737	-10.029511	7.545139
-458.249892	-8.328808	7.555136
-456.731811	-16.044176	7.565133
-454.804465	-15.241746	7.575130
-452.771025	-15.843929	7.585126
-450.745220	-14.117778	7.595123
-449.333030	-12.606478	7.605120
-447.236647	-15.383652	7.615117
-445.160868	-15.695893	7.625114
-443.646602	-15.533186	7.635110
-441.515176	-15.952196	7.645107
-439.521485	-20.391805	7.655104
-437.632675	-16.571617	7.665101
-435.897812	-18.137085	7.675098
-434.311286	-12.477084	7.685094
-432.169106	-10.456693	7.695091
-429.993203	-11.177763	7.705088
-428.167577	-5.847283	7.715085
-426.391440	-9.969359	7.725082
-424.615054	-15.722528	7.735078
-423.016324	-7.915833	7.745075
-421.008054	-7.877783	7.755072
-418.975217	-15.270822	7.765069
-417.192627	-19.745741	7.775066
-415.165045	-19.747757	7.785062
-413.126944	-21.251020	7.795059
-411.492130	-21.874908	7.805056
-409.865408	-19.175629	7.815053
-407.822678	-16.076619	7.825050
-405.806615	-11.893701	7.835046
-403.935765	-19.650207	7.845043
-401.935883	-20.320119	7.855040
-400.407383	-11.699873	7.865037
-398.448522	-13.834528	7.875034
-396.695937	-17.962037	7.885030
-394.705150	-15.763499	7.895027
-392.798873	-15.889343	7.905024
-390.798493	-14.235078	7.915021
-388.783921	-15.486890	7.925018
-386.982630	-19.015306	7.935014
-385.376833	-10.496050	7.945011
-383.218630	-19.651501	7.955008
-381.669201	-15.281420	7.965005
-379.746703	-15.120349	7.975002
-377.626985	-18.024407	7.984998
-375.847868	-18.179413	7.994995
-373.844285	-17.875744	8.004992
-372.139011	-10.424423	8.014989
-370.236971	-18.149908	8.024986
-368.790973	-21.076715	8.034982
-366.401058	-20.280481	8.044979
-364.371078	-21.395019	8.054976
-362.746938	-23.058845	8.064973
-360.871866	-19.529909	8.074970
-358.879992	-16.100052	8.084966
-357.012054	-17.701360	8.094963
-355.312782	-19.946390	8.104960
-353.321513	-17.580344	8.114957
-351.644144	-20.991847	8.124954
-349.645974	-20.855996	8.134950
-347.571284	-18.346962	8.144947
-345.843007	-15.258401	8.154944
-343.904307	-14.062259	8.164941
-342.530566	-17.767489	8.174938
-340.462918	-21.421410	8.184934
-338.053314	-19.443289	8.194931
-336.322538	-20.634540	8.204928
-334.642164	-13.779659	8.214925
-332.859535	-18.574679	8.224922
-330.722078	-16.898055	8.234918
-328.811837	-17.459289	8.244915
-326.885520	-18.014584	8.254912
-325.391994	-18.122163	8.264909
-323.569009	-17.485549	8.274906
-321.468496	-21.124153	8.284902
-319.460217	-17.198724	8.294899
-317.974005	-15.249533	8.304896
-315.712115	-20.774907	8.314893
-314.014556	-18.677402	8.324890
-311.841258	-18.598447	8.334886
-310.210429	-13.468469	8.344883
-308.445089	-16.333842	8.354880
-306.443971	-18.292721	8.364877
-304.622434	-16.756341	8.374874
-302.523894	-19.772926	8.384870
-300.637264	-19.780353	8.394867
-299.094092	-17.275373	8.404864
-297.222537	-11.194689	8.414861
-295.018037	-20.602686	8.424858
-293.150699	-24.555790	8.434854
-291.421131	-24.026446	8.444851
-289.620940	-21.924403	8.454848
-288.051995	-18.770153	8.464845
-285.972822	-23.354388	8.474842
-283.896163	-27.934238	8.484838
-281.811894	-22.391169	8.494835
-280.019559	-17.037524	8.504832
-278.359278	-24.526272	8.514829
-276.481421	-26.528812	8.524826
-274.373781	-25.034378	8.534822
-272.661478	-20.153119	8.544819
-270.881376	-14.212452	8.554816
-269.080866	-10.503113	8.564813
-267.130953	-13.440836	8.574810
-264.797068	-15.738167	8.584807
-263.179264	-17.090628	8.594803
-261.725881	-17.980151	8.604800
-260.048094	-15.694666	8.614797
-257.769943	-16.669529	8.624794
-255.679385	-16.807161	8.634791
-253.474484	-12.879458	8.644787
-251.756377	-19.996736	8.654784
-250.347364	-20.611084	8.664781
-248.412296	-10.820713	8.674778
-246.162598	-9.926853	8.684775
-244.347903	-14.180761	8.694771
-242.570960	-19.501202	8.704768
-240.760485	-12.019648	8.714765
-239.140885	-13.826512	8.724762
-236.863610	-14.492155	8.734759
-235.114325	-17.025534	8.744755
-232.667936	-24.797696	8.754752
-231.761893	-23.691163	8.764749
-229.367375	-23.750495	8.774746
-227.439525	-22.522404	8.784743
-225.166347	-26.033680	8.794739
-224.672047	-27.419893	8.804736
-222.309912	-23.429825	8.814733
-220.074295	-33.194864	8.824730
-217.824161	-22.945531	8.834727
-216.296759	-26.322572	8.844723
-214.731280	-26.504504	8.854720
-212.689327	-27.481913	8.864717
-210.918026	-22.473211	8.874714
-208.722161	-26.403979	8.884711
-206.331232	-29.345384	8.894707
-205.295153	-28.827096	8.904704
-203.722946	-28.798737	8.914701
-201.644438	-26.976382	8.924698
-199.414010	-29.110101	8.934695
-197.574762	-29.928245	8.944691
-195.991940	-22.968047	8.954688
-193.871744	-21.530267	8.964685
-191.789759	-22.071496	8.974682
-189.864532	-21.993806	8.984679
-188.089643	-23.344330	8.994675
-186.621770	-24.073881	9.004672
-184.772389	-19.530288	9.014669
-182.487107	-23.860926	9.024666
-180.443703	-27.735893	9.034663
-178.881592	-24.719942	9.044659
-177.106227	-21.171848	9.054656
-175.320617	-24.627543	9.064653
-173.363504	-19.230971	9.074650
-171.221991	-24.833649	9.084647
-169.087019	-19.043511	9.094643
-167.648550	-30.730896	9.104640
-165.904999	-21.902795	9.114637
-163.823077	-22.632518	9.124634
-162.005484	-22.746613	9.134631
-160.074107	-23.948092	9.144627
-158.268845	-25.987932	9.154624
-156.457538	-28.183337	9.164621
-154.164060	-26.734153	9.174618
-152.755811	-22.248873	9.184615
-150.822594	-31.048684	9.194611
-148.927038	-27.619204	9.204608
-147.023018	-20.799038	9.214605
-145.093571	-28.595143	9.224602
-142.840993	-29.684128	9.234599
-141.253182	-22.463128	9.244595
-139.616698	-19.261517	9.254592
-137.332394	-22.319767	9.264589
-135.625834	-22.515985	9.274586
-133.939705	-22.179110	9.284583
-131.983489	-18.711411	9.294579
-130.004509	-16.368051	9.304576
-128.179363	-17.125654	9.314573
-126.593959	-15.346749	9.324570
-124.338889	-21.285056	9.334567
-122.733984	-19.350222	9.344563
-120.657920	-9.449982	9.354560
-118.919478	-10.263851	9.364557
-116.984509	-14.730019	9.374554
-115.080363	-21.825804	9.384551
-112.758940	-17.163146	9.394547
-111.301434	-15.631841	9.404544
-109.671528	-21.261375	9.414541
-107.520751	-15.174734	9.424538
-105.750033	-21.415705	9.434535
-103.621626	-19.506611	9.444531
-102.020335	-16.610775	9.454528
-100.228496	-17.100231	9.464525
-98.133723	-17.342456	9.474522
-96.296128	-21.701016	9.484519
-94.574590	-19.770759	9.494515
-92.619395	-22.409744	9.504512
-90.651318	-16.162924	9.514509
-88.981464	-18.228526	9.524506
-86.910114	-21.562851	9.534503
-84.713619	-18.110644	9.544499
-83.068712	-17.074262	9.554496
-81.469189	-16.819739	9.564493
-79.810870	-12.974088	9.574490
-77.309607	-16.374226	9.584487
-75.255534	-17.204261	9.594483
-73.913727	-17.668705	9.604480
-71.919415	-14.937474	9.614477
-70.062996	-15.331679	9.624474
-68.185628	-22.427993	9.634471
-66.554447	-17.668292	9.644467
-64.384689	-21.726524	9.654464
-62.229911	-18.596762	9.664461
-60.895409	-20.023092	9.674458
-58.588108	-18.665151	9.684455
-56.889775	-16.754612	9.694451
-54.794617	-19.182428	9.704448
-53.241172	-20.220651	9.714445
-51.384924	-20.370180	9.724442
-49.614607	-16.311335	9.734439
-47.518429	-18.387185	9.744435
-45.517554	-20.166089	9.754432
-43.841794	-18.009803	9.764429
-41.756590	-20.668689	9.774426
-40.054655	-26.207795	9.784423
-38.312153	-21.516574	9.794419
-36.458624	-21.472370	9.804416
-34.408883	-19.168765	9.814413
-32.426067	-18.847945	9.824410
-30.621071	-16.688124	9.834407
-28.839267	-17.041853	9.844403
-26.660982	-15.981899	9.854400
-24.928770	-14.254609	9.864397
-23.038285	-15.786536	9.874394
-21.234421	-15.931023	9.884391
-19.386396	-12.560913	9.894387
-17.539115	-6.751001	9.904384
-15.359586	-11.529788	9.914381
-13.493929	-11.365928	9.924378
-11.842804	-22.245570	9.934375
-10.066012	-21.928146	9.944371
-8.041261	-19.932860	9.954368
-6.451326	-16.283338	9.964365
-4.679103	-10.240021	9.974362
-3.257522	9.103582	9.984359
-2.286858	58.474144	9.994355
-0.977282	123.263166	10.004352
0.000000	180.865541	10.009357
0.777697	226.750241	10.014362
1.406011	264.649092	10.019367
1.696025	298.091638	10.024371
2.564423	311.476089	10.029376
2.626754	348.089090	10.034381
2.921026	354.580734	10.039386
3.076782	371.372685	10.044391
3.553378	392.011858	10.049395
3.397983	390.274496	10.054400
3.529657	409.597228	10.059405
3.659898	421.320249	10.064410
3.700548	423.991473	10.069415
3.974654	446.305902	10.074419
4.273288	442.990345	10.079424
4.075568	451.881435	10.084429
4.150603	447.463071	10.089434
4.577629	450.313175	10.094439
4.173545	458.416259	10.099443
4.634885	456.205657	10.104448
4.527109	455.356144	10.109453
4.331319	446.107019	10.114458
4.483758	461.038123	10.119463
4.364519	467.626371	10.124467
4.616797	466.634600	10.129472
4.504423	467.945800	10.134477
4.815434	487.524055	10.139482
5.175260	493.846628	10.144487
4.774059	482.042917	10.149491
4.847535	478.225187	10.154496
4.716396	482.980807	10.159501
4.794073	492.019299	10.164506
4.920391	499.276750	10.169511
4.979760	514.590561	10.174515
5.088540	504.212372	10.179520
4.899129	512.206047	10.184525
5.452315	515.958187	10.189530
5.297156	506.011687	10.194535
4.900335	518.644993	10.199539
5.487616	515.425978	10.204544
5.512036	534.518973	10.209549
5.580028	520.269594	10.214554
5.651693	517.755151	10.219559
5.518434	528.604513	10.224563
5.458511	523.484553	10.229568
5.258465	532.534766	10.234573
5.193637	530.042145	10.239578
5.610993	526.082549	10.244583
5.472907	530.792797	10.249587
5.600681	536.645585	10.254592
5.666430	535.246067	10.259597
5.376986	541.515777	10.264602
5.617891	565.606413	10.269607
5.519731	570.048518	10.274611
5.904058	571.285221	10.279616
5.915999	573.887579	10.284621
5.966421	572.324507	10.289626
6.120089	574.504286	10.294631
5.977508	578.335870	10.299635
5.958342	572.328271	10.304640
5.797554	586.927159	10.309645
5.878081	588.765017	10.314650
6.311273	597.976292	10.319655
6.324228	614.739702	10.324659
6.729468	606.077413	10.329664
6.709650	621.721872	10.334669
6.594382	613.800125	10.339674
6.449038	609.804755	10.344679
6.672051	617.598694	10.349683
6.654075	614.272652	10.354688
6.472812	624.494800	10.359693
6.588383	625.613382	10.364698
6.783665	614.557146	10.369703
6.859884	633.815062	10.374707
7.131794	629.831827	10.379712
7.060534	622.345414	10.384717
7.054606	630.559131	10.389722
7.286602	623.942804	10.394727
6.947312	635.735834	10.399731
7.025442	627.591056	10.404736
6.871098	633.225810	10.409741
6.751049	639.436910	10.414746
7.113480	626.281266	10.419751
7.040698	639.842375	10.424755
7.384916	636.665011	10.429760
7.098214	634.452384	10.434765
7.179895	641.429009	10.439770
7.436558	642.288932	10.444775
7.404458	644.185975	10.449779
7.302904	628.619151	10.454784
7.388782	635.804654	10.459789
7.219790	644.413039	10.464794
7.795458	660.723576	10.469799
7.559959	676.554673	10.474803
7.994207	673.760541	10.479808
7.783315	685.624749	10.484813
7.909005	681.504733	10.489818
8.069630	678.111345	10.494823
7.608120	671.178520	10.499827
7.970436	671.494946	10.504832
7.657073	688.372410	10.509837
7.488622	687.509603	10.514842
8.055382	675.512544	10.519847
7.671098	687.239907	10.524851
7.950175	683.933969	10.529856
7.799341	677.841540	10.534861
8.027161	674.031245	10.539866
7.938813	694.197301	10.544871
8.005261	707.596442	10.549875
8.392291	710.194510	10.554880
8.571169	709.579643	10.559885
8.321522	710.164415	10.564890
8.785542	708.236735	10.569895
8.246115	714.119909	10.574899
8.572832	717.119496	10.579904
8.848208	718.140818	10.584909
8.593228	726.965698	10.589914
8.975057	716.621076	10.594919
8.447304	721.795291	10.599923
8.764186	718.233395	10.604928
8.570662	723.482143	10.609933
8.558898	718.754513	10.614938
9.036654	712.351796	10.619943
9.027504	715.676597	10.624947
9.050220	708.040216	10.629952
9.100604	710.060490	10.634957
8.838081	718.620611	10.639962
9.275729	730.382340	10.644967
9.620652	739.117395	10.649971
9.750110	719.678436	10.654976
9.579043	720.374864	10.659981
9.795000	719.322990	10.664986
9.946550	721.994986	10.669991
9.930611	718.466471	10.674995
10.225004	713.582929	10.680000
9.639879	707.487189	10.685005
9.433557	691.119992	10.690010
9.797038	689.037451	10.695015
9.368500	687.721880	10.700019
9.673885	708.309910	10.705024
9.666974	713.046273	10.710029
9.560279	725.610659	10.715034
9.687781	722.110837	10.720039
9.242623	731.241085	10.725043
9.186100	724.329586	10.730048
9.580644	728.040691	10.735053
9.255918	739.224206	10.740058
9.945499	747.934908	10.745063
9.532602	757.038325	10.750067
10.019020	755.776657	10.755072
9.795642	757.563223	10.760077
9.683895	758.720395	10.765082
10.276262	767.683825	10.770087
10.284418	780.826580	10.775091
10.451095	787.648962	10.780096
11.026863	786.526708	10.785101
10.771192	778.613555	10.790106
10.633730	771.639335	10.795111
10.342132	768.826746	10.800115
10.423640	759.890279	10.805120
10.504303	772.896650	10.810125
10.449798	769.495918	10.815130
10.923270	776.000039	10.820135
10.819798	791.209018	10.825139
10.554829	789.055799	10.830144
10.870619	796.764448	10.835149
10.916175	802.576960	10.840154
10.889754	796.348680	10.845159
10.535794	803.448623	10.850163
10.955130	802.436477	10.855168
10.723466	802.358571	10.860173
10.614173	803.482169	10.865178
10.901684	797.174010	10.870183
10.673428	806.509083	10.875187
10.996402	816.148723	10.880192
11.110602	825.436933	10.885197
11.121099	828.626153	10.890202
11.516480	826.429179	10.895207
11.356216	837.984430	10.900211
11.567744	830.994161	10.905216
11.569260	820.558760	10.910221
11.779869	821.048831	10.915226
11.942657	819.668966	10.920231
11.775561	826.037415	10.925235
11.495994	820.690940	10.930240
12.025274	832.184012	10.935245
11.637096	832.339781	10.940250
12.042953	823.081616	10.945255
11.488331	831.789380	10.950259
11.973477	826.376919	10.955264
12.070581	832.895859	10.960269
11.527586	830.073074	10.965274
11.854636	831.297120	10.970279
11.839124	848.585130	10.975283
11.988445	837.497934	10.980288
12.123291	835.526022	10.985293
11.920494	839.922987	10.990298
12.192090	836.268962	10.995303
11.847772	839.487047	11.000307
12.283244	845.908109	11.005312
12.512309	859.922124	11.010317
12.539789	869.416279	11.015322
12.853055	856.446897	11.020327
12.431423	843.694318	11.025331
12.807724	832.448604	11.030336
13.073309	838.224587	11.035341
12.620997	834.473237	11.040346
12.580724	834.977114	11.045351
12.464850	836.938280	11.050355
12.998178	828.686534	11.055360
12.945841	831.770478	11.060365
12.783999	842.351013	11.065370
13.093905	833.352054	11.070375
13.184252	844.665002	11.075379
12.932108	835.727673	11.080384
13.245196	840.490129	11.085389
13.204864	840.921780	11.090394
13.076386	841.156178	11.095399
13.101607	836.452565	11.100403
13.399216	840.960309	11.105408
13.366097	842.477028	11.110413
12.981013	850.755081	11.115418
13.437442	840.004039	11.120423
13.071248	840.323405	11.125427
13.262925	840.826197	11.130432
12.812293	855.673582	11.135437
13.207578	869.968183	11.140442
13.063962	869.750839	11.145447
12.931129	872.098598	11.150451
13.137150	871.212232	11.155456
13.711616	878.163287	11.160461
13.609581	897.279198	11.165466
14.165007	891.912295	11.170471
13.800872	894.876818	11.175475
14.218236	907.276496	11.180480
14.452529	891.589063	11.185485
13.876235	881.380979	11.190490
13.864672	865.775200	11.195495
13.652260	877.369026	11.200499
13.909281	892.118008	11.205504
14.362573	904.704549	11.210509
13.957106	906.218406	11.215514
14.256144	898.151663	11.220519
13.998262	908.318054	11.225523
14.416257	898.139612	11.230528
14.403214	903.195635	11.235533
14.865860	906.899054	11.240538
15.089503	901.581535	11.245543
14.709884	889.718156	11.250547
14.495834	873.998666	11.255552
14.837901	865.933640	11.260557
14.616574	872.131408	11.265562
14.715573	875.781907	11.270567
14.657478	873.172419	11.275571
14.563897	878.676845	11.280576
14.610897	873.332386	11.285581
14.658201	897.321730	11.290586
15.084928	899.384081	11.295591
14.930193	906.560438	11.300595
15.039170	904.864530	11.305600
15.271147	911.268010	11.310605
14.790078	899.179651	11.315610
14.871371	901.464649	11.320615
15.434517	908.114897	11.325619
15.153640	906.827278	11.330624
15.088465	911.261061	11.335629
14.783564	926.029842	11.340634
15.171518	912.673794	11.345639
14.807072	915.945082	11.350643
14.997059	912.284900	11.355648
15.064616	910.232543	11.360653
15.094414	917.657527	11.365658
15.516761	935.808054	11.370663
15.398735	944.551154	11.375667
15.661456	935.609569	11.380672
15.420292	941.106558	11.385677
15.333403	940.956065	11.390682
15.915633	933.270615	11.395687
15.622679	950.761043	11.400691
15.369226	939.156257	11.405696
15.631130	941.383846	11.410701
15.798390	942.846087	11.415706
15.802253	951.762502	11.420711
16.007002	968.345776	11.425715
16.046237	961.632095	11.430720
16.569457	962.465676	11.435725
16.290881	956.566355	11.440730
16.586422	934.903922	11.445735
16.339668	937.334381	11.450739
15.967485	934.063870	11.455744
16.184556	930.856538	11.460749
16.229449	942.802610	11.465754
16.517134	950.021947	11.470759
16.406837	964.031873	11.475763
16.525177	957.442394	11.480768
16.507697	967.299580	11.485773
16.775484	963.500521	11.490778
16.813251	956.927619	11.495783
16.496777	964.238312	11.500787
16.495157	962.240046	11.505792
16.923458	962.884639	11.510797
16.986384	959.360310	11.515802
17.008491	958.895472	11.520807
16.989148	954.916304	11.525811
16.848913	962.227568	11.530816
17.242120	964.626858	11.535821
17.063331	961.153052	11.540826
17.099291	956.677297	11.545831
16.973511	961.149512	11.550835
17.161420	962.723872	11.555840
17.118422	960.625332	11.560845
17.426942	960.787174	11.565850
17.462353	962.431102	11.570855
16.917287	967.365602	11.575859
16.839056	971.556115	11.580864
17.062507	961.568488	11.585869
16.996630	975.714887	11.590874
17.168257	963.674437	11.595879
17.453419	975.519733	11.600883
17.640920	987.644678	11.605888
17.856834	985.072664	11.610893
17.879384	986.659984	11.615898
17.915381	969.794236	11.620903
17.780189	974.909515	11.625907
17.350917	968.428923	11.630912
17.916747	974.548214	11.635917
17.610886	986.119460	11.640922
17.714565	976.273937	11.645927
17.900626	991.862942	11.650931
18.006098	989.552627	11.655936
18.144055	984.636613	11.660941
17.794196	999.597119	11.665946
18.070389	994.917532	11.670951
18.014518	991.820538	11.675955
17.918112	1001.923778	11.680960
18.595249	981.967037	11.685965
18.494626	997.177308	11.690970
18.764990	993.643852	11.695975
18.673958	997.204988	11.700979
18.581091	987.848684	11.705984
18.741237	999.933328	11.710989
18.392723	994.112299	11.715994
18.637222	989.720385	11.720999
18.480869	991.655353	11.726003
18.650719	994.964522	11.731008
18.882663	998.701993	11.736013
18.846259	1004.874422	11.741018
18.701170	998.873250	11.746023
18.868292	997.666310	11.751027
18.714655	997.248182	11.756032
18.525763	994.661100	11.761037
18.273972	1007.122695	11.766042
18.774029	1011.504989	11.771047
18.973310	1025.326892	11.776051
18.848381	1024.501998	11.781056
19.065413	1025.685713	11.786061
19.032605	1035.219517	11.791066
19.074622	1030.377965	11.796071
18.914775	1032.481300	11.801075
18.985905	1025.337780	11.806080
19.470106	1043.657040	11.811085
19.442746	1052.945183	11.816090
19.504878	1043.096478	11.821095
19.807975	1044.434386	11.826099
19.989993	1042.122781	11.831104
19.673600	1032.481879	11.836109
19.449630	1034.345550	11.841114
19.766730	1027.280646	11.846119
19.983614	1036.378086	11.851123
19.777907	1028.670976	11.856128
19.830451	1027.583548	11.861133
19.774367	1030.415146	11.866138
20.174787	1037.594668	11.871143
19.746074	1045.153590	11.876147
20.061887	1051.412491	11.881152
19.799667	1054.843518	11.886157
19.784616	1066.306145	11.891162
19.845931	1054.974146	11.896167
19.997475	1059.909631	11.901171
20.067151	1058.494788	11.906176
20.079025	1057.196041	11.911181
19.847347	1067.853440	11.916186
20.041785	1049.449382	11.921191
19.948094	1068.571571	11.926195
20.690649	1090.636475	11.931200
20.811684	1084.131349	11.936205
20.618413	1089.458335	11.941210
20.562846	1086.058505	11.946215
20.705799	1090.236784	11.951219
20.753497	1092.326648	11.956224
20.884697	1083.716215	11.961229
20.768429	1077.615728	11.966234
20.693371	1063.381696	11.971239
20.765902	1073.019436	11.976243
20.958982	1078.779126	11.981248
21.003238	1083.522618	11.986253
20.882202	1086.408389	11.991258
21.090214	1082.518892	11.996263
20.829496	1091.041012	12.001267
20.825657	1083.594133	12.006272
21.174371	1082.937502	12.011277
20.898632	1082.979257	12.016282
21.181262	1083.773964	12.021287
21.166255	1088.122222	12.026291
21.446760	1086.529518	12.031296
21.425423	1082.206052	12.036301
21.006123	1087.032577	12.041306
21.336458	1091.796891	12.046311
21.087206	1082.143262	12.051315
21.279987	1092.523032	12.056320
21.505177	1090.640204	12.061325
20.991099	1074.714977	12.066330
21.198284	1067.434426	12.071335
21.382378	1065.665622	12.076339
21.108740	1058.038433	12.081344
21.387644	1052.143755	12.086349
21.369672	1058.100282	12.091354
21.252510	1059.441168	12.096359
21.199306	1057.428444	12.101363
21.434607	1064.896027	12.106368
21.254205	1051.844151	12.111373
20.641628	1052.843267	12.116378
20.716079	1056.528807	12.121383
20.902835	1063.060894	12.126387
20.333897	1063.940422	12.131392
20.996675	1080.652522	12.136397
21.192668	1085.843685	12.141402
21.275570	1091.302137	12.146407
21.274272	1090.096435	12.151411
21.161286	1093.600173	12.156416
21.657805	1093.264386	12.161421
21.075518	1089.377361	12.166426
21.235378	1064.415495	12.171431
21.338619	1063.725952	12.176435
21.172267	1060.142622	12.181440
21.511863	1059.686898	12.186445
21.325858	1060.890772	12.191450
21.236614	1063.503455	12.196455
21.113263	1061.246178	12.201459
21.144399	1062.640980	12.206464
21.748916	1056.139023	12.211469
21.687752	1068.908247	12.216474
21.356092	1054.520455	12.221479
21.500107	1059.973549	12.226483
21.092635	1051.203649	12.231488
21.027636	1035.823967	12.236493
20.736862	1041.828839	12.241498
21.124900	1051.753130	12.246503
21.276224	1061.989592	12.251507
20.873013	1063.745051	12.256512
21.067042	1055.092282	12.261517
20.935441	1077.509942	12.266522
21.024337	1061.392529	12.271527
21.139613	1059.127891	12.276531
21.054201	1057.696218	12.281536
21.159865	1061.185355	12.286541
21.171812	1062.499762	12.291546
20.980312	1061.617991	12.296551
21.010639	1067.601766	12.301555
20.869550	1070.754263	12.306560
21.243366	1063.942119	12.311565
21.111858	1075.646169	12.316570
21.251943	1074.399649	12.321575
21.432051	1074.344693	12.326579
21.226011	1079.633601	12.331584
21.239012	1068.777246	12.336589
21.136577	1073.275491	12.341594
21.115647	1067.534847	12.346599
21.230891	1071.566688	12.351603
20.968588	1068.072439	12.356608
21.316905	1063.693099	12.361613
20.859357	1071.205267	12.366618
21.148766	1069.417221	12.371623
21.317544	1074.834495	12.376627
21.430695	1077.392743	12.381632
21.639741	1075.141630	12.386637
21.243649	1070.595841	12.391642
21.152475	1053.545359	12.396647
21.373560	1047.150594	12.401651
21.302851	1047.150090	12.406656
21.544853	1037.095680	12.411661
21.091468	1049.353057	12.416666
21.384589	1049.469777	12.421671
21.143902	1049.906575	12.426675
20.983270	1052.234654	12.431680
21.328678	1045.694626	12.436685
20.902646	1054.154280	12.441690
21.204400	1046.636866	12.446695
21.139912	1051.467283	12.451699
21.212662	1050.522047	12.456704
21.541316	1045.338449	12.461709
21.111170	1050.740377	12.466714
21.229391	1048.338262	12.471719
21.528088	1048.017446	12.476723
21.202203	1045.063447	12.481728
21.637691	1052.298148	12.486733
21.073172	1052.726522	12.491738
21.170244	1032.870356	12.496743
20.846665	1031.871890	12.501747
20.823462	1046.074984	12.506752
20.939268	1051.657254	12.511757
20.793254	1054.584408	12.516762
20.859261	1051.521374	12.521767
21.039193	1052.212108	12.526771
20.830988	1056.938484	12.531776
21.143754	1052.920111	12.536781
20.964259	1057.877223	12.541786
21.129835	1057.733574	12.546791
21.346421	1056.393412	12.551795
20.960063	1059.365722	12.556800
21.093392	1059.543787	12.561805
20.891823	1059.821510	12.566810
20.901494	1068.427521	12.571815
20.791494	1067.247959	12.576819
20.849023	1078.150253	12.581824
21.226637	1082.404351	12.586829
21.306436	1090.642296	12.591834
21.217743	1092.740545	12.596839
21.237222	1084.563742	12.601843
20.999037	1078.647185	12.606848
21.351581	1068.022353	12.611853
20.817656	1069.673513	12.616858
21.233159	1080.114957	12.621863
21.537712	1067.397158	12.626867
21.331465	1075.081769	12.631872
21.582964	1067.938883	12.636877
21.165593	1072.565335	12.641882
21.432148	1058.950502	12.646887
21.272336	1059.714488	12.651891
20.912532	1068.908061	12.656896
21.384806	1066.059184	12.661901
21.274272	1066.808800	12.666906
21.322788	1068.941942	12.671911
21.224758	1064.683736	12.676915
21.205004	1078.626925	12.681920
21.248101	1066.222378	12.686925
21.133686	1073.654400	12.691930
21.195807	1064.464503	12.696935
21.513002	1065.910917	12.701939
21.084413	1073.597332	12.706944
21.405619	1057.112065	12.711949
20.971645	1051.974353	12.716954
20.971603	1038.934196	12.721959
20.905008	1047.758931	12.726963
21.345208	1061.147584	12.731968
21.802498	1061.781291	12.736973
21.002225	1050.493202	12.741978
21.074138	1040.884402	12.746983
21.087216	1042.727168	12.751987
20.933137	1041.534639	12.756992
20.627489	1040.119412	12.761997
21.071200	1055.717201	12.767002
21.435029	1070.765410	12.772007
21.393662	1068.597497	12.777011
21.613966	1052.813616	12.782016
21.679452	1043.971313	12.787021
21.250495	1040.361959	12.792026
21.476068	1039.661312	12.797031
21.567677	1038.015736	12.802035
21.513333	1037.408477	12.807040
21.412005	1033.821109	12.812045
21.393920	1035.463954	12.817050
21.195026	1029.284889	12.822055
21.264251	1011.574581	12.827059
21.006882	1018.224244	12.832064
21.117236	1015.889009	12.837069
20.666915	1014.215169	12.842074
20.719973	1025.644378	12.847079
21.195597	1034.219822	12.852083
21.020260	1042.007670	12.857088
20.771855	1031.231687	12.862093
20.938296	1038.267379	12.867098
21.140934	1032.268942	12.872103
20.916201	1030.319184	12.877107
20.577222	1034.072841	12.882112
20.915689	1025.874140	12.887117
20.630130	1034.868647	12.892122
20.774315	1042.786843	12.897127
20.943264	1058.677666	12.902131
21.157292	1071.304182	12.907136
21.265806	1069.354519	12.912141
21.307531	1069.281053	12.917146
21.174411	1077.661288	12.922151
21.218961	1073.148105	12.927155
20.781231	1076.264227	12.932160
21.458290	1072.462470	12.937165
21.325199	1074.710435	12.942170
21.116843	1067.329419	12.947175
21.128457	1052.488824	12.952179
20.980636	1053.667202	12.957184
21.176911	1055.388164	12.962189
21.267686	1067.820283	12.967194
21.213543	1060.820594	12.972199
21.115572	1048.943540	12.977203
20.763965	1063.019008	12.982208
21.412665	1071.427824	12.987213
21.064654	1069.321171	12.992218
21.073793	1074.729106	12.997223
21.391573	1071.603558	13.002227
21.149983	1067.161938	13.007232
21.166062	1045.234635	13.012237
20.810150	1048.211196	13.017242
21.116314	1065.248503	13.022247
20.889232	1071.983390	13.027251
20.931605	1085.986987	13.032256
21.547176	1078.434305	13.037261
21.171240	1086.759860	13.042266
21.269776	1075.898703	13.047271
21.126982	1061.452075	13.052275
20.936621	1068.135665	13.057280
21.264518	1075.311060	13.062285
21.138848	1077.209593	13.067290
21.361895	1074.409762	13.072295
21.425428	1057.793015	13.077299
21.496206	1059.515363	13.082304
21.350548	1054.373612	13.087309
21.210854	1049.005840	13.092314
21.245514	1055.312552	13.097319
21.396200	1046.332876	13.102323
20.888420	1049.378503	13.107328
21.000083	1054.831221	13.112333
20.995500	1055.720961	13.117338
21.195387	1059.977892	13.122343
21.041872	1048.958653	13.127347
21.081721	1058.296066	13.132352
21.301501	1041.223861	13.137357
20.925874	1051.965141	13.142362
21.128939	1052.688620	13.147367
21.038743	1053.540143	13.152371
20.983716	1062.458035	13.157376
21.115564	1055.589092	13.162381
20.763355	1057.280542	13.167386
20.815981	1056.390072	13.172391
20.994328	1068.453096	13.177395
21.050391	1078.214059	13.182400
21.428696	1080.780529	13.187405
21.372818	1082.497753	13.192410
21.164099	1075.986405	13.197415
21.262088	1059.067695	13.202419
21.056969	1055.592855	13.207424
21.273857	1050.109865	13.212429
20.980980	1060.901699	13.217434
21.174734	1059.073213	13.222439
21.471829	1055.410423	13.227443
21.230425	1063.662373	13.232448
21.193672	1056.745363	13.237453
21.015058	1052.358476	13.242458
21.149890	1047.377058	13.247463
21.470423	1051.293563	13.252467
20.938514	1053.734642	13.257472
21.434238	1049.637138	13.262477
21.231687	1054.124516	13.267482
21.043332	1061.133418	13.272487
21.175322	1052.287208	13.277491
20.878220	1060.028441	13.282496
20.954338	1045.009424	13.287501
20.793587	1058.251242	13.292506
21.195012	1060.707560	13.297511
21.126012	1060.039260	13.302515
21.085056	1063.496694	13.307520
21.465225	1063.559016	13.312525
21.290769	1057.998252	13.317530
20.948722	1056.626765	13.322535
21.333651	1058.126302	13.327539
20.721651	1062.897833	13.332544
21.056492	1059.712125	13.337549
21.246691	1056.863060	13.342554
21.328525	1060.895890	13.347559
21.148082	1057.357608	13.352563
21.035004	1062.442281	13.357568
21.258952	1061.481384	13.362573
21.163812	1063.095206	13.367578
20.952281	1061.967394	13.372583
21.335965	1061.990430	13.377587
20.976294	1067.938835	13.382592
21.223085	1060.079520	13.387597
21.646818	1064.459521	13.392602
21.420340	1067.715869	13.397607
21.408016	1060.790326	13.402611
21.243551	1069.085141	13.407616
21.188675	1057.910430	13.412621
21.471565	1056.549031	13.417626
21.281490	1064.241127	13.422631
21.268198	1051.894418	13.427635
20.759642	1057.398213	13.432640
21.296314	1066.545447	13.437645
21.492887	1062.529626	13.442650
21.015581	1054.163673	13.447655
21.078727	1047.745067	13.452659
20.731011	1049.196929	13.457664
21.271052	1059.647796	13.462669
21.433884	1064.783454	13.467674
21.055631	1066.688977	13.472679
21.187378	1058.050832	13.477683
21.096029	1066.576662	13.482688
21.134821	1068.865024	13.487693
21.416949	1063.050316	13.492698
21.114018	1053.513672	13.497703
21.329885	1051.019814	13.502707
20.939206	1053.809310	13.507712
21.412702	1049.429827	13.512717
21.164709	1048.120768	13.517722
21.079820	1043.014391	13.522727
21.130382	1040.604929	13.527731
21.029194	1044.655319	13.532736
21.152648	1047.621138	13.537741
20.964965	1047.524636	13.542746
21.053314	1048.093704	13.547751
21.198149	1046.057291	13.552755
21.259764	1043.881198	13.557760
21.314217	1043.906602	13.562765
21.521325	1049.076900	13.567770
21.251107	1046.681385	13.572775
21.425965	1039.844153	13.577779
21.375184	1050.016576	13.582784
21.197783	1047.156329	13.587789
21.392838	1053.448172	13.592794
21.114550	1055.751424	13.597799
21.457788	1041.605956	13.602803
21.374232	1051.139787	13.607808
21.326914	1044.692358	13.612813
21.295500	1038.817733	13.617818
21.048605	1035.845851	13.622823
20.935261	1022.111843	13.627827
21.097191	1038.545034	13.632832
21.089142	1046.929071	13.637837
21.100587	1048.842776	13.642842
21.199054	1054.265388	13.647847
21.344653	1053.473846	13.652851
20.839432	1050.721516	13.657856
21.236102	1041.479403	13.662861
21.342730	1052.959448	13.667866
21.075212	1052.399791	13.672871
21.244807	1033.832641	13.677875
20.828777	1029.060150	13.682880
20.955115	1035.505084	13.687885
21.142101	1048.416482	13.692890
21.217308	1054.641243	13.697895
21.184180	1055.368508	13.702899
21.305956	1058.474749	13.707904
21.191412	1043.034080	13.712909
21.077958	1049.650397	13.717914
21.103653	1052.239424	13.722919
21.195886	1046.923071	13.727923
21.325888	1057.909242	13.732928
20.875857	1040.737143	13.737933
21.099797	1033.860314	13.742938
21.199780	1041.312403	13.747943
21.092632	1045.261183	13.752947
21.377849	1053.029282	13.757952
21.523653	1044.558472	13.762957
21.234514	1021.171687	13.767962
21.099030	1026.885850	13.772967
21.085471	1011.579871	13.777971
20.870425	1020.102017	13.782976
20.952696	1018.025807	13.787981
21.130391	1015.379815	13.792986
21.132611	1024.543659	13.797991
21.193590	1013.879248	13.802995
20.956354	1023.344674	13.808000
21.085822	1031.615520	13.813005
21.297027	1038.107878	13.818010
20.967574	1028.546980	13.823015
21.079831	1035.183013	13.828019
20.969033	1049.147707	13.833024
21.094752	1052.526429	13.838029
21.264916	1059.688993	13.843034
21.241856	1061.822169	13.848039
21.447229	1051.679688	13.853043
21.306618	1040.812190	13.858048
21.485378	1029.024282	13.863053
20.985972	1024.669115	13.868058
20.997553	1034.386756	13.873063
21.259168	1023.128200	13.878067
21.095863	1024.380284	13.883072
20.900878	1022.050821	13.888077
21.170504	1020.602094	13.893082
20.922739	1021.991422	13.898087
21.145035	1025.615291	13.903091
21.003856	1033.871357	13.908096
21.362820	1037.227848	13.913101
21.132671	1031.789538	13.918106
21.305361	1034.324148	13.923111
21.291086	1021.864736	13.928115
21.107923	1032.378793	13.933120
21.413681	1022.800567	13.938125
21.171776	1033.091406	13.943130
20.852228	1023.741972	13.948135
21.468323	1020.039890	13.953139
21.147353	1026.621514	13.958144
20.976985	1018.710191	13.963149
21.022995	1023.678760	13.968154
20.766620	1033.149842	13.973159
20.942346	1019.389168	13.978163
20.840443	1030.289554	13.983168
21.511209	1038.265489	13.988173
21.071562	1032.110728	13.993178
21.058081	1035.748182	13.998183
21.407283	1018.012758	14.003187
20.979788	1030.451603	14.008192
21.097545	1026.729425	14.013210
21.167770	1024.537696	14.018227
20.991951	1028.921323	14.023245
21.229247	1036.111897	14.028263
21.215895	1045.829105	14.033280
21.092780	1042.098749	14.038298
21.158574	1046.940600	14.043315
21.064323	1061.472451	14.048333
21.324491	1055.899860	14.053351
21.192027	1069.050761	14.058368
21.270519	1058.328599	14.063386
21.442937	1070.027513	14.068403
21.492006	1063.300075	14.073421
21.770554	1058.800794	14.078439
20.908693	1048.242231	14.083456
20.975982	1054.493384	14.088474
21.295117	1058.320860	14.093491
21.340790	1066.964887	14.098509
21.319810	1058.680442	14.103527
21.213855	1066.020047	14.108544
21.350762	1070.487085	14.113562
21.509985	1068.784855	14.118579
21.157286	1076.569558	14.123597
21.391806	1065.916710	14.128615
21.414002	1067.151981	14.133632
21.448920	1061.093559	14.138650
21.497758	1074.689006	14.143667
21.377611	1078.765047	14.148685
21.685633	1086.010059	14.153703
21.838345	1094.973571	14.158720
21.395233	1095.622822	14.163738
21.870567	1090.794492	14.168755
21.517971	1096.345546	14.173773
21.710611	1089.069423	14.178791
21.767725	1089.327766	14.183808
21.590204	1093.412466	14.188826
21.965492	1087.578768	14.193843
21.907769	1085.910977	14.198861
22.060475	1093.604703	14.203879
21.589708	1094.452806	14.208896
21.620671	1100.459005	14.213914
22.220081	1093.784452	14.218931
21.613376	1098.952662	14.223949
21.801236	1093.967699	14.228967
21.725748	1093.971589	14.233984
21.740077	1098.816374	14.239002
21.970241	1106.110574	14.244019
21.625258	1103.960494	14.249037
21.774436	1096.865850	14.254055
21.807246	1111.737408	14.259072
21.645992	1098.046634	14.264090
22.100251	1106.457229	14.269107
21.843742	1127.960435	14.274125
22.090840	1139.315467	14.279143
22.265856	1126.948622	14.284160
22.340234	1130.767289	14.289178
22.155866	1114.866502	14.294195
22.197870	1101.588155	14.299213
22.315913	1096.929752	14.304231
22.381543	1097.387832	14.309248
21.955578	1098.418427	14.314266
22.242647	1096.347396	14.319283
22.015127	1099.013784	14.324301
22.317613	1116.086140	14.329319
22.418191	1128.143112	14.334336
22.297814	1129.052016	14.339354
22.472036	1124.279241	14.344371
22.420299	1119.613719	14.349389
22.089912	1105.253848	14.354407
22.203841	1111.142668	14.359424
22.247486	1130.529682	14.364442
22.654984	1128.144667	14.369459
22.132195	1132.233453	14.374477
22.460867	1135.035607	14.379495
22.551209	1131.763947	14.384512
22.445780	1130.955188	14.389530
22.700737	1125.931149	14.394547
22.268161	1138.096864	14.399565
22.519922	1122.734335	14.404583
22.823756	1127.859833	14.409600
22.545710	1132.460245	14.414618
22.751732	1127.279621	14.419635
22.629403	1123.636126	14.424653
22.715967	1130.243483	14.429671
23.160721	1125.897984	14.434688
22.636884	1132.050898	14.439706
22.830273	1126.839366	14.444723
22.907199	1128.236139	14.449741
23.110036	1118.136764	14.454759
22.761464	1106.400696	14.459776
22.684666	1108.548685	14.464794
22.871227	1098.023733	14.469811
22.663306	1104.705194	14.474829
22.727188	1102.858270	14.479847
23.051973	1112.350995	14.484864
22.916666	1117.026150	14.489882
23.143101	1107.123147	14.494899
23.049309	1102.902276	14.499917
22.535119	1094.440544	14.504935
22.740098	1105.860651	14.509952
22.769915	1123.030556	14.514970
23.448060	1121.539373	14.519987
23.011705	1128.561217	14.525005
22.820435	1125.833159	14.530023
23.157739	1135.053256	14.535040
23.240278	1126.028526	14.540058
23.455079	1116.656689	14.545075
23.164656	1118.757835	14.550093
23.057169	1132.571096	14.555111
23.348309	1124.335472	14.560128
22.960704	1124.284206	14.565146
23.169264	1123.569262	14.570163
22.988353	1126.715893	14.575181
23.088173	1127.459474	14.580199
23.040832	1122.044710	14.585216
22.847047	1130.638089	14.590234
23.130162	1123.215719	14.595251
23.110771	1131.537051	14.600269
23.183325	1127.415223	14.605287
23.256879	1123.535764	14.610304
22.640461	1138.142252	14.615322
23.317804	1139.623892	14.620339
23.539434	1158.092554	14.625357
23.474890	1160.846768	14.630375
23.745526	1144.532476	14.635392
23.406157	1143.297646	14.640410
23.332889	1130.189838	14.645427
23.354641	1138.008803	14.650445
23.589112	1147.409152	14.655463
23.653055	1149.623968	14.660480
23.526829	1161.150907	14.665498
23.424210	1153.046958	14.670515
23.397389	1166.873193	14.675533
23.199301	1158.976965	14.680551
23.365374	1152.650724	14.685568
23.493700	1159.096983	14.690586
23.722320	1154.832632	14.695603
23.934666	1156.851124	14.700621
23.494100	1158.428759	14.705639
23.618216	1154.956012	14.710656
23.497980	1162.999351	14.715674
23.780946	1164.593891	14.720691
23.736656	1167.977363	14.725709
23.380587	1160.408640	14.730727
23.941377	1163.685218	14.735744
23.918776	1174.473080	14.740762
24.045450	1159.136686	14.745779
24.007890	1163.828169	14.750797
24.007775	1167.549372	14.755815
23.851313	1158.419132	14.760832
24.164723	1163.258725	14.765850
24.127699	1169.375828	14.770867
24.159606	1168.200184	14.775885
23.948381	1157.356747	14.780903
24.226389	1148.568198	14.785920
24.202267	1167.572749	14.790938
24.035927	1163.661176	14.795955
24.001925	1153.374414	14.800973
23.663336	1162.941536	14.805991
24.522067	1164.746439	14.811008
24.189903	1168.890352	14.816026
24.091377	1165.131340	14.821043
24.532205	1171.532293	14.826061
23.799236	1167.947417	14.831079
24.256604	1172.296543	14.836096
23.968093	1181.403870	14.841114
24.470902	1188.007607	14.846131
24.660662	1192.291588	14.851149
24.274088	1190.513618	14.856167
24.786882	1184.866563	14.861184
24.750460	1170.577107	14.866202
24.207196	1163.016066	14.871219
24.556083	1159.004345	14.876237
24.166731	1155.523169	14.881255
24.432241	1160.079611	14.886272
24.100429	1166.566968	14.891290
24.301830	1175.581631	14.896307
24.582202	1185.101702	14.901325
24.594279	1193.519256	14.906343
24.548080	1188.131835	14.911360
24.788394	1192.515819	14.916378
24.649560	1195.980474	14.921395
24.697139	1185.600956	14.926413
24.718220	1195.075719	14.931431
24.552953	1197.047139	14.936448
24.965845	1196.883429	14.941466
24.612679	1196.256918	14.946483
24.864648	1188.734730	14.951501
24.494863	1191.877927	14.956519
24.615907	1186.509868	14.961536
24.434000	1186.849748	14.966554
24.723180	1192.452624	14.971571
24.711851	1197.186081	14.976589
24.232433	1196.909590	14.981607
25.003647	1194.703565	14.986624
24.417707	1187.089588	14.991642
24.438591	1200.379676	14.996659
24.987080	1206.640520	15.001677
25.198905	1217.119690	15.006695
25.573111	1202.871227	15.011712
25.347439	1187.390081	15.016730
25.167587	1191.805944	15.021747
25.612701	1177.976091	15.026765
25.513673	1176.572480	15.031783
25.588589	1174.946510	15.036800
25.605977	1179.791583	15.041818
25.698543	1175.070197	15.046835
25.560082	1153.681900	15.051853
25.042630	1152.068119	15.056871
25.295022	1145.183335	15.061888
24.985912	1140.919443	15.066906
24.830825	1145.362151	15.071923
25.388001	1154.600473	15.076941
25.322658	1176.939548	15.081959
25.351213	1167.102720	15.086976
25.552228	1172.390756	15.091994
25.386097	1173.911890	15.097011
25.329215	1163.138451	15.102029
25.536468	1176.232772	15.107047
25.573958	1162.923647	15.112064
25.477297	1150.744320	15.117082
25.491156	1150.869911	15.122099
25.778922	1136.726887	15.127117
25.299675	1131.232617	15.132135
25.289703	1139.823227	15.137152
25.431294	1151.099499	15.142170
25.361245	1167.468398	15.147187
25.474479	1169.619249	15.152205
25.925413	1175.255020	15.157223
25.695379	1171.815429	15.162240
25.554133	1175.418300	15.167258
25.123439	1176.093380	15.172275
25.187387	1169.194434	15.177293
25.198866	1173.884206	15.182311
25.325555	1175.142912	15.187328
25.264853	1183.740669	15.192346
25.838599	1202.228547	15.197363
25.831540	1197.937263	15.202381
25.491558	1204.975297	15.207399
25.713028	1206.913484	15.212416
25.689311	1200.217367	15.217434
25.697538	1205.361288	15.222451
25.751933	1203.509286	15.227469
25.837437	1209.487276	15.232487
25.785592	1202.906620	15.237504
25.882324	1211.048228	15.242522
25.643859	1209.198402	15.247539
25.932066	1214.519932	15.252557
25.887697	1231.126641	15.257575
26.151923	1229.802489	15.262592
26.025293	1233.469408	15.267610
26.182186	1230.510363	15.272627
26.314806	1228.697706	15.277645
26.221380	1239.259545	15.282663
26.208638	1236.386675	15.287680
26.204878	1233.328784	15.292698
26.132154	1240.645449	15.297715
26.537920	1230.193464	15.302733
26.360466	1238.962464	15.307751
26.286744	1230.535776	15.312768
26.405694	1229.939743	15.317786
26.267571	1239.197319	15.322803
26.869427	1227.243475	15.327821
26.921563	1227.377072	15.332839
26.786534	1220.440165	15.337856
26.848079	1203.920301	15.342874
26.395503	1202.432017	15.347891
26.798523	1194.063385	15.352909
26.902154	1204.534323	15.357927
26.422549	1206.449787	15.362944
27.023424	1199.339074	15.367962
27.025966	1207.024348	15.372979
26.630037	1198.161146	15.377997
26.345864	1205.803444	15.383015
26.548359	1200.382041	15.388032
26.475662	1197.752154	15.393050
26.585143	1196.004497	15.398067
26.611422	1202.877362	15.403085
26.489701	1201.664270	15.408103
26.330442	1199.962690	15.413120
26.943995	1204.801232	15.418138
26.525206	1209.962852	15.423155
26.923007	1222.764282	15.428173
26.835652	1229.240069	15.433191
26.993890	1233.192822	15.438208
27.062811	1227.228514	15.443226
26.980703	1242.051784	15.448243
27.189631	1224.329358	15.453261
26.920462	1212.112232	15.458279
26.882183	1206.069453	15.463296
27.055817	1214.017941	15.468314
26.731235	1229.356435	15.473331
27.260811	1224.817610	15.478349
27.002272	1227.333025	15.483367
26.878737	1226.949450	15.488384
27.234402	1218.907849	15.493402
26.907793	1232.523315	15.498419
26.972846	1233.698491	15.503437
27.155045	1234.422047	15.508455
26.911395	1230.198487	15.513472
27.457901	1225.255149	15.518490
27.310236	1233.308739	15.523507
27.129760	1221.569355	15.528525
27.090021	1227.485748	15.533543
26.957268	1223.012054	15.538560
27.346894	1225.193090	15.543578
27.433043	1252.245693	15.548595
27.537239	1250.357979	15.553613
27.665607	1257.545677	15.558631
27.636660	1247.268617	15.563648
27.592940	1237.644549	15.568666
27.686128	1236.935994	15.573683
27.631048	1231.739467	15.578701
27.481380	1231.963969	15.583719
27.546138	1231.667411	15.588736
27.492100	1224.094514	15.593754
27.375540	1251.171239	15.598771
27.499911	1250.992031	15.603789
27.980725	1256.103371	15.608807
27.898780	1259.654752	15.613824
27.836085	1252.895209	15.618842
28.005556	1265.234990	15.623859
28.032238	1246.251544	15.628877
28.158920	1238.576388	15.633895
27.738395	1232.462116	15.638912
28.088186	1227.730080	15.643930
27.636512	1227.107463	15.648947
27.575643	1225.250415	15.653965
27.897461	1233.500307	15.658983
27.936882	1252.259400	15.664000
28.308803	1260.976350	15.669018
28.051821	1267.523366	15.674035
28.317870	1252.894546	15.679053
28.052620	1249.598783	15.684071
27.790565	1243.699090	15.689088
28.412291	1254.219040	15.694106
27.965234	1254.108669	15.699123
28.180012	1255.644824	15.704141
28.078685	1258.043124	15.709159
27.983576	1256.773492	15.714176
28.211295	1259.155143	15.719194
28.143342	1258.924256	15.724211
28.348917	1251.555675	15.729229
28.292544	1258.865608	15.734247
28.154484	1264.828402	15.739264
28.333361	1248.218290	15.744282
28.036179	1255.912846	15.749299
28.266118	1255.571431	15.754317
28.565589	1258.053782	15.759335
28.255737	1265.611921	15.764352
28.628443	1257.959146	15.769370
28.691357	1263.813067	15.774387
28.743503	1255.303756	15.779405
28.318987	1259.069003	15.784423
28.145121	1271.666886	15.789440
28.680167	1260.763149	15.794458
28.369536	1254.800121	15.799475
28.499570	1257.226081	15.804493
28.308059	1265.880173	15.809511
28.631005	1289.360424	15.814528
29.203787	1291.590784	15.819546
29.001108	1294.314369	15.824563
29.634825	1280.120957	15.829581
29.292485	1262.598133	15.834599
28.732510	1266.112960	15.839616
28.803364	1257.540199	15.844634
28.554418	1260.539058	15.849651
28.757598	1260.316019	15.854669
29.156898	1253.756425	15.859687
29.088770	1259.222932	15.864704
29.354834	1253.522871	15.869722
29.200971	1264.253765	15.874739
29.157144	1257.987093	15.879757
29.322323	1253.183149	15.884775
29.022164	1253.721668	15.889792
29.398379	1250.503735	15.894810
29.218051	1253.076617	15.899827
28.947276	1251.437856	15.904845
29.210241	1249.475672	15.909863
29.536188	1260.741676	15.914880
29.368195	1246.702288	15.919898
29.016789	1265.766617	15.924915
29.262346	1257.582443	15.929933
29.347664	1252.501221	15.934951
29.147929	1260.509811	15.939968
29.175564	1257.020116	15.944986
28.796634	1261.541790	15.950003
28.887702	1268.200801	15.955021
29.349245	1280.946071	15.960039
29.352600	1295.227918	15.965056
29.295881	1295.072277	15.970074
29.302570	1296.793734	15.975091
29.416910	1301.269827	15.980109
29.520192	1294.856253	15.985127
29.269476	1297.657767	15.990144
29.498561	1291.741964	15.995162
29.643045	1288.734637	16.000179
29.444067	1293.519982	16.005197
29.379474	1289.633456	16.010215
30.082793	1312.037803	16.015232
30.087543	1313.502484	16.020250
29.784279	1308.995395	16.025267
29.656854	1291.812890	16.030285
29.640056	1293.648227	16.035303
29.737988	1314.994455	16.040320
29.791158	1311.324763	16.045338
30.130873	1313.558074	16.050355
30.228912	1315.887946	16.055373
30.175567	1308.381037	16.060391
29.971570	1287.852691	16.065408
29.867094	1287.671770	16.070426
29.851613	1290.706204	16.075443
29.718410	1316.632640	16.080461
30.170899	1308.743700	16.085479
30.197236	1323.519317	16.090496
30.157483	1314.435517	16.095514
30.487607	1310.426581	16.100531
30.339480	1310.229520	16.105549
30.429906	1307.955934	16.110567
30.009422	1317.909273	16.115584
30.326813	1317.693426	16.120602
30.333808	1316.235401	16.125619
30.031257	1316.560532	16.130637
30.497213	1309.520544	16.135655
30.675727	1315.513340	16.140672
30.583384	1310.689746	16.145690
30.572872	1307.634180	16.150707
30.349356	1318.916474	16.155725
30.598057	1300.698120	16.160743
30.443124	1310.013743	16.165760
30.542528	1313.791154	16.170778
30.572463	1314.166376	16.175795
30.354795	1310.676203	16.180813
30.749440	1304.305199	16.185831
30.160371	1310.190599	16.190848
30.399578	1308.914041	16.195866
30.451589	1309.557551	16.200883
30.519445	1320.546953	16.205901
30.876846	1331.138261	16.210919
31.132753	1341.952116	16.215936
30.869149	1333.117729	16.220954
30.871488	1324.333822	16.225971
30.960930	1318.917587	16.230989
31.101607	1307.457753	16.236007
30.721226	1302.985543	16.241024
30.730532	1316.880921	16.246042
31.227777	1334.023284	16.251059
31.074983	1341.534844	16.256077
31.137409	1341.257977	16.261095
31.321397	1335.443601	16.266112
31.222223	1322.272744	16.271130
31.141562	1312.371471	16.276147
30.995529	1311.716921	16.281165
31.130908	1324.103937	16.286183
31.275126	1346.269121	16.291200
31.148534	1339.168101	16.296218
31.283838	1337.129360	16.301235
31.324959	1349.159685	16.306253
31.247488	1346.728642	16.311271
31.307581	1347.111294	16.316288
31.073660	1344.116468	16.321306
31.148328	1338.554320	16.326323
30.804167	1339.764622	16.331341
31.227425	1336.380717	16.336359
31.424784	1342.745132	16.341376
31.427541	1338.280063	16.346394
31.523937	1333.833590	16.351411
31.133801	1351.969535	16.356429
31.790951	1352.299037	16.361447
31.668944	1364.774313	16.366464
32.059538	1369.978726	16.371482
32.038684	1360.222303	16.376499
31.700597	1350.628948	16.381517
31.895072	1343.785505	16.386535
31.759020	1338.233106	16.391552
31.181764	1338.519108	16.396570
31.688596	1352.322127	16.401587
31.662550	1368.808114	16.406605
31.715751	1364.452510	16.411623
32.020129	1373.732338	16.416640
32.009688	1376.002070	16.421658
32.219834	1356.282635	16.426675
31.968689	1367.717353	16.431693
32.307561	1363.883299	16.436711
32.380504	1369.405586	16.441728
31.984721	1373.245076	16.446746
32.362494	1363.840817	16.451763
32.108297	1378.781132	16.456781
32.098661	1359.857716	16.461799
32.043904	1368.391558	16.466816
32.234504	1369.977937	16.471834
32.265321	1366.940079	16.476851
32.068916	1370.379600	16.481869
32.668275	1357.286605	16.486887
32.399559	1364.025849	16.491904
32.473774	1367.620171	16.496922
32.555070	1372.310238	16.501939
32.381372	1379.374175	16.506957
32.027525	1368.570006	16.511975
32.765250	1360.273440	16.516992
32.709658	1364.959019	16.522010
32.637369	1360.748173	16.527027
31.947068	1364.208587	16.532045
32.071878	1372.157258	16.537063
32.078665	1367.179629	16.542080
32.093798	1383.431777	16.547098
32.737793	1392.671894	16.552115
32.521471	1396.566849	16.557133
32.519530	1389.153460	16.562151
32.575113	1395.890270	16.567168
32.392122	1399.617684	16.572186
32.481078	1397.175423	16.577203
32.461827	1398.412314	16.582221
32.614858	1407.705512	16.587239
33.075072	1414.330037	16.592256
33.423607	1423.661779	16.597274
33.535062	1413.336913	16.602291
33.259647	1404.177312	16.607309
33.358663	1391.927629	16.612327
33.530185	1395.895471	16.617344
33.125220	1398.782509	16.622362
33.260737	1391.628650	16.627379
32.932095	1394.725459	16.632397
33.297190	1391.909444	16.637415
32.969837	1387.460011	16.642432
33.010814	1392.199914	16.647450
33.031835	1376.679827	16.652467
32.913605	1396.535519	16.657485
32.912685	1410.105535	16.662503
33.403215	1417.777725	16.667520
33.196690	1426.640800	16.672538
33.481574	1417.363076	16.677555
33.509693	1422.568232	16.682573
33.790906	1420.451702	16.687591
34.006300	1414.355900	16.692608
34.021104	1417.843479	16.697626
33.912457	1410.075503	16.702643
33.913366	1408.570476	16.707661
33.314720	1388.522695	16.712679
33.965386	1388.301286	16.717696
33.407562	1390.292787	16.722714
33.742092	1392.401396	16.727731
33.443381	1415.982124	16.732749
33.488967	1414.536766	16.737767
34.095294	1420.774789	16.742784
33.794217	1425.728876	16.747802
33.823259	1417.231706	16.752819
33.827433	1415.094559	16.757837
33.784065	1419.155161	16.762855
34.057408	1420.654518	16.767872
33.995500	1424.682470	16.772890
34.055900	1423.003446	16.777907
33.874846	1421.076814	16.782925
33.852846	1430.312624	16.787943
33.849607	1424.546065	16.792960
33.924488	1421.380156	16.797978
33.747258	1421.169577	16.802995
34.008173	1439.901551	16.808013
34.129552	1446.019954	16.813031
34.233546	1446.841583	16.818048
34.368122	1449.904656	16.823066
34.396390	1438.905383	16.828083
34.511779	1446.749004	16.833101
34.324262	1448.702221	16.838119
34.578541	1449.845363	16.843136
34.628879	1445.035064	16.848154
34.526121	1449.756710	16.853171
35.004429	1444.632458	16.858189
34.635678	1440.103484	16.863207
34.892664	1441.299711	16.868224
34.778930	1431.811555	16.873242
34.782989	1412.750280	16.878259
34.786194	1415.435437	16.883277
34.688644	1416.260908	16.888295
34.958276	1403.890222	16.893312
34.580879	1420.610143	16.898330
34.769452	1409.132966	16.903347
34.900769	1420.329297	16.908365
34.703589	1417.586450	16.913383
35.095962	1428.735666	16.918400
35.062385	1445.125376	16.923418
34.949977	1438.421526	16.928435
35.129013	1438.677870	16.933453
34.889805	1442.406664	16.938471
34.699975	1448.503221	16.943488
34.737529	1449.959534	16.948506
34.718643	1452.081891	16.953523
34.749061	1456.521231	16.958541
34.643972	1458.061062	16.963559
34.844086	1458.979610	16.968576
34.836231	1471.712199	16.973594
35.008914	1477.438707	16.978611
35.177431	1473.499962	16.983629
35.107561	1484.317797	16.988647
35.368886	1474.146742	16.993664
35.234148	1469.794983	16.998682
35.767739	1481.264548	17.003699
35.706126	1473.978685	17.008717
35.626908	1475.311306	17.013735
35.719992	1469.973143	17.018752
35.690483	1472.689117	17.023770
35.538750	1472.355256	17.028787
35.274570	1477.647163	17.033805
35.273540	1468.053826	17.038823
35.604567	1468.606193	17.043840
35.559857	1475.978407	17.048858
35.505784	1491.304640	17.053875
35.828918	1501.259352	17.058893
35.849964	1504.557672	17.063911
36.329143	1499.399785	17.068928
36.340890	1496.174600	17.073946
35.884740	1470.339863	17.078963
35.808084	1467.150315	17.083981
35.811502	1472.870011	17.088999
35.967398	1482.781331	17.094016
36.129731	1494.124381	17.099034
36.124262	1494.773816	17.104051
36.583033	1495.449179	17.109069
36.198736	1479.793736	17.114087
36.273997	1465.027334	17.119104
35.805564	1464.514282	17.124122
36.147178	1475.872255	17.129139
36.675972	1490.619764	17.134157
36.536662	1484.564274	17.139175
36.519973	1472.650147	17.144192
36.300154	1462.980533	17.149210
36.312650	1462.455506	17.154227
36.182865	1473.608837	17.159245
36.461719	1492.810289	17.164263
36.444883	1485.432877	17.169280
36.522517	1496.474670	17.174298
36.817008	1492.463135	17.179315
37.045537	1487.883715	17.184333
36.989646	1491.583453	17.189351
36.825843	1475.657509	17.194368
36.493462	1468.429097	17.199386
36.669681	1471.678755	17.204403
37.094441	1486.814608	17.209421
36.855569	1484.758890	17.214439
36.860112	1465.762435	17.219456
36.710461	1474.577198	17.224474
36.836398	1480.504656	17.229491
37.246426	1490.956722	17.234509
36.918374	1498.740557	17.239527
37.296357	1494.308759	17.244544
37.336382	1488.186690	17.249562
37.063503	1472.298743	17.254579
36.988583	1465.679801	17.259597
37.068444	1488.686230	17.264615
36.918722	1486.742406	17.269632
36.951959	1492.503065	17.274650
36.728583	1495.252282	17.279667
37.009455	1489.345639	17.284685
36.676821	1499.119446	17.289703
36.953835	1496.660283	17.294720
36.809601	1515.164536	17.299738
37.107706	1521.179431	17.304755
37.134997	1512.619511	17.309773
36.805380	1525.811685	17.314791
37.011768	1513.391514	17.319808
36.734057	1529.753477	17.324826
37.040244	1537.903444	17.329843
37.464304	1545.793416	17.334861
37.179451	1558.274717	17.339879
37.308798	1546.570954	17.344896
37.608026	1560.473146	17.349914
37.597561	1575.083245	17.354931
38.223043	1568.941091	17.359949
38.060470	1573.202899	17.364967
38.148181	1567.858537	17.369984
38.063731	1550.429377	17.375002
37.973401	1538.393166	17.380019
38.269968	1537.793051	17.385037
37.845284	1535.384890	17.390055
37.992132	1540.311433	17.395072
38.021799	1527.992423	17.400090
38.139123	1530.831674	17.405107
37.988695	1529.316358	17.410125
37.979154	1544.762974	17.415143
38.448778	1564.956722	17.420160
38.410126	1568.582255	17.425178
38.440786	1561.949895	17.430195
38.839153	1549.966910	17.435213
38.162507	1538.932502	17.440231
38.212989	1537.101213	17.445248
38.363688	1543.544190	17.450266
38.516432	1556.797405	17.455283
38.725439	1554.314850	17.460301
38.550908	1556.399332	17.465319
38.713742	1548.610728	17.470336
38.879200	1540.842941	17.475354
38.479143	1539.470434	17.480371
38.915990	1528.150625	17.485389
38.544737	1535.707608	17.490407
38.217107	1532.622501	17.495424
39.123409	1555.144382	17.500442
38.851916	1571.988447	17.505459
39.061127	1561.366771	17.510477
38.713042	1565.940336	17.515495
38.814235	1565.737537	17.520512
39.162642	1565.053721	17.525530
38.663138	1570.060379	17.530547
38.959469	1561.989403	17.535565
39.088285	1561.638939	17.540583
38.915279	1563.649924	17.545600
39.067861	1557.813288	17.550618
39.065342	1561.502317	17.555635
38.879327	1558.295669	17.560653
39.133227	1558.105275	17.565671
39.269706	1556.691569	17.570688
39.522454	1565.119246	17.575706
38.895766	1564.996750	17.580723
39.032592	1562.578544	17.585741
39.004988	1574.711387	17.590759
39.110505	1586.014240	17.595776
39.328314	1585.377227	17.600794
39.418136	1600.165452	17.605811
39.589671	1593.257717	17.610829
39.667762	1595.618219	17.615847
39.665154	1584.100850	17.620864
39.680698	1580.077664	17.625882
39.762845	1590.514352	17.630899
40.056278	1583.800312	17.635917
39.778093	1583.455841	17.640935
39.714450	1582.918664	17.645952
40.167567	1585.304246	17.650970
39.871478	1584.121413	17.655987
39.820991	1576.753270	17.661005
40.138381	1589.831024	17.666023
39.958212	1581.440903	17.671040
40.248834	1581.064271	17.676058
39.775490	1588.135577	17.681075
40.123730	1578.600413	17.686093
40.088474	1575.322239	17.691111
40.037996	1577.369312	17.696128
40.048664	1580.893468	17.701146
39.933565	1582.895315	17.706163
40.121186	1580.698738	17.711181
40.608070	1583.218703	17.716199
40.510123	1574.732195	17.721216
40.512724	1573.061096	17.726234
40.482000	1581.611801	17.731251
40.512920	1587.849717	17.736269
40.709867	1584.787271	17.741287
40.625570	1581.026899	17.746304
40.947258	1573.371694	17.751322
40.460635	1587.138144	17.756339
40.409368	1584.148966	17.761357
40.214208	1579.614206	17.766375
40.200332	1581.015563	17.771392
40.422477	1588.033382	17.776410
40.593937	1605.050778	17.781427
40.340309	1601.215091	17.786445
40.553337	1607.503691	17.791463
40.542875	1608.686724	17.796480
40.675919	1613.757405	17.801498
40.453627	1635.311353	17.806515
41.003939	1636.651815	17.811533
40.855540	1646.600055	17.816551
41.221235	1640.822529	17.821568
41.360620	1633.410781	17.826586
41.212550	1634.550473	17.831603
41.601734	1632.177187	17.836621
41.300146	1626.538486	17.841639
41.321554	1639.996200	17.846656
41.589356	1630.893741	17.851674
41.466822	1632.013697	17.856691
41.350892	1626.801878	17.861709
41.376094	1626.043538	17.866727
41.407011	1632.764599	17.871744
41.544245	1627.173509	17.876762
41.563055	1622.676470	17.881779
41.625273	1623.520234	17.886797
41.796612	1620.427521	17.891815
41.212655	1626.021182	17.896832
41.727989	1620.276283	17.901850
41.686478	1630.149881	17.906867
41.644299	1627.293798	17.911885
41.986197	1624.816403	17.916903
41.954310	1632.892479	17.921920
41.663681	1622.952197	17.926938
41.672424	1630.990199	17.931955
41.303752	1626.479663	17.936973
41.672977	1634.371994	17.941991
41.782950	1655.383908	17.947008
41.860747	1662.186717	17.952026
42.121606	1664.083561	17.957043
42.175278	1666.051364	17.962061
42.112339	1663.807566	17.967079
41.829921	1666.834289	17.972096
42.235741	1662.428778	17.977114
42.355495	1662.070415	17.982131
42.339653	1669.804743	17.987149
42.336953	1659.706397	17.992167
42.287400	1674.413065	17.997184
42.710349	1669.623467	18.002202
42.233137	1668.324813	18.007219
42.586650	1682.608011	18.012237
42.767021	1686.286187	18.017255
42.523981	1702.198239	18.022272
43.111583	1690.674493	18.027290
42.928640	1678.971806	18.032307
42.640807	1666.390549	18.037325
42.632407	1669.880982	18.042343
42.654703	1687.427645	18.047360
42.615839	1689.136481	18.052378
42.924266	1699.343478	18.057395
43.083245	1699.638310	18.062413
43.128190	1695.652578	18.067431
42.698525	1701.572610	18.072448
42.979393	1694.088145	18.077466
43.006669	1695.461588	18.082483
42.956328	1704.331115	18.087501
43.103975	1694.151452	18.092519
42.931736	1702.184689	18.097536
43.220605	1684.816585	18.102554
43.217585	1690.542584	18.107571
43.042158	1691.101861	18.112589
43.381114	1690.688590	18.117607
43.515798	1706.862303	18.122624
43.665180	1707.317461	18.127642
43.700126	1712.090783	18.132659
43.784660	1707.567881	18.137677
43.751524	1687.333769	18.142695
43.664618	1690.080491	18.147712
43.726209	1685.643823	18.152730
44.009008	1682.107529	18.157747
44.031706	1690.736546	18.162765
43.922289	1678.210922	18.167783
43.832930	1684.994757	18.172800
43.965514	1681.178670	18.177818
43.940325	1680.224612	18.182835
43.425976	1678.777976	18.187853
43.843660	1677.175479	18.192871
43.738047	1682.858428	18.197888
44.001178	1697.137447	18.202906
44.045220	1707.783920	18.207923
44.187701	1716.938543	18.212941
44.224253	1705.534070	18.217959
44.356623	1718.184545	18.222976
44.112261	1713.403821	18.227994
43.793497	1707.094726	18.233011
43.848112	1710.031780	18.238029
43.661743	1703.357033	18.243047
44.162152	1710.010232	18.248064
44.388421	1718.937867	18.253082
44.258942	1732.016363	18.258099
44.883873	1741.767107	18.263117
44.960098	1740.725570	18.268135
44.841185	1733.478941	18.273152
44.807217	1733.520994	18.278170
44.808332	1729.786498	18.283187
44.829154	1738.541469	18.288205
45.021659	1726.716100	18.293223
44.499872	1722.949589	18.298240
44.822906	1729.406803	18.303258
44.671135	1730.076606	18.308275
44.680448	1741.566952	18.313293
45.017204	1728.033970	18.318311
44.712600	1735.903676	18.323328
44.764652	1736.172348	18.328346
45.055939	1735.599513	18.333363
44.747377	1735.883156	18.338381
44.802210	1739.129664	18.343399
45.146417	1749.143529	18.348416
45.297122	1759.102771	18.353434
45.160412	1764.278419	18.358451
45.314035	1769.018023	18.363469
45.155679	1757.611492	18.368487
45.433277	1770.748196	18.373504
45.336826	1763.985950	18.378522
45.522684	1757.438330	18.383539
45.500092	1770.766282	18.388557
45.476618	1758.743245	18.393575
45.417264	1772.479518	18.398592
45.326339	1793.300049	18.403610
45.839070	1791.839140	18.408627
45.493777	1792.481487	18.413645
45.886100	1795.433107	18.418663
45.631087	1794.642477	18.423680
45.714036	1795.080284	18.428698
46.498363	1788.496193	18.433715
45.840081	1796.251742	18.438733
46.041814	1788.344526	18.443751
45.981612	1788.822626	18.448768
46.233897	1785.982178	18.453786
46.424827	1784.854822	18.458803
46.018747	1784.910273	18.463821
46.219823	1787.906494	18.468839
46.125829	1785.890077	18.473856
46.300889	1781.641434	18.478874
46.517031	1775.075620	18.483891
46.284575	1780.057034	18.488909
46.572228	1778.601246	18.493927
46.606040	1779.658970	18.498944
46.308116	1787.152313	18.503962
46.783476	1795.175761	18.508979
46.783918	1814.513544	18.513997
46.821642	1797.819162	18.519015
46.682106	1795.769602	18.524032
46.989409	1798.421980	18.529050
46.995827	1789.527650	18.534067
46.523021	1790.324159	18.539085
46.699293	1802.297800	18.544103
46.878725	1799.736015	18.549120
46.913902	1803.838769	18.554138
47.172144	1797.887460	18.559155
47.151955	1809.492377	18.564173
47.182167	1803.061592	18.569191
47.030174	1805.502130	18.574208
46.808582	1804.089157	18.579226
47.224262	1804.258474	18.584243
47.271460	1805.968711	18.589261
47.128163	1807.860052	18.594279
47.093392	1806.880067	18.599296
47.450383	1822.620853	18.604314
47.410158	1822.714378	18.609331
47.395014	1833.706954	18.614349
47.305884	1837.743617	18.619367
47.717297	1839.104762	18.624384
47.753044	1836.912925	18.629402
47.870406	1832.673373	18.634419
47.584167	1843.712829	18.639437
47.924487	1840.608033	18.644455
47.732723	1835.069338	18.649472
47.708892	1836.372018	18.654490
48.052557	1831.395153	18.659507
47.905255	1832.481176	18.664525
48.271252	1832.342042	18.669543
48.304703	1832.830074	18.674560
48.070143	1839.236457	18.679578
48.403488	1828.164917	18.684595
48.019653	1828.227185	18.689613
48.275293	1838.365756	18.694631
48.176747	1840.368735	18.699648
48.064084	1837.552260	18.704666
48.742732	1824.744142	18.709683
48.647923	1839.781205	18.714701
48.354445	1822.634461	18.719719
48.582935	1826.765896	18.724736
48.329268	1834.156780	18.729754
49.118703	1821.290295	18.734771
48.896093	1820.296445	18.739789
48.856920	1827.424538	18.744807
48.953596	1819.692030	18.749824
49.105206	1824.609184	18.754842
49.113211	1810.594632	18.759859
49.087268	1811.101902	18.764877
48.812402	1814.334865	18.769895
49.350723	1809.753821	18.774912
49.171320	1812.012816	18.779930
49.348458	1806.856609	18.784947
49.407300	1803.871742	18.789965
49.377036	1782.638857	18.794983
48.985321	1776.259947	18.800000
48.987102	1780.784614	18.805018
49.403533	1791.648436	18.810035
49.057535	1813.165563	18.815053
49.202356	1809.831660	18.820071
49.488413	1814.957286	18.825088
49.345702	1813.879256	18.830106
49.259239	1816.590486	18.835123
49.257525	1812.826530	18.840141
49.202209	1808.616590	18.845159
49.157029	1807.107614	18.850176
49.459013	1826.455138	18.855194
49.475847	1833.902413	18.860211
49.760256	1844.720788	18.865229
49.723946	1841.599058	18.870247
49.844992	1838.331832	18.875264
50.137121	1846.085108	18.880282
49.949420	1841.418268	18.885299
49.885195	1846.072789	18.890317
50.093979	1842.351487	18.895335
50.121638	1846.340960	18.900352
49.915758	1852.917650	18.905370
49.383263	1838.824853	18.910387
49.713211	1862.788295	18.915405
49.821136	1874.767016	18.920423
50.072151	1871.781476	18.925440
49.961427	1883.443314	18.930458
50.520768	1874.825839	18.935475
50.534076	1875.949691	18.940493
50.516263	1892.423399	18.945511
50.281737	1875.922086	18.950528
50.545478	1892.649924	18.955546
51.129051	1886.313627	18.960563
51.370121	1888.330048	18.965581
51.242524	1873.299576	18.970599
51.263846	1868.033038	18.975616
50.747116	1864.406981	18.980634
50.893457	1863.088027	18.985651
50.969484	1856.917904	18.990669
51.046130	1856.202314	18.995687
51.107891	1864.135665	19.000704
51.194364	1862.274148	19.005722
51.167342	1856.265019	19.010739
51.334976	1859.759569	19.015757
51.443779	1858.424608	19.020775
51.423040	1852.804216	19.025792
51.144097	1851.821597	19.030810
51.382749	1844.397849	19.035827
51.363075	1849.149077	19.040845
51.229536	1852.709831	19.045863
51.720210	1855.608770	19.050880
51.563074	1859.764198	19.055898
51.130470	1849.489010	19.060915
51.508197	1863.389434	19.065933
51.558142	1872.286750	19.070951
51.694135	1877.059336	19.075968
51.233648	1887.775108	19.080986
51.693537	1877.070471	19.086003
51.737139	1884.071391	19.091021
51.507746	1879.287655	19.096039
52.206202	1886.668886	19.101056
52.321101	1908.379600	19.106074
52.648342	1898.098138	19.111091
52.448174	1883.711283	19.116109
52.271931	1879.578363	19.121127
52.326692	1866.796456	19.126144
52.391359	1877.200108	19.131162
52.647207	1874.727585	19.136179
52.263742	1877.412177	19.141197
52.052870	1871.253436	19.146215
52.159707	1870.500776	19.151232
52.328264	1900.884902	19.156250
52.454501	1901.581074	19.161267
52.517592	1906.062584	19.166285
52.768987	1912.576257	19.171303
53.079831	1906.363099	19.176320
53.090512	1909.708957	19.181338
52.944685	1916.065114	19.186355
52.651779	1908.906903	19.191373
53.060768	1918.594375	19.196391
53.163218	1912.503569	19.201408
52.583654	1905.628396	19.206426
53.243066	1900.738339	19.211443
53.058935	1900.885281	19.216461
52.524874	1912.003104	19.221479
52.857265	1913.735333	19.226496
52.428292	1930.555594	19.231514
52.546622	1935.881693	19.236531
52.788218	1936.945541	19.241549
52.870831	1959.151690	19.246567
53.419446	1962.805385	19.251584
53.345785	1976.960096	19.256602
53.505373	1964.042405	19.261619
53.678071	1957.470183	19.266637
54.037372	1968.774690	19.271655
53.932556	1961.893698	19.276672
54.202924	1960.117980	19.281690
53.901473	1966.702835	19.286707
53.770433	1963.917838	19.291725
53.597394	1967.234569	19.296743
53.978759	1965.084653	19.301760
54.038409	1961.994879	19.306778
53.980126	1962.757339	19.311795
54.212402	1958.129498	19.316813
54.214792	1963.169143	19.321831
54.358684	1959.971607	19.326848
54.207889	1966.342024	19.331866
54.091577	1962.175969	19.336883
54.453875	1956.633982	19.341901
54.344853	1965.394411	19.346919
54.475535	1968.148370	19.351936
54.220090	1978.220699	19.356954
54.261961	1989.604451	19.361971
54.368284	1987.234328	19.366989
54.194762	1988.725306	19.372007
54.544875	1983.587817	19.377024
54.367890	1989.685924	19.382042
54.790261	2008.350737	19.387059
54.960296	2017.802430	19.392077
55.031435	2008.174338	19.397095
55.241186	2006.353094	19.402112
55.299436	2006.025351	19.407130
54.945929	2012.371871	19.412147
55.529578	2002.586612	19.417165
55.379289	2004.672510	19.422183
55.399129	2001.172960	19.427200
55.564081	2007.779457	19.432218
55.638501	1997.333767	19.437235
55.964594	1982.409289	19.442253
55.659981	1975.240848	19.447271
55.890648	1963.945052	19.452288
55.595194	1963.516118	19.457306
55.519778	1963.227829	19.462323
55.512071	1956.878296	19.467341
55.557870	1969.342214	19.472359
55.668403	1984.567470	19.477376
55.699260	1992.343171	19.482394
55.753729	2002.059977	19.487411
56.142859	2000.138285	19.492429
55.845397	1998.755232	19.497447
56.054238	2000.072373	19.502464
55.902613	2008.656246	19.507482
56.191401	2000.552870	19.512499
56.247867	1988.064313	19.517517
56.233015	2003.728859	19.522535
56.167867	1997.151329	19.527552
56.223800	1999.535773	19.532570
55.857685	1997.814443	19.537587
56.289488	2008.586792	19.542605
56.368020	2025.314238	19.547623
56.616206	2027.108167	19.552640
56.746310	2034.896011	19.557658
56.892161	2037.842291	19.562675
56.783711	2025.597364	19.567693
56.720741	2029.145665	19.572711
57.183152	2029.982659	19.577728
57.476276	2024.900603	19.582746
56.838454	2033.877339	19.587763
57.038085	2032.848489	19.592781
56.863562	2029.299174	19.597799
56.953266	2017.433329	19.602816
56.936905	2024.674546	19.607834
56.896587	2027.782682	19.612851
57.097663	2016.254880	19.617869
57.062966	2024.590337	19.622887
56.776776	2027.861116	19.627904
57.328670	2033.756706	19.632922
57.456460	2053.521439	19.637939
57.263854	2052.119222	19.642957
57.351865	2054.963989	19.647975
57.413441	2064.619764	19.652992
57.636625	2055.395164	19.658010
57.274038	2062.547312	19.663027
57.576728	2060.231714	19.668045
57.858827	2082.244365	19.673063
57.834535	2086.958656	19.678080
57.775134	2086.056902	19.683098
58.095408	2078.037077	19.688115
58.207484	2079.099910	19.693133
58.272948	2079.510010	19.698151
58.158094	2068.655715	19.703168
58.402071	2072.516807	19.708186
58.194268	2069.686676	19.713203
58.632550	2072.410361	19.718221
58.423432	2071.731942	19.723239
58.530371	2073.546943	19.728256
58.677535	2065.877322	19.733274
58.945254	2069.405949	19.738291
58.912648	2066.900950	19.743309
58.871293	2069.020155	19.748327
59.026125	2071.308116	19.753344
59.181838	2068.104593	19.758362
59.148186	2075.015286	19.763379
58.960058	2068.583632	19.768397
58.688476	2065.059612	19.773415
58.941814	2074.555333	19.778432
58.649697	2071.779820	19.783450
58.947209	2077.313076	19.788467
59.298271	2071.551291	19.793485
58.973237	2075.338261	19.798503
58.822424	2068.624579	19.803520
59.149190	2085.930092	19.808538
58.602029	2103.283866	19.813555
58.833339	2094.214565	19.818573
58.985232	2103.670996	19.823591
59.068375	2123.002856	19.828608
59.461445	2130.624779	19.833626
59.818551	2135.046103	19.838643
59.771533	2132.800295	19.843661
59.609282	2143.735226	19.848679
59.957814	2143.407719	19.853696
59.755777	2128.801635	19.858714
59.863150	2124.526704	19.863731
59.947723	2121.396006	19.868749
60.118813	2128.777993	19.873767
59.740328	2132.681243	19.878784
60.012550	2130.347626	19.883802
59.964518	2152.174027	19.888819
60.121791	2154.760050	19.893837
60.467127	2156.397948	19.898855
60.627570	2158.497530	19.903872
60.430330	2149.087437	19.908890
60.531399	2164.433012	19.913907
60.578168	2162.805860	19.918925
60.727040	2159.740520	19.923943
60.526304	2164.578800	19.928960
60.432972	2153.076567	19.933978
60.410796	2150.750107	19.938995
60.909392	2158.147622	19.944013
60.795422	2171.362035	19.949031
61.216064	2177.489269	19.954048
61.285478	2171.756835	19.959066
61.004484	2176.254495	19.964083
61.476558	2173.976386	19.969101
61.635244	2175.860492	19.974119
61.843124	2161.224262	19.979136
62.050551	2142.319779	19.984154
61.891546	2134.110404	19.989171
61.765029	2137.567247	19.994189
61.841790	2129.971879	19.999207
61.804111	2130.837523	20.004224
61.703443	2129.650673	20.009242
61.726491	2128.482775	20.014259
61.531423	2129.525032	20.019277
61.467833	2124.421018	20.024295
61.475613	2130.085081	20.029312
61.719528	2136.125258	20.034330
61.715112	2143.327075	20.039347
61.827813	2154.315676	20.044365
61.832290	2160.989915	20.049383
61.752723	2169.223676	20.054400
62.233332	2153.217664	20.059418
61.992524	2163.310046	20.064435
62.286159	2158.744865	20.069453
62.408817	2162.799246	20.074471
62.637444	2184.492420	20.079488
62.724692	2195.210570	20.084506
62.654794	2193.270296	20.089523
62.654857	2175.466840	20.094541
62.974994	2183.968352	20.099559
62.591841	2178.952184	20.104576
62.542956	2171.864237	20.109594
62.615584	2184.117397	20.114611
62.269513	2197.233808	20.119629
62.599515	2191.426765	20.124647
62.343816	2191.317828	20.129664
62.966019	2198.750872	20.134682
62.962397	2213.060742	20.139699
62.992763	2214.232096	20.144717
63.071943	2214.639060	20.149735
62.567348	2219.581429	20.154752
63.073323	2216.927367	20.159770
63.244338	2237.533475	20.164787
63.491827	2250.947441	20.169805
63.719058	2253.982188	20.174823
63.677774	2257.590612	20.179840
63.936734	2246.913874	20.184858
64.419407	2246.328686	20.189875
63.976283	2254.339739	20.194893
63.953164	2249.605970	20.199911
64.016332	2254.777043	20.204928
64.244527	2237.491970	20.209946
64.016668	2246.500130	20.214963
64.342867	2245.182597	20.219981
64.433015	2243.517286	20.224999
64.292290	2238.930474	20.230016
64.531296	2239.788851	20.235034
64.481039	2249.801367	20.240051
64.404458	2244.401071	20.245069
64.531217	2244.320278	20.250087
64.388706	2252.349094	20.255104
64.769260	2242.194903	20.260122
64.777947	2241.850845	20.265139
64.394031	2248.053831	20.270157
64.902932	2244.651116	20.275175
64.536741	2242.376536	20.280192
64.926259	2247.888566	20.285210
64.811451	2251.341064	20.290227
64.833798	2245.642661	20.295245
64.795544	2243.701681	20.300263
64.988356	2266.924965	20.305280
65.414062	2261.079438	20.310298
65.272071	2263.525419	20.315315
64.862338	2283.751553	20.320333
65.028467	2269.249960	20.325351
65.063785	2266.752972	20.330368
65.252943	2276.654369	20.335386
65.550274	2287.434217	20.340403
65.543118	2289.677530	20.345421
65.735041	2289.316231	20.350439
65.712661	2290.334403	20.355456
65.920372	2287.947247	20.360474
65.786366	2286.125056	20.365491
65.790929	2294.746885	20.370509
65.849843	2284.788777	20.375527
66.089544	2286.674757	20.380544
66.320281	2287.758212	20.385562
66.105953	2287.128715	20.390579
66.115191	2282.432702	20.395597
66.384742	2294.072569	20.400615
66.004910	2315.658399	20.405632
66.168680	2318.476443	20.410650
66.341050	2313.699689	20.415667
66.209805	2319.201799	20.420685
66.689709	2313.871453	20.425703
66.444168	2316.742346	20.430720
66.794111	2310.780635	20.435738
66.850219	2330.165426	20.440755
66.745510	2341.170956	20.445773
67.534648	2343.905415	20.450791
66.920771	2357.457700	20.455808
66.938576	2354.486458	20.460826
67.336152	2343.643347	20.465843
66.999674	2346.684980	20.470861
67.487713	2347.733776	20.475879
67.187532	2343.247511	20.480896
67.592056	2343.932612	20.485914
67.507666	2343.649399	20.490931
67.018806	2349.343561	20.495949
67.189963	2339.214182	20.500967
67.100461	2352.749014	20.505984
67.481445	2361.930853	20.511002
67.993631	2375.140464	20.516019
67.718382	2371.716231	20.521037
67.797043	2376.589365	20.526055
67.831399	2371.874844	20.531072
68.226858	2368.396261	20.536090
68.516368	2363.545069	20.541107
68.353755	2376.294689	20.546125
68.315261	2372.638496	20.551143
68.061732	2375.621023	20.556160
68.042824	2371.058964	20.561178
68.593245	2379.561266	20.566195
68.195619	2398.373432	20.571213
68.596387	2393.084978	20.576231
68.849625	2400.518375	20.581248
68.792716	2403.027756	20.586266
69.402335	2394.562037	20.591283
68.866697	2394.727113	20.596301
68.879782	2392.033884	20.601319
68.736178	2394.042295	20.606336
68.739902	2392.109062	20.611354
68.805684	2386.928444	20.616371
68.985265	2400.158086	20.621389
69.069632	2403.738701	20.626407
69.412481	2417.645206	20.631424
69.384959	2421.497805	20.636442
69.223045	2423.437694	20.641459
69.312052	2423.024734	20.646477
69.482942	2413.782114	20.651495
69.629454	2419.899740	20.656512
69.368052	2421.382592	20.661530
69.874239	2419.716813	20.666547
69.799523	2418.679059	20.671565
69.912283	2419.357484	20.676583
69.703624	2423.237200	20.681600
69.603994	2436.293446	20.686618
69.825479	2445.009685	20.691635
69.585603	2454.473642	20.696653
70.258220	2449.014132	20.701671
70.157760	2448.941580	20.706688
70.212860	2452.276788	20.711706
70.637827	2448.369437	20.716723
70.400737	2446.578288	20.721741
70.685999	2436.500950	20.726759
71.160620	2450.222661	20.731776
71.128213	2435.904583	20.736794
71.195893	2438.079172	20.741811
70.784022	2448.256191	20.746829
70.988930	2452.524142	20.751847
71.082054	2435.645538	20.756864
70.932873	2442.265912	20.761882
70.931024	2438.866456	20.766899
70.913082	2458.731107	20.771917
71.172014	2465.853271	20.776935
71.410872	2469.826382	20.781952
71.792998	2469.621479	20.786970
71.839435	2466.421648	20.791987
71.983741	2470.930742	20.797005
71.960060	2459.692766	20.802023
71.576488	2453.843371	20.807040
71.815144	2469.312137	20.812058
71.904270	2466.483791	20.817075
71.469613	2469.307594	20.822093
71.634967	2470.055756	20.827111
71.865731	2481.659099	20.832128
71.695299	2475.084849	20.837146
71.895675	2474.072382	20.842163
71.758665	2483.668352	20.847181
72.398115	2494.269983	20.852199
72.109196	2496.204092	20.857216
71.966445	2500.272562	20.862234
72.059376	2499.190310	20.867251
72.008651	2503.035882	20.872269
72.245943	2524.408302	20.877287
72.462026	2528.208925	20.882304
72.186244	2532.134040	20.887322
72.569486	2529.121377	20.892339
72.497120	2540.983068	20.897357
73.049704	2551.505126	20.902375
72.833692	2554.692315	20.907392
72.857746	2572.781100	20.912410
73.468904	2562.485576	20.917427
73.215821	2563.981190	20.922445
73.284345	2561.682434	20.927463
73.288132	2563.167873	20.932480
73.602492	2556.000150	20.937498
73.574377	2559.153551	20.942515
73.762359	2557.904580	20.947533
73.554560	2555.199577	20.952551
74.192833	2556.568362	20.957568
73.669579	2560.482359	20.962586
74.322775	2563.695362	20.967603
73.887312	2557.982405	20.972621
73.646848	2555.061705	20.977639
73.584467	2549.717147	20.982656
73.690925	2562.185313	20.987674
74.001145	2572.319729	20.992691
74.236970	2578.817450	20.997709
74.343573	2581.316940	21.002727
74.351435	2570.235710	21.007744
74.125257	2586.426917	21.012762
74.487470	2580.278718	21.017779
74.689412	2592.403709	21.022797
74.452896	2602.839003	21.027815
74.759731	2607.715617	21.032832
74.948723	2612.290332	21.037850
75.064629	2611.564040	21.042867
74.810280	2609.701015	21.047885
75.053336	2599.329968	21.052903
74.946845	2600.879207	21.057920
74.962349	2610.826339	21.062938
75.076014	2603.265367	21.067955
75.176236	2612.397047	21.072973
75.240900	2626.335680	21.077991
75.368021	2630.834379	21.083008
75.298975	2639.262680	21.088026
75.800854	2628.966159	21.093043
75.597897	2632.667753	21.098061
75.462734	2637.061787	21.103079
75.746410	2636.592609	21.108096
75.982858	2650.460860	21.113114
76.106045	2660.761282	21.118131
76.137745	2658.155383	21.123149
76.020085	2655.208885	21.128167
76.161297	2650.345228	21.133184
76.360250	2661.567474	21.138202
76.729284	2658.358762	21.143219
76.465110	2657.153438	21.148237
76.576644	2652.982393	21.153255
76.973939	2648.991533	21.158272
76.887357	2656.655784	21.163290
77.353823	2660.704116	21.168307
77.386183	2666.848498	21.173325
77.206323	2656.649938	21.178343
77.096881	2647.484381	21.183360
76.946752	2657.930102	21.188378
77.236767	2658.409614	21.193395
77.310135	2660.280842	21.198413
76.961983	2658.444130	21.203431
77.196109	2657.773172	21.208448
77.152860	2663.395774	21.213466
76.994949	2660.857822	21.218483
77.399220	2659.405590	21.223501
77.422274	2660.789292	21.228519
77.800244	2672.814863	21.233536
77.638996	2687.000193	21.238554
77.734521	2674.160238	21.243571
77.482643	2680.055664	21.248589
77.426696	2685.418198	21.253607
77.331467	2684.287076	21.258624
77.267872	2706.672134	21.263642
77.756505	2707.343621	21.268659
77.783219	2713.572469	21.273677
78.124698	2723.826844	21.278695
78.406039	2736.811724	21.283712
78.345895	2749.013271	21.288730
78.310472	2738.462276	21.293747
78.287303	2740.513874	21.298765
78.401166	2748.959704	21.303783
78.482928	2754.736529	21.308800
78.529076	2769.240772	21.313818
78.765719	2769.553814	21.318835
79.041656	2764.674900	21.323853
79.202204	2761.206581	21.328871
79.018075	2762.266690	21.333888
79.266963	2764.487437	21.338906
79.441001	2775.265134	21.343923
79.561556	2787.318387	21.348941
79.360027	2794.603124	21.353959
79.752423	2783.659006	21.358976
79.607219	2790.634028	21.363994
80.156644	2782.323333	21.369011
80.207344	2775.225127	21.374029
80.505894	2777.805936	21.379047
80.253078	2778.882547	21.384064
80.298111	2778.132959	21.389082
80.255013	2761.629394	21.394099
80.476680	2770.411937	21.399117
80.133060	2770.330668	21.404135
80.153482	2764.194530	21.409152
80.242770	2781.266673	21.414170
80.156892	2784.986031	21.419187
80.464024	2787.189709	21.424205
80.125564	2792.077781	21.429223
80.461117	2790.859408	21.434240
80.495261	2812.204833	21.439258
80.372036	2803.779483	21.444275
80.623612	2806.086406	21.449293
80.786540	2819.792576	21.454311
81.004213	2829.033404	21.459328
81.122309	2841.617930	21.464346
81.266790	2842.197216	21.469363
81.224229	2848.374202	21.474381
81.210422	2853.342092	21.479399
81.354518	2843.955754	21.484416
81.536473	2843.381152	21.489434
81.493941	2845.518777	21.494451
81.486484	2842.622653	21.499469
81.701839	2861.610649	21.504487
82.076097	2863.131833	21.509504
82.040636	2872.617699	21.514522
81.879562	2879.500187	21.519539
82.240989	2876.486474	21.524557
82.063914	2884.596355	21.529575
82.496840	2875.069124	21.534592
82.413880	2879.000644	21.539610
82.207009	2868.000122	21.544627
82.569559	2873.036592	21.549645
82.129497	2882.891100	21.554663
82.360665	2883.035759	21.559680
82.291167	2891.024817	21.564698
82.437392	2898.234231	21.569715
82.812094	2899.245008	21.574733
82.559449	2902.454298	21.579751
83.105950	2917.128852	21.584768
83.171660	2926.610793	21.589786
83.413629	2934.368487	21.594803
83.217207	2926.235991	21.599821
83.196499	2931.589417	21.604839
83.098397	2924.416635	21.609856
83.662122	2932.657854	21.614874
83.462257	2933.097715	21.619891
83.683390	2925.752857	21.624909
83.512707	2940.318846	21.629927
83.471967	2957.962400	21.634944
84.264947	2968.101727	21.639962
84.473166	2966.418461	21.644979
84.590468	2962.627525	21.649997
84.518380	2961.753884	21.655015
84.670096	2955.211622	21.660032
85.012397	2947.778250	21.665050
84.515632	2954.664768	21.670067
84.990793	2945.571287	21.675085
84.564509	2952.441783	21.680103
85.016056	2952.113142	21.685120
84.728425	2960.213663	21.690138
84.705422	2956.737391	21.695155
85.028936	2948.518894	21.700173
84.758278	2957.277265	21.705191
84.763496	2953.878849	21.710208
84.760583	2955.128419	21.715226
84.591046	2969.714715	21.720243
85.555457	2977.782519	21.725261
84.971017	2982.441900	21.730279
85.357161	2984.025640	21.735296
85.307744	2983.167013	21.740314
85.525618	2983.321828	21.745331
85.909985	2990.157319	21.750349
85.641170	3000.277876	21.755367
85.809576	3006.170674	21.760384
86.020323	3001.779338	21.765402
86.546671	3006.245928	21.770419
86.455421	3003.234981	21.775437
86.218179	3012.348356	21.780455
85.973175	3012.124168	21.785472
86.489883	3006.261192	21.790490
86.211761	3012.739310	21.795507
86.763965	3003.286060	21.800525
86.472112	3001.954719	21.805543
86.495019	3000.206349	21.810560
86.395835	3014.811341	21.815578
86.797719	3035.070981	21.820595
87.062471	3035.810007	21.825613
86.796831	3042.874306	21.830631
86.780078	3037.279978	21.835648
86.692114	3039.839675	21.840666
86.784332	3064.946335	21.845683
87.180695	3068.476763	21.850701
86.906631	3076.155246	21.855719
86.912665	3076.316453	21.860736
87.295916	3091.402703	21.865754
87.747465	3098.275553	21.870771
87.905169	3093.054528	21.875789
87.692173	3105.710205	21.880807
87.794178	3098.086415	21.885824
87.679680	3099.128308	21.890842
87.822426	3115.451337	21.895859
88.264035	3121.561962	21.900877
88.200034	3123.297709	21.905895
88.221841	3121.939360	21.910912
88.416097	3117.762674	21.915930
88.284167	3127.153397	21.920947
88.888153	3131.483853	21.925965
88.963437	3143.087564	21.930983
89.165675	3143.761707	21.936000
89.344666	3140.177520	21.941018
89.141538	3145.871020	21.946035
89.414744	3141.159423	21.951053
89.662129	3146.798526	21.956071
89.527457	3142.600257	21.961088
89.250950	3141.187515	21.966106
89.387605	3146.281703	21.971123
89.487730	3144.385405	21.976141
89.106930	3135.711848	21.981159
89.205393	3135.694184	21.986176
89.586538	3148.385071	21.991194
89.397775	3163.642700	21.996211
89.660275	3163.323627	22.001229
90.130814	3164.770844	22.006247
89.595601	3167.389912	22.011264
90.213477	3178.335940	22.016282
90.438785	3196.806777	22.021299
90.562508	3191.604934	22.026317
90.575675	3200.779446	22.031335
90.653030	3196.459755	22.036352
90.634401	3187.631932	22.041370
90.631806	3202.145719	22.046387
90.846735	3189.828297	22.051405
90.524038	3194.618493	22.056423
90.415205	3188.353924	22.061440
91.136336	3203.343764	22.066458
91.212463	3227.258697	22.071475
91.080550	3213.762656	22.076493
91.341711	3220.272840	22.081511
91.170013	3220.540914	22.086528
91.552376	3219.724810	22.091546
91.485938	3225.950929	22.096563
91.756123	3218.308487	22.101581
91.671505	3236.894722	22.106599
91.252057	3247.768190	22.111616
91.909826	3254.067055	22.116634
91.770416	3255.445585	22.121651
92.297698	3255.327626	22.126669
92.397846	3255.956270	22.131687
92.416868	3257.858152	22.136704
92.050382	3255.779575	22.141722
92.565823	3282.715225	22.146739
92.696256	3292.446191	22.151757
92.554686	3290.223515	22.156775
92.622025	3291.489420	22.161792
92.956664	3280.343792	22.166810
92.679658	3292.306500	22.171827
92.822608	3285.151296	22.176845
92.834307	3297.507917	22.181863
93.009085	3315.338593	22.186880
92.995454	3313.484618	22.191898
93.056380	3325.107463	22.196915
93.290189	3327.507295	22.201933
93.670033	3339.625992	22.206951
93.983548	3342.427214	22.211968
93.763290	3340.977245	22.216986
93.904771	3344.680597	22.222003
93.909021	3340.830981	22.227021
94.004370	3340.260184	22.232039
93.652434	3336.911890	22.237056
94.196955	3334.180946	22.242074
94.139887	3347.787466	22.247091
94.440822	3360.538744	22.252109
94.537700	3372.678413	22.257127
94.557921	3379.957693	22.262144
94.529257	3360.597626	22.267162
94.686945	3374.273675	22.272179
94.678168	3369.700138	22.277197
94.559191	3375.922722	22.282215
94.686542	3391.444559	22.287232
95.361710	3392.181761	22.292250
94.966121	3400.301014	22.297267
95.312936	3403.643907	22.302285
95.371757	3401.193115	22.307303
95.145938	3402.092658	22.312320
95.275268	3396.232945	22.317338
95.268369	3420.465624	22.322355
96.409634	3420.266032	22.327373
96.905278	3417.912829	22.332391
96.592129	3410.456935	22.337408
97.084157	3382.730890	22.342426
96.752111	3377.372425	22.347443
96.880919	3379.658740	22.352461
96.953320	3372.457311	22.357479
96.517943	3369.243814	22.362496
96.975426	3370.359356	22.367514
96.587062	3373.761337	22.372531
96.237284	3368.253912	22.377549
96.501938	3373.480595	22.382567
96.174456	3381.668496	22.387584
96.976857	3377.942726	22.392602
96.907605	3403.616312	22.397619
96.864238	3407.811316	22.402637
96.978930	3409.427462	22.407655
96.541013	3410.860331	22.412672
96.867933	3425.647828	22.417690
96.782146	3430.176169	22.422707
97.139458	3431.208079	22.427725
97.421748	3450.957142	22.432743
97.065094	3470.411738	22.437760
97.162090	3469.906023	22.442778
97.852651	3487.778422	22.447795
98.030140	3500.550189	22.452813
98.333746	3496.636613	22.457831
98.114079	3495.562994	22.462848
98.379531	3497.186381	22.467866
98.670829	3502.171477	22.472883
98.674715	3486.245848	22.477901
98.905477	3498.869079	22.482919
98.660432	3514.983350	22.487936
99.428918	3517.744409	22.492954
99.336431	3518.514776	22.497971
99.008283	3529.460993	22.502989
99.129180	3517.840699	22.508007
99.192153	3514.375555	22.513024
98.978495	3513.626964	22.518042
99.660562	3513.367482	22.523059
99.335469	3511.692106	22.528077
99.458071	3515.712194	22.533095
99.377609	3537.268057	22.538112
99.533489	3545.057353	22.543130
99.701408	3539.082285	22.548147
99.932690	3542.127617	22.553165
100.309248	3551.254998	22.558183
100.734441	3560.547316	22.563200
100.846043	3546.066499	22.568218
100.904146	3545.186257	22.573235
100.756166	3536.199270	22.578253
100.728152	3527.043655	22.583271
100.676767	3545.945104	22.588288
100.792099	3531.727503	22.593306
100.801141	3535.483533	22.598323
100.744580	3556.313108	22.603341
101.036346	3566.350522	22.608359
100.861883	3573.191502	22.613376
101.218405	3571.276400	22.618394
101.337158	3569.140582	22.623411
100.899220	3565.313164	22.628429
101.402826	3581.766983	22.633447
101.337656	3599.015347	22.638464
101.787220	3594.085937	22.643482
101.693695	3601.382456	22.648499
101.845491	3602.414958	22.653517
101.983535	3611.974697	22.658535
101.882553	3626.412806	22.663552
101.865100	3624.914652	22.668570
102.592112	3625.793410	22.673587
102.454207	3634.310444	22.678605
102.459977	3631.355202	22.683623
102.569441	3648.409862	22.688640
102.633582	3653.088984	22.693658
103.181830	3652.267261	22.698675
103.156008	3661.210872	22.703693
103.155016	3651.236181	22.708711
103.120899	3658.040536	22.713728
103.169539	3649.438775	22.718746
103.221166	3647.339657	22.723763
103.202936	3651.973831	22.728781
103.505163	3656.717674	22.733799
103.574157	3673.867511	22.738816
103.570478	3684.109231	22.743834
103.858725	3680.143112	22.748851
103.491566	3688.638833	22.753869
104.106491	3690.225957	22.758887
103.628220	3703.216636	22.763904
104.019275	3716.608820	22.768922
104.173254	3711.618996	22.773939
104.230391	3724.832155	22.778957
104.447860	3725.636817	22.783975
104.823113	3746.826579	22.788992
105.171341	3731.593825	22.794010
106.165055	3716.224436	22.799027
105.576674	3704.846890	22.804045
105.623640	3694.784402	22.809063
105.894935	3692.049047	22.814080
105.546291	3690.870722	22.819098
105.770656	3692.418477	22.824115
105.755266	3684.276604	22.829133
105.578854	3678.077768	22.834151
105.900865	3684.185492	22.839168
105.903538	3677.608626	22.844186
106.453574	3678.890260	22.849203
105.897247	3686.726115	22.854221
106.308646	3688.164621	22.859239
106.393343	3682.322693	22.864256
106.227524	3685.489688	22.869274
106.250797	3703.653941	22.874291
105.975833	3720.324079	22.879309
106.088724	3714.926236	22.884327
106.035988	3721.485717	22.889344
106.124318	3737.154777	22.894362
106.840239	3745.273462	22.899379
106.730716	3757.782755	22.904397
106.908929	3748.849200	22.909415
106.932941	3769.729827	22.914432
106.885074	3772.429261	22.919450
107.359992	3777.864189	22.924467
107.240248	3785.875703	22.929485
107.526526	3782.663629	22.934503
107.667967	3806.906912	22.939520
108.073912	3816.616960	22.944538
108.134096	3806.351297	22.949555
107.900116	3814.314676	22.954573
108.100911	3809.217559	22.959591
108.286655	3810.137928	22.964608
107.903018	3810.014677	22.969626
107.881711	3823.466620	22.974643
108.059951	3844.069660	22.979661
108.445989	3838.861228	22.984679
108.641093	3852.617126	22.989696
108.647909	3874.294742	22.994714
108.970091	3867.203849	22.999731
108.788040	3877.056481	23.004749
108.886297	3877.208975	23.009767
108.879748	3897.874480	23.014784
109.090626	3898.442425	23.019802
109.882637	3894.087450	23.024819
109.393483	3893.168691	23.029837
109.714541	3890.019942	23.034855
110.213322	3897.200091	23.039872
110.102914	3910.727242	23.044890
110.647097	3909.547057	23.049907
110.280543	3914.706498	23.054925
110.329044	3911.913213	23.059943
110.939447	3913.355429	23.064960
110.493951	3912.307893	23.069978
111.071987	3905.559834	23.074995
110.965629	3907.993658	23.080013
110.974850	3915.635794	23.085031
110.973486	3916.135373	23.090048
111.009651	3919.723811	23.095066
111.024639	3907.918185	23.100083
111.500273	3917.242235	23.105101
111.451259	3908.887056	23.110119
111.798787	3928.147458	23.115136
111.553573	3952.165048	23.120154
111.578441	3941.535964	23.125171
111.291749	3945.269544	23.130189
111.691554	3954.382936	23.135207
111.708565	3947.505784	23.140224
111.767550	3950.728804	23.145242
112.086741	3964.484793	23.150259
111.648848	3966.940808	23.155277
111.569422	3963.259757	23.160295
112.083182	3981.964028	23.165312
112.277874	3992.994205	23.170330
112.530831	3996.797529	23.175347
112.404050	4008.591678	23.180365
112.813916	4017.493878	23.185383
112.933951	4023.020448	23.190400
112.794858	4031.725351	23.195418
113.247422	4024.055982	23.200435
113.163242	4057.310799	23.205453
113.404879	4055.246000	23.210471
113.368618	4050.428880	23.215488
113.659784	4057.892006	23.220506
114.018286	4052.218021	23.225523
114.012005	4067.681521	23.230541
113.739051	4074.414371	23.235559
114.159510	4081.660015	23.240576
114.090288	4090.811363	23.245594
114.035856	4077.075254	23.250611
114.191711	4094.517037	23.255629
114.330813	4104.407692	23.260647
114.444723	4104.507885	23.265664
114.579048	4104.211558	23.270682
114.626467	4123.203088	23.275699
114.522227	4138.090376	23.280717
114.662920	4138.057596	23.285735
115.434663	4154.378623	23.290752
115.156387	4173.487482	23.295770
115.653793	4170.465970	23.300787
115.789053	4164.437983	23.305805
116.002025	4170.640201	23.310823
116.066148	4159.366270	23.315840
116.297570	4168.308599	23.320858
116.471748	4159.430639	23.325875
116.007005	4169.617821	23.330893
116.090840	4172.282143	23.335911
116.778539	4176.704086	23.340928
116.260447	4191.783666	23.345946
116.434306	4192.819514	23.350963
116.357344	4183.802654	23.355981
116.799216	4213.609208	23.360999
116.616133	4227.412153	23.366016
116.930551	4230.029079	23.371034
117.085094	4219.725706	23.376051
116.870667	4236.733349	23.381069
117.180196	4254.592396	23.386087
117.629292	4253.953834	23.391104
117.251756	4256.383791	23.396122
117.638239	4264.122095	23.401139
118.074825	4283.239280	23.406157
118.003592	4279.927722	23.411175
118.513286	4282.600969	23.416192
118.101428	4286.193047	23.421210
118.643673	4280.474879	23.426227
118.788698	4275.802252	23.431245
118.654940	4279.136357	23.436263
119.169847	4279.509636	23.441280
119.004681	4279.430050	23.446298
119.078601	4284.649569	23.451315
118.555932	4284.591102	23.456333
118.601847	4290.035170	23.461351
119.111537	4303.269683	23.466368
118.871786	4309.242394	23.471386
119.192213	4318.589354	23.476403
119.423337	4327.671234	23.481421
119.460379	4341.282954	23.486439
119.650355	4339.968132	23.491456
119.874131	4351.870991	23.496474
120.140745	4367.132837	23.501491
120.180203	4374.049332	23.506509
120.159879	4371.460733	23.511527
120.623393	4372.009803	23.516544
120.491916	4371.885059	23.521562
120.957940	4368.952380	23.526579
120.930624	4381.914348	23.531597
120.754879	4400.260018	23.536615
120.905398	4401.974092	23.541632
120.815181	4408.559974	23.546650
121.087385	4403.366149	23.551667
121.520833	4411.741543	23.556685
121.783855	4423.977985	23.561703
121.680728	4420.226853	23.566720
121.860329	4420.406364	23.571738
122.030914	4420.816622	23.576755
122.219896	4423.889070	23.581773
121.701194	4426.917436	23.586791
122.141138	4432.489336	23.591808
122.344891	4450.273010	23.596826
122.004119	4456.619892	23.601843
122.864454	4451.634766	23.606861
122.548304	4453.609217	23.611879
123.090355	4457.637977	23.616896
123.151816	4463.671740	23.621914
123.457555	4479.138074	23.626931
123.469783	4480.787649	23.631949
123.729615	4476.278013	23.636967
123.641813	4475.045457	23.641984
123.824819	4478.542687	23.647002
123.863166	4481.067572	23.652019
124.320076	4479.007559	23.657037
124.087880	4470.485002	23.662055
124.175135	4471.011152	23.667072
124.159032	4476.576973	23.672090
123.995011	4473.476614	23.677107
123.983007	4480.344479	23.682125
123.990789	4509.994446	23.687143
124.534608	4500.960774	23.692160
124.749608	4505.545762	23.697178
125.056786	4509.721920	23.702195
125.068433	4502.340572	23.707213
125.106264	4515.878269	23.712231
125.205399	4518.711732	23.717248
125.069235	4529.839173	23.722266
125.593141	4530.038425	23.727283
125.496430	4524.875511	23.732301
125.575691	4540.393333	23.737319
125.889025	4533.167400	23.742336
125.806778	4560.608610	23.747354
125.863022	4567.673538	23.752371
126.015554	4568.583107	23.757389
125.654692	4568.265332	23.762407
125.428489	4581.036294	23.767424
126.077943	4587.824679	23.772442
126.116410	4615.429596	23.777459
126.435074	4620.912873	23.782477
126.803642	4634.243533	23.787495
126.795382	4644.552822	23.792512
126.852128	4657.252497	23.797530
127.173284	4660.082580	23.802547
127.689368	4652.157065	23.807565
127.681207	4649.205596	23.812583
128.017141	4672.654426	23.817600
128.106214	4682.420908	23.822618
128.255578	4677.580439	23.827635
128.629978	4671.847587	23.832653
128.795826	4676.248079	23.837671
128.939231	4669.086660	23.842688
128.933755	4666.704194	23.847706
128.835549	4677.713386	23.852723
128.575082	4666.928731	23.857741
128.801274	4673.110766	23.862759
128.999611	4654.346615	23.867776
128.977321	4668.806052	23.872794
129.103398	4665.514935	23.877811
129.345564	4679.471425	23.882829
129.377381	4690.452823	23.887847
129.219108	4695.263325	23.892864
129.614424	4688.061075	23.897882
130.048284	4705.281017	23.902899
130.247067	4712.063226	23.907917
129.961694	4724.303333	23.912935
130.038077	4727.717291	23.917952
130.090806	4729.238652	23.922970
130.063699	4736.286438	23.927987
130.540960	4739.231551	23.933005
130.288960	4751.748723	23.938023
130.354039	4759.018585	23.943040
130.712291	4772.963921	23.948058
130.874078	4788.157504	23.953075
131.039817	4788.888389	23.958093
130.937344	4793.731100	23.963111
130.952838	4799.546816	23.968128
131.435045	4814.826484	23.973146
131.482647	4821.558255	23.978163
131.492377	4825.394027	23.983181
131.672771	4851.888067	23.988199
132.224847	4852.445604	23.993216
132.452979	4840.185287	23.998234
132.253446	4852.985764	24.003251
133.006556	4847.297410	24.008269
132.785253	4851.352379	24.013287
132.550688	4835.369389	24.018304
132.820153	4858.175351	24.023322
132.530440	4868.191194	24.028339
133.059843	4856.577867	24.033357
133.371953	4878.246266	24.038375
133.015332	4886.190246	24.043392
133.387156	4898.126423	24.048410
133.357492	4906.170318	24.053427
133.508733	4906.966706	24.058445
133.624762	4932.177010	24.063463
133.920587	4929.435666	24.068480
134.113025	4935.607837	24.073498
134.282697	4932.782573	24.078515
134.520036	4951.026557	24.083533
134.551107	4960.102138	24.088551
134.364539	4964.447340	24.093568
135.118218	4958.391015	24.098586
135.253363	4958.795549	24.103603
135.192401	4966.453374	24.108621
135.400656	4978.880796	24.113639
135.239749	4988.632822	24.118656
135.587554	4992.201160	24.123674
135.315341	4997.598400	24.128691
135.911919	4998.059309	24.133709
136.085659	5016.734882	24.138727
136.086099	5020.737702	24.143744
136.020575	5018.199280	24.148762
136.105062	5021.809615	24.153779
136.809725	5021.438342	24.158797
136.944421	5031.319306	24.163815
136.979122	5049.446911	24.168832
137.230755	5057.550569	24.173850
136.983921	5055.830887	24.178867
137.035819	5053.017915	24.183885
137.111659	5059.657515	24.188903
137.104778	5055.245425	24.193920
137.375047	5065.812853	24.198938
137.511135	5086.216793	24.203955
137.611085	5077.911863	24.208973
138.488458	5074.573785	24.213991
138.632883	5073.234419	24.219008
138.322618	5064.327943	24.224026
138.184152	5079.408656	24.229043
138.341454	5086.059508	24.234061
138.678526	5097.424436	24.239079
138.624660	5104.241461	24.244096
139.285119	5101.468298	24.249114
139.496427	5100.004828	24.254131
139.225843	5101.645452	24.259149
138.782064	5097.724134	24.264167
138.705984	5119.171912	24.269184
139.107048	5129.356209	24.274202
139.037494	5139.317151	24.279219
139.292419	5151.712291	24.284237
139.384776	5155.873462	24.289255
139.449285	5174.246577	24.294272
139.758692	5184.040973	24.299290
139.636684	5197.208880	24.304307
140.125169	5214.687821	24.309325
140.311888	5220.419988	24.314343
140.541280	5227.375185	24.319360
140.873818	5235.223251	24.324378
140.707821	5247.403911	24.329395
140.869191	5257.967293	24.334413
141.082785	5264.874803	24.339431
141.262847	5281.175557	24.344448
141.543308	5279.348915	24.349466
141.491918	5284.651683	24.354483
141.692942	5286.941652	24.359501
142.020248	5307.997586	24.364519
142.094914	5316.579902	24.369536
142.847319	5303.711064	24.374554
142.647069	5316.941318	24.379571
143.118919	5297.437942	24.384589
143.274734	5296.595992	24.389607
143.296367	5302.384846	24.394624
143.592543	5299.778860	24.399642
143.756446	5297.874525	24.404659
143.633422	5294.668516	24.409677
143.849620	5300.193227	24.414695
143.662671	5291.509661	24.419712
143.890526	5294.403116	24.424730
143.809586	5315.376236	24.429747
143.917220	5324.377463	24.434765
144.504093	5323.919255	24.439783
144.508297	5332.451432	24.444800
144.499753	5316.808082	24.449818
144.534726	5324.771793	24.454835
144.575707	5346.337654	24.459853
144.972521	5345.554421	24.464871
144.777316	5359.929917	24.469888
144.872012	5353.357059	24.474906
144.984541	5376.687696	24.479923
145.061870	5394.029372	24.484941
145.602822	5395.675837	24.489959
145.158808	5404.397529	24.494976
145.554723	5412.493177	24.499994
145.481616	5431.192650	24.505011
145.364186	5432.139885	24.510029
145.792673	5449.727832	24.515047
145.657305	5456.269112	24.520064
146.134924	5455.700451	24.525082
146.268927	5473.198698	24.530099
146.670585	5474.836756	24.535117
147.190510	5472.852464	24.540135
147.421409	5478.976508	24.545152
147.737461	5476.487602	24.550170
147.877111	5486.711430	24.555187
147.896637	5486.420582	24.560205
148.155567	5484.453462	24.565223
148.443810	5488.282608	24.570240
148.675464	5483.990194	24.575258
148.108359	5479.963891	24.580275
148.167561	5484.798001	24.585293
148.720412	5491.616733	24.590311
148.282763	5496.598247	24.595328
148.574053	5497.730630	24.600346
148.403498	5503.375275	24.605363
148.591918	5521.415627	24.610381
148.727659	5518.534638	24.615399
148.343247	5537.516031	24.620416
149.129875	5553.746166	24.625434
149.069675	5565.359127	24.630451
149.132407	5585.952727	24.635469
149.745240	5591.920756	24.640487
149.688623	5606.260112	24.645504
150.355323	5621.438831	24.650522
150.311326	5628.009416	24.655539
150.716677	5633.660144	24.660557
150.656951	5622.646652	24.665575
150.891517	5634.256393	24.670592
150.742447	5642.521991	24.675610
150.697921	5655.171295	24.680627
150.903626	5656.460934	24.685645
151.345101	5668.303834	24.690663
151.265225	5678.546513	24.695680
151.541543	5682.703069	24.700698
151.777660	5691.324077	24.705715
152.303140	5717.246040	24.710733
152.514513	5714.587571	24.715751
152.583771	5718.578770	24.720768
152.525823	5714.465910	24.725786
152.479547	5706.739470	24.730803
152.631891	5700.135320	24.735821
153.023407	5705.488334	24.740839
153.211475	5715.435405	24.745856
153.326427	5721.352563	24.750874
153.329146	5721.902700	24.755891
153.309777	5714.663165	24.760909
153.846854	5712.467953	24.765927
153.712846	5729.570531	24.770944
153.960715	5744.055526	24.775962
154.355865	5747.585989	24.780979
154.128882	5758.285596	24.785997
154.378833	5756.186074	24.791015
154.099134	5763.285492	24.796032
154.244278	5757.838893	24.801050
153.979507	5772.063631	24.806067
154.187498	5785.886745	24.811085
154.795350	5810.943238	24.816103
154.761775	5814.993050	24.821120
154.915812	5823.577000	24.826138
154.910346	5841.645439	24.831155
155.241323	5848.225090	24.836173
155.384668	5864.372834	24.841191
155.467144	5878.561771	24.846208
155.681479	5885.174037	24.851226
155.563024	5903.496650	24.856243
156.178099	5920.335535	24.861261
156.539411	5927.169174	24.866279
156.715382	5950.814311	24.871296
156.738597	5945.575236	24.876314
157.024299	5944.162743	24.881331
156.892942	5960.603440	24.886349
157.163999	5968.746773	24.891367
157.572890	5971.457291	24.896384
157.804501	5968.849663	24.901402
157.660474	5991.532785	24.906419
157.707648	6003.402568	24.911437
158.442177	6011.007237	24.916455
158.134125	6013.084463	24.921472
158.109705	6011.896848	24.926490
158.300299	6033.377337	24.931507
158.512113	6046.054690	24.936525
158.782481	6053.807480	24.941543
158.747705	6068.470407	24.946560
159.428091	6079.600741	24.951578
159.328720	6079.557125	24.956595
159.029984	6101.097170	24.961613
159.454882	6107.226799	24.966631
159.537536	6122.269017	24.971648
159.727329	6139.688327	24.976666
160.330795	6137.361159	24.981683
160.228471	6147.707239	24.986701
160.412973	6152.516922	24.991719
160.844592	6167.817599	24.996736
160.939024	6176.848353	25.001754
160.745145	6173.358130	25.006771
160.788245	6192.041725	25.011789
161.258138	6196.688278	25.016807
161.638208	6208.060024	25.021824
161.658443	6202.060439	25.026842
162.027251	6210.028807	25.031859
161.656007	6243.874631	25.036877
161.867548	6237.463344	25.041895
162.380803	6232.382788	25.046912
162.462858	6237.141527	25.051930
162.751706	6244.888879	25.056947
162.956737	6256.817651	25.061965
162.885521	6256.968502	25.066983
162.895608	6259.629277	25.072000
163.097271	6261.148099	25.077018
163.502900	6249.313154	25.082035
163.397425	6269.070766	25.087053
163.271666	6280.220488	25.092071
163.738398	6285.829420	25.097088
163.915751	6287.242130	25.102106
164.350555	6296.452496	25.107123
164.084345	6319.711587	25.112141
164.155014	6312.776950	25.117159
164.197256	6317.250291	25.122176
164.301743	6351.988420	25.127194
164.797749	6347.628405	25.132211
164.640462	6357.452327	25.137229
165.166733	6373.763386	25.142247
165.417762	6384.607545	25.147264
165.463856	6385.163661	25.152282
165.910179	6387.961575	25.157299
165.684577	6408.219678	25.162317
165.810925	6409.516681	25.167335
166.142994	6426.948152	25.172352
165.815795	6435.784290	25.177370
166.331149	6433.141339	25.182387
166.503811	6458.137966	25.187405
166.584025	6462.649739	25.192423
167.148097	6470.951849	25.197440
166.968314	6478.716631	25.202458
167.325849	6497.706676	25.207475
166.934518	6510.956494	25.212493
167.693377	6522.538451	25.217511
167.681524	6531.414324	25.222528
167.822407	6538.356123	25.227546
168.113158	6545.313985	25.232563
168.197042	6566.655938	25.237581
168.227145	6568.412949	25.242599
168.402445	6586.857716	25.247616
168.063360	6593.547816	25.252634
168.573922	6604.891175	25.257651
168.947330	6631.501611	25.262669
169.148364	6639.262633	25.267687
169.329703	6649.999183	25.272704
169.119575	6661.837152	25.277722
169.678063	6670.776820	25.282739
169.740524	6696.752181	25.287757
170.027171	6701.936816	25.292775
170.462380	6704.319189	25.297792
170.443185	6725.118937	25.302810
170.746447	6728.639379	25.307827
170.858011	6738.749876	25.312845
171.087319	6740.617704	25.317863
170.963345	6763.288241	25.322880
170.935253	6775.499203	25.327898
171.040239	6765.509905	25.332915
171.121565	6784.971448	25.337933
171.715334	6791.801850	25.342951
171.945278	6800.223642	25.347968
171.788991	6823.715912	25.352986
172.098366	6815.739696	25.358003
172.106021	6829.280594	25.363021
172.540817	6837.096171	25.368039
173.314625	6833.424164	25.373056
173.333111	6843.189894	25.378074
173.661557	6840.226006	25.383091
173.703812	6837.965800	25.388109
173.970466	6830.274188	25.393127
175.100540	6827.365886	25.398144
174.698788	6817.036461	25.403162
175.234760	6798.547495	25.408179
175.012532	6806.957788	25.413197
175.319118	6811.532475	25.418215
175.511706	6807.154241	25.423232
174.843325	6803.067754	25.428250
175.135145	6806.984837	25.433267
175.099219	6804.356767	25.438285
175.471361	6815.954816	25.443303
175.311602	6834.307633	25.448320
175.249080	6846.708885	25.453338
175.207790	6845.809265	25.458355
175.409472	6864.115912	25.463373
174.910821	6877.297775	25.468391
175.658418	6895.763745	25.473408
175.474709	6933.931215	25.478426
175.693206	6932.998086	25.483443
176.279109	6969.362097	25.488461
176.356646	6980.655489	25.493479
176.792731	6993.892272	25.498496
176.940924	7014.878760	25.503514
177.446460	7030.040767	25.508531
177.427363	7037.898014	25.513549
177.760798	7058.092616	25.518567
177.903850	7068.800563	25.523584
177.859929	7076.684928	25.528602
178.200031	7083.102826	25.533619
178.481059	7101.940488	25.538637
178.600465	7112.330321	25.543655
179.127575	7111.764945	25.548672
179.258005	7131.842402	25.553690
179.697528	7135.882347	25.558707
179.763621	7131.732103	25.563725
179.999139	7129.326864	25.568743
180.146831	7126.129221	25.573760
180.034405	7149.367091	25.578778
179.879433	7164.779523	25.583795
180.518243	7169.462794	25.588813
180.277878	7169.678885	25.593831
180.687141	7176.869582	25.598848
180.573449	7203.783470	25.603866
180.977563	7193.507086	25.608883
181.081910	7211.683503	25.613901
181.025605	7231.934894	25.618919
181.280681	7227.086565	25.623936
181.297083	7244.169702	25.628954
181.444801	7248.291208	25.633971
182.065629	7268.395060	25.638989
182.056441	7281.068739	25.644007
182.454383	7289.426543	25.649024
182.500334	7300.122929	25.654042
183.178913	7310.938544	25.659059
183.261063	7329.322145	25.664077
183.632691	7316.297981	25.669095
184.509866	7296.509211	25.674112
184.359399	7297.253457	25.679130
184.465657	7297.183253	25.684148
184.649888	7296.526972	25.689165
184.659355	7301.246478	25.694183
184.793705	7291.881250	25.699200
184.618854	7297.583192	25.704218
184.817013	7299.493452	25.709236
184.733722	7293.137012	25.714253
184.959787	7316.900841	25.719271
185.123776	7316.845949	25.724288
185.388021	7337.619176	25.729306
185.186193	7334.613753	25.734324
185.503743	7357.311067	25.739341
185.702915	7371.282018	25.744359
186.363955	7380.063497	25.749376
186.191643	7399.988364	25.754394
186.583936	7399.486267	25.759412
186.357638	7402.046741	25.764429
185.952376	7423.863636	25.769447
186.183488	7428.946952	25.774464
186.560945	7461.319110	25.779482
187.140087	7485.114046	25.784500
187.193212	7483.824009	25.789517
187.160041	7497.968822	25.794535
187.463655	7516.516347	25.799552
187.449203	7536.686896	25.804570
187.986763	7551.676900	25.809588
188.672790	7556.839834	25.814605
188.755438	7591.267705	25.819623
189.189068	7589.879347	25.824640
189.225198	7594.827553	25.829658
188.895741	7593.744103	25.834676
189.572044	7609.647059	25.839693
189.503015	7625.981880	25.844711
189.494821	7620.355323	25.849728
189.823955	7643.106990	25.854746
189.875478	7658.159139	25.859764
189.879438	7669.145787	25.864781
190.337781	7694.453819	25.869799
190.640572	7688.826711	25.874816
191.267638	7708.807153	25.879834
191.688730	7710.112825	25.884852
191.810993	7703.393265	25.889869
192.125774	7701.835412	25.894887
192.609524	7688.497881	25.899904
192.781859	7698.362231	25.904922
193.021699	7695.672562	25.909940
193.018735	7682.762733	25.914957
192.935743	7680.744459	25.919975
193.201442	7678.861786	25.924992
193.101889	7675.546496	25.930010
193.049615	7696.402806	25.935028
193.498440	7686.881816	25.940045
193.280414	7693.050582	25.945063
193.392346	7698.308034	25.950080
193.609726	7700.541194	25.955098
193.819189	7708.851172	25.960116
193.686238	7722.390142	25.965133
193.862310	7740.987364	25.970151
194.101065	7753.060367	25.975168
194.182717	7774.767487	25.980186
194.077091	7791.209588	25.985204
194.323265	7813.954448	25.990221
194.410082	7831.354652	25.995239
195.210296	7858.201210	26.000256
195.068439	7877.073672	26.005274
195.121000	7896.154684	26.010292
195.618729	7908.194441	26.015309
195.197754	7931.554083	26.020327
195.468183	7946.023030	26.025344
196.198872	7969.454742	26.030362
196.132998	7991.081087	26.035380
196.481518	8001.114737	26.040397
196.595923	8022.942625	26.045415
197.223630	8044.866115	26.050432
197.496358	8061.774619	26.055450
197.385922	8064.066387	26.060468
198.151325	8080.659630	26.065485
198.037128	8096.167591	26.070503
198.176846	8106.994187	26.075520
198.530009	8120.237453	26.080538
198.424284	8125.948320	26.085556
198.727856	8141.872369	26.090573
199.208452	8159.094346	26.095591
199.574593	8156.994297	26.100608
199.638635	8178.196838	26.105626
199.752145	8177.071290	26.110644
200.219972	8174.937264	26.115661
200.367333	8197.059898	26.120679
200.522335	8213.523142	26.125696
200.857898	8219.530249	26.130714
200.488100	8237.306959	26.135732
200.895465	8242.011319	26.140749
200.927740	8254.242993	26.145767
201.038689	8255.559334	26.150784
201.419714	8267.223881	26.155802
201.227110	8285.402783	26.160820
202.059798	8302.124955	26.165837
202.303352	8318.781901	26.170855
202.000742	8328.646117	26.175872
202.290872	8326.717429	26.180890
202.143253	8347.115867	26.185908
202.462060	8353.882996	26.190925
202.621495	8367.952227	26.195943
203.113254	8378.994399	26.200960
203.226943	8392.156827	26.205978
203.441254	8405.457219	26.210996
203.982713	8408.061929	26.216013
203.906000	8419.875168	26.221031
204.594410	8427.925371	26.226048
204.801188	8425.770671	26.231066
205.120123	8429.791442	26.236084
205.405207	8428.478901	26.241101
205.589160	8441.393763	26.246119
205.784727	8456.547234	26.251136
206.090353	8454.823862	26.256154
206.141081	8454.134485	26.261172
206.853318	8444.651410	26.266189
206.784758	8457.546544	26.271207
206.965848	8451.288499	26.276224
207.319431	8447.926100	26.281242
207.145109	8454.071906	26.286260
207.227478	8449.270150	26.291277
207.589877	8471.582408	26.296295
207.517617	8478.405595	26.301312
207.561718	8473.681296	26.306330
207.330835	8495.944022	26.311348
207.838422	8505.259005	26.316365
208.007306	8507.738518	26.321383
207.944644	8540.809896	26.326400
208.110358	8544.413409	26.331418
208.494332	8583.626692	26.336436
208.526460	8586.165899	26.341453
208.616754	8606.949315	26.346471
208.975678	8619.653914	26.351488
209.445992	8636.024150	26.356506
209.369688	8653.932999	26.361524
209.849632	8668.351715	26.366541
209.694255	8688.176789	26.371559
210.032642	8708.809088	26.376576
210.095637	8715.449259	26.381594
210.900332	8740.580608	26.386612
211.006106	8748.147842	26.391629
210.878095	8761.219644	26.396647
211.289860	8781.209182	26.401664
211.481792	8789.724415	26.406682
211.733671	8807.226586	26.411700
211.760779	8817.372567	26.416717
211.731991	8831.751002	26.421735
211.919292	8847.601928	26.426752
212.783697	8861.619292	26.431770
212.645148	8872.260110	26.436788
212.961280	8881.830305	26.441805
213.217044	8901.928670	26.446823
213.361567	8913.973792	26.451840
213.678119	8923.069653	26.456858
213.657061	8940.131861	26.461876
214.032284	8945.434406	26.466893
214.806315	8953.868854	26.471911
214.720915	8967.160421	26.476928
215.369009	8965.657981	26.481946
216.086263	8949.592017	26.486964
216.569882	8937.995429	26.491981
216.580226	8943.149373	26.496999
216.234345	8947.994089	26.502016
216.416222	8941.677419	26.507034
215.962386	8954.124522	26.512052
216.288860	8962.591573	26.517069
216.504465	8969.798156	26.522087
216.471775	8987.688081	26.527104
216.918908	9002.900578	26.532122
216.943595	9015.437455	26.537140
216.742064	9030.800561	26.542157
216.981873	9045.326958	26.547175
217.126156	9072.297440	26.552192
217.718417	9093.017499	26.557210
217.690161	9120.184663	26.562228
218.253574	9122.867670	26.567245
218.379516	9150.115602	26.572263
218.338665	9152.854920	26.577280
219.004182	9173.124473	26.582298
219.320377	9189.977865	26.587316
219.353184	9214.367737	26.592333
219.385135	9218.619897	26.597351
219.998186	9239.045069	26.602368
220.033897	9247.198116	26.607386
220.009175	9258.932147	26.612404
220.601943	9275.698828	26.617421
220.304449	9297.759772	26.622439
220.648770	9308.474106	26.627456
220.989570	9323.085866	26.632474
221.164580	9344.618370	26.637492
221.318227	9364.925481	26.642509
221.867892	9380.940150	26.647527
221.931385	9385.872398	26.652544
222.410104	9396.122543	26.657562
222.894161	9414.126059	26.662580
223.083198	9423.527696	26.667597
223.530832	9440.888275	26.672615
223.520353	9454.238307	26.677632
223.465234	9453.157335	26.682650
224.062018	9468.338317	26.687668
224.044905	9480.220902	26.692685
224.118504	9482.001504	26.697703
224.263449	9500.301183	26.702720
224.523747	9502.676939	26.707738
224.891772	9512.843708	26.712756
224.648510	9531.591300	26.717773
225.168559	9540.983540	26.722791
225.335174	9551.726921	26.727808
225.647015	9569.755403	26.732826
225.790170	9584.210610	26.737844
225.700089	9592.588667	26.742861
226.217741	9613.935160	26.747879
226.116423	9629.741780	26.752896
226.475339	9637.877441	26.757914
226.722292	9652.319643	26.762932
226.613679	9671.499716	26.767949
227.154180	9676.468473	26.772967
227.436021	9699.163396	26.777984
227.886200	9703.726909	26.783002
228.409011	9724.147681	26.788020
228.480117	9736.746495	26.793037
228.797823	9732.459484	26.798055
228.840455	9745.967686	26.803072
228.738836	9756.627967	26.808090
229.361133	9772.536029	26.813108
229.611484	9782.636470	26.818125
230.273196	9792.742045	26.823143
230.105986	9796.875644	26.828160
230.042116	9795.613357	26.833178
230.384392	9816.975998	26.838196
230.753204	9820.530804	26.843213
230.861172	9830.072637	26.848231
230.849513	9854.969046	26.853248
231.196273	9865.382356	26.858266
231.508194	9884.425989	26.863284
231.407125	9893.931205	26.868301
231.659486	9918.908520	26.873319
231.661979	9937.720034	26.878336
232.108625	9954.534531	26.883354
232.839332	9969.385750	26.888372
232.816545	9980.585773	26.893389
233.301240	9980.710702	26.898407
233.576977	10011.710046	26.903424
233.857070	10015.313194	26.908442
234.155536	10035.393044	26.913460
234.267911	10047.862113	26.918477
234.538598	10053.078940	26.923495
234.618100	10058.880076	26.928512
234.864487	10080.759036	26.933530
235.313041	10090.055121	26.938548
235.458401	10093.342581	26.943565
235.398433	10108.882569	26.948583
235.619555	10128.567654	26.953600
235.830825	10136.462561	26.958618
236.059318	10147.219369	26.963636
236.288297	10174.998175	26.968653
236.694273	10188.178151	26.973671
236.689064	10202.342599	26.978688
236.783248	10211.337056	26.983706
237.018888	10230.146766	26.988724
236.942240	10253.200170	26.993741
237.297448	10264.110253	26.998759
237.682571	10286.011408	27.003776
238.077070	10282.508465	27.008794
238.103589	10303.795078	27.013812
238.413381	10322.886867	27.018829
238.830611	10337.101939	27.023847
239.050831	10347.920180	27.028864
238.803248	10359.905946	27.033882
239.337630	10386.524948	27.038900
238.974062	10404.818261	27.043917
239.767146	10418.798788	27.048935
239.542039	10446.164227	27.053952
240.005127	10459.057284	27.058970
240.354870	10478.098284	27.063988
240.290626	10517.553034	27.069005
240.817438	10532.770652	27.074023
241.300801	10562.306153	27.079040
241.672657	10569.926335	27.084058
241.763314	10594.029437	27.089076
241.944633	10607.639077	27.094093
242.070483	10632.336609	27.099111
242.085828	10649.117021	27.104128
242.654817	10670.675157	27.109146
242.980979	10689.135797	27.114164
242.960932	10713.622079	27.119181
243.027390	10732.633140	27.124199
243.500463	10756.971927	27.129216
243.381714	10780.773959	27.134234
243.980467	10813.240196	27.139252
244.200133	10830.989614	27.144269
244.399815	10840.459590	27.149287
244.764516	10871.089173	27.154304
245.179253	10879.507434	27.159322
245.225980	10898.977506	27.164340
245.223429	10930.552652	27.169357
245.876342	10944.967397	27.174375
246.162728	10968.504848	27.179392
246.201886	10978.804555	27.184410
246.686384	10991.125464	27.189428
247.092666	11010.601804	27.194445
247.402401	11031.245129	27.199463
247.775700	11048.379061	27.204480
247.873240	11057.579856	27.209498
248.650307	11060.053225	27.214516
248.706480	11072.253777	27.219533
248.778659	11087.240964	27.224551
249.092742	11096.502371	27.229568
249.399844	11100.660584	27.234586
250.084198	11123.140370	27.239604
250.136872	11148.643915	27.244621
250.235873	11140.112249	27.249639
250.002726	11158.841067	27.254656
250.437116	11176.380707	27.259674
250.825594	11178.205232	27.264692
250.805928	11189.635637	27.269709
251.016438	11204.950653	27.274727
251.152325	11222.453255	27.279744
251.379988	11229.059928	27.284762
251.717632	11248.070810	27.289780
251.719279	11272.807938	27.294797
251.710271	11284.247613	27.299815
252.034518	11299.716576	27.304832
252.268550	11329.636610	27.309850
252.691622	11341.613729	27.314868
252.859106	11358.124523	27.319885
253.290813	11376.380316	27.324903
253.613153	11384.663387	27.329920
253.842133	11407.201133	27.334938
254.113516	11413.012413	27.339956
254.440042	11437.196105	27.344973
254.639377	11443.691100	27.349991
255.200744	11470.943938	27.355008
255.281432	11484.404510	27.360026
255.635637	11490.975416	27.365044
255.750475	11512.374546	27.370061
255.788155	11515.797372	27.375079
256.247364	11531.117346	27.380096
256.223078	11556.265945	27.385114
256.819125	11577.704028	27.390132
256.815866	11587.633158	27.395149
257.612512	11603.546235	27.400167
257.685861	11605.407489	27.405184
257.722316	11637.888227	27.410202
257.992210	11637.165879	27.415220
258.099398	11664.238430	27.420237
258.312457	11683.866893	27.425255
258.883068	11704.333976	27.430272
259.011721	11719.526396	27.435290
259.256725	11738.438684	27.440308
259.633029	11745.139864	27.445325
260.091946	11761.717737	27.450343
260.542533	11767.236816	27.455360
260.790195	11788.686036	27.460378
260.853449	11792.723899	27.465396
261.057978	11809.121633	27.470413
261.435104	11822.903606	27.475431
261.707423	11838.996617	27.480448
261.450711	11851.003950	27.485466
261.981361	11866.750121	27.490484
261.999730	11886.952763	27.495501
261.761258	11903.965513	27.500519
262.624022	11924.702724	27.505536
262.333949	11951.733523	27.510554
262.792836	11963.408675	27.515572
263.271016	11997.217053	27.520589
263.116801	12013.772618	27.525607
263.558948	12032.252726	27.530624
263.758339	12054.681390	27.535642
264.359009	12081.476198	27.540660
264.626961	12102.592966	27.545677
265.358066	12116.740039	27.550695
265.150734	12120.006410	27.555712
265.246586	12149.702621	27.560730
265.628687	12152.601621	27.565748
265.760528	12182.173520	27.570765
266.193512	12198.226739	27.575783
266.525660	12215.690463	27.580800
266.762150	12232.477150	27.585818
267.028242	12247.938069	27.590836
266.784191	12269.073465	27.595853
267.001268	12284.232343	27.600871
267.670047	12303.859089	27.605888
267.452518	12334.892239	27.610906
267.629545	12359.369271	27.615924
268.273641	12393.517247	27.620941
268.195403	12406.961690	27.625959
268.966489	12432.402413	27.630976
269.166750	12457.203427	27.635994
269.695552	12467.465851	27.641012
269.749269	12488.679727	27.646029
269.857340	12511.548626	27.651047
270.292442	12524.408721	27.656064
270.391092	12560.433053	27.661082
270.712738	12575.419823	27.666100
270.756068	12603.091165	27.671117
270.985602	12631.066339	27.676135
271.647769	12656.097391	27.681152
271.757715	12680.127765	27.686170
272.459489	12700.357695	27.691188
272.561391	12716.734528	27.696205
272.847560	12739.234363	27.701223
273.084504	12761.748969	27.706240
273.511045	12780.554119	27.711258
273.503410	12803.354996	27.716276
273.944611	12825.393379	27.721293
274.062313	12848.395063	27.726311
274.478693	12873.637217	27.731328
274.605758	12896.536494	27.736346
275.016020	12907.207232	27.741364
275.044813	12923.462834	27.746381
275.191631	12956.439497	27.751399
275.917568	12979.127492	27.756416
276.117651	13013.173190	27.761434
276.292330	13024.259495	27.766452
276.646474	13042.513110	27.771469
276.669615	13057.411212	27.776487
277.076680	13081.894024	27.781504
276.857811	13102.138825	27.786522
277.792315	13128.558181	27.791540
278.187328	13163.466010	27.796557
278.475552	13170.865334	27.801575
280.061752	13170.041825	27.806592
279.902501	13172.923470	27.811610
280.306155	13159.380078	27.816628
280.926203	13167.948744	27.821645
280.832663	13166.163280	27.826663
281.170459	13161.993302	27.831680
281.141714	13171.171223	27.836698
281.349509	13153.855087	27.841716
282.077663	13155.462436	27.846733
282.263325	13176.323602	27.851751
282.644951	13177.760235	27.856768
282.884696	13182.770601	27.861786
282.989448	13183.797615	27.866804
282.936818	13186.917895	27.871821
282.842647	13194.088037	27.876839
282.980320	13191.003623	27.881856
282.988309	13211.576911	27.886874
283.195027	13227.901614	27.891892
283.248705	13252.383783	27.896909
283.555605	13286.550439	27.901927
284.141248	13308.219543	27.906944
284.312421	13329.592477	27.911962
284.204434	13359.135100	27.916980
284.506510	13383.811310	27.921997
284.814532	13416.280545	27.927015
285.138494	13430.842144	27.932032
285.339418	13454.189773	27.937050
285.674268	13478.020422	27.942068
286.160348	13501.724313	27.947085
286.466830	13530.291496	27.952103
286.948688	13555.272869	27.957120
287.319212	13575.469243	27.962138
287.886525	13588.443065	27.967156
288.436527	13597.722201	27.972173
288.384513	13625.351711	27.977191
288.828402	13641.297300	27.982208
288.459906	13662.737945	27.987226
288.819177	13680.944107	27.992244
289.197595	13699.588335	27.997261
289.402410	13735.932769	28.002279
289.750253	13752.091949	28.007296
289.991125	13777.655591	28.012314
290.156557	13806.617830	28.017332
290.529870	13830.280051	28.022349
290.683605	13849.119000	28.027367
291.216259	13880.056429	28.032384
291.311407	13911.967330	28.037402
291.714890	13929.130635	28.042420
292.305173	13947.174555	28.047437
292.384672	13976.550597	28.052455
292.678253	13999.077683	28.057472
292.896992	14026.975121	28.062490
293.332259	14045.439768	28.067508
293.689158	14065.336449	28.072525
294.022933	14092.582225	28.077543
294.048259	14100.173616	28.082560
294.497265	14136.076722	28.087578
294.741898	14139.628551	28.092596
295.227644	14162.918910	28.097613
295.746716	14164.683571	28.102631
296.632330	14178.117150	28.107648
296.707210	14179.606450	28.112666
296.903303	14193.810775	28.117684
297.458859	14191.839865	28.122701
297.298279	14200.230781	28.127719
298.079164	14210.071232	28.132736
298.516532	14206.489195	28.137754
298.723852	14199.685400	28.142772
298.952625	14201.189307	28.147789
299.029476	14226.581579	28.152807
299.433756	14224.160577	28.157824
299.853788	14227.803732	28.162842
300.069101	14234.339657	28.167860
300.140717	14248.778154	28.172877
300.268774	14256.123458	28.177895
300.520494	14268.475713	28.182912
300.699821	14286.004088	28.187930
301.077579	14300.727471	28.192948
301.402467	14321.936638	28.197965
301.008996	14346.608983	28.202983
301.523609	14358.517461	28.208000
301.657666	14389.743262	28.213018
301.593341	14418.897273	28.218036
302.006282	14441.935699	28.223053
302.343248	14469.175246	28.228071
302.616978	14496.198698	28.233088
303.032482	14533.602690	28.238106
303.042274	14562.812030	28.243124
303.436065	14588.621835	28.248141
303.759705	14616.051482	28.253159
304.478553	14651.751837	28.258176
304.842873	14660.120801	28.263194
305.233519	14683.500703	28.268212
305.876562	14711.148459	28.273229
305.922638	14733.077429	28.278247
306.454622	14751.661851	28.283264
306.509757	14772.350375	28.288282
307.106771	14789.558646	28.293300
307.200129	14800.510340	28.298317
307.588340	14825.987303	28.303335
308.106421	14840.516881	28.308352
308.496203	14858.334506	28.313370
308.700158	14876.176118	28.318388
308.248552	14889.191622	28.323405
308.408101	14924.376830	28.328423
308.785024	14942.953365	28.333440
309.047393	14977.124851	28.338458
309.171361	15005.399578	28.343476
309.740232	15041.255736	28.348493
309.707947	15079.000951	28.353511
309.973674	15107.926212	28.358528
310.207125	15138.699754	28.363546
311.015151	15163.369150	28.368564
311.654002	15168.912293	28.373581
312.082263	15197.426812	28.378599
312.363003	15217.536550	28.383616
312.519001	15230.098241	28.388634
312.769455	15254.642653	28.393652
313.150948	15263.749848	28.398669
313.613533	15290.523121	28.403687
313.663233	15307.286637	28.408704
314.067681	15335.236423	28.413722
313.768362	15357.742450	28.418740
314.398576	15380.549481	28.423757
314.578357	15423.024366	28.428775
314.858046	15439.929875	28.433792
315.497828	15456.409552	28.438810
315.609553	15495.401555	28.443828
316.087219	15509.259247	28.448845
316.341162	15541.970499	28.453863
316.166291	15570.868043	28.458880
316.953269	15597.701288	28.463898
316.688937	15630.733264	28.468916
317.403408	15657.787111	28.473933
317.561660	15691.911706	28.478951
318.034793	15720.490370	28.483968
318.770490	15746.924369	28.488986
318.668443	15775.283282	28.494004
319.263002	15802.521859	28.499021
319.440455	15832.366770	28.504039
319.593954	15861.370905	28.509056
320.336591	15888.664640	28.514074
320.261709	15919.081040	28.519092
320.624708	15947.912274	28.524109
321.036113	15983.595682	28.529127
321.365262	16010.255841	28.534144
321.423703	16028.985915	28.539162
322.370813	16064.861434	28.544180
322.820164	16084.355331	28.549197
322.826986	16107.185080	28.554215
323.384318	16127.303690	28.559232
324.160464	16148.992750	28.564250
324.256796	16170.180401	28.569268
325.208654	16190.081713	28.574285
324.985869	16212.809083	28.579303
325.494197	16208.583902	28.584320
325.886745	16225.636391	28.589338
325.716883	16245.649623	28.594356
326.129261	16265.793245	28.599373
326.516040	16283.906131	28.604391
326.336388	16302.905899	28.609408
326.845569	16333.249752	28.614426
326.950902	16354.727732	28.619444
327.327407	16380.886950	28.624461
327.598150	16411.062146	28.629479
328.282966	16432.537072	28.634496
328.724382	16443.428621	28.639514
328.578718	16476.238573	28.644532
329.260823	16477.814758	28.649549
329.416246	16509.841709	28.654567
329.594794	16533.404028	28.659584
330.265515	16551.276216	28.664602
330.678367	16571.998681	28.669620
330.908608	16592.635811	28.674637
331.391172	16618.829249	28.679655
331.175504	16630.442044	28.684672
331.702310	16658.756162	28.689690
332.060532	16680.779235	28.694708
332.314114	16698.229646	28.699725
332.369504	16717.747666	28.704743
332.357632	16745.211534	28.709760
333.165405	16776.673175	28.714778
333.524328	16813.486642	28.719796
333.543492	16828.503896	28.724813
333.819260	16859.405792	28.729831
333.945372	16891.187840	28.734848
334.476584	16925.968335	28.739866
334.519895	16969.391210	28.744884
335.238136	16999.175480	28.749901
335.655396	17028.126980	28.754919
336.225254	17049.023343	28.759936
337.424364	17060.993026	28.764954
337.896604	17083.649756	28.769972
337.627287	17102.897543	28.774989
337.992398	17122.025584	28.780007
338.238795	17148.936646	28.785024
338.746143	17161.944057	28.790042
338.646453	17192.478957	28.795060
339.180279	17214.196752	28.800077
339.551859	17241.299335	28.805095
339.651816	17274.778181	28.810112
340.258323	17293.795682	28.815130
340.403182	17319.753292	28.820148
340.595464	17339.814543	28.825165
340.897860	17363.528647	28.830183
341.077400	17400.014705	28.835200
341.712559	17414.368825	28.840218
341.880206	17455.428946	28.845236
342.283411	17479.447548	28.850253
342.911713	17494.272717	28.855271
342.772532	17539.174020	28.860288
343.353594	17553.058267	28.865306
343.556309	17590.935999	28.870324
344.123622	17619.572726	28.875341
344.235217	17639.425873	28.880359
344.573006	17676.120315	28.885376
344.964655	17700.529044	28.890394
345.405446	17733.728100	28.895412
345.459312	17762.285953	28.900429
346.151413	17784.522851	28.905447
346.083148	17816.106638	28.910464
346.628979	17842.724706	28.915482
347.068997	17871.339537	28.920500
347.552378	17897.009845	28.925517
347.646985	17922.434663	28.930535
347.917804	17964.235099	28.935552
348.172353	17980.417543	28.940570
348.380697	18014.579288	28.945588
348.827914	18037.736645	28.950605
349.145241	18071.990189	28.955623
348.885819	18105.836565	28.960640
349.353259	18128.612200	28.965658
350.059601	18175.564902	28.970676
350.970120	18194.129297	28.975693
351.238989	18218.080538	28.980711
352.005413	18242.372223	28.985728
352.628055	18260.226109	28.990746
352.660249	18273.117170	28.995764
353.332709	18291.698823	29.000781
354.166932	18291.248419	29.005799
354.276603	18322.673381	29.010816
354.590515	18330.578283	29.015834
354.969636	18343.906572	29.020852
354.843244	18368.937950	29.025869
355.080130	18387.886033	29.030887
355.636077	18422.597607	29.035904
355.775509	18437.589383	29.040922
355.940717	18470.362568	29.045940
355.976786	18483.147492	29.050957
356.337007	18515.830585	29.055975
356.540427	18552.026532	29.060992
356.699944	18578.215340	29.066010
356.947275	18607.597581	29.071028
357.382792	18644.354646	29.076045
357.834248	18672.013442	29.081063
358.663716	18709.220269	29.086080
359.405962	18734.975205	29.091098
359.735706	18761.335358	29.096116
359.805500	18791.546129	29.101133
360.788733	18820.897223	29.106151
360.617756	18843.031179	29.111168
361.248341	18869.393549	29.116186
361.855468	18889.354024	29.121204
362.090422	18914.445687	29.126221
362.581550	18929.406008	29.131239
362.548283	18951.664712	29.136256
362.765498	18973.696048	29.141274
363.261205	18999.654463	29.146292
363.343843	19037.947047	29.151309
363.708318	19061.648182	29.156327
363.747217	19090.962928	29.161344
364.180623	19126.143154	29.166362
364.910448	19137.612980	29.171380
365.254934	19161.826949	29.176397
366.034173	19195.781308	29.181415
365.868456	19222.908224	29.186432
366.281776	19241.778154	29.191450
367.013828	19267.660213	29.196468
366.971776	19303.228172	29.201485
367.477018	19322.604325	29.206503
367.271591	19357.218114	29.211520
367.648467	19382.639332	29.216538
367.934510	19421.440312	29.221556
368.191669	19446.527384	29.226573
368.694505	19485.565705	29.231591
368.704793	19515.961409	29.236608
369.186138	19554.582590	29.241626
369.758418	19586.717408	29.246644
369.667298	19639.469719	29.251661
370.140877	19670.166293	29.256679
370.610432	19719.131642	29.261696
370.917848	19746.373825	29.266714
371.216475	19785.491985	29.271732
371.771034	19829.436936	29.276749
372.433149	19868.295901	29.281767
373.007164	19905.344175	29.286784
372.939797	19942.600207	29.291802
374.001619	19971.805820	29.296820
374.018057	20011.619334	29.301837
374.597672	20041.152103	29.306855
374.731883	20071.767234	29.311872
375.436990	20102.346076	29.316890
375.116702	20139.332108	29.321908
375.204162	20174.173304	29.326925
375.906224	20202.324613	29.331943
376.144007	20259.669255	29.336960
376.586897	20297.505600	29.341978
377.916790	20325.043369	29.346996
378.605854	20349.688793	29.352013
379.182464	20367.467663	29.357031
379.692312	20385.527626	29.362048
379.885077	20413.577354	29.367066
380.563939	20433.196239	29.372084
380.807364	20454.463419	29.377101
381.447543	20472.972603	29.382119
381.301621	20492.021766	29.387136
380.799116	20513.812633	29.392154
381.571253	20544.070156	29.397172
381.586455	20573.590206	29.402189
382.218608	20602.663985	29.407207
382.746004	20642.987450	29.412224
382.984934	20667.708904	29.417242
383.246202	20697.655315	29.422260
383.472704	20743.768653	29.427277
384.154144	20779.199948	29.432295
384.256663	20814.131333	29.437312
384.715270	20851.567282	29.442330
385.156646	20884.687295	29.447348
385.269911	20919.509829	29.452365
385.616464	20949.145621	29.457383
386.084386	20978.238728	29.462400
386.689304	21009.851872	29.467418
387.903826	21037.295468	29.472436
388.411272	21065.601408	29.477453
388.786996	21071.864958	29.482471
388.920794	21097.360370	29.487488
388.938656	21119.649424	29.492506
389.097525	21140.786883	29.497524
389.037395	21181.163430	29.502541
389.633218	21194.548297	29.507559
390.226641	21213.973007	29.512576
391.002039	21234.072993	29.517594
391.614692	21267.927609	29.522612
391.788520	21292.344176	29.527629
392.299869	21323.401532	29.532647
392.515611	21338.280305	29.537664
392.605384	21368.992117	29.542682
393.142059	21389.385501	29.547700
393.157226	21435.935884	29.552717
393.492084	21465.541466	29.557735
393.981295	21501.325746	29.562752
394.045028	21536.744637	29.567770
394.305930	21560.549020	29.572788
394.328466	21619.154080	29.577805
394.840764	21656.153679	29.582823
395.762000	21699.690561	29.587840
396.035552	21733.796601	29.592858
396.969829	21764.149938	29.597876
397.018441	21811.272766	29.602893
397.467885	21842.630257	29.607911
398.004492	21879.003287	29.612928
398.431575	21915.420395	29.617946
398.860203	21948.055812	29.622964
398.733662	21985.760112	29.627981
399.581848	22029.195239	29.632999
399.442959	22062.388600	29.638016
399.865164	22115.809665	29.643034
400.400403	22148.023493	29.648052
400.418764	22193.421057	29.653069
400.980916	22236.426333	29.658087
401.543507	22278.769314	29.663104
401.880019	22325.273355	29.668122
402.534393	22371.726205	29.673140
402.520354	22415.609702	29.678157
403.135258	22458.931356	29.683175
403.674505	22495.658492	29.688192
403.942829	22544.593919	29.693210
404.232395	22577.680158	29.698228
404.323081	22626.400249	29.703245
404.926362	22674.692000	29.708263
405.222740	22710.912420	29.713280
406.421530	22749.268094	29.718298
407.100607	22775.935754	29.723316
407.448812	22815.793577	29.728333
407.652918	22848.333565	29.733351
408.207033	22887.058659	29.738368
408.522658	22924.235064	29.743386
408.752985	22943.473225	29.748404
409.924840	22965.183705	29.753421
410.283098	22985.655310	29.758439
411.463322	22996.463927	29.763456
411.774387	23026.144104	29.768474
411.630722	23036.933603	29.773492
412.051700	23061.195218	29.778509
412.102522	23079.675773	29.783527
412.672681	23101.322372	29.788544
413.062971	23133.648059	29.793562
413.393173	23152.594933	29.798580
413.453421	23189.787291	29.803597
413.744543	23228.069338	29.808615
414.071353	23260.488148	29.813632
414.140453	23293.556776	29.818650
414.654836	23331.337137	29.823668
414.302148	23367.499849	29.828685
415.098868	23414.404255	29.833703
415.713629	23457.375194	29.838720
415.663839	23505.459478	29.843738
416.329023	23549.393490	29.848756
416.910343	23591.629264	29.853773
417.485326	23643.309877	29.858791
418.018979	23687.944935	29.863808
417.987734	23734.676682	29.868826
418.670776	23774.630752	29.873844
418.848687	23816.933057	29.878861
419.412927	23860.557123	29.883879
419.968624	23913.604481	29.888896
420.279614	23950.793364	29.893914
421.076671	23989.384685	29.898932
421.734028	24023.748087	29.903949
421.928964	24052.913712	29.908967
422.562532	24096.419250	29.913984
422.795980	24145.075017	29.919002
423.596227	24180.133422	29.924020
423.612036	24223.161600	29.929037
424.052640	24259.698078	29.934055
424.406906	24300.520367	29.939072
424.730615	24350.003444	29.944090
425.159185	24383.315375	29.949108
426.044592	24416.694184	29.954125
426.193169	24459.409999	29.959143
426.717635	24489.980353	29.964160
427.517844	24533.455284	29.969178
427.848225	24557.463262	29.974196
427.941642	24596.624443	29.979213
428.293391	24637.750780	29.984231
429.065048	24670.360980	29.989248
429.411875	24715.103264	29.994266
430.117826	24743.163617	29.999284
430.672127	24782.047512	30.004301
430.949494	24812.389503	30.009319
431.471560	24842.134437	30.014336
431.467647	24881.732480	30.019354
431.884707	24909.766904	30.024372
432.186393	24946.672473	30.029389
432.739151	24977.172599	30.034407
433.133684	24998.981019	30.039424
433.651514	25030.029787	30.044442
433.978879	25069.517863	30.049460
434.321350	25089.644533	30.054477
434.797339	25132.678129	30.059495
435.649883	25164.512022	30.064512
435.879990	25193.433805	30.069530
436.714115	25213.299717	30.074548
437.333704	25235.946815	30.079565
437.598984	25268.443034	30.084583
438.278456	25291.666679	30.089600
438.472476	25325.455941	30.094618
438.805133	25350.534006	30.099636
439.049520	25383.614450	30.104653
439.055368	25419.956594	30.109671
439.592608	25450.617941	30.114688
439.876280	25494.978748	30.119706
440.083838	25530.684043	30.124724
440.341534	25579.803405	30.129741
440.553951	25637.782345	30.134759
440.926224	25680.850849	30.139776
441.148053	25739.147125	30.144794
441.737876	25787.699119	30.149812
442.698533	25828.137186	30.154829
442.952039	25875.444211	30.159847
443.448465	25918.148177	30.164864
443.540037	25982.067016	30.169882
444.093077	26035.745952	30.174900
444.596940	26078.240831	30.179917
445.007361	26129.521736	30.184935
445.692544	26174.414855	30.189952
445.989921	26238.554895	30.194970
446.391256	26279.900609	30.199988
447.258949	26330.523289	30.205005
447.505954	26368.949189	30.210023
448.038575	26414.982677	30.215040
448.368625	26475.919130	30.220058
449.122703	26520.731933	30.225076
449.671634	26556.317740	30.230093
450.692120	26587.876250	30.235111
451.601996	26610.182012	30.240128
452.352373	26639.960313	30.245146
452.642055	26670.284512	30.250164
453.175091	26693.768582	30.255181
453.054359	26727.267479	30.260199
453.846139	26752.473952	30.265216
453.879497	26795.035433	30.270234
454.317490	26831.331707	30.275252
454.874952	26860.745942	30.280269
454.916130	26905.237075	30.285287
455.367336	26931.770392	30.290304
455.882217	26980.691893	30.295322
455.910322	27013.913451	30.300340
456.327072	27045.399579	30.305357
456.398420	27088.873315	30.310375
457.278190	27125.444682	30.315392
457.633067	27162.733884	30.320410
457.842855	27213.680087	30.325428
458.542967	27249.493791	30.330445
458.941901	27294.205389	30.335463
459.811978	27328.983733	30.340480
460.407937	27367.383584	30.345498
460.684219	27406.819465	30.350516
461.326471	27434.838305	30.355533
461.263538	27474.953978	30.360551
461.966379	27514.023601	30.365568
462.203364	27551.967968	30.370586
462.700395	27599.935171	30.375604
463.532488	27631.417436	30.380621
463.765189	27679.061026	30.385639
464.026716	27713.146220	30.390656
464.995722	27752.189696	30.395674
465.104477	27805.641025	30.400692
465.741206	27843.817245	30.405709
465.901120	27890.085701	30.410727
466.435207	27921.815163	30.415744
466.933933	27979.730732	30.420762
466.973807	28027.326280	30.425780
467.918950	28064.743415	30.430797
467.754041	28124.792377	30.435815
468.155912	28173.421077	30.440832
468.798389	28223.412666	30.445850
468.919878	28277.601523	30.450868
470.093482	28323.107426	30.455885
469.887611	28379.050102	30.460903
470.876067	28429.850633	30.465920
471.319795	28480.599520	30.470938
472.094351	28535.242021	30.475956
472.445294	28577.740785	30.480973
473.012725	28623.389200	30.485991
474.050541	28651.821781	30.491008
475.321683	28679.851589	30.496026
475.982446	28703.783431	30.501044
477.092760	28728.862456	30.506061
477.325012	28754.306525	30.511079
477.522532	28763.804294	30.516096
478.062507	28787.312076	30.521114
478.247980	28810.255919	30.526132
478.963926	28825.577597	30.531149
479.204476	28854.636168	30.536167
479.345837	28890.265012	30.541184
479.944730	28916.157623	30.546202
479.955614	28955.935889	30.551220
480.359213	28990.778540	30.556237
480.580057	29027.268020	30.561255
480.849630	29062.023346	30.566272
481.563364	29114.519934	30.571290
481.799662	29154.032847	30.576308
481.942059	29179.925189	30.581325
482.476126	29230.992055	30.586343
482.375961	29268.392100	30.591360
483.047357	29319.836403	30.596378
483.360985	29380.457615	30.601396
483.660054	29414.911990	30.606413
484.220646	29471.944715	30.611431
484.516425	29533.497152	30.616448
485.296692	29580.704983	30.621466
485.719897	29640.819246	30.626484
486.228969	29686.997882	30.631501
486.535852	29743.749963	30.636519
486.672373	29810.757760	30.641536
487.542889	29865.605661	30.646554
487.565796	29936.678517	30.651572
488.045225	29991.890424	30.656589
488.791706	30052.982488	30.661607
489.001722	30117.593407	30.666624
489.964256	30169.873798	30.671642
490.315108	30235.966128	30.676660
490.927697	30288.918978	30.681677
491.652571	30356.973430	30.686695
492.084386	30426.662378	30.691712
492.477715	30469.101632	30.696730
493.282956	30534.451419	30.701748
493.779005	30586.459564	30.706765
494.441995	30645.267657	30.711783
495.135939	30696.115718	30.716800
495.525801	30744.141394	30.721818
495.578341	30798.362409	30.726836
496.076378	30846.729551	30.731853
496.818956	30907.222528	30.736871
497.048830	30975.414657	30.741888
498.020227	31030.523407	30.746906
497.944400	31081.510782	30.751924
498.718342	31142.889046	30.756941
499.030725	31199.199904	30.761959
500.260175	31249.033211	30.766976
501.378514	31285.518709	30.771994
501.856038	31335.187633	30.777012
502.708068	31371.059424	30.782029
502.997229	31405.039713	30.787047
503.628434	31446.525420	30.792064
503.972777	31486.315330	30.797082
504.543197	31524.561363	30.802100
504.993342	31562.528305	30.807117
505.182129	31595.563694	30.812135
505.087434	31641.005162	30.817152
505.825173	31688.222736	30.822170
506.025236	31745.198315	30.827188
506.367804	31795.216676	30.832205
507.006558	31859.738365	30.837223
507.643321	31917.346535	30.842240
508.975711	31940.467120	30.847258
510.022793	31961.616983	30.852276
510.427764	31982.640218	30.857293
510.812282	32009.975217	30.862311
511.100360	32034.723330	30.867328
511.891202	32059.855530	30.872346
511.791920	32090.927856	30.877364
512.404024	32130.960492	30.882381
513.048913	32167.314339	30.887399
513.051116	32207.435872	30.892416
513.705165	32246.420189	30.897434
513.963945	32289.284459	30.902452
514.222096	32342.878498	30.907469
514.699558	32388.214358	30.912487
515.040958	32446.281937	30.917504
515.547464	32492.487233	30.922522
516.049421	32543.502850	30.927540
516.410760	32595.883921	30.932557
516.698501	32656.091537	30.937575
516.926225	32718.616544	30.942592
517.683938	32777.159817	30.947610
518.543941	32840.179672	30.952628
519.427469	32894.324618	30.957645
519.634560	32952.700876	30.962663
520.063297	33005.380869	30.967680
520.254347	33065.145667	30.972698
520.459162	33132.580278	30.977716
520.653099	33199.190159	30.982733
521.814489	33257.198756	30.987751
522.148080	33332.732222	30.992768
522.527668	33396.909364	30.997786
523.483984	33466.930570	31.002804
523.682050	33531.776797	31.007821
524.276029	33589.886848	31.012839
524.572285	33664.462374	31.017856
525.192189	33741.311881	31.022874
525.506770	33813.126539	31.027892
525.906923	33886.864619	31.032909
526.379347	33946.779802	31.037927
526.661572	34022.268149	31.042944
527.686202	34092.033909	31.047962
528.289804	34176.614100	31.052980
528.984801	34242.119411	31.057997
529.546135	34306.770466	31.063015
530.299306	34382.066004	31.068032
531.507378	34443.015079	31.073050
531.932857	34499.881860	31.078068
532.411669	34545.819436	31.083085
533.889150	34585.011760	31.088103
534.370366	34633.085857	31.093120
535.273707	34665.840337	31.098138
535.794957	34698.941243	31.103156
536.185228	34741.855100	31.108173
536.976465	34782.121758	31.113191
537.367101	34823.845867	31.118208
538.501776	34848.948319	31.123226
538.844458	34881.916035	31.128244
538.956806	34909.024332	31.133261
539.745784	34942.155561	31.138279
540.190674	34966.438971	31.143296
540.002672	35000.488882	31.148314
540.510777	35037.982963	31.153332
540.904134	35082.970741	31.158349
541.212432	35121.240943	31.163367
541.575441	35181.440935	31.168384
542.213409	35226.535501	31.173402
542.250280	35292.835978	31.178420
542.394326	35349.015080	31.183437
543.015662	35409.537694	31.188455
543.246236	35479.829933	31.193472
543.498716	35541.293637	31.198490
543.845204	35621.082846	31.203508
544.414746	35693.574606	31.208525
545.218195	35763.564622	31.213543
545.893655	35848.768421	31.218560
546.311855	35911.915733	31.223578
547.379699	35988.363451	31.228596
547.576699	36058.325942	31.233613
548.458696	36125.775616	31.238631
548.650674	36198.539245	31.243648
549.376336	36255.467411	31.248666
550.299170	36333.349195	31.253684
550.404944	36393.272154	31.258701
551.273304	36455.842344	31.263719
551.857461	36542.378121	31.268736
552.546837	36595.080719	31.273754
553.083371	36664.176137	31.278772
553.346522	36740.193557	31.283789
554.494981	36793.070590	31.288807
554.786009	36862.038368	31.293824
555.925371	36910.760137	31.298842
556.848207	36975.873269	31.303860
557.549650	37025.633129	31.308877
558.199966	37056.525558	31.313895
558.806035	37119.758497	31.318912
559.528056	37164.240555	31.323930
560.478446	37204.627362	31.328948
559.874402	37253.715046	31.333965
560.867674	37307.276734	31.338983
561.435475	37364.708900	31.344000
561.988475	37416.357667	31.349018
562.545479	37478.293404	31.354036
562.171149	37524.119514	31.359053
563.239913	37585.150355	31.364071
563.279467	37652.289135	31.369088
563.540750	37715.857836	31.374106
564.299325	37787.943559	31.379124
564.831737	37859.500107	31.384141
565.073791	37923.754672	31.389159
565.294328	37999.771987	31.394176
565.760874	38069.339265	31.399194
566.490685	38146.551570	31.404212
566.383545	38222.594380	31.409229
566.974069	38292.598992	31.414247
567.672876	38382.649942	31.419264
568.148746	38450.525017	31.424282
568.736812	38522.020939	31.429300
569.314773	38612.355733	31.434317
570.183250	38691.178650	31.439335
570.704093	38770.358212	31.444352
571.673027	38843.987307	31.449370
572.245525	38914.483530	31.454388
572.809529	38990.477650	31.459405
573.749800	39050.645126	31.464423
574.393893	39120.163851	31.469440
575.631663	39174.134221	31.474458
576.534034	39230.031127	31.479476
576.847315	39289.236600	31.484493
577.285716	39340.904088	31.489511
577.701744	39405.310794	31.494528
578.342037	39464.659691	31.499546
579.025309	39524.623342	31.504564
579.408464	39591.230440	31.509581
580.507948	39647.173762	31.514599
580.691265	39709.083153	31.519616
581.687516	39744.141782	31.524634
582.908380	39790.224267	31.529652
583.652318	39839.100486	31.534669
584.893011	39873.356632	31.539687
585.519139	39907.879145	31.544704
585.916755	39941.298016	31.549722
586.320594	39981.241553	31.554740
586.569105	40026.389403	31.559757
587.015944	40066.676193	31.564775
587.410342	40119.486789	31.569792
587.442967	40164.356252	31.574810
588.199852	40218.257368	31.579828
588.294970	40283.634514	31.584845
589.006295	40354.144006	31.589863
589.253824	40406.077637	31.594880
589.536618	40481.055780	31.599898
590.024623	40547.001126	31.604916
590.280759	40623.733483	31.609933
590.678853	40701.900459	31.614951
591.512092	40778.578779	31.619968
592.192174	40858.052540	31.624986
593.032804	40936.450932	31.630004
593.480535	41014.534940	31.635021
594.398276	41074.633920	31.640039
595.035175	41143.798375	31.645056
595.933497	41210.244079	31.650074
596.634649	41263.513687	31.655092
597.517167	41330.751851	31.660109
598.556632	41376.007416	31.665127
599.340486	41426.724843	31.670144
599.899817	41475.397039	31.675162
601.029255	41521.120613	31.680180
601.267187	41571.111058	31.685197
601.594384	41599.771068	31.690215
602.000484	41650.380170	31.695232
602.286129	41705.604013	31.700250
602.723465	41745.605586	31.705268
602.817812	41801.907578	31.710285
603.892375	41855.045436	31.715303
604.567387	41921.598238	31.720320
604.470689	41977.870341	31.725338
605.076174	42039.137335	31.730356
605.346821	42117.976185	31.735373
606.193367	42182.467136	31.740391
607.319996	42257.686731	31.745408
607.427601	42321.805883	31.750426
608.128505	42385.870968	31.755444
608.389201	42455.985667	31.760461
608.807013	42525.113827	31.765479
609.702745	42597.447337	31.770496
610.032316	42677.696166	31.775514
611.101832	42750.900389	31.780532
611.218860	42829.850640	31.785549
611.929156	42902.962279	31.790567
612.794750	42984.506754	31.795584
613.212054	43071.180539	31.800602
613.633647	43151.999779	31.805620
614.216828	43238.775377	31.810637
614.584918	43319.206638	31.815655
615.345494	43385.431045	31.820672
615.835931	43486.543614	31.825690
616.552162	43559.353647	31.830708
617.108418	43652.226920	31.835725
618.109971	43732.507207	31.840743
618.699303	43810.632267	31.845760
619.357982	43887.198480	31.850778
620.866289	43952.321035	31.855796
621.627519	44027.060859	31.860813
622.230068	44095.844195	31.865831
623.430430	44146.835496	31.870848
624.355153	44210.568454	31.875866
625.022850	44257.710395	31.880884
625.437138	44318.859674	31.885901
626.020267	44365.132186	31.890919
626.590902	44421.758287	31.895936
627.155479	44488.689600	31.900954
627.556690	44541.517793	31.905972
627.666922	44611.868375	31.910989
628.063104	44673.119791	31.916007
628.749455	44748.791073	31.921024
629.187230	44831.057862	31.926042
629.725688	44901.977206	31.931060
629.988560	44982.086188	31.936077
630.454783	45062.710148	31.941095
631.105349	45146.833446	31.946112
631.683766	45227.299933	31.951130
632.502607	45311.211968	31.956148
632.984582	45385.461816	31.961165
633.999407	45454.687880	31.966183
634.608459	45533.176666	31.971200
635.723396	45602.041893	31.976218
636.818970	45654.469998	31.981236
637.372967	45709.343767	31.986253
637.997518	45761.963395	31.991271
639.036441	45815.573284	31.996288
639.246632	45886.520953	32.001306
640.104918	45928.609913	32.006324
640.996491	45991.236571	32.011341
641.515007	46053.703122	32.016359
642.181753	46111.296797	32.021376
642.936612	46171.149390	32.026394
643.655209	46224.846891	32.031412
644.023682	46278.588734	32.036429
644.329286	46349.963915	32.041447
644.807312	46404.833749	32.046464
645.253208	46476.791733	32.051482
645.804920	46537.258219	32.056500
646.315419	46622.561594	32.061517
646.843793	46700.352090	32.066535
647.552813	46774.922161	32.071552
647.768013	46865.965146	32.076570
648.375460	46937.666632	32.081588
649.028267	47030.779873	32.086605
649.623394	47117.305826	32.091623
650.314578	47197.107525	32.096640
650.362120	47297.839300	32.101658
651.008645	47380.194996	32.106676
651.523831	47488.257049	32.111693
651.866522	47589.672517	32.116711
652.720325	47685.410660	32.121728
652.993649	47795.540379	32.126746
653.983935	47893.479672	32.131764
654.817423	47994.674220	32.136781
655.522733	48100.183561	32.141799
656.338132	48199.127163	32.146816
656.792957	48298.669982	32.151834
657.574502	48389.733687	32.156852
658.190451	48488.469736	32.161869
659.052862	48593.032575	32.166887
659.826785	48678.900044	32.171904
660.892450	48781.148626	32.176922
661.672395	48865.525061	32.181940
663.189435	48955.871624	32.186957
663.582276	49034.680229	32.191975
664.235078	49113.545695	32.196992
664.634848	49199.902822	32.202010
665.399629	49269.349726	32.207028
666.480022	49346.291936	32.212045
666.772191	49435.050151	32.217063
667.456014	49514.253064	32.222080
667.785395	49612.797556	32.227098
668.332387	49680.779713	32.232116
669.129478	49762.573307	32.237133
669.335969	49855.719756	32.242151
669.634867	49925.709989	32.247168
670.163446	50020.078170	32.252186
670.873394	50111.692890	32.257204
671.479353	50203.995515	32.262221
671.573864	50309.457247	32.267239
672.513106	50400.705530	32.272256
673.421898	50495.269896	32.277274
673.539010	50600.577704	32.282292
674.876130	50700.395480	32.287309
675.317163	50800.392547	32.292327
676.339990	50897.049444	32.297344
677.197899	51001.291155	32.302362
677.986897	51089.321045	32.307380
678.641326	51179.130746	32.312397
679.695078	51269.308386	32.317415
681.067952	51353.290763	32.322432
681.948014	51440.769610	32.327450
682.585481	51515.559708	32.332468
683.392884	51583.845045	32.337485
684.026033	51664.063599	32.342503
684.425001	51744.259416	32.347520
685.631700	51822.371227	32.352538
685.900289	51892.455817	32.357556
686.329487	51975.225176	32.362573
686.700335	52053.841227	32.367591
687.630611	52143.172132	32.372608
688.173049	52229.714060	32.377626
688.250521	52313.612867	32.382644
689.200738	52410.283338	32.387661
689.366984	52512.800310	32.392679
690.091548	52616.416330	32.397696
690.997400	52717.998922	32.402714
691.623438	52813.772833	32.407732
692.407534	52910.625854	32.412749
692.811524	53020.870058	32.417767
694.007854	53111.341318	32.422784
695.045302	53212.581667	32.427802
695.514554	53301.522903	32.432820
696.573143	53390.881703	32.437837
697.148654	53483.672514	32.442855
698.092079	53562.480816	32.447872
698.800677	53643.585415	32.452890
699.973984	53733.633798	32.457908
700.631555	53813.932725	32.462925
701.302754	53899.979681	32.467943
702.542701	53957.912257	32.472960
703.731763	54031.751729	32.477978
704.180392	54104.410325	32.482996
704.952348	54170.258991	32.488013
705.390691	54246.957590	32.493031
706.239497	54304.351575	32.498048
706.599807	54384.893298	32.503066
706.672147	54451.481991	32.508084
707.583742	54528.707219	32.513101
707.734996	54612.426178	32.518119
708.424829	54687.453102	32.523136
709.094395	54755.570798	32.528154
710.254956	54842.182536	32.533172
711.104803	54909.991840	32.538189
711.600164	54988.250646	32.543207
712.371622	55064.054888	32.548224
712.689097	55151.039876	32.553242
712.918047	55227.752838	32.558260
714.098543	55320.865638	32.563277
714.107049	55406.925193	32.568295
715.156801	55504.889117	32.573312
715.822309	55596.928682	32.578330
716.483087	55693.892207	32.583348
717.571670	55784.710050	32.588365
717.742364	55876.778788	32.593383
718.508146	55956.416906	32.598400
718.917185	56053.829733	32.603418
719.551564	56159.122684	32.608436
720.864107	56258.422911	32.613453
721.437523	56368.169987	32.618471
722.111180	56458.493200	32.623488
722.829756	56555.855433	32.628506
723.310969	56667.484205	32.633524
724.290533	56769.517184	32.638541
724.580964	56882.355276	32.643559
724.864874	56978.921897	32.648576
725.670606	57091.230507	32.653594
726.401726	57221.601776	32.658612
727.003156	57325.680428	32.663629
728.009170	57454.426158	32.668647
728.953517	57561.967437	32.673664
729.695423	57663.666451	32.678682
730.685199	57780.857932	32.683700
731.187957	57876.089435	32.688717
732.199161	57996.451119	32.693735
733.445797	58108.158964	32.698752
733.591955	58203.819653	32.703770
734.195578	58314.248361	32.708788
735.399363	58410.272382	32.713805
736.024896	58521.052389	32.718823
736.523177	58622.854821	32.723840
737.232839	58733.747978	32.728858
738.276719	58849.033962	32.733876
739.007463	58949.660557	32.738893
739.823657	59057.465558	32.743911
740.447845	59149.212353	32.748928
741.776569	59255.634931	32.753946
742.121071	59356.013672	32.758964
742.944670	59461.209198	32.763981
743.868264	59569.763283	32.768999
744.945765	59655.278536	32.774016
745.710336	59742.655428	32.779034
746.621905	59828.130302	32.784052
747.512226	59913.552287	32.789069
748.314442	59994.622164	32.794087
749.212001	60074.386618	32.799104
749.984433	60145.791597	32.804122
750.659081	60219.722893	32.809140
752.132958	60287.291642	32.814157
752.705475	60363.920938	32.819175
753.356381	60431.232925	32.824192
754.098159	60502.492699	32.829210
754.708284	60578.402104	32.834228
755.681020	60638.763643	32.839245
756.573288	60712.084240	32.844263
757.084915	60779.086220	32.849280
758.117575	60844.968863	32.854298
758.843443	60923.356468	32.859316
759.130672	60986.756715	32.864333
759.901729	61076.287293	32.869351
760.462835	61159.014913	32.874368
761.340076	61233.477721	32.879386
761.959422	61313.756077	32.884404
762.637996	61396.180080	32.889421
763.077143	61493.506301	32.894439
763.791252	61582.201803	32.899456
764.296664	61673.341790	32.904474
764.491627	61774.800941	32.909492
765.603540	61861.994596	32.914509
767.134128	61967.429511	32.919527
767.521303	62057.093308	32.924544
768.705850	62138.270489	32.929562
769.310173	62237.664261	32.934580
770.220535	62327.422928	32.939597
770.464780	62433.914974	32.944615
771.267153	62523.111418	32.949632
772.109981	62626.132610	32.954650
772.437040	62724.242380	32.959668
773.312579	62829.073235	32.964685
774.140400	62927.483799	32.969703
774.380289	63032.803851	32.974720
775.247611	63137.100332	32.979738
776.075072	63252.606078	32.984756
776.625531	63362.552600	32.989773
777.822739	63477.458918	32.994791
778.470107	63577.818934	32.999808
779.452031	63682.585285	33.004826
779.889439	63795.063184	33.009844
780.823646	63903.764648	33.014861
781.869970	64022.372786	33.019879
782.112367	64126.161705	33.024896
783.223311	64237.085220	33.029914
783.340394	64361.405091	33.034932
784.523873	64479.214720	33.039949
785.038291	64588.680739	33.044967
785.382135	64703.379600	33.049984
786.434982	64818.254782	33.055002
786.977046	64940.178750	33.060020
788.238159	65050.840601	33.065037
789.371820	65146.914267	33.070055
789.535608	65261.318254	33.075072
790.859890	65362.019736	33.080090
791.155799	65472.159999	33.085108
791.936633	65577.621447	33.090125
792.690712	65690.801279	33.095143
793.299082	65808.451317	33.100160
794.479583	65922.141009	33.105178
795.059079	66051.525449	33.110196
795.999290	66154.161622	33.115213
796.933590	66277.960812	33.120231
797.469143	66393.837298	33.125248
798.307595	66503.390514	33.130266
799.176558	66629.649795	33.135284
800.079698	66747.235587	33.140301
800.893897	66871.001904	33.145319
801.393986	66994.481315	33.150336
802.202234	67109.537297	33.155354
802.979728	67235.398537	33.160372
803.501638	67359.540222	33.165389
804.217490	67494.366712	33.170407
804.974512	67621.081003	33.175424
806.253572	67741.137066	33.180442
807.158738	67868.560915	33.185460
808.262056	67986.176163	33.190477
809.481446	68107.420592	33.195495
810.246547	68217.279722	33.200512
811.345743	68336.838799	33.205530
812.079811	68450.384509	33.210548
812.671622	68561.059156	33.215565
813.978292	68670.119648	33.220583
814.393885	68781.780426	33.225600
815.640116	68903.448420	33.230618
816.108803	69016.789648	33.235636
816.516605	69128.624290	33.240653
817.925026	69250.696460	33.245671
818.706218	69352.376148	33.250688
819.800783	69463.551085	33.255706
820.734350	69579.452537	33.260724
821.550478	69687.463978	33.265741
822.547155	69790.044706	33.270759
823.591886	69890.790171	33.275776
824.512953	69990.905954	33.280794
825.183518	70087.334149	33.285812
826.364221	70192.496939	33.290829
827.658314	70286.346664	33.295847
828.418543	70389.596785	33.300864
829.191796	70474.405048	33.305882
829.726441	70572.009608	33.310900
830.109844	70673.346272	33.315917
830.795598	70774.334402	33.320935
831.441702	70882.336659	33.325952
831.888935	70969.175749	33.330970
832.833081	71092.362313	33.335988
833.429296	71190.389133	33.341005
834.317633	71293.381297	33.346023
834.572298	71409.800906	33.351040
835.196357	71512.535816	33.356058
836.280641	71627.423198	33.361076
837.088394	71741.504790	33.366093
837.791029	71862.725998	33.371111
838.328260	71983.356436	33.376128
839.217589	72101.669479	33.381146
839.899349	72221.618755	33.386164
841.183933	72346.183376	33.391181
841.646716	72473.254765	33.396199
842.268050	72612.518448	33.401216
843.738755	72729.211129	33.406234
844.155432	72853.813444	33.411252
845.140307	72991.037707	33.416269
846.524091	73102.257597	33.421287
847.458699	73213.377894	33.426304
848.306314	73328.415926	33.431322
849.775348	73447.484433	33.436340
850.711833	73564.222450	33.441357
851.354522	73664.282593	33.446375
852.060123	73780.150541	33.451392
853.436018	73883.020770	33.456410
854.237399	73990.758763	33.461428
855.137666	74090.390910	33.466445
856.340959	74202.539067	33.471463
857.333551	74313.737199	33.476480
858.069070	74410.008869	33.481498
859.392991	74507.236444	33.486516
860.099673	74615.259344	33.491533
861.132830	74714.011343	33.496551
861.422545	74823.415943	33.501568
862.421789	74918.480848	33.506586
863.103913	75030.089949	33.511604
863.692727	75149.229825	33.516621
864.632276	75251.656162	33.521639
865.086895	75375.235180	33.526656
865.798389	75487.651168	33.531674
866.603815	75605.820255	33.536692
867.143773	75719.670994	33.541709
868.447574	75843.644817	33.546727
868.595605	75982.498405	33.551744
869.241659	76112.026168	33.556762
870.419067	76244.208910	33.561780
870.838629	76368.337084	33.566797
871.998189	76513.447386	33.571815
873.041404	76655.219693	33.576832
873.132533	76788.515217	33.581850
873.981500	76930.309877	33.586868
874.601710	77071.246367	33.591885
875.582783	77210.597442	33.596903
876.264994	77379.023051	33.601920
877.042195	77517.961816	33.606938
877.988671	77653.785445	33.611956
878.579657	77798.476370	33.616973
880.024751	77939.555349	33.621991
880.760414	78084.925503	33.627008
881.712856	78223.389451	33.632026
882.654864	78359.363582	33.637044
883.426594	78493.311725	33.642061
884.523153	78624.408894	33.647079
886.468825	78732.055961	33.652096
888.188984	78848.706319	33.657114
889.311725	78964.757387	33.662132
890.651382	79074.281201	33.667149
892.251196	79169.432046	33.672167
893.243191	79249.118447	33.677184
894.085027	79344.950225	33.682202
894.820848	79439.750395	33.687220
895.577893	79537.735801	33.692237
896.609010	79636.642625	33.697255
896.884336	79739.778823	33.702272
897.531422	79839.903702	33.707290
898.527163	79949.142670	33.712308
899.114616	80060.040033	33.717325
899.483922	80167.280606	33.722343
900.614302	80293.807521	33.727360
901.134378	80420.787618	33.732378
902.161306	80535.736954	33.737396
902.924861	80664.473461	33.742413
903.738656	80785.363318	33.747431
904.684942	80918.353121	33.752448
905.435192	81032.251476	33.757466
906.870774	81149.968287	33.762484
907.565591	81269.160177	33.767501
908.973445	81401.770039	33.772519
909.591835	81521.115511	33.777536
910.267655	81636.661938	33.782554
911.371491	81751.559889	33.787572
912.238801	81897.216448	33.792589
912.707393	82010.541497	33.797607
913.635806	82160.978809	33.802624
914.484354	82285.685797	33.807642
915.302914	82408.285328	33.812660
915.903480	82552.992005	33.817677
916.984296	82690.701695	33.822695
917.808333	82830.487224	33.827712
918.400470	82971.755927	33.832730
919.888806	83108.360627	33.837748
920.569579	83239.125075	33.842765
921.570835	83371.562749	33.847783
922.608992	83527.861933	33.852800
923.172622	83670.101519	33.857818
924.528742	83799.943535	33.862836
925.095622	83947.954943	33.867853
925.830826	84094.362889	33.872871
926.615061	84240.390024	33.877888
927.678228	84388.490067	33.882906
928.651816	84523.318203	33.887924
929.242319	84662.553548	33.892941
930.121197	84787.388932	33.897959
930.671683	84939.630024	33.902976
931.677345	85084.371573	33.907994
932.645227	85224.912432	33.913012
933.431500	85376.261698	33.918029
934.194325	85522.496619	33.923047
935.691597	85677.927831	33.928064
936.519409	85831.190284	33.933082
937.472385	85968.498155	33.938100
938.106618	86120.738841	33.943117
939.171834	86266.743057	33.948135
940.573309	86417.892376	33.953152
941.121182	86573.352829	33.958170
942.740168	86721.207779	33.963188
943.785993	86862.979025	33.968205
944.982749	86995.397257	33.973223
945.660451	87139.910091	33.978240
946.611763	87299.748732	33.983258
947.663099	87439.718857	33.988276
948.221236	87594.291890	33.993293
949.338878	87725.000030	33.998311
950.098922	87878.306250	34.003328
951.122810	88038.612044	34.008346
952.127104	88183.062590	34.013364
952.911674	88344.221479	34.018381
953.938189	88496.960733	34.023399
954.603509	88657.085236	34.028416
955.664694	88816.965803	34.033434
956.804541	88977.422547	34.038452
957.619127	89139.619554	34.043469
958.236544	89304.864006	34.048487
958.896210	89468.684651	34.053504
959.298184	89641.645391	34.058522
960.094305	89819.147458	34.063540
961.085375	90002.971909	34.068557
961.988001	90188.483806	34.073575
962.855566	90375.547461	34.078592
963.914003	90565.554637	34.083610
965.279766	90741.794969	34.088628
966.409394	90920.741686	34.093645
967.364630	91096.535871	34.098663
968.494568	91268.649291	34.103680
969.700890	91450.346407	34.108698
970.728100	91620.289874	34.113716
971.377962	91789.292728	34.118733
972.505120	91962.171049	34.123751
973.778337	92143.038984	34.128768
974.995568	92318.676800	34.133786
976.463591	92481.106945	34.138804
977.268118	92643.930294	34.143821
978.309485	92804.315136	34.148839
979.346971	92960.466968	34.153856
980.483573	93117.438368	34.158874
981.339266	93269.344229	34.163892
982.360852	93424.267362	34.168909
983.061091	93573.473462	34.173927
984.076211	93726.279013	34.178944
984.788012	93883.372317	34.183962
985.972558	94026.826389	34.188980
986.544035	94184.926805	34.193997
987.565668	94348.793978	34.199015
989.027606	94497.444726	34.204032
989.977693	94659.205536	34.209050
991.100271	94799.458849	34.214068
992.284174	94947.938327	34.219085
993.553279	95100.575870	34.224103
994.706393	95245.669259	34.229120
995.496118	95409.336205	34.234138
996.735422	95535.564173	34.239156
997.968925	95674.132118	34.244173
999.778597	95810.785271	34.249191
1001.238504	95938.857692	34.254208
1002.230520	96079.317779	34.259226
1003.130872	96199.510652	34.264244
1003.960144	96328.199501	34.269261
1004.733735	96462.862157	34.274279
1005.443978	96594.985051	34.279296
1005.814639	96727.970803	34.284314
1007.055537	96861.270393	34.289332
1008.062804	97021.276611	34.294349
1008.694230	97169.452282	34.299367
1009.920160	97317.951194	34.304384
1010.473343	97474.182432	34.309402
1011.032152	97626.190826	34.314420
1012.626015	97776.655364	34.319437
1013.694714	97927.546270	34.324455
1014.984704	98083.648747	34.329472
1015.683622	98247.995375	34.334490
1016.572976	98400.084734	34.339508
1017.221720	98564.593937	34.344525
1018.388917	98737.246197	34.349543
1019.429533	98895.586984	34.354560
1020.053658	99062.857760	34.359578
1021.279898	99225.011983	34.364596
1022.300109	99396.858090	34.369613
1023.101590	99578.626386	34.374631
1024.236633	99737.576680	34.379648
1024.858012	99920.574899	34.384666
1025.820610	100094.151395	34.389684
1026.690365	100272.373459	34.394701
1027.418989	100454.413658	34.399719
1028.867181	100630.975188	34.404736
1029.717526	100815.966710	34.409754
1031.251627	101001.893565	34.414772
1032.366840	101177.319093	34.419789
1033.346824	101351.394911	34.424807
1034.579237	101522.528588	34.429824
1035.348465	101700.821978	34.434842
1036.531119	101864.418562	34.439860
1036.900470	102032.157364	34.444877
1037.616934	102213.452064	34.449895
1038.810772	102374.922296	34.454912
1039.833076	102548.606230	34.459930
1041.239368	102735.941412	34.464948
1042.128312	102906.813657	34.469965
1042.743406	103084.344953	34.474983
1044.175941	103270.906889	34.480000
1044.917891	103459.944088	34.485018
1045.938879	103635.446505	34.490036
1046.856648	103826.393978	34.495053
1047.289606	104004.760543	34.500071
1048.909686	104196.945613	34.505088
1049.665722	104392.129754	34.510106
1050.808081	104590.225585	34.515124
1052.157291	104789.364052	34.520141
1053.178006	104987.825639	34.525159
1054.416495	105175.928743	34.530176
1055.531779	105377.036855	34.535194
1056.540189	105564.916103	34.540212
1057.721953	105745.433302	34.545229
1058.706039	105938.233782	34.550247
1060.370216	106113.553707	34.555264
1061.131823	106308.231545	34.560282
1062.923276	106502.265793	34.565300
1064.247309	106680.586272	34.570317
1065.625820	106861.520595	34.575335
1066.746558	107038.054246	34.580352
1068.050271	107206.450963	34.585370
1068.495673	107376.401714	34.590388
1069.972189	107551.889776	34.595405
1070.631501	107734.169095	34.600423
1071.719030	107909.700736	34.605440
1072.796080	108078.610351	34.610458
1073.879974	108265.342718	34.615476
1075.129291	108439.672009	34.620493
1076.900400	108606.084584	34.625511
1077.828728	108778.317528	34.630528
1078.796560	108942.804881	34.635546
1079.752446	109119.494246	34.640564
1080.881259	109280.776471	34.645581
1081.900012	109474.837532	34.650599
1083.300963	109640.027637	34.655616
1084.100063	109809.844259	34.660634
1085.164250	109983.302950	34.665652
1086.183154	110150.968465	34.670669
1086.822352	110341.325491	34.675687
1087.561405	110517.807571	34.680704
1088.306887	110706.666711	34.685722
1089.498921	110900.809453	34.690740
1090.348834	111092.351724	34.695757
1091.247890	111307.298622	34.700775
1091.945912	111504.051220	34.705792
1093.279720	111704.053595	34.710810
1094.425043	111888.202803	34.715828
1095.592486	112074.832565	34.720845
1096.470455	112258.738595	34.725863
1097.970186	112446.910248	34.730880
1098.945981	112634.514065	34.735898
1100.295921	112823.157308	34.740916
1101.327030	112998.705509	34.745933
1102.232885	113195.535726	34.750951
1103.156483	113390.501840	34.755968
1104.205120	113579.328417	34.760986
1105.689245	113783.500835	34.766004
1106.922802	113974.553607	34.771021
1107.695359	114169.107487	34.776039
1108.932482	114361.657306	34.781056
1110.156756	114560.342977	34.786074
1111.074187	114750.213403	34.791092
1112.296395	114950.688646	34.796109
1113.130661	115154.766759	34.801127
1114.091833	115361.586765	34.806144
1115.389300	115569.465694	34.811162
1116.009396	115773.293447	34.816180
1116.847829	115983.395304	34.821197
1118.016714	116214.754520	34.826215
1119.117614	116432.645312	34.831232
1120.060145	116664.756457	34.836250
1120.828769	116895.822186	34.841268
1122.198788	117118.803886	34.846285
1123.591011	117355.734674	34.851303
1125.232106	117568.992485	34.856320
1126.140155	117785.532580	34.861338
1127.121537	118005.698489	34.866356
1128.465361	118209.064622	34.871373
1129.776557	118446.803780	34.876391
1130.988330	118666.263598	34.881408
1132.632308	118880.987748	34.886426
1133.916893	119104.049895	34.891444
1134.975270	119309.221265	34.896461
1136.207195	119526.162265	34.901479
1137.374830	119735.284319	34.906496
1139.005499	119933.721703	34.911514
1139.867788	120155.584158	34.916532
1141.070361	120350.422572	34.921549
1142.545750	120578.887056	34.926567
1143.729073	120773.604806	34.931584
1144.461645	120975.523182	34.936602
1145.769176	121182.717842	34.941620
1146.664851	121397.132078	34.946637
1147.573486	121609.898111	34.951655
1148.402441	121831.994157	34.956672
1149.508502	122049.215840	34.961690
1150.314776	122268.252026	34.966708
1151.850049	122491.550045	34.971725
1153.263397	122708.926642	34.976743
1154.219991	122927.941867	34.981760
1155.791698	123139.173018	34.986778
1156.604642	123352.322564	34.991796
1157.927518	123547.934189	34.996813
1158.618735	123763.376097	35.001831
1159.754988	123972.900533	35.006848
1161.111830	124183.960248	35.011866
1162.122031	124397.450867	35.016884
1162.815704	124601.542028	35.021901
1163.452080	124828.319085	35.026919
1164.670768	125059.168070	35.031936
1165.095431	125281.155669	35.036954
1166.579082	125523.293963	35.041972
1168.141998	125745.913889	35.046989
1169.112837	125994.683916	35.052007
1169.938511	126241.579519	35.057024
1171.578070	126479.097513	35.062042
1172.426112	126721.810271	35.067060
1173.810013	126961.822042	35.072077
1175.019726	127214.769137	35.077095
1176.473761	127459.234489	35.082112
1177.990111	127691.142131	35.087130
1179.107282	127929.026741	35.092148
1180.888355	128153.172908	35.097165
1181.844701	128390.188538	35.102183
1182.896651	128631.017749	35.107200
1184.576685	128852.460811	35.112218
1185.539517	129090.165073	35.117236
1186.732682	129324.066801	35.122253
1188.020098	129561.085191	35.127271
1189.047766	129799.873816	35.132288
1190.726699	130036.828705	35.137306
1191.170042	130265.389378	35.142324
1192.622606	130499.293315	35.147341
1193.673836	130747.047460	35.152359
1194.828707	131003.127237	35.157376
1195.901674	131236.759228	35.162394
1196.814929	131494.304091	35.167412
1197.769901	131739.141197	35.172429
1198.954421	132004.338785	35.177447
1199.625812	132259.357597	35.182464
1201.251156	132513.061426	35.187482
1202.248584	132787.197077	35.192500
1203.266865	133049.883384	35.197517
1204.318082	133316.027222	35.202535
1205.497980	133592.902137	35.207552
1207.187925	133861.679484	35.212570
1208.392198	134129.540580	35.217588
1209.593466	134397.886130	35.222605
1210.617745	134666.796640	35.227623
1212.289650	134938.958262	35.232640
1213.579142	135197.925722	35.237658
1214.357285	135479.614260	35.242676
1215.377445	135743.272460	35.247693
1217.146396	136003.951782	35.252711
1218.041000	136275.369796	35.257728
1220.007280	136540.634657	35.262746
1221.024724	136786.221037	35.267764
1222.513380	137026.390537	35.272781
1224.392357	137267.800897	35.277799
1225.274829	137508.280444	35.282816
1226.939422	137742.643033	35.287834
1227.589099	137982.316239	35.292852
1228.676858	138220.191679	35.297869
1230.290755	138463.342275	35.302887
1231.216138	138706.384218	35.307904
1232.928514	138940.138174	35.312922
1233.878464	139180.770049	35.317940
1235.498404	139415.392613	35.322957
1237.365399	139639.766846	35.327975
1238.802150	139867.804726	35.332992
1240.635484	140090.146094	35.338010
1241.432663	140313.072032	35.343028
1242.392667	140542.742963	35.348045
1243.805953	140765.984781	35.353063
1244.838491	140995.861837	35.358080
1246.125810	141228.423166	35.363098
1247.208738	141470.151298	35.368116
1248.151626	141713.781849	35.373133
1249.358102	141951.307384	35.378151
1250.231700	142201.953131	35.383168
1251.370476	142448.814271	35.388186
1251.777277	142708.331630	35.393204
1253.123759	142969.123024	35.398221
1254.109371	143235.938433	35.403239
1255.340668	143501.191971	35.408256
1256.921832	143761.378283	35.413274
1258.075939	144035.221841	35.418292
1259.887912	144294.877902	35.423309
1261.577762	144543.700912	35.428327
1262.765195	144805.522034	35.433344
1264.475823	145048.511175	35.438362
1265.923138	145306.042873	35.443380
1267.469956	145556.076749	35.448397
1268.781796	145805.581846	35.453415
1269.833763	146056.972096	35.458432
1271.399370	146306.170823	35.463450
1272.017702	146554.125605	35.468468
1273.722120	146789.187962	35.473485
1275.061479	147039.013773	35.478503
1276.114527	147296.867872	35.483520
1277.440685	147545.849593	35.488538
1278.967364	147810.842842	35.493556
1280.050283	148065.906853	35.498573
1281.362352	148308.719333	35.503591
1282.288737	148563.458391	35.508608
1283.095166	148835.963921	35.513626
1284.434875	149102.330060	35.518644
1285.033364	149365.654035	35.523661
1286.480846	149634.948087	35.528679
1287.424614	149910.963930	35.533696
1288.724516	150181.352555	35.538714
1290.367791	150447.003908	35.543732
1291.844060	150680.442655	35.548749
1293.619651	150927.657361	35.553767
1294.991343	151177.847493	35.558784
1296.527833	151425.347324	35.563802
1297.591492	151678.751836	35.568820
1298.978778	151927.751817	35.573837
1300.030027	152175.199970	35.578855
1301.095566	152435.167037	35.583872
1302.530360	152682.058053	35.588890
1303.970079	152934.746761	35.593908
1305.430920	153192.063484	35.598925
1306.860019	153440.495129	35.603943
1308.227225	153699.974968	35.608960
1309.351936	153938.821179	35.613978
1310.914367	154196.177805	35.618996
1311.692557	154452.668195	35.624013
1313.315866	154703.370567	35.629031
1314.449209	154970.941301	35.634048
1315.797877	155231.373038	35.639066
1317.172993	155497.878375	35.644084
1318.006053	155769.387648	35.649101
1319.511877	156034.136213	35.654119
1319.903550	156318.930691	35.659136
1321.496415	156601.314195	35.664154
1322.701691	156886.848726	35.669172
1323.712671	157168.511167	35.674189
1325.075868	157455.659163	35.679207
1325.798236	157763.990923	35.684224
1327.422913	158062.173610	35.689242
1329.126084	158356.272630	35.694260
1329.898295	158651.116676	35.699277
1331.148801	158954.748977	35.704295
1332.538283	159262.749348	35.709312
1333.859652	159564.432871	35.714330
1335.266294	159880.161188	35.719348
1336.137315	160189.234009	35.724365
1338.088160	160501.296068	35.729383
1339.634929	160820.191924	35.734400
1340.997948	161114.901391	35.739418
1342.458532	161423.184489	35.744436
1344.355236	161724.125185	35.749453
1346.237314	162015.110686	35.754471
1347.758315	162308.722885	35.759488
1349.320683	162586.292587	35.764506
1350.896444	162878.186428	35.769524
1352.533682	163164.514369	35.774541
1354.306599	163431.712730	35.779559
1355.227413	163712.152745	35.784576
1356.442858	163991.630575	35.789594
1357.905517	164278.452469	35.794612
1359.165649	164572.873182	35.799629
1360.456543	164836.508334	35.804647
1361.745518	165117.807852	35.809664
1362.692014	165395.437307	35.814682
1364.258172	165665.273070	35.819700
1365.107046	165935.804225	35.824717
1366.677738	166204.348203	35.829735
1367.230975	166490.185312	35.834752
1368.727380	166776.446496	35.839770
1370.230955	167061.464730	35.844788
1371.319550	167355.387452	35.849805
1372.448922	167636.755404	35.854823
1373.548780	167932.710197	35.859840
1374.902717	168228.737616	35.864858
1376.442003	168522.273449	35.869876
1377.429507	168834.115155	35.874893
1378.825834	169135.597656	35.879911
1379.925025	169457.170101	35.884928
1381.480686	169759.619170	35.889946
1383.018503	170064.814271	35.894964
1384.212641	170379.993764	35.899981
1386.018241	170688.065775	35.904999
1387.616398	171011.657317	35.910016
1389.316289	171310.284587	35.915034
1391.022658	171613.265405	35.920052
1392.155556	171922.996075	35.925069
1394.289398	172210.729762	35.930087
1395.947247	172515.412413	35.935104
1397.700069	172810.156633	35.940122
1398.959432	173085.189557	35.945140
1400.258752	173382.375338	35.950157
1402.069423	173663.484897	35.955175
1403.945615	173938.988145	35.960192
1405.644311	174224.282711	35.965210
1407.750812	174488.632281	35.970228
1409.042726	174750.711357	35.975245
1410.693306	175014.088391	35.980263
1412.070724	175280.902143	35.985280
1413.432231	175536.412040	35.990298
1415.213704	175787.675885	35.995316
1416.468144	176064.617224	36.000333
1418.158970	176314.071632	36.005351
1419.479232	176570.824911	36.010368
1420.903758	176832.638316	36.015386
1422.147041	177091.349221	36.020404
1423.239117	177361.306876	36.025421
1424.525351	177621.485356	36.030439
1425.926263	177887.788425	36.035456
1426.666737	178156.934678	36.040474
1428.269036	178429.945525	36.045492
1429.439840	178710.278867	36.050509
1430.817449	178987.709880	36.055527
1432.134410	179262.512746	36.060544
1433.379119	179543.688278	36.065562
1434.762137	179840.034457	36.070580
1435.841601	180141.016230	36.075597
1437.084331	180438.354384	36.080615
1438.356918	180733.823266	36.085632
1439.238057	181035.135947	36.090650
1440.573925	181328.109496	36.095668
1442.339450	181623.613132	36.100685
1443.847367	181912.206753	36.105703
1445.229348	182205.545241	36.110720
1446.541237	182493.858161	36.115738
1447.883060	182787.320873	36.120756
1448.674809	183086.870465	36.125773
1450.373344	183394.148996	36.130791
1451.330594	183702.152674	36.135808
1452.925710	184013.438021	36.140826
1454.805205	184314.305875	36.145844
1456.126460	184632.927566	36.150861
1457.662457	184940.382018	36.155879
1458.685274	185268.959364	36.160896
1460.060721	185604.434424	36.165914
1461.794569	185924.960265	36.170932
1462.704265	186251.645834	36.175949
1464.472448	186569.440194	36.180967
1465.944656	186900.945715	36.185984
1467.976376	187233.119012	36.191002
1470.009187	187563.034442	36.196020
1471.484131	187899.305450	36.201037
1472.711037	188272.662836	36.206055
1473.786865	188595.346997	36.211072
1475.426627	188928.307762	36.216090
1476.834164	189263.912491	36.221108
1477.940681	189609.485083	36.226125
1479.496873	189940.218778	36.231143
1480.738274	190280.300687	36.236160
1482.167692	190635.649557	36.241178
1483.801152	190981.571336	36.246196
1485.146047	191322.948853	36.251213
1487.140388	191671.821420	36.256231
1488.306022	192017.727446	36.261248
1489.759984	192363.433686	36.266266
1491.454562	192704.949294	36.271284
1492.862449	193060.785316	36.276301
1494.507219	193406.807338	36.281319
1495.908072	193757.024370	36.286336
1497.613455	194112.307472	36.291354
1499.175024	194454.286764	36.296372
1500.796465	194812.952371	36.301389
1502.301630	195161.203950	36.306407
1504.257364	195503.794112	36.311424
1505.783264	195847.487955	36.316442
1507.714112	196174.647671	36.321460
1509.481048	196516.488175	36.326477
1511.433431	196844.790090	36.331495
1513.305668	197160.131897	36.336512
1514.860604	197491.539301	36.341530
1516.584892	197801.627774	36.346548
1518.152038	198115.959687	36.351565
1519.550951	198430.816966	36.356583
1520.600155	198749.658686	36.361600
1522.209109	199059.607433	36.366618
1523.879321	199356.101471	36.371636
1524.923129	199668.980907	36.376653
1526.244490	199981.674554	36.381671
1527.846218	200282.793021	36.386688
1529.264718	200583.436229	36.391706
1530.583896	200896.032631	36.396724
1531.904692	201210.750462	36.401741
1533.384181	201524.833036	36.406759
1534.766594	201835.568870	36.411776
1536.228168	202164.664985	36.416794
1537.847396	202486.968051	36.421812
1539.290354	202814.927471	36.426829
1540.816158	203146.759463	36.431847
1542.406865	203469.820727	36.436864
1543.818244	203804.938338	36.441882
1545.185355	204134.579743	36.446900
1546.682180	204472.999624	36.451917
1548.102547	204822.061794	36.456935
1549.860444	205160.770105	36.461952
1551.344378	205503.920090	36.466970
1552.962878	205840.648945	36.471988
1554.304084	206185.603942	36.477005
1555.591692	206527.763394	36.482023
1556.894058	206882.416340	36.487040
1558.307123	207251.248020	36.492058
1560.040526	207619.074195	36.497076
1561.601825	207994.156562	36.502093
1562.236570	208362.973981	36.507111
1563.944088	208741.869450	36.512128
1565.343784	209136.310942	36.517146
1566.680255	209510.117887	36.522164
1568.079456	209905.756614	36.527181
1569.428138	210306.307306	36.532199
1571.642819	210698.381547	36.537216
1572.991692	211095.227878	36.542234
1574.963074	211495.880566	36.547252
1576.291060	211894.181620	36.552269
1577.674827	212297.427301	36.557287
1579.375359	212690.461675	36.562304
1580.991572	213099.258465	36.567322
1583.129653	213492.449932	36.572340
1585.117688	213889.376747	36.577357
1586.963457	214273.402175	36.582375
1589.306660	214657.064648	36.587392
1590.975194	215032.208825	36.592410
1592.820747	215401.914397	36.597428
1594.681604	215776.215773	36.602445
1596.163206	216162.418960	36.607463
1597.746479	216518.534775	36.612480
1599.423164	216889.544645	36.617498
1601.186384	217252.845346	36.622516
1602.463322	217631.520401	36.627533
1603.946700	218003.786469	36.632551
1605.925987	218370.279704	36.637568
1607.136230	218731.013285	36.642586
1608.913388	219081.770939	36.647604
1611.621355	219415.886587	36.652621
1613.709437	219746.401073	36.657639
1615.444410	220052.974881	36.662656
1617.341986	220368.208205	36.667674
1619.341118	220682.155080	36.672692
1620.842052	220991.057422	36.677709
1622.127454	221316.202237	36.682727
1623.534623	221627.814664	36.687744
1624.874916	221960.343116	36.692762
1625.980537	222287.197769	36.697780
1627.140158	222620.343183	36.702797
1628.280684	222964.567045	36.707815
1629.776253	223318.814837	36.712832
1630.429831	223683.012047	36.717850
1631.887394	224052.203548	36.722868
1633.059652	224426.143947	36.727885
1634.221044	224825.360357	36.732903
1635.901825	225207.318660	36.737920
1637.346729	225612.762831	36.742938
1638.252320	226017.106716	36.747956
1640.323183	226418.585418	36.752973
1641.454664	226839.377968	36.757991
1643.444377	227260.202776	36.763008
1645.115316	227684.233076	36.768026
1646.798420	228111.767865	36.773044
1648.653700	228533.508509	36.778061
1649.927146	228969.472782	36.783079
1651.485576	229381.334946	36.788096
1653.108914	229827.529236	36.793114
1654.826330	230265.275597	36.798132
1656.649861	230703.614671	36.803149
1657.766932	231149.848600	36.808167
1659.900452	231587.908475	36.813184
1661.268053	232047.285271	36.818202
1663.308039	232494.000018	36.823220
1664.923125	232937.461056	36.828237
1666.502536	233397.440328	36.833255
1668.051899	233831.236919	36.838272
1670.589246	234295.906338	36.843290
1672.061914	234733.122042	36.848308
1674.205738	235163.644891	36.853325
1676.147963	235598.496117	36.858343
1678.290709	236039.943906	36.863360
1680.105230	236477.511537	36.868378
1681.902771	236896.133141	36.873396
1683.655967	237324.517564	36.878413
1685.526256	237758.801514	36.883431
1687.130825	238184.698290	36.888448
1688.964080	238607.533904	36.893466
1690.859842	239024.313885	36.898484
1692.988835	239439.073339	36.903501
1694.885480	239852.095111	36.908519
1696.787717	240244.896347	36.913536
1698.677898	240654.389650	36.918554
1700.532539	241025.354185	36.923572
1702.758964	241388.025241	36.928589
1704.782448	241747.886430	36.933607
1706.889696	242091.374526	36.938624
1708.450023	242456.980646	36.943642
1710.097239	242818.253925	36.948660
1711.251504	243158.832626	36.953677
1713.263542	243523.702327	36.958695
1714.909078	243881.954252	36.963712
1716.697726	244231.494366	36.968730
1718.320791	244598.184635	36.973748
1719.481254	244959.746876	36.978765
1720.985114	245334.434800	36.983783
1722.699226	245703.142885	36.988800
1724.211507	246084.739709	36.993818
1725.795493	246463.225495	36.998836
1727.434144	246839.314416	37.003853
1729.409945	247243.848085	37.008871
1731.040945	247621.259964	37.013888
1732.675142	248009.112235	37.018906
1734.463501	248399.224723	37.023924
1736.425596	248787.453379	37.028941
1737.944967	249176.697980	37.033959
1739.835916	249562.678509	37.038976
1741.391182	249949.504222	37.043994
1742.604373	250356.126897	37.049012
1744.152816	250749.381253	37.054029
1745.953384	251172.238135	37.059047
1747.507082	251575.348458	37.064064
1749.614272	251991.142076	37.069082
1751.294972	252405.586280	37.074100
1753.611651	252810.294069	37.079117
1754.918446	253220.509443	37.084135
1756.745610	253636.783511	37.089152
1758.580969	254049.880909	37.094170
1760.202876	254469.518152	37.099188
1762.278875	254889.814503	37.104205
1763.498222	255306.777242	37.109223
1765.602649	255725.011210	37.114240
1767.384875	256147.085418	37.119258
1768.664294	256578.797272	37.124276
1770.335062	257007.266783	37.129293
1771.683263	257453.827738	37.134311
1773.462040	257886.012996	37.139328
1775.086502	258325.058060	37.144346
1776.583628	258780.789327	37.149364
1778.063991	259242.645524	37.154381
1779.723425	259708.408449	37.159399
1781.198357	260160.459662	37.164416
1782.910061	260632.843534	37.169434
1784.405106	261107.448925	37.174452
1786.589377	261578.481346	37.179469
1788.300386	262062.600857	37.184487
1789.720542	262547.074654	37.189504
1791.613571	263017.444723	37.194522
1792.968051	263491.005751	37.199540
1794.346144	263951.022546	37.204557
1796.002603	264430.805704	37.209575
1797.769346	264912.474788	37.214592
1799.261251	265384.664306	37.219610
1800.679022	265884.809273	37.224628
1803.207384	266376.075903	37.229645
1804.894387	266875.487794	37.234663
1806.627648	267360.411527	37.239680
1808.315766	267853.598286	37.244698
1810.774315	268348.837231	37.249716
1812.769170	268838.693207	37.254733
1814.580024	269326.065078	37.259751
1816.858338	269817.750915	37.264768
1818.711720	270304.656762	37.269786
1820.488712	270798.382782	37.274804
1822.544866	271284.261628	37.279821
1824.527532	271774.343615	37.284839
1826.053084	272267.170167	37.289856
1828.110784	272763.029264	37.294874
1829.804783	273269.923426	37.299892
1831.429489	273759.300811	37.304909
1833.318826	274262.145927	37.309927
1835.109392	274757.970445	37.314944
1837.500305	275254.123022	37.319962
1839.052296	275767.945417	37.324980
1841.416710	276262.423689	37.329997
1843.110217	276761.511697	37.335015
1845.230749	277263.776883	37.340032
1847.472622	277755.605293	37.345050
1849.606607	278246.714261	37.350068
1851.607001	278736.777938	37.355085
1853.368945	279225.839640	37.360103
1855.093642	279716.836914	37.365120
1857.093947	280204.813713	37.370138
1858.766133	280709.762612	37.375156
1860.864141	281193.757274	37.380173
1862.845673	281688.489791	37.385191
1864.041223	282180.256307	37.390208
1865.997030	282679.054389	37.395226
1868.062272	283178.924415	37.400244
1870.515254	283654.671802	37.405261
1872.382205	284146.596685	37.410279
1874.794302	284638.426698	37.415296
1876.847714	285113.348742	37.420314
1878.453880	285605.414930	37.425332
1880.272837	286076.893984	37.430349
1882.404358	286560.129182	37.435367
1884.373952	287048.445039	37.440384
1886.229620	287527.609120	37.445402
1888.160334	288003.888414	37.450420
1890.200477	288478.928050	37.455437
1892.293066	288945.498768	37.460455
1894.285593	289433.217584	37.465472
1896.660540	289881.931218	37.470490
1898.281577	290331.940552	37.475508
1900.175472	290765.747403	37.480525
1901.898390	291207.887569	37.485543
1903.398127	291650.978635	37.490560
1905.630579	292087.923061	37.495578
1906.965221	292534.493302	37.500596
1908.766149	292990.455912	37.505613
1910.597194	293438.563229	37.510631
1912.319079	293915.438974	37.515648
1914.425846	294362.555625	37.520666
1916.436322	294825.738876	37.525684
1918.564762	295280.924795	37.530701
1920.611381	295737.037095	37.535719
1921.869395	296203.111452	37.540736
1924.084569	296671.839206	37.545754
1925.610060	297151.527769	37.550772
1927.229611	297626.372346	37.555789
1928.785411	298103.435183	37.560807
1930.783851	298604.725658	37.565824
1932.805078	299086.326500	37.570842
1934.506393	299575.471913	37.575860
1936.734499	300061.604018	37.580877
1939.110349	300561.575234	37.585895
1941.182813	301060.376593	37.590912
1943.153600	301541.592549	37.595930
1944.898419	302048.114447	37.600948
1946.708127	302541.390729	37.605965
1948.114320	303041.361790	37.610983
1950.097095	303549.104283	37.616000
1952.092984	304057.552671	37.621018
1953.781085	304581.313749	37.626036
1955.276996	305103.504537	37.631053
1957.834961	305619.364677	37.636071
1959.705580	306150.525759	37.641088
1961.302699	306668.626149	37.646106
1963.151571	307202.171323	37.651124
1965.063839	307744.717400	37.656141
1967.452219	308282.531095	37.661159
1969.442663	308828.230781	37.666176
1971.499893	309351.771161	37.671194
1973.492879	309894.517174	37.676212
1975.324763	310432.385815	37.681229
1977.345188	310966.790206	37.686247
1979.114372	311521.878986	37.691264
1981.033941	312058.552886	37.696282
1983.067634	312610.337887	37.701300
1985.053640	313164.158337	37.706317
1987.128321	313725.729670	37.711335
1988.117212	314286.745897	37.716352
1990.078570	314847.464411	37.721370
1991.948221	315418.046419	37.726388
1993.690874	315996.085402	37.731405
1995.688380	316580.754062	37.736423
1997.360906	317169.383629	37.741440
1999.758577	317737.951625	37.746458
2001.258195	318302.148699	37.751476
2003.152718	318862.617101	37.756493
2005.221022	319425.463144	37.761511
2007.299618	320003.410058	37.766528
2009.570810	320550.951780	37.771546
2011.597354	321129.989247	37.776564
2013.628794	321710.874060	37.781581
2015.382126	322276.567155	37.786599
2017.630775	322855.474557	37.791616
2019.682702	323430.525595	37.796634
2021.358273	324021.884629	37.801652
2023.508679	324613.359803	37.806669
2025.385508	325203.784229	37.811687
2027.211870	325792.992793	37.816704
2029.071643	326386.937343	37.821722
2030.965698	326986.886929	37.826740
2032.203875	327605.323090	37.831757
2034.227450	328220.521044	37.836775
2035.925058	328854.808381	37.841792
2037.970954	329496.772000	37.846810
2039.476400	330149.152971	37.851828
2041.624633	330795.729864	37.856845
2044.040091	331446.746762	37.861863
2045.605789	332106.709991	37.866880
2048.042055	332766.186291	37.871898
2049.960638	333422.011427	37.876916
2051.902072	334091.303787	37.881933
2054.279190	334755.233217	37.886951
2056.295627	335425.282654	37.891968
2058.958669	336095.111320	37.896986
2061.111381	336764.663154	37.902004
2062.885605	337417.695846	37.907021
2065.342144	338088.751995	37.912039
2067.500485	338770.967587	37.917056
2069.267502	339434.407343	37.922074
2071.602031	340107.513036	37.927092
2073.499383	340782.283238	37.932109
2075.773568	341449.365352	37.937127
2077.973862	342136.882174	37.942144
2080.107250	342816.608827	37.947162
2082.362505	343483.741888	37.952180
2084.604434	344164.166576	37.957197
2087.221977	344832.817358	37.962215
2089.119616	345507.824735	37.967232
2091.279916	346170.189629	37.972250
2093.884062	346823.409069	37.977268
2096.125933	347487.060456	37.982285
2098.624644	348136.726027	37.987303
2100.857379	348782.621084	37.992320
2103.576117	349429.819319	37.997338
2105.945740	350079.782963	38.002356
2107.637332	350726.249516	38.007373
2110.165104	351356.475479	38.012391
2112.546666	352001.307828	38.017408
2114.379646	352615.267251	38.022426
2117.035129	353212.076420	38.027444
2119.167320	353814.777250	38.032461
2121.568040	354400.068017	38.037479
2123.713341	354986.409171	38.042496
2125.684194	355566.986860	38.047514
2127.927536	356151.518626	38.052532
2129.322979	356743.925521	38.057549
2131.855395	357334.530973	38.062567
2133.880507	357933.916922	38.067584
2135.506173	358528.516392	38.072602
2137.957425	359117.308219	38.077620
2139.561193	359724.122237	38.082637
2141.777204	360329.528398	38.087655
2143.818705	360939.597677	38.092672
2145.858925	361542.427480	38.097690
2147.876195	362153.369816	38.102708
2150.013143	362774.200999	38.107725
2151.788944	363392.217334	38.112743
2153.891429	364028.939677	38.117760
2155.752774	364663.764679	38.122778
2158.258943	365294.384732	38.127796
2159.556959	365949.932699	38.132813
2161.532531	366592.315349	38.137831
2163.490233	367264.088187	38.142848
2165.220021	367934.619507	38.147866
2167.206791	368614.403290	38.152884
2169.063410	369302.338400	38.157901
2171.491122	369993.764365	38.162919
2173.352996	370700.060282	38.167936
2175.500757	371398.228144	38.172954
2177.448141	372112.673439	38.177972
2179.515208	372825.054901	38.182989
2181.393632	373544.504428	38.188007
2183.391352	374269.929075	38.193024
2185.465561	375012.925060	38.198042
2187.476413	375756.600530	38.203060
2189.778028	376506.017221	38.208077
2192.131211	377246.178249	38.213095
2194.713557	377984.889208	38.218112
2196.799420	378729.450158	38.223130
2199.124245	379472.609744	38.228148
2201.351148	380235.952580	38.233165
2203.730169	380978.409780	38.238183
2205.587942	381739.574876	38.243200
2207.693717	382507.677465	38.248218
2210.076317	383262.378606	38.253236
2212.672396	384021.943967	38.258253
2215.340199	384763.276139	38.263271
2218.148657	385515.544196	38.268288
2220.203956	386272.334165	38.273306
2222.862451	387005.807169	38.278324
2225.443444	387745.360131	38.283341
2227.527101	388467.134671	38.288359
2230.412130	389196.892219	38.293376
2232.721775	389908.074660	38.298394
2235.332112	390618.352657	38.303412
2237.446697	391313.262577	38.308429
2239.874066	391989.600269	38.313447
2241.637813	392681.370329	38.318464
2243.402903	393379.891291	38.323482
2246.247444	394059.253621	38.328500
2247.927375	394759.099926	38.333517
2249.938799	395450.915128	38.338535
2251.831776	396162.045374	38.343552
2254.019287	396874.349675	38.348570
2256.633524	397578.048794	38.353588
2258.720936	398299.914155	38.358605
2260.881675	399011.486049	38.363623
2263.087488	399736.462461	38.368640
2264.796950	400459.300742	38.373658
2266.867493	401189.432235	38.378676
2269.140271	401933.141806	38.383693
2271.056296	402673.776154	38.388711
2273.477499	403411.416099	38.393728
2275.292625	404176.071669	38.398746
2277.639244	404931.899972	38.403764
2279.924678	405711.481278	38.408781
2282.335072	406483.241573	38.413799
2284.585132	407253.360684	38.418816
2286.662605	408035.367984	38.423834
2289.063280	408804.707637	38.428852
2291.121968	409585.963562	38.433869
2293.359985	410376.183219	38.438887
2296.201982	411166.782561	38.443904
2298.498298	411969.583590	38.448922
2301.228384	412756.050954	38.453940
2302.912908	413536.594879	38.458957
2305.757799	414326.034208	38.463975
2308.239323	415117.132247	38.468992
2310.530038	415921.128532	38.474010
2313.131550	416699.900089	38.479028
2315.603656	417488.140544	38.484045
2318.021757	418282.113680	38.489063
2320.367558	419070.807270	38.494080
2322.584236	419863.498643	38.499098
2324.881897	420654.277250	38.504116
2326.971036	421454.611371	38.509133
2329.131625	422255.970607	38.514151
2331.526939	423063.137050	38.519168
2333.515233	423872.523532	38.524186
2335.714325	424682.808952	38.529204
2338.477721	425498.894293	38.534221
2340.515738	426312.038261	38.539239
2343.207363	427118.866520	38.544256
2345.534549	427937.271927	38.549274
2348.449511	428738.286440	38.554292
2351.045992	429546.718717	38.559309
2353.351250	430356.742071	38.564327
2356.042591	431154.826968	38.569344
2358.256081	431946.639230	38.574362
2360.687736	432711.713814	38.579380
2363.277924	433476.229744	38.584397
2365.895690	434231.453805	38.589415
2368.307857	434991.900670	38.594432
2370.258043	435750.326169	38.599450
2372.820742	436512.518120	38.604468
2374.932590	437270.561265	38.609485
2377.398303	438028.265287	38.614503
2379.854736	438786.805375	38.619520
2381.905093	439559.404667	38.624538
2384.583903	440321.092553	38.629556
2387.342280	441099.942665	38.634573
2389.217409	441870.720085	38.639591
2391.630199	442643.351468	38.644608
2393.697473	443427.245272	38.649626
2396.211329	444197.325218	38.654644
2398.604272	444990.819439	38.659661
2400.751389	445779.723263	38.664679
2403.316117	446562.102731	38.669696
2405.600499	447372.573216	38.674714
2407.569477	448161.115822	38.679732
2410.005478	448972.055505	38.684749
2412.633971	449802.402021	38.689767
2415.006266	450608.990541	38.694784
2416.993876	451434.223402	38.699802
2419.370569	452250.810956	38.704820
2421.538712	453095.466047	38.709837
2423.579941	453931.562864	38.714855
2426.129006	454781.645526	38.719872
2428.047334	455642.721473	38.724890
2430.535820	456498.456040	38.729908
2432.630358	457373.685558	38.734925
2434.880937	458252.389082	38.739943
2436.912999	459134.983858	38.744960
2439.095412	460028.381868	38.749978
2441.541730	460919.470550	38.754996
2444.314415	461822.290616	38.760013
2446.819603	462730.725128	38.765031
2449.445481	463624.389929	38.770048
2451.959905	464533.092899	38.775066
2454.299788	465443.097090	38.780084
2456.779084	466355.864438	38.785101
2459.167607	467270.322038	38.790119
2461.593695	468183.567451	38.795136
2463.933771	469111.234020	38.800154
2466.347121	470036.619767	38.805172
2468.790561	470962.712888	38.810189
2471.321975	471906.275017	38.815207
2474.584805	472831.580247	38.820224
2477.257964	473767.042869	38.825242
2480.229424	474689.729388	38.830260
2482.848523	475612.379584	38.835277
2485.365950	476535.051433	38.840295
2487.971989	477435.794153	38.845312
2490.487377	478345.648421	38.850330
2493.174452	479225.482823	38.855348
2495.683028	480092.277255	38.860365
2497.986146	480968.204305	38.865383
2500.329302	481837.720041	38.870400
2502.411980	482713.246074	38.875418
2504.699028	483588.239800	38.880436
2507.708330	484459.886542	38.885453
2509.700556	485353.723974	38.890471
2512.195808	486246.874815	38.895488
2514.225270	487149.145279	38.900506
2516.777272	488044.062283	38.905524
2519.128171	488946.184802	38.910541
2521.322603	489869.483291	38.915559
2524.023411	490793.251418	38.920576
2526.147015	491723.880860	38.925594
2528.735981	492650.293007	38.930612
2531.117394	493588.143827	38.935629
2533.812995	494526.444132	38.940647
2536.236169	495467.211000	38.945664
2538.586737	496423.778296	38.950682
2541.174181	497383.226794	38.955700
2543.655033	498331.591615	38.960717
2546.196836	499306.473295	38.965735
2549.108708	500263.077395	38.970752
2551.479449	501232.780665	38.975770
2554.068419	502213.685743	38.980788
2556.440531	503188.921249	38.985805
2558.874978	504171.701761	38.990823
2561.017583	505156.590311	38.995840
2563.571557	506159.498960	39.000858
2566.047949	507154.090369	39.005876
2568.775007	508159.466111	39.010893
2571.186073	509183.886857	39.015911
2573.884792	510189.844993	39.020928
2576.475249	511214.003158	39.025946
2578.880780	512228.701859	39.030964
2581.621834	513261.016766	39.035981
2584.128409	514293.857881	39.040999
2586.451425	515332.355747	39.046016
2588.755315	516381.720892	39.051034
2590.890306	517424.090906	39.056052
2593.591613	518480.349009	39.061069
2595.767806	519546.950790	39.066087
2598.433069	520619.187065	39.071104
2600.918784	521696.666883	39.076122
2603.092146	522780.267685	39.081140
2605.749081	523868.290643	39.086157
2608.510934	524966.439089	39.091175
2611.698445	526041.221282	39.096192
2614.629650	527134.296686	39.101210
2617.609133	528216.509150	39.106228
2620.505964	529283.453007	39.111245
2623.631139	530366.589873	39.116263
2626.403220	531424.992554	39.121280
2629.309712	532483.446311	39.126298
2632.096258	533516.226717	39.131316
2634.799292	534534.202686	39.136333
2637.852080	535541.781541	39.141351
2640.851324	536535.763513	39.146368
2643.616892	537542.898278	39.151386
2646.110499	538545.178492	39.156404
2648.974747	539550.745311	39.161421
2651.097817	540556.467773	39.166439
2653.781618	541556.942349	39.171456
2656.373160	542565.911474	39.176474
2659.057112	543571.522957	39.181492
2662.020047	544575.304296	39.186509
2664.165374	545602.384005	39.191527
2666.912265	546616.664139	39.196544
2669.115027	547635.789065	39.201562
2671.757617	548665.018800	39.206580
2674.672063	549690.253796	39.211597
2677.191267	550732.820671	39.216615
2679.507842	551777.452992	39.221632
2682.206434	552822.542355	39.226650
2685.030277	553877.730666	39.231668
2687.638955	554926.691978	39.236685
2690.377079	556001.324883	39.241703
2693.130222	557061.901257	39.246720
2695.874360	558120.133636	39.251738
2698.727984	559184.591969	39.256756
2701.462271	560254.359157	39.261773
2704.158019	561331.278111	39.266791
2706.823730	562402.137084	39.271808
2709.528758	563468.582553	39.276826
2712.260412	564554.719688	39.281844
2715.375889	565628.649823	39.286861
2718.042736	566718.783068	39.291879
2720.757246	567801.285461	39.296896
2723.340614	568874.783651	39.301914
2726.282405	569958.017861	39.306932
2729.438965	571045.438979	39.311949
2732.021369	572140.492449	39.316967
2734.892081	573211.817394	39.321984
2738.154123	574289.707373	39.327002
2740.921133	575378.626410	39.332020
2744.228784	576448.244708	39.337037
2746.541133	577521.201358	39.342055
2749.522094	578595.455408	39.347072
2752.499618	579671.120974	39.352090
2755.114937	580755.379704	39.357108
2757.852335	581816.605742	39.362125
2760.352429	582899.139404	39.367143
2763.403657	583982.635570	39.372160
2765.971217	585054.938297	39.377178
2768.514755	586154.618909	39.382196
2770.919554	587232.520068	39.387213
2773.900767	588331.475361	39.392231
2776.936886	589411.377662	39.397248
2779.690194	590489.526592	39.402266
2781.943474	591553.383484	39.407284
2784.611871	592599.288609	39.412301
2787.522694	593669.505478	39.417319
2789.942497	594724.431275	39.422336
2792.674231	595784.016844	39.427354
2794.781701	596862.743582	39.432372
2797.654889	597933.127072	39.437389
2800.517800	599013.978435	39.442407
2802.945970	600097.256117	39.447424
2806.186480	601187.451858	39.452442
2808.786433	602285.011737	39.457460
2811.532621	603383.141936	39.462477
2814.041615	604498.072717	39.467495
2816.746288	605616.363501	39.472512
2818.935584	606742.787850	39.477530
2821.329091	607880.772319	39.482548
2823.996740	609020.295585	39.487565
2826.307133	610192.678396	39.492583
2829.065572	611354.457945	39.497600
2832.459703	612534.161618	39.502618
2834.832472	613715.364258	39.507636
2837.656024	614892.913402	39.512653
2840.904108	616089.712109	39.517671
2843.728059	617286.052602	39.522688
2846.662071	618472.146339	39.527706
2849.591397	619677.153517	39.532724
2852.286170	620869.523490	39.537741
2855.499459	622079.611700	39.542759
2857.932723	623297.990806	39.547776
2861.265049	624507.785145	39.552794
2864.155637	625729.406245	39.557812
2867.687587	626933.596525	39.562829
2870.706282	628159.411470	39.567847
2873.350089	629372.465205	39.572864
2876.345455	630582.123835	39.577882
2879.154315	631810.695225	39.582900
2882.288749	633039.166546	39.587917
2884.656089	634260.686599	39.592935
2887.341676	635487.997184	39.597952
2890.452331	636726.466472	39.602970
2893.242998	637983.750896	39.607988
2896.326312	639218.981365	39.613005
2899.199812	640457.340899	39.618023
2902.105421	641702.128069	39.623040
2905.299538	642936.041829	39.628058
2908.437767	644194.247230	39.633076
2911.260060	645428.967501	39.638093
2914.044503	646679.494619	39.643111
2916.871009	647925.273029	39.648128
2920.110089	649167.436742	39.653146
2923.004038	650428.041553	39.658164
2926.178417	651666.316233	39.663181
2929.719466	652922.108554	39.668199
2932.545108	654159.980551	39.673216
2935.816201	655382.230475	39.678234
2938.763809	656583.566790	39.683252
2941.429073	657771.906878	39.688269
2944.041874	658965.637143	39.693287
2946.938558	660162.756181	39.698304
2949.931715	661346.569767	39.703322
2952.374841	662551.981323	39.708340
2955.073485	663742.269061	39.713357
2958.225721	664966.513995	39.718375
2960.696661	666189.922145	39.723392
2963.354658	667405.629620	39.728410
2965.832643	668632.850389	39.733428
2968.771258	669872.663549	39.738445
2971.659135	671129.576329	39.743463
2974.440306	672378.384158	39.748480
2977.356179	673653.945392	39.753498
2979.718498	674935.142518	39.758516
2982.712723	676208.053793	39.763533
2985.597706	677507.939434	39.768551
2988.101730	678822.711220	39.773568
2990.925673	680130.981203	39.778586
2993.280425	681466.064903	39.783604
2995.988378	682804.121055	39.788621
2998.882468	684155.156580	39.793639
3001.816195	685511.345828	39.798656
3004.889182	686876.044167	39.803674
3007.607270	688262.632557	39.808692
3010.504881	689653.690215	39.813709
3014.358464	691033.006089	39.818727
3017.225741	692425.670984	39.823744
3021.018249	693816.768924	39.828762
3023.889837	695210.632076	39.833780
3027.000139	696596.151699	39.838797
3030.343114	697989.989768	39.843815
3033.278411	699387.293962	39.848832
3036.545694	700781.145648	39.853850
3040.016431	702178.455454	39.858868
3043.559704	703565.965173	39.863885
3046.989539	704954.559083	39.868903
3049.979183	706332.652337	39.873920
3053.043250	707716.948993	39.878938
3056.079797	709117.662305	39.883956
3059.101511	710499.286258	39.888973
3062.222901	711888.587587	39.893991
3065.149811	713287.739929	39.899008
3068.226775	714677.183476	39.904026
3071.365006	716076.825179	39.909044
3074.317125	717465.481349	39.914061
3077.719358	718864.956843	39.919079
3080.887474	720270.170226	39.924096
3083.912225	721661.821109	39.929114
3086.650758	723077.210504	39.934132
3089.418220	724475.251379	39.939149
3092.476474	725889.755284	39.944167
3095.107801	727307.644275	39.949184
3098.499175	728704.261871	39.954202
3101.797376	730081.936907	39.959220
3104.733867	731452.427062	39.964237
3108.022468	732817.538789	39.969255
3111.183468	734183.279461	39.974272
3114.207699	735554.733029	39.979290
3117.092816	736927.948495	39.984308
3120.093893	738294.641258	39.989325
3123.264050	739675.325570	39.994343
3126.283040	741068.864279	39.999360
3129.581641	742451.950570	40.004378
3132.458377	743843.641100	40.009396
3135.429834	745245.370360	40.014413
3138.530666	746664.913144	40.019431
3141.059521	748076.755201	40.024448
3144.145347	749491.890661	40.029466
3147.239722	750930.359767	40.034484
3149.709524	752368.765199	40.039501
3152.763799	753824.231782	40.044519
3155.207081	755296.165231	40.049536
3158.008771	756771.247796	40.054554
3160.967923	758275.051039	40.059572
3163.219591	759802.981251	40.064589
3166.066574	761327.056967	40.069607
3169.022473	762867.723020	40.074624
3172.186610	764426.032778	40.079642
3175.276107	765992.632792	40.084660
3178.287810	767568.057776	40.089677
3181.764404	769145.427044	40.094695
3184.387585	770747.611198	40.099712
3187.601295	772342.911205	40.104730
3190.723298	773947.258999	40.109748
3193.809183	775564.418168	40.114765
3197.162955	777192.019916	40.119783
3200.287760	778814.682431	40.124800
3204.108066	780448.195146	40.129818
3207.480640	782089.801313	40.134836
3210.540925	783713.185330	40.139853
3214.265114	785347.118693	40.144871
3217.891960	786992.457885	40.149888
3221.000599	788612.755683	40.154906
3225.034657	790237.962487	40.159924
3228.354327	791854.686885	40.164941
3232.003018	793468.876811	40.169959
3235.649261	795088.569861	40.174976
3239.141767	796701.744952	40.179994
3242.606556	798302.951529	40.185012
3246.097059	799910.339400	40.190029
3249.570795	801500.577259	40.195047
3252.999518	803113.195325	40.200064
3256.416770	804694.437390	40.205082
3260.073525	806280.404704	40.210100
3263.246097	807863.250299	40.215117
3266.549785	809447.120731	40.220135
3269.917373	811035.395858	40.225152
3272.932969	812601.819663	40.230170
3276.183656	814144.450568	40.235188
3279.182292	815680.081138	40.240205
3282.760661	817199.983760	40.245223
3285.880747	818724.691105	40.250240
3289.077383	820248.985489	40.255258
3292.559679	821766.831720	40.260276
3295.610983	823290.154664	40.265293
3299.143616	824807.679478	40.270311
3302.061793	826334.021491	40.275328
3305.485044	827864.597123	40.280346
3308.983488	829400.108728	40.285364
3311.788791	830943.896915	40.290381
3315.190408	832479.618552	40.295399
3317.972764	834044.382538	40.300416
3320.981344	835607.022712	40.305434
3323.576560	837171.443377	40.310452
3326.876426	838769.213372	40.315469
3329.939669	840365.843523	40.320487
3333.035035	841985.692571	40.325504
3336.365643	843591.768007	40.330522
3339.611880	845210.664094	40.335540
3342.201075	846853.057219	40.340557
3345.798650	848500.673932	40.345575
3348.843839	850169.797072	40.350592
3352.278916	851835.880252	40.355610
3355.495653	853508.636206	40.360628
3358.549698	855200.952719	40.365645
3361.863211	856888.199278	40.370663
3364.754186	858595.222488	40.375680
3367.829746	860309.491547	40.380698
3371.002691	862035.568443	40.385716
3374.163812	863779.370056	40.390733
3377.302875	865517.246944	40.395751
3380.520945	867277.169608	40.400768
3383.735933	869044.513356	40.405786
3387.387664	870818.904171	40.410804
3390.351461	872618.617039	40.415821
3393.600424	874406.708787	40.420839
3397.433630	876199.670172	40.425856
3400.584537	878000.223829	40.430874
3404.183224	879810.100330	40.435892
3407.204234	881626.952295	40.440909
3410.844499	883439.751257	40.445927
3413.923070	885267.911034	40.450944
3417.623800	887094.517320	40.455962
3421.748723	888904.938781	40.460980
3425.441259	890730.293401	40.465997
3429.158218	892534.813640	40.471015
3432.672374	894354.314065	40.476032
3436.342811	896165.688601	40.481050
3440.229914	897971.147845	40.486068
3443.821640	899786.574237	40.491085
3447.295795	901578.234809	40.496103
3450.968509	903374.772379	40.501120
3454.080933	905152.036245	40.506125
3457.902369	906885.751050	40.511130
3461.147973	908550.106320	40.516135
3464.525020	910145.716778	40.521140
3467.651481	911675.980991	40.526144
3470.569524	913141.137629	40.531149
3473.808750	914524.683557	40.536154
3476.421843	915820.007218	40.541159
3479.489926	917039.496806	40.546164
3482.435129	918189.940088	40.551168
3485.011524	919255.357763	40.556173
3488.257335	920252.357401	40.561178
3490.456577	921173.095666	40.566183
3492.777450	922008.470403	40.571188
3495.335050	922784.457388	40.576192
3497.648463	923486.554030	40.581197
3499.955038	924121.476334	40.586202
3501.683399	924700.108649	40.591207
3503.211463	925222.116423	40.596212
3505.388297	925689.677206	40.601216
3507.288162	926077.311708	40.606221
3508.982160	926415.766862	40.611226
3510.362960	926714.100187	40.616231
3511.396981	926960.316982	40.621236
3513.010260	927173.285074	40.626240
3514.049204	927328.904542	40.631245
3515.685369	927442.732480	40.636250
3516.053115	927530.265513	40.641255
3517.147985	927571.378778	40.646260
3518.216406	927590.693809	40.651264
3518.930447	927565.119641	40.656269
3519.725377	927534.537094	40.661274
3520.049249	927457.067249	40.666279
3521.022441	927355.472900	40.671284
3521.624048	927237.995354	40.676288
3522.025472	927098.360726	40.681293
3523.139973	926928.054335	40.686298
3523.435857	926742.704558	40.691303
3524.322405	926542.549579	40.696308
3524.378020	926314.572879	40.701312
3524.802957	926085.946948	40.706317
3525.805901	925817.820684	40.711322
3525.870391	925560.025931	40.716327
3526.213158	925264.024404	40.721332
3526.791073	924975.845989	40.726336
3526.929846	924670.333161	40.731341
3527.681399	924334.521469	40.736346
3527.636479	924016.893467	40.741351
3527.925666	923663.242020	40.746356
3528.323000	923311.086742	40.751360
3528.539239	922944.519816	40.756365
3528.604832	922573.723563	40.761370
3529.154136	922182.532926	40.766375
3529.416005	921792.997436	40.771380
3529.660604	921392.955525	40.776384
3529.885278	920982.501490	40.781389
3530.545331	920562.997843	40.786394
3530.445372	920146.380500	40.791399
3530.374799	919707.506683	40.796404
3530.800788	919279.190095	40.801408
3530.469833	918836.345925	40.806413
3530.784265	918385.177377	40.811418
3531.286446	917945.870332	40.816423
3531.175856	917486.424630	40.821428
3531.633779	917021.838713	40.826432
3531.476428	916557.606786	40.831437
3531.737137	916086.333685	40.836442
3531.905561	915621.292396	40.841447
3531.829080	915136.036788	40.846452
3532.146100	914652.788872	40.851456
3532.151220	914164.063076	40.856461
3532.392702	913673.134681	40.861466
3532.075696	913190.828468	40.866471
3532.082660	912685.887464	40.871476
3532.277622	912190.788804	40.876480
3532.346066	911691.910151	40.881485
3532.331574	911183.462783	40.886490
3532.422060	910682.947201	40.891495
3532.607331	910177.648403	40.896500
3532.697040	909675.692256	40.901504
3532.650158	909156.077277	40.906509
3532.785691	908641.008533	40.911514
3532.958105	908137.837966	40.916519
3532.729194	907609.818700	40.921524
3532.713625	907094.824307	40.926528
3532.834212	906575.227048	40.931533
3533.362220	906035.550890	40.936538
3532.958739	905520.572746	40.941543
3533.209966	904999.166042	40.946548
3533.404665	904463.541109	40.951552
3533.432281	903930.594124	40.956557
3533.708552	903385.976779	40.961562
3533.367281	902848.454928	40.966567
3533.415199	902307.341096	40.971572
3533.008219	901772.139112	40.976576
3532.736639	901231.844171	40.981581
3533.161907	900692.632877	40.986586
3532.951449	900157.629000	40.991591
3533.116404	899629.750424	40.996596
3533.301910	899087.433027	41.001600
3533.060357	898553.053918	41.006605
3533.152399	898005.337450	41.011610
3533.411095	897456.573506	41.016615
3533.455097	896898.810327	41.021620
3533.363485	896349.418971	41.026624
3532.811443	895809.423427	41.031629
3533.336258	895254.603811	41.036634
3533.449910	894706.563666	41.041639
3533.189834	894161.626578	41.046644
3533.641403	893606.464915	41.051648
3533.487809	893048.839374	41.056653
3533.797589	892487.503600	41.061658
3533.631654	891932.863960	41.066663
3533.926987	891367.553493	41.071668
3533.968397	890791.787888	41.076672
3533.162017	890233.804952	41.081677
3533.268230	889670.196084	41.086682
3533.401293	889122.872515	41.091687
3533.464802	888554.228534	41.096692
3533.444001	887994.152193	41.101696
3533.382061	887437.801375	41.106701
3533.547877	886877.197358	41.111706
3533.092442	886313.645082	41.116711
3533.708050	885756.145217	41.121716
3533.310558	885191.892776	41.126720
3533.188298	884629.377301	41.131725
3533.657813	884058.477839	41.136730
3533.342687	883500.725717	41.141735
3533.428187	882932.491599	41.146740
3533.348295	882362.099782	41.151744
3533.358232	881800.642816	41.156749
3533.533156	881226.900365	41.161754
3533.056646	880661.251939	41.166759
3533.397859	880090.274961	41.171764
3533.421010	879516.002548	41.176768
3533.069177	878954.623812	41.181773
3532.969920	878380.842104	41.186778
3533.425852	877816.115553	41.191783
3533.428010	877245.500188	41.196788
3533.287461	876671.752084	41.201792
3533.368746	876096.165251	41.206797
3533.682520	875509.139881	41.211802
3532.888011	874936.206626	41.216807
3532.688654	874371.357990	41.221812
3533.104219	873801.986554	41.226816
3533.190776	873237.077620	41.231821
3533.076928	872658.570144	41.236826
3532.857438	872092.149326	41.241831
3532.844369	871529.228539	41.246836
3533.072058	870951.175267	41.251840
3532.618570	870381.138434	41.256845
3533.146013	869785.649565	41.261850
3533.009388	869216.126378	41.266855
3532.785018	868638.119812	41.271860
3532.835451	868064.766646	41.276864
3532.431690	867506.482766	41.281869
3533.227633	866928.136708	41.286874
3532.621966	866353.954979	41.291879
3532.850396	865777.730930	41.296884
3532.813786	865197.126768	41.301888
3533.060684	864627.295846	41.306893
3533.109913	864048.897174	41.311898
3533.071066	863472.012288	41.316903
3532.555588	862897.388064	41.321908
3533.005525	862315.548904	41.326912
3533.065102	861727.695961	41.331917
3533.412319	861149.260318	41.336922
3533.696635	860563.005247	41.341927
3532.966761	859978.324642	41.346932
3532.905549	859378.698268	41.351936
3532.796651	858802.547168	41.356941
3532.779309	858210.769961	41.361946
3532.576805	857640.261261	41.366951
3532.666977	857047.964019	41.371956
3532.846393	856469.404075	41.376960
3532.599879	855906.326792	41.381965
3532.845870	855312.667911	41.386970
3532.361651	854736.878557	41.391975
3532.435425	854145.860102	41.396980
3532.785053	853575.559705	41.401984
3532.689372	852993.800208	41.406989
3532.938354	852406.087955	41.411994
3532.784684	851827.731805	41.416999
3532.808384	851243.840470	41.422004
3532.988499	850644.584221	41.427008
3532.588970	850069.804811	41.432013
3532.512951	849478.559922	41.437018
3532.586885	848893.854457	41.442023
3532.887902	848298.343280	41.447028
3532.823524	847708.778358	41.452032
3532.202328	847121.882513	41.457037
3532.558582	846534.667188	41.462042
3532.509710	845958.279255	41.467047
3532.328301	845360.426844	41.472052
3532.775103	844774.492256	41.477056
3532.590228	844193.677930	41.482061
3532.492915	843606.557823	41.487066
3532.332906	843018.516401	41.492071
3532.413096	842423.360977	41.497076
3532.235367	841841.548411	41.502080
3531.804086	841264.502518	41.507085
3532.414071	840666.361163	41.512090
3532.326364	840091.538279	41.517095
3531.964935	839505.885448	41.522100
3531.923850	838922.952100	41.527104
3531.814912	838340.366939	41.532109
3531.944288	837755.151520	41.537114
3532.213380	837178.882149	41.542119
3532.022860	836590.931604	41.547124
3531.988083	836008.266707	41.552128
3531.687693	835434.571383	41.557133
3531.871193	834833.807326	41.562138
3531.613951	834254.972990	41.567143
3531.968230	833685.157046	41.572148
3532.168920	833092.718670	41.577152
3532.011778	832506.583564	41.582157
3532.601103	831921.732129	41.587162
3532.295757	831333.953406	41.592167
3531.827605	830743.414647	41.597172
3531.829801	830145.661179	41.602176
3531.736497	829565.595763	41.607181
3531.843760	828978.215936	41.612186
3531.481342	828399.996789	41.617191
3532.039885	827802.860147	41.622196
3532.257263	827224.095373	41.627200
3531.881655	826630.185896	41.632205
3532.047509	826035.543483	41.637210
3532.326273	825450.845035	41.642215
3531.844057	824856.108042	41.647220
3532.068520	824265.301752	41.652224
3531.320945	823675.243498	41.657229
3531.624068	823082.117506	41.662234
3531.864596	822502.979355	41.667239
3531.676445	821910.173588	41.672244
3531.788945	821322.397194	41.677248
3531.544749	820727.440826	41.682253
3531.351819	820136.970207	41.687258
3531.060402	819554.973848	41.692263
3531.266872	818968.194444	41.697268
3531.281622	818386.140818	41.702272
3531.129464	817803.624266	41.707277
3531.341163	817223.000458	41.712282
3531.523220	816642.771355	41.717287
3531.313329	816056.735262	41.722292
3531.481148	815465.346588	41.727296
3530.997125	814894.671065	41.732301
3531.155045	814304.209004	41.737306
3530.893481	813721.843557	41.742311
3530.804650	813140.279170	41.747316
3531.063589	812558.458071	41.752320
3531.165715	811977.249851	41.757325
3530.965135	811391.195065	41.762330
3531.136318	810810.755674	41.767335
3530.737639	810230.265596	41.772340
3531.030921	809645.835803	41.777344
3530.760881	809061.598560	41.782349
3531.161886	808473.032080	41.787354
3530.931584	807897.652809	41.792359
3530.952152	807318.261955	41.797364
3531.168404	806724.528321	41.802368
3530.731464	806151.290407	41.807373
3530.777183	805562.924271	41.812378
3530.735458	804974.816346	41.817383
3530.762769	804393.067548	41.822388
3530.850562	803817.877131	41.827392
3530.874891	803244.904467	41.832397
3530.852122	802649.680230	41.837402
3530.430022	802071.978566	41.842407
3530.466003	801492.482689	41.847412
3530.956648	800905.895967	41.852416
3530.895548	800324.895990	41.857421
3530.568119	799736.975985	41.862426
3530.930922	799158.503289	41.867431
3530.871141	798576.816244	41.872436
3530.606878	797984.517011	41.877440
3530.612068	797410.767638	41.882445
3530.693656	796812.911559	41.887450
3530.766003	796228.403910	41.892455
3530.229661	795652.638573	41.897460
3530.590733	795067.296934	41.902464
3530.513135	794488.068237	41.907469
3530.350933	793904.141936	41.912474
3530.441722	793322.136689	41.917479
3530.506995	792744.752133	41.922484
3530.358201	792160.481606	41.927488
3530.353119	791581.687390	41.932493
3530.509004	790987.788864	41.937498
3530.250091	790417.193373	41.942503
3530.068877	789818.882168	41.947508
3530.648850	789237.682995	41.952512
3530.393171	788655.645154	41.957517
3530.196803	788082.590122	41.962522
3530.094298	787501.512130	41.967527
3530.120198	786918.988564	41.972532
3530.259907	786336.840076	41.977536
3530.051412	785757.947318	41.982541
3530.255373	785172.055310	41.987546
3530.247799	784598.686837	41.992551
3529.886841	784011.222764	41.997556
3529.830749	783421.691625	42.002560
3529.865545	782852.207423	42.007565
3529.530014	782268.775403	42.012570
3529.953851	781694.707026	42.017575
3529.767073	781127.435072	42.022580
3530.087748	780544.390264	42.027584
3529.599911	779968.519754	42.032589
3529.744550	779383.492577	42.037594
3529.689934	778818.574322	42.042599
3529.976729	778242.679824	42.047604
3530.121320	777658.054189	42.052608
3530.009174	777081.791010	42.057613
3529.750767	776495.418033	42.062618
3530.169947	775908.439071	42.067623
3529.758349	775335.878303	42.072628
3529.925392	774745.058430	42.077632
3529.923638	774171.400890	42.082637
3529.424676	773593.105910	42.087642
3529.376593	773018.627244	42.092647
3529.085832	772439.073002	42.097652
3529.066442	771866.616487	42.102656
3528.997003	771305.845262	42.107661
3528.911491	770729.174407	42.112666
3529.110672	770156.104047	42.117671
3529.135837	769593.708465	42.122676
3529.124729	769016.890880	42.127680
3528.797030	768458.952178	42.132685
3529.067680	767891.162588	42.137690
3529.151649	767322.474370	42.142695
3529.017179	766750.280954	42.147700
3529.272264	766182.511036	42.152704
3529.011257	765616.806649	42.157709
3528.987405	765040.322585	42.162714
3528.943775	764475.480229	42.167719
3528.782460	763911.896978	42.172724
3528.898057	763334.567165	42.177728
3528.636144	762782.354123	42.182733
3528.771266	762215.042408	42.187738
3528.980624	761649.795605	42.192743
3528.833341	761072.484407	42.197748
3528.604202	760507.275862	42.202752
3528.561779	759934.396998	42.207757
3528.555389	759380.558595	42.212762
3528.430944	758815.452002	42.217767
3528.116447	758258.821367	42.222772
3528.336798	757701.466417	42.227776
3528.070387	757139.071253	42.232781
3528.531144	756575.819419	42.237786
3528.242913	756017.687446	42.242791
3528.250956	755459.661366	42.247796
3528.245963	754900.115915	42.252800
3528.472905	754339.650689	42.257805
3528.377579	753772.979393	42.262810
3528.451149	753215.814765	42.267815
3528.339711	752646.396913	42.272820
3528.286384	752086.456378	42.277824
3528.061909	751528.281884	42.282829
3528.203677	750967.930259	42.287834
3528.384433	750409.704202	42.292839
3528.198190	749856.439382	42.297844
3528.607798	749293.450823	42.302848
3528.428823	748732.448235	42.307853
3528.617610	748162.054841	42.312858
3528.324116	747596.543435	42.317863
3528.029957	747041.860684	42.322868
3527.769351	746469.393848	42.327872
3528.144865	745920.100252	42.332877
3528.204055	745361.827745	42.337882
3528.174452	744802.937376	42.342887
3527.628075	744248.840100	42.347892
3527.770884	743681.684872	42.352896
3527.884133	743127.247282	42.357901
3527.514912	742575.374103	42.362906
3528.040181	742018.760968	42.367911
3527.766088	741469.364722	42.372916
3527.571774	740905.774754	42.377920
3527.412975	740362.660256	42.382925
3527.655113	739803.070796	42.387930
3527.752943	739245.494096	42.392935
3527.537371	738708.556661	42.397940
3527.530418	738154.630572	42.402944
3527.668422	737604.252182	42.407949
3527.677985	737047.228501	42.412954
3527.619004	736494.580728	42.417959
3527.593688	735934.120860	42.422964
3527.567360	735384.359197	42.427968
3527.574551	734840.096234	42.432973
3527.332582	734286.881450	42.437978
3527.347521	733731.208994	42.442983
3527.173738	733194.783701	42.447988
3527.295743	732629.711673	42.452992
3527.324036	732088.822193	42.457997
3527.442097	731539.217694	42.463002
3527.151893	730991.031647	42.468007
3527.036754	730449.858627	42.473012
3527.234709	729898.643417	42.478016
3527.117479	729357.694750	42.483021
3527.152435	728810.642352	42.488026
3527.341234	728256.939986	42.493031
3527.089016	727716.003944	42.498036
3527.120425	727165.820161	42.503040
3527.207301	726618.314167	42.508045
3527.366353	726065.508042	42.513050
3527.198373	725521.291028	42.518055
3526.885250	724976.765300	42.523060
3527.024990	724422.464142	42.528064
3526.862528	723888.542777	42.533069
3526.672510	723338.783433	42.538074
3527.064187	722792.158846	42.543079
3526.657215	722253.712808	42.548084
3526.925470	721701.684312	42.553088
3526.603799	721159.980165	42.558093
3526.988869	720619.111273	42.563098
3527.089247	720071.116930	42.568103
3526.565345	719527.258291	42.573108
3526.883653	718977.270504	42.578112
3526.841863	718442.133455	42.583117
3526.609007	717899.705263	42.588122
3526.573354	717355.274047	42.593127
3526.649829	716813.069469	42.598132
3526.779335	716274.937194	42.603136
3526.529663	715732.470211	42.608141
3526.431880	715194.158444	42.613146
3526.479319	714649.487287	42.618151
3526.423944	714122.509047	42.623156
3526.718523	713580.008426	42.628160
3526.716846	713034.496844	42.633165
3526.586606	712496.613289	42.638170
3526.350090	711951.567963	42.643175
3526.320691	711421.885709	42.648180
3526.433540	710887.729066	42.653184
3526.025729	710352.237952	42.658189
3526.080739	709812.464687	42.663194
3526.375678	709285.124992	42.668199
3525.821526	708744.941214	42.673204
3525.954265	708205.847024	42.678208
3525.928843	707688.143836	42.683213
3525.895448	707153.728077	42.688218
3526.100355	706619.486517	42.693223
3525.818734	706089.465860	42.698228
3526.235416	705550.106173	42.703232
3525.902124	705025.739520	42.708237
3525.663328	704502.169074	42.713242
3525.604566	703965.622137	42.718247
3525.744349	703444.654594	42.723252
3525.982608	702912.561287	42.728256
3526.022829	702390.951110	42.733261
3525.883306	701851.455012	42.738266
3525.773114	701319.869795	42.743271
3525.744464	700799.218959	42.748276
3525.768528	700268.391148	42.753280
3525.582539	699739.753321	42.758285
3525.578070	699210.605168	42.763290
3525.663595	698688.417148	42.768295
3525.711818	698165.160546	42.773300
3525.543703	697629.731826	42.778304
3525.388406	697120.364962	42.783309
3525.599173	696595.247065	42.788314
3525.354012	696068.584767	42.793319
3525.308058	695552.894085	42.798324
3525.400564	695023.078848	42.803329
3525.472880	694510.439336	42.808333
3525.539866	693973.156728	42.813338
3525.613513	693453.593519	42.818343
3525.623680	692927.147692	42.823348
3525.597763	692406.296780	42.828353
3525.673789	691883.458146	42.833357
3525.554648	691356.294661	42.838362
3525.616321	690826.084483	42.843367
3525.125708	690311.756399	42.848372
3524.678392	689779.929298	42.853377
3524.859014	689267.117934	42.858381
3524.876798	688754.006462	42.863386
3524.941874	688239.912140	42.868391
3524.491443	687721.646715	42.873396
3524.884315	687203.306949	42.878401
3524.984533	686692.900153	42.883405
3524.765346	686176.646204	42.888410
3524.731780	685665.109139	42.893415
3524.632909	685153.056507	42.898420
3524.988728	684638.507934	42.903425
3524.886657	684133.267482	42.908429
3524.553868	683624.901926	42.913434
3524.827166	683110.728823	42.918439
3524.540398	682604.289756	42.923444
3524.448923	682089.872302	42.928449
3524.916784	681585.836965	42.933453
3524.548146	681077.484668	42.938458
3524.898643	680556.929726	42.943463
3524.726494	680051.873290	42.948468
3524.416321	679535.755755	42.953473
3524.230631	679041.403985	42.958477
3524.057866	678530.087681	42.963482
3524.125921	678029.162744	42.968487
3524.397833	677536.395486	42.973492
3524.035030	677027.070696	42.978497
3524.072774	676516.453715	42.983501
3524.275876	676017.688407	42.988506
3524.172783	675516.307679	42.993511
3523.957178	675019.852223	42.998516
3524.079621	674514.392476	43.003521
3524.195522	674019.172458	43.008525
3523.923110	673517.513466	43.013530
3524.164902	673015.091768	43.018535
3523.345734	672526.879984	43.023540
3523.983250	672025.882684	43.028545
3524.175330	671536.948138	43.033549
3524.178480	671034.261425	43.038554
3523.742101	670532.071515	43.043559
3523.681563	670039.512623	43.048564
3524.240292	669541.088433	43.053569
3523.766980	669039.573070	43.058573
3523.825322	668544.871435	43.063578
3523.786395	668046.071413	43.068583
3523.686379	667553.788449	43.073588
3523.632272	667063.267466	43.078593
3523.488371	666576.626682	43.083597
3523.427334	666085.158597	43.088602
3523.393562	665597.201936	43.093607
3523.211844	665105.703879	43.098612
3523.262812	664615.637317	43.103617
3523.407020	664133.811023	43.108621
3523.204303	663655.811324	43.113626
3523.274471	663162.174692	43.118631
3522.967091	662678.855500	43.123636
3523.205963	662199.510315	43.128641
3523.142091	661713.656003	43.133645
3522.975130	661230.888727	43.138650
3523.021225	660748.210607	43.143655
3523.053349	660265.111470	43.148660
3523.184790	659787.910527	43.153665
3523.024735	659313.331267	43.158669
3522.629483	658832.629366	43.163674
3523.126705	658350.503336	43.168679
3522.855630	657880.565172	43.173684
3522.916090	657403.608493	43.178689
3522.819910	656920.913845	43.183693
3522.500435	656442.527170	43.188698
3522.807623	655960.764634	43.193703
3522.772803	655493.716804	43.198708
3522.706921	655017.464044	43.203713
3522.662864	654541.184419	43.208717
3522.510735	654067.696736	43.213722
3522.521068	653599.302505	43.218727
3522.680096	653133.307856	43.223732
3522.695439	652660.922551	43.228737
3522.517936	652186.299853	43.233741
3522.498333	651718.121059	43.238746
3523.415737	651246.113522	43.243751
3522.816896	650774.242453	43.248756
3523.173809	650287.148263	43.253761
3522.759975	649817.947848	43.258765
3522.686057	649341.122811	43.263770
3523.085038	648860.296884	43.268775
3522.677768	648385.081907	43.273780
3522.536802	647913.996353	43.278785
3522.017132	647435.707202	43.283789
3522.343376	646963.347740	43.288794
3522.194029	646494.495664	43.293799
3521.810187	646042.354954	43.298804
3522.194876	645569.769994	43.303809
3522.465808	645106.629314	43.308813
3521.897666	644639.311747	43.313818
3521.815336	644181.787401	43.318823
3521.694020	643724.448952	43.323828
3521.782480	643261.354754	43.328833
3522.104469	642811.798354	43.333837
3521.764762	642344.485725	43.338842
3521.712129	641893.002659	43.343847
3521.412615	641437.091474	43.348852
3521.555977	640974.233610	43.353857
3521.617706	640529.071136	43.358861
3521.373519	640082.241164	43.363866
3521.221795	639623.223113	43.368871
3521.448553	639178.273693	43.373876
3521.418151	638729.097520	43.378881
3521.108738	638285.251212	43.383885
3521.179062	637838.519767	43.388890
3521.495698	637385.624154	43.393895
3521.258039	636943.958708	43.398900
3521.255452	636492.879240	43.403905
3521.274575	636047.179463	43.408909
3520.933584	635607.025349	43.413914
3520.985133	635159.630775	43.418919
3521.074478	634728.571932	43.423924
3521.160128	634279.232222	43.428929
3521.075135	633845.064155	43.433933
3520.896737	633392.128348	43.438938
3521.058691	632954.428107	43.443943
3520.682908	632516.951442	43.448948
3520.930890	632079.099713	43.453953
3521.176956	631635.974734	43.458957
3520.773081	631204.754250	43.463962
3521.067546	630764.186841	43.468967
3521.036112	630327.711137	43.473972
3521.024899	629894.617814	43.478977
3520.447202	629447.085874	43.483981
3520.553487	628998.216641	43.488986
3520.779427	628564.978110	43.493991
3520.545467	628136.706860	43.498996
3520.645832	627694.191751	43.504001
3520.659077	627266.243618	43.509005
3520.416953	626839.223121	43.514010
3520.562612	626405.609519	43.519015
3520.265332	625977.111611	43.524020
3520.293522	625543.532998	43.529025
3520.213312	625134.845420	43.534029
3520.159280	624702.198168	43.539034
3520.263437	624272.261052	43.544039
3520.198072	623851.551569	43.549044
3520.187616	623426.809083	43.554049
3520.164257	623004.606604	43.559053
3519.986034	622588.725639	43.564058
3520.317376	622153.455145	43.569063
3520.134550	621740.297370	43.574068
3520.049325	621314.682645	43.579073
3519.838369	620906.858284	43.584077
3519.947100	620483.732811	43.589082
3520.253266	620053.241834	43.594087
3520.068502	619645.315331	43.599092
3520.017386	619226.577390	43.604097
3520.218979	618794.901827	43.609101
3519.832586	618375.186105	43.614106
3520.100941	617951.283167	43.619111
3520.326755	617539.499092	43.624116
3520.222205	617117.331350	43.629121
3519.767990	616695.708190	43.634125
3519.691586	616275.056830	43.639130
3519.659509	615855.935581	43.644135
3519.589998	615452.644402	43.649140
3519.505973	615038.964506	43.654145
3519.684265	614629.184475	43.659149
3519.414665	614217.009230	43.664154
3519.780230	613810.675962	43.669159
3519.803861	613400.375320	43.674164
3519.558046	612989.453663	43.679169
3519.582467	612581.228228	43.684173
3519.493442	612178.071301	43.689178
3519.843175	611755.820866	43.694183
3519.207992	611346.409024	43.699188
3518.970816	610941.377144	43.704193
3519.144132	610540.773747	43.709197
3519.182080	610137.571280	43.714202
3519.028873	609725.359609	43.719207
3518.594401	609335.348511	43.724212
3519.001610	608939.512591	43.729217
3519.217572	608545.601294	43.734221
3519.063259	608140.303218	43.739226
3519.078655	607741.833509	43.744231
3518.719243	607347.677447	43.749236
3519.046923	606949.678138	43.754241
3518.957664	606557.354513	43.759245
3518.950128	606157.979849	43.764250
3518.872778	605765.275486	43.769255
3518.838587	605373.252507	43.774260
3518.897688	604970.713935	43.779265
3518.718448	604579.641537	43.784269
3518.835549	604196.182018	43.789274
3518.545384	603794.263458	43.794279
3518.658025	603414.290782	43.799284
3518.918161	603020.831665	43.804289
3518.693808	602627.792972	43.809293
3518.539251	602244.464672	43.814298
3518.493215	601849.461734	43.819303
3518.560726	601459.043090	43.824308
3518.798333	601073.550901	43.829313
3518.641196	600675.163730	43.834317
3518.511972	600297.287032	43.839322
3519.035280	599906.085243	43.844327
3518.824938	599514.393065	43.849332
3518.583025	599126.708835	43.854337
3518.589949	598737.161895	43.859341
3518.302579	598357.190394	43.864346
3518.482991	597959.906787	43.869351
3518.021759	597579.738635	43.874356
3518.068260	597200.224431	43.879361
3518.304996	596812.782632	43.884365
3518.168656	596448.638849	43.889370
3518.431431	596060.012708	43.894375
3518.271021	595680.986382	43.899380
3518.332894	595302.060435	43.904385
3518.178358	594917.735760	43.909389
3518.065915	594535.048468	43.914394
3518.077879	594158.805782	43.919399
3517.772409	593786.974479	43.924404
3517.661556	593418.563551	43.929409
3517.855757	593041.601040	43.934413
3517.620562	592669.923285	43.939418
3517.935659	592290.002952	43.944423
3517.775820	591926.476009	43.949428
3517.401442	591549.161003	43.954433
3517.640613	591178.309658	43.959437
3517.314289	590823.366965	43.964442
3517.710590	590449.602636	43.969447
3517.318140	590082.341317	43.974452
3517.619046	589721.632005	43.979457
3517.608196	589360.010416	43.984461
3517.111083	588994.994182	43.989466
3517.209027	588637.301171	43.994471
3517.457670	588278.918527	43.999476
3517.380408	587920.128558	44.004481
3517.571644	587550.277718	44.009485
3517.133136	587194.592785	44.014490
3517.380938	586830.940992	44.019495
3517.186416	586475.494579	44.024500
3517.459609	586112.620737	44.029505
3517.535866	585746.251699	44.034509
3517.112576	585391.063572	44.039514
3516.897767	585026.129523	44.044519
3517.089495	584678.756236	44.049524
3517.071915	584326.684142	44.054529
3517.347950	583977.165335	44.059533
3516.872307	583625.754213	44.064538
3517.026121	583263.217254	44.069543
3516.960250	582918.903684	44.074548
3516.721998	582556.462836	44.079553
3516.902613	582208.920159	44.084557
3516.620744	581862.854130	44.089562
3516.711431	581515.508121	44.094567
3516.783958	581168.859173	44.099572
3516.566508	580818.077015	44.104577
3517.029783	580475.615146	44.109581
3516.584229	580133.902218	44.114586
3517.105634	579780.550835	44.119591
3516.702954	579438.308414	44.124596
3516.662447	579088.603049	44.129601
3516.815142	578732.016097	44.134605
3516.624283	578394.586058	44.139610
3516.779736	578047.885125	44.144615
3516.766378	577709.048287	44.149620
3516.180740	577363.410155	44.154625
3516.467371	577028.576938	44.159629
3516.163557	576690.264709	44.164634
3516.224885	576345.543864	44.169639
3516.044389	576018.910777	44.174644
3516.229878	575677.067318	44.179649
3516.320119	575329.748241	44.184653
3515.844305	575011.991612	44.189658
3516.279252	574670.580947	44.194663
3516.288627	574344.072737	44.199668
3516.291547	574006.741866	44.204673
3516.728506	573675.364373	44.209677
3516.310791	573343.822204	44.214682
3516.358366	573002.281258	44.219687
3516.320610	572670.656432	44.224692
3516.254147	572329.217279	44.229697
3516.231631	571993.144693	44.234701
3515.976240	571661.932936	44.239706
3515.752108	571322.606561	44.244711
3516.318869	570992.092198	44.249716
3516.046509	570667.297632	44.254721
3516.362051	570336.406500	44.259725
3515.980320	570014.129757	44.264730
3516.217064	569672.466398	44.269735
3516.034000	569347.773738	44.274740
3516.085899	569014.075114	44.279745
3516.168741	568676.336485	44.284749
3515.594199	568355.459694	44.289754
3515.634790	568026.467773	44.294759
3515.991792	567695.551199	44.299764
3515.675020	567384.420056	44.304769
3516.201510	567049.834099	44.309773
3516.105440	566730.042756	44.314778
3516.091611	566394.877639	44.319783
3515.786804	566075.105612	44.324788
3515.792713	565744.047609	44.329793
3515.682752	565421.759595	44.334797
3515.679835	565102.767598	44.339802
3515.416816	564780.187642	44.344807
3515.588352	564455.562124	44.349812
3515.546657	564146.268973	44.354817
3515.693547	563817.453225	44.359821
3515.465253	563502.437366	44.364826
3515.666086	563178.227928	44.369831
3515.659202	562866.229940	44.374836
3515.617157	562544.060039	44.379841
3515.369414	562215.673892	44.384845
3515.318955	561907.889756	44.389850
3515.373679	561600.332158	44.394855
3515.590053	561274.159264	44.399860
3515.469921	560957.804516	44.404865
3515.719460	560645.155701	44.409869
3515.034526	560332.306470	44.414874
3515.202428	560017.440901	44.419879
3515.379747	559705.638108	44.424884
3515.145496	559394.099630	44.429889
3515.346990	559075.428696	44.434893
3515.085860	558771.585454	44.439898
3515.262089	558456.530015	44.444903
3515.569848	558147.236638	44.449908
3515.263746	557826.506845	44.454913
3515.650210	557512.098128	44.459917
3515.104246	557207.814236	44.464922
3515.187309	556896.565599	44.469927
3515.155159	556580.342555	44.474932
3515.142536	556271.160825	44.479937
3515.349914	555965.813131	44.484941
3514.900991	555653.820239	44.489946
3514.607225	555349.400352	44.494951
3514.831249	555051.534915	44.499956
3514.579121	554746.489639	44.504961
3514.675919	554440.269478	44.509965
3514.316264	554140.518596	44.514970
3514.401306	553843.607227	44.519975
3514.478046	553550.771722	44.524980
3514.221230	553261.009821	44.529985
3514.464736	552955.536859	44.534989
3513.969021	552682.732688	44.539994
3513.963352	552391.145654	44.544999
3514.246511	552113.561347	44.550004
3514.109986	551824.352654	44.555009
3514.345453	551524.844987	44.560013
3514.208387	551252.807308	44.565018
3514.244389	550955.639108	44.570023
3514.564126	550666.781305	44.575028
3513.973211	550386.488758	44.580033
3514.405239	550080.213104	44.585037
3514.023642	549807.180263	44.590042
3514.225843	549511.312795	44.595047
3514.253847	549232.150728	44.600052
3514.013230	548949.248804	44.605057
3514.218721	548661.476743	44.610061
3513.798783	548380.811307	44.615066
3514.137497	548094.919856	44.620071
3514.371911	547804.856691	44.625076
3514.088533	547529.846174	44.630081
3514.117082	547234.815975	44.635085
3514.181126	546960.894085	44.640090
3513.885911	546668.175329	44.645095
3513.788242	546390.085779	44.650100
3513.565857	546115.540641	44.655105
3514.001418	545831.702810	44.660109
3513.778495	545567.128325	44.665114
3513.915002	545272.037653	44.670119
3514.025197	544999.480499	44.675124
3513.747626	544721.892215	44.680129
3513.936792	544442.504518	44.685133
3513.911731	544163.954452	44.690138
3514.027194	543887.341132	44.695143
3513.546793	543604.773692	44.700148
3513.557752	543331.494853	44.705153
3513.796614	543052.675787	44.710157
3513.824969	542787.702878	44.715162
3513.579483	542505.980650	44.720167
3513.588937	542238.580216	44.725172
3513.555502	541962.256674	44.730177
3513.751005	541688.309063	44.735181
3513.333727	541421.621427	44.740186
3513.409826	541154.945338	44.745191
3513.508518	540893.605843	44.750196
3513.235404	540628.895707	44.755201
3513.842187	540345.925516	44.760205
3513.609542	540083.013733	44.765210
3513.306827	539812.796188	44.770215
3513.205407	539542.034756	44.775220
3513.414270	539280.545663	44.780225
3513.302513	539009.422744	44.785229
3513.005197	538747.051926	44.790234
3512.893524	538490.192729	44.795239
3513.112033	538236.651910	44.800244
3512.930367	537977.929149	44.805249
3513.329455	537711.082445	44.810253
3513.164727	537455.474608	44.815258
3512.962940	537191.595927	44.820263
3513.196428	536926.477839	44.825268
3512.785737	536673.369696	44.830273
3513.039615	536411.366111	44.835277
3512.993184	536158.337982	44.840282
3513.070642	535902.358292	44.845287
3512.803451	535642.094338	44.850292
3512.710791	535388.152426	44.855297
3513.223606	535133.093643	44.860301
3512.971464	534883.710520	44.865306
3513.041860	534629.929160	44.870311
3512.606977	534376.532309	44.875316
3512.716361	534124.501218	44.880321
3512.642936	533867.249689	44.885325
3512.369008	533610.986453	44.890330
3512.767122	533366.864746	44.895335
3513.070257	533119.172695	44.900340
3512.523394	532870.309631	44.905345
3512.754213	532612.176493	44.910349
3512.384796	532365.545097	44.915354
3512.529753	532112.917819	44.920359
3512.612620	531866.402561	44.925364
3512.361831	531626.096467	44.930369
3512.438021	531375.637987	44.935373
3512.328309	531139.690050	44.940378
3512.380937	530892.557898	44.945383
3512.670680	530654.363928	44.950388
3512.584871	530409.013517	44.955393
3512.533809	530158.757742	44.960397
3512.607660	529915.440943	44.965402
3512.092405	529674.289907	44.970407
3512.350187	529434.163717	44.975412
3512.164971	529189.011714	44.980417
3512.078368	528950.753354	44.985421
3511.974990	528723.850220	44.990426
3512.182616	528479.275444	44.995431
3512.170518	528249.119139	45.000436
3512.006670	528011.161598	45.005441
3512.105883	527774.871466	45.010445
3511.938233	527546.598346	45.015450
3511.871996	527304.625137	45.020455
3511.944723	527073.476960	45.025460
3512.099450	526844.633187	45.030465
3512.176815	526612.669372	45.035469
3512.121502	526383.248588	45.040474
3511.936850	526147.384788	45.045479
3512.123921	525914.987494	45.050484
3511.552501	525681.454010	45.055489
3511.923379	525445.888093	45.060493
3511.869579	525227.908923	45.065498
3511.959594	524997.381789	45.070503
3511.889329	524771.977503	45.075508
3511.900562	524543.425748	45.080513
3512.022705	524308.035803	45.085517
3511.835777	524090.012270	45.090522
3511.796374	523862.973404	45.095527
3511.947199	523633.828554	45.100532
3511.563032	523403.357824	45.105537
3512.285135	523168.301961	45.110541
3511.754415	522952.895639	45.115546
3511.755090	522718.107391	45.120551
3511.552306	522493.701334	45.125556
3511.467832	522271.190504	45.130561
3511.623690	522040.960161	45.135565
3511.274113	521822.830530	45.140570
3511.646914	521603.312005	45.145575
3511.794551	521383.576256	45.150580
3511.546290	521165.621833	45.155585
3511.496367	520935.561291	45.160589
3511.540956	520722.196343	45.165594
3511.245195	520494.140546	45.170599
3511.209750	520286.287624	45.175604
3511.293946	520078.310430	45.180609
3511.558318	519844.543607	45.185613
3510.806877	519633.975907	45.190618
3511.177039	519421.395668	45.195623
3511.278302	519216.989547	45.200628
3510.882003	518999.029339	45.205633
3511.474414	518786.503326	45.210637
3511.273766	518574.564325	45.215642
3511.126102	518361.805231	45.220647
3511.553484	518138.388895	45.225652
3511.197269	517928.689855	45.230657
3511.307700	517709.412566	45.235661
3511.330242	517501.006760	45.240666
3510.838735	517287.028724	45.245671
3511.139167	517075.791631	45.250676
3511.076082	516872.544070	45.255681
3511.542022	516663.293538	45.260685
3511.509626	516452.458318	45.265690
3510.969962	516228.068066	45.270695
3511.011210	516020.750353	45.275700
3510.935879	515824.613646	45.280705
3510.955269	515609.868411	45.285709
3511.142257	515403.426832	45.290714
3510.958370	515188.659950	45.295719
3511.244359	514989.167347	45.300724
3511.034508	514775.156945	45.305729
3511.003379	514568.943583	45.310733
3511.024714	514369.235612	45.315738
3510.810306	514160.168484	45.320743
3510.946996	513949.826090	45.325748
3510.782623	513761.408297	45.330753
3510.922491	513543.633149	45.335757
3510.739419	513352.485386	45.340762
3510.627621	513150.460468	45.345767
3510.749220	512948.595188	45.350772
3510.588607	512749.251228	45.355777
3510.713963	512546.925402	45.360781
3510.572696	512347.370923	45.365786
3510.598792	512155.819152	45.370791
3510.756095	511953.480221	45.375796
3510.418977	511765.219482	45.380801
3510.872352	511557.014130	45.385805
3510.806899	511352.128514	45.390810
3510.526507	511161.627561	45.395815
3510.954270	510953.317546	45.400820
3510.523681	510756.925218	45.405825
3510.781369	510561.726769	45.410829
3510.485609	510366.064545	45.415834
3510.516040	510162.713640	45.420839
3510.561043	509967.038833	45.425844
3510.125054	509781.449622	45.430849
3510.148071	509582.792273	45.435853
3510.295750	509391.438876	45.440858
3510.349928	509205.405483	45.445863
3510.648964	509016.548560	45.450868
3510.335503	508826.783217	45.455873
3510.278537	508634.545974	45.460877
3509.858351	508448.230952	45.465882
3510.231200	508250.204778	45.470887
3510.049773	508068.999601	45.475892
3509.716682	507889.688272	45.480897
3510.089227	507705.200315	45.485901
3510.032576	507532.104902	45.490906
3509.692563	507348.896963	45.495911
3509.850390	507167.017130	45.500916
3510.017386	506994.787500	45.505921
3510.144569	506807.349025	45.510925
3510.396871	506623.576767	45.515930
3510.014319	506439.102078	45.520935
3509.893477	506261.252647	45.525940
3509.784989	506078.091760	45.530945
3509.818075	505891.972888	45.535949
3510.225565	505712.409681	45.540954
3509.980982	505538.617208	45.545959
3510.074628	505354.908109	45.550964
3509.780675	505186.276243	45.555969
3510.018621	504999.404409	45.560973
3509.766772	504820.601013	45.565978
3509.945016	504640.155126	45.570983
3510.235882	504456.806562	45.575988
3509.640503	504286.144166	45.580993
3509.688490	504106.877282	45.585997
3509.812342	503934.622359	45.591002
3509.521027	503759.706594	45.596007
3509.624036	503585.682151	45.601012
3509.531512	503411.032019	45.606017
3509.692779	503231.786699	45.611021
3509.786098	503062.308300	45.616026
3509.798777	502889.454627	45.621031
3509.495292	502717.613687	45.626036
3509.336227	502550.599799	45.631041
3509.651824	502377.840662	45.636045
3509.670786	502214.433118	45.641050
3509.540622	502039.269149	45.646055
3509.511201	501858.271749	45.651060
3509.684414	501689.372190	45.656065
3509.766928	501527.109823	45.661069
3509.319057	501359.223001	45.666074
3509.211626	501184.602192	45.671079
3509.428094	501019.480482	45.676084
3509.243851	500869.038150	45.681089
3509.225949	500696.419377	45.686093
3509.378317	500532.618371	45.691098
3509.277004	500376.848193	45.696103
3509.995177	500206.525692	45.701108
3509.393450	500044.517229	45.706113
3509.572104	499860.832934	45.711117
3509.466886	499702.478206	45.716122
3509.398620	499535.873274	45.721127
3509.479457	499367.977026	45.726132
3509.440944	499205.661907	45.731137
3509.285404	499040.179380	45.736141
3509.313628	498878.759895	45.741146
3509.130649	498703.518922	45.746151
3509.028142	498550.867054	45.751156
3508.946748	498385.517049	45.756161
3509.068613	498222.810946	45.761165
3509.189708	498076.640171	45.766170
3509.010086	497916.258252	45.771175
3509.336334	497753.512668	45.776180
3508.992629	497601.753005	45.781185
3509.049288	497444.006549	45.786189
3509.022543	497286.424565	45.791194
3508.992085	497127.273932	45.796199
3508.895586	496968.790529	45.801204
3508.746068	496813.804354	45.806209
3508.789901	496669.606881	45.811213
3509.046622	496522.944176	45.816218
3508.394167	496369.152429	45.821223
3509.020714	496213.724739	45.826228
3508.862967	496067.938053	45.831233
3508.918731	495907.951883	45.836237
3508.884930	495757.791656	45.841242
3508.559556	495604.746310	45.846247
3509.024641	495459.202053	45.851252
3508.738050	495310.497211	45.856257
3508.991551	495161.193040	45.861261
3508.752019	495014.753654	45.866266
3508.635623	494867.128611	45.871271
3508.891235	494708.412030	45.876276
3508.711477	494560.339893	45.881281
3508.861956	494415.093259	45.886285
3508.811760	494265.580117	45.891290
3508.355656	494119.018196	45.896295
3508.494962	493974.680188	45.901300
3508.277409	493835.156775	45.906305
3508.272960	493688.261092	45.911309
3508.412519	493552.367039	45.916314
3508.422525	493411.688424	45.921319
3508.517955	493258.954673	45.926324
3508.607484	493126.606755	45.931329
3508.697627	492976.653606	45.936333
3508.716263	492833.034714	45.941338
3508.878709	492690.907678	45.946343
3509.051867	492534.511867	45.951348
3508.880339	492386.722894	45.956353
3509.150009	492241.690278	45.961357
3508.882300	492083.999719	45.966362
3508.796107	491944.236021	45.971367
3508.766653	491796.974173	45.976372
3508.789134	491656.683669	45.981377
3508.738120	491504.161578	45.986381
3508.676584	491355.484866	45.991386
3508.106009	491208.107981	45.996391
3508.598773	491066.062819	46.001396
3507.982565	490931.592346	46.006401
3508.133243	490787.023064	46.011405
3508.094366	490653.058951	46.016410
3508.110396	490525.813391	46.021415
3508.010191	490388.973849	46.026420
3508.183670	490260.535779	46.031425
3507.968626	490122.448863	46.036429
3508.032653	489986.235815	46.041434
3508.264206	489857.430659	46.046439
3508.225536	489718.247883	46.051444
3507.956741	489589.020194	46.056449
3508.240051	489453.069078	46.061453
3508.227171	489329.412008	46.066458
3508.292251	489201.085761	46.071463
3508.273514	489055.569540	46.076468
3508.095207	488928.193592	46.081473
3508.268500	488789.574334	46.086477
3508.187561	488657.221082	46.091482
3508.057461	488526.443803	46.096487
3508.333503	488382.541390	46.101492
3507.806884	488263.063032	46.106497
3507.885108	488132.803823	46.111501
3508.045361	488005.768105	46.116506
3507.776697	487875.363792	46.121511
3508.017651	487751.601537	46.126516
3507.589837	487625.624889	46.131521
3507.863519	487491.835958	46.136525
3507.657882	487372.195472	46.141530
3507.564090	487251.472398	46.146535
3507.832552	487115.454928	46.151540
3507.815868	487003.775038	46.156545
3507.613400	486877.046051	46.161549
3507.808334	486759.255939	46.166554
3507.632467	486643.552548	46.171559
3507.713313	486523.705522	46.176564
3507.708834	486403.669822	46.181569
3507.472796	486270.262211	46.186573
3507.738951	486156.048919	46.191578
3507.610958	486025.353748	46.196583
3507.881808	485903.698803	46.201588
3507.370390	485789.970146	46.206593
3507.786323	485674.412353	46.211597
3507.488618	485557.609229	46.216602
3507.354090	485442.700592	46.221607
3507.624911	485324.685462	46.226612
3507.666604	485208.581205	46.231617
3507.470979	485091.757559	46.236621
3507.732736	484974.399556	46.241626
3507.546724	484844.970769	46.246631
3507.634389	484728.197567	46.251636
3507.608166	484605.470948	46.256641
3507.472490	484484.128670	46.261645
3507.688389	484368.900148	46.266650
3507.413492	484258.410974	46.271655
3507.419315	484138.459298	46.276660
3507.129865	484026.807080	46.281665
3507.436069	483904.221287	46.286669
3507.535701	483797.106966	46.291674
3507.176448	483681.364815	46.296679
3507.308248	483563.108598	46.301684
3507.316145	483456.362180	46.306689
3507.307062	483341.013548	46.311693
3507.412852	483230.452967	46.316698
3507.186373	483122.782881	46.321703
3507.383939	483006.232645	46.326708
3507.484242	482898.100479	46.331713
3507.486711	482792.059622	46.336717
3507.364527	482669.892775	46.341722
3507.458390	482565.960858	46.346727
3507.452234	482446.505974	46.351732
3507.253946	482330.778166	46.356737
3507.423487	482219.744872	46.361741
3507.438145	482109.294131	46.366746
3507.260785	481999.128586	46.371751
3507.377208	481891.746845	46.376756
3507.127225	481785.034449	46.381761
3507.243785	481661.098891	46.386765
3507.433505	481564.282105	46.391770
3507.100646	481459.556083	46.396775
3507.109820	481347.279260	46.401780
3507.343653	481233.647241	46.406785
3507.139860	481129.859045	46.411789
3507.502683	481022.834994	46.416794
3507.391291	480918.321102	46.421799
3507.477908	480806.078293	46.426804
3507.264717	480699.201287	46.431809
3507.371345	480581.486479	46.436813
3507.451731	480482.607013	46.441818
3506.802824	480374.182547	46.446823
3507.055553	480260.034920	46.451828
3507.016093	480159.655447	46.456833
3507.083984	480048.322334	46.461837
3507.177381	479950.652701	46.466842
3507.101893	479844.050854	46.471847
3507.606840	479735.830529	46.476852
3507.572962	479626.992807	46.481857
3507.326750	479510.647507	46.486861
3507.581183	479418.111286	46.491866
3507.054691	479306.318207	46.496871
3507.549804	479192.071822	46.501876
3507.434221	479091.294401	46.506881
3507.159275	478979.253845	46.511885
3507.476671	478864.225709	46.516890
3507.326672	478768.515087	46.521895
3507.218111	478645.002251	46.526900
3506.987308	478540.292473	46.531905
3506.849103	478439.464665	46.536909
3506.863456	478334.053671	46.541914
3506.336634	478239.113398	46.546919
3506.785856	478146.334918	46.551924
3506.764445	478058.496749	46.556929
3506.841968	477951.857648	46.561933
3506.684697	477857.358582	46.566938
3506.535522	477756.478231	46.571943
3506.765381	477670.114194	46.576948
3506.775595	477574.572454	46.581953
3506.676320	477473.935175	46.586957
3506.742687	477375.699361	46.591962
3506.352922	477280.376269	46.596967
3506.663403	477183.667321	46.601972
3506.527271	477096.046632	46.606977
3506.519978	477007.087084	46.611981
3506.635850	476908.384615	46.616986
3506.425343	476818.699360	46.621991
3506.666952	476722.050365	46.626996
3506.666384	476648.075323	46.632001
3506.653005	476550.355027	46.637005
3506.955342	476445.390293	46.642010
3506.209160	476358.174039	46.647015
3506.643816	476271.768435	46.652020
3506.107266	476183.401600	46.657025
3506.119932	476093.624056	46.662029
3506.718825	476004.556141	46.667034
3507.007311	475920.249883	46.672039
3506.832029	475820.021577	46.677044
3506.506015	475724.882050	46.682049
3506.361750	475630.622449	46.687053
3506.475609	475549.028021	46.692058
3506.143821	475468.522055	46.697063
3506.622969	475374.205334	46.702068
3506.586537	475287.875549	46.707073
3506.310851	475201.484936	46.712077
3506.603553	475113.730930	46.717082
3506.305806	475023.494796	46.722087
3506.421905	474931.313950	46.727092
3506.586945	474853.252371	46.732097
3506.225441	474762.519464	46.737101
3506.353280	474677.070268	46.742106
3506.201943	474595.162434	46.747111
3506.520605	474500.767380	46.752116
3506.347667	474416.279842	46.757121
3506.328998	474330.499585	46.762125
3506.443031	474247.987868	46.767130
3506.304628	474165.772086	46.772135
3506.284341	474070.673113	46.777140
3506.118839	474005.324495	46.782145
3505.878409	473916.845596	46.787149
3506.457711	473840.126958	46.792154
3506.149674	473761.888351	46.797159
3506.446190	473668.353744	46.802164
3506.458465	473579.171750	46.807169
3506.349288	473502.366705	46.812173
3506.235596	473422.270374	46.817178
3506.220079	473341.194729	46.822183
3506.552490	473254.083495	46.827188
3506.412935	473170.344225	46.832193
3506.362025	473086.336228	46.837197
3506.315532	473002.175168	46.842202
3506.056850	472931.217275	46.847207
3506.465578	472849.763193	46.852212
3506.476591	472761.185222	46.857217
3505.955217	472683.181081	46.862221
3506.647989	472597.018133	46.867226
3506.353944	472516.543548	46.872231
3506.401989	472424.817690	46.877236
3506.054932	472342.933352	46.882241
3506.121027	472261.130047	46.887245
3506.336806	472185.631519	46.892250
3505.670007	472107.295284	46.897255
3506.160754	472029.723349	46.902260
3505.978300	471955.406100	46.907265
3506.156015	471883.964548	46.912269
3505.959736	471802.153391	46.917274
3505.836518	471729.952289	46.922279
3506.095172	471644.416199	46.927284
3505.806408	471575.230940	46.932289
3505.959143	471496.195098	46.937293
3506.039701	471413.727209	46.942298
3505.583038	471354.395439	46.947303
3505.553082	471281.467618	46.952308
3505.923826	471215.713785	46.957313
3505.766457	471138.046237	46.962317
3505.684860	471065.227692	46.967322
3505.630340	470991.593862	46.972327
3506.034853	470921.426793	46.977332
3505.845002	470853.741456	46.982337
3505.514788	470789.169450	46.987341
3505.637815	470709.375635	46.992346
3505.859032	470643.290788	46.997351
3505.762351	470569.459908	47.002356
3505.693284	470501.195533	47.007361
3505.465589	470433.312547	47.012365
3505.442873	470364.128057	47.017370
3505.283622	470309.908554	47.022375
3505.588553	470236.311701	47.027380
3505.597209	470188.901035	47.032385
3505.526514	470128.334526	47.037389
3505.900849	470054.522511	47.042394
3505.459142	469989.207033	47.047399
3505.524191	469915.852497	47.052404
3505.734856	469855.946197	47.057409
3505.321754	469790.118629	47.062413
3505.726167	469716.502768	47.067418
3505.695917	469661.347640	47.072423
3505.897140	469590.247946	47.077428
3505.399905	469536.489154	47.082433
3505.606820	469465.590631	47.087437
3506.026468	469393.085277	47.092442
3505.989405	469336.157509	47.097447
3505.592531	469261.106448	47.102452
3505.587202	469194.346076	47.107457
3505.802304	469126.737372	47.112461
3505.873951	469055.809762	47.117466
3505.543919	468996.195684	47.122471
3505.448431	468931.020058	47.127476
3505.460297	468868.611872	47.132481
3505.654297	468801.917395	47.137485
3505.693046	468741.277113	47.142490
3505.414168	468683.274272	47.147495
3505.355002	468614.393548	47.152500
3505.575714	468553.974875	47.157505
3505.572947	468490.200254	47.162509
3505.690993	468425.796924	47.167514
3505.268975	468364.980839	47.172519
3505.503830	468297.517784	47.177524
3505.647168	468231.083240	47.182529
3505.354811	468184.022901	47.187533
3505.556422	468119.199017	47.192538
3505.417431	468060.765144	47.197543
3505.539953	467998.081929	47.202548
3505.569984	467934.958390	47.207553
3505.433396	467863.403355	47.212557
3505.858107	467805.125736	47.217562
3505.463064	467751.496418	47.222567
3505.490051	467682.850907	47.227572
3505.524064	467623.828924	47.232577
3505.350373	467556.838274	47.237581
3505.672500	467498.374605	47.242586
3505.318716	467453.501250	47.247591
3505.231831	467391.966285	47.252596
3505.253487	467334.667904	47.257601
3505.313545	467275.741718	47.262605
3505.233015	467218.308461	47.267610
3504.923341	467165.777417	47.272615
3505.431822	467105.457008	47.277620
3505.402104	467051.459395	47.282625
3505.340719	466996.403189	47.287629
3505.253865	466939.071494	47.292634
3504.997130	466885.770751	47.297639
3505.301195	466831.462228	47.302644
3505.196427	466774.791679	47.307649
3505.104109	466721.817027	47.312653
3505.310359	466666.308896	47.317658
3505.183701	466619.267075	47.322663
3505.172495	466557.817833	47.327668
3505.362795	466498.360417	47.332673
3505.264732	466452.782467	47.337677
3505.161208	466400.112807	47.342682
3505.178886	466345.243879	47.347687
3505.423468	466278.734620	47.352692
3505.312597	466235.235454	47.357697
3505.466332	466175.276670	47.362701
3506.044540	466116.866398	47.367706
3505.580254	466062.230943	47.372711
3505.920067	465999.200127	47.377716
3505.476598	465927.082327	47.382721
3505.501812	465872.565402	47.387725
3505.707347	465814.217847	47.392730
3505.702569	465759.047110	47.397735
3505.731496	465691.711384	47.402740
3505.715178	465623.623204	47.407745
3505.544018	465569.797574	47.412749
3505.821962	465497.200346	47.417754
3505.697988	465444.784884	47.422759
3505.797039	465379.411973	47.427764
3505.956655	465315.447086	47.432769
3505.726212	465256.311003	47.437773
3505.781648	465182.483988	47.442778
3505.488845	465126.296677	47.447783
3505.677346	465061.718048	47.452788
3505.312900	464991.812498	47.457793
3505.287542	464953.767629	47.462797
3505.588429	464884.001412	47.467802
3505.141165	464832.348801	47.472807
3505.172992	464776.966353	47.477812
3505.238195	464729.532511	47.482817
3505.301590	464681.896199	47.487821
3505.424468	464625.535129	47.492826
3505.096009	464573.354886	47.497831
3505.214427	464516.234273	47.502836
3505.302079	464463.881355	47.507841
3504.958548	464415.249883	47.512845
3505.209410	464354.914213	47.517850
3504.890499	464298.728961	47.522855
3504.973225	464249.264294	47.527860
3504.960320	464210.658509	47.532865
3504.965085	464159.990927	47.537869
3504.902908	464101.886596	47.542874
3504.993974	464074.764192	47.547879
3505.025051	464023.787760	47.552884
3505.013926	463973.983748	47.557889
3505.080136	463927.966463	47.562893
3505.161924	463873.383590	47.567898
3504.798213	463827.540810	47.572903
3505.074576	463780.220601	47.577908
3505.199753	463725.933913	47.582913
3504.882629	463678.157444	47.587917
3504.788605	463632.673503	47.592922
3504.788198	463594.419040	47.597927
3504.956307	463535.564344	47.602932
3505.234462	463491.739253	47.607937
3504.847443	463446.558248	47.612941
3505.346192	463398.033761	47.617946
3504.756801	463355.116526	47.622951
3504.876464	463308.531295	47.627956
3504.761443	463269.687737	47.632961
3504.837743	463227.669941	47.637965
3504.866862	463173.448788	47.642970
3504.435463	463137.648482	47.647975
3504.665525	463077.768439	47.652980
3505.145246	463043.687168	47.657985
3504.686879	463010.171371	47.662989
3504.880604	462960.887166	47.667994
3504.979267	462921.601071	47.672999
3504.865520	462883.769930	47.678004
3504.894649	462837.705738	47.683009
3504.798706	462787.609162	47.688013
3504.942539	462747.554949	47.693018
3504.457560	462698.132616	47.698023
3504.565329	462656.817610	47.703028
3504.725753	462618.432435	47.708033
3504.598172	462578.677575	47.713037
3504.560362	462541.846226	47.718042
3504.527913	462505.064564	47.723047
3504.871002	462471.715025	47.728052
3505.069170	462427.141142	47.733057
3504.810296	462386.242869	47.738061
3504.551047	462330.548478	47.743066
3504.587752	462290.004907	47.748071
3505.145159	462258.847968	47.753076
3505.074301	462198.205873	47.758081
3504.734029	462176.677726	47.763085
3504.451109	462128.080877	47.768090
3504.837778	462096.699474	47.773095
3504.449006	462047.968485	47.778100
3504.756946	462002.817501	47.783105
3504.396238	461978.911022	47.788109
3504.666612	461927.584236	47.793114
3504.460834	461901.370940	47.798119
3504.748221	461863.824049	47.803124
3504.880450	461824.023299	47.808129
3504.240710	461790.384364	47.813133
3504.751271	461749.454733	47.818138
3504.769959	461713.980359	47.823143
3505.030127	461682.366529	47.828148
3505.336590	461634.225232	47.833153
3504.902615	461586.311590	47.838157
3504.959143	461535.020295	47.843162
3504.890872	461505.438533	47.848167
3505.201055	461446.756009	47.853172
3505.310245	461407.211721	47.858177
3504.767357	461364.130161	47.863181
3504.740277	461315.943690	47.868186
3504.723746	461273.025428	47.873191
3504.592464	461247.051913	47.878196
3504.815073	461197.809032	47.883201
3504.518631	461165.123900	47.888205
3504.521004	461122.658155	47.893210
3504.556445	461086.318321	47.898215
3504.604860	461061.378050	47.903220
3504.689176	461013.425194	47.908225
3504.703049	460981.649598	47.913229
3504.787265	460943.983623	47.918234
3504.463081	460902.333290	47.923239
3504.263108	460870.594028	47.928244
3504.547324	460846.677406	47.933249
3504.493834	460798.950261	47.938253
3504.742853	460762.978770	47.943258
3504.482253	460732.871259	47.948263
3504.566265	460689.630508	47.953268
3504.434057	460663.098950	47.958273
3504.488607	460632.785447	47.963277
3504.515007	460588.895527	47.968282
3504.619858	460564.097021	47.973287
3504.590150	460517.277306	47.978292
3504.764904	460484.966680	47.983297
3504.549135	460458.854526	47.988301
3505.030099	460415.038635	47.993306
3504.976639	460378.053886	47.998311
3504.980423	460329.200946	48.003316
3504.900527	460294.348977	48.008321
3504.511095	460252.505709	48.013325
3504.903549	460215.951289	48.018330
3504.835005	460175.015930	48.023335
3504.729399	460136.620675	48.028340
3504.878169	460098.891395	48.033345
3504.723305	460062.227436	48.038349
3504.786905	460028.009304	48.043354
3504.719821	459977.343208	48.048359
3504.726972	459952.155198	48.053364
3504.472549	459908.767821	48.058369
3504.359879	459872.248340	48.063373
3504.480279	459848.409165	48.068378
3504.721989	459813.704151	48.073383
3504.265814	459771.972621	48.078388
3504.490015	459743.199815	48.083393
3504.483613	459713.047351	48.088397
3504.503085	459667.230800	48.093402
3504.518433	459636.162294	48.098407
3504.426514	459606.125626	48.103412
3504.447193	459567.961103	48.108417
3504.288010	459542.091473	48.113421
3504.309291	459526.225395	48.118426
3504.436863	459488.904008	48.123431
3504.273304	459448.743559	48.128436
3504.651398	459425.772099	48.133441
3504.491775	459391.743025	48.138445
3504.552622	459350.581159	48.143450
3504.556454	459328.788433	48.148455
3504.485139	459287.801042	48.153460
3504.452360	459244.982525	48.158465
3504.707674	459224.971208	48.163469
3504.760115	459181.833927	48.168474
3504.716311	459149.507771	48.173479
3504.639673	459120.836114	48.178484
3504.648213	459083.737013	48.183489
3504.466441	459057.769251	48.188493
3504.568145	459021.718405	48.193498
3504.465380	458976.732020	48.198503
3503.987394	458952.031022	48.203508
3504.384276	458935.897621	48.208513
3504.327221	458904.688296	48.213517
3504.517318	458858.283270	48.218522
3504.421345	458842.233946	48.223527
3504.489966	458809.888044	48.228532
3504.591651	458764.714230	48.233537
3504.586969	458746.013845	48.238541
3504.234708	458713.891694	48.243546
3504.229562	458678.568005	48.248551
3504.183702	458659.165037	48.253556
3504.238268	458645.826624	48.258561
3504.113096	458633.481831	48.263565
3504.246910	458592.914117	48.268570
3504.046475	458558.282416	48.273575
3504.050216	458531.724801	48.278580
3504.087590	458507.492750	48.283585
3503.754675	458503.596452	48.288589
3503.851723	458475.907840	48.293594
3504.233637	458458.915027	48.298599
3504.032655	458424.131142	48.303604
3504.528112	458386.136702	48.308609
3504.120613	458370.038828	48.313613
3503.922026	458344.377100	48.318618
3503.979800	458339.907242	48.323623
3503.785933	458306.439664	48.328628
3504.216012	458270.736852	48.333633
3503.960280	458247.314762	48.338637
3504.162839	458224.523943	48.343642
3503.943010	458214.374383	48.348647
3503.879907	458194.619134	48.353652
3503.836894	458176.786358	48.358657
3503.904548	458161.924923	48.363661
3503.994949	458135.808126	48.368666
3503.935676	458106.980003	48.373671
3504.085881	458090.938725	48.378676
3504.016014	458066.065581	48.383681
3503.981869	458057.354027	48.388685
3504.160073	458032.235753	48.393690
3504.418185	458013.540496	48.398695
3503.897090	457970.143754	48.403700
3503.891281	457944.651328	48.408705
3504.061605	457931.799503	48.413709
3504.078168	457913.601541	48.418714
3504.001265	457901.349420	48.423719
3504.188027	457884.186712	48.428724
3504.292336	457845.497792	48.433729
3503.749814	457824.759694	48.438733
3504.146847	457801.529725	48.443738
3504.391152	457788.715859	48.448743
3503.885201	457780.236794	48.453748
3504.416337	457750.293685	48.458753
3504.060174	457715.585751	48.463757
3504.307531	457686.704669	48.468762
3504.097834	457671.991594	48.473767
3503.966712	457654.933651	48.478772
3504.382912	457629.470136	48.483777
3504.089720	457599.059351	48.488781
3503.839257	457574.520535	48.493786
3503.793955	457559.829992	48.498791
3504.012601	457543.067019	48.503796
3504.103802	457529.468190	48.508801
3504.050672	457513.562538	48.513805
3503.986968	457471.505766	48.518810
3503.903292	457440.095971	48.523815
3504.006607	457427.103213	48.528820
3504.401312	457404.785497	48.533825
3503.873430	457397.171644	48.538829
3504.126809	457378.780711	48.543834
3504.010420	457356.398156	48.548839
3504.049266	457320.456354	48.553844
3504.040628	457296.636173	48.558849
3503.886524	457284.650281	48.563853
3504.244963	457264.974194	48.568858
3504.095165	457254.964243	48.573863
3503.782507	457233.780808	48.578868
3503.855248	457194.538497	48.583873
3503.656107	457180.178052	48.588877
3504.213427	457164.826793	48.593882
3503.950429	457144.243002	48.598887
3504.110452	457133.267764	48.603892
3504.114612	457122.420502	48.608897
3504.012949	457106.168021	48.613901
3503.931270	457080.231290	48.618906
3504.025235	457058.522077	48.623911
3503.725760	457026.844374	48.628916
3504.039282	457007.226390	48.633921
3504.102120	456996.064931	48.638925
3504.064871	456977.672570	48.643930
3504.166250	456966.960681	48.648935
3504.043304	456954.513104	48.653940
3504.199370	456912.265585	48.658945
3504.180851	456882.820524	48.663949
3504.177345	456868.223711	48.668954
3504.376253	456855.214263	48.673959
3503.832344	456833.309609	48.678964
3504.141107	456783.635653	48.683969
3503.963376	456779.661832	48.688973
3503.907748	456761.982013	48.693978
3504.042060	456737.984707	48.698983
3503.714778	456723.595131	48.703988
3504.026496	456725.670715	48.708993
3503.801497	456714.203446	48.713997
3503.932934	456693.906647	48.719002
3503.935765	456673.631787	48.724007
3503.872853	456642.470633	48.729012
3504.092353	456614.606494	48.734017
3503.699589	456603.319866	48.739021
3503.592453	456592.744753	48.744026
3503.913937	456580.677237	48.749031
3503.480014	456574.871730	48.754036
3503.792426	456551.705459	48.759041
3503.470829	456551.912433	48.764045
3503.753342	456532.856833	48.769050
3503.685134	456518.220128	48.774055
3503.569288	456513.323334	48.779060
3504.014430	456498.598963	48.784065
3503.654900	456493.186221	48.789069
3503.582884	456473.532177	48.794074
3503.744179	456463.570088	48.799079
3503.650057	456452.891307	48.804084
3503.598572	456443.320345	48.809089
3503.740763	456426.670873	48.814093
3503.870551	456417.373067	48.819098
3503.958347	456407.626247	48.824103
3503.699275	456401.689461	48.829108
3504.215029	456383.607630	48.834113
3503.880185	456351.580098	48.839117
3503.848634	456329.131231	48.844122
3504.131498	456325.889665	48.849127
3504.031699	456308.774547	48.854132
3504.013679	456292.304381	48.859137
3503.611068	456281.880931	48.864141
3504.196656	456269.464013	48.869146
3503.976930	456246.084131	48.874151
3503.485490	456224.778101	48.879156
3503.791020	456190.461427	48.884161
3503.873302	456181.222311	48.889165
3503.787384	456169.883046	48.894170
3503.816784	456160.348827	48.899175
3503.638411	456145.578600	48.904180
3503.789120	456131.715233	48.909185
3503.525536	456125.424325	48.914189
3503.922218	456108.933889	48.919194
3503.780971	456092.180476	48.924199
3503.666449	456094.430281	48.929204
3503.809027	456076.868082	48.934209
3503.677311	456072.480765	48.939213
3503.790368	456056.494901	48.944218
3503.905606	456048.973474	48.949223
3503.584181	456048.268047	48.954228
3503.870721	456033.570419	48.959233
3503.756645	456026.645701	48.964237
3503.797269	456009.911854	48.969242
3503.858316	456001.791410	48.974247
3503.848352	455980.960477	48.979252
3504.076609	455951.269173	48.984257
3503.966471	455933.800689	48.989261
3503.793540	455916.342911	48.994266
3503.844773	455902.496373	48.999271
3503.731953	455893.341127	49.004276
3503.928989	455879.571053	49.009281
3503.844062	455872.286489	49.014285
3503.959525	455859.848219	49.019290
3504.054377	455856.081113	49.024295
3503.589031	455831.526179	49.029300
3504.016567	455809.150412	49.034305
3503.536593	455778.971527	49.039309
3503.822423	455766.656174	49.044314
3503.829668	455756.365224	49.049319
3503.524471	455740.551903	49.054324
3503.693488	455726.735822	49.059329
3503.638483	455730.344090	49.064333
3503.589994	455709.367390	49.069338
3503.866854	455695.279432	49.074343
3503.642202	455690.806524	49.079348
3503.842322	455677.593360	49.084353
3503.448476	455677.103038	49.089357
3503.480159	455665.743411	49.094362
3503.669448	455650.960736	49.099367
3503.448362	455650.238161	49.104372
3503.964858	455632.662421	49.109377
3503.517379	455626.149314	49.114381
3503.602801	455616.402519	49.119386
3504.104091	455602.580308	49.124391
3503.874380	455600.541299	49.129396
3504.034624	455585.307337	49.134401
3504.049770	455581.351035	49.139405
3504.094954	455568.823209	49.144410
3503.992778	455549.426862	49.149415
3503.675844	455520.993861	49.154420
3503.768215	455502.679406	49.159425
3503.448276	455497.107569	49.164429
3503.711019	455481.197072	49.169434
3503.852726	455468.551325	49.174439
3503.483139	455466.282740	49.179444
3503.544889	455457.097490	49.184449
3503.652379	455445.623418	49.189453
3503.603833	455435.848722	49.194458
3503.601920	455421.453351	49.199463
3503.321377	455417.648884	49.204468
3503.655351	455416.730147	49.209473
3503.533388	455416.852354	49.214477
3503.274714	455421.103722	49.219482
3503.555471	455410.917963	49.224487
3503.318365	455417.142525	49.229492
3503.467580	455399.984121	49.234497
3503.682977	455388.795727	49.239501
3503.933576	455384.748496	49.244506
3503.498812	455374.989027	49.249511
3503.799064	455379.398415	49.254516
3503.915468	455361.282485	49.259521
3503.568164	455351.406693	49.264525
3503.435824	455342.406599	49.269530
3503.475091	455334.593743	49.274535
3503.638169	455326.506297	49.279540
3503.673831	455309.772721	49.284545
3503.248230	455312.937447	49.289549
3503.448424	455298.304722	49.294554
3503.616906	455288.239451	49.299559
3503.352185	455280.731927	49.304564
3503.690911	455266.075524	49.309569
3503.714600	455256.693924	49.314573
3503.114857	455248.128422	49.319578
3503.954560	455250.164700	49.324583
3503.140551	455246.856804	49.329588
3503.451625	455228.656828	49.334593
3503.553892	455225.750063	49.339597
3503.430312	455214.264626	49.344602
3503.512699	455229.710892	49.349607
3503.345294	455241.803597	49.354612
3503.399014	455231.707204	49.359617
3503.451722	455228.048558	49.364621
3503.428392	455217.661176	49.369626
3503.833239	455207.758266	49.374631
3503.395118	455208.644111	49.379636
3503.769864	455193.677369	49.384641
3503.786831	455190.886543	49.389645
3503.702967	455180.357410	49.394650
3503.732775	455168.896446	49.399655
3503.506006	455169.594137	49.404660
3504.193925	455156.753552	49.409665
3504.125199	455152.710109	49.414669
3503.410318	455123.432084	49.419674
3503.391877	455121.002123	49.424679
3503.558845	455124.673977	49.429684
3503.661910	455118.269461	49.434689
3503.382670	455122.625781	49.439693
3503.528076	455097.509465	49.444698
3503.790365	455095.690536	49.449703
3503.638206	455086.643023	49.454708
3504.135501	455068.411107	49.459713
3504.049724	455071.568536	49.464717
3503.516550	455032.425495	49.469722
3503.716251	455023.115114	49.474727
3503.529819	455010.423732	49.479732
3503.612819	454993.884573	49.484737
3503.476344	454995.073754	49.489741
3503.668232	455000.870362	49.494746
3503.787186	454977.583260	49.499751
3503.121661	454979.116225	49.504756
3503.372028	454981.303849	49.509761
3503.174964	454992.894864	49.514765
3503.719739	454985.755913	49.519770
3503.764288	454983.670012	49.524775
3503.653503	454972.739846	49.529780
3503.673949	454964.676611	49.534785
3503.661270	454958.748020	49.539789
3503.514559	454949.293993	49.544794
3503.766381	454936.527734	49.549799
3503.345322	454937.714819	49.554804
3503.739401	454926.799805	49.559809
3503.694632	454918.494235	49.564813
3503.685526	454908.459100	49.569818
3503.932820	454901.573675	49.574823
3503.409424	454894.363628	49.579828
3503.755266	454886.903777	49.584833
3503.506172	454884.158338	49.589837
3503.104795	454876.775379	49.594842
3503.518679	454862.004473	49.599847
3503.328739	454866.396291	49.604852
3503.575845	454847.699993	49.609857
3503.941665	454838.411854	49.614861
3503.450132	454835.555733	49.619866
3503.534960	454828.343191	49.624871
3503.552660	454828.036029	49.629876
3503.865518	454821.190073	49.634881
3503.597759	454810.438695	49.639885
3503.665920	454803.634514	49.644890
3503.632330	454793.755575	49.649895
3503.084447	454793.899819	49.654900
3503.359777	454780.166325	49.659905
3503.582568	454780.331050	49.664909
3503.211741	454787.136234	49.669914
3503.175711	454786.838245	49.674919
3503.420432	454792.676583	49.679924
3503.448049	454781.266466	49.684929
3503.233109	454786.270858	49.689933
3503.261308	454784.441182	49.694938
3503.169273	454778.120563	49.699943
3503.147665	454781.469842	49.704948
3503.369119	454796.081641	49.709953
3503.420290	454800.635067	49.714957
3503.094626	454794.911941	49.719962
3503.029518	454794.213392	49.724967
3503.029734	454788.688075	49.729972
3503.308004	454800.248728	49.734977
3503.450716	454798.500882	49.739981
3503.127095	454808.643581	49.744986
3503.395928	454792.984961	49.749991
3503.028434	454797.356420	49.754996
3503.383267	454787.715300	49.760001
3503.504989	454787.694520	49.765005
3502.884469	454778.574768	49.770010
3503.446526	454790.036281	49.775015
3502.691561	454799.593657	49.780020
3503.206319	454793.473578	49.785025
3503.465985	454785.166663	49.790029
3503.051368	454789.343407	49.795034
3503.778768	454787.292963	49.800039
3503.093630	454797.294634	49.805044
3502.992108	454808.615986	49.810049
3503.335125	454798.571364	49.815053
3503.231763	454796.662771	49.820058
3503.011164	454791.935518	49.825063
3503.195901	454790.586021	49.830068
3503.315856	454805.012381	49.835073
3502.980379	454809.581133	49.840077
3502.746763	454821.634702	49.845082
3503.088023	454804.443006	49.850087
3503.024052	454815.098965	49.855092
3502.817472	454827.705511	49.860097
3503.498408	454829.363417	49.865101
3503.155092	454825.214722	49.870106
3503.279408	454817.995434	49.875111
3503.432818	454820.959989	49.880116
3503.196941	454836.765039	49.885121
3503.492231	454847.055495	49.890125
3503.405223	454850.770764	49.895130
3503.646679	454842.923197	49.900135
3503.750861	454838.748787	49.905140
3503.819055	454831.893920	49.910145
3503.263150	454823.270061	49.915149
3503.758290	454820.397538	49.920154
3503.850778	454805.174563	49.925159
3503.445130	454808.183887	49.930164
3503.879897	454793.155912	49.935169
3503.513001	454790.734719	49.940173
3503.284489	454794.727613	49.945178
3503.447285	454780.202284	49.950183
3502.984124	454783.069359	49.955188
3502.864409	454775.536888	49.960193
3503.122434	454782.792297	49.965197
3502.953019	454801.526086	49.970202
3503.216552	454796.513408	49.975207
3503.025174	454803.085183	49.980212
3503.309269	454789.147437	49.985217
3503.369311	454795.625595	49.990221
3502.923853	454816.129987	49.995226
3503.242356	454815.112485	50.000231
3503.036637	454815.299687	50.005236
3503.146585	454809.907711	50.010241
3502.936706	454808.879048	50.015245
3502.849372	454824.202529	50.020250
3503.339296	454831.519705	50.025255
3503.109865	454843.116331	50.030260
3503.347163	454823.914781	50.035265
3503.302567	454820.576819	50.040269
3503.002054	454846.378946	50.045274
3503.623040	454853.876497	50.050279
3503.361864	454854.073168	50.055284
3503.394568	454844.436386	50.060289
3503.407263	454849.097751	50.065293
3503.144241	454846.861591	50.070298
3503.409802	454825.374142	50.075303
3503.614919	454831.067158	50.080308
3503.713657	454823.700168	50.085313
3504.127021	454816.583597	50.090317
3503.781808	454806.808563	50.095322
3503.321803	454812.412390	50.100327
3502.916952	454799.504716	50.105332
3503.253674	454815.668229	50.110337
3503.084780	454833.286707	50.115341
3502.977877	454832.493915	50.120346
3503.199582	454827.437696	50.125351
3503.132854	454831.808483	50.130356
3503.034222	454823.714834	50.135361
3503.406166	454840.125766	50.140365
3502.967409	454845.573885	50.145370
3503.263769	454844.762928	50.150375
3503.292231	454849.725744	50.155380
3503.131989	454834.292490	50.160385
3503.468559	454848.073547	50.165389
3503.076318	454871.306086	50.170394
3503.486669	454859.273067	50.175399
3503.194113	454870.728385	50.180404
3503.140564	454868.861984	50.185409
3503.222964	454865.654417	50.190413
3502.899547	454858.815735	50.195418
3503.240783	454875.333264	50.200423
3503.085025	454891.682187	50.205428
3503.169581	454885.534210	50.210433
3503.488827	454879.143397	50.215437
3503.258402	454883.744886	50.220442
3503.661845	454872.372030	50.225447
3503.516665	454874.982037	50.230452
3503.170860	454870.681705	50.235457
3503.243861	454881.060789	50.240461
3502.927033	454896.930306	50.245466
3503.232452	454896.776779	50.250471
3503.155842	454899.121623	50.255476
3503.061790	454891.280671	50.260481
3503.436051	454899.276547	50.265485
3502.935121	454910.007066	50.270490
3503.205546	454917.108238	50.275495
3503.258713	454917.656757	50.280500
3503.241752	454911.678193	50.285505
3503.315135	454902.845539	50.290509
3503.137348	454910.073935	50.295514
3503.555187	454920.039287	50.300519
3502.945214	454925.668690	50.305524
3502.832208	454914.181277	50.310529
3502.968829	454912.181029	50.315533
3503.348322	454929.249575	50.320538
3503.016947	454936.757638	50.325543
3502.829283	454953.720243	50.330548
3502.820513	454946.118202	50.335553
3502.984883	454948.168442	50.340557
3502.861629	454970.189063	50.345562
3502.925518	454970.837131	50.350567
3503.201278	454970.181767	50.355572
3502.965464	454967.586143	50.360577
3503.307809	454994.190740	50.365581
3502.844213	455004.255863	50.370586
3503.344905	454999.506881	50.375591
3503.252550	455000.536457	50.380596
3502.877100	454993.098423	50.385601
3502.982055	455003.117158	50.390605
3502.939679	455026.492543	50.395610
3503.187189	455016.008123	50.400615
3503.262989	455027.704598	50.405620
3503.197535	455042.567969	50.410625
3503.528885	455048.239370	50.415629
3503.134000	455059.458605	50.420634
3503.095995	455049.732613	50.425639
3503.238231	455050.012471	50.430644
3502.841440	455048.103314	50.435649
3503.080282	455060.887112	50.440653
3503.038788	455070.829439	50.445658
3503.205780	455069.888510	50.450663
3502.966564	455073.426967	50.455668
3502.925639	455075.968457	50.460673
3502.987255	455099.021863	50.465677
3502.837692	455101.733969	50.470682
3502.929220	455102.022484	50.475687
3503.047429	455123.342743	50.480692
3502.962321	455132.025241	50.485697
3503.300215	455130.396165	50.490701
3502.956882	455129.542375	50.495706
3503.342315	455134.342791	50.500711
3503.243350	455155.193199	50.505716
3503.058843	455152.335390	50.510721
3503.225217	455152.002847	50.515725
3502.931696	455167.209207	50.520730
3502.966588	455158.180477	50.525735
3502.925739	455139.685683	50.530740
3502.965087	455119.656483	50.535745
3503.174145	455088.649262	50.540749
3502.823966	455040.959080	50.545754
3503.319797	454968.387513	50.550759
3502.733604	454901.373623	50.555764
3502.998173	454821.237457	50.560769
3503.247649	454726.048380	50.565773
3502.791300	454622.159128	50.570778
3503.143489	454504.393929	50.575783
3503.254889	454385.655332	50.580788
3502.983904	454238.897962	50.585793
3503.079059	454090.505556	50.590797
3503.059690	453931.587528	50.595802
3503.196374	453748.714416	50.600807
3503.102466	453563.800605	50.605812
3502.965038	453359.831541	50.610817
3503.196970	453150.981385	50.615821
3503.324367	452919.739646	50.620826
3503.299799	452683.705150	50.625831
3503.206641	452439.466835	50.630836
3503.089333	452176.573219	50.635841
3502.967850	451903.334624	50.640845
3502.869406	451621.013461	50.645850
3503.192136	451316.106091	50.650855
3502.514769	451017.195508	50.655860
3502.927140	450695.786240	50.660865
3503.156975	450357.063254	50.665869
3502.726680	450015.608154	50.670874
3502.904986	449654.928435	50.675879
3503.147600	449287.690692	50.680884
3502.785915	448894.588709	50.685889
3503.128204	448497.606928	50.690893
3502.924693	448098.581174	50.695898
3502.939020	447657.169480	50.700903
3502.792386	447224.599457	50.705908
3502.751998	446771.616986	50.710913
3502.740251	446290.931607	50.715917
3502.655372	445814.812006	50.720922
3502.529454	445305.420666	50.725927
3502.808506	444801.577428	50.730932
3502.605401	444278.380457	50.735937
3502.654895	443724.849394	50.740941
3502.482823	443179.152677	50.745946
3502.633637	442592.405340	50.750951
3502.341273	442001.457259	50.755956
3502.380350	441395.067578	50.760961
3502.681575	440763.812190	50.765965
3502.142139	440126.189325	50.770970
3502.274631	439470.120762	50.775975
3501.961767	438797.469767	50.780980
3502.221402	438116.127230	50.785985
3501.973973	437401.215196	50.790989
3501.758355	436678.969274	50.795994
3502.237028	435927.916184	50.800999
3501.678583	435178.232902	50.806004
3501.635285	434401.494638	50.811009
3501.693966	433604.264078	50.816013
3501.365536	432795.705585	50.821018
3501.497010	431960.754699	50.826023
3501.394404	431119.927086	50.831028
3501.177719	430253.207120	50.836033
3501.429898	429357.955048	50.841037
3501.210082	428459.704309	50.846042
3501.433104	427522.009636	50.851047
3501.322939	426586.415770	50.856052
3500.889695	425623.228157	50.861057
3500.951403	424629.562971	50.866061
3500.919017	423628.106357	50.871066
3500.885599	422602.394146	50.876071
3500.721722	421561.888172	50.881076
3500.650772	420499.568027	50.886081
3500.614441	419413.562639	50.891085
3500.347803	418311.733487	50.896090
3500.220038	417182.540587	50.901095
3500.020821	416052.116153	50.906100
3499.788066	414888.183394	50.911105
3500.091919	413713.975144	50.916109
3499.754938	412523.952830	50.921114
3499.725027	411292.610227	50.926119
3499.712830	410061.562347	50.931124
3499.642398	408804.030127	50.936129
3499.303814	407535.081170	50.941133
3499.163428	406243.662706	50.946138
3498.973288	404919.451429	50.951143
3498.941474	403598.857577	50.956148
3498.678951	402250.653568	50.961153
3499.008818	400882.468799	50.966157
3498.710633	399499.412439	50.971162
3498.101002	398083.289277	50.976167
3498.089644	396660.489964	50.981172
3497.987196	395227.981353	50.986177
3497.953363	393763.095713	50.991181
3497.451150	392285.588549	50.996186
3497.500227	390793.150063	51.001191
3497.090282	389288.950149	51.006196
3496.874025	387770.080861	51.011201
3496.871179	386227.896214	51.016205
3496.734479	384675.441014	51.021210
3496.639937	383092.782188	51.026215
3496.084128	381504.404862	51.031220
3495.679077	379897.113026	51.036225
3495.651901	378262.095587	51.041229
3495.345471	376641.359139	51.046234
3495.359228	374977.675873	51.051239
3494.976188	373316.827523	51.056244
3494.759738	371632.021256	51.061249
3494.512899	369929.874318	51.066253
3494.055271	368216.722703	51.071258
3494.187506	366484.367923	51.076263
3494.022141	364747.049231	51.081268
3493.866732	362978.646083	51.086273
3493.664286	361207.015455	51.091277
3493.041307	359410.169790	51.096282
3493.273606	357596.512102	51.101287
3493.281750	355780.674386	51.106292
3492.688801	353938.708191	51.111297
3492.498191	352080.921371	51.116301
3492.177364	350212.289000	51.121306
3492.116859	348325.366442	51.126311
3491.622951	346434.392307	51.131316
3491.156813	344506.593435	51.136321
3490.832942	342565.204202	51.141325
3490.364793	340646.050874	51.146330
3490.242346	338690.983929	51.151335
3489.868323	336737.740659	51.156340
3489.429548	334765.321175	51.161345
3489.183697	332779.661915	51.166349
3488.662432	330776.083960	51.171354
3488.499636	328776.698549	51.176359
3488.290182	326746.732435	51.181364
3487.904977	324726.906876	51.186369
3487.774374	322677.162416	51.191373
3487.307296	320627.534578	51.196378
3486.947737	318549.311484	51.201383
3486.598546	316470.104519	51.206388
3486.255245	314377.747771	51.211393
3486.246508	312273.815512	51.216397
3485.566254	310173.196228	51.221402
3485.616907	308036.164701	51.226407
3485.087088	305895.202803	51.231412
3484.569275	303737.709989	51.236417
3484.476968	301572.630333	51.241421
3484.063558	299402.715894	51.246426
3483.746796	297220.666003	51.251431
3483.307071	295020.103078	51.256436
3482.839350	292812.980434	51.261441
3482.202537	290589.291367	51.266445
3481.667130	288359.330212	51.271450
3481.277376	286138.702101	51.276455
3481.106429	283901.829997	51.281460
3480.501074	281651.832437	51.286465
3480.600256	279386.632614	51.291469
3480.379179	277114.378893	51.296474
3479.730110	274820.932557	51.301479
3479.328522	272521.690140	51.306484
3479.014000	270225.799235	51.311489
3478.159225	267898.835717	51.316493
3477.792287	265583.769085	51.321498
3477.268936	263245.694051	51.326503
3477.022931	260911.433684	51.331508
3476.592791	258571.672183	51.336513
3476.090092	256215.136656	51.341517
3475.650240	253854.872316	51.346522
3475.632746	251482.187303	51.351527
3475.158321	249084.857663	51.356532
3474.442435	246694.761497	51.361537
3474.383631	244285.440427	51.366541
3473.649592	241886.005936	51.371546
3473.429386	239464.551335	51.376551
3472.577098	237028.127025	51.381556
3471.443754	234599.189648	51.386561
3471.318926	232155.799411	51.391565
3470.632903	229726.266561	51.396570
3469.872481	227278.526126	51.401575
3469.620311	224815.538913	51.406580
3468.932647	222368.028062	51.411585
3468.548573	219909.973108	51.416589
3467.809328	217436.831043	51.421594
3467.255667	214961.780391	51.426599
3466.807150	212493.037561	51.431604
3465.870927	210016.372177	51.436609
3465.924300	207523.707147	51.441613
3464.865108	205032.592122	51.446618
3464.243715	202539.188987	51.451623
3463.681110	200038.067489	51.456628
3462.921725	197535.996643	51.461633
3462.199170	195034.009668	51.466637
3461.298241	192537.161880	51.471642
3460.816299	190019.785483	51.476647
3460.078833	187517.331368	51.481652
3459.096669	185013.408394	51.486657
3458.695692	182502.458466	51.491661
3458.377529	179996.354865	51.496666
3457.413289	177476.507688	51.501671
3457.008339	174963.189538	51.506676
3456.382222	172452.923264	51.511681
3455.717298	169930.312438	51.516685
3454.506566	167408.947336	51.521690
3454.120272	164881.550244	51.526695
3453.367085	162354.028291	51.531700
3451.990614	159847.874474	51.536705
3451.359783	157315.948192	51.541709
3450.917508	154805.282711	51.546714
3449.998912	152297.398984	51.551719
3449.344877	149787.036445	51.556724
3448.427646	147195.555071	51.561729
3448.134052	144679.493955	51.566733
3447.207663	142173.478531	51.571738
3446.630821	139654.713965	51.576743
3445.623304	137145.039451	51.581748
3444.447032	134641.031091	51.586753
3444.084167	132125.962616	51.591757
3443.062311	129631.635786	51.596762
3442.117366	127136.396567	51.601767
3441.199236	124635.835544	51.606772
3439.950174	122138.900481	51.611777
3439.561649	119654.741728	51.616781
3438.184499	117186.152982	51.621786
3437.455901	114704.171586	51.626791
3436.863710	112236.226274	51.631796
3435.817023	109785.478908	51.636801
3434.634813	107318.804824	51.641805
3433.500358	104879.393038	51.646810
3432.624900	102426.915716	51.651815
3431.821458	99993.323334	51.656820
3430.367265	97579.264519	51.661825
3429.705748	95157.910513	51.666829
3428.195300	92752.177722	51.671834
3427.535489	90354.115824	51.676839
3426.403577	87960.512983	51.681844
3425.218102	85588.067827	51.686849
3423.763420	83226.359920	51.691853
3422.577610	80876.407499	51.696858
3421.447024	78539.445469	51.701863
3420.573710	76223.632075	51.706868
3419.137802	73916.295040	51.711873
3418.198920	71607.889122	51.716877
3416.556400	69333.053926	51.721882
3415.210252	67054.388116	51.726887
3414.112783	64798.119635	51.731892
3412.162696	62574.065708	51.736897
3411.027044	60362.713929	51.741901
3409.558152	58168.453659	51.746906
3408.098416	56005.745059	51.751911
3406.598555	53850.376595	51.756916
3404.995724	51731.655506	51.761921
3403.636964	49612.258612	51.766925
3402.168453	47536.190338	51.771930
3400.432255	45477.139509	51.776935
3398.930758	43435.514141	51.781940
3396.772256	41429.778557	51.786945
3395.163724	39448.661425	51.791949
3392.897786	37504.402048	51.796954
3390.305230	35613.332593	51.801959
3385.749327	33805.739562	51.806964
3380.292160	32090.561871	51.811969
3374.798288	30445.355251	51.816973
3368.072691	28930.174353	51.821978
3361.123173	27536.802719	51.826983
3354.927331	26249.389245	51.831988
3348.829461	25085.958325	51.836993
3343.244457	24029.132057	51.841997
3337.735737	23083.064123	51.847002
3332.870102	22244.812827	51.852007
3328.235259	21509.484520	51.857012
3323.741450	20894.974283	51.862017
3321.162133	20347.512083	51.867021
3318.111562	19891.203548	51.872026
3315.426056	19497.924775	51.877031
3313.396887	19170.523924	51.882036
3311.579684	18915.642642	51.887041
3309.859991	18691.439742	51.892045
3308.596148	18528.301847	51.897050
3307.330578	18361.923834	51.902055
3306.744534	18248.050448	51.907060
3305.712219	18162.018488	51.912065
3305.260682	18084.053451	51.917069
3304.840135	18036.425744	51.922074
3304.208313	18005.296765	51.927079
3303.871060	17969.418250	51.932084
3303.529226	17957.765612	51.937089
3303.248142	17935.597617	51.942093
3303.042462	17939.086471	51.947098
3302.773885	17936.777190	51.952103
3302.437341	17932.113290	51.957108
3302.143932	17950.797675	51.962113
3302.198536	17938.211132	51.967117
3302.010101	17948.184022	51.972122
3301.570242	17946.460387	51.977127
3301.767116	17937.461324	51.982132
3301.159469	17941.790201	51.987137
3301.311506	17932.568025	51.992141
3301.375827	17932.653460	51.997146
3301.117801	17917.621336	52.002151
3301.692202	17891.657550	52.007156
3300.828859	17866.958921	52.012161
3300.972959	17824.432506	52.017165
3300.662681	17798.239057	52.022170
3300.423066	17762.162532	52.027175
3300.444123	17701.592422	52.032180
3299.559875	17652.486519	52.037185
3299.691873	17605.793046	52.042189
3298.978502	17555.741477	52.047194
3298.760460	17498.069110	52.052199
3298.664376	17434.320825	52.057204
3298.043501	17373.268831	52.062209
3297.575655	17309.935417	52.067213
3296.949246	17231.836661	52.072218
3296.436605	17178.007533	52.077223
3296.486860	17099.939211	52.082228
3295.700655	17032.102870	52.087233
3295.438095	16944.058463	52.092237
3294.806448	16873.256531	52.097242
3294.382945	16791.339753	52.102247
3293.784501	16705.781684	52.107252
3293.160024	16630.972904	52.112257
3292.812001	16526.985154	52.117261
3292.144808	16464.727385	52.122266
3291.387765	16378.172334	52.127271
3291.070265	16280.118846	52.132276
3290.550546	16200.192270	52.137281
3289.851145	16106.202086	52.142285
3289.344697	16032.588044	52.147290
3289.114462	15935.367221	52.152295
3288.468685	15842.640049	52.157300
3287.598064	15761.890462	52.162305
3286.902127	15658.759347	52.167309
3286.526194	15565.777419	52.172314
3285.715429	15477.504070	52.177319
3285.154392	15382.923794	52.182324
3284.326775	15283.999250	52.187329
3283.754410	15191.263161	52.192333
3283.349930	15101.111277	52.197338
3282.370538	15006.841663	52.202343
3281.948836	14919.963491	52.207348
3281.817824	14828.614282	52.212353
3280.931513	14734.191242	52.217357
3280.749716	14633.706324	52.222362
3279.811549	14537.321004	52.227367
3279.473671	14436.595285	52.232372
3278.404644	14334.044981	52.237377
3277.838394	14232.076308	52.242381
3277.143225	14132.081941	52.247386
3276.455948	14034.155413	52.252391
3276.463058	13934.723366	52.257396
3275.168749	13846.168352	52.262401
3274.909029	13736.269607	52.267405
3274.308193	13640.746843	52.272410
3273.551943	13544.958838	52.277415
3272.965760	13436.045453	52.282420
3272.035637	13337.644643	52.287425
3271.829023	13231.741276	52.292429
3270.856000	13131.833607	52.297434
3270.216613	13037.357525	52.302439
3269.770546	12938.536664	52.307444
3268.900586	12839.649755	52.312449
3268.443948	12728.159046	52.317453
3267.642151	12616.321958	52.322458
3267.076293	12531.097439	52.327463
3266.358369	12434.347037	52.332468
3265.416847	12339.906029	52.337473
3265.188051	12233.715800	52.342477
3264.191515	12131.997936	52.347482
3263.858149	12040.137762	52.352487
3262.656729	11934.880383	52.357492
3261.694470	11838.306379	52.362497
3261.609389	11754.343654	52.367501
3260.743519	11660.408733	52.372506
3259.863335	11569.910228	52.377511
3259.653938	11473.467306	52.382516
3258.815425	11373.635832	52.387521
3258.159182	11282.272727	52.392525
3257.437016	11192.008439	52.397530
3256.759092	11097.967217	52.402535
3256.496249	11002.631135	52.407540
3255.367778	10915.052667	52.412545
3254.702912	10820.473618	52.417549
3254.452853	10736.095584	52.422554
3253.654952	10642.583067	52.427559
3253.140246	10544.480368	52.432564
3252.145319	10454.775493	52.437569
3251.413276	10356.041163	52.442573
3250.770392	10263.717720	52.447578
3250.414190	10182.702203	52.452583
3249.609203	10085.610859	52.457588
3249.106879	9998.434337	52.462593
3248.371490	9904.139653	52.467597
3248.203342	9812.709291	52.472602
3247.099147	9718.750424	52.477607
3246.510057	9624.166952	52.482612
3245.506324	9530.583816	52.487617
3245.182696	9443.591440	52.492621
3244.853235	9359.896047	52.497626
3243.878817	9265.595348	52.502631
3243.243400	9169.826513	52.507636
3242.224358	9085.774818	52.512641
3242.053243	8990.376386	52.517645
3241.411057	8896.722504	52.522650
3240.564410	8804.788132	52.527655
3240.097198	8705.857450	52.532660
3239.585056	8617.301406	52.537665
3238.855921	8520.113264	52.542669
3238.177932	8428.891536	52.547674
3237.510842	8333.223103	52.552679
3237.123614	8229.498250	52.557684
3236.226425	8151.583598	52.562689
3235.455427	8051.995573	52.567693
3234.890305	7953.760750	52.572698
3233.980027	7868.636830	52.577703
3233.808067	7773.883114	52.582708
3232.692431	7686.314362	52.587713
3232.248709	7579.210216	52.592717
3231.774106	7487.928256	52.597722
3230.914340	7392.147464	52.602727
3230.081649	7286.317768	52.607732
3229.628036	7208.555414	52.612737
3228.780424	7110.999517	52.617741
3227.799030	7018.932484	52.622746
3227.006364	6934.303624	52.627751
3226.693808	6842.982633	52.632756
3225.608443	6762.426302	52.637761
3225.356719	6679.339652	52.642765
3224.441798	6597.741738	52.647770
3223.721816	6511.234074	52.652775
3223.414980	6419.078144	52.657780
3222.800025	6334.149619	52.662785
3222.514201	6252.211428	52.667789
3221.208111	6152.123205	52.672794
3220.788163	6070.328111	52.677799
3220.320741	5975.714440	52.682804
3219.173038	5892.531427	52.687809
3218.291328	5801.084576	52.692813
3217.976938	5716.153785	52.697818
3217.067383	5642.782556	52.702823
3216.864219	5547.423410	52.707828
3216.027131	5471.179407	52.712833
3215.131698	5388.813560	52.717837
3214.336550	5297.277413	52.722842
3213.929474	5208.392888	52.727847
3213.386148	5126.138820	52.732852
3212.492227	5053.889803	52.737857
3211.716451	4961.378571	52.742861
3211.041812	4878.937363	52.747866
3210.030183	4802.194126	52.752871
3209.612148	4720.151339	52.757876
3208.814980	4647.686267	52.762881
3208.761497	4568.060797	52.767885
3207.986381	4490.872760	52.772890
3207.291598	4408.010219	52.777895
3207.051241	4328.282051	52.782900
3206.363859	4246.598060	52.787905
3205.476278	4161.864283	52.792909
3204.883588	4073.285498	52.797914
3204.239898	3993.536316	52.802919
3203.755391	3912.494535	52.807924
3202.665591	3828.117686	52.812929
3202.047360	3751.852431	52.817933
3201.398130	3667.801513	52.822938
3200.357176	3590.269246	52.827943
3200.082102	3500.905037	52.832948
3199.582744	3433.909380	52.837953
3198.592341	3344.335043	52.842957
3198.446808	3254.912978	52.847962
3197.747157	3191.869839	52.852967
3196.859375	3101.966657	52.857972
3195.951811	3027.376175	52.862977
3195.396325	2947.011568	52.867981
3194.472072	2863.170620	52.872986
3193.331558	2793.469942	52.877991
3192.883899	2712.052166	52.882996
3192.201018	2652.641205	52.888001
3191.677194	2584.618182	52.893005
3191.216074	2506.328926	52.898010
3190.372836	2441.871548	52.903015
3189.869637	2361.183582	52.908020
3188.902978	2293.729373	52.913025
3188.614805	2223.266579	52.918029
3187.930131	2147.368616	52.923034
3186.908863	2078.912444	52.928039
3186.423568	2010.874262	52.933044
3185.219630	1946.419742	52.938049
3184.740510	1865.446754	52.943053
3184.445083	1807.942699	52.948058
3183.592551	1747.185600	52.953063
3183.524790	1674.550324	52.958068
3182.475266	1607.554567	52.963073
3181.576234	1535.465800	52.968077
3181.300581	1468.540542	52.973082
3180.337787	1402.145885	52.978087
3179.586267	1333.068555	52.983092
3178.800829	1273.672035	52.988097
3178.157641	1214.329994	52.993101
3177.544876	1149.958942	52.998106
3176.802876	1085.539967	53.003111
3175.703928	1016.416413	53.008116
3175.526054	963.650141	53.013121
3174.339327	901.416658	53.018125
3173.452738	847.850913	53.023130
3173.187597	795.490126	53.028135
3172.699062	735.842418	53.033140
3171.596109	683.577777	53.038145
3171.019005	628.266858	53.043149
3170.661507	566.592517	53.048154
3169.709812	522.408948	53.053159
3169.128563	463.775621	53.058164
3168.204073	424.169791	53.063169
3167.385381	377.106812	53.068173
3166.768212	328.588898	53.073178
3165.758654	285.912716	53.078183
3164.949572	241.577685	53.083188
3164.198791	211.396933	53.088193
3163.070007	181.077142	53.093197
3162.532192	145.627594	53.098202
3161.135601	137.059017	53.103207
3160.265910	113.058122	53.108212
3158.681691	117.518043	53.113217
3157.980158	129.904090	53.118221
3157.590939	116.658377	53.123226
3156.736063	125.629775	53.128231
3156.143039	121.721052	53.133236
3155.552274	125.797299	53.138241
3154.563794	135.345333	53.143245
3154.388819	131.823858	53.148250
3153.900617	131.053869	53.153255
3153.180152	128.486891	53.158260
3152.436632	121.914597	53.163265
3151.875554	128.112569	53.168269
3151.535344	122.743577	53.173274
3150.601252	129.912367	53.178279
3150.058698	131.022678	53.183284
3149.144352	129.626828	53.188289
3148.526820	135.188673	53.193293
3148.238446	123.626612	53.198298
3147.364505	136.618425	53.203303
3146.216534	137.960067	53.208308
3145.512703	131.737823	53.213313
3145.456211	137.695644	53.218317
3145.256430	128.109851	53.223322
3143.765440	127.694743	53.228327
3144.013510	134.883394	53.233332
3143.042994	132.289273	53.238337
3142.280539	135.077648	53.243341
3141.714449	123.335280	53.248346
3140.947857	134.680890	53.253351
3140.424689	123.239077	53.258356
3139.865767	121.986183	53.263361
3138.872368	129.493125	53.268365
3138.581350	128.801156	53.273370
3137.702044	132.390664	53.278375
3136.787665	124.124573	53.283380
3136.645546	129.820317	53.288385
3136.047176	128.238249	53.293389
3135.012973	123.309535	53.298394
3134.588372	126.925956	53.303399
3134.057678	122.187920	53.308404
3133.326766	126.761393	53.313409
3132.691623	136.926413	53.318413
3131.944540	119.090760	53.323418
3130.867647	134.403513	53.328423
3130.705636	123.653532	53.333428
3130.250703	122.576684	53.338433
3129.098086	122.800856	53.343437
3129.222341	109.202957	53.348442
3128.420773	125.558504	53.353447
3127.323902	119.040272	53.358452
3126.583456	117.895367	53.363457
3125.755514	119.980472	53.368461
3125.576674	113.720251	53.373466
3124.855761	118.993050	53.378471
3123.770412	116.388161	53.383476
3124.170649	121.370722	53.388481
3123.249434	121.603911	53.393485
3122.636964	117.499968	53.398490
3121.195327	122.061061	53.403495
3120.368341	116.541171	53.408500
3120.416916	129.310228	53.413505
3119.404374	119.868837	53.418509
3119.001505	115.531325	53.423514
3118.088834	123.379333	53.428519
3117.880319	120.227928	53.433524
3117.547449	112.786157	53.438529
3116.296297	117.928110	53.443533
3116.006953	114.912883	53.448538
3114.630225	115.352582	53.453543
3114.342044	114.000145	53.458548
3113.595808	120.400274	53.463553
3112.612687	115.465209	53.468557
3112.304133	112.242479	53.473562
3112.145460	127.571624	53.478567
3111.536672	116.800489	53.483572
3110.381361	114.918068	53.488577
3109.264945	122.366688	53.493581
3108.917147	118.181210	53.498586
3108.309532	117.539784	53.503591
3107.673181	113.201115	53.508596
3107.065789	115.322353	53.513601
3106.242133	116.085968	53.518605
3106.480579	116.935737	53.523610
3106.037782	128.992976	53.528615
3104.665808	119.076566	53.533620
3104.176200	113.943500	53.538625
3103.339528	123.858346	53.543629
3102.840309	118.634159	53.548634
3101.701781	120.719046	53.553639
3100.752568	119.877046	53.558644
3100.813667	121.318420	53.563649
3100.248826	119.429451	53.568653
3099.898356	111.824509	53.573658
3098.589833	116.920216	53.578663
3097.875043	123.651283	53.583668
3096.920575	113.046189	53.588673
3096.026435	124.079250	53.593677
3096.000556	108.106667	53.598682
3096.089142	123.928810	53.603687
3095.117926	116.236117	53.608692
3094.372111	109.890410	53.613697
3092.923157	118.844895	53.618701
3092.882646	117.550402	53.623706
3092.105716	125.623504	53.628711
3091.464964	118.097369	53.633716
3091.239234	113.547230	53.638721
3090.561974	116.386969	53.643725
3089.743848	111.645162	53.648730
3089.199199	119.928435	53.653735
3088.408668	121.919918	53.658740
3087.537489	118.745165	53.663745
3086.655487	116.499872	53.668749
3086.069775	104.275368	53.673754
3085.053150	113.827808	53.678759
3084.586561	115.424474	53.683764
3084.776897	122.838894	53.688769
3083.706338	124.054427	53.693773
3083.282049	114.985027	53.698778
3082.406514	121.211860	53.703783
3081.491213	112.614770	53.708788
3080.944792	113.845744	53.713793
3080.435753	117.396856	53.718797
3079.672784	119.048112	53.723802
3078.745383	114.798255	53.728807
3077.881583	115.164926	53.733812
3077.529859	115.871592	53.738817
3077.191310	128.539818	53.743821
3077.071630	115.771083	53.748826
3075.863938	115.711788	53.753831
3075.037433	115.450391	53.758836
3074.872780	114.312502	53.763841
3073.829988	117.348119	53.768845
3073.153033	108.252819	53.773850
3072.326492	107.087897	53.778855
3071.418286	112.402963	53.783860
3071.001116	111.642951	53.788865
3069.889254	123.435961	53.793869
3069.783505	107.482556	53.798874
3069.423694	111.019222	53.803879
3069.065886	109.893812	53.808884
3067.685652	117.278962	53.813889
3067.557320	121.050019	53.818893
3066.700467	109.824323	53.823898
3065.453856	114.272366	53.828903
3065.477461	116.483943	53.833908
3064.850027	115.945380	53.838913
3063.861536	119.352238	53.843917
3063.135275	113.686074	53.848922
3062.157182	116.985762	53.853927
3061.781600	110.402726	53.858932
3061.259376	112.997693	53.863937
3060.665079	123.177040	53.868941
3059.690952	117.879667	53.873946
3059.186991	110.072806	53.878951
3058.977722	122.326577	53.883956
3057.969163	117.426659	53.888961
3057.357852	124.576220	53.893965
3057.014456	113.860408	53.898970
3055.927368	118.687766	53.903975
3055.454328	110.945883	53.908980
3054.755420	111.597796	53.913985
3054.399732	123.584487	53.918989
3053.654320	114.583383	53.923994
3052.308188	118.825414	53.928999
3052.018147	113.915617	53.934004
3051.801351	110.552875	53.939009
3051.311502	120.477931	53.944013
3050.153559	108.623967	53.949018
3048.919638	116.149114	53.954023
3048.830945	116.058091	53.959028
3048.684668	106.978302	53.964033
3047.336690	117.651155	53.969037
3047.416233	106.103231	53.974042
3046.313438	118.200209	53.979047
3044.705762	110.891804	53.984052
3044.699018	107.788823	53.989057
3044.011680	119.139038	53.994061
3043.645548	109.363805	53.999066
3043.148765	113.540441	54.004071
3042.215445	116.076578	54.009076
3041.959320	108.162638	54.014081
3040.906103	108.366290	54.019085
3040.182552	106.539185	54.024090
3039.623757	113.989630	54.029095
3038.863629	114.180701	54.034100
3038.571125	106.682310	54.039105
3037.801416	107.066856	54.044109
3037.139189	108.249728	54.049114
3036.546230	110.485738	54.054119
3035.717461	105.763524	54.059124
3034.750230	104.045952	54.064129
3034.424024	112.122557	54.069133
3033.841261	106.088469	54.074138
3033.248390	112.439499	54.079143
3031.797848	107.217228	54.084148
3031.570942	113.344281	54.089153
3030.842283	116.703981	54.094157
3030.378495	112.458203	54.099162
3029.925775	104.631937	54.104167
3029.114783	108.676346	54.109172
3028.586170	101.380537	54.114177
3027.698103	106.933342	54.119181
3027.036881	106.644499	54.124186
3026.789088	108.769032	54.129191
3025.639177	106.945705	54.134196
3025.601386	98.782890	54.139201
3023.925998	99.889813	54.144205
3023.769937	105.173462	54.149210
3023.443393	103.370098	54.154215
3022.427171	111.332905	54.159220
3021.419871	100.412008	54.164225
3020.962203	115.419990	54.169229
3020.785822	109.651586	54.174234
3020.165269	108.346476	54.179239
3018.811062	112.795544	54.184244
3018.577626	111.580597	54.189249
3018.101909	116.987159	54.194253
3016.998000	115.225050	54.199258
3016.111855	109.315829	54.204263
3016.443883	118.485853	54.209268
3015.226209	109.038498	54.214273
3014.046509	108.981933	54.219277
3014.082747	111.253716	54.224282
3013.641880	110.599992	54.229287
3012.495682	108.965503	54.234292
3011.496376	102.453532	54.239297
3011.430041	106.285041	54.244301
3010.983639	99.211630	54.249306
3009.655639	104.261730	54.254311
3008.851828	110.900641	54.259316
3009.093526	103.877012	54.264321
3008.010670	105.459781	54.269325
3007.313403	106.482857	54.274330
3006.805158	102.768090	54.279335
3005.751151	108.359517	54.284340
3005.686656	105.173645	54.289345
3004.661621	118.160473	54.294349
3004.122983	105.640976	54.299354
3003.669061	103.962009	54.304359
3002.487274	104.729599	54.309364
3002.203000	104.706338	54.314369
3001.770079	115.822028	54.319373
3001.011642	106.347125	54.324378
3000.644938	100.653879	54.329383
2999.126109	108.743228	54.334388
2998.834374	107.007731	54.339393
2997.833111	101.287526	54.344397
2997.929066	99.684330	54.349402
2996.522679	104.956638	54.354407
2995.497473	116.159722	54.359412
2995.776300	107.880434	54.364417
2995.008046	103.056706	54.369421
2993.958281	104.596718	54.374426
2993.560175	96.851522	54.379431
2992.572191	103.772554	54.384436
2991.925480	101.699042	54.389441
2991.271631	105.073196	54.394445
2991.480298	97.923375	54.399450
2990.795376	105.402080	54.404455
2989.959680	102.188523	54.409460
2989.669461	101.757341	54.414465
2988.141226	103.551611	54.419469
2986.977013	98.019119	54.424474
2987.278667	99.089390	54.429479
2986.363820	97.476163	54.434484
2985.229739	99.048741	54.439489
2984.505236	102.555360	54.444493
2984.057548	99.802857	54.449498
2983.809166	98.342578	54.454503
2983.178017	102.850851	54.459508
2981.961479	97.202963	54.464513
2981.124242	103.055368	54.469517
2981.256367	101.007449	54.474522
2980.927374	96.184056	54.479527
2979.641373	106.275939	54.484532
2979.072843	102.525294	54.489537
2978.183693	102.568293	54.494541
2977.811541	93.964081	54.499546
2977.688242	104.357396	54.504551
2976.817888	108.161302	54.509556
2975.687429	107.259509	54.514561
2974.426075	110.171044	54.519565
2973.960127	106.308135	54.524570
2974.301802	111.496071	54.529575
2973.169543	113.016633	54.534580
2972.123334	99.089841	54.539585
2971.106454	104.866369	54.544589
2970.828872	101.772569	54.549594
2970.841529	106.879757	54.554599
2970.046251	102.457747	54.559604
2969.233660	102.784105	54.564609
2968.477449	101.033248	54.569613
2968.022149	101.728803	54.574618
2967.346520	98.016594	54.579623
2966.707444	109.893804	54.584628
2966.243075	103.828444	54.589633
2964.545973	114.345444	54.594637
2964.313224	99.980838	54.599642
2964.071273	99.232733	54.604647
2962.511988	107.354658	54.609652
2962.908159	102.374584	54.614657
2962.008088	104.425849	54.619661
2961.168618	100.931502	54.624666
2960.487593	109.010712	54.629671
2959.864087	105.143151	54.634676
2959.440107	102.362520	54.639681
2958.801679	110.854837	54.644685
2958.296423	106.056828	54.649690
2957.703821	110.552201	54.654695
2956.615318	105.167037	54.659700
2955.719544	102.215982	54.664705
2954.297452	114.811989	54.669709
2954.454369	107.074971	54.674714
2954.465185	105.367116	54.679719
2953.130540	100.229274	54.684724
2952.495582	96.658140	54.689729
2951.858805	108.053389	54.694733
2951.513277	101.503524	54.699738
2950.798590	97.322740	54.704743
2950.042061	102.996360	54.709748
2949.633900	99.229762	54.714753
2949.261943	100.014889	54.719757
2948.047611	91.344607	54.724762
2947.050847	97.429136	54.729767
2946.046932	105.730098	54.734772
2946.269421	97.422947	54.739777
2945.389659	102.509351	54.744781
2944.790799	106.453571	54.749786
2943.717804	103.395044	54.754791
2942.821305	112.048302	54.759796
2942.624084	89.952039	54.764801
2942.447281	108.856911	54.769805
2941.699090	101.782583	54.774810
2941.010734	101.215763	54.779815
2940.318423	104.041507	54.784820
2940.111885	95.090059	54.789825
2938.303802	104.353819	54.794829
2937.711831	98.381321	54.799834
2937.886042	107.060809	54.804839
2937.188756	108.164421	54.809844
2936.427369	105.979464	54.814849
2935.505594	101.876307	54.819853
2934.775766	100.057790	54.824858
2934.538736	92.397576	54.829863
2933.824688	95.154799	54.834868
2932.818958	96.868475	54.839873
2931.734259	109.363402	54.844877
2931.089489	104.164512	54.849882
2930.988908	104.428409	54.854887
2930.008425	108.595342	54.859892
2929.880629	103.388236	54.864897
2929.212456	105.339879	54.869901
2928.126637	103.125105	54.874906
2928.340968	100.478152	54.879911
2926.590145	102.074824	54.884916
2926.089869	91.160471	54.889921
2925.232851	101.629035	54.894925
2925.129551	99.669110	54.899930
2924.164971	103.383337	54.904935
2923.278386	92.429214	54.909940
2922.991422	92.750224	54.914945
2921.928142	88.985063	54.919949
2921.713240	104.289426	54.924954
2921.186962	96.500225	54.929959
2920.989255	101.376523	54.934964
2920.207258	96.502661	54.939969
2919.221127	98.731265	54.944973
2918.313418	101.917102	54.949978
2917.839865	96.110289	54.954983
2916.946236	101.731946	54.959988
2916.790113	96.820994	54.964993
2916.164810	95.885779	54.969997
2914.647102	94.637293	54.975002
2914.039069	99.766866	54.980007
2913.420400	106.531638	54.985012
2913.391646	97.894407	54.990017
2911.792895	103.608541	54.995021
2911.327339	97.587998	55.000026
2911.146339	93.762849	55.005031
2910.658934	93.998117	55.010036
2910.381570	94.933261	55.015041
2909.657671	102.497573	55.020045
2909.027984	100.755102	55.025050
2907.701606	91.044929	55.030055
2906.546046	99.486671	55.035060
2905.940022	94.775366	55.040065
2905.404832	98.112668	55.045069
2905.317595	96.402625	55.050074
2904.702617	86.551144	55.055079
2903.639640	95.333501	55.060084
2903.507366	85.219534	55.065089
2903.008958	90.440104	55.070093
2902.047154	100.199884	55.075098
2901.207909	96.102763	55.080103
2899.766700	94.487138	55.085108
2899.957481	91.514615	55.090113
2899.215704	93.192265	55.095117
2898.349037	98.444194	55.100122
2897.833346	89.191914	55.105127
2897.198998	100.751737	55.110132
2896.775502	95.164919	55.115137
2896.079427	93.678132	55.120141
2895.569358	93.000720	55.125146
2895.258730	98.321040	55.130151
2894.101054	105.687124	55.135156
2892.914530	102.424990	55.140161
2892.369783	97.517692	55.145165
2891.599093	102.857823	55.150170
2891.558088	94.076641	55.155175
2891.062337	98.733880	55.160180
2890.540681	97.572145	55.165185
2889.284404	94.756922	55.170189
2888.001950	97.774706	55.175194
2887.450356	98.705007	55.180199
2887.044471	110.561311	55.185204
2886.818226	96.086273	55.190209
2885.998903	104.205302	55.195213
2885.421034	97.607920	55.200218
2885.235784	104.490458	55.205223
2884.748113	103.110157	55.210228
2883.407758	92.537929	55.215233
2882.280160	98.527591	55.220237
2881.798766	101.642154	55.225242
2881.257852	102.850492	55.230247
2880.456467	103.513228	55.235252
2879.948406	91.882601	55.240257
2879.876039	94.667136	55.245261
2879.159111	99.649141	55.250266
2878.552028	93.905416	55.255271
2877.347014	101.555899	55.260276
2876.611629	94.167961	55.265281
2875.643927	99.555576	55.270285
2875.380543	98.256548	55.275290
2874.985393	93.722362	55.280295
2874.167348	99.491364	55.285300
2873.767361	94.316969	55.290305
2873.143374	95.176356	55.295309
2872.710151	98.551100	55.300314
2871.692092	99.895455	55.305319
2870.564223	98.425230	55.310324
2870.081256	95.831922	55.315329
2869.628776	100.246905	55.320333
2868.883193	101.033523	55.325338
2868.739583	91.213592	55.330343
2867.328144	99.681307	55.335348
2866.708504	94.309589	55.340353
2865.740793	96.694128	55.345357
2864.961201	93.879549	55.350362
2864.701767	92.475639	55.355367
2864.347522	97.415792	55.360372
2864.005936	85.943428	55.365377
2863.370060	94.125836	55.370381
2862.730552	91.219423	55.375386
2861.511751	91.600614	55.380391
2860.593344	97.245062	55.385396
2860.235246	90.952750	55.390401
2859.613370	91.607309	55.395405
2858.780449	94.635111	55.400410
2858.748432	86.727114	55.405415
2858.286409	90.836233	55.410420
2857.594532	91.168423	55.415425
2856.302511	94.353632	55.420429
2854.981291	96.079398	55.425434
2854.927477	87.196994	55.430439
2854.294292	95.250262	55.435444
2854.186342	84.614659	55.440449
2853.116500	87.290987	55.445453
2852.116213	91.957876	55.450458
2851.552865	96.209837	55.455463
2850.853282	98.493293	55.460468
2850.033682	87.086047	55.465473
2849.144842	86.894941	55.470477
2848.697151	91.934744	55.475482
2848.916540	89.138512	55.480487
2848.013109	96.746927	55.485492
2847.341627	91.444861	55.490497
2847.175660	93.564884	55.495501
2845.809911	90.461681	55.500506
2844.955285	89.050550	55.505511
2844.085754	87.941958	55.510516
2843.617247	89.891456	55.515521
2843.503149	83.373111	55.520525
2842.862759	87.433769	55.525530
2842.317042	81.930218	55.530535
2840.689932	96.840409	55.535540
2840.211289	94.476097	55.540545
2839.454723	90.600510	55.545549
2838.984292	88.974513	55.550554
2838.575913	90.768870	55.555559
2837.656869	93.638503	55.560564
2837.665883	90.911776	55.565569
2837.195834	84.483475	55.570573
2836.156515	88.065224	55.575578
2835.423486	88.078405	55.580583
2834.734219	93.035947	55.585588
2834.206423	89.530594	55.590593
2833.281649	85.821912	55.595597
2832.290096	91.558991	55.600602
2831.571108	89.026947	55.605607
2830.996122	94.409815	55.610612
2830.694387	89.663096	55.615617
2829.773679	89.090608	55.620621
2828.943773	97.663406	55.625626
2829.287172	87.978927	55.630631
2828.867975	101.803232	55.635636
2827.872935	87.646313	55.640641
2826.935079	98.761835	55.645645
2826.098608	96.155925	55.650650
2825.284275	89.126878	55.655655
2823.854008	92.762420	55.660660
2823.379120	88.512256	55.665665
2823.656069	95.728678	55.670669
2822.615568	99.581809	55.675674
2822.029689	90.442194	55.680679
2821.170961	89.710302	55.685684
2820.871119	94.804967	55.690689
2820.005255	87.163825	55.695693
2819.804633	84.247146	55.700698
2818.790740	86.365249	55.705703
2817.677183	94.739427	55.710708
2817.106734	89.731933	55.715713
2817.097622	94.949405	55.720717
2815.779072	93.842562	55.725722
2815.516713	91.114455	55.730727
2814.427291	90.598040	55.735732
2814.305393	90.884133	55.740737
2813.988319	98.356022	55.745741
2812.390152	94.164817	55.750746
2811.827363	86.683057	55.755751
2811.238413	96.883970	55.760756
2810.880352	90.837968	55.765761
2810.369982	86.724130	55.770765
2809.601369	87.615346	55.775770
2809.559032	80.231738	55.780775
2808.026815	91.321343	55.785780
2807.013428	87.072037	55.790785
2806.708161	79.437717	55.795789
2805.790640	89.333608	55.800794
2805.702838	81.065690	55.805799
2804.991560	93.509420	55.810804
2804.850437	81.460455	55.815809
2803.866286	90.999851	55.820813
2802.904030	84.125169	55.825818
2802.142017	80.103684	55.830823
2801.577922	92.697122	55.835828
2800.951313	84.053146	55.840833
2800.472608	81.280310	55.845837
2799.163526	87.792036	55.850842
2798.467749	76.459567	55.855847
2797.746538	85.616135	55.860852
2797.324247	80.809108	55.865857
2796.681566	85.152784	55.870861
2796.208180	84.257934	55.875866
2796.073487	75.324237	55.880871
2795.643267	88.229122	55.885876
2794.716490	81.651923	55.890881
2793.739309	86.238291	55.895885
2792.763456	90.284449	55.900890
2792.640549	83.011319	55.905895
2791.962272	93.011188	55.910900
2790.932222	84.537613	55.915905
2790.244187	77.458178	55.920909
2788.814900	90.241328	55.925914
2788.808322	88.856968	55.930919
2787.887959	88.386662	55.935924
2787.797034	86.163715	55.940929
2787.315320	85.235553	55.945933
2786.411649	93.472022	55.950938
2786.451569	76.927769	55.955943
2785.422994	82.525525	55.960948
2783.905765	75.908331	55.965953
2783.534841	80.645678	55.970957
2782.820581	85.043430	55.975962
2782.605947	79.672770	55.980967
2782.067063	86.026018	55.985972
2781.217482	88.451165	55.990977
2780.398562	82.152764	55.995981
2779.407190	92.900862	56.000986
2779.141725	84.219639	56.005991
2778.693361	84.503901	56.010996
2778.125159	73.826984	56.016001
2777.506977	80.824554	56.021005
2776.267685	88.013153	56.026010
2775.475761	83.610742	56.031015
2774.508794	87.664856	56.036020
2774.239518	80.378853	56.041025
2773.817713	73.450098	56.046029
2773.451592	75.654064	56.051034
2773.306438	75.439674	56.056039
2771.842117	82.627259	56.061044
2770.917514	82.686218	56.066049
2770.491746	82.260850	56.071053
2769.630290	88.445423	56.076058
2769.510967	82.269811	56.081063
2768.906553	85.847891	56.086068
2768.126886	82.594802	56.091073
2766.841935	79.214531	56.096077
2765.742692	81.956685	56.101082
2765.646104	79.225908	56.106087
2765.323520	88.497497	56.111092
2764.941142	91.618430	56.116097
2764.537249	88.313350	56.121101
2763.593297	82.618937	56.126106
2763.001651	82.976242	56.131111
2761.476080	86.010734	56.136116
2761.059788	85.566773	56.141121
2760.953435	76.171144	56.146125
2760.519152	82.177311	56.151130
2759.737356	68.380288	56.156135
2758.454032	81.154276	56.161140
2758.093021	75.661011	56.166145
2757.705326	77.753011	56.171149
2756.793956	81.440002	56.176154
2755.676875	71.784906	56.181159
2754.767931	83.190733	56.186164
2754.067929	87.446318	56.191169
2754.082934	90.759059	56.196173
2753.028387	90.276957	56.201178
2753.083587	86.017908	56.206183
2752.466632	91.926621	56.211188
2751.888164	84.076116	56.216193
2751.060122	76.828388	56.221197
2749.582669	85.954352	56.226202
2749.493995	78.397491	56.231207
2748.480952	89.048243	56.236212
2748.285427	88.276820	56.241217
2747.800102	79.308718	56.246221
2746.721023	88.733293	56.251226
2745.981027	79.812668	56.256231
2745.217256	85.295301	56.261236
2744.842695	83.783976	56.266241
2744.423791	80.524096	56.271245
2743.507724	87.682320	56.276250
2742.960060	79.210387	56.281255
2741.765480	84.020624	56.286260
2740.993363	78.598418	56.291265
2740.891324	85.607242	56.296269
2740.126680	85.288743	56.301274
2739.989227	77.671144	56.306279
2739.550107	93.513914	56.311284
2738.143894	88.968618	56.316289
2737.550704	83.490565	56.321293
2736.571778	90.828083	56.326298
2736.407959	89.345472	56.331303
2735.828785	95.156547	56.336308
2734.882888	89.855618	56.341313
2733.855961	86.864265	56.346317
2732.743519	88.915149	56.351322
2732.484656	81.709080	56.356327
2732.073835	84.776059	56.361332
2731.833308	92.873921	56.366337
2731.300834	78.833366	56.371341
2730.410156	95.901577	56.376346
2730.191075	86.139566	56.381351
2728.948968	85.367037	56.386356
2727.911764	85.475644	56.391361
2727.663887	85.695642	56.396365
2727.260040	83.738942	56.401370
2726.718442	91.021052	56.406375
2725.590279	88.990793	56.411380
2724.608673	91.211547	56.416385
2724.335263	80.053604	56.421389
2723.554827	89.616209	56.426394
2723.410527	79.873394	56.431399
2722.660404	88.546237	56.436404
2721.515638	88.785727	56.441409
2721.061352	85.562685	56.446413
2720.240674	88.978003	56.451418
2719.819215	84.143607	56.456423
2719.219021	94.564328	56.461428
2718.211633	89.567194	56.466433
2716.950429	80.780268	56.471437
2716.761056	87.480344	56.476442
2716.862218	80.869956	56.481447
2715.726459	84.257816	56.486452
2715.418563	86.517358	56.491457
2714.895012	79.183250	56.496461
2713.611288	84.881073	56.501466
2712.767448	77.270537	56.506471
2712.288997	83.383331	56.511476
2711.317611	88.753434	56.516481
2711.096399	80.303467	56.521485
2710.563411	88.911565	56.526490
2710.483348	80.529048	56.531495
2709.123143	82.345584	56.536500
2708.201852	84.176304	56.541505
2707.743677	89.332767	56.546509
2707.118378	87.291951	56.551514
2706.721069	82.321591	56.556519
2706.181827	87.581908	56.561524
2705.140611	86.313612	56.566529
2704.324102	87.578939	56.571533
2703.738184	89.283653	56.576538
2703.453598	78.684582	56.581543
2702.944581	90.505595	56.586548
2702.198242	87.548391	56.591553
2701.064732	78.230054	56.596557
2700.262425	88.074678	56.601562
2699.937815	76.520505	56.606567
2699.588285	89.069760	56.611572
2698.680365	88.915095	56.616577
2698.333621	87.657169	56.621581
2696.904836	90.130017	56.626586
2696.355553	80.249199	56.631591
2696.142723	85.946339	56.636596
2695.281738	91.423885	56.641601
2694.520782	86.276875	56.646605
2693.815399	89.096189	56.651610
2693.042467	88.449518	56.656615
2692.629640	89.804524	56.661620
2691.695580	86.394686	56.666625
2691.581927	82.105689	56.671629
2690.923620	93.096458	56.676634
2690.647987	88.468052	56.681639
2689.054575	91.448239	56.686644
2688.617611	82.250834	56.691649
2687.876471	86.941732	56.696653
2687.301124	91.072202	56.701658
2687.096544	79.894606	56.706663
2685.956012	80.699415	56.711668
2684.941898	79.328994	56.716673
2684.288353	78.587315	56.721677
2683.623761	82.560148	56.726682
2683.673183	87.352749	56.731687
2683.273848	81.624865	56.736692
2682.603760	86.290592	56.741697
2681.624871	87.325133	56.746701
2680.350156	87.505136	56.751706
2679.894387	77.412159	56.756711
2679.770073	75.959114	56.761716
2679.043817	81.878220	56.766721
2678.105586	78.873299	56.771725
2677.163993	80.968802	56.776730
2676.435120	80.142107	56.781735
2676.595621	79.649689	56.786740
2675.967541	77.261601	56.791745
2675.274269	78.411132	56.796749
2674.001007	73.364727	56.801754
2673.309069	77.541965	56.806759
2673.166502	80.021529	56.811764
2671.834355	75.476623	56.816769
2671.703087	74.329889	56.821773
2670.349874	77.501118	56.826778
2670.132030	76.535757	56.831783
2669.289322	80.661797	56.836788
2668.320971	86.471109	56.841793
2668.605711	75.529209	56.846797
2667.758474	87.178697	56.851802
2667.139669	84.432587	56.856807
2665.925872	87.696037	56.861812
2665.246933	86.035043	56.866817
2664.902308	81.656454	56.871821
2664.245835	81.227900	56.876826
2663.887095	77.761567	56.881831
2663.207352	80.417030	56.886836
2661.826662	95.732344	56.891841
2661.377704	81.236620	56.896845
2660.577723	84.065397	56.901850
2660.072403	79.887957	56.906855
2660.102130	84.934573	56.911860
2659.268278	82.696525	56.916865
2658.688894	77.469541	56.921869
2657.380650	84.639153	56.926874
2657.238933	88.286565	56.931879
2656.516368	88.577446	56.936884
2655.661480	83.946223	56.941889
2655.433011	76.189065	56.946893
2653.912927	87.137278	56.951898
2653.556524	81.132857	56.956903
2653.200105	81.980868	56.961908
2652.637010	90.941078	56.966913
2651.955334	78.709417	56.971917
2650.651520	92.722020	56.976922
2650.147007	80.211003	56.981927
2649.419282	77.961527	56.986932
2648.460073	74.781388	56.991937
2648.720268	70.597039	56.996941
2647.947495	86.719452	57.001946
2647.624753	79.620232	57.006951
2646.398643	82.060419	57.011956
2645.641086	84.242490	57.016961
2645.075988	74.495438	57.021965
2644.289897	81.730131	57.026970
2644.390017	77.293283	57.031975
2643.332787	82.102951	57.036980
2642.205360	82.942238	57.041985
2641.723821	79.694261	57.046989
2641.092246	85.372588	57.051994
2640.879289	85.501755	57.056999
2639.921138	79.159292	57.062004
2638.826694	90.339872	57.067009
2638.191708	83.327579	57.072013
2637.824136	82.102822	57.077018
2637.361037	83.756942	57.082023
2636.687373	88.555912	57.087028
2635.740768	90.261106	57.092033
2635.105119	80.531245	57.097037
2633.848938	91.115808	57.102042
2633.518557	85.228515	57.107047
2633.611142	79.038008	57.112052
2632.741038	85.427747	57.117057
2632.444727	76.020002	57.122061
2631.311218	86.818849	57.127066
2630.686813	84.935781	57.132071
2630.143293	76.358955	57.137076
2629.556966	79.672248	57.142081
2628.151677	77.209400	57.147085
2627.265672	76.691802	57.152090
2626.969192	81.527343	57.157095
2626.646498	79.122188	57.162100
2625.807630	86.002758	57.167105
2625.903386	78.089524	57.172109
2625.119400	78.351831	57.177114
2624.146338	74.895783	57.182119
2623.098312	76.489240	57.187124
2622.955867	88.914671	57.192129
2622.311978	78.571240	57.197133
2621.012101	81.069829	57.202138
2620.065891	78.393510	57.207143
2619.593739	74.980516	57.212148
2618.787256	82.557764	57.217153
2618.618471	77.215599	57.222157
2617.980206	86.807584	57.227162
2617.709461	76.395237	57.232167
2617.687663	76.307391	57.237172
2616.135502	83.984875	57.242177
2615.494444	87.259765	57.247181
2614.650587	83.086914	57.252186
2614.162459	76.278859	57.257191
2613.884237	82.887541	57.262196
2612.398158	80.498506	57.267201
2611.831958	76.143986	57.272205
2611.081993	88.798792	57.277210
2610.463978	80.582060	57.282215
2610.321428	75.632504	57.287220
2609.395115	80.745839	57.292225
2609.177402	75.297963	57.297229
2608.483126	82.715509	57.302234
2607.377346	76.245534	57.307239
2606.982984	70.697598	57.312244
2606.125837	75.831081	57.317249
2605.336840	70.971904	57.322253
2604.341134	78.255851	57.327258
2603.759283	82.053499	57.332263
2603.633194	76.215761	57.337268
2603.075838	77.021548	57.342273
2603.068044	72.128692	57.347277
2601.653737	74.522113	57.352282
2600.445121	76.079476	57.357287
2600.163628	72.077724	57.362292
2599.676194	74.184413	57.367297
2599.304019	65.748434	57.372301
2597.940869	74.018060	57.377306
2597.104637	79.853342	57.382311
2596.785456	73.500737	57.387316
2595.914645	80.723468	57.392321
2595.954695	72.548585	57.397325
2595.454090	73.669925	57.402330
2594.131861	72.291407	57.407335
2593.305712	69.048666	57.412340
2592.799196	79.948742	57.417345
2592.104944	67.273216	57.422349
2591.867633	73.516491	57.427354
2591.278256	65.380136	57.432359
2590.470860	67.208374	57.437364
2589.188324	75.271595	57.442369
2588.854513	63.488901	57.447373
2588.475159	65.961969	57.452378
2588.075336	66.145977	57.457383
2587.389071	71.938253	57.462388
2586.069511	72.772107	57.467393
2585.795435	68.774616	57.472397
2585.326732	70.660215	57.477402
2583.885736	66.413804	57.482407
2583.324839	65.361441	57.487412
2582.485400	69.165622	57.492417
2581.832449	68.372935	57.497421
2581.785628	72.416212	57.502426
2581.292488	73.003003	57.507431
2580.741622	72.520091	57.512436
2580.137197	77.651031	57.517441
2579.039862	68.053403	57.522445
2577.968876	77.187269	57.527450
2577.231352	75.251313	57.532455
2577.294586	65.407918	57.537460
2576.608131	78.529869	57.542465
2576.256648	76.174639	57.547469
2575.342535	76.043553	57.552474
2574.403673	78.492672	57.557479
2574.212613	65.861784	57.562484
2573.259260	81.503497	57.567489
2573.211956	70.523637	57.572493
2572.457949	79.619105	57.577498
2571.079679	78.432141	57.582503
2570.312471	75.377084	57.587508
2568.934787	80.472853	57.592513
2568.961506	78.845576	57.597517
2568.059884	83.070512	57.602522
2567.665288	81.083826	57.607527
2567.183798	74.958307	57.612532
2566.627608	84.065354	57.617537
2566.444812	80.529085	57.622541
2565.101586	85.924482	57.627546
2564.228871	84.063742	57.632551
2563.849627	82.870196	57.637556
2563.010970	78.795544	57.642561
2562.983008	77.336689	57.647565
2562.522576	71.970575	57.652570
2561.490254	80.812844	57.657575
2560.710279	73.119588	57.662580
2559.625680	76.392546	57.667585
2559.113717	75.372475	57.672589
2558.677315	79.093155	57.677594
2557.624551	82.716319	57.682599
2557.116814	68.803821	57.687604
2556.374397	85.934693	57.692609
2556.181391	70.757373	57.697613
2555.603849	73.279324	57.702618
2554.818393	79.773804	57.707623
2554.243467	76.552461	57.712628
2552.922899	82.505285	57.717633
2552.394063	77.028895	57.722637
2552.318276	73.805903	57.727642
2551.269892	77.016225	57.732647
2550.774739	76.223800	57.737652
2549.479178	79.569930	57.742657
2549.754784	76.361862	57.747661
2548.808567	78.772769	57.752666
2548.242154	82.496335	57.757671
2547.439591	73.051209	57.762676
2546.528676	81.925618	57.767681
2546.070222	76.383514	57.772685
2545.422329	82.406860	57.777690
2544.977339	82.294655	57.782695
2543.647872	76.326739	57.787700
2542.811457	74.673343	57.792705
2542.662499	77.723982	57.797709
2542.291608	79.692333	57.802714
2541.579295	76.469612	57.807719
2541.657982	76.007361	57.812724
2540.228564	82.811665	57.817729
2539.256717	68.580238	57.822733
2538.564124	74.962134	57.827738
2538.197181	75.996287	57.832743
2537.819035	80.201204	57.837748
2536.859763	77.793179	57.842753
2535.937190	75.010208	57.847757
2535.169167	71.127560	57.852762
2534.758762	78.255795	57.857767
2534.189575	71.627002	57.862772
2533.489408	78.468074	57.867777
2532.771491	74.528309	57.872781
2531.899279	78.136397	57.877786
2531.422659	78.085256	57.882791
2530.586331	71.995145	57.887796
2530.299660	78.919075	57.892801
2530.008262	77.088033	57.897805
2529.284417	77.277705	57.902810
2527.954860	80.218743	57.907815
2527.951209	69.542469	57.912820
2527.065955	72.804640	57.917825
2526.260723	72.248382	57.922829
2525.370440	86.877507	57.927834
2524.419507	83.785973	57.932839
2524.452120	71.106588	57.937844
2523.607952	74.343183	57.942849
2523.217993	71.640468	57.947853
2522.017969	71.803000	57.952858
2521.053543	78.785170	57.957863
2520.895565	72.466987	57.962868
2520.341374	84.103875	57.967873
2519.912978	77.936918	57.972877
2519.732729	80.028989	57.977882
2518.462071	77.625652	57.982887
2517.457026	62.381919	57.987892
2516.796349	77.201511	57.992897
2516.222691	73.529971	57.997901
2516.215479	77.669104	58.002906
2515.062528	84.848502	58.007911
2514.340426	75.011876	58.012916
2513.268042	76.410969	58.017921
2513.021240	73.632072	58.022925
2512.857552	72.888769	58.027930
2511.386029	83.075565	58.032935
2510.796051	80.935188	58.037940
2509.980241	84.328775	58.042945
2509.671832	74.865882	58.047949
2509.170655	79.140780	58.052954
2508.779439	82.284545	58.057959
2507.852779	76.316062	58.062964
2507.057071	78.338097	58.067969
2506.244225	80.187804	58.072973
2505.643793	77.346606	58.077978
2505.531889	79.345679	58.082983
2505.069752	69.466587	58.087988
2503.653899	79.347426	58.092993
2503.135773	80.259012	58.097997
2502.799076	65.121273	58.103002
2501.790114	88.090686	58.108007
2500.793714	72.871918	58.113012
2500.299713	77.999772	58.118017
2499.810583	75.099284	58.123021
2499.404339	73.274854	58.128026
2499.124175	80.475952	58.133031
2497.726775	71.719886	58.138036
2496.684333	77.743190	58.143041
2496.234862	80.693237	58.148045
2495.597858	75.016277	58.153050
2495.465250	76.731925	58.158055
2495.223332	69.997057	58.163060
2493.668327	79.570909	58.168065
2492.940243	74.698181	58.173069
2492.250177	78.476837	58.178074
2491.563969	83.071125	58.183079
2491.540883	69.206832	58.188084
2491.139890	72.929749	58.193089
2490.028162	73.408365	58.198093
2489.310951	68.157609	58.203098
2488.553820	69.325972	58.208103
2488.350155	65.860383	58.213108
2486.983118	74.382130	58.218113
2486.454005	70.088393	58.223117
2485.997086	70.882940	58.228122
2484.901225	73.343913	58.233127
2484.818838	75.291756	58.238132
2484.349935	75.090490	58.243137
2483.312088	72.149612	58.248141
2482.357133	77.090231	58.253146
2481.577200	76.639387	58.258151
2481.674517	70.157565	58.263156
2480.915592	78.797971	58.268161
2480.407106	67.954997	58.273165
2479.346705	72.429711	58.278170
2478.204667	68.764962	58.283175
2477.883274	60.868990	58.288180
2477.515176	62.529375	58.293185
2476.839763	70.167899	58.298189
2475.829351	61.927900	58.303194
2474.793135	70.872676	58.308199
2474.930790	61.393137	58.313204
2473.892916	69.935577	58.318209
2473.495804	68.969693	58.323213
2473.496188	66.634444	58.328218
2472.528339	69.753247	58.333223
2471.833589	58.008605	58.338228
2470.669648	66.328658	58.343233
2469.579891	66.818127	58.348237
2468.959148	65.375364	58.353242
2467.789497	72.308547	58.358247
2468.402649	65.828137	58.363252
2467.570719	71.024818	58.368257
2466.838622	63.454056	58.373261
2466.506629	62.719400	58.378266
2465.599942	68.685943	58.383271
2464.722883	55.094378	58.388276
2463.906367	75.275301	58.393281
2463.616054	62.700088	58.398285
2463.195656	58.408691	58.403290
2461.990660	66.507614	58.408295
2461.288373	53.740748	58.413300
2460.458110	61.166147	58.418305
2460.537028	68.582545	58.423309
2460.480505	69.022462	58.428314
2459.103877	69.970309	58.433319
2458.749599	58.375084	58.438324
2458.033678	70.018297	58.443329
2456.937024	70.999984	58.448333
2456.013782	64.940147	58.453338
2455.062256	72.844163	58.458343
2454.660556	57.946497	58.463348
2453.716756	68.441736	58.468353
2453.821976	64.574796	58.473357
2453.564131	66.629608	58.478362
2452.284055	70.230073	58.483367
2451.624740	65.299810	58.488372
2450.595034	65.552444	58.493377
2449.942155	65.814858	58.498381
2449.604690	63.511322	58.503386
2449.151484	66.281224	58.508391
2448.455981	62.949860	58.513396
2447.330169	72.154292	58.518401
2446.768761	69.231434	58.523405
2446.043819	69.771029	58.528410
2445.769039	71.201916	58.533415
2445.527663	67.314896	58.538420
2444.634369	77.000611	58.543425
2443.245291	60.945884	58.548429
2442.762418	67.454551	58.553434
2442.408779	76.851820	58.558439
2442.349943	62.135523	58.563444
2440.935801	68.984594	58.568449
2439.842311	67.593453	58.573453
2439.685849	68.820564	58.578458
2438.924015	72.052959	58.583463
2438.547361	77.860597	58.588468
2438.194135	72.035659	58.593473
2437.067099	59.321681	58.598477
2436.459841	62.605011	58.603482
2435.621848	71.678130	58.608487
2435.154148	65.127923	58.613492
2434.713010	74.013589	58.618497
2434.037627	69.658425	58.623501
2433.326440	66.311588	58.628506
2432.045436	68.436737	58.633511
2432.263671	65.220321	58.638516
2431.056361	69.651478	58.643521
2429.859291	66.531001	58.648525
2429.393136	74.219800	58.653530
2428.876293	78.195415	58.658535
2428.807938	70.442885	58.663540
2428.229729	72.118278	58.668545
2427.513756	68.750944	58.673549
2426.215814	70.464925	58.678554
2425.315709	81.029674	58.683559
2425.129466	79.188556	58.688564
2424.520869	77.416099	58.693569
2424.360730	71.897611	58.698573
2423.777690	75.393508	58.703578
2422.348185	75.859368	58.708583
2422.342308	70.187405	58.713588
2421.333539	74.502515	58.718593
2420.581369	68.233835	58.723597
2419.836269	69.274627	58.728602
2418.458907	80.216626	58.733607
2418.400728	59.809881	58.738612
2417.998794	72.168332	58.743617
2417.751992	74.120208	58.748621
2416.703214	67.996977	58.753626
2415.455569	74.283131	58.758631
2415.071373	66.754733	58.763636
2414.586423	66.453193	58.768641
2413.781987	67.025726	58.773645
2414.130339	55.560630	58.778650
2412.968665	60.810140	58.783655
2412.242703	64.062850	58.788660
2411.210012	68.184689	58.793665
2410.764474	66.937757	58.798669
2409.560204	61.124134	58.803674
2408.921761	65.043962	58.808679
2408.397438	61.772544	58.813684
2407.593451	66.573281	58.818689
2407.261516	67.691452	58.823693
2406.970711	64.110115	58.828698
2406.407562	78.285417	58.833703
2405.953376	70.521494	58.838708
2405.029923	69.697714	58.843713
2404.090728	65.467793	58.848717
2403.517137	61.231806	58.853722
2402.402195	71.080150	58.858727
2402.273243	59.399436	58.863732
2401.542194	65.226219	58.868737
2401.339046	66.799591	58.873741
2400.323191	69.682673	58.878746
2399.009377	69.430886	58.883751
2398.658173	70.554326	58.888756
2398.168175	75.204277	58.893761
2397.620568	73.660993	58.898765
2397.214658	64.192692	58.903770
2396.120031	65.551005	58.908775
2395.264797	67.902562	58.913780
2394.294208	75.606957	58.918785
2394.032338	77.875610	58.923789
2393.803926	71.323570	58.928794
2392.947513	80.021701	58.933799
2392.077271	75.435790	58.938804
2391.478931	72.399257	58.943809
2390.708148	73.738514	58.948813
2390.191393	71.247750	58.953818
2389.473965	66.406774	58.958823
2388.996300	70.906988	58.963828
2388.037003	69.014508	58.968833
2387.423549	74.617906	58.973837
2387.004333	61.323457	58.978842
2386.350252	72.985703	58.983847
2385.657122	58.614709	58.988852
2384.577398	72.545580	58.993857
2384.248123	68.396104	58.998861
2383.603649	65.027605	59.003866
2383.305029	73.342209	59.008871
2382.987840	56.238605	59.013876
2381.629844	74.586252	59.018881
2381.059278	77.716478	59.023885
2380.841516	67.547345	59.028890
2379.282420	75.791696	59.033895
2378.455397	60.666780	59.038900
2377.492824	65.927647	59.043905
2377.203601	71.864802	59.048909
2377.166523	65.434782	59.053914
2376.150289	63.406387	59.058919
2376.011987	61.051435	59.063924
2375.710728	76.790057	59.068929
2374.509701	75.808488	59.073933
2373.871262	67.403468	59.078938
2372.918620	68.200684	59.083943
2371.635430	65.322703	59.088948
2371.314118	69.101470	59.093953
2370.805205	69.250858	59.098957
2370.218622	59.699383	59.103962
2369.670377	72.063111	59.108967
2369.472356	65.756529	59.113972
2368.762706	55.089296	59.118977
2367.680011	65.714074	59.123981
2366.929095	56.569240	59.128986
2366.512593	65.196091	59.133991
2366.093859	61.303486	59.138996
2365.473073	57.350303	59.144001
2364.092310	67.866581	59.149005
2363.523777	61.018639	59.154010
2362.662752	72.850871	59.159015
2362.801727	58.820348	59.164020
2362.599582	64.289863	59.169025
2361.260474	62.025769	59.174029
2360.368942	58.435844	59.179034
2359.722839	60.580730	59.184039
2359.256365	58.459520	59.189044
2358.235460	62.191336	59.194049
2357.416235	64.274249	59.199053
2357.333054	56.308749	59.204058
2356.344827	67.173945	59.209063
2356.073967	58.317278	59.214068
2355.543860	59.647357	59.219073
2354.469734	65.515044	59.224077
2353.744230	51.045395	59.229082
2353.248872	66.587465	59.234087
2352.900788	64.082865	59.239092
2351.917479	65.746220	59.244097
2350.500098	73.154396	59.249101
2350.223424	64.519766	59.254106
2349.590162	67.377696	59.259111
2349.270250	65.033274	59.264116
2348.753514	65.605567	59.269121
2348.597838	70.458079	59.274125
2347.924719	64.108401	59.279130
2346.787794	68.324254	59.284135
2346.156474	63.552244	59.289140
2345.256942	66.836613	59.294145
2344.494980	69.044337	59.299149
2344.105881	60.724976	59.304154
2343.007491	59.158254	59.309159
2342.759060	70.213520	59.314164
2342.375429	65.945848	59.319169
2340.992005	66.954094	59.324173
2340.700176	70.917682	59.329178
2339.866198	74.374391	59.334183
2339.412499	64.327712	59.339188
2338.947516	67.000558	59.344193
2337.568906	65.456490	59.349197
2337.022175	65.445381	59.354202
2336.483746	75.733161	59.359207
2336.174003	68.723736	59.364212
2335.749171	65.897141	59.369217
2334.711104	72.783764	59.374221
2333.920036	75.188303	59.379226
2333.102573	72.810148	59.384231
2332.377264	64.336311	59.389236
2332.141035	72.824580	59.394241
2331.693403	75.191313	59.399245
2331.525453	68.162379	59.404250
2330.039483	80.267659	59.409255
2329.401459	76.977403	59.414260
2329.342149	70.828282	59.419265
2327.970805	74.765682	59.424269
2327.242578	65.226986	59.429274
2326.523948	65.647495	59.434279
2326.469553	68.275790	59.439284
2325.763789	70.622717	59.444289
2324.563895	70.996052	59.449293
2323.662947	66.682242	59.454298
2322.740280	67.542233	59.459303
2322.641528	62.914019	59.464308
2322.861819	68.239459	59.469313
2322.114715	74.676870	59.474317
2321.173679	62.658600	59.479322
2320.100506	69.968449	59.484327
2319.936656	68.099036	59.489332
2319.250442	66.006720	59.494337
2317.514995	68.525775	59.499341
2316.971086	68.867068	59.504346
2316.325240	72.952375	59.509351
2315.884005	60.491812	59.514356
2315.773889	67.896707	59.519361
2315.382284	72.385761	59.524365
2314.647551	68.559828	59.529370
2313.708243	71.176027	59.534375
2312.880022	69.331408	59.539380
2312.375468	64.572067	59.544385
2311.677726	79.175761	59.549389
2311.098530	71.200738	59.554394
2310.095784	66.463432	59.559399
2309.864354	67.883752	59.564404
2309.319612	58.488551	59.569409
2307.836835	66.990641	59.574413
2307.173327	63.168319	59.579418
2306.911198	71.200768	59.584423
2306.458604	63.655664	59.589428
2305.972451	70.946842	59.594433
2305.263554	68.260401	59.599437
2304.290298	64.146059	59.604442
2303.370099	71.140815	59.609447
2302.795631	75.506014	59.614452
2302.579139	63.876200	59.619457
2301.720252	72.395551	59.624461
2301.575650	64.096357	59.629466
2300.114030	73.886763	59.634471
2299.388939	72.409366	59.639476
2298.961243	66.748361	59.644481
2298.599973	67.341046	59.649485
2298.100660	63.619328	59.654490
2296.838113	70.292508	59.659495
2296.335658	59.496309	59.664500
2295.766323	66.497773	59.669505
2295.094295	68.347899	59.674509
2294.749463	66.431280	59.679514
2293.646177	65.412491	59.684519
2292.740680	57.993786	59.689524
2292.975769	69.392270	59.694529
2292.334447	65.934434	59.699533
2291.384305	58.205611	59.704538
2290.272381	67.546624	59.709543
2289.496333	62.394387	59.714548
2288.901345	69.528524	59.719553
2288.761637	69.400450	59.724557
2287.823550	69.223777	59.729562
2286.665585	68.551828	59.734567
2286.081965	69.666861	59.739572
2285.661039	64.660731	59.744577
2285.092878	75.608441	59.749581
2285.322623	66.055142	59.754586
2284.338227	67.621197	59.759591
2283.422049	57.312974	59.764596
2282.765702	59.638033	59.769601
2281.912452	66.724363	59.774605
2281.531779	60.757306	59.779610
2280.359397	68.200568	59.784615
2279.842046	59.441324	59.789620
2279.476868	64.145323	59.794625
2278.248018	67.470622	59.799629
2277.168122	60.514754	59.804634
2276.582352	65.174769	59.809639
2276.165758	65.882307	59.814644
2276.181969	59.275032	59.819649
2275.386926	62.959553	59.824653
2275.198423	55.438374	59.829658
2274.100270	62.303302	59.834663
2272.840570	62.469778	59.839668
2272.435838	59.327133	59.844673
2272.036241	59.760589	59.849677
2271.337532	61.210294	59.854682
2270.869315	62.624530	59.859687
2270.661918	59.735497	59.864692
2269.405117	63.409776	59.869697
2268.369357	66.695347	59.874701
2268.448031	58.459816	59.879706
2267.360680	63.613749	59.884711
2266.448290	64.235157	59.889716
2266.447661	57.110914	59.894721
2265.705516	69.990147	59.899725
2265.012764	60.178964	59.904730
2263.363809	68.141869	59.909735
2263.321221	58.422391	59.914740
2262.857115	61.179561	59.919745
2262.077558	72.785108	59.924750
2261.683391	70.456153	59.929754
2260.400887	63.942686	59.934759
2259.532185	64.021774	59.939764
2259.205808	61.728990	59.944769
2258.323920	66.793317	59.949774
2258.523562	66.718918	59.954778
2257.871372	66.847820	59.959783
2256.782773	67.982900	59.964788
2255.890455	63.973144	59.969793
2255.075791	67.349982	59.974798
2255.061219	54.106367	59.979802
2254.763398	67.995102	59.984807
2253.767993	62.639998	59.989812
2253.099445	65.117931	59.994817
2252.139117	63.794056	59.999822
2251.223196	63.387817	60.004826
2250.095704	70.074618	60.009831
2249.931694	62.944367	60.014836
2248.989783	65.038801	60.019841
2249.099216	61.515346	60.024846
2248.301717	56.604015	60.029850
2247.937881	60.013489	60.034855
2247.088940	61.454546	60.039860
2246.111378	54.342247	60.044865
2245.021114	65.886059	60.049870
2244.779669	68.653310	60.054874
2244.109485	67.981240	60.059879
2244.058997	61.480897	60.064884
2243.497792	57.695564	60.069889
2242.067424	63.456036	60.074894
2241.527086	55.225319	60.079898
2241.150723	64.337917	60.084903
2240.152399	62.702000	60.089908
2239.484870	62.816160	60.094913
2238.826718	69.968205	60.099918
2238.491611	59.632857	60.104922
2238.146544	63.659231	60.109927
2237.189322	65.284592	60.114932
2236.365354	59.852413	60.119937
2235.311656	68.616258	60.124942
2235.036773	58.578890	60.129946
2234.623793	57.921651	60.134951
2233.480662	65.181895	60.139956
2232.630590	62.272513	60.144961
2231.943679	64.307157	60.149966
2231.827251	65.375061	60.154970
2231.607033	67.948031	60.159975
2230.245041	59.508499	60.164980
2229.607269	61.046073	60.169985
2228.802855	70.465158	60.174990
2228.490906	57.176088	60.179994
2228.025008	61.641137	60.184999
2227.183563	72.209673	60.190004
2226.300098	60.509997	60.195009
2225.261245	65.108162	60.200014
2224.889197	54.352441	60.205018
2224.650847	62.926717	60.210023
2224.058756	62.406684	60.215028
2223.414025	69.169212	60.220033
2222.435914	73.855672	60.225038
2221.771839	59.912371	60.230042
2221.126637	63.183260	60.235047
2220.152667	67.613231	60.240052
2219.472455	61.513072	60.245057
2218.737769	64.823343	60.250062
2218.439941	63.728005	60.255066
2217.463708	66.905907	60.260071
2217.198467	55.838642	60.265076
2217.324704	56.093758	60.270081
2216.012288	55.630996	60.275086
2215.452750	53.743209	60.280090
2214.631481	54.335227	60.285095
2213.916442	47.283039	60.290100
2212.961902	53.948155	60.295105
2212.081775	63.071906	60.300110
2211.654599	56.597700	60.305114
2211.329035	66.654470	60.310119
2210.732533	68.586027	60.315124
2210.512380	60.478182	60.320129
2209.009566	63.287866	60.325134
2208.345830	49.713192	60.330138
2208.099751	65.326692	60.335143
2207.349361	62.909459	60.340148
2206.652762	61.439836	60.345153
2205.363267	66.405725	60.350158
2205.052064	58.206483	60.355162
2204.695234	65.554882	60.360167
2204.310278	67.933007	60.365172
2203.702224	59.189684	60.370177
2202.718372	61.380110	60.375182
2202.187063	57.230868	60.380186
2201.520859	61.132169	60.385191
2200.254333	59.154511	60.390196
2199.687427	65.988200	60.395201
2198.894890	72.356812	60.400206
2198.450214	72.825219	60.405210
2198.268780	65.656902	60.410215
2197.578932	75.165736	60.415220
2197.242206	67.476100	60.420225
2196.115701	67.961250	60.425230
2195.027247	65.114747	60.430234
2194.365601	68.633180	60.435239
2194.069976	62.068188	60.440244
2193.792402	61.066096	60.445249
2192.223589	59.749589	60.450254
2192.142052	55.084497	60.455258
2191.837407	61.299010	60.460263
2191.242012	65.941729	60.465268
2190.094311	53.932008	60.470273
2189.195162	65.287224	60.475278
2188.850513	59.816106	60.480282
2188.412873	64.979720	60.485287
2187.526732	65.797960	60.490292
2186.783752	62.488180	60.495297
2185.854093	60.354233	60.500302
2185.926091	56.916916	60.505306
2185.198130	60.124596	60.510311
2183.749262	69.530745	60.515316
2183.362831	57.752790	60.520321
2182.385249	66.813083	60.525326
2182.040798	63.169892	60.530330
2181.634276	56.711105	60.535335
2180.875181	62.615722	60.540340
2180.027935	54.890253	60.545345
2179.249872	67.658789	60.550350
2178.925296	61.306375	60.555354
2178.644501	58.489900	60.560359
2177.717570	64.927679	60.565364
2176.860521	52.298670	60.570369
2175.837027	63.213326	60.575374
2175.757867	57.632071	60.580378
2175.232813	65.600929	60.585383
2173.915042	66.800875	60.590388
2173.358170	64.466994	60.595393
2172.525356	70.020289	60.600398
2172.238537	62.405411	60.605402
2171.629842	66.379377	60.610407
2170.861729	64.854492	60.615412
2170.653260	64.727523	60.620417
2169.526734	69.535684	60.625422
2169.063215	66.481258	60.630426
2168.555929	64.414020	60.635431
2167.737276	67.023419	60.640436
2166.863424	56.581680	60.645441
2165.533621	58.269588	60.650446
2165.477369	63.454419	60.655450
2165.099832	59.494006	60.660455
2164.383472	68.019776	60.665460
2164.275566	55.669209	60.670465
2163.042528	64.520176	60.675470
2161.946784	58.175714	60.680474
2161.475623	53.679098	60.685479
2161.015231	55.236472	60.690484
2160.869407	58.926413	60.695489
2159.769595	55.440044	60.700494
2158.906137	61.399616	60.705498
2158.410691	64.777130	60.710503
2157.731339	70.838634	60.715508
2157.560278	56.604201	60.720513
2156.118719	64.331532	60.725518
2155.489654	52.159310	60.730522
2155.271792	55.917621	60.735527
2154.461688	54.656885	60.740532
2153.479342	56.004329	60.745537
2152.611140	65.303670	60.750542
2152.582924	63.188445	60.755546
2152.492208	59.572122	60.760551
2151.279775	65.846372	60.765556
2150.071178	57.891011	60.770561
2149.078361	68.087951	60.775566
2149.249194	57.920685	60.780570
2148.926579	56.536707	60.785575
2148.431480	67.369680	60.790580
2147.127493	54.532129	60.795585
2146.182995	62.127477	60.800590
2145.692204	52.991496	60.805594
2144.875966	57.682644	60.810599
2144.707718	67.083318	60.815604
2144.373238	60.348933	60.820609
2143.045898	54.896293	60.825614
2142.593095	56.368689	60.830618
2142.170842	57.990985	60.835623
2140.984606	69.488066	60.840628
2140.411611	55.260409	60.845633
2139.586138	66.604211	60.850638
2139.117797	60.756768	60.855642
2138.763712	56.675115	60.860647
2138.642985	60.208796	60.865652
2137.339654	52.313852	60.870657
2136.316318	64.848030	60.875662
2135.861293	54.801229	60.880666
2135.587393	48.684492	60.885671
2134.314434	57.769252	60.890676
2133.780247	57.787596	60.895681
2133.239568	63.834855	60.900686
2132.746559	61.919910	60.905690
2132.705123	63.713119	60.910695
2131.056484	60.532590	60.915700
2130.321962	64.031913	60.920705
2129.955771	55.304082	60.925710
2129.220327	57.045074	60.930714
2128.944349	52.715205	60.935719
2127.720981	53.257591	60.940724
2127.318527	52.563035	60.945729
2126.127340	55.656139	60.950734
2125.964621	52.732635	60.955738
2125.538830	41.053012	60.960743
2124.991384	52.040579	60.965748
2124.122501	48.793002	60.970753
2123.050943	51.037123	60.975758
2122.609982	50.845320	60.980762
2122.585407	58.535556	60.985767
2121.540752	60.788498	60.990772
2120.950922	48.174199	60.995777
2119.757126	49.771752	61.000782
2119.148958	52.958948	61.005786
2119.149734	56.271722	61.010791
2118.288223	52.266597	61.015796
2117.109783	42.776943	61.020801
2116.288424	55.413142	61.025806
2115.837701	51.157371	61.030810
2115.448479	61.729082	61.035815
2114.477880	68.920362	61.040820
2114.791308	56.324851	61.045825
2113.726216	62.706532	61.050830
2113.095824	60.378524	61.055834
2112.651757	43.861153	61.060839
2111.343184	55.930183	61.065844
2111.072901	49.331664	61.070849
2110.090115	57.925498	61.075854
2109.430156	58.037984	61.080858
2109.414996	59.080674	61.085863
2107.795949	59.014581	61.090868
2107.206082	51.222216	61.095873
2106.521997	55.089873	61.100878
2106.088798	56.078936	61.105882
2105.747083	54.983219	61.110887
2104.841077	56.827989	61.115892
2104.406331	40.803617	61.120897
2103.255630	54.314403	61.125902
2102.559721	47.355674	61.130906
2102.578629	48.961725	61.135911
2101.773421	42.568383	61.140916
2101.390941	44.588862	61.145921
2100.245414	45.670946	61.150926
2099.467558	49.704240	61.155930
2099.173195	47.854795	61.160935
2098.084048	45.121722	61.165940
2097.621639	45.188185	61.170945
2096.871733	50.153769	61.175950
2096.025857	48.945738	61.180954
2095.883380	42.776136	61.185959
2095.015721	46.870973	61.190964
2094.364528	41.315731	61.195969
2093.537339	48.188802	61.200974
2092.912170	45.826355	61.205978
2092.763146	48.122287	61.210983
2091.583522	54.845650	61.215988
2090.639529	46.377310	61.220993
2090.307547	58.284833	61.225998
2089.380080	54.195078	61.231002
2089.208014	51.059631	61.236007
2088.624974	50.269655	61.241012
2087.449795	52.645580	61.246017
2086.504730	56.283151	61.251022
2086.316711	55.532185	61.256026
2085.901607	48.860549	61.261031
2085.471531	57.098542	61.266036
2084.493618	39.875550	61.271041
2083.758035	47.928960	61.276046
2083.166877	50.227098	61.281050
2082.514660	42.236204	61.286055
2081.916816	66.012704	61.291060
2080.997353	56.177189	61.296065
2080.265972	54.561566	61.301070
2079.946686	52.444026	61.306074
2079.832202	60.427523	61.311079
2078.518400	63.262145	61.316084
2077.857301	56.356672	61.321089
2076.983381	64.230076	61.326094
2076.503669	62.237471	61.331098
2075.879934	52.360061	61.336103
2074.402517	61.240996	61.341108
2074.347845	47.301667	61.346113
2073.750142	57.131430	61.351118
2073.449132	56.584126	61.356122
2072.908443	49.215578	61.361127
2071.840681	53.112548	61.366132
2071.256266	50.273414	61.371137
2070.381921	55.677112	61.376142
2069.765452	52.562813	61.381146
2069.756831	47.430144	61.386151
2068.413335	66.603838	61.391156
2067.736860	50.566340	61.396161
2067.089239	59.669276	61.401166
2066.843777	66.108526	61.406170
2066.080557	58.624096	61.411175
2064.626476	64.502340	61.416180
2064.391347	58.287005	61.421185
2063.543918	57.869084	61.426190
2063.018225	57.066539	61.431194
2062.754397	46.544571	61.436199
2062.034561	50.630312	61.441204
2061.721953	38.927396	61.446209
2061.286914	51.527908	61.451214
2060.673545	50.242616	61.456218
2059.617352	48.622557	61.461223
2058.216111	56.167749	61.466228
2057.839070	45.544363	61.471233
2057.305128	55.399928	61.476238
2056.478472	48.668038	61.481242
2055.951951	44.207355	61.486247
2054.661283	56.550029	61.491252
2054.612256	52.130429	61.496257
2054.171212	55.951782	61.501262
2053.296786	56.251348	61.506266
2052.936873	61.165231	61.511271
2052.288487	58.786628	61.516276
2051.122480	59.110807	61.521281
2050.674804	62.139116	61.526286
2050.062468	62.337802	61.531290
2049.751330	55.890349	61.536295
2048.873514	58.116344	61.541300
2047.725497	60.617891	61.546305
2047.107284	64.470735	61.551310
2046.777569	58.962740	61.556314
2046.421769	56.770530	61.561319
2045.465919	64.018501	61.566324
2044.221389	57.592156	61.571329
2043.877230	58.019698	61.576334
2043.453979	55.169183	61.581338
2043.154791	50.476991	61.586343
2042.341750	69.377199	61.591348
2041.452963	54.017840	61.596353
2040.438370	53.679435	61.601358
2040.141484	60.572330	61.606362
2040.200667	54.034695	61.611367
2038.754171	54.228834	61.616372
2037.537140	55.610519	61.621377
2036.874520	55.036654	61.626382
2036.705484	56.294735	61.631386
2036.493844	55.768855	61.636391
2035.762590	64.104157	61.641396
2035.349011	55.941399	61.646401
2034.224017	55.107557	61.651406
2033.369254	57.018570	61.656410
2032.804300	48.928681	61.661415
2032.161826	66.693305	61.666420
2032.033063	59.581918	61.671425
2031.219054	58.235426	61.676430
2030.485576	62.924272	61.681434
2029.758346	51.833044	61.686439
2028.578909	61.783632	61.691444
2028.210278	59.241920	61.696449
2027.734011	58.940511	61.701454
2027.264485	61.142458	61.706458
2026.590120	52.501700	61.711463
2025.591452	63.386068	61.716468
2024.995093	48.651278	61.721473
2024.114113	55.036210	61.726478
2023.673944	60.393278	61.731482
2023.286132	49.188734	61.736487
2022.207415	60.146790	61.741492
2021.940918	60.803409	61.746497
2021.354353	48.174365	61.751502
2020.224912	54.934153	61.756506
2019.203497	50.609047	61.761511
2018.483086	57.031643	61.766516
2018.185761	56.379900	61.771521
2017.818766	58.680752	61.776526
2017.322285	59.971951	61.781530
2017.087182	54.941574	61.786535
2015.316360	60.005224	61.791540
2014.839136	53.671446	61.796545
2014.161459	56.675154	61.801550
2013.472130	59.927556	61.806554
2013.436576	60.783477	61.811559
2011.837206	61.627829	61.816564
2011.524996	58.520700	61.821569
2011.207830	62.519412	61.826574
2010.194088	57.008038	61.831578
2009.985262	49.673520	61.836583
2009.731658	62.728116	61.841588
2008.676937	52.589325	61.846593
2007.680310	57.123456	61.851598
2007.070367	55.688774	61.856602
2006.825808	53.668190	61.861607
2005.107039	66.335544	61.866612
2004.814166	50.548620	61.871617
2004.279850	52.934933	61.876622
2003.322681	52.299750	61.881626
2003.484614	45.707835	61.886631
2003.149689	51.045714	61.891636
2002.049543	54.802978	61.896641
2001.159655	53.386185	61.901646
2000.467055	61.585011	61.906650
2000.288826	48.801258	61.911655
1999.226550	55.291412	61.916660
1998.332534	56.991653	61.921665
1997.726733	54.591959	61.926670
1997.129804	53.975284	61.931674
1996.901363	42.777829	61.936679
1995.838902	51.601606	61.941684
1995.218978	56.846138	61.946689
1994.775903	54.073622	61.951694
1993.774386	59.083442	61.956698
1993.850980	56.834640	61.961703
1992.450698	52.003185	61.966708
1991.536451	55.335114	61.971713
1991.182523	51.842377	61.976718
1991.082253	49.947107	61.981722
1990.151069	59.193283	61.986727
1989.587476	56.688874	61.991732
1988.558090	52.384874	61.996737
1988.039727	45.974460	62.001742
1987.130761	56.803220	62.006746
1986.650480	51.242441	62.011751
1985.631528	59.332099	62.016756
1985.056373	56.553362	62.021761
1984.772778	54.288809	62.026766
1983.871381	49.461621	62.031770
1984.069667	48.331564	62.036775
1982.633956	53.891297	62.041780
1982.009798	53.875311	62.046785
1981.328805	52.527783	62.051790
1980.897097	52.745314	62.056794
1979.888620	51.487753	62.061799
1979.045064	59.381230	62.066804
1978.245576	54.110704	62.071809
1978.052285	50.904293	62.076814
1977.333401	48.610786	62.081818
1976.727199	49.269071	62.086823
1976.054875	52.546986	62.091828
1975.553402	49.908800	62.096833
1974.658347	51.085821	62.101838
1974.234602	48.087379	62.106842
1974.151834	43.167525	62.111847
1972.818121	58.095102	62.116852
1972.205229	52.070318	62.121857
1971.516317	48.362134	62.126862
1970.967673	55.194675	62.131866
1970.456938	53.169497	62.136871
1969.286963	56.385312	62.141876
1968.669846	48.035159	62.146881
1968.200322	51.590608	62.151886
1967.529747	54.775466	62.156890
1966.594691	48.527516	62.161895
1965.715604	48.002137	62.166900
1965.206981	53.566696	62.171905
1964.905457	44.994013	62.176910
1964.508886	54.615691	62.181914
1964.079242	45.205222	62.186919
1962.722966	48.843285	62.191924
1962.214006	52.664813	62.196929
1961.947656	48.531859	62.201934
1960.842549	57.011636	62.206938
1959.807983	50.674924	62.211943
1958.906843	53.007943	62.216948
1958.335560	54.363256	62.221953
1957.782624	53.102769	62.226958
1957.304590	49.836521	62.231962
1957.521904	45.661882	62.236967
1957.194438	60.949413	62.241972
1956.241657	61.881322	62.246977
1955.329964	50.922718	62.251982
1954.187661	56.638309	62.256986
1953.359344	56.511994	62.261991
1952.425587	55.851896	62.266996
1951.690184	52.424025	62.272001
1952.021787	56.256887	62.277006
1951.477594	63.391816	62.282010
1950.359492	50.448339	62.287015
1949.524463	52.500849	62.292020
1949.108375	54.988122	62.297025
1948.778529	53.988276	62.302030
1947.981808	59.051091	62.307034
1946.956300	56.502553	62.312039
1946.281160	56.680022	62.317044
1945.586558	57.529874	62.322049
1945.408414	51.095210	62.327054
1944.333261	65.582660	62.332058
1943.486322	58.197050	62.337063
1942.586781	54.745945	62.342068
1941.980580	53.790219	62.347073
1941.610401	49.157549	62.352078
1941.106199	54.518861	62.357082
1940.990563	37.086840	62.362087
1940.226909	51.355601	62.367092
1938.872154	54.893152	62.372097
1938.355266	52.285633	62.377102
1937.968007	57.190379	62.382106
1937.341249	50.734570	62.387111
1935.845693	57.327273	62.392116
1935.164630	50.105522	62.397121
1935.126836	49.198606	62.402126
1934.299662	55.076598	62.407130
1934.285747	56.115915	62.412135
1933.483187	57.733418	62.417140
1932.200031	57.284273	62.422145
1931.997223	55.537199	62.427150
1931.048494	51.170469	62.432154
1930.821850	44.417673	62.437159
1929.868567	54.650882	62.442164
1928.879956	48.559729	62.447169
1928.872789	50.870078	62.452174
1927.956497	59.386635	62.457178
1927.673340	48.089605	62.462183
1926.198000	45.942881	62.467188
1925.423721	51.063828	62.472193
1925.072155	47.985941	62.477198
1924.471216	50.153929	62.482202
1924.624132	44.819958	62.487207
1923.527237	49.850443	62.492212
1922.607009	62.345281	62.497217
1922.372968	46.741729	62.502222
1921.074072	53.825770	62.507226
1920.202130	52.996819	62.512231
1919.587517	58.825820	62.517236
1919.407759	50.586375	62.522241
1918.830767	48.711875	62.527246
1918.418790	52.276823	62.532250
1917.336616	51.407657	62.537255
1916.406015	45.668939	62.542260
1915.782951	46.757598	62.547265
1915.593803	51.536086	62.552270
1914.596721	52.323613	62.557274
1913.877297	48.626185	62.562279
1913.095729	56.531560	62.567284
1912.347754	65.181952	62.572289
1912.648766	54.714947	62.577294
1911.865125	58.403082	62.582298
1910.813738	57.808902	62.587303
1909.721378	55.928230	62.592308
1909.436046	54.605785	62.597313
1909.604521	54.252506	62.602318
1908.445990	65.712105	62.607322
1907.355362	49.087113	62.612327
1906.505888	51.219861	62.617332
1905.831992	53.617034	62.622337
1905.125599	57.341294	62.627342
1904.242974	59.052232	62.632346
1904.000276	52.149425	62.637351
1903.047312	59.432044	62.642356
1902.728626	46.907198	62.647361
1902.392020	48.747347	62.652366
1901.907914	50.527075	62.657370
1901.019201	51.042654	62.662375
1899.966196	48.946051	62.667380
1899.335143	50.161994	62.672385
1899.032583	56.028001	62.677390
1897.769304	57.869979	62.682394
1897.226867	53.112052	62.687399
1896.948464	49.980995	62.692404
1896.263877	50.013250	62.697409
1896.182486	45.732614	62.702414
1894.903104	55.492688	62.707418
1894.155893	50.307970	62.712423
1893.531104	54.444569	62.717428
1893.148023	49.840164	62.722433
1892.370356	52.045100	62.727438
1891.230959	49.080681	62.732442
1890.521509	44.165811	62.737447
1890.265893	47.313236	62.742452
1889.693907	50.535311	62.747457
1889.149787	41.158257	62.752462
1887.922413	58.137960	62.757466
1887.437576	45.624175	62.762471
1886.859808	54.220182	62.767476
1886.333950	52.634557	62.772481
1885.815154	46.744872	62.777486
1884.862315	53.897211	62.782490
1884.375857	44.983956	62.787495
1883.586525	46.869980	62.792500
1882.841699	43.724382	62.797505
1882.923654	46.235395	62.802510
1881.631794	51.325292	62.807514
1881.032705	49.119459	62.812519
1880.585661	49.694870	62.817524
1879.487786	52.796134	62.822529
1878.681631	42.410400	62.827534
1877.808253	48.749834	62.832538
1877.847601	51.395631	62.837543
1877.120705	50.008605	62.842548
1876.772318	54.958805	62.847553
1875.996824	45.881851	62.852558
1874.463983	44.155490	62.857562
1874.185672	46.357889	62.862567
1874.043077	42.734278	62.867572
1873.347798	50.435424	62.872577
1872.299787	48.776112	62.877582
1871.488649	54.484794	62.882586
1871.035426	43.416996	62.887591
1870.767112	47.394323	62.892596
1869.704841	45.431543	62.897601
1869.049211	46.735375	62.902606
1868.110503	56.395724	62.907610
1867.900149	44.337861	62.912615
1867.428122	48.908964	62.917620
1866.781229	43.297372	62.922625
1865.876130	35.473734	62.927630
1864.912304	45.345602	62.932634
1864.649814	42.857590	62.937639
1864.053483	41.004959	62.942644
1862.639873	42.219399	62.947649
1862.141691	42.580937	62.952654
1861.900482	49.285095	62.957658
1861.710059	49.441619	62.962663
1861.013201	54.991020	62.967668
1859.456048	48.453227	62.972673
1859.494627	49.588163	62.977678
1858.576146	54.650107	62.982682
1858.107628	49.084573	62.987687
1856.994969	49.698470	62.992692
1855.752559	55.873290	62.997697
1855.785843	47.794767	63.002702
1855.414825	50.518270	63.007706
1855.070768	43.708995	63.012711
1853.675069	56.484511	63.017716
1852.778337	49.591768	63.022721
1852.356339	40.238038	63.027726
1852.029204	46.475336	63.032730
1851.352199	43.926405	63.037735
1851.304576	42.562902	63.042740
1849.920594	46.852677	63.047745
1848.935815	39.076619	63.052750
1848.493327	45.325362	63.057754
1848.218602	43.366792	63.062759
1846.916083	44.579203	63.067764
1845.933613	39.072790	63.072769
1845.619233	39.593928	63.077774
1845.212092	49.746729	63.082778
1845.032804	46.408464	63.087783
1844.831264	47.737633	63.092788
1843.920229	47.451020	63.097793
1843.096984	38.758416	63.102798
1842.231490	40.361040	63.107802
1841.179218	40.728566	63.112807
1840.530004	44.355419	63.117812
1839.605183	54.145624	63.122817
1839.157486	38.708120	63.127822
1838.958444	42.411105	63.132826
1838.301925	47.003510	63.137831
1837.245695	40.294768	63.142836
1836.099010	40.467272	63.147841
1835.892192	41.716426	63.152846
1835.322446	41.230115	63.157850
1835.158276	44.044144	63.162855
1833.905077	45.425744	63.167860
1833.198597	51.632423	63.172865
1832.625317	38.550391	63.177870
1831.833200	43.692158	63.182874
1831.861223	40.342900	63.187879
1831.402642	45.874821	63.192884
1830.117892	47.000516	63.197889
1829.614970	38.371923	63.202894
1829.093434	42.374810	63.207898
1828.060325	39.102499	63.212903
1826.939727	44.938730	63.217908
1826.298551	48.798279	63.222913
1826.033480	40.270696	63.227918
1825.353187	43.859053	63.232922
1825.088986	44.533049	63.237927
1824.754110	49.626588	63.242932
1823.607827	47.525829	63.247937
1822.895431	42.731472	63.252942
1822.093929	42.011272	63.257946
1821.666717	48.591337	63.262951
1820.514709	48.317142	63.267956
1820.430868	54.636365	63.272961
1819.873255	37.696024	63.277966
1819.321999	43.408399	63.282970
1818.223867	42.991967	63.287975
1817.590461	47.906064	63.292980
1816.750839	52.230996	63.297985
1816.644485	41.453587	63.302990
1815.339857	47.489062	63.307994
1814.361133	41.494141	63.312999
1813.719496	42.881239	63.318004
1812.926816	44.912312	63.323009
1813.025950	37.768676	63.328014
1812.541483	49.585426	63.333018
1812.181152	42.475401	63.338023
1811.472476	48.088401	63.343028
1810.306243	44.708218	63.348033
1809.500405	40.689688	63.353038
1809.314372	45.519348	63.358042
1808.146807	47.816660	63.363047
1807.139788	50.653717	63.368052
1806.285099	48.917924	63.373057
1806.364303	43.006462	63.378062
1805.789930	49.179487	63.383066
1805.788096	43.011111	63.388071
1805.256610	38.690653	63.393076
1803.781116	36.863719	63.398081
1803.648343	37.934421	63.403086
1802.446759	45.884030	63.408090
1801.232503	50.839091	63.413095
1800.482278	51.476643	63.418100
1799.946307	55.875542	63.423105
1799.881525	44.534069	63.428110
1799.323933	50.348185	63.433114
1798.438891	44.057776	63.438119
1797.480318	45.038069	63.443124
1796.922438	44.666963	63.448129
1796.509152	44.995036	63.453134
1796.357803	51.166734	63.458138
1795.212071	43.560721	63.463143
1794.487601	41.735155	63.468148
1793.479745	51.249054	63.473153
1793.584228	50.789884	63.478158
1792.418497	46.292559	63.483162
1791.425176	51.150613	63.488167
1790.601938	39.848523	63.493172
1790.141240	48.739484	63.498177
1789.857992	39.199007	63.503182
1789.565336	46.461810	63.508186
1788.957144	40.498231	63.513191
1787.974667	42.866110	63.518196
1786.743489	50.065291	63.523201
1786.863988	46.161417	63.528206
1786.295607	53.861382	63.533210
1784.894618	46.993753	63.538215
1784.276799	45.205201	63.543220
1783.866215	47.549439	63.548225
1783.682651	45.442255	63.553230
1782.545918	46.926303	63.558234
1781.433743	45.103523	63.563239
1780.688765	42.968849	63.568244
1780.041166	47.699464	63.573249
1780.040184	39.069864	63.578254
1779.722882	47.500913	63.583258
1779.146623	43.795199	63.588263
1778.328779	44.583265	63.593268
1777.224122	45.118050	63.598273
1776.992772	40.524410	63.603278
1775.579559	52.486647	63.608282
1774.614268	53.915313	63.613287
1774.786350	48.722139	63.618292
1773.468345	49.179354	63.623297
1773.670864	42.756946	63.628302
1773.246329	50.542425	63.633306
1772.432182	42.856396	63.638311
1771.452931	40.307090	63.643316
1770.465044	48.100540	63.648321
1770.227782	41.722197	63.653326
1769.186534	40.761591	63.658330
1768.673858	40.085925	63.663335
1768.156580	44.525437	63.668340
1767.948423	51.962065	63.673345
1766.742947	36.997250	63.678350
1765.704016	37.934853	63.683354
1765.235877	45.777524	63.688359
1764.853740	38.121394	63.693364
1764.500564	41.260645	63.698369
1763.406829	36.288006	63.703374
1762.155273	45.694398	63.708378
1761.841094	40.946781	63.713383
1761.652902	32.741570	63.718388
1760.945423	42.289331	63.723393
1760.737800	33.725092	63.728398
1759.130182	37.226605	63.733402
1758.654403	30.588301	63.738407
1758.338192	39.160864	63.743412
1757.777071	43.633534	63.748417
1756.780031	43.851896	63.753422
1755.785934	47.140283	63.758426
1755.410724	40.584238	63.763431
1755.170287	34.515508	63.768436
1754.024125	51.642755	63.773441
1753.578865	40.917817	63.778446
1752.859205	41.027142	63.783450
1752.478523	37.957414	63.788455
1751.999709	43.465169	63.793460
1750.415406	45.518810	63.798465
1750.087728	42.453038	63.803470
1749.531424	43.264645	63.808474
1749.165557	41.171683	63.813479
1748.579819	37.374837	63.818484
1747.190455	48.543555	63.823489
1747.011301	42.962475	63.828494
1746.258651	46.514275	63.833498
1745.364670	46.307258	63.838503
1745.142947	47.365157	63.843508
1743.988806	43.679382	63.848513
1743.446701	37.479909	63.853518
1742.802294	41.694869	63.858522
1742.077105	43.128244	63.863527
1742.122028	34.249621	63.868532
1740.569791	43.724042	63.873537
1740.308105	39.555973	63.878542
1739.318289	37.623062	63.883546
1738.756972	32.735770	63.888551
1738.601687	39.198254	63.893556
1737.592718	46.081932	63.898561
1736.959515	36.788441	63.903566
1736.020094	37.167861	63.908570
1735.650857	37.308804	63.913575
1735.187512	36.829166	63.918580
1734.174874	35.877882	63.923585
1734.301233	37.963675	63.928590
1732.944838	33.584649	63.933594
1732.475840	43.661582	63.938599
1732.156191	40.932713	63.943604
1730.504621	42.708540	63.948609
1729.833663	39.995970	63.953614
1729.439354	37.875904	63.958618
1728.897851	36.691250	63.963623
1728.566509	29.411685	63.968628
1727.910239	38.699641	63.973633
1727.525942	43.288894	63.978638
1726.500817	39.041861	63.983642
1725.629133	31.838964	63.988647
1725.503351	28.830621	63.993652
1724.643515	43.829484	63.998657
1723.536651	37.556525	64.003662
1722.877164	34.927648	64.008666
1722.317652	36.032294	64.013671
1722.051953	29.453573	64.018676
1721.512454	48.391402	64.023681
1720.543175	33.321854	64.028686
1719.684850	27.793445	64.033690
1719.301857	43.126354	64.038695
1719.013778	42.648700	64.043700
1717.961717	42.212958	64.048705
1717.579478	38.498923	64.053710
1716.776786	32.505091	64.058714
1715.271869	42.522843	64.063719
1714.986402	41.129386	64.068724
1714.464220	38.345969	64.073729
1713.832535	34.352526	64.078734
1713.565821	39.558341	64.083738
1712.427292	42.552120	64.088743
1711.998175	33.759351	64.093748
1710.806607	35.992500	64.098753
1710.592054	36.680504	64.103758
1710.074784	35.649988	64.108762
1709.420966	40.392328	64.113767
1708.826569	38.505046	64.118772
1707.635779	36.316806	64.123777
1707.051273	33.964431	64.128782
1706.694927	38.756523	64.133786
1706.179120	37.345246	64.138791
1705.008965	44.464131	64.143796
1704.077816	42.336458	64.148801
1704.250534	45.340726	64.153806
1703.300528	44.058218	64.158810
1702.606520	40.965533	64.163815
1702.484481	34.210263	64.168820
1701.314392	41.224534	64.173825
1700.821540	38.648459	64.178830
1700.242610	36.895895	64.183834
1699.491741	37.548965	64.188839
1698.237285	36.635909	64.193844
1697.670710	47.746339	64.198849
1697.456920	38.488059	64.203854
1696.969177	41.001813	64.208858
1695.649198	43.344173	64.213863
1695.278208	31.185947	64.218868
1694.364702	42.176535	64.223873
1694.133400	32.535614	64.228878
1693.653319	38.087399	64.233882
1693.133026	44.093679	64.238887
1692.447642	35.593043	64.243892
1691.679121	40.483295	64.248897
1691.015727	27.938942	64.253902
1689.759156	34.237779	64.258906
1688.692902	42.702643	64.263911
1688.254170	33.079454	64.268916
1687.913565	41.602113	64.273921
1687.556486	37.655627	64.278926
1687.008932	35.759544	64.283930
1686.578564	31.822443	64.288935
1686.028884	30.483674	64.293940
1684.732570	39.126450	64.298945
1684.420911	36.582132	64.303950
1683.764678	37.762146	64.308954
1682.490362	34.400493	64.313959
1682.121543	33.463783	64.318964
1681.462928	41.377729	64.323969
1681.295069	29.734988	64.328974
1680.125438	33.465903	64.333978
1679.037290	38.527292	64.338983
1678.675822	34.344728	64.343988
1677.982072	39.046141	64.348993
1677.896284	36.362126	64.353998
1677.297434	35.028613	64.359002
1676.325184	36.454932	64.364007
1675.744981	32.745174	64.369012
1674.752150	38.325492	64.374017
1674.525937	36.734802	64.379022
1673.418897	39.427949	64.384026
1672.704560	40.186477	64.389031
1671.995476	34.850424	64.394036
1671.478972	35.854166	64.399041
1671.193735	29.161563	64.404046
1670.568254	32.926860	64.409050
1669.252768	32.988949	64.414055
1668.916142	29.795646	64.419060
1668.150236	43.279685	64.424065
1667.624045	33.311876	64.429070
1667.574321	32.981324	64.434074
1666.228550	44.043911	64.439079
1665.970850	34.643552	64.444084
1665.301881	37.152794	64.449089
1664.676078	31.290935	64.454094
1663.301322	39.497552	64.459098
1662.486206	40.964087	64.464103
1662.366438	41.924019	64.469108
1661.952067	44.187204	64.474113
1661.106215	35.771268	64.479118
1659.957799	49.624308	64.484122
1659.110636	48.625381	64.489127
1659.409841	30.795217	64.494132
1658.529954	39.935528	64.499137
1657.876082	37.392538	64.504142
1657.060101	37.740981	64.509146
1656.414360	40.872276	64.514151
1656.143433	32.216256	64.519156
1655.070902	33.508167	64.524161
1654.694836	43.755503	64.529166
1653.536228	42.881712	64.534170
1652.936632	51.447115	64.539175
1652.495979	35.488216	64.544180
1651.895274	47.072228	64.549185
1651.320829	45.222195	64.554190
1650.249864	38.485238	64.559194
1649.386852	36.791951	64.564199
1649.405462	35.098186	64.569204
1648.789248	48.332807	64.574209
1647.867750	37.142702	64.579214
1647.146966	39.896856	64.584218
1645.618654	43.374567	64.589223
1646.080704	39.359752	64.594228
1645.515752	44.975010	64.599233
1644.809078	42.812488	64.604238
1643.665156	40.187973	64.609242
1643.059283	43.076009	64.614247
1642.683923	36.206995	64.619252
1642.009215	46.124533	64.624257
1641.512388	37.404938	64.629262
1640.621989	35.968170	64.634266
1639.657467	41.089327	64.639271
1639.012874	38.653696	64.644276
1638.934901	47.191410	64.649281
1638.197748	44.813852	64.654286
1637.245054	40.762858	64.659290
1636.442090	45.327051	64.664295
1635.943868	42.704931	64.669300
1635.277925	47.984988	64.674305
1634.052011	50.188508	64.679310
1633.484224	47.142915	64.684314
1633.019549	47.164808	64.689319
1633.238151	44.313051	64.694324
1632.474803	46.423204	64.699329
1631.551383	37.662143	64.704334
1630.641731	44.618438	64.709338
1629.796171	49.718058	64.714343
1629.732677	49.091059	64.719348
1628.602638	48.445664	64.724353
1627.396934	50.318110	64.729358
1627.296799	51.466911	64.734362
1626.122811	52.414627	64.739367
1626.220686	43.844303	64.744372
1625.667493	48.098925	64.749377
1625.269634	40.782991	64.754382
1624.309752	50.350667	64.759386
1623.567623	54.187643	64.764391
1622.892254	38.702317	64.769396
1621.352761	49.968189	64.774401
1620.671468	46.421782	64.779406
1620.404746	45.375635	64.784410
1619.813729	57.629415	64.789415
1619.635943	42.043542	64.794420
1619.080422	43.148699	64.799425
1618.685548	39.777480	64.804430
1617.671198	38.986769	64.809434
1617.179808	43.826840	64.814439
1616.620925	38.077478	64.819444
1615.521348	46.794754	64.824449
1614.395002	32.197367	64.829454
1614.541923	30.157975	64.834458
1613.882550	44.752682	64.839463
1613.134469	34.801936	64.844468
1612.081000	38.700083	64.849473
1611.575008	48.636511	64.854478
1610.737652	38.405791	64.859482
1609.285113	38.119130	64.864487
1608.947576	32.956337	64.869492
1608.572525	40.997410	64.874497
1607.499146	32.577007	64.879502
1607.807307	38.833865	64.884506
1607.035249	43.489873	64.889511
1607.025796	38.471451	64.894516
1605.705640	44.092008	64.899521
1604.836775	43.884270	64.904526
1604.688059	44.538907	64.909530
1603.751952	51.373819	64.914535
1602.929481	40.866222	64.919540
1602.167417	47.926732	64.924545
1601.657320	49.477651	64.929550
1601.363334	35.055177	64.934554
1599.977075	43.804541	64.939559
1599.113668	43.833887	64.944564
1598.311239	49.088753	64.949569
1598.087659	38.923517	64.954574
1597.754923	33.366763	64.959578
1597.324326	51.241519	64.964583
1596.820279	37.625486	64.969588
1595.360736	49.348581	64.974593
1594.787539	43.568907	64.979598
1594.525771	34.042551	64.984602
1593.809572	42.749479	64.989607
1593.275970	29.184300	64.994612
1592.386410	37.636301	64.999617
1591.817205	31.176243	65.004622
1591.308987	34.245324	65.009626
1590.188512	44.774388	65.014631
1589.717593	36.241019	65.019636
1589.217265	42.050473	65.024641
1588.682465	42.602243	65.029646
1587.384430	37.102928	65.034650
1586.505989	38.669122	65.039655
1585.845949	37.253729	65.044660
1585.226638	49.880222	65.049665
1584.999507	39.544287	65.054670
1584.818717	32.280422	65.059674
1584.063178	46.555286	65.064679
1583.358731	34.103242	65.069684
1582.646664	41.965554	65.074689
1581.439021	35.555153	65.079694
1581.478494	38.336699	65.084698
1580.586068	39.441098	65.089703
1579.755444	31.706628	65.094708
1578.980560	38.298824	65.099713
1578.821169	33.848410	65.104718
1578.261072	30.597837	65.109722
1576.935189	41.226392	65.114727
1576.521157	39.366680	65.119732
1575.833257	39.154424	65.124737
1575.221077	40.339146	65.129742
1574.710599	33.005394	65.134746
1573.454944	41.307693	65.139751
1572.883571	34.808141	65.144756
1572.459330	34.674705	65.149761
1571.671904	34.016871	65.154766
1571.762177	38.336233	65.159770
1570.808593	43.181593	65.164775
1569.617945	38.485711	65.169780
1569.056964	39.425630	65.174785
1568.334698	34.791690	65.179790
1568.304210	37.389428	65.184794
1566.967600	47.048025	65.189799
1566.142963	30.478319	65.194804
1565.962772	46.694231	65.199809
1565.418226	32.403855	65.204814
1564.777076	34.595334	65.209818
1563.919860	36.561698	65.214823
1563.470080	36.133436	65.219828
1562.768108	40.229188	65.224833
1562.422727	34.719600	65.229838
1561.338958	30.109243	65.234842
1560.835204	42.053615	65.239847
1560.090961	39.237567	65.244852
1559.277281	38.832901	65.249857
1558.453296	41.766562	65.254862
1558.101193	35.084624	65.259866
1556.669415	38.340977	65.264871
1556.657631	28.719745	65.269876
1556.522133	31.197695	65.274881
1555.699098	41.052200	65.279886
1554.627183	40.393322	65.284890
1553.411427	39.464206	65.289895
1553.300340	35.434981	65.294900
1552.998556	36.461983	65.299905
1552.350544	38.311233	65.304910
1551.156620	30.561187	65.309914
1550.125334	41.371423	65.314919
1550.221666	37.665893	65.319924
1549.443495	38.114061	65.324929
1549.065685	26.299653	65.329934
1548.157234	28.999096	65.334938
1546.938039	34.294106	65.339943
1546.593210	36.941693	65.344948
1546.406204	33.620957	65.349953
1545.790565	34.217354	65.354958
1545.151155	34.663089	65.359962
1544.249779	41.272201	65.364967
1543.434367	33.337776	65.369972
1542.966420	41.043841	65.374977
1542.045126	29.984785	65.379982
1541.871710	27.850223	65.384986
1540.811275	39.222790	65.389991
1540.293073	34.567746	65.394996
1539.183019	40.901139	65.400001
1538.242177	37.032869	65.405006
1538.310049	35.868677	65.410010
1537.718143	37.501493	65.415015
1537.830664	37.045285	65.420020
1536.295123	36.081302	65.425025
1535.228271	39.189946	65.430030
1534.170453	37.182667	65.435034
1533.954158	37.668879	65.440039
1533.475391	33.733765	65.445044
1533.017222	37.122692	65.450049
1532.218685	36.591892	65.455054
1531.730356	40.811339	65.460058
1530.728259	41.970040	65.465063
1530.587610	36.124641	65.470068
1529.795536	35.813384	65.475073
1528.349045	33.605797	65.480078
1528.227562	25.844708	65.485082
1527.112849	36.438310	65.490087
1526.759075	28.643558	65.495092
1526.519816	36.372058	65.500097
1526.132687	33.903826	65.505102
1525.435014	33.295373	65.510106
1524.863899	38.646438	65.515111
1524.014781	30.035713	65.520116
1522.903932	33.035841	65.525121
1521.890272	37.005343	65.530126
1521.775649	33.616960	65.535130
1521.302057	34.571926	65.540135
1520.926538	31.572390	65.545140
1519.690122	35.507784	65.550145
1518.735922	38.299927	65.555150
1518.064198	34.075354	65.560154
1517.670056	36.385608	65.565159
1516.543929	30.102587	65.570164
1515.857332	38.592486	65.575169
1515.162238	43.806490	65.580174
1514.927636	38.119665	65.585178
1514.181261	40.713616	65.590183
1513.778359	42.053177	65.595188
1514.011219	38.627820	65.600193
1512.635800	32.083138	65.605198
1512.273646	37.148977	65.610202
1511.602509	39.179812	65.615207
1510.793367	37.532197	65.620212
1509.793994	34.998234	65.625217
1509.076748	42.836964	65.630222
1508.491899	32.183339	65.635226
1507.272026	41.971956	65.640231
1506.606165	39.628401	65.645236
1506.168114	34.120472	65.650241
1505.477934	38.404465	65.655246
1505.087668	35.912300	65.660250
1504.855440	39.410183	65.665255
1504.391642	33.181562	65.670260
1503.644672	30.786367	65.675265
1502.594168	38.263336	65.680270
1502.017957	32.301839	65.685274
1501.202536	38.112725	65.690279
1500.312610	36.377890	65.695284
1499.506148	38.579513	65.700289
1498.838802	39.742503	65.705294
1498.649269	33.661143	65.710298
1498.295174	41.680865	65.715303
1497.439508	39.261250	65.720308
1496.313016	35.051360	65.725313
1495.661986	32.719875	65.730318
1495.385114	28.144319	65.735322
1495.004284	42.267812	65.740327
1493.943069	26.355178	65.745332
1493.031061	29.756258	65.750337
1492.667549	41.894114	65.755342
1492.517506	27.746232	65.760346
1491.183669	38.675355	65.765351
1490.093810	41.899256	65.770356
1489.459451	37.074240	65.775361
1489.019601	34.504120	65.780366
1488.835352	34.879064	65.785370
1488.181793	43.009249	65.790375
1487.681517	36.283606	65.795380
1486.967472	35.646382	65.800385
1486.294012	50.884919	65.805390
1485.657807	38.387668	65.810394
1484.156487	43.799266	65.815399
1483.439825	38.054038	65.820404
1482.890294	35.900962	65.825409
1482.465396	48.735746	65.830414
1482.797227	42.217797	65.835418
1481.960849	49.212486	65.840423
1481.130376	35.104089	65.845428
1480.035054	35.752200	65.850433
1479.357494	43.805577	65.855438
1478.979586	39.337703	65.860442
1477.933482	41.672709	65.865447
1477.184103	43.019472	65.870452
1476.434775	38.619907	65.875457
1476.223953	37.960499	65.880462
1475.727890	35.923004	65.885466
1474.435337	48.125538	65.890471
1473.804460	42.879946	65.895476
1473.306670	44.034049	65.900481
1472.810977	43.123018	65.905486
1472.584268	37.725361	65.910490
1471.615753	43.528904	65.915495
1470.563409	45.953398	65.920500
1470.094124	44.124072	65.925505
1469.441635	41.196813	65.930510
1469.248305	39.481302	65.935514
1468.080406	45.180032	65.940519
1467.542391	45.139101	65.945524
1466.799725	44.715980	65.950529
1466.021709	46.430392	65.955534
1465.654477	34.802860	65.960538
1464.728419	45.551281	65.965543
1463.835997	41.357780	65.970548
1463.206858	44.759002	65.975553
1462.492680	52.490640	65.980558
1462.674303	42.120285	65.985562
1461.981599	49.597599	65.990567
1461.035902	46.942752	65.995572
1460.448022	45.878956	66.000577
1459.547167	46.943767	66.005582
1459.241995	44.363623	66.010586
1458.475965	43.691882	66.015591
1457.554379	46.731468	66.020596
1457.119996	40.738596	66.025601
1456.216648	41.487664	66.030606
1455.347604	34.795937	66.035610
1454.571186	40.028205	66.040615
1454.018444	39.884012	66.045620
1453.709306	40.259413	66.050625
1453.118707	44.683072	66.055630
1452.972857	32.772531	66.060634
1451.755951	38.427546	66.065639
1451.214064	37.421403	66.070644
1450.600482	34.081323	66.075649
1449.278744	45.846769	66.080654
1448.850336	39.076464	66.085658
1448.208385	47.020332	66.090663
1447.587856	43.220013	66.095668
1447.637544	38.411731	66.100673
1446.408661	45.441631	66.105678
1445.719282	37.871297	66.110682
1444.607647	41.524834	66.115687
1444.376515	31.809320	66.120692
1443.708828	36.424979	66.125697
1443.219944	35.601993	66.130702
1442.104695	39.788230	66.135706
1441.649967	45.027805	66.140711
1441.279610	35.262702	66.145716
1440.792281	30.720411	66.150721
1439.602353	34.742990	66.155726
1438.880104	36.343259	66.160730
1438.062687	34.620498	66.165735
1438.008836	33.855676	66.170740
1437.707414	36.673066	66.175745
1437.048227	37.099306	66.180750
1435.857660	38.135554	66.185754
1435.181135	44.613433	66.190759
1434.573863	36.106590	66.195764
1433.676287	30.038673	66.200769
1432.758846	37.989430	66.205774
1432.330433	42.730313	66.210778
1431.498283	39.073583	66.215783
1431.429293	41.540152	66.220788
1431.353542	34.189643	66.225793
1429.907065	42.327267	66.230798
1429.417942	36.229696	66.235802
1428.755603	40.120528	66.240807
1427.794107	42.236992	66.245812
1426.863835	35.227346	66.250817
1425.697068	40.565114	66.255822
1425.570550	33.365790	66.260826
1425.162416	41.583436	66.265831
1424.760600	42.277452	66.270836
1424.423305	42.768985	66.275841
1423.669269	38.338659	66.280846
1422.965018	33.586011	66.285850
1422.318133	38.546253	66.290855
1421.461045	35.832042	66.295860
1420.320913	41.178673	66.300865
1419.200214	41.239457	66.305870
1419.020319	40.698701	66.310874
1418.743157	41.064289	66.315879
1418.179697	40.658262	66.320884
1417.832437	43.118385	66.325889
1416.425802	45.856941	66.330894
1415.876804	33.589115	66.335898
1415.286964	35.115015	66.340903
1414.585997	35.112640	66.345908
1413.682175	30.358236	66.350913
1412.752020	41.851008	66.355918
1412.424595	36.675456	66.360922
1411.778659	45.481283	66.365927
1411.480234	42.562109	66.370932
1411.416137	40.062278	66.375937
1410.606419	39.483677	66.380942
1409.830626	24.760848	66.385946
1408.954841	41.658666	66.390951
1407.999486	36.076279	66.395956
1407.222547	32.369450	66.400961
1406.216921	49.778557	66.405966
1406.326089	39.310879	66.410970
1405.815920	42.263866	66.415975
1404.665820	36.344173	66.420980
1403.814426	44.908471	66.425985
1403.312017	42.239335	66.430990
1403.109855	40.386399	66.435994
1402.653667	41.202612	66.440999
1401.481366	37.495961	66.446004
1400.907766	24.974606	66.451009
1399.954906	36.070622	66.456014
1399.591747	26.668231	66.461018
1398.618529	40.793646	66.466023
1397.506882	37.441333	66.471028
1397.261376	35.693707	66.476033
1396.453790	41.260906	66.481038
1396.117400	46.418256	66.486042
1395.822555	47.480788	66.491047
1395.526843	42.857545	66.496052
1394.223059	40.527681	66.501057
1393.209408	46.007792	66.506062
1393.204843	33.918347	66.511066
1392.709713	40.502933	66.516071
1391.314073	37.008980	66.521076
1391.115111	29.041309	66.526081
1389.962085	37.955642	66.531086
1389.947409	41.852846	66.536090
1389.376597	30.922518	66.541095
1388.033430	29.076613	66.546100
1387.534491	31.233504	66.551105
1386.952900	37.363569	66.556110
1386.312035	21.307584	66.561114
1385.226244	41.563692	66.566119
1384.575974	34.368766	66.571124
1384.227850	27.021075	66.576129
1383.803770	32.266059	66.581134
1383.777236	27.555695	66.586138
1382.404059	41.390775	66.591143
1381.659094	40.703205	66.596148
1380.789899	39.884933	66.601153
1380.125925	35.065401	66.606158
1379.989296	33.812273	66.611162
1378.999959	41.463121	66.616167
1378.360139	43.145205	66.621172
1378.001981	29.086649	66.626177
1376.824018	36.179680	66.631182
1375.789460	31.123204	66.636186
1374.985186	33.267234	66.641191
1374.786077	40.832943	66.646196
1374.322664	26.352691	66.651201
1373.729961	40.139826	66.656206
1373.421040	33.067648	66.661210
1372.804767	38.879587	66.666215
1371.700207	38.514482	66.671220
1371.366438	34.280241	66.676225
1370.700820	42.052116	66.681230
1369.989923	34.972171	66.686234
1368.914672	38.083071	66.691239
1368.021490	41.447002	66.696244
1367.971923	39.932272	66.701249
1367.112218	45.098285	66.706254
1366.741537	32.545749	66.711258
1365.566776	39.396273	66.716263
1364.688892	35.060577	66.721268
1364.789222	36.007703	66.726273
1363.925868	32.824466	66.731278
1363.177037	36.637745	66.736282
1362.365007	40.176066	66.741287
1361.567969	46.223811	66.746292
1361.418594	40.506624	66.751297
1361.018027	32.558466	66.756302
1360.069979	30.643749	66.761306
1359.291906	37.487944	66.766311
1358.733377	37.720918	66.771316
1358.005864	33.252910	66.776321
1356.813712	44.608571	66.781326
1356.128423	34.441494	66.786330
1355.647117	38.730796	66.791335
1355.128747	41.300340	66.796340
1355.061797	38.267735	66.801345
1354.280884	39.197168	66.806350
1352.914888	36.916254	66.811354
1352.266562	37.543530	66.816359
1351.644235	45.564170	66.821364
1351.514647	31.748714	66.826369
1350.922338	43.576798	66.831374
1349.837619	36.225337	66.836378
1348.878673	35.619794	66.841383
1348.456366	39.673613	66.846388
1348.200971	36.426174	66.851393
1347.369822	37.583276	66.856398
1346.848634	38.868889	66.861402
1346.059746	37.187837	66.866407
1345.260681	48.068863	66.871412
1345.161102	34.120775	66.876417
1344.072362	30.816265	66.881422
1342.953650	32.869658	66.886426
1342.319352	35.192218	66.891431
1342.199177	40.046514	66.896436
1341.713855	30.727407	66.901441
1341.005983	42.073191	66.906446
1339.604527	35.188435	66.911450
1339.364419	45.613792	66.916455
1339.069783	45.762517	66.921460
1338.265346	38.220191	66.926465
1337.046211	41.955305	66.931470
1336.215152	35.689716	66.936474
1336.017658	47.175097	66.941479
1335.522040	46.561291	66.946484
1335.023877	36.997287	66.951489
1333.809756	41.944118	66.956494
1333.481617	32.573237	66.961498
1332.777991	36.384306	66.966503
1332.298520	43.090156	66.971508
1331.970161	39.039720	66.976513
1330.447343	43.854274	66.981518
1329.330423	39.022687	66.986522
1329.335466	39.038800	66.991527
1328.812260	34.443063	66.996532
1328.583607	27.674111	67.001537
1327.725085	39.986691	67.006542
1327.012078	33.534719	67.011546
1326.061588	33.549809	67.016551
1325.666078	37.021173	67.021556
1325.251913	32.410324	67.026561
1323.514679	37.610513	67.031566
1323.195227	41.227930	67.036570
1322.539099	32.413307	67.041575
1321.849787	43.343039	67.046580
1321.491809	34.598554	67.051585
1321.461455	40.018894	67.056590
1320.839604	41.000835	67.061594
1319.716443	41.902024	67.066599
1319.010222	45.286061	67.071604
1317.972701	37.994026	67.076609
1317.064506	38.481065	67.081614
1316.667760	40.948874	67.086618
1316.163553	39.874325	67.091623
1315.387881	43.341695	67.096628
1315.448024	40.290888	67.101633
1314.622852	38.062263	67.106638
1313.686339	35.997956	67.111642
1313.549424	37.804340	67.116647
1312.239126	39.553448	67.121652
1311.581397	38.691489	67.126657
1310.595997	34.076987	67.131662
1310.179163	35.780113	67.136666
1309.941416	43.128630	67.141671
1309.224728	44.277986	67.146676
1308.228667	30.059843	67.151681
1307.634326	38.056743	67.156686
1307.746679	44.438264	67.161690
1306.679041	37.151389	67.166695
1305.726498	44.996071	67.171700
1304.751257	33.872112	67.176705
1304.156538	44.536190	67.181710
1303.468823	35.582905	67.186714
1303.298440	42.003353	67.191719
1302.156766	38.383849	67.196724
1301.400078	33.084439	67.201729
1300.722929	39.418753	67.206734
1300.632493	32.411809	67.211738
1300.419450	36.513485	67.216743
1298.721894	37.092635	67.221748
1298.423083	32.735186	67.226753
1298.102917	44.438527	67.231758
1297.218674	28.226078	67.236762
1296.439320	33.421759	67.241767
1295.289021	44.830654	67.246772
1294.843990	31.771019	67.251777
1294.001907	36.146953	67.256782
1293.862757	38.618425	67.261786
1293.632862	41.442916	67.266791
1292.860201	44.849382	67.271796
1291.944767	36.124152	67.276801
1291.057865	36.672285	67.281806
1290.636777	34.844992	67.286810
1289.997522	42.350266	67.291815
1288.713875	45.601063	67.296820
1288.554496	40.391230	67.301825
1287.750712	36.998083	67.306830
1287.592429	37.046498	67.311834
1286.599590	46.723257	67.316839
1285.649408	43.626343	67.321844
1285.148635	30.702169	67.326849
1284.515912	38.059882	67.331854
1284.250817	39.986495	67.336858
1283.481955	29.972292	67.341863
1282.433222	42.415722	67.346868
1282.472886	32.686240	67.351873
1281.246712	36.759659	67.356878
1280.125335	32.966564	67.361882
1279.552231	30.320996	67.366887
1278.667143	43.215600	67.371892
1278.509477	37.641545	67.376897
1277.742468	40.466019	67.381902
1277.831315	39.239028	67.386906
1277.230158	28.147746	67.391911
1276.240710	41.564664	67.396916
1275.538966	33.277309	67.401921
1274.658035	34.982524	67.406926
1274.070034	39.507191	67.411930
1273.051301	40.009609	67.416935
1272.647538	48.495706	67.421940
1272.086621	38.772728	67.426945
1271.597558	47.849322	67.431950
1270.570096	38.045565	67.436954
1269.864186	31.546999	67.441959
1269.006049	33.964725	67.446964
1268.761393	34.741973	67.451969
1268.299859	45.999011	67.456974
1267.372004	40.776274	67.461978
1266.496187	33.904972	67.466983
1265.603425	43.114620	67.471988
1265.563196	35.460428	67.476993
1264.943907	39.745727	67.481998
1264.225104	35.311375	67.487002
1263.349247	36.629689	67.492007
1262.451183	42.767366	67.497012
1262.003051	31.120966	67.502017
1261.461635	37.251264	67.507022
1261.220369	38.229633	67.512026
1260.315961	39.354292	67.517031
1259.186414	45.353582	67.522036
1259.114041	33.614036	67.527041
1258.276223	43.150578	67.532046
1257.401703	40.369123	67.537050
1256.555133	36.056509	67.542055
1255.872058	39.198968	67.547060
1255.791063	35.082510	67.552065
1255.230297	41.845303	67.557070
1254.148480	41.991437	67.562074
1253.559860	41.262121	67.567079
1252.458688	41.129740	67.572084
1252.551913	34.096488	67.577089
1251.388888	37.661757	67.582094
1250.234838	39.999891	67.587098
1249.718290	44.191027	67.592103
1249.355894	37.540105	67.597108
1249.416101	37.082191	67.602113
1248.690006	36.752972	67.607118
1247.660429	41.421131	67.612122
1246.881607	38.546719	67.617127
1245.707215	41.283450	67.622132
1245.738615	38.178752	67.627137
1245.372682	33.672150	67.632142
1244.018849	33.694733	67.637146
1243.575144	37.407235	67.642151
1242.678069	45.963972	67.647156
1242.316507	30.771213	67.652161
1241.690522	32.820399	67.657166
1241.466004	40.157173	67.662170
1240.403113	39.130916	67.667175
1239.735689	42.121100	67.672180
1239.280298	29.704669	67.677185
1237.784353	38.884564	67.682190
1237.011455	38.530993	67.687194
1236.821555	36.085864	67.692199
1235.972302	40.641841	67.697204
1235.910756	35.457894	67.702209
1235.499357	42.993631	67.707214
1234.776090	36.891970	67.712218
1233.886618	36.391392	67.717223
1232.779629	39.669190	67.722228
1232.833139	34.269371	67.727233
1231.453110	42.913922	67.732238
1230.719704	40.163179	67.737242
1230.457673	33.713751	67.742247
1229.716357	35.655189	67.747252
1229.561047	36.940538	67.752257
1228.171764	41.620549	67.757262
1227.468608	38.619114	67.762266
1227.041082	37.011604	67.767271
1226.516878	36.370337	67.772276
1226.469091	32.722251	67.777281
1225.241541	37.858891	67.782286
1224.370879	40.217194	67.787290
1223.795950	30.643860	67.792295
1223.155263	39.541944	67.797300
1222.667934	37.397594	67.802305
1221.799632	39.627999	67.807310
1220.782825	40.114703	67.812314
1220.641627	29.786619	67.817319
1219.880317	38.617332	67.822324
1219.190898	34.847399	67.827329
1218.276979	34.007210	67.832334
1217.661015	34.788034	67.837338
1217.529609	30.915461	67.842343
1216.665303	42.166456	67.847348
1215.633323	36.858934	67.852353
1214.882139	36.223768	67.857358
1214.566182	38.339082	67.862362
1213.945073	36.814451	67.867367
1213.102548	42.424359	67.872372
1213.036150	30.573674	67.877377
1211.607240	36.540936	67.882382
1210.652418	33.670219	67.887386
1210.576307	32.626199	67.892391
1210.092253	39.077058	67.897396
1209.768390	34.356820	67.902401
1208.878401	38.011134	67.907406
1208.114180	36.972431	67.912410
1207.856923	37.290413	67.917415
1206.509188	41.155724	67.922420
1205.926823	35.879378	67.927425
1205.547944	38.007439	67.932430
1204.880148	40.947956	67.937434
1203.885950	34.333768	67.942439
1202.944259	44.686217	67.947444
1202.565954	40.512116	67.952449
1202.059521	48.247669	67.957454
1201.054954	42.451136	67.962458
1200.697739	40.957505	67.967463
1199.704819	45.020610	67.972468
1199.248700	42.005698	67.977473
1197.995024	43.907764	67.982478
1197.896592	42.465348	67.987482
1197.691075	40.200913	67.992487
1197.031647	46.349843	67.997492
1196.004937	41.087604	68.002497
1195.070487	47.102447	68.007502
1194.798862	44.222912	68.012506
1194.277761	36.763947	68.017511
1193.825758	42.730923	68.022516
1192.784080	42.962956	68.027521
1192.041645	48.403766	68.032526
1191.490220	41.912708	68.037530
1191.180900	38.991868	68.042535
1189.647327	37.109149	68.047540
1189.075928	39.567790	68.052545
1188.705575	41.771363	68.057550
1187.852117	40.539530	68.062554
1187.827173	32.612349	68.067559
1187.107542	46.866456	68.072564
1185.987311	41.895350	68.077569
1185.647341	45.761799	68.082574
1184.940968	40.869433	68.087578
1184.521403	40.573790	68.092583
1183.028254	44.724517	68.097588
1183.002271	38.816098	68.102593
1182.294793	38.596985	68.107598
1181.830086	48.739883	68.112602
1180.895744	42.648714	68.117607
1180.087973	42.954775	68.122612
1179.456903	31.667725	68.127617
1178.782980	30.290293	68.132622
1178.611866	36.036288	68.137626
1177.361648	33.317992	68.142631
1176.609283	37.774495	68.147636
1176.208622	31.439201	68.152641
1175.326805	38.157102	68.157646
1174.918404	35.974772	68.162650
1174.641966	30.235548	68.167655
1173.604499	38.079386	68.172660
1172.867350	30.348355	68.177665
1172.455279	25.311665	68.182670
1171.811602	34.860754	68.187674
1170.819735	38.130298	68.192679
1169.949001	35.591360	68.197684
1169.769385	35.528569	68.202689
1169.242473	39.724246	68.207694
1167.913507	41.662893	68.212698
1167.342394	37.866792	68.217703
1166.604626	47.236614	68.222708
1166.140099	41.045272	68.227713
1165.960538	39.171902	68.232718
1165.136052	38.341278	68.237722
1164.826223	35.213301	68.242727
1163.462032	44.339077	68.247732
1163.080180	35.709227	68.252737
1162.581025	33.590198	68.257742
1161.682554	35.853802	68.262746
1161.008831	35.663648	68.267751
1160.382151	44.389610	68.272756
1159.983103	38.162982	68.277761
1159.312652	42.839136	68.282766
1157.793601	41.529044	68.287770
1157.383581	35.612965	68.292775
1156.741004	29.265414	68.297780
1156.465489	32.288760	68.302785
1156.013393	36.039017	68.307790
1155.533635	43.856840	68.312794
1154.725621	34.746565	68.317799
1153.880982	45.304627	68.322804
1153.607058	36.128561	68.327809
1152.575110	38.330156	68.332814
1151.583783	37.716381	68.337818
1151.183921	38.758222	68.342823
1150.639978	38.170078	68.347828
1150.165152	30.959767	68.352833
1148.883078	43.151859	68.357838
1148.052981	40.301245	68.362842
1148.068315	29.270613	68.367847
1147.128137	43.529719	68.372852
1146.377454	39.744236	68.377857
1145.558385	38.579152	68.382862
1144.487735	40.124250	68.387866
1144.335863	33.891617	68.392871
1143.722098	35.387301	68.397876
1143.634414	39.670003	68.402881
1143.401662	41.969617	68.407886
1142.179709	43.139194	68.412890
1141.587930	38.013674	68.417895
1140.716526	40.209098	68.422900
1139.896568	38.375515	68.427905
1138.823848	39.841630	68.432910
1138.371996	37.849103	68.437914
1137.776550	21.855677	68.442919
1137.543677	34.747151	68.447924
1136.667063	28.624799	68.452929
1135.737801	39.691139	68.457934
1135.048711	35.627890	68.462938
1134.854372	36.444288	68.467943
1134.161615	41.809887	68.472948
1133.079968	41.299208	68.477953
1131.912704	31.164192	68.482958
1131.482682	38.838503	68.487962
1131.170168	40.873498	68.492967
1130.605889	36.005759	68.497972
1130.431434	39.224951	68.502977
1130.186642	39.360417	68.507982
1128.740302	40.402242	68.512986
1128.390765	29.588028	68.517991
1127.734740	42.041987	68.522996
1126.708704	36.918198	68.528001
1125.762887	38.650730	68.533006
1125.131923	44.618747	68.538010
1125.149391	31.967041	68.543015
1123.629759	33.904004	68.548020
1122.851259	31.712818	68.553025
1122.586364	40.481826	68.558030
1121.936237	41.329691	68.563034
1121.831456	28.534718	68.568039
1121.618336	41.670697	68.573044
1119.980589	33.580751	68.578049
1119.126088	34.219675	68.583054
1118.440569	39.991384	68.588058
1118.186254	31.773501	68.593063
1117.435814	36.788205	68.598068
1116.512377	37.404199	68.603073
1115.936272	40.330603	68.608078
1115.024862	48.081820	68.613082
1115.004607	36.976363	68.618087
1114.240083	38.406685	68.623092
1113.888813	40.737250	68.628097
1113.141297	39.455319	68.633102
1112.006582	43.341805	68.638106
1111.903438	33.153264	68.643111
1110.756712	47.956926	68.648116
1109.794386	42.712894	68.653121
1109.122455	38.668815	68.658126
1108.657401	43.655576	68.663130
1108.527181	42.177556	68.668135
1107.590869	38.275453	68.673140
1106.901174	42.382567	68.678145
1106.057026	43.584167	68.683150
1104.957316	46.357873	68.688154
1104.945402	44.416723	68.693159
1104.433537	44.995402	68.698164
1104.199358	47.236843	68.703169
1103.484533	43.826131	68.708174
1102.663098	42.068198	68.713178
1102.068172	46.017382	68.718183
1100.664474	48.305142	68.723188
1100.269308	47.117609	68.728193
1099.889403	44.485165	68.733198
1098.945485	47.500209	68.738202
1097.964044	39.241839	68.743207
1097.209968	48.602615	68.748212
1096.738319	42.433424	68.753217
1096.565239	39.427293	68.758222
1095.648732	44.008224	68.763226
1095.507357	34.989858	68.768231
1094.021616	40.991746	68.773236
1093.812481	37.297876	68.778241
1093.547291	37.230005	68.783246
1091.999922	39.892876	68.788250
1091.391332	40.584825	68.793255
1090.659521	51.665521	68.798260
1090.053811	44.454338	68.803265
1089.926542	44.691650	68.808270
1089.330131	44.345380	68.813274
1088.769503	35.152500	68.818279
1088.139028	41.742508	68.823284
1086.737205	42.361480	68.828289
1086.490817	40.049580	68.833294
1085.768882	42.684394	68.838298
1084.861714	41.256130	68.843303
1084.063487	44.670550	68.848308
1083.672210	48.200015	68.853313
1083.435465	37.689369	68.858318
1082.963540	47.908497	68.863322
1081.849904	35.694018	68.868327
1080.945285	48.039373	68.873332
1080.643012	45.123651	68.878337
1080.187219	46.139551	68.883342
1078.804406	52.615245	68.888346
1078.202446	43.731004	68.893351
1077.569621	48.337964	68.898356
1077.106482	48.448456	68.903361
1077.270364	46.733770	68.908366
1075.763818	49.515177	68.913370
1075.273154	42.833349	68.918375
1074.548933	45.252647	68.923380
1073.850387	44.106014	68.928385
1072.766653	44.039368	68.933390
1071.501881	49.855802	68.938394
1072.025870	37.517607	68.943399
1071.541579	50.481744	68.948404
1070.872649	47.224617	68.953409
1070.126366	40.313813	68.958414
1068.798359	50.278502	68.963418
1068.111012	39.248205	68.968423
1067.486931	42.543600	68.973428
1067.149102	48.576684	68.978433
1066.730983	38.809168	68.983438
1066.200291	42.214486	68.988442
1066.007638	37.808884	68.993447
1065.041711	41.767129	68.998452
1064.261228	41.914991	69.003457
1063.144288	43.505135	69.008462
1062.262361	44.852942	69.013466
1061.835533	39.395652	69.018471
1061.438954	40.435753	69.023476
1060.744015	37.768449	69.028481
1060.248607	35.878517	69.033486
1058.896646	43.938060	69.038490
1058.576856	43.248387	69.043495
1057.843382	46.615014	69.048500
1057.198612	42.397748	69.053505
1057.058407	42.570174	69.058510
1056.186087	41.089766	69.063514
1055.458352	35.736503	69.068519
1054.436793	51.360671	69.073524
1053.894203	46.664877	69.078529
1053.651927	37.506695	69.083534
1052.556796	45.626070	69.088538
1052.224470	37.643777	69.093543
1051.975779	39.054062	69.098548
1051.107118	41.974519	69.103553
1049.851562	37.882767	69.108558
1048.852653	42.762011	69.113562
1048.712413	32.927576	69.118567
1048.268110	37.077537	69.123572
1047.657897	40.290037	69.128577
1046.773981	38.241251	69.133582
1045.785593	48.109498	69.138586
1045.465773	32.032576	69.143591
1045.162617	38.076690	69.148596
1044.341286	34.709885	69.153601
1043.473359	23.484355	69.158606
1042.179705	40.985803	69.163610
1042.146719	28.040398	69.168615
1041.666405	39.609704	69.173620
1040.980156	39.761958	69.178625
1040.236623	41.842346	69.183630
1039.021749	50.983629	69.188634
1038.866144	41.160900	69.193639
1038.269651	35.797403	69.198644
1037.696729	28.637857	69.203649
1036.840302	27.828514	69.208654
1035.903045	33.372165	69.213658
1035.394752	30.848949	69.218663
1035.103324	36.831452	69.223668
1034.677934	36.101053	69.228673
1033.558890	36.441100	69.233678
1032.697619	45.619323	69.238682
1032.418566	40.108312	69.243687
1031.305943	40.085699	69.248692
1031.095710	38.731116	69.253697
1030.296051	34.001592	69.258702
1029.219077	35.244653	69.263706
1029.353276	35.141154	69.268711
1028.417243	41.024450	69.273716
1027.632281	33.819508	69.278721
1027.138759	28.002615	69.283726
1026.007334	37.588262	69.288730
1026.017351	31.181875	69.293735
1025.106030	32.071322	69.298740
1023.958433	32.508625	69.303745
1023.329603	34.973562	69.308750
1022.777016	35.014513	69.313754
1022.720336	27.647756	69.318759
1021.842678	29.230483	69.323764
1020.613138	38.910693	69.328769
1020.867144	24.089792	69.333774
1020.192577	30.785240	69.338778
1019.444712	33.719750	69.343783
1017.657636	34.162358	69.348788
1017.267353	40.672555	69.353793
1017.043006	28.225295	69.358798
1016.093947	37.026594	69.363802
1016.055494	34.506995	69.368807
1015.182510	31.915977	69.373812
1014.340282	27.395844	69.378817
1013.704913	34.179707	69.383822
1012.779677	34.418284	69.388826
1012.696016	29.838111	69.393831
1012.005369	41.815260	69.398836
1010.869030	31.563284	69.403841
1010.278626	24.685804	69.408846
1009.689315	36.532706	69.413850
1009.863835	28.594673	69.418855
1008.690845	25.528876	69.423860
1007.820080	31.470464	69.428865
1007.125134	23.367531	69.433870
1006.632474	35.700749	69.438874
1005.943686	28.585129	69.443879
1004.766088	29.800824	69.448884
1004.207770	27.737734	69.453889
1003.824349	31.706357	69.458894
1003.187357	32.710663	69.463898
1002.938343	30.845645	69.468903
1002.148684	32.981697	69.473908
1001.121724	35.053393	69.478913
1000.868408	29.643766	69.483918
999.661417	34.932446	69.488922
998.704088	21.003827	69.493927
998.111566	28.511367	69.498932
997.638695	31.435889	69.503937
997.390642	31.992688	69.508942
996.865773	34.131945	69.513946
996.267244	22.400056	69.518951
995.147536	31.840415	69.523956
994.330001	34.544108	69.528961
994.239629	27.260094	69.533966
993.605596	35.509708	69.538970
992.476287	25.695463	69.543975
991.805038	37.913222	69.548980
991.245461	33.229430	69.553985
991.106444	34.981705	69.558990
989.890187	37.335282	69.563994
988.780973	31.740669	69.568999
988.441332	39.974210	69.574004
987.711315	34.467808	69.579009
987.725034	32.960407	69.584014
987.086360	40.465199	69.589018
986.258121	34.396963	69.594023
985.313727	33.434545	69.599028
984.619903	34.232676	69.604033
984.649270	27.057624	69.609038
982.726310	37.125786	69.614042
982.463302	32.668693	69.619047
981.842432	32.794759	69.624052
981.337590	27.528863	69.629057
981.230766	29.157209	69.634062
980.191708	37.177782	69.639066
979.142022	32.640291	69.644071
978.851491	36.876020	69.649076
977.922459	36.210957	69.654081
977.732435	36.825710	69.659086
976.666659	30.677374	69.664090
976.203872	28.876993	69.669095
975.697503	29.089235	69.674100
975.148000	33.699296	69.679105
973.990268	22.031208	69.684110
973.144031	33.097150	69.689114
972.804515	29.509301	69.694119
972.339167	30.636576	69.699124
971.374544	29.109234	69.704129
970.415637	25.210246	69.709134
969.427592	36.638749	69.714138
969.165363	33.850385	69.719143
969.281958	45.896912	69.724148
968.202383	39.554369	69.729153
968.200408	26.797076	69.734158
967.076497	32.881886	69.739162
965.831108	30.420179	69.744167
965.351088	35.124126	69.749172
964.812748	36.716642	69.754177
965.003029	30.764099	69.759182
963.281488	37.692144	69.764186
962.743822	41.654819	69.769191
962.432151	39.149251	69.774196
961.585773	37.868488	69.779201
961.061410	34.888582	69.784206
959.746338	38.624413	69.789210
959.301757	33.622921	69.794215
959.034359	29.911413	69.799220
958.543185	38.177220	69.804225
957.734773	36.086707	69.809230
957.255469	41.107096	69.814234
956.479382	29.261548	69.819239
956.140664	27.492024	69.824244
954.814713	36.171174	69.829249
954.480728	27.395016	69.834254
953.340239	33.848175	69.839258
953.236852	29.246123	69.844263
952.579731	23.739484	69.849268
951.572539	36.707897	69.854273
951.110037	31.030564	69.859278
950.524652	41.807905	69.864282
949.742677	32.004446	69.869287
948.518755	32.384972	69.874292
948.217543	34.842359	69.879297
947.723787	31.361450	69.884302
947.267756	42.224001	69.889306
947.023327	37.877800	69.894311
945.452001	35.505075	69.899316
944.792423	42.218096	69.904321
944.374240	34.231184	69.909326
943.495884	41.112719	69.914330
943.322248	37.563565	69.919335
942.207111	35.903724	69.924340
941.274997	29.004650	69.929345
941.310909	28.971662	69.934350
940.454931	31.276178	69.939354
940.268475	36.044712	69.944359
939.373948	32.514421	69.949364
937.868256	40.696624	69.954369
938.112509	33.921327	69.959374
937.126413	35.740128	69.964378
936.301773	34.391308	69.969383
934.937936	38.860591	69.974388
934.523997	40.500881	69.979393
934.015575	36.595401	69.984398
933.651552	48.594770	69.989402
933.108455	34.271157	69.994407
932.915749	36.687068	69.999412
932.312802	40.025431	70.004417
931.442495	38.906659	70.009422
930.334472	42.359155	70.014426
930.054643	44.426454	70.019431
929.468571	34.771807	70.024436
928.525545	39.675837	70.029441
927.562196	33.916924	70.034446
927.235940	44.183332	70.039450
926.875350	29.102584	70.044455
926.233869	37.319926	70.049460
925.098401	35.308722	70.054465
924.828402	34.005826	70.059470
924.121544	44.119140	70.064474
923.531874	30.848718	70.069479
922.539956	38.228100	70.074484
921.488765	37.690149	70.079489
921.193279	32.988768	70.084494
920.422171	40.968590	70.089498
920.116443	28.844348	70.094503
919.260703	33.356870	70.099508
918.354706	41.890293	70.104513
918.242059	32.029047	70.109518
917.456266	34.181816	70.114522
916.655525	38.460721	70.119527
915.708673	38.475266	70.124532
914.568406	39.005676	70.129537
914.581329	37.006595	70.134542
913.932337	41.939213	70.139546
913.508571	36.967318	70.144551
913.038166	37.455629	70.149556
912.542595	45.164853	70.154561
911.839858	33.892906	70.159566
910.786292	47.190967	70.164570
910.269902	41.372084	70.169575
909.387545	32.912470	70.174580
908.779893	36.818453	70.179585
908.222307	31.846192	70.184590
907.213181	41.437356	70.189594
906.302177	34.625458	70.194599
905.527100	32.776339	70.199604
905.130787	40.333963	70.204609
904.867361	33.465626	70.209614
904.261257	37.946841	70.214618
903.907352	35.188394	70.219623
902.975063	43.989599	70.224628
902.450721	40.031984	70.229633
901.934439	30.624721	70.234638
900.633483	40.674399	70.239642
899.692082	35.214876	70.244647
899.265808	33.852305	70.249652
898.911437	40.507923	70.254657
899.051382	32.477137	70.259662
897.140957	41.113517	70.264666
896.710505	29.832046	70.269671
895.825734	34.710313	70.274676
895.202656	36.381688	70.279681
895.617054	33.167591	70.284686
894.204931	37.372009	70.289690
893.322876	33.726703	70.294695
893.282681	34.613019	70.299700
892.452347	36.803814	70.304705
891.508230	37.536674	70.309710
890.018336	40.900643	70.314714
889.346224	29.161248	70.319719
889.323037	34.784403	70.324724
888.896889	37.777900	70.329729
888.834892	36.443724	70.334734
888.069861	40.174176	70.339738
887.435660	38.212514	70.344743
886.677106	38.658211	70.349748
885.638587	36.221880	70.354753
884.834719	43.278549	70.359758
883.489610	41.776525	70.364762
883.176975	40.537774	70.369767
882.889254	40.264968	70.374772
882.533122	48.027676	70.379777
882.083179	42.990402	70.384782
880.997333	39.138830	70.389786
880.379263	39.094307	70.394791
879.786559	36.999625	70.399796
878.934281	43.639871	70.404801
878.734225	38.203371	70.409806
877.433298	40.655155	70.414810
876.807517	39.596348	70.419815
876.409330	31.737860	70.424820
875.757389	40.380133	70.429825
875.545466	34.981980	70.434830
874.470097	39.944605	70.439834
873.908513	37.167260	70.444839
873.616697	32.739584	70.449844
872.049535	40.322888	70.454849
871.495038	35.994279	70.459854
871.018700	42.501060	70.464858
870.192480	37.809275	70.469863
869.876885	35.618187	70.474868
869.231605	35.491094	70.479873
868.360221	36.709238	70.484878
867.477607	39.093718	70.489882
866.708403	33.188285	70.494887
866.312439	35.033910	70.499892
865.840133	38.188465	70.504897
865.586787	35.612130	70.509902
864.578206	30.333063	70.514906
864.149710	34.395854	70.519911
863.616724	36.303631	70.524916
862.109800	42.643922	70.529921
861.719790	41.116467	70.534926
861.199210	36.068008	70.539930
860.489169	32.307594	70.544935
860.485074	36.693201	70.549940
859.183431	46.869316	70.554945
858.073212	35.009184	70.559950
857.769764	40.923093	70.564954
857.015158	35.173442	70.569959
856.922407	32.891295	70.574964
855.675541	35.597100	70.579969
855.121931	32.415782	70.584974
854.449979	30.693870	70.589978
854.007986	36.091140	70.594983
853.659482	34.393165	70.599988
852.208294	28.354693	70.604993
851.657771	25.905047	70.609998
851.196016	38.882671	70.615002
850.937489	36.865748	70.620007
850.454839	33.301244	70.625012
849.388904	38.280807	70.630017
848.420347	32.852396	70.635022
848.322445	35.967295	70.640026
847.290013	31.164003	70.645031
846.500154	39.384660	70.650036
845.359306	36.793374	70.655041
845.085345	30.492479	70.660046
844.660493	35.381578	70.665050
844.157146	41.636815	70.670055
843.911015	29.944857	70.675060
842.740248	33.684021	70.680065
841.992153	26.535968	70.685070
841.717368	40.962937	70.690074
840.274943	42.957808	70.695079
839.683546	29.590606	70.700084
838.474291	46.221873	70.705089
838.579352	35.936918	70.710094
837.929427	36.339149	70.715098
837.585744	35.512672	70.720103
837.478790	36.821717	70.725108
836.820772	45.067556	70.730113
836.081871	36.901529	70.735118
834.820287	42.331034	70.740122
833.167637	32.540562	70.745127
832.761667	34.291197	70.750132
831.994004	46.714941	70.755137
832.272224	31.469929	70.760142
831.562272	38.692873	70.765146
830.970613	38.558969	70.770151
830.670104	38.880826	70.775156
829.413805	41.912710	70.780161
829.181041	32.851219	70.785166
828.385756	34.366582	70.790170
827.829527	33.029830	70.795175
827.124875	33.213685	70.800180
825.836872	35.317891	70.805185
825.471258	33.960726	70.810190
824.752686	39.639045	70.815194
823.772487	42.799287	70.820199
823.406901	32.475353	70.825204
822.188506	33.993719	70.830209
822.864929	33.328021	70.835214
822.243910	33.872532	70.840218
820.874442	39.657210	70.845223
820.322203	39.308934	70.850228
819.220600	43.970157	70.855233
818.876499	32.164332	70.860238
818.330153	35.367884	70.865242
817.407181	28.067826	70.870247
816.817931	26.286756	70.875252
815.659475	27.973663	70.880257
815.499953	26.884340	70.885262
815.343034	29.093211	70.890266
814.729890	31.261419	70.895271
813.433118	33.190297	70.900276
812.929134	32.819546	70.905281
812.726407	31.060686	70.910286
811.799069	32.753399	70.915290
810.503776	35.208970	70.920295
810.263157	35.271503	70.925300
809.547750	34.718295	70.930305
809.315764	22.267650	70.935310
808.928443	31.805202	70.940314
807.506538	36.740752	70.945319
806.851127	37.018012	70.950324
805.878015	38.357796	70.955329
805.984056	31.548549	70.960334
804.791520	33.328529	70.965338
804.031190	47.372905	70.970343
803.437329	29.394271	70.975348
802.715089	37.224421	70.980353
802.415089	26.870708	70.985358
802.275346	38.069053	70.990362
801.797624	28.927561	70.995367
800.877873	25.726869	71.000372
799.897018	35.388194	71.005377
799.304928	29.229820	71.010382
798.315240	33.461764	71.015386
797.663558	29.267047	71.020391
797.096099	28.598109	71.025396
796.807159	37.784487	71.030401
795.580077	33.834770	71.035406
794.994270	35.231760	71.040410
794.040058	38.924763	71.045415
794.081885	38.252506	71.050420
793.364808	38.637826	71.055425
792.419748	33.546833	71.060430
791.350147	36.879885	71.065434
790.775723	36.095304	71.070439
790.887266	34.450761	71.075444
790.046760	36.119920	71.080449
789.136891	30.588319	71.085454
788.433619	43.875327	71.090458
787.612110	29.408405	71.095463
787.555964	21.756202	71.100468
787.031383	35.729398	71.105473
786.296447	33.935394	71.110478
785.220487	41.568782	71.115482
784.543158	37.372537	71.120487
783.857631	31.683304	71.125492
782.523175	38.358393	71.130497
782.006179	31.367727	71.135502
781.601046	38.540039	71.140506
781.310743	41.302258	71.145511
781.020332	39.884849	71.150516
780.348608	43.790374	71.155521
779.615981	48.193017	71.160526
778.771730	35.183728	71.165530
778.179771	42.848677	71.170535
777.350161	27.615821	71.175540
776.164985	36.229838	71.180545
775.592719	29.192987	71.185550
775.506953	36.342169	71.190554
775.064184	38.944199	71.195559
773.708469	30.711753	71.200564
772.474089	42.484823	71.205569
772.445882	31.280914	71.210574
771.771931	30.323132	71.215578
771.130127	38.577245	71.220583
771.300190	34.478597	71.225588
770.436032	33.352487	71.230593
769.343289	34.464889	71.235598
768.605435	31.733149	71.240602
768.030797	33.153490	71.245607
767.751423	30.247298	71.250612
766.548077	29.809652	71.255617
766.117535	31.696336	71.260622
765.351188	35.074939	71.265626
764.882469	38.666231	71.270631
764.838867	17.089079	71.275636
763.344121	38.248477	71.280641
762.838604	28.670067	71.285646
762.558722	30.086493	71.290650
761.389171	39.062160	71.295655
760.460686	35.014332	71.300660
759.493195	32.080365	71.305665
759.210946	21.567710	71.310670
758.513674	28.916765	71.315674
757.909439	35.415456	71.320679
758.093396	45.555381	71.325684
756.910226	41.831823	71.330689
756.365693	31.878011	71.335694
755.536330	33.396853	71.340698
754.713139	37.153861	71.345703
753.912405	32.949553	71.350708
753.044269	43.528239	71.355713
752.927119	41.541575	71.360718
752.140595	36.328307	71.365722
752.195375	41.430891	71.370727
751.243944	31.845582	71.375732
750.222857	40.062043	71.380737
749.805550	30.077361	71.385742
748.978616	27.320624	71.390746
747.673119	44.236789	71.395751
747.314524	29.432438	71.400756
746.925822	38.287765	71.405761
746.620527	35.218260	71.410766
746.163684	38.422276	71.415770
744.810573	37.677150	71.420775
744.150907	31.802320	71.425780
743.819292	37.413569	71.430785
743.372087	33.907741	71.435790
742.028657	38.712634	71.440794
740.999591	41.403654	71.445799
740.975406	43.899247	71.450804
740.193044	48.304888	71.455809
739.837713	34.447688	71.460814
738.944731	31.626087	71.465818
737.777935	38.269305	71.470823
736.982791	29.974396	71.475828
736.620110	34.501946	71.480833
736.149338	35.768320	71.485838
735.935266	37.821598	71.490842
735.241925	45.302218	71.495847
735.250752	40.001650	71.500852
733.968530	36.682284	71.505857
733.355216	42.266006	71.510862
732.542688	35.409259	71.515866
731.309072	34.711558	71.520871
730.889693	40.078909	71.525876
730.619090	45.283414	71.530881
729.632799	33.928651	71.535886
729.103388	34.080922	71.540890
727.814738	34.698369	71.545895
727.661388	29.202572	71.550900
726.646172	32.425272	71.555905
726.687246	34.798768	71.560910
726.298607	29.473140	71.565914
725.182583	30.644800	71.570919
724.786162	28.590723	71.575924
723.746182	34.137408	71.580929
723.210689	27.288469	71.585934
721.962376	31.345662	71.590938
721.305941	37.190177	71.595943
721.266430	28.252696	71.600948
720.555471	30.909355	71.605953
720.228281	32.856491	71.610958
719.599915	31.242390	71.615962
718.180119	35.584737	71.620967
717.778936	32.647708	71.625972
717.340671	30.733819	71.630977
716.568937	26.348905	71.635982
716.117395	28.955598	71.640986
714.755865	29.973933	71.645991
714.485856	27.240606	71.650996
713.889074	37.145602	71.656001
713.533171	33.323364	71.661006
712.766201	23.433724	71.666010
711.758291	29.064910	71.671015
711.321071	27.358464	71.676020
710.633187	40.464421	71.681025
709.976115	30.610816	71.686030
708.968464	34.344563	71.691034
708.294418	34.378727	71.696039
707.975657	35.409469	71.701044
707.320903	38.301621	71.706049
706.684473	32.812402	71.711054
706.347747	28.340732	71.716058
704.910152	41.237642	71.721063
704.676756	30.009686	71.726068
703.845611	29.850512	71.731073
703.526407	34.699807	71.736078
702.656289	29.352460	71.741082
701.669941	29.817868	71.746087
701.597511	26.702556	71.751092
700.727551	38.015724	71.756097
700.085799	32.826613	71.761102
699.191509	40.330211	71.766106
698.386718	34.852073	71.771111
698.471877	26.945155	71.776116
697.746633	35.946155	71.781121
697.356471	34.151126	71.786126
696.158737	28.502689	71.791130
695.231071	34.101580	71.796135
695.011449	31.774074	71.801140
693.690953	35.427610	71.806145
693.057208	37.120176	71.811150
692.859994	34.693704	71.816154
692.184588	34.709156	71.821159
691.756573	28.133900	71.826164
690.599484	36.457739	71.831169
689.977591	32.350300	71.836174
689.726002	29.742497	71.841178
689.039342	32.598275	71.846183
687.949375	27.766991	71.851188
686.864660	36.134876	71.856193
686.240178	32.271816	71.861198
686.017879	37.152271	71.866202
685.799492	38.839598	71.871207
685.478335	36.243712	71.876212
684.305856	37.073361	71.881217
683.344867	37.780731	71.886222
683.208431	34.776246	71.891226
682.241282	33.570302	71.896231
681.497451	31.036565	71.901236
680.213640	29.908159	71.906241
679.982860	32.777413	71.911246
679.903686	31.371190	71.916250
678.968293	35.298999	71.921255
678.157895	37.090511	71.926260
677.237380	41.643766	71.931265
676.931988	34.320041	71.936270
676.692653	32.228400	71.941274
675.853664	33.058547	71.946279
675.151070	29.184399	71.951284
674.271118	33.240072	71.956289
673.595964	26.469935	71.961294
673.160110	32.965440	71.966298
672.091854	36.067770	71.971303
671.404406	32.098663	71.976308
670.938934	32.911792	71.981313
669.980111	39.370585	71.986318
669.991294	32.347476	71.991322
668.604602	33.839057	71.996327
667.999868	29.976564	72.001332
667.666455	24.778845	72.006337
666.675109	29.332786	72.011342
666.833983	19.848594	72.016346
665.890069	35.586951	72.021351
664.935014	27.131573	72.026356
664.271577	35.460444	72.031361
663.735268	30.925870	72.036366
663.307566	25.830353	72.041370
661.986407	30.121474	72.046375
661.399979	24.684487	72.051380
660.355535	22.279620	72.056385
660.560943	24.197483	72.061390
660.371323	23.664346	72.066394
659.360663	27.559265	72.071399
658.469280	26.224694	72.076404
657.453187	28.157626	72.081409
656.893499	38.900565	72.086414
656.743315	29.747195	72.091418
655.575236	38.666970	72.096423
654.667073	25.726701	72.101428
654.338792	37.146007	72.106433
653.757269	34.685515	72.111438
654.062953	31.038871	72.116442
652.499429	31.760663	72.121447
651.826560	28.407188	72.126452
651.001833	34.973659	72.131457
650.446061	32.498494	72.136462
650.212258	28.670740	72.141466
648.938603	28.574756	72.146471
648.570652	25.360085	72.151476
648.291063	28.211254	72.156481
647.338786	30.965710	72.161486
646.326248	32.029267	72.166490
645.813602	32.076049	72.171495
645.525671	34.791683	72.176500
644.897143	26.910334	72.181505
643.479911	30.120611	72.186510
642.807821	23.145889	72.191514
642.357998	31.146862	72.196519
641.768690	28.081819	72.201524
641.557647	28.850965	72.206529
641.056231	32.319187	72.211534
640.416413	28.788350	72.216538
639.088482	37.006080	72.221543
638.936026	25.933604	72.226548
637.710096	29.606080	72.231553
636.554703	29.299981	72.236558
636.630999	28.750890	72.241562
635.942443	34.707486	72.246567
635.607609	24.199124	72.251572
634.717006	32.472577	72.256577
633.516110	34.267054	72.261582
632.900117	25.864116	72.266586
632.249558	35.196121	72.271591
632.070545	28.764124	72.276596
631.823976	31.215317	72.281601
630.996674	32.099124	72.286606
630.201033	35.733013	72.291610
629.329312	39.390199	72.296615
628.753161	36.549074	72.301620
627.839531	38.773521	72.306625
626.908314	34.780269	72.311630
626.291713	27.816172	72.316634
625.778738	32.788266	72.321639
625.555898	26.785335	72.326644
624.946521	25.198389	72.331649
624.179749	32.150831	72.336654
623.530724	24.578115	72.341658
622.658347	35.065167	72.346663
622.543528	29.357527	72.351668
621.480254	29.790739	72.356673
620.390748	38.234056	72.361678
619.956641	27.251282	72.366682
619.360534	29.938009	72.371687
619.033282	30.091575	72.376692
618.171114	29.081595	72.381697
617.468281	25.274601	72.386702
616.689059	33.376614	72.391706
615.933853	31.777549	72.396711
615.701058	24.323380	72.401716
614.649293	23.615869	72.406721
613.600682	33.730111	72.411726
613.695734	29.902856	72.416730
612.827204	29.891806	72.421735
612.570988	31.006569	72.426740
611.187047	29.090908	72.431745
609.770405	28.678794	72.436750
609.500965	28.219727	72.441754
609.814524	34.385926	72.446759
609.151855	22.331984	72.451764
608.451574	24.597243	72.456769
608.064186	29.424669	72.461774
607.026783	19.481136	72.466778
605.940711	19.720504	72.471783
605.995595	18.565248	72.476788
605.212865	23.299758	72.481793
603.898239	20.998430	72.486798
603.522510	16.613190	72.491802
602.879869	25.442152	72.496807
602.760015	24.730889	72.501812
601.370257	28.127511	72.506817
600.293308	26.651072	72.511822
600.209486	19.324533	72.516826
599.556370	21.379222	72.521831
598.964235	23.296366	72.526836
598.760836	18.989357	72.531841
597.764781	23.385044	72.536846
597.048049	20.669849	72.541850
596.577713	33.166191	72.546855
596.049034	24.533577	72.551860
595.304811	28.767309	72.556865
594.279541	34.626871	72.561870
593.850978	22.975693	72.566874
592.318431	24.738191	72.571879
591.647621	24.154482	72.576884
591.730753	22.782819	72.581889
590.850666	20.034433	72.586894
590.801847	19.062725	72.591898
590.219563	24.097611	72.596903
589.434834	24.251802	72.601908
588.153997	20.994612	72.606913
587.582752	27.798298	72.611918
587.408120	15.281034	72.616922
586.301136	21.433656	72.621927
585.256983	17.251359	72.626932
584.926638	23.069612	72.631937
584.427253	20.889516	72.636942
584.557703	16.680037	72.641946
583.190599	32.413537	72.646951
582.001682	23.416050	72.651956
581.938830	28.684817	72.656961
581.553104	32.285581	72.661966
580.317446	24.460116	72.666970
578.976967	24.167192	72.671975
578.668984	20.467807	72.676980
578.351830	21.182903	72.681985
577.960072	21.240952	72.686990
578.221125	23.552673	72.691994
577.297393	32.557688	72.696999
576.326262	26.932828	72.702004
575.032394	35.205913	72.707009
574.026962	29.102615	72.712014
573.315102	21.401343	72.717018
572.702582	20.751996	72.722023
572.036908	18.365933	72.727028
571.786095	16.767294	72.732033
571.546566	30.613481	72.737038
571.626364	22.546844	72.742042
570.333987	27.810367	72.747047
569.088590	22.887729	72.752052
569.228981	26.658859	72.757057
568.087194	28.751100	72.762062
567.166454	22.295419	72.767066
566.272524	30.343671	72.772071
565.998464	19.307836	72.777076
565.019228	27.583454	72.782081
563.968905	32.217776	72.787086
563.517278	23.166595	72.792090
562.707856	33.195651	72.797095
562.531706	32.417066	72.802100
561.989378	33.212585	72.807105
561.720244	29.185641	72.812110
561.454176	23.888376	72.817114
559.794598	32.394245	72.822119
559.484398	25.033868	72.827124
559.283431	31.172173	72.832129
557.427570	35.988333	72.837134
557.067264	25.016217	72.842138
555.778419	35.373327	72.847143
555.516848	32.434105	72.852148
555.350437	29.284379	72.857153
555.034468	25.214544	72.862158
554.942518	19.469839	72.867162
553.989012	34.485934	72.872167
553.417085	23.127341	72.877172
551.997564	18.299278	72.882177
550.937253	20.992132	72.887182
550.140544	26.948712	72.892186
549.614779	33.876444	72.897191
549.592269	25.114482	72.902196
549.114823	26.317282	72.907201
547.979070	25.246829	72.912206
547.254673	14.369080	72.917210
546.812136	31.296454	72.922215
546.222151	26.285599	72.927220
546.051801	22.046744	72.932225
544.746870	34.723980	72.937230
544.245512	21.888117	72.942234
543.545807	23.428589	72.947239
542.876768	28.155073	72.952244
541.865325	25.010807	72.957249
541.058071	26.922582	72.962254
540.488648	24.366883	72.967258
540.163873	27.092779	72.972263
539.745973	23.747344	72.977268
539.478087	16.275124	72.982273
538.472067	24.865579	72.987278
538.000725	22.650686	72.992282
537.019641	25.764943	72.997287
535.421803	24.777617	73.002292
535.356317	18.154088	73.007297
534.591471	32.009367	73.012302
534.457631	21.151209	73.017306
533.937950	17.646384	73.022311
533.175317	25.104935	73.027316
532.119436	20.292724	73.032321
531.505803	27.891130	73.037326
531.371354	21.975693	73.042330
530.256392	23.636659	73.047335
528.837478	24.276083	73.052340
528.792670	22.956340	73.057345
528.129671	24.398950	73.062350
527.922125	28.510338	73.067354
527.407266	32.668859	73.072359
526.539079	25.310154	73.077364
525.710941	21.056124	73.082369
524.413161	26.176906	73.087374
524.146539	25.018321	73.092378
523.651325	27.222796	73.097383
523.087680	24.993327	73.102388
522.418573	27.048003	73.107393
521.479848	24.589531	73.112398
520.975898	19.798402	73.117402
520.514305	18.948736	73.122407
519.800552	24.726113	73.127412
519.189159	25.782930	73.132417
518.104113	33.959852	73.137422
517.728818	14.977615	73.142426
516.900311	21.146080	73.147431
516.414266	19.448022	73.152436
515.805556	24.809923	73.157441
514.674636	30.396694	73.162446
514.132297	19.222901	73.167450
513.892185	25.150028	73.172455
513.441582	25.505911	73.177460
512.183431	23.571096	73.182465
511.642668	35.240736	73.187470
511.146092	23.656885	73.192474
510.558017	25.412693	73.197479
510.137179	30.320849	73.202484
509.169744	21.020979	73.207489
508.415978	25.006896	73.212494
507.757359	20.732111	73.217498
507.285546	27.547577	73.222503
506.580264	28.762580	73.227508
505.463002	14.548144	73.232513
505.015641	28.979772	73.237518
504.442982	25.238121	73.242522
504.092103	31.955897	73.247527
503.511407	28.508500	73.252532
502.242249	12.837941	73.257537
501.360457	32.225443	73.262542
501.135448	23.004398	73.267546
500.628511	27.486805	73.272551
500.402666	25.317476	73.277556
499.480540	25.193664	73.282561
498.495174	31.427301	73.287566
498.768004	17.723439	73.292570
497.599944	25.134629	73.297575
496.431278	26.406538	73.302580
495.821637	28.145124	73.307585
495.197624	31.903953	73.312590
494.646313	25.420906	73.317594
493.659300	25.996595	73.322599
493.152992	28.594924	73.327604
492.854453	27.599302	73.332609
492.005441	26.783659	73.337614
491.113594	16.026191	73.342618
490.613684	13.277021	73.347623
490.050970	23.289851	73.352628
489.648837	20.169077	73.357633
488.276793	27.225641	73.362638
487.645703	22.794966	73.367642
486.927040	27.217345	73.372647
486.775242	30.614616	73.377652
486.178451	18.232861	73.382657
485.493169	23.645383	73.387662
484.814859	19.623436	73.392666
483.740293	27.498976	73.397671
483.358740	33.854925	73.402676
483.218414	20.196598	73.407681
481.866760	27.591886	73.412686
481.069480	23.158902	73.417690
480.069608	26.149291	73.422695
479.990031	25.490732	73.427700
479.836020	15.547438	73.432705
479.100562	30.850229	73.437710
478.317281	25.301357	73.442714
477.458112	32.433057	73.447719
476.877621	28.166597	73.452724
476.372126	24.465149	73.457729
475.136342	31.924659	73.462734
474.224693	23.835696	73.467738
473.485016	25.489599	73.472743
473.458308	26.319527	73.477748
473.080677	23.071800	73.482753
472.773164	32.914992	73.487758
471.557396	30.802014	73.492762
470.510167	26.930912	73.497767
470.047181	21.324790	73.502772
469.972092	24.151578	73.507777
468.839773	37.762351	73.512782
468.400423	24.616291	73.517786
467.675583	35.464496	73.522791
466.911312	23.353402	73.527796
466.293167	21.107625	73.532801
465.031164	35.796085	73.537806
464.851758	27.574539	73.542810
463.888108	19.502781	73.547815
463.764306	28.691630	73.552820
463.369973	17.377626	73.557825
461.986382	25.214548	73.562830
461.541622	23.985053	73.567834
461.022075	28.794869	73.572839
460.158223	26.768423	73.577844
459.708138	21.569805	73.582849
458.257681	30.071836	73.587854
457.957324	14.657228	73.592858
457.606823	23.670987	73.597863
456.997515	24.945730	73.602868
456.974129	22.672636	73.607873
455.460270	28.831062	73.612878
454.842278	21.917370	73.617882
454.710567	26.235618	73.622887
454.183054	27.728832	73.627892
452.992969	30.095412	73.632897
451.757834	36.496194	73.637902
451.752715	25.978334	73.642906
450.988841	25.093244	73.647911
450.615757	31.249200	73.652916
449.615944	31.199891	73.657921
448.886546	28.515706	73.662926
448.153951	25.221052	73.667930
447.706060	31.358250	73.672935
447.130210	33.055922	73.677940
446.312621	20.130994	73.682945
445.435604	29.008416	73.687950
444.967560	19.122096	73.692954
444.778654	33.193663	73.697959
443.502722	38.870428	73.702964
443.158760	24.690848	73.707969
442.190371	27.674269	73.712974
441.875838	24.950965	73.717978
441.481333	33.403092	73.722983
440.346988	30.286621	73.727988
439.612237	23.889491	73.732993
438.682107	36.376206	73.737998
438.489215	27.272026	73.743002
438.082375	31.623607	73.748007
437.293272	34.050153	73.753012
436.500209	28.031283	73.758017
435.413846	34.958383	73.763022
435.084914	26.772334	73.768026
434.883523	33.281740	73.773031
433.698997	29.509961	73.778036
433.008831	29.464036	73.783041
431.987814	31.667051	73.788046
431.946647	33.057188	73.793050
431.699609	37.442567	73.798055
431.001727	34.968498	73.803060
430.123093	31.156930	73.808065
429.439879	36.173998	73.813070
428.679568	34.372563	73.818074
427.146018	27.704189	73.823079
426.789260	29.108542	73.828084
426.420997	31.889656	73.833089
425.677055	30.194359	73.838094
425.479288	22.558565	73.843098
424.995479	26.365211	73.848103
423.996228	37.404515	73.853108
423.021003	27.465382	73.858113
422.460307	29.605696	73.863118
422.305439	25.856405	73.868122
421.624868	30.607376	73.873127
420.341609	24.198070	73.878132
419.978676	25.507171	73.883137
419.211002	31.552732	73.888142
418.850018	25.897165	73.893146
418.114660	29.388125	73.898151
417.290198	31.418519	73.903156
416.775632	23.578873	73.908161
415.924350	33.502618	73.913166
415.785626	23.282777	73.918170
414.350808	34.325281	73.923175
413.398409	33.872350	73.928180
413.163175	33.255862	73.933185
412.604443	27.491297	73.938190
412.670397	22.799085	73.943194
411.681950	26.244212	73.948199
410.535874	21.287237	73.953204
410.174966	27.424132	73.958209
409.355971	28.131298	73.963214
408.837599	31.392454	73.968218
407.833626	27.088454	73.973223
406.891691	33.471758	73.978228
406.694333	25.571042	73.983233
405.933780	33.276341	73.988238
405.905376	35.887510	73.993242
404.990149	30.396790	73.998247
404.161741	25.013160	74.003252
403.872622	24.182499	74.008257
403.060641	29.397282	74.013262
401.921365	27.707374	74.018266
400.965418	25.509235	74.023271
400.435866	36.916442	74.028276
400.112614	27.289507	74.033281
399.668328	28.951216	74.038286
399.317415	30.412987	74.043290
398.293495	30.087573	74.048295
397.629590	23.211364	74.053300
397.147175	18.118555	74.058305
395.853847	19.692493	74.063310
395.339158	21.126281	74.068314
394.816164	24.068510	74.073319
393.964082	26.374414	74.078324
393.990550	19.532649	74.083329
392.707343	30.047885	74.088334
392.270295	25.908033	74.093338
391.675007	25.707310	74.098343
391.322618	26.541344	74.103348
390.448010	19.177858	74.108353
389.101547	21.712559	74.113358
388.234610	33.403754	74.118362
388.185859	33.138181	74.123367
387.068776	32.481387	74.128372
387.067865	25.866931	74.133377
386.824543	22.950254	74.138382
386.022946	19.132997	74.143386
385.091042	23.014464	74.148391
384.385620	25.345364	74.153396
383.677350	16.905804	74.158401
382.269449	23.034246	74.163406
381.774988	16.833964	74.168410
381.565826	31.035301	74.173415
380.768617	24.777960	74.178420
380.948732	23.670711	74.183425
379.941016	30.418165	74.188430
378.974772	23.294187	74.193434
378.313893	19.972653	74.198439
377.477371	25.630170	74.203444
377.543095	19.180340	74.208449
376.116588	26.447170	74.213454
375.630248	28.193846	74.218458
375.063890	28.388407	74.223463
374.371276	34.807929	74.228468
374.221521	30.278994	74.233473
373.092255	24.140927	74.238478
372.299019	25.887703	74.243482
371.973044	27.527953	74.248487
370.738510	25.372829	74.253492
369.914056	22.269976	74.258497
369.118201	31.056922	74.263502
369.151269	30.904819	74.268506
368.690824	28.597295	74.273511
368.171889	32.410754	74.278516
367.612994	22.777636	74.283521
366.093863	38.891280	74.288526
365.893872	32.161739	74.293530
365.487067	29.168482	74.298535
364.422566	36.859171	74.303540
363.740700	22.241367	74.308545
362.957050	25.579171	74.313550
362.707068	21.569097	74.318554
362.292343	20.476562	74.323559
361.363340	27.375911	74.328564
359.926050	23.413015	74.333569
359.417773	19.946128	74.338574
359.177055	19.241772	74.343578
358.719980	23.103441	74.348583
358.127672	37.980279	74.353588
357.361583	22.613535	74.358593
356.130959	25.602837	74.363598
355.886389	23.679082	74.368602
355.508582	19.157658	74.373607
354.514075	25.531819	74.378612
353.820964	22.233575	74.383617
352.786482	33.017226	74.388622
352.469042	18.731291	74.393626
352.247170	28.327311	74.398631
351.390624	32.251524	74.403636
350.524753	28.324900	74.408641
349.541502	34.698320	74.413646
349.343157	31.282123	74.418650
348.740744	21.714886	74.423655
348.114902	30.158109	74.428660
347.114216	26.376952	74.433665
346.241930	30.275445	74.438670
345.880815	25.691163	74.443674
345.438028	22.560796	74.448679
344.886515	28.014743	74.453684
344.593241	17.256963	74.458689
343.287398	26.985868	74.463694
342.495438	24.597409	74.468698
342.220493	22.826089	74.473703
341.103692	25.397621	74.478708
340.669350	30.032193	74.483713
339.975422	39.128894	74.488718
339.652180	27.411168	74.493722
339.136817	22.412035	74.498727
337.941304	30.973812	74.503732
337.038347	30.218757	74.508737
336.370639	29.460091	74.513742
336.257052	28.917490	74.518746
336.016022	28.734606	74.523751
334.760392	35.977689	74.528756
334.400873	28.689739	74.533761
333.507171	34.642443	74.538766
333.059429	32.005922	74.543770
331.928479	29.304138	74.548775
330.709152	30.532272	74.553780
330.958187	21.689059	74.558785
329.863150	33.595789	74.563790
329.844023	30.994749	74.568794
328.914174	26.758983	74.573799
327.626563	28.296434	74.578804
327.512202	23.158711	74.583809
326.775916	31.040240	74.588814
326.722624	30.779788	74.593818
325.547526	25.707028	74.598823
324.548494	32.613650	74.603828
324.338528	30.159786	74.608833
323.808638	31.834989	74.613838
322.976015	26.521570	74.618842
322.172595	22.861339	74.623847
321.372844	32.580875	74.628852
320.995031	27.380153	74.633857
320.614622	32.531636	74.638862
319.249125	37.758409	74.643866
318.651733	21.706355	74.648871
317.825480	25.553542	74.653876
317.737233	20.652120	74.658881
317.121487	31.776086	74.663886
316.731764	29.870107	74.668890
315.449536	23.707751	74.673895
314.758431	34.935815	74.678900
314.435914	26.845784	74.683905
314.031462	37.960776	74.688910
313.014926	27.844032	74.693914
312.009806	33.172055	74.698919
311.479009	36.438901	74.703924
311.314614	35.722651	74.708929
310.035948	37.702628	74.713934
309.025251	29.202815	74.718938
308.949567	25.812570	74.723943
308.040527	26.960293	74.728948
308.226368	23.162483	74.733953
307.507763	30.531013	74.738958
306.188829	20.076917	74.743962
305.554358	26.097289	74.748967
304.907907	26.847922	74.753972
304.862646	26.783845	74.758977
304.225532	37.617811	74.763982
302.532114	32.709679	74.768986
302.372074	36.639252	74.773991
302.202464	33.889147	74.778996
301.383814	26.173479	74.784001
300.112327	33.269689	74.789006
299.378578	31.384783	74.794010
299.238195	23.505105	74.799015
298.668311	37.598539	74.804020
297.756693	23.800876	74.809025
296.788202	27.833094	74.814030
296.071361	37.252257	74.819034
295.710617	24.882981	74.824039
295.501784	26.220149	74.829044
294.788633	27.167730	74.834049
293.792437	26.674176	74.839054
293.045728	23.928650	74.844058
292.633847	24.072271	74.849063
291.912885	29.333436	74.854068
290.920781	26.513924	74.859073
289.960088	31.784208	74.864078
289.836293	31.351114	74.869082
289.473951	28.964420	74.874087
288.889924	30.040257	74.879092
287.821681	31.909177	74.884097
287.019426	37.798848	74.889102
286.680514	22.702310	74.894106
286.012461	25.323642	74.899111
285.112592	29.762496	74.904116
284.183335	20.499176	74.909121
283.438532	25.196830	74.914126
282.910481	15.770015	74.919130
282.877132	26.223005	74.924135
282.152930	30.357426	74.929140
281.412073	28.607549	74.934145
280.455216	31.352985	74.939150
279.831702	34.708746	74.944154
279.564546	28.987776	74.949159
279.138030	32.421869	74.954164
278.318792	29.130652	74.959169
277.098553	29.901483	74.964174
276.864551	27.214125	74.969178
275.727830	30.277741	74.974183
274.562091	36.089590	74.979188
274.488292	34.679696	74.984193
274.137416	27.802356	74.989198
273.551185	33.418961	74.994202
273.039868	30.125884	74.999207
271.951869	32.557898	75.004212
271.460557	23.987232	75.009217
270.924621	37.633162	75.014222
270.144806	28.248312	75.019226
269.436234	18.244187	75.024231
268.316989	24.901434	75.029236
268.158893	20.316312	75.034241
267.459189	34.427257	75.039246
266.884159	29.521250	75.044250
265.912282	28.515537	75.049255
264.898921	29.415902	75.054260
264.515433	15.994286	75.059265
264.247678	28.541146	75.064270
263.916282	28.273892	75.069274
262.741975	26.493716	75.074279
261.475604	31.076310	75.079284
260.963039	22.509685	75.084289
260.972831	34.173764	75.089294
260.470676	29.085541	75.094298
259.964821	24.473583	75.099303
258.900206	33.786181	75.104308
258.209532	20.314196	75.109313
257.814414	29.510853	75.114318
256.438955	22.342191	75.119322
255.743542	19.434731	75.124327
254.915680	26.971192	75.129332
254.655679	22.658127	75.134337
254.139390	26.662181	75.139342
253.677719	25.551257	75.144346
253.594301	21.083986	75.149351
252.192976	32.626010	75.154356
251.395497	24.307947	75.159361
251.218788	31.588729	75.164366
250.128220	31.382134	75.169370
249.590159	31.983939	75.174375
248.290115	33.835367	75.179380
248.264912	27.302448	75.184385
247.625469	31.548652	75.189390
247.177697	27.368029	75.194394
246.153425	24.593909	75.199399
245.643890	31.716225	75.204404
245.236478	23.973897	75.209409
244.603507	29.659695	75.214414
243.433773	27.243252	75.219418
243.084543	25.987537	75.224423
241.937859	28.920638	75.229428
241.701521	19.900906	75.234433
241.231267	28.314305	75.239438
240.205417	26.541054	75.244442
239.279771	23.718848	75.249447
238.478565	23.543178	75.254452
238.342132	29.002952	75.259457
237.908273	24.469047	75.264462
237.421026	21.274082	75.269466
236.312530	22.539685	75.274471
235.686307	30.559055	75.279476
235.230256	17.156988	75.284481
234.435782	26.698790	75.289486
233.225558	19.334457	75.294490
232.978408	12.279886	75.299495
232.113678	15.534504	75.304500
231.786610	16.019229	75.309505
231.256890	28.768480	75.314510
230.470636	21.230822	75.319514
229.710933	20.301637	75.324519
229.137449	24.791915	75.329524
228.847101	24.818794	75.334529
227.747358	26.055269	75.339534
226.765357	19.871087	75.344538
226.009710	23.726709	75.349543
225.445528	22.801113	75.354548
225.233038	14.409234	75.359553
225.109665	18.538162	75.364558
223.676127	27.271407	75.369562
223.042417	21.685115	75.374567
222.209924	27.490373	75.379572
222.548167	6.582872	75.384577
221.389872	25.069654	75.389582
220.379958	20.015190	75.394586
219.604642	19.875346	75.399591
219.176135	29.434941	75.404596
218.782571	24.220356	75.409601
217.818548	23.266989	75.414606
217.175399	26.883474	75.419610
216.635002	15.461541	75.424615
216.237910	19.611338	75.429620
215.349526	14.408554	75.434625
214.470559	18.518589	75.439630
213.539559	16.319375	75.444634
213.430764	18.741040	75.449639
212.243202	27.136878	75.454644
211.229701	20.701535	75.459649
211.029882	21.684286	75.464654
210.489937	24.521284	75.469658
210.084530	20.763249	75.474663
209.479732	23.723462	75.479668
209.167030	19.344441	75.484673
208.048473	19.448556	75.489678
207.056961	23.192646	75.494682
206.839668	17.781675	75.499687
206.016206	25.575922	75.504692
204.916082	16.383757	75.509697
204.131123	14.281478	75.514702
203.788640	27.136387	75.519706
203.640394	12.530585	75.524711
202.817274	24.479126	75.529716
202.011628	20.861931	75.534721
200.834900	14.404052	75.539726
200.251578	20.152387	75.544730
199.983773	11.432910	75.549735
199.177749	28.774247	75.554740
199.253301	17.922482	75.559745
198.959134	21.085616	75.564750
197.497729	24.741319	75.569754
196.795606	21.612797	75.574759
195.998237	27.145605	75.579764
195.270446	22.349084	75.584769
194.560475	18.459718	75.589774
193.753103	16.553113	75.594778
193.619296	20.491210	75.599783
192.828679	19.823104	75.604788
192.345973	10.422485	75.609793
191.453072	13.051187	75.614798
190.829806	20.040242	75.619802
190.668224	22.289782	75.624807
189.189202	25.164213	75.629812
188.236346	21.329902	75.634817
188.029054	13.630254	75.639822
187.666201	21.960112	75.644826
187.322468	19.119477	75.649831
185.844503	28.132303	75.654836
185.306240	17.635218	75.659841
184.758716	23.097963	75.664846
184.644863	22.626855	75.669850
184.181708	16.506894	75.674855
182.825003	23.335511	75.679860
182.514911	21.327480	75.684865
181.576610	17.943018	75.689870
180.379241	22.765232	75.694874
179.961070	18.251146	75.699879
179.076335	24.317584	75.704884
179.289435	28.073854	75.709889
178.638301	18.509090	75.714894
177.913018	20.285691	75.719898
176.879135	9.765028	75.724903
176.280141	24.467740	75.729908
175.469435	24.216346	75.734913
174.555610	25.650686	75.739918
173.622652	33.316088	75.744922
172.842768	17.646266	75.749927
172.756198	32.445476	75.754932
172.476642	19.791146	75.759937
172.130649	19.137609	75.764942
171.393942	25.437210	75.769946
170.479212	25.389559	75.774951
169.852794	24.281624	75.779956
169.170375	26.259682	75.784961
168.580473	21.777403	75.789966
167.377312	25.251485	75.794970
166.811163	20.539360	75.799975
166.192028	20.760754	75.804980
165.805251	21.479522	75.809985
165.422737	14.456453	75.814990
164.032902	23.606532	75.819994
163.726419	11.852034	75.824999
162.928443	28.793725	75.830004
162.471840	20.209635	75.835009
161.417660	14.608995	75.840014
160.788149	19.039017	75.845018
160.354653	16.654273	75.850023
159.013255	21.572624	75.855028
158.590248	17.250411	75.860033
158.893593	17.135259	75.865038
157.882858	27.183453	75.870042
157.060825	21.779449	75.875047
156.367305	21.575860	75.880052
155.976660	26.263339	75.885057
155.278875	24.352559	75.890062
154.604096	31.514652	75.895066
154.151256	15.659704	75.900071
152.931253	20.756576	75.905076
152.873070	19.169941	75.910081
151.519037	29.693804	75.915086
150.487427	31.518186	75.920090
150.357316	17.881064	75.925095
149.589306	28.625762	75.930100
149.182755	25.696432	75.935105
148.845156	27.142514	75.940110
147.867685	22.146057	75.945114
147.457652	16.162250	75.950119
146.455864	22.532556	75.955124
146.162282	23.340736	75.960129
145.207855	15.190524	75.965134
143.994739	22.932766	75.970138
143.546384	20.682799	75.975143
143.055836	26.097493	75.980148
142.649031	21.492257	75.985153
142.237648	21.258461	75.990158
141.078433	12.604970	75.995162
140.571924	7.268062	76.000167
139.843195	15.788524	76.005172
139.249379	12.739731	76.010177
139.276375	10.659709	76.015182
137.978224	23.554896	76.020186
137.919811	14.471525	76.025191
136.816207	24.993112	76.030196
136.228938	17.650301	76.035201
135.332138	13.318531	76.040206
134.509435	20.792935	76.045210
134.132406	14.862680	76.050215
132.684375	17.994691	76.055220
132.167587	17.049537	76.060225
131.574561	12.681480	76.065230
130.845453	21.833156	76.070234
131.091151	15.059217	76.075239
130.435131	12.694074	76.080244
129.292154	14.981602	76.085249
128.233566	16.045659	76.090254
127.663639	14.367950	76.095258
127.284243	0.345320	76.100263
127.054018	13.561075	76.105268
126.687600	11.775063	76.110273
125.734680	9.840927	76.115278
124.941771	12.312374	76.120282
124.686340	12.594179	76.125287
123.698787	9.455398	76.130292
122.538314	10.910716	76.135297
122.277667	13.009091	76.140302
121.103101	18.520522	76.145306
120.134059	14.775052	76.150311
119.414060	23.019303	76.155316
118.736427	11.955641	76.160321
118.810641	11.738066	76.165326
118.159864	17.686642	76.170330
117.959558	9.470313	76.175335
117.340789	16.453863	76.180340
116.504451	18.751585	76.185345
115.776994	10.270781	76.190350
114.475439	13.201644	76.195354
113.837553	11.503222	76.200359
112.839901	15.746901	76.205364
112.629364	4.770526	76.210369
111.681717	12.113200	76.215374
110.991818	13.911373	76.220378
111.413547	10.601252	76.225383
110.770055	13.407853	76.230388
110.140701	10.342659	76.235393
109.077566	10.620444	76.240398
108.010941	6.740534	76.245402
107.644617	8.077864	76.250407
106.491072	10.417337	76.255412
105.900823	12.394993	76.260417
104.984606	10.956249	76.265422
104.423702	14.955328	76.270426
104.185580	13.736233	76.275431
104.130758	16.058650	76.280436
103.519479	14.011873	76.285441
102.641380	13.654816	76.290446
101.612382	19.172872	76.295450
101.499982	10.654123	76.300455
99.893021	9.800350	76.305460
99.150283	7.109443	76.310465
99.123470	10.587116	76.315470
98.403370	12.384152	76.320474
97.916578	4.608103	76.325479
96.724020	2.854392	76.330484
95.899921	14.803887	76.335489
95.673645	12.801626	76.340494
95.199782	12.051210	76.345498
94.643471	12.023437	76.350503
93.615747	13.920974	76.355508
92.857675	14.472494	76.360513
92.255347	11.584237	76.365518
91.889991	19.197724	76.370522
91.381313	8.712173	76.375527
90.065895	17.059686	76.380532
89.668100	9.569149	76.385537
89.380728	21.465709	76.390542
88.740270	19.478801	76.395546
88.099424	22.570725	76.400551
87.629496	14.446803	76.405556
86.633411	17.504897	76.410561
85.896262	5.791098	76.415566
84.785600	16.289028	76.420570
84.308670	11.576623	76.425575
84.050938	23.446789	76.430580
83.718491	22.728178	76.435585
82.242879	15.725956	76.440590
81.306367	19.427087	76.445594
80.786601	12.490718	76.450599
80.276996	15.959984	76.455604
79.692311	14.288759	76.460609
79.009777	1.753679	76.465614
77.923289	14.149581	76.470618
77.749443	5.013385	76.475623
77.155911	7.945231	76.480628
76.640548	13.265500	76.485633
76.221758	12.794968	76.490638
74.771430	16.613793	76.495642
74.336677	22.869922	76.500647
73.655300	22.396255	76.505652
73.198453	16.624946	76.510657
73.142916	10.750891	76.515662
71.803721	13.511387	76.520666
70.947057	7.521278	76.525671
70.206082	15.006146	76.530676
69.725755	14.380386	76.535681
69.293179	13.993134	76.540686
68.907480	15.326685	76.545690
67.882217	3.791754	76.550695
67.194483	11.706807	76.555700
66.959453	9.726180	76.560705
66.605765	8.873458	76.565710
65.239352	17.860864	76.570714
64.839687	15.853597	76.575719
64.055874	17.142911	76.580724
62.970401	19.169558	76.585729
62.493895	4.452318	76.590734
61.673262	11.395483	76.595738
61.103425	5.587897	76.600743
60.570396	6.340824	76.605748
60.277527	9.012716	76.610753
59.794757	1.075733	76.615758
58.414689	6.638193	76.620762
58.377480	2.804425	76.625767
57.833843	0.415291	76.630772
56.606739	11.046863	76.635777
55.750582	-3.767899	76.640782
54.985420	13.225381	76.645786
54.757881	-1.201006	76.650791
54.661579	4.870388	76.655796
52.783152	16.241618	76.660801
52.232216	0.427215	76.665806
51.404351	23.527580	76.670810
51.073446	10.953133	76.675815
50.576145	9.210093	76.680820
50.516584	13.129536	76.685825
50.104568	9.060835	76.690830
48.761717	10.581778	76.695834
48.351894	14.890858	76.700839
47.926233	10.996196	76.705844
46.237209	12.670827	76.710849
45.686981	6.549639	76.715854
45.033811	8.529011	76.720858
45.017204	13.695878	76.725863
44.280033	14.944042	76.730868
43.835726	17.528618	76.735873
42.982891	8.990782	76.740878
42.211123	14.930109	76.745882
41.794361	12.152930	76.750887
41.192973	15.320192	76.755892
39.879370	15.726983	76.760897
39.516586	8.073356	76.765902
38.901689	10.892824	76.770906
38.427916	6.556047	76.775911
37.516681	11.888930	76.780916
36.389503	13.595122	76.785921
36.053765	10.473284	76.790926
35.746766	19.717188	76.795930
35.273688	5.209748	76.800935
34.513711	12.880233	76.805940
33.407887	10.616699	76.810945
33.253686	3.345709	76.815950
32.303133	14.784816	76.820954
31.177142	10.579994	76.825959
30.332045	10.757654	76.830964
29.571070	19.973611	76.835969
29.587485	6.347712	76.840974
28.862147	20.364359	76.845978
28.734466	13.768118	76.850983
28.365898	18.278139	76.855988
27.164617	8.841689	76.860993
26.706154	4.906869	76.865998
25.353077	17.870691	76.871002
24.669535	17.605810	76.876007
23.782551	10.013249	76.881012
23.154634	15.504783	76.886017
22.899358	12.412963	76.891022
22.254924	9.776264	76.896026
22.032695	10.599846	76.901031
21.704295	16.906025	76.906036
20.346544	20.992791	76.911041
19.727692	5.078728	76.916046
19.134057	21.443435	76.921050
18.970225	11.323878	76.926055
17.359166	15.598145	76.931060
16.877117	27.735702	76.936065
16.622125	10.613793	76.941070
15.788373	13.734061	76.946074
15.093377	11.338122	76.951079
14.181734	10.587386	76.956084
13.709763	14.997512	76.961089
13.250165	8.991439	76.966094
12.802932	20.773701	76.971098
12.045449	9.597453	76.976103
10.881907	12.191277	76.981108
10.388727	12.387938	76.986113
10.238412	13.517329	76.991118
8.867599	15.746849	76.996122
7.740045	15.262461	77.001127
7.772826	19.445922	77.006132
7.223282	18.882165	77.011137
7.054251	12.172629	77.016142
5.770824	23.792364	77.021147
5.159633	16.854710	77.026151
4.921968	14.349966	77.031156
4.272507	14.146741	77.036161