Tue Jun 08 18:04:26 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.117503	89.574585	0.000000
-0.928570	93.187726	0.005005
-1.964083	51.860403	0.010010
-3.393908	3.912026	0.015014
-8.094988	-12.471990	0.020019
-13.760807	-14.897013	0.025024
-18.947288	-7.663157	0.030029
-23.217154	-9.663232	0.035034
-26.987972	-11.368373	0.040038
-30.770643	-12.443099	0.045043
-34.177966	-19.446791	0.050048
-38.228917	-9.917793	0.055053
-41.663537	-10.081993	0.060058
-45.228303	-12.605952	0.065062
-49.606306	-3.313736	0.070067
-53.169147	-15.068324	0.075072
-56.797709	-10.704294	0.080077
-60.666740	-11.053707	0.085082
-64.295931	-9.818827	0.090086
-67.986978	-8.718196	0.095091
-71.792090	-22.929339	0.100096
-75.520576	-2.478318	0.105101
-79.936315	-5.915333	0.110106
-83.533929	-10.450204	0.115110
-87.450923	-7.004518	0.120115
-90.634222	-12.555367	0.125120
-94.368711	-15.203723	0.130125
-97.900637	-12.047074	0.135130
-101.840442	-9.236502	0.140134
-105.892265	-10.218433	0.145139
-109.611446	-9.629620	0.150144
-113.311898	-6.727856	0.155149
-117.279016	-16.250437	0.160154
-120.290360	-9.754594	0.165158
-124.370831	-11.321293	0.170163
-128.107607	-19.632527	0.175168
-132.483947	-12.221716	0.180173
-136.439158	-10.947448	0.185178
-139.939243	-3.836889	0.190182
-144.071311	-2.524389	0.195187
-147.112503	-11.217382	0.200192
-151.398813	-12.915323	0.205197
-155.075471	-3.895258	0.210202
-158.451183	-15.531062	0.215206
-162.257802	-6.969857	0.220211
-165.873692	-10.473699	0.225216
-169.626150	-2.929075	0.230221
-173.489547	-1.558422	0.235226
-177.372400	-12.651741	0.240230
-181.252637	-5.658313	0.245235
-184.697106	-9.758737	0.250240
-188.724399	-1.584371	0.255245
-192.298695	-7.591866	0.260250
-196.158708	-11.531807	0.265254
-199.791928	-4.806109	0.270259
-203.247367	-12.032712	0.275264
-207.310987	-10.699134	0.280269
-211.566179	-10.552349	0.285274
-214.982335	-5.599802	0.290278
-218.771062	-7.048700	0.295283
-222.251772	-12.829867	0.300288
-226.471723	-5.698013	0.305293
-230.163065	-10.050905	0.310298
-233.785819	-13.131173	0.315302
-237.200098	-4.751668	0.320307
-240.442504	-5.920066	0.325312
-244.983977	-4.307928	0.330317
-248.964650	-2.891047	0.335322
-252.470208	-5.430124	0.340326
-256.284840	-1.708190	0.345331
-260.126030	-4.149039	0.350336
-263.900399	-5.524971	0.355341
-267.724884	-13.030433	0.360346
-271.260231	-9.982402	0.365350
-275.445547	-7.123257	0.370355
-279.062569	-5.756488	0.375360
-282.997912	-0.185138	0.380365
-286.746329	-2.702661	0.385370
-290.101698	-9.231142	0.390374
-293.511528	-7.324020	0.395379
-297.091998	-8.319527	0.400384
-301.459906	-1.056840	0.405389
-305.205166	-9.019906	0.410394
-309.242291	-7.540003	0.415398
-313.193786	3.098266	0.420403
-316.670340	-4.614851	0.425408
-320.120047	-5.582248	0.430413
-323.714722	-10.580018	0.435418
-327.449058	-14.209447	0.440422
-331.912286	-5.357862	0.445427
-335.411707	-11.727394	0.450432
-339.416251	-8.977352	0.455437
-343.077771	-7.334102	0.460442
-346.184544	-16.602621	0.465446
-350.313895	-7.202810	0.470451
-353.813009	-4.832332	0.475456
-358.398154	-7.419796	0.480461
-361.934238	-11.427785	0.485466
-365.525521	-10.954248	0.490470
-369.312772	-5.566512	0.495475
-372.411558	-15.658165	0.500480
-376.485364	-9.234100	0.505485
-380.515306	-14.152809	0.510490
-384.186693	-14.112720	0.515494
-388.551611	-3.994750	0.520499
-391.840179	-4.027827	0.525504
-395.511017	-5.406014	0.530509
-399.316201	-16.249952	0.535514
-402.839523	-14.332752	0.540518
-406.830019	-5.852309	0.545523
-410.562267	-12.108813	0.550528
-414.311505	-7.833932	0.555533
-418.443357	-10.664874	0.560538
-421.675174	-14.330302	0.565542
-425.434425	-7.291522	0.570547
-429.327744	-4.983612	0.575552
-433.055581	-6.626705	0.580557
-437.072748	-5.538111	0.585562
-440.708759	-14.109881	0.590566
-444.146943	-2.835288	0.595571
-448.132204	-7.840148	0.600576
-452.334296	-10.330609	0.605581
-455.975511	-8.922051	0.610586
-459.283897	-7.608090	0.615590
-462.816850	-5.819049	0.620595
-466.984462	-8.570394	0.625600
-471.178576	-1.995352	0.630605
-474.960709	-8.130353	0.635610
-478.079936	-12.421722	0.640614
-481.981311	-5.333647	0.645619
-485.767570	-0.376219	0.650624
-489.435819	0.287058	0.655629
-493.549553	-3.898011	0.660634
-497.058688	-3.575426	0.665638
-501.087001	2.975540	0.670643
-504.871298	0.816837	0.675648
-508.192837	3.713111	0.680653
-511.841799	-3.988018	0.685658
-515.795948	-6.129014	0.690662
-519.859383	1.307404	0.695667
-523.482834	-5.068318	0.700672
-527.246904	-3.262860	0.705677
-531.209412	-0.492233	0.710682
-534.326272	-3.279734	0.715686
-538.565064	0.727167	0.720691
-542.254715	-7.863334	0.725696
-546.373210	-4.474656	0.730701
-549.772317	-3.495957	0.735706
-552.769507	-5.421015	0.740710
-557.101334	-0.858962	0.745715
-561.019554	-5.065276	0.750720
-564.874613	-0.121635	0.755725
-568.581803	-2.011295	0.760730
-572.522281	-4.649944	0.765734
-576.004617	-3.174216	0.770739
-579.560341	-4.674228	0.775744
-583.444229	-7.756361	0.780749
-587.518076	1.968840	0.785754
-591.159737	-6.205145	0.790758
-595.265175	-2.273571	0.795763
-599.052398	-0.299092	0.800768
-602.605455	-1.588769	0.805773
-606.233994	6.917750	0.810778
-609.812849	-4.842264	0.815782
-613.617534	4.619682	0.820787
-617.191698	-4.434220	0.825792
-620.968705	0.045316	0.830797
-625.088307	-8.881428	0.835802
-628.865794	-2.767318	0.840806
-632.848764	0.809351	0.845811
-636.284428	-7.820700	0.850816
-639.854351	-2.782255	0.855821
-643.617029	-0.733799	0.860826
-647.606321	-3.001264	0.865830
-651.338138	2.647957	0.870835
-654.861049	-5.308734	0.875840
-659.187001	-4.382854	0.880845
-662.879998	-1.009858	0.885850
-666.446156	0.777541	0.890854
-670.460104	4.468894	0.895859
-673.945582	-3.444077	0.900864
-677.438212	-12.533225	0.905869
-681.448996	2.716218	0.910874
-685.193596	-0.474589	0.915878
-689.218720	-5.645652	0.920883
-692.687901	-5.438708	0.925888
-696.591937	-6.875294	0.930893
-699.964034	7.551715	0.935898
-703.736014	-3.924033	0.940902
-707.918729	-7.911538	0.945907
-711.448561	-8.675413	0.950912
-715.530001	-0.600261	0.955917
-719.176821	-4.707357	0.960922
-722.799601	-1.744228	0.965926
-726.545998	2.063085	0.970931
-729.994465	-0.832742	0.975936
-734.223634	-2.641751	0.980941
-738.328488	-5.446229	0.985946
-741.649887	-5.332104	0.990950
-745.372360	11.657517	0.995955
-748.999759	4.304191	1.000960
-752.832520	0.824650	1.005965
-756.807412	0.778204	1.010970
-760.155369	-0.081974	1.015974
-764.073226	-0.188331	1.020979
-767.898988	-2.268635	1.025984
-771.732401	-2.187388	1.030989
-775.301733	-1.956478	1.035994
-779.029284	-0.049321	1.040998
-782.824091	-4.194903	1.046003
-787.093255	-5.543081	1.051008
-790.359637	1.630849	1.056013
-794.190202	2.961665	1.061018
-798.235062	-10.718557	1.066022
-802.293563	-5.493899	1.071027
-805.798337	-9.001661	1.076032
-808.954849	-5.485385	1.081037
-812.792513	2.786016	1.086042
-816.728674	-4.048096	1.091046
-820.413228	0.736237	1.096051
-824.410669	-0.949444	1.101056
-828.202737	2.206237	1.106061
-832.288639	6.388074	1.111066
-835.529789	1.535708	1.116070
-839.472419	-6.473104	1.121075
-842.814575	3.925207	1.126080
-847.324282	1.271242	1.131085
-851.112468	8.259674	1.136090
-854.050686	-1.852445	1.141094
-858.120171	-0.229133	1.146099
-861.725597	-6.873280	1.151104
-865.922224	-3.842714	1.156109
-869.616339	-1.720973	1.161114
-872.958815	-0.115873	1.166118
-877.154618	-2.364645	1.171123
-880.640012	-6.713633	1.176128
-884.662932	-3.920879	1.181133
-888.589039	4.314060	1.186138
-892.285631	-6.888276	1.191142
-895.733419	0.766832	1.196147
-899.447603	-7.115358	1.201152
-903.329298	-10.206253	1.206157
-907.351433	-9.042963	1.211162
-910.834921	2.205775	1.216166
-914.734509	9.745448	1.221171
-918.335180	0.313505	1.226176
-921.892272	-6.538606	1.231181
-926.135339	-1.872240	1.236186
-929.709596	-3.169057	1.241190
-933.767126	4.813765	1.246195
-937.159337	-2.266757	1.251200
-940.570555	0.444718	1.256205
-944.444995	-8.035921	1.261210
-948.500095	-2.231104	1.266214
-952.364975	2.794672	1.271219
-955.954051	2.516397	1.276224
-959.588623	6.001176	1.281229
-963.527655	4.342701	1.286234
-967.027519	1.427082	1.291238
-971.220890	8.660423	1.296243
-974.853176	-2.274606	1.301248
-978.325257	-2.975155	1.306253
-982.310566	-5.170361	1.311258
-985.833101	-9.432755	1.316262
-990.351944	-2.531124	1.321267
-993.465319	-1.101834	1.326272
-997.411043	-0.312341	1.331277
-1001.414433	-2.432194	1.336282
-1004.754106	-2.634441	1.341286
-1009.050384	-3.910245	1.346291
-1012.648621	-4.359386	1.351296
-1016.194663	-3.542584	1.356301
-1020.258793	-6.540868	1.361306
-1023.935267	-5.870994	1.366310
-1027.554848	2.635879	1.371315
-1031.242041	-10.769603	1.376320
-1034.706569	-5.516469	1.381325
-1038.813453	-7.027639	1.386330
-1042.659698	-5.071066	1.391334
-1046.275505	3.432015	1.396339
-1049.821700	-2.380223	1.401344
-1053.747490	-3.010701	1.406349
-1057.944890	4.433787	1.411354
-1061.039220	-3.553497	1.416358
-1065.138264	-6.717438	1.421363
-1069.039735	2.188761	1.426368
-1072.547297	-3.490364	1.431373
-1076.385227	1.065926	1.436378
-1079.734080	-6.154930	1.441382
-1084.035663	1.342598	1.446387
-1087.676085	-10.991730	1.451392
-1091.502883	-9.720505	1.456397
-1095.637602	1.588081	1.461402
-1098.847845	-9.487575	1.466406
-1102.691678	-5.557044	1.471411
-1106.365460	-6.176277	1.476416
-1110.227942	-2.362133	1.481421
-1113.968878	-10.750271	1.486426
-1117.523673	-6.090605	1.491430
-1121.452657	-3.250217	1.496435
-1125.189697	-6.972011	1.501440
-1129.182986	-6.003321	1.506445
-1132.959281	-5.339501	1.511450
-1136.172274	-2.867951	1.516454
-1140.271200	0.766182	1.521459
-1144.292811	-5.697299	1.526464
-1147.999450	-4.748213	1.531469
-1151.704180	0.434163	1.536474
-1155.197349	-17.693216	1.541478
-1159.337340	-4.240423	1.546483
-1162.794735	-9.842822	1.551488
-1166.636716	-7.723464	1.556493
-1170.562074	0.948123	1.561498
-1173.925723	-4.158040	1.566502
-1178.169983	-0.895988	1.571507
-1181.917877	-4.659679	1.576512
-1185.548851	0.613473	1.581517
-1189.000828	-1.864557	1.586522
-1192.612250	-6.896576	1.591526
-1196.811065	1.707531	1.596531
-1200.781859	-7.457301	1.601536
-1204.266036	2.769866	1.606541
-1208.300606	5.922522	1.611546
-1211.612877	2.692680	1.616550
-1215.542447	1.570409	1.621555
-1219.311835	-1.714331	1.626560
-1223.210292	-3.590299	1.631565
-1227.080856	2.650802	1.636570
-1230.357091	-1.185165	1.641574
-1234.731856	1.402306	1.646579
-1238.464112	-3.739567	1.651584
-1241.806797	-9.559740	1.656589
-1245.595078	-10.960043	1.661594
-1248.754061	-7.173846	1.666598
-1252.946407	-2.056049	1.671603
-1256.912206	-5.273075	1.676608
-1260.581096	-3.926986	1.681613
-1264.671378	-9.623476	1.686618
-1268.328127	-7.653068	1.691622
-1272.157397	-0.055710	1.696627
-1275.677635	-0.276068	1.701632
-1279.097414	-7.010527	1.706637
-1283.205536	2.314601	1.711642
-1287.081402	-1.598315	1.716646
-1291.247408	0.699957	1.721651
-1294.609261	-9.397457	1.726656
-1298.297561	-3.100373	1.731661
-1301.906403	-5.514655	1.736666
-1305.638495	-9.210686	1.741670
-1309.659543	-4.634586	1.746675
-1313.304619	-6.108762	1.751680
-1317.112557	-11.119147	1.756685
-1320.963165	1.945029	1.761690
-1324.499813	-6.451154	1.766694
-1328.512639	-4.410849	1.771699
-1332.317129	-12.834036	1.776704
-1335.693464	-9.232267	1.781709
-1339.802803	-7.659283	1.786714
-1343.571732	-13.957554	1.791718
-1347.229265	-1.759746	1.796723
-1350.752608	-11.972646	1.801728
-1354.574681	-10.439518	1.806733
-1358.130088	-10.271691	1.811738
-1362.253392	-7.647161	1.816742
-1366.255859	-10.043109	1.821747
-1369.919196	-10.517863	1.826752
-1373.625428	-5.282156	1.831757
-1377.577835	-0.824749	1.836762
-1380.928442	-16.673676	1.841766
-1384.624537	-2.592397	1.846771
-1387.888420	-9.219732	1.851776
-1392.149963	-8.816901	1.856781
-1395.926629	-7.584407	1.861786
-1399.519814	-12.964338	1.866790
-1404.164491	-5.213774	1.871795
-1407.821119	-11.063550	1.876800
-1411.516737	-16.787422	1.881805
-1415.271296	-7.713168	1.886810
-1418.380328	-17.456426	1.891814
-1422.370364	-13.084878	1.896819
-1425.949602	-9.491602	1.901824
-1429.618053	-13.829975	1.906829
-1433.804450	-1.457967	1.911834
-1437.448094	-14.215300	1.916838
-1441.573659	-14.319291	1.921843
-1444.975630	-15.430146	1.926848
-1448.464017	-8.382612	1.931853
-1452.135524	-15.573757	1.936858
-1455.816352	-9.149551	1.941862
-1460.288053	-6.081026	1.946867
-1463.565821	-10.946711	1.951872
-1467.489243	-11.842053	1.956877
-1471.591233	0.166570	1.961882
-1474.984978	-12.132384	1.966886
-1478.759594	-1.236623	1.971891
-1482.526684	-2.880723	1.976896
-1486.452591	-1.852226	1.981901
-1490.393795	-2.263346	1.986906
-1493.867304	-6.118880	1.991910
-1497.695314	-3.171957	1.996915
-1501.764316	-6.087719	2.006912
-1502.544603	-4.256701	2.016909
-1499.795875	-6.622078	2.026906
-1497.138102	-8.411813	2.036902
-1494.802324	-1.261913	2.046899
-1492.692438	-10.655410	2.056896
-1491.681489	-7.793957	2.066893
-1489.624165	-3.282060	2.076890
-1487.813294	-4.208193	2.086886
-1485.261099	-5.937099	2.096883
-1483.515266	-6.150559	2.106880
-1481.520885	-3.700323	2.116877
-1479.783790	-6.506041	2.126874
-1478.356868	-0.886347	2.136870
-1476.026193	-2.440054	2.146867
-1474.020182	-8.886402	2.156864
-1472.137865	-10.987509	2.166861
-1470.403227	-10.554058	2.176858
-1468.735767	-11.942442	2.186854
-1466.556987	-3.130176	2.196851
-1464.715637	-14.239370	2.206848
-1462.851262	-13.787102	2.216845
-1461.067657	-14.274203	2.226842
-1458.949065	-9.804829	2.236838
-1457.088929	-7.917219	2.246835
-1455.361192	-13.632434	2.256832
-1453.387798	-11.603429	2.266829
-1451.438322	-12.402388	2.276826
-1449.144930	-11.564583	2.286822
-1447.924845	-8.811766	2.296819
-1446.333453	-2.376937	2.306816
-1443.953202	-3.628112	2.316813
-1442.012082	-5.904111	2.326810
-1440.313951	-10.395803	2.336806
-1438.305546	-1.993723	2.346803
-1436.393113	-9.668101	2.356800
-1434.728250	-0.866329	2.366797
-1432.553692	-10.398168	2.376794
-1430.740167	-5.473650	2.386790
-1428.774119	-8.392189	2.396787
-1427.044085	-9.816996	2.406784
-1425.280208	-10.978082	2.416781
-1423.195681	-14.602265	2.426778
-1421.584661	-13.368599	2.436774
-1419.645339	-12.831965	2.446771
-1417.477411	-11.059260	2.456768
-1415.456599	-6.714943	2.466765
-1414.090333	-12.318646	2.476762
-1412.132614	-12.487062	2.486758
-1409.922334	-11.446443	2.496755
-1408.343917	-12.134214	2.506752
-1406.327928	-10.804516	2.516749
-1404.366454	-5.073878	2.526746
-1402.701806	-6.894904	2.536742
-1400.831305	-5.736630	2.546739
-1398.972859	-9.497834	2.556736
-1396.647035	-10.873214	2.566733
-1395.027363	-9.945335	2.576730
-1393.444740	-3.746102	2.586726
-1391.487863	-11.803941	2.596723
-1389.379820	-12.232528	2.606720
-1387.373703	-11.172634	2.616717
-1385.609596	-16.480681	2.626714
-1383.868834	-12.151476	2.636710
-1381.925929	-19.539398	2.646707
-1379.872637	-11.570640	2.656704
-1378.338877	-16.673523	2.666701
-1376.503839	-14.158714	2.676698
-1374.363356	-11.279031	2.686694
-1372.467503	-17.819442	2.696691
-1370.930388	-12.631631	2.706688
-1368.640512	-10.781044	2.716685
-1366.891277	-10.106607	2.726682
-1365.023761	-10.796992	2.736678
-1363.279551	-4.995814	2.746675
-1361.296236	-7.388499	2.756672
-1359.410848	-7.067051	2.766669
-1357.537310	-6.889795	2.776666
-1355.575748	-10.257675	2.786662
-1353.531384	-10.205401	2.796659
-1352.061005	-6.704731	2.806656
-1350.126610	-3.167966	2.816653
-1348.014724	-8.285968	2.826650
-1346.049559	-13.121087	2.836646
-1344.641444	-7.438829	2.846643
-1342.456195	-7.163743	2.856640
-1340.696264	-10.813547	2.866637
-1338.795088	-7.326006	2.876634
-1336.756740	-11.202661	2.886630
-1334.502292	-16.029764	2.896627
-1332.985986	-11.856819	2.906624
-1331.106538	-2.991472	2.916621
-1329.461917	-7.056592	2.926618
-1327.843029	-3.605923	2.936614
-1325.828099	-8.065044	2.946611
-1323.689193	-10.371801	2.956608
-1321.897517	-8.040404	2.966605
-1319.834306	-4.082325	2.976602
-1318.039214	-9.406737	2.986598
-1316.218416	-5.921188	2.996595
-1314.121940	-7.389525	3.006592
-1312.471468	-8.923135	3.016589
-1310.653940	-8.023278	3.026586
-1308.642758	-4.889755	3.036582
-1306.587030	-0.158536	3.046579
-1305.003990	-8.237894	3.056576
-1303.534773	-9.947064	3.066573
-1301.307203	-3.584289	3.076570
-1299.339914	-3.462630	3.086566
-1297.110244	-3.058407	3.096563
-1295.517980	-0.469452	3.106560
-1293.977701	-2.789569	3.116557
-1291.768472	-5.355792	3.126554
-1289.867108	-5.421991	3.136550
-1288.117670	-5.679066	3.146547
-1285.868055	-11.074025	3.156544
-1284.228363	-8.251739	3.166541
-1282.342155	-5.272606	3.176538
-1280.577900	-5.896608	3.186534
-1278.836808	-5.770077	3.196531
-1276.908137	-0.513916	3.206528
-1274.775857	-4.220534	3.216525
-1272.761690	-5.890895	3.226522
-1271.154788	-7.933547	3.236518
-1269.295387	-8.348615	3.246515
-1267.503785	-2.768548	3.256512
-1265.524945	0.522709	3.266509
-1263.612287	-1.549532	3.276506
-1261.476041	0.774091	3.286502
-1260.079652	-8.404290	3.296499
-1258.012359	-6.260106	3.306496
-1256.029482	-6.045463	3.316493
-1254.535971	-11.426343	3.326490
-1252.551080	-1.785479	3.336486
-1250.699511	-2.745770	3.346483
-1248.506811	-3.890326	3.356480
-1246.398616	-0.784497	3.366477
-1245.064228	-2.734888	3.376474
-1243.303457	6.669807	3.386470
-1241.206774	-2.922092	3.396467
-1239.417866	-5.842928	3.406464
-1237.286794	-1.565667	3.416461
-1235.081031	6.103512	3.426458
-1233.532150	-1.699243	3.436454
-1231.649857	-2.403173	3.446451
-1230.082647	-5.136541	3.456448
-1227.937010	-6.505783	3.466445
-1226.176261	-7.293962	3.476442
-1224.472039	-5.501982	3.486438
-1222.329515	-1.086774	3.496435
-1220.409596	-1.296429	3.506432
-1218.486245	-5.077798	3.516429
-1216.672263	1.826755	3.526426
-1215.162495	-2.806007	3.536422
-1212.814270	-5.165653	3.546419
-1211.009041	-11.328824	3.556416
-1209.142026	-11.736478	3.566413
-1207.406809	-4.735402	3.576410
-1205.420777	-6.460577	3.586406
-1203.912773	-12.720904	3.596403
-1201.665237	-8.750154	3.606400
-1199.636357	-11.286543	3.616397
-1198.272107	-10.138852	3.626394
-1195.889364	-5.521040	3.636390
-1194.290105	-4.070663	3.646387
-1192.353039	-13.200788	3.656384
-1190.386933	-10.570077	3.666381
-1188.701576	-7.015363	3.676378
-1186.524213	-6.270120	3.686374
-1184.598833	-4.561947	3.696371
-1182.843198	-5.810837	3.706368
-1181.383410	-6.216127	3.716365
-1179.467749	-9.116023	3.726362
-1177.473440	-1.848394	3.736358
-1175.370759	-2.691716	3.746355
-1173.326308	-9.853551	3.756352
-1171.668711	-4.737721	3.766349
-1169.866816	-4.527131	3.776346
-1167.794401	-0.766970	3.786342
-1166.105692	-9.900283	3.796339
-1164.095197	-7.481900	3.806336
-1162.268653	-7.863614	3.816333
-1160.534149	-6.990535	3.826330
-1158.700555	-4.297925	3.836326
-1156.504746	-4.779803	3.846323
-1154.431156	-12.418120	3.856320
-1153.031492	-12.757351	3.866317
-1151.411913	-12.473158	3.876314
-1149.245343	-3.223866	3.886310
-1147.479064	-0.914902	3.896307
-1145.344448	-6.558791	3.906304
-1143.237674	-8.518085	3.916301
-1141.424994	-5.380030	3.926298
-1139.938106	-6.787077	3.936294
-1137.736854	-4.940901	3.946291
-1136.010806	-3.603567	3.956288
-1134.114709	-2.180031	3.966285
-1132.342758	-9.808831	3.976282
-1130.509981	-2.852529	3.986278
-1128.440481	-7.937860	3.996275
-1126.860708	-8.139650	4.006272
-1125.015551	-7.422300	4.016269
-1122.900096	-5.892570	4.026266
-1120.979715	-0.573253	4.036262
-1119.098462	-5.385967	4.046259
-1117.223953	-4.088346	4.056256
-1115.238591	-9.510962	4.066253
-1113.562372	-7.823204	4.076250
-1111.672916	1.827017	4.086246
-1109.804240	-6.070926	4.096243
-1107.891591	-8.874239	4.106240
-1105.883229	-3.733640	4.116237
-1103.887612	-0.272869	4.126234
-1102.263198	-6.898573	4.136230
-1100.411873	1.459933	4.146227
-1098.707185	-1.522268	4.156224
-1096.798151	2.940218	4.166221
-1094.902647	-0.104388	4.176218
-1092.878211	1.317286	4.186214
-1090.708541	-0.922319	4.196211
-1088.969851	-8.429992	4.206208
-1087.220284	-2.437923	4.216205
-1085.507183	-4.576205	4.226202
-1083.481380	-5.051777	4.236198
-1081.494413	-8.783545	4.246195
-1079.714465	-4.726902	4.256192
-1077.894308	-1.018229	4.266189
-1075.898818	-7.365783	4.276186
-1074.119631	-4.613600	4.286182
-1072.286544	-10.522246	4.296179
-1070.547238	-11.658022	4.306176
-1068.405398	-14.623977	4.316173
-1066.668562	-6.857191	4.326170
-1064.762677	-7.575770	4.336166
-1062.325262	-8.274558	4.346163
-1060.941120	-8.444710	4.356160
-1059.071008	-8.083749	4.366157
-1057.378383	-1.700509	4.376154
-1055.779118	-9.044722	4.386150
-1053.054748	0.276821	4.396147
-1051.308737	0.445284	4.406144
-1049.971986	-3.313943	4.416141
-1048.134299	-2.081896	4.426138
-1045.857990	-4.680856	4.436134
-1044.080926	-17.024980	4.446131
-1042.320957	-7.261595	4.456128
-1040.213331	-5.642741	4.466125
-1038.509264	-11.838276	4.476122
-1036.631722	-3.862459	4.486118
-1034.412374	-7.890598	4.496115
-1033.084690	-5.992389	4.506112
-1030.937557	-9.227189	4.516109
-1029.033101	-8.748411	4.526106
-1027.298002	-7.597149	4.536102
-1025.431794	-8.711618	4.546099
-1023.513518	-9.948452	4.556096
-1021.395655	-6.261228	4.566093
-1019.935674	-7.014282	4.576090
-1017.741261	-6.073878	4.586086
-1015.757580	-6.496341	4.596083
-1014.031476	-2.344267	4.606080
-1012.104224	-5.184431	4.616077
-1010.486236	-3.891724	4.626074
-1008.623348	-8.931255	4.636070
-1006.020950	-3.622664	4.646067
-1004.349930	-8.627670	4.656064
-1003.118922	-11.317070	4.666061
-1001.040406	-5.639116	4.676058
-998.921533	-4.317395	4.686054
-997.104086	-1.523925	4.696051
-995.505765	-2.090470	4.706048
-993.818081	-6.676248	4.716045
-991.221786	-7.389628	4.726042
-989.552976	-8.501018	4.736038
-988.026150	-0.108083	4.746035
-985.700367	-5.628218	4.756032
-984.323967	-5.844836	4.766029
-981.885357	2.057609	4.776026
-980.016668	-2.673853	4.786022
-978.686078	-5.470847	4.796019
-976.707870	-1.350576	4.806016
-974.695388	-4.167417	4.816013
-972.579319	-11.477024	4.826010
-971.076147	-7.183904	4.836006
-969.001843	-2.482567	4.846003
-967.145477	-8.411770	4.856000
-965.226215	-10.434034	4.865997
-963.407504	-4.209537	4.875994
-961.362980	-5.261717	4.885990
-959.568542	-3.013625	4.895987
-957.971617	-5.697858	4.905984
-955.922699	-5.971828	4.915981
-953.806819	-8.486288	4.925978
-952.106457	-6.124820	4.935974
-950.433050	-9.135583	4.945971
-948.281006	-5.425732	4.955968
-946.569230	-7.834059	4.965965
-944.800367	-7.094046	4.975962
-942.908793	-5.681107	4.985958
-940.693440	-1.428032	4.995955
-938.871803	-6.880171	5.005952
-937.192741	-4.224954	5.015949
-935.168850	-4.779960	5.025946
-933.185378	-6.888720	5.035942
-931.609617	-4.869842	5.045939
-929.737724	-7.216333	5.055936
-927.538980	-4.960964	5.065933
-925.893438	-10.030337	5.075930
-923.838060	-8.008428	5.085926
-922.107467	-7.285153	5.095923
-920.225335	-3.931277	5.105920
-918.450201	-0.143662	5.115917
-916.336558	-3.965874	5.125914
-914.681013	0.538242	5.135910
-912.906697	-7.424057	5.145907
-910.966474	-2.611144	5.155904
-908.911358	-2.144342	5.165901
-906.893159	-8.862879	5.175898
-905.261606	-4.548691	5.185894
-903.586995	0.902246	5.195891
-901.536048	-7.804691	5.205888
-899.477817	-5.817643	5.215885
-897.455619	-3.747341	5.225882
-895.726443	-1.415298	5.235878
-894.073396	-9.084075	5.245875
-892.239792	-6.050671	5.255872
-890.154366	-8.406137	5.265869
-888.226855	-9.768989	5.275866
-886.811456	-9.782018	5.285862
-884.396508	-4.360544	5.295859
-882.709252	-1.477487	5.305856
-880.802278	-11.154845	5.315853
-878.810622	-9.683176	5.325850
-877.224243	-2.227188	5.335846
-875.273037	-4.807800	5.345843
-873.162123	-10.040826	5.355840
-871.310150	-9.921305	5.365837
-869.491412	-6.635170	5.375834
-867.851404	-0.215540	5.385830
-865.785837	-6.794383	5.395827
-864.148400	-3.760885	5.405824
-861.905075	-8.701652	5.415821
-860.122672	-11.471438	5.425818
-858.468833	-5.125713	5.435814
-856.658329	-6.061398	5.445811
-854.367877	-5.353180	5.455808
-852.513263	-8.277635	5.465805
-850.988934	-1.198687	5.475802
-848.836534	-3.724901	5.485798
-847.053206	-4.810840	5.495795
-845.164643	-10.864879	5.505792
-843.239237	-11.118385	5.515789
-841.334063	-14.192999	5.525786
-839.826562	-10.180775	5.535782
-837.797081	-10.383376	5.545779
-835.681785	-7.812878	5.555776
-833.694540	-12.558308	5.565773
-831.907618	-7.673593	5.575770
-830.232534	-9.472484	5.585766
-828.520240	-9.540803	5.595763
-826.538509	-10.271110	5.605760
-824.319102	-6.288597	5.615757
-822.584257	-6.284903	5.625754
-820.846710	-10.984307	5.635750
-819.029859	-7.191557	5.645747
-816.880068	-8.329716	5.655744
-814.864878	-13.264499	5.665741
-813.529888	-8.590709	5.675738
-811.670205	-15.952673	5.685734
-809.544425	-11.846584	5.695731
-807.699416	-10.951224	5.705728
-805.455184	-4.623422	5.715725
-804.070230	-7.549844	5.725722
-801.886764	-8.027842	5.735718
-800.143491	-11.180568	5.745715
-798.186948	-7.068742	5.755712
-796.485933	-8.380822	5.765709
-794.415308	-7.875525	5.775706
-792.509289	-10.424237	5.785702
-790.608597	-7.741395	5.795699
-788.825695	-15.535577	5.805696
-787.257885	-13.434261	5.815693
-785.328968	-15.757281	5.825690
-783.264114	-8.530793	5.835686
-781.226596	-7.414341	5.845683
-779.329755	-11.151458	5.855680
-777.742164	-9.196206	5.865677
-775.892287	-3.650012	5.875674
-774.022943	-6.816859	5.885670
-771.893219	-1.890172	5.895667
-770.024150	-3.295507	5.905664
-768.174483	-4.642971	5.915661
-766.301546	-6.098764	5.925658
-764.526844	-4.267705	5.935654
-762.400760	-4.177004	5.945651
-760.866332	-10.823912	5.955648
-758.919999	-0.119347	5.965645
-756.998643	-3.899395	5.975642
-755.285472	-5.751036	5.985638
-753.212001	1.117908	5.995635
-751.180501	-0.223608	6.005632
-749.349174	0.990297	6.015629
-747.778448	-9.064437	6.025626
-745.934391	-0.262255	6.035622
-743.805104	0.763375	6.045619
-741.702095	-1.143708	6.055616
-739.957170	-7.761924	6.065613
-738.443479	-6.304587	6.075610
-736.346733	2.337645	6.085606
-734.292657	-0.006837	6.095603
-732.673675	4.852212	6.105600
-730.890016	-1.873430	6.115597
-728.922915	-7.414088	6.125594
-726.919436	-3.533180	6.135590
-724.982227	-2.352455	6.145587
-723.104083	-5.215292	6.155584
-721.230499	-8.161131	6.165581
-719.420318	-6.665354	6.175578
-717.695037	-4.883099	6.185574
-715.899587	-4.962088	6.195571
-713.680998	-4.209053	6.205568
-711.778743	-2.851591	6.215565
-709.957778	-3.167341	6.225562
-708.218178	0.381435	6.235558
-706.344840	-1.620192	6.245555
-704.569417	-1.510384	6.255552
-702.675286	-3.974420	6.265549
-700.326940	-7.285492	6.275546
-698.894475	-9.012266	6.285542
-697.129951	1.023615	6.295539
-695.147684	-0.384912	6.305536
-693.096775	-3.231938	6.315533
-691.470475	-3.104437	6.325530
-689.356291	-4.974287	6.335526
-687.323664	-5.246915	6.345523
-685.797630	-0.687672	6.355520
-683.679846	-1.193860	6.365517
-681.880950	-8.175431	6.375514
-680.434355	-3.282035	6.385510
-678.419983	-3.522676	6.395507
-676.329199	-3.228663	6.405504
-674.184167	-12.574515	6.415501
-672.189897	-7.799610	6.425498
-670.601388	-1.855584	6.435494
-668.776758	-6.086139	6.445491
-666.825829	-5.185182	6.455488
-664.908938	-8.901982	6.465485
-663.206153	-9.239325	6.475482
-661.072547	-7.090409	6.485478
-659.264787	-4.131901	6.495475
-657.562534	-12.202684	6.505472
-655.487010	-9.796790	6.515469
-653.813731	-2.661114	6.525466
-652.300364	-10.072673	6.535462
-650.481004	-4.420007	6.545459
-648.037535	-1.864625	6.555456
-646.161711	-2.779027	6.565453
-644.294268	-6.616173	6.575450
-642.674121	1.315892	6.585446
-640.361629	-3.586846	6.595443
-638.820556	-7.423708	6.605440
-637.210611	-6.317203	6.615437
-635.009156	4.083999	6.625434
-632.990516	-3.392528	6.635430
-631.343976	2.741140	6.645427
-629.193107	2.356164	6.655424
-627.179675	-1.277201	6.665421
-626.056081	-3.142628	6.675418
-624.001180	-4.364399	6.685414
-621.965242	-3.339289	6.695411
-619.645307	-10.139528	6.705408
-617.599123	-8.901968	6.715405
-616.426100	-7.271912	6.725402
-614.640498	-10.592685	6.735398
-612.521299	-6.447421	6.745395
-610.865717	-5.081177	6.755392
-608.803278	-5.619330	6.765389
-606.496730	-8.159235	6.775386
-604.814591	-10.829910	6.785382
-603.302266	-10.241759	6.795379
-601.552211	-8.387827	6.805376
-599.540698	-0.941036	6.815373
-597.591660	-5.221368	6.825370
-595.658279	-3.641156	6.835366
-593.579672	-2.825308	6.845363
-591.654491	-10.802323	6.855360
-589.754847	-4.664250	6.865357
-588.279104	-4.053613	6.875354
-586.027921	-9.851634	6.885350
-584.576583	-9.610285	6.895347
-582.549222	-4.771454	6.905344
-580.378728	-9.972290	6.915341
-578.612734	-10.172242	6.925338
-576.893732	-2.748361	6.935334
-574.876940	-3.491291	6.945331
-573.205185	-5.290703	6.955328
-571.447103	-2.657587	6.965325
-569.393233	-8.337958	6.975322
-567.302267	-0.822183	6.985318
-565.631985	1.002771	6.995315
-563.795520	-1.850481	7.005312
-561.751331	-4.228363	7.015309
-559.717248	-5.321250	7.025306
-558.227766	-2.751514	7.035302
-556.308099	0.795282	7.045299
-554.169326	-6.657958	7.055296
-552.088904	-10.690094	7.065293
-551.044019	-4.744034	7.075290
-548.780864	-2.352496	7.085286
-546.739446	-3.452169	7.095283
-545.137484	-4.895364	7.105280
-542.917379	-7.169445	7.115277
-541.190078	-5.050741	7.125274
-539.293392	-2.835817	7.135270
-537.565135	2.046852	7.145267
-535.509230	-0.335795	7.155264
-533.456604	-1.548836	7.165261
-531.809396	-10.611609	7.175258
-529.936974	-5.041105	7.185254
-528.205370	-8.921690	7.195251
-526.028922	-8.333247	7.205248
-524.093900	-10.548522	7.215245
-522.516742	-9.574278	7.225242
-520.547065	-5.085953	7.235238
-519.179469	-5.318698	7.245235
-516.877163	-7.241692	7.255232
-514.824083	-11.675004	7.265229
-512.910684	-10.031650	7.275226
-511.126514	-3.442150	7.285222
-509.215479	-0.391030	7.295219
-507.354753	-10.612049	7.305216
-505.557873	-11.999354	7.315213
-503.678080	-11.398337	7.325210
-501.901168	-10.613282	7.335206
-499.903568	-8.733802	7.345203
-497.955222	-10.857687	7.355200
-496.216869	-18.069489	7.365197
-494.436514	-17.905112	7.375194
-492.140901	-10.773386	7.385190
-490.742958	-4.510849	7.395187
-488.844800	-1.745226	7.405184
-486.548896	-1.015220	7.415181
-484.649411	-4.024692	7.425178
-483.227961	-2.904363	7.435174
-481.375536	-3.631697	7.445171
-479.061741	-7.469084	7.455168
-477.371535	-10.838255	7.465165
-475.391916	-14.215582	7.475162
-473.459454	-6.235061	7.485158
-471.931369	-7.267180	7.495155
-469.785699	-7.558313	7.505152
-467.919263	-7.542671	7.515149
-465.978984	-6.158819	7.525146
-464.355934	-5.767068	7.535142
-462.676775	-9.127225	7.545139
-460.872126	-8.770976	7.555136
-458.396123	-4.630724	7.565133
-456.823380	-6.590559	7.575130
-454.722375	-5.446902	7.585126
-452.880399	0.215022	7.595123
-451.012581	-2.541205	7.605120
-449.254938	0.453265	7.615117
-447.218001	-5.783776	7.625114
-445.703692	-10.213550	7.635110
-443.568836	-7.049828	7.645107
-441.738958	-1.106407	7.655104
-439.860026	2.197263	7.665101
-437.928234	-5.462293	7.675098
-436.259020	3.444348	7.685094
-434.287354	6.768867	7.695091
-432.526798	2.094893	7.705088
-430.482738	4.243877	7.715085
-428.513237	1.672959	7.725082
-426.729961	1.055128	7.735078
-424.684497	-3.936071	7.745075
-422.808455	1.153681	7.755072
-420.945648	-4.382402	7.765069
-419.206698	-4.583579	7.775066
-417.489335	-2.122839	7.785062
-415.528746	-5.359343	7.795059
-413.643955	-1.851946	7.805056
-411.564151	-4.564296	7.815053
-409.946847	-9.072592	7.825050
-407.901020	-5.667120	7.835046
-406.156281	-4.517256	7.845043
-404.260711	-1.827821	7.855040
-402.419691	-2.201030	7.865037
-400.417633	-7.532956	7.875034
-398.216755	-0.185333	7.885030
-396.978471	-0.727047	7.895027
-394.778167	-1.722303	7.905024
-392.832376	-2.936713	7.915021
-391.071536	-10.589056	7.925018
-388.811766	-6.533789	7.935014
-387.503471	-0.734436	7.945011
-385.615805	-1.749960	7.955008
-383.609873	0.790131	7.965005
-381.925561	-2.442834	7.975002
-379.650684	5.468331	7.984998
-377.743180	3.646330	7.994995
-376.143288	-0.230184	8.004992
-374.248316	0.194786	8.014989
-372.275795	-3.720751	8.024986
-370.510200	0.947704	8.034982
-368.459335	1.921763	8.044979
-366.744566	-0.826356	8.054976
-364.792853	-4.765195	8.064973
-362.782351	-4.296408	8.074970
-361.139819	-0.878640	8.084966
-359.215974	-0.260613	8.094963
-357.059766	-1.229711	8.104960
-355.599383	-6.263187	8.114957
-353.619314	-4.964363	8.124954
-351.601804	-2.749924	8.134950
-349.740980	-7.938643	8.144947
-347.695369	-1.824302	8.154944
-345.935105	-4.373519	8.164941
-344.158406	-11.312438	8.174938
-342.312397	-14.414644	8.184934
-340.806555	-12.917483	8.194931
-338.682059	-3.892872	8.204928
-336.634573	-6.978260	8.214925
-334.565283	-14.253500	8.224922
-332.772658	-10.734605	8.234918
-331.180941	-8.145965	8.244915
-329.075008	-8.421913	8.254912
-327.509561	-7.911151	8.264909
-325.500384	-5.564060	8.274906
-323.604742	-6.736245	8.284902
-321.673028	-4.271132	8.294899
-319.863120	-6.563271	8.304896
-317.879602	-5.857449	8.314893
-315.690162	-7.884685	8.324890
-314.298256	-3.062788	8.334886
-312.134753	-2.535646	8.344883
-310.253412	-6.464369	8.354880
-308.667260	-3.446746	8.364877
-306.681182	-6.580475	8.374874
-304.663149	-5.914161	8.384870
-303.091928	-12.049523	8.394867
-301.103441	-4.808482	8.404864
-298.866601	-5.491416	8.414861
-297.348291	-9.014420	8.424858
-295.473750	-9.435228	8.434854
-293.565669	-14.219426	8.444851
-291.386858	-9.753029	8.454848
-289.636543	-5.469624	8.464845
-288.106423	-5.149606	8.474842
-285.856959	-0.687812	8.484838
-284.155061	0.198728	8.494835
-281.894365	-2.033185	8.504832
-280.603807	-9.410382	8.514829
-278.523475	-7.410615	8.524826
-276.597210	-10.321447	8.534822
-274.346335	-9.688338	8.544819
-272.952798	-6.663353	8.554816
-271.227998	-3.138329	8.564813
-269.155326	-3.127942	8.574810
-267.243310	-6.222472	8.584807
-265.554596	-5.251064	8.594803
-263.533933	-4.628655	8.604800
-261.268996	-6.626132	8.614797
-259.626380	-3.927234	8.624794
-258.054121	-4.922594	8.634791
-255.909554	3.123235	8.644787
-253.870413	-9.344676	8.654784
-252.262025	-11.040229	8.664781
-250.516180	-8.018754	8.674778
-248.198334	-8.577626	8.684775
-246.482076	-1.336894	8.694771
-245.027451	0.747288	8.704768
-243.024040	0.017472	8.714765
-240.694038	1.692252	8.724762
-238.978107	-2.146420	8.734759
-237.214311	0.464121	8.744755
-235.559760	-2.078782	8.754752
-233.560772	-2.984891	8.764749
-231.821853	-9.997128	8.774746
-229.581377	-10.647453	8.784743
-227.917686	-6.748332	8.794739
-226.003813	-10.515030	8.804736
-224.056155	-7.947085	8.814733
-222.059322	-7.785738	8.824730
-220.170230	-10.739178	8.834727
-218.168613	-11.352482	8.844723
-216.359417	-7.376742	8.854720
-214.577966	-16.106362	8.864717
-212.930453	-12.778709	8.874714
-211.127442	-17.604137	8.884711
-209.079566	-19.916891	8.894707
-207.225897	-11.425935	8.904704
-205.225373	-15.437896	8.914701
-203.293810	-12.788138	8.924698
-201.428596	-7.119808	8.934695
-199.935030	-16.525268	8.944691
-197.856409	-12.041243	8.954688
-196.009896	-16.387222	8.964685
-193.950363	-13.022727	8.974682
-192.030629	-12.599950	8.984679
-190.630925	-12.932953	8.994675
-188.385646	-14.114460	9.004672
-186.674354	-16.694741	9.014669
-184.479830	-20.986973	9.024666
-183.052914	-21.289863	9.034663
-180.871897	-9.851795	9.044659
-178.914205	-9.050582	9.054656
-177.234585	-9.795976	9.064653
-175.223419	-10.977242	9.074650
-173.387887	-8.568682	9.084647
-171.592426	-9.654461	9.094643
-169.707862	-12.111899	9.104640
-167.725806	-15.031860	9.114637
-165.651608	-19.111374	9.124634
-163.981199	-15.955200	9.134631
-162.514324	-9.096915	9.144627
-160.522117	-12.690875	9.154624
-158.394257	-12.394676	9.164621
-156.398724	-8.459561	9.174618
-154.349185	-10.536239	9.184615
-152.988159	-8.834747	9.194611
-150.942475	-7.091795	9.204608
-149.038294	-9.127734	9.214605
-146.927159	-9.229409	9.224602
-145.193844	-12.186141	9.234599
-143.497013	-7.423195	9.244595
-141.708933	-2.779047	9.254592
-139.699946	-3.712124	9.264589
-137.142093	-9.773979	9.274586
-135.750446	-10.677461	9.284583
-134.394204	-11.757460	9.294579
-132.337796	-8.941748	9.304576
-130.522372	-5.492674	9.314573
-128.422388	-10.945228	9.324570
-126.503900	-12.006243	9.334567
-124.607191	-9.359562	9.344563
-122.559731	-9.312376	9.354560
-120.797854	-5.977423	9.364557
-119.118319	-4.447130	9.374554
-117.300691	-3.322691	9.384551
-115.142098	-3.907144	9.394547
-113.506156	-2.105764	9.404544
-111.564097	-4.173477	9.414541
-109.613689	-4.433324	9.424538
-107.676754	1.008548	9.434535
-106.017238	-1.549390	9.444531
-104.145923	-3.512884	9.454528
-102.198462	-0.944848	9.464525
-100.017729	-0.810240	9.474522
-98.643683	-4.078036	9.484519
-96.720258	-2.659511	9.494515
-94.531540	-5.863869	9.504512
-92.343871	-5.033682	9.514509
-90.913900	-11.205230	9.524506
-88.850588	-4.274903	9.534503
-87.123147	-3.693822	9.544499
-85.156120	-4.351723	9.554496
-83.338342	-4.191228	9.564493
-81.412473	-6.054988	9.574490
-80.017273	-3.322286	9.584487
-77.866564	-1.668843	9.594483
-75.838457	-2.228135	9.604480
-73.548535	-10.905398	9.614477
-72.083866	-8.022568	9.624474
-70.276670	-0.596184	9.634471
-68.474615	-0.258300	9.644467
-66.759886	4.187417	9.654464
-64.619358	-1.564133	9.664461
-62.658986	0.717153	9.674458
-60.809015	-0.732045	9.684455
-58.823636	-2.130161	9.694451
-57.059703	2.931168	9.704448
-55.534767	-1.288482	9.714445
-52.900027	-0.754283	9.724442
-51.596938	1.302201	9.734439
-49.824051	5.894458	9.744435
-47.704845	9.522683	9.754432
-46.048830	5.130769	9.764429
-43.854718	-0.298373	9.774426
-41.986793	5.502761	9.784423
-40.179873	-4.606928	9.794419
-38.385129	-2.012281	9.804416
-36.553704	-5.265612	9.814413
-34.466403	-7.557388	9.824410
-32.667754	-4.214869	9.834407
-30.589874	-4.346753	9.844403
-29.078897	-3.895709	9.854400
-27.144862	-4.062603	9.864397
-25.305460	-6.395654	9.874394
-23.369332	-11.113028	9.884391
-21.385990	-7.807707	9.894387
-19.464919	-1.190071	9.904384
-17.616090	-7.900964	9.914381
-16.097129	-6.865969	9.924378
-14.003669	2.089062	9.934375
-11.755925	-0.444819	9.944371
-10.177005	-2.149466	9.954368
-8.233288	-2.073374	9.964365
-6.456105	3.422816	9.974362
-4.951066	9.825662	9.984359
-4.003535	44.767487	9.994355
-2.493473	94.585001	10.004352
-1.206327	159.862786	10.014349
0.000000	216.871521	10.019354
0.656898	260.154433	10.024359
1.229815	299.202720	10.029363
1.925100	332.696552	10.034368
1.742738	358.852704	10.039373
2.730993	374.783068	10.044378
2.726786	401.984754	10.049383
3.093475	421.670940	10.054387
3.040251	433.293930	10.059392
2.830693	447.803891	10.064397
3.183682	450.292842	10.069402
3.450188	469.787459	10.074407
3.386034	476.671339	10.079411
3.685494	489.318597	10.084416
3.641562	487.822593	10.089421
4.003001	487.120738	10.094426
3.797822	504.442404	10.099431
4.172733	512.156908	10.104435
4.211015	522.225640	10.109440
4.063848	526.280972	10.114445
4.467386	525.855704	10.119450
4.209872	536.950132	10.124455
4.379029	533.542646	10.129459
4.230516	538.676600	10.134464
4.266853	542.243776	10.139469
4.703246	530.956764	10.144474
4.600993	548.158203	10.149479
4.304882	546.143345	10.154483
4.713594	552.293305	10.159488
4.669031	553.515084	10.164493
4.667551	549.358849	10.169498
4.724859	555.263940	10.174503
4.174698	551.720057	10.179507
4.933651	549.787181	10.184512
4.621707	559.107985	10.189517
4.842404	574.023487	10.194522
5.163250	586.462689	10.199527
5.070968	589.517471	10.204531
5.351928	581.192651	10.209536
5.139356	584.729097	10.214541
5.054713	578.451647	10.219546
5.352107	585.905934	10.224551
5.233356	594.151953	10.229555
5.445005	594.108917	10.234560
4.910735	602.038565	10.239565
5.540682	598.263117	10.244570
5.434828	603.943973	10.249575
5.174176	609.219542	10.254579
5.280741	618.489939	10.259584
4.877366	612.111604	10.264589
5.217563	615.251706	10.269594
4.954324	607.951342	10.274599
5.803487	637.024957	10.279603
5.994447	646.068536	10.284608
5.672431	653.670902	10.289613
5.992814	648.557106	10.294618
5.973365	646.641636	10.299623
5.737233	653.040752	10.304627
6.117908	648.985145	10.309632
6.034482	659.763239	10.314637
5.892530	655.273833	10.319642
5.953832	660.574346	10.324647
5.777454	664.043816	10.329651
5.962770	661.939290	10.334656
5.777366	672.518567	10.339661
6.145632	657.476258	10.344666
6.002816	668.390064	10.349671
6.059407	672.500100	10.354675
6.140876	673.830934	10.359680
6.204140	697.619011	10.364685
6.494003	702.714168	10.369690
6.459170	707.290275	10.374695
6.546513	711.093082	10.379699
6.602268	703.657847	10.384704
6.613184	709.547268	10.389709
6.896024	712.790775	10.394714
6.657213	712.997868	10.399719
6.594162	710.521456	10.404723
6.992625	714.270128	10.409728
6.810921	722.764636	10.414733
7.232121	714.167810	10.419738
6.897324	719.989803	10.424743
6.848995	721.472762	10.429747
6.867154	722.634065	10.434752
6.618317	727.301344	10.439757
7.041780	717.517177	10.444762
7.001585	722.049603	10.449767
6.782657	718.876773	10.454771
7.254087	721.299278	10.459776
7.402144	732.087466	10.464781
7.549283	735.619505	10.469786
7.279729	748.772688	10.474791
7.333922	749.630583	10.479795
7.778730	750.750311	10.484800
7.657623	751.031563	10.489805
7.780514	751.263083	10.494810
7.704061	746.349138	10.499815
7.781540	733.385921	10.504819
7.704519	736.379695	10.509824
7.679392	738.261301	10.514829
7.721273	735.191378	10.519834
8.094690	748.866279	10.524839
7.966960	743.166535	10.529843
7.755633	738.565055	10.534848
7.393209	748.288172	10.539853
7.547109	754.389142	10.544858
7.983999	761.259473	10.549863
7.851688	756.896277	10.554867
7.845090	763.856861	10.559872
7.605093	764.257575	10.564877
7.789316	776.945747	10.569882
8.086258	787.173980	10.574887
7.886654	795.560677	10.579891
8.172163	788.837970	10.584896
8.006479	799.965391	10.589901
8.080539	790.261220	10.594906
8.011145	802.518431	10.599911
8.273315	818.025073	10.604915
8.674064	826.485294	10.609920
8.342493	833.822941	10.614925
8.809352	828.762523	10.619930
8.413737	830.955163	10.624935
8.646146	833.096567	10.629939
9.124958	829.468162	10.634944
8.825911	838.775473	10.639949
8.905468	834.676319	10.644954
8.906554	842.967447	10.649959
8.786988	844.916180	10.654963
9.004151	833.324309	10.659968
8.715622	843.992830	10.664973
8.927083	845.522440	10.669978
8.807321	839.280906	10.674983
8.817238	843.801618	10.679987
9.229889	859.696179	10.684992
9.139360	873.705341	10.689997
9.437362	874.163021	10.695002
9.306098	878.941632	10.700007
9.324856	881.118491	10.705011
9.438732	873.549659	10.710016
9.785767	883.319766	10.715021
9.785175	882.301025	10.720026
9.568125	879.960332	10.725031
9.635124	879.835916	10.730035
9.788215	878.036095	10.735040
9.685216	879.546995	10.740045
9.623933	878.072086	10.745050
9.708359	882.773848	10.750055
9.578988	891.089738	10.755059
9.837389	887.166745	10.760064
9.774321	886.474109	10.765069
9.938770	885.403780	10.770074
9.879379	884.425516	10.775079
9.934980	881.228870	10.780083
9.947923	884.048564	10.785088
9.820690	892.808163	10.790093
10.240591	900.925275	10.795098
10.165932	923.881957	10.800103
10.248682	920.390913	10.805107
10.111844	915.836213	10.810112
10.116314	938.219220	10.815117
10.225286	920.304424	10.820122
10.171595	925.423824	10.825127
10.383470	928.412310	10.830131
10.323817	925.589889	10.835136
10.236155	929.488676	10.840141
10.129135	930.204486	10.845146
10.826979	941.463418	10.850151
10.686457	948.095338	10.855155
10.953568	957.563407	10.860160
10.814340	953.426341	10.865165
11.011636	949.196049	10.870170
10.997828	959.393204	10.875175
10.780006	968.149826	10.880179
11.113092	960.780206	10.885184
10.945582	962.656648	10.890189
11.180599	966.618933	10.895194
11.220941	967.804081	10.900199
11.071885	966.384872	10.905203
11.070238	968.727084	10.910208
10.864382	975.209165	10.915213
11.262676	970.262301	10.920218
11.615983	972.937994	10.925223
11.372126	967.806367	10.930227
11.232181	965.716519	10.935232
11.117770	974.426597	10.940237
11.341371	969.260213	10.945242
11.339869	979.230667	10.950247
11.382362	975.394804	10.955251
11.379186	989.182250	10.960256
12.024886	1005.620422	10.965261
11.813858	994.311060	10.970266
11.623452	988.435263	10.975271
11.779228	998.745867	10.980275
11.973925	997.975081	10.985280
11.926556	999.281455	10.990285
11.824687	996.516785	10.995290
11.650316	1002.220191	11.000295
12.087067	1003.713163	11.005299
12.226121	999.801132	11.010304
11.826224	1019.679120	11.015309
11.788711	1010.537890	11.020314
11.933635	1005.739852	11.025319
11.891728	1013.344890	11.030323
12.120189	1014.911076	11.035328
12.062778	1034.154438	11.040333
12.318386	1040.715713	11.045338
12.655085	1040.689526	11.050343
12.528345	1033.324505	11.055347
12.962372	1028.857417	11.060352
12.804502	1035.024980	11.065357
12.753854	1015.512705	11.070362
12.854356	1009.792678	11.075367
13.109977	996.955409	11.080371
13.076744	999.105673	11.085376
13.001668	1001.231139	11.090381
13.141446	1002.469109	11.095386
13.199789	1014.020111	11.100391
12.679012	1007.393716	11.105395
12.999109	1011.061556	11.110400
12.592668	1008.178186	11.115405
12.873404	1007.099358	11.120410
12.873384	998.968153	11.125415
13.000812	1007.547178	11.130419
13.058389	1001.197805	11.135424
13.159591	1019.882638	11.140429
13.120705	1029.798350	11.145434
13.338823	1035.666183	11.150439
13.239795	1047.813404	11.155443
13.482232	1037.655866	11.160448
13.656030	1048.533019	11.165453
13.503520	1041.130965	11.170458
13.645608	1046.718548	11.175463
13.300366	1044.643757	11.180467
13.985986	1048.015644	11.185472
13.394313	1047.421530	11.190477
13.868443	1046.101513	11.195482
14.128098	1048.776303	11.200487
13.497016	1048.951184	11.205491
13.906705	1049.330114	11.210496
13.481783	1052.344915	11.215501
13.771656	1048.153197	11.220506
14.045085	1048.217595	11.225511
14.014062	1042.534318	11.230515
13.920210	1041.394189	11.235520
13.964274	1047.192001	11.240525
13.857102	1045.572181	11.245530
13.794669	1056.569186	11.250535
13.896096	1058.258605	11.255539
14.467744	1066.307154	11.260544
14.468866	1073.101946	11.265549
14.811471	1067.016702	11.270554
14.628623	1055.128515	11.275559
14.616669	1044.578801	11.280563
14.700656	1036.493961	11.285568
14.394061	1045.851637	11.290573
14.335072	1043.941713	11.295578
14.616477	1045.537509	11.300583
15.021546	1061.730420	11.305587
14.819169	1047.077687	11.310592
14.673720	1046.435878	11.315597
14.701531	1044.505545	11.320602
14.641410	1052.958858	11.325607
14.760424	1065.480814	11.330611
14.760715	1071.932326	11.335616
14.395005	1069.474593	11.340621
14.768017	1064.566771	11.345626
14.810882	1069.618743	11.350631
14.522554	1077.564880	11.355635
14.955149	1082.803059	11.360640
14.904930	1103.322647	11.365645
15.326094	1093.848511	11.370650
15.328717	1101.413983	11.375655
15.349692	1102.474172	11.380659
15.542832	1105.349457	11.385664
15.457854	1109.341381	11.390669
15.533706	1103.973312	11.395674
15.500994	1106.616136	11.400679
15.680892	1103.768793	11.405683
15.899514	1099.107302	11.410688
15.896998	1100.363756	11.415693
15.454804	1100.869015	11.420698
15.517606	1098.776754	11.425703
15.579610	1099.497144	11.430707
16.035042	1100.729947	11.435712
15.673220	1104.868813	11.440717
16.037912	1102.160707	11.445722
16.260706	1100.949308	11.450727
15.795151	1104.655167	11.455731
16.108369	1098.093763	11.460736
15.962581	1113.178015	11.465741
16.212063	1099.238024	11.470746
16.214146	1094.648004	11.475751
16.009402	1109.526833	11.480755
16.302184	1105.419075	11.485760
15.934548	1108.596960	11.490765
15.957502	1100.732553	11.495770
16.281458	1106.571608	11.500775
16.004840	1102.217268	11.505779
16.492230	1117.015326	11.510784
16.353761	1133.343349	11.515789
16.935330	1122.688658	11.520794
17.247150	1127.057424	11.525799
16.916795	1110.424060	11.530803
17.015023	1097.420668	11.535808
16.591381	1103.448695	11.540813
16.589873	1092.446365	11.545818
16.688902	1095.367784	11.550823
16.872025	1089.398298	11.555827
16.838776	1097.978871	11.560832
16.702607	1102.171808	11.565837
16.684579	1116.199546	11.570842
16.943433	1127.943229	11.575847
17.268385	1131.315395	11.580851
17.625477	1122.348810	11.585856
17.590712	1120.892226	11.590861
17.388798	1099.768798	11.595866
17.515228	1101.216303	11.600871
17.354918	1101.622703	11.605875
17.666018	1097.313648	11.610880
17.429522	1102.638925	11.615885
17.492797	1093.425496	11.620890
17.217303	1094.573228	11.625895
17.288179	1093.222876	11.630899
17.377636	1089.025642	11.635904
17.164311	1121.068404	11.640909
17.119330	1120.676210	11.645914
17.444655	1124.283575	11.650919
17.257074	1130.935089	11.655923
17.391402	1128.904376	11.660928
17.439607	1143.645130	11.665933
17.784827	1154.427832	11.670938
17.896056	1159.367452	11.675943
18.039401	1162.735632	11.680947
18.569067	1157.374602	11.685952
18.039328	1161.898329	11.690957
17.918383	1158.720055	11.695962
17.949167	1161.095420	11.700967
18.185532	1158.866023	11.705971
18.779716	1159.700038	11.710976
18.345235	1162.443732	11.715981
18.627634	1167.666640	11.720986
18.716467	1143.434063	11.725991
18.565877	1138.242572	11.730995
18.613236	1135.045709	11.736000
18.616716	1131.541367	11.741005
18.369032	1131.232876	11.746010
18.652020	1128.997463	11.751015
18.621451	1127.911214	11.756019
18.561064	1128.437851	11.761024
18.424877	1132.976592	11.766029
18.947288	1147.738675	11.771034
18.832292	1147.396775	11.776039
18.953053	1150.708429	11.781043
18.900640	1137.070827	11.786048
18.708212	1145.298190	11.791053
18.907966	1158.658620	11.796058
18.941519	1157.640718	11.801063
18.915387	1166.168396	11.806067
19.253150	1165.030833	11.811072
18.915097	1171.905929	11.816077
18.884774	1162.759034	11.821082
18.830374	1161.421472	11.826087
18.774187	1173.203416	11.831091
19.318347	1160.460620	11.836096
18.729684	1170.812926	11.841101
18.906929	1184.802902	11.846106
19.512296	1193.203372	11.851111
19.294274	1190.554110	11.856115
19.484321	1187.231718	11.861120
19.439574	1187.285539	11.866125
19.349018	1187.713140	11.871130
19.527268	1192.814175	11.876135
19.392830	1198.386857	11.881139
19.893926	1191.312012	11.886144
19.815603	1192.104624	11.891149
19.667208	1195.277303	11.896154
19.720904	1208.746505	11.901159
19.811658	1223.088455	11.906163
20.033754	1219.098578	11.911168
20.236605	1216.877682	11.916173
20.826891	1214.819307	11.921178
20.384114	1205.297838	11.926183
19.861831	1196.274354	11.931187
20.116240	1191.374987	11.936192
19.974991	1202.621269	11.941197
20.342183	1217.281740	11.946202
20.089185	1221.656586	11.951207
19.897071	1223.798990	11.956211
20.114666	1218.460263	11.961216
20.081106	1229.433491	11.966221
20.277005	1223.330709	11.971226
20.258508	1221.572112	11.976231
20.115975	1233.481013	11.981235
20.563564	1245.495191	11.986240
20.662495	1243.763827	11.991245
20.672491	1246.884885	11.996250
20.840465	1252.822583	12.001255
20.710166	1259.168272	12.006259
21.035206	1253.928743	12.011264
20.797577	1265.768314	12.016269
21.120718	1257.801042	12.021274
21.271573	1252.196243	12.026279
21.315051	1269.296118	12.031283
21.312611	1244.649553	12.036288
20.713357	1240.285360	12.041293
20.998018	1230.236118	12.046298
20.985459	1227.968864	12.051303
21.057644	1227.199336	12.056307
21.263249	1218.726440	12.061312
20.720097	1224.500658	12.066317
21.030597	1221.749718	12.071322
20.756060	1229.447248	12.076327
20.245357	1225.460645	12.081331
20.933863	1245.646125	12.086336
20.840359	1258.228753	12.091341
20.767023	1259.152752	12.096346
20.925395	1260.900326	12.101351
20.958947	1266.129224	12.106355
21.032480	1258.192512	12.111360
20.627553	1256.831357	12.116365
20.743227	1259.363500	12.121370
20.849734	1254.481578	12.126375
21.162931	1266.385787	12.131379
21.204804	1259.808865	12.136384
21.637284	1265.409106	12.141389
21.123590	1252.495110	12.146394
20.739962	1233.918352	12.151399
20.724466	1234.339005	12.156403
21.284313	1248.450940	12.161408
21.524837	1253.381843	12.166413
21.253422	1233.922937	12.171418
21.222518	1235.425457	12.176423
20.745987	1233.319071	12.181427
20.935546	1225.131558	12.186432
21.466190	1234.799747	12.191437
21.231453	1221.434915	12.196442
21.310684	1229.050077	12.201447
20.849429	1230.064667	12.206451
20.882543	1234.036770	12.211456
20.856763	1238.506874	12.216461
21.076046	1239.901760	12.221466
21.169377	1240.249280	12.226471
21.205229	1237.829643	12.231475
21.028666	1219.772405	12.236480
20.914154	1213.411004	12.241485
20.924959	1205.534811	12.246490
21.259460	1197.974179	12.251495
20.935493	1205.924518	12.256499
21.419942	1195.569460	12.261504
21.014526	1200.072276	12.266509
20.817871	1204.128373	12.271514
21.040781	1203.871826	12.276519
20.975391	1202.528250	12.281523
20.863006	1200.151403	12.286528
20.754998	1199.792119	12.291533
20.463716	1204.351552	12.296538
20.505789	1207.242100	12.301543
20.974621	1223.589250	12.306547
21.048992	1226.395710	12.311552
21.177133	1225.095134	12.316557
21.220214	1213.644542	12.321562
21.139146	1196.812815	12.326567
20.997876	1204.245112	12.331571
21.310873	1197.872391	12.336576
21.154907	1203.224947	12.341581
21.098863	1200.693176	12.346586
21.300176	1201.446132	12.351591
20.615819	1207.180212	12.356595
20.711919	1209.578333	12.361600
20.700859	1209.042951	12.366605
20.664885	1209.898962	12.371610
21.079040	1210.266474	12.376615
20.929102	1217.697500	12.381619
21.033055	1206.916221	12.386624
21.147878	1201.128536	12.391629
20.868688	1207.867238	12.396634
20.976085	1214.290971	12.401639
20.813868	1217.903004	12.406643
20.692617	1212.621982	12.411648
20.334474	1217.098934	12.416653
20.606786	1217.590241	12.421658
21.386867	1227.805007	12.426663
20.792143	1226.667847	12.431667
20.691036	1221.458765	12.436672
20.789968	1231.418080	12.441677
21.060375	1236.879519	12.446682
20.908223	1236.132666	12.451687
20.827329	1249.629716	12.456691
21.483562	1241.995346	12.461696
20.954215	1241.427247	12.466701
20.737477	1228.822754	12.471706
20.884307	1226.273563	12.476711
20.703128	1228.664360	12.481715
21.000489	1241.176009	12.486720
21.080425	1255.091942	12.491725
21.338967	1245.536255	12.496730
21.369199	1235.934850	12.501735
20.896536	1229.247608	12.506739
20.905857	1219.776905	12.511744
20.968126	1228.425251	12.516749
21.171581	1219.046396	12.521754
20.918920	1227.713213	12.526759
21.185369	1225.717072	12.531763
20.836534	1221.534951	12.536768
20.865852	1228.375109	12.541773
20.849978	1234.493535	12.546778
21.095308	1223.653661	12.551783
20.943833	1227.967285	12.556787
21.405816	1217.375272	12.561792
21.266882	1230.236855	12.566797
21.165827	1227.511478	12.571802
21.310045	1222.512572	12.576807
21.145339	1225.571210	12.581811
21.673296	1213.683398	12.586816
21.308857	1200.467535	12.591821
21.084235	1191.478281	12.596826
20.951772	1189.730938	12.601831
20.840626	1196.208714	12.606835
20.907245	1188.976652	12.611840
21.033313	1198.024179	12.616845
20.836763	1200.639452	12.621850
21.173091	1195.114978	12.626855
20.851692	1199.817733	12.631859
20.882475	1197.229232	12.636864
20.727301	1198.979638	12.641869
20.875637	1200.876559	12.646874
20.838818	1202.531671	12.651879
20.585672	1207.450886	12.656883
20.792676	1191.572021	12.661888
20.608399	1199.297877	12.666893
20.344497	1198.570976	12.671898
20.688287	1218.417231	12.676903
20.796610	1222.476305	12.681907
21.345506	1227.873807	12.686912
21.089449	1231.597460	12.691917
20.869275	1229.963048	12.696922
21.019882	1231.622738	12.701927
20.796167	1244.003072	12.706931
21.201178	1233.078576	12.711936
21.167221	1239.047734	12.716941
20.732930	1235.246977	12.721946
21.271949	1219.890242	12.726951
21.018653	1222.792752	12.731955
21.134870	1205.923242	12.736960
20.678958	1201.566062	12.741965
20.630921	1205.642468	12.746970
21.037408	1214.585476	12.751975
20.664354	1236.527582	12.756979
21.016593	1232.361834	12.761984
21.087762	1235.694641	12.766989
21.243530	1231.295733	12.771994
20.846105	1221.770425	12.776999
20.664660	1222.322165	12.782003
20.746168	1225.207139	12.787008
20.880511	1238.533458	12.792013
20.819466	1241.017739	12.797018
21.490957	1236.532378	12.802023
21.058210	1235.996665	12.807027
20.997019	1213.554199	12.812032
20.772916	1214.190227	12.817037
20.912104	1209.285347	12.822042
21.030630	1202.531884	12.827047
20.949009	1204.957318	12.832051
21.329902	1204.306968	12.837056
21.038031	1214.082619	12.842061
21.007505	1212.288585	12.847066
20.979895	1208.800610	12.852071
21.010184	1219.615645	12.857075
21.339854	1208.643688	12.862080
20.942223	1207.918399	12.867085
20.978850	1210.892383	12.872090
21.028286	1207.430672	12.877095
20.933776	1219.294617	12.882099
20.762457	1208.829354	12.887104
20.623136	1213.949320	12.892109
20.742165	1202.588741	12.897114
20.951151	1204.048154	12.902119
20.836519	1218.369656	12.907123
21.301709	1206.601560	12.912128
21.200257	1209.282635	12.917133
21.083278	1207.779744	12.922138
21.229544	1211.852047	12.927143
21.193280	1211.864940	12.932147
21.317906	1202.436451	12.937152
20.953105	1204.505040	12.942157
21.112089	1204.683406	12.947162
21.276961	1207.953166	12.952167
21.361902	1193.142872	12.957171
20.861394	1178.352051	12.962176
20.884566	1178.486991	12.967181
20.894203	1171.259575	12.972186
20.883275	1173.889991	12.977191
20.673241	1178.355353	12.982195
20.909715	1171.642865	12.987200
20.876957	1186.365962	12.992205
20.888909	1202.059576	12.997210
21.161424	1203.044669	13.002215
20.804849	1188.966141	13.007219
21.053846	1182.819533	13.012224
20.951801	1189.763120	13.017229
20.407449	1189.668916	13.022234
20.934436	1194.624105	13.027239
20.846915	1214.639045	13.032243
21.248047	1206.548688	13.037248
21.090696	1214.961128	13.042253
20.905570	1211.318184	13.047258
21.137357	1207.222437	13.052263
20.557034	1196.760203	13.057267
20.698568	1204.797702	13.062272
20.850027	1211.571910	13.067277
20.975914	1215.127439	13.072282
20.874535	1212.893179	13.077287
20.978822	1219.223894	13.082291
21.189595	1215.574648	13.087296
20.805364	1215.529965	13.092301
20.700266	1218.288641	13.097306
20.870052	1214.914453	13.102311
20.664813	1216.920553	13.107315
20.939558	1216.608933	13.112320
20.724870	1214.672789	13.117325
21.018384	1216.677058	13.122330
20.974568	1215.959000	13.127335
20.777988	1225.508712	13.132339
21.108650	1214.312367	13.137344
20.568583	1218.457744	13.142349
21.014191	1220.019484	13.147354
21.289217	1220.404535	13.152359
20.977434	1227.834105	13.157363
21.100365	1222.896086	13.162368
20.826533	1221.034819	13.167373
20.711143	1224.493165	13.172378
20.895987	1226.813309	13.177383
20.708685	1233.036523	13.182387
20.817501	1225.136410	13.187392
20.738724	1223.574072	13.192397
20.507976	1223.868209	13.197402
21.020775	1226.135280	13.202407
20.935216	1227.320324	13.207411
21.294446	1218.809245	13.212416
21.034833	1229.841759	13.217421
21.036345	1225.635883	13.222426
21.333755	1224.620499	13.227431
20.962310	1227.465503	13.232435
21.131396	1220.347306	13.237440
21.086756	1222.959826	13.242445
21.126711	1228.419721	13.247450
20.858545	1229.506205	13.252455
20.944284	1226.460245	13.257459
20.920771	1228.618348	13.262464
20.939517	1231.134342	13.267469
21.255225	1224.819173	13.272474
21.511557	1218.611293	13.277479
21.015248	1211.391264	13.282483
21.206647	1200.577232	13.287488
20.992943	1198.110784	13.292493
20.759562	1198.068657	13.297498
20.961370	1190.543412	13.302503
20.571868	1191.757672	13.307507
20.780598	1203.695535	13.312512
20.737294	1217.419010	13.317517
20.696479	1229.294282	13.322522
21.345804	1224.276666	13.327527
20.962504	1233.552867	13.332531
20.805845	1227.782510	13.337536
20.998185	1232.999960	13.342541
20.967059	1228.753494	13.347546
21.135760	1229.104670	13.352551
20.995742	1227.912837	13.357555
21.190995	1216.064304	13.362560
20.426710	1215.086088	13.367565
20.831912	1229.657159	13.372570
21.303466	1223.143161	13.377575
21.180792	1228.827127	13.382579
21.133211	1208.347757	13.387584
20.807556	1195.951836	13.392589
20.888058	1192.352563	13.397594
21.143168	1190.718770	13.402599
20.887595	1198.673563	13.407603
21.152025	1186.922535	13.412608
21.328281	1195.528029	13.417613
20.780366	1194.904299	13.422618
20.804807	1191.515563	13.427623
20.733688	1208.301859	13.432627
20.523986	1203.616276	13.437632
21.005161	1198.699736	13.442637
21.176386	1200.032990	13.447642
21.228522	1196.325289	13.452647
20.972497	1205.604914	13.457651
21.056777	1187.152066	13.462656
21.098614	1203.373062	13.467661
20.878709	1192.522583	13.472666
20.878489	1198.149227	13.477671
20.837390	1204.847104	13.482675
21.168483	1199.886822	13.487680
21.602140	1199.057292	13.492685
21.632705	1201.766652	13.497690
21.249484	1194.263949	13.502695
21.424698	1200.123806	13.507699
21.337152	1173.886926	13.512704
21.236848	1178.511107	13.517709
21.186887	1175.892638	13.522714
21.113601	1166.491789	13.527719
20.718181	1183.399585	13.532723
20.325630	1168.892634	13.537728
20.845674	1170.754240	13.542733
20.760446	1165.190344	13.547738
20.917597	1162.539919	13.552743
20.621302	1164.603467	13.557747
21.036151	1166.802060	13.562752
20.652498	1171.166530	13.567757
20.654273	1185.622386	13.572762
20.930255	1196.891469	13.577767
20.764870	1202.260245	13.582771
20.776439	1195.150120	13.587776
20.923564	1206.088010	13.592781
20.978612	1207.259997	13.597786
21.377621	1200.944765	13.602791
20.921707	1210.683802	13.607795
21.103296	1203.841367	13.612800
21.181180	1203.407973	13.617805
21.003833	1195.186673	13.622810
21.101641	1177.057968	13.627815
20.709961	1184.936616	13.632819
21.050492	1175.927050	13.637824
20.821628	1165.516683	13.642829
20.785247	1169.551607	13.647834
21.117742	1170.154568	13.652839
20.986533	1171.632833	13.657843
20.901022	1168.900854	13.662848
20.745531	1171.773164	13.667853
20.993620	1189.585509	13.672858
21.026865	1177.502675	13.677863
20.619972	1177.517141	13.682867
20.972471	1192.979460	13.687872
21.053233	1205.002028	13.692877
21.219838	1196.677148	13.697882
20.780681	1188.715875	13.702887
20.628819	1181.285222	13.707891
20.810415	1198.136730	13.712896
21.177344	1203.748188	13.717901
21.182144	1205.291953	13.722906
20.807216	1190.830908	13.727911
20.801656	1197.659664	13.732915
20.836069	1204.468937	13.737920
20.873034	1204.367036	13.742925
20.950042	1215.511562	13.747930
21.289383	1210.547099	13.752935
21.084493	1214.106053	13.757939
21.048440	1197.942799	13.762944
20.553042	1187.422588	13.767949
20.772847	1205.645595	13.772954
21.192143	1205.111030	13.777959
21.388828	1199.101676	13.782963
20.789268	1185.429554	13.787968
20.779575	1185.707500	13.792973
20.383150	1188.123354	13.797978
20.775326	1203.851252	13.802983
20.789166	1212.840660	13.807987
20.995611	1214.786831	13.812992
21.359609	1213.628187	13.817997
20.795235	1220.802638	13.823002
21.265854	1210.739683	13.828007
21.088262	1219.547178	13.833011
20.960785	1197.752820	13.838016
21.084449	1194.104698	13.843021
20.750353	1183.287621	13.848026
21.180008	1183.235233	13.853031
21.071514	1184.412759	13.858035
20.821759	1186.755307	13.863040
20.913617	1195.421458	13.868045
20.772083	1182.911082	13.873050
20.881136	1185.385138	13.878055
20.780972	1189.797717	13.883059
21.047535	1201.244078	13.888064
21.049091	1214.909727	13.893069
20.888705	1201.172554	13.898074
20.818615	1198.139502	13.903079
20.821275	1213.177081	13.908083
20.825770	1212.458634	13.913088
20.980724	1217.142483	13.918093
21.199121	1222.923101	13.923098
21.255009	1204.721024	13.928103
20.888672	1198.546492	13.933107
21.069712	1190.613092	13.938112
20.981014	1182.298835	13.943117
20.835863	1190.166006	13.948122
20.992021	1183.895578	13.953127
20.952761	1187.326651	13.958131
20.851511	1183.775913	13.963136
20.798497	1197.635642	13.968141
20.814115	1189.835607	13.973146
21.115124	1190.414757	13.978151
21.156014	1193.976959	13.983155
21.182570	1184.499770	13.988160
21.140824	1191.217884	13.993165
20.864545	1198.190953	13.998170
21.042338	1194.056704	14.003175
20.856792	1196.976803	14.008179
20.565797	1193.892416	14.013184
20.507429	1191.359861	14.018189
20.820629	1202.775324	14.023207
21.230045	1208.240603	14.028224
20.937162	1206.112646	14.033242
20.947020	1202.044824	14.038259
20.980124	1206.850548	14.043277
20.790178	1216.987098	14.048295
20.964901	1216.346816	14.053312
21.002226	1220.347813	14.058330
21.279018	1224.660539	14.063347
21.331107	1224.186571	14.068365
20.918620	1219.869085	14.073383
21.172971	1224.632942	14.078400
20.769592	1231.916870	14.083418
21.157064	1219.028814	14.088435
21.463153	1227.999126	14.093453
21.063926	1236.020990	14.098471
21.385738	1228.836809	14.103488
21.149214	1241.167378	14.108506
21.357852	1224.927399	14.113523
21.511874	1226.736548	14.118541
21.210942	1236.961832	14.123559
21.191315	1229.160543	14.128576
21.078369	1233.824373	14.133594
21.350583	1228.617371	14.138611
20.924974	1225.808957	14.143629
21.268383	1237.345540	14.148647
21.429782	1224.622237	14.153664
21.054866	1233.194705	14.158682
21.128197	1236.161490	14.163699
21.342434	1238.918273	14.168717
21.420589	1240.328584	14.173735
21.175513	1225.994511	14.178752
21.194986	1246.980375	14.183770
21.404292	1262.321012	14.188787
21.442326	1261.094661	14.193805
21.390422	1266.251229	14.198823
22.152505	1253.090234	14.203840
21.835981	1257.381459	14.208858
22.011045	1246.800867	14.213875
21.578625	1228.107582	14.218893
21.673356	1229.965089	14.223911
22.083887	1224.958015	14.228928
21.411879	1228.663277	14.233946
21.678119	1221.965046	14.238963
21.587674	1228.162551	14.243981
21.931568	1244.238034	14.248999
21.918424	1233.644441	14.254016
21.441958	1226.889284	14.259034
21.535268	1245.118546	14.264051
21.874594	1248.145642	14.269069
21.862759	1256.815332	14.274087
22.218616	1262.915066	14.279104
21.776893	1266.464306	14.284122
22.154183	1259.101292	14.289139
21.951387	1242.852304	14.294157
21.684995	1244.998916	14.299175
21.871440	1241.776869	14.304192
21.830920	1257.643449	14.309210
21.917194	1257.775879	14.314227
22.268626	1262.751468	14.319245
21.649757	1259.911218	14.324263
22.116605	1266.551028	14.329280
22.249348	1263.536626	14.334298
22.099152	1264.408088	14.339315
22.382823	1269.483495	14.344333
21.580434	1270.232508	14.349351
21.632948	1260.167846	14.354368
21.948973	1267.665086	14.359386
21.706444	1265.287914	14.364403
22.089343	1268.597333	14.369421
22.075651	1266.820745	14.374439
22.668386	1260.861077	14.379456
22.296599	1275.551294	14.384474
22.004649	1268.332159	14.389491
22.166104	1264.470633	14.394509
22.191602	1273.611533	14.399527
22.183977	1269.193905	14.404544
21.930495	1275.103999	14.409562
22.186992	1285.724728	14.414579
22.455157	1284.898721	14.419597
22.669286	1293.572999	14.424615
22.970240	1286.203374	14.429632
22.712388	1280.039901	14.434650
22.427283	1280.341134	14.439667
22.478704	1265.063588	14.444685
22.286797	1275.770642	14.449703
22.287123	1273.205753	14.454720
22.481145	1285.504666	14.459738
22.314651	1298.926522	14.464755
22.678000	1302.302298	14.469773
22.797059	1306.921251	14.474791
22.826827	1301.764851	14.479808
22.456705	1290.448103	14.484826
22.641015	1293.816382	14.489843
23.088304	1292.869890	14.494861
22.512368	1298.787639	14.499879
22.594739	1277.834965	14.504896
22.717994	1297.343915	14.509914
22.728535	1297.194027	14.514931
22.641087	1307.477644	14.519949
22.575633	1304.886229	14.524967
23.061529	1296.888772	14.529984
23.357160	1302.378712	14.535002
22.846281	1293.917852	14.540019
23.048121	1279.035799	14.545037
22.848892	1268.085077	14.550055
23.119182	1267.554797	14.555072
23.083792	1267.180480	14.560090
22.915225	1268.406304	14.565107
22.701487	1268.255497	14.570125
22.729751	1271.769042	14.575143
22.824356	1282.125767	14.580160
23.053813	1292.658608	14.585178
23.028350	1302.486671	14.590195
23.321674	1294.217875	14.595213
22.844344	1300.109267	14.600231
22.971566	1299.229860	14.605248
23.067765	1294.551487	14.610266
23.062007	1301.842475	14.615283
23.529134	1304.870112	14.620301
23.611823	1299.571162	14.625319
23.131121	1279.257599	14.630336
23.029595	1280.994417	14.635354
23.102864	1296.680096	14.640371
23.151928	1293.759177	14.645389
22.917939	1297.133030	14.650407
23.089933	1293.919749	14.655424
23.321792	1302.252379	14.660442
22.883746	1304.380394	14.665459
23.087274	1302.756340	14.670477
23.131732	1299.627135	14.675495
23.073697	1293.941648	14.680512
23.590987	1294.936088	14.685530
22.993682	1304.630289	14.690547
23.642333	1304.220190	14.695565
23.832823	1312.288240	14.700583
23.186373	1305.536994	14.705600
23.527446	1319.980606	14.710618
23.680112	1330.717602	14.715635
23.567781	1317.191865	14.720653
23.933096	1309.285161	14.725671
23.956787	1309.021590	14.730688
24.183810	1293.848959	14.735706
23.721639	1307.285296	14.740723
23.901385	1295.044267	14.745741
23.950604	1297.161577	14.750759
24.050615	1302.365344	14.755776
23.771461	1298.758506	14.760794
23.575723	1296.736332	14.765811
23.831332	1299.760074	14.770829
23.198041	1309.017493	14.775847
23.474033	1302.566004	14.780864
23.429443	1303.510314	14.785882
23.293972	1310.507376	14.790899
23.593232	1314.493017	14.795917
23.349845	1325.073879	14.800935
23.726136	1342.555458	14.805952
23.854095	1331.134775	14.810970
23.691784	1326.234155	14.815987
24.151514	1335.360881	14.821005
23.990255	1331.742090	14.826023
24.060518	1323.224095	14.831040
24.359326	1327.896101	14.836058
23.792612	1328.622426	14.841075
24.108546	1325.079707	14.846093
24.165638	1331.245262	14.851111
23.838405	1328.592025	14.856128
24.093019	1332.963313	14.861146
23.997652	1330.959361	14.866163
23.986243	1320.932001	14.871181
24.028500	1328.166339	14.876199
24.277819	1325.703251	14.881216
24.394028	1321.221852	14.886234
24.499570	1331.783841	14.891251
24.504253	1329.327261	14.896269
24.425880	1327.456235	14.901287
24.672534	1323.280058	14.906304
24.585686	1316.836046	14.911322
24.746010	1337.219875	14.916339
24.665095	1323.063097	14.921357
24.405540	1325.228234	14.926375
24.483601	1325.824320	14.931392
24.420936	1325.716907	14.936410
24.333324	1327.619865	14.941427
24.377949	1315.608306	14.946445
24.618524	1326.555051	14.951463
24.114827	1317.751182	14.956480
24.246360	1319.448438	14.961498
24.456570	1321.762185	14.966515
24.590705	1319.198757	14.971533
24.423696	1326.847357	14.976551
24.383730	1325.418607	14.981568
24.691029	1321.381654	14.986586
24.463646	1330.557677	14.991603
24.657801	1317.895617	14.996621
24.454320	1325.846954	15.001639
24.409008	1329.800725	15.006656
24.656175	1343.859635	15.011674
24.585948	1358.884482	15.016691
25.027364	1357.896864	15.021709
24.788413	1352.008101	15.026727
24.978876	1361.396384	15.031744
25.119690	1355.743322	15.036762
24.895872	1364.150571	15.041779
25.225031	1359.585400	15.046797
25.025615	1356.104654	15.051815
24.726141	1347.016910	15.056832
25.038580	1347.494456	15.061850
24.913359	1356.213173	15.066867
25.317968	1358.113243	15.071885
25.043737	1359.986778	15.076903
24.994124	1352.085048	15.081920
25.270398	1348.404621	15.086938
25.216051	1353.587229	15.091955
25.396783	1343.688736	15.096973
25.358075	1336.040286	15.101991
25.492461	1330.060745	15.107008
24.773173	1326.777814	15.112026
24.565952	1324.897775	15.117043
25.343168	1338.356696	15.122061
24.925208	1350.623569	15.127079
24.757412	1350.678291	15.132096
25.102129	1346.344336	15.137114
24.870555	1356.759400	15.142131
24.978920	1358.891383	15.147149
25.420349	1348.139843	15.152167
25.030982	1357.026303	15.157184
25.249030	1360.086420	15.162202
25.441426	1384.440782	15.167219
25.395199	1383.070980	15.172237
25.687457	1386.647958	15.177255
26.009920	1382.165432	15.182272
25.820763	1358.824717	15.187290
25.412021	1359.201486	15.192307
25.448015	1357.552209	15.197325
25.554472	1345.321738	15.202343
25.351650	1353.710419	15.207360
25.622615	1349.607634	15.212378
25.982350	1374.127401	15.217395
25.505140	1358.097407	15.222413
25.510723	1360.826990	15.227431
25.731098	1378.896814	15.232448
26.167762	1381.599343	15.237466
25.619092	1371.750690	15.242483
25.634682	1358.998729	15.247501
25.664736	1367.149438	15.252519
25.762377	1380.417799	15.257536
26.038662	1380.397560	15.262554
26.009825	1384.314265	15.267571
26.301127	1386.145174	15.272589
25.830035	1366.277530	15.277607
25.976870	1369.395927	15.282624
26.019236	1366.240688	15.287642
25.891899	1376.406768	15.292659
25.933538	1379.147496	15.297677
26.212854	1372.298126	15.302695
26.267659	1382.889717	15.307712
26.484259	1372.169623	15.312730
26.071981	1358.729533	15.317747
25.735567	1351.606968	15.322765
26.067565	1360.956022	15.327783
25.891993	1386.210959	15.332800
26.235856	1376.146667	15.337818
25.982041	1386.385231	15.342835
26.284986	1386.712817	15.347853
26.323736	1379.770426	15.352871
26.164963	1384.844165	15.357888
26.390684	1391.299366	15.362906
26.100420	1390.781327	15.367923
25.878254	1385.341292	15.372941
26.510247	1385.903040	15.377959
26.416994	1386.765532	15.382976
26.325796	1386.590957	15.387994
26.227372	1382.985005	15.393011
26.453464	1389.038134	15.398029
26.351454	1386.872699	15.403047
26.227568	1387.816830	15.408064
26.488116	1387.038191	15.413082
26.203548	1397.219825	15.418099
26.585799	1404.881385	15.423117
26.680805	1407.924416	15.428135
26.442712	1412.235309	15.433152
26.913175	1405.749647	15.438170
26.758602	1411.648740	15.443187
26.814076	1416.272328	15.448205
26.795405	1415.010014	15.453223
26.574068	1414.064761	15.458240
26.605897	1410.258499	15.463258
26.569705	1411.897507	15.468275
26.175095	1405.876341	15.473293
26.631360	1409.078713	15.478311
26.688327	1416.394437	15.483328
26.964340	1405.764537	15.488346
26.726656	1417.284733	15.493363
26.927195	1412.527799	15.498381
27.171663	1405.757626	15.503399
26.916870	1412.844097	15.508416
26.887727	1403.003994	15.513434
26.660533	1421.956198	15.518451
26.791693	1430.611704	15.523469
27.305552	1439.697711	15.528487
26.792354	1439.525405	15.533504
27.262207	1425.018563	15.538522
27.783113	1428.382314	15.543539
27.364907	1411.616091	15.548557
27.744292	1396.623163	15.553575
27.528862	1398.068470	15.558592
27.765352	1391.884767	15.563610
27.444379	1390.121477	15.568627
27.558524	1387.652026	15.573645
27.531858	1383.325433	15.578663
27.161204	1397.721447	15.583680
27.227217	1396.442646	15.588698
27.544924	1398.052867	15.593715
27.306196	1397.572452	15.598733
27.558816	1383.725397	15.603751
27.441814	1390.213767	15.608768
27.577314	1397.408133	15.613786
27.239301	1396.538402	15.618803
27.221882	1398.811260	15.623821
27.896442	1392.720967	15.628839
27.459045	1394.967398	15.633856
27.926515	1396.854332	15.638874
27.671323	1397.193749	15.643891
27.396442	1396.051358	15.648909
27.170687	1388.857435	15.653927
27.261646	1399.628683	15.658944
27.477860	1397.644929	15.663962
27.331459	1410.492515	15.668979
28.019751	1426.576073	15.673997
28.146854	1425.723059	15.679015
28.336365	1435.280859	15.684032
27.805110	1413.894970	15.689050
28.238906	1406.571023	15.694067
27.993486	1404.725873	15.699085
28.237334	1406.886606	15.704103
27.960275	1402.652158	15.709120
27.946334	1402.689555	15.714138
27.710541	1399.838720	15.719155
27.709117	1406.795123	15.724173
27.890126	1396.002761	15.729191
27.440800	1406.735535	15.734208
27.972325	1422.289613	15.739226
27.984424	1423.135225	15.744243
27.847300	1431.192966	15.749261
28.182995	1422.326621	15.754279
27.979036	1428.118429	15.759296
27.828923	1429.815558	15.764314
28.510786	1427.202693	15.769331
28.061448	1434.757219	15.774349
28.320536	1422.454845	15.779367
27.904631	1433.035435	15.784384
28.127743	1431.465496	15.789402
28.164763	1441.203791	15.794419
28.450828	1461.520549	15.799437
28.879823	1465.309952	15.804455
28.747421	1444.962834	15.809472
28.571525	1433.478020	15.814490
28.615245	1430.349310	15.819507
28.416315	1428.842677	15.824525
28.551917	1427.254275	15.829543
28.502048	1427.408474	15.834560
28.234288	1426.657811	15.839578
28.750677	1437.029338	15.844595
28.622705	1453.747811	15.849613
28.431839	1449.128061	15.854631
28.704683	1461.996729	15.859648
28.767313	1462.650983	15.864666
28.811577	1451.827298	15.869683
28.672415	1466.807370	15.874701
28.910200	1461.859764	15.879719
29.072115	1469.932795	15.884736
28.684816	1463.689858	15.889754
29.007863	1461.846456	15.894771
29.002863	1468.789325	15.899789
29.439359	1462.652806	15.904807
28.843095	1461.950592	15.909824
29.107797	1461.434651	15.914842
29.198551	1458.619557	15.919859
28.709860	1457.574456	15.924877
28.811763	1458.158191	15.929895
29.204542	1468.409973	15.934912
29.027968	1468.496912	15.939930
29.160113	1461.923156	15.944947
29.146565	1465.521086	15.949965
29.053612	1460.973136	15.954983
29.396808	1470.142365	15.960000
28.976924	1467.894793	15.965018
29.160438	1453.946914	15.970035
28.852688	1467.453771	15.975053
29.217085	1462.553361	15.980071
29.226817	1473.056275	15.985088
28.973417	1462.529708	15.990106
29.110542	1460.552419	15.995123
28.779682	1476.480815	16.000141
29.441260	1490.710167	16.005159
29.199839	1500.696261	16.010176
29.607838	1490.285825	16.015194
29.529592	1489.976731	16.020211
29.389468	1496.666768	16.025229
29.870858	1490.094150	16.030247
29.896105	1496.262080	16.035264
29.725005	1495.723605	16.040282
30.060200	1494.329345	16.045299
29.945555	1502.197816	16.050317
29.885384	1479.614413	16.055335
29.661909	1472.633862	16.060352
29.263931	1467.072352	16.065370
29.786540	1474.894940	16.070387
29.659916	1487.971899	16.075405
29.739709	1484.349541	16.080423
30.167277	1486.151587	16.085440
30.069826	1491.614100	16.090458
29.983075	1488.532948	16.095475
29.803803	1494.942659	16.100493
30.344275	1485.449768	16.105511
30.438808	1494.324210	16.110528
30.074030	1473.445971	16.115546
29.899378	1455.441362	16.120563
29.737402	1468.877552	16.125581
29.967495	1482.456395	16.130599
30.153842	1488.663637	16.135616
29.939764	1490.772175	16.140634
30.217543	1490.417000	16.145651
29.902570	1493.933927	16.150669
29.933850	1490.002924	16.155687
30.155522	1489.978662	16.160704
29.912074	1489.933350	16.165722
30.063409	1486.558595	16.170739
30.098270	1499.411005	16.175757
30.193209	1513.741471	16.180775
30.220740	1527.792531	16.185792
30.325241	1524.760085	16.190810
30.558047	1519.371142	16.195827
30.289014	1522.941229	16.200845
30.640509	1513.468910	16.205863
30.902044	1512.162876	16.210880
30.361404	1510.415580	16.215898
30.806194	1504.658765	16.220915
30.501014	1513.308414	16.225933
30.767747	1506.682426	16.230951
30.619746	1510.447529	16.235968
30.434081	1512.484262	16.240986
31.008353	1516.648418	16.246003
30.326322	1517.911899	16.251021
30.559665	1521.773842	16.256039
30.716034	1520.038941	16.261056
30.800738	1517.924554	16.266074
31.070091	1512.921908	16.271091
30.847347	1521.449148	16.276109
30.754590	1513.727980	16.281127
31.004066	1512.159419	16.286144
30.803268	1509.482897	16.291162
31.058158	1506.424275	16.296179
31.051863	1513.889489	16.301197
31.062061	1514.898835	16.306215
31.072949	1514.064955	16.311232
30.828693	1517.958780	16.316250
31.125881	1510.405818	16.321267
31.249636	1517.665252	16.326285
31.131273	1507.359621	16.331303
31.146078	1517.365974	16.336320
31.174438	1538.149896	16.341338
31.294721	1543.481385	16.346355
31.416358	1550.594725	16.351373
31.761985	1537.073750	16.356391
31.756860	1516.724402	16.361408
31.417686	1512.488761	16.366426
31.158740	1503.010865	16.371443
31.313793	1502.951564	16.376461
31.245918	1513.449699	16.381479
31.547854	1527.142654	16.386496
31.776180	1540.206441	16.391514
31.704335	1535.949764	16.396531
31.521031	1526.738048	16.401549
31.827384	1532.780622	16.406567
31.957231	1522.822229	16.411584
31.210451	1517.533520	16.416602
31.676678	1520.042009	16.421619
31.840274	1542.988021	16.426637
31.619964	1541.595291	16.431655
31.874698	1540.849930	16.436672
31.846845	1544.231410	16.441690
32.055535	1535.601760	16.446707
31.968738	1542.494901	16.451725
31.955922	1543.064446	16.456743
32.173684	1532.513747	16.461760
31.846194	1536.936075	16.466778
31.796948	1531.350186	16.471795
31.814842	1528.847998	16.476813
31.958661	1533.988026	16.481831
32.114041	1524.008324	16.486848
31.870267	1541.228292	16.491866
32.159271	1532.817182	16.496883
32.332053	1539.769369	16.501901
32.232341	1533.476307	16.506919
32.427354	1534.706356	16.511936
32.045416	1537.583917	16.516954
32.050651	1533.012024	16.521971
32.043069	1541.789816	16.526989
31.775375	1540.930464	16.532007
32.296003	1527.481078	16.537024
31.720065	1538.307311	16.542042
32.373851	1545.186873	16.547059
32.321439	1563.092636	16.552077
32.514517	1564.695893	16.557095
32.616639	1564.472420	16.562112
32.374322	1574.211443	16.567130
32.607730	1558.808302	16.572147
32.772015	1565.533193	16.577165
32.875518	1566.411571	16.582183
33.174877	1562.924009	16.587200
32.525205	1547.260040	16.592218
32.458009	1535.318277	16.597235
32.793594	1549.320477	16.602253
32.603659	1556.703012	16.607271
32.853839	1557.108949	16.612288
32.829840	1563.759023	16.617306
32.896613	1561.651642	16.622323
32.958706	1560.564072	16.627341
32.710699	1568.220377	16.632359
33.193692	1561.149763	16.637376
32.801675	1567.792852	16.642394
32.836679	1560.936465	16.647411
33.102655	1567.926235	16.652429
33.223814	1566.338720	16.657447
33.774915	1562.646561	16.662464
33.367887	1566.626579	16.667482
33.285411	1559.463529	16.672499
33.443459	1559.343078	16.677517
33.135325	1550.731159	16.682535
33.177160	1542.790421	16.687552
33.117861	1549.720981	16.692570
33.274602	1557.332296	16.697587
32.843139	1561.749621	16.702605
33.044575	1561.556763	16.707623
32.901333	1563.859487	16.712640
32.602790	1565.162349	16.717658
32.717472	1577.223100	16.722675
33.356669	1581.448591	16.727693
32.868435	1598.866065	16.732711
33.195915	1596.229280	16.737728
33.411080	1596.485693	16.742746
33.408607	1595.763560	16.747763
33.464756	1601.285612	16.752781
33.562183	1615.524790	16.757799
34.146995	1605.813177	16.762816
33.964668	1616.685769	16.767834
33.950190	1602.998502	16.772851
33.841699	1590.513716	16.777869
33.692181	1587.305496	16.782887
34.065211	1583.081990	16.787904
33.834530	1588.449651	16.792922
34.045078	1582.759745	16.797939
34.333185	1590.252479	16.802957
33.722514	1596.015251	16.807975
34.085218	1582.191277	16.812992
33.690326	1587.435894	16.818010
34.170380	1584.982030	16.823027
34.206877	1585.769525	16.828045
34.093118	1585.421631	16.833063
34.376663	1590.079797	16.838080
34.070392	1591.264681	16.843098
34.068045	1586.358209	16.848115
34.254240	1590.405832	16.853133
33.828955	1613.899028	16.858151
34.460181	1611.674387	16.863168
34.291254	1615.984502	16.868186
34.282920	1617.591193	16.873203
34.595942	1615.775086	16.878221
34.349932	1618.164343	16.883239
34.744864	1617.666231	16.888256
34.503574	1627.123189	16.893274
34.349523	1627.107436	16.898291
34.341707	1617.545463	16.903309
34.265005	1624.639293	16.908327
34.543410	1611.043157	16.913344
34.650110	1618.264612	16.918362
34.308115	1623.246994	16.923379
34.346528	1615.698583	16.928397
34.463753	1623.909292	16.933415
34.569229	1631.066782	16.938432
34.568980	1640.076075	16.943450
34.672707	1647.168511	16.948467
35.395540	1644.035932	16.953485
35.099677	1652.616335	16.958503
35.135958	1649.257728	16.963520
34.992988	1647.631230	16.968538
35.143786	1646.035476	16.973555
35.143184	1635.288656	16.978573
34.906077	1638.726902	16.983591
35.474135	1634.116361	16.988608
35.328993	1637.377797	16.993626
35.051218	1616.634072	16.998643
35.153123	1615.462105	17.003661
35.138576	1629.838617	17.008679
35.453002	1633.247267	17.013696
35.422362	1628.228296	17.018714
34.995538	1628.325854	17.023731
35.376000	1636.810370	17.028749
34.814592	1646.376169	17.033767
34.992896	1649.120288	17.038784
34.965059	1640.174008	17.043802
34.787876	1646.767695	17.048819
35.292171	1657.918304	17.053837
35.261589	1673.583580	17.058855
35.510055	1669.881466	17.063872
35.792360	1675.144665	17.068890
35.537651	1674.733917	17.073907
35.942516	1674.207719	17.078925
35.644883	1677.799675	17.083943
35.657498	1674.028931	17.088960
35.675386	1676.969476	17.093978
35.626928	1671.626737	17.098995
36.001611	1673.372117	17.104013
35.901142	1679.886516	17.109031
36.029003	1671.183633	17.114048
36.296202	1680.802682	17.119066
36.394877	1675.578432	17.124083
36.353305	1670.345943	17.129101
36.393583	1662.689303	17.134119
36.257118	1650.245884	17.139136
36.188958	1644.876214	17.144154
35.641162	1646.117082	17.149171
35.889843	1645.764531	17.154189
36.038205	1661.921615	17.159207
36.125767	1664.746656	17.164224
36.424470	1674.884376	17.169242
36.248871	1680.513521	17.174259
36.011761	1681.717266	17.179277
36.166698	1673.531454	17.184295
36.179926	1672.508166	17.189312
36.393172	1679.990548	17.194330
36.169069	1680.499463	17.199347
36.638618	1673.842569	17.204365
35.986773	1681.900885	17.209383
36.318565	1673.378809	17.214400
36.524475	1680.153312	17.219418
36.386282	1698.289316	17.224435
36.703222	1699.969788	17.229453
36.638630	1706.129581	17.234471
36.736697	1696.074546	17.239488
36.548116	1695.647735	17.244506
36.679968	1705.824320	17.249523
36.783540	1698.454089	17.254541
36.725067	1703.331185	17.259559
37.019208	1705.682180	17.264576
37.044252	1700.018131	17.269594
36.661061	1701.902119	17.274611
36.853362	1696.223963	17.279629
36.770091	1704.481297	17.284647
36.695641	1699.854112	17.289664
37.223817	1701.354255	17.294682
36.721473	1700.348883	17.299699
37.155470	1705.858556	17.304717
36.952970	1727.639118	17.309735
37.258727	1727.570909	17.314752
37.230834	1723.502731	17.319770
37.047840	1726.592308	17.324787
37.278019	1720.244972	17.329805
37.492202	1730.464156	17.334823
37.498676	1723.856320	17.339840
37.595036	1720.063724	17.344858
37.348596	1733.482729	17.349875
37.491014	1725.734127	17.354893
37.505606	1731.111758	17.359911
37.381315	1725.786333	17.364928
37.549371	1717.697473	17.369946
37.729516	1721.650093	17.374963
37.424120	1708.398485	17.379981
37.613103	1719.413021	17.384999
37.861826	1716.764914	17.390016
37.720189	1719.346159	17.395034
37.569430	1728.558889	17.400051
37.947277	1713.693103	17.405069
37.578839	1713.673944	17.410087
37.672235	1718.366720	17.415104
37.802536	1737.444647	17.420122
37.735985	1743.537065	17.425139
38.109460	1752.551646	17.430157
38.129416	1749.482465	17.435175
38.348055	1752.473260	17.440192
38.081902	1743.352008	17.445210
38.058766	1750.930078	17.450227
38.037963	1747.464294	17.455245
38.207417	1746.364997	17.460263
38.183375	1746.848275	17.465280
38.309023	1741.980052	17.470298
38.636099	1749.079521	17.475315
38.569966	1745.749478	17.480333
38.516198	1745.573993	17.485351
38.290287	1746.900641	17.490368
38.599263	1740.361419	17.495386
38.426564	1745.586498	17.500403
38.527754	1748.217069	17.505421
38.541791	1746.767603	17.510439
38.532884	1746.686013	17.515456
38.556605	1735.995591	17.520474
38.369098	1751.354346	17.525491
38.411889	1745.642351	17.530509
38.734844	1740.611543	17.535527
38.738307	1741.761052	17.540544
39.302280	1740.481107	17.545562
38.826208	1750.630835	17.550579
38.970834	1750.083105	17.555597
38.863802	1740.814872	17.560615
38.826769	1744.204663	17.565632
38.741015	1734.493363	17.570650
38.851434	1759.569931	17.575667
39.402043	1768.634869	17.580685
39.457295	1767.051153	17.585703
39.323116	1759.927588	17.590720
39.250573	1740.265180	17.595738
39.318427	1746.591279	17.600755
39.103088	1741.963825	17.605773
39.460436	1737.711468	17.610791
39.157615	1741.644132	17.615808
39.662701	1733.243117	17.620826
39.446464	1742.438732	17.625843
39.689956	1742.608391	17.630861
39.174587	1746.787366	17.635879
39.141703	1737.497366	17.640896
39.739431	1745.313907	17.645914
39.583026	1760.840981	17.650931
39.626702	1760.340484	17.655949
39.952361	1758.085922	17.660967
39.862483	1753.344029	17.665984
40.154101	1737.316878	17.671002
39.859765	1741.014595	17.676019
39.493766	1742.726722	17.681037
39.705922	1743.238802	17.686055
39.624082	1736.863845	17.691072
40.027542	1744.712512	17.696090
39.594800	1764.624105	17.701107
39.847940	1769.029239	17.706125
39.812939	1766.622313	17.711143
39.321883	1774.866913	17.716160
39.744371	1767.145084	17.721178
39.559621	1768.898587	17.726195
39.757086	1779.367157	17.731213
39.949624	1797.940332	17.736231
39.955275	1806.960129	17.741248
40.092275	1804.547331	17.746266
40.112018	1817.299826	17.751283
40.274014	1797.305760	17.756301
40.408779	1803.872409	17.761319
40.480236	1808.095293	17.766336
40.397157	1797.044353	17.771354
40.604453	1801.248669	17.776371
40.769685	1795.685762	17.781389
40.686342	1801.014452	17.786407
40.395920	1804.691431	17.791424
40.899719	1798.085706	17.796442
40.752442	1801.699161	17.801459
41.003868	1801.513873	17.806477
40.924716	1796.657122	17.811495
40.703778	1805.783887	17.816512
40.864359	1801.995223	17.821530
40.948261	1799.346618	17.826547
40.696425	1789.617297	17.831565
40.720356	1795.705641	17.836583
40.735772	1800.314161	17.841600
40.919621	1799.620317	17.846618
40.846013	1807.934324	17.851635
40.970741	1815.008667	17.856653
41.120910	1817.569427	17.861671
41.085695	1816.924954	17.866688
41.384500	1821.967630	17.871706
40.992754	1814.270407	17.876723
41.023780	1824.628550	17.881741
41.297016	1815.365555	17.886759
41.011904	1814.191417	17.891776
41.283623	1809.304034	17.896794
41.001617	1823.237545	17.901811
41.151821	1819.513656	17.906829
41.382646	1831.209372	17.911847
41.449788	1850.118321	17.916864
41.656392	1852.017360	17.921882
41.459405	1844.985243	17.926899
41.903801	1848.657520	17.931917
41.649256	1845.907860	17.936935
41.775427	1849.679192	17.941952
42.112825	1837.633179	17.946970
41.717752	1841.686029	17.951987
41.969862	1846.857600	17.957005
41.868816	1842.897221	17.962023
41.751565	1843.835515	17.967040
41.933486	1844.146851	17.972058
42.019595	1854.451470	17.977075
42.330237	1845.237169	17.982093
42.558976	1841.241510	17.987111
42.343136	1850.469801	17.992128
42.368985	1837.355016	17.997146
42.262437	1837.735892	18.002163
41.912890	1839.277865	18.007181
41.959618	1838.626429	18.012199
41.944298	1843.789514	18.017216
42.215889	1838.618644	18.022234
42.333463	1834.323502	18.027251
42.314023	1830.389691	18.032269
42.667060	1826.606218	18.037287
42.331449	1835.473098	18.042304
42.734073	1823.827382	18.047322
42.544671	1830.066897	18.052339
42.551433	1827.017682	18.057357
42.927845	1828.723410	18.062375
42.661602	1828.355979	18.067392
42.828902	1825.415477	18.072410
42.861538	1833.014343	18.077427
42.373973	1832.440733	18.082445
42.990139	1827.517519	18.087463
42.938356	1839.351865	18.092480
43.230066	1840.131053	18.097498
43.338461	1833.447813	18.102515
42.644371	1826.222554	18.107533
43.224294	1826.202625	18.112551
42.973382	1842.710673	18.117568
43.319728	1845.392940	18.122586
42.875062	1842.134471	18.127603
42.923953	1856.103414	18.132621
43.155894	1854.447264	18.137639
43.446066	1860.113165	18.142656
43.310695	1857.347402	18.147674
43.404416	1855.161336	18.152691
43.232893	1857.161039	18.157709
43.444162	1850.556229	18.162727
43.354095	1862.714519	18.167744
43.531334	1853.343536	18.172762
43.704439	1861.262076	18.177779
43.020048	1860.750956	18.182797
43.573710	1857.380772	18.187815
43.508785	1863.083145	18.192832
43.553476	1872.549099	18.197850
43.768608	1882.303201	18.202867
43.736145	1900.016140	18.207885
43.921935	1893.828727	18.212903
43.913298	1888.384980	18.217920
43.822720	1896.045164	18.222938
43.902240	1890.610320	18.227955
43.704896	1890.985109	18.232973
44.004696	1888.936563	18.237991
44.109808	1892.501252	18.243008
44.146333	1882.223943	18.248026
44.079949	1889.816976	18.253043
44.277904	1895.236856	18.258061
44.539850	1881.836640	18.263079
44.338743	1890.949029	18.268096
44.459906	1891.125489	18.273114
44.623787	1878.187422	18.278131
44.313391	1889.908645	18.283149
44.428320	1879.717907	18.288167
44.537929	1886.376318	18.293184
44.674334	1880.556085	18.298202
44.708720	1885.503941	18.303219
44.421509	1884.305350	18.308237
44.595263	1876.542639	18.313255
44.520498	1884.530858	18.318272
44.677291	1876.261541	18.323290
44.766241	1894.726985	18.328307
44.979510	1905.866246	18.333325
45.230192	1909.693026	18.338343
44.891973	1896.300410	18.343360
44.896579	1893.321640	18.348378
45.343696	1898.957102	18.353395
45.017578	1902.700468	18.358413
45.442037	1896.328414	18.363431
44.979651	1898.179146	18.368448
45.537161	1889.786385	18.373466
45.267197	1877.475137	18.378483
45.364550	1879.053891	18.383501
45.166382	1879.397320	18.388519
45.348855	1894.056872	18.393536
45.481003	1899.640813	18.398554
45.433395	1899.876922	18.403571
45.210958	1909.348143	18.408589
45.765570	1897.996827	18.413607
45.304165	1902.834787	18.418624
45.421081	1897.942813	18.423642
45.681454	1896.673961	18.428659
45.149657	1911.176823	18.433677
45.831432	1898.257833	18.438695
45.393128	1900.849415	18.443712
45.616552	1897.243286	18.448730
45.557744	1903.102913	18.453747
45.732509	1924.168193	18.458765
45.849196	1935.922538	18.463783
45.867001	1933.716796	18.468800
45.861141	1933.333463	18.473818
46.055818	1938.290079	18.478835
46.333248	1933.230397	18.483853
46.168687	1928.031902	18.488871
46.218553	1934.772239	18.493888
46.311566	1940.531824	18.498906
46.488920	1930.352400	18.503923
46.454609	1929.135646	18.508941
46.492457	1933.632077	18.513959
46.588687	1929.885129	18.518976
46.699960	1929.229711	18.523994
46.553344	1925.921303	18.529011
46.024545	1931.722921	18.534029
46.476975	1927.715269	18.539047
46.222207	1933.761675	18.544064
46.435049	1933.725934	18.549082
46.837880	1937.440797	18.554099
46.495170	1931.166399	18.559117
46.580540	1932.207772	18.564135
46.770604	1944.157051	18.569152
46.779728	1956.063336	18.574170
46.907049	1961.132702	18.579187
46.801164	1967.535929	18.584205
47.140824	1957.670438	18.589223
47.032469	1957.908301	18.594240
46.928503	1957.889078	18.599258
47.007797	1966.699070	18.604275
46.989095	1967.877202	18.609293
47.085237	1957.231700	18.614311
47.212007	1961.699112	18.619328
47.278797	1954.461462	18.624346
47.407057	1950.919675	18.629363
46.871806	1965.692901	18.634381
47.222194	1978.082103	18.639399
47.090825	1985.706406	18.644416
47.255363	1987.118119	18.649434
47.345761	1980.222125	18.654451
47.317512	1987.237725	18.659469
47.730942	1983.363534	18.664487
47.666359	1987.586165	18.669504
47.648423	2000.866207	18.674522
48.310574	1998.522025	18.679539
47.740060	2002.965674	18.684557
47.664268	1998.924931	18.689575
48.183530	2005.355260	18.694592
48.027145	2009.975185	18.699610
48.345408	1997.220422	18.704627
47.871831	2008.664552	18.709645
48.042998	2003.708117	18.714663
48.384016	2002.814066	18.719680
48.246196	2003.752746	18.724698
48.868125	1993.326562	18.729715
48.093618	1999.894052	18.734733
48.173287	2000.467445	18.739751
48.141258	1999.307782	18.744768
48.263406	2000.392466	18.749786
48.470273	1998.550023	18.754803
48.276097	2002.745658	18.759821
48.179220	2005.405113	18.764839
48.406013	2002.133469	18.769856
48.534802	2004.181713	18.774874
48.402293	2002.506133	18.779891
48.452535	2020.502314	18.784909
48.784318	2031.845392	18.789927
49.055149	2037.269364	18.794944
49.041917	2043.581529	18.799962
49.175410	2042.978604	18.804979
48.787931	2037.577314	18.809997
49.467685	2035.092688	18.815015
49.582235	2039.702788	18.820032
49.152348	2026.649444	18.825050
49.047454	2006.142131	18.830067
49.217451	2020.375930	18.835085
49.421927	2032.383837	18.840103
49.255433	2029.309950	18.845120
49.204630	2042.374765	18.850138
49.436098	2039.370852	18.855155
48.828289	2042.312429	18.860173
48.938156	2034.043199	18.865191
49.113016	2034.197461	18.870208
48.802731	2047.495772	18.875226
49.506183	2053.048754	18.880243
49.708818	2064.330916	18.885261
49.668306	2060.364040	18.890279
49.938625	2065.927500	18.895296
49.981349	2063.997429	18.900314
50.053974	2060.064706	18.905331
49.799368	2061.383305	18.910349
50.088007	2057.404885	18.915367
50.100020	2058.863230	18.920384
50.054884	2059.664745	18.925402
50.040129	2060.294887	18.930419
50.087577	2072.457718	18.935437
50.014314	2057.714234	18.940455
50.418664	2046.995352	18.945472
50.306823	2052.831445	18.950490
50.367714	2043.668513	18.955507
50.253839	2044.757048	18.960525
50.153937	2048.802261	18.965543
50.361053	2060.167915	18.970560
50.149725	2075.808276	18.975578
50.849016	2077.765410	18.980595
50.804396	2091.047741	18.985613
50.474292	2084.197023	18.990631
50.618903	2080.012550	18.995648
50.523767	2088.022084	19.000666
50.717526	2079.678595	19.005683
50.876921	2086.648679	19.010701
50.699493	2084.639798	19.015719
50.840144	2079.745273	19.020736
50.566675	2081.198623	19.025754
51.080280	2076.878434	19.030771
50.925028	2084.093829	19.035789
50.897413	2081.037858	19.040807
51.429483	2093.004214	19.045824
51.243972	2096.690836	19.050842
51.098414	2101.361302	19.055859
51.393510	2101.345322	19.060877
51.441888	2110.182352	19.065895
51.387630	2092.688332	19.070912
51.225525	2101.336216	19.075930
51.608843	2096.443787	19.080947
51.598892	2097.624366	19.085965
51.302650	2098.106679	19.090983
52.064784	2097.215235	19.096000
51.700695	2104.141596	19.101018
51.889098	2100.240201	19.106035
51.567161	2100.826147	19.111053
51.674912	2095.924264	19.116071
52.326747	2103.801011	19.121088
52.042096	2102.381066	19.126106
52.183749	2102.519759	19.131123
52.277213	2105.843546	19.136141
52.155043	2106.395242	19.141159
52.068661	2094.588644	19.146176
51.880365	2097.059822	19.151194
52.268573	2089.872529	19.156211
52.434203	2093.951767	19.161229
51.990460	2095.648515	19.166247
52.268068	2106.793033	19.171264
52.041904	2115.186515	19.176282
52.268282	2120.540568	19.181299
52.466807	2124.952018	19.186317
52.619847	2133.086766	19.191335
52.934351	2126.998077	19.196352
52.924271	2129.652909	19.201370
53.107000	2116.453503	19.206387
53.025495	2128.255755	19.211405
52.536743	2126.559733	19.216423
52.838584	2119.843993	19.221440
52.588094	2126.105124	19.226458
52.709402	2124.153302	19.231475
52.984153	2123.968345	19.236493
52.818123	2123.061207	19.241511
53.154436	2117.966564	19.246528
53.676721	2143.011327	19.251546
53.082168	2123.448175	19.256563
53.342013	2122.838153	19.261581
53.292558	2139.930172	19.266599
53.631328	2139.103438	19.271616
53.827515	2142.586812	19.276634
53.365007	2118.699614	19.281651
53.641105	2121.110076	19.286669
53.427051	2123.456522	19.291687
53.524157	2123.500476	19.296704
53.385137	2135.359845	19.301722
53.583690	2144.844473	19.306739
53.466949	2147.875916	19.311757
53.647941	2152.010024	19.316775
53.866070	2140.302385	19.321792
53.798644	2146.913296	19.326810
53.665289	2143.316699	19.331827
53.893553	2141.821410	19.336845
54.038702	2152.165716	19.341863
54.255395	2167.404783	19.346880
54.328612	2178.078021	19.351898
54.422969	2173.658795	19.356915
54.685506	2166.576491	19.361933
54.454371	2155.333327	19.366951
54.526169	2137.794806	19.371968
54.474652	2134.681890	19.376986
54.341751	2128.159599	19.382003
54.531658	2139.561731	19.387021
54.274946	2166.911275	19.392039
54.500273	2167.309678	19.397056
54.742240	2170.141808	19.402074
55.187538	2169.944936	19.407091
55.020574	2165.656356	19.412109
54.801973	2169.137613	19.417127
54.922810	2159.113029	19.422144
54.500836	2170.961874	19.427162
54.856344	2173.380779	19.432179
55.175479	2165.876112	19.437197
54.815081	2163.204395	19.442215
54.738451	2165.383170	19.447232
55.064754	2169.867227	19.452250
55.274449	2182.926873	19.457267
55.409213	2186.636568	19.462285
55.052963	2198.933290	19.467303
55.621072	2186.356831	19.472320
55.213948	2185.769807	19.477338
55.252077	2186.967349	19.482355
55.577398	2183.992994	19.487373
55.165224	2199.527342	19.492391
55.507886	2187.054899	19.497408
55.703110	2199.670517	19.502426
55.462069	2213.020885	19.507443
55.796842	2211.705783	19.512461
55.921199	2215.524373	19.517479
56.103376	2207.799036	19.522496
55.978106	2211.606872	19.527514
56.092612	2207.021166	19.532531
56.706960	2213.237219	19.537549
56.607243	2212.842407	19.542567
56.560516	2212.855896	19.547584
56.440966	2212.309343	19.552602
56.569872	2210.356208	19.557619
56.858340	2185.242350	19.562637
56.715472	2185.670019	19.567655
56.779438	2180.798454	19.572672
56.570591	2172.374709	19.577690
56.511535	2171.414577	19.582707
56.861535	2172.916968	19.587725
56.564010	2172.933293	19.592743
56.585853	2164.930698	19.597760
56.635059	2172.516256	19.602778
56.703708	2179.565336	19.607795
56.751048	2197.808711	19.612813
56.259182	2208.164619	19.617831
56.436293	2197.410569	19.622848
56.290031	2201.223577	19.627866
56.406124	2221.878389	19.632883
57.084687	2232.271472	19.637901
56.811621	2241.888208	19.642919
56.879960	2234.227265	19.647936
56.807398	2234.714545	19.652954
57.062380	2258.899674	19.657971
57.432149	2265.447490	19.662989
57.191947	2277.043169	19.668007
57.461426	2267.438768	19.673024
57.261305	2267.044632	19.678042
57.237543	2268.056699	19.683059
57.867398	2278.588893	19.688077
58.204391	2284.783226	19.693095
57.981364	2279.942722	19.698112
57.860195	2265.707726	19.703130
57.661434	2261.973474	19.708147
57.991499	2276.586818	19.713165
57.866596	2291.501049	19.718183
58.069865	2290.173049	19.723200
57.993866	2285.639670	19.728218
57.533492	2299.729400	19.733235
57.919603	2287.430559	19.738253
58.159702	2300.770174	19.743271
58.378617	2295.871220	19.748288
58.033631	2316.820204	19.753306
58.388839	2324.338408	19.758323
58.885059	2324.502941	19.763341
58.887233	2321.374483	19.768359
58.460766	2316.046719	19.773376
59.213294	2311.701255	19.778394
58.916766	2316.272451	19.783411
59.418482	2314.184508	19.788429
59.272855	2312.558001	19.793447
59.126852	2304.947948	19.798464
59.380174	2286.591401	19.803482
59.132500	2282.018943	19.808499
59.142596	2276.154855	19.813517
58.870444	2283.104907	19.818535
59.213249	2295.995346	19.823552
59.402158	2302.525360	19.828570
59.146758	2309.659194	19.833587
59.112443	2315.795134	19.838605
59.217221	2314.926608	19.843623
59.371095	2317.651014	19.848640
59.199263	2313.860944	19.853658
58.966335	2316.830437	19.858675
59.298515	2308.906077	19.863693
59.181400	2334.550613	19.868711
59.505889	2331.889021	19.873728
59.738282	2339.010114	19.878746
59.768997	2336.582383	19.883763
59.992963	2327.868565	19.888781
59.913215	2336.844244	19.893799
59.817810	2331.191956	19.898816
60.088517	2328.042657	19.903834
60.188874	2342.342634	19.908851
60.422613	2346.948141	19.913869
60.265975	2342.027721	19.918887
60.740853	2354.560867	19.923904
60.725902	2339.826413	19.928922
60.423080	2327.883492	19.933939
60.751958	2324.647042	19.938957
60.643038	2326.368311	19.943975
60.440521	2328.000099	19.948992
60.586668	2337.480441	19.954010
60.503097	2365.192832	19.959027
61.091168	2356.275606	19.964045
60.896566	2363.492757	19.969063
60.971121	2365.751167	19.974080
60.995134	2360.534372	19.979098
61.186002	2361.063119	19.984115
61.322159	2355.318356	19.989133
61.108100	2353.662626	19.994151
60.900057	2363.028091	19.999168
61.568543	2359.793261	20.004186
61.561838	2364.363607	20.009203
61.774184	2357.919057	20.014221
61.124146	2353.346261	20.019239
61.110054	2355.527728	20.024256
61.009234	2358.238320	20.029274
61.224317	2360.109586	20.034291
61.331802	2369.204388	20.039309
61.372586	2380.443257	20.044327
61.577337	2379.433945	20.049344
62.006932	2378.926327	20.054362
61.583095	2386.860065	20.059379
61.512836	2382.416240	20.064397
61.268861	2400.999608	20.069415
61.470039	2412.754396	20.074432
61.700940	2420.063213	20.079450
61.806869	2432.154083	20.084467
62.013474	2439.841940	20.089485
62.332089	2445.769365	20.094503
62.229617	2450.662505	20.099520
62.776891	2450.993119	20.104538
62.616313	2449.322697	20.109555
62.810469	2443.753815	20.114573
62.508071	2446.662789	20.119591
62.480229	2450.501230	20.124608
62.824090	2437.833077	20.129626
62.687917	2445.687598	20.134643
62.828775	2446.404479	20.139661
63.251324	2440.917720	20.144679
63.056256	2441.804813	20.149696
63.090699	2435.326942	20.154714
62.990943	2441.218991	20.159731
63.224411	2437.929574	20.164749
63.168485	2435.899422	20.169767
62.886623	2441.569895	20.174784
63.229349	2438.294035	20.179802
63.290802	2436.754866	20.184819
63.106723	2445.282276	20.189837
63.663644	2458.487379	20.194855
63.749248	2463.343553	20.199872
64.066898	2465.143694	20.204890
63.220116	2464.939175	20.209907
63.770068	2462.974461	20.214925
63.458148	2465.287334	20.219943
63.667964	2466.994923	20.224960
63.868076	2464.068759	20.229978
63.809270	2468.957569	20.234995
63.801186	2470.504846	20.240013
64.027968	2468.399443	20.245031
63.780225	2473.828606	20.250048
63.951493	2479.130804	20.255066
64.042626	2495.424174	20.260083
64.082491	2490.159728	20.265101
64.457456	2498.926022	20.270119
64.413209	2500.452725	20.275136
64.222270	2488.210925	20.280154
64.436277	2509.456516	20.285171
64.520748	2514.431818	20.290189
64.541079	2521.027052	20.295207
64.646486	2523.045510	20.300224
65.130154	2521.001588	20.305242
64.821777	2531.526281	20.310259
65.014517	2522.353064	20.315277
64.915709	2535.595053	20.320295
64.874890	2527.613254	20.325312
65.086049	2522.014654	20.330330
64.832873	2527.045486	20.335347
64.643715	2540.069859	20.340365
65.207377	2554.415027	20.345383
65.207298	2551.023084	20.350400
65.622443	2554.046104	20.355418
65.394928	2551.517706	20.360435
66.035371	2548.609749	20.365453
65.802968	2545.814428	20.370471
65.850639	2550.297540	20.375488
66.141465	2546.083937	20.380506
65.939351	2556.204535	20.385523
65.736550	2552.983593	20.390541
65.949984	2549.532205	20.395559
66.141384	2544.469359	20.400576
66.381234	2547.976840	20.405594
66.013487	2553.528197	20.410611
65.886215	2554.924234	20.415629
66.069975	2550.410822	20.420647
65.729087	2562.728818	20.425664
66.207213	2574.361428	20.430682
66.116933	2581.392259	20.435699
66.420521	2583.572057	20.440717
66.108279	2580.452564	20.445735
65.975194	2590.495984	20.450752
66.452864	2602.020800	20.455770
66.336630	2616.095910	20.460787
66.744224	2613.145173	20.465805
67.236089	2607.481089	20.470823
67.245838	2608.375602	20.475840
67.184960	2609.531087	20.480858
67.104155	2598.369723	20.485875
66.902662	2600.357330	20.490893
67.066042	2602.912411	20.495911
67.009068	2610.936145	20.500928
67.204291	2619.260011	20.505946
67.186525	2633.238713	20.510963
67.167670	2637.201666	20.515981
67.666341	2634.171518	20.520999
67.139719	2634.976071	20.526016
67.491299	2629.006052	20.531034
67.787650	2624.894649	20.536051
67.752106	2630.811986	20.541069
67.870151	2632.383332	20.546087
67.965989	2647.624686	20.551104
68.184200	2653.878908	20.556122
68.373389	2653.608599	20.561139
68.112188	2662.001290	20.566157
68.516334	2655.811976	20.571175
68.085565	2655.046275	20.576192
68.518214	2652.653539	20.581210
68.694686	2652.954016	20.586227
68.612589	2652.698716	20.591245
69.018376	2644.025218	20.596263
68.814640	2649.246073	20.601280
68.739575	2644.249356	20.606298
68.818835	2643.699416	20.611315
68.543504	2650.328069	20.616333
68.947031	2646.836194	20.621351
68.866880	2649.704738	20.626368
69.079001	2648.728798	20.631386
68.892660	2652.044759	20.636403
69.039599	2649.150516	20.641421
69.334501	2640.526745	20.646439
68.843583	2648.753267	20.651456
68.929181	2647.070543	20.656474
68.882580	2653.120516	20.661491
69.033688	2671.237183	20.666509
69.292704	2674.317709	20.671527
68.959538	2689.787801	20.676544
69.097060	2686.139913	20.681562
69.575024	2692.919011	20.686579
69.650983	2700.248224	20.691597
69.945626	2708.958315	20.696615
69.754138	2708.404389	20.701632
70.040956	2715.068998	20.706650
70.075139	2710.904078	20.711667
69.855042	2709.271395	20.716685
70.240227	2703.530275	20.721703
70.141681	2704.385870	20.726720
70.360165	2701.121807	20.731738
70.764087	2707.744284	20.736755
70.374086	2701.613927	20.741773
70.736170	2704.348382	20.746791
70.105689	2714.038496	20.751808
70.452572	2709.599452	20.756826
70.482616	2721.455479	20.761843
70.554500	2735.757546	20.766861
70.923765	2738.959366	20.771879
70.783068	2744.868785	20.776896
70.733048	2731.009429	20.781914
71.338546	2741.127140	20.786931
71.440390	2737.044330	20.791949
71.387079	2723.854958	20.796967
71.541236	2728.886109	20.801984
71.648223	2730.913774	20.807002
71.446454	2725.000788	20.812019
71.549037	2732.582979	20.817037
71.538405	2729.679510	20.822055
71.343165	2729.695622	20.827072
71.157062	2728.332751	20.832090
71.513032	2735.378497	20.837107
71.411185	2753.218883	20.842125
71.802938	2745.842463	20.847143
71.581258	2752.038260	20.852160
71.931292	2754.336915	20.857178
72.007128	2756.578624	20.862195
71.715097	2757.179939	20.867213
72.104711	2773.980007	20.872231
71.957927	2794.545972	20.877248
71.854845	2795.878816	20.882266
72.320463	2789.253634	20.887283
72.429870	2787.936174	20.892301
72.834063	2781.850758	20.897319
72.716940	2784.961143	20.902336
72.768900	2788.701717	20.907354
73.087146	2783.712340	20.912371
72.694904	2777.133435	20.917389
72.866815	2774.442802	20.922407
72.671772	2786.462688	20.927424
73.110623	2792.268825	20.932442
73.452245	2803.961238	20.937459
73.358165	2807.155882	20.942477
73.403994	2797.972253	20.947495
73.481539	2813.608316	20.952512
73.659528	2803.467992	20.957530
73.900032	2795.614235	20.962547
73.666451	2795.706225	20.967565
73.705090	2774.562554	20.972583
73.441508	2775.842584	20.977600
73.675344	2783.685814	20.982618
74.106483	2786.158792	20.987635
74.080525	2792.573065	20.992653
74.161476	2788.985255	20.997671
73.930060	2791.709648	21.002688
73.914892	2794.719074	21.007706
74.537109	2794.865165	21.012723
74.429764	2803.135472	21.017741
74.327403	2797.462156	21.022759
74.147479	2798.397074	21.027776
74.025692	2793.550866	21.032794
74.126591	2795.856801	21.037811
74.135080	2800.419157	21.042829
74.440716	2817.257296	21.047847
74.443838	2827.394859	21.052864
74.538052	2827.203834	21.057882
74.777898	2828.178618	21.062899
74.662589	2827.420252	21.067917
74.709204	2828.392725	21.072935
74.975557	2848.817838	21.077952
74.940434	2850.898235	21.082970
75.241516	2855.301760	21.087987
75.114514	2860.272475	21.093005
75.480556	2853.350106	21.098023
74.927979	2861.000581	21.103040
74.999409	2861.452167	21.108058
75.448097	2880.491471	21.113075
75.468117	2886.280457	21.118093
76.007928	2884.719873	21.123111
75.998287	2877.598072	21.128128
75.751416	2879.123324	21.133146
76.198094	2883.791715	21.138163
76.187054	2878.468925	21.143181
76.157193	2883.924665	21.148199
76.165117	2881.673231	21.153216
76.068842	2877.163634	21.158234
76.750046	2873.127945	21.163251
76.413041	2878.892296	21.168269
76.352850	2872.929779	21.173287
76.129640	2883.672433	21.178304
76.428383	2897.054481	21.183322
76.821195	2904.711430	21.188339
76.703381	2910.143668	21.193357
77.007632	2904.474631	21.198375
76.770592	2904.527836	21.203392
76.834185	2909.343031	21.208410
77.242047	2894.517454	21.213427
76.886857	2898.107343	21.218445
76.876564	2891.014787	21.223463
77.304143	2905.126868	21.228480
77.174489	2923.384105	21.233498
77.710849	2928.497854	21.238515
77.575909	2941.018677	21.243533
77.631577	2931.952204	21.248551
77.622958	2934.628186	21.253568
77.389726	2938.338935	21.258586
77.673190	2934.281641	21.263603
77.687250	2931.203002	21.268621
78.231500	2934.114182	21.273639
78.099501	2927.636293	21.278656
77.988908	2927.719010	21.283674
78.310305	2929.955659	21.288691
78.015263	2925.513990	21.293709
78.592599	2924.803830	21.298727
78.421871	2922.826374	21.303744
78.389971	2939.042066	21.308762
78.665875	2942.766334	21.313779
78.552499	2956.495522	21.318797
78.820789	2957.213419	21.323815
78.866892	2947.616188	21.328832
79.143057	2955.581407	21.333850
79.065943	2944.252202	21.338867
79.196163	2953.918362	21.343885
79.522282	2945.967159	21.348903
79.613352	2938.398846	21.353920
79.563326	2937.488309	21.358938
79.804080	2935.501734	21.363955
79.203124	2925.976862	21.368973
78.915853	2930.853793	21.373991
79.507342	2927.243002	21.379008
79.066567	2929.129913	21.384026
79.381290	2933.812279	21.389043
79.658278	2947.883275	21.394061
79.399469	2958.538363	21.399079
79.958179	2964.799701	21.404096
79.540224	2959.759288	21.409114
80.130003	2961.137957	21.414131
79.745938	2963.082092	21.419149
79.949472	2977.693371	21.424167
80.116219	2986.194790	21.429184
79.997815	2996.992008	21.434202
80.368380	2988.984335	21.439219
80.327547	2996.679449	21.444237
80.671969	2990.727061	21.449255
80.393637	2990.526663	21.454272
80.329459	3012.177395	21.459290
80.725453	3014.546965	21.464307
80.990017	3029.386459	21.469325
80.844417	3025.133358	21.474343
80.654407	3025.358063	21.479360
80.571947	3029.480081	21.484378
81.077217	3039.844351	21.489395
81.072984	3056.012104	21.494413
81.147127	3052.197009	21.499431
81.516844	3055.227917	21.504448
81.214433	3055.549075	21.509466
81.747225	3049.627374	21.514483
81.385136	3056.625474	21.519501
81.860369	3045.699237	21.524519
81.879896	3051.278878	21.529536
82.006937	3073.914440	21.534554
82.019934	3073.724736	21.539571
82.090895	3068.977708	21.544589
82.471724	3075.312903	21.549607
82.745197	3069.626245	21.554624
82.749005	3078.404520	21.559642
82.704659	3065.850461	21.564659
82.663291	3048.784749	21.569677
82.376031	3054.274439	21.574695
82.620468	3057.900960	21.579712
82.632669	3060.196938	21.584730
82.838858	3068.393154	21.589747
82.694520	3068.458030	21.594765
82.657804	3080.303722	21.599783
82.984180	3070.855255	21.604800
82.628728	3072.586581	21.609818
82.985755	3075.670861	21.614835
83.055493	3088.918284	21.619853
83.050223	3092.434048	21.624871
83.201686	3085.580656	21.629888
83.454407	3098.232033	21.634906
83.465471	3091.862646	21.639923
83.727342	3107.112997	21.644941
83.603821	3126.618496	21.649959
83.966991	3120.558099	21.654976
83.886235	3132.643712	21.659994
84.045170	3125.338534	21.665011
84.242918	3127.148286	21.670029
83.884964	3129.151757	21.675047
84.101210	3122.113978	21.680064
84.056065	3132.823910	21.685082
84.840716	3141.032824	21.690099
84.419490	3154.673201	21.695117
84.252192	3163.951824	21.700135
84.723826	3152.737093	21.705152
84.679758	3161.177880	21.710170
84.528026	3162.053643	21.715187
84.393810	3152.694333	21.720205
84.585419	3161.089989	21.725223
85.296047	3176.293397	21.730240
85.142543	3182.731270	21.735258
85.826526	3179.175447	21.740275
85.676841	3174.552060	21.745293
85.471194	3185.836118	21.750311
85.559225	3179.681107	21.755328
85.559601	3174.001067	21.760346
85.838673	3169.428610	21.765363
86.077433	3172.552874	21.770381
85.839022	3165.872611	21.775399
86.547300	3164.987205	21.780416
86.301713	3165.663265	21.785434
86.257767	3156.496394	21.790451
86.471769	3146.630836	21.795469
85.961996	3141.795121	21.800487
86.647937	3149.661833	21.805504
86.229005	3155.504910	21.810522
86.135580	3163.450905	21.815539
86.549032	3168.318033	21.820557
86.136037	3164.687237	21.825575
86.471304	3158.079525	21.830592
86.400829	3173.765739	21.835610
86.248177	3187.701116	21.840627
86.465591	3191.683556	21.845645
86.435583	3195.602095	21.850663
86.741311	3208.338981	21.855680
86.916066	3217.022656	21.860698
87.169726	3226.982849	21.865715
87.656214	3228.116205	21.870733
87.300275	3213.469320	21.875751
87.446547	3216.404682	21.880768
87.620638	3223.058907	21.885786
87.380082	3237.845799	21.890803
87.627494	3244.806429	21.895821
87.793299	3250.750909	21.900839
87.805170	3244.436453	21.905856
88.240152	3246.737158	21.910874
88.229534	3253.879855	21.915891
88.369234	3245.835239	21.920909
87.774578	3250.532633	21.925927
88.552878	3255.444348	21.930944
88.913618	3275.616776	21.935962
88.852334	3280.252663	21.940979
88.846462	3273.652198	21.945997
88.613656	3271.579805	21.951015
88.626139	3271.531163	21.956032
88.811925	3280.605193	21.961050
88.444223	3272.750727	21.966067
89.073763	3275.307120	21.971085
88.704813	3283.245282	21.976103
89.394273	3289.633974	21.981120
88.823632	3308.923377	21.986138
89.260889	3310.178590	21.991155
89.534510	3301.087139	21.996173
89.255067	3309.580173	22.001191
89.430752	3309.827243	22.006208
89.569737	3325.884086	22.011226
89.599642	3338.116275	22.016243
89.729826	3331.546015	22.021261
89.936600	3337.912733	22.026279
90.147357	3331.530278	22.031296
90.156378	3333.051080	22.036314
90.200033	3355.456408	22.041331
90.542396	3362.722930	22.046349
90.240511	3372.132647	22.051367
90.633029	3364.142287	22.056384
90.651891	3362.259858	22.061402
90.855517	3366.044662	22.066419
91.378987	3360.708041	22.071437
91.041612	3361.235242	22.076455
90.962836	3354.813420	22.081472
90.992406	3364.357688	22.086490
91.135751	3364.060575	22.091507
91.157609	3356.519678	22.096525
91.147571	3361.665030	22.101543
91.328930	3361.628388	22.106560
91.431750	3383.415603	22.111578
91.244780	3392.762313	22.116595
91.534829	3387.394032	22.121613
91.418394	3397.594201	22.126631
91.684308	3397.309153	22.131648
91.626868	3394.999545	22.136666
91.881090	3411.629766	22.141683
92.412236	3414.646458	22.146701
92.285816	3423.032985	22.151719
92.410740	3415.645295	22.156736
92.611009	3413.651426	22.161754
92.308935	3418.227038	22.166771
92.375765	3411.274604	22.171789
92.542973	3418.297104	22.176807
92.671598	3420.165996	22.181824
92.912072	3442.925982	22.186842
92.538749	3442.133849	22.191859
92.486714	3437.869320	22.196877
92.623857	3447.450325	22.201895
92.945652	3450.086286	22.206912
93.379275	3456.382658	22.211930
93.355404	3462.348711	22.216947
93.695326	3463.734037	22.221965
93.630080	3466.217408	22.226983
93.882964	3462.025034	22.232000
94.064345	3464.358224	22.237018
93.952437	3463.380295	22.242035
94.248062	3457.402233	22.247053
94.002891	3460.948183	22.252071
94.097099	3447.036690	22.257088
94.229829	3454.995252	22.262106
94.374953	3466.552519	22.267123
94.461699	3480.411670	22.272141
94.356166	3497.424993	22.277159
94.708466	3489.489508	22.282176
94.727748	3488.729299	22.287194
94.635622	3490.384807	22.292211
94.669399	3484.444539	22.297229
94.792778	3491.228860	22.302247
94.922287	3481.691825	22.307264
94.890761	3496.538419	22.312282
94.952892	3508.374574	22.317299
95.170757	3507.375547	22.322317
94.959143	3517.614164	22.327335
95.095218	3510.755350	22.332352
95.072640	3518.437350	22.337370
94.997711	3539.588169	22.342387
95.722434	3544.213030	22.347405
95.865913	3542.759715	22.352423
95.770884	3552.489276	22.357440
96.062021	3549.319696	22.362458
96.087316	3554.314137	22.367475
96.355280	3567.555544	22.372493
96.111180	3576.186789	22.377511
96.437785	3573.462411	22.382528
97.028402	3562.633389	22.387546
96.917048	3562.413018	22.392563
97.011479	3560.474293	22.397581
97.070844	3566.592296	22.402599
97.222402	3566.486731	22.407616
97.255692	3560.966302	22.412634
96.874040	3567.985306	22.417651
97.426292	3562.861058	22.422669
97.431227	3566.738257	22.427687
97.028996	3567.375031	22.432704
96.898844	3560.951694	22.437722
97.165834	3582.065216	22.442739
97.348695	3591.751097	22.447757
97.482352	3604.702101	22.452775
97.444769	3601.873187	22.457792
97.645088	3596.456425	22.462810
97.488597	3619.231166	22.467827
97.635239	3630.409463	22.472845
97.375608	3637.635192	22.477863
97.638654	3640.589993	22.482880
98.278734	3650.245567	22.487898
98.600271	3663.838587	22.492915
98.917510	3655.812944	22.497933
99.006499	3652.370840	22.502951
99.126773	3654.274271	22.507968
99.072616	3646.027197	22.512986
98.889993	3652.771114	22.518003
98.949799	3647.354796	22.523021
99.186783	3661.350593	22.528039
99.190344	3674.820142	22.533056
99.357210	3676.297376	22.538074
99.129226	3686.077379	22.543091
99.595761	3680.254230	22.548109
99.484316	3672.495820	22.553127
99.542090	3678.788198	22.558144
99.897768	3690.205570	22.563162
99.897604	3707.881536	22.568179
100.373295	3707.688108	22.573197
100.030013	3709.785220	22.578215
99.929851	3706.188873	22.583232
100.737296	3694.039598	22.588250
100.925246	3692.984255	22.593267
101.281795	3689.819186	22.598285
101.135447	3687.310552	22.603303
100.887122	3688.906224	22.608320
101.056160	3678.782625	22.613338
100.947138	3687.811347	22.618355
100.977137	3677.528077	22.623373
101.122190	3688.401889	22.628391
100.930250	3684.644072	22.633408
101.412377	3685.253675	22.638426
101.050366	3690.471290	22.643443
101.293584	3675.685811	22.648461
101.454372	3694.365915	22.653479
101.231425	3712.814118	22.658496
101.571085	3713.021270	22.663514
101.776592	3713.976009	22.668531
101.814942	3711.340407	22.673549
101.761619	3730.120269	22.678567
101.686305	3739.862316	22.683584
102.045549	3746.842590	22.688602
102.074672	3747.636184	22.693619
102.227181	3755.047278	22.698637
102.408032	3774.499820	22.703655
102.474781	3783.659920	22.708672
102.863887	3779.601628	22.713690
102.901291	3781.436585	22.718707
102.851682	3777.326704	22.723725
102.896018	3792.952894	22.728743
103.181918	3794.700357	22.733760
103.784768	3801.335665	22.738778
103.821169	3813.481261	22.743795
103.594581	3812.344973	22.748813
104.063594	3804.703574	22.753831
103.923701	3808.395372	22.758848
103.829382	3804.255345	22.763866
104.003250	3806.797801	22.768883
104.225461	3794.436893	22.773901
104.191583	3802.935346	22.778919
104.209533	3804.194755	22.783936
104.136487	3798.832666	22.788954
103.951503	3803.870324	22.793971
104.211512	3805.527714	22.798989
104.683227	3821.287802	22.804007
104.433558	3833.063454	22.809024
104.726165	3830.246412	22.814042
104.488631	3836.902946	22.819059
104.772189	3833.251811	22.824077
104.312729	3848.165013	22.829095
104.333423	3857.415750	22.834112
104.595909	3864.272471	22.839130
104.738486	3890.092394	22.844147
104.911703	3892.345925	22.849165
104.977883	3905.565504	22.854183
105.517905	3915.496730	22.859200
105.586500	3914.347633	22.864218
105.558894	3923.093171	22.869235
105.922554	3929.148908	22.874253
106.723670	3930.147256	22.879271
106.501006	3942.401949	22.884288
106.707697	3935.018114	22.889306
106.680850	3920.715040	22.894323
106.967682	3910.990104	22.899341
107.188121	3906.913441	22.904359
106.801921	3902.248476	22.909376
106.820323	3892.913754	22.914394
107.026894	3908.411432	22.919411
107.145809	3915.737786	22.924429
107.443481	3919.321515	22.929447
107.226168	3930.338741	22.934464
107.583468	3923.658414	22.939482
107.694013	3930.560903	22.944499
107.373233	3927.315008	22.949517
107.586072	3927.082369	22.954535
107.552179	3930.327566	22.959552
107.467647	3929.736353	22.964570
107.691444	3949.825223	22.969587
107.894512	3960.241916	22.974605
108.614307	3956.751459	22.979623
108.219913	3960.820870	22.984640
108.654672	3952.348047	22.989658
108.317019	3962.515621	22.994675
108.568336	3961.369850	22.999693
108.851063	3976.410329	23.004711
108.772338	3989.719404	23.009728
109.075507	3985.137069	23.014746
108.859131	3993.774027	23.019763
108.987796	3985.211894	23.024781
108.993767	3983.522202	23.029799
109.183347	3998.712565	23.034816
109.504599	4011.490760	23.039834
109.711596	4013.879500	23.044851
109.434723	4017.310503	23.049869
109.837427	4015.691412	23.054887
110.048448	4020.295797	23.059904
109.825975	4016.748701	23.064922
109.728141	4033.594308	23.069939
110.154282	4032.910817	23.074957
110.075316	4041.308437	23.079975
109.809307	4049.538076	23.084992
110.313357	4054.211951	23.090010
110.454062	4076.322849	23.095027
110.310710	4088.923997	23.100045
110.485379	4087.866181	23.105063
110.459238	4092.153669	23.110080
110.941502	4103.145594	23.115098
110.983715	4110.323728	23.120115
111.079657	4114.739939	23.125133
111.311253	4105.116505	23.130151
111.751867	4129.505038	23.135168
111.851608	4127.366067	23.140186
112.374727	4120.902178	23.145203
112.335924	4107.927328	23.150221
112.635300	4097.592877	23.155239
112.170329	4093.011457	23.160256
112.254383	4082.350840	23.165274
112.364043	4094.914918	23.170291
112.064196	4089.669586	23.175309
112.635149	4094.969971	23.180327
112.172565	4118.101925	23.185344
112.649977	4110.398295	23.190362
112.858462	4119.330299	23.195379
112.473468	4123.687981	23.200397
112.509726	4125.023038	23.205415
113.004508	4140.075363	23.210432
112.991827	4147.785902	23.215450
113.180677	4148.263865	23.220467
113.261386	4144.431629	23.225485
113.726273	4152.832948	23.230503
113.603467	4169.147401	23.235520
114.021628	4172.417538	23.240538
114.082910	4171.804469	23.245555
113.892825	4177.362160	23.250573
114.230367	4175.862128	23.255591
113.871288	4176.596278	23.260608
113.881122	4174.649141	23.265626
113.926971	4194.861769	23.270643
113.962580	4203.895131	23.275661
114.664810	4213.790076	23.280679
114.501152	4235.572956	23.285696
114.591721	4235.985072	23.290714
114.560667	4244.037484	23.295731
114.796637	4243.299162	23.300749
115.182152	4250.800500	23.305767
115.070460	4264.659705	23.310784
115.564693	4256.099338	23.315802
115.711304	4260.156412	23.320819
115.334625	4258.140057	23.325837
115.701428	4278.648260	23.330855
115.707761	4295.752743	23.335872
115.806365	4287.987162	23.340890
115.707189	4288.957153	23.345907
115.748167	4306.001361	23.350925
116.248929	4319.201916	23.355943
116.083632	4320.926763	23.360960
116.266913	4322.335872	23.365978
116.580729	4339.048221	23.370995
116.943757	4352.971829	23.376013
117.334413	4345.496405	23.381031
117.341576	4344.399554	23.386048
117.451463	4342.399012	23.391066
117.739750	4339.607827	23.396083
117.958281	4338.125033	23.401101
118.014170	4334.334812	23.406119
117.936795	4335.361716	23.411136
118.313405	4331.908750	23.416154
118.449328	4333.300775	23.421171
118.101854	4344.091713	23.426189
118.317703	4336.762044	23.431207
118.199754	4338.678044	23.436224
118.373053	4335.712817	23.441242
118.189824	4334.551728	23.446259
118.018588	4331.365961	23.451277
117.955975	4324.572364	23.456295
118.290797	4352.782822	23.461312
118.508325	4362.090687	23.466330
118.569661	4368.591450	23.471347
118.295497	4390.914899	23.476365
118.789027	4397.501469	23.481383
119.055085	4404.575987	23.486400
118.772473	4428.347811	23.491418
118.992574	4425.447793	23.496435
119.218009	4444.676920	23.501453
119.703301	4447.922217	23.506471
119.614824	4458.416001	23.511488
119.674683	4462.839283	23.516506
120.246951	4465.228482	23.521523
120.463591	4488.035808	23.526541
120.561236	4483.323950	23.531559
120.435239	4490.399559	23.536576
120.587527	4497.851210	23.541594
120.824826	4483.762261	23.546611
120.744694	4499.034787	23.551629
120.559336	4497.419587	23.556647
120.780425	4506.133050	23.561664
120.840039	4516.843288	23.566682
121.315137	4515.400770	23.571699
121.203283	4533.656027	23.576717
121.441882	4545.733653	23.581735
121.505298	4547.647729	23.586752
121.669999	4557.713020	23.591770
122.202542	4553.161300	23.596787
122.034694	4565.456697	23.601805
122.144726	4573.632377	23.606823
122.359524	4585.325808	23.611840
122.446658	4588.229822	23.616858
122.758705	4578.706517	23.621875
122.467387	4583.529511	23.626893
122.762603	4590.395116	23.631911
122.844319	4588.720729	23.636928
122.562628	4610.609425	23.641946
123.044560	4613.046427	23.646963
122.983223	4620.621399	23.651981
122.776020	4620.608052	23.656999
123.345846	4640.461259	23.662016
123.468004	4642.413322	23.667034
123.755147	4644.888449	23.672051
123.847351	4645.546827	23.677069
123.893858	4649.421890	23.682087
123.945889	4673.221775	23.687104
124.071080	4680.330807	23.692122
124.292151	4680.926137	23.697139
124.120479	4679.029745	23.702157
124.499086	4681.523854	23.707175
124.937174	4683.417822	23.712192
126.507500	4649.305953	23.717210
127.098915	4629.113385	23.722227
126.718714	4619.445660	23.727245
126.733954	4595.879994	23.732263
126.497956	4569.949626	23.737280
126.555430	4546.178308	23.742298
126.315066	4540.130264	23.747315
126.063365	4548.544377	23.752333
126.495249	4536.504533	23.757351
126.444119	4533.249301	23.762368
126.471977	4523.017044	23.767386
126.204977	4508.890869	23.772403
126.253878	4524.485496	23.777421
126.253223	4528.520628	23.782439
126.350075	4532.370492	23.787456
126.445466	4542.589430	23.792474
126.440939	4548.335190	23.797491
126.523489	4576.252975	23.802509
126.869523	4572.794173	23.807527
126.722411	4580.042784	23.812544
126.888858	4593.226845	23.817562
127.346001	4605.744361	23.822579
126.770040	4615.641301	23.827597
127.064817	4622.543227	23.832615
127.350515	4638.726695	23.837632
127.204323	4662.165939	23.842650
127.449300	4678.020892	23.847667
127.375158	4677.820116	23.852685
127.330246	4691.839164	23.857703
127.633453	4710.589784	23.862720
127.477832	4727.531888	23.867738
128.183248	4729.009839	23.872755
128.239761	4744.263902	23.877773
128.678697	4760.074659	23.882791
129.091726	4763.184334	23.887808
129.078388	4777.164175	23.892826
129.174592	4768.888375	23.897843
129.196676	4780.995423	23.902861
129.240784	4788.666607	23.907879
129.499100	4792.949628	23.912896
129.833672	4800.793139	23.917914
130.000944	4797.064841	23.922931
129.816683	4819.669634	23.927949
130.058455	4822.802380	23.932967
130.166894	4829.722164	23.937984
129.880914	4835.390254	23.943002
130.492556	4844.678886	23.948019
130.420793	4866.608346	23.953037
130.629367	4861.851368	23.958055
130.740725	4874.099925	23.963072
130.540179	4877.574736	23.968090
130.820451	4891.598074	23.973107
131.046925	4901.765629	23.978125
130.820151	4905.332373	23.983143
131.457023	4916.523632	23.988160
131.476408	4927.125259	23.993178
131.576206	4927.634268	23.998195
131.590649	4941.566958	24.003213
131.835877	4951.457225	24.008231
132.801955	4952.094980	24.013248
132.408983	4961.436970	24.018266
132.959845	4958.435257	24.023283
132.736780	4957.497556	24.028301
132.651965	4958.115405	24.033319
132.809368	4961.832118	24.038336
132.683057	4960.576945	24.043354
133.140542	4969.403731	24.048371
133.240785	4983.308359	24.053389
133.631375	4982.385178	24.058407
133.972016	4982.164488	24.063424
133.408877	4983.310942	24.068442
133.618995	4978.617464	24.073459
134.102385	4979.852310	24.078477
133.642656	4989.140385	24.083495
134.037864	5003.923113	24.088512
133.692986	5009.134279	24.093530
134.110250	4999.771485	24.098547
134.431669	5025.958796	24.103565
135.062506	5033.525575	24.108583
135.085060	5030.533289	24.113600
134.912198	5044.811669	24.118618
135.440493	5038.765562	24.123635
135.169278	5038.036176	24.128653
135.625010	5043.293627	24.133671
135.472538	5051.457845	24.138688
135.624008	5067.365452	24.143706
135.400505	5068.524575	24.148723
135.712458	5070.849013	24.153741
135.920297	5074.409025	24.158759
136.092447	5092.076687	24.163776
135.962945	5112.118905	24.168794
135.880976	5106.025373	24.173811
135.969322	5121.013624	24.178829
136.398798	5132.963669	24.183847
136.471212	5140.436405	24.188864
136.298975	5150.247920	24.193882
136.295717	5157.428022	24.198899
136.526202	5169.524057	24.203917
137.138022	5170.744779	24.208935
137.307615	5180.457541	24.213952
137.588432	5177.685609	24.218970
137.742596	5185.995821	24.223987
138.026256	5196.822492	24.229005
138.349603	5204.594088	24.234023
138.573039	5194.439720	24.239040
138.743952	5197.198730	24.244058
139.146236	5191.205676	24.249075
138.802338	5193.158150	24.254093
139.063270	5190.942569	24.259111
139.405043	5184.066675	24.264128
139.098076	5197.050413	24.269146
139.000478	5192.092195	24.274163
139.214899	5189.202466	24.279181
139.074725	5195.195411	24.284199
139.267800	5187.079225	24.289216
139.403970	5218.338900	24.294234
139.376613	5221.584028	24.299251
139.666551	5227.539483	24.304269
139.580398	5238.173588	24.309287
139.813063	5249.851058	24.314304
139.682263	5267.699242	24.319322
140.306706	5271.874730	24.324339
140.523673	5286.714272	24.329357
140.263200	5294.318189	24.334375
140.418590	5294.219836	24.339392
140.790013	5309.731587	24.344410
141.211556	5310.538330	24.349427
141.274178	5321.340753	24.354445
141.254102	5311.954292	24.359463
141.417962	5330.839810	24.364480
141.333037	5348.885804	24.369498
141.814643	5351.418290	24.374515
141.942844	5347.752487	24.379533
142.019179	5357.441961	24.384551
142.123088	5368.680014	24.389568
142.447155	5382.405626	24.394586
142.451167	5379.529879	24.399603
142.759046	5377.176257	24.404621
142.627917	5401.435555	24.409639
142.926366	5399.779855	24.414656
142.907370	5410.660921	24.419674
143.198644	5411.883053	24.424691
143.377886	5410.343884	24.429709
143.331333	5431.481335	24.434727
143.706136	5436.126587	24.439744
143.566072	5446.904767	24.444762
143.696721	5444.807582	24.449779
143.964243	5459.157346	24.454797
143.942969	5467.254387	24.459815
144.294566	5462.296271	24.464832
144.312101	5478.581707	24.469850
144.608278	5492.204283	24.474867
145.124928	5489.137448	24.479885
144.931136	5503.938122	24.484903
145.355992	5491.745956	24.489920
145.442210	5490.941093	24.494938
145.515614	5484.769581	24.499955
145.874224	5499.888299	24.504973
146.158608	5517.633292	24.509991
146.096036	5509.641111	24.515008
146.211399	5515.038990	24.520026
146.059006	5521.151518	24.525043
146.508782	5508.298925	24.530061
146.478140	5515.241277	24.535079
146.626197	5511.553128	24.540096
146.464523	5513.020695	24.545114
146.635103	5511.499543	24.550131
146.829054	5519.655024	24.555149
146.957761	5541.289537	24.560167
147.446672	5540.933148	24.565184
147.297579	5543.481629	24.570202
147.425259	5552.922964	24.575219
147.552560	5554.622987	24.580237
147.505476	5573.047926	24.585255
147.614417	5578.744673	24.590272
147.916906	5582.972288	24.595290
147.911771	5582.923509	24.600307
147.927110	5593.903576	24.605325
148.001616	5607.008145	24.610343
148.182106	5614.616176	24.615360
148.797449	5630.868602	24.620378
148.671090	5633.665260	24.625395
149.021548	5638.443139	24.630413
149.223073	5653.833905	24.635431
149.559678	5657.537390	24.640448
149.481351	5662.702285	24.645466
149.529962	5662.441067	24.650483
149.694239	5669.357160	24.655501
150.003286	5694.191290	24.660519
150.191238	5694.974296	24.665536
150.449375	5695.100937	24.670554
150.389708	5690.059655	24.675571
150.628529	5704.903718	24.680589
150.838750	5717.514072	24.685607
151.067275	5717.261395	24.690624
150.954059	5722.684352	24.695642
150.996125	5727.064564	24.700659
151.186452	5724.090649	24.705677
151.138049	5746.431645	24.710695
151.494757	5756.616020	24.715712
151.655125	5759.703044	24.720730
151.314414	5779.971356	24.725747
152.018312	5784.701292	24.730765
152.103387	5790.269086	24.735783
152.159909	5800.247374	24.740800
152.195102	5819.357969	24.745818
152.342295	5817.146834	24.750835
152.616635	5828.542679	24.755853
152.448672	5854.400135	24.760871
152.816375	5848.568730	24.765888
153.143493	5865.698682	24.770906
153.071050	5872.019768	24.775923
153.800975	5878.415988	24.780941
153.581377	5880.817492	24.785959
153.599740	5874.424468	24.790976
153.989450	5899.368760	24.795994
153.779311	5916.697208	24.801011
154.330724	5900.015967	24.806029
154.017703	5904.863555	24.811047
154.418761	5916.611900	24.816064
154.718010	5926.567561	24.821082
155.027895	5922.805889	24.826099
156.336143	5898.946526	24.831117
156.494470	5901.935465	24.836135
156.545226	5895.229675	24.841152
156.703875	5875.666630	24.846170
156.141533	5867.175470	24.851187
156.602386	5862.683726	24.856205
157.018549	5863.706465	24.861223
156.765324	5858.212299	24.866240
156.718812	5858.018585	24.871258
156.922357	5855.973443	24.876275
156.680250	5860.814375	24.881293
156.645594	5856.568269	24.886311
156.777291	5861.213575	24.891328
157.223680	5869.203868	24.896346
156.683137	5892.596734	24.901363
157.055277	5898.285499	24.906381
157.015803	5915.249127	24.911399
157.040588	5930.464869	24.916416
157.555161	5933.001253	24.921434
157.093788	5958.594882	24.926451
157.400822	5962.518554	24.931469
157.553676	5976.200776	24.936487
157.712278	6005.796879	24.941504
157.994940	6018.667601	24.946522
157.985885	6041.986114	24.951539
158.181107	6043.439809	24.956557
158.263636	6063.422455	24.961575
158.635329	6080.506399	24.966592
158.844887	6097.974202	24.971610
158.892020	6103.795165	24.976627
159.455940	6115.355832	24.981645
159.467279	6126.961610	24.986663
159.276430	6139.356688	24.991680
160.032385	6159.120030	24.996698
159.989166	6166.407478	25.001715
160.299149	6171.787184	25.006733
160.232414	6188.801463	25.011751
160.441952	6191.913227	25.016768
160.612673	6204.909630	25.021786
160.772171	6220.362501	25.026803
161.422481	6216.484112	25.031821
161.493248	6241.179557	25.036839
161.612819	6251.092965	25.041856
161.983863	6255.899800	25.046874
161.763564	6255.030075	25.051891
162.180819	6248.181750	25.056909
162.508053	6268.682772	25.061927
162.433662	6283.225020	25.066944
162.897272	6279.219501	25.071962
162.765946	6282.170730	25.076979
162.987365	6275.918397	25.081997
162.719705	6281.728796	25.087015
163.203237	6280.956613	25.092032
163.210420	6285.587940	25.097050
163.252490	6301.799117	25.102067
163.807250	6303.597666	25.107085
163.734951	6302.498548	25.112103
163.525205	6321.772256	25.117120
164.026547	6329.036532	25.122138
163.765965	6344.266140	25.127155
163.826592	6347.712250	25.132173
163.960852	6368.148804	25.137191
164.302796	6375.162359	25.142208
164.475259	6397.838999	25.147226
164.549114	6409.064032	25.152243
165.151427	6425.644053	25.157261
165.143153	6436.267181	25.162279
165.179731	6436.015891	25.167296
165.538996	6444.611420	25.172314
165.805890	6470.200755	25.177331
166.401888	6467.413961	25.182349
166.509425	6460.546168	25.187367
166.253261	6471.155098	25.192384
166.690980	6480.008964	25.197402
166.546588	6494.917883	25.202419
166.954062	6486.119132	25.207437
167.112617	6497.253298	25.212455
167.119115	6523.390720	25.217472
167.466734	6531.408520	25.222490
167.181050	6534.455576	25.227507
167.465627	6536.774687	25.232525
167.713160	6555.726089	25.237543
167.550021	6554.425109	25.242560
167.886919	6570.054295	25.247578
167.768169	6589.282003	25.252595
168.303527	6599.713580	25.257613
167.918617	6619.582481	25.262631
167.990010	6635.180047	25.267648
168.600791	6653.820369	25.272666
168.500167	6669.409644	25.277683
168.933703	6670.859569	25.282701
169.456101	6675.187634	25.287719
169.598513	6698.152651	25.292736
170.017115	6703.525734	25.297754
169.862606	6716.008770	25.302771
170.190008	6711.653893	25.307789
170.429443	6726.092329	25.312807
170.590320	6738.669412	25.317824
170.963395	6734.673789	25.322842
170.900818	6741.865561	25.327859
170.825291	6752.368086	25.332877
171.753066	6762.608035	25.337895
171.570997	6772.554571	25.342912
171.674770	6775.073289	25.347930
172.065819	6779.984776	25.352947
172.024524	6773.960045	25.357965
172.199005	6772.323883	25.362983
171.570628	6780.654854	25.368000
172.143025	6797.349101	25.373018
172.325460	6813.403604	25.378035
172.357419	6806.881837	25.383053
172.402798	6823.521510	25.388071
172.147391	6843.362974	25.393088
172.699865	6852.668451	25.398106
172.785197	6877.371835	25.403123
173.068482	6887.739678	25.408141
173.276960	6907.353602	25.413159
173.010059	6921.582030	25.418176
173.565195	6939.970693	25.423194
173.636147	6954.321630	25.428211
173.905163	6968.400724	25.433229
174.032682	6975.719928	25.438247
173.982017	7001.160522	25.443264
174.523590	7007.961315	25.448282
174.740184	7038.307213	25.453299
175.010279	7035.085419	25.458317
175.765310	7034.769253	25.463335
176.117738	7054.079026	25.468352
176.124839	7052.279317	25.473370
176.621924	7055.816977	25.478387
176.706887	7055.178471	25.483405
177.044071	7052.333538	25.488423
177.126234	7049.061243	25.493440
177.349831	7039.218420	25.498458
177.117885	7047.650149	25.503475
176.981399	7050.726868	25.508493
177.397837	7042.935399	25.513511
177.183670	7055.451770	25.518528
177.482173	7070.597253	25.523546
177.547939	7087.212436	25.528563
177.699327	7092.271452	25.533581
177.776013	7108.011944	25.538599
177.853094	7112.759146	25.543616
178.023802	7129.803045	25.548634
178.094347	7148.772886	25.553651
178.331339	7160.532946	25.558669
179.015761	7175.914088	25.563687
178.594457	7187.085115	25.568704
178.901291	7204.164053	25.573722
178.893454	7226.278011	25.578739
179.015132	7243.732197	25.583757
179.592396	7253.408639	25.588775
179.696255	7265.400357	25.593792
179.795931	7283.249093	25.598810
180.163003	7294.615912	25.603827
180.103969	7310.186076	25.608845
180.458162	7323.478077	25.613863
181.059008	7324.457443	25.618880
181.653712	7305.324441	25.623898
181.910639	7298.722158	25.628915
181.971186	7301.338963	25.633933
182.135085	7290.805103	25.638951
182.173378	7296.437375	25.643968
182.459564	7290.919567	25.648986
182.495124	7298.934531	25.654003
182.497874	7316.202000	25.659021
182.776842	7317.784045	25.664039
182.735330	7328.872734	25.669056
182.795776	7320.610410	25.674074
182.956335	7330.170842	25.679092
182.782907	7339.959480	25.684109
183.326241	7350.692689	25.689127
182.928419	7365.287423	25.694144
183.159763	7383.697441	25.699162
183.764523	7389.157014	25.704180
183.637211	7407.270103	25.709197
183.915942	7419.288679	25.714215
184.016427	7436.875905	25.719232
184.144277	7458.097215	25.724250
184.433698	7466.873856	25.729268
184.597583	7487.070427	25.734285
184.786542	7492.463451	25.739303
184.822237	7513.706934	25.744320
185.157829	7523.213055	25.749338
185.505563	7536.551245	25.754356
185.397916	7556.691250	25.759373
185.759784	7555.812249	25.764391
185.649969	7585.952806	25.769408
186.052187	7593.182663	25.774426
186.030568	7614.430590	25.779444
186.417790	7629.031213	25.784461
187.021281	7641.867943	25.789479
186.949410	7655.456989	25.794496
187.421589	7651.683642	25.799514
187.768671	7660.259072	25.804532
187.977153	7676.057883	25.809549
188.420962	7676.092847	25.814567
188.512346	7670.691022	25.819584
188.980007	7661.455909	25.824602
189.322064	7656.861144	25.829620
189.005260	7660.625905	25.834637
189.381726	7672.022107	25.839655
189.501654	7688.782248	25.844672
189.937218	7692.199827	25.849690
190.288138	7695.608282	25.854708
190.223560	7698.144977	25.859725
190.316962	7694.165550	25.864743
190.221445	7693.364949	25.869760
190.195190	7692.850259	25.874778
190.254848	7700.816388	25.879796
190.294149	7726.834343	25.884813
190.692778	7724.165468	25.889831
190.604245	7736.611201	25.894848
190.647719	7749.588134	25.899866
191.032699	7748.410526	25.904884
190.963545	7767.636659	25.909901
191.361594	7779.442830	25.914919
191.627442	7790.371222	25.919936
191.723807	7815.647675	25.924954
191.762190	7818.429076	25.929972
192.075689	7830.084341	25.934989
192.202698	7849.712598	25.940007
192.403089	7863.066076	25.945024
192.623090	7882.210478	25.950042
193.118989	7891.137879	25.955060
192.823259	7898.785307	25.960077
193.349196	7915.297254	25.965095
193.385899	7929.419382	25.970112
193.527136	7957.236121	25.975130
193.697446	7960.834731	25.980148
193.588454	7980.607593	25.985165
194.198248	7993.209548	25.990183
194.504744	8021.082364	25.995200
194.593806	8034.236846	26.000218
194.977011	8037.521670	26.005236
194.849826	8055.271499	26.010253
194.930631	8060.468183	26.015271
195.226513	8075.635551	26.020288
195.190707	8090.231119	26.025306
195.795449	8109.057739	26.030324
195.961489	8121.529457	26.035341
196.247516	8136.119529	26.040359
196.007966	8158.911044	26.045376
196.309181	8166.642981	26.050394
197.068281	8183.498115	26.055412
197.063784	8199.113362	26.060429
197.364022	8212.325540	26.065447
197.499116	8225.947342	26.070464
197.904960	8228.525592	26.075482
197.910361	8240.339537	26.080500
198.113198	8257.514632	26.085517
198.591179	8255.712064	26.090535
198.499210	8277.515733	26.095552
198.883163	8288.956785	26.100570
198.957369	8289.760211	26.105588
198.870304	8304.612923	26.110605
199.228905	8319.922608	26.115623
199.381977	8333.495725	26.120640
199.641381	8354.687790	26.125658
200.080202	8355.128557	26.130676
200.050149	8372.201099	26.135693
200.631376	8371.347482	26.140711
200.272145	8389.144546	26.145728
200.261106	8392.761734	26.150746
201.558500	8387.155300	26.155764
201.771926	8407.966131	26.160781
202.043146	8393.826969	26.165799
202.577048	8396.875686	26.170816
202.429070	8395.582984	26.175834
202.646599	8395.144657	26.180852
202.517205	8403.117542	26.185869
202.868862	8390.896344	26.190887
203.052718	8392.698063	26.195904
202.809928	8391.118301	26.200922
203.205926	8394.720864	26.205940
202.888463	8413.358495	26.210957
203.085017	8420.710644	26.215975
203.236431	8427.524570	26.220992
203.266295	8447.694902	26.226010
203.243575	8453.496392	26.231028
203.712179	8479.038604	26.236045
203.898667	8479.891334	26.241063
204.189760	8508.418384	26.246080
204.172018	8523.950342	26.251098
204.610651	8533.332257	26.256116
204.703174	8555.166915	26.261133
204.789887	8565.492336	26.266151
205.278828	8584.537901	26.271168
205.386114	8602.237108	26.276186
205.879809	8611.363826	26.281204
205.886299	8624.407679	26.286221
206.195005	8629.131383	26.291239
206.421792	8652.578707	26.296256
206.432455	8662.018303	26.301274
206.741439	8674.960710	26.306292
206.937576	8698.625285	26.311309
207.394306	8710.506384	26.316327
207.432222	8725.675255	26.321344
207.591265	8728.613394	26.326362
207.814080	8743.687560	26.331380
208.002119	8766.028469	26.336397
208.270653	8771.489433	26.341415
208.660249	8780.013270	26.346432
208.604795	8798.943629	26.351450
208.969094	8806.293200	26.356468
209.161376	8820.608461	26.361485
209.445113	8830.707256	26.366503
209.648961	8837.094808	26.371520
209.938305	8841.417728	26.376538
210.443183	8851.054767	26.381556
210.507669	8868.352711	26.386573
211.033223	8868.256283	26.391591
211.151810	8863.401679	26.396608
211.379132	8866.536132	26.401626
211.888843	8849.502102	26.406644
212.332260	8858.223171	26.411661
212.412950	8865.046255	26.416679
212.269179	8863.603890	26.421696
212.636860	8869.678171	26.426714
212.848465	8867.199531	26.431732
212.616293	8878.459842	26.436749
213.086890	8881.508477	26.441767
213.147711	8867.094554	26.446784
213.061841	8878.687471	26.451802
213.759541	8869.688776	26.456820
213.322620	8892.396981	26.461837
213.611418	8898.675454	26.466855
213.718710	8906.458325	26.471872
213.508569	8913.926897	26.476890
213.763934	8940.633811	26.481908
213.975335	8952.219943	26.486925
214.324225	8972.058132	26.491943
214.576200	8979.750057	26.496960
214.566918	9002.456018	26.501978
214.678787	9008.744379	26.506996
215.081134	9024.681462	26.512013
215.036863	9038.183429	26.517031
215.273184	9060.957672	26.522048
215.354699	9083.167588	26.527066
216.063716	9090.305354	26.532084
215.762773	9122.745855	26.537101
216.421294	9140.496918	26.542119
216.382002	9153.011724	26.547136
216.367874	9174.582659	26.552154
217.242616	9200.302999	26.557172
217.822487	9200.633739	26.562189
217.621351	9216.523188	26.567207
218.107121	9223.316380	26.572224
218.316317	9238.253103	26.577242
218.697578	9255.922610	26.582260
218.424716	9268.680813	26.587277
218.876801	9286.528877	26.592295
219.262245	9297.221918	26.597312
219.016845	9309.638238	26.602330
219.526973	9323.518133	26.607348
219.693377	9337.234779	26.612365
219.710291	9344.722932	26.617383
220.047843	9362.083323	26.622400
219.824567	9376.164616	26.627418
220.469904	9386.245897	26.632436
220.536011	9404.773221	26.637453
220.487669	9435.796994	26.642471
221.233517	9451.144590	26.647488
220.884318	9472.711903	26.652506
221.537008	9485.893077	26.657524
221.832315	9502.167284	26.662541
222.192921	9509.237326	26.667559
222.518870	9531.229473	26.672576
222.319272	9542.541388	26.677594
222.828327	9545.425983	26.682612
222.747315	9576.044350	26.687629
222.888873	9583.103123	26.692647
223.061557	9594.987871	26.697664
223.314974	9619.230162	26.702682
223.592277	9612.562780	26.707700
224.221351	9643.306951	26.712717
224.971848	9657.555633	26.717735
225.484419	9661.203898	26.722752
224.973130	9664.101112	26.727770
225.323190	9663.327245	26.732788
225.451951	9670.744376	26.737805
226.606275	9653.786527	26.742823
227.321349	9643.660904	26.747840
227.422081	9625.248032	26.752858
227.382956	9609.512751	26.757876
228.001427	9603.398290	26.762893
228.523741	9579.661165	26.767911
228.799507	9558.218105	26.772928
228.828375	9546.475249	26.777946
228.951457	9531.949213	26.782964
229.049722	9518.554114	26.787981
228.967697	9506.075507	26.792999
229.081811	9499.377840	26.798016
228.899353	9495.427136	26.803034
229.196430	9499.440061	26.808052
229.162922	9501.747954	26.813069
229.049546	9503.018506	26.818087
229.415602	9509.211492	26.823104
229.314939	9533.449745	26.828122
229.353244	9530.762770	26.833140
229.093371	9550.529538	26.838157
229.312958	9571.178512	26.843175
229.793424	9599.975218	26.848192
229.721473	9613.022285	26.853210
229.792897	9636.136032	26.858228
230.065396	9668.914244	26.863245
230.244271	9693.664220	26.868263
230.295349	9711.135549	26.873280
230.374750	9749.036793	26.878298
230.790652	9773.768322	26.883316
231.186059	9807.319942	26.888333
231.523533	9836.351159	26.893351
231.994712	9855.395760	26.898368
232.170637	9890.058289	26.903386
232.223323	9901.095567	26.908404
232.573567	9933.816865	26.913421
232.859917	9947.215644	26.918439
233.003046	9966.464732	26.923456
233.663524	9991.272857	26.928474
233.667676	9997.624190	26.933492
234.063126	10010.485879	26.938509
234.381374	10030.266014	26.943527
234.453036	10046.304914	26.948544
234.471538	10063.547410	26.953562
235.091071	10087.217083	26.958580
235.016759	10106.716346	26.963597
235.467985	10129.773573	26.968615
235.911487	10136.861198	26.973632
235.666947	10158.496575	26.978650
236.040532	10184.978848	26.983668
236.537740	10192.919269	26.988685
236.447601	10216.882543	26.993703
236.674190	10231.736836	26.998720
236.847537	10256.556379	27.003738
237.184259	10262.910691	27.008756
237.733019	10287.768361	27.013773
237.727990	10297.953820	27.018791
238.282651	10309.553000	27.023808
238.345378	10330.655306	27.028826
238.382694	10344.347659	27.033844
238.675387	10355.030513	27.038861
238.873461	10364.943246	27.043879
239.659631	10382.190016	27.048896
240.050269	10386.688246	27.053914
240.112558	10393.256690	27.058932
240.629734	10412.234180	27.063949
240.657950	10430.917302	27.068967
240.958772	10430.567867	27.073984
241.197263	10445.155573	27.079002
241.180979	10457.356998	27.084020
241.587449	10470.026486	27.089037
241.437626	10486.193610	27.094055
241.785620	10490.360369	27.099072
241.870528	10510.332369	27.104090
241.932485	10530.842545	27.109108
242.146298	10539.471514	27.114125
242.400375	10568.359175	27.119143
242.743341	10586.708020	27.124160
242.314230	10607.709040	27.129178
242.221071	10631.764842	27.134196
243.171906	10655.660639	27.139213
243.107024	10681.824912	27.144231
243.493853	10705.543257	27.149248
243.720832	10732.781185	27.154266
244.109589	10757.260424	27.159284
245.013331	10771.419217	27.164301
245.023041	10795.106206	27.169319
245.558518	10800.136012	27.174336
245.577734	10822.377900	27.179354
246.231708	10828.323481	27.184372
246.498642	10837.901644	27.189389
246.784027	10871.196967	27.194407
247.350503	10866.862258	27.199424
247.432958	10868.316820	27.204442
247.208879	10889.322454	27.209460
247.424294	10906.732229	27.214477
247.388872	10921.372042	27.219495
247.534702	10927.751458	27.224512
247.796264	10956.190970	27.229530
247.844508	10966.448086	27.234548
248.573439	10988.576428	27.239565
248.724441	11004.238641	27.244583
249.235614	11025.792909	27.249600
249.554651	11038.504619	27.254618
249.462435	11052.008599	27.259636
250.136153	11073.494095	27.264653
250.266357	11076.196493	27.269671
250.824897	11088.862463	27.274688
250.910358	11097.764300	27.279706
250.664041	11113.102318	27.284724
251.373272	11108.465716	27.289741
251.215774	11128.569852	27.294759
251.802974	11125.972913	27.299776
251.908376	11144.498639	27.304794
251.762450	11154.428270	27.309812
252.066300	11164.720494	27.314829
252.615730	11195.519088	27.319847
252.498066	11205.661384	27.324864
252.603042	11227.392708	27.329882
252.863144	11246.218249	27.334900
253.045794	11269.769121	27.339917
252.849537	11291.003740	27.344935
253.255690	11311.076100	27.349952
253.565674	11338.155826	27.354970
253.896090	11365.635537	27.359988
254.306335	11386.551992	27.365005
254.261646	11416.512004	27.370023
254.870335	11437.208548	27.375040
255.446888	11462.282311	27.380058
255.029672	11486.171134	27.385076
255.542113	11506.474516	27.390093
255.736796	11532.756410	27.395111
255.848203	11556.745415	27.400128
256.257986	11581.888923	27.405146
256.500026	11618.811610	27.410164
257.136182	11627.980240	27.415181
257.297231	11643.951810	27.420199
257.740332	11667.895156	27.425216
257.654671	11679.458511	27.430234
258.011122	11709.421220	27.435252
258.917276	11714.761284	27.440269
259.103243	11738.736201	27.445287
259.144105	11745.305712	27.450304
259.691082	11753.459010	27.455322
259.922439	11771.538344	27.460340
260.264041	11785.129319	27.465357
260.807522	11811.224220	27.470375
260.980495	11811.374198	27.475392
261.387751	11818.766639	27.480410
261.126725	11827.889015	27.485428
261.205854	11844.954373	27.490445
260.912699	11855.240622	27.495463
261.212331	11885.388327	27.500480
261.899225	11913.223919	27.505498
262.027476	11928.498496	27.510516
262.455933	11942.651530	27.515533
262.516443	11963.129082	27.520551
262.834940	11983.417447	27.525568
263.336771	12000.315954	27.530586
263.441530	12019.986960	27.535604
264.025011	12035.889658	27.540621
263.994609	12048.680966	27.545639
264.009056	12056.235405	27.550656
264.615808	12084.080298	27.555674
264.500862	12101.932522	27.560692
264.919353	12108.156921	27.565709
265.167585	12128.678152	27.570727
265.471534	12152.138585	27.575744
265.956039	12152.901824	27.580762
265.817181	12182.822642	27.585780
266.173934	12188.036394	27.590797
266.158758	12210.557142	27.595815
266.540627	12229.235288	27.600832
266.812613	12250.888914	27.605850
266.904162	12277.139250	27.610868
267.466890	12300.186748	27.615885
267.630028	12317.326457	27.620903
267.960183	12335.328015	27.625920
268.191992	12349.220390	27.630938
268.222655	12380.846151	27.635956
269.069365	12391.057135	27.640973
269.042391	12418.973398	27.645991
269.214697	12440.625448	27.651008
269.508469	12458.876089	27.656026
269.954614	12478.898903	27.661044
270.625419	12481.567189	27.666061
270.868788	12506.751678	27.671079
271.198239	12517.987576	27.676096
271.774051	12506.672092	27.681114
272.415917	12527.118473	27.686132
272.509561	12538.040192	27.691149
273.006380	12548.497223	27.696167
272.902578	12544.817557	27.701184
273.085522	12547.957184	27.706202
273.224059	12567.181763	27.711220
273.449490	12572.028862	27.716237
273.519958	12583.025506	27.721255
273.867661	12604.217446	27.726272
274.354461	12602.499598	27.731290
274.239557	12638.519644	27.736308
274.518021	12646.218230	27.741325
274.833292	12660.550470	27.746343
275.224217	12683.779261	27.751360
275.425200	12693.191725	27.756378
274.957711	12717.978280	27.761396
275.563196	12734.684838	27.766413
275.586578	12757.185543	27.771431
275.788718	12783.086757	27.776448
276.025166	12805.968669	27.781466
276.706483	12832.427717	27.786484
277.052830	12845.123548	27.791501
277.070018	12874.128392	27.796519
277.319310	12893.392685	27.801536
277.816847	12916.384456	27.806554
277.777700	12943.862392	27.811572
278.455508	12960.769558	27.816589
278.999474	12987.821370	27.821607
278.876012	13002.722427	27.826624
279.064515	13019.051561	27.831642
279.977527	13024.895244	27.836660
280.747402	13025.686845	27.841677
281.533338	13024.390514	27.846695
281.989028	13022.159420	27.851712
282.262407	13019.020220	27.856730
282.296628	13023.980608	27.861748
282.427419	13022.631079	27.866765
282.772591	13029.123728	27.871783
282.830470	13033.920879	27.876800
283.206429	13025.930195	27.881818
282.878674	13036.260936	27.886836
283.229236	13033.948565	27.891853
283.269240	13040.547113	27.896871
283.408522	13063.936207	27.901888
283.445482	13076.585953	27.906906
283.809190	13096.760777	27.911924
283.735763	13112.332660	27.916941
284.088807	13133.464478	27.921959
284.272390	13160.617749	27.926976
284.760906	13182.267016	27.931994
284.641033	13209.166613	27.937012
287.503785	13158.125161	27.942029
288.152938	13156.421987	27.947047
288.322863	13149.869297	27.952064
288.508890	13142.763788	27.957082
288.244346	13139.713613	27.962100
288.444508	13124.312195	27.967117
288.678840	13107.383990	27.972135
288.106994	13112.776116	27.977152
288.543387	13117.566730	27.982170
288.785494	13132.383182	27.987188
288.687694	13137.355201	27.992205
289.078019	13152.102135	27.997223
288.993517	13159.648825	28.002240
289.265605	13170.483641	28.007258
289.489223	13205.154494	28.012276
289.688091	13227.080429	28.017293
289.517148	13252.945461	28.022311
289.104555	13283.148468	28.027328
290.082512	13311.644239	28.032346
290.175381	13348.079424	28.037364
290.212066	13376.831210	28.042381
290.617928	13412.207317	28.047399
290.908781	13454.943300	28.052416
291.251794	13481.855421	28.057434
291.481991	13512.802943	28.062452
291.564603	13549.738395	28.067469
292.178709	13581.318479	28.072487
292.262751	13620.408445	28.077504
292.971940	13635.463677	28.082522
293.485930	13668.162822	28.087540
293.519881	13694.817760	28.092557
293.908368	13716.368242	28.097575
294.322095	13737.121613	28.102592
294.600852	13754.990111	28.107610
294.973364	13785.385736	28.112628
295.264783	13801.513596	28.117645
296.009255	13813.055957	28.122663
295.940705	13837.553573	28.127680
296.642245	13857.660394	28.132698
297.027732	13874.166247	28.137716
296.641127	13886.410055	28.142733
296.873941	13912.924080	28.147751
297.012487	13938.248523	28.152768
297.507514	13955.851623	28.157786
297.459526	13986.639659	28.162804
297.650125	14020.469896	28.167821
298.287031	14054.825814	28.172839
298.456914	14076.357492	28.177856
298.957118	14097.645014	28.182874
299.489234	14109.630643	28.187892
299.695348	14144.761996	28.192909
300.372618	14165.019942	28.197927
300.475598	14189.666791	28.202944
300.967246	14210.804609	28.207962
300.720713	14236.603750	28.212980
301.287124	14258.728137	28.217997
301.355404	14280.261734	28.223015
301.892500	14312.877812	28.228032
302.293631	14327.303977	28.233050
302.532502	14353.615915	28.238068
302.216684	14370.608152	28.243085
302.740604	14395.348664	28.248103
302.948301	14421.845745	28.253120
303.665401	14458.750139	28.258138
304.142439	14481.556892	28.263156
304.450752	14508.599584	28.268173
305.466216	14507.932138	28.273191
305.737362	14535.279154	28.278208
306.130763	14533.586584	28.283226
306.573287	14554.764789	28.288244
306.673551	14558.089211	28.293261
307.061132	14561.536199	28.298279
306.901293	14589.915532	28.303296
307.225030	14596.157127	28.308314
307.378564	14618.469406	28.313332
306.873309	14644.335592	28.318349
307.574775	14667.346879	28.323367
307.523936	14696.051336	28.328384
308.043293	14728.690192	28.333402
308.339059	14759.551578	28.338420
308.581976	14786.468798	28.343437
308.878039	14815.601071	28.348455
308.984278	14847.801833	28.353472
309.272170	14870.110338	28.358490
309.499439	14905.536021	28.363508
309.619992	14947.097625	28.368525
310.372627	14960.934467	28.373543
310.587425	15000.533340	28.378560
310.969347	15033.533680	28.383578
311.533854	15059.236074	28.388596
311.355908	15081.277921	28.393613
311.750712	15103.565263	28.398631
311.841072	15134.862933	28.403648
312.081293	15162.512630	28.408666
312.669646	15201.062767	28.413684
312.650296	15244.149738	28.418701
313.305469	15258.920949	28.423719
313.707284	15301.480329	28.428736
313.712084	15331.982808	28.433754
314.211299	15359.482829	28.438772
314.605220	15387.439162	28.443789
315.206124	15408.908158	28.448807
315.641355	15438.615101	28.453824
316.166233	15457.649151	28.458842
316.976064	15475.294500	28.463860
316.681816	15496.215564	28.468877
317.689978	15498.082515	28.473895
317.854933	15519.271698	28.478912
318.239137	15525.474908	28.483930
318.423819	15546.703306	28.488948
318.677664	15565.249554	28.493965
318.867979	15573.303536	28.498983
319.183789	15597.832456	28.504000
319.366785	15626.419625	28.509018
319.678748	15644.456298	28.514036
319.865856	15673.695453	28.519053
320.579791	15693.424069	28.524071
320.188024	15719.009220	28.529088
320.540555	15742.319841	28.534106
320.620742	15766.954026	28.539124
320.997630	15807.138670	28.544141
321.305629	15830.704537	28.549159
321.625279	15863.348331	28.554176
322.110940	15895.895952	28.559194
322.413535	15924.133672	28.564212
322.873205	15963.095425	28.569229
323.172495	15979.376971	28.574247
323.327179	16011.816025	28.579264
323.607490	16038.609063	28.584282
323.697619	16064.506245	28.589300
324.188026	16098.836346	28.594317
324.604699	16132.851265	28.599335
325.087956	16168.095468	28.604352
325.411802	16195.513432	28.609370
325.890886	16215.476820	28.614388
325.816995	16258.775969	28.619405
326.538691	16273.508312	28.624423
326.931247	16297.497014	28.629440
327.265083	16323.868317	28.634458
327.941672	16343.731800	28.639476
328.216453	16362.751427	28.644493
328.420200	16383.441643	28.649511
328.573513	16403.081174	28.654528
329.067383	16422.583539	28.659546
329.728336	16427.415462	28.664564
329.680232	16451.970180	28.669581
330.356625	16468.143433	28.674599
330.591421	16484.209522	28.679616
331.055115	16492.461442	28.684634
331.763265	16515.907677	28.689652
332.750972	16496.245789	28.694669
333.336844	16492.413931	28.699687
333.558259	16497.548214	28.704704
333.520343	16493.378714	28.709722
334.232141	16485.543214	28.714740
334.347403	16495.779675	28.719757
334.564478	16490.846044	28.724775
334.761831	16492.424871	28.729792
334.731207	16500.736295	28.734810
335.049754	16510.282128	28.739828
335.108524	16520.480993	28.744845
335.231955	16529.383989	28.749863
335.580635	16553.618623	28.754880
335.475828	16576.050325	28.759898
335.538978	16601.380720	28.764916
335.445399	16638.171956	28.769933
335.868501	16661.689322	28.774951
336.172518	16708.780856	28.779968
336.330153	16743.810937	28.784986
336.635267	16771.794280	28.790004
336.874826	16817.472051	28.795021
336.995196	16859.987493	28.800039
337.378601	16902.200996	28.805056
337.269063	16935.320873	28.810074
337.949451	16978.782683	28.815092
338.050072	17035.055132	28.820109
338.526580	17080.108135	28.825127
339.232193	17113.049243	28.830144
339.242162	17162.615513	28.835162
340.030203	17197.283108	28.840180
340.002810	17234.951878	28.845197
340.661481	17285.725287	28.850215
341.357207	17312.691956	28.855232
342.707531	17330.186745	28.860250
343.550846	17340.035667	28.865268
343.755728	17364.799030	28.870285
343.924294	17384.561647	28.875303
344.643349	17390.448045	28.880320
344.727386	17416.953752	28.885338
345.249774	17428.375915	28.890356
345.155987	17440.185888	28.895373
345.812900	17459.239018	28.900391
345.899913	17478.993651	28.905408
345.940968	17504.835265	28.910426
346.152425	17521.242152	28.915444
346.587331	17545.966361	28.920461
346.473132	17570.453645	28.925479
346.750204	17590.532132	28.930496
347.053080	17616.493004	28.935514
347.090668	17647.427641	28.940532
347.268881	17676.909888	28.945549
347.517699	17709.384979	28.950567
348.267589	17754.856450	28.955584
347.926178	17785.846838	28.960602
348.565264	17815.600335	28.965620
348.746652	17853.401826	28.970637
349.529964	17888.100045	28.975655
350.151516	17917.057412	28.980672
350.505249	17941.209635	28.985690
350.830655	17967.462007	28.990708
351.413360	17998.619179	28.995725
351.853767	18031.197643	29.000743
352.057391	18055.002108	29.005760
352.274221	18086.652555	29.010778
352.641215	18109.927747	29.015796
352.901268	18149.245707	29.020813
353.186729	18169.916247	29.025831
353.736061	18207.469438	29.030848
353.981138	18242.107707	29.035866
354.494558	18260.439039	29.040884
354.486469	18295.112923	29.045901
354.925562	18330.976250	29.050919
355.430759	18365.453524	29.055936
355.562835	18400.663299	29.060954
356.132818	18429.351330	29.065972
356.433045	18463.036212	29.070989
356.931416	18503.220709	29.076007
357.371029	18528.382284	29.081024
357.359543	18565.961444	29.086042
357.885112	18597.599356	29.091060
358.237055	18635.374951	29.096077
358.369478	18662.377274	29.101095
358.979944	18695.377221	29.106112
359.036124	18729.364607	29.111130
360.101405	18742.889312	29.116148
360.791485	18781.258437	29.121165
360.798724	18812.077438	29.126183
361.263411	18829.840693	29.131200
361.526895	18865.903959	29.136218
361.720232	18887.545045	29.141236
362.075098	18911.780456	29.146253
362.681157	18932.266127	29.151271
362.932482	18959.380988	29.156288
362.850153	18989.996509	29.161306
363.928113	19017.326118	29.166324
364.421517	19043.299112	29.171341
364.322123	19061.348486	29.176359
364.918631	19091.997635	29.181376
365.434193	19110.498234	29.186394
366.149872	19131.726895	29.191412
366.285456	19159.716474	29.196429
366.826145	19174.252217	29.201447
367.229105	19187.269582	29.206464
366.841750	19210.172618	29.211482
367.028770	19230.668979	29.216500
367.535134	19257.833635	29.221517
367.483792	19284.560995	29.226535
368.175685	19307.583500	29.231552
368.115383	19349.488183	29.236570
368.609793	19373.796522	29.241588
369.122593	19412.189585	29.246605
369.213549	19448.085000	29.251623
369.494702	19472.286549	29.256640
369.278622	19524.003421	29.261658
369.405403	19569.496721	29.266676
370.058318	19613.007906	29.271693
370.328983	19653.101726	29.276711
370.938905	19688.594941	29.281728
371.240923	19744.425676	29.286746
371.551332	19780.977949	29.291764
372.322489	19827.217676	29.296781
372.328675	19871.002768	29.301799
372.995816	19910.428509	29.306816
373.249119	19963.067512	29.311834
373.799323	19990.760355	29.316852
373.957263	20031.314304	29.321869
374.630464	20080.460139	29.326887
375.318010	20102.751280	29.331904
375.612639	20135.368258	29.336922
376.510755	20169.870184	29.341940
377.190179	20201.276604	29.346957
377.463915	20237.218052	29.351975
378.042831	20255.690130	29.356992
377.809751	20283.680101	29.362010
378.651433	20305.882024	29.367028
379.183389	20336.114034	29.372045
379.120861	20366.496861	29.377063
379.433168	20392.834095	29.382080
379.712262	20427.067358	29.387098
379.810406	20452.563112	29.392116
380.288314	20475.513510	29.397133
380.779446	20513.652615	29.402151
381.792168	20548.105714	29.407168
381.463559	20591.623642	29.412186
381.879076	20615.450593	29.417204
382.778503	20650.259178	29.422221
382.565757	20676.570152	29.427239
383.196557	20704.196739	29.432256
383.102935	20747.427231	29.437274
383.593432	20783.980765	29.442292
384.721065	20803.180933	29.447309
385.949019	20820.094865	29.452327
386.654285	20819.292770	29.457344
387.241679	20834.895769	29.462362
387.294936	20857.960460	29.467380
387.792064	20864.311881	29.472397
387.727371	20872.033674	29.477415
388.078318	20877.317403	29.482432
388.115924	20894.955768	29.487450
388.346629	20903.899463	29.492468
388.459260	20927.308862	29.497485
388.825717	20945.920601	29.502503
389.170816	20971.595571	29.507520
389.298390	21001.505436	29.512538
389.679041	21031.436632	29.517556
390.060653	21056.551997	29.522573
390.173624	21077.526878	29.527591
391.262969	21091.880370	29.532608
392.177847	21121.289688	29.537626
392.305994	21142.809221	29.542644
392.730931	21158.490820	29.547661
392.549085	21176.553418	29.552679
393.094539	21189.443836	29.557696
393.526767	21219.860085	29.562714
393.596580	21245.544802	29.567732
394.177706	21279.007390	29.572749
394.568957	21304.905178	29.577767
394.829043	21336.276765	29.582784
395.063073	21370.138047	29.587802
395.729791	21398.658436	29.592820
395.836754	21429.703214	29.597837
395.701317	21469.833078	29.602855
396.495371	21497.246907	29.607872
396.768301	21537.983436	29.612890
396.859847	21583.421938	29.617908
397.752477	21625.451189	29.622925
397.637730	21661.612032	29.627943
398.457311	21696.958410	29.632960
398.880976	21738.609427	29.637978
398.876151	21767.702828	29.642996
399.442730	21806.743367	29.648013
399.866905	21857.233257	29.653031
400.084274	21894.253871	29.658048
400.736159	21934.391822	29.663066
400.556051	21976.388161	29.668084
401.150148	22024.663785	29.673101
401.514543	22070.462098	29.678119
402.054674	22110.200145	29.683136
402.310787	22168.585602	29.688154
402.466025	22201.593130	29.693172
403.075713	22244.833042	29.698189
403.862663	22300.358825	29.703207
404.328316	22328.535180	29.708224
405.173467	22361.058925	29.713242
405.471867	22390.771636	29.718260
406.271790	22425.539412	29.723277
406.254896	22461.390279	29.728295
407.137911	22494.847674	29.733312
407.650253	22519.710975	29.738330
408.044709	22545.127538	29.743348
408.452624	22576.092860	29.748365
408.681215	22601.414926	29.753383
409.176560	22627.218033	29.758400
409.719174	22647.219169	29.763418
410.156213	22655.521279	29.768436
410.837832	22681.093844	29.773453
410.846769	22700.707090	29.778471
411.560989	22721.886894	29.783488
411.677377	22744.433939	29.788506
411.979744	22763.990664	29.793524
412.615139	22783.547112	29.798541
412.866124	22819.784923	29.803559
413.328270	22843.064508	29.808576
413.133978	22867.462761	29.813594
413.381578	22908.511261	29.818612
414.142451	22936.527635	29.823629
414.407458	22967.057662	29.828647
414.422004	22994.186421	29.833664
414.750631	23039.299560	29.838682
415.068682	23081.380400	29.843700
415.463327	23108.778535	29.848717
416.017602	23164.470007	29.853735
416.489090	23207.398547	29.858752
416.591848	23251.563715	29.863770
416.787873	23297.741117	29.868788
417.439563	23334.914357	29.873805
417.739281	23387.486582	29.878823
418.456546	23424.756020	29.883840
419.091147	23477.583391	29.888858
419.126492	23523.003548	29.893876
419.633829	23563.674759	29.898893
420.085608	23616.625359	29.903911
420.594855	23651.846024	29.908928
421.238665	23696.496830	29.913946
421.565363	23737.669386	29.918964
421.760286	23780.722454	29.923981
421.744591	23821.483907	29.928999
422.751741	23870.211238	29.934016
423.914361	23918.801666	29.939034
423.863437	23958.490731	29.944052
424.825660	23993.634469	29.949069
424.704674	24031.058337	29.954087
425.088881	24059.254649	29.959104
426.160547	24087.453061	29.964122
426.723260	24114.562193	29.969140
427.364812	24138.169224	29.974157
427.376058	24169.981351	29.979175
428.004005	24195.628461	29.984192
428.410244	24232.735307	29.989210
428.476810	24272.335565	29.994228
429.334190	24301.255534	29.999245
429.436619	24337.768037	30.004263
429.267217	24365.586574	30.009280
429.936857	24406.228810	30.014298
430.088437	24450.909148	30.019316
430.372200	24486.854653	30.024333
430.471301	24529.531717	30.029351
431.236071	24564.738850	30.034368
431.817871	24600.911102	30.039386
432.798557	24635.377955	30.044404
433.438565	24651.431242	30.049421
433.875382	24684.508840	30.054439
434.690507	24703.342718	30.059456
435.276214	24719.679805	30.064474
435.636308	24737.042895	30.069492
435.863147	24760.595674	30.074509
435.998005	24788.179796	30.079527
436.180615	24814.203812	30.084544
436.538962	24842.705506	30.089562
436.739078	24878.401190	30.094580
437.249644	24905.936888	30.099597
437.383614	24949.284058	30.104615
437.726911	24990.182323	30.109632
438.100920	25033.236213	30.114650
438.195581	25082.650138	30.119668
439.238423	25121.977788	30.124685
439.456509	25169.370883	30.129703
439.406690	25214.750144	30.134720
440.101236	25268.651561	30.139738
440.040686	25321.319802	30.144756
440.410844	25364.772642	30.149773
441.083378	25424.324876	30.154791
441.608271	25463.489700	30.159808
442.920923	25512.077840	30.164826
443.115844	25550.693738	30.169844
443.670069	25595.718120	30.174861
444.188562	25643.310238	30.179879
444.383941	25688.121907	30.184896
445.352821	25723.293270	30.189914
445.575387	25774.002698	30.194932
446.168532	25810.043043	30.199949
446.465564	25850.916565	30.204967
446.609705	25892.800618	30.209984
447.434052	25925.946672	30.215002
447.930746	25974.234292	30.220020
448.385404	25999.721348	30.225037
448.749256	26041.066523	30.230055
448.896941	26081.108121	30.235072
449.869369	26109.342625	30.240090
450.245440	26153.802757	30.245108
451.129038	26189.462879	30.250125
451.401181	26228.338349	30.255143
451.786624	26262.128098	30.260160
452.381852	26300.812714	30.265178
452.489630	26343.663104	30.270196
453.032024	26377.511357	30.275213
453.257671	26419.726571	30.280231
453.721661	26460.891540	30.285248
454.198996	26498.334918	30.290266
454.194361	26544.287213	30.295284
454.873356	26586.450382	30.300301
455.200979	26624.727296	30.305319
455.350132	26669.603042	30.310336
455.733980	26718.476762	30.315354
456.014723	26766.759419	30.320372
456.194449	26800.393023	30.325389
456.490422	26859.879048	30.330407
457.118219	26908.831378	30.335424
458.284063	26954.192983	30.340442
458.783826	27003.489308	30.345460
459.208651	27038.185549	30.350477
459.537462	27081.403687	30.355495
460.367281	27129.905584	30.360512
460.685899	27164.705457	30.365530
461.161622	27206.867101	30.370548
461.802584	27237.662028	30.375565
462.395400	27274.932697	30.380583
462.486945	27313.718494	30.385600
463.371490	27359.097808	30.390618
463.443845	27408.698823	30.395636
463.934885	27449.129557	30.400653
464.331511	27492.292921	30.405671
464.658934	27542.276515	30.410688
464.821512	27588.931680	30.415706
465.240855	27643.171551	30.420724
465.745657	27697.040440	30.425741
466.555463	27742.916262	30.430759
466.904338	27788.278061	30.435776
467.703612	27822.567805	30.440794
467.986122	27879.579814	30.445812
468.620190	27918.939678	30.450829
469.481224	27958.503671	30.455847
469.610960	28002.386034	30.460864
470.362985	28044.208936	30.465882
470.855867	28095.178503	30.470900
471.255683	28135.938800	30.475917
471.669607	28179.993759	30.480935
472.009004	28223.231830	30.485952
472.814041	28252.192603	30.490970
473.468520	28304.548538	30.495988
473.685507	28334.941640	30.501005
474.359917	28367.357671	30.506023
474.911722	28405.801987	30.511040
475.439162	28443.199929	30.516058
475.843188	28476.798315	30.521076
476.151856	28511.022035	30.526093
476.875266	28551.712071	30.531111
476.990194	28603.782745	30.536128
477.582638	28647.470692	30.541146
477.844420	28686.577409	30.546164
477.518730	28728.132281	30.551181
478.102565	28781.662824	30.556199
478.297665	28836.418073	30.561216
478.550796	28891.838749	30.566234
479.275864	28958.388972	30.571252
479.680383	29013.042627	30.576269
480.047999	29063.695709	30.581287
480.519112	29132.154811	30.586304
481.625802	29163.589544	30.591322
482.445994	29199.938735	30.596340
482.984473	29243.558528	30.601357
483.562315	29276.242045	30.606375
484.275234	29317.339516	30.611392
484.790125	29351.049938	30.616410
485.455002	29393.493633	30.621428
485.333930	29422.823279	30.626445
486.191950	29460.040525	30.631463
486.276804	29506.906562	30.636480
486.943511	29543.222813	30.641498
487.175097	29597.346275	30.646516
487.375773	29642.069331	30.651533
488.009396	29685.424647	30.656551
488.165516	29737.740873	30.661568
488.561483	29784.879330	30.666586
488.942875	29838.403595	30.671604
489.158441	29894.695251	30.676621
489.746990	29949.320268	30.681639
489.991147	30019.008098	30.686656
490.512450	30084.205977	30.691674
491.078518	30145.985479	30.696692
491.705294	30209.029564	30.701709
492.369278	30269.372800	30.706727
492.725375	30324.389052	30.711744
493.284597	30386.139010	30.716762
493.909355	30450.171940	30.721780
494.302937	30514.244714	30.726797
495.367965	30563.204872	30.731815
495.567504	30615.916988	30.736832
496.139483	30672.613890	30.741850
496.881684	30714.451124	30.746868
498.330627	30746.117185	30.751885
499.241932	30782.334115	30.756903
500.018255	30814.629897	30.761920
500.790916	30831.650664	30.766938
501.177192	30861.157655	30.771956
501.393666	30892.710152	30.776973
502.135610	30913.021131	30.781991
502.328613	30935.754956	30.787008
502.434539	30963.208591	30.792026
503.127408	30991.069732	30.797044
503.306297	31042.240451	30.802061
504.012157	31068.370262	30.807079
504.117746	31109.153124	30.812096
504.614542	31143.299213	30.817114
505.124100	31189.835009	30.822132
505.241532	31231.903587	30.827149
505.433975	31271.674783	30.832167
505.926246	31338.478957	30.837184
506.295687	31378.772289	30.842202
506.600231	31439.364115	30.847220
507.347468	31504.888232	30.852237
508.635092	31525.551351	30.857255
509.522595	31542.158674	30.862272
510.337309	31574.843714	30.867290
510.820251	31593.637826	30.872308
511.242256	31626.409186	30.877325
511.711192	31655.691905	30.882343
512.091422	31693.118789	30.887360
512.368779	31720.092959	30.892378
512.871133	31752.746648	30.897396
512.554772	31793.852673	30.902413
513.281240	31837.528684	30.907431
513.470993	31889.403685	30.912448
513.717545	31936.617632	30.917466
514.139264	31989.062220	30.922484
514.269997	32051.206947	30.927501
514.939795	32103.527315	30.932519
515.065647	32167.942238	30.937536
515.516917	32217.599088	30.942554
516.325193	32284.762901	30.947572
516.581866	32355.426539	30.952589
517.206747	32413.966033	30.957607
517.532261	32489.929556	30.962624
518.350260	32558.721111	30.967642
518.862549	32615.929881	30.972660
519.454304	32689.901502	30.977677
520.081134	32743.742738	30.982695
520.615250	32795.289954	30.987712
522.158771	32844.534168	30.992730
522.764513	32893.326970	30.997748
523.178084	32945.176144	31.002765
523.621040	32990.961171	31.007783
524.225195	33046.975282	31.012800
524.908997	33095.767884	31.017818
525.283718	33131.494543	31.022836
526.326536	33176.675473	31.027853
528.090411	33189.710029	31.032871
528.890663	33211.597907	31.037888
529.550350	33232.376928	31.042906
530.041966	33244.685906	31.047924
529.824615	33271.141246	31.052941
530.287820	33291.723620	31.057959
530.902621	33331.322879	31.062976
530.894955	33357.527814	31.067994
531.305435	33393.258336	31.073012
531.759890	33433.033622	31.078029
531.784449	33466.820081	31.083047
532.181679	33519.267031	31.088064
532.292211	33568.619916	31.093082
532.994810	33621.513482	31.098100
532.864578	33673.012942	31.103117
533.581121	33735.552300	31.108135
533.779271	33806.155928	31.113152
534.352380	33864.396580	31.118170
534.695212	33935.171595	31.123188
535.022174	34010.604769	31.128205
535.603617	34071.770315	31.133223
535.992866	34129.752970	31.138240
536.187965	34198.253559	31.143258
536.959311	34259.352484	31.148276
537.666368	34345.910261	31.153293
538.179236	34404.421778	31.158311
538.208494	34471.155988	31.163328
539.053134	34544.135595	31.168346
539.851106	34602.895581	31.173364
540.494905	34670.573069	31.178381
541.703041	34721.038214	31.183399
541.927898	34786.130425	31.188416
542.563672	34848.191957	31.193434
542.825045	34901.871864	31.198452
543.094345	34973.509402	31.203469
543.974771	35033.336082	31.208487
544.483908	35095.448565	31.213504
544.801490	35158.364206	31.218522
546.091917	35214.008649	31.223540
546.642595	35282.105222	31.228557
547.659421	35325.209710	31.233575
548.341301	35386.684432	31.238592
548.744661	35433.754425	31.243610
549.460022	35476.399607	31.248628
549.930316	35537.131487	31.253645
550.517827	35584.220818	31.258663
550.749350	35637.150498	31.263680
551.474386	35688.550172	31.268698
552.042144	35743.619360	31.273716
552.096897	35804.909411	31.278733
552.876526	35852.294780	31.283751
553.306882	35911.851119	31.288768
554.011293	35965.347785	31.293786
554.473228	36014.085283	31.298804
554.800910	36080.000956	31.303821
555.460293	36130.090594	31.308839
556.371445	36170.712165	31.313856
557.424224	36220.179118	31.318874
558.112978	36270.339865	31.323892
558.662930	36326.619628	31.328909
559.169784	36378.961381	31.333927
559.398364	36424.993847	31.338944
559.772922	36484.814136	31.343962
560.555290	36523.296377	31.348980
561.524821	36567.349395	31.353997
562.187871	36616.893673	31.359015
562.362701	36658.781991	31.364032
562.356844	36704.527053	31.369050
563.394333	36761.030804	31.374068
563.832867	36820.743380	31.379085
564.414194	36873.351566	31.384103
564.685090	36931.413947	31.389120
564.831627	36993.415111	31.394138
565.440321	37046.479964	31.399156
565.738548	37122.199282	31.404173
566.560388	37190.840497	31.409191
566.750090	37245.145655	31.414208
567.358562	37306.090182	31.419226
567.900727	37354.662839	31.424244
568.264037	37425.627857	31.429261
568.856066	37488.813864	31.434279
569.440215	37554.807706	31.439296
569.778131	37624.101658	31.444314
570.700809	37681.685411	31.449332
571.438058	37747.978855	31.454349
572.039773	37804.683607	31.459367
572.376660	37868.413396	31.464384
572.787632	37945.480492	31.469402
573.496816	38005.983932	31.474420
573.838228	38085.623647	31.479437
574.447182	38147.164354	31.484455
574.973447	38215.377063	31.489472
575.531946	38292.379298	31.494490
576.179093	38364.265284	31.499508
576.906968	38444.080250	31.504525
577.568894	38503.280190	31.509543
578.254404	38576.764097	31.514560
578.782009	38641.685580	31.519578
579.946472	38697.122320	31.524596
580.272335	38760.029988	31.529613
580.468743	38828.888660	31.534631
581.526330	38892.391177	31.539648
581.905303	38965.562955	31.544666
582.489703	39022.435428	31.549684
583.075165	39094.372713	31.554701
583.830804	39164.551121	31.559719
584.586692	39219.450149	31.564736
584.996780	39291.257244	31.569754
585.927031	39347.758924	31.574772
586.233278	39400.973944	31.579789
586.849343	39473.614624	31.584807
587.746605	39530.823367	31.589824
588.044997	39598.909754	31.594842
588.819312	39657.980491	31.599860
589.447398	39713.063889	31.604877
590.379517	39766.535786	31.609895
591.373262	39812.887617	31.614912
591.538733	39872.937855	31.619930
592.353650	39913.719966	31.624948
592.605151	39978.803948	31.629965
593.429459	40025.804128	31.634983
594.331320	40071.932413	31.640000
594.790635	40124.340328	31.645018
595.302561	40179.757569	31.650036
595.990758	40235.261588	31.655053
596.190594	40287.338723	31.660071
596.819984	40346.101830	31.665088
596.948612	40406.115904	31.670106
598.163591	40458.796251	31.675124
598.905815	40507.649181	31.680141
599.320520	40572.198976	31.685159
599.979555	40606.985438	31.690176
600.435009	40661.261421	31.695194
600.864795	40715.071538	31.700212
601.335337	40778.633751	31.705229
601.528687	40824.197026	31.710247
602.036383	40885.656849	31.715264
602.142986	40950.112351	31.720282
602.980965	41012.144293	31.725300
603.539694	41090.796734	31.730317
604.056431	41163.738881	31.735335
604.664198	41220.923504	31.740352
604.862246	41297.210661	31.745370
605.200282	41370.215804	31.750388
605.706042	41450.097553	31.755405
606.382901	41529.183098	31.760423
606.953938	41617.023489	31.765440
607.138590	41709.445522	31.770458
608.142872	41796.344252	31.775476
608.964438	41871.911235	31.780493
609.224707	41963.677458	31.785511
610.018822	42048.538951	31.790528
610.082490	42139.660872	31.795546
611.093940	42228.956876	31.800564
612.374970	42317.042015	31.805581
612.706011	42387.444253	31.810599
613.754305	42470.644322	31.815616
614.384759	42552.274446	31.820634
615.249077	42623.078773	31.825652
615.686039	42704.881641	31.830669
616.094122	42779.856885	31.835687
616.941717	42862.625761	31.840704
617.775932	42931.042978	31.845722
618.589356	43002.267938	31.850740
619.073884	43075.589322	31.855757
619.661364	43149.572238	31.860775
620.821185	43222.194340	31.865792
621.126436	43294.423179	31.870810
622.037191	43352.727560	31.875828
623.163369	43403.233714	31.880845
623.799687	43468.983846	31.885863
624.698964	43507.662675	31.890880
625.063302	43579.847750	31.895898
626.018494	43633.550968	31.900916
626.319053	43687.410702	31.905933
627.035765	43745.373779	31.910951
628.260460	43787.126717	31.915968
628.555259	43834.729274	31.920986
629.297621	43879.258588	31.926004
629.793534	43947.566941	31.931021
630.006955	43993.402874	31.936039
630.807238	44055.451341	31.941056
630.838708	44116.731764	31.946074
631.282964	44182.340450	31.951092
632.190031	44261.391731	31.956109
632.163490	44328.148914	31.961127
632.892520	44388.173897	31.966144
633.448898	44461.898869	31.971162
633.323412	44531.692599	31.976180
634.080214	44604.085915	31.981197
634.775690	44678.965777	31.986215
635.906161	44744.430423	31.991232
636.169535	44820.666969	31.996250
636.665170	44893.118763	32.001268
637.847677	44957.533125	32.006285
638.618486	45030.143563	32.011303
639.479943	45092.977586	32.016320
639.995044	45158.160661	32.021338
640.586339	45217.826599	32.026356
641.240595	45280.958851	32.031373
641.690193	45372.355501	32.036391
642.347779	45437.104585	32.041408
642.747738	45509.827759	32.046426
643.483495	45596.938427	32.051444
643.767489	45670.338947	32.056461
644.289150	45751.903614	32.061479
645.064612	45831.786120	32.066496
645.139031	45923.256001	32.071514
645.679398	46005.671225	32.076532
646.633916	46106.206484	32.081549
646.886055	46193.964871	32.086567
647.678307	46283.788128	32.091584
648.213262	46384.602008	32.096602
649.809752	46458.147040	32.101620
650.659917	46547.484733	32.106637
651.001630	46628.711305	32.111655
651.820456	46708.612153	32.116672
652.349157	46786.049104	32.121690
653.019169	46883.197896	32.126708
653.703543	46959.873012	32.131725
653.823100	47052.082732	32.136743
654.708439	47138.274691	32.141760
655.290262	47231.622010	32.146778
656.078316	47311.514849	32.151796
656.907516	47388.969074	32.156813
657.672933	47478.553019	32.161831
658.484195	47567.242035	32.166848
658.990795	47654.625562	32.171866
659.709164	47736.127072	32.176884
660.641079	47812.103081	32.181901
661.762507	47897.803192	32.186919
662.285030	47956.507187	32.191936
662.963099	48033.898306	32.196954
664.039526	48101.521965	32.201972
664.227538	48171.821652	32.206989
664.963547	48254.617291	32.212007
666.014946	48314.877325	32.217024
666.808329	48372.743411	32.222042
667.287048	48448.925909	32.227060
668.031130	48507.483077	32.232077
668.960143	48588.010870	32.237095
669.487289	48642.152120	32.242112
670.010220	48702.282803	32.247130
670.786228	48755.630009	32.252148
671.418966	48814.510402	32.257165
671.980914	48875.197158	32.262183
672.983135	48925.593896	32.267200
673.680888	48979.485765	32.272218
674.304382	49029.612847	32.277236
675.126670	49076.465296	32.282253
675.758165	49135.169997	32.287271
676.344685	49192.972903	32.292288
677.037322	49258.167908	32.297306
677.416650	49321.231039	32.302324
678.438220	49372.194179	32.307341
678.512968	49442.195700	32.312359
678.838705	49502.337378	32.317376
679.382691	49578.892176	32.322394
679.886840	49647.961718	32.327412
680.713214	49735.663111	32.332429
681.307922	49815.975313	32.337447
681.908261	49891.447728	32.342464
682.355131	49976.903041	32.347482
683.045332	50061.388373	32.352500
683.571649	50139.072913	32.357517
683.766002	50236.537995	32.362535
684.736094	50328.266981	32.367552
685.120259	50423.331389	32.372570
685.842564	50522.229994	32.377588
686.632812	50614.591311	32.382605
687.037904	50711.959485	32.387623
687.924331	50801.121087	32.392640
688.910921	50900.696553	32.397658
689.538262	50996.176964	32.402676
690.138923	51088.295014	32.407693
690.911446	51183.966275	32.412711
691.379598	51270.984108	32.417728
692.359333	51374.082214	32.422746
693.116030	51471.773004	32.427764
693.864532	51545.956519	32.432781
694.884455	51644.089558	32.437799
695.527423	51728.040513	32.442816
696.616172	51810.696076	32.447834
697.609121	51886.443787	32.452852
698.611093	51969.222291	32.457869
698.942060	52054.472755	32.462887
699.608311	52134.453673	32.467904
700.463310	52208.059129	32.472922
701.139058	52287.135540	32.477940
701.722592	52370.303324	32.482957
702.337232	52452.063477	32.487975
702.950964	52538.891388	32.492992
703.076514	52627.395525	32.498010
703.871369	52727.910301	32.503028
704.502797	52811.438203	32.508045
704.688058	52902.435416	32.513063
705.378474	52994.528058	32.518080
705.988140	53080.398643	32.523098
706.323256	53187.382472	32.528116
707.026939	53286.898430	32.533133
707.220371	53391.348629	32.538151
708.283981	53493.047052	32.543168
708.946845	53598.517359	32.548186
709.521947	53694.026106	32.553204
710.359827	53796.541949	32.558221
711.418263	53906.994761	32.563239
711.656319	54015.313973	32.568256
712.795229	54114.784800	32.573274
712.993576	54218.701408	32.578292
715.253522	54302.462122	32.583309
716.106036	54395.045323	32.588327
716.801562	54484.047753	32.593344
717.499689	54581.707073	32.598362
718.105462	54673.310167	32.603380
718.716430	54767.794252	32.608397
719.233477	54852.095974	32.613415
719.718009	54952.213881	32.618432
720.675774	55048.605113	32.623450
721.301277	55150.121656	32.628468
721.955855	55235.425131	32.633485
722.583235	55332.019666	32.638503
723.467355	55432.608656	32.643520
724.467115	55526.132398	32.648538
725.166406	55630.185387	32.653556
726.394984	55714.033932	32.658573
726.691115	55819.035345	32.663591
727.634172	55909.619466	32.668608
728.491901	55990.474129	32.673626
729.282910	56082.178328	32.678644
729.938224	56171.391056	32.683661
730.555298	56267.126097	32.688679
731.429665	56359.537702	32.693696
732.468906	56436.881029	32.698714
732.720042	56533.943929	32.703732
734.074291	56617.281799	32.708749
734.881229	56710.003584	32.713767
735.380183	56800.383414	32.718784
736.248701	56877.391141	32.723802
736.695492	56966.908539	32.728820
737.539016	57056.364694	32.733837
737.992155	57160.739514	32.738855
738.654824	57246.568359	32.743872
739.558023	57334.675733	32.748890
739.959624	57433.069618	32.753908
740.980757	57522.611170	32.758925
741.400093	57632.328174	32.763943
741.767181	57734.325453	32.768960
742.540242	57825.168503	32.773978
742.934175	57946.987952	32.778996
743.516545	58048.292653	32.784013
744.312269	58166.025057	32.789031
744.838112	58276.928112	32.794048
745.494433	58373.544898	32.799066
746.210534	58492.392533	32.804084
746.882301	58591.207124	32.809101
747.625216	58705.140621	32.814119
747.961186	58811.629675	32.819136
748.781228	58922.479530	32.824154
749.219206	59047.312799	32.829172
750.425916	59158.325233	32.834189
751.263817	59269.736429	32.839207
751.859713	59387.023449	32.844224
752.944376	59492.913774	32.849242
753.809871	59617.658334	32.854260
754.745289	59725.123953	32.859277
755.482000	59837.844968	32.864295
756.474058	59943.835659	32.869312
757.474736	60050.173057	32.874330
757.988828	60148.383803	32.879348
758.841964	60258.438827	32.884365
759.848898	60373.214972	32.889383
760.258256	60482.411744	32.894400
761.241111	60584.899294	32.899418
761.247511	60701.422538	32.904436
762.309244	60816.880745	32.909453
763.033973	60940.273184	32.914471
763.435342	61056.452658	32.919488
764.469917	61169.433359	32.924506
765.205805	61288.129478	32.929524
766.298577	61406.752504	32.934541
766.960011	61522.725707	32.939559
767.727366	61638.055625	32.944576
768.650244	61759.035951	32.949594
768.878109	61878.144857	32.954612
769.704216	62000.761399	32.959629
770.257655	62127.527881	32.964647
770.927648	62256.158925	32.969664
772.048062	62369.713042	32.974682
772.932115	62499.086451	32.979700
773.879560	62621.730129	32.984717
775.482995	62736.575265	32.989735
776.396387	62843.270720	32.994752
777.088273	62941.982649	32.999770
777.519362	63062.947349	33.004788
778.564336	63173.958551	33.009805
779.922831	63267.513207	33.014823
781.276438	63356.372134	33.019840
782.617256	63436.218923	33.024858
783.776150	63510.053637	33.029876
784.894415	63578.452574	33.034893
785.986094	63654.082037	33.039911
786.068439	63724.650243	33.044928
787.121834	63794.097768	33.049946
787.632679	63871.224622	33.054964
788.400995	63951.152482	33.059981
789.106864	64010.943605	33.064999
789.301828	64093.770797	33.070016
790.240722	64154.647710	33.075034
790.927344	64231.094627	33.080052
791.127441	64318.106933	33.085069
791.900730	64398.149443	33.090087
791.875314	64489.310363	33.095104
792.839106	64578.374023	33.100122
792.922403	64680.169754	33.105140
793.531356	64795.025868	33.110157
794.534957	64904.283158	33.115175
794.636124	65028.040553	33.120192
795.241463	65142.766417	33.125210
795.565370	65269.717716	33.130228
796.201484	65396.325477	33.135245
796.558138	65535.860397	33.140263
797.318483	65681.383900	33.145280
798.371519	65815.376810	33.150298
799.031863	65961.791862	33.155316
799.778431	66089.927531	33.160333
801.053644	66235.467816	33.165351
802.092304	66370.655337	33.170368
803.493365	66489.671680	33.175386
804.505735	66611.505612	33.180404
805.386769	66737.636859	33.185421
806.415762	66859.987828	33.190439
807.261675	66986.297280	33.195456
807.710453	67114.230907	33.200474
808.534095	67242.834540	33.205492
809.324483	67362.276513	33.210509
810.191430	67484.273132	33.215527
810.777603	67620.431306	33.220544
811.387165	67756.390330	33.225562
812.234745	67895.148479	33.230580
812.891729	68025.321863	33.235597
813.981674	68157.413650	33.240615
814.867941	68284.368825	33.245632
815.958181	68414.350225	33.250650
816.622166	68551.038460	33.255668
817.313819	68687.065208	33.260685
818.225040	68817.098680	33.265703
818.607727	68952.598287	33.270720
819.503091	69093.265646	33.275738
819.777102	69244.379113	33.280756
820.679571	69390.504294	33.285773
821.427881	69540.811402	33.290791
822.121323	69690.218366	33.295808
823.011124	69839.908910	33.300826
824.189729	69981.861501	33.305844
824.873514	70121.117367	33.310861
826.092930	70261.136084	33.315879
827.025842	70404.701810	33.320896
828.239198	70547.588074	33.325914
830.378698	70661.397813	33.330932
831.605555	70771.665017	33.335949
832.625289	70874.600936	33.340967
833.247395	70979.976915	33.345984
834.368755	71059.314455	33.351002
835.061999	71153.966352	33.356020
835.322250	71254.137778	33.361037
836.434302	71343.906213	33.366055
837.069824	71457.958760	33.371072
837.587266	71557.783976	33.376090
838.384819	71661.305543	33.381108
838.849186	71775.888671	33.386125
840.051698	71882.124547	33.391143
840.504551	71998.266559	33.396160
841.416577	72106.020494	33.401178
842.274100	72234.388768	33.406196
842.861352	72351.534167	33.411213
843.842824	72475.948909	33.416231
844.530479	72602.577618	33.421248
844.781617	72722.925786	33.426266
845.854443	72845.499220	33.431284
846.628566	72969.256583	33.436301
847.674616	73099.906068	33.441319
848.015421	73231.878787	33.446336
849.250808	73360.422934	33.451354
850.026993	73498.021139	33.456372
850.427718	73638.283952	33.461389
851.273478	73773.474906	33.466407
852.053472	73913.668183	33.471424
852.809219	74061.222240	33.476442
853.680178	74202.008946	33.481460
854.330409	74353.460149	33.486477
855.673626	74497.817306	33.491495
855.622108	74651.187011	33.496512
856.513579	74799.779008	33.501530
857.762666	74966.520576	33.506548
858.036293	75128.465259	33.511565
859.035551	75280.678942	33.516583
860.131038	75454.256329	33.521600
860.658056	75605.452527	33.526618
862.020792	75761.990632	33.531636
862.886326	75917.666193	33.536653
864.087562	76075.499221	33.541671
864.679062	76225.524702	33.546688
865.310273	76374.317248	33.551706
866.917672	76526.416285	33.556724
867.338593	76678.631007	33.561741
868.823939	76814.243250	33.566759
870.098959	76961.038073	33.571776
871.359342	77103.851196	33.576794
872.022532	77237.316916	33.581812
872.969713	77376.965636	33.586829
874.023498	77506.292278	33.591847
874.715431	77645.284216	33.596864
875.571972	77787.639472	33.601882
876.858564	77917.067766	33.606900
877.382570	78053.895895	33.611917
878.546980	78175.281040	33.616935
879.509972	78295.372875	33.621952
880.344450	78410.173495	33.626970
881.254248	78530.180795	33.631988
881.944593	78650.112446	33.637005
882.836024	78771.465299	33.642023
883.541806	78893.552800	33.647040
884.004701	79020.471484	33.652058
884.716656	79154.895412	33.657076
885.331779	79292.468221	33.662093
886.338135	79426.337229	33.667111
887.309716	79573.719727	33.672128
887.800826	79695.728092	33.677146
888.536221	79843.488079	33.682164
889.185433	79996.888009	33.687181
890.589110	80141.327949	33.692199
891.151826	80298.198983	33.697216
892.006819	80449.067711	33.702234
892.814386	80591.259090	33.707252
893.405756	80750.981620	33.712269
894.323361	80910.756941	33.717287
895.714709	81070.256106	33.722304
896.990096	81210.416226	33.727322
898.212332	81352.262914	33.732340
898.524557	81509.191434	33.737357
899.384048	81660.700023	33.742375
900.582787	81819.788151	33.747392
901.299732	81970.146367	33.752410
901.774069	82118.686956	33.757428
902.544100	82292.619089	33.762445
903.618716	82467.632920	33.767463
904.164460	82629.660349	33.772480
904.899389	82802.830398	33.777498
905.644711	82971.741696	33.782516
906.308299	83156.644718	33.787533
907.400754	83318.488400	33.792551
907.889028	83494.774608	33.797568
908.783236	83685.963421	33.802586
910.424609	83863.497593	33.807604
911.183885	84038.216553	33.812621
912.955235	84196.425591	33.817639
914.350822	84355.788409	33.822656
915.041466	84516.627165	33.827674
916.436848	84673.840761	33.832692
916.925391	84832.020670	33.837709
917.964513	84985.399449	33.842727
919.349696	85144.453005	33.847744
919.801226	85307.166866	33.852762
920.951863	85454.334576	33.857780
921.847673	85621.131975	33.862797
922.709435	85764.269532	33.867815
923.427780	85927.454537	33.872832
924.714728	86076.716353	33.877850
926.167223	86220.780656	33.882868
926.871566	86364.967635	33.887885
928.356896	86497.865072	33.892903
929.356095	86629.846642	33.897920
929.880802	86763.745411	33.902938
930.920070	86889.570455	33.907956
931.565168	87036.809251	33.912973
932.740533	87171.706347	33.917991
933.533638	87305.549537	33.923008
934.397353	87448.241253	33.928026
935.094874	87574.470174	33.933044
935.791772	87732.734987	33.938061
937.093714	87875.101058	33.943079
937.352796	88015.267006	33.948096
938.011261	88175.231065	33.953114
938.999079	88323.431670	33.958132
940.134386	88483.524967	33.963149
941.146699	88644.836535	33.968167
942.173045	88793.811882	33.973184
943.220395	88953.385417	33.978202
944.105980	89098.532468	33.983220
944.983663	89258.630732	33.988237
945.744288	89413.914751	33.993255
946.270038	89577.334827	33.998272
947.350431	89751.793876	34.003290
948.213310	89908.006583	34.008308
948.473846	90083.038797	34.013325
949.526518	90256.227727	34.018343
951.305682	90418.609688	34.023360
952.302310	90577.132958	34.028378
954.762111	90710.361507	34.033396
955.761508	90865.525305	34.038413
956.702164	91006.072880	34.043431
957.701520	91146.858060	34.048448
958.501021	91301.020829	34.053466
958.813287	91442.134246	34.058484
959.638089	91596.693302	34.063501
960.450959	91756.002578	34.068519
961.160054	91921.039999	34.073536
962.181107	92095.437354	34.078554
962.678849	92260.177771	34.083572
963.221838	92442.565290	34.088589
964.369868	92618.932157	34.093607
965.117703	92791.824092	34.098624
965.962523	92992.830778	34.103642
966.757195	93166.192054	34.108660
967.542330	93348.063709	34.113677
968.682868	93532.781333	34.118695
970.323215	93710.603548	34.123712
971.344239	93898.319508	34.128730
972.627570	94069.951246	34.133748
973.933642	94239.522946	34.138765
974.994326	94414.024801	34.143783
975.759966	94582.279727	34.148800
977.095693	94757.737075	34.153818
977.701783	94917.760451	34.158836
978.704869	95087.699988	34.163853
979.459084	95250.719751	34.168871
980.574843	95409.164989	34.173888
981.746824	95560.093541	34.178906
983.046621	95714.907099	34.183924
983.703827	95867.584271	34.188941
984.759487	96022.124994	34.193959
985.715012	96176.379938	34.198976
986.692110	96343.034103	34.203994
987.276424	96484.129524	34.209012
988.407494	96656.305173	34.214029
989.250679	96836.299295	34.219047
990.342471	97004.052412	34.224064
990.618174	97171.477896	34.229082
991.676321	97344.303803	34.234100
992.151098	97519.218737	34.239117
993.049168	97702.989246	34.244135
994.140889	97894.958418	34.249152
995.070272	98080.600309	34.254170
996.196832	98264.924540	34.259188
997.424209	98454.164913	34.264205
998.335990	98645.455102	34.269223
999.854248	98816.699000	34.274240
1000.697941	99007.117152	34.279258
1001.332387	99195.609789	34.284276
1002.402586	99390.873564	34.289293
1003.093417	99595.960736	34.294311
1003.949675	99782.919102	34.299328
1004.656509	99989.766853	34.304346
1005.303146	100187.983766	34.309364
1006.477821	100400.700172	34.314381
1007.673037	100617.587478	34.319399
1008.890442	100827.868649	34.324416
1009.450102	101033.021319	34.329434
1010.745239	101238.296609	34.334452
1011.919964	101452.129705	34.339469
1012.703751	101660.940507	34.344487
1013.953172	101872.763320	34.349504
1014.360232	102094.192370	34.354522
1015.422974	102310.305913	34.359540
1016.891393	102539.611579	34.364557
1017.398921	102744.324331	34.369575
1018.862212	102950.369455	34.374592
1019.723032	103180.430649	34.379610
1020.825042	103405.500534	34.384628
1022.029763	103627.375807	34.389645
1022.776655	103834.513048	34.394663
1024.039305	104048.567501	34.399680
1025.262337	104274.928573	34.404698
1026.005647	104489.810104	34.409716
1027.306241	104696.124646	34.414733
1028.515779	104915.768039	34.419751
1029.258971	105132.022659	34.424768
1030.638890	105351.285813	34.429786
1032.347979	105556.384452	34.434804
1033.893176	105761.082078	34.439821
1034.505188	105959.734616	34.444839
1036.358640	106131.108176	34.449856
1037.367417	106314.141196	34.454874
1038.630283	106476.257635	34.459892
1039.519329	106658.515507	34.464909
1040.198011	106841.228629	34.469927
1041.542797	107016.140237	34.474944
1041.875649	107199.041656	34.479962
1042.952460	107377.434181	34.484980
1044.149032	107562.824865	34.489997
1044.728893	107752.350533	34.495015
1045.886247	107944.096720	34.500032
1046.820799	108131.904899	34.505050
1047.699676	108327.197617	34.510068
1049.885283	108499.973361	34.515085
1050.954653	108685.026102	34.520103
1052.618878	108867.698076	34.525120
1053.064322	109055.685020	34.530138
1054.192437	109240.668114	34.535156
1055.129505	109427.560002	34.540173
1055.523552	109619.081250	34.545191
1056.577068	109805.791080	34.550208
1056.835640	110005.686414	34.555226
1057.886523	110214.809308	34.560244
1058.910228	110425.091248	34.565261
1059.674077	110643.096312	34.570279
1060.782225	110858.130383	34.575296
1061.437562	111079.109200	34.580314
1062.487272	111296.170964	34.585332
1064.332802	111505.306860	34.590349
1065.584686	111713.874521	34.595367
1066.293538	111925.108517	34.600384
1067.549450	112146.651728	34.605402
1068.503002	112355.972049	34.610420
1070.143103	112563.516704	34.615437
1070.840857	112780.789596	34.620455
1072.076651	112994.728660	34.625472
1073.238896	113216.334338	34.630490
1074.461261	113430.874473	34.635508
1075.650212	113636.806541	34.640525
1076.934530	113846.866806	34.645543
1078.778227	114027.894781	34.650560
1080.209101	114222.716188	34.655578
1081.079602	114421.005117	34.660596
1082.255608	114614.111700	34.665613
1083.027078	114827.320521	34.670631
1084.272410	115013.094524	34.675648
1084.962462	115222.975264	34.680666
1085.825266	115425.212976	34.685684
1086.970727	115612.439732	34.690701
1087.445700	115830.521603	34.695719
1088.696361	116041.123250	34.700736
1089.828240	116263.315291	34.705754
1090.799438	116472.498112	34.710772
1091.498469	116689.851203	34.715789
1092.285624	116909.243563	34.720807
1092.867748	117124.123703	34.725824
1093.757604	117348.887083	34.730842
1094.886263	117572.724309	34.735860
1095.863369	117793.915502	34.740877
1096.802180	118024.859427	34.745895
1098.502303	118217.114703	34.750912
1100.515560	118426.792072	34.755930
1101.593235	118641.078974	34.760948
1102.909149	118852.019252	34.765965
1104.009952	119066.609422	34.770983
1104.834084	119273.024272	34.776000
1105.896646	119495.785002	34.781018
1106.734448	119711.578065	34.786036
1108.204877	119914.224414	34.791053
1109.161460	120144.016037	34.796071
1110.179379	120354.257698	34.801088
1111.220585	120577.917292	34.806106
1112.266988	120802.920996	34.811124
1113.416444	121032.217549	34.816141
1114.251081	121264.294464	34.821159
1115.564742	121482.401405	34.826176
1116.637560	121710.613707	34.831194
1117.402138	121946.383124	34.836212
1118.911412	122170.227926	34.841229
1120.050318	122412.856587	34.846247
1121.187895	122627.960327	34.851264
1122.476957	122862.645880	34.856282
1123.229616	123092.279524	34.861300
1124.376848	123329.020774	34.866317
1125.242849	123577.129901	34.871335
1126.702880	123811.172475	34.876352
1127.528371	124048.988327	34.881370
1128.723397	124304.765618	34.886388
1130.197228	124533.272679	34.891405
1130.868190	124782.489616	34.896423
1132.128800	125016.829025	34.901440
1133.303493	125269.094279	34.906458
1134.244211	125516.673948	34.911476
1136.071666	125753.976528	34.916493
1136.588189	126011.088252	34.921511
1137.223798	126251.754771	34.926528
1138.147293	126524.708320	34.931546
1138.914949	126787.449275	34.936564
1140.142272	127047.844835	34.941581
1141.282224	127325.787786	34.946599
1142.339619	127589.854820	34.951616
1143.887355	127851.850025	34.956634
1144.766364	128122.505430	34.961652
1145.708637	128400.225513	34.966669
1147.136397	128683.239571	34.971687
1148.845689	128938.966815	34.976704
1150.184586	129200.552597	34.981722
1151.031113	129470.096866	34.986740
1152.633755	129720.587941	34.991757
1154.012368	129975.137816	34.996775
1155.080534	130215.633700	35.001792
1156.958090	130448.526185	35.006810
1157.914828	130678.155250	35.011828
1159.508312	130887.698046	35.016845
1160.524107	131121.338751	35.021863
1162.194274	131345.082360	35.026880
1164.053752	131558.805454	35.031898
1164.901748	131775.821744	35.036916
1166.377076	131986.608902	35.041933
1167.576710	132204.493298	35.046951
1168.154336	132416.527188	35.051968
1169.111342	132639.349559	35.056986
1170.197832	132862.671064	35.062004
1171.453143	133084.329749	35.067021
1172.288896	133323.646007	35.072039
1173.914893	133544.749894	35.077056
1175.135623	133775.293745	35.082074
1175.822493	134014.881388	35.087092
1177.181899	134240.827922	35.092109
1178.536379	134457.242728	35.097127
1179.452991	134680.478827	35.102144
1180.483133	134916.654423	35.107162
1181.733472	135159.817939	35.112180
1182.928245	135398.174831	35.117197
1184.711053	135617.756904	35.122215
1186.479787	135835.948150	35.127232
1187.618196	136069.640965	35.132250
1188.788386	136295.519674	35.137268
1190.151850	136509.625946	35.142285
1190.575213	136748.745747	35.147303
1191.603349	136979.192496	35.152320
1192.565193	137220.391592	35.157338
1193.278224	137466.377114	35.162356
1193.892120	137709.896188	35.167373
1195.125416	137975.703227	35.172391
1195.747163	138236.202769	35.177408
1197.218639	138489.863856	35.182426
1198.667739	138761.219169	35.187444
1200.116772	139012.504120	35.192461
1201.494530	139270.447492	35.197479
1202.521572	139529.226322	35.202496
1203.951432	139780.634255	35.207514
1205.057432	140047.696362	35.212532
1205.857381	140303.780862	35.217549
1207.229162	140581.808242	35.222567
1208.277973	140839.933684	35.227584
1210.131393	141092.470537	35.232602
1211.527918	141346.203341	35.237620
1213.093882	141595.901776	35.242637
1214.487767	141849.575249	35.247655
1215.552868	142097.663710	35.252672
1217.086935	142353.574039	35.257690
1218.123516	142596.928083	35.262708
1219.057346	142860.173173	35.267725
1220.079550	143108.859370	35.272743
1220.810242	143351.408576	35.277760
1221.985099	143593.122482	35.282778
1222.695524	143858.188582	35.287796
1223.721442	144117.584550	35.292813
1224.824206	144383.031205	35.297831
1226.104495	144647.231937	35.302848
1227.014211	144902.037149	35.307866
1228.324483	145179.946025	35.312884
1230.042448	145435.073162	35.317901
1232.167819	145694.571187	35.322919
1233.012362	145944.917941	35.327936
1234.956400	146196.283026	35.332954
1235.828553	146452.462503	35.337972
1237.275506	146694.809922	35.342989
1238.710169	146953.788253	35.348007
1239.500152	147216.468028	35.353024
1240.854473	147464.505616	35.358042
1241.793971	147730.105886	35.363060
1242.767716	147986.760521	35.368077
1244.039109	148255.389726	35.373095
1245.295676	148525.697601	35.378112
1246.924550	148783.564612	35.383130
1247.865290	149057.646629	35.388148
1249.321168	149334.179182	35.393165
1250.478951	149589.240462	35.398183
1252.193056	149859.200512	35.403200
1254.420420	150100.434323	35.408218
1255.920427	150340.183308	35.413236
1257.914452	150580.990795	35.418253
1259.296137	150823.743822	35.423271
1260.638387	151056.586064	35.428288
1261.975601	151282.187837	35.433306
1263.218550	151520.123601	35.438324
1264.988975	151751.894678	35.443341
1266.356127	151971.533655	35.448359
1267.081958	152202.978862	35.453376
1268.653774	152422.154074	35.458394
1270.138591	152648.791359	35.463412
1271.358188	152860.075986	35.468429
1272.664951	153080.226253	35.473447
1273.468704	153305.119243	35.478464
1274.927759	153524.218447	35.483482
1275.629447	153755.930660	35.488500
1276.902807	153999.039149	35.493517
1278.033611	154226.557976	35.498535
1278.660753	154483.886066	35.503552
1279.309678	154730.835415	35.508570
1280.081795	154990.260420	35.513588
1281.356971	155253.964836	35.518605
1282.777325	155518.077446	35.523623
1283.434855	155791.887428	35.528640
1285.072791	156055.801405	35.533658
1285.848180	156337.548932	35.538676
1287.455321	156617.443426	35.543693
1288.621834	156880.694996	35.548711
1289.788950	157152.866546	35.553728
1291.119743	157414.888253	35.558746
1292.250933	157685.838930	35.563764
1293.629143	157943.301497	35.568781
1294.944861	158208.667376	35.573799
1295.591761	158500.068148	35.578816
1297.240345	158750.220044	35.583834
1298.902477	159024.171473	35.588852
1300.166953	159291.151578	35.593869
1301.564533	159562.068923	35.598887
1302.812296	159830.869563	35.603904
1304.222528	160117.888136	35.608922
1305.141720	160391.810748	35.613940
1306.897721	160662.749952	35.618957
1308.290249	160932.243314	35.623975
1309.757107	161206.318505	35.628992
1311.500120	161462.661828	35.634010
1312.716241	161734.448833	35.639028
1313.622306	162010.997752	35.644045
1315.738305	162283.776091	35.649063
1316.589756	162564.436049	35.654080
1318.013690	162841.980117	35.659098
1318.640801	163123.202298	35.664116
1319.813845	163411.894931	35.669133
1321.057363	163702.252245	35.674151
1322.003658	164005.655107	35.679168
1323.754046	164284.395916	35.684186
1325.208226	164567.287543	35.689204
1326.737104	164851.348223	35.694221
1328.498502	165135.599318	35.699239
1329.943412	165420.388572	35.704256
1331.574430	165703.028774	35.709274
1332.975743	165992.232122	35.714292
1333.956019	166274.048341	35.719309
1335.413191	166547.130826	35.724327
1336.598412	166843.355555	35.729344
1338.005948	167127.844799	35.734362
1339.288117	167417.978598	35.739380
1340.029732	167708.308280	35.744397
1341.652705	167991.750896	35.749415
1342.966314	168293.432180	35.754432
1344.853193	168577.455020	35.759450
1346.769468	168862.388227	35.764468
1348.719376	169118.105811	35.769485
1350.654735	169386.669308	35.774503
1351.866397	169660.167662	35.779520
1352.787867	169914.479419	35.784538
1353.955968	170190.437471	35.789556
1354.860216	170469.234109	35.794573
1355.686233	170757.982136	35.799591
1357.069900	171045.354765	35.804608
1358.354069	171325.322359	35.809626
1359.687096	171604.255316	35.814644
1361.480322	171894.570571	35.819661
1362.747415	172160.485001	35.824679
1364.184232	172440.458363	35.829696
1365.708285	172698.070225	35.834714
1367.428296	172955.434175	35.839732
1368.686331	173214.502977	35.844749
1370.350956	173474.239631	35.849767
1371.798606	173730.512116	35.854784
1373.089802	173966.024936	35.859802
1375.030897	174221.009882	35.864820
1375.931738	174472.722221	35.869837
1376.849555	174727.174219	35.874855
1378.347799	174996.643411	35.879872
1379.628759	175253.510733	35.884890
1380.999948	175512.787979	35.889908
1382.000173	175790.494533	35.894925
1383.287576	176065.780159	35.899943
1384.291827	176345.507025	35.904960
1385.195059	176631.839679	35.909978
1385.978478	176921.392758	35.914996
1387.429750	177230.492728	35.920013
1388.830455	177520.425832	35.925031
1389.956334	177838.532907	35.930048
1391.199532	178145.325979	35.935066
1392.841246	178458.893687	35.940084
1393.721842	178777.568876	35.945101
1395.762839	179086.769381	35.950119
1397.582642	179395.476490	35.955136
1399.589881	179695.408281	35.960154
1400.879987	179997.000299	35.965172
1402.295410	180298.306038	35.970189
1404.008416	180598.800993	35.975207
1405.242170	180910.193809	35.980224
1406.238881	181207.210050	35.985242
1407.680504	181511.818233	35.990260
1408.529709	181827.635789	35.995277
1410.370706	182132.839132	36.000295
1411.511438	182460.351437	36.005312
1413.205550	182773.186614	36.010330
1414.501634	183091.372048	36.015348
1415.568358	183422.329891	36.020365
1417.099331	183730.476511	36.025383
1418.756495	184070.692128	36.030400
1420.385224	184401.089928	36.035418
1421.409221	184717.681043	36.040436
1422.675967	185052.841218	36.045453
1424.214909	185376.240508	36.050471
1425.145169	185720.538184	36.055488
1426.706459	186053.445102	36.060506
1428.103727	186387.105567	36.065524
1429.232892	186735.856209	36.070541
1430.962165	187066.277563	36.075559
1432.313948	187418.865871	36.080576
1433.931324	187794.844353	36.085594
1435.921650	188120.657037	36.090612
1437.748692	188459.600027	36.095629
1440.098541	188765.323020	36.100647
1444.433589	188997.181404	36.105664
1446.577398	189243.887455	36.110682
1448.731045	189473.658273	36.115700
1449.849333	189711.604766	36.120717
1451.401709	189935.310650	36.125735
1452.249951	190169.331716	36.130752
1453.270605	190395.618449	36.135770
1454.495404	190627.621825	36.140788
1455.691817	190877.467210	36.145805
1456.943760	191113.580902	36.150823
1457.887302	191363.661945	36.155840
1459.056970	191612.169196	36.160858
1460.051347	191882.454075	36.165876
1460.883474	192156.627200	36.170893
1461.758478	192433.333211	36.175911
1463.168247	192728.306218	36.180928
1464.551969	193017.838768	36.185946
1465.467413	193316.415685	36.190964
1466.677123	193617.152629	36.195981
1467.785631	193930.959236	36.200999
1468.959804	194264.942022	36.206016
1470.263323	194587.795730	36.211034
1471.417833	194919.004882	36.216052
1471.784522	195265.978961	36.221069
1473.414632	195611.621407	36.226087
1474.229303	195968.767991	36.231104
1475.982506	196341.257591	36.236122
1477.755805	196693.648036	36.241140
1479.143961	197062.598412	36.246157
1480.645446	197421.171339	36.251175
1482.012640	197793.214394	36.256192
1483.387826	198173.802672	36.261210
1485.098681	198545.486236	36.266228
1486.280285	198935.964154	36.271245
1488.075423	199294.432987	36.276263
1489.772226	199678.186575	36.281280
1491.274563	200054.382930	36.286298
1492.770491	200432.639209	36.291316
1494.198315	200813.334195	36.296333
1496.482610	201186.482361	36.301351
1497.645485	201565.271291	36.306368
1499.314504	201942.934396	36.311386
1501.178849	202321.632539	36.316404
1502.736135	202709.171511	36.321421
1504.273783	203079.942925	36.326439
1505.721625	203453.321742	36.331456
1506.934508	203824.901486	36.336474
1508.951936	204198.884802	36.341492
1510.656339	204569.774540	36.346509
1512.424763	204931.157401	36.351527
1513.793063	205298.946441	36.356544
1515.344277	205669.461253	36.361562
1517.118649	206039.736433	36.366580
1518.585516	206411.983287	36.371597
1520.089786	206770.956329	36.376615
1521.844178	207109.076489	36.381632
1523.357778	207457.270531	36.386650
1525.397800	207784.792689	36.391668
1527.373773	208124.910744	36.396685
1529.120701	208437.387777	36.401703
1531.091014	208747.338928	36.406720
1532.828133	209058.981865	36.411738
1534.586053	209368.082754	36.416756
1535.704350	209685.395634	36.421773
1537.358275	210002.237071	36.426791
1538.845502	210313.520953	36.431808
1540.242668	210629.824478	36.436826
1541.826228	210952.979741	36.441844
1543.459699	211265.080036	36.446861
1544.905481	211584.146879	36.451879
1545.994312	211902.209259	36.456896
1547.305888	212230.342658	36.461914
1549.235083	212557.889000	36.466932
1549.856888	212892.136517	36.471949
1551.210366	213229.688670	36.476967
1552.516601	213570.424798	36.481984
1553.842809	213917.203343	36.487002
1555.807150	214269.766197	36.492020
1557.280405	214619.849212	36.497037
1558.642168	214977.292531	36.502055
1559.574491	215346.874634	36.507072
1561.191061	215722.106376	36.512090
1562.645276	216084.515891	36.517108
1564.571093	216462.084914	36.522125
1565.941428	216844.068101	36.527143
1567.668886	217211.184364	36.532160
1568.714849	217604.680538	36.537178
1570.269615	217982.471030	36.542196
1571.400265	218379.130436	36.547213
1573.072228	218771.203120	36.552231
1574.538506	219176.976996	36.557248
1576.402508	219571.559605	36.562266
1578.034277	219959.503433	36.567284
1579.057173	220373.764668	36.572301
1580.481005	220782.498000	36.577319
1582.502449	221177.567331	36.582336
1583.651593	221597.297671	36.587354
1585.320627	222004.317037	36.592372
1586.627537	222424.048750	36.597389
1588.399604	222839.740008	36.602407
1590.034598	223257.411934	36.607424
1591.924983	223673.187405	36.612442
1593.464444	224077.187973	36.617460
1595.122466	224507.001336	36.622477
1596.679862	224919.129532	36.627495
1598.809400	225331.237354	36.632512
1600.185982	225753.686210	36.637530
1602.178452	226166.709126	36.642548
1603.753128	226584.757882	36.647565
1605.462060	226990.897543	36.652583
1606.841190	227390.998709	36.657600
1608.061798	227790.213729	36.662618
1609.706173	228183.947026	36.667636
1611.372506	228585.577281	36.672653
1612.811584	228982.700789	36.677671
1614.354434	229389.104335	36.682688
1615.487471	229786.968186	36.687706
1617.027020	230195.355750	36.692724
1618.371916	230620.364613	36.697741
1619.611160	231049.507696	36.702759
1621.351899	231475.517984	36.707776
1622.542033	231914.781473	36.712794
1624.262941	232346.817536	36.717812
1626.109093	232772.762346	36.722829
1628.052344	233198.767812	36.727847
1629.865558	233639.199252	36.732864
1631.254336	234086.537444	36.737882
1633.005556	234527.184896	36.742900
1634.488349	234973.264500	36.747917
1636.308732	235412.403517	36.752935
1637.733326	235868.020857	36.757952
1639.377759	236321.061453	36.762970
1640.656536	236770.964990	36.767988
1642.509524	237240.457840	36.773005
1643.956230	237711.164350	36.778023
1645.977634	238167.624573	36.783040
1647.522459	238641.643992	36.788058
1649.112845	239083.167146	36.793076
1651.378336	239540.121835	36.798093
1653.161490	239997.159930	36.803111
1655.132074	240445.098164	36.808128
1656.390117	240904.869629	36.813146
1658.542527	241361.313584	36.818164
1660.438377	241822.831919	36.823181
1661.670562	242266.428765	36.828199
1663.293101	242723.473703	36.833216
1665.153172	243176.084062	36.838234
1666.605558	243633.438946	36.843252
1668.481043	244096.894971	36.848269
1670.227554	244555.852039	36.853287
1672.272221	245013.513988	36.858304
1673.552108	245483.856375	36.863322
1675.362171	245938.612929	36.868340
1677.230943	246388.939885	36.873357
1678.280719	246855.614530	36.878375
1680.219053	247315.558320	36.883392
1682.081897	247795.990298	36.888410
1683.599036	248238.758498	36.893428
1685.679171	248695.275422	36.898445
1687.522389	249162.502563	36.903463
1689.454879	249606.801286	36.908480
1691.702119	250060.394834	36.913498
1693.968111	250499.912202	36.918516
1696.600280	250918.689093	36.923533
1698.824342	251328.797385	36.928551
1701.097511	251704.501664	36.933568
1703.226110	252069.205889	36.938586
1705.067157	252446.000555	36.943604
1706.850846	252799.891535	36.948621
1708.568409	253162.481833	36.953639
1710.236292	253524.750505	36.958656
1711.873800	253896.830105	36.963674
1713.070279	254256.436080	36.968692
1714.812555	254613.738679	36.973709
1716.252649	254988.468831	36.978727
1718.031836	255356.332972	36.983744
1719.115792	255729.117307	36.988762
1720.616729	256115.852908	36.993780
1722.486985	256498.130594	36.998797
1724.110909	256891.170584	37.003815
1725.180228	257283.543356	37.008832
1726.080382	257690.729712	37.013850
1727.257331	258104.498911	37.018868
1729.132020	258531.129718	37.023885
1730.055635	258965.696531	37.028903
1731.591467	259391.851662	37.033920
1733.084221	259847.380118	37.038938
1734.296309	260295.106854	37.043956
1735.747317	260765.096513	37.048973
1737.088240	261233.758421	37.053991
1738.717621	261706.790884	37.059008
1740.658089	262188.025868	37.064026
1742.529964	262665.538022	37.069044
1744.640009	263147.200610	37.074061
1746.117742	263630.800028	37.079079
1748.535661	264113.577730	37.084096
1750.404936	264596.321856	37.089114
1752.267675	265080.209788	37.094132
1753.975745	265562.497912	37.099149
1755.551375	266048.415408	37.104167
1757.232474	266523.111641	37.109184
1758.924057	267024.503966	37.114202
1760.287123	267520.693471	37.119220
1762.202644	268017.016441	37.124237
1764.006891	268519.937087	37.129255
1765.680500	269025.521237	37.134272
1767.874874	269520.193982	37.139290
1769.616894	270023.529445	37.144308
1771.669830	270528.639884	37.149325
1773.188232	271037.397266	37.154343
1775.050822	271533.774636	37.159360
1776.858487	272035.571239	37.164378
1778.874160	272525.442979	37.169396
1781.431480	273018.218614	37.174413
1783.146922	273504.354878	37.179431
1785.092281	274010.137608	37.184448
1786.446083	274495.266834	37.189466
1788.638421	274986.170299	37.194484
1790.697631	275480.346933	37.199501
1792.364536	275962.599785	37.204519
1794.638714	276413.223776	37.209536
1796.427731	276876.884776	37.214554
1798.382363	277331.270099	37.219572
1800.028723	277780.753759	37.224589
1801.830724	278237.042830	37.229607
1803.557962	278688.415664	37.234624
1805.369374	279148.282555	37.239642
1807.140368	279604.573578	37.244660
1808.820602	280062.657068	37.249677
1810.600633	280528.825350	37.254695
1812.625025	280983.291334	37.259712
1814.590357	281453.870624	37.264730
1815.652649	281917.719315	37.269748
1818.411869	282349.982168	37.274765
1820.833719	282802.825647	37.279783
1822.698139	283253.146865	37.284800
1824.151983	283707.550349	37.289818
1825.767794	284164.617256	37.294836
1827.850389	284623.787382	37.299853
1829.233608	285105.885538	37.304871
1831.457423	285564.241112	37.309888
1833.021019	286031.572927	37.314906
1834.607360	286503.725372	37.319924
1836.671724	286972.543178	37.324941
1838.373225	287454.121564	37.329959
1840.085120	287917.560697	37.334976
1841.339878	288394.894037	37.339994
1842.765828	288891.144726	37.345012
1844.621401	289380.766815	37.350029
1846.373411	289897.125285	37.355047
1847.980092	290393.389899	37.360064
1849.296055	290909.539284	37.365082
1850.666632	291429.156826	37.370100
1852.721048	291957.443280	37.375117
1854.345289	292489.991783	37.380135
1856.175254	293020.597681	37.385152
1857.962727	293565.050798	37.390170
1859.945094	294115.258847	37.395188
1861.598329	294655.233936	37.400205
1863.097161	295211.945012	37.405223
1864.907231	295761.488361	37.410240
1866.960027	296314.695464	37.415258
1868.957208	296870.372739	37.420276
1871.531925	297431.840545	37.425293
1873.527825	297977.682902	37.430311
1875.371185	298537.110756	37.435328
1877.406152	299092.362820	37.440346
1879.179762	299641.611788	37.445364
1880.996104	300185.618427	37.450381
1882.185787	300747.786507	37.455399
1885.072577	301295.971899	37.460416
1887.043109	301842.659934	37.465434
1888.989070	302391.228229	37.470452
1891.335197	302935.102538	37.475469
1893.122126	303475.361270	37.480487
1895.207576	304004.949965	37.485504
1897.374762	304517.810793	37.490522
1898.789788	305024.118057	37.495540
1900.971648	305548.931650	37.500557
1902.660654	306061.915692	37.505575
1904.456010	306588.261785	37.510592
1906.615497	307096.765490	37.515610
1908.414194	307611.422554	37.520628
1910.670501	308131.229418	37.525645
1912.430107	308649.111644	37.530663
1914.034385	309165.671110	37.535680
1915.729781	309694.680261	37.540698
1917.757764	310235.894351	37.545716
1919.864773	310756.902750	37.550733
1921.773765	311290.435252	37.555751
1923.215939	311818.000075	37.560768
1925.184391	312369.569649	37.565786
1926.766801	312926.127423	37.570804
1928.473033	313483.904023	37.575821
1929.977574	314053.518538	37.580839
1931.713073	314618.340545	37.585856
1933.061674	315189.089890	37.590874
1934.986541	315772.330629	37.595892
1936.955377	316362.059321	37.600909
1938.459728	316959.276821	37.605927
1940.271650	317567.710373	37.610944
1942.818469	318161.895057	37.615962
1944.241159	318774.878473	37.620980
1946.160211	319376.878543	37.625997
1947.964256	320000.322532	37.631015
1949.738450	320613.584003	37.636032
1951.838730	321234.223170	37.641050
1953.363786	321866.303971	37.646068
1955.753433	322495.132976	37.651085
1957.551510	323138.173349	37.656103
1959.595534	323770.272948	37.661120
1961.523738	324399.009059	37.666138
1963.687410	325055.575143	37.671156
1965.526740	325695.940890	37.676173
1967.383147	326338.607110	37.681191
1969.460560	326988.260927	37.686208
1971.533780	327628.794054	37.691226
1973.415986	328288.367805	37.696244
1975.798603	328931.626052	37.701261
1977.956136	329581.439858	37.706279
1980.043105	330228.186435	37.711296
1981.918643	330868.056613	37.716314
1983.968960	331512.382753	37.721332
1986.270985	332154.170454	37.726349
1989.243459	332800.303678	37.731367
1991.148946	333438.818423	37.736384
1992.726218	334064.156251	37.741402
1994.764401	334705.856876	37.746420
1997.421135	335328.456614	37.751437
1999.566317	335946.414999	37.756455
2001.085851	336558.076349	37.761472
2003.685665	337137.969052	37.766490
2005.618326	337728.274642	37.771508
2008.070535	338311.022001	37.776525
2010.441773	338893.522591	37.781543
2013.071303	339468.839852	37.786560
2015.644769	340034.641871	37.791578
2017.147276	340600.823550	37.796596
2019.205707	341167.690380	37.801613
2020.827480	341737.772442	37.806631
2022.817709	342308.266948	37.811648
2025.078924	342875.891086	37.816666
2026.729268	343463.612187	37.821684
2028.596893	344047.177305	37.826701
2030.733172	344627.212238	37.831719
2032.496139	345211.973470	37.836736
2034.382831	345792.493286	37.841754
2035.941250	346397.551859	37.846772
2037.619038	347000.678628	37.851789
2040.352107	347612.955812	37.856807
2041.484557	348215.931159	37.861824
2044.099302	348821.334809	37.866842
2046.236138	349432.039462	37.871860
2048.684130	350039.332771	37.876877
2050.958563	350634.492314	37.881895
2053.181115	351240.614758	37.886912
2055.466122	351846.718002	37.891930
2057.218927	352458.866741	37.896948
2059.042308	353055.846121	37.901965
2061.623822	353668.901416	37.906983
2063.328979	354280.245356	37.912000
2065.426592	354884.992315	37.917018
2067.277528	355502.763561	37.922036
2069.408972	356128.825137	37.927053
2071.321169	356745.273247	37.932071
2073.178276	357377.604143	37.937088
2075.247694	357999.258277	37.942106
2076.649376	358652.045620	37.947124
2078.680830	359289.238612	37.952141
2081.002318	359929.390828	37.957159
2082.872429	360581.711183	37.962176
2084.899905	361223.135743	37.967194
2086.941856	361882.965045	37.972212
2088.885055	362530.014325	37.977229
2090.960800	363193.265564	37.982247
2093.089575	363850.813913	37.987264
2095.066404	364506.271405	37.992282
2097.293238	365175.220565	37.997300
2099.365757	365830.131329	38.002317
2101.944290	366501.127418	38.007335
2103.761878	367173.129273	38.012352
2106.038984	367838.141077	38.017370
2108.241925	368519.133035	38.022388
2110.460646	369184.688329	38.027405
2111.850008	369845.757063	38.032423
2113.735216	370508.250650	38.037440
2116.108368	371148.405640	38.042458
2117.875154	371803.337410	38.047476
2119.867429	372449.722380	38.052493
2122.166596	373106.491765	38.057511
2123.998002	373766.574958	38.062528
2126.283311	374432.958761	38.067546
2128.894219	375092.097273	38.072564
2130.824913	375737.518720	38.077581
2133.079832	376386.676350	38.082599
2135.499565	377054.203446	38.087616
2137.686080	377719.880776	38.092634
2139.600994	378392.158878	38.097652
2141.927937	379059.636679	38.102669
2144.310247	379720.169388	38.107687
2146.625450	380384.351595	38.112704
2148.439685	381047.667912	38.117722
2151.073085	381706.064052	38.122740
2153.515157	382365.645876	38.127757
2156.086544	383021.668002	38.132775
2158.590135	383667.978128	38.137792
2161.363225	384312.505161	38.142810
2163.710178	384958.156808	38.147828
2166.093426	385594.206223	38.152845
2168.799850	386226.156745	38.157863
2170.527524	386870.531548	38.162880
2172.598193	387510.068620	38.167898
2174.673226	388153.242116	38.172916
2176.652554	388791.069978	38.177933
2178.676732	389435.949168	38.182951
2180.858971	390092.980087	38.187968
2183.387030	390734.146331	38.192986
2185.455655	391386.149963	38.198004
2187.121793	392047.358322	38.203021
2189.303147	392703.673707	38.208039
2190.648047	393375.831669	38.213056
2192.817158	394055.969121	38.218074
2194.613354	394730.274908	38.223092
2197.038472	395407.498931	38.228109
2199.075384	396096.710123	38.233127
2200.940300	396791.382997	38.238144
2202.881327	397483.314682	38.243162
2205.345133	398192.017468	38.248180
2206.820522	398901.860033	38.253197
2209.139290	399612.148927	38.258215
2210.938554	400333.328667	38.263232
2213.111979	401064.282684	38.268250
2215.129409	401790.202183	38.273268
2217.357153	402521.387690	38.278285
2219.734726	403262.536264	38.283303
2221.752119	404000.331615	38.288320
2224.529649	404730.427429	38.293338
2227.133882	405467.627061	38.298356
2229.096698	406202.940421	38.303373
2231.885456	406916.736958	38.308391
2233.649927	407633.957636	38.313408
2236.079618	408336.910402	38.318426
2238.400640	409049.261090	38.323444
2240.158397	409748.289299	38.328461
2242.667902	410453.097705	38.333479
2244.347243	411172.390749	38.338496
2246.386271	411898.238621	38.343514
2248.288407	412626.495872	38.348532
2249.986678	413363.226769	38.353549
2252.463154	414099.575741	38.358567
2254.357424	414845.398935	38.363584
2256.485672	415602.987059	38.368602
2258.407131	416364.563911	38.373620
2260.691922	417128.689431	38.378637
2263.000450	417900.485798	38.383655
2265.169993	418675.422132	38.388672
2267.470039	419444.640326	38.393690
2270.197525	420221.864103	38.398708
2272.670390	421008.323236	38.403725
2274.856400	421786.096832	38.408743
2276.714771	422574.839008	38.413760
2278.993152	423370.066292	38.418778
2281.521269	424173.832299	38.423796
2283.654269	424973.183718	38.428813
2285.720823	425772.823751	38.433831
2287.640054	426594.029293	38.438848
2289.743447	427417.503843	38.443866
2292.708390	428232.095358	38.448884
2295.101334	429063.664135	38.453901
2297.836826	429871.100604	38.458919
2299.997330	430686.554521	38.463936
2302.283227	431493.708021	38.468954
2305.164103	432311.816253	38.473972
2307.239034	433149.367243	38.478989
2309.325224	433967.805525	38.484007
2311.713136	434805.040032	38.489024
2313.662450	435641.559592	38.494042
2315.822644	436477.506141	38.499060
2318.123723	437315.725336	38.504077
2320.703084	438153.359609	38.509095
2323.073975	438994.995432	38.514112
2325.276185	439844.824995	38.519130
2327.523454	440690.617137	38.524148
2330.007824	441547.517421	38.529165
2333.338531	442369.027711	38.534183
2336.492321	443196.658635	38.539200
2338.861428	444019.232164	38.544218
2341.525048	444841.319338	38.549236
2343.914862	445665.394665	38.554253
2346.796360	446471.448183	38.559271
2349.242209	447279.973534	38.564288
2351.405283	448087.353125	38.569306
2353.820865	448897.946167	38.574324
2356.298238	449690.189511	38.579341
2358.633669	450484.753497	38.584359
2360.817413	451267.378513	38.589376
2363.198787	452034.112286	38.594394
2365.407253	452802.414782	38.599412
2367.536206	453581.674816	38.604429
2369.626879	454350.748663	38.609447
2371.660137	455132.140301	38.614464
2373.349528	455930.144121	38.619482
2375.395451	456729.723993	38.624500
2376.826280	457541.712793	38.629517
2379.249027	458364.064847	38.634535
2381.059523	459197.912294	38.639552
2383.437803	460049.016598	38.644570
2386.129920	460882.642780	38.649588
2387.746300	461748.462850	38.654605
2390.199393	462604.751551	38.659623
2391.969513	463482.194750	38.664640
2394.056535	464363.941133	38.669658
2396.280099	465256.590348	38.674676
2398.402616	466157.300942	38.679693
2400.771074	467064.647966	38.684711
2402.761581	467984.396076	38.689728
2405.206091	468903.264417	38.694746
2408.182065	469840.438482	38.699764
2410.018638	470780.236414	38.704781
2413.046820	471714.681476	38.709799
2415.600859	472657.445592	38.714816
2417.911507	473597.425504	38.719834
2420.613495	474539.614492	38.724852
2422.759622	475502.811308	38.729869
2425.766875	476444.446876	38.734887
2428.394922	477403.572841	38.739904
2431.190575	478342.015787	38.744922
2434.016793	479283.535914	38.749940
2436.713761	480225.736094	38.754957
2439.398263	481163.395357	38.759975
2442.087057	482101.610775	38.764992
2444.634750	483036.065028	38.770010
2447.177025	483964.211099	38.775028
2449.381457	484903.674173	38.780045
2452.186655	485835.967992	38.785063
2454.262119	486768.084690	38.790080
2456.863763	487709.399405	38.795098
2459.469372	488642.839627	38.800116
2461.725802	489591.278321	38.805133
2464.179876	490524.643006	38.810151
2466.636689	491469.663905	38.815168
2469.190149	492412.194111	38.820186
2471.618903	493349.597429	38.825204
2474.102072	494303.892338	38.830221
2477.028489	495249.935037	38.835239
2479.425838	496193.139501	38.840256
2481.739019	497126.872033	38.845274
2484.589327	498077.863390	38.850292
2486.627275	499020.465377	38.855309
2489.255569	499956.154343	38.860327
2492.243381	500866.310014	38.865344
2494.568538	501772.040191	38.870362
2497.135731	502670.770230	38.875380
2499.098740	503581.555442	38.880397
2501.766170	504482.185511	38.885415
2504.402504	505397.241467	38.890432
2506.308918	506323.058797	38.895450
2508.589858	507241.347912	38.900468
2510.607115	508180.550265	38.905485
2512.777263	509117.402848	38.910503
2514.694617	510064.173339	38.915520
2517.156357	511025.310132	38.920538
2519.287787	511985.638434	38.925556
2521.340638	512969.355766	38.930573
2523.770947	513931.428914	38.935591
2526.582480	514933.840697	38.940608
2528.954763	515931.576880	38.945626
2531.309757	516935.297670	38.950644
2533.619944	517954.729689	38.955661
2535.812139	518970.940412	38.960679
2538.950129	519991.908887	38.965696
2541.309546	521019.892971	38.970714
2544.274061	522055.460374	38.975732
2546.540664	523097.975737	38.980749
2548.858337	524135.071984	38.985767
2551.696124	525179.863060	38.990784
2553.716765	526243.753808	38.995802
2556.070369	527296.082278	39.000820
2558.843540	528372.329194	39.005837
2561.285575	529438.838159	39.010855
2564.257643	530508.148951	39.015872
2566.572818	531596.620700	39.020890
2568.981859	532668.889287	39.025908
2571.585385	533757.049165	39.030925
2574.440433	534842.215618	39.035943
2577.074102	535936.496024	39.040960
2579.426090	537037.583768	39.045978
2582.636940	538120.227045	39.050996
2584.939260	539223.367806	39.056013
2587.552382	540316.660847	39.061031
2590.604952	541420.457416	39.066048
2592.854890	542523.499546	39.071066
2595.793807	543617.234081	39.076084
2598.369493	544730.104275	39.081101
2600.711294	545833.471766	39.086119
2603.758595	546941.356774	39.091136
2606.408859	548047.661797	39.096154
2609.288647	549144.940175	39.101172
2612.477090	550241.574846	39.106189
2615.330794	551332.800005	39.111207
2618.487484	552410.717455	39.116224
2620.632934	553494.450602	39.121242
2623.550561	554570.125157	39.126260
2626.194771	555658.321720	39.131277
2628.478919	556733.779460	39.136295
2631.418145	557780.904280	39.141312
2634.146872	558837.426363	39.146330
2636.577550	559875.881713	39.151348
2639.542754	560915.268597	39.156365
2641.882982	561962.815840	39.161383
2644.351126	563002.222000	39.166400
2646.932939	564050.212771	39.171418
2649.524769	565089.279841	39.176436
2652.242522	566147.119476	39.181453
2655.264939	567194.076576	39.186471
2658.068559	568222.361726	39.191488
2660.676595	569279.609922	39.196506
2663.261034	570337.778042	39.201524
2665.440453	571409.778370	39.206541
2667.859721	572467.445210	39.211559
2670.910902	573528.226872	39.216576
2673.149620	574609.829359	39.221594
2675.816363	575673.304531	39.226612
2678.655936	576759.233421	39.231629
2681.227232	577848.774747	39.236647
2683.896956	578932.686033	39.241664
2686.342928	580043.521573	39.246682
2688.803602	581145.478320	39.251700
2691.520213	582246.640140	39.256717
2693.678843	583364.744286	39.261735
2696.348784	584498.449961	39.266752
2698.917257	585632.317303	39.271770
2701.513998	586761.612087	39.276788
2704.200580	587895.546552	39.281805
2706.927867	589048.309645	39.286823
2710.098021	590195.874610	39.291840
2712.934806	591342.132971	39.296858
2716.361343	592485.674491	39.301876
2718.849251	593630.317379	39.306893
2721.606445	594773.350070	39.311911
2724.788895	595923.310461	39.316928
2727.111367	597072.903686	39.321946
2730.109459	598223.118974	39.326964
2732.906786	599373.154095	39.331981
2735.290905	600526.098945	39.336999
2738.964199	601665.992640	39.342016
2742.181960	602801.295648	39.347034
2745.130401	603932.227383	39.352052
2748.127252	605070.344905	39.357069
2750.967320	606202.219962	39.362087
2754.169745	607328.715995	39.367104
2756.840086	608448.536151	39.372122
2759.980438	609568.064116	39.377140
2762.867177	610680.820563	39.382157
2765.714620	611807.226635	39.387175
2768.909692	612905.603494	39.392192
2771.478953	614030.030748	39.397210
2774.295946	615137.701072	39.402228
2776.840021	616246.506232	39.407245
2779.306828	617354.312518	39.412263
2781.954868	618426.186369	39.417280
2784.347022	619515.941093	39.422298
2786.730628	620595.642805	39.427316
2789.117756	621681.132519	39.432333
2791.599699	622771.593098	39.437351
2794.821863	623858.519176	39.442368
2797.389006	624968.625690	39.447386
2799.806803	626064.206907	39.452404
2802.533582	627181.947529	39.457421
2805.027970	628301.108189	39.462439
2807.411330	629420.818446	39.467456
2809.817796	630568.015993	39.472474
2812.577827	631719.271219	39.477492
2814.950048	632879.501027	39.482509
2817.180101	634060.788505	39.487527
2819.682080	635240.448032	39.492544
2822.108397	636443.139732	39.497562
2824.040867	637657.401012	39.502580
2827.257284	638870.052459	39.507597
2830.027837	640107.428057	39.512615
2832.885171	641348.678928	39.517632
2835.332299	642598.625646	39.522650
2838.196924	643852.435878	39.527668
2841.547596	645104.810989	39.532685
2843.998751	646391.531552	39.537703
2846.986355	647663.540558	39.542720
2849.891339	648943.774763	39.547738
2852.447942	650239.451609	39.552756
2855.396768	651524.030462	39.557773
2857.995694	652831.867416	39.562791
2860.693527	654151.568571	39.567808
2863.457826	655471.479543	39.572826
2866.007326	656798.221061	39.577844
2868.704722	658125.702892	39.582861
2871.629848	659472.828742	39.587879
2874.657455	660808.549568	39.592896
2877.716928	662146.518790	39.597914
2880.360084	663504.228823	39.602932
2883.986767	664866.106272	39.607949
2886.455178	666229.230922	39.612967
2889.911531	667576.222875	39.617984
2892.862280	668936.389095	39.623002
2895.616694	670294.552872	39.628020
2898.951338	671650.681137	39.633037
2901.710859	673018.891334	39.638055
2904.787607	674369.797362	39.643072
2907.862299	675734.671976	39.648090
2910.831972	677093.847697	39.653108
2913.868275	678459.867293	39.658125
2916.891407	679822.208941	39.663143
2919.771791	681174.190171	39.668160
2922.684387	682550.350344	39.673178
2925.859489	683903.366565	39.678196
2929.427762	685248.070868	39.683213
2932.180046	686597.430393	39.688231
2935.325549	687906.516238	39.693248
2938.166192	689203.553012	39.698266
2941.126733	690501.572187	39.703284
2944.121845	691792.550132	39.708301
2947.078186	693106.264531	39.713319
2950.086652	694397.406911	39.718336
2952.945549	695697.907341	39.723354
2955.512239	696999.009277	39.728372
2958.704312	698300.604650	39.733389
2961.244092	699614.360929	39.738407
2964.399967	700941.740385	39.743424
2966.772451	702265.086586	39.748442
2969.621390	703593.004562	39.753460
2972.475833	704931.565923	39.758477
2975.541278	706276.965630	39.763495
2978.476893	707623.265795	39.768512
2981.285564	708981.704428	39.773530
2984.283644	710336.428537	39.778548
2987.193235	711689.615008	39.783565
2989.556032	713062.870310	39.788583
2992.855499	714442.026107	39.793600
2996.144078	715822.837295	39.798618
2999.035710	717210.512610	39.803636
3001.841190	718609.693205	39.808653
3004.591306	720014.087176	39.813671
3007.986462	721406.761614	39.818688
3010.729320	722810.978558	39.823706
3013.445217	724235.965569	39.828724
3016.532306	725665.088944	39.833741
3019.285961	727091.351419	39.838759
3022.046462	728526.550940	39.843776
3024.924758	729980.343108	39.848794
3027.815976	731447.549986	39.853812
3030.672227	732900.128848	39.858829
3033.437085	734375.710070	39.863847
3036.670544	735853.456222	39.868864
3039.981042	737333.777330	39.873882
3042.834480	738814.196768	39.878900
3046.251787	740295.426989	39.883917
3049.101832	741797.829769	39.888935
3052.294462	743291.850117	39.893952
3055.398157	744780.079571	39.898970
3058.168529	746264.829362	39.903988
3061.866349	747757.416214	39.909005
3065.312265	749258.971984	39.914023
3068.986852	750734.976332	39.919040
3072.123364	752232.114697	39.924058
3075.099858	753723.670430	39.929076
3078.611801	755193.822489	39.934093
3081.327256	756683.810639	39.939111
3084.575857	758165.344872	39.944128
3088.302192	759640.357366	39.949146
3091.189051	761126.342170	39.954164
3094.649346	762595.656080	39.959181
3097.204346	764057.362242	39.964199
3100.573075	765487.179028	39.969216
3103.603374	766923.070634	39.974234
3106.048241	768346.744021	39.979252
3109.586184	769773.003075	39.984269
3112.915447	771206.783579	39.989287
3115.607328	772629.489490	39.994304
3119.225604	774050.091267	39.999322
3122.284197	775485.535703	40.004340
3125.458212	776908.454692	40.009357
3128.520498	778336.266757	40.014375
3131.837594	779764.832869	40.019392
3135.048467	781200.051115	40.024410
3137.961637	782635.229702	40.029428
3141.199677	784070.261389	40.034445
3144.043701	785519.535194	40.039463
3146.798654	786968.333011	40.044480
3150.123057	788431.881171	40.049498
3152.966973	789901.529146	40.054516
3155.711692	791383.428413	40.059533
3158.500913	792868.386923	40.064551
3161.186021	794370.431451	40.069568
3164.122197	795888.412187	40.074586
3166.854282	797421.807904	40.079604
3169.878531	798948.648892	40.084621
3172.910176	800505.141234	40.089639
3175.609999	802057.767858	40.094656
3178.694511	803624.012182	40.099674
3181.657953	805201.749858	40.104692
3185.103959	806764.132059	40.109709
3188.198636	808368.484926	40.114727
3191.481818	809964.706286	40.119744
3194.776284	811562.550672	40.124762
3197.916431	813176.302785	40.129780
3201.011816	814799.340309	40.134797
3204.117642	816416.466221	40.139815
3207.264668	818048.221419	40.144832
3210.615024	819679.735519	40.149850
3213.426183	821322.254042	40.154868
3216.478364	822967.393648	40.159885
3219.710254	824622.668416	40.164903
3222.464248	826282.723011	40.169920
3226.251007	827938.280584	40.174938
3229.388017	829605.704585	40.179956
3232.745962	831267.450558	40.184973
3236.329502	832941.582676	40.189991
3239.403691	834612.347890	40.195008
3243.009213	836270.762132	40.200026
3245.826837	837947.122551	40.205044
3249.296876	839621.032957	40.210061
3252.794626	841301.692404	40.215079
3255.778198	842990.450175	40.220096
3259.336067	844668.354510	40.225114
3262.448686	846346.080214	40.230132
3266.057832	848019.968020	40.235149
3269.579264	849671.376307	40.240167
3272.492057	851304.682160	40.245184
3276.598842	852923.861336	40.250202
3279.993279	854536.623512	40.255220
3283.680332	856134.360778	40.260237
3287.101779	857740.746187	40.265255
3290.194988	859341.722973	40.270272
3293.571407	860928.562375	40.275290
3296.457691	862532.513893	40.280308
3300.067522	864132.234750	40.285325
3303.243537	865739.062942	40.290343
3306.646772	867348.133718	40.295360
3310.010487	868943.516353	40.300378
3313.115552	870553.227068	40.305396
3316.461958	872168.266106	40.310413
3319.365351	873795.128337	40.315431
3322.434973	875418.806698	40.320448
3326.079222	877049.769863	40.325466
3329.133204	878692.847983	40.330484
3332.567083	880334.916756	40.335501
3336.049635	881982.986477	40.340519
3338.537092	883641.863647	40.345536
3341.975517	885295.083646	40.350554
3345.266506	886983.274041	40.355572
3348.436819	888659.026325	40.360589
3351.680832	890347.876135	40.365607
3354.585372	892047.470029	40.370624
3358.008447	893746.854014	40.375642
3360.784027	895466.558400	40.380660
3363.929441	897194.732637	40.385677
3367.036030	898928.354923	40.390695
3369.842159	900687.295680	40.395712
3373.289777	902437.971259	40.400730
3376.515049	904201.990677	40.405748
3380.411048	905976.493573	40.410765
3383.762877	907740.617494	40.415783
3386.424409	909538.515475	40.420800
3390.171735	911322.092200	40.425818
3393.436573	913117.947288	40.430836
3396.786797	914913.485951	40.435853
3400.324396	916718.672397	40.440871
3403.925442	918521.232475	40.445888
3407.223773	920334.179807	40.450906
3410.540872	922155.720576	40.455924
3413.908769	923968.006998	40.460941
3417.472848	925801.113228	40.465959
3420.799192	927626.732388	40.470976
3424.586133	929457.391988	40.475994
3427.796513	931291.250911	40.481012
3431.008075	933115.955035	40.486029
3434.645887	934953.059937	40.491047
3437.749831	936798.792928	40.496064
3441.228077	938639.029722	40.501082
3444.568779	940485.424524	40.506100
3447.943123	942334.213251	40.511117
3451.788159	944162.622183	40.516122
3455.297434	945943.588209	40.521127
3458.696729	947661.573427	40.526132
3461.839730	949322.211588	40.531136
3465.094939	950918.699883	40.536141
3468.830863	952468.491576	40.541146
3471.841176	953944.643358	40.546151
3474.893114	955332.963362	40.551156
3478.261190	956634.251924	40.556160
3481.487952	957851.879527	40.561165
3484.372563	958999.747530	40.566170
3486.872406	960066.444049	40.571175
3489.642300	961045.536330	40.576180
3491.791919	961961.407920	40.581184
3494.041314	962793.601116	40.586189
3496.358094	963553.219932	40.591194
3498.123604	964258.605082	40.596199
3500.144199	964886.932419	40.601204
3502.128346	965462.155609	40.606208
3503.992816	965988.903951	40.611213
3505.526955	966444.526422	40.616218
3506.719497	966844.109203	40.621223
3508.189437	967194.700205	40.626228
3509.730895	967511.604756	40.631232
3510.827335	967780.830029	40.636237
3512.234339	968001.569037	40.641242
3513.405945	968180.180843	40.646247
3514.487721	968313.514481	40.651252
3515.387420	968409.707331	40.656256
3516.266746	968468.342417	40.661261
3517.282110	968497.023485	40.666266
3518.165882	968511.935523	40.671271
3518.925682	968473.365907	40.676276
3520.042534	968417.715703	40.681280
3520.193757	968328.092729	40.686285
3521.250528	968225.304275	40.691290
3521.534189	968084.986004	40.696295
3522.392306	967939.381745	40.701300
3522.863033	967765.471088	40.706304
3523.594310	967565.488709	40.711309
3524.136228	967338.726037	40.716314
3524.421383	967112.976588	40.721319
3525.093637	966858.681031	40.726324
3525.555257	966590.516362	40.731328
3525.513556	966319.391784	40.736333
3526.244396	966018.570827	40.741338
3526.239024	965713.358285	40.746343
3527.018970	965394.783817	40.751348
3527.174511	965062.205029	40.756352
3527.747624	964711.232953	40.761357
3528.164542	964358.210589	40.766362
3528.166969	963999.266128	40.771367
3528.538557	963612.434243	40.776372
3528.931568	963219.013292	40.781376
3528.907174	962820.153823	40.786381
3529.468625	962421.362512	40.791386
3529.380965	962014.233091	40.796391
3529.836781	961593.761689	40.801396
3530.181434	961173.082668	40.806400
3530.140989	960730.107525	40.811405
3530.383000	960289.107044	40.816410
3530.449191	959852.217054	40.821415
3530.629591	959392.252360	40.826420
3530.781806	958929.806385	40.831424
3530.810584	958465.776639	40.836429
3530.986475	958005.114055	40.841434
3531.251690	957539.107515	40.846439
3531.495061	957047.585456	40.851444
3531.245941	956567.475244	40.856448
3531.510123	956080.767934	40.861453
3532.039361	955594.562499	40.866458
3531.455483	955114.780606	40.871463
3532.041480	954604.462422	40.876468
3532.025517	954108.027824	40.881472
3532.191325	953605.341426	40.886477
3532.757484	953096.266234	40.891482
3532.451921	952580.527314	40.896487
3531.936212	952054.772925	40.901492
3531.732714	951544.515266	40.906496
3532.013104	951029.322637	40.911501
3532.212225	950511.855178	40.916506
3532.371762	950020.965631	40.921511
3532.748661	949502.637832	40.926516
3533.202925	948993.809415	40.931520
3532.830262	948472.348352	40.936525
3533.108566	947944.599909	40.941530
3533.031872	947416.092148	40.946535
3532.864706	946875.679436	40.951540
3532.875857	946358.147788	40.956544
3533.011491	945833.077166	40.961549
3532.917956	945300.621409	40.966554
3532.695746	944771.578780	40.971559
3532.470159	944243.726952	40.976564
3532.500894	943720.756311	40.981568
3532.661739	943187.942804	40.986573
3532.850278	942663.593150	40.991578
3532.560021	942142.049628	40.996583
3532.922817	941606.452456	41.001588
3532.963627	941066.256425	41.006592
3532.982820	940532.618658	41.011597
3533.119155	939995.360651	41.016602
3533.165168	939449.246110	41.021607
3533.037686	938896.203307	41.026612
3533.094916	938354.380515	41.031616
3533.097465	937812.894128	41.036621
3533.131773	937262.909500	41.041626
3532.931330	936721.536209	41.046631
3533.013139	936163.757280	41.051636
3533.107130	935611.095417	41.056640
3533.116134	935058.197901	41.061645
3533.286165	934510.490211	41.066650
3533.151534	933966.326786	41.071655
3533.127392	933406.353833	41.076660
3533.200710	932851.294054	41.081664
3533.025764	932294.874660	41.086669
3532.977603	931736.263487	41.091674
3532.766293	931193.361933	41.096679
3533.352904	930637.885488	41.101684
3533.080855	930077.985190	41.106688
3532.917381	929526.456113	41.111693
3533.162858	928974.127645	41.116698
3533.284492	928418.881849	41.121703
3533.227333	927842.479317	41.126708
3533.251657	927282.425273	41.131712
3533.012429	926712.751033	41.136717
3533.537202	926154.702347	41.141722
3533.061798	925592.538365	41.146727
3533.166229	925020.799093	41.151732
3533.241948	924461.785234	41.156736
3533.199139	923896.389734	41.161741
3533.334449	923329.270033	41.166746
3533.395703	922768.928439	41.171751
3533.204100	922193.573135	41.176756
3533.160200	921621.977141	41.181760
3532.963295	921052.365954	41.186765
3533.170398	920479.932661	41.191770
3532.932788	919918.960415	41.196775
3533.353168	919337.039555	41.201780
3533.421398	918773.010205	41.206784
3533.028178	918190.142715	41.211789
3532.880081	917620.257234	41.216794
3532.855927	917066.554380	41.221799
3533.180964	916488.962936	41.226804
3532.862793	915918.446512	41.231808
3532.850855	915351.476027	41.236813
3533.048940	914776.997446	41.241818
3532.630248	914212.769852	41.246823
3533.205257	913632.618122	41.251828
3532.962064	913056.878215	41.256832
3533.056628	912482.753712	41.261837
3533.154805	911902.499850	41.266842
3532.922157	911335.342735	41.271847
3533.391068	910748.641668	41.276852
3532.966692	910166.848259	41.281856
3533.133509	909595.878154	41.286861
3533.242993	909004.715912	41.291866
3532.914877	908437.179761	41.296871
3533.091093	907847.713456	41.301876
3533.155291	907260.999189	41.306880
3532.758715	906678.350867	41.311885
3533.266476	906099.247520	41.316890
3533.025374	905529.855265	41.321895
3532.852294	904938.595846	41.326900
3533.115320	904355.108595	41.331904
3532.937011	903774.722448	41.336909
3533.147578	903181.667286	41.341914
3532.697654	902596.380849	41.346919
3532.685163	902020.125683	41.351924
3532.639198	901438.605360	41.356928
3532.504870	900860.996913	41.361933
3532.729355	900277.958592	41.366938
3532.810355	899708.689091	41.371943
3532.722518	899109.750434	41.376948
3533.138040	898527.656300	41.381952
3532.835266	897943.693202	41.386957
3533.152662	897352.803203	41.391962
3533.124784	896768.768020	41.396967
3532.895167	896176.109591	41.401972
3533.112575	895581.863575	41.406976
3532.683947	894992.496382	41.411981
3532.730249	894404.436225	41.416986
3532.626187	893812.088661	41.421991
3532.780434	893216.639095	41.426996
3532.941363	892633.981677	41.432000
3532.806727	892046.384965	41.437005
3533.306693	891442.087232	41.442010
3533.188293	890859.682813	41.447015
3533.394898	890264.786069	41.452020
3533.369221	889655.167299	41.457024
3533.139641	889051.998639	41.462029
3533.023292	888459.290703	41.467034
3532.456205	887841.736393	41.472039
3532.640772	887243.240664	41.477044
3532.822142	886651.553185	41.482048
3532.832476	886062.350142	41.487053
3532.799449	885463.222766	41.492058
3532.452644	884873.668970	41.497063
3532.203955	884278.520704	41.502068
3532.429153	883686.231432	41.507072
3532.382957	883097.897547	41.512077
3532.249962	882491.799032	41.517082
3532.123475	881913.816413	41.522087
3532.351371	881312.859489	41.527092
3532.638686	880723.356621	41.532096
3532.178554	880138.571428	41.537101
3532.263878	879540.846548	41.542106
3532.538567	878956.398788	41.547111
3532.645517	878349.150213	41.552116
3532.869915	877754.804332	41.557120
3532.537410	877152.449079	41.562125
3532.915025	876550.201573	41.567130
3532.505995	875959.368381	41.572135
3532.714431	875349.271761	41.577140
3532.385528	874743.760713	41.582144
3532.050813	874153.606338	41.587149
3532.465980	873549.785134	41.592154
3532.181005	872962.509612	41.597159
3532.313027	872354.929309	41.602164
3532.359497	871762.725409	41.607168
3532.374668	871156.400374	41.612173
3532.328586	870556.136585	41.617178
3532.177935	869966.018858	41.622183
3532.123340	869363.598507	41.627188
3532.177565	868770.124880	41.632192
3532.015298	868171.096506	41.637197
3532.182297	867567.486444	41.642202
3531.831977	866974.486044	41.647207
3531.847181	866379.908138	41.652212
3531.961310	865780.787642	41.657216
3531.743573	865188.559100	41.662221
3532.217174	864594.406002	41.667226
3531.761799	863997.244624	41.672231
3531.850624	863396.531200	41.677236
3531.966076	862800.319588	41.682240
3531.574783	862215.406383	41.687245
3532.079478	861605.893776	41.692250
3531.838032	861022.102921	41.697255
3531.799396	860426.947217	41.702260
3531.691356	859828.926241	41.707264
3531.592979	859228.706188	41.712269
3531.734116	858625.663938	41.717274
3531.698182	858035.912523	41.722279
3531.742882	857426.448326	41.727284
3531.964859	856832.841652	41.732288
3531.581023	856240.253362	41.737293
3531.703629	855634.195797	41.742298
3531.561625	855043.784915	41.747303
3531.881530	854450.417134	41.752308
3531.982425	853846.813542	41.757312
3531.850539	853241.730931	41.762317
3531.792214	852628.304669	41.767322
3531.485972	852040.261132	41.772327
3531.578501	851430.680370	41.777332
3531.403386	850835.783896	41.782336
3531.673865	850238.417769	41.787341
3531.453913	849632.899501	41.792346
3531.420481	849045.595948	41.797351
3531.429432	848450.049792	41.802356
3531.523221	847849.367942	41.807360
3531.011273	847248.634191	41.812365
3531.571320	846656.718491	41.817370
3531.603559	846063.862650	41.822375
3531.650556	845464.030841	41.827380
3531.806444	844859.933262	41.832384
3531.146306	844259.522239	41.837389
3530.867114	843657.039657	41.842394
3530.649872	843065.112250	41.847399
3531.040062	842474.585028	41.852404
3531.189023	841881.314166	41.857408
3530.956025	841287.077808	41.862413
3530.884277	840681.253002	41.867418
3530.771967	840102.192140	41.872423
3530.873702	839500.612599	41.877428
3531.071954	838908.273381	41.882432
3530.912876	838320.865485	41.887437
3530.848239	837725.876164	41.892442
3530.593770	837142.911609	41.897447
3530.865728	836541.022846	41.902452
3530.888292	835955.316962	41.907456
3530.858268	835350.440315	41.912461
3530.595374	834752.426377	41.917466
3530.811927	834164.766742	41.922471
3530.507090	833570.407229	41.927476
3530.466095	832976.923812	41.932480
3530.702511	832382.410776	41.937485
3530.695850	831787.640223	41.942490
3530.741270	831194.807598	41.947495
3530.633983	830606.194511	41.952500
3530.613086	830019.905771	41.957504
3530.491504	829421.860451	41.962509
3530.538686	828830.617580	41.967514
3530.350570	828251.230241	41.972519
3530.211723	827654.148217	41.977524
3530.595809	827059.120484	41.982528
3530.491918	826466.027121	41.987533
3530.441587	825868.375263	41.992538
3530.665675	825285.672858	41.997543
3530.723477	824689.800454	42.002548
3530.706251	824083.231612	42.007552
3530.477342	823492.675505	42.012557
3530.850058	822882.800632	42.017562
3530.490087	822297.389990	42.022567
3530.145921	821706.692880	42.027572
3530.228206	821107.117185	42.032576
3529.959471	820516.691637	42.037581
3530.208638	819922.505726	42.042586
3530.118871	819328.324239	42.047591
3530.464285	818740.178463	42.052596
3530.436686	818149.011103	42.057600
3530.006268	817555.804982	42.062605
3530.336786	816969.608476	42.067610
3530.272868	816377.506727	42.072615
3530.389749	815781.161762	42.077620
3530.200049	815183.592234	42.082624
3529.669415	814598.557608	42.087629
3530.196015	813992.487314	42.092634
3530.507508	813409.260791	42.097639
3530.381726	812817.294466	42.102644
3530.393478	812213.648066	42.107648
3530.048047	811614.758271	42.112653
3530.475938	811011.618419	42.117658
3530.039495	810417.094039	42.122663
3529.941936	809826.230900	42.127668
3529.912638	809228.495444	42.132672
3529.911855	808643.194588	42.137677
3529.839182	808045.068015	42.142682
3529.684699	807462.239009	42.147687
3529.626034	806875.619407	42.152692
3529.641399	806292.366964	42.157696
3529.812407	805699.774923	42.162701
3529.832197	805089.854832	42.167706
3529.647008	804510.356219	42.172711
3529.509937	803925.701770	42.177716
3529.678026	803333.934270	42.182720
3529.888694	802752.601181	42.187725
3529.877197	802157.036261	42.192730
3529.706641	801563.555549	42.197735
3529.735126	800969.597246	42.202740
3529.422792	800386.387539	42.207744
3529.384645	799807.643568	42.212749
3529.678835	799206.129950	42.217754
3529.400422	798622.912529	42.222759
3529.530338	798020.587875	42.227764
3529.511994	797443.261706	42.232768
3529.336469	796862.233774	42.237773
3529.402934	796263.104310	42.242778
3529.159634	795682.332814	42.247783
3529.302446	795097.127359	42.252788
3529.553833	794508.761549	42.257792
3529.541615	793930.995540	42.262797
3529.317655	793328.128551	42.267802
3529.333157	792739.457651	42.272807
3529.082347	792152.403278	42.277812
3529.234139	791564.396156	42.282816
3529.121780	790977.023404	42.287821
3529.030777	790385.766652	42.292826
3529.139181	789803.612274	42.297831
3529.134457	789214.502194	42.302836
3529.400049	788629.816909	42.307840
3528.793539	788058.744402	42.312845
3529.205761	787461.997662	42.317850
3528.925753	786877.309910	42.322855
3529.005445	786297.427340	42.327860
3529.123987	785717.589125	42.332864
3528.896754	785119.378465	42.337869
3529.097970	784546.165079	42.342874
3528.625713	783958.566486	42.347879
3528.732893	783366.493861	42.352884
3528.866668	782781.251749	42.357888
3528.468083	782205.740334	42.362893
3529.082364	781617.665691	42.367898
3528.951154	781055.934287	42.372903
3529.000484	780463.484295	42.377908
3528.838615	779872.940080	42.382912
3528.887841	779285.558366	42.387917
3529.008584	778701.413026	42.392922
3528.923865	778117.353960	42.397927
3528.745608	777529.720770	42.402932
3528.954468	776946.895003	42.407936
3528.938026	776365.094416	42.412941
3528.791676	775775.591166	42.417946
3528.819092	775182.318711	42.422951
3528.570682	774602.484148	42.427956
3528.349854	774018.167948	42.432960
3528.582371	773435.500079	42.437965
3528.639357	772853.061955	42.442970
3528.094350	772275.604595	42.447975
3528.132182	771689.137772	42.452980
3528.328199	771110.723518	42.457984
3527.867089	770542.620945	42.462989
3528.595025	769960.676149	42.467994
3528.703427	769394.259619	42.472999
3528.235716	768819.473440	42.478004
3528.663147	768233.059053	42.483008
3528.066015	767653.770032	42.488013
3528.424670	767074.371097	42.493018
3527.896740	766492.663470	42.498023
3528.112803	765918.570396	42.503028
3528.555101	765337.444596	42.508032
3528.573505	764762.753957	42.513037
3528.046864	764178.449862	42.518042
3528.185795	763595.564048	42.523047
3528.225935	763020.341209	42.528052
3528.347854	762436.727084	42.533056
3527.875417	761858.987861	42.538061
3528.061525	761272.362785	42.543066
3527.924288	760710.653721	42.548071
3527.819383	760132.028546	42.553076
3528.060012	759562.277556	42.558080
3528.016119	758990.361565	42.563085
3527.842995	758421.187109	42.568090
3527.780206	757843.218075	42.573095
3527.862689	757260.788684	42.578100
3528.098043	756680.706455	42.583104
3527.439119	756118.202465	42.588109
3527.709906	755539.408907	42.593114
3527.728288	754966.734776	42.598119
3527.335362	754399.122686	42.603124
3527.555615	753826.871546	42.608128
3527.529600	753259.951414	42.613133
3527.794438	752695.408259	42.618138
3527.859725	752123.006896	42.623143
3527.618961	751549.331250	42.628148
3527.454738	750974.217004	42.633152
3527.304760	750411.552182	42.638157
3527.445074	749840.005270	42.643162
3527.342512	749268.655082	42.648167
3526.914053	748706.802622	42.653172
3527.097972	748135.616214	42.658176
3527.062622	747577.616213	42.663181
3526.561298	747015.900609	42.668186
3526.713635	746464.755159	42.673191
3526.857104	745902.503156	42.678196
3527.035719	745345.245306	42.683200
3526.869547	744788.154780	42.688205
3526.735619	744225.730438	42.693210
3526.417086	743674.369367	42.698215
3526.478185	743125.672904	42.703220
3526.810557	742557.957591	42.708224
3526.436633	742014.942921	42.713229
3526.330289	741462.104721	42.718234
3526.649485	740915.335900	42.723239
3526.712046	740361.155436	42.728244
3526.729218	739807.685617	42.733248
3526.811584	739257.528997	42.738253
3526.832424	738689.340951	42.743258
3526.722206	738130.928458	42.748263
3526.285210	737579.111649	42.753268
3526.616786	737019.803572	42.758272
3526.594345	736467.789381	42.763277
3526.821028	735910.350784	42.768282
3526.668069	735358.133600	42.773287
3526.585521	734802.303301	42.778292
3526.522092	734252.518167	42.783296
3526.369459	733704.393232	42.788301
3526.656595	733142.396115	42.793306
3526.828314	732592.655014	42.798311
3526.175789	732033.017650	42.803316
3526.834164	731483.761229	42.808321
3526.500103	730930.775145	42.813325
3526.436226	730365.970663	42.818330
3526.506513	729811.551605	42.823335
3526.004508	729255.855257	42.828340
3526.225483	728706.088620	42.833345
3525.866999	728161.980069	42.838349
3526.002493	727614.779006	42.843354
3526.214425	727065.299142	42.848359
3525.769137	726520.204024	42.853364
3526.005867	725963.908848	42.858369
3525.575957	725428.893718	42.863373
3525.642236	724886.772957	42.868378
3525.792175	724353.025326	42.873383
3525.885141	723821.185214	42.878388
3526.343456	723262.240663	42.883393
3525.905598	722729.132055	42.888397
3526.021871	722178.993735	42.893402
3526.355900	721627.096317	42.898407
3525.748278	721085.533870	42.903412
3526.007918	720534.121388	42.908417
3525.941828	719995.270262	42.913421
3526.075292	719434.138975	42.918426
3525.565978	718899.704801	42.923431
3525.516232	718356.381294	42.928436
3525.890924	717815.181310	42.933441
3525.378700	717282.875232	42.938445
3525.683415	716731.549858	42.943450
3525.747394	716192.926204	42.948455
3525.568206	715653.019764	42.953460
3525.403866	715110.248558	42.958465
3525.336125	714569.658059	42.963469
3525.157642	714022.800756	42.968474
3525.403593	713497.367736	42.973479
3525.105399	712966.338536	42.978484
3525.483117	712421.862381	42.983489
3525.054678	711901.357412	42.988493
3525.073353	711359.404859	42.993498
3525.126541	710824.707222	42.998503
3525.161415	710297.473469	43.003508
3525.098798	709765.160799	43.008513
3524.966916	709238.336489	43.013517
3525.395841	708704.285075	43.018522
3524.906318	708173.286036	43.023527
3524.794412	707645.317287	43.028532
3525.002186	707112.296249	43.033537
3524.879124	706581.930148	43.038541
3524.819856	706053.059685	43.043546
3524.882563	705522.596329	43.048551
3524.488811	705001.912112	43.053556
3524.721514	704470.709196	43.058561
3524.527615	703953.453718	43.063565
3524.389437	703415.245712	43.068570
3524.481323	702903.392114	43.073575
3524.669549	702384.288439	43.078580
3524.756792	701853.297081	43.083585
3524.590138	701340.898434	43.088589
3524.716850	700820.121707	43.093594
3524.845124	700300.903594	43.098599
3524.578805	699777.895507	43.103604
3524.565978	699247.706210	43.108609
3524.431583	698730.278113	43.113613
3524.537917	698197.519755	43.118618
3524.304051	697682.929374	43.123623
3524.391666	697165.122279	43.128628
3524.342135	696642.784346	43.133633
3523.873510	696124.016579	43.138637
3524.177839	695602.401540	43.143642
3524.172479	695092.641764	43.148647
3524.358943	694581.775599	43.153652
3524.677089	694056.238123	43.158657
3524.458002	693544.784538	43.163661
3524.242801	693009.777842	43.168666
3523.758695	692505.321597	43.173671
3523.830197	691994.922591	43.178676
3523.956517	691473.442657	43.183681
3523.564978	690968.435708	43.188685
3523.966149	690456.797873	43.193690
3524.133644	689948.503751	43.198695
3523.473557	689431.963782	43.203700
3523.958750	688930.423227	43.208705
3523.727972	688429.175861	43.213709
3523.764320	687916.758463	43.218714
3524.010618	687406.515303	43.223719
3523.664609	686906.148095	43.228724
3523.930860	686400.024756	43.233729
3523.806986	685893.840074	43.238733
3523.737239	685379.255785	43.243738
3523.875619	684865.353322	43.248743
3523.808166	684363.652775	43.253748
3523.767531	683846.835895	43.258753
3523.734789	683350.449854	43.263757
3523.341233	682836.423682	43.268762
3523.550768	682331.178006	43.273767
3523.362728	681833.242005	43.278772
3523.539707	681327.597734	43.283777
3523.551820	680830.319806	43.288781
3523.548794	680324.899808	43.293786
3523.492720	679815.128018	43.298791
3523.523746	679313.730395	43.303796
3523.799560	678816.347998	43.308801
3523.479402	678309.227428	43.313805
3523.366684	677797.609968	43.318810
3523.292470	677302.895604	43.323815
3523.348332	676802.801737	43.328820
3523.430868	676292.063929	43.333825
3522.982766	675795.937707	43.338829
3523.221094	675300.066364	43.343834
3523.253129	674802.708817	43.348839
3522.998428	674308.961648	43.353844
3522.991021	673812.155869	43.358849
3523.108791	673318.043388	43.363853
3523.101215	672817.895284	43.368858
3523.181763	672318.353340	43.373863
3522.790768	671829.931289	43.378868
3522.899337	671327.191306	43.383873
3523.161539	670835.714649	43.388877
3522.930180	670348.484359	43.393882
3523.062449	669847.455909	43.398887
3522.951355	669358.259229	43.403892
3523.179544	668850.928899	43.408897
3522.852567	668363.662163	43.413901
3522.528532	667868.341052	43.418906
3522.796173	667380.074381	43.423911
3522.414627	666891.095427	43.428916
3522.316528	666398.900711	43.433921
3522.739069	665920.956580	43.438925
3523.014955	665430.992210	43.443930
3522.973585	664933.973368	43.448935
3523.002408	664448.041238	43.453940
3523.136691	663951.490015	43.458945
3522.846433	663464.215366	43.463949
3522.903280	662967.227186	43.468954
3523.017205	662471.101649	43.473959
3522.790683	661984.090201	43.478964
3522.705720	661484.105466	43.483969
3522.281691	661002.267798	43.488973
3522.623974	660516.382520	43.493978
3522.602306	660030.085756	43.498983
3522.431542	659545.287333	43.503988
3522.743283	659051.048347	43.508993
3522.517901	658574.097058	43.513997
3522.372058	658078.039721	43.519002
3522.378651	657586.873273	43.524007
3522.302198	657111.621970	43.529012
3522.403834	656627.579969	43.534017
3522.303999	656143.598289	43.539021
3521.885244	655658.698391	43.544026
3521.970894	655179.580535	43.549031
3521.488564	654704.980546	43.554036
3521.874783	654227.762316	43.559041
3521.865386	653770.315159	43.564045
3521.707815	653292.694911	43.569050
3521.515632	652811.910823	43.574055
3521.284749	652354.435717	43.579060
3521.729812	651881.938762	43.584065
3521.588786	651422.107427	43.589069
3521.611918	650944.492602	43.594074
3521.593708	650476.853355	43.599079
3521.406395	650018.463540	43.604084
3521.539944	649548.556443	43.609089
3521.282977	649088.087182	43.614093
3521.076341	648611.548655	43.619098
3521.306258	648161.146724	43.624103
3521.358834	647691.915495	43.629108
3521.059306	647230.518302	43.634113
3521.089861	646780.587992	43.639117
3521.178824	646315.434087	43.644122
3521.136456	645864.125722	43.649127
3520.901286	645407.931687	43.654132
3521.250735	644950.767419	43.659137
3521.164558	644498.455596	43.664141
3520.929511	644048.948341	43.669146
3521.375086	643581.557743	43.674151
3520.965576	643127.840000	43.679156
3520.903558	642668.692983	43.684161
3520.987158	642212.650247	43.689165
3520.868709	641759.521593	43.694170
3521.183639	641302.648527	43.699175
3520.807953	640857.224113	43.704180
3520.873174	640389.451558	43.709185
3520.768143	639938.239938	43.714189
3520.273488	639485.324498	43.719194
3520.419840	639039.531654	43.724199
3520.500779	638588.178760	43.729204
3521.196377	638142.653305	43.734209
3520.641146	637695.171199	43.739213
3520.656513	637241.119235	43.744218
3520.608190	636792.961114	43.749223
3520.562409	636349.785829	43.754228
3520.680269	635890.904337	43.759233
3520.526825	635455.813894	43.764237
3520.524570	635014.725333	43.769242
3520.276527	634568.256085	43.774247
3520.038140	634129.071550	43.779252
3520.104458	633685.813217	43.784257
3520.548164	633245.123823	43.789261
3520.222309	632810.252254	43.794266
3520.022929	632368.884961	43.799271
3519.986653	631932.576135	43.804276
3519.798722	631490.218863	43.809281
3519.945818	631066.855836	43.814285
3520.010251	630629.074041	43.819290
3520.439715	630199.821466	43.824295
3520.164093	629761.460898	43.829300
3520.261150	629319.714413	43.834305
3519.996190	628888.424363	43.839309
3519.727045	628457.918441	43.844314
3519.738272	628029.449933	43.849319
3519.959406	627613.295331	43.854324
3519.933169	627168.325595	43.859329
3519.628561	626731.045943	43.864333
3519.585662	626312.632089	43.869338
3519.716225	625884.557310	43.874343
3519.653877	625463.559443	43.879348
3519.745530	625039.163209	43.884353
3519.704667	624609.163394	43.889357
3519.778054	624177.774467	43.894362
3519.886984	623749.116884	43.899367
3519.530378	623322.925921	43.904372
3519.477548	622901.575106	43.909377
3519.417080	622482.312982	43.914381
3519.182840	622061.411036	43.919386
3519.384170	621640.267977	43.924391
3519.388850	621220.093926	43.929396
3519.531640	620791.813663	43.934401
3518.968487	620375.060455	43.939405
3518.903446	619958.807406	43.944410
3519.244798	619550.536188	43.949415
3518.952965	619142.658364	43.954420
3519.164323	618723.003526	43.959425
3519.081920	618312.453028	43.964429
3518.992410	617898.280019	43.969434
3519.247180	617479.572135	43.974439
3519.279839	617066.399125	43.979444
3519.048973	616646.940341	43.984449
3518.874318	616247.304224	43.989453
3519.294533	615827.803140	43.994458
3519.153936	615412.542212	43.999463
3519.029793	615004.731802	44.004468
3519.037872	614598.387580	44.009473
3519.087266	614186.356453	44.014477
3518.894780	613776.456820	44.019482
3518.781398	613357.905202	44.024487
3519.110161	612957.913229	44.029492
3519.067922	612544.081675	44.034497
3518.748840	612135.646986	44.039501
3518.548401	611724.720008	44.044506
3518.862661	611320.208725	44.049511
3518.444419	610918.766417	44.054516
3518.843532	610517.170079	44.059521
3518.573880	610111.360566	44.064525
3518.508730	609704.448192	44.069530
3518.545655	609305.427824	44.074535
3518.440533	608904.461419	44.079540
3518.685110	608498.254774	44.084545
3518.519691	608104.592979	44.089549
3518.520071	607705.672368	44.094554
3518.788540	607299.568762	44.099559
3518.278135	606905.321916	44.104564
3518.606905	606507.607043	44.109569
3518.611722	606116.354933	44.114573
3518.338551	605712.293345	44.119578
3518.624415	605311.884720	44.124583
3518.506115	604915.193577	44.129588
3518.424215	604513.063458	44.134593
3518.410164	604111.810688	44.139597
3518.322564	603714.721112	44.144602
3518.335674	603307.965902	44.149607
3518.001467	602924.439497	44.154612
3518.315271	602530.100464	44.159617
3518.189575	602138.081195	44.164621
3518.131676	601747.341771	44.169626
3518.228657	601348.582562	44.174631
3517.885810	600963.435998	44.179636
3517.925369	600573.844503	44.184641
3517.686253	600183.283501	44.189645
3517.573357	599805.889107	44.194650
3517.986263	599407.259566	44.199655
3517.540426	599034.916490	44.204660
3517.819189	598645.921728	44.209665
3517.864296	598266.893806	44.214669
3517.606520	597886.951311	44.219674
3517.754195	597490.861373	44.224679
3517.650219	597119.251781	44.229684
3517.843947	596726.642407	44.234689
3517.815778	596344.501451	44.239693
3517.335985	595969.002847	44.244698
3517.607771	595577.496278	44.249703
3517.515371	595200.450589	44.254708
3517.692741	594824.451450	44.259713
3517.598618	594450.344672	44.264717
3517.317852	594072.541512	44.269722
3517.450246	593683.255269	44.274727
3517.150562	593314.822435	44.279732
3517.037562	592942.830421	44.284737
3517.188387	592574.347699	44.289741
3516.822145	592209.307026	44.294746
3517.332220	591833.506953	44.299751
3517.160215	591471.775703	44.304756
3517.026979	591098.071335	44.309761
3517.319160	590735.183421	44.314765
3517.103113	590362.022549	44.319770
3517.513774	590000.799965	44.324775
3517.267588	589628.173787	44.329780
3517.296339	589249.409864	44.334785
3517.264220	588884.712134	44.339789
3517.186909	588519.156820	44.344794
3517.661696	588151.034026	44.349799
3517.489279	587779.794592	44.354804
3517.028981	587402.914708	44.359809
3516.855075	587036.878332	44.364813
3516.999211	586663.490001	44.369818
3517.219811	586298.519536	44.374823
3517.002758	585936.376722	44.379828
3517.056235	585562.668154	44.384833
3516.485010	585196.894864	44.389837
3516.260580	584840.701045	44.394842
3516.492625	584477.030458	44.399847
3516.184642	584126.760625	44.404852
3516.348965	583781.325853	44.409857
3516.396987	583426.350730	44.414861
3516.611449	583073.297202	44.419866
3516.672853	582720.611425	44.424871
3516.294835	582373.771432	44.429876
3516.088960	582011.710352	44.434881
3516.347062	581674.293310	44.439885
3516.251776	581320.286665	44.444890
3516.335884	580972.774914	44.449895
3516.068660	580632.050343	44.454900
3516.167322	580274.913454	44.459905
3515.982885	579930.736334	44.464909
3516.380750	579585.293682	44.469914
3516.260467	579231.884613	44.474919
3516.056510	578893.413955	44.479924
3516.535938	578544.408293	44.484929
3516.154520	578198.808359	44.489933
3516.154618	577852.027273	44.494938
3516.025404	577499.072937	44.499943
3515.927901	577166.420602	44.504948
3516.069373	576815.713942	44.509953
3515.996572	576479.317324	44.514957
3516.002948	576137.415926	44.519962
3516.068176	575794.640036	44.524967
3515.571682	575460.551514	44.529972
3516.123799	575113.901428	44.534977
3515.750439	574769.512341	44.539981
3515.545524	574438.062862	44.544986
3515.476837	574100.997683	44.549991
3515.557614	573778.486204	44.554996
3515.788864	573438.585238	44.560001
3515.551396	573109.369897	44.565005
3515.875892	572776.981158	44.570010
3515.816916	572444.498175	44.575015
3515.558379	572104.041006	44.580020
3515.489437	571766.057888	44.585025
3515.432007	571448.893662	44.590029
3515.742068	571120.388152	44.595034
3515.759005	570778.841886	44.600039
3515.484758	570452.381127	44.605044
3515.316685	570127.252438	44.610049
3515.468316	569795.166942	44.615053
3515.279948	569467.106220	44.620058
3515.645617	569137.734684	44.625063
3515.251406	568797.815618	44.630068
3515.027955	568477.133025	44.635073
3515.308727	568148.203328	44.640077
3515.305439	567833.053235	44.645082
3515.519473	567504.520985	44.650087
3515.236520	567178.833340	44.655092
3515.762205	566856.522584	44.660097
3515.373860	566536.171783	44.665101
3515.067418	566200.295981	44.670106
3515.473654	565870.934045	44.675111
3514.775864	565552.473971	44.680116
3514.501862	565234.487381	44.685121
3514.981415	564916.011911	44.690125
3514.500017	564619.590870	44.695130
3514.884162	564291.652245	44.700135
3514.553959	563979.030920	44.705140
3514.854177	563661.511692	44.710145
3514.868728	563353.347402	44.715149
3514.536551	563038.488521	44.720154
3514.909441	562722.041531	44.725159
3514.428303	562415.097619	44.730164
3514.810760	562109.660584	44.735169
3514.624927	561805.572210	44.740173
3514.630413	561491.524584	44.745178
3514.626835	561182.053168	44.750183
3514.745060	560883.581411	44.755188
3514.885399	560568.934693	44.760193
3514.779960	560254.221668	44.765197
3514.082003	559951.738713	44.770202
3514.394722	559632.608533	44.775207
3514.309302	559347.733773	44.780212
3514.352712	559040.973667	44.785217
3514.111025	558739.442521	44.790221
3514.310413	558440.297031	44.795226
3514.339051	558124.200683	44.800231
3514.240619	557840.403621	44.805236
3514.119614	557532.276619	44.810241
3514.559950	557235.278918	44.815245
3514.108157	556937.520219	44.820250
3514.144887	556623.552583	44.825255
3514.113823	556338.402202	44.830260
3514.269851	556032.359083	44.835265
3514.181555	555738.440595	44.840269
3513.937329	555440.764054	44.845274
3514.253131	555148.677852	44.850279
3513.999071	554865.901748	44.855284
3514.054503	554545.181661	44.860289
3514.189062	554268.724742	44.865293
3513.731636	553976.896109	44.870298
3514.229303	553678.046029	44.875303
3513.711330	553390.648638	44.880308
3513.538077	553104.143549	44.885313
3513.602689	552813.006638	44.890317
3513.562578	552532.412161	44.895322
3513.734205	552241.647725	44.900327
3513.482643	551963.596909	44.905332
3513.516782	551678.084256	44.910337
3513.493761	551407.239127	44.915341
3513.295307	551115.757782	44.920346
3513.229501	550837.803276	44.925351
3513.177027	550562.209321	44.930356
3513.300367	550286.075799	44.935361
3513.536001	550005.583417	44.940365
3513.425616	549725.849891	44.945370
3513.449787	549445.634058	44.950375
3513.433440	549173.180875	44.955380
3513.573000	548885.877930	44.960385
3513.280141	548612.855966	44.965389
3513.365298	548341.276076	44.970394
3513.264097	548053.190295	44.975399
3513.277083	547786.652065	44.980404
3513.104681	547510.311249	44.985409
3513.037065	547233.140472	44.990413
3512.949736	546963.276548	44.995418
3513.014110	546693.431833	45.000423
3512.748845	546432.560573	45.005428
3512.948855	546161.573269	45.010433
3512.848999	545896.630791	45.015437
3512.584763	545631.912941	45.020442
3513.121165	545352.836765	45.025447
3513.064522	545097.954253	45.030452
3513.066730	544825.512503	45.035457
3513.255382	544558.982678	45.040461
3512.787245	544298.458680	45.045466
3513.181390	544022.707541	45.050471
3512.794469	543759.134467	45.055476
3512.703033	543492.228639	45.060481
3513.199422	543219.166801	45.065485
3512.844752	542957.085664	45.070490
3512.815294	542696.658456	45.075495
3513.040268	542438.855417	45.080500
3513.256477	542171.770948	45.085505
3513.351530	541912.013810	45.090509
3512.844008	541635.966039	45.095514
3513.191532	541371.012231	45.100519
3512.684130	541108.519110	45.105524
3512.772080	540834.673619	45.110529
3512.642928	540578.813162	45.115533
3512.631994	540319.095073	45.120538
3512.963499	540052.253183	45.125543
3512.280462	539801.163387	45.130548
3512.586278	539540.872547	45.135553
3512.491607	539276.257425	45.140557
3513.125344	539024.626386	45.145562
3512.945867	538754.770631	45.150567
3512.651703	538505.659345	45.155572
3512.293881	538251.964611	45.160577
3512.251990	537987.165080	45.165581
3512.093686	537741.800173	45.170586
3512.364849	537488.236609	45.175591
3512.017125	537249.654728	45.180596
3512.380671	536984.615985	45.185601
3512.071035	536739.007420	45.190605
3511.957139	536495.025894	45.195610
3511.931860	536245.930027	45.200615
3512.350873	536014.561697	45.205620
3512.301583	535761.627539	45.210625
3511.855556	535509.816075	45.215629
3512.067269	535268.179572	45.220634
3511.786287	535034.745619	45.225639
3511.895471	534793.471786	45.230644
3511.892071	534556.350187	45.235649
3512.197751	534303.127920	45.240653
3511.807669	534063.339770	45.245658
3511.947435	533817.907168	45.250663
3511.475654	533590.082813	45.255668
3511.893769	533347.319273	45.260673
3512.243815	533106.329277	45.265677
3512.029400	532872.748030	45.270682
3512.431334	532630.631185	45.275687
3512.197296	532382.967418	45.280692
3512.183326	532132.436066	45.285697
3512.179338	531889.013725	45.290701
3512.030751	531653.130845	45.295706
3512.083478	531403.231544	45.300711
3511.715306	531166.873645	45.305716
3511.982037	530923.944043	45.310721
3512.059857	530674.280283	45.315725
3512.036895	530445.875765	45.320730
3512.324109	530208.532519	45.325735
3511.975001	529968.467868	45.330740
3511.772856	529728.727468	45.335745
3511.911139	529485.543561	45.340749
3511.737241	529244.528682	45.345754
3511.791347	529006.600130	45.350759
3511.499933	528780.486695	45.355764
3511.516324	528542.809437	45.360769
3511.723981	528307.316524	45.365773
3511.770878	528090.775184	45.370778
3511.556280	527839.497946	45.375783
3512.096506	527604.946542	45.380788
3511.993482	527372.621272	45.385793
3511.824905	527131.722353	45.390797
3511.398869	526900.656284	45.395802
3511.470591	526658.598114	45.400807
3511.509810	526437.995546	45.405812
3511.422275	526205.094041	45.410817
3511.410377	525972.680786	45.415821
3511.130315	525748.992644	45.420826
3511.438582	525523.231847	45.425831
3511.697744	525297.980853	45.430836
3511.365934	525070.303129	45.435841
3511.703890	524838.468742	45.440845
3511.069902	524619.721165	45.445850
3511.725285	524386.260495	45.450855
3511.519224	524159.001794	45.455860
3510.771706	523927.540571	45.460865
3511.260217	523707.578231	45.465869
3510.922036	523500.022871	45.470874
3511.078897	523277.081454	45.475879
3511.030690	523065.027393	45.480884
3510.924548	522839.397857	45.485889
3510.965259	522621.768230	45.490893
3511.212862	522415.663162	45.495898
3511.245998	522181.719050	45.500903
3510.777586	521972.044087	45.505908
3510.670099	521750.741059	45.510913
3510.963734	521529.164316	45.515917
3511.056627	521321.404347	45.520922
3511.064105	521109.010305	45.525927
3510.835899	520889.482721	45.530932
3510.991690	520672.411363	45.535937
3510.774807	520460.905041	45.540941
3510.920046	520249.687450	45.545946
3511.070141	520035.688515	45.550951
3510.819320	519822.310549	45.555956
3510.816868	519603.382368	45.560961
3510.865298	519391.714878	45.565965
3510.631360	519187.415788	45.570970
3510.504286	518963.752303	45.575975
3510.347389	518762.717204	45.580980
3510.361218	518568.165631	45.585985
3510.600922	518349.178128	45.590989
3510.511686	518157.770376	45.595994
3510.416848	517939.541249	45.600999
3510.365007	517746.404693	45.606004
3510.383223	517547.495641	45.611009
3510.307483	517347.084746	45.616013
3510.522136	517144.146618	45.621018
3510.551327	516934.165843	45.626023
3510.133700	516726.683092	45.631028
3510.223748	516531.082460	45.636033
3510.266836	516340.589246	45.641037
3510.483849	516145.517701	45.646042
3510.365068	515936.104267	45.651047
3510.317080	515730.919225	45.656052
3510.170738	515542.014502	45.661057
3510.378095	515347.187125	45.666061
3509.838526	515160.668670	45.671066
3510.188117	514967.428798	45.676071
3510.116115	514768.549885	45.681076
3510.117077	514569.302332	45.686081
3510.173005	514370.143883	45.691085
3509.961947	514187.750821	45.696090
3510.015569	513983.586274	45.701095
3510.074423	513801.900430	45.706100
3510.044139	513606.839220	45.711105
3509.974820	513414.358920	45.716109
3510.255013	513228.182570	45.721114
3510.159652	513023.828817	45.726119
3509.754111	512836.299678	45.731124
3509.681859	512655.784974	45.736129
3510.133271	512459.970385	45.741133
3509.637604	512274.622540	45.746138
3509.652323	512089.842218	45.751143
3509.750360	511894.889357	45.756148
3509.679681	511701.529276	45.761153
3509.618668	511518.372086	45.766157
3509.540068	511349.111475	45.771162
3509.532314	511160.130095	45.776167
3509.461482	510981.061300	45.781172
3509.636250	510804.222459	45.786177
3509.874050	510617.213914	45.791181
3509.703027	510436.286358	45.796186
3509.504827	510251.419773	45.801191
3509.681482	510072.702696	45.806196
3509.936193	509894.071344	45.811201
3509.774754	509702.875269	45.816205
3509.608606	509526.333037	45.821210
3509.407692	509330.540470	45.826215
3509.643054	509156.705069	45.831220
3509.789938	508987.784999	45.836225
3510.113866	508798.112357	45.841229
3509.797788	508616.936132	45.846234
3509.742749	508421.461240	45.851239
3509.849302	508241.067747	45.856244
3509.540760	508067.111166	45.861249
3509.608043	507885.406311	45.866253
3509.449363	507714.553835	45.871258
3509.086981	507538.477951	45.876263
3509.258223	507371.558293	45.881268
3509.583438	507192.682453	45.886273
3509.826902	507007.551168	45.891277
3509.558177	506834.079819	45.896282
3509.297522	506660.150314	45.901287
3509.715334	506493.331053	45.906292
3509.108891	506316.626336	45.911297
3509.359192	506139.116290	45.916301
3509.155356	505973.257067	45.921306
3509.414712	505794.124173	45.926311
3509.363663	505624.646406	45.931316
3509.236840	505453.916084	45.936321
3509.523160	505284.276042	45.941325
3509.010918	505117.854092	45.946330
3509.448211	504945.707792	45.951335
3509.082034	504775.061715	45.956340
3509.088821	504602.631418	45.961345
3509.704281	504427.315016	45.966349
3509.446263	504260.183667	45.971354
3509.529499	504087.330419	45.976359
3509.477501	503912.425737	45.981364
3509.542612	503749.379328	45.986369
3509.607813	503564.946774	45.991373
3509.401992	503388.040538	45.996378
3509.493012	503212.547806	46.001383
3509.536528	503045.605263	46.006388
3509.440619	502869.230744	46.011393
3509.616881	502699.279154	46.016397
3509.226774	502527.299081	46.021402
3509.702824	502346.119395	46.026407
3509.700964	502168.811210	46.031412
3509.607141	502000.718589	46.036417
3509.551002	501823.264251	46.041421
3509.023884	501661.410423	46.046426
3508.963240	501486.531783	46.051431
3509.001661	501322.403931	46.056436
3509.309678	501160.099197	46.061441
3509.358506	500987.724646	46.066445
3509.087339	500824.504244	46.071450
3509.022314	500646.128574	46.076455
3509.458130	500490.924859	46.081460
3508.889522	500324.918714	46.086465
3509.242114	500148.691188	46.091469
3508.727120	499989.397646	46.096474
3508.863840	499829.991290	46.101479
3509.021109	499666.585142	46.106484
3508.793525	499494.545582	46.111489
3508.588972	499344.497132	46.116493
3508.615041	499199.414161	46.121498
3509.263588	499040.317353	46.126503
3509.087344	498879.741648	46.131508
3509.032130	498714.946471	46.136513
3508.841830	498549.515316	46.141517
3508.541400	498400.233242	46.146522
3508.373431	498238.891374	46.151527
3508.542000	498088.767864	46.156532
3508.683674	497935.259292	46.161537
3508.585358	497774.963041	46.166541
3508.537907	497627.502013	46.171546
3508.728508	497463.613357	46.176551
3508.554830	497312.883850	46.181556
3508.553487	497158.987968	46.186561
3509.012683	496997.122411	46.191565
3508.419847	496856.069510	46.196570
3508.824142	496700.886356	46.201575
3508.427810	496552.413332	46.206580
3508.146292	496401.289419	46.211585
3508.668029	496242.086437	46.216589
3508.226640	496100.748433	46.221594
3508.532566	495946.182023	46.226599
3508.663703	495795.235084	46.231604
3508.119721	495652.090010	46.236609
3508.537314	495511.409641	46.241613
3508.383413	495362.429492	46.246618
3508.174822	495221.448984	46.251623
3508.116862	495069.971453	46.256628
3507.988116	494924.726083	46.261633
3508.238745	494777.442021	46.266637
3508.012862	494645.007869	46.271642
3508.194817	494503.044208	46.276647
3508.265060	494356.090767	46.281652
3507.915698	494214.265985	46.286657
3508.528630	494067.267959	46.291661
3508.464409	493931.816207	46.296666
3508.612116	493778.319226	46.301671
3508.429035	493636.612970	46.306676
3507.940362	493489.443940	46.311681
3508.226368	493347.402251	46.316685
3507.602382	493216.947160	46.321690
3507.642038	493065.991484	46.326695
3507.705565	492928.233531	46.331700
3508.013830	492800.195989	46.336705
3508.370633	492654.848272	46.341709
3508.098748	492522.810114	46.346714
3508.528063	492376.132356	46.351719
3507.525547	492237.943787	46.356724
3507.583144	492093.805922	46.361729
3508.043836	491963.661923	46.366733
3507.887027	491830.536382	46.371738
3508.001690	491696.048103	46.376743
3507.525192	491559.534893	46.381748
3507.433347	491428.671718	46.386753
3507.852096	491306.826838	46.391757
3507.746783	491173.485031	46.396762
3508.009963	491034.969447	46.401767
3507.746058	490898.364080	46.406772
3507.632043	490770.687014	46.411777
3507.980614	490631.597074	46.416781
3507.754811	490510.817881	46.421786
3507.739935	490377.758021	46.426791
3508.029350	490242.317823	46.431796
3507.701670	490115.380702	46.436801
3507.571317	489977.480345	46.441805
3507.354199	489848.447968	46.446810
3507.371931	489718.615584	46.451815
3507.718314	489596.568574	46.456820
3507.224972	489480.027353	46.461825
3507.792307	489345.544604	46.466829
3507.174753	489224.975088	46.471834
3507.403323	489093.128700	46.476839
3507.388248	488978.678153	46.481844
3507.071078	488861.647298	46.486849
3507.556993	488736.433283	46.491853
3507.080719	488624.437299	46.496858
3507.277998	488497.499864	46.501863
3507.282532	488378.184430	46.506868
3506.875008	488263.694974	46.511873
3507.343327	488134.735194	46.516877
3507.213983	488029.962654	46.521882
3507.073424	487915.374720	46.526887
3507.076360	487793.576076	46.531892
3507.143771	487683.606471	46.536897
3507.005151	487566.080985	46.541901
3506.539004	487451.494989	46.546906
3506.952172	487337.770163	46.551911
3506.866049	487230.607089	46.556916
3506.731790	487123.147954	46.561921
3507.169701	487007.240791	46.566925
3506.961623	486896.554206	46.571930
3506.836168	486775.428236	46.576935
3507.104499	486669.314505	46.581940
3506.936057	486563.628945	46.586945
3507.068955	486461.990353	46.591949
3507.035149	486348.132992	46.596954
3506.814332	486232.231964	46.601959
3507.049541	486119.744164	46.606964
3506.846122	486015.731292	46.611969
3506.988816	485893.693125	46.616973
3506.605087	485788.596334	46.621978
3506.953869	485675.985085	46.626983
3506.897733	485576.347352	46.631988
3506.463865	485470.396880	46.636993
3506.876792	485348.207570	46.641997
3506.418239	485259.062174	46.647002
3506.946971	485154.615542	46.652007
3507.063125	485053.174102	46.657012
3506.726449	484942.497153	46.662017
3506.714933	484839.001268	46.667021
3506.585845	484728.287531	46.672026
3506.564209	484623.779900	46.677031
3506.737413	484526.779456	46.682036
3506.432459	484424.596527	46.687041
3506.650960	484320.096709	46.692045
3506.244773	484225.167400	46.697050
3506.400795	484121.183197	46.702055
3506.752729	484018.177186	46.707060
3506.335752	483931.751072	46.712065
3506.138701	483831.823877	46.717069
3506.148387	483744.261121	46.722074
3506.219725	483647.627550	46.727079
3506.166316	483556.936590	46.732084
3506.280628	483464.495645	46.737089
3506.639902	483365.078203	46.742093
3506.571769	483274.793233	46.747098
3506.511415	483174.029158	46.752103
3506.574752	483074.154469	46.757108
3506.457671	482979.574051	46.762113
3506.588147	482868.854997	46.767117
3506.697740	482778.334699	46.772122
3506.685853	482674.421314	46.777127
3506.923825	482575.070790	46.782132
3506.612148	482479.154289	46.787137
3506.496097	482377.129789	46.792141
3506.408615	482282.490001	46.797146
3506.285316	482187.197794	46.802151
3506.256520	482094.521087	46.807156
3506.196671	481997.242925	46.812161
3506.350292	481905.394604	46.817165
3506.427587	481814.773698	46.822170
3506.516135	481720.505830	46.827175
3506.467301	481621.249594	46.832180
3506.318702	481531.273257	46.837185
3506.486377	481429.245524	46.842189
3506.263984	481338.622759	46.847194
3506.180742	481239.522145	46.852199
3506.242733	481157.050436	46.857204
3506.159971	481073.894369	46.862209
3506.348468	480978.238764	46.867213
3506.428923	480894.598407	46.872218
3506.173954	480806.914569	46.877223
3506.458387	480712.354849	46.882228
3506.226070	480625.982433	46.887233
3506.651002	480529.727228	46.892237
3506.512568	480431.542788	46.897242
3506.321757	480339.492152	46.902247
3506.527568	480236.236181	46.907252
3505.964228	480161.055198	46.912257
3506.280109	480064.613635	46.917261
3506.353452	479971.807283	46.922266
3506.019488	479889.397373	46.927271
3506.215660	479796.822271	46.932276
3505.920475	479717.442432	46.937281
3506.346381	479619.055960	46.942285
3506.104049	479538.704433	46.947290
3505.875435	479449.338853	46.952295
3506.326756	479365.729332	46.957300
3505.965977	479270.664716	46.962305
3506.164654	479186.388740	46.967309
3506.367693	479110.870021	46.972314
3506.628982	479015.090329	46.977319
3506.310618	478922.446730	46.982324
3506.029413	478831.365759	46.987329
3506.380486	478738.809427	46.992333
3505.946663	478657.980413	46.997338
3506.012848	478578.635132	47.002343
3506.386523	478491.389622	47.007348
3506.011170	478416.118656	47.012353
3506.036380	478320.071837	47.017357
3505.895802	478247.696553	47.022362
3506.261636	478161.868412	47.027367
3505.914769	478078.743659	47.032372
3505.953545	477997.122198	47.037377
3506.020535	477908.711149	47.042381
3505.934203	477832.274559	47.047386
3505.929315	477749.140539	47.052391
3505.965245	477669.543310	47.057396
3505.945459	477581.196120	47.062401
3505.928637	477490.974648	47.067405
3506.017932	477426.303400	47.072410
3505.957364	477334.367161	47.077415
3506.019322	477254.561153	47.082420
3505.644701	477180.145692	47.087425
3506.238496	477095.438147	47.092429
3505.907950	477027.141026	47.097434
3505.947828	476940.907111	47.102439
3505.909301	476861.015277	47.107444
3506.111940	476779.562927	47.112449
3506.020116	476703.274449	47.117453
3505.969751	476616.801251	47.122458
3505.690084	476533.202284	47.127463
3505.969126	476466.419264	47.132468
3505.715821	476382.106233	47.137473
3506.093871	476300.976245	47.142477
3506.026830	476224.732179	47.147482
3505.961558	476146.462105	47.152487
3505.996086	476054.604475	47.157492
3505.815246	475982.429636	47.162497
3505.715470	475892.366360	47.167501
3505.819755	475831.788400	47.172506
3505.745345	475751.999136	47.177511
3506.068945	475676.546906	47.182516
3505.660650	475598.890067	47.187521
3505.798054	475522.456273	47.192525
3505.222075	475447.156703	47.197530
3505.245309	475379.603229	47.202535
3506.142627	475301.165200	47.207540
3505.654017	475234.053048	47.212545
3505.875086	475155.729869	47.217549
3505.736608	475079.847721	47.222554
3505.588271	475000.270377	47.227559
3505.833281	474935.361219	47.232564
3505.406573	474863.375891	47.237569
3505.749992	474784.371949	47.242573
3505.627532	474715.929430	47.247578
3505.693963	474643.403295	47.252583
3505.775483	474570.570464	47.257588
3505.538310	474503.007609	47.262593
3505.961561	474425.305125	47.267597
3505.727716	474363.159617	47.272602
3505.999379	474284.672192	47.277607
3506.167447	474200.024032	47.282612
3505.922303	474129.827890	47.287617
3506.035311	474042.301914	47.292621
3505.740265	473970.239989	47.297626
3505.811344	473894.266558	47.302631
3506.180774	473811.810446	47.307636
3505.760805	473744.326679	47.312641
3505.954452	473663.419164	47.317645
3506.008833	473591.498671	47.322650
3506.032588	473509.100240	47.327655
3506.178321	473430.833278	47.332660
3505.423401	473352.719771	47.337665
3505.575772	473274.856159	47.342669
3505.772946	473214.101844	47.347674
3505.663881	473146.613462	47.352679
3505.820374	473082.118083	47.357684
3505.971899	473015.344379	47.362689
3505.835889	472920.360427	47.367693
3505.762641	472857.118943	47.372698
3505.453315	472779.889179	47.377703
3505.744386	472711.875106	47.382708
3505.294060	472649.203744	47.387713
3505.542884	472564.129200	47.392717
3505.257459	472505.278184	47.397722
3505.251186	472442.226437	47.402727
3505.557225	472378.665346	47.407732
3505.315743	472307.499450	47.412737
3505.370151	472237.498251	47.417741
3505.526664	472179.836887	47.422746
3505.843505	472106.447778	47.427751
3505.561488	472035.895520	47.432756
3505.442565	471972.557549	47.437761
3505.627239	471898.379855	47.442765
3505.139446	471830.039749	47.447770
3505.467924	471777.918905	47.452775
3505.384926	471716.701097	47.457780
3505.416792	471647.511892	47.462785
3505.123810	471576.250716	47.467789
3505.385828	471524.140515	47.472794
3505.109735	471458.345923	47.477799
3505.374292	471381.468225	47.482804
3505.317495	471332.855979	47.487809
3505.175760	471267.797495	47.492813
3505.189395	471214.462646	47.497818
3505.185540	471152.976245	47.502823
3505.065365	471077.479854	47.507828
3505.180277	471024.988200	47.512833
3505.337169	470957.598462	47.517837
3505.432623	470902.881239	47.522842
3505.000037	470838.833266	47.527847
3505.124061	470772.208214	47.532852
3504.700079	470717.680444	47.537857
3504.930033	470661.521367	47.542861
3504.807273	470606.941843	47.547866
3504.730800	470553.164657	47.552871
3505.145877	470492.414968	47.557876
3504.760021	470445.173519	47.562881
3505.013559	470382.374397	47.567885
3505.375342	470335.359569	47.572890
3504.816688	470276.649519	47.577895
3505.157870	470219.659725	47.582900
3504.839278	470174.128241	47.587905
3504.862327	470116.989853	47.592909
3504.880672	470057.826044	47.597914
3504.766796	470006.130390	47.602919
3504.869484	469955.815862	47.607924
3504.485207	469912.067768	47.612929
3505.363903	469850.375777	47.617933
3505.199088	469801.980634	47.622938
3504.986680	469748.224368	47.627943
3505.313431	469678.774979	47.632948
3505.283481	469639.828377	47.637953
3505.013837	469573.418275	47.642957
3504.844257	469515.247257	47.647962
3504.947666	469456.320307	47.652967
3505.246055	469403.691516	47.657972
3504.932056	469345.645943	47.662977
3505.336755	469293.100000	47.667981
3504.992386	469230.399150	47.672986
3504.698351	469180.352917	47.677991
3505.031270	469122.804046	47.682996
3504.866093	469077.902229	47.688001
3504.916049	469017.260810	47.693005
3504.968305	468972.422926	47.698010
3504.883038	468918.895870	47.703015
3504.790617	468865.420540	47.708020
3504.516384	468822.309647	47.713025
3504.702340	468772.990857	47.718029
3504.732015	468733.272394	47.723034
3504.721603	468683.682973	47.728039
3504.979118	468626.297441	47.733044
3504.779634	468581.400309	47.738049
3504.979984	468531.521228	47.743053
3505.048822	468479.536940	47.748058
3504.665717	468431.074264	47.753063
3505.206054	468364.572289	47.758068
3504.776885	468320.524253	47.763073
3504.841462	468267.476340	47.768077
3504.702291	468213.247319	47.773082
3504.624545	468173.495374	47.778087
3504.643492	468121.265347	47.783092
3504.734013	468078.597053	47.788097
3504.531303	468031.723570	47.793101
3504.794230	467984.770464	47.798106
3504.863744	467934.050996	47.803111
3505.042384	467877.183249	47.808116
3504.654767	467831.961875	47.813121
3505.089960	467782.243368	47.818125
3504.893414	467730.606298	47.823130
3504.884848	467684.104072	47.828135
3504.960596	467627.861044	47.833140
3504.464116	467596.233981	47.838145
3504.789157	467537.871150	47.843149
3504.723730	467501.357816	47.848154
3504.771664	467447.702572	47.853159
3504.926109	467403.958035	47.858164
3504.433010	467366.554959	47.863169
3504.696707	467314.838182	47.868173
3504.552618	467275.906236	47.873178
3504.754360	467230.126878	47.878183
3504.522114	467178.646391	47.883188
3504.715487	467133.780094	47.888193
3504.951732	467085.410886	47.893197
3504.637789	467041.340224	47.898202
3504.744673	467002.972783	47.903207
3504.798185	466949.365851	47.908212
3504.270930	466904.875362	47.913217
3504.673620	466856.021219	47.918221
3504.755643	466827.536335	47.923226
3504.821801	466788.111561	47.928231
3504.595729	466729.891033	47.933236
3504.572168	466681.919792	47.938241
3504.516733	466635.169722	47.943245
3504.531490	466591.903131	47.948250
3504.235523	466554.920754	47.953255
3504.705833	466516.388966	47.958260
3504.532689	466476.041858	47.963265
3504.583515	466439.253349	47.968269
3504.527347	466396.555698	47.973274
3503.989839	466351.913694	47.978279
3504.455686	466312.622344	47.983284
3504.287388	466269.183637	47.988289
3504.497641	466220.968678	47.993293
3504.352945	466201.589985	47.998298
3504.296417	466154.534965	48.003303
3504.483863	466117.013250	48.008308
3504.128541	466083.991720	48.013313
3504.413673	466034.446300	48.018317
3504.341143	466008.367707	48.023322
3504.130308	465981.654087	48.028327
3503.963978	465936.542444	48.033332
3503.994463	465905.075923	48.038337
3504.029765	465872.848592	48.043341
3504.099634	465848.721303	48.048346
3504.169793	465809.445830	48.053351
3504.646505	465768.074350	48.058356
3504.333795	465747.963950	48.063361
3504.211427	465703.908174	48.068365
3504.414672	465670.233269	48.073370
3504.326400	465645.778088	48.078375
3504.399058	465601.080821	48.083380
3504.067936	465561.468056	48.088385
3504.257260	465537.117329	48.093389
3504.468418	465494.068054	48.098394
3504.131078	465456.685326	48.103399
3504.286188	465423.372855	48.108404
3504.208535	465386.097639	48.113409
3504.192934	465343.390730	48.118413
3504.325743	465315.756227	48.123418
3504.037943	465286.014952	48.128423
3504.437189	465252.508510	48.133428
3504.230437	465226.147795	48.138433
3504.425159	465187.407094	48.143437
3504.069970	465144.707066	48.148442
3504.081885	465112.938441	48.153447
3504.446220	465083.946800	48.158452
3504.154629	465042.299641	48.163457
3504.237160	465005.198999	48.168461
3504.365585	464981.263289	48.173466
3504.097719	464951.720755	48.178471
3504.416797	464905.003877	48.183476
3504.053659	464882.519932	48.188481
3504.279788	464849.802329	48.193485
3504.119209	464806.764336	48.198490
3504.287721	464785.506795	48.203495
3504.515300	464751.572813	48.208500
3504.104207	464709.894679	48.213505
3504.152795	464672.900528	48.218509
3503.924506	464658.905109	48.223514
3504.182947	464620.051064	48.228519
3504.260415	464583.102477	48.233524
3504.096784	464556.784153	48.238529
3504.160697	464522.067062	48.243533
3504.289315	464486.072209	48.248538
3503.740466	464460.579521	48.253543
3504.102323	464425.862050	48.258548
3503.975949	464403.894450	48.263553
3504.084298	464381.937413	48.268557
3504.367169	464346.929291	48.273562
3504.162187	464318.540382	48.278567
3504.448890	464283.936824	48.283572
3504.105718	464248.528755	48.288577
3504.078790	464214.485292	48.293581
3504.256695	464196.974843	48.298586
3504.125651	464162.797067	48.303591
3504.261683	464117.528224	48.308596
3503.859356	464095.911396	48.313601
3504.087666	464078.848239	48.318605
3504.304547	464036.605429	48.323610
3503.941683	463999.325581	48.328615
3504.219459	463971.056404	48.333620
3504.277262	463963.902397	48.338625
3504.461930	463931.240996	48.343629
3504.359904	463892.649719	48.348634
3504.374536	463865.590675	48.353639
3504.612322	463814.882315	48.358644
3504.398558	463787.051476	48.363649
3504.393867	463753.966100	48.368653
3504.441019	463715.551672	48.373658
3504.070453	463695.499685	48.378663
3504.568942	463657.413422	48.383668
3504.275401	463621.337050	48.388673
3504.496440	463587.503492	48.393677
3504.251105	463550.304053	48.398682
3504.440904	463523.923985	48.403687
3504.354154	463490.953511	48.408692
3504.089118	463450.261109	48.413697
3504.019333	463420.023731	48.418701
3504.011999	463394.538517	48.423706
3503.855451	463376.121731	48.428711
3504.176266	463333.960992	48.433716
3503.848365	463305.490257	48.438721
3503.942227	463286.523938	48.443725
3504.069136	463263.903774	48.448730
3503.896233	463243.462886	48.453735
3504.067126	463194.081738	48.458740
3503.857488	463181.247466	48.463745
3504.076869	463153.848459	48.468749
3503.861059	463140.559188	48.473754
3503.696201	463121.332868	48.478759
3503.930163	463092.107179	48.483764
3503.643226	463063.679766	48.488769
3503.979335	463033.321813	48.493773
3503.904078	463012.357313	48.498778
3503.878862	462998.275354	48.503783
3504.024778	462971.699354	48.508788
3503.900928	462949.831024	48.513793
3504.028600	462910.691884	48.518797
3504.145935	462884.272657	48.523802
3503.577309	462871.752829	48.528807
3503.679736	462849.288377	48.533812
3503.465543	462838.126777	48.538817
3503.717560	462816.194119	48.543821
3503.529634	462803.153209	48.548826
3503.861383	462788.554115	48.553831
3503.804877	462748.331349	48.558836
3503.816375	462727.655753	48.563841
3503.575910	462699.422558	48.568845
3503.731146	462684.549501	48.573850
3503.423959	462669.806062	48.578855
3503.548124	462644.804126	48.583860
3503.483253	462631.640749	48.588865
3503.839563	462614.149092	48.593869
3503.905948	462600.203219	48.598874
3503.668264	462590.312262	48.603879
3503.840670	462556.941267	48.608884
3503.601688	462520.904217	48.613889
3503.546192	462498.111631	48.618893
3503.318330	462489.029684	48.623898
3503.646731	462470.022528	48.628903
3504.157296	462446.322487	48.633908
3503.902651	462446.112575	48.638913
3503.589287	462418.499478	48.643917
3503.945788	462406.277429	48.648922
3503.570149	462395.548514	48.653927
3503.975173	462364.721718	48.658932
3504.057639	462331.315025	48.663937
3503.930573	462312.030785	48.668941
3504.208951	462292.981328	48.673946
3503.743803	462278.619267	48.678951
3503.858551	462238.467558	48.683956
3503.708762	462216.349479	48.688961
3503.787621	462197.232653	48.693965
3504.110428	462174.932488	48.698970
3503.675935	462164.466856	48.703975
3503.719742	462144.849243	48.708980
3503.898754	462131.542543	48.713985
3504.064265	462099.793458	48.718989
3503.929885	462072.960068	48.723994
3503.741472	462054.446135	48.728999
3504.556875	462022.585957	48.734004
3504.101661	462009.843520	48.739009
3503.923691	461974.200429	48.744013
3504.281930	461952.806069	48.749018
3504.238261	461941.513496	48.754023
3504.110520	461907.888613	48.759028
3503.627923	461888.259281	48.764033
3503.659193	461866.717966	48.769037
3504.006968	461846.794790	48.774042
3503.734142	461834.578498	48.779047
3504.072761	461806.954561	48.784052
3503.638835	461782.553552	48.789057
3503.890730	461748.711556	48.794061
3503.929068	461734.111107	48.799066
3503.735002	461711.087902	48.804071
3504.073503	461697.044252	48.809076
3503.719645	461682.409385	48.814081
3503.855730	461656.998772	48.819085
3503.994543	461627.128398	48.824090
3503.833471	461604.454149	48.829095
3504.108554	461583.529649	48.834100
3504.066090	461576.949301	48.839105
3503.753123	461556.581243	48.844109
3504.062416	461511.935555	48.849114
3503.915782	461496.150343	48.854119
3504.460389	461475.787794	48.859124
3503.999915	461466.441048	48.864129
3503.651569	461421.552729	48.869133
3503.723777	461391.592023	48.874138
3503.458607	461388.698170	48.879143
3503.704156	461362.508376	48.884148
3503.452240	461351.301696	48.889153
3503.249540	461339.073123	48.894157
3503.648853	461321.471629	48.899162
3503.225699	461307.557754	48.904167
3503.509093	461293.979296	48.909172
3503.728041	461293.384458	48.914177
3503.581176	461264.221080	48.919181
3503.666917	461256.250525	48.924186
3503.152961	461251.777551	48.929191
3503.483011	461231.248688	48.934196
3503.463456	461230.491874	48.939201
3503.388842	461210.842877	48.944205
3503.618289	461201.530226	48.949210
3503.364033	461196.810197	48.954215
3503.906352	461172.393762	48.959220
3503.810440	461169.977722	48.964225
3503.794288	461152.294995	48.969229
3504.115689	461135.720133	48.974234
3503.417389	461100.671053	48.979239
3503.767568	461071.219821	48.984244
3503.767966	461056.574674	48.989249
3503.678257	461045.086749	48.994253
3503.907713	461030.858546	48.999258
3503.751245	461016.898929	49.004263
3503.875297	460998.279973	49.009268
3503.706559	460995.065546	49.014273
3503.365184	460963.806583	49.019277
3503.698845	460938.462660	49.024282
3503.326903	460915.924975	49.029287
3503.733878	460906.328496	49.034292
3503.394466	460897.264860	49.039297
3503.393871	460888.700795	49.044301
3503.446885	460873.438424	49.049306
3503.143954	460871.209722	49.054311
3503.424805	460854.945602	49.059316
3503.637205	460859.368736	49.064321
3503.363971	460833.064122	49.069325
3503.810909	460814.237835	49.074330
3503.448430	460807.762547	49.079335
3503.683591	460791.100772	49.084340
3503.894189	460774.392501	49.089345
3503.734595	460764.842019	49.094349
3503.909306	460755.437153	49.099354
3503.768337	460748.721321	49.104359
3503.542796	460730.567212	49.109364
3503.484527	460721.455490	49.114369
3503.348956	460714.079939	49.119373
3503.751422	460693.335451	49.124378
3503.329118	460675.518944	49.129383
3503.395179	460660.102153	49.134388
3503.713902	460657.716604	49.139393
3503.290104	460630.069177	49.144397
3503.746677	460599.585557	49.149402
3503.482198	460588.127208	49.154407
3503.498996	460576.418119	49.159412
3503.444051	460569.788890	49.164417
3503.524448	460558.474341	49.169421
3503.677218	460545.373760	49.174426
3503.284552	460538.548805	49.179431
3503.404423	460522.666633	49.184436
3503.326362	460515.433217	49.189441
3503.360207	460500.123156	49.194445
3503.294289	460490.505869	49.199450
3503.160805	460487.488045	49.204455
3503.492281	460493.563250	49.209460
3503.234835	460496.293019	49.214465
3503.161825	460494.481102	49.219469
3503.382271	460476.250608	49.224474
3503.162117	460476.085458	49.229479
3503.417729	460462.105763	49.234484
3502.997015	460458.224802	49.239489
3503.278718	460440.997345	49.244493
3503.455629	460429.564889	49.249498
3503.214064	460426.210774	49.254503
3503.683274	460414.170958	49.259508
3503.254619	460408.264281	49.264513
3503.161084	460398.651666	49.269517
3503.559209	460389.715245	49.274522
3503.096054	460369.726342	49.279527
3503.269380	460354.899119	49.284532
3503.522057	460353.538345	49.289537
3503.000497	460346.532624	49.294541
3503.416399	460343.674354	49.299546
3503.064393	460367.096384	49.304551
3502.946552	460359.008200	49.309556
3503.252683	460352.165215	49.314561
3503.241365	460340.562142	49.319565
3503.660719	460331.165979	49.324570
3503.560163	460325.000547	49.329575
3503.251432	460317.502385	49.334580
3503.389417	460307.191395	49.339585
3503.270050	460292.262072	49.344589
3503.466551	460286.451321	49.349594
3503.043325	460280.493001	49.354599
3503.174264	460258.628853	49.359604
3503.437858	460254.783038	49.364609
3503.165020	460255.336359	49.369613
3503.606431	460239.652443	49.374618
3503.633508	460240.154554	49.379623
3503.289825	460222.526921	49.384628
3503.427743	460212.317248	49.389633
3503.527935	460215.138021	49.394637
3503.726351	460194.985302	49.399642
3503.480653	460191.682529	49.404647
3503.461650	460176.685304	49.409652
3503.328067	460170.221401	49.414657
3503.191203	460165.785142	49.419661
3503.198737	460151.442171	49.424666
3503.387779	460146.798229	49.429671
3503.069513	460147.866081	49.434676
3503.121819	460154.597186	49.439681
3503.235782	460161.723178	49.444685
3503.965447	460150.905661	49.449690
3503.491743	460145.918787	49.454695
3503.541159	460133.494386	49.459700
3503.606390	460131.101381	49.464705
3503.485998	460105.631215	49.469709
3503.713525	460075.692675	49.474714
3503.727592	460069.102172	49.479719
3503.622118	460050.774906	49.484724
3503.151711	460040.466305	49.489729
3503.407841	460028.969415	49.494733
3503.828589	460016.481537	49.499738
3503.331068	460008.356685	49.504743
3503.246173	459996.765973	49.509748
3503.435666	459991.767175	49.514753
3503.252179	459981.156164	49.519757
3503.446163	459967.389355	49.524762
3503.319998	459967.664251	49.529767
3503.607428	459953.526733	49.534772
3503.327279	459952.408945	49.539777
3503.153761	459939.769100	49.544781
3503.430573	459944.333475	49.549786
3503.209279	459953.087797	49.554791
3503.520008	459946.142533	49.559796
3503.317199	459949.116436	49.564801
3503.388261	459949.002911	49.569805
3503.537185	459941.730529	49.574810
3503.380787	459937.145522	49.579815
3503.479189	459919.796878	49.584820
3503.460587	459914.326814	49.589825
3503.172133	459901.605214	49.594829
3503.578511	459898.140374	49.599834
3502.962410	459891.860124	49.604839
3503.289640	459884.101174	49.609844
3503.051455	459882.165370	49.614849
3502.992944	459871.786350	49.619853
3503.233490	459853.501175	49.624858
3503.068584	459847.752006	49.629863
3503.155608	459838.817781	49.634868
3503.032670	459854.143495	49.639873
3502.793588	459852.258519	49.644877
3503.434365	459849.615172	49.649882
3503.195026	459849.098545	49.654887
3503.359777	459833.208159	49.659892
3503.234599	459835.256619	49.664897
3502.982345	459822.275397	49.669901
3503.359449	459811.517897	49.674906
3503.038538	459820.187931	49.679911
3503.400520	459822.862703	49.684916
3503.347117	459836.453503	49.689921
3503.224868	459836.677054	49.694925
3503.485764	459824.824487	49.699930
3503.472761	459821.329885	49.704935
3503.111917	459813.688395	49.709940
3503.286431	459800.330220	49.714945
3503.107736	459797.167975	49.719949
3503.372422	459790.686622	49.724954
3503.230402	459791.775077	49.729959
3503.392094	459773.655327	49.734964
3503.331446	459772.398693	49.739969
3503.258385	459760.856501	49.744973
3503.230656	459751.891153	49.749978
3503.254529	459752.343146	49.754983
3503.264374	459740.381360	49.759988
3503.338696	459729.118054	49.764993
3503.360621	459737.425515	49.769997
3503.528450	459729.947115	49.775002
3503.368707	459723.892958	49.780007
3503.413423	459734.933157	49.785012
3503.364801	459718.724365	49.790017
3503.377580	459730.428839	49.795021
3503.477565	459721.796418	49.800026
3503.683367	459724.447193	49.805031
3503.370583	459704.786691	49.810036
3503.256392	459697.052362	49.815041
3503.903144	459694.509332	49.820045
3504.065050	459660.375065	49.825050
3503.874053	459657.873719	49.830055
3504.003742	459647.057019	49.835060
3503.531191	459640.650820	49.840065
3503.453307	459624.649662	49.845069
3503.440893	459609.802920	49.850074
3503.174446	459607.213093	49.855079
3503.162550	459601.387047	49.860084
3502.932517	459595.598246	49.865089
3503.081882	459592.886739	49.870093
3503.390403	459576.211420	49.875098
3503.114811	459573.420434	49.880103
3503.220600	459565.800529	49.885108
3503.225661	459567.624064	49.890113
3503.015393	459581.900645	49.895117
3503.299986	459583.828484	49.900122
3503.284316	459586.010307	49.905127
3503.266302	459582.263126	49.910132
3503.140078	459571.186010	49.915137
3503.229308	459562.504678	49.920141
3502.957288	459552.668735	49.925146
3503.109533	459551.477093	49.930151
3503.315075	459536.542402	49.935156
3503.370669	459542.867722	49.940161
3502.839954	459564.446096	49.945165
3503.322941	459564.870378	49.950170
3503.046254	459565.373695	49.955175
3503.288378	459560.061730	49.960180
3503.568737	459555.655452	49.965185
3503.438713	459547.721054	49.970189
3503.806123	459530.731569	49.975194
3503.164488	459532.412135	49.980199
3503.165660	459522.478852	49.985204
3503.302488	459520.783051	49.990209
3503.049880	459518.798995	49.995213
3503.299873	459503.197864	50.000218
3503.043625	459505.420775	50.005223
3503.255801	459491.549173	50.010228
3503.265297	459505.940321	50.015233
3503.326723	459504.409431	50.020237
3503.484384	459502.203284	50.025242
3502.883656	459502.052428	50.030247
3503.212155	459502.503090	50.035252
3503.445837	459489.387999	50.040257
3503.169113	459484.063248	50.045261
3503.555132	459476.142065	50.050266
3503.196571	459466.675609	50.055271
3503.453012	459465.820923	50.060276
3503.170416	459450.107974	50.065281
3503.361412	459452.964030	50.070285
3503.268404	459440.918268	50.075290
3503.370602	459444.296278	50.080295
3503.191146	459437.383857	50.085300
3503.184317	459430.746031	50.090305
3503.158449	459431.054487	50.095309
3503.259602	459440.919595	50.100314
3503.167263	459454.010513	50.105319
3503.069940	459441.965489	50.110324
3503.393203	459437.602539	50.115329
3503.049475	459442.272987	50.120333
3503.565244	459429.312406	50.125338
3502.950469	459430.177529	50.130343
3503.255468	459417.202250	50.135348
3503.185178	459409.308276	50.140353
3502.856285	459404.904636	50.145357
3502.767738	459419.768699	50.150362
3503.335375	459432.493546	50.155367
3503.099298	459436.841540	50.160372
3503.098175	459427.770145	50.165377
3503.387561	459433.548789	50.170381
3503.410613	459415.959178	50.175386
3503.413020	459420.823925	50.180391
3503.194046	459407.431316	50.185396
3503.433335	459394.974034	50.190401
3503.418521	459391.935778	50.195405
3503.398586	459384.235913	50.200410
3503.336011	459389.821271	50.205415
3503.527253	459373.672600	50.210420
3503.543114	459369.919595	50.215425
3503.236381	459364.954690	50.220429
3503.500250	459355.787336	50.225434
3503.278392	459361.146504	50.230439
3503.348488	459355.306386	50.235444
3503.745119	459346.015000	50.240449
3503.540337	459338.904152	50.245453
3503.327873	459331.338498	50.250458
3503.499389	459332.981594	50.255463
3503.333508	459319.883937	50.260468
3503.560059	459318.882311	50.265473
3503.161884	459311.905833	50.270477
3503.434242	459301.317982	50.275482
3503.344181	459303.765935	50.280487
3503.255285	459318.832850	50.285492
3503.572824	459323.795850	50.290497
3503.459598	459325.386208	50.295501
3503.595751	459312.946484	50.300506
3503.204191	459291.373208	50.305511
3503.477376	459297.509415	50.310516
3503.499458	459294.464845	50.315521
3503.511571	459306.524437	50.320525
3503.776252	459278.149415	50.325530
3503.573298	459254.212639	50.330535
3503.205702	459239.476947	50.335540
3503.450007	459223.015017	50.340545
3503.187263	459223.313243	50.345549
3503.364033	459226.475838	50.350554
3503.365450	459243.301175	50.355559
3503.126482	459245.166406	50.360564
3503.286548	459246.507387	50.365569
3503.221454	459244.795362	50.370573
3503.415278	459236.501466	50.375578
3503.366927	459238.840946	50.380583
3503.118798	459224.186203	50.385588
3503.157233	459226.764264	50.390593
3503.357896	459221.509968	50.395597
3503.415407	459216.432153	50.400602
3503.261494	459209.718009	50.405607
3503.121261	459205.484829	50.410612
3503.060121	459203.011931	50.415617
3503.040382	459205.802646	50.420621
3503.101057	459205.082736	50.425626
3503.303190	459220.809547	50.430631
3503.266353	459217.470948	50.435636
3503.267495	459213.467029	50.440641
3503.011816	459208.290649	50.445645
3503.164765	459202.436340	50.450650
3503.004820	459200.284390	50.455655
3503.103430	459187.850999	50.460660
3503.222713	459202.933136	50.465665
3503.035395	459218.067612	50.470669
3503.162229	459213.535435	50.475674
3503.362356	459212.690354	50.480679
3503.361150	459209.953825	50.485684
3503.618145	459207.933403	50.490689
3503.027036	459199.418760	50.495693
3503.350773	459193.028490	50.500698
3502.858249	459188.450022	50.505703
3503.118991	459190.229934	50.510708
3503.478268	459179.677857	50.515713
3503.409821	459174.874937	50.520717
3503.364210	459167.179372	50.525722
3503.049067	459171.034126	50.530727
3503.196235	459166.093028	50.535732
3503.366608	459144.626362	50.540737
3503.225191	459105.576318	50.545741
3503.293265	459056.709186	50.550746
3503.392347	459016.756342	50.555751
3502.859083	458942.499494	50.560756
3503.498873	458872.704677	50.565761
3503.525897	458785.681454	50.570765
3503.339626	458667.170714	50.575770
3503.121356	458558.243498	50.580775
3503.147412	458423.983861	50.585780
3503.197857	458281.863454	50.590785
3502.743430	458140.132339	50.595789
3502.956273	457979.787095	50.600794
3502.846280	457820.560040	50.605799
3502.629792	457634.082141	50.610804
3503.111325	457442.212181	50.615809
3502.705482	457258.905550	50.620813
3502.821410	457026.394316	50.625818
3503.112933	456810.576701	50.630823
3502.968906	456574.455277	50.635828
3503.433054	456318.053866	50.640833
3503.067612	456046.077712	50.645837
3503.207567	455765.394601	50.650842
3503.026207	455477.970146	50.655847
3503.056430	455171.344771	50.660852
3503.372324	454845.707729	50.665857
3502.984955	454520.337644	50.670861
3502.948049	454173.561104	50.675866
3502.815573	453818.937572	50.680871
3502.535010	453454.650633	50.685876
3503.003244	453076.338958	50.690881
3502.685924	452684.720049	50.695885
3502.857295	452276.026791	50.700890
3502.675143	451845.332202	50.705895
3502.559774	451419.687158	50.710900
3502.572891	450952.995050	50.715905
3502.452997	450513.288267	50.720909
3502.610518	450031.441888	50.725914
3502.354555	449540.984698	50.730919
3502.780224	449035.289614	50.735924
3502.604878	448512.901289	50.740929
3502.405878	447977.979343	50.745933
3502.764020	447415.413919	50.750938
3502.255104	446855.517127	50.755943
3502.557408	446261.845405	50.760948
3502.457518	445663.053131	50.765953
3502.338304	445052.684543	50.770957
3502.388282	444410.521628	50.775962
3502.439570	443752.971995	50.780967
3502.356585	443084.774325	50.785972
3502.331958	442383.070563	50.790977
3501.947053	441685.311334	50.795981
3502.193153	440955.516796	50.800986
3501.857935	440211.898461	50.805991
3501.617321	439458.955795	50.810996
3501.856923	438684.751506	50.816001
3501.911619	437895.231118	50.821005
3501.975955	437083.916851	50.826010
3501.958790	436244.429470	50.831015
3502.139102	435382.908197	50.836020
3501.654882	434511.421420	50.841025
3501.577427	433612.939379	50.846029
3501.450870	432698.649536	50.851034
3501.514629	431772.518133	50.856039
3501.617737	430823.050242	50.861044
3501.862740	429847.180781	50.866049
3501.168140	428864.681192	50.871053
3501.216137	427846.740412	50.876058
3500.772940	426815.744879	50.881063
3500.402369	425773.424154	50.886068
3500.800114	424708.643390	50.891073
3500.255100	423625.702296	50.896077
3500.476216	422521.971776	50.901082
3500.303010	421406.480905	50.906087
3499.991759	420266.797037	50.911092
3500.260583	419104.190782	50.916097
3499.863956	417931.768539	50.921101
3500.064766	416725.474293	50.926106
3500.245660	415512.753328	50.931111
3499.992304	414257.926092	50.936116
3499.692096	412993.371436	50.941121
3499.059521	411720.279874	50.946125
3499.010913	410417.696307	50.951130
3499.024369	409121.742279	50.956135
3498.861075	407786.060227	50.961140
3499.122024	406428.219218	50.966145
3498.561601	405055.337858	50.971149
3498.606960	403667.932825	50.976154
3498.466363	402261.616259	50.981159
3497.972683	400831.765730	50.986164
3498.029956	399396.591438	50.991169
3498.020526	397951.371698	50.996173
3497.664692	396456.493078	51.001178
3497.831791	394961.473679	51.006183
3497.508019	393444.508070	51.011188
3497.428311	391903.841933	51.016193
3497.084802	390350.791478	51.021197
3496.559373	388787.120695	51.026202
3496.668293	387203.819720	51.031207
3496.660638	385595.524872	51.036212
3496.505652	383975.506526	51.041217
3496.251464	382333.588204	51.046221
3495.884227	380680.624392	51.051226
3495.700435	379016.055474	51.056231
3495.648837	377323.746215	51.061236
3495.667795	375623.229721	51.066241
3495.121565	373906.249654	51.071245
3494.992942	372162.390109	51.076250
3494.875824	370406.338678	51.081255
3494.587086	368640.745350	51.086260
3494.630468	366850.342230	51.091265
3494.104385	365052.599881	51.096269
3493.955501	363225.790118	51.101274
3493.654316	361398.079674	51.106279
3493.172391	359544.599291	51.111284
3493.048446	357685.603903	51.116289
3492.950180	355826.925375	51.121293
3492.741608	353918.754392	51.126298
3492.520289	352030.239845	51.131303
3492.057437	350094.693757	51.136308
3492.025174	348153.060197	51.141313
3491.219018	346203.815725	51.146317
3491.210758	344241.858366	51.151322
3491.184293	342271.882429	51.156327
3491.059892	340275.504737	51.161332
3490.649274	338255.708005	51.166337
3490.148496	336249.688847	51.171341
3489.914928	334219.139512	51.176346
3489.493059	332161.566483	51.181351
3489.149273	330116.398230	51.186356
3489.096877	328044.354513	51.191361
3488.692818	325976.851724	51.196365
3488.647608	323875.004715	51.201370
3488.215302	321760.168916	51.206375
3487.890387	319639.464841	51.211380
3487.829162	317508.030806	51.216385
3487.215072	315360.941571	51.221389
3486.998467	313197.730291	51.226394
3486.587579	311010.377637	51.231399
3485.986809	308832.082637	51.236404
3485.711388	306626.072269	51.241409
3485.534711	304430.220637	51.246413
3485.441721	302212.783028	51.251418
3484.867641	299975.206414	51.256423
3484.233003	297734.353057	51.261428
3484.112764	295483.786901	51.266433
3483.601492	293226.924108	51.271437
3483.402514	290950.660103	51.276442
3482.835993	288658.983389	51.281447
3482.143643	286380.936246	51.286452
3482.102337	284066.094648	51.291457
3481.446294	281756.618809	51.296461
3481.113847	279432.487841	51.301466
3481.079076	277101.603364	51.306471
3480.022408	274760.959242	51.311476
3479.855795	272400.579632	51.316481
3479.509540	270057.628805	51.321485
3479.327616	267668.560413	51.326490
3479.071115	265294.846255	51.331495
3478.280234	262911.304084	51.336500
3478.147994	260506.807513	51.341505
3477.476325	258097.532889	51.346509
3476.976583	255674.728410	51.351514
3476.402487	253247.684538	51.356519
3476.174860	250811.774129	51.361524
3475.370901	248371.513399	51.366529
3474.240428	245932.186071	51.371533
3473.899133	243479.164981	51.376538
3473.910134	241033.895815	51.381543
3473.090953	238568.519044	51.386548
3472.796905	236098.214954	51.391553
3472.261196	233624.391678	51.396557
3471.605438	231134.910379	51.401562
3471.296112	228657.147964	51.406567
3470.695020	226158.391762	51.411572
3470.002837	223654.324241	51.416577
3469.535559	221152.433020	51.421581
3468.903805	218629.056088	51.426586
3468.383242	216115.878800	51.431591
3468.187592	213598.328733	51.436596
3467.960204	211066.846483	51.441601
3466.835922	208532.584083	51.446605
3466.152956	205988.697567	51.451610
3465.571983	203445.102597	51.456615
3465.129468	200901.402341	51.461620
3464.758659	198334.318467	51.466625
3463.574937	195782.601093	51.471629
3463.146557	193215.310598	51.476634
3462.276438	190645.359276	51.481639
3461.799069	188088.695808	51.486644
3461.471847	185507.668852	51.491649
3460.643933	182939.530529	51.496653
3460.190166	180366.153302	51.501658
3459.302396	177780.719832	51.506663
3458.906411	175199.211839	51.511668
3458.370091	172611.282472	51.516673
3457.322638	170025.664336	51.521677
3456.417932	167436.041438	51.526682
3455.938878	164851.911176	51.531687
3455.014663	162261.252264	51.536692
3454.415526	159672.397086	51.541697
3453.178791	157083.262785	51.546701
3452.727596	154504.751557	51.551706
3452.108053	151909.724921	51.556711
3451.178026	149341.500757	51.561716
3450.760909	146699.066374	51.566721
3449.855076	144094.932183	51.571725
3449.227486	141496.925366	51.576730
3448.472481	138926.500771	51.581735
3447.095637	136349.648390	51.586740
3446.724374	133766.235809	51.591745
3445.943074	131197.926325	51.596749
3444.879893	128619.332283	51.601754
3444.214823	126060.753586	51.606759
3442.660386	123486.259249	51.611764
3441.947344	120927.999004	51.616769
3440.849433	118397.679798	51.621773
3440.207516	115851.214228	51.626778
3438.945287	113313.411235	51.631783
3438.039283	110787.560525	51.636788
3437.090286	108257.703841	51.641793
3436.056230	105749.390589	51.646797
3435.156650	103235.827616	51.651802
3434.346749	100739.513166	51.656807
3433.043894	98254.801215	51.661812
3432.261523	95761.913560	51.666817
3430.925606	93301.630800	51.671821
3430.081776	90829.507485	51.676826
3429.156687	88374.480639	51.681831
3427.677803	85926.364329	51.686836
3426.834625	83492.892996	51.691841
3425.583430	81082.407512	51.696845
3424.218513	78671.323721	51.701850
3422.601012	76274.895568	51.706855
3421.399154	73901.130655	51.711860
3420.607648	71528.322925	51.716865
3419.027890	69188.797015	51.721869
3417.677985	66850.575138	51.726874
3416.718085	64540.202939	51.731879
3414.983307	62242.251177	51.736884
3414.038290	59963.929219	51.741889
3412.473867	57704.942012	51.746893
3410.609268	55460.004803	51.751898
3409.586198	53239.417604	51.756903
3407.748879	51042.045372	51.761908
3406.397792	48860.782923	51.766913
3404.672236	46720.988181	51.771917
3402.776445	44578.832383	51.776922
3401.420340	42487.912292	51.781927
3398.594780	40430.336965	51.786932
3396.488062	38416.181021	51.791937
3393.541898	36453.163941	51.796941
3390.279110	34533.173254	51.801946
3385.510673	32706.555564	51.806951
3379.295261	30985.735932	51.811956
3373.121117	29359.378265	51.816961
3367.029963	27845.148272	51.821965
3360.775554	26419.800482	51.826970
3354.879051	25138.839602	51.831975
3348.942873	23970.848972	51.836980
3343.555488	22918.197518	51.841985
3338.076183	21986.836328	51.846989
3333.110437	21163.098518	51.851994
3329.097610	20444.236188	51.856999
3324.922671	19799.610116	51.862004
3321.926157	19258.518017	51.867009
3318.844353	18806.626356	51.872013
3316.025793	18413.495488	51.877018
3314.038880	18088.904932	51.882023
3312.116081	17823.085492	51.887028
3311.154693	17595.445341	51.892033
3309.457666	17408.261221	51.897037
3308.205732	17259.555092	51.902042
3307.431137	17138.284874	51.907047
3306.565545	17057.066695	51.912052
3306.346608	16981.842550	51.917057
3305.558189	16928.813697	51.922061
3304.884745	16890.388589	51.927066
3304.734926	16860.443832	51.932071
3304.676984	16851.398757	51.937076
3304.197458	16839.379999	51.942081
3303.793592	16842.508886	51.947085
3303.957075	16835.796808	51.952090
3304.119094	16823.151631	51.957095
3303.738560	16828.429227	51.962100
3303.894574	16821.620437	51.967105
3303.669688	16822.915349	51.972109
3302.937785	16810.792734	51.977114
3302.887854	16789.285351	51.982119
3302.754955	16784.575889	51.987124
3302.756624	16761.189951	51.992129
3302.451564	16760.050305	51.997133
3302.432487	16734.512099	52.002138
3302.595057	16705.377225	52.007143
3302.009275	16666.537784	52.012148
3302.052614	16629.579259	52.017153
3301.623248	16597.983664	52.022157
3300.941802	16552.467330	52.027162
3301.243710	16507.208291	52.032167
3300.913321	16467.821500	52.037172
3300.759639	16416.343794	52.042177
3300.193932	16356.553673	52.047181
3299.884448	16303.429183	52.052186
3299.463007	16237.008388	52.057191
3298.607107	16186.163427	52.062196
3298.377214	16118.752609	52.067201
3298.147483	16058.269229	52.072205
3297.651921	15972.425552	52.077210
3297.136175	15906.731807	52.082215
3296.501686	15835.745140	52.087220
3296.283664	15756.221207	52.092225
3295.592885	15673.358358	52.097229
3295.070685	15588.105968	52.102234
3294.740034	15510.984145	52.107239
3293.728948	15435.428153	52.112244
3293.650129	15352.702580	52.117249
3292.857301	15285.245897	52.122253
3292.257750	15205.039082	52.127258
3291.726062	15127.005147	52.132263
3291.413715	15036.180499	52.137268
3290.750099	14952.949949	52.142273
3290.151492	14873.280317	52.147277
3289.342212	14784.149160	52.152282
3288.709226	14700.168720	52.157287
3288.219674	14618.631100	52.162292
3287.714032	14520.063898	52.167297
3286.997194	14438.262570	52.172301
3286.581361	14350.678450	52.177306
3285.842361	14269.858369	52.182311
3285.234754	14186.897065	52.187316
3285.114832	14091.139488	52.192321
3284.127792	14008.254960	52.197325
3283.618164	13914.442345	52.202330
3283.415516	13815.892359	52.207335
3282.729650	13722.404867	52.212340
3282.332298	13632.267708	52.217345
3281.757616	13523.893886	52.222349
3280.867960	13430.752582	52.227354
3280.283269	13315.706990	52.232359
3279.291010	13229.033184	52.237364
3278.867272	13123.461601	52.242369
3278.263221	13033.521040	52.247373
3277.226561	12931.653465	52.252378
3276.905688	12833.252789	52.257383
3276.013719	12750.826064	52.262388
3275.560949	12660.563045	52.267393
3274.893600	12563.522049	52.272397
3274.041558	12470.171171	52.277402
3273.754155	12372.581294	52.282407
3272.768509	12284.097360	52.287412
3272.177876	12186.901691	52.292417
3271.630483	12097.223604	52.297421
3270.922131	11994.844361	52.302426
3270.462471	11908.522631	52.307431
3269.654418	11816.043317	52.312436
3269.092905	11707.998369	52.317441
3268.292661	11616.738648	52.322445
3267.549520	11524.708102	52.327450
3267.345669	11422.800837	52.332455
3266.749654	11340.635581	52.337460
3266.254878	11236.140545	52.342465
3265.698011	11141.939417	52.347469
3265.199597	11046.221534	52.352474
3264.437050	10941.559245	52.357479
3263.528310	10842.912269	52.362484
3262.931911	10746.026326	52.367489
3261.884237	10641.427311	52.372493
3261.290047	10548.049658	52.377498
3260.699051	10443.969529	52.382503
3259.840389	10359.454161	52.387508
3259.432222	10254.819471	52.392513
3258.547174	10167.260374	52.397517
3257.807404	10078.011719	52.402522
3257.191786	9982.568142	52.407527
3256.856524	9891.036404	52.412532
3256.151757	9796.034138	52.417537
3255.592742	9701.878030	52.422541
3254.574392	9615.834483	52.427546
3254.086898	9514.053940	52.432551
3253.669899	9429.997197	52.437556
3252.789899	9329.618244	52.442561
3252.400803	9244.037905	52.447565
3251.263340	9144.857345	52.452570
3250.831106	9056.185788	52.457575
3249.988581	8962.616373	52.462580
3249.528423	8861.817878	52.467585
3248.820524	8790.841002	52.472589
3247.875434	8686.110667	52.477594
3247.548948	8597.938553	52.482599
3246.839510	8515.614206	52.487604
3246.314719	8417.246531	52.492609
3245.481855	8328.631602	52.497613
3244.679508	8234.860487	52.502618
3244.181336	8142.133479	52.507623
3243.348650	8060.111328	52.512628
3242.953301	7963.503042	52.517633
3241.840869	7876.364029	52.522637
3241.533490	7795.119148	52.527642
3240.822727	7702.126900	52.532647
3239.970352	7600.739025	52.537652
3239.273703	7522.229271	52.542657
3238.703875	7441.284543	52.547661
3237.772947	7352.341843	52.552666
3237.748034	7263.300928	52.557671
3236.750396	7183.193543	52.562676
3236.195054	7089.439811	52.567681
3235.686465	7004.060767	52.572685
3235.121992	6918.931822	52.577690
3234.210733	6822.709160	52.582695
3233.507697	6740.547588	52.587700
3232.930146	6657.643929	52.592705
3232.324817	6568.589919	52.597709
3231.644904	6485.630397	52.602714
3231.219497	6391.584489	52.607719
3230.168433	6306.104392	52.612724
3229.568969	6224.475867	52.617729
3228.830066	6133.779909	52.622733
3228.000244	6044.922744	52.627738
3227.321733	5965.406624	52.632743
3226.674787	5884.679567	52.637748
3226.419833	5801.621767	52.642753
3225.607869	5717.016909	52.647757
3224.511158	5637.516215	52.652762
3224.044636	5553.315991	52.657767
3223.628139	5475.134040	52.662772
3223.057669	5384.487002	52.667777
3222.281121	5307.195800	52.672781
3221.375842	5224.830172	52.677786
3220.992965	5144.935160	52.682791
3220.167551	5069.339485	52.687796
3219.952880	4976.761591	52.692801
3219.008148	4899.109411	52.697805
3218.212856	4823.191510	52.702810
3217.533968	4733.550650	52.707815
3216.754659	4654.939571	52.712820
3216.495237	4576.394837	52.717825
3215.426576	4499.459909	52.722829
3214.538396	4410.795547	52.727834
3214.289354	4325.981873	52.732839
3213.470575	4262.218106	52.737844
3212.706532	4179.407343	52.742849
3212.083643	4096.862700	52.747853
3211.239864	4025.038623	52.752858
3210.963975	3933.326132	52.757863
3210.007426	3866.480233	52.762868
3209.686215	3804.331033	52.767873
3209.077312	3727.011765	52.772877
3208.225316	3645.822566	52.777882
3207.467197	3568.738027	52.782887
3206.908570	3499.990595	52.787892
3206.698939	3416.102068	52.792897
3206.111641	3338.980777	52.797901
3204.778971	3261.286819	52.802906
3204.430285	3174.295671	52.807911
3203.903347	3098.941069	52.812916
3203.209384	3012.673068	52.817921
3202.541198	2931.024222	52.822925
3201.720969	2863.999773	52.827930
3201.145665	2785.679740	52.832935
3199.932607	2709.966513	52.837940
3199.322593	2636.011667	52.842945
3198.675935	2564.460589	52.847949
3198.024154	2488.943096	52.852954
3197.771623	2421.188722	52.857959
3196.970273	2348.081174	52.862964
3196.268759	2278.836827	52.867969
3195.209840	2200.036209	52.872973
3194.710293	2128.521193	52.877978
3194.284901	2060.996078	52.882983
3192.844026	1991.608497	52.887988
3192.404424	1925.089912	52.892993
3191.664447	1862.985942	52.897997
3190.765180	1801.406843	52.903002
3190.545695	1736.882934	52.908007
3189.684974	1676.383354	52.913012
3189.027475	1616.749352	52.918017
3188.456790	1557.401554	52.923021
3187.480094	1483.138563	52.928026
3187.114268	1424.619218	52.933031
3186.205086	1370.113672	52.938036
3185.072617	1313.878738	52.943041
3184.601982	1259.053509	52.948045
3184.108329	1206.028935	52.953050
3183.541947	1140.348134	52.958055
3182.643495	1100.407714	52.963060
3182.263723	1031.423778	52.968065
3181.731435	985.135082	52.973069
3180.872747	927.647618	52.978074
3180.551977	873.713948	52.983079
3179.351102	828.306148	52.988084
3178.604217	777.077383	52.993089
3178.218780	724.674647	52.998093
3177.113535	671.583477	53.003098
3176.308519	616.554334	53.008103
3175.592480	582.150310	53.013108
3175.112352	536.369166	53.018113
3174.579125	485.668541	53.023117
3173.142097	452.396144	53.028122
3172.994498	409.331977	53.033127
3172.027542	375.507724	53.038132
3171.131318	329.831040	53.043137
3170.472602	288.112153	53.048141
3169.739209	267.490709	53.053146
3168.905330	226.100332	53.058151
3168.325710	204.176141	53.063156
3167.482658	184.677603	53.068161
3166.674831	162.643648	53.073165
3165.319224	153.050422	53.078170
3164.671837	138.348414	53.083175
3163.666395	149.377168	53.088180
3162.490348	133.474331	53.093185
3161.846119	136.809294	53.098189
3161.013901	150.465369	53.103194
3160.732904	141.406168	53.108199
3160.170663	150.205956	53.113204
3159.548658	143.666149	53.118209
3158.738706	146.245104	53.123213
3157.957231	149.017347	53.128218
3157.409137	139.489056	53.133223
3156.861092	146.019493	53.138228
3156.216260	152.902382	53.143233
3156.246606	142.776323	53.148237
3155.070823	141.854569	53.153242
3154.569084	137.858373	53.158247
3153.623500	147.871132	53.163252
3153.302590	147.009366	53.168257
3152.624111	140.376581	53.173261
3151.821411	144.555315	53.178266
3151.262667	150.375886	53.183271
3150.417537	149.287904	53.188276
3149.870379	139.188677	53.193281
3149.607414	143.722027	53.198285
3148.719616	138.709841	53.203290
3148.227152	131.763049	53.208295
3147.419243	141.415972	53.213300
3146.944596	153.744668	53.218305
3146.287169	143.105344	53.223309
3145.133728	147.029407	53.228314
3144.936306	142.350836	53.233319
3143.840587	155.104587	53.238324
3143.674381	148.417433	53.243329
3143.184889	142.688655	53.248333
3141.938934	151.930518	53.253338
3141.786377	138.086583	53.258343
3140.972737	148.316398	53.263348
3140.150373	140.982689	53.268353
3139.714449	137.834573	53.273357
3139.007208	141.946473	53.278362
3138.385615	138.630347	53.283367
3137.459209	138.272292	53.288372
3137.101404	148.878162	53.293377
3136.649940	148.108965	53.298381
3135.132602	148.816591	53.303386
3135.424290	137.410780	53.308391
3134.406125	150.347458	53.313396
3133.461739	134.581493	53.318401
3133.202187	135.605520	53.323405
3131.953179	138.979082	53.328410
3131.794568	136.601463	53.333415
3131.211960	144.131335	53.338420
3130.537269	139.530758	53.343425
3130.026000	140.132804	53.348429
3129.307062	139.053264	53.353434
3128.896101	139.166470	53.358439
3128.025283	146.682431	53.363444
3127.239416	141.306261	53.368449
3126.547753	141.430325	53.373453
3126.005063	143.232581	53.378458
3125.770383	133.625488	53.383463
3124.403412	149.168941	53.388468
3123.892291	150.873044	53.393473
3123.554281	137.063168	53.398477
3122.714223	146.711720	53.403482
3122.510119	134.763005	53.408487
3121.471519	146.348070	53.413492
3120.015140	142.500383	53.418497
3120.214653	140.250649	53.423501
3119.948642	145.060829	53.428506
3119.074024	138.360909	53.433511
3117.875196	137.017978	53.438516
3117.196344	143.678525	53.443521
3117.188430	141.673833	53.448525
3116.569468	143.433465	53.453530
3115.411084	137.679643	53.458535
3114.896988	128.127006	53.463540
3113.772183	140.734141	53.468545
3113.604815	140.733493	53.473549
3112.943724	138.748433	53.478554
3112.629512	139.075237	53.483559
3111.522627	144.909334	53.488564
3110.568269	138.393167	53.493569
3110.847339	137.582835	53.498573
3110.219319	148.209611	53.503578
3109.529894	137.539846	53.508583
3108.518467	140.467038	53.513588
3107.354699	139.848366	53.518593
3106.671123	135.967718	53.523597
3105.845613	143.878165	53.528602
3105.575338	137.424717	53.533607
3105.163135	147.799490	53.538612
3104.710474	146.185388	53.543617
3104.243807	133.381559	53.548621
3103.327237	142.142019	53.553626
3102.606261	135.989391	53.558631
3101.768293	138.045781	53.563636
3100.725737	142.758122	53.568641
3100.455210	134.416734	53.573645
3099.785535	136.220953	53.578650
3099.428671	136.708594	53.583655
3098.602358	134.969657	53.588660
3097.988765	138.942403	53.593665
3097.193869	130.325885	53.598669
3096.036026	137.117614	53.603674
3095.691996	142.599924	53.608679
3095.247887	140.437269	53.613684
3094.705190	139.773268	53.618689
3094.260880	129.939900	53.623693
3093.197785	135.376128	53.628698
3093.002852	129.449010	53.633703
3091.779734	142.836745	53.638708
3091.098468	136.189055	53.643713
3090.895065	128.767366	53.648717
3090.306195	137.334466	53.653722
3089.708265	129.176521	53.658727
3089.015894	134.642167	53.663732
3087.996712	138.404352	53.668737
3087.778438	128.601442	53.673741
3086.675516	131.084017	53.678746
3085.653268	128.272534	53.683751
3085.157442	135.779286	53.688756
3084.295474	138.319768	53.693761
3083.789629	136.747123	53.698765
3083.745782	137.889817	53.703770
3083.386758	128.015039	53.708775
3082.631138	136.683261	53.713780
3080.904576	136.486802	53.718785
3080.813978	131.926168	53.723789
3080.292269	134.860868	53.728794
3079.480766	130.834325	53.733799
3078.746944	130.273639	53.738804
3078.151482	133.574618	53.743809
3077.300196	132.027842	53.748813
3076.471451	130.531293	53.753818
3076.752413	126.943727	53.758823
3075.439080	139.241638	53.763828
3075.245815	131.790191	53.768833
3074.691329	129.205883	53.773837
3073.297994	134.905378	53.778842
3073.325128	128.491512	53.783847
3072.257270	133.823953	53.788852
3072.039023	132.475320	53.793857
3071.104317	134.090753	53.798861
3070.048710	136.185913	53.803866
3069.489951	131.628697	53.808871
3068.731243	134.146010	53.813876
3068.573655	128.177777	53.818881
3068.154041	130.192685	53.823885
3066.649839	133.288160	53.828890
3066.601899	133.636571	53.833895
3065.747315	134.230575	53.838900
3065.140857	128.522984	53.843905
3064.288153	127.418943	53.848909
3063.675206	134.155856	53.853914
3062.724654	129.062048	53.858919
3062.304779	132.958274	53.863924
3061.954385	122.930847	53.868929
3061.103811	123.993102	53.873933
3061.048597	133.085183	53.878938
3059.634227	131.070559	53.883943
3059.117826	138.584775	53.888948
3058.737187	137.754932	53.893953
3057.472854	139.982863	53.898957
3057.539987	133.209670	53.903962
3056.970363	126.280421	53.908967
3055.608163	134.169284	53.913972
3055.228853	130.033370	53.918977
3054.964873	127.500870	53.923981
3053.324837	132.044524	53.928986
3053.540387	132.587513	53.933991
3052.577282	120.699830	53.938996
3051.897407	129.410368	53.944001
3051.233249	126.358893	53.949005
3050.591853	138.161078	53.954010
3049.893960	126.147549	53.959015
3049.081775	136.206984	53.964020
3048.499644	128.888302	53.969025
3047.761224	123.257343	53.974029
3046.967807	133.225544	53.979034
3046.149182	125.054401	53.984039
3045.488045	124.946290	53.989044
3045.253953	123.715627	53.994049
3045.404052	128.976134	53.999053
3044.244337	134.665319	54.004058
3043.322866	129.614308	54.009063
3042.484899	122.930253	54.014068
3042.160408	136.721790	54.019073
3041.403304	128.825916	54.024077
3040.493865	136.336635	54.029082
3040.680499	131.011806	54.034087
3039.624471	130.572891	54.039092
3038.933961	133.483545	54.044097
3038.353382	136.070684	54.049101
3037.550088	134.683473	54.054106
3037.155141	128.894351	54.059111
3036.380005	128.810851	54.064116
3035.268407	138.197914	54.069121
3034.624177	130.437093	54.074125
3033.555549	130.902285	54.079130
3033.406984	131.984321	54.084135
3032.457641	131.793224	54.089140
3031.961416	127.242697	54.094145
3031.668753	128.165413	54.099149
3030.891251	127.303916	54.104154
3030.640985	128.462539	54.109159
3029.532103	129.387363	54.114164
3028.648761	129.676819	54.119169
3028.407821	124.361504	54.124173
3027.463683	133.252592	54.129178
3026.538229	120.518109	54.134183
3026.218608	124.851928	54.139188
3025.686964	123.357908	54.144193
3024.938587	127.081719	54.149197
3024.477193	126.116077	54.154202
3023.413138	117.783597	54.159207
3023.065969	127.884748	54.164212
3022.391539	128.985986	54.169217
3021.814666	121.473393	54.174221
3021.149672	127.170014	54.179226
3020.088432	123.063792	54.184231
3020.010470	131.147675	54.189236
3019.013464	128.708068	54.194241
3018.897652	126.741554	54.199245
3017.694607	133.686275	54.204250
3017.373800	126.653333	54.209255
3016.809818	126.004425	54.214260
3015.466291	130.275978	54.219265
3015.315602	122.549641	54.224269
3013.780128	126.749786	54.229274
3013.730346	127.792048	54.234279
3013.498340	126.876418	54.239284
3012.036197	126.457564	54.244289
3011.755031	115.539658	54.249293
3011.561549	119.585086	54.254298
3010.501467	126.500638	54.259303
3009.554908	116.562071	54.264308
3008.287212	124.851225	54.269313
3008.879671	117.502364	54.274317
3007.875766	122.836118	54.279322
3006.864639	126.094842	54.284327
3006.199374	116.975818	54.289332
3006.115830	115.128921	54.294337
3005.494412	125.530742	54.299341
3004.232420	123.588777	54.304346
3003.818191	118.791355	54.309351
3003.019839	115.175862	54.314356
3002.373490	129.833157	54.319361
3001.859889	120.469932	54.324365
3001.090940	128.640705	54.329370
3000.696648	122.621747	54.334375
2999.969353	124.986465	54.339380
2999.233015	124.942918	54.344385
2998.647219	119.982976	54.349389
2997.811891	122.939299	54.354394
2997.628209	122.899995	54.359399
2996.969046	122.000123	54.364404
2996.034664	121.057284	54.369409
2996.134484	123.979725	54.374413
2994.737395	123.183847	54.379418
2993.546086	119.080518	54.384423
2993.105658	129.106816	54.389428
2992.298589	126.883042	54.394433
2992.528444	121.439913	54.399437
2991.450802	131.513919	54.404442
2990.283670	118.481281	54.409447
2990.225571	108.530240	54.414452
2989.337722	121.287134	54.419457
2988.951414	112.810035	54.424461
2988.314802	117.828400	54.429466
2987.675828	122.360077	54.434471
2987.340350	121.841463	54.439476
2986.368887	121.808492	54.444481
2985.106434	121.238683	54.449485
2984.150069	117.227442	54.454490
2984.447044	112.782558	54.459495
2982.975076	117.486184	54.464500
2982.587165	125.943150	54.469505
2982.419106	118.531622	54.474509
2981.087624	124.603446	54.479514
2980.428210	114.401482	54.484519
2980.498012	121.288162	54.489524
2979.495013	124.327611	54.494529
2978.923122	117.107064	54.499533
2978.301640	127.409821	54.504538
2977.589861	124.783327	54.509543
2976.660334	119.716342	54.514548
2976.438837	121.824501	54.519553
2975.895823	115.625705	54.524557
2975.130151	128.750533	54.529562
2974.238776	118.467420	54.534567
2973.204218	115.008741	54.539572
2972.644795	120.501010	54.544577
2972.747492	119.860941	54.549581
2971.408749	119.293119	54.554586
2970.283204	113.253476	54.559591
2970.105276	117.066908	54.564596
2969.333400	122.372068	54.569601
2968.954494	113.809236	54.574605
2967.871964	118.136455	54.579610
2967.762031	116.748794	54.584615
2967.124348	120.074754	54.589620
2966.159298	121.055534	54.594625
2965.536082	115.815817	54.599629
2965.187362	118.165579	54.604634
2964.851897	114.430729	54.609639
2964.181839	116.370021	54.614644
2963.067352	113.821428	54.619649
2962.211045	121.449773	54.624653
2960.969075	126.210810	54.629658
2961.039215	124.274494	54.634663
2961.195248	121.095900	54.639668
2959.624329	126.420375	54.644673
2959.161745	119.189045	54.649677
2958.298640	127.703139	54.654682
2957.501089	129.338569	54.659687
2957.104429	125.738514	54.664692
2956.172180	129.826114	54.669697
2955.961350	121.828622	54.674701
2955.549436	121.165181	54.679706
2954.347996	117.311087	54.684711
2953.842857	116.150432	54.689716
2952.393886	123.299021	54.694721
2952.729443	115.169083	54.699725
2951.824402	116.633808	54.704730
2950.962330	120.375475	54.709735
2950.214716	118.814952	54.714740
2949.371175	129.155263	54.719745
2949.271946	118.073646	54.724749
2948.244985	124.297114	54.729754
2947.871569	121.473859	54.734759
2947.402062	115.986040	54.739764
2946.814616	120.109450	54.744769
2946.427906	112.532799	54.749773
2945.803704	119.622546	54.754778
2944.528266	120.244277	54.759783
2943.492226	110.317865	54.764788
2942.618332	120.636911	54.769793
2942.277906	109.666386	54.774797
2941.551342	112.064929	54.779802
2941.510023	117.399187	54.784807
2940.744843	117.608859	54.789812
2940.189311	121.739447	54.794817
2939.700864	114.709117	54.799821
2938.879968	114.076491	54.804826
2938.336985	115.475398	54.809831
2937.121113	118.025849	54.814836
2936.281875	115.420355	54.819841
2936.037279	111.262228	54.824845
2934.781893	113.817852	54.829850
2934.779609	119.569376	54.834855
2934.141873	112.397590	54.839860
2933.295610	113.459125	54.844865
2933.264284	111.627780	54.849869
2932.474631	109.261308	54.854874
2931.415987	108.132485	54.859879
2930.216959	112.889738	54.864884
2929.403710	117.980133	54.869889
2929.612308	116.319754	54.874893
2928.805511	119.774090	54.879898
2927.815037	115.463566	54.884903
2927.519292	105.992872	54.889908
2926.701293	108.208494	54.894913
2926.311236	108.528926	54.899917
2925.924601	112.454601	54.904922
2925.001800	112.376615	54.909927
2923.844376	119.081841	54.914932
2922.778348	117.819679	54.919937
2922.953490	112.004599	54.924941
2921.939658	113.676204	54.929946
2921.644245	119.175066	54.934951
2921.352855	113.046961	54.939956
2920.444972	115.292550	54.944961
2919.775595	106.341223	54.949965
2918.849348	113.317196	54.954970
2917.799547	115.335598	54.959975
2917.252362	117.982166	54.964980
2916.489355	122.854378	54.969985
2915.911736	113.528955	54.974989
2915.490792	116.423153	54.979994
2915.151568	114.445089	54.984999
2914.484505	109.661680	54.990004
2913.742230	113.240380	54.995009
2913.264324	114.420936	55.000013
2912.636104	122.387665	55.005018
2911.412916	126.338284	55.010023
2910.638639	113.825104	55.015028
2910.092510	119.783249	55.020033
2909.521936	114.781644	55.025037
2908.838748	120.467956	55.030042
2908.183740	117.140212	55.035047
2907.598009	115.262301	55.040052
2906.627184	116.974716	55.045057
2906.114248	113.821240	55.050061
2905.705485	113.260288	55.055066
2905.236808	113.177326	55.060071
2904.751385	105.439534	55.065076
2903.243692	122.871713	55.070081
2902.511948	115.764549	55.075085
2902.075360	117.348955	55.080090
2901.507680	122.640538	55.085095
2900.788209	115.007475	55.090100
2900.393355	112.587747	55.095105
2899.978743	108.379734	55.100109
2899.357330	116.673314	55.105114
2898.938116	118.790001	55.110119
2897.764121	119.433088	55.115124
2896.778335	125.991360	55.120129
2896.049733	125.385992	55.125133
2895.644194	121.761015	55.130138
2894.739965	115.885668	55.135143
2894.459079	112.287941	55.140148
2894.127541	114.500562	55.145153
2893.741567	110.036214	55.150157
2893.437365	118.013485	55.155162
2891.487140	112.025198	55.160167
2890.442872	108.320704	55.165172
2889.718394	111.915706	55.170177
2889.342164	109.295435	55.175181
2889.079139	114.602449	55.180186
2888.087118	115.379039	55.185191
2888.080446	107.767056	55.190196
2887.479480	114.258373	55.195201
2887.078039	110.796906	55.200205
2886.292173	110.621710	55.205210
2885.374387	110.547610	55.210215
2884.190302	111.147426	55.215220
2883.705623	118.469112	55.220225
2883.566520	113.355484	55.225229
2882.870542	110.412105	55.230234
2882.120939	102.334213	55.235239
2881.564613	100.923375	55.240244
2879.996887	109.041976	55.245249
2879.660007	110.112382	55.250253
2878.995924	116.780273	55.255258
2878.328801	110.323634	55.260263
2877.941351	109.605493	55.265268
2877.420684	110.797307	55.270273
2876.941665	110.381782	55.275277
2876.507402	110.481226	55.280282
2875.061357	120.240442	55.285287
2874.492970	104.108765	55.290292
2873.234853	113.188509	55.295297
2873.084358	109.079435	55.300301
2872.642446	106.466048	55.305306
2872.271016	112.565251	55.310311
2872.150860	101.044746	55.315316
2871.160460	108.769032	55.320321
2869.976967	104.045866	55.325325
2868.855321	109.902241	55.330330
2868.296698	110.726341	55.335335
2867.995311	101.973051	55.340340
2867.278094	104.939988	55.345345
2866.756208	109.159955	55.350349
2866.541227	117.686041	55.355354
2865.755226	104.500692	55.360359
2864.760450	102.148763	55.365364
2863.657695	109.521605	55.370369
2863.180067	97.777204	55.375373
2862.457714	106.763407	55.380378
2861.756235	110.640657	55.385383
2861.604067	105.827284	55.390388
2860.834035	109.469546	55.395393
2860.960459	105.649849	55.400397
2860.324257	108.557547	55.405402
2858.671630	109.582041	55.410407
2858.117332	98.366256	55.415412
2857.023095	102.161818	55.420417
2857.101969	109.382843	55.425421
2856.133106	110.453894	55.430426
2855.275141	104.867487	55.435431
2854.704507	110.285096	55.440436
2853.710307	107.144802	55.445441
2853.191736	100.214770	55.450445
2852.772429	114.984026	55.455450
2851.958205	113.739236	55.460455
2851.583931	111.356259	55.465460
2850.954673	118.103460	55.470465
2850.610701	109.986640	55.475469
2849.788352	107.240912	55.480474
2849.160685	116.466326	55.485479
2848.015016	105.060301	55.490484
2847.473561	107.451689	55.495489
2846.908675	103.544885	55.500493
2846.387834	104.473843	55.505498
2845.796475	104.896182	55.510503
2845.561732	102.572647	55.515508
2844.203183	104.050159	55.520513
2843.227258	104.042843	55.525517
2842.615099	100.212013	55.530522
2841.821722	108.434720	55.535527
2841.717395	104.352889	55.540532
2841.213857	103.646303	55.545537
2840.434297	107.207303	55.550541
2840.023582	105.908552	55.555546
2839.155191	110.370500	55.560551
2838.296478	104.404498	55.565556
2837.211065	103.453948	55.570561
2836.770822	102.176429	55.575565
2836.085909	104.351158	55.580570
2835.758450	108.340929	55.585575
2835.317187	97.227802	55.590580
2834.775585	102.171907	55.595585
2833.890081	102.183480	55.600589
2832.920890	109.291926	55.605594
2832.097152	112.992316	55.610599
2831.726099	98.140975	55.615604
2830.695206	106.047837	55.620609
2830.461370	107.419178	55.625613
2829.983049	105.794097	55.630618
2829.313619	103.413807	55.635623
2828.719724	98.486466	55.640628
2827.374081	107.746956	55.645633
2827.134400	103.344060	55.650637
2826.372453	103.397673	55.655642
2825.954999	103.897658	55.660647
2825.459518	104.707023	55.665652
2824.394573	105.381222	55.670657
2823.800594	106.296235	55.675661
2822.781438	104.124923	55.680666
2821.973898	113.760805	55.685671
2821.609964	105.068735	55.690676
2821.196393	96.121477	55.695681
2821.090349	102.789907	55.700685
2820.522348	104.693611	55.705690
2819.757895	102.892046	55.710695
2818.263259	101.849604	55.715700
2817.460221	108.431904	55.720705
2817.055105	103.600980	55.725709
2816.749070	99.734411	55.730714
2815.786645	106.803807	55.735719
2815.788940	98.946361	55.740724
2814.364845	112.391332	55.745729
2813.508233	99.178203	55.750733
2812.796355	104.278515	55.755738
2811.873393	108.015996	55.760743
2811.849264	100.676209	55.765748
2811.469455	101.429490	55.770753
2811.373822	95.258868	55.775757
2810.816821	99.727198	55.780762
2809.470084	96.358230	55.785767
2808.551484	97.901078	55.790772
2807.679388	108.025214	55.795777
2807.636837	100.465951	55.800781
2807.121932	106.218631	55.805786
2806.014410	105.204763	55.810791
2805.426671	107.808533	55.815796
2804.447094	106.147946	55.820801
2804.290710	99.334830	55.825805
2803.800100	100.328490	55.830810
2802.667573	114.787022	55.835815
2801.592035	99.337297	55.840820
2801.102715	106.191627	55.845825
2800.332575	95.396816	55.850829
2799.698043	98.186999	55.855834
2799.050512	105.551513	55.860839
2798.577860	95.453073	55.865844
2797.934719	101.864362	55.870849
2798.027418	101.760854	55.875853
2797.176864	93.301567	55.880858
2796.134968	100.590197	55.885863
2795.643256	94.339251	55.890868
2794.825393	100.596856	55.895873
2793.979563	105.165474	55.900877
2793.616705	100.776134	55.905882
2792.476385	105.829679	55.910887
2792.172288	97.946447	55.915892
2791.090760	100.931447	55.920897
2790.649298	96.617121	55.925901
2789.901436	99.775218	55.930906
2789.136475	95.022777	55.935911
2789.495597	93.862445	55.940916
2788.443037	93.955077	55.945921
2787.880724	88.684858	55.950925
2786.831626	95.091322	55.955930
2785.630476	102.774662	55.960935
2785.406624	93.003561	55.965940
2784.933945	103.486520	55.970945
2784.462058	91.142755	55.975949
2783.876166	97.714385	55.980954
2782.599143	102.984711	55.985959
2782.093976	103.025230	55.990964
2780.974013	104.979463	55.995969
2780.448613	105.764341	56.000973
2780.106666	95.096475	56.005978
2779.188275	98.807915	56.010983
2779.416233	93.102237	56.015988
2778.958742	102.056985	56.020993
2778.210297	100.150852	56.025997
2776.880359	104.189996	56.031002
2776.036597	98.424343	56.036007
2775.883659	101.548255	56.041012
2775.194045	101.250442	56.046017
2774.451976	96.533169	56.051021
2773.545162	102.256521	56.056026
2772.520095	105.537392	56.061031
2772.114809	99.155232	56.066036
2771.638824	108.841808	56.071041
2771.279165	102.758155	56.076045
2770.690055	99.793767	56.081050
2770.022341	107.640929	56.086055
2769.141607	100.218617	56.091060
2767.991628	104.352132	56.096065
2766.943903	108.026077	56.101069
2766.892940	102.495566	56.106074
2766.252497	105.298999	56.111079
2766.003570	98.272764	56.116084
2765.685521	113.057465	56.121089
2764.727342	105.453789	56.126093
2763.295202	103.197161	56.131098
2762.864449	99.824007	56.136103
2762.589483	90.147697	56.141108
2761.915239	103.865146	56.146113
2761.375455	100.183795	56.151117
2760.656603	89.797063	56.156122
2759.500727	104.403653	56.161127
2759.138830	98.657087	56.166132
2758.431871	96.928203	56.171137
2757.577041	105.615745	56.176141
2757.547233	100.552527	56.181146
2756.560616	101.143879	56.186151
2755.630311	90.232780	56.191156
2754.598746	103.664734	56.196161
2754.417915	99.812691	56.201165
2754.129368	93.822676	56.206170
2753.103562	96.914996	56.211175
2753.064443	96.856912	56.216180
2751.639071	101.057631	56.221185
2750.798353	95.398830	56.226189
2750.481319	93.561459	56.231194
2749.358367	102.107334	56.236199
2749.295309	91.173525	56.241204
2748.497556	100.094459	56.246209
2748.201339	92.083183	56.251213
2748.128645	93.799996	56.256218
2746.513375	96.885707	56.261223
2746.206586	90.103045	56.266228
2745.555594	90.785843	56.271233
2744.647374	88.436909	56.276237
2743.560400	86.415362	56.281242
2742.530109	92.648094	56.286247
2742.821931	90.582316	56.291252
2741.596057	91.103648	56.296257
2741.093823	96.292466	56.301261
2740.460697	95.291471	56.306266
2740.009054	103.162882	56.311271
2739.778613	93.377913	56.316276
2739.430943	95.880654	56.321281
2738.051453	95.090124	56.326285
2737.464603	91.942203	56.331290
2736.635884	102.497858	56.336295
2736.627278	99.943051	56.341300
2735.209932	97.691403	56.346305
2734.236424	102.975777	56.351309
2733.895282	97.879333	56.356314
2733.216241	96.905133	56.361319
2733.065776	98.932863	56.366324
2732.397475	95.508741	56.371329
2731.349821	89.285335	56.376333
2730.500766	89.239774	56.381338
2729.594918	97.057375	56.386343
2729.326126	92.404869	56.391348
2728.581381	100.461374	56.396353
2728.229821	86.292374	56.401357
2727.996358	98.338602	56.406362
2726.889289	94.393838	56.411367
2726.315889	92.699760	56.416372
2725.178794	93.299865	56.421377
2724.502663	90.076419	56.426381
2724.187015	96.769221	56.431386
2723.321335	93.025164	56.436391
2723.396126	91.717646	56.441396
2721.991087	99.737020	56.446401
2720.986661	101.413364	56.451405
2720.702331	92.199699	56.456410
2720.564671	95.971110	56.461415
2720.168216	95.068606	56.466420
2719.091389	97.548355	56.471425
2718.201701	100.629651	56.476429
2718.001803	91.746940	56.481434
2716.860559	98.705990	56.486439
2716.339776	89.018813	56.491444
2714.789882	90.165518	56.496449
2713.592580	87.324439	56.501453
2714.104640	82.770169	56.506458
2713.747288	91.559376	56.511463
2713.155214	91.235820	56.516468
2711.962455	96.481490	56.521473
2711.424058	101.474393	56.526477
2711.154975	92.911394	56.531482
2710.691137	94.168898	56.536487
2710.326440	84.025978	56.541492
2708.763974	97.141321	56.546497
2708.236734	96.295514	56.551501
2707.835470	91.013567	56.556506
2707.006495	92.393878	56.561511
2705.874493	82.360013	56.566516
2705.080128	94.703027	56.571521
2704.920549	87.329963	56.576525
2704.365229	91.823271	56.581530
2703.341657	96.152680	56.586535
2703.356674	96.328494	56.591540
2702.983362	92.271733	56.596545
2701.823602	96.535214	56.601549
2701.191126	95.069520	56.606554
2700.419756	97.957309	56.611559
2700.045654	88.765310	56.616564
2699.164846	94.779081	56.621569
2697.574073	99.882399	56.626573
2697.300445	95.147829	56.631578
2696.623530	93.909594	56.636583
2696.875352	89.935447	56.641588
2696.038091	95.489420	56.646593
2695.377162	93.115986	56.651597
2694.357271	97.628709	56.656602
2693.365171	95.797791	56.661607
2693.255221	92.232051	56.666612
2692.382630	92.178677	56.671617
2691.655248	89.906206	56.676621
2691.091771	93.490280	56.681626
2690.806090	94.354579	56.686631
2690.267562	84.193220	56.691636
2688.915855	92.868591	56.696641
2688.052934	93.796825	56.701645
2687.875800	88.664460	56.706650
2687.298362	97.652338	56.711655
2686.800500	91.224835	56.716660
2685.470177	90.291314	56.721665
2684.650314	91.173505	56.726669
2684.074995	88.189800	56.731674
2683.551204	89.370714	56.736679
2683.933621	82.036451	56.741684
2682.832036	94.053834	56.746689
2682.173455	91.766445	56.751693
2681.322743	91.955247	56.756698
2680.480096	93.583023	56.761703
2679.958324	81.805562	56.766708
2679.161532	93.923603	56.771713
2678.632660	91.933771	56.776717
2678.151950	88.969024	56.781722
2676.875759	103.127250	56.786727
2676.221953	89.084527	56.791732
2675.635422	95.976390	56.796737
2675.092428	93.620693	56.801741
2674.727832	87.328699	56.806746
2674.307203	95.241382	56.811751
2674.195897	85.622374	56.816756
2672.922631	91.812965	56.821761
2671.665909	92.613129	56.826765
2671.231188	92.797927	56.831770
2670.365960	98.153400	56.836775
2670.429930	90.296875	56.841780
2669.444949	99.478758	56.846785
2668.512529	93.220274	56.851789
2668.378216	88.887803	56.856794
2667.595114	90.409877	56.861799
2667.135417	89.125042	56.866804
2665.840774	90.236022	56.871809
2664.873949	84.619326	56.876813
2664.761713	81.941322	56.881818
2664.301035	83.940765	56.886823
2663.701442	83.538371	56.891828
2662.309395	82.438965	56.896833
2661.764963	79.556560	56.901837
2661.095416	79.855314	56.906842
2660.169192	91.408917	56.911847
2660.078765	76.653739	56.916852
2659.582873	84.737567	56.921857
2659.103323	88.373214	56.926861
2658.856613	79.336682	56.931866
2657.035639	81.108012	56.936871
2656.351264	73.835721	56.941876
2656.100574	76.360566	56.946881
2655.383778	76.292014	56.951885
2655.645758	76.994409	56.956890
2654.493165	86.752420	56.961895
2653.800253	89.178393	56.966900
2653.268169	88.261186	56.971905
2652.041642	87.377823	56.976909
2651.334792	81.686691	56.981914
2650.548519	93.804512	56.986919
2649.632614	84.274102	56.991924
2648.921669	84.150473	56.996929
2648.841727	86.017731	57.001933
2648.789924	91.396387	57.006938
2648.132952	83.597977	57.011943
2646.964041	73.624127	57.016948
2646.075022	77.816858	57.021953
2645.338009	79.188560	57.026957
2645.088271	82.566244	57.031962
2644.563828	89.119476	57.036967
2643.432927	78.295995	57.041972
2642.641773	78.032530	57.046977
2642.189089	80.023503	57.051981
2641.543449	77.348659	57.056986
2641.049873	80.530796	57.061991
2640.917463	72.533383	57.066996
2639.958107	80.323026	57.072001
2638.534970	76.054566	57.077005
2638.562750	74.759033	57.082010
2637.531715	83.121044	57.087015
2637.068390	75.092176	57.092020
2635.816993	78.250704	57.097025
2634.969675	78.479590	57.102029
2635.175745	70.265244	57.107034
2634.107276	72.980014	57.112039
2633.585687	75.414989	57.117044
2633.291784	77.816568	57.122049
2632.560864	81.565051	57.127053
2632.290672	81.839355	57.132058
2630.652602	85.994351	57.137063
2630.234741	78.321251	57.142068
2629.870433	83.744642	57.147073
2628.767086	82.483001	57.152077
2628.869000	76.581385	57.157082
2627.682044	88.440077	57.162087
2626.507065	79.399213	57.167092
2626.200403	81.002473	57.172097
2625.526139	88.146562	57.177101
2625.503442	82.904911	57.182106
2624.819281	80.514145	57.187111
2624.324143	85.639780	57.192116
2623.150435	81.691041	57.197121
2622.693958	82.998606	57.202125
2621.991312	80.362325	57.207130
2620.578908	84.401380	57.212135
2620.067483	77.178869	57.217140
2619.697209	80.135461	57.222145
2618.550186	85.023992	57.227149
2618.315107	83.140650	57.232154
2617.605105	86.311235	57.237159
2617.687841	80.215930	57.242164
2617.204892	78.435355	57.247169
2616.178428	83.779314	57.252173
2614.859429	82.830848	57.257178
2614.384781	85.704629	57.262183
2614.254677	74.890859	57.267188
2613.652364	77.381081	57.272193
2612.613568	85.193387	57.277197
2611.657482	83.203571	57.282202
2611.299643	86.188828	57.287207
2610.983281	83.842159	57.292212
2609.983320	77.348539	57.297217
2609.052813	87.797251	57.302221
2608.473487	79.527697	57.307226
2608.010104	85.176834	57.312231
2607.575416	78.380534	57.317236
2607.251747	80.128013	57.322241
2605.461559	84.887292	57.327245
2604.645826	80.999332	57.332250
2604.158059	83.645627	57.337255
2603.953687	85.296926	57.342260
2603.589796	83.014829	57.347265
2602.768008	83.602107	57.352269
2602.560175	82.216198	57.357274
2601.340860	82.425789	57.362279
2600.710334	82.724984	57.367284
2599.371241	82.978341	57.372289
2599.239826	84.238627	57.377293
2598.963394	76.492410	57.382298
2597.319569	82.970561	57.387303
2597.474368	79.927579	57.392308
2596.999199	79.756940	57.397313
2595.973340	84.996591	57.402317
2595.902201	81.029895	57.407322
2594.975468	89.761702	57.412327
2593.485609	88.971920	57.417332
2592.878122	85.105597	57.422337
2592.087050	84.218855	57.427341
2592.131409	79.723220	57.432346
2591.287442	88.809945	57.437351
2591.074386	86.421540	57.442356
2590.671288	82.014635	57.447361
2589.545189	77.715146	57.452365
2589.146145	82.116612	57.457370
2588.149577	89.333170	57.462375
2587.684402	85.100687	57.467380
2586.803604	82.609336	57.472385
2585.589207	81.528131	57.477389
2585.112058	80.016953	57.482394
2584.669104	84.198565	57.487399
2584.677202	91.757699	57.492404
2583.968601	79.997596	57.497409
2582.686045	81.503619	57.502413
2581.654431	80.471297	57.507418
2581.019903	83.033343	57.512423
2580.544964	78.840031	57.517428
2580.179647	78.297336	57.522433
2579.326396	86.097662	57.527437
2579.077130	73.457749	57.532442
2578.696874	87.108736	57.537447
2577.974676	76.492110	57.542452
2577.319133	72.416119	57.547457
2576.568114	83.384391	57.552461
2575.726936	71.455125	57.557466
2574.371276	74.980425	57.562471
2573.847660	75.532521	57.567476
2573.444344	84.018535	57.572481
2572.506761	78.002929	57.577485
2572.349457	79.208827	57.582490
2571.792402	88.527547	57.587495
2571.125949	75.514100	57.592500
2569.878972	81.389956	57.597505
2569.043938	88.783367	57.602509
2568.864993	74.380041	57.607514
2568.474688	80.383777	57.612519
2567.814635	77.019852	57.617524
2567.493886	80.290468	57.622529
2566.596896	75.184080	57.627533
2565.814431	79.936085	57.632538
2564.978075	75.877587	57.637543
2564.483816	81.201223	57.642548
2563.707737	80.351395	57.647553
2562.557993	85.317371	57.652557
2561.883768	69.672843	57.657562
2561.334166	81.551254	57.662567
2560.627451	86.066898	57.667572
2560.415727	73.428464	57.672577
2560.148338	86.011371	57.677581
2559.784645	74.945842	57.682586
2558.624370	85.671854	57.687591
2557.790977	85.616932	57.692596
2557.629263	83.290408	57.697601
2556.235473	81.276751	57.702605
2555.648045	72.369143	57.707610
2554.759949	83.917016	57.712615
2553.940465	81.003097	57.717620
2553.895455	78.724909	57.722625
2553.136089	76.004392	57.727629
2552.924034	83.044200	57.732634
2551.610609	80.962728	57.737639
2550.947841	78.388322	57.742644
2550.517464	79.222497	57.747649
2549.618039	75.003474	57.752653
2549.493705	78.091701	57.757658
2549.117043	79.235630	57.762663
2548.128000	82.021308	57.767668
2547.314551	91.444651	57.772673
2546.560046	85.132494	57.777677
2545.527796	74.961634	57.782682
2544.620311	84.613806	57.787687
2544.393980	77.081260	57.792692
2543.905903	78.640145	57.797697
2543.060530	81.079167	57.802701
2543.032451	76.375663	57.807706
2542.323632	79.471054	57.812711
2541.437161	82.478400	57.817716
2540.570545	77.819573	57.822721
2539.613527	83.629679	57.827725
2539.650095	73.382276	57.832730
2538.374919	81.529069	57.837735
2537.348740	74.892718	57.842740
2536.922958	73.846433	57.847745
2536.026495	80.013280	57.852749
2536.098110	75.938501	57.857754
2535.407757	76.752783	57.862759
2535.095999	76.874729	57.867764
2534.724183	79.327130	57.872769
2533.500533	75.547606	57.877773
2532.906298	74.624460	57.882778
2532.547627	85.423423	57.887783
2530.974029	77.292291	57.892788
2530.262604	74.497268	57.897793
2529.412622	85.471014	57.902797
2529.025960	75.520566	57.907802
2528.509893	79.435213	57.912807
2528.140193	84.221257	57.917812
2528.172340	79.045629	57.922817
2526.416749	77.636582	57.927821
2525.961047	77.466569	57.932826
2525.540669	85.483014	57.937831
2524.834048	81.609967	57.942836
2524.448921	78.928101	57.947841
2522.925784	80.018178	57.952845
2522.683319	73.751117	57.957850
2521.815195	79.461950	57.962855
2521.491145	69.661850	57.967860
2520.972420	75.848587	57.972865
2520.382519	75.074696	57.977869
2519.493156	60.856793	57.982874
2518.354635	76.658782	57.987879
2517.946988	80.025965	57.992884
2517.591426	76.573675	57.997889
2516.828202	75.044311	58.002893
2516.675717	69.990644	58.007898
2515.129636	79.795017	58.012903
2514.443460	84.461095	58.017908
2514.176225	73.846437	58.022913
2513.317683	82.308438	58.027917
2513.410092	73.832880	58.032922
2512.157341	77.492173	58.037927
2511.040631	74.763680	58.042932
2510.704420	79.683335	58.047937
2510.208778	79.031089	58.052941
2509.712771	79.095723	58.057946
2509.069330	71.324638	58.062951
2507.971239	81.493724	58.067956
2507.649362	78.666839	58.072961
2506.574891	79.039181	58.077965
2506.438302	76.219302	58.082970
2505.958888	77.136861	58.087975
2504.922274	73.746539	58.092980
2503.812696	74.401980	58.097985
2503.429563	78.180221	58.102989
2503.061970	77.085702	58.107994
2502.486264	84.113868	58.112999
2501.806441	82.469592	58.118004
2501.054336	72.305323	58.123009
2499.742860	83.068242	58.128013
2499.410090	79.070101	58.133018
2499.063372	84.677583	58.138023
2498.646547	77.006302	58.143028
2498.098522	81.406005	58.148033
2496.671950	84.251495	58.153037
2495.978721	72.264194	58.158042
2495.516026	77.601381	58.163047
2495.284527	80.588329	58.168052
2495.026069	81.882572	58.173057
2493.716308	81.178471	58.178061
2492.635508	76.483248	58.183066
2492.620735	82.154368	58.188071
2492.187800	86.251379	58.193076
2491.425824	83.793808	58.198081
2489.950072	83.136639	58.203085
2489.722432	74.602121	58.208090
2489.532096	83.907481	58.213095
2488.797547	80.825110	58.218100
2487.781198	81.453168	58.223105
2486.890396	81.659906	58.228109
2486.735836	76.703302	58.233114
2485.774532	76.746836	58.238119
2484.734280	81.144252	58.243124
2483.870737	71.892301	58.248129
2482.884488	84.912304	58.253133
2482.646197	76.944852	58.258138
2481.975417	73.718954	58.263143
2481.855354	75.757668	58.268148
2481.676495	64.601351	58.273153
2480.686656	76.584629	58.278157
2480.578784	70.542843	58.283162
2479.499041	72.313808	58.288167
2478.446016	81.017082	58.293172
2478.603881	73.347809	58.298177
2476.945725	87.829095	58.303181
2476.457052	79.671958	58.308186
2475.780045	78.446007	58.313191
2475.012047	80.828388	58.318196
2474.634014	77.777037	58.323201
2473.419532	80.492720	58.328205
2472.302616	77.767824	58.333210
2472.380545	80.163464	58.338215
2471.919622	79.006354	58.343220
2471.680770	82.948212	58.348225
2470.634532	77.535398	58.353229
2470.402220	71.571335	58.358234
2469.083502	80.146357	58.363239
2468.076404	78.928292	58.368244
2467.925156	74.172039	58.373249
2466.910288	76.293876	58.378253
2466.760600	75.019214	58.383258
2466.379989	76.709725	58.388263
2465.235656	79.549597	58.393268
2464.268174	80.674945	58.398273
2463.542443	82.073160	58.403277
2463.591131	78.767672	58.408282
2463.280979	71.600380	58.413287
2462.489999	77.549072	58.418292
2461.627951	73.164604	58.423297
2460.476051	79.233030	58.428301
2459.951299	70.448538	58.433306
2458.855351	73.410001	58.438311
2458.149409	73.588294	58.443316
2457.804596	67.815963	58.448321
2456.988816	80.208022	58.453325
2456.658780	72.178501	58.458330
2456.250943	75.543744	58.463335
2456.027926	72.403525	58.468340
2455.573688	73.351124	58.473345
2454.218978	71.682514	58.478349
2453.447518	67.753465	58.483354
2452.776263	75.466627	58.488359
2451.558817	74.604257	58.493364
2450.861357	68.139088	58.498369
2450.316528	78.451994	58.503373
2449.882091	74.903464	58.508378
2449.328586	71.907381	58.513383
2448.766362	79.526510	58.518388
2448.924959	68.765246	58.523393
2447.473707	75.144583	58.528397
2446.687744	71.804179	58.533402
2445.843990	79.090930	58.538407
2445.435361	72.002844	58.543412
2445.523744	66.495910	58.548417
2444.242784	74.445156	58.553421
2443.363679	69.084694	58.558426
2442.863859	72.426586	58.563431
2442.000410	74.682401	58.568436
2441.956127	72.316464	58.573441
2440.928337	77.992238	58.578445
2439.782411	75.358753	58.583450
2439.408534	73.583232	58.588455
2438.571214	76.525346	58.593460
2438.258522	67.262906	58.598465
2437.586438	73.391000	58.603469
2437.438880	80.610032	58.608474
2436.195763	79.346673	58.613479
2435.388815	79.630657	58.618484
2435.126777	70.239165	58.623489
2434.312693	80.692448	58.628493
2433.542098	73.626385	58.633498
2433.065185	78.819168	58.638503
2432.504221	71.778840	58.643508
2432.254035	72.354063	58.648513
2430.730404	87.795611	58.653517
2429.994412	72.469960	58.658522
2429.704390	73.840652	58.663527
2428.852983	83.095623	58.668532
2428.526219	80.734960	58.673537
2427.342296	81.087743	58.678541
2426.620044	75.963744	58.683546
2426.124480	78.929529	58.688551
2425.729543	79.400428	58.693556
2425.585204	82.405630	58.698561
2424.812050	81.054814	58.703565
2423.774574	82.232398	58.708570
2423.053799	77.001177	58.713575
2422.291756	77.010258	58.718580
2421.881414	75.515700	58.723585
2420.698293	76.500300	58.728589
2419.750773	71.090753	58.733594
2419.202269	83.370802	58.738599
2418.702728	86.548840	58.743604
2418.255822	81.226582	58.748609
2417.832702	82.876209	58.753613
2417.815176	81.527242	58.758618
2416.692062	82.352772	58.763623
2415.606454	90.144684	58.768628
2414.971844	80.835839	58.773633
2414.184454	83.105100	58.778637
2413.904835	80.760060	58.783642
2413.480184	75.654650	58.788647
2412.022425	87.429009	58.793652
2411.839993	81.301688	58.798657
2410.636144	86.683109	58.803661
2410.334524	78.242562	58.808666
2410.189848	73.984909	58.813671
2409.258866	75.568615	58.818676
2408.645205	73.499370	58.823681
2408.009847	75.258704	58.828685
2407.810103	74.430746	58.833690
2406.697389	70.625579	58.838695
2405.809706	67.486912	58.843700
2405.501847	76.950510	58.848705
2404.771601	72.379706	58.853709
2404.142457	70.099170	58.858714
2402.943873	76.665043	58.863719
2402.000199	72.701898	58.868724
2401.914499	71.273408	58.873729
2401.234240	85.921432	58.878733
2400.602879	75.007091	58.883738
2399.821373	83.056862	58.888743
2398.665425	80.888111	58.893748
2398.222054	72.878767	58.898753
2397.473722	83.419491	58.903757
2397.020374	70.407154	58.908762
2397.026670	70.778267	58.913767
2395.916591	76.056419	58.918772
2395.973040	73.301431	58.923777
2395.070471	83.056582	58.928781
2393.909350	70.593936	58.933786
2393.493725	77.196059	58.938791
2392.962138	77.101004	58.943796
2391.724032	80.690319	58.948801
2390.988372	79.859658	58.953805
2390.604985	75.597824	58.958810
2390.031584	76.392915	58.963815
2389.475035	76.162002	58.968820
2388.380956	79.657613	58.973825
2387.452066	82.125540	58.978829
2387.196579	75.242979	58.983834
2386.949717	76.549453	58.988839
2386.113404	78.149736	58.993844
2385.682144	69.358746	58.998849
2384.748501	75.640906	59.003853
2384.084651	71.196907	59.008858
2383.406337	72.283481	59.013863
2382.902688	75.984835	59.018868
2382.567259	65.775799	59.023873
2381.264593	69.763376	59.028877
2380.413127	59.959938	59.033882
2379.931148	73.191727	59.038887
2379.314904	75.503566	59.043892
2379.325554	65.056545	59.048897
2378.226307	76.471187	59.053901
2377.425033	73.393536	59.058906
2377.179603	71.414484	59.063911
2376.612627	72.759117	59.068916
2375.560789	69.642603	59.073921
2374.421512	74.563395	59.078925
2374.344212	77.302931	59.083930
2373.858279	77.075733	59.088935
2372.704290	84.994205	59.093940
2371.935560	75.479760	59.098945
2371.066028	87.596422	59.103949
2369.940355	79.410073	59.108954
2369.931996	70.343490	59.113959
2369.326025	76.447653	59.118964
2369.206485	77.961691	59.123969
2368.918887	86.507649	59.128973
2368.057622	74.922915	59.133978
2366.861226	74.457214	59.138983
2366.162825	78.649355	59.143988
2365.823845	76.786559	59.148993
2364.537233	77.552822	59.153997
2363.660607	74.670420	59.159002
2363.410367	76.760209	59.164007
2363.382156	77.816540	59.169012
2362.581712	76.497636	59.174017
2361.931333	79.991985	59.179021
2360.742488	80.635745	59.184026
2359.954178	72.630129	59.189031
2359.194051	74.009369	59.194036
2359.097663	70.308313	59.199041
2358.670538	77.088055	59.204045
2357.522564	76.355533	59.209050
2356.751889	75.398238	59.214055
2356.253188	76.736329	59.219060
2356.012091	74.884822	59.224065
2355.504423	75.374213	59.229069
2354.460506	65.948675	59.234074
2353.766884	69.457126	59.239079
2352.735578	68.032443	59.244084
2352.440766	68.725428	59.249089
2351.280896	69.525677	59.254093
2350.395663	68.905329	59.259098
2349.796379	62.213009	59.264103
2349.480962	68.011311	59.269108
2349.194167	69.379480	59.274113
2348.600227	66.115598	59.279117
2347.953981	70.395133	59.284122
2347.504307	61.244947	59.289127
2346.090323	73.318518	59.294132
2345.912757	66.403694	59.299137
2345.465040	74.414150	59.304141
2344.646675	66.616172	59.309146
2343.545620	68.414094	59.314151
2342.342719	71.386364	59.319156
2342.499037	67.031462	59.324161
2341.616210	73.697290	59.329165
2341.458475	76.489657	59.334170
2341.109342	76.611689	59.339175
2339.587320	79.998123	59.344180
2338.956611	71.004017	59.349185
2338.319147	73.870522	59.354189
2338.129381	82.855653	59.359194
2337.914789	67.811126	59.364199
2336.656201	67.768553	59.369204
2335.920949	65.017109	59.374209
2335.017274	76.224634	59.379213
2334.901389	69.800561	59.384218
2333.925669	72.722539	59.389223
2332.763593	80.117414	59.394228
2332.195035	74.973863	59.399233
2331.791142	76.329690	59.404237
2331.325106	72.885258	59.409242
2330.681530	68.341490	59.414247
2329.942726	68.088067	59.419252
2329.127808	68.470136	59.424257
2328.348721	74.104579	59.429261
2328.213600	73.635035	59.434266
2327.828371	68.137648	59.439271
2326.377073	70.130854	59.444276
2326.179873	67.849885	59.449281
2325.791099	71.461336	59.454285
2324.386214	65.610173	59.459290
2323.765077	69.766998	59.464295
2322.861859	73.068540	59.469300
2322.726100	67.731382	59.474305
2322.391116	69.988815	59.479309
2321.554890	70.099802	59.484314
2320.417997	70.759555	59.489319
2319.530122	81.334009	59.494324
2319.243333	70.595629	59.499329
2318.664360	67.830095	59.504333
2318.114097	69.580412	59.509338
2317.633278	69.770752	59.514343
2316.249061	74.707386	59.519348
2316.224157	74.657532	59.524353
2315.070033	78.114477	59.529357
2314.533839	67.324015	59.534362
2314.266139	62.874655	59.539367
2313.477354	70.641468	59.544372
2312.813453	70.706016	59.549377
2311.981140	75.496566	59.554381
2311.471119	71.291133	59.559386
2311.261349	64.396821	59.564391
2309.660652	79.642744	59.569396
2308.881344	70.323147	59.574401
2308.499563	84.315410	59.579405
2307.843042	82.634020	59.584410
2307.875729	77.238056	59.589415
2306.854282	75.363290	59.594420
2306.346115	72.425786	59.599425
2305.450975	75.291359	59.604429
2304.876387	69.350715	59.609434
2304.315746	70.990312	59.614439
2303.350051	73.881371	59.619444
2302.528521	72.938701	59.624449
2301.565999	75.900662	59.629453
2300.935492	75.551752	59.634458
2300.981185	72.993993	59.639463
2300.401009	79.433211	59.644468
2300.011912	67.068705	59.649473
2299.396744	72.195924	59.654477
2298.534435	74.106575	59.659482
2297.380467	66.053378	59.664487
2296.892542	76.033666	59.669492
2296.660926	73.069397	59.674497
2295.398537	77.981256	59.679501
2294.857687	74.897373	59.684506
2294.661932	72.747206	59.689511
2293.312954	72.715758	59.694516
2292.668189	74.059885	59.699521
2291.734413	81.390069	59.704525
2291.025770	80.510593	59.709530
2291.028259	74.236405	59.714535
2290.415397	84.345822	59.719540
2290.585098	68.896126	59.724545
2289.434533	73.115070	59.729549
2288.518632	80.876392	59.734554
2288.074327	66.239042	59.739559
2286.369862	68.949737	59.744564
2286.155065	58.767460	59.749569
2285.344787	73.000350	59.754573
2285.039340	68.716914	59.759578
2284.723247	60.778589	59.764583
2283.276444	67.161931	59.769588
2282.692685	72.543113	59.774593
2282.033454	66.099467	59.779597
2281.340986	78.473992	59.784602
2280.781599	65.912436	59.789607
2280.292836	76.253643	59.794612
2280.126525	58.056519	59.799617
2279.653406	67.321400	59.804621
2278.675086	70.230805	59.809626
2278.005877	68.790792	59.814631
2277.097224	73.194150	59.819636
2276.381947	56.419544	59.824641
2275.429211	64.702666	59.829645
2274.565711	63.635341	59.834650
2274.576787	59.677108	59.839655
2273.878084	64.753878	59.844660
2273.420735	67.662609	59.849665
2272.004413	74.617039	59.854669
2271.094049	72.899330	59.859674
2270.722109	64.147559	59.864679
2270.251565	68.328765	59.869684
2270.210938	66.729156	59.874689
2269.837367	64.262439	59.879693
2269.419739	75.924854	59.884698
2268.247869	72.155099	59.889703
2267.085026	72.883640	59.894708
2266.399834	73.585759	59.899713
2265.083261	72.839854	59.904718
2264.496209	75.266707	59.909722
2264.199676	70.421241	59.914727
2263.857178	72.460890	59.919732
2263.708494	72.094322	59.924737
2263.113183	72.689890	59.929742
2261.787208	77.711309	59.934746
2260.583765	71.173633	59.939751
2260.066148	76.337461	59.944756
2260.101393	71.594726	59.949761
2259.751473	75.486104	59.954766
2259.126681	71.957125	59.959770
2258.400322	72.806412	59.964775
2257.225498	73.372799	59.969780
2256.890615	61.299024	59.974785
2255.605593	74.956680	59.979790
2254.697492	73.738306	59.984794
2254.197236	68.756372	59.989799
2253.819731	69.702705	59.994804
2253.464894	73.358880	59.999809
2253.293565	73.344330	60.004814
2251.994852	70.971880	60.009818
2251.077533	68.180141	60.014823
2250.441020	73.129836	60.019828
2250.274580	70.818348	60.024833
2249.533943	72.516363	60.029838
2248.203600	74.406802	60.034842
2247.638407	76.222440	60.039847
2246.960908	79.239874	60.044852
2246.631759	70.342633	60.049857
2246.123571	76.923087	60.054862
2245.744695	75.107781	60.059866
2245.517772	63.829067	60.064871
2243.753698	68.250828	60.069876
2243.573133	68.298645	60.074881
2243.180110	77.142086	60.079886
2241.666114	77.250577	60.084890
2241.157967	68.386713	60.089895
2240.513070	83.656685	60.094900
2240.120322	78.391110	60.099905
2240.073260	77.065750	60.104910
2238.800481	81.099560	60.109914
2238.176999	70.258121	60.114919
2237.462564	75.619024	60.119924
2237.269791	71.797490	60.124929
2236.144873	73.233605	60.129934
2234.923896	85.078014	60.134938
2234.622307	76.369867	60.139943
2233.914645	87.460596	60.144948
2233.873280	78.720971	60.149953
2233.322469	87.672320	60.154958
2232.227114	79.941073	60.159962
2231.508047	69.491759	60.164967
2230.770003	73.369780	60.169972
2230.089497	67.494235	60.174977
2229.399107	72.301967	60.179982
2228.337971	72.506299	60.184986
2227.894448	76.601179	60.189991
2227.018049	73.191810	60.194996
2226.907114	69.340887	60.200001
2226.342799	80.136316	60.205006
2225.908264	77.833969	60.210010
2225.070780	71.736594	60.215015
2223.830534	77.539515	60.220020
2223.229993	74.898466	60.225025
2223.146171	73.990299	60.230030
2222.422654	88.656770	60.235034
2221.742611	77.910263	60.240039
2220.427799	83.475684	60.245044
2220.076166	69.724835	60.250049
2219.618132	74.351519	60.255054
2219.040922	83.235936	60.260058
2218.689171	77.855199	60.265063
2217.533069	85.606689	60.270068
2216.985387	69.378142	60.275073
2216.619405	73.001094	60.280078
2216.072218	75.562838	60.285082
2215.387252	73.930930	60.290087
2214.205545	72.275426	60.295092
2213.847401	69.462272	60.300097
2213.029821	76.331289	60.305102
2211.747169	75.575649	60.310106
2211.471966	79.392280	60.315111
2210.263554	85.082792	60.320116
2210.142565	74.027135	60.325121
2209.882260	79.754044	60.330126
2209.409685	77.755430	60.335130
2209.219544	69.825965	60.340135
2207.680594	77.513854	60.345140
2206.739504	75.883119	60.350145
2206.666642	73.374847	60.355150
2205.596230	78.908734	60.360154
2204.963828	69.103793	60.365159
2203.938534	71.705859	60.370164
2203.928090	69.059812	60.375169
2203.010349	68.312422	60.380174
2202.771655	73.327895	60.385178
2202.099089	70.975474	60.390183
2201.148164	73.751525	60.395188
2200.469439	71.661464	60.400193
2199.821003	69.802661	60.405198
2199.253403	70.458625	60.410202
2198.251213	71.252070	60.415207
2197.342262	74.898807	60.420212
2197.043118	70.926132	60.425217
2196.578517	70.997659	60.430222
2196.138010	84.737467	60.435226
2195.532540	77.780972	60.440231
2194.361161	74.607972	60.445236
2193.927171	68.023982	60.450241
2193.355773	65.300589	60.455246
2192.380764	72.861243	60.460250
2191.644146	74.564103	60.465255
2190.865195	79.867364	60.470260
2190.401626	75.560848	60.475265
2190.011238	71.173531	60.480270
2189.537699	78.410406	60.485274
2189.018828	68.418689	60.490279
2187.497165	78.934575	60.495284
2187.320348	72.978418	60.500289
2186.538118	80.195459	60.505294
2185.911180	75.421113	60.510298
2185.726628	70.651237	60.515303
2184.058414	79.717900	60.520308
2183.806007	75.477109	60.525313
2183.163055	78.445616	60.530318
2182.580490	83.531745	60.535322
2182.527927	71.112861	60.540327
2181.396161	77.578922	60.545332
2180.717279	68.782556	60.550337
2180.177953	66.965489	60.555342
2179.418940	71.306951	60.560346
2178.322216	59.963072	60.565351
2177.340859	72.800668	60.570356
2176.927599	62.666558	60.575361
2176.531224	66.257998	60.580366
2176.078193	72.864544	60.585370
2175.907345	62.582005	60.590375
2175.100996	72.375572	60.595380
2173.923296	70.055470	60.600385
2173.412099	75.651609	60.605390
2172.986233	70.367631	60.610394
2172.317984	66.982673	60.615399
2170.866971	68.068402	60.620404
2170.242683	66.084294	60.625409
2169.999587	64.053939	60.630414
2169.170299	69.171998	60.635418
2169.036525	53.136366	60.640423
2168.270427	66.496857	60.645428
2167.866699	67.722407	60.650433
2167.308122	62.711384	60.655438
2166.261439	61.154770	60.660442
2164.684948	58.740251	60.665447
2164.129209	74.971110	60.670452
2164.116982	66.358353	60.675457
2163.572542	67.499815	60.680462
2162.832268	71.021394	60.685466
2162.697828	71.723274	60.690471
2161.852106	74.561073	60.695476
2160.725861	71.389047	60.700481
2160.237371	69.459474	60.705486
2159.261721	80.839972	60.710490
2159.175748	62.488214	60.715495
2157.873110	67.686047	60.720500
2157.195802	73.084420	60.725505
2156.405770	75.129565	60.730510
2155.496546	77.061681	60.735514
2155.456615	66.017831	60.740519
2155.015164	77.520901	60.745524
2154.770090	67.413683	60.750529
2154.228204	71.208426	60.755534
2152.808896	72.438732	60.760538
2152.556824	76.181936	60.765543
2151.307105	86.678952	60.770548
2150.239950	72.758002	60.775553
2149.888100	77.202325	60.780558
2149.147069	87.219591	60.785562
2148.982440	68.200780	60.790567
2148.320854	78.592464	60.795572
2147.988435	70.294592	60.800577
2147.623834	74.051515	60.805582
2146.810053	70.893548	60.810586
2145.873714	72.246113	60.815591
2144.664336	82.462290	60.820596
2144.224035	75.162569	60.825601
2143.189379	70.647036	60.830606
2142.319319	80.673341	60.835610
2142.666893	75.576412	60.840615
2142.093409	77.057568	60.845620
2141.831410	78.116780	60.850625
2140.595023	70.953219	60.855630
2139.779308	76.281716	60.860634
2139.217050	70.654374	60.865639
2137.913221	73.812492	60.870644
2137.027479	72.953855	60.875649
2136.764523	77.580336	60.880654
2136.004890	71.537558	60.885658
2135.853923	74.376133	60.890663
2135.404424	73.590115	60.895668
2134.590091	68.675337	60.900673
2133.968902	77.085712	60.905678
2132.849758	71.913999	60.910682
2132.905950	70.243362	60.915687
2132.032759	81.356873	60.920692
2130.994582	72.473948	60.925697
2130.251989	73.787063	60.930702
2129.457338	74.087935	60.935706
2129.132913	79.819889	60.940711
2128.981500	80.263366	60.945716
2127.942287	76.784367	60.950721
2126.784704	68.247909	60.955726
2126.282077	69.153284	60.960730
2126.092734	68.734861	60.965735
2125.133626	73.869209	60.970740
2124.789167	67.187025	60.975745
2123.338403	69.579649	60.980750
2122.983031	78.950312	60.985754
2122.705217	75.490291	60.990759
2121.953571	83.519971	60.995764
2121.273475	74.619617	61.000769
2120.357026	72.602594	61.005774
2119.497029	76.127288	61.010778
2119.341922	71.242255	61.015783
2118.588923	80.288179	61.020788
2118.205650	85.521798	61.025793
2117.148775	74.538598	61.030798
2116.366546	82.028398	61.035802
2116.047484	76.183810	61.040807
2115.348498	74.872066	61.045812
2114.641462	75.471364	61.050817
2113.749199	58.732605	61.055822
2112.760073	76.387930	61.060826
2112.566327	67.590311	61.065831
2112.286398	77.000962	61.070836
2111.612895	76.312862	61.075841
2110.879694	65.615745	61.080846
2110.211305	66.097911	61.085850
2109.581610	74.148175	61.090855
2108.697327	68.039490	61.095860
2108.106719	75.044950	61.100865
2107.268126	69.717895	61.105870
2106.660022	75.125750	61.110874
2106.260341	72.119981	61.115879
2104.643831	69.282077	61.120884
2104.109978	70.032933	61.125889
2103.961082	68.152252	61.130894
2103.480899	72.249065	61.135898
2103.036058	71.892105	61.140903
2102.143196	71.618092	61.145908
2101.414017	75.787098	61.150913
2100.309952	65.560375	61.155918
2099.878210	74.777130	61.160922
2099.646801	62.872390	61.165927
2098.736190	72.096052	61.170932
2098.499168	67.969478	61.175937
2097.621485	64.011298	61.180942
2096.370404	68.450748	61.185946
2095.907288	56.679588	61.190951
2095.796515	66.718511	61.195956
2094.971965	68.713122	61.200961
2093.977219	63.194105	61.205966
2093.148460	70.119117	61.210970
2092.854957	66.519685	61.215975
2092.742604	61.617476	61.220980
2091.433473	60.250630	61.225985
2090.807892	67.749945	61.230990
2089.894757	68.792640	61.235994
2089.841071	64.680892	61.240999
2089.236383	62.568316	61.246004
2088.069252	72.828581	61.251009
2087.295914	69.377930	61.256014
2086.391844	69.428718	61.261018
2086.555930	68.383419	61.266023
2085.676959	77.801403	61.271028
2084.475394	72.546699	61.276033
2083.514619	74.936836	61.281038
2082.963631	74.360016	61.286042
2083.027517	75.753080	61.291047
2082.493819	75.631575	61.296052
2081.635081	66.249047	61.301057
2081.568460	63.999046	61.306062
2080.146516	64.458929	61.311066
2079.459740	64.208483	61.316071
2078.752158	72.642712	61.321076
2078.735410	72.025433	61.326081
2077.834174	70.356724	61.331086
2076.796401	69.819354	61.336090
2076.543511	67.663579	61.341095
2076.004682	73.562857	61.346100
2074.669716	72.714360	61.351105
2074.238418	70.329769	61.356110
2073.211064	83.763381	61.361114
2072.913031	64.798200	61.366119
2072.480064	74.588299	61.371124
2071.641689	69.414367	61.376129
2070.926980	63.498127	61.381134
2070.164696	72.161178	61.386138
2069.833980	63.681063	61.391143
2069.392338	78.443380	61.396148
2068.554865	66.740199	61.401153
2067.603956	67.669364	61.406158
2067.035746	70.899820	61.411162
2066.768827	66.367458	61.416167
2066.030590	68.103371	61.421172
2064.625571	72.984800	61.426177
2064.143543	73.385756	61.431182
2063.357830	77.735745	61.436186
2063.308414	63.925741	61.441191
2062.680160	69.542299	61.446196
2061.910054	74.716165	61.451201
2061.225875	66.984904	61.456206
2060.237274	82.637723	61.461210
2059.980594	67.952545	61.466215
2059.344732	71.180759	61.471220
2058.125482	64.949785	61.476225
2057.495795	67.417104	61.481230
2056.812174	72.796826	61.486234
2056.577949	67.591003	61.491239
2056.067324	73.768472	61.496244
2055.448850	71.243800	61.501249
2054.650699	65.417622	61.506254
2053.648570	77.967871	61.511258
2053.480888	62.738153	61.516263
2052.617482	69.781986	61.521268
2051.579418	75.969546	61.526273
2051.203539	64.372145	61.531278
2050.285566	76.274470	61.536282
2050.063647	66.365011	61.541287
2049.577787	75.138276	61.546292
2048.560641	71.039361	61.551297
2048.182314	63.726691	61.556302
2047.538664	70.228875	61.561306
2046.346741	61.585824	61.566311
2045.581365	76.378644	61.571316
2044.783912	70.934832	61.576321
2044.325003	70.075041	61.581326
2043.934044	71.223417	61.586330
2043.733188	63.103579	61.591335
2042.903485	73.655065	61.596340
2041.749168	66.469604	61.601345
2041.100154	74.815663	61.606350
2040.306803	69.584300	61.611354
2040.484922	71.432673	61.616359
2039.298375	69.370291	61.621364
2038.310829	76.792980	61.626369
2037.924100	72.686097	61.631374
2037.241845	74.725058	61.636378
2036.938338	79.370317	61.641383
2036.337116	67.160567	61.646388
2035.143084	73.158499	61.651393
2034.661757	61.920181	61.656398
2034.105651	75.548301	61.661402
2033.795279	67.359961	61.666407
2032.234119	67.928536	61.671412
2031.751662	76.230711	61.676417
2031.194279	71.236476	61.681422
2030.659170	71.613752	61.686426
2030.219608	69.916606	61.691431
2029.892985	69.029451	61.696436
2028.780867	70.749984	61.701441
2028.414774	63.830340	61.706446
2027.320050	76.462741	61.711450
2026.833390	70.581706	61.716455
2025.744163	71.740978	61.721460
2025.029671	68.353295	61.726465
2024.539746	64.837599	61.731470
2024.023872	77.883334	61.736474
2023.753542	64.036917	61.741479
2023.629517	64.006388	61.746484
2022.162891	69.987795	61.751489
2021.912289	63.747449	61.756494
2020.244021	75.480497	61.761498
2019.458970	61.692920	61.766503
2019.327493	69.963080	61.771508
2018.249538	71.841976	61.776513
2018.081340	73.883792	61.781518
2017.234432	66.944558	61.786522
2017.161505	67.481582	61.791527
2016.428148	73.049413	61.796532
2016.019678	68.021420	61.801537
2015.168250	65.677125	61.806542
2014.237564	67.953181	61.811546
2013.754148	59.638139	61.816551
2012.577297	65.571557	61.821556
2011.748821	71.715769	61.826561
2011.381522	63.759401	61.831566
2010.708513	78.413664	61.836570
2010.559685	76.300485	61.841575
2009.647002	69.310136	61.846580
2008.951309	62.553452	61.851585
2008.098307	59.969832	61.856590
2007.091232	70.588368	61.861594
2006.783152	66.606584	61.866599
2006.537606	66.502504	61.871604
2005.907595	63.565751	61.876609
2004.770462	66.074484	61.881614
2003.998237	68.176600	61.886618
2003.955276	62.347563	61.891623
2003.701991	62.881098	61.896628
2002.199537	70.343317	61.901633
2002.003251	57.555124	61.906638
2001.366755	67.302272	61.911642
2000.608492	65.355316	61.916647
1999.166935	65.443195	61.921652
1998.653072	67.288756	61.926657
1998.308226	57.495861	61.931662
1997.646697	64.301091	61.936666
1997.558407	62.863979	61.941671
1996.454187	72.098268	61.946676
1995.403980	69.135504	61.951681
1995.103026	57.219395	61.956686
1994.304970	70.179582	61.961690
1994.158874	66.780724	61.966695
1992.757751	65.677919	61.971700
1992.047513	66.317253	61.976705
1991.732315	59.717318	61.981710
1991.105107	70.826643	61.986714
1990.825486	64.410087	61.991719
1989.842353	70.388133	61.996724
1988.597290	68.326300	62.001729
1988.404714	62.812188	62.006734
1987.875011	60.768113	62.011738
1987.606407	62.361332	62.016743
1986.493175	64.285345	62.021748
1985.415045	69.305864	62.026753
1985.408585	63.640314	62.031758
1984.692480	72.564275	62.036762
1984.041693	62.031114	62.041767
1983.049749	65.137884	62.046772
1981.733917	70.786411	62.051777
1981.783770	64.242446	62.056782
1981.378504	77.954495	62.061786
1980.928340	65.696025	62.066791
1979.790159	65.164009	62.071796
1978.853231	71.333487	62.076801
1978.501514	59.458034	62.081806
1977.744531	67.774800	62.086810
1977.227841	61.604056	62.091815
1976.850970	57.971927	62.096820
1975.582944	70.918171	62.101825
1975.388979	63.642262	62.106830
1974.745693	68.187358	62.111834
1974.390676	63.430086	62.116839
1972.914524	59.405369	62.121844
1972.502192	62.559431	62.126849
1971.463812	66.492405	62.131854
1971.118263	64.238019	62.136858
1970.915448	58.883156	62.141863
1970.547634	59.925344	62.146868
1969.258438	61.131464	62.151873
1969.226777	62.885854	62.156878
1967.792075	67.767643	62.161882
1966.802273	64.845473	62.166887
1966.151371	66.400675	62.171892
1965.242196	65.838171	62.176897
1965.410098	60.795270	62.181902
1964.828338	76.762946	62.186906
1964.185383	63.050941	62.191911
1963.892474	62.985754	62.196916
1962.725092	61.761265	62.201921
1962.252747	61.565333	62.206926
1961.413244	69.774248	62.211930
1960.833796	60.643571	62.216935
1959.836527	60.994523	62.221940
1958.704570	61.586797	62.226945
1958.581295	68.257718	62.231950
1957.758187	67.597601	62.236954
1957.644097	66.181086	62.241959
1957.271591	65.385861	62.246964
1956.186314	72.259245	62.251969
1955.157867	57.311402	62.256974
1955.113805	72.191999	62.261978
1954.259716	63.206589	62.266983
1953.373333	58.797579	62.271988
1952.067341	66.283827	62.276993
1951.673385	56.316191	62.281998
1951.170622	54.975641	62.287002
1950.828227	64.107631	62.292007
1950.730813	64.388329	62.297012
1949.861624	64.955389	62.302017
1949.443323	60.392097	62.307022
1948.598873	65.983278	62.312026
1947.690184	69.830914	62.317031
1946.792455	54.490467	62.322036
1946.068202	64.080923	62.327041
1945.467822	55.978529	62.332046
1944.897180	61.021178	62.337050
1943.988582	57.636324	62.342055
1943.358987	63.372716	62.347060
1942.146250	65.252183	62.352065
1942.023310	65.684083	62.357070
1941.242951	63.581450	62.362074
1940.931824	63.085977	62.367079
1941.058574	67.343035	62.372084
1939.691592	75.331940	62.377089
1938.967103	69.861064	62.382094
1938.141368	73.717405	62.387098
1937.872155	64.845883	62.392103
1936.750476	65.283251	62.397108
1935.763435	66.194541	62.402113
1935.575913	60.310901	62.407118
1935.124001	71.269058	62.412122
1934.779602	74.254008	62.417127
1933.788844	71.181618	62.422132
1932.333258	64.892037	62.427137
1931.911744	62.827092	62.432142
1931.712203	61.885442	62.437146
1931.714639	57.961463	62.442151
1931.044267	58.930287	62.447156
1929.545695	58.067977	62.452161
1929.628766	59.857211	62.457166
1927.940399	68.877240	62.462170
1927.074465	62.487577	62.467175
1926.813741	67.406950	62.472180
1926.093636	69.776464	62.477185
1925.544540	65.087134	62.482190
1925.116461	65.385717	62.487194
1924.627693	63.830416	62.492199
1923.713924	65.838339	62.497204
1922.547687	69.894242	62.502209
1922.242048	61.696429	62.507214
1921.548091	66.804385	62.512218
1920.804124	58.334996	62.517223
1920.621976	51.049182	62.522228
1919.892757	62.649617	62.527233
1919.364484	61.888937	62.532238
1918.520638	72.838358	62.537242
1917.865112	69.351794	62.542247
1917.506233	62.192127	62.547252
1916.335320	66.754073	62.552257
1915.657901	61.890917	62.557262
1915.146651	70.804702	62.562266
1914.662693	63.133954	62.567271
1913.678931	64.757158	62.572276
1912.826518	68.897527	62.577281
1912.625581	63.141310	62.582286
1911.755862	68.340913	62.587290
1910.979803	58.052616	62.592295
1911.165096	68.267442	62.597300
1909.497501	71.478761	62.602305
1908.999732	62.418986	62.607310
1908.575450	66.652289	62.612314
1908.314442	67.266094	62.617319
1907.700667	62.324159	62.622324
1906.132394	66.837249	62.627329
1905.860842	65.142161	62.632334
1905.456241	63.359313	62.637338
1904.407687	64.248765	62.642343
1903.326779	63.101071	62.647348
1902.571823	64.674476	62.652353
1902.194831	62.749542	62.657358
1901.565719	72.496616	62.662362
1901.117695	61.986021	62.667367
1900.846442	66.322613	62.672372
1900.668136	72.506389	62.677377
1900.069033	59.372274	62.682382
1898.829605	56.878862	62.687386
1898.260781	60.514418	62.692391
1897.273778	61.269793	62.697396
1896.638806	70.049223	62.702401
1896.414821	61.610085	62.707406
1895.268478	70.739096	62.712410
1894.266078	71.865776	62.717415
1893.305574	68.272713	62.722420
1892.530523	64.019135	62.727425
1892.755207	66.070708	62.732430
1892.498400	70.872968	62.737434
1892.279768	65.255958	62.742439
1891.044913	61.818383	62.747444
1889.931415	69.866949	62.752449
1889.521828	61.206549	62.757454
1888.797278	68.422815	62.762458
1887.646709	69.782863	62.767463
1887.140239	58.216131	62.772468
1886.089655	70.670860	62.777473
1885.941391	62.593754	62.782478
1885.675621	70.712808	62.787482
1884.894009	70.136389	62.792487
1884.433108	64.145582	62.797492
1883.203245	67.707529	62.802497
1882.757596	59.573542	62.807502
1882.085917	58.739116	62.812506
1881.944902	57.243531	62.817511
1880.654976	63.390121	62.822516
1879.675718	65.498857	62.827521
1879.350008	59.741097	62.832526
1878.897989	69.201698	62.837530
1878.457085	64.331636	62.842535
1877.218808	59.339055	62.847540
1876.239394	67.457047	62.852545
1876.431854	62.307713	62.857550
1875.667170	67.941306	62.862554
1875.154513	62.885370	62.867559
1874.303385	62.188220	62.872564
1873.323797	64.118204	62.877569
1872.832503	61.983101	62.882574
1872.276723	59.083010	62.887578
1871.705390	64.293933	62.892583
1871.256705	69.216254	62.897588
1870.210350	66.254834	62.902593
1869.922332	58.110066	62.907598
1869.008789	66.491514	62.912602
1867.766195	68.700960	62.917607
1867.073321	63.409027	62.922612
1866.677484	61.662577	62.927617
1866.734999	62.886203	62.932622
1866.133496	65.936062	62.937626
1864.963530	65.178597	62.942631
1864.183446	57.078149	62.947636
1863.261917	62.146099	62.952641
1863.065502	51.480766	62.957646
1862.363717	61.173165	62.962650
1861.411500	63.962906	62.967655
1860.772854	57.292412	62.972660
1860.074640	59.807391	62.977665
1859.809886	57.621690	62.982670
1859.244961	59.087986	62.987674
1858.434288	57.158310	62.992679
1857.638673	55.721038	62.997684
1856.755294	64.687038	63.002689
1856.317118	54.388711	63.007694
1855.919099	57.196921	63.012698
1854.350185	59.130239	63.017703
1854.131270	57.571012	63.022708
1853.093972	61.662100	63.027713
1852.853594	52.171874	63.032718
1852.706317	71.523743	63.037722
1852.110338	62.387627	63.042727
1852.028740	62.405105	63.047732
1850.479177	63.061349	63.052737
1849.844333	58.170396	63.057742
1849.165720	59.325368	63.062746
1848.331421	57.821692	63.067751
1847.420401	57.360179	63.072756
1846.583268	56.482225	63.077761
1846.816951	62.450646	63.082766
1846.445348	60.175863	63.087770
1845.095482	52.659595	63.092775
1844.738165	50.951951	63.097780
1843.876310	66.555047	63.102785
1843.463358	54.692471	63.107790
1841.993136	64.889749	63.112794
1841.251917	66.976317	63.117799
1840.673166	66.337962	63.122804
1840.137793	61.949444	63.127809
1839.671637	59.840832	63.132814
1838.918628	62.371898	63.137818
1839.102970	62.346245	63.142823
1838.628283	65.645976	63.147828
1836.746477	64.686636	63.152833
1836.671158	54.756477	63.157838
1836.244016	60.252586	63.162842
1835.500066	55.589900	63.167847
1834.504466	54.340789	63.172852
1833.821051	71.753942	63.177857
1833.414905	53.738875	63.182862
1832.353294	62.361175	63.187866
1831.045652	64.478736	63.192871
1831.056712	60.351189	63.197876
1830.179661	62.547441	63.202881
1829.840045	60.072589	63.207886
1829.522217	61.434246	63.212890
1828.796672	67.920058	63.217895
1828.863953	62.539521	63.222900
1827.719810	66.895990	63.227905
1827.078154	58.246098	63.232910
1825.790647	60.004571	63.237914
1824.952013	64.256666	63.242919
1824.267578	59.283417	63.247924
1823.729235	62.256158	63.252929
1823.813094	67.065261	63.257934
1822.910061	62.084018	63.262938
1821.982725	71.606997	63.267943
1821.088885	61.972398	63.272948
1820.447378	71.858957	63.277953
1820.277660	65.305991	63.282958
1819.513671	69.828727	63.287962
1818.531473	66.077558	63.292967
1818.255400	54.962851	63.297972
1817.481880	66.213252	63.302977
1817.214955	55.113954	63.307982
1816.041235	65.564836	63.312986
1815.169600	56.467211	63.317991
1814.488328	60.910663	63.322996
1814.103089	68.756877	63.328001
1813.948905	58.575354	63.333006
1812.556211	60.006446	63.338010
1811.354306	63.215874	63.343015
1811.554925	59.882440	63.348020
1810.983848	54.874405	63.353025
1810.162042	56.703196	63.358030
1809.137334	58.427367	63.363034
1808.175835	62.221689	63.368039
1807.803836	59.207271	63.373044
1807.464823	57.174800	63.378049
1807.844097	59.863442	63.383054
1806.496652	73.933248	63.388058
1805.201686	71.838950	63.393063
1804.933024	63.036036	63.398068
1803.832071	63.202265	63.403073
1804.045833	51.348519	63.408078
1802.806250	59.112755	63.413082
1801.921153	62.133775	63.418087
1801.428164	58.282726	63.423092
1800.819005	64.432059	63.428097
1800.344722	48.257407	63.433102
1799.349709	58.332330	63.438106
1798.829162	59.888929	63.443111
1798.103325	49.807591	63.448116
1797.114243	62.722698	63.453121
1797.055721	62.795831	63.458126
1796.469369	56.046537	63.463130
1795.772556	58.661936	63.468135
1794.863227	58.857352	63.473140
1794.115478	58.827762	63.478145
1793.932925	56.957199	63.483150
1793.079284	58.402245	63.488154
1791.843716	67.593899	63.493159
1791.748793	55.691522	63.498164
1791.257259	61.767442	63.503169
1790.748312	60.784795	63.508174
1789.239665	58.975343	63.513178
1788.434808	66.609154	63.518183
1788.027479	60.043957	63.523188
1787.696331	56.906504	63.528193
1787.529827	58.429763	63.533198
1786.793906	53.787818	63.538202
1785.615111	58.061409	63.543207
1785.150645	56.633802	63.548212
1784.127090	60.741890	63.553217
1784.096527	53.153851	63.558222
1782.762143	57.034870	63.563226
1782.053988	56.531948	63.568231
1782.024520	56.020266	63.573236
1781.300231	59.141268	63.578241
1780.600043	59.070780	63.583246
1779.748117	66.663305	63.588250
1778.750031	73.957565	63.593255
1778.365497	51.730308	63.598260
1777.722708	69.361099	63.603265
1777.428863	64.847189	63.608270
1776.307220	67.656065	63.613274
1775.443317	60.064958	63.618279
1775.238307	59.697385	63.623284
1774.333667	66.241869	63.628289
1774.102159	63.081052	63.633294
1772.979395	63.089185	63.638298
1772.296452	63.989128	63.643303
1772.147921	60.501891	63.648308
1771.425366	64.934253	63.653313
1770.518574	54.146938	63.658318
1769.397821	55.669269	63.663322
1768.992942	63.287929	63.668327
1768.544422	52.965733	63.673332
1767.706643	65.369450	63.678337
1767.531027	58.324496	63.683342
1766.555555	66.025789	63.688346
1765.806348	60.492078	63.693351
1765.570655	58.268650	63.698356
1764.431641	63.931959	63.703361
1763.491626	63.302534	63.708366
1762.984276	63.290234	63.713370
1762.148147	67.085217	63.718375
1761.866109	62.955324	63.723380
1761.300399	64.643202	63.728385
1761.422419	63.181560	63.733390
1759.974524	59.770210	63.738394
1759.098612	59.653611	63.743399
1758.821639	58.976261	63.748404
1758.215559	61.841786	63.753409
1757.539724	53.509590	63.758414
1756.569195	59.541158	63.763418
1755.674000	65.943507	63.768423
1755.622378	66.618198	63.773428
1754.522287	68.428301	63.778433
1754.113760	69.613647	63.783438
1753.604289	70.427070	63.788442
1752.607465	63.042651	63.793447
1751.801745	67.733183	63.798452
1750.539549	53.801163	63.803457
1750.321414	67.659974	63.808462
1749.845112	60.726863	63.813466
1749.535571	64.415955	63.818471
1749.169723	58.486666	63.823476
1748.235477	73.247191	63.828481
1746.966223	68.793213	63.833486
1746.444451	66.158492	63.838490
1745.922137	74.093291	63.843495
1745.768923	64.753546	63.848500
1744.508172	62.885507	63.853505
1744.060708	68.075638	63.858510
1743.770057	63.613682	63.863514
1743.019778	69.991633	63.868519
1742.664272	58.156744	63.873524
1741.210690	65.846299	63.878529
1740.461067	61.905359	63.883534
1739.983159	70.463322	63.888538
1739.235861	73.438274	63.893543
1739.175585	67.463407	63.898548
1738.101203	73.886554	63.903553
1737.214908	62.368660	63.908558
1736.666529	64.028313	63.913562
1735.898241	68.021287	63.918567
1735.644797	67.523852	63.923572
1734.816765	68.494413	63.928577
1734.010225	64.436114	63.933582
1733.189344	66.508300	63.938586
1732.720264	58.362167	63.943591
1732.456627	58.802752	63.948596
1732.000467	68.680883	63.953601
1730.799915	63.995691	63.958606
1730.159590	60.509321	63.963610
1729.204927	64.709047	63.968615
1729.370312	62.599748	63.973620
1727.937231	64.367759	63.978625
1727.111082	64.516982	63.983630
1726.367777	68.877114	63.988634
1725.989854	68.781489	63.993639
1725.859713	61.782834	63.998644
1725.327977	67.624858	64.003649
1724.498069	66.736610	64.008654
1723.656471	69.740330	64.013658
1722.801564	72.458578	64.018663
1722.494061	60.999145	64.023668
1721.964881	60.194039	64.028673
1720.724383	63.902304	64.033678
1719.931012	64.077891	64.038682
1719.634802	67.087758	64.043687
1719.313145	61.355770	64.048692
1718.082456	68.137623	64.053697
1717.728254	60.786141	64.058702
1716.661971	66.281888	64.063706
1716.283653	63.499472	64.068711
1715.993207	56.207738	64.073716
1715.209376	73.854376	64.078721
1714.566748	68.117706	64.083726
1714.067110	66.404820	64.088730
1713.180893	62.422130	64.093735
1712.361734	64.773881	64.098740
1711.054767	62.937048	64.103745
1710.498884	59.832137	64.108750
1710.303387	58.741391	64.113754
1709.678196	64.487306	64.118759
1709.562407	60.863028	64.123764
1708.695094	67.197456	64.128769
1707.478925	66.110053	64.133774
1706.973635	64.622337	64.138778
1706.456147	61.569669	64.143783
1706.247260	55.266965	64.148788
1705.026267	61.231667	64.153793
1704.102264	63.594649	64.158798
1703.855968	61.508033	64.163802
1703.244231	58.745035	64.168807
1702.906481	54.643631	64.173812
1701.122090	59.375717	64.178817
1700.736243	58.510562	64.183822
1700.086020	60.558682	64.188826
1699.783759	68.578582	64.193831
1699.852048	59.663161	64.198836
1698.661306	69.491735	64.203841
1697.426472	60.286559	64.208846
1697.001060	69.217626	64.213850
1696.312888	60.919917	64.218855
1696.453216	63.626147	64.223860
1695.225128	57.682181	64.228865
1694.284527	59.196593	64.233870
1693.988464	64.347791	64.238874
1693.314464	63.170381	64.243879
1692.919273	62.864959	64.248884
1691.699709	63.643194	64.253889
1691.161207	54.865161	64.258894
1690.217249	58.184412	64.263898
1689.897480	57.390448	64.268903
1689.641623	54.258673	64.273908
1688.843417	64.790174	64.278913
1688.145849	52.464778	64.283918
1688.013930	58.387588	64.288922
1686.700847	61.549356	64.293927
1686.163919	56.269852	64.298932
1684.871548	59.555966	64.303937
1684.270319	61.821877	64.308942
1684.110293	62.600772	64.313946
1682.939535	64.249699	64.318951
1682.340909	55.345382	64.323956
1681.664590	63.161668	64.328961
1681.352621	60.312641	64.333966
1680.888616	67.553806	64.338970
1680.188762	65.648616	64.343975
1679.446964	59.360529	64.348980
1678.623415	75.538500	64.353985
1678.233198	62.572371	64.358990
1677.773049	63.779187	64.363994
1676.114528	64.559911	64.368999
1675.941334	59.556834	64.374004
1675.143857	63.575729	64.379009
1674.582997	66.073540	64.384014
1674.161247	56.885547	64.389018
1673.539118	66.338543	64.394023
1672.967931	50.260633	64.399028
1671.533006	59.602855	64.404033
1671.425418	57.855648	64.409038
1671.250587	50.450591	64.414042
1670.296463	53.966970	64.419047
1669.415486	53.679156	64.424052
1668.408463	61.300991	64.429057
1667.649198	59.525176	64.434062
1667.778135	49.268390	64.439066
1667.236473	65.267856	64.444071
1666.283558	54.779372	64.449076
1665.005093	63.715498	64.454081
1664.906430	49.826371	64.459086
1664.621419	50.548104	64.464090
1663.239544	57.604901	64.469095
1662.663392	54.916737	64.474100
1661.761720	62.963026	64.479105
1661.634289	53.748356	64.484110
1661.280251	57.750970	64.489114
1660.037616	59.611534	64.494119
1659.130738	46.146099	64.499124
1658.974504	53.457742	64.504129
1658.570545	58.990543	64.509134
1658.195869	56.810248	64.514138
1656.769578	66.741105	64.519143
1656.140086	57.331307	64.524148
1655.243407	60.972855	64.529153
1654.981368	62.754033	64.534158
1654.665377	59.197175	64.539162
1653.224494	58.908471	64.544167
1652.678317	57.565516	64.549172
1651.988731	62.410650	64.554177
1651.803692	58.336010	64.559182
1651.426648	50.429529	64.564186
1649.776834	64.034398	64.569191
1649.219180	54.881509	64.574196
1648.380245	65.921670	64.579201
1648.014915	61.371457	64.584206
1647.494247	55.224740	64.589210
1647.262613	61.545912	64.594215
1646.975378	57.395213	64.599220
1645.887936	65.175676	64.604225
1645.028907	66.761792	64.609230
1644.605334	56.074181	64.614234
1643.715678	60.512256	64.619239
1642.839660	55.488146	64.624244
1641.548278	54.297190	64.629249
1641.387421	55.057281	64.634254
1641.370039	57.845757	64.639258
1640.531816	55.012584	64.644263
1639.886198	50.159434	64.649268
1638.659341	59.727360	64.654273
1638.286826	48.918917	64.659278
1637.811184	51.567533	64.664282
1637.139320	54.898253	64.669287
1636.543654	53.899280	64.674292
1635.474394	62.426993	64.679297
1635.144506	53.511434	64.684302
1634.753026	52.295949	64.689306
1634.301187	58.653224	64.694311
1633.266343	53.965757	64.699316
1632.282973	64.068309	64.704321
1631.703734	57.193886	64.709326
1631.461016	57.632475	64.714330
1630.002545	58.729490	64.719335
1629.214167	61.745429	64.724340
1628.725336	66.351351	64.729345
1628.233264	63.585647	64.734350
1628.297966	61.281218	64.739354
1627.605620	72.464055	64.744359
1626.868424	59.847832	64.749364
1626.034874	64.739315	64.754369
1625.291568	59.975906	64.759374
1624.968667	66.237701	64.764378
1623.547175	67.343390	64.769383
1623.528108	62.849181	64.774388
1622.287712	67.518196	64.779393
1621.961429	67.963192	64.784398
1620.992624	59.501956	64.789402
1620.206875	67.138430	64.794407
1619.687932	58.214173	64.799412
1619.127195	60.899853	64.804417
1619.033925	69.544747	64.809422
1618.618447	64.703920	64.814426
1617.272853	67.426815	64.819431
1616.619257	65.431617	64.824436
1616.189486	66.012739	64.829441
1614.780383	67.396561	64.834446
1614.537292	65.524130	64.839450
1613.360394	64.818040	64.844455
1612.966682	58.288038	64.849460
1612.923253	60.587177	64.854465
1612.472007	60.348194	64.859470
1611.361347	58.908828	64.864474
1610.367049	61.261355	64.869479
1610.130167	59.828370	64.874484
1609.572388	58.883703	64.879489
1608.957683	64.725719	64.884494
1607.765425	61.813803	64.889498
1606.962915	67.416393	64.894503
1606.188038	60.507167	64.899508
1605.669483	66.407332	64.904513
1605.151090	66.286415	64.909518
1605.215394	61.118758	64.914522
1604.230400	66.917570	64.919527
1603.260495	53.234390	64.924532
1602.458044	66.332297	64.929537
1602.244086	68.054726	64.934542
1601.772574	59.273138	64.939546
1600.588424	71.151560	64.944551
1599.940252	66.745277	64.949556
1599.374924	73.750375	64.954561
1599.247594	57.036807	64.959566
1598.346353	64.773963	64.964570
1597.336072	73.148704	64.969575
1596.432503	61.238695	64.974580
1595.924962	62.408234	64.979585
1595.730106	61.418433	64.984590
1594.994399	55.869422	64.989594
1593.711973	64.034560	64.994599
1593.069876	62.456985	64.999604
1592.667961	64.180397	65.004609
1592.340110	55.405805	65.009614
1592.236105	52.683822	65.014618
1591.101709	63.517981	65.019623
1590.049851	55.528844	65.024628
1589.449851	65.143441	65.029633
1588.518767	60.544406	65.034638
1587.618476	56.760328	65.039642
1587.034317	62.059115	65.044647
1587.518235	50.086526	65.049652
1586.651912	60.931646	65.054657
1586.183781	60.640689	65.059662
1585.477136	54.277927	65.064666
1584.519682	61.246711	65.069671
1584.371661	60.346391	65.074676
1582.300489	59.562838	65.079681
1581.464529	65.804679	65.084686
1581.410679	60.516723	65.089690
1580.526613	71.283969	65.094695
1580.419614	68.058834	65.099700
1579.949624	64.751355	65.104705
1578.875854	65.074815	65.109710
1578.131322	55.891162	65.114714
1577.199411	62.771106	65.119719
1577.396452	55.977385	65.124724
1576.960154	60.223806	65.129729
1575.637967	64.595394	65.134734
1574.956821	56.680574	65.139738
1574.651884	66.676498	65.144743
1573.609558	55.758100	65.149748
1572.352245	62.349539	65.154753
1571.476195	61.320010	65.159758
1571.232421	62.446383	65.164762
1570.676224	66.553860	65.169767
1570.714301	60.574018	65.174772
1570.322029	59.250915	65.179777
1569.459352	69.681357	65.184782
1568.516087	67.029587	65.189786
1567.628956	70.375448	65.194791
1567.360592	57.390072	65.199796
1566.149124	64.845208	65.204801
1565.608074	58.182936	65.209806
1564.992211	58.488029	65.214810
1564.246987	63.283089	65.219815
1563.766585	53.801222	65.224820
1563.298785	65.758747	65.229825
1562.205246	63.706225	65.234830
1561.984537	58.017769	65.239834
1561.294884	62.502543	65.244839
1560.768108	53.663716	65.249844
1559.626671	54.676889	65.254849
1558.507920	58.950507	65.259854
1558.479187	52.976971	65.264858
1558.224618	60.227288	65.269863
1557.796331	55.816935	65.274868
1556.514438	51.063221	65.279873
1556.015041	57.528895	65.284878
1555.482859	51.389692	65.289882
1554.218052	57.607432	65.294887
1553.579366	55.473120	65.299892
1552.748792	61.201300	65.304897
1552.220648	57.481428	65.309902
1552.124027	58.529331	65.314906
1551.869526	59.409262	65.319911
1550.483331	51.019090	65.324916
1549.133612	57.429381	65.329921
1548.567789	64.873094	65.334926
1548.585430	61.922670	65.339930
1548.144084	64.004133	65.344935
1547.713454	52.799485	65.349940
1546.596884	61.107157	65.354945
1545.716383	64.341364	65.359950
1545.354677	55.134040	65.364954
1544.683917	69.920521	65.369959
1544.108749	66.665386	65.374964
1543.244000	65.194211	65.379969
1542.414925	63.128009	65.384974
1542.344159	57.135221	65.389978
1541.267854	60.177554	65.394983
1540.474018	57.799019	65.399988
1539.910102	61.362710	65.404993
1538.714678	59.884581	65.409998
1538.431359	58.376262	65.415002
1538.066051	62.785396	65.420007
1537.949049	56.157130	65.425012
1536.916861	62.642943	65.430017
1535.917672	60.573096	65.435022
1535.458802	54.764753	65.440026
1534.830388	62.990460	65.445031
1533.926700	53.908265	65.450036
1533.165245	62.081744	65.455041
1532.736714	71.759364	65.460046
1532.390064	48.522328	65.465050
1531.456374	63.614317	65.470055
1530.395688	56.878363	65.475060
1529.959050	59.383344	65.480065
1529.108019	62.324758	65.485070
1529.104948	62.484320	65.490074
1528.540082	68.954889	65.495079
1527.459567	56.770071	65.500084
1526.696258	70.034960	65.505089
1526.015211	62.911148	65.510094
1525.750252	51.786699	65.515098
1524.384663	68.100060	65.520103
1524.015153	60.725965	65.525108
1523.401485	56.542336	65.530113
1522.928737	63.611320	65.535118
1522.876562	58.799903	65.540122
1521.549622	72.352699	65.545127
1520.994813	59.642135	65.550132
1520.324283	61.188508	65.555137
1519.314578	61.297735	65.560142
1518.116017	53.648320	65.565146
1517.497581	61.867187	65.570151
1517.780748	62.989819	65.575156
1516.806268	57.599711	65.580161
1515.975739	60.096322	65.585166
1515.889819	56.649700	65.590170
1515.218626	65.487045	65.595175
1514.636214	56.640775	65.600180
1513.256772	59.976959	65.605185
1512.685756	60.625682	65.610190
1512.763833	50.967324	65.615194
1511.195079	53.195565	65.620199
1510.501309	54.221729	65.625204
1509.983856	57.331042	65.630209
1509.220274	53.593450	65.635214
1509.517380	52.373801	65.640218
1508.508849	60.453390	65.645223
1507.834682	60.129024	65.650228
1507.230137	52.157692	65.655233
1506.360928	60.087915	65.660238
1505.420906	49.933182	65.665242
1504.664578	58.107757	65.670247
1504.082405	67.019074	65.675252
1503.449472	60.397800	65.680257
1503.191148	57.167783	65.685262
1502.846338	59.273382	65.690266
1501.515531	60.066358	65.695271
1501.061620	57.494263	65.700276
1500.598966	57.914055	65.705281
1499.742935	57.683972	65.710286
1499.075836	48.547482	65.715290
1497.725203	59.767984	65.720295
1497.251455	58.205028	65.725300
1496.785853	53.283989	65.730305
1496.265184	53.966726	65.735310
1496.515745	56.072656	65.740314
1495.244671	63.815885	65.745319
1494.552910	55.943557	65.750324
1494.005787	53.938839	65.755329
1493.056507	55.676997	65.760334
1492.071561	45.328259	65.765338
1490.946096	57.296106	65.770343
1490.875252	54.623713	65.775348
1490.287786	61.395372	65.780353
1489.786822	57.391396	65.785358
1489.553747	61.456597	65.790362
1488.755304	63.176439	65.795367
1487.996643	58.546732	65.800372
1487.073594	57.994189	65.805377
1486.868630	58.947746	65.810382
1485.700876	57.115173	65.815386
1485.032211	55.212176	65.820391
1484.428387	57.011203	65.825396
1484.213232	62.197892	65.830401
1483.560383	61.955534	65.835406
1482.466339	60.094161	65.840410
1481.500132	57.854872	65.845415
1481.209599	57.034998	65.850420
1480.923251	55.961393	65.855425
1479.820529	59.955584	65.860430
1479.051778	57.950513	65.865434
1478.113851	55.664150	65.870439
1477.616423	58.000731	65.875444
1477.022595	55.148653	65.880449
1476.937014	56.887793	65.885454
1476.528625	55.317600	65.890458
1475.525243	57.907746	65.895463
1474.881511	52.579455	65.900468
1473.493905	53.767011	65.905473
1472.784758	52.348160	65.910478
1472.122569	48.334287	65.915482
1471.293083	52.927469	65.920487
1470.942610	53.640286	65.925492
1470.567088	52.795093	65.930497
1470.336387	54.522362	65.935502
1470.021943	50.424495	65.940506
1468.965996	58.179456	65.945511
1468.359818	54.743731	65.950516
1467.567034	59.867057	65.955521
1466.415317	51.553619	65.960526
1465.656901	43.178788	65.965530
1465.381173	55.409727	65.970535
1465.055954	49.878508	65.975540
1464.178527	54.786594	65.980545
1463.124028	50.567119	65.985550
1462.522740	45.929036	65.990554
1461.793700	52.280866	65.995559
1461.202765	48.099279	66.000564
1461.067214	51.132964	66.005569
1459.944297	54.943122	66.010574
1459.193988	49.514267	66.015578
1458.964300	58.214465	66.020583
1458.245623	44.863323	66.025588
1457.960821	45.426748	66.030593
1456.640361	55.249916	66.035598
1455.840844	52.016621	66.040602
1455.100194	58.222816	66.045607
1454.436299	50.234024	66.050612
1454.151958	48.217095	66.055617
1453.798296	63.004551	66.060622
1453.128500	44.613563	66.065626
1451.905078	53.698181	66.070631
1451.712914	42.618921	66.075636
1451.134453	48.583809	66.080641
1449.938361	52.150320	66.085646
1449.165900	40.092412	66.090650
1448.676047	46.600659	66.095655
1448.061031	48.782507	66.100660
1448.155704	52.837790	66.105665
1447.011840	51.478747	66.110670
1446.261449	47.092362	66.115674
1445.361310	52.672201	66.120679
1445.204833	48.073636	66.125684
1443.984203	50.444405	66.130689
1442.782821	51.201427	66.135694
1442.562294	52.818013	66.140698
1442.083030	61.316599	66.145703
1441.716940	55.083461	66.150708
1441.298170	49.572995	66.155713
1440.420881	56.032699	66.160718
1439.941773	47.677955	66.165722
1439.002583	56.744714	66.170727
1438.315144	57.293773	66.175732
1436.883230	51.917251	66.180737
1436.058960	65.087970	66.185742
1436.619172	45.205587	66.190746
1435.294084	54.643516	66.195751
1435.105631	46.943990	66.200756
1434.482772	48.851274	66.205761
1433.880966	54.045328	66.210766
1432.998954	46.553330	66.215770
1432.405627	49.608532	66.220775
1431.868655	49.244904	66.225780
1431.327651	46.228668	66.230785
1430.085163	47.594675	66.235790
1430.062396	50.566820	66.240794
1429.239810	55.480522	66.245799
1428.329969	52.986083	66.250804
1427.445941	58.639349	66.255809
1426.326403	64.098466	66.260814
1426.226500	47.272887	66.265818
1425.839003	52.067906	66.270823
1425.712236	47.274793	66.275828
1424.553627	50.413729	66.280833
1424.120983	53.572475	66.285838
1423.145051	45.424745	66.290842
1422.491651	56.089351	66.295847
1421.428274	48.587743	66.300852
1420.820736	56.850138	66.305857
1420.058218	57.813480	66.310862
1419.449352	60.844503	66.315866
1418.821329	65.520837	66.320871
1418.642341	52.033508	66.325876
1418.128707	55.749250	66.330881
1416.999263	58.050341	66.335886
1416.606399	58.455431	66.340890
1415.789532	50.925838	66.345895
1415.278512	54.457589	66.350900
1414.202827	53.657252	66.355905
1413.388011	55.405168	66.360910
1413.310445	51.410833	66.365914
1412.980315	54.462431	66.370919
1411.982956	52.354405	66.375924
1410.876138	48.883997	66.380929
1410.186277	48.817318	66.385934
1409.568660	48.248034	66.390938
1409.167330	44.673839	66.395943
1408.919427	49.587063	66.400948
1408.338093	49.348262	66.405953
1407.306880	46.978020	66.410958
1406.706515	49.532346	66.415962
1405.734909	61.677148	66.420967
1405.166034	43.746117	66.425972
1404.387330	53.462743	66.430977
1403.779596	55.130610	66.435982
1403.790068	51.641049	66.440986
1402.976358	46.447655	66.445991
1401.893103	51.566235	66.450996
1401.127084	53.241066	66.456001
1400.341885	58.620062	66.461006
1400.302842	51.946493	66.466010
1399.454340	57.027260	66.471015
1398.206597	57.996692	66.476020
1397.743530	53.703625	66.481025
1397.107357	56.717220	66.486030
1396.868305	49.162143	66.491034
1396.407409	58.190453	66.496039
1395.400495	51.055748	66.501044
1394.516198	44.518186	66.506049
1393.485720	53.158489	66.511054
1393.444989	55.470581	66.516058
1392.519221	50.234398	66.521063
1392.167381	47.334202	66.526068
1391.370152	54.290577	66.531073
1390.366494	63.681786	66.536078
1390.212630	46.350344	66.541082
1389.780590	51.631387	66.546087
1389.405780	48.344352	66.551092
1388.281479	48.265204	66.556097
1387.290920	58.777142	66.561102
1386.739538	40.186315	66.566106
1385.474960	49.966374	66.571111
1384.505740	51.412318	66.576116
1384.434999	50.402072	66.581121
1383.859460	49.016810	66.586126
1383.861871	52.232526	66.591130
1383.115822	51.455898	66.596135
1382.670224	50.592315	66.601140
1381.193101	46.957156	66.606145
1380.756305	53.323700	66.611150
1380.242204	40.395834	66.616154
1379.918783	53.354105	66.621159
1378.878228	53.820335	66.626164
1378.453393	51.614708	66.631169
1377.786785	52.886490	66.636174
1376.812438	54.273712	66.641178
1375.909443	57.008130	66.646183
1375.268743	59.468713	66.651188
1374.507323	52.297910	66.656193
1374.439137	51.235518	66.661198
1373.987710	47.010329	66.666202
1372.912930	59.378440	66.671207
1372.138816	55.335586	66.676212
1371.317228	48.078379	66.681217
1370.934741	55.835299	66.686222
1370.486101	52.161448	66.691226
1369.339322	48.652103	66.696231
1368.882221	45.821242	66.701236
1367.935147	41.300787	66.706241
1367.707893	52.544123	66.711246
1367.226896	49.572884	66.716250
1365.902955	49.176617	66.721255
1365.255409	50.989454	66.726260
1364.841880	49.211347	66.731265
1364.518668	51.826782	66.736270
1364.285749	50.537602	66.741274
1363.150697	56.632510	66.746279
1362.404919	58.699390	66.751284
1362.008503	51.339010	66.756289
1360.459639	51.816470	66.761294
1359.395559	45.932163	66.766298
1359.267009	51.169544	66.771303
1359.143563	56.319610	66.776308
1358.891992	57.337988	66.781313
1358.457015	53.987837	66.786318
1357.183193	53.841928	66.791322
1356.103782	55.704222	66.796327
1355.419083	49.591557	66.801332
1355.080926	53.774214	66.806337
1354.531878	54.449587	66.811342
1353.526587	49.855813	66.816346
1352.782751	56.382282	66.821351
1352.087073	50.966991	66.826356
1351.999931	49.450761	66.831361
1351.475984	57.514910	66.836366
1350.520295	49.665693	66.841370
1349.908835	51.327098	66.846375
1348.909147	46.351464	66.851380
1348.536559	51.484969	66.856385
1347.593675	57.014904	66.861390
1347.089960	55.145268	66.866394
1346.284942	55.954061	66.871399
1345.566837	52.505543	66.876404
1345.586370	51.501948	66.881409
1344.608198	52.124866	66.886414
1343.854161	40.537101	66.891418
1342.788023	53.954864	66.896423
1342.327781	50.073408	66.901428
1341.968897	53.202163	66.906433
1341.072809	58.438708	66.911438
1340.686290	49.525394	66.916442
1339.885133	49.649875	66.921447
1339.425392	44.496553	66.926452
1338.817047	57.631488	66.931457
1337.151756	53.175962	66.936462
1337.021614	47.676493	66.941466
1336.047041	56.533013	66.946471
1335.949666	49.392616	66.951476
1335.631299	58.904135	66.956481
1334.923836	58.495101	66.961486
1333.883576	51.801890	66.966490
1333.219528	59.061511	66.971495
1332.459443	56.931435	66.976500
1332.390084	54.946788	66.981505
1331.020324	58.742782	66.986510
1330.104932	48.472181	66.991514
1329.864195	51.833726	66.996519
1329.538172	50.288920	67.001524
1329.263747	57.538285	67.006529
1328.117102	65.350633	67.011534
1326.767717	51.172406	67.016538
1326.423624	56.219724	67.021543
1325.711181	53.164959	67.026548
1325.875848	56.358424	67.031553
1324.623249	60.199097	67.036558
1323.881861	49.882525	67.041562
1322.931508	51.350513	67.046567
1322.534563	59.383054	67.051572
1322.276446	49.360314	67.056577
1321.358031	50.028267	67.061582
1320.549366	55.284582	67.066586
1320.158857	61.437953	67.071591
1319.146508	54.192098	67.076596
1319.007758	51.529759	67.081601
1318.087890	56.924711	67.086606
1316.869458	52.964246	67.091610
1316.360580	57.609532	67.096615
1316.026473	50.400721	67.101620
1315.750347	56.182421	67.106625
1314.845864	55.475950	67.111630
1314.204293	53.367824	67.116634
1313.492563	56.847498	67.121639
1312.960431	52.794414	67.126644
1312.544827	50.790493	67.131649
1311.303234	55.843042	67.136654
1310.671899	55.346377	67.141658
1310.044195	60.526718	67.146663
1309.702803	58.523908	67.151668
1308.749386	56.054320	67.156673
1307.713790	52.726079	67.161678
1307.330550	45.528447	67.166682
1307.027385	54.021750	67.171687
1306.350883	46.416843	67.176692
1306.086247	49.675510	67.181697
1304.849251	61.763518	67.186702
1304.119809	55.591024	67.191706
1303.448444	55.486854	67.196711
1302.829361	53.489743	67.201716
1301.937315	50.532043	67.206721
1301.105496	62.805281	67.211726
1300.579463	55.676299	67.216730
1300.352631	52.589718	67.221735
1299.681790	56.430271	67.226740
1299.317908	52.920331	67.231745
1297.724236	56.854923	67.236750
1297.427199	59.818364	67.241754
1296.727453	59.193288	67.246759
1296.466314	58.806531	67.251764
1296.058489	54.370606	67.256769
1294.475052	57.159160	67.261774
1294.282841	38.995141	67.266778
1293.518277	54.744586	67.271783
1293.591484	52.527912	67.276788
1292.760136	50.492541	67.281793
1291.566528	56.424994	67.286798
1290.888703	50.287087	67.291802
1290.145190	55.921838	67.296807
1289.669889	55.278075	67.301812
1288.401112	48.999377	67.306817
1288.112023	60.934581	67.311822
1287.583929	53.315320	67.316826
1286.734076	56.271564	67.321831
1286.396527	52.909874	67.326836
1286.239567	48.638231	67.331841
1284.924482	57.309115	67.336846
1284.556362	54.134623	67.341850
1284.011299	55.423502	67.346855
1283.355169	57.190057	67.351860
1282.354896	54.964538	67.356865
1281.105718	54.699566	67.361870
1281.126443	55.731723	67.366874
1280.473465	49.511806	67.371879
1280.326033	52.023733	67.376884
1279.341166	44.044145	67.381889
1278.586389	57.862537	67.386894
1277.772976	47.329768	67.391898
1276.528419	62.875225	67.396903
1275.969636	61.054890	67.401908
1275.644406	52.304770	67.406913
1274.848429	64.893965	67.411918
1274.802297	57.695458	67.416922
1274.161929	63.375710	67.421927
1273.488086	58.077082	67.426932
1272.591457	51.372720	67.431937
1272.061665	61.296204	67.436942
1271.644457	54.666467	67.441946
1270.373201	60.359598	67.446951
1269.631303	59.298869	67.451956
1269.448229	56.265980	67.456961
1268.643163	70.629809	67.461966
1267.526527	55.807048	67.466970
1266.678186	60.667551	67.471975
1266.507508	63.516207	67.476980
1265.776410	50.771162	67.481985
1265.377069	59.192120	67.486990
1264.822667	54.758399	67.491994
1263.645787	62.457516	67.496999
1262.544591	64.290008	67.502004
1262.531392	58.368303	67.507009
1261.805018	64.540494	67.512014
1261.881570	57.053762	67.517018
1259.987516	61.432930	67.522023
1259.437624	53.294010	67.527028
1258.805944	63.714916	67.532033
1258.197620	63.509963	67.537038
1257.900613	57.290285	67.542042
1257.688723	54.667706	67.547047
1257.561160	55.591045	67.552052
1256.137006	50.634816	67.557057
1255.248235	54.352032	67.562062
1254.999115	51.006389	67.567066
1253.580245	55.897466	67.572071
1252.460264	61.446287	67.577076
1252.309479	43.790683	67.582081
1251.991307	56.043871	67.587086
1251.699962	51.764450	67.592090
1251.163460	49.666766	67.597095
1250.183652	54.786212	67.602100
1249.524278	56.410044	67.607105
1248.807418	50.543290	67.612110
1248.440899	47.634570	67.617114
1247.609830	60.187535	67.622119
1246.352892	59.521288	67.627124
1245.608537	50.496367	67.632129
1245.186196	62.985673	67.637134
1244.685299	59.104873	67.642138
1244.398544	58.855919	67.647143
1243.498862	54.594600	67.652148
1242.492766	52.632969	67.657153
1241.721743	64.000188	67.662158
1241.594546	53.398097	67.667162
1241.021392	52.891086	67.672167
1240.052793	58.446752	67.677172
1239.970080	48.788319	67.682177
1238.694605	56.934953	67.687182
1238.559632	54.006326	67.692186
1237.397984	52.751822	67.697191
1236.748962	64.484187	67.702196
1235.862486	54.465621	67.707201
1235.245732	62.673552	67.712206
1235.066042	51.581921	67.717210
1234.003875	61.469453	67.722215
1233.001710	50.324436	67.727220
1232.190168	55.570990	67.732225
1231.883547	56.221843	67.737230
1231.827920	51.211311	67.742234
1231.030716	51.755111	67.747239
1230.659557	60.123484	67.752244
1230.078570	59.926090	67.757249
1229.274585	52.290526	67.762254
1228.281269	43.703350	67.767258
1227.194748	54.870380	67.772263
1226.366894	51.812104	67.777268
1226.151803	49.984248	67.782273
1225.701647	53.120345	67.787278
1225.240845	47.473429	67.792282
1224.273893	43.725715	67.797287
1223.577547	48.413756	67.802292
1223.754593	57.544411	67.807297
1222.339610	51.872973	67.812302
1221.594065	54.678741	67.817306
1220.681877	54.540027	67.822311
1219.979997	55.015407	67.827316
1219.308820	53.240770	67.832321
1219.223371	60.766054	67.837326
1218.653604	61.321046	67.842330
1217.502992	59.946636	67.847335
1216.743558	48.388638	67.852340
1216.344910	54.912067	67.857345
1215.729139	63.060228	67.862350
1215.342430	42.951198	67.867354
1214.490585	53.789511	67.872359
1213.877481	61.332508	67.877364
1213.341276	50.690718	67.882369
1211.881608	62.012426	67.887374
1211.530152	51.551363	67.892378
1210.973279	45.508024	67.897383
1209.981708	57.044834	67.902388
1209.933865	45.611706	67.907393
1209.287691	57.972759	67.912398
1208.623410	46.736351	67.917402
1207.421965	53.906810	67.922407
1206.842635	52.277889	67.927412
1206.510961	50.962207	67.932417
1206.010396	49.321775	67.937422
1205.333425	49.550535	67.942426
1204.211374	53.040080	67.947431
1203.355201	53.140056	67.952436
1203.409099	56.380897	67.957441
1202.686510	56.125650	67.962446
1201.932505	52.198592	67.967450
1200.834284	52.748938	67.972455
1199.964300	53.239681	67.977460
1199.918490	49.977649	67.982465
1199.276095	51.184125	67.987470
1198.948694	55.388628	67.992474
1197.863052	61.616808	67.997479
1197.231346	55.991260	68.002484
1196.576401	52.121450	68.007489
1195.534320	59.566586	68.012494
1194.676037	58.531322	68.017498
1194.474183	48.716459	68.022503
1193.357672	50.685395	68.027508
1192.969334	51.459972	68.032513
1192.497204	59.394074	68.037518
1192.092699	55.321918	68.042522
1192.190207	48.067648	68.047527
1191.006078	53.188139	68.052532
1190.430127	43.900335	68.057537
1189.094778	52.513914	68.062542
1187.799417	47.071470	68.067546
1187.180979	44.007741	68.072551
1186.933603	57.793334	68.077556
1186.757325	47.975278	68.082561
1186.477324	54.722329	68.087566
1185.819246	60.091816	68.092570
1184.957604	55.065350	68.097575
1184.069717	64.458466	68.102580
1183.650121	53.251216	68.107585
1182.452330	61.339958	68.112590
1181.823214	55.337804	68.117594
1181.316577	58.807243	68.122599
1180.622952	60.306296	68.127604
1180.279753	52.865389	68.132609
1178.764617	59.696030	68.137614
1177.978874	56.003346	68.142618
1177.902392	59.522288	68.147623
1177.051571	65.282788	68.152628
1177.128960	55.047104	68.157633
1176.743460	60.682144	68.162638
1175.557125	57.851432	68.167642
1174.969892	55.614424	68.172647
1173.606310	59.417291	68.177652
1173.734185	48.700490	68.182657
1172.675015	58.294633	68.187662
1171.924005	53.162784	68.192666
1171.471290	58.846830	68.197671
1170.840110	52.523733	68.202676
1170.652274	50.529379	68.207681
1169.451287	65.647012	68.212686
1168.964644	60.235830	68.217690
1168.511617	54.916783	68.222695
1166.640615	63.179214	68.227700
1166.021350	53.216359	68.232705
1166.151365	60.971577	68.237710
1165.540589	55.681908	68.242714
1164.852025	53.271604	68.247719
1164.217233	56.525762	68.252724
1164.099797	47.907049	68.257729
1163.008854	53.977858	68.262734
1162.382203	43.174737	68.267738
1161.854782	57.422335	68.272743
1160.757745	57.714736	68.277748
1159.907134	57.192876	68.282753
1159.376435	52.114094	68.287758
1158.988913	51.076781	68.292762
1158.619206	56.539387	68.297767
1157.268224	63.682175	68.302772
1156.703101	48.185587	68.307777
1156.418919	59.362084	68.312782
1155.546991	46.637240	68.317786
1155.242872	53.444863	68.322791
1154.235902	59.674184	68.327796
1153.650226	53.005814	68.332801
1153.157925	59.658171	68.337806
1152.043922	55.108322	68.342810
1151.137524	50.918434	68.347815
1149.876371	60.510062	68.352820
1150.290669	54.616216	68.357825
1149.390283	54.991785	68.362830
1149.024482	47.391341	68.367834
1148.936821	49.125704	68.372839
1147.971709	59.648303	68.377844
1146.776244	49.820429	68.382849
1145.895141	55.863600	68.387854
1145.639950	45.503696	68.392858
1145.420589	51.863407	68.397863
1144.527083	51.078513	68.402868
1143.792279	53.406028	68.407873
1142.516273	55.072695	68.412878
1142.434791	61.312885	68.417882
1142.112611	57.437418	68.422887
1140.847335	60.717433	68.427892
1140.392485	63.184504	68.432897
1139.787879	64.433464	68.437902
1139.608885	65.694806	68.442906
1138.172494	52.232970	68.447911
1137.026055	56.751785	68.452916
1136.920596	45.971527	68.457921
1135.914769	58.682305	68.462926
1135.617361	58.754903	68.467930
1135.197116	52.330566	68.472935
1135.021555	57.584676	68.477940
1134.171799	49.261482	68.482945
1133.247631	52.063505	68.487950
1132.798087	55.506593	68.492954
1131.183637	53.941639	68.497959
1130.330427	59.985564	68.502964
1130.897195	51.726122	68.507969
1129.802770	59.424954	68.512974
1129.287355	51.470806	68.517978
1128.936531	55.974964	68.522983
1127.728515	53.991093	68.527988
1126.988891	53.891924	68.532993
1126.432164	55.798574	68.537998
1126.068450	56.592228	68.543002
1125.567638	52.235798	68.548007
1124.043311	54.804288	68.553012
1123.693757	54.174536	68.558017
1123.315014	51.758159	68.563022
1122.711382	53.511007	68.568026
1122.168597	54.743461	68.573031
1121.134917	48.854803	68.578036
1120.502295	43.048256	68.583041
1120.172266	53.824853	68.588046
1119.507234	49.664693	68.593050
1118.586560	57.439953	68.598055
1117.659356	57.670522	68.603060
1117.330671	51.550231	68.608065
1117.121925	48.605036	68.613070
1115.354343	50.614421	68.618074
1114.913445	44.893066	68.623079
1113.837307	52.428905	68.628084
1113.627517	44.221915	68.633089
1113.566501	48.844596	68.638094
1113.024319	41.950908	68.643098
1112.582344	46.088585	68.648103
1111.339396	47.800911	68.653108
1111.029021	43.689757	68.658113
1110.227657	54.844679	68.663118
1109.145226	52.860625	68.668122
1108.311159	48.952426	68.673127
1107.407776	58.173733	68.678132
1107.376528	49.927091	68.683137
1106.943402	56.673125	68.688142
1106.148378	49.023427	68.693146
1105.188770	52.757925	68.698151
1104.218591	58.497028	68.703156
1104.105705	50.338177	68.708161
1103.369161	55.911359	68.713166
1103.231162	54.579890	68.718170
1102.423122	52.413464	68.723175
1101.263869	57.834435	68.728180
1100.875931	49.235996	68.733185
1100.224918	53.878394	68.738190
1099.299071	59.929629	68.743194
1098.592872	45.903461	68.748199
1097.740141	48.915878	68.753204
1097.564901	51.803206	68.758209
1097.082401	56.200839	68.763214
1096.651712	48.253111	68.768218
1095.506124	49.140390	68.773223
1094.478941	50.640125	68.778228
1094.566178	45.457517	68.783233
1093.177450	51.693794	68.788238
1092.301327	50.182023	68.793242
1091.742551	57.489547	68.798247
1091.016975	56.915896	68.803252
1090.809198	46.868786	68.808257
1090.274952	58.752801	68.813262
1090.098784	46.177247	68.818266
1089.587479	53.077186	68.823271
1088.110329	55.728788	68.828276
1087.628096	54.040233	68.833281
1086.785027	56.268273	68.838286
1086.006870	50.389945	68.843290
1085.525912	51.732204	68.848295
1084.945784	53.194072	68.853300
1084.728207	54.500703	68.858305
1083.257349	54.244927	68.863310
1082.542864	50.010351	68.868314
1081.948141	51.885224	68.873319
1081.503540	55.401675	68.878324
1080.893265	52.324722	68.883329
1080.655183	57.476252	68.888334
1079.810377	56.303313	68.893338
1079.538052	51.986708	68.898343
1078.842503	57.835885	68.903348
1077.727141	56.725065	68.908353
1076.675587	51.756801	68.913358
1075.700607	49.250302	68.918362
1075.712879	45.407964	68.923367
1075.139622	51.893796	68.928372
1074.685593	41.684397	68.933377
1072.724438	54.349171	68.938382
1072.126991	39.573773	68.943386
1071.991616	36.316429	68.948391
1071.234406	53.016665	68.953396
1071.512543	45.705420	68.958401
1070.734528	53.568748	68.963406
1070.367770	48.548746	68.968410
1069.586895	43.431509	68.973415
1068.791191	51.120243	68.978420
1067.561415	48.154113	68.983425
1066.575442	45.217284	68.988430
1066.028944	52.290215	68.993434
1065.745986	50.500831	68.998439
1065.282084	51.701626	69.003444
1064.859071	42.350558	69.008449
1063.469053	50.401970	69.013454
1063.007577	47.009818	69.018458
1062.808180	45.422825	69.023463
1062.203284	49.356311	69.028468
1061.259054	44.240997	69.033473
1060.328870	48.102692	69.038478
1059.276731	54.285682	69.043482
1059.387167	48.526761	69.048487
1058.454671	53.085134	69.053492
1057.539599	43.939900	69.058497
1056.977654	48.838613	69.063502
1056.023799	48.359319	69.068506
1056.310773	52.878595	69.073511
1055.622649	50.915448	69.078516
1054.696891	54.315357	69.083521
1053.972940	52.834374	69.088526
1053.466329	58.374108	69.093530
1052.821786	55.443941	69.098535
1051.175266	53.890427	69.103540
1050.457976	49.143206	69.108545
1049.828072	49.665491	69.113550
1049.310878	44.192462	69.118554
1049.380387	54.237514	69.123559
1048.626426	57.415778	69.128564
1048.507988	49.588657	69.133569
1047.999065	53.258223	69.138574
1046.845154	49.098114	69.143578
1045.989891	39.761863	69.148583
1045.555985	55.080094	69.153588
1044.747993	43.123116	69.158593
1043.595078	45.460270	69.163598
1043.248997	49.108659	69.168602
1043.028444	47.429769	69.173607
1041.210734	49.199882	69.178612
1040.656857	44.690719	69.183617
1040.270836	48.973547	69.188622
1039.865485	45.533105	69.193626
1040.037486	51.232139	69.198631
1038.799278	56.948075	69.203636
1037.845398	51.497329	69.208641
1037.183261	55.292207	69.213646
1036.736859	52.924924	69.218650
1036.608903	53.409408	69.223655
1035.269995	47.500416	69.228660
1034.745014	48.652069	69.233665
1033.988490	45.981072	69.238670
1033.625878	43.974817	69.243674
1033.656224	40.532787	69.248679
1032.032815	48.730746	69.253684
1031.241947	45.152650	69.258689
1030.729949	43.526434	69.263694
1029.698231	47.460385	69.268698
1029.264468	48.886141	69.273703
1028.340719	50.253313	69.278708
1027.640996	48.950545	69.283713
1027.158161	54.661856	69.288718
1026.857836	51.733928	69.293722
1026.469583	46.716824	69.298727
1025.627217	56.164122	69.303732
1024.774970	57.473659	69.308737
1024.161976	57.840295	69.313742
1023.798867	54.927066	69.318746
1023.066589	50.543582	69.323751
1021.883123	55.163491	69.328756
1021.465190	49.384139	69.333761
1021.084482	50.672922	69.338766
1020.528083	55.676868	69.343770
1019.299002	52.035665	69.348775
1018.884137	54.343141	69.353780
1018.501103	50.948218	69.358785
1017.765796	52.152865	69.363790
1016.826972	50.275286	69.368794
1016.434142	43.286569	69.373799
1015.343370	47.663640	69.378804
1015.252754	48.778804	69.383809
1013.791199	43.136337	69.388814
1012.743281	46.634930	69.393818
1012.468710	44.750567	69.398823
1011.621499	48.832127	69.403828
1011.430601	43.877539	69.408833
1011.295503	53.115299	69.413838
1010.522365	58.611077	69.418842
1010.220192	46.444333	69.423847
1008.815128	58.036181	69.428852
1008.449041	50.580668	69.433857
1007.996743	52.784824	69.438862
1006.476342	52.394667	69.443866
1005.753274	54.539014	69.448871
1004.568833	58.230720	69.453876
1004.672741	52.207274	69.458881
1004.340117	56.235447	69.463886
1003.965628	58.061165	69.468890
1003.842606	52.231705	69.473895
1002.648432	55.066569	69.478900
1001.931810	49.479680	69.483905
1001.095777	51.840731	69.488910
999.912248	52.425071	69.493914
999.648879	46.239142	69.498919
998.403713	53.334625	69.503924
998.358960	47.061128	69.508929
997.643207	50.250616	69.513934
997.287277	52.244858	69.518938
996.656814	41.453484	69.523943
995.593811	48.873015	69.528948
995.016616	43.225938	69.533953
994.548508	47.208631	69.538958
994.219697	47.260564	69.543962
993.094731	45.669461	69.548967
991.992250	48.995438	69.553972
991.775038	45.932892	69.558977
991.462238	51.528641	69.563982
990.806381	43.247673	69.568986
989.663443	41.942266	69.573991
989.008376	43.909582	69.578996
988.690852	46.925877	69.584001
987.997043	45.753543	69.589006
986.603554	51.825272	69.594010
985.945401	39.238737	69.599015
985.494421	42.511164	69.604020
985.033704	45.157660	69.609025
984.734903	43.811500	69.614030
984.263417	51.422611	69.619034
983.398201	54.479023	69.624039
982.444655	51.504686	69.629044
981.984786	55.615043	69.634049
981.277112	55.680942	69.639054
980.230888	52.068432	69.644058
979.566197	51.357273	69.649063
978.867039	54.558132	69.654068
979.202236	50.602864	69.659073
978.558513	54.846939	69.664078
977.495790	55.883860	69.669082
976.569451	48.210107	69.674087
975.823364	55.056316	69.679092
975.026130	44.548494	69.684097
974.150578	54.798016	69.689102
973.337176	56.237875	69.694106
973.221610	56.296313	69.699111
972.359916	63.193902	69.704116
972.236118	56.561723	69.709121
972.051717	49.960450	69.714126
971.128215	50.591444	69.719130
970.509615	48.456544	69.724135
969.468122	59.268145	69.729140
968.427830	45.081746	69.734145
967.734040	54.465314	69.739150
967.224642	58.876640	69.744154
967.107822	54.801820	69.749159
965.558209	52.737161	69.754164
964.900287	51.915902	69.759169
964.120023	50.232221	69.764174
963.481549	48.292953	69.769178
963.478266	55.208913	69.774183
962.801932	65.710494	69.779188
962.351443	52.463159	69.784193
961.911807	48.942154	69.789198
960.801875	57.647428	69.794202
960.496335	51.276102	69.799207
959.134007	58.442184	69.804212
958.405877	46.482603	69.809217
957.611514	50.584723	69.814222
957.156500	49.930810	69.819226
956.723414	47.052073	69.824231
956.416837	61.424464	69.829236
956.216906	49.875316	69.834241
954.811030	53.511012	69.839246
953.708304	52.893427	69.844250
953.006200	46.218593	69.849255
952.832758	54.763480	69.854260
952.451257	50.951876	69.859265
951.592926	49.846011	69.864270
950.612197	57.799723	69.869274
950.504441	55.304587	69.874279
949.599488	60.203636	69.879284
948.347607	52.392626	69.884289
947.788134	57.883789	69.889294
947.024456	50.665317	69.894298
946.649672	48.045003	69.899303
946.129794	57.797848	69.904308
946.102131	52.541373	69.909313
945.608325	47.106985	69.914318
944.358825	53.765085	69.919322
944.066758	47.873405	69.924327
942.444453	45.071638	69.929332
941.590454	44.075554	69.934337
941.055688	47.504826	69.939342
940.458513	51.788692	69.944346
940.711175	50.491370	69.949351
939.844405	57.346410	69.954356
939.424915	45.684485	69.959361
938.554336	51.798898	69.964366
937.919302	52.111691	69.969370
937.377723	47.607148	69.974375
936.012401	60.700810	69.979380
935.072648	54.598361	69.984385
934.455818	53.269568	69.989390
934.057508	61.702189	69.994394
934.037125	47.110214	69.999399
933.308726	63.165291	70.004404
932.276098	52.256498	70.009409
931.270223	54.354163	70.014414
930.892068	53.028702	70.019418
931.178107	44.852468	70.024423
929.806727	53.913163	70.029428
928.895800	46.365857	70.034433
928.449834	49.984385	70.039438
927.294961	49.412052	70.044442
927.241120	40.355001	70.049447
926.340843	50.501001	70.054452
925.728784	44.082317	70.059457
925.045669	46.878217	70.064462
924.274930	54.288359	70.069466
924.217356	50.729159	70.074471
922.853115	57.103774	70.079476
922.199848	42.784796	70.084481
921.506885	53.599070	70.089486
921.114140	49.215479	70.094490
920.810801	38.164821	70.099495
919.696959	52.291797	70.104500
918.907033	47.191141	70.109505
918.598294	53.100783	70.114510
917.735693	48.728985	70.119514
917.401917	53.858614	70.124519
916.337192	55.739005	70.129524
915.534557	49.632815	70.134529
914.993002	58.314165	70.139534
914.300520	57.495281	70.144538
914.226718	54.862101	70.149543
912.902178	57.946274	70.154548
912.386404	54.623042	70.159553
911.823605	51.559299	70.164558
911.398841	54.025573	70.169562
910.987825	51.199110	70.174567
909.864453	53.696226	70.179572
909.090954	50.576996	70.184577
908.298893	53.531683	70.189582
908.074716	53.932787	70.194586
906.982721	50.771402	70.199591
905.934565	55.571831	70.204596
905.401297	52.465533	70.209601
905.330805	58.908685	70.214606
904.611149	55.773523	70.219610
904.411342	50.407201	70.224615
903.688885	55.786945	70.229620
902.556945	51.858364	70.234625
902.024653	49.220429	70.239630
901.010880	52.514652	70.244634
900.958208	57.394438	70.249639
899.609515	52.068582	70.254644
899.192934	48.137474	70.259649
898.412136	55.019633	70.264654
897.875095	51.384668	70.269658
897.819815	44.523277	70.274663
896.537415	60.001430	70.279668
895.758856	51.837805	70.284673
895.325866	47.912271	70.289678
894.764257	50.368038	70.294682
894.513713	45.915493	70.299687
893.104935	60.150227	70.304692
892.181058	64.458478	70.309697
892.281548	55.712077	70.314702
891.699260	59.897088	70.319706
891.017738	49.208818	70.324711
889.977064	57.943289	70.329716
889.509271	54.779202	70.334721
889.024913	44.119137	70.339726
887.843137	53.064079	70.344730
887.271983	47.322043	70.349735
886.154907	59.097074	70.354740
886.036977	47.690992	70.359745
885.689459	51.597777	70.364750
884.959291	61.692152	70.369754
884.292610	47.709802	70.374759
883.094259	52.279788	70.379764
882.781165	50.876087	70.384769
882.222431	56.601982	70.389774
881.378878	60.253483	70.394778
880.781353	52.811184	70.399783
880.073691	59.417544	70.404788
879.363298	55.278221	70.409793
879.203036	56.352028	70.414798
877.878049	54.548908	70.419802
877.130404	58.658431	70.424807
876.728509	61.204867	70.429812
876.688093	52.836664	70.434817
876.174782	55.437311	70.439822
874.605535	66.123409	70.444826
874.133629	50.742375	70.449831
873.098315	60.195104	70.454836
872.672417	55.103943	70.459841
872.465507	59.427545	70.464846
871.617382	60.980334	70.469850
870.757437	54.858706	70.474855
869.802414	52.776707	70.479860
869.467233	53.730087	70.484865
869.081022	55.071136	70.489870
868.648022	58.903753	70.494874
867.812581	55.993287	70.499879
866.891332	54.103256	70.504884
866.406558	52.536340	70.509889
865.982311	52.773567	70.514894
864.654297	62.866533	70.519898
864.255042	61.214314	70.524903
863.618690	66.658655	70.529908
863.365702	58.652107	70.534913
862.128368	54.903027	70.539918
861.365407	57.049883	70.544922
861.005715	58.955176	70.549927
860.659673	62.710535	70.554932
859.783126	56.637145	70.559937
858.822183	53.795544	70.564942
858.006031	61.158213	70.569946
857.732064	53.003690	70.574951
857.235944	60.377461	70.579956
856.679735	53.867119	70.584961
855.786338	56.133418	70.589966
854.953060	55.025648	70.594970
854.402702	42.638961	70.599975
853.819925	56.441311	70.604980
852.748979	49.892039	70.609985
851.867157	56.052992	70.614990
851.338764	60.209039	70.619994
850.905007	55.274745	70.624999
850.495467	57.101739	70.630004
850.344423	47.948059	70.635009
849.480561	53.629118	70.640014
848.321555	54.135087	70.645018
847.938347	54.857891	70.650023
847.348831	55.969304	70.655028
846.509505	53.383176	70.660033
845.486403	56.643484	70.665038
844.455566	49.022795	70.670042
844.754850	52.274480	70.675047
844.028073	58.286121	70.680052
843.072503	54.915473	70.685057
842.236877	47.960786	70.690062
841.555675	53.971724	70.695066
841.010403	43.436571	70.700071
840.545267	54.463653	70.705076
840.268127	55.824308	70.710081
839.323746	45.911302	70.715086
838.668506	59.590284	70.720090
838.349601	47.798656	70.725095
837.056351	55.574606	70.730100
836.074228	54.194325	70.735105
835.479709	53.291176	70.740110
834.924038	64.413505	70.745114
834.668196	56.931633	70.750119
834.139237	54.779030	70.755124
833.596627	56.657632	70.760129
832.701226	55.376570	70.765134
831.519695	53.326667	70.770138
831.484252	45.567457	70.775143
830.980483	55.950271	70.780148
830.017141	48.932598	70.785153
829.219825	41.872676	70.790158
828.326698	50.051379	70.795162
828.500631	48.246514	70.800167
827.205347	62.509974	70.805172
826.465562	55.270858	70.810177
826.051104	49.749874	70.815182
825.187118	63.600003	70.820186
824.869430	52.497340	70.825191
823.565219	54.098261	70.830196
822.778018	55.007497	70.835201
822.527477	58.024957	70.840206
821.868027	48.406157	70.845210
822.020521	54.296003	70.850215
821.011692	54.162076	70.855220
820.188738	46.748537	70.860225
819.584895	49.353249	70.865230
818.952219	52.523790	70.870234
817.848667	48.230390	70.875239
817.091320	53.260084	70.880244
816.609059	46.079884	70.885249
815.997110	46.019284	70.890254
815.330158	59.711719	70.895258
815.125681	41.140199	70.900263
814.045158	50.823293	70.905268
813.226879	51.660490	70.910273
812.830069	48.970545	70.915278
812.401148	54.791438	70.920282
811.895650	57.496536	70.925287
810.743950	54.382111	70.930292
809.987629	51.868215	70.935297
809.618632	51.777447	70.940302
808.841811	56.198274	70.945306
807.756346	50.336729	70.950311
806.936367	56.126324	70.955316
806.295388	51.754875	70.960321
806.002401	52.027646	70.965326
805.722014	55.493089	70.970330
805.674268	42.813094	70.975335
804.252222	48.197817	70.980340
803.548095	49.421230	70.985345
802.951834	50.356576	70.990350
802.533267	52.914158	70.995354
801.582129	50.082733	71.000359
800.584746	51.687152	71.005364
800.088139	49.497830	71.010369
799.917809	48.799115	71.015374
799.403917	57.196270	71.020378
798.732411	50.854103	71.025383
797.875172	47.680954	71.030388
796.296348	54.769289	71.035393
795.572452	59.125398	71.040398
794.817522	52.430436	71.045402
794.766778	48.965199	71.050407
793.936592	56.714334	71.055412
793.495552	53.456077	71.060417
793.018504	45.230965	71.065422
792.552357	62.561045	71.070426
792.664913	49.690569	71.075431
791.253178	57.547216	71.080436
790.547776	56.678066	71.085441
788.988033	52.649912	71.090446
788.215036	57.686633	71.095450
787.889975	49.490746	71.100455
787.319722	52.040367	71.105460
786.873746	50.653909	71.110465
786.803220	53.515803	71.115470
786.344263	48.635177	71.120474
785.749448	52.452491	71.125479
784.727764	50.308907	71.130484
783.930302	46.271357	71.135489
782.673243	51.687427	71.140494
781.948627	56.735596	71.145498
781.456503	50.970568	71.150503
780.977403	52.017287	71.155508
780.160424	59.882577	71.160513
780.609262	52.578804	71.165518
779.169742	52.325646	71.170522
778.195096	63.746705	71.175527
777.342461	62.755549	71.180532
776.911413	54.071790	71.185537
776.794546	55.487884	71.190542
775.468774	53.289424	71.195546
774.570639	47.101737	71.200551
774.125714	53.984394	71.205556
773.828894	40.680002	71.210561
773.234520	47.592204	71.215566
772.769277	61.136409	71.220570
772.118139	49.178689	71.225575
771.254502	55.733620	71.230580
770.539258	53.649646	71.235585
770.087610	57.703739	71.240590
768.785609	61.549045	71.245594
768.352533	52.511577	71.250599
767.744921	51.599233	71.255604
767.056015	56.037766	71.260609
766.793437	52.075557	71.265614
766.069433	56.857190	71.270618
764.992461	50.667377	71.275623
764.383894	57.092173	71.280628
764.016810	50.142895	71.285633
763.578246	50.725196	71.290638
762.510487	56.094240	71.295642
761.916197	47.092681	71.300647
761.723768	59.021945	71.305652
760.816739	47.272661	71.310657
759.600013	46.512422	71.315662
758.723277	56.840317	71.320666
758.593914	48.173171	71.325671
758.149442	50.730852	71.330676
757.416516	55.813603	71.335681
757.025164	48.180100	71.340686
755.782390	60.787424	71.345690
755.153256	53.706203	71.350695
754.801069	47.699326	71.355700
754.352688	47.426776	71.360705
753.262201	50.804821	71.365710
752.457646	59.337027	71.370714
751.839447	54.845638	71.375719
751.203260	54.933664	71.380724
750.914921	50.551945	71.385729
749.755250	41.855260	71.390734
749.117755	53.908521	71.395738
748.833639	46.432299	71.400743
748.149851	57.621172	71.405748
747.463706	54.530822	71.410753
746.331134	57.403343	71.415758
745.486271	56.288500	71.420762
745.246192	50.210315	71.425767
744.931178	54.898205	71.430772
744.896841	58.038883	71.435777
744.236995	46.725657	71.440782
743.003471	55.102807	71.445786
742.451618	40.283773	71.450791
741.164999	44.045924	71.455796
740.202373	52.764672	71.460801
739.693565	48.490982	71.465806
739.322758	53.291449	71.470810
739.290180	45.325321	71.475815
738.246387	44.917942	71.480820
737.204523	48.273055	71.485825
736.950697	41.732255	71.490830
736.022531	40.008035	71.495834
735.742975	48.893172	71.500839
734.682863	47.270892	71.505844
733.397848	52.868594	71.510849
733.039429	48.730186	71.515854
732.333301	59.201347	71.520858
732.223377	49.980246	71.525863
731.668831	46.208182	71.530868
731.170717	47.157904	71.535873
730.959680	37.152860	71.540878
729.764590	58.357203	71.545882
729.182865	43.269750	71.550887
728.183518	52.240696	71.555892
727.100908	43.363062	71.560897
726.530466	48.986369	71.565902
725.833486	53.755086	71.570906
725.865335	49.812703	71.575911
725.064034	49.983094	71.580916
724.533650	46.945010	71.585921
723.644961	45.892150	71.590926
722.732594	55.794332	71.595930
722.426387	48.645563	71.600935
721.718413	49.835306	71.605940
720.842468	47.665982	71.610945
719.968289	50.062817	71.615950
719.216278	53.504456	71.620954
719.142052	47.618509	71.625959
718.778690	45.224014	71.630964
717.494008	45.507214	71.635969
716.614114	46.537735	71.640974
716.178187	56.326720	71.645978
715.813605	41.799672	71.650983
715.477814	47.653161	71.655988
714.488496	46.771480	71.660993
713.282058	44.008285	71.665998
712.647050	53.694013	71.671002
712.669795	57.431589	71.676007
712.284025	53.148665	71.681012
711.375554	55.468093	71.686017
710.766073	48.516931	71.691022
709.887980	43.010660	71.696026
709.032734	46.793651	71.701031
708.040922	44.760226	71.706036
707.614327	48.480046	71.711041
707.214624	39.114397	71.716046
706.287040	49.527971	71.721050
705.840881	52.989053	71.726055
705.006246	54.033532	71.731060
704.163243	49.511985	71.736065
703.891392	49.933501	71.741070
703.186085	53.063210	71.746074
702.523101	43.525570	71.751079
701.354479	49.433319	71.756084
700.654372	45.984996	71.761089
700.256999	45.093089	71.766094
699.653563	49.140426	71.771098
699.698007	44.438823	71.776103
698.991946	46.082558	71.781108
698.094126	40.244952	71.786113
697.377593	49.403095	71.791118
696.450707	47.499857	71.796122
695.613693	42.728222	71.801127
694.835871	53.838471	71.806132
694.087700	51.460167	71.811137
693.465935	49.544918	71.816142
692.861618	51.103333	71.821146
692.743267	49.223808	71.826151
692.415599	55.617063	71.831156
691.884972	52.532447	71.836161
690.788842	40.842033	71.841166
690.385264	43.112463	71.846170
689.008833	56.503699	71.851175
688.302335	54.050366	71.856180
687.394855	50.550733	71.861185
687.112323	45.810021	71.866190
686.732402	55.017863	71.871194
686.271116	50.280537	71.876199
685.161842	53.010139	71.881204
684.276487	51.222150	71.886209
683.737771	45.399204	71.891214
683.118088	49.950614	71.896218
683.051000	36.167570	71.901223
682.664823	45.783034	71.906228
681.445716	42.526256	71.911233
680.739509	46.671328	71.916238
680.048044	55.977146	71.921242
679.151910	39.611016	71.926247
678.740838	42.665846	71.931252
677.665896	46.745412	71.936257
677.397518	43.974668	71.941262
676.732845	47.755013	71.946266
676.317364	43.832430	71.951271
675.113839	46.855665	71.956276
674.483036	45.552592	71.961281
674.310644	41.647966	71.966286
673.764048	48.050699	71.971290
672.470222	48.854133	71.976295
671.991264	47.316637	71.981300
670.852802	45.933178	71.986305
670.912563	41.485518	71.991310
670.067861	50.797456	71.996314
669.852614	39.165336	72.001319
668.768840	51.642796	72.006324
668.131367	45.366666	72.011329
667.433755	49.993399	72.016334
666.907740	49.600745	72.021338
666.254172	49.152974	72.026343
665.172386	49.487869	72.031348
664.467564	51.712812	72.036353
664.366167	45.796791	72.041358
663.472430	46.577864	72.046362
662.960162	43.137234	72.051367
662.175611	50.670939	72.056372
661.390543	43.800790	72.061377
660.918228	44.299282	72.066382
660.183073	48.622201	72.071386
659.359081	43.671115	72.076391
658.641401	39.852412	72.081396
658.474663	47.500126	72.086401
658.074483	44.734597	72.091406
656.863084	53.041657	72.096410
655.797107	49.122764	72.101415
655.134146	42.232881	72.106420
654.620401	51.033803	72.111425
654.567030	43.653451	72.116430
653.825520	50.893219	72.121434
653.222160	41.961132	72.126439
652.592460	52.848254	72.131444
651.860570	45.123121	72.136449
651.241884	41.017079	72.141454
649.717550	50.052715	72.146458
649.171988	48.573603	72.151463
648.646552	40.151165	72.156468
648.098416	40.808693	72.161473
647.607320	34.131331	72.166478
647.398963	45.456231	72.171482
646.838245	43.241600	72.176487
645.967569	37.346071	72.181492
645.200959	49.636174	72.186497
644.272668	45.934472	72.191502
643.013423	42.729974	72.196506
642.691774	46.329191	72.201511
642.176731	50.882413	72.206516
641.590946	48.737994	72.211521
641.875737	39.914259	72.216526
640.515627	45.617995	72.221530
639.834265	51.023483	72.226535
638.685343	40.726003	72.231540
638.523866	47.822977	72.236545
638.161618	39.973734	72.241550
636.723106	48.219053	72.246554
636.249815	38.561306	72.251559
635.637545	43.703915	72.256564
635.429469	49.642096	72.261569
634.463032	51.575962	72.266574
633.775102	44.866404	72.271578
633.354249	36.941551	72.276583
632.718638	38.406259	72.281588
631.605391	43.723511	72.286593
630.975206	39.788776	72.291598
630.041893	49.917563	72.296602
629.570723	50.013647	72.301607
629.424282	49.851212	72.306612
628.485727	47.362257	72.311617
628.119989	43.304455	72.316622
626.901846	54.183849	72.321626
626.395748	48.064813	72.326631
625.706303	46.109858	72.331636
625.183560	46.331219	72.336641
624.924939	42.961999	72.341646
623.446924	49.021055	72.346650
623.147477	45.794611	72.351655
622.544055	49.412897	72.356660
622.061673	48.606610	72.361665
621.786926	41.390500	72.366670
620.482001	45.762492	72.371674
620.168753	42.881815	72.376679
619.639327	42.646848	72.381684
618.138540	49.605019	72.386689
617.788061	49.219399	72.391694
616.542514	59.538261	72.396698
616.585746	49.410324	72.401703
616.246580	50.372691	72.406708
615.274895	54.470498	72.411713
614.606379	45.540108	72.416718
613.733266	50.809513	72.421722
613.445008	48.816216	72.426727
613.025154	47.889486	72.431732
611.908182	50.036638	72.436737
610.711446	48.657652	72.441742
610.145471	56.111285	72.446746
610.233995	50.401135	72.451751
610.052286	49.379527	72.456756
609.207207	55.038056	72.461761
608.616376	54.918210	72.466766
607.544112	51.001195	72.471770
606.918644	53.067689	72.476775
605.720135	54.506484	72.481780
605.163659	49.117623	72.486785
604.967187	53.596529	72.491790
603.995284	56.430104	72.496794
603.254132	49.383109	72.501799
602.636712	53.340093	72.506804
601.644243	58.427858	72.511809
601.434503	47.099520	72.516814
600.535007	51.139568	72.521818
600.245441	47.625659	72.526823
599.447228	46.948485	72.531828
598.280499	51.014979	72.536833
598.018429	37.905582	72.541838
597.555964	45.590935	72.546842
597.100529	43.671281	72.551847
596.218897	42.534742	72.556852
595.311700	52.177902	72.561857
595.388563	47.331809	72.566862
594.658396	49.649913	72.571866
593.056083	44.995215	72.576871
592.193075	51.104028	72.581876
591.826756	58.406619	72.586881
591.315741	49.284650	72.591886
591.159739	53.453482	72.596890
590.501901	48.169223	72.601895
589.413652	45.899730	72.606900
588.198553	49.435333	72.611905
588.396828	43.657042	72.616910
587.976541	55.367579	72.621914
586.559670	37.381986	72.626919
586.057134	40.987725	72.631924
585.269635	44.742152	72.636929
585.063431	44.075644	72.641934
584.333268	57.779694	72.646938
583.838322	42.662810	72.651943
583.138123	46.888569	72.656948
582.280972	53.355176	72.661953
581.918316	45.899145	72.666958
580.887238	49.803855	72.671962
580.201735	45.277060	72.676967
579.373272	45.578043	72.681972
578.435999	51.028172	72.686977
578.425913	38.037438	72.691982
577.647648	46.010572	72.696986
577.134951	44.963183	72.701991
576.160900	49.113897	72.706996
575.262139	50.066364	72.712001
575.163777	48.066979	72.717006
574.444980	50.957054	72.722010
574.091944	47.588226	72.727015
573.364901	43.055130	72.732020
572.708326	47.285651	72.737025
572.124327	41.980062	72.742030
570.263200	50.499902	72.747034
569.953713	43.021344	72.752039
569.483271	41.613052	72.757044
569.046085	48.465964	72.762049
568.833354	43.176099	72.767054
568.220917	53.983295	72.772058
567.064434	48.619883	72.777063
566.214883	42.725883	72.782068
565.392768	54.074635	72.787073
565.179776	40.671060	72.792078
563.997180	49.195817	72.797082
563.113305	54.679035	72.802087
563.060659	40.944450	72.807092
562.443635	51.502576	72.812097
562.038580	48.258314	72.817102
561.711194	49.765740	72.822106
560.903751	47.429983	72.827111
560.015028	44.216099	72.832116
559.099335	42.509515	72.837121
558.578836	47.903233	72.842126
557.674752	52.075909	72.847130
557.193395	43.799479	72.852135
557.121599	47.031827	72.857140
555.684286	44.412440	72.862145
554.844398	41.472016	72.867150
554.046247	47.115402	72.872154
553.632755	43.189337	72.877159
553.565495	45.335048	72.882164
552.561654	53.207505	72.887169
551.737389	45.415334	72.892174
550.596201	50.459116	72.897178
550.225990	47.802141	72.902183
549.777894	49.888378	72.907188
549.516159	50.924713	72.912193
549.063291	43.696897	72.917198
547.523430	46.820023	72.922202
547.105527	40.121451	72.927207
547.000530	47.878574	72.932212
546.363111	44.277047	72.937217
545.595189	39.201520	72.942222
544.569075	48.436004	72.947226
544.110179	49.075093	72.952231
543.338271	47.161517	72.957236
541.993672	52.196342	72.962241
541.681338	47.820731	72.967246
541.209035	42.921116	72.972250
540.780767	43.596403	72.977255
540.156113	37.236006	72.982260
539.449406	49.815831	72.987265
538.788518	50.168235	72.992270
537.973143	50.210418	72.997274
537.574306	44.860081	73.002279
536.979833	37.768633	73.007284
535.834706	39.607615	73.012289
535.139921	32.864129	73.017294
534.688101	44.668869	73.022298
534.405911	41.228306	73.027303
533.336038	44.733510	73.032308
532.398122	47.349310	73.037313
531.889892	37.163918	73.042318
531.417369	39.384200	73.047322
531.055990	39.148078	73.052327
530.066938	47.295485	73.057332
529.077875	41.170415	73.062337
528.574157	40.547390	73.067342
527.735225	50.491076	73.072346
527.428848	44.037460	73.077351
527.539690	40.595469	73.082356
526.071225	54.699167	73.087361
525.660704	37.535847	73.092366
524.939969	46.397891	73.097370
524.012287	53.011977	73.102375
522.869529	46.569841	73.107380
522.180461	49.715734	73.112385
521.834591	37.735780	73.117390
521.082263	43.248956	73.122394
520.820435	38.706810	73.127399
520.944503	42.045323	73.132404
519.982024	45.835268	73.137409
519.230361	39.268097	73.142414
518.087538	40.200030	73.147418
517.691072	45.300933	73.152423
516.187083	46.530397	73.157428
515.331595	47.112323	73.162433
515.819362	39.896613	73.167438
515.097579	50.245729	73.172442
514.647907	46.021543	73.177447
514.227471	41.513680	73.182452
512.386904	47.269775	73.187457
512.094538	46.130169	73.192462
511.677901	48.242989	73.197466
511.355105	42.777001	73.202471
510.006075	36.019318	73.207476
509.196945	46.879160	73.212481
508.663359	39.394805	73.217486
508.623429	47.701664	73.222490
507.907630	50.955949	73.227495
507.212768	44.497461	73.232500
506.064326	52.935854	73.237505
505.506890	43.376624	73.242510
505.421820	47.959590	73.247514
504.255839	45.405824	73.252519
503.412299	44.836691	73.257524
502.740087	52.432076	73.262529
502.354634	46.038588	73.267534
501.519041	52.074034	73.272538
501.292790	46.352700	73.277543
500.203124	41.122722	73.282548
499.047101	49.873844	73.287553
498.969238	36.635408	73.292558
498.660712	40.419868	73.297562
498.241831	40.840933	73.302567
497.377233	44.437277	73.307572
496.089099	42.986357	73.312577
495.878533	36.157141	73.317582
495.573749	53.071921	73.322586
494.111830	45.772695	73.327591
493.345260	46.701735	73.332596
492.561471	53.490498	73.337601
492.330361	37.482956	73.342606
492.007489	45.193334	73.347610
491.570527	45.088580	73.352615
490.473654	45.409917	73.357620
489.322985	48.552812	73.362625
488.817120	46.056845	73.367630
488.633067	47.570896	73.372634
488.065237	49.990268	73.377639
487.404763	45.027384	73.382644
486.345045	48.031543	73.387649
486.110181	41.097548	73.392654
485.341776	52.087777	73.397658
484.240369	48.898118	73.402663
483.680135	41.595560	73.407668
483.050156	52.284189	73.412673
482.868507	44.062199	73.417678
482.158076	55.562729	73.422682
480.885811	54.647090	73.427687
480.519426	41.275737	73.432692
479.724668	53.206744	73.437697
479.677537	42.881164	73.442702
478.412535	39.339038	73.447706
477.109739	46.342652	73.452711
476.584978	47.316305	73.457716
476.047320	45.831915	73.462721
476.174083	34.759347	73.467726
475.918252	43.717374	73.472730
475.093459	38.556087	73.477735
474.103599	44.866638	73.482740
473.575969	47.470953	73.487745
472.533188	41.640088	73.492750
471.510398	45.033819	73.497754
470.720439	43.169926	73.502759
470.451052	38.955115	73.507764
470.182787	48.778515	73.512769
469.814740	31.696748	73.517774
469.036832	42.097318	73.522778
467.413623	43.133687	73.527783
467.052124	48.737386	73.532788
466.279936	50.168681	73.537793
466.349954	34.656618	73.542798
465.703641	47.545021	73.547802
464.405863	44.355469	73.552807
463.934683	39.033725	73.557812
462.794969	43.826231	73.562817
462.763651	38.776064	73.567822
462.367162	40.084164	73.572826
461.675818	44.145795	73.577831
460.766970	36.857197	73.582836
460.097630	49.979666	73.587841
459.652269	42.487701	73.592846
458.667670	49.148255	73.597850
457.847703	46.432976	73.602855
457.263505	42.651039	73.607860
456.948985	45.190416	73.612865
456.358997	39.104341	73.617870
455.199868	53.798424	73.622874
454.352539	45.999573	73.627879
454.084594	47.024346	73.632884
453.434302	51.395504	73.637889
453.193349	46.850575	73.642894
452.092020	43.848007	73.647898
451.168506	48.901082	73.652903
450.766794	44.834861	73.657908
450.393869	49.818845	73.662913
449.619401	48.231363	73.667918
448.850386	44.007441	73.672922
448.152219	47.728026	73.677927
447.902279	36.740538	73.682932
447.136800	44.349932	73.687937
446.187328	41.886968	73.692942
445.251082	47.812964	73.697946
444.684073	43.900985	73.702951
444.216275	42.365945	73.707956
443.617185	48.530988	73.712961
443.011942	38.814977	73.717966
442.045023	45.480396	73.722970
441.399120	48.567588	73.727975
441.083053	45.145074	73.732980
440.073898	48.547528	73.737985
439.507455	42.037050	73.742990
438.611822	46.690239	73.747994
438.223090	48.690130	73.752999
437.981838	40.936624	73.758004
437.233951	46.201168	73.763009
436.472921	49.066524	73.768014
435.560959	53.276881	73.773018
434.938197	51.842604	73.778023
434.638640	49.110774	73.783028
433.614971	55.293716	73.788033
433.192822	52.069766	73.793038
432.341906	47.940798	73.798042
431.608529	51.966612	73.803047
431.067183	45.362234	73.808052
430.006704	48.909661	73.813057
429.316794	36.861193	73.818062
429.064557	39.991836	73.823066
428.461481	51.631457	73.828071
427.811022	38.097629	73.833076
426.141625	49.648029	73.838081
426.031116	40.974934	73.843086
425.173136	52.096562	73.848090
424.710553	46.431526	73.853095
424.596136	44.323195	73.858100
424.165559	45.393207	73.863105
423.561811	38.972411	73.868110
422.708669	51.291560	73.873114
421.978529	48.386826	73.878119
421.290275	41.745262	73.883124
419.761005	54.271068	73.888129
419.214478	43.852273	73.893134
418.814994	49.846540	73.898138
418.497622	40.436442	73.903143
418.633393	38.774287	73.908148
417.210553	51.258169	73.913153
416.250721	47.078796	73.918158
415.445633	45.879046	73.923162
414.845200	45.237479	73.928167
414.763426	35.258882	73.933172
414.053388	47.056954	73.938177
413.534328	44.653649	73.943182
412.545896	40.816265	73.948186
411.948395	52.441906	73.953191
411.617651	42.440845	73.958196
410.163843	52.167039	73.963201
409.519622	48.869446	73.968206
408.757363	46.393747	73.973210
408.151043	56.633483	73.978215
408.055130	48.176162	73.983220
407.384098	51.642248	73.988225
407.212322	40.623213	73.993230
406.383105	39.285504	73.998234
405.557795	44.394380	74.003239
404.659723	43.692908	74.008244
404.147285	47.351275	74.013249
403.453431	35.174420	74.018254
402.413743	46.158643	74.023258
401.077960	45.399956	74.028263
400.735698	39.399719	74.033268
400.054129	49.562352	74.038273
399.734076	40.734525	74.043278
399.672335	49.052219	74.048282
398.937946	49.841161	74.053287
398.953406	38.785304	74.058292
397.829567	51.462670	74.063297
397.114721	46.089541	74.068302
395.057558	52.652883	74.073306
394.320534	45.585891	74.078311
394.644370	44.669091	74.083316
394.078523	45.664399	74.088321
393.695706	40.938144	74.093326
393.145738	49.663175	74.098330
392.400008	53.711637	74.103335
391.520409	45.028253	74.108340
390.592953	59.423710	74.113345
389.920921	52.626614	74.118350
389.401151	49.160468	74.123354
388.034538	45.025160	74.128359
387.654713	46.059241	74.133364
386.896705	49.646018	74.138369
386.782973	46.377507	74.143374
386.186584	47.942096	74.148378
385.665397	44.714601	74.153383
385.398790	40.980478	74.158388
384.453136	44.795980	74.163393
383.937049	49.256638	74.168398
382.525526	45.337832	74.173402
381.617348	50.658667	74.178407
380.899048	44.038838	74.183412
380.620010	52.891508	74.188417
380.229140	48.534112	74.193422
379.849900	49.829394	74.198426
378.914101	48.869934	74.203431
378.181907	41.811198	74.208436
377.549672	50.866495	74.213441
377.073110	35.596927	74.218446
376.188500	42.647698	74.223450
375.130461	43.800382	74.228455
374.497450	44.257367	74.233460
373.721338	45.026622	74.238465
373.846954	42.489942	74.243470
373.415194	42.491276	74.248474
372.034365	43.392590	74.253479
371.955231	35.225282	74.258484
370.870582	47.203998	74.263489
370.631213	35.457258	74.268494
369.551577	40.335004	74.273498
368.202514	44.349507	74.278503
368.102932	38.438334	74.283508
367.658750	45.245477	74.288513
367.329063	34.896110	74.293518
366.435438	38.346270	74.298522
365.117776	46.338053	74.303527
364.774172	37.823726	74.308532
364.002071	36.753325	74.313537
363.763989	34.946834	74.318542
363.566354	44.720623	74.323546
362.190805	40.468442	74.328551
361.373298	40.166042	74.333556
361.057250	49.773034	74.338561
360.636338	46.224822	74.343566
359.870731	44.008244	74.348570
358.966603	44.815230	74.353575
358.753671	37.812366	74.358580
358.144682	41.922256	74.363585
356.860233	34.990938	74.368590
356.201919	47.406163	74.373594
355.594053	44.051826	74.378599
355.241370	37.447102	74.383604
354.210965	43.781986	74.388609
352.916174	43.255485	74.393614
352.527235	41.523004	74.398618
352.217179	48.974622	74.403623
352.126708	36.815545	74.408628
351.313810	43.402871	74.413633
350.817265	35.733395	74.418638
350.046984	42.911408	74.423642
348.960085	38.765278	74.428647
348.455845	45.813622	74.433652
347.632687	48.393602	74.438657
346.970205	40.537841	74.443662
345.821119	50.086302	74.448666
345.589371	40.486288	74.453671
345.204506	42.876288	74.458676
344.624909	48.578945	74.463681
344.418402	38.127946	74.468686
343.017905	44.303249	74.473690
342.179272	46.618661	74.478695
342.082316	38.196267	74.483700
341.478303	55.234154	74.488705
340.419179	39.895105	74.493710
339.520187	37.402989	74.498714
338.942178	46.505434	74.503719
339.256727	36.719037	74.508724
337.750022	51.597033	74.513729
337.005890	42.026815	74.518734
336.397453	46.699081	74.523738
335.472807	50.053913	74.528743
335.411335	48.205706	74.533748
334.499794	47.598525	74.538753
334.021138	42.742660	74.543758
333.225035	40.216333	74.548762
332.466405	32.746114	74.553767
332.394269	30.690540	74.558772
331.283939	41.995145	74.563777
330.449822	43.330895	74.568782
329.671272	42.473961	74.573786
329.233772	42.833103	74.578791
329.399189	39.311108	74.583796
327.904346	50.465714	74.588801
327.120662	43.123331	74.593806
326.622757	51.417887	74.598810
326.068609	41.278300	74.603815
325.749181	41.499976	74.608820
324.405930	41.069809	74.613825
323.945036	43.842293	74.618830
323.201824	41.632541	74.623834
322.686505	40.389065	74.628839
322.438852	32.952448	74.633844
320.942869	40.788890	74.638849
320.595862	30.825375	74.643854
319.708504	40.543304	74.648858
319.198349	39.353414	74.653863
319.016983	32.893009	74.658868
318.385747	35.139720	74.663873
317.293125	29.534144	74.668878
317.128670	40.615056	74.673882
316.288782	36.035044	74.678887
315.200757	35.839804	74.683892
314.237390	43.802053	74.688897
313.887801	38.412128	74.693902
313.495283	37.741649	74.698906
312.907882	43.393541	74.703911
312.644178	32.222924	74.708916
311.426856	31.425409	74.713921
311.057329	39.247193	74.718926
310.288803	38.094089	74.723930
308.900477	28.968621	74.728935
308.399679	30.012784	74.733940
307.281508	39.307671	74.738945
307.053317	39.319117	74.743950
306.966139	37.128761	74.748954
306.330264	39.891765	74.753959
306.040552	29.156636	74.758964
305.084745	38.254362	74.763969
304.328101	29.244035	74.768974
303.558691	40.063525	74.773978
302.769868	46.930529	74.778983
302.188429	38.631440	74.783988
301.165030	44.127549	74.788993
300.768146	40.971520	74.793998
300.285147	49.413906	74.799002
300.065901	48.239284	74.804007
299.134294	45.586197	74.809012
297.927504	47.582635	74.814017
297.462095	43.824966	74.819022
297.120735	44.147503	74.824026
296.400108	41.100250	74.829031
295.720298	35.411291	74.834036
294.278594	47.819482	74.839041
294.133296	47.070317	74.844046
294.030553	38.313808	74.849050
293.339064	45.681994	74.854055
292.424971	34.673774	74.859060
291.876186	40.156821	74.864065
291.064131	39.953361	74.869070
289.521618	28.217250	74.874074
289.099781	38.203922	74.879079
289.072126	39.045024	74.884084
288.265071	47.487298	74.889089
287.611407	38.646413	74.894094
287.587771	42.222190	74.899098
286.530404	40.762171	74.904103
285.561873	33.526087	74.909108
284.813828	38.727516	74.914113
284.252864	38.154987	74.919118
284.007739	30.502824	74.924122
282.980982	43.172632	74.929127
282.019503	35.710353	74.934132
281.393346	39.285593	74.939137
280.856574	36.244723	74.944142
280.418687	30.957960	74.949146
280.175666	33.440485	74.954151
279.401539	33.118428	74.959156
278.404018	34.578109	74.964161
277.744286	34.986399	74.969166
277.326013	31.434197	74.974170
276.304209	38.584672	74.979175
275.408610	29.848418	74.984180
274.820401	38.842879	74.989185
274.665980	42.156484	74.994190
274.130355	36.766480	74.999194
273.206572	44.605509	75.004199
272.336533	42.560391	75.009204
271.472618	35.253882	75.014209
270.976684	47.056309	75.019214
270.406756	45.537611	75.024218
270.242861	42.199158	75.029223
269.309689	37.988414	75.034228
268.407746	40.042336	75.039233
268.410789	41.212499	75.044238
267.429984	46.311732	75.049242
266.420854	40.921183	75.054247
266.049699	37.397218	75.059252
265.141381	48.012775	75.064257
264.606206	36.693313	75.069262
263.411392	38.230233	75.074266
262.677131	43.379964	75.079271
262.261213	40.646387	75.084276
261.537916	42.664953	75.089281
261.437138	39.141220	75.094286
261.124092	43.666549	75.099290
260.174636	39.020466	75.104295
259.236745	37.389984	75.109300
258.701233	42.326448	75.114305
258.359452	38.108675	75.119310
257.302993	39.069678	75.124314
255.992732	48.637094	75.129319
255.587174	40.494170	75.134324
254.986679	41.740154	75.139329
255.022118	40.017042	75.144334
254.455690	42.096346	75.149338
253.148461	43.091651	75.154343
252.799426	42.502929	75.159348
251.712960	50.648517	75.164353
251.843701	37.809339	75.169358
251.092906	47.875295	75.174362
249.876129	48.346311	75.179367
249.892538	42.418028	75.184372
248.736928	45.491561	75.189377
247.502795	41.972633	75.194382
247.174756	41.666086	75.199386
246.615219	42.483496	75.204391
246.565440	42.213326	75.209396
245.486642	45.053838	75.214401
244.626118	41.153127	75.219406
244.208172	44.282969	75.224410
243.395204	53.978295	75.229415
243.329626	41.400910	75.234420
242.323351	52.426396	75.239425
241.270177	45.831633	75.244430
240.795363	41.157087	75.249434
239.918440	40.166251	75.254439
238.748881	37.372004	75.259444
238.298919	41.562402	75.264449
237.907419	47.786210	75.269454
237.241270	49.168574	75.274458
236.528264	49.704022	75.279463
236.437003	49.585822	75.284468
235.714661	54.006849	75.289473
235.097428	57.463337	75.294478
234.313131	43.827772	75.299482
233.203625	47.605468	75.304487
233.002441	41.802900	75.309492
232.482936	40.890528	75.314497
231.382871	36.635379	75.319502
230.585035	37.284046	75.324506
230.049433	46.499218	75.329511
229.822335	39.072902	75.334516
229.098008	40.129338	75.339521
228.236635	38.439170	75.344526
227.350391	41.402590	75.349530
226.520630	44.107265	75.354535
226.446868	47.949775	75.359540
225.980677	43.904110	75.364545
225.075091	44.759921	75.369550
224.746440	51.859483	75.374554
223.928503	52.541991	75.379559
222.692062	50.221420	75.384564
221.724480	49.303360	75.389569
221.117039	47.619399	75.394574
220.683245	44.538780	75.399578
220.010118	56.754458	75.404583
219.538058	41.742693	75.409588
219.319278	44.986414	75.414593
218.904334	40.131488	75.419598
217.772980	39.316498	75.424602
216.988031	40.738570	75.429607
216.704246	36.806895	75.434612
215.264328	38.996462	75.439617
214.890822	39.200180	75.444622
214.365251	38.580148	75.449626
213.648671	49.803857	75.454631
213.480258	45.855955	75.459636
212.376955	51.340122	75.464641
211.719119	48.612890	75.469646
211.174745	47.313622	75.474650
210.269896	58.875907	75.479655
209.264202	44.614787	75.484660
208.446505	47.609879	75.489665
207.705618	49.038215	75.494670
207.761397	46.787831	75.499674
206.823645	49.063022	75.504679
206.891107	50.116753	75.509684
206.626687	45.089586	75.514689
205.530112	45.415674	75.519694
204.734437	42.488270	75.524698
203.493695	51.541310	75.529703
203.057985	39.565770	75.534708
201.864120	49.282575	75.539713
201.568703	51.308324	75.544718
200.870035	39.159190	75.549722
200.496953	47.264990	75.554727
200.281934	46.610670	75.559732
199.238688	46.684475	75.564737
198.570051	60.077999	75.569742
198.159614	54.080788	75.574746
197.319034	53.665931	75.579751
196.775169	51.183228	75.584756
195.687124	46.695513	75.589761
194.861622	48.785685	75.594766
194.709998	44.119687	75.599770
194.226556	50.627268	75.604775
193.152851	45.921978	75.609780
192.036761	48.849021	75.614785
191.494369	40.792325	75.619790
191.446363	41.547315	75.624794
190.751571	51.806165	75.629799
190.476157	33.171185	75.634804
189.246890	44.871569	75.639809
188.682069	43.876580	75.644814
188.178118	41.884770	75.649818
187.221129	45.248327	75.654823
186.531570	39.105957	75.659828
185.672386	39.388592	75.664833
185.310768	46.687212	75.669838
185.170334	41.752472	75.674842
183.641330	47.689332	75.679847
183.055807	41.536627	75.684852
182.014457	44.826230	75.689857
181.812638	45.527856	75.694862
181.787707	43.870353	75.699866
181.055899	53.198107	75.704871
180.103606	37.802128	75.709876
179.285435	52.142934	75.714881
178.789074	51.356855	75.719886
178.293621	45.669075	75.724890
177.106425	48.904739	75.729895
176.551075	40.031633	75.734900
176.026192	51.210246	75.739905
175.721550	45.796448	75.744910
174.851987	36.556050	75.749914
173.662038	38.227149	75.754919
173.295377	41.822254	75.759924
172.481001	36.673067	75.764929
172.095815	42.530683	75.769934
171.895225	45.716421	75.774938
170.850609	45.879277	75.779943
170.029994	43.950042	75.784948
169.285278	43.091284	75.789953
168.852855	45.184728	75.794958
168.475250	43.415194	75.799962
167.065772	49.942189	75.804967
166.419008	39.837858	75.809972
166.119595	48.167857	75.814977
165.371973	46.768840	75.819982
165.655748	41.143655	75.824986
164.336819	49.495280	75.829991
163.967049	45.646633	75.834996
162.800279	46.454473	75.840001
161.552860	47.961359	75.845006
161.164300	45.341124	75.850010
160.390776	45.708152	75.855015
160.490532	40.925253	75.860020
159.786816	42.288410	75.865025
158.906355	46.796546	75.870030
158.689367	43.110382	75.875034
157.294889	52.678046	75.880039
156.815787	42.507870	75.885044
156.404827	38.897984	75.890049
155.759367	47.236387	75.895054
154.857544	38.457417	75.900058
153.323252	40.787910	75.905063
153.355209	28.440919	75.910068
152.857839	41.798357	75.915073
152.404193	39.562285	75.920078
151.997192	41.670713	75.925082
151.030611	38.711439	75.930087
150.517717	33.924234	75.935092
150.005906	39.839870	75.940097
149.405882	41.403923	75.945102
148.362485	36.559251	75.950106
147.464943	43.633579	75.955111
147.359585	34.809648	75.960116
146.182799	41.185050	75.965121
145.463963	40.859853	75.970126
145.177134	38.995027	75.975130
144.411742	43.177535	75.980135
143.851843	49.853742	75.985140
142.739865	41.579325	75.990145
141.820953	36.035592	75.995150
141.239091	40.738050	76.000154
140.982701	44.855009	76.005159
140.759450	39.473841	76.010164
140.075428	38.046164	76.015169
139.328292	39.284933	76.020174
138.644543	44.184849	76.025178
137.667601	32.191989	76.030183
137.000435	32.010294	76.035188
136.054805	41.029325	76.040193
135.490308	39.966398	76.045198
135.160093	38.628848	76.050202
134.534954	38.734798	76.055207
134.316365	43.451555	76.060212
132.761903	43.440524	76.065217
132.043109	42.175905	76.070222
131.660653	33.772484	76.075226
131.047519	37.185646	76.080231
130.897889	34.712338	76.085236
130.139596	35.767507	76.090241
129.111590	37.751096	76.095246
128.486858	41.761869	76.100250
127.708833	47.566447	76.105255
127.702116	34.672302	76.110260
126.490975	40.733881	76.115265
125.889794	40.807306	76.120270
125.179221	34.502774	76.125274
124.115931	43.031616	76.130279
123.205001	33.878453	76.135284
122.610663	41.230782	76.140289
122.474548	41.850098	76.145294
121.663928	46.119306	76.150298
121.005003	38.832952	76.155303
121.158382	35.145269	76.160308
120.273628	30.265909	76.165313
119.506962	37.027293	76.170318
118.608583	37.419680	76.175322
117.727560	41.331900	76.180327
117.873822	36.082770	76.185332
116.860284	45.262649	76.190337
115.677417	43.536047	76.195342
115.428828	31.882905	76.200346
114.721503	46.042081	76.205351
113.821635	33.023972	76.210356
113.198184	37.258723	76.215361
112.765206	39.603303	76.220366
112.305096	32.256029	76.225370
110.881223	42.854197	76.230375
110.432358	30.335447	76.235380
109.674209	42.686474	76.240385
108.772810	40.359811	76.245390
108.879894	36.770059	76.250394
108.228904	44.138024	76.255399
107.769527	42.268048	76.260404
106.584934	37.482328	76.265409
105.803228	42.443247	76.270414
105.700945	31.885218	76.275418
105.252531	41.940783	76.280423
104.110540	29.840451	76.285428
103.318354	41.081461	76.290433
102.779255	42.402194	76.295438
102.146984	45.958370	76.300442
100.970680	44.536154	76.305447
100.521678	35.309724	76.310452
99.839861	42.480486	76.315457
99.240339	44.667710	76.320462
98.964137	37.391532	76.325466
98.501034	41.526562	76.330471
97.331027	46.303412	76.335476
96.647362	51.485144	76.340481
96.282160	41.737533	76.345486
96.006073	42.147571	76.350490
94.496070	46.282097	76.355495
93.845617	39.937265	76.360500
93.163341	46.078697	76.365505
92.863524	45.916524	76.370510
92.533486	41.388485	76.375514
91.385310	47.121140	76.380519
90.690382	38.957599	76.385524
90.284244	41.741236	76.390529
89.746267	41.101636	76.395534
89.272684	31.507606	76.400538
87.560741	45.588770	76.405543
87.112830	38.126913	76.410548
86.478959	40.509884	76.415553
86.083346	36.974740	76.420558
86.320463	39.678092	76.425562
85.262628	47.191991	76.430567
84.642947	35.615893	76.435572
83.962884	38.941462	76.440577
82.524535	41.059751	76.445582
81.595097	40.093344	76.450586
80.561483	49.727433	76.455591
80.975852	45.989081	76.460596
80.423263	45.421457	76.465601
79.555717	42.505612	76.470606
79.256550	42.995787	76.475610
78.444539	42.947874	76.480615
77.762705	38.257930	76.485620
76.797267	53.260658	76.490625
76.349315	50.550751	76.495630
75.989575	37.560830	76.500634
75.067883	46.060273	76.505639
73.873995	44.960796	76.510644
73.528932	43.547643	76.515649
72.962944	44.891936	76.520654
72.464990	36.565559	76.525658
72.002887	48.745053	76.530663
71.418214	45.883730	76.535668
70.586599	47.235672	76.540673
69.598993	41.732942	76.545678
68.731729	38.312609	76.550682
68.027184	44.219455	76.555687
67.640663	37.706228	76.560692
66.765661	37.534126	76.565697
66.327880	40.762109	76.570702
66.140107	42.815194	76.575706
65.311251	44.511642	76.580711
64.387171	43.737334	76.585716
63.498593	38.043561	76.590721
63.002245	39.182506	76.595726
62.563904	33.660210	76.600730
61.218227	46.872978	76.605735
61.296718	40.742627	76.610740
60.418024	40.924426	76.615745
59.636136	40.227971	76.620750
59.720419	35.252347	76.625754
58.661012	40.747958	76.630759
58.076926	42.192455	76.635764
57.406372	38.957463	76.640769
56.511069	42.546504	76.645774
55.493523	33.668204	76.650778
54.677556	43.147747	76.655783
54.577704	35.683456	76.660788
53.893306	41.429357	76.665793
53.553441	45.337616	76.670798
52.524509	36.113920	76.675802
51.122899	45.602302	76.680807
50.876121	46.248092	76.685812
50.622147	40.656688	76.690817
50.283513	38.703654	76.695822
49.990044	34.482359	76.700826
48.538696	42.947885	76.705831
47.785898	34.941111	76.710836
47.356804	37.253452	76.715841
46.896042	41.412950	76.720846
46.375992	37.205242	76.725850
45.356771	41.048411	76.730855
44.922486	35.375826	76.735860
43.767816	48.220738	76.740865
42.716510	41.909119	76.745870
42.435426	43.771374	76.750874
41.972820	51.865684	76.755879
41.288836	42.163266	76.760884
40.996896	39.492139	76.765889
39.858084	34.275855	76.770894
39.234713	43.598044	76.775898
38.608208	45.176519	76.780903
38.075434	37.698829	76.785908
37.503179	39.103012	76.790913
36.269624	43.716701	76.795918
35.614823	34.362159	76.800922
35.070183	39.109949	76.805927
34.492497	35.623792	76.810932
34.362994	41.066936	76.815937
33.962037	45.169212	76.820942
33.229777	44.907119	76.825946
32.121952	40.712958	76.830951
31.498288	44.113727	76.835956
30.305916	41.654614	76.840961
29.680928	48.193178	76.845966
29.203172	33.161529	76.850970
28.823893	40.316736	76.855975
28.548682	36.357955	76.860980
27.454294	47.890772	76.865985
26.268053	48.998807	76.870990
25.718593	43.475830	76.875994
25.274290	40.243891	76.880999
25.198479	35.624119	76.886004
24.976244	39.664173	76.891009
23.795884	39.897702	76.896014
23.252909	32.568994	76.901018
21.843432	37.035227	76.906023
20.867690	40.409132	76.911028
20.132844	41.425957	76.916033
19.618056	32.090832	76.921038
19.468289	34.939061	76.926042
18.721609	43.162595	76.931047
18.893972	39.567177	76.936052
18.207968	44.916278	76.941057
16.799104	39.226861	76.946062
16.645668	33.382187	76.951066
15.856560	40.240581	76.956071
14.694173	41.366238	76.961076
14.075431	42.368289	76.966081
13.560684	41.006734	76.971086
13.023549	39.775327	76.976090
12.314437	41.091669	76.981095
11.165376	36.475929	76.986100
10.404088	42.062134	76.991105
9.569850	34.379183	76.996110
9.531816	43.644429	77.001114
8.998229	45.544059	77.006119
8.674808	37.161718	77.011124
8.188268	40.973555	77.016129
7.250661	47.384944	77.021134
6.843188	40.795192	77.026139
5.165913	49.383542	77.031143
4.308146	43.435830	77.036148
3.848828	42.216342	77.041153
3.216995	47.578261	77.046158