Tue Jun 08 18:10:40 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.698578	92.765213	0.000000
0.259708	91.239099	0.005005
-0.168276	43.745248	0.010010
-2.702564	11.350811	0.015014
-7.271153	4.271497	0.020019
-12.212164	-2.160175	0.025024
-17.194358	-4.439130	0.030029
-21.496352	-1.322179	0.035034
-25.685091	2.050864	0.040038
-29.839855	5.991601	0.045043
-33.150549	-4.077399	0.050048
-36.745590	3.110964	0.055053
-40.010096	-9.796813	0.060058
-43.713764	-8.519955	0.065062
-47.716346	1.066299	0.070067
-51.255762	-2.704142	0.075072
-55.285028	4.503038	0.080077
-59.211546	-0.511855	0.085082
-62.804351	10.515892	0.090086
-66.506978	1.510768	0.095091
-69.932405	4.468769	0.100096
-74.122565	5.373579	0.105101
-77.917026	3.467693	0.110106
-81.732610	5.193219	0.115110
-85.532430	5.416144	0.120115
-88.942795	1.337043	0.125120
-93.254329	9.774818	0.130125
-96.577686	1.212676	0.135130
-100.331086	-2.442089	0.140134
-104.082613	-8.010331	0.145139
-107.906407	-0.169707	0.150144
-111.625076	6.840582	0.155149
-115.461644	6.756828	0.160154
-119.561199	11.485887	0.165158
-123.176020	4.635086	0.170163
-126.658093	-3.632196	0.175168
-130.232633	-2.140191	0.180173
-134.348454	-7.124522	0.185178
-138.278817	-9.815414	0.190182
-141.824964	5.521326	0.195187
-145.873222	0.702642	0.200192
-149.954047	8.881836	0.205197
-153.762148	5.375434	0.210202
-157.072617	3.388588	0.215206
-161.029945	11.456224	0.220211
-164.252581	2.547281	0.225216
-168.123052	12.407011	0.230221
-171.514875	5.284339	0.235226
-175.515036	-0.616572	0.240230
-179.527835	12.933645	0.245235
-183.240186	3.919242	0.250240
-187.300928	2.217792	0.255245
-191.172522	0.327206	0.260250
-194.518765	0.037856	0.265254
-198.382030	-2.544894	0.270259
-201.814523	-1.535848	0.275264
-206.100596	-2.902997	0.280269
-209.625573	2.318079	0.285274
-213.307443	-5.813420	0.290278
-217.470932	1.900825	0.295283
-220.918647	-5.121826	0.300288
-224.541024	7.998326	0.305293
-228.323420	-3.624893	0.310298
-232.007329	2.822192	0.315302
-236.065518	9.724634	0.320307
-239.379986	0.853607	0.325312
-243.336896	7.328975	0.330317
-247.596051	1.944626	0.335322
-250.864498	-2.737330	0.340326
-254.878805	1.534751	0.345331
-258.551263	3.494804	0.350336
-262.330513	5.839862	0.355341
-265.964147	-3.759501	0.360346
-269.777900	3.932695	0.365350
-273.677045	5.994005	0.370355
-277.071868	-3.000564	0.375360
-281.528029	-3.351296	0.380365
-284.735547	0.905971	0.385370
-288.293654	5.528487	0.390374
-292.449323	2.401541	0.395379
-296.299706	2.046777	0.400384
-300.212221	3.538864	0.405389
-303.497157	1.223298	0.410394
-307.236506	-4.850108	0.415398
-311.417207	5.868936	0.420403
-314.512701	2.892900	0.425408
-319.051251	7.983200	0.430413
-322.634677	1.850693	0.435418
-326.389407	-1.065539	0.440422
-330.116156	5.548826	0.445427
-333.478769	1.896700	0.450432
-337.435119	4.113525	0.455437
-341.368382	0.425881	0.460442
-344.804334	3.040911	0.465446
-348.921663	8.018725	0.470451
-352.198940	-3.836668	0.475456
-356.337814	2.085833	0.480461
-360.009823	-1.313474	0.485466
-363.749481	4.875660	0.490470
-368.233117	7.394134	0.495475
-371.474645	-5.632161	0.500480
-375.337590	2.329851	0.505485
-378.794707	-0.625154	0.510490
-382.445101	10.310064	0.515494
-386.091036	15.567810	0.520499
-390.107038	1.824179	0.525504
-394.389372	-1.389483	0.530509
-397.935485	0.359546	0.535514
-400.856778	-1.599936	0.540518
-404.973897	4.157439	0.545523
-409.101189	-3.923520	0.550528
-413.138197	8.915019	0.555533
-416.630394	4.030802	0.560538
-420.405151	-1.822890	0.565542
-423.906987	4.608893	0.570547
-427.549588	-3.421788	0.575552
-431.106894	5.790770	0.580557
-435.281511	-5.993493	0.585562
-438.804153	-1.125127	0.590566
-442.949865	-0.177869	0.595571
-446.680168	-2.519148	0.600576
-450.640823	2.708959	0.605581
-454.539318	4.639269	0.610586
-457.855109	5.673090	0.615590
-462.028266	2.582858	0.620595
-465.254633	-4.492560	0.625600
-469.131748	8.684090	0.630605
-473.204625	-0.558297	0.635610
-476.576649	-0.666576	0.640614
-480.835864	13.922389	0.645619
-484.190239	-0.237396	0.650624
-487.930449	2.309950	0.655629
-492.143137	-1.092788	0.660634
-495.068297	4.630675	0.665638
-499.461513	10.533393	0.670643
-503.027690	4.810160	0.675648
-506.677115	-0.198967	0.680653
-510.478554	2.924521	0.685658
-514.023537	1.854043	0.690662
-518.405299	1.688138	0.695667
-521.577006	-3.209137	0.700672
-525.331988	6.685120	0.705677
-529.298454	7.220809	0.710682
-533.234561	-2.012616	0.715686
-537.066027	11.105335	0.720691
-540.501679	-0.204075	0.725696
-544.437316	11.962747	0.730701
-548.410337	6.185816	0.735706
-551.789606	6.556830	0.740710
-556.167353	19.997862	0.745715
-559.699082	12.115232	0.750720
-563.153917	17.160337	0.755725
-566.786704	8.074616	0.760730
-570.536934	13.888387	0.765734
-574.758962	6.372098	0.770739
-578.283563	4.564411	0.775744
-582.022589	9.756180	0.780749
-585.892238	12.484097	0.785754
-589.546528	10.224627	0.790758
-593.460882	17.098348	0.795763
-596.650562	10.608403	0.800768
-600.791400	15.151557	0.805773
-604.593387	8.912730	0.810778
-608.608316	5.579190	0.815782
-612.412032	8.612766	0.820787
-616.209367	-1.402625	0.825792
-619.839649	13.949255	0.830797
-623.287116	10.977793	0.835802
-626.907529	-3.076211	0.840806
-631.173209	6.305015	0.845811
-635.123661	1.037813	0.850816
-638.761618	10.124238	0.855821
-642.194071	9.249669	0.860826
-645.467615	-0.263911	0.865830
-649.488971	7.302376	0.870835
-653.373067	-0.512591	0.875840
-657.384915	4.742633	0.880845
-661.245150	7.324929	0.885850
-664.942751	-5.331152	0.890854
-668.895270	11.929211	0.895859
-671.845832	-0.480489	0.900864
-675.950996	3.556512	0.905869
-679.687970	5.738752	0.910874
-683.114556	0.116450	0.915878
-687.610132	7.088017	0.920883
-691.081811	-0.480344	0.925888
-694.814477	3.982185	0.930893
-698.903895	7.347081	0.935898
-702.561984	6.595751	0.940902
-706.240320	11.120410	0.945907
-709.634109	-1.577113	0.950912
-713.555316	7.160111	0.955917
-717.725428	4.279988	0.960922
-721.079012	-1.668997	0.965926
-724.902133	1.453259	0.970931
-728.753073	-3.862901	0.975936
-732.648409	2.081286	0.980941
-736.881525	2.559118	0.985946
-740.070734	4.915404	0.990950
-743.792014	4.306787	0.995955
-747.620224	-8.632692	1.000960
-751.063248	1.277658	1.005965
-754.958482	2.750992	1.010970
-758.708597	3.914049	1.015974
-762.438283	12.206764	1.020979
-766.153037	-0.405623	1.025984
-770.070808	6.088327	1.030989
-774.059762	11.505896	1.035994
-777.816806	8.829652	1.040998
-781.535888	8.397124	1.046003
-785.254229	1.865845	1.051008
-789.230800	2.144575	1.056013
-792.906343	8.834189	1.061018
-796.317067	9.483138	1.066022
-800.216760	12.296127	1.071027
-803.877090	3.317192	1.076032
-807.780674	4.960546	1.081037
-811.313927	3.923033	1.086042
-815.221263	8.328018	1.091046
-819.204974	11.263199	1.096051
-822.812244	-0.323578	1.101056
-826.512249	2.785921	1.106061
-830.721179	14.858569	1.111066
-833.979965	7.716385	1.116070
-837.504401	10.102258	1.121075
-841.105606	4.274027	1.126080
-845.033179	7.565094	1.131085
-849.301053	7.650742	1.136090
-852.913120	2.410528	1.141094
-856.574255	7.245751	1.146099
-860.147639	4.196634	1.151104
-864.138316	7.204097	1.156109
-868.211838	13.166357	1.161114
-871.901550	2.846972	1.166118
-875.358131	6.585729	1.171123
-879.394384	-2.390174	1.176128
-882.852628	6.334419	1.181133
-886.584641	3.236377	1.186138
-889.939142	7.017223	1.191142
-894.310052	11.996816	1.196147
-898.259114	4.500717	1.201152
-902.165189	8.174957	1.206157
-905.762105	4.346424	1.211162
-909.627518	-2.018185	1.216166
-913.318452	3.338869	1.221171
-916.817771	0.488651	1.226176
-920.382697	4.752055	1.231181
-923.768987	0.379395	1.236186
-927.998042	1.745596	1.241190
-932.139518	10.130446	1.246195
-935.739650	1.965452	1.251200
-939.441056	-1.099115	1.256205
-943.490141	-1.966259	1.261210
-946.669388	-1.699141	1.266214
-950.361528	14.379577	1.271219
-954.023685	12.230713	1.276224
-958.173450	-2.792663	1.281229
-962.059418	6.001865	1.286234
-965.837049	-3.636064	1.291238
-969.705803	-2.176164	1.296243
-973.417428	1.201089	1.301248
-976.990956	3.777459	1.306253
-980.683098	9.415018	1.311258
-983.838083	-0.515699	1.316262
-988.397651	1.995116	1.321267
-991.945552	1.906381	1.326272
-995.883675	-0.481228	1.331277
-1000.012406	8.680644	1.336282
-1003.066929	1.235530	1.341286
-1007.140866	-4.519673	1.346291
-1011.132804	-2.204178	1.351296
-1014.637626	6.099855	1.356301
-1018.524446	12.143473	1.361306
-1022.220148	3.880107	1.366310
-1026.090437	7.118080	1.371315
-1029.453793	-1.973989	1.376320
-1033.151025	0.731421	1.381325
-1037.344506	13.250766	1.386330
-1040.868231	3.277624	1.391334
-1044.874890	15.760165	1.396339
-1048.620454	7.528276	1.401344
-1052.323654	5.600478	1.406349
-1055.983827	9.283942	1.411354
-1059.646792	-2.418162	1.416358
-1063.836514	5.106731	1.421363
-1067.485844	-1.522177	1.426368
-1070.907311	0.402156	1.431373
-1074.808337	-5.038879	1.436378
-1078.256484	-2.568817	1.441382
-1082.227590	1.031093	1.446387
-1086.289732	2.650214	1.451392
-1089.701662	-3.554076	1.456397
-1093.568084	4.501469	1.461402
-1097.341203	-5.814813	1.466406
-1101.211499	1.061231	1.471411
-1104.747812	-1.450922	1.476416
-1108.577654	-5.638718	1.481421
-1112.738277	1.692157	1.486426
-1116.088872	-7.183749	1.491430
-1120.153915	10.919224	1.496435
-1123.766495	-2.714083	1.501440
-1127.414907	-0.124732	1.506445
-1131.391165	-0.606732	1.511450
-1134.571375	3.422239	1.516454
-1138.882699	6.198455	1.521459
-1142.710167	7.894954	1.526464
-1146.212978	8.158182	1.531469
-1150.002440	8.210920	1.536474
-1153.497251	0.726674	1.541478
-1157.628441	3.681564	1.546483
-1161.575044	2.011566	1.551488
-1164.992541	4.386045	1.556493
-1168.700454	10.387620	1.561498
-1172.105573	2.186201	1.566502
-1176.519104	6.063868	1.571507
-1179.903084	2.346632	1.576512
-1184.266019	9.093814	1.581517
-1188.283845	2.424097	1.586522
-1191.310918	-4.092493	1.591526
-1195.236046	0.782811	1.596531
-1198.676125	2.172062	1.601536
-1202.334776	7.848255	1.606541
-1206.148918	5.909254	1.611546
-1210.268772	2.603397	1.616550
-1214.371057	2.415466	1.621555
-1217.788125	-3.099464	1.626560
-1221.399629	4.303773	1.631565
-1225.449970	6.617654	1.636570
-1228.626218	-1.500265	1.641574
-1232.715072	2.193024	1.646579
-1236.441265	-1.858123	1.651584
-1240.358004	-1.377687	1.656589
-1244.515088	6.284649	1.661594
-1247.925482	3.379575	1.666598
-1251.844924	7.735706	1.671603
-1255.197931	-3.663412	1.676608
-1258.711084	3.832689	1.681613
-1263.011791	12.004015	1.686618
-1266.624976	1.208097	1.691622
-1270.587967	-0.902630	1.696627
-1274.161179	-0.153164	1.701632
-1277.840208	-1.423778	1.706637
-1281.569139	2.141428	1.711642
-1285.188558	0.460745	1.716646
-1289.030195	7.185986	1.721651
-1292.908653	-2.009991	1.726656
-1296.941936	-2.193510	1.731661
-1300.857689	-4.187594	1.736666
-1303.870191	2.171056	1.741670
-1308.216500	10.031334	1.746675
-1311.882626	8.175157	1.751680
-1315.095302	-0.048923	1.756685
-1319.122616	-1.134163	1.761690
-1322.884164	-7.112026	1.766694
-1327.056391	0.931111	1.771699
-1330.576534	3.241253	1.776704
-1334.624453	-5.772821	1.781709
-1338.193088	5.740311	1.786714
-1341.295844	2.107134	1.791718
-1345.328442	0.158423	1.796723
-1349.734663	10.849594	1.801728
-1353.404189	-0.962792	1.806733
-1356.972728	2.764386	1.811738
-1360.642935	-0.778013	1.816742
-1364.435604	-1.999033	1.821747
-1368.253149	-10.200472	1.826752
-1371.732720	-5.732706	1.831757
-1375.773019	1.635761	1.836762
-1379.239427	-0.570029	1.841766
-1383.056982	2.255811	1.846771
-1386.900665	5.090880	1.851776
-1390.884822	-1.183390	1.856781
-1394.819511	5.745410	1.861786
-1397.955917	-2.768782	1.866790
-1401.760180	6.634522	1.871795
-1405.974185	2.252495	1.876800
-1409.423068	4.014450	1.881805
-1413.477549	8.240777	1.886810
-1417.113113	1.793370	1.891814
-1420.951090	6.733634	1.896819
-1424.730746	-2.858886	1.901824
-1427.983200	0.475789	1.906829
-1432.428687	7.030171	1.911834
-1435.549046	7.702374	1.916838
-1439.391833	13.602616	1.921843
-1443.252300	7.680538	1.926848
-1447.051292	-0.094181	1.931853
-1451.129650	3.938929	1.936858
-1454.622358	-0.441443	1.941862
-1458.514866	1.764630	1.946867
-1462.462782	2.952414	1.951872
-1466.054434	0.868864	1.956877
-1469.696863	5.660322	1.961882
-1473.595134	2.857018	1.966886
-1477.500467	1.368508	1.971891
-1481.189740	0.998577	1.976896
-1484.738810	2.662158	1.981901
-1488.533478	9.500675	1.986906
-1491.556322	5.994006	1.991910
-1495.533270	3.810901	1.996915
-1499.826052	0.866859	2.006912
-1501.177672	2.167696	2.016909
-1498.475893	5.587221	2.026906
-1495.607897	7.116357	2.036902
-1493.374745	7.294657	2.046899
-1491.861057	6.806145	2.056896
-1489.636881	6.356420	2.066893
-1487.890135	9.844784	2.076890
-1486.005234	10.376165	2.086886
-1483.963106	7.360794	2.096883
-1482.177415	8.209581	2.106880
-1480.267707	6.866963	2.116877
-1478.281155	4.546043	2.126874
-1476.165069	3.130822	2.136870
-1474.346570	0.506799	2.146867
-1472.583688	3.007138	2.156864
-1470.702203	-1.825467	2.166861
-1468.932038	4.008798	2.176858
-1466.874171	10.223630	2.186854
-1465.055593	7.955680	2.196851
-1463.277768	-3.445684	2.206848
-1460.863245	-3.289830	2.216845
-1459.171978	1.096112	2.226842
-1457.397644	7.165214	2.236838
-1455.583863	4.058666	2.246835
-1453.953752	8.331024	2.256832
-1452.058273	7.427966	2.266829
-1449.787058	-1.134391	2.276826
-1448.235738	6.532921	2.286822
-1446.270648	0.434727	2.296819
-1444.293420	6.194308	2.306816
-1442.421428	-0.931640	2.316813
-1440.230344	4.944941	2.326810
-1438.374687	1.332847	2.336806
-1436.816294	1.630256	2.346803
-1434.592274	3.516279	2.356800
-1432.761038	3.290591	2.366797
-1431.417092	5.136916	2.376794
-1429.393311	0.111523	2.386790
-1427.181380	-1.158892	2.396787
-1425.473213	4.552465	2.406784
-1423.661487	2.555243	2.416781
-1421.664742	0.154346	2.426778
-1419.890249	5.970504	2.436774
-1417.723081	3.061337	2.446771
-1416.157331	-1.124983	2.456768
-1414.236972	0.067454	2.466765
-1412.268389	3.931923	2.476762
-1410.413593	4.334534	2.486758
-1408.840660	4.002257	2.496755
-1406.824644	5.441871	2.506752
-1404.681605	3.730391	2.516749
-1402.943621	7.250334	2.526746
-1400.860667	1.222020	2.536742
-1399.319986	4.089772	2.546739
-1397.028865	-1.705951	2.556736
-1395.086386	-0.282155	2.566733
-1393.750784	-1.545874	2.576730
-1391.560322	-2.954068	2.586726
-1389.616508	-2.500345	2.596723
-1387.527614	4.998375	2.606720
-1385.945430	2.439089	2.616717
-1384.564207	6.294205	2.626714
-1382.310882	0.497472	2.636710
-1380.260768	3.267052	2.646707
-1378.669903	8.023203	2.656704
-1376.430655	9.043504	2.666701
-1374.616663	1.578572	2.676698
-1372.820527	4.335664	2.686694
-1371.010848	5.376008	2.696691
-1369.064370	5.346731	2.706688
-1367.204068	4.199981	2.716685
-1365.376016	4.859350	2.726682
-1363.413104	7.396913	2.736678
-1361.464815	4.445538	2.746675
-1359.978294	0.847086	2.756672
-1357.981321	10.423824	2.766669
-1355.729605	3.484824	2.776666
-1354.119026	5.146262	2.786662
-1351.903521	4.469669	2.796659
-1350.247512	1.314383	2.806656
-1348.616892	1.330677	2.816653
-1346.592615	5.070608	2.826650
-1344.689209	8.375229	2.836646
-1342.710574	2.743470	2.846643
-1340.860168	5.273494	2.856640
-1338.888099	5.841347	2.866637
-1337.349951	-0.564452	2.876634
-1335.433343	7.404948	2.886630
-1333.334836	5.215438	2.896627
-1331.519836	4.269742	2.906624
-1329.835588	4.786258	2.916621
-1327.631039	9.434651	2.926618
-1325.709442	5.882809	2.936614
-1323.877075	3.892753	2.946611
-1322.429327	7.367735	2.956608
-1320.337385	11.241892	2.966605
-1318.223839	3.746077	2.976602
-1316.663139	7.387409	2.986598
-1314.652548	7.640788	2.996595
-1312.691425	2.358253	3.006592
-1310.882086	6.836225	3.016589
-1309.303048	9.535390	3.026586
-1306.825217	7.952993	3.036582
-1305.323308	4.713138	3.046579
-1303.280635	7.814038	3.056576
-1301.364546	11.768602	3.066573
-1299.491260	8.991381	3.076570
-1297.825922	6.195735	3.086566
-1296.039953	6.225283	3.096563
-1293.787545	4.309323	3.106560
-1292.142110	6.927533	3.116557
-1290.280098	12.162389	3.126554
-1288.243587	10.879491	3.136550
-1286.611711	7.069556	3.146547
-1284.863574	6.988229	3.156544
-1282.704000	8.759729	3.166541
-1280.745331	12.871397	3.176538
-1278.971766	0.462239	3.186534
-1277.207377	8.353479	3.196531
-1275.120094	5.203981	3.206528
-1273.182792	5.533991	3.216525
-1271.345240	7.407044	3.226522
-1269.529671	11.419594	3.236518
-1267.535158	6.032144	3.246515
-1266.134380	0.885784	3.256512
-1263.762108	5.503826	3.266509
-1262.158610	0.807179	3.276506
-1260.409383	-0.847659	3.286502
-1258.145635	4.040774	3.296499
-1256.476192	2.349448	3.306496
-1254.505692	1.111497	3.316493
-1252.783515	4.906523	3.326490
-1250.855298	8.577242	3.336486
-1248.668407	8.487367	3.346483
-1247.115171	8.845016	3.356480
-1245.075434	8.904512	3.366477
-1243.447473	8.494475	3.376474
-1241.220623	6.598740	3.386470
-1239.355724	5.792718	3.396467
-1237.813992	10.978269	3.406464
-1236.235603	15.096780	3.416461
-1233.817571	12.498331	3.426458
-1231.960839	11.456588	3.436454
-1230.326972	10.893780	3.446451
-1227.890770	9.876221	3.456448
-1226.548209	10.653809	3.466445
-1224.398577	11.461942	3.476442
-1222.548184	11.270996	3.486438
-1220.615603	9.825762	3.496435
-1218.925136	4.885365	3.506432
-1217.361962	13.225771	3.516429
-1215.434423	13.780780	3.526426
-1213.088444	2.666454	3.536422
-1211.479996	3.004753	3.546419
-1209.774662	11.987469	3.556416
-1207.621915	5.861884	3.566413
-1205.647082	7.866314	3.576410
-1203.727782	4.554020	3.586406
-1202.038380	8.496580	3.596403
-1199.827955	5.269058	3.606400
-1198.263063	7.461666	3.616397
-1196.407836	4.215708	3.626394
-1194.798767	2.905086	3.636390
-1192.429924	7.918578	3.646387
-1190.689476	2.859739	3.656384
-1188.678717	3.615463	3.666381
-1187.114948	-3.795365	3.676378
-1185.538257	9.369841	3.686374
-1183.358433	-0.031545	3.696371
-1181.215780	4.246182	3.706368
-1179.269826	5.895546	3.716365
-1177.627287	1.273241	3.726362
-1175.857910	6.135171	3.736358
-1173.892458	6.369890	3.746355
-1172.020073	3.028516	3.756352
-1169.955798	7.782503	3.766349
-1168.083336	8.533926	3.776346
-1166.202938	3.664477	3.786342
-1164.632253	4.894553	3.796339
-1162.591397	0.673758	3.806336
-1160.983537	6.475580	3.816333
-1158.903817	5.561959	3.826330
-1156.745895	8.535648	3.836326
-1154.943713	1.945447	3.846323
-1153.524583	1.353940	3.856320
-1151.419669	1.596337	3.866317
-1149.443430	7.277205	3.876314
-1147.604981	6.075020	3.886310
-1145.680757	6.844439	3.896307
-1144.017509	7.354757	3.906304
-1141.839456	1.151348	3.916301
-1139.989595	1.584962	3.926298
-1138.043647	5.578347	3.936294
-1136.278922	1.250057	3.946291
-1134.295368	4.727558	3.956288
-1132.749428	4.083060	3.966285
-1130.715633	8.929248	3.976282
-1128.867963	5.863646	3.986278
-1126.828415	7.802462	3.996275
-1124.959008	8.192811	4.006272
-1123.188721	7.758776	4.016269
-1121.658421	7.070728	4.026266
-1119.412957	10.707193	4.036262
-1117.378274	3.625749	4.046259
-1115.571199	8.120407	4.056256
-1113.656480	6.970745	4.066253
-1111.823456	7.583923	4.076250
-1110.048479	10.456220	4.086246
-1108.378643	7.586755	4.096243
-1106.422268	9.415373	4.106240
-1104.522343	2.478009	4.116237
-1102.536900	4.630452	4.126234
-1100.884694	7.555845	4.136230
-1098.694893	3.858451	4.146227
-1096.985140	4.104309	4.156224
-1095.120339	7.207010	4.166221
-1093.001471	14.212672	4.176218
-1091.249776	9.004917	4.186214
-1089.322600	0.246092	4.196211
-1087.486435	10.534710	4.206208
-1085.854794	6.601973	4.216205
-1083.637927	10.323992	4.226202
-1081.905036	8.578759	4.236198
-1080.076288	9.514388	4.246195
-1078.079179	7.507212	4.256192
-1076.160932	6.134852	4.266189
-1074.486519	6.731807	4.276186
-1072.362789	1.993717	4.286182
-1070.730145	3.142052	4.296179
-1068.799421	-1.067301	4.306176
-1066.836634	2.916508	4.316173
-1065.139014	6.109186	4.326170
-1063.135212	1.565980	4.336166
-1061.152799	1.735396	4.346163
-1059.247597	-1.568488	4.356160
-1057.714468	-1.497007	4.366157
-1055.837551	1.456217	4.376154
-1053.843941	4.556580	4.386150
-1051.910848	1.839937	4.396147
-1049.817208	-2.774412	4.406144
-1048.076044	1.018631	4.416141
-1046.327433	8.538827	4.426138
-1044.383082	9.619031	4.436134
-1042.397034	3.027336	4.446131
-1040.689346	2.505675	4.456128
-1038.563390	3.981134	4.466125
-1036.995754	4.664019	4.476122
-1034.957547	5.260577	4.486118
-1032.988960	10.631789	4.496115
-1031.418277	4.228792	4.506112
-1029.564925	3.804641	4.516109
-1027.407416	4.239629	4.526106
-1025.452671	6.489070	4.536102
-1023.913908	2.963562	4.546099
-1021.813482	1.040243	4.556096
-1019.858937	2.737215	4.566093
-1018.235643	2.897960	4.576090
-1016.169647	1.279336	4.586086
-1014.358844	5.319303	4.596083
-1012.557785	-1.673770	4.606080
-1010.332204	5.328632	4.616077
-1008.699855	7.536607	4.626074
-1006.808738	5.126760	4.636070
-1005.213460	3.925677	4.646067
-1002.880200	1.628834	4.656064
-1000.983056	9.957844	4.666061
-999.249743	6.976346	4.676058
-997.619898	6.447516	4.686054
-995.993556	8.062523	4.696051
-993.569368	10.739231	4.706048
-991.725851	8.959627	4.716045
-989.694701	14.717706	4.726042
-988.014880	9.727441	4.736038
-986.360620	12.877012	4.746035
-984.370367	11.814426	4.756032
-982.529699	14.187416	4.766029
-980.801605	9.837014	4.776026
-978.756764	10.044362	4.786022
-977.145116	14.111426	4.796019
-974.815022	2.541484	4.806016
-973.036956	11.900325	4.816013
-971.014330	12.742250	4.826010
-969.495378	12.890892	4.836006
-967.153309	6.302919	4.846003
-965.665064	12.842675	4.856000
-963.826486	15.190738	4.865997
-961.745800	9.567299	4.875994
-959.723520	5.720885	4.885990
-958.153337	10.058286	4.895987
-956.202300	8.003744	4.905984
-954.302395	9.137465	4.915981
-952.686891	13.145781	4.925978
-950.540643	8.559591	4.935974
-948.693299	8.086710	4.945971
-946.703472	6.441277	4.955968
-945.139586	10.939035	4.965965
-942.871702	7.539341	4.975962
-941.218983	8.603263	4.985958
-939.198780	9.877586	4.995955
-937.206810	6.434363	5.005952
-935.377323	6.766835	5.015949
-933.929830	12.640158	5.025946
-931.861252	0.729007	5.035942
-929.805119	2.289622	5.045939
-927.889063	5.569352	5.055936
-926.178916	11.091694	5.065933
-924.201666	4.346237	5.075930
-922.361157	8.613533	5.085926
-920.435985	6.188391	5.095923
-918.995259	1.138418	5.105920
-916.834201	12.420251	5.115917
-914.838676	5.911158	5.125914
-913.138053	6.605643	5.135910
-911.178675	9.945131	5.145907
-909.056209	9.341253	5.155904
-907.425200	11.586254	5.165901
-905.529338	9.483109	5.175898
-903.498542	11.001058	5.185894
-901.880364	7.242217	5.195891
-899.945453	10.204926	5.205888
-898.121275	5.163434	5.215885
-896.265170	16.234815	5.225882
-894.337518	9.552815	5.235878
-892.267175	11.667866	5.245875
-890.184535	10.507260	5.255872
-888.612321	7.024663	5.265869
-886.849622	10.441004	5.275866
-884.911847	5.818307	5.285862
-882.927460	5.597392	5.295859
-881.080371	0.909641	5.305856
-879.317862	6.649076	5.315853
-877.212172	14.210027	5.325850
-875.427871	7.737603	5.335846
-873.684966	5.613698	5.345843
-871.981414	9.529866	5.355840
-870.100960	12.237541	5.365837
-867.628882	5.784988	5.375834
-866.078025	12.644041	5.385830
-864.352714	7.008532	5.395827
-862.126655	8.332526	5.405824
-860.438968	6.784445	5.415821
-858.754368	10.898713	5.425818
-856.663488	13.527195	5.435814
-854.799843	12.282866	5.445811
-852.675639	6.307774	5.455808
-851.292867	9.844281	5.465805
-849.436703	11.726187	5.475802
-847.393772	5.155235	5.485798
-845.605748	4.695741	5.495795
-843.751869	9.818392	5.505792
-841.474723	9.485591	5.515789
-839.960918	9.335196	5.525786
-837.900984	11.330730	5.535782
-835.844309	5.535993	5.545779
-834.183536	7.505588	5.555776
-832.457853	4.679200	5.565773
-830.374645	8.580412	5.575770
-828.518118	4.201697	5.585766
-826.627292	6.942785	5.595763
-825.089275	3.510738	5.605760
-822.805572	7.037261	5.615757
-821.276615	4.618911	5.625754
-819.259996	2.682407	5.635750
-817.237228	6.789234	5.645747
-815.490124	5.930498	5.655744
-813.480683	3.483032	5.665741
-811.844267	9.813250	5.675738
-809.907460	7.022956	5.685734
-807.799168	5.909759	5.695731
-805.939457	12.412697	5.705728
-804.187142	6.712501	5.715725
-802.281288	4.661434	5.725722
-800.459403	9.505834	5.735718
-798.534816	11.064196	5.745715
-796.625786	0.786623	5.755712
-794.940241	7.959703	5.765709
-793.002744	8.892601	5.775706
-791.134893	12.890080	5.785702
-789.008337	8.412073	5.795699
-787.204124	11.515438	5.805696
-785.453251	8.936494	5.815693
-783.644358	11.711821	5.825690
-781.557221	7.395112	5.835686
-779.872236	7.345778	5.845683
-777.756426	10.106765	5.855680
-775.813097	13.681065	5.865677
-774.366559	8.744744	5.875674
-772.353544	10.253953	5.885670
-770.113673	4.012036	5.895667
-768.831538	5.554999	5.905664
-766.878048	7.622192	5.915661
-764.862335	7.097173	5.925658
-763.027491	15.279711	5.935654
-761.011624	11.398516	5.945651
-758.965255	12.754987	5.955648
-757.236957	15.768245	5.965645
-755.280748	15.199300	5.975642
-753.619155	15.866165	5.985638
-751.499029	14.507906	5.995635
-749.670028	12.286276	6.005632
-747.954009	12.333198	6.015629
-746.054090	14.499309	6.025626
-744.243585	17.396894	6.035622
-742.173036	9.574739	6.045619
-740.607870	10.582628	6.055616
-738.649951	14.105041	6.065613
-736.580773	11.340275	6.075610
-734.643835	6.159739	6.085606
-732.458464	6.283409	6.095603
-731.011319	12.493990	6.105600
-729.342211	10.764581	6.115597
-727.158004	14.353685	6.125594
-725.507388	5.884320	6.135590
-723.660992	9.359088	6.145587
-721.533647	10.096608	6.155584
-719.574851	10.713665	6.165581
-717.989048	6.647432	6.175578
-716.002811	0.568029	6.185574
-714.300633	-2.487061	6.195571
-712.417431	0.990088	6.205568
-710.130945	4.236385	6.215565
-708.314060	-2.900786	6.225562
-706.538055	-1.097935	6.235558
-704.818391	4.000389	6.245555
-702.809413	-0.520238	6.255552
-701.122429	2.079230	6.265549
-699.143955	0.077397	6.275546
-697.013822	12.717885	6.285542
-695.400693	-4.954299	6.295539
-693.359561	-5.308567	6.305536
-691.654739	-2.756026	6.315533
-689.661383	-2.855086	6.325530
-687.639015	-6.622355	6.335526
-685.954189	-1.480105	6.345523
-684.328589	-3.062124	6.355520
-682.244515	-2.140104	6.365517
-680.480213	-1.035947	6.375514
-678.665645	-1.619677	6.385510
-676.294530	-0.013793	6.395507
-674.411363	-3.183319	6.405504
-673.026943	0.418177	6.415501
-670.967417	1.682718	6.425498
-668.696364	2.011849	6.435494
-667.179707	-5.836151	6.445491
-665.322419	-0.633379	6.455488
-663.459853	-2.757583	6.465485
-661.640258	-6.206675	6.475482
-659.511206	-2.386359	6.485478
-657.739106	-3.787208	6.495475
-656.051644	-3.780404	6.505472
-654.469997	-3.835670	6.515469
-652.521696	-1.786900	6.525466
-650.491696	-2.058219	6.535462
-648.202299	-1.300652	6.545459
-646.435646	1.577229	6.555456
-644.752388	2.054668	6.565453
-642.883718	-1.302456	6.575450
-640.814750	-1.317641	6.585446
-638.988895	-8.765778	6.595443
-637.075760	-7.491908	6.605440
-635.339079	-8.559038	6.615437
-633.716803	-1.484504	6.625434
-631.701906	-4.735899	6.635430
-629.574331	-9.607639	6.645427
-627.903952	-5.979319	6.655424
-625.978310	-8.122630	6.665421
-624.206873	4.483017	6.675418
-621.881913	-3.993347	6.685414
-620.238008	-4.563972	6.695411
-618.077014	-2.958754	6.705408
-616.681954	-5.824363	6.715405
-614.713578	0.992789	6.725402
-612.738850	-4.656186	6.735398
-610.767800	-7.573997	6.745395
-609.076584	-9.982178	6.755392
-607.400115	-5.362118	6.765389
-605.403637	-3.880426	6.775386
-603.217689	-2.396861	6.785382
-601.771179	0.078713	6.795379
-599.972353	-7.649327	6.805376
-597.727734	-2.573850	6.815373
-595.743531	-3.736397	6.825370
-593.950776	-10.159187	6.835366
-592.135737	-10.040273	6.845363
-590.249808	-6.694352	6.855360
-588.285071	-7.319227	6.865357
-586.503088	-11.688216	6.875354
-584.821264	-13.241906	6.885350
-582.933878	-3.987394	6.895347
-580.750477	-10.669680	6.905344
-579.231309	-9.293009	6.915341
-577.303456	-9.786267	6.925338
-575.119437	-7.063758	6.935334
-573.124052	-11.337754	6.945331
-571.517278	-10.235373	6.955328
-569.657588	-11.861075	6.965325
-567.625704	-8.354833	6.975322
-566.002292	-5.846368	6.985318
-564.149963	-6.137749	6.995315
-561.893537	-4.158406	7.005312
-560.489199	-2.471543	7.015309
-558.301591	-3.576099	7.025306
-556.460900	-7.848840	7.035302
-554.652574	-10.374714	7.045299
-553.040172	-8.579692	7.055296
-550.898933	-3.871389	7.065293
-548.936060	-4.494345	7.075290
-547.111080	-5.271487	7.085286
-545.129504	-1.549112	7.095283
-543.249325	-6.918624	7.105280
-541.679713	-5.037212	7.115277
-539.409806	-7.996786	7.125274
-537.652872	0.149429	7.135270
-535.761111	1.660584	7.145267
-534.005420	-3.280890	7.155264
-532.257471	-2.860353	7.165261
-530.295830	-6.403720	7.175258
-527.887758	-3.574980	7.185254
-526.636531	-5.477647	7.195251
-524.838172	-2.970332	7.205248
-522.772380	-1.410384	7.215245
-520.713677	-2.822018	7.225242
-518.923667	-3.239432	7.235238
-517.024035	-3.101012	7.245235
-515.447638	0.064482	7.255232
-513.319829	5.056900	7.265229
-511.483579	3.138832	7.275226
-509.647280	0.538221	7.285222
-507.486643	-3.478759	7.295219
-505.714617	-3.301051	7.305216
-504.054223	0.050409	7.315213
-502.265162	-2.178496	7.325210
-500.261129	-2.898207	7.335206
-498.258895	-3.413678	7.345203
-496.460800	-5.806169	7.355200
-494.837086	-3.034514	7.365197
-492.436737	-3.728947	7.375194
-490.891019	-1.711415	7.385190
-488.804234	2.256941	7.395187
-486.800906	-1.310557	7.405184
-485.313117	-1.646069	7.415181
-483.242525	2.011662	7.425178
-481.616209	2.952640	7.435174
-479.511469	2.282056	7.445171
-477.488494	-0.177466	7.455168
-476.129249	2.762088	7.465165
-473.972301	6.902584	7.475162
-472.037869	2.425272	7.485158
-470.326039	4.801624	7.495155
-468.060068	6.377843	7.505152
-466.355612	5.592956	7.515149
-464.683263	0.055592	7.525146
-462.550350	2.444675	7.535142
-460.821655	-1.392261	7.545139
-458.975860	-3.150699	7.555136
-456.973092	6.183291	7.565133
-455.168608	2.134165	7.575130
-453.097835	2.878756	7.585126
-451.475302	1.672798	7.595123
-449.631899	-1.745916	7.605120
-447.311536	3.263694	7.615117
-445.852310	-0.940006	7.625114
-444.216641	0.132963	7.635110
-442.008927	1.561104	7.645107
-439.684336	4.163534	7.655104
-438.605298	4.016331	7.665101
-436.649757	4.001731	7.675098
-434.626218	-0.454889	7.685094
-432.332803	-1.339222	7.695091
-430.538907	0.493479	7.705088
-429.152035	2.144257	7.715085
-426.977852	3.158836	7.725082
-425.012562	2.976579	7.735078
-423.360169	6.853501	7.745075
-421.495284	5.588588	7.755072
-419.382810	12.891744	7.765069
-417.667891	-0.764296	7.775066
-415.959502	-2.580163	7.785062
-414.133458	-7.593341	7.795059
-412.066402	-1.897638	7.805056
-410.054945	-0.084861	7.815053
-408.240101	-2.113434	7.825050
-406.264131	1.692571	7.835046
-404.319643	1.071251	7.845043
-402.464518	-1.091093	7.855040
-400.777118	-1.915713	7.865037
-399.007785	0.195495	7.875034
-396.975502	1.091759	7.885030
-395.233288	0.507909	7.895027
-392.807964	-9.004435	7.905024
-391.298228	-1.015325	7.915021
-389.919335	-1.190638	7.925018
-387.823201	1.383034	7.935014
-385.647367	-0.260469	7.945011
-383.572238	-2.587805	7.955008
-381.953321	2.053688	7.965005
-380.482979	2.344062	7.975002
-378.286596	2.995212	7.984998
-376.074484	-0.617541	7.994995
-374.337979	2.331630	8.004992
-372.691755	4.783697	8.014989
-370.706448	2.592314	8.024986
-368.997442	1.037990	8.034982
-366.673214	1.707131	8.044979
-365.056024	6.808564	8.054976
-363.570099	-0.764553	8.064973
-361.592753	5.586817	8.074970
-359.409186	11.781485	8.084966
-357.239848	5.966824	8.094963
-355.726957	3.735155	8.104960
-354.059567	4.481012	8.114957
-351.913953	-0.338375	8.124954
-349.973145	5.397991	8.134950
-347.962934	4.612077	8.144947
-346.425798	-1.895625	8.154944
-344.508483	1.914939	8.164941
-342.700753	-0.437650	8.174938
-340.810673	0.361702	8.184934
-338.782064	3.398713	8.194931
-336.864204	2.672514	8.204928
-335.102837	2.017821	8.214925
-333.267384	-1.849636	8.224922
-331.257069	2.628307	8.234918
-329.402295	-1.954639	8.244915
-327.667441	2.779231	8.254912
-325.770326	5.981081	8.264909
-323.668921	3.209388	8.274906
-321.994592	7.365564	8.284902
-320.041651	4.041930	8.294899
-318.065654	0.079627	8.304896
-316.291120	2.982779	8.314893
-314.452423	1.391606	8.324890
-312.619243	-0.934905	8.334886
-310.499385	-1.481139	8.344883
-308.882931	-0.696887	8.354880
-307.158670	3.274069	8.364877
-305.219282	-0.710009	8.374874
-303.181826	-2.108417	8.384870
-301.143876	-1.977426	8.394867
-299.396487	-4.110975	8.404864
-297.354047	-0.146376	8.414861
-295.789667	5.113535	8.424858
-293.888895	10.198369	8.434854
-291.785189	-2.829538	8.444851
-290.131353	0.029117	8.454848
-288.191742	1.282398	8.464845
-286.292675	6.837438	8.474842
-284.502909	4.937707	8.484838
-282.431162	6.400713	8.494835
-280.759030	2.011544	8.504832
-278.747703	8.139365	8.514829
-277.232929	6.672930	8.524826
-275.097056	4.467223	8.534822
-272.972125	4.146989	8.544819
-271.107433	3.592372	8.554816
-269.213890	6.276734	8.564813
-267.111308	7.260990	8.574810
-265.972328	4.111373	8.584807
-263.981936	0.424854	8.594803
-261.791238	-1.161463	8.604800
-260.037252	-0.828404	8.614797
-258.317601	2.869873	8.624794
-256.088865	-0.026780	8.634791
-254.456200	-1.082248	8.644787
-252.799087	0.402486	8.654784
-250.613510	-0.574315	8.664781
-248.644994	0.968461	8.674778
-246.971261	0.580584	8.684775
-245.084375	1.904581	8.694771
-243.101017	3.319532	8.704768
-241.214192	1.596430	8.714765
-239.343700	6.714148	8.724762
-237.792262	4.363664	8.734759
-235.303507	-0.159229	8.744755
-233.666528	3.761913	8.754752
-232.077869	5.478136	8.764749
-230.059780	4.314283	8.774746
-227.958122	-5.703684	8.784743
-225.573411	-3.257284	8.794739
-224.182344	-5.106394	8.804736
-222.609772	-10.118319	8.814733
-220.634784	-5.076220	8.824730
-218.751482	-7.813225	8.834727
-216.791456	-6.625068	8.844723
-214.974507	-1.512386	8.854720
-213.025673	-3.486006	8.864717
-211.558667	-4.420567	8.874714
-209.210743	-5.321646	8.884711
-207.526009	-6.574150	8.894707
-205.541171	-9.144393	8.904704
-203.965578	-6.779347	8.914701
-201.997896	-8.284308	8.924698
-199.815994	-8.155037	8.934695
-198.134006	-7.831344	8.944691
-196.196699	-3.102894	8.954688
-194.331443	-2.120584	8.964685
-192.592372	-12.263681	8.974682
-190.571346	-5.317411	8.984679
-188.847090	-11.220862	8.994675
-186.891166	-14.673396	9.004672
-185.109879	-8.717916	9.014669
-182.980711	-7.512907	9.024666
-181.366624	-9.322001	9.034663
-179.183251	-7.018893	9.044659
-177.436724	-13.486179	9.054656
-175.630414	-3.955915	9.064653
-173.589031	-3.674482	9.074650
-171.958363	-0.509863	9.084647
-169.863152	-7.212819	9.094643
-168.063317	-5.697199	9.104640
-166.244877	-5.422188	9.114637
-164.600232	-5.061646	9.124634
-162.687373	-6.782066	9.134631
-160.374134	-5.389664	9.144627
-158.563234	-10.233374	9.154624
-156.958799	-6.363929	9.164621
-155.143352	-2.817992	9.174618
-153.128645	-4.375261	9.184615
-150.893971	3.274237	9.194611
-149.135961	1.156707	9.204608
-147.389386	2.773160	9.214605
-145.530654	-0.939739	9.224602
-143.927428	-7.553570	9.234599
-142.139552	-6.895877	9.244595
-139.837939	-8.303550	9.254592
-137.673654	-8.167671	9.264589
-136.341579	-9.622885	9.274586
-134.434928	-8.991091	9.284583
-132.559768	-7.091182	9.294579
-130.709755	-1.835135	9.304576
-128.732117	-0.643635	9.314573
-126.480546	-0.803323	9.324570
-125.165178	-0.212008	9.334567
-122.780134	-2.509778	9.344563
-121.241850	-0.481349	9.354560
-119.472834	-0.541682	9.364557
-117.345816	1.952132	9.374554
-115.608825	1.909940	9.384551
-113.710002	-3.521897	9.394547
-111.724582	2.045688	9.404544
-109.985526	6.333525	9.414541
-108.164940	2.366338	9.424538
-106.107363	8.501731	9.434535
-104.071167	3.309552	9.444531
-102.443970	-0.888078	9.454528
-100.929053	1.394932	9.464525
-98.744213	3.189188	9.474522
-96.358415	3.670856	9.484519
-94.792942	-0.831569	9.494515
-93.254899	3.865410	9.504512
-91.193891	10.043301	9.514509
-89.286417	6.180576	9.524506
-87.528431	7.780869	9.534503
-85.528348	4.414860	9.544499
-83.892662	2.850290	9.554496
-81.758413	2.751451	9.564493
-79.987088	6.220808	9.574490
-78.010919	4.593112	9.584487
-75.908681	0.842434	9.594483
-74.045315	-0.222890	9.604480
-72.463235	4.728179	9.614477
-70.393524	10.601853	9.624474
-68.586734	6.368693	9.634471
-66.876179	8.648206	9.644467
-65.178264	8.140450	9.654464
-63.220022	12.929405	9.664461
-61.107640	2.739710	9.674458
-58.752432	1.780942	9.684455
-57.600688	4.956593	9.694451
-55.895675	7.941731	9.704448
-53.656484	7.943474	9.714445
-51.461131	5.621355	9.724442
-49.844325	3.330069	9.734439
-48.168200	3.380545	9.744435
-46.040600	8.094225	9.754432
-44.367272	9.875044	9.764429
-42.251748	3.612873	9.774426
-40.581200	9.501258	9.784423
-38.246780	5.665728	9.794419
-36.844059	1.127992	9.804416
-34.824636	6.553436	9.814413
-33.142164	2.983438	9.824410
-31.188255	5.749641	9.834407
-29.196394	-1.166349	9.844403
-27.302468	5.793901	9.854400
-25.432961	3.437556	9.864397
-23.540905	4.152130	9.874394
-21.679874	6.521262	9.884391
-19.779350	6.336453	9.894387
-17.976479	0.824273	9.904384
-16.041398	-2.102542	9.914381
-14.384609	0.641499	9.924378
-12.795464	5.021084	9.934375
-10.325442	9.284806	9.944371
-8.504479	2.973165	9.954368
-6.656079	2.272452	9.964365
-5.235203	-0.676457	9.974362
-3.469176	22.921436	9.984359
-2.264999	62.051326	9.994355
-1.112325	109.620959	10.004352
0.000000	157.913606	10.009357
0.890462	198.866979	10.014362
1.314172	231.796952	10.019367
1.697745	254.258072	10.024371
2.333056	281.029407	10.029376
2.113377	306.046421	10.034381
2.745186	309.934210	10.039386
2.828262	328.120054	10.044391
2.803112	350.096813	10.049395
3.236329	350.526183	10.054400
2.809283	352.859163	10.059405
3.165173	359.281405	10.064410
3.421816	382.161957	10.069415
3.240510	389.082487	10.074419
3.941801	395.509072	10.079424
3.647088	401.894074	10.084429
3.915719	397.641854	10.089434
3.550883	403.910202	10.094439
3.601316	399.951173	10.099443
4.230198	401.073283	10.104448
3.761704	410.776903	10.109453
3.868502	404.714606	10.114458
3.682538	408.440676	10.119463
3.640930	418.350174	10.124467
4.294014	435.024911	10.129472
4.237574	446.262446	10.134477
4.330437	444.813669	10.139482
4.315104	447.911698	10.144487
4.495946	456.531809	10.149491
4.452186	447.435422	10.154496
4.592449	457.468493	10.159501
4.277373	461.547490	10.164506
4.445120	458.130416	10.169511
4.437744	452.376615	10.174515
4.800851	452.674725	10.179520
4.514245	459.429795	10.184525
4.639023	461.207534	10.189530
4.791533	462.776446	10.194535
4.853227	474.114531	10.199539
4.623408	468.516491	10.204544
4.513799	478.616497	10.209549
4.888172	478.504138	10.214554
4.695711	477.816361	10.219559
4.508283	485.200598	10.224563
4.868054	480.301172	10.229568
4.990888	492.714671	10.234573
5.186095	502.797558	10.239578
5.477331	512.837146	10.244583
5.026720	515.303660	10.249587
5.159722	505.421429	10.254592
5.183503	516.694996	10.259597
5.327540	509.317369	10.264602
5.538256	518.170411	10.269607
5.465926	522.565422	10.274611
5.668711	525.494229	10.279616
5.351401	534.875960	10.284621
5.479617	525.999506	10.289626
5.586299	523.638908	10.294631
5.523363	527.416540	10.299635
5.663194	524.169234	10.304640
5.909887	539.864981	10.309645
5.779651	531.717686	10.314650
5.700350	533.218592	10.319655
5.576601	537.509927	10.324659
5.828803	536.687880	10.329664
5.707093	539.330892	10.334669
5.820496	538.961709	10.339674
5.942326	545.207457	10.344679
5.700398	544.177248	10.349683
5.886956	551.668308	10.354688
5.710919	566.621062	10.359693
5.846199	564.662517	10.364698
6.226640	571.221554	10.369703
6.280797	576.839463	10.374707
6.255096	561.525355	10.379712
5.840763	574.540217	10.384717
6.303551	573.429832	10.389722
6.503917	581.786541	10.394727
6.486223	589.583028	10.399731
6.963229	595.607639	10.404736
6.384232	590.751117	10.409741
6.537232	587.895871	10.414746
6.548045	603.279241	10.419751
6.824899	614.287650	10.424755
6.629658	608.356007	10.429760
6.398604	620.003729	10.434765
6.641332	616.077593	10.439770
7.010620	627.042927	10.444775
7.031442	621.976184	10.449779
6.852121	624.121074	10.454784
6.650408	630.238388	10.459789
6.626127	620.140691	10.464794
7.086717	626.851005	10.469799
7.150873	643.911148	10.474803
7.386848	646.214566	10.479808
7.481354	656.697310	10.484813
7.461286	644.701814	10.489818
7.436656	635.293360	10.494823
7.360859	630.843561	10.499827
7.557062	634.777703	10.504832
7.175169	633.396890	10.509837
7.585307	643.823928	10.514842
7.693951	653.551107	10.519847
7.425429	667.499444	10.524851
7.729104	656.935764	10.529856
7.748113	665.828865	10.534861
7.700079	664.007525	10.539866
7.644165	661.470711	10.544871
7.470315	663.816769	10.549875
7.905100	660.287946	10.554880
7.606874	667.180884	10.559885
7.746873	658.555355	10.564890
7.934829	666.975421	10.569895
7.794682	666.151957	10.574899
8.021876	665.582081	10.579904
7.480540	672.059215	10.584909
8.196035	685.185574	10.589914
8.206649	691.579525	10.594919
8.224121	697.195083	10.599923
8.442478	701.364254	10.604928
8.374018	702.138201	10.609933
8.674944	705.673492	10.614938
8.814255	700.975216	10.619943
8.572899	698.911893	10.624947
8.840182	699.436435	10.629952
8.634060	708.545789	10.634957
8.585189	705.909472	10.639962
8.777258	718.352332	10.644967
9.003790	710.937572	10.649971
8.674658	706.824865	10.654976
8.494612	697.570914	10.659981
9.053793	707.411531	10.664986
9.080851	702.668160	10.669991
8.820785	709.729043	10.674995
8.983645	708.117849	10.680000
9.120762	720.040012	10.685005
8.858599	718.423534	10.690010
9.087672	714.847867	10.695015
8.841309	718.928175	10.700019
9.026741	707.946980	10.705024
8.725906	723.115488	10.710029
9.226834	719.335710	10.715034
9.402805	718.044366	10.720039
9.150701	726.175976	10.725043
9.010024	717.984979	10.730048
8.965793	730.746254	10.735053
9.539894	746.337521	10.740058
9.602753	751.748346	10.745063
9.357421	745.935764	10.750067
9.831201	748.050004	10.755072
9.528544	755.082685	10.760077
9.654717	748.185238	10.765082
9.870891	751.500207	10.770087
9.737722	755.960977	10.775091
9.903946	749.094161	10.780096
9.888382	753.021223	10.785101
9.785251	754.261372	10.790106
10.134113	760.461569	10.795111
9.627769	751.557212	10.800115
10.212049	751.248996	10.805120
10.075490	764.529804	10.810125
9.896946	755.080959	10.815130
10.125108	755.291691	10.820135
10.038398	755.199968	10.825139
10.179826	769.562045	10.830144
10.197910	780.818622	10.835149
10.511525	778.750921	10.840154
10.501859	784.313927	10.845159
10.342989	784.623387	10.850163
10.444913	775.540119	10.855168
10.237986	787.307773	10.860173
10.502247	779.759407	10.865178
10.850330	787.463278	10.870183
10.468002	792.658743	10.875187
10.805213	787.519146	10.880192
10.371235	785.906858	10.885197
10.849496	780.435979	10.890202
10.850884	788.635077	10.895207
10.441593	797.356166	10.900211
10.842747	793.694135	10.905216
11.166347	812.061537	10.910221
10.965814	813.339312	10.915226
11.358372	813.570803	10.920231
10.737700	803.912345	10.925235
11.170425	807.202433	10.930240
11.319102	812.346726	10.935245
11.377813	815.231213	10.940250
11.287100	816.558448	10.945255
11.213983	822.302871	10.950259
11.757167	817.789519	10.955264
11.492902	817.749160	10.960269
11.647349	816.073477	10.965274
11.421556	809.966209	10.970279
11.536689	817.395830	10.975283
11.561087	823.571159	10.980288
11.740573	825.607188	10.985293
11.711272	816.868102	10.990298
11.685354	816.137543	10.995303
11.568212	821.945172	11.000307
11.668068	811.670936	11.005312
11.749120	823.158323	11.010317
11.332876	827.033315	11.015322
11.956193	816.928268	11.020327
11.633560	825.227152	11.025331
11.829597	811.637652	11.030336
12.041717	840.322355	11.035341
12.509301	846.229076	11.040346
12.341409	835.374687	11.045351
11.983240	827.188950	11.050355
12.462471	826.982429	11.055360
12.516450	833.193347	11.060365
12.353675	830.764827	11.065370
12.075448	823.044590	11.070375
12.161509	845.366131	11.075379
12.420862	850.865667	11.080384
12.547536	846.896216	11.085389
12.898724	854.707744	11.090394
13.080820	847.985399	11.095399
12.950959	841.984431	11.100403
13.401296	835.739909	11.105408
13.055748	817.718449	11.110413
12.849392	815.960947	11.115418
12.935074	811.783799	11.120423
12.577812	809.269814	11.125427
12.907000	810.046243	11.130432
12.783983	812.738866	11.135437
12.969126	816.297587	11.140442
13.054695	824.788188	11.145447
12.912911	835.249593	11.150451
13.117052	842.064762	11.155456
13.431188	847.865163	11.160461
13.167112	851.221050	11.165466
13.699026	845.368322	11.170471
13.498608	825.161205	11.175475
13.426684	827.654809	11.180480
13.323866	817.524266	11.185485
13.651380	812.027118	11.190490
13.889704	813.187805	11.195495
13.578184	811.370968	11.200499
13.793611	803.811227	11.205504
13.430900	814.997332	11.210509
13.586598	815.432460	11.215514
13.413651	817.361154	11.220519
13.611478	828.937864	11.225523
14.022997	837.135745	11.230528
14.033145	845.999285	11.235533
13.868118	842.496292	11.240538
14.199623	840.565251	11.245543
13.846611	845.705576	11.250547
13.957500	840.342664	11.255552
14.064627	851.092583	11.260557
14.081988	848.868434	11.265562
13.763249	843.570501	11.270567
13.963347	848.663359	11.275571
14.377848	845.135210	11.280576
14.234963	843.967210	11.285581
14.603712	843.439768	11.290586
14.559784	842.282827	11.295591
14.323781	847.634797	11.300595
14.222611	842.054826	11.305600
14.257431	848.781399	11.310605
14.634931	847.489833	11.315610
14.622506	853.870038	11.320615
14.462306	851.381468	11.325619
14.462581	851.014307	11.330624
14.519100	850.815527	11.335629
14.172777	858.796389	11.340634
14.782375	859.399611	11.345639
15.047657	881.874421	11.350643
15.016037	860.948322	11.355648
15.167951	875.930404	11.360653
14.928043	879.669386	11.365658
16.042194	852.883609	11.370663
15.725365	841.963174	11.375667
15.620906	839.443733	11.380672
15.467770	839.387478	11.385677
15.242166	832.346626	11.390682
15.603445	833.688336	11.395687
15.452498	832.718691	11.400691
15.710569	825.590965	11.405696
15.291330	832.066966	11.410701
15.462289	827.644274	11.415706
15.812602	833.265969	11.420711
15.445519	836.652541	11.425715
15.596147	829.874810	11.430720
15.427245	828.234435	11.435725
15.712118	834.485107	11.440730
15.611952	833.309784	11.445735
15.282010	841.138224	11.450739
15.603239	830.271026	11.455744
15.594390	833.795120	11.460749
15.317435	842.721700	11.465754
15.698619	838.735060	11.470759
15.638586	841.153996	11.475763
15.885176	850.940935	11.480768
15.912691	863.127918	11.485773
16.309315	874.358343	11.490778
16.328082	865.357569	11.495783
16.005395	872.123344	11.500787
16.075544	868.895019	11.505792
16.317274	866.662792	11.510797
16.150354	867.466260	11.515802
16.174246	868.803059	11.520807
16.286825	876.101306	11.525811
16.431256	861.571672	11.530816
16.227610	864.513388	11.535821
16.213903	868.510028	11.540826
16.764304	864.458053	11.545831
16.368431	865.806035	11.550835
16.635390	872.287160	11.555840
16.489533	878.663412	11.560845
16.615329	878.110125	11.565850
16.831876	884.078061	11.570855
16.701549	899.123163	11.575859
16.882175	897.999953	11.580864
17.032424	903.652819	11.585869
16.941169	896.024434	11.590874
17.589350	896.176967	11.595879
16.861470	881.188595	11.600883
16.964622	886.910319	11.605888
17.015913	893.673561	11.610893
16.856134	901.917720	11.615898
17.141721	903.565308	11.620903
16.973861	904.830777	11.625907
17.274924	903.376261	11.630912
17.255841	904.143330	11.635917
16.772320	903.239782	11.640922
17.234113	895.352363	11.645927
17.209275	906.441523	11.650931
17.652796	920.153132	11.655936
17.938797	926.141150	11.660941
17.677285	918.231684	11.665946
17.950489	899.234045	11.670951
17.481903	911.743362	11.675955
17.831133	900.589474	11.680960
17.881965	914.456039	11.685965
17.817416	915.864453	11.690970
18.140006	916.239390	11.695975
17.858855	910.690254	11.700979
17.857245	909.013687	11.705984
18.124036	925.686503	11.710989
17.779107	928.659166	11.715994
18.326182	927.412729	11.720999
17.905677	939.802904	11.726003
18.210496	927.052015	11.731008
18.199351	934.535317	11.736013
18.253262	931.400948	11.741018
18.693585	932.179644	11.746023
18.444089	928.971376	11.751027
18.376425	929.333094	11.756032
18.424928	932.149881	11.761037
18.635247	936.823386	11.766042
18.569555	931.152827	11.771047
18.290707	931.085757	11.776051
18.601080	923.217971	11.781056
18.646422	930.663955	11.786061
18.693142	934.099202	11.791066
19.012361	932.855516	11.796071
18.668943	930.011507	11.801075
18.706621	931.287527	11.806080
18.884571	937.586179	11.811085
18.922680	944.936304	11.816090
18.731615	938.262902	11.821095
18.321778	937.692110	11.826099
18.983338	939.849182	11.831104
18.824740	947.905270	11.836109
18.836382	970.686590	11.841114
19.394350	957.586353	11.846119
19.184564	956.367447	11.851123
19.591077	951.184731	11.856128
19.445543	955.945703	11.861133
19.552573	953.391955	11.866138
19.863196	950.756327	11.871143
19.451133	954.674844	11.876147
19.564539	953.833548	11.881152
19.753570	950.233115	11.886157
19.812492	945.594337	11.891162
19.502967	924.077516	11.896167
19.803750	937.152039	11.901171
19.873187	940.611813	11.906176
19.744211	932.941720	11.911181
19.880192	942.273210	11.916186
19.681113	941.972596	11.921191
19.811462	951.507557	11.926195
19.691927	949.557522	11.931200
19.784175	950.977344	11.936205
19.799461	947.572490	11.941210
19.994719	948.153206	11.946215
19.647482	953.817178	11.951219
19.836300	953.903212	11.956224
20.186178	947.061663	11.961229
19.983576	948.414408	11.966234
20.514429	964.547782	11.971239
20.332668	976.134817	11.976243
20.621425	968.663476	11.981248
20.386197	949.279663	11.986253
20.456099	957.803418	11.991258
20.624416	956.270605	11.996263
20.628374	974.193270	12.001267
20.996108	954.558042	12.006272
20.847206	955.289346	12.011277
20.418617	952.523488	12.016282
20.904957	943.984866	12.021287
20.647965	955.653074	12.026291
20.531127	956.505196	12.031296
20.606867	945.770009	12.036301
20.640431	953.278812	12.041306
20.556457	957.043971	12.046311
20.564587	963.360303	12.051315
20.495585	956.935962	12.056320
20.577214	956.822875	12.061325
20.185373	965.665407	12.066330
20.554890	966.876244	12.071335
20.442258	983.623651	12.076339
20.649707	979.352555	12.081344
20.696987	984.023634	12.086349
20.686884	989.928236	12.091354
20.554122	984.949681	12.096359
20.621506	988.477318	12.101363
20.824849	987.704285	12.106368
20.851916	978.943995	12.111373
20.525681	986.587136	12.116378
20.988170	989.355846	12.121383
20.600489	978.115095	12.126387
20.702492	978.852723	12.131392
20.976350	967.842368	12.136397
20.506248	965.655203	12.141402
20.662235	958.934129	12.146407
20.450264	958.300595	12.151411
20.685560	961.180491	12.156416
20.598452	968.733281	12.161421
20.567869	969.461667	12.166426
20.875860	960.082829	12.171431
20.611846	958.680984	12.176435
20.413954	963.630146	12.181440
21.087630	967.469086	12.186445
20.772667	967.163472	12.191450
20.925346	960.328096	12.196455
20.808730	964.688588	12.201459
20.796208	962.244153	12.206464
21.079924	971.382568	12.211469
20.512896	960.652973	12.216474
20.653047	959.342094	12.221479
20.405272	964.576518	12.226483
20.597905	965.771894	12.231488
20.646968	971.424766	12.236493
20.679068	967.535447	12.241498
20.723085	967.057362	12.246503
20.886571	973.165878	12.251507
21.041312	969.133557	12.256512
21.038099	967.964494	12.261517
20.794134	969.667358	12.266522
20.924111	964.707314	12.271527
20.603828	947.952024	12.276531
20.501331	933.483213	12.281536
20.452150	948.133926	12.286541
20.734529	959.617289	12.291546
20.710349	961.698520	12.296551
20.461680	969.569536	12.301555
20.780042	959.055240	12.306560
20.707970	962.088099	12.311565
20.780776	969.896497	12.316570
21.007303	947.454051	12.321575
20.768445	940.618316	12.326579
20.782183	938.917404	12.331584
20.721667	937.898694	12.336589
20.787242	934.075485	12.341594
21.016037	928.861274	12.346599
20.713834	933.896600	12.351603
20.293470	935.169050	12.356608
20.866018	933.788378	12.361613
20.737495	937.605380	12.366618
20.720029	934.319828	12.371623
20.322412	932.848919	12.376627
20.226699	936.458192	12.381632
20.573255	931.606682	12.386637
20.293695	946.390050	12.391642
20.216949	929.431577	12.396647
20.466552	947.160121	12.401651
20.948935	957.593143	12.406656
20.885141	960.581556	12.411661
20.657025	953.489370	12.416666
20.880700	946.422749	12.421671
20.528066	951.128440	12.426675
20.400127	944.450132	12.431680
20.669211	936.987706	12.436685
20.363928	940.280019	12.441690
20.610648	944.914918	12.446695
20.947674	962.835726	12.451699
20.866514	955.286896	12.456704
21.197834	947.569848	12.461709
20.980637	945.722216	12.466714
21.047444	936.666190	12.471719
20.721252	944.564696	12.476723
20.747192	941.197490	12.481728
20.812512	935.035127	12.486733
20.813629	940.281736	12.491738
20.989788	935.198916	12.496743
20.782390	934.204206	12.501747
20.867137	927.124704	12.506752
20.794888	911.201657	12.511757
20.615291	915.025438	12.516762
20.487468	912.816699	12.521767
20.516655	916.865602	12.526771
20.603370	920.100174	12.531776
20.656464	921.889073	12.536781
20.730267	927.226241	12.541786
20.467074	914.968276	12.546791
20.790939	928.156861	12.551795
20.657203	932.022124	12.556800
20.582241	921.812921	12.561805
20.502308	933.874304	12.566810
20.585927	935.871917	12.571815
21.033569	938.866979	12.576819
21.017883	924.235266	12.581824
20.907804	915.965892	12.586829
20.795685	917.198516	12.591834
21.005279	910.317878	12.596839
20.486622	917.937136	12.601843
20.232518	918.502530	12.606848
20.631231	918.091526	12.611853
20.431616	911.553415	12.616858
20.786474	911.586111	12.621863
20.814401	919.306258	12.626867
20.866060	911.254680	12.631872
20.792581	913.696854	12.636877
20.368086	922.190490	12.641882
20.590200	917.967816	12.646887
20.773420	919.968086	12.651891
20.474819	920.666241	12.656896
20.619429	915.803176	12.661901
20.729110	921.730240	12.666906
20.649485	914.099852	12.671911
20.556638	920.255454	12.676915
20.674785	918.961377	12.681920
20.520879	917.021582	12.686925
20.617632	923.630200	12.691930
20.834687	912.976595	12.696935
20.583557	909.995583	12.701939
20.506065	923.644160	12.706944
20.830530	921.024716	12.711949
20.617878	923.505754	12.716954
20.841364	919.448633	12.721959
20.581468	924.943279	12.726963
20.416245	928.616968	12.731968
20.855556	929.655573	12.736973
20.449374	930.747171	12.741978
20.569924	921.166022	12.746983
20.184760	931.105540	12.751987
20.650676	927.557506	12.756992
20.802501	920.254139	12.761997
20.610172	927.027981	12.767002
20.574443	919.854272	12.772007
20.715899	925.538259	12.777011
20.926740	924.778548	12.782016
20.728923	921.603262	12.787021
20.542956	932.995593	12.792026
20.651639	924.093841	12.797031
20.760084	923.562080	12.802035
20.573561	928.106652	12.807040
20.995605	927.431912	12.812045
20.689745	924.710543	12.817050
21.042894	930.056658	12.822055
20.884695	925.809980	12.827059
20.668039	930.511692	12.832064
20.980352	919.711882	12.837069
20.725163	929.129381	12.842074
20.746396	919.756707	12.847079
20.801751	921.002853	12.852083
20.526246	924.836765	12.857088
20.799113	927.983369	12.862093
20.903129	922.947658	12.867098
20.449622	908.914051	12.872103
20.410707	904.483901	12.877107
20.562188	920.130833	12.882112
21.029282	917.202331	12.887117
21.094860	908.086928	12.892122
20.802460	889.297198	12.897127
20.450258	891.426371	12.902131
20.682220	888.304113	12.907136
20.726041	892.927996	12.912141
20.740442	899.193885	12.917146
20.891690	895.168103	12.922151
20.771414	894.820031	12.927155
20.652732	893.179724	12.932160
20.663584	900.337135	12.937165
20.498669	903.543006	12.942170
21.084523	895.299582	12.947175
20.990597	901.325889	12.952179
20.629555	902.270800	12.957184
20.910832	899.404161	12.962189
20.581839	895.847164	12.967194
20.545416	898.055221	12.972199
20.416603	901.992264	12.977203
20.443772	904.933097	12.982208
20.791395	901.508771	12.987213
20.462267	903.281887	12.992218
20.507599	900.171100	12.997223
20.397932	900.410941	13.002227
20.500436	910.802487	13.007232
20.367580	904.043724	13.012237
20.146334	907.531226	13.017242
20.431980	901.728991	13.022247
20.611057	916.414747	13.027251
20.439925	926.317566	13.032256
20.825840	936.646720	13.037261
20.830539	940.470881	13.042266
20.976463	920.160047	13.047271
20.782242	909.614065	13.052275
20.469652	907.478454	13.057280
20.600399	900.709627	13.062285
20.652473	912.214680	13.067290
20.978769	909.224664	13.072295
20.429962	922.954840	13.077299
20.486262	916.682321	13.082304
20.761545	902.872707	13.087309
20.318551	921.290758	13.092314
20.182470	925.987732	13.097319
20.527464	940.163487	13.102323
20.503476	953.169367	13.107328
20.872369	946.996002	13.112333
20.977695	943.019923	13.117338
20.994617	929.765766	13.122343
20.807714	925.435194	13.127347
20.446079	917.505790	13.132352
20.638154	911.857752	13.137357
20.496718	910.087924	13.142362
20.903813	908.192467	13.147367
20.582425	910.413464	13.152371
20.062277	916.128385	13.157376
20.936498	920.337137	13.162381
20.592724	928.441148	13.167386
20.610747	918.646265	13.172391
20.747892	922.850342	13.177395
20.602349	926.182369	13.182400
20.923555	914.242623	13.187405
20.581809	918.954727	13.192410
20.238868	912.018825	13.197415
20.612678	915.697194	13.202419
20.773341	939.540807	13.207424
20.720651	926.825164	13.212429
20.767469	925.306080	13.217434
20.610967	919.129651	13.222439
20.644687	915.668749	13.227443
20.362990	919.753193	13.232448
21.195262	931.130805	13.237453
20.912508	928.644682	13.242458
20.625015	912.191701	13.247463
21.101275	907.390985	13.252467
20.750286	911.207046	13.257472
21.262982	906.151796	13.262477
20.896002	913.049129	13.267482
20.879377	920.024947	13.272487
20.814977	918.162962	13.277491
20.460434	917.431507	13.282496
20.888201	912.891339	13.287501
20.935244	912.794840	13.292506
20.553539	903.235081	13.297511
20.498970	894.488046	13.302515
20.514460	898.303242	13.307520
20.872590	906.194922	13.312525
20.626098	910.284380	13.317530
20.424259	897.022759	13.322535
20.671300	905.176642	13.327539
20.518619	908.109234	13.332544
20.685141	908.977111	13.337549
20.323606	916.276930	13.342554
20.387069	914.370128	13.347559
20.741315	918.373956	13.352563
20.480422	926.661518	13.357568
20.594983	918.625598	13.362573
20.435439	924.267641	13.367578
20.907828	921.807175	13.372583
20.800727	911.911382	13.377587
20.198176	922.163297	13.382592
20.848452	914.674602	13.387597
20.828297	918.988938	13.392602
20.541894	918.987900	13.397607
20.987052	920.781023	13.402611
20.645102	919.392150	13.407616
21.005588	920.029404	13.412621
20.974349	919.670803	13.417626
21.095170	901.028497	13.422631
20.973317	894.899030	13.427635
20.675407	895.832721	13.432640
20.639748	889.353745	13.437645
20.794241	891.463936	13.442650
20.764497	887.718660	13.447655
20.575555	889.519449	13.452659
20.757715	895.369339	13.457664
20.888529	892.025609	13.462669
20.813040	898.154543	13.467674
20.423359	890.105621	13.472679
20.308644	890.464353	13.477683
20.390419	905.830330	13.482688
20.365904	889.995041	13.487693
20.316171	898.272435	13.492698
20.224997	894.043089	13.497703
20.370481	902.594117	13.502707
20.339188	922.182228	13.507712
20.852895	920.720461	13.512717
20.493902	926.250651	13.517722
20.486781	928.118164	13.522727
20.885977	926.176296	13.527731
20.434877	930.922548	13.532736
20.385194	926.148056	13.537741
20.219912	928.949392	13.542746
20.379259	931.554543	13.547751
20.463220	924.384783	13.552755
20.488586	931.498668	13.557760
20.831082	928.954683	13.562765
20.599470	932.607388	13.567770
20.652629	931.575109	13.572775
20.737465	930.287137	13.577779
20.555126	936.664141	13.582784
20.636212	928.882244	13.587789
20.832154	935.958990	13.592794
20.662371	933.242708	13.597799
20.670579	930.789987	13.602803
20.461236	935.947549	13.607808
20.890512	929.601601	13.612813
20.584793	944.769188	13.617818
20.594947	937.444314	13.622823
20.635007	938.154666	13.627827
20.339470	931.166812	13.632832
20.651385	932.663837	13.637837
20.562036	942.009489	13.642842
20.717887	939.499478	13.647847
20.688819	942.098646	13.652851
20.847343	940.345673	13.657856
20.882307	931.796818	13.662861
21.391393	931.731229	13.667866
21.062349	940.425218	13.672871
21.398658	929.633918	13.677875
20.811985	921.914016	13.682880
20.781756	916.659748	13.687885
20.698085	910.033469	13.692890
20.927762	909.251977	13.697895
20.983293	907.348115	13.702899
20.472471	918.796924	13.707904
20.716676	906.254601	13.712909
20.801574	913.845373	13.717914
20.749086	908.352951	13.722919
20.888845	910.680801	13.727923
20.607894	912.672236	13.732928
20.713051	906.388580	13.737933
20.603816	916.707093	13.742938
20.764777	904.852856	13.747943
20.445927	912.361669	13.752947
20.457014	918.522345	13.757952
20.747581	910.230859	13.762957
20.698326	914.097817	13.767962
20.488413	916.755225	13.772967
20.901926	912.664735	13.777971
20.373683	915.583959	13.782976
20.558659	912.039492	13.787981
20.562839	914.247695	13.792986
20.675112	917.046834	13.797991
20.591650	913.147342	13.802995
20.497547	914.318062	13.808000
20.853732	904.649943	13.813005
20.653183	909.940593	13.818010
20.680685	911.735852	13.823015
20.940606	913.191264	13.828019
20.759671	913.273195	13.833024
20.724937	916.127539	13.838029
20.654309	920.336845	13.843034
20.563648	911.005072	13.848039
20.621959	919.948422	13.853043
20.373378	921.276680	13.858048
20.762662	913.365764	13.863053
20.648627	916.858964	13.868058
20.700978	916.409847	13.873063
20.735593	913.354973	13.878067
20.573153	919.058695	13.883072
20.507475	915.770360	13.888077
20.680496	918.805793	13.893082
20.782416	916.625162	13.898087
20.719041	911.928022	13.903091
20.484893	922.468480	13.908096
20.396018	919.400436	13.913101
20.488841	914.823355	13.918106
20.439289	922.505472	13.923111
20.593723	913.331015	13.928115
20.510460	913.456199	13.933120
20.606069	915.711489	13.938125
20.428650	915.754527	13.943130
20.707522	914.449077	13.948135
21.029425	915.391760	13.953139
20.827091	925.309007	13.958144
21.180650	918.179472	13.963149
20.936294	917.910305	13.968154
21.015244	920.736475	13.973159
20.815094	911.163739	13.978163
20.678273	899.357010	13.983168
20.619920	884.168576	13.988173
20.677128	885.491375	13.993178
20.676737	879.244380	13.998183
21.317117	878.741810	14.003187
21.067419	890.893452	14.008192
21.220462	885.558306	14.013210
21.218883	885.762515	14.018227
20.751443	891.270562	14.023245
20.977290	872.873942	14.028263
21.063503	866.139031	14.033280
20.912110	851.562475	14.038298
20.811398	861.986688	14.043315
20.411981	850.720583	14.048333
20.752018	853.141559	14.053351
20.603131	852.665074	14.058368
20.930911	853.042747	14.063386
20.222070	846.393766	14.068403
20.125059	869.268922	14.073421
20.238324	877.313394	14.078439
20.286244	886.253384	14.083456
20.626652	889.069603	14.088474
20.779712	901.856788	14.093491
20.742841	912.069288	14.098509
20.701571	917.921231	14.103527
21.110089	923.166888	14.108544
21.153765	914.247764	14.113562
20.987759	914.301413	14.118579
20.782062	922.080496	14.123597
20.982421	922.328433	14.128615
20.811781	920.294547	14.133632
20.730482	920.161613	14.138650
20.896269	926.129643	14.143667
20.765471	925.890228	14.148685
20.804464	920.710346	14.153703
20.961316	928.871789	14.158720
20.796392	945.503159	14.163738
21.069765	955.130960	14.168755
21.067477	949.537251	14.173773
21.242158	943.150156	14.178791
21.209043	942.877062	14.183808
21.263565	948.364931	14.188826
21.134298	953.155917	14.193843
21.382940	959.187712	14.198861
21.536513	951.863616	14.203879
21.158453	964.643879	14.208896
21.184428	952.342097	14.213914
21.448329	956.027412	14.218931
21.225251	967.929076	14.223949
21.455665	956.675780	14.228967
21.428396	958.091565	14.233984
21.314332	956.147193	14.239002
21.391870	962.077215	14.244019
21.444026	965.398415	14.249037
21.560837	956.246633	14.254055
21.278072	955.354092	14.259072
21.784582	957.065785	14.264090
21.656603	952.394869	14.269107
21.658084	960.906613	14.274125
21.965739	954.387652	14.279143
21.512482	963.651035	14.284160
22.059414	956.212245	14.289178
21.792126	957.595556	14.294195
21.560304	966.124468	14.299213
21.520987	958.949591	14.304231
21.577236	960.702262	14.309248
21.425224	961.444111	14.314266
21.670418	958.479807	14.319283
21.158934	954.814474	14.324301
21.377742	960.507267	14.329319
21.790495	979.633508	14.334336
21.575850	992.020000	14.339354
21.769032	995.632010	14.344371
21.567814	993.587608	14.349389
21.908351	992.217696	14.354407
21.853088	993.542607	14.359424
21.588103	991.437086	14.364442
21.982873	988.593992	14.369459
21.978515	995.085350	14.374477
22.281013	996.222929	14.379495
22.046894	994.648768	14.384512
22.096003	986.606293	14.389530
22.332162	991.578748	14.394547
22.225499	994.079485	14.399565
22.254623	987.553932	14.404583
22.046074	989.744949	14.409600
21.970055	988.961063	14.414618
22.158337	988.332663	14.419635
21.879094	994.086450	14.424653
22.088243	991.084616	14.429671
21.920493	992.022092	14.434688
21.843462	993.411371	14.439706
21.834117	998.831068	14.444723
21.968657	998.132742	14.449741
22.000944	990.169927	14.454759
22.523567	1006.942945	14.459776
22.205081	1011.751036	14.464794
22.200570	1000.417900	14.469811
22.083894	1007.383279	14.474829
22.379449	1023.673556	14.479847
22.406231	1024.691862	14.484864
22.429018	1029.045352	14.489882
22.922903	1023.205508	14.494899
22.363932	1011.426446	14.499917
22.877448	1004.285117	14.504935
22.623906	994.906240	14.509952
22.666520	1001.339544	14.514970
22.850003	997.756634	14.519987
22.772108	1003.490077	14.525005
23.045624	994.529925	14.530023
22.887966	990.880695	14.535040
22.508567	990.343327	14.540058
22.877348	989.808003	14.545075
22.735455	990.717422	14.550093
22.723339	980.200231	14.555111
22.755243	984.482849	14.560128
22.769093	991.191967	14.565146
22.739469	981.316405	14.570163
22.774948	992.167386	14.575181
22.690977	982.338152	14.580199
22.595193	986.572187	14.585216
22.222119	986.840879	14.590234
22.442924	986.313603	14.595251
22.474354	993.552817	14.600269
22.698058	1001.416988	14.605287
22.337186	993.263689	14.610304
22.379537	994.182860	14.615322
22.686370	1010.963351	14.620339
22.683032	1020.864244	14.625357
22.767455	1019.559110	14.630375
23.162902	1019.529094	14.635392
23.146537	1031.270552	14.640410
22.938313	1018.585614	14.645427
22.599951	1024.744460	14.650445
22.801319	1024.425255	14.655463
22.976205	1028.114824	14.660480
22.712408	1026.923729	14.665498
22.618621	1016.786291	14.670515
22.972193	1022.995804	14.675533
23.153432	1037.035054	14.680551
23.119744	1043.064104	14.685568
23.102059	1046.896940	14.690586
23.186409	1046.663157	14.695603
23.719247	1058.828227	14.700621
23.532413	1035.945527	14.705639
23.674361	1017.793847	14.710656
23.364540	1025.290025	14.715674
23.587348	1016.775988	14.720691
23.797106	1023.722022	14.725709
23.384862	1013.662024	14.730727
23.232997	1018.013564	14.735744
23.181536	1015.495418	14.740762
23.538917	1012.739050	14.745779
23.265901	1014.808044	14.750797
23.597892	1019.041188	14.755815
23.661926	1014.752323	14.760832
23.256741	1013.972114	14.765850
23.321847	1010.935520	14.770867
23.326099	1017.006090	14.775885
23.473340	1018.479367	14.780903
23.577369	1014.156871	14.785920
23.304611	1021.905766	14.790938
23.454110	1012.608179	14.795955
23.571226	1023.451485	14.800973
23.431125	1035.706718	14.805991
24.243128	1043.571232	14.811008
24.048091	1040.305199	14.816026
24.298981	1021.524161	14.821043
24.238343	1023.002764	14.826061
24.278251	1026.504830	14.831079
23.864136	1014.164668	14.836096
23.892814	1019.660537	14.841114
23.992078	1005.617674	14.846131
23.615682	1013.472137	14.851149
24.088988	1013.567757	14.856167
24.031841	1004.802886	14.861184
23.600556	1005.694990	14.866202
23.774740	1009.013388	14.871219
23.533188	1017.899534	14.876237
23.593533	1015.684289	14.881255
23.553893	1019.865002	14.886272
23.640785	1027.124251	14.891290
23.594848	1015.117055	14.896307
23.546309	1027.666842	14.901325
23.859047	1038.860898	14.906343
23.977120	1034.191474	14.911360
23.997863	1038.447672	14.916378
23.870246	1047.127278	14.921395
23.863052	1051.045331	14.926413
24.208831	1050.529304	14.931431
24.088529	1051.001921	14.936448
23.936910	1053.223741	14.941466
23.999801	1041.398667	14.946483
24.197098	1047.408983	14.951501
23.873422	1046.333673	14.956519
24.592459	1050.280369	14.961536
24.308985	1046.778298	14.966554
24.584195	1043.404077	14.971571
24.755479	1042.327767	14.976589
24.365067	1035.140212	14.981607
24.793024	1041.470453	14.986624
24.347061	1051.334650	14.991642
24.245891	1038.000191	14.996659
24.780588	1047.515917	15.001677
24.229976	1048.949781	15.006695
24.492671	1044.241384	15.011712
24.145526	1040.053328	15.016730
24.375946	1037.586068	15.021747
24.303309	1046.059381	15.026765
24.644436	1067.932864	15.031783
24.897873	1056.960610	15.036800
24.930959	1068.561718	15.041818
24.704336	1044.598342	15.046835
24.594272	1040.264904	15.051853
24.588405	1043.931134	15.056871
24.929786	1050.878630	15.061888
24.894511	1046.048867	15.066906
25.219705	1045.083581	15.071923
24.951342	1050.485891	15.076941
24.840689	1046.246261	15.081959
24.961015	1040.721660	15.086976
24.736987	1045.586013	15.091994
24.761968	1040.543936	15.097011
25.074316	1052.330633	15.102029
24.703864	1049.257679	15.107047
25.045076	1043.518026	15.112064
25.030314	1041.006182	15.117082
25.080811	1046.362089	15.122099
24.956451	1035.244767	15.127117
24.559229	1035.497520	15.132135
25.061365	1035.222423	15.137152
24.686097	1049.833515	15.142170
25.120354	1062.437964	15.147187
25.397104	1067.119603	15.152205
25.263840	1065.018261	15.157223
25.386928	1050.835042	15.162240
24.900141	1044.249878	15.167258
24.597910	1052.388910	15.172275
24.876874	1060.585789	15.177293
24.702158	1071.753595	15.182311
24.863712	1071.836915	15.187328
24.755401	1083.064215	15.192346
24.960811	1075.027182	15.197363
25.441485	1090.012856	15.202381
25.367291	1098.447091	15.207399
26.008156	1095.401928	15.212416
25.685347	1088.214570	15.217434
25.439735	1074.164236	15.222451
25.569971	1064.012768	15.227469
25.449685	1065.579167	15.232487
25.513216	1061.733717	15.237504
25.364543	1070.035026	15.242522
25.268482	1066.537041	15.247539
25.490181	1060.986390	15.252557
25.234068	1078.827328	15.257575
25.496831	1089.200397	15.262592
25.843308	1094.663459	15.267610
25.641605	1094.624008	15.272627
26.124250	1092.084357	15.277645
25.630031	1095.478790	15.282663
26.260046	1086.981518	15.287680
25.697131	1074.450663	15.292698
25.436616	1062.685748	15.297715
25.657547	1071.242216	15.302733
25.355840	1083.699224	15.307751
26.001958	1089.313680	15.312768
26.286033	1097.280944	15.317786
25.820787	1100.080994	15.322803
25.839314	1101.462560	15.327821
26.022561	1098.721860	15.332839
25.967463	1091.326776	15.337856
26.046232	1092.838574	15.342874
26.209994	1094.691733	15.347891
26.669124	1079.523240	15.352909
25.994303	1072.588384	15.357927
25.843491	1059.361244	15.362944
26.159295	1056.487185	15.367962
25.932257	1064.152666	15.372979
26.240711	1067.621297	15.377997
26.040907	1080.044688	15.383015
26.127210	1081.647327	15.388032
26.243024	1082.959450	15.393050
25.973098	1095.680331	15.398067
26.042126	1092.616275	15.403085
26.054295	1103.949715	15.408103
26.573131	1092.601590	15.413120
26.393842	1094.875014	15.418138
26.882658	1080.751905	15.423155
26.873277	1069.126225	15.428173
26.958123	1061.910325	15.433191
26.654330	1048.119221	15.438208
26.890776	1051.708077	15.443226
26.483599	1048.022475	15.448243
26.775757	1042.145160	15.453261
26.326001	1040.331567	15.458279
26.329317	1039.510846	15.463296
26.630443	1045.614785	15.468314
26.170672	1050.665238	15.473331
26.429048	1041.639933	15.478349
26.631537	1047.140659	15.483367
26.563630	1037.259026	15.488384
26.773113	1042.069523	15.493402
26.665286	1044.891359	15.498419
26.680373	1035.185275	15.503437
26.157025	1048.514572	15.508455
26.415720	1047.316180	15.513472
26.640359	1064.318318	15.518490
26.525992	1080.566725	15.523507
26.939457	1064.116605	15.528525
26.672867	1078.014156	15.533543
26.887318	1078.813266	15.538560
27.271331	1079.662050	15.543578
26.936060	1091.192857	15.548595
27.320526	1076.813212	15.553613
27.089051	1081.770198	15.558631
26.708946	1082.929143	15.563648
26.790551	1081.102793	15.568666
26.969497	1086.318177	15.573683
27.441486	1078.037389	15.578701
26.890001	1087.013331	15.583719
27.074566	1089.149559	15.588736
26.792487	1085.445650	15.593754
26.694669	1094.037489	15.598771
26.706725	1085.407569	15.603789
26.754267	1078.622500	15.608807
27.159761	1095.024328	15.613824
27.537678	1107.988501	15.618842
27.405187	1110.786228	15.623859
27.542741	1095.300385	15.628877
27.618448	1089.148722	15.633895
27.391577	1074.663644	15.638912
27.569687	1079.710258	15.643930
26.927642	1078.879310	15.648947
27.286085	1084.113921	15.653965
27.694580	1093.255220	15.658983
27.464747	1101.795283	15.664000
27.331801	1096.652303	15.669018
27.227076	1102.445505	15.674035
27.683707	1110.244990	15.679053
27.782942	1121.977721	15.684071
27.955969	1114.110801	15.689088
28.033697	1104.256128	15.694106
27.644945	1100.775245	15.699123
27.614802	1084.491721	15.704141
27.531247	1072.910254	15.709159
27.369025	1079.206650	15.714176
27.745206	1088.887780	15.719194
27.646555	1102.256519	15.724211
28.207460	1099.085290	15.729229
27.968964	1102.372882	15.734247
27.952218	1102.386372	15.739264
27.888531	1074.923477	15.744282
27.441594	1082.736915	15.749299
27.784831	1083.045798	15.754317
27.895138	1099.736843	15.759335
27.738398	1101.082706	15.764352
28.043532	1100.157867	15.769370
28.164338	1104.137458	15.774387
27.931663	1098.924561	15.779405
28.015224	1105.482395	15.784423
27.917764	1111.771638	15.789440
28.221732	1108.300339	15.794458
27.866195	1112.980550	15.799475
28.177753	1101.842381	15.804493
27.827195	1104.572370	15.809511
27.740283	1112.139827	15.814528
28.280139	1107.621705	15.819546
27.908132	1113.604450	15.824563
28.350531	1130.506327	15.829581
28.352231	1134.691401	15.834599
28.451476	1133.943998	15.839616
28.451221	1131.982453	15.844634
28.301088	1139.137107	15.849651
28.561104	1126.512754	15.854669
28.816686	1133.712419	15.859687
28.722542	1138.173003	15.864704
28.659920	1114.370392	15.869722
28.670703	1111.185206	15.874739
28.410794	1098.656319	15.879757
28.494960	1095.986943	15.884775
28.509169	1108.385868	15.889792
28.715278	1105.047499	15.894810
28.679211	1130.339552	15.899827
28.660169	1130.795990	15.904845
28.728799	1127.696560	15.909863
28.745626	1131.813287	15.914880
28.960607	1135.489314	15.919898
29.076196	1126.598687	15.924915
28.799721	1110.243976	15.929933
28.819696	1107.834049	15.934951
28.435799	1109.777959	15.939968
28.857427	1112.287358	15.944986
29.089261	1131.338105	15.950003
28.847920	1135.100246	15.955021
29.063173	1133.250582	15.960039
28.986264	1134.290217	15.965056
29.404549	1132.918382	15.970074
28.859011	1130.797158	15.975091
29.243783	1135.296899	15.980109
29.351021	1134.905241	15.985127
28.801620	1116.583770	15.990144
29.127577	1121.027443	15.995162
29.087485	1123.492770	16.000179
29.400232	1121.105877	16.005197
29.403020	1121.883401	16.010215
28.934489	1121.499117	16.015232
29.005804	1122.960224	16.020250
29.178124	1132.307800	16.025267
29.396104	1122.970451	16.030285
28.940811	1130.973549	16.035303
29.100389	1130.382351	16.040320
29.475217	1125.499967	16.045338
29.285541	1125.928177	16.050355
29.354816	1125.047319	16.055373
29.597465	1123.717016	16.060391
28.943255	1140.828186	16.065408
29.168102	1133.709913	16.070426
29.258409	1146.667915	16.075443
29.297216	1157.752318	16.080461
29.405986	1156.478434	16.085479
29.477165	1159.743654	16.090496
29.702513	1160.977157	16.095514
29.481434	1153.693579	16.100531
29.815259	1156.124724	16.105549
29.864746	1153.426241	16.110567
29.801207	1162.173278	16.115584
29.624753	1155.511627	16.120602
29.804656	1158.004206	16.125619
29.848989	1157.998955	16.130637
30.085482	1155.610956	16.135655
29.783821	1155.520921	16.140672
29.905555	1155.698084	16.145690
29.952298	1161.950418	16.150707
29.734613	1160.550208	16.155725
29.878197	1158.464383	16.160743
29.972147	1180.285121	16.165760
30.368249	1174.972661	16.170778
30.257778	1168.534357	16.175795
29.980512	1168.396435	16.180813
30.176549	1166.899303	16.185831
30.189893	1182.367194	16.190848
30.426939	1176.424469	16.195866
30.422629	1162.388592	16.200883
30.048899	1153.556647	16.205901
30.237471	1156.337921	16.210919
30.185458	1179.422763	16.215936
30.449829	1172.669774	16.220954
30.677589	1184.953399	16.225971
30.534647	1180.090081	16.230989
30.497805	1159.893520	16.236007
30.519811	1153.926644	16.241024
30.500814	1142.008045	16.246042
30.353604	1150.005578	16.251059
30.551951	1165.942956	16.256077
30.625025	1163.781417	16.261095
30.643913	1165.575954	16.266112
30.759513	1160.825807	16.271130
30.652738	1150.384578	16.276147
30.681962	1156.013483	16.281165
30.302694	1146.302891	16.286183
30.018544	1169.539734	16.291200
30.337886	1176.019373	16.296218
30.374101	1180.004430	16.301235
30.391265	1183.771871	16.306253
30.664777	1175.153771	16.311271
30.717272	1197.780921	16.316288
31.182176	1204.725420	16.321306
31.557311	1202.262065	16.326323
31.510610	1185.655657	16.331341
31.525191	1176.876422	16.336359
31.438807	1170.856463	16.341376
31.536505	1161.589325	16.346394
31.837248	1163.014249	16.351411
31.275209	1151.043462	16.356429
31.161578	1139.005253	16.361447
30.990841	1135.824805	16.366464
31.120712	1135.500532	16.371482
31.243893	1131.729095	16.376499
30.995798	1144.920721	16.381517
31.719227	1150.408945	16.386535
31.026470	1141.213954	16.391552
30.964718	1145.974524	16.396570
30.821175	1150.172299	16.401587
31.029412	1167.267527	16.406605
31.374740	1168.734417	16.411623
31.425948	1168.382289	16.416640
31.620719	1175.836909	16.421658
31.500768	1168.258403	16.426675
31.028740	1175.881684	16.431693
31.208052	1168.723955	16.436711
30.890356	1181.260954	16.441728
31.074381	1186.458176	16.446746
31.214746	1194.204834	16.451763
31.284485	1198.216829	16.456781
31.567252	1200.668154	16.461799
31.400922	1206.949950	16.466816
31.449064	1206.128621	16.471834
31.972438	1218.291503	16.476851
31.825246	1227.697857	16.481869
32.237989	1226.104110	16.486887
31.904885	1207.648981	16.491904
32.056215	1197.824547	16.496922
32.152674	1188.677693	16.501939
32.037356	1190.700772	16.506957
32.233186	1192.555926	16.511975
32.261899	1186.655216	16.516992
32.099250	1195.029860	16.522010
32.493073	1192.699928	16.527027
31.960266	1195.243838	16.532045
31.951261	1187.841986	16.537063
32.196635	1189.740619	16.542080
31.981005	1190.976498	16.547098
32.529066	1194.980896	16.552115
32.203492	1196.438399	16.557133
32.360964	1193.288681	16.562151
32.175769	1194.914257	16.567168
31.644352	1192.956760	16.572186
31.914634	1198.344332	16.577203
32.129868	1212.989777	16.582221
32.590732	1220.467699	16.587239
32.645826	1223.496693	16.592256
32.535688	1231.893065	16.597274
32.965218	1230.276360	16.602291
32.479884	1218.420334	16.607309
32.526671	1205.430473	16.612327
32.769598	1201.929065	16.617344
32.483021	1198.953126	16.622362
32.480890	1193.601055	16.627379
32.567085	1213.269837	16.632397
32.702734	1220.014475	16.637415
32.740969	1222.539228	16.642432
32.485226	1232.613071	16.647450
32.957010	1217.314311	16.652467
32.874920	1222.524886	16.657485
33.219694	1212.212906	16.662503
33.050490	1221.089519	16.667520
32.801371	1213.776072	16.672538
33.038214	1214.059101	16.677555
32.851705	1227.900531	16.682573
33.135265	1217.168690	16.687591
32.976338	1220.861992	16.692608
32.947676	1219.112805	16.697626
33.071963	1218.622150	16.702643
33.169863	1225.671320	16.707661
33.083675	1215.357631	16.712679
33.003417	1216.034822	16.717696
32.947802	1226.837406	16.722714
33.049752	1220.558347	16.727731
33.067880	1221.106849	16.732749
33.151148	1220.761822	16.737767
33.066241	1218.735246	16.742784
33.129630	1235.883733	16.747802
33.320166	1236.334953	16.752819
33.328888	1249.696432	16.757837
33.373768	1251.901125	16.762855
33.508779	1251.941750	16.767872
33.380442	1249.238697	16.772890
33.726339	1244.097040	16.777907
33.900149	1253.271191	16.782925
34.172647	1244.440609	16.787943
33.956900	1235.940617	16.792960
33.173219	1229.139325	16.797978
33.503037	1237.492554	16.802995
33.541970	1253.023851	16.808013
33.688304	1252.528234	16.813031
33.514895	1246.521986	16.818048
33.188623	1249.672283	16.823066
33.491578	1245.831803	16.828083
33.442955	1248.756920	16.833101
33.540434	1268.110423	16.838119
34.367638	1271.074374	16.843136
33.770532	1281.700128	16.848154
34.237406	1278.000843	16.853171
34.482016	1282.341177	16.858189
34.300658	1262.966576	16.863207
34.340868	1254.348272	16.868224
34.033823	1251.058876	16.873242
34.240638	1241.227263	16.878259
33.912189	1249.112996	16.883277
34.085102	1245.264101	16.888295
34.373403	1268.902986	16.893312
34.450586	1274.580803	16.898330
34.535415	1251.894535	16.903347
34.443683	1250.139621	16.908365
34.013638	1245.596792	16.913383
34.666564	1258.366683	16.918400
34.675043	1269.220124	16.923418
34.665769	1257.911636	16.928435
34.258182	1257.055439	16.933453
34.713820	1262.712463	16.938471
34.489736	1256.295177	16.943488
34.741264	1265.335920	16.948506
34.600513	1263.220478	16.953523
35.017358	1269.964961	16.958541
34.557036	1260.794225	16.963559
35.083172	1257.281653	16.968576
34.372607	1255.550549	16.973594
35.143782	1259.034385	16.978611
34.686471	1260.164055	16.983629
34.261132	1269.265335	16.988647
35.139662	1263.346856	16.993664
34.936932	1273.156494	16.998682
34.939992	1268.248823	17.003699
35.484383	1269.680019	17.008717
35.112118	1277.468938	17.013735
35.046537	1277.640420	17.018752
34.994793	1285.134209	17.023770
35.339300	1270.918733	17.028787
35.445489	1279.952904	17.033805
35.482266	1265.830355	17.038823
35.228242	1251.558842	17.043840
34.980519	1238.928137	17.048858
35.317512	1256.871937	17.053875
35.507639	1270.570475	17.058893
35.496719	1268.147708	17.063911
35.451956	1244.769038	17.068928
34.956707	1254.476837	17.073946
35.304147	1259.628742	17.078963
35.672321	1261.492548	17.083981
35.024012	1273.622484	17.088999
35.548106	1271.606456	17.094016
34.867532	1271.416804	17.099034
34.897636	1270.280032	17.104051
35.262429	1279.663601	17.109069
34.957403	1281.461320	17.114087
35.055635	1292.802190	17.119104
35.227968	1308.371700	17.124122
35.505990	1302.361659	17.129139
35.664047	1300.408386	17.134157
35.372269	1312.495729	17.139175
35.887328	1326.088994	17.144192
35.986664	1336.078400	17.149210
36.358855	1339.849186	17.154227
36.246304	1343.429044	17.159245
36.162846	1318.588256	17.164263
35.937358	1298.474257	17.169280
36.443813	1312.161514	17.174298
36.150943	1303.848739	17.179315
36.073294	1296.896046	17.184333
36.101520	1307.874880	17.189351
36.050751	1296.791215	17.194368
36.039352	1305.001784	17.199386
36.187876	1315.574923	17.204403
36.481299	1321.709429	17.209421
36.645524	1329.270944	17.214439
36.526003	1319.436961	17.219456
36.317949	1318.772949	17.224474
36.176489	1311.658340	17.229491
36.468599	1324.577165	17.234509
36.329216	1334.770900	17.239527
36.324988	1332.595030	17.244544
36.649984	1326.371395	17.249562
36.380857	1337.058681	17.254579
36.521765	1333.762154	17.259597
36.352078	1334.415703	17.264615
36.711429	1326.639576	17.269632
36.259542	1336.803026	17.274650
36.581378	1336.804926	17.279667
36.648726	1336.291744	17.284685
36.637954	1352.981771	17.289703
37.035680	1355.779587	17.294720
37.144465	1360.404280	17.299738
36.642542	1354.007028	17.304755
36.828850	1359.590962	17.309773
36.637317	1358.666217	17.314791
36.514793	1357.698929	17.319808
36.584566	1366.934688	17.324826
36.992393	1352.831522	17.329843
37.089979	1361.637667	17.334861
37.367961	1363.043676	17.339879
37.405115	1354.742800	17.344896
37.461231	1355.107218	17.349914
37.557435	1356.579041	17.354931
37.535333	1351.920170	17.359949
37.323650	1355.155574	17.364967
37.791250	1349.412253	17.369984
37.684719	1352.498120	17.375002
37.126502	1354.044348	17.380019
37.925844	1347.951995	17.385037
37.496225	1351.219646	17.390055
37.494022	1340.223301	17.395072
37.624580	1353.409242	17.400090
37.225505	1345.558790	17.405107
37.641737	1339.976656	17.410125
37.438824	1343.667291	17.415143
37.661543	1339.631865	17.420160
37.524267	1345.992208	17.425178
37.439857	1345.605842	17.430195
37.696033	1344.892947	17.435213
37.549150	1355.582516	17.440231
37.991910	1362.065878	17.445248
37.990662	1373.434494	17.450266
37.927837	1374.544572	17.455283
37.822497	1376.463591	17.460301
37.831668	1376.202139	17.465319
38.175689	1367.525777	17.470336
37.901247	1369.321018	17.475354
38.077651	1383.522057	17.480371
38.018959	1371.975872	17.485389
37.863198	1381.572781	17.490407
37.995766	1371.736099	17.495424
37.906499	1374.554024	17.500442
37.779755	1379.978626	17.505459
38.201781	1390.550991	17.510477
38.214969	1407.055847	17.515495
38.219340	1402.879084	17.520512
38.412636	1411.621598	17.525530
38.389976	1410.845866	17.530547
38.529295	1396.854452	17.535565
38.182899	1408.266520	17.540583
38.432271	1395.651257	17.545600
38.665043	1393.645395	17.550618
38.472206	1398.847455	17.555635
38.702022	1401.319703	17.560653
38.859553	1420.304008	17.565671
39.014481	1417.344071	17.570688
39.051804	1403.513459	17.575706
38.887513	1395.986543	17.580723
39.252718	1398.206028	17.585741
39.151150	1397.767086	17.590759
39.194235	1394.543230	17.595776
39.243386	1396.031787	17.600794
38.960666	1399.820378	17.605811
39.170883	1386.122359	17.610829
39.154049	1395.857284	17.615847
39.242588	1395.358973	17.620864
39.413949	1390.514149	17.625882
39.152889	1396.802420	17.630899
39.454823	1391.807637	17.635917
39.136519	1399.009354	17.640935
39.213660	1391.170941	17.645952
39.024479	1392.111327	17.650970
39.006595	1405.833048	17.655987
39.301052	1401.140361	17.661005
39.490644	1399.356490	17.666023
39.509092	1397.343668	17.671040
39.459888	1397.789930	17.676058
39.107183	1416.682168	17.681075
39.803088	1427.009155	17.686093
39.675921	1431.633374	17.691111
39.656580	1429.664040	17.696128
40.219549	1427.420046	17.701146
39.752684	1431.178793	17.706163
40.180928	1421.790647	17.711181
40.007689	1412.477284	17.716199
39.945547	1401.204531	17.721216
40.261781	1399.635583	17.726234
40.060992	1395.309727	17.731251
39.838781	1385.085001	17.736269
39.791775	1386.037234	17.741287
39.714020	1395.383353	17.746304
39.785220	1401.021687	17.751322
40.013936	1428.335957	17.756339
40.331328	1427.251109	17.761357
40.185785	1429.352636	17.766375
39.998435	1429.275679	17.771392
39.995099	1431.502052	17.776410
39.886999	1442.876832	17.781427
39.859438	1431.307154	17.786445
40.141483	1430.558714	17.791463
39.758650	1448.911219	17.796480
40.251916	1453.992513	17.801498
40.396994	1460.364340	17.806515
40.795742	1456.514080	17.811533
40.544744	1455.065218	17.816551
40.207837	1451.136737	17.821568
40.523045	1447.448455	17.826586
40.577149	1454.697383	17.831603
40.709572	1451.477491	17.836621
40.565672	1450.769793	17.841639
40.549484	1450.734363	17.846656
40.704600	1468.107560	17.851674
40.649425	1477.121476	17.856691
41.342355	1479.020583	17.861709
41.254468	1476.708234	17.866727
41.176449	1465.197974	17.871744
41.516086	1447.351306	17.876762
41.124330	1444.378390	17.881779
41.183116	1443.735557	17.886797
41.402297	1437.077614	17.891815
41.050480	1442.951105	17.896832
41.480687	1431.871896	17.901850
41.355649	1439.342101	17.906867
41.239648	1439.513567	17.911885
41.317966	1439.801338	17.916903
41.389892	1437.947863	17.921920
41.165655	1432.388491	17.926938
41.302735	1440.170878	17.931955
41.391045	1434.270487	17.936973
41.079389	1440.184340	17.941991
41.351409	1463.258144	17.947008
41.564176	1464.560372	17.952026
41.730520	1475.149464	17.957043
41.857763	1472.746682	17.962061
41.507695	1474.690741	17.967079
41.493453	1473.465879	17.972096
41.670901	1469.309035	17.977114
41.426279	1479.612649	17.982131
41.887854	1475.663808	17.987149
41.853534	1468.581550	17.992167
42.534533	1472.423452	17.997184
42.590438	1467.836219	18.002202
42.426298	1472.701853	18.007219
42.430186	1470.216273	18.012237
42.572444	1472.233812	18.017255
42.378658	1460.008684	18.022272
42.027651	1447.231721	18.027290
41.531653	1451.014761	18.032307
41.956574	1459.932179	18.037325
42.041399	1468.260602	18.042343
41.570929	1473.797325	18.047360
41.990059	1467.836264	18.052378
41.868838	1476.874497	18.057395
42.028754	1487.615896	18.062413
42.266585	1491.375895	18.067431
42.415204	1507.567450	18.072448
42.333477	1498.958500	18.077466
42.099280	1500.016858	18.082483
42.473136	1499.847224	18.087501
42.691921	1506.256832	18.092519
42.575368	1520.846448	18.097536
43.119125	1523.434987	18.102554
42.637450	1528.365318	18.107571
42.806531	1519.626731	18.112589
42.957488	1522.208593	18.117607
43.005726	1525.401830	18.122624
43.017463	1527.964251	18.127642
43.032402	1526.315439	18.132659
42.960184	1528.068545	18.137677
43.291740	1525.028692	18.142695
43.073720	1530.023279	18.147712
42.795791	1522.227960	18.152730
42.823603	1528.401787	18.157747
43.468188	1534.364347	18.162765
43.418837	1532.155237	18.167783
43.576521	1532.536106	18.172800
43.555160	1519.561606	18.177818
43.189207	1531.664592	18.182835
43.214557	1532.939109	18.187853
43.358570	1521.430902	18.192871
43.165461	1527.996581	18.197888
43.353100	1527.419064	18.202906
42.967624	1529.787749	18.207923
43.325588	1545.069735	18.212941
43.216394	1548.030493	18.217959
42.762864	1549.470591	18.222976
43.569524	1542.557924	18.227994
43.986221	1562.664629	18.233011
44.163826	1558.753430	18.238029
44.275706	1546.868782	18.243047
44.245478	1538.059621	18.248064
44.205951	1531.833437	18.253082
44.036654	1541.314248	18.258099
44.080329	1533.842564	18.263117
44.180286	1541.141156	18.268135
43.926346	1538.547785	18.273152
44.415889	1532.028113	18.278170
44.608058	1540.092475	18.283187
44.304314	1533.530841	18.288205
44.684628	1530.295993	18.293223
44.469106	1537.894369	18.298240
44.656059	1539.318758	18.303258
44.335973	1533.863981	18.308275
44.217727	1533.117231	18.313293
44.334532	1529.911420	18.318311
44.408985	1532.862344	18.323328
44.024357	1531.544664	18.328346
44.147713	1538.551024	18.333363
43.935201	1558.690792	18.338381
44.691063	1564.026345	18.343399
44.319413	1567.497116	18.348416
44.740390	1572.653055	18.353434
44.890562	1578.982321	18.358451
44.448809	1579.993583	18.363469
44.953974	1588.802425	18.368487
44.817296	1604.476397	18.373504
45.184852	1590.687437	18.378522
44.820717	1595.075531	18.383539
45.333450	1605.205278	18.388557
45.360687	1594.193076	18.393575
45.389918	1595.820515	18.398592
45.437983	1599.436285	18.403610
45.870223	1597.919879	18.408627
45.662920	1590.506948	18.413645
45.632040	1566.063489	18.418663
45.358913	1570.324149	18.423680
45.358643	1562.311894	18.428698
45.558563	1553.679824	18.433715
45.516767	1562.397762	18.438733
45.567826	1553.008059	18.443751
45.262230	1558.038933	18.448768
45.690581	1570.723557	18.453786
45.556735	1580.667657	18.458803
45.390022	1596.619636	18.463821
45.676479	1589.999311	18.468839
45.092975	1599.294059	18.473856
45.492380	1594.145871	18.478874
45.755977	1582.368664	18.483891
45.767867	1593.809605	18.488909
45.872141	1604.316503	18.493927
45.898803	1619.426206	18.498944
46.102350	1623.359851	18.503962
46.406235	1620.061309	18.508979
46.378343	1621.937548	18.513997
46.312199	1620.078588	18.519015
46.206831	1628.426317	18.524032
46.510242	1621.693218	18.529050
46.483919	1610.162963	18.534067
46.416554	1613.670560	18.539085
46.555615	1623.254081	18.544103
46.623705	1624.659089	18.549120
46.628329	1607.472896	18.554138
46.432890	1602.221158	18.559155
46.474104	1612.382928	18.564173
46.665034	1614.656738	18.569191
46.319946	1618.149740	18.574208
46.706534	1624.914135	18.579226
46.876094	1615.136713	18.584243
46.512190	1619.968918	18.589261
46.720652	1618.053820	18.594279
46.902011	1613.094209	18.599296
46.513729	1613.629324	18.604314
46.604808	1612.645871	18.609331
46.638400	1625.086377	18.614349
47.316580	1630.511658	18.619367
47.018635	1644.563134	18.624384
47.177596	1639.976688	18.629402
47.407754	1636.514780	18.634419
47.418564	1648.314255	18.639437
47.445808	1640.806355	18.644455
47.221246	1638.284711	18.649472
47.348003	1633.907355	18.654490
47.454598	1634.508428	18.659507
47.412615	1639.673284	18.664525
47.860486	1630.461198	18.669543
47.589726	1638.002550	18.674560
47.401762	1640.281869	18.679578
47.597622	1637.325504	18.684595
47.291438	1631.254853	18.689613
47.624326	1640.913434	18.694631
47.532579	1642.686438	18.699648
47.819745	1644.746485	18.704666
47.885122	1631.563692	18.709683
47.798100	1636.726425	18.714701
47.795926	1648.059963	18.719719
47.720454	1665.289429	18.724736
47.922627	1669.708417	18.729754
47.913437	1662.265422	18.734771
47.986742	1672.071295	18.739789
48.278750	1677.026915	18.744807
48.287238	1670.287660	18.749824
48.069762	1666.298092	18.754842
48.262061	1669.056376	18.759859
47.950771	1674.076843	18.764877
48.085693	1661.325066	18.769895
48.425139	1672.717387	18.774912
48.422678	1689.439816	18.779930
48.938631	1689.274956	18.784947
48.805849	1682.419349	18.789965
48.949269	1673.574434	18.794983
48.731478	1661.748584	18.800000
48.879872	1662.946891	18.805018
48.728280	1659.180308	18.810035
48.084741	1667.683722	18.815053
48.656760	1676.862298	18.820071
48.936155	1689.582797	18.825088
48.621648	1693.081991	18.830106
48.849400	1696.464983	18.835123
48.735851	1694.671235	18.840141
48.814514	1690.766730	18.845159
48.795981	1698.118786	18.850176
48.948190	1713.355496	18.855194
49.558384	1715.841723	18.860211
49.301884	1728.941568	18.865229
49.424802	1727.986905	18.870247
49.908675	1729.282837	18.875264
49.675438	1729.032227	18.880282
49.962857	1713.614577	18.885299
49.460558	1699.898272	18.890317
49.255068	1686.055885	18.895335
49.550726	1696.350484	18.900352
49.532849	1715.975531	18.905370
50.217822	1719.756572	18.910387
49.923750	1720.100321	18.915405
49.958937	1712.065766	18.920423
49.997853	1710.367937	18.925440
49.597206	1709.967662	18.930458
50.238343	1710.005776	18.935475
50.064563	1723.233577	18.940493
50.154381	1719.848080	18.945511
50.383187	1718.281098	18.950528
50.130864	1721.535751	18.955546
49.913668	1717.916638	18.960563
49.955113	1715.263537	18.965581
50.113562	1710.978375	18.970599
50.478734	1714.562641	18.975616
49.869278	1715.367203	18.980634
50.095629	1718.958733	18.985651
49.891257	1714.127830	18.990669
50.143865	1724.604259	18.995687
50.167776	1736.851608	19.000704
50.365321	1750.685140	19.005722
50.680568	1744.088952	19.010739
50.673741	1742.175313	19.015757
50.699946	1751.266784	19.020775
50.806878	1742.249324	19.025792
50.677770	1742.610858	19.030810
51.126680	1743.186320	19.035827
50.785709	1738.029968	19.040845
51.039760	1746.640980	19.045863
51.138653	1738.458072	19.050880
50.870446	1744.200002	19.055898
51.056140	1737.632723	19.060915
50.549365	1752.589495	19.065933
50.921302	1763.347102	19.070951
51.463740	1766.696632	19.075968
51.052594	1771.171584	19.080986
51.296362	1778.741730	19.086003
51.076696	1772.469947	19.091021
51.310386	1774.532487	19.096039
51.427496	1769.434612	19.101056
51.308763	1771.815874	19.106074
51.288329	1774.376369	19.111091
51.552844	1788.870976	19.116109
51.820574	1793.859933	19.121127
52.398781	1781.855386	19.126144
51.910512	1784.589019	19.131162
51.965874	1784.185372	19.136179
52.512948	1779.236637	19.141197
52.133326	1762.474858	19.146215
52.605339	1756.660547	19.151232
52.486788	1759.405206	19.156250
52.848007	1751.085965	19.161267
52.282618	1751.117920	19.166285
52.019757	1756.748689	19.171303
52.396277	1752.095378	19.176320
52.322811	1757.971662	19.181338
52.531012	1747.352787	19.186355
52.614125	1751.251594	19.191373
52.140823	1751.925714	19.196391
52.515445	1745.993837	19.201408
52.248322	1747.533503	19.206426
52.501364	1750.484955	19.211443
52.748306	1748.774293	19.216461
52.534950	1748.442706	19.221479
52.879281	1747.492212	19.226496
52.728342	1754.717372	19.231514
52.530502	1747.816584	19.236531
52.724222	1758.660262	19.241549
52.403484	1772.868928	19.246567
52.864149	1770.984203	19.251584
52.511321	1785.066083	19.256602
53.010874	1776.684130	19.261619
53.237194	1778.089980	19.266637
52.788131	1778.955244	19.271655
52.880444	1775.467720	19.276672
53.094000	1800.369199	19.281690
53.258193	1811.678269	19.286707
53.279753	1814.861571	19.291725
53.558766	1814.107334	19.296743
53.512110	1816.121477	19.301760
53.478178	1813.880151	19.306778
53.543241	1812.045135	19.311795
53.537874	1814.951522	19.316813
53.283764	1818.988095	19.321831
53.499413	1808.273795	19.326848
53.249350	1811.932460	19.331866
53.595171	1820.074179	19.336883
54.053181	1833.565059	19.341901
54.159017	1835.800728	19.346919
54.478525	1833.786634	19.351936
54.202161	1836.537888	19.356954
53.969264	1834.004647	19.361971
54.178640	1828.160920	19.366989
53.941652	1841.416589	19.372007
53.736393	1832.330146	19.377024
53.935742	1840.879714	19.382042
54.034003	1830.778907	19.387059
54.306505	1836.534479	19.392077
54.068404	1844.602287	19.397095
54.616065	1852.679887	19.402112
54.504897	1867.890241	19.407130
54.789906	1871.798564	19.412147
54.824740	1866.057593	19.417165
54.930987	1874.225847	19.422183
54.862475	1864.282762	19.427200
54.566650	1861.196453	19.432218
54.899806	1868.233142	19.437235
55.182718	1862.534689	19.442253
54.902001	1872.357285	19.447271
54.913048	1867.176762	19.452288
54.912449	1866.694507	19.457306
54.774841	1857.234593	19.462323
55.060083	1867.503922	19.467341
54.654195	1879.182470	19.472359
55.304475	1881.220063	19.477376
55.283501	1893.388605	19.482394
55.220353	1896.894754	19.487411
55.650059	1885.508580	19.492429
55.456858	1891.873219	19.497447
55.811765	1888.013441	19.502464
56.014672	1881.265963	19.507482
55.863422	1880.328372	19.512499
55.845101	1868.018502	19.517517
55.833904	1874.804744	19.522535
56.367782	1867.331936	19.527552
56.156803	1872.182493	19.532570
55.721495	1857.148883	19.537587
56.261584	1857.687455	19.542605
55.869688	1859.190249	19.547623
55.853568	1857.611696	19.552640
55.866424	1870.307559	19.557658
55.817891	1866.213767	19.562675
56.353341	1863.871271	19.567693
56.358572	1875.973881	19.572711
56.472252	1868.085652	19.577728
56.596890	1867.567750	19.582746
56.353454	1867.891794	19.587763
56.586257	1861.400255	19.592781
56.558708	1867.069470	19.597799
56.827317	1861.628227	19.602816
56.803395	1866.915668	19.607834
56.632762	1862.899117	19.612851
56.682678	1860.039789	19.617869
56.458602	1864.434656	19.622887
56.573917	1858.864558	19.627904
56.695999	1870.052134	19.632922
56.673965	1892.297743	19.637939
57.020057	1891.248501	19.642957
57.318847	1902.733405	19.647975
57.393951	1893.198019	19.652992
57.382855	1892.477768	19.658010
56.906575	1895.245982	19.663027
57.405085	1885.904183	19.668045
57.261096	1899.216407	19.673063
57.319793	1897.118264	19.678080
57.448960	1887.982720	19.683098
57.403343	1899.289238	19.688115
57.449561	1890.366365	19.693133
57.489606	1892.874379	19.698151
57.651771	1896.715176	19.703168
57.953380	1907.285309	19.708186
57.890213	1912.898040	19.713203
58.235256	1915.679793	19.718221
57.979915	1910.702035	19.723239
57.926200	1907.587595	19.728256
58.114779	1912.323197	19.733274
58.223468	1915.995585	19.738291
58.224728	1911.417197	19.743309
58.080259	1915.865368	19.748327
57.932479	1906.950153	19.753344
58.220824	1906.131312	19.758362
58.324621	1914.658322	19.763379
57.943169	1901.768079	19.768397
57.901305	1906.429394	19.773415
58.182962	1918.781534	19.778432
58.937195	1933.875475	19.783450
58.908066	1945.132736	19.788467
58.496359	1942.919543	19.793485
58.764319	1945.018362	19.798503
58.996661	1950.418609	19.803520
59.203562	1939.064689	19.808538
58.745554	1948.185348	19.813555
59.202301	1935.799093	19.818573
59.033801	1942.132743	19.823591
58.987569	1939.026070	19.828608
59.080144	1944.418384	19.833626
59.042103	1937.852762	19.838643
59.152002	1935.854905	19.843661
59.108145	1940.818974	19.848679
59.373570	1938.289661	19.853696
59.353197	1926.371487	19.858714
58.811577	1935.588374	19.863731
59.393206	1948.642751	19.868749
59.390981	1957.817573	19.873767
59.066901	1970.997326	19.878784
59.262917	1965.267665	19.883802
58.927853	1974.152665	19.888819
59.270459	1971.040746	19.893837
59.530817	1992.651387	19.898855
59.941289	1998.756644	19.903872
60.176887	1993.631294	19.908890
59.919985	2003.961770	19.913907
60.158685	1991.899114	19.918925
60.440001	1995.343472	19.923943
60.115515	1993.952438	19.928960
60.616609	1986.464327	19.933978
60.387997	1986.216857	19.938995
60.364796	1990.091820	19.944013
60.457096	1986.310905	19.949031
60.499820	1993.391932	19.954048
60.435104	1990.480570	19.959066
60.489487	1989.645137	19.964083
60.802443	1981.754580	19.969101
60.481556	1987.695026	19.974119
60.885274	2005.794414	19.979136
61.013644	2006.021246	19.984154
61.589403	2014.715065	19.989171
61.491937	1995.413765	19.994189
61.315174	1991.086379	19.999207
60.996333	1979.861943	20.004224
60.902523	1978.834959	20.009242
60.763950	1986.653461	20.014259
61.246653	1993.447609	20.019277
61.026636	2010.384477	20.024295
60.875657	2020.696409	20.029312
60.932362	2006.594188	20.034330
61.026190	2012.645849	20.039347
61.205946	2028.358526	20.044365
61.536755	2042.168681	20.049383
61.690147	2042.364054	20.054400
62.001596	2038.517991	20.059418
61.965261	2038.637216	20.064435
62.013927	2036.076537	20.069453
62.075860	2040.105837	20.074471
62.329446	2042.575296	20.079488
62.360282	2032.185877	20.084506
62.774567	2042.273727	20.089523
62.430187	2016.354754	20.094541
62.231822	2004.957261	20.099559
62.305821	2005.410767	20.104576
62.593655	2003.621405	20.109594
62.201713	2009.486628	20.114611
62.113309	2009.059585	20.119629
62.300411	2017.321153	20.124647
62.228844	2028.784597	20.129664
62.409021	2029.156505	20.134682
62.293289	2041.204775	20.139699
62.262560	2042.739377	20.144717
62.264519	2042.218878	20.149735
61.964546	2056.106873	20.154752
62.877924	2058.821532	20.159770
62.891645	2064.294739	20.164787
63.072786	2064.484567	20.169805
63.207997	2062.501255	20.174823
63.216982	2067.956375	20.179840
63.532300	2057.931610	20.184858
63.139499	2061.100952	20.189875
63.454448	2060.106259	20.194893
63.348318	2058.564775	20.199911
63.223955	2060.513126	20.204928
63.307515	2046.801595	20.209946
63.408681	2079.298255	20.214963
64.027980	2080.375304	20.219981
64.062004	2082.097655	20.224999
64.067335	2078.385967	20.230016
64.267758	2060.871964	20.235034
63.688951	2054.802605	20.240051
63.895250	2049.003031	20.245069
64.036217	2056.680715	20.250087
63.874961	2075.367274	20.255104
64.312583	2070.241126	20.260122
64.451528	2078.585402	20.265139
64.383467	2081.697891	20.270157
64.728934	2078.902435	20.275175
64.357476	2086.491978	20.280192
64.520298	2084.392103	20.285210
64.695421	2079.318438	20.290227
64.812570	2082.006598	20.295245
64.913809	2073.316348	20.300263
64.445212	2066.808738	20.305280
64.843043	2065.871499	20.310298
64.518980	2072.937877	20.315315
64.451296	2077.397735	20.320333
64.351073	2072.339385	20.325351
64.649765	2079.357665	20.330368
64.275690	2087.235100	20.335386
64.587785	2101.757673	20.340403
64.638986	2111.180942	20.345421
64.754114	2106.701496	20.350439
64.856881	2127.023800	20.355456
65.141203	2138.872829	20.360474
65.034346	2139.709366	20.365491
65.120243	2143.875550	20.370509
65.572329	2134.901460	20.375527
65.541843	2143.738667	20.380544
65.672484	2135.575702	20.385562
65.291587	2149.791085	20.390579
65.554138	2167.454167	20.395597
65.700749	2171.217765	20.400615
65.568795	2183.386266	20.405632
65.947767	2176.343082	20.410650
65.769233	2185.082054	20.415667
65.630896	2171.917982	20.420685
66.005760	2171.258336	20.425703
65.836040	2194.774366	20.430720
65.877614	2204.079639	20.435738
66.429071	2200.709001	20.440755
66.749118	2201.430611	20.445773
66.552498	2196.812433	20.450791
66.595121	2207.086176	20.455808
66.589187	2194.228569	20.460826
66.843122	2200.174889	20.465843
66.189035	2199.942084	20.470861
66.903792	2195.301532	20.475879
66.956846	2194.885277	20.480896
66.998412	2205.481295	20.485914
66.678587	2206.440188	20.490931
67.060462	2221.534460	20.495949
67.417368	2221.874893	20.500967
67.092125	2220.172110	20.505984
67.519840	2211.687266	20.511002
67.944023	2206.798059	20.516019
67.817972	2215.934411	20.521037
68.044547	2189.493182	20.526055
68.046782	2191.590736	20.531072
68.262964	2182.494047	20.536090
68.011008	2181.955256	20.541107
67.858777	2188.240539	20.546125
67.643675	2181.573261	20.551143
67.565097	2186.874906	20.556160
67.252155	2188.909943	20.561178
67.635395	2188.192160	20.566195
67.553097	2208.720340	20.571213
67.922189	2204.183938	20.576231
67.932455	2205.302805	20.581248
67.902973	2209.261195	20.586266
68.204426	2207.629735	20.591283
68.224139	2208.180757	20.596301
67.933312	2209.954486	20.601319
68.079427	2237.648562	20.606336
68.563012	2236.585964	20.611354
68.398768	2242.529969	20.616371
68.059346	2246.003630	20.621389
68.438845	2245.202221	20.626407
68.569947	2259.040901	20.631424
68.570213	2266.360075	20.636442
69.039390	2261.713569	20.641459
69.392754	2273.661117	20.646477
69.793343	2274.477600	20.651495
69.634579	2267.962069	20.656512
69.540861	2262.952156	20.661530
69.724055	2246.936404	20.666547
69.317370	2241.710035	20.671565
69.657358	2233.164619	20.676583
69.655621	2230.890544	20.681600
69.641799	2233.979195	20.686618
69.351047	2230.839572	20.691635
69.199608	2244.556576	20.696653
69.236477	2250.121957	20.701671
69.221501	2269.824378	20.706688
69.329019	2265.050871	20.711706
69.675356	2270.064700	20.716723
69.495193	2295.812148	20.721741
69.937938	2293.335069	20.726759
70.221274	2294.384287	20.731776
70.044802	2292.959974	20.736794
70.122893	2291.852702	20.741811
70.282300	2300.210127	20.746829
70.358025	2284.308053	20.751847
70.273829	2295.401358	20.756864
70.216983	2301.339572	20.761882
70.519871	2306.330937	20.766899
70.886242	2306.887105	20.771917
70.647221	2303.528329	20.776935
71.105794	2308.085065	20.781952
71.037522	2314.550522	20.786970
71.159968	2300.747050	20.791987
71.358035	2311.591155	20.797005
71.267326	2301.223184	20.802023
71.230305	2301.738259	20.807040
71.173971	2310.098027	20.812058
71.439886	2297.583551	20.817075
71.196202	2310.078440	20.822093
71.576108	2305.635445	20.827111
71.566887	2297.757046	20.832128
71.506389	2304.113275	20.837146
71.654726	2296.157463	20.842163
71.371440	2305.837440	20.847181
71.665701	2312.874699	20.852199
71.651219	2329.430949	20.857216
71.876777	2329.792328	20.862234
71.967045	2329.737463	20.867251
72.052105	2324.948100	20.872269
72.484488	2316.921528	20.877287
72.392918	2322.083692	20.882304
72.282775	2320.539325	20.887322
72.727127	2314.040076	20.892339
72.288238	2323.549860	20.897357
72.583177	2320.770506	20.902375
72.648943	2317.559504	20.907392
72.570687	2324.766951	20.912410
72.668917	2311.691357	20.917427
72.758237	2324.423699	20.922445
72.630982	2319.074581	20.927463
72.572648	2324.868155	20.932480
72.306384	2325.858823	20.937498
72.616232	2345.567077	20.942515
72.718487	2353.885502	20.947533
72.812209	2351.636783	20.952551
72.883146	2359.452626	20.957568
73.026286	2383.030278	20.962586
73.589879	2380.649021	20.967603
73.419943	2388.976330	20.972621
73.578041	2379.182286	20.977639
73.595346	2385.460632	20.982656
73.726485	2383.904031	20.987674
73.630985	2376.795624	20.992691
73.591082	2381.837907	20.997709
73.764135	2376.397907	21.002727
73.826270	2372.136954	21.007744
73.955719	2372.502212	21.012762
74.140853	2375.292171	21.017779
74.117371	2388.542410	21.022797
74.631210	2409.440378	21.027815
74.338455	2394.617279	21.032832
74.643516	2408.635750	21.037850
74.767663	2395.615495	21.042867
74.389619	2396.047285	21.047885
74.442816	2399.414289	21.052903
74.445453	2397.385937	21.057920
74.139797	2400.512054	21.062938
74.595232	2393.851791	21.067955
74.584205	2404.853876	21.072973
74.467992	2406.270865	21.077991
74.625407	2421.968473	21.083008
74.832298	2431.597565	21.088026
74.826748	2428.386166	21.093043
75.195136	2431.175431	21.098061
75.376997	2429.816463	21.103079
75.391987	2423.138772	21.108096
75.038922	2443.424657	21.113114
75.723495	2456.601600	21.118131
75.656467	2462.937750	21.123149
75.799286	2475.178285	21.128167
76.037895	2468.241727	21.133184
76.044542	2461.734770	21.138202
76.242485	2456.951214	21.143219
75.782088	2464.826704	21.148237
75.651846	2457.766743	21.153255
76.076394	2463.863471	21.158272
75.663758	2471.944984	21.163290
75.886127	2466.116120	21.168307
76.177406	2486.316005	21.173325
76.180888	2487.163569	21.178343
76.572402	2488.486430	21.183360
76.901533	2491.458057	21.188378
76.863730	2477.970928	21.193395
76.704118	2491.911633	21.198413
76.871611	2493.461910	21.203431
76.692745	2492.456956	21.208448
76.411485	2495.698614	21.213466
76.958532	2489.150186	21.218483
76.883974	2484.996904	21.223501
77.019032	2489.335884	21.228519
77.299755	2500.274629	21.233536
77.269411	2510.654010	21.238554
77.330308	2504.273190	21.243571
77.661523	2512.561109	21.248589
77.774944	2504.446583	21.253607
78.000944	2497.916967	21.258624
77.878009	2500.722751	21.263642
77.551761	2494.917056	21.268659
77.848501	2497.895025	21.273677
78.190438	2506.243318	21.278695
77.884201	2493.934671	21.283712
78.041210	2509.294585	21.288730
78.220350	2500.073333	21.293747
77.774952	2512.708494	21.298765
77.877658	2506.602443	21.303783
78.232643	2495.021519	21.308800
77.930609	2501.281420	21.313818
78.238685	2516.976132	21.318835
78.769105	2519.964444	21.323853
78.288716	2531.106153	21.328871
78.718902	2527.871219	21.333888
78.463007	2530.400541	21.338906
78.808616	2524.875778	21.343923
78.433778	2528.587894	21.348941
78.487375	2542.380260	21.353959
78.816511	2549.027330	21.358976
78.839947	2560.562290	21.363994
78.757549	2568.766006	21.369011
79.364471	2579.250387	21.374029
79.288027	2585.464557	21.379047
79.566945	2588.436148	21.384064
79.745232	2589.461659	21.389082
80.060315	2584.794226	21.394099
80.222761	2576.732686	21.399117
80.258582	2578.455178	21.404135
80.349963	2568.410204	21.409152
80.283871	2559.419183	21.414170
80.145516	2539.389057	21.419187
80.268841	2538.970195	21.424205
80.607018	2533.681390	21.429223
80.416390	2535.945936	21.434240
80.075863	2536.901308	21.439258
80.416105	2537.753355	21.444275
80.411970	2553.499268	21.449293
80.370023	2571.066954	21.454311
80.949578	2569.154669	21.459328
80.529711	2567.074300	21.464346
80.771594	2570.852375	21.469363
80.331776	2574.223613	21.474381
80.346862	2570.118729	21.479399
80.678045	2578.623262	21.484416
80.532390	2602.104274	21.489434
81.045684	2595.883693	21.494451
81.110544	2599.486578	21.499469
80.719494	2598.982642	21.504487
81.103144	2597.369341	21.509504
81.474614	2620.286836	21.514522
81.461962	2630.874325	21.519539
82.067244	2627.551861	21.524557
81.658855	2635.411430	21.529575
82.150319	2624.226773	21.534592
81.993983	2624.085818	21.539610
82.178864	2622.796406	21.544627
82.145592	2621.944467	21.549645
81.597674	2628.927008	21.554663
82.084052	2622.410978	21.559680
82.124833	2633.723295	21.564698
81.932831	2631.673155	21.569715
82.161645	2633.034948	21.574733
82.480691	2647.147316	21.579751
82.341977	2658.030500	21.584768
82.557674	2661.524846	21.589786
82.158084	2660.687668	21.594803
82.507788	2660.478855	21.599821
82.434718	2676.125666	21.604839
82.555284	2672.536626	21.609856
83.010131	2684.225315	21.614874
83.624470	2680.617773	21.619891
83.461228	2684.224344	21.624909
83.434222	2684.268338	21.629927
83.332538	2682.364941	21.634944
83.637997	2679.979856	21.639962
83.393559	2679.846129	21.644979
83.435004	2673.048027	21.649997
83.275962	2700.184105	21.655015
83.390622	2697.710447	21.660032
83.712370	2699.579243	21.665050
83.838121	2706.838519	21.670067
83.652176	2704.719602	21.675085
83.708768	2729.322245	21.680103
83.928795	2732.813503	21.685120
84.042434	2741.318406	21.690138
84.229228	2738.094444	21.695155
84.294898	2737.914638	21.700173
84.445049	2753.283842	21.705191
84.850383	2759.272937	21.710208
84.612913	2756.570610	21.715226
84.684193	2756.362278	21.720243
84.948461	2759.323814	21.725261
85.012311	2759.503441	21.730279
85.044579	2757.659761	21.735296
85.388631	2757.230616	21.740314
85.050783	2756.989257	21.745331
85.181219	2753.794643	21.750349
85.300264	2757.947433	21.755367
85.234873	2749.330267	21.760384
85.266639	2757.038830	21.765402
85.366363	2776.877370	21.770419
85.568144	2773.327149	21.775437
85.787342	2786.870826	21.780455
86.031254	2780.712108	21.785472
85.967487	2783.061259	21.790490
85.913818	2785.457507	21.795507
86.439674	2781.489451	21.800525
86.158623	2783.430889	21.805543
85.811869	2776.538637	21.810560
86.493646	2783.467145	21.815578
86.001224	2784.353279	21.820595
86.144963	2799.047911	21.825613
86.239173	2808.539043	21.830631
86.558399	2813.279692	21.835648
86.936406	2818.478857	21.840666
86.712081	2817.914827	21.845683
87.231551	2810.518867	21.850701
86.966499	2813.794038	21.855719
86.887842	2815.204624	21.860736
87.516207	2825.215328	21.865754
87.378317	2834.684839	21.870771
87.306151	2836.970859	21.875789
87.503633	2841.536288	21.880807
87.524344	2838.980272	21.885824
87.612196	2847.555021	21.890842
87.224720	2852.003376	21.895859
87.603629	2847.684835	21.900877
86.822182	2851.027281	21.905895
87.252002	2864.207294	21.910912
87.561645	2871.480009	21.915930
87.386537	2889.861583	21.920947
87.612267	2904.381596	21.925965
87.683053	2911.317254	21.930983
87.887918	2921.483319	21.936000
88.390998	2933.330887	21.941018
88.323390	2947.412945	21.946035
88.336507	2944.373866	21.951053
88.059624	2948.946623	21.956071
88.340622	2957.739548	21.961088
88.804941	2966.771183	21.966106
88.815425	2973.795963	21.971123
88.892073	2968.494359	21.976141
88.956251	2974.415229	21.981159
89.194714	2974.440488	21.986176
89.222584	2979.740689	21.991194
89.232163	2999.966692	21.996211
89.334617	3001.605351	22.001229
89.169960	3002.071451	22.006247
89.683708	2998.720503	22.011264
90.349109	3004.587138	22.016282
89.771899	3008.111967	22.021299
90.258944	2992.787608	22.026317
90.030254	3002.189305	22.031335
90.219620	2999.873693	22.036352
89.932230	2995.103877	22.041370
90.509796	2999.771153	22.046387
90.153231	2989.665672	22.051405
90.319720	3008.585003	22.056423
90.678344	3015.507587	22.061440
90.959967	3030.555250	22.066458
90.538646	3028.401035	22.071475
90.680882	3023.639461	22.076493
90.701125	3022.911423	22.081511
90.798927	3022.329174	22.086528
91.212434	3013.879417	22.091546
91.037695	3015.871962	22.096563
91.431532	3008.931395	22.101581
91.245713	3015.879590	22.106599
91.211867	3016.854079	22.111616
91.659583	3022.597379	22.116634
91.394677	3041.148886	22.121651
91.693961	3037.270804	22.126669
91.878588	3029.989641	22.131687
91.502532	3034.864521	22.136704
91.907773	3033.506584	22.141722
91.925971	3037.475909	22.146739
91.778083	3037.948585	22.151757
91.862695	3052.875683	22.156775
92.031402	3071.953010	22.161792
92.215961	3064.775013	22.166810
92.244520	3065.835676	22.171827
92.557511	3067.568983	22.176845
92.155230	3074.928407	22.181863
92.433201	3086.400426	22.186880
92.537415	3092.090809	22.191898
92.802736	3102.267103	22.196915
93.039645	3093.785363	22.201933
92.799535	3101.620249	22.206951
93.083506	3121.268548	22.211968
93.303588	3124.054226	22.216986
93.667371	3119.974475	22.222003
93.642272	3118.725749	22.227021
93.696405	3130.595306	22.232039
94.116738	3127.321776	22.237056
94.553967	3116.513865	22.242074
94.308816	3126.068095	22.247091
94.396668	3112.428931	22.252109
94.660225	3105.779216	22.257127
94.303439	3096.794408	22.262144
94.699694	3076.129311	22.267162
94.205776	3083.402066	22.272179
94.503500	3076.941034	22.277197
94.335970	3090.545762	22.282215
94.329781	3099.172211	22.287232
94.993568	3107.831865	22.292250
94.794142	3110.772944	22.297267
94.633528	3111.659700	22.302285
95.030302	3109.234483	22.307303
94.780679	3112.294427	22.312320
95.017863	3107.076301	22.317338
95.051449	3110.911483	22.322355
94.960938	3110.614325	22.327373
95.655749	3117.673060	22.332391
94.937208	3132.917492	22.337408
95.060278	3134.499865	22.342426
95.120624	3135.837819	22.347443
95.006026	3144.219044	22.352461
95.200433	3144.985082	22.357479
95.249231	3163.341189	22.362496
95.559469	3163.819597	22.367514
95.829189	3186.203280	22.372531
96.061347	3190.520295	22.377549
95.995461	3189.202163	22.382567
96.370505	3191.568289	22.387584
96.420795	3186.560957	22.392602
96.641947	3211.872519	22.397619
96.637853	3218.444692	22.402637
96.888632	3222.688431	22.407655
96.698089	3223.356654	22.412672
96.999308	3213.205201	22.417690
96.979789	3221.085811	22.422707
97.192962	3218.361275	22.427725
97.663995	3201.750995	22.432743
97.348263	3220.879264	22.437760
97.127743	3217.888063	22.442778
97.465330	3239.122147	22.447795
97.527708	3241.380433	22.452813
98.081814	3248.379080	22.457831
97.752436	3247.096665	22.462848
97.653965	3248.945426	22.467866
97.318595	3246.351155	22.472883
97.653755	3266.627218	22.477901
97.663491	3270.629555	22.482919
97.791154	3283.480538	22.487936
98.067373	3289.947191	22.492954
98.170619	3305.102881	22.497971
98.323949	3310.879431	22.502989
98.462875	3308.104602	22.508007
98.672142	3316.736762	22.513024
99.084487	3331.979673	22.518042
99.965610	3324.877459	22.523059
99.829181	3315.331797	22.528077
99.707429	3303.692614	22.533095
100.010461	3308.866206	22.538112
99.983130	3305.243311	22.543130
100.024292	3300.159538	22.548147
99.456585	3296.589120	22.553165
99.849174	3290.609484	22.558183
99.618417	3303.603051	22.563200
99.810823	3292.221110	22.568218
100.065751	3294.021890	22.573235
99.642141	3299.299578	22.578253
99.699214	3289.771950	22.583271
99.821158	3303.776150	22.588288
100.088766	3322.655684	22.593306
100.129103	3325.536007	22.598323
99.959797	3328.234902	22.603341
100.539162	3323.195102	22.608359
100.109451	3349.224902	22.613376
100.316489	3358.040184	22.618394
100.803530	3360.832905	22.623411
100.331936	3361.111424	22.628429
101.035203	3371.221476	22.633447
100.741381	3391.834718	22.638464
100.994241	3379.665009	22.643482
101.281646	3384.379785	22.648499
101.395563	3386.248068	22.653517
101.762239	3400.832585	22.658535
101.498667	3416.698659	22.663552
101.830117	3420.227675	22.668570
102.042779	3423.562836	22.673587
101.779462	3425.773025	22.678605
101.946425	3414.734016	22.683623
101.848791	3420.266953	22.688640
101.981636	3424.472685	22.693658
102.092300	3440.703068	22.698675
102.266201	3445.852377	22.703693
102.585196	3449.869473	22.708711
102.524053	3454.788940	22.713728
102.502989	3449.022714	22.718746
102.747329	3470.388871	22.723763
102.832914	3477.455344	22.728781
103.408766	3472.476744	22.733799
103.152961	3479.609621	22.738816
103.158270	3474.333467	22.743834
103.239901	3471.403828	22.748851
102.978935	3484.436588	22.753869
103.741631	3496.607090	22.758887
103.575267	3506.671785	22.763904
103.325008	3510.517923	22.768922
103.582735	3508.724500	22.773939
104.206689	3523.276838	22.778957
104.057295	3528.892719	22.783975
104.142993	3539.626987	22.788992
104.563617	3530.675619	22.794010
104.820487	3531.463260	22.799027
104.452076	3527.429386	22.804045
104.909747	3517.024092	22.809063
104.760994	3523.428235	22.814080
104.792198	3520.323724	22.819098
104.855192	3528.206881	22.824115
104.622394	3525.736744	22.829133
105.075515	3539.173234	22.834151
104.906373	3557.443512	22.839168
105.036374	3557.648825	22.844186
105.585992	3557.416759	22.849203
105.299226	3569.087549	22.854221
105.549246	3561.390898	22.859239
105.660960	3560.366772	22.864256
105.888865	3579.302250	22.869274
105.944750	3579.571463	22.874291
106.016274	3580.606681	22.879309
106.807765	3564.676690	22.884327
106.113718	3574.074234	22.889344
106.522036	3573.223721	22.894362
106.829305	3563.363990	22.899379
106.420850	3559.402343	22.904397
106.723123	3558.870868	22.909415
106.800908	3562.089778	22.914432
106.693332	3559.660387	22.919450
107.077055	3553.709740	22.924467
107.244851	3552.608267	22.929485
107.234931	3548.502690	22.934503
107.577650	3561.993569	22.939520
107.575430	3578.356860	22.944538
107.458652	3582.193520	22.949555
107.670241	3586.525986	22.954573
107.605817	3586.981218	22.959591
107.769621	3584.735274	22.964608
107.461876	3585.339333	22.969626
107.619878	3583.570875	22.974643
107.888333	3600.226447	22.979661
108.531482	3602.985362	22.984679
108.725764	3610.039560	22.989696
108.705911	3607.714049	22.994714
108.798257	3604.701426	22.999731
108.417035	3605.996197	23.004749
108.742295	3607.252547	23.009767
108.973934	3606.148789	23.014784
108.880902	3603.104941	23.019802
109.116217	3591.954854	23.024819
109.204013	3620.778169	23.029837
109.434048	3632.338353	23.034855
109.174254	3637.667614	23.039872
109.494918	3637.255849	23.044890
109.577506	3638.796382	23.049907
109.409109	3640.103500	23.054925
109.711152	3641.047221	23.059943
109.789102	3661.766411	23.064960
110.068895	3669.723522	23.069978
110.107823	3663.231011	23.074995
109.934670	3673.502538	23.080013
109.949835	3670.878029	23.085031
110.085924	3685.527545	23.090048
110.611265	3699.560602	23.095066
110.886257	3692.250254	23.100083
110.655042	3695.523740	23.105101
110.619157	3691.267422	23.110119
111.155713	3694.706207	23.115136
110.956594	3696.832180	23.120154
111.577154	3709.532853	23.125171
111.535395	3715.295742	23.130189
111.596466	3716.024811	23.135207
111.687483	3725.260289	23.140224
111.819375	3725.006112	23.145242
111.926048	3715.635906	23.150259
111.711512	3716.498860	23.155277
111.856898	3717.702571	23.160295
112.239713	3711.707128	23.165312
112.072266	3715.247707	23.170330
112.305622	3711.230335	23.175347
112.606428	3718.211976	23.180365
112.716616	3718.546703	23.185383
112.272540	3714.974681	23.190400
112.019118	3736.065029	23.195418
112.590339	3742.945978	23.200435
112.401407	3749.461062	23.205453
112.615103	3756.685269	23.210471
113.056102	3773.652474	23.215488
113.167451	3778.463711	23.220506
113.411471	3773.799452	23.225523
113.764819	3773.444301	23.230541
113.527332	3775.661923	23.235559
113.945561	3795.156519	23.240576
113.783787	3804.648820	23.245594
114.220399	3794.691162	23.250611
114.067917	3796.500414	23.255629
114.071210	3798.275085	23.260647
114.116502	3807.243578	23.265664
114.173208	3815.387076	23.270682
114.666708	3807.493408	23.275699
114.493010	3832.972899	23.280717
114.909838	3829.491903	23.285735
114.810183	3833.279220	23.290752
114.753283	3839.437763	23.295770
114.560050	3825.126305	23.300787
114.467731	3844.978636	23.305805
114.472307	3859.839097	23.310823
115.306866	3862.332903	23.315840
115.542164	3870.729350	23.320858
116.543517	3869.295142	23.325875
116.096379	3869.228441	23.330893
116.397094	3860.050926	23.335911
116.431946	3848.705047	23.340928
116.305418	3851.637702	23.345946
116.544522	3845.154117	23.350963
116.736512	3857.934683	23.355981
116.548169	3861.311118	23.360999
117.149389	3856.019312	23.366016
116.935480	3862.797846	23.371034
116.896688	3857.028997	23.376051
117.021414	3859.803589	23.381069
117.211526	3865.676427	23.386087
117.293828	3861.259608	23.391104
117.203596	3863.559111	23.396122
117.455030	3860.941322	23.401139
117.292047	3857.710152	23.406157
117.173888	3864.910179	23.411175
117.279044	3865.997933	23.416192
117.258864	3884.951107	23.421210
117.660099	3887.998068	23.426227
117.598236	3889.523222	23.431245
117.736882	3901.267819	23.436263
118.050689	3910.790492	23.441280
118.302144	3919.813492	23.446298
117.986213	3921.280605	23.451315
118.279411	3925.256566	23.456333
118.346039	3953.064167	23.461351
118.691050	3957.200589	23.466368
118.969201	3961.113768	23.471386
118.768670	3954.013202	23.476403
118.692090	3955.932326	23.481421
118.591071	3970.417979	23.486439
119.155413	3975.443819	23.491456
119.047184	3989.981132	23.496474
119.332375	4004.332083	23.501491
119.813794	4001.815038	23.506509
119.838462	4000.623870	23.511527
120.154132	4004.611751	23.516544
120.192310	4010.931273	23.521562
120.380840	3998.900498	23.526579
120.071424	4008.718311	23.531597
120.305272	4031.472435	23.536615
120.715366	4030.381374	23.541632
120.685122	4035.322503	23.546650
120.766211	4036.425422	23.551667
120.626211	4030.984966	23.556685
120.753484	4055.805971	23.561703
121.103122	4060.136167	23.566720
121.128627	4068.708881	23.571738
121.232699	4058.332350	23.576755
121.305619	4066.535420	23.581773
121.269189	4090.763117	23.586791
121.484928	4080.358764	23.591808
121.403441	4097.065403	23.596826
121.750156	4113.340287	23.601843
122.044059	4124.733148	23.606861
121.927099	4130.110548	23.611879
122.365036	4127.770275	23.616896
122.569413	4129.467192	23.621914
122.694755	4144.266261	23.626931
122.604435	4149.892712	23.631949
122.492889	4158.898530	23.636967
122.986550	4143.444336	23.641984
123.410401	4145.502162	23.647002
123.452977	4136.365592	23.652019
123.737694	4130.980672	23.657037
123.752817	4128.741238	23.662055
124.077031	4126.351152	23.667072
124.142265	4133.250495	23.672090
124.394316	4125.876146	23.677107
124.628106	4120.266826	23.682125
124.336821	4124.985733	23.687143
124.310605	4115.189132	23.692160
124.352982	4121.064552	23.697178
124.224527	4118.273987	23.702195
124.445248	4126.068969	23.707213
124.665855	4152.906174	23.712231
124.739717	4149.610713	23.717248
124.678303	4160.206012	23.722266
124.523097	4164.369173	23.727283
124.872651	4162.282696	23.732301
124.704957	4185.845452	23.737319
124.816319	4188.091539	23.742336
124.905651	4197.173996	23.747354
125.030687	4223.950519	23.752371
124.876396	4222.730155	23.757389
125.164461	4233.381370	23.762407
125.380208	4249.994683	23.767424
125.625699	4262.795548	23.772442
126.182954	4282.753665	23.777459
126.380791	4290.208460	23.782477
126.339982	4295.486222	23.787495
127.013321	4282.190684	23.792512
127.139511	4273.324820	23.797530
126.985907	4278.413980	23.802547
127.528207	4264.115436	23.807565
127.308635	4270.179953	23.812583
127.620467	4264.654869	23.817600
127.719717	4263.349291	23.822618
128.017461	4264.619865	23.827635
128.192653	4261.618120	23.832653
128.119438	4258.432914	23.837671
128.009770	4261.710094	23.842688
128.191926	4267.024447	23.847706
128.168466	4279.593403	23.852723
128.244158	4293.994711	23.857741
128.010786	4304.658179	23.862759
128.680816	4286.951721	23.867776
129.247010	4281.707526	23.872794
129.618815	4278.540538	23.877811
129.873619	4277.239798	23.882829
129.437508	4278.160456	23.887847
129.482868	4271.363358	23.892864
129.645288	4270.926726	23.897882
129.378596	4263.155280	23.902899
129.829100	4263.390722	23.907917
129.578485	4275.231472	23.912935
129.643099	4270.122100	23.917952
129.771470	4272.825255	23.922970
129.506608	4277.311267	23.927987
130.178862	4285.025770	23.933005
130.073718	4296.157152	23.938023
130.202695	4291.706220	23.943040
130.162695	4307.589203	23.948058
130.426075	4332.791362	23.953075
131.278207	4326.366315	23.958093
130.638872	4328.990006	23.963111
130.618707	4329.689711	23.968128
131.023899	4332.065813	23.973146
130.838860	4348.802285	23.978163
131.213771	4356.285040	23.983181
131.248903	4361.947556	23.988199
131.392714	4368.920171	23.993216
131.746662	4368.191572	23.998234
131.938861	4379.402785	24.003251
132.399135	4366.284689	24.008269
132.268312	4371.229776	24.013287
132.520241	4368.533845	24.018304
132.867983	4367.938631	24.023322
132.676341	4368.612601	24.028339
132.724784	4373.133931	24.033357
132.852143	4380.891486	24.038375
132.806550	4391.177053	24.043392
132.910837	4399.033875	24.048410
132.854647	4404.748294	24.053427
133.400306	4394.981077	24.058445
133.470868	4392.374519	24.063463
133.524773	4409.409560	24.068480
133.673466	4419.702007	24.073498
133.586472	4425.397297	24.078515
134.086405	4414.079187	24.083533
134.234612	4421.110932	24.088551
133.926745	4421.668569	24.093568
134.511575	4442.742174	24.098586
134.619079	4453.560753	24.103603
134.907712	4449.465983	24.108621
134.373472	4455.455343	24.113639
134.429750	4454.982555	24.118656
134.623777	4473.502746	24.123674
134.991953	4475.851348	24.128691
135.162206	4482.422514	24.133709
135.214182	4505.739365	24.138727
135.513845	4511.797661	24.143744
135.617439	4507.915754	24.148762
135.593791	4520.768482	24.153779
135.515882	4529.485983	24.158797
135.377765	4537.483673	24.163815
135.855918	4551.498803	24.168832
136.176923	4565.837826	24.173850
136.197568	4578.420724	24.178867
136.164143	4571.707891	24.183885
136.242124	4597.838587	24.188903
136.898939	4610.436110	24.193920
137.648015	4604.138891	24.198938
137.355470	4605.297238	24.203955
137.548259	4599.313561	24.208973
137.329949	4610.162898	24.213991
137.521889	4624.655636	24.219008
137.532023	4623.262126	24.224026
137.546506	4631.429824	24.229043
138.013468	4606.920318	24.234061
138.721474	4612.646367	24.239079
138.773234	4608.628396	24.244096
139.193282	4603.715542	24.249114
138.987170	4610.952251	24.254131
139.088222	4613.642033	24.259149
138.945367	4612.663845	24.264167
138.824419	4605.518622	24.269184
139.306115	4603.304680	24.274202
139.305056	4625.906172	24.279219
139.507535	4626.512588	24.284237
139.619778	4639.910005	24.289255
139.460694	4642.093038	24.294272
139.676735	4632.705117	24.299290
139.543330	4643.313080	24.304307
139.498795	4649.434374	24.309325
139.493947	4666.583733	24.314343
140.071215	4674.998387	24.319360
139.980177	4684.896538	24.324378
140.138332	4699.891352	24.329395
140.450282	4699.020287	24.334413
140.813719	4718.962564	24.339431
141.068022	4731.240091	24.344448
140.961413	4730.509304	24.349466
141.222163	4738.295364	24.354483
141.182876	4738.384002	24.359501
141.482476	4752.708748	24.364519
141.398239	4759.497727	24.369536
141.590628	4761.004583	24.374554
141.540963	4774.257374	24.379571
141.813649	4787.626624	24.384589
142.466438	4801.241845	24.389607
142.011405	4804.557076	24.394624
142.489893	4802.900526	24.399642
142.510172	4819.877973	24.404659
142.573150	4824.769498	24.409677
142.889217	4824.223809	24.414695
142.863684	4832.096800	24.419712
143.512740	4839.220092	24.424730
143.246617	4856.779129	24.429747
143.346324	4846.319339	24.434765
143.533809	4843.424074	24.439783
143.627180	4869.109919	24.444800
144.037971	4868.807128	24.449818
143.881245	4873.647327	24.454835
144.188938	4876.038653	24.459853
144.161436	4884.495659	24.464871
144.764145	4901.081915	24.469888
145.269212	4888.591349	24.474906
145.049003	4905.181631	24.479923
145.066290	4901.745271	24.484941
145.008694	4895.512188	24.489959
144.987812	4899.056259	24.494976
145.608924	4913.989239	24.499994
145.088333	4923.553960	24.505011
145.433473	4922.622058	24.510029
145.811969	4926.000788	24.515047
145.778785	4927.874783	24.520064
145.909005	4931.154298	24.525082
145.553766	4957.719025	24.530099
146.185085	4961.029217	24.535117
146.438860	4963.723595	24.540135
146.277698	4973.362993	24.545152
146.566355	4984.614024	24.550170
146.703453	4988.665852	24.555187
146.700663	4991.981572	24.560205
146.798357	5007.123307	24.565223
146.820334	5033.042201	24.570240
147.052455	5035.285824	24.575258
147.494928	5049.518608	24.580275
147.261122	5052.804629	24.585293
147.949364	5058.472007	24.590311
147.555148	5083.798332	24.595328
147.752000	5083.190367	24.600346
147.629407	5094.997964	24.605363
147.822141	5120.138660	24.610381
148.093923	5126.098789	24.615399
148.155341	5150.468865	24.620416
148.479276	5158.966591	24.625434
149.038245	5168.927687	24.630451
149.228021	5185.599997	24.635469
149.079573	5190.044252	24.640487
149.169752	5194.825680	24.645504
149.398154	5203.507582	24.650522
149.956565	5223.114605	24.655539
149.954913	5222.788780	24.660557
150.491845	5225.526820	24.665575
150.453994	5218.000022	24.670592
150.979542	5214.960093	24.675610
150.905595	5220.384835	24.680627
151.130404	5223.319737	24.685645
151.234851	5223.275827	24.690663
151.328551	5242.074834	24.695680
151.452421	5239.948931	24.700698
151.276069	5244.930449	24.705715
151.590846	5236.448397	24.710733
151.623442	5233.326772	24.715751
151.664903	5244.278515	24.720768
152.126569	5253.919223	24.725786
151.965242	5263.160262	24.730803
151.985849	5269.727477	24.735821
152.453816	5270.301798	24.740839
152.203426	5283.672129	24.745856
152.673854	5284.357090	24.750874
152.792399	5290.779134	24.755891
152.596144	5289.133446	24.760909
152.833091	5314.781221	24.765927
152.834209	5329.767319	24.770944
153.243156	5323.656521	24.775962
153.391717	5335.616307	24.780979
153.279860	5351.782038	24.785997
153.598193	5360.307615	24.791015
153.696880	5365.954869	24.796032
153.894569	5379.121652	24.801050
154.067441	5391.828757	24.806067
154.031704	5400.128337	24.811085
154.468460	5404.180890	24.816103
154.417196	5411.217338	24.821120
154.777877	5422.429552	24.826138
154.871952	5420.353629	24.831155
155.097080	5424.733120	24.836173
155.429280	5443.597817	24.841191
155.318427	5452.961856	24.846208
155.660095	5452.043912	24.851226
155.860842	5450.986288	24.856243
155.876360	5465.105170	24.861261
156.037233	5471.528696	24.866279
156.250941	5480.099054	24.871296
156.533581	5481.462117	24.876314
157.147545	5480.744825	24.881331
156.805122	5488.017900	24.886349
156.991870	5504.334244	24.891367
156.926910	5515.168935	24.896384
156.485357	5507.277191	24.901402
156.709216	5522.697897	24.906419
157.168482	5540.633514	24.911437
157.565777	5538.280319	24.916455
157.610592	5566.381994	24.921472
157.839244	5569.105991	24.926490
157.880661	5571.972361	24.931507
157.772526	5584.732519	24.936525
158.192730	5596.127635	24.941543
158.797574	5597.242490	24.946560
158.482670	5603.916196	24.951578
159.180755	5622.406459	24.956595
159.165536	5628.882290	24.961613
159.143370	5631.969097	24.966631
159.370849	5644.789923	24.971648
159.504174	5650.097360	24.976666
159.717230	5654.386036	24.981683
159.449886	5664.001517	24.986701
159.945133	5668.533268	24.991719
159.961386	5690.974980	24.996736
160.343634	5696.076708	25.001754
160.389673	5695.299227	25.006771
160.181951	5704.776118	25.011789
161.035051	5717.262899	25.016807
160.848559	5723.360104	25.021824
160.902609	5717.320236	25.026842
161.361858	5737.857835	25.031859
161.557955	5750.573849	25.036877
161.652650	5742.125320	25.041895
161.738188	5748.031753	25.046912
162.003352	5749.659350	25.051930
162.088197	5750.537253	25.056947
161.949390	5774.422729	25.061965
162.195001	5778.649144	25.066983
162.104278	5771.260330	25.072000
162.175275	5793.441526	25.077018
162.691595	5799.161490	25.082035
162.489323	5818.609780	25.087053
162.735449	5821.096878	25.092071
163.375945	5830.750606	25.097088
163.470052	5831.191327	25.102106
163.737090	5832.223111	25.107123
163.813641	5851.107699	25.112141
164.461948	5849.573175	25.117159
164.364157	5849.214981	25.122176
164.610428	5855.644503	25.127194
164.899856	5852.660688	25.132211
164.871511	5859.991944	25.137229
164.934284	5856.411308	25.142247
164.934193	5855.319557	25.147264
164.785414	5877.036780	25.152282
164.811929	5875.296126	25.157299
164.922037	5893.876474	25.162317
165.408929	5914.290619	25.167335
165.238195	5926.411137	25.172352
165.547629	5946.375245	25.177370
165.774206	5954.658504	25.182387
165.808986	5966.783208	25.187405
166.343223	5984.558387	25.192423
166.361683	5991.023079	25.197440
166.446458	5996.489406	25.202458
167.009860	6010.061130	25.207475
167.077552	6024.459866	25.212493
167.435311	6008.633313	25.217511
167.654689	6008.156152	25.222528
167.625883	6031.218905	25.227546
168.237067	6030.617076	25.232563
168.486606	6026.985480	25.237581
168.669521	6031.057292	25.242599
169.066148	6025.438297	25.247616
169.111990	6018.564751	25.252634
169.452984	6009.754048	25.257651
169.546632	6011.056607	25.262669
169.873281	6007.988400	25.267687
169.971064	6000.145740	25.272704
169.805610	5989.545545	25.277722
169.895609	5975.743647	25.282739
170.265298	5980.396264	25.287757
170.181909	5990.358507	25.292775
170.357337	5992.822305	25.297792
170.315794	6003.675370	25.302810
170.801283	5997.450370	25.307827
170.378877	5994.239600	25.312845
170.245827	5984.122233	25.317863
170.686456	6000.124594	25.322880
170.792166	6026.814523	25.327898
171.100375	6020.500960	25.332915
170.769792	6035.382315	25.337933
170.667451	6049.268277	25.342951
171.405206	6050.913357	25.347968
171.348199	6062.006213	25.352986
171.237031	6079.189499	25.358003
171.458341	6094.344950	25.363021
171.731521	6105.922393	25.368039
172.029257	6116.439311	25.373056
171.898538	6131.577948	25.378074
172.300439	6140.849765	25.383091
172.400748	6148.055909	25.388109
172.831163	6173.944455	25.393127
173.053541	6186.524764	25.398144
173.260079	6197.836422	25.403162
173.790648	6195.614680	25.408179
174.046555	6206.178214	25.413197
174.045164	6209.934282	25.418215
174.026739	6211.189901	25.423232
174.008730	6210.855044	25.428250
174.547395	6217.162908	25.433267
174.390957	6233.679833	25.438285
174.850475	6230.836151	25.443303
175.382732	6242.217252	25.448320
175.076214	6251.972926	25.453338
175.594214	6254.088947	25.458355
175.433956	6259.438250	25.463373
175.579794	6257.161930	25.468391
176.074921	6273.462436	25.473408
175.981615	6285.970904	25.478426
176.340702	6279.196366	25.483443
176.450625	6297.749647	25.488461
176.164221	6296.220133	25.493479
176.445288	6305.775073	25.498496
176.844968	6321.468113	25.503514
176.877910	6336.222837	25.508531
177.128383	6340.951926	25.513549
177.650655	6347.799882	25.518567
177.832742	6342.745331	25.523584
177.631761	6365.329211	25.528602
178.235138	6371.171526	25.533619
178.256421	6380.240116	25.538637
178.249758	6380.467323	25.543655
178.595193	6395.185076	25.548672
178.573740	6403.907315	25.553690
178.621964	6416.779974	25.558707
178.555965	6424.539379	25.563725
179.284425	6445.117607	25.568743
179.295496	6450.465963	25.573760
179.393530	6457.444982	25.578778
179.981250	6471.984995	25.583795
180.087099	6479.921354	25.588813
179.888140	6484.402983	25.593831
180.094510	6485.425518	25.598848
180.205106	6508.560380	25.603866
180.327216	6510.092058	25.608883
180.225360	6518.757247	25.613901
180.470737	6540.811912	25.618919
181.303975	6538.924231	25.623936
181.227524	6549.243263	25.628954
181.502980	6553.877544	25.633971
182.043493	6567.337874	25.638989
181.682381	6565.263423	25.644007
182.250586	6557.400506	25.649024
182.589279	6559.474048	25.654042
182.870160	6546.774064	25.659059
183.201537	6542.498924	25.664077
183.216940	6540.643518	25.669095
183.597484	6533.211375	25.674112
183.606088	6535.739304	25.679130
183.427272	6543.125026	25.684148
183.806103	6562.442310	25.689165
183.582813	6573.872030	25.694183
184.048197	6566.495437	25.699200
183.808098	6573.962575	25.704218
184.138526	6577.045839	25.709236
184.255443	6600.045835	25.714253
184.376568	6608.672849	25.719271
184.583271	6607.599952	25.724288
184.468140	6635.414259	25.729306
184.505894	6650.878202	25.734324
185.102852	6660.565113	25.739341
184.999555	6669.329885	25.744359
185.232757	6677.693524	25.749376
185.478262	6691.247856	25.754394
185.794871	6695.280379	25.759412
185.904262	6711.771921	25.764429
185.842403	6730.049507	25.769447
186.414138	6733.493974	25.774464
186.163140	6762.107720	25.779482
186.892557	6769.769541	25.784500
187.148236	6780.549338	25.789517
187.122378	6794.825374	25.794535
186.891507	6789.902128	25.799552
187.515417	6817.949279	25.804570
187.637890	6816.220433	25.809588
188.426222	6821.642851	25.814605
188.454962	6835.410132	25.819623
188.889890	6835.170136	25.824640
189.126387	6838.068677	25.829658
189.091476	6835.828775	25.834676
189.153031	6838.266537	25.839693
189.101149	6846.865043	25.844711
189.532193	6858.271028	25.849728
189.305920	6870.050443	25.854746
189.374671	6881.258591	25.859764
189.891231	6893.780365	25.864781
190.066742	6907.187753	25.869799
190.461505	6900.628199	25.874816
190.170009	6924.212286	25.879834
190.370039	6928.461790	25.884852
191.067222	6923.728392	25.889869
190.944761	6933.850743	25.894887
191.308579	6950.348547	25.899904
191.318245	6964.064064	25.904922
191.457367	6958.228142	25.909940
191.648960	6971.264157	25.914957
191.530618	7001.858855	25.919975
192.106773	6995.596663	25.924992
191.764267	7000.810448	25.930010
191.919525	7027.629838	25.935028
192.281767	7041.880531	25.940045
192.184460	7055.798800	25.945063
192.581679	7072.719546	25.950080
192.472918	7095.034986	25.955098
192.671398	7113.154155	25.960116
193.192147	7133.101646	25.965133
193.039631	7145.091557	25.970151
193.717457	7154.506521	25.975168
193.865117	7174.927656	25.980186
193.698662	7194.280095	25.985204
194.238646	7203.002636	25.990221
194.288154	7231.374278	25.995239
194.814351	7236.676345	26.000256
195.311705	7253.369783	26.005274
195.354813	7266.005308	26.010292
195.793077	7259.458634	26.015309
195.856739	7272.304126	26.020327
196.247909	7283.206775	26.025344
196.255444	7297.433419	26.030362
196.402798	7301.205210	26.035380
196.520183	7306.074780	26.040397
196.853070	7327.865807	26.045415
196.853999	7325.387299	26.050432
196.827865	7340.719485	26.055450
197.332527	7348.748618	26.060468
198.121672	7348.529828	26.065485
198.018134	7357.488810	26.070503
198.301951	7355.735400	26.075520
198.369112	7375.437960	26.080538
198.247054	7388.781745	26.085556
198.512609	7395.022671	26.090573
198.056843	7396.981209	26.095591
198.748324	7418.691983	26.100608
199.112610	7425.868421	26.105626
199.193616	7451.147749	26.110644
199.679841	7449.532157	26.115661
200.326341	7450.784182	26.120679
200.752104	7426.245128	26.125696
201.070456	7427.360395	26.130714
200.713361	7420.419032	26.135732
201.395500	7409.589096	26.140749
201.574803	7412.150924	26.145767
201.458199	7408.109117	26.150784
201.893334	7415.125304	26.155802
201.762057	7409.002339	26.160820
201.597446	7408.433408	26.165837
201.748466	7430.652003	26.170855
201.846307	7441.785444	26.175872
202.006695	7439.252800	26.180890
201.834992	7453.427591	26.185908
201.842680	7458.944660	26.190925
202.526074	7481.733803	26.195943
202.807057	7494.363395	26.200960
202.799936	7511.281442	26.205978
203.108471	7519.438027	26.210996
203.545688	7522.187271	26.216013
203.349930	7545.772402	26.221031
203.192792	7549.075722	26.226048
203.941494	7555.465500	26.231066
204.048194	7571.733871	26.236084
204.642859	7572.363776	26.241101
204.907356	7593.819476	26.246119
205.374019	7591.952769	26.251136
205.541850	7601.343556	26.256154
205.556157	7607.390510	26.261172
205.826452	7604.387599	26.266189
205.717957	7617.651258	26.271207
205.576979	7622.701500	26.276224
205.850356	7624.946302	26.281242
205.800359	7652.917432	26.286260
206.170681	7655.451283	26.291277
206.291873	7672.000088	26.296295
206.925156	7682.118622	26.301312
207.140514	7694.207380	26.306330
207.248405	7719.073658	26.311348
207.485720	7724.931173	26.316365
207.717988	7722.759577	26.321383
209.057702	7703.002900	26.326400
209.453336	7703.351024	26.331418
209.295835	7699.356330	26.336436
210.073551	7678.943676	26.341453
209.866019	7666.127220	26.346471
209.948367	7657.547449	26.351488
209.761141	7664.675943	26.356506
209.522602	7670.685909	26.361524
209.480627	7670.502446	26.366541
210.215708	7692.773332	26.371559
209.894338	7704.781575	26.376576
210.225433	7700.053200	26.381594
209.800348	7722.508817	26.386612
210.152263	7727.828321	26.391629
210.331546	7758.909932	26.396647
210.327089	7771.471291	26.401664
210.794555	7796.884231	26.406682
211.005793	7817.144819	26.411700
210.933387	7833.314959	26.416717
211.245433	7863.051299	26.421735
211.171214	7876.687441	26.426752
211.430478	7893.771358	26.431770
211.465569	7915.040712	26.436788
211.921982	7937.690584	26.441805
212.288390	7952.414057	26.446823
212.296655	7974.334876	26.451840
212.821200	7998.863100	26.456858
212.680543	8018.296403	26.461876
213.157779	8033.397221	26.466893
213.233577	8054.102801	26.471911
213.532678	8081.702862	26.476928
214.254864	8083.543857	26.481946
214.287558	8111.167576	26.486964
214.870379	8115.878829	26.491981
214.951452	8118.673471	26.496999
214.963029	8141.977349	26.502016
215.350195	8147.335857	26.507034
215.326981	8162.080617	26.512052
215.527657	8173.235541	26.517069
215.792130	8175.718293	26.522087
216.097797	8202.976313	26.527104
216.384864	8201.624045	26.532122
216.590006	8231.132017	26.537140
216.742998	8242.705616	26.542157
216.996961	8248.157107	26.547175
217.022442	8270.871863	26.552192
217.690315	8275.677304	26.557210
217.971066	8292.858016	26.562228
218.537676	8289.994052	26.567245
218.670313	8292.577415	26.572263
218.763118	8296.317038	26.577280
218.797387	8298.838482	26.582298
218.998251	8321.073400	26.587316
219.578115	8329.490353	26.592333
219.841345	8335.145907	26.597351
219.301813	8335.630713	26.602368
219.959669	8349.547496	26.607386
220.207620	8355.315183	26.612404
220.549101	8363.038765	26.617421
220.772321	8374.923430	26.622439
220.636124	8384.549566	26.627456
220.944002	8391.833800	26.632474
220.845443	8397.867309	26.637492
221.037725	8422.390898	26.642509
221.190981	8433.572251	26.647527
221.354755	8451.854873	26.652544
221.837353	8463.509215	26.657562
221.532739	8494.253704	26.662580
222.064672	8498.032337	26.667597
222.204554	8520.840495	26.672615
222.006734	8536.160707	26.677632
222.104456	8555.332414	26.682650
222.632059	8583.912839	26.687668
222.560820	8591.109309	26.692685
222.988608	8605.980429	26.697703
222.966600	8635.695888	26.702720
223.694385	8653.432992	26.707738
224.027876	8675.194233	26.712756
224.530877	8677.706296	26.717773
224.774862	8686.294461	26.722791
224.794458	8705.769664	26.727808
225.363654	8710.061936	26.732826
225.481071	8715.394392	26.737844
225.784025	8730.313024	26.742861
226.058427	8737.774116	26.747879
226.223435	8749.555587	26.752896
226.880557	8756.626493	26.757914
226.748523	8777.057429	26.762932
226.960352	8770.535570	26.767949
227.607152	8773.092330	26.772967
227.419907	8777.180237	26.777984
227.769254	8782.608470	26.783002
227.607220	8791.055145	26.788020
227.934772	8801.987857	26.793037
228.266961	8799.335740	26.798055
228.213810	8817.199009	26.803072
228.974534	8819.622799	26.808090
228.643822	8838.371937	26.813108
229.043932	8856.006289	26.818125
228.952379	8860.537918	26.823143
229.158512	8888.890364	26.828160
229.128872	8892.889833	26.833178
229.621100	8926.946190	26.838196
229.274745	8933.076735	26.843213
229.756652	8958.933388	26.848231
229.884621	8986.840873	26.853248
230.619175	8996.928704	26.858266
230.714216	9013.451070	26.863284
230.618396	9040.606000	26.868301
231.556813	9056.846759	26.873319
231.646664	9069.712834	26.878336
231.807385	9089.919079	26.883354
231.920131	9106.175359	26.888372
231.998603	9124.284278	26.893389
231.967253	9134.873776	26.898407
231.798908	9165.197522	26.903424
232.404401	9182.370004	26.908442
232.780209	9208.519421	26.913460
233.143627	9236.004075	26.918477
233.803082	9245.342281	26.923495
234.057329	9261.282951	26.928512
234.067341	9270.321226	26.933530
234.827545	9285.253388	26.938548
234.667741	9293.991454	26.943565
235.236295	9314.829278	26.948583
235.346894	9327.622669	26.953600
235.724886	9333.673325	26.958618
236.153415	9343.155170	26.963636
236.293434	9357.293955	26.968653
236.729137	9353.347652	26.973671
236.588268	9364.113646	26.978688
236.867185	9380.762444	26.983706
237.470005	9389.372993	26.988724
237.586793	9390.071503	26.993741
237.354118	9388.095990	26.998759
237.255083	9402.518456	27.003776
237.350675	9416.132305	27.008794
237.934178	9420.732742	27.013812
237.571848	9451.041426	27.018829
238.640456	9452.005394	27.023847
238.710707	9471.695018	27.028864
238.853694	9484.539709	27.033882
240.151678	9468.543878	27.038900
240.224260	9464.382457	27.043917
240.547743	9455.756460	27.048935
240.834167	9476.560914	27.053952
240.810399	9474.702430	27.058970
241.033783	9474.219764	27.063988
240.923017	9488.171590	27.069005
241.259242	9479.603275	27.074023
241.516608	9484.595271	27.079040
241.871772	9498.534999	27.084058
241.746189	9511.734597	27.089076
241.977072	9523.413948	27.094093
242.057781	9528.381086	27.099111
242.478121	9551.253719	27.104128
242.449082	9562.820075	27.109146
242.305157	9575.170378	27.114164
242.247064	9602.597119	27.119181
242.909186	9613.068063	27.124199
243.106208	9634.452170	27.129216
242.658767	9650.176285	27.134234
242.716234	9682.838562	27.139252
242.833860	9707.714117	27.144269
243.603320	9735.563363	27.149287
243.549074	9779.401528	27.154304
243.738159	9796.652345	27.159322
244.324461	9818.326098	27.164340
244.407512	9862.309563	27.169357
245.062819	9876.239141	27.174375
245.254675	9908.174455	27.179392
245.698816	9939.480390	27.184410
246.125140	9952.021606	27.189428
245.948396	9973.771206	27.194445
246.696663	9994.870629	27.199463
246.690653	10006.427050	27.204480
247.082914	10013.298090	27.209498
247.893413	10040.921790	27.214516
248.357206	10056.384525	27.219533
248.942788	10036.931581	27.224551
249.762641	10031.354490	27.229568
250.393830	10028.094665	27.234586
250.801354	10025.935275	27.239604
250.606964	10033.609691	27.244621
250.879001	10024.396555	27.249639
250.770175	10011.238272	27.254656
250.560653	9995.117405	27.259674
250.844567	9989.509279	27.264692
250.604326	10000.730803	27.269709
250.975073	10019.091605	27.274727
250.895672	10024.554355	27.279744
251.197008	10028.234212	27.284762
250.975796	10044.704684	27.289780
251.072612	10063.197584	27.294797
251.454242	10085.872754	27.299815
251.464989	10106.282467	27.304832
251.489085	10122.307560	27.309850
251.429465	10136.522217	27.314868
251.513687	10175.537766	27.319885
251.711880	10197.083150	27.324903
252.207366	10230.148925	27.329920
252.572708	10257.184299	27.334938
253.363708	10294.071375	27.339956
253.022871	10322.330986	27.344973
253.652706	10344.343092	27.349991
253.799923	10372.082626	27.355008
254.198612	10396.603772	27.360026
254.715624	10406.827486	27.365044
254.917433	10435.860997	27.370061
255.298863	10436.451160	27.375079
255.804925	10467.270019	27.380096
255.700936	10478.621374	27.385114
256.517419	10500.764015	27.390132
256.596195	10521.952093	27.395149
256.615299	10535.461802	27.400167
257.282399	10561.999993	27.405184
257.118261	10578.714935	27.410202
257.506851	10585.104634	27.415220
257.451628	10602.417095	27.420237
258.182757	10609.236610	27.425255
258.590587	10631.126421	27.430272
258.783524	10643.526954	27.435290
258.694609	10644.517646	27.440308
259.485254	10671.425656	27.445325
259.559794	10684.473711	27.450343
260.137293	10700.048371	27.455360
259.841944	10709.934029	27.460378
260.596937	10724.299532	27.465396
260.736383	10734.217839	27.470413
261.017062	10737.698112	27.475431
261.463290	10753.747601	27.480448
261.323989	10763.868141	27.485466
262.567575	10734.858898	27.490484
263.191728	10736.089825	27.495501
263.728406	10717.678232	27.500519
263.753672	10716.731514	27.505536
263.693251	10717.113765	27.510554
263.893157	10717.523885	27.515572
264.108229	10717.359362	27.520589
264.197864	10719.860663	27.525607
264.158201	10717.914936	27.530624
264.412215	10740.682236	27.535642
264.722606	10746.841142	27.540660
264.404972	10757.356274	27.545677
264.878687	10749.373595	27.550695
264.892443	10757.545322	27.555712
264.722142	10779.747173	27.560730
265.145424	10786.569102	27.565748
265.106686	10813.466648	27.570765
265.298667	10833.568853	27.575783
265.719261	10856.788409	27.580800
265.566408	10882.478009	27.585818
265.675867	10905.193096	27.590836
265.953017	10943.477722	27.595853
266.249936	10967.973051	27.600871
266.799073	10984.309279	27.605888
267.141913	11005.801001	27.610906
267.669377	11028.253929	27.615924
267.587933	11050.404671	27.620941
268.359210	11071.195832	27.625959
269.002177	11091.643401	27.630976
268.825442	11115.585044	27.635994
269.614308	11122.697460	27.641012
269.358072	11137.629063	27.646029
269.526705	11154.547583	27.651047
270.154387	11183.277774	27.656064
270.080577	11194.660702	27.661082
270.832778	11209.964792	27.666100
271.245771	11218.637229	27.671117
271.630477	11238.484696	27.676135
271.415716	11252.343967	27.681152
271.886558	11266.348917	27.686170
272.384455	11268.168865	27.691188
272.629408	11276.518703	27.696205
273.048077	11288.920436	27.701223
273.980665	11289.228629	27.706240
273.991600	11293.514857	27.711258
274.776886	11286.882672	27.716276
274.586383	11288.628352	27.721293
275.025646	11292.878986	27.726311
275.123097	11274.906092	27.731328
275.121258	11289.423886	27.736346
275.243386	11306.076324	27.741364
275.341814	11319.910338	27.746381
275.532620	11334.770226	27.751399
275.662768	11349.673618	27.756416
275.172632	11360.984610	27.761434
276.554540	11376.847550	27.766452
276.278584	11390.915996	27.771469
276.680870	11423.993876	27.776487
276.997555	11438.255486	27.781504
276.912758	11461.639752	27.786522
277.232713	11474.148377	27.791540
277.264809	11496.303903	27.796557
277.461300	11529.920000	27.801575
277.940791	11554.852979	27.806592
277.863474	11581.146930	27.811610
278.266534	11591.132470	27.816628
279.043161	11609.973941	27.821645
279.687199	11635.263375	27.826663
279.768124	11635.769561	27.831680
280.412976	11657.429439	27.836698
280.483328	11659.393634	27.841716
280.597029	11673.616171	27.846733
280.670689	11692.494700	27.851751
280.819685	11694.852020	27.856768
281.029312	11713.853835	27.861786
281.288813	11735.389173	27.866804
281.421629	11756.501828	27.871821
281.397051	11765.942989	27.876839
282.379326	11791.225124	27.881856
282.566740	11819.559107	27.886874
282.870179	11826.060030	27.891892
283.091980	11858.309238	27.896909
283.245522	11868.667098	27.901927
283.449788	11893.074108	27.906944
283.862240	11921.180577	27.911962
284.287372	11941.277284	27.916980
284.074939	11960.228798	27.921997
284.175212	11987.120210	27.927015
284.775520	12008.758247	27.932032
284.967235	12048.505305	27.937050
285.168119	12058.514753	27.942068
285.364717	12091.024053	27.947085
285.707556	12123.621824	27.952103
286.198947	12149.445697	27.957120
286.139771	12186.340950	27.962138
287.105232	12184.485966	27.967156
287.916268	12194.948830	27.972173
288.043274	12225.993594	27.977191
288.174407	12227.417896	27.982208
287.989161	12259.266430	27.987226
288.537758	12283.731631	27.992244
288.756455	12299.410304	27.997261
288.894136	12326.765519	28.002279
289.545047	12341.380402	28.007296
289.246574	12377.049967	28.012314
289.861265	12407.173035	28.017332
290.209445	12422.569585	28.022349
290.037839	12447.513083	28.027367
290.487152	12464.447895	28.032384
290.527525	12499.197550	28.037402
290.749296	12530.228224	28.042420
291.348894	12562.901067	28.047437
291.379923	12599.163973	28.052455
292.564103	12608.957943	28.057472
292.615237	12626.763385	28.062490
292.771761	12648.141056	28.067508
293.281161	12669.759302	28.072525
293.362995	12692.908723	28.077543
293.939248	12721.273761	28.082560
294.107697	12739.951275	28.087578
294.474978	12752.350324	28.092596
294.985097	12756.721593	28.097613
294.860187	12784.371598	28.102631
295.339240	12796.121092	28.107648
295.487876	12812.969106	28.112666
295.858867	12829.994949	28.117684
296.259561	12836.750694	28.122701
296.412693	12860.392477	28.127719
296.851716	12879.020622	28.132736
297.203363	12891.107239	28.137754
297.570232	12900.619080	28.142772
298.273968	12929.043009	28.147789
298.409517	12941.075288	28.152807
298.428145	12951.633480	28.157824
298.797839	12971.595955	28.162842
298.639835	12987.921431	28.167860
299.181225	12997.592548	28.172877
299.755786	13014.627824	28.177895
300.267010	13015.588295	28.182912
300.584540	13023.677567	28.187930
300.953877	13035.223809	28.192948
301.204020	13054.021647	28.197965
301.231704	13062.384423	28.202983
301.536866	13077.371296	28.208000
301.536566	13090.519210	28.213018
301.569924	13122.938750	28.218036
302.172480	13135.504236	28.223053
302.356737	13161.615613	28.228071
302.428166	13185.011809	28.233088
302.517097	13212.941106	28.238106
302.637530	13235.395912	28.243124
303.384071	13242.533863	28.248141
303.478780	13267.631549	28.253159
304.047482	13289.885086	28.258176
304.303983	13314.102429	28.263194
304.844451	13332.400053	28.268212
304.933504	13347.822974	28.273229
305.396072	13380.270330	28.278247
305.722123	13393.231731	28.283264
305.854312	13419.487990	28.288282
306.205397	13446.061404	28.293300
306.337997	13464.332937	28.298317
306.313619	13497.317913	28.303335
306.583455	13524.706061	28.308352
307.511920	13548.351496	28.313370
307.274879	13573.492323	28.318388
307.911124	13602.114974	28.323405
308.295137	13628.905277	28.328423
308.576127	13655.405931	28.333440
309.233135	13679.309287	28.338458
308.980289	13709.345439	28.343476
309.649909	13723.745574	28.348493
309.871529	13754.567380	28.353511
309.716621	13778.192351	28.358528
310.416970	13803.503862	28.363546
310.440270	13827.955800	28.368564
310.888018	13850.068480	28.373581
310.913952	13872.452086	28.378599
311.001595	13892.736702	28.383616
311.399810	13929.234352	28.388634
311.528864	13949.524550	28.393652
312.423496	13973.411249	28.398669
312.447568	14001.657204	28.403687
312.967127	14023.184075	28.408704
313.341838	14054.163041	28.413722
312.998124	14084.686732	28.418740
313.635953	14103.739292	28.423757
313.898154	14154.561651	28.428775
314.187641	14185.170875	28.433792
314.759967	14198.788964	28.438810
315.260015	14246.366400	28.443828
315.597218	14258.308337	28.448845
315.774024	14291.252535	28.453863
316.002970	14310.667016	28.458880
316.703682	14330.347432	28.463898
316.733604	14362.536715	28.468916
316.970560	14384.544381	28.473933
317.450256	14414.785694	28.478951
317.867925	14435.920747	28.483968
318.555186	14448.299339	28.488986
318.274187	14480.792764	28.494004
319.103029	14505.487514	28.499021
319.685333	14523.544436	28.504039
319.834396	14546.984426	28.509056
320.400071	14556.141601	28.514074
320.608710	14590.967708	28.519092
320.805658	14597.883627	28.524109
320.976851	14624.294318	28.529127
321.434192	14646.322882	28.534144
321.660964	14655.278116	28.539162
322.029622	14682.172068	28.544180
323.172829	14672.253762	28.549197
323.882674	14672.058005	28.554215
324.834671	14671.083057	28.559232
325.615928	14658.908119	28.564250
326.071340	14654.903599	28.569268
326.594573	14634.108226	28.574285
326.287809	14626.058847	28.579303
326.480066	14623.604759	28.584320
326.993205	14598.574192	28.589338
326.923728	14589.910407	28.594356
327.151261	14582.513465	28.599373
327.238767	14591.654888	28.604391
326.919303	14592.760987	28.609408
326.997149	14604.050925	28.614426
327.378276	14620.875130	28.619444
327.176589	14629.550704	28.624461
327.506033	14657.606732	28.629479
327.625450	14680.672116	28.634496
327.845752	14697.200830	28.639514
327.848304	14728.282678	28.644532
328.035518	14748.998939	28.649549
328.617228	14775.686294	28.654567
328.618478	14801.056109	28.659584
329.376703	14820.443529	28.664602
330.062676	14854.214246	28.669620
329.975989	14869.383404	28.674637
330.294899	14893.877678	28.679655
330.863746	14921.495902	28.684672
331.391639	14931.443176	28.689690
331.350177	14961.175825	28.694708
331.279903	14988.295252	28.699725
332.084742	15011.995513	28.704743
331.791247	15041.938589	28.709760
332.372146	15060.910593	28.714778
332.431884	15096.598721	28.719796
332.694869	15125.470845	28.724813
333.326278	15163.811785	28.729831
333.729191	15204.323143	28.734848
333.968114	15224.028605	28.739866
334.084056	15272.538646	28.744884
334.434076	15296.977743	28.749901
335.063165	15330.839575	28.754919
334.839637	15369.710562	28.759936
336.126357	15403.114617	28.764954
336.416534	15436.741554	28.769972
336.356000	15472.796320	28.774989
336.629875	15494.463377	28.780007
337.295842	15514.088112	28.785024
337.693868	15544.408543	28.790042
338.016340	15574.256466	28.795060
338.663537	15593.830917	28.800077
338.934787	15625.245139	28.805095
339.284464	15649.259200	28.810112
339.534834	15669.245395	28.815130
339.963728	15699.552939	28.820148
340.234187	15728.647097	28.825165
340.795390	15756.373640	28.830183
340.478584	15780.628226	28.835200
341.502101	15800.472615	28.840218
341.377448	15834.732640	28.845236
342.111559	15862.248443	28.850253
342.704994	15869.005513	28.855271
343.029312	15893.029002	28.860288
343.976457	15906.453430	28.865306
344.256723	15925.982391	28.870324
344.557584	15933.358703	28.875341
344.681277	15956.850750	28.880359
344.587905	15971.571213	28.885376
345.106277	15990.406821	28.890394
345.437456	16012.209761	28.895412
345.307226	16031.702006	28.900429
345.787930	16055.900706	28.905447
345.441447	16087.163144	28.910464
345.794934	16111.029039	28.915482
346.024059	16147.529033	28.920500
346.229914	16179.902926	28.925517
346.603258	16212.270246	28.930535
346.690086	16245.670411	28.935552
347.508765	16269.970716	28.940570
347.635445	16309.274137	28.945588
348.054038	16347.537632	28.950605
348.583697	16372.183986	28.955623
349.010423	16417.663094	28.960640
349.342658	16427.789837	28.965658
349.892134	16461.003946	28.970676
350.528990	16498.079588	28.975693
350.906513	16523.010775	28.980711
351.101268	16554.758301	28.985728
351.417400	16582.086822	28.990746
351.847678	16598.497891	28.995764
352.256484	16626.471130	29.000781
352.429635	16645.804899	29.005799
352.579583	16683.483052	29.010816
353.138847	16707.007128	29.015834
353.786090	16730.284420	29.020852
353.680499	16759.028645	29.025869
354.249550	16782.459716	29.030887
354.098402	16819.065764	29.035904
354.570052	16842.772152	29.040922
355.600996	16879.675480	29.045940
355.637918	16911.524829	29.050957
356.523382	16923.727859	29.055975
358.030342	16925.988779	29.060992
358.790178	16916.399721	29.066010
359.456325	16914.751637	29.071028
359.698695	16917.924509	29.076045
360.226922	16916.938533	29.081063
360.471356	16918.747405	29.086080
359.920565	16915.110283	29.091098
360.137376	16923.705865	29.096116
359.948739	16932.085596	29.101133
360.762340	16936.637726	29.106151
360.832554	16956.155026	29.111168
360.785563	16966.238314	29.116186
361.225576	16981.546139	29.121204
361.446854	17019.083555	29.126221
361.761526	17041.768772	29.131239
361.539423	17066.745209	29.136256
362.427913	17089.459844	29.141274
362.276824	17126.128037	29.146292
362.790563	17145.183305	29.151309
362.857789	17171.631627	29.156327
363.166933	17213.425143	29.161344
363.416164	17241.437799	29.166362
364.269369	17274.718139	29.171380
364.341473	17307.547527	29.176397
364.648705	17338.471673	29.181415
364.768211	17383.224116	29.186432
365.500711	17409.815770	29.191450
365.494946	17445.340428	29.196468
365.598114	17482.342613	29.201485
366.055518	17515.836306	29.206503
366.339831	17548.346023	29.211520
366.767464	17593.162882	29.216538
367.026587	17630.855990	29.221556
367.372207	17671.518750	29.226573
368.176110	17710.356257	29.231591
368.282472	17747.006909	29.236608
368.433353	17778.493111	29.241626
368.969540	17815.767085	29.246644
369.276960	17864.354318	29.251661
369.924278	17888.255957	29.256679
370.368050	17927.210866	29.261696
370.830087	17971.158882	29.266714
370.902954	18009.242642	29.271732
371.487581	18047.435854	29.276749
372.587210	18066.101674	29.281767
372.721377	18105.624022	29.286784
373.013323	18134.434906	29.291802
373.404423	18162.733798	29.296820
373.733325	18192.878548	29.301837
374.668618	18214.278127	29.306855
374.465145	18243.829966	29.311872
374.962761	18269.758505	29.316890
375.664964	18296.686272	29.321908
375.817388	18326.807903	29.326925
376.649044	18347.199046	29.331943
376.528114	18380.590200	29.336960
376.901338	18400.918078	29.341978
377.730795	18428.331917	29.346996
378.032900	18454.574885	29.352013
377.816943	18476.933605	29.357031
378.307378	18502.389174	29.362048
378.928820	18534.004262	29.367066
379.517262	18554.770007	29.372084
379.685232	18579.278223	29.377101
380.146247	18600.955080	29.382119
380.625731	18639.489292	29.387136
380.778921	18661.572148	29.392154
381.447000	18686.913991	29.397172
381.768864	18719.421117	29.402189
382.397165	18742.264581	29.407207
382.082517	18767.942087	29.412224
382.623701	18800.276191	29.417242
383.458686	18821.920777	29.422260
383.693219	18848.712002	29.427277
383.906895	18866.589292	29.432295
384.131446	18903.862331	29.437312
384.653172	18924.532755	29.442330
385.073659	18954.149185	29.447348
385.226663	18992.855254	29.452365
385.862379	19014.572079	29.457383
386.010053	19047.902755	29.462400
386.343805	19072.980836	29.467418
386.773557	19088.407446	29.472436
387.275724	19109.418858	29.477453
388.872570	19113.473159	29.482471
389.634891	19123.551484	29.487488
389.736035	19119.767457	29.492506
389.877761	19118.235853	29.497524
390.019689	19132.732715	29.502541
390.466276	19146.366965	29.507559
390.879182	19154.822873	29.512576
390.568827	19168.528525	29.517594
391.118721	19187.228325	29.522612
390.951390	19213.399990	29.527629
391.476616	19247.055798	29.532647
391.658770	19272.833403	29.537664
391.585953	19307.140510	29.542682
392.473323	19335.482465	29.547700
392.433450	19368.238886	29.552717
392.743639	19401.012638	29.557735
393.363164	19440.581076	29.562752
392.969253	19485.750322	29.567770
393.753140	19534.287526	29.572788
394.081712	19587.577874	29.577805
394.371570	19628.418900	29.582823
394.514695	19675.219976	29.587840
394.884077	19730.739582	29.592858
395.187296	19765.114042	29.597876
395.650932	19825.647597	29.602893
396.116311	19862.402150	29.607911
396.925335	19910.352731	29.612928
396.686693	19964.646527	29.617946
397.467115	20002.287139	29.622964
397.913111	20048.879667	29.627981
398.541075	20105.800504	29.632999
398.923997	20150.269175	29.638016
399.487074	20206.695327	29.643034
399.397242	20232.826900	29.648052
400.361151	20272.588975	29.653069
401.034530	20303.156230	29.658087
402.215632	20325.522373	29.663104
402.828292	20353.285556	29.668122
403.763911	20385.972956	29.673140
403.982818	20397.567446	29.678157
404.529351	20424.791778	29.683175
404.587209	20430.229688	29.688192
404.710661	20448.877825	29.693210
405.465395	20464.314652	29.698228
405.800196	20488.986264	29.703245
405.737434	20507.412512	29.708263
406.289462	20524.237032	29.713280
406.386256	20554.127763	29.718298
406.622516	20566.182977	29.723316
406.829463	20595.424179	29.728333
407.235781	20634.746546	29.733351
407.807921	20659.705712	29.738368
407.973741	20704.976225	29.743386
408.778188	20733.844057	29.748404
408.615833	20763.503622	29.753421
409.163774	20787.177276	29.758439
409.939295	20798.698729	29.763456
410.729994	20832.876706	29.768474
410.933482	20846.705369	29.773492
411.848079	20871.111033	29.778509
411.986648	20879.835581	29.783527
412.696549	20911.678073	29.788544
412.114762	20932.160050	29.793562
413.175403	20947.682083	29.798580
413.659526	20978.856965	29.803597
413.466449	20998.679513	29.808615
414.092318	21028.915622	29.813632
414.438845	21054.428088	29.818650
414.455070	21092.359774	29.823668
414.366922	21131.466849	29.828685
414.886431	21159.166898	29.833703
415.195861	21197.162105	29.838720
415.277348	21258.262976	29.843738
415.609013	21288.997798	29.848756
416.392935	21343.576474	29.853773
416.491972	21399.710817	29.858791
417.136642	21437.358962	29.863808
417.230604	21486.928284	29.868826
417.706040	21534.328791	29.873844
418.241032	21594.165741	29.878861
418.687455	21638.599042	29.883879
419.002382	21690.542185	29.888896
419.490831	21753.152001	29.893914
419.807256	21793.056988	29.898932
420.025337	21838.132324	29.903949
420.411010	21896.612957	29.908967
420.881523	21943.799405	29.913984
421.220550	21993.351853	29.919002
421.586811	22041.524680	29.924020
422.072144	22108.389360	29.929037
422.689986	22162.373067	29.934055
423.438637	22207.014676	29.939072
423.709681	22273.724335	29.944090
424.151279	22311.237320	29.949108
425.099526	22351.246651	29.954125
425.662565	22389.451790	29.959143
426.613977	22428.524034	29.964160
427.396847	22452.741655	29.969178
427.878911	22484.220848	29.974196
428.366799	22500.629380	29.979213
428.942264	22531.237926	29.984231
429.617108	22559.924486	29.989248
429.423304	22584.826919	29.994266
429.558877	22606.764957	29.999284
429.978063	22635.650001	30.004301
430.061416	22671.834253	30.009319
430.885905	22700.296702	30.014336
431.208441	22728.094559	30.019354
431.658139	22753.044663	30.024372
432.153826	22788.250141	30.029389
432.649775	22826.745310	30.034407
432.591538	22850.637682	30.039424
433.098509	22887.490996	30.044442
433.986319	22909.902937	30.049460
435.573608	22912.135237	30.054477
435.979816	22918.897300	30.059495
436.826240	22915.771657	30.064512
436.748072	22942.947792	30.069530
437.378262	22937.780674	30.074548
437.854270	22946.120433	30.079565
438.128698	22950.394458	30.084583
438.981646	22954.219245	30.089600
438.662357	22982.610075	30.094618
439.279634	22988.847116	30.099636
439.701264	23004.775453	30.104653
439.515168	23034.323167	30.109671
440.009138	23047.015680	30.114688
440.022844	23079.803169	30.119706
440.507720	23106.116634	30.124724
440.535460	23133.659722	30.129741
440.326670	23182.051004	30.134759
440.767125	23224.568600	30.139776
441.047282	23272.393769	30.144794
441.052486	23326.713232	30.149812
441.981195	23375.648199	30.154829
441.555126	23436.060012	30.159847
441.841568	23484.137024	30.164864
442.140989	23549.074143	30.169882
442.292444	23620.335769	30.174900
443.297601	23688.978505	30.179917
443.662851	23757.507222	30.184935
444.655576	23818.888462	30.189952
445.080053	23879.225466	30.194970
445.365902	23930.773483	30.199988
446.170069	23984.216857	30.205005
446.460758	24042.533404	30.210023
446.700438	24094.190756	30.215040
447.406916	24148.433640	30.220058
447.961529	24200.485251	30.225076
448.633000	24253.627308	30.230093
448.578644	24315.688129	30.235111
449.595001	24363.257687	30.240128
450.035545	24414.332725	30.245146
450.384204	24459.802628	30.250164
451.190737	24514.344950	30.255181
451.441416	24565.210086	30.260199
452.130379	24608.694753	30.265216
453.033615	24663.000169	30.270234
453.361724	24703.730055	30.275252
454.003050	24739.621154	30.280269
454.361551	24783.809541	30.285287
454.991502	24808.104016	30.290304
456.364434	24807.474436	30.295322
457.402169	24820.002532	30.300340
458.275262	24816.045540	30.305357
458.442270	24842.782044	30.310375
459.008978	24855.097521	30.315392
459.685347	24851.704174	30.320410
459.872867	24860.822974	30.325428
459.826811	24860.480714	30.330445
459.967099	24890.215406	30.335463
460.251942	24898.790761	30.340480
460.406008	24925.274103	30.345498
460.741557	24965.489161	30.350516
461.116654	24990.004214	30.355533
461.044229	25021.122526	30.360551
461.622887	25063.570506	30.365568
461.743770	25107.488149	30.370586
462.403907	25144.165481	30.375604
462.963902	25189.263562	30.380621
463.027742	25239.184810	30.385639
463.503254	25279.950730	30.390656
463.891358	25322.258500	30.395674
464.098874	25372.865274	30.400692
465.061987	25408.327237	30.405709
465.519637	25455.178529	30.410727
466.135295	25494.302670	30.415744
466.312677	25537.378924	30.420762
466.393776	25588.228805	30.425780
466.823460	25631.315686	30.430797
466.617928	25699.561897	30.435815
467.296976	25752.079505	30.440832
468.382511	25808.287879	30.445850
468.985000	25869.784291	30.450868
469.425783	25919.939434	30.455885
469.518513	25971.274251	30.460903
469.825482	26010.761604	30.465920
470.544272	26059.964136	30.470938
471.603625	26110.852965	30.475956
472.233985	26144.080033	30.480973
472.861565	26191.456254	30.485991
473.475275	26234.216558	30.491008
473.769301	26265.447808	30.496026
474.087295	26313.397932	30.501044
474.846821	26358.909670	30.506061
475.625263	26397.238209	30.511079
476.186503	26430.745819	30.516096
476.514321	26460.775999	30.521114
477.033446	26494.167914	30.526132
477.349933	26536.241690	30.531149
477.541666	26577.302195	30.536167
477.625455	26625.050396	30.541184
478.297704	26672.237298	30.546202
478.463657	26719.353348	30.551220
479.206873	26764.613407	30.556237
479.765160	26811.268132	30.561255
479.996018	26855.064077	30.566272
480.727818	26903.209916	30.571290
481.182306	26944.667930	30.576308
481.958537	26992.159669	30.581325
482.096282	27035.072904	30.586343
482.616520	27062.481053	30.591360
483.081466	27098.836313	30.596378
482.993615	27148.028711	30.601396
483.927719	27190.919442	30.606413
484.157988	27238.502250	30.611431
484.478243	27283.542733	30.616448
485.105519	27333.376585	30.621466
485.421803	27383.793887	30.626484
486.039214	27436.402852	30.631501
486.157653	27484.377766	30.636519
486.569150	27545.168262	30.641536
487.122786	27595.545502	30.646554
487.353755	27648.804981	30.651572
488.646245	27700.756419	30.656589
489.499633	27744.690847	30.661607
489.477771	27794.529977	30.666624
489.933716	27848.559178	30.671642
489.922492	27896.702566	30.676660
490.711915	27945.103262	30.681677
490.977469	28009.106893	30.686695
491.268280	28069.935662	30.691712
491.920621	28126.863054	30.696730
492.355277	28191.847974	30.701748
493.093797	28256.339364	30.706765
493.278995	28322.717864	30.711783
493.296998	28385.228779	30.716800
493.933902	28437.193777	30.721818
494.309208	28499.489274	30.726836
495.691029	28567.771240	30.731853
496.206617	28626.970104	30.736871
496.826335	28685.602336	30.741888
497.626475	28741.055045	30.746906
497.790639	28794.121205	30.751924
497.887343	28852.610133	30.756941
498.890733	28907.798216	30.761959
499.488631	28962.970765	30.766976
500.277562	29020.682211	30.771994
500.727602	29065.439989	30.777012
501.641248	29117.529957	30.782029
501.818022	29161.915166	30.787047
502.289329	29208.430258	30.792064
503.035802	29251.487548	30.797082
503.375220	29309.860677	30.802100
503.481227	29350.895030	30.807117
504.791073	29388.284002	30.812135
505.541452	29426.882716	30.817152
506.312888	29457.782275	30.822170
506.843804	29492.367410	30.827188
507.725990	29514.930866	30.832205
508.376005	29536.060630	30.837223
508.832551	29573.078747	30.842240
509.744603	29585.183802	30.847258
509.884240	29625.913282	30.852276
510.168398	29640.628093	30.857293
510.533745	29663.264524	30.862311
510.842219	29683.446455	30.867328
511.338423	29710.389569	30.872346
511.434150	29760.438131	30.877364
511.497313	29783.221153	30.882381
511.845084	29828.645228	30.887399
512.061271	29868.784729	30.892416
512.491318	29920.164794	30.897434
513.154624	29974.073480	30.902452
513.657341	30021.288971	30.907469
513.978361	30071.514371	30.912487
514.541667	30135.272754	30.917504
514.886172	30180.206054	30.922522
515.118181	30242.696335	30.927540
515.659384	30299.242743	30.932557
516.134042	30354.686877	30.937575
515.998393	30420.030153	30.942592
516.462690	30480.275835	30.947610
517.230935	30551.829202	30.952628
518.316480	30604.367417	30.957645
519.747517	30663.460421	30.962663
520.019002	30700.768197	30.967680
520.928733	30746.293972	30.972698
521.582014	30797.496333	30.977716
521.868656	30843.738129	30.982733
522.673394	30877.988750	30.987751
523.332055	30923.933505	30.992768
523.527047	30966.240638	30.997786
524.189732	31012.986432	31.002804
524.589537	31063.119094	31.007821
524.843960	31097.281412	31.012839
525.104086	31166.399895	31.017856
525.456557	31220.296207	31.022874
525.747706	31270.299758	31.027892
526.035750	31336.387933	31.032909
526.695997	31394.217524	31.037927
526.646349	31463.399702	31.042944
527.628421	31525.355741	31.047962
528.513038	31590.405421	31.052980
529.027933	31652.262080	31.057997
529.584825	31704.985647	31.063015
530.365923	31774.471632	31.068032
530.896449	31825.638027	31.073050
531.094029	31882.150518	31.078068
531.205155	31942.550021	31.083085
532.259718	32011.879624	31.088103
532.430822	32064.752404	31.093120
534.076379	32113.724700	31.098138
535.188074	32164.240237	31.103156
535.378428	32200.454240	31.108173
536.402281	32235.089644	31.113191
536.514419	32283.223798	31.118208
537.400516	32324.708848	31.123226
537.504051	32371.613972	31.128244
537.516574	32402.939032	31.133261
538.016359	32443.575379	31.138279
538.216615	32494.765566	31.143296
538.601847	32550.525342	31.148314
539.051594	32600.221419	31.153332
539.708824	32663.745540	31.158349
540.357884	32708.156503	31.163367
540.952644	32759.907859	31.168384
541.883875	32807.660076	31.173402
542.127749	32861.056074	31.178420
542.820604	32910.616682	31.183437
543.087497	32960.635427	31.188455
543.271653	33022.045397	31.193472
543.852467	33068.573912	31.198490
544.452895	33130.752392	31.203508
544.910349	33197.490614	31.208525
545.700468	33247.493093	31.213543
546.202019	33310.979906	31.218560
547.016674	33356.276162	31.223578
547.498634	33426.851803	31.228596
548.293280	33480.754901	31.233613
549.249530	33521.842524	31.238631
549.311247	33575.536954	31.243648
549.830382	33630.674351	31.248666
550.060296	33682.077444	31.253684
550.639212	33738.975438	31.258701
551.415766	33793.062463	31.263719
552.245953	33853.979547	31.268736
552.780644	33902.152939	31.273754
553.284159	33960.055542	31.278772
553.368125	34010.099078	31.283789
554.730545	34066.223184	31.288807
554.831199	34119.357095	31.293824
555.474867	34174.275986	31.298842
556.273046	34218.636729	31.303860
556.700373	34273.845477	31.308877
557.215890	34332.899193	31.313895
557.585409	34390.015017	31.318912
558.197630	34446.268846	31.323930
558.447905	34502.992006	31.328948
558.597862	34578.817716	31.333965
559.279574	34635.110724	31.338983
559.650283	34716.321457	31.344000
560.069952	34772.167427	31.349018
561.324757	34828.874147	31.354036
561.970401	34896.949884	31.359053
562.493071	34950.402140	31.364071
562.967975	35014.590720	31.369088
563.621362	35069.021451	31.374106
564.374839	35134.523061	31.379124
564.423973	35206.174027	31.384141
565.134353	35257.625527	31.389159
565.900125	35329.599226	31.394176
566.102293	35396.790161	31.399194
566.831311	35454.722036	31.404212
567.090929	35509.496153	31.409229
567.608794	35575.626797	31.414247
567.871167	35645.226072	31.419264
568.452638	35710.538289	31.424282
568.975265	35771.142079	31.429300
568.981723	35846.375866	31.434317
569.701661	35914.559475	31.439335
570.120780	35997.172227	31.444352
570.931278	36078.853441	31.449370
571.889211	36144.210030	31.454388
572.324161	36216.793139	31.459405
573.241240	36279.051289	31.464423
573.383543	36351.511471	31.469440
574.304920	36408.949430	31.474458
575.337498	36476.832218	31.479476
575.660669	36545.641709	31.484493
576.133117	36605.998042	31.489511
577.019408	36678.303641	31.494528
577.012653	36741.094121	31.499546
577.599440	36807.542548	31.504564
577.741856	36888.896784	31.509581
578.794986	36954.934409	31.514599
579.649687	37018.130640	31.519616
580.711710	37074.479678	31.524634
581.571245	37143.193207	31.529652
581.753182	37222.553505	31.534669
582.312584	37284.024084	31.539687
583.096046	37352.492591	31.544704
583.566212	37412.012312	31.549722
584.720301	37461.585265	31.554740
585.125712	37509.556781	31.559757
585.939732	37568.301537	31.564775
586.687218	37627.010532	31.569792
587.000720	37692.391533	31.574810
587.516705	37741.269618	31.579828
587.795048	37805.728978	31.584845
588.504759	37866.850619	31.589863
588.970337	37929.419032	31.594880
589.439621	37999.923050	31.599898
590.255604	38054.284324	31.604916
590.707336	38107.215023	31.609933
591.345570	38163.453775	31.614951
592.092432	38236.616488	31.619968
592.606943	38299.619726	31.624986
593.369120	38365.380824	31.630004
593.895862	38436.795300	31.635021
594.006448	38508.843267	31.640039
594.869917	38562.083550	31.645056
595.128247	38632.916563	31.650074
596.265385	38692.023101	31.655092
596.594575	38756.192961	31.660109
597.546513	38813.229148	31.665127
598.354714	38871.587617	31.670144
598.657499	38919.409921	31.675162
599.538002	38972.695827	31.680180
599.761220	39028.032842	31.685197
600.225908	39080.935707	31.690215
600.639252	39142.124986	31.695232
600.917014	39215.441408	31.700250
601.474279	39277.288376	31.705268
602.168793	39350.546560	31.710285
602.612813	39407.917850	31.715303
603.093575	39477.611051	31.720320
603.797601	39557.554922	31.725338
604.558831	39620.984479	31.730356
605.043739	39695.470132	31.735373
605.628832	39771.220676	31.740391
605.990328	39832.013861	31.745408
605.953366	39913.563718	31.750426
606.673260	39994.179208	31.755444
607.045408	40074.276879	31.760461
608.023802	40159.795958	31.765479
608.584861	40250.491990	31.770496
608.805722	40339.087271	31.775514
609.641546	40422.551435	31.780532
610.034351	40516.343179	31.785549
610.670517	40604.862257	31.790567
611.906881	40683.696849	31.795584
612.437410	40765.749922	31.800602
613.099954	40847.351356	31.805620
613.949277	40929.240029	31.810637
614.326839	41015.756322	31.815655
615.126907	41094.828424	31.820672
615.416799	41185.411289	31.825690
616.226807	41255.765134	31.830708
617.165913	41334.909152	31.835725
618.229058	41403.651008	31.840743
619.220074	41461.812654	31.845760
620.083360	41545.930712	31.850778
620.650881	41610.947340	31.855796
621.572820	41667.148119	31.860813
622.125970	41723.636424	31.865831
622.329271	41782.022429	31.870848
622.971410	41861.008011	31.875866
623.797631	41926.341356	31.880884
624.215811	41996.979826	31.885901
624.616986	42071.334608	31.890919
625.320006	42131.622109	31.895936
625.637824	42204.621373	31.900954
626.399050	42280.648738	31.905972
626.665688	42349.085330	31.910989
627.512232	42421.906446	31.916007
628.223278	42506.860063	31.921024
628.483247	42579.472849	31.926042
629.647440	42649.348149	31.931060
629.626652	42732.536809	31.936077
630.276740	42798.001250	31.941095
631.418819	42873.416354	31.946112
631.977739	42950.807267	31.951130
632.569990	43016.992834	31.956148
633.002453	43086.477277	31.961165
633.485256	43160.923427	31.966183
634.277228	43224.104197	31.971200
634.592972	43303.805391	31.976218
635.479496	43370.083877	31.981236
636.553827	43432.727538	31.986253
636.846226	43499.452450	31.991271
638.170537	43549.593532	31.996288
639.155483	43605.271468	32.001306
640.172395	43642.919996	32.006324
641.402323	43693.920737	32.011341
641.551294	43745.087860	32.016359
642.628532	43785.824049	32.021376
642.868706	43843.480704	32.026394
643.641827	43890.543616	32.031412
644.174508	43944.964318	32.036429
644.508403	44001.847541	32.041447
644.753111	44051.274960	32.046464
644.972076	44118.134632	32.051482
645.437632	44180.196680	32.056500
645.975242	44253.140960	32.061517
646.156498	44327.337064	32.066535
646.933696	44406.341764	32.071552
647.149443	44493.640707	32.076570
647.747629	44568.726307	32.081588
649.249255	44637.853290	32.086605
650.661546	44708.104243	32.091623
651.361833	44762.122794	32.096640
651.733349	44828.434627	32.101658
652.427008	44886.888341	32.106676
652.923201	44954.533993	32.111693
653.490149	45026.377270	32.116711
653.925621	45107.672926	32.121728
654.396550	45184.573311	32.126746
654.915845	45258.367764	32.131764
656.015994	45327.404988	32.136781
656.335018	45411.993550	32.141799
656.935111	45489.536214	32.146816
657.550134	45568.039830	32.151834
657.905697	45647.879849	32.156852
658.770042	45724.781334	32.161869
658.904298	45826.987333	32.166887
659.629088	45911.868614	32.171904
660.032767	46005.512110	32.176922
660.324128	46095.376117	32.181940
661.047498	46198.219011	32.186957
662.229496	46285.351153	32.191975
663.260821	46356.643009	32.196992
664.139205	46446.967093	32.202010
664.802476	46538.714891	32.207028
666.283088	46595.810503	32.212045
667.542734	46663.044027	32.217063
668.293308	46718.303837	32.222080
668.889257	46777.812819	32.227098
669.676254	46831.636047	32.232116
670.561267	46874.673088	32.237133
670.924753	46928.439655	32.242151
671.855753	46980.495288	32.247168
672.158818	47024.349282	32.252186
672.690462	47082.894329	32.257204
673.086101	47132.468109	32.262221
673.300971	47211.937654	32.267239
673.969092	47276.103756	32.272256
674.194733	47344.148470	32.277274
674.629368	47423.435958	32.282292
675.388353	47498.167591	32.287309
675.540773	47579.620148	32.292327
676.116983	47660.577229	32.297344
676.630271	47753.774628	32.302362
676.916401	47844.396250	32.307380
677.693864	47940.480275	32.312397
677.883155	48050.133024	32.317415
678.824865	48154.768241	32.322432
679.134349	48261.189469	32.327450
679.987535	48368.010862	32.332468
680.791986	48475.286541	32.337485
681.031150	48593.126939	32.342503
681.651011	48696.133580	32.347520
682.536368	48800.838800	32.352538
683.420067	48911.754593	32.357556
684.346165	49020.844418	32.362573
684.437220	49140.343339	32.367591
685.343942	49242.141375	32.372608
686.166336	49355.483387	32.377626
686.979114	49465.113138	32.382644
688.678833	49549.353848	32.387661
689.642612	49636.614345	32.392679
691.011006	49714.797340	32.397696
692.047128	49799.241261	32.402714
692.387976	49888.751204	32.407732
693.290257	49969.030333	32.412749
693.638836	50045.146663	32.417767
694.123212	50123.842840	32.422784
694.601579	50215.977762	32.427802
695.473587	50307.249673	32.432820
696.499984	50383.529180	32.437837
696.408405	50472.035569	32.442855
697.202765	50570.265077	32.447872
697.771904	50668.641061	32.452890
698.307184	50760.320246	32.457908
699.011346	50850.587343	32.462925
699.578294	50961.758610	32.467943
700.516084	51052.239326	32.472960
701.543138	51153.085379	32.477978
703.230485	51216.834046	32.482996
704.499931	51286.991348	32.488013
705.645827	51365.857190	32.493031
706.047607	51427.356468	32.498048
706.717950	51487.969646	32.503066
707.029531	51552.801692	32.508084
707.734910	51616.574568	32.513101
708.255868	51673.688472	32.518119
709.748262	51707.600621	32.523136
710.490080	51750.758326	32.528154
711.148853	51813.926979	32.533172
712.292779	51854.450900	32.538189
712.554285	51923.848075	32.543207
713.239897	51963.212387	32.548224
713.800391	52027.763274	32.553242
714.134308	52084.449191	32.558260
714.457896	52153.015181	32.563277
714.889354	52225.423342	32.568295
715.901864	52297.340504	32.573312
716.156493	52372.995466	32.578330
716.400994	52454.288339	32.583348
716.890955	52536.026006	32.588365
717.490803	52628.663230	32.593383
718.236831	52719.494076	32.598400
718.411355	52807.011319	32.603418
718.994421	52909.920091	32.608436
719.576071	53019.792560	32.613453
720.087027	53133.361420	32.618471
720.671937	53237.339401	32.623488
722.216849	53348.388209	32.628506
722.207203	53454.358422	32.633524
723.019803	53560.618013	32.638541
723.528274	53690.005976	32.643559
724.159174	53789.713885	32.648576
724.895291	53908.771142	32.653594
725.681651	54015.334642	32.658612
726.834840	54129.519524	32.663629
727.097646	54252.432236	32.668647
727.936303	54369.079847	32.673664
728.832274	54491.247365	32.678682
729.626352	54609.496384	32.683700
730.713495	54713.952123	32.688717
731.274523	54832.273979	32.693735
731.953470	54943.404214	32.698752
732.993225	55059.263127	32.703770
733.594289	55156.657563	32.708788
735.420977	55236.231070	32.713805
737.338861	55314.310589	32.718823
738.010010	55396.534516	32.723840
739.292923	55480.246430	32.728858
739.367059	55561.833954	32.733876
740.279903	55633.742365	32.738893
741.072244	55711.384315	32.743911
741.601571	55787.523387	32.748928
742.340641	55866.527397	32.753946
743.217352	55936.155482	32.758964
744.133238	56009.505536	32.763981
744.484039	56094.719398	32.768999
745.519443	56163.613315	32.774016
746.406024	56227.300454	32.779034
747.158345	56293.241568	32.784052
747.769599	56358.910046	32.789069
748.513466	56424.189491	32.794087
748.889186	56490.360070	32.799104
749.590880	56566.984453	32.804122
750.454197	56642.601908	32.809140
750.483755	56715.910458	32.814157
750.923893	56798.356647	32.819175
751.415727	56886.096511	32.824192
751.491208	56983.716234	32.829210
751.854702	57090.570764	32.834228
752.722251	57196.871855	32.839245
754.365816	57293.662011	32.844263
755.276377	57388.821282	32.849280
755.738020	57478.591232	32.854298
756.635875	57591.329130	32.859316
757.251352	57679.386212	32.864333
757.740223	57783.284167	32.869351
758.351443	57886.706658	32.874368
759.124319	57997.831353	32.879386
759.714183	58119.416077	32.884404
760.301838	58227.578055	32.889421
761.038498	58345.119414	32.894439
761.188296	58470.832813	32.899456
762.365015	58579.060082	32.904474
762.830723	58704.758732	32.909492
763.633760	58821.343438	32.914509
764.570392	58950.198910	32.919527
765.050286	59067.895867	32.924544
765.973061	59194.005906	32.929562
767.035695	59330.363447	32.934580
767.723931	59457.039880	32.939597
768.379290	59572.219425	32.944615
768.769403	59702.936678	32.949632
769.929199	59829.028996	32.954650
770.861586	59951.052646	32.959668
771.537997	60073.443222	32.964685
772.276517	60203.661542	32.969703
772.911347	60326.300934	32.974720
774.226537	60447.098951	32.979738
774.661715	60575.614416	32.984756
775.555452	60707.206237	32.989773
776.702306	60829.147802	32.994791
777.024374	60941.484513	32.999808
778.095631	61058.073926	33.004826
779.067949	61183.321737	33.009844
780.219176	61299.962031	33.014861
781.224176	61411.027573	33.019879
781.475677	61534.789115	33.024896
782.638345	61644.716393	33.029914
783.521770	61761.904537	33.034932
784.441255	61872.222344	33.039949
784.895760	61987.797475	33.044967
785.786027	62102.906691	33.049984
786.830002	62203.615575	33.055002
787.440139	62305.170463	33.060020
788.752133	62394.557114	33.065037
789.455795	62491.836300	33.070055
790.497809	62588.811451	33.075072
791.390952	62665.097182	33.080090
792.152273	62769.106448	33.085108
792.970588	62851.784048	33.090125
794.352419	62931.988563	33.095143
795.519603	63011.458925	33.100160
796.474829	63096.547845	33.105178
797.057310	63166.617630	33.110196
797.552273	63247.443068	33.115213
798.240246	63327.856461	33.120231
798.283394	63417.774612	33.125248
799.306923	63508.328079	33.130266
799.779493	63616.430599	33.135284
800.434719	63719.666244	33.140301
801.920622	63797.289633	33.145319
802.320505	63903.958401	33.150336
803.101068	64000.327437	33.155354
803.937760	64098.596510	33.160372
804.432181	64203.075883	33.165389
805.291142	64311.684782	33.170407
805.761395	64427.182231	33.175424
806.389694	64521.082563	33.180442
807.163377	64636.257343	33.185460
807.767017	64760.546699	33.190477
808.892069	64872.375112	33.195495
809.168657	64998.106431	33.200512
809.993106	65119.230623	33.205530
810.199016	65245.847986	33.210548
811.157433	65369.751414	33.215565
812.243412	65490.965714	33.220583
812.878737	65620.584408	33.225600
813.957718	65748.648472	33.230618
814.967308	65864.333282	33.235636
815.642868	65996.830408	33.240653
816.955603	66117.883018	33.245671
817.851732	66232.021297	33.250688
818.483619	66341.115801	33.255706
819.238558	66469.372503	33.260724
820.446070	66586.766071	33.265741
821.895636	66694.603238	33.270759
822.204033	66805.178131	33.275776
823.486930	66907.778132	33.280794
824.392848	67024.403825	33.285812
825.023864	67139.597711	33.290829
826.008134	67237.717017	33.295847
826.908373	67347.314485	33.300864
827.752799	67445.945563	33.305882
829.438211	67540.968104	33.310900
830.032772	67639.250853	33.315917
830.907077	67722.342654	33.320935
831.986381	67821.605474	33.325952
832.922046	67893.717056	33.330970
834.179496	67977.597833	33.335988
834.656410	68055.928201	33.341005
835.684090	68136.219523	33.346023
835.935622	68221.399057	33.351040
836.725332	68308.345751	33.356058
837.468841	68385.411299	33.361076
837.611116	68475.074700	33.366093
838.379637	68570.372684	33.371111
838.583646	68687.981315	33.376128
839.177139	68797.733605	33.381146
839.904940	68909.777782	33.386164
840.361397	69031.417262	33.391181
841.373592	69145.905355	33.396199
841.756438	69262.500048	33.401216
842.465638	69390.864319	33.406234
843.477739	69523.502739	33.411252
844.404516	69659.368939	33.416269
845.351787	69785.310812	33.421287
845.903414	69918.871563	33.426304
846.616730	70058.615262	33.431322
847.284847	70193.055710	33.436340
848.252816	70342.104026	33.441357
849.388031	70469.092723	33.446375
849.727635	70606.273276	33.451392
850.757696	70738.916071	33.456410
852.200860	70872.051749	33.461428
853.126683	71013.301905	33.466445
854.039744	71138.163461	33.471463
855.100630	71287.739891	33.476480
855.559037	71419.428640	33.481498
856.590684	71554.947254	33.486516
857.201141	71694.915139	33.491533
858.240346	71827.993045	33.496551
859.022394	71967.357789	33.501568
859.765430	72099.507823	33.506586
861.005386	72234.634496	33.511604
861.432552	72388.393512	33.516621
862.609466	72522.856059	33.521639
863.167433	72663.617023	33.526656
864.014714	72807.453611	33.531674
865.852532	72917.955939	33.536692
867.005423	73050.161672	33.541709
868.011312	73167.808977	33.546727
869.962000	73263.076869	33.551744
870.995299	73368.855665	33.556762
872.118862	73472.152905	33.561780
873.348854	73563.820328	33.566797
873.948292	73657.227896	33.571815
874.593930	73761.430554	33.576832
875.565306	73874.344011	33.581850
876.301255	73963.068156	33.586868
876.734609	74078.452915	33.591885
877.153080	74191.974998	33.596903
878.134209	74304.914283	33.601920
879.158263	74417.473623	33.606938
880.288442	74500.958639	33.611956
880.790869	74611.691852	33.616973
881.383595	74712.505224	33.621991
882.094734	74814.367700	33.627008
882.589916	74933.357901	33.632026
883.491739	75044.113417	33.637044
884.058251	75161.289974	33.642061
885.047438	75282.727482	33.647079
885.497435	75405.864593	33.652096
885.989579	75542.727215	33.657114
886.767414	75678.738438	33.662132
886.916872	75819.855095	33.667149
887.717807	75956.774898	33.672167
888.568775	76106.400979	33.677184
889.193541	76269.552604	33.682202
890.138844	76424.281922	33.687220
890.685298	76584.419350	33.692237
891.647503	76742.791467	33.697255
892.025751	76921.101813	33.702272
892.997088	77090.709101	33.707290
893.724727	77265.084705	33.712308
894.525851	77456.794298	33.717325
895.437366	77628.876602	33.722343
895.925583	77810.540476	33.727360
896.693412	78004.847698	33.732378
897.655030	78191.399395	33.737396
898.912885	78373.448378	33.742413
899.550584	78556.996769	33.747431
901.084677	78748.560143	33.752448
901.726053	78940.448828	33.757466
903.095837	79105.815056	33.762484
904.609755	79285.512101	33.767501
906.343852	79444.327647	33.772519
907.763462	79598.763383	33.777536
908.997367	79745.096223	33.782554
910.279604	79885.044677	33.787572
911.379919	80032.117122	33.792589
912.712954	80148.226667	33.797607
915.099721	80271.615333	33.802624
916.643381	80367.704387	33.807642
917.773661	80471.292064	33.812660
918.326299	80579.490020	33.817677
919.344381	80675.240165	33.822695
920.284482	80764.721672	33.827712
920.956681	80873.248504	33.832730
921.868399	80975.465032	33.837748
922.895849	81078.022821	33.842765
923.346070	81174.175981	33.847783
924.273304	81281.421011	33.852800
924.673678	81379.120980	33.857818
926.158208	81478.502120	33.862836
926.727886	81601.095603	33.867853
927.258419	81713.516395	33.872871
928.247677	81824.669703	33.877888
928.904286	81949.401315	33.882906
929.470843	82051.757650	33.887924
930.052717	82168.265448	33.892941
930.683019	82294.869908	33.897959
931.703649	82419.256990	33.902976
931.602306	82549.721146	33.907994
932.431881	82681.855169	33.913012
933.041869	82831.060480	33.918029
933.783057	82966.659606	33.923047
934.435775	83123.275044	33.928064
934.851193	83286.114008	33.933082
935.402536	83454.378730	33.938100
936.143232	83625.529194	33.943117
937.189566	83796.109713	33.948135
938.193180	83978.404763	33.953152
938.748563	84163.384964	33.958170
939.921421	84335.187952	33.963188
940.618672	84524.759563	33.968205
941.610700	84715.206072	33.973223
942.905327	84895.768899	33.978240
943.540924	85082.729526	33.983258
944.494042	85264.030740	33.988276
945.624396	85451.776485	33.993293
946.809507	85632.053635	33.998311
947.954181	85814.680461	34.003328
948.710806	86004.620820	34.008346
949.798402	86181.356134	34.013364
950.502185	86371.510980	34.018381
951.491418	86557.258303	34.023399
953.005707	86744.796663	34.028416
953.497755	86936.207314	34.033434
954.693095	87134.346385	34.038452
955.861609	87312.322937	34.043469
956.559759	87499.652606	34.048487
958.243984	87669.835401	34.053504
959.215426	87856.905895	34.058522
960.427483	88028.380860	34.063540
961.497154	88197.413249	34.068557
963.416593	88340.214330	34.073575
965.346823	88477.666618	34.078592
967.278047	88622.809003	34.083610
968.108633	88753.717353	34.088628
969.722849	88882.789757	34.093645
970.490519	89008.280105	34.098663
971.726635	89125.235446	34.103680
972.368702	89255.305411	34.108698
973.191350	89361.238045	34.113716
974.276026	89490.796783	34.118733
974.715319	89613.194656	34.123751
975.885335	89739.107235	34.128768
976.379890	89884.939947	34.133786
977.049250	90012.420695	34.138804
977.851597	90152.487080	34.143821
978.455499	90303.620099	34.148839
979.194905	90451.832047	34.153856
979.662050	90604.901792	34.158874
981.065094	90743.400314	34.163892
982.031993	90895.272338	34.168909
982.310418	91032.578951	34.173927
983.550958	91166.803701	34.178944
984.199069	91328.619616	34.183962
985.166953	91485.178963	34.188980
986.534507	91630.714377	34.193997
987.252728	91786.698105	34.199015
988.363808	91944.672687	34.204032
988.902377	92107.829068	34.209050
989.886050	92260.080131	34.214068
991.006331	92426.284887	34.219085
991.868911	92592.781756	34.224103
993.254874	92750.296669	34.229120
993.845984	92916.171241	34.234138
994.675971	93085.221632	34.239156
995.856017	93246.440008	34.244173
996.825918	93425.134652	34.249191
997.942704	93584.055597	34.254208
998.728366	93759.663473	34.259226
999.762436	93928.482101	34.264244
1000.823634	94106.722904	34.269261
1001.356757	94291.145112	34.274279
1001.938900	94477.529011	34.279296
1002.767913	94655.402025	34.284314
1003.587461	94838.500497	34.289332
1004.547416	95034.996795	34.294349
1005.547407	95243.338458	34.299367
1006.433475	95434.298696	34.304384
1007.451952	95645.274035	34.309402
1008.192270	95849.278088	34.314420
1009.016042	96051.344970	34.319437
1009.711507	96265.090350	34.324455
1011.209075	96476.440090	34.329472
1012.032137	96690.179877	34.334490
1013.918285	96888.386977	34.339508
1015.152948	97089.784032	34.344525
1016.066716	97291.313607	34.349543
1017.719180	97464.956622	34.354560
1018.985020	97654.570737	34.359578
1021.025164	97839.621876	34.364596
1022.350997	98021.852674	34.369613
1022.859079	98195.677639	34.374631
1024.095264	98362.566659	34.379648
1025.029664	98548.755644	34.384666
1026.198402	98712.442186	34.389684
1027.287021	98876.998231	34.394701
1028.281240	99054.696574	34.399719
1029.104343	99217.521132	34.404736
1030.032035	99404.920456	34.409754
1030.999173	99574.402370	34.414772
1032.538781	99749.910043	34.419789
1033.072324	99930.111984	34.424807
1034.009336	100097.481387	34.429824
1035.088569	100266.980311	34.434842
1035.602350	100436.906421	34.439860
1036.596436	100607.378250	34.444877
1037.842478	100793.549075	34.449895
1038.619798	100964.326303	34.454912
1039.869021	101131.072710	34.459930
1040.647662	101313.008897	34.464948
1041.902977	101476.058584	34.469965
1042.884952	101651.035067	34.474983
1043.994508	101832.171025	34.480000
1045.062046	102004.387082	34.485018
1045.572174	102189.794715	34.490036
1046.709404	102362.153163	34.495053
1047.457950	102560.883638	34.500071
1048.715350	102747.952964	34.505088
1050.133250	102920.418989	34.510106
1051.495335	103104.674012	34.515124
1052.670982	103281.641911	34.520141
1053.401225	103477.000891	34.525159
1054.434815	103648.498947	34.530176
1055.441810	103836.708066	34.535194
1055.917035	104021.716598	34.540212
1057.030927	104213.595686	34.545229
1058.163148	104416.390661	34.550247
1059.102136	104610.797662	34.555264
1059.918195	104808.241557	34.560282
1060.523779	105015.855560	34.565300
1061.873711	105225.585580	34.570317
1062.566614	105450.540240	34.575335
1063.387406	105653.385264	34.580352
1064.313250	105874.275783	34.585370
1065.036370	106096.482121	34.590388
1066.328454	106314.526964	34.595405
1067.402637	106542.655400	34.600423
1068.793711	106770.148840	34.605440
1070.142610	106998.284751	34.610458
1070.772323	107218.540308	34.615476
1072.139165	107443.117521	34.620493
1073.147552	107660.968451	34.625511
1074.394581	107892.650749	34.630528
1075.547724	108108.137056	34.635546
1076.523032	108327.658385	34.640564
1077.895735	108548.582853	34.645581
1079.484116	108766.431973	34.650599
1080.460922	108979.421835	34.655616
1081.734079	109197.885731	34.660634
1082.887473	109430.610498	34.665652
1083.741268	109633.973613	34.670669
1084.910816	109849.002075	34.675687
1085.806272	110061.228815	34.680704
1087.270759	110283.139613	34.685722
1088.250334	110500.701307	34.690740
1089.719312	110703.941620	34.695757
1090.955931	110897.595149	34.700775
1092.580035	111092.729249	34.705792
1094.204846	111279.300577	34.710810
1095.122724	111459.976539	34.715828
1096.495268	111628.287059	34.720845
1097.925244	111811.892797	34.725863
1098.453086	111992.727665	34.730880
1099.389951	112167.032442	34.735898
1100.160420	112346.130390	34.740916
1101.098162	112528.292132	34.745933
1101.954649	112729.751666	34.750951
1102.365504	112916.529078	34.755968
1103.673926	113118.484133	34.760986
1104.852084	113328.913551	34.766004
1105.567109	113549.078131	34.771021
1106.246322	113758.848658	34.776039
1107.102440	113973.785096	34.781056
1108.302360	114189.044392	34.786074
1109.000999	114418.543615	34.791092
1110.220112	114635.108013	34.796109
1111.511453	114876.280027	34.801127
1111.983945	115100.489259	34.806144
1113.239976	115333.701505	34.811162
1113.886574	115580.602857	34.816180
1115.175414	115811.139867	34.821197
1116.388502	116063.536145	34.826215
1117.327016	116309.557490	34.831232
1119.018551	116544.516915	34.836250
1120.507577	116791.360416	34.841268
1122.121832	117011.879121	34.846285
1123.447355	117242.243862	34.851303
1124.696267	117451.082144	34.856320
1126.343676	117669.293963	34.861338
1126.999161	117904.479785	34.866356
1128.131231	118114.609980	34.871373
1129.480465	118349.870679	34.876391
1130.316541	118573.474276	34.881408
1131.349810	118815.584937	34.886426
1131.968532	119044.133387	34.891444
1133.134386	119280.877548	34.896461
1133.779644	119524.733191	34.901479
1134.745245	119775.341078	34.906496
1135.969772	120016.250298	34.911514
1137.027798	120277.022624	34.916532
1138.286277	120521.820623	34.921549
1139.907882	120769.308466	34.926567
1141.064358	121015.293878	34.931584
1142.344520	121259.992833	34.936602
1143.286720	121504.599570	34.941620
1144.550593	121748.950453	34.946637
1145.693926	122001.675696	34.951655
1146.920426	122245.770869	34.956672
1148.502810	122487.487826	34.961690
1149.666237	122734.854852	34.966708
1150.776599	122971.232159	34.971725
1152.065118	123203.259021	34.976743
1153.331001	123446.431932	34.981760
1154.793334	123667.279496	34.986778
1155.586486	123891.576525	34.991796
1156.901738	124101.324516	34.996813
1158.064967	124326.790776	35.001831
1159.058718	124535.950395	35.006848
1160.436710	124749.076143	35.011866
1161.460687	124974.431576	35.016884
1162.779459	125200.688788	35.021901
1164.063399	125416.826480	35.026919
1165.028808	125640.853279	35.031936
1166.253589	125854.798733	35.036954
1167.280976	126073.722720	35.041972
1168.936227	126291.412670	35.046989
1170.159695	126509.951254	35.052007
1171.467474	126730.213452	35.057024
1172.516479	126938.505236	35.062042
1174.081444	127162.858628	35.067060
1175.152890	127376.359104	35.072077
1176.548493	127586.180301	35.077095
1177.970208	127803.806679	35.082112
1179.585908	128009.587487	35.087130
1180.773664	128209.130304	35.092148
1182.643664	128400.939320	35.097165
1184.358304	128582.102863	35.102183
1185.360459	128778.461331	35.107200
1186.378688	128965.843510	35.112218
1187.575320	129161.714708	35.117236
1188.371968	129343.382015	35.122253
1189.273488	129543.844219	35.127271
1189.889687	129749.794750	35.132288
1190.956311	129967.458728	35.137306
1191.913663	130178.905963	35.142324
1192.364134	130396.995254	35.147341
1193.493008	130627.773507	35.152359
1194.253709	130862.850543	35.157376
1195.821425	131090.463802	35.162394
1196.498295	131334.331131	35.167412
1197.747200	131586.215791	35.172429
1198.769885	131825.501837	35.177447
1199.745673	132076.752479	35.182464
1201.050880	132330.382746	35.187482
1201.831051	132587.185527	35.192500
1202.937698	132844.213341	35.197517
1203.911348	133107.097734	35.202535
1204.817276	133377.805424	35.207552
1206.336317	133639.548433	35.212570
1207.472840	133907.393792	35.217588
1208.630336	134179.104588	35.222605
1209.879687	134441.825624	35.227623
1211.295617	134715.284211	35.232640
1212.601026	134994.342522	35.237658
1213.971742	135256.554743	35.242676
1215.163553	135527.801554	35.247693
1216.402969	135795.581083	35.252711
1217.297734	136067.276148	35.257728
1218.543349	136335.451959	35.262746
1219.944932	136598.265277	35.267764
1221.437773	136854.636637	35.272781
1222.758947	137097.713340	35.277799
1223.882185	137350.157725	35.282816
1225.358696	137592.780274	35.287834
1227.354559	137833.160107	35.292852
1228.482998	138072.586993	35.297869
1229.728150	138305.313326	35.302887
1230.614489	138557.452146	35.307904
1232.143054	138801.773451	35.312922
1233.143923	139047.213908	35.317940
1233.769413	139311.778633	35.322957
1235.178955	139562.072682	35.327975
1236.267948	139822.707164	35.332992
1237.849021	140068.131607	35.338010
1239.049160	140335.255960	35.343028
1240.318562	140595.167905	35.348045
1241.492898	140848.478722	35.353063
1242.523983	141117.400599	35.358080
1244.064293	141375.509316	35.363098
1245.967130	141618.467486	35.368116
1246.902110	141876.112845	35.373133
1248.207185	142124.097077	35.378151
1249.596943	142399.307897	35.383168
1250.739607	142652.484896	35.388186
1251.611287	142922.715905	35.393204
1252.525795	143187.070068	35.398221
1253.833849	143448.530807	35.403239
1254.630898	143726.237454	35.408256
1255.937002	144005.495058	35.413274
1257.151193	144290.223789	35.418292
1257.984813	144579.889809	35.423309
1259.372994	144859.761376	35.428327
1260.340519	145157.272000	35.433344
1261.462582	145453.059164	35.438362
1262.962781	145748.783990	35.443380
1264.329248	146044.483364	35.448397
1265.834848	146327.592800	35.453415
1267.264517	146622.436263	35.458432
1268.356124	146920.066760	35.463450
1269.545960	147211.544287	35.468468
1270.364638	147508.795004	35.473485
1271.901531	147812.786732	35.478503
1272.909009	148118.139884	35.483520
1274.446143	148419.434967	35.488538
1275.746144	148717.982700	35.493556
1276.602407	149031.448519	35.498573
1277.994675	149338.939965	35.503591
1279.448269	149653.818044	35.508608
1280.955758	149949.346606	35.513626
1282.556050	150250.543990	35.518644
1283.938243	150558.021645	35.523661
1285.660187	150836.498343	35.528679
1287.833899	151126.987824	35.533696
1289.300245	151394.565805	35.538714
1290.725800	151657.421329	35.543732
1292.176741	151913.209018	35.548749
1294.143407	152143.388713	35.553767
1295.715600	152383.949929	35.558784
1297.142597	152618.740555	35.563802
1298.701733	152851.455033	35.568820
1300.009042	153076.691859	35.573837
1301.432391	153311.943923	35.578855
1302.498078	153540.408693	35.583872
1303.696587	153777.021266	35.588890
1305.067864	154005.182715	35.593908
1305.856913	154237.390256	35.598925
1307.413485	154475.379145	35.603943
1308.241662	154719.798790	35.608960
1309.254604	154963.642829	35.613978
1310.802553	155211.912840	35.618996
1311.407223	155475.314924	35.624013
1312.110220	155731.255373	35.629031
1313.294363	156008.630240	35.634048
1314.315852	156287.087783	35.639066
1315.592392	156570.172029	35.644084
1316.748935	156852.137038	35.649101
1318.522927	157129.964107	35.654119
1318.960682	157428.256377	35.659136
1320.004106	157719.672628	35.664154
1321.557667	158010.483481	35.669172
1322.557661	158330.214955	35.674189
1323.532900	158618.985056	35.679207
1324.614797	158945.075943	35.684224
1325.842118	159267.617552	35.689242
1327.160507	159584.246642	35.694260
1328.375655	159901.669704	35.699277
1330.367366	160210.728302	35.704295
1332.185657	160532.036631	35.709312
1333.482115	160848.945415	35.714330
1334.657510	161153.012263	35.719348
1336.000638	161469.232559	35.724365
1337.286642	161780.986255	35.729383
1339.022707	162114.196172	35.734400
1340.262999	162422.815805	35.739418
1342.229114	162733.178525	35.744436
1343.290147	163051.805989	35.749453
1344.656533	163360.258462	35.754471
1345.879341	163675.551220	35.759488
1346.790588	163995.289703	35.764506
1348.890905	164308.089491	35.769524
1349.716332	164639.710926	35.774541
1350.904965	164956.554010	35.779559
1352.666445	165276.448078	35.784576
1354.388576	165594.003773	35.789594
1355.664714	165898.048384	35.794612
1356.895236	166222.646131	35.799629
1358.456572	166538.916398	35.804647
1359.817114	166851.987543	35.809664
1361.099747	167166.888730	35.814682
1362.275131	167453.602335	35.819700
1363.628368	167766.782542	35.824717
1364.940939	168060.341381	35.829735
1366.594746	168362.726312	35.834752
1367.506508	168660.748136	35.839770
1369.000125	168965.867307	35.844788
1369.878847	169275.319402	35.849805
1371.079134	169587.116883	35.854823
1372.406887	169901.914819	35.859840
1373.938568	170218.316968	35.864858
1375.462243	170532.717586	35.869876
1376.427485	170867.850037	35.874893
1377.949216	171177.724890	35.879911
1379.341259	171491.583333	35.884928
1381.011118	171817.883630	35.889946
1382.712457	172139.878688	35.894964
1383.775183	172463.761879	35.899981
1385.321326	172783.896903	35.904999
1387.134242	173107.427567	35.910016
1388.524724	173423.646629	35.915034
1390.715891	173735.326956	35.920052
1392.250268	174033.783465	35.925069
1394.249216	174328.253428	35.930087
1395.922642	174635.027792	35.935104
1397.189593	174927.354890	35.940122
1398.834589	175218.641772	35.945140
1399.200929	175518.373188	35.950157
1400.629206	175821.820909	35.955175
1402.198705	176131.718954	35.960192
1403.055567	176447.820133	35.965210
1404.369733	176761.103614	35.970228
1405.654625	177084.458580	35.975245
1406.438344	177401.656989	35.980263
1408.108606	177730.001413	35.985280
1409.205070	178073.574975	35.990298
1410.678154	178405.193890	35.995316
1412.004277	178745.737265	36.000333
1413.304487	179084.345383	36.005351
1415.105703	179410.545706	36.010368
1416.284292	179764.320941	36.015386
1417.489676	180087.987405	36.020404
1418.700002	180438.550506	36.025421
1419.945346	180787.866035	36.030439
1421.136776	181147.271084	36.035456
1422.067234	181512.333411	36.040474
1423.308971	181870.909626	36.045492
1424.583271	182244.612656	36.050509
1425.672152	182617.372603	36.055527
1427.450125	182992.771555	36.060544
1428.551165	183376.679139	36.065562
1430.385331	183752.898682	36.070580
1431.794327	184146.367709	36.075597
1432.941021	184532.699862	36.080615
1434.372901	184906.850783	36.085632
1435.935928	185286.668487	36.090650
1437.291857	185661.446663	36.095668
1438.818346	186030.612810	36.100685
1440.023002	186397.640352	36.105703
1442.070288	186762.888484	36.110720
1443.480996	187135.051874	36.115738
1445.024209	187499.895812	36.120756
1446.229251	187870.131463	36.125773
1448.421391	188233.561372	36.130791
1450.575433	188638.485290	36.135808
1451.949178	188992.716809	36.140826
1453.688754	189347.471754	36.145844
1454.982535	189700.197765	36.150861
1456.832601	190039.488500	36.155879
1458.562241	190391.978889	36.160896
1459.664277	190733.026410	36.165914
1461.198915	191067.628937	36.170932
1463.062290	191423.669594	36.175949
1464.411423	191756.682615	36.180967
1466.141884	192098.315598	36.185984
1467.796495	192443.911613	36.191002
1469.563230	192771.996274	36.196020
1470.942785	193117.871539	36.201037
1472.309652	193457.441236	36.206055
1474.030510	193792.407174	36.211072
1475.275989	194130.465033	36.216090
1476.842453	194475.604629	36.221108
1478.783510	194808.164034	36.226125
1480.200572	195142.249407	36.231143
1481.688209	195474.140716	36.236160
1482.795905	195815.988754	36.241178
1484.502842	196155.349159	36.246196
1485.656243	196501.623734	36.251213
1486.385496	196843.998808	36.256231
1488.275108	197182.228544	36.261248
1489.682368	197533.530662	36.266266
1491.456752	197879.617080	36.271284
1493.070289	198216.388290	36.276301
1494.954055	198558.447348	36.281319
1496.528346	198902.097300	36.286336
1497.956766	199240.289016	36.291354
1500.089086	199568.839493	36.296372
1501.960760	199898.235974	36.301389
1503.961702	200220.704874	36.306407
1506.004733	200530.357049	36.311424
1506.979018	200842.326491	36.316442
1508.580921	201165.502716	36.321460
1510.202108	201477.910127	36.326477
1511.118451	201799.632043	36.331495
1512.620275	202124.708736	36.336512
1513.603080	202450.612089	36.341530
1515.051768	202776.538706	36.346548
1516.910023	203106.561302	36.351565
1518.075839	203447.826561	36.356583
1519.220008	203778.405964	36.361600
1520.224672	204126.456749	36.366618
1521.798428	204455.860872	36.371636
1522.860152	204779.170368	36.376653
1523.971698	205118.077848	36.381671
1525.443915	205449.077998	36.386688
1526.900954	205800.639487	36.391706
1528.362716	206137.891488	36.396724
1530.537690	206474.895876	36.401741
1532.420279	206804.599713	36.406759
1534.335387	207117.563644	36.411776
1536.028639	207447.302468	36.416794
1537.664753	207779.376095	36.421812
1539.268699	208114.656428	36.426829
1540.819179	208442.912570	36.431847
1542.305160	208777.149097	36.436864
1543.621240	209113.523893	36.441882
1545.407245	209430.873990	36.446900
1546.931186	209757.869919	36.451917
1548.605659	210105.437837	36.456935
1550.352501	210427.902967	36.461952
1551.542095	210770.832734	36.466970
1552.732308	211104.697086	36.471988
1554.857495	211430.174121	36.477005
1556.028812	211770.088626	36.482023
1557.919973	212110.770123	36.487040
1559.605673	212449.507073	36.492058
1561.009777	212796.598340	36.497076
1562.063015	213137.020658	36.502093
1563.255173	213491.465201	36.507111
1564.692004	213844.396153	36.512128
1566.069185	214211.713655	36.517146
1567.688590	214578.940318	36.522164
1569.415575	214940.029102	36.527181
1571.011641	215305.535456	36.532199
1572.469839	215666.622114	36.537216
1573.689899	216038.900579	36.542234
1575.374086	216414.453564	36.547252
1576.959234	216787.612056	36.552269
1578.106031	217177.432036	36.557287
1579.367527	217562.585947	36.562304
1580.868896	217953.618094	36.567322
1581.962846	218355.363432	36.572340
1584.086113	218752.235398	36.577357
1585.545050	219160.448780	36.582375
1587.371277	219544.852869	36.587392
1588.874243	219946.788128	36.592410
1590.394841	220355.630379	36.597428
1592.236377	220752.506988	36.602445
1593.550448	221155.367870	36.607463
1595.107687	221564.716195	36.612480
1596.495375	221989.385445	36.617498
1597.512050	222398.625992	36.622516
1599.258293	222821.001719	36.627533
1600.805265	223251.896533	36.632551
1602.329007	223670.782734	36.637568
1603.979668	224087.819847	36.642586
1605.102473	224497.252477	36.647604
1607.154311	224897.637449	36.652621
1608.559467	225319.749838	36.657639
1610.426594	225726.544422	36.662656
1611.905065	226135.286386	36.667674
1613.295879	226555.042962	36.672692
1614.854571	226958.744432	36.677709
1616.303815	227385.097686	36.682727
1617.703070	227810.571780	36.687744
1619.739192	228232.585297	36.692762
1620.962482	228660.174897	36.697780
1622.735182	229091.608878	36.702797
1623.912021	229533.789051	36.707815
1625.814185	229975.998830	36.712832
1627.814618	230412.528641	36.717850
1629.668146	230847.459146	36.722868
1631.448221	231281.082557	36.727885
1633.302228	231712.052759	36.732903
1634.913637	232146.850406	36.737920
1636.624408	232576.932934	36.742938
1638.135205	233014.391793	36.747956
1640.022788	233446.630788	36.752973
1641.615565	233895.254508	36.757991
1643.159040	234331.339376	36.763008
1644.907447	234766.729780	36.768026
1645.957896	235207.778207	36.773044
1648.013454	235648.858904	36.778061
1649.385481	236102.860105	36.783079
1651.168903	236551.609963	36.788096
1653.581965	236997.738292	36.793114
1655.531923	237438.637791	36.798132
1657.842639	237860.145486	36.803149
1659.703299	238285.160297	36.808167
1661.233652	238711.375536	36.813184
1663.260457	239145.635356	36.818202
1664.548237	239575.475421	36.823220
1666.547242	239990.512027	36.828237
1668.128999	240410.142351	36.833255
1669.567122	240843.566066	36.838272
1671.361830	241269.232558	36.843290
1672.860085	241701.428095	36.848308
1674.727894	242122.612597	36.853325
1676.524188	242553.564562	36.858343
1678.320501	242981.214828	36.863360
1679.926352	243395.053850	36.868378
1681.743554	243814.445864	36.873396
1683.811947	244238.037713	36.878413
1685.325904	244660.531041	36.883431
1686.949740	245085.825806	36.888448
1689.015071	245490.926526	36.893466
1690.347800	245915.840239	36.898484
1692.185358	246332.361322	36.903501
1693.586123	246758.686887	36.908519
1694.897574	247188.305154	36.913536
1696.818891	247605.143442	36.918554
1697.996124	248018.451393	36.923572
1700.031951	248426.201980	36.928589
1701.798333	248834.761093	36.933607
1702.762806	249235.100127	36.938624
1704.690199	249671.067613	36.943642
1705.595013	250101.291460	36.948660
1707.431049	250508.315692	36.953677
1709.345611	250936.538333	36.958695
1710.689783	251376.798283	36.963712
1712.522311	251807.321750	36.968730
1714.240110	252240.329173	36.973748
1715.738410	252686.660207	36.978765
1717.177666	253127.539858	36.983783
1718.742994	253577.797289	36.988800
1720.633271	254034.654918	36.993818
1721.891391	254490.833336	36.998836
1723.895770	254942.235415	37.003853
1726.029708	255405.834359	37.008871
1727.313448	255864.447377	37.013888
1729.034131	256329.133265	37.018906
1730.545929	256798.783133	37.023924
1732.339358	257269.248526	37.028941
1734.284467	257751.500432	37.033959
1735.571111	258228.123805	37.038976
1737.718126	258700.764024	37.043994
1739.233325	259183.013018	37.049012
1741.460896	259663.031539	37.054029
1743.327074	260139.758503	37.059047
1744.697533	260621.218862	37.064064
1746.441773	261099.236438	37.069082
1747.756289	261591.629248	37.074100
1749.272348	262085.994139	37.079117
1750.858630	262589.212379	37.084135
1752.550973	263090.430672	37.089152
1754.417956	263601.703715	37.094170
1756.074630	264113.672775	37.099188
1757.944651	264617.831543	37.104205
1760.387254	265122.882586	37.109223
1761.743915	265645.875548	37.114240
1763.707562	266145.012336	37.119258
1765.736893	266654.171461	37.124276
1767.373051	267154.963465	37.129293
1769.486259	267660.271134	37.134311
1771.200574	268174.105492	37.139328
1773.332446	268676.258618	37.144346
1775.095587	269176.111632	37.149364
1777.211976	269683.321041	37.154381
1778.898540	270177.165165	37.159399
1780.918956	270686.523172	37.164416
1782.798001	271175.912665	37.169434
1784.384891	271665.656119	37.174452
1786.318083	272167.329421	37.179469
1788.085688	272668.268027	37.184487
1789.747648	273156.954384	37.189504
1792.113888	273629.769866	37.194522
1794.584824	274115.242247	37.199540
1796.341072	274558.998431	37.204557
1798.144766	275011.026747	37.209575
1799.811406	275477.378985	37.214592
1801.607311	275929.000321	37.219610
1802.915907	276386.470314	37.224628
1804.621958	276854.184503	37.229645
1806.331147	277320.245956	37.234663
1807.447889	277791.742043	37.239680
1809.643107	278270.571424	37.244698
1811.109914	278751.302317	37.249716
1813.116403	279232.396876	37.254733
1814.948340	279707.398243	37.259751
1816.324296	280198.885708	37.264768
1818.084911	280693.481166	37.269786
1819.680350	281187.874831	37.274804
1821.691221	281693.702747	37.279821
1822.827777	282195.004839	37.284839
1824.376159	282719.908755	37.289856
1826.191659	283241.132880	37.294874
1827.703423	283770.281489	37.299892
1829.759449	284296.337847	37.304909
1832.010466	284806.686717	37.309927
1833.565604	285341.232662	37.314944
1836.036154	285869.676289	37.319962
1837.751548	286402.158769	37.324980
1839.696855	286917.810216	37.329997
1841.686264	287436.728790	37.335015
1843.614256	287973.689972	37.340032
1845.504144	288496.761628	37.345050
1847.352447	289035.535449	37.350068
1848.924629	289572.652416	37.355085
1851.178295	290108.786905	37.360103
1852.352011	290638.550665	37.365120
1854.425386	291179.283201	37.370138
1856.624785	291723.522232	37.375156
1858.215609	292278.378125	37.380173
1859.740757	292830.397867	37.385191
1860.642321	293380.667451	37.390208
1862.890354	293936.139375	37.395226
1864.656707	294510.079592	37.400244
1866.151212	295083.275904	37.405261
1868.292584	295657.628412	37.410279
1869.887585	296239.106577	37.415296
1872.013002	296817.036590	37.420314
1873.910339	297397.719931	37.425332
1875.533696	297974.967262	37.430349
1877.853514	298552.803242	37.435367
1880.042555	299133.680488	37.440384
1882.065248	299706.353905	37.445402
1883.841185	300273.199297	37.450420
1885.460151	300852.360339	37.455437
1887.881725	301430.796347	37.460455
1889.731422	302004.805871	37.465472
1891.394869	302571.478563	37.470490
1893.329337	303138.837794	37.475508
1895.067198	303694.747845	37.480525
1896.621251	304252.539703	37.485543
1898.156464	304811.347005	37.490560
1900.364833	305368.130805	37.495578
1902.281800	305938.039532	37.500596
1904.216266	306515.179072	37.505613
1906.310205	307073.088407	37.510631
1907.847924	307645.894414	37.515648
1910.300325	308219.123970	37.520666
1912.116601	308793.651739	37.525684
1913.361111	309365.530475	37.530701
1915.249480	309942.195995	37.535719
1917.203914	310539.567561	37.540736
1919.266510	311124.904557	37.545754
1921.029273	311720.725128	37.550772
1922.515828	312321.692274	37.555789
1924.604925	312901.195600	37.560807
1926.361901	313520.770780	37.565824
1928.150034	314118.395768	37.570842
1930.485998	314726.891710	37.575860
1932.295494	315344.537569	37.580877
1934.417449	315948.539626	37.585895
1936.172394	316581.419174	37.590912
1937.918949	317194.793350	37.595930
1939.532365	317820.677399	37.600948
1941.439413	318464.609412	37.605965
1943.248148	319091.082879	37.610983
1945.196349	319730.552018	37.616000
1947.023043	320373.311018	37.621018
1949.559490	321017.948027	37.626036
1951.684715	321658.408674	37.631053
1953.359208	322293.811135	37.636071
1955.169001	322952.491608	37.641088
1956.854335	323600.243538	37.646106
1959.018945	324245.570834	37.651124
1960.984890	324910.830009	37.656141
1963.289484	325562.796475	37.661159
1965.352546	326227.922779	37.666176
1967.373846	326875.759525	37.671194
1969.903467	327532.210078	37.676212
1971.853186	328187.533739	37.681229
1973.339857	328832.190352	37.686247
1975.311897	329484.017226	37.691264
1977.851968	330133.353052	37.696282
1980.220193	330779.029688	37.701300
1982.609237	331418.374116	37.706317
1984.829321	332046.113363	37.711335
1987.045212	332680.827005	37.716352
1988.994763	333312.050184	37.721370
1991.234601	333938.646997	37.726388
1993.044615	334575.082872	37.731405
1995.071850	335193.628871	37.736423
1997.331469	335823.728149	37.741440
1999.469820	336424.522574	37.746458
2002.024736	337022.040427	37.751476
2004.019170	337616.245798	37.756493
2005.944844	338200.480576	37.761511
2008.184634	338774.197317	37.766528
2010.410150	339347.757585	37.771546
2012.756739	339920.960521	37.776564
2014.329958	340495.075835	37.781581
2016.387858	341068.213154	37.786599
2018.357760	341649.683628	37.791616
2020.092114	342216.669705	37.796634
2022.294810	342798.568640	37.801652
2024.173090	343383.992947	37.806669
2025.822260	343965.058491	37.811687
2027.782326	344552.180040	37.816704
2029.599503	345155.078900	37.821722
2031.431876	345759.337722	37.826740
2033.104725	346373.183444	37.831757
2034.918989	346986.514519	37.836775
2036.976694	347615.275931	37.841792
2038.517918	348236.300684	37.846810
2040.588654	348857.860651	37.851828
2042.163141	349500.229315	37.856845
2044.242599	350137.300140	37.861863
2046.518780	350781.179465	37.866880
2048.111298	351440.188327	37.871898
2049.942206	352093.183225	37.876916
2051.854182	352767.874889	37.881933
2053.543860	353429.932151	37.886951
2055.332911	354106.501170	37.891968
2057.531201	354803.643145	37.896986
2060.023205	355480.247283	37.902004
2061.785688	356172.290046	37.907021
2063.396389	356861.657645	37.912039
2065.724738	357559.364962	37.917056
2067.660784	358269.635297	37.922074
2069.842127	358977.237933	37.927092
2071.742386	359686.322174	37.932109
2073.643465	360391.943280	37.937127
2075.707485	361121.624718	37.942144
2077.215728	361845.628824	37.947162
2079.589435	362574.189932	37.952180
2081.480986	363310.937420	37.957197
2083.106533	364046.828335	37.962215
2085.455442	364787.882975	37.967232
2087.491326	365540.746578	37.972250
2089.640724	366279.142443	37.977268
2091.475474	367027.901155	37.982285
2093.927915	367776.107861	37.987303
2096.370934	368536.069964	37.992320
2098.538859	369288.378017	37.997338
2100.745925	370029.021986	38.002356
2102.946919	370792.681111	38.007373
2105.275343	371543.468833	38.012391
2107.576132	372287.955689	38.017408
2109.906272	373006.325172	38.022426
2112.555209	373713.238475	38.027444
2115.544179	374414.423963	38.032461
2118.011871	375093.418614	38.037479
2120.201755	375772.371283	38.042496
2122.395636	376452.932736	38.047514
2125.072479	377120.034254	38.052532
2126.807090	377792.405954	38.057549
2129.294361	378468.109436	38.062567
2131.821101	379131.672053	38.067584
2133.852505	379803.242576	38.072602
2135.714956	380461.795579	38.077620
2137.319483	381124.106692	38.082637
2139.130437	381806.044232	38.087655
2140.896683	382493.755836	38.092672
2143.038035	383193.558345	38.097690
2145.365980	383882.361269	38.102708
2147.526825	384579.290689	38.107725
2149.356717	385281.813474	38.112743
2151.574178	385979.843280	38.117760
2153.465883	386692.743442	38.122778
2155.441610	387397.222119	38.127796
2157.253618	388115.198785	38.132813
2159.752432	388847.135359	38.137831
2161.592161	389561.093875	38.142848
2163.314790	390308.413346	38.147866
2165.496025	391043.722935	38.152884
2167.379171	391796.630724	38.157901
2169.333269	392556.072116	38.162919
2171.419667	393302.292132	38.167936
2173.422073	394069.923928	38.172954
2175.323294	394835.626984	38.177972
2177.839353	395617.424641	38.182989
2180.019957	396386.131343	38.188007
2182.454739	397155.509196	38.193024
2184.313735	397942.323737	38.198042
2186.954050	398718.948356	38.203060
2189.480005	399500.664744	38.208077
2191.682869	400282.262864	38.213095
2194.071293	401055.648716	38.218112
2195.831172	401839.863960	38.223130
2198.634806	402607.941829	38.228148
2200.914612	403400.334877	38.233165
2202.881767	404182.573823	38.238183
2205.435737	404955.189668	38.243200
2207.609183	405738.210433	38.248218
2209.888789	406514.629207	38.253236
2212.085391	407302.363630	38.258253
2214.623947	408082.568999	38.263271
2217.000418	408847.656673	38.268288
2218.940706	409633.897250	38.273306
2221.031051	410407.120089	38.278324
2223.547680	411198.458927	38.283341
2225.736990	411982.535378	38.288359
2227.935833	412748.984123	38.293376
2230.396476	413537.070489	38.298394
2232.940169	414280.063853	38.303412
2234.984319	415025.299153	38.308429
2236.697136	415775.127838	38.313447
2239.224639	416512.867732	38.318464
2241.585756	417262.212561	38.323482
2244.100057	417995.631939	38.328500
2246.599210	418735.388216	38.333517
2248.593343	419477.842331	38.338535
2251.175775	420216.451713	38.343552
2253.809334	420957.055898	38.348570
2256.073323	421680.281933	38.353588
2258.617723	422412.249325	38.358605
2260.619411	423148.237052	38.363623
2262.995142	423886.062632	38.368640
2265.192658	424630.528876	38.373658
2267.261750	425374.234682	38.378676
2269.060819	426114.925977	38.383693
2271.496958	426864.345014	38.388711
2273.526975	427614.265524	38.393728
2275.530218	428383.251741	38.398746
2277.712781	429158.155563	38.403764
2280.154029	429923.574371	38.408781
2282.160827	430704.835192	38.413799
2283.946350	431483.880523	38.418816
2286.344702	432272.664737	38.423834
2288.327968	433072.071009	38.428852
2290.341397	433879.137169	38.433869
2292.225734	434688.524934	38.438887
2294.496303	435489.821930	38.443904
2297.054414	436306.830357	38.448922
2299.366199	437126.027248	38.453940
2301.765883	437949.530970	38.458957
2304.035549	438787.295746	38.463975
2306.420977	439614.383587	38.468992
2308.680239	440443.890703	38.474010
2310.819263	441277.687654	38.479028
2313.470293	442113.389071	38.484045
2315.378537	442955.003360	38.489063
2317.750254	443800.755249	38.494080
2319.732893	444655.039089	38.499098
2321.781983	445522.631939	38.504116
2324.232703	446380.156302	38.509133
2326.175417	447257.004094	38.514151
2328.477088	448123.942159	38.519168
2330.330187	449012.517302	38.524186
2332.448331	449897.165990	38.529204
2334.940506	450787.832537	38.534221
2337.170571	451690.895349	38.539239
2339.785741	452573.170966	38.544256
2341.583563	453493.573580	38.549274
2343.735911	454406.289936	38.554292
2346.588474	455305.497857	38.559309
2348.729448	456229.257923	38.564327
2350.777784	457148.997775	38.569344
2353.378466	458054.951747	38.574362
2355.575596	458954.766520	38.579380
2358.168117	459842.594111	38.584397
2360.253127	460734.411478	38.589415
2363.144326	461619.732781	38.594432
2365.496327	462506.622752	38.599450
2367.813955	463403.182214	38.604468
2370.125445	464294.192962	38.609485
2372.325281	465192.307478	38.614503
2374.725045	466089.133371	38.619520
2377.193068	466992.373813	38.624538
2379.619854	467901.743254	38.629556
2382.458831	468805.390584	38.634573
2384.460719	469711.411632	38.639591
2387.331667	470604.559998	38.644608
2390.037841	471507.797975	38.649626
2392.104050	472425.195933	38.654644
2394.718707	473337.201707	38.659661
2397.031093	474254.366620	38.664679
2399.254822	475167.763658	38.669696
2401.597320	476094.731889	38.674714
2404.275373	477032.605811	38.679732
2406.543064	477956.462492	38.684749
2408.776627	478891.387836	38.689767
2411.196495	479814.114128	38.694784
2413.598171	480756.690765	38.699802
2415.927825	481705.642622	38.704820
2418.230306	482647.177591	38.709837
2420.395801	483595.552256	38.714855
2423.018473	484538.800342	38.719872
2425.653221	485499.512545	38.724890
2427.944385	486453.769962	38.729908
2430.456839	487395.571377	38.734925
2432.875774	488367.065732	38.739943
2435.629266	489329.515618	38.744960
2438.518393	490288.002897	38.749978
2440.957961	491247.775262	38.754996
2443.908348	492191.158390	38.760013
2446.387067	493129.726104	38.765031
2449.030929	494074.772943	38.770048
2452.047627	495024.698092	38.775066
2454.457974	495959.387303	38.780084
2457.521237	496900.269179	38.785101
2459.874913	497837.436174	38.790119
2462.623221	498761.570225	38.795136
2465.351022	499690.094879	38.800154
2467.355891	500622.725765	38.805172
2470.386583	501543.327402	38.810189
2472.591849	502480.054993	38.815207
2474.928905	503403.898065	38.820224
2477.028053	504339.780619	38.825242
2479.219788	505280.484155	38.830260
2481.951895	506207.730285	38.835277
2484.164116	507149.329643	38.840295
2486.367217	508096.370143	38.845312
2489.466295	509030.044643	38.850330
2491.263342	509947.656153	38.855348
2493.992222	510851.950490	38.860365
2496.166969	511758.656540	38.865383
2498.811719	512660.442261	38.870400
2501.418353	513575.436315	38.875418
2503.725262	514498.238630	38.880436
2506.209702	515402.664886	38.885453
2508.412953	516336.612273	38.890471
2510.633726	517262.086336	38.895488
2513.387441	518188.118959	38.900506
2515.139355	519121.118013	38.905524
2517.804826	520070.325586	38.910541
2520.101828	521032.784198	38.915559
2522.130868	521992.507692	38.920576
2524.534619	522959.862136	38.925594
2527.231486	523943.924588	38.930612
2529.696378	524907.567515	38.935629
2532.120186	525892.958389	38.940647
2535.063136	526878.195254	38.945664
2537.786474	527870.855465	38.950682
2539.748909	528859.400436	38.955700
2542.718126	529863.211647	38.960717
2545.000170	530865.762738	38.965735
2547.023316	531872.718511	38.970752
2549.479848	532889.395081	38.975770
2552.009765	533915.398699	38.980788
2554.871497	534949.072607	38.985805
2557.227552	535979.437518	38.990823
2559.396958	537005.030527	38.995840
2562.393820	538041.678152	39.000858
2564.858168	539083.019736	39.005876
2567.276742	540144.766265	39.010893
2569.994720	541197.428191	39.015911
2572.452973	542249.049632	39.020928
2575.199072	543314.473883	39.025946
2577.487184	544386.533028	39.030964
2580.138492	545444.116074	39.035981
2582.839253	546521.671896	39.040999
2585.531574	547592.457967	39.046016
2588.470171	548658.091028	39.051034
2590.984598	549727.131758	39.056052
2594.177553	550784.411540	39.061069
2597.402930	551844.317436	39.066087
2600.347880	552899.112062	39.071104
2602.996831	553946.386801	39.076122
2605.370789	555017.294284	39.081140
2607.754884	556068.367671	39.086157
2610.697782	557127.451933	39.091175
2613.330169	558191.880061	39.096192
2616.350964	559228.778753	39.101210
2618.746223	560293.630278	39.106228
2621.238354	561336.982718	39.111245
2624.412233	562396.206214	39.116263
2626.968112	563442.693890	39.121280
2629.313464	564485.065824	39.126298
2631.349041	565520.377320	39.131316
2634.016415	566535.064063	39.136333
2636.681768	567558.907973	39.141351
2639.015866	568586.139936	39.146368
2641.603503	569616.156990	39.151386
2643.802544	570649.369013	39.156404
2646.573560	571692.586523	39.161421
2648.780217	572741.685327	39.166439
2650.820334	573797.599221	39.171456
2653.477607	574856.328982	39.176474
2655.791003	575938.004654	39.181492
2657.909099	577010.289163	39.186509
2660.771085	578095.645994	39.191527
2663.225024	579194.117694	39.196544
2665.813448	580290.813366	39.201562
2668.235385	581409.503514	39.206580
2670.941487	582524.783459	39.211597
2673.833309	583652.463581	39.216615
2676.098231	584772.776534	39.221632
2678.881367	585913.749953	39.226650
2681.263577	587065.259521	39.231668
2684.456361	588207.298382	39.236685
2687.207313	589346.146440	39.241703
2689.801674	590506.107938	39.246720
2693.220581	591649.481510	39.251738
2695.919289	592800.682786	39.256756
2698.225894	593956.296782	39.261773
2700.948469	595126.101190	39.266791
2703.717795	596295.029261	39.271808
2706.662446	597460.004076	39.276826
2709.156699	598630.597114	39.281844
2711.827830	599799.589409	39.286861
2714.661268	600980.300226	39.291879
2717.511178	602163.289498	39.296896
2720.239952	603342.072735	39.301914
2722.905533	604525.048852	39.306932
2725.659011	605710.138538	39.311949
2728.513617	606901.841718	39.316967
2730.912791	608101.001385	39.321984
2733.601504	609297.232051	39.327002
2736.104015	610504.771329	39.332020
2738.939790	611701.169457	39.337037
2742.242064	612900.409570	39.342055
2744.823460	614114.494168	39.347072
2747.854547	615312.368534	39.352090
2750.584841	616525.161693	39.357108
2753.265118	617728.831152	39.362125
2756.529048	618938.465846	39.367143
2759.186485	620146.220319	39.372160
2762.390013	621340.654263	39.377178
2765.050099	622544.592251	39.382196
2768.085384	623733.443151	39.387213
2770.956338	624941.222887	39.392231
2773.854602	626147.063123	39.397248
2776.146671	627332.892878	39.402266
2778.875778	628497.091982	39.407284
2781.835424	629653.134206	39.412301
2784.632506	630812.721912	39.417319
2787.200898	631974.916283	39.422336
2789.974077	633127.013257	39.427354
2792.555745	634299.179346	39.432372
2794.754009	635470.330482	39.437389
2797.949306	636650.010921	39.442407
2800.172049	637837.555845	39.447424
2803.283197	639016.181344	39.452442
2805.865225	640209.376995	39.457460
2808.346769	641419.308426	39.462477
2811.069123	642626.711028	39.467495
2813.497954	643845.139695	39.472512
2816.310359	645059.367376	39.477530
2819.046080	646287.769264	39.482548
2821.944816	647512.852745	39.487565
2824.608404	648752.529039	39.492583
2827.519314	650002.623439	39.497600
2830.153127	651247.276434	39.502618
2833.232336	652502.109418	39.507636
2835.925546	653754.856207	39.512653
2838.941650	655010.227312	39.517671
2841.956855	656279.431970	39.522688
2844.925273	657542.554077	39.527706
2847.634266	658818.949666	39.532724
2850.437040	660094.514104	39.537741
2853.353940	661371.931496	39.542759
2856.009088	662669.380478	39.547776
2858.791777	663950.957309	39.552794
2861.773052	665252.479356	39.557812
2864.256076	666541.670698	39.562829
2867.346504	667842.620787	39.567847
2870.074047	669160.662254	39.572864
2872.966379	670471.479794	39.577882
2875.699813	671796.411524	39.582900
2878.180325	673121.099620	39.587917
2881.443569	674434.033492	39.592935
2884.521330	675771.762875	39.597952
2887.502234	677109.961717	39.602970
2890.189584	678437.235134	39.607988
2892.875632	679776.339436	39.613005
2895.961726	681111.653274	39.618023
2898.690971	682466.201671	39.623040
2901.773835	683812.493602	39.628058
2904.763971	685157.211489	39.633076
2907.201117	686527.091214	39.638093
2910.160316	687888.632927	39.643111
2912.977351	689252.225662	39.648128
2915.872088	690616.639335	39.653146
2919.026435	691990.672447	39.658164
2921.858926	693360.133392	39.663181
2925.080305	694723.959817	39.668199
2927.730049	696102.053529	39.673216
2930.972261	697456.031697	39.678234
2933.793521	698804.221305	39.683252
2936.232483	700131.302187	39.688269
2939.452414	701459.831421	39.693287
2942.470413	702791.115106	39.698304
2945.330413	704120.734527	39.703322
2948.646767	705445.761352	39.708340
2951.235398	706779.920010	39.713357
2954.292368	708115.424879	39.718375
2956.978315	709457.913674	39.723392
2960.132604	710807.635041	39.728410
2963.356699	712153.268876	39.733428
2965.579547	713516.773813	39.738445
2968.770436	714869.650360	39.743463
2971.446057	716231.548983	39.748480
2974.555110	717603.835870	39.753498
2977.315462	718973.631966	39.758516
2979.834380	720359.709252	39.763533
2982.716415	721741.636260	39.768551
2985.494130	723150.536264	39.773568
2988.150507	724549.677209	39.778586
2991.342810	725970.674289	39.783604
2994.205673	727402.596392	39.788621
2997.339079	728832.985466	39.793639
3000.244896	730266.470074	39.798656
3003.694286	731713.236009	39.803674
3006.718154	733140.659424	39.808692
3009.382078	734586.746229	39.813709
3012.566140	736025.326832	39.818727
3015.828802	737481.052373	39.823744
3019.206361	738925.638160	39.828762
3022.156490	740378.122594	39.833780
3025.235507	741835.051934	39.838797
3028.580889	743291.665844	39.843815
3031.436791	744753.761754	39.848832
3034.436786	746217.136553	39.853850
3037.599543	747677.941598	39.858868
3040.613017	749147.513284	39.863885
3043.294514	750621.591226	39.868903
3046.324012	752100.006473	39.873920
3049.278086	753587.948817	39.878938
3052.268884	755067.915444	39.883956
3055.239643	756554.587701	39.888973
3058.928015	758043.897670	39.893991
3062.564696	759525.051147	39.899008
3065.885711	760998.342931	39.904026
3069.553176	762466.712905	39.909044
3073.070807	763924.150146	39.914061
3076.836921	765374.967618	39.919079
3080.381107	766826.031810	39.924096
3083.454489	768263.820159	39.929114
3087.030810	769697.754555	39.934132
3089.889554	771132.957247	39.939149
3093.135443	772557.008021	39.944167
3096.360992	773983.338981	39.949184
3099.212805	775394.529660	39.954202
3102.024169	776769.374235	39.959220
3105.019303	778146.724431	39.964237
3108.090970	779514.770598	39.969255
3111.093092	780893.166056	39.974272
3113.914591	782263.185742	39.979290
3117.356908	783637.251262	39.984308
3119.901470	785015.569669	39.989325
3123.046956	786400.725063	39.994343
3126.396398	787784.252146	39.999360
3129.489767	789180.195330	40.004378
3132.641680	790566.739747	40.009396
3135.345426	791965.725228	40.014413
3138.153678	793365.491340	40.019431
3140.868869	794787.418597	40.024448
3143.280083	796217.038295	40.029466
3146.241283	797660.414731	40.034484
3149.196682	799117.584236	40.039501
3152.274266	800575.501769	40.044519
3154.813424	802056.729343	40.049536
3157.709295	803556.843571	40.054554
3160.545834	805045.931907	40.059572
3163.345250	806560.412320	40.064589
3166.311415	808080.488833	40.069607
3168.982253	809622.798219	40.074624
3172.090146	811175.426970	40.079642
3175.311538	812737.445179	40.084660
3178.136897	814322.700289	40.089677
3181.424507	815897.103544	40.094695
3184.696314	817486.460786	40.099712
3187.446316	819086.504127	40.104730
3190.917524	820687.598293	40.109748
3194.136979	822297.026848	40.114765
3197.174500	823904.824737	40.119783
3200.577154	825518.940599	40.124800
3203.517758	827157.782809	40.129818
3206.938378	828779.517830	40.134836
3210.030084	830416.586070	40.139853
3213.419282	832064.046957	40.144871
3216.484305	833706.273654	40.149888
3219.408112	835365.332179	40.154906
3222.573280	837025.621900	40.159924
3225.740144	838687.716191	40.164941
3228.833161	840360.426700	40.169959
3232.163354	842032.265590	40.174976
3235.592427	843713.559268	40.179994
3238.716945	845380.364024	40.185012
3241.821658	847066.547813	40.190029
3245.143178	848762.534417	40.195047
3248.457552	850455.146646	40.200064
3251.171114	852157.494791	40.205082
3254.769553	853862.522176	40.210100
3258.158750	855572.642946	40.215117
3261.454509	857279.683910	40.220135
3264.745621	858986.733602	40.225152
3268.077785	860678.369173	40.230170
3271.509615	862337.535191	40.235188
3274.834155	863989.482318	40.240205
3277.456877	865641.290221	40.245223
3280.593344	867300.883838	40.250240
3283.761439	868959.334385	40.255258
3287.487152	870614.615756	40.260276
3290.565885	872268.482546	40.265293
3294.115241	873924.128903	40.270311
3297.999510	875586.603024	40.275328
3301.219262	877252.974594	40.280346
3304.589623	878907.250151	40.285364
3308.109108	880579.099335	40.290381
3311.109403	882247.273666	40.295399
3314.208311	883916.883377	40.300416
3317.458844	885597.666097	40.305434
3321.163374	887284.347494	40.310452
3324.376872	888971.293385	40.315469
3326.868556	890675.322833	40.320487
3330.351324	892372.504193	40.325504
3333.374381	894088.343039	40.330522
3337.400371	895788.941634	40.335540
3340.884089	897506.364466	40.340557
3344.018372	899213.019469	40.345575
3347.801521	900939.454728	40.350592
3351.016516	902675.848611	40.355610
3354.302580	904392.159072	40.360628
3357.375229	906142.505400	40.365645
3360.086316	907886.014678	40.370663
3363.427055	909634.441103	40.375680
3366.250055	911400.849728	40.380698
3369.294937	913171.262488	40.385716
3372.863167	914960.217963	40.390733
3376.080722	916741.158117	40.395751
3379.573305	918530.487659	40.400768
3382.850019	920330.774025	40.405786
3386.416133	922131.081080	40.410804
3389.984918	923940.562817	40.415821
3393.467547	925745.614216	40.420839
3397.155595	927542.834576	40.425856
3400.798855	929360.428624	40.430874
3404.183620	931173.230740	40.435892
3407.946399	932982.761826	40.440909
3410.747402	934790.782272	40.445927
3414.573409	936600.490879	40.450944
3417.751742	938421.442552	40.455962
3421.016997	940247.954668	40.460980
3424.577739	942071.575981	40.465997
3428.215239	943900.844207	40.471015
3431.776643	945705.512965	40.476032
3435.271626	947543.724941	40.481050
3438.687774	949360.492376	40.486068
3442.556057	951196.667918	40.491085
3445.566509	953062.253318	40.496103
3449.161349	954937.893369	40.501120
3452.238259	956801.992547	40.506125
3455.650652	958607.757715	40.511130
3459.553054	960349.597474	40.516135
3462.450406	962031.447484	40.521140
3465.840636	963634.210683	40.526144
3468.692673	965165.273075	40.531149
3471.533480	966625.384446	40.536154
3474.613007	968006.143412	40.541159
3477.461500	969324.508295	40.546164
3480.135167	970542.770683	40.551168
3482.768015	971705.744101	40.556173
3485.131016	972786.818679	40.561178
3487.433150	973803.008487	40.566183
3489.672833	974736.077464	40.571188
3492.079518	975603.806669	40.576192
3494.247021	976411.569629	40.581197
3496.417935	977140.208252	40.586202
3498.580227	977802.059057	40.591207
3500.211291	978417.739296	40.596212
3502.003034	978962.249539	40.601216
3503.701765	979452.542460	40.606221
3505.134684	979892.370961	40.611226
3506.849620	980279.896229	40.616231
3507.913615	980621.144419	40.621236
3509.452320	980898.461438	40.626240
3510.721670	981145.068499	40.631245
3512.447238	981350.208256	40.636250
3513.530332	981501.776501	40.641255
3514.758057	981629.407266	40.646260
3515.750478	981707.794811	40.651264
3516.751053	981756.806942	40.656269
3517.722268	981761.227634	40.661274
3518.836736	981728.736769	40.666279
3519.671548	981679.801433	40.671284
3520.329305	981591.275477	40.676288
3520.947833	981484.896013	40.681293
3521.811887	981345.486728	40.686298
3522.786419	981177.557613	40.691303
3523.235938	980991.560007	40.696308
3524.028030	980791.540899	40.701312
3524.384214	980557.329841	40.706317
3524.778727	980316.465192	40.711322
3525.594354	980050.334153	40.716327
3525.906330	979766.510084	40.721332
3526.651414	979465.123311	40.726336
3527.033237	979145.233075	40.731341
3527.324889	978817.529507	40.736346
3528.020875	978470.991078	40.741351
3528.138608	978122.186802	40.746356
3528.579276	977757.681613	40.751360
3528.981459	977372.553564	40.756365
3529.245742	976979.219113	40.761370
3529.748744	976571.361186	40.766375
3529.775743	976163.848444	40.771380
3530.356722	975734.134693	40.776384
3530.633324	975291.349445	40.781389
3530.736405	974852.076828	40.786394
3531.188856	974403.232921	40.791399
3530.920606	973949.493186	40.796404
3531.184673	973482.140387	40.801408
3531.651016	973017.158246	40.806413
3531.864330	972537.617932	40.811418
3532.149797	972059.784641	40.816423
3531.958187	971575.736350	40.821428
3532.375607	971072.869645	40.826432
3532.267595	970584.323757	40.831437
3532.549214	970072.690402	40.836442
3532.403946	969570.178995	40.841447
3532.635174	969053.671421	40.846452
3532.530559	968534.435945	40.851456
3532.605885	968022.263555	40.856461
3532.797099	967504.155958	40.861466
3532.708835	966976.852589	40.866471
3532.968322	966460.106631	40.871476
3533.064033	965917.704086	40.876480
3533.259416	965399.503637	40.881485
3533.074787	964858.712602	40.886490
3533.628080	964305.215709	40.891495
3533.698648	963759.970845	40.896500
3533.430628	963207.976849	40.901504
3533.708264	962664.061202	40.906509
3533.695873	962116.128895	40.911514
3533.312651	961555.280990	40.916519
3533.545851	960997.798981	40.921524
3533.800244	960437.027048	40.926528
3533.552596	959877.755550	40.931533
3533.830300	959327.842894	40.936538
3533.987826	958769.080323	40.941543
3533.896362	958205.700685	40.946548
3533.844451	957640.691263	40.951552
3533.785975	957070.237244	40.956557
3533.945612	956496.160977	40.961562
3534.018003	955927.531869	40.966567
3534.001845	955361.410723	40.971572
3534.292407	954774.004006	40.976576
3533.954342	954184.389542	40.981581
3533.752202	953625.287814	40.986586
3533.757014	953040.499262	40.991591
3533.571322	952468.925373	40.996596
3533.943281	951886.899881	41.001600
3534.051944	951314.082467	41.006605
3534.115739	950734.249889	41.011610
3534.076303	950162.797957	41.016615
3533.921011	949604.119416	41.021620
3534.065957	949022.180640	41.026624
3534.481387	948450.269601	41.031629
3534.341897	947870.926736	41.036634
3534.448024	947291.476312	41.041639
3534.281475	946712.198245	41.046644
3534.066166	946135.734206	41.051648
3534.060697	945564.242564	41.056653
3533.969797	944977.768436	41.061658
3534.120876	944400.951436	41.066663
3533.944681	943818.284978	41.071668
3534.154282	943242.860301	41.076672
3533.977428	942670.693618	41.081677
3533.982549	942083.490614	41.086682
3533.943582	941500.539101	41.091687
3533.907767	940926.239459	41.096692
3534.139707	940335.637983	41.101696
3534.227757	939754.767942	41.106701
3533.905291	939167.769562	41.111706
3534.241608	938581.455068	41.116711
3534.173754	937996.102106	41.121716
3534.185499	937404.438411	41.126720
3534.287309	936814.513937	41.131725
3534.087637	936232.724886	41.136730
3533.827616	935634.962000	41.141735
3533.852419	935046.769239	41.146740
3534.141945	934450.791540	41.151744
3534.314136	933868.196744	41.156749
3533.762075	933272.132971	41.161754
3534.231591	932684.750970	41.166759
3533.963571	932093.878650	41.171764
3533.732339	931490.169035	41.176768
3534.034680	930904.248757	41.181773
3533.817701	930315.952221	41.186778
3534.388132	929713.534683	41.191783
3533.886646	929123.714046	41.196788
3533.576145	928511.420262	41.201792
3534.078369	927923.599546	41.206797
3533.896076	927336.791169	41.211802
3534.044162	926732.762654	41.216807
3534.144541	926131.267742	41.221812
3534.197728	925538.072297	41.226816
3534.663457	924931.863879	41.231821
3534.369648	924320.814989	41.236826
3534.447406	923707.422197	41.241831
3533.731223	923105.629958	41.246836
3534.040274	922503.979710	41.251840
3534.121468	921904.704662	41.256845
3533.867296	921302.054471	41.261850
3534.195176	920692.505510	41.266855
3533.946067	920089.718768	41.271860
3534.144820	919482.940534	41.276864
3534.144082	918875.839575	41.281869
3534.113429	918260.689828	41.286874
3534.051725	917649.035784	41.291879
3534.024377	917047.219074	41.296884
3534.063121	916432.042390	41.301888
3533.763154	915819.549055	41.306893
3533.864639	915212.790537	41.311898
3533.977436	914607.888051	41.316903
3533.545606	914003.300285	41.321908
3533.770977	913377.154784	41.326912
3533.854908	912772.439020	41.331917
3533.701005	912172.127800	41.336922
3533.930354	911553.382292	41.341927
3533.691227	910956.131396	41.346932
3533.620197	910340.287008	41.351936
3533.950175	909731.821579	41.356941
3533.569154	909122.639261	41.361946
3533.896594	908504.593960	41.366951
3533.881713	907894.056775	41.371956
3533.779557	907281.828088	41.376960
3533.863909	906662.075628	41.381965
3533.556607	906054.181343	41.386970
3533.762844	905430.509617	41.391975
3533.784561	904813.647255	41.396980
3533.647167	904195.875434	41.401984
3533.946696	903587.704017	41.406989
3533.960647	902976.716992	41.411994
3534.114747	902349.524891	41.416999
3534.044464	901732.240482	41.422004
3533.891017	901111.620641	41.427008
3534.200571	900485.640624	41.432013
3533.858212	899863.756466	41.437018
3533.778505	899228.338628	41.442023
3533.779686	898613.787980	41.447028
3533.757038	897982.950922	41.452032
3533.638909	897356.308953	41.457037
3533.440669	896741.684642	41.462042
3533.688188	896107.211016	41.467047
3533.712001	895497.340012	41.472052
3533.650173	894878.722057	41.477056
3533.559659	894259.365046	41.482061
3533.340017	893629.041929	41.487066
3533.744881	892990.616738	41.492071
3533.436009	892380.564121	41.497076
3533.611838	891751.898728	41.502080
3533.712558	891124.723802	41.507085
3532.959992	890508.165389	41.512090
3533.007052	889880.766352	41.517095
3532.956684	889261.826179	41.522100
3533.293689	888653.199470	41.527104
3533.169360	888027.464570	41.532109
3533.217421	887414.596201	41.537114
3532.994231	886785.743835	41.542119
3532.956514	886172.854628	41.547124
3533.165564	885550.180314	41.552128
3532.824763	884931.888196	41.557133
3532.758350	884321.227009	41.562138
3532.597784	883696.383291	41.567143
3532.995869	883080.671520	41.572148
3533.003934	882462.927560	41.577152
3533.199814	881849.734172	41.582157
3532.816632	881230.182848	41.587162
3533.004953	880608.143371	41.592167
3532.904078	879993.061618	41.597172
3532.828122	879366.091263	41.602176
3533.044683	878747.433300	41.607181
3532.792221	878132.181568	41.612186
3533.083592	877502.332467	41.617191
3532.578323	876885.733211	41.622196
3532.684592	876261.307132	41.627200
3532.629610	875641.204718	41.632205
3532.514052	875018.914366	41.637210
3532.535345	874399.152979	41.642215
3532.708432	873788.416124	41.647220
3532.368434	873168.296343	41.652224
3532.515550	872542.887741	41.657229
3532.040977	871932.845882	41.662234
3532.231804	871319.135190	41.667239
3532.335722	870704.502715	41.672244
3532.472484	870086.598993	41.677248
3532.332370	869473.045398	41.682253
3531.893138	868860.547309	41.687258
3532.393161	868238.702012	41.692263
3532.122425	867627.601748	41.697268
3532.224116	867013.074643	41.702272
3532.692011	866386.867818	41.707277
3532.042815	865767.389415	41.712282
3531.951274	865143.770231	41.717287
3532.148952	864542.278418	41.722292
3532.158937	863923.954440	41.727296
3532.182767	863301.678934	41.732301
3532.196707	862680.312513	41.737306
3532.318656	862052.450964	41.742311
3532.000024	861443.548392	41.747316
3531.927675	860825.893251	41.752320
3531.984288	860203.390733	41.757325
3531.970361	859583.655374	41.762330
3532.103406	858969.761796	41.767335
3532.071859	858349.223269	41.772340
3531.887188	857730.203463	41.777344
3532.525846	857104.562316	41.782349
3531.952615	856486.260749	41.787354
3532.053587	855859.417031	41.792359
3531.798684	855244.339943	41.797364
3531.938994	854628.939171	41.802368
3532.262918	854008.386242	41.807373
3532.172326	853384.338624	41.812378
3532.186459	852753.203456	41.817383
3531.924408	852135.870547	41.822388
3531.658901	851518.865840	41.827392
3531.819670	850896.373036	41.832397
3531.425479	850280.532250	41.837402
3531.689961	849655.755390	41.842407
3531.550533	849047.440188	41.847412
3531.768569	848429.850728	41.852416
3532.030669	847805.083032	41.857421
3531.595277	847191.767484	41.862426
3531.489758	846561.873224	41.867431
3531.412158	845943.698354	41.872436
3531.250164	845332.589058	41.877440
3531.456547	844716.290491	41.882445
3531.238104	844105.266037	41.887450
3531.367849	843492.465919	41.892455
3531.456191	842872.010778	41.897460
3531.089141	842262.879425	41.902464
3531.340441	841638.765879	41.907469
3531.488407	841024.552753	41.912474
3531.408908	840406.321085	41.917479
3531.618095	839795.927114	41.922484
3531.561501	839169.184558	41.927488
3531.655525	838545.036532	41.932493
3531.289188	837932.220702	41.937498
3531.182107	837307.010019	41.942503
3531.297108	836690.041556	41.947508
3530.970890	836076.357349	41.952512
3531.114079	835453.019941	41.957517
3531.031474	834848.348743	41.962522
3531.034685	834230.527526	41.967527
3530.851465	833611.019241	41.972532
3531.137151	832997.667457	41.977536
3531.468801	832380.148959	41.982541
3531.193410	831769.021204	41.987546
3531.714901	831135.582667	41.992551
3531.510881	830519.441986	41.997556
3531.037710	829889.127094	42.002560
3531.057185	829254.857370	42.007565
3530.896907	828645.123686	42.012570
3530.767974	828027.511898	42.017575
3530.892287	827418.053963	42.022580
3530.407394	826802.242818	42.027584
3530.785231	826185.786396	42.032589
3530.886219	825577.625979	42.037594
3531.057019	824956.006766	42.042599
3531.137007	824345.291734	42.047604
3530.747898	823725.459492	42.052608
3530.946425	823097.842502	42.057613
3530.818602	822497.549538	42.062618
3530.512891	821865.940967	42.067623
3530.145030	821255.503706	42.072628
3530.078920	820652.391390	42.077632
3530.688698	820029.546130	42.082637
3530.178250	819426.299824	42.087642
3530.294175	818816.141272	42.092647
3529.905729	818208.752098	42.097652
3530.216612	817593.898204	42.102656
3530.144586	816992.557033	42.107661
3530.059627	816389.206352	42.112666
3530.214646	815779.398147	42.117671
3530.104325	815173.886337	42.122676
3530.234635	814569.110594	42.127680
3530.434509	813951.247330	42.132685
3530.086149	813355.156754	42.137690
3530.065103	812735.505585	42.142695
3530.112567	812131.209206	42.147700
3530.175092	811531.263062	42.152704
3530.371915	810902.640257	42.157709
3529.745004	810299.126936	42.162714
3530.047657	809680.706332	42.167719
3529.589025	809083.129277	42.172724
3530.024671	808480.888587	42.177728
3530.064226	807870.577772	42.182733
3529.626818	807267.692351	42.187738
3529.715579	806654.519760	42.192743
3529.722217	806060.370062	42.197748
3529.539732	805448.017153	42.202752
3529.739772	804845.298276	42.207757
3529.682607	804253.550811	42.212762
3529.497725	803629.122932	42.217767
3529.557289	803028.768104	42.222772
3529.379711	802441.395191	42.227776
3529.765246	801834.554736	42.232781
3529.443810	801239.943952	42.237786
3529.247797	800635.009526	42.242791
3529.404644	800027.361997	42.247796
3529.464891	799437.435527	42.252800
3529.512780	798825.972586	42.257805
3529.235818	798236.001094	42.262810
3529.219959	797638.967051	42.267815
3529.213542	797034.175587	42.272820
3528.985611	796438.006747	42.277824
3529.220663	795840.186212	42.282829
3529.300985	795247.347425	42.287834
3529.122009	794644.439146	42.292839
3529.257354	794051.047448	42.297844
3529.190747	793447.771175	42.302848
3529.012947	792849.961279	42.307853
3529.006939	792260.271755	42.312858
3529.063493	791661.878562	42.317863
3528.913205	791062.978548	42.322868
3529.044777	790472.034862	42.327872
3529.154001	789873.382247	42.332877
3528.770243	789280.609066	42.337882
3528.866563	788678.270981	42.342887
3528.946309	788082.714205	42.347892
3528.491046	787487.002096	42.352896
3528.597184	786895.321264	42.357901
3528.346038	786309.156622	42.362906
3528.710954	785722.101181	42.367911
3528.661176	785131.971301	42.372916
3528.653644	784546.897938	42.377920
3528.935526	783950.468685	42.382925
3528.524743	783362.663096	42.387930
3528.466097	782762.406924	42.392935
3528.712100	782171.244360	42.397940
3528.713441	781574.369948	42.402944
3528.625607	780986.265116	42.407949
3528.404251	780400.151689	42.412954
3528.426745	779802.979060	42.417959
3528.731183	779208.709811	42.422964
3528.226894	778626.436177	42.427968
3528.220850	778022.429897	42.432973
3528.166594	777447.611203	42.437978
3528.341076	776867.934292	42.442983
3528.108036	776274.007966	42.447988
3527.969727	775677.949671	42.452992
3528.165160	775087.151015	42.457997
3527.675070	774517.097311	42.463002
3527.954258	773917.230047	42.468007
3527.951651	773342.718222	42.473012
3527.696809	772763.181867	42.478016
3528.031433	772173.256307	42.483021
3527.697256	771594.133493	42.488026
3527.970603	771016.535845	42.493031
3527.749313	770434.938325	42.498036
3527.779772	769850.591876	42.503040
3527.880747	769271.014879	42.508045
3527.580436	768703.432796	42.513050
3527.440087	768110.158932	42.518055
3527.763010	767542.874111	42.523060
3527.459936	766967.373941	42.528064
3527.711790	766389.615257	42.533069
3527.429160	765814.564359	42.538074
3527.476533	765237.983264	42.543079
3527.449961	764654.961964	42.548084
3527.330584	764080.981730	42.553088
3527.533395	763506.507977	42.558093
3527.746067	762943.279328	42.563098
3527.756912	762356.916863	42.568103
3528.041964	761773.371204	42.573108
3527.701889	761196.347415	42.578112
3527.208898	760610.131828	42.583117
3526.888781	760034.297838	42.588122
3526.958134	759467.627045	42.593127
3527.099129	758895.179007	42.598132
3526.905586	758330.490401	42.603136
3527.218950	757760.344500	42.608141
3527.220335	757193.564290	42.613146
3526.895571	756613.325818	42.618151
3526.970032	756043.831953	42.623156
3527.051397	755481.549322	42.628160
3527.118564	754910.343251	42.633165
3526.674106	754339.971536	42.638170
3526.962622	753778.021604	42.643175
3526.983823	753207.732733	42.648180
3527.109552	752647.949223	42.653184
3527.056538	752071.960077	42.658189
3526.700482	751513.953633	42.663194
3526.661492	750940.938844	42.668199
3527.053617	750370.919185	42.673204
3526.809388	749801.558713	42.678208
3527.129862	749224.897687	42.683213
3526.473228	748666.094274	42.688218
3526.545571	748090.329589	42.693223
3526.396058	747536.199414	42.698228
3526.534066	746985.636815	42.703232
3526.725530	746415.607160	42.708237
3526.711860	745861.186118	42.713242
3526.349808	745290.031998	42.718247
3526.560366	744719.875030	42.723252
3526.611711	744166.113196	42.728256
3526.546905	743605.065802	42.733261
3526.521545	743033.343293	42.738266
3526.256429	742468.491791	42.743271
3526.469945	741911.527321	42.748276
3526.256618	741356.574039	42.753280
3526.675039	740784.018801	42.758285
3526.475705	740234.373884	42.763290
3526.078865	739667.514227	42.768295
3526.161278	739106.615451	42.773300
3526.297008	738556.895615	42.778304
3526.054483	737989.246423	42.783309
3526.109926	737431.251075	42.788314
3526.119960	736878.567284	42.793319
3526.373648	736315.067336	42.798324
3525.809643	735758.346803	42.803329
3525.901818	735196.081811	42.808333
3525.792377	734654.249334	42.813338
3526.154851	734100.026277	42.818343
3526.136132	733540.187797	42.823348
3526.149452	732992.678801	42.828353
3525.931502	732422.501195	42.833357
3525.966923	731877.832959	42.838362
3525.680196	731330.707569	42.843367
3525.968788	730777.159111	42.848372
3525.737359	730222.176096	42.853377
3525.592149	729662.881846	42.858381
3525.465625	729115.529578	42.863386
3525.356813	728567.196389	42.868391
3525.788274	728018.733926	42.873396
3525.544682	727482.187339	42.878401
3525.341006	726926.726443	42.883405
3525.225762	726377.999093	42.888410
3525.426310	725836.116509	42.893415
3525.791545	725303.236258	42.898420
3525.025182	724754.065120	42.903425
3525.308447	724210.227526	42.908429
3525.501933	723660.720178	42.913434
3525.186894	723117.903427	42.918439
3525.097556	722569.858126	42.923444
3525.081394	722030.387791	42.928449
3525.171237	721496.217196	42.933453
3525.363949	720954.757386	42.938458
3524.841327	720409.368872	42.943463
3525.329610	719873.637413	42.948468
3524.787251	719339.832134	42.953473
3524.966121	718792.184728	42.958477
3524.991160	718264.907090	42.963482
3524.994969	717722.673540	42.968487
3524.761406	717181.437071	42.973492
3524.524234	716648.944414	42.978497
3524.683341	716116.846147	42.983501
3524.707082	715582.703506	42.988506
3524.763404	715047.628369	42.993511
3524.576908	714518.860716	42.998516
3524.281393	713992.310864	43.003521
3524.622532	713457.978835	43.008525
3524.444551	712938.239282	43.013530
3524.130315	712406.681411	43.018535
3524.221171	711883.754571	43.023540
3524.273539	711363.184014	43.028545
3524.297144	710829.583514	43.033549
3524.371184	710297.777212	43.038554
3524.337779	709780.201291	43.043559
3524.561425	709249.147596	43.048564
3524.255817	708720.236065	43.053569
3524.420569	708192.353225	43.058573
3524.304740	707667.464490	43.063578
3523.956953	707149.782453	43.068583
3523.959702	706628.483828	43.073588
3523.993400	706111.666953	43.078593
3524.315670	705588.909830	43.083597
3524.099783	705068.050286	43.088602
3523.726468	704544.553783	43.093607
3524.056444	704029.100719	43.098612
3523.696742	703504.942695	43.103617
3523.968991	702978.459265	43.108621
3524.001382	702473.445494	43.113626
3523.675890	701951.124828	43.118631
3523.744209	701432.580767	43.123636
3523.836763	700920.510525	43.128641
3523.717977	700396.520706	43.133645
3523.627948	699884.917543	43.138650
3523.561558	699370.547051	43.143655
3523.800958	698857.187388	43.148660
3523.402256	698357.127010	43.153665
3523.664760	697832.321639	43.158669
3523.607246	697320.214760	43.163674
3523.556349	696808.225972	43.168679
3523.597120	696298.379042	43.173684
3523.553921	695790.107782	43.178689
3523.934965	695276.464577	43.183693
3523.916640	694763.555728	43.188698
3523.495985	694246.707806	43.193703
3523.389465	693721.819646	43.198708
3522.900067	693227.002764	43.203713
3523.284854	692720.122826	43.208717
3523.205111	692211.602222	43.213722
3522.894044	691714.581623	43.218727
3523.320953	691207.359493	43.223732
3523.159240	690702.298233	43.228737
3522.907193	690194.388203	43.233741
3523.180964	689694.070744	43.238746
3522.747335	689203.448318	43.243751
3522.825864	688679.922739	43.248756
3523.039554	688199.633226	43.253761
3523.408238	687697.844611	43.258765
3523.210143	687196.871201	43.263770
3522.583777	686682.854414	43.268775
3522.514689	686187.326891	43.273780
3522.740095	685697.794060	43.278785
3522.879683	685193.665358	43.283789
3522.658530	684704.403844	43.288794
3522.479695	684210.578676	43.293799
3523.111405	683715.343664	43.298804
3522.699580	683223.446083	43.303809
3522.783781	682727.653289	43.308813
3522.713572	682231.212572	43.313818
3522.377899	681737.478997	43.318823
3522.888363	681239.441150	43.323828
3522.514432	680759.504627	43.328833
3522.534327	680253.827804	43.333837
3522.161538	679763.330678	43.338842
3522.308099	679276.454188	43.343847
3522.279452	678782.160154	43.348852
3521.926633	678302.639371	43.353857
3522.151400	677816.369615	43.358861
3522.019870	677329.088877	43.363866
3522.045965	676846.089869	43.368871
3522.085462	676354.892391	43.373876
3522.026530	675883.914791	43.378881
3521.749900	675393.666988	43.383885
3521.905230	674917.720590	43.388890
3521.818698	674440.794443	43.393895
3522.202915	673958.331384	43.398900
3521.695151	673480.630587	43.403905
3521.682859	672997.886482	43.408909
3521.920430	672520.358169	43.413914
3521.657759	672057.396039	43.418919
3521.802258	671576.595470	43.423924
3521.765550	671109.909001	43.428929
3521.830380	670617.308041	43.433933
3521.609942	670136.496009	43.438938
3521.697279	669677.195624	43.443943
3521.901759	669189.930680	43.448948
3521.993821	668726.743885	43.453953
3522.202183	668235.888728	43.458957
3521.774489	667755.988062	43.463962
3521.572179	667288.941221	43.468967
3521.838990	666807.028693	43.473972
3521.712789	666335.582920	43.478977
3521.711682	665855.862436	43.483981
3521.546771	665381.233617	43.488986
3521.402970	664914.209743	43.493991
3521.448720	664430.568481	43.498996
3521.491339	663962.468510	43.504001
3521.405440	663499.656020	43.509005
3521.392994	663029.923343	43.514010
3521.124937	662561.408799	43.519015
3521.254771	662088.113026	43.524020
3521.118448	661633.651960	43.529025
3521.434366	661167.963856	43.534029
3521.063307	660693.237840	43.539034
3521.124034	660238.278103	43.544039
3521.287064	659760.819862	43.549044
3521.144414	659305.152203	43.554049
3521.149256	658836.060697	43.559053
3521.211367	658374.424353	43.564058
3521.304494	657907.019992	43.569063
3521.601281	657441.854825	43.574068
3521.298422	656978.317480	43.579073
3521.364261	656497.620100	43.584077
3521.296972	656032.799363	43.589082
3520.722300	655568.542465	43.594087
3521.238985	655099.333466	43.599092
3520.951618	654635.232943	43.604097
3520.765975	654182.229479	43.609101
3520.938336	653722.701591	43.614106
3520.738102	653256.473471	43.619111
3520.707782	652798.135675	43.624116
3520.596976	652353.126488	43.629121
3520.523636	651889.958835	43.634125
3520.711044	651438.713642	43.639130
3520.569660	650992.599433	43.644135
3520.603825	650532.746870	43.649140
3520.635585	650084.064369	43.654145
3520.504624	649627.395491	43.659149
3520.532654	649177.823384	43.664154
3520.396616	648733.755304	43.669159
3520.422822	648279.096373	43.674164
3520.256716	647828.896988	43.679169
3520.391691	647381.524374	43.684173
3520.351833	646925.216025	43.689178
3520.153962	646486.506014	43.694183
3520.282271	646032.877131	43.699188
3520.137569	645587.221538	43.704193
3520.252843	645146.800155	43.709197
3520.113022	644705.203397	43.714202
3520.157842	644254.407859	43.719207
3520.175472	643801.297262	43.724212
3520.021398	643369.192784	43.729217
3519.787596	642916.885400	43.734221
3519.989290	642467.883313	43.739226
3519.908164	642028.309597	43.744231
3519.799391	641584.171421	43.749236
3519.772250	641145.900398	43.754241
3519.734692	640715.563276	43.759245
3519.753126	640281.197784	43.764250
3519.623176	639844.938760	43.769255
3519.285272	639401.844911	43.774260
3518.855291	638982.454547	43.779265
3519.330014	638555.540115	43.784269
3519.623801	638124.037099	43.789274
3519.408409	637697.504945	43.794279
3519.407371	637269.417822	43.799284
3520.050714	636847.756172	43.804289
3519.723951	636413.636101	43.809293
3519.830833	635971.869334	43.814298
3519.790919	635550.671621	43.819303
3520.008958	635114.202603	43.824308
3519.784129	634682.344045	43.829313
3519.867018	634247.162539	43.834317
3520.128506	633804.076094	43.839322
3519.830052	633369.273232	43.844327
3519.938853	632928.527558	43.849332
3519.742903	632490.868097	43.854337
3519.398158	632055.217619	43.859341
3519.513638	631626.927884	43.864346
3519.414713	631192.751079	43.869351
3519.763129	630763.535398	43.874356
3519.463782	630336.965630	43.879361
3519.270673	629905.805101	43.884365
3519.580388	629472.088099	43.889370
3519.369375	629048.755006	43.894375
3519.511720	628617.384352	43.899380
3519.211926	628197.386584	43.904385
3519.205977	627765.305540	43.909389
3519.416379	627334.521830	43.914394
3519.041577	626924.800900	43.919399
3519.228181	626493.436303	43.924404
3519.010618	626077.747059	43.929409
3518.714544	625650.486864	43.934413
3518.675395	625233.382071	43.939418
3518.295450	624817.070387	43.944423
3518.029977	624400.372336	43.949428
3518.330986	624002.744347	43.954433
3518.379465	623595.177186	43.959437
3518.109195	623184.443189	43.964442
3518.155415	622791.422045	43.969447
3518.080410	622383.178739	43.974452
3518.142109	621983.062183	43.979457
3517.972656	621583.471201	43.984461
3518.457238	621173.333087	43.989466
3518.361182	620776.705654	43.994471
3518.041160	620383.458804	43.999476
3518.041698	619976.564513	44.004481
3518.057886	619578.671482	44.009485
3517.882092	619181.498153	44.014490
3517.559638	618782.781911	44.019495
3517.779143	618395.784997	44.024500
3517.816608	618000.987624	44.029505
3517.792715	617614.756226	44.034509
3518.012767	617211.229054	44.039514
3518.221925	616823.225866	44.044519
3517.810329	616421.531559	44.049524
3517.913679	616031.262898	44.054529
3518.066358	615630.696328	44.059533
3518.001194	615236.668801	44.064538
3517.692538	614847.481046	44.069543
3517.653800	614445.801135	44.074548
3517.707662	614066.399525	44.079553
3517.658498	613672.012459	44.084557
3517.922317	613282.972508	44.089562
3517.485330	612892.283709	44.094567
3517.688051	612506.184967	44.099572
3517.522760	612112.413913	44.104577
3517.681547	611732.362764	44.109581
3517.349985	611339.946536	44.114586
3517.307723	610956.042043	44.119591
3517.721547	610570.993336	44.124596
3517.875528	610194.300513	44.129601
3517.239600	609815.222273	44.134605
3517.382781	609421.855015	44.139610
3517.280060	609046.471284	44.144615
3517.237234	608660.481747	44.149620
3517.347693	608284.634838	44.154625
3516.996517	607898.721885	44.159629
3517.221824	607519.619534	44.164634
3516.985133	607154.879777	44.169639
3517.149699	606767.385218	44.174644
3516.815076	606392.052700	44.179649
3516.852218	606029.487268	44.184653
3516.901398	605644.432092	44.189658
3516.983065	605288.006165	44.194663
3516.608192	604908.567376	44.199668
3516.504770	604544.724052	44.204673
3516.508822	604184.212525	44.209677
3516.847982	603821.675411	44.214682
3516.533008	603453.216888	44.219687
3516.729864	603083.203805	44.224692
3516.886861	602719.608911	44.229697
3516.664804	602350.045033	44.234701
3516.691102	601984.943537	44.239706
3516.529004	601624.630371	44.244711
3516.728461	601247.731910	44.249716
3516.636863	600884.623035	44.254721
3516.893631	600523.601469	44.259725
3517.100795	600152.688826	44.264730
3516.753892	599788.785813	44.269735
3516.640569	599416.398298	44.274740
3516.981045	599056.772165	44.279745
3516.617293	598693.540243	44.284749
3516.824847	598323.673115	44.289754
3516.646954	597964.402712	44.294759
3516.684799	597594.240037	44.299764
3516.075757	597232.711127	44.304769
3515.952456	596878.719669	44.309773
3516.101180	596525.373923	44.314778
3515.768272	596178.878193	44.319783
3516.063623	595821.218092	44.324788
3516.035851	595467.066979	44.329793
3515.771959	595121.331470	44.334797
3516.352193	594770.018150	44.339802
3515.984591	594421.467490	44.344807
3516.301795	594071.584252	44.349812
3516.207345	593718.697333	44.354817
3516.022683	593364.459181	44.359821
3516.524149	593004.267129	44.364826
3516.132112	592662.649663	44.369831
3516.239572	592314.256717	44.374836
3515.960506	591960.444483	44.379841
3515.844154	591616.539551	44.384845
3515.724275	591260.318320	44.389850
3515.583995	590921.269778	44.394855
3515.502442	590561.605088	44.399860
3515.455254	590227.393615	44.404865
3515.483954	589891.702873	44.409869
3515.465613	589543.551289	44.414874
3515.517030	589208.440254	44.419879
3515.296562	588872.813545	44.424884
3515.532407	588536.295578	44.429889
3515.456279	588203.740513	44.434893
3515.495704	587874.372242	44.439898
3515.019494	587535.033349	44.444903
3515.012652	587195.303202	44.449908
3514.958183	586872.455819	44.454913
3514.936047	586539.543807	44.459917
3514.918695	586219.335888	44.464922
3514.986808	585891.968665	44.469927
3515.066648	585560.570041	44.474932
3515.127681	585233.789214	44.479937
3515.033785	584905.920290	44.484941
3515.571627	584579.894758	44.489946
3515.242907	584252.601061	44.494951
3515.417974	583921.493034	44.499956
3515.271044	583599.729846	44.504961
3515.028489	583273.701861	44.509965
3515.068419	582941.283236	44.514970
3514.970029	582610.085579	44.519975
3514.685265	582289.467386	44.524980
3514.857913	581963.986899	44.529985
3514.935791	581645.049325	44.534989
3515.017904	581316.751771	44.539994
3514.772231	581006.248476	44.544999
3514.757963	580674.833082	44.550004
3514.925962	580359.013985	44.555009
3514.575923	580038.850643	44.560013
3515.064355	579712.451863	44.565018
3515.009729	579397.048260	44.570023
3514.476674	579072.566746	44.575028
3514.748597	578756.940129	44.580033
3514.713651	578438.541829	44.585037
3514.797885	578118.807502	44.590042
3514.592177	577805.651863	44.595047
3514.398895	577486.099405	44.600052
3514.548965	577176.186186	44.605057
3514.438767	576862.889794	44.610061
3514.663995	576548.673230	44.615066
3514.496065	576237.483217	44.620071
3514.555762	575930.722869	44.625076
3514.279131	575615.461882	44.630081
3514.250420	575302.011619	44.635085
3514.126889	574995.511002	44.640090
3513.948029	574694.344182	44.645095
3514.104341	574391.000189	44.650100
3514.265440	574081.712239	44.655105
3514.165032	573781.063357	44.660109
3514.403347	573464.352220	44.665114
3514.327046	573166.753133	44.670119
3514.155889	572858.497864	44.675124
3514.158680	572552.268016	44.680129
3513.683193	572257.029763	44.685133
3513.714162	571953.899794	44.690138
3513.731103	571660.575954	44.695143
3513.882798	571365.863806	44.700148
3514.144868	571058.295536	44.705153
3513.990720	570765.483270	44.710157
3513.894386	570464.553211	44.715162
3513.932558	570159.014019	44.720167
3513.939596	569866.958562	44.725172
3513.928538	569565.690689	44.730177
3513.775262	569271.887672	44.735181
3514.228345	568971.230979	44.740186
3514.072105	568681.591696	44.745191
3514.014600	568380.052056	44.750196
3513.976795	568078.099307	44.755201
3513.427420	567781.662216	44.760205
3513.743069	567486.781758	44.765210
3513.870034	567196.506807	44.770215
3513.854219	566897.542261	44.775220
3513.675379	566601.266223	44.780225
3513.430616	566304.793263	44.785229
3513.307319	566013.980603	44.790234
3513.102901	565731.279369	44.795239
3513.079750	565446.376465	44.800244
3513.309624	565158.152053	44.805249
3512.970633	564894.886117	44.810253
3513.430653	564599.411366	44.815258
3513.078987	564320.681264	44.820263
3513.410339	564047.466945	44.825268
3513.172057	563768.000777	44.830273
3513.123513	563476.111289	44.835277
3513.506195	563191.844583	44.840282
3513.338917	562917.634321	44.845287
3512.988864	562621.094790	44.850292
3513.221247	562347.710543	44.855297
3512.958926	562071.635741	44.860301
3513.252204	561780.556137	44.865306
3513.035538	561518.056768	44.870311
3512.957235	561231.358692	44.875316
3513.145478	560963.693316	44.880321
3513.023571	560684.846056	44.885325
3513.556311	560407.391797	44.890330
3513.447282	560128.329067	44.895335
3513.054839	559843.366414	44.900340
3513.123276	559562.297345	44.905345
3512.532587	559295.133791	44.910349
3512.952090	559013.942704	44.915354
3512.925142	558749.844658	44.920359
3512.530307	558479.307132	44.925364
3512.854813	558202.395931	44.930369
3512.492642	557945.490908	44.935373
3512.886187	557669.614453	44.940378
3512.631909	557395.102068	44.945383
3512.547499	557122.569772	44.950388
3512.703400	556851.904926	44.955393
3512.425008	556597.578721	44.960397
3512.860678	556329.172544	44.965402
3512.594890	556061.636319	44.970407
3512.306238	555797.020343	44.975412
3512.652889	555534.305662	44.980417
3512.264653	555275.691024	44.985421
3512.466957	555008.305614	44.990426
3512.312590	554752.159780	44.995431
3512.211658	554484.059978	45.000436
3512.543193	554226.259348	45.005441
3512.110833	553973.017750	45.010445
3512.121266	553711.483435	45.015450
3512.021066	553459.938820	45.020455
3511.993138	553207.470237	45.025460
3511.950508	552947.844717	45.030465
3512.253297	552710.375525	45.035469
3512.405930	552446.625722	45.040474
3512.108185	552194.486532	45.045479
3512.173778	551945.858213	45.050484
3512.300899	551680.535732	45.055489
3512.101975	551439.904884	45.060493
3512.295688	551178.340498	45.065498
3511.978386	550924.114878	45.070503
3511.992169	550674.514579	45.075508
3512.062369	550420.868480	45.080513
3511.857493	550171.598632	45.085517
3512.015176	549921.455964	45.090522
3512.076892	549675.104892	45.095527
3511.848313	549425.775025	45.100532
3511.862134	549173.828843	45.105537
3511.571932	548930.548352	45.110541
3511.769518	548678.813656	45.115546
3511.923953	548438.170139	45.120551
3511.576980	548199.472905	45.125556
3511.795132	547948.628509	45.130561
3511.719115	547713.757638	45.135565
3511.725165	547466.065715	45.140570
3511.389018	547225.030998	45.145575
3511.546138	546975.086538	45.150580
3511.563870	546741.745660	45.155585
3511.004227	546510.666995	45.160589
3511.250033	546271.230106	45.165594
3511.313069	546040.541338	45.170599
3511.371917	545814.890594	45.175604
3511.629435	545564.903409	45.180609
3511.470043	545338.626783	45.185613
3511.643687	545091.770993	45.190618
3511.426582	544863.984028	45.195623
3511.207539	544634.882833	45.200628
3511.464163	544392.134516	45.205633
3511.472503	544164.196727	45.210637
3511.481976	543922.440332	45.215642
3511.583134	543690.243763	45.220647
3511.201783	543451.974434	45.225652
3511.474752	543215.202784	45.230657
3511.053042	542987.722512	45.235661
3511.292416	542755.738878	45.240666
3511.467174	542529.107321	45.245671
3511.124106	542296.610423	45.250676
3511.279984	542061.301504	45.255681
3511.062835	541832.607712	45.260685
3511.205602	541607.025629	45.265690
3511.227797	541384.587020	45.270695
3511.130473	541148.650448	45.275700
3511.164656	540918.839842	45.280705
3510.894252	540699.869540	45.285709
3510.922866	540477.516333	45.290714
3510.805408	540265.220467	45.295719
3510.809149	540034.442412	45.300724
3511.312172	539806.550901	45.305729
3510.841621	539577.863690	45.310733
3510.955048	539346.046966	45.315738
3510.872321	539135.089913	45.320743
3510.955229	538915.829845	45.325748
3511.266900	538690.727031	45.330753
3510.861564	538466.903140	45.335757
3510.888140	538236.192714	45.340762
3511.242105	538024.841939	45.345767
3510.668529	537804.768865	45.350772
3510.972369	537582.373599	45.355777
3510.936234	537363.614291	45.360781
3510.719965	537128.690224	45.365786
3510.626299	536929.405007	45.370791
3510.474215	536712.673246	45.375796
3510.731484	536493.144265	45.380801
3510.634660	536280.331227	45.385805
3510.637043	536063.058778	45.390810
3510.954360	535854.254868	45.395815
3510.584869	535634.012558	45.400820
3510.578691	535416.630867	45.405825
3510.687150	535202.808236	45.410829
3510.691545	534990.009197	45.415834
3510.449303	534781.688818	45.420839
3510.312509	534571.228436	45.425844
3510.351063	534360.634132	45.430849
3510.090097	534153.215997	45.435853
3510.207468	533938.969430	45.440858
3510.346577	533734.302389	45.445863
3509.936035	533521.653406	45.450868
3510.361690	533328.233726	45.455873
3510.189066	533132.491678	45.460877
3510.015491	532914.646698	45.465882
3510.042032	532716.695340	45.470887
3510.242319	532505.995927	45.475892
3510.462093	532299.125072	45.480897
3510.066371	532099.017148	45.485901
3509.921897	531898.560801	45.490906
3510.461858	531695.461733	45.495911
3510.003644	531494.548764	45.500916
3510.284587	531293.759134	45.505921
3510.172103	531092.579735	45.510925
3510.409611	530875.845132	45.515930
3509.909370	530688.250908	45.520935
3509.699025	530495.053509	45.525940
3510.129483	530286.503183	45.530945
3509.896492	530094.263223	45.535949
3510.274720	529891.923687	45.540954
3509.992423	529688.381945	45.545959
3510.024259	529489.931635	45.550964
3510.234712	529299.472905	45.555969
3510.098288	529105.790325	45.560973
3510.561149	528891.965664	45.565978
3510.352098	528691.577303	45.570983
3510.110180	528495.532498	45.575988
3510.377933	528286.274915	45.580993
3510.498088	528086.124948	45.585997
3510.342334	527883.798473	45.591002
3510.290931	527677.716201	45.596007
3510.172039	527477.094033	45.601012
3510.024629	527273.243475	45.606017
3509.687603	527090.825065	45.611021
3509.696645	526886.690080	45.616026
3509.915488	526695.943907	45.621031
3509.945952	526499.573713	45.626036
3509.701350	526303.348846	45.631041
3509.604128	526115.678005	45.636045
3509.956391	525933.380073	45.641050
3510.059097	525749.204189	45.646055
3509.878550	525551.090608	45.651060
3510.226252	525353.792904	45.656065
3509.757353	525157.641703	45.661069
3509.793757	524954.889081	45.666074
3509.622828	524765.749749	45.671079
3509.376229	524586.617222	45.676084
3509.755048	524385.010072	45.681089
3509.304210	524203.030066	45.686093
3509.514286	524007.252705	45.691098
3509.371669	523828.194321	45.696103
3509.387067	523652.691566	45.701108
3509.185304	523461.874873	45.706113
3509.146940	523286.730448	45.711117
3509.264957	523110.749422	45.716122
3509.559099	522919.386747	45.721127
3509.103112	522744.559771	45.726132
3509.117025	522554.957052	45.731137
3508.737997	522389.100574	45.736141
3508.716431	522213.031900	45.741146
3509.183309	522043.139131	45.746151
3509.158664	521864.542179	45.751156
3509.551040	521681.630250	45.756161
3509.181454	521500.815575	45.761165
3509.047949	521318.746496	45.766170
3509.065970	521144.830001	45.771175
3509.005614	520980.772071	45.776180
3509.031603	520808.516801	45.781185
3508.924038	520633.908903	45.786189
3508.858062	520454.494387	45.791194
3508.884563	520285.061096	45.796199
3508.952585	520125.315058	45.801204
3509.303565	519948.550445	45.806209
3509.002258	519779.066485	45.811213
3509.170591	519598.137297	45.816218
3509.141473	519416.835646	45.821223
3509.177972	519243.045751	45.826228
3509.014656	519064.944591	45.831233
3508.778978	518907.863894	45.836237
3508.775071	518732.509428	45.841242
3508.756209	518569.024499	45.846247
3508.566617	518402.940616	45.851252
3509.106593	518232.487740	45.856257
3509.029809	518066.835520	45.861261
3508.817960	517892.618119	45.866266
3508.677045	517724.397213	45.871271
3508.927677	517564.290177	45.876276
3508.704449	517393.907792	45.881281
3508.773626	517231.757357	45.886285
3508.923754	517066.964805	45.891290
3509.183830	516897.454117	45.896295
3508.961918	516727.367200	45.901300
3509.082980	516554.946763	45.906305
3508.776887	516392.396953	45.911309
3508.930617	516230.322574	45.916314
3508.881522	516059.996738	45.921319
3508.579708	515900.774984	45.926324
3508.803799	515723.326681	45.931329
3508.995507	515567.149202	45.936333
3508.747621	515391.293166	45.941338
3509.009270	515239.343849	45.946343
3508.528999	515070.596267	45.951348
3508.946317	514897.955234	45.956353
3508.278736	514743.886398	45.961357
3508.342629	514584.184529	45.966362
3508.589675	514412.830166	45.971367
3508.236509	514269.615248	45.976372
3508.976888	514102.568514	45.981377
3508.600420	513944.299334	45.986381
3508.653830	513782.822787	45.991386
3508.643851	513626.155028	45.996391
3508.754363	513470.374538	46.001396
3508.956558	513297.651461	46.006401
3508.747344	513151.168187	46.011405
3508.234425	512979.574176	46.016410
3508.520932	512825.929775	46.021415
3508.375920	512659.018789	46.026420
3508.234282	512503.019093	46.031425
3508.019707	512352.234540	46.036429
3508.162040	512202.196031	46.041434
3508.367665	512052.397921	46.046439
3508.212289	511894.322891	46.051444
3508.265813	511732.673603	46.056449
3507.827144	511589.196103	46.061453
3507.824765	511439.326610	46.066458
3507.777273	511296.335475	46.071463
3507.702719	511158.703890	46.076468
3507.845600	511005.217807	46.081473
3507.634953	510872.356866	46.086477
3507.749698	510722.915350	46.091482
3508.127311	510583.938254	46.096487
3507.592361	510442.791244	46.101492
3507.950270	510297.043605	46.106497
3508.230076	510157.473065	46.111501
3507.841736	510016.549887	46.116506
3508.072726	509872.790845	46.121511
3507.734602	509730.340510	46.126516
3507.944371	509581.781628	46.131521
3507.528844	509445.102990	46.136525
3507.583692	509307.281599	46.141530
3507.675343	509166.016227	46.146535
3507.170697	509028.338482	46.151540
3507.793500	508882.785314	46.156545
3507.402142	508754.940707	46.161549
3507.682679	508628.648122	46.166554
3508.137691	508494.693372	46.171559
3507.750984	508355.877817	46.176564
3507.764705	508209.411711	46.181569
3507.627467	508075.200782	46.186573
3507.494040	507927.038841	46.191578
3507.842150	507791.883471	46.196583
3507.448165	507662.463779	46.201588
3507.549285	507528.106475	46.206593
3507.445624	507398.938332	46.211597
3507.388327	507261.977639	46.216602
3507.225693	507132.564703	46.221607
3507.341365	507007.551043	46.226612
3507.461491	506870.556712	46.231617
3507.493067	506740.854735	46.236621
3507.328146	506606.080229	46.241626
3507.547497	506478.972411	46.246631
3507.053999	506356.130048	46.251636
3507.550216	506215.325536	46.256641
3507.536021	506090.882926	46.261645
3507.870442	505966.329284	46.266650
3508.087987	505828.551241	46.271655
3507.614208	505692.507587	46.276660
3507.699475	505555.356367	46.281665
3507.551142	505427.494262	46.286669
3507.077180	505287.807726	46.291674
3507.594745	505154.875960	46.296679
3507.393281	505028.384602	46.301684
3507.225489	504896.325978	46.306689
3507.211176	504775.007358	46.311693
3506.919934	504656.363765	46.316698
3507.120712	504524.694137	46.321703
3507.178569	504415.341180	46.326708
3507.294940	504278.477135	46.331713
3507.291163	504154.927778	46.336717
3507.301903	504019.191738	46.341722
3507.210724	503892.369363	46.346727
3507.018130	503777.291784	46.351732
3506.866894	503652.196615	46.356737
3507.182527	503544.007078	46.361741
3506.937229	503421.150589	46.366746
3507.033980	503299.953647	46.371751
3506.942195	503187.129667	46.376756
3507.370829	503063.700413	46.381761
3507.134217	502945.995563	46.386765
3506.912935	502806.699529	46.391770
3507.064885	502692.768821	46.396775
3506.697691	502576.398085	46.401780
3507.042934	502457.023081	46.406785
3506.930746	502344.702338	46.411789
3506.545091	502238.646214	46.416794
3507.018241	502114.797725	46.421799
3506.836215	502000.059714	46.426804
3506.922769	501881.887548	46.431809
3506.727503	501774.784718	46.436813
3506.810341	501645.892774	46.441818
3507.097661	501531.223025	46.446823
3507.069851	501424.797167	46.451828
3506.909141	501306.865322	46.456833
3506.918801	501181.268714	46.461837
3506.746051	501079.618173	46.466842
3506.978745	500966.622359	46.471847
3506.955939	500849.017619	46.476852
3507.099381	500735.226452	46.481857
3506.718006	500627.591724	46.486861
3506.888328	500504.136746	46.491866
3507.045747	500386.497932	46.496871
3506.780743	500273.885731	46.501876
3506.882573	500152.512962	46.506881
3507.013479	500044.635265	46.511885
3506.721231	499932.429907	46.516890
3506.731937	499823.559977	46.521895
3506.931449	499715.061624	46.526900
3507.512691	499601.390154	46.531905
3507.185676	499485.294069	46.536909
3506.983020	499362.905586	46.541914
3507.048467	499234.857405	46.546919
3506.859779	499135.776565	46.551924
3506.676286	499013.129386	46.556929
3507.007462	498908.851018	46.561933
3506.966493	498803.725294	46.566938
3506.829753	498676.617568	46.571943
3506.701097	498564.728997	46.576948
3506.884523	498447.577665	46.581953
3506.910399	498346.786666	46.586957
3506.724936	498243.148609	46.591962
3506.910234	498122.505287	46.596967
3506.627967	498017.415790	46.601972
3506.771129	497906.336095	46.606977
3506.831847	497793.954861	46.611981
3506.706384	497681.806949	46.616986
3506.854327	497566.425515	46.621991
3506.749680	497465.246888	46.626996
3506.831297	497349.976429	46.632001
3506.556788	497230.517780	46.637005
3506.280423	497138.722648	46.642010
3506.551658	497032.723256	46.647015
3506.092977	496937.923685	46.652020
3506.308767	496839.417590	46.657025
3506.351009	496727.892116	46.662029
3506.062681	496630.027193	46.667034
3506.275942	496529.142652	46.672039
3506.321760	496434.759851	46.677044
3506.481181	496319.317282	46.682049
3506.455902	496226.715630	46.687053
3506.196866	496123.380447	46.692058
3506.204084	496024.702872	46.697063
3506.318449	495932.075752	46.702068
3506.600448	495835.272102	46.707073
3506.702007	495730.659062	46.712077
3506.366778	495638.461139	46.717082
3506.964593	495531.384934	46.722087
3506.335737	495419.763043	46.727092
3506.357368	495307.422390	46.732097
3506.578959	495208.956327	46.737101
3506.198691	495116.662076	46.742106
3506.459399	495012.877269	46.747111
3506.028254	494913.964549	46.752116
3506.059010	494817.552017	46.757121
3506.172052	494724.969070	46.762125
3506.009090	494634.000771	46.767130
3506.249449	494524.753624	46.772135
3506.127894	494433.827760	46.777140
3506.210737	494336.644859	46.782145
3506.046017	494236.569867	46.787149
3505.839224	494146.618087	46.792154
3506.121689	494055.317708	46.797159
3506.219104	493968.752710	46.802164
3506.120056	493871.193527	46.807169
3506.235889	493774.052351	46.812173
3506.078533	493685.708378	46.817178
3506.160881	493579.466599	46.822183
3505.990142	493491.781504	46.827188
3506.187303	493392.398516	46.832193
3505.971363	493307.805895	46.837197
3506.136589	493219.859690	46.842202
3506.464037	493127.433754	46.847207
3506.474939	493028.080441	46.852212
3506.473025	492932.775672	46.857217
3506.573620	492831.584776	46.862221
3506.376150	492736.008774	46.867226
3506.307728	492636.514959	46.872231
3505.938418	492538.741337	46.877236
3506.114816	492425.039876	46.882241
3506.131236	492333.674507	46.887245
3505.832268	492250.304933	46.892250
3505.889954	492152.000889	46.897255
3505.946759	492067.456717	46.902260
3506.092096	491985.122950	46.907265
3506.109378	491890.163207	46.912269
3506.118738	491809.167144	46.917274
3506.509476	491716.975717	46.922279
3506.164547	491622.481056	46.927284
3506.034326	491525.723216	46.932289
3506.235353	491442.061966	46.937293
3506.169826	491347.012168	46.942298
3506.367056	491248.830886	46.947303
3505.930331	491160.015616	46.952308
3505.726194	491060.485213	46.957313
3505.899856	490978.394734	46.962317
3505.636961	490897.592628	46.967322
3505.815598	490799.462544	46.972327
3505.742453	490730.668387	46.977332
3505.833203	490635.891528	46.982337
3505.731547	490551.113969	46.987341
3505.468117	490476.027064	46.992346
3505.654476	490395.297671	46.997351
3505.532937	490317.757326	47.002356
3505.723173	490226.249863	47.007361
3506.333872	490148.027188	47.012365
3505.875940	490053.745569	47.017370
3506.144313	489960.250140	47.022375
3505.954892	489869.159775	47.027380
3506.054926	489778.626659	47.032385
3506.029568	489695.956898	47.037389
3505.754473	489611.406716	47.042394
3506.152919	489523.553521	47.047399
3505.905640	489437.075060	47.052404
3505.810616	489355.984075	47.057409
3505.825922	489267.942016	47.062413
3506.043289	489193.526397	47.067418
3506.094226	489095.965005	47.072423
3506.070379	489018.199753	47.077428
3506.125953	488928.327554	47.082433
3505.986801	488830.392335	47.087437
3505.927846	488746.964796	47.092442
3506.408129	488645.633832	47.097447
3506.316002	488567.018026	47.102452
3506.047118	488470.114914	47.107457
3506.137219	488382.207385	47.112461
3505.925138	488296.678623	47.117466
3505.591107	488200.392334	47.122471
3505.339971	488138.398732	47.127476
3505.401199	488064.156735	47.132481
3505.530976	487972.698289	47.137485
3505.382116	487900.262509	47.142490
3505.097113	487817.324515	47.147495
3505.461200	487749.810097	47.152500
3505.398491	487672.399669	47.157505
3505.562856	487601.123615	47.162509
3505.422401	487523.472788	47.167514
3505.448556	487443.516041	47.172519
3505.486672	487383.039049	47.177524
3505.341503	487292.585438	47.182529
3505.399434	487212.875225	47.187533
3505.483131	487141.864086	47.192538
3505.367523	487070.380650	47.197543
3505.190450	487000.476144	47.202548
3505.280116	486923.036375	47.207553
3505.244156	486849.564868	47.212557
3504.899371	486780.042347	47.217562
3505.357137	486709.876469	47.222567
3504.718469	486643.895327	47.227572
3505.255394	486577.713209	47.232577
3505.122929	486504.307335	47.237581
3505.212251	486442.755632	47.242586
3505.044422	486369.962502	47.247591
3505.108344	486308.313451	47.252596
3505.273752	486238.398030	47.257601
3505.384536	486173.754733	47.262605
3505.138752	486099.404989	47.267610
3505.346103	486028.064581	47.272615
3505.397483	485951.740409	47.277620
3505.565513	485882.430409	47.282625
3505.572107	485808.896667	47.287629
3505.493289	485734.314438	47.292634
3505.245410	485656.926712	47.297639
3505.116907	485589.943549	47.302644
3505.058110	485524.264046	47.307649
3505.365395	485455.181627	47.312653
3505.477921	485387.245584	47.317658
3505.648527	485313.378114	47.322663
3505.524988	485246.392796	47.327668
3504.975655	485173.558630	47.332673
3505.223192	485095.932019	47.337677
3505.006052	485033.769785	47.342682
3505.124597	484955.405434	47.347687
3504.857394	484907.624535	47.352692
3504.969597	484841.812071	47.357697
3505.166527	484769.911632	47.362701
3505.205565	484716.865043	47.367706
3505.023943	484636.526101	47.372711
3504.848914	484576.278279	47.377716
3505.201852	484512.245482	47.382721
3505.298474	484440.613887	47.387725
3505.201168	484378.023991	47.392730
3505.219425	484311.668865	47.397735
3505.138583	484250.290389	47.402740
3505.259318	484181.032391	47.407745
3504.765758	484107.728792	47.412749
3504.516831	484045.011768	47.417754
3504.892122	483979.151173	47.422759
3505.087219	483921.469789	47.427764
3504.871996	483862.289270	47.432769
3505.129330	483805.457304	47.437773
3504.927482	483747.590064	47.442778
3504.980395	483671.559452	47.447783
3505.409177	483614.242078	47.452788
3505.446098	483543.477486	47.457793
3505.608151	483475.373800	47.462797
3505.013463	483416.661499	47.467802
3505.517726	483340.451176	47.472807
3505.699291	483263.384558	47.477812
3505.703553	483201.886694	47.482817
3505.586911	483122.491477	47.487821
3505.343967	483062.806874	47.492826
3505.378933	482983.233303	47.497831
3505.335047	482918.503280	47.502836
3505.122006	482841.957756	47.507841
3505.641662	482769.234866	47.512845
3505.207316	482710.189155	47.517850
3505.231403	482640.233024	47.522855
3505.043722	482577.905295	47.527860
3504.644996	482521.130630	47.532865
3504.912073	482452.802632	47.537869
3504.728024	482411.783503	47.542874
3504.882731	482334.211279	47.547879
3504.592038	482284.098918	47.552884
3504.310228	482233.934282	47.557889
3504.892309	482164.387188	47.562893
3504.502798	482119.808593	47.567898
3504.642633	482061.826912	47.572903
3504.913501	482004.430090	47.577908
3504.932295	481946.418084	47.582913
3504.843906	481885.032734	47.587917
3504.523874	481828.039952	47.592922
3504.850679	481769.266115	47.597927
3504.879932	481715.351718	47.602932
3504.965842	481662.237394	47.607937
3505.286950	481600.325574	47.612941
3504.791452	481544.677958	47.617946
3505.072931	481482.974978	47.622951
3504.980398	481424.271610	47.627956
3504.860944	481360.257523	47.632961
3505.181694	481300.521399	47.637965
3504.533328	481241.406134	47.642970
3504.888951	481175.589172	47.647975
3504.933895	481133.211871	47.652980
3504.821485	481084.027503	47.657985
3505.327266	481022.841475	47.662989
3505.030458	480962.703461	47.667994
3504.757249	480896.891605	47.672999
3504.951471	480835.302542	47.678004
3504.890864	480784.792345	47.683009
3505.010773	480720.380754	47.688013
3505.145078	480667.508334	47.693018
3505.220043	480604.167066	47.698023
3504.980799	480534.956388	47.703028
3504.718109	480482.961171	47.708033
3504.936588	480420.910944	47.713037
3504.640831	480364.415595	47.718042
3504.580515	480303.981882	47.723047
3504.932802	480254.007175	47.728052
3504.436932	480197.292353	47.733057
3504.639358	480139.293777	47.738061
3504.638540	480095.301888	47.743066
3504.609618	480038.962452	47.748071
3504.496176	479987.092193	47.753076
3504.377510	479937.905760	47.758081
3504.605700	479892.203674	47.763085
3504.560540	479851.964965	47.768090
3504.594798	479785.235931	47.773095
3504.599127	479741.292925	47.778100
3504.634868	479696.838200	47.783105
3504.728437	479647.159113	47.788109
3504.820497	479601.074535	47.793114
3504.702528	479536.446206	47.798119
3505.186936	479485.079929	47.803124
3505.076155	479428.195685	47.808129
3505.140066	479361.004392	47.813133
3504.727538	479312.068934	47.818138
3504.956687	479251.835405	47.823143
3504.855587	479190.746791	47.828148
3505.189966	479135.861299	47.833153
3504.927192	479077.128724	47.838157
3504.675912	479036.619635	47.843162
3504.638256	478977.493912	47.848167
3504.468722	478925.275795	47.853172
3504.530166	478876.207603	47.858177
3504.726389	478817.142678	47.863181
3504.720077	478761.858580	47.868186
3504.574308	478711.559635	47.873191
3504.641647	478662.388603	47.878196
3504.475055	478617.155731	47.883201
3505.012009	478561.373239	47.888205
3504.345511	478517.643062	47.893210
3504.479663	478462.384696	47.898215
3504.432797	478410.346665	47.903220
3504.488240	478367.100399	47.908225
3504.558221	478309.675495	47.913229
3504.548476	478276.920298	47.918234
3504.545303	478225.380567	47.923239
3504.319935	478170.790250	47.928244
3504.129220	478130.066279	47.933249
3504.481153	478081.604523	47.938253
3504.201230	478039.376698	47.943258
3504.056638	477982.392435	47.948263
3504.311710	477959.059199	47.953268
3503.922578	477906.723760	47.958273
3504.560350	477870.161288	47.963277
3504.188183	477829.720777	47.968282
3504.355132	477776.429304	47.973287
3504.522828	477730.833368	47.978292
3504.194710	477685.119453	47.983297
3504.220260	477641.066479	47.988301
3504.304070	477603.231032	47.993306
3504.417357	477562.909563	47.998311
3504.505656	477512.061027	48.003316
3504.400550	477484.181263	48.008321
3504.402237	477426.258926	48.013325
3504.390066	477386.717957	48.018330
3504.389787	477341.909201	48.023335
3504.578440	477298.890812	48.028340
3504.207135	477247.664332	48.033345
3504.667074	477199.688111	48.038349
3504.317044	477161.672667	48.043354
3504.237092	477113.990933	48.048359
3504.457978	477072.485472	48.053364
3504.235067	477030.194943	48.058369
3504.556126	476980.773524	48.063373
3504.372930	476937.159555	48.068378
3504.376991	476894.931224	48.073383
3504.590090	476853.781025	48.078388
3504.203328	476818.454678	48.083393
3504.446265	476771.982744	48.088397
3504.389166	476741.663264	48.093402
3504.687752	476679.535951	48.098407
3504.514637	476635.362575	48.103412
3504.209343	476587.110344	48.108417
3504.749005	476542.258071	48.113421
3504.452257	476498.713079	48.118426
3504.249733	476452.670833	48.123431
3504.240555	476404.671364	48.128436
3504.217282	476376.067061	48.133441
3504.421586	476330.258849	48.138445
3504.637535	476294.271603	48.143450
3504.488984	476240.016839	48.148455
3504.793020	476192.520316	48.153460
3504.420445	476136.024937	48.158465
3504.655126	476094.869352	48.163469
3504.962206	476049.954321	48.168474
3504.909369	475997.809171	48.173479
3504.734065	475949.431796	48.178484
3504.647675	475905.292490	48.183489
3504.643988	475847.011631	48.188493
3504.705636	475801.884723	48.193498
3504.818155	475751.938613	48.198503
3504.644121	475701.636207	48.203508
3504.388837	475656.411149	48.208513
3504.506080	475611.730008	48.213517
3504.434153	475563.333967	48.218522
3504.180880	475525.197334	48.223527
3504.110559	475466.521556	48.228532
3504.063658	475435.134808	48.233537
3504.436875	475394.308460	48.238541
3504.432530	475361.547126	48.243546
3504.336446	475332.751085	48.248551
3504.158716	475277.586998	48.253556
3503.962398	475251.896811	48.258561
3504.216359	475205.722862	48.263565
3504.064507	475166.606060	48.268570
3503.982943	475135.427270	48.273575
3504.286854	475082.560327	48.278580
3504.088460	475049.223919	48.283585
3504.336534	475016.874613	48.288589
3504.108245	474979.137687	48.293594
3504.363020	474944.153935	48.298599
3504.591565	474901.832060	48.303604
3504.086686	474860.091062	48.308609
3504.573364	474805.926163	48.313613
3504.182216	474776.268142	48.318618
3504.418491	474735.311806	48.323623
3504.446274	474694.087146	48.328628
3504.129514	474657.326805	48.333633
3504.260204	474605.348935	48.338637
3504.224185	474576.440181	48.343642
3504.135056	474532.855087	48.348647
3504.341596	474496.410188	48.353652
3504.276337	474449.681186	48.358657
3504.153360	474409.646340	48.363661
3504.255091	474378.333698	48.368666
3504.265385	474324.046173	48.373671
3504.191166	474295.143501	48.378676
3503.954367	474252.646398	48.383681
3503.849441	474218.938053	48.388685
3503.736111	474197.637915	48.393690
3504.074720	474166.740230	48.398695
3504.180636	474116.335065	48.403700
3503.930378	474095.210109	48.408705
3503.701821	474054.939323	48.413709
3503.843116	474011.414939	48.418714
3503.883025	473983.859592	48.423719
3504.566050	473958.169385	48.428724
3504.146783	473920.766753	48.433729
3504.209902	473874.065020	48.438733
3504.421115	473843.289832	48.443738
3504.175506	473810.870794	48.448743
3504.201766	473776.531551	48.453748
3504.031528	473740.098860	48.458753
3504.444580	473704.629972	48.463757
3504.003143	473665.508801	48.468762
3504.053999	473628.886216	48.473767
3504.201248	473597.918976	48.478772
3504.080429	473562.135840	48.483777
3504.359382	473525.828598	48.488781
3504.391861	473492.855102	48.493786
3504.392815	473452.391895	48.498791
3504.276303	473399.946437	48.503796
3504.169780	473367.350949	48.508801
3504.452061	473325.674655	48.513805
3504.093837	473284.715343	48.518810
3504.312840	473249.329366	48.523815
3504.443543	473202.563765	48.528820
3503.848605	473180.230549	48.533825
3503.971059	473140.404275	48.538829
3504.204625	473107.800907	48.543834
3503.768860	473074.146974	48.548839
3504.128525	473049.270377	48.553844
3503.947431	473012.939401	48.558849
3503.886669	472971.168958	48.563853
3503.744943	472944.504024	48.568858
3503.724326	472905.663904	48.573863
3504.014118	472869.606752	48.578868
3503.883789	472852.156897	48.583873
3503.734606	472822.403790	48.588877
3503.628138	472781.552317	48.593882
3503.694514	472756.725408	48.598887
3503.932888	472725.336008	48.603892
3503.794997	472706.266695	48.608897
3503.611850	472676.316578	48.613901
3503.889275	472647.553881	48.618906
3503.596574	472622.079084	48.623911
3503.822968	472597.072707	48.628916
3503.620369	472577.305289	48.633921
3503.720741	472538.241168	48.638925
3503.753036	472505.873694	48.643930
3503.969499	472485.123020	48.648935
3503.812393	472456.586158	48.653940
3503.759266	472426.461505	48.658945
3503.892710	472390.582060	48.663949
3503.539057	472367.548283	48.668954
3503.419316	472354.654213	48.673959
3503.726288	472319.048872	48.678964
3503.463510	472284.857524	48.683969
3503.887496	472257.993726	48.688973
3503.757265	472241.049736	48.693978
3503.627431	472220.560479	48.698983
3503.596534	472197.623321	48.703988
3503.500028	472160.313976	48.708993
3503.580575	472133.306057	48.713997
3503.278053	472117.809454	48.719002
3503.315576	472104.331255	48.724007
3503.524041	472075.427516	48.729012
3503.399596	472071.295789	48.734017
3503.609599	472047.253749	48.739021
3503.736522	472021.909068	48.744026
3503.728873	471982.710294	48.749031
3503.949935	471958.261083	48.754036
3503.475708	471939.400354	48.759041
3503.647714	471918.656644	48.764045
3503.246089	471891.477474	48.769050
3503.459979	471859.584339	48.774055
3503.850521	471838.600640	48.779060
3503.755787	471820.839865	48.784065
3503.591916	471801.571479	48.789069
3503.782315	471777.481794	48.794074
3503.790576	471744.256114	48.799079
3503.789604	471711.943594	48.804084
3503.504442	471704.800416	48.809089
3503.649134	471674.438188	48.814093
3503.513577	471653.138936	48.819098
3503.521247	471629.637380	48.824103
3504.026776	471592.021520	48.829108
3503.493405	471575.804176	48.834113
3503.660733	471550.705196	48.839117
3503.399044	471540.367166	48.844122
3503.220661	471529.356490	48.849127
3503.665308	471485.571834	48.854132
3503.370862	471457.512726	48.859137
3503.560704	471428.054048	48.864141
3503.597889	471415.740307	48.869146
3503.272983	471409.312869	48.874151
3503.807416	471385.771712	48.879156
3503.624248	471368.278847	48.884161
3503.907332	471325.382416	48.889165
3503.681657	471302.325476	48.894170
3503.811386	471287.767340	48.899175
3503.522309	471262.036831	48.904180
3503.261305	471261.777496	48.909185
3503.713771	471225.436166	48.914189
3503.649304	471185.029871	48.919194
3503.731171	471174.329088	48.924199
3504.020342	471147.385426	48.929204
3503.808447	471127.972603	48.934209
3504.025711	471088.024479	48.939213
3504.021589	471076.831838	48.944218
3503.881521	471043.731542	48.949223
3503.836985	471004.840917	48.954228
3503.742066	470984.091104	48.959233
3503.950167	470955.084407	48.964237
3504.013851	470927.469847	48.969242
3503.518228	470905.066299	48.974247
3504.124055	470875.687676	48.979252
3503.861964	470862.361042	48.984257
3503.692318	470821.110889	48.989261
3503.924572	470796.050466	48.994266
3503.834237	470771.298338	48.999271
3504.136244	470750.733740	49.004276
3503.900780	470719.624492	49.009281
3504.073436	470687.432514	49.014285
3504.021354	470665.206196	49.019290
3503.879537	470633.776917	49.024295
3504.466136	470605.414152	49.029300
3504.272474	470566.548085	49.034305
3504.396662	470533.249822	49.039309
3504.403836	470498.401325	49.044314
3504.290578	470461.952520	49.049319
3504.243585	470434.305485	49.054324
3503.906732	470404.783188	49.059329
3503.915743	470378.595370	49.064333
3503.966102	470360.707139	49.069338
3503.774548	470318.649220	49.074343
3504.181208	470286.973761	49.079348
3503.826532	470270.724775	49.084353
3503.916241	470237.026671	49.089357
3504.192396	470202.992765	49.094362
3503.922919	470182.221223	49.099367
3503.639135	470139.317585	49.104372
3503.296689	470124.484615	49.109377
3503.545466	470098.255470	49.114381
3503.675566	470089.673187	49.119386
3503.163909	470070.968923	49.124391
3503.526071	470051.456971	49.129396
3503.458218	470040.375899	49.134401
3503.119973	470021.793931	49.139405
3503.134198	470009.939055	49.144410
3503.124315	469991.452945	49.149415
3503.409604	469971.042309	49.154420
3503.452769	469965.361952	49.159425
3503.410773	469926.873884	49.164429
3503.522702	469902.339338	49.169434
3503.205442	469890.540988	49.174439
3503.230062	469874.378852	49.179444
3503.037860	469854.556139	49.184449
3503.373721	469839.911039	49.189453
3503.082276	469831.501920	49.194458
3503.136453	469820.906403	49.199463
3503.425915	469795.480322	49.204468
3503.584965	469794.693372	49.209473
3503.395075	469770.058233	49.214477
3503.248290	469765.119379	49.219482
3503.318665	469748.290846	49.224487
3503.510046	469738.077072	49.229492
3503.315613	469719.672860	49.234497
3503.411499	469692.962736	49.239501
3503.489911	469664.938598	49.244506
3503.028791	469645.516149	49.249511
3503.257020	469632.763405	49.254516
3503.236327	469629.677127	49.259521
3503.448097	469611.456713	49.264525
3503.627715	469599.775951	49.269530
3503.393941	469598.802804	49.274535
3503.473766	469573.868094	49.279540
3503.381347	469565.678137	49.284545
3503.542937	469550.252127	49.289549
3503.357589	469516.447747	49.294554
3503.408693	469491.872402	49.299559
3503.229075	469468.349479	49.304564
3503.303441	469460.840139	49.309569
3503.355855	469447.357498	49.314573
3503.456565	469429.358485	49.319578
3503.220615	469428.740271	49.324583
3503.416911	469403.886757	49.329588
3503.494311	469404.532018	49.334593
3503.512682	469382.798693	49.339597
3503.515277	469369.273849	49.344602
3503.398910	469330.999882	49.349607
3503.478978	469307.331111	49.354612
3503.355525	469293.523816	49.359617
3502.724841	469286.134792	49.364621
3503.340227	469260.247118	49.369626
3503.079036	469261.254118	49.374631
3503.294530	469241.968992	49.379636
3503.023154	469245.003872	49.384641
3503.012725	469226.365148	49.389645
3503.086240	469209.029065	49.394650
3503.155478	469201.115269	49.399655
3503.253295	469187.827306	49.404660
3503.180612	469183.736758	49.409665
3503.082319	469168.101545	49.414669
3503.357437	469157.214663	49.419674
3503.192473	469145.491151	49.424679
3503.356054	469133.914148	49.429684
3503.363446	469124.237998	49.434689
3503.336500	469109.046437	49.439693
3503.225227	469099.998383	49.444698
3502.908583	469091.846507	49.449703
3503.258653	469080.845476	49.454708
3503.116432	469065.724218	49.459713
3503.133584	469063.492502	49.464717
3502.934243	469040.428301	49.469722
3503.223388	469029.538952	49.474727
3503.220498	469017.787687	49.479732
3503.090903	469011.326077	49.484737
3503.237219	469006.944828	49.489741
3503.687498	468987.315430	49.494746
3503.102429	468980.779618	49.499751
3503.285162	468966.666534	49.504756
3503.380279	468962.699250	49.509761
3503.287879	468946.961539	49.514765
3503.640364	468934.592346	49.519770
3503.456117	468917.755899	49.524775
3503.249198	468885.575017	49.529780
3503.330282	468875.734194	49.534785
3503.283539	468858.823562	49.539789
3503.392685	468844.064443	49.544794
3502.858520	468836.253524	49.549799
3503.324756	468826.448222	49.554804
3503.306641	468818.802456	49.559809
3503.163507	468803.427871	49.564813
3503.542576	468786.089886	49.569818
3503.370791	468784.700873	49.574823
3503.377804	468778.215859	49.579828
3503.509484	468765.276401	49.584833
3503.352481	468740.836928	49.589837
3503.473074	468706.117734	49.594842
3502.943484	468689.086775	49.599847
3503.152707	468668.839695	49.604852
3503.302323	468665.015009	49.609857
3503.186604	468651.915097	49.614861
3503.182386	468636.617968	49.619866
3502.952023	468637.670391	49.624871
3503.313662	468616.333474	49.629876
3503.109278	468610.391049	49.634881
3503.356009	468602.953250	49.639885
3503.392479	468584.204578	49.644890
3503.063798	468587.097381	49.649895
3503.548224	468567.714998	49.654900
3503.479386	468557.798299	49.659905
3503.081556	468544.493206	49.664909
3503.649615	468543.231126	49.669914
3503.546215	468529.774439	49.674919
3503.652506	468521.955346	49.679924
3503.507698	468495.385948	49.684929
3503.442941	468472.095455	49.689933
3503.323100	468460.009226	49.694938
3503.167179	468449.296851	49.699943
3503.336131	468428.600491	49.704948
3503.198926	468413.072612	49.709953
3502.767879	468410.208168	49.714957
3503.256097	468399.791026	49.719962
3503.023312	468393.397481	49.724967
3502.908046	468375.687627	49.729972
3502.915961	468375.027737	49.734977
3502.717652	468362.498942	49.739981
3503.340197	468349.627356	49.744986
3503.339836	468347.449203	49.749991
3503.421220	468340.748718	49.754996
3503.196818	468327.211236	49.760001
3503.354566	468316.951788	49.765005
3503.425659	468306.555162	49.770010
3503.088653	468304.079893	49.775015
3503.309062	468284.539679	49.780020
3503.127709	468277.377472	49.785025
3502.946071	468270.975152	49.790029
3502.857994	468257.515656	49.795034
3502.855034	468253.716940	49.800039
3503.118352	468238.475123	49.805044
3503.198451	468233.395817	49.810049
3503.050263	468230.584360	49.815053
3503.069762	468216.295968	49.820058
3502.741742	468220.151181	49.825063
3502.826360	468224.898404	49.830068
3503.093184	468230.171732	49.835073
3502.663643	468232.220654	49.840077
3502.986275	468209.826163	49.845082
3502.737693	468209.058095	49.850087
3502.968840	468189.921201	49.855092
3502.749023	468186.767374	49.860097
3502.786716	468179.567729	49.865101
3502.982917	468167.933915	49.870106
3502.940494	468179.136197	49.875111
3502.782588	468192.029848	49.880116
3502.844677	468190.043639	49.885121
3502.583114	468185.731846	49.890125
3503.006084	468180.340699	49.895130
3502.910849	468174.784752	49.900135
3503.043356	468158.957331	49.905140
3502.924768	468156.090153	49.910145
3503.232177	468151.529233	49.915149
3503.289790	468134.093574	49.920154
3503.174240	468145.257706	49.925159
3503.085656	468130.278514	49.930164
3503.038856	468115.089550	49.935169
3503.025674	468114.028002	49.940173
3502.994364	468102.179712	49.945178
3503.070249	468110.677037	49.950183
3502.823246	468095.420928	49.955188
3502.868000	468097.794132	49.960193
3502.867629	468111.978009	49.965197
3503.181303	468102.502326	49.970202
3503.002045	468101.975699	49.975207
3503.196422	468097.028814	49.980212
3503.064344	468085.501658	49.985217
3502.780638	468084.334329	49.990221
3503.239250	468068.096555	49.995226
3502.910321	468071.040134	50.000231
3502.910592	468061.364660	50.005236
3502.845145	468047.293272	50.010241
3503.052215	468050.905183	50.015245
3503.161706	468036.601290	50.020250
3503.118472	468029.415407	50.025255
3503.047049	468011.647072	50.030260
3502.932993	468005.182466	50.035265
3502.592219	468002.859771	50.040269
3502.716375	468012.108750	50.045274
3502.738275	468024.262619	50.050279
3502.657383	468025.745463	50.055284
3502.787741	468015.135933	50.060289
3503.065912	468014.987110	50.065293
3503.232873	468004.827235	50.070298
3503.096649	467999.582176	50.075303
3503.393089	467979.927355	50.080308
3503.090227	467974.761398	50.085313
3503.015779	467979.231901	50.090317
3503.501007	467958.633001	50.095322
3503.152782	467959.097702	50.100327
3503.140603	467945.726340	50.105332
3503.400422	467943.959628	50.110337
3503.033496	467932.219194	50.115341
3502.990560	467921.639202	50.120346
3502.871029	467921.507627	50.125351
3503.086625	467912.200568	50.130356
3502.992521	467906.239093	50.135361
3503.000445	467903.603560	50.140365
3503.176938	467892.732799	50.145370
3503.243164	467875.650034	50.150375
3503.214869	467868.714825	50.155380
3502.764832	467865.853539	50.160385
3503.105898	467863.262433	50.165389
3503.182010	467848.204242	50.170394
3502.772438	467850.401765	50.175399
3503.110898	467865.490457	50.180404
3503.119354	467866.299515	50.185409
3502.684883	467864.702001	50.190413
3503.092825	467860.174503	50.195418
3502.919288	467857.519292	50.200423
3502.751216	467857.699949	50.205428
3503.165511	467843.546496	50.210433
3503.116210	467838.033264	50.215437
3503.117223	467822.329331	50.220442
3502.864656	467825.310565	50.225447
3502.750908	467809.879503	50.230452
3503.035459	467804.967803	50.235457
3502.596773	467799.622361	50.240461
3502.916430	467809.851203	50.245466
3502.938870	467819.877503	50.250471
3503.221690	467809.089854	50.255476
3503.151400	467815.434006	50.260481
3502.945409	467808.985031	50.265485
3503.158722	467805.098641	50.270490
3503.184699	467800.940292	50.275495
3503.370182	467791.486344	50.280500
3503.721131	467777.191687	50.285505
3503.320417	467759.428685	50.290509
3503.464251	467728.401736	50.295514
3503.290862	467729.444480	50.300519
3503.226823	467705.393066	50.305524
3503.381257	467704.404190	50.310529
3503.297785	467700.315166	50.315533
3503.313375	467684.102054	50.320538
3503.374072	467685.206146	50.325543
3503.049171	467682.374124	50.330548
3503.155158	467668.475815	50.335553
3502.876819	467673.234492	50.340557
3502.964165	467662.733426	50.345562
3502.770290	467660.486920	50.350567
3503.001424	467643.983683	50.355572
3503.138658	467636.361575	50.360577
3502.837468	467646.645855	50.365581
3502.969872	467628.031837	50.370586
3503.001377	467630.863281	50.375591
3502.823896	467640.721179	50.380596
3502.809541	467642.091377	50.385601
3502.743524	467646.864465	50.390605
3503.037164	467643.876165	50.395610
3502.865478	467639.396928	50.400615
3502.908938	467630.980305	50.405620
3502.856049	467629.266959	50.410625
3502.690193	467631.321577	50.415629
3503.014527	467614.194507	50.420634
3502.871201	467633.114325	50.425639
3502.965725	467635.276457	50.430644
3503.109758	467639.912366	50.435649
3502.895992	467641.975163	50.440653
3502.962872	467627.171663	50.445658
3502.986942	467622.304392	50.450663
3503.032940	467617.889297	50.455668
3502.971925	467607.565506	50.460673
3502.915356	467604.890286	50.465677
3503.278328	467596.571067	50.470682
3503.255094	467590.141471	50.475687
3503.011510	467589.321866	50.480692
3503.141309	467577.597715	50.485697
3503.017198	467570.020204	50.490701
3503.111312	467560.379111	50.495706
3503.167942	467557.836531	50.500711
3503.047996	467547.218822	50.505716
3503.228129	467553.064379	50.510721
3502.922050	467536.754093	50.515725
3503.173530	467535.849955	50.520730
3503.132706	467531.550980	50.525735
3503.185849	467497.347685	50.530740
3503.134917	467457.032453	50.535745
3503.240530	467409.699555	50.540749
3503.285003	467340.897767	50.545754
3503.321476	467275.389915	50.550759
3503.079479	467180.293913	50.555764
3503.216837	467082.245089	50.560769
3502.957906	466977.171100	50.565773
3502.993025	466864.346038	50.570778
3503.070344	466733.680744	50.575783
3503.034192	466597.410620	50.580788
3503.283079	466435.000497	50.585793
3503.149013	466268.246853	50.590797
3503.189922	466093.355997	50.595802
3503.292392	465903.659647	50.600807
3502.893492	465700.064093	50.605812
3503.041086	465485.480445	50.610817
3502.607546	465260.810178	50.615821
3502.775624	465026.306970	50.620826
3502.810874	464783.159846	50.625831
3502.800786	464527.300270	50.630836
3502.954506	464248.508037	50.635841
3502.468930	463969.618297	50.640845
3502.675630	463687.059589	50.645850
3502.650465	463378.847253	50.650855
3502.781646	463060.317402	50.655860
3503.161112	462730.136407	50.660865
3502.324865	462377.405935	50.665869
3502.615451	462001.420751	50.670874
3502.496296	461649.264178	50.675879
3502.395065	461261.778235	50.680884
3502.916015	460867.945378	50.685889
3502.516058	460453.129854	50.690893
3502.524586	460022.272475	50.695898
3502.273899	459583.341424	50.700903
3502.520479	459127.236691	50.705908
3502.453094	458650.547968	50.710913
3502.140990	458159.191813	50.715917
3502.330326	457665.913388	50.720922
3502.382234	457153.639526	50.725927
3501.971188	456626.175169	50.730932
3502.316951	456084.527385	50.735937
3501.925578	455521.701660	50.740941
3502.023419	454938.855512	50.745946
3502.044874	454360.263854	50.750951
3502.250595	453743.756483	50.755956
3502.222348	453121.795489	50.760961
3502.403071	452474.837378	50.765965
3501.886910	451810.132273	50.770970
3501.843323	451136.554095	50.775975
3501.629506	450440.725253	50.780980
3501.757237	449724.330823	50.785985
3501.600935	448997.920823	50.790989
3501.898194	448241.744867	50.795994
3501.626526	447466.521847	50.800999
3501.565100	446678.100570	50.806004
3501.598931	445879.389934	50.811009
3501.384295	445061.572605	50.816013
3501.676411	444221.981762	50.821018
3501.427579	443361.503969	50.826023
3501.017482	442476.318745	50.831028
3500.991252	441576.068876	50.836033
3500.923036	440666.861629	50.841037
3500.864535	439717.439603	50.846042
3500.752547	438762.101394	50.851047
3500.341166	437794.547057	50.856052
3500.733572	436802.360114	50.861057
3500.373699	435798.943794	50.866061
3500.347630	434763.461049	50.871066
3500.338566	433709.408051	50.876071
3500.071911	432643.882639	50.881076
3500.089542	431564.101503	50.886081
3499.826391	430454.377004	50.891085
3499.873292	429326.987282	50.896090
3499.413274	428188.007676	50.901095
3499.202883	427032.688996	50.906100
3499.394633	425848.313876	50.911105
3499.291309	424650.428474	50.916109
3499.189160	423419.386318	50.921114
3499.308770	422180.223091	50.926119
3498.733398	420923.829488	50.931124
3498.981296	419642.633192	50.936129
3498.610387	418349.418046	50.941133
3498.143204	417034.065326	50.946138
3498.153948	415708.178458	50.951143
3498.093692	414365.984936	50.956148
3498.148240	412982.567149	50.961153
3497.783724	411601.915045	50.966157
3497.862501	410194.221729	50.971162
3497.628582	408775.231103	50.976167
3497.621768	407335.757697	50.981172
3497.335660	405867.072132	50.986177
3497.048793	404391.703439	50.991181
3496.970234	402880.200912	50.996186
3496.604544	401381.442715	51.001191
3496.312981	399854.063056	51.006196
3496.454389	398305.770975	51.011201
3496.212446	396743.105918	51.016205
3495.900786	395167.435797	51.021210
3495.896656	393566.752562	51.026215
3495.221748	391958.702963	51.031220
3495.612735	390326.141919	51.036225
3495.516036	388673.880904	51.041229
3495.568114	387010.297791	51.046234
3495.361099	385323.210838	51.051239
3494.658480	383624.197505	51.056244
3494.398965	381900.005943	51.061249
3494.428647	380170.385983	51.066253
3494.213702	378415.295129	51.071258
3494.121753	376650.023493	51.076263
3493.727291	374867.575495	51.081268
3493.718843	373072.230936	51.086273
3493.032862	371266.433881	51.091277
3493.040509	369429.734447	51.096282
3492.523237	367589.292997	51.101287
3492.236539	365739.412107	51.106292
3492.283577	363862.678672	51.111297
3491.611271	361982.668957	51.116301
3491.702070	360086.718821	51.121306
3490.897169	358169.082581	51.126311
3490.673746	356257.080459	51.131316
3490.814133	354313.815695	51.136321
3490.385331	352353.538520	51.141325
3490.115598	350384.951970	51.146330
3489.871270	348406.324129	51.151335
3489.560293	346414.643555	51.156340
3489.533229	344407.840514	51.161345
3488.986775	342386.713767	51.166349
3488.727978	340344.789556	51.171354
3488.725731	338299.453169	51.176359
3488.064628	336248.190532	51.181364
3487.301617	334169.021476	51.186369
3487.143727	332098.141795	51.191373
3487.022442	329997.958317	51.196378
3486.946957	327898.654797	51.201383
3486.249626	325779.221454	51.206388
3486.303575	323642.325701	51.211393
3485.712441	321503.530440	51.216397
3485.538789	319347.179255	51.221402
3484.831015	317180.614125	51.226407
3484.599001	315008.501007	51.231412
3484.716869	312813.729964	51.236417
3484.195712	310621.318399	51.241421
3483.923857	308397.230443	51.246426
3483.287951	306165.045364	51.251431
3483.031971	303942.766508	51.256436
3482.701323	301675.502949	51.261441
3482.269802	299428.773399	51.266445
3481.926627	297166.163170	51.271450
3481.558300	294884.510428	51.276455
3481.071118	292592.159587	51.281460
3481.166735	290274.783846	51.286465
3480.715051	287983.915375	51.291469
3480.217171	285651.658315	51.296474
3480.398096	283312.574417	51.301479
3479.377867	280963.524111	51.306484
3479.502514	278605.204550	51.311489
3478.933302	276232.813718	51.316493
3478.089742	273858.939938	51.321498
3477.939008	271464.142385	51.326503
3476.913685	269068.123338	51.331508
3476.866695	266655.365388	51.336513
3476.364732	264253.774642	51.341517
3475.681833	261821.565662	51.346522
3475.450197	259397.574451	51.351527
3474.657077	256967.791723	51.356532
3474.389121	254523.427155	51.361537
3473.873995	252072.689621	51.366541
3473.282970	249608.931817	51.371546
3473.055609	247151.820095	51.376551
3472.440955	244681.137494	51.381556
3472.311186	242188.258319	51.386561
3471.332769	239706.955061	51.391565
3470.802162	237212.586847	51.396570
3470.382413	234707.405576	51.401575
3469.911440	232205.067677	51.406580
3469.487319	229685.671201	51.411585
3469.016357	227168.030411	51.416589
3468.574966	224638.283090	51.421594
3468.120512	222104.844454	51.426599
3467.123246	219568.496704	51.431604
3467.312250	217018.508768	51.436609
3466.398331	214470.605155	51.441613
3465.750454	211902.123944	51.446618
3465.126813	209338.115226	51.451623
3464.469646	206772.685770	51.456628
3463.991475	204187.905387	51.461633
3463.263980	201617.089818	51.466637
3462.657857	199033.231295	51.471642
3461.731688	196441.502214	51.476647
3460.885543	193869.662806	51.481652
3460.592138	191267.704282	51.486657
3459.579503	188682.699729	51.491661
3458.941942	186093.453106	51.496666
3458.886098	183501.995515	51.501671
3457.860833	180906.547670	51.506676
3457.008982	178310.965699	51.511681
3456.693668	175712.698008	51.516685
3455.720772	173112.182263	51.521690
3455.049747	170509.882710	51.526695
3454.295665	167905.462608	51.531700
3453.864304	165301.935886	51.536705
3452.815836	162702.481979	51.541709
3452.229790	160112.338719	51.546714
3451.460946	157499.770878	51.551719
3450.725987	154897.295506	51.556724
3450.128650	152289.445901	51.561729
3449.273803	149705.771480	51.566733
3448.618873	147021.683683	51.571738
3448.201076	144410.653787	51.576743
3447.387197	141816.304822	51.581748
3446.276228	139199.033299	51.586753
3445.436912	136606.433303	51.591757
3444.746417	134009.760121	51.596762
3443.825178	131409.477868	51.601767
3442.810250	128811.134785	51.606772
3442.134856	126231.879679	51.611777
3441.267779	123654.814101	51.616781
3440.164976	121081.054681	51.621786
3439.434760	118502.077894	51.626791
3438.650585	115930.792565	51.631796
3437.579237	113357.853822	51.636801
3436.771298	110801.779355	51.641805
3435.925119	108244.929343	51.646810
3434.853712	105693.460881	51.651815
3433.695775	103145.841938	51.656820
3432.818595	100611.306477	51.661825
3431.494679	98083.841007	51.666829
3430.270837	95577.825007	51.671834
3429.803967	93069.732610	51.676839
3428.613022	90575.348999	51.681844
3427.473944	88078.495060	51.686849
3426.294356	85607.499457	51.691853
3424.967198	83150.596152	51.696858
3423.849246	80686.867906	51.701863
3422.651778	78258.482700	51.706868
3421.377764	75829.938441	51.711873
3420.125504	73426.592023	51.716877
3418.704752	71019.445739	51.721882
3417.747340	68640.785106	51.726887
3416.031414	66285.424840	51.731892
3414.709322	63936.240984	51.736897
3412.925649	61610.897503	51.741901
3411.696387	59310.160307	51.746906
3410.173645	57037.058292	51.751911
3408.534289	54785.694872	51.756916
3406.220856	52554.817972	51.761921
3403.054794	50401.592191	51.766925
3398.551820	48319.737865	51.771930
3392.783419	46327.729290	51.776935
3386.324041	44442.285651	51.781940
3380.392785	42644.630767	51.786945
3374.325075	40960.462682	51.791949
3368.453663	39376.009312	51.796954
3362.870926	37912.767458	51.801959
3357.658529	36582.341149	51.806964
3352.056656	35341.852614	51.811969
3347.029781	34246.683303	51.816973
3342.551838	33240.978575	51.821978
3338.233314	32352.442849	51.826983
3333.711502	31554.194085	51.831988
3329.893653	30851.782103	51.836993
3326.528087	30236.336495	51.841997
3323.376945	29697.326217	51.847002
3320.804661	29235.115485	51.852007
3318.399537	28846.203620	51.857012
3316.301461	28502.912131	51.862017
3314.031897	28221.831884	51.867021
3312.682295	27987.609398	51.872026
3311.141008	27793.989468	51.877031
3310.170776	27646.138608	51.882036
3309.469053	27516.130156	51.887041
3308.576115	27410.023537	51.892045
3307.775355	27333.210294	51.897050
3307.103506	27258.738129	51.902055
3306.653354	27226.384779	51.907060
3305.673758	27184.737340	51.912065
3305.613474	27167.354356	51.917069
3305.052856	27140.931657	51.922074
3305.102656	27136.795447	51.927079
3304.752942	27139.809399	51.932084
3304.449001	27133.158952	51.937089
3304.190399	27141.309834	51.942093
3304.045266	27143.551864	51.947098
3304.010662	27135.533280	51.952103
3303.614345	27142.625950	51.957108
3303.525187	27136.378465	51.962113
3303.445123	27138.530305	51.967117
3303.276157	27136.439959	51.972122
3303.090105	27123.709108	51.977127
3302.723253	27113.232723	51.982132
3302.989860	27099.251100	51.987137
3303.083921	27078.931903	51.992141
3302.973974	27035.364998	51.997146
3302.529763	27003.156543	52.002151
3302.361579	26970.856713	52.007156
3302.496038	26920.637777	52.012161
3302.168277	26866.262778	52.017165
3301.848181	26808.755346	52.022170
3301.798232	26754.190906	52.027175
3301.190089	26678.464140	52.032180
3300.831319	26613.347699	52.037185
3300.236883	26540.668211	52.042189
3299.797435	26470.922985	52.047194
3299.639725	26390.467953	52.052199
3299.049541	26309.068737	52.057204
3298.711116	26217.698815	52.062209
3298.217640	26139.152544	52.067213
3297.436753	26058.720098	52.072218
3296.954740	25977.161625	52.077223
3296.378543	25899.044889	52.082228
3296.232319	25804.127312	52.087233
3295.891421	25739.672087	52.092237
3295.146524	25638.642921	52.097242
3294.329804	25545.340417	52.102247
3293.710488	25468.972455	52.107252
3293.379223	25358.620257	52.112257
3293.343746	25279.199469	52.117261
3292.589659	25184.284740	52.122266
3292.076597	25082.934559	52.127271
3291.327822	24984.547470	52.132276
3290.831621	24875.592751	52.137281
3290.033796	24768.369556	52.142285
3289.168548	24677.208400	52.147290
3288.852338	24565.258424	52.152295
3287.844000	24480.232727	52.157300
3287.542908	24380.276726	52.162305
3286.843132	24285.297550	52.167309
3286.568818	24175.426997	52.172314
3286.089749	24067.280853	52.177319
3285.244976	23971.543887	52.182324
3285.021531	23860.591423	52.187329
3283.843619	23757.610605	52.192333
3283.506750	23650.891137	52.197338
3282.840184	23537.578274	52.202343
3282.212334	23434.745753	52.207348
3281.742141	23320.018843	52.212353
3280.778794	23223.958429	52.217357
3279.906998	23115.072632	52.222362
3279.656768	23007.864840	52.227367
3278.884465	22909.338628	52.232372
3278.095748	22799.488809	52.237377
3278.067252	22696.131412	52.242381
3277.124469	22592.099176	52.247386
3276.796766	22467.275824	52.252391
3275.821041	22366.532874	52.257396
3275.322352	22245.443177	52.262401
3274.668753	22146.123188	52.267405
3273.679098	22031.939460	52.272410
3273.520790	21926.022312	52.277415
3272.576621	21828.040751	52.282420
3272.236693	21712.625642	52.287425
3271.762465	21606.015047	52.292429
3270.882507	21495.869802	52.297434
3270.080044	21381.797558	52.302439
3269.216280	21282.674996	52.307444
3268.921917	21166.710354	52.312449
3268.252157	21060.938099	52.317453
3267.381916	20956.968224	52.322458
3267.080714	20840.286064	52.327463
3265.981003	20733.138011	52.332468
3265.352759	20620.241001	52.337473
3264.468340	20514.298549	52.342477
3263.949566	20426.630874	52.347482
3263.246440	20298.074403	52.352487
3262.711364	20201.526213	52.357492
3261.901643	20101.770526	52.362497
3261.274033	19995.762138	52.367501
3260.586852	19894.584531	52.372506
3260.277505	19796.786002	52.377511
3259.419641	19693.691182	52.382516
3258.754296	19585.200449	52.387521
3258.086698	19472.627618	52.392525
3257.113208	19374.530814	52.397530
3257.067573	19277.594432	52.402535
3256.069536	19175.941497	52.407540
3255.384534	19069.537704	52.412545
3254.900070	18963.840108	52.417549
3254.124138	18865.443780	52.422554
3253.925800	18761.198684	52.427559
3253.058386	18662.188459	52.432564
3252.380266	18550.921321	52.437569
3251.865307	18445.793322	52.442573
3250.965425	18334.042289	52.447578
3250.485193	18230.430315	52.452583
3249.497912	18134.058100	52.457588
3249.175748	18020.174558	52.462593
3248.673992	17914.295226	52.467597
3247.795427	17808.093677	52.472602
3247.421440	17699.699628	52.477607
3246.616173	17599.829911	52.482612
3245.490001	17493.196886	52.487617
3245.161560	17389.162684	52.492621
3244.343955	17283.875518	52.497626
3243.824094	17178.389574	52.502631
3243.062478	17079.898493	52.507636
3242.758883	16975.396342	52.512641
3241.832020	16872.321073	52.517645
3241.387312	16761.552213	52.522650
3241.054830	16653.221047	52.527655
3240.196597	16552.138547	52.532660
3239.561111	16428.521711	52.537665
3238.685810	16320.707424	52.542669
3237.603807	16219.611427	52.547674
3237.237370	16108.618569	52.552679
3236.676149	16016.277581	52.557684
3235.881269	15915.093284	52.562689
3235.482931	15806.145091	52.567693
3234.832319	15708.408056	52.572698
3234.314539	15598.838384	52.577703
3233.489916	15490.897526	52.582708
3232.892169	15384.475306	52.587713
3232.289887	15276.776001	52.592717
3231.184137	15164.121982	52.597722
3230.532935	15051.003880	52.602727
3229.385021	14961.174295	52.607732
3229.056535	14856.283495	52.612737
3228.160039	14760.454110	52.617741
3227.731635	14670.683335	52.622746
3227.337334	14566.082169	52.627751
3226.713538	14477.319301	52.632756
3225.901132	14366.573851	52.637761
3225.481417	14274.404827	52.642765
3224.670330	14176.340745	52.647770
3224.168341	14066.042062	52.652775
3223.357645	13966.743376	52.657780
3222.561747	13861.981381	52.662785
3222.039359	13759.128090	52.667789
3221.333701	13662.068305	52.672794
3220.559492	13558.363288	52.677799
3219.892822	13457.010882	52.682804
3219.637928	13360.618562	52.687809
3218.828147	13270.724582	52.692813
3218.096394	13170.518059	52.697818
3217.818771	13057.386090	52.702823
3217.242532	12966.058571	52.707828
3216.567280	12855.560540	52.712833
3216.028036	12745.676815	52.717837
3214.621698	12644.615363	52.722842
3213.828488	12541.386130	52.727847
3213.139399	12445.681687	52.732852
3212.439106	12350.330500	52.737857
3212.083362	12249.633971	52.742861
3211.322509	12145.643244	52.747866
3210.908059	12046.860421	52.752871
3209.961367	11957.794948	52.757876
3209.210614	11857.422699	52.762881
3208.946097	11758.036113	52.767885
3208.148855	11669.106262	52.772890
3207.286452	11559.927175	52.777895
3206.623408	11465.222583	52.782900
3206.186122	11363.897606	52.787905
3205.561387	11263.637026	52.792909
3204.559619	11172.333720	52.797914
3204.250588	11072.928873	52.802919
3203.190882	10982.387023	52.807924
3202.819314	10877.664764	52.812929
3202.441034	10777.897508	52.817933
3201.657416	10679.454593	52.822938
3200.879523	10593.205310	52.827943
3200.665617	10493.435407	52.832948
3199.976883	10385.539521	52.837953
3199.320061	10285.037641	52.842957
3198.284120	10182.983327	52.847962
3198.089210	10075.624448	52.852967
3197.228650	9980.355532	52.857972
3196.516163	9876.527383	52.862977
3195.958034	9768.630649	52.867981
3194.756649	9667.920701	52.872986
3194.548072	9571.825536	52.877991
3193.566340	9476.338559	52.882996
3192.603122	9380.515638	52.888001
3192.164514	9279.295465	52.893005
3191.264420	9184.323920	52.898010
3190.841583	9089.854339	52.903015
3190.216842	8996.536714	52.908020
3189.761141	8906.231827	52.913025
3188.986856	8797.975629	52.918029
3188.023456	8697.904031	52.923034
3187.756371	8609.636480	52.928039
3186.996808	8517.877008	52.933044
3186.766084	8419.500242	52.938049
3186.025332	8317.497278	52.943053
3184.941622	8228.946377	52.948058
3184.529384	8121.376898	52.953063
3183.473654	8032.817553	52.958068
3182.901283	7938.744358	52.963073
3182.364823	7836.222988	52.968077
3181.579982	7747.270612	52.973082
3180.792677	7649.348262	52.978087
3179.563391	7559.456346	52.983092
3179.147500	7472.108987	52.988097
3178.779840	7380.783453	52.993101
3178.116744	7283.071945	52.998106
3177.312315	7197.103546	53.003111
3176.627271	7117.986499	53.008116
3176.019817	7023.328342	53.013121
3175.428238	6939.169137	53.018125
3175.309924	6854.976904	53.023130
3174.183028	6752.760757	53.028135
3173.445233	6672.762457	53.033140
3173.061645	6581.471825	53.038145
3172.247083	6485.471692	53.043149
3171.477046	6400.234593	53.048154
3171.252566	6304.494072	53.053159
3170.125671	6208.510262	53.058164
3169.588723	6127.649542	53.063169
3168.852257	6028.718290	53.068173
3167.910836	5959.070902	53.073178
3167.958908	5870.153257	53.078183
3166.795853	5773.585139	53.083188
3166.105239	5678.205199	53.088193
3165.933164	5592.048130	53.093197
3164.638641	5515.121692	53.098202
3164.324770	5425.128786	53.103207
3163.982402	5323.237084	53.108212
3163.019285	5243.808007	53.113217
3162.597050	5153.103085	53.118221
3161.551094	5062.648179	53.123226
3160.759729	4966.454989	53.128231
3159.759130	4877.197676	53.133236
3159.514497	4802.244061	53.138241
3159.180885	4718.549969	53.143245
3158.187505	4640.856903	53.148250
3157.064034	4541.768033	53.153255
3156.563258	4470.854715	53.158260
3156.080680	4390.945061	53.163265
3155.174562	4308.810247	53.168269
3154.159081	4227.811913	53.173274
3153.871401	4140.858819	53.178279
3153.082151	4061.882894	53.183284
3152.495640	3990.698144	53.188289
3151.651060	3905.458690	53.193293
3150.942136	3842.803155	53.198298
3150.096063	3764.235610	53.203303
3149.840748	3691.151025	53.208308
3149.304188	3610.615708	53.213313
3148.739587	3527.761721	53.218317
3147.580468	3462.247200	53.223322
3147.305967	3376.200954	53.228327
3146.689364	3307.135856	53.233332
3146.060265	3238.595918	53.238337
3145.658095	3151.609377	53.243341
3144.704473	3076.359445	53.248346
3143.962575	3003.909940	53.253351
3142.896566	2918.100906	53.258356
3141.985102	2846.124850	53.263361
3141.653045	2779.683052	53.268365
3140.852141	2717.144813	53.273370
3140.352719	2645.392998	53.278375
3139.699880	2573.916439	53.283380
3138.545572	2504.135037	53.288385
3138.346846	2431.853546	53.293389
3137.830922	2366.868499	53.298394
3137.448455	2293.073062	53.303399
3136.483640	2222.791530	53.308404
3135.557110	2151.535773	53.313409
3135.124761	2079.521627	53.318413
3134.634469	2019.867068	53.323418
3133.399970	1938.362841	53.328423
3132.556688	1873.618147	53.333428
3132.103841	1808.235383	53.338433
3131.705557	1740.991316	53.343437
3130.556827	1672.123781	53.348442
3130.320974	1607.560631	53.353447
3129.274452	1544.483978	53.358452
3128.759312	1479.165730	53.363457
3128.205545	1421.381644	53.368461
3127.446204	1363.574864	53.373466
3126.666362	1293.007323	53.378471
3126.066712	1242.029851	53.383476
3125.494167	1175.076546	53.388481
3124.656609	1106.602428	53.393485
3123.987642	1057.209306	53.398490
3123.115341	993.815751	53.403495
3122.618881	941.114336	53.408500
3122.246828	883.197762	53.413505
3121.410869	816.236128	53.418509
3120.502345	761.640680	53.423514
3120.034492	698.025665	53.428519
3119.324132	655.332950	53.433524
3118.716640	596.397785	53.438529
3118.134728	533.573458	53.443533
3116.934913	483.589952	53.448538
3116.668474	425.649527	53.453543
3115.847609	378.212786	53.458548
3114.993698	330.024343	53.463553
3114.272481	286.379634	53.468557
3113.393780	238.782280	53.473562
3112.685436	202.848644	53.478567
3111.733700	154.655749	53.483572
3110.271259	132.532811	53.488577
3108.205425	137.812370	53.493581
3106.748040	146.677100	53.498586
3105.815400	144.531228	53.503591
3105.163835	138.922932	53.508596
3105.149900	143.472569	53.513601
3105.084804	144.740888	53.518605
3104.603100	149.740705	53.523610
3103.986524	146.673217	53.528615
3103.249831	141.202226	53.533620
3102.296944	145.160733	53.538625
3101.775637	142.084467	53.543629
3101.276835	149.708595	53.548634
3100.377057	145.702675	53.553639
3100.244002	144.058855	53.558644
3098.840030	153.692473	53.563649
3098.702613	142.369871	53.568653
3097.860812	154.138439	53.573658
3097.421527	145.065261	53.578663
3096.541918	142.617046	53.583668
3096.063622	148.513104	53.588673
3095.429829	144.531210	53.593677
3094.958532	153.833761	53.598682
3094.532727	150.083954	53.603687
3093.972171	142.490416	53.608692
3092.728338	149.004765	53.613697
3091.985230	146.965060	53.618701
3091.349875	143.089221	53.623706
3090.827599	148.203731	53.628711
3090.024010	146.105678	53.633716
3089.291032	149.418731	53.638721
3089.030861	140.034696	53.643725
3088.627224	152.233648	53.648730
3087.763956	145.282345	53.653735
3087.154084	144.516953	53.658740
3086.688682	151.920643	53.663745
3085.864606	147.823634	53.668749
3085.052736	155.208764	53.673754
3084.466873	143.162674	53.678759
3083.809867	145.741182	53.683764
3082.795376	145.614518	53.688769
3082.722559	144.095403	53.693773
3081.626714	152.572714	53.698778
3081.402717	143.936034	53.703783
3080.942165	142.383698	53.708788
3079.939741	146.799872	53.713793
3079.246527	139.761097	53.718797
3078.409470	147.073161	53.723802
3077.710883	146.392795	53.728807
3077.260226	142.565134	53.733812
3076.702092	149.131267	53.738817
3076.218164	153.043595	53.743821
3075.535766	144.622606	53.748826
3074.314096	153.402070	53.753831
3074.390354	149.970681	53.758836
3073.337747	150.662093	53.763841
3072.618486	144.522617	53.768845
3072.813490	152.874100	53.773850
3072.451387	145.842694	53.778855
3071.566432	143.519342	53.783860
3070.472159	156.059324	53.788865
3069.695026	148.529634	53.793869
3068.248683	150.537243	53.798874
3067.781095	145.197510	53.803879
3067.779927	136.595391	53.808884
3066.807068	147.619392	53.813889
3066.176196	139.517622	53.818893
3065.199611	148.220077	53.823898
3064.645174	145.813803	53.828903
3064.366919	139.938442	53.833908
3063.437298	154.693923	53.838913
3063.272769	138.723301	53.843917
3062.568031	139.137384	53.848922
3062.045819	149.806101	53.853927
3061.166936	144.054289	53.858932
3060.073362	150.735597	53.863937
3059.688246	151.082830	53.868941
3059.353198	151.627556	53.873946
3058.664069	153.493152	53.878951
3058.167620	145.337229	53.883956
3057.196266	149.918620	53.888961
3056.077812	148.728959	53.893965
3055.338140	142.830996	53.898970
3055.018157	152.482683	53.903975
3054.438295	146.951745	53.908980
3053.605855	147.099498	53.913985
3053.467562	146.111033	53.918989
3053.002427	147.204555	53.923994
3052.231615	149.908300	53.928999
3051.525258	148.437440	53.934004
3050.578645	158.901583	53.939009
3049.858371	148.398167	53.944013
3049.045245	146.508588	53.949018
3048.029383	146.774129	53.954023
3047.919247	139.771910	53.959028
3047.469558	148.587224	53.964033
3046.907985	140.945711	53.969037
3045.888419	148.307515	53.974042
3044.781471	150.137534	53.979047
3045.051104	145.689442	53.984052
3044.572648	148.755723	53.989057
3043.965843	143.056501	53.994061
3043.262113	145.141692	53.999066
3041.678049	148.640044	54.004071
3041.562323	144.250300	54.009076
3040.541681	149.863250	54.014081
3040.034270	145.195442	54.019085
3038.929198	147.653153	54.024090
3039.076647	152.119950	54.029095
3038.845251	145.976458	54.034100
3037.421724	153.653602	54.039105
3036.923531	148.547254	54.044109
3036.574567	148.902126	54.049114
3035.633044	152.901726	54.054119
3034.729560	151.870727	54.059124
3033.722526	149.944416	54.064129
3033.209186	145.168678	54.069133
3032.274466	145.071812	54.074138
3031.972529	149.582240	54.079143
3032.254210	139.390773	54.084148
3030.982767	149.242930	54.089153
3030.454147	148.739180	54.094157
3029.256472	144.706021	54.099162
3028.418870	152.673037	54.104167
3028.531052	150.638374	54.109172
3028.422905	155.783965	54.114177
3027.203205	143.127394	54.119181
3026.031824	151.879717	54.124186
3026.037268	149.058048	54.129191
3025.607470	136.439005	54.134196
3024.270317	142.843785	54.139201
3024.202588	141.300907	54.144205
3023.285160	153.660280	54.149210
3022.504429	147.958412	54.154215
3021.709107	138.478337	54.159220
3020.800988	141.310150	54.164225
3020.551634	144.496753	54.169229
3019.602253	147.979024	54.174234
3018.850261	141.904756	54.179239
3018.236381	145.252725	54.184244
3017.259418	146.579758	54.189249
3017.160187	137.083763	54.194253
3017.127253	132.326596	54.199258
3016.492031	138.223019	54.204263
3015.599602	138.485236	54.209268
3013.958846	144.036392	54.214273
3013.819116	140.382972	54.219277
3013.670377	142.726217	54.224282
3012.645128	132.415458	54.229287
3012.500044	137.527091	54.234292
3010.850014	142.514186	54.239297
3010.691449	130.603128	54.244301
3010.011213	138.465486	54.249306
3009.057512	138.637914	54.254311
3008.946446	137.963344	54.259316
3007.808151	144.944001	54.264321
3007.035570	134.150339	54.269325
3006.693021	142.450774	54.274330
3005.800373	139.366529	54.279335
3005.217772	136.740082	54.284340
3004.544796	140.794844	54.289345
3003.765091	139.999272	54.294349
3003.309854	140.764272	54.299354
3003.334210	144.129098	54.304359
3002.406673	140.363990	54.309364
3001.191293	136.549387	54.314369
3000.545218	141.545714	54.319373
2999.804125	131.279953	54.324378
2999.387795	133.021964	54.329383
2999.761410	133.257312	54.334388
2998.143524	136.105414	54.339393
2997.021219	136.209946	54.344397
2996.860851	139.911462	54.349402
2996.331582	141.018315	54.354407
2995.763706	134.846278	54.359412
2994.621647	143.737271	54.364417
2994.392098	140.573663	54.369421
2993.442633	131.023232	54.374426
2993.155581	134.560083	54.379431
2992.324270	139.575037	54.384436
2990.569469	126.266660	54.389441
2990.950017	128.670243	54.394445
2990.208913	126.615609	54.399450
2989.465013	131.895881	54.404455
2989.332675	128.465013	54.409460
2988.272017	133.575208	54.414465
2987.868850	138.203982	54.419469
2987.648380	140.833819	54.424474
2986.134887	133.809714	54.429479
2984.858983	132.799339	54.434484
2984.484586	135.849023	54.439489
2984.079535	136.343348	54.444493
2983.674198	134.016211	54.449498
2982.801362	136.400692	54.454503
2982.457613	138.605554	54.459508
2981.612924	142.795053	54.464513
2981.239469	139.706563	54.469517
2980.539918	137.261943	54.474522
2979.768280	138.553500	54.479527
2979.306609	125.380593	54.484532
2978.552404	134.125964	54.489537
2978.233941	139.054071	54.494541
2977.400224	133.809287	54.499546
2975.801018	138.097326	54.504551
2975.322851	134.305565	54.509556
2974.886261	144.195058	54.514561
2974.571450	138.715156	54.519565
2974.131508	137.244176	54.524570
2973.478796	143.150696	54.529575
2972.808308	128.783106	54.534580
2971.046614	133.019966	54.539585
2970.694505	126.596334	54.544589
2970.740298	125.474971	54.549594
2970.224896	133.025351	54.554599
2969.628972	126.977323	54.559604
2967.845282	142.281757	54.564609
2967.798125	138.087534	54.569613
2967.602430	136.420872	54.574618
2966.669910	128.740930	54.579623
2965.936715	132.261259	54.584628
2964.452317	135.451286	54.589633
2964.668695	130.135609	54.594637
2964.092953	132.929181	54.599642
2962.693993	133.008762	54.604647
2963.129722	134.417674	54.609652
2961.764361	137.481968	54.614657
2960.960910	132.227279	54.619661
2960.826706	126.607181	54.624666
2959.478493	137.897818	54.629671
2959.640041	121.887695	54.634676
2958.566862	130.909804	54.639681
2957.621798	131.068528	54.644685
2957.501131	129.521674	54.649690
2956.552036	140.516747	54.654695
2955.880096	132.508072	54.659700
2954.934585	139.224083	54.664705
2955.030673	135.955886	54.669709
2954.906432	128.268871	54.674714
2953.961608	124.672121	54.679719
2953.207935	125.270628	54.684724
2952.503810	130.071616	54.689729
2950.640355	127.457224	54.694733
2950.012845	125.246608	54.699738
2949.900066	132.588846	54.704743
2949.623138	139.763354	54.709748
2949.145188	137.529547	54.714753
2948.233824	132.435798	54.719757
2947.135478	127.108748	54.724762
2945.921495	136.182554	54.729767
2945.865292	128.449178	54.734772
2945.599825	133.730192	54.739777
2945.150839	130.272124	54.744781
2944.706431	129.807675	54.749786
2943.382843	142.367104	54.754791
2942.194730	131.809862	54.759796
2942.053163	137.203121	54.764801
2941.716836	136.895856	54.769805
2940.342300	123.486206	54.774810
2940.111711	137.294470	54.779815
2940.117084	127.903769	54.784820
2938.791720	128.064724	54.789825
2937.704914	133.978717	54.794829
2937.141660	129.037452	54.799834
2936.759292	144.790034	54.804839
2936.795874	126.687499	54.809844
2935.736493	126.872473	54.814849
2934.502232	132.758771	54.819853
2934.371851	124.792158	54.824858
2933.714614	135.637881	54.829863
2932.910834	125.848236	54.834868
2932.445358	125.446597	54.839873
2931.943581	125.361023	54.844877
2931.428349	128.085835	54.849882
2930.520265	130.029121	54.854887
2929.219657	126.467519	54.859892
2928.768648	129.223987	54.864897
2928.149657	129.021868	54.869901
2927.690307	120.983980	54.874906
2926.893623	121.312742	54.879911
2926.038324	118.663438	54.884916
2925.615490	124.312781	54.889921
2925.161649	125.512535	54.894925
2924.258614	126.521823	54.899930
2923.431839	132.102045	54.904935
2923.080828	127.074776	54.909940
2922.578250	124.658082	54.914945
2921.804309	125.875830	54.919949
2921.654800	121.840812	54.924954
2920.667787	126.913561	54.929959
2920.457849	123.951869	54.934964
2918.765424	127.613628	54.939969
2917.670650	127.538608	54.944973
2917.964729	123.546596	54.949978
2917.090556	131.164603	54.954983
2916.440688	126.211302	54.959988
2915.307479	132.964917	54.964993
2915.472030	132.369956	54.969997
2914.572149	123.623030	54.975002
2913.464269	127.167132	54.980007
2913.249229	124.298679	54.985012
2912.189552	127.564945	54.990017
2911.707658	123.633703	54.995021
2911.552389	123.618385	55.000026
2910.458457	126.724720	55.005031
2910.044355	117.565974	55.010036
2909.780071	123.567553	55.015041
2909.015880	126.687404	55.020045
2908.255765	126.403223	55.025050
2906.706786	123.951415	55.030055
2906.192477	126.191347	55.035060
2905.763377	134.401568	55.040065
2905.042192	131.456984	55.045069
2904.420423	126.138893	55.050074
2904.084369	129.095185	55.055079
2903.505817	114.444291	55.060084
2902.957723	128.505746	55.065089
2902.325460	126.730149	55.070093
2901.885326	119.936713	55.075098
2900.365252	123.724544	55.080103
2899.153254	113.464298	55.085108
2898.916826	127.240389	55.090113
2898.867154	119.234728	55.095117
2898.731791	123.247352	55.100122
2896.772843	127.609911	55.105127
2896.816605	118.637781	55.110132
2895.554087	125.072055	55.115137
2895.481541	126.503088	55.120141
2894.827999	121.855150	55.125146
2894.182418	125.489191	55.130151
2893.791003	127.410103	55.135156
2892.996862	123.605250	55.140161
2892.046733	122.479226	55.145165
2890.887560	123.058620	55.150170
2890.364579	128.412456	55.155175
2890.724383	122.409920	55.160180
2889.787970	123.950299	55.165185
2888.581893	126.133985	55.170189
2888.000965	120.849575	55.175194
2887.174828	117.557417	55.180199
2886.641333	117.376217	55.185204
2886.443648	115.430830	55.190209
2885.813989	126.225256	55.195213
2885.161199	109.909864	55.200218
2883.757855	122.366074	55.205223
2882.739376	120.077025	55.210228
2882.913527	124.258589	55.215233
2882.091053	121.144616	55.220237
2881.753995	118.357018	55.225242
2880.530377	120.509361	55.230247
2880.103061	114.871474	55.235252
2879.305851	117.102124	55.240257
2878.912790	121.073131	55.245261
2878.355337	110.853395	55.250266
2877.603456	132.118702	55.255271
2877.202084	115.981780	55.260276
2877.074706	118.006379	55.265281
2875.862758	117.163123	55.270285
2874.952843	116.736789	55.275290
2874.097571	122.525955	55.280295
2873.656481	120.045076	55.285300
2873.290534	117.932661	55.290305
2872.683226	124.700213	55.295309
2871.732893	109.388152	55.300314
2870.460135	114.173036	55.305319
2869.806214	116.409198	55.310324
2869.446020	114.540531	55.315329
2868.843254	121.928605	55.320333
2868.238924	112.815405	55.325338
2867.135728	121.861594	55.330343
2866.775978	104.684969	55.335348
2866.271758	116.365820	55.340353
2865.659289	122.687423	55.345357
2865.693356	114.565222	55.350362
2864.552310	114.272336	55.355367
2864.180905	115.413401	55.360372
2863.230216	119.251557	55.365377
2861.932155	124.384576	55.370381
2861.539856	115.702101	55.375386
2860.775046	121.671197	55.380391
2860.310495	116.548083	55.385396
2859.724689	123.987338	55.390401
2859.306150	120.577367	55.395405
2859.112157	122.841503	55.400410
2858.229293	124.822328	55.405415
2857.263136	115.208482	55.410420
2856.354073	121.105524	55.415425
2855.497574	116.675038	55.420429
2855.113797	104.860144	55.425434
2854.212738	117.356033	55.430439
2853.728932	112.471469	55.435444
2853.506997	112.176237	55.440449
2852.738467	111.952712	55.445453
2852.344308	112.623995	55.450458
2850.565827	124.080535	55.455463
2850.010044	120.076669	55.460468
2849.364137	118.733268	55.465473
2849.497724	119.579218	55.470477
2849.045551	119.495041	55.475482
2847.753298	118.411707	55.480487
2847.110488	121.984885	55.485492
2846.556501	125.198681	55.490497
2846.351299	122.014744	55.495501
2845.736739	109.799171	55.500506
2843.874264	123.179752	55.505511
2843.452854	123.031110	55.510516
2843.096629	117.662911	55.515521
2842.545702	130.411199	55.520525
2842.192782	119.062722	55.525530
2841.158946	127.030511	55.530535
2840.715654	111.566277	55.535540
2840.171421	113.531069	55.540545
2839.609559	124.640345	55.545549
2839.029783	113.437614	55.550554
2837.472896	119.241697	55.555559
2836.879189	115.166159	55.560564
2836.412985	114.424400	55.565569
2835.388129	122.007373	55.570573
2835.499228	104.530421	55.575578
2834.686956	113.589648	55.580583
2834.252999	117.679748	55.585588
2833.592008	113.078489	55.590593
2833.014263	122.414604	55.595597
2832.365091	113.253024	55.600602
2831.341638	121.345350	55.605607
2830.512308	118.699125	55.610612
2829.701751	126.165740	55.615617
2829.434510	123.796070	55.620621
2828.815244	117.328123	55.625626
2828.509519	127.232339	55.630631
2828.273618	118.047493	55.635636
2826.968581	119.134580	55.640641
2825.473905	124.197000	55.645645
2824.839753	115.088511	55.650650
2824.288998	122.448356	55.655655
2823.723067	113.436757	55.660660
2823.671115	110.707803	55.665665
2822.983003	120.413691	55.670669
2822.764715	116.435041	55.675674
2821.997924	118.640368	55.680679
2821.008069	119.014395	55.685684
2819.657033	113.256503	55.690689
2818.918715	123.576879	55.695693
2818.622117	116.910106	55.700698
2817.932084	118.004580	55.705703
2817.410911	118.796255	55.710708
2817.097509	124.744256	55.715713
2816.418154	124.958245	55.720717
2816.500968	120.066050	55.725722
2815.089011	130.371698	55.730727
2814.138750	123.673355	55.735732
2813.515230	115.266848	55.740737
2812.973483	117.319637	55.745741
2812.390438	119.487640	55.750746
2811.960642	114.745030	55.755751
2810.844493	115.428005	55.760756
2809.811278	117.011386	55.765761
2809.089594	119.426105	55.770765
2808.785952	116.948978	55.775770
2808.099011	120.567989	55.780775
2807.417377	125.420798	55.785780
2806.926052	122.182348	55.790785
2806.714993	124.520453	55.795789
2806.570969	114.749923	55.800794
2804.911079	126.881713	55.805799
2803.810779	126.058863	55.810804
2803.565443	119.504904	55.815809
2802.637228	117.387151	55.820813
2802.165166	109.702768	55.825818
2801.752619	128.305663	55.830823
2801.099821	114.385888	55.835828
2801.108715	116.087993	55.840833
2800.220731	122.807600	55.845837
2798.862169	111.429310	55.850842
2798.199050	114.300980	55.855847
2797.685221	115.593492	55.860852
2797.002998	118.466060	55.865857
2796.462305	125.822213	55.870861
2796.149937	114.964567	55.875866
2795.304302	118.381760	55.880871
2794.195120	124.267619	55.885876
2793.374974	114.775279	55.890881
2792.681635	115.972160	55.895885
2792.359906	110.849515	55.900890
2791.574886	120.035534	55.905895
2791.214805	113.823683	55.910900
2790.547510	116.392523	55.915905
2790.131652	115.977285	55.920909
2789.993436	106.370766	55.925914
2788.243938	119.331003	55.930919
2787.361265	113.212420	55.935924
2787.120316	117.121116	55.940929
2786.241120	111.922045	55.945933
2786.050459	112.661969	55.950938
2785.363249	117.297052	55.955943
2785.110370	113.912460	55.960948
2784.498469	120.406463	55.965953
2783.603061	115.394105	55.970957
2783.314140	116.206875	55.975962
2781.334866	110.014019	55.980967
2780.534691	120.111287	55.985972
2780.401004	107.393948	55.990977
2779.867549	118.979139	55.995981
2778.575563	114.604944	56.000986
2778.277478	117.928158	56.005991
2778.267929	118.137009	56.010996
2777.391641	110.055944	56.016001
2776.332368	110.568945	56.021005
2776.351558	116.998108	56.026010
2775.622710	117.606998	56.031015
2774.839969	119.700586	56.036020
2773.867677	115.131228	56.041025
2772.943532	123.322241	56.046029
2772.630277	113.054472	56.051034
2771.576970	114.973652	56.056039
2771.239435	117.590340	56.061044
2771.169501	113.019117	56.066049
2770.149449	122.621879	56.071053
2769.807161	118.294568	56.076058
2768.261988	106.857795	56.081063
2767.576939	114.330194	56.086068
2767.477714	115.436190	56.091073
2766.840736	122.443283	56.096077
2766.335273	117.690717	56.101082
2765.799046	115.480314	56.106087
2764.468807	112.940638	56.111092
2763.933813	113.424425	56.116097
2763.480498	127.079287	56.121101
2763.156838	123.654294	56.126106
2762.820108	116.129147	56.131111
2761.557791	120.311494	56.136116
2760.301565	111.211059	56.141121
2759.315512	123.374518	56.146125
2759.358796	116.385982	56.151130
2758.912477	124.659532	56.156135
2758.295981	126.530107	56.161140
2757.915134	115.450493	56.166145
2757.009423	119.405314	56.171149
2756.120913	115.189130	56.176154
2755.381411	122.948727	56.181159
2754.331928	114.501357	56.186164
2754.183449	112.354941	56.191169
2753.461914	114.854111	56.196173
2753.368281	105.710885	56.201178
2752.539110	116.170729	56.206183
2751.198926	116.152686	56.211188
2750.351202	110.507731	56.216193
2749.859170	113.438186	56.221197
2749.535440	115.195564	56.226202
2748.725557	122.797854	56.231207
2747.415055	123.864183	56.236212
2747.326296	117.095580	56.241217
2746.673274	120.706035	56.246221
2746.504008	113.641729	56.251226
2746.059373	111.440148	56.256231
2745.852481	119.595010	56.261236
2744.847340	114.610100	56.266241
2743.906565	122.513439	56.271245
2743.325688	110.976982	56.276250
2741.819240	115.004879	56.281255
2740.854395	120.377007	56.286260
2740.997934	109.609996	56.291265
2740.354512	117.729737	56.296269
2739.488035	121.710616	56.301274
2739.230930	121.404822	56.306279
2738.455753	118.274502	56.311284
2737.937598	120.506418	56.316289
2736.898773	122.393130	56.321293
2736.039098	121.130887	56.326298
2735.207091	115.512061	56.331303
2734.476762	118.109443	56.336308
2734.162947	109.434893	56.341313
2733.492456	115.353533	56.346317
2733.031003	113.639550	56.351322
2732.658864	108.952621	56.356327
2731.901273	110.434037	56.361332
2731.981869	106.412204	56.366337
2730.436097	119.426837	56.371341
2729.541643	116.273092	56.376346
2729.142863	117.492262	56.381351
2728.221062	115.785125	56.386356
2727.871646	114.892364	56.391361
2727.352263	120.978199	56.396365
2726.783513	110.327412	56.401370
2725.683705	119.182381	56.406375
2724.777196	121.644884	56.411380
2724.210163	111.168272	56.416385
2723.972112	120.394219	56.421389
2723.535711	116.201418	56.426394
2722.791407	115.163397	56.431399
2721.155246	117.616016	56.436404
2720.672083	115.022349	56.441409
2720.055022	117.119991	56.446413
2719.517457	105.100891	56.451418
2719.186395	103.410806	56.456423
2718.943307	112.961284	56.461428
2718.606303	109.382662	56.466433
2717.248586	119.375896	56.471437
2716.582418	111.353268	56.476442
2715.814926	113.786088	56.481447
2714.953922	110.777020	56.486452
2714.866201	104.410868	56.491457
2714.411297	112.837058	56.496461
2713.179957	107.950426	56.501466
2712.496061	110.715526	56.506471
2711.320857	116.062035	56.511476
2710.940541	112.771861	56.516481
2710.329007	121.661396	56.521485
2710.295213	114.228157	56.526490
2710.019109	113.830089	56.531495
2708.915065	114.777059	56.536500
2708.046950	110.557400	56.541505
2707.543761	117.871220	56.546509
2706.813182	112.225590	56.551514
2706.411594	111.593189	56.556519
2704.956361	108.196630	56.561524
2704.531801	105.959649	56.566529
2703.706725	120.445394	56.571533
2703.164263	115.751265	56.576538
2702.964705	114.650922	56.581543
2702.092164	120.428844	56.586548
2702.040529	110.767272	56.591553
2700.610887	116.765547	56.596557
2699.671520	105.300644	56.601562
2699.371192	113.505023	56.606567
2698.476208	112.508946	56.611572
2698.391741	105.125031	56.616577
2697.776529	118.021656	56.621581
2696.701621	108.577233	56.626586
2695.945397	108.687537	56.631591
2694.990866	115.194320	56.636596
2694.734554	105.974306	56.641601
2694.208446	104.825179	56.646605
2693.761277	116.723238	56.651610
2693.099018	114.442022	56.656615
2691.948067	121.094880	56.661620
2691.192807	110.018494	56.666625
2690.732491	118.599555	56.671629
2689.780711	108.785544	56.676634
2689.662785	104.636599	56.681639
2688.817415	118.753979	56.686644
2688.835476	104.932722	56.691649
2687.173475	109.743513	56.696653
2686.295618	111.491011	56.701658
2685.945353	110.861680	56.706663
2685.492941	121.790798	56.711668
2685.186658	108.003665	56.716673
2684.231089	111.610972	56.721677
2683.648985	105.130783	56.726682
2683.194813	111.096129	56.731687
2682.001441	119.365929	56.736692
2681.686369	108.663107	56.741697
2680.890517	115.261580	56.746701
2680.435844	118.094867	56.751706
2679.268853	112.263322	56.756711
2678.361783	123.055428	56.761716
2678.020607	111.600376	56.766721
2677.310437	115.512702	56.771725
2676.897052	109.114985	56.776730
2676.285790	115.313626	56.781735
2675.742640	116.656554	56.786740
2675.479705	113.284742	56.791745
2674.699393	114.255720	56.796749
2673.729289	111.031237	56.801754
2673.429325	107.203532	56.806759
2672.372543	108.211507	56.811764
2671.824972	102.776572	56.816769
2670.456089	117.826967	56.821773
2670.032583	106.955583	56.826778
2669.332536	115.077898	56.831783
2668.497759	108.401698	56.836788
2668.374668	109.499143	56.841793
2667.752203	108.657008	56.846797
2667.384720	109.459133	56.851802
2666.978819	106.870818	56.856807
2665.798871	109.579404	56.861812
2665.174113	102.960857	56.866817
2664.502416	112.688804	56.871821
2663.981881	107.446610	56.876826
2663.166389	108.481233	56.881831
2662.091207	110.146021	56.886836
2661.860672	105.659100	56.891841
2661.074928	105.842348	56.896845
2660.648142	107.285381	56.901850
2660.169208	111.354753	56.906855
2658.747122	110.431812	56.911860
2658.547233	103.401174	56.916865
2657.819217	104.554263	56.921869
2657.352246	107.409387	56.926874
2656.796518	100.747464	56.931879
2655.428976	109.697937	56.936884
2654.456475	103.913285	56.941889
2654.124307	102.604699	56.946893
2653.579409	105.224862	56.951898
2652.989213	99.770376	56.956903
2652.125208	102.542584	56.961908
2651.886920	109.007063	56.966913
2651.618744	111.676238	56.971917
2651.131240	108.284003	56.976922
2650.370139	110.201015	56.981927
2649.183628	110.492639	56.986932
2649.032383	105.346395	56.991937
2648.113012	110.121037	56.996941
2646.825309	104.647629	57.001946
2645.988037	105.635848	57.006951
2645.491123	108.560827	57.011956
2645.033281	99.416720	57.016961
2644.571239	104.114368	57.021965
2644.386902	105.720820	57.026970
2643.674483	103.312007	57.031975
2642.733363	107.600118	57.036980
2641.846050	106.264460	57.041985
2640.918419	113.205978	57.046989
2640.450339	109.028473	57.051994
2640.161278	108.260397	57.056999
2639.250505	112.098862	57.062004
2639.149404	105.744082	57.067009
2637.833463	110.643357	57.072013
2637.174266	110.188414	57.077018
2636.663059	103.599407	57.082023
2636.044198	117.440835	57.087028
2635.780222	108.740413	57.092033
2634.725366	106.977883	57.097037
2633.504320	104.485891	57.102042
2633.182523	109.457585	57.107047
2632.539200	116.012620	57.112052
2632.128776	112.099988	57.117057
2631.595944	108.883262	57.122061
2631.015379	100.313146	57.127066
2630.213236	107.818589	57.132071
2629.089084	117.168371	57.137076
2628.474319	103.550431	57.142081
2627.684917	106.880663	57.147085
2627.479235	105.913998	57.152090
2627.516286	106.866439	57.157095
2626.121065	105.741157	57.162100
2625.836903	109.120017	57.167105
2624.874289	110.194006	57.172109
2624.151676	114.725813	57.177114
2623.831366	108.042596	57.182119
2622.345492	110.409551	57.187124
2621.509949	111.700626	57.192129
2620.658894	110.500085	57.197133
2620.948712	112.943614	57.202138
2620.720230	105.420909	57.207143
2619.682451	102.119984	57.212148
2619.408225	106.547113	57.217153
2617.763578	108.549249	57.222157
2616.950543	103.065363	57.227162
2616.626923	107.265680	57.232167
2615.726274	106.492422	57.237172
2615.485220	100.966415	57.242177
2615.030726	104.569386	57.247181
2614.904112	111.380290	57.252186
2613.775188	101.932498	57.257191
2612.589040	104.125063	57.262196
2612.282102	103.695956	57.267201
2611.977782	101.900259	57.272205
2611.198540	110.087821	57.277210
2610.437070	96.388000	57.282215
2608.912250	104.298816	57.287220
2609.072693	103.363903	57.292225
2608.388204	110.829500	57.297229
2607.721528	118.445603	57.302234
2607.585144	108.869582	57.307239
2606.164874	116.503987	57.312244
2605.252444	118.542793	57.317249
2604.608425	105.658521	57.322253
2604.119159	108.853371	57.327258
2603.921859	103.836185	57.332263
2603.548805	106.925119	57.337268
2602.806654	107.546172	57.342273
2601.937279	99.131615	57.347277
2600.520052	101.730779	57.352282
2600.382213	102.815351	57.357287
2599.457267	96.889563	57.362292
2599.461706	100.289741	57.367297
2598.111018	100.560890	57.372301
2597.009781	107.478405	57.377306
2596.942978	94.037194	57.382311
2595.953363	104.555647	57.387316
2595.985381	101.914188	57.392321
2595.671529	92.665745	57.397325
2594.747117	104.648137	57.402330
2593.729450	105.205374	57.407335
2593.143028	106.333869	57.412340
2592.319981	102.367839	57.417345
2592.206505	103.103256	57.422349
2590.752868	111.098223	57.427354
2590.183769	100.289248	57.432359
2589.094334	110.840164	57.437364
2588.609717	105.262641	57.442369
2588.483415	98.628764	57.447373
2587.977719	100.133052	57.452378
2587.778047	94.348931	57.457383
2586.549751	105.890264	57.462388
2585.728855	103.257643	57.467393
2584.914884	103.458357	57.472397
2584.072775	112.992814	57.477402
2583.915742	101.261579	57.482407
2583.992727	110.419445	57.487412
2582.914599	104.864045	57.492417
2582.131712	102.828066	57.497421
2580.991294	101.986859	57.502426
2580.579076	101.445493	57.507431
2579.979940	105.651070	57.512436
2579.082123	105.394423	57.517441
2578.485769	106.528565	57.522445
2577.724093	111.534407	57.527450
2577.566155	95.983183	57.532455
2576.468965	108.966929	57.537460
2576.056968	106.156646	57.542465
2575.154440	105.429109	57.547469
2574.364560	111.273826	57.552474
2573.574086	110.875280	57.557479
2572.981955	103.525667	57.562484
2572.749108	106.602474	57.567489
2572.513639	103.741883	57.572493
2571.622818	109.672144	57.577498
2570.909180	99.444051	57.582503
2570.006613	105.798279	57.587508
2569.122303	103.504913	57.592513
2568.854183	102.848521	57.597517
2567.844205	105.445570	57.602522
2566.915296	104.135193	57.607527
2566.204502	110.580978	57.612532
2565.849696	102.538709	57.617537
2565.623423	111.100674	57.622541
2564.622317	116.364549	57.627546
2564.855330	106.302634	57.632551
2563.116639	127.870415	57.637556
2562.545262	113.003655	57.642561
2561.992698	102.935914	57.647565
2561.418560	111.751948	57.652570
2561.083583	107.630249	57.657575
2559.935552	109.090804	57.662580
2559.163504	105.393157	57.667585
2558.619768	114.453856	57.672589
2557.638501	114.404105	57.677594
2557.361454	102.606156	57.682599
2556.787735	117.142868	57.687604
2556.192928	109.863974	57.692609
2555.844011	105.760843	57.697613
2554.619925	114.802462	57.702618
2554.491463	104.978393	57.707623
2553.629155	107.791770	57.712628
2553.591223	109.274514	57.717633
2552.208618	106.409121	57.722637
2551.107173	107.375017	57.727642
2551.205716	102.853558	57.732647
2550.277944	110.176017	57.737652
2549.649872	109.471035	57.742657
2548.296061	114.026680	57.747661
2547.827801	112.411377	57.752666
2547.192105	105.400785	57.757671
2546.723975	116.262715	57.762676
2546.485821	113.783887	57.767681
2546.045787	101.570924	57.772685
2545.179637	114.161504	57.777690
2544.222298	109.310967	57.782695
2543.427120	105.342154	57.787700
2542.735426	107.668484	57.792705
2542.509632	99.789290	57.797709
2541.342648	110.154131	57.802714
2540.518939	98.917000	57.807719
2539.726140	113.621421	57.812724
2539.352660	104.872237	57.817729
2538.715781	101.808704	57.822733
2538.317626	109.009436	57.827738
2538.092373	104.216107	57.832743
2537.639453	109.769543	57.837748
2536.338358	101.338416	57.842753
2535.715978	107.021082	57.847757
2535.180385	107.416968	57.852762
2534.969206	98.035718	57.857767
2533.528745	102.957087	57.862772
2532.790924	105.545901	57.867777
2532.303217	111.037787	57.872781
2531.788399	110.343838	57.877786
2531.341981	100.222039	57.882791
2529.843626	104.057156	57.887796
2529.109812	106.282139	57.892801
2528.691167	100.378357	57.897805
2528.204690	115.878279	57.902810
2527.564640	99.160575	57.907815
2527.262043	100.478966	57.912820
2526.998542	101.683309	57.917825
2525.864903	94.798906	57.922829
2524.599087	106.448104	57.927834
2524.447075	96.768197	57.932839
2523.808405	110.298011	57.937844
2523.651228	106.658667	57.942849
2522.442675	99.131433	57.947853
2521.656958	103.378779	57.952858
2521.171909	95.465363	57.957863
2520.621378	102.313997	57.962868
2519.816966	104.689599	57.967873
2519.123447	104.387377	57.972877
2518.142684	109.399101	57.977882
2517.684909	109.711818	57.982887
2516.755503	104.322451	57.987892
2516.248712	103.059913	57.992897
2516.122643	101.669129	57.997901
2515.553177	105.395573	58.002906
2514.762934	97.378418	58.007911
2513.728482	107.277327	58.012916
2512.842545	111.087877	58.017921
2512.772191	102.913303	58.022925
2511.913742	106.657970	58.027930
2511.089913	104.239409	58.032935
2509.891283	109.083520	58.037940
2509.413312	110.791885	58.042945
2509.223822	103.995927	58.047949
2508.687460	107.292383	58.052954
2508.328902	93.729361	58.057959
2507.837688	99.268815	58.062964
2506.903696	101.224875	58.067969
2506.075568	102.429437	58.072973
2505.241893	108.308883	58.077978
2504.754033	107.315864	58.082983
2503.683509	104.879088	58.087988
2502.586695	101.034088	58.092993
2502.483875	104.381156	58.097997
2501.672524	113.162355	58.103002
2501.494348	106.936813	58.108007
2500.966464	111.386390	58.113012
2500.133052	110.242851	58.118017
2499.334452	107.187629	58.123021
2498.085119	108.253423	58.128026
2498.321168	99.968442	58.133031
2497.918848	106.457803	58.138036
2496.848658	103.572170	58.143041
2495.949018	99.842667	58.148045
2494.785773	106.427386	58.153050
2494.646406	98.574474	58.158055
2494.056253	111.331017	58.163060
2493.440078	96.612077	58.168065
2493.305072	104.398981	58.173069
2491.746144	108.221176	58.178074
2491.198602	102.873103	58.183079
2490.600116	109.920197	58.188084
2490.398909	105.805635	58.193089
2489.764397	100.050472	58.198093
2488.555516	111.043779	58.203098
2488.301460	113.931983	58.208103
2487.256387	102.462324	58.213108
2487.140128	106.858893	58.218113
2486.567078	102.181083	58.223117
2485.163756	108.862111	58.228122
2484.544373	107.978025	58.233127
2484.033828	107.985961	58.238132
2483.333849	103.863125	58.243137
2483.326984	102.624457	58.248141
2481.738161	113.866667	58.253146
2481.165107	103.860470	58.258151
2480.060892	103.792675	58.263156
2479.539508	100.591776	58.268161
2479.625323	93.380874	58.273165
2478.658525	102.868359	58.278170
2478.193725	96.429731	58.283175
2478.032010	102.969135	58.288180
2477.363389	95.372103	58.293185
2476.388826	96.020672	58.298189
2475.624228	103.463257	58.303194
2474.948936	89.910979	58.308199
2474.186372	99.153157	58.313204
2473.499850	103.273420	58.318209
2472.590650	98.281255	58.323213
2471.911521	106.309210	58.328218
2471.829493	102.694915	58.333223
2471.107064	107.325382	58.338228
2470.741322	101.670318	58.343233
2470.128672	98.286874	58.348237
2468.894184	103.125278	58.353242
2468.380671	92.593007	58.358247
2467.616728	93.894360	58.363252
2466.237388	93.999129	58.368257
2466.244597	101.314493	58.373261
2465.164898	105.957887	58.378266
2464.743343	94.447554	58.383271
2464.403678	108.077422	58.388276
2463.857676	113.177447	58.393281
2463.852935	104.013927	58.398285
2462.634413	107.616091	58.403290
2461.666552	104.230222	58.408295
2461.141583	102.640808	58.413300
2459.999319	109.090107	58.418305
2459.712688	105.699472	58.423309
2458.937144	107.745288	58.428314
2458.469773	98.291802	58.433319
2457.722946	100.835585	58.438324
2457.562806	108.423898	58.443329
2456.533852	103.959431	58.448333
2455.334520	99.987897	58.453338
2454.981886	101.632599	58.458343
2454.486977	100.634870	58.463348
2453.796155	99.361963	58.468353
2453.203582	91.131824	58.473357
2451.980065	100.293741	58.478362
2451.720391	101.699531	58.483367
2451.013417	98.449844	58.488372
2450.239567	101.066141	58.493377
2450.194688	95.245699	58.498381
2449.527638	103.274746	58.503386
2448.334448	102.239307	58.508391
2447.733538	95.139109	58.513396
2447.161556	109.639197	58.518401
2446.856093	99.418711	58.523405
2445.693305	102.185584	58.528410
2444.454019	100.731331	58.533415
2444.257746	103.338084	58.538420
2443.584499	106.338616	58.543425
2443.764459	96.893267	58.548429
2443.027387	107.471181	58.553434
2442.455258	97.213004	58.558439
2441.625627	101.763514	58.563444
2440.283774	101.848065	58.568449
2440.108655	96.599743	58.573453
2438.527947	99.981213	58.578458
2438.093210	102.038625	58.583463
2437.481695	98.229084	58.588468
2436.515361	98.729415	58.593473
2437.085206	97.101625	58.598477
2436.150299	99.826380	58.603482
2435.849072	95.228021	58.608487
2435.036972	100.532615	58.613492
2433.792051	100.739142	58.618497
2432.848828	88.328047	58.623501
2432.255784	92.923759	58.628506
2431.963312	96.984149	58.633511
2431.269080	93.047047	58.638516
2430.961326	97.699373	58.643521
2430.333188	89.403876	58.648525
2429.322831	94.809075	58.653530
2428.975077	95.299955	58.658535
2428.169686	91.619088	58.663540
2426.768391	98.145834	58.668545
2426.193284	96.693677	58.673549
2425.736531	100.495982	58.678554
2424.991924	89.966130	58.683559
2424.887617	96.275852	58.688564
2423.991851	103.907836	58.693569
2423.850655	86.568847	58.698573
2422.956088	101.805375	58.703578
2422.343144	97.801087	58.708583
2421.598752	96.540896	58.713588
2420.617077	101.900143	58.718593
2419.237934	94.261589	58.723597
2419.402080	100.302787	58.728602
2418.561188	94.469246	58.733607
2418.133473	97.806338	58.738612
2417.404692	99.539829	58.743617
2417.483886	93.392660	58.748621
2416.158338	102.954516	58.753626
2415.359774	100.374553	58.758631
2414.749428	100.099964	58.763636
2414.363204	102.104479	58.768641
2413.814627	92.328979	58.773645
2412.501338	109.650201	58.778650
2411.515001	97.632123	58.783655
2411.007040	91.745606	58.788660
2410.562489	105.357875	58.793665
2410.252101	98.305900	58.798669
2409.893018	107.899083	58.803674
2409.212556	102.210210	58.808679
2408.590219	96.271014	58.813684
2407.431934	100.844565	58.818689
2407.253053	102.315881	58.823693
2406.308574	95.740210	58.828698
2405.182107	97.574857	58.833703
2404.817177	101.107261	58.838708
2403.820370	104.851125	58.843713
2403.395905	97.144862	58.848717
2403.277780	103.144722	58.853722
2402.796309	102.116675	58.858727
2401.944267	92.673714	58.863732
2400.706483	95.214215	58.868737
2400.739576	95.442616	58.873741
2399.569904	102.733027	58.878746
2398.939676	96.948334	58.883751
2398.459435	98.617226	58.888756
2397.645403	106.925216	58.893761
2397.319663	98.332891	58.898765
2395.812397	104.911711	58.903770
2394.973260	99.823901	58.908775
2394.477911	95.020326	58.913780
2393.957342	106.844073	58.918785
2393.708890	84.711350	58.923789
2393.835374	93.407973	58.928794
2393.091000	98.781908	58.933799
2391.926752	92.405262	58.938804
2390.830436	93.805297	58.943809
2390.651069	95.061966	58.948813
2389.817686	100.278627	58.953818
2388.889447	98.280560	58.958823
2388.348142	92.043312	58.963828
2387.524434	91.380486	58.968833
2387.408254	92.175971	58.973837
2386.200391	94.805698	58.978842
2385.172696	103.297058	58.983847
2384.684042	96.665950	58.988852
2383.595548	107.375399	58.993857
2383.510705	98.185324	58.998861
2383.176360	96.987259	59.003866
2382.686575	93.212569	59.008871
2382.131696	90.365558	59.013876
2381.426482	102.853222	59.018881
2380.598968	91.935332	59.023885
2379.514920	91.399125	59.028890
2378.913134	92.932490	59.033895
2378.755863	91.727042	59.038900
2378.191988	97.983111	59.043905
2376.908466	99.294373	59.048909
2376.100796	95.666403	59.053914
2375.782424	96.416333	59.058919
2375.212970	106.755593	59.063924
2374.692172	105.534543	59.068929
2374.362907	94.878419	59.073933
2373.274495	99.221351	59.078938
2371.977102	92.226050	59.083943
2372.218838	89.540450	59.088948
2371.512426	92.375347	59.093953
2370.293367	93.456911	59.098957
2369.813547	99.789394	59.103962
2368.945216	97.398205	59.108967
2368.526669	93.016093	59.113972
2367.592535	97.021602	59.118977
2367.522090	88.584969	59.123981
2366.659769	91.223902	59.128986
2365.687138	91.903341	59.133991
2365.255292	91.128120	59.138996
2364.495488	95.056059	59.144001
2364.088066	92.818553	59.149005
2363.319892	94.505893	59.154010
2362.045307	93.462287	59.159015
2361.500063	95.904902	59.164020
2360.936211	98.957786	59.169025
2360.661309	98.143492	59.174029
2360.488681	99.944123	59.179034
2360.060466	93.035459	59.184039
2359.154135	86.134738	59.189044
2358.168373	96.707014	59.194049
2357.879465	91.318690	59.199053
2356.169894	97.375547	59.204058
2355.453147	96.324185	59.209063
2354.593156	92.917133	59.214068
2353.998780	93.728863	59.219073
2354.203875	91.350701	59.224077
2353.648972	94.669676	59.229082
2352.966506	89.399963	59.234087
2352.826787	86.946162	59.239092
2351.870460	93.050660	59.244097
2350.801780	88.785245	59.249101
2350.399281	95.684750	59.254106
2349.091040	96.923669	59.259111
2348.536957	93.990476	59.264116
2347.951575	91.749850	59.269121
2347.518152	87.095952	59.274125
2346.833273	96.062753	59.279130
2346.360120	93.680571	59.284135
2345.304446	93.933703	59.289140
2344.183958	94.066475	59.294145
2344.355628	97.694223	59.299149
2343.911957	95.598306	59.304154
2343.057289	87.937990	59.309159
2341.905812	97.885337	59.314164
2341.073411	98.850266	59.319169
2340.974345	90.958117	59.324173
2340.197026	91.388644	59.329178
2339.847338	91.322115	59.334183
2339.001585	87.380151	59.339188
2337.893038	93.005039	59.344193
2337.748013	101.041926	59.349197
2336.744749	93.026900	59.354202
2336.274442	97.727943	59.359207
2335.610459	86.291464	59.364212
2334.347612	96.787179	59.369217
2333.835628	90.816892	59.374221
2333.470064	87.564503	59.379226
2333.018560	95.103944	59.384231
2332.665289	84.909030	59.389236
2331.680156	100.250645	59.394241
2331.301482	96.586430	59.399245
2330.114134	99.171214	59.404250
2330.019250	98.093253	59.409255
2329.368520	92.244188	59.414260
2328.045754	103.539206	59.419265
2327.382310	97.493768	59.424269
2326.964066	100.577411	59.429274
2326.039170	100.628584	59.434279
2325.636230	91.724617	59.439284
2324.141709	98.501394	59.444289
2323.594483	87.074952	59.449293
2323.355790	93.621587	59.454298
2323.543739	95.756073	59.459303
2322.586650	87.822759	59.464308
2321.630873	95.755526	59.469313
2321.428299	88.141202	59.474317
2320.539792	95.074473	59.479322
2319.594415	102.190755	59.484327
2319.153636	91.745154	59.489332
2318.642947	97.666088	59.494337
2317.625652	99.219987	59.499341
2317.058504	99.348535	59.504346
2316.044312	97.836480	59.509351
2315.999151	94.764557	59.514356
2315.064729	96.186262	59.519361
2314.336780	94.495396	59.524365
2313.287035	97.876099	59.529370
2312.584591	103.787590	59.534375
2312.252648	91.189108	59.539380
2311.572299	96.076854	59.544385
2311.729638	89.899750	59.549389
2310.988942	98.616765	59.554394
2310.011045	90.832269	59.559399
2309.401823	86.928019	59.564404
2308.022305	83.508770	59.569409
2308.131104	81.272598	59.574413
2307.365007	84.370724	59.579418
2306.068671	95.596090	59.584423
2305.436222	82.127720	59.589428
2304.790395	92.663182	59.594433
2304.656810	83.890393	59.599437
2304.194177	92.169869	59.604442
2303.197128	89.120991	59.609447
2302.791134	80.538861	59.614452
2301.737490	90.733942	59.619457
2301.431515	83.594790	59.624461
2300.490215	87.271147	59.629466
2299.489221	88.932389	59.634471
2299.075964	88.283859	59.639476
2297.948566	88.588342	59.644481
2297.832717	83.611339	59.649485
2297.539063	94.637613	59.654490
2297.094593	94.242702	59.659495
2295.902708	88.287244	59.664500
2294.811592	84.747629	59.669505
2294.717983	89.390175	59.674509
2294.048541	97.962773	59.679514
2293.725713	102.425844	59.684519
2292.569689	91.319821	59.689524
2291.733099	95.874692	59.694529
2291.197579	88.916103	59.699533
2290.952885	88.069018	59.704538
2289.824755	92.475987	59.709543
2289.555423	90.028565	59.714548
2288.927501	96.389138	59.719553
2288.297082	91.124350	59.724557
2287.064373	92.115506	59.729562
2286.353091	94.856117	59.734567
2285.551266	82.951794	59.739572
2285.045754	97.061166	59.744577
2284.744420	90.068056	59.749581
2284.130088	91.757517	59.754586
2283.294198	94.496937	59.759591
2283.371377	84.023956	59.764596
2282.146394	93.795988	59.769601
2281.557842	82.230183	59.774605
2280.936356	86.176710	59.779610
2279.674481	97.528420	59.784615
2279.102346	91.757500	59.789620
2278.044754	93.370794	59.794625
2277.600442	84.533124	59.799629
2277.588531	87.221239	59.804634
2276.774342	86.158921	59.809639
2276.551701	86.800909	59.814644
2275.950355	95.781057	59.819649
2274.981646	94.786215	59.824653
2274.374862	95.630863	59.829658
2273.633317	101.311419	59.834663
2272.760228	95.437627	59.839668
2271.873808	97.442427	59.844673
2271.118807	98.706750	59.849677
2270.547884	91.301075	59.854682
2270.589540	100.255737	59.859687
2269.820391	90.362468	59.864692
2268.619879	89.303061	59.869697
2267.662773	84.569788	59.874701
2267.645001	91.598886	59.879706
2266.543467	89.005632	59.884711
2266.488003	84.856697	59.889716
2265.698123	82.231068	59.894721
2264.674962	87.259936	59.899725
2264.170500	86.074788	59.904730
2263.203483	89.093598	59.909735
2263.462347	84.740915	59.914740
2262.706462	96.965274	59.919745
2261.591358	92.673479	59.924750
2261.164254	90.746838	59.929754
2259.977127	90.006843	59.934759
2259.825855	85.699035	59.939764
2258.131468	88.563954	59.944769
2257.460965	93.665143	59.949774
2257.807168	90.696027	59.954778
2257.148719	87.914901	59.959783
2256.543173	78.536804	59.964788
2256.179169	85.066180	59.969793
2255.332069	89.080896	59.974798
2254.392868	84.163386	59.979802
2253.716432	93.732276	59.984807
2253.213569	87.167569	59.989812
2251.783142	94.839287	59.994817
2251.643638	88.604401	59.999822
2251.381329	83.952438	60.004826
2250.387502	88.035666	60.009831
2249.965414	91.522585	60.014836
2248.827452	93.433040	60.019841
2247.651258	90.110084	60.024846
2247.307683	83.875758	60.029850
2246.580882	86.594552	60.034855
2246.419598	79.794994	60.039860
2246.260306	93.899229	60.044865
2245.565784	93.855363	60.049870
2244.571310	90.370283	60.054874
2243.456060	92.299354	60.059879
2243.192316	87.000289	60.064884
2242.636768	90.727525	60.069889
2241.765744	81.373514	60.074894
2240.933535	83.357993	60.079898
2240.361682	89.338332	60.084903
2239.845375	85.113082	60.089908
2239.508626	88.425544	60.094913
2238.317012	91.443296	60.099918
2237.773605	78.418782	60.104922
2236.986220	86.790106	60.109927
2236.574032	80.509887	60.114932
2235.864818	84.617862	60.119937
2235.265906	84.670142	60.124942
2234.817562	89.715971	60.129946
2233.725307	92.162146	60.134951
2233.407946	90.360419	60.139956
2232.316194	96.679532	60.144961
2231.299653	93.245199	60.149966
2230.911056	83.917631	60.154970
2230.281157	92.995816	60.159975
2230.035754	85.071077	60.164980
2229.448059	87.129790	60.169985
2229.159960	89.083586	60.174990
2227.686649	86.110647	60.179994
2226.824731	86.010151	60.184999
2227.050446	85.185250	60.190004
2226.026596	87.193821	60.195009
2225.123713	82.928899	60.200014
2224.454798	91.798632	60.205018
2223.380108	91.154676	60.210023
2223.179647	79.608961	60.215028
2222.709131	87.562161	60.220033
2222.003740	84.656837	60.225038
2222.018405	83.570013	60.230042
2220.265975	90.160002	60.235047
2220.186307	86.299803	60.240052
2219.498741	85.996208	60.245057
2218.694581	89.169140	60.250062
2217.969333	81.427516	60.255066
2216.707112	89.958598	60.260071
2216.304334	82.379318	60.265076
2216.093962	83.916019	60.270081
2215.369617	87.552127	60.275086
2215.329033	83.907869	60.280090
2214.039797	98.776116	60.285095
2213.508452	87.770915	60.290100
2212.869503	90.540212	60.295105
2212.052812	84.363909	60.300110
2211.301185	85.901600	60.305114
2210.603252	90.815252	60.310119
2209.807324	86.112056	60.315124
2209.316998	89.590516	60.320129
2208.828669	88.099468	60.325134
2208.845300	82.004854	60.330138
2207.377342	82.752453	60.335143
2206.279753	75.763699	60.340148
2205.999520	83.526861	60.345153
2205.659168	83.551109	60.350158
2204.475465	78.390438	60.355162
2203.713128	76.094836	60.360167
2203.380247	71.454161	60.365172
2202.896535	84.962178	60.370177
2202.257392	78.431842	60.375182
2201.945476	84.025107	60.380186
2200.662575	93.970864	60.385191
2200.187864	84.528164	60.390196
2199.591263	93.084357	60.395201
2198.672439	88.924005	60.400206
2198.499736	87.409372	60.405210
2197.542685	92.208662	60.410215
2196.646015	83.275086	60.415220
2195.910609	85.297092	60.420225
2195.465200	93.817956	60.425230
2195.242222	90.169365	60.430234
2194.503354	92.095258	60.435239
2193.591623	86.790181	60.440244
2192.678784	94.357207	60.445249
2191.715608	92.755140	60.450254
2191.647726	82.162904	60.455258
2190.828934	88.954792	60.460263
2189.964844	83.643543	60.465268
2189.206163	93.246236	60.470273
2188.942314	84.247853	60.475278
2188.468561	82.395907	60.480282
2187.455449	94.145985	60.485287
2187.443579	84.215198	60.490292
2186.173100	84.323130	60.495297
2185.276626	84.577880	60.500302
2185.273008	81.924371	60.505306
2184.710293	88.740356	60.510311
2183.624238	84.092311	60.515316
2183.420857	88.223909	60.520321
2182.624132	87.494529	60.525326
2181.974526	85.735025	60.530330
2180.572199	92.981175	60.535335
2180.259937	89.666002	60.540340
2179.818302	87.578834	60.545345
2179.243855	97.846312	60.550350
2178.425814	91.502882	60.555354
2177.123541	93.265800	60.560359
2176.585067	86.733643	60.565364
2176.151013	92.060835	60.570369
2175.648812	89.749561	60.575374
2175.668602	84.539771	60.580378
2174.375441	91.411606	60.585383
2173.349084	87.026896	60.590388
2172.792229	87.530264	60.595393
2172.312449	97.790235	60.600398
2172.051549	91.168763	60.605402
2171.172593	98.460402	60.610407
2170.467176	91.914166	60.615412
2169.655254	85.273257	60.620417
2168.793797	91.601145	60.625422
2168.696965	90.436683	60.630426
2167.601764	88.518529	60.635431
2167.204651	85.240764	60.640436
2166.412574	90.785104	60.645441
2165.387232	96.925110	60.650446
2165.191633	92.051356	60.655450
2164.475133	101.357508	60.660455
2164.142087	87.831254	60.665460
2163.548882	91.251130	60.670465
2162.196535	96.004746	60.675470
2161.927564	95.637461	60.680474
2160.821861	90.561348	60.685479
2160.560091	85.850487	60.690484
2160.486610	90.649054	60.695489
2158.943453	88.938958	60.700494
2158.536060	89.269139	60.705498
2157.723653	95.438646	60.710503
2157.342892	86.626836	60.715508
2157.093981	92.915881	60.720513
2155.827696	88.597866	60.725518
2154.906571	83.867149	60.730522
2154.364250	90.232032	60.735527
2154.017830	83.380465	60.740532
2153.560687	80.484403	60.745537
2152.387822	85.736645	60.750542
2151.980105	84.392074	60.755546
2151.178787	92.361987	60.760551
2150.858355	84.641532	60.765556
2149.910989	87.124517	60.770561
2149.021369	86.737071	60.775566
2148.519125	81.276317	60.780570
2147.606334	87.963104	60.785575
2147.252625	89.094075	60.790580
2147.091992	84.275921	60.795585
2146.146143	92.673961	60.800590
2145.122757	78.995008	60.805594
2144.368455	92.119060	60.810599
2144.338156	84.587791	60.815604
2144.024486	88.197877	60.820609
2142.555889	85.727824	60.825614
2141.925043	88.575476	60.830618
2141.089497	96.275729	60.835623
2140.679509	88.520066	60.840628
2140.232460	87.967326	60.845633
2139.033511	100.933364	60.850638
2138.325631	86.062854	60.855642
2137.594754	97.367575	60.860647
2137.219381	90.667006	60.865652
2136.815155	85.216330	60.870657
2136.428887	84.651221	60.875662
2136.461779	80.818749	60.880666
2134.717796	90.712720	60.885671
2134.373206	80.008351	60.890676
2133.750306	86.336490	60.895681
2132.740067	88.011972	60.900686
2131.953412	85.962504	60.905690
2131.361906	89.229334	60.910695
2130.943032	88.648487	60.915700
2130.194293	81.515615	60.920705
2128.980960	91.895913	60.925710
2128.331087	87.010258	60.930714
2127.765690	94.657992	60.935719
2127.011670	85.901343	60.940724
2126.937482	81.659701	60.945729
2126.239313	89.829070	60.950734
2126.337733	76.177329	60.955738
2125.177870	91.563823	60.960743
2124.777787	90.246762	60.965748
2123.982151	88.402509	60.970753
2122.359366	78.292142	60.975758
2121.824982	76.821217	60.980762
2121.534298	83.262660	60.985767
2120.856361	87.387795	60.990772
2120.489098	89.843801	60.995777
2119.862978	79.806906	61.000782
2118.609255	75.147297	61.005786
2118.098472	88.582971	61.010791
2117.905873	84.423553	61.015796
2117.177611	81.756229	61.020801
2116.521203	81.403109	61.025806
2115.553123	67.801161	61.030810
2114.453685	82.977978	61.035815
2113.988357	77.395263	61.040820
2113.752138	80.826317	61.045825
2113.122086	86.019274	61.050830
2112.332278	76.392078	61.055834
2111.380642	83.852061	61.060839
2110.678786	77.759164	61.065844
2110.953524	80.566003	61.070849
2110.297203	80.924948	61.075854
2109.533043	74.915732	61.080858
2108.179799	81.529439	61.085863
2107.151287	77.713516	61.090868
2106.626905	86.598001	61.095873
2106.252678	88.708631	61.100878
2105.402596	72.806189	61.105882
2104.845840	78.241204	61.110887
2104.217869	73.600487	61.115892
2104.278238	82.174961	61.120897
2103.118408	78.104404	61.125902
2102.395626	66.409645	61.130906
2101.625534	76.242825	61.135911
2100.811699	78.297992	61.140916
2100.590483	75.390005	61.145921
2099.896129	82.219032	61.150926
2099.590640	75.165482	61.155930
2098.270129	79.774719	61.160935
2097.744183	84.664487	61.165940
2097.600456	73.743018	61.170945
2096.746512	80.685784	61.175950
2095.508170	68.268052	61.180954
2094.686906	77.729870	61.185959
2094.457091	76.518291	61.190964
2094.166307	81.390729	61.195969
2093.420331	85.362904	61.200974
2092.238656	78.111073	61.205978
2091.682816	79.138071	61.210983
2091.033627	77.704944	61.215988
2090.818154	68.058467	61.220993
2089.988360	78.644333	61.225998
2089.195967	66.355979	61.231002
2088.717473	77.169904	61.236007
2087.870359	80.305988	61.241012
2087.475566	74.903443	61.246017
2086.016061	87.031837	61.251022
2085.537414	83.180681	61.256026
2084.637825	84.986844	61.261031
2084.345777	84.829949	61.266036
2084.013723	80.470581	61.271041
2083.602594	77.469162	61.276046
2083.082343	74.521143	61.281050
2081.696685	77.222388	61.286055
2080.857344	80.863572	61.291060
2080.414061	77.653713	61.296065
2080.074975	84.689597	61.301070
2079.634276	79.268457	61.306074
2078.704501	77.836747	61.311079
2077.697917	78.631382	61.316084
2077.289204	80.254114	61.321089
2076.623236	93.056753	61.326094
2076.236770	76.045582	61.331098
2075.598891	79.512181	61.336103
2074.711722	82.744325	61.341108
2074.231337	76.709472	61.346113
2073.549580	80.963152	61.351118
2072.703121	78.835113	61.356122
2071.756812	83.305749	61.361127
2071.586533	86.233701	61.366132
2070.826199	78.473640	61.371137
2070.336324	83.025277	61.376142
2069.094383	87.178995	61.381146
2068.229480	87.751247	61.386151
2067.894552	92.812812	61.391156
2067.549016	93.693319	61.396161
2067.208264	87.003813	61.401166
2066.438970	80.774833	61.406170
2065.444735	87.991855	61.411175
2064.528823	91.422727	61.416180
2064.523720	79.276408	61.421185
2063.285831	83.101813	61.426190
2062.330031	85.819928	61.431194
2061.634675	89.194129	61.436199
2061.374791	92.934354	61.441204
2060.879328	79.984967	61.446209
2060.409206	86.160272	61.451214
2059.894489	81.161122	61.456218
2058.848952	88.065616	61.461223
2058.029754	94.636541	61.466228
2057.614477	81.478841	61.471233
2056.812780	83.899424	61.476238
2056.053402	84.826246	61.481242
2054.937306	89.550129	61.486247
2054.477775	83.427239	61.491252
2054.193706	85.590342	61.496257
2053.518146	95.711698	61.501262
2053.567387	80.291335	61.506266
2051.921852	85.072226	61.511271
2050.900521	91.335106	61.516276
2050.670713	78.772504	61.521281
2050.006000	89.164753	61.526286
2049.911169	87.086566	61.531290
2049.460147	80.241459	61.536295
2048.403656	81.553038	61.541300
2047.656426	79.353953	61.546305
2046.664542	90.284910	61.551310
2046.703851	83.108046	61.556314
2045.575306	85.230078	61.561319
2044.795853	78.731272	61.566324
2044.570188	79.019324	61.571329
2043.773557	89.804782	61.576334
2043.601102	85.375487	61.581338
2041.856738	90.171707	61.586343
2040.948063	86.212541	61.591348
2040.598266	77.990305	61.596353
2039.807611	85.416839	61.601358
2039.845574	83.841313	61.606362
2039.754106	88.824918	61.611367
2038.419328	86.603181	61.616372
2037.827055	79.077659	61.621377
2037.318195	91.949736	61.626382
2036.848547	82.751720	61.631386
2035.347323	87.398988	61.636391
2034.300600	90.391204	61.641396
2033.930217	82.438136	61.646401
2033.617777	93.450237	61.651406
2033.525888	88.709145	61.656410
2033.046041	95.627011	61.661415
2031.815854	99.029939	61.666420
2031.593655	88.663056	61.671425
2030.059912	88.535015	61.676430
2028.902738	80.158789	61.681434
2028.976591	87.055752	61.686439
2027.913110	85.200491	61.691444
2027.642554	77.558759	61.696449
2027.123653	89.404300	61.701454
2026.915155	85.096825	61.706458
2026.246072	90.492643	61.711463
2025.006619	83.215583	61.716468
2024.403268	81.849226	61.721473
2023.963971	85.356465	61.726478
2023.538778	77.133708	61.731482
2022.530812	78.443306	61.736487
2021.516406	87.817386	61.741492
2020.775235	78.704503	61.746497
2020.528711	87.961838	61.751502
2020.134642	86.860461	61.756506
2019.653924	85.025513	61.761511
2018.849362	85.064839	61.766516
2018.065984	81.684618	61.771521
2017.156200	85.816263	61.776526
2015.960166	92.784006	61.781530
2015.554454	88.278564	61.786535
2014.545218	84.206347	61.791540
2014.616932	89.880827	61.796545
2014.016916	94.040010	61.801550
2013.531119	80.811097	61.806554
2012.926181	91.623764	61.811559
2011.845826	89.311147	61.816564
2011.106266	91.097842	61.821569
2010.673635	92.570334	61.826574
2010.324323	88.236028	61.831578
2009.234477	84.128656	61.836583
2008.120506	85.240082	61.841588
2007.544056	79.803096	61.846593
2007.355699	84.617358	61.851598
2007.018951	80.288010	61.856602
2006.478940	86.298436	61.861607
2005.211952	85.709918	61.866612
2004.400735	78.836437	61.871617
2003.962394	88.498411	61.876622
2003.466614	86.464338	61.881626
2003.011993	87.914146	61.886631
2001.733369	92.923988	61.891636
2000.998805	80.074725	61.896641
2000.550164	90.695267	61.901646
2000.085602	83.892745	61.906650
1999.622416	86.751201	61.911655
1998.806805	90.055982	61.916660
1997.995607	88.379406	61.921665
1997.552113	93.154422	61.926670
1996.823713	86.217038	61.931674
1996.416032	86.863847	61.936679
1995.143200	89.400555	61.941684
1994.306196	81.416397	61.946689
1993.440659	80.632900	61.951694
1993.316544	87.658063	61.956698
1992.843234	83.530490	61.961703
1992.266696	77.326184	61.966708
1992.039971	80.044720	61.971713
1990.746633	89.562435	61.976718
1990.203303	90.388364	61.981722
1989.701234	83.524367	61.986727
1988.401482	92.743193	61.991732
1987.709720	85.575341	61.996737
1987.302356	91.845700	62.001742
1986.752320	88.109395	62.006746
1986.616886	93.099336	62.011751
1986.016245	84.573449	62.016756
1985.130148	74.265679	62.021761
1983.750533	85.093232	62.026766
1983.407056	86.569421	62.031770
1983.245053	79.588442	62.036775
1981.760429	85.235475	62.041780
1981.119241	81.321746	62.046785
1980.510704	91.427688	62.051790
1980.190376	91.444578	62.056794
1979.895628	94.893543	62.061799
1979.264126	90.485542	62.066804
1978.156498	84.602997	62.071809
1977.180530	86.059887	62.076814
1976.563235	88.966022	62.081818
1976.398786	80.111717	62.086823
1975.807341	82.967642	62.091828
1975.450444	78.401359	62.096833
1974.368164	88.158487	62.101838
1974.085641	85.407042	62.106842
1973.403177	90.224516	62.111847
1971.993084	95.454610	62.116852
1971.718109	83.378149	62.121857
1970.757264	80.432490	62.126862
1970.483880	83.033488	62.131866
1969.786135	79.039835	62.136871
1968.318696	93.141636	62.141876
1967.924435	82.860251	62.146881
1967.202103	86.579719	62.151886
1966.898538	87.709226	62.156890
1966.271583	80.769891	62.161895
1965.950568	81.621736	62.166900
1965.660758	74.465263	62.171905
1964.397937	85.548356	62.176910
1963.889640	79.156334	62.181914
1963.238356	81.806978	62.186919
1962.627619	87.316761	62.191924
1961.380357	87.243938	62.196929
1960.814435	83.886921	62.201934
1960.251881	87.088813	62.206938
1960.204551	80.798323	62.211943
1958.862312	84.580812	62.216948
1958.933340	78.142976	62.221953
1957.719618	79.838296	62.226958
1956.931124	86.619491	62.231962
1956.914342	82.949859	62.236967
1955.569528	89.129145	62.241972
1954.670279	86.823058	62.246977
1953.977244	85.335874	62.251982
1953.446199	78.234088	62.256986
1953.618001	80.309342	62.261991
1952.871826	92.141263	62.266996
1951.969097	77.880838	62.272001
1951.086632	84.417987	62.277006
1950.274162	79.556234	62.282010
1950.389076	83.213000	62.287015
1949.065598	87.901721	62.292020
1948.069147	85.241225	62.297025
1947.497102	83.124683	62.302030
1946.919223	78.760806	62.307034
1946.975183	84.540207	62.312039
1946.169651	75.751763	62.317044
1945.178017	82.169829	62.322049
1944.015268	81.737172	62.327054
1943.685579	80.486636	62.332058
1943.438561	81.979483	62.337063
1942.741539	84.490722	62.342068
1942.005992	77.692729	62.347073
1940.842661	78.091850	62.352078
1940.183593	78.975081	62.357082
1939.679178	71.416395	62.362087
1939.199963	78.545717	62.367092
1939.215107	81.882063	62.372097
1938.149502	77.940688	62.377102
1937.626838	86.787775	62.382106
1937.418689	82.913258	62.387111
1935.731747	80.153792	62.392116
1934.977529	85.252743	62.397121
1934.398076	87.298230	62.402126
1933.868766	83.481813	62.407130
1933.645890	82.739169	62.412135
1932.652270	83.117154	62.417140
1931.920358	79.454604	62.422145
1930.583316	89.187427	62.427150
1930.173447	83.408941	62.432154
1930.283434	82.692245	62.437159
1929.791432	87.372143	62.442164
1929.303788	93.224016	62.447169
1928.045132	89.297509	62.452174
1927.550966	91.274725	62.457178
1927.442567	88.557441	62.462183
1925.818641	91.162516	62.467188
1924.874077	82.605877	62.472193
1924.095037	87.736312	62.477198
1923.670476	85.945449	62.482202
1923.677074	82.151429	62.487207
1923.144931	87.206470	62.492212
1922.361010	76.267839	62.497217
1921.530449	87.671316	62.502222
1920.723874	82.733168	62.507226
1920.290812	78.291628	62.512231
1919.642761	87.846981	62.517236
1918.713976	78.015064	62.522241
1918.073671	87.662245	62.527246
1917.298731	82.980387	62.532250
1917.320452	78.453545	62.537255
1915.836951	89.823074	62.542260
1915.034133	85.948453	62.547265
1914.486827	86.492053	62.552270
1913.786831	89.219717	62.557274
1913.770788	89.860320	62.562279
1913.014151	88.963472	62.567284
1912.855001	85.200570	62.572289
1911.610470	89.342919	62.577294
1911.346061	84.787660	62.582298
1910.891730	81.034206	62.587303
1909.431618	95.897365	62.592308
1908.560492	85.717700	62.597313
1908.185400	94.991502	62.602318
1907.375723	90.469921	62.607322
1907.130842	78.111233	62.612327
1905.960843	91.206140	62.617332
1905.402532	79.890243	62.622337
1904.908981	81.834592	62.627342
1903.970493	93.372981	62.632346
1903.882784	75.436042	62.637351
1903.053987	81.294961	62.642356
1902.212604	82.107942	62.647361
1901.404491	81.568837	62.652366
1901.040052	78.366037	62.657370
1900.959955	78.442094	62.662375
1899.648627	84.917622	62.667380
1898.794644	80.723745	62.672385
1898.097515	89.879748	62.677390
1897.784548	83.489844	62.682394
1897.364933	83.279392	62.687399
1896.052291	94.131032	62.692404
1895.222377	84.978886	62.697409
1894.834094	90.726132	62.702414
1894.422978	89.304010	62.707418
1894.158942	86.001536	62.712423
1893.093411	84.359410	62.717428
1892.357950	77.323396	62.722433
1891.753562	73.802452	62.727438
1891.222013	83.272347	62.732442
1890.877173	84.884558	62.737447
1889.362499	85.768519	62.742452
1888.671332	72.668720	62.747457
1888.256586	80.815263	62.752462
1887.923154	78.827638	62.757466
1887.447437	78.588497	62.762471
1886.084426	90.267009	62.767476
1885.571963	78.046073	62.772481
1884.550514	83.744145	62.777486
1883.958314	80.977006	62.782490
1884.451845	76.005517	62.787495
1883.620312	79.988401	62.792500
1882.495249	82.924967	62.797505
1881.905538	84.409341	62.802510
1881.111366	83.436818	62.807514
1880.886646	83.562090	62.812519
1879.422370	85.013329	62.817524
1878.623729	79.984627	62.822529
1878.600052	75.685809	62.827534
1878.225714	80.750562	62.832538
1877.973590	80.962229	62.837543
1876.393403	83.013145	62.842548
1875.423421	81.217709	62.847553
1874.849413	81.116959	62.852558
1874.295389	88.859851	62.857562
1874.388200	77.617692	62.862567
1873.377003	82.118006	62.867572
1872.097410	75.359028	62.872577
1871.686335	75.325927	62.877582
1870.846610	83.470970	62.882586
1870.838163	80.619357	62.887591
1870.387061	79.165002	62.892596
1868.882759	73.647580	62.897601
1868.432370	77.916560	62.902606
1867.708843	71.640718	62.907610
1867.384864	71.653898	62.912615
1867.001266	76.944435	62.917620
1866.159346	81.001332	62.922625
1865.218224	82.172422	62.927630
1864.388165	73.286753	62.932634
1863.983475	74.530666	62.937639
1863.448710	82.598668	62.942644
1862.952922	86.239126	62.947649
1861.624380	80.190338	62.952654
1861.099278	80.669358	62.957658
1860.762834	78.463970	62.962663
1860.077341	81.612298	62.967668
1859.788595	82.159429	62.972673
1858.599021	81.494943	62.977678
1857.830429	86.020462	62.982682
1857.587317	75.937445	62.987687
1856.818490	81.229945	62.992692
1855.817120	84.820723	62.997697
1855.140795	81.794439	63.002702
1854.417037	81.611553	63.007706
1854.340737	79.525072	63.012711
1854.003815	78.709579	63.017716
1852.738859	75.546776	63.022721
1851.932790	73.043593	63.027726
1851.662786	85.510069	63.032730
1851.303711	78.858861	63.037735
1850.219554	81.449763	63.042740
1849.675400	83.168310	63.047745
1849.012323	79.441500	63.052750
1847.685526	81.176714	63.057754
1846.747211	70.305179	63.062759
1845.923629	78.839022	63.067764
1846.321890	75.485609	63.072769
1845.824371	79.469376	63.077774
1845.209965	82.049776	63.082778
1844.617509	70.471726	63.087783
1843.197823	81.663770	63.092788
1842.173132	79.029051	63.097793
1841.867343	85.371631	63.102798
1841.025382	80.192459	63.107802
1841.239136	75.998674	63.112807
1840.518898	80.841170	63.117812
1839.862489	78.551190	63.122817
1839.064248	79.240356	63.127822
1838.357694	86.180035	63.132826
1838.243077	78.560200	63.137831
1837.036852	78.815110	63.142836
1835.830165	78.245527	63.147841
1835.677678	77.352693	63.152846
1834.975707	77.043718	63.157850
1833.906933	72.976997	63.162855
1833.001454	79.860710	63.167860
1832.414508	81.839991	63.172865
1832.045107	75.921577	63.177870
1831.716774	86.833752	63.182874
1831.370873	73.548981	63.187879
1830.706976	79.902303	63.192884
1829.849835	73.851426	63.197889
1829.082782	80.106350	63.202894
1828.338322	82.718477	63.207898
1827.797104	77.575877	63.212903
1826.558877	78.116122	63.217908
1825.543101	74.570839	63.222913
1825.247825	77.325184	63.227918
1824.887839	85.238158	63.232922
1824.704308	75.407047	63.237927
1824.125508	79.970751	63.242932
1823.890552	80.173168	63.247937
1822.763617	81.634992	63.252942
1821.796837	78.159482	63.257946
1820.629654	73.547912	63.262951
1820.048331	80.012234	63.267956
1819.070398	85.689450	63.272961
1818.567901	77.259700	63.277966
1817.986429	76.840115	63.282970
1817.720745	75.795340	63.287975
1817.415793	78.179514	63.292980
1817.172898	87.428321	63.297985
1815.974535	78.647121	63.302990
1815.313271	78.747616	63.307994
1814.629089	68.915330	63.312999
1813.379563	78.011110	63.318004
1812.667424	73.332345	63.323009
1812.365189	80.996630	63.328014
1811.611254	87.345625	63.333018
1811.273534	68.560999	63.338023
1810.921610	76.960463	63.343028
1809.665569	75.618573	63.348033
1809.228909	75.805372	63.353038
1808.297519	75.770512	63.358042
1808.134344	83.744545	63.363047
1807.649778	86.783110	63.368052
1806.410344	80.172011	63.373057
1806.099639	74.270400	63.378062
1805.312863	78.841663	63.383066
1804.795350	81.651401	63.388071
1803.828663	83.758021	63.393076
1803.125722	77.657477	63.398081
1802.367572	79.566977	63.403086
1802.107031	78.286859	63.408090
1801.029136	72.629797	63.413095
1800.075148	77.409662	63.418100
1799.690585	79.634570	63.423105
1799.261534	72.130117	63.428110
1798.430903	82.881923	63.433114
1798.203275	77.732646	63.438119
1797.244515	76.375025	63.443124
1796.534051	82.640401	63.448129
1795.850413	81.999098	63.453134
1795.051955	85.971992	63.458138
1795.088871	75.635423	63.463143
1794.112782	84.216682	63.468148
1793.226481	74.791201	63.473153
1792.521990	73.202190	63.478158
1792.360289	83.492585	63.483162
1791.541816	80.277878	63.488167
1790.285844	81.050501	63.493172
1789.586370	80.612821	63.498177
1789.492813	75.753619	63.503182
1788.582300	84.764561	63.508186
1788.312116	78.346038	63.513191
1787.386984	72.748892	63.518196
1786.067480	71.416682	63.523201
1786.021660	73.023128	63.528206
1785.385899	78.324839	63.533210
1785.525883	73.810927	63.538215
1784.485476	81.997812	63.543220
1783.490078	80.443181	63.548225
1782.677396	73.082524	63.553230
1781.979651	78.967186	63.558234
1781.031386	77.568301	63.563239
1780.241172	80.348123	63.568244
1779.793006	76.232068	63.573249
1779.327788	75.103019	63.578254
1778.838164	77.100387	63.583258
1778.513177	67.912413	63.588263
1777.636581	80.782654	63.593268
1776.634149	74.813883	63.598273
1776.219026	64.729923	63.603278
1775.492867	78.839896	63.608282
1775.442490	70.123993	63.613287
1773.897363	72.699047	63.618292
1773.023978	78.066284	63.623297
1772.682389	65.374060	63.628302
1771.976213	76.122725	63.633306
1771.800804	65.955910	63.638311
1771.185759	71.529985	63.643316
1769.865936	74.373188	63.648321
1769.646544	73.744821	63.653326
1768.812393	76.316644	63.658330
1768.686786	63.818773	63.663335
1767.261826	70.201266	63.668340
1766.375742	70.995470	63.673345
1766.151473	69.835459	63.678350
1765.502495	71.242356	63.683354
1765.299996	66.502058	63.688359
1764.160983	80.286373	63.693364
1763.299687	72.501820	63.698369
1763.180336	65.251873	63.703374
1762.565393	79.287161	63.708378
1761.712893	71.613599	63.713383
1760.928374	72.683308	63.718388
1760.026794	73.060182	63.723393
1759.593531	65.525276	63.728398
1758.877625	70.262829	63.733402
1758.845309	71.274488	63.738407
1757.417240	73.624658	63.743412
1756.685229	82.393883	63.748417
1756.245283	73.268604	63.753422
1755.654038	82.127423	63.758426
1755.176979	79.659142	63.763431
1754.187661	79.359478	63.768436
1753.523393	82.522343	63.773441
1753.277553	71.365382	63.778446
1752.756511	87.099670	63.783450
1751.961063	78.135871	63.788455
1751.185968	78.819906	63.793460
1749.897233	86.333658	63.798465
1749.737024	77.512999	63.803470
1749.091582	76.277428	63.808474
1748.301762	80.850008	63.813479
1747.279129	83.446980	63.818484
1746.655869	79.711400	63.823489
1746.287586	75.513789	63.828494
1745.565907	81.472810	63.833498
1745.543689	76.285628	63.838503
1745.069765	75.090970	63.843508
1743.920234	76.854296	63.848513
1743.179239	72.748090	63.853518
1742.115064	82.971068	63.858522
1742.000723	79.837196	63.863527
1741.006091	74.877979	63.868532
1740.189563	76.579195	63.873537
1739.604364	79.829974	63.878542
1739.143701	88.448962	63.883546
1739.016113	80.885038	63.888551
1737.736241	83.387086	63.893556
1736.675376	84.758678	63.898561
1736.466433	69.612282	63.903566
1735.882681	69.757942	63.908570
1735.543938	67.942548	63.913575
1734.515506	76.075678	63.918580
1733.726871	61.315442	63.923585
1733.361522	71.917369	63.928590
1732.756356	75.814564	63.933594
1732.134266	75.313917	63.938599
1730.762452	71.707610	63.943604
1730.054784	80.426093	63.948609
1730.110457	78.166252	63.953614
1729.186668	86.055307	63.958618
1728.891908	86.475979	63.963623
1728.374453	80.218189	63.968628
1726.921020	78.452220	63.973633
1726.512824	74.944307	63.978638
1726.162291	85.842907	63.983642
1725.240785	81.123010	63.988647
1724.207723	80.103762	63.993652
1723.571196	86.438595	63.998657
1723.233678	79.970024	64.003662
1722.672045	81.922484	64.008666
1722.468092	77.557026	64.013671
1721.325319	75.679087	64.018676
1720.195582	79.169880	64.023681
1719.996303	76.135805	64.028686
1719.556510	77.707036	64.033690
1718.975477	74.218436	64.038695
1718.001952	76.198351	64.043700
1717.007538	78.582876	64.048705
1716.729569	71.988862	64.053710
1715.726644	82.711340	64.058714
1715.363417	82.871370	64.063719
1715.438906	77.023682	64.068724
1714.037562	82.282723	64.073729
1713.773629	73.593893	64.078734
1712.761203	80.903270	64.083738
1711.770871	78.722945	64.088743
1710.695065	82.013073	64.093748
1710.271613	83.441778	64.098753
1709.954878	79.321399	64.103758
1709.071143	80.808734	64.108762
1709.130756	76.046482	64.113767
1708.738351	81.422605	64.118772
1707.617562	79.758399	64.123777
1707.139592	71.659989	64.128782
1706.313944	76.690262	64.133786
1705.229158	78.677376	64.138791
1704.343607	75.309567	64.143796
1703.540622	76.341393	64.148801
1703.538907	74.099662	64.153806
1703.229460	75.449652	64.158810
1702.785675	73.587895	64.163815
1701.781019	77.827387	64.168820
1700.762128	75.909309	64.173825
1700.596821	68.007259	64.178830
1698.934698	82.668954	64.183834
1698.130463	83.931907	64.188839
1698.131189	78.760143	64.193844
1697.578622	81.362342	64.198849
1697.012114	73.515125	64.203854
1696.715590	82.751391	64.208858
1696.016412	74.878326	64.213863
1695.003417	73.535137	64.218868
1693.968995	78.224969	64.223873
1693.758814	74.894352	64.228878
1692.583032	77.170974	64.233882
1691.831481	72.753966	64.238887
1691.450284	74.623054	64.243892
1690.575193	75.638011	64.248897
1690.370297	70.531434	64.253902
1689.989475	79.235040	64.258906
1689.396830	80.463366	64.263911
1688.205801	78.151606	64.268916
1687.623169	77.880650	64.273921
1687.244032	71.629201	64.278926
1686.795595	78.773785	64.283930
1685.168183	68.558220	64.288935
1684.503110	77.759657	64.293940
1683.624281	74.179526	64.298945
1683.946016	72.092834	64.303950
1683.084963	78.330697	64.308954
1682.779066	70.269160	64.313959
1681.798083	73.487015	64.318964
1680.900402	78.157791	64.323969
1680.598034	65.482557	64.328974
1679.620098	77.967131	64.333978
1678.519350	77.977853	64.338983
1677.803536	72.818579	64.343988
1677.412405	75.350919	64.348993
1677.352196	66.581055	64.353998
1676.821093	73.014681	64.359002
1676.155717	76.857844	64.364007
1675.134209	75.964124	64.369012
1674.372256	70.195010	64.374017
1674.284821	76.119709	64.379022
1673.001986	71.091806	64.384026
1671.736972	72.747018	64.389031
1671.477387	67.102720	64.394036
1670.993133	73.356627	64.399041
1670.618933	70.428275	64.404046
1670.093096	75.056736	64.409050
1669.659484	74.071495	64.414055
1668.576947	72.974281	64.419060
1667.825788	74.739318	64.424065
1667.398614	68.170844	64.429070
1665.958718	76.323867	64.434074
1665.518150	76.515688	64.439079
1665.188864	70.873054	64.444084
1664.390232	79.995115	64.449089
1664.606844	73.593567	64.454094
1663.487940	85.483743	64.459098
1662.625979	82.246109	64.464103
1662.071638	72.496634	64.469108
1661.009251	81.719487	64.474113
1660.190921	71.929533	64.479118
1658.934611	74.715711	64.484122
1659.270994	78.016414	64.489127
1658.648518	72.814725	64.494132
1657.948090	74.330303	64.499137
1657.635850	66.526030	64.504142
1656.838423	74.154657	64.509146
1655.432549	78.213745	64.514151
1654.991070	72.022309	64.519156
1654.701230	71.835062	64.524161
1654.089133	69.079259	64.529166
1653.763161	81.323196	64.534170
1652.515717	69.650049	64.539175
1651.899375	71.395964	64.544180
1651.234178	80.842151	64.549185
1651.064322	72.464850	64.554190
1649.797345	76.835683	64.559194
1648.997422	82.639160	64.564199
1648.648079	75.299110	64.569204
1647.884824	79.710844	64.574209
1647.801987	78.928462	64.579214
1646.894943	81.058453	64.584218
1646.096106	75.494198	64.589223
1645.160066	71.251264	64.594228
1644.491272	79.920468	64.599233
1644.334566	70.825685	64.604238
1642.943728	75.889133	64.609242
1641.993712	69.202907	64.614247
1641.692445	75.570758	64.619252
1641.207574	84.694391	64.624257
1640.891995	74.354216	64.629262
1640.555382	83.234987	64.634266
1639.673146	74.099762	64.639271
1638.757277	85.578633	64.644276
1638.127695	79.366098	64.649281
1637.707934	72.824778	64.654286
1636.653741	76.833162	64.659290
1635.819276	71.366188	64.664295
1635.328033	70.970656	64.669300
1634.643795	74.277073	64.674305
1634.499250	73.078953	64.679310
1633.739287	72.632306	64.684314
1632.349710	68.791843	64.689319
1632.295412	67.860110	64.694324
1631.456648	77.342313	64.699329
1631.326960	72.228792	64.704334
1630.200465	75.310115	64.709338
1629.032986	68.647291	64.714343
1628.706700	71.853375	64.719348
1627.928139	77.878977	64.724353
1627.705387	67.481083	64.729358
1627.548981	76.139572	64.734362
1626.205329	76.418442	64.739367
1625.779165	67.090709	64.744372
1625.112038	75.359381	64.749377
1624.079804	65.804590	64.754382
1623.232728	71.892439	64.759386
1622.514096	74.358463	64.764391
1622.109798	60.688232	64.769396
1621.678356	64.707670	64.774401
1621.149971	68.070702	64.779406
1620.415171	78.153641	64.784410
1619.638257	69.976543	64.789415
1619.011300	71.442842	64.794420
1618.215542	83.540999	64.799425
1617.893847	70.283316	64.804430
1616.613621	63.550586	64.809434
1615.888138	73.121555	64.814439
1616.067356	77.388583	64.819444
1615.026561	81.690719	64.824449
1614.384872	82.508253	64.829454
1613.294406	75.809752	64.834458
1612.704307	73.712529	64.839463
1612.072842	60.182223	64.844468
1611.717155	72.745433	64.849473
1611.406827	68.224909	64.854478
1610.880809	77.015725	64.859482
1609.478875	76.440137	64.864487
1609.011608	76.433646	64.869492
1608.483830	77.356023	64.874497
1607.779637	70.153283	64.879502
1606.649303	74.621919	64.884506
1605.849472	72.000876	64.889511
1605.740489	69.282527	64.894516
1605.139290	77.211116	64.899521
1604.799538	68.478046	64.904526
1603.688253	79.629582	64.909530
1602.588467	79.834358	64.914535
1602.437086	76.950771	64.919540
1601.767142	78.742574	64.924545
1601.689365	71.902745	64.929550
1600.575029	76.553768	64.934554
1599.741163	72.122445	64.939559
1599.402923	71.051812	64.944564
1598.586419	73.900889	64.949569
1598.261444	79.404415	64.954574
1597.092494	72.809742	64.959578
1596.760695	73.422672	64.964583
1596.351488	66.549174	64.969588
1595.269279	74.372193	64.974593
1594.296216	73.076269	64.979598
1593.965974	77.035763	64.984602
1592.980687	70.313349	64.989607
1592.220290	75.548379	64.994612
1591.109393	68.691154	64.999617
1591.190614	66.933370	65.004622
1590.659417	74.243688	65.009626
1590.087078	77.710953	65.014631
1589.881460	78.695825	65.019636
1588.467319	82.573589	65.024641
1587.654333	71.618711	65.029646
1587.211244	78.092936	65.034650
1586.516772	80.769953	65.039655
1585.533184	75.734676	65.044660
1584.718311	79.799213	65.049665
1584.768598	77.272677	65.054670
1583.945793	81.098977	65.059674
1583.284613	84.178043	65.064679
1583.098813	67.188325	65.069684
1581.905780	81.149259	65.074689
1580.764635	76.055688	65.079694
1580.205755	80.185753	65.084698
1579.926699	85.836548	65.089703
1579.467405	76.589090	65.094708
1579.061636	81.332398	65.099713
1578.232564	80.814300	65.104718
1577.335684	75.694321	65.109722
1576.734614	76.010323	65.114727
1576.357656	75.369854	65.119732
1574.947548	75.898916	65.124737
1574.186766	78.112829	65.129742
1573.772049	69.441538	65.134746
1573.302560	73.504201	65.139751
1572.698622	64.753196	65.144756
1572.321604	72.881827	65.149761
1571.847748	77.546396	65.154766
1570.848572	76.734925	65.159770
1570.234512	88.423060	65.164775
1569.640447	74.907273	65.169780
1568.343878	86.010399	65.174785
1567.831236	79.910095	65.179790
1567.095587	75.476968	65.184794
1566.409957	75.475879	65.189799
1566.335698	70.903906	65.194804
1565.519776	85.472119	65.199809
1564.923766	76.666070	65.204814
1563.959850	73.670503	65.209818
1563.209612	89.043363	65.214823
1562.944784	73.640522	65.219828
1562.286271	75.579182	65.224833
1561.204439	72.585638	65.229838
1560.711649	70.553476	65.234842
1560.120306	81.684716	65.239847
1559.872207	68.915745	65.244852
1558.819889	75.964740	65.249857
1557.965118	79.962296	65.254862
1557.684408	79.725732	65.259866
1557.075158	80.797051	65.264871
1556.499039	73.202155	65.269876
1555.061448	69.264937	65.274881
1554.522246	62.400670	65.279886
1553.871639	69.008692	65.284890
1553.203243	73.024084	65.289895
1553.103352	70.091428	65.294900
1552.776496	72.122137	65.299905
1551.895522	63.105932	65.304910
1551.231630	69.720570	65.309914
1550.107593	73.915781	65.314919
1550.004090	61.289038	65.319924
1548.848864	71.265910	65.324929
1548.058345	66.285231	65.329934
1547.442156	71.131651	65.334938
1546.808542	72.835140	65.339943
1546.867248	67.594652	65.344948
1545.570171	78.476425	65.349953
1545.173659	71.162621	65.354958
1544.548718	71.390348	65.359962
1543.517947	76.966512	65.364967
1542.527757	64.164693	65.369972
1541.842899	72.079573	65.374977
1541.507185	71.038512	65.379982
1541.270263	73.850374	65.384986
1540.218936	70.449396	65.389991
1540.440625	70.701166	65.394996
1539.472813	76.127219	65.400001
1538.877519	69.797133	65.405006
1537.474660	73.830864	65.410010
1536.453795	76.657295	65.415015
1535.634712	64.241834	65.420020
1535.121690	72.528341	65.425025
1534.984542	67.391238	65.430030
1534.819103	77.793954	65.435034
1534.328421	74.551223	65.440039
1533.594858	71.322036	65.445044
1532.283976	86.720192	65.450049
1531.606441	77.031299	65.455054
1531.456748	77.798190	65.460058
1530.031759	85.236617	65.465063
1529.542972	71.609672	65.470068
1528.734850	77.491927	65.475073
1528.167734	71.091892	65.480078
1527.801081	77.909862	65.485082
1527.314256	73.840718	65.490087
1526.991655	69.733602	65.495092
1525.728654	76.229343	65.500097
1524.988081	71.414190	65.505102
1524.537961	65.299252	65.510106
1524.064288	74.900546	65.515111
1522.750100	66.913712	65.520116
1521.732862	80.098543	65.525121
1521.063783	71.087522	65.530126
1521.294349	76.353473	65.535130
1521.212895	71.260520	65.540135
1520.860175	69.467273	65.545140
1519.680271	71.672007	65.550145
1518.997964	73.566193	65.555150
1517.745703	70.897869	65.560154
1516.265097	76.393927	65.565159
1515.809906	71.392570	65.570164
1516.029272	76.210063	65.575169
1515.477596	74.465867	65.580174
1514.889937	70.841070	65.585178
1514.102438	75.903517	65.590183
1513.456877	74.414194	65.595188
1512.140177	64.512616	65.600193
1512.040280	73.396282	65.605198
1511.699357	64.579749	65.610202
1510.880525	70.066749	65.615207
1510.131116	65.806509	65.620212
1508.741136	78.888564	65.625217
1508.066191	72.738293	65.630222
1507.635271	72.268110	65.635226
1507.394373	70.385860	65.640231
1507.198332	69.803243	65.645236
1505.801272	68.545565	65.650241
1505.295319	65.942136	65.655246
1504.739613	72.048020	65.660250
1504.130280	71.995593	65.665255
1503.445558	64.471007	65.670260
1502.523547	68.659672	65.675265
1501.611933	67.017739	65.680270
1501.376337	65.312996	65.685274
1500.896023	67.578778	65.690279
1500.516834	69.947247	65.695284
1499.336287	71.606593	65.700289
1498.500660	71.121997	65.705294
1498.402734	70.084450	65.710298
1497.390040	64.833532	65.715303
1496.715003	71.647836	65.720308
1495.366152	68.118194	65.725313
1494.986831	72.762637	65.730318
1494.797896	56.909489	65.735322
1494.256044	68.483017	65.740327
1493.871093	61.852875	65.745332
1493.186642	72.752555	65.750337
1492.443078	63.844288	65.755342
1491.951808	67.863710	65.760346
1490.392719	68.632232	65.765351
1489.796522	68.131525	65.770356
1489.136441	71.832093	65.775361
1489.038174	76.628162	65.780366
1488.570296	66.479868	65.785370
1487.352060	74.679455	65.790375
1486.867148	64.179621	65.795380
1486.367141	71.323951	65.800385
1485.729503	74.815819	65.805390
1484.932775	62.875737	65.810394
1483.609968	72.753411	65.815399
1482.967898	63.915798	65.820404
1482.642578	70.792214	65.825409
1482.042999	61.946145	65.830414
1481.930328	66.402849	65.835418
1481.146696	74.521737	65.840423
1480.433723	74.719146	65.845428
1479.917211	71.422426	65.850433
1479.104730	73.415078	65.855438
1478.152978	67.327586	65.860442
1476.866720	72.638420	65.865447
1476.569465	68.504472	65.870452
1476.083050	66.149928	65.875457
1475.456643	73.394048	65.880462
1475.269819	74.079273	65.885466
1474.734125	74.025692	65.890471
1474.165700	61.858257	65.895476
1473.042583	73.554960	65.900481
1472.616097	68.952889	65.905486
1471.931160	66.364705	65.910490
1470.411801	67.919818	65.915495
1470.233500	63.018309	65.920500
1469.265714	72.251035	65.925505
1468.975179	68.369742	65.930510
1468.777831	69.091108	65.935514
1467.365487	70.809872	65.940519
1466.638033	67.541364	65.945524
1466.169220	64.217537	65.950529
1465.957696	70.068730	65.955534
1465.415138	65.203910	65.960538
1464.272234	72.479990	65.965543
1463.421148	68.134140	65.970548
1462.936445	73.685135	65.975553
1462.259884	68.453267	65.980558
1462.000969	65.918871	65.985562
1461.451911	65.228135	65.990567
1460.415262	64.340604	65.995572
1459.611348	71.208151	66.000577
1458.999962	71.069243	66.005582
1458.902894	61.051692	66.010586
1457.665853	67.971268	66.015591
1456.809440	65.040216	66.020596
1456.304484	66.884712	66.025601
1455.666008	64.213581	66.030606
1455.561654	62.230205	66.035610
1454.485538	74.588704	66.040615
1454.119365	75.428174	66.045620
1453.296119	67.376675	66.050625
1452.533263	70.503942	66.055630
1451.279814	68.079776	66.060634
1450.394573	78.047951	66.065639
1450.479443	66.742864	66.070644
1449.868907	70.237990	66.075649
1449.155231	58.522906	66.080654
1449.446321	59.900373	66.085658
1447.951991	67.710266	66.090663
1447.131471	64.715839	66.095668
1446.361511	75.606474	66.100673
1446.100641	71.960489	66.105678
1445.400949	57.147231	66.110682
1443.911825	69.735096	66.115687
1443.612209	60.558233	66.120692
1443.030329	63.948984	66.125697
1442.680515	61.694610	66.130702
1442.529743	57.635854	66.135706
1441.488755	64.321752	66.140711
1440.663476	61.769831	66.145716
1440.236452	61.267016	66.150721
1439.476249	58.456074	66.155726
1438.383348	62.891092	66.160730
1437.497774	74.021769	66.165735
1436.933223	73.348686	66.170740
1436.175996	66.838716	66.175745
1435.787979	71.348470	66.180750
1435.836198	66.182411	66.185754
1435.332052	63.091204	66.190759
1434.521457	70.588289	66.195764
1433.722054	57.852535	66.200769
1432.347997	66.004591	66.205774
1431.796373	61.865638	66.210778
1430.990486	79.945126	66.215783
1430.383864	62.215936	66.220788
1430.214934	69.961199	66.225793
1429.394266	77.049108	66.230798
1429.210256	72.653028	66.235802
1428.218792	74.336470	66.240807
1427.760837	67.405818	66.245812
1426.583099	74.224466	66.250817
1425.528953	72.735623	66.255822
1425.139954	67.968071	66.260826
1424.296289	76.228680	66.265831
1423.538218	63.848991	66.270836
1423.467747	64.940597	66.275841
1423.109679	73.271632	66.280846
1423.032310	63.641484	66.285850
1421.925772	68.431324	66.290855
1421.096863	66.793013	66.295860
1420.163226	72.559004	66.300865
1418.828005	70.779604	66.305870
1418.276665	60.647194	66.310874
1417.608369	63.981294	66.315879
1417.938155	63.216707	66.320884
1417.533475	64.920888	66.325889
1415.970311	71.011336	66.330894
1415.363805	65.495131	66.335898
1414.597818	75.430262	66.340903
1413.944148	65.766529	66.345908
1413.660115	71.937225	66.350913
1413.215808	69.429039	66.355918
1412.445596	67.553719	66.360922
1411.490817	66.037608	66.365927
1410.949440	60.142774	66.370932
1410.811397	71.203519	66.375937
1409.484782	80.710430	66.380942
1408.935840	62.673359	66.385946
1408.167428	71.509217	66.390951
1407.820184	60.760847	66.395956
1406.713441	65.210477	66.400961
1405.225004	68.401162	66.405966
1404.959111	64.467897	66.410970
1404.353596	74.382270	66.415975
1404.173001	62.964349	66.420980
1404.062406	59.991695	66.425985
1403.371069	67.803878	66.430990
1402.721597	69.818766	66.435994
1401.676661	77.459386	66.440999
1401.169117	62.998886	66.446004
1400.821549	75.279259	66.451009
1399.550938	58.955654	66.456014
1398.579419	60.070448	66.461018
1398.144034	69.935961	66.466023
1397.859323	63.079473	66.471028
1397.396810	56.136981	66.476033
1396.403410	74.029884	66.481038
1395.591034	59.675250	66.486042
1394.499002	67.275377	66.491047
1394.460863	60.348264	66.496052
1394.088987	59.458662	66.501057
1392.627985	62.630442	66.506062
1392.202396	65.600515	66.511066
1391.667430	61.618184	66.516071
1391.272609	58.592345	66.521076
1390.850366	63.546490	66.526081
1389.822015	63.535408	66.531086
1389.254303	63.398111	66.536090
1388.569632	73.756671	66.541095
1388.082734	69.809924	66.546100
1387.160328	69.067846	66.551105
1386.072430	72.729160	66.556110
1385.509759	72.580737	66.561114
1385.058927	74.830824	66.566119
1384.873058	68.699488	66.571124
1383.736171	67.301788	66.576129
1383.031480	74.511552	66.581134
1382.585273	64.975332	66.586138
1381.785777	75.488543	66.591143
1381.151413	62.400881	66.596148
1380.577877	71.710200	66.601153
1379.619944	73.595138	66.606158
1378.835272	67.135271	66.611162
1378.803359	72.951772	66.616167
1378.032656	79.586286	66.621172
1377.208084	70.261273	66.626177
1376.339994	73.091183	66.631182
1376.257482	65.302099	66.636186
1375.745119	66.415271	66.641191
1374.503691	68.114669	66.646196
1373.723969	76.051719	66.651201
1372.855352	66.921740	66.656206
1372.741351	63.827307	66.661210
1372.355009	71.377294	66.666215
1371.252249	68.612765	66.671220
1370.203956	72.156781	66.676225
1369.362897	71.227894	66.681230
1369.231384	65.360796	66.686234
1368.752464	75.377836	66.691239
1368.269911	67.807224	66.696244
1367.301175	67.875938	66.701249
1366.473519	67.089620	66.706254
1365.942574	62.894639	66.711258
1365.447936	70.205413	66.716263
1365.011056	70.886868	66.721268
1363.696242	72.568833	66.726273
1363.115526	77.735233	66.731278
1362.738897	63.789545	66.736282
1361.974414	71.341108	66.741287
1361.494767	70.422195	66.746292
1360.319572	65.746604	66.751297
1359.498437	73.074587	66.756302
1359.235566	62.944121	66.761306
1359.076792	71.306561	66.766311
1358.310308	77.141048	66.771316
1357.207650	68.186130	66.776321
1356.298922	74.078517	66.781326
1356.280585	69.982884	66.786330
1355.666262	77.983987	66.791335
1355.117625	64.355100	66.796340
1354.290702	70.682672	66.801345
1353.686797	75.195835	66.806350
1352.867071	60.337232	66.811354
1351.709402	74.264890	66.816359
1350.747545	70.853773	66.821364
1350.111078	67.026973	66.826369
1349.620293	75.828338	66.831374
1349.357587	67.739722	66.836378
1348.580535	76.241159	66.841383
1348.332177	75.993148	66.846388
1348.316402	73.332669	66.851393
1347.402942	80.913687	66.856398
1346.312980	75.065401	66.861402
1345.845359	73.317890	66.866407
1344.395045	69.406602	66.871412
1343.733519	68.457250	66.876417
1343.604952	76.302570	66.881422
1343.324722	68.934159	66.886426
1342.701684	75.345642	66.891431
1341.358921	73.204020	66.896436
1340.668211	70.591583	66.901441
1340.020902	68.639975	66.906446
1339.772451	59.915796	66.911450
1339.192970	75.419268	66.916455
1338.244033	73.494032	66.921460
1337.524187	70.862900	66.926465
1336.619421	73.320954	66.931470
1336.429777	59.507864	66.936474
1335.439750	73.198807	66.941479
1334.422768	69.050719	66.946484
1333.389132	68.055336	66.951489
1332.727229	74.657807	66.956494
1333.246668	58.204239	66.961498
1332.801336	76.499484	66.966503
1332.276296	58.410984	66.971508
1331.249945	69.675494	66.976513
1330.076523	73.602894	66.981518
1330.049615	67.721444	66.986522
1328.850403	72.205471	66.991527
1327.752940	69.638983	66.996532
1327.614156	62.500562	67.001537
1326.505314	75.753974	67.006542
1326.641503	70.868504	67.011546
1325.664060	74.205803	67.016551
1325.507135	75.691929	67.021556
1324.469412	73.339415	67.026561
1323.527274	80.412210	67.031566
1323.406557	77.172486	67.036570
1322.636176	80.391054	67.041575
1321.362305	77.676748	67.046580
1321.116639	68.019765	67.051585
1320.091959	72.852845	67.056590
1319.915372	67.142276	67.061594
1319.275000	74.137358	67.066599
1318.036176	75.707251	67.071604
1317.582372	69.332460	67.076609
1317.012744	81.086398	67.081614
1317.020682	73.104209	67.086618
1316.290648	73.913218	67.091623
1314.896822	71.790608	67.096628
1314.651474	72.154292	67.101633
1313.801966	81.730720	67.106638
1313.569058	67.928191	67.111642
1312.023434	79.150557	67.116647
1311.166365	68.336721	67.121652
1311.384927	74.556371	67.126657
1310.546957	77.088254	67.131662
1310.167780	64.155467	67.136666
1308.701863	77.496061	67.141671
1308.284600	75.981895	67.146676
1307.799884	67.221983	67.151681
1306.848993	74.293907	67.156686
1307.335077	68.874877	67.161690
1306.241636	71.585882	67.166695
1304.869695	68.431681	67.171700
1304.096452	66.403353	67.176705
1303.251728	73.444471	67.181710
1303.563657	73.978795	67.186714
1302.945090	74.364926	67.191719
1301.903757	71.484508	67.196724
1301.171442	68.538953	67.201729
1300.281350	71.705387	67.206734
1300.004976	68.703488	67.211738
1299.742150	73.149186	67.216743
1298.260421	81.770870	67.221748
1297.804541	67.926782	67.226753
1297.044180	66.151238	67.231758
1296.890019	66.331162	67.236762
1296.142614	71.355188	67.241767
1295.666095	65.856618	67.246772
1294.899770	64.599177	67.251777
1293.977397	67.852450	67.256782
1293.424147	69.646808	67.261786
1292.320480	74.462626	67.266791
1291.660265	65.398831	67.271796
1291.155473	63.487172	67.276801
1290.791509	69.338012	67.281806
1290.192648	62.802544	67.286810
1289.215965	65.040426	67.291815
1288.606678	59.707872	67.296820
1288.076161	66.755195	67.301825
1287.909501	72.553313	67.306830
1287.177370	67.518484	67.311834
1286.613131	67.114564	67.316839
1285.597468	72.493184	67.321844
1284.545658	65.609752	67.326849
1283.419338	72.681712	67.331854
1282.800461	72.390563	67.336858
1282.072858	64.720215	67.341863
1281.608715	72.271680	67.346868
1281.783699	64.079726	67.351873
1281.253539	74.627748	67.356878
1280.662158	68.565845	67.361882
1279.537768	70.228650	67.366887
1278.766030	75.278553	67.371892
1278.520882	68.172948	67.376897
1276.791945	69.713866	67.381902
1275.880101	63.383949	67.386906
1276.114678	68.996932	67.391911
1275.271324	65.203196	67.396916
1275.109003	64.907698	67.401921
1274.648188	73.311974	67.406926
1273.800474	65.929810	67.411930
1272.379168	68.222894	67.416935
1271.752471	74.389493	67.421940
1271.411010	55.600933	67.426945
1271.015884	70.427867	67.431950
1270.707553	65.978089	67.436954
1269.898135	68.582452	67.441959
1268.732532	72.349454	67.446964
1268.165751	77.295984	67.451969
1267.537597	76.355139	67.456974
1266.231747	70.505944	67.461978
1265.463354	75.615274	67.466983
1265.675098	75.408097	67.471988
1264.917824	63.876173	67.476993
1264.370509	74.676594	67.481998
1263.791272	74.276428	67.487002
1263.512091	76.578448	67.492007
1262.829056	77.222715	67.497012
1262.309546	66.332157	67.502017
1260.881555	66.165321	67.507022
1259.843452	68.433065	67.512026
1259.134180	72.372196	67.517031
1258.492135	73.833223	67.522036
1258.432317	66.450773	67.527041
1258.090869	78.997710	67.532046
1257.280656	65.811111	67.537050
1256.124001	69.330672	67.542055
1255.160925	65.001279	67.547060
1255.165363	70.387621	67.552065
1254.211933	64.517175	67.557070
1253.757099	64.683447	67.562074
1252.600485	62.569191	67.567079
1252.037845	64.684092	67.572084
1252.147710	67.899985	67.577089
1251.439837	69.341495	67.582094
1250.481825	65.281222	67.587098
1249.456820	61.121899	67.592103
1248.423220	69.228729	67.597108
1248.197628	61.855322	67.602113
1247.572885	72.668602	67.607118
1247.569046	59.621839	67.612122
1246.995483	69.014054	67.617127
1245.977565	65.601114	67.622132
1245.539336	54.895986	67.627137
1244.478842	61.923126	67.632142
1243.568822	66.242793	67.637146
1242.709015	67.724130	67.642151
1242.317337	61.449240	67.647156
1241.834963	65.198347	67.652161
1241.511553	76.856051	67.657166
1240.227175	72.187739	67.662170
1239.591283	66.723962	67.667175
1238.835499	65.742212	67.672180
1238.651593	69.972302	67.677185
1237.822196	80.539192	67.682190
1237.277652	70.326707	67.687194
1236.084344	70.293375	67.692199
1235.589717	73.819988	67.697204
1235.618642	72.871252	67.702209
1234.761053	70.201355	67.707214
1234.478629	63.048063	67.712218
1233.465169	67.101245	67.717223
1232.775222	75.988414	67.722228
1231.968633	68.008326	67.727233
1230.393573	71.440455	67.732238
1230.169398	70.603338	67.737242
1229.808351	69.595058	67.742247
1229.255895	67.073044	67.747252
1229.287536	70.899537	67.752257
1227.920913	72.884470	67.757262
1226.745326	67.908603	67.762266
1226.470999	70.360969	67.767271
1226.047317	73.414800	67.772276
1225.792758	57.329798	67.777281
1224.461876	69.034856	67.782286
1223.475649	70.055100	67.787290
1223.061110	68.339961	67.792295
1222.578230	72.063896	67.797300
1222.386560	72.597991	67.802305
1221.695627	74.253304	67.807310
1220.677099	68.672287	67.812314
1220.237375	69.116620	67.817319
1219.205233	69.940657	67.822324
1218.756159	66.532564	67.827329
1217.461156	66.090352	67.832334
1216.800759	75.618616	67.837338
1216.448621	64.217070	67.842343
1216.177016	76.277987	67.847348
1216.032481	66.776594	67.852353
1214.881569	67.353347	67.857358
1213.559449	76.545716	67.862362
1213.243254	72.467140	67.867367
1212.477307	70.538231	67.872372
1212.336398	72.076877	67.877377
1211.762133	66.450589	67.882382
1210.682173	72.866496	67.887386
1210.166404	69.216413	67.892391
1209.284780	86.575086	67.897396
1209.072223	74.141920	67.902401
1208.040037	73.516956	67.907406
1207.377243	69.712844	67.912410
1207.056910	71.033537	67.917415
1206.006610	75.936939	67.922420
1205.648465	73.305083	67.927425
1204.746285	74.587244	67.932430
1204.134077	64.190970	67.937434
1203.605071	66.031314	67.942439
1202.751196	71.429613	67.947444
1202.429123	65.802383	67.952449
1201.135677	62.450838	67.957454
1200.813725	71.158954	67.962458
1200.235569	68.700156	67.967463
1199.252825	68.190671	67.972468
1199.499020	66.431089	67.977473
1198.240808	72.137815	67.982478
1197.031906	66.444538	67.987482
1197.336615	62.061117	67.992487
1196.295311	77.528790	67.997492
1195.647948	69.116862	68.002497
1194.429077	71.258076	68.007502
1193.820877	76.171441	68.012506
1193.565683	72.205180	68.017511
1193.195956	81.556977	68.022516
1192.530382	75.234646	68.027521
1191.633430	78.247937	68.032526
1191.011385	79.357801	68.037530
1190.792516	68.418547	68.042535
1189.828670	76.403318	68.047540
1188.757813	68.496906	68.052545
1187.971337	76.823133	68.057550
1187.352037	79.759283	68.062554
1187.308458	75.730344	68.067559
1186.347122	77.359331	68.072564
1185.482363	68.208216	68.077569
1184.756136	78.760206	68.082574
1184.454333	72.263099	68.087578
1183.889016	68.773076	68.092583
1183.010289	78.343461	68.097588
1182.375237	80.902590	68.102593
1181.333898	73.129670	68.107598
1180.893438	75.074850	68.112602
1180.921712	75.825093	68.117607
1179.766542	75.529466	68.122612
1178.992645	75.620513	68.127617
1178.025345	78.007986	68.132622
1177.578648	79.214928	68.137626
1177.244410	65.400175	68.142631
1176.735645	72.045114	68.147636
1175.698879	60.778560	68.152641
1174.824079	71.996611	68.157646
1174.007973	66.733432	68.162650
1174.179061	74.712952	68.167655
1173.365909	65.381305	68.172660
1172.844733	68.916413	68.177665
1171.610687	73.640502	68.182670
1171.095649	67.924346	68.187674
1170.741506	72.677376	68.192679
1169.426344	72.739525	68.197684
1168.883403	70.448772	68.202689
1168.180502	68.252905	68.207694
1168.117751	73.808634	68.212698
1167.422549	72.648767	68.217703
1166.166965	72.814395	68.222708
1165.380042	58.141282	68.227713
1164.811283	72.898075	68.232718
1164.450748	69.416016	68.237722
1164.284716	70.579245	68.242727
1163.441949	75.591982	68.247732
1162.723931	74.079591	68.252737
1161.723183	73.907128	68.257742
1161.076460	80.677135	68.262746
1161.101934	72.403813	68.267751
1159.593429	76.776627	68.272756
1159.331631	72.290078	68.277761
1158.491888	67.595396	68.282766
1158.220420	67.887379	68.287770
1157.852740	69.406040	68.292775
1156.527787	73.479807	68.297780
1156.307498	63.467209	68.302785
1155.298892	67.513651	68.307790
1154.190896	74.672489	68.312794
1153.413725	68.197573	68.317799
1152.751600	73.036098	68.322804
1152.683891	68.254226	68.327809
1151.683504	73.543018	68.332814
1151.431676	70.051426	68.337818
1151.126273	63.732172	68.342823
1149.743378	75.258265	68.347828
1148.937984	66.430928	68.352833
1148.681482	67.042439	68.357838
1148.062010	72.054836	68.362842
1147.940985	65.146276	68.367847
1146.643771	75.548937	68.372852
1145.992336	66.684583	68.377857
1145.136851	76.825699	68.382862
1144.723818	72.333469	68.387866
1144.256553	71.536400	68.392871
1142.989478	82.361385	68.397876
1142.509866	72.024914	68.402881
1141.865435	73.006780	68.407886
1141.405410	77.856095	68.412890
1141.497325	70.077823	68.417895
1140.015979	76.433791	68.422900
1139.231572	62.434825	68.427905
1138.731571	74.540763	68.432910
1137.947479	74.301209	68.437914
1137.849490	73.449990	68.442919
1136.341204	72.060682	68.447924
1135.911384	74.372710	68.452929
1135.304614	68.748447	68.457934
1134.963436	74.276063	68.462938
1134.593866	68.331726	68.467943
1133.825921	78.356017	68.472948
1133.187508	72.765197	68.477953
1132.601478	75.751310	68.482958
1131.518328	74.451043	68.487962
1131.037597	75.287255	68.492967
1130.394606	72.697470	68.497972
1129.437205	71.924330	68.502977
1128.550428	66.278938	68.507982
1127.542155	65.983829	68.512986
1127.446108	66.309326	68.517991
1126.485177	72.117919	68.522996
1126.349805	68.270089	68.528001
1125.876600	74.489358	68.533006
1124.547610	71.168787	68.538010
1123.839509	72.113007	68.543015
1123.240778	69.604456	68.548020
1122.776020	62.190705	68.553025
1122.229103	60.736258	68.558030
1121.946369	68.990440	68.563034
1121.313156	63.444128	68.568039
1119.872032	67.743047	68.573044
1119.614710	57.811795	68.578049
1119.459606	62.308515	68.583054
1118.451279	74.986206	68.588058
1117.725044	65.480225	68.593063
1116.888882	68.911385	68.598068
1116.678480	67.850479	68.603073
1115.537700	66.159841	68.608078
1114.476596	72.796338	68.613082
1114.102370	70.302633	68.618087
1113.246543	71.314779	68.623092
1112.919378	61.193390	68.628097
1112.438988	66.100661	68.633102
1112.365298	69.116278	68.638106
1111.179876	63.815304	68.643111
1110.302819	74.850992	68.648116
1110.089941	77.231660	68.653121
1108.911680	63.723279	68.658126
1107.738845	66.506334	68.663130
1107.557540	62.560588	68.668135
1106.571259	75.261740	68.673140
1106.120534	74.658018	68.678145
1105.918167	72.162122	68.683150
1105.812899	70.478902	68.688154
1105.067322	65.290499	68.693159
1103.676122	66.678122	68.698164
1103.435045	61.625560	68.703169
1101.970952	63.425513	68.708174
1100.961533	71.014298	68.713178
1100.777055	58.346630	68.718183
1100.235086	62.712630	68.723188
1099.831958	62.226673	68.728193
1099.693148	66.359438	68.733198
1098.929202	65.146225	68.738202
1098.277478	58.111056	68.743207
1097.030962	63.193327	68.748212
1096.724730	58.109689	68.753217
1095.588463	63.430832	68.758222
1094.568988	71.037523	68.763226
1094.351737	56.297282	68.768231
1093.821070	64.079204	68.773236
1093.359988	65.274010	68.778241
1093.063676	60.722332	68.783246
1091.981969	76.412048	68.788250
1091.202037	62.237865	68.793255
1090.333935	62.106252	68.798260
1090.200987	61.960856	68.803265
1089.215893	66.195509	68.808270
1088.155311	69.897590	68.813274
1087.817123	63.129638	68.818279
1086.928029	72.104200	68.823284
1086.955267	66.343358	68.828289
1085.999916	64.059292	68.833294
1084.970483	74.224671	68.838298
1085.027639	64.715205	68.843303
1083.876239	74.580958	68.848308
1083.653947	63.148125	68.853313
1082.285458	67.280281	68.858318
1081.543015	64.301371	68.863322
1081.209538	66.410992	68.868327
1080.761980	59.169558	68.873332
1080.008505	59.095684	68.878337
1079.427962	70.547942	68.883342
1078.396062	65.570013	68.888346
1078.345864	52.472801	68.893351
1077.942331	57.469537	68.898356
1076.657671	57.663454	68.903361
1075.673282	60.255569	68.908366
1075.149551	59.343052	68.913370
1074.537793	60.095921	68.918375
1073.850921	68.737447	68.923380
1073.812794	59.230882	68.928385
1072.485051	61.571150	68.933390
1071.916002	62.372756	68.938394
1071.705962	63.623255	68.943399
1071.214629	63.719219	68.948404
1069.846223	55.822356	68.953409
1069.246983	63.098941	68.958414
1068.640716	68.857466	68.963418
1068.137088	55.041358	68.968423
1067.713769	57.296225	68.973428
1066.476601	61.345504	68.978433
1065.778689	69.798274	68.983438
1064.974153	60.724117	68.988442
1064.728904	66.826195	68.993447
1064.333107	69.614745	68.998452
1063.995951	66.791030	69.003457
1062.832155	70.581445	69.008462
1061.852045	72.525495	69.013466
1061.631211	57.797319	69.018471
1061.323903	67.328274	69.023476
1060.205930	67.102093	69.028481
1059.189814	66.857680	69.033486
1058.569986	74.359233	69.038490
1058.437836	70.583089	69.043495
1057.560975	73.325735	69.048500
1056.772124	72.771235	69.053505
1055.802903	70.635595	69.058510
1055.432298	75.972471	69.063514
1055.145764	72.695635	69.068519
1054.382254	81.381476	69.073524
1053.749292	65.661288	69.078529
1053.206045	67.220676	69.083534
1052.336553	64.073668	69.088538
1051.574263	67.060366	69.093543
1050.048856	74.934876	69.098548
1049.678783	72.836763	69.103553
1049.139841	65.878599	69.108558
1048.422983	72.400501	69.113562
1048.720070	71.657675	69.118567
1048.031387	73.521429	69.123572
1047.418234	68.832178	69.128577
1046.454029	68.437175	69.133582
1045.579182	75.829248	69.138586
1044.909110	75.818461	69.143591
1044.295644	75.123803	69.148596
1043.798606	72.416674	69.153601
1042.975308	63.196926	69.158606
1042.407231	75.476748	69.163610
1042.401701	62.838046	69.168615
1040.886130	69.703553	69.173620
1040.138862	74.816392	69.178625
1039.568549	66.287100	69.183630
1038.790129	80.864282	69.188634
1038.581108	66.730498	69.193639
1037.478822	74.531764	69.198644
1036.556191	74.629356	69.203649
1036.212873	59.105883	69.208654
1035.184812	74.707865	69.213658
1035.321041	63.074310	69.218663
1034.783121	62.688411	69.223668
1034.050941	66.731349	69.228673
1033.495357	66.368211	69.233678
1032.575686	82.676735	69.238682
1031.717007	72.118636	69.243687
1030.531492	72.676489	69.248692
1030.034246	68.527496	69.253697
1029.854331	69.080504	69.258702
1028.821800	72.737926	69.263706
1028.928855	68.161780	69.268711
1028.130517	77.055284	69.273716
1027.276108	71.217277	69.278721
1026.644016	67.256368	69.283726
1025.857679	77.476041	69.288730
1025.029053	75.246071	69.293735
1024.041030	72.613552	69.298740
1023.352997	69.123253	69.303745
1023.315900	70.883322	69.308750
1022.692537	77.844720	69.313754
1022.372603	66.968590	69.318759
1021.018588	76.134480	69.323764
1020.494113	75.902983	69.328769
1020.314510	63.471321	69.333774
1019.332907	70.322757	69.338778
1018.568420	60.736911	69.343783
1017.758086	64.232341	69.348788
1016.882642	72.576575	69.353793
1016.430394	63.463416	69.358798
1015.899295	76.833430	69.363802
1015.550916	68.475731	69.368807
1014.431826	72.706109	69.373812
1013.673974	77.104746	69.378817
1013.350684	73.997622	69.383822
1012.578709	82.038762	69.388826
1012.173827	67.590778	69.393831
1011.170325	68.056679	69.398836
1010.415354	65.210578	69.403841
1010.229647	70.258828	69.408846
1009.011543	78.842528	69.413850
1008.857015	59.005233	69.418855
1007.992653	65.970005	69.423860
1007.316980	64.950891	69.428865
1007.336986	67.151552	69.433870
1005.859662	68.748545	69.438874
1005.003138	60.838250	69.443879
1004.119049	70.895852	69.448884
1003.532069	67.133659	69.453889
1003.524130	58.309530	69.458894
1002.731521	66.707863	69.463898
1002.686927	67.549525	69.468903
1001.443369	58.553727	69.473908
1000.861975	65.631480	69.478913
1000.379122	61.226226	69.483918
999.530923	70.866782	69.488922
998.701732	59.082397	69.493927
997.794534	74.117787	69.498932
997.288425	66.096168	69.503937
997.274791	59.659868	69.508942
995.915508	75.601586	69.513946
995.206075	62.815818	69.518951
994.751843	66.214743	69.523956
994.073502	61.660213	69.528961
993.598087	62.203041	69.533966
992.344358	68.068897	69.538970
991.956719	54.426358	69.543975
991.368736	61.546683	69.548980
990.871665	63.580119	69.553985
990.646715	71.173119	69.558990
989.356770	74.354789	69.563994
988.656088	60.227461	69.568999
988.099469	60.999711	69.574004
987.381594	68.663706	69.579009
987.216023	65.949949	69.584014
985.914351	57.298041	69.589018
985.364809	61.938094	69.594023
985.165443	70.241939	69.599028
984.212343	64.639913	69.604033
984.082350	55.544994	69.609038
982.744298	62.583785	69.614042
982.061570	59.711108	69.619047
981.460755	64.012987	69.624052
981.010493	65.798024	69.629057
980.530256	60.167518	69.634062
979.202442	63.572373	69.639066
978.771527	55.462890	69.644071
978.150044	67.578570	69.649076
977.810375	63.933888	69.654081
977.261020	56.973578	69.659086
976.268482	70.759698	69.664090
975.747221	58.285906	69.669095
975.334555	65.785926	69.674100
974.423068	63.334118	69.679105
973.240047	65.355168	69.684110
972.405332	71.266501	69.689114
972.199191	59.737770	69.694119
972.050935	71.723860	69.699124
971.205053	66.455562	69.704129
970.418229	59.335405	69.709134
969.903214	70.281859	69.714138
969.230985	57.859186	69.719143
968.187867	69.021207	69.724148
967.169023	67.171967	69.729153
966.780587	64.163633	69.734158
966.168968	63.731156	69.739162
965.759828	60.043904	69.744167
965.816186	61.196286	69.749172
964.546327	63.366018	69.754177
963.609006	70.502362	69.759182
962.851233	72.245335	69.764186
962.681924	62.023915	69.769191
961.359538	62.234585	69.774196
960.550974	69.032316	69.779201
960.157556	64.495308	69.784206
959.620158	72.516799	69.789210
959.105332	66.311984	69.794215
958.774459	74.036803	69.799220
958.152542	71.773419	69.804225
957.154212	56.162815	69.809230
956.214762	68.354660	69.814234
955.795010	70.957065	69.819239
955.270337	68.816758	69.824244
954.460788	70.224011	69.829249
953.757323	65.515114	69.834254
952.986298	70.327307	69.839258
952.387334	54.979082	69.844263
952.115468	62.863913	69.849268
951.299604	74.021754	69.854273
950.337794	69.408020	69.859278
949.491343	66.687723	69.864282
949.063465	65.923006	69.869287
948.628454	67.430317	69.874292
947.885033	72.243704	69.879297
947.126132	75.874803	69.884302
946.377567	69.084788	69.889306
945.773448	66.251545	69.894311
945.395294	68.510528	69.899316
944.953252	67.076034	69.904321
944.026981	58.913241	69.909326
942.949844	69.500068	69.914330
942.706235	64.386380	69.919335
942.159314	62.596842	69.924340
941.407231	67.691172	69.929345
940.329549	60.285720	69.934350
939.991634	67.298883	69.939354
939.165537	65.457295	69.944359
939.036683	58.714696	69.949364
937.782192	63.168396	69.954369
937.424808	56.849392	69.959374
936.761609	67.325459	69.964378
936.135165	63.340311	69.969383
935.135139	54.349802	69.974388
934.260814	66.114068	69.979393
934.022422	61.809053	69.984398
933.127971	70.175495	69.989402
932.904946	58.130612	69.994407
932.487750	59.679080	69.999412
931.210556	66.150909	70.004417
930.734200	64.102589	70.009422
929.630095	76.056603	70.014426
929.310672	63.777185	70.019431
929.025881	69.638547	70.024436
927.564567	70.574037	70.029441
927.069338	64.044573	70.034446
926.425519	65.261216	70.039450
926.438363	62.034958	70.044455
925.841824	56.514771	70.049460
925.120331	66.569396	70.054465
924.537994	60.390757	70.059470
923.519890	66.893604	70.064474
922.560093	62.998314	70.069479
921.655917	66.136821	70.074484
920.382744	66.150005	70.079489
920.673265	63.201436	70.084494
920.094060	68.159585	70.089498
919.835661	65.132933	70.094503
919.640205	63.031373	70.099508
918.040252	68.112637	70.104513
917.543366	60.108798	70.109518
916.929460	70.238548	70.114522
916.549573	56.857577	70.119527
915.483902	58.611053	70.124532
914.218229	61.899890	70.129537
914.037579	59.272007	70.134542
913.202941	73.775130	70.139546
912.799810	65.191971	70.144551
912.932369	62.930422	70.149556
911.698091	64.165700	70.154561
911.343442	62.880050	70.159566
910.455820	67.429993	70.164570
909.042642	66.346953	70.169575
908.285972	61.693755	70.174580
907.477254	68.441388	70.179585
907.839764	73.040103	70.184590
906.492103	70.535124	70.189594
906.487926	63.952743	70.194599
906.475514	65.420439	70.199604
905.108598	63.768189	70.204609
904.454109	60.822403	70.209614
903.892050	61.214693	70.214618
903.137532	64.764522	70.219623
901.884564	66.968085	70.224628
901.004357	62.930095	70.229633
900.961909	55.163413	70.234638
900.377417	57.360636	70.239642
900.145862	60.718269	70.244647
899.261499	63.311440	70.249652
898.206919	63.068912	70.254657
897.961663	63.359971	70.259662
896.848247	65.492268	70.264666
895.493349	64.418591	70.269671
895.610392	64.153018	70.274676
895.155612	68.278322	70.279681
894.394434	60.563293	70.284686
893.802052	66.454837	70.289690
893.247796	58.294259	70.294695
892.399943	63.098694	70.299700
891.728328	61.618663	70.304705
891.593377	57.324356	70.309710
890.685062	62.623859	70.314714
889.637615	56.801190	70.319719
888.984169	57.111639	70.324724
888.055197	66.117515	70.329729
887.727687	55.017333	70.334734
887.235356	63.824876	70.339738
886.444520	68.253252	70.344743
885.972012	61.279795	70.349748
884.986047	65.057152	70.354753
884.997473	60.352925	70.359758
883.204711	71.873866	70.364762
882.543532	57.694414	70.369767
882.156144	64.726312	70.374772
881.515905	74.204556	70.379777
881.290085	60.698523	70.384782
880.941632	67.342852	70.389786
880.492787	62.290770	70.394791
879.416663	61.048173	70.399796
878.472900	67.910117	70.404801
878.039860	63.066897	70.409806
876.595094	67.167957	70.414810
875.986130	57.624983	70.419815
875.357484	51.181538	70.424820
874.628633	57.558272	70.429825
874.646963	54.224109	70.434830
874.550240	67.369719	70.439834
873.789279	64.688476	70.444839
873.091831	59.072298	70.449844
872.144009	68.350208	70.454849
871.840457	58.905310	70.459854
870.130678	62.086286	70.464858
869.506331	67.995542	70.469863
869.378391	62.842710	70.474868
868.418246	69.008419	70.479873
868.788669	56.991765	70.484878
867.307405	63.382906	70.489882
866.728369	67.216877	70.494887
866.474923	62.115541	70.499892
865.051629	66.179770	70.504897
864.403375	60.046378	70.509902
863.208802	66.498147	70.514906
863.207743	59.783796	70.519911
862.970951	61.408733	70.524916
862.571660	66.095293	70.529921
861.251768	67.265908	70.534926
860.268659	68.451468	70.539930
859.964944	64.998788	70.544935
859.844269	64.705646	70.549940
858.563685	66.791982	70.554945
857.530617	69.568911	70.559950
856.664485	69.726330	70.564954
856.541300	62.777119	70.569959
855.991208	64.097316	70.574964
855.306346	74.849060	70.579969
855.170647	67.464251	70.584974
854.705202	66.172715	70.589978
853.591733	63.560145	70.594983
852.858693	57.744814	70.599988
852.333762	68.846509	70.604993
851.319133	62.009727	70.609998
850.513982	70.419300	70.615002
850.340603	63.794066	70.620007
850.204998	63.274545	70.625012
848.715698	64.931262	70.630017
848.157259	65.495429	70.635022
846.933889	64.961314	70.640026
846.234207	64.416443	70.645031
846.108727	64.979079	70.650036
845.556663	62.496129	70.655041
845.405068	66.732916	70.660046
844.257695	65.761859	70.665050
843.458266	58.708624	70.670055
842.924823	58.766826	70.675060
842.065505	62.629465	70.680065
841.253739	62.695473	70.685070
840.828956	68.737514	70.690074
840.125531	61.748752	70.695079
839.827695	62.075661	70.700084
839.207032	67.228802	70.705089
837.809907	61.746683	70.710094
837.165461	55.466601	70.715098
836.764237	60.270327	70.720103
836.534060	55.225797	70.725108
835.878470	62.858999	70.730113
835.142002	56.150622	70.735118
834.091456	60.587567	70.740122
833.533525	56.990551	70.745127
833.155088	49.088807	70.750132
831.883349	63.090900	70.755137
831.305928	52.740473	70.760142
830.297725	63.307211	70.765146
829.824325	59.842156	70.770151
830.123190	56.583489	70.775156
829.001777	66.401108	70.780161
829.211163	57.807784	70.785166
827.905068	60.172034	70.790170
826.972061	56.938854	70.795175
826.673882	53.795480	70.800180
825.320525	52.880631	70.805185
824.615253	51.358221	70.810190
824.140999	49.048648	70.815194
823.720953	62.298968	70.820199
823.513349	60.495138	70.825204
822.428107	61.437686	70.830209
821.414596	58.073041	70.835214
820.738332	69.272101	70.840218
820.369755	70.612524	70.845223
820.227116	63.726646	70.850228
819.252520	64.504986	70.855233
818.436231	60.153715	70.860238
817.755343	63.972769	70.865242
816.976601	64.379290	70.870247
816.780479	64.503656	70.875252
815.373758	70.528378	70.880257
814.899004	65.312199	70.885262
814.083080	63.898343	70.890266
813.563548	66.989928	70.895271
813.657829	65.969213	70.900276
812.836783	67.576208	70.905281
811.646609	60.883581	70.910286
810.901041	65.701294	70.915290
810.290415	59.098071	70.920295
810.525513	66.471741	70.925300
808.701070	77.954712	70.930305
808.332101	68.824562	70.935310
807.508749	67.284486	70.940314
807.066487	70.401123	70.945319
807.029262	68.276809	70.950324
806.300946	75.386845	70.955329
805.203267	63.709685	70.960334
804.359056	63.623370	70.965338
803.965395	66.494458	70.970343
803.559623	56.898144	70.975348
802.070291	64.822970	70.980353
801.353836	64.855291	70.985358
800.832807	57.397162	70.990362
800.186523	60.540456	70.995367
800.216998	62.691952	71.000372
799.695832	57.216111	71.005377
798.928737	56.750291	71.010382
798.344623	68.209867	71.015386
797.397800	59.432509	71.020391
796.780431	55.634508	71.025396
795.586303	66.438351	71.030401
794.683687	58.205630	71.035406
794.130159	68.318722	71.040410
794.073512	68.511561	71.045415
793.896129	61.038775	71.050420
793.229569	75.873486	71.055425
792.163085	55.028050	71.060430
791.358910	68.715206	71.065434
790.649620	61.013418	71.070439
789.823989	58.222487	71.075444
788.709967	65.267545	71.080449
788.557777	59.134453	71.085454
787.946577	59.389918	71.090458
787.414632	61.612491	71.095463
787.470673	53.182011	71.100468
786.144750	63.845017	71.105473
785.319763	65.421114	71.110478
784.745808	59.865506	71.115482
784.313898	62.104495	71.120487
783.251546	59.938689	71.125492
782.168758	59.543133	71.130497
781.844578	61.235538	71.135502
781.331159	56.895944	71.140506
780.764527	62.307449	71.145511
780.758942	56.901575	71.150516
779.577251	66.159951	71.155521
778.760910	61.599892	71.160526
778.033177	64.299271	71.165530
777.569959	54.466895	71.170535
776.718360	47.752207	71.175540
775.614127	66.072618	71.180545
775.327777	53.020642	71.185550
774.845090	50.816725	71.190554
774.226064	61.874535	71.195559
773.946135	52.209307	71.200564
772.935192	62.586661	71.205569
772.264848	54.873473	71.210574
771.702709	58.830864	71.215578
770.678914	70.278526	71.220583
769.768161	56.627360	71.225588
769.343061	61.633326	71.230593
768.975160	60.422981	71.235598
768.580176	63.081939	71.240602
768.021027	59.065953	71.245607
766.974230	54.235129	71.250612
766.569262	64.465263	71.255617
765.560615	47.132783	71.260622
765.047176	54.076143	71.265626
763.585848	54.163439	71.270631
763.191480	56.068384	71.275636
762.818061	55.513819	71.280641
762.399984	58.994583	71.285646
761.822036	48.420462	71.290650
761.420079	58.692705	71.295655
760.646868	53.825675	71.300660
759.376129	57.514472	71.305665
759.316639	51.816666	71.310670
758.429536	59.211255	71.315674
757.245785	54.678221	71.320679
756.806388	54.526911	71.325684
756.180983	59.174447	71.330689
755.933245	45.905483	71.335694
755.087941	54.585602	71.340698
753.743848	55.013983	71.345703
753.487476	55.476681	71.350708
752.584642	55.137143	71.355713
752.674569	55.516836	71.360718
752.650395	59.858890	71.365722
751.248501	60.698600	71.370727
750.653835	57.171439	71.375732
749.768987	52.123809	71.380737
748.855651	54.293698	71.385742
748.631810	56.954916	71.390746
747.738469	64.952518	71.395751
747.582169	55.609517	71.400756
746.224999	57.920961	71.405761
745.330633	57.596156	71.410766
744.562714	57.123777	71.415770
744.003249	60.056425	71.420775
743.979077	55.146737	71.425780
743.675683	59.793583	71.430785
742.641045	48.177101	71.435790
741.911876	56.654970	71.440794
741.376922	59.058842	71.445799
740.786857	54.882377	71.450804
739.479955	62.987138	71.455809
738.937012	59.086795	71.460814
738.375684	45.082913	71.465818
737.701174	56.589543	71.470823
737.017676	61.125854	71.475828
736.532855	66.334280	71.480833
736.056551	65.314998	71.485838
734.566086	63.822510	71.490842
733.680813	72.730134	71.495847
734.103446	55.589025	71.500852
733.098948	57.747694	71.505857
733.233755	59.682772	71.510862
731.976471	67.409583	71.515866
730.966309	64.655406	71.520871
730.819907	63.662896	71.525876
729.965688	61.258169	71.530881
729.365724	52.273003	71.535886
728.065358	61.296727	71.540890
727.417410	67.278321	71.545895
727.272011	68.390659	71.550900
726.498259	62.960466	71.555905
726.368852	64.532276	71.560910
725.766852	57.927198	71.565914
724.451762	64.368059	71.570919
724.404047	51.142196	71.575924
723.386750	65.778836	71.580929
722.235261	65.234018	71.585934
721.745574	56.803876	71.590938
721.141369	61.766319	71.595943
721.140899	55.452516	71.600948
720.398820	58.931948	71.605953
719.505781	70.142094	71.610958
718.740250	67.748227	71.615962
717.822413	66.603281	71.620967
717.510191	56.706763	71.625972
716.364429	60.248640	71.630977
715.322336	57.194428	71.635982
715.341320	58.075721	71.640986
714.755378	65.476353	71.645991
714.375984	52.254813	71.650996
713.398822	58.600286	71.656001
712.553060	50.906112	71.661006
712.040343	49.587168	71.666010
711.236011	47.244161	71.671015
710.932634	49.698358	71.676020
710.530067	50.932509	71.681025
709.376985	58.154389	71.686030
708.876528	54.437422	71.691034
707.915804	58.759926	71.696039
707.439715	48.121791	71.701044
706.958120	59.420121	71.706049
705.573224	50.730079	71.711054
705.048482	59.378182	71.716058
704.757376	56.121113	71.721063
704.429204	56.112982	71.726068
703.910830	55.437604	71.731073
703.002778	58.640751	71.736078
702.037127	54.314305	71.741082
701.131038	57.211211	71.746087
701.087801	56.028933	71.751092
700.271282	57.993571	71.756097
699.463711	59.996938	71.761102
699.016534	55.845340	71.766106
697.898529	58.201477	71.771111
697.833819	54.816024	71.776116
696.799847	56.347019	71.781121
695.676527	54.795989	71.786126
695.449323	48.822596	71.791130
695.126473	65.703429	71.796135
694.620335	56.823372	71.801140
693.939468	54.728806	71.806145
692.894223	52.708505	71.811150
692.461909	61.605630	71.816154
691.555361	55.139570	71.821159
690.928119	49.648372	71.826164
689.723225	55.237115	71.831169
688.963562	55.323826	71.836174
688.644078	46.296147	71.841178
687.975458	63.471858	71.846183
688.064880	47.601598	71.851188
687.642949	59.277316	71.856193
686.931404	60.927936	71.861198
686.335373	58.506617	71.866202
684.693343	63.678437	71.871207
683.625066	51.771699	71.876212
683.303514	53.773115	71.881217
682.390832	52.169820	71.886222
682.261078	58.899435	71.891226
681.696683	60.188943	71.896231
681.495833	55.319395	71.901236
680.829442	60.233681	71.906241
679.932363	52.455943	71.911246
679.539013	58.886920	71.916250
678.337697	58.849570	71.921255
677.658849	55.960888	71.926260
676.334982	54.368040	71.931265
675.746466	57.820774	71.936270
675.793132	56.069704	71.941274
675.166683	59.834447	71.946279
674.797841	49.087950	71.951284
673.982638	55.110828	71.956289
672.707922	58.845718	71.961294
672.348236	57.468984	71.966298
672.200281	56.812251	71.971303
671.999823	52.008950	71.976308
670.583999	54.576368	71.981313
669.943525	57.428169	71.986318
669.357729	58.479384	71.991322
668.106903	60.479356	71.996327
667.490803	54.955858	72.001332
667.143466	56.833805	72.006337
666.692609	62.804924	72.011342
666.504868	57.152779	72.016346
665.296457	53.849589	72.021351
663.995042	58.013374	72.026356
663.786073	58.480586	72.031361
663.004432	49.183553	72.036366
662.988518	47.216639	72.041370
661.980666	61.576544	72.046375
661.342843	65.442311	72.051380
660.268594	59.501936	72.056385
659.897914	65.978766	72.061390
658.934148	59.070567	72.066394
657.770672	61.884873	72.071399
657.583186	52.806951	72.076404
657.011417	54.374421	72.081409
656.391399	52.353906	72.086414
656.126541	49.083267	72.091418
655.499469	52.770358	72.096423
655.103178	54.654324	72.101428
653.852422	49.301927	72.106433
653.327772	52.652935	72.111438
653.118739	52.593214	72.116442
651.907638	59.371122	72.121447
651.574697	51.381880	72.126452
650.965914	55.278590	72.131457
650.064902	58.915120	72.136462
649.226556	49.528338	72.141466
647.460818	52.211366	72.146471
647.466410	47.888660	72.151476
646.634803	49.371969	72.156481
646.425417	55.809320	72.161486
645.964366	45.228226	72.166490
645.394291	47.341296	72.171495
645.376999	46.500741	72.176500
644.927855	45.616941	72.181505
644.103363	48.075952	72.186510
643.304179	51.261638	72.191514
641.739814	55.197729	72.196519
641.310068	51.385373	72.201524
640.539038	57.271221	72.206529
640.260006	57.023767	72.211534
639.338417	55.906716	72.216538
638.038099	60.946587	72.221543
637.762639	50.951424	72.226548
637.080041	59.447768	72.231553
637.064644	55.816644	72.236558
636.943094	53.380750	72.241562
635.304619	56.908773	72.246567
634.521079	48.671490	72.251572
634.142347	41.544264	72.256577
633.532449	53.249417	72.261582
633.149922	44.882250	72.266586
631.804320	57.030408	72.271591
631.203157	50.931232	72.276596
630.659308	47.218554	72.281601
630.109960	40.187268	72.286606
629.870733	44.199073	72.291610
628.666499	43.786467	72.296615
627.992124	45.823466	72.301620
627.573928	47.310155	72.306625
626.813742	47.546168	72.311630
626.616316	51.409900	72.316634
625.318931	49.574518	72.321639
624.425640	42.673997	72.326644
624.242650	50.470167	72.331649
623.589362	52.654336	72.336654
623.525070	47.311030	72.341658
622.273279	55.923048	72.346663
621.786025	41.575738	72.351668
620.957041	45.375972	72.356673
620.262756	40.891353	72.361678
619.865318	44.550943	72.366682
619.040114	52.443330	72.371687
617.930523	45.062398	72.376692
617.828017	47.388240	72.381697
616.999555	50.826433	72.386702
616.365763	44.168017	72.391706
615.648422	61.060374	72.396711
615.033765	51.458048	72.401716
614.488960	50.234609	72.406721
613.641962	53.088248	72.411726
612.975535	44.534871	72.416730
612.203748	54.325369	72.421735
611.298665	49.719769	72.426740
611.252191	53.636186	72.431745
610.325045	49.272774	72.436750
609.478768	49.696820	72.441754
608.789553	60.344705	72.446759
608.496491	53.460154	72.451764
608.005866	51.512209	72.456769
607.175251	50.165644	72.461774
606.358588	43.356992	72.466778
605.398521	54.273110	72.471783
605.039017	53.712227	72.476788
604.904954	42.781057	72.481793
603.561475	47.856351	72.486798
602.883254	53.292113	72.491802
602.011225	57.908894	72.496807
601.460495	52.784318	72.501812
601.322189	53.028253	72.506817
601.021349	57.787156	72.511822
599.879843	47.417782	72.516826
598.948875	58.419307	72.521831
598.780545	53.685109	72.526836
598.067390	51.723979	72.531841
596.948876	49.060634	72.536846
596.217028	46.662206	72.541850
595.660625	59.644179	72.546855
595.646551	52.408294	72.551860
595.258306	52.429014	72.556865
593.894915	50.091821	72.561870
593.249049	51.324642	72.566874
592.565110	55.036877	72.571879
591.264974	59.918446	72.576884
590.425071	57.894959	72.581889
590.371374	54.199746	72.586894
590.114630	49.473199	72.591898
588.982705	56.196106	72.596903
588.546455	51.262696	72.601908
588.256074	49.850413	72.606913
587.197514	58.741945	72.611918
586.313049	52.343969	72.616922
585.989989	61.394468	72.621927
585.340614	53.522607	72.626932
584.920449	51.875996	72.631937
583.915862	51.828646	72.636942
583.013192	49.088851	72.641946
582.640495	56.773850	72.646951
582.405828	49.152234	72.651956
581.825783	47.232245	72.656961
580.486701	59.409293	72.661966
579.810886	50.725694	72.666970
579.204329	53.229474	72.671975
578.680892	51.378729	72.676980
577.715574	51.912776	72.681985
577.283562	54.180609	72.686990
576.571310	49.536847	72.691994
576.192617	56.281479	72.696999
575.329301	53.439421	72.702004
574.441340	52.427142	72.707009
573.569104	57.890625	72.712014
573.285580	54.563984	72.717018
572.664009	50.679905	72.722023
572.384717	54.442407	72.727028
571.888660	54.770534	72.732033
570.585493	54.829999	72.737038
570.011453	48.129381	72.742042
569.310975	52.608224	72.747047
568.912835	44.244928	72.752052
568.057204	38.572639	72.757057
566.863614	45.970810	72.762062
566.441397	43.481837	72.767066
566.002552	47.064846	72.772071
565.639351	50.057821	72.777076
565.663066	45.272567	72.782081
564.255383	54.626133	72.787086
563.773552	41.870583	72.792090
563.230690	54.253816	72.797095
561.830717	55.892548	72.802100
561.252353	57.795086	72.807105
560.551896	66.071482	72.812110
560.425704	49.616507	72.817114
559.335411	60.155889	72.822119
558.069607	56.615867	72.827124
558.147961	61.685568	72.832129
557.240755	54.287734	72.837134
556.834316	48.255862	72.842138
556.057073	58.323996	72.847143
556.065975	52.359896	72.852148
555.449215	50.357785	72.857153
554.571074	56.552898	72.862158
554.105796	51.779195	72.867162
552.542717	61.224916	72.872167
551.840852	61.322271	72.877172
551.382659	55.708189	72.882177
550.993806	55.592051	72.887182
550.687687	54.979001	72.892186
549.431460	53.652876	72.897191
548.548685	50.844946	72.902196
548.400867	51.985725	72.907201
547.636266	48.097344	72.912206
547.367579	53.848575	72.917210
546.186676	56.295253	72.922215
545.336260	49.394903	72.927220
545.227848	57.197636	72.932225
544.518559	55.490049	72.937230
544.138511	51.456438	72.942234
542.935446	53.288791	72.947239
542.276396	55.497245	72.952244
541.872279	49.213148	72.957249
540.976122	58.784188	72.962254
540.267845	55.409942	72.967258
539.546260	53.724988	72.972263
538.954905	62.004004	72.977268
538.487209	57.422547	72.982273
537.536736	52.909210	72.987278
536.880306	54.230686	72.992282
535.951339	54.584444	72.997287
535.360110	59.798478	73.002292
535.277548	56.721206	73.007297
534.228499	56.018758	73.012302
534.006618	47.601977	73.017306
532.349741	49.763524	73.022311
531.770702	57.254551	73.027316
531.571520	50.921131	73.032321
530.768599	48.326484	73.037326
530.463087	46.284070	73.042330
529.967811	54.122301	73.047335
529.798329	56.298183	73.052340
529.057399	45.748493	73.057345
527.826134	50.937991	73.062350
527.426943	49.130696	73.067354
526.338646	48.036314	73.072359
525.235511	44.851304	73.077364
524.807164	49.954140	73.082369
524.327249	52.535694	73.087374
524.235584	57.314410	73.092378
524.190556	55.377749	73.097383
523.055911	47.096452	73.102388
521.873172	45.821686	73.107393
520.366172	51.141323	73.112398
519.995957	52.852680	73.117402
519.618128	57.908182	73.122407
519.024183	50.450368	73.127412
518.596459	45.151582	73.132417
517.908169	52.437524	73.137422
517.599244	47.568751	73.142426
516.495558	54.138418	73.147431
515.508993	49.222742	73.152436
514.798890	42.503611	73.157441
514.229673	53.351973	73.162446
514.350191	44.471154	73.167450
513.760994	49.927981	73.172455
512.776576	53.028591	73.177460
511.993721	51.648992	73.182465
511.596973	54.548251	73.187470
510.625070	47.701489	73.192474
509.889001	52.240907	73.197479
509.328676	55.424760	73.202484
508.894859	48.952349	73.207489
508.010345	59.126493	73.212494
506.744106	53.429051	73.217498
506.278032	51.501779	73.222503
505.881964	50.176687	73.227508
505.345991	48.451645	73.232513
504.741122	56.172480	73.237518
504.400794	46.707507	73.242522
503.362551	52.241677	73.247527
502.523294	54.933752	73.252532
502.157921	45.348737	73.257537
501.626303	52.946104	73.262542
500.787233	58.259448	73.267546
499.990055	53.599858	73.272551
499.098475	58.324207	73.277556
498.955943	58.586237	73.282561
498.053634	59.814069	73.287566
497.630926	48.921320	73.292570
496.175866	51.197104	73.297575
495.598585	61.984488	73.302580
495.490281	56.012055	73.307585
494.753930	49.829894	73.312590
494.482502	55.998020	73.317594
493.775402	57.389365	73.322599
493.097912	59.381129	73.327604
492.764438	48.399673	73.332609
490.927776	49.663278	73.337614
490.324900	46.728457	73.342618
489.865958	48.357130	73.347623
489.326994	56.217849	73.352628
488.985773	48.953959	73.357633
488.301189	61.079655	73.362638
487.943410	62.843750	73.367642
486.619704	60.265327	73.372647
485.819397	52.092134	73.377652
485.727295	46.156401	73.382657
484.931598	61.685023	73.387662
484.220484	61.826602	73.392666
482.895525	57.011548	73.397671
482.446131	60.746363	73.402676
482.557391	49.799614	73.407681
481.494778	56.790909	73.412686
481.559542	57.500153	73.417690
480.167676	58.194939	73.422695
479.516807	60.569753	73.427700
479.504298	60.137303	73.432705
477.803025	70.588382	73.437710
477.328071	63.597258	73.442714
476.683238	61.179202	73.447719
475.906954	65.185154	73.452724
475.712786	62.918017	73.457729
475.708200	68.149550	73.462734
474.882663	65.752197	73.467738
473.689566	70.543615	73.472743
472.820894	55.214513	73.477748
472.146168	55.870881	73.482753
470.579256	58.967111	73.487758
470.961580	58.929213	73.492762
470.191508	64.803864	73.497767
469.355388	62.178207	73.502772
469.195591	52.817688	73.507777
468.720606	72.251927	73.512782
468.033832	60.668678	73.517786
466.736011	66.959406	73.522791
466.242227	64.132594	73.527796
466.372733	59.986634	73.532801
465.486010	65.959034	73.537806
464.527605	52.539551	73.542810
464.094044	57.250545	73.547815
462.918296	58.190128	73.552820
462.259187	63.348303	73.557825
461.318027	63.819027	73.562830
461.057572	62.433201	73.567834
460.605645	62.542210	73.572839
459.840532	61.131555	73.577844
458.934431	57.327039	73.582849
457.856954	55.735058	73.587854
457.647765	56.824780	73.592858
456.861860	56.582096	73.597863
456.352922	62.142804	73.602868
456.311498	54.610843	73.607873
455.100993	58.022560	73.612878
454.594972	56.599479	73.617882
453.870721	67.355608	73.622887
453.215750	64.528790	73.627892
452.920346	63.435516	73.632897
451.234462	57.542782	73.637902
450.718448	50.722117	73.642906
450.625222	57.439540	73.647911
449.716138	60.154247	73.652916
450.082973	57.498887	73.657921
448.200254	68.995087	73.662926
447.976695	58.790148	73.667930
447.334592	59.144893	73.672935
446.569644	75.236648	73.677940
445.860583	59.654422	73.682945
444.829668	72.911917	73.687950
444.480854	60.423307	73.692954
444.121307	61.949694	73.697959
443.403015	67.595619	73.702964
442.570946	63.682898	73.707969
441.792888	68.674761	73.712974
441.305507	64.282207	73.717978
440.524065	62.365961	73.722983
440.223167	73.805819	73.727988
439.310113	69.608176	73.732993
438.567074	66.047284	73.737998
437.744267	63.712230	73.743002
437.345724	57.860587	73.748007
436.578456	68.861708	73.753012
436.154516	56.851346	73.758017
434.879570	55.656347	73.763022
434.555967	58.635045	73.768026
433.836373	51.698488	73.773031
433.182330	58.660036	73.778036
433.124780	51.482928	73.783041
431.998379	59.223278	73.788046
431.169724	54.072152	73.793050
430.647270	63.201816	73.798055
430.037791	62.716546	73.803060
429.804612	48.174959	73.808065
428.699405	60.448127	73.813070
428.044792	65.410547	73.818074
427.441744	57.603013	73.823079
426.784164	59.199421	73.828084
426.142072	54.514850	73.833089
424.921330	56.246844	73.838094
424.787564	55.039826	73.843098
424.338291	53.035083	73.848103
423.976596	51.776341	73.853108
422.709332	50.154922	73.858113
422.132666	60.691557	73.863118
421.670378	53.046999	73.868122
421.183554	51.265785	73.873127
419.734360	61.828007	73.878132
419.014213	53.734245	73.883137
418.630293	56.460795	73.888142
418.379722	58.661626	73.893146
418.089471	60.287449	73.898151
416.416119	49.561282	73.903156
416.386431	54.771452	73.908161
415.276249	60.418619	73.913166
414.691373	55.330714	73.918170
414.388918	46.716192	73.923175
413.440869	62.347498	73.928180
412.840511	61.298200	73.933185
412.117955	58.664935	73.938190
411.839942	55.412361	73.943194
411.114814	62.461878	73.948199
409.904963	61.337436	73.953204
409.361545	58.650974	73.958209
409.071178	67.541535	73.963214
408.578412	57.796793	73.968218
407.922919	61.155640	73.973223
406.669453	59.676326	73.978228
406.478268	57.181328	73.983233
405.473981	55.968767	73.988238
404.357081	53.433478	73.993242
403.824188	58.749622	73.998247
403.311290	59.302086	74.003252
403.086690	54.457556	74.008257
402.662598	61.264836	74.013262
401.931377	56.410422	74.018266
400.804997	61.369224	74.023271
399.977092	58.517976	74.028276
399.545020	61.211729	74.033281
398.957782	54.325914	74.038286
398.889112	50.529863	74.043290
397.979448	51.314920	74.048295
396.280919	53.178142	74.053300
396.236336	52.383711	74.058305
395.998405	58.921074	74.063310
395.360208	59.583428	74.068314
394.539540	52.228044	74.073319
393.222790	58.638468	74.078324
393.036522	49.517747	74.083329
392.690485	60.274579	74.088334
391.458677	62.588709	74.093338
390.644328	50.182270	74.098343
390.026608	62.393213	74.103348
389.589717	56.211855	74.108353
389.452389	57.874230	74.113358
389.085073	67.488069	74.118362
388.252529	60.350626	74.123367
387.255334	64.444971	74.128372
387.022714	60.225069	74.133377
385.283244	62.310826	74.138382
384.823566	62.097504	74.143386
384.053938	54.542727	74.148391
383.562462	57.720712	74.153396
383.490852	55.981626	74.158401
382.735372	55.734530	74.163406
381.530458	52.082291	74.168410
380.889090	52.814660	74.173415
380.341352	56.650013	74.178420
380.036561	48.615336	74.183425
379.363541	52.682542	74.188430
378.251976	54.356365	74.193434
377.805226	54.327923	74.198439
377.497563	61.407339	74.203444
376.621864	50.871705	74.208449
376.055504	58.862642	74.213454
375.239299	60.934637	74.218458
374.286172	57.607911	74.223463
373.525147	62.130703	74.228468
373.452175	55.396348	74.233473
372.825524	62.287289	74.238478
371.862131	60.569598	74.243482
371.216955	58.294505	74.248487
370.499939	64.381902	74.253492
369.640805	47.421435	74.258497
369.628900	57.162240	74.263502
368.344531	54.442121	74.268506
367.810948	57.114590	74.273511
366.860826	60.853522	74.278516
366.476340	57.225275	74.283521
366.157802	58.337688	74.288526
365.994653	64.477391	74.293530
364.620923	58.823678	74.298535
363.667332	64.312184	74.303540
363.456157	61.517078	74.308545
362.825351	52.283874	74.313550
361.810876	58.701707	74.318554
360.903378	55.853846	74.323559
360.543330	61.286809	74.328564
360.212055	53.784798	74.333569
360.245641	57.844584	74.338574
359.004794	63.443502	74.343578
358.344214	61.305253	74.348583
357.690888	66.317982	74.353588
356.552539	51.316970	74.358593
355.520717	59.031649	74.363598
355.028044	67.355731	74.368602
354.862130	54.907242	74.373607
353.942506	63.584742	74.378612
353.534542	50.789736	74.383617
352.682737	60.412398	74.388622
351.580222	65.163053	74.393626
351.531234	63.355356	74.398631
350.903080	64.133620	74.403636
350.387195	54.036428	74.408641
349.378630	61.078083	74.413646
348.492978	59.576007	74.418650
347.862150	58.323926	74.423655
347.478621	64.544817	74.428660
347.282147	55.717148	74.433665
346.457034	59.290192	74.438670
345.352934	65.538665	74.443674
345.036987	57.325910	74.448679
344.551035	67.548205	74.453684
343.513167	58.367399	74.458689
342.389524	56.857959	74.463694
341.612438	65.220128	74.468698
341.210228	52.739119	74.473703
340.713607	67.747174	74.478708
340.719287	46.992130	74.483713
339.754414	58.054744	74.488718
338.509310	62.620245	74.493722
338.646902	51.288887	74.498727
337.958806	58.698751	74.503732
336.905285	62.541852	74.508737
336.132914	64.759095	74.513742
335.378381	61.942651	74.518746
335.173324	58.596663	74.523751
334.102146	66.107711	74.528756
333.373156	50.924055	74.533761
333.361204	49.823261	74.538766
331.983713	58.602128	74.543770
331.712024	53.665023	74.548775
331.158305	62.781889	74.553780
330.265268	59.609075	74.558785
328.969507	56.292139	74.563790
328.717738	62.585573	74.568794
328.524899	53.257577	74.573799
327.712804	57.783205	74.578804
327.623520	49.796068	74.583809
326.132983	60.290002	74.588814
325.394447	61.387170	74.593818
324.954468	49.056317	74.598823
324.686992	67.282274	74.603828
323.774741	60.373628	74.608833
323.127472	63.142951	74.613838
322.190957	58.025336	74.618842
321.859100	51.034192	74.623847
321.121335	67.359685	74.628852
320.258569	62.853076	74.633857
319.522061	68.135841	74.638862
319.188656	62.696184	74.643866
318.958895	64.552814	74.648871
317.772639	57.368652	74.653876
317.409110	51.038162	74.658881
316.605856	53.800669	74.663886
315.331358	55.970957	74.668890
314.349505	48.359027	74.673895
314.427816	54.927048	74.678900
313.881399	57.715794	74.683905
313.219228	56.480537	74.688910
312.467483	60.341783	74.693914
312.351905	57.223210	74.698919
310.964759	59.054802	74.703924
310.450725	59.333144	74.708929
309.969581	62.573309	74.713934
309.236475	63.568896	74.718938
308.541756	56.313517	74.723943
307.551253	62.668043	74.728948
307.026933	62.498965	74.733953
307.003562	58.323727	74.738958
306.130704	70.337631	74.743962
305.147876	60.911759	74.748967
304.259827	62.097315	74.753972
303.768794	53.068313	74.758977
303.517336	58.304648	74.763982
302.534712	53.085211	74.768986
301.387171	53.200573	74.773991
300.708827	55.521302	74.778996
300.421596	53.026196	74.784001
300.182774	56.773873	74.789006
299.157337	63.339245	74.794010
298.985322	55.725478	74.799015
297.668925	62.203359	74.804020
296.804834	52.980551	74.809025
296.290848	58.060973	74.814030
295.767667	61.352156	74.819034
295.663781	53.853021	74.824039
294.926392	56.615689	74.829044
294.248442	58.858593	74.834049
293.520920	58.393180	74.839054
293.075776	60.430403	74.844058
291.899545	61.107625	74.849063
290.787148	57.019184	74.854068
290.176968	55.124532	74.859073
290.477614	58.387399	74.864078
289.853840	58.156821	74.869082
289.061193	58.677119	74.874087
287.600346	63.831814	74.879092
287.199173	55.104762	74.884097
286.765251	61.183114	74.889102
285.988111	54.756556	74.894106
285.503770	48.180742	74.899111
284.586888	59.029096	74.904116
283.934004	52.075220	74.909121
283.341275	50.889246	74.914126
282.775345	62.693047	74.919130
282.840737	48.700280	74.924135
281.664762	68.508049	74.929140
280.813882	54.311954	74.934145
279.957776	53.814901	74.939150
278.899709	54.965660	74.944154
278.600944	55.882858	74.949159
278.114937	53.307357	74.954164
277.326444	54.193239	74.959169
276.794310	57.335177	74.964174
276.310268	59.171054	74.969178
275.645271	56.336513	74.974183
275.104180	55.089586	74.979188
274.640610	49.818689	74.984193
273.598292	49.296717	74.989198
271.809245	53.763238	74.994202
271.858424	55.184843	74.999207
271.116658	66.977736	75.004212
270.645031	60.936156	75.009217
270.574820	56.665535	75.014222
269.824168	53.532274	75.019226
269.648789	52.183588	75.024231
268.244970	61.501029	75.029236
267.738226	51.885025	75.034241
266.434441	45.064037	75.039246
265.610355	61.455237	75.044250
265.250357	58.121208	75.049255
264.457974	60.818311	75.054260
264.228971	54.896191	75.059265
263.692653	54.973107	75.064270
262.865070	61.441021	75.069274
262.889931	52.219791	75.074279
261.721759	51.902540	75.079284
261.160299	48.535549	75.084289
260.627536	46.127530	75.089294
259.188713	58.217912	75.094298
258.850868	44.440708	75.099303
258.338966	52.628351	75.104308
257.569631	53.017956	75.109313
257.447544	56.607869	75.114318
256.669225	49.278813	75.119322
256.244688	52.159165	75.124327
255.356639	56.449152	75.129332
254.325390	47.189883	75.134337
253.786391	51.215972	75.139342
252.830217	52.706487	75.144346
252.573706	49.023953	75.149351
251.337562	53.463600	75.154356
250.496432	57.285309	75.159361
250.494157	55.488161	75.164366
249.914314	55.323870	75.169370
249.530997	56.412264	75.174375
248.492933	49.510999	75.179380
247.265507	52.176100	75.184385
246.625327	53.294312	75.189390
246.282867	55.692862	75.194394
245.949643	51.155502	75.199399
245.255654	52.801986	75.204404
245.138230	62.174049	75.209409
243.847590	47.563117	75.214414
242.881986	54.761225	75.219418
242.507116	49.651566	75.224423
241.045783	59.017157	75.229428
240.609498	56.496292	75.234433
240.561204	53.846558	75.239438
239.491491	52.150674	75.244442
238.865035	57.381818	75.249447
238.497716	59.771209	75.254452
238.183916	47.160211	75.259457
237.455386	51.303258	75.264462
236.269398	53.056576	75.269466
236.197804	49.458392	75.274471
235.357043	52.671391	75.279476
234.690156	47.323648	75.284481
234.017299	47.337530	75.289486
232.979515	51.059141	75.294490
232.751933	45.936079	75.299495
232.090965	47.193638	75.304500
231.275419	43.831130	75.309505
230.370153	51.782666	75.314510
229.416435	55.360403	75.319514
229.580492	43.264701	75.324519
229.047073	53.386180	75.329524
227.550579	49.472935	75.334529
227.183372	45.152181	75.339534
226.082587	49.438770	75.344538
226.135590	50.822615	75.349543
225.584231	58.307726	75.354548
224.498913	52.326354	75.359553
224.230905	47.041285	75.364558
223.074730	56.527850	75.369562
223.010554	49.076783	75.374567
221.971407	57.850566	75.379572
221.081102	57.482932	75.384577
220.627503	57.853156	75.389582
219.638939	53.842188	75.394586
219.765789	49.509768	75.399591
218.950922	49.696012	75.404596
217.658302	49.768766	75.409601
216.937124	48.675869	75.414606
216.390426	50.745897	75.419610
216.350283	38.322857	75.424615
215.705817	47.711045	75.429620
214.848033	44.628133	75.434625
213.997848	43.670632	75.439630
213.529323	53.533108	75.444634
212.857814	49.061635	75.449639
211.943299	55.293417	75.454644
210.661270	48.858694	75.459649
210.459562	52.370286	75.464654
209.885252	54.288348	75.469658
209.682161	49.311475	75.474663
209.523136	58.560013	75.479668
208.238894	54.864980	75.484673
207.533582	51.442529	75.489678
206.746772	56.035281	75.494682
206.526018	46.391584	75.499687
205.195492	46.301508	75.504692
205.032303	52.081623	75.509697
204.537645	49.133033	75.514702
203.608199	52.072704	75.519706
202.353806	49.084620	75.524711
201.581614	49.365782	75.529716
201.177105	50.808711	75.534721
200.812528	46.116875	75.539726
200.068344	56.092128	75.544730
199.980175	44.755279	75.549735
198.871329	49.809393	75.554740
198.280306	48.722211	75.559745
197.716408	45.990743	75.564750
196.907810	50.946812	75.569754
196.951111	48.735299	75.574759
195.679491	51.875723	75.579764
194.894205	43.173883	75.584769
194.449032	47.399800	75.589774
192.998178	53.683656	75.594778
192.525115	50.140480	75.599783
191.986620	55.775339	75.604788
191.206146	47.024123	75.609793
191.059307	51.785049	75.614798
190.539159	58.491962	75.619802
189.983780	50.909587	75.624807
188.777547	61.856890	75.629812
188.236850	52.241591	75.634817
187.765012	51.833018	75.639822
187.169778	55.421148	75.644826
186.744202	57.244246	75.649831
186.073511	51.049320	75.654836
185.190318	57.340469	75.659841
184.344156	49.544668	75.664846
183.235320	52.165773	75.669850
182.707896	49.247669	75.674855
181.975772	55.337669	75.679860
181.624197	49.127512	75.684865
181.721271	48.818376	75.689870
180.388907	58.054115	75.694874
179.370277	46.066424	75.699879
178.858020	46.162119	75.704884
178.600167	47.405446	75.709889
178.252124	45.154842	75.714894
176.757462	52.596799	75.719898
176.183114	45.119912	75.724903
175.385779	50.478634	75.729908
175.071994	44.755788	75.734913
174.774181	42.093966	75.739918
173.291502	49.865033	75.744922
172.659438	50.964101	75.749927
172.022472	56.447299	75.754932
171.466448	64.043339	75.759937
171.155260	46.700085	75.764942
170.680406	43.074726	75.769946
170.551013	44.678114	75.774951
169.555942	43.100104	75.779956
168.767872	56.274530	75.784961
167.998963	49.080059	75.789966
166.630937	48.692099	75.794970
166.073813	41.786964	75.799975
165.465762	48.550783	75.804980
164.864206	53.815949	75.809985
164.786488	49.762137	75.814990
164.056870	53.130951	75.819994
163.401699	47.283481	75.824999
162.436756	43.571621	75.830004
161.466435	51.702859	75.835009
161.562621	53.365073	75.840014
160.639864	55.334189	75.845018
160.389663	50.155409	75.850023
159.086806	51.005546	75.855028
158.595102	48.108163	75.860033
158.387107	46.324575	75.865038
157.198763	59.035549	75.870042
156.706880	51.607680	75.875047
155.674643	51.951190	75.880052
155.464209	54.188566	75.885057
155.067173	50.725515	75.890062
153.947067	54.832284	75.895066
153.109407	49.137276	75.900071
153.119855	51.633215	75.905076
151.865043	57.528629	75.910081
150.970540	54.122833	75.915086
150.064258	60.075729	75.920090
149.914382	47.684528	75.925095
149.580053	46.385201	75.930100
148.684290	50.679682	75.935105
148.540599	49.761333	75.940110
147.092027	53.647718	75.945114
146.607355	55.058607	75.950119
146.193592	55.806854	75.955124
145.001922	46.748007	75.960129
144.328569	46.756066	75.965134
143.711698	51.928338	75.970138
143.414401	41.670972	75.975143
142.894994	39.455275	75.980148
142.487833	50.734115	75.985153
141.725960	50.050024	75.990158
140.461637	59.738683	75.995162
139.853174	44.176825	76.000167
139.374255	47.481349	76.005172
138.780146	49.774237	76.010177
138.246596	47.364791	76.015182
137.102723	55.905500	76.020186
136.837172	53.836140	76.025191
136.378873	46.430939	76.030196
135.294356	48.740007	76.035201
134.934462	46.300792	76.040206
133.798375	57.023719	76.045210
133.557204	49.764835	76.050215
132.959443	51.368787	76.055220
132.444976	52.135482	76.060225
131.382112	47.641517	76.065230
130.339211	52.989057	76.070234
129.808924	36.858051	76.075239
129.292102	48.098850	76.080244
129.079122	48.312181	76.085249
128.694056	44.276327	76.090254
127.008427	49.472357	76.095258
126.831095	42.646191	76.100263
126.270600	43.767336	76.105268
125.657268	49.764741	76.110273
125.119018	42.034587	76.115278
124.128007	44.158690	76.120282
123.766771	52.765348	76.125287
123.417959	47.679263	76.130292
122.319125	56.252909	76.135297
121.563296	50.553353	76.140302
120.672952	55.350168	76.145306
120.469549	55.334108	76.150311
119.641181	55.521894	76.155316
118.586280	49.821903	76.160321
118.154967	53.058667	76.165326
117.106953	50.883860	76.170330
116.958821	53.208050	76.175335
116.602709	51.669317	76.180340
116.209990	63.919841	76.185345
115.176147	55.840066	76.190350
114.112246	59.651831	76.195354
113.643021	63.602817	76.200359
112.977968	56.508965	76.205364
111.826983	58.123294	76.210369
111.158049	50.827623	76.215374
110.508331	62.989187	76.220378
110.232648	56.937726	76.225383
110.003752	59.181427	76.230388
109.323809	51.586872	76.235393
109.349945	58.199740	76.240398
108.012503	56.411638	76.245402
107.178373	52.756701	76.250407
106.366023	48.644900	76.255412
105.333985	55.552067	76.260417
105.252371	46.383843	76.265422
104.109898	51.208096	76.270426
103.920062	46.854582	76.275431
103.253509	49.621706	76.280436
102.057867	61.134407	76.285441
101.668680	50.132580	76.290446
100.996039	52.520640	76.295450
100.893348	55.737381	76.300455
100.303540	55.077873	76.305460
98.891780	48.515045	76.310465
98.584685	55.466865	76.315470
97.838335	62.808975	76.320474
97.448967	56.262696	76.325479
96.406944	57.061422	76.330484
95.280403	54.180916	76.335489
94.998179	55.994444	76.340494
94.603449	54.056569	76.345498
94.177553	51.096995	76.350503
92.833899	54.251372	76.355508
92.016431	59.599744	76.360513
91.676254	53.868009	76.365518
91.255528	52.221547	76.370522
90.942683	51.398513	76.375527
90.508604	58.286846	76.380532
89.329622	59.595736	76.385537
88.955968	51.065702	76.390542
87.400343	61.484798	76.395546
86.461975	59.658677	76.400551
86.484184	52.662520	76.405556
85.344018	50.971649	76.410561
85.072648	48.544103	76.415566
84.827796	48.409237	76.420570
84.315369	49.346104	76.425575
83.704413	56.614476	76.430580
82.686257	57.275306	76.435585
81.953789	52.983246	76.440590
81.020357	61.189880	76.445594
80.356000	53.872115	76.450599
80.413506	51.248851	76.455604
79.018791	58.530814	76.460609
78.632423	63.528584	76.465614
78.146856	57.448773	76.470618
77.708481	57.272880	76.475623
76.898313	51.989993	76.480628
76.132769	60.349806	76.485633
75.131190	53.748633	76.490638
75.054967	55.987079	76.495642
73.544088	51.041814	76.500647
72.837341	57.354038	76.505652
72.463285	64.551407	76.510657
72.214011	48.708523	76.515662
71.698000	53.367750	76.520666
71.082063	55.270464	76.525671
69.930782	53.427960	76.530676
69.132775	57.658328	76.535681
68.640871	46.318090	76.540686
68.167968	51.861582	76.545690
67.509407	52.021448	76.550695
66.655643	51.490484	76.555700
65.900293	60.978218	76.560705
65.654441	44.771616	76.565710
65.065475	51.191928	76.570714
64.581855	55.520754	76.575719
63.716232	53.910706	76.580724
62.313986	55.018290	76.585729
62.188169	48.279606	76.590734
61.488799	51.978358	76.595738
60.279094	55.748423	76.600743
59.834643	60.681946	76.605748
58.911657	54.522802	76.610753
58.606725	51.413422	76.615758
58.253843	50.451210	76.620762
57.901665	62.522685	76.625767
57.644249	57.767494	76.630772
56.251457	64.974929	76.635777
55.829974	56.115224	76.640782
55.237378	56.708229	76.645786
53.988222	58.788191	76.650791
53.579225	51.687557	76.655796
52.911442	54.208204	76.660801
52.146720	49.305140	76.665806
50.930884	46.920322	76.670810
50.617106	51.627767	76.675815
50.134368	54.040508	76.680820
49.606273	61.244944	76.685825
49.221492	52.400265	76.690830
48.516870	54.522648	76.695834
47.774735	50.355404	76.700839
46.879399	54.796265	76.705844
46.331555	56.527449	76.710849
46.259184	53.429510	76.715854
44.995973	47.420672	76.720858
43.935553	56.062738	76.725863
43.447428	52.084824	76.730868
42.714532	50.776477	76.735873
42.610113	55.862082	76.740878
41.996877	59.116228	76.745882
40.876687	59.807981	76.750887
40.312916	58.142631	76.755892
39.605447	57.423179	76.760897
39.625742	62.612526	76.765902
38.399497	63.794935	76.770906
37.351599	62.177856	76.775911
37.144092	57.953287	76.780916
36.489295	64.126356	76.785921
35.448609	52.719957	76.790926
34.462016	60.300618	76.795930
34.028678	56.666183	76.800935
33.753922	61.254448	76.805940
33.043386	58.813390	76.810945
32.972360	55.608648	76.815950
32.194094	60.305740	76.820954
31.087167	58.141449	76.825959
30.595972	56.948365	76.830964
29.915907	59.146667	76.835969
28.894230	48.958256	76.840974
28.129429	60.837990	76.845978
27.462726	56.743072	76.850983
27.309594	64.034791	76.855988
26.391085	65.455737	76.860993
26.158271	53.615582	76.865998
24.934458	48.535464	76.871002
23.898023	53.864547	76.876007
23.813977	53.089519	76.881012
23.329913	57.143310	76.886017
23.086866	61.936520	76.891022
21.595523	61.401204	76.896026
21.113836	56.736967	76.901031
20.608539	53.242760	76.906036
19.884953	64.408501	76.911041
19.240690	56.962574	76.916046
18.173675	61.096582	76.921050
17.570723	57.870155	76.926055
17.189555	47.826912	76.931060
16.523422	60.876235	76.936065
16.423029	59.082889	76.941070
15.836682	58.742122	76.946074
14.257695	59.413868	76.951079
13.849031	55.797704	76.956084
13.266913	63.801620	76.961089
12.955064	51.750428	76.966094
11.605031	59.115529	76.971098
11.377438	56.696664	76.976103
10.989166	53.753937	76.981108
9.875266	60.278075	76.986113
8.519310	43.653180	76.991118
8.013883	52.746766	76.996122
7.348141	56.446864	77.001127
7.595954	57.634285	77.006132
7.141828	52.761260	77.011137
6.835823	55.741297	77.016142
5.527660	57.726789	77.021147
4.759755	51.718296	77.026151
4.272808	47.245217	77.031156
3.515905	58.694150	77.036161