Thu Jun 16 17:58:34 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.533470	129.154052	0.000000
0.633203	110.571891	0.005005
0.575396	112.793346	0.010010
0.808019	103.737318	0.015014
0.775741	112.898199	0.020019
0.566627	101.592699	0.025024
0.689994	88.356508	0.030029
0.169819	80.664815	0.035034
0.052536	58.789717	0.040038
-0.278908	50.991082	0.045043
-1.085101	48.857806	0.050048
-0.536561	33.290001	0.055053
-1.252926	22.982535	0.060058
-1.424374	20.011055	0.065062
-1.856358	7.273469	0.070067
-2.297831	7.319317	0.075072
-2.178236	-5.309832	0.080077
-2.947773	-14.478481	0.085082
-3.212268	-8.220915	0.090086
-3.343959	-5.710243	0.095091
-3.708940	-11.174237	0.100096
-3.851878	-15.548669	0.105101
-4.703409	-12.446180	0.110106
-4.883917	-9.341327	0.115110
-5.112169	-2.802857	0.120115
-5.158917	-12.231935	0.125120
-4.828036	-7.157579	0.130125
-5.031492	-15.221406	0.135130
-5.935604	-10.280655	0.140134
-6.423904	-6.899014	0.145139
-6.753289	2.938549	0.150144
-6.668260	-7.726565	0.155149
-6.556888	-9.177137	0.160154
-6.487630	-16.681666	0.165158
-6.779938	-21.231584	0.170163
-7.668094	-15.250779	0.175168
-7.785156	-20.862387	0.180173
-8.270102	-11.069762	0.185178
-8.353376	-22.894374	0.190182
-8.127092	-15.345518	0.195187
-9.448538	-10.644690	0.200192
-9.469696	-16.097725	0.205197
-9.452784	-21.172687	0.210202
-9.581718	-25.702841	0.215206
-9.803385	-17.647845	0.220211
-9.831910	-18.636673	0.225216
-9.512123	-18.460817	0.230221
-10.257456	-8.105638	0.235226
-10.911315	-20.224758	0.240230
-10.955743	-18.172558	0.245235
-11.174676	-2.774467	0.250240
-11.507670	-22.226129	0.255245
-12.440702	-6.590852	0.260250
-12.859920	-13.425582	0.265254
-12.463931	-18.660269	0.270259
-12.470513	-14.615657	0.275264
-12.613762	-20.101097	0.280269
-13.052903	-13.337868	0.285274
-12.657601	-14.342873	0.290278
-13.236748	-22.894218	0.295283
-13.857514	-19.742062	0.300288
-13.977083	-16.763991	0.305293
-14.296633	-10.959136	0.310298
-14.560534	-14.827204	0.315302
-14.909524	-14.497121	0.320307
-15.329571	-20.386490	0.325312
-15.276246	-22.256422	0.330317
-15.607107	-11.432561	0.335322
-15.270217	-10.391163	0.340326
-15.510589	-20.238600	0.345331
-16.731763	-14.580216	0.350336
-16.716294	-23.850175	0.355341
-17.030051	-12.780233	0.360346
-17.163851	-14.392728	0.365350
-17.064807	-14.720532	0.370355
-17.580174	-17.170400	0.375360
-17.866253	-16.772282	0.380365
-18.349469	-15.936405	0.385370
-18.847962	-12.367508	0.390374
-18.718731	-8.990548	0.395379
-18.782135	-8.806514	0.400384
-18.843404	-23.659744	0.405389
-19.057219	-18.233741	0.410394
-19.679569	-19.028539	0.415398
-20.227096	-17.397425	0.420403
-20.475343	-19.767426	0.425408
-20.430484	-19.979135	0.430413
-20.835788	-10.543685	0.435418
-21.173880	-12.671339	0.440422
-20.378443	-22.830439	0.445427
-20.893900	-20.342769	0.450432
-21.548335	-25.465518	0.455437
-22.062916	-15.688224	0.460442
-22.246001	-24.599114	0.465446
-22.136039	-8.299410	0.470451
-22.261926	-17.110249	0.475456
-22.545999	-22.930732	0.480461
-23.472443	-17.503569	0.485466
-23.682059	-22.258050	0.490470
-23.368800	-13.506552	0.495475
-24.069189	-14.376847	0.500480
-23.804653	-18.566553	0.505485
-24.411692	-15.420610	0.510490
-25.143804	-25.635067	0.515494
-25.208636	-13.076410	0.520499
-25.532178	-17.140713	0.525504
-25.230242	-18.032421	0.530509
-25.699986	-25.454871	0.535514
-25.659438	-16.264867	0.540518
-25.299194	-21.293177	0.545523
-26.099130	-15.499500	0.550528
-26.808084	-21.876821	0.555533
-27.078339	-13.214560	0.560538
-27.077315	-27.072877	0.565542
-26.904957	-18.556574	0.570547
-27.658779	-13.085031	0.575552
-27.970939	-13.653769	0.580557
-28.280030	-12.811349	0.585562
-28.328070	-18.039050	0.590566
-28.587434	-25.874810	0.595571
-28.614137	-17.498652	0.600576
-29.114561	-17.336314	0.605581
-29.835179	-12.400434	0.610586
-30.060291	-28.749825	0.615590
-30.445269	-14.672534	0.620595
-30.427047	-8.337781	0.625600
-30.068815	-21.816512	0.630605
-30.132053	-17.730376	0.635610
-30.083860	-19.168138	0.640614
-30.954064	-19.148610	0.645619
-32.147171	-14.380297	0.650624
-31.730982	-14.246123	0.655629
-31.806459	-14.262634	0.660634
-31.994217	-12.567558	0.665638
-31.909234	-16.801582	0.670643
-32.629821	-14.445554	0.675648
-33.052314	-10.498243	0.680653
-33.378950	-9.533551	0.685658
-33.401943	-12.518211	0.690662
-33.338804	-18.103957	0.695667
-33.944790	1.999263	0.700672
-33.986478	-12.849417	0.705677
-34.765875	-5.577517	0.710682
-35.103835	-8.499766	0.715686
-34.558287	-16.511174	0.720691
-35.025627	-24.983816	0.725696
-34.874594	-15.109643	0.730701
-35.547230	-15.216193	0.735706
-36.110043	-9.163760	0.740710
-36.452093	-15.453933	0.745715
-36.680546	-1.211205	0.750720
-36.498802	-13.310079	0.755725
-36.522343	-15.145900	0.760730
-36.924835	-26.180003	0.765734
-37.290969	-24.044251	0.770739
-37.924663	-10.418836	0.775744
-37.984101	-14.636983	0.780749
-38.076561	-18.898309	0.785754
-38.323822	-17.937658	0.790758
-38.296873	-21.956787	0.795763
-39.434258	-16.376867	0.800768
-39.248122	-27.800071	0.805773
-39.958790	-14.589808	0.810778
-39.984432	-23.127852	0.815782
-39.859889	-17.138112	0.820787
-40.000462	-12.926924	0.825792
-39.744216	-17.352033	0.830797
-40.574465	-13.684899	0.835802
-40.903375	-18.500267	0.840806
-41.392735	-24.202272	0.845811
-41.615552	-17.212668	0.850816
-41.033331	-17.350403	0.855821
-41.329550	-20.026397	0.860826
-42.234468	-18.671253	0.865830
-42.841777	-25.857573	0.870835
-42.827889	-21.251839	0.875840
-42.987355	-24.769374	0.880845
-42.840666	-17.254526	0.885850
-43.378457	-12.717734	0.890854
-43.873037	-20.067020	0.895859
-44.565650	-17.917662	0.900864
-44.932196	-6.521125	0.905869
-44.227118	-16.767405	0.910874
-44.200105	-10.041456	0.915878
-44.409920	-23.703330	0.920883
-44.878376	-23.108441	0.925888
-45.515850	-14.875417	0.930893
-46.170653	-14.826965	0.935898
-46.431379	-17.685912	0.940902
-46.296084	-20.021629	0.945907
-46.523786	-7.216939	0.950912
-46.289114	-20.429103	0.955917
-46.542634	-25.595217	0.960922
-46.873837	-10.653512	0.965926
-47.364729	-15.281202	0.970931
-48.149209	-25.092080	0.975936
-48.093416	-25.295632	0.980941
-48.126533	-17.403900	0.985946
-48.401390	-13.198439	0.990950
-48.343619	-20.546373	0.995955
-48.869782	-11.275239	1.000960
-49.159852	-17.187664	1.005965
-49.707639	-23.306403	1.010970
-49.795080	-18.259012	1.015974
-49.819901	-15.919610	1.020979
-50.136299	-6.814451	1.025984
-49.928108	-11.805797	1.030989
-50.585864	-12.998044	1.035994
-50.977913	-13.968820	1.040998
-51.464021	-18.172882	1.046003
-51.518370	-18.614539	1.051008
-51.613994	-13.285908	1.056013
-51.718345	-12.913186	1.061018
-52.221871	-14.004938	1.066022
-52.297627	-23.151198	1.071027
-52.877488	-20.842795	1.076032
-52.824341	-19.910778	1.081037
-52.681031	-16.537134	1.086042
-53.519122	-12.053215	1.091046
-53.692323	-17.070415	1.096051
-54.411877	-11.033711	1.101056
-54.112997	-31.612444	1.106061
-54.247053	-26.095249	1.111066
-54.617309	-15.742080	1.116070
-54.771891	-24.410840	1.121075
-56.072706	-11.502598	1.126080
-55.775897	-19.379468	1.131085
-55.972346	-19.465170	1.136090
-55.777377	-20.060104	1.141094
-55.770440	-27.248986	1.146099
-56.013362	-10.498518	1.151104
-56.726698	-18.013697	1.156109
-57.368291	-25.158143	1.161114
-57.456566	-19.478232	1.166118
-57.505252	-28.177119	1.171123
-57.601116	-11.637613	1.176128
-57.359227	-13.483956	1.181133
-57.779652	-16.721491	1.186138
-58.778497	-12.599806	1.191142
-59.063273	-22.999372	1.196147
-59.564092	-21.462595	1.201152
-59.478373	-19.496426	1.206157
-59.359343	-14.743510	1.211162
-59.392100	-3.248726	1.216166
-59.225828	-16.816291	1.221171
-60.164649	-6.359383	1.226176
-60.613151	-20.622776	1.231181
-60.934698	-14.209677	1.236186
-61.326241	-17.186107	1.241190
-61.038050	-13.932992	1.246195
-60.882978	-14.361806	1.251200
-61.487794	-30.004707	1.256205
-61.964127	-17.720583	1.261210
-62.487491	-12.307250	1.266214
-62.226386	-24.783860	1.271219
-62.459758	-18.662162	1.276224
-62.641966	-18.308241	1.281229
-63.637079	-22.986272	1.286234
-64.198778	-13.056955	1.291238
-64.046632	-22.768293	1.296243
-64.173479	-11.897945	1.301248
-64.121256	-10.207803	1.306253
-64.345368	-13.649443	1.311258
-64.510704	-17.489796	1.316262
-64.530666	-15.493632	1.321267
-65.466320	-17.762947	1.326272
-65.528272	-9.546012	1.331277
-65.480457	-14.892057	1.336282
-65.934609	-14.831087	1.341286
-65.485834	-13.812623	1.346291
-66.611804	-10.896809	1.351296
-66.845014	-19.680730	1.356301
-66.674482	-8.781985	1.361306
-67.254965	-7.049428	1.366310
-67.194532	-13.655320	1.371315
-67.979352	-15.152721	1.376320
-68.179612	-19.008710	1.381325
-68.760880	-17.354751	1.386330
-68.678279	-15.454857	1.391334
-68.661525	-17.427858	1.396339
-68.921456	-15.059269	1.401344
-68.836291	-9.711484	1.406349
-69.046109	-17.897866	1.411354
-70.046210	-17.511274	1.416358
-70.215766	-22.284211	1.421363
-70.834895	-6.303429	1.426368
-70.359442	-20.852707	1.431373
-70.403521	-26.958697	1.436378
-70.448676	-15.171137	1.441382
-71.053449	-12.969306	1.446387
-71.786270	-16.374126	1.451392
-72.007341	-18.347482	1.456397
-71.992323	-10.036425	1.461402
-72.053642	-11.067384	1.466406
-71.934245	-14.537876	1.471411
-72.659714	-15.046986	1.476416
-73.296822	-28.572330	1.481421
-73.565094	-11.960727	1.486426
-73.730798	-8.533546	1.491430
-73.427936	-4.264135	1.496435
-73.899730	-8.372795	1.501440
-74.151929	-23.447315	1.506445
-74.655083	-10.969335	1.511450
-75.038343	-15.284017	1.516454
-75.351231	-15.572943	1.521459
-75.910665	-12.841129	1.526464
-75.667174	-11.416708	1.531469
-75.390360	-21.894289	1.536474
-75.586506	-19.214427	1.541478
-75.373897	-15.321470	1.546483
-76.361093	-11.790584	1.551488
-76.575957	-18.695283	1.556493
-76.832060	-12.860960	1.561498
-77.479338	-10.953003	1.566502
-77.803155	-11.256105	1.571507
-78.463171	-13.958493	1.576512
-77.974754	-26.179760	1.581517
-78.081163	-28.723351	1.586522
-78.695499	-12.945021	1.591526
-78.532798	-16.985401	1.596531
-78.593754	-13.141152	1.601536
-78.847501	-30.642437	1.606541
-79.713073	-20.992217	1.611546
-80.160866	-15.839395	1.616550
-80.464089	-18.320370	1.621555
-80.464743	-21.022322	1.626560
-80.505145	-20.578678	1.631565
-80.668211	-21.775729	1.636570
-80.798652	-16.282510	1.641574
-80.939207	-14.278550	1.646579
-81.765593	-10.094995	1.651584
-82.003468	-23.895276	1.656589
-81.968666	-23.879994	1.661594
-82.361251	-12.765458	1.666598
-82.052043	-24.193217	1.671603
-83.056157	-15.693998	1.676608
-83.282675	-23.102675	1.681613
-83.473346	-25.517111	1.686618
-83.648233	-12.624377	1.691622
-83.331194	-18.703038	1.696627
-83.921013	-2.736667	1.701632
-83.776854	-28.432555	1.706637
-84.467532	-23.223710	1.711642
-84.922799	-17.570062	1.716646
-85.024254	-18.364026	1.721651
-85.075417	-10.222375	1.726656
-85.330418	-15.604596	1.731661
-85.720698	-15.305273	1.736666
-86.229429	-15.369354	1.741670
-86.376639	-12.203215	1.746675
-86.554351	-19.259669	1.751680
-86.532183	-17.002026	1.756685
-86.612576	-20.054049	1.761690
-87.233821	-11.936073	1.766694
-88.358686	-21.312541	1.771699
-88.571567	-19.718479	1.776704
-88.146509	-19.526088	1.781709
-88.255854	-9.320120	1.786714
-88.793311	-9.849252	1.791718
-88.928153	-14.578401	1.796723
-88.896408	-17.585720	1.801728
-88.587241	-27.374798	1.806733
-89.113465	-22.602454	1.811738
-89.646936	-18.646471	1.816742
-89.932057	-17.599453	1.821747
-90.264895	-11.212110	1.826752
-90.156164	-18.948387	1.831757
-91.242806	-20.843699	1.836762
-91.529141	-28.156162	1.841766
-91.954770	-27.523164	1.846771
-91.760336	-12.066441	1.851776
-91.432531	-21.406267	1.856781
-91.563275	-16.399272	1.861786
-91.861024	-22.359552	1.866790
-91.965897	-22.751323	1.871795
-92.871308	-9.390583	1.876800
-93.091061	-4.708644	1.881805
-93.153679	-12.687020	1.886810
-93.551661	-15.675998	1.891814
-93.451630	-17.885527	1.896819
-94.694988	-12.822601	1.901824
-94.950370	-16.011050	1.906829
-94.566739	-23.219668	1.911834
-94.877587	-16.020375	1.916838
-94.736097	-23.018003	1.921843
-94.819600	-20.394938	1.926848
-95.262529	-18.088445	1.931853
-95.845781	-9.139161	1.936858
-96.344724	-11.551187	1.941862
-96.431776	-27.143806	1.946867
-96.395667	-9.983276	1.951872
-96.553924	-6.644241	1.956877
-96.666694	-15.472434	1.961882
-97.616799	-18.846764	1.966886
-97.794630	-26.023456	1.971891
-98.341183	-18.144835	1.976896
-98.210821	-15.301005	1.981901
-98.247965	-16.278541	1.986906
-98.463651	-19.343818	1.991910
-98.009518	-15.098526	1.996915
-99.224378	-16.008920	2.006912
-98.767774	-16.412400	2.016909
-98.308430	-15.536317	2.026906
-98.210489	-5.007187	2.036902
-97.329680	-4.222394	2.046899
-96.642835	-16.342431	2.056896
-95.833201	-20.717506	2.066893
-95.627302	-17.007956	2.076890
-95.768141	-15.973901	2.086886
-94.934121	-27.281472	2.096883
-94.540291	-9.813415	2.106880
-93.591863	-21.742666	2.116877
-92.658543	-20.989272	2.126874
-93.038807	-19.866256	2.136870
-92.731186	-26.290765	2.146867
-91.748798	-12.717950	2.156864
-91.525643	-11.518930	2.166861
-90.486751	-19.377708	2.176858
-89.837752	-17.532011	2.186854
-89.749327	-24.182560	2.196851
-89.755070	-23.520917	2.206848
-88.350068	-14.275253	2.216845
-88.022423	-25.165351	2.226842
-87.918454	-18.330780	2.236838
-87.657688	-15.685585	2.246835
-86.797805	-19.188323	2.256832
-86.157445	-19.237219	2.266829
-85.216088	-17.508395	2.276826
-85.148929	-23.222532	2.286822
-85.091077	-16.112738	2.296819
-84.465400	-14.657524	2.306816
-83.829363	-12.293250	2.316813
-83.431393	-5.847371	2.326810
-81.983634	-15.007413	2.336806
-81.877931	-17.819386	2.346803
-81.488666	-13.181460	2.356800
-81.542627	-16.408304	2.366797
-81.286134	-24.833590	2.376794
-80.214495	-16.440832	2.386790
-79.890700	-10.939399	2.396787
-79.023305	-15.225929	2.406784
-78.733743	-7.020902	2.416781
-78.417580	-9.106642	2.426778
-77.583114	-16.491560	2.436774
-76.999726	-11.903399	2.446771
-77.037062	-12.225243	2.456768
-75.896563	-23.194071	2.466765
-75.363131	-16.023000	2.476762
-75.205027	-18.720650	2.486758
-75.016587	-21.723017	2.496755
-74.351021	-17.749131	2.506752
-74.053122	-15.458575	2.516749
-73.002038	-21.510370	2.526746
-72.511706	-15.116010	2.536742
-72.366400	-21.089526	2.546739
-71.602662	-18.010135	2.556736
-70.733977	-18.121066	2.566733
-70.498177	-19.755820	2.576730
-70.641223	-20.838497	2.586726
-69.860539	-25.861732	2.596723
-69.343155	-18.294166	2.606720
-68.768460	-21.245881	2.616717
-68.117128	-25.362751	2.626714
-68.052009	-29.890870	2.636710
-67.291713	-23.803693	2.646707
-66.750334	-21.607411	2.656704
-66.365267	-20.134753	2.666701
-65.482229	-23.111843	2.676698
-65.129124	-23.337498	2.686694
-65.050589	-22.010163	2.696691
-63.772998	-15.137712	2.706688
-63.509695	-24.900941	2.716685
-63.207598	-17.128086	2.726682
-62.826738	-14.057723	2.736678
-62.131627	-13.264757	2.746675
-61.946873	-25.988441	2.756672
-60.979587	-17.038096	2.766669
-60.837190	-22.740566	2.776666
-60.318995	-21.148257	2.786662
-59.271117	-17.422177	2.796659
-58.760063	-26.716833	2.806656
-58.549161	-25.406930	2.816653
-58.624595	-18.143233	2.826650
-57.787167	-15.498015	2.836646
-57.294601	-23.916285	2.846643
-56.503694	-17.832582	2.856640
-55.695389	-14.791967	2.866637
-55.434634	-19.718607	2.876634
-55.344763	-18.635260	2.886630
-55.093257	-22.638438	2.896627
-54.444198	-14.608598	2.906624
-53.562483	-23.150254	2.916621
-52.796916	-15.369139	2.926618
-52.570046	-17.804725	2.936614
-52.311479	-30.585551	2.946611
-51.946224	-22.355896	2.956608
-51.049761	-13.306617	2.966605
-50.715573	-23.464145	2.976602
-49.931232	-19.519665	2.986598
-49.254223	-16.126431	2.996595
-49.301437	-17.776743	3.006592
-49.123787	-24.505754	3.016589
-47.893163	-12.709946	3.026586
-47.777080	-20.998826	3.036582
-47.114789	-17.008194	3.046579
-46.201306	-15.503635	3.056576
-46.223426	-18.133270	3.066573
-46.127968	-10.817107	3.076570
-45.069592	-17.433262	3.086566
-44.392324	-20.790438	3.096563
-44.392809	-9.894856	3.106560
-43.782395	-22.128700	3.116557
-43.150621	-19.458383	3.126554
-42.401823	-25.796272	3.136550
-41.501990	-18.580943	3.146547
-41.783462	-14.031110	3.156544
-41.331194	-17.208559	3.166541
-40.757330	-12.367813	3.176538
-39.916877	-18.961287	3.186534
-39.615724	-19.272593	3.196531
-39.280241	-23.375392	3.206528
-38.238558	-21.559914	3.216525
-37.827951	-8.864005	3.226522
-37.677230	-25.872470	3.236518
-37.502517	-25.898538	3.246515
-36.490896	-15.883827	3.256512
-36.105887	-12.939107	3.266509
-35.919176	-16.770168	3.276506
-34.873622	-23.662766	3.286502
-34.714263	-22.137593	3.296499
-34.240007	-17.083414	3.306496
-33.172454	-23.439705	3.316493
-33.059549	-21.150086	3.326490
-33.005251	-18.526281	3.336486
-31.964032	-21.058516	3.346483
-31.408751	-14.841135	3.356480
-31.712818	-22.390244	3.366477
-30.651391	-18.800741	3.376474
-30.043919	-24.586098	3.386470
-29.190931	-12.404363	3.396467
-28.757492	-15.744950	3.406464
-28.393103	-19.217852	3.416461
-28.176279	-16.603521	3.426458
-27.941775	-16.185369	3.436454
-26.904864	-13.420396	3.446451
-26.661267	-14.959138	3.456448
-26.262449	-20.766517	3.466445
-25.322682	-6.216494	3.476442
-25.127669	-16.540097	3.486438
-24.832244	-21.227388	3.496435
-23.896163	-15.453150	3.506432
-23.449790	-15.373866	3.516429
-23.434095	-19.092304	3.526426
-22.251709	-22.072236	3.536422
-21.723764	-10.479554	3.546419
-21.523089	-13.406894	3.556416
-21.452518	-19.463979	3.566413
-20.462885	-26.769824	3.576410
-20.076099	-18.157285	3.586406
-19.618432	-22.080540	3.596403
-18.684884	-22.325956	3.606400
-18.439931	-16.957883	3.616397
-18.208580	-13.337090	3.626394
-17.819539	-29.535019	3.636390
-17.122570	-22.011843	3.646387
-16.928837	-14.731577	3.656384
-16.077691	-16.264137	3.666381
-15.611077	-15.840386	3.676378
-14.863051	-16.351390	3.686374
-13.919842	-19.695516	3.696371
-14.056457	-27.083526	3.706368
-14.053472	-17.291420	3.716365
-13.216674	-22.616124	3.726362
-12.321918	-19.607866	3.736358
-12.217159	-19.327706	3.746355
-11.683306	-19.832258	3.756352
-11.022163	-19.633675	3.766349
-10.699132	-22.990389	3.776346
-10.023376	-23.207723	3.786342
-9.141554	-21.020379	3.796339
-9.185214	-13.699004	3.806336
-8.501661	-16.458300	3.816333
-7.824968	-15.845426	3.826330
-7.451180	-24.229052	3.836326
-7.286305	-21.759347	3.846323
-6.126129	-18.385302	3.856320
-6.021316	-25.208568	3.866317
-6.101677	-19.457394	3.876314
-4.661406	-21.376051	3.886310
-4.240805	-28.487987	3.896307
-4.193463	-11.159125	3.906304
-3.986299	-13.344894	3.916301
-3.376218	-4.410668	3.926298
-2.516840	3.727274	3.936294
-2.060846	14.549811	3.946291
-2.225662	24.001217	3.956288
-1.934241	37.579139	3.966285
-1.250134	57.663883	3.976282
-0.767241	80.762180	3.986278
-0.085586	102.651458	3.996275
0.000000	134.170832	4.001280
0.775781	133.842374	4.006285
0.348353	142.269357	4.011290
0.416658	144.186928	4.016294
0.962123	165.825485	4.021299
0.753075	182.176437	4.026304
0.880435	171.821484	4.031309
0.830600	173.129151	4.036314
1.076470	173.671601	4.041318
1.660381	168.963504	4.046323
1.107483	180.543896	4.051328
1.324472	177.949289	4.056333
1.610782	174.964679	4.061338
1.362168	176.290595	4.066342
1.549013	168.645392	4.071347
1.643910	170.789330	4.076352
1.556741	171.238438	4.081357
1.571837	181.676834	4.086362
1.511082	173.687883	4.091366
1.639523	171.905749	4.096371
1.360509	173.353499	4.101376
1.530391	173.223235	4.106381
1.464771	172.925896	4.111386
1.190282	181.554930	4.116390
1.651895	182.535775	4.121395
1.032230	180.428677	4.126400
1.494414	166.825952	4.131405
1.397986	174.923294	4.136410
1.609302	184.433755	4.141414
1.373381	181.842962	4.146419
1.383724	173.642481	4.151424
1.386781	165.314362	4.156429
1.373515	175.657797	4.161434
1.476779	184.903561	4.166438
1.604630	183.695905	4.171443
1.493511	178.958822	4.176448
1.568005	165.120842	4.181453
1.617114	171.559584	4.186458
1.535581	176.229885	4.191462
1.656074	174.048319	4.196467
1.494500	171.425608	4.201472
1.569865	177.959755	4.206477
1.719973	179.079587	4.211482
1.591835	189.601347	4.216486
1.781132	186.535195	4.221491
1.831086	193.607381	4.226496
1.762306	191.716857	4.231501
1.717282	185.095844	4.236506
1.448130	175.110970	4.241510
1.776794	185.795592	4.246515
1.746189	197.526658	4.251520
2.166562	203.887878	4.256525
1.862523	201.459086	4.261530
1.635653	191.215046	4.266534
1.764152	198.275833	4.271539
1.876423	200.894602	4.276544
2.078840	195.178323	4.281549
1.954319	191.285786	4.286554
1.649332	186.465607	4.291558
2.171314	197.111284	4.296563
1.939487	201.395819	4.301568
1.789716	187.270200	4.306573
1.877047	182.694675	4.311578
1.511846	189.989077	4.316582
2.204618	207.930644	4.321587
1.886339	217.504968	4.326592
1.966567	217.949204	4.331597
2.068532	219.913016	4.336602
1.671211	218.766496	4.341606
2.081106	211.017028	4.346611
1.987136	219.855890	4.351616
2.012343	216.888475	4.356621
2.301063	210.891059	4.361626
2.075770	210.380862	4.366630
2.151715	214.122239	4.371635
2.074095	217.649357	4.376640
1.828067	208.039385	4.381645
2.018764	209.231733	4.386650
2.262310	201.175215	4.391654
2.279930	206.515004	4.396659
2.096417	217.671815	4.401664
2.272562	218.262688	4.406669
2.219467	219.723125	4.411674
2.008596	225.115677	4.416678
2.348940	216.190952	4.421683
1.951701	216.515496	4.426688
2.213439	218.540611	4.431693
2.024601	220.218823	4.436698
1.748631	219.924674	4.441702
1.906040	218.596997	4.446707
1.919496	220.673404	4.451712
1.962266	224.273858	4.456717
2.279139	232.408591	4.461722
2.353753	245.185732	4.466726
2.046063	243.821163	4.471731
2.569707	242.380770	4.476736
2.552119	245.553955	4.481741
2.498551	251.240861	4.486746
2.623247	250.986456	4.491750
2.589726	229.487857	4.496755
1.960397	215.221064	4.501760
2.387038	224.528347	4.506765
2.604662	239.158509	4.511770
2.479259	239.794086	4.516774
2.228709	236.715275	4.521779
2.761431	241.618927	4.526784
2.878681	232.227514	4.531789
2.471401	220.966514	4.536794
1.962990	231.495601	4.541798
2.830500	227.146002	4.546803
2.031378	224.808001	4.551808
2.402533	232.686232	4.556813
2.516598	239.606074	4.561818
2.534603	237.341990	4.566822
2.731738	249.519473	4.571827
2.620524	244.925834	4.576832
2.697603	246.312078	4.581837
3.091870	244.059115	4.586842
2.662670	239.210710	4.591846
2.512088	223.759828	4.596851
2.696591	233.382583	4.601856
2.712904	237.830539	4.606861
2.778094	239.046097	4.611866
2.405018	232.746738	4.616870
2.775276	234.648260	4.621875
2.853627	242.083274	4.626880
2.885000	242.854347	4.631885
2.865335	226.842466	4.636890
2.307907	214.653748	4.641894
2.685851	220.222666	4.646899
2.659292	233.160162	4.651904
2.701000	234.861148	4.656909
3.004230	240.061208	4.661914
2.770058	236.092267	4.666918
2.727912	227.662864	4.671923
2.826674	243.094138	4.676928
2.547415	230.873150	4.681933
2.836032	236.198946	4.686938
2.492225	249.996197	4.691942
2.913441	241.046945	4.696947
2.751307	256.817813	4.701952
2.642070	241.891352	4.706957
2.797751	240.629467	4.711962
2.444728	241.592318	4.716966
3.074002	251.107841	4.721971
2.874681	265.478304	4.726976
2.986441	254.834142	4.731981
3.203147	251.714613	4.736986
3.049430	243.247109	4.741990
3.444770	231.713071	4.746995
2.813958	241.700836	4.752000
2.702964	252.724931	4.757005
2.963235	249.636876	4.762010
3.122476	258.613373	4.767014
3.253907	267.615584	4.772019
2.986643	266.889059	4.777024
3.296314	259.777179	4.782029
2.988444	250.069864	4.787034
2.826252	253.166415	4.792038
3.315435	264.382966	4.797043
3.092693	269.893614	4.802048
3.490241	268.094226	4.807053
3.315834	265.771171	4.812058
3.006378	261.018794	4.817062
3.317142	257.675157	4.822067
3.199860	268.336848	4.827072
3.473528	248.459901	4.832077
3.163097	241.674065	4.837082
2.791351	251.224393	4.842086
3.254398	253.549115	4.847091
2.990817	275.315807	4.852096
3.165906	270.171396	4.857101
3.326157	267.090988	4.862106
3.180270	268.452717	4.867110
3.461634	281.580387	4.872115
3.276139	282.019209	4.877120
3.274768	282.315034	4.882125
3.405675	276.159874	4.887130
3.283400	285.773277	4.892134
3.358526	273.211135	4.897139
2.938519	274.530655	4.902144
3.220177	265.518225	4.907149
3.553051	273.337986	4.912154
3.193848	269.944055	4.917158
3.484267	268.713867	4.922163
3.243466	270.959370	4.927168
3.149072	276.931147	4.932173
3.156055	282.754959	4.937178
3.413513	300.518181	4.942182
3.465793	296.410824	4.947187
3.550531	305.974441	4.952192
3.828672	301.652567	4.957197
3.957140	298.237430	4.962202
3.209256	285.890805	4.967206
4.055084	286.646857	4.972211
3.667815	284.940267	4.977216
3.402569	287.854074	4.982221
3.397480	279.746457	4.987226
3.697602	291.888801	4.992230
3.730402	280.927956	4.997235
3.644232	296.769578	5.002240
3.761402	305.048145	5.007245
3.828244	307.271522	5.012250
3.590742	291.438135	5.017254
3.986361	281.397297	5.022259
3.837490	282.175566	5.027264
3.401565	275.389637	5.032269
3.670293	280.863367	5.037274
3.917867	299.886995	5.042278
3.627807	298.605142	5.047283
3.785569	309.185397	5.052288
4.047799	299.622983	5.057293
3.748287	279.482493	5.062298
3.555495	283.320784	5.067302
3.808401	291.073659	5.072307
3.593287	300.340143	5.077312
4.024549	314.776232	5.082317
3.785602	299.536601	5.087322
3.560411	310.034131	5.092326
3.804289	306.581470	5.097331
3.850574	305.815853	5.102336
3.209805	304.088507	5.107341
3.641345	297.363927	5.112346
3.224946	299.916075	5.117350
3.769142	316.471714	5.122355
3.692138	330.230964	5.127360
4.183056	330.528110	5.132365
3.978316	325.351444	5.137370
3.854986	326.672157	5.142374
4.115386	318.924650	5.147379
3.849959	334.872790	5.152384
4.008092	334.364042	5.157389
3.872224	342.559052	5.162394
4.052332	329.172294	5.167398
4.204681	330.408874	5.172403
4.043928	325.581290	5.177408
3.964936	324.805200	5.182413
3.959151	329.874532	5.187418
4.136162	345.745817	5.192422
4.119018	335.485175	5.197427
4.267309	336.489199	5.202432
4.159330	333.372895	5.207437
3.896417	327.966990	5.212442
3.785971	337.840309	5.217446
4.098361	338.415577	5.222451
3.865764	339.714985	5.227456
4.437417	338.599719	5.232461
4.539753	339.046027	5.237466
4.068709	346.227272	5.242470
4.247268	340.932008	5.247475
3.926253	356.879590	5.252480
4.297724	355.033693	5.257485
4.232270	360.544821	5.262490
4.144482	368.309642	5.267494
4.422837	359.200623	5.272499
4.293617	362.744292	5.277504
4.276081	370.624379	5.282509
4.490682	366.231496	5.287514
4.551803	363.404132	5.292518
4.829077	349.551911	5.297523
5.019176	349.103882	5.302528
4.395245	335.257453	5.307533
4.541651	341.351557	5.312538
4.164772	340.489433	5.317542
4.597510	339.292449	5.322547
4.172404	336.211091	5.327552
4.587283	341.653981	5.332557
4.964699	328.888720	5.337562
4.392759	339.633686	5.342566
4.357032	329.774105	5.347571
4.518368	321.860845	5.352576
4.099473	324.999734	5.357581
4.488270	344.758660	5.362586
4.470988	356.081174	5.367590
4.677098	353.068051	5.372595
4.836151	370.626820	5.377600
4.780341	363.440031	5.382605
4.510145	340.033963	5.387610
4.561761	349.375576	5.392614
4.573718	353.084941	5.397619
4.579491	365.845442	5.402624
4.796698	360.375967	5.407629
4.671318	366.396803	5.412634
4.534717	360.706792	5.417638
4.709553	359.456629	5.422643
4.764641	367.366050	5.427648
4.447549	368.117071	5.432653
4.785553	365.935149	5.437658
4.459626	363.483606	5.442662
4.976789	361.026714	5.447667
4.692202	369.313698	5.452672
4.936848	375.867606	5.457677
5.195158	365.864698	5.462682
4.519260	365.034526	5.467686
4.945340	365.951603	5.472691
4.965696	369.058953	5.477696
4.890712	365.718268	5.482701
5.046382	366.390964	5.487706
4.741383	373.383968	5.492710
4.937444	370.921733	5.497715
5.143490	365.454002	5.502720
5.038634	354.733789	5.507725
5.024280	366.086805	5.512730
5.100904	363.378524	5.517734
4.911463	356.714315	5.522739
4.859685	356.817308	5.527744
5.091954	362.662325	5.532749
5.039149	361.767955	5.537754
4.798484	373.694682	5.542758
4.787497	358.891274	5.547763
4.965005	364.120737	5.552768
4.734697	360.035694	5.557773
4.895893	355.526345	5.562778
5.015971	370.246055	5.567782
5.120535	363.807230	5.572787
5.182515	366.379880	5.577792
4.989959	358.692705	5.582797
4.992874	356.003315	5.587802
4.935980	354.285628	5.592806
5.260155	358.383512	5.597811
4.732638	363.392765	5.602816
4.897229	362.991079	5.607821
5.070125	355.747260	5.612826
4.884483	362.788412	5.617830
5.308511	366.813758	5.622835
5.396333	389.890338	5.627840
5.002051	394.976735	5.632845
5.484158	392.039738	5.637850
5.474690	391.841244	5.642854
5.213835	365.128835	5.647859
5.094840	369.769671	5.652864
5.332262	383.759368	5.657869
5.521824	389.549890	5.662874
5.540879	388.567084	5.667878
5.212271	372.947268	5.672883
5.127662	360.262971	5.677888
5.123856	382.432030	5.682893
5.235525	390.433237	5.687898
5.203396	395.857675	5.692902
5.518162	385.180664	5.697907
5.520269	388.820040	5.702912
5.573121	397.884247	5.707917
5.697534	394.233670	5.712922
5.231419	399.365286	5.717926
5.749740	390.370697	5.722931
5.828381	401.516973	5.727936
5.492952	383.788364	5.732941
5.442740	377.050624	5.737946
5.090944	390.821994	5.742950
5.416192	383.085344	5.747955
5.871642	391.507047	5.752960
5.662830	399.196876	5.757965
5.493400	400.495222	5.762970
5.080148	396.677577	5.767974
5.569228	395.299119	5.772979
5.615519	389.419046	5.777984
5.880927	399.929977	5.782989
5.639225	395.241045	5.787994
5.540204	402.478042	5.792998
5.891870	397.147640	5.798003
5.326361	406.439437	5.803008
5.472296	396.019799	5.808013
5.558222	392.936751	5.813018
5.444758	398.449907	5.818022
5.761233	394.115852	5.823027
5.865221	400.992938	5.828032
5.743795	403.893062	5.833037
5.771848	383.853590	5.838042
5.580794	393.669134	5.843046
5.708257	395.606163	5.848051
5.711987	395.830508	5.853056
5.572930	393.540955	5.858061
5.572076	394.968112	5.863066
5.504688	395.431321	5.868070
5.712498	398.138716	5.873075
5.743945	405.499281	5.878080
5.437320	405.063488	5.883085
5.877387	400.742057	5.888090
5.827957	418.662189	5.893094
6.315939	418.950451	5.898099
6.021497	428.448452	5.903104
5.757894	427.272220	5.908109
5.984887	420.695735	5.913114
5.728805	422.480780	5.918118
5.844319	417.956665	5.923123
5.926583	425.845346	5.928128
5.821685	428.907602	5.933133
5.945844	421.174073	5.938138
6.217571	419.879086	5.943142
5.800910	417.713544	5.948147
6.198970	422.166343	5.953152
6.099882	431.418763	5.958157
6.232091	419.784620	5.963162
5.837802	418.178721	5.968166
5.875835	420.344523	5.973171
6.412111	426.899687	5.978176
5.903119	424.573691	5.983181
6.237587	418.820412	5.988186
6.346397	431.154704	5.993190
6.332718	422.023368	5.998195
6.101132	434.228339	6.003200
5.946565	433.743936	6.008205
6.071078	437.598396	6.013210
6.020593	432.870354	6.018214
6.228273	426.204911	6.023219
6.205289	423.834116	6.028224
6.056291	418.741340	6.033229
6.263072	419.180453	6.038234
6.046836	426.632570	6.043238
5.979247	433.462650	6.048243
6.150912	441.166970	6.053248
5.971730	430.441525	6.058253
5.902812	420.780544	6.063258
5.923229	426.987453	6.068262
5.835194	429.382456	6.073267
6.313834	419.259637	6.078272
5.767412	426.109254	6.083277
6.166319	419.389225	6.088282
6.307504	429.568494	6.093286
6.191643	423.398117	6.098291
6.146457	419.253262	6.103296
6.134374	422.061228	6.108301
6.139949	410.557333	6.113306
6.033258	424.948943	6.118310
6.147645	413.518225	6.123315
6.455236	440.193832	6.128320
6.015690	429.313209	6.133325
6.343561	419.519372	6.138330
6.298400	426.823348	6.143334
6.056994	421.684377	6.148339
6.279759	422.790938	6.153344
6.209221	429.940565	6.158349
6.153100	422.266328	6.163354
5.702653	419.289871	6.168358
6.049840	425.531372	6.173363
6.360451	422.745541	6.178368
6.282847	423.373719	6.183373
6.559722	427.997002	6.188378
6.384736	432.608535	6.193382
6.377566	412.339644	6.198387
6.660279	417.687790	6.203392
6.054429	429.077729	6.208397
6.169421	419.601334	6.213402
6.016141	435.991090	6.218406
6.535633	425.864672	6.223411
6.616006	422.581568	6.228416
6.251388	423.554930	6.233421
6.321040	429.177339	6.238426
6.103343	426.082701	6.243430
6.277904	425.251877	6.248435
6.261855	422.263912	6.253440
6.249857	421.751707	6.258445
5.958995	416.254690	6.263450
6.251680	426.911389	6.268454
6.343259	420.369812	6.273459
5.991565	417.074647	6.278464
6.323758	419.872679	6.283469
6.221993	403.829983	6.288474
5.946034	406.062471	6.293478
6.040012	414.706612	6.298483
6.359494	420.813878	6.303488
6.200755	418.993242	6.308493
6.399172	406.582973	6.313498
5.914916	412.399913	6.318502
6.109082	415.043465	6.323507
6.281231	419.780539	6.328512
6.078917	414.752613	6.333517
6.239564	402.781699	6.338522
5.893173	415.379345	6.343526
6.278514	419.643342	6.348531
6.202295	422.959442	6.353536
6.231427	422.021436	6.358541
6.211777	415.557142	6.363546
6.013423	408.038916	6.368550
6.255627	406.171853	6.373555
6.069035	406.993161	6.378560
5.746550	415.592077	6.383565
6.252330	428.473236	6.388570
5.917701	422.612198	6.393574
6.141340	421.756295	6.398579
6.040451	429.590597	6.403584
6.251083	426.428034	6.408589
6.510612	422.238248	6.413594
6.443031	435.755802	6.418598
6.112434	430.164814	6.423603
6.281226	412.553319	6.428608
5.928410	421.485586	6.433613
6.465993	418.404551	6.438618
5.936304	435.951128	6.443622
6.226336	424.786857	6.448627
6.503651	432.252028	6.453632
5.946564	410.594928	6.458637
6.103434	407.217497	6.463642
5.958590	424.224632	6.468646
6.436572	424.349885	6.473651
6.365787	421.346202	6.478656
5.896305	407.650190	6.483661
6.036526	418.331684	6.488666
6.303463	429.397731	6.493670
6.144417	425.490418	6.498675
6.326957	425.331522	6.503680
6.104497	400.420428	6.508685
6.520045	397.519983	6.513690
5.881817	409.793517	6.518694
5.852353	403.523826	6.523699
5.992924	407.293540	6.528704
6.202221	411.258982	6.533709
6.479651	410.893008	6.538714
6.321602	424.936258	6.543718
6.045005	414.096101	6.548723
6.082739	404.591835	6.553728
5.949343	412.867472	6.558733
6.317329	420.454788	6.563738
6.080868	420.586131	6.568742
6.471056	424.206863	6.573747
6.198486	405.349940	6.578752
6.150838	401.109207	6.583757
6.243793	390.247755	6.588762
6.059491	400.360925	6.593766
5.907480	398.875605	6.598771
6.410166	413.255095	6.603776
6.131812	412.415261	6.608781
6.409579	393.671726	6.613786
6.069876	397.731937	6.618790
5.845012	396.244056	6.623795
6.062721	399.266509	6.628800
6.387331	413.236496	6.633805
6.349904	408.502357	6.638810
6.186952	410.832687	6.643814
6.098469	397.317506	6.648819
5.994895	392.949967	6.653824
6.247095	401.777898	6.658829
6.308851	394.160852	6.663834
5.968023	393.544643	6.668838
5.986012	393.221149	6.673843
5.981628	407.014935	6.678848
6.192840	424.667158	6.683853
6.376599	415.004085	6.688858
6.350590	434.126958	6.693862
6.121557	418.855973	6.698867
6.192211	407.009340	6.703872
5.854162	417.496291	6.708877
6.198902	415.321733	6.713882
6.282657	420.314932	6.718886
5.999201	424.652556	6.723891
6.068328	415.758527	6.728896
5.913610	430.177811	6.733901
6.307468	421.855215	6.738906
5.722440	433.602018	6.743910
6.105139	433.254559	6.748915
6.378416	429.291091	6.753920
6.233089	423.100820	6.758925
6.398528	425.563742	6.763930
6.216568	432.127105	6.768934
6.052536	431.627889	6.773939
6.141098	432.845322	6.778944
6.178221	427.457873	6.783949
6.198485	424.962527	6.788954
6.145755	434.482347	6.793958
6.009950	430.455662	6.798963
6.210452	431.156864	6.803968
6.125259	428.927367	6.808973
6.102805	431.177851	6.813978
6.156699	431.644993	6.818982
6.283369	429.360160	6.823987
6.333547	426.843591	6.828992
6.339890	431.402663	6.833997
6.387532	426.347929	6.839002
6.146761	428.862294	6.844006
6.498390	421.355579	6.849011
6.235077	413.038493	6.854016
5.867344	398.315214	6.859021
6.278640	391.007710	6.864026
6.068227	398.570731	6.869030
5.959370	410.502145	6.874035
5.845924	415.029114	6.879040
6.028624	418.455640	6.884045
6.460193	418.717313	6.889050
6.577256	427.160526	6.894054
6.310311	421.157185	6.899059
6.488032	403.414292	6.904064
6.087045	401.747446	6.909069
6.155298	391.942563	6.914074
5.990633	393.359892	6.919078
6.049176	391.567875	6.924083
6.283995	389.723049	6.929088
6.256300	393.853441	6.934093
6.468951	393.374159	6.939098
6.447476	382.975783	6.944102
6.289509	395.299377	6.949107
6.683045	392.252215	6.954112
6.196405	400.722765	6.959117
6.115228	394.323206	6.964122
5.983606	396.081465	6.969126
5.872679	393.283909	6.974131
6.070556	403.703200	6.979136
5.677027	400.947017	6.984141
5.669438	394.711896	6.989146
5.585548	401.356513	6.994150
5.807398	411.503201	6.999155
6.566371	420.730624	7.004160
5.898699	425.932653	7.009165
6.281505	430.208220	7.014170
5.940497	443.264453	7.019174
5.992948	435.708613	7.024179
6.164783	424.331436	7.029184
6.044980	427.962751	7.034189
6.209396	426.551815	7.039194
6.176897	429.027321	7.044198
6.069923	434.596147	7.049203
6.522461	424.460569	7.054208
6.334239	429.666141	7.059213
6.314412	427.935414	7.064218
6.201001	426.348903	7.069222
6.425997	426.945424	7.074227
6.397077	424.955150	7.079232
5.930278	415.170600	7.084237
6.175099	409.975353	7.089242
6.238384	413.760603	7.094246
5.980485	426.273883	7.099251
6.361555	417.228657	7.104256
5.889993	430.611112	7.109261
6.177665	423.659364	7.114266
5.882913	432.032415	7.119270
5.874056	433.462180	7.124275
6.118712	429.474831	7.129280
5.896403	441.343526	7.134285
6.022292	431.946814	7.139290
6.278731	430.524320	7.144294
6.159969	438.001179	7.149299
6.314998	431.988479	7.154304
6.118212	440.918354	7.159309
6.359313	428.280116	7.164314
6.319137	433.454022	7.169318
6.332792	430.763535	7.174323
6.424103	438.025626	7.179328
6.442738	431.298683	7.184333
6.410338	406.506526	7.189338
5.984665	403.000622	7.194342
6.137516	403.159774	7.199347
5.909851	407.830025	7.204352
6.012025	435.003364	7.209357
6.221998	418.163276	7.214362
6.134197	425.947169	7.219366
6.192423	431.654932	7.224371
6.229719	429.834062	7.229376
6.028095	429.822710	7.234381
6.453099	433.011288	7.239386
6.079697	427.195429	7.244390
6.685025	424.199290	7.249395
6.443339	408.318328	7.254400
5.718489	407.955400	7.259405
6.072518	399.361379	7.264410
5.638171	405.171647	7.269414
5.793308	408.885679	7.274419
6.069804	426.841935	7.279424
6.245120	435.076828	7.284429
6.219055	434.503509	7.289434
6.038952	436.977561	7.294438
5.940027	421.100322	7.299443
6.139294	418.566022	7.304448
5.719425	426.367105	7.309453
6.093158	431.309130	7.314458
6.209945	440.808340	7.319462
6.351379	430.828650	7.324467
6.740079	424.260267	7.329472
6.314307	429.199649	7.334477
6.343169	427.714922	7.339482
6.713277	431.768928	7.344486
6.591842	418.092540	7.349491
6.322398	399.924139	7.354496
5.998302	400.436579	7.359501
6.344692	404.376404	7.364506
6.119266	400.229573	7.369510
5.904850	411.624070	7.374515
6.033474	391.065797	7.379520
6.005746	403.539245	7.384525
6.007137	400.926165	7.389530
5.810938	410.880691	7.394534
6.116754	434.182756	7.399539
6.247204	422.342114	7.404544
6.194291	435.649172	7.409549
6.481391	431.478210	7.414554
6.195006	429.727011	7.419558
6.160398	409.874657	7.424563
6.381301	405.825829	7.429568
5.761200	412.649633	7.434573
6.262166	414.958939	7.439578
6.201421	422.584353	7.444582
6.101342	421.215252	7.449587
6.060361	400.811574	7.454592
6.518385	424.477087	7.459597
6.088587	414.141235	7.464602
6.087666	408.650766	7.469606
6.221842	401.373367	7.474611
6.019480	392.589924	7.479616
6.220889	412.014869	7.484621
6.367524	409.469241	7.489626
6.150826	407.093168	7.494630
6.048822	401.303304	7.499635
6.403178	397.320724	7.504640
5.858266	391.993463	7.509645
6.098331	404.532266	7.514650
5.894538	404.298403	7.519654
6.125738	423.889216	7.524659
6.201263	416.785572	7.529664
6.237549	431.488506	7.534669
6.416537	421.397940	7.539674
6.307403	417.158090	7.544678
6.022687	417.663727	7.549683
6.087148	407.543359	7.554688
6.204998	412.241358	7.559693
6.028610	406.534720	7.564698
6.193335	417.735844	7.569702
5.998896	431.722268	7.574707
6.101936	430.465515	7.579712
6.061308	435.367790	7.584717
6.741921	434.751385	7.589722
6.556226	415.708328	7.594726
6.071508	412.654366	7.599731
5.947338	407.907432	7.604736
5.927713	405.553745	7.609741
6.111193	404.608189	7.614746
5.964047	409.150097	7.619750
6.082898	411.692638	7.624755
6.535801	423.018399	7.629760
6.178397	428.694906	7.634765
6.254031	409.620904	7.639770
6.611457	396.201528	7.644774
6.066673	396.423288	7.649779
6.454185	392.611729	7.654784
6.401557	399.424128	7.659789
6.368852	402.530289	7.664794
5.934846	402.080228	7.669798
6.106113	402.731405	7.674803
6.643803	400.443668	7.679808
6.499000	400.479458	7.684813
6.264901	405.325396	7.689818
6.181488	415.075710	7.694822
6.171354	400.892288	7.699827
6.212545	399.550455	7.704832
6.222268	392.607559	7.709837
6.357975	391.305948	7.714842
6.552245	398.258976	7.719846
6.238957	393.880317	7.724851
6.362299	373.348197	7.729856
5.605926	372.893301	7.734861
6.116822	375.149756	7.739866
6.109017	392.212149	7.744870
6.152945	390.870358	7.749875
6.145156	390.043330	7.754880
6.159186	398.269339	7.759885
5.979137	391.092118	7.764890
5.857463	397.558980	7.769894
6.011050	395.007470	7.774899
6.267109	395.436367	7.779904
5.930568	402.044304	7.784909
6.411979	403.353779	7.789914
6.464545	400.409136	7.794918
6.045171	396.293568	7.799923
6.308360	389.748210	7.804928
6.024013	398.627812	7.809933
6.302619	396.797256	7.814938
6.328207	396.764832	7.819942
5.939650	397.002111	7.824947
6.545118	387.410741	7.829952
6.319074	390.263630	7.834957
6.458306	396.699904	7.839962
5.947676	387.923801	7.844966
5.895052	388.989444	7.849971
6.207580	388.082942	7.854976
6.013567	401.424931	7.859981
5.935916	399.253584	7.864986
6.278669	402.323349	7.869990
6.144445	397.814761	7.874995
6.663838	397.408998	7.880000
6.433199	397.652342	7.885005
6.087241	379.285974	7.890010
5.991713	363.683194	7.895014
5.893417	377.478858	7.900019
6.027443	385.423289	7.905024
6.091052	400.202775	7.910029
6.319254	396.898404	7.915034
6.152594	401.657822	7.920038
6.078823	399.349981	7.925043
6.488853	387.581257	7.930048
6.123781	398.813980	7.935053
6.156558	397.458542	7.940058
6.381549	391.042622	7.945062
5.988516	399.337777	7.950067
6.181345	386.780459	7.955072
6.010795	389.775419	7.960077
5.860005	388.993037	7.965082
5.934456	400.743499	7.970086
6.015014	405.475283	7.975091
6.077405	394.025449	7.980096
5.926150	392.352061	7.985101
6.075685	405.510700	7.990106
6.302924	400.475031	7.995110
5.996564	406.975576	8.000115
5.984025	398.869724	8.005133
5.861282	403.596824	8.010150
6.277754	390.063223	8.015168
6.214408	401.215125	8.020186
6.140022	400.135911	8.025203
6.086578	404.558504	8.030221
5.906516	399.075141	8.035238
6.141011	398.097215	8.040256
5.867625	396.542223	8.045274
5.790380	411.569818	8.050291
6.117777	423.212275	8.055309
6.098893	429.368211	8.060326
6.179153	418.641900	8.065344
6.223248	421.022575	8.070362
6.184155	422.157783	8.075379
6.302493	430.427161	8.080397
6.181891	431.591683	8.085414
6.183023	434.787382	8.090432
6.429684	432.561316	8.095450
5.982989	428.518106	8.100467
6.430560	435.009874	8.105485
6.137179	442.747015	8.110502
6.124990	431.123052	8.115520
6.190535	425.188931	8.120538
6.285869	427.262179	8.125555
6.353310	432.775620	8.130573
6.295837	436.620256	8.135590
6.235681	436.573437	8.140608
6.328052	432.317738	8.145626
5.842449	436.312047	8.150643
6.216835	413.990849	8.155661
6.104744	437.581885	8.160678
6.080899	433.435336	8.165696
6.049326	431.450588	8.170714
6.041595	442.665265	8.175731
6.094808	448.734111	8.180749
6.480001	460.954732	8.185766
6.513646	465.486058	8.190784
6.436813	460.476469	8.195802
6.301114	471.785627	8.200819
6.319019	462.297221	8.205837
6.420894	471.645227	8.210854
6.463207	464.315776	8.215872
6.523896	452.691660	8.220890
6.731843	454.071131	8.225907
6.617344	447.578379	8.230925
6.529443	441.201389	8.235942
6.392424	434.143768	8.240960
6.533852	426.522613	8.245978
6.464850	436.379850	8.250995
7.060857	426.404958	8.256013
6.874647	434.690225	8.261030
6.808983	425.169204	8.266048
6.845722	425.967630	8.271066
6.772929	430.112181	8.276083
6.641684	405.077633	8.281101
6.442630	405.140366	8.286118
6.532879	399.643330	8.291136
6.403212	393.539944	8.296154
6.401146	405.082532	8.301171
6.547217	394.881581	8.306189
6.173089	411.357483	8.311206
5.985214	405.938585	8.316224
6.604606	415.899623	8.321242
6.809259	421.634041	8.326259
6.794047	410.770392	8.331277
6.194017	397.841007	8.336294
6.237034	410.129058	8.341312
6.790389	412.907668	8.346330
6.552116	427.521912	8.351347
5.992412	417.138424	8.356365
6.532378	423.654576	8.361382
6.521762	430.649541	8.366400
6.343335	434.461615	8.371418
6.733379	431.377954	8.376435
6.623885	419.529868	8.381453
6.601031	423.110264	8.386470
6.306261	433.270409	8.391488
6.582611	433.475206	8.396506
6.053493	433.391243	8.401523
6.681015	425.942958	8.406541
6.942900	428.017418	8.411558
6.329067	433.136551	8.416576
6.750492	422.601351	8.421594
6.713542	430.672811	8.426611
6.952000	422.101151	8.431629
6.708626	432.670145	8.436646
6.667686	424.829372	8.441664
6.953834	428.963808	8.446682
6.805177	426.174942	8.451699
6.210864	400.445614	8.456717
6.501065	414.668041	8.461734
6.703457	419.053575	8.466752
7.211558	428.347609	8.471770
6.848247	426.206011	8.476787
6.519283	415.620939	8.481805
6.753546	414.994954	8.486822
6.407291	416.287399	8.491840
6.779904	394.427853	8.496858
6.325011	395.484459	8.501875
6.791334	410.160854	8.506893
6.692175	425.932300	8.511910
6.832590	422.074494	8.516928
6.815873	424.311016	8.521946
6.666458	415.987381	8.526963
6.460992	412.079965	8.531981
6.739857	422.475952	8.536998
6.797383	423.282948	8.542016
7.160425	427.381847	8.547034
6.627672	416.573511	8.552051
6.799548	414.370336	8.557069
6.858995	396.991340	8.562087
6.488792	403.065193	8.567104
6.525785	410.479367	8.572122
6.721287	420.212089	8.577139
6.774101	416.065964	8.582157
6.898967	423.674047	8.587175
6.852401	424.357721	8.592192
6.666956	421.301560	8.597210
6.673415	428.836417	8.602227
6.898065	422.727211	8.607245
6.512455	424.778876	8.612263
6.842765	430.100871	8.617280
6.919769	417.305502	8.622298
6.650210	422.679492	8.627315
6.648628	423.304756	8.632333
6.804977	421.398383	8.637351
6.549680	424.893397	8.642368
6.531147	416.197213	8.647386
6.631258	415.806842	8.652403
6.281271	428.801370	8.657421
6.728846	423.833256	8.662439
6.489981	444.754514	8.667456
6.988086	449.782595	8.672474
6.889055	451.038812	8.677491
7.117963	452.481342	8.682509
6.784484	448.098806	8.687527
7.000794	463.856043	8.692544
7.006796	453.945080	8.697562
6.908480	442.344789	8.702579
6.485154	446.806772	8.707597
6.851978	447.083512	8.712615
6.576682	465.287305	8.717632
6.807433	448.661590	8.722650
6.480480	462.396297	8.727667
6.967643	457.272641	8.732685
7.038688	457.961875	8.737703
6.878898	472.358406	8.742720
6.776140	459.532682	8.747738
6.941287	456.069723	8.752755
7.019316	464.315864	8.757773
6.957483	458.537402	8.762791
6.384368	456.378119	8.767808
6.664695	467.103460	8.772826
6.820940	464.081752	8.777843
7.235163	471.143116	8.782861
7.151709	472.346967	8.787879
6.843473	469.814540	8.792896
6.976665	456.215315	8.797914
7.162855	460.327703	8.802931
6.633293	463.142592	8.807949
6.974205	473.084445	8.812967
7.252753	488.735574	8.817984
7.551521	481.705797	8.823002
7.215021	478.081094	8.828019
7.351879	462.110332	8.833037
7.356293	451.742532	8.838055
6.798533	449.546369	8.843072
7.047106	445.694989	8.848090
7.169497	461.190139	8.853107
7.226825	460.706068	8.858125
7.216962	454.148687	8.863143
7.093996	458.893948	8.868160
7.081199	463.465029	8.873178
6.979227	464.404370	8.878195
6.595418	459.907631	8.883213
6.962059	458.233972	8.888231
6.594833	461.707144	8.893248
6.902110	474.558945	8.898266
7.381776	482.069357	8.903283
7.421256	482.214203	8.908301
7.282258	479.746014	8.913319
7.134309	480.339082	8.918336
7.214244	486.015704	8.923354
7.478428	476.334648	8.928371
7.189093	478.257044	8.933389
7.377077	466.605090	8.938407
6.979056	463.275348	8.943424
7.191367	458.042024	8.948442
7.186765	448.604777	8.953459
6.813096	454.837462	8.958477
7.346955	471.566450	8.963495
7.217870	485.264444	8.968512
7.025218	495.671879	8.973530
7.220945	484.063408	8.978547
7.370338	493.968827	8.983565
7.306491	481.375488	8.988583
7.122760	490.360937	8.993600
7.176768	474.222193	8.998618
7.283997	479.912212	9.003635
7.126586	494.523785	9.008653
7.267058	491.851268	9.013671
7.162429	486.952839	9.018688
7.381712	479.748930	9.023706
7.334731	481.378270	9.028723
7.242613	492.845369	9.033741
7.279957	483.180836	9.038759
7.240837	491.993693	9.043776
7.294666	483.446016	9.048794
7.765169	482.564787	9.053811
7.243826	490.425141	9.058829
7.681927	492.494597	9.063847
7.149285	488.835586	9.068864
7.418734	490.269943	9.073882
7.676053	488.760974	9.078899
7.422386	482.465583	9.083917
7.567803	483.757475	9.088935
7.238995	481.843688	9.093952
7.103828	487.255224	9.098970
7.565674	499.172415	9.103987
7.243788	490.588809	9.109005
7.560740	481.148001	9.114023
7.145853	482.049603	9.119040
7.242142	485.222205	9.124058
7.251193	478.329958	9.129075
7.149218	480.865269	9.134093
7.316566	480.432098	9.139111
7.440960	485.573319	9.144128
7.837315	495.524820	9.149146
7.429532	485.343697	9.154163
7.567859	493.559814	9.159181
7.518831	477.925113	9.164199
7.383926	486.439976	9.169216
7.525649	483.781819	9.174234
7.693076	494.050037	9.179251
7.238482	491.786926	9.184269
7.805071	485.339349	9.189287
7.449271	483.270702	9.194304
7.307962	483.667432	9.199322
7.684991	488.532203	9.204339
7.487290	482.404500	9.209357
7.654271	465.980313	9.214375
7.883622	485.847264	9.219392
8.090232	482.253060	9.224410
7.475025	471.308634	9.229427
7.124428	468.359369	9.234445
7.817725	472.635942	9.239463
7.632658	476.325722	9.244480
7.437841	486.513175	9.249498
7.581067	487.305421	9.254515
7.188879	488.819400	9.259533
7.524296	483.540924	9.264551
7.527795	479.968380	9.269568
7.278044	486.197327	9.274586
7.738648	481.539386	9.279603
7.244361	498.367264	9.284621
7.281611	475.797316	9.289639
7.606764	486.387924	9.294656
7.230405	495.103885	9.299674
7.362988	483.700893	9.304691
7.343105	494.871561	9.309709
7.890577	504.978475	9.314727
7.565421	502.303590	9.319744
7.626035	515.296859	9.324762
7.992011	503.178534	9.329779
7.448380	498.983933	9.334797
7.740529	499.755801	9.339815
7.887128	505.622164	9.344832
7.734550	498.908264	9.349850
7.763624	487.771148	9.354867
7.765149	493.236066	9.359885
7.841463	490.397906	9.364903
7.746931	494.066036	9.369920
7.759216	487.364258	9.374938
8.015644	485.616405	9.379955
7.470310	481.137693	9.384973
7.778908	484.035687	9.389991
7.515377	491.411882	9.395008
7.717913	495.899266	9.400026
8.027122	492.462974	9.405043
7.628490	482.099469	9.410061
7.774669	487.966091	9.415079
7.718097	494.581054	9.420096
7.721817	504.357135	9.425114
7.791482	496.954854	9.430131
7.641466	515.317596	9.435149
8.017592	527.279678	9.440167
7.979724	521.785664	9.445184
7.444469	523.037809	9.450202
8.117222	521.531331	9.455219
7.772550	521.375752	9.460237
7.902771	524.689776	9.465255
8.029528	530.388592	9.470272
7.678203	518.357305	9.475290
8.051712	513.918927	9.480307
8.011321	517.656152	9.485325
8.098322	508.808740	9.490343
7.983237	494.293105	9.495360
7.865342	495.173574	9.500378
7.901704	491.769088	9.505395
7.581022	491.862156	9.510413
7.763052	496.551810	9.515431
8.215141	517.844031	9.520448
8.097038	511.720384	9.525466
8.547977	498.479265	9.530483
8.143766	490.838919	9.535501
8.282336	491.686650	9.540519
8.408588	497.832405	9.545536
7.960798	490.349431	9.550554
8.085576	489.817113	9.555571
7.743119	488.216745	9.560589
8.179922	487.164050	9.565607
8.233973	484.326322	9.570624
8.033821	499.094541	9.575642
8.352173	493.581622	9.580659
8.345056	485.089971	9.585677
8.173859	469.035587	9.590695
8.077070	470.077400	9.595712
8.084111	476.412599	9.600730
7.860297	468.163621	9.605747
7.842705	470.770601	9.610765
8.077416	477.105177	9.615783
7.848536	468.258327	9.620800
7.694169	482.393291	9.625818
7.893396	484.574551	9.630835
8.045968	496.029951	9.635853
8.170909	485.704207	9.640871
8.538410	486.869158	9.645888
8.259362	478.295898	9.650906
8.425321	486.969370	9.655923
8.073046	493.559885	9.660941
8.089746	491.943856	9.665959
8.324851	487.499033	9.670976
8.041801	485.308245	9.675994
8.446030	483.966990	9.681011
8.195782	494.447711	9.686029
8.066401	484.089896	9.691047
8.111842	480.613747	9.696064
7.978107	493.719317	9.701082
8.473465	482.866598	9.706099
8.302742	487.096332	9.711117
7.982853	487.260122	9.716135
8.317735	480.567131	9.721152
8.127481	480.657538	9.726170
8.371705	490.081620	9.731187
7.927765	498.722743	9.736205
7.741240	482.344855	9.741223
7.993320	477.001920	9.746240
7.768383	482.228128	9.751258
7.723761	483.466992	9.756275
7.715447	493.336574	9.761293
8.097632	499.937878	9.766311
8.259992	513.110359	9.771328
8.032545	527.229394	9.776346
8.312668	517.902209	9.781363
8.237004	517.486661	9.786381
8.202817	517.870610	9.791399
8.378846	512.559420	9.796416
8.278746	523.390969	9.801434
8.134969	510.979190	9.806451
7.920321	522.572251	9.811469
7.912564	517.915925	9.816487
8.294035	509.051143	9.821504
8.019728	513.342679	9.826522
8.147292	511.771898	9.831539
8.553393	515.551949	9.836557
8.603429	520.706553	9.841575
8.761376	514.471253	9.846592
8.542445	521.415464	9.851610
8.328921	518.575697	9.856627
8.753609	518.378983	9.861645
8.485484	525.713540	9.866663
8.515918	524.927569	9.871680
8.403341	526.659470	9.876698
8.335613	529.811066	9.881715
8.628698	521.211134	9.886733
8.320400	518.768653	9.891751
8.765482	518.857985	9.896768
8.140741	522.356604	9.901786
8.674865	514.503414	9.906803
8.814860	515.102333	9.911821
8.353056	520.576716	9.916839
8.742027	511.170436	9.921856
8.487415	516.487765	9.926874
8.563101	512.055306	9.931891
8.786772	515.070963	9.936909
8.238306	521.379894	9.941927
8.375131	509.914382	9.946944
8.356889	526.872736	9.951962
8.490035	520.981826	9.956979
8.219029	516.770409	9.961997
8.177371	520.518866	9.967015
8.258288	519.617387	9.972032
8.491567	527.168145	9.977050
8.111830	519.679027	9.982067
8.533645	536.245434	9.987085
8.321683	539.948727	9.992103
8.558512	544.668407	9.997120
8.465264	558.801410	10.002138
8.752383	546.512749	10.007155
8.971408	534.291542	10.012173
8.910044	545.303876	10.017191
9.112444	534.087403	10.022208
8.758204	535.061845	10.027226
8.568838	525.850719	10.032243
8.632715	511.943173	10.037261
8.528667	519.527925	10.042279
8.729818	523.251017	10.047296
8.683382	530.738966	10.052314
8.831296	540.660011	10.057331
8.572819	534.329574	10.062349
8.676671	547.047760	10.067367
8.693834	539.638094	10.072384
8.861217	549.656992	10.077402
8.569541	542.393523	10.082419
9.078005	543.190560	10.087437
8.850750	536.016628	10.092455
8.818615	512.606867	10.097472
8.560938	515.248019	10.102490
8.509770	513.038981	10.107507
9.078881	524.414249	10.112525
8.903519	534.717789	10.117543
8.623317	513.253308	10.122560
8.813609	520.064155	10.127578
8.682682	533.051206	10.132595
8.919592	539.238325	10.137613
8.706559	546.474434	10.142631
8.899845	544.930971	10.147648
8.851196	536.995762	10.152666
8.708935	532.787372	10.157683
8.695894	542.182261	10.162701
8.986967	546.497477	10.167719
9.065956	552.971874	10.172736
9.192347	534.722659	10.177754
9.164338	522.882973	10.182771
9.040630	507.110413	10.187789
8.897782	521.612340	10.192807
8.998970	502.726400	10.197824
8.787114	518.360982	10.202842
8.868815	514.999678	10.207859
9.041646	509.761741	10.212877
8.750869	510.047174	10.217895
8.944339	501.224191	10.222912
9.136606	504.406621	10.227930
8.580562	515.513476	10.232947
8.940720	521.121758	10.237965
9.096668	536.054746	10.242983
9.008037	534.600090	10.248000
9.217284	530.513204	10.253018
8.761145	510.537876	10.258035
9.345206	522.812182	10.263053
8.866140	526.436013	10.268071
9.015064	517.324077	10.273088
9.321851	517.878310	10.278106
8.887686	513.933283	10.283123
9.430366	505.532128	10.288141
8.927041	515.997708	10.293159
8.904951	508.236242	10.298176
8.981335	518.021581	10.303194
8.986540	523.956782	10.308211
9.008668	521.754328	10.313229
8.938969	533.301497	10.318247
9.340820	537.158522	10.323264
9.503393	538.871720	10.328282
9.222537	532.079317	10.333299
9.476751	510.459213	10.338317
9.025921	506.304972	10.343335
9.143595	509.855473	10.348352
9.142576	520.129109	10.353370
9.117516	517.823351	10.358387
9.197706	518.976741	10.363405
9.192519	511.699204	10.368423
9.543677	522.036470	10.373440
9.536166	519.235085	10.378458
9.465678	519.566579	10.383475
9.723314	518.220715	10.388493
9.389145	521.240683	10.393511
9.351591	520.998627	10.398528
9.383913	517.987744	10.403546
9.250485	521.715744	10.408563
9.214233	511.862702	10.413581
8.797311	519.343084	10.418599
8.992216	515.982557	10.423616
9.079089	510.194064	10.428634
8.992550	510.661060	10.433651
9.289563	508.523200	10.438669
9.040315	523.214335	10.443687
9.445037	512.537175	10.448704
9.353628	515.610019	10.453722
9.172477	518.453742	10.458739
9.173865	512.352367	10.463757
9.179193	514.919057	10.468775
9.244964	509.916391	10.473792
9.062389	513.646705	10.478810
9.033503	536.547985	10.483827
9.460313	540.456782	10.488845
9.387658	541.208638	10.493863
9.451437	544.316855	10.498880
9.519249	540.994940	10.503898
9.233582	550.085048	10.508915
9.556943	546.531171	10.513933
9.333241	556.884537	10.518951
9.421923	546.764118	10.523968
9.648906	540.308184	10.528986
9.273505	554.566537	10.534003
9.570395	544.659896	10.539021
9.386587	550.574777	10.544039
9.115602	546.966884	10.549056
9.317377	533.516267	10.554074
9.201865	539.694021	10.559091
9.482255	539.194046	10.564109
9.314306	551.948691	10.569127
9.308743	546.830560	10.574144
9.538980	546.901371	10.579162
9.483153	544.112789	10.584179
9.581412	531.255950	10.589197
9.577329	535.988477	10.594215
9.581754	553.608154	10.599232
9.406728	544.943073	10.604250
9.627090	550.747666	10.609267
9.366396	530.591122	10.614285
9.507642	544.251480	10.619303
9.002599	542.045017	10.624320
9.608911	553.384833	10.629338
10.004617	573.874193	10.634355
9.918699	559.396778	10.639373
9.695492	553.088551	10.644391
9.622204	562.117884	10.649408
9.790698	542.449255	10.654426
9.733973	548.022424	10.659443
9.793815	538.320778	10.664461
9.675950	545.517935	10.669479
9.479020	548.083809	10.674496
9.907480	544.084785	10.679514
9.323208	540.677064	10.684531
9.684139	538.116999	10.689549
9.799200	549.764727	10.694567
9.500319	553.098891	10.699584
9.553947	563.313042	10.704602
9.539457	572.993473	10.709619
9.959578	561.581875	10.714637
9.969318	565.418879	10.719655
9.720853	577.013239	10.724672
9.918719	573.942513	10.729690
9.907641	568.589206	10.734707
9.698509	568.639238	10.739725
10.024970	554.979546	10.744743
9.809579	543.828862	10.749760
9.944153	547.870094	10.754778
9.783880	543.900855	10.759795
9.549609	539.716918	10.764813
9.676719	552.202566	10.769831
9.662048	564.385334	10.774848
9.930628	563.005379	10.779866
9.847135	573.495302	10.784883
9.997277	564.766830	10.789901
10.041490	564.107002	10.794919
10.123896	568.904661	10.799936
10.187784	561.346441	10.804954
9.849929	555.630680	10.809971
9.612608	548.430260	10.814989
9.861817	563.034926	10.820007
9.802685	562.707869	10.825024
10.250249	560.633099	10.830042
9.690573	567.372073	10.835059
9.734571	576.584556	10.840077
9.838419	567.034942	10.845095
9.821638	560.775851	10.850112
9.775532	557.578350	10.855130
9.966384	568.316482	10.860147
10.040046	569.497819	10.865165
9.963750	573.537396	10.870183
9.870708	574.628588	10.875200
10.072363	571.863088	10.880218
9.858558	570.719023	10.885235
9.823544	576.493007	10.890253
10.032456	564.640509	10.895271
10.061745	570.999723	10.900288
9.793785	564.716010	10.905306
9.808354	574.283490	10.910323
10.214108	585.596150	10.915341
10.528075	588.959041	10.920359
10.310140	590.889529	10.925376
10.278686	581.086625	10.930394
10.033581	583.451251	10.935411
10.252367	570.640493	10.940429
10.182307	571.597004	10.945447
10.110676	567.614783	10.950464
10.413099	567.465237	10.955482
10.367534	566.313347	10.960499
10.417754	562.597850	10.965517
10.057040	557.147630	10.970535
9.537767	562.816335	10.975552
9.989744	569.009650	10.980570
9.831465	574.750273	10.985587
9.786558	585.965490	10.990605
10.424859	598.485181	10.995623
10.222952	595.861847	11.000640
10.407721	590.040712	11.005658
9.988684	594.991805	11.010675
10.093687	590.056239	11.015693
10.593081	590.918841	11.020711
10.419847	600.859833	11.025728
10.264304	590.042276	11.030746
9.997509	586.447851	11.035763
10.237378	596.109487	11.040781
10.756761	581.643517	11.045799
10.150859	592.229232	11.050816
10.308015	594.194862	11.055834
10.293931	595.623240	11.060851
10.220612	594.198818	11.065869
10.108893	588.583149	11.070887
9.995309	601.703490	11.075904
10.419044	600.729115	11.080922
10.478230	595.203093	11.085939
10.306942	592.967545	11.090957
10.186014	591.439100	11.095975
10.324126	607.621442	11.100992
10.876948	614.090776	11.106010
10.487308	608.232792	11.111027
10.601579	603.575365	11.116045
10.791047	593.180923	11.121063
10.520409	590.316237	11.126080
10.908631	587.461645	11.131098
10.449450	603.593110	11.136115
10.303894	598.328639	11.141133
10.240878	595.612876	11.146151
10.067145	599.944990	11.151168
10.622401	610.999243	11.156186
10.924196	612.121824	11.161203
10.504196	604.847156	11.166221
10.621032	594.712507	11.171239
10.386644	599.932149	11.176256
10.551242	592.214777	11.181274
10.514879	603.850273	11.186291
10.552329	629.667976	11.191309
10.900188	631.641360	11.196327
10.588678	630.876564	11.201344
10.820896	616.173127	11.206362
10.383180	608.374311	11.211379
10.732793	615.964243	11.216397
11.146760	616.745410	11.221415
10.621770	607.204432	11.226432
10.590584	597.311922	11.231450
10.600082	598.970024	11.236467
10.632587	612.231163	11.241485
10.935300	609.735028	11.246503
10.773304	596.919175	11.251520
10.580851	586.972825	11.256538
10.615744	611.889011	11.261555
10.762013	613.166799	11.266573
10.822975	618.952788	11.271591
10.401323	619.910525	11.276608
10.985606	622.627872	11.281626
11.258959	620.382902	11.286643
11.327652	622.410490	11.291661
11.107480	595.907414	11.296679
11.042903	599.693334	11.301696
10.857449	582.324094	11.306714
11.475736	600.032700	11.311731
10.971188	591.021824	11.316749
10.615876	592.341267	11.321767
10.975622	595.399698	11.326784
10.834733	594.518632	11.331802
11.103648	587.541174	11.336819
10.837344	589.884407	11.341837
11.547326	592.133711	11.346855
11.193519	589.261415	11.351872
11.165346	592.307193	11.356890
11.241762	575.314198	11.361907
11.048306	563.386586	11.366925
11.218886	561.561885	11.371943
10.724270	565.190459	11.376960
10.549725	561.524702	11.381978
10.538997	571.552383	11.386995
10.354359	582.223564	11.392013
11.044122	589.647349	11.397031
10.881647	589.650603	11.402048
11.316186	588.857187	11.407066
11.132746	598.667112	11.412083
10.677670	592.984288	11.417101
10.869123	598.038592	11.422119
10.875749	602.776948	11.427136
10.819215	598.194887	11.432154
11.063210	593.015523	11.437171
10.917020	610.351056	11.442189
11.121396	596.144771	11.447207
10.903264	598.373173	11.452224
10.986895	596.542761	11.457242
11.538830	616.134169	11.462259
11.054545	613.973075	11.467277
11.024471	595.712840	11.472295
11.135541	602.907913	11.477312
11.145986	614.587346	11.482330
11.318034	629.314158	11.487347
11.083917	632.214087	11.492365
11.275671	632.040023	11.497383
11.423558	626.094677	11.502400
11.100703	619.605285	11.507418
11.272336	612.366283	11.512435
11.183344	627.050616	11.517453
11.432245	621.438814	11.522471
11.210155	613.116355	11.527488
11.274082	615.364868	11.532506
11.425563	613.519404	11.537523
11.426875	619.943882	11.542541
11.430483	611.115014	11.547559
11.504846	609.325594	11.552576
11.210540	600.950029	11.557594
11.270374	599.534796	11.562611
10.737728	601.274423	11.567629
11.373260	617.356663	11.572647
11.600441	622.380173	11.577664
11.682162	626.943851	11.582682
11.556414	618.397728	11.587699
11.454599	617.186835	11.592717
11.442636	601.399057	11.597735
11.241725	602.675961	11.602752
11.502363	612.377474	11.607770
11.486500	606.000123	11.612787
11.587671	613.235412	11.617805
11.198437	595.304465	11.622823
11.375267	613.923887	11.627840
11.432406	631.867463	11.632858
11.780703	621.086875	11.637875
11.598838	627.556389	11.642893
11.544180	606.129196	11.647911
11.682329	615.892876	11.652928
11.314348	615.084962	11.657946
11.729622	610.704112	11.662963
11.234286	621.148662	11.667981
11.561772	627.898604	11.672999
12.000794	631.772046	11.678016
11.864303	624.226343	11.683034
11.605634	600.361253	11.688051
11.248605	608.098466	11.693069
11.642634	605.676202	11.698087
11.693999	623.138916	11.703104
11.534223	635.600204	11.708122
11.626426	626.192020	11.713139
11.528630	626.209974	11.718157
11.731198	625.883164	11.723175
11.406735	636.150201	11.728192
11.019089	632.041774	11.733210
11.320870	629.049123	11.738227
11.125898	626.735608	11.743245
11.331730	629.099428	11.748263
11.673414	637.249935	11.753280
11.856261	654.391992	11.758298
11.772507	649.046633	11.763315
11.963139	652.482569	11.768333
11.657553	648.785404	11.773351
11.853604	641.148130	11.778368
11.612228	654.408708	11.783386
11.990532	643.353704	11.788403
11.933953	660.479340	11.793421
11.758866	647.766673	11.798439
11.784751	651.327259	11.803456
11.470538	656.565032	11.808474
11.701161	651.918575	11.813491
11.582802	660.180153	11.818509
11.767641	665.710787	11.823527
11.801141	657.097388	11.828544
11.560431	652.800429	11.833562
12.128063	653.066917	11.838579
11.935892	657.010134	11.843597
11.552364	650.162020	11.848615
11.622885	642.101373	11.853632
11.171358	650.769224	11.858650
12.101095	668.203642	11.863667
11.874505	674.017982	11.868685
12.158719	670.274713	11.873703
12.242805	666.802469	11.878720
12.219353	664.286026	11.883738
12.416595	662.163945	11.888755
12.256846	658.034086	11.893773
12.057811	639.918630	11.898791
12.068077	644.550706	11.903808
11.655541	640.283130	11.908826
12.223571	633.264290	11.913843
11.791735	641.372186	11.918861
12.020406	660.367381	11.923879
12.313604	664.652561	11.928896
12.241242	662.730912	11.933914
12.174388	645.781395	11.938931
12.017734	655.101481	11.943949
12.047968	663.211952	11.948967
12.373938	661.122919	11.953984
12.348395	660.819241	11.959002
12.205335	654.635597	11.964019
12.211470	653.433923	11.969037
11.970624	646.477601	11.974055
12.433489	656.232814	11.979072
12.370395	671.137083	11.984090
12.602538	652.094991	11.989107
12.240685	644.545779	11.994125
12.020791	651.032904	11.999143
12.397432	644.408322	12.004160
12.205558	644.400393	12.009178
12.289354	635.637675	12.014195
12.367383	641.979122	12.019213
12.589691	646.112359	12.024231
12.741480	646.031104	12.029248
12.302288	642.688444	12.034266
12.632036	642.831871	12.039283
12.461098	641.970726	12.044301
12.342972	637.468505	12.049319
12.381859	643.923982	12.054336
11.985506	647.277424	12.059354
12.065949	627.365801	12.064371
12.108290	647.362471	12.069389
12.067478	658.738651	12.074407
12.685555	669.771347	12.079424
12.324349	676.832726	12.084442
12.752534	673.898200	12.089459
12.509421	665.602510	12.094477
12.689117	663.652000	12.099495
12.857592	659.610001	12.104512
12.376631	668.637489	12.109530
12.751317	655.428519	12.114547
12.464284	649.077363	12.119565
12.315671	645.259787	12.124583
12.588758	658.695935	12.129600
12.267772	662.418750	12.134618
12.637478	670.439665	12.139635
12.741712	681.627746	12.144653
12.444639	676.805146	12.149671
12.623142	658.842201	12.154688
12.710887	669.873577	12.159706
12.776310	671.128418	12.164723
12.695762	667.926449	12.169741
13.072187	667.676795	12.174759
12.878159	657.884471	12.179776
12.466452	654.904723	12.184794
12.560405	659.394452	12.189811
12.683592	669.233559	12.194829
12.599282	673.321919	12.199847
12.839055	667.860304	12.204864
12.763301	666.940817	12.209882
12.589287	669.466906	12.214899
12.742742	673.862175	12.219917
12.543938	677.354011	12.224935
12.873279	671.431211	12.229952
12.658419	668.061904	12.234970
12.709858	670.456264	12.239987
12.833942	670.664579	12.245005
12.774749	673.292539	12.250023
12.960995	673.512034	12.255040
12.926504	673.081904	12.260058
12.699915	662.980444	12.265075
12.808132	665.269767	12.270093
12.854223	667.811836	12.275111
13.018995	665.244606	12.280128
12.696447	669.742155	12.285146
12.689796	657.999310	12.290163
12.903165	669.312039	12.295181
12.593711	670.518810	12.300199
12.723524	670.319160	12.305216
12.980427	683.774341	12.310234
12.528575	696.430476	12.315251
13.232227	696.505815	12.320269
13.164990	694.137918	12.325287
13.350264	695.193654	12.330304
13.438808	689.423023	12.335322
12.976217	669.340796	12.340339
13.644225	659.779178	12.345357
13.243907	667.225298	12.350375
13.459761	669.683417	12.355392
12.731814	668.504449	12.360410
13.361355	672.672247	12.365427
13.351982	669.826367	12.370445
13.394133	677.702239	12.375463
13.369980	661.926550	12.380480
13.088225	670.490483	12.385498
13.370182	668.261503	12.390515
13.254499	663.238291	12.395533
13.199284	666.522962	12.400551
13.392529	652.000703	12.405568
13.106729	672.420370	12.410586
13.289017	665.589355	12.415603
13.231231	664.494290	12.420621
13.254148	662.051471	12.425639
13.199923	660.335058	12.430656
13.022904	662.641799	12.435674
13.048177	665.539216	12.440691
13.349946	672.434348	12.445709
12.888656	670.110909	12.450727
13.317021	664.360298	12.455744
13.163516	664.134450	12.460762
12.976789	662.056141	12.465779
13.340093	654.955493	12.470797
13.071913	663.318001	12.475815
13.368986	685.921288	12.480832
13.232095	697.119312	12.485850
13.548137	695.119696	12.490867
13.367243	686.748959	12.495885
13.361887	694.683469	12.500903
13.589776	691.953468	12.505920
13.805707	689.203793	12.510938
13.853940	690.727573	12.515955
13.484850	659.451086	12.520973
13.225442	668.524033	12.525991
13.882585	674.152967	12.531008
13.420544	675.513082	12.536026
13.402625	673.840659	12.541043
13.736943	682.019569	12.546061
13.693988	678.185310	12.551079
13.523781	653.620103	12.556096
13.635657	674.870948	12.561114
13.710114	660.210663	12.566131
13.219609	663.327938	12.571149
13.474720	675.044137	12.576167
13.615067	685.615530	12.581184
13.888105	693.719351	12.586202
13.426975	694.971462	12.591219
13.823074	686.874405	12.596237
13.923142	693.238211	12.601255
13.827582	688.911547	12.606272
13.943425	694.605339	12.611290
14.051022	673.013370	12.616307
13.818299	672.839385	12.621325
13.397679	672.540377	12.626343
13.239981	664.348072	12.631360
13.743847	681.997939	12.636378
13.610964	687.440953	12.641395
13.498421	684.343858	12.646413
13.492304	694.385815	12.651431
13.632596	687.538702	12.656448
13.682460	690.729648	12.661466
13.639783	684.245002	12.666483
13.945118	686.375593	12.671501
13.291686	689.401315	12.676519
13.562964	700.171516	12.681536
13.724302	715.535113	12.686554
13.655670	717.508255	12.691571
14.277687	721.307096	12.696589
13.925182	713.907461	12.701607
13.944631	726.265889	12.706624
14.131411	726.951755	12.711642
14.107143	723.442492	12.716659
14.155272	720.988609	12.721677
13.884154	724.570935	12.726695
14.118184	718.584157	12.731712
14.175634	727.147175	12.736730
13.927075	721.053760	12.741747
14.186260	713.232620	12.746765
13.845396	722.883139	12.751783
13.925915	726.088708	12.756800
14.166666	724.239697	12.761818
14.228085	717.878361	12.766835
14.417044	714.943408	12.771853
14.154774	728.350589	12.776871
14.463636	707.636576	12.781888
14.061266	725.827332	12.786906
13.902978	719.799892	12.791923
14.057279	719.732590	12.796941
14.368354	725.578942	12.801959
14.460182	728.515364	12.806976
14.219308	722.234687	12.811994
14.140997	721.686817	12.817011
14.201950	716.668052	12.822029
13.944028	728.261235	12.827047
13.896017	723.812745	12.832064
14.431270	729.870239	12.837082
13.747989	731.656620	12.842099
14.167870	720.941482	12.847117
14.221509	734.642074	12.852135
14.164280	731.111490	12.857152
14.578517	725.767061	12.862170
14.193983	726.798283	12.867187
14.033201	727.731711	12.872205
14.468449	740.833704	12.877223
14.736621	749.628796	12.882240
14.505813	729.049994	12.887258
14.319713	716.153295	12.892275
14.408669	711.667610	12.897293
14.611445	724.396264	12.902311
14.464852	733.745636	12.907328
14.683080	715.104715	12.912346
14.423819	722.679691	12.917363
14.200841	721.424157	12.922381
14.801456	729.011538	12.927399
14.787506	735.010409	12.932416
14.583603	729.675627	12.937434
14.477116	725.357450	12.942451
14.561938	722.043903	12.947469
14.748258	724.699596	12.952487
14.366911	717.083109	12.957504
14.784569	723.103744	12.962522
14.885892	738.386746	12.967539
14.729267	717.109200	12.972557
14.858946	727.935887	12.977575
14.723459	723.320978	12.982592
14.694609	714.980799	12.987610
14.529999	716.621631	12.992627
14.648714	723.375413	12.997645
14.935846	723.173973	13.002663
14.388570	740.381380	13.007680
14.727236	730.201028	13.012698
14.965918	742.944823	13.017715
14.838172	742.513372	13.022733
14.715993	747.012274	13.027751
14.967624	753.184944	13.032768
15.046249	741.120513	13.037786
14.725579	736.083916	13.042803
15.110359	731.457227	13.047821
14.855736	727.865776	13.052839
14.312455	728.200123	13.057856
14.928382	736.138068	13.062874
15.049020	752.706458	13.067891
15.295044	745.416918	13.072909
15.507681	744.159461	13.077927
14.675518	734.433968	13.082944
14.846956	723.994886	13.087962
14.980574	730.444683	13.092979
15.271272	738.208067	13.097997
15.025262	731.113212	13.103015
14.599650	721.506534	13.108032
14.897745	728.563690	13.113050
14.589705	740.352141	13.118067
14.706441	739.601199	13.123085
14.896927	740.400017	13.128103
14.660796	745.707383	13.133120
15.220795	749.916415	13.138138
15.003294	753.408011	13.143155
15.363034	743.759513	13.148173
15.350953	738.652433	13.153191
14.946799	743.631522	13.158208
15.409513	738.988606	13.163226
14.995526	752.819634	13.168243
15.004074	749.872172	13.173261
15.439033	740.182903	13.178279
15.015768	742.931071	13.183296
15.061826	748.068793	13.188314
14.986724	753.160998	13.193331
15.226771	765.110426	13.198349
15.630195	767.878846	13.203367
15.250331	747.510252	13.208384
15.320758	746.595535	13.213402
15.372186	765.237831	13.218419
15.252956	772.588346	13.223437
15.561256	763.548238	13.228455
15.246908	752.113214	13.233472
15.672222	745.900949	13.238490
15.434261	746.978411	13.243507
15.228511	740.622445	13.248525
15.600287	751.561870	13.253543
15.588463	750.201963	13.258560
15.361540	734.555558	13.263578
15.278071	736.730334	13.268595
15.535250	747.228141	13.273613
15.672092	758.021387	13.278631
15.401402	775.273661	13.283648
15.721053	774.493515	13.288666
15.645947	768.134251	13.293683
15.498160	763.060612	13.298701
15.890045	746.079852	13.303719
15.721633	747.434749	13.308736
15.533420	736.463852	13.313754
15.915662	733.776041	13.318771
15.918096	738.818624	13.323789
15.907312	729.836187	13.328807
15.679979	732.948758	13.333824
15.880545	725.160327	13.338842
15.614341	735.296267	13.343859
15.728038	736.286485	13.348877
15.581989	741.309323	13.353895
15.464204	744.242205	13.358912
15.590320	728.008616	13.363930
15.961512	733.469311	13.368947
15.800060	731.916059	13.373965
15.812353	728.066360	13.378983
15.786143	740.866328	13.384000
15.880880	726.031003	13.389018
15.684308	732.817998	13.394035
15.583471	739.987535	13.399053
15.902010	750.758031	13.404071
15.705318	759.635855	13.409088
15.511420	764.599099	13.414106
15.969315	753.895173	13.419123
15.643278	759.852140	13.424141
15.930768	753.700437	13.429159
15.721729	773.649163	13.434176
16.314037	770.599321	13.439194
16.344546	766.200432	13.444211
16.093477	767.087967	13.449229
16.232175	755.021076	13.454247
16.031837	767.831146	13.459264
16.209686	761.047271	13.464282
16.291413	770.699626	13.469299
16.109868	770.947034	13.474317
16.479827	761.729442	13.479335
16.116254	753.909048	13.484352
16.124246	747.030632	13.489370
16.046529	750.037195	13.494387
16.208951	760.898645	13.499405
16.207500	755.279848	13.504423
15.806301	761.188025	13.509440
16.052544	769.160903	13.514458
16.121091	757.411657	13.519475
16.230124	763.241617	13.524493
16.144839	753.846744	13.529511
16.155722	767.409377	13.534528
16.337295	765.486099	13.539546
16.575762	766.465934	13.544563
16.456826	764.776736	13.549581
16.274120	760.418791	13.554599
16.455226	762.384717	13.559616
16.557824	766.508935	13.564634
16.200516	772.109520	13.569651
16.138085	763.729792	13.574669
16.231172	758.396896	13.579687
15.851772	763.100291	13.584704
16.431840	762.366859	13.589722
16.204092	758.150589	13.594739
16.046330	758.962477	13.599757
15.967746	762.647028	13.604775
16.210019	782.999649	13.609792
16.640257	788.106961	13.614810
16.969009	784.042969	13.619827
16.309369	785.636897	13.624845
16.690502	784.631074	13.629863
16.388637	791.196951	13.634880
16.926959	779.885521	13.639898
17.429862	783.417102	13.644915
16.607468	762.374693	13.649933
16.754121	753.213297	13.654951
16.519099	762.563719	13.659968
16.453885	754.901268	13.664986
16.426593	756.928400	13.670003
16.555384	775.148936	13.675021
16.791677	781.014556	13.680039
16.737590	785.452815	13.685056
17.086524	781.042435	13.690074
17.132230	775.258579	13.695091
16.652943	763.273339	13.700109
16.571379	757.787446	13.705127
16.409143	757.739585	13.710144
16.691569	775.175014	13.715162
16.737025	776.453632	13.720179
16.581660	783.815044	13.725197
17.040588	780.460524	13.730215
16.834295	789.881203	13.735232
16.808707	793.145849	13.740250
16.761317	782.981237	13.745267
16.621881	787.528861	13.750285
16.733944	785.905013	13.755303
16.662513	785.752987	13.760320
16.742477	784.072446	13.765338
16.824287	790.097239	13.770355
16.960826	805.807292	13.775373
17.018347	809.172756	13.780391
17.207583	809.960172	13.785408
17.018906	813.375377	13.790426
17.587196	796.441381	13.795443
16.947951	786.225190	13.800461
17.152782	777.384820	13.805479
17.076098	794.420636	13.810496
17.426704	785.569949	13.815514
17.275639	772.412532	13.820531
17.090178	770.636902	13.825549
17.223432	775.731095	13.830567
17.296288	781.956348	13.835584
17.026053	792.150069	13.840602
17.454346	772.201735	13.845619
17.357124	774.846036	13.850637
17.320637	758.344452	13.855655
17.161326	777.412667	13.860672
17.231684	777.558811	13.865690
17.756135	773.901976	13.870707
17.411651	779.479581	13.875725
17.737460	777.332105	13.880743
17.642217	772.204314	13.885760
17.694591	772.547689	13.890778
17.964665	756.828183	13.895795
17.825148	768.500041	13.900813
17.686554	764.771118	13.905831
17.697798	753.600542	13.910848
17.578773	747.590418	13.915866
17.812498	755.758436	13.920883
17.577868	745.736584	13.925901
17.392772	742.770935	13.930919
17.602294	747.829684	13.935936
17.621876	743.437527	13.940954
17.373155	731.535646	13.945971
17.216458	747.916831	13.950989
17.534473	741.346574	13.956007
17.497862	748.264989	13.961024
17.341387	755.716123	13.966042
17.399081	767.730328	13.971059
17.665904	783.350729	13.976077
17.494857	776.600887	13.981095
17.650604	775.937773	13.986112
17.344985	783.095706	13.991130
17.852495	777.738994	13.996147
17.761422	781.250249	14.001165
17.406331	772.349485	14.006183
17.078706	782.300166	14.011200
17.454964	771.178884	14.016218
17.369318	782.061662	14.021235
17.704033	805.563286	14.026253
17.727909	815.351586	14.031271
17.550585	813.657073	14.036288
17.660307	811.761803	14.041306
18.058593	812.458775	14.046323
17.666081	809.654535	14.051341
17.738598	810.347872	14.056359
17.613710	815.129480	14.061376
17.983353	808.942922	14.066394
17.765035	810.804417	14.071411
17.827156	811.655155	14.076429
18.022964	821.262709	14.081447
18.321927	824.784702	14.086464
18.093285	826.375114	14.091482
18.096365	803.707297	14.096499
17.818707	815.598247	14.101517
18.199734	825.896733	14.106535
18.174075	816.857461	14.111552
18.280475	820.632499	14.116570
17.795829	807.214088	14.121587
18.124056	835.137379	14.126605
18.328752	834.143390	14.131623
18.429807	832.332607	14.136640
18.218421	833.873522	14.141658
18.441650	822.619446	14.146675
17.983115	822.149562	14.151693
18.299626	815.314210	14.156711
18.505250	826.598813	14.161728
18.016061	828.654459	14.166746
18.182045	823.621452	14.171763
18.334742	832.991294	14.176781
18.400211	831.315111	14.181799
18.447434	832.780223	14.186816
18.350302	840.380031	14.191834
18.896892	822.597366	14.196851
18.678372	828.263407	14.201869
18.041928	817.616288	14.206887
18.144102	819.520474	14.211904
18.429779	832.353413	14.216922
18.517037	823.123851	14.221939
18.608277	834.593280	14.226957
18.270617	835.557323	14.231975
18.561008	825.972784	14.236992
18.435232	830.189870	14.242010
18.876993	821.984032	14.247027
18.317715	835.715738	14.252045
18.568095	834.880315	14.257063
18.682840	825.376370	14.262080
18.466449	834.818427	14.267098
18.871129	821.374671	14.272115
18.510151	830.300154	14.277133
18.899281	831.504859	14.282151
18.889793	825.333712	14.287168
18.673204	849.395135	14.292186
18.606242	832.604263	14.297203
18.622869	819.961133	14.302221
18.300599	827.204502	14.307239
18.576492	829.084705	14.312256
18.759756	840.513936	14.317274
19.060041	837.580243	14.322291
18.709692	834.856025	14.327309
18.507412	828.964139	14.332327
18.660553	840.208417	14.337344
18.818385	864.075922	14.342362
18.858467	859.812213	14.347379
19.231438	867.363082	14.352397
19.069072	869.417077	14.357415
18.815627	859.895032	14.362432
18.661974	864.022850	14.367450
18.841511	866.460629	14.372467
18.887974	864.940315	14.377485
19.007271	863.815382	14.382503
19.083609	855.537258	14.387520
18.819947	868.497027	14.392538
19.033695	866.518821	14.397555
19.017082	867.640604	14.402573
18.881548	867.548769	14.407591
18.958872	872.097796	14.412608
18.716369	867.001001	14.417626
19.224895	887.162736	14.422643
19.381748	897.238710	14.427661
19.254017	895.506076	14.432679
19.425809	899.814141	14.437696
19.600128	892.972927	14.442714
19.413757	879.524252	14.447731
19.633881	869.795417	14.452749
19.401454	859.932747	14.457767
19.208188	847.702961	14.462784
19.273096	854.515291	14.467802
19.399975	859.405086	14.472819
19.140076	868.572901	14.477837
19.349107	885.834394	14.482855
19.551125	885.399419	14.487872
19.626193	883.183933	14.492890
19.324852	876.853548	14.497907
19.464886	882.496767	14.502925
19.753503	893.425631	14.507943
19.942342	881.452899	14.512960
19.744659	874.322239	14.517978
19.559258	855.901369	14.522995
19.352729	867.584770	14.528013
19.628578	861.259778	14.533031
19.794195	855.828852	14.538048
19.013446	857.915954	14.543066
19.369687	867.902276	14.548083
19.484457	876.499795	14.553101
19.404374	889.453649	14.558119
19.859034	882.075833	14.563136
19.828327	885.458060	14.568154
19.763813	877.686984	14.573171
19.880321	886.197620	14.578189
19.927494	888.694672	14.583207
19.884973	882.925159	14.588224
20.153218	885.258925	14.593242
19.708222	884.953311	14.598259
19.966841	877.684457	14.603277
19.704349	885.686555	14.608295
20.021471	882.704804	14.613312
19.575130	891.119904	14.618330
19.513977	891.622966	14.623347
19.841029	885.688654	14.628365
19.434731	891.672712	14.633383
20.055042	874.218697	14.638400
20.023019	886.277737	14.643418
20.029472	877.911166	14.648435
20.124119	878.492402	14.653453
19.875459	878.903241	14.658471
20.323077	879.649536	14.663488
19.785019	879.363237	14.668506
19.984612	885.467604	14.673523
20.235779	911.766425	14.678541
20.578492	913.293720	14.683559
20.491908	886.451284	14.688576
20.469379	890.490522	14.693594
20.403439	877.560052	14.698611
20.666496	870.250908	14.703629
20.138477	873.210867	14.708647
20.802777	875.356168	14.713664
20.596715	886.647244	14.718682
20.118592	879.248606	14.723699
20.348946	870.570671	14.728717
20.249652	868.713674	14.733735
20.354732	872.899116	14.738752
20.399855	878.184651	14.743770
20.214276	878.172925	14.748787
20.515516	875.387076	14.753805
20.101675	872.747741	14.758823
20.177506	881.150745	14.763840
20.291998	886.988511	14.768858
20.141292	884.103752	14.773875
20.811048	892.622950	14.778893
20.567116	907.826976	14.783911
20.828866	903.771664	14.788928
20.524414	904.379884	14.793946
20.414240	895.776317	14.798963
20.665052	903.520396	14.803981
20.492520	916.837923	14.808999
20.712431	891.521357	14.814016
20.694498	914.056977	14.819034
20.527047	918.083957	14.824051
20.948855	916.568529	14.829069
20.521961	920.019187	14.834087
20.910862	910.758618	14.839104
20.980262	912.677286	14.844122
20.820162	918.614568	14.849139
21.146655	916.076862	14.854157
20.420683	920.765345	14.859175
20.837898	908.068343	14.864192
20.711706	917.686853	14.869210
20.631356	912.267819	14.874227
21.023381	911.641232	14.879245
20.792159	924.137490	14.884263
20.585382	919.644916	14.889280
21.171018	912.726863	14.894298
20.980109	917.289724	14.899315
20.916530	905.555113	14.904333
20.674350	923.832998	14.909351
20.689873	915.727466	14.914368
20.925811	925.321958	14.919386
21.246231	938.669440	14.924403
21.381846	927.142803	14.929421
21.120647	917.270285	14.934439
20.902769	916.231379	14.939456
20.940766	932.630381	14.944474
21.306984	935.143800	14.949491
21.641557	939.459616	14.954509
21.076992	937.002437	14.959527
21.328847	938.394182	14.964544
21.514613	935.853749	14.969562
21.377670	943.620594	14.974579
21.542658	921.961517	14.979597
21.174391	914.552383	14.984615
21.400502	908.485947	14.989632
21.257298	920.966672	14.994650
21.277275	937.937074	14.999667
21.391983	936.764673	15.004685
21.428948	937.543013	15.009703
21.387974	936.113902	15.014720
21.772863	940.254696	15.019738
21.491734	948.166810	15.024755
21.471114	940.084558	15.029773
21.945531	947.332919	15.034791
21.596709	935.920972	15.039808
21.637321	937.539722	15.044826
21.396565	940.928330	15.049843
22.045022	930.169173	15.054861
21.627420	945.952838	15.059879
21.752815	945.774975	15.064896
21.638343	936.361589	15.069914
21.382707	942.884069	15.074931
21.894878	938.120733	15.079949
21.429902	945.803425	15.084967
21.690662	952.162040	15.089984
21.763468	933.643494	15.095002
21.289250	937.507033	15.100019
21.383201	944.553543	15.105037
21.129058	935.128796	15.110055
21.364215	945.271574	15.115072
21.853647	960.958305	15.120090
21.942723	967.435245	15.125107
22.296861	972.342827	15.130125
22.252940	969.013501	15.135143
22.311915	965.085763	15.140160
22.091158	963.313581	15.145178
21.919687	976.613073	15.150195
22.255038	962.566964	15.155213
22.133332	960.295416	15.160231
21.811924	952.856082	15.165248
22.272476	969.019964	15.170266
22.139008	975.659059	15.175283
21.919343	974.143153	15.180301
21.840822	967.862312	15.185319
21.788955	970.524737	15.190336
22.221636	969.723542	15.195354
21.918717	972.777599	15.200371
22.357508	972.903798	15.205389
22.041976	960.698260	15.210407
21.708048	959.498831	15.215424
22.331429	964.776027	15.220442
22.105711	976.566799	15.225459
22.230787	985.464993	15.230477
22.351523	993.619728	15.235495
22.378778	992.244288	15.240512
22.540732	994.276195	15.245530
22.557434	990.432197	15.250547
22.564709	986.866685	15.255565
22.701046	1000.980556	15.260583
22.698600	994.640288	15.265600
22.584180	967.961736	15.270618
22.251112	972.459339	15.275635
22.708175	982.456432	15.280653
22.407730	983.670201	15.285671
22.259021	993.987848	15.290688
22.660456	993.430953	15.295706
22.288724	994.768100	15.300723
22.890650	984.818444	15.305741
22.850854	996.561383	15.310759
22.297114	993.608385	15.315776
22.572675	995.364864	15.320794
22.638173	992.693334	15.325811
22.605339	991.660649	15.330829
22.386490	988.588342	15.335847
22.392570	1010.702087	15.340864
22.977705	1015.691570	15.345882
23.121596	1028.226891	15.350899
23.346902	1011.607768	15.355917
23.089978	995.254743	15.360935
22.983198	987.233942	15.365952
23.277181	981.765619	15.370970
23.064233	995.848244	15.375987
23.078197	984.694174	15.381005
23.018341	990.232691	15.386023
22.832273	984.911208	15.391040
23.043487	990.916663	15.396058
22.943470	993.972031	15.401075
23.419279	995.299217	15.406093
22.969219	990.241010	15.411111
22.866984	989.974405	15.416128
23.052804	995.628403	15.421146
23.022210	1016.342718	15.426163
23.020679	1026.120787	15.431181
23.147272	1017.126108	15.436199
23.332096	1009.651703	15.441216
23.422264	1019.248890	15.446234
23.041818	1023.922226	15.451251
23.328421	1025.817414	15.456269
22.997111	1023.511410	15.461287
22.829502	1027.139486	15.466304
23.206710	1022.554508	15.471322
23.282883	1025.031635	15.476339
23.394817	1038.248917	15.481357
23.703165	1041.251178	15.486375
23.329521	1039.118286	15.491392
23.900160	1040.933864	15.496410
23.699967	1049.375095	15.501427
23.601736	1026.809113	15.506445
23.738064	1023.116573	15.511463
23.382240	1026.126832	15.516480
24.014321	1014.093936	15.521498
23.688869	1015.004798	15.526515
23.917553	1015.546765	15.531533
23.519142	1010.520562	15.536551
23.597393	1016.532451	15.541568
23.779674	1014.502546	15.546586
23.692458	1020.439237	15.551603
23.469408	1022.138964	15.556621
23.777283	1016.947229	15.561639
23.978404	1036.337444	15.566656
23.975731	1026.521922	15.571674
23.751834	1036.187751	15.576691
24.042339	1038.856592	15.581709
24.012820	1042.983626	15.586727
23.676168	1038.586681	15.591744
23.674957	1039.604372	15.596762
23.829603	1037.117286	15.601779
23.863218	1051.247588	15.606797
23.954046	1042.659338	15.611815
23.759940	1042.832065	15.616832
23.924017	1027.965702	15.621850
24.062425	1033.851532	15.626867
23.972863	1041.433064	15.631885
23.904338	1038.464036	15.636903
23.663597	1042.462024	15.641920
24.129425	1058.914850	15.646938
24.461655	1056.287604	15.651955
24.805347	1060.162641	15.656973
24.254866	1041.760154	15.661991
24.217751	1027.163029	15.667008
24.285887	1023.996052	15.672026
24.643326	1042.366887	15.677043
24.333032	1044.177477	15.682061
24.496541	1026.672223	15.687079
24.279748	1035.439568	15.692096
24.605266	1032.479625	15.697114
24.476388	1031.523429	15.702131
24.508656	1027.962635	15.707149
24.395276	1031.213694	15.712167
24.467090	1043.161420	15.717184
25.008037	1046.051239	15.722202
24.956760	1027.449557	15.727219
24.739003	1030.039618	15.732237
24.709281	1026.516820	15.737255
24.632892	1029.096903	15.742272
24.421047	1025.593573	15.747290
24.480021	1020.395929	15.752307
24.707461	1032.372842	15.757325
24.994461	1035.579191	15.762343
24.799721	1044.667849	15.767360
24.977725	1027.795933	15.772378
25.197199	1023.199822	15.777395
24.659649	1016.711395	15.782413
25.226761	1019.104044	15.787431
25.076893	1029.900183	15.792448
24.906827	1027.064063	15.797466
24.669472	1031.658054	15.802483
24.912041	1027.078004	15.807501
24.563337	1018.978482	15.812519
24.556206	1036.604165	15.817536
24.972324	1049.132700	15.822554
25.069215	1064.458485	15.827571
25.113211	1050.129586	15.832589
25.032077	1052.261310	15.837607
24.870898	1049.006651	15.842624
25.016364	1058.521507	15.847642
24.984119	1059.459497	15.852659
24.986580	1052.685977	15.857677
25.120336	1048.117408	15.862695
24.828783	1044.446170	15.867712
25.053047	1053.277625	15.872730
25.027717	1060.287807	15.877747
25.153263	1080.253083	15.882765
25.422338	1078.157652	15.887783
25.438562	1076.309882	15.892800
25.330772	1081.592808	15.897818
25.718340	1083.599056	15.902835
25.494612	1082.502451	15.907853
25.747936	1092.499235	15.912871
25.503373	1078.415016	15.917888
25.347707	1066.807885	15.922906
25.370877	1065.575022	15.927923
25.801650	1083.272466	15.932941
25.882162	1078.858925	15.937959
25.655863	1075.611283	15.942976
25.689923	1062.652322	15.947994
25.698648	1049.252349	15.953011
25.526817	1046.542285	15.958029
25.423091	1059.035100	15.963047
25.577469	1081.143925	15.968064
25.589221	1070.159229	15.973082
25.922212	1065.109369	15.978099
25.716226	1080.732037	15.983117
25.896659	1079.913869	15.988135
25.835709	1076.922719	15.993152
25.786747	1074.864887	15.998170
26.127812	1083.360371	16.003187
25.817992	1080.310756	16.008205
26.154613	1071.035309	16.013223
25.821249	1083.609000	16.018240
26.006000	1079.748427	16.023258
26.368444	1073.993404	16.028275
26.213197	1072.571946	16.033293
26.216171	1074.885808	16.038311
26.140960	1075.362266	16.043328
26.072941	1076.081004	16.048346
26.159188	1071.571060	16.053363
25.767750	1071.885240	16.058381
26.305382	1077.258524	16.063399
25.915417	1077.566555	16.068416
25.915012	1080.227581	16.073434
26.133275	1076.514796	16.078451
25.995525	1079.769499	16.083469
26.675108	1084.891604	16.088487
26.301846	1089.171112	16.093504
26.384658	1080.637110	16.098522
26.384148	1088.230716	16.103539
26.262827	1104.466493	16.108557
26.408426	1105.824836	16.113575
26.326962	1114.183498	16.118592
26.386811	1103.524248	16.123610
26.727056	1106.262429	16.128627
26.296922	1119.058016	16.133645
26.377528	1116.410933	16.138663
26.329186	1119.459558	16.143680
26.172262	1106.892504	16.148698
26.513252	1098.317402	16.153715
26.825940	1095.071026	16.158733
26.740201	1104.814839	16.163751
26.978075	1107.033399	16.168768
26.787624	1104.846014	16.173786
27.046795	1105.667552	16.178803
27.240683	1109.926559	16.183821
26.700630	1110.083828	16.188839
26.694965	1111.167014	16.193856
26.545001	1104.602493	16.198874
26.981850	1104.825458	16.203891
26.703135	1097.927739	16.208909
26.951813	1088.869739	16.213927
26.450732	1105.406232	16.218944
26.970245	1119.458465	16.223962
27.073427	1125.572955	16.228979
27.018108	1139.828650	16.233997
26.943764	1135.488709	16.239015
27.286199	1135.866233	16.244032
26.969467	1132.465830	16.249050
27.173352	1126.351021	16.254067
27.156411	1138.789406	16.259085
27.533612	1125.319617	16.264103
27.421911	1124.115138	16.269120
27.167131	1131.235897	16.274138
27.709458	1131.411711	16.279155
27.513695	1132.178921	16.284173
27.692175	1126.683972	16.289191
27.514444	1126.545966	16.294208
27.449202	1112.553324	16.299226
27.434327	1112.314203	16.304243
27.633014	1123.305527	16.309261
27.328678	1125.946521	16.314279
27.785019	1121.143544	16.319296
27.529921	1112.196731	16.324314
27.525666	1106.688686	16.329331
27.669013	1122.600272	16.334349
27.455488	1122.907883	16.339367
27.627723	1118.920254	16.344384
27.841041	1117.927578	16.349402
28.124165	1120.331746	16.354419
27.873664	1124.469537	16.359437
27.975204	1103.155289	16.364455
27.966772	1090.290322	16.369472
27.521783	1087.078030	16.374490
27.594395	1100.683109	16.379507
27.885470	1120.001880	16.384525
27.976481	1118.141156	16.389543
28.181744	1117.578492	16.394560
27.791629	1115.879942	16.399578
28.017724	1125.128007	16.404595
28.127265	1119.378742	16.409613
28.104067	1118.702082	16.414631
28.116390	1109.716982	16.419648
27.901475	1129.316204	16.424666
27.821820	1126.339748	16.429683
28.010569	1124.382765	16.434701
28.071986	1110.074550	16.439719
28.050266	1108.750100	16.444736
27.961575	1125.512125	16.449754
28.470315	1116.111174	16.454771
28.128281	1125.900897	16.459789
27.929510	1121.995834	16.464807
28.359865	1117.740384	16.469824
28.047174	1118.399375	16.474842
28.129008	1124.077494	16.479859
28.005203	1140.893756	16.484877
28.438177	1149.856305	16.489895
28.473215	1145.282764	16.494912
28.606560	1156.935214	16.499930
28.526133	1153.536891	16.504947
28.347691	1153.520245	16.509965
28.692964	1149.919309	16.514983
28.865865	1146.514356	16.520000
28.434152	1152.463742	16.525018
28.649962	1148.333687	16.530035
28.711573	1168.741868	16.535053
28.731775	1147.181981	16.540071
28.743126	1143.170348	16.545088
28.562928	1147.404189	16.550106
28.861839	1154.851904	16.555123
28.687262	1153.751699	16.560141
28.434089	1153.343128	16.565159
28.685693	1143.037541	16.570176
28.420288	1147.159694	16.575194
28.635263	1153.206318	16.580211
28.925335	1178.821111	16.585229
29.102807	1175.492748	16.590247
29.540372	1176.868784	16.595264
29.210085	1165.674438	16.600282
29.387422	1156.503993	16.605299
28.960538	1150.041899	16.610317
29.120640	1153.300145	16.615335
29.166264	1144.780126	16.620352
28.716519	1151.633942	16.625370
29.586073	1160.783763	16.630387
29.385183	1163.587565	16.635405
29.323150	1149.504804	16.640423
29.757343	1143.577882	16.645440
28.937015	1150.822026	16.650458
29.217860	1143.633616	16.655475
29.018820	1163.048984	16.660493
29.170952	1165.969620	16.665511
29.149540	1161.949422	16.670528
29.179196	1168.394343	16.675546
29.445805	1167.818587	16.680563
29.680426	1175.926651	16.685581
29.726477	1169.943601	16.690599
29.536413	1161.117490	16.695616
29.500287	1172.070892	16.700634
29.778143	1160.501089	16.705651
29.484986	1161.794168	16.710669
29.331124	1169.407645	16.715687
29.677552	1176.471389	16.720704
29.381659	1177.454334	16.725722
29.579650	1179.636785	16.730739
30.078848	1184.383671	16.735757
30.206866	1198.381792	16.740775
30.214133	1182.416346	16.745792
29.783960	1178.071228	16.750810
30.157912	1171.760012	16.755827
30.172320	1168.207844	16.760845
29.713348	1164.531374	16.765863
30.077643	1160.757630	16.770880
30.096364	1166.904006	16.775898
30.100270	1161.123370	16.780915
29.968812	1168.207430	16.785933
29.748668	1179.176879	16.790951
30.453172	1193.029931	16.795968
30.009593	1203.902875	16.800986
30.497900	1199.690574	16.806003
30.419506	1193.529092	16.811021
29.765080	1203.057538	16.816039
30.215081	1201.506327	16.821056
30.390392	1202.727897	16.826074
30.379456	1193.019131	16.831091
30.279257	1203.026581	16.836109
30.290739	1200.408818	16.841127
30.386735	1202.454409	16.846144
30.546528	1201.725854	16.851162
30.559450	1185.467384	16.856179
30.797842	1194.548521	16.861197
30.633474	1208.212934	16.866215
30.726814	1196.459452	16.871232
30.774159	1204.747671	16.876250
30.789986	1192.998931	16.881267
30.848687	1199.994502	16.886285
30.652268	1201.748698	16.891303
30.534603	1197.802067	16.896320
30.234174	1203.108208	16.901338
30.396041	1197.009369	16.906355
30.552889	1196.924718	16.911373
30.482107	1209.783026	16.916391
30.426089	1214.275066	16.921408
30.631699	1216.374189	16.926426
31.018076	1218.611526	16.931443
30.898364	1218.400751	16.936461
30.840234	1222.592593	16.941479
31.391436	1230.981198	16.946496
30.966179	1223.002275	16.951514
30.868986	1209.677925	16.956531
30.805345	1219.672652	16.961549
30.930492	1227.518360	16.966567
31.115411	1221.820568	16.971584
31.123732	1223.992447	16.976602
31.498404	1220.731275	16.981619
31.277957	1209.879130	16.986637
31.113266	1220.848695	16.991655
31.264557	1236.186722	16.996672
31.414315	1243.344407	17.001690
31.411611	1246.942724	17.006707
31.696301	1246.665906	17.011725
31.591690	1240.760476	17.016743
31.578534	1231.232935	17.021760
31.498723	1248.858865	17.026778
31.415268	1250.684150	17.031795
31.618219	1248.856086	17.036813
31.470747	1251.240303	17.041831
31.707388	1230.195247	17.046848
31.718779	1241.081602	17.051866
31.825642	1241.303596	17.056883
31.700578	1240.608336	17.061901
31.675053	1242.819467	17.066919
31.837746	1245.655313	17.071936
31.998534	1235.784696	17.076954
31.661557	1237.583971	17.081971
31.561851	1235.704756	17.086989
31.364312	1245.520079	17.092007
31.864734	1234.098850	17.097024
31.777966	1239.669065	17.102042
31.652813	1244.836427	17.107059
32.067552	1252.163094	17.112077
31.974112	1258.612255	17.117095
32.303497	1257.453166	17.122112
32.335524	1255.851550	17.127130
32.313571	1261.562026	17.132147
32.557696	1269.599090	17.137165
32.376782	1251.359264	17.142183
32.511188	1236.903061	17.147200
32.495493	1231.223066	17.152218
32.170493	1226.330112	17.157235
32.449562	1226.614975	17.162253
32.301279	1228.318705	17.167271
32.341848	1222.048785	17.172288
32.149414	1222.537336	17.177306
32.092465	1248.809120	17.182323
32.440897	1258.892644	17.187341
32.318914	1270.396257	17.192359
32.534904	1265.364487	17.197376
32.602624	1273.654101	17.202394
32.596176	1269.875661	17.207411
32.698532	1264.515078	17.212429
32.365054	1266.740691	17.217447
32.798443	1260.451109	17.222464
32.758209	1267.125309	17.227482
32.440808	1279.682742	17.232499
32.641627	1262.308439	17.237517
32.261557	1263.198620	17.242535
32.521983	1290.776117	17.247552
32.904713	1287.723218	17.252570
33.117467	1282.821882	17.257587
33.402078	1284.579261	17.262605
33.477586	1285.524061	17.267623
33.417975	1284.002340	17.272640
33.500703	1279.737176	17.277658
33.375085	1275.742239	17.282675
33.387116	1257.969077	17.287693
33.137306	1257.865812	17.292711
33.413450	1245.397725	17.297728
33.393959	1247.059507	17.302746
33.346064	1255.474108	17.307763
33.431793	1248.254318	17.312781
33.354961	1254.682035	17.317799
33.242316	1246.627033	17.322816
33.376106	1258.885509	17.327834
33.145314	1261.474023	17.332851
33.197943	1249.026533	17.337869
33.206441	1261.749752	17.342887
33.261838	1263.248983	17.347904
33.534961	1281.457881	17.352922
33.552155	1289.917052	17.357939
33.765292	1286.664650	17.362957
33.766809	1287.367774	17.367975
33.885005	1283.469730	17.372992
33.424005	1277.441118	17.378010
33.751253	1280.796359	17.383027
33.918858	1280.967968	17.388045
33.905915	1286.076452	17.393063
33.895509	1280.655964	17.398080
34.313348	1275.654999	17.403098
34.025510	1276.515768	17.408115
34.409701	1264.888556	17.413133
33.838694	1263.533817	17.418151
34.132358	1270.991510	17.423168
33.929024	1267.621739	17.428186
34.011668	1268.576972	17.433203
34.129951	1266.458017	17.438221
34.129075	1279.381198	17.443239
33.998367	1275.458747	17.448256
33.900585	1269.707078	17.453274
33.725204	1282.229235	17.458291
34.055881	1268.614863	17.463309
33.983959	1278.424998	17.468327
34.214765	1297.097344	17.473344
34.425897	1301.657256	17.478362
34.123770	1295.522470	17.483379
34.317702	1296.862608	17.488397
34.126161	1296.950082	17.493415
34.322069	1305.799163	17.498432
34.259788	1290.497770	17.503450
34.190158	1309.883867	17.508467
34.788567	1306.917355	17.513485
34.777061	1325.125119	17.518503
35.147864	1322.327892	17.523520
35.325277	1311.461299	17.528538
34.701594	1300.478704	17.533555
35.284454	1288.610599	17.538573
35.076606	1288.577161	17.543591
34.835341	1290.162816	17.548608
35.166609	1292.843271	17.553626
35.198511	1281.246906	17.558643
35.497241	1274.346976	17.563661
34.958136	1273.346170	17.568679
34.992339	1269.402372	17.573696
35.129549	1265.660422	17.578714
35.085317	1274.571213	17.583731
35.349212	1272.074894	17.588749
34.967362	1273.742630	17.593767
35.159659	1273.741479	17.598784
35.417521	1273.701544	17.603802
35.208267	1282.165263	17.608819
35.222387	1267.592706	17.613837
35.277028	1263.553812	17.618855
35.225467	1275.614222	17.623872
35.969791	1268.315505	17.628890
35.543255	1277.214878	17.633907
35.907144	1274.393413	17.638925
35.303030	1282.136463	17.643943
35.541906	1285.082742	17.648960
35.486732	1274.290630	17.653978
35.420695	1290.777866	17.658995
35.398776	1275.111400	17.664013
35.586836	1278.348913	17.669031
35.659809	1268.176883	17.674048
35.692596	1265.423912	17.679066
35.463218	1278.279356	17.684083
35.740804	1286.548467	17.689101
35.947590	1296.742224	17.694119
35.509114	1316.093232	17.699136
36.271759	1306.818297	17.704154
36.226176	1315.548847	17.709171
36.445183	1300.224579	17.714189
36.171932	1292.345287	17.719207
35.921802	1288.581131	17.724224
35.953853	1279.305898	17.729242
35.796366	1288.265331	17.734259
35.945577	1309.625240	17.739277
36.013534	1310.556134	17.744295
35.897601	1312.253543	17.749312
36.405054	1311.204376	17.754330
35.948385	1313.241915	17.759347
36.318557	1307.904963	17.764365
36.418032	1305.639326	17.769383
36.103225	1301.842554	17.774400
36.537705	1305.054310	17.779418
36.360626	1320.782666	17.784435
36.664923	1329.003100	17.789453
36.523117	1333.936464	17.794471
36.864288	1338.485526	17.799488
36.791986	1333.273845	17.804506
36.483671	1330.779961	17.809523
36.570602	1334.790008	17.814541
36.877674	1334.668525	17.819559
36.451585	1336.204816	17.824576
36.816901	1332.815066	17.829594
36.666114	1322.073558	17.834611
36.671102	1325.156909	17.839629
36.590841	1329.139472	17.844647
36.902608	1339.410976	17.849664
36.985540	1335.158359	17.854682
36.913046	1336.602954	17.859699
36.804347	1335.294826	17.864717
36.916145	1341.731167	17.869735
36.866963	1359.096485	17.874752
37.358255	1358.031878	17.879770
37.383997	1360.542586	17.884787
37.431901	1365.121421	17.889805
37.517299	1366.044713	17.894823
37.329228	1374.872456	17.899840
37.365108	1349.609956	17.904858
37.824986	1356.357829	17.909875
37.340654	1328.374203	17.914893
37.222364	1331.412581	17.919911
37.602358	1352.573015	17.924928
37.715780	1351.139411	17.929946
37.516817	1358.327812	17.934963
37.686805	1354.895345	17.939981
37.389514	1353.199142	17.944999
37.612766	1368.365586	17.950016
37.924287	1360.234525	17.955034
37.777397	1359.819603	17.960051
37.746299	1358.059530	17.965069
38.029252	1354.702282	17.970087
37.883068	1365.629329	17.975104
38.013207	1358.918227	17.980122
38.274476	1365.499343	17.985139
37.841963	1357.347948	17.990157
38.251690	1349.374066	17.995175
38.030110	1365.050380	18.000192
38.122518	1350.896250	18.005210
37.913277	1354.241555	18.010227
37.968585	1344.420775	18.015245
38.159244	1350.725795	18.020263
38.190158	1358.131688	18.025280
38.147849	1350.125039	18.030298
37.970775	1363.615531	18.035315
37.682114	1353.936025	18.040333
37.996403	1340.337486	18.045351
37.841648	1364.252505	18.050368
38.219924	1368.602752	18.055386
38.146990	1378.989030	18.060403
38.446792	1375.247150	18.065421
38.326327	1370.758090	18.070439
38.385628	1363.481007	18.075456
38.285508	1368.906643	18.080474
38.351584	1401.333181	18.085491
38.573936	1411.818894	18.090509
38.923717	1404.919524	18.095527
38.712353	1405.434632	18.100544
38.682400	1397.802249	18.105562
38.921722	1401.672971	18.110579
38.804395	1397.840194	18.115597
39.282519	1408.777476	18.120615
39.355620	1401.597098	18.125632
39.275036	1397.792497	18.130650
38.856457	1398.124551	18.135667
39.003082	1404.628776	18.140685
39.106113	1389.658190	18.145703
39.260213	1395.340213	18.150720
39.303595	1391.494264	18.155738
39.475061	1389.961902	18.160755
39.085280	1394.401881	18.165773
39.422650	1401.854187	18.170791
39.475704	1401.812865	18.175808
39.518686	1391.889184	18.180826
39.474562	1404.456474	18.185843
39.729980	1399.535256	18.190861
39.417436	1397.710876	18.195879
39.299198	1393.030521	18.200896
39.203887	1389.259061	18.205914
39.321581	1400.450166	18.210931
39.561091	1418.678166	18.215949
39.863933	1419.245684	18.220967
39.631867	1430.436940	18.225984
39.641807	1427.290126	18.231002
39.969021	1419.894343	18.236019
39.997855	1431.407401	18.241037
40.258590	1422.888684	18.246055
39.998514	1424.637087	18.251072
40.010997	1422.094309	18.256090
39.973763	1420.081928	18.261107
39.899066	1428.364258	18.266125
40.150281	1423.765932	18.271143
40.349784	1417.947366	18.276160
40.365900	1415.628961	18.281178
40.395393	1411.184392	18.286195
40.126263	1419.330955	18.291213
40.107540	1417.281858	18.296231
40.117849	1427.898477	18.301248
40.358624	1419.385029	18.306266
40.488192	1404.629504	18.311283
40.514664	1415.583364	18.316301
40.667317	1406.909505	18.321319
40.543887	1423.143211	18.326336
40.548066	1417.267760	18.331354
40.789013	1408.494084	18.336371
40.599850	1419.289707	18.341389
40.713209	1415.407782	18.346407
40.689420	1419.124571	18.351424
40.708260	1411.405388	18.356442
40.810391	1407.029711	18.361459
40.394061	1409.358394	18.366477
40.554421	1402.056720	18.371495
40.664201	1415.692153	18.376512
40.518152	1438.825234	18.381530
40.692131	1443.353931	18.386547
40.985890	1444.955308	18.391565
41.210613	1443.577507	18.396583
41.276893	1442.914586	18.401600
41.201903	1436.043670	18.406618
41.249965	1449.933594	18.411635
40.779078	1445.484313	18.416653
41.203995	1430.421523	18.421671
40.909986	1446.342538	18.426688
41.224449	1446.175350	18.431706
41.663298	1459.339956	18.436723
41.748552	1459.528916	18.441741
42.072913	1446.596059	18.446759
41.590329	1438.859342	18.451776
41.550040	1434.792592	18.456794
41.441584	1435.976833	18.461811
41.214960	1440.828786	18.466829
41.648258	1449.989663	18.471847
41.988762	1450.154746	18.476864
42.131364	1464.032209	18.481882
42.413574	1454.808631	18.486899
42.260413	1447.656765	18.491917
42.133176	1427.962361	18.496935
41.835134	1423.255811	18.501952
41.820016	1426.883581	18.506970
42.086330	1429.331123	18.511987
42.060516	1424.020007	18.517005
42.222560	1418.626084	18.522023
41.891140	1422.795828	18.527040
41.739450	1432.193703	18.532058
42.276700	1444.588583	18.537075
42.177183	1458.647177	18.542093
42.531685	1453.519434	18.547111
42.364644	1465.168024	18.552128
42.319984	1458.494030	18.557146
42.447637	1458.100264	18.562163
42.427803	1455.824010	18.567181
42.748900	1458.659898	18.572199
42.752037	1460.091612	18.577216
42.780543	1448.231146	18.582234
42.680066	1445.600744	18.587251
42.517609	1451.895860	18.592269
42.415410	1452.829492	18.597287
42.666671	1453.258309	18.602304
42.344745	1454.502037	18.607322
42.723342	1443.740670	18.612339
42.348306	1464.340875	18.617357
42.824986	1477.799210	18.622375
42.915004	1475.545543	18.627392
42.743869	1480.985709	18.632410
42.965750	1482.006322	18.637427
42.951849	1483.472740	18.642445
43.096781	1485.226654	18.647463
43.300992	1488.514686	18.652480
43.130601	1480.730096	18.657498
43.389293	1482.633891	18.662515
42.810154	1477.959211	18.667533
42.749035	1475.850584	18.672551
43.454234	1497.326922	18.677568
43.278491	1500.834223	18.682586
43.728281	1503.158555	18.687603
43.463262	1509.842253	18.692621
43.679737	1507.598586	18.697639
43.556974	1501.812577	18.702656
43.662004	1503.549861	18.707674
43.762569	1485.315991	18.712691
43.722317	1489.467947	18.717709
43.871216	1496.034032	18.722727
43.860064	1499.383047	18.727744
44.092528	1497.421746	18.732762
44.082938	1486.945142	18.737779
44.207040	1497.981537	18.742797
44.370753	1492.925068	18.747815
44.279901	1491.943270	18.752832
44.093053	1496.678247	18.757850
44.012568	1497.495116	18.762867
44.117410	1494.424918	18.767885
43.951166	1494.679058	18.772903
44.007690	1489.065371	18.777920
44.050818	1490.381634	18.782938
44.347552	1490.030193	18.787955
44.217253	1493.432947	18.792973
44.079944	1481.676226	18.797991
44.420069	1493.244176	18.803008
44.345640	1489.340909	18.808026
44.457557	1504.196988	18.813043
44.570015	1507.731065	18.818061
44.863210	1502.241433	18.823079
45.136965	1506.152352	18.828096
44.960764	1503.350026	18.833114
44.771484	1486.624513	18.838131
44.888418	1482.422924	18.843149
45.002361	1491.027616	18.848167
45.062935	1493.919553	18.853184
45.012041	1499.234553	18.858202
45.175265	1488.236337	18.863219
44.744215	1490.890458	18.868237
44.542722	1492.988398	18.873255
45.001638	1492.312553	18.878272
44.849813	1501.274323	18.883290
44.943348	1505.470112	18.888307
45.424176	1507.563751	18.893325
45.138711	1508.936088	18.898343
45.490550	1493.529251	18.903360
45.187977	1505.227037	18.908378
44.971539	1509.915930	18.913395
45.238497	1523.172178	18.918413
45.594338	1534.168729	18.923431
45.851187	1526.139125	18.928448
45.873513	1534.144878	18.933466
45.592710	1534.819479	18.938483
45.665846	1528.545823	18.943501
45.967100	1524.852087	18.948519
45.929892	1523.753757	18.953536
45.988200	1528.807442	18.958554
46.149726	1520.064936	18.963571
46.351557	1514.231186	18.968589
45.944461	1498.729904	18.973607
46.123975	1490.742227	18.978624
45.940693	1491.983123	18.983642
46.147564	1503.339861	18.988659
46.204128	1500.530563	18.993677
46.565976	1506.248171	18.998695
46.537248	1499.940775	19.003712
46.054723	1501.325994	19.008730
46.225172	1491.796096	19.013747
46.427722	1495.695357	19.018765
46.220725	1511.222576	19.023783
46.719744	1512.495194	19.028800
46.563677	1516.105731	19.033818
46.479496	1507.242043	19.038835
46.476405	1522.247641	19.043853
46.584406	1532.537792	19.048871
47.015375	1516.283503	19.053888
46.395962	1519.454330	19.058906
46.358341	1510.387890	19.063923
46.645860	1521.459691	19.068941
46.050514	1530.819340	19.073959
46.466597	1520.885292	19.078976
46.731418	1543.747901	19.083994
47.037471	1546.155237	19.089011
46.852471	1553.178448	19.094029
47.095861	1554.404149	19.099047
46.869148	1556.833000	19.104064
46.936036	1558.752558	19.109082
46.935927	1552.371521	19.114099
47.062946	1560.583585	19.119117
47.023350	1572.969969	19.124135
47.297575	1568.536284	19.129152
47.228592	1590.436324	19.134170
47.431589	1573.927160	19.139187
47.855464	1573.517113	19.144205
47.957869	1577.963987	19.149223
47.834544	1580.026189	19.154240
47.644437	1576.325067	19.159258
47.826568	1572.969670	19.164275
47.904287	1575.986925	19.169293
47.701256	1573.406712	19.174311
47.784055	1570.954837	19.179328
47.792920	1579.622608	19.184346
47.972690	1566.476564	19.189363
48.098256	1573.388822	19.194381
47.872076	1575.326501	19.199399
48.189055	1575.823587	19.204416
48.085143	1572.025357	19.209434
48.076805	1564.425733	19.214451
48.089329	1574.871438	19.219469
48.243666	1595.804370	19.224487
48.805109	1604.041901	19.229504
48.152678	1594.206829	19.234522
48.272477	1600.308921	19.239539
48.459910	1600.061162	19.244557
48.539000	1606.731143	19.249575
48.704203	1606.425843	19.254592
48.558444	1602.373328	19.259610
48.768366	1594.789584	19.264627
49.155103	1589.540734	19.269645
49.060116	1609.778550	19.274663
49.244044	1595.427988	19.279680
49.046846	1587.509207	19.284698
48.623220	1573.170098	19.289715
48.956331	1568.323971	19.294733
48.604096	1590.643219	19.299751
49.096538	1594.253485	19.304768
48.629632	1599.973056	19.309786
48.597424	1599.574408	19.314803
48.790171	1600.825213	19.319821
48.764169	1599.299087	19.324839
48.883008	1603.673182	19.329856
48.975453	1613.025706	19.334874
49.196513	1617.850382	19.339891
49.172760	1621.509937	19.344909
49.275126	1625.380909	19.349927
49.723250	1620.385853	19.354944
49.770222	1616.196379	19.359962
49.446175	1614.266010	19.364979
49.673103	1609.245706	19.369997
49.530031	1609.396619	19.375015
49.716379	1614.615374	19.380032
49.505136	1615.879599	19.385050
49.711803	1638.694092	19.390067
49.955185	1636.117255	19.395085
49.832589	1641.848047	19.400103
50.049812	1643.257785	19.405120
50.009640	1646.648040	19.410138
50.025062	1638.379366	19.415155
50.418980	1628.304046	19.420173
50.354308	1646.216874	19.425191
50.399183	1638.522012	19.430208
50.066258	1637.308582	19.435226
50.390000	1633.611695	19.440243
50.648182	1640.443610	19.445261
50.619032	1639.230567	19.450279
50.475988	1630.743031	19.455296
50.519015	1635.715033	19.460314
50.476881	1645.262239	19.465331
50.742255	1641.196689	19.470349
50.550717	1638.705501	19.475367
50.456739	1638.633955	19.480384
50.836296	1638.859313	19.485402
50.684451	1653.254649	19.490419
51.020004	1664.133400	19.495437
51.273993	1660.449214	19.500455
51.362605	1661.605826	19.505472
51.197449	1638.237689	19.510490
51.073707	1639.336882	19.515507
51.213381	1645.567190	19.520525
51.039780	1650.273453	19.525543
51.507833	1647.557529	19.530560
51.158658	1658.548641	19.535578
51.174712	1654.733715	19.540595
51.536591	1656.282131	19.545613
50.923566	1654.204453	19.550631
51.640212	1641.519567	19.555648
51.766447	1662.383817	19.560666
51.217063	1655.233558	19.565683
51.646577	1656.798353	19.570701
51.410096	1655.237720	19.575719
51.753262	1653.945828	19.580736
51.805133	1643.290081	19.585754
51.634245	1676.670434	19.590771
51.953224	1681.468123	19.595789
52.038275	1693.114789	19.600807
52.170971	1692.093871	19.605824
52.452246	1687.812514	19.610842
52.409933	1675.668134	19.615859
52.390433	1660.787998	19.620877
51.978526	1653.826613	19.625895
52.210863	1648.890826	19.630912
52.394991	1656.204622	19.635930
52.356900	1662.807977	19.640947
52.502034	1671.909533	19.645965
52.786532	1688.210148	19.650983
52.814515	1664.728960	19.656000
52.628707	1654.506535	19.661018
52.754003	1641.144453	19.666035
52.709025	1630.171684	19.671053
52.491858	1648.682883	19.676071
52.560523	1668.285923	19.681088
52.544058	1677.136459	19.686106
52.658871	1670.745043	19.691123
52.979139	1665.636075	19.696141
52.842984	1681.402323	19.701159
52.821733	1676.815488	19.706176
52.860285	1675.835716	19.711194
52.704572	1667.760840	19.716211
52.978948	1665.021807	19.721229
53.046740	1681.490692	19.726247
52.982192	1696.031665	19.731264
53.146649	1694.954913	19.736282
52.703894	1695.259473	19.741299
52.779768	1692.162727	19.746317
52.945343	1711.990138	19.751335
53.257014	1722.135353	19.756352
53.885247	1716.737509	19.761370
53.419608	1724.336055	19.766387
53.884079	1718.145474	19.771405
53.932000	1719.205282	19.776423
53.577955	1709.555842	19.781440
53.987987	1713.273249	19.786458
53.809934	1720.265469	19.791475
54.145622	1710.257980	19.796493
54.072726	1720.894063	19.801511
53.985356	1717.811100	19.806528
54.122148	1713.769339	19.811546
54.064401	1742.833545	19.816563
54.638875	1733.585911	19.821581
54.811825	1740.332163	19.826599
54.563107	1734.706235	19.831616
54.665922	1708.297161	19.836634
54.448008	1701.198983	19.841651
54.456166	1698.524800	19.846669
54.505056	1713.395631	19.851687
54.783505	1727.726622	19.856704
54.999514	1735.441052	19.861722
54.714485	1732.628324	19.866739
54.648354	1732.059509	19.871757
54.495720	1730.775140	19.876775
54.642249	1734.263487	19.881792
54.930655	1731.916375	19.886810
54.760228	1735.628341	19.891827
54.815214	1731.712878	19.896845
54.745446	1729.971160	19.901863
54.776718	1745.433849	19.906880
55.193380	1751.525917	19.911898
55.246371	1762.410293	19.916915
55.407721	1767.953279	19.921933
55.210485	1778.860908	19.926951
55.543755	1765.837149	19.931968
55.414429	1765.842303	19.936986
55.248807	1772.141418	19.942003
55.512650	1764.040069	19.947021
55.673052	1768.473478	19.952039
55.752006	1760.393630	19.957056
55.801618	1754.117274	19.962074
55.718023	1756.135733	19.967091
55.633193	1762.888573	19.972109
55.911401	1760.717731	19.977127
56.009442	1774.330622	19.982144
55.795236	1781.982323	19.987162
55.822320	1782.782415	19.992179
56.317817	1790.709126	19.997197
56.123119	1790.129668	20.002215
56.080651	1793.178636	20.007232
56.176705	1784.017904	20.012250
56.056403	1784.991944	20.017267
56.224971	1780.237110	20.022285
56.491217	1783.458464	20.027303
56.448586	1776.567483	20.032320
56.617698	1777.992073	20.037338
56.376753	1789.867863	20.042355
56.564602	1805.238996	20.047373
56.869844	1811.447916	20.052391
56.886589	1814.862462	20.057408
57.361338	1812.212524	20.062426
57.277222	1814.699929	20.067443
57.148358	1814.004088	20.072461
57.229487	1801.036925	20.077479
56.873514	1798.118597	20.082496
57.030756	1787.924425	20.087514
56.978590	1798.345149	20.092531
57.072667	1798.546827	20.097549
56.898917	1813.974377	20.102567
57.321532	1805.961718	20.107584
57.210834	1792.701883	20.112602
57.012723	1795.382516	20.117619
57.084595	1813.631798	20.122637
57.431292	1826.424388	20.127655
57.721694	1822.015120	20.132672
57.902383	1825.317742	20.137690
57.598764	1831.246612	20.142707
57.610948	1833.931472	20.147725
57.325302	1825.043419	20.152743
57.651081	1849.158887	20.157760
57.816629	1845.797906	20.162778
58.179064	1864.670233	20.167795
58.060731	1861.704159	20.172813
58.512167	1858.412456	20.177831
58.227861	1864.360783	20.182848
58.410171	1861.388330	20.187866
58.444259	1858.581107	20.192883
58.501839	1853.920174	20.197901
58.769174	1861.227207	20.202919
58.388106	1851.124902	20.207936
58.567409	1857.801068	20.212954
58.700278	1860.664002	20.217971
58.631410	1859.784640	20.222989
59.230354	1854.864970	20.228007
58.589222	1852.359074	20.233024
58.952891	1851.219276	20.238042
58.931661	1848.508983	20.243059
59.079418	1855.235632	20.248077
59.056336	1847.053714	20.253095
59.038285	1867.538382	20.258112
59.247912	1851.826964	20.263130
58.927897	1847.579186	20.268147
58.768772	1855.168479	20.273165
59.379275	1863.931656	20.278183
59.291004	1871.122276	20.283200
59.732710	1878.439475	20.288218
59.470519	1885.574992	20.293235
59.501084	1877.282036	20.298253
59.483712	1871.590665	20.303271
59.593512	1876.302325	20.308288
59.471074	1867.458529	20.313306
59.462610	1879.147362	20.318323
59.539033	1870.766524	20.323341
60.139654	1869.996783	20.328359
59.602232	1873.327539	20.333376
60.029685	1883.460421	20.338394
60.267897	1896.698713	20.343411
60.392183	1911.295488	20.348429
60.679941	1893.392768	20.353447
60.219585	1877.043091	20.358464
60.499040	1864.399368	20.363482
60.283406	1863.383840	20.368499
60.502532	1877.846220	20.373517
60.498298	1887.900061	20.378535
60.336409	1885.351576	20.383552
60.699384	1885.269471	20.388570
60.911382	1886.022675	20.393587
60.750595	1895.172751	20.398605
60.984688	1885.366960	20.403623
60.932413	1881.944927	20.408640
60.856293	1869.451289	20.413658
60.765815	1885.712907	20.418675
60.900227	1891.971348	20.423693
61.369857	1874.492688	20.428711
61.283812	1873.216593	20.433728
61.580724	1867.548479	20.438746
61.756254	1865.940603	20.443763
61.698433	1878.242457	20.448781
61.704419	1874.722223	20.453799
61.553222	1876.663688	20.458816
61.372008	1874.744325	20.463834
61.545166	1874.819757	20.468851
61.392984	1870.931210	20.473869
61.884204	1862.442661	20.478887
61.553906	1869.630564	20.483904
61.461266	1868.158136	20.488922
61.871727	1869.346020	20.493939
61.764668	1879.216275	20.498957
61.824803	1885.966274	20.503975
61.851342	1898.417772	20.508992
62.052368	1900.834451	20.514010
62.014081	1904.231341	20.519027
61.674156	1916.454657	20.524045
62.067102	1903.433912	20.529063
61.597508	1915.719400	20.534080
62.142621	1913.115686	20.539098
62.267839	1933.941893	20.544115
62.584597	1940.226712	20.549133
62.583949	1921.291595	20.554151
62.348192	1927.522842	20.559168
62.347890	1935.121359	20.564186
62.717745	1951.361696	20.569203
62.707365	1954.492787	20.574221
63.221379	1955.722419	20.579239
62.893672	1954.839765	20.584256
62.903783	1963.532740	20.589274
63.223166	1947.379109	20.594291
63.001022	1951.447084	20.599309
63.312500	1967.962417	20.604327
63.364260	1956.523468	20.609344
63.225807	1944.883303	20.614362
63.372940	1943.647010	20.619379
63.108653	1955.542531	20.624397
63.404503	1967.724206	20.629415
63.624278	1981.527381	20.634432
63.627343	1987.526093	20.639450
64.091481	1974.561235	20.644467
63.693604	1981.632021	20.649485
63.951312	1976.479751	20.654503
63.776422	1973.568863	20.659520
63.818206	1975.972896	20.664538
63.874119	1979.890214	20.669555
63.740608	1983.044021	20.674573
64.123044	1974.176768	20.679591
64.147387	1979.451353	20.684608
64.322715	1988.021773	20.689626
64.747213	2005.514448	20.694643
64.737494	1995.866978	20.699661
64.708538	1964.751290	20.704679
64.629849	1966.013124	20.709696
64.702541	1966.154761	20.714714
64.837132	1962.914017	20.719731
64.345659	1973.957407	20.724749
64.930494	1966.253658	20.729767
65.405772	1980.662981	20.734784
65.333105	1969.298517	20.739802
65.422085	1953.675037	20.744819
64.911391	1964.870009	20.749837
65.422370	1950.653442	20.754855
65.184346	1957.130133	20.759872
65.256288	1946.310244	20.764890
65.467863	1950.577980	20.769907
65.165471	1955.580988	20.774925
65.625082	1968.900070	20.779943
65.615454	1972.801841	20.784960
65.707849	1980.971824	20.789978
65.902392	1983.351008	20.794995
65.551809	1984.332999	20.800013
65.936932	1971.083588	20.805031
65.672343	1977.382410	20.810048
65.251426	1976.699196	20.815066
66.047083	1976.500713	20.820083
65.282674	1982.153847	20.825101
65.707426	1988.442295	20.830119
65.730644	1996.694381	20.835136
66.070951	2007.737144	20.840154
66.171056	2011.865456	20.845171
66.081606	2009.376430	20.850189
65.974370	2016.329130	20.855207
66.018803	2030.637270	20.860224
65.933797	2037.013715	20.865242
66.236313	2022.230595	20.870259
66.550529	2032.060267	20.875277
67.126311	2051.454217	20.880295
66.932318	2046.285826	20.885312
67.453564	2041.988929	20.890330
67.625080	2031.192680	20.895347
67.209257	2030.424771	20.900365
67.223543	2020.695569	20.905383
67.193753	2014.717638	20.910400
67.493399	2020.203219	20.915418
67.197908	2016.655219	20.920435
67.037203	2019.624369	20.925453
67.361705	2033.925401	20.930471
67.558319	2038.264329	20.935488
67.498495	2045.003909	20.940506
68.132090	2047.159185	20.945523
67.430422	2046.551690	20.950541
67.809178	2061.419916	20.955559
67.853450	2061.647347	20.960576
67.846731	2051.273420	20.965594
67.862114	2044.019611	20.970611
67.409156	2050.174013	20.975629
67.748063	2040.105155	20.980647
67.657496	2049.494092	20.985664
67.869663	2063.374182	20.990682
68.653238	2062.399411	20.995699
68.530754	2076.535389	21.000717
68.494240	2071.832267	21.005735
68.507078	2069.071821	21.010752
68.398810	2076.310916	21.015770
68.682806	2073.997748	21.020787
68.729138	2078.426083	21.025805
68.691056	2074.824117	21.030823
68.919138	2076.052194	21.035840
68.720933	2067.713285	21.040858
68.807298	2057.963684	21.045875
68.631563	2075.426110	21.050893
69.248140	2077.588730	21.055911
69.096373	2084.838955	21.060928
69.125641	2102.706871	21.065946
69.487043	2098.351733	21.070963
68.979382	2109.390414	21.075981
69.100939	2101.391333	21.080999
69.288415	2095.701656	21.086016
69.106670	2105.079317	21.091034
69.496274	2107.336531	21.096051
69.708723	2122.703129	21.101069
69.480511	2123.218876	21.106087
70.087010	2126.329948	21.111104
69.916240	2126.718496	21.116122
70.106325	2119.306264	21.121139
70.037916	2120.906151	21.126157
70.002689	2115.843184	21.131175
69.874847	2114.538545	21.136192
70.018499	2120.813661	21.141210
70.362459	2119.969205	21.146227
70.299698	2129.565588	21.151245
70.514716	2143.906072	21.156263
70.717687	2140.528214	21.161280
70.804103	2147.573766	21.166298
71.036230	2141.723752	21.171315
71.157184	2149.921386	21.176333
70.927569	2149.056956	21.181351
71.254551	2145.924726	21.186368
71.058854	2143.648300	21.191386
71.424130	2136.932647	21.196403
71.229558	2137.727657	21.201421
71.304737	2154.158822	21.206439
71.341418	2145.515721	21.211456
71.532250	2141.112976	21.216474
71.457358	2138.845719	21.221491
71.653908	2134.373926	21.226509
71.651928	2138.466784	21.231527
71.730027	2140.924876	21.236544
71.536276	2143.978049	21.241562
71.708970	2134.585366	21.246579
71.652662	2139.815661	21.251597
71.605209	2145.953876	21.256615
71.773953	2140.637526	21.261632
71.430283	2148.954848	21.266650
71.796538	2152.852814	21.271667
71.736921	2161.503687	21.276685
71.842251	2158.994654	21.281703
71.768426	2165.934026	21.286720
71.794557	2182.508553	21.291738
72.507108	2189.531753	21.296755
72.038187	2200.434972	21.301773
72.065223	2200.357007	21.306791
72.507082	2202.081621	21.311808
72.342117	2204.493872	21.316826
72.814515	2214.703595	21.321843
73.065743	2220.345861	21.326861
73.168567	2210.173985	21.331879
73.466523	2207.413443	21.336896
73.625643	2223.683380	21.341914
73.316844	2212.586875	21.346931
73.611463	2192.916460	21.351949
73.244924	2192.264601	21.356967
73.302533	2175.470377	21.361984
73.342804	2181.126230	21.367002
73.326564	2201.731506	21.372019
73.575636	2209.049793	21.377037
73.906426	2210.341810	21.382055
74.088786	2202.861725	21.387072
73.875437	2218.731035	21.392090
74.022827	2218.075936	21.397107
74.139666	2214.047381	21.402125
74.127911	2201.434577	21.407143
74.468746	2204.700188	21.412160
74.202474	2208.433813	21.417178
74.088427	2207.870535	21.422195
74.245151	2207.398921	21.427213
74.020118	2197.039123	21.432231
74.295969	2197.530235	21.437248
73.748928	2205.816828	21.442266
74.196528	2235.778308	21.447283
74.286984	2234.795632	21.452301
73.956714	2253.045357	21.457319
74.700923	2248.088964	21.462336
74.567228	2264.561061	21.467354
74.899690	2270.644812	21.472371
74.814761	2270.850291	21.477389
74.499622	2280.179240	21.482407
75.172569	2277.827161	21.487424
75.446007	2294.710721	21.492442
75.834652	2297.488955	21.497459
75.588391	2296.686121	21.502477
75.504344	2304.467349	21.507495
75.842145	2290.686937	21.512512
75.796295	2285.162708	21.517530
76.136959	2290.602633	21.522547
76.198845	2288.977670	21.527565
76.278398	2287.007290	21.532583
76.339682	2261.461754	21.537600
76.297705	2256.118378	21.542618
75.766292	2248.675321	21.547635
76.327166	2259.508207	21.552653
76.370191	2275.636174	21.557671
76.489800	2278.238207	21.562688
76.433627	2285.490443	21.567706
76.493771	2281.091736	21.572723
76.489532	2286.379417	21.577741
76.226161	2283.165395	21.582759
76.451479	2279.366321	21.587776
76.358359	2284.338986	21.592794
76.667661	2301.643962	21.597811
76.777531	2311.361527	21.602829
76.307513	2307.352960	21.607847
76.839164	2305.162996	21.612864
76.828087	2317.626362	21.617882
76.944942	2334.589184	21.622899
77.516968	2334.260934	21.627917
77.596708	2341.559237	21.632935
77.539755	2334.711709	21.637952
77.676493	2338.738983	21.642970
77.509323	2320.926496	21.647987
78.206208	2327.211057	21.653005
77.850622	2332.231832	21.658023
78.092335	2322.695749	21.663040
78.160456	2320.856773	21.668058
78.066119	2330.856899	21.673075
77.671379	2318.480111	21.678093
78.083664	2334.155608	21.683111
78.274489	2323.407931	21.688128
77.833422	2326.465001	21.693146
77.893866	2334.347162	21.698163
78.377175	2353.199328	21.703181
78.281177	2371.127622	21.708199
78.347585	2364.244343	21.713216
78.060761	2356.448630	21.718234
78.513270	2367.529603	21.723251
79.058749	2376.552035	21.728269
79.072494	2390.565990	21.733287
79.330923	2384.037563	21.738304
79.507732	2390.389982	21.743322
79.307192	2381.430065	21.748339
79.554139	2380.520136	21.753357
79.515216	2383.282825	21.758375
79.505816	2371.876115	21.763392
79.390846	2380.027036	21.768410
79.440256	2377.251043	21.773427
79.657475	2376.813716	21.778445
79.421798	2376.522091	21.783463
79.816961	2377.077346	21.788480
79.760528	2384.722563	21.793498
79.663705	2385.752796	21.798515
79.936564	2386.334954	21.803533
79.915355	2400.460594	21.808551
80.012010	2387.224248	21.813568
79.969329	2403.322221	21.818586
79.878987	2400.263036	21.823603
80.123159	2412.473682	21.828621
80.263608	2430.302739	21.833639
80.702020	2425.185418	21.838656
80.722446	2429.711437	21.843674
80.517351	2425.740946	21.848691
80.947744	2415.264230	21.853709
80.661040	2427.019730	21.858727
80.796961	2422.100812	21.863744
80.937067	2429.307690	21.868762
80.933667	2445.738568	21.873779
81.374291	2448.415332	21.878797
81.282655	2446.679508	21.883815
81.455048	2445.399239	21.888832
81.331055	2442.386943	21.893850
81.572630	2439.116218	21.898867
82.065402	2430.912916	21.903885
81.927719	2438.773936	21.908903
82.218715	2426.526251	21.913920
82.140910	2429.302459	21.918938
82.082604	2432.460464	21.923955
82.079703	2438.267041	21.928973
82.195813	2432.168388	21.933991
82.544166	2442.532416	21.939008
82.773733	2431.989667	21.944026
82.203306	2424.729732	21.949043
82.331987	2419.959247	21.954061
82.285521	2444.973533	21.959079
82.633652	2455.355716	21.964096
82.923337	2455.919743	21.969114
82.885714	2454.163970	21.974131
83.058788	2454.720103	21.979149
82.797875	2463.048719	21.984167
83.176364	2459.909687	21.989184
83.323650	2456.239601	21.994202
83.024260	2459.193368	21.999219
83.053933	2463.400169	22.004237
82.902819	2460.409673	22.009255
83.019692	2462.706497	22.014272
83.098114	2476.462612	22.019290
82.961328	2483.600316	22.024307
83.570236	2480.907431	22.029325
83.294723	2490.343928	22.034343
83.752334	2497.536952	22.039360
84.338631	2502.365134	22.044378
84.350466	2496.987194	22.049395
84.446097	2485.944520	22.054413
84.264739	2482.931853	22.059431
84.444759	2475.830154	22.064448
84.096102	2488.162050	22.069466
84.360359	2497.330232	22.074483
84.552945	2504.300532	22.079501
84.481032	2510.881493	22.084519
84.745067	2503.832037	22.089536
84.982503	2498.880572	22.094554
84.679069	2503.500679	22.099571
84.817272	2494.811474	22.104589
84.777313	2498.823503	22.109607
84.713467	2511.965790	22.114624
85.031042	2523.127045	22.119642
84.785649	2529.903208	22.124659
85.228877	2525.465340	22.129677
85.000757	2528.355771	22.134695
85.250225	2544.016657	22.139712
85.887005	2540.812094	22.144730
86.302843	2553.365333	22.149747
86.234408	2541.304899	22.154765
86.137577	2532.472631	22.159783
85.729052	2515.482440	22.164800
86.367651	2533.403700	22.169818
86.024099	2549.774762	22.174835
86.573201	2550.162074	22.179853
86.432952	2550.444411	22.184871
86.375541	2548.741895	22.189888
85.997156	2551.350875	22.194906
85.992962	2560.708330	22.199923
86.541014	2560.139956	22.204941
86.606147	2562.832334	22.209959
86.503075	2581.285638	22.214976
86.676345	2580.911865	22.219994
86.465097	2595.485997	22.225011
86.704182	2591.540878	22.230029
86.886367	2596.126433	22.235047
87.297753	2609.061144	22.240064
87.428710	2613.582337	22.245082
87.060710	2616.371494	22.250099
87.423770	2610.200469	22.255117
87.318710	2612.880037	22.260135
87.688055	2606.736320	22.265152
87.851172	2619.201851	22.270170
87.825537	2622.204502	22.275187
87.736009	2613.448537	22.280205
87.969550	2615.359979	22.285223
88.254058	2621.553758	22.290240
88.514587	2617.914525	22.295258
88.449728	2618.900910	22.300275
88.809429	2611.773001	22.305293
88.571709	2601.502228	22.310311
88.472031	2606.215460	22.315328
88.689755	2605.031621	22.320346
88.554714	2617.795228	22.325363
89.143543	2600.984214	22.330381
88.738082	2602.581581	22.335399
88.491514	2607.945831	22.340416
89.031129	2621.128249	22.345434
88.734350	2634.118982	22.350451
88.990430	2641.678827	22.355469
89.221641	2639.482956	22.360487
89.014475	2645.637524	22.365504
89.316526	2647.858109	22.370522
89.121094	2672.529677	22.375539
89.127079	2663.280754	22.380557
89.092279	2669.024975	22.385575
88.985591	2670.986740	22.390592
89.690025	2691.057849	22.395610
89.562741	2700.664460	22.400627
89.938704	2701.694143	22.405645
90.055143	2700.197912	22.410663
90.318485	2710.449402	22.415680
90.945869	2715.144489	22.420698
90.832600	2725.164138	22.425715
91.033098	2706.785743	22.430733
91.165078	2686.838046	22.435751
90.906536	2689.326462	22.440768
90.957932	2673.995068	22.445786
91.208383	2668.758340	22.450803
91.292764	2669.989741	22.455821
91.667056	2678.968596	22.460839
91.012681	2678.190268	22.465856
91.520005	2681.728459	22.470874
91.337575	2686.060130	22.475891
91.147277	2697.535347	22.480909
91.601895	2699.426803	22.485927
91.641659	2722.731684	22.490944
91.738292	2709.857257	22.495962
91.678969	2712.959189	22.500979
91.617299	2714.524953	22.505997
91.461121	2722.697035	22.511015
91.704325	2738.948897	22.516032
92.201708	2739.085716	22.521050
92.080270	2744.289970	22.526067
92.060517	2739.970672	22.531085
92.444244	2748.348817	22.536103
92.549731	2767.269829	22.541120
92.829533	2760.547168	22.546138
92.629304	2759.687885	22.551155
92.942165	2766.552605	22.556173
93.109869	2748.196903	22.561191
92.481407	2757.178517	22.566208
92.759350	2751.043548	22.571226
93.034499	2778.753163	22.576243
93.458324	2784.644863	22.581261
93.334967	2782.566222	22.586279
93.297086	2788.201551	22.591296
93.392797	2779.590860	22.596314
93.300807	2789.524754	22.601331
93.510458	2804.403139	22.606349
94.056589	2806.783408	22.611367
93.737836	2803.385521	22.616384
94.190736	2800.248299	22.621402
94.393329	2803.854196	22.626419
94.458555	2809.595719	22.631437
94.655926	2802.328804	22.636455
94.757934	2803.918710	22.641472
94.713263	2791.186458	22.646490
94.929182	2799.754954	22.651507
94.834544	2794.596467	22.656525
95.039714	2796.207906	22.661543
94.812796	2793.118063	22.666560
95.158956	2782.648720	22.671578
94.832929	2798.230165	22.676595
94.890265	2802.871844	22.681613
94.964552	2814.624676	22.686631
95.193264	2830.872730	22.691648
95.510913	2820.620665	22.696666
95.506106	2818.807067	22.701683
95.454824	2832.330609	22.706701
95.727664	2823.109539	22.711719
95.597949	2830.344263	22.716736
95.527487	2828.988743	22.721754
95.983943	2843.077587	22.726771
96.008200	2841.166272	22.731789
96.160488	2851.585415	22.736807
96.517913	2859.075866	22.741824
96.416067	2851.146188	22.746842
96.156120	2848.109035	22.751859
96.155910	2844.744324	22.756877
96.443602	2861.736186	22.761895
96.529653	2885.912774	22.766912
96.697429	2885.920207	22.771930
96.692567	2887.056533	22.776947
96.998970	2881.431758	22.781965
97.408159	2881.813068	22.786983
97.333542	2897.897542	22.792000
97.368157	2900.987532	22.797018
97.381275	2899.398122	22.802035
97.793210	2902.943073	22.807053
97.905814	2897.078275	22.812071
97.687560	2902.505662	22.817088
97.886970	2896.294246	22.822106
97.730438	2904.357824	22.827123
97.599176	2900.241942	22.832141
98.294788	2905.081716	22.837159
97.746824	2927.701365	22.842176
98.075176	2920.661959	22.847194
97.939063	2934.403933	22.852211
98.108006	2946.017604	22.857229
98.659739	2946.618269	22.862247
98.560440	2957.433380	22.867264
98.359046	2958.327389	22.872282
98.626708	2960.143475	22.877299
98.704598	2965.484941	22.882317
99.425189	2969.098980	22.887335
99.306605	2967.423848	22.892352
99.733349	2968.916409	22.897370
99.643268	2973.086840	22.902387
99.952686	2976.593237	22.907405
99.811843	2968.523489	22.912423
99.671157	2968.176785	22.917440
100.137334	2969.465197	22.922458
100.185788	2974.194613	22.927475
99.806818	2983.054815	22.932493
100.168040	2973.341503	22.937511
99.883999	2976.235350	22.942528
100.104745	2971.133348	22.947546
100.355573	2985.403935	22.952563
100.685856	2987.228181	22.957581
100.953384	2984.157774	22.962599
100.784013	3000.526511	22.967616
100.835682	2992.107622	22.972634
101.116701	3007.759435	22.977651
100.924867	2993.209243	22.982669
101.174414	2993.503947	22.987687
100.940539	2992.026600	22.992704
101.074188	2988.983827	22.997722
101.289726	3013.744323	23.002739
100.895773	3029.700209	23.007757
101.311723	3022.399435	23.012775
101.406868	3039.807949	23.017792
101.687606	3046.335982	23.022810
101.986363	3054.218107	23.027827
101.718143	3063.384851	23.032845
101.829181	3052.573478	23.037863
101.791496	3051.542439	23.042880
102.016357	3053.898277	23.047898
102.179189	3060.450130	23.052915
102.370493	3081.493929	23.057933
102.651708	3077.112993	23.062951
102.949524	3083.558299	23.067968
103.087572	3069.396039	23.072986
103.100407	3070.145602	23.078003
103.011742	3080.446449	23.083021
102.991526	3066.000112	23.088039
103.162520	3085.977603	23.093056
103.160882	3080.637514	23.098074
103.086781	3082.880162	23.103091
103.039936	3103.369257	23.108109
103.328198	3105.187862	23.113127
103.141573	3108.850272	23.118144
103.432897	3131.183500	23.123162
103.999647	3138.351312	23.128179
103.642492	3139.618704	23.133197
104.101594	3132.220199	23.138215
104.291407	3133.236973	23.143232
104.290343	3130.847923	23.148250
104.408878	3145.932243	23.153267
104.622133	3162.059185	23.158285
104.589265	3157.867920	23.163303
104.622497	3156.369648	23.168320
105.013551	3146.685549	23.173338
105.398045	3145.986707	23.178355
104.899267	3145.948774	23.183373
105.204614	3147.039765	23.188391
105.139022	3154.221130	23.193408
105.143685	3171.174275	23.198426
105.506007	3172.229475	23.203443
105.398034	3180.578870	23.208461
105.661822	3170.451223	23.213479
105.688128	3177.537493	23.218496
105.827992	3191.510073	23.223514
106.107347	3198.552963	23.228531
106.178531	3213.742811	23.233549
106.495735	3202.604354	23.238567
106.568611	3204.403838	23.243584
106.835888	3195.996061	23.248602
107.296747	3202.507389	23.253619
106.874405	3208.598917	23.258637
107.088789	3207.736056	23.263655
106.915826	3204.384066	23.268672
107.164991	3201.132401	23.273690
107.253097	3183.040124	23.278707
106.969845	3194.591303	23.283725
106.884216	3194.876830	23.288743
107.107169	3215.737630	23.293760
107.249980	3216.969656	23.298778
107.641971	3220.522701	23.303795
107.372574	3230.184618	23.308813
107.596893	3226.370127	23.313831
107.801419	3243.628906	23.318848
107.620174	3251.550685	23.323866
107.726842	3243.224933	23.328883
108.045361	3248.885395	23.333901
108.339288	3270.154224	23.338919
108.867505	3273.322173	23.343936
108.536727	3280.459228	23.348954
108.884531	3268.496376	23.353971
108.915157	3273.177255	23.358989
109.052919	3272.190438	23.364007
109.190312	3276.221786	23.369024
108.941347	3275.619345	23.374042
109.329785	3268.959223	23.379059
109.243495	3274.064145	23.384077
109.154273	3257.184942	23.389095
109.361017	3271.404416	23.394112
109.313618	3302.282437	23.399130
109.439798	3292.734537	23.404147
109.675454	3299.448473	23.409165
109.825971	3286.143011	23.414183
110.243452	3295.980444	23.419200
110.003341	3305.523395	23.424218
110.201219	3308.979402	23.429235
110.561446	3320.866865	23.434253
110.597452	3314.849607	23.439271
110.737491	3321.241164	23.444288
110.743705	3325.654832	23.449306
110.919550	3326.832590	23.454323
111.031545	3325.405932	23.459341
110.978612	3313.721863	23.464359
111.040521	3329.593279	23.469376
110.996588	3344.711726	23.474394
111.510326	3347.859643	23.479411
111.346276	3343.095515	23.484429
111.516667	3342.347397	23.489447
111.693715	3340.110773	23.494464
111.497500	3370.071390	23.499482
111.735397	3363.840436	23.504499
111.925983	3375.164238	23.509517
111.971231	3364.058793	23.514535
112.386276	3371.226979	23.519552
112.734768	3389.757808	23.524570
112.903737	3388.937875	23.529587
112.807438	3390.420058	23.534605
112.914814	3383.255934	23.539623
113.329840	3389.819797	23.544640
113.415890	3391.086808	23.549658
113.725726	3372.026957	23.554675
113.675731	3376.905836	23.559693
113.782641	3359.940174	23.564711
113.647622	3348.123579	23.569728
113.243290	3359.702369	23.574746
113.529957	3366.512631	23.579763
113.684903	3373.884428	23.584781
113.713961	3372.027373	23.589799
113.739159	3377.291467	23.594816
113.806576	3392.143134	23.599834
114.324951	3400.696631	23.604851
114.247651	3399.501247	23.609869
114.185745	3410.007342	23.614887
114.770938	3403.297721	23.619904
114.671188	3395.677262	23.624922
114.854334	3406.177114	23.629939
115.020024	3422.111398	23.634957
115.153639	3443.336482	23.639975
115.228504	3429.390635	23.644992
115.026663	3432.524922	23.650010
115.426839	3428.479746	23.655027
115.236161	3424.888113	23.660045
114.949382	3434.121135	23.665063
115.660579	3449.848377	23.670080
115.824805	3461.949440	23.675098
115.953203	3460.831087	23.680115
115.888706	3456.156380	23.685133
115.879791	3456.108759	23.690151
116.316591	3476.502285	23.695168
116.430498	3483.329335	23.700186
116.291939	3483.559833	23.705203
116.369275	3484.658604	23.710221
116.393510	3484.695664	23.715239
116.854600	3480.068748	23.720256
116.603044	3506.303295	23.725274
117.014428	3510.755972	23.730291
117.160694	3517.911946	23.735309
117.088820	3513.906167	23.740327
117.587233	3516.738143	23.745344
117.245606	3515.449418	23.750362
117.382383	3516.921052	23.755379
117.680119	3534.037193	23.760397
117.302275	3532.215860	23.765415
118.129459	3526.658738	23.770432
117.710848	3534.062000	23.775450
118.271249	3545.191745	23.780467
118.244478	3549.590848	23.785485
118.445215	3552.231858	23.790503
118.631724	3550.001121	23.795520
118.804718	3553.281765	23.800538
118.682503	3557.723021	23.805555
118.909708	3561.020299	23.810573
118.803771	3577.099628	23.815591
119.302517	3578.160662	23.820608
119.511731	3575.284032	23.825626
119.465644	3581.882046	23.830643
119.421609	3584.096963	23.835661
119.252967	3578.316967	23.840679
119.596365	3585.801035	23.845696
119.593655	3612.017081	23.850714
119.694308	3613.452960	23.855731
119.963385	3620.502073	23.860749
120.003498	3621.001873	23.865767
120.519559	3628.949961	23.870784
120.190905	3645.890196	23.875802
120.413913	3637.400126	23.880819
120.777127	3635.880746	23.885837
120.598188	3653.342719	23.890855
121.064809	3667.421581	23.895872
121.402619	3657.903843	23.900890
121.564272	3646.209264	23.905907
121.650335	3653.513834	23.910925
121.415410	3658.677696	23.915943
121.937734	3645.999088	23.920960
121.665360	3652.814449	23.925978
121.774684	3654.490243	23.930995
121.873748	3662.794268	23.936013
121.930273	3669.635606	23.941031
122.344888	3675.581929	23.946048
122.303076	3687.165625	23.951066
121.877874	3680.975217	23.956083
122.388437	3680.704352	23.961101
122.366017	3709.398684	23.966119
122.632009	3710.617877	23.971136
122.571428	3723.253549	23.976154
122.563361	3730.518984	23.981171
122.915796	3740.242248	23.986189
122.781207	3743.684391	23.991207
123.209551	3743.481443	23.996224
122.975582	3769.166659	24.001242
123.442750	3782.427794	24.006259
123.659720	3775.131597	24.011277
123.773962	3791.329493	24.016295
123.959779	3795.888820	24.021312
124.081397	3799.955590	24.026330
124.178821	3802.468434	24.031347
124.407696	3792.738686	24.036365
124.434742	3804.441805	24.041383
124.566902	3789.033365	24.046400
124.951720	3806.701971	24.051418
124.854921	3827.080583	24.056435
125.052169	3829.925374	24.061453
125.078860	3835.477575	24.066471
125.643245	3820.867006	24.071488
125.405406	3827.253887	24.076506
125.396816	3828.942491	24.081523
125.611282	3820.665945	24.086541
125.379230	3825.928209	24.091559
125.600278	3831.882166	24.096576
125.777676	3841.237947	24.101594
126.029287	3848.016024	24.106611
126.366774	3842.505064	24.111629
125.928854	3846.015069	24.116647
126.360865	3855.235082	24.121664
126.466228	3862.916497	24.126682
126.777819	3868.620459	24.131699
126.631666	3862.192129	24.136717
127.049532	3882.019612	24.141735
127.445613	3884.859117	24.146752
127.335045	3896.484253	24.151770
127.398176	3895.866830	24.156787
127.818008	3891.063535	24.161805
127.703126	3897.758487	24.166823
127.817833	3900.201165	24.171840
127.695778	3911.396697	24.176858
127.820086	3899.928580	24.181875
127.941230	3903.445040	24.186893
128.116215	3925.060025	24.191911
128.292696	3919.250039	24.196928
128.427835	3927.039169	24.201946
128.585381	3920.940961	24.206963
128.874330	3929.429509	24.211981
128.858017	3944.729022	24.216999
129.093346	3948.159692	24.222016
129.013488	3950.191597	24.227034
129.257205	3955.881609	24.232051
129.485355	3945.350671	24.237069
129.633339	3959.473395	24.242087
129.932613	3970.472966	24.247104
129.862039	3974.360507	24.252122
129.749731	3973.014163	24.257139
129.684541	3965.879467	24.262157
130.161115	3986.889955	24.267175
130.372176	3994.291753	24.272192
130.196887	3995.063390	24.277210
130.034909	4000.188144	24.282227
130.767647	4001.528276	24.287245
130.894514	4017.076261	24.292263
130.966673	4023.163167	24.297280
131.034481	4036.161754	24.302298
131.018107	4031.490734	24.307315
131.428094	4019.645780	24.312333
131.618405	4047.024027	24.317351
131.849279	4055.300182	24.322368
131.996176	4050.054906	24.327386
131.507670	4053.439844	24.332403
131.774220	4044.919916	24.337421
131.861047	4059.992252	24.342439
132.393027	4071.585364	24.347456
132.536355	4081.620181	24.352474
132.564785	4076.577946	24.357491
132.524270	4075.365407	24.362509
132.715407	4100.221830	24.367527
132.514084	4110.180931	24.372544
132.575184	4114.236129	24.377562
132.903009	4113.511178	24.382579
133.446425	4118.609574	24.387597
133.263677	4132.589063	24.392615
133.710006	4139.252804	24.397632
133.749145	4139.640572	24.402650
133.833561	4133.527199	24.407667
133.958646	4129.169013	24.412685
134.121860	4131.050928	24.417703
134.122831	4128.442478	24.422720
134.506589	4140.744816	24.427738
134.176934	4152.472095	24.432755
134.384476	4152.475324	24.437773
134.561587	4158.460685	24.442791
134.400879	4155.602947	24.447808
134.823865	4170.570235	24.452826
134.850201	4190.356896	24.457843
134.882227	4190.058793	24.462861
135.187110	4216.777031	24.467879
135.417609	4220.532990	24.472896
135.604963	4219.917864	24.477914
135.886066	4218.656107	24.482931
136.155008	4229.771117	24.487949
136.348992	4229.939195	24.492967
136.339460	4227.958880	24.497984
136.662495	4234.502476	24.503002
136.619803	4229.899529	24.508019
137.056609	4229.987323	24.513037
137.213241	4231.017530	24.518055
137.090883	4229.285793	24.523072
137.136341	4219.782162	24.528090
137.141425	4227.183853	24.533107
137.288885	4251.029563	24.538125
137.329776	4258.637176	24.543143
137.315943	4254.256239	24.548160
137.341855	4263.857791	24.553178
137.639824	4281.632632	24.558195
138.181834	4287.929425	24.563213
138.125431	4293.271096	24.568231
138.330160	4298.817667	24.573248
138.463714	4310.294498	24.578266
138.493623	4322.759787	24.583283
138.704842	4316.562787	24.588301
138.576388	4319.925691	24.593319
139.055502	4333.943643	24.598336
139.273709	4350.280857	24.603354
139.024309	4354.090554	24.608371
139.505033	4344.652730	24.613389
139.630833	4364.695636	24.618407
139.288298	4355.794654	24.623424
139.554203	4362.602880	24.628442
139.931871	4371.731780	24.633459
139.932892	4367.773189	24.638477
140.000952	4370.523277	24.643495
140.234678	4381.502472	24.648512
140.642137	4391.993093	24.653530
140.986202	4398.215938	24.658547
141.225092	4396.595763	24.663565
141.369075	4386.224509	24.668583
141.226610	4391.703278	24.673600
141.428654	4394.954496	24.678618
141.422019	4414.062983	24.683635
141.878511	4414.916086	24.688653
141.982308	4414.795109	24.693671
141.938630	4419.007868	24.698688
142.366499	4403.038112	24.703706
142.039460	4401.224815	24.708723
142.138321	4403.487501	24.713741
142.466704	4427.425248	24.718759
142.438471	4450.274235	24.723776
142.944776	4438.399664	24.728794
142.734896	4438.056482	24.733811
142.921146	4434.347603	24.738829
143.030996	4431.425814	24.743847
142.783743	4428.153555	24.748864
143.314970	4440.620754	24.753882
143.300326	4458.806928	24.758899
143.305314	4464.125521	24.763917
143.885219	4464.945241	24.768935
143.940850	4467.739135	24.773952
144.021144	4482.211340	24.778970
143.921578	4488.614621	24.783987
144.226722	4504.135602	24.789005
144.219850	4502.583193	24.794023
144.371392	4510.698670	24.799040
145.152954	4503.448618	24.804058
144.770285	4513.937586	24.809075
144.867725	4516.763954	24.814093
145.011542	4527.349022	24.819111
144.749385	4552.066877	24.824128
145.325971	4551.555153	24.829146
145.091190	4553.265462	24.834163
145.634895	4558.305685	24.839181
145.834421	4569.838741	24.844199
145.507742	4582.438362	24.849216
145.882286	4600.461172	24.854234
146.156490	4604.583656	24.859251
146.116838	4600.148221	24.864269
146.474163	4617.509274	24.869287
146.596628	4633.694875	24.874304
146.795647	4636.443845	24.879322
146.822202	4651.445603	24.884339
146.755053	4655.547727	24.889357
147.157404	4656.922040	24.894375
147.194816	4669.168237	24.899392
148.052777	4678.674296	24.904410
147.764380	4690.273101	24.909427
148.275592	4697.422077	24.914445
148.644907	4682.610242	24.919463
148.599537	4677.917833	24.924480
148.989863	4671.721810	24.929498
148.952577	4682.490070	24.934515
148.965415	4676.870245	24.939533
148.942112	4693.843449	24.944551
148.874453	4706.996881	24.949568
149.273294	4707.009057	24.954586
149.407906	4711.483405	24.959603
149.775760	4706.851460	24.964621
149.753635	4717.897580	24.969639
149.770695	4729.769594	24.974656
150.035807	4731.115799	24.979674
149.963034	4742.462852	24.984691
149.865969	4742.206543	24.989709
150.319500	4759.047480	24.994727
150.378830	4768.660358	24.999744
150.423620	4768.136885	25.004762
150.582616	4770.700348	25.009779
150.882203	4790.520973	25.014797
151.142834	4800.251411	25.019815
151.069086	4807.343536	25.024832
151.163256	4795.064309	25.029850
151.374805	4810.048645	25.034867
151.749415	4811.429919	25.039885
152.032424	4801.909520	25.044903
151.913140	4821.300529	25.049920
152.261236	4819.222854	25.054938
152.551512	4841.689043	25.059955
152.551835	4841.337105	25.064973
152.466790	4845.479246	25.069991
152.576648	4842.236483	25.075008
152.736400	4845.886949	25.080026
153.058820	4860.101364	25.085043
153.065084	4866.671977	25.090061
153.441529	4871.649774	25.095079
153.389669	4885.070457	25.100096
153.411847	4877.401957	25.105114
153.835887	4889.256062	25.110131
153.653268	4896.636717	25.115149
153.916241	4894.863678	25.120167
153.778223	4907.921807	25.125184
154.408703	4920.713579	25.130202
154.468238	4932.885453	25.135219
153.958618	4935.354283	25.140237
154.599596	4942.433107	25.145255
154.610962	4960.703372	25.150272
155.028668	4962.092108	25.155290
155.488409	4980.375719	25.160307
155.330805	4991.256209	25.165325
155.390340	4990.688556	25.170343
155.304960	5005.528421	25.175360
156.379952	5005.406431	25.180378
156.913592	5007.597759	25.185395
156.896814	5000.987720	25.190413
157.318421	4991.378943	25.195431
157.140502	4995.454965	25.200448
157.624342	4983.602989	25.205466
157.734919	4994.882524	25.210483
157.376483	4993.772844	25.215501
157.756252	4987.677271	25.220519
157.763868	4982.964202	25.225536
157.807181	4988.183717	25.230554
157.709165	4993.819542	25.235571
157.937865	4993.342848	25.240589
158.038602	4988.636046	25.245607
157.826322	5008.782105	25.250624
158.236374	5011.906160	25.255642
158.122550	5022.701476	25.260659
158.028694	5040.506096	25.265677
158.301165	5055.886159	25.270695
158.269718	5073.411970	25.275712
158.684494	5076.068668	25.280730
158.847955	5088.761349	25.285747
158.839880	5113.873983	25.290765
159.503280	5112.807681	25.295783
159.463535	5130.484551	25.300800
160.059686	5144.042505	25.305818
160.238803	5142.570731	25.310835
159.994514	5142.093044	25.315853
160.205229	5154.219241	25.320871
160.660940	5173.533790	25.325888
160.257877	5180.469843	25.330906
160.816948	5186.828760	25.335923
161.016373	5191.218119	25.340941
160.971210	5197.673731	25.345959
161.137780	5209.799391	25.350976
161.303131	5228.233131	25.355994
161.271418	5236.605279	25.361011
161.448157	5230.139567	25.366029
161.976246	5246.180818	25.371047
161.796995	5255.452267	25.376064
162.122144	5268.425108	25.381082
162.295059	5285.273999	25.386099
162.301966	5289.916091	25.391117
162.737496	5283.438702	25.396135
162.708970	5306.093686	25.401152
162.795924	5319.727662	25.406170
163.392879	5319.663400	25.411187
163.114491	5318.925165	25.416205
163.518596	5332.991063	25.421223
163.379621	5350.673157	25.426240
163.614468	5349.494164	25.431258
163.770468	5354.069508	25.436275
163.986370	5370.128607	25.441293
164.513163	5372.540047	25.446311
164.585628	5377.230001	25.451328
164.583471	5389.873115	25.456346
164.948114	5385.379711	25.461363
165.112671	5407.569809	25.466381
165.219613	5399.838222	25.471399
165.143590	5405.907233	25.476416
165.545585	5434.964979	25.481434
165.789552	5426.343296	25.486451
165.832044	5435.040737	25.491469
166.043215	5421.005228	25.496487
166.260525	5446.720612	25.501504
166.332947	5459.123082	25.506522
166.515638	5465.307264	25.511539
166.547979	5471.228456	25.516557
167.087006	5484.100774	25.521575
166.882905	5487.059831	25.526592
167.114036	5491.199513	25.531610
167.117432	5490.968724	25.536627
167.224921	5517.767087	25.541645
167.358610	5514.425746	25.546663
167.540019	5535.293761	25.551680
167.791174	5544.452918	25.556698
168.187986	5542.831341	25.561715
168.125002	5565.773929	25.566733
168.489237	5577.199006	25.571751
168.577360	5581.422193	25.576768
168.868151	5582.767382	25.581786
169.125373	5597.071992	25.586803
169.201820	5610.703232	25.591821
169.549357	5605.067934	25.596839
169.554475	5608.281070	25.601856
169.900087	5625.949556	25.606874
170.207291	5628.231548	25.611891
170.060765	5649.701620	25.616909
170.421266	5643.219945	25.621927
171.157081	5640.488642	25.626944
170.787208	5648.064394	25.631962
171.185227	5640.800812	25.636979
171.232746	5655.262980	25.641997
171.851800	5656.801217	25.647015
171.877132	5655.188245	25.652032
172.028836	5647.490485	25.657050
172.211438	5639.165483	25.662067
171.966379	5642.693232	25.667085
171.806514	5631.496034	25.672103
172.219936	5639.441643	25.677120
172.459888	5657.622974	25.682138
172.808930	5659.910658	25.687156
172.362123	5669.054486	25.692173
172.704490	5671.580318	25.697191
172.873696	5690.243527	25.702208
172.844280	5692.585086	25.707226
173.364069	5708.517538	25.712244
173.324428	5739.091170	25.717261
173.175543	5741.835214	25.722279
173.380888	5744.604206	25.727296
173.671230	5761.295996	25.732314
173.756294	5765.697719	25.737332
174.074930	5793.991436	25.742349
174.469584	5801.077099	25.747367
174.553344	5799.492260	25.752384
174.443301	5821.742492	25.757402
174.684941	5831.638155	25.762420
174.958471	5836.217452	25.767437
174.784871	5856.655892	25.772455
175.423654	5862.087594	25.777472
175.434491	5864.917884	25.782490
175.802816	5869.534293	25.787508
176.180923	5887.044137	25.792525
176.655812	5888.838541	25.797543
176.688848	5883.517359	25.802560
176.697220	5885.940906	25.807578
176.709811	5895.988648	25.812596
176.864895	5903.563624	25.817613
177.206368	5901.406182	25.822631
177.673081	5906.355223	25.827648
177.605580	5919.571859	25.832666
178.159797	5925.731851	25.837684
177.889220	5930.321539	25.842701
178.207944	5931.099056	25.847719
178.669286	5928.263426	25.852736
178.327920	5940.083356	25.857754
178.579680	5945.485320	25.862772
178.839768	5968.529866	25.867789
178.641569	5966.982936	25.872807
178.639363	5969.189309	25.877824
178.741430	5982.236224	25.882842
178.958069	5999.440532	25.887860
178.941008	6026.064640	25.892877
179.065613	6036.499546	25.897895
179.737635	6042.880318	25.902912
179.558558	6055.683146	25.907930
180.226240	6082.022523	25.912948
180.109576	6100.920890	25.917965
180.756351	6107.334999	25.922983
181.176837	6119.903355	25.928000
181.402315	6117.986351	25.933018
181.627117	6112.952360	25.938036
181.576422	6108.031621	25.943053
181.658049	6128.159689	25.948071
181.954938	6137.184842	25.953088
181.887891	6156.401909	25.958106
182.025558	6152.465966	25.963124
182.473927	6161.019566	25.968141
182.405999	6172.651943	25.973159
182.602514	6178.622274	25.978176
182.555585	6187.427837	25.983194
183.412055	6189.916849	25.988212
183.399323	6203.609804	25.993229
183.486916	6211.515825	25.998247
183.790474	6211.396483	26.003264
183.950422	6213.841501	26.008282
184.036238	6207.236447	26.013300
184.767049	6223.648039	26.018317
184.693661	6240.365787	26.023335
185.310138	6236.965786	26.028352
184.711734	6246.705181	26.033370
185.409782	6235.987961	26.038388
185.337163	6244.531609	26.043405
185.053888	6252.416236	26.048423
185.629318	6276.168329	26.053440
185.529389	6271.935330	26.058458
185.420136	6279.599054	26.063476
186.025570	6296.757562	26.068493
186.130385	6300.870290	26.073511
186.310253	6308.817029	26.078528
186.267343	6333.191950	26.083546
186.857267	6332.442500	26.088564
186.976392	6339.084075	26.093581
186.681479	6346.439072	26.098599
187.282657	6358.265814	26.103616
187.461517	6362.962504	26.108634
187.658929	6370.770916	26.113652
187.689636	6390.324942	26.118669
188.174597	6394.430012	26.123687
188.286221	6392.051377	26.128704
188.005980	6412.532572	26.133722
188.663542	6414.756791	26.138740
188.753520	6415.865102	26.143757
188.969984	6425.710171	26.148775
189.135979	6433.018192	26.153792
189.236233	6440.221308	26.158810
189.580091	6448.825412	26.163828
189.696370	6453.730147	26.168845
189.739284	6470.399783	26.173863
190.353972	6473.879380	26.178880
190.376546	6481.546623	26.183898
190.945137	6487.973809	26.188916
190.622878	6502.982206	26.193933
190.486339	6516.304470	26.198951
190.862858	6507.602017	26.203968
190.879533	6522.294533	26.208986
190.871338	6536.760416	26.214004
190.936887	6564.053815	26.219021
191.190889	6576.919394	26.224039
191.707947	6586.885012	26.229056
191.766782	6602.051052	26.234074
192.309914	6615.202819	26.239092
192.851848	6609.145199	26.244109
192.885662	6630.048114	26.249127
193.086977	6636.412398	26.254144
192.957425	6640.100061	26.259162
193.539248	6646.881897	26.264180
193.738778	6665.827143	26.269197
193.891334	6665.470488	26.274215
194.405767	6658.399064	26.279232
194.601847	6660.910640	26.284250
194.701705	6665.215663	26.289268
195.175003	6682.881571	26.294285
195.350735	6687.871065	26.299303
195.398905	6687.341064	26.304320
195.497815	6682.887658	26.309338
195.957087	6678.162067	26.314356
195.787486	6688.368792	26.319373
195.754579	6701.409466	26.324391
195.896192	6702.342300	26.329408
195.850773	6717.455584	26.334426
196.259345	6725.834928	26.339444
196.526358	6743.848443	26.344461
196.175018	6756.389686	26.349479
196.492266	6763.280657	26.354496
196.528755	6786.502749	26.359514
196.955628	6793.915898	26.364532
197.395646	6814.866927	26.369549
197.601746	6841.705203	26.374567
197.977776	6850.015958	26.379584
197.790597	6863.596545	26.384602
197.987883	6855.684319	26.389620
198.540479	6865.678109	26.394637
198.517779	6883.961752	26.399655
198.956109	6897.599684	26.404672
198.789621	6917.102673	26.409690
198.794535	6916.801910	26.414708
199.585089	6933.274472	26.419725
199.601797	6941.547772	26.424743
200.014373	6942.599668	26.429760
199.721935	6959.867877	26.434778
199.844941	6976.255460	26.439796
200.415441	6969.009242	26.444813
200.167602	6991.978545	26.449831
200.852196	7012.894940	26.454848
200.818704	7009.935322	26.459866
201.263039	7033.918146	26.464884
201.211343	7033.372343	26.469901
201.276914	7041.524997	26.474919
201.640502	7048.308413	26.479936
201.778837	7055.810316	26.484954
201.747708	7060.738809	26.489972
202.121011	7076.700008	26.494989
201.943616	7084.050893	26.500007
202.680661	7111.528849	26.505024
202.699584	7119.632544	26.510042
203.015774	7131.332114	26.515060
203.449881	7147.564509	26.520077
203.432777	7157.367507	26.525095
204.052997	7171.022878	26.530112
204.131865	7188.022848	26.535130
203.927833	7178.700025	26.540148
204.397349	7185.890513	26.545165
204.370690	7209.533999	26.550183
204.714381	7210.473643	26.555200
204.918616	7236.967931	26.560218
205.118099	7243.901412	26.565236
205.459311	7258.794599	26.570253
205.277758	7277.219145	26.575271
205.661280	7286.948940	26.580288
205.884610	7301.081918	26.585306
206.384341	7309.970268	26.590324
206.708927	7322.979166	26.595341
206.627863	7334.428694	26.600359
207.099733	7342.205631	26.605376
207.128354	7336.890201	26.610394
207.373399	7353.171375	26.615412
207.412491	7353.655713	26.620429
207.594144	7384.422803	26.625447
207.780543	7395.254018	26.630464
208.334154	7407.584819	26.635482
208.312572	7422.897253	26.640500
208.960932	7430.902622	26.645517
208.819802	7433.318029	26.650535
208.765819	7448.657896	26.655552
209.122889	7468.211315	26.660570
209.449983	7474.878865	26.665588
209.576178	7481.029860	26.670605
209.540953	7495.668061	26.675623
209.946197	7516.150838	26.680640
210.211447	7527.949695	26.685658
210.311530	7537.981664	26.690676
210.543566	7535.746000	26.695693
210.600304	7552.827204	26.700711
211.084551	7574.049177	26.705728
211.838091	7570.544341	26.710746
212.043243	7572.086584	26.715764
212.340120	7555.725335	26.720781
212.501206	7588.032070	26.725799
212.646611	7592.481832	26.730816
213.177729	7596.541003	26.735834
213.348916	7599.843673	26.740852
213.231713	7592.763572	26.745869
213.481564	7588.711861	26.750887
213.652425	7586.137383	26.755904
213.665369	7606.807178	26.760922
213.486970	7615.341477	26.765940
214.288900	7623.606688	26.770957
214.227175	7620.725657	26.775975
214.090638	7625.094417	26.780992
214.525483	7637.385951	26.786010
214.506783	7654.067017	26.791028
214.530376	7660.196440	26.796045
214.705335	7684.868249	26.801063
214.992631	7683.986808	26.806080
215.174699	7702.667605	26.811098
215.234836	7718.425220	26.816116
215.432698	7726.876933	26.821133
215.742082	7755.937338	26.826151
215.644429	7773.397934	26.831168
216.088993	7790.724066	26.836186
216.128293	7814.157499	26.841204
216.748181	7820.105761	26.846221
216.770701	7835.188408	26.851239
216.901900	7855.433359	26.856256
217.679014	7877.745478	26.861274
217.698069	7879.918675	26.866292
218.248064	7887.582946	26.871309
218.188396	7902.929705	26.876327
218.369332	7920.145161	26.881344
219.300777	7920.839664	26.886362
218.717994	7932.533985	26.891380
219.370535	7936.178579	26.896397
219.775701	7955.862492	26.901415
219.728472	7962.876434	26.906432
219.791655	7965.100637	26.911450
220.274843	7980.002554	26.916468
220.242396	7977.045732	26.921485
220.445598	8003.862832	26.926503
220.676180	8018.189801	26.931520
220.804300	8021.757233	26.936538
220.829332	8035.903942	26.941556
221.245646	8035.832913	26.946573
221.539279	8072.206585	26.951591
221.746249	8087.900138	26.956608
221.912667	8093.980927	26.961626
222.012482	8103.792759	26.966644
222.652549	8119.666830	26.971661
222.721969	8126.143302	26.976679
222.934816	8141.538995	26.981696
223.164657	8155.083291	26.986714
223.294474	8172.331097	26.991732
223.649409	8179.237730	26.996749
223.893835	8202.867839	27.001767
224.144546	8200.724303	27.006784
224.442793	8229.158874	27.011802
224.358057	8244.886601	27.016820
224.992599	8241.105129	27.021837
224.560005	8265.144134	27.026855
224.939209	8279.256172	27.031872
225.212298	8290.686471	27.036890
225.505456	8313.451727	27.041908
225.823535	8326.818546	27.046925
225.915773	8328.040042	27.051943
226.138662	8352.761683	27.056960
226.822357	8372.021232	27.061978
226.222644	8381.286396	27.066996
226.768632	8393.155300	27.072013
226.927565	8407.397577	27.077031
227.029522	8426.395712	27.082048
227.507806	8444.300646	27.087066
227.301596	8461.494013	27.092084
228.341548	8479.488923	27.097101
228.363696	8502.149571	27.102119
228.583039	8508.988959	27.107136
228.705465	8505.258958	27.112154
228.664982	8521.804330	27.117172
228.940598	8529.735583	27.122189
229.311676	8549.483365	27.127207
229.598119	8559.173275	27.132224
230.336554	8561.477398	27.137242
230.684743	8563.968874	27.142260
230.890976	8558.492149	27.147277
231.316255	8566.227769	27.152295
231.289825	8572.951834	27.157312
231.351352	8582.151970	27.162330
231.440518	8592.175384	27.167348
231.934947	8599.977574	27.172365
231.686929	8606.260937	27.177383
231.765002	8617.797734	27.182400
231.618572	8625.344282	27.187418
232.038592	8655.708191	27.192436
232.363827	8670.998398	27.197453
232.543383	8697.340885	27.202471
232.645563	8715.370492	27.207488
233.108824	8723.878135	27.212506
233.098081	8738.697752	27.217524
233.850651	8760.715071	27.222541
234.338476	8768.655492	27.227559
234.490244	8784.844063	27.232576
234.776706	8779.543050	27.237594
234.811045	8813.051586	27.242612
234.953554	8815.227357	27.247629
235.392882	8821.769024	27.252647
235.403778	8850.965035	27.257664
235.493389	8855.218787	27.262682
235.672873	8882.949486	27.267700
235.986745	8900.491410	27.272717
236.450820	8916.065322	27.277735
236.606845	8923.577004	27.282752
236.791609	8931.520318	27.287770
237.017803	8952.532356	27.292788
237.258114	8981.791526	27.297805
237.553417	8981.266305	27.302823
237.565060	9004.550101	27.307840
238.054795	9007.063948	27.312858
238.152965	9030.856512	27.317876
238.140189	9039.198005	27.322893
238.637317	9065.247599	27.327911
238.334038	9080.039461	27.332928
239.210033	9100.869503	27.337946
239.223058	9123.016604	27.342964
239.769651	9138.814197	27.347981
240.275391	9145.132349	27.352999
240.733647	9157.749668	27.358016
240.831851	9155.999845	27.363034
241.244430	9160.710743	27.368052
241.494036	9173.984040	27.373069
242.071543	9171.315341	27.378087
241.771630	9188.329624	27.383104
242.536982	9178.931317	27.388122
242.535416	9186.221037	27.393140
242.814824	9195.770713	27.398157
243.197790	9205.203248	27.403175
243.052550	9203.922937	27.408192
243.442732	9212.938380	27.413210
243.433912	9220.383703	27.418228
243.504643	9231.581873	27.423245
243.882724	9246.186482	27.428263
243.849016	9269.352915	27.433280
244.008433	9270.780002	27.438298
244.139284	9288.720451	27.443316
244.256940	9307.532723	27.448333
245.362729	9319.312985	27.453351
245.116418	9330.309965	27.458368
245.054661	9338.611658	27.463386
245.327839	9354.739002	27.468404
245.258528	9372.893001	27.473421
245.524588	9379.411539	27.478439
245.754343	9393.453949	27.483456
245.973050	9427.742291	27.488474
246.541470	9446.833145	27.493492
246.533611	9470.988113	27.498509
246.867164	9492.521920	27.503527
247.237781	9497.734536	27.508544
247.485431	9509.524387	27.513562
247.663441	9528.994929	27.518580
247.852116	9540.592893	27.523597
248.427560	9548.095440	27.528615
248.473790	9568.055705	27.533632
249.013279	9578.411798	27.538650
249.510566	9600.128231	27.543668
249.590104	9613.919954	27.548685
249.895098	9620.097379	27.553703
250.234776	9635.867425	27.558720
250.401727	9622.383367	27.563738
250.591964	9653.289711	27.568756
251.127160	9677.808207	27.573773
251.480470	9676.751910	27.578791
251.401070	9693.616866	27.583808
251.613843	9697.392040	27.588826
251.861531	9719.650866	27.593844
251.881725	9740.818501	27.598861
252.203806	9758.080374	27.603879
252.211021	9775.330481	27.608896
252.473807	9783.002169	27.613914
252.916863	9814.880070	27.618932
252.783702	9832.570928	27.623949
253.368262	9848.595336	27.628967
253.472705	9866.404520	27.633984
253.469029	9885.496683	27.639002
254.370133	9912.068567	27.644020
254.322259	9927.375940	27.649037
254.619767	9945.864637	27.654055
254.436781	9973.075772	27.659072
255.154286	9977.621527	27.664090
255.296020	10002.671870	27.669108
254.986722	10028.131560	27.674125
255.923782	10039.119417	27.679143
256.087656	10059.944702	27.684160
256.392917	10092.506837	27.689178
257.009570	10101.676002	27.694196
257.095998	10115.233060	27.699213
257.537880	10121.501499	27.704231
257.057729	10145.763088	27.709248
257.829593	10172.500130	27.714266
257.951058	10192.886730	27.719284
257.991554	10207.198238	27.724301
258.642118	10228.738169	27.729319
258.435765	10235.573798	27.734336
258.585010	10267.733532	27.739354
259.557882	10285.365041	27.744372
259.564949	10299.971259	27.749389
260.401033	10304.002023	27.754407
260.662620	10327.215730	27.759424
261.373001	10328.892982	27.764442
261.549236	10333.229710	27.769460
261.154646	10344.802523	27.774477
261.761023	10354.907809	27.779495
261.951784	10362.414431	27.784512
262.230070	10371.485257	27.789530
262.595454	10378.306049	27.794548
262.549220	10404.829670	27.799565
262.941812	10396.562807	27.804583
262.881858	10401.486067	27.809600
262.886823	10419.277641	27.814618
263.328030	10425.636117	27.819636
263.218585	10452.319146	27.824653
263.279262	10466.335293	27.829671
263.873125	10486.170775	27.834688
264.293642	10486.909660	27.839706
264.546062	10504.261837	27.844724
264.464704	10534.284410	27.849741
264.807704	10540.606377	27.854759
265.237793	10570.828900	27.859776
265.418693	10584.996233	27.864794
265.809607	10599.042226	27.869812
265.974103	10613.841720	27.874829
266.300819	10628.904324	27.879847
266.271900	10652.459549	27.884864
266.712504	10685.880469	27.889882
267.186669	10693.313640	27.894900
266.980331	10717.321305	27.899917
267.759673	10739.813549	27.904935
267.779048	10758.401132	27.909952
268.167154	10791.372462	27.914970
268.533105	10794.485280	27.919988
268.585625	10810.344107	27.925005
269.462044	10826.319704	27.930023
269.816540	10850.618557	27.935040
270.175040	10859.926922	27.940058
270.528477	10869.258974	27.945076
270.409419	10879.266233	27.950093
270.586110	10874.321415	27.955111
270.895141	10906.632495	27.960128
271.090774	10930.041526	27.965146
271.150216	10945.932430	27.970164
270.913792	10962.608810	27.975181
271.501994	10974.491583	27.980199
272.167968	11002.407130	27.985216
272.254537	11024.688877	27.990234
273.112140	11031.911540	27.995252
273.232079	11052.079694	28.000269
273.503791	11052.016803	28.005287
274.126322	11069.591261	28.010304
274.292282	11088.559932	28.015322
274.494078	11101.043913	28.020340
274.440085	11117.327141	28.025357
274.822019	11130.988280	28.030375
275.078955	11124.948489	28.035392
275.365966	11152.389634	28.040410
275.649595	11163.918731	28.045428
275.935017	11185.162623	28.050445
276.376294	11198.479990	28.055463
276.490897	11209.844824	28.060480
276.414145	11232.243651	28.065498
276.600328	11241.612220	28.070516
276.878489	11264.299086	28.075533
277.175914	11292.221671	28.080551
277.454764	11309.082706	28.085568
277.702159	11335.993430	28.090586
277.904753	11343.768775	28.095604
278.240188	11369.883510	28.100621
278.779480	11399.812248	28.105639
278.760747	11415.583394	28.110656
278.581779	11442.406389	28.115674
279.344384	11457.510414	28.120692
279.353420	11490.174751	28.125709
279.916647	11501.694924	28.130727
280.811159	11513.937153	28.135744
281.121365	11543.543191	28.140762
281.065434	11534.711723	28.145780
281.234461	11548.725882	28.150797
281.821898	11560.231068	28.155815
281.960825	11563.434330	28.160832
282.207992	11583.370997	28.165850
282.747788	11597.576043	28.170868
282.578760	11612.201519	28.175885
282.833872	11629.662401	28.180903
283.557888	11635.691024	28.185920
283.337094	11667.546788	28.190938
283.448316	11672.885698	28.195956
283.513795	11709.919064	28.200973
283.995873	11722.012944	28.205991
284.336033	11740.669989	28.211008
284.031153	11761.908177	28.216026
284.860251	11777.668806	28.221044
285.263012	11810.812342	28.226061
285.325785	11827.721438	28.231079
285.746229	11854.156166	28.236096
285.912960	11872.932618	28.241114
286.590837	11877.806909	28.246132
287.092890	11900.130734	28.251149
287.193119	11926.591699	28.256167
287.697891	11941.931799	28.261184
287.967505	11957.196529	28.266202
288.535715	11964.080607	28.271220
288.640074	11982.055235	28.276237
288.779814	11989.455239	28.281255
289.619766	12004.427253	28.286272
289.547873	12035.075814	28.291290
289.910913	12046.816959	28.296308
290.070409	12059.349641	28.301325
290.135726	12066.988086	28.306343
290.378898	12079.926877	28.311360
290.295673	12103.838271	28.316378
291.084067	12123.623950	28.321396
291.180242	12147.307234	28.326413
291.275896	12163.490374	28.331431
291.907158	12172.403850	28.336448
292.035195	12195.307490	28.341466
292.706667	12205.142421	28.346484
292.985451	12233.941077	28.351501
293.319564	12240.749712	28.356519
293.836038	12253.051030	28.361536
293.748998	12276.045467	28.366554
294.281799	12286.243709	28.371572
294.295724	12310.229961	28.376589
294.381171	12343.794157	28.381607
294.713507	12343.737794	28.386624
294.882478	12372.841618	28.391642
295.223385	12385.621119	28.396660
295.575477	12401.217724	28.401677
295.529451	12428.693221	28.406695
296.408355	12448.137387	28.411712
296.236393	12474.839609	28.416730
296.845028	12505.312814	28.421748
297.040977	12519.685786	28.426765
297.146117	12542.543278	28.431783
297.603948	12555.095601	28.436800
297.621187	12586.492344	28.441818
298.342392	12599.748083	28.446836
298.577794	12634.042881	28.451853
298.741200	12640.345717	28.456871
299.279788	12666.347842	28.461888
299.747118	12680.137221	28.466906
300.202781	12698.535994	28.471924
300.465913	12716.640419	28.476941
300.624418	12744.079509	28.481959
300.731455	12738.244306	28.486976
300.846622	12741.449366	28.491994
300.872774	12770.181989	28.497012
301.199054	12795.897948	28.502029
301.634146	12819.330043	28.507047
301.924527	12830.901766	28.512064
301.760508	12861.180266	28.517082
301.907653	12880.011550	28.522100
302.729532	12913.863382	28.527117
303.070193	12935.328942	28.532135
303.729426	12955.807472	28.537152
303.786928	12986.454579	28.542170
303.916298	12998.428056	28.547188
304.585633	13017.633352	28.552205
304.584147	13045.204961	28.557223
305.274530	13050.694464	28.562240
305.233656	13080.243931	28.567258
305.590567	13097.818011	28.572276
306.105921	13108.051175	28.577293
306.264222	13137.084075	28.582311
306.722480	13161.781343	28.587328
306.702832	13190.092089	28.592346
306.853564	13216.567308	28.597364
307.208435	13235.645177	28.602381
307.335024	13259.169848	28.607399
307.832326	13281.459341	28.612416
308.118822	13301.802916	28.617434
308.605663	13347.598820	28.622452
308.861165	13370.910108	28.627469
309.405912	13402.935121	28.632487
309.994686	13416.714522	28.637504
310.020918	13436.721495	28.642522
310.257168	13459.558621	28.647540
310.777499	13485.226282	28.652557
310.830472	13506.800011	28.657575
311.314131	13526.186291	28.662592
311.775791	13561.053937	28.667610
312.201363	13577.276172	28.672628
312.711207	13591.108157	28.677645
312.796953	13608.935601	28.682663
312.854349	13620.302128	28.687680
313.187471	13655.454377	28.692698
313.304058	13674.375151	28.697716
313.688023	13697.214997	28.702733
314.211391	13720.531385	28.707751
314.641817	13735.465517	28.712768
314.676129	13761.086268	28.717786
315.179301	13797.472978	28.722804
315.415086	13811.779059	28.727821
315.828910	13831.468774	28.732839
316.428643	13849.722141	28.737856
316.721569	13881.707761	28.742874
317.103517	13895.499678	28.747892
317.252480	13901.397246	28.752909
317.409149	13920.168282	28.757927
317.944347	13940.564547	28.762944
317.794030	13972.697639	28.767962
317.905267	14000.048960	28.772980
318.538466	14012.240938	28.777997
318.969716	14040.292721	28.783015
319.066272	14061.833197	28.788032
319.434053	14091.041210	28.793050
319.884591	14116.653640	28.798068
320.114501	14140.829114	28.803085
319.909623	14151.371034	28.808103
320.348339	14180.870059	28.813120
320.923600	14214.546310	28.818138
321.202237	14239.181918	28.823156
321.627109	14248.850829	28.828173
321.551969	14281.853031	28.833191
321.769531	14294.771036	28.838208
322.282526	14325.236681	28.843226
323.093133	14345.082093	28.848244
323.537222	14370.598283	28.853261
323.913324	14383.707641	28.858279
324.303725	14397.473375	28.863296
324.734122	14404.202408	28.868314
324.940461	14424.886847	28.873332
325.258496	14443.084989	28.878349
325.846036	14468.386948	28.883367
325.938200	14469.167675	28.888384
326.086099	14489.444235	28.893402
326.268920	14509.415627	28.898420
327.123756	14542.307267	28.903437
327.301950	14552.073845	28.908455
327.456305	14559.381208	28.913472
327.641943	14585.290287	28.918490
327.819201	14617.201907	28.923508
328.158267	14631.282050	28.928525
328.235095	14659.128699	28.933543
328.550332	14686.040880	28.938560
328.702761	14716.354075	28.943578
329.341837	14736.288191	28.948596
329.632390	14762.022624	28.953613
330.271563	14802.856901	28.958631
330.683061	14832.508167	28.963648
330.995050	14838.520978	28.968666
331.198994	14856.468944	28.973684
331.629299	14869.424754	28.978701
332.247033	14896.522124	28.983719
332.615593	14910.887611	28.988736
332.364609	14946.626118	28.993754
332.882656	14963.111830	28.998772
333.259728	14987.221698	29.003789
333.355812	15016.506202	29.008807
333.689136	15052.058577	29.013824
334.045443	15064.588649	29.018842
334.068829	15099.439019	29.023860
334.614900	15122.893932	29.028877
335.079600	15158.043448	29.033895
335.198121	15193.828616	29.038912
336.105560	15221.704480	29.043930
335.819591	15243.483069	29.048948
336.655874	15261.197784	29.053965
336.965101	15295.328403	29.058983
337.453544	15310.457704	29.064000
337.455863	15320.152935	29.069018
337.856703	15365.979761	29.074036
338.512761	15378.413274	29.079053
338.732724	15405.586662	29.084071
338.913080	15421.663707	29.089088
339.189525	15447.437801	29.094106
339.319937	15484.025401	29.099124
339.786949	15511.865778	29.104141
339.781073	15544.181402	29.109159
340.328133	15572.227724	29.114176
340.605045	15597.935784	29.119194
341.448434	15613.851474	29.124212
342.075894	15644.127313	29.129229
342.262065	15662.559788	29.134247
342.661393	15678.492165	29.139264
343.002905	15696.568051	29.144282
343.343683	15725.641612	29.149300
343.567820	15748.414604	29.154317
343.864664	15770.397055	29.159335
343.743953	15785.383147	29.164352
344.350133	15804.868533	29.169370
344.235236	15844.206672	29.174388
344.559118	15859.344757	29.179405
345.039571	15890.122879	29.184423
345.615573	15917.074388	29.189440
346.017985	15939.826074	29.194458
346.041400	15969.535638	29.199476
346.808363	15992.871778	29.204493
346.816658	16011.370282	29.209511
347.172160	16040.150399	29.214528
347.720136	16055.049907	29.219546
347.591050	16089.098563	29.224564
348.345317	16112.868815	29.229581
348.553386	16147.241723	29.234599
348.972990	16172.656029	29.239616
349.667183	16194.661666	29.244634
349.786226	16229.038421	29.249652
350.378998	16249.740134	29.254669
350.470726	16273.205564	29.259687
350.908492	16305.868634	29.264704
351.335814	16325.336907	29.269722
351.060523	16365.019584	29.274740
351.367716	16384.737883	29.279757
352.430953	16407.888551	29.284775
352.728843	16433.096410	29.289792
353.420214	16449.517166	29.294810
353.761219	16489.443496	29.299828
353.924184	16512.445157	29.304845
354.358997	16530.144045	29.309863
354.549506	16547.128356	29.314880
354.730098	16564.790474	29.319898
354.805767	16614.186086	29.324916
355.241507	16636.543934	29.329933
355.690958	16663.638939	29.334951
356.147546	16700.013025	29.339968
356.247272	16728.587577	29.344986
356.722581	16766.257444	29.350004
356.819121	16789.454873	29.355021
357.476661	16821.445905	29.360039
357.728755	16852.594548	29.365056
358.284019	16881.061010	29.370074
358.682416	16918.236414	29.375092
359.380686	16954.539613	29.380109
359.676224	16966.748617	29.385127
359.928335	16989.266525	29.390144
360.677920	17021.494925	29.395162
360.374263	17050.239125	29.400180
360.951253	17071.633265	29.405197
361.123506	17096.837679	29.410215
360.990541	17135.475769	29.415232
361.760525	17167.418952	29.420250
361.970329	17210.353968	29.425268
362.367245	17241.815147	29.430285
362.659158	17273.238567	29.435303
363.029879	17300.382305	29.440320
363.465266	17335.107882	29.445338
363.864094	17370.375477	29.450356
364.624171	17403.956839	29.455373
364.750175	17433.864882	29.460391
365.252977	17463.403374	29.465408
366.261432	17489.330850	29.470426
366.328163	17508.272174	29.475444
366.696471	17540.361249	29.480461
367.377337	17553.974478	29.485479
367.445134	17569.706542	29.490496
368.073617	17579.135736	29.495514
368.240175	17607.878883	29.500532
368.478978	17638.143800	29.505549
369.028047	17639.697203	29.510567
368.756064	17670.498936	29.515584
369.281621	17673.872028	29.520602
369.559589	17712.730452	29.525620
369.520871	17752.074746	29.530637
370.295898	17770.380782	29.535655
370.550793	17797.319073	29.540672
371.016519	17815.450855	29.545690
371.120260	17852.946580	29.550708
371.487866	17881.970661	29.555725
371.774346	17914.955098	29.560743
372.068390	17946.683663	29.565760
372.739963	17976.962824	29.570778
372.916779	18007.076305	29.575796
373.324651	18046.218269	29.580813
373.536222	18081.398522	29.585831
373.911279	18107.434765	29.590848
374.435204	18133.717572	29.595866
375.039635	18177.557733	29.600884
375.613036	18206.543659	29.605901
376.140688	18225.912489	29.610919
376.546912	18260.228697	29.615936
376.989190	18279.786661	29.620954
377.397534	18305.951701	29.625972
377.737861	18329.605971	29.630989
377.874109	18366.336146	29.636007
378.212360	18388.832277	29.641024
378.670894	18416.458297	29.646042
378.817266	18449.810578	29.651060
379.243538	18481.032826	29.656077
379.821249	18504.946051	29.661095
380.147017	18545.404780	29.666112
380.663518	18566.063689	29.671130
381.138179	18598.449357	29.676148
381.359495	18634.351123	29.681165
381.635113	18667.873224	29.686183
381.848512	18699.345428	29.691200
382.328087	18715.521282	29.696218
382.377937	18759.571249	29.701236
382.901875	18775.990469	29.706253
383.639454	18812.860318	29.711271
383.880838	18849.459123	29.716288
384.686683	18872.846531	29.721306
385.291906	18911.879123	29.726324
385.467731	18934.585682	29.731341
385.931383	18945.559330	29.736359
385.905364	18975.708078	29.741376
386.944737	18999.960331	29.746394
386.767255	19033.458712	29.751412
387.048909	19064.070682	29.756429
387.575757	19086.309610	29.761447
387.894684	19125.676897	29.766464
388.207630	19159.592642	29.771482
388.754246	19186.812884	29.776500
388.613545	19220.876208	29.781517
389.148704	19238.824683	29.786535
389.356321	19282.104351	29.791552
389.940487	19313.038828	29.796570
390.214673	19348.594484	29.801588
390.492051	19394.306302	29.806605
391.236259	19424.695920	29.811623
391.295302	19468.698955	29.816640
392.065458	19503.157815	29.821658
392.706881	19530.287291	29.826676
392.798239	19566.636590	29.831693
393.494230	19599.924029	29.836711
393.557370	19627.514919	29.841728
394.420523	19644.846875	29.846746
394.178304	19674.827671	29.851764
394.581683	19701.886403	29.856781
394.832706	19733.636528	29.861799
395.057950	19764.095158	29.866816
394.959993	19802.445187	29.871834
395.528031	19846.685148	29.876852
395.787685	19885.934757	29.881869
396.316909	19918.334479	29.886887
396.556998	19958.999974	29.891904
397.171762	19983.646983	29.896922
397.891094	20022.428444	29.901940
398.436122	20063.748488	29.906957
399.160517	20103.159878	29.911975
399.607450	20140.961925	29.916992
399.950466	20177.999302	29.922010
400.400778	20201.912374	29.927028
400.569276	20238.299262	29.932045
401.333922	20263.470534	29.937063
401.669705	20301.266082	29.942080
402.017053	20321.381288	29.947098
402.202163	20357.641151	29.952116
402.714601	20411.200859	29.957133
403.247961	20428.118325	29.962151
403.432973	20464.050528	29.967168
403.826282	20486.146282	29.972186
403.874378	20536.540274	29.977204
404.302335	20577.594009	29.982221
404.768539	20621.627409	29.987239
404.829948	20660.782316	29.992256
405.319376	20683.187212	29.997274
406.271561	20738.455195	30.002292
406.289317	20784.737109	30.007309
407.118786	20825.616346	30.012327
407.830828	20849.036226	30.017344
408.449447	20860.092745	30.022362
409.177886	20895.999165	30.027380
409.674667	20909.038614	30.032397
410.408805	20934.884386	30.037415
411.117060	20953.854509	30.042432
411.267728	20981.387456	30.047450
411.568654	20986.696489	30.052468
411.927167	21000.294871	30.057485
412.128996	21013.474565	30.062503
412.150709	21050.254799	30.067520
412.831711	21083.254443	30.072538
413.307268	21100.715012	30.077556
413.142192	21126.384859	30.082573
413.545540	21154.998848	30.087591
413.765349	21199.637300	30.092608
413.696777	21227.905280	30.097626
414.120441	21268.486878	30.102644
414.256880	21312.001127	30.107661
414.953248	21350.125735	30.112679
415.067291	21405.242713	30.117696
415.737645	21455.352213	30.122714
415.963513	21501.024698	30.127732
416.142195	21552.634631	30.132749
416.761197	21586.288754	30.137767
417.122791	21637.665352	30.142784
417.359176	21694.363307	30.147802
418.311943	21743.755386	30.152820
418.938385	21789.758211	30.157837
419.250061	21827.132346	30.162855
419.366873	21873.274767	30.167872
419.906109	21913.436795	30.172890
420.761222	21951.301630	30.177908
420.731826	21992.785969	30.182925
421.172510	22032.494727	30.187943
421.541920	22080.341316	30.192960
421.899124	22118.448018	30.197978
422.730059	22156.433981	30.202996
422.631948	22184.949673	30.208013
423.529970	22225.936098	30.213031
423.465084	22265.203898	30.218048
424.081459	22300.490143	30.223066
424.705793	22339.511824	30.228084
425.601019	22390.813606	30.233101
425.920402	22429.293045	30.238119
426.493057	22452.194246	30.243136
427.216002	22476.932698	30.248154
427.076373	22509.168854	30.253172
427.341008	22555.790106	30.258189
427.806468	22589.254021	30.263207
428.150389	22623.901672	30.268224
429.027564	22663.979709	30.273242
429.374808	22689.926789	30.278260
429.620796	22735.935134	30.283277
430.391584	22774.027030	30.288295
430.459220	22809.031310	30.293312
430.641774	22839.169892	30.298330
431.703285	22862.227402	30.303348
432.387700	22902.309469	30.308365
433.070437	22926.911745	30.313383
433.759473	22960.478215	30.318400
433.575313	22987.755988	30.323418
434.200691	23007.546256	30.328436
434.097284	23047.427697	30.333453
434.859847	23089.081905	30.338471
434.686124	23126.226913	30.343488
434.860471	23171.519828	30.348506
435.240593	23211.323357	30.353524
435.694751	23257.957811	30.358541
436.488169	23299.776154	30.363559
436.896706	23340.083004	30.368576
437.174737	23390.204731	30.373594
437.614895	23434.451624	30.378612
438.139043	23478.905506	30.383629
438.980137	23512.157830	30.388647
439.027125	23553.407902	30.393664
439.354638	23595.247174	30.398682
439.787224	23642.838623	30.403700
440.041656	23687.884750	30.408717
440.617124	23738.827181	30.413735
441.026432	23778.461659	30.418752
441.309195	23837.059178	30.423770
441.691736	23878.327143	30.428788
442.185410	23936.431316	30.433805
443.061136	23979.781435	30.438823
443.491607	24013.045810	30.443840
444.179072	24057.838476	30.448858
444.524421	24092.291796	30.453876
444.856153	24158.227163	30.458893
445.219865	24191.823012	30.463911
445.968086	24225.776425	30.468928
446.708222	24267.199137	30.473946
447.154146	24286.159596	30.478964
447.934146	24334.676390	30.483981
448.342124	24369.495216	30.488999
448.806728	24395.576902	30.494016
449.289467	24431.993468	30.499034
449.775007	24459.063633	30.504052
450.062227	24487.483277	30.509069
450.481037	24524.564998	30.514087
450.848877	24560.860479	30.519104
451.191144	24596.975770	30.524122
451.582701	24621.111400	30.529140
451.402076	24658.478502	30.534157
451.545081	24696.728891	30.539175
452.220133	24733.420249	30.544192
452.430360	24783.254525	30.549210
453.215211	24825.098547	30.554228
453.538825	24863.638007	30.559245
453.662275	24904.397772	30.564263
454.440528	24950.664808	30.569280
454.536222	25004.441976	30.574298
455.104158	25060.019405	30.579316
455.320501	25116.388359	30.584333
456.162017	25146.269223	30.589351
456.949542	25194.142268	30.594368
457.016581	25248.103129	30.599386
457.858045	25285.894115	30.604404
458.317780	25332.318880	30.609421
458.477247	25382.015058	30.614439
459.131453	25418.425909	30.619456
459.839244	25474.489362	30.624474
460.545016	25505.214870	30.629492
460.676603	25555.034428	30.634509
461.574515	25591.093155	30.639527
462.073451	25627.441792	30.644544
461.866723	25675.784779	30.649562
462.851267	25710.470103	30.654580
463.479564	25762.870141	30.659597
463.802757	25815.323892	30.664615
464.129019	25835.367153	30.669632
464.053862	25887.628302	30.674650
464.739543	25926.646528	30.679668
465.632470	25958.805385	30.684685
466.056163	26005.625872	30.689703
466.385969	26056.205797	30.694720
466.596780	26092.902648	30.699738
467.368732	26149.452895	30.704756
467.593657	26182.157771	30.709773
468.341000	26234.356655	30.714791
469.199923	26278.816166	30.719808
469.400896	26320.372357	30.724826
470.187527	26351.032413	30.729844
470.489954	26396.997173	30.734861
470.589672	26431.773350	30.739879
471.459132	26478.635043	30.744896
471.586969	26528.729300	30.749914
472.394965	26563.574839	30.754932
472.624332	26603.442738	30.759949
472.643968	26655.841964	30.764967
473.216050	26700.611743	30.769984
473.481099	26748.649568	30.775002
474.172173	26795.036931	30.780020
474.465509	26859.415145	30.785037
475.187801	26904.942874	30.790055
475.615987	26969.091049	30.795072
476.185549	27013.228071	30.800090
476.818659	27049.485016	30.805108
477.338083	27091.406820	30.810125
477.455517	27136.527250	30.815143
477.813882	27187.597845	30.820160
479.030308	27233.637814	30.825178
479.110556	27278.137067	30.830196
479.589538	27321.189017	30.835213
479.937701	27369.533423	30.840231
480.803497	27423.621520	30.845248
480.946303	27465.410883	30.850266
482.105527	27504.647825	30.855284
482.867885	27533.405674	30.860301
483.266852	27560.955576	30.865319
484.190016	27580.331354	30.870336
484.684719	27616.183375	30.875354
484.895372	27635.765230	30.880372
485.253593	27659.155201	30.885389
485.336511	27687.965608	30.890407
486.160028	27713.284930	30.895424
486.180998	27750.903037	30.900442
486.495084	27791.381092	30.905460
486.882999	27831.859664	30.910477
487.287515	27871.603783	30.915495
487.716611	27906.978324	30.920512
487.731578	27955.448806	30.925530
488.273096	28009.270564	30.930548
489.014582	28072.730759	30.935565
488.683069	28127.378437	30.940583
489.565412	28174.182691	30.945600
489.825109	28241.864805	30.950618
490.469114	28294.569635	30.955636
490.951819	28350.067698	30.960653
491.242113	28402.351811	30.965671
492.008943	28469.244452	30.970688
492.344770	28532.173995	30.975706
492.648791	28579.144272	30.980724
494.038575	28622.976434	30.985741
495.214861	28652.465860	30.990759
496.156522	28697.861147	30.995776
496.426045	28742.055309	31.000794
496.664510	28793.251399	31.005812
497.049049	28829.628855	31.010829
497.416474	28868.958688	31.015847
497.865175	28908.984953	31.020864
498.127062	28962.518330	31.025882
498.297221	29016.354088	31.030900
499.202276	29059.469326	31.035917
499.098136	29113.659840	31.040935
499.967310	29164.547797	31.045952
500.186474	29219.940758	31.050970
500.640904	29275.077366	31.055988
501.686843	29335.842045	31.061005
501.875654	29393.821037	31.066023
502.427574	29442.970395	31.071040
502.870968	29495.847664	31.076058
503.182876	29563.936410	31.081076
503.506525	29620.941183	31.086093
503.949732	29682.563750	31.091111
504.730238	29738.726862	31.096128
505.150265	29800.684917	31.101146
505.092590	29856.926921	31.106164
506.025488	29926.223706	31.111181
506.544875	29982.875551	31.116199
507.270544	30050.484585	31.121216
507.782498	30098.935737	31.126234
509.097609	30146.784302	31.131252
510.243796	30182.947295	31.136269
510.414380	30234.404907	31.141287
510.697952	30291.986352	31.146304
511.421629	30324.818583	31.151322
511.528409	30371.286811	31.156340
512.262543	30407.433154	31.161357
512.685545	30451.988035	31.166375
513.444825	30505.904598	31.171392
513.898884	30555.918751	31.176410
514.122340	30596.702247	31.181428
514.717800	30636.610444	31.186445
514.999678	30682.725629	31.191463
515.628698	30724.780088	31.196480
515.847320	30780.234879	31.201498
516.238233	30830.171911	31.206516
516.862717	30877.350998	31.211533
517.557431	30916.442099	31.216551
517.709483	30959.282601	31.221568
518.043059	31012.627446	31.226586
518.769606	31060.954329	31.231604
519.702896	31111.745895	31.236621
519.968798	31160.376295	31.241639
520.849078	31206.264665	31.246656
520.880501	31252.640411	31.251674
521.030875	31314.629443	31.256692
521.881660	31364.517277	31.261709
522.204823	31411.466782	31.266727
523.106651	31462.236167	31.271744
523.391303	31498.427462	31.276762
524.313518	31558.699750	31.281780
524.901938	31611.089370	31.286797
524.717216	31666.847058	31.291815
525.477895	31720.489490	31.296832
525.860171	31773.973736	31.301850
526.142710	31840.669044	31.306868
526.669257	31904.614101	31.311885
527.261428	31969.053363	31.316903
527.482186	32021.618518	31.321920
528.065033	32091.249882	31.326938
528.462745	32149.610502	31.331956
529.259366	32208.839340	31.336973
530.029316	32276.083658	31.341991
530.646010	32338.182268	31.347008
530.916801	32398.110695	31.352026
531.581479	32458.864021	31.357044
532.483249	32514.593220	31.362061
533.107918	32578.032307	31.367079
533.547505	32637.135403	31.372096
534.116363	32693.838320	31.377114
534.391746	32753.044651	31.382132
535.129867	32808.533618	31.387149
534.955118	32876.942784	31.392167
535.801768	32945.820866	31.397184
536.533128	33004.542542	31.402202
536.858540	33075.110096	31.407220
537.395177	33142.181694	31.412237
537.779015	33209.789943	31.417255
538.067559	33285.302465	31.422272
538.747842	33352.310113	31.427290
539.337935	33424.917856	31.432308
540.293099	33472.128167	31.437325
541.228188	33530.448763	31.442343
541.953674	33587.093965	31.447360
542.850646	33638.690824	31.452378
543.615954	33691.682172	31.457396
544.521691	33728.415998	31.462413
544.674668	33779.959455	31.467431
544.923118	33834.349247	31.472448
545.626192	33880.598867	31.477466
545.904292	33935.403742	31.482484
546.709160	33985.148811	31.487501
547.274373	34025.419944	31.492519
547.800417	34075.394337	31.497536
548.734115	34114.658174	31.502554
548.979750	34161.031414	31.507572
549.797515	34205.947111	31.512589
549.766425	34265.319557	31.517607
550.100770	34325.272406	31.522624
550.781366	34365.866047	31.527642
551.293660	34423.442142	31.532660
552.572466	34458.364553	31.537677
553.141247	34513.855280	31.542695
553.094061	34558.984156	31.547712
553.763291	34600.694116	31.552730
554.000729	34646.568244	31.557748
554.240041	34691.839469	31.562765
554.984295	34746.323714	31.567783
555.335164	34794.189585	31.572800
555.475635	34845.062899	31.577818
555.744803	34911.674156	31.582836
556.464217	34975.866676	31.587853
556.959708	35044.883491	31.592871
557.419125	35102.145484	31.597888
558.141360	35169.579070	31.602906
558.541457	35231.793018	31.607924
559.522466	35296.697686	31.612941
559.888128	35363.995251	31.617959
560.313202	35431.317968	31.622976
561.000121	35486.347256	31.627994
561.745709	35555.782314	31.633012
562.169260	35615.841528	31.638029
562.860842	35681.540151	31.643047
563.173261	35744.745487	31.648064
563.855409	35818.038896	31.653082
564.262265	35887.597461	31.658100
565.007408	35947.992832	31.663117
565.641379	36018.139236	31.668135
565.788706	36092.648723	31.673152
566.839384	36163.184459	31.678170
567.155791	36230.739570	31.683188
567.929037	36281.146375	31.688205
568.360344	36369.555770	31.693223
568.546601	36448.150292	31.698240
569.506099	36513.015589	31.703258
570.113123	36579.634053	31.708276
570.736454	36643.580175	31.713293
571.049582	36725.058383	31.718311
571.430938	36801.510915	31.723328
571.940526	36875.269506	31.728346
572.430155	36954.204312	31.733364
573.310406	37035.716493	31.738381
574.115149	37113.170293	31.743399
574.537237	37186.837310	31.748416
575.064266	37238.338415	31.753434
575.737264	37323.660718	31.758452
577.242175	37386.091001	31.763469
577.368861	37450.223011	31.768487
577.842107	37527.184192	31.773504
578.664285	37582.569982	31.778522
579.224801	37655.843634	31.783540
579.818553	37729.219401	31.788557
580.776473	37799.454957	31.793575
581.203011	37860.022994	31.798592
581.772501	37910.294433	31.803610
582.340722	37970.634291	31.808628
582.779531	38036.247554	31.813645
583.112299	38112.439080	31.818663
583.679516	38182.450290	31.823680
584.659612	38240.999752	31.828698
585.450564	38295.689059	31.833716
585.945970	38355.401520	31.838733
587.053611	38407.703270	31.843751
587.809273	38472.129543	31.848768
588.014744	38529.958859	31.853786
588.764183	38579.710064	31.858804
589.316402	38617.869513	31.863821
590.015232	38667.982819	31.868839
590.649447	38716.203708	31.873856
591.796245	38763.197493	31.878874
591.996288	38812.014289	31.883892
592.658153	38855.398714	31.888909
593.219328	38902.205519	31.893927
593.361221	38956.255980	31.898944
593.788554	38996.990307	31.903962
594.313964	39048.490523	31.908980
594.493984	39100.344627	31.913997
594.984242	39168.860474	31.919015
594.976442	39229.836242	31.924032
596.015241	39293.123412	31.929050
596.290212	39357.928922	31.934068
596.563189	39433.419369	31.939085
597.132210	39513.551649	31.944103
597.457337	39592.269454	31.949120
598.332640	39665.208843	31.954138
599.026594	39732.673640	31.959156
599.352408	39804.129275	31.964173
600.184479	39882.865613	31.969191
600.800497	39961.117156	31.974208
601.612575	40029.914517	31.979226
602.297855	40116.772515	31.984244
602.713573	40188.877674	31.989261
603.742232	40265.054819	31.994279
604.412885	40314.523913	31.999296
605.834313	40383.929033	32.004314
606.371504	40459.642079	32.009332
606.836013	40511.816211	32.014349
607.699748	40569.148705	32.019367
608.160615	40625.569372	32.024384
608.847342	40691.116538	32.029402
609.187753	40761.730691	32.034420
610.105169	40818.395367	32.039437
610.234331	40877.390585	32.044455
610.608699	40940.796370	32.049472
611.179407	41016.856571	32.054490
611.756264	41093.345380	32.059508
612.116359	41172.793403	32.064525
612.735734	41245.872913	32.069543
612.958196	41321.455254	32.074560
613.653205	41405.470399	32.079578
614.096781	41492.270667	32.084596
615.018652	41561.715412	32.089613
615.606539	41644.672889	32.094631
616.212880	41725.386375	32.099648
616.894871	41808.865704	32.104666
618.474408	41875.412403	32.109684
618.917534	41944.072696	32.114701
619.727173	42010.005186	32.119719
620.444166	42081.679732	32.124736
620.957136	42159.196872	32.129754
621.570559	42223.303143	32.134772
621.921671	42289.568071	32.139789
622.528182	42348.820638	32.144807
623.129134	42434.387105	32.149824
623.895086	42505.695325	32.154842
624.667709	42576.005128	32.159860
624.721934	42652.097405	32.164877
625.568216	42722.449268	32.169895
626.082233	42791.539821	32.174912
626.715216	42860.860385	32.179930
627.093129	42940.840298	32.184948
627.834445	43021.076237	32.189965
628.493185	43091.630958	32.194983
628.829608	43175.227206	32.200000
629.674714	43238.291640	32.205018
630.442322	43327.904143	32.210036
631.069493	43402.225316	32.215053
631.717929	43470.844741	32.220071
632.145331	43545.979283	32.225088
632.901483	43623.421351	32.230106
633.486198	43682.542874	32.235124
634.068340	43756.907634	32.240141
635.201346	43837.262370	32.245159
635.850265	43899.745812	32.250176
636.245633	43958.268055	32.255194
636.854307	44024.234602	32.260212
637.494702	44085.267774	32.265229
637.997563	44158.545375	32.270247
638.427696	44234.522064	32.275264
639.186116	44295.157566	32.280282
640.853806	44350.515750	32.285300
641.183916	44415.449917	32.290317
642.187651	44481.381252	32.295335
642.955852	44530.899222	32.300352
643.378914	44585.983762	32.305370
644.248555	44642.185005	32.310388
644.300846	44718.352360	32.315405
645.020496	44780.429258	32.320423
645.412646	44848.815092	32.325440
645.959624	44925.094185	32.330458
646.643103	44987.676604	32.335476
647.319883	45053.386115	32.340493
648.034247	45118.221376	32.345511
648.513227	45197.865930	32.350528
649.435468	45267.542364	32.355546
650.068785	45337.623561	32.360564
650.555554	45412.664256	32.365581
651.294491	45489.810653	32.370599
651.415106	45563.898893	32.375616
651.909418	45648.443172	32.380634
652.453133	45730.662093	32.385652
652.579162	45814.598561	32.390669
653.450683	45915.475380	32.395687
653.913249	46005.798412	32.400704
654.616034	46089.186171	32.405722
655.156433	46189.222409	32.410740
655.908385	46291.254549	32.415757
656.457995	46386.607656	32.420775
656.808364	46491.031177	32.425792
657.882327	46579.948747	32.430810
658.814711	46665.015720	32.435828
659.430656	46777.774138	32.440845
660.540122	46861.331818	32.445863
661.047230	46955.611748	32.450880
662.220445	47027.905708	32.455898
663.055883	47114.206426	32.460916
663.618127	47212.504596	32.465933
664.909936	47264.415800	32.470951
665.291756	47339.749918	32.475968
666.174352	47420.284542	32.480986
666.749845	47482.871001	32.486004
667.463469	47568.777090	32.491021
668.015825	47631.440491	32.496039
668.465485	47718.546602	32.501056
669.266516	47809.103413	32.506074
669.994637	47870.668079	32.511092
670.135313	47952.252738	32.516109
671.271763	48018.847197	32.521127
672.137914	48104.541055	32.526144
672.696109	48174.199950	32.531162
673.365522	48242.940736	32.536180
673.906527	48325.073511	32.541197
674.712530	48395.838610	32.546215
675.437656	48462.619403	32.551232
675.896608	48543.509821	32.556250
677.267713	48612.666593	32.561268
677.509517	48690.741875	32.566285
678.307035	48761.291838	32.571303
678.881593	48826.323996	32.576320
679.140459	48901.400400	32.581338
680.000057	48957.947777	32.586356
680.151024	49047.923091	32.591373
680.522833	49122.511169	32.596391
681.019621	49201.380151	32.601408
681.476983	49278.155864	32.606426
682.255747	49363.092942	32.611444
682.699732	49467.173154	32.616461
683.332979	49558.985027	32.621479
683.985200	49658.162096	32.626496
684.144449	49754.929326	32.631514
685.138378	49843.976480	32.636532
685.737352	49951.943520	32.641549
686.768707	50049.168260	32.646567
687.825916	50151.009669	32.651584
688.336524	50242.210274	32.656602
688.998071	50324.574928	32.661620
689.731352	50421.285460	32.666637
690.488319	50519.022160	32.671655
690.859810	50616.342960	32.676672
691.597415	50733.838977	32.681690
692.397506	50824.252339	32.686708
692.903163	50915.630666	32.691725
693.671615	51017.082192	32.696743
694.507738	51120.986596	32.701760
694.848393	51238.042750	32.706778
695.865838	51332.790642	32.711796
696.451473	51434.511437	32.716813
697.150279	51532.382908	32.721831
698.346202	51640.516677	32.726848
698.854283	51743.433166	32.731866
699.466699	51849.497767	32.736884
700.030572	51945.864913	32.741901
700.896037	52044.835880	32.746919
701.941853	52157.700355	32.751936
702.180477	52261.115767	32.756954
703.279298	52350.409883	32.761972
704.471215	52438.002358	32.766989
705.315547	52531.319139	32.772007
706.396581	52615.159373	32.777024
707.091590	52709.746163	32.782042
707.760717	52786.346122	32.787060
708.787389	52871.080857	32.792077
709.488105	52954.960099	32.797095
710.240483	53043.025888	32.802112
710.662795	53119.036185	32.807130
711.681366	53185.712283	32.812148
712.285384	53275.818875	32.817165
712.633864	53356.479279	32.822183
713.747501	53437.980228	32.827200
714.283013	53518.275588	32.832218
714.990216	53597.639520	32.837236
715.580384	53690.214150	32.842253
716.197747	53769.713652	32.847271
716.862903	53854.948289	32.852288
717.364918	53959.965493	32.857306
718.037388	54055.541778	32.862324
718.568996	54142.574991	32.867341
720.405640	54216.340650	32.872359
721.281535	54290.897026	32.877376
721.812123	54372.302318	32.882394
723.185293	54445.500973	32.887412
723.795735	54524.985738	32.892429
724.528792	54602.321462	32.897447
725.221320	54665.796458	32.902464
725.767593	54734.805013	32.907482
726.472869	54798.151976	32.912500
726.933387	54874.680865	32.917517
727.696524	54948.974063	32.922535
728.346447	55016.134283	32.927552
728.746646	55085.136603	32.932570
729.012086	55150.395878	32.937588
729.530861	55234.081188	32.942605
729.839403	55324.334466	32.947623
730.842437	55415.383275	32.952640
731.013046	55504.308081	32.957658
731.871830	55602.325212	32.962676
732.548995	55706.071842	32.967693
733.039119	55813.527120	32.972711
733.780234	55906.851794	32.977728
734.317935	56010.313460	32.982746
735.231118	56098.657080	32.987764
736.522617	56206.917272	32.992781
737.172974	56311.037975	32.997799
737.904434	56407.993372	33.002816
738.526979	56506.793266	33.007834
739.224134	56604.911572	33.012852
739.974589	56702.351799	33.017869
740.569066	56807.571128	33.022887
741.421449	56910.416867	33.027904
742.327551	57013.551243	33.032922
743.682845	57108.517783	33.037940
744.537518	57203.763331	33.042957
745.275130	57292.893201	33.047975
746.388595	57387.161724	33.052992
746.967220	57488.627634	33.058010
747.375045	57574.445323	33.063028
748.164493	57664.655134	33.068045
748.740638	57778.520473	33.073063
749.421184	57875.984325	33.078080
749.859067	57971.574092	33.083098
751.115795	58050.549269	33.088116
752.330745	58142.807827	33.093133
752.655542	58239.043130	33.098151
754.420122	58327.015956	33.103168
754.660536	58432.826833	33.108186
755.252054	58518.005299	33.113204
755.898388	58613.323591	33.118221
756.740073	58703.738008	33.123239
756.926996	58796.453717	33.128256
757.358773	58905.167591	33.133274
758.291650	59016.314367	33.138292
758.978353	59132.330349	33.143309
759.901393	59227.226711	33.148327
760.491450	59338.627786	33.153344
761.209011	59449.306970	33.158362
761.800466	59556.361282	33.163380
762.260451	59689.657320	33.168397
762.905781	59807.485082	33.173415
764.103965	59903.710536	33.178432
764.891488	60022.230182	33.183450
766.045933	60132.158465	33.188468
766.761253	60240.839060	33.193485
767.009417	60346.134204	33.198503
768.036224	60455.251131	33.203520
768.709640	60577.401435	33.208538
769.441762	60691.497702	33.213556
770.417288	60801.446540	33.218573
770.771934	60918.545136	33.223591
772.014238	61030.505116	33.228608
772.306116	61148.715069	33.233626
773.201157	61258.344724	33.238644
774.175660	61377.713597	33.243661
775.157330	61488.632111	33.248679
775.970811	61580.700988	33.253696
776.797781	61673.121981	33.258714
777.372696	61781.195705	33.263732
778.091117	61893.417606	33.268749
778.585714	62002.972046	33.273767
779.523600	62108.971432	33.278784
780.327506	62200.558042	33.283802
780.921844	62310.559045	33.288820
781.801022	62422.081044	33.293837
782.593656	62529.484434	33.298855
783.561695	62637.478822	33.303872
784.076312	62761.495076	33.308890
784.638874	62868.186110	33.313908
786.116584	62956.826965	33.318925
787.002254	63064.312612	33.323943
787.948673	63167.377050	33.328960
788.680035	63284.850522	33.333978
789.349722	63386.899905	33.338996
790.569204	63487.626481	33.344013
791.103577	63588.302348	33.349031
792.006377	63681.231890	33.354048
792.533802	63798.040382	33.359066
792.944780	63906.462134	33.364084
793.860754	64013.182939	33.369101
795.037746	64117.427672	33.374119
796.313546	64216.353408	33.379136
796.903710	64324.785700	33.384154
797.693581	64431.542142	33.389172
799.481310	64535.428985	33.394189
799.829340	64636.608507	33.399207
800.550898	64729.534790	33.404224
801.387244	64817.069640	33.409242
801.779321	64933.862676	33.414260
802.582441	65037.054970	33.419277
803.044501	65140.556944	33.424295
803.888215	65254.205130	33.429312
805.082487	65361.007059	33.434330
805.694324	65473.910910	33.439348
806.575166	65570.822348	33.444365
807.021964	65680.360046	33.449383
808.323548	65787.860767	33.454400
809.266248	65906.837728	33.459418
809.572928	66013.302842	33.464436
810.167995	66117.268156	33.469453
810.936946	66230.086961	33.474471
812.075360	66339.577143	33.479488
812.934449	66456.712532	33.484506
813.590231	66581.916894	33.489524
814.385777	66681.970467	33.494541
815.033727	66799.224828	33.499559
815.803568	66919.209657	33.504576
816.606524	67046.112002	33.509594
816.930639	67174.959110	33.514612
818.755308	67264.313470	33.519629
819.275396	67389.513471	33.524647
820.609996	67498.800333	33.529664
821.474957	67614.310205	33.534682
822.104938	67735.492364	33.539700
822.877424	67850.405579	33.544717
823.159362	67960.026720	33.549735
823.853166	68071.831068	33.554752
825.028453	68179.333360	33.559770
825.305599	68311.735569	33.564788
826.450295	68440.018720	33.569805
827.119631	68573.407290	33.574823
827.639896	68694.069382	33.579840
828.540345	68816.003384	33.584858
828.760112	68938.284415	33.589876
830.212517	69051.037166	33.594893
831.017736	69183.269134	33.599911
831.838409	69306.806061	33.604928
832.979121	69424.569047	33.609946
833.540178	69544.710822	33.614964
834.953645	69639.605820	33.619981
835.668632	69755.063681	33.624999
836.426654	69870.571967	33.630016
837.175026	69972.242280	33.635034
838.478368	70085.309680	33.640052
839.730094	70189.439621	33.645069
840.091187	70291.776068	33.650087
841.160818	70397.384996	33.655104
841.731482	70510.215247	33.660122
842.294859	70636.489581	33.665140
843.564508	70740.859531	33.670157
844.048472	70863.038477	33.675175
844.883234	70985.330916	33.680192
845.537333	71103.714693	33.685210
846.253245	71223.928906	33.690228
846.976379	71333.045712	33.695245
848.015069	71470.735415	33.700263
848.547613	71596.103672	33.705280
849.421847	71723.724185	33.710298
850.246530	71853.339113	33.715316
851.419922	71976.820647	33.720333
852.140817	72119.277780	33.725351
852.905766	72258.010491	33.730368
853.903740	72373.005807	33.735386
854.860302	72509.330933	33.740404
855.772624	72627.124029	33.745421
856.951327	72759.259589	33.750439
857.428922	72890.841441	33.755456
858.682735	73010.761845	33.760474
859.251908	73142.753787	33.765492
860.040293	73260.589780	33.770509
860.698900	73403.919378	33.775527
861.602646	73536.041860	33.780544
862.659833	73672.737143	33.785562
863.134981	73812.375079	33.790580
864.066307	73944.002246	33.795597
864.901320	74093.441344	33.800615
865.750853	74229.206879	33.805632
867.009334	74363.274171	33.810650
867.613256	74500.574398	33.815668
868.676998	74636.041500	33.820685
869.274782	74774.172907	33.825703
870.014390	74912.092051	33.830720
870.851918	75056.655176	33.835738
872.150450	75208.808002	33.840756
872.964009	75346.515308	33.845773
873.837656	75486.768547	33.850791
874.709643	75620.584856	33.855808
875.775561	75747.874904	33.860826
876.373648	75889.434759	33.865844
877.151390	76022.579734	33.870861
878.384806	76167.578133	33.875879
879.242338	76316.940193	33.880896
880.204597	76447.287161	33.885914
881.232074	76577.529264	33.890932
882.660012	76694.683714	33.895949
883.664037	76829.611368	33.900967
884.249186	76948.272444	33.905984
885.501189	77076.235176	33.911002
886.193364	77202.001540	33.916020
887.191406	77331.633140	33.921037
888.026238	77446.998421	33.926055
888.646526	77578.996070	33.931072
889.711185	77687.228200	33.936090
890.651242	77809.402520	33.941108
891.359276	77924.297885	33.946125
892.018427	78043.351089	33.951143
892.736751	78158.663416	33.956160
894.067860	78273.426084	33.961178
894.648826	78401.210004	33.966196
895.489108	78526.940460	33.971213
896.328010	78641.489022	33.976231
897.476004	78765.127000	33.981248
898.547174	78877.987560	33.986266
898.971236	79005.149359	33.991284
900.197867	79121.824903	33.996301
900.813293	79242.713422	34.001319
901.288366	79386.991566	34.006336
902.249046	79513.548977	34.011354
902.960357	79659.244708	34.016372
903.922862	79791.053485	34.021389
905.142896	79934.105197	34.026407
906.225902	80069.596132	34.031424
908.008906	80172.161590	34.036442
909.090110	80287.051789	34.041460
910.087286	80412.950394	34.046477
910.579120	80532.202636	34.051495
911.277182	80668.753876	34.056512
912.315210	80783.818212	34.061530
912.961736	80919.266151	34.066548
913.493227	81059.889432	34.071565
914.102155	81194.231886	34.076583
914.538143	81347.239763	34.081600
915.275229	81492.057483	34.086618
915.957817	81649.049978	34.091636
916.663009	81796.601408	34.096653
917.613390	81972.839966	34.101671
918.331234	82145.556684	34.106688
919.591198	82293.095657	34.111706
920.494817	82464.050756	34.116724
921.979936	82611.459727	34.121741
922.729476	82769.309281	34.126759
923.338888	82938.823517	34.131776
924.377143	83081.836597	34.136794
925.189443	83258.228108	34.141812
926.314945	83426.686484	34.146829
927.138034	83579.386073	34.151847
927.884693	83756.045320	34.156864
929.127778	83904.160565	34.161882
930.071959	84068.478043	34.166900
931.098946	84234.238164	34.171917
932.342299	84395.750149	34.176935
933.183612	84558.816443	34.181952
934.946768	84702.017304	34.186970
935.795092	84844.402095	34.191988
936.801182	84989.558206	34.197005
938.281269	85127.234451	34.202023
939.286613	85289.228557	34.207040
940.135088	85413.180013	34.212058
941.067687	85558.668185	34.217076
941.772653	85698.272695	34.222093
943.117811	85841.378810	34.227111
943.836739	85996.332438	34.232128
944.923993	86127.739668	34.237146
945.913212	86256.303914	34.242164
946.798411	86395.408315	34.247181
948.245108	86523.809926	34.252199
949.008584	86653.875252	34.257216
950.154388	86780.170329	34.262234
951.161911	86914.341254	34.267252
952.043129	87038.719915	34.272269
953.241969	87156.390278	34.277287
953.756740	87296.181308	34.282304
954.904248	87405.224325	34.287322
955.835154	87521.251305	34.292340
956.277676	87639.605800	34.297357
957.366323	87763.599722	34.302375
957.778319	87902.285013	34.307392
958.695120	88035.869889	34.312410
959.318935	88167.162627	34.317428
959.692181	88312.393314	34.322445
960.668448	88452.089721	34.327463
960.919025	88627.298609	34.332480
962.255562	88777.966971	34.337498
962.795191	88937.285315	34.342516
963.743265	89106.605163	34.347533
964.648331	89276.755972	34.352551
965.761250	89440.577223	34.357568
966.838088	89608.018937	34.362586
967.677064	89767.255471	34.367604
968.578096	89947.878591	34.372621
970.115772	90096.573042	34.377639
971.266004	90260.583641	34.382656
972.213011	90422.483608	34.387674
973.486529	90598.841809	34.392692
974.455661	90753.810763	34.397709
975.635324	90909.296544	34.402727
976.440310	91080.255182	34.407744
977.112334	91239.788589	34.412762
978.064852	91395.156815	34.417780
978.943596	91570.593768	34.422797
980.090355	91731.488673	34.427815
980.584780	91916.029000	34.432832
981.810104	92078.603037	34.437850
982.995653	92249.912217	34.442868
983.877933	92420.038552	34.447885
985.156479	92591.657580	34.452903
985.934259	92764.063022	34.457920
987.149005	92939.049413	34.462938
988.116323	93102.350151	34.467956
988.786377	93287.846641	34.472973
989.834148	93465.655544	34.477991
990.772858	93642.395132	34.483008
991.812263	93818.334552	34.488026
992.413699	93998.809711	34.493044
993.761667	94183.821355	34.498061
995.059664	94352.354576	34.503079
996.030101	94530.703037	34.508096
996.751369	94697.416038	34.513114
998.170947	94875.325750	34.518132
999.239347	95052.079457	34.523149
1000.512506	95216.217349	34.528167
1001.255211	95398.673345	34.533184
1001.830983	95578.233930	34.538202
1003.081234	95749.259563	34.543220
1004.305984	95926.917896	34.548237
1005.333143	96094.665945	34.553255
1006.258457	96279.851803	34.558272
1007.657608	96445.945693	34.563290
1008.529465	96614.488836	34.568308
1009.621308	96784.819852	34.573325
1010.923655	96946.337490	34.578343
1011.919485	97109.590593	34.583360
1012.842127	97281.440530	34.588378
1014.107666	97444.493052	34.593396
1015.055633	97620.740634	34.598413
1016.087954	97780.143334	34.603431
1016.788274	97944.172353	34.608448
1017.991147	98109.201970	34.613466
1019.078211	98278.398209	34.618484
1019.578333	98447.971034	34.623501
1019.992226	98603.138402	34.628519
1020.981680	98771.986923	34.633536
1021.739613	98936.823241	34.638554
1023.037816	99115.511445	34.643572
1023.694060	99293.857427	34.648589
1024.941255	99456.989402	34.653607
1025.408518	99643.079845	34.658624
1026.244751	99833.263742	34.663642
1027.275474	100015.066588	34.668660
1027.795689	100214.130709	34.673677
1029.115588	100411.589263	34.678695
1030.219275	100613.212853	34.683712
1031.674336	100786.853853	34.688730
1032.844625	100969.419219	34.693748
1033.768571	101161.118053	34.698765
1035.554347	101332.365666	34.703783
1036.695882	101521.074633	34.708800
1037.875418	101694.013896	34.713818
1039.097923	101880.166985	34.718836
1040.232388	102051.286360	34.723853
1040.792269	102235.329125	34.728871
1042.231463	102412.991582	34.733888
1043.322294	102594.214087	34.738906
1044.603547	102776.457464	34.743924
1045.449359	102956.146422	34.748941
1046.555368	103126.099984	34.753959
1047.550880	103298.700543	34.758976
1048.327698	103476.941907	34.763994
1049.716748	103665.353503	34.769012
1050.320955	103860.126518	34.774029
1051.295141	104053.389926	34.779047
1052.248731	104230.467561	34.784064
1053.184748	104415.603506	34.789082
1054.615763	104614.652698	34.794100
1055.540284	104810.184112	34.799117
1056.476153	104997.179497	34.804135
1057.551087	105198.489157	34.809152
1058.699614	105393.848654	34.814170
1059.769183	105585.537300	34.819188
1060.900355	105786.398943	34.824205
1061.771510	105972.044207	34.829223
1062.632852	106176.410814	34.834240
1063.600092	106374.885061	34.839258
1064.910500	106563.678840	34.844276
1066.435512	106762.063921	34.849293
1068.025080	106948.028070	34.854311
1069.273104	107133.543307	34.859328
1070.562768	107318.128408	34.864346
1072.084240	107488.491361	34.869364
1073.021006	107659.078590	34.874381
1074.097704	107828.757229	34.879399
1075.246754	108013.433706	34.884416
1076.112074	108185.631969	34.889434
1077.337846	108368.449055	34.894452
1077.978671	108546.373624	34.899469
1079.058728	108731.041126	34.904487
1079.880371	108920.920291	34.909504
1080.336698	109104.832051	34.914522
1081.615804	109298.995507	34.919540
1082.536448	109497.310749	34.924557
1083.690103	109689.851123	34.929575
1084.566341	109873.458156	34.934592
1086.027774	110066.773732	34.939610
1087.270078	110249.980899	34.944628
1088.532364	110442.331376	34.949645
1089.209949	110640.087139	34.954663
1090.192713	110835.982595	34.959680
1090.913722	111016.975631	34.964698
1091.877973	111197.207693	34.969716
1092.821481	111383.891955	34.974733
1093.630089	111584.837749	34.979751
1095.395143	111775.277912	34.984768
1096.301613	111970.218737	34.989786
1097.488144	112152.523208	34.994804
1097.793679	112352.911652	34.999821
1098.879028	112536.679489	35.004839
1100.993199	112725.928542	35.009856
1102.240907	112911.876280	35.014874
1103.714612	113093.594876	35.019892
1104.840290	113297.224481	35.024909
1105.994498	113476.705431	35.029927
1107.143921	113661.204945	35.034944
1108.132971	113842.641102	35.039962
1110.036650	114028.842786	35.044980
1110.824035	114209.871245	35.049997
1112.416421	114373.868168	35.055015
1114.041213	114537.011914	35.060032
1114.822296	114725.379891	35.065050
1115.954211	114893.256499	35.070068
1116.851991	115072.726753	35.075085
1117.967978	115258.192550	35.080103
1118.634539	115433.307169	35.085120
1119.774820	115616.110833	35.090138
1120.305928	115806.136329	35.095156
1121.240473	116003.964123	35.100173
1122.768556	116186.492104	35.105191
1124.288763	116377.371726	35.110208
1125.203067	116576.587853	35.115226
1126.463618	116765.181770	35.120244
1127.354639	116952.431611	35.125261
1128.110425	117151.525918	35.130279
1129.161615	117354.551197	35.135296
1130.155921	117566.228233	35.140314
1131.551613	117760.824698	35.145332
1132.126117	117981.468500	35.150349
1133.038938	118191.503844	35.155367
1134.632883	118410.221508	35.160384
1135.332383	118609.259269	35.165402
1136.611383	118821.468784	35.170420
1137.845540	119050.526525	35.175437
1138.764363	119264.826073	35.180455
1140.151175	119479.734184	35.185472
1141.107596	119709.514569	35.190490
1142.044846	119929.416556	35.195508
1143.336448	120157.878072	35.200525
1144.095981	120377.711431	35.205543
1145.355669	120607.765660	35.210560
1146.480185	120843.305400	35.215578
1147.698832	121066.831588	35.220596
1149.037335	121290.010242	35.225613
1149.660078	121525.980457	35.230631
1151.169665	121749.565215	35.235648
1151.927424	122000.038847	35.240666
1153.438461	122226.110692	35.245684
1154.785741	122449.372756	35.250701
1155.993332	122675.979688	35.255719
1157.087901	122907.828004	35.260736
1158.026941	123145.697856	35.265754
1159.530418	123363.770709	35.270772
1160.912436	123596.666802	35.275789
1162.068627	123839.854208	35.280807
1163.524739	124046.901980	35.285824
1165.193110	124264.105143	35.290842
1166.227267	124476.053914	35.295860
1167.307237	124692.001310	35.300877
1168.027827	124896.046136	35.305895
1169.358294	125097.393663	35.310912
1170.569196	125303.147244	35.315930
1172.808698	125472.321777	35.320948
1174.995150	125643.229611	35.325965
1176.090604	125827.321552	35.330983
1177.524115	125990.130518	35.336000
1178.373674	126190.373416	35.341018
1179.475071	126371.590762	35.346036
1180.366300	126551.829977	35.351053
1181.036407	126739.989937	35.356071
1182.524370	126917.496642	35.361088
1182.910021	127122.030022	35.366106
1184.017246	127328.929796	35.371124
1185.406665	127517.951730	35.376141
1186.399760	127708.193616	35.381159
1187.402424	127909.753342	35.386176
1188.785518	128131.327985	35.391194
1190.067540	128335.518710	35.396212
1191.456758	128532.785406	35.401229
1192.717289	128725.334254	35.406247
1194.064306	128918.617841	35.411264
1195.304586	129141.883723	35.416282
1196.739220	129334.610425	35.421300
1197.601989	129535.215212	35.426317
1198.152700	129739.548598	35.431335
1199.606633	129955.091244	35.436352
1200.394376	130184.764261	35.441370
1201.951381	130398.378981	35.446388
1203.231855	130603.890457	35.451405
1204.200076	130820.229073	35.456423
1205.792280	131025.856642	35.461440
1207.165417	131228.479536	35.466458
1208.317810	131439.607632	35.471476
1209.494512	131668.580833	35.476493
1210.529005	131880.276401	35.481511
1211.530660	132099.977426	35.486528
1212.851462	132314.087797	35.491546
1213.751292	132540.932700	35.496564
1215.105001	132764.611267	35.501581
1215.866065	133004.868626	35.506599
1217.281921	133225.713316	35.511616
1218.477285	133454.341353	35.516634
1219.478039	133681.507290	35.521652
1220.745530	133912.459205	35.526669
1222.031823	134148.607210	35.531687
1223.079291	134395.292930	35.536704
1224.316851	134651.444312	35.541722
1225.029581	134890.227836	35.546740
1226.200789	135129.824850	35.551757
1226.852360	135393.152748	35.556775
1228.197190	135646.910927	35.561792
1229.550231	135898.666665	35.566810
1230.825400	136154.519413	35.571828
1232.882243	136414.783787	35.576845
1233.692263	136666.799873	35.581863
1234.768838	136909.442890	35.586880
1235.865761	137167.285356	35.591898
1237.423870	137420.692416	35.596916
1239.311193	137658.642970	35.601933
1241.143633	137907.634472	35.606951
1242.496839	138142.253497	35.611968
1243.701675	138368.721004	35.616986
1245.097050	138598.328256	35.622004
1247.069433	138818.345486	35.627021
1248.308417	139038.028782	35.632039
1249.647926	139268.486654	35.637056
1250.565206	139493.234190	35.642074
1251.432369	139708.380775	35.647092
1252.701615	139908.247410	35.652109
1253.681372	140118.458523	35.657127
1255.134688	140334.425248	35.662144
1255.746823	140565.050070	35.667162
1257.053159	140774.120917	35.672180
1258.236522	141002.524273	35.677197
1258.809036	141241.008845	35.682215
1260.355684	141465.094980	35.687232
1261.334056	141708.435546	35.692250
1262.443115	141945.885481	35.697268
1263.530499	142189.731340	35.702285
1264.368831	142445.640733	35.707303
1265.702547	142699.542872	35.712320
1267.320387	142963.569543	35.717338
1268.389670	143213.651619	35.722356
1269.706789	143471.670586	35.727373
1270.885208	143730.982410	35.732391
1272.397408	143979.957079	35.737408
1273.522923	144238.875625	35.742426
1274.643510	144490.442025	35.747444
1276.490136	144757.348412	35.752461
1277.492564	145011.968781	35.757479
1279.284351	145277.100135	35.762496
1280.699468	145531.453234	35.767514
1281.993489	145785.752058	35.772532
1283.591292	146042.488109	35.777549
1284.873820	146295.397523	35.782567
1286.656270	146531.270992	35.787584
1288.210175	146785.952548	35.792602
1289.189588	147039.006022	35.797620
1290.622673	147274.143096	35.802637
1291.709606	147531.278509	35.807655
1292.827344	147784.656801	35.812672
1294.096003	148030.478809	35.817690
1295.313737	148293.812266	35.822708
1296.731717	148546.233209	35.827725
1297.882122	148805.434387	35.832743
1299.113665	149066.982945	35.837760
1300.561464	149320.076487	35.842778
1301.503754	149590.858669	35.847796
1302.881318	149850.397542	35.852813
1304.217222	150120.065985	35.857831
1305.691239	150379.148761	35.862848
1307.490060	150645.142691	35.867866
1308.454832	150910.007882	35.872884
1310.020327	151147.088499	35.877901
1311.096949	151420.322414	35.882919
1312.327864	151674.419090	35.887936
1313.526415	151944.364408	35.892954
1314.528478	152219.924837	35.897972
1316.420901	152479.574621	35.902989
1317.689832	152744.719662	35.908007
1319.339134	153005.605453	35.913024
1320.450248	153264.869545	35.918042
1321.621753	153539.967682	35.923060
1323.219296	153790.149465	35.928077
1324.226936	154071.328757	35.933095
1325.495117	154322.798742	35.938112
1326.948101	154587.456902	35.943130
1328.728434	154831.653693	35.948148
1330.559395	155087.488002	35.953165
1331.925014	155345.582549	35.958183
1333.824399	155587.405138	35.963200
1335.304699	155831.657755	35.968218
1336.232755	156079.377200	35.973236
1337.423894	156331.025155	35.978253
1338.868841	156565.368634	35.983271
1340.015338	156803.669755	35.988288
1341.360411	157026.451052	35.993306
1342.483146	157255.942697	35.998324
1343.770659	157491.928689	36.003341
1344.828528	157731.087260	36.008359
1346.346847	157964.196461	36.013376
1347.471957	158197.130900	36.018394
1348.674865	158430.370998	36.023412
1350.019562	158666.519430	36.028429
1351.235228	158933.009345	36.033447
1351.974047	159182.580790	36.038464
1353.245559	159445.830012	36.043482
1354.066166	159713.658876	36.048500
1355.676015	159972.859618	36.053517
1357.571387	160244.256981	36.058535
1358.613519	160500.522808	36.063552
1359.810385	160767.852500	36.068570
1361.063629	161044.689396	36.073588
1362.279570	161333.535687	36.078605
1363.262809	161621.242563	36.083623
1364.780786	161911.489319	36.088640
1366.185511	162184.972291	36.093658
1367.356906	162460.829942	36.098676
1368.731195	162767.548474	36.103693
1370.131203	163070.864904	36.108711
1371.488044	163367.796375	36.113728
1373.008204	163644.441616	36.118746
1374.453246	163948.112185	36.123764
1376.166706	164235.221741	36.128781
1377.053272	164548.161716	36.133799
1378.422418	164851.026593	36.138816
1379.518045	165167.222672	36.143834
1380.843187	165469.236431	36.148852
1382.407399	165776.782792	36.153869
1384.187362	166083.077704	36.158887
1385.696277	166384.915295	36.163904
1387.808885	166672.330555	36.168922
1389.781406	166974.083040	36.173940
1391.436111	167233.980907	36.178957
1392.757132	167523.232633	36.183975
1394.336873	167798.943141	36.188992
1396.020475	168078.850798	36.194010
1397.428738	168369.514788	36.199028
1398.501791	168643.994583	36.204045
1399.829130	168923.776044	36.209063
1400.981181	169210.922296	36.214080
1402.632233	169487.062939	36.219098
1403.863231	169772.918189	36.224116
1405.207221	170074.173755	36.229133
1406.312275	170356.919305	36.234151
1407.781215	170663.348010	36.239168
1409.431016	170945.436311	36.244186
1410.225699	171231.575796	36.249204
1412.092346	171526.397370	36.254221
1413.187013	171826.893552	36.259239
1414.836367	172112.643686	36.264256
1416.389699	172406.672401	36.269274
1417.386451	172711.834909	36.274292
1419.365078	172991.229315	36.279309
1421.390088	173280.325510	36.284327
1422.610563	173550.115227	36.289344
1424.568272	173829.124698	36.294362
1425.489616	174115.159519	36.299380
1427.369382	174383.982276	36.304397
1428.983318	174663.929030	36.309415
1430.206574	174951.518041	36.314432
1431.939543	175214.659063	36.319450
1433.172384	175475.003327	36.324468
1434.676535	175733.806742	36.329485
1435.975175	175995.627758	36.334503
1436.946448	176248.113108	36.339520
1438.219329	176514.078340	36.344538
1439.115956	176790.348616	36.349556
1440.267383	177067.949021	36.354573
1441.697694	177342.903327	36.359591
1442.402705	177643.360954	36.364608
1443.801368	177920.227363	36.369626
1444.991001	178221.154243	36.374644
1446.148514	178527.177446	36.379661
1447.440059	178845.668699	36.384679
1448.587787	179170.163377	36.389696
1449.870577	179475.867109	36.394714
1451.069514	179807.655063	36.399732
1452.763909	180130.593475	36.404749
1454.116792	180462.372993	36.409767
1455.183057	180809.876391	36.414784
1457.013600	181138.941562	36.419802
1458.175722	181487.994831	36.424820
1459.697617	181833.678443	36.429837
1461.382257	182167.622614	36.434855
1462.804034	182513.403412	36.439872
1464.444409	182859.721570	36.444890
1466.151150	183207.554145	36.449908
1467.724262	183546.500916	36.454925
1469.173223	183895.751336	36.459943
1470.708023	184226.001635	36.464960
1472.761874	184581.528432	36.469978
1473.917923	184920.083096	36.474996
1475.832231	185247.129205	36.480013
1478.039767	185576.413631	36.485031
1480.053341	185901.594114	36.490048
1482.173933	186205.739033	36.495066
1483.719662	186523.498762	36.500084
1485.030365	186849.638586	36.505101
1486.648328	187153.871667	36.510119
1487.945987	187477.656360	36.515136
1489.533636	187787.724174	36.520154
1490.962551	188113.496446	36.525172
1492.272502	188431.648655	36.530189
1494.797264	188731.615195	36.535207
1496.285929	189027.082985	36.540224
1497.858778	189343.495935	36.545242
1499.608173	189648.114239	36.550260
1501.056795	189936.637050	36.555277
1502.299757	190240.478854	36.560295
1503.582985	190553.912341	36.565312
1505.049861	190855.714728	36.570330
1506.139498	191175.746370	36.575348
1507.567711	191491.763252	36.580365
1508.946325	191801.684008	36.585383
1510.080890	192115.848508	36.590400
1511.168895	192448.937158	36.595418
1512.907294	192784.522714	36.600436
1514.453248	193118.440807	36.605453
1515.984379	193434.933333	36.610471
1517.211286	193759.132656	36.615488
1519.458921	194083.393763	36.620506
1520.136400	194415.723053	36.625524
1521.565087	194752.766953	36.630541
1523.413935	195096.522505	36.635559
1524.537863	195432.934834	36.640576
1525.948400	195775.141454	36.645594
1527.926614	196095.090325	36.650612
1529.121738	196446.489396	36.655629
1530.876561	196777.688532	36.660647
1532.199848	197115.092492	36.665664
1534.093488	197418.583223	36.670682
1536.231977	197722.999835	36.675700
1537.595026	198034.211037	36.680717
1539.191453	198342.515978	36.685735
1540.216468	198661.771526	36.690752
1541.795084	198966.425939	36.695770
1543.208914	199282.065480	36.700788
1544.450095	199603.168862	36.705805
1545.842832	199923.499704	36.710823
1547.029886	200263.836908	36.715840
1548.252590	200612.105011	36.720858
1549.727363	200953.909020	36.725876
1550.795548	201312.147292	36.730893
1552.384319	201656.462524	36.735911
1553.293858	202018.945798	36.740928
1554.700841	202386.592497	36.745946
1556.352763	202759.964914	36.750964
1557.774262	203137.719551	36.755981
1559.926131	203523.621188	36.760999
1560.985817	203901.934723	36.766016
1562.709471	204269.564250	36.771034
1564.307228	204650.763944	36.776052
1565.693418	205044.468903	36.781069
1567.809256	205426.183879	36.786087
1569.793896	205804.443470	36.791104
1571.340287	206179.323671	36.796122
1573.206993	206561.453756	36.801140
1574.539854	206957.209110	36.806157
1576.404076	207337.223051	36.811175
1577.662994	207717.884732	36.816192
1579.307972	208098.586154	36.821210
1581.595622	208480.275368	36.826228
1583.780334	208849.184285	36.831245
1585.484844	209207.203421	36.836263
1587.177690	209586.380395	36.841280
1588.522097	209958.709085	36.846298
1590.070907	210326.751999	36.851316
1591.482578	210708.570959	36.856333
1592.987740	211080.611577	36.861351
1594.384762	211477.000993	36.866368
1595.790112	211850.267821	36.871386
1597.144987	212236.318892	36.876404
1598.992826	212640.093155	36.881421
1600.821383	213020.126885	36.886439
1602.340283	213405.902194	36.891456
1603.703135	213796.200158	36.896474
1605.519550	214181.066310	36.901492
1606.686352	214596.339739	36.906509
1608.287277	214983.251265	36.911527
1609.678828	215385.767392	36.916544
1611.452182	215776.133251	36.921562
1613.124068	216178.200258	36.926580
1614.307589	216592.718118	36.931597
1616.142882	216996.006168	36.936615
1617.666230	217436.504115	36.941632
1619.310049	217876.755640	36.946650
1620.784906	218282.572183	36.951668
1622.459219	218692.954537	36.956685
1624.505446	219105.944034	36.961703
1626.158744	219515.647528	36.966720
1627.744993	219927.319425	36.971738
1629.040157	220343.104763	36.976756
1630.594524	220755.598018	36.981773
1632.622348	221160.369832	36.986791
1634.110703	221581.284181	36.991808
1635.404657	221991.285416	36.996826
1637.223922	222408.364030	37.001844
1638.699472	222811.506143	37.006861
1640.538645	223202.144216	37.011879
1642.550826	223575.864706	37.016896
1643.913249	223981.595078	37.021914
1645.822850	224362.802492	37.026932
1647.013117	224760.410884	37.031949
1648.500436	225152.358350	37.036967
1650.215553	225549.425664	37.041984
1651.787052	225965.313760	37.047002
1653.852599	226358.414422	37.052020
1655.331630	226760.020481	37.057037
1657.073314	227153.177157	37.062055
1658.595862	227566.310234	37.067072
1660.243975	227971.727736	37.072090
1662.174536	228373.569315	37.077108
1663.582223	228786.750729	37.082125
1665.015512	229201.478653	37.087143
1666.643920	229619.630145	37.092160
1668.717870	230037.633236	37.097178
1670.964892	230428.989289	37.102196
1672.751844	230835.053127	37.107213
1674.112833	231245.684356	37.112231
1675.934021	231671.405114	37.117248
1677.696590	232084.487191	37.122266
1679.083164	232500.807594	37.127284
1680.506660	232916.640465	37.132301
1682.233298	233344.058163	37.137319
1684.007779	233760.800696	37.142336
1685.453730	234196.598657	37.147354
1687.145943	234613.763469	37.152372
1688.153213	235058.323417	37.157389
1689.756417	235504.157937	37.162407
1691.356013	235952.153381	37.167424
1693.219945	236391.012655	37.172442
1695.048215	236836.991388	37.177460
1696.929320	237282.149691	37.182477
1698.830446	237729.896782	37.187495
1700.364830	238177.807093	37.192512
1701.964519	238629.797413	37.197530
1703.991966	239070.947827	37.202548
1705.380151	239530.646555	37.207565
1707.018700	239982.989261	37.212583
1709.224806	240458.406051	37.217600
1710.628567	240904.159591	37.222618
1713.183397	241339.842708	37.227636
1714.907359	241795.274322	37.232653
1716.665998	242237.237932	37.237671
1718.640595	242685.618971	37.242688
1720.073287	243123.878516	37.247706
1721.626033	243576.471441	37.252724
1723.813846	244035.311050	37.257741
1725.085868	244464.429201	37.262759
1727.516762	244909.284286	37.267776
1729.472291	245354.828205	37.272794
1731.555870	245786.659688	37.277812
1733.100394	246227.547918	37.282829
1734.967544	246667.189660	37.287847
1736.855519	247097.150153	37.292864
1738.241841	247524.501307	37.297882
1739.988084	247965.765212	37.302900
1741.508379	248405.314181	37.307917
1743.244877	248846.047380	37.312935
1744.838548	249276.618109	37.317952
1746.144379	249736.501039	37.322970
1748.302989	250181.789517	37.327988
1749.784357	250629.273264	37.333005
1751.736822	251075.282593	37.338023
1753.471287	251512.462662	37.343040
1754.767507	251952.738410	37.348058
1756.635898	252382.631892	37.353076
1758.128721	252811.978016	37.358093
1759.550206	253248.093485	37.363111
1761.137321	253679.888817	37.368128
1763.210420	254128.090945	37.373146
1765.285375	254555.589453	37.378164
1766.823642	254989.146515	37.383181
1768.612077	255431.604486	37.388199
1770.775173	255858.403283	37.393216
1772.056201	256298.938540	37.398234
1773.730788	256736.665504	37.403252
1775.419398	257198.244000	37.408269
1777.054379	257658.739160	37.413287
1779.358140	258108.734176	37.418304
1780.910918	258562.587476	37.423322
1782.672890	258994.864348	37.428340
1784.735489	259454.298623	37.433357
1786.358832	259910.477572	37.438375
1788.479423	260362.357556	37.443392
1790.066247	260832.285731	37.448410
1792.016337	261278.147822	37.453428
1793.581076	261750.569078	37.458445
1795.429576	262208.412755	37.463463
1797.743769	262667.500476	37.468480
1799.758474	263142.260498	37.473498
1801.749231	263581.383519	37.478516
1803.233017	264040.404564	37.483533
1804.787666	264506.552036	37.488551
1806.781499	264969.146587	37.493568
1807.994069	265452.141549	37.498586
1809.865290	265923.392886	37.503604
1811.159796	266403.401544	37.508621
1812.829387	266890.460865	37.513639
1814.695834	267379.468771	37.518656
1816.311717	267871.591374	37.523674
1818.499430	268366.388129	37.528692
1820.456777	268864.397786	37.533709
1821.668075	269362.784024	37.538727
1823.924742	269849.134045	37.543744
1825.528769	270345.574550	37.548762
1828.378979	270847.626145	37.553780
1830.162258	271325.593300	37.558797
1832.295372	271826.542548	37.563815
1834.295402	272314.684597	37.568832
1836.018699	272797.003543	37.573850
1838.076620	273279.418989	37.578868
1840.063781	273761.337311	37.583885
1842.021823	274250.601049	37.588903
1843.870925	274725.986685	37.593920
1845.952117	275218.149763	37.598938
1848.024621	275689.762710	37.603956
1849.946645	276163.635062	37.608973
1851.327936	276641.863356	37.613991
1853.530200	277127.194993	37.619008
1855.303029	277613.053740	37.624026
1856.923194	278083.314241	37.629044
1858.866627	278563.655954	37.634061
1860.310240	279043.367822	37.639079
1862.391114	279537.401931	37.644096
1864.206297	280021.063858	37.649114
1865.856595	280506.504592	37.654132
1867.665397	281006.346330	37.659149
1869.134881	281507.741485	37.664167
1870.837102	281999.926875	37.669184
1872.555151	282512.937816	37.674202
1874.864265	283010.481794	37.679220
1876.470640	283505.244530	37.684237
1878.004731	284014.877706	37.689255
1880.032187	284499.407529	37.694272
1881.371478	284987.402462	37.699290
1882.940419	285468.169495	37.704308
1884.761742	285960.247828	37.709325
1886.663425	286463.894317	37.714343
1888.689911	286962.920993	37.719360
1890.650161	287456.673557	37.724378
1892.325130	287962.460791	37.729396
1894.562313	288462.209753	37.734413
1896.253040	288969.083138	37.739431
1898.180244	289486.837989	37.744448
1899.882420	289999.522528	37.749466
1901.576751	290520.563199	37.754484
1903.383628	291041.862696	37.759501
1904.572228	291575.098654	37.764519
1906.159525	292119.620532	37.769536
1908.015717	292666.686546	37.774554
1909.783257	293217.371598	37.779572
1911.850525	293770.570143	37.784589
1913.599607	294345.560802	37.789607
1914.993314	294916.162396	37.794624
1916.956155	295483.975006	37.799642
1919.338156	296047.245411	37.804660
1921.949721	296622.793779	37.809677
1923.821341	297196.632519	37.814695
1925.788946	297751.454043	37.819712
1927.895341	298319.254036	37.824730
1929.676404	298894.622692	37.829748
1931.632786	299471.407012	37.834765
1933.110161	300056.242243	37.839783
1935.234248	300645.335962	37.844800
1937.160860	301229.836369	37.849818
1938.942551	301815.931925	37.854836
1941.307732	302395.476700	37.859853
1943.042780	302990.817685	37.864871
1945.382987	303578.385105	37.869888
1947.214632	304194.020581	37.874906
1949.215400	304780.087209	37.879924
1951.866930	305362.563363	37.884941
1953.575784	305957.635700	37.889959
1956.118843	306534.991994	37.894976
1958.061756	307104.748366	37.899994
1960.040852	307702.278611	37.905012
1962.199377	308280.220087	37.910029
1964.684828	308865.189182	37.915047
1966.723039	309427.930471	37.920064
1968.481669	310002.192879	37.925082
1970.570607	310591.964187	37.930100
1972.547728	311168.874259	37.935117
1974.337927	311747.791826	37.940135
1976.550729	312307.360747	37.945152
1979.010252	312878.261804	37.950170
1980.989627	313443.854220	37.955188
1983.125036	314002.382502	37.960205
1985.041243	314586.006843	37.965223
1987.863120	315131.132420	37.970240
1990.157817	315668.570464	37.975258
1992.423223	316219.010927	37.980276
1994.468079	316756.126693	37.985293
1996.122966	317302.698268	37.990311
1998.617580	317851.666463	37.995328
2000.445350	318392.106842	38.000346
2002.112863	318928.303535	38.005364
2004.240165	319455.405953	38.010381
2005.830027	320011.006869	38.015399
2007.464959	320570.150712	38.020416
2009.320582	321126.384262	38.025434
2010.850099	321673.475234	38.030452
2012.538099	322202.304556	38.035469
2014.459585	322753.663870	38.040487
2015.995371	323295.281239	38.045504
2017.838942	323843.698810	38.050522
2018.913857	324406.228647	38.055540
2020.970652	324969.835688	38.060557
2022.615230	325544.398015	38.065575
2024.657262	326120.006658	38.070592
2026.903264	326698.978515	38.075610
2028.338220	327301.284535	38.080628
2031.100462	327867.795570	38.085645
2032.883765	328460.156261	38.090663
2035.205355	329043.358577	38.095680
2037.265504	329643.684631	38.100698
2038.930226	330250.416793	38.105716
2041.081419	330845.764830	38.110733
2042.518371	331463.108600	38.115751
2044.886496	332067.522343	38.120768
2047.044661	332680.519701	38.125786
2049.437291	333306.266623	38.130804
2051.735137	333911.256062	38.135821
2054.436312	334513.227576	38.140839
2056.965692	335105.904205	38.145856
2059.378535	335697.705110	38.150874
2061.478558	336303.208437	38.155892
2064.432387	336871.578098	38.160909
2066.442580	337461.953614	38.165927
2068.850770	338048.525371	38.170944
2070.834875	338636.861249	38.175962
2072.498961	339236.056802	38.180980
2074.686390	339805.917157	38.185997
2076.720219	340386.812879	38.191015
2078.979639	340972.005267	38.196032
2081.256039	341559.193312	38.201050
2083.254675	342144.821197	38.206068
2085.716296	342723.131922	38.211085
2087.487636	343318.784007	38.216103
2089.635243	343910.178855	38.221120
2091.416028	344497.972126	38.226138
2093.587503	345101.100046	38.231156
2095.805958	345673.806677	38.236173
2098.047651	346276.451361	38.241191
2099.536470	346859.771487	38.246208
2101.839725	347464.801954	38.251226
2103.566194	348077.635029	38.256244
2105.704305	348672.931380	38.261261
2107.459017	349291.098691	38.266279
2109.401678	349912.931892	38.271296
2111.675587	350526.733279	38.276314
2113.319732	351166.515347	38.281332
2115.125231	351791.415988	38.286349
2116.969187	352422.341217	38.291367
2118.882224	353061.468047	38.296384
2120.776027	353696.807701	38.301402
2122.596009	354367.168840	38.306420
2125.175153	355011.816025	38.311437
2127.318490	355678.627038	38.316455
2129.652298	356316.596057	38.321472
2132.082315	356972.123949	38.326490
2134.032810	357619.626473	38.331508
2136.192622	358264.318755	38.336525
2138.659334	358910.954896	38.341543
2140.527582	359566.915246	38.346560
2143.324141	360212.740730	38.351578
2145.447170	360857.880527	38.356596
2148.162641	361480.686971	38.361613
2150.155274	362125.269845	38.366631
2152.611776	362756.116435	38.371648
2155.159408	363358.903874	38.376666
2157.453964	363963.702697	38.381684
2159.487166	364555.622249	38.386701
2161.348274	365156.897031	38.391719
2163.448346	365754.038735	38.396736
2165.755692	366354.231951	38.401754
2167.083737	366966.703132	38.406772
2169.332388	367570.159416	38.411789
2170.881194	368196.196741	38.416807
2172.667760	368834.132157	38.421824
2174.562482	369463.160715	38.426842
2176.126904	370103.546268	38.431860
2178.377877	370744.492403	38.436877
2180.602668	371408.995681	38.441895
2182.646208	372064.563156	38.446912
2185.041810	372734.797227	38.451930
2186.684236	373412.219502	38.456948
2188.597793	374093.363397	38.461965
2190.820602	374767.874432	38.466983
2192.599320	375470.927449	38.472000
2194.823438	376164.331740	38.477018
2196.974371	376874.548752	38.482036
2199.191245	377575.534583	38.487053
2201.491062	378289.527594	38.492071
2203.756713	379004.449753	38.497088
2205.894940	379725.920607	38.502106
2208.329971	380442.661296	38.507124
2211.091873	381153.906333	38.512141
2213.418264	381865.588513	38.517159
2215.311932	382602.455445	38.522176
2218.349026	383304.557017	38.527194
2221.154428	383995.905726	38.532212
2223.866801	384694.456090	38.537229
2226.512947	385402.104738	38.542247
2228.633586	386092.710666	38.547264
2231.249823	386786.845663	38.552282
2233.167540	387489.498031	38.557300
2235.224201	388183.213359	38.562317
2237.636296	388886.032298	38.567335
2239.381379	389591.328621	38.572352
2242.221501	390277.009923	38.577370
2244.332397	390996.005106	38.582388
2246.243052	391692.075356	38.587405
2249.060329	392402.302611	38.592423
2251.007516	393115.546659	38.597440
2253.333215	393802.654136	38.602458
2255.613001	394510.208882	38.607476
2257.754009	395214.703036	38.612493
2260.240603	395931.239125	38.617511
2262.301909	396646.383514	38.622528
2264.749970	397337.470775	38.627546
2267.324176	398043.879723	38.632564
2269.593269	398736.940634	38.637581
2271.971138	399455.335590	38.642599
2273.721631	400182.914229	38.647616
2276.355899	400890.790431	38.652634
2278.105593	401605.713274	38.657652
2280.304412	402304.377045	38.662669
2282.571100	403024.551446	38.667687
2284.356556	403759.838465	38.672704
2286.587071	404486.265861	38.677722
2288.612488	405235.943183	38.682740
2290.617426	405983.931567	38.687757
2292.526422	406721.325033	38.692775
2294.127908	407469.314646	38.697792
2296.781494	408225.876461	38.702810
2299.256976	408976.493187	38.707828
2301.578006	409728.254763	38.712845
2304.234840	410454.455100	38.717863
2306.228779	411174.614790	38.722880
2308.975857	411889.741993	38.727898
2311.766629	412589.846901	38.732916
2314.385259	413316.280059	38.737933
2316.965209	414020.510889	38.742951
2319.374288	414728.221177	38.747968
2321.407758	415435.746378	38.752986
2323.529198	416154.534059	38.758004
2325.651717	416884.496214	38.763021
2327.619906	417598.330452	38.768039
2329.764565	418339.416727	38.773056
2332.058440	419070.428394	38.778074
2334.379568	419805.339873	38.783092
2336.395809	420565.578350	38.788109
2338.334081	421323.223948	38.793127
2340.770826	422089.171385	38.798144
2342.851272	422843.683756	38.803162
2345.258334	423623.085173	38.808180
2347.554833	424388.655954	38.813197
2349.953213	425156.642118	38.818215
2351.949197	425956.115368	38.823232
2354.500529	426744.078292	38.828250
2356.589425	427549.762638	38.833268
2359.006340	428344.024857	38.838285
2361.230780	429140.267180	38.843303
2363.628510	429944.352365	38.848320
2366.332248	430754.333837	38.853338
2368.340407	431561.769955	38.858356
2370.803236	432388.795525	38.863373
2373.140385	433208.877786	38.868391
2376.048494	434013.145463	38.873408
2378.974998	434829.530379	38.878426
2381.661535	435654.024525	38.883444
2384.336305	436457.587940	38.888461
2386.777592	437266.273509	38.893479
2388.916893	438076.852839	38.898496
2391.578097	438887.469094	38.903514
2394.235222	439698.613697	38.908532
2396.284300	440525.668484	38.913549
2398.767491	441326.055046	38.918567
2400.590701	442162.852895	38.923584
2403.626833	442949.579716	38.928602
2405.846733	443776.839992	38.933620
2408.350335	444590.361855	38.938637
2411.276243	445400.748364	38.943655
2413.505279	446231.658514	38.948672
2416.012863	447055.206171	38.953690
2418.454716	447863.152483	38.958708
2421.300406	448677.325107	38.963725
2424.535309	449469.348298	38.968743
2427.130322	450269.641850	38.973760
2429.556518	451068.264012	38.978778
2432.184454	451860.753487	38.983796
2433.956816	452668.729320	38.988813
2436.341212	453466.660702	38.993831
2439.080867	454268.953417	38.998848
2441.397432	455069.059912	39.003866
2443.406353	455875.507284	39.008884
2446.021991	456685.767308	39.013901
2448.387493	457495.379327	39.018919
2450.563783	458319.956919	39.023936
2452.446649	459134.387002	39.028954
2454.554825	459951.831332	39.033972
2456.881074	460785.940690	39.038989
2459.684893	461618.369609	39.044007
2461.658141	462465.510349	39.049024
2463.758414	463292.829355	39.054042
2466.373238	464110.778935	39.059060
2468.624326	464921.981622	39.064077
2470.831080	465723.656116	39.069095
2473.217486	466553.217596	39.074112
2475.438272	467371.652618	39.079130
2477.734692	468183.673143	39.084148
2479.943173	469030.492692	39.089165
2482.578468	469856.233758	39.094183
2484.159858	470711.875565	39.099200
2486.649756	471555.455310	39.104218
2488.930183	472431.621498	39.109236
2491.225060	473321.032604	39.114253
2494.023863	474181.925988	39.119271
2496.613823	475067.265589	39.124288
2499.297220	475945.273674	39.129306
2501.682056	476830.008108	39.134324
2503.801769	477750.556902	39.139341
2506.348013	478658.311908	39.144359
2508.974610	479574.847665	39.149376
2511.118835	480473.084278	39.154394
2513.959857	481377.525132	39.159412
2516.478111	482287.428203	39.164429
2519.428755	483201.759051	39.169447
2521.505348	484131.941820	39.174464
2524.138298	485069.810934	39.179482
2526.787251	485996.773267	39.184500
2529.360046	486924.103880	39.189517
2532.299684	487861.220344	39.194535
2535.474070	488766.597073	39.199552
2538.045154	489712.712050	39.204570
2541.125366	490608.923367	39.209588
2543.850052	491535.582413	39.214605
2546.804491	492455.542653	39.219623
2549.214944	493380.540000	39.224640
2551.996227	494288.571435	39.229658
2554.714770	495196.918476	39.234676
2556.770402	496119.202927	39.239693
2559.536757	497033.449109	39.244711
2562.166938	497957.153853	39.249728
2564.707008	498886.574437	39.254746
2567.426688	499794.019564	39.259764
2570.259607	500703.414779	39.264781
2573.267626	501617.826381	39.269799
2575.780447	502536.153281	39.274816
2578.175880	503456.466177	39.279834
2580.805474	504377.445726	39.284852
2583.210495	505312.329878	39.289869
2585.911848	506227.444654	39.294887
2588.065423	507142.043755	39.299904
2590.914156	508064.645383	39.304922
2593.338982	508984.945024	39.309940
2595.592844	509929.672766	39.314957
2598.383063	510861.451352	39.319975
2601.021150	511797.788240	39.324992
2603.508959	512731.171259	39.330010
2606.835580	513657.858884	39.335028
2609.665903	514577.366506	39.340045
2612.203041	515508.410355	39.345063
2614.764898	516435.967998	39.350080
2617.328835	517364.175850	39.355098
2619.618437	518297.160788	39.360116
2622.117386	519236.958291	39.365133
2624.715740	520167.361222	39.370151
2627.614479	521102.394359	39.375168
2630.145645	522025.894527	39.380186
2633.357067	522955.372639	39.385204
2636.434579	523879.325589	39.390221
2639.532036	524781.661023	39.395239
2642.307108	525656.546169	39.400256
2644.609833	526538.559690	39.405274
2646.876188	527411.512950	39.410292
2649.327860	528300.801371	39.415309
2651.543802	529180.860821	39.420327
2654.156270	530060.299360	39.425344
2656.557860	530951.904864	39.430362
2658.868523	531852.231691	39.435380
2661.228353	532758.385448	39.440397
2663.786077	533675.927997	39.445415
2665.754803	534598.594023	39.450432
2668.055961	535541.581980	39.455450
2670.260263	536480.900966	39.460468
2672.620129	537438.150139	39.465485
2675.557174	538389.453514	39.470503
2678.574577	539351.801267	39.475520
2680.909299	540308.712408	39.480538
2683.613343	541284.818571	39.485556
2686.072685	542280.921090	39.490573
2688.894611	543271.662010	39.495591
2691.704626	544261.932916	39.500608
2694.118787	545250.187380	39.505626
2697.488995	546237.661301	39.510644
2700.384123	547241.689520	39.515661
2703.006307	548230.302189	39.520679
2705.888639	549257.469923	39.525696
2708.327028	550274.829746	39.530714
2711.387032	551273.510066	39.535732
2714.158725	552280.359622	39.540749
2716.506044	553292.382621	39.545767
2719.059073	554329.479436	39.550784
2722.218365	555352.776097	39.555802
2725.483807	556367.031833	39.560820
2728.055045	557398.512405	39.565837
2730.714135	558411.256356	39.570855
2733.749698	559439.689079	39.575872
2735.831777	560483.774640	39.580890
2738.852862	561508.432182	39.585908
2741.287522	562548.478698	39.590925
2744.776402	563597.612192	39.595943
2747.686455	564625.360690	39.600960
2750.148105	565665.256160	39.605978
2752.457442	566703.838268	39.610996
2755.237702	567768.069904	39.616013
2757.445995	568812.726217	39.621031
2760.464132	569873.079760	39.626048
2763.075573	570938.683980	39.631066
2766.242436	572002.852958	39.636084
2768.719551	573083.209125	39.641101
2771.212623	574154.687640	39.646119
2774.088968	575234.292815	39.651136
2776.669988	576327.653933	39.656154
2779.460324	577400.614148	39.661172
2782.583817	578491.288748	39.666189
2785.159652	579570.921344	39.671207
2788.172275	580656.357603	39.676224
2790.284135	581753.333564	39.681242
2793.611719	582852.770139	39.686260
2796.485613	583946.115019	39.691277
2799.403680	585035.794708	39.696295
2802.042254	586123.918955	39.701312
2804.970059	587222.527123	39.706330
2808.146882	588315.480155	39.711348
2810.755144	589426.173048	39.716365
2813.920459	590510.708057	39.721383
2817.130005	591577.746640	39.726400
2820.157096	592656.847547	39.731418
2823.926012	593692.634396	39.736436
2827.293098	594714.267429	39.741453
2830.175606	595730.130499	39.746471
2833.205046	596734.860611	39.751488
2835.693833	597752.968558	39.756506
2838.528073	598749.593690	39.761524
2840.879510	599756.630740	39.766541
2843.338225	600775.181397	39.771559
2846.203086	601780.756586	39.776576
2848.531588	602814.672627	39.781594
2851.396155	603827.029494	39.786612
2854.197412	604855.377388	39.791629
2856.794935	605894.729161	39.796647
2859.522475	606934.665674	39.801664
2862.320399	607987.457976	39.806682
2865.291264	609031.716872	39.811700
2867.980253	610077.527055	39.816717
2871.518753	611129.104305	39.821735
2874.736679	612183.687760	39.826752
2877.496118	613244.100355	39.831770
2880.614898	614297.950529	39.836788
2883.065949	615371.616860	39.841805
2885.741347	616453.994105	39.846823
2888.997060	617523.168474	39.851840
2891.863261	618605.903387	39.856858
2894.084100	619675.939172	39.861876
2897.127724	620772.979590	39.866893
2899.393527	621857.041778	39.871911
2902.283487	622959.735701	39.876928
2905.028871	624084.680224	39.881946
2908.018457	625219.761232	39.886964
2910.407406	626339.432556	39.891981
2912.882982	627469.414387	39.896999
2916.174300	628609.532943	39.902016
2918.736852	629763.835146	39.907034
2921.639104	630911.163780	39.912052
2924.654917	632071.632913	39.917069
2927.478840	633235.900855	39.922087
2930.411043	634409.158743	39.927104
2933.240871	635594.832442	39.932122
2936.166225	636757.444760	39.937140
2939.259862	637952.590505	39.942157
2942.565519	639144.819014	39.947175
2945.593622	640323.433457	39.952192
2948.385843	641520.911215	39.957210
2951.320862	642707.200965	39.962228
2954.299661	643907.512273	39.967245
2957.132780	645110.449567	39.972263
2960.002741	646312.141432	39.977280
2963.023979	647520.297733	39.982298
2966.230059	648719.254969	39.987316
2969.122684	649927.144171	39.992333
2972.281425	651145.211942	39.997351
2975.221368	652348.913445	40.002368
2978.404261	653565.485832	40.007386
2981.031815	654769.593839	40.012404
2983.990527	655977.934924	40.017421
2986.917561	657207.952134	40.022439
2990.092677	658427.364671	40.027456
2993.239174	659653.453135	40.032474
2996.647351	660878.199288	40.037492
2998.974292	662098.936575	40.042509
3001.549315	663329.983758	40.047527
3005.064251	664544.790707	40.052544
3008.148988	665769.519381	40.057562
3011.197511	666989.718630	40.062580
3015.506784	668198.757125	40.067597
3018.840731	669395.464660	40.072615
3022.936787	670547.920776	40.077632
3026.307608	671698.615427	40.082650
3029.741462	672820.761580	40.087668
3032.936630	673929.038789	40.092685
3036.165072	675027.086202	40.097703
3039.235217	676120.655981	40.102720
3042.162583	677235.049473	40.107738
3044.809508	678340.061117	40.112756
3047.626169	679444.118183	40.117773
3050.336627	680565.950553	40.122791
3052.798708	681669.204127	40.127808
3055.541380	682798.858509	40.132826
3058.498327	683927.096740	40.137844
3061.673073	685074.878382	40.142861
3064.281855	686225.836970	40.147879
3067.230712	687371.678039	40.152896
3070.116645	688540.769660	40.157914
3072.732123	689709.605819	40.162932
3075.922297	690874.473063	40.167949
3078.769103	692062.274301	40.172967
3082.103636	693243.585230	40.177984
3085.465786	694437.536578	40.183002
3088.422264	695621.919205	40.188020
3091.438059	696832.225570	40.193037
3094.153429	698045.937368	40.198055
3097.113718	699254.235015	40.203072
3100.273353	700476.861727	40.208090
3102.904755	701718.144796	40.213108
3106.103907	702954.796096	40.218125
3108.462561	704211.631675	40.223143
3111.530886	705459.298324	40.228160
3114.567530	706720.515147	40.233178
3117.537659	708006.031539	40.238196
3120.581955	709290.452161	40.243213
3123.195810	710578.168688	40.248231
3126.480404	711885.635497	40.253248
3129.236531	713194.622692	40.258266
3132.700500	714520.914456	40.263284
3135.823292	715825.920580	40.268301
3139.043130	717150.701693	40.273319
3142.845099	718459.691388	40.278336
3145.922738	719799.416731	40.283354
3148.870544	721136.327238	40.288372
3152.121692	722453.636243	40.293389
3154.830794	723804.103801	40.298407
3158.275770	725145.330777	40.303424
3161.551548	726483.006297	40.308442
3164.549837	727837.363315	40.313460
3167.630407	729192.817257	40.318477
3170.851196	730550.394798	40.323495
3173.655640	731910.976163	40.328512
3177.136321	733267.908960	40.333530
3180.331295	734625.698291	40.338548
3183.909503	735983.541519	40.343565
3187.505202	737345.397920	40.348583
3190.597806	738694.717160	40.353600
3193.884143	740057.495443	40.358618
3197.044379	741418.087634	40.363636
3200.105896	742778.512157	40.368653
3202.947901	744151.118980	40.373671
3206.597159	745511.912927	40.378688
3210.386429	746882.703808	40.383706
3213.352134	748251.270709	40.388724
3216.632898	749591.599183	40.393741
3220.434102	750947.528651	40.398759
3223.849133	752293.873907	40.403776
3227.614419	753629.680399	40.408794
3230.853907	754964.258493	40.413812
3234.543761	756295.625185	40.418829
3237.539191	757578.966766	40.423847
3240.714272	758870.875287	40.428864
3244.250964	760130.855923	40.433882
3247.379504	761403.883883	40.438900
3250.584800	762667.287108	40.443917
3253.752777	763939.930844	40.448935
3256.920295	765213.392509	40.453952
3260.073600	766483.984799	40.458970
3263.006484	767778.737593	40.463988
3266.332094	769050.192880	40.469005
3269.673566	770323.738587	40.474023
3272.987922	771609.749861	40.479040
3276.158519	772908.533569	40.484058
3279.339267	774195.148672	40.489076
3282.966302	775493.057562	40.494093
3286.069759	776799.564827	40.499111
3289.055183	778104.532354	40.504128
3292.159388	779414.205239	40.509146
3295.587521	780737.185328	40.514164
3298.738266	782063.355866	40.519181
3301.809325	783410.787398	40.524199
3305.295572	784739.060480	40.529216
3308.622752	786083.447292	40.534234
3311.500954	787446.584821	40.539252
3314.933667	788804.222694	40.544269
3317.649555	790159.219711	40.549287
3320.842502	791542.403850	40.554304
3323.911311	792924.652065	40.559322
3327.065671	794331.454080	40.564340
3330.405147	795716.294300	40.569357
3333.570966	797130.370748	40.574375
3336.704365	798550.629454	40.579392
3340.493163	799974.064219	40.584410
3343.235682	801412.160064	40.589428
3346.345702	802845.639707	40.594445
3349.245485	804302.632112	40.599463
3352.466654	805754.372026	40.604480
3356.053581	807217.040486	40.609498
3359.280420	808690.700079	40.614516
3362.742880	810162.487007	40.619533
3366.199190	811656.093656	40.624551
3369.496674	813144.071574	40.629568
3373.158867	814651.786433	40.634586
3376.486689	816152.283836	40.639604
3379.762578	817642.200861	40.644621
3382.621348	819159.190545	40.649639
3385.925951	820662.438317	40.654656
3389.428540	822181.561040	40.659674
3392.637387	823690.042132	40.664692
3396.224808	825216.843627	40.669709
3399.875394	826749.228880	40.674727
3402.963099	828285.930953	40.679744
3406.798534	829813.327547	40.684762
3410.259845	831346.810494	40.689780
3413.827600	832882.739129	40.694797
3417.692768	834411.777157	40.699815
3420.866810	835944.559185	40.704832
3424.161403	837468.486219	40.709850
3427.988627	838986.561385	40.714868
3431.672711	840519.722948	40.719885
3435.548170	842045.722680	40.724903
3438.967596	843569.436934	40.729920
3442.877616	845077.242682	40.734938
3445.914593	846603.400056	40.739956
3449.504410	848106.839230	40.744973
3453.649814	849599.720890	40.749991
3457.515164	851075.388781	40.755008
3462.351227	852539.243838	40.760013
3465.305673	853954.764237	40.765018
3468.951869	855307.557812	40.770023
3472.350297	856595.289489	40.775028
3475.029320	857814.671842	40.780032
3478.224877	858942.974632	40.785037
3480.678553	860032.679887	40.790042
3483.453343	861022.762449	40.795047
3485.849355	861968.413651	40.800052
3487.781075	862848.476608	40.805056
3490.392484	863648.600588	40.810061
3492.177251	864405.994790	40.815066
3494.415883	865091.604085	40.820071
3496.303641	865713.261067	40.825076
3497.773997	866281.391724	40.830080
3499.459228	866805.815722	40.835085
3501.360989	867290.235318	40.840090
3502.568537	867700.134687	40.845095
3504.012876	868066.067076	40.850100
3505.229820	868402.393441	40.855104
3506.524060	868699.260025	40.860109
3507.617315	868950.309234	40.865114
3508.676777	869159.597753	40.870119
3509.589003	869338.509793	40.875124
3510.377613	869483.548527	40.880128
3511.560960	869605.311989	40.885133
3512.557121	869684.477824	40.890138
3513.223290	869735.150387	40.895143
3513.690528	869763.620123	40.900148
3514.448724	869770.777626	40.905152
3515.002203	869753.403316	40.910157
3515.485085	869717.397852	40.915162
3516.166924	869662.133910	40.920167
3516.668312	869577.866363	40.925172
3516.937938	869481.983640	40.930176
3517.617733	869368.164837	40.935181
3517.557887	869245.920446	40.940186
3518.203083	869086.656549	40.945191
3518.640012	868932.375373	40.950196
3518.691331	868764.363711	40.955200
3519.431698	868580.306845	40.960205
3519.328914	868401.433421	40.965210
3519.488296	868194.637461	40.970215
3519.653898	867969.282351	40.975220
3519.685590	867748.797345	40.980224
3520.103095	867508.134151	40.985229
3519.806010	867281.761077	40.990234
3520.252304	867020.966311	40.995239
3520.437762	866781.186616	41.000244
3520.285790	866541.452979	41.005248
3520.630456	866278.699925	41.010253
3520.882892	866018.671050	41.015258
3520.862755	865740.020857	41.020263
3520.805704	865458.254589	41.025268
3520.742527	865190.663143	41.030272
3521.147278	864893.635907	41.035277
3521.055377	864618.347059	41.040282
3520.925074	864316.423509	41.045287
3521.062756	864021.146863	41.050292
3520.598091	863727.024208	41.055296
3520.628748	863426.876594	41.060301
3520.742385	863141.281026	41.065306
3520.921810	862834.955877	41.070311
3520.888500	862535.163635	41.075316
3520.825976	862229.722808	41.080320
3520.883519	861921.135762	41.085325
3520.292229	861618.570865	41.090330
3520.749369	861309.692614	41.095335
3520.797274	861005.922500	41.100340
3520.377112	860701.144714	41.105344
3520.124771	860406.340536	41.110349
3520.415481	860093.538358	41.115354
3520.403933	859785.243803	41.120359
3520.323136	859469.650497	41.125364
3519.816306	859178.427789	41.130368
3520.096571	858855.351126	41.135373
3520.129698	858556.033648	41.140378
3519.626252	858241.419522	41.145383
3519.875266	857930.459505	41.150388
3519.335097	857618.640839	41.155392
3519.783117	857323.573100	41.160397
3519.255316	857030.208763	41.165402
3519.093523	856731.321067	41.170407
3519.129479	856421.195646	41.175412
3518.767283	856123.868467	41.180416
3519.196354	855828.148375	41.185421
3519.048044	855542.436285	41.190426
3519.154722	855241.291058	41.195431
3519.101426	854935.582838	41.200436
3518.756635	854637.986600	41.205440
3518.886595	854335.820075	41.210445
3518.484376	854044.337360	41.215450
3518.562933	853741.760938	41.220455
3518.687396	853447.924321	41.225460
3518.288982	853152.310046	41.230464
3518.342989	852846.481078	41.235469
3517.971511	852575.955393	41.240474
3518.044155	852280.708895	41.245479
3518.275921	851994.575872	41.250484
3517.654744	851700.487297	41.255488
3517.959116	851401.557704	41.260493
3517.275558	851134.137174	41.265498
3517.817450	850835.141297	41.270503
3517.555220	850562.854369	41.275508
3516.755729	850285.481516	41.280512
3516.959734	849998.677019	41.285517
3516.841413	849734.415355	41.290522
3516.546584	849465.203218	41.295527
3516.685301	849198.051395	41.300532
3516.415914	848934.657635	41.305536
3516.529013	848649.559957	41.310541
3516.350536	848395.871747	41.315546
3516.228417	848134.758561	41.320551
3515.869006	847860.323758	41.325556
3515.995636	847605.286543	41.330560
3515.718980	847342.801587	41.335565
3515.597719	847084.957964	41.340570
3515.483685	846829.539078	41.345575
3515.498712	846578.864299	41.350580
3515.377743	846325.472834	41.355584
3515.508687	846073.686700	41.360589
3515.540229	845823.758915	41.365594
3515.216407	845578.266333	41.370599
3515.220100	845328.128529	41.375604
3515.016410	845087.861169	41.380608
3515.033679	844836.726782	41.385613
3514.731176	844598.406889	41.390618
3514.710486	844350.964239	41.395623
3514.678081	844100.393761	41.400628
3514.320990	843860.299989	41.405632
3514.439892	843623.824069	41.410637
3514.460490	843402.226270	41.415642
3513.934150	843153.698691	41.420647
3514.274410	842920.426871	41.425652
3513.935678	842691.012988	41.430656
3514.055030	842469.512605	41.435661
3513.854056	842249.276391	41.440666
3513.931748	842014.892935	41.445671
3513.963733	841779.630521	41.450676
3513.635042	841549.686052	41.455680
3513.711817	841326.153221	41.460685
3513.416020	841098.235454	41.465690
3513.295597	840883.498908	41.470695
3513.524605	840671.672992	41.475700
3513.389873	840451.217263	41.480704
3513.450243	840237.209623	41.485709
3513.061838	840026.634708	41.490714
3513.166873	839801.385122	41.495719
3512.905451	839575.212231	41.500724
3512.613229	839363.087213	41.505728
3512.696309	839161.968449	41.510733
3512.525264	838944.345195	41.515738
3512.424604	838735.875893	41.520743
3512.315847	838535.110557	41.525748
3512.294697	838337.301007	41.530752
3512.283945	838135.482291	41.535757
3512.406954	837938.124635	41.540762
3512.471541	837745.455309	41.545767
3512.678408	837533.577822	41.550772
3512.206963	837324.879657	41.555776
3512.257061	837119.261091	41.560781
3512.211229	836937.322680	41.565786
3511.827772	836727.419244	41.570791
3511.680798	836539.873359	41.575796
3511.548339	836345.339715	41.580800
3511.875232	836150.578086	41.585805
3511.893076	835962.841784	41.590810
3511.382453	835768.499421	41.595815
3511.746942	835568.637244	41.600820
3511.586612	835383.061299	41.605824
3511.379028	835183.623130	41.610829
3511.317030	835014.765369	41.615834
3511.557345	834815.486137	41.620839
3511.485509	834643.593309	41.625844
3510.957273	834449.848765	41.630848
3510.762580	834262.195572	41.635853
3511.084057	834085.096326	41.640858
3510.986269	833905.229209	41.645863
3511.219716	833721.249608	41.650868
3510.735876	833553.204382	41.655872
3510.842644	833360.885184	41.660877
3510.508539	833187.775989	41.665882
3510.361970	833016.584697	41.670887
3510.532825	832844.262180	41.675892
3510.595060	832669.511058	41.680896
3510.392721	832493.773171	41.685901
3510.132310	832338.504397	41.690906
3509.765400	832171.722737	41.695911
3510.116216	832004.965095	41.700916
3510.167153	831841.134392	41.705920
3510.105091	831667.158243	41.710925
3509.897564	831513.961390	41.715930
3509.699270	831354.604535	41.720935
3509.769464	831199.107493	41.725940
3509.513646	831038.189172	41.730944
3509.525157	830885.820737	41.735949
3509.521073	830723.485314	41.740954
3509.304324	830567.629612	41.745959
3509.629401	830408.554191	41.750964
3509.457334	830244.035990	41.755968
3509.117145	830093.856628	41.760973
3509.365528	829945.628922	41.765978
3509.269745	829811.330723	41.770983
3509.431104	829647.524292	41.775988
3509.223381	829513.873595	41.780992
3509.162463	829355.129216	41.785997
3509.040375	829215.350396	41.791002
3509.079155	829068.310020	41.796007
3509.175587	828910.897146	41.801012
3508.824791	828769.289518	41.806016
3508.945106	828614.504416	41.811021
3508.812527	828480.184880	41.816026
3508.556808	828343.585941	41.821031
3508.539688	828210.463613	41.826036
3508.309415	828079.670702	41.831040
3508.071342	827936.560278	41.836045
3508.102162	827799.951659	41.841050
3507.996396	827675.239502	41.846055
3508.335687	827539.307771	41.851060
3507.609874	827407.507759	41.856064
3507.905200	827282.086638	41.861069
3507.711718	827157.525707	41.866074
3507.666620	827048.530837	41.871079
3508.052965	826901.971082	41.876084
3507.703030	826792.337824	41.881088
3507.788738	826661.611191	41.886093
3507.494217	826540.428125	41.891098
3507.402194	826417.400717	41.896103
3507.830669	826288.223397	41.901108
3507.435817	826172.280868	41.906112
3507.702121	826057.889572	41.911117
3507.747614	825936.883799	41.916122
3507.511116	825818.464504	41.921127
3507.478135	825692.089294	41.926132
3507.165515	825579.740657	41.931136
3507.352045	825461.294139	41.936141
3507.240869	825351.304136	41.941146
3506.991121	825240.895075	41.946151
3507.223777	825136.712111	41.951156
3506.586606	825020.006851	41.956160
3507.086728	824899.689441	41.961165
3506.956232	824777.224433	41.966170
3507.056867	824683.568962	41.971175
3506.959867	824571.998868	41.976180
3506.910851	824473.181779	41.981184
3506.653987	824360.509746	41.986189
3506.699053	824251.893756	41.991194
3506.780129	824144.492597	41.996199
3506.698791	824043.767219	42.001204
3506.648036	823942.692940	42.006208
3506.935313	823837.942520	42.011213
3506.456579	823737.229015	42.016218
3506.741425	823633.551663	42.021223
3506.761677	823527.960006	42.026228
3506.534281	823430.330438	42.031232
3506.578681	823328.595291	42.036237
3506.472515	823219.498146	42.041242
3506.200717	823118.692210	42.046247
3506.314414	823022.859002	42.051252
3506.170784	822931.713336	42.056256
3506.064076	822833.223579	42.061261
3505.814374	822741.016699	42.066266
3505.978162	822653.436077	42.071271
3506.343592	822548.994754	42.076276
3505.802818	822460.745014	42.081280
3506.212771	822353.749726	42.086285
3506.225139	822278.368973	42.091290
3505.848021	822176.343126	42.096295
3506.121279	822079.785150	42.101300
3505.687855	821997.185948	42.106304
3505.858475	821916.540794	42.111309
3505.822922	821825.704526	42.116314
3505.729607	821734.974366	42.121319
3505.923641	821637.444603	42.126324
3505.445163	821569.621476	42.131328
3505.489001	821471.673725	42.136333
3505.547459	821386.148420	42.141338
3505.567671	821304.101847	42.146343
3506.126681	821229.255124	42.151348
3505.510958	821138.456083	42.156352
3505.592325	821055.075405	42.161357
3505.277322	820970.486907	42.166362
3505.173240	820906.509362	42.171367
3505.433365	820798.535158	42.176372
3505.460901	820726.265576	42.181376
3505.555222	820639.892990	42.186381
3505.454662	820560.792801	42.191386
3505.581277	820482.241399	42.196391
3505.379307	820395.669799	42.201396
3505.356748	820336.028074	42.206400
3505.429510	820247.745671	42.211405
3505.573157	820168.502728	42.216410
3504.907005	820085.624468	42.221415
3505.299226	820005.164268	42.226420
3505.441226	819931.350285	42.231424
3505.802006	819851.235938	42.236429
3505.775180	819760.223185	42.241434
3505.534075	819691.852429	42.246439
3505.470554	819602.947769	42.251444
3505.505034	819514.613014	42.256448
3505.574294	819428.375641	42.261453
3505.398522	819354.950172	42.266458
3505.528181	819280.592701	42.271463
3505.813218	819185.752513	42.276468
3505.391007	819108.351954	42.281472
3505.147156	819019.028754	42.286477
3505.516896	818943.600245	42.291482
3505.095568	818877.257368	42.296487
3505.345073	818791.569361	42.301492
3504.940100	818715.776470	42.306496
3505.286463	818637.607601	42.311501
3505.251031	818567.135837	42.316506
3505.073590	818481.563119	42.321511
3505.312266	818407.716346	42.326516
3504.917014	818342.636405	42.331520
3504.841686	818255.967191	42.336525
3504.971684	818189.575605	42.341530
3504.761012	818122.064760	42.346535
3504.982680	818052.132569	42.351540
3504.831417	817984.953182	42.356544
3504.581880	817908.489203	42.361549
3504.964268	817850.422769	42.366554
3504.534306	817786.077345	42.371559
3504.765076	817705.616022	42.376564
3504.693934	817640.329001	42.381568
3505.082812	817562.972714	42.386573
3504.774263	817496.989141	42.391578
3504.814614	817418.024255	42.396583
3504.998783	817351.419621	42.401588
3504.736250	817294.972112	42.406592
3504.889472	817229.595174	42.411597
3504.879669	817162.041549	42.416602
3504.751448	817094.849424	42.421607
3504.738247	817022.007922	42.426612
3504.442333	816949.603835	42.431616
3504.431028	816875.193865	42.436621
3504.431249	816808.761001	42.441626
3504.360801	816745.031724	42.446631
3504.364404	816676.736649	42.451636
3504.375714	816632.967246	42.456640
3504.391672	816570.739754	42.461645
3504.644438	816498.044578	42.466650
3504.295842	816460.453111	42.471655
3504.379565	816393.072161	42.476660
3504.418057	816323.445847	42.481664
3504.332896	816265.051017	42.486669
3504.505202	816190.652166	42.491674
3504.586506	816142.265744	42.496679
3504.357558	816081.249112	42.501684
3504.264604	816022.265917	42.506688
3504.228732	815947.898665	42.511693
3504.505719	815900.800251	42.516698
3504.226031	815838.712594	42.521703
3504.253601	815770.306417	42.526708
3503.969280	815716.542193	42.531712
3504.095242	815656.589410	42.536717
3504.108286	815600.082230	42.541722
3504.095763	815546.761524	42.546727
3504.169702	815488.333731	42.551732
3504.155112	815436.187663	42.556736
3504.151931	815368.712817	42.561741
3503.984351	815315.170981	42.566746
3503.798743	815276.223920	42.571751
3504.186478	815206.136758	42.576756
3503.852888	815161.141411	42.581760
3503.776193	815105.575247	42.586765
3503.960005	815045.705425	42.591770
3503.758376	814999.071284	42.596775
3503.923586	814941.945877	42.601780
3503.884613	814899.348727	42.606784
3504.186419	814846.607303	42.611789
3504.003902	814791.888473	42.616794
3503.865668	814739.218689	42.621799
3503.789150	814680.123063	42.626804
3503.809530	814638.591859	42.631808
3503.805803	814574.879968	42.636813
3504.061167	814531.840232	42.641818
3503.987999	814486.258772	42.646823
3504.136822	814408.954672	42.651828
3503.483517	814366.651236	42.656832
3503.954628	814323.525659	42.661837
3503.842660	814272.806863	42.666842
3503.853716	814222.899993	42.671847
3504.134856	814156.786432	42.676852
3503.793030	814107.965318	42.681856
3503.614897	814054.758019	42.686861
3503.834030	813998.448323	42.691866
3504.113772	813961.522987	42.696871
3503.899309	813912.483570	42.701876
3503.691409	813866.871135	42.706880
3503.608425	813810.070878	42.711885
3503.877138	813754.632582	42.716890
3503.396241	813706.811032	42.721895
3503.766466	813657.379578	42.726900
3503.981943	813612.479348	42.731904
3503.393221	813566.584753	42.736909
3503.626852	813512.766575	42.741914
3503.479714	813473.263964	42.746919
3503.483974	813418.650153	42.751924
3503.496909	813393.618972	42.756928
3503.188133	813332.884439	42.761933
3503.328688	813292.892551	42.766938
3503.226926	813247.258441	42.771943
3503.798809	813195.929083	42.776948
3503.366266	813164.210870	42.781952
3503.469612	813108.843494	42.786957
3503.557484	813062.246222	42.791962
3503.188976	813032.329221	42.796967
3503.405604	812989.922819	42.801972
3503.679100	812946.478119	42.806977
3503.393670	812902.880283	42.811981
3503.264398	812843.483341	42.816986
3503.047218	812808.348025	42.821991
3503.398140	812765.330273	42.826996
3503.230928	812728.520807	42.832001
3503.186354	812700.606374	42.837005
3503.765237	812647.802131	42.842010
3503.103688	812606.909594	42.847015
3503.187961	812566.089906	42.852020
3503.056804	812535.641737	42.857025
3503.092565	812492.331254	42.862029
3503.224291	812446.800239	42.867034
3503.163204	812421.728662	42.872039
3503.563145	812369.343626	42.877044
3503.331438	812342.193362	42.882049
3503.079059	812297.116517	42.887053
3503.380531	812255.965249	42.892058
3503.230327	812207.735675	42.897063
3503.399776	812169.300047	42.902068
3503.416945	812119.915514	42.907073
3502.957457	812085.649183	42.912077
3503.221856	812045.874475	42.917082
3503.025768	812019.549888	42.922087
3502.961837	811986.393678	42.927092
3503.051744	811943.560674	42.932097
3502.863668	811902.487897	42.937101
3503.295868	811864.497176	42.942106
3502.979572	811821.681319	42.947111
3502.829433	811788.685317	42.952116
3502.947543	811756.281874	42.957121
3503.045640	811727.458057	42.962125
3503.049956	811691.349584	42.967130
3502.802150	811652.391834	42.972135
3502.973684	811617.970198	42.977140
3502.823579	811595.359908	42.982145
3503.209009	811557.130201	42.987149
3503.263514	811525.862999	42.992154
3502.892480	811488.688403	42.997159
3503.299796	811437.519818	43.002164
3503.035781	811409.097259	43.007169
3502.557498	811369.391920	43.012173
3502.913162	811345.276616	43.017178
3502.886257	811317.010597	43.022183
3502.910793	811277.662860	43.027188
3502.759989	811254.806567	43.032193
3502.420639	811213.656536	43.037197
3502.727036	811190.479733	43.042202
3502.779082	811165.874839	43.047207
3503.223938	811120.773306	43.052212
3502.648741	811087.010946	43.057217
3502.422520	811048.291154	43.062221
3502.704170	811025.754838	43.067226
3502.569083	811001.915142	43.072231
3502.085586	810979.896692	43.077236
3502.196129	810939.062875	43.082241
3502.166539	810927.259189	43.087245
3502.577217	810904.260229	43.092250
3502.459233	810881.250273	43.097255
3502.742504	810853.323223	43.102260
3502.684454	810840.936084	43.107265
3502.575388	810792.346660	43.112269
3502.869358	810774.952448	43.117274
3502.460287	810750.079002	43.122279
3502.773571	810708.965406	43.127284
3502.413595	810682.760618	43.132289
3502.423800	810660.561806	43.137293
3502.841717	810632.464668	43.142298
3502.599366	810600.899096	43.147303
3502.958960	810577.025426	43.152308
3502.258217	810553.130322	43.157313
3502.224841	810538.582505	43.162317
3502.455396	810495.619189	43.167322
3502.501784	810477.627974	43.172327
3502.689278	810439.571590	43.177332
3502.380454	810433.056276	43.182337
3502.578402	810393.184825	43.187341
3502.496895	810373.940337	43.192346
3502.285935	810349.277799	43.197351
3502.239117	810323.461065	43.202356
3502.567742	810291.064955	43.207361
3502.480403	810280.004706	43.212365
3502.498585	810237.564774	43.217370
3502.549101	810215.602887	43.222375
3502.288464	810193.153138	43.227380
3502.500934	810161.608613	43.232385
3502.288189	810146.501451	43.237389
3502.291867	810118.862460	43.242394
3502.129475	810104.432974	43.247399
3502.492309	810070.756060	43.252404
3502.287162	810056.529534	43.257409
3502.092915	810027.746655	43.262413
3502.220375	810012.485146	43.267418
3502.307497	809993.113792	43.272423
3502.100515	809964.381748	43.277428
3502.193591	809971.864395	43.282433
3502.244084	809942.109735	43.287437
3502.512925	809911.583888	43.292442
3501.993458	809891.234026	43.297447
3502.403915	809863.674014	43.302452
3502.473904	809860.477188	43.307457
3502.112388	809829.760767	43.312461
3502.491203	809808.723622	43.317466
3502.636624	809779.295661	43.322471
3502.422476	809758.160003	43.327476
3502.215714	809726.486488	43.332481
3502.151411	809705.963082	43.337485
3502.249652	809687.030092	43.342490
3502.330884	809669.080007	43.347495
3502.276550	809647.476611	43.352500
3502.535174	809609.599900	43.357505
3502.095722	809593.254635	43.362509
3502.453582	809570.700950	43.367514
3502.377380	809553.854680	43.372519
3502.286997	809532.403883	43.377524
3502.176704	809517.964568	43.382529
3502.238592	809501.928575	43.387533
3502.549759	809469.237379	43.392538
3502.187199	809458.368153	43.397543
3502.242934	809411.211986	43.402548
3502.277397	809403.462901	43.407553
3502.196214	809384.705655	43.412557
3502.375136	809352.133700	43.417562
3502.195579	809345.449013	43.422567
3502.417819	809309.537032	43.427572
3502.208218	809304.670637	43.432577
3502.308780	809280.590041	43.437581
3502.373306	809254.358823	43.442586
3502.094981	809228.380022	43.447591
3502.185920	809204.202720	43.452596
3502.299901	809183.599361	43.457601
3502.214332	809160.725271	43.462605
3502.112390	809147.656115	43.467610
3502.068877	809142.272130	43.472615
3502.282251	809103.811923	43.477620
3502.258542	809099.404880	43.482625
3502.164710	809073.395097	43.487629
3502.148048	809053.744093	43.492634
3502.192410	809040.454584	43.497639
3502.157445	808998.309751	43.502644
3502.012625	808990.197627	43.507649
3502.197613	808980.070659	43.512653
3502.374576	808956.662513	43.517658
3502.181142	808943.608035	43.522663
3502.520943	808910.909447	43.527668
3501.963506	808906.345127	43.532673
3502.066667	808878.978795	43.537677
3502.096454	808848.634606	43.542682
3501.811001	808834.761843	43.547687
3502.015642	808825.513657	43.552692
3502.299166	808804.047989	43.557697
3501.656160	808798.027269	43.562701
3502.213036	808773.330564	43.567706
3502.122402	808755.847512	43.572711
3502.274240	808743.765079	43.577716
3502.200641	808713.192245	43.582721
3502.368092	808688.216276	43.587725
3502.206454	808666.774488	43.592730
3501.828126	808656.641798	43.597735
3502.033691	808640.776173	43.602740
3502.223449	808628.638276	43.607745
3502.205143	808599.085142	43.612749
3502.230913	808588.199572	43.617754
3502.291042	808560.152832	43.622759
3502.196155	808535.415579	43.627764
3502.141021	808527.092065	43.632769
3502.340139	808502.404297	43.637773
3502.485119	808482.774038	43.642778
3502.206004	808453.753398	43.647783
3502.411480	808440.632247	43.652788
3502.243524	808419.631872	43.657793
3501.814243	808407.448498	43.662797
3502.131273	808395.877426	43.667802
3501.969528	808357.964974	43.672807
3502.430034	808334.802095	43.677812
3502.133861	808320.537910	43.682817
3502.084444	808302.899854	43.687821
3502.473724	808289.159926	43.692826
3501.819736	808253.141627	43.697831
3502.285562	808244.094723	43.702836
3502.398175	808241.870480	43.707841
3502.409111	808206.820808	43.712845
3502.591309	808182.330743	43.717850
3502.124426	808156.673021	43.722855
3502.011064	808136.447079	43.727860
3501.938819	808125.674953	43.732865
3501.992552	808107.970384	43.737869
3502.143631	808091.818346	43.742874
3502.058767	808083.205073	43.747879
3502.044974	808044.531220	43.752884
3502.155204	808037.111239	43.757889
3501.915788	808024.258650	43.762893
3502.074523	807990.310972	43.767898
3501.859352	807997.797546	43.772903
3502.031103	807977.720249	43.777908
3501.938796	807957.882468	43.782913
3501.795242	807937.415808	43.787917
3501.985521	807931.011952	43.792922
3502.284492	807909.295829	43.797927
3502.032211	807882.670338	43.802932
3502.282348	807875.913426	43.807937
3501.873222	807853.088245	43.812941
3502.018042	807832.720833	43.817946
3501.879971	807842.106695	43.822951
3502.003388	807809.487500	43.827956
3502.104625	807797.754880	43.832961
3501.932962	807789.547703	43.837965
3502.068950	807749.621976	43.842970
3502.204164	807733.373662	43.847975
3502.073518	807728.248021	43.852980
3502.011844	807700.806076	43.857985
3501.821132	807682.650450	43.862989
3502.098026	807676.771331	43.867994
3501.775945	807656.431280	43.872999
3502.214710	807631.308713	43.878004
3502.271469	807629.240541	43.883009
3501.879233	807613.765137	43.888013
3502.383511	807586.572669	43.893018
3502.117780	807587.498967	43.898023
3502.233769	807556.350471	43.903028
3502.130411	807534.013108	43.908033
3502.128220	807521.463657	43.913037
3502.222073	807502.329237	43.918042
3501.957416	807490.215148	43.923047
3502.054673	807461.030241	43.928052
3502.117929	807446.508926	43.933057
3502.071316	807440.928012	43.938061
3502.271699	807405.843026	43.943066
3502.359480	807403.083338	43.948071
3502.184212	807379.139520	43.953076
3502.354254	807342.735553	43.958081
3501.641979	807349.373250	43.963085
3501.991937	807321.175635	43.968090
3501.706084	807303.671992	43.973095
3501.985333	807284.114226	43.978100
3502.059600	807285.523834	43.983105
3501.733446	807260.918106	43.988109
3501.933760	807236.372645	43.993114
3501.928873	807243.237101	43.998119
3501.694220	807220.233986	44.003124
3502.035545	807200.224527	44.008129
3501.751341	807188.701428	44.013133
3501.876902	807186.425686	44.018138
3501.989643	807184.004979	44.023143
3502.017266	807150.417909	44.028148
3502.053944	807137.027910	44.033153
3501.886530	807131.515668	44.038157
3501.822667	807100.541800	44.043162
3502.055288	807088.688270	44.048167
3501.752507	807083.786603	44.053172
3501.993131	807067.960584	44.058177
3501.804607	807048.773356	44.063181
3502.264334	807021.242799	44.068186
3501.856978	807019.545051	44.073191
3501.634149	806993.303454	44.078196
3502.072888	806987.789305	44.083201
3501.971919	806989.227839	44.088205
3501.908649	806965.509258	44.093210
3501.600068	806952.764095	44.098215
3501.703189	806933.283367	44.103220
3501.900920	806932.221340	44.108225
3501.826843	806916.397781	44.113229
3501.981504	806895.143463	44.118234
3501.690378	806877.149318	44.123239
3501.954941	806868.427927	44.128244
3501.647359	806849.602946	44.133249
3501.707438	806836.306561	44.138253
3502.023593	806827.037310	44.143258
3501.946058	806827.540481	44.148263
3501.673036	806803.316578	44.153268
3501.596225	806794.896466	44.158273
3501.596339	806788.964124	44.163277
3501.774426	806780.158809	44.168282
3501.909069	806779.450350	44.173287
3501.933734	806752.627748	44.178292
3501.841112	806735.875281	44.183297
3501.905653	806726.255109	44.188301
3502.078086	806720.147237	44.193306
3501.839954	806706.654576	44.198311
3501.855892	806700.229261	44.203316
3501.735283	806691.963324	44.208321
3501.868577	806664.926369	44.213325
3502.132582	806640.417313	44.218330
3501.707208	806638.624376	44.223335
3502.050208	806629.448497	44.228340
3502.122938	806606.441714	44.233345
3501.882701	806598.097308	44.238349
3502.065235	806587.771089	44.243354
3501.705653	806562.285812	44.248359
3501.695145	806540.812451	44.253364
3501.808874	806540.156443	44.258369
3501.849620	806542.454271	44.263373
3502.055875	806505.647649	44.268378
3501.951323	806499.143931	44.273383
3501.949822	806493.701906	44.278388
3501.951680	806459.037015	44.283393
3501.664405	806457.711590	44.288397
3501.924746	806436.144257	44.293402
3501.491272	806439.451821	44.298407
3501.753282	806417.639000	44.303412
3501.919071	806404.961770	44.308417
3501.898686	806395.845436	44.313421
3502.047386	806388.515397	44.318426
3501.998245	806368.175579	44.323431
3501.802090	806342.613533	44.328436
3501.949035	806342.834605	44.333441
3501.930136	806339.944968	44.338445
3501.969881	806306.253698	44.343450
3501.806079	806290.051215	44.348455
3502.100528	806291.817017	44.353460
3502.173830	806268.269653	44.358465
3501.768666	806256.078452	44.363469
3502.084915	806241.120651	44.368474
3501.854111	806223.703238	44.373479
3501.933900	806209.568838	44.378484
3501.813747	806206.156464	44.383489
3501.847239	806194.334192	44.388493
3502.075083	806159.385399	44.393498
3501.962947	806150.676115	44.398503
3501.838868	806138.536470	44.403508
3501.719907	806129.730217	44.408513
3501.731173	806095.160004	44.413517
3501.993093	806083.594115	44.418522
3502.031381	806102.661934	44.423527
3501.716572	806081.090157	44.428532
3502.344709	806060.932069	44.433537
3501.918613	806054.039589	44.438541
3502.009750	806024.015995	44.443546
3502.026445	806015.138216	44.448551
3502.162364	805997.169480	44.453556
3502.071523	805971.196427	44.458561
3501.848805	805951.962720	44.463565
3501.957059	805948.512595	44.468570
3501.912643	805943.518512	44.473575
3501.947848	805909.531833	44.478580
3501.990377	805907.171278	44.483585
3501.701205	805908.395863	44.488589
3502.021338	805873.528482	44.493594
3501.891974	805868.744477	44.498599
3501.786805	805858.611658	44.503604
3501.915328	805847.606731	44.508609
3501.438769	805828.463525	44.513613
3501.850311	805812.949709	44.518618
3501.963575	805806.801738	44.523623
3501.847560	805807.556498	44.528628
3501.961807	805778.067412	44.533633
3501.920490	805773.268837	44.538637
3501.997075	805757.466819	44.543642
3501.941993	805744.824752	44.548647
3501.566519	805724.830995	44.553652
3501.873121	805711.442786	44.558657
3501.872817	805705.166323	44.563661
3501.936824	805672.546740	44.568666
3501.970349	805667.196362	44.573671
3501.738865	805658.309965	44.578676
3502.145776	805650.789498	44.583681
3501.847615	805632.695164	44.588685
3502.095695	805619.267379	44.593690
3501.799880	805614.902908	44.598695
3501.835338	805604.991734	44.603700
3501.907027	805567.908027	44.608705
3501.942055	805557.996856	44.613709
3501.992896	805547.935954	44.618714
3501.856424	805518.045713	44.623719
3501.895125	805506.809849	44.628724
3502.103768	805499.321877	44.633729
3501.965511	805489.095886	44.638733
3502.323311	805473.148818	44.643738
3501.716814	805467.266215	44.648743
3502.032893	805444.411603	44.653748
3502.217817	805413.830474	44.658753
3502.114720	805413.602382	44.663757
3502.048008	805384.337566	44.668762
3501.744534	805377.228047	44.673767
3501.739891	805371.981804	44.678772
3502.141669	805350.387767	44.683777
3502.024162	805334.812902	44.688781
3501.840608	805313.315164	44.693786
3501.623844	805315.067353	44.698791
3501.438469	805294.697753	44.703796
3501.728666	805268.659276	44.708801
3501.404410	805266.947389	44.713805
3501.540037	805263.443373	44.718810
3501.577837	805263.682462	44.723815
3501.252409	805261.137098	44.728820
3501.384083	805259.055873	44.733825
3501.481547	805258.255307	44.738829
3501.741534	805237.223704	44.743834
3501.853476	805222.640621	44.748839
3501.289297	805227.980911	44.753844
3501.790184	805207.547053	44.758849
3501.466147	805216.918095	44.763853
3501.689963	805205.357008	44.768858
3501.661197	805187.413282	44.773863
3501.466518	805170.379558	44.778868
3501.520992	805162.965655	44.783873
3501.623536	805156.426549	44.788877
3501.569179	805155.405778	44.793882
3501.430514	805151.995927	44.798887
3501.612455	805155.938328	44.803892
3501.757951	805126.392257	44.808897
3501.630229	805124.991244	44.813901
3501.804419	805123.393379	44.818906
3501.373916	805120.571027	44.823911
3501.614333	805120.384423	44.828916
3501.596501	805083.263806	44.833921
3501.702732	805079.617417	44.838925
3501.506259	805067.585881	44.843930
3501.520867	805071.653975	44.848935
3501.421071	805067.403987	44.853940
3501.717769	805054.996950	44.858945
3501.738583	805049.010653	44.863949
3501.643895	805021.367248	44.868954
3501.769195	805013.941518	44.873959
3501.545677	805011.575437	44.878964
3501.841002	805003.533196	44.883969
3501.746511	804993.201174	44.888973
3501.628680	804959.529250	44.893978
3501.742863	804957.205608	44.898983
3501.370163	804966.928295	44.903988
3501.591671	804958.211580	44.908993
3501.508691	804965.336387	44.913997
3501.651547	804944.028933	44.919002
3501.645982	804929.415542	44.924007
3501.333240	804917.108643	44.929012
3501.664856	804910.825823	44.934017
3501.674186	804910.824404	44.939021
3501.625295	804904.457128	44.944026
3501.930682	804884.103556	44.949031
3501.320646	804865.322935	44.954036
3501.805285	804855.483819	44.959041
3501.356024	804864.777881	44.964045
3501.580456	804864.348693	44.969050
3501.838868	804864.943795	44.974055
3501.182220	804843.081131	44.979060
3501.767956	804830.086614	44.984065
3501.533705	804810.066924	44.989069
3501.830379	804812.372219	44.994074
3501.953719	804818.678511	44.999079
3501.291800	804800.887110	45.004084
3501.511348	804773.289032	45.009089
3501.402370	804769.579842	45.014093
3501.282553	804758.810252	45.019098
3501.625956	804765.325561	45.024103
3501.556268	804773.184021	45.029108
3502.000311	804767.127765	45.034113
3501.401813	804762.175046	45.039117
3501.482581	804742.642742	45.044122
3501.618361	804730.752059	45.049127
3501.209140	804721.452333	45.054132
3501.886047	804713.494030	45.059137
3501.866367	804714.723473	45.064141
3502.118674	804697.173558	45.069146
3501.778106	804679.083691	45.074151
3501.711993	804692.287397	45.079156
3501.594553	804670.090146	45.084161
3501.822163	804661.911531	45.089165
3501.449017	804622.738077	45.094170
3501.461425	804629.160904	45.099175
3501.432735	804618.277996	45.104180
3501.718129	804607.343335	45.109185
3501.627688	804621.532065	45.114189
3501.323494	804621.386114	45.119194
3501.084959	804614.706500	45.124199
3501.313211	804608.489475	45.129204
3501.282573	804603.492147	45.134209
3500.853207	804597.971963	45.139213
3501.314754	804609.421413	45.144218
3501.548092	804600.064725	45.149223
3501.351248	804571.308321	45.154228
3501.426409	804565.165519	45.159233
3501.154491	804560.796434	45.164237
3501.349506	804547.865747	45.169242
3501.205466	804560.101654	45.174247
3501.662762	804557.770405	45.179252
3501.431134	804546.822723	45.184257
3501.529758	804560.244770	45.189261
3501.319490	804559.004369	45.194266
3501.440632	804553.638693	45.199271
3501.515618	804561.130253	45.204276
3501.506206	804524.299498	45.209281
3501.107053	804519.313764	45.214285
3501.717673	804513.622207	45.219290
3501.643515	804516.184866	45.224295
3501.259466	804515.708752	45.229300
3501.737038	804509.401526	45.234305
3501.548224	804506.637195	45.239309
3501.640844	804499.804832	45.244314
3501.718213	804473.357002	45.249319
3501.349465	804469.592349	45.254324
3501.376399	804472.923092	45.259329
3501.772661	804466.531130	45.264333
3501.655284	804464.784961	45.269338
3501.559144	804463.476698	45.274343
3501.581087	804439.146804	45.279348
3501.625339	804417.216374	45.284353
3501.301992	804419.672978	45.289357
3501.333832	804424.376207	45.294362
3501.572432	804415.852173	45.299367
3501.601247	804420.899221	45.304372
3501.551217	804413.648861	45.309377
3501.328693	804403.582268	45.314381
3501.595952	804378.377977	45.319386
3501.123462	804375.905548	45.324391
3501.328283	804381.708364	45.329396
3501.355753	804360.418111	45.334401
3501.205423	804368.486499	45.339405
3501.339045	804366.061365	45.344410
3501.376926	804369.439401	45.349415
3501.423109	804383.066615	45.354420
3501.710383	804368.305705	45.359425
3501.774399	804370.894703	45.364429
3501.633350	804357.724741	45.369434
3501.246774	804336.944028	45.374439
3501.050679	804337.712137	45.379444
3501.352095	804323.046893	45.384449
3501.567589	804325.071450	45.389453
3501.516993	804334.006279	45.394458
3501.441302	804333.675544	45.399463
3501.301185	804342.576061	45.404468
3501.703815	804332.406390	45.409473
3501.544141	804334.737971	45.414477
3501.583177	804297.554700	45.419482
3501.544400	804294.127967	45.424487
3501.617505	804287.838118	45.429492
3501.420777	804274.235750	45.434497
3501.615629	804281.119314	45.439501
3501.559343	804275.194091	45.444506
3501.399337	804263.351323	45.449511
3501.579342	804241.201786	45.454516
3501.401589	804222.004868	45.459521
3501.455042	804233.424075	45.464525
3501.497469	804221.106469	45.469530
3501.677966	804225.932488	45.474535
3501.426579	804232.202950	45.479540
3501.875515	804215.796544	45.484545
3501.734987	804206.402811	45.489549
3501.908566	804190.728359	45.494554
3501.814794	804188.438713	45.499559
3501.396503	804183.750168	45.504564
3501.351885	804165.364962	45.509569
3501.567557	804150.811570	45.514573
3501.749322	804137.735155	45.519578
3501.524437	804130.268061	45.524583
3501.276161	804136.390956	45.529588
3501.542125	804126.194446	45.534593
3501.717507	804132.247560	45.539597
3501.604742	804127.753887	45.544602
3501.600801	804102.200880	45.549607
3501.512109	804100.695130	45.554612
3501.864811	804088.228084	45.559617
3501.942375	804086.596851	45.564621
3501.681484	804073.347988	45.569626
3502.052999	804036.942359	45.574631
3501.640641	804036.961352	45.579636
3502.071624	804032.427100	45.584641
3502.127343	804015.300218	45.589645
3501.901474	803997.582047	45.594650
3502.023954	803984.318913	45.599655
3501.754990	803971.561669	45.604660
3501.899661	803947.504114	45.609665
3501.607473	803950.691480	45.614669
3501.841740	803945.797185	45.619674
3501.658925	803935.576219	45.624679
3501.640171	803911.594506	45.629684
3501.560835	803902.435523	45.634689
3501.763379	803898.968844	45.639693
3501.775927	803892.786707	45.644698
3501.989552	803874.161990	45.649703
3501.985640	803857.044537	45.654708
3501.806945	803847.754700	45.659713
3502.055624	803849.724884	45.664717
3501.799737	803819.111182	45.669722
3501.654799	803808.246141	45.674727
3501.450841	803793.859218	45.679732
3501.644626	803794.857463	45.684737
3501.661843	803796.277190	45.689741
3501.618945	803773.329020	45.694746
3502.099362	803752.599930	45.699751
3501.726863	803758.105968	45.704756
3502.142313	803748.080478	45.709761
3501.861109	803724.190394	45.714765
3501.610318	803703.140146	45.719770
3502.029900	803712.292637	45.724775
3501.490202	803703.699724	45.729780
3501.665451	803674.731131	45.734785
3501.336815	803679.984752	45.739789
3501.609209	803673.416263	45.744794
3501.511363	803668.821731	45.749799
3501.313624	803661.643960	45.754804
3501.478747	803661.714981	45.759809
3501.387304	803657.855150	45.764813
3501.329571	803612.051171	45.769818
3501.432131	803553.957609	45.774823
3501.606091	803438.558870	45.779828
3501.450481	803262.533428	45.784833
3501.487264	803032.756511	45.789837
3501.277248	802724.570196	45.794842
3501.346650	802372.317475	45.799847
3500.934883	801967.040301	45.804852
3500.922676	801507.210437	45.809857
3500.250606	800991.813892	45.814861
3500.262389	800418.997518	45.819866
3500.160690	799767.333146	45.824871
3499.599142	799067.532870	45.829876
3499.641933	798310.767367	45.834881
3499.390522	797494.269697	45.839885
3498.781736	796613.315816	45.844890
3498.407724	795676.034037	45.849895
3497.680335	794674.444212	45.854900
3497.647060	793614.535907	45.859905
3496.520661	792498.444530	45.864909
3496.382684	791321.624235	45.869914
3495.998720	790083.462325	45.874919
3494.967004	788799.182349	45.879924
3494.243873	787427.943603	45.884929
3493.519154	786015.430781	45.889933
3492.697663	784534.338843	45.894938
3492.352929	782991.911141	45.899943
3490.963221	781399.382246	45.904948
3490.891019	779730.049302	45.909953
3489.371740	778010.752122	45.914957
3488.843509	776237.411394	45.919962
3488.310938	774397.298702	45.924967
3487.497479	772488.785640	45.929972
3486.569841	770516.573870	45.934977
3485.296885	768490.462172	45.939981
3484.045825	766415.575063	45.944986
3483.235568	764270.203692	45.949991
3482.154063	762066.001744	45.954996
3481.356957	759792.861014	45.960001
3480.048509	757485.261217	45.965005
3479.120922	755105.055301	45.970010
3477.867183	752664.793398	45.975015
3476.728565	750170.477310	45.980020
3475.807436	747617.297944	45.985025
3474.176739	745005.998267	45.990029
3472.681663	742334.704879	45.995034
3471.686072	739616.760766	46.000039
3469.894083	736847.784437	46.005044
3468.757694	734004.912875	46.010049
3467.340172	731127.753905	46.015053
3465.819838	728181.516487	46.020058
3464.767907	725187.104913	46.025063
3463.129039	722148.764218	46.030068
3461.629799	719040.442767	46.035073
3460.034770	715883.397638	46.040077
3458.498965	712659.538975	46.045082
3456.832990	709401.904498	46.050087
3455.143785	706081.138823	46.055092
3453.979999	702711.799931	46.060097
3452.039523	699273.922447	46.065101
3450.453602	695801.569190	46.070106
3448.818841	692279.802301	46.075111
3446.727555	688682.312424	46.080116
3445.458666	685035.352811	46.085121
3443.635350	681365.856095	46.090125
3441.830524	677631.654581	46.095130
3439.980073	673829.355673	46.100135
3438.137020	669977.537379	46.105140
3436.335482	666073.555735	46.110145
3434.596448	662130.089489	46.115149
3432.453082	658138.046605	46.120154
3430.480770	654084.801738	46.125159
3428.465453	649989.675565	46.130164
3426.462419	645830.327901	46.135169
3424.296703	641657.298255	46.140173
3422.184374	637410.407701	46.145178
3420.347598	633102.315862	46.150183
3417.984320	628767.657819	46.155188
3416.311481	624380.621880	46.160193
3413.829607	619938.858675	46.165197
3411.568790	615452.334817	46.170202
3409.434420	610915.167655	46.175207
3407.042611	606355.186069	46.180212
3404.811908	601735.220232	46.185217
3402.481181	597073.197810	46.190221
3400.260126	592363.635654	46.195226
3397.571099	587611.225202	46.200231
3394.968629	582813.590997	46.205236
3393.025341	577973.583489	46.210241
3390.649494	573096.396186	46.215245
3388.290136	568167.596323	46.220250
3386.087694	563198.162568	46.225255
3383.414591	558184.557773	46.230260
3380.748501	553134.549128	46.235265
3378.297190	548036.853258	46.240269
3375.268024	542902.981581	46.245274
3373.000315	537722.215381	46.250279
3370.145198	532500.415806	46.255284
3367.614188	527237.527190	46.260289
3364.990483	521954.674622	46.265293
3361.959274	516624.998470	46.270298
3359.480573	511247.573833	46.275303
3356.583039	505857.943917	46.280308
3353.869700	500424.934395	46.285313
3350.821301	494938.966967	46.290317
3347.960531	489425.908637	46.295322
3345.278016	483879.754436	46.300327
3342.154778	478300.011874	46.305332
3339.269427	472683.746448	46.310337
3336.586855	467039.691746	46.315341
3333.589154	461361.264611	46.320346
3331.083809	455653.571089	46.325351
3327.541949	449898.274923	46.330356
3324.710145	444117.467346	46.335361
3321.597308	438303.932621	46.340365
3318.433036	432466.843095	46.345370
3315.660377	426595.853237	46.350375
3312.261494	420711.467114	46.355380
3309.355784	414776.772086	46.360385
3306.187384	408829.653772	46.365389
3302.776196	402854.478646	46.370394
3299.783205	396853.866572	46.375399
3296.606178	390808.258460	46.380404
3293.275435	384749.833614	46.385409
3290.158965	378669.070693	46.390413
3286.521205	372568.016343	46.395418
3283.453902	366425.935703	46.400423
3280.032240	360273.695297	46.405428
3276.458016	354090.707721	46.410433
3273.020706	347901.091197	46.415437
3269.416294	341682.455991	46.420442
3266.192120	335436.516001	46.425447
3262.564683	329190.736512	46.430452
3259.299949	322926.621130	46.435457
3255.751080	316646.775257	46.440461
3251.827656	310345.821697	46.445466
3248.447765	304024.530986	46.450471
3244.707474	297711.603599	46.455476
3241.274046	291362.275839	46.460481
3237.467959	285021.078844	46.465485
3233.795159	278663.747905	46.470490
3230.404620	272277.814970	46.475495
3226.441748	265902.550645	46.480500
3222.895481	259501.563448	46.485505
3218.808093	253105.331122	46.490509
3215.324999	246692.004814	46.495514
3211.808786	240282.841580	46.500519
3207.423805	233832.815280	46.505524
3203.715211	227409.478172	46.510529
3199.914259	220961.632631	46.515533
3195.597459	214515.261971	46.520538
3191.962954	208007.029915	46.525543
3187.714453	201566.493122	46.530548
3183.733691	195120.052296	46.535553
3179.663254	188681.501750	46.540557
3175.149451	182236.507507	46.545562
3171.308714	175815.094727	46.550567
3167.004756	169395.905925	46.555572
3162.579100	162989.658919	46.560577
3158.256443	156578.024512	46.565581
3153.728847	150185.928766	46.570586
3149.744733	143792.962210	46.575591
3145.371109	137441.098519	46.580596
3140.485695	131069.970821	46.585601
3136.001710	124737.594400	46.590605
3131.314794	118425.041130	46.595610
3126.655763	112123.953663	46.600615
3121.495262	105849.850258	46.605620
3116.631455	99608.621327	46.610625
3111.504684	93398.073871	46.615629
3106.055041	87234.025723	46.620634
3100.403455	81103.123646	46.625639
3094.085078	75031.668196	46.630644
3087.339809	69030.479760	46.635649
3074.843746	63231.490450	46.640653
3057.148779	57699.432663	46.645658
3040.270249	52365.676958	46.650663
3023.509374	47246.033095	46.655668
3007.548238	42385.160760	46.660673
2992.013369	37822.072735	46.665677
2977.092334	33548.381877	46.670682
2962.923420	29555.750872	46.675687
2949.079550	25863.905387	46.680692
2935.180386	22462.678800	46.685697
2920.358901	19364.182176	46.690701
2902.481525	16664.379941	46.695706
2883.344866	14314.866682	46.700711
2864.561406	12313.983468	46.705716
2847.055465	10629.849086	46.710721
2832.799456	9251.105827	46.715725
2820.503779	8142.196917	46.720730
2810.722506	7250.599996	46.725735
2803.040638	6577.247974	46.730740
2797.298389	6070.024052	46.735745
2792.368710	5691.320000	46.740749
2788.923937	5417.206980	46.745754
2786.126555	5208.929831	46.750759
2783.855835	5061.088500	46.755764
2782.188527	4942.507390	46.760769
2780.879885	4842.256650	46.765773
2779.879113	4762.755865	46.770778
2778.699144	4673.341178	46.775783
2777.434250	4592.880152	46.780788
2776.084749	4474.876659	46.785793
2774.707119	4364.271099	46.790797
2773.251946	4246.741496	46.795802
2771.338811	4103.841782	46.800807
2769.496517	3950.766464	46.805812
2767.434176	3761.009455	46.810817
2765.448331	3587.586960	46.815821
2763.044329	3395.199485	46.820826
2760.812413	3187.486808	46.825831
2758.041116	2979.831488	46.830836
2755.418215	2745.935384	46.835841
2752.906273	2518.697685	46.840845
2749.353277	2279.683635	46.845850
2746.751577	2030.634654	46.850855
2743.471843	1788.993975	46.855860
2740.191463	1530.285342	46.860865
2736.888866	1289.781845	46.865869
2733.584476	1040.511626	46.870874
2730.179978	793.428203	46.875879
2726.350035	549.716772	46.880884
2721.953128	314.576454	46.885889
2716.169548	140.645437	46.890893
2702.224376	229.027138	46.895898
2694.310746	220.366563	46.900903
2689.984488	217.581496	46.905908
2687.692789	204.389857	46.910913
2686.391099	210.308824	46.915917
2684.525464	221.574328	46.920922
2682.375164	219.658224	46.925927
2679.867393	215.298448	46.930932
2676.562937	207.641594	46.935937
2673.133939	213.806832	46.940941
2669.234212	224.053908	46.945946
2666.157173	205.751728	46.950951
2662.618020	206.902780	46.955956
2659.379388	204.246915	46.960961
2656.347904	206.867863	46.965965
2653.082765	222.921528	46.970970
2649.578225	219.603397	46.975975
2646.171014	218.841486	46.980980
2642.580498	217.028289	46.985985
2639.418164	213.918742	46.990989
2636.003807	214.630219	46.995994
2633.152156	199.766500	47.000999
2629.581694	210.199232	47.006004
2625.779948	211.044835	47.011009
2622.535980	199.628269	47.016013
2619.006886	202.971878	47.021018
2616.023834	198.194140	47.026023
2612.620943	198.850165	47.031028
2608.984901	203.940231	47.036033
2605.026242	201.571724	47.041037
2601.892765	205.958454	47.046042
2599.095170	193.341212	47.051047
2595.802342	206.397024	47.056052
2592.400661	202.134759	47.061057
2587.960215	198.525240	47.066061
2584.888037	199.162953	47.071066
2581.707254	198.450163	47.076071
2578.224922	205.746682	47.081076
2574.526655	204.083097	47.086081
2570.613930	191.080579	47.091085
2567.931095	200.228726	47.096090
2564.223452	197.947207	47.101095
2560.220048	198.456711	47.106100
2556.906424	200.361479	47.111105
2553.706612	192.304739	47.116109
2550.500753	193.576003	47.121114
2547.641698	194.738876	47.126119
2544.051040	193.414219	47.131124
2540.335831	201.129287	47.136129
2536.739706	194.139698	47.141133
2532.965208	196.116821	47.146138
2529.396544	193.567136	47.151143
2526.083112	194.106235	47.156148
2523.114032	195.036566	47.161153
2519.819073	187.414741	47.166157
2516.059333	201.201186	47.171162
2512.452809	189.886897	47.176167
2508.591295	192.915195	47.181172
2505.534338	177.076625	47.186177
2502.259062	190.739668	47.191181
2498.218075	190.305703	47.196186
2495.254762	183.128126	47.201191
2491.796799	190.316073	47.206196
2488.013347	184.020103	47.211201
2484.284279	190.439705	47.216205
2480.949923	190.248344	47.221210
2477.575007	177.595951	47.226215
2474.120675	188.309894	47.231220
2470.638993	184.391101	47.236225
2467.637354	192.680916	47.241229
2463.824170	189.394148	47.246234
2460.117514	183.049224	47.251239
2456.671917	182.795614	47.256244
2453.509430	182.659783	47.261249
2449.780115	183.662925	47.266253
2446.110843	193.919818	47.271258
2443.011451	187.771724	47.276263
2439.327634	179.834625	47.281268
2436.010588	176.427975	47.286273
2432.882619	179.346191	47.291277
2428.874082	193.275702	47.296282
2425.866916	186.619207	47.301287
2421.993272	181.836395	47.306292
2418.185779	189.012555	47.311297
2414.910393	184.867382	47.316301
2411.111320	188.277206	47.321306
2408.111262	178.846624	47.326311
2404.831190	193.430587	47.331316
2401.405773	187.841021	47.336321
2398.116493	181.710650	47.341325
2393.710295	184.996452	47.346330
2390.427672	174.241112	47.351335
2387.477999	174.344684	47.356340
2383.854029	176.954519	47.361345
2380.257907	174.379941	47.366349
2376.305158	182.252632	47.371354
2372.872194	182.145755	47.376359
2369.616240	185.740894	47.381364
2366.078337	182.106291	47.386369
2362.774911	183.284407	47.391373
2359.343313	181.769932	47.396378
2355.916903	168.410335	47.401383
2352.472362	170.252225	47.406388
2348.777480	178.652453	47.411393
2345.270456	171.790947	47.416397
2341.674351	180.750468	47.421402
2338.238981	170.916475	47.426407
2334.596169	185.508478	47.431412
2331.241134	180.913375	47.436417
2327.805900	179.046512	47.441421
2324.215842	176.850109	47.446426
2320.730349	171.771393	47.451431
2316.971956	172.466052	47.456436
2313.864844	175.708719	47.461441
2310.555849	170.431699	47.466445
2306.710995	177.635570	47.471450
2303.597250	167.311494	47.476455
2300.091100	175.009630	47.481460
2296.298705	179.336234	47.486465
2293.002969	170.746913	47.491469
2289.197703	179.038495	47.496474
2286.008405	168.623097	47.501479
2282.785750	170.292272	47.506484
2279.245729	173.633581	47.511489
2275.444919	172.613057	47.516493
2271.623639	177.177272	47.521498
2268.251848	163.064142	47.526503
2264.693665	162.515256	47.531508
2260.828337	166.031773	47.536513
2257.922518	171.323268	47.541517
2254.580749	173.032917	47.546522
2251.299669	165.076472	47.551527
2247.683547	155.913046	47.556532
2243.858416	170.372151	47.561537
2240.248638	165.387973	47.566541
2236.945864	168.739104	47.571546
2233.457679	168.234331	47.576551
2229.929581	160.637114	47.581556
2226.183631	171.789526	47.586561
2223.169417	157.682860	47.591565
2219.301543	164.233688	47.596570
2215.828217	155.794862	47.601575
2212.467711	155.512038	47.606580
2209.144036	161.541771	47.611585
2205.491140	167.678099	47.616589
2201.804927	169.830243	47.621594
2198.305367	157.164059	47.626599
2194.793566	159.783002	47.631604
2191.549673	166.759242	47.636609
2188.284374	158.761359	47.641613
2184.756588	178.724186	47.646618
2181.271192	158.582528	47.651623
2177.548673	156.088001	47.656628
2173.602018	161.264498	47.661633
2170.339341	158.820311	47.666637
2166.822781	161.686403	47.671642
2163.874411	143.753872	47.676647
2160.118050	145.794772	47.681652
2156.512473	153.031647	47.686657
2153.399490	158.210440	47.691661
2149.670851	157.276246	47.696666
2145.848789	156.840203	47.701671
2142.460591	153.852404	47.706676
2138.679652	160.129749	47.711681
2135.646309	156.315852	47.716685
2132.313924	158.863692	47.721690
2128.771282	159.008744	47.726695
2125.173565	165.101670	47.731700
2121.343626	159.310634	47.736705
2118.058919	147.709707	47.741709
2114.418170	164.091000	47.746714
2110.900461	159.755683	47.751719
2107.586100	165.233599	47.756724
2104.052572	154.208946	47.761729
2100.810157	144.562892	47.766733
2096.884595	155.385555	47.771738
2093.457082	151.807477	47.776743
2089.753409	155.396365	47.781748
2086.248905	146.489491	47.786753
2083.353223	151.943535	47.791757
2079.632412	153.561974	47.796762
2076.230933	151.552138	47.801767
2072.744994	144.576224	47.806772
2069.208970	155.402914	47.811777
2065.799560	139.263363	47.816781
2062.092432	155.501113	47.821786
2058.415735	148.885208	47.826791
2054.849619	146.836834	47.831796
2051.194569	151.965578	47.836801
2047.954451	144.523019	47.841805
2044.385307	153.746644	47.846810
2041.470626	160.595523	47.851815
2037.780421	153.511449	47.856820
2034.062373	153.910622	47.861825
2030.723453	147.287157	47.866829
2027.060274	150.432827	47.871834
2023.459679	141.101924	47.876839
2019.823527	144.727553	47.881844
2016.000363	152.564906	47.886849
2013.317039	144.004855	47.891853
2009.660427	147.552076	47.896858
2006.144147	141.703254	47.901863
2002.708498	140.626288	47.906868
1998.832607	152.076257	47.911873
1995.507864	149.871578	47.916877
1992.015355	149.943211	47.921882
1988.441039	148.227027	47.926887
1985.124155	147.509721	47.931892
1981.616371	134.626812	47.936897
1977.995937	139.312421	47.941901
1974.508414	143.428452	47.946906
1971.161941	137.312094	47.951911
1967.522546	138.576585	47.956916
1963.764606	143.231512	47.961921
1960.796651	138.582913	47.966925
1957.161484	151.417228	47.971930
1953.344232	139.016131	47.976935
1950.014335	142.369482	47.981940
1946.476235	148.421861	47.986945
1943.074851	142.475290	47.991949
1939.371600	148.982604	47.996954
1936.107159	139.067288	48.001959
1932.719132	143.115323	48.006964
1929.331458	142.529297	48.011969
1925.689237	139.402280	48.016973
1922.275465	140.255358	48.021978
1918.561603	136.065179	48.026983
1915.145133	144.433349	48.031988
1911.332297	144.520575	48.036993
1907.879744	138.262516	48.041997
1904.198569	150.784884	48.047002
1900.987873	144.773823	48.052007
1898.091634	139.180898	48.057012
1893.763323	134.544056	48.062017
1890.550856	135.002944	48.067021
1886.922542	142.174419	48.072026
1883.314429	140.656842	48.077031
1879.789696	147.546234	48.082036
1876.525269	144.877437	48.087041
1873.600665	126.946997	48.092045
1869.582549	139.302879	48.097050
1865.837563	144.624128	48.102055
1862.521420	144.637819	48.107060
1858.969622	139.943523	48.112065
1855.653303	134.531313	48.117069
1852.149114	129.322459	48.122074
1848.311215	142.184137	48.127079
1845.173213	135.053474	48.132084
1841.308586	145.190668	48.137089
1838.014546	134.641281	48.142093
1834.558189	142.346761	48.147098
1830.949762	130.793208	48.152103
1827.750655	135.382829	48.157108
1823.846487	138.616795	48.162113
1820.890913	124.174547	48.167117
1816.708142	141.409058	48.172122
1813.566748	144.440421	48.177127
1810.106048	137.673595	48.182132
1806.406997	135.071117	48.187137
1802.857060	142.037409	48.192141
1799.434742	141.531352	48.197146
1795.768019	136.168305	48.202151
1792.527209	132.081480	48.207156
1788.826598	145.159484	48.212161
1785.632292	137.597530	48.217165
1781.974133	139.987549	48.222170
1778.498484	131.327286	48.227175
1775.431740	133.043066	48.232180
1771.462466	137.571546	48.237185
1767.984115	129.604912	48.242189
1764.165180	132.825830	48.247194
1760.904119	124.631065	48.252199
1757.711016	138.312985	48.257204
1753.876315	140.051403	48.262209
1750.429141	136.999342	48.267213
1746.879396	141.713941	48.272218
1743.558697	141.863798	48.277223
1740.139998	141.561691	48.282228
1736.213817	131.110652	48.287233
1733.106175	130.874233	48.292237
1729.239225	136.190311	48.297242
1725.703299	134.614141	48.302247
1722.543076	128.134214	48.307252
1718.543376	128.127178	48.312257
1715.122437	129.441382	48.317261
1711.793117	142.734193	48.322266
1708.803129	142.143128	48.327271
1705.268518	132.094448	48.332276
1701.587973	124.842258	48.337281
1698.017888	120.594742	48.342285
1694.501274	133.047696	48.347290
1690.940454	132.532679	48.352295
1687.451153	133.850284	48.357300
1683.670865	133.562389	48.362305
1680.214842	133.632296	48.367309
1676.700023	137.046171	48.372314
1673.291469	145.440357	48.377319
1670.110107	136.953279	48.382324
1666.202760	136.879238	48.387329
1663.124718	128.086741	48.392333
1659.593217	136.909366	48.397338
1655.863456	143.161608	48.402343
1652.668044	133.723917	48.407348
1648.773087	136.707437	48.412353
1645.068121	125.698449	48.417357
1641.812653	130.255810	48.422362
1638.453884	125.728287	48.427367
1635.123513	129.552844	48.432372
1631.358966	123.745796	48.437377
1627.802508	129.303701	48.442381
1624.107088	140.635244	48.447386
1620.686367	135.804907	48.452391
1617.733706	134.326012	48.457396
1613.378604	134.818391	48.462401
1610.432253	122.674076	48.467405
1607.256102	135.106989	48.472410
1603.684232	121.754535	48.477415
1600.057133	135.685902	48.482420
1596.151764	136.854373	48.487425
1592.838236	130.756066	48.492429
1589.208826	124.211173	48.497434
1585.512639	126.316618	48.502439
1582.483049	119.775646	48.507444
1578.860468	145.777923	48.512449
1575.403181	129.169982	48.517453
1571.468014	134.290212	48.522458
1568.230110	130.272377	48.527463
1564.871328	132.440641	48.532468
1561.490944	135.566695	48.537473
1558.067341	124.923525	48.542477
1554.602307	124.285134	48.547482
1550.613034	132.813477	48.552487
1546.883220	126.642124	48.557492
1543.713396	132.237484	48.562497
1540.228672	122.424955	48.567501
1537.068706	125.333111	48.572506
1533.359030	126.492899	48.577511
1529.834185	131.833022	48.582516
1526.053559	131.777017	48.587521
1522.910716	121.188562	48.592525
1519.354287	126.903179	48.597530
1515.748943	122.682694	48.602535
1512.268327	120.184820	48.607540
1508.475629	140.110504	48.612545
1505.545064	129.034375	48.617549
1501.950095	136.305680	48.622554
1498.329211	117.548400	48.627559
1494.980424	128.039531	48.632564
1490.953127	135.941287	48.637569
1487.712002	132.658831	48.642573
1484.437991	132.476123	48.647578
1480.939154	136.630346	48.652583
1477.263876	114.144492	48.657588
1473.260868	121.401554	48.662593
1470.035394	118.621362	48.667597
1466.628117	128.130642	48.672602
1463.239971	130.790183	48.677607
1459.953178	114.301494	48.682612
1456.313720	126.027567	48.687617
1453.264413	123.970082	48.692621
1449.220327	131.631237	48.697626
1445.542982	132.974468	48.702631
1442.315283	125.881612	48.707636
1438.620421	128.408084	48.712641
1435.226905	119.585401	48.717645
1431.759133	123.410622	48.722650
1428.342531	130.302971	48.727655
1424.699554	129.199736	48.732660
1420.882943	126.009436	48.737665
1417.648422	127.116709	48.742669
1414.010250	132.492656	48.747674
1410.589263	130.545469	48.752679
1407.575296	122.443305	48.757684
1403.697116	135.105215	48.762689
1400.071571	128.052196	48.767693
1396.813029	128.501053	48.772698
1393.488726	122.871781	48.777703
1389.840009	117.718117	48.782708
1385.912996	125.200349	48.787713
1382.543409	112.921703	48.792717
1378.876866	119.441747	48.797722
1375.673880	119.427616	48.802727
1372.361313	114.946479	48.807732
1368.684128	120.705263	48.812737
1365.070130	126.744466	48.817741
1361.691102	127.761863	48.822746
1357.878867	128.193209	48.827751
1354.667078	118.861001	48.832756
1351.125590	131.698019	48.837761
1347.629266	118.010556	48.842765
1344.138304	118.888683	48.847770
1340.455471	118.739091	48.852775
1337.065367	129.694382	48.857780
1333.426577	122.993434	48.862785
1330.131196	108.054692	48.867789
1326.951298	109.755987	48.872794
1323.389449	114.578530	48.877799
1319.700294	115.419138	48.882804
1315.970114	127.584275	48.887809
1312.739795	120.718936	48.892813
1309.114729	119.858762	48.897818
1305.619448	119.833125	48.902823
1302.245214	114.821360	48.907828
1298.749468	122.695448	48.912833
1295.090433	118.935410	48.917837
1291.790434	112.640782	48.922842
1287.933684	117.229266	48.927847
1284.658641	117.757950	48.932852
1280.587008	129.258276	48.937857
1277.512776	122.215948	48.942861
1274.265710	121.382879	48.947866
1270.556265	109.604169	48.952871
1267.146822	112.516917	48.957876
1263.269296	120.155106	48.962881
1260.342499	118.910161	48.967885
1256.653003	126.757746	48.972890
1253.047188	139.040904	48.977895
1249.702505	130.302606	48.982900
1245.746432	124.497019	48.987905
1242.253908	124.520484	48.992909
1239.211838	114.343736	48.997914
1235.725032	122.287408	49.002919
1232.165657	115.136952	49.007924
1228.249948	122.349340	49.012929
1224.806517	117.593415	49.017933
1221.625755	113.834086	49.022938
1218.194620	123.734138	49.027943
1214.680804	124.235775	49.032948
1210.883625	128.016226	49.037953
1207.528612	129.717083	49.042957
1203.765374	127.603140	49.047962
1200.431366	114.708631	49.052967
1197.428002	114.362893	49.057972
1193.456607	122.630264	49.062977
1190.037585	124.483862	49.067981
1186.505255	113.091316	49.072986
1182.853836	129.344814	49.077991
1179.694377	110.517816	49.082996
1175.959791	128.848473	49.088001
1172.715650	118.869383	49.093005
1168.609396	117.593458	49.098010
1165.172480	117.902177	49.103015
1162.089545	113.367754	49.108020
1158.421732	124.072387	49.113025
1155.160710	119.926874	49.118029
1151.605638	114.348560	49.123034
1147.807138	114.002205	49.128039
1144.496087	113.858331	49.133044
1140.948081	111.710572	49.138049
1137.718129	116.055759	49.143053
1133.890067	117.281373	49.148058
1130.086847	114.871787	49.153063
1127.055731	110.788376	49.158068
1123.285214	113.321083	49.163073
1120.433518	121.423468	49.168077
1116.330930	120.137795	49.173082
1112.271773	117.570492	49.178087
1109.485943	114.444122	49.183092
1105.706998	115.228140	49.188097
1102.580541	119.622753	49.193101
1099.238674	115.450562	49.198106
1095.600707	113.098067	49.203111
1092.222158	109.485802	49.208116
1088.375544	120.579392	49.213121
1085.152723	118.473377	49.218125
1081.551204	122.655981	49.223130
1077.611945	123.272422	49.228135
1074.210702	109.786989	49.233140
1070.559103	111.862643	49.238145
1067.604453	106.958236	49.243149
1063.987616	113.549932	49.248154
1060.229301	111.364030	49.253159
1057.029365	114.208645	49.258164
1053.234139	104.940978	49.263169
1049.782145	100.382701	49.268173
1046.419444	105.231390	49.273178
1042.703467	119.710376	49.278183
1039.134488	115.549373	49.283188
1036.186791	106.851727	49.288193
1032.658233	108.566125	49.293197
1028.962267	114.667748	49.298202
1025.329555	125.821456	49.303207
1022.189430	111.537816	49.308212
1018.144064	107.589064	49.313217
1014.689506	112.297352	49.318221
1011.433769	118.317619	49.323226
1007.568944	128.882393	49.328231
1004.242575	115.047722	49.333236
1000.883662	113.236712	49.338241
997.565635	114.391706	49.343245
994.263025	119.717771	49.348250
990.528969	118.662664	49.353255
986.919116	118.047092	49.358260
983.141884	111.740764	49.363265
979.748151	106.512392	49.368269
976.238501	113.548939	49.373274
972.710545	121.799042	49.378279
969.522156	117.273641	49.383284
965.793715	121.989094	49.388289
962.239503	106.979179	49.393293
958.982925	101.316970	49.398298
955.051837	110.418064	49.403303
951.726396	111.776947	49.408308
948.047787	111.495952	49.413313
944.706854	121.293116	49.418317
941.292777	120.436582	49.423322
937.607253	122.145968	49.428327
934.150996	109.228803	49.433332
930.647556	121.877174	49.438337
927.441566	104.450983	49.443341
924.123146	110.724726	49.448346
920.311117	120.877013	49.453351
916.568310	111.587556	49.458356
912.905440	108.310712	49.463361
909.868383	106.910197	49.468365
905.993149	114.040290	49.473370
902.793749	106.081589	49.478375
899.515693	108.511492	49.483380
895.740469	111.978891	49.488385
892.437127	118.127726	49.493389
888.828927	115.842452	49.498394
885.181061	120.379290	49.503399
882.073811	112.389891	49.508404
878.124298	118.206209	49.513409
874.285387	116.903883	49.518413
871.235533	116.836783	49.523418
867.729823	124.579613	49.528423
864.434591	103.535728	49.533428
860.445568	112.912121	49.538433
857.383660	111.597915	49.543437
853.538368	118.416070	49.548442
850.036484	119.139186	49.553447
846.893662	119.834582	49.558452
843.228277	110.252006	49.563457
839.963569	104.739682	49.568461
836.067919	119.035319	49.573466
832.748355	127.918887	49.578471
829.358748	119.284551	49.583476
825.595366	118.819222	49.588481
821.990404	114.374923	49.593485
818.634277	114.956584	49.598490
814.874708	117.399745	49.603495
811.579109	111.100809	49.608500
807.840250	115.092731	49.613505
804.687944	111.123610	49.618509
801.212454	127.519363	49.623514
797.594462	127.721235	49.628519
794.287374	115.291457	49.633524
790.859349	116.011483	49.638529
787.304435	111.187496	49.643533
783.772961	105.732082	49.648538
780.008262	111.807292	49.653543
776.712362	116.265341	49.658548
772.978433	122.579949	49.663553
769.596752	121.018378	49.668557
766.204160	112.053877	49.673562
762.455001	108.620891	49.678567
759.338223	111.518400	49.683572
755.441149	123.344227	49.688577
751.853350	121.545987	49.693581
748.385976	104.496939	49.698586
745.074538	110.020994	49.703591
741.834435	98.712590	49.708596
738.297056	108.098608	49.713601
734.831528	111.254590	49.718605
731.103739	104.509226	49.723610
727.529050	116.294841	49.728615
723.934625	107.314373	49.733620
720.095919	111.843740	49.738625
716.813211	108.294876	49.743629
713.546044	102.279285	49.748634
710.023770	106.633076	49.753639
707.014847	110.119439	49.758644
702.916809	108.849948	49.763649
699.586430	111.399082	49.768653
696.017311	115.731514	49.773658
692.584586	106.827458	49.778663
689.341575	99.341056	49.783668
685.712671	108.095909	49.788673
681.816579	116.304629	49.793677
678.547077	114.991053	49.798682
674.772725	117.226689	49.803687
671.813679	113.651820	49.808692
667.828012	118.899049	49.813697
664.542028	115.899386	49.818701
661.156965	111.633741	49.823706
657.171482	120.498808	49.828711
654.033019	111.094914	49.833716
650.658105	101.692393	49.838721
646.932902	104.200113	49.843725
643.163810	102.238019	49.848730
639.487180	111.609690	49.853735
636.788584	110.914445	49.858740
633.109784	107.129648	49.863745
629.508047	112.858665	49.868749
626.173052	114.626936	49.873754
622.683609	120.451953	49.878759
618.853768	109.362960	49.883764
615.407859	103.721555	49.888769
611.939002	106.060772	49.893773
608.603623	106.205907	49.898778
604.642798	113.809539	49.903783
601.203360	108.881547	49.908788
597.751756	103.122212	49.913793
594.306594	100.352213	49.918797
591.186491	94.967487	49.923802
587.606521	105.061858	49.928807
584.122687	108.216695	49.933812
580.579076	106.177044	49.938817
577.177212	111.791977	49.943821
573.570226	115.086438	49.948826
569.787373	107.927228	49.953831
566.286303	105.898613	49.958836
562.659046	114.649407	49.963841
559.128999	113.215649	49.968845
555.804696	113.016740	49.973850
552.458519	114.853981	49.978855
548.898451	117.780311	49.983860
545.563137	118.884711	49.988865
541.945570	106.895488	49.993869
538.722797	102.183126	49.998874
534.779893	112.279463	50.003879
531.619158	105.137487	50.008884
527.557036	101.870091	50.013889
523.795833	107.770623	50.018893
521.110319	101.852728	50.023898
517.413203	110.701897	50.028903
514.465791	104.493606	50.033908
511.032314	105.117894	50.038913
506.600450	108.461628	50.043917
503.513805	99.920510	50.048922
499.426420	112.906324	50.053927
496.158149	98.357991	50.058932
492.462604	108.843434	50.063937
489.486312	103.054287	50.068941
486.606777	105.747970	50.073946
482.368213	108.141588	50.078951
478.965357	103.018205	50.083956
475.418305	109.333955	50.088961
471.624138	107.734032	50.093965
468.072506	95.789225	50.098970
464.682440	107.865872	50.103975
461.627903	105.566338	50.108980
457.781086	108.394069	50.113985
453.980725	104.938652	50.118989
450.918866	103.949413	50.123994
447.074100	113.311064	50.128999
443.840314	108.807257	50.134004
440.065244	99.806997	50.139009
437.047761	106.163044	50.144013
433.665662	99.583831	50.149018
429.863085	100.782545	50.154023
426.284347	102.283270	50.159028
422.424949	95.638972	50.164033
418.989053	105.931991	50.169037
415.736719	95.802493	50.174042
412.291503	112.906558	50.179047
409.531409	103.051105	50.184052
405.272789	105.479260	50.189057
401.365171	107.704308	50.194061
398.238763	100.106863	50.199066
394.666857	106.493941	50.204071
391.174127	96.789426	50.209076
387.906505	97.841681	50.214081
384.590162	100.546696	50.219085
380.784570	95.504112	50.224090
377.123734	108.819273	50.229095
373.736633	117.701257	50.234100
370.332510	106.437537	50.239105
366.442928	93.262441	50.244109
363.248208	94.232125	50.249114
359.751302	104.304686	50.254119
356.339531	99.619504	50.259124
352.619365	104.204759	50.264129
349.123824	98.473945	50.269133
345.991086	98.409339	50.274138
342.093422	98.007024	50.279143
338.703448	100.791411	50.284148
334.986590	105.424076	50.289153
331.772120	108.448905	50.294157
328.267730	99.197020	50.299162
324.382115	109.601277	50.304167
321.134873	102.495417	50.309172
317.746777	104.987185	50.314177
314.198741	107.013672	50.319181
310.790212	104.558710	50.324186
306.891021	99.066568	50.329191
303.474590	94.107429	50.334196
300.073102	92.816745	50.339201
296.581410	97.917253	50.344205
293.291695	102.924608	50.349210
289.316660	107.184015	50.354215
286.115240	103.252092	50.359220
283.030496	109.565053	50.364225
279.219033	106.646893	50.369229
275.902094	103.246978	50.374234
272.049414	110.940453	50.379239
268.679411	100.285601	50.384244
265.072008	111.065285	50.389249
261.900659	100.606599	50.394253
258.223893	96.569334	50.399258
254.496853	100.452945	50.404263
251.160606	102.761951	50.409268
247.737571	106.639340	50.414273
243.782795	109.619400	50.419277
240.566725	94.048326	50.424282
237.022293	102.009941	50.429287
233.995030	95.740212	50.434292
230.166932	95.426214	50.439297
226.292148	98.895525	50.444301
223.235219	93.465834	50.449306
219.482114	102.235404	50.454311
216.083445	91.566979	50.459316
212.592449	95.683411	50.464321
208.796390	95.471076	50.469325
205.616997	90.181399	50.474330
201.762813	100.023008	50.479335
198.601651	95.418156	50.484340
194.745143	98.483919	50.489345
191.742924	90.550968	50.494349
187.979920	95.578166	50.499354
184.689098	104.506766	50.504359
181.449262	92.806412	50.509364
177.751806	89.561772	50.514369
174.290572	97.046869	50.519373
170.866876	91.513052	50.524378
167.063143	102.436204	50.529383
163.307673	98.160131	50.534388
159.784011	96.586242	50.539393
156.033237	99.490518	50.544397
153.008090	89.347226	50.549402
149.471911	96.210751	50.554407
146.020597	90.821901	50.559412
142.815050	101.414477	50.564417
139.154523	94.587158	50.569421
135.889593	89.353879	50.574426
131.668902	94.065069	50.579431
128.076866	100.039567	50.584436
125.023266	94.822674	50.589441
121.256287	95.042339	50.594445
118.193197	98.325891	50.599450
114.538889	100.127251	50.604455
111.054378	85.792797	50.609460
107.382878	93.127983	50.614465
103.398195	95.975243	50.619469
100.296860	84.602292	50.624474
96.905961	94.224244	50.629479
93.669945	95.262249	50.634484
90.174587	99.298862	50.639489
86.174083	95.135448	50.644493
82.960397	92.338046	50.649498
79.588036	90.997584	50.654503
76.046515	91.376346	50.659508
72.576928	106.070328	50.664513
68.971366	89.133118	50.669517
65.416490	79.768807	50.674522
61.661723	94.786542	50.679527
58.521993	87.871342	50.684532
55.058583	89.922951	50.689537
51.091347	95.022351	50.694541
48.058056	93.069846	50.699546
44.137084	91.821839	50.704551
41.063522	103.532621	50.709556
37.793184	93.432576	50.714561
33.843740	95.486579	50.719565
30.494342	83.504617	50.724570
26.734555	92.633604	50.729575
23.340994	91.947710	50.734580
20.139705	83.678683	50.739585
16.158280	84.411347	50.744589
12.978646	86.290887	50.749594
9.627845	100.996928	50.754599
6.025112	96.189508	50.759604
2.246463	89.749199	50.764609