Thu Jun 16 18:04:45 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.126993	104.061779	0.000000
0.005156	103.697721	0.005005
-0.212167	86.600397	0.010010
-0.177432	66.962771	0.015014
-0.363929	81.967359	0.020019
-0.772013	83.019407	0.025024
-0.828886	72.961250	0.030029
-0.843895	65.519251	0.035034
-1.118002	50.547625	0.040038
-1.721668	44.193916	0.045043
-1.652029	32.929525	0.050048
-1.964260	24.993957	0.055053
-1.998089	17.031920	0.060058
-2.705914	9.608350	0.065062
-2.622040	7.725277	0.070067
-2.796273	-16.586451	0.075072
-3.315985	-14.853785	0.080077
-3.693059	-19.617291	0.085082
-4.497712	-22.300422	0.090086
-5.164168	-15.814842	0.095091
-5.306048	-12.567901	0.100096
-5.559661	-7.213360	0.105101
-5.178197	-10.446879	0.110106
-5.476954	-18.368668	0.115110
-5.500738	-15.705257	0.120115
-5.215460	-15.819961	0.125120
-6.209732	-11.636103	0.130125
-6.431316	-27.368483	0.135130
-6.635173	-18.273355	0.140134
-6.973276	-16.987423	0.145139
-6.994452	-18.593372	0.150144
-7.605420	-3.004034	0.155149
-8.468565	-15.937890	0.160154
-8.615529	-9.770097	0.165158
-8.677230	-12.508033	0.170163
-8.252944	-30.225450	0.175168
-8.593240	-13.486135	0.180173
-8.570757	-4.353326	0.185178
-8.478344	-12.477880	0.190182
-9.006453	-9.801565	0.195187
-9.374522	-20.212623	0.200192
-10.080667	-20.881699	0.205197
-10.742720	-29.009914	0.210202
-11.084887	-16.448355	0.215206
-11.109099	-10.901662	0.220211
-10.737343	-12.207619	0.225216
-11.115766	-26.068331	0.230221
-11.571069	-22.664331	0.235226
-11.208651	-26.732284	0.240230
-11.594613	-26.615898	0.245235
-12.605267	-24.990434	0.250240
-13.161379	-8.896665	0.255245
-12.651201	-24.049620	0.260250
-12.632095	-14.905704	0.265254
-12.788331	-16.059491	0.270259
-12.898315	-24.760381	0.275264
-13.888591	-22.094113	0.280269
-13.903984	-20.657097	0.285274
-13.910792	-21.380084	0.290278
-14.820970	-14.048704	0.295283
-15.275174	-26.012568	0.300288
-15.611019	-15.996974	0.305293
-15.532922	-13.922701	0.310298
-15.574924	-17.152238	0.315302
-15.860543	-15.281861	0.320307
-15.656856	-13.352353	0.325312
-16.003706	-11.225809	0.330317
-15.994199	-8.275583	0.335322
-16.792862	-14.200838	0.340326
-17.327376	-7.841635	0.345331
-17.390686	-13.878153	0.350336
-17.670268	-8.071031	0.355341
-17.638341	-15.162527	0.360346
-17.371228	-18.092328	0.365350
-18.429808	-8.880312	0.370355
-18.799693	-12.361003	0.375360
-19.330419	-25.449623	0.380365
-19.335461	-19.595730	0.385370
-19.376539	-15.610930	0.390374
-19.581530	-17.854301	0.395379
-19.021647	-22.529065	0.400384
-20.204586	-12.784872	0.405389
-20.772506	-9.708736	0.410394
-20.755368	-18.320044	0.415398
-21.131817	-13.760891	0.420403
-20.888555	-16.931515	0.425408
-20.975413	-6.109117	0.430413
-21.248897	0.676357	0.435418
-21.867483	-13.905015	0.440422
-22.305508	-19.089572	0.445427
-22.326181	-27.835308	0.450432
-22.391742	-12.912855	0.455437
-22.586921	-6.729004	0.460442
-22.775393	-12.941657	0.465446
-23.644369	-16.920455	0.470451
-24.087746	-20.050117	0.475456
-24.276157	-19.651567	0.480461
-24.295258	-10.999250	0.485466
-23.878709	-23.752224	0.490470
-24.543665	-9.532979	0.495475
-24.257651	-9.216384	0.500480
-24.913305	-7.813846	0.505485
-25.242968	-14.153713	0.510490
-25.515546	-14.790851	0.515494
-25.754555	-12.056751	0.520499
-25.696663	-3.620286	0.525504
-25.982372	-3.821564	0.530509
-26.841289	-8.979087	0.535514
-27.124015	-14.971649	0.540518
-27.638276	-23.299105	0.545523
-27.588360	-20.643634	0.550528
-27.733488	-15.957067	0.555533
-28.055789	-1.861430	0.560538
-27.655806	-9.625123	0.565542
-27.972406	1.894070	0.570547
-28.006451	-8.919954	0.575552
-28.834336	3.996448	0.580557
-29.089987	-7.923980	0.585562
-29.008813	-12.753646	0.590566
-29.382376	-1.692769	0.595571
-30.051213	-9.952560	0.600576
-30.439172	2.187526	0.605581
-30.923968	-8.339996	0.610586
-30.634814	-13.754631	0.615590
-31.029979	-19.723577	0.620595
-30.763378	-13.934602	0.625600
-30.935427	-14.710982	0.630605
-31.106722	-15.031796	0.635610
-31.744393	-8.616675	0.640614
-32.384610	7.402712	0.645619
-32.466383	-1.913530	0.650624
-32.685501	-0.272861	0.655629
-32.383600	-10.650801	0.660634
-32.687628	-17.210762	0.665638
-33.515024	-10.422247	0.670643
-33.535472	-8.660311	0.675648
-33.982187	-7.648547	0.680653
-34.209968	-7.554650	0.685658
-33.948908	-14.751394	0.690662
-34.693657	-13.233799	0.695667
-34.548517	-7.802205	0.700672
-34.994781	-9.065121	0.705677
-35.330570	-3.861163	0.710682
-35.266548	-15.883840	0.715686
-36.076964	0.285802	0.720691
-36.634317	-21.498173	0.725696
-36.824351	-18.619251	0.730701
-36.715454	-14.420588	0.735706
-36.799897	-12.351419	0.740710
-37.243631	-9.463717	0.745715
-37.062319	-12.588094	0.750720
-36.863732	-7.116401	0.755725
-37.713761	-18.957434	0.760730
-38.096263	-10.593119	0.765734
-38.510850	-14.859710	0.770739
-38.444739	-17.927658	0.775744
-38.113078	-11.527707	0.780749
-39.102558	-9.203901	0.785754
-39.460865	-14.526530	0.790758
-40.210893	-11.991020	0.795763
-40.174231	-22.752889	0.800768
-39.901228	-7.548391	0.805773
-40.181169	-11.027667	0.810778
-40.031285	-17.577599	0.815782
-41.075368	-9.379396	0.820787
-41.431755	-17.924730	0.825792
-41.430342	-2.392696	0.830797
-41.723246	-10.470440	0.835802
-41.568113	-14.129841	0.840806
-41.733049	-3.016626	0.845811
-42.409373	-5.918471	0.850816
-42.818062	-7.621483	0.855821
-43.417681	-13.177706	0.860826
-43.204823	-21.685308	0.865830
-43.205852	-15.852008	0.870835
-43.005854	-16.357403	0.875840
-43.271140	-16.834542	0.880845
-44.471863	-17.842941	0.885850
-44.648671	-13.299517	0.890854
-44.970868	-7.288040	0.895859
-45.205173	-16.424273	0.900864
-44.889107	-15.442577	0.905869
-45.486854	-23.824009	0.910874
-44.900596	-20.745646	0.915878
-45.888952	-19.107091	0.920883
-46.426746	-9.550509	0.925888
-46.769284	-10.990881	0.930893
-46.692767	-3.036173	0.935898
-46.795612	-8.482117	0.940902
-46.957265	-9.354135	0.945907
-46.909918	-21.315449	0.950912
-47.629119	-12.807096	0.955917
-48.342293	-6.726467	0.960922
-48.171440	-9.014490	0.965926
-48.552872	-5.743447	0.970931
-48.387835	-7.512862	0.975936
-48.441380	-14.609962	0.980941
-49.100518	-16.715731	0.985946
-49.440364	-11.699931	0.990950
-49.894446	-13.816109	0.995955
-50.008198	-18.364354	1.000960
-49.902629	-5.946238	1.005965
-49.891738	-15.620908	1.010970
-50.526558	-16.924580	1.015974
-51.438233	-19.462653	1.020979
-51.313773	-16.212177	1.025984
-51.380238	-10.431792	1.030989
-51.653405	-9.473274	1.035994
-51.279061	-11.008937	1.040998
-52.191113	-13.607128	1.046003
-52.442877	-19.239382	1.051008
-52.970792	-16.645376	1.056013
-52.890241	-10.978769	1.061018
-52.960117	-11.511583	1.066022
-53.345248	-7.404612	1.071027
-53.180448	-10.097700	1.076032
-53.919604	-9.269249	1.081037
-54.310124	-9.113631	1.086042
-54.225579	-13.966346	1.091046
-54.677950	-7.172623	1.096051
-54.635488	-12.691610	1.101056
-54.563914	-2.037460	1.106061
-55.508422	-20.180980	1.111066
-55.980077	-14.783602	1.116070
-56.360467	-7.960537	1.121075
-56.032444	-19.706109	1.126080
-56.238369	-11.216680	1.131085
-56.330458	-2.330521	1.136090
-56.818557	-12.521567	1.141094
-57.646710	-16.844705	1.146099
-57.338597	-18.521253	1.151104
-57.495160	-17.202576	1.156109
-57.796618	-6.214884	1.161114
-57.391787	-15.051170	1.166118
-58.548209	-11.902635	1.171123
-58.804982	-18.223071	1.176128
-59.163037	-21.311089	1.181133
-59.170241	-17.285520	1.186138
-58.963892	-24.572070	1.191142
-59.241411	-8.707846	1.196147
-59.828091	-11.453137	1.201152
-59.945370	-17.663147	1.206157
-60.403643	-10.513487	1.211162
-60.475550	-20.404041	1.216166
-60.958880	-20.259327	1.221171
-61.396938	-23.322480	1.226176
-61.581316	-18.127568	1.231181
-62.198303	-12.575056	1.236186
-62.245897	-22.940510	1.241190
-62.256876	-20.211540	1.246195
-62.213908	-16.613648	1.251200
-62.291922	-14.696781	1.256205
-62.668771	-11.304360	1.261210
-63.065289	-14.151222	1.266214
-63.646671	-20.755413	1.271219
-63.603027	-22.009415	1.276224
-63.543400	-23.241493	1.281229
-64.016070	-15.314320	1.286234
-64.772450	-17.976908	1.291238
-65.177518	-10.412020	1.296243
-65.148472	-9.321920	1.301248
-65.072933	-8.191261	1.306253
-65.516055	-14.091409	1.311258
-65.466531	-20.427442	1.316262
-65.637850	-15.237745	1.321267
-65.574649	-10.403489	1.326272
-66.615573	-9.302202	1.331277
-66.976929	-10.232768	1.336282
-66.704318	-22.888649	1.341286
-67.118265	-15.577321	1.346291
-67.141249	-6.458907	1.351296
-67.700692	-10.562649	1.356301
-68.690101	-4.254050	1.361306
-68.434445	-18.013063	1.366310
-68.506672	-10.190444	1.371315
-68.807882	-26.339988	1.376320
-68.582653	-20.470092	1.381325
-68.988547	-20.888772	1.386330
-68.752537	-30.396813	1.391334
-69.376254	-14.607974	1.396339
-69.689163	-14.624609	1.401344
-70.222185	-19.200047	1.406349
-70.560858	-20.361169	1.411354
-70.655517	-20.646602	1.416358
-71.578577	-22.351518	1.421363
-71.165916	-24.922983	1.426368
-71.699110	-25.721559	1.431373
-72.022158	-13.239917	1.436378
-71.772113	-9.895262	1.441382
-71.972314	-19.935089	1.446387
-72.035357	-21.240617	1.451392
-72.026365	-28.359192	1.456397
-73.103939	-14.401074	1.461402
-73.509732	-12.405174	1.466406
-73.986373	-11.813372	1.471411
-73.769458	-15.363117	1.476416
-73.625454	-9.220625	1.481421
-73.891724	-12.916732	1.486426
-74.297557	-22.019578	1.491430
-74.883671	-15.335263	1.496435
-75.334457	-22.976989	1.501440
-75.350031	-24.765092	1.506445
-75.744803	-2.146074	1.511450
-75.636169	-25.970787	1.516454
-75.524365	-18.881804	1.521459
-75.844272	-9.233572	1.526464
-76.330919	-20.260462	1.531469
-76.927826	-20.494262	1.536474
-76.615665	-21.659752	1.541478
-76.772856	-12.982943	1.546483
-77.348318	-21.787537	1.551488
-78.131342	-19.706504	1.556493
-78.438658	-27.534029	1.561498
-78.263344	-20.362412	1.566502
-78.655318	-17.917842	1.571507
-78.727105	-21.278794	1.576512
-78.482330	-19.212735	1.581517
-78.899135	-19.965730	1.586522
-79.663800	-29.744448	1.591526
-80.081554	-28.098181	1.596531
-80.538056	-21.955303	1.601536
-80.424726	-19.095047	1.606541
-80.656050	-12.261104	1.611546
-80.050273	-20.766064	1.616550
-80.308037	-23.301905	1.621555
-80.812891	-35.423514	1.626560
-81.375468	-22.910087	1.631565
-81.745154	-19.781868	1.636570
-81.749148	-23.167934	1.641574
-82.061163	-27.692879	1.646579
-82.874499	-36.098255	1.651584
-83.050253	-25.117345	1.656589
-83.486267	-20.984702	1.661594
-83.517562	-21.594726	1.666598
-83.696223	-20.878438	1.671603
-83.755812	-13.060179	1.676608
-83.630592	-22.159337	1.681613
-83.774688	-16.093245	1.686618
-83.863430	-21.824751	1.691622
-84.761815	-12.012549	1.696627
-85.103019	-26.834086	1.701632
-85.157949	-25.436412	1.706637
-85.502462	-18.660618	1.711642
-85.182223	-19.652034	1.716646
-85.985967	-7.169671	1.721651
-86.406558	-21.929258	1.726656
-86.326319	-24.425560	1.731661
-86.416135	-13.220888	1.736666
-86.616695	-17.587662	1.741670
-87.418215	-7.188383	1.746675
-87.897889	-12.464410	1.751680
-87.972313	-19.158301	1.756685
-88.384678	-17.672252	1.761690
-88.293252	-5.550929	1.766694
-88.534341	-10.371136	1.771699
-88.288763	-13.371272	1.776704
-88.290658	-15.474375	1.781709
-89.549169	-9.111929	1.786714
-89.715981	-24.106524	1.791718
-89.973636	-16.261847	1.796723
-89.799938	-13.357603	1.801728
-89.518430	-15.310923	1.806733
-90.403056	-13.544678	1.811738
-91.054081	-21.630801	1.816742
-91.353588	-18.613033	1.821747
-91.594204	-24.143338	1.826752
-91.492371	-16.949612	1.831757
-91.925190	-8.376316	1.836762
-91.708655	-16.487931	1.841766
-91.957886	-16.937631	1.846771
-92.009470	-17.097392	1.851776
-92.512013	-17.679256	1.856781
-93.102262	-12.286742	1.861786
-92.791983	-25.953947	1.866790
-93.211536	-11.326284	1.871795
-94.081325	-16.384228	1.876800
-94.465031	-16.207437	1.881805
-94.828027	-8.821557	1.886810
-94.481597	-19.868234	1.891814
-94.436115	-17.540751	1.896819
-94.565208	-19.524669	1.901824
-94.825974	-24.811812	1.906829
-95.703467	-9.575329	1.911834
-95.800988	-21.764562	1.916838
-96.281781	-22.757565	1.921843
-96.240949	-24.547394	1.926848
-96.392030	-24.143271	1.931853
-96.412831	-17.051907	1.936858
-96.787342	-16.447879	1.941862
-97.496335	-7.138153	1.946867
-98.016327	-21.115348	1.951872
-97.642414	-26.300207	1.956877
-98.330839	-11.159593	1.961882
-97.892103	-15.710652	1.966886
-98.248787	-12.456722	1.971891
-98.850136	-23.696193	1.976896
-99.129102	-24.995137	1.981901
-99.482148	-22.466040	1.986906
-99.593307	-24.511227	1.991910
-100.284146	-20.686893	1.996915
-99.922969	-25.219082	2.006912
-99.781509	-27.617730	2.016909
-99.183155	-19.223518	2.026906
-98.659656	-17.778188	2.036902
-98.323148	-23.559951	2.046899
-97.545443	-22.534278	2.056896
-97.097666	-22.891155	2.066893
-97.105100	-20.953368	2.076890
-96.176065	-14.851017	2.086886
-95.335896	-25.757155	2.096883
-95.481801	-22.192266	2.106880
-94.467767	-5.969432	2.116877
-93.896060	-19.433813	2.126874
-94.182002	-16.661421	2.136870
-93.214692	-19.035841	2.146867
-92.572821	-18.109021	2.156864
-92.336646	-23.197349	2.166861
-91.933817	-13.541972	2.176858
-91.254340	-7.644042	2.186854
-90.599473	-15.540693	2.196851
-89.806216	-15.673535	2.206848
-89.399096	-11.551539	2.216845
-89.343869	-16.749048	2.226842
-89.356390	-21.154784	2.236838
-88.204735	-16.063707	2.246835
-87.629473	-24.345980	2.256832
-86.889909	-18.779124	2.266829
-86.735369	-21.502063	2.276826
-86.612329	-15.772266	2.286822
-85.380836	-24.332405	2.296819
-85.112223	-24.272051	2.306816
-84.958229	-16.266793	2.316813
-83.785032	-20.459734	2.326810
-83.606775	-22.393274	2.336806
-83.702778	-18.456519	2.346803
-82.375377	-19.667234	2.356800
-82.053572	-16.853137	2.366797
-82.122264	-15.021886	2.376794
-81.000709	-13.424686	2.386790
-80.512630	-18.578256	2.396787
-80.594518	-20.704299	2.406784
-79.441911	-19.199258	2.416781
-78.841470	-17.368256	2.426778
-78.795497	-20.992812	2.436774
-78.373330	-11.848070	2.446771
-77.340076	-12.774082	2.456768
-77.332069	-18.586805	2.466765
-76.772020	-4.720746	2.476762
-75.785711	-9.225575	2.486758
-75.627238	-16.614832	2.496755
-75.445421	-13.072197	2.506752
-74.656902	-13.261942	2.516749
-74.476953	-18.702422	2.526746
-73.347495	-18.143144	2.536742
-72.997926	-19.368380	2.546739
-72.799094	-16.693393	2.556736
-72.037936	-19.476777	2.566733
-71.322795	-13.844043	2.576730
-70.902710	-19.397999	2.586726
-70.889045	-14.624509	2.596723
-70.507753	-17.602935	2.606720
-69.764006	-16.981491	2.616717
-69.192675	-16.019600	2.626714
-68.277259	-9.802872	2.636710
-68.009964	-16.006358	2.646707
-67.622555	-22.177140	2.656704
-67.355766	-13.880247	2.666701
-66.501358	-8.779944	2.676698
-66.198467	-14.624216	2.686694
-65.732947	-16.510204	2.696691
-64.991610	-7.095978	2.706688
-64.610863	-9.548005	2.716685
-64.205917	-9.702806	2.726682
-63.085201	-4.097680	2.736678
-62.978005	-15.212127	2.746675
-63.001208	-13.655698	2.756672
-62.482961	-20.049323	2.766669
-61.615902	-14.279989	2.776666
-61.069286	-6.486795	2.786662
-60.215766	-19.791890	2.796659
-59.881251	-15.412025	2.806656
-60.019119	-11.935983	2.816653
-59.329663	-15.530963	2.826650
-58.456668	-10.746672	2.836646
-58.368374	-14.613721	2.846643
-57.186678	-6.492325	2.856640
-56.963105	-5.187381	2.866637
-56.836398	-13.283807	2.876634
-56.074044	-13.297344	2.886630
-55.374863	-19.148529	2.896627
-54.973461	-23.800481	2.906624
-55.133608	-17.871955	2.916621
-53.971613	-12.760944	2.926618
-53.476955	-11.796257	2.936614
-53.299402	-20.917154	2.946611
-52.279003	-13.948560	2.956608
-51.814237	-18.146117	2.966605
-51.816782	-7.970228	2.976602
-51.075433	-15.726182	2.986598
-50.136932	-22.619553	2.996595
-50.034884	-15.064350	3.006592
-50.115893	-15.669792	3.016589
-49.027363	-10.976636	3.026586
-48.646679	-19.347664	3.036582
-48.008924	-16.079028	3.046579
-47.301398	-7.693655	3.056576
-47.069119	-12.534586	3.066573
-47.090069	-23.337234	3.076570
-46.046576	-19.044211	3.086566
-45.533017	-18.256701	3.096563
-45.084308	-7.359995	3.106560
-44.070223	-15.340707	3.116557
-43.695682	-5.124202	3.126554
-43.509584	-15.360875	3.136550
-43.183413	-21.283670	3.146547
-42.882289	-20.875246	3.156544
-42.126807	-16.768440	3.166541
-41.733144	-21.465837	3.176538
-40.736742	-18.592824	3.186534
-40.402090	-12.765626	3.196531
-40.306742	-17.086360	3.206528
-39.609189	-6.317606	3.216525
-38.800258	-12.904878	3.226522
-38.733742	-14.422750	3.236518
-37.885438	-15.503802	3.246515
-37.300270	-15.219467	3.256512
-36.937410	-17.305413	3.266509
-36.908574	-11.237420	3.276506
-36.236009	-22.315302	3.286502
-36.002294	-13.018896	3.296499
-34.748594	-16.016735	3.306496
-34.563879	-18.393886	3.316493
-34.567365	-15.735938	3.326490
-33.392065	-17.152261	3.336486
-32.878056	-17.945336	3.346483
-32.560377	-10.013251	3.356480
-31.415185	-15.617597	3.366477
-31.431805	-17.334902	3.376474
-30.996722	-19.271570	3.386470
-30.973862	-17.883966	3.396467
-30.083196	-11.860309	3.406464
-29.717372	-18.092920	3.416461
-28.932756	-20.348631	3.426458
-28.410530	-20.476285	3.436454
-28.440842	-12.947016	3.446451
-27.409463	-20.788237	3.456448
-26.694122	-17.723267	3.466445
-26.468955	-21.327949	3.476442
-26.356235	-11.711643	3.486438
-25.159536	-21.826091	3.496435
-24.667880	-20.976185	3.506432
-24.834380	-14.407981	3.516429
-24.066678	-17.833142	3.526426
-23.308377	-14.035887	3.536422
-22.807176	-26.681269	3.546419
-22.761103	-18.617670	3.556416
-21.911096	-18.641244	3.566413
-21.503743	-22.607546	3.576410
-21.279383	-25.936986	3.586406
-20.145400	-24.664549	3.596403
-19.648363	-25.876024	3.606400
-19.455143	-24.503435	3.616397
-19.525250	-25.040544	3.626394
-18.495012	-13.181393	3.636390
-17.940462	-19.431066	3.646387
-17.550560	-24.412629	3.656384
-16.569895	-26.228757	3.666381
-16.670907	-15.080486	3.676378
-16.391331	-12.616995	3.686374
-15.303639	-21.655571	3.696371
-14.984482	-19.743800	3.706368
-14.571681	-13.412588	3.716365
-13.730101	-19.133006	3.726362
-13.512279	-19.249175	3.736358
-13.296949	-9.839386	3.746355
-12.245889	-17.331504	3.756352
-11.708076	-20.232172	3.766349
-11.626158	-11.529248	3.776346
-11.387388	-14.310362	3.786342
-10.784695	-17.757545	3.796339
-9.453284	-18.420767	3.806336
-9.473626	-9.390866	3.816333
-8.706432	-7.787149	3.826330
-8.746066	-14.251868	3.836326
-8.287069	-13.999429	3.846323
-7.366191	-19.386819	3.856320
-7.264066	-15.100023	3.866317
-6.043393	-16.929736	3.876314
-5.739221	-18.482733	3.886310
-5.703515	-11.315146	3.896307
-5.125905	-14.745047	3.906304
-4.459326	-18.478488	3.916301
-4.067275	-18.682817	3.926298
-3.547533	-16.527207	3.936294
-3.022636	5.295058	3.946291
-2.871919	6.562457	3.956288
-2.332523	17.920432	3.966285
-2.035389	38.223082	3.976282
-1.567505	45.163594	3.986278
-1.018957	66.302514	3.996275
-0.742782	96.002232	4.006272
-0.301876	108.362896	4.016269
0.000000	137.644274	4.021274
0.225084	163.020084	4.026278
0.248031	166.028008	4.031283
0.565401	182.712129	4.036288
0.751217	181.118222	4.041293
1.475283	180.163060	4.046298
1.308511	181.871261	4.051302
1.297877	186.306385	4.056307
1.527812	198.272102	4.061312
1.754269	186.153557	4.066317
1.277615	196.012609	4.071322
1.440476	195.380553	4.076326
1.262263	190.174099	4.081331
1.430973	189.932547	4.086336
1.677514	190.457918	4.091341
1.777231	186.270440	4.096346
1.461343	184.821793	4.101350
1.598384	186.938740	4.106355
1.634716	196.469434	4.111360
1.827882	178.636361	4.116365
1.312586	191.525137	4.121370
1.171011	190.792150	4.126374
1.623616	200.397995	4.131379
1.341290	201.382702	4.136384
1.658505	189.588931	4.141389
1.450527	190.236474	4.146394
1.265001	183.349129	4.151398
1.511907	180.767338	4.156403
1.609183	189.849821	4.161408
1.727421	183.761912	4.166413
1.413763	193.613264	4.171418
1.418352	187.745098	4.176422
1.245312	184.911478	4.181427
0.958818	195.723306	4.186432
1.467956	199.756146	4.191437
1.200647	196.176174	4.196442
1.660819	195.273599	4.201446
1.681970	209.299256	4.206451
1.612564	224.931133	4.211456
1.873006	220.347219	4.216461
1.907451	229.866308	4.221466
1.663517	214.158880	4.226470
1.876381	210.511885	4.231475
1.678512	213.711004	4.236480
2.050291	210.496701	4.241485
1.576135	207.317519	4.246490
1.628526	217.402195	4.251494
2.087840	220.035633	4.256499
1.751332	205.798509	4.261504
1.601806	214.558536	4.266509
1.817813	216.040108	4.271514
1.711033	222.571021	4.276518
2.006024	230.730671	4.281523
2.007334	230.469723	4.286528
2.048853	223.845251	4.291533
2.047477	223.186567	4.296538
1.736577	216.095481	4.301542
1.772301	215.697830	4.306547
1.875354	234.214069	4.311552
1.977339	222.760988	4.316557
1.845358	228.868686	4.321562
1.577193	222.116033	4.326566
1.942087	225.825147	4.331571
1.772189	223.973528	4.336576
2.264561	230.760597	4.341581
1.629781	233.564090	4.346586
2.203747	234.137858	4.351590
1.769993	226.216053	4.356595
1.745358	229.849447	4.361600
2.109365	233.944657	4.366605
1.823824	237.566513	4.371610
1.754915	228.196405	4.376614
2.141603	235.895368	4.381619
1.852724	249.680271	4.386624
2.094840	248.933695	4.391629
2.030928	262.940507	4.396634
2.186247	263.207477	4.401638
2.463827	264.884875	4.406643
2.276237	260.484597	4.411648
2.365363	248.733308	4.416653
1.876443	252.924388	4.421658
2.235501	253.670905	4.426662
2.603880	256.249331	4.431667
2.039088	261.171671	4.436672
2.489596	260.875262	4.441677
2.289198	261.205160	4.446682
2.320385	264.491633	4.451686
2.496475	264.238107	4.456691
2.060705	242.777474	4.461696
2.331274	249.333648	4.466701
2.489719	253.480493	4.471706
2.336253	251.617276	4.476710
1.918541	240.448366	4.481715
2.124644	260.126956	4.486720
2.435799	261.026120	4.491725
2.200665	265.168259	4.496730
2.422603	265.641464	4.501734
2.316540	257.683839	4.506739
2.323346	274.939998	4.511744
2.591078	260.270394	4.516749
2.583205	270.093756	4.521754
2.085964	260.408365	4.526758
2.524635	264.966971	4.531763
2.483101	256.554330	4.536768
2.266192	259.882591	4.541773
2.397935	271.623276	4.546778
2.485727	260.615583	4.551782
2.625137	264.886630	4.556787
2.307194	271.655497	4.561792
2.410492	260.766294	4.566797
2.748155	256.599261	4.571802
2.238806	259.517585	4.576806
2.613570	263.588532	4.581811
2.496943	289.504540	4.586816
2.812583	287.439290	4.591821
2.705983	288.909955	4.596826
3.054264	276.952737	4.601830
2.744999	277.591568	4.606835
2.917269	274.829910	4.611840
2.866721	259.334655	4.616845
2.732712	269.151139	4.621850
2.608481	265.747879	4.626854
2.655014	267.161567	4.631859
2.440638	264.101636	4.636864
2.978084	252.690519	4.641869
2.705702	265.725972	4.646874
2.648604	265.261378	4.651878
2.595208	264.929854	4.656883
2.438721	281.045393	4.661888
2.727967	289.935400	4.666893
2.600409	298.273142	4.671898
2.790500	299.777749	4.676902
2.903091	291.399406	4.681907
2.684576	300.034045	4.686912
2.710418	296.104994	4.691917
2.837749	305.276205	4.696922
2.919607	304.536280	4.701926
2.786535	302.085534	4.706931
2.742600	302.734287	4.711936
2.993068	306.565230	4.716941
3.006591	291.946879	4.721946
3.081504	305.560132	4.726950
3.106211	299.202710	4.731955
3.074997	299.721697	4.736960
3.031310	287.230788	4.741965
3.155622	288.534447	4.746970
2.747715	294.411429	4.751974
2.926076	291.993472	4.756979
2.746433	303.310603	4.761984
2.803528	285.848747	4.766989
2.852586	295.242041	4.771994
3.081848	316.846128	4.776998
3.364692	325.864777	4.782003
2.918186	313.648386	4.787008
3.302813	308.521826	4.792013
3.423805	311.983977	4.797018
3.238971	293.833702	4.802022
2.916874	291.261078	4.807027
3.010225	305.333691	4.812032
3.078052	309.900024	4.817037
2.989052	321.078373	4.822042
2.813932	324.264482	4.827046
3.370736	313.837686	4.832051
3.280877	315.468175	4.837056
3.067520	327.453876	4.842061
3.147111	323.130086	4.847066
3.154129	323.472669	4.852070
2.976297	317.048178	4.857075
3.046894	334.009135	4.862080
3.174680	326.538775	4.867085
2.845680	326.130163	4.872090
2.994180	342.471904	4.877094
3.425292	334.556584	4.882099
3.225945	352.754946	4.887104
3.368898	344.956992	4.892109
3.657669	347.868241	4.897114
3.453545	356.711859	4.902118
3.673311	348.674001	4.907123
3.526009	355.018593	4.912128
3.669414	341.432103	4.917133
3.602929	346.574607	4.922138
3.202857	351.746490	4.927142
3.609977	341.256705	4.932147
3.508958	348.628963	4.937152
3.795810	336.898700	4.942157
3.470807	328.197625	4.947162
2.910197	342.414353	4.952166
3.400518	340.188915	4.957171
3.402116	353.210243	4.962176
3.666067	345.229311	4.967181
3.842822	357.689535	4.972186
3.363539	349.824913	4.977190
3.682874	349.182679	4.982195
3.641125	352.900521	4.987200
3.857758	343.547084	4.992205
3.897832	349.960256	4.997210
3.857645	351.950633	5.002214
3.838181	349.662241	5.007219
3.690973	344.059333	5.012224
3.768812	350.685975	5.017229
3.523006	356.956476	5.022234
3.281679	350.377803	5.027238
3.376934	337.955941	5.032243
3.236327	347.558095	5.037248
3.744467	348.328816	5.042253
3.630158	352.863402	5.047258
3.458200	361.469861	5.052262
3.727004	349.006582	5.057267
3.761455	357.558703	5.062272
4.052642	360.320976	5.067277
3.990653	359.606794	5.072282
3.580020	361.316047	5.077286
3.674659	355.890118	5.082291
3.748365	358.568066	5.087296
4.047347	373.130634	5.092301
3.971659	372.113960	5.097306
4.320871	377.256641	5.102310
4.182227	366.335227	5.107315
3.883683	355.831621	5.112320
3.801289	343.280469	5.117325
3.645989	353.766762	5.122330
3.843397	364.288599	5.127334
4.118080	374.189445	5.132339
4.015015	387.851815	5.137344
3.903771	389.656722	5.142349
4.231202	378.345432	5.147354
4.236778	388.210846	5.152358
4.060221	363.261865	5.157363
3.984822	359.574962	5.162368
3.862766	361.809928	5.167373
4.002652	378.123335	5.172378
4.150685	378.903055	5.177382
4.649527	371.430450	5.182387
4.171875	364.601757	5.187392
4.002725	363.527226	5.192397
4.075671	365.443759	5.197402
3.912194	379.386428	5.202406
4.362215	377.920802	5.207411
4.422075	374.139326	5.212416
4.326490	364.343195	5.217421
4.308901	363.042256	5.222426
3.802360	355.636259	5.227430
4.172075	365.128834	5.232435
4.248547	380.209237	5.237440
4.308275	380.455306	5.242445
4.483334	378.257297	5.247450
3.945167	384.308661	5.252454
4.321119	386.585838	5.257459
4.052071	387.546459	5.262464
4.238571	383.328209	5.267469
4.553631	381.187963	5.272474
4.047672	376.728386	5.277478
4.187011	376.003327	5.282483
4.167763	373.706411	5.287488
4.157655	370.004671	5.292493
4.334299	384.548103	5.297498
4.105478	386.779405	5.302502
4.035159	390.391973	5.307507
4.166142	401.051194	5.312512
4.451188	407.055515	5.317517
4.758694	411.576153	5.322522
4.460065	402.795006	5.327526
4.768216	398.680366	5.332531
4.752867	409.619990	5.337536
4.581459	395.055977	5.342541
4.586403	389.606776	5.347546
4.438052	388.287685	5.352550
4.753001	382.807876	5.357555
4.543722	389.567914	5.362560
4.684215	383.586054	5.367565
4.680783	384.446250	5.372570
4.258037	389.190263	5.377574
4.526396	384.104696	5.382579
4.176592	391.282886	5.387584
4.502357	403.553369	5.392589
4.473693	407.547179	5.397594
4.471522	412.559799	5.402598
4.922768	417.216708	5.407603
4.730720	422.757948	5.412608
4.860693	421.867209	5.417613
5.116931	421.426994	5.422618
4.886138	418.666706	5.427622
4.844602	408.980302	5.432627
4.804417	409.371040	5.437632
4.632871	384.486211	5.442637
4.992049	398.460324	5.447642
4.324131	398.172832	5.452646
4.675704	415.054790	5.457651
4.483537	421.414321	5.462656
4.695388	416.753927	5.467661
4.744842	415.656684	5.472666
4.860689	416.705931	5.477670
5.054325	412.843933	5.482675
4.977485	429.845935	5.487680
5.324921	423.004188	5.492685
5.356505	423.137702	5.497690
5.114018	432.353036	5.502694
5.128989	414.264312	5.507699
4.789259	402.984329	5.512704
4.936004	395.187795	5.517709
4.985941	413.141402	5.522714
4.920754	427.164852	5.527718
5.149749	427.480918	5.532723
4.955450	427.178693	5.537728
5.064242	412.432900	5.542733
5.440651	403.811313	5.547738
4.772008	393.770874	5.552742
4.549403	388.497004	5.557747
4.388506	420.545255	5.562752
4.960357	413.171853	5.567757
5.145641	415.901716	5.572762
4.994021	436.445391	5.577766
4.878152	423.879678	5.582771
4.727777	423.712756	5.587776
5.023191	411.775614	5.592781
4.967409	411.229701	5.597786
4.912186	419.727813	5.602790
5.197160	437.968279	5.607795
5.089187	448.855360	5.612800
5.171785	442.529650	5.617805
5.071605	445.120228	5.622810
5.306007	450.006650	5.627814
5.434604	450.243410	5.632819
5.100152	461.278129	5.637824
5.413871	456.068527	5.642829
5.456038	446.549009	5.647834
5.084975	445.092782	5.652838
5.244524	438.954041	5.657843
5.391448	451.625863	5.662848
5.209567	451.334707	5.667853
5.298922	452.000113	5.672858
5.219691	455.394358	5.677862
5.337185	452.990479	5.682867
5.168712	461.100559	5.687872
5.306357	446.350756	5.692877
5.309005	450.124228	5.697882
5.173917	447.534979	5.702886
4.984694	447.518419	5.707891
5.011159	460.513925	5.712896
4.860083	463.003603	5.717901
5.844246	472.891155	5.722906
5.823139	481.068744	5.727910
5.532989	460.076050	5.732915
5.340753	453.458143	5.737920
5.444265	458.837490	5.742925
5.676970	462.786740	5.747930
5.258620	471.396191	5.752934
6.034046	469.866225	5.757939
5.668948	460.646836	5.762944
5.442196	452.401635	5.767949
5.513506	449.457734	5.772954
5.520524	468.945241	5.777958
5.666087	469.321761	5.782963
5.841148	482.436869	5.787968
5.788969	463.669262	5.792973
5.811619	458.514468	5.797978
5.457863	452.849560	5.802982
5.371481	457.825203	5.807987
5.210674	480.483428	5.812992
5.533895	491.187798	5.817997
5.868137	479.132901	5.823002
5.681023	487.725064	5.828006
5.867122	481.563569	5.833011
5.910560	484.158538	5.838016
5.853654	476.700079	5.843021
5.638005	485.133379	5.848026
5.559866	496.445322	5.853030
5.831043	481.668486	5.858035
5.395229	480.044087	5.863040
5.709688	485.519207	5.868045
5.674492	481.541396	5.873050
5.535778	487.315559	5.878054
5.959847	484.336936	5.883059
5.650686	486.724979	5.888064
5.697675	483.300677	5.893069
5.750733	489.825811	5.898074
5.938337	502.761770	5.903078
6.163662	509.278077	5.908083
6.102881	502.904706	5.913088
5.931362	486.910563	5.918093
5.935106	478.814018	5.923098
5.754115	474.939129	5.928102
5.899588	485.024089	5.933107
6.133550	506.850931	5.938112
6.227316	510.087651	5.943117
6.321197	493.367119	5.948122
5.773914	498.544633	5.953126
5.967922	487.100812	5.958131
6.271870	513.607724	5.963136
6.025509	502.526329	5.968141
6.158362	499.187380	5.973146
6.061970	509.119742	5.978150
6.233447	499.906666	5.983155
6.165325	492.848931	5.988160
5.830153	484.552667	5.993165
6.257719	503.397709	5.998170
6.007711	513.795873	6.003174
6.399893	510.313632	6.008179
6.141731	520.621199	6.013184
6.105357	512.685075	6.018189
6.478056	513.198391	6.023194
6.666852	513.161883	6.028198
6.310620	497.846048	6.033203
6.003785	494.155726	6.038208
5.898316	490.400556	6.043213
6.252005	498.018088	6.048218
5.977868	505.728818	6.053222
6.304590	509.215718	6.058227
6.199561	517.556663	6.063232
6.086259	514.821535	6.068237
6.427937	513.834835	6.073242
6.389544	515.977957	6.078246
6.431445	509.414566	6.083251
6.122443	500.392475	6.088256
6.073910	492.052094	6.093261
6.259858	498.883903	6.098266
6.184522	505.947530	6.103270
6.307813	507.524366	6.108275
6.541335	514.066945	6.113280
5.785485	507.884009	6.118285
6.173482	511.062339	6.123290
5.950676	511.832708	6.128294
6.269477	513.600797	6.133299
6.358067	510.003374	6.138304
6.535836	522.207939	6.143309
6.670652	510.470506	6.148314
6.301519	486.942563	6.153318
6.427122	485.973123	6.158323
6.326492	488.606304	6.163328
6.288038	492.754281	6.168333
6.051024	487.611705	6.173338
6.064346	487.337422	6.178342
6.351226	479.720038	6.183347
6.188432	483.370601	6.188352
6.011446	479.489722	6.193357
6.191966	470.932533	6.198362
5.860276	480.972724	6.203366
6.237410	487.845744	6.208371
6.410394	503.789468	6.213376
5.668740	492.690876	6.218381
6.370534	494.242651	6.223386
6.328370	507.203957	6.228390
6.424844	506.975917	6.233395
6.354515	497.519650	6.238400
6.280399	501.139975	6.243405
6.488234	486.296253	6.248410
5.968554	484.110532	6.253414
5.984814	488.956061	6.258419
6.365779	486.835987	6.263424
6.125532	494.568638	6.268429
6.262875	486.021338	6.273434
6.030919	490.126212	6.278438
6.865692	496.639274	6.283443
6.523692	485.283934	6.288448
6.207823	485.391007	6.293453
6.620804	482.941845	6.298458
6.315647	487.875119	6.303462
6.135519	486.521116	6.308467
6.590126	488.007977	6.313472
5.809839	485.029188	6.318477
6.252461	475.637833	6.323482
6.175003	479.217268	6.328486
6.356832	483.036020	6.333491
6.492301	486.263674	6.338496
6.347684	492.685129	6.343501
6.619939	482.657751	6.348506
6.441202	476.324208	6.353510
6.267908	478.973342	6.358515
6.096102	483.196531	6.363520
5.981485	481.814634	6.368525
6.099234	475.834820	6.373530
5.845373	476.755250	6.378534
6.418938	473.491367	6.383539
6.526223	480.175946	6.388544
6.409299	473.993397	6.393549
6.410070	476.463311	6.398554
6.066805	486.809682	6.403558
5.930426	481.068588	6.408563
6.359785	478.691701	6.413568
6.246992	478.375808	6.418573
6.274344	480.454489	6.423578
6.178442	483.262501	6.428582
6.361763	480.034594	6.433587
6.127395	488.432414	6.438592
5.928762	486.079687	6.443597
6.277238	478.623001	6.448602
5.850617	479.979737	6.453606
5.926540	489.510779	6.458611
5.924661	487.381458	6.463616
5.783020	486.423130	6.468621
6.057540	473.599885	6.473626
5.622420	484.644252	6.478630
5.865223	492.118108	6.483635
6.286177	490.988867	6.488640
6.311467	507.360715	6.493645
6.181322	511.956469	6.498650
6.131710	518.015053	6.503654
6.188373	515.567744	6.508659
6.292547	516.116950	6.513664
6.061410	508.771622	6.518669
6.508454	511.187525	6.523674
6.188298	507.897095	6.528678
5.977253	507.759633	6.533683
6.211764	506.739044	6.538688
6.228757	506.646476	6.543693
6.443874	502.785148	6.548698
6.367729	515.861095	6.553702
6.475559	506.084337	6.558707
6.259241	517.445966	6.563712
6.158154	516.303841	6.568717
6.471357	514.110510	6.573722
6.634295	515.283791	6.578726
6.412322	489.266331	6.583731
6.496428	484.484465	6.588736
5.982929	489.205719	6.593741
6.288292	480.703959	6.598746
5.982940	485.935017	6.603750
6.258251	480.529601	6.608755
6.191813	482.089840	6.613760
5.727872	490.217094	6.618765
6.227991	487.515171	6.623770
6.567781	511.088552	6.628774
6.596686	493.585045	6.633779
6.455278	493.549435	6.638784
6.050438	489.343636	6.643789
6.276995	475.487958	6.648794
6.181197	487.071559	6.653798
6.175398	470.779819	6.658803
6.080036	473.726849	6.663808
5.973012	484.770963	6.668813
6.284323	469.171202	6.673818
6.257975	475.398085	6.678822
6.289417	475.428327	6.683827
6.532183	487.426878	6.688832
6.104515	498.665565	6.693837
6.308001	483.709895	6.698842
6.387673	479.904401	6.703846
6.341140	476.830305	6.708851
5.980396	476.646942	6.713856
5.953402	484.171792	6.718861
6.207135	479.553097	6.723866
5.822076	479.838633	6.728870
6.343600	490.333929	6.733875
6.320841	491.441999	6.738880
6.319676	494.611037	6.743885
6.347732	475.841699	6.748890
6.370521	485.472976	6.753894
6.025730	477.391309	6.758899
6.397302	477.057824	6.763904
6.425590	477.400349	6.768909
6.814441	477.051577	6.773914
6.158580	477.311324	6.778918
6.299376	478.530290	6.783923
6.317428	477.151233	6.788928
6.499496	484.117360	6.793933
6.653525	481.240191	6.798938
6.514188	484.128882	6.803942
6.633157	474.385624	6.808947
6.845152	473.979850	6.813952
6.231051	472.866765	6.818957
6.098399	454.139895	6.823962
6.390546	453.537569	6.828966
6.682766	448.678998	6.833971
6.303227	448.574216	6.838976
5.954963	459.475560	6.843981
6.067561	445.346909	6.848986
5.845785	451.258306	6.853990
6.093094	444.247125	6.858995
5.896713	441.355455	6.864000
6.080187	453.848981	6.869005
6.775457	467.201216	6.874010
6.289180	464.817198	6.879014
6.199718	450.529450	6.884019
6.362354	446.735017	6.889024
6.259431	443.588951	6.894029
6.331131	448.031559	6.899034
6.560866	464.779108	6.904038
6.218730	454.907838	6.909043
6.493711	450.321552	6.914048
6.228496	442.599782	6.919053
6.187336	439.042660	6.924058
5.927505	449.966480	6.929062
6.315834	446.577727	6.934067
6.368728	451.118649	6.939072
6.157210	444.995549	6.944077
6.512349	444.674053	6.949082
6.327201	450.287860	6.954086
6.150340	448.449400	6.959091
6.123690	452.901060	6.964096
6.254164	457.633683	6.969101
6.443870	451.432436	6.974106
6.135945	453.860819	6.979110
6.160005	439.230326	6.984115
6.251803	442.577263	6.989120
5.890159	448.545909	6.994125
6.138981	444.985163	6.999130
6.041628	456.693407	7.004134
5.899192	444.813699	7.009139
6.134439	447.784523	7.014144
6.120283	453.724949	7.019149
6.329590	441.117619	7.024154
6.371872	446.740605	7.029158
6.165856	453.340996	7.034163
6.180900	443.437839	7.039168
6.211123	453.292118	7.044173
6.575300	443.423017	7.049178
6.206534	449.012807	7.054182
6.276898	456.119125	7.059187
6.373107	444.806534	7.064192
6.168045	444.856523	7.069197
6.268160	432.410102	7.074202
6.184493	445.716120	7.079206
6.219067	450.892965	7.084211
6.320591	452.584876	7.089216
6.195837	446.141102	7.094221
6.645358	439.698916	7.099226
6.557464	448.241709	7.104230
6.303838	445.933593	7.109235
6.277098	447.968919	7.114240
6.317289	456.439444	7.119245
6.219226	454.225588	7.124250
6.139423	456.572173	7.129254
6.103781	451.994005	7.134259
6.152958	451.316105	7.139264
6.188762	454.629184	7.144269
6.223197	448.210601	7.149274
6.276425	453.838786	7.154278
6.664547	452.999999	7.159283
6.506491	454.576855	7.164288
6.267218	452.857825	7.169293
6.140280	461.210450	7.174298
6.201184	459.994795	7.179302
6.391921	465.312867	7.184307
6.163418	456.209622	7.189312
6.139823	455.074230	7.194317
6.140497	458.648740	7.199322
6.316492	449.609475	7.204326
6.232732	463.056013	7.209331
6.172856	455.949083	7.214336
6.037773	446.330797	7.219341
6.388400	448.058990	7.224346
5.802548	453.922818	7.229350
5.913260	454.775896	7.234355
6.239667	455.868389	7.239360
6.090380	456.602632	7.244365
6.114680	445.756937	7.249370
5.865084	460.956419	7.254374
5.931300	462.221449	7.259379
6.210275	453.498630	7.264384
5.956336	459.003445	7.269389
5.962347	450.024531	7.274394
5.670346	456.085854	7.279398
6.464617	473.228480	7.284403
6.266662	485.163218	7.289408
6.050645	494.474648	7.294413
6.487394	484.727705	7.299418
6.435509	488.805879	7.304422
6.147109	475.052368	7.309427
6.394049	464.454006	7.314432
6.129996	468.691645	7.319437
5.964908	460.183781	7.324442
6.194534	471.671170	7.329446
6.290590	481.328615	7.334451
6.714025	482.503044	7.339456
6.241428	469.602398	7.344461
6.460576	452.933526	7.349466
6.015677	454.224121	7.354470
5.935721	456.801986	7.359475
5.839377	451.346613	7.364480
5.946760	467.771940	7.369485
6.001164	481.191715	7.374490
6.213726	489.816391	7.379494
6.032193	496.972249	7.384499
6.195771	482.816294	7.389504
6.045562	488.458773	7.394509
6.212709	482.615230	7.399514
6.165351	476.005929	7.404518
6.143248	491.434915	7.409523
6.408182	485.160646	7.414528
6.025069	499.406789	7.419533
6.146608	499.171845	7.424538
5.718997	494.370849	7.429542
5.926303	497.876592	7.434547
6.050923	491.057727	7.439552
5.694075	493.269159	7.444557
6.451789	504.539566	7.449562
6.471074	514.692458	7.454566
6.159572	510.415684	7.459571
6.335540	488.975260	7.464576
6.019144	501.685804	7.469581
6.119861	500.134046	7.474586
6.342417	512.440910	7.479590
6.348290	507.179559	7.484595
6.206174	501.198184	7.489600
5.951437	509.826988	7.494605
6.649896	511.966239	7.499610
6.239944	500.189892	7.504614
6.013553	493.629803	7.509619
6.303066	484.255063	7.514624
5.986119	489.187029	7.519629
6.288239	493.893962	7.524634
6.394034	515.598941	7.529638
6.234954	499.264723	7.534643
6.420784	494.468214	7.539648
6.411430	487.710164	7.544653
6.387713	488.993907	7.549658
6.149966	479.219322	7.554662
6.009253	492.169572	7.559667
6.496364	488.120144	7.564672
5.886317	495.864084	7.569677
6.249278	491.665676	7.574682
6.301627	483.949714	7.579686
6.217134	489.892010	7.584691
6.699436	484.513161	7.589696
6.509022	491.724746	7.594701
6.509638	481.664910	7.599706
6.521688	482.041493	7.604710
6.323394	482.686262	7.609715
6.558021	488.509721	7.614720
6.459132	490.419149	7.619725
6.597661	491.880797	7.624730
6.262829	471.582236	7.629734
6.199833	469.840782	7.634739
6.354649	460.664717	7.639744
6.379443	460.238578	7.644749
6.539848	457.271369	7.649754
6.334329	462.800051	7.654758
6.084017	454.195283	7.659763
6.021088	456.819269	7.664768
5.877600	463.446919	7.669773
5.758453	456.804798	7.674778
5.799799	475.331031	7.679782
6.101666	491.269427	7.684787
6.249315	482.104400	7.689792
5.908508	489.045945	7.694797
6.276439	472.850593	7.699802
6.173370	483.007997	7.704806
6.111438	493.694328	7.709811
6.249955	487.197854	7.714816
6.190325	488.971946	7.719821
6.570013	487.828905	7.724826
6.371443	482.508509	7.729830
6.124366	487.827215	7.734835
6.267903	483.296382	7.739840
6.300635	495.731683	7.744845
6.213182	486.376321	7.749850
6.041831	497.886779	7.754854
6.067719	485.273319	7.759859
5.921658	480.165045	7.764864
6.145231	493.482486	7.769869
6.161255	496.772403	7.774874
6.017880	490.782953	7.779878
5.832693	483.375090	7.784883
6.572867	473.358988	7.789888
6.202227	487.850989	7.794893
6.535892	486.244063	7.799898
6.200168	490.269696	7.804902
6.012804	495.412789	7.809907
6.105633	485.709558	7.814912
5.999623	494.580747	7.819917
5.966373	483.823956	7.824922
6.214153	486.630620	7.829926
6.417093	495.155862	7.834931
6.174334	495.208529	7.839936
5.969836	497.276296	7.844941
5.823855	489.174397	7.849946
6.523808	508.830594	7.854950
6.540714	514.931066	7.859955
6.079099	494.645237	7.864960
5.743419	506.263463	7.869965
6.097834	510.227439	7.874970
6.448758	528.735234	7.879974
6.403410	521.314011	7.884979
6.469043	518.039049	7.889984
6.185489	507.471200	7.894989
6.188945	489.281882	7.899994
6.175164	493.379018	7.904998
5.781958	506.645968	7.910003
6.664848	512.360333	7.915008
6.207615	505.855948	7.920013
6.358105	485.046718	7.925018
6.246249	493.202707	7.930022
6.078633	496.501759	7.935027
6.374254	493.188795	7.940032
6.013401	496.043653	7.945037
6.286877	496.289621	7.950042
6.019450	494.472535	7.955046
6.225203	509.584286	7.960051
6.313547	519.759609	7.965056
6.275916	526.489960	7.970061
6.338137	517.535952	7.975066
6.268664	505.826265	7.980070
5.950759	495.936462	7.985075
6.508331	502.227772	7.990080
6.174668	501.854159	7.995085
6.272601	507.072644	8.000090
6.290536	498.851900	8.005094
6.146567	490.891243	8.010099
6.439064	497.735437	8.015104
6.047443	492.965491	8.020109
6.377516	486.157402	8.025126
6.298119	500.927202	8.030144
6.211185	497.517605	8.035162
6.063750	495.709352	8.040179
5.877836	500.008609	8.045197
6.405197	499.940276	8.050214
6.599734	513.396743	8.055232
6.087277	506.105916	8.060250
6.455206	493.948713	8.065267
6.320008	505.743245	8.070285
6.178471	501.045564	8.075302
6.288757	490.026116	8.080320
6.037017	481.396784	8.085338
6.220361	492.715415	8.090355
6.557908	523.092911	8.095373
6.472473	515.502322	8.100390
6.577699	498.464322	8.105408
6.164538	484.896821	8.110426
6.225965	486.163622	8.115443
6.251864	495.749540	8.120461
6.410282	483.728524	8.125478
6.506621	494.158649	8.130496
6.457625	499.147748	8.135514
6.204446	495.244657	8.140531
6.211185	496.306854	8.145549
6.450021	486.561401	8.150566
6.369955	484.839832	8.155584
6.090327	488.231219	8.160602
6.367704	487.561597	8.165619
6.432019	501.957812	8.170637
6.683030	486.496919	8.175654
6.607265	488.442571	8.180672
6.186666	492.828533	8.185690
6.420468	490.393012	8.190707
6.596690	501.682025	8.195725
6.433111	494.734954	8.200742
6.682816	493.347498	8.205760
6.063337	484.625911	8.210778
6.655944	481.179204	8.215795
6.672517	496.302856	8.220813
6.497337	492.610949	8.225830
6.573056	497.684438	8.230848
6.460101	492.963438	8.235866
6.536213	492.985224	8.240883
6.398693	491.749046	8.245901
6.574417	488.833940	8.250918
6.681073	493.180499	8.255936
6.309891	496.527775	8.260954
6.760570	491.708613	8.265971
6.304363	501.987382	8.270989
6.552981	490.151812	8.276006
7.002965	484.477018	8.281024
6.538386	490.253361	8.286042
6.271628	489.738412	8.291059
6.532273	482.277622	8.296077
6.537080	495.177345	8.301094
6.590916	484.712110	8.306112
5.983731	494.282986	8.311130
6.305050	491.322858	8.316147
6.543252	500.679833	8.321165
6.787426	496.214422	8.326182
6.597118	489.666383	8.331200
6.544970	491.792647	8.336218
6.734654	487.458563	8.341235
6.487464	491.348336	8.346253
6.230101	491.875149	8.351270
6.594274	496.548868	8.356288
6.549726	506.892658	8.361306
6.603037	495.314319	8.366323
6.439726	491.462212	8.371341
6.308127	486.028874	8.376358
6.438264	482.168524	8.381376
6.253691	493.983015	8.386394
6.471299	493.168476	8.391411
6.426124	498.414672	8.396429
6.560816	511.840975	8.401446
7.005155	511.217469	8.406464
6.629005	502.358730	8.411482
6.303970	490.845772	8.416499
6.714374	504.081552	8.421517
6.550288	509.680216	8.426534
7.162537	507.664840	8.431552
6.576896	504.002480	8.436570
6.730826	490.189712	8.441587
6.838142	490.035802	8.446605
6.457384	501.207743	8.451622
6.599676	493.570478	8.456640
6.564737	502.403799	8.461658
6.876261	491.052625	8.466675
6.780142	492.011960	8.471693
6.684179	492.735780	8.476710
6.788071	482.811190	8.481728
6.749420	503.633191	8.486746
6.809256	500.307882	8.491763
6.849209	497.830490	8.496781
6.365052	492.215888	8.501798
6.627748	484.193443	8.506816
6.633359	500.967428	8.511834
6.944338	511.129065	8.516851
6.955476	502.025649	8.521869
6.322947	510.210817	8.526886
6.649290	500.913311	8.531904
6.569650	516.049930	8.536922
6.843041	513.145938	8.541939
7.209439	518.906403	8.546957
6.649178	507.661299	8.551974
6.696370	502.808042	8.556992
6.591125	512.183697	8.562010
6.897547	521.611975	8.567027
6.942027	519.277113	8.572045
6.938669	516.223122	8.577063
6.930505	505.810335	8.582080
6.670012	511.079129	8.587098
7.035891	516.033919	8.592115
6.975790	494.564111	8.597133
6.396989	498.680801	8.602151
6.908798	513.267298	8.607168
6.991020	522.173673	8.612186
6.789061	514.180862	8.617203
7.049692	502.923704	8.622221
6.786831	497.457339	8.627239
6.878170	490.320729	8.632256
6.515827	505.418933	8.637274
6.510187	517.279646	8.642291
6.784507	518.059971	8.647309
6.669854	527.369683	8.652327
7.120217	519.846228	8.657344
7.014932	528.010701	8.662362
6.926013	519.014935	8.667379
6.965479	522.685230	8.672397
6.653277	535.328867	8.677415
7.232558	536.163109	8.682432
7.295033	533.295740	8.687450
7.152930	530.090001	8.692467
6.891580	519.152908	8.697485
6.582651	527.155302	8.702503
7.268457	522.218351	8.707520
7.272731	533.697093	8.712538
7.159787	515.911213	8.717555
6.789153	500.285762	8.722573
6.563511	509.718903	8.727591
6.896067	505.011170	8.732608
7.061433	516.517303	8.737626
6.992457	534.592591	8.742643
7.440227	529.091048	8.747661
6.888060	513.854868	8.752679
6.762256	507.597387	8.757696
6.824283	522.276526	8.762714
6.978850	530.731266	8.767731
7.453543	531.539492	8.772749
7.117659	530.096273	8.777767
7.121924	514.220108	8.782784
7.056754	523.345293	8.787802
7.167349	514.722687	8.792819
6.706183	513.418852	8.797837
6.633271	515.497083	8.802855
7.091711	513.878316	8.807872
7.114615	525.455037	8.812890
6.926504	511.758605	8.817907
6.837186	521.191170	8.822925
6.928932	532.852075	8.827943
7.097853	521.467762	8.832960
7.133916	519.790963	8.837978
7.009994	527.549042	8.842995
7.065390	527.451242	8.848013
6.899934	530.031492	8.853031
7.338441	520.741909	8.858048
7.117775	527.407515	8.863066
7.204582	520.136527	8.868083
7.157004	514.702677	8.873101
7.164980	529.801901	8.878119
7.403282	515.776089	8.883136
7.089678	525.768658	8.888154
6.991593	523.660959	8.893171
7.178998	513.869766	8.898189
7.028086	517.327765	8.903207
7.202195	511.768813	8.908224
7.045260	522.761879	8.913242
6.877555	522.702720	8.918259
7.100166	514.946383	8.923277
6.659196	530.145483	8.928295
7.224808	535.777283	8.933312
7.425051	546.317808	8.938330
7.317029	557.990291	8.943347
7.513834	529.183809	8.948365
6.918780	531.189302	8.953383
6.824034	536.114825	8.958400
7.311026	543.111739	8.963418
7.391567	552.973160	8.968435
7.415415	548.799905	8.973453
7.547830	560.903144	8.978471
7.305370	544.894227	8.983488
7.231383	521.549650	8.988506
7.188844	534.895341	8.993523
7.311183	542.532431	8.998541
7.451757	554.366746	9.003559
7.263434	541.945292	9.008576
7.371203	531.239166	9.013594
7.202378	534.786433	9.018611
7.451031	533.720251	9.023629
6.963296	552.939569	9.028647
7.334055	551.455444	9.033664
7.421526	554.318448	9.038682
7.427110	553.946155	9.043699
7.334790	551.059785	9.048717
7.384629	557.153728	9.053735
7.140569	558.845951	9.058752
7.098418	562.056205	9.063770
7.284328	555.167374	9.068787
7.667159	546.213691	9.073805
7.495586	553.605906	9.078823
7.589619	559.575835	9.083840
7.442450	557.999182	9.088858
7.625760	564.596469	9.093875
7.609764	557.140225	9.098893
7.479624	563.498517	9.103911
7.368786	547.930755	9.108928
6.919118	542.253261	9.113946
7.271831	560.473716	9.118963
7.231149	553.502078	9.123981
7.327094	566.438463	9.128999
7.224066	570.546713	9.134016
7.722618	558.438825	9.139034
6.978414	562.690227	9.144051
7.690716	561.210574	9.149069
7.666926	565.881806	9.154087
7.450193	558.313483	9.159104
7.727254	560.672113	9.164122
7.429596	556.687297	9.169139
7.453614	555.120044	9.174157
7.509869	563.587309	9.179175
7.626198	559.006516	9.184192
7.726662	557.778831	9.189210
7.458159	552.267127	9.194227
7.370683	556.360698	9.199245
7.496225	560.100522	9.204263
7.436759	559.310414	9.209280
7.620303	562.371087	9.214298
7.442256	566.205366	9.219315
7.525052	556.737383	9.224333
7.424520	560.881431	9.229351
7.072041	557.849404	9.234368
7.155781	559.362676	9.239386
7.395871	564.269285	9.244403
7.528299	565.850778	9.249421
7.519370	580.149051	9.254439
7.433634	590.518204	9.259456
7.688539	591.119392	9.264474
7.361539	596.902857	9.269491
7.780608	589.375585	9.274509
8.055882	592.214843	9.279527
7.609847	585.486327	9.284544
7.596837	589.418316	9.289562
7.954756	590.205693	9.294579
7.869419	584.693329	9.299597
7.802601	588.995760	9.304615
7.714622	601.490803	9.309632
7.969561	590.584264	9.314650
7.768480	587.943280	9.319667
7.675815	556.616926	9.324685
7.743935	565.247261	9.329703
7.429676	546.314804	9.334720
7.439130	565.223079	9.339738
7.631805	583.729608	9.344755
7.870956	589.741108	9.349773
7.906926	577.702564	9.354791
7.724291	584.033227	9.359808
7.816514	587.970459	9.364826
7.775515	589.752828	9.369843
7.783392	590.044801	9.374861
7.818527	585.956664	9.379879
7.794516	592.870163	9.384896
7.984829	586.631362	9.389914
7.838238	591.816903	9.394931
7.740299	578.665156	9.399949
7.913667	586.641707	9.404967
7.787047	581.301492	9.409984
7.945597	578.630306	9.415002
7.597145	570.130862	9.420019
7.659150	579.752198	9.425037
7.821691	581.536455	9.430055
7.516304	592.127504	9.435072
7.654798	591.836870	9.440090
7.927457	603.094669	9.445107
7.694215	593.804951	9.450125
7.730131	595.852612	9.455143
7.739268	591.370906	9.460160
7.886115	583.835778	9.465178
7.855907	597.593290	9.470195
7.968222	594.321778	9.475213
7.707600	600.420595	9.480231
7.857335	596.466148	9.485248
7.998820	590.371020	9.490266
7.867926	594.370219	9.495283
7.946412	597.797314	9.500301
7.781218	599.343363	9.505319
7.724165	595.851360	9.510336
8.164183	585.866729	9.515354
7.806654	589.846008	9.520371
8.061968	581.872656	9.525389
7.951162	589.170806	9.530407
7.695671	594.814227	9.535424
8.211612	590.415965	9.540442
8.232454	595.889136	9.545459
7.832519	590.601564	9.550477
7.863206	585.293805	9.555495
8.024226	588.429159	9.560512
8.118932	590.514733	9.565530
8.161971	584.315327	9.570547
8.029397	592.132536	9.575565
8.341319	593.868884	9.580583
8.085868	594.359366	9.585600
8.348665	588.096088	9.590618
8.026411	592.096207	9.595635
7.960059	602.376550	9.600653
8.215049	592.347603	9.605671
8.337243	597.658973	9.610688
8.383893	586.943228	9.615706
8.259925	599.225750	9.620723
8.249113	585.506251	9.625741
8.308694	587.979846	9.630759
8.155730	597.727843	9.635776
8.130076	591.537916	9.640794
8.316702	593.112226	9.645811
8.297327	589.503092	9.650829
8.073407	593.140467	9.655847
7.964570	590.453929	9.660864
7.860660	585.394752	9.665882
8.159601	588.656401	9.670899
8.003110	595.157127	9.675917
8.206491	588.850035	9.680935
7.773460	606.337750	9.685952
8.244765	595.413953	9.690970
8.103106	589.944550	9.695987
8.180038	592.225253	9.701005
8.269330	585.964275	9.706023
8.120136	594.775297	9.711040
8.129711	591.858106	9.716058
8.321456	599.043970	9.721075
8.290419	595.598249	9.726093
8.274567	592.697954	9.731111
8.084675	590.608764	9.736128
8.162970	587.322997	9.741146
8.234657	600.734400	9.746163
8.024405	595.120650	9.751181
7.894086	593.157319	9.756199
7.996266	616.379689	9.761216
8.304306	614.449802	9.766234
8.514523	617.836631	9.771251
8.681756	617.287847	9.776269
8.701151	618.905737	9.781287
8.133814	607.234638	9.786304
8.093907	593.996628	9.791322
8.307164	605.187979	9.796339
8.468267	612.972511	9.801357
8.450702	625.714946	9.806375
8.426685	629.774629	9.811392
8.390547	625.146977	9.816410
8.425462	613.116551	9.821427
8.092651	610.197778	9.826445
8.437787	615.713806	9.831463
8.514182	623.901348	9.836480
8.631471	608.956242	9.841498
8.424886	606.697299	9.846515
8.354284	603.684516	9.851533
8.520430	607.645948	9.856551
8.377166	618.929980	9.861568
8.643818	615.418823	9.866586
8.429013	599.836896	9.871603
8.312230	607.596493	9.876621
8.850888	604.426049	9.881639
8.627577	597.912054	9.886656
8.535064	587.677296	9.891674
8.643842	583.718500	9.896691
8.259468	588.906333	9.901709
8.473738	582.014280	9.906727
8.681463	593.314195	9.911744
8.732420	595.487596	9.916762
8.364527	591.617115	9.921779
8.165418	596.173555	9.926797
8.585814	589.502705	9.931815
8.377129	591.062828	9.936832
8.441991	604.949493	9.941850
8.508741	616.928709	9.946867
8.482093	625.611150	9.951885
8.945911	622.851721	9.956903
8.852835	626.201484	9.961920
8.751922	602.277969	9.966938
8.558945	592.768249	9.971955
8.523596	597.129644	9.976973
8.709433	587.169402	9.981991
8.598312	594.627125	9.987008
8.613900	590.873359	9.992026
8.798001	581.316191	9.997043
8.389074	573.420631	10.002061
9.011893	582.132801	10.007079
8.694529	581.268599	10.012096
8.764028	586.538682	10.017114
8.762554	580.311010	10.022131
8.459871	575.345205	10.027149
8.747679	575.744730	10.032167
8.803569	586.675314	10.037184
8.764601	587.289737	10.042202
8.839558	583.333873	10.047219
8.534726	592.127019	10.052237
8.527547	585.949983	10.057255
8.339574	585.726683	10.062272
8.817780	606.360277	10.067290
8.979104	613.809890	10.072307
8.819799	621.708289	10.077325
8.534362	609.707975	10.082343
8.991632	608.594028	10.087360
8.750289	611.577314	10.092378
8.990467	593.439636	10.097395
8.791112	596.457016	10.102413
9.151297	574.400214	10.107431
8.747847	579.208587	10.112448
8.363696	586.286894	10.117466
9.278070	590.863717	10.122483
8.879910	609.617792	10.127501
8.923739	582.489941	10.132519
8.947419	584.935222	10.137536
8.702467	591.158884	10.142554
8.901043	590.222999	10.147571
9.043698	607.818793	10.152589
8.917618	601.975912	10.157607
8.770651	598.182484	10.162624
8.498395	594.854368	10.167642
8.873844	579.267620	10.172659
8.791701	598.832888	10.177677
8.974515	616.369112	10.182695
9.062851	610.283645	10.187712
8.901315	608.194293	10.192730
8.830622	609.138510	10.197747
8.608865	626.048023	10.202765
9.231046	619.179079	10.207783
9.096854	623.081505	10.212800
9.033658	627.305705	10.217818
9.158442	622.329174	10.222835
8.975054	605.610160	10.227853
8.791801	594.414874	10.232871
8.756948	607.254919	10.237888
8.823436	618.676994	10.242906
9.362286	624.447183	10.247923
9.106258	618.171519	10.252941
9.068804	612.990936	10.257959
9.413197	615.499443	10.262976
9.418348	601.461894	10.267994
9.074360	596.060564	10.273011
8.849144	592.113956	10.278029
9.037329	580.824922	10.283047
8.852518	581.220871	10.288064
8.819592	596.869148	10.293082
9.318383	614.003509	10.298099
9.453268	630.322686	10.303117
9.079289	605.754549	10.308135
9.032729	588.591756	10.313152
8.936914	591.953773	10.318170
9.007450	608.701401	10.323187
9.222995	615.472880	10.328205
9.341948	624.742471	10.333223
9.192582	614.080454	10.338240
9.099530	620.893092	10.343258
9.225935	612.186927	10.348275
8.932298	620.247263	10.353293
9.136948	610.745825	10.358311
9.234608	619.177346	10.363328
8.868311	629.755755	10.368346
9.279317	607.081164	10.373363
9.393890	615.347712	10.378381
9.041170	623.494868	10.383399
8.968644	607.801543	10.388416
8.604350	609.935516	10.393434
9.091665	613.904199	10.398451
9.022483	619.877703	10.403469
9.034664	619.696017	10.408487
9.108560	624.031789	10.413504
9.129840	639.661114	10.418522
9.499240	635.151449	10.423539
9.301116	641.077088	10.428557
9.504050	644.679953	10.433575
9.208126	629.788646	10.438592
9.293490	630.751555	10.443610
9.439174	635.482680	10.448627
9.416418	627.765359	10.453645
9.491230	615.436755	10.458663
9.429624	615.660599	10.463680
9.161728	620.046752	10.468698
9.078709	617.705784	10.473715
9.179756	631.508160	10.478733
9.615160	642.522596	10.483751
9.418168	643.868526	10.488768
9.370117	644.559440	10.493786
9.468124	642.917265	10.498803
9.275808	647.681518	10.503821
9.213022	653.194313	10.508839
9.583304	655.303733	10.513856
9.343003	647.478283	10.518874
9.177245	644.784511	10.523891
9.253073	647.465729	10.528909
9.427440	648.203239	10.533927
9.227937	646.033753	10.538944
9.483078	652.009668	10.543962
9.502415	644.486824	10.548979
9.584735	640.196519	10.553997
9.511478	635.157944	10.559015
9.756591	652.510224	10.564032
9.536950	653.799770	10.569050
9.715230	650.198797	10.574067
9.645884	646.555887	10.579085
9.433832	661.808117	10.584103
10.324809	648.374502	10.589120
9.975217	649.232648	10.594138
9.825532	642.235682	10.599155
9.736146	653.996481	10.604173
9.681739	638.539951	10.609191
9.653350	619.941986	10.614208
9.201616	628.207261	10.619226
9.519250	635.613438	10.624243
9.667340	635.426612	10.629261
9.356815	646.795776	10.634279
9.817243	645.038305	10.639296
9.425550	639.669348	10.644314
9.651324	642.720303	10.649331
9.363357	637.732955	10.654349
9.497896	642.483146	10.659367
9.675566	644.580702	10.664384
9.451600	653.697173	10.669402
9.880085	649.097242	10.674419
9.799120	637.278729	10.679437
9.582459	633.098256	10.684455
9.887867	637.706448	10.689472
9.937136	652.621933	10.694490
10.117766	643.234267	10.699507
9.782422	640.647248	10.704525
9.768831	640.684941	10.709543
9.916806	639.080465	10.714560
9.459565	648.369811	10.719578
9.564222	655.429566	10.724595
9.291249	653.184244	10.729613
9.482311	652.496012	10.734631
9.651485	647.734934	10.739648
9.705880	658.383875	10.744666
10.059069	670.800263	10.749683
9.972973	661.980491	10.754701
9.648268	661.734321	10.759719
9.800323	653.948636	10.764736
9.738276	664.070068	10.769754
9.969474	669.405470	10.774771
10.181027	663.769225	10.779789
9.998633	670.684528	10.784807
10.070600	642.935195	10.789824
9.396255	654.628320	10.794842
9.757959	651.277007	10.799859
9.998212	667.080964	10.804877
9.877845	674.223772	10.809895
10.096170	674.875686	10.814912
10.232260	672.502339	10.819930
9.942893	667.725511	10.824947
10.314496	670.701693	10.829965
10.128992	660.049847	10.834983
10.211783	648.682134	10.840000
10.004954	647.427088	10.845018
10.131239	643.676862	10.850035
9.897630	634.940036	10.855053
9.729387	644.922143	10.860071
10.046858	639.527020	10.865088
10.112365	654.664981	10.870106
10.343733	656.879234	10.875123
10.026812	640.700860	10.880141
9.832340	644.274532	10.885159
9.953892	631.464650	10.890176
10.049899	649.085225	10.895194
10.328508	663.744551	10.900211
10.442897	670.381124	10.905229
9.643905	660.240433	10.910247
10.176829	659.079439	10.915264
9.838673	664.571909	10.920282
10.100033	665.900846	10.925299
10.246821	665.778495	10.930317
10.218908	666.829111	10.935335
10.268672	671.764255	10.940352
10.089287	678.577113	10.945370
10.396299	669.934458	10.950387
10.436514	673.107309	10.955405
10.309009	679.607709	10.960423
10.202283	668.628129	10.965440
10.186056	660.884028	10.970458
10.081789	657.636091	10.975475
10.247311	652.680471	10.980493
10.223362	668.411574	10.985511
10.187319	667.458955	10.990528
10.224412	673.771352	10.995546
10.275658	683.145459	11.000563
10.516292	675.776351	11.005581
9.927664	673.440694	11.010599
10.190098	672.188595	11.015616
10.277706	676.754754	11.020634
10.057648	669.126798	11.025651
10.439102	662.269374	11.030669
10.060043	668.628497	11.035687
10.380036	668.325778	11.040704
10.509965	666.057959	11.045722
10.332140	671.142505	11.050739
10.530659	681.116773	11.055757
10.228430	674.822642	11.060775
10.426999	666.898381	11.065792
10.486427	672.149984	11.070810
9.969640	679.679117	11.075827
10.109019	677.095024	11.080845
10.086553	674.985043	11.085863
10.616652	675.242777	11.090880
10.629433	675.425594	11.095898
10.490394	673.940089	11.100915
10.136449	674.710191	11.105933
10.474845	692.990247	11.110951
10.520676	694.019428	11.115968
10.500466	694.219900	11.120986
10.466231	698.802264	11.126003
10.942495	688.333312	11.131021
10.485201	688.467849	11.136039
10.363585	669.494647	11.141056
10.596731	682.701419	11.146074
10.196086	686.120720	11.151091
10.709569	694.049191	11.156109
10.620308	691.616443	11.161127
10.652293	696.120158	11.166144
10.745269	697.008696	11.171162
10.637261	696.564734	11.176179
10.615353	685.015117	11.181197
10.460331	688.013774	11.186215
10.689787	688.033838	11.191232
11.099195	694.203038	11.196250
10.610395	679.055811	11.201267
10.517508	670.023611	11.206285
10.522874	683.667958	11.211303
10.611200	697.331475	11.216320
10.727243	691.914709	11.221338
10.629910	695.983573	11.226355
10.539240	698.550015	11.231373
10.913648	691.230631	11.236391
10.776448	692.686841	11.241408
10.898227	691.945304	11.246426
10.866749	699.990012	11.251443
11.000482	686.865132	11.256461
10.719569	684.554790	11.261479
10.488198	678.790588	11.266496
10.944222	687.529989	11.271514
10.775889	691.598776	11.276531
11.281562	692.587195	11.281549
10.871455	678.831844	11.286567
10.689730	663.408728	11.291584
10.436893	671.072750	11.296602
10.631238	682.916090	11.301619
10.898808	692.342431	11.306637
10.996010	694.785322	11.311655
10.603747	690.277614	11.316672
10.724608	692.518597	11.321690
10.649424	684.671056	11.326707
10.783072	684.088161	11.331725
10.625673	697.689548	11.336743
10.834527	686.913468	11.341760
10.788490	682.962419	11.346778
10.648777	679.951103	11.351795
10.892340	675.464682	11.356813
10.631866	689.926456	11.361831
10.512691	703.854939	11.366848
10.862529	724.851975	11.371866
10.914018	724.628660	11.376883
11.482130	714.079956	11.381901
11.122851	715.927139	11.386919
11.333305	718.004920	11.391936
11.172881	711.045912	11.396954
11.020103	715.099144	11.401971
11.176000	697.037368	11.406989
10.828072	691.871655	11.412007
11.079520	696.127327	11.417024
11.370954	707.270506	11.422042
10.858201	708.046384	11.427059
11.297846	711.368751	11.432077
11.203033	708.436412	11.437095
11.086670	698.371438	11.442112
11.019404	694.439049	11.447130
11.145100	701.131237	11.452147
11.324403	696.620395	11.457165
10.934473	700.352048	11.462183
10.831530	720.558104	11.467200
11.246306	713.502663	11.472218
11.248011	721.554889	11.477235
11.355682	721.184714	11.482253
11.322204	726.211965	11.487271
11.239740	715.071282	11.492288
11.288786	720.459831	11.497306
11.222083	731.587223	11.502323
11.510573	717.274733	11.507341
11.397846	704.883166	11.512359
11.235880	705.033848	11.517376
11.203241	688.739166	11.522394
11.083715	687.922958	11.527411
11.415310	705.688886	11.532429
11.187180	726.203581	11.537447
11.155318	738.329777	11.542464
11.550572	726.161282	11.547482
11.628125	730.050295	11.552499
11.228387	705.674708	11.557517
11.211026	708.243405	11.562535
11.293764	721.461879	11.567552
11.684747	710.672809	11.572570
11.597095	722.669653	11.577587
11.359102	707.522873	11.582605
11.510581	706.977771	11.587623
11.117516	702.091515	11.592640
11.539261	701.026240	11.597658
11.521997	716.814153	11.602675
11.668531	712.303408	11.607693
11.417159	704.379283	11.612711
11.503137	710.779861	11.617728
11.531646	693.496886	11.622746
10.847909	702.542933	11.627763
11.015469	710.414227	11.632781
11.238965	720.101173	11.637799
11.280497	725.417355	11.642816
11.875907	726.024277	11.647834
11.504268	729.092197	11.652851
11.483977	718.276024	11.657869
11.455788	720.699096	11.662887
11.369546	725.468576	11.667904
11.847986	726.027516	11.672922
11.504394	726.384364	11.677939
11.341707	721.262033	11.682957
11.772825	719.999572	11.687975
11.785017	729.668892	11.692992
11.943522	710.839867	11.698010
11.538572	722.367776	11.703027
11.547287	724.254918	11.708045
11.696051	715.410475	11.713063
11.370049	728.263503	11.718080
11.486310	716.151947	11.723098
11.733387	723.211816	11.728115
11.545916	708.854977	11.733133
11.781710	723.781137	11.738151
11.676363	722.805720	11.743168
12.031266	736.767289	11.748186
11.432996	728.346436	11.753203
11.728153	735.122821	11.758221
12.291936	737.183940	11.763239
12.156153	726.943643	11.768256
12.289650	713.860505	11.773274
12.042575	724.885438	11.778291
12.209548	715.824636	11.783309
11.961985	715.812328	11.788327
12.026446	722.351876	11.793344
12.182206	713.410231	11.798362
12.079940	713.175914	11.803379
12.267126	710.089511	11.808397
12.021208	693.264416	11.813415
11.553314	697.042608	11.818432
11.476740	687.798878	11.823450
11.792433	692.105143	11.828467
11.823570	704.894607	11.833485
11.961997	713.622148	11.838503
11.478978	725.678032	11.843520
12.000305	720.773318	11.848538
11.722910	721.086555	11.853555
11.802176	716.969342	11.858573
12.025993	716.941724	11.863591
11.376735	720.531229	11.868608
11.878671	721.772194	11.873626
11.834530	726.405211	11.878643
12.093811	726.114689	11.883661
11.953560	718.187151	11.888679
11.716388	724.711007	11.893696
12.094012	733.210086	11.898714
12.292972	748.885344	11.903731
12.105000	742.608321	11.908749
12.428261	737.676894	11.913767
12.110148	736.347332	11.918784
12.013799	725.556319	11.923802
12.130837	730.408723	11.928819
12.243140	738.935315	11.933837
12.187012	735.950720	11.938855
11.767199	741.990087	11.943872
12.106261	746.852451	11.948890
12.338552	745.445512	11.953907
12.389641	746.784209	11.958925
12.318195	743.455547	11.963943
11.968432	754.433309	11.968960
12.200625	747.127757	11.973978
11.978759	746.054094	11.978995
11.910708	738.856224	11.984013
12.379556	728.807298	11.989031
12.186386	738.998077	11.994048
12.310155	737.153834	11.999066
12.307734	743.818401	12.004083
12.273885	744.951879	12.009101
12.437613	743.670622	12.014119
12.111245	734.161502	12.019136
12.027589	744.559741	12.024154
12.247468	744.771120	12.029171
12.201847	752.281471	12.034189
12.293770	732.170133	12.039207
12.526269	737.450038	12.044224
12.419385	730.208401	12.049242
12.475098	737.908460	12.054259
12.155640	750.710434	12.059277
12.494101	733.570059	12.064295
12.278245	739.941408	12.069312
12.457986	737.314618	12.074330
12.515801	742.464757	12.079347
12.269620	750.862045	12.084365
12.648290	745.047392	12.089383
12.617395	763.664891	12.094400
12.727604	754.357780	12.099418
12.516329	748.695134	12.104435
12.479027	740.737582	12.109453
12.671759	739.434409	12.114471
12.428533	751.628216	12.119488
12.768898	746.880346	12.124506
12.527686	736.290400	12.129523
12.705221	742.417046	12.134541
12.797861	741.588801	12.139559
12.592513	751.134465	12.144576
12.600535	748.660637	12.149594
12.515044	738.286058	12.154611
12.342809	746.356019	12.159629
12.496062	752.671887	12.164647
12.348036	775.940668	12.169664
12.665456	770.629944	12.174682
13.235846	768.097424	12.179699
12.507917	770.570993	12.184717
12.965545	770.839524	12.189735
12.901849	772.637474	12.194752
12.659489	761.557820	12.199770
13.016627	761.315092	12.204787
12.622060	756.153325	12.209805
12.711458	743.687191	12.214823
12.709539	758.185422	12.219840
12.697259	766.740293	12.224858
12.713580	766.651508	12.229875
12.873165	776.423054	12.234893
12.769984	763.252826	12.239911
12.737129	781.974591	12.244928
12.653078	777.057124	12.249946
12.703623	773.490418	12.254963
12.595726	764.600580	12.259981
12.517199	770.091121	12.264999
12.654604	780.050163	12.270016
13.087704	768.789995	12.275034
13.359958	771.124849	12.280051
13.232740	779.732378	12.285069
13.038642	762.046421	12.290087
12.585875	772.500755	12.295104
12.950420	774.403301	12.300122
13.377944	765.861721	12.305139
13.043261	777.859871	12.310157
13.024569	767.166607	12.315175
12.977574	771.348608	12.320192
12.988839	770.963858	12.325210
12.918533	770.681155	12.330227
12.765624	775.248710	12.335245
13.106681	761.816125	12.340263
12.974760	769.275401	12.345280
12.689779	773.122187	12.350298
13.091402	779.635171	12.355315
12.782505	773.251368	12.360333
12.947829	774.646768	12.365351
13.136982	778.766325	12.370368
13.296461	783.287770	12.375386
13.772087	791.619924	12.380403
12.958137	783.112065	12.385421
13.453884	764.138873	12.390439
13.335566	751.305352	12.395456
13.209931	764.197728	12.400474
13.396135	754.645420	12.405491
12.948717	762.722091	12.410509
13.263245	757.338436	12.415527
13.130916	768.281063	12.420544
13.223154	764.241995	12.425562
13.461796	773.583417	12.430579
13.202500	776.387547	12.435597
13.410560	777.958925	12.440615
13.332060	770.995405	12.445632
13.312614	770.993423	12.450650
13.553536	760.648339	12.455667
13.365617	772.429349	12.460685
13.345617	757.034523	12.465703
13.279437	763.549426	12.470720
13.347109	765.860813	12.475738
13.708247	772.926458	12.480755
13.554736	781.588522	12.485773
13.679831	766.278745	12.490791
13.625207	774.699697	12.495808
13.253416	773.854712	12.500826
13.661557	758.082883	12.505843
13.110802	766.776338	12.510861
13.525472	763.070340	12.515879
13.424125	762.716205	12.520896
13.180253	781.298854	12.525914
13.469525	774.717201	12.530931
13.097299	787.582248	12.535949
13.442897	782.545754	12.540967
13.784862	787.790463	12.545984
13.500963	793.817034	12.551002
14.170272	791.953486	12.556019
14.157183	795.367810	12.561037
13.566796	777.537122	12.566055
13.969608	763.793198	12.571072
13.723161	770.042667	12.576090
14.051868	766.731324	12.581107
13.788288	763.930980	12.586125
13.741122	762.005551	12.591143
13.772192	766.941256	12.596160
13.450976	768.718583	12.601178
14.127923	770.877523	12.606195
13.790723	770.772368	12.611213
13.816039	764.057006	12.616231
13.670577	764.342734	12.621248
13.644614	762.118967	12.626266
14.041436	762.861250	12.631283
13.760483	774.289193	12.636301
13.810302	766.093842	12.641319
14.007893	767.296735	12.646336
13.667624	762.929600	12.651354
13.778818	754.360197	12.656371
13.678773	764.444674	12.661389
13.746931	768.566707	12.666407
13.946712	767.405847	12.671424
13.447963	766.048663	12.676442
13.968349	760.986440	12.681459
13.861832	762.736159	12.686477
13.869288	768.758266	12.691495
13.840967	766.288866	12.696512
13.775039	768.602453	12.701530
14.178131	777.350260	12.706547
14.111277	781.703628	12.711565
14.127727	777.599732	12.716583
14.400180	768.178414	12.721600
14.071991	766.514742	12.726618
14.266999	771.312156	12.731635
13.657795	778.491117	12.736653
13.777977	774.127009	12.741671
14.007383	773.274981	12.746688
13.926381	787.287571	12.751706
13.896387	789.899898	12.756723
14.188599	787.141343	12.761741
14.086779	788.456895	12.766759
14.649529	790.186554	12.771776
14.037540	787.577815	12.776794
14.385967	775.713823	12.781811
14.154526	776.732145	12.786829
13.817558	776.593099	12.791847
14.065803	791.436769	12.796864
13.970065	792.131929	12.801882
14.172568	792.257218	12.806899
14.350566	798.322009	12.811917
14.265632	786.783518	12.816935
14.276828	782.683637	12.821952
13.970916	789.915813	12.826970
13.778756	788.388493	12.831987
13.911837	790.578857	12.837005
13.970347	791.495140	12.842023
14.146422	793.789208	12.847040
14.185486	801.252522	12.852058
14.491673	810.738686	12.857075
14.395768	813.914575	12.862093
14.317885	820.018904	12.867111
14.655504	813.073397	12.872128
14.523438	815.657722	12.877146
14.339977	795.538668	12.882163
14.096982	798.150375	12.887181
14.385647	805.858421	12.892199
14.955692	814.041148	12.897216
14.525992	806.087591	12.902234
14.530996	800.865879	12.907251
14.452912	795.817913	12.912269
13.748027	809.837379	12.917287
14.349227	809.958386	12.922304
14.324698	823.704632	12.927322
14.525344	818.051830	12.932339
14.491554	810.183017	12.937357
14.303875	827.963454	12.942375
14.793528	814.727884	12.947392
14.709821	815.334851	12.952410
14.726804	812.652084	12.957427
14.774138	814.906613	12.962445
14.451071	818.212154	12.967463
14.865216	815.624555	12.972480
14.619152	814.290362	12.977498
14.759567	805.688350	12.982515
14.835665	815.921086	12.987533
14.218303	812.859761	12.992551
14.857750	808.505093	12.997568
14.621689	810.794054	13.002586
14.970303	803.421016	13.007603
14.964422	805.144268	13.012621
14.766991	812.238665	13.017639
15.186438	802.575156	13.022656
14.935797	807.856789	13.027674
15.311657	808.218152	13.032691
15.011891	798.814421	13.037709
14.827843	800.590537	13.042727
15.249919	797.446602	13.047744
15.527728	805.692182	13.052762
15.440529	794.084189	13.057779
15.299416	775.365612	13.062797
15.146257	772.351973	13.067815
15.465226	763.747835	13.072832
14.988375	769.943464	13.077850
15.349445	774.572712	13.082867
15.457253	765.405535	13.087885
15.217329	769.088796	13.092903
15.162134	751.638909	13.097920
15.201327	753.815851	13.102938
15.184717	746.970834	13.107955
15.276527	745.173792	13.112973
14.713132	760.599713	13.117991
14.967178	755.515572	13.123008
15.000836	750.165541	13.128026
15.093297	745.472219	13.133043
15.108006	740.187516	13.138061
15.098096	754.698284	13.143079
15.328885	755.572317	13.148096
14.967591	745.184856	13.153114
15.078901	756.172435	13.158131
15.342908	756.686313	13.163149
15.325135	766.560969	13.168167
15.079048	759.213406	13.173184
15.015791	771.165909	13.178202
15.451868	774.817368	13.183219
15.357249	765.220727	13.188237
15.001115	763.883865	13.193255
15.158313	766.134993	13.198272
15.165279	766.853724	13.203290
15.070572	773.940772	13.208307
15.468893	769.234490	13.213325
15.082067	766.339375	13.218343
15.369660	759.123661	13.223360
15.136471	773.609346	13.228378
15.029578	770.517798	13.233395
15.390015	769.420925	13.238413
15.156073	761.177799	13.243431
15.179811	754.943135	13.248448
15.326540	764.463887	13.253466
15.188719	775.767997	13.258483
15.682207	783.460292	13.263501
15.460419	795.948968	13.268519
15.606225	781.724159	13.273536
15.442276	786.465758	13.278554
15.314268	794.677427	13.283571
15.671773	804.071655	13.288589
15.359490	798.673674	13.293607
15.541001	802.281002	13.298624
15.515454	795.289629	13.303642
15.821142	800.443503	13.308659
16.147323	801.920376	13.313677
15.656208	802.991060	13.318695
15.955637	791.847831	13.323712
15.936549	769.341600	13.328730
15.679929	763.947029	13.333747
15.887874	764.423527	13.338765
15.567643	768.521568	13.343783
15.744575	764.744443	13.348800
15.370877	763.282552	13.353818
15.491635	765.684757	13.358835
15.805699	777.244847	13.363853
15.774373	799.379602	13.368871
15.726001	795.462368	13.373888
15.795539	794.947140	13.378906
15.909465	796.880477	13.383923
16.134376	796.476755	13.388941
15.723247	794.119225	13.393959
15.540392	800.133430	13.398976
15.570228	797.709917	13.403994
15.672923	798.836580	13.409011
16.124549	786.888213	13.414029
15.792039	803.223504	13.419047
15.954990	795.804391	13.424064
16.128508	803.885148	13.429082
15.999551	793.801133	13.434099
16.146412	781.479580	13.439117
15.868734	791.759348	13.444135
15.991039	790.864201	13.449152
15.959598	796.305048	13.454170
15.573331	803.700878	13.459187
15.986840	797.625371	13.464205
15.973468	808.789668	13.469223
15.662963	801.014809	13.474240
15.498319	800.124174	13.479258
15.493885	812.067578	13.484275
16.135876	826.144949	13.489293
15.972539	837.596015	13.494311
15.899848	827.240911	13.499328
15.826590	829.838744	13.504346
16.011542	817.094006	13.509363
15.907623	825.725658	13.514381
16.032882	834.358019	13.519399
16.401539	827.813807	13.524416
16.436022	824.077134	13.529434
16.000445	832.344374	13.534451
16.445508	820.791884	13.539469
16.305876	831.654870	13.544487
16.346919	829.119872	13.549504
16.571985	824.345370	13.554522
16.303756	819.988948	13.559539
16.469460	816.357541	13.564557
16.222123	829.997525	13.569575
16.351803	815.700755	13.574592
16.574629	814.001131	13.579610
16.299034	823.989481	13.584627
16.430787	818.963318	13.589645
16.351237	831.731028	13.594663
16.651931	829.812661	13.599680
16.529382	821.476894	13.604698
16.176521	818.359065	13.609715
16.706473	825.232297	13.614733
16.506535	825.300687	13.619751
16.722925	839.719028	13.624768
16.727443	828.869548	13.629786
16.490806	826.297774	13.634803
16.777532	825.810029	13.639821
16.815717	824.740032	13.644839
16.455345	829.181480	13.649856
16.360552	817.939036	13.654874
16.469781	830.808991	13.659891
16.994535	836.649002	13.664909
16.696154	836.282944	13.669927
16.675822	828.709488	13.674944
16.866083	817.471111	13.679962
16.359289	817.149926	13.684979
16.818163	838.145042	13.689997
16.942857	844.134027	13.695015
16.804947	837.428090	13.700032
17.052335	836.708499	13.705050
16.799497	832.266079	13.710067
16.926634	814.819645	13.715085
16.985411	809.923242	13.720103
16.484400	816.116781	13.725120
16.867013	831.394313	13.730138
16.656857	856.811528	13.735155
17.243758	843.603360	13.740173
17.175108	847.812383	13.745191
16.924663	843.880900	13.750208
16.979734	826.137947	13.755226
16.831337	826.411171	13.760243
16.904896	839.538169	13.765261
16.887165	846.484007	13.770279
16.801506	849.410809	13.775296
16.853127	834.985212	13.780314
16.547217	847.935791	13.785331
16.949969	846.068065	13.790349
16.936691	852.633900	13.795367
16.822302	847.846797	13.800384
16.984984	848.158955	13.805402
16.979329	842.219026	13.810419
17.215051	841.350796	13.815437
17.194457	844.997634	13.820455
17.310404	850.553294	13.825472
17.010384	840.892926	13.830490
17.061979	845.922691	13.835507
17.275280	844.334068	13.840525
17.230698	843.585573	13.845543
16.947079	851.724184	13.850560
17.635512	847.004774	13.855578
17.219384	859.216414	13.860595
17.138117	851.669746	13.865613
17.025489	855.672489	13.870631
17.549145	876.864203	13.875648
17.586103	870.969772	13.880666
17.108262	858.605746	13.885683
17.564296	864.809823	13.890701
17.593447	864.379405	13.895719
17.357022	864.348329	13.900736
17.302173	853.693258	13.905754
17.319440	853.127227	13.910771
17.522046	877.610262	13.915789
17.739461	884.747734	13.920807
17.684833	870.893117	13.925824
17.891101	854.181672	13.930842
17.370130	849.238172	13.935859
17.496442	846.092324	13.940877
17.385794	840.411047	13.945895
17.346612	838.482517	13.950912
17.803411	862.944385	13.955930
17.773518	866.355991	13.960947
17.867558	848.451873	13.965965
17.543104	838.572745	13.970983
17.457570	851.175345	13.976000
17.652410	841.594197	13.981018
17.553525	860.421640	13.986035
17.749348	858.261389	13.991053
18.040152	871.968755	13.996071
17.466743	858.629537	14.001088
17.979588	867.240576	14.006106
18.059773	852.822641	14.011123
17.718377	842.195840	14.016141
17.734214	840.295219	14.021159
17.672410	850.999121	14.026176
18.048201	859.112612	14.031194
18.242106	862.405554	14.036211
17.877478	844.964970	14.041229
17.879710	837.896164	14.046247
17.588160	847.865713	14.051264
17.966579	842.765714	14.056282
17.733668	856.189790	14.061299
17.835201	865.762555	14.066317
18.123139	868.534133	14.071335
17.926477	864.910439	14.076352
18.388001	859.297765	14.081370
18.033883	870.809512	14.086387
18.169391	870.601243	14.091405
18.099995	857.160628	14.096423
18.157796	861.699293	14.101440
18.109103	838.215922	14.106458
18.380300	846.619679	14.111475
17.706616	837.530233	14.116493
18.007591	847.921271	14.121511
17.984230	859.895985	14.126528
18.046201	861.618462	14.131546
17.956152	867.693723	14.136563
17.968249	863.183894	14.141581
18.303843	858.998894	14.146599
18.285795	870.244508	14.151616
18.301036	865.108470	14.156634
18.203255	866.984886	14.161651
18.317785	868.961039	14.166669
18.373648	861.476534	14.171687
18.383791	860.245840	14.176704
18.354569	868.371157	14.181722
18.326943	866.757199	14.186739
18.167331	872.878991	14.191757
18.531027	859.535282	14.196775
18.134698	864.662888	14.201792
18.592843	860.988851	14.206810
18.405961	859.414005	14.211827
18.252722	860.336942	14.216845
18.652762	856.854959	14.221863
18.266123	866.396997	14.226880
18.165927	857.610541	14.231898
18.148952	865.321102	14.236915
18.577327	873.014558	14.241933
18.923499	885.586980	14.246951
18.698200	870.605827	14.251968
18.556653	862.725075	14.256986
18.592490	864.258004	14.262003
18.792262	851.343099	14.267021
19.082567	853.714347	14.272039
18.528162	861.865434	14.277056
18.370901	857.423745	14.282074
18.680878	857.996556	14.287091
18.628298	884.324635	14.292109
18.853414	891.573418	14.297127
18.650052	889.187247	14.302144
18.989621	894.576855	14.307162
19.083501	881.371007	14.312179
18.792902	877.802197	14.317197
19.079832	858.232985	14.322215
18.683523	859.826699	14.327232
18.767209	863.340185	14.332250
19.176026	863.429807	14.337267
18.786501	859.838182	14.342285
18.942075	849.913967	14.347303
18.849796	861.278714	14.352320
19.040159	875.349871	14.357338
19.120510	879.460865	14.362355
18.457662	866.679051	14.367373
18.625305	881.755384	14.372391
18.644591	885.450948	14.377408
18.712637	884.015242	14.382426
18.976798	894.487973	14.387443
18.648205	882.601941	14.392461
18.814552	883.410069	14.397479
18.433354	892.981928	14.402496
18.802230	905.210117	14.407514
19.023540	901.992465	14.412531
19.268147	909.947375	14.417549
19.118816	903.993376	14.422567
19.075336	909.848983	14.427584
19.124235	908.460724	14.432602
19.129832	916.983005	14.437619
19.326172	912.450391	14.442637
19.435522	900.950760	14.447655
19.439969	912.488507	14.452672
19.359437	906.053723	14.457690
19.391612	908.680005	14.462707
19.355274	911.353037	14.467725
19.343041	908.059430	14.472743
19.655447	907.500521	14.477760
19.604960	898.829822	14.482778
19.678131	898.223847	14.487795
19.180096	911.355221	14.492813
19.589484	901.987559	14.497831
19.606706	904.673389	14.502848
19.670849	907.878353	14.507866
19.968892	897.891003	14.512883
19.570421	901.803024	14.517901
19.610224	903.693710	14.522919
19.422141	913.804447	14.527936
19.617264	901.886766	14.532954
19.705418	904.996240	14.537971
19.371667	899.968249	14.542989
19.794283	895.703711	14.548007
19.521390	894.269827	14.553024
19.290919	905.901303	14.558042
19.795439	902.944676	14.563059
20.102707	895.530402	14.568077
20.064894	897.574444	14.573095
20.151713	890.931330	14.578112
20.048545	906.697812	14.583130
20.143294	893.449297	14.588147
19.308943	896.392762	14.593165
19.589628	893.606571	14.598183
20.121959	901.029555	14.603200
19.982600	896.515813	14.608218
20.035411	898.749571	14.613235
19.970063	907.183980	14.618253
19.949050	906.371950	14.623271
20.044116	899.327532	14.628288
19.889381	899.012526	14.633306
20.297815	889.503909	14.638323
19.896762	890.004683	14.643341
19.943729	896.637538	14.648359
19.967278	889.099116	14.653376
20.248941	897.564350	14.658394
20.344576	893.796692	14.663411
20.058886	889.151449	14.668429
20.191843	890.900185	14.673447
20.009359	886.160538	14.678464
20.148960	893.438412	14.683482
20.115494	910.220778	14.688499
20.052040	902.417244	14.693517
20.240908	902.841592	14.698535
20.245669	904.991573	14.703552
20.014771	901.037754	14.708570
19.854500	907.838107	14.713587
19.969021	906.964709	14.718605
20.139764	903.342879	14.723623
20.125345	895.084858	14.728640
19.742705	901.109287	14.733658
20.046068	894.519743	14.738675
20.024677	929.291034	14.743693
20.590908	936.914308	14.748711
20.312178	937.637746	14.753728
20.811214	942.040339	14.758746
20.743227	924.553399	14.763763
20.852746	925.848603	14.768781
20.824441	919.214070	14.773799
20.735635	900.169422	14.778816
20.824709	906.343031	14.783834
20.838298	906.257256	14.788851
20.603391	901.055671	14.793869
20.439096	892.308916	14.798887
20.409292	881.899451	14.803904
20.268038	892.987910	14.808922
20.707389	890.107202	14.813939
20.371812	896.118341	14.818957
20.394722	908.962279	14.823975
20.828189	916.907436	14.828992
20.922583	923.931812	14.834010
20.964699	921.046085	14.839027
21.009798	928.598214	14.844045
20.824044	907.168374	14.849063
20.826575	903.148621	14.854080
20.647325	896.372927	14.859098
20.648182	896.480170	14.864115
20.685196	913.100325	14.869133
20.529769	922.427445	14.874151
20.451809	928.327334	14.879168
20.421293	926.954361	14.884186
21.145548	926.543894	14.889203
21.079776	931.799350	14.894221
20.933419	922.609917	14.899239
20.617582	922.262881	14.904256
20.795863	928.545163	14.909274
20.896350	925.064840	14.914291
20.675915	933.265876	14.919309
20.866525	951.741110	14.924327
21.877181	955.357103	14.929344
21.349804	943.868384	14.934362
21.457014	924.153617	14.939379
21.234289	925.956017	14.944397
21.194639	922.188861	14.949415
21.072478	923.444606	14.954432
21.197057	917.517964	14.959450
21.243786	916.237133	14.964467
20.864438	918.223264	14.969485
21.139894	933.868553	14.974503
21.152895	947.086150	14.979520
20.726121	957.274149	14.984538
21.360078	944.085871	14.989555
21.385124	948.602419	14.994573
21.417415	951.372762	14.999591
21.436256	941.419124	15.004608
21.624853	956.898306	15.009626
21.692948	956.028247	15.014643
21.324460	962.246984	15.019661
21.519849	951.520970	15.024679
21.304133	943.658337	15.029696
21.131612	953.740941	15.034714
21.411672	946.178013	15.039731
21.328688	952.368658	15.044749
21.489977	951.931162	15.049767
21.505382	948.776067	15.054784
21.365366	953.848553	15.059802
21.612934	966.870735	15.064819
21.556368	979.503884	15.069837
21.800606	981.657405	15.074855
21.970319	977.370475	15.079872
21.972111	981.789906	15.084890
21.727449	959.856419	15.089907
21.811708	968.869000	15.094925
21.873593	975.498045	15.099943
21.780329	966.070911	15.104960
21.905828	985.169450	15.109978
22.198470	972.230043	15.114995
21.830566	962.286569	15.120013
21.622674	948.934696	15.125031
21.973244	956.124398	15.130048
21.692490	973.279144	15.135066
21.683622	982.073692	15.140083
22.062946	971.479842	15.145101
21.960503	964.184809	15.150119
22.021416	963.691273	15.155136
21.819148	973.646740	15.160154
22.266763	978.940779	15.165171
22.047911	975.827342	15.170189
21.677485	970.977803	15.175207
21.969725	969.469416	15.180224
21.938917	983.498099	15.185242
22.053854	963.853057	15.190259
22.228461	971.566258	15.195277
22.163987	973.265162	15.200295
22.454300	974.041197	15.205312
22.104563	975.401276	15.210330
22.227510	973.221758	15.215347
22.180466	969.197780	15.220365
22.391644	974.019747	15.225383
22.649994	970.070676	15.230400
22.374358	971.829274	15.235418
22.372580	965.108461	15.240435
22.510166	965.893004	15.245453
22.356831	967.592618	15.250471
22.686951	970.758758	15.255488
22.644594	970.774733	15.260506
22.299227	968.696028	15.265523
22.609222	972.753352	15.270541
22.246243	969.349805	15.275559
22.386839	969.392625	15.280576
22.432189	981.658789	15.285594
22.674147	988.224426	15.290611
22.947423	992.535425	15.295629
22.644063	984.100334	15.300647
22.618771	971.628759	15.305664
22.508636	978.532849	15.310682
22.818043	987.619438	15.315699
22.866195	994.367672	15.320717
22.578108	993.665314	15.325735
22.812597	990.858593	15.330752
22.556134	993.169060	15.335770
22.632827	984.044685	15.340787
22.657224	992.728837	15.345805
22.690121	1001.264564	15.350823
23.231558	983.128899	15.355840
22.805987	994.668882	15.360858
23.062084	998.272394	15.365875
22.996209	989.360523	15.370893
22.727484	991.788747	15.375911
22.754575	994.799094	15.380928
22.678253	991.212561	15.385946
22.963426	995.958143	15.390963
22.879614	997.672251	15.395981
22.760856	991.860388	15.400999
23.028188	989.262776	15.406016
22.714743	992.926355	15.411034
22.859489	1005.779566	15.416051
23.387058	1019.797296	15.421069
23.667260	1019.026612	15.426087
23.399449	1011.156020	15.431104
23.114252	1002.254799	15.436122
23.359534	993.917002	15.441139
23.540599	997.259726	15.446157
23.474062	995.716152	15.451175
23.520512	984.353409	15.456192
23.239895	985.064958	15.461210
23.352076	977.553769	15.466227
23.342162	974.566410	15.471245
23.283466	988.197996	15.476263
23.412317	999.671753	15.481280
23.632335	1008.924678	15.486298
23.339477	999.536018	15.491315
23.503706	999.741246	15.496333
23.487095	1011.354977	15.501351
23.534283	1013.834920	15.506368
23.574933	1027.174770	15.511386
23.782683	1018.094652	15.516403
24.151330	1002.040560	15.521421
23.935068	995.955088	15.526439
23.709335	973.027854	15.531456
23.464926	980.306639	15.536474
23.101368	984.780739	15.541491
23.649514	995.631940	15.546509
23.732481	1012.651438	15.551527
23.890031	1011.835284	15.556544
23.628938	1013.519644	15.561562
23.450884	1016.703442	15.566579
24.023562	1014.576155	15.571597
23.837923	1002.833704	15.576615
24.226725	1007.487372	15.581632
24.252598	1019.663690	15.586650
24.044588	1002.028960	15.591667
24.131393	1006.232609	15.596685
24.039058	988.393767	15.601703
23.937709	984.849358	15.606720
24.118385	984.643071	15.611738
23.634847	992.660487	15.616755
23.713379	991.254332	15.621773
23.859153	1004.461847	15.626791
24.077127	1004.717831	15.631808
23.759970	1013.364750	15.636826
24.200586	1025.133609	15.641843
24.613763	1014.817951	15.646861
24.155643	1016.466967	15.651879
24.088033	1011.139091	15.656896
24.329829	999.810383	15.661914
24.169499	1006.056935	15.666931
24.388330	1006.925874	15.671949
24.486667	1017.208802	15.676967
24.506826	1006.214507	15.681984
24.573039	1004.376791	15.687002
24.466972	1004.796936	15.692019
24.746747	1011.361255	15.697037
24.451671	1008.194275	15.702055
24.077805	1006.321228	15.707072
24.528390	1005.848914	15.712090
24.068410	1012.863777	15.717107
24.557352	1009.022238	15.722125
24.164730	1004.375146	15.727143
24.059157	1002.773661	15.732160
24.658501	1010.219281	15.737178
24.589542	1011.707741	15.742195
24.453984	1011.296074	15.747213
24.832245	1029.058800	15.752231
24.916704	1030.450856	15.757248
24.627453	1019.093571	15.762266
24.574531	1031.933216	15.767283
24.772019	1021.534317	15.772301
24.941552	1016.887813	15.777319
24.967589	1025.632727	15.782336
25.105410	1029.883849	15.787354
24.489037	1022.404465	15.792371
24.782998	1016.703496	15.797389
24.865497	1029.660308	15.802407
24.804052	1021.992777	15.807424
25.149824	1020.229316	15.812442
24.773672	1034.230678	15.817459
25.138659	1024.362480	15.822477
25.042458	1029.885754	15.827495
25.283347	1022.161767	15.832512
24.981433	1022.669978	15.837530
25.023704	1025.279850	15.842547
25.014708	1018.034693	15.847565
25.353454	1032.329468	15.852583
25.171459	1035.753257	15.857600
25.181601	1029.431765	15.862618
24.838715	1023.267811	15.867635
25.302116	1027.253547	15.872653
25.413684	1023.219877	15.877671
25.350683	1023.002881	15.882688
25.264358	1033.934158	15.887706
25.303047	1030.511064	15.892723
25.607242	1013.763581	15.897741
25.546630	1018.520256	15.902759
25.525440	1019.567226	15.907776
25.739257	1021.350442	15.912794
25.259567	1024.802757	15.917811
25.698723	1027.010085	15.922829
25.440915	1025.623097	15.927847
25.359388	1021.963413	15.932864
25.676457	1022.631894	15.937882
25.176070	1031.662398	15.942899
25.538732	1033.274190	15.947917
25.418203	1031.735007	15.952935
25.125893	1031.695255	15.957952
25.521471	1020.038999	15.962970
25.363702	1015.720361	15.967987
25.412834	1031.170114	15.973005
25.509129	1059.191157	15.978023
25.809425	1057.262594	15.983040
26.225304	1047.316493	15.988058
25.735006	1050.605827	15.993075
26.114014	1049.416904	15.998093
25.910381	1056.976149	16.003111
25.922409	1055.435725	16.008128
26.209261	1051.281166	16.013146
25.943766	1044.032919	16.018163
25.714635	1047.892980	16.023181
25.717544	1054.439496	16.028199
25.727422	1058.066784	16.033216
25.806035	1048.264789	16.038234
25.646569	1056.384960	16.043251
25.899308	1043.119852	16.048269
25.937410	1060.639658	16.053287
25.937911	1060.969764	16.058304
26.503828	1055.092954	16.063322
26.314800	1058.667495	16.068339
26.179995	1047.881231	16.073357
26.111828	1051.034281	16.078375
26.185060	1054.796550	16.083392
26.251183	1053.096815	16.088410
26.263424	1069.058731	16.093427
26.394226	1080.764279	16.098445
26.544768	1078.792557	16.103463
26.628693	1074.948258	16.108480
26.939114	1056.409408	16.113498
26.559690	1062.311731	16.118515
26.675373	1050.772562	16.123533
26.532905	1046.504725	16.128551
26.257713	1038.669389	16.133568
26.434398	1035.920434	16.138586
26.176853	1047.500397	16.143603
26.326189	1055.314259	16.148621
26.403638	1067.010309	16.153639
26.510004	1072.769770	16.158656
26.703316	1059.151726	16.163674
26.664628	1074.932131	16.168691
26.708311	1070.310147	16.173709
27.146083	1066.346558	16.178727
26.994911	1071.127662	16.183744
27.417827	1068.028804	16.188762
27.041166	1065.924552	16.193779
26.872756	1048.125177	16.198797
27.210472	1046.160908	16.203815
26.566446	1044.282114	16.208832
27.141737	1039.166051	16.213850
26.805951	1035.288969	16.218867
26.865656	1050.635041	16.223885
26.897687	1058.892441	16.228903
26.772111	1060.860469	16.233920
27.483669	1068.270255	16.238938
27.258913	1068.681870	16.243955
27.492073	1061.532483	16.248973
27.323990	1039.734039	16.253991
27.081454	1034.938137	16.259008
27.135331	1032.377169	16.264026
27.026097	1030.591077	16.269043
27.099069	1045.569651	16.274061
27.368659	1047.519022	16.279079
27.135421	1054.415934	16.284096
27.491038	1070.210493	16.289114
27.144985	1057.697576	16.294131
27.192699	1064.474257	16.299149
27.322631	1053.945181	16.304167
27.730648	1069.283902	16.309184
27.520597	1057.918420	16.314202
27.565429	1066.833455	16.319219
27.659216	1069.054562	16.324237
27.527470	1059.362114	16.329255
27.350208	1059.111645	16.334272
27.438241	1061.137864	16.339290
27.315040	1063.963446	16.344307
27.745775	1061.114639	16.349325
27.754798	1068.582852	16.354343
27.254968	1075.168367	16.359360
27.603416	1066.176174	16.364378
27.637786	1056.248040	16.369395
27.575471	1058.172745	16.374413
27.595429	1057.987309	16.379431
27.511377	1069.292196	16.384448
28.127235	1074.971203	16.389466
28.147544	1075.525562	16.394483
28.114835	1078.745779	16.399501
27.800145	1054.042044	16.404519
27.850821	1068.744641	16.409536
28.074002	1067.485812	16.414554
28.022122	1073.015948	16.419571
27.807038	1085.508080	16.424589
27.900316	1089.137733	16.429607
28.326333	1095.349425	16.434624
28.260420	1083.626884	16.439642
28.287497	1086.340641	16.444659
28.125192	1087.937041	16.449677
28.457277	1087.505170	16.454695
28.227772	1086.516394	16.459712
28.047507	1083.175724	16.464730
28.152475	1090.100806	16.469747
28.014091	1084.735787	16.474765
28.133739	1085.014122	16.479783
28.166643	1087.493683	16.484800
28.517973	1086.550241	16.489818
28.360388	1088.951453	16.494835
28.289477	1085.120535	16.499853
28.509859	1077.280438	16.504871
28.349683	1095.383955	16.509888
28.359838	1088.088363	16.514906
28.346264	1088.417646	16.519923
27.959164	1089.075349	16.524941
28.420016	1088.343106	16.529959
28.534391	1105.205570	16.534976
28.499640	1095.285881	16.539994
28.594842	1106.503308	16.545011
28.630953	1110.490001	16.550029
28.680771	1103.893849	16.555047
28.643565	1107.243537	16.560064
28.815765	1095.696766	16.565082
29.173931	1101.586453	16.570099
28.613164	1096.409914	16.575117
29.028257	1102.624004	16.580135
28.836149	1099.083348	16.585152
28.630645	1098.650957	16.590170
29.241637	1091.655624	16.595187
28.763306	1104.810083	16.600205
29.070020	1090.303513	16.605223
28.817608	1095.372772	16.610240
29.106757	1091.883082	16.615258
29.054231	1093.935092	16.620275
28.911981	1099.519536	16.625293
29.148014	1098.842158	16.630311
28.969620	1123.221641	16.635328
29.279103	1136.350255	16.640346
29.763326	1129.495325	16.645363
29.313222	1126.617681	16.650381
29.489592	1096.658460	16.655399
29.450942	1099.966856	16.660416
29.224630	1088.408003	16.665434
29.037307	1089.394058	16.670451
29.148131	1114.184722	16.675469
29.311558	1119.113627	16.680487
29.244342	1127.189854	16.685504
29.255219	1127.075396	16.690522
29.215637	1113.653839	16.695539
29.182763	1117.123466	16.700557
29.304388	1128.413303	16.705575
29.423875	1129.891693	16.710592
30.089276	1142.637921	16.715610
30.305131	1128.291389	16.720627
30.197350	1132.577418	16.725645
30.276037	1120.119637	16.730663
29.949416	1127.491790	16.735680
29.721764	1126.875881	16.740698
29.811154	1126.211319	16.745715
29.821663	1132.384421	16.750733
30.169195	1123.513196	16.755751
30.047814	1116.893368	16.760768
29.792805	1125.897351	16.765786
30.112737	1120.330223	16.770803
30.302227	1131.288224	16.775821
30.424818	1131.248008	16.780839
29.588412	1119.084539	16.785856
29.430273	1121.050279	16.790874
29.982481	1114.956256	16.795891
29.406608	1121.522668	16.800909
29.725147	1119.976068	16.805927
30.179481	1149.815404	16.810944
30.040689	1148.886032	16.815962
30.215039	1143.950152	16.820979
30.329030	1142.934722	16.825997
30.431534	1139.907891	16.831015
30.396965	1150.083362	16.836032
30.187647	1152.881858	16.841050
30.239462	1149.626820	16.846067
30.361418	1149.593598	16.851085
30.290985	1153.630582	16.856103
30.389327	1154.044901	16.861120
30.324819	1156.425625	16.866138
30.425271	1143.139147	16.871155
30.138829	1148.838959	16.876173
29.990041	1156.052033	16.881191
30.581795	1164.206365	16.886208
30.721096	1179.274291	16.891226
31.172230	1175.451164	16.896243
30.892321	1176.660369	16.901261
31.031786	1162.832462	16.906279
31.044974	1155.079117	16.911296
30.778636	1143.366623	16.916314
30.900903	1149.866097	16.921331
30.707248	1143.572134	16.926349
30.723154	1142.523905	16.931367
30.546234	1157.665519	16.936384
30.983484	1163.737410	16.941402
31.353228	1164.187380	16.946419
31.620645	1165.300431	16.951437
31.257170	1154.025576	16.956455
31.101665	1136.082254	16.961472
30.916779	1124.460433	16.966490
31.029437	1135.969641	16.971507
30.852918	1143.182764	16.976525
31.314165	1149.819895	16.981543
31.239908	1160.605784	16.986560
31.222246	1174.131161	16.991578
31.332417	1173.174030	16.996595
31.354079	1172.317144	17.001613
31.422848	1160.881497	17.006631
31.628791	1167.921799	17.011648
31.252086	1154.729317	17.016666
31.320580	1151.985230	17.021683
31.397616	1164.311453	17.026701
31.415620	1150.534529	17.031719
31.800752	1154.089988	17.036736
31.236190	1151.785704	17.041754
31.700788	1160.987479	17.046771
31.556788	1168.264128	17.051789
31.659474	1162.734066	17.056807
31.802989	1154.547628	17.061824
31.726813	1146.277042	17.066842
31.663299	1155.428703	17.071859
31.399564	1156.003236	17.076877
31.660784	1161.096481	17.081895
31.543470	1162.317788	17.086912
31.402901	1156.121331	17.091930
31.852843	1160.154793	17.096947
31.828524	1181.537076	17.101965
31.862838	1190.794229	17.106983
32.333324	1195.533262	17.112000
31.904893	1195.139283	17.117018
32.102039	1186.543232	17.122035
31.912988	1183.140221	17.127053
32.219008	1184.652941	17.132071
32.103915	1175.506018	17.137088
31.997697	1177.739131	17.142106
31.980334	1187.309898	17.147123
32.248547	1190.401878	17.152141
32.202551	1183.831957	17.157159
32.440917	1185.038577	17.162176
32.087678	1187.217054	17.167194
32.273776	1185.493345	17.172211
32.261439	1185.538213	17.177229
32.449190	1179.082992	17.182247
32.281374	1183.928880	17.187264
32.482221	1176.411406	17.192282
32.451454	1179.870661	17.197299
32.439252	1193.080038	17.202317
32.928578	1208.110029	17.207335
32.790632	1190.616830	17.212352
32.722349	1191.075809	17.217370
32.593405	1181.907158	17.222387
32.770365	1189.254777	17.227405
32.489729	1179.466402	17.232423
32.817349	1196.636003	17.237440
33.040231	1208.254592	17.242458
32.943414	1197.834926	17.247475
33.039223	1188.083733	17.252493
32.658745	1172.963384	17.257511
32.749690	1172.491647	17.262528
32.828137	1200.505467	17.267546
32.968840	1204.220407	17.272563
33.350620	1206.492945	17.277581
33.087098	1207.379804	17.282599
33.492600	1207.133803	17.287616
33.176907	1196.665870	17.292634
33.401661	1189.213328	17.297651
33.120996	1177.558286	17.302669
33.071912	1184.260870	17.307687
33.151355	1184.664929	17.312704
33.376563	1200.716378	17.317722
33.768297	1201.278842	17.322739
33.487727	1191.070033	17.327757
33.185211	1188.012301	17.332775
33.450820	1175.953251	17.337792
33.080807	1175.534070	17.342810
33.028775	1184.793481	17.347827
33.428183	1203.329187	17.352845
33.414017	1203.600311	17.357863
33.773464	1193.558141	17.362880
33.440856	1199.168370	17.367898
33.397117	1198.409876	17.372915
33.494841	1201.036202	17.377933
33.609193	1200.113807	17.382951
33.532772	1196.670136	17.387968
33.610124	1204.698699	17.392986
33.888032	1208.066011	17.398003
33.814051	1189.466722	17.403021
33.533938	1207.530159	17.408039
33.869806	1223.665299	17.413056
33.948973	1224.169392	17.418074
34.156953	1227.811024	17.423091
34.086280	1225.842576	17.428109
34.128568	1223.974541	17.433127
34.438988	1225.828617	17.438144
34.058856	1222.592982	17.443162
34.335847	1219.393816	17.448179
34.316971	1207.064670	17.453197
34.162484	1210.810679	17.458215
34.188026	1200.573914	17.463232
34.380903	1217.230641	17.468250
34.355091	1216.683328	17.473267
33.922943	1213.000446	17.478285
34.158353	1226.328755	17.483303
34.465788	1216.154436	17.488320
34.577923	1226.549186	17.493338
34.704678	1222.751111	17.498355
34.181752	1224.829698	17.503373
34.140327	1222.473989	17.508391
34.216029	1222.498404	17.513408
34.178235	1221.326384	17.518426
34.376534	1218.945428	17.523443
34.459982	1226.650794	17.528461
34.425998	1239.440246	17.533479
34.804759	1252.341202	17.538496
35.136538	1248.892851	17.543514
34.828745	1253.507005	17.548531
35.352015	1248.630345	17.553549
35.258746	1241.745420	17.558567
35.185755	1229.284469	17.563584
34.903718	1228.296688	17.568602
34.882949	1221.064403	17.573619
34.829844	1212.850001	17.578637
34.578744	1213.054977	17.583655
34.852502	1228.759502	17.588672
34.810520	1247.938991	17.593690
34.886736	1248.457547	17.598707
35.041930	1235.311529	17.603725
34.578094	1244.306001	17.608743
35.099552	1251.723476	17.613760
34.759698	1244.436443	17.618778
35.006564	1251.867409	17.623795
35.347124	1264.717609	17.628813
35.381128	1271.899349	17.633831
35.811823	1252.908358	17.638848
35.777679	1273.897367	17.643866
35.883542	1256.236851	17.648883
35.734105	1248.827811	17.653901
35.425583	1242.130994	17.658919
35.308219	1236.104073	17.663936
35.635137	1239.067283	17.668954
35.878708	1238.123336	17.673971
35.634200	1235.340813	17.678989
35.492696	1234.056222	17.684007
36.101402	1239.793749	17.689024
35.840204	1250.201199	17.694042
35.967497	1251.637963	17.699059
35.896243	1240.363960	17.704077
35.749978	1234.834072	17.709095
35.815011	1235.745958	17.714112
35.840623	1253.732159	17.719130
35.917791	1267.453533	17.724147
35.958144	1267.878816	17.729165
36.143950	1272.335237	17.734183
36.305559	1266.022471	17.739200
36.371946	1269.976057	17.744218
36.259900	1264.484001	17.749235
36.484842	1258.664052	17.754253
36.096587	1269.638502	17.759271
36.323928	1266.548502	17.764288
36.219981	1256.107144	17.769306
35.899462	1269.495865	17.774323
36.269747	1264.686602	17.779341
36.250368	1266.168862	17.784359
36.113183	1263.115876	17.789376
36.267695	1262.782037	17.794394
36.357017	1263.817453	17.799411
36.475570	1256.852051	17.804429
36.760052	1267.773392	17.809447
36.709679	1271.015857	17.814464
36.699098	1270.946277	17.819482
36.944596	1259.128447	17.824499
36.927070	1251.118155	17.829517
36.752895	1257.316513	17.834535
36.842838	1266.642855	17.839552
36.721034	1274.025910	17.844570
37.055183	1272.721566	17.849587
36.899795	1269.234833	17.854605
37.134156	1269.834328	17.859623
37.226313	1272.623179	17.864640
37.006485	1263.002434	17.869658
36.712590	1260.559914	17.874675
37.066281	1276.757511	17.879693
37.075100	1279.761880	17.884711
37.223615	1286.287189	17.889728
37.405207	1286.625952	17.894746
36.917723	1286.239366	17.899763
37.205593	1279.614035	17.904781
37.136165	1286.262356	17.909799
37.333090	1287.242399	17.914816
37.306703	1291.703776	17.919834
37.156929	1290.852578	17.924851
37.661042	1285.727334	17.929869
37.370538	1279.418812	17.934887
37.955109	1280.033654	17.939904
37.702718	1275.820527	17.944922
37.471974	1285.283918	17.949939
37.583267	1288.364256	17.954957
37.558161	1280.062524	17.959975
37.418150	1285.426812	17.964992
37.893359	1284.942943	17.970010
37.759684	1290.256980	17.975027
37.835855	1279.386680	17.980045
37.519064	1282.984747	17.985063
37.900333	1277.135415	17.990080
38.134530	1277.031093	17.995098
37.753087	1279.907065	18.000115
37.508206	1281.187645	18.005133
37.811023	1303.803272	18.010151
37.938833	1300.319531	18.015168
38.596424	1299.166826	18.020186
38.188263	1311.645384	18.025203
38.652714	1296.589592	18.030221
38.437775	1299.929524	18.035239
38.446266	1287.833949	18.040256
38.441755	1286.207073	18.045274
38.341220	1288.100528	18.050291
38.476000	1277.878136	18.055309
38.417564	1293.336284	18.060327
38.497981	1292.586005	18.065344
38.513584	1291.997007	18.070362
38.548843	1301.734717	18.075379
38.964066	1303.650411	18.080397
38.328451	1290.869446	18.085415
38.598719	1287.998500	18.090432
38.744530	1292.257429	18.095450
38.520001	1297.076903	18.100467
38.602546	1293.103070	18.105485
38.684690	1304.379682	18.110503
38.428124	1302.352388	18.115520
38.643940	1300.813888	18.120538
38.482515	1303.926109	18.125555
38.418080	1299.189263	18.130573
38.573744	1313.348042	18.135591
38.784463	1328.443875	18.140608
38.949083	1322.667134	18.145626
38.901993	1338.442703	18.150643
39.066185	1320.263681	18.155661
39.180338	1328.879655	18.160679
39.263828	1313.924392	18.165696
39.525212	1325.152899	18.170714
39.145413	1323.943108	18.175731
39.281847	1320.126680	18.180749
38.841280	1325.679411	18.185767
39.104539	1323.562080	18.190784
39.552846	1331.378050	18.195802
39.248194	1347.136945	18.200819
39.770477	1332.317199	18.205837
40.096096	1340.763212	18.210855
39.585771	1337.092235	18.215872
39.486446	1335.560343	18.220890
39.867536	1336.673320	18.225907
40.152469	1334.187098	18.230925
39.727946	1328.478383	18.235943
39.736918	1311.515814	18.240960
40.042490	1299.404204	18.245978
39.915112	1307.271599	18.250995
39.773208	1309.133906	18.256013
40.016689	1321.705353	18.261031
40.082395	1321.282068	18.266048
40.188324	1312.119797	18.271066
39.768975	1307.485096	18.276083
40.045481	1318.403856	18.281101
40.150356	1328.663081	18.286119
40.351396	1341.239589	18.291136
40.292008	1323.761401	18.296154
40.189558	1340.969757	18.301171
40.124582	1333.231010	18.306189
40.008888	1332.943791	18.311207
40.260720	1336.046184	18.316224
40.241906	1344.631194	18.321242
40.034098	1333.662526	18.326259
40.195401	1334.822452	18.331277
40.132200	1333.626279	18.336295
40.197009	1338.382600	18.341312
40.284819	1347.122213	18.346330
40.217176	1363.161997	18.351347
40.508508	1370.398295	18.356365
40.364158	1365.780527	18.361383
40.527212	1359.832792	18.366400
40.717326	1362.541897	18.371418
40.515613	1360.801557	18.376435
40.776619	1374.197606	18.381453
41.184611	1376.890982	18.386471
41.244944	1383.973357	18.391488
41.415036	1359.086276	18.396506
41.277497	1369.613708	18.401523
41.088114	1349.188055	18.406541
41.341252	1352.542763	18.411559
41.170971	1339.464612	18.416576
41.339844	1336.798185	18.421594
41.266843	1353.313193	18.426611
41.319117	1352.551619	18.431629
41.010453	1346.372431	18.436647
40.954594	1350.922150	18.441664
41.632644	1368.447172	18.446682
41.246557	1382.167259	18.451699
41.628826	1378.954009	18.456717
41.860578	1383.198959	18.461735
41.659707	1385.272372	18.466752
41.812772	1376.635081	18.471770
41.699867	1367.982108	18.476787
41.869173	1361.475142	18.481805
41.868071	1352.773784	18.486823
41.300278	1353.403490	18.491840
42.029113	1361.786820	18.496858
42.009547	1373.420406	18.501875
42.264878	1377.591387	18.506893
41.931556	1371.526880	18.511911
41.778377	1371.371232	18.516928
41.943354	1369.514396	18.521946
42.125986	1372.422352	18.526963
42.150417	1375.646967	18.531981
42.381420	1373.388324	18.536999
42.035343	1382.191784	18.542016
41.913414	1379.570648	18.547034
41.977806	1373.181396	18.552051
41.958702	1380.931932	18.557069
42.274486	1375.000483	18.562087
42.180014	1383.937935	18.567104
42.146333	1371.119236	18.572122
42.355382	1392.892527	18.577139
42.419726	1397.397989	18.582157
42.499819	1406.373528	18.587175
42.306332	1411.902190	18.592192
42.225833	1405.080427	18.597210
42.318694	1406.806128	18.602227
42.593897	1408.882556	18.607245
42.608953	1409.123267	18.612263
42.569384	1419.549515	18.617280
42.742442	1399.401852	18.622298
42.749866	1398.154835	18.627315
42.610513	1404.424849	18.632333
42.984088	1410.570149	18.637351
42.883794	1427.055498	18.642368
43.242962	1415.556912	18.647386
43.142236	1430.785995	18.652403
43.344818	1420.022841	18.657421
43.303774	1416.130809	18.662439
43.079021	1424.782568	18.667456
43.284312	1425.829142	18.672474
43.137238	1428.200720	18.677491
43.427691	1417.041007	18.682509
43.577385	1412.557880	18.687527
43.406236	1422.118580	18.692544
43.540167	1421.146682	18.697562
43.633510	1423.097869	18.702579
43.434782	1420.966721	18.707597
43.951340	1430.757245	18.712615
43.606735	1428.412042	18.717632
43.627671	1426.428824	18.722650
43.936102	1417.634946	18.727667
43.679986	1420.644152	18.732685
43.866587	1409.583485	18.737703
43.691146	1426.920520	18.742720
43.940280	1422.023171	18.747738
43.869362	1419.464653	18.752755
43.665751	1419.320881	18.757773
43.723053	1416.669924	18.762791
43.662232	1421.097861	18.767808
43.884179	1423.648980	18.772826
43.862079	1439.121346	18.777843
43.825592	1445.515503	18.782861
44.312095	1442.591082	18.787879
44.217761	1447.497735	18.792896
44.523447	1439.364849	18.797914
44.679636	1425.679003	18.802931
44.367096	1427.272117	18.807949
44.782109	1437.805125	18.812967
44.379937	1438.005348	18.817984
44.695043	1426.103061	18.823002
44.810876	1418.173585	18.828019
44.638996	1431.706762	18.833037
44.854287	1430.656270	18.838055
44.834979	1438.396831	18.843072
44.890310	1427.274390	18.848090
44.971872	1425.112276	18.853107
44.716341	1430.734651	18.858125
45.049689	1424.620382	18.863143
44.585795	1429.840627	18.868160
44.603929	1428.601482	18.873178
44.624339	1431.870862	18.878195
44.826112	1433.795275	18.883213
45.194009	1422.126954	18.888231
45.026347	1444.229859	18.893248
44.930763	1453.258863	18.898266
45.283063	1452.809669	18.903283
45.222600	1465.288565	18.908301
45.395802	1450.974369	18.913319
45.517488	1452.640397	18.918336
45.711560	1444.906222	18.923354
45.818503	1444.079710	18.928371
45.563656	1455.030868	18.933389
45.662053	1454.101450	18.938407
45.640649	1443.689035	18.943424
45.606680	1433.215521	18.948442
45.700439	1451.092476	18.953459
45.452093	1446.780811	18.958477
45.734539	1449.669729	18.963495
45.518472	1450.885726	18.968512
45.871332	1461.686274	18.973530
45.685440	1452.199353	18.978547
45.556732	1453.160588	18.983565
45.875400	1445.733539	18.988583
45.746378	1450.673679	18.993600
45.638786	1450.519944	18.998618
46.172348	1460.022279	19.003635
46.523244	1473.482685	19.008653
46.801045	1465.585074	19.013671
46.212141	1454.245686	19.018688
45.910131	1441.154379	19.023706
46.401953	1468.379402	19.028723
46.352273	1475.661670	19.033741
46.476384	1470.151576	19.038759
46.821833	1475.631157	19.043776
46.797609	1473.947684	19.048794
46.928706	1468.360461	19.053811
46.486537	1468.350980	19.058829
46.797404	1458.421773	19.063847
46.774176	1470.510904	19.068864
46.459054	1469.325644	19.073882
47.003874	1477.055277	19.078899
46.711299	1471.630770	19.083917
46.704689	1470.000679	19.088935
46.728804	1476.889499	19.093952
46.920472	1475.346313	19.098970
47.124683	1474.852701	19.103987
47.067090	1469.930835	19.109005
47.077035	1468.365717	19.114023
46.976467	1469.028440	19.119040
47.032400	1466.544414	19.124058
47.115714	1467.778254	19.129075
47.121648	1471.334843	19.134093
47.258972	1489.101112	19.139111
47.367971	1494.074956	19.144128
47.297611	1498.628099	19.149146
47.415883	1493.371885	19.154163
47.519581	1486.003960	19.159181
47.186763	1485.525871	19.164199
47.653472	1492.551575	19.169216
47.547159	1496.188522	19.174234
47.743010	1489.900318	19.179251
47.829274	1493.349161	19.184269
47.638909	1482.995541	19.189287
47.926676	1496.927763	19.194304
47.935505	1503.737831	19.199322
48.003363	1511.200670	19.204339
48.281536	1518.659069	19.209357
48.117441	1500.017018	19.214375
48.267974	1503.182440	19.219392
48.240865	1506.189641	19.224410
48.520480	1500.003719	19.229427
48.427887	1504.499324	19.234445
48.606939	1497.242746	19.239463
48.542436	1484.325712	19.244480
47.845212	1492.573160	19.249498
48.384853	1488.738087	19.254515
48.694760	1507.645800	19.259533
48.700791	1504.369713	19.264551
48.796359	1501.363640	19.269568
48.608586	1507.454317	19.274586
48.992162	1501.013054	19.279603
48.316312	1504.568549	19.284621
48.688856	1503.699325	19.289639
48.455488	1510.430536	19.294656
48.779288	1503.831452	19.299674
49.158526	1503.007967	19.304691
49.166216	1504.541282	19.309709
49.049273	1515.686991	19.314727
48.799620	1504.117116	19.319744
48.498289	1510.045085	19.324762
48.497735	1507.834528	19.329779
48.651026	1510.004533	19.334797
48.477389	1526.192696	19.339815
49.302473	1536.501728	19.344832
49.195526	1535.367289	19.349850
49.391555	1539.635309	19.354867
49.722702	1545.783148	19.359885
49.742898	1531.869119	19.364903
49.617847	1527.284722	19.369920
49.148405	1533.571742	19.374938
49.683148	1528.886582	19.379955
49.471103	1530.050745	19.384973
49.618322	1536.964716	19.389991
49.815331	1532.746145	19.395008
49.944390	1549.031342	19.400026
50.188082	1538.066846	19.405043
49.741608	1546.797040	19.410061
49.988569	1549.660939	19.415079
49.885419	1551.369250	19.420096
50.318692	1542.533217	19.425114
50.525274	1545.775006	19.430131
50.265719	1557.799924	19.435149
50.225965	1553.543512	19.440167
50.610670	1557.175309	19.445184
50.221825	1550.531389	19.450202
50.297475	1540.777597	19.455219
50.066501	1553.747089	19.460237
50.558628	1555.697938	19.465255
50.607398	1546.879186	19.470272
49.860819	1550.946322	19.475290
50.279399	1549.728583	19.480307
50.404870	1562.536436	19.485325
50.645958	1554.245483	19.490343
50.804246	1543.118148	19.495360
50.829144	1569.831600	19.500378
51.189220	1565.576823	19.505395
51.126102	1573.480382	19.510413
50.696065	1563.349758	19.515431
50.963244	1577.287424	19.520448
50.791561	1572.684541	19.525466
51.245448	1570.502019	19.530483
51.158174	1557.384968	19.535501
50.989780	1571.992964	19.540519
51.358787	1569.806162	19.545536
51.142633	1571.461110	19.550554
51.514228	1565.672317	19.555571
51.154858	1576.125339	19.560589
51.450679	1571.495394	19.565607
51.435531	1568.794973	19.570624
51.078775	1573.694841	19.575642
51.159096	1580.421680	19.580659
51.242329	1596.106497	19.585677
51.377698	1602.514048	19.590695
51.578528	1595.692950	19.595712
51.377696	1593.233225	19.600730
51.827115	1599.094838	19.605747
52.294388	1608.151577	19.610765
52.455160	1603.130403	19.615783
52.591929	1580.359262	19.620800
52.307803	1592.680754	19.625818
52.429296	1583.822605	19.630835
52.667278	1584.380575	19.635853
52.353435	1574.874371	19.640871
52.447826	1573.335834	19.645888
52.474065	1579.871830	19.650906
52.544992	1564.860730	19.655923
52.634134	1574.139759	19.660941
52.816315	1563.422784	19.665959
52.872284	1570.438061	19.670976
52.794196	1577.783530	19.675994
52.866072	1577.887703	19.681011
52.656427	1556.943328	19.686029
52.745897	1563.815680	19.691047
52.642224	1567.268764	19.696064
52.679025	1579.449624	19.701082
53.315654	1562.710778	19.706099
52.813469	1573.705057	19.711117
52.453063	1579.993562	19.716135
52.931457	1574.430201	19.721152
52.768464	1570.982841	19.726170
52.961983	1561.233570	19.731187
53.086379	1570.261720	19.736205
52.755560	1574.697117	19.741223
53.469362	1589.379206	19.746240
53.322819	1604.301893	19.751258
53.751715	1597.018548	19.756275
53.978874	1602.834420	19.761293
53.810042	1591.043272	19.766311
53.977382	1569.069369	19.771328
53.489395	1573.511842	19.776346
53.632307	1570.085183	19.781363
53.616769	1577.842906	19.786381
53.768143	1591.519831	19.791399
53.646408	1588.274484	19.796416
53.388550	1599.950177	19.801434
53.670689	1589.316852	19.806451
53.783433	1604.221690	19.811469
53.683231	1607.189027	19.816487
53.947770	1598.390293	19.821504
53.793550	1611.894138	19.826522
54.398152	1620.764430	19.831539
54.494844	1626.884517	19.836557
54.293602	1636.819968	19.841575
54.334901	1641.549365	19.846592
54.389402	1633.599209	19.851610
54.354325	1634.350515	19.856627
54.215823	1634.542597	19.861645
54.265160	1632.823922	19.866663
54.509348	1625.892901	19.871680
54.416624	1634.719985	19.876698
54.820345	1635.977853	19.881715
54.613337	1644.142996	19.886733
54.778727	1640.724810	19.891751
55.143457	1639.618314	19.896768
54.996079	1645.299265	19.901786
55.074368	1652.879333	19.906803
55.505673	1660.734106	19.911821
55.066254	1646.974851	19.916839
55.574649	1642.444586	19.921856
55.460060	1644.924202	19.926874
55.395499	1650.236389	19.931891
55.590122	1643.594427	19.936909
55.360051	1637.995179	19.941927
55.851910	1636.873974	19.946944
55.281269	1631.877798	19.951962
55.573634	1647.458628	19.956979
55.548142	1635.279429	19.961997
55.400845	1637.654421	19.967015
55.640966	1630.201883	19.972032
55.202682	1642.100315	19.977050
55.472393	1641.069160	19.982067
55.520128	1631.590563	19.987085
55.508770	1650.206695	19.992103
56.295390	1655.493964	19.997120
56.325127	1660.552409	20.002138
56.315481	1659.700866	20.007155
56.201394	1649.002674	20.012173
55.883011	1651.777555	20.017191
56.261908	1656.269299	20.022208
56.238605	1655.736712	20.027226
56.582601	1666.312319	20.032243
56.598276	1659.567257	20.037261
56.336796	1663.671373	20.042279
56.681949	1659.123989	20.047296
56.607619	1663.636896	20.052314
56.616713	1663.998465	20.057331
56.505483	1654.066450	20.062349
56.474499	1660.395030	20.067367
56.894313	1654.467542	20.072384
56.429987	1663.795175	20.077402
56.383780	1667.084865	20.082419
56.866654	1692.952855	20.087437
56.709819	1684.309127	20.092455
56.886703	1686.717359	20.097472
56.886498	1688.433474	20.102490
57.017913	1690.015449	20.107507
57.734300	1692.850028	20.112525
57.182027	1693.761205	20.117543
57.335053	1701.756068	20.122560
57.493701	1693.276519	20.127578
57.398823	1684.353290	20.132595
57.443184	1698.134206	20.137613
57.635775	1719.087733	20.142631
57.852857	1712.483954	20.147648
58.088064	1722.351864	20.152666
58.281454	1722.674911	20.157683
57.755753	1705.605989	20.162701
57.719247	1701.199605	20.167719
57.854658	1714.556870	20.172736
58.150701	1717.887052	20.177754
57.850718	1719.518076	20.182771
58.169742	1720.818684	20.187789
58.136557	1736.531346	20.192807
58.099449	1724.123507	20.197824
58.106011	1719.725551	20.202842
57.900620	1734.985811	20.207859
58.094716	1712.909064	20.212877
58.172625	1720.112102	20.217895
58.692280	1721.140802	20.222912
58.528251	1734.217088	20.227930
58.752596	1736.985558	20.232947
58.779719	1729.450858	20.237965
58.515799	1732.153373	20.242983
58.886591	1720.918361	20.248000
58.809087	1733.741987	20.253018
58.480449	1734.855556	20.258035
58.812619	1732.795477	20.263053
58.696869	1736.393099	20.268071
58.748921	1740.431647	20.273088
59.470691	1750.403406	20.278106
59.129223	1751.534253	20.283123
59.557364	1756.559174	20.288141
59.480138	1753.360762	20.293159
59.541634	1757.735909	20.298176
59.720812	1746.804758	20.303194
59.588110	1756.984840	20.308211
59.784945	1748.271414	20.313229
59.911188	1748.779358	20.318247
60.048943	1742.668942	20.323264
59.823620	1736.869681	20.328282
59.865332	1720.919651	20.333299
59.843735	1714.935370	20.338317
59.886049	1721.950217	20.343335
59.801314	1724.080460	20.348352
59.949452	1738.212138	20.353370
59.761735	1749.612403	20.358387
60.047136	1749.014628	20.363405
60.055121	1753.285832	20.368423
60.327165	1752.870168	20.373440
60.216628	1749.205852	20.378458
60.018980	1751.775384	20.383475
60.151027	1745.717676	20.388493
60.000957	1758.335619	20.393511
59.937433	1768.760944	20.398528
60.271331	1779.366445	20.403546
60.218042	1780.969307	20.408563
60.245740	1781.795278	20.413581
60.315410	1802.755650	20.418599
60.656420	1805.134221	20.423616
61.062296	1800.602349	20.428634
61.226543	1806.884556	20.433651
60.935111	1785.046388	20.438669
61.025195	1801.500875	20.443687
61.062605	1799.073788	20.448704
61.176319	1804.240438	20.453722
61.162902	1798.913765	20.458739
61.452448	1787.900574	20.463757
61.348756	1789.781817	20.468775
61.308701	1794.891599	20.473792
61.926995	1803.115113	20.478810
61.420395	1815.348951	20.483827
61.772117	1822.194222	20.488845
61.882778	1822.118383	20.493863
61.868141	1818.003008	20.498880
62.255986	1808.004563	20.503898
62.028814	1819.645826	20.508915
62.164106	1808.674250	20.513933
62.009774	1818.197774	20.518951
62.093280	1811.510328	20.523968
62.191734	1817.832149	20.528986
62.306584	1814.593520	20.534003
62.773709	1807.044729	20.539021
62.779773	1806.585229	20.544039
62.799713	1797.517973	20.549056
62.437873	1779.521782	20.554074
62.288657	1784.476781	20.559091
62.727938	1794.282869	20.564109
62.490091	1793.764078	20.569127
62.212380	1803.981144	20.574144
62.693347	1800.929042	20.579162
62.406842	1808.550572	20.584179
62.479198	1816.211418	20.589197
62.922660	1810.132734	20.594215
62.672767	1815.767110	20.599232
63.059644	1830.477473	20.604250
63.192599	1838.648149	20.609267
63.204988	1836.883396	20.614285
63.400068	1849.618181	20.619303
63.451829	1842.958405	20.624320
63.761947	1838.985996	20.629338
63.640198	1841.480999	20.634355
63.567184	1830.624727	20.639373
63.518137	1838.850083	20.644391
63.226031	1834.900228	20.649408
63.821604	1815.160504	20.654426
63.892067	1829.511775	20.659443
63.980258	1827.825826	20.664461
64.208915	1833.303382	20.669479
63.494461	1839.543815	20.674496
64.119398	1824.661758	20.679514
64.014646	1832.285547	20.684531
64.015996	1829.099525	20.689549
64.230576	1825.662345	20.694567
63.900344	1834.268383	20.699584
64.297677	1829.319845	20.704602
64.292201	1830.109769	20.709619
64.049290	1830.574988	20.714637
64.199928	1846.336708	20.719655
64.131247	1853.430580	20.724672
64.294165	1851.223667	20.729690
64.608031	1855.900217	20.734707
64.460256	1858.351299	20.739725
64.569089	1863.911849	20.744743
64.631564	1876.675459	20.749760
64.897776	1888.610603	20.754778
64.815294	1887.323289	20.759795
65.292891	1883.020662	20.764813
65.155611	1879.119024	20.769831
65.377942	1869.670676	20.774848
65.351218	1875.591985	20.779866
65.128440	1886.938112	20.784883
65.066207	1871.525724	20.789901
65.627979	1881.679310	20.794919
65.692239	1869.770894	20.799936
65.817052	1869.587410	20.804954
65.751416	1880.980000	20.809971
65.611380	1871.383282	20.814989
65.977585	1878.902303	20.820007
65.778208	1881.852619	20.825024
65.903000	1867.374793	20.830042
65.677212	1879.140663	20.835059
65.806035	1881.158677	20.840077
66.391574	1892.236603	20.845095
66.072733	1907.773828	20.850112
66.837066	1888.643271	20.855130
66.453327	1894.263182	20.860147
66.759967	1906.392626	20.865165
66.719354	1896.426542	20.870183
66.594248	1886.175832	20.875200
66.766417	1887.149377	20.880218
66.725789	1895.989851	20.885235
66.743176	1891.427276	20.890253
66.969163	1896.181740	20.895271
66.689876	1892.857057	20.900288
66.717581	1886.033734	20.905306
66.811951	1887.085090	20.910323
66.795097	1892.379241	20.915341
66.581593	1892.535889	20.920359
66.751214	1895.140219	20.925376
67.136735	1917.014017	20.930394
66.943322	1927.162908	20.935411
67.233946	1919.943595	20.940429
67.255330	1921.742578	20.945447
67.128334	1929.317930	20.950464
67.228921	1927.318729	20.955482
67.672247	1944.070675	20.960499
67.487606	1942.199897	20.965517
67.598473	1941.817948	20.970535
68.059349	1950.763951	20.975552
67.893275	1948.459630	20.980570
67.899355	1947.658617	20.985587
67.818127	1937.147102	20.990605
67.968336	1932.870020	20.995623
67.963759	1948.534080	21.000640
67.804945	1941.280570	21.005658
68.345342	1950.086869	21.010675
68.183493	1959.847134	21.015693
68.445572	1950.990541	21.020711
68.465760	1954.600394	21.025728
68.378081	1963.413644	21.030746
68.714021	1967.769483	21.035763
68.827581	1959.486592	21.040781
69.163922	1964.826530	21.045799
68.778017	1960.030209	21.050816
68.964341	1949.429399	21.055834
69.303586	1953.872671	21.060851
69.160798	1950.988372	21.065869
69.500451	1954.495832	21.070887
69.402655	1958.896768	21.075904
69.697747	1960.515696	21.080922
69.541170	1961.012907	21.085939
69.632127	1954.821565	21.090957
69.578587	1930.056139	21.095975
68.997896	1943.399073	21.100992
69.275921	1953.364182	21.106010
69.212712	1956.938805	21.111027
69.173665	1948.419153	21.116045
69.630077	1954.584250	21.121063
69.563033	1969.700435	21.126080
69.762465	1969.804398	21.131098
69.926092	1977.355762	21.136115
70.017645	1980.769001	21.141133
69.962693	1972.468875	21.146151
69.896530	1975.424949	21.151168
69.959567	1973.968909	21.156186
69.992971	1987.801496	21.161203
69.993762	1997.878582	21.166221
70.594048	2010.833526	21.171239
70.591011	2009.199638	21.176256
70.813794	2007.354826	21.181274
70.612530	2004.877390	21.186291
70.796313	2008.317714	21.191309
71.092902	2001.303661	21.196327
70.872060	2007.157893	21.201344
71.031202	2001.449909	21.206362
71.081709	2002.423489	21.211379
70.845968	2015.250860	21.216397
70.949246	2002.809954	21.221415
71.081515	2021.263246	21.226432
71.358524	2023.857332	21.231450
71.363600	2033.493021	21.236467
71.168805	2024.396948	21.241485
71.634753	2025.672321	21.246503
71.231972	2032.745900	21.251520
71.455224	2020.004863	21.256538
71.826625	2012.028914	21.261555
71.838513	2026.624477	21.266573
72.294401	2030.091883	21.271591
72.125118	2026.276985	21.276608
71.851812	2025.339080	21.281626
71.924522	2021.326531	21.286643
72.216651	2050.682657	21.291661
72.655350	2042.625696	21.296679
72.422261	2046.976185	21.301696
72.655407	2041.532116	21.306714
72.743606	2042.705358	21.311731
72.391731	2042.370741	21.316749
72.708841	2053.937396	21.321767
72.670329	2045.242026	21.326784
72.217060	2039.025827	21.331802
72.963278	2034.011503	21.336819
72.784888	2034.759741	21.341837
73.127811	2031.731784	21.346855
73.059315	2035.992085	21.351872
73.391483	2037.798579	21.356890
73.403714	2034.045213	21.361907
73.181567	2038.368893	21.366925
72.908289	2027.834528	21.371943
72.949337	2034.862126	21.376960
72.990636	2026.865528	21.381978
73.327569	2045.012413	21.386995
73.479099	2053.069513	21.392013
73.799739	2049.419695	21.397031
73.972769	2053.237760	21.402048
73.828934	2055.754752	21.407066
74.093411	2041.048973	21.412083
73.948211	2042.768813	21.417101
73.825894	2049.933247	21.422119
73.640667	2055.627688	21.427136
73.665811	2061.918814	21.432154
74.131627	2062.131700	21.437171
73.692181	2084.951442	21.442189
74.226271	2068.638609	21.447207
74.036987	2071.246179	21.452224
74.235184	2074.183782	21.457242
74.693167	2088.178958	21.462259
74.538784	2092.030075	21.467277
74.437108	2107.082240	21.472295
74.498974	2108.995019	21.477312
74.875927	2092.936455	21.482330
74.877252	2098.702833	21.487347
74.610841	2105.458461	21.492365
75.304343	2112.516656	21.497383
75.272751	2128.995340	21.502400
75.396571	2136.375618	21.507418
75.916072	2123.709351	21.512435
75.254874	2120.502054	21.517453
75.686324	2121.530597	21.522471
75.606049	2121.667396	21.527488
75.481569	2123.192694	21.532506
75.683056	2113.825785	21.537523
75.553722	2116.018959	21.542541
75.692662	2117.365698	21.547559
75.950351	2125.048234	21.552576
75.670430	2133.486096	21.557594
75.841617	2136.916721	21.562611
75.893474	2147.308276	21.567629
76.336690	2139.745560	21.572647
76.099641	2140.535187	21.577664
75.904248	2144.436200	21.582682
76.284214	2157.248555	21.587699
76.810205	2170.730441	21.592717
77.197323	2159.655985	21.597735
77.227094	2156.389418	21.602752
77.054983	2148.572892	21.607770
77.016017	2128.784682	21.612787
76.777104	2128.257984	21.617805
76.728431	2148.647876	21.622823
77.074933	2162.495610	21.627840
77.365690	2145.231247	21.632858
77.491448	2142.992051	21.637875
77.477682	2158.251770	21.642893
77.301923	2160.100679	21.647911
77.554679	2146.923985	21.652928
77.366588	2152.811637	21.657946
77.540497	2144.478718	21.662963
77.581039	2155.142010	21.667981
77.508784	2156.815559	21.672999
77.699005	2176.939454	21.678016
77.829365	2173.458245	21.683034
78.142870	2173.309125	21.688051
77.784249	2181.905283	21.693069
78.033730	2184.835221	21.698087
78.425571	2172.339606	21.703104
77.974060	2188.269480	21.708122
78.339701	2174.079103	21.713139
78.270036	2181.699037	21.718157
78.334022	2172.760690	21.723175
78.504470	2183.045672	21.728192
78.328036	2205.338307	21.733210
78.675588	2202.955176	21.738227
78.795675	2209.308620	21.743245
79.053660	2201.903639	21.748263
79.151470	2207.307289	21.753280
78.708374	2213.031014	21.758298
79.197668	2213.989970	21.763315
79.167087	2209.832050	21.768333
79.258425	2204.345023	21.773351
79.299797	2211.840923	21.778368
79.560413	2233.881668	21.783386
79.471457	2228.063820	21.788403
79.675671	2248.641174	21.793421
79.334878	2234.677310	21.798439
79.857924	2228.119991	21.803456
80.085331	2229.795208	21.808474
80.105810	2231.374904	21.813491
80.027195	2237.908428	21.818509
80.028210	2234.274772	21.823527
80.201468	2236.165419	21.828544
79.904801	2237.489472	21.833562
80.045673	2248.012636	21.838579
80.113807	2259.217662	21.843597
80.333691	2263.376439	21.848615
80.361653	2260.942180	21.853632
80.266622	2257.005907	21.858650
80.784101	2267.166675	21.863667
81.040619	2279.818244	21.868685
81.220057	2286.356585	21.873703
81.544938	2289.995690	21.878720
81.250394	2287.780455	21.883738
81.387370	2274.916663	21.888755
81.120785	2274.596291	21.893773
80.952872	2279.836014	21.898791
80.957596	2273.766858	21.903808
81.085766	2272.652170	21.908826
81.570805	2280.386973	21.913843
81.678488	2279.429990	21.918861
81.832160	2285.526752	21.923879
81.833988	2304.222789	21.928896
81.819061	2310.733616	21.933914
82.010641	2300.786182	21.938931
81.996511	2305.452507	21.943949
81.875491	2301.410681	21.948967
82.226455	2299.917859	21.953984
82.318952	2309.870947	21.959002
82.547183	2309.347950	21.964019
82.540497	2304.008573	21.969037
82.424003	2302.979190	21.974055
82.246364	2300.028147	21.979072
82.424910	2327.023408	21.984090
82.456571	2332.357722	21.989107
82.770141	2332.759934	21.994125
82.763936	2331.787911	21.999143
82.927317	2334.001049	22.004160
82.809072	2332.758581	22.009178
83.242010	2344.298639	22.014195
83.150051	2351.624524	22.019213
83.262574	2358.300914	22.024231
83.783988	2350.731474	22.029248
83.411098	2359.915091	22.034266
83.679651	2351.791014	22.039283
83.267429	2347.653997	22.044301
83.670684	2356.090894	22.049319
83.776337	2350.569562	22.054336
83.757434	2357.053902	22.059354
83.774716	2338.325945	22.064371
84.208094	2350.157649	22.069389
84.182162	2366.018956	22.074407
84.334641	2362.783838	22.079424
84.585435	2369.151574	22.084442
84.761230	2368.479376	22.089459
84.666365	2369.064427	22.094477
84.661713	2369.877864	22.099495
85.090043	2350.834346	22.104512
85.059002	2361.382649	22.109530
84.901364	2357.733450	22.114547
85.060764	2355.155810	22.119565
84.971515	2355.828904	22.124583
85.075293	2363.656670	22.129600
85.135574	2366.702942	22.134618
85.231737	2349.452004	22.139635
85.388335	2355.896714	22.144653
85.182944	2356.780720	22.149671
85.565057	2363.824743	22.154688
85.519899	2368.060808	22.159706
85.804540	2365.814812	22.164723
85.490438	2372.207395	22.169741
85.588111	2386.738142	22.174759
85.550990	2383.254051	22.179776
85.509693	2398.196331	22.184794
85.605747	2396.394856	22.189811
85.958495	2410.997642	22.194829
85.862195	2415.984253	22.199847
85.995772	2409.549283	22.204864
85.927511	2416.310686	22.209882
86.006575	2427.515604	22.214899
86.546349	2440.540751	22.219917
86.378602	2456.346455	22.224935
86.379991	2453.419340	22.229952
86.394397	2459.426197	22.234970
86.751259	2463.021478	22.239987
87.134102	2465.781409	22.245005
87.088405	2470.832901	22.250023
87.324186	2473.845863	22.255040
87.452653	2475.154997	22.260058
87.175995	2458.560394	22.265075
87.506856	2464.617318	22.270093
87.418783	2475.286927	22.275111
87.493443	2473.105534	22.280128
87.799196	2489.186947	22.285146
87.753854	2505.163409	22.290163
88.020585	2493.124802	22.295181
87.814733	2501.706127	22.300199
88.090369	2500.055664	22.305216
88.084737	2496.940341	22.310234
88.167239	2485.744344	22.315251
87.752856	2484.544893	22.320269
88.308746	2512.961512	22.325287
88.453121	2506.726675	22.330304
88.599244	2524.589925	22.335322
88.518920	2516.194294	22.340339
88.840101	2509.538922	22.345357
88.729834	2521.993635	22.350375
88.914503	2506.926605	22.355392
89.090391	2519.494259	22.360410
89.202916	2530.631914	22.365427
89.804692	2536.976367	22.370445
89.624615	2524.014766	22.375463
89.674954	2502.961187	22.380480
89.571791	2496.690884	22.385498
89.728400	2496.119877	22.390515
89.960185	2495.003799	22.395533
89.762501	2502.032282	22.400551
90.035146	2493.136629	22.405568
89.685417	2498.729287	22.410586
89.714816	2516.090582	22.415603
90.218812	2520.296571	22.420621
90.083082	2528.662004	22.425639
90.327409	2523.827109	22.430656
90.314440	2535.649251	22.435674
90.209183	2527.773456	22.440691
90.417183	2523.211874	22.445709
90.159018	2530.810177	22.450727
90.884110	2537.229525	22.455744
91.073647	2555.548999	22.460762
90.995542	2567.988198	22.465779
91.093179	2556.469586	22.470797
90.891763	2559.916208	22.475815
90.956727	2543.451669	22.480832
91.350658	2551.397718	22.485850
91.138456	2553.354855	22.490867
91.294127	2546.247707	22.495885
91.247495	2566.406918	22.500903
91.447578	2570.020257	22.505920
91.796062	2576.456579	22.510938
91.486244	2571.245149	22.515955
92.015675	2577.360247	22.520973
91.718746	2597.199457	22.525991
91.923205	2596.731559	22.531008
91.893851	2602.175256	22.536026
92.268332	2612.208315	22.541043
92.644546	2596.374541	22.546061
92.162890	2599.650166	22.551079
92.618939	2592.768545	22.556096
92.688927	2600.853579	22.561114
92.212606	2605.599517	22.566131
92.626416	2614.635966	22.571149
92.490166	2629.517785	22.576167
92.763661	2631.440735	22.581184
93.066132	2634.360035	22.586202
92.852887	2638.849923	22.591219
93.393481	2657.035527	22.596237
93.079174	2665.944694	22.601255
93.696492	2657.041204	22.606272
93.485417	2663.336176	22.611290
93.711926	2659.076601	22.616307
93.536553	2656.813668	22.621325
93.770282	2658.490054	22.626343
94.083801	2647.220729	22.631360
94.287157	2662.120081	22.636378
94.084469	2676.405469	22.641395
94.328536	2689.485596	22.646413
93.821330	2686.887743	22.651431
94.150760	2679.849849	22.656448
94.359334	2679.838336	22.661466
94.626239	2680.288425	22.666483
94.660743	2675.270054	22.671501
94.803037	2689.709070	22.676519
94.709775	2699.955691	22.681536
95.263228	2695.800343	22.686554
95.478260	2705.749579	22.691571
95.770069	2690.122169	22.696589
95.753655	2692.197358	22.701607
95.328031	2671.063937	22.706624
95.386593	2658.570644	22.711642
95.270223	2675.489688	22.716659
95.977868	2682.584000	22.721677
95.695531	2691.130433	22.726695
95.658278	2689.115134	22.731712
96.072424	2688.738957	22.736730
95.732962	2699.136099	22.741747
96.065869	2687.154908	22.746765
96.029966	2690.418310	22.751783
95.915842	2682.598623	22.756800
96.247579	2694.361958	22.761818
95.871334	2718.139078	22.766835
96.513017	2716.595817	22.771853
96.231603	2732.976470	22.776871
96.729584	2715.755969	22.781888
96.792125	2715.066645	22.786906
96.562077	2741.504974	22.791923
97.113409	2752.356115	22.796941
97.440649	2756.924042	22.801959
97.344296	2742.556741	22.806976
97.186119	2739.707117	22.811994
96.858177	2738.059125	22.817011
97.094450	2752.766913	22.822029
97.310574	2772.208982	22.827047
97.809612	2785.236429	22.832064
97.607526	2772.809341	22.837082
97.773338	2781.551446	22.842099
97.818060	2770.603998	22.847117
97.924459	2774.474196	22.852135
98.155285	2791.704882	22.857152
98.492704	2793.591306	22.862170
98.681914	2785.990727	22.867187
99.177022	2781.413909	22.872205
99.110235	2782.112049	22.877223
98.957541	2775.093150	22.882240
99.250817	2769.987895	22.887258
99.025567	2776.416353	22.892275
98.850900	2777.850798	22.897293
98.843334	2774.160954	22.902311
99.049495	2777.178083	22.907328
99.346687	2775.694103	22.912346
99.197839	2781.633971	22.917363
99.364373	2778.776746	22.922381
99.401741	2790.117158	22.927399
99.297354	2801.932957	22.932416
99.502240	2799.239070	22.937434
99.473285	2816.495387	22.942451
99.637846	2822.359467	22.947469
99.994952	2832.634510	22.952487
100.200848	2840.194865	22.957504
100.445060	2839.058993	22.962522
100.252408	2831.757310	22.967539
100.538463	2825.497360	22.972557
100.819405	2831.761885	22.977575
100.540531	2831.546282	22.982592
100.869837	2829.173947	22.987610
100.957241	2841.447045	22.992627
100.881430	2854.862050	22.997645
101.233956	2855.840502	23.002663
101.078873	2857.850441	23.007680
101.325593	2859.285733	23.012698
101.485943	2861.024265	23.017715
101.586133	2850.103814	23.022733
101.663016	2847.429890	23.027751
101.308489	2851.975467	23.032768
101.589838	2865.586969	23.037786
101.362281	2877.733798	23.042803
101.739839	2886.323261	23.047821
102.002756	2884.235109	23.052839
101.767142	2883.432845	23.057856
102.160225	2873.913546	23.062874
102.009155	2898.501348	23.067891
102.248964	2912.002042	23.072909
102.311035	2898.017069	23.077927
102.429697	2901.142379	23.082944
102.756714	2902.562832	23.087962
102.666277	2912.345360	23.092979
102.535988	2930.284673	23.097997
103.148936	2936.333753	23.103015
103.088556	2946.112123	23.108032
103.416405	2942.771137	23.113050
103.589326	2937.566426	23.118067
103.604200	2951.146053	23.123085
103.536064	2939.558095	23.128103
103.159244	2936.159144	23.133120
104.147322	2937.477847	23.138138
104.359260	2948.311194	23.143155
104.535496	2953.690335	23.148173
104.352428	2931.859799	23.153191
104.495329	2921.828282	23.158208
104.528729	2921.350846	23.163226
104.617086	2928.043680	23.168243
104.963079	2942.434706	23.173261
105.386664	2930.658024	23.178279
105.051690	2917.668146	23.183296
105.543946	2900.880659	23.188314
105.232690	2890.804130	23.193331
105.125721	2891.240811	23.198349
105.710442	2888.483358	23.203367
105.436602	2896.232458	23.208384
105.293457	2896.070014	23.213402
105.133002	2907.806577	23.218419
105.141881	2927.922442	23.223437
105.354139	2937.953780	23.228455
105.702016	2943.761238	23.233472
105.835908	2930.185618	23.238490
105.837716	2927.896124	23.243507
105.739684	2944.088827	23.248525
105.554205	2958.708630	23.253543
105.585596	2962.549933	23.258560
105.891358	2976.440170	23.263578
106.135302	2999.605802	23.268595
106.078762	2994.648040	23.273613
106.796042	3007.595914	23.278631
106.349962	3022.188367	23.283648
106.948222	3025.356893	23.288666
106.495564	3024.758199	23.293683
106.680092	3024.582159	23.298701
107.114288	3033.356830	23.303719
107.225799	3044.456835	23.308736
107.595905	3036.653411	23.313754
107.794821	3048.115740	23.318771
107.699243	3041.162478	23.323789
107.999767	3040.703497	23.328807
107.725744	3042.673272	23.333824
108.211551	3057.324762	23.338842
108.356274	3053.134105	23.343859
108.431656	3064.840872	23.348877
108.430265	3061.349149	23.353895
108.288861	3069.691402	23.358912
108.536465	3068.846682	23.363930
108.578049	3063.613239	23.368947
108.536461	3058.290786	23.373965
108.565392	3053.439352	23.378983
108.717653	3084.641392	23.384000
108.750167	3093.787585	23.389018
109.261597	3101.147977	23.394035
109.002975	3104.935663	23.399053
109.265698	3091.058697	23.404071
109.084349	3096.232412	23.409088
109.487375	3113.709802	23.414106
109.418708	3105.787903	23.419123
109.497586	3120.795667	23.424141
109.519516	3117.635113	23.429159
109.686021	3125.982816	23.434176
110.532954	3131.037417	23.439194
110.955908	3141.574224	23.444211
111.034935	3120.053653	23.449229
111.107934	3103.844668	23.454247
110.966332	3096.879695	23.459264
111.162290	3088.945967	23.464282
111.223944	3098.844818	23.469299
111.044462	3089.083783	23.474317
111.387847	3085.156350	23.479335
110.773476	3094.856671	23.484352
111.391935	3105.022177	23.489370
111.567235	3120.428570	23.494387
111.385172	3117.444635	23.499405
111.440302	3124.169816	23.504423
111.491791	3136.093574	23.509440
111.640794	3128.607738	23.514458
111.526920	3123.895626	23.519475
111.532952	3133.677313	23.524493
111.753842	3145.611276	23.529511
111.870058	3160.734562	23.534528
111.848899	3157.894896	23.539546
112.190868	3174.904103	23.544563
112.007900	3168.194749	23.549581
112.181888	3185.909671	23.554599
112.550610	3194.230296	23.559616
113.005000	3201.092291	23.564634
113.083569	3209.565986	23.569651
113.042699	3208.567353	23.574669
113.623060	3197.172436	23.579687
113.871271	3197.331539	23.584704
113.628650	3193.107605	23.589722
113.721107	3191.047973	23.594739
113.835211	3211.284219	23.599757
114.229072	3223.240053	23.604775
114.036236	3231.798371	23.609792
114.060886	3226.109011	23.614810
114.058332	3219.283211	23.619827
113.851199	3227.211608	23.624845
114.652587	3219.458481	23.629863
114.474900	3232.131989	23.634880
114.691955	3237.781256	23.639898
114.707138	3245.800092	23.644915
114.659443	3256.733250	23.649933
114.919466	3257.469140	23.654951
114.908475	3257.375800	23.659968
114.993881	3252.624420	23.664986
114.979777	3264.572502	23.670003
115.153066	3290.675828	23.675021
115.509157	3279.293106	23.680039
115.451244	3288.829159	23.685056
115.235347	3292.517704	23.690074
115.954698	3297.291080	23.695091
116.044855	3302.540473	23.700109
116.120397	3299.997008	23.705127
116.195891	3310.264966	23.710144
116.233613	3312.160033	23.715162
116.400164	3306.118063	23.720179
116.244130	3331.201858	23.725197
116.844219	3336.112671	23.730215
116.894957	3331.342980	23.735232
116.885623	3326.191090	23.740250
117.137886	3331.046382	23.745267
117.110534	3337.271504	23.750285
117.264150	3336.497026	23.755303
117.381392	3340.199039	23.760320
117.533781	3325.042849	23.765338
117.633215	3323.880079	23.770355
117.432191	3355.348128	23.775373
117.624525	3359.605062	23.780391
117.383669	3355.245753	23.785408
117.492761	3356.647141	23.790426
117.841619	3371.834553	23.795443
117.986452	3381.821809	23.800461
118.299011	3383.221076	23.805479
118.488568	3379.903636	23.810496
118.576675	3390.808149	23.815514
119.112920	3405.839041	23.820531
119.235670	3405.337377	23.825549
119.041340	3399.271144	23.830567
119.268336	3393.370334	23.835584
119.625232	3394.155186	23.840602
119.622697	3397.492750	23.845619
119.986293	3403.413534	23.850637
120.076875	3393.691147	23.855655
119.998926	3402.372701	23.860672
119.939447	3391.349119	23.865690
120.284341	3392.169025	23.870707
120.035786	3385.138129	23.875725
120.079642	3399.077929	23.880743
120.522661	3387.530370	23.885760
120.149584	3384.452749	23.890778
120.477747	3399.795578	23.895795
120.453317	3410.510038	23.900813
120.916387	3403.297373	23.905831
120.642990	3397.280032	23.910848
120.984339	3414.620316	23.915866
121.362548	3427.386775	23.920883
121.313485	3434.658051	23.925901
121.035960	3425.657499	23.930919
121.350420	3427.370237	23.935936
121.546777	3437.639569	23.940954
122.162024	3456.874422	23.945971
122.052191	3474.053101	23.950989
121.877648	3472.715904	23.956007
122.095621	3462.975574	23.961024
121.823730	3472.825839	23.966042
122.292010	3465.688270	23.971059
122.246825	3481.733036	23.976077
122.263307	3488.740354	23.981095
122.549850	3497.084565	23.986112
122.433899	3502.195639	23.991130
123.017754	3514.856929	23.996147
122.915135	3529.703738	24.001165
123.051987	3530.770629	24.006183
123.108942	3521.361991	24.011200
123.065022	3529.121051	24.016218
123.563232	3534.603101	24.021235
123.767168	3549.956369	24.026253
123.634852	3552.789419	24.031271
123.726640	3553.662574	24.036288
123.498042	3564.476232	24.041306
124.313018	3563.596398	24.046323
124.713328	3574.418350	24.051341
125.000306	3564.592931	24.056359
125.141692	3564.526380	24.061376
124.784280	3560.309895	24.066394
125.210581	3551.818965	24.071411
125.373914	3557.989832	24.076429
125.129117	3557.354799	24.081447
125.068902	3562.732671	24.086464
125.041413	3558.970735	24.091482
125.532389	3554.403827	24.096499
125.347178	3547.885234	24.101517
125.418215	3570.008226	24.106535
125.741286	3583.208736	24.111552
125.793414	3586.529041	24.116570
126.255306	3578.258204	24.121587
125.766652	3581.480460	24.126605
125.790687	3601.567921	24.131623
126.245512	3610.693063	24.136640
126.183725	3620.043735	24.141658
126.286245	3625.359305	24.146675
126.300425	3640.951109	24.151693
126.704701	3649.912970	24.156711
127.063504	3647.515167	24.161728
126.819693	3639.330197	24.166746
127.581875	3645.213167	24.171763
127.565822	3669.349554	24.176781
127.559605	3677.946966	24.181799
127.542210	3680.867352	24.186816
127.637004	3670.499986	24.191834
127.866485	3671.998837	24.196851
128.053351	3685.196348	24.201869
128.270485	3690.751670	24.206887
128.739075	3703.554999	24.211904
128.952273	3689.278981	24.216922
129.378728	3678.978071	24.221939
129.505761	3687.923164	24.226957
129.298665	3682.388863	24.231975
129.347736	3670.914065	24.236992
129.174697	3686.077390	24.242010
129.312387	3687.474871	24.247027
129.568341	3686.765751	24.252045
129.310642	3686.242295	24.257063
129.766112	3676.251560	24.262080
129.136895	3685.412166	24.267098
129.305296	3701.428165	24.272115
129.357035	3714.575587	24.277133
129.480252	3726.435583	24.282151
130.175879	3732.853221	24.287168
130.387460	3740.456385	24.292186
130.209354	3750.555903	24.297203
130.567741	3755.805617	24.302221
130.806058	3772.586931	24.307239
130.974123	3763.316485	24.312256
130.831161	3764.118202	24.317274
131.531907	3763.106049	24.322291
131.337812	3755.069107	24.327309
131.371096	3761.144217	24.332327
131.656035	3773.854325	24.337344
131.366080	3792.258823	24.342362
131.507784	3792.037096	24.347379
132.012387	3803.478216	24.352397
132.211988	3810.764093	24.357415
132.797322	3812.637637	24.362432
132.259974	3810.303237	24.367450
132.193295	3820.056031	24.372467
132.367801	3809.946670	24.377485
132.451868	3824.435737	24.382503
132.859082	3828.013573	24.387520
132.668163	3849.877876	24.392538
132.850276	3851.493236	24.397555
133.309037	3842.900325	24.402573
132.984127	3852.794237	24.407591
133.378642	3855.547771	24.412608
133.820618	3866.655967	24.417626
134.114337	3863.838556	24.422643
134.192499	3872.944593	24.427661
134.040090	3876.907834	24.432679
133.992250	3866.396184	24.437696
134.449274	3862.669474	24.442714
134.102315	3881.122473	24.447731
134.586791	3891.540569	24.452749
134.861284	3894.604898	24.457767
135.042647	3881.118640	24.462784
135.276342	3877.839867	24.467802
135.279554	3876.290579	24.472819
135.372587	3871.783036	24.477837
135.341815	3885.096996	24.482855
135.682503	3894.567163	24.487872
135.925119	3904.846091	24.492890
135.780838	3902.543189	24.497907
135.821723	3915.895731	24.502925
135.984923	3909.863531	24.507943
136.106433	3896.608418	24.512960
135.975606	3910.868496	24.517978
136.323258	3917.750812	24.522995
136.799237	3919.394004	24.528013
136.385583	3928.691186	24.533031
136.349160	3935.596419	24.538048
136.585912	3950.940725	24.543066
136.868980	3953.439059	24.548083
137.344507	3954.177173	24.553101
137.239706	3970.726409	24.558119
137.671982	3972.339030	24.563136
137.694240	3983.020578	24.568154
137.768076	3979.891432	24.573171
138.039345	3982.434241	24.578189
137.971043	4002.923321	24.583207
138.181651	4001.187777	24.588224
138.474596	4002.741137	24.593242
138.422754	3991.920600	24.598259
138.731775	3995.552892	24.603277
139.304431	4000.107807	24.608295
139.454947	4015.847546	24.613312
139.715311	4014.851057	24.618330
139.651680	4019.661909	24.623347
139.906187	4008.110789	24.628365
139.826484	4012.110872	24.633383
139.857889	4009.571041	24.638400
140.033522	4012.735591	24.643418
140.119393	4008.572908	24.648435
140.292424	4019.184290	24.653453
140.182050	4016.144632	24.658471
140.417269	4012.160429	24.663488
140.199246	4025.391666	24.668506
140.156067	4039.666121	24.673523
140.447936	4042.855173	24.678541
140.482109	4049.815725	24.683559
140.373542	4068.563823	24.688576
140.524783	4076.518085	24.693594
141.060316	4096.877985	24.698611
141.224492	4107.848783	24.703629
141.177235	4113.012882	24.708647
141.396053	4107.762795	24.713664
141.717977	4126.570546	24.718682
141.837971	4139.825559	24.723699
142.263559	4134.073951	24.728717
141.972452	4139.226379	24.733735
142.440254	4151.054567	24.738752
142.144644	4165.260211	24.743770
142.516444	4168.064015	24.748787
142.641745	4169.776203	24.753805
142.758521	4183.129427	24.758823
142.949144	4202.128660	24.763840
143.227977	4185.260487	24.768858
143.326218	4198.669546	24.773875
143.529766	4188.211028	24.778893
143.798026	4208.705794	24.783911
143.808592	4218.628761	24.788928
144.022756	4214.064881	24.793946
143.836651	4226.388205	24.798963
144.348358	4225.849808	24.803981
144.343841	4226.135729	24.808999
144.916485	4231.057667	24.814016
145.003069	4247.477141	24.819034
144.708347	4240.901149	24.824051
144.731047	4249.321647	24.829069
144.768020	4246.945041	24.834087
145.113346	4258.974268	24.839104
145.472335	4273.236425	24.844122
145.567379	4278.113664	24.849139
145.873561	4260.586125	24.854157
145.675724	4277.620772	24.859175
145.793006	4290.531064	24.864192
145.535689	4300.857425	24.869210
145.793653	4300.963748	24.874227
146.261942	4318.439589	24.879245
146.496549	4323.677665	24.884263
146.833550	4327.622361	24.889280
147.022425	4334.942543	24.894298
147.026456	4328.966405	24.899315
147.506491	4337.571243	24.904333
147.728303	4350.093422	24.909351
147.843590	4352.649861	24.914368
148.201978	4357.958053	24.919386
148.032610	4357.017588	24.924403
148.215888	4346.702480	24.929421
147.954125	4348.469588	24.934439
148.118218	4344.606116	24.939456
148.259789	4344.924204	24.944474
148.187754	4375.842648	24.949491
148.306164	4377.808771	24.954509
148.096558	4390.374706	24.959527
148.326122	4403.576009	24.964544
148.814672	4408.522136	24.969562
148.875372	4420.525285	24.974579
149.567477	4421.572152	24.979597
149.618209	4432.434749	24.984615
149.791017	4432.569318	24.989632
149.966707	4435.344547	24.994650
149.977757	4454.092636	24.999667
150.541463	4443.599242	25.004685
150.050718	4452.110200	25.009703
150.251250	4457.700827	25.014720
150.726563	4457.547206	25.019738
150.190569	4481.740445	25.024755
150.959327	4485.468555	25.029773
150.572351	4483.278114	25.034791
150.895440	4487.926778	25.039808
151.159428	4501.534713	25.044826
151.145646	4507.576943	25.049843
151.763839	4512.324110	25.054861
151.984213	4537.865014	25.059879
152.378623	4528.105893	25.064896
152.709985	4523.411526	25.069914
152.605551	4516.137388	25.074931
152.950279	4520.497032	25.079949
153.048758	4510.938011	25.084967
152.849845	4510.480801	25.089984
153.162497	4517.888893	25.095002
153.000706	4523.299630	25.100019
153.299921	4505.199302	25.105037
153.417130	4514.405964	25.110055
153.729558	4518.016161	25.115072
153.978100	4499.926574	25.120090
153.806756	4515.349893	25.125107
154.051482	4515.465493	25.130125
154.139440	4546.695267	25.135143
153.968610	4541.909057	25.140160
154.113540	4543.199112	25.145178
154.143581	4558.017892	25.150195
154.437602	4558.939586	25.155213
154.571991	4569.830192	25.160231
154.394641	4567.595651	25.165248
154.765480	4595.789565	25.170266
154.867734	4607.587944	25.175283
155.317524	4606.307343	25.180301
155.299585	4633.619815	25.185319
155.560080	4619.084325	25.190336
156.017508	4626.302392	25.195354
155.643297	4630.235536	25.200371
156.189889	4646.338851	25.205389
156.346801	4654.004257	25.210407
155.958656	4651.017459	25.215424
156.662224	4664.684805	25.220442
156.872235	4682.365164	25.225459
156.542992	4678.048826	25.230477
156.952321	4692.846406	25.235495
157.081625	4709.214028	25.240512
157.436772	4720.418294	25.245530
157.378503	4721.555702	25.250547
157.894383	4740.877867	25.255565
157.800339	4735.376482	25.260583
157.811158	4741.096599	25.265600
158.265571	4738.557234	25.270618
158.119665	4757.800169	25.275635
158.836878	4755.266989	25.280653
158.533186	4761.287135	25.285671
158.386612	4770.710384	25.290688
158.886077	4783.373273	25.295706
158.955075	4795.552127	25.300723
159.155966	4803.801736	25.305741
159.660939	4819.271887	25.310759
159.766101	4814.246271	25.315776
160.037700	4814.113315	25.320794
160.105848	4802.415220	25.325811
160.448972	4799.355207	25.330829
160.930042	4818.235933	25.335847
160.871467	4832.895190	25.340864
161.258380	4843.128060	25.345882
161.110506	4834.767929	25.350899
161.267282	4828.948269	25.355917
161.052201	4826.850253	25.360935
161.244621	4840.930985	25.365952
161.214830	4823.446124	25.370970
161.252074	4846.467151	25.375987
161.722634	4858.340704	25.381005
161.575477	4861.316219	25.386023
161.721734	4869.525672	25.391040
162.206495	4885.368558	25.396058
162.145255	4891.959778	25.401075
162.343968	4907.337300	25.406093
162.749079	4913.575855	25.411111
162.469197	4930.974805	25.416128
162.925495	4931.970113	25.421146
163.280331	4948.125112	25.426163
163.014299	4955.687697	25.431181
163.407171	4959.129178	25.436199
163.332275	4956.466979	25.441216
163.937093	4965.620507	25.446234
163.662874	4977.621543	25.451251
163.766198	4978.888979	25.456269
163.905028	4988.160072	25.461287
164.268344	5001.981190	25.466304
164.553937	4999.772468	25.471322
164.757834	5009.210794	25.476339
164.834216	5035.372039	25.481357
165.232944	5042.371627	25.486375
165.126943	5042.237275	25.491392
165.492192	5035.296358	25.496410
165.622091	5049.818758	25.501427
166.063879	5058.476386	25.506445
166.130533	5061.150045	25.511463
166.199647	5077.937100	25.516480
166.425933	5065.243673	25.521498
166.707757	5066.838355	25.526515
166.758728	5076.391371	25.531533
167.148276	5089.661714	25.536551
166.683521	5089.302748	25.541568
166.921868	5087.962155	25.546586
166.814655	5116.103698	25.551603
166.950126	5124.734014	25.556621
167.539454	5121.698227	25.561639
167.632992	5132.699137	25.566656
167.567832	5149.049739	25.571674
167.839264	5153.968588	25.576691
168.171082	5172.203459	25.581709
168.425571	5178.265409	25.586727
168.719076	5182.555348	25.591744
169.154521	5178.537769	25.596762
168.983300	5201.079526	25.601779
169.075734	5201.330152	25.606797
169.299899	5190.582092	25.611815
169.631656	5203.497865	25.616832
169.510779	5215.705663	25.621850
169.554839	5224.581481	25.626867
169.892118	5225.307463	25.631885
170.008200	5231.143060	25.636903
170.174111	5246.858267	25.641920
170.488179	5253.766020	25.646938
170.542279	5261.765288	25.651955
171.012156	5281.722970	25.656973
171.255413	5271.360332	25.661991
171.112996	5283.070104	25.667008
171.456675	5278.564449	25.672026
171.489814	5296.024301	25.677044
171.433300	5314.882629	25.682061
171.715988	5306.261316	25.687079
172.080225	5333.050385	25.692096
172.372690	5329.050486	25.697114
172.483892	5337.504198	25.702132
172.696972	5341.647607	25.707149
172.956066	5336.920053	25.712167
172.783307	5360.831370	25.717184
173.140580	5367.592647	25.722202
173.492066	5371.973072	25.727220
173.542988	5351.338045	25.732237
174.110007	5359.520759	25.737255
173.745612	5372.413095	25.742272
174.213234	5384.651757	25.747290
174.565274	5369.399566	25.752308
174.541486	5383.273172	25.757325
174.884836	5378.321814	25.762343
174.736094	5381.133494	25.767360
174.992419	5376.464267	25.772378
174.879486	5391.284229	25.777396
174.945691	5391.458866	25.782413
175.293096	5399.160102	25.787431
175.316240	5411.057998	25.792448
175.430877	5418.770141	25.797466
175.700533	5436.275727	25.802484
176.064686	5433.896463	25.807501
176.014751	5422.714335	25.812519
175.998312	5448.390751	25.817536
176.340035	5459.289458	25.822554
176.438053	5466.378299	25.827572
176.473959	5483.151982	25.832589
176.663202	5489.649303	25.837607
176.984312	5505.338338	25.842624
177.122987	5520.915780	25.847642
177.035569	5526.383873	25.852660
177.086344	5537.512623	25.857677
177.700733	5548.490767	25.862695
177.558644	5564.792299	25.867712
178.131570	5566.594486	25.872730
178.370448	5577.537831	25.877748
178.357465	5585.553073	25.882765
178.701339	5603.714005	25.887783
178.632756	5610.908403	25.892800
178.978523	5615.688326	25.897818
179.546398	5622.920898	25.902836
179.424272	5632.231553	25.907853
179.795920	5629.977812	25.912871
179.966100	5650.389875	25.917888
180.192176	5662.891534	25.922906
180.299050	5651.788074	25.927924
180.189597	5660.373708	25.932941
180.890337	5680.394951	25.937959
180.851192	5694.279244	25.942976
180.797592	5691.197195	25.947994
180.866390	5701.145738	25.953012
181.143149	5715.867754	25.958029
181.565489	5724.427770	25.963047
181.683815	5725.282489	25.968064
181.844566	5745.966355	25.973082
182.220496	5754.756138	25.978100
182.161613	5750.756696	25.983117
182.833097	5766.055373	25.988135
183.127100	5787.789099	25.993152
183.473074	5772.198885	25.998170
183.540009	5773.183377	26.003188
183.658596	5767.911105	26.008205
183.520044	5765.784958	26.013223
183.952493	5773.373100	26.018240
183.788557	5776.891408	26.023258
184.064325	5784.203033	26.028276
184.020568	5789.781345	26.033293
184.465826	5782.424062	26.038311
185.129187	5782.645336	26.043328
184.909210	5794.608893	26.048346
185.085962	5799.018311	26.053364
185.156615	5817.629423	26.058381
185.356607	5812.953232	26.063399
185.393513	5813.559162	26.068416
185.534540	5812.838229	26.073434
185.840282	5828.583287	26.078452
185.855255	5851.587813	26.083469
185.704050	5844.734630	26.088487
186.090534	5862.398191	26.093504
185.956950	5861.343040	26.098522
186.223670	5881.731577	26.103540
186.445170	5898.314382	26.108557
186.707947	5903.331765	26.113575
186.730644	5927.378606	26.118592
186.536670	5939.765608	26.123610
187.136374	5949.788033	26.128628
186.877792	5968.626193	26.133645
187.743918	5976.742881	26.138663
188.032067	5995.572642	26.143680
188.196749	5999.796677	26.148698
188.787340	6002.926542	26.153716
188.934718	6021.900087	26.158733
188.955217	6016.780183	26.163751
189.344392	6025.599432	26.168768
189.506243	6016.272768	26.173786
189.842289	6011.601603	26.178804
190.110852	6019.967467	26.183821
190.072898	6017.707322	26.188839
190.433601	6042.268669	26.193856
190.278855	6048.101672	26.198874
190.777677	6052.011412	26.203892
190.465374	6048.686948	26.208909
190.770745	6055.768573	26.213927
191.003759	6064.790843	26.218944
190.961412	6071.097496	26.223962
191.216436	6063.977063	26.228980
190.916728	6100.194541	26.233997
191.367249	6104.964395	26.239015
191.685533	6118.289128	26.244032
191.583578	6131.435231	26.249050
192.292412	6140.541949	26.254068
192.147917	6154.100685	26.259085
192.490765	6156.974611	26.264103
192.772578	6175.857614	26.269120
193.045231	6199.700550	26.274138
193.251814	6199.390107	26.279156
193.090744	6216.713749	26.284173
193.663656	6220.211215	26.289191
193.663880	6227.333098	26.294208
193.782422	6246.034461	26.299226
194.408977	6241.860213	26.304244
194.678791	6250.255134	26.309261
195.160439	6266.184993	26.314279
195.492973	6267.171310	26.319296
195.411893	6274.493298	26.324314
195.913445	6265.367889	26.329332
195.361557	6272.005315	26.334349
195.572819	6263.016864	26.339367
195.800438	6274.171258	26.344384
195.767053	6290.474482	26.349402
196.166437	6299.461523	26.354420
196.622678	6316.297379	26.359437
196.362354	6310.033786	26.364455
196.630873	6329.315309	26.369472
196.644208	6337.282483	26.374490
197.276066	6344.525297	26.379508
197.621684	6353.095186	26.384525
198.060312	6374.638081	26.389543
198.422977	6364.392032	26.394560
198.807895	6370.135200	26.399578
199.009915	6367.827479	26.404596
198.919844	6354.676129	26.409613
199.278442	6361.428563	26.414631
199.628188	6361.519743	26.419648
199.412283	6361.550022	26.424666
199.366264	6353.343543	26.429684
199.146525	6353.447698	26.434701
199.539104	6368.934021	26.439719
199.804607	6390.883571	26.444736
199.809314	6391.211323	26.449754
200.370618	6390.029509	26.454772
200.391900	6407.940677	26.459789
200.217784	6420.804398	26.464807
200.139128	6418.713944	26.469824
200.215170	6442.553506	26.474842
200.827862	6446.992674	26.479860
200.910977	6463.620993	26.484877
201.038440	6484.746853	26.489895
201.312153	6484.381997	26.494912
201.259429	6497.487194	26.499930
201.812311	6509.073152	26.504948
201.748782	6531.856949	26.509965
202.125289	6546.532550	26.514983
202.388818	6561.281961	26.520000
202.534062	6573.312563	26.525018
202.669652	6577.029642	26.530036
202.716720	6595.700702	26.535053
203.093296	6614.417363	26.540071
203.384389	6624.687318	26.545088
203.901339	6641.974221	26.550106
204.191529	6655.845114	26.555124
204.667869	6655.962634	26.560141
204.867832	6649.453526	26.565159
205.099509	6662.445714	26.570176
205.032164	6684.000177	26.575194
205.257073	6683.028287	26.580212
205.719673	6678.160389	26.585229
206.632887	6660.647625	26.590247
206.923737	6646.439967	26.595264
206.902511	6651.966032	26.600282
207.111482	6643.921252	26.605300
207.378034	6645.499723	26.610317
207.096242	6652.937743	26.615335
207.450139	6652.180815	26.620352
207.412996	6655.376729	26.625370
207.440163	6664.055322	26.630388
207.468870	6678.684553	26.635405
207.670357	6682.297836	26.640423
207.918381	6694.106780	26.645440
207.917085	6714.684021	26.650458
208.069164	6718.596879	26.655476
208.118423	6726.622896	26.660493
208.338668	6746.745373	26.665511
208.507951	6751.357913	26.670528
208.578134	6785.674500	26.675546
208.900746	6804.921680	26.680564
208.868875	6818.609655	26.685581
209.084379	6832.216604	26.690599
209.759343	6838.586979	26.695616
209.919405	6861.952560	26.700634
209.928518	6879.504775	26.705652
210.423913	6904.946998	26.710669
210.623970	6908.183318	26.715687
210.918521	6905.586153	26.720704
210.916472	6930.171807	26.725722
211.444220	6938.463836	26.730740
211.519290	6952.633587	26.735757
211.573577	6972.799525	26.740775
211.967173	6963.847495	26.745792
212.238507	6983.367207	26.750810
212.318607	6988.958557	26.755828
212.900404	6996.622644	26.760845
213.005757	7017.805640	26.765863
213.247113	7027.939949	26.770880
212.957786	7031.481615	26.775898
213.177312	7038.365220	26.780916
213.687537	7054.418749	26.785933
214.229280	7045.344535	26.790951
214.744239	7052.636137	26.795968
214.310351	7077.639910	26.800986
214.575001	7065.229551	26.806004
214.806056	7071.218138	26.811021
215.040229	7089.053163	26.816039
215.344090	7102.633145	26.821056
215.436515	7115.046994	26.826074
215.660842	7107.649994	26.831092
215.749583	7118.634973	26.836109
215.479818	7142.561083	26.841127
216.242320	7138.385409	26.846144
216.432225	7163.387065	26.851162
216.635967	7169.337673	26.856180
216.767531	7174.710298	26.861197
216.616369	7198.976828	26.866215
217.240405	7199.704757	26.871232
217.211622	7222.097100	26.876250
217.418322	7226.116048	26.881268
217.926766	7243.612946	26.886285
218.009363	7263.272089	26.891303
218.558230	7269.235808	26.896320
218.301882	7288.759597	26.901338
218.728118	7291.562463	26.906356
219.253542	7297.359157	26.911373
219.194105	7308.199417	26.916391
220.214418	7311.761832	26.921408
219.784083	7326.581709	26.926426
220.122525	7342.910435	26.931444
220.530196	7342.298963	26.936461
220.274873	7344.652098	26.941479
220.833513	7355.258740	26.946496
221.131187	7373.451407	26.951514
220.987306	7385.086976	26.956532
221.457560	7402.466706	26.961549
221.452846	7408.785003	26.966567
222.113077	7410.786039	26.971584
222.024446	7418.694208	26.976602
221.790973	7434.144038	26.981620
222.305052	7436.433073	26.986637
222.149828	7449.318924	26.991655
222.857758	7459.997847	26.996672
222.693194	7494.683193	27.001690
223.064739	7502.610675	27.006708
223.857742	7522.063765	27.011725
223.713915	7517.999147	27.016743
223.795735	7511.751791	27.021760
223.864484	7548.572518	27.026778
224.428976	7551.925973	27.031796
224.616027	7583.180853	27.036813
224.731174	7586.669203	27.041831
225.145328	7598.879053	27.046848
225.255776	7602.157889	27.051866
225.068068	7614.864151	27.056884
225.810302	7638.596239	27.061901
225.779227	7645.656985	27.066919
226.295766	7659.215699	27.071936
226.434520	7668.047320	27.076954
226.593465	7683.890165	27.081972
227.111358	7691.257192	27.086989
226.870674	7703.918720	27.092007
227.510831	7718.522713	27.097024
227.651319	7736.520447	27.102042
227.634070	7740.160663	27.107060
228.281322	7744.974131	27.112077
228.826401	7736.654307	27.117095
229.350773	7736.446494	27.122112
229.640488	7743.137658	27.127130
229.573205	7740.684417	27.132148
229.757314	7738.164437	27.137165
229.884618	7743.315851	27.142183
230.015315	7737.270626	27.147200
230.207674	7744.240942	27.152218
230.360921	7759.162496	27.157236
230.658103	7770.797150	27.162253
230.572903	7757.565849	27.167271
230.922650	7776.878257	27.172288
231.159143	7797.607438	27.177306
230.995967	7808.827488	27.182324
231.334268	7804.691015	27.187341
231.191189	7831.989545	27.192359
231.411855	7832.720356	27.197376
231.245341	7858.240399	27.202394
231.736343	7881.515005	27.207412
232.117672	7896.958223	27.212429
232.074979	7915.885114	27.217447
232.036004	7940.651719	27.222464
232.542657	7964.757178	27.227482
232.450271	7995.873947	27.232500
233.105082	8005.517613	27.237517
233.336488	8025.994314	27.242535
233.694975	8064.260156	27.247552
234.236256	8060.127888	27.252570
234.209187	8086.293965	27.257588
234.501931	8093.828341	27.262605
234.622286	8122.580365	27.267623
234.857126	8127.977998	27.272640
235.228914	8147.052498	27.277658
235.342249	8170.189077	27.282676
236.229588	8198.820033	27.287693
236.317458	8212.735175	27.292711
236.945959	8210.318133	27.297728
237.388612	8207.122095	27.302746
237.229617	8217.734466	27.307764
237.636352	8229.442725	27.312781
237.656859	8237.067045	27.317799
238.039375	8245.952445	27.322816
238.342236	8266.851647	27.327834
238.403890	8280.334035	27.332852
238.907446	8270.280874	27.337869
238.957369	8285.921004	27.342887
239.139161	8291.388106	27.347904
239.013019	8302.256606	27.352922
239.321565	8320.282372	27.357940
239.816915	8333.820751	27.362957
239.794114	8365.312697	27.367975
240.114723	8371.436638	27.372992
240.158831	8378.040263	27.378010
240.138684	8398.499145	27.383028
240.634592	8413.108713	27.388045
240.634978	8429.864615	27.393063
240.604654	8444.391021	27.398080
241.153080	8469.623002	27.403098
241.395264	8503.108330	27.408116
241.674778	8511.584773	27.413133
242.236856	8519.007903	27.418151
242.635878	8528.078987	27.423168
243.028957	8549.025093	27.428186
243.140963	8557.292937	27.433204
243.629073	8564.926013	27.438221
243.766170	8583.621565	27.443239
243.955386	8584.861714	27.448256
244.371739	8602.420233	27.453274
244.459039	8609.238940	27.458292
244.502888	8617.830780	27.463309
244.633314	8639.304816	27.468327
244.634867	8646.325959	27.473344
245.111594	8661.652553	27.478362
245.258971	8673.379574	27.483380
245.655681	8678.315857	27.488397
245.662708	8707.003382	27.493415
245.952382	8709.339926	27.498432
246.133982	8717.979164	27.503450
246.055056	8746.223323	27.508468
247.071087	8753.020978	27.513485
246.992731	8768.290516	27.518503
247.411864	8778.461954	27.523520
247.646478	8787.734427	27.528538
247.609093	8808.493638	27.533556
248.262693	8821.340702	27.538573
248.669811	8821.354688	27.543591
248.617858	8821.797401	27.548608
249.228786	8843.208867	27.553626
249.560503	8853.247500	27.558644
249.552631	8855.426065	27.563661
249.692777	8873.972584	27.568679
249.855040	8888.650318	27.573696
250.071912	8891.343921	27.578714
250.552863	8908.262748	27.583732
250.691255	8916.399603	27.588749
250.718382	8935.988066	27.593767
250.852175	8954.918542	27.598784
251.173797	8956.672472	27.603802
251.617602	8971.551100	27.608820
251.988682	8985.702120	27.613837
252.109237	9009.393260	27.618855
252.517009	9020.542676	27.623872
253.077321	9035.478521	27.628890
253.054547	9040.792998	27.633908
253.268887	9038.723893	27.638925
253.487218	9055.787879	27.643943
253.661887	9064.103923	27.648960
254.192664	9079.491309	27.653978
254.063724	9092.989334	27.658996
254.316644	9105.776798	27.664013
254.887063	9124.532939	27.669031
255.203554	9136.940498	27.674048
255.597715	9146.414464	27.679066
255.610090	9160.624905	27.684084
255.583590	9164.572601	27.689101
255.831951	9188.095593	27.694119
256.045381	9212.590894	27.699136
256.803096	9216.271192	27.704154
256.728756	9227.041966	27.709172
256.992454	9251.555016	27.714189
257.141291	9253.117758	27.719207
257.572882	9280.152109	27.724224
257.893363	9283.017710	27.729242
258.170212	9304.499960	27.734260
258.425957	9304.410564	27.739277
258.912050	9313.895437	27.744295
258.801222	9342.338122	27.749312
259.439451	9350.810889	27.754330
259.578015	9354.555704	27.759348
259.984540	9358.698937	27.764365
259.466919	9377.480748	27.769383
259.450465	9389.792273	27.774400
260.120131	9393.031078	27.779418
259.737129	9442.119798	27.784436
260.060606	9457.665471	27.789453
260.612662	9476.861454	27.794471
260.602083	9508.641155	27.799488
260.992564	9528.490913	27.804506
261.447471	9553.363543	27.809524
262.174126	9561.430320	27.814541
262.678433	9575.529135	27.819559
262.691684	9591.920210	27.824576
263.045722	9588.901601	27.829594
263.464030	9609.629104	27.834612
263.915634	9614.017815	27.839629
263.871795	9621.921253	27.844647
263.947281	9632.950338	27.849664
264.306161	9644.592718	27.854682
264.359079	9656.664548	27.859700
264.824978	9667.447979	27.864717
264.786144	9682.111619	27.869735
265.284790	9698.105945	27.874752
265.451284	9702.572506	27.879770
265.389703	9728.112867	27.884788
266.070273	9746.743627	27.889805
266.805953	9753.597494	27.894823
266.844223	9768.420985	27.899840
266.866669	9769.606072	27.904858
267.386921	9789.212577	27.909876
267.516358	9803.290030	27.914893
267.547555	9814.805495	27.919911
267.723890	9843.571861	27.924928
268.116088	9842.678493	27.929946
268.603069	9860.742697	27.934964
268.549031	9873.579130	27.939981
269.048057	9901.127234	27.944999
269.074429	9912.941330	27.950016
269.587089	9921.748668	27.955034
269.542957	9955.276477	27.960052
269.627110	9970.072093	27.965069
269.789832	9983.447060	27.970087
270.051556	10010.984145	27.975104
270.875646	10022.574363	27.980122
271.107191	10048.343302	27.985140
271.153287	10066.293098	27.990157
271.736737	10081.653061	27.995175
272.104193	10088.934997	28.000192
272.162960	10118.287667	28.005210
272.635923	10139.759912	28.010228
272.987806	10137.168514	28.015245
273.073366	10149.516548	28.020263
272.918791	10177.926985	28.025280
273.642985	10181.831257	28.030298
273.665611	10215.578604	28.035316
273.879708	10220.931538	28.040333
274.202243	10242.727331	28.045351
274.196831	10275.605036	28.050368
274.880403	10295.799627	28.055386
275.141428	10315.482693	28.060404
275.395084	10332.624137	28.065421
275.855170	10352.901413	28.070439
275.519613	10369.581724	28.075456
276.080639	10386.425089	28.080474
276.383491	10410.319003	28.085492
276.530639	10418.930983	28.090509
277.110423	10444.655632	28.095527
277.471383	10462.754731	28.100544
278.122444	10469.110060	28.105562
278.291165	10489.668036	28.110580
278.526954	10514.442872	28.115597
279.149289	10513.005706	28.120615
279.243187	10539.823055	28.125632
279.570088	10524.737089	28.130650
279.855805	10542.722668	28.135668
279.743888	10563.554767	28.140685
280.294650	10556.761601	28.145703
280.486102	10586.235793	28.150720
280.525352	10603.724904	28.155738
280.768358	10622.671614	28.160756
280.708147	10638.478771	28.165773
280.945697	10647.202770	28.170791
281.098405	10670.349865	28.175808
281.544080	10678.376983	28.180826
282.090825	10701.269958	28.185844
281.888265	10724.589265	28.190861
282.257368	10745.668268	28.195879
282.628337	10780.498372	28.200896
282.793132	10803.505014	28.205914
283.333905	10818.556842	28.210932
283.825120	10824.858370	28.215949
284.356641	10839.907020	28.220967
284.440250	10857.133840	28.225984
284.996932	10861.159705	28.231002
285.524660	10873.353317	28.236020
285.448642	10890.475773	28.241037
285.920378	10891.232214	28.246055
286.760543	10898.671971	28.251072
287.127951	10897.789736	28.256090
287.080963	10904.716691	28.261108
287.089953	10915.137663	28.266125
287.586787	10930.794782	28.271143
287.491885	10941.139977	28.276160
287.537388	10954.895927	28.281178
288.095497	10974.310143	28.286196
288.100856	10999.158461	28.291213
288.534117	11000.519194	28.296231
288.514749	11037.965983	28.301248
288.544195	11054.690689	28.306266
289.039021	11076.585987	28.311284
288.879438	11106.824989	28.316301
289.356755	11132.295886	28.321319
289.455696	11157.539427	28.326336
290.014775	11177.087654	28.331354
290.671924	11200.757202	28.336372
290.438293	11229.374780	28.341389
290.999003	11251.239738	28.346407
290.854502	11275.203335	28.351424
291.242493	11308.503445	28.356442
291.946740	11324.899515	28.361460
292.363465	11358.343876	28.366477
292.927668	11371.100636	28.371495
293.366739	11390.457820	28.376512
293.885145	11409.484434	28.381530
293.941405	11411.728381	28.386548
294.124885	11439.280060	28.391565
294.381154	11445.814451	28.396583
294.581031	11457.452124	28.401600
294.834228	11470.873260	28.406618
295.274970	11487.068810	28.411636
295.749170	11508.682920	28.416653
296.015772	11532.085024	28.421671
295.953272	11543.383230	28.426688
296.489886	11568.310099	28.431706
297.070195	11576.453295	28.436724
297.100000	11594.233385	28.441741
297.551116	11595.994582	28.446759
297.633244	11627.911277	28.451776
297.668688	11650.218075	28.456794
298.243253	11661.968890	28.461812
298.281591	11685.949372	28.466829
298.626082	11693.046760	28.471847
298.857749	11722.201265	28.476864
299.245071	11744.748645	28.481882
299.609952	11772.605750	28.486900
299.775024	11787.888367	28.491917
300.110263	11799.125769	28.496935
300.040763	11836.969520	28.501952
300.232935	11852.001131	28.506970
300.998179	11876.147786	28.511988
300.873199	11893.477142	28.517005
301.256714	11912.236717	28.522023
301.608560	11923.503764	28.527040
301.563456	11952.439699	28.532058
302.175321	11968.274212	28.537076
302.423260	11995.100841	28.542093
303.027702	12024.418841	28.547111
303.084793	12050.595615	28.552128
303.470546	12070.116055	28.557146
304.103308	12079.805246	28.562164
303.838195	12107.633866	28.567181
304.534690	12131.076117	28.572199
304.373599	12151.783673	28.577216
304.512726	12185.661658	28.582234
305.363840	12194.831897	28.587252
305.780292	12211.846822	28.592269
306.366596	12232.955711	28.597287
306.835841	12253.201579	28.602304
307.205855	12266.292880	28.607322
307.464657	12280.179384	28.612340
307.584377	12309.351082	28.617357
307.843313	12323.354202	28.622375
308.147481	12329.723471	28.627392
308.537446	12365.837282	28.632410
308.638983	12367.719349	28.637428
308.917906	12406.282905	28.642445
309.355348	12419.246590	28.647463
309.504492	12447.838544	28.652480
309.847431	12472.629423	28.657498
310.231903	12483.912745	28.662516
310.277426	12509.446131	28.667533
310.442995	12510.920555	28.672551
310.790514	12547.586983	28.677568
310.899367	12567.399584	28.682586
311.859937	12579.129847	28.687604
312.494586	12602.271797	28.692621
312.703409	12625.258801	28.697639
313.025772	12646.161296	28.702656
313.505599	12662.200304	28.707674
313.683358	12671.356004	28.712692
313.739494	12682.088627	28.717709
314.471993	12708.118643	28.722727
314.750335	12709.954208	28.727744
314.912077	12741.467593	28.732762
314.927090	12757.113916	28.737780
315.096479	12782.141940	28.742797
315.068944	12802.309844	28.747815
315.798116	12834.029058	28.752832
316.155298	12852.565596	28.757850
316.429855	12865.879579	28.762868
316.810840	12891.717420	28.767885
316.719045	12930.809897	28.772903
317.518881	12948.580082	28.777920
317.743965	12964.795417	28.782938
318.144744	12979.779434	28.787956
318.399281	13002.387542	28.792973
318.518255	13028.237371	28.797991
318.792120	13044.520364	28.803008
319.043091	13071.257674	28.808026
319.934459	13084.282420	28.813044
320.245555	13115.264459	28.818061
320.509153	13124.787573	28.823079
321.170923	13142.919575	28.828096
321.385333	13156.503739	28.833114
321.911424	13172.633311	28.838132
322.125599	13192.314246	28.843149
322.086407	13192.517812	28.848167
322.901673	13206.399851	28.853184
322.806937	13234.002921	28.858202
323.120595	13230.818555	28.863220
323.474808	13261.850481	28.868237
323.673059	13250.177484	28.873255
324.096851	13270.492020	28.878272
324.183016	13285.474720	28.883290
324.808672	13304.777382	28.888308
324.968652	13317.931027	28.893325
324.744648	13352.621527	28.898343
325.360615	13370.983540	28.903360
325.250492	13395.113209	28.908378
325.518255	13413.961415	28.913396
325.864949	13440.131989	28.918413
326.008401	13477.691478	28.923431
326.579729	13498.007138	28.928448
326.697511	13523.123624	28.933466
327.112482	13550.756485	28.938484
327.236903	13591.962676	28.943501
327.512566	13615.746866	28.948519
328.178847	13641.757812	28.953536
328.681098	13676.823832	28.958554
329.115655	13697.111912	28.963572
329.190508	13728.282280	28.968589
329.918119	13758.955637	28.973607
330.035579	13785.520779	28.978624
330.481017	13819.302727	28.983642
330.553442	13846.181122	28.988660
331.257371	13865.870213	28.993677
331.041115	13901.244520	28.998695
331.972881	13919.488800	29.003712
331.725324	13949.672792	29.008730
332.500164	13967.161426	29.013748
332.517185	14005.600289	29.018765
332.615110	14044.865814	29.023783
333.645600	14060.548920	29.028800
333.926201	14085.480214	29.033818
334.072893	14108.577291	29.038836
334.369193	14137.466240	29.043853
334.565253	14154.962445	29.048871
335.261592	14188.730502	29.053888
334.885843	14227.861977	29.058906
335.261207	14254.631116	29.063924
336.162056	14283.083211	29.068941
336.185115	14316.519937	29.073959
336.718087	14338.880619	29.078976
337.019310	14387.107020	29.083994
337.754573	14395.399403	29.089012
338.190341	14427.602009	29.094029
338.622069	14458.913384	29.099047
339.347756	14465.781190	29.104064
339.658197	14487.291603	29.109082
340.407263	14487.443758	29.114100
340.414571	14502.015113	29.119117
340.503377	14531.188034	29.124135
341.043874	14536.748513	29.129152
341.284736	14561.956585	29.134170
341.620036	14580.249721	29.139188
341.757945	14600.082067	29.144205
341.688989	14611.890922	29.149223
342.215648	14626.943921	29.154240
342.247852	14653.541899	29.159258
342.639747	14680.803849	29.164276
343.083002	14703.595901	29.169293
343.102933	14735.078272	29.174311
343.618908	14765.369297	29.179328
343.772680	14799.439433	29.184346
343.927104	14808.283431	29.189364
344.328242	14843.871399	29.194381
344.514714	14872.406298	29.199399
345.276083	14895.410824	29.204416
345.306876	14938.818580	29.209434
345.887664	14965.636902	29.214452
345.954576	14983.977981	29.219469
346.223249	15013.939973	29.224487
346.983784	15042.686070	29.229504
347.196125	15068.706530	29.234522
347.821046	15089.897873	29.239540
348.168102	15113.361992	29.244557
348.921847	15138.695830	29.249575
349.272284	15156.722350	29.254592
349.721277	15160.963313	29.259610
350.027509	15171.022721	29.264628
350.642778	15193.140892	29.269645
350.664373	15220.190698	29.274663
350.779568	15233.949012	29.279680
351.124623	15274.167963	29.284698
351.359105	15289.611834	29.289716
351.738566	15302.579531	29.294733
351.739568	15330.532811	29.299751
352.555692	15371.726943	29.304768
352.429364	15393.595963	29.309786
352.792399	15419.973478	29.314804
353.145569	15453.006548	29.319821
353.165018	15492.239664	29.324839
353.247047	15523.401245	29.329856
353.878907	15559.630342	29.334874
354.255224	15596.186994	29.339892
354.699656	15634.150894	29.344909
355.161785	15661.248430	29.349927
355.929189	15702.772954	29.354944
356.007026	15722.269861	29.359962
356.497108	15748.322744	29.364980
357.250658	15772.098905	29.369997
357.431400	15801.047717	29.375015
357.948640	15833.958313	29.380032
358.415575	15862.240570	29.385050
358.677243	15881.959465	29.390068
358.791260	15902.295368	29.395085
359.109032	15935.083091	29.400103
359.488141	15954.193229	29.405120
359.954509	15995.301716	29.410138
360.091891	16032.384240	29.415156
360.780356	16045.879894	29.420173
361.309584	16067.819609	29.425191
361.646721	16082.757116	29.430208
362.023668	16119.026412	29.435226
362.312859	16140.110672	29.440244
362.657766	16162.892640	29.445261
362.776423	16189.757796	29.450279
363.324999	16210.937992	29.455296
363.307225	16250.119178	29.460314
363.637673	16271.688529	29.465332
364.425954	16297.273787	29.470349
364.564079	16337.862089	29.475367
364.985614	16360.009117	29.480384
365.368590	16381.733849	29.485402
365.946843	16418.244791	29.490420
366.157171	16435.871898	29.495437
366.624898	16477.504635	29.500455
366.915943	16486.702085	29.505472
367.038783	16515.368567	29.510490
367.442453	16545.456062	29.515508
368.010152	16572.293370	29.520525
368.254780	16601.428477	29.525543
368.666468	16620.808254	29.530560
368.913219	16642.901005	29.535578
369.338765	16659.625934	29.540596
369.681621	16689.206773	29.545613
370.321795	16693.482754	29.550631
371.233079	16695.898257	29.555648
372.006297	16715.016679	29.560666
372.287487	16731.187092	29.565684
372.682043	16739.380930	29.570701
372.865143	16756.331993	29.575719
372.740502	16771.636420	29.580736
372.883666	16789.610718	29.585754
373.197300	16811.966894	29.590772
373.602231	16820.072372	29.595789
373.466456	16859.741039	29.600807
373.642292	16888.180333	29.605824
374.029864	16921.951467	29.610842
374.333747	16957.011597	29.615860
375.035616	16978.998093	29.620877
375.436129	17007.999415	29.625895
375.919165	17040.990588	29.630912
375.984080	17083.432197	29.635930
376.220352	17126.841741	29.640948
377.221236	17148.252629	29.645965
376.835649	17191.467178	29.650983
377.278772	17220.028387	29.656000
377.552677	17258.255913	29.661018
377.848122	17313.129160	29.666036
378.606209	17342.146081	29.671053
378.714623	17373.385619	29.676071
379.333715	17409.179581	29.681088
379.836151	17442.461526	29.686106
379.854040	17487.418089	29.691124
380.793792	17509.780538	29.696141
380.882543	17551.358806	29.701159
381.690855	17581.650883	29.706176
382.242367	17613.634153	29.711194
382.695517	17643.773804	29.716212
382.982289	17671.452150	29.721229
383.382678	17704.340089	29.726247
383.454661	17733.846183	29.731264
383.779343	17763.100946	29.736282
384.225117	17798.520872	29.741300
384.517943	17817.031128	29.746317
385.309674	17861.469968	29.751335
385.810845	17896.059735	29.756352
386.568193	17927.369659	29.761370
386.420878	17950.057300	29.766388
386.648813	17975.182907	29.771405
387.062688	18002.326955	29.776423
387.652888	18031.703839	29.781440
388.215265	18057.146317	29.786458
388.676859	18084.884746	29.791476
389.356717	18101.718877	29.796493
389.619005	18130.306809	29.801511
390.246220	18145.882369	29.806528
390.693699	18159.607156	29.811546
390.871250	18185.318317	29.816564
391.312641	18208.110823	29.821581
391.354486	18233.204512	29.826599
391.841720	18252.253750	29.831616
391.988675	18288.756548	29.836634
392.293134	18311.992683	29.841652
392.474644	18345.425617	29.846669
392.693138	18369.397969	29.851687
393.052139	18408.410121	29.856704
393.641820	18455.993950	29.861722
393.959001	18479.259744	29.866740
394.434251	18512.332385	29.871757
394.643799	18533.752855	29.876775
395.299416	18557.047971	29.881792
396.349828	18558.785043	29.886810
396.708760	18582.283683	29.891828
396.835190	18595.500704	29.896845
397.171753	18627.371698	29.901863
397.567740	18656.777048	29.906880
398.278597	18672.159591	29.911898
398.288677	18693.225445	29.916916
398.295089	18724.315719	29.921933
398.627419	18757.341525	29.926951
398.789497	18785.775323	29.931968
399.434210	18827.690562	29.936986
399.374933	18860.212210	29.942004
399.840888	18903.724040	29.947021
400.134398	18948.040029	29.952039
400.000349	18989.371818	29.957056
400.480770	19033.939324	29.962074
400.791430	19079.069375	29.967092
401.344583	19125.895056	29.972109
401.802844	19174.694381	29.977127
402.361413	19225.922217	29.982144
403.032798	19269.717920	29.987162
403.430272	19309.655891	29.992180
404.142628	19353.591649	29.997197
404.882545	19387.837701	30.002215
405.116385	19433.090173	30.007232
405.600270	19443.400298	30.012250
406.164272	19493.595531	30.017268
407.334560	19513.524935	30.022285
407.456854	19542.113203	30.027303
407.522072	19565.141544	30.032320
408.331632	19590.558159	30.037338
408.279478	19620.578372	30.042356
408.695662	19660.900315	30.047373
409.479529	19678.994186	30.052391
409.389535	19705.412411	30.057408
410.355985	19731.772816	30.062426
410.699862	19767.921593	30.067444
410.809334	19801.107671	30.072461
411.396629	19832.627428	30.077479
411.501891	19859.431394	30.082496
412.074753	19888.257957	30.087514
412.200646	19912.995060	30.092532
412.407221	19953.473721	30.097549
412.834647	19987.468379	30.102567
412.855674	20031.991485	30.107584
413.442591	20076.219445	30.112602
413.772839	20118.831499	30.117620
414.192857	20165.332127	30.122637
414.448284	20218.418131	30.127655
415.319642	20247.246454	30.132672
415.655240	20275.058230	30.137690
416.351360	20318.635056	30.142708
416.748217	20353.816283	30.147725
417.250986	20384.223871	30.152743
417.606774	20417.345261	30.157760
418.029397	20443.482913	30.162778
418.498341	20485.423483	30.167796
419.179165	20516.460869	30.172813
419.392824	20554.675985	30.177831
419.597430	20578.691651	30.182848
420.265697	20611.850092	30.187866
420.726024	20657.924508	30.192884
421.045586	20686.920416	30.197901
421.707984	20713.826052	30.202919
421.837782	20750.526261	30.207936
422.517058	20767.339555	30.212954
423.015732	20793.291777	30.217972
423.282094	20811.008875	30.222989
423.857945	20837.604245	30.228007
423.823801	20875.429063	30.233024
424.476014	20898.162059	30.238042
424.506506	20936.644783	30.243060
424.765378	20968.427463	30.248077
425.238850	21004.816060	30.253095
425.615066	21045.460103	30.258112
426.161483	21085.398217	30.263130
426.406984	21131.540955	30.268148
426.742842	21173.513117	30.273165
427.268657	21201.277670	30.278183
427.060107	21252.083502	30.283200
427.931202	21286.201429	30.288218
428.993179	21328.490739	30.293236
429.402108	21362.341476	30.298253
430.134985	21404.083093	30.303271
429.915752	21439.961165	30.308288
430.459318	21473.711057	30.313306
430.616153	21502.643816	30.318324
431.157256	21554.967947	30.323341
431.624620	21597.130708	30.328359
431.882010	21638.994022	30.333376
432.422319	21688.219123	30.338394
432.770521	21741.822788	30.343412
433.088599	21799.907580	30.348429
433.788955	21823.940888	30.353447
434.174881	21880.220571	30.358464
434.668852	21920.215058	30.363482
435.094636	21961.736036	30.368500
435.313728	21997.978037	30.373517
436.283738	22034.181211	30.378535
436.489500	22078.975639	30.383552
437.251028	22111.180396	30.388570
438.417138	22147.357729	30.393588
438.922276	22172.527431	30.398605
439.642702	22202.088820	30.403623
439.817810	22214.200168	30.408640
440.238262	22243.079619	30.413658
440.444350	22273.987414	30.418676
440.454676	22314.633478	30.423693
441.077566	22338.659824	30.428711
441.662681	22377.166170	30.433728
442.075470	22412.399538	30.438746
442.327480	22444.890914	30.443764
442.495967	22488.577886	30.448781
443.161188	22522.032295	30.453799
443.526611	22558.834700	30.458816
443.974138	22592.020910	30.463834
444.421551	22626.337686	30.468852
444.675931	22669.444908	30.473869
444.910603	22708.907035	30.478887
445.550118	22755.797985	30.483904
446.547908	22768.354059	30.488922
447.247525	22810.350630	30.493940
447.340827	22854.678495	30.498957
447.849244	22864.072200	30.503975
448.000557	22914.484604	30.508992
448.359178	22942.623378	30.514010
448.955313	22982.184106	30.519028
449.312907	23029.593824	30.524045
449.972360	23057.151740	30.529063
450.091316	23089.578039	30.534080
450.373722	23125.979138	30.539098
451.078893	23175.542425	30.544116
451.566045	23212.067561	30.549133
451.728647	23245.382535	30.554151
452.207885	23288.157766	30.559168
452.718281	23311.491396	30.564186
453.069344	23336.098585	30.569204
453.377243	23375.528098	30.574221
454.409634	23403.065972	30.579239
455.213275	23424.410333	30.584256
455.924873	23455.651476	30.589274
456.460510	23480.810212	30.594292
456.819878	23512.953212	30.599309
457.014506	23525.355555	30.604327
457.205128	23554.519614	30.609344
457.822989	23580.680356	30.614362
458.532518	23624.011263	30.619380
458.727086	23652.146782	30.624397
459.052466	23674.678936	30.629415
459.755282	23700.264496	30.634432
460.076157	23727.553042	30.639450
460.278806	23764.191016	30.644468
460.383337	23806.200062	30.649485
460.984574	23831.876710	30.654503
461.122564	23885.583399	30.659520
461.652605	23923.714478	30.664538
461.889563	23968.690093	30.669556
462.270743	24019.663849	30.674573
462.910207	24063.228207	30.679591
463.031957	24112.182618	30.684608
463.553528	24162.359393	30.689626
464.514494	24206.143802	30.694644
464.845055	24249.887388	30.699661
465.903556	24296.382265	30.704679
466.098646	24338.421819	30.709696
466.340037	24369.351262	30.714714
466.937322	24413.338196	30.719732
467.293415	24459.257309	30.724749
467.614496	24498.543761	30.729767
467.676915	24568.464144	30.734784
468.250691	24617.919321	30.739802
469.118057	24653.720900	30.744820
469.153624	24718.688653	30.749837
469.601132	24756.802121	30.754855
470.178751	24810.817563	30.759872
470.852491	24867.288286	30.764890
471.692165	24920.335155	30.769908
472.051483	24973.034194	30.774925
472.618080	25008.816819	30.779943
472.778104	25053.573050	30.784960
473.603351	25092.429097	30.789978
474.046256	25143.441753	30.794996
474.416313	25185.143842	30.800013
474.719491	25230.834082	30.805031
475.172296	25278.502428	30.810048
475.612844	25328.943603	30.815066
476.104586	25374.271923	30.820084
476.066913	25434.195682	30.825101
476.527407	25487.294332	30.830119
477.331856	25546.202598	30.835136
477.591231	25607.522386	30.840154
478.240855	25656.376688	30.845172
478.897404	25698.732879	30.850189
479.586179	25741.418170	30.855207
480.272012	25795.269042	30.860224
480.597389	25846.123434	30.865242
481.463595	25870.221839	30.870260
481.803224	25929.807460	30.875277
482.553782	25955.666085	30.880295
483.046266	25999.264405	30.885312
483.585632	26030.084559	30.890330
484.250390	26064.823405	30.895348
484.410965	26098.712016	30.900365
484.789697	26137.204215	30.905383
485.107876	26175.041003	30.910400
485.300049	26209.889745	30.915418
485.829527	26238.945654	30.920436
485.825434	26284.377212	30.925453
486.377797	26336.056619	30.930471
487.310861	26375.407158	30.935488
487.389680	26431.031948	30.940506
488.388956	26473.011731	30.945524
488.587986	26528.758914	30.950541
488.904179	26562.114927	30.955559
489.597735	26601.294223	30.960576
490.173827	26665.558722	30.965594
490.641098	26712.285592	30.970612
491.225060	26766.866023	30.975629
491.687246	26810.767900	30.980647
491.888245	26853.643775	30.985664
492.064281	26910.881598	30.990682
492.781605	26950.619206	30.995700
493.344038	27011.657392	31.000717
494.175318	27068.989376	31.005735
494.402467	27110.394876	31.010752
494.892809	27157.138069	31.015770
495.877191	27217.287195	31.020788
496.027999	27263.440147	31.025805
496.341242	27303.204311	31.030823
497.151642	27354.371025	31.035840
497.383679	27419.660369	31.040858
497.904372	27467.355129	31.045876
498.775904	27526.621859	31.050893
498.941030	27578.697009	31.055911
499.731995	27621.344867	31.060928
499.878795	27671.820947	31.065946
500.821857	27709.233003	31.070964
501.067347	27776.972370	31.075981
501.841684	27834.136513	31.080999
502.261464	27871.632201	31.086016
502.374432	27924.212238	31.091034
502.917009	27977.402813	31.096052
503.718002	28036.809123	31.101069
504.247977	28082.125661	31.106087
505.228947	28129.178437	31.111104
505.300461	28170.672121	31.116122
506.097721	28212.449791	31.121140
507.052316	28259.100362	31.126157
507.477570	28303.166706	31.131175
508.150480	28333.530472	31.136192
508.416475	28385.225478	31.141210
509.066000	28421.337472	31.146228
509.297448	28460.095774	31.151245
509.883618	28509.044374	31.156263
510.513776	28548.172330	31.161280
510.684867	28591.073233	31.166298
511.056134	28624.853148	31.171316
511.408661	28682.720665	31.176333
511.784562	28732.468011	31.181351
512.543569	28780.218514	31.186368
512.821471	28842.934738	31.191386
513.159486	28887.360820	31.196404
513.926835	28942.274302	31.201421
513.921368	28993.785680	31.206439
514.468061	29042.398462	31.211456
515.006721	29108.132483	31.216474
515.931940	29147.496967	31.221492
516.356978	29207.732800	31.226509
516.601305	29261.632736	31.231527
517.628086	29304.201633	31.236544
518.040221	29342.490418	31.241562
518.710558	29382.888082	31.246580
519.038157	29444.550940	31.251597
519.383051	29499.646376	31.256615
519.889258	29538.276527	31.261632
519.921370	29589.997978	31.266650
520.902172	29641.446162	31.271668
521.333395	29701.430310	31.276685
521.500738	29767.269166	31.281703
522.233548	29804.979171	31.286720
522.527990	29880.816740	31.291738
522.949708	29928.872180	31.296756
523.494639	29987.705993	31.301773
524.086350	30033.131000	31.306791
524.940119	30091.759571	31.311808
525.056594	30156.936340	31.316826
525.780958	30218.325032	31.321844
526.512722	30278.242595	31.326861
526.539468	30335.226141	31.331879
527.516830	30395.620925	31.336896
528.151597	30465.549532	31.341914
528.593247	30513.120603	31.346932
529.476371	30569.133747	31.351949
529.564192	30633.354804	31.356967
530.426138	30680.437317	31.361984
531.000470	30743.136656	31.367002
531.298661	30782.191970	31.372020
532.041281	30856.991207	31.377037
532.566557	30907.022959	31.382055
533.281726	30952.224900	31.387072
533.498367	31023.852725	31.392090
534.330121	31061.637444	31.397108
535.907198	31098.989958	31.402125
536.252154	31139.363410	31.407143
537.238432	31182.189677	31.412160
537.377023	31226.329700	31.417178
537.686514	31259.298334	31.422196
538.518214	31300.869516	31.427213
538.903415	31345.890354	31.432231
539.407327	31388.415048	31.437248
539.746671	31433.153427	31.442266
540.155383	31482.467812	31.447284
540.814830	31528.652181	31.452301
541.064178	31592.730182	31.457319
541.230929	31636.835036	31.462336
541.607411	31700.504364	31.467354
542.234824	31762.028068	31.472372
542.914538	31811.683530	31.477389
543.017021	31874.139880	31.482407
544.476314	31913.668497	31.487424
544.774980	31986.211134	31.492442
545.370078	32030.779433	31.497460
546.287832	32091.783073	31.502477
546.420103	32145.991206	31.507495
546.774846	32196.319831	31.512512
547.512791	32253.570750	31.517530
547.886693	32307.124219	31.522548
548.358854	32358.206920	31.527565
548.534614	32427.310481	31.532583
549.169887	32474.574082	31.537600
549.647681	32544.429626	31.542618
549.953730	32601.652046	31.547636
550.621412	32666.396861	31.552653
551.212797	32737.701576	31.557671
551.743725	32794.597199	31.562688
551.924325	32865.156230	31.567706
552.505403	32919.355713	31.572724
553.135833	32991.383864	31.577741
553.874445	33057.251133	31.582759
554.479415	33109.270118	31.587776
554.771183	33175.372551	31.592794
555.546631	33217.850506	31.597812
556.155618	33288.700174	31.602829
556.356779	33349.990602	31.607847
556.908701	33410.869910	31.612864
557.521446	33481.460992	31.617882
558.034213	33555.050680	31.622900
558.753358	33613.246254	31.627917
559.382715	33679.118107	31.632935
560.268387	33740.000219	31.637952
560.358564	33802.285557	31.642970
561.006059	33864.955529	31.647988
561.625204	33927.472634	31.653005
562.073267	34003.157447	31.658023
562.607719	34061.637433	31.663040
563.256248	34130.738974	31.668058
564.377645	34204.297094	31.673076
565.116861	34253.204903	31.678093
565.136456	34329.987407	31.683111
565.864603	34385.612302	31.688128
566.664072	34457.246141	31.693146
567.320547	34515.451870	31.698164
567.839401	34573.642654	31.703181
568.037885	34642.687984	31.708199
569.070321	34691.889371	31.713216
569.895262	34754.015660	31.718234
569.970944	34810.491207	31.723252
570.713489	34878.027578	31.728269
570.896871	34942.497802	31.733287
571.611874	35001.471732	31.738304
572.487960	35065.648120	31.743322
573.015603	35135.139579	31.748340
574.534811	35169.578721	31.753357
574.811628	35226.779719	31.758375
575.488689	35287.701590	31.763392
576.121117	35336.090396	31.768410
576.564584	35377.927795	31.773428
577.246751	35418.668713	31.778445
577.855764	35488.015568	31.783463
578.655723	35524.189911	31.788480
579.311366	35585.012195	31.793498
579.419773	35638.701614	31.798516
579.885351	35682.981763	31.803533
580.312074	35730.881763	31.808551
580.882244	35787.720530	31.813568
581.701734	35847.661438	31.818586
582.134866	35895.920578	31.823604
582.388820	35957.444783	31.828621
582.519223	36034.980010	31.833639
583.420112	36101.273563	31.838656
583.909232	36161.961209	31.843674
584.030479	36230.056589	31.848692
585.029754	36295.327900	31.853709
585.065654	36372.012335	31.858727
585.727506	36438.160418	31.863744
586.200179	36518.509884	31.868762
586.392099	36600.417753	31.873780
587.121789	36650.504543	31.878797
588.160021	36750.044212	31.883815
588.632929	36816.316415	31.888832
588.813918	36892.594081	31.893850
589.545512	36966.322639	31.898868
590.948235	37031.211240	31.903885
591.762517	37090.181965	31.908903
592.513300	37155.459574	31.913920
592.806489	37215.217404	31.918938
593.364853	37278.996579	31.923956
594.035703	37322.464178	31.928973
594.481703	37388.010733	31.933991
595.123537	37457.403960	31.939008
596.012639	37508.609300	31.944026
595.865485	37572.954199	31.949044
596.720625	37626.434693	31.954061
596.899621	37699.361194	31.959079
597.742076	37766.001926	31.964096
598.128736	37838.588549	31.969114
598.293639	37906.998665	31.974132
598.945222	37981.448404	31.979149
599.210488	38069.798814	31.984167
600.154922	38142.932078	31.989184
600.640636	38222.598938	31.994202
601.048945	38313.663319	31.999220
601.769031	38399.011269	32.004237
602.359236	38466.980823	32.009255
603.085785	38547.016485	32.014272
604.244084	38621.959604	32.019290
604.989704	38702.819741	32.024308
605.741704	38769.867331	32.029325
606.471159	38849.039028	32.034343
607.156506	38921.097744	32.039360
608.279350	38969.948740	32.044378
608.838756	39039.901377	32.049396
609.434148	39086.797663	32.054413
609.935468	39154.367838	32.059431
610.578069	39215.829486	32.064448
611.009690	39290.462965	32.069466
611.577333	39348.749515	32.074484
612.294553	39411.682996	32.079501
612.887411	39483.203693	32.084519
613.366317	39549.772147	32.089536
613.791232	39629.306867	32.094554
614.598701	39702.939348	32.099572
615.190780	39756.646339	32.104589
616.120035	39822.418585	32.109607
616.491169	39891.452339	32.114624
617.144100	39952.797979	32.119642
617.769419	40033.305123	32.124660
618.983694	40099.631029	32.129677
619.225784	40164.059694	32.134695
619.577558	40228.735618	32.139712
620.527047	40288.808678	32.144730
621.072961	40352.439729	32.149748
621.518019	40415.866699	32.154765
621.828131	40493.359754	32.159783
622.210199	40565.815973	32.164800
622.745114	40635.100108	32.169818
623.185834	40718.046079	32.174836
623.696593	40801.094497	32.179853
624.398015	40887.252657	32.184871
625.088189	40974.164363	32.189888
625.498333	41036.999486	32.194906
626.390240	41132.139615	32.199924
626.915425	41206.446639	32.204941
627.460035	41297.967439	32.209959
628.058718	41375.129298	32.214976
628.946896	41462.206330	32.219994
629.315388	41543.441225	32.225012
630.595480	41620.242191	32.230029
631.094309	41697.604988	32.235047
631.312127	41763.539590	32.240064
632.140094	41841.877747	32.245082
633.392129	41915.540408	32.250100
634.370225	41981.918454	32.255117
634.864504	42047.025519	32.260135
635.614425	42110.897304	32.265152
635.892174	42166.708910	32.270170
636.276901	42229.122970	32.275188
637.111167	42281.664046	32.280205
637.821962	42337.900281	32.285223
638.480555	42417.165414	32.290240
639.109084	42479.366426	32.295258
639.678654	42549.112959	32.300276
640.148015	42612.224644	32.305293
640.692989	42676.271140	32.310311
641.508702	42738.906182	32.315328
642.279047	42810.382124	32.320346
642.998195	42878.760329	32.325364
643.168413	42955.181907	32.330381
643.803865	43023.536586	32.335399
644.416733	43105.985014	32.340416
645.036540	43176.486457	32.345434
645.495758	43254.831527	32.350452
646.180334	43323.535946	32.355469
646.771320	43407.842522	32.360487
647.448897	43492.431946	32.365504
648.121662	43572.975150	32.370522
648.505698	43665.560258	32.375540
649.353680	43730.968430	32.380557
650.438067	43801.483921	32.385575
651.204955	43866.602879	32.390592
651.986820	43952.171675	32.395610
652.896206	44032.570450	32.400628
653.776029	44107.765095	32.405645
654.191313	44181.625495	32.410663
654.594486	44251.630073	32.415680
655.117224	44327.560222	32.420698
655.818909	44403.319051	32.425716
656.262142	44479.575517	32.430733
656.492836	44552.583841	32.435751
657.086842	44649.152043	32.440768
657.965108	44732.495251	32.445786
658.591614	44828.879050	32.450804
659.188250	44904.060530	32.455821
660.123937	45000.435197	32.460839
660.404125	45088.570573	32.465856
661.373921	45161.396064	32.470874
662.035898	45241.923006	32.475892
663.103253	45316.810547	32.480909
665.123548	45361.681455	32.485927
666.078663	45434.905113	32.490944
666.725538	45489.933215	32.495962
667.179926	45550.935555	32.500980
667.380173	45610.508696	32.505997
668.110207	45671.361708	32.511015
668.531528	45738.214563	32.516032
669.108797	45799.980469	32.521050
669.467722	45872.382316	32.526068
670.041201	45947.884404	32.531085
670.757688	46010.430016	32.536103
671.067553	46096.774922	32.541120
671.483957	46174.924608	32.546138
672.290109	46263.161777	32.551156
672.841135	46347.295610	32.556173
673.605028	46418.723301	32.561191
674.063409	46504.865570	32.566208
674.350518	46583.837176	32.571226
675.006908	46679.628763	32.576244
676.025106	46776.564144	32.581261
676.441394	46869.453430	32.586279
677.013969	46960.429076	32.591296
677.751096	47034.572802	32.596314
678.107914	47124.741771	32.601332
678.613098	47211.416344	32.606349
679.442920	47283.341657	32.611367
680.085729	47375.457114	32.616384
681.053519	47452.788439	32.621402
681.764801	47543.911348	32.626420
682.159705	47638.866809	32.631437
682.771177	47722.873636	32.636455
683.641526	47816.200989	32.641472
684.762781	47891.623551	32.646490
685.835819	47981.788845	32.651508
686.299126	48068.357417	32.656525
687.375761	48145.420970	32.661543
687.689737	48227.031816	32.666560
688.417905	48306.041980	32.671578
689.090048	48394.519655	32.676596
689.648431	48497.006127	32.681613
690.385493	48567.028458	32.686631
690.984467	48655.481536	32.691648
691.443644	48741.302263	32.696666
691.911543	48828.931458	32.701684
692.363735	48934.289476	32.706701
693.316111	49028.540849	32.711719
693.682370	49131.473004	32.716736
694.636846	49220.318434	32.721754
695.333890	49321.608491	32.726772
695.815987	49418.428008	32.731789
697.058801	49508.600926	32.736807
697.519306	49623.921999	32.741824
698.488933	49713.499904	32.746842
699.132801	49806.694409	32.751860
700.006031	49902.033775	32.756877
700.699652	49993.048160	32.761895
701.187188	50086.926746	32.766912
702.524352	50168.452716	32.771930
702.858372	50256.344272	32.776948
703.744611	50356.297904	32.781965
704.743188	50450.975023	32.786983
705.359616	50545.993647	32.792000
706.286140	50646.299020	32.797018
707.062277	50730.756168	32.802036
708.137142	50805.288333	32.807053
708.936304	50878.685108	32.812071
709.520728	50959.413367	32.817088
710.143925	51026.627332	32.822106
711.060363	51118.286140	32.827124
711.661060	51201.220417	32.832141
712.965797	51263.771449	32.837159
713.850637	51341.321744	32.842176
714.376683	51401.531957	32.847194
715.196053	51471.371295	32.852212
715.488339	51551.900767	32.857229
716.275820	51623.555702	32.862247
716.963551	51710.182644	32.867264
717.305265	51794.621447	32.872282
718.280009	51871.363093	32.877300
718.374915	51959.121874	32.882317
719.126962	52029.988228	32.887335
719.809850	52135.641562	32.892352
720.163305	52212.209212	32.897370
721.359311	52298.164205	32.902388
721.644909	52402.273743	32.907405
722.477284	52488.428608	32.912423
722.962390	52586.422764	32.917440
723.955617	52661.427264	32.922458
724.994233	52753.980178	32.927476
725.002698	52836.703408	32.932493
725.905536	52917.617843	32.937511
726.592211	53014.064717	32.942528
727.189724	53100.002073	32.947546
727.301380	53204.113045	32.952564
728.046625	53287.430383	32.957581
728.833698	53374.348433	32.962599
729.372871	53473.089904	32.967616
730.952399	53550.281626	32.972634
732.279786	53646.531066	32.977652
732.462416	53735.180468	32.982669
733.679802	53804.232806	32.987687
734.599914	53882.709815	32.992704
735.730628	53955.232736	32.997722
736.541640	54036.470234	33.002740
736.874651	54108.272571	33.007757
737.445438	54186.972750	33.012775
738.162852	54273.691511	33.017792
738.945341	54360.121929	33.022810
739.464334	54450.014168	33.027828
739.747868	54532.534897	33.032845
740.738058	54639.800025	33.037863
741.243192	54732.159811	33.042880
741.646388	54815.287440	33.047898
742.817549	54917.880539	33.052916
743.030244	55020.145970	33.057933
744.018707	55125.265926	33.062951
744.449078	55219.662115	33.067968
744.879407	55331.389245	33.072986
745.956658	55433.400329	33.078004
746.883069	55535.695895	33.083021
747.448659	55645.829256	33.088039
748.174401	55756.770788	33.093056
748.858713	55873.741080	33.098074
749.782044	55973.537402	33.103092
750.041743	56090.446413	33.108109
750.813251	56195.209854	33.113127
751.717652	56305.802734	33.118144
752.401481	56415.857681	33.123162
753.677793	56526.952723	33.128180
753.941242	56643.308358	33.133197
754.980691	56758.411831	33.138215
755.776221	56873.657351	33.143232
756.584726	56976.763356	33.148250
757.781946	57084.171886	33.153268
758.306784	57198.086529	33.158285
759.058311	57299.617634	33.163303
759.834892	57412.752648	33.168320
760.371625	57531.355744	33.173338
761.600314	57620.386975	33.178356
762.111604	57725.593242	33.183373
763.557421	57825.868674	33.188391
764.575685	57914.019733	33.193408
765.071744	58006.668029	33.198426
766.200623	58109.651180	33.203444
766.585001	58209.408739	33.208461
767.116833	58310.696926	33.213479
768.000781	58414.379276	33.218496
768.577031	58519.041883	33.223514
769.320395	58634.938126	33.228532
769.903548	58735.543844	33.233549
770.807184	58840.438432	33.238567
771.148336	58945.597074	33.243584
771.987366	59058.219249	33.248602
773.502608	59148.574946	33.253620
774.450603	59243.050129	33.258637
775.670844	59331.142493	33.263655
777.022008	59427.770063	33.268672
777.381034	59522.817776	33.273690
778.245217	59587.948471	33.278708
778.755624	59672.039282	33.283725
779.209587	59750.679733	33.288743
779.948801	59835.694006	33.293760
780.125404	59923.190327	33.298778
781.406150	60018.808606	33.303796
781.864443	60111.365437	33.308813
782.192518	60196.727189	33.313831
783.131345	60291.903976	33.318848
783.819565	60402.725892	33.323866
784.709163	60495.921071	33.328884
785.400231	60605.157380	33.333901
785.958125	60708.475676	33.338919
786.611742	60818.502975	33.343936
787.008114	60939.348697	33.348954
787.847937	61045.150098	33.353972
788.178196	61172.795688	33.358989
788.756789	61287.141791	33.364007
789.990864	61414.089816	33.369024
790.680580	61524.614268	33.374042
791.464408	61651.808771	33.379060
792.426759	61797.618935	33.384077
792.931042	61910.413429	33.389095
793.637247	62043.627349	33.394112
794.388554	62166.874001	33.399130
795.201388	62292.525583	33.404148
796.024640	62430.222738	33.409165
796.901764	62565.295298	33.414183
798.279780	62687.727411	33.419200
798.582274	62817.024878	33.424218
799.559403	62929.323458	33.429236
800.377679	63076.196794	33.434253
801.363326	63189.999682	33.439271
802.945672	63313.128667	33.444288
803.816016	63432.792169	33.449306
804.847709	63542.266106	33.454324
805.847897	63640.318020	33.459341
806.606765	63760.039765	33.464359
807.779747	63867.355701	33.469376
808.416965	63973.755662	33.474394
809.593660	64079.624633	33.479412
810.186605	64179.396105	33.484429
811.192212	64268.809519	33.489447
811.868739	64376.601988	33.494464
812.185190	64491.679324	33.499482
812.937465	64600.813141	33.504500
814.101567	64717.180308	33.509517
814.493459	64833.745176	33.514535
815.413421	64938.143902	33.519552
816.038768	65059.222675	33.524570
816.922300	65165.897851	33.529588
817.679824	65287.265870	33.534605
818.594052	65396.383468	33.539623
819.333834	65517.458669	33.544640
819.752901	65634.933823	33.549658
821.164076	65755.419131	33.554676
821.669055	65875.315174	33.559693
822.227555	65992.965293	33.564711
823.295044	66107.251202	33.569728
824.123078	66233.467983	33.574746
824.843950	66337.976173	33.579764
825.450649	66466.582519	33.584781
826.667894	66585.265092	33.589799
827.781075	66696.101426	33.594816
828.214566	66826.306354	33.599834
829.395398	66934.300680	33.604852
830.471888	67045.100676	33.609869
831.773439	67140.388433	33.614887
832.986957	67218.729819	33.619904
833.981605	67307.544941	33.624922
834.858565	67404.187339	33.629940
835.797225	67484.604418	33.634957
836.140672	67576.461553	33.639975
836.935849	67675.318725	33.644992
837.046203	67763.194428	33.650010
837.995855	67858.486668	33.655028
838.506143	67963.872264	33.660045
839.575346	68079.414124	33.665063
840.447378	68172.855607	33.670080
840.949501	68281.828759	33.675098
841.599498	68394.520762	33.680116
842.614132	68505.604227	33.685133
843.348650	68613.086623	33.690151
844.067086	68724.789152	33.695168
844.680077	68841.586464	33.700186
845.753143	68960.299981	33.705204
846.645920	69086.346238	33.710221
847.514142	69219.535269	33.715239
848.744556	69333.249188	33.720256
848.849248	69446.997861	33.725274
849.589227	69563.689683	33.730292
850.814783	69692.788946	33.735309
851.582520	69817.665252	33.740327
852.398342	69948.072948	33.745344
852.510822	70083.459690	33.750362
853.183238	70210.092769	33.755380
854.462326	70343.707869	33.760397
855.164358	70481.307588	33.765415
855.983653	70626.160053	33.770432
856.747167	70762.436294	33.775450
857.749315	70894.355477	33.780468
858.769916	71019.121210	33.785485
859.576817	71169.986187	33.790503
860.806713	71292.954856	33.795520
861.556875	71427.745323	33.800538
862.507422	71578.867681	33.805556
863.145250	71708.227968	33.810573
863.403064	71856.829928	33.815591
864.717266	71982.488632	33.820608
866.064933	72131.367810	33.825626
867.424909	72265.613906	33.830644
868.700177	72380.405325	33.835661
869.489652	72506.406672	33.840679
870.940926	72634.670755	33.845696
871.677773	72752.120360	33.850714
872.453238	72880.655582	33.855732
873.414835	72997.386480	33.860749
874.227210	73114.326031	33.865767
874.933970	73220.274327	33.870784
875.470266	73345.171493	33.875802
876.377449	73472.543919	33.880820
877.499455	73592.166744	33.885837
878.642800	73711.786707	33.890855
879.873852	73828.281568	33.895872
880.295974	73949.090640	33.900890
881.195592	74065.413846	33.905908
881.749213	74182.016140	33.910925
882.274240	74308.508005	33.915943
883.605389	74437.536196	33.920960
884.307107	74568.952031	33.925978
885.422899	74697.119320	33.930996
886.255978	74818.149946	33.936013
886.877923	74941.657195	33.941031
887.823042	75071.657228	33.946048
888.648005	75184.046179	33.951066
889.488211	75320.224724	33.956084
890.663335	75427.194212	33.961101
891.263803	75548.393780	33.966119
892.195659	75652.451117	33.971136
892.795682	75771.773688	33.976154
893.361454	75893.556407	33.981172
894.312608	76028.234819	33.986189
895.379539	76155.988680	33.991207
896.154186	76268.676108	33.996224
896.911001	76395.426383	34.001242
897.595172	76522.967300	34.006260
898.695265	76654.753631	34.011277
899.183844	76790.645190	34.016295
900.456498	76921.645675	34.021312
901.319344	77068.589540	34.026330
901.846285	77216.456331	34.031348
902.847681	77338.940414	34.036365
903.927788	77492.587093	34.041383
904.961442	77624.301641	34.046400
905.598895	77759.320726	34.051418
906.260422	77914.032448	34.056436
907.517940	78063.257977	34.061453
907.824076	78225.044930	34.066471
908.809302	78362.489668	34.071488
909.628833	78512.252259	34.076506
910.058439	78662.029639	34.081524
911.159861	78819.148158	34.086541
912.020495	78988.584798	34.091559
913.105006	79154.544814	34.096576
913.697749	79314.799594	34.101594
914.294219	79486.212848	34.106612
915.764911	79663.005158	34.111629
916.114493	79835.809166	34.116647
917.356007	79995.171015	34.121664
918.488989	80154.804939	34.126682
919.596794	80315.791507	34.131700
921.245163	80469.421814	34.136717
922.111629	80648.200371	34.141735
923.690773	80779.533521	34.146752
924.764166	80922.463840	34.151770
925.303256	81075.269313	34.156788
926.470577	81229.376433	34.161805
926.953746	81390.903978	34.166823
927.848818	81542.236831	34.171840
928.919596	81682.616712	34.176858
929.945141	81834.088124	34.181876
930.658299	81989.009224	34.186893
931.623503	82154.947810	34.191911
932.639296	82303.779654	34.196928
933.722545	82455.403840	34.201946
935.231419	82585.683631	34.206964
936.294325	82723.667284	34.211981
937.468217	82864.429678	34.216999
938.420752	82989.293420	34.222016
940.130878	83130.810329	34.227034
941.232155	83242.397128	34.232052
942.434504	83364.109080	34.237069
942.998659	83491.848640	34.242087
944.016731	83613.978264	34.247104
945.099621	83737.622537	34.252122
945.755321	83871.681980	34.257140
946.619250	83978.826009	34.262157
947.442192	84097.339968	34.267175
948.353332	84228.841317	34.272192
949.305750	84362.310541	34.277210
950.035781	84504.940448	34.282228
950.826728	84623.304233	34.287245
951.491037	84763.086879	34.292263
952.242524	84887.791700	34.297280
953.182160	85024.499902	34.302298
953.829121	85161.934220	34.307316
954.359999	85293.744853	34.312333
954.724691	85438.541407	34.317351
955.733782	85597.772058	34.322368
956.471328	85744.274214	34.327386
957.041341	85893.955873	34.332404
958.248147	86053.448059	34.337421
958.759394	86216.631066	34.342439
959.724873	86374.115274	34.347456
960.881626	86543.850294	34.352474
961.594301	86721.353948	34.357492
962.579155	86884.887376	34.362509
963.672042	87070.588186	34.367527
964.774975	87224.113434	34.372544
965.766632	87402.183642	34.377562
966.327253	87582.484081	34.382580
966.834907	87745.716330	34.387597
967.915900	87929.799715	34.392615
968.746095	88109.066243	34.397632
969.848700	88305.728561	34.402650
970.663734	88482.051681	34.407668
971.765668	88678.793159	34.412685
972.945124	88872.068419	34.417703
973.641711	89061.558576	34.422720
975.022629	89235.522146	34.427738
975.643987	89429.514254	34.432756
976.665133	89627.536256	34.437773
977.347550	89827.159916	34.442791
978.119627	90021.252212	34.447808
979.567346	90223.258835	34.452826
980.809865	90412.176035	34.457844
981.693229	90620.183559	34.462861
982.832332	90805.887133	34.467879
983.793227	90992.659449	34.472896
985.230075	91189.132273	34.477914
986.403722	91370.246319	34.482932
987.281793	91554.150842	34.487949
989.222612	91732.818352	34.492967
990.141723	91914.124088	34.497984
991.525471	92089.639573	34.503002
992.144206	92267.231925	34.508020
993.282919	92432.999644	34.513037
994.523018	92602.226348	34.518055
995.504703	92776.832232	34.523072
996.795423	92944.318836	34.528090
997.641659	93117.955888	34.533108
999.041693	93285.395159	34.538125
1000.432864	93437.944550	34.543143
1001.637663	93591.418085	34.548160
1003.074099	93724.733725	34.553178
1004.132415	93894.119725	34.558196
1005.092745	94027.528288	34.563213
1006.201449	94178.711200	34.568231
1006.907800	94329.651336	34.573248
1008.039780	94469.445647	34.578266
1008.738301	94623.616899	34.583284
1009.426820	94774.214606	34.588301
1010.607370	94931.397013	34.593319
1011.253753	95095.732430	34.598336
1012.534662	95252.033173	34.603354
1012.932537	95406.214676	34.608372
1014.149146	95575.257048	34.613389
1014.650803	95742.253842	34.618407
1015.553263	95912.369484	34.623424
1016.721530	96082.955133	34.628442
1017.574396	96250.732928	34.633460
1018.359318	96415.459396	34.638477
1019.025530	96585.036324	34.643495
1020.396684	96743.059709	34.648512
1021.884493	96898.412555	34.653530
1022.637129	97051.083520	34.658548
1023.831608	97205.739770	34.663565
1024.616290	97367.199931	34.668583
1025.778950	97542.227676	34.673600
1026.695364	97695.312344	34.678618
1027.368624	97863.561156	34.683636
1028.478115	98030.624944	34.688653
1029.985345	98192.066119	34.693671
1031.007977	98354.645521	34.698688
1031.939756	98520.532815	34.703706
1033.005518	98693.691824	34.708724
1033.756464	98865.669546	34.713741
1034.999182	99018.797075	34.718759
1036.066951	99179.342257	34.723776
1037.643752	99335.740142	34.728794
1038.324353	99514.406434	34.733812
1039.337434	99688.182409	34.738829
1040.769926	99861.814372	34.743847
1040.999437	100037.728974	34.748864
1042.217604	100200.762842	34.753882
1043.127339	100370.052982	34.758900
1043.493140	100551.196983	34.763917
1044.858734	100738.008084	34.768935
1045.799951	100927.049510	34.773952
1046.749460	101124.998841	34.778970
1047.686952	101313.138401	34.783988
1048.694769	101508.447324	34.789005
1049.853037	101698.591927	34.794023
1050.493159	101898.485047	34.799040
1051.970973	102092.663516	34.804058
1052.983988	102297.601259	34.809076
1053.892456	102503.032757	34.814093
1055.198925	102696.129747	34.819111
1056.124090	102884.935033	34.824128
1057.071359	103073.573432	34.829146
1058.551738	103281.746951	34.834164
1059.616021	103474.427546	34.839181
1061.137144	103669.598512	34.844199
1062.016271	103862.065624	34.849216
1063.352002	104050.020174	34.854234
1064.182877	104232.968603	34.859252
1065.406143	104427.175014	34.864269
1066.960068	104616.465338	34.869287
1067.853492	104817.441000	34.874304
1069.026258	104999.470890	34.879322
1070.815937	105172.319971	34.884340
1072.118369	105344.693406	34.889357
1073.438359	105515.469368	34.894375
1074.032072	105685.897756	34.899392
1074.732622	105862.008655	34.904410
1075.547737	106041.546598	34.909428
1076.718855	106225.687611	34.914445
1077.952907	106416.367225	34.919463
1078.808670	106600.664237	34.924480
1079.497949	106782.836975	34.929498
1080.510433	106965.654190	34.934516
1081.498901	107168.208950	34.939533
1082.696577	107348.389214	34.944551
1083.290901	107546.148474	34.949568
1084.704860	107748.194136	34.954586
1085.847049	107945.042667	34.959604
1086.821222	108139.197281	34.964621
1087.255899	108335.215571	34.969639
1088.346502	108538.967155	34.974656
1089.504778	108728.307983	34.979674
1090.600490	108937.964076	34.984692
1091.699569	109129.394738	34.989709
1092.950926	109323.208202	34.994727
1094.047235	109518.061963	34.999744
1094.913981	109694.842131	35.004762
1096.054857	109901.015035	35.009780
1097.129690	110078.941351	35.014797
1098.537477	110278.207811	35.019815
1099.551324	110481.277457	35.024832
1101.218692	110649.673004	35.029850
1102.706321	110845.143085	35.034868
1103.362564	111033.176960	35.039885
1104.697436	111218.845369	35.044903
1105.597634	111424.106899	35.049920
1106.896063	111599.333507	35.054938
1108.111542	111793.233919	35.059956
1108.885410	111982.052965	35.064973
1110.179846	112174.270945	35.069991
1110.666984	112380.329893	35.075008
1111.895330	112566.962454	35.080026
1112.980874	112778.347380	35.085044
1114.296759	112974.013061	35.090061
1115.203798	113174.852818	35.095079
1116.532765	113376.523819	35.100096
1118.180038	113572.772449	35.105114
1119.054643	113772.000378	35.110132
1120.019337	113977.663054	35.115149
1121.055822	114170.862334	35.120167
1122.522708	114379.320820	35.125184
1123.581520	114585.187824	35.130202
1124.781634	114782.392962	35.135220
1125.828020	114987.403515	35.140237
1128.073903	115156.694006	35.145255
1129.233795	115347.917401	35.150272
1130.540914	115536.254593	35.155290
1131.610817	115723.162590	35.160308
1132.520731	115909.882865	35.165325
1133.828898	116105.331136	35.170343
1134.560796	116301.395337	35.175360
1135.502288	116503.114901	35.180378
1136.374637	116696.472732	35.185396
1137.030823	116900.548091	35.190413
1138.916604	117090.561239	35.195431
1139.375388	117311.548255	35.200448
1140.662072	117507.592582	35.205466
1141.997662	117704.871851	35.210484
1142.937193	117922.781462	35.215501
1144.369571	118123.924712	35.220519
1145.579745	118329.388622	35.225536
1147.065936	118523.075666	35.230554
1148.263857	118713.643990	35.235572
1149.749218	118908.309403	35.240589
1151.039540	119110.838790	35.245607
1151.998381	119310.801481	35.250624
1152.957590	119507.331706	35.255642
1154.084675	119690.391733	35.260660
1155.112569	119893.299383	35.265677
1156.592385	120089.418188	35.270695
1157.927222	120304.087494	35.275712
1158.854050	120487.717812	35.280730
1159.683089	120690.182359	35.285748
1160.175217	120896.670085	35.290765
1161.423962	121096.787322	35.295783
1162.621215	121299.448753	35.300800
1163.978791	121519.179236	35.305818
1165.343490	121726.213064	35.310836
1166.433658	121930.417156	35.315853
1167.678233	122128.438609	35.320871
1168.875596	122315.786659	35.325888
1169.821456	122516.850638	35.330906
1171.337485	122692.147981	35.335924
1172.065035	122889.258791	35.340941
1173.607214	123079.786211	35.345959
1174.554576	123275.177885	35.350976
1175.316490	123479.953789	35.355994
1176.683043	123676.406766	35.361012
1177.598348	123874.076072	35.366029
1178.666040	124066.715784	35.371047
1179.523992	124273.242812	35.376064
1180.668740	124492.853119	35.381082
1181.964329	124696.320010	35.386100
1182.764382	124917.751887	35.391117
1184.185580	125124.888840	35.396135
1186.034384	125338.090526	35.401152
1187.297670	125538.235373	35.406170
1188.690552	125747.865278	35.411188
1189.503722	125964.790928	35.416205
1190.590448	126187.236723	35.421223
1191.807209	126410.004879	35.426240
1193.010202	126632.650205	35.431258
1193.821707	126849.252935	35.436276
1195.087822	127080.002448	35.441293
1196.242973	127302.799986	35.446311
1197.458954	127528.668948	35.451328
1198.643044	127759.830038	35.456346
1199.947913	127984.749790	35.461364
1201.043448	128225.954483	35.466381
1202.259486	128446.190026	35.471399
1203.603057	128686.026546	35.476416
1204.697767	128908.085224	35.481434
1206.108786	129130.891804	35.486452
1207.301485	129370.200838	35.491469
1208.756786	129596.413028	35.496487
1210.238519	129823.319637	35.501504
1211.621432	130050.155485	35.506522
1213.012026	130271.946920	35.511540
1213.690423	130493.211039	35.516557
1215.266368	130713.086366	35.521575
1216.693234	130943.381860	35.526592
1217.655920	131176.202077	35.531610
1219.108823	131392.578619	35.536628
1220.230432	131633.627940	35.541645
1221.314501	131841.702343	35.546663
1222.909881	132066.007832	35.551680
1223.816463	132299.403335	35.556698
1225.429978	132521.363960	35.561716
1226.656171	132749.297247	35.566733
1227.434230	132976.076518	35.571751
1228.606745	133198.380856	35.576768
1229.666944	133434.383357	35.581786
1231.274656	133653.931581	35.586804
1232.338527	133902.360101	35.591821
1233.472659	134130.850847	35.596839
1235.049989	134354.326032	35.601856
1236.091089	134571.235811	35.606874
1237.363516	134795.081300	35.611892
1238.237102	135045.185378	35.616909
1239.860222	135270.396117	35.621927
1241.025127	135495.569953	35.626944
1242.229364	135741.821581	35.631962
1243.966296	135952.046089	35.636980
1244.903436	136193.477006	35.641997
1246.256158	136421.263185	35.647015
1247.535006	136661.576212	35.652032
1249.151045	136876.022983	35.657050
1250.618832	137096.226101	35.662068
1251.325309	137309.558017	35.667085
1252.846068	137508.227672	35.672103
1253.596203	137719.336336	35.677120
1254.331076	137938.981408	35.682138
1255.450430	138171.610607	35.687156
1256.744271	138396.149073	35.692173
1257.637021	138621.820258	35.697191
1258.998406	138855.187673	35.702208
1260.210090	139093.919204	35.707226
1261.112683	139341.997089	35.712244
1262.140900	139587.063824	35.717261
1263.240608	139821.571539	35.722279
1264.550141	140065.264012	35.727296
1265.489734	140314.661576	35.732314
1267.074873	140570.218033	35.737332
1268.412506	140814.532544	35.742349
1269.833293	141076.497702	35.747367
1270.977676	141335.467376	35.752384
1272.558692	141581.966152	35.757402
1273.941244	141827.586512	35.762420
1275.802882	142073.015435	35.767437
1277.222500	142319.140388	35.772455
1278.611590	142568.556285	35.777472
1279.784156	142820.139994	35.782490
1281.106502	143061.011324	35.787508
1282.227177	143312.657893	35.792525
1283.467095	143543.642802	35.797543
1285.260459	143790.046207	35.802560
1286.887006	144039.813896	35.807578
1288.483714	144272.342499	35.812596
1289.644060	144524.282910	35.817613
1290.910792	144753.153683	35.822631
1292.284005	144996.591503	35.827648
1293.814282	145210.039710	35.832666
1295.722437	145449.372463	35.837684
1296.591709	145676.032212	35.842701
1297.981418	145905.625662	35.847719
1299.439436	146140.421375	35.852736
1300.202293	146389.435179	35.857754
1301.870931	146624.529034	35.862772
1302.514087	146862.190520	35.867789
1303.629454	147105.938967	35.872807
1304.791764	147354.373594	35.877824
1305.599276	147612.696976	35.882842
1307.265489	147854.127550	35.887860
1308.499788	148125.801718	35.892877
1309.428112	148379.342163	35.897895
1310.794312	148623.731598	35.902912
1311.754604	148904.981196	35.907930
1312.870806	149173.727682	35.912948
1314.100899	149440.783245	35.917965
1315.221447	149712.361170	35.922983
1316.915906	149991.861869	35.928000
1318.346178	150263.938098	35.933018
1319.696113	150539.441297	35.938036
1320.774078	150804.134762	35.943053
1321.730680	151080.658119	35.948071
1323.219477	151370.425746	35.953088
1324.639085	151654.829315	35.958106
1325.945206	151927.179174	35.963124
1327.375307	152210.646654	35.968141
1328.694667	152495.707311	35.973159
1330.482406	152768.973090	35.978176
1331.639357	153043.841636	35.983194
1333.143418	153303.180568	35.988212
1335.165807	153570.134880	35.993229
1336.451804	153829.323126	35.998247
1337.782135	154096.205076	36.003264
1339.897517	154338.846634	36.008282
1341.012780	154575.109698	36.013300
1342.342110	154804.984016	36.018317
1343.348141	155053.381603	36.023335
1344.859079	155298.475586	36.028352
1345.803365	155532.946153	36.033370
1346.979385	155785.937571	36.038388
1348.538803	156034.897025	36.043405
1350.442238	156271.877541	36.048423
1351.829698	156508.564103	36.053440
1352.930713	156755.485417	36.058458
1353.879694	157014.699841	36.063476
1354.961765	157267.564109	36.068493
1356.152189	157523.799071	36.073511
1357.399407	157789.400771	36.078528
1358.046619	158064.109913	36.083546
1359.604733	158348.768273	36.088564
1360.803206	158621.195678	36.093581
1362.027605	158913.651345	36.098599
1363.389856	159186.461501	36.103616
1364.389098	159465.042050	36.108634
1365.941673	159753.707327	36.113652
1367.014474	160058.476308	36.118669
1368.667118	160360.703455	36.123687
1370.285344	160633.100524	36.128704
1371.704749	160935.789069	36.133722
1372.948471	161222.067262	36.138740
1374.540034	161522.498914	36.143757
1375.541559	161828.802530	36.148775
1377.127652	162114.776685	36.153792
1378.537741	162425.508368	36.158810
1379.994454	162731.984576	36.163828
1381.325060	163018.019789	36.168845
1382.468701	163317.079340	36.173863
1384.260466	163620.170062	36.178880
1385.585960	163933.756127	36.183898
1387.033112	164224.817139	36.188916
1388.930522	164528.911929	36.193933
1389.924114	164837.129240	36.198951
1391.896417	165127.564200	36.203968
1393.690088	165405.634762	36.208986
1394.915766	165713.617079	36.214004
1396.230864	166010.446913	36.219021
1397.492801	166306.221773	36.224039
1399.161178	166601.766631	36.229056
1400.645665	166902.685537	36.234074
1402.327388	167194.438472	36.239092
1403.995617	167479.699185	36.244109
1405.427002	167764.759761	36.249127
1407.278950	168026.862846	36.254144
1409.035319	168312.621949	36.259162
1410.153220	168585.622034	36.264180
1411.961898	168864.816064	36.269197
1413.153917	169137.921503	36.274215
1414.643239	169413.758399	36.279232
1415.524714	169685.459212	36.284250
1416.824521	169964.338034	36.289268
1418.149753	170245.485726	36.294285
1419.354967	170539.217217	36.299303
1420.654356	170829.940410	36.304320
1421.691931	171128.068460	36.309338
1422.330440	171423.701055	36.314356
1424.084545	171729.709086	36.319373
1425.085973	172041.629803	36.324391
1426.401021	172362.573963	36.329408
1427.439729	172671.256912	36.334426
1428.577032	172988.059807	36.339444
1430.255651	173311.031639	36.344461
1431.410534	173627.163396	36.349479
1432.816759	173932.393098	36.354496
1434.171418	174245.374277	36.359514
1435.790724	174536.778524	36.364532
1437.803268	174831.419144	36.369549
1439.187428	175158.297356	36.374567
1440.957557	175445.646722	36.379584
1441.781043	175766.707846	36.384602
1443.007121	176076.993768	36.389620
1444.606944	176388.920558	36.394637
1445.904005	176700.556663	36.399655
1447.423611	177016.942495	36.404672
1448.762268	177343.068822	36.409690
1450.383546	177666.904358	36.414708
1451.608223	177987.139730	36.419725
1453.015915	178324.581642	36.424743
1454.820469	178634.940572	36.429760
1456.638480	178973.918272	36.434778
1458.234163	179285.610229	36.439796
1459.917923	179602.455040	36.444813
1461.354471	179924.406590	36.449831
1462.788255	180232.983586	36.454848
1464.153487	180566.284658	36.459866
1465.497070	180906.876605	36.464884
1467.215213	181230.211410	36.469901
1468.456753	181557.167968	36.474919
1469.675482	181891.885230	36.479936
1471.292158	182216.156766	36.484954
1472.710064	182557.864216	36.489972
1474.557881	182883.269432	36.494989
1475.668167	183213.837259	36.500007
1477.359297	183550.911403	36.505024
1479.064398	183901.134903	36.510042
1480.522527	184236.703342	36.515060
1482.094626	184566.797191	36.520077
1483.160719	184913.109148	36.525095
1484.701616	185238.731686	36.530112
1486.261979	185587.403423	36.535130
1487.495533	185929.378604	36.540148
1489.533323	186282.431251	36.545165
1490.943510	186627.770699	36.550183
1492.075398	186991.830081	36.555200
1493.710748	187337.834921	36.560218
1494.925389	187693.875700	36.565236
1497.053825	188031.095734	36.570253
1497.786264	188382.574600	36.575271
1500.015927	188726.941282	36.580288
1501.809034	189064.311651	36.585306
1503.178371	189407.973925	36.590324
1504.854548	189760.904960	36.595341
1506.045699	190100.729114	36.600359
1507.649053	190447.037379	36.605376
1509.513855	190786.195829	36.610394
1510.571492	191132.814002	36.615412
1512.385917	191478.890418	36.620429
1513.412497	191833.566009	36.625447
1515.129134	192179.116780	36.630464
1516.858461	192522.979079	36.635482
1518.630586	192873.272441	36.640500
1520.763843	193189.346892	36.645517
1522.128195	193527.600614	36.650535
1524.219798	193870.560228	36.655552
1525.606269	194193.504045	36.660570
1526.865887	194524.252480	36.665588
1528.209137	194864.611694	36.670605
1529.517049	195202.147593	36.675623
1530.616474	195542.246046	36.680640
1532.325548	195878.932284	36.685658
1533.268030	196203.191177	36.690676
1535.031683	196530.972477	36.695693
1536.392080	196861.703856	36.700711
1537.685278	197193.298619	36.705728
1539.226258	197520.042588	36.710746
1540.447240	197864.221281	36.715764
1541.998145	198199.269941	36.720781
1543.565788	198548.105115	36.725799
1544.993290	198900.520079	36.730816
1546.646401	199248.684655	36.735834
1547.995064	199598.335922	36.740852
1549.745838	199937.397670	36.745869
1551.498715	200289.613895	36.750887
1553.822654	200620.547874	36.755904
1555.524156	200951.383025	36.760922
1557.267438	201295.670898	36.765940
1559.132523	201628.970772	36.770957
1561.074521	201966.284303	36.775975
1562.010491	202311.573769	36.780992
1563.524397	202644.034978	36.786010
1564.585408	202974.680692	36.791028
1566.492654	203320.132222	36.796045
1567.618452	203668.507632	36.801063
1569.242492	204027.340805	36.806080
1570.475540	204389.769980	36.811098
1571.669115	204753.451759	36.816116
1573.024811	205116.930830	36.821133
1574.319402	205500.140198	36.826151
1576.025981	205875.449471	36.831168
1577.637121	206255.550488	36.836186
1578.626336	206659.639448	36.841204
1580.378016	207039.695810	36.846221
1581.914230	207421.833877	36.851239
1583.600755	207819.477928	36.856256
1584.813431	208211.374071	36.861274
1586.338217	208612.832687	36.866292
1588.155541	209008.124843	36.871309
1589.818363	209407.850534	36.876327
1591.352045	209811.065997	36.881344
1593.466825	210206.124508	36.886362
1594.893421	210618.211988	36.891380
1597.357207	210998.728522	36.896397
1599.389172	211392.955648	36.901415
1601.178581	211767.276095	36.906432
1603.077498	212147.522830	36.911450
1604.357499	212524.317919	36.916468
1606.427278	212916.171368	36.921485
1607.798466	213285.564417	36.926503
1608.875187	213679.388323	36.931520
1610.636549	214059.666190	36.936538
1612.036237	214453.211700	36.941556
1613.530638	214851.390953	36.946573
1614.857378	215243.478954	36.951591
1616.238949	215636.092941	36.956608
1618.074552	216039.732290	36.961626
1619.198989	216453.700477	36.966644
1620.920766	216859.317769	36.971661
1622.013080	217281.650679	36.976679
1623.588445	217683.917791	36.981696
1624.967143	218158.628144	36.986714
1626.302857	218597.257468	36.991732
1628.139376	219018.408476	36.996749
1630.029534	219437.495178	37.001767
1632.038985	219861.262628	37.006784
1633.672444	220274.553580	37.011802
1635.117494	220703.954508	37.016820
1636.921233	221119.049453	37.021837
1638.182315	221538.883539	37.026855
1639.829479	221957.969828	37.031872
1641.513217	222354.065774	37.036890
1643.201388	222762.607926	37.041908
1644.546992	223165.925133	37.046925
1646.039922	223578.109205	37.051943
1647.170796	223994.164422	37.056960
1649.310919	224408.149710	37.061978
1650.728331	224827.361026	37.066996
1652.478011	225247.992216	37.072013
1654.268082	225673.698178	37.077031
1655.697937	226101.471682	37.082048
1657.537086	226525.877217	37.087066
1659.280252	226951.849469	37.092084
1660.854905	227379.019402	37.097101
1662.163423	227813.321324	37.102119
1663.817850	228250.234686	37.107136
1665.537720	228686.706944	37.112154
1667.368162	229128.166290	37.117172
1669.324163	229568.031583	37.122189
1671.149320	230010.663169	37.127207
1672.840311	230449.508260	37.132224
1674.684832	230885.865566	37.137242
1676.951644	231320.478122	37.142260
1678.339936	231738.599450	37.147277
1680.932080	232162.746588	37.152295
1682.855412	232596.200448	37.157312
1685.227500	232993.918535	37.162330
1687.208552	233399.144707	37.167348
1688.980893	233798.818146	37.172365
1690.974658	234205.466819	37.177383
1692.428599	234618.860743	37.182400
1694.147299	235020.425840	37.187418
1696.015241	235422.373735	37.192436
1697.968085	235816.053133	37.197453
1699.239558	236221.454366	37.202471
1700.329970	236636.615242	37.207488
1702.297672	237046.958474	37.212506
1703.962024	237462.306042	37.217524
1705.291524	237883.933249	37.222541
1706.477992	238303.248060	37.227559
1708.180135	238721.488066	37.232576
1709.663108	239148.681229	37.237594
1711.468763	239600.614432	37.242612
1712.842092	240030.342407	37.247629
1714.554791	240460.294730	37.252647
1715.881913	240900.370811	37.257664
1718.415639	241339.080242	37.262682
1720.294250	241782.750476	37.267700
1722.028555	242222.050812	37.272717
1723.896023	242650.508631	37.277735
1725.446323	243088.113625	37.282752
1727.670553	243505.337094	37.287770
1729.381526	243940.402289	37.292788
1731.511933	244369.099216	37.297805
1733.318815	244800.314283	37.302823
1734.537572	245235.767708	37.307840
1736.339494	245657.027150	37.312858
1737.834311	246088.956216	37.317876
1739.743233	246525.110670	37.322893
1741.303384	246966.530871	37.327911
1742.454721	247416.300462	37.332928
1744.436829	247860.751453	37.337946
1746.081274	248307.417994	37.342964
1747.673713	248751.832841	37.347981
1749.561204	249192.236712	37.352999
1750.946001	249642.402568	37.358016
1752.740324	250088.259090	37.363034
1754.820703	250529.216939	37.368052
1756.475320	250962.014907	37.373069
1758.413151	251382.319076	37.378087
1759.547849	251814.644772	37.383104
1761.605148	252248.495253	37.388122
1763.159154	252693.123853	37.393140
1764.796963	253122.344684	37.398157
1766.683488	253565.318727	37.403175
1767.983828	254008.237378	37.408192
1769.591815	254448.362029	37.413210
1771.305943	254901.425088	37.418228
1773.003456	255354.033899	37.423245
1775.156005	255809.641681	37.428263
1776.477012	256279.866730	37.433280
1778.208911	256730.616109	37.438298
1779.840010	257200.536366	37.443316
1781.378483	257676.009986	37.448333
1783.460489	258152.435618	37.453351
1784.725666	258641.773980	37.458368
1786.606447	259114.955992	37.463386
1788.016016	259609.097322	37.468404
1789.405063	260103.140463	37.473421
1791.893696	260596.367132	37.478439
1793.617637	261096.172373	37.483456
1795.624398	261603.475688	37.488474
1797.384183	262097.686156	37.493492
1798.725398	262607.995043	37.498509
1800.587207	263110.165058	37.503527
1802.334632	263626.122342	37.508544
1804.457174	264136.835258	37.513562
1806.436639	264645.996530	37.518580
1808.560134	265150.434165	37.523597
1810.938651	265644.033057	37.528615
1812.975862	266150.719776	37.533632
1815.087751	266655.513969	37.538650
1816.969158	267155.697008	37.543668
1819.014436	267648.104634	37.548685
1821.006569	268135.617787	37.553703
1822.674099	268640.356521	37.558720
1824.678492	269146.436330	37.563738
1826.423764	269640.771320	37.568756
1828.005465	270130.356967	37.573773
1830.098935	270619.959224	37.578791
1831.654398	271120.293458	37.583808
1834.083840	271599.627064	37.588826
1836.172688	272089.431397	37.593844
1838.261116	272584.849132	37.598861
1840.259679	273059.831698	37.603879
1841.891856	273557.380843	37.608896
1843.416464	274038.943214	37.613914
1845.703891	274530.235206	37.618932
1847.137206	275014.325890	37.623949
1849.003176	275502.688199	37.628967
1850.714167	276002.709548	37.633984
1852.920968	276491.547255	37.639002
1854.969737	276981.705607	37.644020
1857.249414	277464.305779	37.649037
1859.475087	277929.233851	37.654055
1861.544747	278401.832813	37.659072
1863.260735	278871.847291	37.664090
1865.277684	279331.040595	37.669108
1867.273494	279805.706293	37.674125
1869.178865	280270.402821	37.679143
1870.708672	280743.746122	37.684160
1872.347124	281220.017003	37.689178
1874.218670	281694.724157	37.694196
1875.709532	282159.433805	37.699213
1877.143836	282630.629073	37.704231
1879.200556	283118.764985	37.709248
1881.078921	283572.560597	37.714266
1883.082265	284035.631385	37.719284
1884.554661	284506.586763	37.724301
1886.638653	284952.292542	37.729319
1888.332117	285412.565706	37.734336
1890.083282	285884.614237	37.739354
1892.048604	286340.191472	37.744372
1893.450042	286823.344406	37.749389
1895.624717	287284.066164	37.754407
1897.362008	287757.051126	37.759424
1898.888670	288239.061236	37.764442
1900.918639	288728.784776	37.769460
1902.691972	289220.174623	37.774477
1905.155324	289692.195271	37.779495
1906.995914	290175.442471	37.784512
1908.799416	290667.381028	37.789530
1910.772483	291155.987768	37.794548
1912.350427	291661.091838	37.799565
1914.243729	292155.346866	37.804583
1916.092403	292655.982760	37.809600
1917.419563	293174.330251	37.814618
1919.766826	293677.064211	37.819636
1921.272191	294197.359189	37.824653
1923.473569	294705.142096	37.829671
1926.002279	295230.165902	37.834688
1927.777386	295743.958124	37.839706
1929.600149	296263.785221	37.844724
1931.557714	296791.613835	37.849741
1933.126001	297311.986052	37.854759
1935.065988	297846.949679	37.859776
1936.764523	298381.594915	37.864794
1938.540579	298913.329249	37.869812
1940.204343	299466.642785	37.874829
1942.432852	300021.003157	37.879847
1944.078507	300563.544893	37.884864
1945.702366	301137.504793	37.889882
1947.547762	301687.017404	37.894900
1949.366199	302260.202176	37.899917
1951.269013	302817.013547	37.904935
1953.633355	303392.184167	37.909952
1955.505430	303949.781315	37.914970
1957.764422	304516.860672	37.919988
1960.040018	305090.283071	37.925005
1962.504137	305647.391349	37.930023
1964.955918	306203.152184	37.935040
1966.579037	306769.585808	37.940058
1968.775086	307319.210431	37.945076
1971.386553	307877.880312	37.950093
1973.516843	308419.305779	37.955111
1975.647624	308967.127483	37.960128
1977.477046	309520.074467	37.965146
1978.831496	310069.083600	37.970164
1980.597220	310615.380097	37.975181
1982.799934	311171.758938	37.980199
1984.984227	311733.063601	37.985216
1986.737860	312287.654888	37.990234
1989.007606	312837.484501	37.995252
1990.475090	313407.301068	38.000269
1992.345710	313964.248169	38.005287
1994.532923	314535.969157	38.010304
1996.190745	315102.211839	38.015322
1998.504468	315661.968196	38.020340
2000.455511	316232.166091	38.025357
2002.569732	316798.726755	38.030375
2004.606099	317359.785495	38.035392
2006.471883	317932.244019	38.040410
2008.575743	318474.542822	38.045428
2010.536661	319027.932169	38.050445
2012.798663	319577.737908	38.055463
2014.630667	320111.714676	38.060480
2016.470424	320654.954055	38.065498
2018.562856	321199.416980	38.070516
2020.859523	321742.165951	38.075533
2022.703127	322285.772341	38.080551
2024.942217	322816.994307	38.085568
2026.659202	323352.512955	38.090586
2028.708548	323890.257518	38.095604
2030.157283	324452.547688	38.100621
2031.949269	325010.358365	38.105639
2033.955983	325559.597633	38.110656
2035.897120	326141.011795	38.115674
2038.232806	326697.194350	38.120692
2040.520801	327268.257895	38.125709
2042.497211	327837.818738	38.130727
2044.466176	328396.864443	38.135744
2046.551750	328970.255664	38.140762
2048.792260	329530.489998	38.145780
2050.747932	330110.746451	38.150797
2053.117774	330677.117819	38.155815
2055.417781	331253.574062	38.160832
2057.329398	331843.746990	38.165850
2059.360493	332418.966476	38.170868
2061.310465	333003.865883	38.175885
2063.382804	333584.067876	38.180903
2065.435326	334162.388497	38.185920
2067.138621	334758.251652	38.190938
2069.666996	335339.502350	38.195956
2071.305029	335948.893882	38.200973
2073.142067	336555.174093	38.205991
2075.168379	337146.718342	38.211008
2077.354883	337759.501904	38.216026
2079.428396	338366.280877	38.221044
2081.855265	338976.472137	38.226061
2084.141818	339576.602004	38.231079
2086.183733	340176.765213	38.236096
2088.216508	340804.488968	38.241114
2090.318612	341417.826828	38.246132
2092.294606	342026.279173	38.251149
2094.032099	342641.515098	38.256167
2096.102875	343256.231538	38.261184
2098.156517	343896.553113	38.266202
2100.057519	344530.013141	38.271220
2102.144428	345163.764169	38.276237
2104.168369	345802.999418	38.281255
2106.376940	346425.368561	38.286272
2108.593714	347071.483736	38.291290
2110.994934	347696.672248	38.296308
2113.081272	348339.415949	38.301325
2115.047733	348990.012554	38.306343
2117.769282	349621.213157	38.311360
2119.370265	350258.452174	38.316378
2122.099933	350883.771559	38.321396
2124.052659	351524.386073	38.326413
2126.455889	352152.152448	38.331431
2128.728478	352779.728470	38.336448
2130.475126	353417.253678	38.341466
2132.804546	354050.993977	38.346484
2134.708712	354694.793143	38.351501
2136.872526	355330.597448	38.356519
2139.237843	355955.600165	38.361536
2141.505518	356603.979680	38.366554
2143.450827	357232.813645	38.371572
2145.358867	357877.680512	38.376589
2147.685219	358517.596763	38.381607
2150.041933	359145.725107	38.386624
2152.155602	359770.230315	38.391642
2154.590545	360382.773486	38.396660
2156.576806	360974.576588	38.401677
2158.662577	361583.886249	38.406695
2161.398713	362180.723747	38.411712
2163.006084	362792.605660	38.416730
2165.248468	363393.870156	38.421748
2167.416409	363987.729781	38.426765
2169.377430	364594.679819	38.431783
2172.002974	365193.012199	38.436800
2174.502428	365803.609214	38.441818
2176.727250	366393.135455	38.446836
2178.856924	367005.651627	38.451853
2180.330875	367609.057710	38.456871
2182.684189	368225.423952	38.461888
2184.232409	368853.657640	38.466906
2186.206043	369480.035017	38.471924
2188.764390	370100.090832	38.476941
2190.810350	370731.330795	38.481959
2193.074484	371368.915926	38.486976
2195.203986	372013.233749	38.491994
2197.440286	372649.989453	38.497012
2199.400113	373305.497866	38.502029
2201.430029	373961.058881	38.507047
2203.471961	374611.533385	38.512064
2205.393781	375271.526624	38.517082
2207.638907	375953.341372	38.522100
2209.798254	376614.157990	38.527117
2212.108382	377305.826597	38.532135
2214.340917	377955.624549	38.537152
2216.239087	378637.621563	38.542170
2218.946855	379315.135119	38.547188
2221.275186	379987.981093	38.552205
2223.244252	380678.699808	38.557223
2225.573771	381359.100464	38.562240
2228.129282	382044.901866	38.567258
2230.737355	382737.349318	38.572276
2233.253224	383409.816918	38.577293
2235.714333	384086.007132	38.582311
2238.104102	384766.429491	38.587328
2240.103306	385443.910245	38.592346
2242.415847	386117.927768	38.597364
2244.590494	386805.619504	38.602381
2246.249791	387509.100327	38.607399
2249.147255	388182.344279	38.612416
2251.995031	388862.249702	38.617434
2254.352883	389540.598807	38.622452
2256.931585	390205.410258	38.627469
2259.183146	390889.831899	38.632487
2261.511409	391546.062365	38.637504
2263.602722	392239.606557	38.642522
2265.673644	392905.508582	38.647540
2268.161508	393575.687246	38.652557
2270.332724	394272.619589	38.657575
2272.366306	394929.485237	38.662592
2274.937742	395617.373166	38.667610
2276.978390	396304.724563	38.672628
2278.875028	396977.713204	38.677645
2280.571895	397681.513183	38.682663
2282.915795	398377.181042	38.687680
2284.967142	399085.324271	38.692698
2287.015741	399787.672683	38.697716
2289.389638	400494.005258	38.702733
2291.462616	401207.389823	38.707751
2293.606764	401917.121258	38.712768
2295.824041	402633.310170	38.717786
2297.981751	403369.179779	38.722804
2300.469869	404086.478423	38.727821
2302.318428	404807.994446	38.732839
2304.380610	405504.803202	38.737856
2306.725889	406205.576502	38.742874
2308.984193	406907.739996	38.747892
2312.141092	407581.513506	38.752909
2313.990818	408294.096790	38.757927
2316.664598	408988.563568	38.762944
2319.114671	409680.161509	38.767962
2321.603299	410385.263396	38.772980
2324.006493	411072.298913	38.777997
2325.863633	411784.409464	38.783015
2327.920188	412482.485405	38.788032
2330.688934	413196.738486	38.793050
2332.818142	413905.555893	38.798068
2335.197827	414611.729409	38.803085
2337.490298	415355.561727	38.808103
2339.953352	416057.630020	38.813120
2343.215619	416759.269013	38.818138
2345.946524	417459.305083	38.823156
2348.826285	418153.675317	38.828173
2351.334985	418860.294611	38.833191
2354.103936	419550.086788	38.838208
2356.486737	420238.708412	38.843226
2358.806770	420923.092753	38.848244
2361.206126	421615.346001	38.853261
2363.502766	422317.371232	38.858279
2366.024324	423017.845756	38.863296
2368.083326	423722.225508	38.868314
2370.063956	424433.712930	38.873332
2372.214283	425122.896780	38.878349
2374.424948	425847.749663	38.883367
2376.739234	426554.892612	38.888384
2378.743139	427296.496577	38.893402
2381.213172	428014.508100	38.898420
2383.677268	428752.649928	38.903437
2385.984660	429492.617558	38.908455
2388.301653	430221.169742	38.913472
2390.457342	430968.761302	38.918490
2392.701641	431714.289772	38.923508
2395.209230	432451.398699	38.928525
2397.863028	433209.771577	38.933543
2400.109819	433960.847302	38.938560
2402.694088	434712.197518	38.943578
2404.917274	435472.592491	38.948596
2407.556738	436221.961261	38.953613
2409.992792	436986.219111	38.958631
2412.799247	437732.980439	38.963648
2415.419299	438474.434139	38.968666
2417.768376	439241.768523	38.973684
2420.233324	439990.890464	38.978701
2422.486529	440751.661241	38.983719
2424.983156	441491.214471	38.988736
2427.274062	442260.024077	38.993754
2429.375208	443031.874302	38.998772
2431.504568	443796.255260	39.003789
2434.318135	444567.023668	39.008807
2436.742075	445335.451373	39.013824
2439.348931	446103.923096	39.018842
2441.363361	446880.863236	39.023860
2443.766035	447655.536254	39.028877
2445.978423	448436.687846	39.033895
2448.283989	449223.208189	39.038912
2450.698938	450020.202698	39.043930
2452.652073	450815.877875	39.048948
2455.309119	451607.613796	39.053965
2458.063577	452397.280931	39.058983
2459.835214	453196.790789	39.064000
2462.306765	453996.357051	39.069018
2464.599819	454796.225529	39.074036
2467.329325	455569.695487	39.079053
2469.489997	456366.238258	39.084071
2471.838848	457124.997755	39.089088
2474.894579	457898.983858	39.094106
2476.965701	458681.091647	39.099124
2479.524626	459456.010687	39.104141
2481.827690	460238.677568	39.109159
2484.348374	461026.991002	39.114176
2486.631112	461827.496125	39.119194
2488.515759	462631.067979	39.124212
2491.156884	463429.528945	39.129229
2493.277516	464251.800818	39.134247
2495.404617	465070.954225	39.139264
2498.215889	465901.585682	39.144282
2500.673297	466731.785464	39.149300
2502.946971	467567.084686	39.154317
2505.416173	468406.712513	39.159335
2507.626142	469258.727607	39.164352
2510.254806	470098.003088	39.169370
2513.067613	470956.059188	39.174388
2515.877897	471810.186638	39.179405
2518.720335	472665.887337	39.184423
2521.014822	473525.277464	39.189440
2524.380718	474378.541002	39.194458
2526.498267	475252.583153	39.199476
2529.393905	476103.370510	39.204493
2532.503957	476945.799520	39.209511
2535.119477	477797.667032	39.214528
2537.842827	478641.699209	39.219546
2539.884748	479511.917119	39.224564
2542.075457	480371.968447	39.229581
2544.718664	481245.085799	39.234599
2547.220436	482114.851692	39.239616
2549.599497	482988.787422	39.244634
2551.947310	483862.029653	39.249652
2554.731220	484743.892820	39.254669
2557.018320	485632.055263	39.259687
2559.657696	486535.463587	39.264704
2562.299859	487408.534837	39.269722
2565.312189	488296.141881	39.274740
2568.288693	489181.691018	39.279757
2571.015382	490060.624246	39.284775
2573.460887	490946.727100	39.289792
2576.753962	491809.630020	39.294810
2579.206396	492697.207281	39.299828
2581.896651	493559.718742	39.304845
2584.626801	494451.147003	39.309863
2586.955958	495327.204294	39.314880
2589.583971	496199.837171	39.319898
2592.329452	497086.483376	39.324916
2594.749830	497971.169174	39.329933
2597.422787	498847.039005	39.334951
2600.194871	499718.054350	39.339968
2602.955788	500594.676291	39.344986
2605.428433	501475.940588	39.350004
2607.744864	502355.771685	39.355021
2610.694057	503238.225934	39.360039
2613.042076	504128.095732	39.365056
2615.720906	505003.489658	39.370074
2618.194839	505885.123973	39.375092
2620.924993	506763.239473	39.380109
2623.335738	507663.194055	39.385127
2625.877898	508555.412998	39.390144
2628.565159	509442.466494	39.395162
2630.944615	510335.773472	39.400180
2633.209353	511241.501704	39.405197
2636.052074	512132.615603	39.410215
2638.427366	513034.392692	39.415232
2640.929094	513897.890959	39.420250
2643.650157	514765.842110	39.425268
2646.910084	515613.648141	39.430285
2649.525303	516484.394680	39.435303
2651.964059	517348.973836	39.440320
2654.317081	518216.341089	39.445338
2656.883357	519095.617141	39.450356
2659.437873	519965.927037	39.455373
2662.064546	520839.450814	39.460391
2664.775819	521722.583885	39.465408
2668.800890	522576.835613	39.470426
2671.467538	523443.151662	39.475444
2674.493985	524308.150196	39.480461
2678.094074	525160.362465	39.485479
2680.856050	526016.039296	39.490496
2683.728062	526857.699019	39.495514
2686.121539	527716.764484	39.500532
2688.851637	528574.063395	39.505549
2691.530793	529425.278986	39.510567
2693.878779	530289.239193	39.515584
2696.308284	531148.553944	39.520602
2698.629689	532035.928979	39.525620
2701.042527	532921.121100	39.530637
2703.907107	533787.660671	39.535655
2706.138591	534684.756736	39.540672
2708.759017	535578.562517	39.545690
2711.302145	536484.354791	39.550708
2713.601064	537404.121355	39.555725
2716.337554	538311.377662	39.560743
2718.637505	539246.073013	39.565760
2721.498962	540177.344251	39.570778
2723.868929	541123.629096	39.575796
2726.299451	542071.803100	39.580813
2728.792127	543023.173360	39.585831
2731.180762	543994.165200	39.590848
2733.955569	544964.875506	39.595866
2736.684509	545945.434505	39.600884
2739.364749	546910.342030	39.605901
2743.107918	547875.108071	39.610919
2746.638215	548848.139212	39.615936
2750.644303	549781.401150	39.620954
2754.039815	550729.834379	39.625972
2756.623809	551677.732540	39.630989
2759.302990	552616.852344	39.636007
2761.847953	553571.914914	39.641024
2764.498051	554527.094110	39.646042
2766.805634	555478.945171	39.651060
2769.191174	556432.575809	39.656077
2772.000013	557392.803135	39.661095
2773.778088	558375.543249	39.666112
2776.539457	559356.843126	39.671130
2779.150726	560335.382308	39.676148
2781.438723	561330.129880	39.681165
2784.421247	562330.615941	39.686183
2786.933708	563348.182229	39.691200
2789.065654	564363.070327	39.696218
2792.262665	565379.763361	39.701236
2795.012866	566400.468336	39.706253
2797.784966	567407.681899	39.711271
2800.316225	568442.372923	39.716288
2803.371415	569462.033115	39.721306
2806.247997	570492.787133	39.726324
2809.186084	571518.076714	39.731341
2812.473125	572542.624102	39.736359
2815.631964	573577.048067	39.741376
2818.863395	574592.956815	39.746394
2821.611385	575604.447394	39.751412
2824.319365	576607.483332	39.756429
2827.413848	577582.076333	39.761447
2829.991106	578555.926068	39.766464
2832.905333	579529.744551	39.771482
2835.548439	580502.327480	39.776500
2838.066654	581473.550485	39.781517
2840.750015	582451.892370	39.786535
2843.877215	583438.910113	39.791552
2846.835427	584422.867420	39.796570
2849.665237	585393.127559	39.801588
2852.192032	586384.669907	39.806605
2855.247621	587373.186466	39.811623
2857.935483	588370.857061	39.816640
2860.539953	589362.594040	39.821658
2863.716383	590374.254529	39.826676
2866.250985	591387.940237	39.831693
2869.802501	592377.066685	39.836711
2872.609563	593393.093085	39.841728
2875.562911	594379.746306	39.846746
2879.151755	595401.484599	39.851764
2881.531733	596399.236564	39.856781
2884.149192	597420.158359	39.861799
2886.857499	598442.879719	39.866816
2889.606151	599485.588983	39.871834
2892.319842	600518.645375	39.876852
2894.772711	601566.625553	39.881869
2897.601970	602615.500348	39.886887
2900.305332	603692.187678	39.891904
2903.405047	604764.353515	39.896922
2906.641776	605820.928791	39.901940
2908.922843	606898.535883	39.906957
2911.770084	607971.543504	39.911975
2914.906157	609052.258850	39.916992
2918.258446	610125.279527	39.922010
2921.246042	611220.322944	39.927028
2923.873078	612309.215583	39.932045
2926.956486	613382.970053	39.937063
2929.784236	614483.373470	39.942080
2932.773160	615583.791539	39.947098
2935.895394	616687.879119	39.952116
2938.477200	617797.145864	39.957133
2941.440232	618910.687990	39.962151
2944.147455	620034.208067	39.967168
2947.193891	621141.710503	39.972186
2950.293341	622271.784240	39.977204
2952.995982	623396.058368	39.982221
2956.340794	624508.666159	39.987239
2959.426289	625635.742690	39.992256
2962.220252	626760.900597	39.997274
2965.199570	627899.098686	40.002292
2968.062427	629028.053549	40.007309
2971.380053	630150.670393	40.012327
2974.414605	631294.690034	40.017344
2977.381526	632433.303944	40.022362
2980.457678	633572.076543	40.027380
2983.150275	634720.524424	40.032397
2985.895170	635860.201725	40.037415
2988.790382	637019.346214	40.042432
2991.868144	638158.218355	40.047450
2995.294123	639304.094177	40.052468
2998.394867	640438.869223	40.057485
3001.646967	641583.472850	40.062503
3004.485756	642729.413897	40.067520
3007.722749	643870.222887	40.072538
3010.572365	645000.294857	40.077556
3013.393641	646156.377840	40.082573
3017.022901	647280.083343	40.087591
3020.222957	648409.219120	40.092608
3022.929945	649543.843336	40.097626
3026.730999	650625.320659	40.102644
3029.840866	651711.430412	40.107661
3033.684165	652767.797672	40.112679
3038.238579	653785.814263	40.117696
3041.364149	654824.689798	40.122714
3044.777302	655852.946392	40.127732
3047.738591	656875.092715	40.132749
3050.938648	657895.051290	40.137767
3053.780833	658917.154303	40.142784
3056.382176	659932.118552	40.147802
3059.680989	660956.721883	40.152820
3062.096854	661992.515875	40.157837
3064.622793	663018.970978	40.162855
3067.237860	664083.085327	40.167872
3069.943824	665143.732519	40.172890
3072.671355	666218.194466	40.177908
3074.827984	667306.613561	40.182925
3077.716150	668407.675438	40.187943
3080.356151	669491.387363	40.192960
3083.512449	670608.568614	40.197978
3086.630247	671721.894103	40.202996
3089.754704	672852.991592	40.208013
3092.948184	673973.250481	40.213031
3095.953943	675115.831349	40.218048
3098.985151	676257.771534	40.223066
3102.064923	677414.029636	40.228084
3104.706517	678584.878887	40.233101
3107.724929	679755.617800	40.238119
3110.670569	680929.947428	40.243136
3113.488505	682100.372621	40.248154
3116.808078	683283.333523	40.253172
3119.478992	684486.365697	40.258189
3122.885910	685675.013419	40.263207
3125.848771	686900.078264	40.268224
3128.615140	688105.993658	40.273242
3132.092061	689327.071047	40.278260
3135.685157	690534.412818	40.283277
3139.343616	691758.109189	40.288295
3142.666308	692986.060927	40.293312
3145.660859	694210.573691	40.298330
3149.333641	695415.755758	40.303348
3152.955097	696635.713801	40.308365
3156.561661	697837.155103	40.313383
3160.169079	699030.795777	40.318400
3163.643411	700219.090182	40.323418
3167.217084	701407.009040	40.328436
3170.424661	702611.433217	40.333453
3173.816476	703790.581354	40.338471
3176.773854	704970.582824	40.343488
3179.774158	706153.191534	40.348506
3183.014558	707352.691590	40.353524
3186.321006	708533.586144	40.358541
3189.688290	709702.966029	40.363559
3192.854143	710892.722248	40.368576
3195.730697	712083.994539	40.373594
3199.295832	713254.687914	40.378612
3202.210164	714453.246717	40.383629
3205.475807	715641.183973	40.388647
3208.975251	716826.886579	40.393664
3211.701901	718018.833726	40.398682
3215.027193	719200.717062	40.403700
3218.357403	720396.877310	40.408717
3221.261145	721587.149520	40.413735
3224.264587	722778.471440	40.418752
3227.681874	723983.053036	40.423770
3230.962810	725152.379868	40.428788
3234.539128	726358.912509	40.433805
3237.981157	727511.960721	40.438823
3241.409223	728642.610929	40.443840
3244.296372	729791.426817	40.448858
3247.707490	730908.375721	40.453876
3250.129026	732059.418763	40.458893
3253.136922	733210.597081	40.463911
3256.478701	734352.716958	40.468928
3259.013199	735512.040611	40.473946
3262.353275	736682.962585	40.478964
3264.792070	737864.672488	40.483981
3267.046176	739042.832869	40.488999
3270.403345	740244.225702	40.494016
3272.813438	741478.453480	40.499034
3276.071242	742700.509954	40.504052
3278.596234	743951.550439	40.509069
3281.550452	745208.338438	40.514087
3285.094022	746478.486974	40.519104
3287.887691	747771.625871	40.524122
3291.531885	749043.116533	40.529140
3294.805383	750357.485835	40.534157
3297.555451	751665.362484	40.539175
3300.764960	752983.830733	40.544192
3303.638539	754328.679704	40.549210
3307.144425	755654.917820	40.554228
3310.538654	757012.853672	40.559245
3313.248948	758367.411823	40.564263
3317.053662	759711.064437	40.569280
3320.810247	761085.394667	40.574298
3324.518081	762446.493263	40.579316
3327.886109	763818.029258	40.584333
3330.963579	765198.807530	40.589351
3335.122006	766555.646102	40.594368
3338.484304	767934.348984	40.599386
3342.343442	769302.145594	40.604404
3345.966351	770678.773576	40.609421
3349.293730	772038.338561	40.614439
3352.859117	773413.681125	40.619456
3356.083389	774791.918046	40.624474
3359.540807	776176.243017	40.629492
3362.691683	777561.928202	40.634509
3365.450689	778942.014278	40.639527
3368.923651	780326.924363	40.644544
3372.402887	781730.758607	40.649562
3376.046274	783119.131124	40.654580
3379.718852	784503.748266	40.659597
3383.372239	785910.125131	40.664615
3387.246761	787289.511728	40.669632
3390.330201	788670.184134	40.674650
3394.204296	790046.634988	40.679668
3397.919741	791436.029210	40.684685
3401.252886	792816.932320	40.689703
3404.707092	794195.340599	40.694720
3408.183048	795581.263470	40.699738
3412.292028	796940.509616	40.704756
3415.862502	798316.864372	40.709773
3419.562936	799667.518858	40.714791
3423.537640	801013.509625	40.719808
3427.150701	802373.293932	40.724826
3431.250683	803696.329879	40.729844
3434.527326	805022.377981	40.734861
3437.732649	806381.487282	40.739879
3440.970548	807701.448521	40.744896
3444.159028	809055.432937	40.749914
3447.267075	810393.178425	40.754932
3450.825424	811741.581535	40.759949
3453.741930	813088.111789	40.764967
3457.005017	814433.974483	40.769984
3460.342912	815786.979277	40.775002
3463.873281	817120.830680	40.780007
3467.377499	818398.953420	40.785012
3470.561202	819630.591395	40.790016
3473.728207	820812.637316	40.795021
3476.635483	821927.155080	40.800026
3479.325132	822968.057467	40.805031
3481.970153	823962.834152	40.810036
3484.422818	824885.468106	40.815040
3487.204824	825741.672484	40.820045
3489.582668	826537.753233	40.825050
3491.842185	827257.457178	40.830055
3494.316858	827930.763099	40.835060
3495.779511	828536.238201	40.840064
3497.956373	829109.288617	40.845069
3499.766613	829613.210583	40.850074
3501.577629	830056.949462	40.855079
3503.314889	830449.372576	40.860084
3505.034803	830805.477608	40.865088
3506.611768	831086.894967	40.870093
3507.932348	831345.774449	40.875098
3509.178609	831543.402149	40.880103
3510.256618	831722.929872	40.885108
3511.168828	831859.106162	40.890112
3512.327737	831961.097278	40.895117
3513.155011	832032.858704	40.900122
3514.065470	832067.973543	40.905127
3514.929577	832088.833755	40.910132
3515.423614	832078.642039	40.915136
3516.193759	832032.114441	40.920141
3516.700457	831983.822692	40.925146
3517.031105	831894.970163	40.930151
3517.654698	831783.746015	40.935156
3517.783157	831672.406135	40.940160
3518.225455	831543.574348	40.945165
3518.726902	831400.808618	40.950170
3519.237207	831224.723187	40.955175
3519.052548	831059.641129	40.960180
3519.068838	830872.929274	40.965184
3519.415144	830677.168688	40.970189
3519.670153	830483.371446	40.975194
3519.940288	830263.720923	40.980199
3520.171644	830051.935534	40.985204
3520.262087	829826.925494	40.990208
3520.376098	829574.687931	40.995213
3520.633578	829340.936233	41.000218
3520.664937	829078.871567	41.005223
3520.949773	828830.095394	41.010228
3520.856780	828569.838871	41.015232
3520.750749	828288.559522	41.020237
3520.546815	828021.213093	41.025242
3520.478830	827742.640901	41.030247
3521.096269	827462.624268	41.035252
3520.942272	827196.604507	41.040256
3521.008496	826903.897260	41.045261
3520.716708	826613.728992	41.050266
3520.735323	826328.238694	41.055271
3520.746130	826026.848650	41.060276
3520.548937	825744.399587	41.065280
3520.705061	825428.682218	41.070285
3520.750013	825142.109320	41.075290
3520.402417	824842.875417	41.080295
3520.497156	824547.418090	41.085300
3520.418679	824247.232623	41.090304
3520.364469	823949.425770	41.095309
3520.180997	823657.935608	41.100314
3519.834127	823353.694527	41.105319
3520.279583	823051.412066	41.110324
3519.940348	822759.418819	41.115328
3519.935644	822454.786539	41.120333
3519.516143	822164.687938	41.125338
3519.382250	821862.348770	41.130343
3519.379494	821580.863537	41.135348
3519.199584	821283.984733	41.140352
3519.291911	820997.077514	41.145357
3519.209475	820703.875040	41.150362
3518.790149	820407.975057	41.155367
3518.791882	820116.102823	41.160372
3518.665450	819842.589120	41.165376
3518.598510	819548.745963	41.170381
3518.334815	819268.233424	41.175386
3518.509400	818986.853844	41.180391
3518.476701	818699.525587	41.185396
3517.990729	818420.775933	41.190400
3517.935793	818133.867489	41.195405
3517.906756	817855.997926	41.200410
3517.677509	817578.100841	41.205415
3517.751226	817312.869946	41.210420
3517.072296	817028.660292	41.215424
3517.330734	816753.977564	41.220429
3517.105915	816497.428842	41.225434
3516.817037	816233.879535	41.230439
3516.828340	815958.176752	41.235444
3516.512313	815698.576837	41.240448
3516.423533	815437.509437	41.245453
3516.421821	815182.832360	41.250458
3516.429021	814924.765251	41.255463
3516.325215	814675.374516	41.260468
3516.123730	814418.056925	41.265472
3516.199676	814165.434415	41.270477
3515.815102	813917.384190	41.275482
3515.737091	813658.596921	41.280487
3515.743989	813413.059552	41.285492
3515.401591	813171.244479	41.290496
3515.547979	812916.604299	41.295501
3515.087394	812691.740111	41.300506
3515.112464	812436.611970	41.305511
3515.122744	812199.651812	41.310516
3514.867214	811958.660859	41.315520
3515.053855	811714.795888	41.320525
3514.926363	811487.926091	41.325530
3514.688500	811254.746340	41.330535
3514.545792	811020.268945	41.335540
3514.526360	810784.293145	41.340544
3514.424533	810535.827310	41.345549
3513.968079	810331.464731	41.350554
3514.060388	810096.132657	41.355559
3514.142763	809874.221843	41.360564
3513.793322	809661.686429	41.365568
3513.953592	809432.985295	41.370573
3513.866401	809211.276831	41.375578
3513.485506	809009.214606	41.380583
3513.373319	808776.125157	41.385588
3513.397964	808554.916073	41.390592
3513.427569	808349.678679	41.395597
3513.114351	808142.285733	41.400602
3512.933741	807931.972441	41.405607
3513.094654	807719.586520	41.410612
3512.151318	807533.358247	41.415616
3512.624592	807335.027601	41.420621
3512.666351	807124.750888	41.425626
3512.217182	806925.677847	41.430631
3512.196199	806738.050291	41.435636
3512.057063	806538.620751	41.440640
3512.156910	806349.933025	41.445645
3511.629940	806155.557448	41.450650
3511.505471	805983.812987	41.455655
3511.566333	805789.281165	41.460660
3511.020888	805612.791254	41.465664
3511.164032	805428.631488	41.470669
3511.263202	805245.209622	41.475674
3511.275622	805072.537099	41.480679
3510.924611	804890.454977	41.485684
3510.714620	804728.256405	41.490688
3511.108964	804552.957674	41.495693
3511.015281	804387.740198	41.500698
3511.045897	804209.353703	41.505703
3511.164254	804030.457653	41.510708
3510.589900	803864.178676	41.515712
3510.734280	803693.804196	41.520717
3510.886450	803520.432058	41.525722
3510.761491	803341.607258	41.530727
3510.391229	803187.394453	41.535732
3510.281143	803021.263940	41.540736
3509.964753	802863.061520	41.545741
3509.737584	802700.474643	41.550746
3509.729546	802543.146199	41.555751
3509.768908	802397.826044	41.560756
3509.623927	802248.363021	41.565760
3509.567774	802091.522834	41.570765
3509.465091	801943.861558	41.575770
3509.378992	801794.231833	41.580775
3509.469562	801655.805696	41.585780
3509.276211	801519.288070	41.590784
3509.469473	801375.638412	41.595789
3509.287150	801222.086804	41.600794
3508.966939	801079.791362	41.605799
3508.937502	800939.555122	41.610804
3508.605960	800803.340572	41.615808
3508.711473	800670.977125	41.620813
3509.107541	800531.545849	41.625818
3508.462762	800395.669327	41.630823
3508.883727	800253.087619	41.635828
3508.396159	800115.167632	41.640832
3508.324634	799974.771603	41.645837
3508.039939	799862.823958	41.650842
3508.264155	799732.288027	41.655847
3508.504873	799603.170239	41.660852
3508.108832	799474.007697	41.665856
3508.267931	799345.585701	41.670861
3508.241394	799230.640467	41.675866
3508.425779	799093.914755	41.680871
3508.210289	798973.008235	41.685876
3507.921618	798847.841277	41.690880
3507.921264	798729.103908	41.695885
3507.795458	798604.740214	41.700890
3507.598714	798490.007140	41.705895
3507.754500	798360.733047	41.710900
3507.364838	798262.030795	41.715904
3507.458728	798147.931467	41.720909
3507.298273	798035.295798	41.725914
3507.420541	797930.711831	41.730919
3507.522249	797807.376455	41.735924
3507.433953	797700.221827	41.740928
3507.462409	797581.214710	41.745933
3507.307216	797463.217710	41.750938
3507.476698	797356.899061	41.755943
3507.550741	797245.144836	41.760948
3507.023468	797139.674093	41.765952
3507.113402	797032.872650	41.770957
3506.901004	796922.289693	41.775962
3506.800132	796816.252850	41.780967
3506.645249	796716.704491	41.785972
3506.414457	796616.381610	41.790976
3506.848802	796519.728534	41.795981
3506.652600	796409.724025	41.800986
3506.657707	796315.004708	41.805991
3506.609552	796210.963226	41.810996
3506.287710	796117.473576	41.816000
3506.535021	796016.523203	41.821005
3506.364885	795933.563647	41.826010
3506.062216	795832.553900	41.831015
3506.238136	795740.941482	41.836020
3506.628131	795659.948910	41.841024
3506.064246	795568.210558	41.846029
3506.206457	795474.832331	41.851034
3506.062967	795392.598615	41.856039
3506.126533	795299.329226	41.861044
3505.957224	795211.204450	41.866048
3505.954366	795124.966483	41.871053
3505.819215	795032.708507	41.876058
3505.801175	794944.359019	41.881063
3506.325312	794851.253380	41.886068
3506.042694	794768.789711	41.891072
3505.872752	794673.143906	41.896077
3506.013046	794600.284100	41.901082
3505.620741	794512.776670	41.906087
3505.784415	794436.129428	41.911092
3505.662524	794351.178588	41.916096
3505.548764	794261.411906	41.921101
3505.611600	794191.753241	41.926106
3505.249715	794118.823813	41.931111
3505.387256	794029.258367	41.936116
3505.617859	793964.383454	41.941120
3505.470082	793880.167980	41.946125
3505.696508	793811.510124	41.951130
3504.892327	793731.281488	41.956135
3505.526072	793660.295508	41.961140
3505.167960	793586.868733	41.966144
3505.098566	793505.877913	41.971149
3505.307148	793436.531630	41.976154
3505.077707	793363.523439	41.981159
3505.311111	793286.901331	41.986164
3504.900809	793216.230229	41.991168
3505.124967	793143.832789	41.996173
3505.283472	793079.256359	42.001178
3505.007100	793006.252198	42.006183
3504.933035	792930.708512	42.011188
3504.925640	792877.112738	42.016192
3504.975146	792799.926114	42.021197
3504.837807	792732.840625	42.026202
3505.021766	792678.622292	42.031207
3504.907331	792604.555609	42.036212
3504.257801	792535.292689	42.041216
3504.765292	792468.049341	42.046221
3504.423623	792412.441656	42.051226
3504.349518	792349.026854	42.056231
3504.701031	792282.298737	42.061236
3504.456017	792242.346536	42.066240
3504.580888	792173.935137	42.071245
3504.752271	792121.483342	42.076250
3504.516287	792044.040694	42.081255
3504.868215	791979.618885	42.086260
3504.505507	791926.860557	42.091264
3504.736236	791847.766615	42.096269
3504.535628	791796.307228	42.101274
3504.555062	791739.897755	42.106279
3504.551137	791675.826605	42.111284
3504.560017	791624.970222	42.116288
3504.279934	791540.306401	42.121293
3504.356694	791497.496232	42.126298
3503.920529	791442.535251	42.131303
3504.468881	791384.807409	42.136308
3504.031348	791330.288017	42.141312
3504.152730	791271.401142	42.146317
3504.156467	791231.598807	42.151322
3504.206500	791166.334841	42.156327
3504.297220	791120.964887	42.161332
3504.069328	791073.337575	42.166336
3504.159003	791017.156472	42.171341
3504.544599	790970.213651	42.176346
3504.433069	790908.708567	42.181351
3504.761159	790851.700636	42.186356
3504.086779	790797.265291	42.191360
3503.894901	790740.735245	42.196365
3504.194932	790675.032446	42.201370
3504.018411	790623.609709	42.206375
3503.695521	790570.539854	42.211380
3503.919052	790522.244768	42.216384
3504.027215	790465.122528	42.221389
3503.974845	790427.487236	42.226394
3503.948774	790381.640352	42.231399
3504.099851	790326.033392	42.236404
3504.299575	790276.954248	42.241408
3503.932010	790221.775914	42.246413
3504.218481	790170.421065	42.251418
3503.737014	790123.762907	42.256423
3503.747591	790069.356581	42.261428
3503.557777	790029.923408	42.266432
3503.362808	789990.146837	42.271437
3503.985438	789950.333665	42.276442
3503.631486	789904.537708	42.281447
3503.776956	789860.035328	42.286452
3503.663180	789810.414828	42.291456
3503.504770	789759.277733	42.296461
3503.654227	789727.650738	42.301466
3503.416603	789676.182052	42.306471
3503.736147	789620.050329	42.311476
3503.253691	789585.332078	42.316480
3503.131718	789541.609001	42.321485
3503.527704	789498.488442	42.326490
3503.418309	789467.345279	42.331495
3503.386089	789417.118794	42.336500
3502.862600	789393.366976	42.341504
3502.987362	789348.274993	42.346509
3503.264040	789314.364248	42.351514
3503.068407	789288.641168	42.356519
3503.125613	789246.754527	42.361524
3503.253318	789225.254176	42.366528
3503.520923	789177.040998	42.371533
3503.614763	789148.468041	42.376538
3503.402459	789114.735195	42.381543
3503.821515	789064.382735	42.386548
3503.352957	789012.848979	42.391552
3503.250524	788979.638084	42.396557
3503.212883	788949.365601	42.401562
3503.220209	788907.386872	42.406567
3503.339217	788865.143727	42.411572
3502.997729	788842.539795	42.416576
3502.921855	788805.293022	42.421581
3503.165006	788763.471220	42.426586
3503.313682	788724.220824	42.431591
3502.996884	788685.735065	42.436596
3503.106203	788654.257382	42.441600
3503.135843	788616.304056	42.446605
3503.188205	788585.671109	42.451610
3503.201364	788558.337987	42.456615
3503.299411	788506.756391	42.461620
3503.462143	788471.975582	42.466624
3503.358473	788442.596654	42.471629
3503.176922	788413.476221	42.476634
3503.244857	788377.186676	42.481639
3503.252059	788330.829512	42.486644
3503.139689	788288.866855	42.491648
3503.100787	788266.702837	42.496653
3502.847673	788225.008780	42.501658
3502.687409	788201.143984	42.506663
3503.217157	788164.089057	42.511668
3502.971658	788141.516246	42.516672
3503.143512	788105.306519	42.521677
3503.499376	788074.375585	42.526682
3502.867972	788032.791875	42.531687
3502.964578	787991.874575	42.536692
3502.762184	787967.917616	42.541696
3502.785473	787934.042047	42.546701
3502.842246	787904.880280	42.551706
3502.932420	787875.663730	42.556711
3503.035352	787849.296332	42.561716
3502.824672	787824.848641	42.566720
3502.569943	787787.232714	42.571725
3503.088271	787756.716103	42.576730
3502.409075	787725.904991	42.581735
3502.735547	787700.041008	42.586740
3502.761958	787676.438682	42.591744
3502.763656	787648.858149	42.596749
3502.806894	787627.809365	42.601754
3502.690648	787590.415405	42.606759
3502.570693	787561.576326	42.611764
3502.622541	787547.703764	42.616768
3502.675663	787519.180151	42.621773
3502.708041	787481.318664	42.626778
3502.531413	787465.615340	42.631783
3502.682954	787446.809737	42.636788
3502.520590	787410.799035	42.641792
3502.696522	787385.696181	42.646797
3503.174635	787361.969249	42.651802
3502.622683	787331.774615	42.656807
3502.748462	787293.945916	42.661812
3502.629277	787280.248504	42.666816
3502.638163	787244.061256	42.671821
3502.926752	787216.235135	42.676826
3502.758747	787200.185645	42.681831
3502.631580	787148.680500	42.686836
3502.780441	787139.806139	42.691840
3502.985597	787102.061683	42.696845
3502.801295	787069.937047	42.701850
3502.654737	787042.919432	42.706855
3502.910978	787012.246152	42.711860
3502.615350	786990.612133	42.716864
3502.414966	786961.980551	42.721869
3502.850864	786930.785652	42.726874
3502.918336	786922.268604	42.731879
3502.673710	786880.761965	42.736884
3502.564117	786873.404894	42.741888
3502.572797	786847.639346	42.746893
3502.662273	786815.566807	42.751898
3502.236789	786793.363555	42.756903
3502.423315	786767.863439	42.761908
3502.649589	786753.567254	42.766912
3502.575164	786726.192377	42.771917
3502.796364	786716.322190	42.776922
3502.343530	786673.914427	42.781927
3502.383832	786646.225328	42.786932
3502.440866	786630.039149	42.791937
3502.506473	786615.867494	42.796941
3502.517826	786579.528968	42.801946
3502.456313	786563.903040	42.806951
3502.780711	786534.003213	42.811956
3502.697430	786519.069161	42.816961
3502.617613	786498.234004	42.821965
3502.737330	786465.023983	42.826970
3502.584486	786441.987992	42.831975
3502.685136	786413.206283	42.836980
3502.702392	786392.059799	42.841985
3502.676282	786360.299290	42.846989
3502.763540	786331.912836	42.851994
3502.540909	786322.311902	42.856999
3502.787863	786281.900947	42.862004
3502.583766	786260.200466	42.867009
3502.321111	786232.313806	42.872013
3502.439751	786202.692353	42.877018
3502.364694	786200.737918	42.882023
3502.177138	786164.085837	42.887028
3502.301996	786158.312125	42.892033
3501.777725	786138.040861	42.897037
3502.192117	786119.532691	42.902042
3502.075020	786119.306229	42.907047
3502.449178	786090.330652	42.912052
3502.128564	786073.615337	42.917057
3502.142788	786054.779525	42.922061
3502.222367	786021.721583	42.927066
3502.013658	786023.968915	42.932071
3502.487257	785988.485559	42.937076
3502.111002	785981.712411	42.942081
3501.971026	785957.443379	42.947085
3502.206859	785949.536713	42.952090
3502.092064	785937.016194	42.957095
3502.023047	785924.930686	42.962100
3502.188917	785912.462244	42.967105
3501.849481	785878.931739	42.972109
3501.742397	785868.426010	42.977114
3501.874573	785872.436721	42.982119
3502.167921	785857.291726	42.987124
3501.933293	785830.972494	42.992129
3502.279139	785828.260170	42.997133
3502.084069	785795.492302	43.002138
3501.909299	785782.194580	43.007143
3501.945280	785769.206350	43.012148
3501.934911	785774.912576	43.017153
3502.289730	785744.906099	43.022157
3502.180959	785727.171558	43.027162
3501.831776	785717.541481	43.032167
3502.048747	785678.853234	43.037172
3501.813229	785679.974029	43.042177
3501.932612	785675.971186	43.047181
3502.089704	785668.323063	43.052186
3501.681734	785650.244202	43.057191
3502.021968	785639.074336	43.062196
3502.423727	785625.681359	43.067201
3502.156484	785608.661104	43.072205
3502.457238	785593.711042	43.077210
3502.126791	785575.914286	43.082215
3502.015841	785537.672711	43.087220
3502.084601	785546.120023	43.092225
3501.804843	785521.970895	43.097229
3502.177744	785489.353960	43.102234
3501.938968	785489.540942	43.107239
3501.905485	785486.890974	43.112244
3501.952899	785467.015416	43.117249
3501.690100	785460.223083	43.122253
3502.005018	785445.663804	43.127258
3501.625708	785441.890508	43.132263
3501.783874	785425.439061	43.137268
3501.815595	785408.467442	43.142273
3501.988175	785394.964251	43.147277
3502.307687	785387.141541	43.152282
3502.247391	785378.151920	43.157287
3501.876661	785364.639807	43.162292
3501.460378	785363.724921	43.167297
3501.915217	785355.683172	43.172301
3502.097142	785351.178059	43.177306
3501.801086	785324.326118	43.182311
3502.082937	785306.378657	43.187316
3501.838376	785311.091067	43.192321
3501.965555	785296.906664	43.197325
3501.912204	785274.784933	43.202330
3502.137988	785280.796908	43.207335
3502.172897	785244.644452	43.212340
3501.808233	785232.704834	43.217345
3501.804182	785222.968060	43.222349
3501.849980	785225.763872	43.227354
3501.718747	785201.294121	43.232359
3501.850008	785174.076152	43.237364
3501.889114	785175.594407	43.242369
3501.852130	785173.682598	43.247373
3502.014670	785156.147855	43.252378
3501.825568	785138.474270	43.257383
3501.887414	785129.021596	43.262388
3501.984413	785120.448364	43.267393
3501.901985	785108.462050	43.272397
3501.901288	785084.511383	43.277402
3501.726160	785091.327264	43.282407
3502.130997	785077.834402	43.287412
3502.003003	785047.806182	43.292417
3501.913336	785040.591485	43.297421
3502.176470	785022.302133	43.302426
3501.799288	785010.413386	43.307431
3502.058808	784994.337707	43.312436
3501.869313	784990.631266	43.317441
3501.810179	784988.034520	43.322445
3501.977981	784973.941151	43.327450
3501.872652	784948.384282	43.332455
3501.947360	784936.076707	43.337460
3502.007636	784935.525899	43.342465
3501.909519	784913.066155	43.347469
3502.249951	784894.419474	43.352474
3502.205723	784889.459506	43.357479
3502.218128	784868.161783	43.362484
3502.074777	784864.988679	43.367489
3502.178714	784845.249637	43.372493
3502.413679	784814.521288	43.377498
3501.887788	784812.689914	43.382503
3502.132806	784800.649150	43.387508
3502.357816	784778.480038	43.392513
3502.161614	784766.020066	43.397517
3502.198496	784738.619263	43.402522
3502.498854	784720.027914	43.407527
3502.601956	784708.403836	43.412532
3502.264590	784678.261009	43.417537
3502.236603	784670.543946	43.422541
3502.198258	784654.713306	43.427546
3502.074172	784643.224911	43.432551
3502.635094	784628.721829	43.437556
3502.202159	784599.873190	43.442561
3502.196424	784591.709722	43.447565
3502.173563	784556.005973	43.452570
3502.335509	784536.108975	43.457575
3502.209228	784533.818230	43.462580
3502.332888	784504.090575	43.467585
3502.298948	784496.915337	43.472589
3502.276853	784472.769418	43.477594
3502.121171	784450.120970	43.482599
3502.471292	784437.668808	43.487604
3502.483829	784418.779797	43.492609
3502.274040	784407.010030	43.497613
3502.362911	784371.286960	43.502618
3502.421209	784351.554081	43.507623
3502.297114	784336.818949	43.512628
3502.438286	784307.628641	43.517633
3502.337111	784304.153225	43.522637
3502.548717	784267.720821	43.527642
3502.036638	784265.837841	43.532647
3502.102736	784226.133720	43.537652
3502.063284	784234.157722	43.542657
3502.226102	784217.506002	43.547661
3502.396171	784180.735694	43.552666
3502.167243	784175.461349	43.557671
3502.101347	784161.257324	43.562676
3502.459681	784136.358997	43.567681
3502.225816	784120.952884	43.572685
3502.233906	784087.602695	43.577690
3501.944184	784084.748478	43.582695
3501.978284	784074.610365	43.587700
3501.988323	784047.112975	43.592705
3502.027738	784028.267699	43.597709
3502.202760	784021.500257	43.602714
3501.660184	784011.358668	43.607719
3501.896160	783993.120365	43.612724
3502.066787	783987.140623	43.617729
3502.102349	783983.593341	43.622733
3502.048462	783964.566514	43.627738
3501.859119	783954.760167	43.632743
3501.743387	783931.267302	43.637748
3502.036977	783933.039034	43.642753
3502.024750	783916.120319	43.647757
3502.237735	783894.885053	43.652762
3502.228706	783901.822263	43.657767
3501.988594	783878.595657	43.662772
3502.308161	783852.423826	43.667777
3502.025358	783859.307794	43.672781
3502.326930	783817.349129	43.677786
3501.924994	783820.465185	43.682791
3501.814539	783805.284013	43.687796
3502.242505	783783.816251	43.692801
3502.079244	783773.956171	43.697805
3501.861676	783758.644975	43.702810
3501.573760	783726.965131	43.707815
3501.841088	783718.952454	43.712820
3502.052671	783713.211689	43.717825
3502.035193	783719.904516	43.722829
3502.147322	783685.797481	43.727834
3502.116270	783662.830883	43.732839
3502.078776	783656.147294	43.737844
3502.327722	783638.151910	43.742849
3502.029770	783631.462010	43.747853
3502.086434	783629.534364	43.752858
3502.263309	783610.173447	43.757863
3502.327130	783584.682250	43.762868
3502.256853	783585.923714	43.767873
3501.833281	783547.132750	43.772877
3502.227263	783538.016808	43.777882
3502.345938	783530.520320	43.782887
3502.139850	783507.926399	43.787892
3502.383677	783494.752251	43.792897
3502.472911	783463.697806	43.797901
3502.572239	783448.333751	43.802906
3501.944812	783417.052808	43.807911
3501.913193	783381.246290	43.812916
3501.918843	783386.164697	43.817921
3502.037399	783378.520495	43.822925
3501.871347	783357.887197	43.827930
3501.872198	783359.313753	43.832935
3502.104486	783340.139754	43.837940
3502.039041	783338.625684	43.842945
3501.471087	783316.385922	43.847949
3501.781819	783307.185017	43.852954
3501.601363	783308.051135	43.857959
3501.410018	783295.735389	43.862964
3502.274817	783298.938169	43.867969
3501.578899	783282.720896	43.872973
3502.331904	783253.425540	43.877978
3501.923443	783254.034063	43.882983
3502.067156	783240.236432	43.887988
3502.147207	783218.529141	43.892993
3502.152316	783215.134077	43.897997
3502.370754	783195.420848	43.903002
3502.167946	783176.662437	43.908007
3502.168652	783164.609994	43.913012
3501.809271	783137.169982	43.918017
3502.146809	783121.274055	43.923021
3502.501473	783105.522854	43.928026
3502.206475	783082.942244	43.933031
3502.386650	783073.910131	43.938036
3502.286822	783067.088680	43.943041
3502.338355	783037.711218	43.948045
3502.277348	783023.602533	43.953050
3502.227821	782996.012555	43.958055
3502.142687	782992.041913	43.963060
3502.052689	782975.871725	43.968065
3502.185407	782954.597720	43.973069
3502.027164	782944.637286	43.978074
3502.034134	782941.684543	43.983079
3501.925371	782908.938491	43.988084
3502.391264	782889.036080	43.993089
3501.804377	782881.458355	43.998093
3502.077425	782848.796725	44.003098
3501.941119	782853.542095	44.008103
3501.383053	782838.826181	44.013108
3501.800876	782835.658133	44.018113
3502.021911	782829.619936	44.023117
3502.061979	782812.394842	44.028122
3501.720118	782794.937439	44.033127
3501.699709	782805.419705	44.038132
3501.895074	782784.134878	44.043137
3501.769338	782762.755291	44.048141
3501.984307	782743.730151	44.053146
3501.813904	782756.106664	44.058151
3501.739206	782735.997699	44.063156
3501.805538	782716.160628	44.068161
3501.716259	782718.143321	44.073165
3501.449252	782709.577986	44.078170
3501.606288	782714.078341	44.083175
3501.672106	782719.479259	44.088180
3502.054868	782690.832975	44.093185
3501.594331	782671.525338	44.098189
3501.931421	782663.155624	44.103194
3501.789786	782659.341696	44.108199
3501.953563	782657.543740	44.113204
3501.900222	782628.231084	44.118209
3501.919371	782618.240979	44.123213
3501.994443	782615.818057	44.128218
3502.362886	782593.864595	44.133223
3501.872810	782572.347666	44.138228
3501.903060	782564.126776	44.143233
3501.565092	782565.560101	44.148237
3501.896051	782524.081058	44.153242
3501.505431	782532.558381	44.158247
3501.852677	782534.567617	44.163252
3502.134599	782526.944804	44.168257
3501.774925	782521.149597	44.173261
3502.083819	782487.988452	44.178266
3501.810435	782489.411154	44.183271
3501.747704	782478.893162	44.188276
3502.196563	782463.272644	44.193281
3502.124566	782452.116560	44.198285
3501.832992	782441.636208	44.203290
3502.038888	782425.268451	44.208295
3501.391575	782408.795201	44.213300
3501.709355	782391.523359	44.218305
3501.779410	782398.006198	44.223309
3501.872082	782383.920147	44.228314
3501.774385	782400.614804	44.233319
3502.188752	782368.764109	44.238324
3502.404851	782361.397960	44.243329
3501.860462	782345.202806	44.248333
3502.075604	782311.564303	44.253338
3501.584036	782315.138554	44.258343
3502.090759	782314.907608	44.263348
3501.666150	782305.088564	44.268353
3501.670159	782273.354242	44.273357
3501.783555	782261.134129	44.278362
3501.587659	782269.087686	44.283367
3501.409591	782270.248730	44.288372
3501.814532	782263.441773	44.293377
3501.705982	782260.704580	44.298381
3502.102588	782223.148986	44.303386
3501.695544	782225.528556	44.308391
3501.521353	782220.489755	44.313396
3501.994373	782208.702319	44.318401
3501.692885	782209.982102	44.323405
3501.652069	782182.239979	44.328410
3502.066028	782167.313378	44.333415
3501.931361	782177.077368	44.338420
3501.916699	782147.215184	44.343425
3501.795387	782134.787516	44.348429
3501.943612	782117.739753	44.353434
3501.707822	782120.583156	44.358439
3502.006858	782116.056743	44.363444
3502.020149	782083.631248	44.368449
3501.719527	782075.119895	44.373453
3502.001742	782069.661403	44.378458
3501.986139	782052.640472	44.383463
3501.596248	782033.270285	44.388468
3501.838844	782029.786344	44.393473
3501.756906	782032.063224	44.398477
3501.962195	782019.876770	44.403482
3501.776752	782004.162939	44.408487
3501.869026	781990.026985	44.413492
3502.071118	781986.598898	44.418497
3501.605991	781974.571998	44.423501
3501.717600	781959.842379	44.428506
3501.357371	781933.037546	44.433511
3501.725674	781930.861308	44.438516
3501.918667	781928.172723	44.443521
3501.765939	781932.035762	44.448525
3501.942909	781922.313912	44.453530
3501.721020	781909.311996	44.458535
3501.973324	781892.098952	44.463540
3502.179499	781881.831012	44.468545
3501.974974	781868.284935	44.473549
3502.054472	781848.394112	44.478554
3502.119679	781850.154785	44.483559
3502.074622	781839.928167	44.488564
3502.119658	781807.348597	44.493569
3502.020845	781805.839700	44.498573
3502.230032	781790.355619	44.503578
3502.203767	781772.204115	44.508583
3501.771916	781759.334920	44.513588
3501.951564	781741.641454	44.518593
3501.802156	781729.709750	44.523597
3502.021756	781718.996536	44.528602
3502.020701	781720.374527	44.533607
3501.946280	781695.932709	44.538612
3502.101236	781678.144747	44.543617
3501.569624	781682.709977	44.548621
3501.971979	781670.687291	44.553626
3501.957210	781655.338219	44.558631
3501.685182	781642.639305	44.563636
3501.871044	781621.401829	44.568641
3501.805702	781623.971328	44.573645
3501.720877	781606.813138	44.578650
3501.376510	781587.286641	44.583655
3501.740836	781583.634824	44.588660
3501.912759	781567.861180	44.593665
3502.001748	781579.901748	44.598669
3501.899221	781561.516254	44.603674
3502.041961	781549.191698	44.608679
3501.801395	781554.053499	44.613684
3501.984620	781529.962319	44.618689
3501.851708	781516.846631	44.623693
3502.222106	781496.168850	44.628698
3501.675937	781495.717676	44.633703
3501.746655	781480.649383	44.638708
3501.682456	781485.728205	44.643713
3501.462072	781462.293743	44.648717
3501.726738	781438.090432	44.653722
3501.910311	781449.672788	44.658727
3501.794047	781431.879692	44.663732
3501.568416	781435.312153	44.668737
3501.622873	781427.922477	44.673741
3501.747049	781400.347000	44.678746
3501.617118	781398.695526	44.683751
3501.769021	781396.948422	44.688756
3501.968245	781383.187314	44.693761
3501.662962	781377.825075	44.698765
3501.893636	781350.330277	44.703770
3502.190541	781351.314817	44.708775
3502.012153	781351.983997	44.713780
3501.996931	781328.515307	44.718785
3501.575145	781324.205548	44.723789
3501.929936	781311.845661	44.728794
3501.604933	781309.291378	44.733799
3501.475960	781304.884169	44.738804
3502.044097	781282.697019	44.743809
3501.551637	781272.297262	44.748813
3501.680283	781261.106289	44.753818
3501.392941	781253.674322	44.758823
3501.414229	781250.226464	44.763828
3501.537444	781237.806182	44.768833
3501.341847	781243.349678	44.773837
3501.960926	781241.820826	44.778842
3501.788110	781226.546085	44.783847
3501.619092	781211.713550	44.788852
3501.979158	781196.252556	44.793857
3501.659885	781215.348382	44.798861
3501.591088	781181.406950	44.803866
3501.669752	781168.649437	44.808871
3501.232763	781162.915074	44.813876
3501.742439	781158.205750	44.818881
3501.624327	781165.065141	44.823885
3501.775189	781162.284800	44.828890
3501.658032	781169.980554	44.833895
3501.377665	781137.303946	44.838900
3501.426267	781110.084265	44.843905
3501.448682	781113.082359	44.848909
3501.510758	781117.304109	44.853914
3501.444183	781110.327707	44.858919
3501.436281	781114.905438	44.863924
3501.524775	781090.188701	44.868929
3501.587261	781108.139355	44.873933
3501.558970	781102.190000	44.878938
3501.652622	781104.881117	44.883943
3501.323958	781091.895316	44.888948
3501.653166	781067.089643	44.893953
3501.571826	781073.352568	44.898957
3501.569922	781071.778346	44.903962
3501.580576	781068.135321	44.908967
3501.440258	781061.023394	44.913972
3501.918273	781062.863887	44.918977
3501.724220	781053.349611	44.923981
3501.561488	781030.297917	44.928986
3501.637489	781024.183695	44.933991
3501.823969	781032.666120	44.938996
3501.798566	781028.536932	44.944001
3501.955094	781008.040616	44.949005
3501.499796	780993.845289	44.954010
3501.672921	780990.273879	44.959015
3501.823750	780984.934634	44.964020
3501.643790	780983.094471	44.969025
3501.463369	780989.127746	44.974029
3501.911312	780956.625609	44.979034
3501.820282	780938.433473	44.984039
3501.264899	780952.598787	44.989044
3501.663406	780938.902429	44.994049
3501.508319	780946.014161	44.999053
3501.679761	780935.209307	45.004058
3501.712072	780926.149666	45.009063
3501.684731	780919.412662	45.014068
3502.097545	780908.174338	45.019073
3501.675475	780913.755389	45.024077
3501.493403	780901.089562	45.029082
3501.869071	780901.126220	45.034087
3501.800890	780875.056702	45.039092
3502.043349	780862.320880	45.044097
3501.615622	780858.208655	45.049101
3501.901186	780863.328719	45.054106
3501.798683	780836.428157	45.059111
3501.710285	780816.857416	45.064116
3502.237754	780806.387403	45.069121
3501.976053	780809.678470	45.074125
3502.032253	780785.950210	45.079130
3501.926540	780770.761873	45.084135
3502.100256	780775.752793	45.089140
3502.234738	780758.654889	45.094145
3502.234123	780732.622940	45.099149
3502.119902	780724.128496	45.104154
3501.851714	780693.219449	45.109159
3502.219155	780688.434833	45.114164
3501.995902	780683.698301	45.119169
3501.900288	780654.187767	45.124173
3501.814506	780637.175069	45.129178
3502.351670	780636.151699	45.134183
3502.040181	780615.731366	45.139188
3501.931712	780592.324862	45.144193
3501.806530	780590.327941	45.149197
3502.164393	780585.052723	45.154202
3501.831218	780561.289443	45.159207
3501.739575	780545.655415	45.164212
3501.869799	780541.205046	45.169217
3501.670565	780554.869563	45.174221
3501.688346	780526.078001	45.179226
3502.019036	780510.768025	45.184231
3501.585060	780511.233320	45.189236
3501.510587	780495.350296	45.194241
3501.365743	780498.031712	45.199245
3501.800951	780491.021272	45.204250
3502.032131	780483.306254	45.209255
3501.616793	780476.731172	45.214260
3502.050247	780455.744774	45.219265
3501.828254	780451.057094	45.224269
3501.738930	780428.975637	45.229274
3501.876065	780416.010321	45.234279
3501.812057	780407.753297	45.239284
3501.797642	780404.261705	45.244289
3501.926377	780406.307542	45.249293
3502.106749	780371.533876	45.254298
3501.700332	780371.010386	45.259303
3501.527797	780367.052695	45.264308
3502.195750	780358.330559	45.269313
3501.944779	780353.844439	45.274317
3501.933944	780318.511461	45.279322
3501.849996	780328.072731	45.284327
3501.728608	780322.285710	45.289332
3501.594833	780310.152237	45.294337
3501.672116	780298.180831	45.299341
3502.031094	780283.062570	45.304346
3501.952896	780283.912194	45.309351
3501.785596	780278.870900	45.314356
3501.649772	780254.188265	45.319361
3501.764874	780238.076597	45.324365
3501.792106	780234.430423	45.329370
3501.643986	780232.289539	45.334375
3501.628752	780234.605207	45.339380
3501.945120	780215.556733	45.344385
3501.689107	780201.425449	45.349389
3501.827225	780190.231267	45.354394
3501.843266	780185.602633	45.359399
3501.605534	780184.214705	45.364404
3501.886985	780159.364587	45.369409
3501.243435	780148.938879	45.374413
3501.712979	780147.631300	45.379418
3502.145753	780138.110999	45.384423
3501.826755	780133.635947	45.389428
3501.574573	780117.289224	45.394433
3501.575937	780108.479733	45.399437
3501.780735	780098.012642	45.404442
3501.941353	780094.147568	45.409447
3501.428599	780102.106472	45.414452
3501.668576	780088.237770	45.419457
3501.423667	780061.849938	45.424461
3501.760610	780057.611297	45.429466
3501.857546	780046.522106	45.434471
3501.692460	780061.609157	45.439476
3501.796487	780050.863309	45.444481
3501.789360	780030.784910	45.449485
3501.818420	780010.995787	45.454490
3502.117713	779998.249091	45.459495
3501.813057	780011.833563	45.464500
3502.081970	779972.712473	45.469505
3501.684269	779962.245998	45.474509
3501.700017	779955.451786	45.479514
3502.201528	779957.239485	45.484519
3501.920277	779934.056180	45.489524
3501.823293	779930.430314	45.494529
3501.689558	779911.061459	45.499533
3501.762327	779911.148022	45.504538
3501.949245	779898.419662	45.509543
3501.608828	779888.238940	45.514548
3501.808036	779867.978457	45.519553
3501.886126	779869.786707	45.524557
3501.839721	779849.861927	45.529562
3501.905944	779834.101929	45.534567
3501.461954	779819.410267	45.539572
3501.983907	779817.946350	45.544577
3501.607670	779815.399969	45.549581
3501.717529	779816.366320	45.554586
3501.768567	779791.651332	45.559591
3501.671112	779792.651835	45.564596
3501.920811	779764.704953	45.569601
3501.822925	779782.340786	45.574605
3501.659576	779769.030079	45.579610
3501.814139	779742.378417	45.584615
3501.531273	779741.539223	45.589620
3501.846057	779725.541180	45.594625
3501.605519	779728.730810	45.599629
3501.537499	779720.030710	45.604634
3501.462124	779742.043254	45.609639
3501.460964	779715.860098	45.614644
3501.686192	779702.485263	45.619649
3501.366578	779698.945169	45.624653
3501.416666	779696.869912	45.629658
3501.714542	779691.160978	45.634663
3501.295482	779689.901255	45.639668
3501.607981	779685.518775	45.644673
3501.098534	779693.034621	45.649677
3501.612955	779685.370539	45.654682
3501.651726	779684.133838	45.659687
3501.213186	779682.385149	45.664692
3501.452762	779652.815331	45.669697
3501.708570	779650.509305	45.674701
3501.583645	779649.102691	45.679706
3502.037898	779638.347762	45.684711
3501.648707	779653.472573	45.689716
3501.505406	779630.659316	45.694721
3501.625712	779608.294745	45.699725
3501.620497	779600.322425	45.704730
3501.710491	779594.204695	45.709735
3501.533840	779604.963416	45.714740
3501.466966	779597.788736	45.719745
3501.741032	779594.889070	45.724749
3501.454017	779606.207366	45.729754
3501.797025	779581.689661	45.734759
3501.800660	779573.026800	45.739764
3501.921986	779551.400158	45.744769
3501.745558	779560.190179	45.749773
3501.842216	779564.850101	45.754778
3501.723871	779540.752779	45.759783
3501.884293	779526.748458	45.764788
3501.653861	779519.846733	45.769793
3501.778871	779532.426173	45.774797
3501.443193	779505.608304	45.779802
3501.494196	779487.143040	45.784807
3501.516945	779468.436290	45.789812
3501.285404	779394.399870	45.794817
3501.149738	779290.224321	45.799821
3501.008775	779120.042874	45.804826
3501.216664	778892.898771	45.809831
3500.611656	778606.221472	45.814836
3500.041858	778261.636412	45.819841
3500.155352	777894.424691	45.824845
3499.913124	777432.825668	45.829850
3499.533755	776925.283052	45.834855
3498.981879	776372.876407	45.839860
3498.700046	775769.416507	45.844865
3498.177656	775105.814767	45.849869
3498.319118	774384.122369	45.854874
3498.002493	773590.419292	45.859879
3496.974366	772760.046415	45.864884
3496.683203	771854.076123	45.869889
3496.217924	770903.083755	45.874893
3495.507040	769887.547973	45.879898
3494.789524	768810.656392	45.884903
3493.908085	767699.078659	45.889908
3493.351978	766513.324288	45.894913
3492.460315	765289.762117	45.899917
3491.346947	763988.306200	45.904922
3490.732312	762648.657363	45.909927
3489.510270	761256.571100	45.914932
3488.822355	759805.267810	45.919937
3487.697142	758296.207266	45.924941
3486.891728	756734.711447	45.929946
3485.761677	755115.325128	45.934951
3484.466866	753445.938451	45.939956
3483.450359	751711.330632	45.944961
3482.420244	749933.792621	45.949965
3480.947664	748108.672069	45.954970
3480.086331	746220.587033	45.959975
3478.537050	744279.943953	45.964980
3477.662820	742290.834169	45.969985
3476.083263	740256.617316	45.974989
3474.824278	738159.970054	45.979994
3473.764911	736011.656930	45.984999
3471.985744	733810.553177	45.990004
3470.494690	731569.131611	45.995009
3468.947995	729283.951109	46.000013
3467.409885	726933.015207	46.005018
3466.394545	724539.285936	46.010023
3464.626421	722099.469577	46.015028
3463.301709	719598.205177	46.020033
3461.289498	717065.446489	46.025037
3459.294543	714465.569177	46.030042
3457.984954	711836.980274	46.035047
3456.377832	709150.720076	46.040052
3454.214424	706433.756602	46.045057
3452.607297	703661.634169	46.050061
3450.761368	700850.144958	46.055066
3448.739078	697977.070645	46.060071
3447.103791	695072.208693	46.065076
3445.059229	692125.864463	46.070081
3442.837424	689135.278539	46.075085
3441.079185	686110.964168	46.080090
3439.277955	683018.911934	46.085095
3436.816106	679910.680843	46.090100
3435.135777	676733.793454	46.095105
3432.826806	673548.698639	46.100109
3430.952094	670294.376001	46.105114
3428.977992	666999.789234	46.110119
3426.794984	663661.581222	46.115124
3424.497197	660302.218556	46.120129
3421.944305	656880.959645	46.125133
3419.918829	653422.652793	46.130138
3417.708847	649923.390228	46.135143
3415.211828	646401.356656	46.140148
3413.053653	642837.932733	46.145153
3410.604251	639219.983724	46.150157
3407.839057	635585.906935	46.155162
3405.213769	631905.083866	46.160167
3402.770360	628194.551169	46.165172
3400.502249	624450.736168	46.170177
3397.785935	620661.442669	46.175181
3395.051548	616847.123163	46.180186
3392.850527	613001.557671	46.185191
3390.490656	609125.797070	46.190196
3387.850548	605178.190606	46.195201
3385.130145	601231.595734	46.200205
3382.320250	597241.485131	46.205210
3379.934451	593212.469615	46.210215
3376.872925	589171.646092	46.215220
3374.192599	585082.147179	46.220225
3371.393532	580965.951314	46.225229
3368.369702	576813.208100	46.230234
3366.045392	572625.157300	46.235239
3362.878176	568436.923642	46.240244
3359.861865	564191.460492	46.245249
3356.946931	559942.135720	46.250253
3354.076855	555657.986647	46.255258
3351.347032	551339.388561	46.260263
3348.259586	546995.941804	46.265268
3345.530427	542600.795658	46.270273
3342.501239	538212.102931	46.275277
3339.440233	533773.879767	46.280282
3336.637137	529322.857977	46.285287
3333.488676	524839.909212	46.290292
3330.593224	520335.133562	46.295297
3327.372248	515793.321431	46.300301
3324.192362	511239.523831	46.305306
3320.920039	506648.650834	46.310311
3317.819938	502046.342221	46.315316
3314.943991	497413.787998	46.320321
3311.675162	492780.589297	46.325325
3308.020830	488107.141478	46.330330
3305.262276	483400.770650	46.335335
3301.698834	478691.330564	46.340340
3298.420456	473946.097742	46.345345
3295.102514	469186.759147	46.350349
3291.696066	464412.782540	46.355354
3288.740874	459627.137396	46.360359
3285.181897	454821.956014	46.365364
3281.969333	449991.619525	46.370369
3278.236964	445145.412150	46.375373
3274.887126	440274.629379	46.380378
3271.432500	435387.889775	46.385383
3267.860602	430503.638829	46.390388
3264.434819	425600.085709	46.395393
3261.077361	420683.151192	46.400397
3257.554230	415742.332483	46.405402
3254.398903	410787.412390	46.410407
3250.487485	405821.062743	46.415412
3247.186263	400835.918188	46.420417
3243.606649	395850.187936	46.425421
3240.036959	390857.755515	46.430426
3236.352419	385829.411998	46.435431
3233.043425	380806.860892	46.440436
3229.519193	375782.097218	46.445441
3225.967899	370718.526561	46.450445
3222.152419	365646.139096	46.455450
3218.598889	360578.739924	46.460455
3214.827757	355496.039387	46.465460
3211.128900	350407.150527	46.470465
3207.451552	345298.091538	46.475469
3203.332280	340187.516813	46.480474
3200.112463	335071.954552	46.485479
3196.242448	329965.614466	46.490484
3192.363091	324835.308950	46.495489
3188.353361	319701.858119	46.500493
3184.567002	314572.899313	46.505498
3181.058857	309443.161746	46.510503
3177.297080	304319.029709	46.515508
3173.310916	299167.939034	46.520513
3169.347136	294019.926612	46.525517
3165.433758	288873.009860	46.530522
3162.108056	283721.989493	46.535527
3158.317994	278584.211348	46.540532
3154.199902	273417.971044	46.545537
3150.311879	268259.627942	46.550541
3146.393230	263098.052851	46.555546
3142.234485	257934.103352	46.560551
3138.332334	252783.317734	46.565556
3134.666573	247630.935701	46.570561
3130.782314	242488.143997	46.575565
3126.684480	237348.658787	46.580570
3122.877386	232194.578333	46.585575
3118.507166	227049.531398	46.590580
3114.567906	221906.485772	46.595585
3110.758573	216778.662710	46.600589
3106.688224	211647.621718	46.605594
3102.663866	206456.265977	46.610599
3098.718747	201308.846408	46.615604
3094.389941	196193.092014	46.620609
3090.037036	191075.663237	46.625613
3086.047243	185987.338276	46.630618
3082.143694	180896.083701	46.635623
3078.004049	175823.729707	46.640628
3073.543979	170749.020408	46.645633
3069.934674	165683.638335	46.650637
3065.713392	160633.831206	46.655642
3061.526264	155589.713837	46.660647
3056.907791	150560.712963	46.665652
3053.052438	145535.647159	46.670657
3048.830441	140533.037510	46.675661
3044.317860	135550.694065	46.680666
3040.216241	130551.987303	46.685671
3035.526442	125577.093539	46.690676
3031.158144	120628.511737	46.695681
3026.754608	115707.321195	46.700685
3022.098160	110810.284320	46.705690
3017.777934	105903.546299	46.710695
3012.990747	101044.565655	46.715700
3008.475700	96198.947065	46.720705
3004.048585	91367.109763	46.725709
2999.625654	86577.748164	46.730714
2995.270683	81808.871366	46.735719
2990.001817	77057.428372	46.740724
2985.625168	72339.702999	46.745729
2980.635312	67652.506481	46.750733
2975.629215	62993.192813	46.755738
2970.571674	58356.047697	46.760743
2965.530197	53781.226882	46.765748
2959.949240	49220.838735	46.770753
2954.838589	44731.290866	46.775757
2948.478740	40281.623224	46.780762
2942.500855	35883.881335	46.785767
2935.793784	31565.176199	46.790772
2924.619191	27436.220709	46.795777
2909.895006	23512.143687	46.800781
2895.314851	19750.758980	46.805786
2881.188731	16171.825664	46.810791
2867.496722	12832.948667	46.815796
2854.569652	9700.332158	46.820801
2842.311210	6797.520250	46.825805
2829.307413	4144.875977	46.830810
2816.075995	1726.049996	46.835815
2777.026350	284.842616	46.840820
2703.030306	241.016316	46.845825
2660.486355	237.561893	46.850829
2650.468780	238.980669	46.855834
2662.796879	229.172737	46.860839
2683.148226	237.624033	46.865844
2702.203295	230.838340	46.870849
2714.715530	223.586010	46.875853
2719.419016	231.913827	46.880858
2719.491333	219.242945	46.885863
2715.789756	225.214734	46.890868
2710.610405	224.981943	46.895873
2706.649788	233.744328	46.900877
2702.860870	229.897269	46.905882
2700.418107	221.285958	46.910887
2697.591450	225.790077	46.915892
2694.860632	226.947238	46.920897
2692.571888	214.634762	46.925901
2689.441359	223.563865	46.930906
2686.779801	216.408749	46.935911
2683.820969	214.507359	46.940916
2680.646223	202.388236	46.945921
2677.647890	205.825142	46.950925
2674.031739	216.243474	46.955930
2671.613257	212.138418	46.960935
2668.157364	210.848497	46.965940
2665.014621	205.781054	46.970945
2662.071967	198.914612	46.975949
2658.363908	205.484181	46.980954
2655.116208	195.654375	46.985959
2651.621155	208.168898	46.990964
2648.203239	207.215568	46.995969
2645.638127	199.817460	47.000973
2642.404837	205.891128	47.005978
2638.871724	199.355481	47.010983
2635.328278	195.786271	47.015988
2631.863695	202.681634	47.020993
2629.042161	205.516390	47.025997
2625.278223	208.607068	47.031002
2621.877976	199.094067	47.036007
2618.823421	203.164386	47.041012
2615.151657	200.879779	47.046017
2611.915942	203.165321	47.051021
2608.360985	208.659433	47.056026
2605.400314	211.252829	47.061031
2602.079227	197.042122	47.066036
2598.561972	196.121573	47.071041
2594.456670	188.415779	47.076045
2591.118926	198.604913	47.081050
2587.945185	195.192113	47.086055
2584.670046	194.792924	47.091060
2581.071702	196.071363	47.096065
2577.854152	184.672777	47.101069
2574.437289	191.927994	47.106074
2571.300784	198.239676	47.111079
2567.484601	203.583504	47.116084
2563.628420	198.188400	47.121089
2561.102596	180.440570	47.126093
2556.699184	192.315910	47.131098
2554.107860	184.774673	47.136103
2550.153338	193.257680	47.141108
2546.558262	193.097532	47.146113
2543.547465	175.692219	47.151117
2539.811557	184.873106	47.156122
2536.938034	176.818027	47.161127
2533.460913	183.855978	47.166132
2529.410513	190.039359	47.171137
2526.369787	182.961254	47.176141
2522.966169	190.097887	47.181146
2519.389866	180.326491	47.186151
2515.558289	179.447750	47.191156
2512.227505	180.367474	47.196161
2508.931007	182.016166	47.201165
2505.251127	179.840397	47.206170
2502.269622	177.918357	47.211175
2498.449571	178.998286	47.216180
2495.245392	183.393636	47.221185
2491.419481	180.990176	47.226189
2487.702711	187.421148	47.231194
2484.624463	176.989598	47.236199
2481.267626	186.996133	47.241204
2477.657587	186.801981	47.246209
2473.937214	166.428842	47.251213
2470.278553	182.407974	47.256218
2467.489567	177.223891	47.261223
2464.185888	179.543979	47.266228
2460.067027	175.825863	47.271233
2456.969452	178.950671	47.276237
2452.933338	185.368709	47.281242
2449.760460	182.545225	47.286247
2446.465502	172.209420	47.291252
2442.883626	187.097752	47.296257
2439.594972	172.003548	47.301261
2436.115802	167.784334	47.306266
2432.244827	165.868909	47.311271
2428.600301	174.768384	47.316276
2425.099299	174.383030	47.321281
2422.102408	177.701491	47.326285
2418.734495	172.673674	47.331290
2415.821854	172.579918	47.336295
2411.893869	169.907814	47.341300
2408.189304	162.268760	47.346305
2404.636303	170.056846	47.351309
2400.646669	174.715640	47.356314
2397.476834	176.151301	47.361319
2393.932206	164.609944	47.366324
2390.562478	172.079825	47.371329
2387.270764	170.626912	47.376333
2383.936008	177.559947	47.381338
2380.444132	175.010889	47.386343
2376.520693	175.477002	47.391348
2373.232179	167.449400	47.396353
2369.879012	168.544642	47.401357
2366.205312	172.403117	47.406362
2362.934814	161.003631	47.411367
2359.608577	175.413844	47.416372
2355.748867	175.212286	47.421377
2352.161672	173.032755	47.426381
2348.619227	171.337959	47.431386
2345.434870	162.131680	47.436391
2342.108489	164.909295	47.441396
2338.340273	172.973037	47.446401
2334.962109	167.106772	47.451405
2331.356021	173.228703	47.456410
2328.088380	161.019167	47.461415
2324.455669	162.177007	47.466420
2320.853917	166.241870	47.471425
2317.388243	170.038729	47.476429
2313.550989	171.168943	47.481434
2310.297033	166.663535	47.486439
2306.802712	164.666227	47.491444
2303.503133	161.865682	47.496449
2300.013551	157.972550	47.501453
2296.669469	163.106421	47.506458
2293.135680	162.023985	47.511463
2289.385435	165.436352	47.516468
2285.952733	174.186797	47.521473
2282.538177	167.458556	47.526477
2278.860264	168.039120	47.531482
2275.563389	162.138959	47.536487
2272.135760	172.983601	47.541492
2268.362664	172.879091	47.546497
2265.351493	165.569822	47.551501
2261.472825	174.223544	47.556506
2258.234991	165.119559	47.561511
2254.437678	164.024665	47.566516
2250.887757	163.038241	47.571521
2247.388362	166.551817	47.576525
2243.663038	176.486307	47.581530
2240.611406	166.908343	47.586535
2237.312652	161.073331	47.591540
2233.665479	163.517057	47.596545
2230.194732	152.128975	47.601549
2226.372677	166.858073	47.606554
2222.940254	157.427777	47.611559
2219.862961	156.434155	47.616564
2215.973750	148.257496	47.621569
2212.567365	160.109802	47.626573
2208.895172	162.634620	47.631578
2205.608275	163.239520	47.636583
2201.947227	164.736152	47.641588
2198.286206	163.132911	47.646593
2195.280851	164.577041	47.651597
2191.821277	168.835461	47.656602
2188.102905	160.544307	47.661607
2184.690281	161.508058	47.666612
2181.214760	156.895908	47.671617
2177.945870	158.947645	47.676621
2174.097690	164.140441	47.681626
2170.418795	164.272912	47.686631
2167.170304	165.647546	47.691636
2163.450895	154.767766	47.696641
2160.100931	154.952934	47.701645
2156.279898	166.171402	47.706650
2153.231190	170.922650	47.711655
2149.815938	161.414481	47.716660
2146.107624	166.200732	47.721665
2143.182852	149.646439	47.726669
2139.114107	158.321099	47.731674
2135.645828	160.240390	47.736679
2132.000763	162.810395	47.741684
2128.470341	172.609088	47.746689
2125.114460	162.761814	47.751693
2121.436670	155.539985	47.756698
2118.129011	154.046318	47.761703
2114.551255	155.261492	47.766708
2111.029178	155.889933	47.771713
2107.758379	140.250588	47.776717
2104.021732	153.949443	47.781722
2100.570024	160.370983	47.786727
2096.871162	153.225159	47.791732
2093.291376	156.125477	47.796737
2090.553868	143.782865	47.801741
2086.730197	147.080066	47.806746
2083.523313	155.214001	47.811751
2079.701567	146.081145	47.816756
2076.065266	155.214395	47.821761
2072.466691	158.984147	47.826765
2068.921081	158.921734	47.831770
2065.359634	164.224643	47.836775
2062.337206	152.799999	47.841780
2058.832787	157.226585	47.846785
2055.442388	147.441192	47.851789
2051.570989	162.613870	47.856794
2048.303149	157.832960	47.861799
2045.035175	161.938385	47.866804
2041.428438	159.447810	47.871809
2037.962986	151.052775	47.876813
2034.079849	148.853857	47.881818
2030.648006	152.870097	47.886823
2027.295674	153.618368	47.891828
2024.040118	158.095373	47.896833
2020.137274	148.803376	47.901837
2016.325984	148.355847	47.906842
2012.938054	145.147758	47.911847
2009.531508	142.601389	47.916852
2006.306971	153.951383	47.921857
2002.762829	147.332582	47.926861
1998.901411	159.487235	47.931866
1995.638152	145.602245	47.936871
1992.242449	147.729241	47.941876
1988.402161	145.508383	47.946881
1985.293014	138.733581	47.951885
1981.724035	148.221882	47.956890
1978.235142	153.224082	47.961895
1974.726522	145.985681	47.966900
1971.178266	155.990109	47.971905
1967.974328	141.144776	47.976909
1964.058529	153.177982	47.981914
1960.364366	149.475644	47.986919
1956.743689	151.199258	47.991924
1953.669838	156.290754	47.996929
1950.323819	148.666324	48.001933
1946.739579	153.941667	48.006938
1943.357513	151.079331	48.011943
1939.305756	155.049004	48.016948
1935.827459	148.227683	48.021953
1932.805338	146.044532	48.026957
1929.133009	144.857960	48.031962
1925.870662	141.830658	48.036967
1922.292900	142.051444	48.041972
1918.885654	152.949363	48.046977
1915.291111	154.165921	48.051981
1911.341712	147.654677	48.056986
1908.047177	135.395576	48.061991
1904.844404	140.309952	48.066996
1901.094622	145.933462	48.072001
1897.644307	140.540863	48.077005
1894.143621	146.172314	48.082010
1890.512410	141.480936	48.087015
1886.937372	126.854842	48.092020
1883.353987	139.536665	48.097025
1880.206536	130.506194	48.102029
1876.509017	133.943693	48.107034
1873.353074	138.363672	48.112039
1870.123687	143.813039	48.117044
1866.303536	144.189075	48.122049
1862.537160	142.297550	48.127053
1859.071969	137.738528	48.132058
1855.575727	133.933254	48.137063
1852.064851	142.688059	48.142068
1848.417233	140.068086	48.147073
1845.265261	153.296557	48.152077
1841.626912	142.845110	48.157082
1838.424677	143.435413	48.162087
1834.399883	127.744149	48.167092
1830.568512	139.207825	48.172097
1827.766265	136.647086	48.177101
1823.957263	134.016263	48.182106
1820.783717	136.063172	48.187111
1817.274017	144.901263	48.192116
1814.044691	149.712915	48.197121
1810.518310	131.594314	48.202125
1806.460279	139.278299	48.207130
1803.195393	135.318167	48.212135
1799.677727	134.135052	48.217140
1795.834919	124.829459	48.222145
1792.548605	127.113316	48.227149
1789.223392	139.226134	48.232154
1785.304973	129.824891	48.237159
1782.486419	137.762056	48.242164
1778.375903	132.765452	48.247169
1775.405922	118.728540	48.252173
1771.593070	135.001740	48.257178
1767.944985	128.010233	48.262183
1764.587375	126.400470	48.267188
1760.507368	136.024471	48.272193
1757.434569	131.333969	48.277197
1754.319092	141.111380	48.282202
1750.524133	142.950077	48.287207
1747.284151	139.163250	48.292212
1743.622370	141.743297	48.297217
1740.182814	134.260903	48.302221
1736.482230	145.499509	48.307226
1732.689823	137.151204	48.312231
1729.488836	129.546876	48.317236
1726.007363	142.724769	48.322241
1722.924496	139.477048	48.327245
1718.792187	139.991389	48.332250
1715.575146	125.869974	48.337255
1712.537316	131.100044	48.342260
1708.728439	131.756170	48.347265
1705.544603	121.606898	48.352269
1701.517006	131.084450	48.357274
1697.904618	136.954321	48.362279
1694.075188	133.255216	48.367284
1690.585623	136.529839	48.372289
1687.350091	131.216065	48.377293
1684.155198	132.553943	48.382298
1680.375168	129.390697	48.387303
1676.723048	127.524226	48.392308
1673.658586	130.124823	48.397313
1670.312226	123.347499	48.402317
1666.836006	128.843097	48.407322
1662.942958	138.584380	48.412327
1659.968988	138.753216	48.417332
1656.232853	134.676957	48.422337
1652.822354	121.612468	48.427341
1648.836633	128.087670	48.432346
1645.043990	134.289203	48.437351
1641.873449	133.121302	48.442356
1638.430812	129.146979	48.447361
1635.375730	124.239131	48.452365
1631.819455	138.765625	48.457370
1627.718649	134.729037	48.462375
1624.570030	118.281276	48.467380
1620.794229	132.104254	48.472385
1617.373219	118.598154	48.477389
1613.763304	130.561280	48.482394
1610.784064	127.549868	48.487399
1607.255850	121.547064	48.492404
1603.696971	142.067292	48.497409
1600.241238	127.325901	48.502413
1596.234187	116.042020	48.507418
1592.715881	124.360693	48.512423
1588.998441	117.342955	48.517428
1585.809482	128.355507	48.522433
1582.607985	128.183568	48.527437
1579.273833	129.548814	48.532442
1575.844784	127.412949	48.537447
1571.903382	113.268904	48.542452
1568.315940	132.005861	48.547457
1564.911073	118.255812	48.552461
1561.382028	121.561771	48.557466
1557.684245	126.148833	48.562471
1554.181895	128.901062	48.567476
1550.776086	128.334677	48.572481
1547.667393	126.520071	48.577485
1543.858642	122.941261	48.582490
1540.145009	130.843990	48.587495
1536.958125	127.955967	48.592500
1533.217561	132.782048	48.597505
1529.979247	122.383083	48.602509
1526.244762	123.369570	48.607514
1522.915279	123.917279	48.612519
1519.579587	118.676853	48.617524
1515.843474	129.056464	48.622529
1512.379629	118.238043	48.627533
1508.870152	111.567349	48.632538
1505.677147	130.061644	48.637543
1502.063746	120.215620	48.642548
1498.290827	132.608120	48.647553
1494.772075	125.444680	48.652557
1491.168335	132.590740	48.657562
1487.665033	134.091777	48.662567
1484.660573	123.234749	48.667572
1481.117781	125.793114	48.672577
1477.349025	125.949549	48.677581
1474.044770	123.278638	48.682586
1470.640445	133.796883	48.687591
1466.784675	126.400012	48.692596
1462.880044	134.438876	48.697601
1459.745977	121.423104	48.702605
1456.384978	127.680163	48.707610
1452.736025	133.318806	48.712615
1449.827806	124.329395	48.717620
1445.850216	125.157546	48.722625
1442.477648	125.934089	48.727629
1438.951675	124.545742	48.732634
1435.271547	121.497858	48.737639
1431.764267	114.359994	48.742644
1428.054186	121.776192	48.747649
1424.850209	111.706474	48.752653
1421.569758	128.569408	48.757658
1416.977653	129.367190	48.762663
1414.276815	115.214343	48.767668
1410.579708	119.525612	48.772673
1407.378011	110.018767	48.777677
1404.080799	124.375991	48.782682
1400.598863	123.917549	48.787687
1397.107668	122.795385	48.792692
1392.939370	128.826500	48.797697
1389.835876	123.300087	48.802701
1386.342361	128.184120	48.807706
1382.576856	116.803987	48.812711
1379.410125	116.833092	48.817716
1375.657185	125.872604	48.822721
1372.078992	123.683225	48.827725
1368.398644	125.557364	48.832730
1365.153318	127.672548	48.837735
1361.865311	118.976336	48.842740
1358.375051	125.548276	48.847745
1355.302730	119.610956	48.852749
1351.514639	128.335743	48.857754
1347.214635	119.696570	48.862759
1344.254327	119.740258	48.867764
1340.375402	108.492041	48.872769
1337.203639	106.755527	48.877773
1333.476905	114.333451	48.882778
1330.101739	132.322937	48.887783
1326.787542	121.771066	48.892788
1323.163540	119.188033	48.897793
1319.866762	106.313657	48.902797
1316.388669	113.948319	48.907802
1312.697653	113.640750	48.912807
1309.228884	104.868257	48.917812
1305.432224	120.029729	48.922817
1302.484872	120.063600	48.927821
1299.003073	131.498205	48.932826
1295.494340	119.552562	48.937831
1291.990452	116.524997	48.942836
1288.165535	112.776751	48.947841
1284.559987	121.762968	48.952845
1281.165325	123.929772	48.957850
1277.628999	133.194626	48.962855
1274.287914	125.820655	48.967860
1270.382118	125.710656	48.972865
1267.283712	123.521161	48.977869
1263.792945	113.754791	48.982874
1260.172230	124.295015	48.987879
1256.806882	112.323268	48.992884
1253.222485	124.536262	48.997889
1249.693111	110.774613	49.002893
1246.212233	126.000601	49.007898
1242.696309	116.657887	49.012903
1239.602349	115.940536	49.017908
1235.412659	120.701196	49.022913
1231.982886	118.528040	49.027917
1228.647948	121.226346	49.032922
1225.184501	122.876811	49.037927
1221.944643	112.968714	49.042932
1217.723939	115.069755	49.047937
1214.830702	115.493111	49.052941
1211.195710	116.570285	49.057946
1207.558635	120.757794	49.062951
1204.191357	119.496590	49.067956
1200.805194	115.140453	49.072961
1197.236286	111.144792	49.077965
1193.927198	117.918048	49.082970
1190.044591	111.227741	49.087975
1186.601350	101.724298	49.092980
1182.841251	121.047083	49.097985
1179.357909	127.218790	49.102989
1176.135921	121.308241	49.107994
1172.847401	126.266757	49.112999
1168.917369	122.751696	49.118004
1165.297684	113.474800	49.123009
1162.021900	107.794729	49.128013
1158.987384	109.094426	49.133018
1154.969149	120.683242	49.138023
1151.930713	120.717810	49.143028
1148.009743	122.006097	49.148033
1144.338877	115.128929	49.153037
1140.883309	118.110408	49.158042
1137.324009	111.515931	49.163047
1133.881716	106.958071	49.168052
1130.308647	119.834784	49.173057
1126.877468	108.921535	49.178061
1123.465506	114.919285	49.183066
1120.443136	111.346954	49.188071
1117.112946	105.550990	49.193076
1113.060478	116.344276	49.198081
1109.374103	113.039817	49.203085
1105.981804	112.716983	49.208090
1102.431590	120.080496	49.213095
1099.516083	104.135636	49.218100
1095.455086	109.843154	49.223105
1092.061909	113.024199	49.228109
1088.310237	113.639546	49.233114
1084.778313	125.137062	49.238119
1081.769545	109.831021	49.243124
1077.678360	107.639579	49.248129
1074.367695	103.349186	49.253133
1071.283318	103.188733	49.258138
1067.084761	113.484061	49.263143
1064.124042	110.270954	49.268148
1060.422392	114.975012	49.273153
1056.779831	113.894689	49.278157
1053.426935	109.985289	49.283162
1049.844264	112.278743	49.288167
1046.669372	107.228187	49.293172
1042.959615	115.142923	49.298177
1039.339144	116.132351	49.303181
1036.058209	112.029944	49.308186
1032.212975	114.989679	49.313191
1029.467268	106.103994	49.318196
1025.784445	118.376140	49.323201
1021.796691	107.329121	49.328205
1018.388387	108.309181	49.333210
1014.598419	123.762579	49.338215
1011.516498	117.785387	49.343220
1008.003740	126.171168	49.348225
1004.511686	114.045871	49.353229
1001.191488	106.238963	49.358234
997.604356	106.320389	49.363239
994.417169	103.526117	49.368244
990.229850	108.406685	49.373249
986.726097	117.756249	49.378253
983.143610	104.831289	49.383258
979.985536	118.813762	49.388263
976.470782	109.523609	49.393268
972.734317	114.432945	49.398273
969.352540	110.039510	49.403277
966.041464	109.799429	49.408282
962.404200	114.581203	49.413287
959.138472	106.311895	49.418292
955.484113	113.148768	49.423297
951.849181	111.681591	49.428301
948.331495	110.421477	49.433306
945.052484	117.704369	49.438311
941.605774	110.489806	49.443316
937.587887	122.832213	49.448321
934.458953	111.229975	49.453325
930.836428	109.433022	49.458330
927.196166	126.283294	49.463335
923.782531	111.030583	49.468340
920.029872	115.240967	49.473345
916.730492	105.596234	49.478349
913.497766	112.935128	49.483354
909.653323	105.791784	49.488359
906.461697	89.706876	49.493364
902.768405	102.358845	49.498369
899.531102	108.525068	49.503373
896.070245	105.829703	49.508378
892.368616	117.014055	49.513383
888.964374	102.999852	49.518388
885.476673	98.160465	49.523393
881.912324	104.049405	49.528397
878.350379	96.144075	49.533402
874.534771	107.100902	49.538407
871.449181	102.098834	49.543412
867.433211	112.861150	49.548417
864.274757	105.574965	49.553421
861.112507	107.653177	49.558426
857.187725	108.877834	49.563431
854.010986	106.651160	49.568436
850.466336	108.679559	49.573441
846.881778	108.117591	49.578445
843.544399	98.034730	49.583450
839.572649	110.105350	49.588455
836.067646	105.251089	49.593460
832.363011	105.769031	49.598465
829.337960	109.405585	49.603469
825.913786	107.591130	49.608474
822.437038	107.631336	49.613479
818.921235	107.483737	49.618484
815.189071	98.814828	49.623489
811.556506	106.378132	49.628493
808.167577	102.343011	49.633498
804.902492	110.957406	49.638503
801.400691	100.711212	49.643508
797.838054	117.035882	49.648513
794.586784	100.844567	49.653517
791.001801	98.190576	49.658522
786.826145	113.643224	49.663527
783.533093	105.301282	49.668532
779.766139	107.071639	49.673537
776.763207	112.396733	49.678541
773.714413	95.945286	49.683546
769.898784	114.580957	49.688551
766.175347	97.175030	49.693556
762.754992	107.329765	49.698561
759.383316	104.080487	49.703565
755.386354	99.262431	49.708570
752.067372	99.872312	49.713575
749.101218	105.319201	49.718580
745.101253	106.533943	49.723585
741.719816	110.103996	49.728589
738.268803	112.966921	49.733594
734.425488	103.434816	49.738599
730.834802	106.825245	49.743604
727.528144	113.668044	49.748609
724.260231	102.914354	49.753613
721.297299	103.240315	49.758618
717.145052	99.866224	49.763623
713.491624	108.994270	49.768628
709.629994	99.214325	49.773633
706.360378	101.808655	49.778637
703.465103	110.298185	49.783642
700.044776	108.351454	49.788647
696.711892	106.327736	49.793652
692.493289	97.070546	49.798657
689.100915	101.313296	49.803661
685.507591	104.040615	49.808666
681.897120	94.583652	49.813671
678.777996	97.707593	49.818676
675.063926	104.971480	49.823681
671.497067	107.603178	49.828685
668.334255	103.695153	49.833690
664.463246	102.453985	49.838695
661.324438	98.887004	49.843700
657.730217	102.248949	49.848705
654.009690	103.969186	49.853709
650.965219	102.039432	49.858714
647.026371	115.463518	49.863719
643.481830	111.260423	49.868724
640.094313	112.326821	49.873729
636.587573	109.511217	49.878733
633.151354	92.824426	49.883738
629.251240	108.540628	49.888743
626.213314	101.840326	49.893748
622.457361	109.115401	49.898753
618.896402	99.815253	49.903757
615.516150	100.693803	49.908762
611.898062	111.568999	49.913767
608.705989	103.865368	49.918772
604.953491	110.006508	49.923777
601.516538	104.037862	49.928781
598.639046	98.335731	49.933786
594.666677	105.608283	49.938791
591.191929	96.387147	49.943796
587.302964	113.457768	49.948801
583.649624	110.451730	49.953805
580.934428	107.252760	49.958810
577.196057	111.314160	49.963815
573.443354	97.837791	49.968820
569.811647	99.155879	49.973825
566.093345	98.146451	49.978829
563.205996	101.398202	49.983834
559.552387	104.699170	49.988839
556.334025	104.375217	49.993844
552.576622	98.393430	49.998849
549.136912	102.994593	50.003853
545.625148	98.123665	50.008858
541.660685	104.558821	50.013863
538.294094	100.807056	50.018868
535.041885	90.599035	50.023873
531.655055	97.545623	50.028877
528.222322	96.693268	50.033882
524.281215	103.072977	50.038887
521.154385	97.882959	50.043892
517.454197	94.709290	50.048897
513.612024	95.733448	50.053901
510.358100	98.916726	50.058906
506.926979	111.628759	50.063911
503.840269	98.612078	50.068916
500.329241	104.274656	50.073921
496.761855	119.119973	50.078925
492.922298	98.165796	50.083930
489.036922	117.168755	50.088935
485.867540	104.154192	50.093940
482.668521	98.058117	50.098945
479.011655	105.218039	50.103949
475.398022	97.222446	50.108954
471.414942	90.175898	50.113959
468.420770	91.972186	50.118964
465.091289	95.604621	50.123969
461.369727	93.063553	50.128973
457.838779	95.199103	50.133978
454.363910	102.210190	50.138983
451.108880	89.584805	50.143988
447.635761	91.272968	50.148993
443.707020	99.643544	50.153997
440.298877	95.397226	50.159002
437.015189	117.643111	50.164007
433.204254	99.826576	50.169012
429.894723	95.062403	50.174017
426.463094	100.752250	50.179021
422.814051	84.766806	50.184026
419.679999	97.812676	50.189031
416.152214	90.545633	50.194036
412.221803	105.742174	50.199041
408.953355	99.795531	50.204045
405.452062	98.619726	50.209050
401.989171	106.528906	50.214055
398.642561	89.147046	50.219060
394.928031	88.383639	50.224065
391.288457	97.133360	50.229069
387.928394	96.299067	50.234074
383.877763	105.163958	50.239079
380.709114	96.726532	50.244084
377.363856	87.205637	50.249089
373.800429	96.421469	50.254093
370.332305	85.734826	50.259098
366.370704	88.556691	50.264103
363.283532	83.620469	50.269108
359.966890	93.291089	50.274113
356.467244	93.865309	50.279117
353.037665	83.662240	50.284122
349.691057	95.558380	50.289127
346.434086	83.955472	50.294132
342.550289	91.862385	50.299137
338.760058	87.930134	50.304141
335.176800	86.058273	50.309146
331.537706	96.655190	50.314151
328.102141	95.326603	50.319156
324.768098	88.608008	50.324161
320.853537	99.122680	50.329165
317.983127	99.771437	50.334170
314.390016	91.758552	50.339175
311.033458	85.040036	50.344180
307.469132	95.646216	50.349185
303.456361	83.610198	50.354189
300.136532	94.443446	50.359194
296.258725	88.483892	50.364199
293.318863	91.122693	50.369204
289.847459	91.896502	50.374209
286.178819	98.235270	50.379213
282.817887	90.362418	50.384218
279.434093	96.458196	50.389223
275.806201	87.736120	50.394228
272.091442	88.356186	50.399233
268.415767	102.739109	50.404237
265.240143	94.880440	50.409242
261.310514	98.031335	50.414247
258.389957	93.747974	50.419252
254.989923	96.749220	50.424257
251.345025	93.181620	50.429261
248.105172	85.671181	50.434266
244.218937	100.360108	50.439271
240.574630	100.082220	50.444276
236.990212	89.695455	50.449281
233.610029	91.068657	50.454285
230.047250	86.777571	50.459290
226.716578	87.464134	50.464295
223.235579	80.566059	50.469300
219.915847	85.964035	50.474305
215.949374	96.697769	50.479309
213.005229	95.160390	50.484314
209.090211	94.942935	50.489319
205.957741	82.167533	50.494324
202.614267	79.331721	50.499329
198.506008	90.533728	50.504333
195.384587	85.591613	50.509338
191.622810	84.107554	50.514343
188.064891	86.893112	50.519348
184.570941	97.312703	50.524353
180.937679	87.999046	50.529357
177.691233	79.433425	50.534362
174.047129	84.216818	50.539367
170.493346	88.322515	50.544372
166.957813	88.205168	50.549377
163.631963	104.228410	50.554381
160.317932	87.435547	50.559386
156.548970	88.122251	50.564391
153.267278	85.451569	50.569396
149.932851	85.501274	50.574401
145.958969	85.682291	50.579405
142.717948	84.926920	50.584410
139.137483	95.336063	50.589415
135.556184	93.074695	50.594420
132.202683	92.541640	50.599425
128.352419	79.432555	50.604429
125.297970	83.227081	50.609434
121.338480	90.898890	50.614439
118.261142	92.210369	50.619444
114.477049	92.667361	50.624449
110.663201	91.086096	50.629453
107.800760	81.238953	50.634458
104.338440	89.669960	50.639463
100.829328	82.910482	50.644468
97.232617	94.383673	50.649473
93.355929	92.839440	50.654477
89.907650	88.746266	50.659482
86.454181	90.708695	50.664487
82.998310	85.884455	50.669492
79.497117	90.466307	50.674497
75.709635	103.444965	50.679501
72.627908	91.606186	50.684506
69.247193	93.991677	50.689511
65.533128	88.642344	50.694516
62.187138	94.484644	50.699521
58.728438	99.811940	50.704525
55.182926	87.095018	50.709530
51.367297	91.849009	50.714535
47.908065	91.297264	50.719540
44.378967	88.845599	50.724545
40.868531	99.077770	50.729549
37.756419	99.784647	50.734554
34.157273	93.695064	50.739559
30.390644	92.581965	50.744564
26.968328	87.170929	50.749569
23.352849	88.311719	50.754573
20.210198	83.133177	50.759578
16.275364	87.829835	50.764583
13.274684	96.521412	50.769588
9.742500	88.363499	50.774593
6.321218	95.747541	50.779597
2.766843	81.553069	50.784602