Thu Jun 16 18:07:51 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.625063	87.629059	0.000000
-0.608260	112.621524	0.005005
-0.602569	112.343074	0.010010
-0.293573	100.080653	0.015014
-0.824954	101.987994	0.020019
-0.511942	93.210536	0.025024
-0.854448	88.715353	0.030029
-1.041831	66.430140	0.035034
-0.914027	75.407443	0.040038
-1.733965	64.725523	0.045043
-1.678649	55.929209	0.050048
-2.097249	49.656107	0.055053
-2.262438	33.302214	0.060058
-2.395683	22.779825	0.065062
-3.173387	12.876360	0.070067
-3.167731	8.184166	0.075072
-3.784697	9.945422	0.080077
-4.142854	5.886934	0.085082
-4.497020	1.844460	0.090086
-4.911202	-0.266778	0.095091
-4.529617	-9.916475	0.100096
-5.071967	2.889362	0.105101
-5.742323	-0.892399	0.110106
-5.485339	-1.671714	0.115110
-6.087502	6.382798	0.120115
-6.164615	-0.500864	0.125120
-6.403308	-4.047239	0.130125
-7.552109	-6.708131	0.135130
-7.108725	-5.370026	0.140134
-7.444205	-1.351387	0.145139
-7.777656	-6.146964	0.150144
-7.966270	-1.672044	0.155149
-8.069330	-0.821955	0.160154
-7.981934	-8.781704	0.165158
-8.041460	-2.756536	0.170163
-7.973613	-3.746399	0.175168
-9.173519	5.649558	0.180173
-9.708292	1.892548	0.185178
-9.290342	-6.410791	0.190182
-9.339704	-3.661678	0.195187
-9.801774	-0.822755	0.200192
-10.447361	1.596034	0.205197
-10.549874	7.362236	0.210202
-10.757463	3.588744	0.215206
-11.060849	13.538880	0.220211
-11.168688	10.469877	0.225216
-11.172056	1.904874	0.230221
-11.789321	13.096665	0.235226
-12.302703	-0.090419	0.240230
-12.563885	1.422820	0.245235
-12.376837	4.514960	0.250240
-12.603981	11.553896	0.255245
-12.548454	3.709013	0.260250
-12.937388	-0.899126	0.265254
-13.700837	6.909356	0.270259
-14.056729	2.640656	0.275264
-13.906437	4.643300	0.280269
-14.292263	3.943675	0.285274
-14.038874	8.910061	0.290278
-15.163367	8.416658	0.295283
-15.600736	-4.135703	0.300288
-15.439518	3.001042	0.305293
-15.546174	-6.642457	0.310298
-15.296460	-3.128564	0.315302
-15.767817	3.919354	0.320307
-15.989882	1.674259	0.325312
-16.350310	5.881411	0.330317
-17.141137	9.899831	0.335322
-17.075399	6.677444	0.340326
-17.144878	3.227312	0.345331
-16.840048	-0.534769	0.350336
-17.609175	8.566152	0.355341
-18.121926	8.804308	0.360346
-18.312763	1.354412	0.365350
-18.409791	8.386051	0.370355
-18.009544	1.673692	0.375360
-19.188504	5.917259	0.380365
-19.382694	3.548579	0.385370
-19.779941	0.715246	0.390374
-20.088688	6.372972	0.395379
-19.720848	-0.046252	0.400384
-19.866398	4.908220	0.405389
-20.660931	3.722680	0.410394
-21.118588	-1.034712	0.415398
-21.766649	3.923485	0.420403
-21.653900	-8.011240	0.425408
-21.597785	0.153499	0.430413
-21.518685	9.536588	0.435418
-21.472785	-5.097160	0.440422
-21.780384	10.627975	0.445427
-22.431241	-8.561669	0.450432
-22.946609	-4.334835	0.455437
-23.138665	-5.463668	0.460442
-23.048280	-4.250135	0.465446
-22.997286	12.950623	0.470451
-23.632109	5.836719	0.475456
-24.765316	0.461311	0.480461
-24.935788	8.736307	0.485466
-24.762604	7.615383	0.490470
-24.937861	11.018673	0.495475
-25.079072	-6.542239	0.500480
-25.273414	4.407993	0.505485
-25.087692	9.807511	0.510490
-25.007821	5.899007	0.515494
-25.931155	1.190553	0.520499
-26.092605	-3.565277	0.525504
-26.408070	8.780528	0.530509
-26.794816	16.535642	0.535514
-27.537148	10.623863	0.540518
-27.896177	14.981532	0.545523
-27.953168	4.419328	0.550528
-27.937910	5.909574	0.555533
-27.812929	4.777774	0.560538
-27.550413	3.539190	0.565542
-28.087987	8.902363	0.570547
-28.760415	4.252876	0.575552
-29.279035	11.523282	0.580557
-29.586970	16.615088	0.585562
-29.821135	8.491035	0.590566
-29.885759	6.942771	0.595571
-29.622430	2.553982	0.600576
-29.871068	5.832957	0.605581
-30.711139	-8.890947	0.610586
-31.033564	0.615909	0.615590
-31.303702	-2.118266	0.620595
-31.490839	-0.797704	0.625600
-31.623839	13.862203	0.630605
-31.475830	8.135265	0.635610
-31.641610	5.801846	0.640614
-32.225782	6.835329	0.645619
-32.756326	10.498196	0.650624
-32.844412	14.519857	0.655629
-32.984483	15.973128	0.660634
-33.000219	0.953756	0.665638
-33.945820	7.405936	0.670643
-34.207780	5.365535	0.675648
-34.497527	7.471384	0.680653
-34.618636	10.177899	0.685658
-34.499795	13.558237	0.690662
-34.996903	10.905865	0.695667
-34.675759	-1.677236	0.700672
-34.421682	10.492070	0.705677
-35.090982	8.798477	0.710682
-35.805024	5.370022	0.715686
-36.014673	14.333796	0.720691
-36.188365	10.280046	0.725696
-36.709925	4.178970	0.730701
-37.813245	4.048282	0.735706
-36.652512	-2.977100	0.740710
-37.447694	6.510021	0.745715
-37.960579	8.958283	0.750720
-38.031658	8.583705	0.755725
-38.186506	10.427923	0.760730
-38.067386	4.451329	0.765734
-38.664755	13.393248	0.770739
-38.271532	10.552798	0.775744
-39.034062	7.576306	0.780749
-39.697538	3.782559	0.785754
-39.626714	12.295592	0.790758
-39.789506	11.507907	0.795763
-39.777113	2.985979	0.800768
-39.727139	8.644504	0.805773
-40.911593	9.324954	0.810778
-40.827894	11.406774	0.815782
-41.311948	9.414619	0.820787
-41.064497	4.179918	0.825792
-41.330103	11.507561	0.830797
-41.967421	-0.649392	0.835802
-42.593015	1.006941	0.840806
-42.794749	4.370901	0.845811
-42.627200	9.527866	0.850816
-42.449421	9.071220	0.855821
-42.672970	-1.713248	0.860826
-42.619299	7.910912	0.865830
-43.621436	6.341483	0.870835
-43.820984	0.334190	0.875840
-43.921089	3.758108	0.880845
-44.001541	22.053573	0.885850
-44.375591	8.400795	0.890854
-45.402832	4.382051	0.895859
-45.348196	-6.274457	0.900864
-45.668013	-2.908250	0.905869
-45.997033	-1.224766	0.910874
-45.770172	-4.932822	0.915878
-45.755669	2.802341	0.920883
-45.713545	2.493505	0.925888
-46.556042	-0.459410	0.930893
-47.371469	7.880538	0.935898
-47.164138	-0.363825	0.940902
-47.290946	10.353964	0.945907
-47.454163	18.193582	0.950912
-47.373705	2.537276	0.955917
-47.805494	6.218451	0.960922
-48.683754	8.672539	0.965926
-49.017859	3.719814	0.970931
-48.803833	-1.597461	0.975936
-49.331038	9.206722	0.980941
-49.159686	10.186478	0.985946
-48.895480	5.380033	0.990950
-50.030751	6.901878	0.995955
-50.352054	-0.223086	1.000960
-50.316668	10.313010	1.005965
-50.588969	3.569437	1.010970
-50.158066	-3.465558	1.015974
-51.232266	4.720139	1.020979
-51.790007	3.123540	1.025984
-52.210601	4.848400	1.030989
-52.433926	-3.387042	1.035994
-52.182564	-7.236573	1.040998
-52.288384	6.128320	1.046003
-52.377403	-2.773538	1.051008
-52.118055	2.325042	1.056013
-52.984091	4.789541	1.061018
-53.578657	-3.191677	1.066022
-54.095893	9.433321	1.071027
-54.177226	-2.182933	1.076032
-54.313350	-8.276174	1.081037
-53.945558	8.543597	1.086042
-53.918284	0.435045	1.091046
-54.773974	8.286890	1.096051
-55.346008	-1.294791	1.101056
-55.494336	0.899167	1.106061
-55.548792	-3.922882	1.111066
-55.675873	1.159847	1.116070
-55.867624	9.191719	1.121075
-55.927049	-5.957948	1.126080
-56.382915	-4.031034	1.131085
-57.214216	0.370546	1.136090
-56.853719	9.099211	1.141094
-57.035622	8.271770	1.146099
-57.549926	2.119086	1.151104
-58.501641	-5.871967	1.156109
-58.396944	-6.281217	1.161114
-58.405849	-4.218822	1.166118
-58.628855	10.993230	1.171123
-58.865282	10.187626	1.176128
-58.545888	9.117714	1.181133
-59.368801	7.523207	1.186138
-59.805424	3.588187	1.191142
-60.263489	4.715764	1.196147
-60.444695	0.606533	1.201152
-60.464732	-0.554772	1.206157
-60.668242	0.747680	1.211162
-60.444762	-8.708962	1.216166
-60.815882	2.276006	1.221171
-61.476074	-9.230667	1.226176
-61.870136	-14.184821	1.231181
-62.314717	8.295583	1.236186
-62.041424	-2.338166	1.241190
-62.345664	-1.158861	1.246195
-61.822713	4.406894	1.251200
-62.656212	0.380800	1.256205
-63.391498	1.256746	1.261210
-63.295645	-4.252121	1.266214
-64.020462	4.046510	1.271219
-63.833308	8.165929	1.276224
-63.893890	6.572110	1.281229
-64.874093	0.982401	1.286234
-65.030552	-2.986389	1.291238
-65.459087	2.211963	1.296243
-64.875416	1.860292	1.301248
-65.158364	6.821489	1.306253
-65.580932	7.760490	1.311258
-65.343280	3.926146	1.316262
-66.535214	10.475274	1.321267
-66.939400	-0.486022	1.326272
-66.617096	-2.481013	1.331277
-66.955710	5.512088	1.336282
-67.093987	-4.319052	1.341286
-67.584075	8.689470	1.346291
-67.234019	-1.554450	1.351296
-67.360960	7.791850	1.356301
-68.308355	-2.832538	1.361306
-68.651842	-4.989884	1.366310
-68.808338	4.813830	1.371315
-68.682907	13.478447	1.376320
-68.780014	9.830638	1.381325
-69.529395	1.173763	1.386330
-69.648110	-4.809987	1.391334
-70.105392	-2.913816	1.396339
-70.367610	3.812945	1.401344
-70.425377	13.583182	1.406349
-70.281922	12.793721	1.411354
-70.291702	0.557233	1.416358
-71.326278	4.705421	1.421363
-72.134323	5.870319	1.426368
-71.875502	5.341973	1.431373
-72.180598	7.525634	1.436378
-71.937074	-2.032486	1.441382
-72.218801	5.241091	1.446387
-72.243574	-4.048246	1.451392
-72.581891	2.873701	1.456397
-73.184256	6.497335	1.461402
-73.387811	2.153446	1.466406
-73.926283	8.461098	1.471411
-73.899154	2.163985	1.476416
-73.533687	-6.258635	1.481421
-74.458861	3.072586	1.486426
-75.043614	-9.137041	1.491430
-75.348843	-2.597230	1.496435
-75.086453	-0.568129	1.501440
-75.337698	2.617850	1.506445
-75.497136	7.003796	1.511450
-75.533832	-4.626736	1.516454
-76.669689	0.609982	1.521459
-76.835474	0.585894	1.526464
-76.861587	-5.715242	1.531469
-76.957464	3.766603	1.536474
-76.972852	-1.246387	1.541478
-77.143202	3.094895	1.546483
-77.178840	-0.254476	1.551488
-77.652457	6.972778	1.556493
-78.235816	5.105757	1.561498
-78.080734	5.502088	1.566502
-78.717716	8.037058	1.571507
-79.009106	13.069895	1.576512
-79.462288	-0.453179	1.581517
-80.157585	13.921110	1.586522
-79.921430	-2.343774	1.591526
-79.895257	4.921536	1.596531
-80.025009	-4.735602	1.601536
-80.198100	5.357548	1.606541
-80.444983	2.585891	1.611546
-80.580771	4.625946	1.616550
-81.538572	4.781883	1.621555
-81.624718	7.176096	1.626560
-81.766288	3.948411	1.631565
-82.056489	10.695485	1.636570
-81.831123	-1.662929	1.641574
-82.020269	13.627976	1.646579
-82.256908	14.469560	1.651584
-82.892114	6.049038	1.656589
-82.995876	1.337444	1.661594
-82.897293	-0.991321	1.666598
-84.242740	11.642400	1.671603
-84.666127	4.332263	1.676608
-84.078464	5.801899	1.681613
-85.003902	15.940963	1.686618
-85.002492	-3.363965	1.691622
-84.788920	7.881211	1.696627
-84.870273	-0.490060	1.701632
-84.998361	-2.140103	1.706637
-85.438293	-1.915653	1.711642
-85.825755	10.636892	1.716646
-86.511443	11.129852	1.721651
-86.542794	-2.536136	1.726656
-86.615063	7.531867	1.731661
-86.721568	-6.092889	1.736666
-87.037823	-5.771183	1.741670
-87.528949	-5.769718	1.746675
-87.824519	-2.671223	1.751680
-88.198284	1.252328	1.756685
-88.374168	13.677764	1.761690
-88.194710	15.068559	1.766694
-88.092576	3.528334	1.771699
-88.797090	5.140593	1.776704
-89.691235	2.339074	1.781709
-90.121172	6.567481	1.786714
-89.784023	2.100689	1.791718
-90.170550	10.063431	1.796723
-90.018025	-0.987992	1.801728
-89.777317	3.248654	1.806733
-90.429351	6.339669	1.811738
-91.093154	9.731062	1.816742
-91.734263	6.799130	1.821747
-91.636657	7.219857	1.826752
-91.534055	-4.713679	1.831757
-91.719174	-11.450043	1.836762
-91.678986	-7.886632	1.841766
-92.868671	2.236408	1.846771
-93.298681	5.951523	1.851776
-93.109573	-0.911905	1.856781
-93.257831	10.474067	1.861786
-93.134403	-0.174177	1.866790
-93.417084	-3.837286	1.871795
-93.753376	-2.788926	1.876800
-94.069544	-10.230722	1.881805
-94.696646	2.935201	1.886810
-94.537877	-3.872799	1.891814
-94.833616	-3.688161	1.896819
-94.837669	1.866030	1.901824
-95.274028	10.106436	1.906829
-95.917434	12.273499	1.911834
-95.754757	-3.646966	1.916838
-96.204237	8.218628	1.921843
-96.454120	14.171967	1.926848
-96.290833	5.617507	1.931853
-97.102500	13.729142	1.936858
-97.346028	-1.102910	1.941862
-97.614452	9.353066	1.946867
-98.200311	14.568248	1.951872
-97.492058	-0.640416	1.956877
-97.843200	9.848568	1.961882
-98.728614	5.369745	1.966886
-99.224839	7.729722	1.971891
-99.599807	-5.613890	1.976896
-99.336411	-12.181687	1.981901
-99.684628	5.040236	1.986906
-99.667402	-6.344179	1.991910
-99.965333	1.320281	1.996915
-99.716623	5.347284	2.006912
-99.842064	2.052427	2.016909
-100.049758	0.799549	2.026906
-98.878966	6.342232	2.036902
-98.496133	8.979875	2.046899
-97.747277	6.752772	2.056896
-96.914047	4.385285	2.066893
-96.924987	10.521859	2.076890
-96.583645	3.245407	2.086886
-96.483115	6.488415	2.096883
-95.854461	3.479763	2.106880
-94.518297	-4.623727	2.116877
-94.256342	-0.469664	2.126874
-94.128663	-1.327129	2.136870
-93.737678	-3.043948	2.146867
-92.716997	2.706783	2.156864
-92.737355	0.766046	2.166861
-91.599292	-5.639736	2.176858
-91.025446	3.867624	2.186854
-90.823066	7.313096	2.196851
-90.786804	6.735375	2.206848
-90.097871	-5.527037	2.216845
-89.515491	7.977106	2.226842
-88.974589	9.627281	2.236838
-88.281657	8.874455	2.246835
-88.020384	5.139228	2.256832
-87.250800	0.310643	2.266829
-86.565149	10.281980	2.276826
-86.060828	9.905272	2.286822
-86.187030	-0.552028	2.296819
-85.890027	7.346890	2.306816
-85.054085	8.939809	2.316813
-84.173365	-2.392562	2.326810
-83.640128	5.150915	2.336806
-83.061166	7.905404	2.346803
-83.059719	15.705198	2.356800
-82.755971	6.049870	2.366797
-81.801736	7.222087	2.376794
-81.442412	7.865952	2.386790
-80.890735	1.210354	2.396787
-80.219302	-3.313368	2.406784
-79.937846	10.280124	2.416781
-79.698065	4.966359	2.426778
-78.404215	-0.767770	2.436774
-78.293325	5.632073	2.446771
-78.202125	-2.194245	2.456768
-77.269223	-2.822554	2.466765
-76.939483	4.029498	2.476762
-76.836116	5.545925	2.486758
-75.752709	0.062610	2.496755
-75.603827	0.624395	2.506752
-74.349442	3.330381	2.516749
-73.988670	5.635221	2.526746
-73.799352	3.998750	2.536742
-73.722382	5.603900	2.546739
-73.192082	-1.508684	2.556736
-72.257097	-2.376586	2.566733
-72.066908	8.078382	2.576730
-71.201779	6.422386	2.586726
-70.665914	-1.127634	2.596723
-70.689523	-4.534250	2.606720
-70.031803	-10.887709	2.616717
-69.329673	-3.108794	2.626714
-68.913477	-4.302580	2.636710
-67.967972	-1.597407	2.646707
-67.742234	-0.294717	2.656704
-67.823531	-1.545765	2.666701
-66.715840	5.117957	2.676698
-66.171921	0.711620	2.686694
-65.965476	5.066398	2.696691
-65.384668	-1.268625	2.706688
-64.483994	-2.128287	2.716685
-64.404166	5.051338	2.726682
-64.100857	1.858095	2.736678
-63.313033	5.639578	2.746675
-62.819927	0.649738	2.756672
-62.494853	0.885467	2.766669
-61.537909	10.580431	2.776666
-61.375367	4.831455	2.786662
-61.141308	2.480708	2.796659
-59.998815	5.014837	2.806656
-59.774488	-2.706252	2.816653
-59.694030	-0.626835	2.826650
-58.502442	0.336649	2.836646
-57.783269	7.273111	2.846643
-57.547919	10.316922	2.856640
-57.849586	8.319150	2.866637
-56.817441	1.503148	2.876634
-56.444199	13.391025	2.886630
-56.136116	5.220857	2.896627
-55.077837	8.638087	2.906624
-54.407143	3.474281	2.916621
-54.654157	8.704825	2.926618
-54.059976	3.561863	2.936614
-53.257467	0.491192	2.946611
-52.892216	-0.088345	2.956608
-51.924076	1.029619	2.966605
-51.533270	4.841450	2.976602
-51.289229	4.629755	2.986598
-51.259442	2.061960	2.996595
-50.260651	7.524815	3.006592
-49.722895	9.343246	3.016589
-49.697472	10.833339	3.026586
-48.648444	10.764606	3.036582
-48.082208	6.802061	3.046579
-48.076916	3.987112	3.056576
-46.950094	-1.532218	3.066573
-46.689148	5.861665	3.076570
-46.464102	5.062492	3.086566
-46.153399	1.891439	3.096563
-45.428639	-4.665232	3.106560
-44.886085	1.084611	3.116557
-43.931010	-2.201624	3.126554
-43.727389	3.600381	3.136550
-43.680521	2.616001	3.146547
-42.434550	-2.323314	3.156544
-42.353852	-0.596983	3.166541
-42.281851	3.450579	3.176538
-41.239540	13.949257	3.186534
-40.618341	2.110346	3.196531
-40.197561	-2.089633	3.206528
-39.540231	3.185169	3.216525
-38.704991	3.639158	3.226522
-38.795998	-3.040520	3.236518
-38.632391	2.403395	3.246515
-37.893211	1.829727	3.256512
-37.365738	6.196948	3.266509
-37.002302	6.183434	3.276506
-35.838085	5.752400	3.286502
-35.644194	3.637070	3.296499
-35.505866	0.123875	3.306496
-35.307152	-0.675193	3.316493
-34.402995	8.761196	3.326490
-33.206655	-2.631236	3.336486
-32.910351	-5.983346	3.346483
-32.552831	0.107845	3.356480
-32.105340	-4.612781	3.366477
-32.319926	5.726041	3.376474
-31.569797	1.379668	3.386470
-30.931150	-1.711336	3.396467
-29.765466	1.764901	3.406464
-29.272463	-3.878460	3.416461
-29.258927	12.433639	3.426458
-29.372578	7.799915	3.436454
-28.214437	-4.423280	3.446451
-27.536204	-2.644264	3.456448
-27.159794	0.072877	3.466445
-27.118308	-4.886086	3.476442
-26.250734	-1.271878	3.486438
-26.027762	4.304968	3.496435
-24.658389	-2.812628	3.506432
-24.612376	-6.326272	3.516429
-24.444039	4.428064	3.526426
-23.826144	3.437925	3.536422
-23.088405	4.507338	3.546419
-23.029828	-9.099735	3.556416
-22.166958	-6.311257	3.566413
-21.430696	3.715836	3.576410
-21.238278	2.261206	3.586406
-21.136278	0.791290	3.596403
-20.331513	-2.264636	3.606400
-19.974832	4.818961	3.616397
-18.823479	11.919605	3.626394
-18.405215	7.783161	3.636390
-18.426381	-7.322494	3.646387
-17.965957	-1.241491	3.656384
-16.965650	5.420332	3.666381
-16.788861	4.659065	3.676378
-16.432749	-1.756572	3.686374
-15.352848	-6.446277	3.696371
-14.998555	-1.158537	3.706368
-14.838212	-7.341193	3.716365
-14.529008	-4.639518	3.726362
-13.491671	-4.545891	3.736358
-13.096701	-3.712721	3.746355
-13.046952	-1.703005	3.756352
-12.117024	1.128428	3.766349
-11.694459	-6.945870	3.776346
-11.502445	-4.897038	3.786342
-10.804454	-10.913983	3.796339
-10.236900	-4.864711	3.806336
-9.112997	-4.938008	3.816333
-9.231728	-6.048231	3.826330
-8.559408	-0.623088	3.836326
-8.304086	2.608272	3.846323
-7.707816	-5.133982	3.856320
-6.644575	-3.342921	3.866317
-6.761295	3.675873	3.876314
-6.475550	2.018826	3.886310
-5.846354	-3.537197	3.896307
-5.298049	0.081670	3.906304
-5.019675	3.528022	3.916301
-4.282476	12.569127	3.926298
-3.859101	18.309142	3.936294
-2.997037	30.134241	3.946291
-2.834475	31.146388	3.956288
-2.811721	41.801532	3.966285
-1.939213	52.823701	3.976282
-1.416925	68.411682	3.986278
-1.155424	75.712855	3.996275
-0.813846	95.840636	4.006272
-0.480046	116.255506	4.016269
0.000000	130.013241	4.021274
0.126440	149.032355	4.026278
0.227055	150.397621	4.031283
0.375927	163.184271	4.036288
1.092467	170.815642	4.041293
0.984706	175.270839	4.046298
1.138669	175.878684	4.051302
1.192259	187.562729	4.056307
0.611868	183.652302	4.061312
0.516452	179.293742	4.066317
0.717706	192.146147	4.071322
0.918673	182.147434	4.076326
0.911369	181.778098	4.081331
0.847739	184.128958	4.086336
1.055974	194.061354	4.091341
0.924205	210.648805	4.096346
0.838216	205.723771	4.101350
1.246518	211.119728	4.106355
1.002887	217.910204	4.111360
1.226922	211.878700	4.116365
0.904120	215.487255	4.121370
1.010238	208.196153	4.126374
1.401148	202.619409	4.131379
0.969568	213.450850	4.136384
1.110864	201.668896	4.141389
0.901911	211.742660	4.146394
1.113849	212.237830	4.151398
1.434585	227.809728	4.156403
1.398204	230.663880	4.161408
1.350230	220.139399	4.166413
1.341349	226.625599	4.171418
1.555771	228.780262	4.176422
1.646744	214.449723	4.181427
1.038173	212.398694	4.186432
1.411611	227.871712	4.191437
1.247396	240.664389	4.196442
1.407900	247.949155	4.201446
1.437002	246.014920	4.206451
1.391927	245.451747	4.211456
1.426974	239.295093	4.216461
1.297165	237.279682	4.221466
1.522625	231.961521	4.226470
1.753693	243.349609	4.231475
1.434362	243.610952	4.236480
1.583344	250.490072	4.241485
1.292344	240.684400	4.246490
1.630411	233.187731	4.251494
1.441477	240.684639	4.256499
1.175635	246.674052	4.261504
1.568762	232.314972	4.266509
1.588906	240.443756	4.271514
1.477172	234.649556	4.276518
1.888703	245.363396	4.281523
1.708275	240.290284	4.286528
1.718181	239.367892	4.291533
1.646495	241.162779	4.296538
1.664164	240.280934	4.301542
1.785311	246.586522	4.306547
1.552340	238.819087	4.311552
1.670257	246.189816	4.316557
1.487084	240.172517	4.321562
1.700833	246.856936	4.326566
1.771202	244.284279	4.331571
1.680111	254.426891	4.336576
1.781320	254.573356	4.341581
1.637024	245.796800	4.346586
1.473732	246.024859	4.351590
1.888016	244.591684	4.356595
1.936277	263.075523	4.361600
2.090297	249.561476	4.366605
1.660906	257.391634	4.371610
1.710386	251.697461	4.376614
2.110248	258.080711	4.381619
1.882463	258.085906	4.386624
2.007826	248.114838	4.391629
1.675700	256.597521	4.396634
1.800461	263.487555	4.401638
2.292658	272.250159	4.406643
1.941042	267.832789	4.411648
2.202762	250.961889	4.416653
1.838813	245.133201	4.421658
1.716978	250.176867	4.426662
2.203869	260.598966	4.431667
2.191599	276.367024	4.436672
2.192255	259.152718	4.441677
1.999189	252.492423	4.446682
2.067885	256.602978	4.451686
2.132334	251.195693	4.456691
1.768762	244.796113	4.461696
2.469627	249.709053	4.466701
1.837317	261.610684	4.471706
2.235865	262.329652	4.476710
2.217742	269.420193	4.481715
2.345792	267.819442	4.486720
2.791798	256.289871	4.491725
1.957889	250.482018	4.496730
1.862334	263.240775	4.501734
2.053882	255.391635	4.506739
2.071245	255.930602	4.511744
2.051407	265.621041	4.516749
2.222233	274.494568	4.521754
2.397514	276.619992	4.526758
2.375558	279.309577	4.531763
2.280688	283.054513	4.536768
2.482554	278.395813	4.541773
2.342242	282.404373	4.546778
2.079411	264.688719	4.551782
2.457553	266.339226	4.556787
2.155968	272.568077	4.561792
2.208344	271.418067	4.566797
2.212452	280.555926	4.571802
2.126963	276.467301	4.576806
2.394696	287.173067	4.581811
2.391699	286.979021	4.586816
2.692384	272.641395	4.591821
2.526006	288.388762	4.596826
2.436558	284.874580	4.601830
2.773281	274.314014	4.606835
2.399908	277.339984	4.611840
2.564108	268.498918	4.616845
2.665655	274.197265	4.621850
2.603786	275.472780	4.626854
2.332307	269.902674	4.631859
2.355407	274.828081	4.636864
2.594346	270.783121	4.641869
2.374384	268.505772	4.646874
2.438555	274.366765	4.651878
2.598136	274.758811	4.656883
2.308391	283.466349	4.661888
2.561636	279.117329	4.666893
2.457085	279.985241	4.671898
2.495932	277.640654	4.676902
2.881213	275.494044	4.681907
2.476315	279.069319	4.686912
2.838833	279.510601	4.691917
2.919323	276.597871	4.696922
2.789952	272.641202	4.701926
2.870623	270.731295	4.706931
2.527307	287.551892	4.711936
2.960197	282.814267	4.716941
2.877196	282.293371	4.721946
2.572445	278.644291	4.726950
2.499919	274.694210	4.731955
2.495249	283.732694	4.736960
2.468300	279.951972	4.741965
2.768269	280.097852	4.746970
2.586438	280.658096	4.751974
2.798503	276.816370	4.756979
2.504309	283.332479	4.761984
2.812250	277.779976	4.766989
2.702116	290.933328	4.771994
2.709695	305.977642	4.776998
2.993452	312.184956	4.782003
2.928675	307.658215	4.787008
3.322439	302.231319	4.792013
2.967630	298.181670	4.797018
2.770684	283.362344	4.802022
2.969686	297.079546	4.807027
2.935679	299.207200	4.812032
2.956602	298.498649	4.817037
2.791092	310.379312	4.822042
3.051702	311.781589	4.827046
3.212417	307.265039	4.832051
3.015599	310.116023	4.837056
3.425741	315.603070	4.842061
2.808804	305.801199	4.847066
3.073788	283.987182	4.852070
2.927835	311.854414	4.857075
2.988596	318.097891	4.862080
3.146735	316.846540	4.867085
2.803352	309.523615	4.872090
3.012917	316.807114	4.877094
3.235564	313.840006	4.882099
2.832399	324.996838	4.887104
3.110791	317.321258	4.892109
3.014490	319.724104	4.897114
3.074274	324.578055	4.902118
3.205406	315.436983	4.907123
2.696327	315.120769	4.912128
3.137685	302.979269	4.917133
3.011589	317.986392	4.922138
3.138133	316.116253	4.927142
3.314804	314.221553	4.932147
2.980512	320.877196	4.937152
3.428988	328.256874	4.942157
3.422610	339.246232	4.947162
3.296139	336.319449	4.952166
3.346976	327.292763	4.957171
3.299620	322.529320	4.962176
3.591795	334.805458	4.967181
3.377605	320.910310	4.972186
3.148394	322.117489	4.977190
3.347966	316.469128	4.982195
3.437359	337.391783	4.987200
3.458604	344.490750	4.992205
3.376400	354.883735	4.997210
3.422395	343.942892	5.002214
3.739751	348.372677	5.007219
3.198014	346.812457	5.012224
3.419517	335.690092	5.017229
3.432550	354.274672	5.022234
3.517517	345.855395	5.027238
3.700141	341.002245	5.032243
3.499614	356.809586	5.037248
3.635497	346.213396	5.042253
3.446693	347.766403	5.047258
3.634466	333.199651	5.052262
3.580736	335.221848	5.057267
3.461258	361.257654	5.062272
3.577903	346.632004	5.067277
3.552319	351.310549	5.072282
3.263742	350.907975	5.077286
3.409039	339.446583	5.082291
3.482717	343.984019	5.087296
3.428511	348.961688	5.092301
3.445014	341.552637	5.097306
3.762383	356.489867	5.102310
3.906882	349.109483	5.107315
3.447859	355.253987	5.112320
3.407931	345.936056	5.117325
3.624540	345.418821	5.122330
3.516671	353.226083	5.127334
3.915141	355.664477	5.132339
3.649228	363.988289	5.137344
3.854091	372.655973	5.142349
3.771079	382.677268	5.147354
4.067523	372.536866	5.152358
3.908310	358.923737	5.157363
3.519544	354.003800	5.162368
3.919463	367.007420	5.167373
3.973701	377.073118	5.172378
4.121506	382.229924	5.177382
3.882704	352.348042	5.182387
3.658922	360.321956	5.187392
4.026981	356.199697	5.192397
3.989981	368.603069	5.197402
3.554267	355.062767	5.202406
4.159263	357.857322	5.207411
3.759727	379.782888	5.212416
4.343871	371.741937	5.217421
4.163632	379.140297	5.222426
4.246949	385.343570	5.227430
4.219112	352.282595	5.232435
3.587636	364.186041	5.237440
3.953737	348.993023	5.242445
4.168550	372.253709	5.247450
4.029614	376.726941	5.252454
3.733585	365.921826	5.257459
3.562831	371.390149	5.262464
4.281796	371.221428	5.267469
4.306111	377.815465	5.272474
4.039338	383.613689	5.277478
4.396356	381.547604	5.282483
4.384204	379.592150	5.287488
4.371331	361.501021	5.292493
4.376600	375.261161	5.297498
4.081922	378.357807	5.302502
4.267804	368.570622	5.307507
4.516690	374.340849	5.312512
4.464673	354.627453	5.317517
4.367560	346.774470	5.322522
3.919184	351.779098	5.327526
3.930646	345.308620	5.332531
3.847795	369.123816	5.337536
4.272952	372.600123	5.342541
4.301357	375.231185	5.347546
4.235347	373.209850	5.352550
4.114412	373.697583	5.357555
4.121908	371.001909	5.362560
4.239045	369.987894	5.367565
3.973939	376.131931	5.372570
4.482151	376.908650	5.377574
4.216793	374.819429	5.382579
3.966883	386.013726	5.387584
4.089352	383.619590	5.392589
4.259997	380.647250	5.397594
4.436657	410.035434	5.402598
4.498021	400.691654	5.407603
4.296550	416.970108	5.412608
4.231561	414.678769	5.417613
4.623428	411.811045	5.422618
4.513617	413.946308	5.427622
4.693779	406.445560	5.432627
4.362145	413.854452	5.437632
4.301392	406.101586	5.442637
4.291884	419.281335	5.447642
4.442035	409.078856	5.452646
4.818439	402.524961	5.457651
4.820586	408.253595	5.462656
4.777796	391.785369	5.467661
4.920130	411.612954	5.472666
4.465091	418.736105	5.477670
4.443553	410.265135	5.482675
4.413155	409.794933	5.487680
4.254830	413.339456	5.492685
4.448547	411.778647	5.497690
4.358296	413.628220	5.502694
4.616585	403.555665	5.507699
4.461592	418.639583	5.512704
4.715847	425.527923	5.517709
5.239584	427.987853	5.522714
5.095092	423.969615	5.527718
4.800122	399.433743	5.532723
4.739300	411.245290	5.537728
4.801798	416.771966	5.542733
4.670197	418.745085	5.547738
4.887356	418.035078	5.552742
5.148690	413.559684	5.557747
4.430027	404.111971	5.562752
4.804995	405.474739	5.567757
4.860647	414.675884	5.572762
4.470614	411.352724	5.577766
5.104328	421.683286	5.582771
4.813775	441.179032	5.587776
4.689031	428.295347	5.592781
4.961274	439.831079	5.597786
4.838815	438.478989	5.602790
5.306103	447.032807	5.607795
4.807906	452.870682	5.612800
5.103568	447.106848	5.617805
5.137242	451.644119	5.622810
5.031732	443.752616	5.627814
4.935108	440.901780	5.632819
5.064462	448.812844	5.637824
5.192492	450.755197	5.642829
5.406556	438.145626	5.647834
4.862417	434.157024	5.652838
5.158200	414.810701	5.657843
4.827096	424.286597	5.662848
5.049086	425.828258	5.667853
5.229560	441.143561	5.672858
5.240570	444.291223	5.677862
5.463214	432.400347	5.682867
4.846110	430.816661	5.687872
5.197980	431.447159	5.692877
5.320720	435.980856	5.697882
4.956886	439.858181	5.702886
4.943610	434.181514	5.707891
4.954769	443.801434	5.712896
5.553723	440.126002	5.717901
5.306077	452.352531	5.722906
5.139007	451.280800	5.727910
5.393966	451.997559	5.732915
5.067803	446.649231	5.737920
5.455671	439.954514	5.742925
5.138929	449.043679	5.747930
5.281308	450.938081	5.752934
5.384687	451.948437	5.757939
5.309347	453.535092	5.762944
5.433010	444.867259	5.767949
5.655080	448.520494	5.772954
5.067694	451.993861	5.777958
5.292127	442.497812	5.782963
5.433218	458.147284	5.787968
5.532351	448.364517	5.792973
5.495387	453.694738	5.797978
5.401613	452.267860	5.802982
5.762330	450.661001	5.807987
5.404440	450.634322	5.812992
5.436060	454.775228	5.817997
5.544542	458.262252	5.823002
5.312699	446.225279	5.828006
5.049227	445.744658	5.833011
5.400060	454.007542	5.838016
5.441941	446.430079	5.843021
5.348429	440.776436	5.848026
5.408930	449.330589	5.853030
5.226678	448.290570	5.858035
4.930273	458.468824	5.863040
5.315204	457.818305	5.868045
5.068337	468.226935	5.873050
5.179382	479.314195	5.878054
5.850889	473.859099	5.883059
5.213183	478.604407	5.888064
5.503139	476.701819	5.893069
5.545053	483.111067	5.898074
5.526490	481.616902	5.903078
6.225754	491.530403	5.908083
5.643531	493.239698	5.913088
5.786593	480.382453	5.918093
6.177544	492.306856	5.923098
5.707588	478.001481	5.928102
5.669115	473.495306	5.933107
5.586652	479.812833	5.938112
5.708506	473.566956	5.943117
5.918485	481.186101	5.948122
5.955925	484.483805	5.953126
6.010027	475.934691	5.958131
5.323424	495.747337	5.963136
5.660769	485.209412	5.968141
6.148639	502.140914	5.973146
5.930079	511.449192	5.978150
6.051491	486.732394	5.983155
5.631143	497.755449	5.988160
6.128746	503.446738	5.993165
5.915777	492.800065	5.998170
5.973055	485.182055	6.003174
5.914865	473.863110	6.008179
5.877874	483.383178	6.013184
6.279721	494.749348	6.018189
6.265556	497.119509	6.023194
6.100978	492.269623	6.028198
5.767315	474.038102	6.033203
5.878911	487.800010	6.038208
5.621563	479.952423	6.043213
5.994978	496.115142	6.048218
5.632031	512.682517	6.053222
6.075804	505.186007	6.058227
6.137240	524.445809	6.063232
6.428861	516.194638	6.068237
6.121746	503.037356	6.073242
5.879264	494.359855	6.078246
6.327176	493.672979	6.083251
6.213894	485.752352	6.088256
6.221478	496.642732	6.093261
6.189118	483.194107	6.098266
5.897009	484.946816	6.103270
6.060782	471.334969	6.108275
5.918012	484.485690	6.113280
5.823527	477.435484	6.118285
6.145340	474.162691	6.123290
6.031628	480.931122	6.128294
6.233518	480.389579	6.133299
6.073800	482.212459	6.138304
6.402062	478.740098	6.143309
6.563076	478.561172	6.148314
6.051692	482.360089	6.153318
6.376770	479.245102	6.158323
6.032017	466.649716	6.163328
5.766043	455.601113	6.168333
6.141618	471.043735	6.173338
6.109269	471.933960	6.178342
6.006127	453.436270	6.183347
5.895235	458.484017	6.188352
5.947458	458.205962	6.193357
6.264055	468.259441	6.198362
5.562291	460.316600	6.203366
5.717019	469.979504	6.208371
5.882650	474.607447	6.213376
5.752531	477.524294	6.218381
5.979964	477.520363	6.223386
5.700327	486.534752	6.228390
6.025471	471.196251	6.233395
5.734756	485.830384	6.238400
5.721145	476.195475	6.243405
5.887995	475.787584	6.248410
5.563879	481.372549	6.253414
6.147376	471.132751	6.258419
6.113020	487.186148	6.263424
6.058876	479.627892	6.268429
6.123016	482.029605	6.273434
6.221371	480.124149	6.278438
6.443201	476.487746	6.283443
5.896334	488.110631	6.288448
5.869105	479.329887	6.293453
5.807050	488.861203	6.298458
5.794741	491.610399	6.303462
6.002327	481.798936	6.308467
6.052198	480.937999	6.313472
6.103008	478.972030	6.318477
5.977586	478.280255	6.323482
5.917920	488.338507	6.328486
6.279316	481.878021	6.333491
5.818913	483.404890	6.338496
5.910966	483.392057	6.343501
6.039430	479.253717	6.348506
5.929938	475.162001	6.353510
6.009470	471.150731	6.358515
5.878161	480.016097	6.363520
5.901714	489.999430	6.368525
6.042185	490.319165	6.373530
6.037712	478.642285	6.378534
6.259920	487.832426	6.383539
5.962371	486.022879	6.388544
5.833505	485.125378	6.393549
5.960006	477.581667	6.398554
5.904281	481.032394	6.403558
6.506433	483.999405	6.408563
5.879747	482.572783	6.413568
5.988627	485.137783	6.418573
6.139818	479.423561	6.423578
5.987937	479.263686	6.428582
5.940676	483.926714	6.433587
5.754211	473.956221	6.438592
6.116853	487.299767	6.443597
6.045454	483.233818	6.448602
6.027690	485.633479	6.453606
6.228990	485.029879	6.458611
5.946107	481.734872	6.463616
5.888340	479.346138	6.468621
6.073538	480.487806	6.473626
5.635230	487.458065	6.478630
5.949551	478.627983	6.483635
5.986022	487.541101	6.488640
5.678055	487.481113	6.493645
6.317531	487.173592	6.498650
6.040355	484.483110	6.503654
6.051537	479.713201	6.508659
6.051697	487.814736	6.513664
6.040482	473.592694	6.518669
6.084300	479.349887	6.523674
5.718288	476.634426	6.528678
5.885008	471.636369	6.533683
6.037449	477.746765	6.538688
5.938044	487.722002	6.543693
5.946751	470.111692	6.548698
5.720797	479.139699	6.553702
6.241720	474.383425	6.558707
5.776598	479.232513	6.563712
6.084192	485.380414	6.568717
6.114628	481.425302	6.573722
5.833456	483.513813	6.578726
6.129389	471.918610	6.583731
5.772796	483.963581	6.588736
5.731247	470.718933	6.593741
5.979816	486.544439	6.598746
5.961941	500.596401	6.603750
5.841601	499.542694	6.608755
6.055811	508.407806	6.613760
6.275038	512.542686	6.618765
6.124625	485.274308	6.623770
5.687710	493.004899	6.628774
5.753963	494.437930	6.633779
6.198470	511.671203	6.638784
6.342420	518.842811	6.643789
6.112673	492.463129	6.648794
5.336706	492.313252	6.653798
5.971850	496.334210	6.658803
6.018169	514.890496	6.663808
6.411121	513.255317	6.668813
6.503932	497.100502	6.673818
6.238166	492.434860	6.678822
6.426126	490.668207	6.683827
5.949034	481.751167	6.688832
6.101014	485.687700	6.693837
5.932043	492.280875	6.698842
5.514293	501.919026	6.703846
5.914593	486.916256	6.708851
6.137486	482.625470	6.713856
6.062683	480.846400	6.718861
6.344274	489.386236	6.723866
6.113541	487.789011	6.728870
6.169871	484.478299	6.733875
6.534010	489.493925	6.738880
6.142569	487.660924	6.743885
6.150527	483.628329	6.748890
6.005091	484.548293	6.753894
6.035842	487.135380	6.758899
5.845775	492.832175	6.763904
5.939607	492.993871	6.768909
6.090593	485.677465	6.773914
5.973670	486.464756	6.778918
5.800301	483.450588	6.783923
5.716233	485.500806	6.788928
5.846409	488.338037	6.793933
6.421024	476.242652	6.798938
6.188457	493.056713	6.803942
6.317676	483.308318	6.808947
6.351803	482.055447	6.813952
5.790933	474.062579	6.818957
5.902924	459.472516	6.823962
5.889487	461.696044	6.828966
6.190140	468.470284	6.833971
6.121939	470.407281	6.838976
5.772656	470.099680	6.843981
6.225975	458.985484	6.848986
5.824187	461.029205	6.853990
5.967746	464.326831	6.858995
6.051100	466.008711	6.864000
5.983797	465.307727	6.869005
6.374639	460.169144	6.874010
5.712557	460.054809	6.879014
6.090070	456.609041	6.884019
6.070055	453.166714	6.889024
6.074377	452.409991	6.894029
6.315042	454.371025	6.899034
6.432173	456.556991	6.904038
6.642193	452.310962	6.909043
6.338417	453.555927	6.914048
6.292884	451.771332	6.919053
6.206633	452.663558	6.924058
6.288329	456.857653	6.929062
6.382952	436.680199	6.934067
5.719462	430.086417	6.939072
5.544820	426.767616	6.944077
5.843067	424.426312	6.949082
5.549692	448.196705	6.954086
5.822505	443.557112	6.959091
5.920835	454.768989	6.964096
5.980857	457.029212	6.969101
5.947301	460.068418	6.974106
6.080000	460.678901	6.979110
6.026788	445.965203	6.984115
6.082743	455.345388	6.989120
6.139112	439.533673	6.994125
6.001797	446.335093	6.999130
5.860553	453.664791	7.004134
5.978386	454.468438	7.009139
6.184996	458.898107	7.014144
6.103459	454.240707	7.019149
6.211621	451.195214	7.024154
6.010935	458.306540	7.029158
6.036274	454.098133	7.034163
5.984276	443.925288	7.039168
5.752020	456.760170	7.044173
6.066509	455.330840	7.049178
5.941453	459.508392	7.054182
5.915760	454.143064	7.059187
5.627973	448.390209	7.064192
5.951680	448.946435	7.069197
6.068231	445.311948	7.074202
5.843091	461.720051	7.079206
5.982492	458.875985	7.084211
6.155134	457.985783	7.089216
6.105657	447.184559	7.094221
6.662969	446.312874	7.099226
6.024994	453.694864	7.104230
5.678284	456.826071	7.109235
6.000842	464.545882	7.114240
6.012732	456.151743	7.119245
6.144392	451.637584	7.124250
6.172202	445.918113	7.129254
6.447131	451.473627	7.134259
5.905254	443.095336	7.139264
5.615436	439.143335	7.144269
6.316156	446.532590	7.149274
6.036076	446.966711	7.154278
5.957393	436.392499	7.159283
5.976322	433.920853	7.164288
5.962467	446.030210	7.169293
5.797530	444.277483	7.174298
6.155743	451.888495	7.179302
5.965621	448.417650	7.184307
5.936727	447.264087	7.189312
5.578303	447.726546	7.194317
6.151473	451.536541	7.199322
5.920895	465.338005	7.204326
6.119340	464.910884	7.209331
5.742317	461.970233	7.214336
5.849954	462.271814	7.219341
5.935051	458.123775	7.224346
5.943863	459.176693	7.229350
6.126442	458.862692	7.234355
6.124919	452.925492	7.239360
5.948761	457.964193	7.244365
5.933609	452.898230	7.249370
5.942778	450.858442	7.254374
6.106716	457.095680	7.259379
5.984539	458.185930	7.264384
5.798682	465.161325	7.269389
6.291441	455.541801	7.274394
6.155094	461.514436	7.279398
6.339221	450.879815	7.284403
6.251566	453.898164	7.289408
5.538276	435.665887	7.294413
5.776270	446.137926	7.299418
5.918847	459.218089	7.304422
5.934458	454.117443	7.309427
5.828459	460.684709	7.314432
5.752373	470.419498	7.319437
6.120980	454.946166	7.324442
6.139331	450.797122	7.329446
6.238941	455.604971	7.334451
6.298589	462.260590	7.339456
5.997988	468.585944	7.344461
6.446610	455.019482	7.349466
6.418297	451.070435	7.354470
6.259634	427.689086	7.359475
5.842171	421.897587	7.364480
5.741809	413.544317	7.369485
5.970736	415.741204	7.374490
5.837034	418.025542	7.379494
5.890824	421.434678	7.384499
5.834513	423.539003	7.389504
5.885175	432.006373	7.394509
6.335975	443.212679	7.399514
5.956842	433.899249	7.404518
6.123156	444.829660	7.409523
5.835367	418.981597	7.414528
6.070716	427.720241	7.419533
6.172854	419.764148	7.424538
5.782228	417.336309	7.429542
5.846421	414.234257	7.434547
5.929928	426.530745	7.439552
6.110502	432.764039	7.444557
6.141310	418.037274	7.449562
5.809127	428.826689	7.454566
6.006720	436.070886	7.459571
6.124510	447.786942	7.464576
5.832880	424.248704	7.469581
6.074002	435.406288	7.474586
5.966250	439.205876	7.479590
5.953404	443.086369	7.484595
6.010840	449.264940	7.489600
5.922492	447.591801	7.494605
6.045237	450.843140	7.499610
5.953195	456.041481	7.504614
6.102862	458.060173	7.509619
6.193267	442.997863	7.514624
5.971030	440.971456	7.519629
6.167752	421.460851	7.524634
5.915825	429.325995	7.529638
5.894437	419.671786	7.534643
5.804172	424.411062	7.539648
5.449052	439.010905	7.544653
5.998779	446.118285	7.549658
5.865706	455.742809	7.554662
5.886000	445.142270	7.559667
6.066296	447.968844	7.564672
5.802353	462.236455	7.569677
6.007630	451.137900	7.574682
5.603293	458.319778	7.579686
6.067264	454.674936	7.584691
6.056147	447.959922	7.589696
5.793941	449.386948	7.594701
5.969589	438.519817	7.599706
5.655353	450.191247	7.604710
6.017588	435.119837	7.609715
6.079909	447.615087	7.614720
5.895679	450.848390	7.619725
5.891692	447.367503	7.624730
5.637689	462.206479	7.629734
5.717675	445.385427	7.634739
5.922211	456.464324	7.639744
6.329812	468.682328	7.644749
6.197316	454.782338	7.649754
6.187812	454.237944	7.654758
5.998595	444.610763	7.659763
5.986655	445.523167	7.664768
5.860879	440.582236	7.669773
6.056699	435.519595	7.674778
5.787101	455.166000	7.679782
5.971658	451.535466	7.684787
6.215770	444.443725	7.689792
6.225138	445.930845	7.694797
6.252103	445.958266	7.699802
6.230985	448.655733	7.704806
6.099134	442.709984	7.709811
6.132856	441.433308	7.714816
6.079987	459.377464	7.719821
6.044382	458.184265	7.724826
5.910886	462.707629	7.729830
6.073067	453.740212	7.734835
6.280757	442.496236	7.739840
5.998638	445.701712	7.744845
6.207047	444.533303	7.749850
6.101309	442.410493	7.754854
5.816472	445.267661	7.759859
5.948851	455.934646	7.764864
5.815452	456.483341	7.769869
6.035852	454.054167	7.774874
6.113692	445.269497	7.779878
6.372875	455.539539	7.784883
6.367845	440.878856	7.789888
6.019425	445.962990	7.794893
6.120989	431.858398	7.799898
5.702519	425.360572	7.804902
6.138969	430.235578	7.809907
5.885078	440.439451	7.814912
5.569469	441.749709	7.819917
5.908929	434.706837	7.824922
6.133516	446.032118	7.829926
5.819037	446.268194	7.834931
6.352326	441.596212	7.839936
5.815430	446.088958	7.844941
6.075203	450.679533	7.849946
5.990685	456.922015	7.854950
6.191263	456.452810	7.859955
6.126644	449.451845	7.864960
6.015347	449.052430	7.869965
6.086463	443.437386	7.874970
5.690020	451.099212	7.879974
5.683893	441.291520	7.884979
6.170999	444.065024	7.889984
5.875962	450.892116	7.894989
6.267864	446.062065	7.899994
5.991784	452.239812	7.904998
5.959905	455.927715	7.910003
6.226407	454.470107	7.915008
6.071766	453.068481	7.920013
6.004839	454.987507	7.925018
5.673419	445.480807	7.930022
5.726208	439.240536	7.935027
5.352852	442.230623	7.940032
5.301268	444.192791	7.945037
5.731191	449.066021	7.950042
5.555345	452.676885	7.955046
5.449432	457.836970	7.960051
6.139263	478.214261	7.965056
5.814002	474.050073	7.970061
6.199311	474.422876	7.975066
6.007661	482.517924	7.980070
5.769481	478.169060	7.985075
5.909131	486.431344	7.990080
5.605634	488.531043	7.995085
5.891620	481.479327	8.000090
5.886138	493.662022	8.005094
6.015742	483.649257	8.010099
5.977334	476.493691	8.015104
5.706319	483.293643	8.020109
6.341498	486.813914	8.025126
6.431416	481.411384	8.030144
6.089104	485.580095	8.035162
6.161310	471.693686	8.040179
6.006405	475.434746	8.045197
6.452848	476.521789	8.050214
6.404627	486.952245	8.055232
6.121046	475.002921	8.060250
6.222175	454.524785	8.065267
5.660580	456.824275	8.070285
6.082451	457.274651	8.075302
6.270453	472.863907	8.080320
5.808805	453.557214	8.085338
6.307968	462.271123	8.090355
5.884369	465.820505	8.095373
6.164929	465.588952	8.100390
6.093431	457.191819	8.105408
5.951606	454.480150	8.110426
6.063078	455.240827	8.115443
6.195875	478.104486	8.120461
6.073905	476.811315	8.125478
6.284824	465.952208	8.130496
5.958056	455.478660	8.135514
6.103709	452.181495	8.140531
6.233549	463.934618	8.145549
6.341003	459.963773	8.150566
5.881717	462.534591	8.155584
5.931499	463.212862	8.160602
6.278270	454.942734	8.165619
6.073734	481.696170	8.170637
6.275456	463.132832	8.175654
6.628949	462.815421	8.180672
6.183594	454.141355	8.185690
6.012951	445.134451	8.190707
5.996853	457.169708	8.195725
6.394227	447.324095	8.200742
6.011924	448.444663	8.205760
6.033021	444.217179	8.210778
6.102680	456.464895	8.215795
6.003125	474.986173	8.220813
6.178731	478.808712	8.225830
6.498682	484.446232	8.230848
6.348967	485.095573	8.235866
6.174243	461.588190	8.240883
6.409169	471.313798	8.245901
6.414640	453.214023	8.250918
6.034480	460.314910	8.255936
6.019906	449.994362	8.260954
6.631722	460.809433	8.265971
6.251982	460.909101	8.270989
6.218359	465.131105	8.276006
6.034808	459.134918	8.281024
6.175540	467.431576	8.286042
6.646017	461.696431	8.291059
6.026381	450.428528	8.296077
6.069994	468.409110	8.301094
6.173360	475.088037	8.306112
6.280970	494.111027	8.311130
6.586581	482.335738	8.316147
6.276748	485.978902	8.321165
6.521994	485.477743	8.326182
6.336304	462.673812	8.331200
6.139135	469.037902	8.336218
6.297091	470.647628	8.341235
6.466488	480.060115	8.346253
6.259501	465.660405	8.351270
6.699103	469.158561	8.356288
6.540456	461.384966	8.361306
6.542200	451.795441	8.366323
6.057704	460.742362	8.371341
6.038931	450.419949	8.376358
6.487638	455.394667	8.381376
6.196581	452.546666	8.386394
6.433671	470.765994	8.391411
6.486202	465.688880	8.396429
6.384731	469.294164	8.401446
6.386275	464.780589	8.406464
6.113790	462.431589	8.411482
6.621543	468.315575	8.416499
6.315955	470.617930	8.421517
6.650970	476.023374	8.426534
6.275542	461.316822	8.431552
6.416990	469.481399	8.436570
6.774459	469.823640	8.441587
6.410856	464.564455	8.446605
6.096208	449.411830	8.451622
6.529753	462.404384	8.456640
6.435407	480.034324	8.461658
6.470618	482.105788	8.466675
6.534688	485.955323	8.471693
6.357418	478.078813	8.476710
6.628700	483.951695	8.481728
6.299361	467.508608	8.486746
6.290197	475.083527	8.491763
6.297231	481.345189	8.496781
6.241447	489.233372	8.501798
6.255218	487.514497	8.506816
6.304934	488.930045	8.511834
6.563140	478.338851	8.516851
6.465930	487.259771	8.521869
6.248634	489.115728	8.526886
6.627666	491.152912	8.531904
6.373417	481.538264	8.536922
6.189498	473.871576	8.541939
6.064595	485.612591	8.546957
6.223663	484.900911	8.551974
6.275005	488.943460	8.556992
6.433742	511.962006	8.562010
6.600263	515.550076	8.567027
6.460390	527.700117	8.572045
6.150343	517.348642	8.577063
6.560367	517.294378	8.582080
6.468554	525.675058	8.587098
6.461339	513.433032	8.592115
6.346864	524.329496	8.597133
6.547711	517.912643	8.602151
6.440316	517.128384	8.607168
6.599396	529.763177	8.612186
6.593441	523.566191	8.617203
6.563793	520.491646	8.622221
6.350233	526.552028	8.627239
6.396950	516.282713	8.632256
6.416034	530.379256	8.637274
7.151987	540.535108	8.642291
7.209906	537.158051	8.647309
6.595533	538.277613	8.652327
6.933692	518.554762	8.657344
6.578148	527.497534	8.662362
6.712462	518.470304	8.667379
6.706938	522.120363	8.672397
6.678138	525.717489	8.677415
6.831021	521.330534	8.682432
6.760332	518.390307	8.687450
6.624979	515.735421	8.692467
6.792135	517.725353	8.697485
6.667373	530.207877	8.702503
6.646410	523.202003	8.707520
6.844910	525.751023	8.712538
6.709382	517.632992	8.717555
6.729582	521.765621	8.722573
6.680078	511.229093	8.727591
6.753741	517.727942	8.732608
6.620023	519.595677	8.737626
6.692912	522.494626	8.742643
7.142082	520.089046	8.747661
6.683225	526.779523	8.752679
6.583315	522.927362	8.757696
6.661385	520.839852	8.762714
6.659900	514.551104	8.767731
6.772735	517.384604	8.772749
6.893786	516.680288	8.777767
7.428558	511.222439	8.782784
6.911190	516.193370	8.787802
7.016427	510.492093	8.792819
6.905904	515.401204	8.797837
6.712476	523.732349	8.802855
6.911988	518.065875	8.807872
6.798231	520.237637	8.812890
6.804161	517.671194	8.817907
6.891365	513.518676	8.822925
6.758001	514.849837	8.827943
7.055971	509.879661	8.832960
7.063368	516.863880	8.837978
6.921945	522.769945	8.842995
6.966063	523.120278	8.848013
6.798019	521.311388	8.853031
6.707960	516.216588	8.858048
6.364824	515.904966	8.863066
6.442601	513.942778	8.868083
6.841642	531.166794	8.873101
6.641967	543.553755	8.878119
6.921442	544.012904	8.883136
6.804886	562.199755	8.888154
6.899582	548.285647	8.893171
6.789760	546.087181	8.898189
6.740112	546.905192	8.903207
7.068504	545.163741	8.908224
6.830321	547.799690	8.913242
7.005668	550.744399	8.918259
7.235317	537.282421	8.923277
7.025714	543.072618	8.928295
7.182422	549.119647	8.933312
6.915015	546.392796	8.938330
7.004252	551.251784	8.943347
7.206368	545.139182	8.948365
7.016849	546.275037	8.953383
7.384831	536.735842	8.958400
7.285527	543.737608	8.963418
7.290789	542.184473	8.968435
7.269606	525.966039	8.973453
7.041720	534.638158	8.978471
6.940980	516.769602	8.983488
6.631999	514.983510	8.988506
6.692309	534.076953	8.993523
7.220042	532.918985	8.998541
6.714417	542.373584	9.003559
6.673844	531.668865	9.008576
6.808449	549.885640	9.013594
6.593611	553.108373	9.018611
7.036412	554.942345	9.023629
6.966370	551.656988	9.028647
7.129092	543.182626	9.033664
7.137759	545.061080	9.038682
7.081524	537.721425	9.043699
7.026858	548.369090	9.048717
6.920786	554.489560	9.053735
6.892229	551.671770	9.058752
7.022812	572.800423	9.063770
7.182719	584.820177	9.068787
7.603496	583.432976	9.073805
7.261185	571.048579	9.078823
7.218896	561.989790	9.083840
7.149837	554.033165	9.088858
7.141590	555.127452	9.093875
7.065987	543.085056	9.098893
6.919372	566.085062	9.103911
7.136130	574.063265	9.108928
7.306876	573.161595	9.113946
7.329996	569.368998	9.118963
7.599238	578.016755	9.123981
7.460506	574.434040	9.128999
7.289649	562.566888	9.134016
7.260803	548.413301	9.139034
7.144486	552.872970	9.144051
6.970842	542.047051	9.149069
7.099742	561.271293	9.154087
7.066534	584.592780	9.159104
7.504647	588.122208	9.164122
7.342044	592.706053	9.169139
7.225467	578.786385	9.174157
7.297142	579.069086	9.179175
7.427658	577.706628	9.184192
7.646373	581.766219	9.189210
7.142924	570.420671	9.194227
7.378674	558.534056	9.199245
7.383044	566.286081	9.204263
7.381997	559.017695	9.209280
7.406473	556.034673	9.214298
7.567933	549.154420	9.219315
7.110288	541.915540	9.224333
7.111798	554.319156	9.229351
7.373154	569.822484	9.234368
7.364039	578.915676	9.239386
7.100077	582.105300	9.244403
7.155711	576.782208	9.249421
6.935476	589.135406	9.254439
7.177526	584.886131	9.259456
7.115071	593.017158	9.264474
7.063582	592.487094	9.269491
7.382902	585.399077	9.274509
7.028808	587.051119	9.279527
7.391346	586.714399	9.284544
7.385559	580.899380	9.289562
7.492916	586.306763	9.294579
7.397241	596.719843	9.299597
7.412990	596.778364	9.304615
7.474839	603.357927	9.309632
7.489661	598.137913	9.314650
7.521718	604.352879	9.319667
7.759846	593.954852	9.324685
7.615955	601.689769	9.329703
7.507540	587.175248	9.334720
7.659155	589.485024	9.339738
7.380290	591.389055	9.344755
7.549186	582.153353	9.349773
7.529804	588.980249	9.354791
7.507234	583.137988	9.359808
7.493325	588.674742	9.364826
7.026567	585.695740	9.369843
7.411410	585.613261	9.374861
7.804275	610.924738	9.379879
7.956759	606.189658	9.384896
7.722439	592.150582	9.389914
7.245615	596.787732	9.394931
7.320800	591.751903	9.399949
7.691590	608.188001	9.404967
7.666285	598.216211	9.409984
7.778667	587.099434	9.415002
7.469655	585.677152	9.420019
7.488039	584.606502	9.425037
7.239130	606.356770	9.430055
7.496490	619.959572	9.435072
7.989956	623.311879	9.440090
8.055105	619.482409	9.445107
7.627678	593.503643	9.450125
7.498738	592.904600	9.455143
7.634681	599.867222	9.460160
7.801748	607.720803	9.465178
7.959550	608.611799	9.470195
7.803876	593.149445	9.475213
7.147839	594.387785	9.480231
7.466493	588.309737	9.485248
7.588620	599.021708	9.490266
7.697132	624.316036	9.495283
7.992221	615.758648	9.500301
8.023992	618.588833	9.505319
7.523275	612.012139	9.510336
7.923063	599.786825	9.515354
7.702494	603.416545	9.520371
7.738999	611.166136	9.525389
7.841183	605.318505	9.530407
7.881292	602.515436	9.535424
7.932131	588.863513	9.540442
7.629636	589.341389	9.545459
7.742966	577.742364	9.550477
7.753970	588.171465	9.555495
7.497839	592.861202	9.560512
7.812497	604.293883	9.565530
8.135725	611.652256	9.570547
7.970931	607.463319	9.575565
7.842025	589.947695	9.580583
7.709127	590.890567	9.585600
7.935566	589.293890	9.590618
7.580790	594.841708	9.595635
7.942336	592.827597	9.600653
8.165038	607.076749	9.605671
8.025716	598.023444	9.610688
7.667244	584.669341	9.615706
7.726722	588.477345	9.620723
7.751782	588.109796	9.625741
8.015823	598.591954	9.630759
7.875113	606.280096	9.635776
8.173200	601.772979	9.640794
7.763620	605.712329	9.645811
7.718801	595.393828	9.650829
7.909293	592.577030	9.655847
8.103462	607.416226	9.660864
8.177218	589.273714	9.665882
7.488150	599.825795	9.670899
7.967067	611.857604	9.675917
7.993362	615.347435	9.680935
7.970234	627.851818	9.685952
8.257446	610.545802	9.690970
7.641099	607.013076	9.695987
8.034648	606.469298	9.701005
8.030265	620.164854	9.706023
7.939496	627.282648	9.711040
8.017949	622.704948	9.716058
7.902629	624.699259	9.721075
7.858823	611.891255	9.726093
8.154022	613.032037	9.731111
8.177079	618.564365	9.736128
8.193155	604.443552	9.741146
8.090292	617.474595	9.746163
8.307510	619.031539	9.751181
8.203901	608.372905	9.756199
7.928516	600.865829	9.761216
7.965250	597.767408	9.766234
7.964348	600.460987	9.771251
8.215010	615.305517	9.776269
8.307775	613.864074	9.781287
8.026797	619.605475	9.786304
8.109361	606.573184	9.791322
8.235801	613.931898	9.796339
8.039996	605.496969	9.801357
8.210722	603.671154	9.806375
8.026498	611.420319	9.811392
8.115781	623.846388	9.816410
7.764503	627.912405	9.821427
7.777520	618.744068	9.826445
8.048709	616.487943	9.831463
8.265505	616.137420	9.836480
8.317506	610.909388	9.841498
8.348861	614.687702	9.846515
7.807759	621.567074	9.851533
8.281294	621.707003	9.856551
8.174899	628.316151	9.861568
8.116056	620.790010	9.866586
7.981804	611.374507	9.871603
8.012057	613.004269	9.876621
7.703298	616.289869	9.881639
7.663480	611.122574	9.886656
8.121700	630.329383	9.891674
8.227474	641.635321	9.896691
8.468090	655.153929	9.901709
8.803871	644.449426	9.906727
8.224164	640.130753	9.911744
8.566078	616.950971	9.916762
8.092747	624.246629	9.921779
8.118066	605.350032	9.926797
8.380600	622.888882	9.931815
8.396136	644.272430	9.936832
8.403177	631.431011	9.941850
8.387106	622.422176	9.946867
8.410595	632.072806	9.951885
8.249403	612.880012	9.956903
8.306552	623.398344	9.961920
8.483129	634.346870	9.966938
8.198474	633.249044	9.971955
8.195862	639.170003	9.976973
8.542054	653.739381	9.981991
8.276076	659.027314	9.987008
8.002528	654.147208	9.992026
8.485708	648.583782	9.997043
8.631451	655.973672	10.002061
8.696138	648.069784	10.007079
8.476522	652.163746	10.012096
8.533222	652.863516	10.017114
8.437352	657.525214	10.022131
8.255766	646.002919	10.027149
8.478145	639.421659	10.032167
8.560883	653.491460	10.037184
8.803948	648.025578	10.042202
8.701884	649.344788	10.047219
8.279292	634.494118	10.052237
8.508001	636.459526	10.057255
8.610431	637.877103	10.062272
8.530378	633.211835	10.067290
8.487249	626.697385	10.072307
8.461010	634.369478	10.077325
8.670575	629.701618	10.082343
8.467522	649.113480	10.087360
8.591083	636.651452	10.092378
8.565155	637.169536	10.097395
8.147245	650.228461	10.102413
8.766549	652.255581	10.107431
8.656550	661.142698	10.112448
8.876368	648.895717	10.117466
8.625697	627.489538	10.122483
8.247365	627.041727	10.127501
8.545450	637.810853	10.132519
8.497595	652.140085	10.137536
8.774607	663.973944	10.142554
8.662293	646.456400	10.147571
8.354637	643.931325	10.152589
8.704758	650.002820	10.157607
8.536122	642.405458	10.162624
8.645358	648.147729	10.167642
8.702360	649.661972	10.172659
8.557721	661.074353	10.177677
8.858686	653.162810	10.182695
8.876569	655.078036	10.187712
8.670220	647.343622	10.192730
9.013782	649.352836	10.197747
8.770228	652.167316	10.202765
8.974267	657.782329	10.207783
8.732076	652.167936	10.212800
8.601698	635.926199	10.217818
8.762099	651.018513	10.222835
8.714567	657.538334	10.227853
9.030767	646.909199	10.232871
8.617287	662.482119	10.237888
8.897641	662.888577	10.242906
8.802781	654.565165	10.247923
8.496256	656.372513	10.252941
9.091941	647.410476	10.257959
8.749766	659.001536	10.262976
8.981339	644.536664	10.267994
8.987577	648.185991	10.273011
8.698348	649.244055	10.278029
8.946217	649.228101	10.283047
8.575889	663.380949	10.288064
8.478269	647.465224	10.293082
8.577489	641.016796	10.298099
8.271501	643.921303	10.303117
8.687738	644.325479	10.308135
8.794703	654.781771	10.313152
8.248979	659.433277	10.318170
8.985003	656.128453	10.323187
9.046882	681.120202	10.328205
9.043148	673.467232	10.333223
9.097622	665.764202	10.338240
8.945514	672.901404	10.343258
8.866098	652.951277	10.348275
8.724953	663.206001	10.353293
8.995605	656.992380	10.358311
8.884280	669.797641	10.363328
9.377933	671.917662	10.368346
9.132010	662.727828	10.373363
8.774661	654.032905	10.378381
9.078010	660.327745	10.383399
9.023486	660.578359	10.388416
8.889388	660.473879	10.393434
9.219949	665.953539	10.398451
8.952125	662.262041	10.403469
9.071013	666.109943	10.408487
9.204466	674.618607	10.413504
8.953627	657.285824	10.418522
9.228208	662.621118	10.423539
8.882710	654.743779	10.428557
9.014674	664.871300	10.433575
9.301330	680.868898	10.438592
9.122963	668.603171	10.443610
9.421421	660.035656	10.448627
8.991492	654.708935	10.453645
9.060381	649.668420	10.458663
9.043052	644.157102	10.463680
9.014483	660.768484	10.468698
9.298641	670.365827	10.473715
9.027675	673.028274	10.478733
9.310120	674.720876	10.483751
9.326159	680.703817	10.488768
8.848542	666.487298	10.493786
9.176477	668.626143	10.498803
9.089068	673.515837	10.503821
9.205390	666.931721	10.508839
9.041907	679.528520	10.513856
9.012496	669.730758	10.518874
9.302809	668.411952	10.523891
9.375966	675.679322	10.528909
9.243357	663.772410	10.533927
9.100581	672.998062	10.538944
9.084428	671.433002	10.543962
9.227789	667.794300	10.548979
9.091139	679.512605	10.553997
9.010395	671.438481	10.559015
9.216251	667.936965	10.564032
8.964127	664.961645	10.569050
9.174924	658.109799	10.574067
9.192986	674.075215	10.579085
9.292953	671.268737	10.584103
9.053859	676.553120	10.589120
9.276090	690.880858	10.594138
9.582299	700.482745	10.599155
9.484178	700.600036	10.604173
9.384266	695.157358	10.609191
9.148525	683.905454	10.614208
8.839428	702.656186	10.619226
9.352098	708.737844	10.624243
9.083211	716.204350	10.629261
9.335483	699.972034	10.634279
9.673933	700.181523	10.639296
9.464430	704.225607	10.644314
9.264501	697.581357	10.649331
9.272136	699.114785	10.654349
9.363563	704.157384	10.659367
9.593114	697.212083	10.664384
9.297029	715.656992	10.669402
9.710139	714.119006	10.674419
9.718739	704.643919	10.679437
9.610671	700.739528	10.684455
9.620065	701.197455	10.689472
9.662498	708.557994	10.694490
9.892118	704.372836	10.699507
9.445996	708.622530	10.704525
9.660242	707.684240	10.709543
9.822344	701.742826	10.714560
9.799617	707.275273	10.719578
10.095648	700.478012	10.724595
10.153187	685.903400	10.729613
9.735078	675.710891	10.734631
9.663243	680.869424	10.739648
9.800221	687.856516	10.744666
9.832527	672.056968	10.749683
9.560848	668.160236	10.754701
9.560153	665.767175	10.759719
9.952079	671.825275	10.764736
9.574783	675.212356	10.769754
9.949071	674.263169	10.774771
9.600898	667.573560	10.779789
9.671943	677.722276	10.784807
9.852634	666.209673	10.789824
9.588317	671.524202	10.794842
9.823524	662.692875	10.799859
10.138961	670.405258	10.804877
9.786931	666.376259	10.809895
10.144041	673.317421	10.814912
9.670869	676.547935	10.819930
9.716951	659.922151	10.824947
9.731755	663.321684	10.829965
9.822574	667.694114	10.834983
9.476715	674.045367	10.840000
9.703546	666.447590	10.845018
9.656961	673.443360	10.850035
9.573866	664.477657	10.855053
9.623640	664.850676	10.860071
10.035129	667.361177	10.865088
9.743495	659.014582	10.870106
9.875433	666.636934	10.875123
9.605065	672.209111	10.880141
9.636322	673.592103	10.885159
9.919326	672.210932	10.890176
9.729195	668.860371	10.895194
9.582654	667.561207	10.900211
9.283626	671.372678	10.905229
9.600761	675.874022	10.910247
9.705744	689.653517	10.915264
9.938143	714.987550	10.920282
9.992028	713.906694	10.925299
9.848001	701.478993	10.930317
9.914749	706.046423	10.935335
9.952533	701.993540	10.940352
10.099557	702.989062	10.945370
9.920723	712.113430	10.950387
9.682907	705.595495	10.955405
9.764969	703.189541	10.960423
10.211492	701.942243	10.965440
10.060222	711.626527	10.970458
10.082058	702.780248	10.975475
9.768742	694.825732	10.980493
9.979236	701.163685	10.985511
10.033849	700.251185	10.990528
10.031959	704.443015	10.995546
10.089422	704.939842	11.000563
9.966006	704.561399	11.005581
10.122687	710.016570	11.010599
9.992615	699.991862	11.015616
10.068778	708.432861	11.020634
10.277846	708.021714	11.025651
10.385801	715.388748	11.030669
10.050176	711.323370	11.035687
10.225943	709.817324	11.040704
10.105763	717.581840	11.045722
9.686895	706.630215	11.050739
10.263423	703.151969	11.055757
10.172281	695.876462	11.060775
10.400396	704.792065	11.065792
9.706457	704.574034	11.070810
10.220071	714.639896	11.075827
10.013672	707.297420	11.080845
9.931149	709.555272	11.085863
10.093245	695.668764	11.090880
10.119647	708.863038	11.095898
10.183945	713.005160	11.100915
10.445800	726.168609	11.105933
10.428318	731.708662	11.110951
10.611415	705.096228	11.115968
10.103883	718.699556	11.120986
10.423375	700.540119	11.126003
10.332903	699.885216	11.131021
10.459155	701.487216	11.136039
10.278367	697.980406	11.141056
9.860850	706.619501	11.146074
10.138821	706.819894	11.151091
10.472875	705.737023	11.156109
10.165898	722.226004	11.161127
10.618944	719.051971	11.166144
10.257179	731.999046	11.171162
10.540228	719.733786	11.176179
10.459780	714.075715	11.181197
9.987612	711.963281	11.186215
10.244571	719.816630	11.191232
10.532737	728.437332	11.196250
10.424854	729.979422	11.201267
10.377342	730.423530	11.206285
10.187417	731.532008	11.211303
10.528362	737.510976	11.216320
10.192562	735.937522	11.221338
10.349898	731.491120	11.226355
10.514467	735.178760	11.231373
10.079524	747.308160	11.236391
10.377642	737.985176	11.241408
10.337858	741.040755	11.246426
10.408922	729.522209	11.251443
10.350330	735.297955	11.256461
9.979915	733.031521	11.261479
10.649160	732.589597	11.266496
11.039938	758.528623	11.271514
10.825017	739.594606	11.276531
11.097368	733.356661	11.281549
10.603301	749.466422	11.286567
10.710391	731.732140	11.291584
10.330896	737.175549	11.296602
10.646735	729.642054	11.301619
10.808451	724.287801	11.306637
10.402414	733.670163	11.311655
10.700005	728.010431	11.316672
10.570195	739.545399	11.321690
10.914691	733.462040	11.326707
10.967013	736.341007	11.331725
10.604819	736.888880	11.336743
10.910587	724.251224	11.341760
10.829450	730.773087	11.346778
10.477562	731.935885	11.351795
10.508288	737.942105	11.356813
10.399915	734.816561	11.361831
10.617948	731.642786	11.366848
10.582017	733.632553	11.371866
10.483125	748.917492	11.376883
11.163696	767.594702	11.381901
10.696379	758.129540	11.386919
10.851445	761.897681	11.391936
10.954537	767.722691	11.396954
10.485030	763.805190	11.401971
10.944183	761.879930	11.406989
11.022010	759.844683	11.412007
10.855187	758.726687	11.417024
10.830422	754.935070	11.422042
10.732538	765.511594	11.427059
11.023364	755.146672	11.432077
10.926796	768.820493	11.437095
11.035518	762.296834	11.442112
10.732346	747.881756	11.447130
10.808960	759.457613	11.452147
11.026708	762.762519	11.457165
10.737823	772.839795	11.462183
10.716217	763.943978	11.467200
11.012882	760.962089	11.472218
10.795072	758.497037	11.477235
10.938434	758.675784	11.482253
10.600747	767.916382	11.487271
10.760942	767.411950	11.492288
10.804029	759.143723	11.497306
10.951400	769.160320	11.502323
11.103573	767.764449	11.507341
10.960104	765.946253	11.512359
11.084238	758.663482	11.517376
10.718323	761.350196	11.522394
10.566135	769.560504	11.527411
10.912532	772.689651	11.532429
10.955246	791.078662	11.537447
11.090123	788.204200	11.542464
11.413658	791.924432	11.547482
11.392237	793.567969	11.552499
11.227505	782.597714	11.557517
11.333103	774.444325	11.562535
11.340833	762.149738	11.567552
11.307361	752.776244	11.572570
10.953366	762.857975	11.577587
11.228450	762.663439	11.582605
10.733669	758.533026	11.587623
10.761171	759.559324	11.592640
11.158669	776.907571	11.597658
11.304283	794.041796	11.602675
11.242180	785.408915	11.607693
11.192748	786.851207	11.612711
11.240985	787.009067	11.617728
11.471518	783.353570	11.622746
10.992756	788.364066	11.627763
11.333665	785.489606	11.632781
11.280982	789.313341	11.637799
11.499707	774.908827	11.642816
11.433090	780.115341	11.647834
11.531017	782.628966	11.652851
11.780671	774.186855	11.657869
11.370290	772.009093	11.662887
11.396720	765.749580	11.667904
11.292080	760.785336	11.672922
11.022651	759.204061	11.677939
11.445422	773.266197	11.682957
11.237202	782.044340	11.687975
11.650449	783.170450	11.692992
11.725448	776.829100	11.698010
11.348307	763.746876	11.703027
11.494616	762.325995	11.708045
11.286395	761.878311	11.713063
11.554701	782.454070	11.718080
11.388066	768.001648	11.723098
11.433564	775.492399	11.728115
11.582972	779.559067	11.733133
11.851804	782.790389	11.738151
11.632676	781.047675	11.743168
11.612173	762.208449	11.748186
11.264474	762.430557	11.753203
11.387041	752.432755	11.758221
11.216018	769.769646	11.763239
11.436153	774.230069	11.768256
11.889880	775.757689	11.773274
11.582313	782.318369	11.778291
11.518590	784.413113	11.783309
11.618792	781.570952	11.788327
11.616539	789.494136	11.793344
11.564461	781.898602	11.798362
11.605575	777.575115	11.803379
12.072592	785.379221	11.808397
11.769127	795.587246	11.813415
11.599137	776.990977	11.818432
11.550634	767.798668	11.823450
11.309426	779.781136	11.828467
11.816995	773.874716	11.833485
11.782888	775.646113	11.838503
12.012937	776.224443	11.843520
12.081667	772.381353	11.848538
11.497588	777.215974	11.853555
11.659975	773.392834	11.858573
11.719369	776.056897	11.863591
11.567039	780.980578	11.868608
11.951727	781.146016	11.873626
11.706413	788.848582	11.878643
11.669249	779.978157	11.883661
11.815260	772.007627	11.888679
11.828490	785.748344	11.893696
11.953661	778.806084	11.898714
11.920856	789.423240	11.903731
11.874303	789.050004	11.908749
11.928894	791.355473	11.913767
11.740835	794.088773	11.918784
11.687113	786.121522	11.923802
11.833486	783.330973	11.928819
11.646935	789.509121	11.933837
11.685191	786.649838	11.938855
11.831900	790.352843	11.943872
12.125295	776.415435	11.948890
11.786295	781.596501	11.953907
11.828632	774.145971	11.958925
11.567064	775.926812	11.963943
11.391257	787.146635	11.968960
12.005116	794.895382	11.973978
11.871803	812.690777	11.978995
12.081611	810.206618	11.984013
12.448522	808.989198	11.989031
12.256718	813.896188	11.994048
12.535433	806.292032	11.999066
12.096002	792.437726	12.004083
12.384521	779.526149	12.009101
12.075513	782.222357	12.014119
11.774607	782.509161	12.019136
12.081771	777.304840	12.024154
12.112305	781.373046	12.029171
11.881141	780.683328	12.034189
12.089609	792.639126	12.039207
12.238160	806.597815	12.044224
12.625455	803.770795	12.049242
12.221469	800.493137	12.054259
12.005323	788.185337	12.059277
12.321977	783.240820	12.064295
11.965937	783.052170	12.069312
12.267722	793.636671	12.074330
12.270316	802.807280	12.079347
12.078348	817.827990	12.084365
12.159553	811.311613	12.089383
11.864029	816.489836	12.094400
12.198859	806.598237	12.099418
12.064740	810.660201	12.104435
12.039731	813.284487	12.109453
12.475683	814.379489	12.114471
12.185166	821.197955	12.119488
12.326132	829.147091	12.124506
12.131269	816.095714	12.129523
12.238066	810.580259	12.134541
12.419694	805.289605	12.139559
12.148922	810.195079	12.144576
12.485650	805.067346	12.149594
12.549827	816.077088	12.154611
12.095686	814.646981	12.159629
12.112251	809.332628	12.164647
12.253286	818.448286	12.169664
12.767153	827.823744	12.174682
12.718783	821.293938	12.179699
12.488396	820.378930	12.184717
12.851688	807.461862	12.189735
12.758547	808.940509	12.194752
12.728313	796.570489	12.199770
12.782089	809.975448	12.204787
12.494093	800.562502	12.209805
12.651864	791.642143	12.214823
12.420822	801.584113	12.219840
12.628757	799.075663	12.224858
12.522568	813.642305	12.229875
12.376824	805.403487	12.234893
12.726106	796.211754	12.239911
12.641792	806.592198	12.244928
12.866627	795.024771	12.249946
12.696233	810.450896	12.254963
12.591610	809.915040	12.259981
12.723214	806.911019	12.264999
12.495302	809.883349	12.270016
12.783365	805.299987	12.275034
12.851216	800.243850	12.280051
12.935727	798.265554	12.285069
12.715743	799.409118	12.290087
12.829173	804.210555	12.295104
12.732987	798.211410	12.300122
12.999384	803.861440	12.305139
12.863283	801.696803	12.310157
12.859586	795.897300	12.315175
12.797311	805.024899	12.320192
12.787994	804.239474	12.325210
12.901340	810.759935	12.330227
12.891573	810.020049	12.335245
13.178181	800.322416	12.340263
13.034532	808.639387	12.345280
13.020862	808.402425	12.350298
13.282549	805.281057	12.355315
13.010431	807.132925	12.360333
13.175135	792.798531	12.365351
13.035632	797.061151	12.370368
12.885561	775.648080	12.375386
12.914293	768.446807	12.380403
12.869623	767.446593	12.385421
13.050217	750.357513	12.390439
12.878774	770.556199	12.395456
12.916028	777.809180	12.400474
12.941645	793.146803	12.405491
12.668415	811.640600	12.410509
12.947276	806.680278	12.415527
12.639173	799.412233	12.420544
12.722640	805.061790	12.425562
12.977614	795.561679	12.430579
12.652504	813.107319	12.435597
13.077397	795.001601	12.440615
13.034661	805.391510	12.445632
13.031692	807.716729	12.450650
13.225297	808.783090	12.455667
13.074573	806.180193	12.460685
13.270663	800.298075	12.465703
13.247106	800.404226	12.470720
13.007731	799.742631	12.475738
13.265986	807.866239	12.480755
13.000124	803.102807	12.485773
13.242396	804.575820	12.490791
13.231845	806.614150	12.495808
12.915276	789.261769	12.500826
13.191435	810.352915	12.505843
13.271234	826.016011	12.510861
13.436499	826.107492	12.515879
13.119913	828.507961	12.520896
13.442084	829.526901	12.525914
13.411187	819.115905	12.530931
13.114477	814.632522	12.535949
13.319369	816.098921	12.540967
13.234600	841.169780	12.545984
13.169587	834.079425	12.551002
13.556595	832.645529	12.556019
13.315960	838.982805	12.561037
13.427842	833.084084	12.566055
13.384055	836.156088	12.571072
13.344842	835.161660	12.576090
13.517318	837.057365	12.581107
13.766992	843.226822	12.586125
13.952249	838.168000	12.591143
13.280573	813.742363	12.596160
13.139907	813.402589	12.601178
13.405660	815.575742	12.606195
13.396122	834.218282	12.611213
13.451976	839.064278	12.616231
13.534327	840.677878	12.621248
13.470767	833.931321	12.626266
13.469300	832.071150	12.631283
13.296119	836.764277	12.636301
13.812582	828.845079	12.641319
13.497512	841.041147	12.646336
13.569821	839.731093	12.651354
13.585784	842.328340	12.656371
13.539873	826.662012	12.661389
13.626987	822.649954	12.666407
13.510756	833.655472	12.671424
13.631438	842.109459	12.676442
13.710652	830.018324	12.681459
13.541093	843.223840	12.686477
13.874427	832.103341	12.691495
13.552721	833.987221	12.696512
13.246451	831.577517	12.701530
13.552761	820.670513	12.706547
13.457152	836.071709	12.711565
13.782298	853.905347	12.716583
13.859998	861.292999	12.721600
13.948360	868.436412	12.726618
14.224810	852.494184	12.731635
13.826899	855.916398	12.736653
13.646151	840.569731	12.741671
13.550195	838.675182	12.746688
13.721169	844.436847	12.751706
14.129616	852.845845	12.756723
13.977123	868.514109	12.761741
14.013211	857.485225	12.766759
13.819630	854.899637	12.771776
13.838022	862.409867	12.776794
14.080394	858.959647	12.781811
14.009799	865.735886	12.786829
14.089717	855.443341	12.791847
13.987306	846.463994	12.796864
14.019082	846.423623	12.801882
14.015417	831.347259	12.806899
14.129106	855.488052	12.811917
14.001381	835.856349	12.816935
13.738299	841.199467	12.821952
13.746080	853.648442	12.826970
14.136804	859.951461	12.831987
14.120424	859.048715	12.837005
14.091094	850.080907	12.842023
14.061273	859.995370	12.847040
13.741540	859.208491	12.852058
13.907576	857.494821	12.857075
13.636921	866.358121	12.862093
13.849955	866.308855	12.867111
13.771542	855.653562	12.872128
13.829627	854.892619	12.877146
13.936923	863.261837	12.882163
14.221831	878.737770	12.887181
14.270151	879.088696	12.892199
14.324554	880.088119	12.897216
15.107589	873.056392	12.902234
15.141739	848.735284	12.907251
14.739929	856.470240	12.912269
14.705989	842.077106	12.917287
14.817957	849.415396	12.922304
14.645404	848.698276	12.927322
14.966659	829.788123	12.932339
14.502373	815.080366	12.937357
14.452990	808.491885	12.942375
14.503673	807.490278	12.947392
14.366023	806.397571	12.952410
14.607423	803.784787	12.957427
14.707570	820.122750	12.962445
14.463664	812.320357	12.967463
14.566477	799.159773	12.972480
14.241333	811.978836	12.977498
14.677094	808.916876	12.982515
14.597745	803.499889	12.987533
14.969207	795.711936	12.992551
14.542447	799.881893	12.997568
14.167073	807.660283	13.002586
14.848822	799.753543	13.007603
14.815925	814.964857	13.012621
14.512734	812.660339	13.017639
14.917999	809.025953	13.022656
14.519742	805.332849	13.027674
14.563360	805.170067	13.032691
14.257171	800.407199	13.037709
14.511630	810.467140	13.042727
14.519245	807.256086	13.047744
14.103730	813.166618	13.052762
14.450523	801.702634	13.057779
14.226737	805.740444	13.062797
14.301509	801.016375	13.067815
14.652032	822.726248	13.072832
14.352558	844.702003	13.077850
14.581895	840.318660	13.082867
14.429860	849.564841	13.087885
14.546508	846.947276	13.092903
14.707945	835.338336	13.097920
14.402403	842.959755	13.102938
14.942509	843.774992	13.107955
14.588601	845.758668	13.112973
14.435377	842.804267	13.117991
14.556736	849.278349	13.123008
14.542852	860.185687	13.128026
15.071907	867.562130	13.133043
14.866666	882.003693	13.138061
14.937683	880.425586	13.143079
14.801676	869.522951	13.148096
14.564261	881.797935	13.153114
15.183688	873.172834	13.158131
15.236638	874.145532	13.163149
15.061976	880.761051	13.168167
14.905097	883.025508	13.173184
14.868529	881.525209	13.178202
14.989715	874.259010	13.183219
14.845335	882.088818	13.188237
14.862572	873.528589	13.193255
15.077470	873.839785	13.198272
14.671414	881.962008	13.203290
14.774177	884.471505	13.208307
14.974064	870.293994	13.213325
15.077491	871.798029	13.218343
15.203733	874.055062	13.223360
14.933162	873.559223	13.228378
15.116916	874.915163	13.233395
15.132275	885.748603	13.238413
15.253157	890.399647	13.243431
15.452742	883.680832	13.248448
15.221396	894.397394	13.253466
15.119402	880.012125	13.258483
15.726347	877.889818	13.263501
15.414072	885.527723	13.268519
15.423275	883.094417	13.273536
15.511896	878.072217	13.278554
15.280125	875.431332	13.283571
15.414211	877.578031	13.288589
15.501084	877.114054	13.293607
15.609387	875.048760	13.298624
15.359370	882.868470	13.303642
15.438545	881.658640	13.308659
15.389822	880.751790	13.313677
15.200236	872.429448	13.318695
15.479761	878.880161	13.323712
15.316616	874.727585	13.328730
15.195971	878.098670	13.333747
15.449836	873.785465	13.338765
15.214105	867.916225	13.343783
15.281320	863.505344	13.348800
15.042153	872.706105	13.353818
15.127197	896.334455	13.358835
15.693732	905.480032	13.363853
15.387435	895.466998	13.368871
15.882291	887.836729	13.373888
15.872972	906.784193	13.378906
16.049261	899.404562	13.383923
15.699837	879.316605	13.388941
15.702892	872.515133	13.393959
15.777129	877.831453	13.398976
15.666105	873.944236	13.403994
15.872265	877.631729	13.409011
15.776597	867.980693	13.414029
15.202063	878.064107	13.419047
15.612118	874.813302	13.424064
15.494164	881.108673	13.429082
15.661307	891.405108	13.434099
15.793860	902.240253	13.439117
15.363340	906.693688	13.444135
15.740264	900.498229	13.449152
16.297996	913.118534	13.454170
16.289741	917.087691	13.459187
16.011649	904.754016	13.464205
15.642923	897.045620	13.469223
15.965632	880.389728	13.474240
15.731187	897.392614	13.479258
16.070596	899.668550	13.484275
16.069779	892.686635	13.489293
15.624619	887.180881	13.494311
16.267548	884.956382	13.499328
16.072259	879.226298	13.504346
15.759606	876.615902	13.509363
15.764107	879.396516	13.514381
15.668652	906.019197	13.519399
16.081829	899.630769	13.524416
16.005201	902.499389	13.529434
15.690185	909.197159	13.534451
15.938019	909.886907	13.539469
15.995067	915.153333	13.544487
16.109142	903.069764	13.549504
15.924361	907.830961	13.554522
16.121406	907.826654	13.559539
16.049705	898.456633	13.564557
15.540384	907.427495	13.569575
16.075755	903.328941	13.574592
16.010135	911.159132	13.579610
15.777883	910.200142	13.584627
16.195548	915.150126	13.589645
16.416496	927.617469	13.594663
16.436607	928.068319	13.599680
16.393050	920.289249	13.604698
16.125155	915.417671	13.609715
16.286596	910.168303	13.614733
16.046427	935.842268	13.619751
16.257232	930.265101	13.624768
16.136047	935.408452	13.629786
16.190429	927.212864	13.634803
16.317752	928.470473	13.639821
16.266574	941.148913	13.644839
16.731635	929.341718	13.649856
16.813257	928.879788	13.654874
16.597725	937.271296	13.659891
16.795070	929.177062	13.664909
16.456862	924.233058	13.669927
16.374424	914.266076	13.674944
16.475267	913.956654	13.679962
16.349878	921.015158	13.684979
16.982425	920.842442	13.689997
16.579655	930.025988	13.695015
16.536302	905.390287	13.700032
16.354945	906.872894	13.705050
16.181354	933.821083	13.710067
16.630044	925.496566	13.715085
16.519097	932.947705	13.720103
16.397522	922.770880	13.725120
16.443280	937.189124	13.730138
16.465927	932.841682	13.735155
16.767677	935.217139	13.740173
16.429593	943.769235	13.745191
16.444319	931.375734	13.750208
16.519667	928.327647	13.755226
16.598072	932.102200	13.760243
16.480810	930.029495	13.765261
16.728214	932.962469	13.770279
16.933284	945.303533	13.775296
16.852362	934.630886	13.780314
16.857908	932.327880	13.785331
17.060604	918.034919	13.790349
16.971552	925.088994	13.795367
16.669259	924.281712	13.800384
16.812742	923.649152	13.805402
17.394657	936.230250	13.810419
17.076095	920.928910	13.815437
17.056272	927.788308	13.820455
17.074836	929.947216	13.825472
17.240190	916.225300	13.830490
16.934663	916.816759	13.835507
16.972743	899.905567	13.840525
17.091627	914.269390	13.845543
16.720217	922.716762	13.850560
17.098563	909.596365	13.855578
17.257283	917.700659	13.860595
17.059543	911.227974	13.865613
17.056333	923.147016	13.870631
17.121016	914.935363	13.875648
17.043401	906.888547	13.880666
17.284852	904.841200	13.885683
17.233074	904.745946	13.890701
17.107514	922.880881	13.895719
17.149155	919.351828	13.900736
17.210377	907.792262	13.905754
16.990348	916.951507	13.910771
16.979567	919.020594	13.915789
16.977399	913.449498	13.920807
17.228456	916.258459	13.925824
17.421002	920.526861	13.930842
17.251843	939.486609	13.935859
17.631517	928.492614	13.940877
17.608559	930.554267	13.945895
17.432246	929.166609	13.950912
17.356467	911.335784	13.955930
16.809175	919.278643	13.960947
17.334296	920.534284	13.965965
17.812971	933.928576	13.970983
17.489071	929.260311	13.976000
17.247859	927.870781	13.981018
17.017379	931.225192	13.986035
17.393944	931.943070	13.991053
17.461606	945.631832	13.996071
17.361958	947.738438	14.001088
17.640374	939.644776	14.006106
17.629833	954.080212	14.011123
17.269633	940.130211	14.016141
17.445526	953.082309	14.021159
17.739463	944.067717	14.026176
18.191139	936.635869	14.031194
17.962641	946.531652	14.036211
18.050355	937.793822	14.041229
17.433219	929.359257	14.046247
17.297574	940.498550	14.051264
17.619397	933.783132	14.056282
17.482896	942.720945	14.061299
17.835252	945.433065	14.066317
17.844580	943.764767	14.071335
17.857073	955.758589	14.076352
18.101377	942.388310	14.081370
17.905186	950.431998	14.086387
18.065963	944.919580	14.091405
17.688967	947.188930	14.096423
17.517068	947.067667	14.101440
17.916171	955.962836	14.106458
17.719783	947.121579	14.111475
18.166614	950.848243	14.116493
18.179904	954.634547	14.121511
17.637173	942.296943	14.126528
17.897512	938.681556	14.131546
17.766541	954.195587	14.136563
18.097055	935.585106	14.141581
18.048263	945.603925	14.146599
17.477603	948.216253	14.151616
18.115757	943.054016	14.156634
17.894183	945.959587	14.161651
17.954369	945.836186	14.166669
18.056071	946.136369	14.171687
18.114211	961.206032	14.176704
17.977450	947.623565	14.181722
17.735840	957.337890	14.186739
18.106618	939.459612	14.191757
18.137703	940.468207	14.196775
17.989683	958.901339	14.201792
18.381407	969.113674	14.206810
18.343332	981.667952	14.211827
18.279725	952.078803	14.216845
17.983911	951.952037	14.221863
18.153361	950.483227	14.226880
18.491960	956.539034	14.231898
18.477179	964.350026	14.236915
18.652008	956.003830	14.241933
19.010417	946.049987	14.246951
18.551943	946.702936	14.251968
18.731961	930.176854	14.256986
18.627619	940.029679	14.262003
18.547493	935.150092	14.267021
18.570019	936.398056	14.272039
18.342105	941.908402	14.277056
18.390390	929.902208	14.282074
18.339468	942.193068	14.287091
18.099514	937.623313	14.292109
18.452889	929.248216	14.297127
18.202044	938.315141	14.302144
18.277785	925.761388	14.307162
17.893593	942.751674	14.312179
18.413126	958.525281	14.317197
18.503532	961.938662	14.322215
18.503277	973.836785	14.327232
18.582953	967.413297	14.332250
18.383003	964.286109	14.337267
18.583101	952.341215	14.342285
18.733077	959.057624	14.347303
18.822318	964.873976	14.352320
18.926406	957.104933	14.357338
18.884355	976.001995	14.362355
18.984529	962.388825	14.367373
19.332915	953.301264	14.372391
18.764176	955.859938	14.377408
19.133990	952.811209	14.382426
18.885738	961.130787	14.387443
19.041950	954.579911	14.392461
19.441459	947.272998	14.397479
18.808216	950.503843	14.402496
19.258859	936.367694	14.407514
18.877357	927.957173	14.412531
18.478268	923.919348	14.417549
18.671282	937.028027	14.422567
18.843877	954.979498	14.427584
19.139856	954.966518	14.432602
18.843126	953.362180	14.437619
19.355476	952.336233	14.442637
19.266854	949.190652	14.447655
19.093019	960.274469	14.452672
19.357269	971.103645	14.457690
19.400633	959.554274	14.462707
19.518724	950.300079	14.467725
19.476314	941.099770	14.472743
19.075412	935.987803	14.477760
19.109018	927.130791	14.482778
18.747233	931.808074	14.487795
18.952868	918.156652	14.492813
19.296688	941.763173	14.497831
19.315880	952.517495	14.502848
19.104127	958.997860	14.507866
19.015367	964.017180	14.512883
19.151392	956.229476	14.517901
19.291447	954.430142	14.522919
19.014374	962.819828	14.527936
19.280533	962.482299	14.532954
19.453124	961.666215	14.537971
19.131783	971.891875	14.542989
19.045284	965.847173	14.548007
18.866079	964.065365	14.553024
19.056042	963.975825	14.558042
19.502327	979.991838	14.563059
19.518051	992.501021	14.568077
19.577911	983.643967	14.573095
19.590254	985.999748	14.578112
19.737362	975.104379	14.583130
19.497738	991.035160	14.588147
19.462139	979.153796	14.593165
19.762445	983.406574	14.598183
19.823036	993.490407	14.603200
19.826238	977.554628	14.608218
19.998725	989.943823	14.613235
19.256389	972.936551	14.618253
19.850856	964.603274	14.623271
19.699539	981.982416	14.628288
19.644739	974.689355	14.633306
19.727722	983.305138	14.638323
19.774061	985.069367	14.643341
20.030818	972.885011	14.648359
19.822732	985.263088	14.653376
19.789384	984.291103	14.658394
19.718206	987.811494	14.663411
19.775742	995.841816	14.668429
20.127663	983.627160	14.673447
19.838705	1001.111931	14.678464
20.085809	979.686082	14.683482
20.162460	988.985487	14.688499
19.803178	987.638491	14.693517
20.375912	983.276498	14.698535
20.268109	987.871479	14.703552
19.790131	976.064993	14.708570
20.023303	970.018242	14.713587
19.860660	977.191573	14.718605
19.977368	983.716079	14.723623
20.016509	976.974926	14.728640
19.903769	978.866411	14.733658
20.089198	978.328870	14.738675
20.009372	982.540937	14.743693
20.063620	983.777758	14.748711
19.738031	988.026898	14.753728
19.889478	978.195410	14.758746
20.010073	975.649601	14.763763
19.971624	983.997110	14.768781
20.193387	997.465994	14.773799
20.036341	1007.296081	14.778816
20.243628	1020.421957	14.783834
20.271116	1008.740744	14.788851
20.219549	1021.371289	14.793869
20.416496	1005.928779	14.798887
20.335097	1012.204975	14.803904
20.409215	1006.885569	14.808922
20.698847	1014.266418	14.813939
20.628388	1012.877005	14.818957
20.495057	999.504721	14.823975
20.739071	1007.582568	14.828992
20.695232	1008.185501	14.834010
20.607347	1008.059605	14.839027
20.616831	1009.973606	14.844045
20.619492	1000.586313	14.849063
21.030462	1001.058585	14.854080
20.650174	1007.670545	14.859098
20.721602	988.286796	14.864115
20.477888	980.498063	14.869133
20.334523	967.054051	14.874151
20.438878	995.797670	14.879168
20.776066	994.770160	14.884186
20.821349	999.724434	14.889203
20.894999	1001.478641	14.894221
21.004502	1010.647649	14.899239
20.524853	1007.735545	14.904256
21.052322	1011.495743	14.909274
21.280345	1007.206847	14.914291
20.558362	1000.723723	14.919309
20.979112	990.197234	14.924327
20.632032	994.227519	14.929344
20.990351	1008.919917	14.934362
20.981013	1005.937377	14.939379
20.970242	1006.717298	14.944397
21.111374	1005.515131	14.949415
20.955738	998.569971	14.954432
20.516950	1006.939954	14.959450
20.990963	1002.270500	14.964467
20.805730	1013.118677	14.969485
21.085508	1012.200047	14.974503
21.160812	1011.130196	14.979520
20.783498	1007.824663	14.984538
20.961156	1007.288011	14.989555
20.923768	1010.209607	14.994573
21.123582	1005.700406	14.999591
21.040091	1015.781885	15.004608
20.875032	1018.340583	15.009626
21.009751	1011.261031	15.014643
20.946579	1016.971114	15.019661
20.892787	1027.562576	15.024679
21.305854	1044.589507	15.029696
21.604359	1043.300907	15.034714
21.643211	1039.544172	15.039731
21.450665	1040.149046	15.044749
21.368100	1036.099037	15.049767
21.470292	1037.888683	15.054784
21.492362	1038.872794	15.059802
21.774810	1036.455126	15.064819
21.430603	1026.264834	15.069837
21.692650	1008.931136	15.074855
21.453317	1001.823848	15.079872
21.290293	993.660214	15.084890
21.498188	1010.002814	15.089907
21.710518	1021.537745	15.094925
21.644848	1032.303588	15.099943
21.750125	1017.962666	15.104960
21.230744	1011.281122	15.109978
21.703225	1017.209727	15.114995
21.138528	1027.953521	15.120013
21.750476	1033.240674	15.125031
21.471604	1041.486627	15.130048
21.240824	1029.693572	15.135066
21.664295	1038.914045	15.140083
21.592521	1036.652734	15.145101
21.741887	1037.933477	15.150119
21.984276	1035.428940	15.155136
21.621051	1042.278808	15.160154
21.879365	1038.557449	15.165171
21.714495	1039.554935	15.170189
21.771896	1042.063097	15.175207
22.044042	1041.251813	15.180224
21.615108	1039.142225	15.185242
22.001296	1034.524080	15.190259
21.735571	1040.989189	15.195277
21.929822	1059.230861	15.200295
21.925750	1055.590254	15.205312
21.979582	1069.232797	15.210330
22.181152	1056.018278	15.215347
21.738893	1064.868323	15.220365
22.227642	1054.425224	15.225383
22.373571	1047.547906	15.230400
22.148623	1060.330936	15.235418
22.496679	1048.571131	15.240435
22.425195	1057.962174	15.245453
22.313932	1046.156639	15.250471
22.069205	1036.081180	15.255488
21.904285	1029.199145	15.260506
22.470018	1039.910253	15.265523
22.112992	1056.141562	15.270541
22.322575	1047.334719	15.275559
22.140635	1058.919873	15.280576
22.178116	1056.921368	15.285594
22.297246	1049.595986	15.290611
22.414367	1046.905288	15.295629
22.190130	1052.247374	15.300647
22.694531	1049.597387	15.305664
22.720955	1047.484388	15.310682
22.748998	1054.058611	15.315699
22.461524	1054.012540	15.320717
22.545446	1058.026137	15.325735
22.438008	1046.472098	15.330752
22.502760	1048.025251	15.335770
22.811906	1045.573844	15.340787
22.600282	1058.217486	15.345805
22.448393	1044.637040	15.350823
22.821469	1043.339856	15.355840
22.655369	1048.746732	15.360858
22.991488	1049.026878	15.365875
22.598944	1053.515411	15.370893
22.566537	1052.070698	15.375911
22.736825	1048.384157	15.380928
22.778485	1064.239992	15.385946
22.874528	1046.386915	15.390963
22.604110	1053.596592	15.395981
22.129596	1048.941764	15.400999
22.614009	1041.888257	15.406016
22.525380	1053.390083	15.411034
22.441589	1068.699218	15.416051
22.955451	1078.128366	15.421069
22.903837	1096.875801	15.426087
23.246914	1072.294068	15.431104
23.070530	1084.052115	15.436122
23.060894	1081.838985	15.441139
23.121474	1078.256773	15.446157
23.346689	1078.227736	15.451175
23.413215	1067.228115	15.456192
23.339901	1076.527753	15.461210
23.244892	1071.280951	15.466227
23.060916	1071.628543	15.471245
22.922366	1075.389188	15.476263
23.361762	1073.854304	15.481280
23.152760	1076.159090	15.486298
23.313022	1077.480353	15.491315
23.316727	1071.602959	15.496333
23.288855	1079.199473	15.501351
23.407081	1073.562564	15.506368
23.345489	1076.240373	15.511386
23.601328	1063.227086	15.516403
23.409552	1072.209929	15.521421
23.116619	1081.389192	15.526439
23.642753	1069.681034	15.531456
23.497849	1078.613622	15.536474
23.485537	1073.136060	15.541491
23.886918	1070.008875	15.546509
23.508121	1058.438851	15.551527
23.882444	1061.302065	15.556544
23.163475	1054.053966	15.561562
23.226516	1056.927483	15.566579
23.582574	1067.097360	15.571597
23.444802	1074.452228	15.576615
23.773312	1065.895957	15.581632
23.288432	1071.850328	15.586650
23.329881	1074.342631	15.591667
23.259537	1073.414346	15.596685
23.522172	1087.336920	15.601703
24.070601	1073.038053	15.606720
23.450482	1070.044441	15.611738
23.697958	1077.020930	15.616755
23.735221	1068.987913	15.621773
23.688864	1083.905698	15.626791
24.113518	1093.572597	15.631808
24.001029	1106.853344	15.636826
24.010187	1091.440403	15.641843
24.121867	1068.036118	15.646861
23.603594	1084.806233	15.651879
24.104856	1095.191665	15.656896
23.757374	1103.003975	15.661914
23.923760	1107.459404	15.666931
23.976352	1101.341473	15.671949
23.853205	1110.086849	15.676967
24.319143	1099.845492	15.681984
24.141110	1101.371458	15.687002
24.105169	1096.052495	15.692019
24.216580	1096.286323	15.697037
23.925017	1096.068314	15.702055
24.247704	1097.292276	15.707072
24.142236	1102.481504	15.712090
23.993381	1095.122247	15.717107
23.885481	1100.814362	15.722125
24.029768	1095.154047	15.727143
24.170252	1113.396205	15.732160
24.607108	1116.031804	15.737178
25.083459	1120.568476	15.742195
24.733594	1089.343538	15.747213
24.621930	1086.417255	15.752231
24.706941	1083.053610	15.757248
24.634783	1088.373136	15.762266
24.512151	1096.974543	15.767283
25.092115	1094.093983	15.772301
25.141415	1090.736828	15.777319
25.117808	1079.777483	15.782336
24.679189	1061.461248	15.787354
24.695587	1060.855981	15.792371
24.590451	1057.268290	15.797389
24.400291	1067.619362	15.802407
24.656335	1077.528452	15.807424
24.765592	1089.302678	15.812442
24.920357	1091.953594	15.817459
24.911886	1089.248215	15.822477
24.649041	1090.388451	15.827495
24.865341	1086.685046	15.832512
24.824649	1083.789746	15.837530
24.698282	1090.729806	15.842547
24.899802	1080.778577	15.847565
24.707151	1077.081936	15.852583
24.830976	1083.330547	15.857600
24.787335	1083.314250	15.862618
24.665279	1075.765364	15.867635
24.745035	1085.457171	15.872653
24.648173	1091.608611	15.877671
24.843163	1078.184365	15.882688
24.888392	1089.270061	15.887706
25.057034	1112.903235	15.892723
25.304626	1114.616901	15.897741
25.021285	1122.305448	15.902759
25.126191	1125.077585	15.907776
25.367137	1110.446479	15.912794
25.343254	1116.134754	15.917811
25.256369	1107.806530	15.922829
25.047390	1118.029072	15.927847
25.114190	1118.390333	15.932864
25.037459	1125.228912	15.937882
25.126254	1114.222823	15.942899
25.449269	1103.177642	15.947917
25.472965	1110.610357	15.952935
25.122095	1110.503118	15.957952
25.022632	1112.003702	15.962970
25.162545	1120.928219	15.967987
25.305266	1112.231783	15.973005
25.396395	1126.013664	15.978023
25.664950	1127.469770	15.983040
25.917384	1122.484388	15.988058
25.604748	1118.547169	15.993075
25.851907	1110.414888	15.998093
25.609554	1115.830058	16.003111
25.488931	1117.248127	16.008128
25.708210	1122.398262	16.013146
25.584119	1116.022556	16.018163
25.936658	1125.484494	16.023181
25.968468	1133.989150	16.028199
25.937697	1113.517369	16.033216
25.582812	1108.353455	16.038234
25.821782	1110.720813	16.043251
25.788420	1121.861443	16.048269
25.826248	1134.931575	16.053287
25.684602	1144.970591	16.058304
25.809425	1136.023789	16.063322
25.936026	1135.841584	16.068339
26.057843	1132.086075	16.073357
25.824386	1130.385250	16.078375
26.016547	1130.478587	16.083392
26.075278	1134.791404	16.088410
26.108162	1144.215442	16.093427
26.043449	1126.797834	16.098445
26.332614	1135.536301	16.103463
26.182065	1129.786526	16.108480
26.154214	1130.985162	16.113498
26.257359	1128.152096	16.118515
26.213669	1119.616166	16.123533
25.886064	1140.904966	16.128551
25.855952	1134.709167	16.133568
26.339014	1131.946567	16.138586
26.208798	1131.987681	16.143603
26.280271	1134.179601	16.148621
26.102785	1142.827888	16.153639
26.828068	1158.777122	16.158656
26.785189	1157.286498	16.163674
26.577447	1137.944167	16.168691
26.527716	1117.556998	16.173709
26.561210	1120.965452	16.178727
26.465166	1127.467508	16.183744
26.662252	1127.100649	16.188762
26.582127	1131.761955	16.193779
26.882572	1140.277923	16.198797
26.787873	1133.921758	16.203815
26.742025	1126.746223	16.208832
26.962746	1128.123042	16.213850
26.531261	1131.450287	16.218867
26.811921	1123.799204	16.223885
26.614052	1123.868621	16.228903
26.410650	1129.775909	16.233920
26.894657	1142.131660	16.238938
26.916484	1150.804290	16.243955
26.982115	1151.346429	16.248973
27.048210	1159.778711	16.253991
27.064366	1144.901491	16.259008
26.802893	1148.094558	16.264026
26.659347	1154.010072	16.269043
27.025161	1146.545469	16.274061
27.143519	1159.806615	16.279079
26.621351	1155.094678	16.284096
27.197832	1157.502319	16.289114
27.296319	1148.679923	16.294131
27.220562	1147.676162	16.299149
27.329498	1152.300130	16.304167
26.960861	1151.102675	16.309184
27.167332	1153.066019	16.314202
26.793871	1150.903357	16.319219
27.157987	1148.557598	16.324237
27.331972	1153.596544	16.329255
27.295287	1158.951761	16.334272
27.125170	1157.707329	16.339290
26.838937	1149.404743	16.344307
27.142587	1154.976711	16.349325
27.151629	1165.835011	16.354343
27.497306	1177.106521	16.359360
27.807171	1174.853767	16.364378
27.345753	1174.522310	16.369395
27.601538	1173.054367	16.374413
27.978034	1185.051791	16.379431
27.986217	1174.617168	16.384448
27.902148	1164.246610	16.389466
27.632174	1161.223657	16.394483
27.549421	1151.725797	16.399501
27.987063	1162.413283	16.404519
27.719994	1158.489190	16.409536
27.659843	1155.798442	16.414554
27.406898	1174.073407	16.419571
28.106472	1166.607766	16.424589
27.984193	1167.032160	16.429607
28.190562	1176.153178	16.434624
27.698139	1167.740187	16.439642
27.699385	1182.137281	16.444659
27.975293	1179.778341	16.449677
27.767636	1169.217012	16.454695
27.814779	1166.583521	16.459712
27.945690	1168.464485	16.464730
27.612941	1172.719778	16.469747
27.447774	1157.927423	16.474765
27.703869	1169.994724	16.479783
27.515765	1196.002794	16.484800
28.297740	1194.168211	16.489818
28.238256	1203.832518	16.494835
28.474851	1203.756331	16.499853
28.421502	1204.444690	16.504871
28.454908	1204.484155	16.509888
28.764961	1200.040135	16.514906
28.526300	1189.032599	16.519923
28.295323	1168.930396	16.524941
28.526635	1172.402811	16.529959
28.458290	1163.350729	16.534976
28.619539	1153.954653	16.539994
28.451018	1158.883688	16.545011
28.508254	1154.324394	16.550029
28.181764	1153.867112	16.555047
28.188815	1178.562769	16.560064
28.500194	1184.838294	16.565082
28.902512	1202.586565	16.570099
29.036884	1199.225367	16.575117
28.895172	1191.538748	16.580135
28.616354	1175.817454	16.585152
28.938235	1165.227470	16.590170
28.900435	1166.860960	16.595187
28.636226	1161.464947	16.600205
28.771878	1166.666313	16.605223
28.586189	1169.281389	16.610240
28.951331	1184.799878	16.615258
28.797561	1181.698277	16.620275
29.069894	1193.033881	16.625293
29.213109	1197.279022	16.630311
28.712549	1184.641380	16.635328
28.815154	1182.947407	16.640346
28.629832	1184.688729	16.645363
28.874653	1199.200487	16.650381
29.075141	1192.092073	16.655399
28.822747	1202.210640	16.660416
29.006088	1188.939382	16.665434
29.224679	1187.820056	16.670451
29.026762	1192.731719	16.675469
29.011221	1194.691211	16.680487
29.085433	1211.194681	16.685504
29.488109	1202.942964	16.690522
29.371782	1197.528406	16.695539
29.291899	1193.227160	16.700557
29.318958	1188.563803	16.705575
29.041171	1202.785207	16.710592
29.546220	1210.322653	16.715610
29.594063	1225.087822	16.720627
29.697264	1208.807567	16.725645
29.911336	1188.755989	16.730663
29.617794	1191.840797	16.735680
29.819415	1186.199908	16.740698
29.766640	1189.836185	16.745715
29.576050	1191.600619	16.750733
29.752363	1185.479727	16.755751
29.627460	1192.741199	16.760768
29.870896	1180.711221	16.765786
29.497667	1178.824068	16.770803
29.666844	1192.743878	16.775821
29.586682	1180.909678	16.780839
29.488755	1191.217839	16.785856
29.964115	1199.821652	16.790874
29.917490	1203.367952	16.795891
30.114521	1210.411098	16.800909
30.329661	1209.111461	16.805927
29.839424	1195.466928	16.810944
29.995413	1186.406103	16.815962
29.911717	1206.976831	16.820979
29.824467	1214.473002	16.825997
30.206489	1208.239182	16.831015
30.080216	1205.163737	16.836032
30.149599	1203.523867	16.841050
30.025152	1205.958184	16.846067
30.125489	1210.565680	16.851085
30.203259	1198.445561	16.856103
29.766975	1214.441940	16.861120
29.850032	1207.997324	16.866138
29.524255	1207.410018	16.871155
29.766805	1222.500244	16.876173
30.066517	1227.044487	16.881191
29.896186	1234.394380	16.886208
30.327215	1232.197569	16.891226
30.318862	1229.631497	16.896243
30.278082	1230.050495	16.901261
30.124907	1229.228986	16.906279
30.788924	1244.783174	16.911296
30.839316	1251.550218	16.916314
30.663565	1224.146105	16.921331
30.595866	1231.936061	16.926349
30.784414	1225.737158	16.931367
30.456458	1226.858442	16.936384
30.561517	1235.449856	16.941402
30.743118	1255.051933	16.946419
30.834776	1268.355376	16.951437
31.206271	1253.569508	16.956455
31.117119	1244.214362	16.961472
31.026635	1225.104282	16.966490
30.878299	1220.132347	16.971507
30.588003	1223.068811	16.976525
31.122356	1222.812138	16.981543
30.948356	1249.722568	16.986560
31.128306	1250.823103	16.991578
31.377581	1249.679611	16.996595
30.857274	1240.856086	17.001613
31.177781	1235.217380	17.006631
30.895756	1244.716547	17.011648
31.338647	1240.144672	17.016666
31.400912	1250.563390	17.021683
31.335453	1248.911157	17.026701
31.748365	1245.208488	17.031719
31.369963	1229.512846	17.036736
31.231214	1212.242002	17.041754
31.456960	1221.926500	17.046771
31.160210	1231.457418	17.051789
31.352956	1232.901853	17.056807
31.370769	1236.200143	17.061824
31.017654	1237.884762	17.066842
31.668610	1241.727747	17.071859
31.217119	1244.479070	17.076877
31.529338	1236.123993	17.081895
31.469554	1240.831570	17.086912
31.372726	1247.880386	17.091930
31.438382	1245.842560	17.096947
31.165556	1245.540557	17.101965
31.651349	1258.075610	17.106983
31.755636	1280.568651	17.112000
31.805957	1270.575366	17.117018
31.883721	1277.561490	17.122035
31.867078	1280.872373	17.127053
31.982766	1278.772935	17.132071
31.723002	1283.184088	17.137088
31.779855	1271.567695	17.142106
32.125286	1272.407256	17.147123
31.856878	1268.592003	17.152141
32.018793	1272.830728	17.157159
32.219417	1269.979166	17.162176
31.889541	1270.504197	17.167194
31.839091	1272.525957	17.172211
31.726607	1278.154336	17.177229
31.995437	1265.208013	17.182247
32.171776	1275.599434	17.187264
32.294575	1290.094440	17.192282
32.476681	1287.293960	17.197299
32.281063	1293.171485	17.202317
32.718842	1289.985296	17.207335
32.593766	1278.411952	17.212352
32.732499	1262.400338	17.217370
32.923592	1251.710862	17.222387
32.511750	1268.218739	17.227405
32.675048	1261.453008	17.232423
32.255885	1258.818025	17.237440
32.701671	1256.866967	17.242458
32.945953	1261.066688	17.247475
32.337136	1263.812127	17.252493
32.615602	1265.863576	17.257511
32.776347	1258.829406	17.262528
32.653306	1261.993716	17.267546
33.065255	1260.391510	17.272563
32.556644	1257.070222	17.277581
32.581144	1266.468165	17.282599
32.483922	1262.338640	17.287616
32.813445	1274.552529	17.292634
33.147083	1284.669374	17.297651
32.813107	1293.948840	17.302669
32.993436	1290.022818	17.307687
33.122732	1294.356888	17.312704
32.843917	1287.530758	17.317722
32.914980	1289.712337	17.322739
32.613566	1301.214279	17.327757
32.816819	1295.970272	17.332775
32.905511	1294.036295	17.337792
32.959433	1287.180373	17.342810
33.394117	1279.775379	17.347827
33.489508	1292.517671	17.352845
33.450970	1288.901600	17.357863
33.398992	1288.145834	17.362880
33.117208	1290.591402	17.367898
33.264466	1282.350556	17.372915
33.656698	1290.574509	17.377933
33.457240	1296.858324	17.382951
33.502219	1299.097555	17.387968
33.818096	1313.530366	17.392986
33.613737	1295.415068	17.398003
33.557217	1300.586236	17.403021
33.455069	1294.690623	17.408039
33.632101	1303.716579	17.413056
33.675022	1312.574373	17.418074
34.179237	1312.802931	17.423091
33.881624	1323.952931	17.428109
33.996578	1318.829399	17.433127
33.787268	1297.075828	17.438144
33.913816	1303.028251	17.443162
34.399621	1296.462327	17.448179
33.871475	1294.726923	17.453197
34.012797	1276.703126	17.458215
34.203898	1271.415668	17.463232
34.000455	1284.372668	17.468250
34.126549	1270.009176	17.473267
33.790050	1282.472483	17.478285
33.829179	1291.029947	17.483303
34.237274	1300.999871	17.488320
34.221218	1310.423044	17.493338
34.147876	1300.662154	17.498355
34.262268	1317.077613	17.503373
34.182279	1315.161273	17.508391
34.457139	1307.722841	17.513408
34.335805	1311.164008	17.518426
34.515036	1300.310338	17.523443
34.426173	1317.249083	17.528461
34.466481	1311.926499	17.533479
34.213556	1304.696725	17.538496
34.264367	1311.784944	17.543514
34.472859	1306.880573	17.548531
34.250383	1324.170103	17.553549
34.407096	1317.516641	17.558567
34.621176	1321.651103	17.563584
34.652351	1327.300637	17.568602
34.697040	1329.025813	17.573619
34.814650	1332.926844	17.578637
35.106970	1330.543913	17.583655
35.227675	1320.845223	17.588672
35.077068	1311.033127	17.593690
35.075958	1295.582706	17.598707
35.107416	1291.256538	17.603725
34.910249	1287.382859	17.608743
35.209660	1288.578405	17.613760
35.005302	1298.782392	17.618778
35.032230	1299.728910	17.623795
34.781926	1296.802272	17.628813
35.032092	1305.457333	17.633831
35.069964	1310.825673	17.638848
34.750713	1318.158882	17.643866
35.052660	1311.692222	17.648883
34.718206	1322.009639	17.653901
34.597175	1327.536312	17.658919
34.969994	1332.397794	17.663936
35.099732	1351.342117	17.668954
35.497688	1355.037201	17.673971
36.018424	1349.656863	17.678989
35.660176	1347.327900	17.684007
35.850836	1351.304844	17.689024
35.323500	1339.742225	17.694042
35.328730	1339.191346	17.699059
35.469723	1348.401803	17.704077
35.392535	1353.062297	17.709095
35.857962	1349.052932	17.714112
35.359709	1351.666154	17.719130
35.787501	1351.529635	17.724147
36.009466	1356.132822	17.729165
35.619748	1358.521246	17.734183
35.708868	1351.803752	17.739200
35.563619	1355.833648	17.744218
35.955303	1341.343534	17.749235
36.013084	1351.239507	17.754253
35.922076	1351.057831	17.759271
36.401530	1351.259975	17.764288
36.272587	1358.270847	17.769306
36.481895	1365.500397	17.774323
36.280009	1343.951216	17.779341
36.049157	1354.195636	17.784359
36.412084	1341.268144	17.789376
35.860310	1344.769229	17.794394
36.169151	1343.136815	17.799411
35.924440	1347.645486	17.804429
36.050764	1366.670106	17.809447
36.539750	1366.433722	17.814464
36.698100	1377.036623	17.819482
36.806197	1369.893401	17.824499
36.766168	1365.989012	17.829517
36.413012	1365.492631	17.834535
36.634406	1363.002730	17.839552
36.378044	1372.115893	17.844570
36.526765	1368.664700	17.849587
36.754937	1370.228475	17.854605
36.797951	1369.398157	17.859623
36.629427	1353.312829	17.864640
37.004765	1367.095397	17.869658
37.121426	1354.615033	17.874675
37.062112	1359.244626	17.879693
36.880659	1357.337962	17.884711
37.351214	1349.065897	17.889728
37.095898	1360.092610	17.894746
37.104665	1362.458487	17.899763
37.221572	1363.926096	17.904781
37.095184	1368.975581	17.909799
37.151300	1359.115516	17.914816
36.976246	1356.106755	17.919834
37.158075	1349.913636	17.924851
37.179422	1352.631521	17.929869
37.224520	1351.827824	17.934887
37.211297	1355.686119	17.939904
36.984136	1355.561583	17.944922
37.139092	1355.075516	17.949939
37.178441	1350.569310	17.954957
36.942521	1356.715296	17.959975
37.415600	1344.619884	17.964992
37.411179	1354.873337	17.970010
37.107113	1352.240378	17.975027
37.486925	1371.976562	17.980045
37.357896	1383.571324	17.985063
37.703997	1391.687419	17.990080
37.861673	1382.307934	17.995098
37.906911	1376.835515	18.000115
37.734019	1373.096566	18.005133
37.791033	1380.972667	18.010151
38.042664	1373.092627	18.015168
37.812397	1377.355053	18.020186
37.845980	1375.219963	18.025203
37.929009	1372.959592	18.030221
37.396057	1383.581471	18.035239
37.832343	1384.587301	18.040256
37.979960	1368.168649	18.045274
37.890066	1372.664341	18.050291
38.355940	1374.035313	18.055309
38.092000	1378.712897	18.060327
38.457171	1382.761786	18.065344
38.268631	1391.907843	18.070362
38.503305	1394.764280	18.075379
38.495734	1385.920894	18.080397
38.097426	1388.266850	18.085415
38.549070	1395.285918	18.090432
38.389365	1400.208062	18.095450
38.561344	1405.122241	18.100467
38.589481	1404.556552	18.105485
38.477640	1407.930628	18.110503
39.104803	1410.948363	18.115520
38.826812	1388.218341	18.120538
38.155679	1394.325250	18.125555
38.556800	1392.281766	18.130573
38.615849	1401.848864	18.135591
38.910755	1400.011883	18.140608
38.597061	1406.871047	18.145626
38.627456	1399.701089	18.150643
38.660674	1397.164533	18.155661
38.503564	1396.563716	18.160679
38.884150	1390.943565	18.165696
39.018909	1404.513198	18.170714
39.059271	1412.158238	18.175731
39.273057	1411.654575	18.180749
39.010935	1412.300484	18.185767
39.065138	1409.158958	18.190784
39.140109	1427.702437	18.195802
39.028713	1432.312316	18.200819
39.553514	1419.516848	18.205837
38.807637	1417.925860	18.210855
39.286148	1413.203972	18.215872
39.316013	1418.931109	18.220890
39.370528	1429.639186	18.225907
39.578598	1421.564179	18.230925
39.172157	1429.864485	18.235943
39.237479	1423.880133	18.240960
39.491218	1433.497155	18.245978
39.542250	1446.936387	18.250995
39.956000	1437.537384	18.256013
40.075477	1436.388560	18.261031
39.829766	1417.579447	18.266048
40.143601	1411.572731	18.271066
40.094703	1414.104032	18.276083
40.004899	1412.414470	18.281101
39.978109	1424.414559	18.286119
40.143058	1414.839782	18.291136
40.083023	1408.147895	18.296154
39.765435	1425.359172	18.301171
40.393385	1417.325203	18.306189
40.107405	1409.241697	18.311207
39.985725	1409.699655	18.316224
40.117804	1411.416894	18.321242
40.024671	1410.315408	18.326259
40.365205	1402.684802	18.331277
40.208123	1412.860385	18.336295
40.109515	1409.552009	18.341312
40.091559	1410.394745	18.346330
39.911100	1424.482961	18.351347
40.348990	1424.022964	18.356365
39.931557	1443.245000	18.361383
40.479880	1434.598666	18.366400
40.373028	1438.687191	18.371418
40.565526	1436.385101	18.376435
40.635133	1432.184070	18.381453
40.166887	1431.959822	18.386471
40.695068	1455.741172	18.391488
40.731205	1463.423349	18.396506
40.835371	1467.012697	18.401523
41.215719	1460.170662	18.406541
41.047320	1470.623119	18.411559
41.289289	1465.296485	18.416576
41.023955	1443.750955	18.421594
41.095205	1441.198659	18.426611
40.874242	1432.630243	18.431629
40.950770	1446.905906	18.436647
41.038694	1462.375224	18.441664
41.037581	1452.338751	18.446682
41.011989	1458.069162	18.451699
41.284056	1455.515761	18.456717
41.168808	1457.366582	18.461735
41.341335	1447.132739	18.466752
41.494072	1453.834738	18.471770
40.793038	1461.627511	18.476787
41.328578	1467.896225	18.481805
41.194150	1466.662599	18.486823
41.485364	1479.657101	18.491840
41.566139	1480.496123	18.496858
41.506967	1486.499974	18.501875
42.103186	1484.859226	18.506893
42.122012	1489.170667	18.511911
42.184836	1481.880366	18.516928
41.925655	1462.151094	18.521946
41.637644	1454.594804	18.526963
41.677427	1447.205190	18.531981
41.811121	1461.435007	18.536999
41.756023	1481.316617	18.542016
42.025964	1465.118564	18.547034
41.922059	1490.838842	18.552051
42.317690	1483.759260	18.557069
42.158398	1487.732265	18.562087
41.884860	1491.984552	18.567104
41.884364	1475.284196	18.572122
42.151099	1478.266241	18.577139
42.188249	1473.910738	18.582157
42.321541	1477.931247	18.587175
42.155996	1487.240074	18.592192
42.342694	1487.363842	18.597210
42.246527	1482.264514	18.602227
42.056364	1475.404754	18.607245
42.106799	1498.025503	18.612263
42.319663	1495.423225	18.617280
42.392766	1501.203673	18.622298
42.729261	1509.884539	18.627315
42.823803	1512.781476	18.632333
42.422666	1507.623494	18.637351
42.574224	1506.564824	18.642368
42.727189	1503.055622	18.647386
42.666225	1515.592469	18.652403
42.713621	1507.489841	18.657421
43.006924	1510.957601	18.662439
42.779196	1510.408404	18.667456
43.009018	1526.035811	18.672474
43.264838	1525.505713	18.677491
43.515316	1513.338895	18.682509
43.294570	1514.621399	18.687527
43.657389	1499.652696	18.692544
43.523345	1501.971730	18.697562
43.502605	1497.485252	18.702579
43.199710	1499.108258	18.707597
43.428163	1502.488713	18.712615
43.211221	1496.417331	18.717632
43.363201	1497.266238	18.722650
43.525113	1491.341873	18.727667
43.419128	1492.522940	18.732685
43.566312	1507.641803	18.737703
43.795736	1509.870464	18.742720
43.662875	1497.982530	18.747738
43.681726	1511.487366	18.752755
43.797841	1520.846116	18.757773
43.797279	1520.479236	18.762791
43.782162	1525.614704	18.767808
44.240293	1514.553791	18.772826
43.672416	1524.591056	18.777843
43.948651	1518.594252	18.782861
43.939550	1517.477888	18.787879
43.718439	1525.042782	18.792896
43.987883	1519.148860	18.797914
43.805287	1523.418801	18.802931
43.595034	1518.669180	18.807949
44.068988	1528.191610	18.812967
44.289220	1538.619652	18.817984
44.335723	1539.508627	18.823002
44.535258	1545.329412	18.828019
44.575306	1538.176100	18.833037
44.589566	1550.360820	18.838055
44.429391	1551.212697	18.843072
44.581836	1540.538264	18.848090
44.511248	1548.878400	18.853107
44.416045	1541.996226	18.858125
44.581883	1535.219326	18.863143
44.465159	1546.622436	18.868160
44.610491	1547.998761	18.873178
44.758596	1540.398311	18.878195
44.899521	1537.312302	18.883213
45.064855	1537.345124	18.888231
44.661125	1542.472972	18.893248
45.167101	1537.537282	18.898266
44.844725	1537.481031	18.903283
44.975043	1539.645374	18.908301
45.132719	1538.232189	18.913319
45.193491	1535.326139	18.918336
45.167193	1534.166951	18.923354
45.095187	1541.152948	18.928371
45.348191	1554.444739	18.933389
45.633766	1557.533713	18.938407
45.469981	1546.030336	18.943424
45.461131	1531.484985	18.948442
45.404344	1527.507349	18.953459
45.267248	1533.811267	18.958477
45.640552	1551.023463	18.963495
45.257535	1560.094090	18.968512
45.810490	1562.278548	18.973530
45.670028	1554.267955	18.978547
46.052284	1556.643986	18.983565
46.049899	1558.083300	18.988583
45.943551	1564.904333	18.993600
46.156607	1551.833537	18.998618
45.733102	1542.996792	19.003635
45.767573	1553.842307	19.008653
46.619064	1554.387654	19.013671
45.887271	1553.054726	19.018688
45.777533	1535.411641	19.023706
45.811093	1549.227822	19.028723
46.230524	1556.389871	19.033741
46.354647	1552.663206	19.038759
46.008518	1569.496530	19.043776
46.067962	1556.827253	19.048794
46.112177	1562.774487	19.053811
45.711381	1566.317593	19.058829
45.980847	1563.261119	19.063847
46.091780	1574.426456	19.068864
46.536842	1572.036357	19.073882
46.687449	1589.610752	19.078899
46.429233	1596.099652	19.083917
46.831143	1592.252870	19.088935
46.678290	1594.102047	19.093952
47.218017	1584.826020	19.098970
47.229657	1586.022102	19.103987
47.035096	1583.270821	19.109005
47.265553	1584.259897	19.114023
46.883828	1595.504888	19.119040
47.252361	1575.392247	19.124058
47.373054	1580.046091	19.129075
47.443391	1587.155814	19.134093
47.613601	1575.668081	19.139111
47.046790	1557.019916	19.144128
47.172576	1539.316649	19.149146
47.221269	1548.983177	19.154163
47.505949	1570.303462	19.159181
47.647990	1567.439482	19.164199
47.217940	1576.469078	19.169216
47.307834	1573.044094	19.174234
47.423282	1573.869912	19.179251
47.653895	1574.621587	19.184269
47.878794	1572.892601	19.189287
47.805919	1586.286690	19.194304
47.831462	1578.193934	19.199322
47.871311	1576.118011	19.204339
47.672486	1580.144417	19.209357
47.484095	1571.545347	19.214375
47.554949	1581.691051	19.219392
47.857791	1562.125442	19.224410
47.794152	1564.708409	19.229427
47.839808	1586.616184	19.234445
47.749265	1575.854926	19.239463
47.723754	1591.644659	19.244480
47.899436	1597.010599	19.249498
48.026640	1605.169475	19.254515
48.021336	1610.076997	19.259533
48.636650	1596.725346	19.264551
48.283719	1601.578708	19.269568
48.197045	1598.958202	19.274586
48.311699	1600.032943	19.279603
48.165773	1607.936594	19.284621
48.605984	1595.717299	19.289639
48.354384	1603.634868	19.294656
48.374937	1610.741806	19.299674
48.639716	1624.977276	19.304691
48.679685	1635.449934	19.309709
48.913392	1621.969806	19.314727
48.869127	1627.980894	19.319744
48.828199	1620.023890	19.324762
48.729681	1623.572563	19.329779
48.425951	1630.584295	19.334797
48.847686	1614.531258	19.339815
48.693203	1631.898076	19.344832
48.889758	1628.873715	19.349850
49.341179	1642.323915	19.354867
48.893470	1646.911094	19.359885
49.264516	1644.323199	19.364903
49.551268	1649.458819	19.369920
49.711703	1642.598523	19.374938
49.583645	1642.842211	19.379955
49.380825	1647.190519	19.384973
49.494963	1637.907631	19.389991
49.692663	1649.702117	19.395008
49.757149	1643.079699	19.400026
49.864023	1641.938847	19.405043
49.482518	1641.701835	19.410061
50.072416	1645.543206	19.415079
50.033835	1640.395535	19.420096
50.017432	1643.340354	19.425114
49.960604	1646.742395	19.430131
49.711270	1642.948499	19.435149
50.128017	1639.869248	19.440167
49.952675	1637.594059	19.445184
50.062065	1648.236730	19.450202
50.325055	1642.907152	19.455219
50.360118	1644.581992	19.460237
50.340533	1645.982822	19.465255
50.220468	1642.709237	19.470272
50.384246	1641.288933	19.475290
50.815212	1639.583952	19.480307
50.449924	1650.420996	19.485325
50.432076	1637.412495	19.490343
50.209199	1643.821370	19.495360
49.910933	1640.958687	19.500378
50.321385	1635.003431	19.505395
50.096831	1648.727724	19.510413
50.436995	1654.420797	19.515431
50.511401	1669.052883	19.520448
50.513401	1673.398256	19.525466
50.623284	1673.109371	19.530483
50.516142	1684.949535	19.535501
50.917991	1677.709209	19.540519
50.917914	1681.380393	19.545536
51.005410	1678.727549	19.550554
51.485108	1674.804711	19.555571
51.311634	1679.882549	19.560589
51.237746	1678.257643	19.565607
51.121201	1688.747934	19.570624
51.388221	1687.182233	19.575642
51.581092	1687.199088	19.580659
51.149074	1684.236662	19.585677
51.692387	1678.778277	19.590695
51.690504	1679.457759	19.595712
51.477139	1679.089036	19.600730
51.966646	1672.401293	19.605747
51.751079	1678.869992	19.610765
52.087624	1671.591450	19.615783
51.921664	1678.014750	19.620800
51.977320	1681.271650	19.625818
52.164618	1670.635458	19.630835
51.736721	1678.296008	19.635853
51.681129	1669.003554	19.640871
51.973799	1684.277074	19.645888
51.759740	1681.776018	19.650906
51.939656	1673.094574	19.655923
51.705965	1684.107709	19.660941
51.744198	1692.754905	19.665959
51.877436	1695.596078	19.670976
51.821816	1693.983899	19.675994
52.584745	1702.397776	19.681011
52.549106	1710.298018	19.686029
52.640244	1714.223990	19.691047
52.375761	1711.095305	19.696064
51.971909	1716.699362	19.701082
52.614208	1720.412618	19.706099
52.693197	1733.196761	19.711117
53.102399	1716.414271	19.716135
53.183638	1730.246552	19.721152
52.829922	1733.727787	19.726170
52.925408	1727.882412	19.731187
53.265936	1729.530600	19.736205
53.254387	1726.075303	19.741223
53.336145	1722.888023	19.746240
52.975361	1730.712293	19.751258
53.274465	1719.689323	19.756275
53.029324	1727.357686	19.761293
53.366698	1724.873757	19.766311
53.210128	1718.978707	19.771328
53.006906	1718.834858	19.776346
53.231626	1722.162048	19.781363
53.245253	1727.987642	19.786381
52.823653	1716.236023	19.791399
53.362805	1742.555502	19.796416
53.214388	1751.361907	19.801434
53.562617	1748.981878	19.806451
53.562833	1748.391266	19.811469
53.773847	1749.887057	19.816487
54.104919	1749.950754	19.821504
53.704020	1752.666051	19.826522
54.205310	1745.322262	19.831539
53.709197	1747.157715	19.836557
54.104451	1762.016174	19.841575
54.285175	1772.803427	19.846592
54.140429	1790.050911	19.851610
54.488338	1777.019250	19.856627
54.696162	1773.801876	19.861645
54.371240	1769.617920	19.866663
54.580704	1774.418949	19.871680
54.693026	1777.123254	19.876698
54.665567	1764.989766	19.881715
54.614710	1773.666492	19.886733
54.445296	1767.812125	19.891751
54.542653	1784.597002	19.896768
54.523847	1782.589399	19.901786
54.202346	1763.037148	19.906803
54.093813	1772.524109	19.911821
54.419056	1779.194202	19.916839
54.817208	1790.619682	19.921856
55.109410	1802.153812	19.926874
55.363686	1789.031324	19.931891
55.348065	1806.387792	19.936909
55.371979	1792.808535	19.941927
55.422467	1792.756212	19.946944
55.193876	1796.034322	19.951962
55.381893	1795.455780	19.956979
55.562778	1802.817977	19.961997
55.443924	1789.745534	19.967015
55.669902	1782.259447	19.972032
55.333905	1790.079060	19.977050
55.445841	1783.502476	19.982067
55.349733	1798.352607	19.987085
55.499418	1799.831966	19.992103
55.897913	1786.550622	19.997120
55.657317	1791.784062	20.002138
55.899677	1785.259343	20.007155
55.291034	1793.026777	20.012173
55.476369	1803.194454	20.017191
55.774462	1813.763345	20.022208
55.786089	1823.574739	20.027226
55.635852	1817.310138	20.032243
55.832818	1822.907066	20.037261
56.037020	1838.229607	20.042279
56.230897	1843.732771	20.047296
56.028165	1849.208374	20.052314
56.516603	1841.613933	20.057331
56.558366	1843.642378	20.062349
56.205786	1846.982125	20.067367
56.688347	1838.744427	20.072384
56.501860	1840.294891	20.077402
56.539711	1841.248299	20.082419
56.456177	1834.500863	20.087437
56.413714	1840.643416	20.092455
56.908214	1845.828033	20.097472
56.931191	1862.633159	20.102490
57.188821	1870.535017	20.107507
57.623827	1867.192690	20.112525
57.605607	1873.206852	20.117543
57.540267	1859.583038	20.122560
56.922127	1844.807398	20.127578
57.181328	1844.597566	20.132595
57.407642	1854.749846	20.137613
57.267384	1864.874919	20.142631
57.738577	1861.770291	20.147648
57.771811	1860.170180	20.152666
57.684572	1855.215892	20.157683
57.705844	1847.866936	20.162701
57.765795	1858.624409	20.167719
58.085737	1846.599970	20.172736
58.040314	1852.451903	20.177754
57.959015	1825.764502	20.182771
58.258335	1828.432601	20.187789
57.833603	1816.951670	20.192807
58.149144	1820.824842	20.197824
57.773969	1831.339072	20.202842
57.859702	1842.503059	20.207859
58.271056	1849.534901	20.212877
57.845801	1853.805664	20.217895
58.334038	1851.935504	20.222912
58.330444	1848.203498	20.227930
58.135624	1853.146744	20.232947
58.369767	1847.300456	20.237965
58.084820	1858.930788	20.242983
58.289862	1858.024658	20.248000
58.528201	1883.698682	20.253018
58.534188	1881.365740	20.258035
58.528658	1889.797858	20.263053
58.742754	1892.363920	20.268071
59.123495	1874.799814	20.273088
59.193501	1871.279045	20.278106
59.343146	1873.777808	20.283123
59.345754	1881.340156	20.288141
59.216690	1879.913699	20.293159
59.045511	1875.136252	20.298176
59.187000	1868.984628	20.303194
59.084377	1868.240154	20.308211
59.112826	1866.250320	20.313229
59.044411	1865.559243	20.318247
59.158001	1872.713718	20.323264
59.215942	1892.884040	20.328282
59.456187	1904.531744	20.333299
59.386873	1897.244973	20.338317
59.502991	1900.251006	20.343335
59.417713	1902.509487	20.348352
59.546004	1898.848579	20.353370
59.637666	1901.030581	20.358387
59.977304	1919.009116	20.363405
60.264419	1933.809830	20.368423
60.328041	1921.499372	20.373440
60.094503	1902.660294	20.378458
59.997154	1912.386415	20.383475
60.266875	1907.386903	20.388493
60.093835	1917.840232	20.393511
60.555897	1930.811216	20.398528
60.448450	1920.502863	20.403546
60.553875	1928.889308	20.408563
60.614051	1917.026036	20.413581
60.528365	1932.317250	20.418599
60.610881	1920.664240	20.423616
60.504350	1921.701545	20.428634
60.655140	1923.422050	20.433651
60.736978	1910.569861	20.438669
60.359374	1918.071838	20.443687
60.399887	1916.266207	20.448704
60.745683	1924.915854	20.453722
60.662825	1935.603090	20.458739
60.973314	1939.499566	20.463757
61.169927	1950.734277	20.468775
60.918397	1945.148507	20.473792
60.673803	1953.245001	20.478810
61.244076	1960.461244	20.483827
61.436042	1965.049299	20.488845
61.488930	1961.683686	20.493863
61.830114	1965.866605	20.498880
61.740388	1970.087467	20.503898
61.835965	1972.388507	20.508915
61.837426	1966.090510	20.513933
61.998845	1971.126489	20.518951
62.174388	1963.356745	20.523968
62.088824	1970.821708	20.528986
61.941807	1967.308238	20.534003
62.041682	1966.597614	20.539021
62.025993	1973.553439	20.544039
62.028442	1957.481939	20.549056
61.908079	1975.336964	20.554074
61.960740	1971.678696	20.559091
61.838560	1964.593132	20.564109
61.945486	1969.751687	20.569127
61.978326	1979.572862	20.574144
62.070533	2001.620568	20.579162
61.815757	2006.998340	20.584179
62.888311	2016.821733	20.589197
62.649402	2027.123633	20.594215
62.957622	2027.141703	20.599232
63.159621	2022.261209	20.604250
62.507660	2024.955839	20.609267
63.278482	2022.760051	20.614285
63.122110	2020.688345	20.619303
63.189077	2024.957732	20.624320
63.123019	2016.554124	20.629338
63.070171	2023.150592	20.634355
63.441504	2011.262009	20.639373
63.376162	2014.506103	20.644391
63.522287	2021.708612	20.649408
63.387749	2016.793975	20.654426
63.781121	2017.667782	20.659443
63.951926	2011.351231	20.664461
63.465655	2022.103811	20.669479
63.926562	2015.829273	20.674496
64.001469	2007.112637	20.679514
63.802559	2011.240735	20.684531
63.784097	2015.074275	20.689549
63.817885	2015.182965	20.694567
63.975820	2017.225304	20.699584
63.869274	2015.734488	20.704602
63.963651	2009.667949	20.709619
64.157549	2009.425013	20.714637
64.122512	2022.775830	20.719655
64.431436	2032.872650	20.724672
64.256487	2040.165426	20.729690
64.062315	2039.340607	20.734707
64.335863	2044.786588	20.739725
64.240972	2044.099485	20.744743
64.411996	2036.495595	20.749760
64.774997	2034.052261	20.754778
64.571739	2031.713128	20.759795
64.883484	2048.043020	20.764813
64.901709	2065.047758	20.769831
64.659654	2062.603623	20.774848
65.013910	2067.681186	20.779866
64.680174	2065.363019	20.784883
65.106744	2062.734978	20.789901
64.937967	2056.536723	20.794919
64.806211	2063.002952	20.799936
65.472202	2072.276094	20.804954
65.110598	2082.576457	20.809971
65.594743	2079.616091	20.814989
65.586283	2083.575347	20.820007
65.516912	2079.235898	20.825024
65.894751	2081.690492	20.830042
65.509851	2088.133017	20.835059
65.610625	2089.883654	20.840077
65.584051	2082.135242	20.845095
65.846206	2080.335483	20.850112
65.956117	2101.347814	20.855130
65.871660	2115.726480	20.860147
66.569824	2097.904962	20.865165
66.449681	2116.378567	20.870183
66.725160	2114.129000	20.875200
67.200987	2110.409828	20.880218
66.966142	2092.581282	20.885235
66.918235	2078.637097	20.890253
66.845615	2065.849668	20.895271
66.610875	2077.466356	20.900288
67.054954	2069.007946	20.905306
66.831837	2083.705141	20.910323
66.856057	2069.343173	20.915341
66.844901	2063.381446	20.920359
66.957973	2058.595747	20.925376
67.163106	2064.254008	20.930394
66.876798	2073.149716	20.935411
66.696799	2071.218313	20.940429
66.954271	2080.018656	20.945447
66.833315	2094.629104	20.950464
67.026199	2103.566501	20.955482
67.202719	2098.461866	20.960499
67.469423	2086.272824	20.965517
67.464256	2099.248723	20.970535
67.493217	2107.626839	20.975552
67.401385	2098.164538	20.980570
67.338601	2118.221453	20.985587
68.040310	2113.500660	20.990605
67.962318	2125.405630	20.995623
67.882241	2122.323350	21.000640
67.741675	2117.624227	21.005658
68.164511	2134.034664	21.010675
68.340349	2127.738099	21.015693
68.162280	2114.922193	21.020711
68.059432	2122.149947	21.025728
68.589759	2118.306619	21.030746
68.198074	2111.782212	21.035763
68.492695	2112.366658	21.040781
67.995988	2109.944912	21.045799
68.164867	2122.467497	21.050816
68.285724	2144.405958	21.055834
68.435304	2147.971033	21.060851
68.861580	2141.027811	21.065869
69.028055	2143.507304	21.070887
68.912947	2151.165411	21.075904
69.145166	2143.162410	21.080922
68.798985	2146.635011	21.085939
68.831408	2147.540323	21.090957
68.952981	2155.343166	21.095975
69.036510	2173.994192	21.100992
69.108137	2177.571959	21.106010
69.439655	2174.777730	21.111027
69.588348	2170.140233	21.116045
69.447088	2176.357705	21.121063
69.385657	2179.719879	21.126080
69.762000	2176.496228	21.131098
69.856105	2173.712296	21.136115
69.899192	2167.372499	21.141133
69.927438	2167.921836	21.146151
69.647341	2161.351412	21.151168
70.012299	2182.699436	21.156186
70.157919	2196.088065	21.161203
70.467133	2183.479748	21.166221
70.982948	2180.625540	21.171239
70.489339	2186.867580	21.176256
70.757179	2164.370206	21.181274
70.601243	2165.446397	21.186291
70.665219	2160.246568	21.191309
70.594731	2157.594750	21.196327
70.705719	2167.749365	21.201344
70.983448	2170.377395	21.206362
70.542439	2178.732824	21.211379
70.736947	2184.579485	21.216397
70.930081	2181.684116	21.221415
71.053999	2180.525253	21.226432
71.165596	2169.701045	21.231450
71.100913	2170.351165	21.236467
71.298568	2173.022543	21.241485
71.531409	2170.767613	21.246503
71.223620	2162.221206	21.251520
71.520907	2166.096105	21.256538
71.396237	2178.688698	21.261555
71.595004	2181.267381	21.266573
71.757731	2181.152026	21.271591
71.692956	2199.131382	21.276608
71.799975	2203.520765	21.281626
71.494315	2204.799640	21.286643
71.452520	2215.974342	21.291661
71.806701	2211.636317	21.296679
71.327911	2213.885464	21.301696
71.941476	2215.409658	21.306714
72.218876	2226.498555	21.311731
72.364985	2241.695871	21.316749
72.259678	2232.908500	21.321767
72.057037	2242.036326	21.326784
72.654032	2235.882314	21.331802
72.592997	2234.823688	21.336819
72.528806	2223.586003	21.341837
72.764487	2227.217376	21.346855
72.323504	2243.484864	21.351872
72.674963	2249.641615	21.356890
72.773826	2257.478182	21.361907
73.128676	2258.498319	21.366925
73.183975	2249.573187	21.371943
73.093427	2255.668343	21.376960
73.251615	2256.702869	21.381978
73.350755	2258.070751	21.386995
73.275322	2259.409611	21.392013
73.365196	2266.859309	21.397031
73.056241	2266.441213	21.402048
73.446358	2267.189007	21.407066
73.476565	2272.725670	21.412083
73.320308	2285.426122	21.417101
73.785376	2281.483506	21.422119
73.995060	2286.625581	21.427136
73.451157	2274.194578	21.432154
73.339987	2287.658197	21.437171
73.736071	2305.789657	21.442189
74.057429	2305.669740	21.447207
74.326534	2308.958230	21.452224
74.463900	2306.527338	21.457242
74.563343	2302.980741	21.462259
74.545761	2306.117207	21.467277
75.051066	2295.968356	21.472295
74.992352	2298.394933	21.477312
74.809172	2294.903504	21.482330
74.896200	2292.658872	21.487347
74.809287	2308.526016	21.492365
74.997667	2302.335765	21.497383
74.947250	2296.648527	21.502400
74.815611	2298.787373	21.507418
74.725729	2303.552605	21.512435
74.874895	2297.885928	21.517453
74.996656	2318.143694	21.522471
75.239465	2327.533571	21.527488
75.411752	2329.175378	21.532506
75.398087	2336.563484	21.537523
75.504142	2331.913497	21.542541
75.274234	2323.775560	21.547559
75.588042	2335.418324	21.552576
75.744483	2353.747107	21.557594
76.051267	2347.383149	21.562611
75.660950	2348.309905	21.567629
76.144741	2351.980619	21.572647
76.124291	2359.143099	21.577664
76.082010	2356.409032	21.582682
75.867879	2357.790897	21.587699
76.029380	2359.220526	21.592717
76.320572	2380.302685	21.597735
76.523607	2390.748517	21.602752
76.633121	2386.269389	21.607770
76.824024	2381.990185	21.612787
76.650493	2390.299166	21.617805
76.995234	2382.772300	21.622823
77.013914	2391.132586	21.627840
77.137939	2381.221475	21.632858
77.173984	2376.005324	21.637875
76.982816	2386.204107	21.642893
77.236323	2377.480189	21.647911
77.301633	2383.313632	21.652928
76.991138	2375.985587	21.657946
76.953721	2387.527384	21.662963
77.143564	2404.592320	21.667981
77.178927	2401.045464	21.672999
77.183062	2415.208207	21.678016
77.483971	2412.974080	21.683034
77.164372	2397.793279	21.688051
77.214382	2408.026235	21.693069
78.104333	2407.525372	21.698087
77.870196	2419.478809	21.703104
78.230789	2424.866253	21.708122
78.437192	2420.661639	21.713139
77.996354	2425.864210	21.718157
78.723995	2410.570975	21.723175
78.375550	2412.032515	21.728192
78.527891	2408.881656	21.733210
78.796791	2415.676291	21.738227
78.442791	2421.096781	21.743245
78.612965	2423.397766	21.748263
78.806494	2413.551523	21.753280
78.935897	2413.003117	21.758298
78.688103	2413.493752	21.763315
78.645346	2433.127319	21.768333
79.247339	2444.585546	21.773351
79.247999	2437.909165	21.778368
79.020814	2452.058988	21.783386
79.506627	2443.768273	21.788403
79.190750	2444.907130	21.793421
79.286658	2443.855625	21.798439
79.211697	2449.249306	21.803456
79.141090	2459.507738	21.808474
79.742632	2471.652241	21.813491
79.459324	2482.654851	21.818509
79.997656	2471.194596	21.823527
79.740994	2467.291278	21.828544
80.024293	2478.375838	21.833562
80.025424	2477.035679	21.838579
80.101938	2496.136653	21.843597
80.446770	2486.892493	21.848615
81.066006	2478.921032	21.853632
81.343220	2470.896255	21.858650
81.309834	2451.497870	21.863667
81.004702	2451.631073	21.868685
81.135849	2439.530292	21.873703
81.471993	2445.043824	21.878720
81.207109	2451.047595	21.883738
81.683269	2440.519630	21.888755
81.213658	2424.997864	21.893773
80.974383	2411.939476	21.898791
80.853560	2422.195553	21.903808
80.903437	2442.500792	21.908826
81.357992	2434.143991	21.913843
81.161218	2441.051017	21.918861
81.053859	2427.725163	21.923879
81.499508	2453.873332	21.928896
81.497089	2460.457717	21.933914
81.723459	2471.531208	21.938931
81.730432	2485.531351	21.943949
81.660488	2474.408601	21.948967
81.778479	2476.511536	21.953984
81.601767	2470.849434	21.959002
81.796648	2484.107936	21.964019
81.664722	2497.815312	21.969037
82.029107	2494.605777	21.974055
82.079547	2506.735867	21.979072
82.140483	2506.784960	21.984090
82.190053	2516.094094	21.989107
82.354833	2542.491963	21.994125
82.599056	2543.389464	21.999143
82.746754	2539.320496	22.004160
82.933048	2532.484666	22.009178
83.483415	2530.819899	22.014195
83.123046	2536.963097	22.019213
83.192567	2524.958648	22.024231
83.222328	2525.763246	22.029248
83.181882	2525.019292	22.034266
83.636038	2527.465090	22.039283
83.280187	2535.675148	22.044301
83.444075	2519.174243	22.049319
83.906789	2531.255518	22.054336
83.833675	2534.167558	22.059354
83.743232	2514.307287	22.064371
83.416972	2535.940876	22.069389
83.755995	2548.560293	22.074407
84.146430	2545.364158	22.079424
84.586644	2541.875955	22.084442
84.973949	2531.326786	22.089459
84.672218	2531.391715	22.094477
84.728582	2517.037208	22.099495
84.821501	2506.193805	22.104512
84.294208	2503.878814	22.109530
84.581824	2519.577008	22.114547
84.764725	2533.484349	22.119565
84.468516	2524.545689	22.124583
84.777300	2525.681326	22.129600
84.451074	2523.383892	22.134618
84.675731	2524.961361	22.139635
84.658944	2532.303229	22.144653
84.811471	2549.254026	22.149671
85.136831	2557.747968	22.154688
85.078158	2552.148217	22.159706
85.283155	2549.769297	22.164723
85.269475	2558.771602	22.169741
85.754211	2573.149943	22.174759
85.942450	2576.425083	22.179776
85.621871	2596.129566	22.184794
85.737502	2583.347411	22.189811
85.786743	2578.514426	22.194829
85.826141	2577.769873	22.199847
86.092653	2568.461445	22.204864
86.008787	2584.797439	22.209882
86.206038	2587.152633	22.214899
86.550404	2591.048403	22.219917
86.459729	2599.552456	22.224935
86.690009	2596.434741	22.229952
86.429693	2614.926593	22.234970
86.770577	2608.817512	22.239987
86.825722	2602.360785	22.245005
86.759445	2610.828137	22.250023
86.645356	2600.688135	22.255040
86.746038	2632.204772	22.260058
87.123422	2630.009550	22.265075
87.209780	2635.475453	22.270093
87.332669	2634.937958	22.275111
87.670972	2634.016064	22.280128
87.252226	2632.131127	22.285146
87.305619	2630.558707	22.290163
87.626121	2652.786736	22.295181
87.927825	2666.569058	22.300199
88.036417	2659.360202	22.305216
87.935470	2661.143056	22.310234
88.231029	2661.314397	22.315251
88.169488	2651.144420	22.320269
87.983390	2660.328417	22.325287
88.259099	2652.054200	22.330304
87.878188	2671.477423	22.335322
88.317016	2679.975123	22.340339
88.256320	2686.989295	22.345357
88.454119	2680.558568	22.350375
88.642843	2684.695819	22.355392
88.700728	2689.050745	22.360410
88.614288	2681.268227	22.365427
88.974288	2686.953093	22.370445
88.790058	2692.988116	22.375463
88.949763	2710.212696	22.380480
88.832938	2720.770265	22.385498
88.952986	2716.578659	22.390515
89.076254	2718.015822	22.395533
89.022771	2718.877097	22.400551
89.665454	2729.549712	22.405568
89.598895	2747.675466	22.410586
89.429296	2741.728241	22.415603
90.007275	2740.285654	22.420621
89.793514	2737.895197	22.425639
90.194403	2737.663322	22.430656
89.938621	2745.775463	22.435674
89.974328	2734.705931	22.440691
90.360603	2750.250267	22.445709
90.271687	2762.454371	22.450727
90.342836	2753.719039	22.455744
90.444359	2763.908680	22.460762
90.268783	2753.644884	22.465779
90.666629	2758.025542	22.470797
90.625804	2781.412239	22.475815
91.176569	2782.050054	22.480832
91.036246	2790.004561	22.485850
90.961387	2782.183071	22.490867
91.319777	2787.132048	22.495885
91.241730	2788.915463	22.500903
91.725394	2773.746043	22.505920
91.480497	2784.781888	22.510938
91.264479	2782.943352	22.515955
91.381782	2790.873792	22.520973
91.792969	2805.926684	22.525991
92.292622	2797.096507	22.531008
92.188713	2799.862115	22.536026
92.054627	2800.911511	22.541043
92.488878	2802.033918	22.546061
92.220567	2809.701720	22.551079
92.583243	2801.793749	22.556096
92.689781	2804.068695	22.561114
92.735740	2800.708572	22.566131
92.691863	2795.290533	22.571149
92.631515	2796.363963	22.576167
92.679665	2791.275982	22.581184
92.698840	2801.117457	22.586202
92.793314	2801.613750	22.591219
93.212794	2810.473762	22.596237
93.057659	2826.860762	22.601255
93.402192	2818.745552	22.606272
93.369205	2828.345672	22.611290
93.164996	2828.670067	22.616307
93.275731	2822.039108	22.621325
93.424976	2812.774714	22.626343
93.608587	2826.575905	22.631360
93.490386	2850.357369	22.636378
93.994628	2840.313062	22.641395
94.246451	2846.913078	22.646413
93.856442	2838.712153	22.651431
94.028239	2838.896861	22.656448
94.522789	2847.996450	22.661466
93.829575	2858.887143	22.666483
94.225031	2862.762730	22.671501
94.225361	2874.414790	22.676519
94.427412	2873.013838	22.681536
94.306378	2869.568306	22.686554
94.365920	2874.918650	22.691571
94.515558	2887.345630	22.696589
94.523180	2908.643472	22.701607
94.893977	2902.765154	22.706624
95.182435	2909.257178	22.711642
95.281935	2917.104407	22.716659
95.381617	2897.931893	22.721677
95.517546	2915.532273	22.726695
95.942225	2926.077667	22.731712
95.732530	2935.026362	22.736730
95.995445	2930.873294	22.741747
96.460340	2931.427277	22.746765
96.007594	2918.303343	22.751783
95.961785	2912.628503	22.756800
95.941489	2918.919588	22.761818
95.815599	2921.555389	22.766835
95.997215	2923.102218	22.771853
96.199499	2926.762897	22.776871
96.267447	2930.203655	22.781888
96.554070	2940.434479	22.786906
96.518367	2948.100133	22.791923
96.672171	2946.579197	22.796941
96.669106	2958.598407	22.801959
96.951433	2959.740025	22.806976
96.773099	2949.824578	22.811994
96.795217	2976.539666	22.817011
97.086062	2976.235424	22.822029
97.023296	2984.153987	22.827047
97.263375	2989.134390	22.832064
97.393996	2997.268243	22.837082
97.162646	3008.142168	22.842099
97.550657	3010.256856	22.847117
97.703781	3007.856519	22.852135
98.021062	3000.930337	22.857152
98.032347	3005.217464	22.862170
98.153187	3034.858008	22.867187
98.481237	3029.447327	22.872205
98.487556	3028.840893	22.877223
98.620108	3039.144878	22.882240
98.418843	3041.365603	22.887258
98.092933	3040.458562	22.892275
98.642531	3035.260871	22.897293
98.698890	3036.521328	22.902311
98.755140	3035.083038	22.907328
99.408613	3047.293037	22.912346
99.519424	3049.150392	22.917363
99.445927	3045.944992	22.922381
99.285865	3043.680256	22.927399
99.372233	3044.364900	22.932416
99.495802	3042.810369	22.937434
99.695334	3041.097621	22.942451
99.968761	3038.855742	22.947469
99.766416	3050.670556	22.952487
99.977788	3068.586983	22.957504
100.317390	3073.695060	22.962522
99.993920	3076.726521	22.967539
100.298317	3071.818150	22.972557
100.511125	3070.685477	22.977575
100.573980	3071.657073	22.982592
100.661215	3068.163697	22.987610
100.248436	3081.068798	22.992627
100.758563	3063.730588	22.997645
100.773890	3069.215862	23.002663
100.628734	3095.306445	23.007680
100.958567	3096.752423	23.012698
100.979869	3085.544079	23.017715
101.301500	3087.318571	23.022733
101.259631	3096.366397	23.027751
101.412385	3089.119336	23.032768
101.707998	3102.298340	23.037786
101.312161	3113.726282	23.042803
101.992802	3117.265051	23.047821
102.001059	3124.866049	23.052839
101.834875	3121.366504	23.057856
102.139671	3123.499683	23.062874
101.884718	3125.232449	23.067891
102.560873	3119.334694	23.072909
102.520760	3118.079640	23.077927
101.998865	3122.781668	23.082944
102.479024	3109.785699	23.087962
102.457916	3118.578142	23.092979
102.726810	3135.629250	23.097997
102.678793	3137.754589	23.103015
102.429917	3135.691520	23.108032
102.812388	3135.074895	23.113050
102.956695	3137.126723	23.118067
102.886870	3155.417664	23.123085
102.956920	3173.507957	23.128103
103.099288	3173.084153	23.133120
103.459724	3174.016426	23.138138
103.591632	3173.523092	23.143155
103.736941	3186.474250	23.148173
103.618533	3192.729296	23.153191
103.820473	3190.558263	23.158208
104.040690	3199.538827	23.163226
104.069499	3203.701461	23.168243
104.203902	3193.059778	23.173261
104.050075	3203.629301	23.178279
104.216779	3212.501392	23.183296
104.831918	3220.422232	23.188314
104.789865	3218.603322	23.193331
105.166963	3204.166835	23.198349
105.344487	3197.919165	23.203367
105.469415	3203.227717	23.208384
105.605518	3201.792358	23.213402
105.400220	3216.160124	23.218419
105.792199	3207.516010	23.223437
105.638926	3200.050176	23.228455
105.708506	3204.843863	23.233472
105.298815	3204.453800	23.238490
105.454350	3206.370318	23.243507
105.736885	3223.775958	23.248525
106.213283	3235.279940	23.253543
106.165409	3240.050526	23.258560
106.300456	3227.799275	23.263578
106.472797	3229.726405	23.268595
106.498961	3227.070637	23.273613
106.875158	3232.473111	23.278631
106.956429	3220.827203	23.283648
107.027225	3219.640822	23.288666
106.878832	3220.698908	23.293683
106.585841	3226.245814	23.298701
106.916537	3227.993629	23.303719
107.387843	3238.939010	23.308736
107.369676	3242.958237	23.313754
107.418762	3253.013559	23.318771
107.528950	3244.041580	23.323789
107.624178	3251.368823	23.328807
107.295689	3252.749581	23.333824
107.954420	3243.672002	23.338842
107.806975	3253.800744	23.343859
107.602200	3260.366543	23.348877
107.998538	3264.547991	23.353895
107.893831	3275.511019	23.358912
108.061378	3275.152737	23.363930
107.958518	3299.555186	23.368947
108.136333	3296.374349	23.373965
108.709055	3310.317581	23.378983
108.914230	3316.627476	23.384000
109.048887	3304.014813	23.389018
108.613941	3310.037171	23.394035
109.058292	3312.797316	23.399053
109.122184	3310.928605	23.404071
108.806083	3313.594721	23.409088
108.855123	3323.722537	23.414106
109.336788	3318.980861	23.419123
109.335593	3326.894149	23.424141
109.822486	3314.870911	23.429159
109.944068	3326.526897	23.434176
109.900033	3334.077977	23.439194
110.143319	3346.963080	23.444211
110.368790	3348.951525	23.449229
110.219652	3349.223916	23.454247
110.561305	3353.486472	23.459264
110.791401	3342.737142	23.464282
110.653561	3344.039556	23.469299
110.568870	3344.094998	23.474317
110.556834	3341.370326	23.479335
110.555711	3339.623378	23.484352
110.801175	3360.354588	23.489370
111.058652	3360.656642	23.494387
110.837730	3369.712560	23.499405
111.341111	3371.876740	23.504423
111.330685	3387.727427	23.509440
111.728433	3390.104341	23.514458
111.742660	3405.537586	23.519475
111.557120	3410.654201	23.524493
111.759892	3410.420805	23.529511
111.609481	3404.978030	23.534528
111.783635	3409.898202	23.539546
112.483924	3426.079919	23.544563
112.550944	3418.199624	23.549581
112.490592	3425.318403	23.554599
112.076240	3426.233047	23.559616
112.663470	3430.952686	23.564634
112.424713	3447.604947	23.569651
112.549893	3464.638431	23.574669
112.942506	3456.014155	23.579687
112.832834	3458.575712	23.584704
112.964785	3465.987933	23.589722
113.241239	3477.341668	23.594739
113.261178	3489.214967	23.599757
113.470458	3487.404102	23.604775
113.592121	3498.304685	23.609792
114.105632	3490.547429	23.614810
114.534077	3487.818452	23.619827
114.688779	3485.597704	23.624845
115.107876	3466.147692	23.629863
114.572942	3471.123239	23.634880
114.664296	3466.494832	23.639898
114.893022	3464.196894	23.644915
114.722939	3470.406259	23.649933
114.667726	3453.498042	23.654951
114.886429	3469.253078	23.659968
115.159379	3479.873136	23.664986
115.349297	3490.524244	23.670003
115.543970	3500.023776	23.675021
115.077282	3488.201673	23.680039
115.211087	3496.629360	23.685056
115.334447	3484.263301	23.690074
115.166915	3491.384073	23.695091
115.473221	3501.773041	23.700109
116.055500	3515.286530	23.705127
115.598404	3528.412711	23.710144
115.837400	3515.970433	23.715162
116.138231	3521.284280	23.720179
116.149100	3545.944705	23.725197
116.253942	3543.807385	23.730215
116.068673	3548.824787	23.735232
116.446433	3547.114031	23.740250
116.293062	3549.334394	23.745267
116.291892	3563.260083	23.750285
116.738335	3565.110074	23.755303
116.850392	3565.097573	23.760320
116.847921	3581.631012	23.765338
117.060131	3587.804814	23.770355
117.152430	3606.902582	23.775373
117.380481	3604.360243	23.780391
117.145575	3609.753983	23.785408
117.419087	3626.214700	23.790426
117.763996	3624.928269	23.795443
117.732275	3630.057729	23.800461
118.165531	3639.476584	23.805479
118.231138	3665.264001	23.810496
118.427183	3662.499771	23.815514
118.628568	3660.560661	23.820531
118.423923	3658.948883	23.825549
118.675142	3654.422353	23.830567
118.768822	3668.880507	23.835584
119.212685	3673.058545	23.840602
119.316734	3683.269634	23.845619
118.997335	3686.763934	23.850637
119.435677	3673.515740	23.855655
119.292287	3680.668829	23.860672
119.386601	3683.341209	23.865690
119.675370	3696.433265	23.870707
120.120104	3702.797831	23.875725
119.903078	3710.070978	23.880743
120.069924	3719.389804	23.885760
120.250733	3707.870789	23.890778
120.567482	3704.999598	23.895795
120.342965	3708.339639	23.900813
120.644542	3721.132349	23.905831
120.600971	3728.612282	23.910848
120.709198	3723.897543	23.915866
120.849920	3728.219783	23.920883
120.850647	3731.630487	23.925901
120.987334	3741.429519	23.930919
121.216727	3760.106780	23.935936
121.252884	3759.508774	23.940954
121.395701	3746.646366	23.945971
121.398262	3759.060552	23.950989
121.938141	3771.569432	23.956007
121.883750	3781.431953	23.961024
121.964208	3781.219156	23.966042
122.458315	3785.387348	23.971059
122.413536	3775.591827	23.976077
122.442523	3773.757176	23.981095
122.747987	3778.438046	23.986112
122.646705	3779.104515	23.991130
122.945411	3779.059993	23.996147
123.040942	3813.644928	24.001165
122.872736	3806.807666	24.006183
123.054754	3806.197762	24.011200
122.962166	3816.617420	24.016218
123.129378	3801.186291	24.021235
123.170924	3821.082101	24.026253
123.612405	3833.346260	24.031271
123.851827	3842.246068	24.036288
123.592398	3849.436913	24.041306
123.785248	3834.964538	24.046323
123.505145	3853.737517	24.051341
123.904098	3849.875519	24.056359
124.050787	3857.261082	24.061376
123.931567	3874.277129	24.066394
124.235817	3886.215961	24.071411
124.656517	3896.852838	24.076429
124.647382	3894.507131	24.081447
124.838055	3895.753339	24.086464
125.215016	3892.737121	24.091482
125.393399	3910.695801	24.096499
125.195870	3923.127036	24.101517
125.278416	3923.256426	24.106535
125.662830	3927.417190	24.111552
125.494284	3918.544426	24.116570
125.824999	3918.410360	24.121587
125.660375	3930.343626	24.126605
125.891747	3936.479361	24.131623
126.225537	3949.838219	24.136640
126.135749	3935.951844	24.141658
126.599101	3929.418849	24.146675
126.380819	3937.945899	24.151693
126.515409	3941.695174	24.156711
126.899691	3962.620008	24.161728
126.994704	3968.379451	24.166746
127.192147	3970.198980	24.171763
127.102961	3967.500726	24.176781
127.104884	3960.181723	24.181799
127.510464	3971.448340	24.186816
127.389484	3988.581737	24.191834
127.800808	3983.185316	24.196851
127.982756	4000.523013	24.201869
128.029200	3995.167980	24.206887
128.037789	3988.894363	24.211904
127.984595	3997.578033	24.216922
128.523163	4008.604978	24.221939
128.203784	4018.728765	24.226957
128.384620	4028.518321	24.231975
128.676256	4026.144550	24.236992
128.823094	4044.457037	24.242010
129.015605	4046.428184	24.247027
129.321476	4043.824095	24.252045
129.359888	4048.728710	24.257063
129.483670	4046.566538	24.262080
129.572591	4047.866187	24.267098
129.418320	4052.066780	24.272115
129.649565	4066.683684	24.277133
129.546951	4069.042197	24.282151
129.802755	4075.425142	24.287168
129.998852	4081.519124	24.292186
130.046417	4087.204164	24.297203
130.242565	4105.321952	24.302221
130.257743	4100.848471	24.307239
130.415271	4111.563234	24.312256
130.425698	4141.674944	24.317274
130.814388	4141.923837	24.322291
131.062267	4125.288842	24.327309
130.876932	4128.470521	24.332327
131.826321	4145.028783	24.337344
131.885837	4152.987974	24.342362
132.155399	4153.499084	24.347379
132.260543	4150.281655	24.352397
132.252386	4160.465533	24.357415
132.361623	4146.906732	24.362432
132.584436	4151.376558	24.367450
132.808276	4145.055893	24.372467
133.112288	4146.872008	24.377485
132.871248	4143.056630	24.382503
133.136659	4139.349705	24.387520
132.773505	4147.639770	24.392538
132.917288	4130.779437	24.397555
133.129105	4149.364396	24.402573
132.993131	4149.084596	24.407591
133.314844	4151.785628	24.412608
133.244778	4142.721256	24.417626
133.184280	4149.413203	24.422643
133.060113	4166.591418	24.427661
133.311407	4175.995389	24.432679
133.870537	4178.504039	24.437696
133.781605	4201.209445	24.442714
133.970407	4199.255812	24.447731
133.970207	4207.573736	24.452749
133.792599	4223.563141	24.457767
134.299847	4227.300125	24.462784
134.092029	4237.153637	24.467802
134.572118	4240.325000	24.472819
135.008729	4259.694649	24.477837
134.865608	4267.375552	24.482855
134.900949	4264.835420	24.487872
135.020213	4282.579875	24.492890
135.388496	4284.785805	24.497907
135.817617	4280.478928	24.502925
136.478283	4282.016036	24.507943
136.524121	4286.180083	24.512960
136.408126	4273.778535	24.517978
136.489291	4276.644146	24.522995
136.382152	4265.152613	24.528013
136.434306	4271.211788	24.533031
136.935655	4287.401689	24.538048
136.824066	4305.263453	24.543066
137.050299	4301.058209	24.548083
137.018923	4312.983925	24.553101
136.847050	4306.586052	24.558119
137.400628	4309.881910	24.563136
137.122467	4314.531416	24.568154
137.531907	4325.402354	24.573171
138.056846	4335.471093	24.578189
137.743012	4344.808692	24.583207
137.878595	4339.424639	24.588224
137.883060	4355.960509	24.593242
138.062099	4348.106907	24.598259
138.273141	4348.769042	24.603277
137.761268	4379.196660	24.608295
138.496736	4376.004177	24.613312
138.284899	4395.442554	24.618330
138.954179	4399.546929	24.623347
139.169696	4407.761202	24.628365
139.032872	4425.002427	24.633383
139.362217	4430.489842	24.638400
139.237942	4426.807079	24.643418
139.425692	4435.692143	24.648435
140.185699	4430.678538	24.653453
140.250053	4428.765126	24.658471
140.847125	4433.055863	24.663488
140.585463	4445.181946	24.668506
140.923483	4429.248713	24.673523
140.976531	4425.994950	24.678541
140.897946	4428.239696	24.683559
140.964606	4414.234124	24.688576
141.114222	4443.641876	24.693594
141.078303	4455.762166	24.698611
141.529141	4460.290474	24.703629
140.915368	4459.753371	24.708647
141.070133	4455.881177	24.713664
141.260861	4469.175138	24.718682
141.236018	4489.671790	24.723699
141.599719	4489.287766	24.728717
141.441340	4518.168160	24.733735
141.849370	4506.986631	24.738752
141.911281	4528.520259	24.743770
142.437527	4537.586476	24.748787
142.906680	4536.025883	24.753805
143.054576	4533.329698	24.758823
143.276872	4538.604507	24.763840
143.172146	4550.838610	24.768858
143.642244	4543.710107	24.773875
143.409990	4534.202192	24.778893
143.334754	4535.194336	24.783911
143.557424	4532.578323	24.788928
143.784386	4540.658088	24.793946
143.614395	4553.689652	24.798963
143.857021	4562.875981	24.803981
143.630921	4569.201738	24.808999
143.813807	4581.324951	24.814016
144.118339	4592.892598	24.819034
144.047886	4584.089473	24.824051
144.627661	4601.232567	24.829069
145.295588	4605.515582	24.834087
145.879072	4599.847966	24.839104
145.847389	4601.408161	24.844122
145.948711	4608.135382	24.849139
146.323247	4597.401485	24.854157
146.152493	4605.534794	24.859175
146.013546	4597.960005	24.864192
146.114296	4599.502255	24.869210
145.907240	4606.906464	24.874227
146.305461	4604.552795	24.879245
146.043329	4605.277768	24.884263
146.110431	4622.132731	24.889280
146.411243	4636.478025	24.894298
146.343603	4636.785399	24.899315
146.795778	4633.896389	24.904333
146.630065	4664.328000	24.909351
146.915305	4661.183867	24.914368
147.168900	4662.994200	24.919386
147.583310	4671.149762	24.924403
147.716792	4676.922799	24.929421
147.246338	4682.131791	24.934439
148.227224	4691.876981	24.939456
148.166712	4708.772810	24.944474
148.026986	4722.440120	24.949491
148.363902	4726.036065	24.954509
148.164228	4723.842986	24.959527
148.312729	4753.358996	24.964544
148.530212	4759.567831	24.969562
148.538305	4767.424012	24.974579
149.125222	4764.215444	24.979597
149.364478	4772.151159	24.984615
149.181276	4772.387070	24.989632
149.144950	4791.174047	24.994650
149.439177	4796.077577	24.999667
149.855267	4787.681391	25.004685
149.887047	4811.561156	25.009703
150.465769	4817.590630	25.014720
150.655477	4819.389489	25.019738
150.317489	4821.975605	25.024755
150.572745	4820.002648	25.029773
150.692492	4835.762819	25.034791
151.218358	4839.713041	25.039808
151.168313	4845.845630	25.044826
150.960509	4863.290423	25.049843
151.622400	4851.280014	25.054861
151.359797	4878.500967	25.059879
151.481156	4874.939338	25.064896
151.726445	4877.242062	25.069914
151.784589	4885.698753	25.074931
152.184634	4892.705905	25.079949
151.622141	4917.282115	25.084967
152.075345	4915.722152	25.089984
152.335392	4931.018249	25.095002
152.522674	4953.373959	25.100019
152.854040	4941.508261	25.105037
152.708975	4949.882803	25.110055
152.777576	4970.203999	25.115072
153.188105	4969.611025	25.120090
152.759906	4983.070295	25.125107
153.458256	4983.985440	25.130125
153.424253	5009.442288	25.135143
153.521298	5002.274421	25.140160
153.773598	5018.482610	25.145178
153.957870	5030.116914	25.150195
154.415569	5033.221270	25.155213
154.534756	5033.590311	25.160231
154.816563	5043.630386	25.165248
155.183913	5050.502445	25.170266
155.480297	5055.975842	25.175283
155.445543	5043.396461	25.180301
155.566582	5051.469974	25.185319
155.805515	5053.221353	25.190336
155.913351	5051.681037	25.195354
155.716099	5052.811497	25.200371
155.594403	5061.126720	25.205389
155.684149	5087.951198	25.210407
156.023504	5085.328020	25.215424
156.045520	5083.235283	25.220442
156.316362	5103.205877	25.225459
156.378381	5115.349082	25.230477
156.543689	5145.209944	25.235495
156.571102	5157.234870	25.240512
157.360328	5159.665897	25.245530
156.969307	5177.930775	25.250547
157.528665	5176.075657	25.255565
157.521578	5181.452766	25.260583
157.619567	5199.928243	25.265600
157.870445	5208.429257	25.270618
158.132084	5215.912233	25.275635
158.317573	5207.874044	25.280653
158.044751	5223.491178	25.285671
158.839521	5212.755546	25.290688
159.318527	5207.485732	25.295706
159.379670	5208.536102	25.300723
159.969682	5202.289172	25.305741
159.950075	5194.148641	25.310759
159.870938	5186.388467	25.315776
160.380188	5190.717948	25.320794
160.348173	5201.058432	25.325811
160.393168	5203.007246	25.330829
160.181030	5198.018581	25.335847
160.580438	5208.889433	25.340864
160.718913	5216.030512	25.345882
160.261865	5235.908134	25.350899
160.680821	5222.893362	25.355917
160.786532	5237.317120	25.360935
160.573898	5252.508540	25.365952
160.964251	5252.892238	25.370970
161.000700	5268.427210	25.375987
161.521918	5285.204311	25.381005
161.425924	5301.391198	25.386023
161.333428	5304.315224	25.391040
161.801644	5314.130554	25.396058
161.688654	5334.410564	25.401075
161.910642	5327.769612	25.406093
162.460842	5350.325800	25.411111
162.413721	5350.430165	25.416128
162.357652	5356.447399	25.421146
162.200489	5378.042413	25.426163
163.239566	5373.968361	25.431181
163.656696	5382.204568	25.436199
163.694940	5372.407320	25.441216
163.750116	5362.753757	25.446234
164.149146	5394.594849	25.451251
164.575194	5389.640064	25.456269
164.599042	5399.426102	25.461287
164.782497	5404.671792	25.466304
165.125368	5390.379520	25.471322
165.170601	5405.029596	25.476339
164.855938	5399.302195	25.481357
165.078760	5392.040523	25.486375
165.100654	5390.773071	25.491392
165.425092	5395.810006	25.496410
164.986042	5399.546134	25.501427
165.040129	5415.113381	25.506445
165.534889	5432.184026	25.511463
165.539819	5434.323765	25.516480
165.800473	5448.095655	25.521498
165.733691	5458.239664	25.526515
165.801720	5472.112309	25.531533
166.210990	5477.616816	25.536551
166.242131	5493.233607	25.541568
166.382454	5504.271506	25.546586
166.691406	5516.532118	25.551603
166.960432	5544.696057	25.556621
167.212939	5552.661875	25.561639
166.843987	5553.060789	25.566656
167.630592	5571.959222	25.571674
167.642711	5585.501787	25.576691
168.273206	5578.162039	25.581709
168.058885	5577.739621	25.586727
168.313835	5610.034546	25.591744
168.684586	5610.525446	25.596762
168.745662	5615.504378	25.601779
169.859913	5605.251600	25.606797
170.313702	5601.925473	25.611815
170.038679	5590.271307	25.616832
170.361092	5581.510202	25.621850
170.024262	5576.547138	25.626867
170.069345	5578.686956	25.631885
170.242526	5568.292406	25.636903
169.879144	5585.724331	25.641920
170.220856	5604.737264	25.646938
170.663212	5616.823923	25.651955
170.381263	5609.291959	25.656973
170.519438	5628.369264	25.661991
170.514055	5638.170124	25.667008
170.702875	5641.668689	25.672026
170.969893	5650.588205	25.677044
170.876935	5664.397055	25.682061
171.301603	5674.620656	25.687079
171.468090	5690.297971	25.692096
171.498065	5712.142093	25.697114
171.561218	5727.674289	25.702132
171.716953	5740.849111	25.707149
172.204065	5738.643214	25.712167
172.271952	5770.890626	25.717184
172.979599	5775.363503	25.722202
173.129107	5768.672521	25.727220
173.167481	5778.111065	25.732237
173.752873	5778.300324	25.737255
173.530953	5789.699505	25.742272
173.768441	5797.184389	25.747290
174.456401	5807.286609	25.752308
174.577596	5810.050598	25.757325
174.675130	5809.484900	25.762343
174.590815	5798.092422	25.767360
174.424912	5803.290835	25.772378
174.716388	5807.016608	25.777396
174.999559	5827.466087	25.782413
175.310993	5835.674322	25.787431
175.342215	5833.651629	25.792448
175.223526	5834.204505	25.797466
175.458183	5846.300065	25.802484
175.401767	5856.341027	25.807501
175.678201	5865.977336	25.812519
175.814496	5878.354570	25.817536
175.696437	5895.471456	25.822554
176.154378	5905.626708	25.827572
176.018438	5921.805478	25.832589
176.404533	5923.920107	25.837607
176.687281	5941.830804	25.842624
177.136461	5963.991116	25.847642
176.643536	5971.903905	25.852660
177.072676	5983.338197	25.857677
177.379013	5979.843017	25.862695
177.494987	6006.447373	25.867712
177.783654	6009.976775	25.872730
178.053754	6033.677268	25.877748
178.434098	6043.237453	25.882765
179.128868	6048.467786	25.887783
179.038229	6058.756306	25.892800
178.886965	6053.237140	25.897818
179.216932	6048.665413	25.902836
179.356708	6050.993229	25.907853
179.704428	6067.623036	25.912871
179.687049	6079.993531	25.917888
179.429182	6080.226044	25.922906
180.013700	6086.233795	25.927924
179.907979	6121.604068	25.932941
180.133677	6104.281937	25.937959
180.273357	6134.151673	25.942976
180.423089	6137.323677	25.947994
180.497468	6147.636967	25.953012
180.847729	6159.464804	25.958029
181.249268	6160.813785	25.963047
181.042548	6165.094485	25.968064
181.810892	6190.741605	25.973082
182.089028	6200.365239	25.978100
181.741886	6203.025543	25.983117
182.351395	6213.229195	25.988135
182.453477	6221.706125	25.993152
182.391516	6228.677597	25.998170
183.165691	6240.722908	26.003188
182.946454	6249.949135	26.008205
183.072959	6250.729280	26.013223
183.403389	6264.899490	26.018240
183.400726	6280.454133	26.023258
183.534297	6289.005438	26.028276
183.585154	6300.558381	26.033293
184.042148	6311.227537	26.038311
184.473586	6324.623489	26.043328
184.619244	6328.559342	26.048346
184.628669	6325.799889	26.053364
184.327544	6340.914835	26.058381
184.822502	6345.990059	26.063399
184.881554	6365.514093	26.068416
185.319393	6382.593213	26.073434
185.381817	6381.719061	26.078452
185.313134	6396.324698	26.083469
185.440585	6412.558109	26.088487
185.521817	6422.367199	26.093504
185.973201	6429.120844	26.098522
186.485595	6440.915018	26.103540
186.413685	6445.437351	26.108557
187.020207	6450.635937	26.113575
187.071212	6472.479215	26.118592
187.569762	6474.672211	26.123610
187.361343	6458.260956	26.128628
187.475367	6467.126674	26.133645
187.425917	6470.428525	26.138663
187.670360	6484.925803	26.143680
187.776456	6505.166004	26.148698
188.350901	6507.688266	26.153716
187.949198	6530.879122	26.158733
188.540498	6538.444514	26.163751
188.384821	6540.551873	26.168768
188.511060	6561.810287	26.173786
188.969964	6566.421365	26.178804
188.817848	6584.795278	26.183821
189.307187	6579.289793	26.188839
189.718434	6598.771676	26.193856
189.472585	6616.768905	26.198874
189.894756	6615.877830	26.203892
190.103270	6633.211694	26.208909
190.482944	6636.504108	26.213927
190.843537	6641.629982	26.218944
191.076787	6666.405460	26.223962
191.567058	6661.410138	26.228980
191.543639	6666.364773	26.233997
192.124239	6672.959351	26.239015
191.908386	6663.342682	26.244032
192.121579	6679.326719	26.249050
192.396292	6698.621791	26.254068
192.214644	6694.201355	26.259085
192.311724	6695.614865	26.264103
192.402263	6710.122815	26.269120
192.549755	6733.908416	26.274138
192.744990	6738.874989	26.279156
192.602095	6758.881793	26.284173
193.159954	6767.764131	26.289191
193.136035	6779.209280	26.294208
193.112691	6799.979232	26.299226
193.778432	6810.103890	26.304244
193.928623	6821.837697	26.309261
194.891291	6832.851314	26.314279
195.185688	6836.028698	26.319296
195.259556	6835.022681	26.324314
195.437655	6828.047724	26.329332
195.459469	6838.374090	26.334349
195.894613	6815.938276	26.339367
196.058434	6823.271219	26.344384
196.387421	6846.995501	26.349402
196.647810	6848.821510	26.354420
196.685979	6861.447279	26.359437
196.983325	6856.657827	26.364455
197.489775	6843.102740	26.369472
197.885367	6824.532579	26.374490
198.369947	6825.323685	26.379508
198.232640	6798.627966	26.384525
198.191048	6790.339420	26.389543
198.424283	6781.065894	26.394560
198.361341	6781.232343	26.399578
198.703702	6785.974579	26.404596
198.623535	6781.973666	26.409613
198.588984	6795.830564	26.414631
198.342237	6810.071428	26.419648
198.263117	6815.636234	26.424666
198.828940	6824.266053	26.429684
198.983855	6849.557237	26.434701
199.183435	6842.217226	26.439719
199.026544	6858.893442	26.444736
198.930665	6885.706768	26.449754
199.165092	6906.168856	26.454772
199.412022	6911.828678	26.459789
200.095258	6927.342302	26.464807
200.302935	6927.168697	26.469824
200.589878	6950.256627	26.474842
200.716626	6959.927005	26.479860
201.250085	6964.404597	26.484877
201.078324	6963.467509	26.489895
201.903751	6974.450347	26.494912
201.655996	6973.646314	26.499930
201.846981	6975.510584	26.504948
201.903756	6982.249336	26.509965
202.368653	7003.321654	26.514983
202.747564	7012.911023	26.520000
202.603032	7027.740061	26.525018
202.779948	7034.674784	26.530036
202.629189	7042.692238	26.535053
202.835219	7060.312090	26.540071
203.733093	7063.806448	26.545088
203.448268	7077.429286	26.550106
203.871129	7073.635021	26.555124
203.868635	7098.493448	26.560141
204.125084	7116.820952	26.565159
204.188007	7119.022222	26.570176
204.248338	7152.870161	26.575194
204.671798	7155.497025	26.580212
205.031557	7178.501587	26.585229
205.094360	7184.708591	26.590247
205.528617	7193.920332	26.595264
205.697445	7209.610589	26.600282
205.663703	7213.954352	26.605300
205.747408	7235.008052	26.610317
205.775050	7251.161156	26.615335
206.124928	7268.751174	26.620352
206.764251	7269.601798	26.625370
207.161769	7277.456325	26.630388
207.492995	7295.911875	26.635405
207.508917	7301.150834	26.640423
207.867811	7302.855872	26.645440
207.792185	7330.199811	26.650458
207.902382	7332.142055	26.655476
208.331197	7340.370278	26.660493
208.546357	7354.362830	26.665511
208.849130	7354.444445	26.670528
208.739028	7372.216116	26.675546
208.962308	7390.155616	26.680564
209.013951	7397.344328	26.685581
209.477110	7401.966767	26.690599
209.890232	7415.500571	26.695616
209.855411	7428.806743	26.700634
209.893890	7433.641127	26.705652
210.161526	7454.467040	26.710669
210.276040	7460.703413	26.715687
210.962895	7471.758330	26.720704
210.988779	7482.294736	26.725722
211.120362	7491.025023	26.730740
211.030376	7499.342985	26.735757
211.386647	7521.601183	26.740775
211.520616	7535.955434	26.745792
211.637331	7557.019073	26.750810
211.435651	7564.118971	26.755828
211.947385	7581.813340	26.760845
212.263487	7594.526093	26.765863
212.528785	7613.485167	26.770880
212.373412	7636.762961	26.775898
212.867426	7627.465546	26.780916
213.456458	7658.039730	26.785933
213.458337	7681.052171	26.790951
213.616070	7682.981092	26.795968
213.868273	7709.676869	26.800986
214.242526	7713.619408	26.806004
214.466224	7714.687591	26.811021
214.719374	7731.349748	26.816039
215.058207	7728.426933	26.821056
215.322886	7740.046418	26.826074
215.378388	7752.862215	26.831092
215.867336	7764.317856	26.836109
215.712352	7774.895367	26.841127
215.924330	7770.784500	26.846144
216.064939	7802.167118	26.851162
216.098305	7791.491759	26.856180
216.724023	7817.793629	26.861197
216.576251	7822.859749	26.866215
217.073053	7828.474679	26.871232
217.249376	7849.076761	26.876250
217.350682	7851.437193	26.881268
217.965350	7852.751115	26.886285
217.999291	7883.579699	26.891303
218.192433	7885.709941	26.896320
218.066254	7901.388979	26.901338
218.338423	7911.863713	26.906356
218.647596	7924.577878	26.911373
218.625232	7941.311769	26.916391
219.124093	7948.277192	26.921408
219.261183	7977.985444	26.926426
219.794358	7983.940980	26.931444
219.899779	7997.274079	26.936461
219.975848	8009.836218	26.941479
220.208205	8020.736625	26.946496
220.373468	8035.481552	26.951514
220.545293	8039.326084	26.956532
220.726009	8051.685872	26.961549
221.124062	8061.012010	26.966567
221.786244	8077.977930	26.971584
222.187213	8084.164072	26.976602
222.550725	8081.469469	26.981620
222.547818	8081.785115	26.986637
222.990890	8111.803016	26.991655
223.180369	8106.111048	26.996672
223.294256	8113.629274	27.001690
223.606361	8110.127953	27.006708
223.653070	8114.603596	27.011725
223.470335	8136.629570	27.016743
224.216269	8147.471203	27.021760
224.448826	8153.617460	27.026778
224.145661	8155.785630	27.031796
224.581116	8157.204803	27.036813
224.752318	8167.098567	27.041831
225.159825	8164.027278	27.046848
225.518240	8192.325716	27.051866
225.513070	8198.937383	27.056884
225.728391	8202.206089	27.061901
225.705270	8227.413896	27.066919
225.987812	8216.456063	27.071936
225.961555	8235.901198	27.076954
226.125202	8253.420688	27.081972
226.492436	8263.898854	27.086989
226.772260	8290.517009	27.092007
227.027562	8298.850017	27.097024
227.270500	8312.215009	27.102042
227.580738	8325.892618	27.107060
227.893130	8326.746914	27.112077
227.579556	8354.872326	27.117095
228.023375	8364.981886	27.122112
227.951366	8381.735471	27.127130
227.915730	8398.821756	27.132148
228.526762	8417.813678	27.137165
228.644136	8435.985317	27.142183
228.838363	8455.927537	27.147200
228.685809	8467.903987	27.152218
229.176213	8473.391030	27.157236
229.802794	8497.826352	27.162253
229.871250	8514.601766	27.167271
230.285658	8516.708139	27.172288
230.598415	8547.606947	27.177306
230.542433	8563.018261	27.182324
231.229110	8573.836899	27.187341
230.919678	8585.799185	27.192359
231.406729	8597.332150	27.197376
231.737186	8612.569393	27.202394
231.793685	8608.908551	27.207412
232.087056	8637.639932	27.212429
232.210528	8657.410568	27.217447
232.577539	8678.443796	27.222464
232.932482	8685.580618	27.227482
232.918372	8708.924075	27.232500
233.931164	8692.137808	27.237517
234.116707	8715.370309	27.242535
234.503809	8726.999436	27.247552
234.325980	8725.324407	27.252570
234.489706	8734.135138	27.257588
235.042976	8748.275493	27.262605
234.791990	8766.947104	27.267623
234.957448	8770.584921	27.272640
235.465828	8786.146600	27.277658
235.565263	8794.545006	27.282676
235.883352	8796.351474	27.287693
235.886373	8823.692081	27.292711
236.214157	8833.751010	27.297728
236.771475	8847.184239	27.302746
237.090763	8853.231370	27.307764
237.481123	8863.441453	27.312781
237.530887	8879.865886	27.317799
237.734214	8872.015481	27.322816
238.090807	8894.196001	27.327834
237.732463	8913.332135	27.332852
238.353021	8919.220816	27.337869
238.311518	8941.370290	27.342887
238.075335	8950.989210	27.347904
238.893539	8963.642952	27.352922
238.838338	8988.064068	27.357940
239.067030	8994.363314	27.362957
239.328532	9013.725624	27.367975
239.339225	9024.343544	27.372992
239.427846	9049.449909	27.378010
239.585930	9072.871000	27.383028
240.283872	9096.633010	27.388045
240.208602	9122.463673	27.393063
240.547977	9132.182170	27.398080
241.347551	9152.368683	27.403098
241.441912	9167.824273	27.408116
242.258226	9186.234180	27.413133
242.292041	9187.950602	27.418151
242.452022	9201.173299	27.423168
243.102951	9210.784443	27.428186
243.701407	9207.173347	27.433204
243.788497	9208.153927	27.438221
243.967608	9204.502624	27.443239
244.110109	9202.149189	27.448256
244.667989	9220.189082	27.453274
244.530354	9233.757938	27.458292
244.893299	9229.766692	27.463309
244.836775	9229.102661	27.468327
245.084462	9230.534840	27.473344
245.321182	9247.308434	27.478362
245.274403	9263.428621	27.483380
245.558446	9271.914933	27.488397
245.522512	9283.075577	27.493415
245.489079	9303.192745	27.498432
245.641899	9316.435625	27.503450
245.752266	9346.201265	27.508468
246.086945	9360.821759	27.513485
246.509092	9383.448999	27.518503
246.818284	9397.493988	27.523520
246.814895	9390.252506	27.528538
246.979003	9425.272065	27.533556
247.408182	9434.380405	27.538573
247.385921	9463.063022	27.543591
247.630832	9492.925650	27.548608
248.192341	9495.289067	27.553626
248.135863	9529.927814	27.558644
249.052028	9543.689114	27.563661
249.248690	9567.629175	27.568679
249.255133	9588.194624	27.573696
249.516067	9593.782990	27.578714
249.714044	9617.644137	27.583732
250.227653	9622.804000	27.588749
250.518256	9645.265081	27.593767
251.216663	9648.956051	27.598784
251.645708	9656.053499	27.603802
251.859067	9672.545459	27.608820
252.190590	9676.033952	27.613837
252.767786	9679.828453	27.618855
252.583603	9689.981176	27.623872
252.851368	9703.074625	27.628890
252.980505	9710.145239	27.633908
253.152099	9698.778565	27.638925
253.417754	9716.345045	27.643943
253.422915	9736.304352	27.648960
254.007637	9747.822021	27.653978
254.014040	9761.119394	27.658996
254.080482	9769.491469	27.664013
254.675056	9784.887859	27.669031
254.622936	9806.228932	27.674048
254.765835	9817.945683	27.679066
254.921002	9841.032026	27.684084
255.606178	9860.653851	27.689101
255.640989	9873.931658	27.694119
255.714547	9905.622540	27.699136
255.963204	9903.059259	27.704154
256.078153	9922.390170	27.709172
256.198565	9945.235059	27.714189
256.561199	9958.643892	27.719207
256.705489	9988.969929	27.724224
257.266296	10010.609392	27.729242
257.869078	10009.445684	27.734260
258.652912	10007.081491	27.739277
259.315215	10015.174072	27.744295
259.597615	10030.011781	27.749312
260.231261	10019.065604	27.754330
260.506551	10021.414159	27.759348
260.656149	10017.252369	27.764365
260.828168	10020.232420	27.769383
260.819837	10028.765079	27.774400
260.542185	10003.646871	27.779418
260.739819	10016.576501	27.784436
260.774840	10016.470783	27.789453
261.087773	10027.436455	27.794471
261.175623	10046.401759	27.799488
261.756758	10062.760102	27.804506
261.711124	10083.831856	27.809524
261.234810	10086.592120	27.814541
261.673310	10107.449216	27.819559
261.797384	10142.918098	27.824576
261.979474	10153.905475	27.829594
262.149243	10185.154847	27.834612
262.357655	10200.558722	27.839629
262.862016	10228.395536	27.844647
262.582738	10264.696227	27.849664
263.095609	10278.046636	27.854682
263.435916	10302.042841	27.859700
263.519844	10331.413720	27.864717
264.198178	10361.140195	27.869735
264.101900	10381.818953	27.874752
264.676361	10400.656229	27.879770
264.912758	10424.657969	27.884788
265.344006	10453.649499	27.889805
265.649370	10469.405498	27.894823
265.609588	10504.875468	27.899840
265.865803	10510.006461	27.904858
266.418285	10539.845441	27.909876
266.704193	10555.125780	27.914893
267.225091	10575.457041	27.919911
267.651111	10591.027008	27.924928
267.646752	10619.993125	27.929946
268.409608	10636.418142	27.934964
268.580393	10659.446367	27.939981
269.153875	10659.714104	27.944999
269.095765	10681.200705	27.950016
269.415005	10684.230608	27.955034
269.819382	10704.553713	27.960052
269.929716	10715.913341	27.965069
270.233382	10724.056871	27.970087
270.305627	10754.882316	27.975104
270.482547	10758.099602	27.980122
270.803248	10785.055489	27.985140
270.662736	10803.270069	27.990157
271.344641	10817.432770	27.995175
271.133811	10848.168088	28.000192
271.506475	10866.191606	28.005210
271.749564	10885.487543	28.010228
272.103496	10921.058820	28.015245
273.039560	10929.098763	28.020263
273.529483	10951.772964	28.025280
273.587746	10955.659025	28.030298
274.327933	10954.839661	28.035316
274.356438	10972.898889	28.040333
274.851155	10981.301679	28.045351
275.384432	10992.160711	28.050368
276.012785	10981.038296	28.055386
276.689043	10980.842388	28.060404
276.578006	10979.571243	28.065421
276.955244	10976.341358	28.070439
276.815645	10977.866044	28.075456
276.845518	10984.927625	28.080474
277.117574	10977.238938	28.085492
277.342091	10996.320649	28.090509
277.570911	11011.113765	28.095527
277.429250	11017.038568	28.100544
277.629356	11033.584541	28.105562
278.011360	11047.997880	28.110580
277.774245	11069.780846	28.115597
278.044216	11085.014694	28.120615
278.168663	11109.422760	28.125632
278.534176	11125.557060	28.130650
279.200567	11140.964169	28.135668
279.029002	11170.840441	28.140685
279.536217	11193.795734	28.145703
279.494294	11218.482757	28.150720
279.736565	11242.224780	28.155738
280.092111	11256.573352	28.160756
279.895180	11286.632859	28.165773
280.677749	11299.732377	28.170791
280.645824	11329.032050	28.175808
280.852483	11358.286058	28.180826
281.607873	11377.512918	28.185844
281.725584	11401.612147	28.190861
281.695956	11419.464047	28.195879
282.083756	11437.221793	28.200896
282.574703	11456.792591	28.205914
282.666123	11477.380300	28.210932
282.967461	11499.287597	28.215949
283.384510	11523.094909	28.220967
284.587694	11528.120202	28.225984
284.946174	11535.808404	28.231002
285.645727	11543.404021	28.236020
285.596359	11564.388524	28.241037
285.936415	11554.414706	28.246055
286.060407	11578.884222	28.251072
286.337406	11586.042319	28.256090
286.813175	11592.609809	28.261108
286.612197	11613.810075	28.266125
287.351568	11618.778884	28.271143
287.385820	11633.234445	28.276160
287.424125	11650.155211	28.281178
288.000362	11653.678556	28.286196
287.730291	11685.531353	28.291213
288.212007	11700.307746	28.296231
288.330257	11720.094063	28.301248
288.493574	11743.951500	28.306266
288.955005	11754.723657	28.311284
289.065786	11787.419728	28.316301
289.325210	11794.119946	28.321319
289.630435	11832.151417	28.326336
289.626298	11851.540568	28.331354
290.147276	11880.788504	28.336372
290.021690	11914.934880	28.341389
290.676793	11947.836785	28.346407
290.768753	11964.426795	28.351424
290.900348	11990.770716	28.356442
291.669495	12013.449922	28.361460
292.107450	12049.922916	28.366477
292.151855	12071.629212	28.371495
292.370284	12089.448751	28.376512
292.622712	12113.132082	28.381530
293.185021	12141.612613	28.386548
293.269402	12174.469822	28.391565
293.654729	12190.917844	28.396583
294.240915	12208.408105	28.401600
294.426733	12231.016967	28.406618
295.022583	12250.126270	28.411636
295.198841	12279.888832	28.416653
295.436740	12285.109298	28.421671
295.908490	12302.271126	28.426688
296.025899	12329.396336	28.431706
296.604853	12343.195295	28.436724
297.743761	12362.876808	28.441741
297.729782	12363.071463	28.446759
298.179928	12360.061677	28.451776
298.221145	12366.836789	28.456794
298.678596	12390.374782	28.461812
298.654518	12401.407213	28.466829
298.768127	12415.168086	28.471847
299.229281	12437.559998	28.476864
299.049977	12449.169605	28.481882
299.371550	12466.603805	28.486900
299.544127	12474.857337	28.491917
299.774407	12490.037622	28.496935
299.656979	12516.275425	28.501952
299.752222	12538.738959	28.506970
300.365930	12560.784393	28.511988
300.672221	12596.915599	28.517005
301.319908	12622.949961	28.522023
301.562433	12627.552091	28.527040
301.857386	12659.188189	28.532058
302.403513	12662.188079	28.537076
302.342005	12690.403920	28.542093
302.609369	12702.957838	28.547111
303.133592	12728.309991	28.552128
303.547402	12744.355213	28.557146
304.042969	12757.025895	28.562164
303.730534	12778.435188	28.567181
303.961224	12806.711684	28.572199
304.579692	12832.409276	28.577216
304.541970	12860.287425	28.582234
304.911990	12874.786324	28.587252
304.960354	12900.701118	28.592269
305.391663	12928.812321	28.597287
305.760148	12949.464864	28.602304
305.927402	12990.657614	28.607322
306.515858	13019.122771	28.612340
306.732018	13042.005089	28.617357
307.535995	13044.543301	28.622375
308.226926	13047.498857	28.627392
309.006575	13065.868095	28.632410
309.458408	13073.737008	28.637428
309.692370	13091.011447	28.642445
309.956323	13084.524627	28.647463
310.381055	13093.291488	28.652480
310.497321	13094.752039	28.657498
311.204120	13089.622856	28.662516
311.397097	13109.066043	28.667533
311.735204	13123.165464	28.672551
312.050006	13114.237237	28.677568
312.040002	13116.057441	28.682586
312.351456	13121.128936	28.687604
312.408789	13136.327371	28.692621
312.715539	13148.846766	28.697639
313.017141	13171.715154	28.702656
312.875589	13194.005988	28.707674
313.303674	13201.530640	28.712692
314.053597	13216.200300	28.717709
313.789746	13236.655125	28.722727
314.301286	13256.096286	28.727744
314.334112	13291.212142	28.732762
314.663185	13304.344103	28.737780
314.855637	13333.834895	28.742797
315.105817	13358.111346	28.747815
315.453819	13374.445408	28.752832
315.712512	13405.589429	28.757850
315.809146	13431.380489	28.762868
316.111724	13461.707406	28.767885
316.142330	13492.856184	28.772903
316.774544	13523.940301	28.777920
316.915125	13546.268526	28.782938
317.525250	13573.525583	28.787956
317.555263	13592.821357	28.792973
317.753303	13639.037534	28.797991
318.266684	13655.706997	28.803008
318.290983	13695.138169	28.808026
318.769937	13712.007205	28.813044
319.720911	13746.961333	28.818061
319.982894	13776.638421	28.823079
320.375485	13791.106050	28.828096
320.558543	13820.176952	28.833114
320.841495	13845.184637	28.838132
321.366302	13862.091953	28.843149
320.949301	13883.754776	28.848167
321.574223	13909.019658	28.853184
321.936104	13932.720665	28.858202
322.412600	13949.186936	28.863220
322.783723	13974.829506	28.868237
323.094019	13995.076971	28.873255
323.604285	14013.624165	28.878272
323.945726	14038.652427	28.883290
324.320045	14049.892787	28.888308
325.236629	14056.341192	28.893325
324.978536	14083.350150	28.898343
325.376598	14082.851135	28.903360
325.617954	14118.608800	28.908378
325.809906	14118.591382	28.913396
326.152311	14146.629563	28.918413
326.659105	14173.321627	28.923431
327.174539	14177.997306	28.928448
327.093380	14206.646090	28.933466
327.558342	14222.118590	28.938484
327.834705	14259.359987	28.943501
327.662995	14272.488791	28.948519
327.985205	14295.104794	28.953536
327.750589	14342.968759	28.958554
328.290126	14373.302356	28.963572
328.663809	14403.056689	28.968589
328.853799	14439.813209	28.973607
329.018784	14466.631562	28.978624
329.143057	14513.688184	28.983642
329.451635	14550.586104	28.988660
330.574641	14584.512915	28.993677
331.292979	14619.103923	28.998695
332.070039	14640.289973	29.003712
332.486654	14664.952198	29.008730
332.966607	14674.634288	29.013748
333.085950	14687.078670	29.018765
333.465998	14707.845010	29.023783
334.177397	14718.853645	29.028800
334.303213	14732.652290	29.033818
334.690131	14750.347640	29.038836
334.968573	14768.836288	29.043853
334.827776	14796.652836	29.048871
335.542433	14802.414701	29.053888
335.682358	14821.301365	29.058906
336.199454	14845.182934	29.063924
336.750135	14863.458090	29.068941
336.915792	14880.663770	29.073959
337.322451	14892.052239	29.078976
337.939931	14893.297773	29.083994
338.133493	14902.978459	29.089012
338.472461	14910.119918	29.094029
338.456397	14948.541154	29.099047
338.911562	14959.458328	29.104064
339.015578	14990.668762	29.109082
339.361280	15010.568084	29.114100
339.385788	15032.793025	29.119117
339.671088	15056.208890	29.124135
339.911849	15084.932110	29.129152
340.010051	15106.459433	29.134170
340.826916	15120.328632	29.139188
341.140702	15152.880541	29.144205
341.356790	15167.974272	29.149223
341.983109	15205.273488	29.154240
342.491257	15235.410579	29.159258
342.344514	15266.169683	29.164276
342.936655	15265.022367	29.169293
343.339910	15299.447813	29.174311
343.690671	15321.581425	29.179328
343.752725	15357.705538	29.184346
344.214487	15376.506581	29.189364
344.341328	15395.140760	29.194381
344.569986	15412.560384	29.199399
344.843677	15433.491788	29.204416
345.371968	15461.183172	29.209434
345.314050	15490.957208	29.214452
346.040245	15512.151224	29.219469
346.136044	15545.297831	29.224487
346.691096	15572.307300	29.229504
347.031262	15595.836228	29.234522
347.292305	15630.517538	29.239540
347.752125	15649.725829	29.244557
348.038213	15678.666400	29.249575
348.578759	15700.879495	29.254592
348.782348	15728.550901	29.259610
349.267385	15744.633032	29.264628
350.055325	15753.930771	29.269645
350.179211	15790.442783	29.274663
350.642798	15803.636498	29.279680
351.155947	15821.457154	29.284698
351.212443	15855.167221	29.289716
351.793877	15868.059410	29.294733
351.946080	15902.166686	29.299751
352.043929	15916.588760	29.304768
352.607206	15938.820489	29.309786
352.924736	15971.155914	29.314804
353.579364	15991.142514	29.319821
353.662240	16022.194498	29.324839
353.997216	16046.594913	29.329856
354.439225	16079.425359	29.334874
354.482345	16096.734517	29.339892
354.943822	16109.955622	29.344909
355.455314	16149.119955	29.349927
355.770837	16169.200619	29.354944
356.592246	16206.599131	29.359962
356.712057	16227.610558	29.364980
357.137730	16239.285251	29.369997
357.415352	16265.454367	29.375015
357.564476	16293.074256	29.380032
357.896886	16298.415950	29.385050
357.917037	16340.005540	29.390068
358.362728	16375.884118	29.395085
358.854140	16421.574272	29.400103
358.928287	16448.954634	29.405120
359.639749	16463.226962	29.410138
359.990358	16499.994676	29.415156
361.102808	16504.638606	29.420173
361.444196	16538.162739	29.425191
361.961193	16546.697153	29.430208
362.743016	16558.341609	29.435226
363.674291	16563.905985	29.440244
364.149078	16562.420200	29.445261
364.329298	16573.550945	29.450279
364.258768	16571.403440	29.455296
364.581049	16572.658479	29.460314
364.870202	16594.770894	29.465332
365.139605	16602.162582	29.470349
365.506992	16606.193581	29.475367
365.759876	16628.729703	29.480384
366.022205	16628.664412	29.485402
365.724919	16658.201136	29.490420
366.213280	16675.383764	29.495437
366.297287	16709.516592	29.500455
366.278929	16743.442592	29.505472
366.906407	16772.757405	29.510490
366.944685	16794.219613	29.515508
367.111015	16808.859697	29.520525
367.398792	16843.269638	29.525543
367.560459	16876.455337	29.530560
368.016829	16917.881334	29.535578
368.242711	16957.099507	29.540596
368.621449	16992.735159	29.545613
368.829471	17037.967900	29.550631
369.428257	17063.891366	29.555648
370.035216	17101.354142	29.560666
369.849515	17138.486132	29.565684
370.344259	17174.080946	29.570701
370.911822	17211.284108	29.575719
371.695174	17241.407799	29.580736
372.003351	17265.330570	29.585754
372.741686	17293.827303	29.590772
373.215145	17316.718821	29.595789
373.805353	17352.794748	29.600807
373.935630	17372.001181	29.605824
374.221491	17402.636073	29.610842
374.392605	17426.624277	29.615860
375.248674	17454.389403	29.620877
375.409963	17485.292490	29.625895
375.963177	17518.112170	29.630912
376.103048	17536.819132	29.635930
376.326203	17571.577000	29.640948
376.419073	17594.203925	29.645965
377.086390	17633.382308	29.650983
377.234981	17666.623772	29.656000
377.840691	17698.051224	29.661018
377.957307	17736.687188	29.666036
378.350094	17778.819389	29.671053
378.884800	17824.071248	29.676071
379.124633	17859.717535	29.681088
379.498243	17887.536296	29.686106
380.143434	17928.366198	29.691124
380.263752	17945.767001	29.696141
380.620373	17985.936984	29.701159
380.900744	18013.109338	29.706176
381.588968	18051.574374	29.711194
382.040971	18090.431603	29.716212
382.712156	18118.523151	29.721229
383.387842	18150.163734	29.726247
383.697215	18179.167910	29.731264
383.962793	18203.565651	29.736282
384.256899	18240.554649	29.741300
384.565345	18273.039538	29.746317
384.660084	18300.977571	29.751335
384.951024	18339.893518	29.756352
385.498427	18373.756201	29.761370
385.693884	18412.867789	29.766388
386.170518	18447.434301	29.771405
386.545467	18468.466335	29.776423
386.953528	18513.804055	29.781440
387.704338	18531.478054	29.786458
388.389471	18577.701768	29.791476
388.743203	18596.123968	29.796493
389.300417	18624.071269	29.801511
389.085168	18658.103079	29.806528
390.277997	18665.333694	29.811546
391.143399	18689.294159	29.816564
391.511407	18714.482803	29.821581
392.223947	18717.451623	29.826599
392.330093	18742.306829	29.831616
392.509679	18751.257532	29.836634
392.683410	18769.715967	29.841652
392.723797	18797.244515	29.846669
392.972983	18814.607604	29.851687
393.155871	18843.912847	29.856704
393.362566	18865.055149	29.861722
393.799694	18910.713877	29.866740
394.059672	18933.097493	29.871757
394.019349	18965.538891	29.876775
394.820837	19006.471743	29.881792
395.116631	19028.494895	29.886810
395.231255	19058.847450	29.891828
396.090161	19078.498254	29.896845
396.603973	19113.876563	29.901863
397.504901	19125.687609	29.906880
398.161871	19151.970460	29.911898
398.708722	19180.519427	29.916916
398.875091	19212.695440	29.921933
398.924673	19219.278113	29.926951
399.088342	19243.106238	29.931968
399.613073	19269.609743	29.936986
399.644513	19303.841731	29.942004
399.948817	19343.605911	29.947021
400.361038	19363.556264	29.952039
400.483772	19400.766901	29.957056
401.568184	19433.797417	29.962074
401.634685	19469.450576	29.967092
401.848913	19499.610927	29.972109
402.927507	19528.075805	29.977127
403.269230	19560.117905	29.982144
403.770072	19586.633744	29.987162
404.005028	19612.506240	29.992180
404.500908	19626.449634	29.997197
404.866790	19667.504944	30.002215
405.042061	19695.135656	30.007232
405.735246	19713.326467	30.012250
405.905747	19748.504310	30.017268
406.135876	19783.450102	30.022285
406.779493	19824.117838	30.027303
407.355323	19853.780854	30.032320
407.425514	19877.149250	30.037338
407.846666	19922.832313	30.042356
408.035595	19957.845181	30.047373
408.726812	19992.593860	30.052391
408.844717	20032.507133	30.057408
409.523043	20071.960614	30.062426
410.560217	20091.329369	30.067444
410.903056	20115.644642	30.072461
411.438712	20137.457809	30.077479
411.420534	20182.916210	30.082496
411.778215	20194.157230	30.087514
412.545086	20221.803016	30.092532
412.743531	20245.278434	30.097549
413.313341	20267.827064	30.102567
413.250837	20315.370919	30.107584
413.749545	20343.255110	30.112602
414.156212	20373.110948	30.117620
414.790760	20407.951831	30.122637
415.332023	20434.528557	30.127655
415.460144	20471.731234	30.132672
415.847740	20506.723471	30.137690
416.338855	20533.204590	30.142708
416.754141	20578.083258	30.147725
417.034795	20598.865565	30.152743
417.106871	20645.863157	30.157760
417.622697	20670.957828	30.162778
418.158100	20708.979745	30.167796
418.263840	20759.043114	30.172813
418.966419	20784.778697	30.177831
419.639775	20819.707044	30.182848
420.151952	20851.299387	30.187866
420.747880	20879.136884	30.192884
421.268599	20917.730823	30.197901
422.084325	20920.552159	30.202919
422.905985	20939.430949	30.207936
423.466407	20947.069745	30.212954
423.697306	20947.870422	30.217972
423.939413	20958.487830	30.222989
423.881535	20984.185382	30.228007
424.081871	21010.079951	30.233024
424.296489	21036.030534	30.238042
424.506391	21058.278660	30.243060
424.415075	21101.780973	30.248077
425.201499	21137.378677	30.253095
425.502163	21173.326287	30.258112
426.168375	21202.530611	30.263130
426.405613	21245.096157	30.268148
426.237578	21297.646857	30.273165
427.071483	21315.073621	30.278183
427.598584	21363.968757	30.283200
427.735885	21396.850620	30.288218
428.355129	21445.711855	30.293236
428.204331	21482.989652	30.298253
428.695145	21536.305686	30.303271
429.250722	21588.961640	30.308288
429.967356	21621.071890	30.313306
430.722944	21658.769502	30.318324
431.180660	21702.587859	30.323341
431.635146	21746.197177	30.328359
431.980809	21782.736190	30.333376
432.107191	21822.756382	30.338394
433.035597	21862.782928	30.343412
433.484385	21893.659316	30.348429
434.097149	21920.150915	30.353447
434.547903	21957.145931	30.358464
435.287784	21991.397249	30.363482
435.652792	22024.638457	30.368500
436.219017	22055.774807	30.373517
436.271210	22084.421490	30.378535
436.873657	22117.787631	30.383552
437.351408	22150.739284	30.388570
437.461975	22182.985410	30.393588
437.485654	22231.067544	30.398605
438.286621	22268.978185	30.403623
438.614089	22306.945052	30.408640
439.014519	22347.465167	30.413658
439.672081	22385.555847	30.418676
439.763077	22426.401605	30.423693
440.792516	22453.798018	30.428711
441.082932	22499.735166	30.433728
441.153507	22532.439492	30.438746
442.189972	22560.370987	30.443764
442.525263	22603.726300	30.448781
443.205782	22633.856264	30.453799
442.868951	22671.741330	30.458816
443.525854	22724.095568	30.463834
443.975613	22762.002266	30.468852
444.246098	22805.125990	30.473869
444.689360	22842.988219	30.478887
445.226011	22893.937511	30.483904
445.653368	22934.366293	30.488922
446.305708	22968.925754	30.493940
446.489338	23024.007973	30.498957
447.240512	23070.108648	30.503975
447.212060	23109.760136	30.508992
447.672623	23141.682236	30.514010
448.677563	23176.123962	30.519028
448.815767	23213.092950	30.524045
449.370006	23249.700024	30.529063
449.869486	23297.807510	30.534080
450.184475	23343.074354	30.539098
450.982781	23376.021178	30.544116
450.798013	23407.150054	30.549133
451.572415	23449.039576	30.554151
451.851246	23483.527764	30.559168
452.043103	23523.284160	30.564186
452.993240	23551.781852	30.569204
453.373303	23593.705336	30.574221
454.328668	23615.411130	30.579239
454.738687	23650.081391	30.584256
455.245799	23682.502967	30.589274
455.709432	23705.341813	30.594292
455.595924	23738.097798	30.599309
456.181385	23783.593926	30.604327
456.283814	23817.184781	30.609344
456.796934	23859.496910	30.614362
457.341352	23896.668345	30.619380
457.567231	23933.387902	30.624397
458.240571	23977.365767	30.629415
458.581615	24022.589125	30.634432
458.867460	24063.061324	30.639450
459.864005	24101.716417	30.644468
459.950605	24145.255518	30.649485
460.669673	24187.291616	30.654503
461.520805	24209.519976	30.659520
462.070212	24246.177308	30.664538
462.893509	24271.024732	30.669556
463.234886	24317.674278	30.674573
463.825612	24341.355518	30.679591
464.114547	24369.823471	30.684608
464.636826	24401.327774	30.689626
465.533075	24419.048646	30.694644
465.884833	24458.913277	30.699661
465.940230	24488.629449	30.704679
466.256123	24531.300663	30.709696
466.551755	24556.489540	30.714714
467.466537	24593.213418	30.719732
467.349745	24635.084359	30.724749
468.223350	24657.301713	30.729767
468.820057	24693.327759	30.734784
469.101246	24731.312439	30.739802
469.875510	24756.313747	30.744820
470.419458	24808.147488	30.749837
470.844878	24820.026940	30.754855
471.211010	24861.265182	30.759872
471.186690	24900.399794	30.764890
472.073667	24919.780035	30.769908
472.215805	24957.045472	30.774925
472.995094	24997.592925	30.779943
472.930513	25039.011547	30.784960
473.376188	25081.320515	30.789978
474.128407	25123.481184	30.794996
474.744770	25158.800090	30.800013
474.920186	25198.623043	30.805031
475.514272	25236.424705	30.810048
475.535251	25286.064478	30.815066
476.304700	25322.239938	30.820084
476.557301	25371.169927	30.825101
476.647529	25400.454585	30.830119
477.538923	25447.333338	30.835136
477.659013	25505.089661	30.840154
478.293858	25547.849507	30.845172
478.730706	25597.173909	30.850189
479.375170	25650.258324	30.855207
479.811706	25709.473794	30.860224
479.967838	25760.015142	30.865242
480.739267	25804.711666	30.870260
480.905936	25862.745357	30.875277
481.466429	25907.442299	30.880295
481.995890	25959.269312	30.885312
482.293290	25998.578805	30.890330
483.355997	26027.205574	30.895348
484.201027	26061.577076	30.900365
484.778380	26097.500473	30.905383
485.108472	26124.942662	30.910400
485.608782	26165.427006	30.915418
486.596269	26189.496308	30.920436
486.933902	26221.794596	30.925453
487.294581	26241.835736	30.930471
488.029747	26278.499876	30.935488
487.983291	26310.483289	30.940506
488.657875	26362.189777	30.945524
489.343190	26379.130644	30.950541
490.083974	26389.265376	30.955559
490.937136	26417.911645	30.960576
491.131968	26449.249882	30.965594
491.729728	26480.143134	30.970612
492.015818	26520.660548	30.975629
492.096384	26552.472035	30.980647
492.769112	26584.198386	30.985664
493.136243	26617.303148	30.990682
493.309917	26653.256543	30.995700
493.546527	26694.066408	31.000717
493.887807	26736.341518	31.005735
494.724680	26779.484263	31.010752
494.993243	26812.895863	31.015770
495.860378	26873.709613	31.020788
496.309680	26909.507621	31.025805
497.022897	26956.033560	31.030823
497.297204	26989.684271	31.035840
497.747989	27041.114356	31.040858
497.774332	27094.128711	31.045876
498.352500	27141.339837	31.050893
498.738009	27195.610477	31.055911
499.151277	27238.143036	31.060928
499.327474	27293.265497	31.065946
499.816761	27352.276054	31.070964
500.054066	27421.412548	31.075981
500.064381	27482.275349	31.080999
501.141923	27537.596678	31.086016
501.769148	27600.026603	31.091034
502.857863	27649.447951	31.096052
503.445505	27715.528032	31.101069
503.916866	27768.048275	31.106087
504.976243	27815.503505	31.111104
505.088154	27876.915538	31.116122
505.869889	27913.525010	31.121140
506.069728	27950.394700	31.126157
506.437129	27998.778552	31.131175
507.093958	28043.515610	31.136192
507.479491	28107.040846	31.141210
507.916197	28153.836499	31.146228
508.914891	28204.384651	31.151245
508.906868	28245.796923	31.156263
509.699316	28306.423034	31.161280
510.147279	28356.759775	31.166298
510.935620	28408.614498	31.171316
512.029968	28437.946665	31.176333
512.315617	28489.884664	31.181351
513.053438	28512.809249	31.186368
513.602359	28557.341497	31.191386
514.055145	28579.480477	31.196404
514.060016	28621.307905	31.201421
514.266916	28677.499071	31.206439
514.975818	28714.888811	31.211456
515.244934	28774.968954	31.216474
515.393554	28823.388093	31.221492
515.860892	28878.070050	31.226509
516.183713	28934.504726	31.231527
517.026315	28991.812709	31.236544
516.961947	29045.661894	31.241562
517.420720	29096.090479	31.246580
518.157649	29154.558400	31.251597
518.438501	29217.612885	31.256615
519.406384	29268.024125	31.261632
519.481730	29336.021511	31.266650
520.006404	29384.288616	31.271668
520.674352	29438.283044	31.276685
521.324542	29506.419589	31.281703
522.341615	29545.211345	31.286720
522.745873	29615.859015	31.291738
523.362165	29652.215578	31.296756
524.462602	29692.722643	31.301773
524.948828	29732.394319	31.306791
525.730938	29770.821593	31.311808
526.091236	29818.549214	31.316826
526.767852	29852.107494	31.321844
527.094000	29899.228968	31.326861
527.615589	29942.794485	31.331879
527.959330	29991.992252	31.336896
528.411600	30040.194269	31.341914
528.676101	30089.588373	31.346932
529.377603	30128.073917	31.351949
529.832555	30195.522972	31.356967
530.265752	30244.063107	31.361984
530.886629	30306.876088	31.367002
531.464694	30346.612863	31.372020
532.330770	30399.924512	31.377037
532.931882	30441.619973	31.382055
534.155026	30464.224064	31.387072
534.709186	30505.081947	31.392090
535.222686	30553.120683	31.397108
535.767727	30586.891402	31.402125
536.040646	30633.925852	31.407143
536.557129	30658.296889	31.412160
537.104397	30705.620630	31.417178
537.473530	30747.027034	31.422196
538.079487	30785.561361	31.427213
538.230106	30841.844521	31.432231
538.508641	30886.124525	31.437248
539.314907	30939.132214	31.442266
539.914851	30988.385118	31.447284
540.489170	31042.945780	31.452301
540.620539	31083.546737	31.457319
541.118729	31125.920208	31.462336
541.767955	31192.296744	31.467354
541.920150	31262.800259	31.472372
542.923987	31314.025460	31.477389
543.117294	31369.489286	31.482407
543.737981	31421.336513	31.487424
544.334943	31473.377110	31.492442
545.566277	31510.841164	31.497460
547.301455	31538.845448	31.502477
548.099492	31567.515672	31.507495
548.648094	31587.658164	31.512512
548.934035	31611.327186	31.517530
549.095839	31658.344879	31.522548
549.774169	31682.113246	31.527565
549.646705	31728.270260	31.532583
550.079466	31771.489024	31.537600
550.462416	31824.253809	31.542618
550.674039	31867.626071	31.547636
551.236107	31914.471067	31.552653
551.739222	31973.059617	31.557671
551.742481	32018.138851	31.562688
552.554866	32075.547144	31.567706
552.682956	32133.106509	31.572724
553.441689	32182.099907	31.577741
554.415829	32226.230540	31.582759
555.547000	32258.011451	31.587776
556.272955	32292.992386	31.592794
556.408853	32350.380795	31.597812
556.721784	32380.590146	31.602829
557.051818	32418.731917	31.607847
557.640135	32475.168877	31.612864
558.352784	32522.662670	31.617882
559.200465	32556.977217	31.622900
560.274920	32595.081608	31.627917
560.448389	32650.306645	31.632935
560.860112	32694.957299	31.637952
561.224596	32742.695348	31.642970
561.864187	32790.915008	31.647988
562.434230	32832.602357	31.653005
562.947285	32876.826556	31.658023
563.033768	32920.013832	31.663040
563.594973	32986.594686	31.668058
563.964380	33044.445312	31.673076
564.814862	33109.842958	31.678093
565.223672	33171.057320	31.683111
565.543674	33229.535147	31.688128
566.248642	33277.227870	31.693146
566.751012	33330.157289	31.698164
567.464444	33394.089317	31.703181
568.078661	33462.594264	31.708199
568.656290	33530.181002	31.713216
569.362954	33586.021382	31.718234
569.800781	33640.009966	31.723252
570.621797	33698.056345	31.728269
570.890992	33761.529813	31.733287
571.538442	33824.404617	31.738304
572.765280	33883.208134	31.743322
572.955661	33947.159129	31.748340
573.774781	33996.128658	31.753357
574.449494	34039.268839	31.758375
574.995297	34084.705491	31.763392
575.985634	34129.403038	31.768410
576.192634	34185.264723	31.773428
577.294895	34233.143686	31.778445
578.169235	34287.731106	31.783463
578.435966	34331.807139	31.788480
579.030314	34376.677999	31.793498
579.412990	34421.028565	31.798516
579.836697	34467.237372	31.803533
580.258863	34527.917775	31.808551
580.506720	34582.076287	31.813568
581.059653	34637.339505	31.818586
581.288829	34706.872134	31.823604
581.716007	34762.200688	31.828621
582.205367	34826.616665	31.833639
582.532747	34896.165368	31.838656
583.036402	34968.944963	31.843674
583.474134	35050.120210	31.848692
584.204351	35126.261625	31.853709
585.011277	35193.479165	31.858727
585.511328	35262.309690	31.863744
586.585758	35321.641738	31.868762
586.544848	35393.257050	31.873780
587.432028	35450.982659	31.878797
588.233050	35537.389049	31.883815
588.543403	35602.421195	31.888832
589.660401	35660.036942	31.893850
590.163912	35740.415530	31.898868
590.564859	35804.231111	31.903885
591.356041	35866.931600	31.908903
592.292469	35923.530309	31.913920
592.778096	35970.184055	31.918938
593.382825	36032.142753	31.923956
593.631364	36091.531713	31.928973
593.998582	36147.865381	31.933991
594.378750	36208.530026	31.939008
595.068291	36276.443215	31.944026
595.314586	36340.033780	31.949044
596.346064	36412.810970	31.954061
597.012471	36466.609411	31.959079
597.432325	36536.935026	31.964096
598.533078	36593.234150	31.969114
598.856780	36665.220366	31.974132
599.652750	36726.638621	31.979149
599.951710	36783.900772	31.984167
600.418906	36863.147944	31.989184
601.658939	36904.219759	31.994202
602.181265	36978.348866	31.999220
602.773390	37035.989454	32.004237
603.549901	37109.676314	32.009255
603.867203	37178.282431	32.014272
604.559966	37238.504425	32.019290
605.131687	37292.901683	32.024308
605.662066	37348.940750	32.029325
606.427566	37412.345204	32.034343
607.524745	37478.147347	32.039360
608.174916	37525.159837	32.044378
608.585615	37593.117742	32.049396
609.351083	37646.054370	32.054413
610.127360	37702.580989	32.059431
610.811482	37759.650073	32.064448
611.758045	37807.936752	32.069466
611.829808	37864.059476	32.074484
612.467277	37919.006395	32.079501
612.971615	37969.345430	32.084519
613.189825	38035.774507	32.089536
614.016992	38091.877330	32.094554
614.345393	38175.641236	32.099572
614.713342	38244.839554	32.104589
615.713941	38310.780620	32.109607
616.028399	38388.528965	32.114624
616.686263	38448.372547	32.119642
617.427704	38528.831597	32.124660
617.774276	38593.859094	32.129677
618.749451	38661.462660	32.134695
619.506873	38737.845283	32.139712
620.255173	38786.214666	32.144730
620.774570	38846.514841	32.149748
621.168064	38903.064243	32.154765
622.407385	38971.973079	32.159783
623.101840	39022.731837	32.164800
624.070958	39075.446482	32.169818
625.215435	39128.066036	32.174836
626.000214	39170.234547	32.179853
626.710247	39222.648369	32.184871
626.573018	39276.663664	32.189888
627.251534	39326.526343	32.194906
627.788736	39382.725243	32.199924
628.065753	39441.700715	32.204941
628.889826	39503.250025	32.209959
628.908104	39560.892428	32.214976
629.409175	39624.569250	32.219994
630.073456	39696.498648	32.225012
631.226376	39748.531511	32.230029
632.087713	39802.676994	32.235047
632.385594	39859.440861	32.240064
633.482382	39911.896958	32.245082
633.532709	39960.271108	32.250100
633.935662	40022.983864	32.255117
634.438031	40071.144766	32.260135
634.949469	40137.031211	32.265152
635.544948	40202.080164	32.270170
636.362863	40264.715748	32.275188
636.918662	40331.757171	32.280205
637.207524	40386.548173	32.285223
637.494685	40451.582646	32.290240
638.237032	40525.872994	32.295258
638.788941	40592.909703	32.300276
639.747477	40660.207788	32.305293
640.986225	40715.673083	32.310311
641.662948	40795.341590	32.315328
642.149220	40855.151979	32.320346
642.718752	40918.989310	32.325364
643.180875	40984.088321	32.330381
643.680155	41061.094666	32.335399
644.276595	41125.218683	32.340416
644.561670	41193.595895	32.345434
645.543923	41268.301040	32.350452
646.006399	41358.276118	32.355469
646.891195	41424.601138	32.360487
647.416984	41500.275967	32.365504
648.853461	41547.907675	32.370522
649.507255	41614.612462	32.375540
650.058064	41686.413741	32.380557
650.719119	41752.827407	32.385575
651.587532	41818.938741	32.390592
652.388344	41885.733875	32.395610
653.042872	41945.119113	32.400628
653.400322	42019.352803	32.405645
654.510294	42067.071353	32.410663
654.659607	42139.594171	32.415680
655.127668	42206.934737	32.420698
655.880853	42279.311022	32.425716
656.261191	42363.442267	32.430733
656.880946	42418.512997	32.435751
658.104396	42484.741716	32.440768
658.809739	42552.154846	32.445786
659.220093	42611.424710	32.450804
659.989165	42677.811243	32.455821
660.995336	42747.893532	32.460839
661.362300	42819.881120	32.465856
661.655712	42889.257688	32.470874
662.226491	42962.658066	32.475892
662.593495	43047.211348	32.480909
663.070244	43126.506243	32.485927
663.564049	43223.411736	32.490944
664.099527	43301.908424	32.495962
664.505107	43392.556322	32.500980
665.319967	43489.927942	32.505997
665.883196	43568.878954	32.511015
666.506872	43667.432260	32.516032
667.051879	43764.894088	32.521050
667.827861	43852.979461	32.526068
669.113701	43940.788464	32.531085
670.793117	43997.485310	32.536103
671.506936	44080.899958	32.541120
672.833534	44125.850782	32.546138
673.648380	44184.809455	32.551156
673.863525	44259.227167	32.556173
674.565253	44311.618989	32.561191
675.207822	44383.358747	32.566208
675.492160	44440.647267	32.571226
676.184455	44508.142279	32.576244
676.663938	44577.131335	32.581261
677.376283	44641.254721	32.586279
677.630293	44722.613862	32.591296
678.259985	44795.512899	32.596314
679.072587	44861.271751	32.601332
679.669608	44942.461540	32.606349
680.498474	44999.406104	32.611367
680.881981	45068.131822	32.616384
681.501012	45136.275832	32.621402
682.219728	45205.957053	32.626420
682.810447	45288.567044	32.631437
683.581428	45358.151793	32.636455
684.142686	45433.325313	32.641472
684.857010	45513.835155	32.646490
685.118461	45591.771046	32.651508
686.012252	45678.999395	32.656525
686.353871	45760.730631	32.661543
686.909914	45851.968703	32.666560
687.429853	45939.439979	32.671578
688.240350	46030.510597	32.676596
688.856233	46120.404466	32.681613
689.683689	46214.709637	32.686631
690.154731	46300.870819	32.691648
691.116729	46401.274043	32.696666
691.764399	46487.602680	32.701684
692.306783	46594.615589	32.706701
693.070441	46671.216292	32.711719
694.071432	46767.052277	32.716736
694.701820	46853.060207	32.721754
695.581768	46942.178660	32.726772
696.450257	47034.125545	32.731789
697.405942	47119.550480	32.736807
698.294398	47212.578025	32.741824
699.466650	47280.180582	32.746842
700.332218	47358.052437	32.751860
700.621310	47446.241427	32.756877
701.482717	47510.296315	32.761895
701.795514	47599.483113	32.766912
702.330566	47686.985262	32.771930
703.253359	47771.332299	32.776948
703.555916	47848.238129	32.781965
704.296576	47940.914727	32.786983
705.036877	48017.524748	32.792000
705.800060	48109.961615	32.797018
706.615057	48206.669289	32.802036
707.412867	48288.358236	32.807053
707.848131	48374.329516	32.812071
708.657430	48472.495276	32.817088
709.057212	48570.527064	32.822106
710.032555	48656.328322	32.827124
710.294634	48755.119603	32.832141
711.272294	48845.092997	32.837159
712.267595	48919.371854	32.842176
712.654759	49017.202756	32.847194
713.626124	49103.155113	32.852212
714.312736	49197.902635	32.857229
715.068689	49276.918410	32.862247
716.377537	49359.708674	32.867264
717.137469	49447.892355	32.872282
718.099883	49516.447065	32.877300
718.531088	49594.554569	32.882317
719.386570	49667.899372	32.887335
720.593812	49744.571876	32.892352
721.047357	49826.074779	32.897370
721.870417	49896.469796	32.902388
722.410641	49977.845338	32.907405
723.102042	50050.056500	32.912423
723.836111	50129.218375	32.917440
724.276369	50216.965716	32.922458
724.991852	50279.869705	32.927476
725.656288	50365.148881	32.932493
726.299851	50435.875555	32.937511
727.134979	50512.637855	32.942528
728.584349	50561.335781	32.947546
729.649837	50605.669335	32.952564
730.358330	50680.160318	32.957581
730.833505	50722.864048	32.962599
731.374735	50793.975304	32.967616
731.690458	50870.363698	32.972634
732.543224	50940.422865	32.977652
732.820903	51025.873068	32.982669
733.235600	51098.534979	32.987687
734.175372	51170.065038	32.992704
734.712458	51253.066742	32.997722
735.284814	51329.139797	33.002740
735.762237	51423.437000	33.007757
736.503938	51513.821962	33.012775
737.607026	51591.084407	33.017792
738.120137	51688.696521	33.022810
739.563067	51772.236253	33.027828
739.856895	51860.890163	33.032845
740.721870	51943.524843	33.037863
741.765004	52000.117077	33.042880
742.826879	52082.505059	33.047898
743.721036	52146.841720	33.052916
744.739767	52222.377123	33.057933
745.836591	52290.679496	33.062951
747.349066	52359.096668	33.067968
747.813903	52416.265721	33.072986
748.444870	52474.892036	33.078004
749.087636	52550.168631	33.083021
749.760992	52612.344929	33.088039
750.065034	52674.367629	33.093056
750.260683	52756.137143	33.098074
750.951080	52834.218144	33.103092
751.376572	52929.279856	33.108109
751.666611	53012.045626	33.113127
752.426177	53099.295337	33.118144
752.829411	53206.832528	33.123162
753.658220	53294.027456	33.128180
755.088170	53375.873716	33.133197
756.254669	53461.472176	33.138215
757.268936	53544.537569	33.143232
757.440125	53642.285469	33.148250
758.399774	53722.284006	33.153268
759.221117	53822.755710	33.158285
759.369979	53899.673214	33.163303
760.284311	53994.804706	33.168320
760.602765	54093.048590	33.173338
761.272997	54187.848590	33.178356
762.101438	54296.452439	33.183373
762.365710	54408.542697	33.188391
763.382043	54508.840421	33.193408
763.578675	54617.923136	33.198426
764.360815	54723.011644	33.203444
764.952436	54849.031819	33.208461
765.776942	54969.385050	33.213479
766.949890	55073.311576	33.218496
767.479932	55194.182343	33.223514
768.270296	55299.790658	33.228532
769.366068	55419.975495	33.233549
770.155029	55529.641495	33.238567
771.372139	55631.447108	33.243584
771.897034	55743.198671	33.248602
772.468886	55848.226830	33.253620
773.873557	55945.302329	33.258637
774.402579	56063.922982	33.263655
775.192486	56150.776907	33.268672
775.957236	56243.302937	33.273690
776.810420	56338.841306	33.278708
778.109323	56425.182738	33.283725
778.577566	56513.784713	33.288743
779.731818	56590.717319	33.293760
780.320884	56674.826588	33.298778
781.416800	56756.558894	33.303796
781.990651	56855.418881	33.308813
782.335003	56946.153647	33.313831
783.417334	57014.121071	33.318848
784.106131	57122.194892	33.323866
784.827104	57208.540399	33.328884
785.859887	57304.925750	33.333901
786.383153	57403.720999	33.338919
787.299263	57488.095649	33.343936
787.857464	57584.004672	33.348954
788.677056	57678.266015	33.353972
789.263914	57782.720624	33.358989
790.185226	57883.702038	33.364007
790.913857	57980.071381	33.369024
791.697998	58084.425487	33.374042
792.456505	58178.225362	33.379060
793.415832	58291.183344	33.384077
793.638043	58400.276366	33.389095
794.854125	58499.126937	33.394112
796.229699	58605.104893	33.399130
796.797839	58698.957609	33.404148
797.776896	58798.689249	33.409165
798.139560	58894.194518	33.414183
799.410966	58995.610326	33.419200
800.112874	59097.044858	33.424218
801.078714	59186.619239	33.429236
801.889371	59294.526728	33.434253
802.253787	59397.945906	33.439271
802.948017	59502.082120	33.444288
803.716749	59614.851547	33.449306
803.837243	59721.883146	33.454324
804.655472	59836.250785	33.459341
805.202040	59976.428683	33.464359
806.143134	60094.752494	33.469376
806.605933	60216.366344	33.474394
807.156682	60333.593203	33.479412
808.170820	60470.133042	33.484429
808.580430	60602.476207	33.489447
810.682440	60717.622740	33.494464
812.003226	60832.001519	33.499482
813.240262	60936.422064	33.504500
814.263885	61033.231343	33.509517
814.989190	61131.942076	33.514535
816.952171	61205.870716	33.519552
818.032926	61279.471309	33.524570
819.168705	61364.533834	33.529588
819.909546	61449.655612	33.534605
820.372957	61530.595459	33.539623
821.031600	61618.423849	33.544640
821.469751	61712.059262	33.549658
822.190107	61800.093130	33.554676
822.745909	61893.444507	33.559693
823.188795	61994.304359	33.564711
823.941312	62089.109392	33.569728
824.560966	62185.826554	33.574746
825.234422	62300.010817	33.579764
826.184789	62398.880156	33.584781
826.651578	62515.830122	33.589799
827.454047	62621.645726	33.594816
827.798734	62738.591849	33.599834
828.683168	62860.467943	33.604852
829.426006	62969.341647	33.609869
829.912532	63094.622050	33.614887
830.514278	63202.521653	33.619904
831.656253	63327.752138	33.624922
832.471770	63437.507534	33.629940
833.156696	63550.040886	33.634957
833.835394	63673.295769	33.639975
835.134558	63780.122508	33.644992
836.185171	63896.231792	33.650010
836.962882	64010.054421	33.655028
837.909263	64116.195308	33.660045
838.768371	64219.765924	33.665063
840.290538	64322.045570	33.670080
841.473338	64411.758890	33.675098
843.278721	64481.730637	33.680116
844.985360	64545.258910	33.685133
846.066096	64624.143251	33.690151
847.033498	64693.881152	33.695168
847.794067	64762.913883	33.700186
848.851285	64823.566727	33.705204
849.609171	64887.082047	33.710221
850.305818	64953.509052	33.715239
850.680133	65019.256245	33.720256
850.702003	65113.152930	33.725274
851.372171	65200.836754	33.730292
852.351587	65279.929970	33.735309
852.447027	65390.623793	33.740327
853.287109	65494.197632	33.745344
853.830613	65587.491992	33.750362
854.812888	65695.544107	33.755380
855.463105	65810.605091	33.760397
855.926012	65941.102846	33.765415
856.316902	66050.531377	33.770432
857.113465	66177.214279	33.775450
857.430164	66305.816741	33.780468
858.240621	66437.208445	33.785485
858.879599	66580.039736	33.790503
859.478405	66727.923291	33.795520
860.429169	66873.221114	33.800538
861.069752	67017.793594	33.805556
862.233339	67159.733050	33.810573
862.748628	67321.580388	33.815591
863.584817	67466.332291	33.820608
864.456422	67620.290339	33.825626
865.618325	67775.857933	33.830644
866.354257	67928.108433	33.835661
867.017159	68085.613059	33.840679
867.940314	68231.392695	33.845696
869.142655	68368.440653	33.850714
870.549299	68531.528366	33.855732
871.695244	68659.685928	33.860749
872.228249	68804.983926	33.865767
873.679329	68947.975435	33.870784
874.831391	69078.897378	33.875802
875.478955	69214.114131	33.880820
876.731522	69332.578633	33.885837
877.721494	69465.350588	33.890855
878.580835	69580.435675	33.895872
879.699927	69720.578892	33.900890
880.127080	69857.069038	33.905908
881.493639	69986.513317	33.910925
882.407974	70124.201906	33.915943
883.138065	70229.929063	33.920960
884.340214	70347.617235	33.925978
884.989454	70462.444631	33.930996
886.243526	70597.785039	33.936013
886.745462	70716.178884	33.941031
887.405375	70839.327379	33.946048
888.311365	70962.682547	33.951066
888.964005	71092.542292	33.956084
889.841047	71217.060807	33.961101
890.497741	71344.948652	33.966119
891.287233	71468.876082	33.971136
892.157993	71600.214103	33.976154
892.767590	71723.970374	33.981172
893.930791	71857.436840	33.986189
894.744116	71990.234739	33.991207
895.500413	72126.419482	33.996224
896.403681	72248.056269	34.001242
896.756839	72395.956748	34.006260
898.269035	72523.179210	34.011277
898.942101	72653.196798	34.016295
899.556679	72789.288996	34.021312
900.976467	72926.501149	34.026330
901.961965	73072.221445	34.031348
902.696738	73209.719240	34.036365
903.417825	73360.120300	34.041383
904.517826	73503.560755	34.046400
905.494166	73630.075126	34.051418
905.963823	73778.927045	34.056436
907.415943	73913.800359	34.061453
908.668069	74059.255629	34.066471
910.535459	74170.853650	34.071488
913.093786	74260.843364	34.076506
914.102261	74360.511938	34.081524
915.448446	74442.892547	34.086541
916.072502	74540.412050	34.091559
916.621660	74654.140043	34.096576
917.530642	74741.393866	34.101594
917.864835	74854.759987	34.106612
918.791577	74963.595695	34.111629
919.737983	75078.006551	34.116647
920.222917	75196.105278	34.121664
921.191696	75287.032057	34.126682
921.795883	75397.093154	34.131700
922.668381	75516.792886	34.136717
923.449361	75642.042108	34.141735
923.944092	75773.796415	34.146752
925.198448	75880.400719	34.151770
925.996060	76026.551305	34.156788
926.905885	76137.255016	34.161805
927.644986	76277.029287	34.166823
928.116340	76417.987062	34.171840
929.144218	76548.253957	34.176858
929.881933	76704.867053	34.181876
930.596112	76838.103083	34.186893
931.593642	76977.415387	34.191911
932.464220	77124.275906	34.196928
933.109900	77273.470410	34.201946
933.915722	77433.012105	34.206964
934.704899	77583.538511	34.211981
936.003414	77732.343708	34.216999
936.816338	77898.111245	34.222016
937.749143	78042.747547	34.227034
938.721343	78196.030874	34.232052
939.947730	78331.278577	34.237069
941.246044	78473.415879	34.242087
942.030862	78630.287829	34.247104
943.058796	78766.538691	34.252122
944.002555	78919.762127	34.257140
945.143006	79062.542801	34.262157
946.232872	79213.808613	34.267175
946.745206	79356.625296	34.272192
948.126934	79497.129752	34.277210
948.880055	79642.875102	34.282228
950.554504	79748.770851	34.287245
951.634706	79875.050974	34.292263
952.698379	80018.546235	34.297280
953.586720	80134.365485	34.302298
954.082545	80263.989284	34.307316
954.650258	80387.598957	34.312333
955.638657	80510.108772	34.317351
956.898570	80649.021200	34.322368
957.339643	80783.844096	34.327386
958.138631	80919.222304	34.332404
959.025569	81047.299487	34.337421
960.080530	81184.231125	34.342439
961.173685	81334.523861	34.347456
962.130029	81456.854340	34.352474
962.834443	81603.531367	34.357492
963.611483	81752.525318	34.362509
964.379927	81893.424347	34.367527
964.845524	82066.188085	34.372544
966.112027	82217.482887	34.377562
966.973604	82381.339728	34.382580
967.807741	82542.766689	34.387597
968.803484	82689.174890	34.392615
969.527476	82851.375048	34.397632
970.793953	83010.291993	34.402650
972.040502	83177.652736	34.407668
972.480284	83341.238168	34.412685
973.863757	83510.830957	34.417703
974.719868	83670.237793	34.422720
975.941746	83826.213289	34.427738
978.127030	83949.733467	34.432756
979.495408	84107.382221	34.437773
980.809010	84244.004873	34.442791
982.265294	84381.825840	34.447808
983.011194	84508.534922	34.452826
984.281765	84650.057677	34.457844
985.309924	84770.249291	34.462861
986.573883	84885.163962	34.467879
986.978440	85015.437269	34.472896
987.855911	85155.882863	34.477914
988.512180	85295.347188	34.482932
989.183069	85437.157262	34.487949
990.491637	85581.374763	34.492967
990.831622	85732.029547	34.497984
992.223504	85866.409100	34.503002
993.603581	86000.766074	34.508020
994.830639	86136.800488	34.513037
996.069923	86265.532050	34.518055
996.899139	86403.778644	34.523072
997.880357	86532.794729	34.528090
998.788021	86675.617286	34.533108
999.391431	86823.692060	34.538125
1000.307830	86964.180136	34.543143
1000.723750	87117.001657	34.548160
1001.726714	87264.494410	34.553178
1003.073792	87411.842696	34.558196
1003.679750	87570.014216	34.563213
1004.858360	87711.064611	34.568231
1005.532320	87859.545591	34.573248
1006.596022	88018.157103	34.578266
1007.861996	88185.361022	34.583284
1008.849768	88335.134683	34.588301
1010.064939	88486.649878	34.593319
1011.122935	88642.589870	34.598336
1012.407605	88782.806566	34.603354
1013.836089	88909.578769	34.608372
1014.636488	89057.862923	34.613389
1015.981611	89194.901766	34.618407
1016.740688	89345.295449	34.623424
1017.166813	89490.739524	34.628442
1018.234697	89636.578465	34.633460
1019.055166	89780.908745	34.638477
1020.176135	89928.949255	34.643495
1021.008871	90070.558136	34.648512
1022.117890	90198.143045	34.653530
1023.328655	90338.406468	34.658548
1024.028544	90477.033743	34.663565
1025.384246	90608.098697	34.668583
1026.855282	90744.391606	34.673600
1028.040028	90870.499419	34.678618
1029.644507	90990.532854	34.683636
1030.334535	91132.779143	34.688653
1031.129374	91257.124418	34.693671
1031.991379	91394.989815	34.698688
1033.064139	91533.283203	34.703706
1034.089482	91663.535134	34.708724
1034.826172	91796.278309	34.713741
1035.651445	91950.443081	34.718759
1036.677136	92089.962567	34.723776
1037.138048	92259.973489	34.728794
1038.119912	92405.868852	34.733812
1038.807497	92572.376330	34.738829
1039.525294	92738.266059	34.743847
1040.793420	92910.483686	34.748864
1042.390093	93061.762436	34.753882
1043.993540	93212.730889	34.758900
1044.999025	93380.552203	34.763917
1045.882820	93535.166798	34.768935
1046.854030	93697.774399	34.773952
1047.602330	93859.464171	34.778970
1048.656081	94018.566542	34.783988
1050.311467	94171.165342	34.789005
1051.715972	94320.559547	34.794023
1052.599853	94479.749939	34.799040
1053.597662	94637.352855	34.804058
1055.270340	94791.376810	34.809076
1055.723047	94960.629463	34.814093
1056.571322	95113.595262	34.819111
1057.611103	95268.498912	34.824128
1058.750529	95424.247924	34.829146
1060.334434	95568.417155	34.834164
1061.066156	95738.838083	34.839181
1061.763503	95904.980602	34.844199
1062.594162	96073.001181	34.849216
1063.426602	96240.573189	34.854234
1064.598255	96409.698133	34.859252
1065.482978	96585.030651	34.864269
1066.272954	96770.045968	34.869287
1067.342819	96952.661681	34.874304
1068.076263	97133.663131	34.879322
1068.959702	97326.029069	34.884340
1069.787716	97520.545252	34.889357
1070.685405	97716.640343	34.894375
1071.772700	97918.542210	34.899392
1072.430383	98133.974956	34.904410
1073.357984	98332.342543	34.909428
1074.263267	98536.026636	34.914445
1075.457726	98737.999725	34.919463
1076.727109	98961.479637	34.924480
1077.562052	99179.202760	34.929498
1079.256385	99385.713557	34.934516
1080.299198	99589.446796	34.939533
1081.628442	99785.398198	34.944551
1082.775715	99978.557618	34.949568
1083.922287	100181.119964	34.954586
1085.355565	100387.669397	34.959604
1086.334718	100582.215995	34.964621
1086.899686	100785.759191	34.969639
1088.572154	100986.639411	34.974656
1090.503623	101153.746293	34.979674
1092.012377	101327.723712	34.984692
1093.141959	101507.608608	34.989709
1094.215536	101662.001792	34.994727
1094.898102	101823.887041	34.999744
1095.945705	102002.598676	35.004762
1097.300976	102168.781656	35.009780
1098.086051	102337.313821	35.014797
1099.217764	102508.436413	35.019815
1100.332689	102680.499976	35.024832
1101.054776	102866.805838	35.029850
1101.878639	103036.830427	35.034868
1102.813779	103249.221637	35.039885
1103.834672	103416.911494	35.044903
1104.959384	103627.704269	35.049920
1105.878103	103815.510460	35.054938
1107.487577	103995.225905	35.059956
1108.941552	104174.771979	35.064973
1110.229704	104353.605837	35.069991
1111.501165	104559.829333	35.075008
1112.367098	104736.367375	35.080026
1113.805318	104923.677910	35.085044
1115.237697	105096.471301	35.090061
1116.575139	105271.193807	35.095079
1117.881813	105432.637692	35.100096
1119.011650	105611.322680	35.105114
1120.271093	105779.159357	35.110132
1121.205702	105967.390027	35.115149
1122.233939	106148.020458	35.120167
1122.905556	106322.859886	35.125184
1124.048328	106502.511322	35.130202
1125.255776	106672.135360	35.135220
1126.033703	106870.960891	35.140237
1127.485319	107052.274863	35.145255
1129.157315	107227.651728	35.150272
1130.158769	107415.945026	35.155290
1131.473675	107590.572663	35.160308
1132.615612	107758.453996	35.165325
1133.744710	107939.713291	35.170343
1134.419281	108124.582555	35.175360
1135.155678	108313.913884	35.180378
1136.326979	108507.202485	35.185396
1137.026653	108701.482280	35.190413
1138.276337	108888.187107	35.195431
1140.016327	109065.350759	35.200448
1141.166368	109261.751502	35.205466
1143.233293	109430.047963	35.210484
1144.497229	109618.630125	35.215501
1145.392685	109795.127360	35.220519
1146.552230	109954.761083	35.225536
1147.702701	110149.787593	35.230554
1149.382504	110328.578159	35.235572
1149.830267	110516.401993	35.240589
1150.711801	110697.860118	35.245607
1152.110312	110875.560717	35.250624
1152.887595	111058.127813	35.255642
1154.220210	111242.124514	35.260660
1155.643664	111421.661295	35.265677
1156.275338	111611.121734	35.270695
1157.408597	111778.826900	35.275712
1157.805762	111984.872165	35.280730
1158.912488	112188.471032	35.285748
1159.874904	112396.490891	35.290765
1161.055933	112592.973972	35.295783
1162.093315	112806.013635	35.300800
1162.851015	113019.139118	35.305818
1164.209822	113223.844158	35.310836
1165.509004	113456.252994	35.315853
1166.436146	113660.741162	35.320871
1167.876629	113852.477830	35.325888
1168.950091	114047.304147	35.330906
1170.289707	114236.463108	35.335924
1171.514621	114437.094648	35.340941
1172.499355	114634.030036	35.345959
1173.929179	114825.661167	35.350976
1174.686111	115033.481402	35.355994
1175.776137	115232.455982	35.361012
1177.244185	115431.927014	35.366029
1178.486216	115643.092331	35.371047
1179.890324	115826.499662	35.376064
1180.988243	116036.171426	35.381082
1182.354125	116235.221609	35.386100
1183.143441	116442.286773	35.391117
1184.214931	116658.226236	35.396135
1185.333663	116861.097156	35.401152
1185.967815	117082.597999	35.406170
1187.544735	117307.505176	35.411188
1188.199752	117521.290074	35.416205
1188.790612	117757.601806	35.421223
1190.600010	117971.858381	35.426240
1191.917781	118203.555929	35.431258
1193.427952	118438.821972	35.436276
1194.635099	118658.821414	35.441293
1196.079526	118881.228790	35.446311
1197.481377	119094.116607	35.451328
1198.628251	119320.542406	35.456346
1200.337344	119533.889594	35.461364
1201.621426	119744.318181	35.466381
1202.849335	119965.502584	35.471399
1204.667975	120180.762465	35.476416
1205.614393	120402.123380	35.481434
1206.772118	120612.046942	35.486452
1207.849053	120812.557851	35.491469
1208.531507	121038.782307	35.496487
1210.071626	121242.881780	35.501504
1211.228544	121482.856041	35.506522
1212.021448	121706.381044	35.511540
1213.357379	121925.851826	35.516557
1214.278840	122168.607689	35.521575
1215.930274	122387.041428	35.526592
1216.657804	122619.011084	35.531610
1217.780315	122856.860655	35.536628
1219.210618	123095.649781	35.541645
1220.551452	123330.958002	35.546663
1222.169264	123543.855311	35.551680
1223.042607	123772.882581	35.556698
1224.287744	124000.950481	35.561716
1225.914986	124235.610300	35.566733
1227.361787	124465.397320	35.571751
1228.341065	124693.717164	35.576768
1229.700973	124920.214355	35.581786
1231.319283	125134.833811	35.586804
1232.630649	125360.696005	35.591821
1233.910705	125580.709944	35.596839
1235.892053	125792.346611	35.601856
1238.002113	125965.714643	35.606874
1239.470157	126164.777749	35.611892
1240.850851	126360.498040	35.616909
1241.722098	126555.847425	35.621927
1243.039602	126736.397337	35.626944
1244.131759	126933.258901	35.631962
1245.343106	127119.569922	35.636980
1246.651639	127325.865831	35.641997
1247.257632	127519.782306	35.647015
1248.226876	127712.372622	35.652032
1249.222462	127929.674855	35.657050
1250.082817	128129.421446	35.662068
1251.493955	128328.710864	35.667085
1252.069832	128536.225857	35.672103
1253.402200	128739.130529	35.677120
1254.779295	128928.720608	35.682138
1255.555739	129149.755985	35.687156
1256.650357	129371.095322	35.692173
1257.169166	129602.899489	35.697191
1258.338004	129820.034324	35.702208
1259.161130	130058.319365	35.707226
1260.281500	130301.614632	35.712244
1261.421505	130546.201449	35.717261
1262.211920	130800.646087	35.722279
1263.853958	131068.692648	35.727296
1265.401840	131304.408463	35.732314
1266.397673	131551.511355	35.737332
1267.509390	131808.649095	35.742349
1268.917692	132077.199145	35.747367
1269.959109	132335.290794	35.752384
1271.388020	132594.702299	35.757402
1272.223870	132856.165968	35.762420
1273.841214	133125.083334	35.767437
1275.497773	133385.122874	35.772455
1276.900000	133646.562910	35.777472
1278.622594	133904.744969	35.782490
1279.755530	134176.147024	35.787508
1281.491528	134432.353506	35.792525
1282.197466	134698.873724	35.797543
1284.148298	134952.437386	35.802560
1285.689462	135222.158161	35.807578
1286.679364	135478.153773	35.812596
1288.349676	135731.693755	35.817613
1289.292303	135984.772642	35.822631
1290.437260	136240.102080	35.827648
1292.109604	136500.011898	35.832666
1293.241618	136771.778061	35.837684
1294.619105	137028.710703	35.842701
1295.883499	137290.545088	35.847719
1297.533907	137546.980308	35.852736
1299.126047	137805.442983	35.857754
1299.758555	138067.413158	35.862772
1301.544618	138333.454984	35.867789
1302.736613	138594.893217	35.872807
1303.769710	138857.323304	35.877824
1305.941443	139114.407243	35.882842
1306.871256	139359.982820	35.887860
1308.644548	139606.131000	35.892877
1309.629082	139878.935826	35.897895
1311.076550	140122.225359	35.902912
1312.166751	140386.128727	35.907930
1312.767274	140646.057563	35.912948
1314.687971	140915.026521	35.917965
1316.008314	141177.135597	35.922983
1317.048939	141430.480477	35.928000
1318.522742	141693.493802	35.933018
1319.740028	141970.169667	35.938036
1321.143421	142232.197032	35.943053
1322.106896	142505.127776	35.948071
1323.560128	142769.636293	35.953088
1325.171410	143035.629699	35.958106
1326.208173	143308.567364	35.963124
1327.659402	143583.873415	35.968141
1328.876106	143848.961771	35.973159
1330.554191	144104.465498	35.978176
1332.194035	144372.861045	35.983194
1333.348950	144636.824299	35.988212
1335.236049	144885.565691	35.993229
1336.419585	145143.339722	35.998247
1337.871368	145400.158321	36.003264
1339.197501	145635.378058	36.008282
1340.306943	145892.928832	36.013300
1341.803226	146120.324703	36.018317
1343.219784	146351.907384	36.023335
1344.879147	146582.525742	36.028352
1346.452166	146819.982554	36.033370
1347.334933	147055.525785	36.038388
1348.374353	147301.431096	36.043405
1349.609946	147534.725283	36.048423
1350.743503	147776.560098	36.053440
1351.927841	148026.098836	36.058458
1353.083095	148287.070701	36.063476
1354.409731	148547.255222	36.068493
1355.752818	148807.159876	36.073511
1356.796114	149071.757622	36.078528
1357.984828	149342.420885	36.083546
1359.365387	149604.163981	36.088564
1360.966192	149874.369994	36.093581
1362.490356	150156.918308	36.098599
1363.619396	150427.497937	36.103616
1364.545033	150710.491695	36.108634
1366.092007	151001.540284	36.113652
1367.317544	151271.247685	36.118669
1368.418576	151568.119770	36.123687
1369.959146	151854.495940	36.128704
1371.534522	152137.418649	36.133722
1372.485745	152445.915087	36.138740
1374.107635	152735.747157	36.143757
1375.473485	153038.713346	36.148775
1376.859247	153343.061209	36.153792
1378.383481	153621.754365	36.158810
1379.630916	153918.303650	36.163828
1380.770569	154212.095191	36.168845
1382.203560	154526.642748	36.173863
1384.012928	154814.531663	36.178880
1385.666513	155111.023125	36.183898
1387.172539	155411.270468	36.188916
1388.534554	155702.030418	36.193933
1390.297868	156001.326565	36.198951
1391.421111	156295.885033	36.203968
1392.843952	156600.303207	36.208986
1393.837267	156893.403469	36.214004
1396.098851	157177.581929	36.219021
1397.898545	157459.529955	36.224039
1399.620939	157735.784363	36.229056
1401.088270	158020.823021	36.234074
1402.557384	158308.641546	36.239092
1403.646757	158585.983106	36.244109
1405.180822	158866.830555	36.249127
1406.429962	159148.006077	36.254144
1408.176190	159408.525110	36.259162
1409.433164	159695.284922	36.264180
1411.162387	159979.939070	36.269197
1412.214072	160263.451105	36.274215
1414.217954	160542.240948	36.279232
1415.993043	160797.613550	36.284250
1417.503237	161078.315347	36.289268
1418.726118	161336.446572	36.294285
1419.865514	161605.364040	36.299303
1421.188107	161876.967959	36.304320
1422.783679	162156.800326	36.309338
1423.816651	162439.429707	36.314356
1425.226619	162718.027807	36.319373
1426.143008	162999.639903	36.324391
1427.366662	163285.288408	36.329408
1428.673582	163569.351912	36.334426
1429.345018	163863.151787	36.339444
1430.663434	164172.604544	36.344461
1432.308460	164463.710462	36.349479
1434.206671	164736.011840	36.354496
1435.854666	164992.179642	36.359514
1437.027240	165279.588218	36.364532
1438.394587	165551.614459	36.369549
1439.742215	165834.354163	36.374567
1441.152012	166127.020061	36.379584
1442.537929	166405.405247	36.384602
1443.556982	166702.453417	36.389620
1444.817354	166997.560573	36.394637
1445.987376	167305.487036	36.399655
1446.853443	167612.196993	36.404672
1448.252357	167929.251012	36.409690
1449.548921	168265.750271	36.414708
1450.211466	168592.941788	36.419725
1451.572971	168922.824564	36.424743
1453.130234	169267.409138	36.429760
1454.707548	169596.170039	36.434778
1455.904408	169958.609193	36.439796
1458.107117	170283.769757	36.444813
1460.816969	170599.484378	36.449831
1462.726211	170913.442620	36.454848
1465.137413	171215.379540	36.459866
1466.892977	171525.611316	36.464884
1468.531364	171831.829268	36.469901
1469.755506	172128.232440	36.474919
1471.188704	172426.125772	36.479936
1473.009921	172719.845513	36.484954
1474.778528	173014.476769	36.489972
1476.241562	173316.050922	36.494989
1477.572565	173605.111110	36.500007
1478.499884	173913.668163	36.505024
1480.014071	174210.696575	36.510042
1481.481774	174529.447484	36.515060
1483.007095	174847.467676	36.520077
1484.549328	175140.131806	36.525095
1485.397631	175457.290618	36.530112
1486.845822	175769.885457	36.535130
1487.892492	176105.975492	36.540148
1488.768625	176425.001596	36.545165
1490.430412	176760.626629	36.550183
1491.857336	177099.985778	36.555200
1493.610817	177433.150955	36.560218
1494.974782	177776.421302	36.565236
1496.326945	178109.974555	36.570253
1498.344197	178443.026872	36.575271
1500.028188	178769.752675	36.580288
1502.068652	179079.275703	36.585306
1503.610955	179414.951153	36.590324
1505.349252	179737.778012	36.595341
1507.199462	180060.499622	36.600359
1508.380218	180380.770024	36.605376
1510.204738	180696.785985	36.610394
1511.423267	181009.007486	36.615412
1513.539132	181322.491617	36.620429
1516.029663	181618.248515	36.625447
1517.303403	181923.181210	36.630464
1518.872846	182205.462126	36.635482
1520.432085	182514.069976	36.640500
1521.367337	182821.031069	36.645517
1522.873217	183136.086388	36.650535
1523.985978	183456.716991	36.655552
1525.480599	183776.588429	36.660570
1526.515906	184085.634612	36.665588
1527.730963	184407.434469	36.670605
1529.447335	184731.006677	36.675623
1530.783774	185076.614857	36.680640
1532.760501	185391.656534	36.685658
1533.762843	185711.303373	36.690676
1534.960025	186013.225773	36.695693
1536.611990	186317.423023	36.700711
1537.852682	186635.779292	36.705728
1539.345943	186949.348423	36.710746
1540.785711	187270.823423	36.715764
1541.927884	187601.412497	36.720781
1543.623618	187933.790816	36.725799
1544.378082	188274.463007	36.730816
1545.930764	188611.997134	36.735834
1547.474746	188957.760246	36.740852
1548.433664	189317.674053	36.745869
1549.834673	189676.336631	36.750887
1550.989589	190043.001171	36.755904
1552.132586	190419.304789	36.760922
1553.726064	190809.220793	36.765940
1554.885147	191190.909036	36.770957
1557.085321	191572.897648	36.775975
1558.559135	191967.741057	36.780992
1560.208675	192350.904546	36.786010
1561.678861	192737.883055	36.791028
1563.226778	193139.005746	36.796045
1565.116601	193530.426676	36.801063
1566.863524	193926.735806	36.806080
1569.024177	194323.423545	36.811098
1570.409849	194708.625807	36.816116
1572.064806	195099.384538	36.821133
1574.425037	195468.536487	36.826151
1576.391541	195846.426391	36.831168
1578.224761	196221.293678	36.836186
1579.782724	196588.362866	36.841204
1581.609643	196970.916281	36.846221
1583.178753	197328.707508	36.851239
1584.740309	197703.755230	36.856256
1586.343754	198085.818888	36.861274
1588.076034	198450.978215	36.866292
1589.824460	198823.119580	36.871309
1591.986317	199169.828504	36.876327
1593.858454	199536.976678	36.881344
1595.202622	199896.596382	36.886362
1597.127722	200253.100486	36.891380
1598.034371	200623.003863	36.896397
1599.828604	200969.719207	36.901415
1601.361903	201340.627626	36.906432
1602.890119	201696.404856	36.911450
1604.710823	202076.665063	36.916468
1606.131070	202446.721975	36.921485
1607.879405	202807.255090	36.926503
1609.503316	203178.729629	36.931520
1611.010854	203536.005053	36.936538
1612.785787	203903.014602	36.941556
1614.643944	204273.529289	36.946573
1616.211995	204627.752892	36.951591
1617.303556	204989.535303	36.956608
1618.971904	205351.706803	36.961626
1621.276565	205715.387602	36.966644
1622.693635	206092.129561	36.971661
1624.773183	206450.480200	36.976679
1626.430029	206806.908816	36.981696
1627.763542	207161.551343	36.986714
1629.301867	207520.821633	36.991732
1630.948101	207885.738822	36.996749
1632.485047	208256.554671	37.001767
1633.899976	208617.475654	37.006784
1635.574631	208988.234137	37.011802
1637.210366	209353.985209	37.016820
1638.650808	209724.341338	37.021837
1640.565063	210062.178272	37.026855
1641.519017	210414.574348	37.031872
1643.066220	210778.632262	37.036890
1644.533335	211147.288940	37.041908
1645.791812	211507.118505	37.046925
1647.591335	211862.543024	37.051943
1648.917275	212224.802551	37.056960
1650.734150	212576.138430	37.061978
1652.533677	212949.294072	37.066996
1653.623395	213332.015924	37.072013
1655.439884	213721.806779	37.077031
1656.806571	214094.099078	37.082048
1658.707459	214471.815910	37.087066
1660.589568	214850.172364	37.092084
1661.869337	215230.179011	37.097101
1663.853300	215614.388574	37.102119
1665.864108	216006.112900	37.107136
1667.603335	216395.775722	37.112154
1669.488152	216777.365171	37.117172
1671.093929	217155.319571	37.122189
1673.130711	217538.791848	37.127207
1674.416486	217944.485602	37.132224
1675.824373	218381.171688	37.137242
1677.428417	218768.860103	37.142260
1678.843425	219174.791641	37.147277
1681.003279	219557.616616	37.152295
1683.073650	219951.633049	37.157312
1685.049540	220341.856852	37.162330
1686.951520	220730.519637	37.167348
1688.515179	221132.243758	37.172365
1690.087332	221529.929642	37.177383
1691.707460	221903.632708	37.182400
1693.258333	222306.887344	37.187418
1694.771503	222688.992415	37.192436
1696.565989	223111.614636	37.197453
1697.955290	223514.798817	37.202471
1699.550598	223921.023777	37.207488
1701.042062	224332.347198	37.212506
1703.023813	224745.877164	37.217524
1704.386960	225160.171065	37.222541
1706.681651	225580.611846	37.227559
1708.532179	225976.286549	37.232576
1710.237493	226390.858530	37.237594
1712.059071	226809.806927	37.242612
1713.504918	227216.448996	37.247629
1715.589288	227627.051058	37.252647
1717.429900	228026.594851	37.257664
1719.044597	228441.823675	37.262682
1721.089433	228854.798458	37.267700
1722.318779	229273.319363	37.272717
1723.867198	229692.449368	37.277735
1725.270193	230112.671501	37.282752
1726.907888	230536.259893	37.287770
1728.928075	230946.755963	37.292788
1730.586123	231381.469067	37.297805
1732.346715	231818.732070	37.302823
1733.802829	232243.727219	37.307840
1735.684048	232665.427555	37.312858
1737.707623	233090.204533	37.317876
1739.699841	233523.294041	37.322893
1741.367693	233952.399508	37.327911
1743.216481	234366.337183	37.332928
1745.224485	234777.277730	37.337946
1747.373313	235175.419220	37.342964
1749.857979	235574.954160	37.347981
1752.161988	235961.488917	37.352999
1754.243660	236355.376886	37.358016
1755.592938	236745.525551	37.363034
1757.660180	237122.347793	37.368052
1759.166024	237495.935836	37.373069
1760.744394	237854.043029	37.378087
1762.757885	238236.134644	37.383104
1764.346247	238588.653227	37.388122
1765.805940	238950.160566	37.393140
1767.046259	239322.195782	37.398157
1768.831054	239693.176608	37.403175
1770.900888	240062.383766	37.408192
1772.550146	240447.207061	37.413210
1774.427516	240807.607396	37.418228
1776.295785	241198.644876	37.423245
1777.839552	241572.234475	37.428263
1779.617280	241959.681155	37.433280
1780.173474	242368.515555	37.438298
1782.037707	242765.144986	37.443316
1783.255558	243179.256968	37.448333
1784.365386	243589.907354	37.453351
1786.149959	244011.598807	37.458368
1787.591358	244450.291070	37.463386
1789.382741	244888.596109	37.468404
1790.662565	245338.671467	37.473421
1792.001239	245809.364816	37.478439
1793.864263	246257.668878	37.483456
1795.495491	246730.169873	37.488474
1797.297034	247188.036917	37.493492
1799.229438	247669.456856	37.498509
1800.507489	248150.045553	37.503527
1802.383619	248640.214773	37.508544
1803.681212	249132.131309	37.513562
1805.483291	249622.060059	37.518580
1807.153456	250142.647202	37.523597
1809.197486	250644.984781	37.528615
1811.264542	251137.259549	37.533632
1813.094939	251650.531440	37.538650
1815.527145	252156.083679	37.543668
1817.599613	252660.196987	37.548685
1819.486889	253166.932442	37.553703
1821.193587	253649.234879	37.558720
1822.714545	254159.029186	37.563738
1824.896643	254656.114825	37.568756
1826.727893	255180.973604	37.573773
1828.350645	255706.629220	37.578791
1830.600177	256208.455107	37.583808
1832.109739	256720.056557	37.588826
1834.246964	257233.078891	37.593844
1836.579282	257731.665575	37.598861
1838.832692	258233.110600	37.603879
1840.974065	258724.336705	37.608896
1842.995332	259236.794475	37.613914
1844.694995	259719.456478	37.618932
1846.403310	260198.357397	37.623949
1848.501099	260694.823970	37.628967
1850.355346	261191.051257	37.633984
1851.652380	261707.667647	37.639002
1854.005510	262188.468904	37.644020
1855.908505	262678.311671	37.649037
1857.731528	263188.566325	37.654055
1860.060434	263683.673205	37.659072
1861.088414	264176.555767	37.664090
1863.142786	264666.017170	37.669108
1865.162729	265178.651746	37.674125
1866.782635	265686.296757	37.679143
1868.771568	266179.045085	37.684160
1870.570703	266678.098957	37.689178
1872.288565	267176.708590	37.694196
1874.263263	267686.681446	37.699213
1875.711169	268204.412471	37.704231
1877.506968	268687.359566	37.709248
1879.109327	269185.427512	37.714266
1880.930486	269665.575087	37.719284
1882.632102	270162.507838	37.724301
1884.379506	270656.180859	37.729319
1886.515734	271150.424196	37.734336
1888.337704	271656.683492	37.739354
1890.044808	272157.601017	37.744372
1892.167705	272646.560701	37.749389
1893.980510	273157.950674	37.754407
1895.711503	273657.439429	37.759424
1897.451798	274175.469811	37.764442
1899.280360	274689.420296	37.769460
1901.338105	275213.188260	37.774477
1902.322314	275746.785281	37.779495
1904.762570	276267.947839	37.784512
1906.419410	276794.039627	37.789530
1908.372286	277329.759782	37.794548
1910.459470	277859.563241	37.799565
1912.102300	278411.564184	37.804583
1914.499726	278929.806756	37.809600
1916.394322	279481.382479	37.814618
1918.193173	280028.857428	37.819636
1920.645519	280554.733016	37.824653
1922.502584	281091.171032	37.829671
1924.877235	281629.300342	37.834688
1927.011545	282164.698983	37.839706
1929.073817	282692.944680	37.844724
1931.339836	283218.284849	37.849741
1933.787899	283743.720450	37.854759
1935.766347	284264.634252	37.859776
1937.610407	284807.464671	37.864794
1939.708214	285322.640190	37.869812
1942.019614	285841.716049	37.874829
1943.515204	286363.871327	37.879847
1945.829096	286879.234798	37.884864
1948.234405	287402.963799	37.889882
1950.563610	287920.886719	37.894900
1952.894664	288426.462707	37.899917
1954.330492	288942.040090	37.904935
1956.194629	289436.665615	37.909952
1958.405731	289949.672983	37.914970
1960.705051	290475.135523	37.919988
1962.456286	290980.645526	37.925005
1963.865353	291493.322127	37.930023
1965.499827	292001.819311	37.935040
1967.433593	292538.484610	37.940058
1968.874386	293069.920354	37.945076
1970.744398	293595.110869	37.950093
1972.565915	294149.262848	37.955111
1974.500666	294678.755962	37.960128
1976.113911	295229.660740	37.965146
1977.935464	295782.484316	37.970164
1980.071816	296333.424566	37.975181
1981.460206	296909.427465	37.980199
1983.308218	297456.599899	37.985216
1985.205599	298034.036936	37.990234
1986.751198	298594.587950	37.995252
1989.045510	299172.181988	38.000269
1991.209325	299752.283423	38.005287
1993.249769	300315.410474	38.010304
1995.378580	300893.758754	38.015322
1997.747234	301456.622141	38.020340
2000.356743	302022.591948	38.025357
2002.981071	302584.263816	38.030375
2005.186416	303123.600836	38.035392
2007.237393	303665.601601	38.040410
2009.493672	304209.140018	38.045428
2011.851015	304738.385380	38.050445
2013.801052	305257.459872	38.055463
2015.984191	305756.784971	38.060480
2018.110981	306258.199120	38.065498
2019.229085	306779.078216	38.070516
2021.872870	307281.874285	38.075533
2023.103981	307793.433596	38.080551
2025.114612	308312.911872	38.085568
2026.993877	308833.729231	38.090586
2028.761870	309370.611879	38.095604
2030.462661	309890.639427	38.100621
2032.953099	310424.805723	38.105639
2034.625770	310965.325245	38.110656
2036.528082	311504.584299	38.115674
2038.401755	312055.856254	38.120692
2040.195914	312596.293890	38.125709
2042.481613	313141.674850	38.130727
2044.183983	313699.464473	38.135744
2046.369392	314262.503152	38.140762
2048.018712	314839.897519	38.145780
2050.091783	315412.291133	38.150797
2051.572571	315990.466189	38.155815
2053.759601	316561.994085	38.160832
2055.777182	317162.519134	38.165850
2057.506489	317746.124150	38.170868
2059.987664	318338.208540	38.175885
2061.576151	318942.369703	38.180903
2063.782361	319562.547911	38.185920
2065.678669	320177.870958	38.190938
2067.824097	320791.471496	38.195956
2070.317444	321401.708152	38.200973
2072.014443	322005.392613	38.205991
2074.031112	322636.339808	38.211008
2076.299491	323246.012545	38.216026
2079.077182	323860.876826	38.221044
2082.303316	324443.846950	38.226061
2084.777897	325041.230405	38.231079
2087.296981	325622.148113	38.236096
2089.399129	326211.482424	38.241114
2091.563065	326807.935399	38.246132
2094.171600	327375.314656	38.251149
2096.577990	327954.172431	38.256167
2098.633708	328529.705768	38.261184
2100.912789	329109.157347	38.266202
2102.911560	329673.949643	38.271220
2105.173614	330236.205059	38.276237
2106.913768	330810.828848	38.281255
2108.995916	331375.337039	38.286272
2110.650295	331967.836303	38.291290
2112.434709	332550.559318	38.296308
2114.565088	333138.855136	38.301325
2116.206185	333737.202375	38.306343
2118.051495	334327.817453	38.311360
2120.090633	334933.295811	38.316378
2121.792241	335539.990869	38.321396
2124.024608	336144.129220	38.326413
2125.964413	336758.615396	38.331431
2127.838709	337378.080726	38.336448
2130.217503	338008.294798	38.341466
2132.041930	338637.628126	38.346484
2134.311202	339245.329536	38.351501
2136.208256	339878.468802	38.356519
2138.047747	340517.117915	38.361536
2140.313876	341150.459753	38.366554
2142.433542	341788.894323	38.371572
2145.024025	342417.115552	38.376589
2146.942833	343055.389349	38.381607
2149.027842	343680.505139	38.386624
2151.868333	344280.208505	38.391642
2154.442324	344893.857230	38.396660
2156.716706	345488.588140	38.401677
2158.970626	346072.452212	38.406695
2160.890028	346657.404861	38.411712
2163.053651	347240.101945	38.416730
2165.289605	347831.028190	38.421748
2167.493697	348422.307500	38.426765
2169.740765	349016.059289	38.431783
2172.158949	349601.349522	38.436800
2174.586700	350187.772690	38.441818
2176.793871	350779.655507	38.446836
2178.496541	351363.797469	38.451853
2180.544187	351972.287764	38.456871
2182.484001	352578.605107	38.461888
2184.882435	353171.262080	38.466906
2186.788773	353789.647466	38.471924
2189.184604	354390.637086	38.476941
2191.269238	354999.510688	38.481959
2193.142511	355618.941176	38.486976
2195.449308	356245.802103	38.491994
2197.517144	356873.784278	38.497012
2199.551201	357498.235701	38.502029
2201.411904	358134.073756	38.507047
2203.323322	358780.220611	38.512064
2205.458191	359425.153381	38.517082
2207.289155	360083.116786	38.522100
2209.181344	360741.313212	38.527117
2211.357378	361410.209672	38.532135
2213.587017	362095.501276	38.537152
2216.409363	362764.928235	38.542170
2218.761169	363431.656158	38.547188
2220.879344	364097.751737	38.552205
2223.216667	364771.258463	38.557223
2225.124131	365458.701234	38.562240
2228.188024	366127.980235	38.567258
2230.805593	366802.597741	38.572276
2232.816237	367475.375490	38.577293
2235.641760	368145.876115	38.582311
2238.428196	368820.024077	38.587328
2240.759868	369471.177017	38.592346
2242.575435	370117.863217	38.597364
2244.953960	370790.191126	38.602381
2247.210173	371462.831314	38.607399
2248.976306	372140.790392	38.612416
2251.206505	372819.953882	38.617434
2253.524761	373496.097217	38.622452
2255.528844	374161.322841	38.627469
2257.547803	374848.877991	38.632487
2260.014537	375532.719238	38.637504
2262.237865	376220.645221	38.642522
2264.917287	376906.402915	38.647540
2267.295558	377570.006343	38.652557
2269.935784	378262.007832	38.657575
2271.648014	378952.652250	38.662592
2274.334241	379618.701437	38.667610
2275.962194	380314.074395	38.672628
2278.551400	380998.066366	38.677645
2281.026744	381681.961801	38.682663
2283.220586	382373.953206	38.687680
2285.303913	383054.943782	38.692698
2287.504785	383756.287119	38.697716
2289.453327	384440.339434	38.702733
2292.228102	385129.286840	38.707751
2293.973515	385820.645942	38.712768
2297.494225	386496.307841	38.717786
2299.821268	387187.009376	38.722804
2301.979261	387867.658893	38.727821
2304.389517	388524.649446	38.732839
2306.179658	389199.905742	38.737856
2308.030394	389850.623113	38.742874
2310.443603	390524.455346	38.747892
2312.266285	391195.657958	38.752909
2314.801574	391867.210207	38.757927
2316.617074	392540.108640	38.762944
2318.837759	393211.353940	38.767962
2320.985198	393904.040794	38.772980
2322.674994	394592.300888	38.777997
2324.701305	395305.000004	38.783015
2326.407544	396017.988485	38.788032
2328.301240	396746.541835	38.793050
2330.714543	397479.731158	38.798068
2332.508404	398235.256591	38.803085
2334.672145	398979.803986	38.808103
2336.370885	399741.667578	38.813120
2338.675768	400509.316027	38.818138
2341.100114	401294.207305	38.823156
2343.296108	402082.789263	38.828173
2346.188640	402853.521982	38.833191
2348.691993	403643.327877	38.838208
2351.909495	404418.120223	38.843226
2354.472569	405203.666444	38.848244
2357.142296	405978.911483	38.853261
2359.428929	406747.002548	38.858279
2361.897074	407536.121823	38.863296
2364.558744	408314.115172	38.868314
2367.152844	409096.227102	38.873332
2369.068669	409892.235284	38.878349
2371.661632	410656.265011	38.883367
2374.025917	411455.345240	38.888384
2376.339503	412241.035061	38.893402
2378.875215	413039.786445	38.898420
2381.216222	413830.009741	38.903437
2383.581362	414635.250953	38.908455
2385.682319	415438.864722	38.913472
2388.421451	416241.386137	38.918490
2390.307642	417056.965424	38.923508
2392.319471	417862.393231	38.928525
2394.930738	418684.031772	38.933543
2397.357642	419506.560707	38.938560
2400.080872	420324.025492	38.943578
2402.682719	421155.411433	38.948596
2404.738270	421983.011103	38.953613
2407.431426	422793.057451	38.958631
2409.594567	423628.738338	38.963648
2412.531946	424453.097601	38.968666
2415.141871	425263.178357	38.973684
2417.927078	426082.368526	38.978701
2421.005012	426879.811746	38.983719
2423.553181	427700.201872	38.988736
2426.080687	428492.366495	38.993754
2428.855506	429290.894151	38.998772
2431.541383	430095.434496	39.003789
2434.003928	430895.630763	39.008807
2436.188421	431685.923687	39.013824
2438.812763	432484.976516	39.018842
2441.107942	433275.147322	39.023860
2443.264800	434080.601058	39.028877
2445.979039	434864.676044	39.033895
2448.419775	435660.208622	39.038912
2451.416163	436431.125354	39.043930
2453.737485	437234.620172	39.048948
2455.814061	438016.061262	39.053965
2458.388818	438815.713543	39.058983
2460.255897	439604.624561	39.064000
2462.977770	440409.256907	39.069018
2465.562624	441176.943064	39.074036
2467.853350	441953.506551	39.079053
2470.716282	442712.947295	39.084071
2473.415068	443454.477572	39.089088
2475.845507	444205.235646	39.094106
2478.582767	444959.003762	39.099124
2480.857598	445713.783438	39.104141
2483.344165	446460.913508	39.109159
2485.323600	447214.779231	39.114176
2487.467210	447976.331459	39.119194
2489.774677	448744.203514	39.124212
2492.078898	449517.461066	39.129229
2494.414797	450302.015702	39.134247
2496.328699	451096.777515	39.139264
2498.535198	451898.441030	39.144282
2501.159611	452708.754821	39.149300
2503.199950	453521.004886	39.154317
2505.868650	454335.395570	39.159335
2508.383295	455162.826853	39.164352
2510.438784	455987.216185	39.169370
2513.040986	456817.246994	39.174388
2515.109927	457660.731618	39.179405
2517.600937	458511.645609	39.184423
2520.180216	459371.863046	39.189440
2522.794327	460233.049428	39.194458
2525.499342	461080.079207	39.199476
2528.249328	461947.236596	39.204493
2531.043873	462796.352974	39.209511
2533.501915	463672.228954	39.214528
2536.209205	464534.175473	39.219546
2538.779693	465413.292019	39.224564
2541.464308	466301.195335	39.229581
2543.844446	467172.632673	39.234599
2546.117615	468054.813206	39.239616
2548.496018	468941.383427	39.244634
2551.419904	469819.838909	39.249652
2553.600893	470725.410593	39.254669
2556.047314	471626.600875	39.259687
2558.225784	472552.045100	39.264704
2560.582175	473458.822414	39.269722
2563.545967	474371.821766	39.274740
2565.875637	475288.114575	39.279757
2568.886236	476201.926651	39.284775
2571.339865	477111.492191	39.289792
2574.078934	478034.604125	39.294810
2577.069043	478959.295425	39.299828
2580.287779	479866.831686	39.304845
2583.828933	480752.250453	39.309863
2586.570681	481645.585744	39.314880
2589.144835	482544.308154	39.319898
2592.034628	483425.512881	39.324916
2594.820301	484315.225156	39.329933
2597.338421	485203.927692	39.334951
2600.360979	486099.015983	39.339968
2602.973272	486983.070559	39.344986
2605.542431	487857.597362	39.350004
2607.757880	488747.838815	39.355021
2609.850079	489622.962584	39.360039
2612.455804	490511.687511	39.365056
2614.769671	491412.478478	39.370074
2617.934095	492304.553107	39.375092
2620.494979	493190.221423	39.380109
2623.256747	494080.050319	39.385127
2625.559239	494967.486691	39.390144
2628.177322	495869.761322	39.395162
2631.062703	496755.898712	39.400180
2633.401046	497653.533364	39.405197
2636.315761	498545.223444	39.410215
2639.429689	499416.805074	39.415232
2641.752660	500281.510200	39.420250
2644.512229	501130.713165	39.425268
2646.833392	501982.366390	39.430285
2649.278250	502813.376357	39.435303
2651.548294	503681.545363	39.440320
2654.497425	504538.209108	39.445338
2657.093857	505391.759613	39.450356
2659.703699	506252.979061	39.455373
2662.087428	507115.501437	39.460391
2665.007484	507986.562520	39.465408
2667.621739	508860.753283	39.470426
2670.416827	509739.001198	39.475444
2672.857842	510620.687777	39.480461
2675.833384	511504.960038	39.485479
2678.330586	512380.793372	39.490496
2680.894370	513263.422877	39.495514
2683.747261	514143.032174	39.500532
2686.189399	515051.237699	39.505549
2689.230535	515935.453714	39.510567
2691.785994	516822.774065	39.515584
2694.590990	517726.279722	39.520602
2697.864737	518616.302442	39.525620
2700.754714	519515.205436	39.530637
2703.466644	520420.836949	39.535655
2706.171830	521321.075971	39.540672
2708.557839	522228.720360	39.545690
2711.357591	523131.658589	39.550708
2713.911351	524045.363455	39.555725
2715.867146	524975.179562	39.560743
2718.429897	525913.602133	39.565760
2720.545914	526858.435966	39.570778
2723.268499	527793.239972	39.575796
2726.075084	528752.193057	39.580813
2728.561712	529719.193662	39.585831
2731.423553	530669.705861	39.590848
2734.223699	531640.305723	39.595866
2737.249712	532595.097444	39.600884
2740.118843	533561.078730	39.605901
2742.456706	534555.775554	39.610919
2745.171476	535522.558642	39.615936
2747.815754	536511.736005	39.620954
2750.641538	537494.223135	39.625972
2753.065854	538501.669525	39.630989
2755.185799	539500.893434	39.636007
2758.519054	540494.715429	39.641024
2761.221779	541521.073636	39.646042
2763.683046	542531.298813	39.651060
2766.272605	543551.692912	39.656077
2769.153745	544576.089796	39.661095
2772.085971	545606.238044	39.666112
2774.946891	546635.567796	39.671130
2777.821190	547651.039877	39.676148
2780.641111	548682.940577	39.681165
2783.423084	549717.385264	39.686183
2786.156047	550746.682246	39.691200
2788.532873	551798.986701	39.696218
2791.790286	552829.197182	39.701236
2794.132243	553882.201468	39.706253
2797.071121	554925.827541	39.711271
2800.357037	555972.934589	39.716288
2803.473496	557006.972016	39.721306
2805.959674	558043.094015	39.726324
2809.247090	559099.605314	39.731341
2811.850753	560123.889038	39.736359
2815.341431	561156.387900	39.741376
2818.504262	562182.580721	39.746394
2821.946917	563183.481234	39.751412
2825.149745	564174.902078	39.756429
2828.401195	565138.766941	39.761447
2831.606186	566090.866765	39.766464
2834.063328	567044.526667	39.771482
2836.818176	567985.965866	39.776500
2839.585674	568936.673470	39.781517
2841.852878	569885.184283	39.786535
2845.232795	570836.604422	39.791552
2847.395632	571791.467528	39.796570
2850.029950	572755.116199	39.801588
2852.809859	573722.281619	39.806605
2855.079559	574692.167440	39.811623
2857.831607	575673.692442	39.816640
2860.258707	576667.990270	39.821658
2862.839575	577675.129271	39.826676
2864.982655	578689.734874	39.831693
2867.339449	579705.727711	39.836711
2870.503450	580737.757311	39.841728
2873.037717	581794.934272	39.846746
2875.811078	582831.768956	39.851764
2878.651009	583887.562380	39.856781
2881.186499	584954.647998	39.861799
2883.856653	586020.464926	39.866816
2886.892474	587110.745570	39.871834
2889.762683	588197.847251	39.876852
2892.290201	589305.560340	39.881869
2895.173893	590409.854810	39.886887
2898.609299	591517.815852	39.891904
2901.182254	592636.039586	39.896922
2904.260466	593733.379923	39.901940
2907.641246	594827.412342	39.906957
2910.597383	595950.170981	39.911975
2914.217471	597044.209022	39.916992
2917.377201	598162.414778	39.922010
2920.435992	599258.492557	39.927028
2924.134603	600369.286066	39.932045
2927.063814	601481.402171	39.937063
2930.347519	602568.317298	39.942080
2933.097391	603677.347580	39.947098
2936.007099	604777.033201	39.952116
2938.937979	605879.913617	39.957133
2941.961024	606998.038435	39.962151
2944.791596	608100.270188	39.967168
2947.616766	609216.457708	39.972186
2950.610854	610325.451921	39.977204
2953.914704	611440.790193	39.982221
2956.673822	612562.060745	39.987239
2959.886059	613677.041548	39.992256
2962.691903	614781.374124	39.997274
2965.344008	615891.473823	40.002292
2968.475630	617015.135386	40.007309
2971.300953	618138.883086	40.012327
2973.948704	619258.945496	40.017344
2976.688489	620398.525320	40.022362
2979.904689	621531.459521	40.027380
2982.959955	622676.847840	40.032397
2985.538145	623807.200991	40.037415
2988.753678	624962.566527	40.042432
2990.977345	626117.771856	40.047450
2994.223899	627272.884323	40.052468
2997.148321	628423.629155	40.057485
3000.004794	629586.149148	40.062503
3003.351668	630728.084063	40.067520
3006.548904	631894.840101	40.072538
3009.532545	633054.561778	40.077556
3012.919426	634198.362043	40.082573
3016.421542	635359.042183	40.087591
3019.103986	636508.297649	40.092608
3022.362457	637628.283112	40.097626
3025.364587	638744.347343	40.102644
3028.551881	639832.466099	40.107661
3031.707199	640938.986704	40.112679
3035.407334	642002.642463	40.117696
3038.306635	643098.196476	40.122714
3041.421104	644185.068306	40.127732
3044.643572	645258.440184	40.132749
3047.562916	646356.384033	40.137767
3050.191059	647449.619637	40.142784
3052.845483	648539.940602	40.147802
3055.488333	649642.857966	40.152820
3058.766663	650739.019524	40.157837
3062.167904	651847.451447	40.162855
3065.748433	652942.274934	40.167872
3069.301268	654038.975758	40.172890
3072.655611	655124.626467	40.177908
3076.047693	656223.951905	40.182925
3078.892433	657323.444233	40.187943
3082.156997	658417.663951	40.192960
3084.733546	659518.797523	40.197978
3087.566142	660638.289518	40.202996
3091.060294	661733.295299	40.208013
3094.099644	662850.258046	40.213031
3097.111711	663966.648442	40.218048
3099.656785	665095.181469	40.223066
3102.452650	666228.169368	40.228084
3105.008602	667384.202705	40.233101
3107.936665	668539.686756	40.238119
3110.629274	669699.447661	40.243136
3114.330682	670865.765624	40.248154
3117.346508	672043.890712	40.253172
3120.911136	673207.604814	40.258189
3123.770606	674376.711428	40.263207
3127.075471	675560.564725	40.268224
3130.154849	676751.911570	40.273242
3132.790519	677941.887020	40.278260
3136.424249	679128.613454	40.283277
3139.101634	680343.223991	40.288295
3142.399012	681540.977096	40.293312
3145.294445	682747.235549	40.298330
3148.347828	683960.313672	40.303348
3151.997762	685180.284957	40.308365
3154.881358	686401.411263	40.313383
3158.091475	687630.562527	40.318400
3160.992062	688844.505211	40.323418
3164.132050	690082.768184	40.328436
3167.328181	691323.085280	40.333453
3170.157484	692568.105391	40.338471
3173.232577	693818.370134	40.343488
3176.118846	695075.982468	40.348506
3179.109121	696330.324282	40.353524
3182.266636	697598.249738	40.358541
3185.263203	698870.235158	40.363559
3188.474225	700141.257826	40.368576
3191.933533	701418.847780	40.373594
3194.756510	702689.267490	40.378612
3198.457899	703973.235247	40.383629
3201.732640	705259.115505	40.388647
3204.991550	706532.420462	40.393664
3208.398386	707808.535435	40.398682
3211.917467	709092.665482	40.403700
3215.097518	710369.279850	40.408717
3218.093983	711654.003738	40.413735
3221.931327	712915.669737	40.418752
3225.622066	714173.608358	40.423770
3228.848266	715437.821961	40.428788
3232.324747	716687.651157	40.433805
3235.806288	717931.257244	40.438823
3239.243425	719148.909932	40.443840
3242.847910	720346.174989	40.448858
3245.550149	721551.231834	40.453876
3248.593458	722742.062616	40.458893
3251.672650	723937.265759	40.463911
3254.760591	725140.600724	40.468928
3258.124502	726348.657997	40.473946
3260.537768	727560.549665	40.478964
3264.219528	728772.053368	40.483981
3267.211334	729999.055558	40.488999
3270.078761	731229.302453	40.494016
3273.239583	732465.835093	40.499034
3275.966469	733722.450231	40.504052
3279.419444	734968.429986	40.509069
3282.474911	736222.824007	40.514087
3285.861450	737495.824945	40.519104
3289.544515	738762.651918	40.524122
3292.797284	740052.296017	40.529140
3296.232568	741319.596463	40.534157
3299.370146	742601.444846	40.539175
3302.840617	743878.246249	40.544192
3306.214788	745164.473692	40.549210
3309.421017	746445.686213	40.554228
3313.479133	747726.401186	40.559245
3316.841353	749030.188524	40.564263
3320.204781	750314.733820	40.569280
3324.094915	751597.008973	40.574298
3327.746019	752891.970238	40.579316
3330.734520	754176.823818	40.584333
3333.950542	755477.777111	40.589351
3336.901110	756781.015885	40.594368
3340.377706	758085.669381	40.599386
3343.478190	759391.441700	40.604404
3347.172679	760707.473941	40.609421
3350.683332	762017.501456	40.614439
3354.182721	763313.380091	40.619456
3357.620733	764629.756098	40.624474
3361.095145	765943.288888	40.629492
3364.377653	767261.540602	40.634509
3367.860000	768574.708564	40.639527
3371.475466	769880.052869	40.644544
3374.906769	771197.878569	40.649562
3378.185618	772531.809433	40.654580
3381.569764	773839.933707	40.659597
3384.994312	775163.046901	40.664615
3388.209592	776485.121136	40.669632
3391.838140	777818.329883	40.674650
3395.195188	779148.884948	40.679668
3398.315855	780482.720753	40.684685
3401.382769	781809.694638	40.689703
3404.477894	783178.570329	40.694720
3407.986818	784520.773158	40.699738
3410.898541	785887.201603	40.704756
3414.064050	787250.924732	40.709773
3417.454184	788595.669626	40.714791
3420.466965	789974.832345	40.719808
3424.414412	791343.917836	40.724826
3427.811543	792715.230335	40.729844
3431.149048	794093.782224	40.734861
3434.652768	795480.118991	40.739879
3437.992414	796878.795134	40.744896
3441.277858	798264.127080	40.749914
3443.908449	799668.481790	40.754932
3447.394908	801055.183408	40.759949
3451.030932	802463.554583	40.764967
3454.212160	803886.342016	40.769984
3457.765753	805280.061438	40.775002
3461.052899	806671.610449	40.780007
3464.756607	808016.587227	40.785012
3468.118842	809331.948911	40.790016
3471.172722	810560.962626	40.795021
3474.713270	811720.544352	40.800026
3477.691748	812826.969096	40.805031
3480.851533	813849.235045	40.810036
3483.304359	814813.774844	40.815040
3486.012976	815710.416752	40.820045
3488.525151	816543.766330	40.825050
3491.131219	817311.889996	40.830055
3493.295910	817997.766522	40.835060
3495.323365	818637.246349	40.840064
3497.188011	819208.079808	40.845069
3499.491455	819723.985067	40.850074
3501.160166	820196.161261	40.855079
3503.080188	820601.671066	40.860084
3504.953343	820953.639016	40.865088
3506.164910	821271.206185	40.870093
3507.658359	821519.487722	40.875098
3509.227790	821742.357923	40.880103
3510.452216	821925.359817	40.885108
3511.243422	822059.608205	40.890112
3512.236013	822160.752844	40.895117
3513.367513	822219.413552	40.900122
3514.158090	822257.438308	40.905127
3514.918793	822254.622720	40.910132
3515.774283	822249.101118	40.915136
3516.175079	822212.983718	40.920141
3516.969226	822123.628403	40.925146
3517.529062	822058.231336	40.930151
3518.068451	821944.554456	40.935156
3518.281667	821826.037402	40.940160
3518.500599	821681.246981	40.945165
3519.118489	821508.649045	40.950170
3519.385544	821341.828417	40.955175
3519.507254	821166.906094	40.960180
3519.947878	820955.966165	40.965184
3520.099801	820760.381383	40.970189
3520.404408	820538.295153	40.975194
3520.217397	820315.450661	40.980199
3520.497611	820079.114282	40.985204
3520.558820	819830.816713	40.990208
3520.775262	819601.079988	40.995213
3520.951521	819323.285072	41.000218
3520.439088	819072.606834	41.005223
3520.556271	818805.713648	41.010228
3520.628562	818532.797106	41.015232
3520.392082	818257.375089	41.020237
3520.809240	817982.176687	41.025242
3520.535432	817707.863968	41.030247
3520.623516	817425.697049	41.035252
3520.740013	817152.667931	41.040256
3520.533931	816871.309362	41.045261
3520.034017	816579.167656	41.050266
3520.066983	816301.907238	41.055271
3520.300809	816017.453811	41.060276
3520.100479	815732.276417	41.065280
3519.995102	815449.029925	41.070285
3520.125708	815144.186521	41.075290
3519.742982	814865.955931	41.080295
3519.612269	814564.997994	41.085300
3519.662920	814276.926095	41.090304
3519.422761	813989.477504	41.095309
3519.335389	813708.309774	41.100314
3519.115557	813424.311247	41.105319
3518.990721	813126.520867	41.110324
3519.096101	812847.832671	41.115328
3518.937755	812571.135913	41.120333
3518.951558	812276.273453	41.125338
3518.714019	812002.799785	41.130343
3518.579061	811709.259892	41.135348
3518.798913	811435.541001	41.140352
3518.478401	811154.060482	41.145357
3518.419501	810867.919237	41.150362
3517.621628	810584.337724	41.155367
3517.889845	810307.135242	41.160372
3517.376525	810035.342782	41.165376
3517.055339	809770.221825	41.170381
3517.204055	809497.955788	41.175386
3516.996731	809249.164888	41.180391
3516.854368	808989.032196	41.185396
3516.847783	808728.328045	41.190400
3516.536908	808467.811099	41.195405
3516.601033	808201.732343	41.200410
3516.329018	807935.502502	41.205415
3516.169733	807686.009394	41.210420
3516.266377	807434.258934	41.215424
3516.148278	807184.985879	41.220429
3515.855559	806919.798457	41.225434
3515.781472	806673.637309	41.230439
3515.483006	806432.162255	41.235444
3515.592586	806195.710920	41.240448
3515.304768	805939.408748	41.245453
3515.507604	805699.296357	41.250458
3515.136538	805464.762390	41.255463
3514.833735	805235.407401	41.260468
3514.903887	804988.573543	41.265472
3514.210712	804769.173703	41.270477
3515.046573	804523.913560	41.275482
3514.420126	804296.689496	41.280487
3514.197527	804071.059047	41.285492
3514.352831	803835.450885	41.290496
3514.310555	803613.503543	41.295501
3513.797586	803385.249684	41.300506
3513.671642	803175.270967	41.305511
3513.712236	802950.394415	41.310516
3513.713353	802725.320813	41.315520
3513.217414	802532.259345	41.320525
3513.333381	802312.549886	41.325530
3513.233645	802103.957046	41.330535
3513.052217	801894.880734	41.335540
3512.896354	801681.966810	41.340544
3512.588974	801474.566763	41.345549
3512.693130	801278.623723	41.350554
3512.683633	801083.331768	41.355559
3512.361094	800894.661361	41.360564
3512.809579	800680.243132	41.365568
3512.729769	800497.557834	41.370573
3512.655746	800292.733972	41.375578
3512.506215	800074.469537	41.380583
3512.248965	799871.675577	41.385588
3512.116186	799681.517681	41.390592
3511.868192	799488.183317	41.395597
3511.875006	799297.206629	41.400602
3511.950875	799115.097418	41.405607
3511.802267	798929.682665	41.410612
3511.876729	798743.833545	41.415616
3511.380829	798553.017426	41.420621
3511.237514	798364.150639	41.425626
3511.257834	798192.825968	41.430631
3511.300077	798014.375275	41.435636
3511.205850	797822.883922	41.440640
3510.867258	797650.721399	41.445645
3510.706843	797477.003341	41.450650
3510.565222	797313.293464	41.455655
3510.524235	797134.735815	41.460660
3510.487101	796966.974641	41.465664
3510.716118	796813.404483	41.470669
3510.255446	796648.798712	41.475674
3510.081894	796480.311830	41.480679
3510.013376	796320.642136	41.485684
3509.948964	796150.508945	41.490688
3509.736718	796007.060139	41.495693
3509.713018	795841.774159	41.500698
3509.658249	795688.668050	41.505703
3509.603920	795532.612018	41.510708
3509.512401	795382.353571	41.515712
3509.302113	795247.679516	41.520717
3509.452194	795093.691809	41.525722
3509.208686	794953.909986	41.530727
3508.642485	794797.234346	41.535732
3509.061969	794659.351117	41.540736
3508.828681	794528.547117	41.545741
3508.889762	794389.391514	41.550746
3508.383656	794247.330417	41.555751
3508.704277	794108.568568	41.560756
3508.888671	793972.380634	41.565760
3508.543478	793844.480393	41.570765
3508.649482	793717.485933	41.575770
3508.045712	793571.104608	41.580775
3507.980435	793439.466739	41.585780
3508.360525	793299.303714	41.590784
3507.753662	793184.354213	41.595789
3508.232439	793064.900953	41.600794
3508.096573	792932.921377	41.605799
3507.852371	792814.418118	41.610804
3508.044307	792681.151654	41.615808
3507.485833	792574.093904	41.620813
3507.352494	792449.375981	41.625818
3507.512886	792346.618073	41.630823
3507.129833	792233.040997	41.635828
3507.128125	792114.338652	41.640832
3507.303231	792004.940487	41.645837
3507.608975	791894.585568	41.650842
3507.486938	791779.484197	41.655847
3507.507959	791652.761410	41.660852
3507.373912	791534.660765	41.665856
3507.141220	791428.072490	41.670861
3507.441997	791310.240440	41.675866
3507.323984	791191.001251	41.680871
3507.098090	791083.571312	41.685876
3507.332194	790979.356371	41.690880
3507.105979	790879.589262	41.695885
3506.980316	790764.766841	41.700890
3506.889819	790663.844082	41.705895
3506.942596	790564.665438	41.710900
3506.880301	790449.385187	41.715904
3506.593564	790344.460407	41.720909
3506.624075	790245.428404	41.725914
3506.588087	790130.728387	41.730919
3506.475892	790045.723728	41.735924
3506.472996	789939.910722	41.740928
3506.306640	789848.916641	41.745933
3506.329607	789747.618130	41.750938
3506.148696	789648.022839	41.755943
3506.116802	789558.428224	41.760948
3506.302629	789459.851190	41.765952
3506.044422	789380.514956	41.770957
3506.137659	789281.016822	41.775962
3506.251826	789197.095223	41.780967
3505.851324	789103.770850	41.785972
3505.718877	789020.428475	41.790976
3505.771918	788934.547698	41.795981
3505.884741	788844.182938	41.800986
3505.925013	788753.189959	41.805991
3505.510075	788679.131367	41.810996
3506.052839	788588.594236	41.816000
3505.900061	788506.379799	41.821005
3505.349829	788414.250824	41.826010
3505.706686	788336.669645	41.831015
3505.374259	788250.106736	41.836020
3505.610211	788164.284869	41.841024
3505.447765	788084.328501	41.846029
3505.707242	787996.780137	41.851034
3505.339618	787921.476855	41.856039
3505.278476	787851.087643	41.861044
3505.651767	787771.432819	41.866048
3505.338653	787698.330510	41.871053
3505.311585	787609.251381	41.876058
3505.254716	787542.496520	41.881063
3504.969247	787465.011674	41.886068
3505.305617	787390.422625	41.891072
3505.004383	787302.908950	41.896077
3504.994444	787232.554372	41.901082
3505.182706	787168.115608	41.906087
3504.659427	787076.899081	41.911092
3504.843297	787009.657084	41.916096
3504.714858	786955.790435	41.921101
3504.692181	786884.844518	41.926106
3504.726309	786810.987571	41.931111
3504.755669	786759.355224	41.936116
3505.048320	786676.652991	41.941120
3504.702233	786614.706584	41.946125
3504.626021	786541.061708	41.951130
3504.567593	786469.822540	41.956135
3504.417731	786406.022665	41.961140
3504.449067	786337.373497	41.966144
3504.611772	786285.568252	41.971149
3504.501479	786236.167901	41.976154
3504.732395	786176.237093	41.981159
3504.616357	786104.561221	41.986164
3504.328216	786037.977934	41.991168
3504.400778	785981.218733	41.996173
3504.396985	785910.358399	42.001178
3504.317052	785858.983440	42.006183
3504.312619	785795.940984	42.011188
3504.508132	785728.340812	42.016192
3504.327662	785668.522699	42.021197
3504.257548	785610.751353	42.026202
3504.299338	785545.830351	42.031207
3504.034653	785500.777995	42.036212
3504.146930	785435.696853	42.041216
3503.579357	785385.185675	42.046221
3503.899661	785334.281997	42.051226
3503.444806	785290.390763	42.056231
3503.430871	785237.180839	42.061236
3503.947071	785188.506132	42.066240
3503.684168	785151.516823	42.071245
3503.561529	785092.127000	42.076250
3503.712211	785044.839408	42.081255
3503.227672	785004.836621	42.086260
3503.971925	784955.975232	42.091264
3503.492545	784911.741447	42.096269
3503.548240	784857.386055	42.101274
3503.288646	784816.361516	42.106279
3503.437279	784770.547937	42.111284
3503.558297	784730.050408	42.116288
3503.360379	784693.736601	42.121293
3503.148051	784648.276799	42.126298
3503.289532	784595.036520	42.131303
3503.200881	784554.916830	42.136308
3503.291540	784519.980960	42.141312
3502.859324	784482.229135	42.146317
3503.301111	784445.857890	42.151322
3503.338917	784407.192102	42.156327
3502.954754	784364.464009	42.161332
3502.952102	784320.246425	42.166336
3502.624515	784293.543228	42.171341
3502.904975	784249.524507	42.176346
3502.954977	784225.316562	42.181351
3502.960973	784191.475149	42.186356
3502.747856	784144.930182	42.191360
3502.789756	784114.082914	42.196365
3502.771719	784083.392949	42.201370
3503.056565	784046.750415	42.206375
3502.513914	784012.949347	42.211380
3502.621295	783979.090236	42.216384
3502.614814	783967.089436	42.221389
3502.554032	783929.421090	42.226394
3502.916791	783915.932911	42.231399
3502.624906	783883.073703	42.236404
3502.917640	783838.066666	42.241408
3502.829455	783815.503353	42.246413
3503.194071	783777.026297	42.251418
3503.154621	783730.843564	42.256423
3502.686338	783706.325723	42.261428
3503.212850	783669.739848	42.266432
3503.145146	783644.516337	42.271437
3502.979533	783599.042209	42.276442
3502.806039	783557.356821	42.281447
3502.488183	783540.044747	42.286452
3502.931825	783502.487847	42.291456
3502.765634	783468.327058	42.296461
3502.879252	783447.844602	42.301466
3502.907283	783402.140567	42.306471
3502.609578	783372.231523	42.311476
3502.863841	783349.315188	42.316480
3502.547966	783320.196003	42.321485
3502.467706	783285.626650	42.326490
3502.840522	783247.440579	42.331495
3502.692817	783237.773915	42.336500
3502.655620	783196.654311	42.341504
3502.389612	783166.985162	42.346509
3502.626506	783137.774190	42.351514
3502.731267	783105.928370	42.356519
3502.526975	783086.776308	42.361524
3502.764866	783050.185643	42.366528
3502.578529	783032.850685	42.371533
3502.483486	782985.786827	42.376538
3502.992401	782972.272817	42.381543
3502.662332	782940.202718	42.386548
3502.865062	782889.055151	42.391552
3502.440918	782873.972794	42.396557
3502.410992	782840.426130	42.401562
3502.752340	782819.264831	42.406567
3502.806555	782789.000221	42.411572
3502.613950	782753.118515	42.416576
3502.562163	782734.432364	42.421581
3502.327415	782712.184919	42.426586
3502.853506	782678.841102	42.431591
3502.755385	782663.507812	42.436596
3503.005113	782630.504478	42.441600
3502.966525	782596.712122	42.446605
3502.953471	782564.342144	42.451610
3502.979391	782511.400700	42.456615
3502.525506	782494.748097	42.461620
3502.890129	782469.301669	42.466624
3502.720822	782423.230350	42.471629
3502.750748	782398.133997	42.476634
3503.039108	782363.991503	42.481639
3503.269343	782331.826407	42.486644
3502.865254	782276.248090	42.491648
3502.797154	782245.755352	42.496653
3502.364042	782223.391472	42.501658
3502.650153	782192.003756	42.506663
3502.582023	782155.360567	42.511668
3502.534759	782139.279775	42.516672
3502.452493	782120.793860	42.521677
3502.298172	782093.758755	42.526682
3502.295162	782069.650711	42.531687
3502.363619	782058.569220	42.536692
3502.464067	782020.864350	42.541696
3502.555132	782002.595591	42.546701
3502.321792	781967.454718	42.551706
3502.608321	781947.825168	42.556711
3502.252424	781921.954275	42.561716
3502.266144	781888.149988	42.566720
3502.100210	781866.971060	42.571725
3501.808945	781851.766266	42.576730
3501.875028	781833.845616	42.581735
3501.853274	781833.898512	42.586740
3502.350752	781796.619106	42.591744
3502.315978	781768.136198	42.596749
3501.869742	781761.419729	42.601754
3502.466264	781736.473769	42.606759
3502.265750	781737.687795	42.611764
3502.212682	781705.615785	42.616768
3502.131467	781694.017146	42.621773
3502.075353	781661.994648	42.626778
3502.432980	781642.254152	42.631783
3502.100773	781627.449263	42.636788
3502.145397	781595.409877	42.641792
3502.185233	781593.779672	42.646797
3502.242668	781552.438302	42.651802
3502.126084	781547.143481	42.656807
3502.307112	781512.571808	42.661812
3502.406125	781490.413237	42.666816
3501.902933	781464.663377	42.671821
3501.876829	781445.871253	42.676826
3501.908658	781435.828161	42.681831
3501.909542	781420.820365	42.686836
3501.974949	781391.532179	42.691840
3501.756648	781380.890533	42.696845
3501.932124	781362.557050	42.701850
3502.127765	781364.542388	42.706855
3501.863058	781328.665483	42.711860
3501.985252	781323.232754	42.716864
3501.908160	781314.191564	42.721869
3501.861695	781289.399186	42.726874
3501.929611	781270.984775	42.731879
3501.744391	781264.028019	42.736884
3502.109618	781232.770738	42.741888
3501.897147	781228.623240	42.746893
3501.790644	781224.359872	42.751898
3501.782532	781189.719398	42.756903
3501.874823	781182.962890	42.761908
3502.430782	781151.969089	42.766912
3502.071540	781134.756468	42.771917
3501.938370	781132.416539	42.776922
3502.029851	781098.841798	42.781927
3501.837645	781089.425624	42.786932
3501.960909	781071.936544	42.791937
3501.978748	781045.262827	42.796941
3502.221705	781037.841659	42.801946
3502.168330	781021.562554	42.806951
3501.986667	781010.520659	42.811956
3501.722373	781001.411496	42.816961
3501.813446	780978.563746	42.821965
3501.634203	780962.551286	42.826970
3501.890043	780938.544465	42.831975
3502.046801	780940.093445	42.836980
3501.915919	780919.939360	42.841985
3501.727823	780908.209439	42.846989
3501.848311	780879.599042	42.851994
3501.919419	780857.000246	42.856999
3501.800907	780852.344958	42.862004
3501.794181	780837.780095	42.867009
3501.513170	780821.390407	42.872013
3501.451102	780817.956047	42.877018
3501.674321	780810.439478	42.882023
3501.587319	780817.392520	42.887028
3501.612030	780792.045408	42.892033
3502.163322	780779.209286	42.897037
3501.831963	780765.731165	42.902042
3501.910918	780745.591242	42.907047
3501.650048	780741.402225	42.912052
3501.691018	780722.400334	42.917057
3501.988771	780716.741393	42.922061
3501.483624	780699.502556	42.927066
3501.654068	780679.987121	42.932071
3501.682115	780687.413445	42.937076
3501.720759	780654.977200	42.942081
3501.822411	780648.710764	42.947085
3501.643629	780644.065269	42.952090
3501.684567	780630.328728	42.957095
3501.612897	780616.659920	42.962100
3501.532546	780588.425935	42.967105
3501.288823	780597.717941	42.972109
3501.373242	780586.582358	42.977114
3501.466589	780584.746267	42.982119
3501.691072	780584.118862	42.987124
3501.854834	780558.748031	42.992129
3501.685265	780562.319310	42.997133
3501.588293	780545.898684	43.002138
3501.921552	780529.161095	43.007143
3502.027601	780510.689261	43.012148
3502.143624	780492.757071	43.017153
3501.803319	780482.724743	43.022157
3501.650359	780477.435129	43.027162
3502.027910	780451.635011	43.032167
3501.630872	780437.232060	43.037172
3501.986102	780416.553592	43.042177
3502.215470	780408.198981	43.047181
3501.728359	780388.741861	43.052186
3502.178236	780378.579232	43.057191
3501.692134	780370.637705	43.062196
3501.785940	780329.627862	43.067201
3502.046743	780329.732653	43.072205
3501.736282	780325.354709	43.077210
3502.001432	780301.590316	43.082215
3501.939650	780307.506210	43.087220
3501.758966	780288.785761	43.092225
3501.850369	780261.850979	43.097229
3501.844477	780251.566392	43.102234
3501.982249	780236.878095	43.107239
3501.596916	780221.045583	43.112244
3502.130195	780204.520371	43.117249
3502.152892	780198.857121	43.122253
3501.843602	780178.681148	43.127258
3502.038464	780159.996937	43.132263
3501.784529	780160.629446	43.137268
3501.866801	780129.266382	43.142273
3501.960672	780120.441614	43.147277
3501.514989	780108.654396	43.152282
3501.785346	780090.695792	43.157287
3501.614374	780081.717741	43.162292
3501.789966	780067.121302	43.167297
3501.894956	780060.361659	43.172301
3501.964535	780038.449577	43.177306
3501.769354	780033.215808	43.182311
3501.517308	780005.549204	43.187316
3501.675867	779992.628745	43.192321
3501.788249	779986.409186	43.197325
3501.769110	779983.804024	43.202330
3501.694824	779959.749916	43.207335
3501.796261	779953.482917	43.212340
3501.867043	779942.791537	43.217345
3501.879991	779923.201580	43.222349
3501.740437	779903.144530	43.227354
3501.682593	779901.136306	43.232359
3501.743742	779890.692516	43.237364
3501.385880	779865.848132	43.242369
3501.606008	779858.774039	43.247373
3501.593400	779851.492192	43.252378
3501.822284	779848.107880	43.257383
3501.629121	779825.795487	43.262388
3501.379466	779811.465446	43.267393
3501.594636	779814.186250	43.272397
3501.716294	779813.477286	43.277402
3501.701065	779796.795416	43.282407
3501.841718	779793.720913	43.287412
3501.653022	779768.553030	43.292417
3501.957395	779767.863183	43.297421
3501.569115	779749.323188	43.302426
3501.743158	779726.310181	43.307431
3501.580112	779734.999388	43.312436
3501.833729	779715.664534	43.317441
3501.802863	779677.673808	43.322445
3501.679512	779688.177585	43.327450
3501.670252	779661.798554	43.332455
3501.822610	779649.469120	43.337460
3501.729757	779631.372339	43.342465
3501.891931	779629.278582	43.347469
3501.798462	779625.159776	43.352474
3501.951898	779585.760108	43.357479
3501.730625	779597.559821	43.362484
3501.543753	779581.693220	43.367489
3501.751811	779562.906866	43.372493
3501.870967	779558.162379	43.377498
3502.205864	779546.442543	43.382503
3501.793769	779524.854346	43.387508
3501.904717	779506.133060	43.392513
3502.075887	779507.040132	43.397517
3502.067456	779483.318132	43.402522
3502.103497	779456.783239	43.407527
3501.754052	779445.274401	43.412532
3501.754549	779425.635936	43.417537
3501.672761	779425.994053	43.422541
3501.890684	779413.456542	43.427546
3502.158308	779377.137760	43.432551
3501.969561	779377.808815	43.437556
3501.683830	779363.680710	43.442561
3501.871089	779333.035216	43.447565
3501.817320	779337.572418	43.452570
3501.829311	779320.737312	43.457575
3502.051786	779289.888956	43.462580
3502.085935	779283.829345	43.467585
3501.734460	779266.266457	43.472589
3501.575860	779245.718524	43.477594
3501.689168	779236.791042	43.482599
3501.767200	779237.615049	43.487604
3501.829563	779206.743493	43.492609
3501.984742	779188.506313	43.497613
3501.769679	779200.354865	43.502618
3502.142089	779168.644544	43.507623
3502.100698	779151.817840	43.512628
3501.682854	779144.159043	43.517633
3501.935318	779109.613389	43.522637
3501.719856	779105.760490	43.527642
3501.721357	779103.840713	43.532647
3501.493350	779080.842670	43.537652
3501.535496	779072.123595	43.542657
3501.731870	779060.278131	43.547661
3501.391203	779073.624233	43.552666
3501.713959	779046.056181	43.557671
3501.586327	779037.611139	43.562676
3501.721380	779017.260301	43.567681
3501.667428	779024.357277	43.572685
3501.537708	779018.422882	43.577690
3501.638146	778980.406886	43.582695
3501.779696	778973.689436	43.587700
3501.691670	778980.890512	43.592705
3501.898083	778956.442293	43.597709
3501.694282	778948.944922	43.602714
3501.878959	778928.733330	43.607719
3501.580091	778932.228257	43.612724
3501.722112	778907.839704	43.617729
3501.648560	778894.414078	43.622733
3501.709003	778903.953476	43.627738
3501.779598	778891.587005	43.632743
3501.656795	778870.933670	43.637748
3501.749594	778850.687773	43.642753
3501.929540	778847.754071	43.647757
3501.956266	778830.767735	43.652762
3501.982687	778809.351296	43.657767
3501.657083	778808.026779	43.662772
3501.844356	778792.687510	43.667777
3501.996446	778772.283958	43.672781
3501.647916	778771.455448	43.677786
3501.741962	778743.776255	43.682791
3501.488613	778733.087264	43.687796
3501.713680	778726.355831	43.692801
3501.973694	778721.784495	43.697805
3501.465577	778700.898801	43.702810
3501.515131	778683.563792	43.707815
3501.334349	778684.233596	43.712820
3501.471481	778686.820008	43.717825
3501.851063	778680.112305	43.722829
3501.248030	778654.664242	43.727834
3501.911286	778638.163305	43.732839
3501.737262	778636.419991	43.737844
3501.612745	778624.232879	43.742849
3501.916983	778601.244099	43.747853
3501.818532	778594.565833	43.752858
3502.090507	778589.155620	43.757863
3502.015323	778572.333144	43.762868
3501.504785	778556.419167	43.767873
3501.913991	778548.525059	43.772877
3501.796090	778531.857201	43.777882
3501.830099	778500.248941	43.782887
3501.679126	778511.841925	43.787892
3501.454768	778494.403908	43.792897
3501.832007	778471.353469	43.797901
3501.715706	778473.784799	43.802906
3501.848205	778456.977073	43.807911
3501.836260	778432.710744	43.812916
3501.754680	778416.775030	43.817921
3502.137166	778415.776841	43.822925
3501.847315	778404.305760	43.827930
3501.806698	778372.610786	43.832935
3501.766915	778372.912807	43.837940
3501.196313	778359.961880	43.842945
3501.679466	778331.330951	43.847949
3501.637601	778335.768362	43.852954
3501.947008	778322.229375	43.857959
3501.653940	778326.068221	43.862964
3501.616015	778312.143386	43.867969
3501.775415	778301.533454	43.872973
3501.876893	778290.637686	43.877978
3501.586884	778267.991874	43.882983
3501.522078	778250.773128	43.887988
3501.370806	778251.733473	43.892993
3501.447242	778240.300254	43.897997
3501.408507	778247.493935	43.903002
3501.365033	778247.845796	43.908007
3501.539619	778224.335685	43.913012
3501.414665	778211.507997	43.918017
3501.702827	778216.137257	43.923021
3501.744112	778210.026351	43.928026
3501.769194	778192.595752	43.933031
3501.783286	778172.902442	43.938036
3501.542808	778167.822468	43.943041
3501.575524	778162.303667	43.948045
3501.559623	778152.510040	43.953050
3501.342958	778130.590140	43.958055
3501.510277	778130.808829	43.963060
3501.638345	778113.213392	43.968065
3501.690005	778124.970526	43.973069
3501.574673	778101.803144	43.978074
3501.683605	778074.069730	43.983079
3501.529705	778078.033466	43.988084
3501.348185	778077.866561	43.993089
3501.730971	778061.410526	43.998093
3501.667716	778054.233681	44.003098
3501.910117	778040.803668	44.008103
3501.787761	778034.473426	44.013108
3501.485947	778016.997795	44.018113
3501.633444	777998.660448	44.023117
3501.874853	777990.645693	44.028122
3501.821690	777986.765464	44.033127
3501.708571	777964.483405	44.038132
3501.752473	777953.104325	44.043137
3501.791017	777948.864365	44.048141
3501.709486	777941.985795	44.053146
3502.023569	777919.731690	44.058151
3501.915409	777900.697766	44.063156
3501.987062	777882.815689	44.068161
3502.192165	777865.896185	44.073165
3501.998054	777862.629865	44.078170
3501.982334	777832.996101	44.083175
3502.227213	777821.682172	44.088180
3501.607181	777808.295329	44.093185
3501.841050	777786.595565	44.098189
3501.726590	777776.128441	44.103194
3501.605381	777766.105489	44.108199
3501.842352	777751.445076	44.113204
3501.541748	777738.005488	44.118209
3502.026396	777720.153447	44.123213
3502.015434	777713.312268	44.128218
3502.057896	777686.179101	44.133223
3501.704872	777684.661964	44.138228
3501.696925	777662.164733	44.143233
3501.897358	777637.319232	44.148237
3501.763403	777635.519844	44.153242
3501.713124	777626.617339	44.158247
3501.678523	777605.699732	44.163252
3501.424296	777586.885976	44.168257
3501.850800	777587.997395	44.173261
3501.239742	777603.409216	44.178266
3501.624379	777569.474514	44.183271
3501.749572	777554.930582	44.188276
3501.555808	777548.857840	44.193281
3501.677823	777542.388454	44.198285
3501.475125	777531.590889	44.203290
3502.134920	777516.417270	44.208295
3502.104902	777511.056008	44.213300
3501.791157	777484.916179	44.218305
3501.564981	777470.233026	44.223309
3501.470941	777471.873299	44.228314
3501.776162	777455.871773	44.233319
3502.067985	777439.626256	44.238324
3501.930234	777432.165673	44.243329
3502.031258	777421.957944	44.248333
3501.501256	777393.145598	44.253338
3501.550147	777370.293475	44.258343
3501.504502	777385.021821	44.263348
3501.434813	777384.984177	44.268353
3501.605387	777371.466301	44.273357
3501.625673	777358.367022	44.278362
3501.631124	777341.331491	44.283367
3502.025321	777342.152871	44.288372
3501.678717	777321.778177	44.293377
3501.817682	777305.606774	44.298381
3501.878937	777300.870361	44.303386
3502.029819	777279.035060	44.308391
3501.681093	777269.048901	44.313396
3501.851346	777257.647926	44.318401
3501.937742	777240.254188	44.323405
3501.471628	777218.668038	44.328410
3501.784844	777213.053084	44.333415
3501.861479	777208.166375	44.338420
3501.631233	777198.997587	44.343425
3501.717173	777167.621175	44.348429
3501.523834	777172.970464	44.353434
3501.706416	777162.453532	44.358439
3501.700922	777147.979553	44.363444
3501.812237	777134.569470	44.368449
3502.053429	777117.100708	44.373453
3501.718850	777103.616310	44.378458
3501.953980	777076.744555	44.383463
3501.862962	777073.805544	44.388468
3501.877820	777051.647324	44.393473
3502.079586	777024.780873	44.398477
3501.692423	777028.685127	44.403482
3501.963267	777005.746069	44.408487
3501.503508	776993.119093	44.413492
3501.816935	776991.098145	44.418497
3502.061230	776972.840755	44.423501
3501.677750	776956.163805	44.428506
3501.735214	776936.952379	44.433511
3501.741760	776935.868215	44.438516
3501.586519	776918.710459	44.443521
3501.840551	776888.634542	44.448525
3501.729587	776891.459407	44.453530
3501.730383	776880.824305	44.458535
3501.641268	776863.261635	44.463540
3501.540252	776857.862351	44.468545
3501.832318	776842.550968	44.473549
3501.622767	776846.376824	44.478554
3501.839684	776832.751848	44.483559
3502.085294	776819.023647	44.488564
3501.939248	776800.977835	44.493569
3502.049166	776772.402291	44.498573
3501.923595	776765.726815	44.503578
3502.119333	776754.517809	44.508583
3501.641066	776726.235918	44.513588
3501.471113	776724.196043	44.518593
3501.922964	776719.838055	44.523597
3501.604267	776697.290565	44.528602
3501.793285	776674.413187	44.533607
3501.431377	776674.620622	44.538612
3500.907442	776672.491326	44.543617
3501.235393	776676.179498	44.548621
3500.977482	776673.710956	44.553626
3501.214150	776671.899517	44.558631
3501.234312	776652.791966	44.563636
3501.107745	776635.234916	44.568641
3501.279273	776639.835159	44.573645
3501.477615	776640.984314	44.578650
3501.550067	776635.260863	44.583655
3501.121154	776645.031535	44.588660
3501.232165	776632.408393	44.593665
3501.268686	776633.190298	44.598669
3501.430651	776634.345445	44.603674
3501.358903	776595.360632	44.608679
3501.342457	776577.588352	44.613684
3500.934323	776585.878523	44.618689
3501.104616	776587.130783	44.623693
3501.459674	776584.315052	44.628698
3500.825517	776580.923683	44.633703
3501.474982	776582.047778	44.638708
3501.418929	776589.393657	44.643713
3501.151781	776592.441317	44.648717
3501.211053	776593.317955	44.653722
3501.148139	776574.863985	44.658727
3501.100068	776558.377070	44.663732
3501.204702	776549.546214	44.668737
3501.441832	776547.685430	44.673741
3501.595367	776542.047028	44.678746
3501.528452	776542.698264	44.683751
3501.450633	776541.283267	44.688756
3501.457625	776541.479180	44.693761
3501.394770	776509.238156	44.698765
3501.704973	776501.013488	44.703770
3501.553834	776488.728713	44.708775
3501.762800	776489.432990	44.713780
3501.454017	776489.040809	44.718785
3501.668700	776459.560483	44.723789
3501.771962	776464.221320	44.728794
3501.434304	776463.883133	44.733799
3501.327439	776459.518543	44.738804
3501.013094	776439.185310	44.743809
3501.388514	776418.886123	44.748813
3501.415337	776420.014325	44.753818
3501.098677	776411.991292	44.758823
3501.193982	776422.512986	44.763828
3501.360165	776411.406803	44.768833
3501.297902	776404.031213	44.773837
3501.184248	776396.910279	44.778842
3501.480322	776402.918110	44.783847
3501.167367	776406.564268	44.788852
3501.079136	776384.076329	44.793857
3501.374430	776373.982860	44.798861
3501.276926	776372.718791	44.803866
3501.282625	776378.134353	44.808871
3501.533389	776376.812920	44.813876
3501.303141	776385.911093	44.818881
3501.390238	776363.541931	44.823885
3501.177619	776374.951493	44.828890
3501.427229	776376.683124	44.833895
3501.972382	776339.220250	44.838900
3501.769292	776324.777190	44.843905
3501.888330	776325.102374	44.848909
3501.733514	776304.693249	44.853914
3501.548250	776287.046552	44.858919
3501.757748	776289.227976	44.863924
3501.557618	776277.147878	44.868929
3501.759913	776255.350298	44.873933
3501.823916	776257.211012	44.878938
3501.772429	776244.269283	44.883943
3501.684758	776238.867344	44.888948
3501.632907	776220.607621	44.893953
3502.005524	776206.512667	44.898957
3501.851391	776202.352674	44.903962
3501.734122	776165.490437	44.908967
3501.881346	776158.326300	44.913972
3501.453387	776154.260624	44.918977
3501.479327	776143.029412	44.923981
3501.709854	776128.022124	44.928986
3501.784338	776117.915434	44.933991
3501.890971	776109.970069	44.938996
3501.443002	776089.263939	44.944001
3501.745776	776069.468171	44.949005
3501.729735	776074.887538	44.954010
3501.382563	776069.725185	44.959015
3501.757506	776057.648484	44.964020
3501.460718	776039.083959	44.969025
3501.632650	776034.919404	44.974029
3501.355102	776021.768307	44.979034
3501.571266	776027.543399	44.984039
3501.300076	776007.694280	44.989044
3500.888549	775994.712929	44.994049
3501.592080	775979.135001	44.999053
3501.213125	775986.583914	45.004058
3501.281846	775977.709043	45.009063
3501.440398	775969.361034	45.014068
3501.317616	775969.873794	45.019073
3501.510838	775962.800375	45.024077
3501.580450	775961.705679	45.029082
3501.592451	775941.268063	45.034087
3501.769996	775935.772971	45.039092
3501.297839	775948.457017	45.044097
3501.850516	775932.854597	45.049101
3501.762664	775922.183461	45.054106
3501.759930	775901.895892	45.059111
3501.971319	775892.406501	45.064116
3501.639368	775874.290538	45.069121
3501.768904	775846.643776	45.074125
3501.662536	775854.244896	45.079130
3501.549388	775839.835307	45.084135
3501.439525	775827.296405	45.089140
3501.276789	775814.322997	45.094145
3501.387746	775806.672054	45.099149
3501.427564	775811.589977	45.104154
3501.339332	775808.994703	45.109159
3501.816044	775804.139647	45.114164
3501.687240	775791.603804	45.119169
3501.721210	775765.597524	45.124173
3501.665502	775770.137258	45.129178
3501.909367	775754.486839	45.134183
3501.874085	775725.143223	45.139188
3501.530787	775722.589932	45.144193
3501.670740	775709.812703	45.149197
3501.786724	775694.872643	45.154202
3501.818387	775681.817735	45.159207
3501.643117	775672.834951	45.164212
3501.645072	775672.834738	45.169217
3501.710029	775651.402699	45.174221
3501.655525	775651.510276	45.179226
3501.662692	775636.440286	45.184231
3501.999391	775623.285785	45.189236
3501.554131	775611.195719	45.194241
3501.695910	775589.455375	45.199245
3501.198683	775585.991731	45.204250
3501.397676	775593.001126	45.209255
3501.796752	775577.620236	45.214260
3501.536190	775549.494911	45.219265
3501.538891	775556.191956	45.224269
3501.677851	775534.156440	45.229274
3501.651293	775535.293572	45.234279
3501.783537	775511.043043	45.239284
3501.591441	775515.162188	45.244289
3501.656958	775493.532613	45.249293
3501.545265	775476.265809	45.254298
3501.330582	775465.368670	45.259303
3501.441426	775456.584722	45.264308
3501.579168	775447.156134	45.269313
3501.611389	775456.409207	45.274317
3501.881487	775449.273387	45.279322
3501.722870	775434.624259	45.284327
3501.672636	775418.479859	45.289332
3501.375009	775409.664645	45.294337
3501.688977	775408.775850	45.299341
3501.911957	775387.267765	45.304346
3501.673477	775381.446813	45.309351
3501.518914	775377.286420	45.314356
3501.541142	775368.418471	45.319361
3501.752154	775344.499144	45.324365
3501.606460	775342.553378	45.329370
3501.604259	775323.741527	45.334375
3501.802337	775321.049673	45.339380
3501.602101	775294.784820	45.344385
3502.064298	775267.573554	45.349389
3501.805197	775266.582147	45.354394
3501.524454	775255.991062	45.359399
3501.516192	775242.449475	45.364404
3501.753388	775237.879740	45.369409
3501.842802	775227.326137	45.374413
3501.578994	775215.205526	45.379418
3501.405199	775206.271174	45.384423
3501.887100	775193.879954	45.389428
3501.752467	775206.805165	45.394433
3501.980416	775169.290083	45.399437
3501.778156	775157.503974	45.404442
3501.500879	775154.053141	45.409447
3501.708431	775128.853231	45.414452
3501.688513	775117.972741	45.419457
3501.701307	775108.071816	45.424461
3501.644244	775112.710676	45.429466
3501.465949	775092.006549	45.434471
3501.802072	775065.701778	45.439476
3501.543261	775062.641848	45.444481
3501.827681	775058.261219	45.449485
3501.671171	775037.159360	45.454490
3501.558989	775028.460886	45.459495
3501.781324	775025.863427	45.464500
3501.832119	775018.714065	45.469505
3501.516200	775002.070772	45.474509
3501.793961	774973.214328	45.479514
3501.696234	774971.309810	45.484519
3501.990113	774955.206209	45.489524
3501.474353	774937.758448	45.494529
3501.449018	774925.302579	45.499533
3501.809658	774925.440283	45.504538
3502.023171	774915.013540	45.509543
3501.936466	774893.801271	45.514548
3501.558216	774895.291930	45.519553
3501.912187	774884.989758	45.524557
3501.838955	774868.798688	45.529562
3501.558871	774845.795881	45.534567
3501.930002	774841.450092	45.539572
3501.678238	774827.061344	45.544577
3501.567192	774812.403138	45.549581
3501.850505	774802.851246	45.554586
3501.736834	774799.668797	45.559591
3501.943001	774769.395082	45.564596
3501.268740	774762.857407	45.569601
3501.767655	774764.794616	45.574605
3501.846864	774752.419736	45.579610
3501.551348	774738.776784	45.584615
3501.811674	774721.988687	45.589620
3501.133636	774727.370337	45.594625
3501.619760	774713.795594	45.599629
3501.578845	774702.770194	45.604634
3501.407535	774677.680396	45.609639
3501.719335	774663.444755	45.614644
3501.579371	774674.992739	45.619649
3501.730156	774658.518049	45.624653
3501.863605	774641.898423	45.629658
3501.848038	774637.468456	45.634663
3501.527762	774623.189096	45.639668
3501.359251	774604.944568	45.644673
3501.665566	774597.063182	45.649677
3501.733620	774581.045213	45.654682
3501.897309	774583.825721	45.659687
3501.985471	774557.559978	45.664692
3501.463224	774547.007645	45.669697
3501.689624	774554.555296	45.674701
3501.926336	774533.436471	45.679706
3501.543425	774513.946472	45.684711
3501.846443	774495.082225	45.689716
3501.482573	774482.287348	45.694721
3501.645179	774481.817400	45.699725
3501.825127	774458.983869	45.704730
3501.460042	774448.356254	45.709735
3501.704113	774444.129667	45.714740
3501.672101	774444.726084	45.719745
3501.680509	774417.340161	45.724749
3501.656532	774411.630864	45.729754
3501.461001	774404.324466	45.734759
3501.578922	774391.991856	45.739764
3501.565837	774379.237524	45.744769
3501.558026	774368.600198	45.749773
3501.606397	774359.578966	45.754778
3501.340068	774350.954333	45.759783
3501.957552	774338.243826	45.764788
3501.495271	774323.248469	45.769793
3501.532894	774311.273726	45.774797
3501.793145	774306.010067	45.779802
3501.691889	774306.519393	45.784807
3501.527529	774270.246437	45.789812
3501.440168	774192.636162	45.794817
3501.375626	774081.429268	45.799821
3501.364612	773900.859038	45.804826
3501.190180	773668.541255	45.809831
3500.768425	773373.992467	45.814836
3500.366141	773044.403335	45.819841
3500.373394	772642.460742	45.824845
3500.217927	772188.693388	45.829850
3499.854021	771691.721755	45.834855
3499.678625	771110.327176	45.839860
3499.001298	770487.920158	45.844865
3498.624802	769816.669951	45.849869
3498.041378	769081.022596	45.854874
3497.540602	768295.157323	45.859879
3497.281816	767443.946561	45.864884
3496.489288	766542.879228	45.869889
3495.626744	765596.940223	45.874893
3495.060835	764591.552907	45.879898
3494.320312	763540.977009	45.884903
3493.486293	762431.219592	45.889908
3492.558706	761259.788006	45.894913
3492.034392	760025.141196	45.899917
3491.089305	758742.339646	45.904922
3489.616479	757416.313756	45.909927
3489.275248	756026.920143	45.914932
3487.932717	754587.661891	45.919937
3486.743440	753088.393746	45.924941
3485.809294	751555.050725	45.929946
3484.528833	749958.608858	45.934951
3483.774428	748305.904864	45.939956
3482.450594	746620.714236	45.944961
3481.164319	744847.687755	45.949965
3480.060972	743047.278312	45.954970
3478.599578	741193.439234	45.959975
3477.331913	739280.205509	45.964980
3475.897117	737327.491648	45.969985
3474.794877	735306.179374	45.974989
3473.420751	733254.149948	45.979994
3471.550274	731158.789579	45.984999
3470.540906	728997.896553	45.990004
3468.516639	726810.682016	45.995009
3467.069567	724559.738402	46.000013
3465.615967	722252.253238	46.005018
3463.865650	719913.922208	46.010023
3461.928601	717515.682611	46.015028
3460.124277	715098.326098	46.020033
3458.165303	712625.601225	46.025037
3456.674703	710106.299383	46.030042
3454.587475	707554.616146	46.035047
3452.840167	704948.561996	46.040052
3450.745652	702315.888934	46.045057
3448.896259	699621.233160	46.050061
3446.863798	696899.972002	46.055066
3444.598649	694130.505594	46.060071
3443.000790	691325.236494	46.065076
3440.937311	688489.003385	46.070081
3439.005618	685583.245617	46.075085
3436.951791	682649.685247	46.080090
3434.582164	679680.163709	46.085095
3432.886178	676664.971426	46.090100
3430.688925	673612.791254	46.095105
3428.616433	670511.672270	46.100109
3426.707088	667383.769676	46.105114
3424.214706	664208.428087	46.110119
3422.006243	660985.766462	46.115124
3419.645870	657745.782811	46.120129
3417.129788	654451.403178	46.125133
3415.194274	651130.696685	46.130138
3412.452910	647769.729113	46.135143
3409.997032	644371.591507	46.140148
3407.450084	640930.467221	46.145153
3404.949878	637468.869776	46.150157
3402.445801	633966.075534	46.155162
3399.857942	630439.894510	46.160167
3397.402783	626869.693179	46.165172
3394.640198	623275.856029	46.170177
3392.478448	619644.539252	46.175181
3389.758174	615982.578574	46.180186
3386.718801	612285.253157	46.185191
3384.113246	608553.471506	46.190196
3381.569053	604790.638050	46.195201
3378.669816	600994.496013	46.200205
3375.902714	597178.155938	46.205210
3373.124496	593344.349941	46.210215
3370.435224	589469.138676	46.215220
3367.599201	585558.720160	46.220225
3364.819123	581631.498825	46.225229
3361.990860	577665.157558	46.230234
3358.827657	573677.687251	46.235239
3355.986643	569647.936653	46.240244
3353.105332	565614.512219	46.245249
3350.473185	561540.814479	46.250253
3347.555426	557444.394968	46.255258
3344.202909	553330.517118	46.260263
3341.612675	549176.754422	46.265268
3338.539568	544997.868770	46.270273
3335.094967	540794.141296	46.275277
3332.094252	536569.270056	46.280282
3328.800837	532324.235909	46.285287
3325.902727	528062.765177	46.290292
3322.770248	523776.433272	46.295297
3319.850624	519463.600101	46.300301
3316.555445	515122.087590	46.305306
3313.345517	510770.670023	46.310311
3310.117153	506380.257111	46.315316
3306.795831	501984.025834	46.320321
3303.287118	497572.752415	46.325325
3299.788812	493138.218029	46.330330
3296.773585	488689.509758	46.335335
3293.578200	484217.080014	46.340340
3290.347628	479721.619042	46.345345
3286.715579	475226.390043	46.350349
3283.587084	470688.004284	46.355354
3280.109031	466148.500654	46.360359
3276.891488	461581.801444	46.365364
3273.282513	457017.118282	46.370369
3269.762652	452432.442103	46.375373
3266.551723	447821.357752	46.380378
3262.696007	443211.017099	46.385383
3259.288866	438564.886343	46.390388
3255.523328	433939.482688	46.395393
3252.388256	429277.527318	46.400397
3249.028543	424611.098052	46.405402
3245.328283	419938.561361	46.410407
3241.767043	415233.019837	46.415412
3238.410894	410532.745075	46.420417
3234.647687	405818.561241	46.425421
3231.155955	401093.627573	46.430426
3227.321448	396351.434200	46.435431
3223.997228	391596.001335	46.440436
3220.230467	386857.906792	46.445441
3216.488779	382097.475094	46.450445
3213.133935	377318.731786	46.455450
3209.089893	372534.410039	46.460455
3205.448535	367741.099479	46.465460
3201.914298	362951.997252	46.470465
3197.968110	358157.780026	46.475469
3194.418710	353348.316113	46.480474
3190.263554	348535.802580	46.485479
3186.835556	343715.923935	46.490484
3182.649734	338885.489213	46.495489
3179.156567	334059.096696	46.500493
3175.437469	329231.123165	46.505498
3171.729301	324399.800423	46.510503
3167.864052	319563.553800	46.515508
3164.019172	314736.001292	46.520513
3160.221399	309895.475464	46.525517
3156.453470	305046.027555	46.530522
3152.463267	300207.765151	46.535527
3148.751291	295355.068936	46.540532
3144.711197	290510.321638	46.545537
3140.679725	285663.157222	46.550541
3137.058476	280821.355479	46.555546
3132.963301	275977.271800	46.560551
3129.303495	271134.043870	46.565556
3125.301274	266280.545288	46.570561
3121.147996	261442.214960	46.575565
3117.280128	256595.527125	46.580570
3112.653946	251766.964694	46.585575
3109.248728	246952.688606	46.590580
3104.850433	242132.029027	46.595585
3101.107068	237312.865979	46.600589
3097.216501	232507.760808	46.605594
3093.662842	227700.107359	46.610599
3089.555473	222876.711273	46.615604
3085.227139	218081.597748	46.620609
3081.285668	213290.246659	46.625613
3077.404377	208499.046491	46.630618
3073.086626	203630.878030	46.635623
3069.192512	198858.289232	46.640628
3064.823075	194088.130864	46.645633
3060.433358	189318.457829	46.650637
3056.691319	184563.782458	46.655642
3052.182661	179842.377761	46.660647
3048.085319	175108.467653	46.665652
3043.938370	170385.845437	46.670657
3040.019762	165694.598586	46.675661
3035.792189	161001.940188	46.680666
3031.594403	156315.865077	46.685671
3027.397567	151651.494828	46.690676
3023.224113	146997.234868	46.695681
3018.849458	142346.850640	46.700685
3014.841195	137707.517178	46.705690
3010.266831	133107.571596	46.710695
3006.248251	128496.211216	46.715700
3001.901593	123908.169345	46.720705
2997.277049	119342.092004	46.725709
2993.382914	114798.487016	46.730714
2988.836086	110251.345821	46.735719
2984.289043	105740.188137	46.740724
2979.758505	101250.385237	46.745729
2975.401045	96781.891221	46.750733
2970.387181	92326.719458	46.755738
2966.005595	87901.503097	46.760743
2961.278384	83506.757332	46.765748
2957.032854	79129.958662	46.770753
2952.182446	74786.355144	46.775757
2947.785100	70462.651929	46.780762
2942.287921	66183.944743	46.785767
2937.336422	61923.899661	46.790772
2931.695758	57716.076285	46.795777
2926.597158	53552.847625	46.800781
2920.911605	49429.533073	46.805786
2914.607868	45367.291910	46.810791
2904.956790	41465.181868	46.815796
2890.914992	37758.128159	46.820801
2877.304546	34184.163920	46.825805
2864.208133	30793.863271	46.830810
2851.786539	27593.489216	46.835815
2839.906835	24571.034784	46.840820
2828.542644	21761.306194	46.845825
2817.388023	19132.312212	46.850829
2807.246394	16701.453010	46.855834
2797.347560	14465.692897	46.860839
2788.001694	12381.515600	46.865844
2778.971429	10483.142714	46.870849
2770.429295	8745.513899	46.875853
2760.985006	7194.049568	46.880858
2750.057399	5836.918345	46.885863
2738.592332	4676.954622	46.890868
2727.411095	3676.105343	46.895873
2717.177568	2839.272396	46.900877
2709.045635	2143.504435	46.905882
2701.819015	1588.999933	46.910887
2695.801399	1130.988845	46.915892
2690.867823	766.390317	46.920897
2686.127677	488.832522	46.925901
2682.318004	248.517128	46.930906
2678.102071	92.991686	46.935911
2665.470772	228.058869	46.940916
2661.577407	230.172417	46.945921
2660.824409	242.739069	46.950925
2661.865454	232.675698	46.955930
2661.730125	242.729264	46.960935
2660.922776	239.930019	46.965940
2659.188042	229.662700	46.970945
2656.244684	232.586285	46.975949
2653.677155	228.686155	46.980954
2650.636248	216.343130	46.985959
2647.501988	215.186942	46.990964
2644.348666	222.998023	46.995969
2641.228878	217.558210	47.000973
2638.479619	222.192324	47.005978
2635.014879	227.737437	47.010983
2632.130666	223.212330	47.015988
2628.868674	217.263109	47.020993
2625.721847	227.037737	47.025997
2622.853829	222.715671	47.031002
2619.620062	221.999447	47.036007
2616.618144	221.673574	47.041012
2613.178437	217.823345	47.046017
2609.597227	224.593194	47.051021
2606.327243	204.395394	47.056026
2603.198114	213.097041	47.061031
2599.827612	211.591501	47.066036
2597.008678	214.996667	47.071041
2592.905245	222.416665	47.076045
2589.958934	212.856264	47.081050
2586.383425	212.064693	47.086055
2583.094401	223.355302	47.091060
2579.758962	213.374254	47.096065
2576.411312	206.045225	47.101069
2572.862745	218.068062	47.106074
2569.905700	214.002613	47.111079
2566.090475	218.298597	47.116084
2562.767493	201.797366	47.121089
2559.391328	216.448878	47.126093
2555.654629	208.327051	47.131098
2552.616751	214.278529	47.136103
2549.329497	213.427408	47.141108
2546.023740	212.706807	47.146113
2542.167397	216.447814	47.151117
2539.415232	196.617629	47.156122
2535.926429	202.075282	47.161127
2532.003338	211.762064	47.166132
2528.694457	197.428650	47.171137
2525.585594	206.632211	47.176141
2521.996131	208.582550	47.181146
2517.856492	203.052382	47.186151
2514.212864	211.376872	47.191156
2511.623796	196.511391	47.196161
2508.228952	202.193995	47.201165
2504.618156	194.909485	47.206170
2501.186804	205.020819	47.211175
2497.473278	203.147556	47.216180
2494.441696	203.053442	47.221185
2491.060645	206.711655	47.226189
2487.501665	195.389554	47.231194
2483.614684	200.834848	47.236199
2480.406291	192.858890	47.241204
2477.519048	190.111018	47.246209
2473.740520	200.457589	47.251213
2470.145063	193.145214	47.256218
2466.235535	199.900780	47.261223
2462.854185	192.454542	47.266228
2459.920660	189.763639	47.271233
2455.770011	200.012048	47.276237
2452.498596	198.895333	47.281242
2449.744899	197.672527	47.286247
2445.777726	199.747242	47.291252
2442.410720	195.186902	47.296257
2438.905442	198.272973	47.301261
2435.589426	198.958037	47.306266
2431.851513	197.286544	47.311271
2428.150324	191.912922	47.316276
2425.287668	186.531549	47.321281
2421.694183	190.993079	47.326285
2418.223004	177.851679	47.331290
2414.628519	188.885662	47.336295
2410.643357	199.502720	47.341300
2407.624032	185.647690	47.346305
2403.637053	194.718366	47.351309
2400.812719	183.909948	47.356314
2397.343769	188.882132	47.361319
2393.984108	191.661746	47.366324
2390.403644	193.397258	47.371329
2386.826521	191.992784	47.376333
2383.720016	188.431949	47.381338
2380.002339	190.094197	47.386343
2376.300127	186.503448	47.391348
2372.577757	193.077338	47.396353
2369.090225	203.115994	47.401357
2365.615458	187.569697	47.406362
2362.427200	193.881374	47.411367
2358.744797	192.573499	47.416372
2355.296098	185.915468	47.421377
2352.206485	191.706829	47.426381
2348.765224	179.500068	47.431386
2345.013714	187.619927	47.436391
2341.081518	189.749305	47.441396
2337.926249	185.671074	47.446401
2334.342175	192.898579	47.451405
2331.166618	176.497911	47.456410
2327.520265	182.321505	47.461415
2323.937834	183.768497	47.466420
2320.322021	187.737694	47.471425
2316.430920	188.941197	47.476429
2313.549315	185.027693	47.481434
2310.250314	192.819090	47.486439
2306.553903	184.268810	47.491444
2303.175127	181.090628	47.496449
2299.286543	178.097357	47.501453
2296.273166	183.315975	47.506458
2292.604390	188.241145	47.511463
2289.297679	193.656136	47.516468
2285.703478	182.789662	47.521473
2282.028773	186.693902	47.526477
2278.637003	171.748339	47.531482
2275.190678	184.257254	47.536487
2271.663133	179.049639	47.541492
2268.758365	179.803591	47.546497
2264.391788	194.465987	47.551501
2261.065281	179.766275	47.556506
2257.909109	180.054588	47.561511
2253.704809	177.031033	47.566516
2250.525108	177.253280	47.571521
2246.988553	188.230214	47.576525
2243.748945	179.941948	47.581530
2240.297843	179.751480	47.586535
2236.898350	177.309883	47.591540
2233.534745	179.670517	47.596545
2229.704165	180.548669	47.601549
2226.302814	176.613981	47.606554
2222.663767	181.020756	47.611559
2218.991991	180.408226	47.616564
2215.912281	179.266412	47.621569
2212.646866	181.411372	47.626573
2208.713947	180.885526	47.631578
2205.097182	174.681211	47.636583
2202.025676	178.855573	47.641588
2198.591140	181.973389	47.646593
2194.699784	182.088293	47.651597
2191.082447	178.117423	47.656602
2187.652899	180.467642	47.661607
2183.873938	183.057127	47.666612
2180.934559	174.697179	47.671617
2177.520485	181.192573	47.676621
2174.129633	178.768129	47.681626
2170.481700	182.848253	47.686631
2166.659363	184.346431	47.691636
2163.391612	179.392887	47.696641
2159.634214	186.358300	47.701645
2156.233204	169.922120	47.706650
2152.629700	176.838667	47.711655
2149.404142	176.867947	47.716660
2146.054328	174.369068	47.721665
2142.012614	176.454256	47.726669
2138.289097	169.635283	47.731674
2135.384283	167.246811	47.736679
2132.246262	173.257161	47.741684
2128.726538	165.835911	47.746689
2125.035560	181.578518	47.751693
2121.482975	184.275820	47.756698
2117.724481	181.309632	47.761703
2114.190489	166.542036	47.766708
2111.226746	163.190914	47.771713
2107.276250	165.486606	47.776717
2104.075835	163.729586	47.781722
2100.476032	164.851703	47.786727
2096.458931	179.602822	47.791732
2093.365215	167.352411	47.796737
2089.609564	170.401001	47.801741
2086.766923	174.228555	47.806746
2082.848384	178.645581	47.811751
2079.365208	168.204300	47.816756
2075.810186	164.322566	47.821761
2072.465735	174.427489	47.826765
2069.010031	160.116037	47.831770
2065.620028	166.637590	47.836775
2061.642789	168.051663	47.841780
2058.259185	172.549462	47.846785
2054.978603	178.355455	47.851789
2051.566842	163.488614	47.856794
2047.822841	170.476918	47.861799
2044.207065	164.686407	47.866804
2040.901832	148.986403	47.871809
2036.970544	167.359542	47.876813
2033.933986	146.028575	47.881818
2030.790588	169.481911	47.886823
2026.896277	166.869969	47.891828
2023.511428	167.328603	47.896833
2019.805243	165.850693	47.901837
2016.694006	160.001240	47.906842
2013.090237	154.581404	47.911847
2009.058959	162.783158	47.916852
2006.168154	157.664419	47.921857
2002.242209	164.877112	47.926861
1999.086610	157.685039	47.931866
1995.544586	157.993902	47.936871
1991.871477	160.320552	47.941876
1988.420804	157.561653	47.946881
1984.726090	164.043032	47.951885
1981.068583	163.446028	47.956890
1977.988888	154.464110	47.961895
1974.393885	162.851605	47.966900
1971.144138	161.704701	47.971905
1967.336161	159.218055	47.976909
1964.003859	159.079449	47.981914
1960.333635	167.250769	47.986919
1956.583899	160.355628	47.991924
1953.789326	158.118050	47.996929
1950.224857	161.831202	48.001933
1946.569222	167.149282	48.006938
1942.755310	170.381883	48.011943
1939.367438	164.318631	48.016948
1935.786108	161.569275	48.021953
1932.298557	165.615645	48.026957
1928.869749	158.654158	48.031962
1925.481452	159.512775	48.036967
1922.109400	157.868705	48.041972
1918.659606	160.296769	48.046977
1915.034685	171.196932	48.051981
1911.068071	154.308950	48.056986
1907.728900	156.221924	48.061991
1904.060663	147.981878	48.066996
1900.667130	155.340401	48.072001
1897.502964	161.622706	48.077005
1894.298288	158.218296	48.082010
1890.705197	158.510279	48.087015
1886.920336	155.175446	48.092020
1883.469794	155.234660	48.097025
1879.636349	158.103109	48.102029
1876.343182	161.563070	48.107034
1872.653246	153.004105	48.112039
1869.236548	157.614384	48.117044
1866.342284	155.644080	48.122049
1862.306048	163.035450	48.127053
1858.666834	170.733563	48.132058
1855.287896	155.125643	48.137063
1851.815866	158.466642	48.142068
1848.527523	148.169374	48.147073
1844.862855	154.754674	48.152077
1841.642826	164.013470	48.157082
1837.896982	151.793061	48.162087
1834.100024	167.610459	48.167092
1830.852573	159.229400	48.172097
1827.377925	152.618768	48.177101
1823.979296	147.423580	48.182106
1820.296067	155.886266	48.187111
1816.640444	158.013192	48.192116
1813.678102	168.032565	48.197121
1809.833722	164.158755	48.202125
1806.352938	156.016091	48.207130
1802.740634	148.051704	48.212135
1799.225873	160.088031	48.217140
1796.036897	149.631638	48.222145
1791.996096	156.562071	48.227149
1788.789226	157.536732	48.232154
1785.595756	156.184496	48.237159
1782.320382	163.472763	48.242164
1778.377764	142.314744	48.247169
1774.848153	150.335269	48.252173
1771.352078	161.146049	48.257178
1767.854639	155.876720	48.262183
1763.946517	158.620709	48.267188
1761.004322	152.752077	48.272193
1757.326540	147.328910	48.277197
1753.708232	142.135280	48.282202
1750.383624	149.493635	48.287207
1746.354111	152.425873	48.292212
1743.456170	139.792449	48.297217
1739.732884	149.645951	48.302221
1736.392432	146.241232	48.307226
1732.886175	140.942010	48.312231
1729.561032	155.573059	48.317236
1726.211100	147.686973	48.322241
1722.033392	159.993232	48.327245
1718.750538	157.082370	48.332250
1715.547042	146.703005	48.337255
1711.745262	149.950685	48.342260
1708.399062	144.401703	48.347265
1704.584825	152.980863	48.352269
1701.219757	146.504650	48.357274
1697.648995	151.391704	48.362279
1693.932549	155.091276	48.367284
1691.020324	150.684781	48.372289
1687.366154	147.526603	48.377293
1684.037827	137.892604	48.382298
1680.864138	143.924285	48.387303
1676.715573	159.643376	48.392308
1673.264313	157.648349	48.397313
1669.607298	154.838122	48.402317
1665.885463	151.717265	48.407322
1662.647905	148.398504	48.412327
1659.423486	144.343463	48.417332
1655.932392	142.819996	48.422337
1652.405153	153.571434	48.427341
1648.917550	144.146744	48.432346
1645.634114	142.530117	48.437351
1641.483864	142.389103	48.442356
1638.164606	138.738042	48.447361
1634.674576	139.770643	48.452365
1631.212688	154.376339	48.457370
1628.146623	150.339675	48.462375
1623.942911	146.803193	48.467380
1621.202871	137.529335	48.472385
1617.165270	143.449950	48.477389
1613.810849	136.524912	48.482394
1610.431589	139.158522	48.487399
1606.555856	144.648623	48.492404
1603.149507	135.650079	48.497409
1599.909635	145.037815	48.502413
1595.974124	138.983933	48.507418
1592.844537	132.864741	48.512423
1589.151244	133.983294	48.517428
1585.844733	136.229811	48.522433
1582.098207	148.364242	48.527437
1578.881514	143.086084	48.532442
1575.423167	145.423468	48.537447
1571.578695	143.484306	48.542452
1568.261484	139.017237	48.547457
1564.940369	134.038780	48.552461
1561.330984	143.605404	48.557466
1557.984104	138.912672	48.562471
1554.161226	142.562489	48.567476
1550.561961	135.919012	48.572481
1546.812331	138.503471	48.577485
1543.228133	139.348026	48.582490
1540.111850	146.333783	48.587495
1536.578363	140.549227	48.592500
1533.539376	140.181873	48.597505
1529.546085	145.036323	48.602509
1526.207111	152.115172	48.607514
1522.938950	144.279537	48.612519
1518.812465	144.214192	48.617524
1515.573182	141.985468	48.622529
1511.952497	141.459288	48.627533
1508.794717	147.463845	48.632538
1505.335636	140.254638	48.637543
1501.733975	149.754308	48.642548
1498.213735	147.815151	48.647553
1494.680329	141.393965	48.652557
1490.952496	136.056465	48.657562
1487.729514	127.269246	48.662567
1484.213899	141.345370	48.667572
1481.233352	134.379719	48.672577
1476.992649	151.986225	48.677581
1473.616785	147.273851	48.682586
1470.040815	137.393848	48.687591
1466.446754	144.015606	48.692596
1463.097597	147.560059	48.697601
1459.610237	142.882077	48.702605
1456.399717	139.397456	48.707610
1452.819970	136.007021	48.712615
1448.888250	138.449324	48.717620
1445.270903	132.022391	48.722625
1441.915527	143.901810	48.727629
1438.348738	138.610176	48.732634
1435.080626	129.684420	48.737639
1431.380913	139.278334	48.742644
1428.305951	132.366374	48.747649
1424.982439	125.640368	48.752653
1421.174520	135.787560	48.757658
1417.859721	123.298896	48.762663
1414.084908	133.688650	48.767668
1410.511391	138.952961	48.772673
1406.686764	137.818035	48.777677
1403.340083	135.613506	48.782682
1400.253825	131.115611	48.787687
1396.210953	134.653039	48.792692
1392.861455	137.257367	48.797697
1389.543104	137.385177	48.802701
1386.129369	142.001485	48.807706
1382.942692	130.689791	48.812711
1378.790795	130.629414	48.817716
1375.585559	130.835935	48.822721
1371.845521	143.834408	48.827725
1368.534597	140.136232	48.832730
1365.362588	137.545257	48.837735
1361.680463	142.619941	48.842740
1358.110649	136.395451	48.847745
1354.820637	134.919553	48.852749
1351.202338	126.569599	48.857754
1347.643023	123.162040	48.862759
1343.812434	142.918135	48.867764
1340.402844	131.012539	48.872769
1337.159716	142.102555	48.877773
1333.377376	135.629023	48.882778
1330.051606	138.314507	48.887783
1326.471827	144.055027	48.892788
1323.212139	140.519787	48.897793
1319.526769	137.693127	48.902797
1315.728384	136.091018	48.907802
1312.932124	123.236049	48.912807
1308.698974	138.277842	48.917812
1305.296035	125.437476	48.922817
1302.052731	142.829099	48.927821
1298.249310	135.523733	48.932826
1295.396169	131.651674	48.937831
1291.494663	142.367547	48.942836
1287.729874	137.136011	48.947841
1284.403134	133.110382	48.952845
1280.700567	127.032755	48.957850
1277.608229	125.906467	48.962855
1274.121428	139.726923	48.967860
1270.790517	125.054849	48.972865
1266.959778	137.988121	48.977869
1263.341806	133.956018	48.982874
1260.048736	139.381386	48.987879
1256.280014	138.874842	48.992884
1252.990159	131.434419	48.997889
1249.310628	130.815782	49.002893
1245.737451	133.203154	49.007898
1242.229796	134.426700	49.012903
1239.007221	135.009270	49.017908
1235.627214	116.209602	49.022913
1232.051538	139.673134	49.027917
1228.288543	128.182199	49.032922
1224.974032	126.120339	49.037927
1221.114987	133.325996	49.042932
1218.121101	130.306817	49.047937
1214.985057	133.292918	49.052941
1210.633337	133.639243	49.057946
1207.371971	126.889582	49.062951
1203.665934	129.887399	49.067956
1200.592602	125.460280	49.072961
1196.821713	126.949676	49.077965
1193.480852	126.359911	49.082970
1189.842841	121.568143	49.087975
1186.203067	134.498434	49.092980
1183.094637	122.844824	49.097985
1179.285689	122.663826	49.102989
1175.968820	129.747050	49.107994
1172.654951	125.956235	49.112999
1169.020522	140.639787	49.118004
1165.408174	127.761959	49.123009
1162.027308	125.097829	49.128013
1158.186701	125.724056	49.133018
1154.889678	126.462600	49.138023
1151.444143	120.605545	49.143028
1147.844939	126.737861	49.148033
1144.219998	128.943715	49.153037
1140.985258	122.897763	49.158042
1137.683495	114.609542	49.163047
1133.896834	122.612377	49.168052
1129.977026	123.274386	49.173057
1126.909380	118.926970	49.178061
1123.043151	125.341440	49.183066
1119.932572	119.280035	49.188071
1116.101218	127.669399	49.193076
1112.714908	119.922768	49.198081
1109.585037	119.772163	49.203085
1105.876229	125.192034	49.208090
1102.313515	125.286330	49.213095
1098.664983	140.262092	49.218100
1095.196919	134.576993	49.223105
1091.397834	128.278044	49.228109
1088.156774	129.754021	49.233114
1084.887111	117.354602	49.238119
1081.397984	129.069955	49.243124
1077.793741	123.341350	49.248129
1074.485167	123.967595	49.253133
1070.918608	130.052037	49.258138
1067.516676	115.039030	49.263143
1063.858684	123.293936	49.268148
1060.202023	121.622603	49.273153
1056.989659	124.467859	49.278157
1053.159458	126.772365	49.283162
1049.763455	126.730149	49.288167
1045.739753	124.611926	49.293172
1042.270407	118.126668	49.298177
1039.361813	122.244084	49.303181
1035.818202	117.910576	49.308186
1032.474138	126.175034	49.313191
1028.700460	117.623629	49.318196
1025.262430	121.967765	49.323201
1022.048663	126.303981	49.328205
1017.778920	118.634892	49.333210
1014.713614	116.289299	49.338215
1011.139712	113.844472	49.343220
1007.470450	128.284123	49.348225
1004.508344	124.832020	49.353229
1000.641187	119.735067	49.358234
997.495797	118.378228	49.363239
993.468101	123.493860	49.368244
990.210486	115.581916	49.373249
986.596555	127.544329	49.378253
983.238050	121.253607	49.383258
980.033504	116.319857	49.388263
976.496554	122.487059	49.393268
973.217330	124.537064	49.398273
969.310892	109.268242	49.403277
965.603986	121.440365	49.408282
961.968367	123.565893	49.413287
958.251847	126.640446	49.418292
954.764453	116.454228	49.423297
951.608517	118.055912	49.428301
948.238901	124.811811	49.433306
944.845338	119.192245	49.438311
941.113358	119.460981	49.443316
937.724043	125.258130	49.448321
934.244516	116.284901	49.453325
930.530895	112.817717	49.458330
927.274250	121.257400	49.463335
923.809546	116.121965	49.468340
920.394880	109.042124	49.473345
916.657007	125.288599	49.478349
912.932615	124.597345	49.483354
909.528722	106.329185	49.488359
906.271688	122.206312	49.493364
902.798416	122.028646	49.498369
898.914369	130.872155	49.503373
895.369944	116.706183	49.508378
892.255189	101.796142	49.513383
888.334383	112.821501	49.518388
885.063960	115.915563	49.523393
881.782002	124.235630	49.528397
877.889802	118.087454	49.533402
874.979476	125.614617	49.538407
870.703234	119.791202	49.543412
867.383995	119.920694	49.548417
864.070115	116.836925	49.553421
860.966815	120.370446	49.558426
857.817609	119.322608	49.563431
853.946040	131.461696	49.568436
850.256222	114.245506	49.573441
846.683632	124.706295	49.578445
843.011429	119.986971	49.583450
839.433704	117.456447	49.588455
835.583882	120.346092	49.593460
831.938383	119.759654	49.598465
829.289036	128.595343	49.603469
825.389865	126.460343	49.608474
822.152527	117.924986	49.613479
818.873385	120.412101	49.618484
815.044871	120.076984	49.623489
811.588831	124.760812	49.628493
808.052149	131.701523	49.633498
804.460928	122.989609	49.638503
800.839447	134.760081	49.643508
797.532185	121.494126	49.648513
793.973791	117.699202	49.653517
790.064216	122.918366	49.658522
787.079470	110.832975	49.663527
783.815582	131.594808	49.668532
780.457553	127.642394	49.673537
776.689722	123.813892	49.678541
773.217145	116.260375	49.683546
769.564339	104.541633	49.688551
765.951583	121.661431	49.693556
762.395225	124.738840	49.698561
758.900697	120.438820	49.703565
755.426470	126.181704	49.708570
752.187850	120.292878	49.713575
748.231370	117.590543	49.718580
744.964301	126.334998	49.723585
741.749348	127.659136	49.728589
737.824152	121.330529	49.733594
734.571680	116.747361	49.738599
730.903231	117.956184	49.743604
727.507075	121.112914	49.748609
723.971521	120.298930	49.753613
720.405552	120.186983	49.758618
716.997844	112.648441	49.763623
713.135309	118.425773	49.768628
709.803401	126.633107	49.773633
706.255379	120.913792	49.778637
702.947516	128.126544	49.783642
699.879855	120.475418	49.788647
695.850399	127.341878	49.793652
692.010811	125.012632	49.798657
689.018684	119.639164	49.803661
685.024372	111.915163	49.808666
682.008000	110.952319	49.813671
678.331843	118.489710	49.818676
674.769374	116.586684	49.823681
671.557825	116.817665	49.828685
668.054967	117.041215	49.833690
664.562400	106.744658	49.838695
661.170049	118.285940	49.843700
657.388192	115.962671	49.848705
653.884463	113.780919	49.853709
649.868543	131.547753	49.858714
647.124469	115.694540	49.863719
643.543158	110.498615	49.868724
640.060330	110.538625	49.873729
636.320406	117.907505	49.878733
632.804566	121.439015	49.883738
629.483279	111.102943	49.888743
625.963913	118.107959	49.893748
622.360622	111.825813	49.898753
618.918184	111.829270	49.903757
615.071967	124.548618	49.908762
611.572806	110.830772	49.913767
608.235572	118.878017	49.918772
604.902809	111.444368	49.923777
601.388811	107.876536	49.928781
597.425870	113.331920	49.933786
594.252887	113.179898	49.938791
590.946841	105.373661	49.943796
587.390430	108.561759	49.948801
584.332117	109.882986	49.953805
579.990691	120.273755	49.958810
576.956782	116.346651	49.963815
573.710592	112.618974	49.968820
570.161829	102.680219	49.973825
566.351429	108.393568	49.978829
562.388230	108.424763	49.983834
559.133391	107.178559	49.988839
555.543342	117.208261	49.993844
552.178539	117.468757	49.998849
549.051159	112.057129	50.003853
545.594235	122.318792	50.008858
542.298152	101.160795	50.013863
538.117714	97.411549	50.018868
534.113880	110.400934	50.023873
531.404694	103.384158	50.028877
527.702488	112.070437	50.033882
524.725274	102.045298	50.038887
520.894520	104.130281	50.043892
517.095305	101.117297	50.048897
513.976821	106.717175	50.053901
510.414600	106.571772	50.058906
506.629238	106.758312	50.063911
502.999294	108.671720	50.068916
499.646422	106.339448	50.073921
496.308444	95.457990	50.078925
492.527023	103.744489	50.083930
488.951124	106.605948	50.088935
485.741706	111.278589	50.093940
481.997321	110.509592	50.098945
479.048032	112.807221	50.103949
475.198187	107.781838	50.108954
472.357599	101.985673	50.113959
468.054892	105.832319	50.118964
464.796327	120.790951	50.123969
461.079262	112.270727	50.128973
457.399817	106.848825	50.133978
454.257361	107.079056	50.138983
450.595851	110.529747	50.143988
447.067763	108.487689	50.148993
443.932806	94.126947	50.153997
440.213772	106.073292	50.159002
436.629352	101.437293	50.164007
433.274743	106.273243	50.169012
429.576548	117.539275	50.174017
426.029654	107.394405	50.179021
422.357195	114.441378	50.184026
419.087184	94.017324	50.189031
415.740549	103.763879	50.194036
412.065688	99.915909	50.199041
408.932570	102.615375	50.204045
405.139444	109.663937	50.209050
401.773872	105.190204	50.214055
398.153239	101.973171	50.219060
394.791017	103.824061	50.224065
391.357332	97.029150	50.229069
387.221815	107.720349	50.234074
384.132771	105.400002	50.239079
380.845274	106.513725	50.244084
377.571293	108.665551	50.249089
374.141520	98.867981	50.254093
370.179832	99.377725	50.259098
366.428582	95.757869	50.264103
362.903226	109.964145	50.269108
359.244182	106.581225	50.274113
356.262114	97.349495	50.279117
352.469263	103.843685	50.284122
349.246866	98.991365	50.289127
345.573797	111.550120	50.294132
341.986057	106.180622	50.299137
338.524554	96.006715	50.304141
334.768822	94.165706	50.309146
331.858885	88.807368	50.314151
328.544875	92.311799	50.319156
324.568241	84.797649	50.324161
321.130933	101.467440	50.329165
317.199898	107.904468	50.334170
313.972639	110.475888	50.339175
310.809153	100.886432	50.344180
307.011516	92.840754	50.349185
303.511566	88.636023	50.354189
299.973535	106.767981	50.359194
296.208485	102.764601	50.364199
292.811060	114.517892	50.369204
289.329260	112.974975	50.374209
286.083620	94.672153	50.379213
282.147611	100.291072	50.384218
279.246973	92.759302	50.389223
275.699919	105.517859	50.394228
272.086118	102.896841	50.399233
268.670831	105.702381	50.404237
264.890377	107.562945	50.409242
261.751138	100.329475	50.414247
258.032996	97.468014	50.419252
254.464912	101.869712	50.424257
250.957966	94.897965	50.429261
247.024255	112.008522	50.434266
243.990116	114.711247	50.439271
240.622772	97.806989	50.444276
237.282265	101.675741	50.449281
233.437875	100.211214	50.454285
230.006616	97.734389	50.459290
226.779107	91.384986	50.464295
223.104758	89.778424	50.469300
219.320162	104.249955	50.474305
216.029551	100.234339	50.479309
212.390341	105.469125	50.484314
208.953798	98.232026	50.489319
205.412600	98.281027	50.494324
201.911292	106.669967	50.499329
198.502292	86.768842	50.504333
194.646971	105.440228	50.509338
191.532323	105.723114	50.514343
187.870791	113.005764	50.519348
184.257425	106.826780	50.524353
180.979590	103.332444	50.529357
177.605834	106.677429	50.534362
174.203069	98.195252	50.539367
170.353504	97.171231	50.544372
166.924892	109.234076	50.549377
163.480677	99.701848	50.554381
159.873180	115.120456	50.559386
156.315885	102.167160	50.564391
153.125521	97.873182	50.569396
149.364492	103.916689	50.574401
145.992268	99.834094	50.579405
142.012858	100.171890	50.584410
138.926703	91.963385	50.589415
135.785782	103.287023	50.594420
131.831229	109.106898	50.599425
128.486935	95.802732	50.604429
124.877372	107.185562	50.609434
121.556978	111.509801	50.614439
117.985785	105.203333	50.619444
114.070557	98.680539	50.624449
110.833540	91.274390	50.629453
107.607736	90.277566	50.634458
103.931992	103.024309	50.639463
100.246917	94.920019	50.644468
96.688604	101.064918	50.649473
93.480411	95.819124	50.654477
89.607278	103.302033	50.659482
86.542362	96.609353	50.664487
83.138140	105.579371	50.669492
78.991629	98.379167	50.674497
75.937899	90.670658	50.679501
72.297836	104.337408	50.684506
68.959828	100.543692	50.689511
65.412313	106.651013	50.694516
61.846566	101.244612	50.699521
58.417525	94.330849	50.704525
54.733808	99.088569	50.709530
51.437522	89.089699	50.714535
47.774140	92.305222	50.719540
44.001223	93.769548	50.724545
40.537106	99.074440	50.729549
37.158623	106.514508	50.734554
33.972488	106.267168	50.739559
30.339907	107.105227	50.744564
26.811244	106.943697	50.749569
23.633156	97.994049	50.754573
19.649221	103.203424	50.759578
16.190433	102.154582	50.764583
12.696267	104.730198	50.769588
9.417388	95.136221	50.774593
6.054608	89.942564	50.779597
2.090068	93.516377	50.784602