Thu Jun 16 18:10:40 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.342844	78.957215	0.000000
-0.312182	89.268547	0.005005
-0.390940	76.282680	0.010010
-0.394174	80.557522	0.015014
-0.382451	73.966485	0.020019
-0.269541	85.608410	0.025024
-0.219220	86.540519	0.030029
-0.429360	70.143436	0.035034
-0.987590	65.562296	0.040038
-0.868652	52.128041	0.045043
-1.367440	33.692425	0.050048
-1.883470	39.787848	0.055053
-1.910066	27.167111	0.060058
-2.118506	23.502697	0.065062
-2.031012	6.373501	0.070067
-2.425941	7.226174	0.075072
-3.482537	-1.753716	0.080077
-3.563091	-10.740310	0.085082
-4.189988	-3.412922	0.090086
-3.954128	-9.708199	0.095091
-4.077813	-6.910572	0.100096
-4.787073	-12.850667	0.105101
-5.365765	-17.971399	0.110106
-5.673229	-8.378994	0.115110
-5.658478	-11.904973	0.120115
-5.815927	-2.586954	0.125120
-6.157019	-5.492284	0.130125
-5.990360	-16.307169	0.135130
-6.132296	-0.840154	0.140134
-6.587964	-13.481599	0.145139
-6.940203	-5.873152	0.150144
-7.438732	-14.788004	0.155149
-7.476139	-29.202239	0.160154
-7.524246	-17.837543	0.165158
-7.561958	-19.673170	0.170163
-8.631828	-17.420812	0.175168
-9.104063	-10.370657	0.180173
-8.804739	-19.413218	0.185178
-9.641049	-14.880367	0.190182
-9.391224	-24.172532	0.195187
-9.403008	-22.248150	0.200192
-9.640686	-8.700050	0.205197
-9.330067	-7.437554	0.210202
-10.370489	-13.755128	0.215206
-10.663136	-15.757971	0.220211
-10.646046	-18.046407	0.225216
-10.776007	-13.065783	0.230221
-10.987544	-24.455277	0.235226
-11.704397	-6.411086	0.240230
-11.934188	-9.270288	0.245235
-12.270895	-13.061280	0.250240
-12.623544	-5.451187	0.255245
-12.141729	-8.833170	0.260250
-12.344430	-3.000766	0.265254
-12.439155	-18.883988	0.270259
-13.587091	-8.299413	0.275264
-13.955824	-14.893042	0.280269
-13.733028	-16.081233	0.285274
-14.049568	-13.438293	0.290278
-13.895889	-22.771295	0.295283
-14.639413	-11.484934	0.300288
-15.620538	-15.774479	0.305293
-15.614036	-13.817208	0.310298
-15.184247	-11.398336	0.315302
-15.363256	-7.021958	0.320307
-15.457527	-3.824309	0.325312
-15.840326	-5.678083	0.330317
-15.832074	-12.111745	0.335322
-16.791012	-13.980007	0.340326
-16.906378	-26.640880	0.345331
-17.258442	-11.612696	0.350336
-17.685879	2.522400	0.355341
-16.961645	-12.054618	0.360346
-17.261863	-4.800062	0.365350
-18.319270	-6.987776	0.370355
-18.479070	-15.452207	0.375360
-18.589407	-12.776950	0.380365
-18.397179	-27.279351	0.385370
-18.622020	-12.438032	0.390374
-19.556020	-15.082986	0.395379
-19.791390	-21.269106	0.400384
-19.848589	-13.660095	0.405389
-19.819967	-24.814719	0.410394
-20.327861	-3.221602	0.415398
-20.511298	-14.445861	0.420403
-20.609492	-18.688747	0.425408
-21.449693	-0.200933	0.430413
-21.819398	-16.135295	0.435418
-22.159806	-16.520386	0.440422
-22.088032	-14.946820	0.445427
-21.941422	-13.578788	0.450432
-22.372714	-9.526039	0.455437
-22.314951	-13.185799	0.460442
-22.562148	-7.185334	0.465446
-22.733352	-13.667274	0.470451
-23.258027	-16.050957	0.475456
-23.416946	-11.496177	0.480461
-23.569956	-24.819812	0.485466
-23.506700	-12.891255	0.490470
-24.108615	-16.840066	0.495475
-24.604809	-12.955947	0.500480
-25.146610	-8.191879	0.505485
-24.859481	-14.104162	0.510490
-25.200741	-12.231679	0.515494
-25.427889	-19.386376	0.520499
-26.043355	-17.777762	0.525504
-26.690958	-14.657074	0.530509
-26.718283	-15.326634	0.535514
-26.647446	-13.929704	0.540518
-26.616740	-5.925600	0.545523
-26.292270	-9.438047	0.550528
-27.150081	-10.770945	0.555533
-27.772468	-26.721150	0.560538
-28.122623	-7.855982	0.565542
-28.161639	-21.735932	0.570547
-28.655783	-14.564068	0.575552
-28.544229	-15.244347	0.580557
-28.389262	-14.432732	0.585562
-28.998909	-10.147474	0.590566
-29.546929	-17.619099	0.595571
-29.457690	-19.558380	0.600576
-30.164588	-18.710284	0.605581
-29.887323	-15.108387	0.610586
-30.175819	-8.046274	0.615590
-30.420566	-9.247368	0.620595
-30.695696	-17.652780	0.625600
-31.428939	-14.179846	0.630605
-31.631708	-28.291797	0.635610
-32.001911	-14.745184	0.640614
-32.103220	-8.838481	0.645619
-31.717935	-19.710803	0.650624
-31.890603	-12.163902	0.655629
-31.841361	-25.551248	0.660634
-32.870378	-14.187813	0.665638
-33.203694	-18.269409	0.670643
-32.767726	-26.239276	0.675648
-33.547343	-19.116719	0.680653
-34.344280	-23.364286	0.685658
-35.010274	-20.381931	0.690662
-34.592700	-25.036110	0.695667
-34.593570	-23.068447	0.700672
-35.011590	-15.166092	0.705677
-34.801602	-20.262273	0.710682
-35.115429	-11.468224	0.715686
-35.139629	-19.421336	0.720691
-35.578534	-23.864710	0.725696
-36.123239	-21.980803	0.730701
-36.423720	-16.826680	0.735706
-36.608110	-10.320628	0.740710
-36.634094	-15.888156	0.745715
-36.907720	-32.294954	0.750720
-37.861902	-17.913397	0.755725
-37.867530	-28.181758	0.760730
-38.544743	-17.425780	0.765734
-38.214641	-23.131672	0.770739
-38.170309	-19.838152	0.775744
-38.690946	-19.021529	0.780749
-38.551259	-9.737431	0.785754
-38.626631	-16.665246	0.790758
-39.614302	-25.166285	0.795763
-39.889860	-18.874050	0.800768
-40.143487	-17.117665	0.805773
-39.789250	-24.010718	0.810778
-39.993924	-1.111696	0.815782
-39.926137	-3.390853	0.820787
-40.990848	-18.202779	0.825792
-41.262488	-13.379279	0.830797
-40.871921	-30.054486	0.835802
-41.198717	-23.589229	0.840806
-42.123323	-20.190723	0.845811
-42.544766	-18.550246	0.850816
-42.854048	-7.056946	0.855821
-42.552072	-16.063246	0.860826
-42.880642	-18.700719	0.865830
-43.002009	-22.559555	0.870835
-42.861697	-14.865493	0.875840
-43.186253	-20.077152	0.880845
-43.778170	-19.621172	0.885850
-44.245347	-29.011086	0.890854
-44.726856	-25.927616	0.895859
-44.579663	-27.386749	0.900864
-44.795418	-14.147915	0.905869
-44.879181	-20.787943	0.910874
-45.861223	-21.185969	0.915878
-46.157406	-25.067311	0.920883
-45.886755	-19.454617	0.925888
-46.370370	-14.129248	0.930893
-46.230040	-20.494561	0.935898
-46.271922	-15.678452	0.940902
-46.176112	-8.142675	0.945907
-46.603698	-11.840805	0.950912
-47.539604	-12.952827	0.955917
-47.400751	-23.456783	0.960922
-47.534256	-13.063936	0.965926
-48.225047	-26.621190	0.970931
-48.450919	-20.678812	0.975936
-49.088717	-14.749545	0.980941
-49.180464	-16.303361	0.985946
-49.289245	-11.173717	0.990950
-49.306640	-15.088706	0.995955
-49.272527	-14.804853	1.000960
-49.873068	-19.419022	1.005965
-50.059891	-25.461528	1.010970
-50.983850	-18.824571	1.015974
-50.898510	-14.554432	1.020979
-51.011990	-22.704499	1.025984
-51.131627	-9.411404	1.030989
-50.925331	-14.682977	1.035994
-51.023274	-10.991250	1.040998
-51.859726	-18.354233	1.046003
-51.890409	-19.667260	1.051008
-52.116469	-13.433222	1.056013
-52.230145	-12.677443	1.061018
-53.084483	-9.825753	1.066022
-53.687528	-25.606403	1.071027
-53.859408	-24.320303	1.076032
-54.148604	-19.002995	1.081037
-53.779350	-21.281955	1.086042
-53.744881	-18.031793	1.091046
-53.990669	-26.527976	1.096051
-53.953646	-29.379868	1.101056
-54.772642	-22.368795	1.106061
-54.986544	-19.566817	1.111066
-55.208603	-10.143912	1.116070
-55.848421	-15.778001	1.121075
-56.326497	-19.120517	1.126080
-56.889707	-26.389452	1.131085
-56.089018	-23.505262	1.136090
-56.567399	-14.591679	1.141094
-57.289347	-16.265880	1.146099
-57.120696	-21.884415	1.151104
-57.649242	-23.340192	1.156109
-57.165617	-13.086532	1.161114
-57.437640	-23.900727	1.166118
-57.912962	-21.847055	1.171123
-58.128549	-17.442931	1.176128
-58.377263	-9.702134	1.181133
-59.069136	-13.264242	1.186138
-59.814466	-20.612489	1.191142
-60.165935	-14.001777	1.196147
-59.540434	-23.969959	1.201152
-60.070463	-24.440812	1.206157
-60.138303	-28.101809	1.211162
-60.278809	-16.649730	1.216166
-60.258753	-14.832719	1.221171
-60.548383	-14.578626	1.226176
-61.487050	-11.706289	1.231181
-61.792784	-10.319339	1.236186
-62.183238	-10.294234	1.241190
-62.248641	-20.832406	1.246195
-62.101964	-19.940301	1.251200
-62.177113	-21.132427	1.256205
-61.937204	-22.529143	1.261210
-62.363160	-20.986081	1.266214
-63.191365	-18.764184	1.271219
-63.413117	-17.758704	1.276224
-63.697308	-17.450953	1.281229
-63.481620	-23.270725	1.286234
-64.157746	-34.723016	1.291238
-64.654550	-21.126878	1.296243
-64.872006	-26.946291	1.301248
-65.120200	-5.636331	1.306253
-64.990928	-7.380972	1.311258
-65.320271	-12.604074	1.316262
-65.513070	-17.533649	1.321267
-66.377693	-15.250486	1.326272
-66.597986	-10.074394	1.331277
-66.072391	-20.104695	1.336282
-66.598797	-22.207905	1.341286
-66.746917	-13.873454	1.346291
-66.762830	-20.986303	1.351296
-67.442474	-8.920466	1.356301
-67.928842	-20.683521	1.361306
-68.059300	-20.621771	1.366310
-68.175934	-19.510936	1.371315
-68.623064	-26.977817	1.376320
-68.464501	-19.560840	1.381325
-68.551584	-22.427936	1.386330
-69.188204	-22.629008	1.391334
-69.909490	-21.717068	1.396339
-70.067427	-17.944988	1.401344
-70.211155	-19.447000	1.406349
-69.947466	-21.513866	1.411354
-69.993850	-20.067277	1.416358
-70.507821	-18.683301	1.421363
-70.926321	-17.884641	1.426368
-71.433008	-14.465327	1.431373
-71.207017	-19.335567	1.436378
-71.540872	-11.965752	1.441382
-71.654879	-24.394214	1.446387
-71.587790	-19.579543	1.451392
-72.556799	-17.810386	1.456397
-72.742670	-18.563151	1.461402
-73.026070	-14.648988	1.466406
-73.247170	-23.216731	1.471411
-72.905988	-21.271861	1.476416
-74.279807	-17.124504	1.481421
-74.475576	-14.669335	1.486426
-74.179290	-21.195481	1.491430
-74.249263	-22.572157	1.496435
-74.426520	-34.142314	1.501440
-74.661317	-18.766428	1.506445
-75.001256	-14.597762	1.511450
-75.869541	-18.485278	1.516454
-76.015979	-22.565790	1.521459
-76.161658	-23.652535	1.526464
-76.447616	-15.216677	1.531469
-76.473499	-21.882645	1.536474
-76.684914	-19.302953	1.541478
-76.733928	-24.386613	1.546483
-76.642595	-21.887738	1.551488
-77.392509	-22.488778	1.556493
-77.744559	-26.096488	1.561498
-77.649724	-16.791866	1.566502
-78.083122	-11.880762	1.571507
-77.951210	-15.727986	1.576512
-79.115283	-5.189079	1.581517
-79.678986	-19.879972	1.586522
-79.237759	-21.656833	1.591526
-79.698717	-13.863499	1.596531
-79.530987	-22.265046	1.601536
-80.086544	-12.644272	1.606541
-79.866896	-21.944370	1.611546
-80.153782	-15.598962	1.616550
-81.051251	-13.789439	1.621555
-80.863103	-27.314174	1.626560
-81.493113	-13.875371	1.631565
-81.734140	-16.135944	1.636570
-81.572931	-24.540161	1.641574
-81.683202	-19.670922	1.646579
-81.573447	-25.964783	1.651584
-82.414244	-17.267834	1.656589
-82.826651	-23.744922	1.661594
-82.796065	-18.445148	1.666598
-83.274257	-12.571460	1.671603
-83.488943	-25.418251	1.676608
-84.121418	-23.208182	1.681613
-84.480863	-19.413552	1.686618
-84.129161	-23.244319	1.691622
-84.632498	-17.509133	1.696627
-84.350985	-18.889345	1.701632
-84.773003	-14.302134	1.706637
-84.923921	-20.505856	1.711642
-85.429700	-21.903634	1.716646
-85.839363	-18.821578	1.721651
-85.751290	-17.764899	1.726656
-86.003240	-19.400954	1.731661
-86.197463	-21.498291	1.736666
-86.978867	-24.994196	1.741670
-87.503966	-19.417208	1.746675
-87.486821	-17.018341	1.751680
-87.995501	-27.074416	1.756685
-87.827295	-26.966628	1.761690
-87.746914	-25.411357	1.766694
-87.734833	-18.526588	1.771699
-88.059235	-19.375040	1.776704
-88.571780	-26.758792	1.781709
-89.075824	-15.788249	1.786714
-89.305922	-15.470397	1.791718
-89.407899	-14.555151	1.796723
-89.166472	-25.323187	1.801728
-90.336035	-13.996602	1.806733
-90.331807	-15.610871	1.811738
-90.590104	-12.400125	1.816742
-91.284675	-3.383916	1.821747
-91.181752	-23.237713	1.826752
-91.320961	-19.128664	1.831757
-90.852145	-31.843256	1.836762
-91.421404	-24.030745	1.841766
-92.183027	-19.219001	1.846771
-92.575046	-22.768607	1.851776
-92.634522	-19.642517	1.856781
-92.928099	-21.609092	1.861786
-92.913949	-30.289011	1.866790
-92.897414	-13.583058	1.871795
-93.076449	-27.844239	1.876800
-94.091131	-28.706954	1.881805
-94.145885	-37.513202	1.886810
-94.425110	-32.222606	1.891814
-94.362740	-23.139037	1.896819
-94.235528	-18.291488	1.901824
-95.251239	-19.815220	1.906829
-95.606749	-28.638654	1.911834
-96.078497	-26.735725	1.916838
-96.323374	-30.458913	1.921843
-95.755458	-33.050986	1.926848
-96.241793	-27.210388	1.931853
-96.132156	-24.736145	1.936858
-96.325583	-35.988125	1.941862
-96.789288	-27.467058	1.946867
-97.254859	-30.456574	1.951872
-97.655565	-28.792983	1.956877
-97.960424	-28.629009	1.961882
-97.657700	-35.413506	1.966886
-98.144026	-27.346065	1.971891
-98.246086	-31.397406	1.976896
-99.221276	-35.642824	1.981901
-99.694543	-41.300476	1.986906
-99.493581	-27.745483	1.991910
-99.902916	-24.790154	1.996915
-99.676159	-29.487975	2.006912
-98.986426	-26.666410	2.016909
-98.806548	-30.203800	2.026906
-98.494637	-33.409571	2.036902
-98.239493	-29.096490	2.046899
-97.407610	-27.222125	2.056896
-97.056827	-36.034936	2.066893
-96.574994	-31.535088	2.076890
-95.499772	-23.099568	2.086886
-95.463141	-29.120655	2.096883
-95.162967	-31.765186	2.106880
-94.792133	-28.191935	2.116877
-93.745119	-26.139164	2.126874
-93.445215	-19.753929	2.136870
-93.179830	-11.801841	2.146867
-92.359832	-19.003540	2.156864
-92.142307	-21.495723	2.166861
-91.282106	-20.361070	2.176858
-90.757196	-18.880978	2.186854
-90.669308	-20.556247	2.196851
-90.192081	-17.665081	2.206848
-89.167628	-17.123395	2.216845
-89.044621	-16.165814	2.226842
-88.531209	-19.591984	2.236838
-87.701360	-13.284454	2.246835
-87.365783	-17.853967	2.256832
-87.578296	-23.239313	2.266829
-86.206404	-24.173554	2.276826
-86.152673	-15.894191	2.286822
-85.118341	-15.603659	2.296819
-84.817975	-20.425173	2.306816
-84.695186	-21.685005	2.316813
-83.569926	-23.530145	2.326810
-83.160652	-23.274008	2.336806
-83.209646	-17.628077	2.346803
-82.804220	-19.517236	2.356800
-81.779405	-22.008895	2.366797
-81.568742	-13.127611	2.376794
-80.895454	-25.482304	2.386790
-79.918291	-25.002936	2.396787
-79.740203	-18.457789	2.406784
-79.678664	-23.921126	2.416781
-79.193761	-28.463456	2.426778
-79.007011	-25.148715	2.436774
-77.761985	-25.226887	2.446771
-76.828095	-16.595922	2.456768
-76.621081	-24.833382	2.466765
-76.358856	-30.559256	2.476762
-76.479109	-19.385684	2.486758
-75.435617	-23.628962	2.496755
-75.145470	-20.599402	2.506752
-73.843149	-27.661516	2.516749
-73.698265	-18.986090	2.526746
-73.798785	-22.393866	2.536742
-73.153669	-19.781550	2.546739
-72.266903	-26.514793	2.556736
-72.027495	-20.957226	2.566733
-71.151669	-20.360943	2.576730
-70.731094	-20.587147	2.586726
-70.592383	-16.275660	2.596723
-70.088089	-26.542824	2.606720
-69.234701	-24.806055	2.616717
-68.911029	-31.386568	2.626714
-68.401565	-24.906563	2.636710
-67.526852	-22.913324	2.646707
-67.142662	-18.421138	2.656704
-67.057398	-17.377206	2.666701
-66.667851	-25.786981	2.676698
-66.183823	-19.372410	2.686694
-65.331631	-20.579134	2.696691
-64.593199	-19.201501	2.706688
-64.473858	-23.512127	2.716685
-64.104302	-18.537048	2.726682
-63.015182	-17.755337	2.736678
-62.675288	-20.811932	2.746675
-62.592065	-17.949192	2.756672
-62.285175	-18.551042	2.766669
-61.263950	-20.837529	2.776666
-60.965894	-26.881970	2.786662
-60.008284	-22.450869	2.796659
-59.474369	-19.464756	2.806656
-59.315425	-22.178209	2.816653
-59.234260	-22.258623	2.826650
-58.760372	-21.193968	2.836646
-58.087879	-18.801222	2.846643
-57.082371	-19.895286	2.856640
-56.586212	-19.372473	2.866637
-56.070701	-21.038205	2.876634
-56.414016	-16.286598	2.886630
-55.139796	-15.657374	2.896627
-54.436092	-15.211734	2.906624
-54.431101	-19.240901	2.916621
-54.099575	-20.444056	2.926618
-53.504981	-17.447621	2.936614
-53.205206	-21.287542	2.946611
-51.898521	-23.530623	2.956608
-51.678230	-24.071535	2.966605
-51.808540	-25.452230	2.976602
-51.322105	-17.512075	2.986598
-50.312099	-19.933618	2.996595
-49.290558	-19.077121	3.006592
-49.197443	-25.446764	3.016589
-48.651838	-28.949570	3.026586
-48.533899	-20.904953	3.036582
-48.209620	-14.940894	3.046579
-47.126689	-19.943009	3.056576
-46.970206	-27.848016	3.066573
-46.204024	-23.067298	3.076570
-45.324446	-19.332351	3.086566
-45.448282	-18.400651	3.096563
-45.186352	-22.969252	3.106560
-44.272114	-23.863113	3.116557
-43.758917	-28.349170	3.126554
-43.514877	-17.618281	3.136550
-42.389893	-16.708744	3.146547
-41.962923	-18.533303	3.156544
-42.177715	-21.513437	3.166541
-41.556642	-21.227699	3.176538
-40.700332	-23.693677	3.186534
-40.499574	-28.131851	3.196531
-39.746117	-19.027628	3.206528
-39.049538	-15.348277	3.216525
-39.039159	-13.496281	3.226522
-38.458984	-17.617645	3.236518
-37.626275	-16.541462	3.246515
-37.252756	-15.245663	3.256512
-36.889343	-10.766435	3.266509
-36.116312	-17.889444	3.276506
-35.793205	-22.559134	3.286502
-35.522315	-11.633435	3.296499
-34.843466	-12.665213	3.306496
-34.211602	-26.133145	3.316493
-33.799739	-26.742661	3.326490
-33.278431	-21.446726	3.336486
-32.536794	-16.088717	3.346483
-32.323297	-19.384810	3.356480
-32.125987	-31.350958	3.366477
-31.059172	-15.926907	3.376474
-30.747598	-16.835160	3.386470
-30.458365	-16.451213	3.396467
-29.403825	-16.250446	3.406464
-29.108316	-20.583373	3.416461
-28.984169	-15.859236	3.426458
-28.770819	-14.136504	3.436454
-27.953003	-17.873861	3.446451
-27.385089	-12.936102	3.456448
-26.688232	-13.749188	3.466445
-26.323355	-21.349127	3.476442
-25.785639	-15.018891	3.486438
-25.032112	-11.984213	3.496435
-24.875629	-18.582344	3.506432
-24.298417	-8.563307	3.516429
-23.247434	-11.530968	3.526426
-23.198373	-18.168837	3.536422
-23.039694	-14.364235	3.546419
-22.660443	-21.384034	3.556416
-21.816299	-17.722351	3.566413
-21.209344	-19.871418	3.576410
-20.413783	-14.732327	3.586406
-20.144020	-14.191161	3.596403
-20.048698	-15.901541	3.606400
-19.544745	-20.954560	3.616397
-18.785049	-20.519552	3.626394
-18.258540	-14.412289	3.636390
-17.516968	-18.750578	3.646387
-16.984398	-15.754062	3.656384
-16.633097	-17.118535	3.666381
-16.413168	-21.828072	3.676378
-15.987922	-25.091395	3.686374
-15.159414	-10.135489	3.696371
-14.945354	-23.509385	3.706368
-13.851776	-20.374238	3.716365
-13.518352	-19.541321	3.726362
-13.432950	-14.516311	3.736358
-12.829023	-22.886246	3.746355
-11.918207	-26.626819	3.756352
-11.917363	-24.053526	3.766349
-11.534073	-15.765992	3.776346
-10.644329	-17.258468	3.786342
-10.331563	-9.699546	3.796339
-9.654623	-20.453595	3.806336
-8.884238	-10.286797	3.816333
-8.428860	-14.479996	3.826330
-8.227427	-18.604751	3.836326
-8.371709	-20.257555	3.846323
-6.984018	-17.324222	3.856320
-7.105389	-13.785685	3.866317
-6.088444	-12.586932	3.876314
-5.576779	-21.280344	3.886310
-5.398951	-18.048185	3.896307
-5.034879	-3.607516	3.906304
-4.100796	-4.863230	3.916301
-3.970945	-9.710798	3.926298
-3.326412	0.262055	3.936294
-3.488316	12.531809	3.946291
-2.838530	23.807039	3.956288
-2.003285	42.702991	3.966285
-2.029554	64.328153	3.976282
-1.391219	79.871031	3.986278
-0.656198	90.361130	3.996275
-0.371178	116.363632	4.006272
0.000000	139.412999	4.011277
0.254598	145.867780	4.016282
0.445008	143.716715	4.021286
0.669060	146.073820	4.026291
0.538535	162.099383	4.031296
1.321287	179.826510	4.036301
1.500604	174.714813	4.041306
1.092575	168.939343	4.046310
1.387382	154.650278	4.051315
0.977817	148.331571	4.056320
1.074357	143.326794	4.061325
1.200418	148.755680	4.066330
0.950388	147.836123	4.071334
0.967384	148.243169	4.076339
1.012304	159.590749	4.081344
1.235958	157.132003	4.086349
1.051780	168.675794	4.091354
1.196799	171.526914	4.096358
1.171506	180.526938	4.101363
1.080065	187.714328	4.106368
1.205970	183.812797	4.111373
1.428220	185.714313	4.116378
1.482742	172.310627	4.121382
1.353361	153.759555	4.126387
0.826238	148.590484	4.131392
1.536554	174.034548	4.136397
1.483467	168.069404	4.141402
0.936456	171.989097	4.146406
1.084080	174.720906	4.151411
1.509567	177.027067	4.156416
1.362804	193.739728	4.161421
1.505887	188.364286	4.166426
1.585801	186.548756	4.171430
1.177621	176.536793	4.176435
1.421620	184.706121	4.181440
1.264555	183.547642	4.186445
1.368845	186.250309	4.191450
1.473774	176.506838	4.196454
1.643290	184.013071	4.201459
1.620306	186.643443	4.206464
1.367960	170.419266	4.211469
1.224749	179.200225	4.216474
1.120430	186.768189	4.221478
1.448236	171.586337	4.226483
1.521188	188.609065	4.231488
1.655685	182.533596	4.236493
1.816862	186.413011	4.241498
1.671992	181.444171	4.246502
1.752818	191.638957	4.251507
1.640289	194.428265	4.256512
1.319691	179.261022	4.261517
1.363341	173.720391	4.266522
1.523942	189.950630	4.271526
1.884779	178.929487	4.276531
1.351199	189.281155	4.281536
1.285321	183.245508	4.286541
1.560788	192.203036	4.291546
1.553176	186.210047	4.296550
1.338578	179.115433	4.301555
1.188412	189.187186	4.306560
1.460200	194.790206	4.311565
1.624615	200.140753	4.316570
1.514022	201.271322	4.321574
1.922408	202.386368	4.326579
1.646827	209.248541	4.331584
1.959052	211.616636	4.336589
1.753173	204.703677	4.341594
1.671556	215.181141	4.346598
1.674899	203.749058	4.351603
1.429764	214.863245	4.356608
1.768060	210.253767	4.361613
1.938528	215.361708	4.366618
1.754085	213.913260	4.371622
1.959538	207.466746	4.376627
1.924828	217.660122	4.381632
2.061401	212.583001	4.386637
1.993205	218.349752	4.391642
2.087221	220.996113	4.396646
1.931515	211.719425	4.401651
1.892543	218.804927	4.406656
1.995478	225.475807	4.411661
2.200625	226.506350	4.416666
1.748122	232.312447	4.421670
1.897799	223.324170	4.426675
1.611663	228.640761	4.431680
1.964666	223.431481	4.436685
1.957727	218.332298	4.441690
2.156940	225.166921	4.446694
1.986246	223.293751	4.451699
1.915798	231.197196	4.456704
1.503273	224.897199	4.461709
1.605150	233.169754	4.466714
1.518527	242.942174	4.471718
2.033609	236.726439	4.476723
1.779691	265.610352	4.481728
2.249771	260.938631	4.486733
2.478502	260.994098	4.491738
1.966512	256.169171	4.496742
2.399713	245.195709	4.501747
2.381353	255.806983	4.506752
2.537663	259.408910	4.511757
2.235656	251.464372	4.516762
2.329226	249.685449	4.521766
2.826897	239.242865	4.526771
1.968656	232.594075	4.531776
2.492577	231.482481	4.536781
2.427904	233.505511	4.541786
2.460369	224.184695	4.546790
2.454772	224.387410	4.551795
2.340118	234.539945	4.556800
2.022249	226.713864	4.561805
1.943053	234.798017	4.566810
2.090546	240.917150	4.571814
2.400461	249.339428	4.576819
2.601984	260.326261	4.581824
2.346568	264.374679	4.586829
2.589420	258.659228	4.591834
2.080146	244.298152	4.596838
2.421126	249.016051	4.601843
2.016051	256.936038	4.606848
2.303258	264.687756	4.611853
2.498120	256.431231	4.616858
2.275321	267.180875	4.621862
2.886561	265.780286	4.626867
2.348126	259.249802	4.631872
2.415094	256.323846	4.636877
2.566910	258.125923	4.641882
2.211517	254.542270	4.646886
2.564317	256.976378	4.651891
2.575114	265.500484	4.656896
2.524315	255.748070	4.661901
2.483351	266.171199	4.666906
2.517961	268.268394	4.671910
2.570894	263.330571	4.676915
2.384008	259.524419	4.681920
2.496197	267.479783	4.686925
2.482664	267.588605	4.691930
2.407427	271.587616	4.696934
2.845553	261.126742	4.701939
2.707511	275.147373	4.706944
3.001819	274.372654	4.711949
2.772772	266.847084	4.716954
2.675630	272.787344	4.721958
2.810698	273.180701	4.726963
2.540189	288.617264	4.731968
2.613539	277.298162	4.736973
2.973618	282.415535	4.741978
2.937684	283.621379	4.746982
2.952659	276.568792	4.751987
2.715545	280.628002	4.756992
2.764048	269.647361	4.761997
3.018112	274.686456	4.767002
2.801848	271.069447	4.772006
3.154645	273.509477	4.777011
3.029071	280.436472	4.782016
2.901971	279.153658	4.787021
3.114222	283.772776	4.792026
2.970946	277.025738	4.797030
3.159156	270.240003	4.802035
2.820887	285.031492	4.807040
2.827776	276.837788	4.812045
2.911660	279.530032	4.817050
2.865607	285.865658	4.822054
3.021514	269.990439	4.827059
2.880217	281.608225	4.832064
2.703345	277.296373	4.837069
2.844590	288.420258	4.842074
2.783016	303.284821	4.847078
3.309219	308.285168	4.852083
2.941588	317.502067	4.857088
3.223383	304.439255	4.862093
3.424511	307.098020	4.867098
2.959875	306.728812	4.872102
3.178461	315.779869	4.877107
3.424145	315.022260	4.882112
3.202629	297.360446	4.887117
3.129829	290.013264	4.892122
2.978838	294.954744	4.897126
3.296994	303.009178	4.902131
2.965661	312.073864	4.907136
3.404487	316.815866	4.912141
3.617054	306.608889	4.917146
3.021185	299.407636	4.922150
3.051548	297.099595	4.927155
3.017231	318.175579	4.932160
3.107706	310.882698	4.937165
3.280924	307.681283	4.942170
2.902256	312.893622	4.947174
3.219232	300.414676	4.952179
2.956365	318.303615	4.957184
3.446843	309.515280	4.962189
3.510798	303.501439	4.967194
2.897352	312.411290	4.972198
3.350876	301.580245	4.977203
3.328543	304.499398	4.982208
3.649737	315.604417	4.987213
3.516066	310.884472	4.992218
3.376533	319.510010	4.997222
3.646996	302.572620	5.002227
3.479329	310.142235	5.007232
3.300643	317.506691	5.012237
3.615408	308.378021	5.017242
3.211464	310.752905	5.022246
3.428087	299.182605	5.027251
3.156929	306.036395	5.032256
3.328009	305.754313	5.037261
3.467555	299.682994	5.042266
3.402053	308.701280	5.047270
3.861239	330.108112	5.052275
3.398045	331.696427	5.057280
3.474561	334.713199	5.062285
3.541341	340.680952	5.067290
3.655530	345.926394	5.072294
4.154817	339.418144	5.077299
3.808657	331.087612	5.082304
3.526028	321.520469	5.087309
3.391186	308.689391	5.092314
3.386137	330.063433	5.097318
3.660106	334.598867	5.102323
3.447807	340.597449	5.107328
3.729596	350.822763	5.112333
3.983417	342.200393	5.117338
3.645932	342.409023	5.122342
3.738413	339.410663	5.127347
4.016577	350.664589	5.132352
3.689473	356.190243	5.137357
3.585187	350.313402	5.142362
3.463745	335.993118	5.147366
3.800979	332.998509	5.152371
3.584599	337.208115	5.157376
3.624036	338.371220	5.162381
3.826071	337.105338	5.167386
3.359506	340.295128	5.172390
3.728652	327.532481	5.177395
3.457867	334.457748	5.182400
3.432131	338.387231	5.187405
3.762064	343.586165	5.192410
3.824712	358.046967	5.197414
4.279964	364.052542	5.202419
4.046533	373.369730	5.207424
3.803549	364.319981	5.212429
4.072081	364.976603	5.217434
3.936237	369.607693	5.222438
4.253255	366.315020	5.227443
4.038808	373.972606	5.232448
4.009538	369.545471	5.237453
4.288730	365.851098	5.242458
4.386532	367.545304	5.247462
4.179275	359.527041	5.252467
3.626793	344.299297	5.257472
3.925474	348.700324	5.262477
4.425643	357.758048	5.267482
3.976701	363.897167	5.272486
4.200615	365.196124	5.277491
3.916116	372.810926	5.282496
3.978590	365.853150	5.287501
4.353105	360.262904	5.292506
3.881608	365.501848	5.297510
4.075802	361.769432	5.302515
4.094823	371.225541	5.307520
3.828453	360.618299	5.312525
4.250109	357.899196	5.317530
4.101772	354.991835	5.322534
4.101385	359.733921	5.327539
4.287846	363.891266	5.332544
4.269753	371.865551	5.337549
4.358865	361.536971	5.342554
4.283262	360.667895	5.347558
4.194890	359.695563	5.352563
4.408887	358.163891	5.357568
4.592834	361.985622	5.362573
4.619066	372.951978	5.367578
4.183883	368.128430	5.372582
4.477183	364.423143	5.377587
4.433200	368.576544	5.382592
4.681286	359.719320	5.387597
4.376271	368.442280	5.392602
4.458000	368.663220	5.397606
4.655088	362.458552	5.402611
4.443456	368.082233	5.407616
4.807501	352.848831	5.412621
4.644903	361.982543	5.417626
4.218304	367.749189	5.422630
4.384589	348.906716	5.427635
4.676483	355.621601	5.432640
4.290715	362.021687	5.437645
4.441000	358.811127	5.442650
4.257168	362.173218	5.447654
4.393450	363.598634	5.452659
4.474411	361.474901	5.457664
4.419922	355.718281	5.462669
4.253040	348.385140	5.467674
4.414775	362.584110	5.472678
4.338337	363.937242	5.477683
4.689539	387.611793	5.482688
4.727177	391.182061	5.487693
4.837465	388.627472	5.492698
4.479726	388.271278	5.497702
4.968936	395.122080	5.502707
4.781563	395.557875	5.507712
4.805070	382.273378	5.512717
4.343864	381.484304	5.517722
4.389994	392.275425	5.522726
4.521859	389.871374	5.527731
4.418264	388.047868	5.532736
4.333298	402.322965	5.537741
4.517773	392.907766	5.542746
4.438880	407.546405	5.547750
4.639660	397.024229	5.552755
4.851178	412.960970	5.557760
4.644415	416.947323	5.562765
4.910513	428.629110	5.567770
4.599395	434.163494	5.572774
4.869987	426.919226	5.577779
5.206764	429.086277	5.582784
4.764862	438.266883	5.587789
4.933527	434.631802	5.592794
4.905068	443.644341	5.597798
5.318058	427.592595	5.602803
5.061630	425.197262	5.607808
4.752084	421.653250	5.612813
4.714344	421.450959	5.617818
4.592344	435.078201	5.622822
4.842499	430.419295	5.627827
5.014871	427.227269	5.632832
5.252659	432.377827	5.637837
5.477003	434.941716	5.642842
5.152792	440.860864	5.647846
5.186608	425.349880	5.652851
5.152686	428.291000	5.657856
5.373170	423.947574	5.662861
5.061567	418.098556	5.667866
4.909337	429.698530	5.672870
4.964160	421.897281	5.677875
5.151024	423.851834	5.682880
5.112833	429.114594	5.687885
5.211179	410.853911	5.692890
5.048375	435.924156	5.697894
4.934852	428.097351	5.702899
4.886596	434.899167	5.707904
5.308268	438.217542	5.712909
5.468101	430.427645	5.717914
5.332655	429.352492	5.722918
5.051104	426.437238	5.727923
5.090807	421.777005	5.732928
5.209818	428.326925	5.737933
5.125174	438.605357	5.742938
5.305107	424.912572	5.747942
4.868151	426.918916	5.752947
5.202327	432.388687	5.757952
5.020640	428.992051	5.762957
5.277011	420.655522	5.767962
5.089400	430.059884	5.772966
5.274394	442.182176	5.777971
5.396268	451.409023	5.782976
5.192024	456.679306	5.787981
5.806763	454.137236	5.792986
5.556192	466.463336	5.797990
5.691478	461.109708	5.802995
5.666802	446.532602	5.808000
5.521041	431.430236	5.813005
5.431464	426.223292	5.818010
5.181554	435.634796	5.823014
5.100268	447.839870	5.828019
5.308813	460.310790	5.833024
5.468973	458.084077	5.838029
5.523090	451.672239	5.843034
5.280335	461.403610	5.848038
5.412833	462.506061	5.853043
5.932631	458.729284	5.858048
5.455935	461.314813	5.863053
5.817183	459.251198	5.868058
5.609020	463.761178	5.873062
5.098169	460.065440	5.878067
5.483588	472.077679	5.883072
5.480913	469.445652	5.888077
5.807536	457.663881	5.893082
5.738528	456.048049	5.898086
5.499149	463.214534	5.903091
5.461400	461.111787	5.908096
5.584830	470.532746	5.913101
5.865550	472.816606	5.918106
5.518744	467.689944	5.923110
5.854779	462.055506	5.928115
5.936662	460.448380	5.933120
5.729754	465.927571	5.938125
5.478239	470.116776	5.943130
5.594952	470.583812	5.948134
5.924203	477.459705	5.953139
6.245764	486.421232	5.958144
5.765766	481.573780	5.963149
6.019924	465.112764	5.968154
5.916765	470.598982	5.973158
5.835889	459.543297	5.978163
5.881403	459.789067	5.983168
5.674452	465.652836	5.988173
6.008080	458.881956	5.993178
5.890946	460.352122	5.998182
5.658568	468.708063	6.003187
6.127722	484.269921	6.008192
5.846434	490.202613	6.013197
6.159692	484.959759	6.018202
5.949689	498.317069	6.023206
5.944169	500.314870	6.028211
6.054110	492.866455	6.033216
5.804402	482.837770	6.038221
5.721565	481.448275	6.043226
5.609695	494.713200	6.048230
5.940609	499.708295	6.053235
5.760554	498.301518	6.058240
5.571869	499.446790	6.063245
6.087785	491.349100	6.068250
5.875296	497.631319	6.073254
5.735571	493.472107	6.078259
5.917742	489.783084	6.083264
5.905887	500.741619	6.088269
5.945968	502.203467	6.093274
6.179840	488.738098	6.098278
5.899352	483.254179	6.103283
5.953572	495.819594	6.108288
5.904891	497.206134	6.113293
6.142073	500.090132	6.118298
5.796347	506.399307	6.123302
5.917168	508.295230	6.128307
6.153541	500.924182	6.133312
5.717744	505.954135	6.138317
5.868393	491.033489	6.143322
5.747152	493.943470	6.148326
6.021170	503.194437	6.153331
5.969255	500.234017	6.158336
5.916961	495.616687	6.163341
5.974492	488.815652	6.168346
5.848309	486.458375	6.173350
5.774909	502.020924	6.178355
6.070623	493.704491	6.183360
5.675194	495.285767	6.188365
5.650701	502.753381	6.193370
6.402496	522.779345	6.198374
5.923251	515.833185	6.203379
6.203805	497.325535	6.208384
5.741629	502.145067	6.213389
6.137707	491.630606	6.218394
6.033265	496.510887	6.223398
6.015168	494.925312	6.228403
6.081460	498.447162	6.233408
5.828497	505.148368	6.238413
6.222445	495.630316	6.243418
6.096580	499.487200	6.248422
6.031702	489.064704	6.253427
6.229297	504.415935	6.258432
6.218877	507.140970	6.263437
6.254094	501.305441	6.268442
6.218284	497.858834	6.273446
6.308658	498.693189	6.278451
6.385130	488.065408	6.283456
6.211537	488.347290	6.288461
6.183355	479.400886	6.293466
5.562924	481.978602	6.298470
5.880195	474.799801	6.303475
5.769695	477.378583	6.308480
5.583985	490.917548	6.313485
5.781992	482.686231	6.318490
5.768693	491.686822	6.323494
5.569372	499.063851	6.328499
5.651555	490.943029	6.333504
5.859346	486.063205	6.338509
6.102587	491.882083	6.343514
6.045316	499.906813	6.348518
6.010722	494.299380	6.353523
6.076933	499.856573	6.358528
5.629890	507.257279	6.363533
6.205574	487.682709	6.368538
6.264858	497.038911	6.373542
5.868709	486.318755	6.378547
5.924656	497.223165	6.383552
5.905916	497.568447	6.388557
6.011491	499.284764	6.393562
6.091682	493.545299	6.398566
5.988239	487.664715	6.403571
6.168979	500.493461	6.408576
6.020889	495.934189	6.413581
6.370776	496.735226	6.418586
6.149103	497.161795	6.423590
5.955135	494.833182	6.428595
6.217014	495.052667	6.433600
5.983451	495.957920	6.438605
6.226988	492.081959	6.443610
5.900260	492.884711	6.448614
6.128886	492.150039	6.453619
6.007098	485.684580	6.458624
5.589639	483.974693	6.463629
6.121470	493.217873	6.468634
5.867479	492.547469	6.473638
6.316565	486.858724	6.478643
6.163374	483.013502	6.483648
5.965775	477.257106	6.488653
5.807324	480.104666	6.493658
5.788794	477.580921	6.498662
5.785496	488.010604	6.503667
6.185038	487.874169	6.508672
6.131415	493.240330	6.513677
5.919797	475.881925	6.518682
5.564415	480.879046	6.523686
5.945542	490.467968	6.528691
6.169433	488.935930	6.533696
6.133545	490.071440	6.538701
6.012136	477.929499	6.543706
6.126756	483.481449	6.548710
5.838785	482.319718	6.553715
5.706640	476.880150	6.558720
5.674275	494.361132	6.563725
5.934474	483.734562	6.568730
5.853473	495.825381	6.573734
6.152321	488.501630	6.578739
6.253044	495.657604	6.583744
5.737810	509.440072	6.588749
5.968109	490.545212	6.593754
6.090054	500.940788	6.598758
6.049006	496.502442	6.603763
6.279356	490.925022	6.608768
5.898165	498.993909	6.613773
6.047120	483.771062	6.618778
5.765095	472.645412	6.623782
5.744974	487.198743	6.628787
5.805695	495.334200	6.633792
5.328598	496.935287	6.638797
5.942866	495.108564	6.643802
6.018012	496.693465	6.648806
6.088640	492.369557	6.653811
5.824863	493.773590	6.658816
5.912896	503.256457	6.663821
6.041143	493.580657	6.668826
6.164577	500.763168	6.673830
6.090961	506.449036	6.678835
6.181337	501.859035	6.683840
6.113376	500.570869	6.688845
6.186493	501.085264	6.693850
6.368605	502.907818	6.698854
6.013789	498.437464	6.703859
5.883666	472.713052	6.708864
5.949835	476.421186	6.713869
5.891109	472.939500	6.718874
5.513548	483.161593	6.723878
5.793933	481.171028	6.728883
6.249598	491.341754	6.733888
5.941613	495.633333	6.738893
6.155996	495.752933	6.743898
6.276870	494.060236	6.748902
6.302725	484.233249	6.753907
5.986985	471.258094	6.758912
5.285559	478.254890	6.763917
5.833001	484.568483	6.768922
6.052630	487.899047	6.773926
6.183990	491.045007	6.778931
6.305778	482.546589	6.783936
5.490115	474.175475	6.788941
5.955745	480.725654	6.793946
6.040082	495.170668	6.798950
5.610189	500.184154	6.803955
5.990868	497.696840	6.808960
5.456167	497.928099	6.813965
6.316096	500.477333	6.818970
6.128317	499.931051	6.823974
5.454854	498.996503	6.828979
6.060311	501.272774	6.833984
5.469669	509.734709	6.838989
6.073185	490.718482	6.843994
6.117782	498.731013	6.848998
5.968335	502.287137	6.854003
6.020901	502.051571	6.859008
5.891836	499.277836	6.864013
5.669361	503.471328	6.869018
5.795283	503.058089	6.874022
5.851087	512.267281	6.879027
5.892767	499.508787	6.884032
6.010586	499.893951	6.889037
6.354033	496.741122	6.894042
6.197826	510.537857	6.899046
6.153572	504.579706	6.904051
6.179562	499.651686	6.909056
6.047576	497.477392	6.914061
6.246080	496.783116	6.919066
6.316130	506.727227	6.924070
6.087535	501.698027	6.929075
5.960519	502.197351	6.934080
5.792915	488.940300	6.939085
5.796894	485.793850	6.944090
5.950418	498.404912	6.949094
6.085912	497.518799	6.954099
6.204443	491.086631	6.959104
5.994632	495.224061	6.964109
6.022880	481.771862	6.969114
5.888406	476.989548	6.974118
6.086570	475.853240	6.979123
6.403429	472.489635	6.984128
5.775478	482.633436	6.989133
5.772427	477.702034	6.994138
5.633604	480.147672	6.999142
5.423237	480.026593	7.004147
5.878224	495.686699	7.009152
5.770254	507.506430	7.014157
6.022476	497.486144	7.019162
5.700044	501.984632	7.024166
6.175039	496.259736	7.029171
6.265325	496.270502	7.034176
5.909922	503.531457	7.039181
5.878967	503.889708	7.044186
5.922204	499.933093	7.049190
5.595614	502.440645	7.054195
5.775364	496.998361	7.059200
5.538549	499.642123	7.064205
5.809595	497.132379	7.069210
5.852993	509.513523	7.074214
5.689365	503.305762	7.079219
6.013225	497.305031	7.084224
5.877717	503.017800	7.089229
5.799286	495.272672	7.094234
5.722136	508.545584	7.099238
5.836883	518.367872	7.104243
6.059698	525.799955	7.109248
5.936543	523.318651	7.114253
6.373444	515.683495	7.119258
5.876652	507.263514	7.124262
5.636090	504.743604	7.129267
5.839775	517.244083	7.134272
6.161248	536.224855	7.139277
6.203614	522.426758	7.144282
6.056661	516.782044	7.149286
5.903253	509.120235	7.154291
6.018965	497.711295	7.159296
5.733412	518.077095	7.164301
6.153748	516.089443	7.169306
6.025623	507.108039	7.174310
6.111157	503.478196	7.179315
6.195711	492.722497	7.184320
5.827436	497.165813	7.189325
5.760954	496.506252	7.194330
5.999582	507.401889	7.199334
5.996413	504.561175	7.204339
6.177907	489.781645	7.209344
6.108773	502.387380	7.214349
5.708310	500.116865	7.219354
5.880740	506.723106	7.224358
5.830937	511.404345	7.229363
5.913006	508.239855	7.234368
5.673554	522.531813	7.239373
6.283071	515.150591	7.244378
6.007669	513.121445	7.249382
5.929109	507.166002	7.254387
6.188573	504.668530	7.259392
5.785254	500.985003	7.264397
5.930463	495.263897	7.269402
5.953888	499.960655	7.274406
5.716942	494.194081	7.279411
6.150597	516.985924	7.284416
5.759582	525.909256	7.289421
6.116884	521.853080	7.294426
6.071029	531.713263	7.299430
5.856281	524.835760	7.304435
6.271746	512.372036	7.309440
5.809805	512.370472	7.314445
5.938759	500.029680	7.319450
5.772118	508.910495	7.324454
5.993680	530.358159	7.329459
6.128223	529.318886	7.334464
6.042170	524.830549	7.339469
6.322270	511.793790	7.344474
6.078910	505.858282	7.349478
6.056347	499.240172	7.354483
6.034801	501.604376	7.359488
5.667161	499.027232	7.364493
5.847017	504.585180	7.369498
6.195195	502.554501	7.374502
5.842135	505.627698	7.379507
5.985141	508.985037	7.384512
5.755788	505.105139	7.389517
5.707532	502.978273	7.394522
5.870211	501.400510	7.399526
5.958888	521.704470	7.404531
6.123298	519.416370	7.409536
6.095990	536.569708	7.414541
6.560070	516.772818	7.419546
6.292323	517.175529	7.424550
6.013818	513.152409	7.429555
6.414065	495.047044	7.434560
6.137920	502.114847	7.439565
5.895774	499.123316	7.444570
5.937060	500.036620	7.449574
5.802208	503.161364	7.454579
6.022832	498.607061	7.459584
6.031882	502.126040	7.464589
6.133786	505.898125	7.469594
6.126143	506.648738	7.474598
5.886618	506.700493	7.479603
6.314456	504.188217	7.484608
5.937695	508.095841	7.489613
6.076746	503.733491	7.494618
6.210535	506.388719	7.499622
5.741436	509.899011	7.504627
6.037158	498.063220	7.509632
5.772302	504.290363	7.514637
6.270543	505.754535	7.519642
6.060602	499.884739	7.524646
5.860019	505.983560	7.529651
5.767321	505.187250	7.534656
5.830715	509.910358	7.539661
5.630539	499.768306	7.544666
5.873310	495.776941	7.549670
5.792153	499.815960	7.554675
6.078040	498.097373	7.559680
6.036551	510.908887	7.564685
6.096571	516.598523	7.569690
5.713519	507.080319	7.574694
5.662236	515.598347	7.579699
5.912208	508.986792	7.584704
5.467672	507.169398	7.589709
5.563504	502.603456	7.594714
5.965319	508.588125	7.599718
5.963616	517.237858	7.604723
5.896256	507.705861	7.609728
5.733118	514.467502	7.614733
6.101655	521.128654	7.619738
6.042910	519.589060	7.624742
6.118085	522.724580	7.629747
6.434530	507.870638	7.634752
5.960807	511.371928	7.639757
6.143624	498.094547	7.644762
6.188806	501.394649	7.649766
5.716239	511.436526	7.654771
6.272297	496.406256	7.659776
6.295263	510.089422	7.664781
6.319072	500.812489	7.669786
6.314807	496.444919	7.674790
6.062694	507.279588	7.679795
5.682473	500.167010	7.684800
5.837074	501.580730	7.689805
6.064910	502.680648	7.694810
6.228364	511.726627	7.699814
5.934480	503.580930	7.704819
6.163345	499.615441	7.709824
5.946986	507.295706	7.714829
6.043813	504.092175	7.719834
6.139450	501.416666	7.724838
5.759843	506.766261	7.729843
6.132698	497.957399	7.734848
5.869866	511.321971	7.739853
5.818846	507.961932	7.744858
6.085128	505.338431	7.749862
5.855840	508.055536	7.754867
5.890158	503.900413	7.759872
5.952212	510.016212	7.764877
6.121785	504.370496	7.769882
6.111771	503.929406	7.774886
5.643336	507.392627	7.779891
5.917475	501.471146	7.784896
5.646657	513.862587	7.789901
5.666253	507.779538	7.794906
5.686477	506.165924	7.799910
5.531986	503.972656	7.804915
5.904981	498.776358	7.809920
5.816386	513.446002	7.814925
5.960574	506.403625	7.819930
5.787246	502.775914	7.824934
6.021375	510.921692	7.829939
6.304154	504.985166	7.834944
5.746282	513.858323	7.839949
5.822130	507.683696	7.844954
6.194333	512.617512	7.849958
5.815325	512.915485	7.854963
5.842346	503.872334	7.859968
5.849814	497.034285	7.864973
5.811998	510.975524	7.869978
5.911209	509.898681	7.874982
6.361273	522.179974	7.879987
6.156731	508.448937	7.884992
6.094877	515.125667	7.889997
6.225045	503.178616	7.895002
6.092843	509.302346	7.900006
5.590608	519.972359	7.905011
6.022066	505.277295	7.910016
5.964553	514.945233	7.915021
5.705392	505.846968	7.920026
6.020600	505.301126	7.925030
6.096517	512.734689	7.930035
6.259383	513.104615	7.935040
5.813234	511.816003	7.940045
6.190792	507.043279	7.945050
6.474636	504.914905	7.950054
5.742009	523.150757	7.955059
6.415619	510.175250	7.960064
6.289582	505.683760	7.965069
6.269592	507.284681	7.970074
6.416015	502.914108	7.975078
5.975665	493.156761	7.980083
6.608784	481.903545	7.985088
5.814740	483.503142	7.990093
6.445456	483.862739	7.995098
6.303358	492.544737	8.000102
6.009664	488.257558	8.005107
6.017971	482.696710	8.010112
5.708682	492.232856	8.015130
5.921745	487.162098	8.020147
6.349176	485.528597	8.025165
5.507991	495.148963	8.030182
6.088746	489.570869	8.035200
6.108931	484.763834	8.040218
6.171149	479.563706	8.045235
6.079986	480.619362	8.050253
6.144786	489.318982	8.055270
6.027979	484.064103	8.060288
6.204474	485.102096	8.065306
6.039778	484.661721	8.070323
6.357297	470.812343	8.075341
6.000067	475.201021	8.080358
6.189402	473.959954	8.085376
5.790429	495.794719	8.090394
5.853884	485.858745	8.095411
6.334899	484.141993	8.100429
6.150781	483.866313	8.105446
6.188977	481.667826	8.110464
6.073185	482.826648	8.115482
6.136191	485.020193	8.120499
6.297729	489.637850	8.125517
5.670755	486.073775	8.130534
5.940305	477.157390	8.135552
5.878934	478.875026	8.140570
6.027057	490.140416	8.145587
6.686067	477.634929	8.150605
6.333926	489.578748	8.155622
6.024284	482.931691	8.160640
6.028601	484.991064	8.165658
5.960870	482.986034	8.170675
6.311634	474.109369	8.175693
5.770883	483.983564	8.180710
5.794998	481.491691	8.185728
6.060037	480.684093	8.190746
6.185742	486.476842	8.195763
6.188719	478.798186	8.200781
5.640996	484.925413	8.205798
5.956958	485.839885	8.210816
5.957285	486.947929	8.215834
5.897976	488.085412	8.220851
6.072026	478.514756	8.225869
5.794743	489.948364	8.230886
5.877427	488.089999	8.235904
6.500485	506.202599	8.240922
6.128813	508.934924	8.245939
6.074500	507.910662	8.250957
5.975369	515.632258	8.255974
6.106229	511.706169	8.260992
6.317632	516.467927	8.266010
6.025638	513.932244	8.271027
6.362337	512.051972	8.276045
6.067170	510.826514	8.281062
6.292068	508.499647	8.286080
6.116266	512.798325	8.291098
6.072069	498.990002	8.296115
6.435908	503.698617	8.301133
6.247066	518.214008	8.306150
6.567324	510.075596	8.311168
6.508639	511.858134	8.316186
6.445459	508.045693	8.321203
6.738261	503.023946	8.326221
6.179386	510.459674	8.331238
6.369723	515.970052	8.336256
6.465238	508.664403	8.341274
6.431134	506.281342	8.346291
6.161802	497.398204	8.351309
6.281676	502.802822	8.356326
6.323354	504.869112	8.361344
6.254887	511.295030	8.366362
6.192558	514.463153	8.371379
6.401680	508.049094	8.376397
6.022683	507.568950	8.381414
6.405461	510.935805	8.386432
6.402615	501.583802	8.391450
6.282044	509.030742	8.396467
6.434219	505.887109	8.401485
6.462386	508.068899	8.406502
6.442870	508.709838	8.411520
6.280574	505.585996	8.416538
6.500233	514.695686	8.421555
6.741022	504.512520	8.426573
6.587409	510.179227	8.431590
6.257393	493.053114	8.436608
6.436520	489.784777	8.441626
6.255335	507.329532	8.446643
6.542787	505.641716	8.451661
6.159684	511.064412	8.456678
6.333214	507.051956	8.461696
6.160789	506.871963	8.466714
5.867366	510.001518	8.471731
6.110189	499.915048	8.476749
5.986531	505.678260	8.481766
5.883930	506.572355	8.486784
5.844126	518.548914	8.491802
6.068885	528.835900	8.496819
6.323203	534.731406	8.501837
6.158732	549.534281	8.506854
5.822284	540.882249	8.511872
6.123288	536.152488	8.516890
6.187752	556.810952	8.521907
6.597420	556.330368	8.526925
6.598865	565.286126	8.531942
6.806065	567.829211	8.536960
6.672407	559.163239	8.541978
6.346332	560.555306	8.546995
6.542968	559.067401	8.552013
6.589093	562.983220	8.557030
6.622253	577.320370	8.562048
6.918951	555.580600	8.567066
6.430092	546.306527	8.572083
6.773492	540.635971	8.577101
6.781228	550.874601	8.582119
6.832230	546.765772	8.587136
6.830218	539.013023	8.592154
6.721474	540.626212	8.597171
7.019284	537.239352	8.602189
6.797386	551.585171	8.607207
6.683273	541.294225	8.612224
6.818840	536.599874	8.617242
6.643584	543.569243	8.622259
6.779535	553.240132	8.627277
6.889295	557.430224	8.632295
6.764171	542.514277	8.637312
6.835159	524.980287	8.642330
6.537857	511.084474	8.647347
6.699995	508.112981	8.652365
6.532818	517.791332	8.657383
6.484692	526.157928	8.662400
6.707830	524.907728	8.667418
6.335238	534.441230	8.672435
6.936683	536.958520	8.677453
6.796804	542.488938	8.682471
6.621163	554.495453	8.687488
6.632946	544.925297	8.692506
6.527062	541.249802	8.697523
6.600885	542.321201	8.702541
6.247306	540.540142	8.707559
6.261185	544.016484	8.712576
6.398756	543.916634	8.717594
6.112259	547.047610	8.722611
6.014568	551.313905	8.727629
6.498840	556.749742	8.732647
6.591090	566.479131	8.737664
6.844206	566.243769	8.742682
6.435748	580.184599	8.747699
6.645752	579.114388	8.752717
6.380469	577.137466	8.757735
6.322468	575.020403	8.762752
7.151927	564.435047	8.767770
6.872927	571.469793	8.772787
6.953840	567.842640	8.777805
7.116655	574.660896	8.782823
7.016529	573.393359	8.787840
6.870706	564.392348	8.792858
6.643397	580.258302	8.797875
6.773114	575.519737	8.802893
6.892192	568.137246	8.807911
6.817310	570.604530	8.812928
6.788469	569.151721	8.817946
6.621152	577.770973	8.822963
6.756878	577.285768	8.827981
6.846079	580.502766	8.832999
6.613322	576.315255	8.838016
7.551237	571.885272	8.843034
7.428542	581.594002	8.848051
7.409207	573.689598	8.853069
7.199906	580.080660	8.858087
7.014132	566.728273	8.863104
7.177011	557.227119	8.868122
6.914082	552.317567	8.873139
6.835652	544.577444	8.878157
6.592703	547.563060	8.883175
6.700303	553.116744	8.888192
7.025166	562.811133	8.893210
6.846226	560.415392	8.898227
7.113020	555.996636	8.903245
6.881729	562.945261	8.908263
6.850530	562.839253	8.913280
7.111977	569.384264	8.918298
6.664460	560.445021	8.923315
6.943456	570.934057	8.928333
7.078336	573.004832	8.933351
7.113214	579.012886	8.938368
7.221863	568.665722	8.943386
6.617008	564.342794	8.948403
7.135605	576.614940	8.953421
7.037941	574.480420	8.958439
6.946053	585.221079	8.963456
7.129815	571.433768	8.968474
6.894408	580.166913	8.973491
7.234713	579.186368	8.978509
7.075851	572.131844	8.983527
6.630827	558.142411	8.988544
7.170705	567.749803	8.993562
6.535628	574.550535	8.998579
6.872650	573.136950	9.003597
7.108204	571.205092	9.008615
6.920735	578.232194	9.013632
6.892849	572.152302	9.018650
6.658040	578.389537	9.023667
6.892962	590.454487	9.028685
6.822027	588.214188	9.033703
6.777820	577.283628	9.038720
7.406831	571.433208	9.043738
7.106073	570.405582	9.048755
7.043580	576.365761	9.053773
7.412598	581.499648	9.058791
7.019003	585.005059	9.063808
7.151565	581.363757	9.068826
6.677333	584.594849	9.073843
7.079360	594.738332	9.078861
7.539748	595.336672	9.083879
7.078937	590.316331	9.088896
7.418794	584.610131	9.093914
6.909929	581.154641	9.098931
6.964374	573.736577	9.103949
7.006113	588.752218	9.108967
7.248333	610.116875	9.113984
7.490138	608.892810	9.119002
7.612829	603.351209	9.124019
7.182046	585.912177	9.129037
7.136441	582.187249	9.134055
6.962749	583.925427	9.139072
7.095415	586.170357	9.144090
7.176328	604.806154	9.149107
7.331820	609.679919	9.154125
7.476377	605.357321	9.159143
7.307200	591.666304	9.164160
7.501933	595.606284	9.169178
7.164516	579.513889	9.174195
7.067829	587.666536	9.179213
6.836237	588.710275	9.184231
7.354853	608.588665	9.189248
7.611646	601.512277	9.194266
7.335871	611.294642	9.199283
7.209574	617.556275	9.204301
7.329721	619.685780	9.209319
7.135162	622.187021	9.214336
7.275546	613.374665	9.219354
7.070573	612.572306	9.224371
6.913304	616.143472	9.229389
7.194199	617.711860	9.234407
6.858542	622.171509	9.239424
7.088644	607.826506	9.244442
7.511002	611.975581	9.249459
7.416464	616.872659	9.254477
7.718383	611.078641	9.259495
7.103747	619.664477	9.264512
7.292138	604.271243	9.269530
7.060954	606.923094	9.274547
7.347607	611.854303	9.279565
7.609405	611.825540	9.284583
7.677475	615.890081	9.289600
7.471271	619.178245	9.294618
7.353537	603.240726	9.299635
7.246574	610.423898	9.304653
7.504472	608.988648	9.309671
7.326771	619.343977	9.314688
7.451843	615.919910	9.319706
7.705526	608.785383	9.324723
7.395498	603.355050	9.329741
7.548418	607.672350	9.334759
7.120956	617.644816	9.339776
7.699336	609.629413	9.344794
7.617934	598.757338	9.349811
7.449862	610.109513	9.354829
7.826218	602.218528	9.359847
7.738812	617.935536	9.364864
7.471474	620.022994	9.369882
7.711710	605.592573	9.374899
7.616741	607.960839	9.379917
7.477102	612.808391	9.384935
7.290652	611.293844	9.389952
7.589293	608.876837	9.394970
7.357453	609.023042	9.399987
7.431022	617.794993	9.405005
7.382969	620.007009	9.410023
7.489954	610.271795	9.415040
7.462327	616.522731	9.420058
7.767949	626.428079	9.425075
7.686187	621.509525	9.430093
7.536010	613.379327	9.435111
7.819121	623.680057	9.440128
7.946337	617.643991	9.445146
7.842033	607.757016	9.450163
7.601200	618.348132	9.455181
7.754691	603.034274	9.460199
7.943426	615.428178	9.465216
7.447842	612.838934	9.470234
7.448340	617.187035	9.475251
7.657619	616.581229	9.480269
7.712382	603.275461	9.485287
7.464048	615.691210	9.490304
7.237583	616.917339	9.495322
7.849667	625.266205	9.500339
7.386382	632.580406	9.505357
7.671072	634.444770	9.510375
7.931116	644.072574	9.515392
7.677018	633.095278	9.520410
7.815275	643.091178	9.525427
7.751553	644.870923	9.530445
7.904258	635.836970	9.535463
7.502208	629.568540	9.540480
7.609847	635.701280	9.545498
7.754942	644.877790	9.550515
7.843177	657.510344	9.555533
7.893418	637.697473	9.560551
7.989119	635.518098	9.565568
7.678232	634.251731	9.570586
7.823702	633.318832	9.575603
7.714343	652.400231	9.580621
7.830201	642.899119	9.585639
7.318658	646.997458	9.590656
7.298716	643.830086	9.595674
7.567641	649.860797	9.600691
7.448194	660.373032	9.605709
7.619155	652.940792	9.610727
7.876716	651.698768	9.615744
7.821407	652.818184	9.620762
7.902729	653.023345	9.625779
7.940732	653.025465	9.630797
7.691298	646.114593	9.635815
7.934171	651.543909	9.640832
7.798130	650.302573	9.645850
7.830488	648.362758	9.650867
7.714674	660.367144	9.655885
7.791499	668.341086	9.660903
7.811646	670.271808	9.665920
8.193968	689.283117	9.670938
8.461524	673.217691	9.675955
7.825882	663.690392	9.680973
7.869705	647.877086	9.685991
8.036678	655.074938	9.691008
7.788290	661.210827	9.696026
8.213012	639.833966	9.701043
7.639910	649.099744	9.706061
7.749191	649.245077	9.711079
7.958933	666.704448	9.716096
8.371516	677.080059	9.721114
7.928615	662.096061	9.726131
8.037868	674.053127	9.731149
8.222990	671.563744	9.736167
8.032917	653.908507	9.741184
8.025901	647.377282	9.746202
7.990938	655.518682	9.751219
8.214617	650.271246	9.756237
7.988701	643.348418	9.761255
8.061364	644.588786	9.766272
7.956706	642.235273	9.771290
8.031497	645.340120	9.776307
8.128990	657.303938	9.781325
8.459968	658.373490	9.786343
8.139949	658.536826	9.791360
7.878812	650.273791	9.796378
8.298898	641.328596	9.801395
7.828655	646.461955	9.806413
8.218197	657.079705	9.811431
8.096719	663.671801	9.816448
8.112835	673.617053	9.821466
8.357237	660.508596	9.826483
7.440827	663.863753	9.831501
7.887369	668.583943	9.836519
8.408055	682.468739	9.841536
8.136067	685.874364	9.846554
8.528823	676.355812	9.851571
8.347606	685.994076	9.856589
8.491501	689.993457	9.861607
8.059214	674.510436	9.866624
7.953819	676.773269	9.871642
8.149121	669.356188	9.876659
7.856724	681.103503	9.881677
8.068637	679.370288	9.886695
8.160959	682.312233	9.891712
7.822422	686.360735	9.896730
7.925185	682.070117	9.901747
7.977092	681.361499	9.906765
8.072818	685.823781	9.911783
7.856087	680.571375	9.916800
8.087186	707.338056	9.921818
8.284169	711.369607	9.926835
8.192545	724.572104	9.931853
8.314433	725.654959	9.936871
8.313926	716.894169	9.941888
8.013827	729.178135	9.946906
8.068550	712.434576	9.951923
8.285874	713.317635	9.956941
7.861060	716.412163	9.961959
8.276567	719.177104	9.966976
8.014571	729.390361	9.971994
8.581900	710.770859	9.977011
8.273608	710.023752	9.982029
8.720812	711.201244	9.987047
8.583494	711.258416	9.992064
8.397660	716.124165	9.997082
8.446279	718.171130	10.002099
8.534627	709.321658	10.007117
8.290022	715.130423	10.012135
8.796242	704.497621	10.017152
8.614066	715.588274	10.022170
8.500065	709.897298	10.027187
8.487066	713.384517	10.032205
8.568155	716.170674	10.037223
8.471749	712.763605	10.042240
8.157369	711.698857	10.047258
8.227540	717.986419	10.052275
8.625161	715.410739	10.057293
8.638560	706.890332	10.062311
8.544435	704.162692	10.067328
8.106561	717.819777	10.072346
8.305585	715.895316	10.077363
8.572429	707.587705	10.082381
8.534833	717.492263	10.087399
8.518870	708.612596	10.092416
8.498153	712.343765	10.097434
8.412379	710.322301	10.102451
8.354920	715.651987	10.107469
8.249129	717.241679	10.112487
8.572505	716.789916	10.117504
8.268446	730.938197	10.122522
8.945273	734.071499	10.127539
9.039969	744.867640	10.132557
8.745094	729.196037	10.137575
8.846761	718.298052	10.142592
8.348111	709.535942	10.147610
8.650788	707.686266	10.152627
8.309935	709.834793	10.157645
8.663835	720.068091	10.162663
8.605839	721.122809	10.167680
8.327550	726.442741	10.172698
8.876820	741.229602	10.177715
9.047288	744.725871	10.182733
8.579304	722.259823	10.187751
8.971176	724.896017	10.192768
8.187756	718.537256	10.197786
8.999041	730.412200	10.202803
8.549182	726.603775	10.207821
8.358854	734.779158	10.212839
8.530362	740.514246	10.217856
8.504416	755.031281	10.222874
9.169480	745.772949	10.227891
8.803073	750.380212	10.232909
8.588111	755.802465	10.237927
9.021072	749.619183	10.242944
8.905450	758.469716	10.247962
9.030298	748.706270	10.252979
8.990670	747.694523	10.257997
8.802590	734.015163	10.263015
8.642614	729.600264	10.268032
8.382528	733.100767	10.273050
9.161202	739.364147	10.278067
8.576900	737.921635	10.283085
8.434828	749.635499	10.288103
8.822454	747.573388	10.293120
8.622133	756.895124	10.298138
8.791843	746.905798	10.303155
8.755084	749.499268	10.308173
8.673382	750.847817	10.313191
8.959187	753.252965	10.318208
8.488864	756.913982	10.323226
8.595563	758.109764	10.328243
8.755511	748.599333	10.333261
8.841171	754.956384	10.338279
8.910825	750.895394	10.343296
8.828899	769.441490	10.348314
8.998273	785.408508	10.353331
8.781021	779.989449	10.358349
8.840291	787.845115	10.363367
9.218950	777.104625	10.368384
8.924600	770.180060	10.373402
8.801419	781.578477	10.378419
8.762430	780.869721	10.383437
9.027646	793.477764	10.388455
9.308047	769.720249	10.393472
9.143792	775.921596	10.398490
8.971881	781.953963	10.403507
9.228007	776.528513	10.408525
9.023109	781.333663	10.413543
9.056511	771.768356	10.418560
9.059284	784.437870	10.423578
9.391454	780.524205	10.428595
9.257552	763.000875	10.433613
8.929347	755.209026	10.438631
9.267708	746.049362	10.443648
9.228507	754.885295	10.448666
8.932406	753.794496	10.453683
9.133786	738.759845	10.458701
8.994904	739.279009	10.463719
9.044486	740.185264	10.468736
9.243704	758.642963	10.473754
9.290915	769.504046	10.478771
9.043616	747.904489	10.483789
8.990990	753.545147	10.488807
9.250500	766.846712	10.493824
9.289764	781.160704	10.498842
9.119851	775.896592	10.503859
8.869685	778.361779	10.508877
9.170123	775.134741	10.513895
9.622781	776.322950	10.518912
9.388446	782.471325	10.523930
9.081835	775.039813	10.528947
9.240973	770.892978	10.533965
9.213686	778.216381	10.538983
9.250138	781.205367	10.544000
9.042521	781.860280	10.549018
9.018531	784.189288	10.554035
9.573788	784.185146	10.559053
9.257727	785.663162	10.564071
9.192083	783.357109	10.569088
9.069790	784.821603	10.574106
9.302207	786.693346	10.579123
9.534229	778.032063	10.584141
9.000787	781.904665	10.589159
9.466553	777.861656	10.594176
9.404173	786.195814	10.599194
9.212215	781.253793	10.604211
9.073930	774.188690	10.609229
9.061044	781.639615	10.614247
8.974025	781.185015	10.619264
9.217483	787.320760	10.624282
9.060131	790.059342	10.629299
9.084062	797.707503	10.634317
9.218493	810.320050	10.639335
9.351179	807.130767	10.644352
9.428399	811.326601	10.649370
9.313258	814.677401	10.654387
9.742952	805.811416	10.659405
9.712285	812.850402	10.664423
9.832637	814.671585	10.669440
9.678428	816.147261	10.674458
9.283483	792.427709	10.679475
9.612783	790.000686	10.684493
9.355907	797.541342	10.689511
9.385794	803.480536	10.694528
9.582332	816.140492	10.699546
9.874162	822.458579	10.704563
9.815510	798.424429	10.709581
9.504530	792.522709	10.714599
9.698775	775.260437	10.719616
9.838025	777.709883	10.724634
9.375079	786.093115	10.729651
9.498238	776.028013	10.734669
9.304614	780.926756	10.739687
9.551153	779.848820	10.744704
9.663499	788.393630	10.749722
9.472989	785.074132	10.754739
9.809537	785.343299	10.759757
9.457560	782.397869	10.764775
9.348565	794.565083	10.769792
9.734902	809.407671	10.774810
9.647741	822.209579	10.779827
9.979438	805.336892	10.784845
9.871402	803.965445	10.789863
9.582420	788.904516	10.794880
9.760182	776.897049	10.799898
9.769680	781.602803	10.804915
9.656469	776.939847	10.809933
9.705889	784.771750	10.814951
9.593151	777.482775	10.819968
9.518645	789.876137	10.824986
9.893706	815.761484	10.830003
9.911377	808.720387	10.835021
9.910106	808.115024	10.840039
9.910028	798.704421	10.845056
9.856070	785.688367	10.850074
9.626469	779.893262	10.855091
9.675459	779.152253	10.860109
9.501232	792.828815	10.865127
9.712779	804.376622	10.870144
9.943401	811.195291	10.875162
9.927791	820.864627	10.880179
9.801137	808.897799	10.885197
9.924370	818.123785	10.890215
9.661238	821.466569	10.895232
10.003527	813.036412	10.900250
9.560844	818.071783	10.905267
10.079773	813.314387	10.910285
9.839230	812.011483	10.915303
9.847879	810.688456	10.920320
10.085861	805.720448	10.925338
9.792576	820.080577	10.930355
9.870979	821.529621	10.935373
9.884718	808.359864	10.940391
9.834385	820.386323	10.945408
10.072763	818.635040	10.950426
9.621463	819.550072	10.955443
9.866123	809.551665	10.960461
10.087293	820.196271	10.965479
9.945956	826.660146	10.970496
10.033060	811.427219	10.975514
10.020552	825.621286	10.980531
10.134479	816.821453	10.985549
10.111616	810.128140	10.990567
9.753755	806.235604	10.995584
9.630604	813.771488	11.000602
9.907443	816.085622	11.005619
9.929584	817.220789	11.010637
9.980063	819.632165	11.015655
9.906546	818.439233	11.020672
10.170666	811.399919	11.025690
10.330086	820.185352	11.030707
10.120517	815.845345	11.035725
10.425553	828.236635	11.040743
10.035719	825.078590	11.045760
10.002380	818.988874	11.050778
9.556878	815.891204	11.055795
10.014383	832.318248	11.060813
10.100302	844.327326	11.065831
10.219226	850.857434	11.070848
10.503847	848.698571	11.075866
10.046042	855.650514	11.080883
10.169886	851.545508	11.085901
10.192118	844.591618	11.090919
9.842190	854.123736	11.095936
9.958531	850.255562	11.100954
9.788920	845.805220	11.105971
10.022482	851.350989	11.110989
10.207259	849.070657	11.116007
10.126621	853.895248	11.121024
10.310673	849.214833	11.126042
10.070794	863.762798	11.131059
9.830216	853.925643	11.136077
9.952200	860.271224	11.141095
10.259122	869.805610	11.146112
10.443893	871.352220	11.151130
10.444476	880.342451	11.156147
10.461400	891.926227	11.161165
10.411284	888.039300	11.166183
10.533932	889.244265	11.171200
10.523534	881.157744	11.176218
10.014906	869.376219	11.181235
10.076934	881.324127	11.186253
10.677541	879.724359	11.191271
10.455958	891.041103	11.196288
10.639594	886.355825	11.201306
10.317686	888.102884	11.206323
10.398793	887.363254	11.211341
10.559000	882.235267	11.216359
10.418579	874.587493	11.221376
10.824190	869.772244	11.226394
10.435142	866.376304	11.231411
10.227227	864.298835	11.236429
10.231296	862.600638	11.241447
10.158712	875.897936	11.246464
10.331712	875.558211	11.251482
10.412779	875.198449	11.256499
10.405097	870.629228	11.261517
10.286985	874.981159	11.266535
10.083593	860.645465	11.271552
10.498505	859.548358	11.276570
10.430806	869.897092	11.281587
10.221616	866.572593	11.286605
10.499210	875.060226	11.291623
10.448944	890.801685	11.296640
10.916058	893.627804	11.301658
10.276601	893.366252	11.306675
10.675487	889.198463	11.311693
11.023633	897.978731	11.316711
10.982148	901.370125	11.321728
10.973682	876.995918	11.326746
10.368959	874.361093	11.331763
10.335701	862.423860	11.336781
10.425259	883.550389	11.341799
10.656492	894.852727	11.346816
10.706484	896.729241	11.351834
10.787181	907.108191	11.356851
10.679207	896.416745	11.361869
10.655347	887.735100	11.366887
10.469759	906.854702	11.371904
10.651640	907.371838	11.376922
10.981657	895.275545	11.381939
10.767185	899.952217	11.386957
10.917757	899.880133	11.391975
10.835119	904.873942	11.396992
10.953644	902.785427	11.402010
11.082613	907.136685	11.407027
11.000712	895.427903	11.412045
11.009415	896.568446	11.417063
10.661986	900.403447	11.422080
11.226975	892.660345	11.427098
10.892125	903.517349	11.432115
10.750803	889.918889	11.437133
10.953838	884.466748	11.442151
10.965709	900.845680	11.447168
11.171693	897.923157	11.452186
10.702661	873.219228	11.457203
10.916933	875.551387	11.462221
10.982285	882.462744	11.467239
10.913903	896.390957	11.472256
11.085023	882.043146	11.477274
10.916306	877.826271	11.482291
10.909533	871.563077	11.487309
11.324803	880.422582	11.492327
10.798765	879.114105	11.497344
10.997365	873.384005	11.502362
11.252614	876.289615	11.507379
11.027115	877.317309	11.512397
11.005021	875.501406	11.517415
10.690603	872.896152	11.522432
11.273443	877.545564	11.527450
11.257892	882.990804	11.532467
10.983561	878.489265	11.537485
10.992507	878.942671	11.542503
10.994478	897.279615	11.547520
11.004428	893.349694	11.552538
10.860932	895.450083	11.557555
10.938930	887.335960	11.562573
11.076892	894.918875	11.567591
10.983349	895.760814	11.572608
11.447693	892.289967	11.577626
11.525144	904.407955	11.582643
10.895265	900.443438	11.587661
11.286215	885.720175	11.592679
11.262321	895.218120	11.597696
11.216239	892.851937	11.602714
11.499935	894.958487	11.607731
11.035040	899.608838	11.612749
11.349287	903.455339	11.617767
10.959697	905.648358	11.622784
11.200826	895.278098	11.627802
11.163807	891.901522	11.632819
11.010222	894.337974	11.637837
11.165285	889.370454	11.642855
11.106625	905.107214	11.647872
11.097845	895.205351	11.652890
10.909215	892.852491	11.657907
10.659590	899.582284	11.662925
11.592169	917.584583	11.667943
11.504540	924.413973	11.672960
11.728379	925.610485	11.677978
11.340452	895.384337	11.682995
11.285120	901.308523	11.688013
11.277241	890.039606	11.693031
11.382820	922.835111	11.698048
11.436768	926.986405	11.703066
11.665674	927.504037	11.708083
11.394239	916.068649	11.713101
11.249604	904.627274	11.718119
11.424482	916.392215	11.723136
11.747806	925.889285	11.728154
11.601812	914.597119	11.733171
11.384230	911.898505	11.738189
11.557427	902.356266	11.743207
11.145141	919.534922	11.748224
11.395286	924.130095	11.753242
11.384352	921.308169	11.758259
11.343371	927.115642	11.763277
11.462292	928.880587	11.768295
11.435827	933.051077	11.773312
11.790251	936.457944	11.778330
11.941156	924.114696	11.783347
11.616932	934.455480	11.788365
11.780089	930.901152	11.793383
11.852226	925.943586	11.798400
11.332686	931.961032	11.803418
11.538512	934.687251	11.808435
11.337924	939.319324	11.813453
11.553432	934.371718	11.818471
11.639127	928.591172	11.823488
11.771265	930.368695	11.828506
11.872998	923.189854	11.833523
11.641160	936.046667	11.838541
11.503311	930.225517	11.843559
11.544368	931.328043	11.848576
11.270212	930.059419	11.853594
11.360534	925.855225	11.858611
11.239062	933.706982	11.863629
11.412627	935.693374	11.868647
11.481931	960.791240	11.873664
11.440387	963.316649	11.878682
11.368849	955.308096	11.883699
11.302251	955.400228	11.888717
11.809387	958.341183	11.893735
11.435951	969.773027	11.898752
11.391049	985.655997	11.903770
11.831541	985.565720	11.908787
11.968512	994.652358	11.913805
12.321129	992.211414	11.918823
11.911735	995.462085	11.923840
12.087829	991.710556	11.928858
11.912090	979.683804	11.933875
11.828817	982.457218	11.938893
11.857357	984.393578	11.943911
11.977241	985.973164	11.948928
12.249811	988.718870	11.953946
11.985260	972.259450	11.958963
11.630226	974.573914	11.963981
11.742300	990.529948	11.968999
11.246620	989.660274	11.974016
11.421489	994.759565	11.979034
11.911413	996.746038	11.984051
11.849688	1008.219295	11.989069
11.852460	997.990310	11.994087
12.105421	1002.137471	11.999104
11.676926	995.843935	12.004122
12.317667	1002.148524	12.009139
12.201765	1015.873510	12.014157
12.338493	1005.290346	12.019175
11.996885	992.032525	12.024192
12.289002	989.016039	12.029210
12.026875	980.653398	12.034227
11.860654	986.647706	12.039245
12.492516	1002.270645	12.044263
12.041577	1000.401995	12.049280
12.384528	1011.014995	12.054298
12.704242	994.813076	12.059315
12.321292	1006.025883	12.064333
12.264487	994.459903	12.069351
12.392329	991.614636	12.074368
12.102464	989.971889	12.079386
12.516475	982.615448	12.084403
12.323314	989.350907	12.089421
12.078662	988.862125	12.094439
12.513322	987.114011	12.099456
12.468001	985.502887	12.104474
12.038309	982.293334	12.109491
12.278499	977.165284	12.114509
11.964314	989.153012	12.119527
12.156868	984.316253	12.124544
12.129332	996.470361	12.129562
11.969276	996.941465	12.134579
12.083581	999.976674	12.139597
12.304374	1002.291242	12.144615
12.049145	993.653086	12.149632
12.317364	1013.489043	12.154650
12.884462	1003.829686	12.159667
12.556031	1016.088448	12.164685
12.282502	1010.686677	12.169703
12.472682	1016.763415	12.174720
12.471243	1019.593576	12.179738
12.590825	1012.724689	12.184755
12.650682	1008.879194	12.189773
12.710655	1003.267413	12.194791
12.645321	1011.939728	12.199808
12.645652	1023.220092	12.204826
12.838110	1020.438934	12.209843
12.654204	1007.107604	12.214861
12.450346	998.244257	12.219879
12.500312	998.252963	12.224896
12.242405	1007.985289	12.229914
12.346384	1013.942040	12.234931
12.596449	1026.296124	12.239949
12.811186	1024.429649	12.244967
12.695654	1025.824162	12.249984
12.628286	1033.760124	12.255002
13.176020	1014.001542	12.260019
12.640122	1007.902102	12.265037
12.900794	1007.683889	12.270055
12.737618	1000.794423	12.275072
12.325882	1009.502529	12.280090
12.753473	1008.287783	12.285107
12.628508	1010.616192	12.290125
12.513450	1018.290581	12.295143
12.956262	1011.190548	12.300160
12.491954	1029.257514	12.305178
12.679891	1024.739175	12.310195
12.638257	1027.082748	12.315213
12.349573	1022.059405	12.320231
12.903855	1015.278300	12.325248
12.633351	1028.194327	12.330266
12.757828	1021.542113	12.335283
12.534042	1027.286343	12.340301
12.656229	1023.468334	12.345319
12.928675	1013.045385	12.350336
12.777661	1021.125854	12.355354
13.176611	1010.508799	12.360371
13.278767	1019.865732	12.365389
13.275873	1024.582268	12.370407
13.100388	1017.576342	12.375424
13.099567	1018.832623	12.380442
13.035297	1026.210477	12.385459
13.398680	1023.364266	12.390477
13.339009	1021.229211	12.395495
13.471695	1019.634329	12.400512
13.021600	1012.346474	12.405530
13.038129	998.448251	12.410547
12.905553	990.997911	12.415565
12.700673	985.908967	12.420583
13.167768	1006.268066	12.425600
12.942726	1018.367246	12.430618
13.209924	1015.896129	12.435635
13.400084	1021.050571	12.440653
13.044532	1007.924943	12.445671
13.283682	991.333449	12.450688
13.241018	1001.281540	12.455706
13.005883	995.276079	12.460723
13.176838	1005.673443	12.465741
12.729948	1003.709058	12.470759
13.163530	995.328470	12.475776
13.019060	1020.210815	12.480794
13.339890	1021.405674	12.485811
13.148783	1017.075943	12.490829
13.281277	1018.316097	12.495847
13.305761	1015.902018	12.500864
13.119098	1023.288091	12.505882
13.124284	1020.214308	12.510899
13.116461	1029.536675	12.515917
13.393457	1026.533899	12.520935
13.163104	1021.234421	12.525952
13.378951	1020.229445	12.530970
13.280776	1024.906026	12.535987
13.307538	1021.904651	12.541005
13.369670	1026.379570	12.546023
13.550119	1017.940817	12.551040
13.381476	1017.107239	12.556058
13.422875	1020.553061	12.561075
13.529959	1019.899277	12.566093
13.544548	1021.981430	12.571111
13.198742	1026.212985	12.576128
13.288618	1025.867116	12.581146
13.565332	1021.701964	12.586163
13.374775	1014.629840	12.591181
13.449406	1025.932371	12.596199
13.340563	1018.146059	12.601216
13.660812	1029.126351	12.606234
13.203616	1022.737562	12.611251
13.359117	1020.925949	12.616269
13.438750	1016.380045	12.621287
13.397700	1028.334867	12.626304
13.515555	1025.673501	12.631322
13.281892	1024.434589	12.636339
13.454278	1018.669009	12.641357
13.319933	1032.665522	12.646375
13.277141	1018.314555	12.651392
13.427318	1020.434331	12.656410
13.469018	1040.283548	12.661427
13.939946	1046.567997	12.666445
13.812684	1053.648446	12.671463
13.885602	1037.010764	12.676480
13.529481	1028.243418	12.681498
13.494862	1016.777282	12.686515
13.745755	1029.152489	12.691533
13.528171	1048.398403	12.696551
13.569859	1043.137609	12.701568
13.797794	1051.174560	12.706586
13.349999	1054.395768	12.711603
13.633636	1042.285571	12.716621
13.388709	1049.525600	12.721639
14.004781	1052.820563	12.726656
13.689336	1061.622611	12.731674
13.509135	1050.947128	12.736691
13.781912	1053.383212	12.741709
13.273103	1057.446860	12.746727
13.612077	1055.958610	12.751744
13.993568	1063.528524	12.756762
13.766691	1065.684638	12.761779
13.996706	1076.931217	12.766797
13.785756	1084.853538	12.771815
13.876786	1075.443849	12.776832
13.872953	1076.493577	12.781850
13.818535	1081.029696	12.786867
14.066723	1079.055930	12.791885
14.015790	1091.670605	12.796903
13.651116	1087.591946	12.801920
13.850006	1081.110847	12.806938
13.868777	1074.630388	12.811955
14.238449	1084.205120	12.816973
14.224725	1090.379748	12.821991
13.873539	1088.129694	12.827008
14.128507	1086.060333	12.832026
13.940192	1080.998537	12.837043
13.934894	1078.860786	12.842061
14.131152	1090.999438	12.847079
14.261765	1083.321925	12.852096
13.976814	1089.814170	12.857114
14.170366	1086.967868	12.862131
14.392983	1078.889776	12.867149
13.973407	1090.245093	12.872167
14.289256	1082.448989	12.877184
14.392364	1089.409506	12.882202
13.887222	1096.184169	12.887219
14.228709	1082.939151	12.892237
14.133506	1086.293210	12.897255
14.250217	1089.182784	12.902272
14.507322	1096.917344	12.907290
14.079542	1094.938571	12.912307
13.995692	1093.495787	12.917325
13.978765	1090.529173	12.922343
14.144256	1094.894132	12.927360
14.079571	1093.039776	12.932378
13.930678	1104.585770	12.937395
14.270524	1105.914481	12.942413
14.600063	1116.499460	12.947431
14.624773	1119.467818	12.952448
14.422375	1125.245946	12.957466
14.420000	1127.267737	12.962483
14.250344	1122.878336	12.967501
14.052903	1117.012641	12.972519
14.650576	1113.201648	12.977536
14.692194	1129.039369	12.982554
14.552756	1132.938073	12.987571
15.007907	1120.191291	12.992589
14.841093	1100.362719	12.997607
14.690366	1095.282897	13.002624
15.017034	1095.270478	13.007642
14.558029	1092.253317	13.012659
14.813053	1085.966059	13.017677
14.474199	1094.291160	13.022695
14.723620	1079.634599	13.027712
14.705667	1092.218435	13.032730
14.457372	1084.202219	13.037747
14.715377	1076.897103	13.042765
14.624862	1087.778021	13.047783
14.819129	1082.258962	13.052800
14.841173	1084.815413	13.057818
14.627589	1087.502719	13.062835
14.917614	1088.935711	13.067853
14.745375	1095.457357	13.072871
14.937930	1091.579283	13.077888
15.193231	1082.964959	13.082906
14.623511	1088.340656	13.087923
14.697822	1093.449906	13.092941
14.567925	1088.617198	13.097959
14.546060	1079.137397	13.102976
14.677067	1081.996462	13.107994
14.275493	1081.342692	13.113011
14.980243	1080.692285	13.118029
15.109021	1078.341657	13.123047
14.915287	1075.126353	13.128064
15.090954	1074.889122	13.133082
14.925164	1084.680081	13.138099
14.820681	1084.599761	13.143117
14.724411	1083.208039	13.148135
14.742831	1071.215457	13.153152
14.997163	1076.792516	13.158170
14.583240	1085.941119	13.163187
14.750738	1082.812945	13.168205
15.084231	1084.545008	13.173223
14.748680	1088.184224	13.178240
15.268283	1109.786568	13.183258
14.923592	1106.915252	13.188275
15.125854	1094.690331	13.193293
15.030967	1091.521671	13.198311
15.247784	1106.227822	13.203328
15.193744	1098.104508	13.208346
14.601274	1106.778766	13.213363
15.199149	1110.297582	13.218381
15.237849	1112.109660	13.223399
15.027569	1120.604838	13.228416
15.438497	1117.930254	13.233434
15.288480	1122.588862	13.238451
15.260865	1106.234215	13.243469
15.333240	1106.960766	13.248487
14.922780	1099.412223	13.253504
15.326295	1100.016146	13.258522
15.227619	1106.722264	13.263539
15.208116	1117.838087	13.268557
15.118011	1119.826941	13.273575
14.645078	1126.780323	13.278592
15.293793	1119.428922	13.283610
15.146368	1123.341343	13.288627
15.286758	1117.391869	13.293645
15.191432	1125.383082	13.298663
15.160377	1126.329651	13.303680
15.258698	1118.278771	13.308698
15.163323	1123.164731	13.313715
15.273286	1135.007094	13.318733
15.416708	1127.644916	13.323751
14.852806	1124.523054	13.328768
15.632318	1141.013339	13.333786
15.408073	1148.720204	13.338803
15.211429	1143.552102	13.343821
15.427268	1160.058405	13.348839
15.470786	1157.433117	13.353856
15.710535	1143.756105	13.358874
15.483249	1148.753821	13.363891
15.614243	1147.181052	13.368909
15.711677	1147.155539	13.373927
15.542000	1154.882717	13.378944
15.437230	1141.241188	13.383962
15.280941	1151.267790	13.388979
15.175420	1153.712872	13.393997
15.157281	1150.038477	13.399015
14.984968	1148.719937	13.404032
15.920368	1163.440245	13.409050
15.846864	1159.360095	13.414067
16.130911	1151.724701	13.419085
15.727867	1138.025199	13.424103
15.453722	1151.995914	13.429120
15.925828	1146.644666	13.434138
15.889518	1145.055261	13.439155
16.063734	1146.700283	13.444173
16.277636	1138.789521	13.449191
16.215955	1137.471595	13.454208
16.439625	1147.204137	13.459226
15.839829	1153.931091	13.464243
15.912191	1141.317816	13.469261
16.011129	1145.374935	13.474279
15.754055	1141.432789	13.479296
15.929525	1141.812233	13.484314
15.881541	1142.643506	13.489331
15.718870	1144.844524	13.494349
16.094176	1150.342374	13.499367
15.946727	1153.334466	13.504384
16.073574	1133.554158	13.509402
16.251291	1139.435591	13.514419
16.047011	1150.925428	13.519437
16.270311	1145.951077	13.524455
15.837451	1144.028050	13.529472
15.974488	1135.208667	13.534490
15.866164	1143.809038	13.539507
15.924042	1149.325099	13.544525
16.035992	1157.839869	13.549543
16.013217	1151.964583	13.554560
15.847195	1136.659994	13.559578
15.758042	1156.292240	13.564595
16.000070	1148.705518	13.569613
16.171980	1143.346212	13.574631
16.152062	1152.863341	13.579648
16.311266	1141.628627	13.584666
16.183695	1143.448504	13.589683
15.804107	1138.422825	13.594701
16.027053	1144.161569	13.599719
15.709658	1150.823745	13.604736
16.225888	1154.321424	13.609754
16.165868	1175.615375	13.614771
16.144801	1176.377251	13.619789
16.131925	1182.858032	13.624807
16.218427	1186.672763	13.629824
16.305404	1177.999012	13.634842
16.270445	1178.496488	13.639859
16.610281	1177.303121	13.644877
16.644464	1171.645943	13.649895
16.508856	1177.691163	13.654912
16.563907	1168.723128	13.659930
16.389797	1179.985394	13.664947
16.371241	1183.621845	13.669965
16.431909	1176.958459	13.674983
16.351474	1190.697225	13.680000
16.412949	1171.041830	13.685018
15.995992	1178.104275	13.690035
15.725270	1187.524309	13.695053
16.167784	1185.342259	13.700071
16.490598	1207.395116	13.705088
16.361634	1202.419718	13.710106
16.484674	1210.672682	13.715123
16.926265	1208.619110	13.720141
16.772412	1209.226775	13.725159
16.580661	1211.275346	13.730176
16.982464	1202.074225	13.735194
16.790084	1206.028933	13.740211
16.751592	1204.564669	13.745229
16.890692	1207.569840	13.750247
16.901852	1208.167752	13.755264
16.775051	1194.188329	13.760282
16.827573	1189.689762	13.765299
16.794015	1186.474732	13.770317
17.022026	1173.091718	13.775335
16.843211	1168.899263	13.780352
16.858667	1161.716068	13.785370
16.769011	1177.019116	13.790387
16.633566	1178.364578	13.795405
17.060855	1170.308708	13.800423
16.936093	1176.777273	13.805440
17.287073	1171.424186	13.810458
17.045526	1168.127997	13.815475
16.753853	1163.485953	13.820493
16.904123	1172.468151	13.825511
16.841454	1184.416235	13.830528
16.929309	1177.274998	13.835546
16.815449	1172.951155	13.840563
16.863646	1175.323599	13.845581
16.846676	1184.509401	13.850599
17.181876	1201.156237	13.855616
17.221899	1202.872451	13.860634
17.573412	1198.303213	13.865651
17.121736	1191.167679	13.870669
17.054854	1172.920504	13.875687
16.848502	1166.554561	13.880704
16.742896	1181.850409	13.885722
17.042733	1196.413613	13.890739
16.995161	1199.482895	13.895757
16.975119	1198.691669	13.900775
16.820778	1207.354790	13.905792
16.995437	1201.967849	13.910810
16.900500	1204.915253	13.915827
16.986349	1218.308497	13.920845
17.283452	1207.433570	13.925863
17.039032	1208.489016	13.930880
17.213088	1202.426283	13.935898
17.350646	1218.582054	13.940915
16.937929	1238.301532	13.945933
17.501243	1234.718009	13.950951
17.280485	1239.999479	13.955968
17.797006	1227.159407	13.960986
17.541592	1230.240015	13.966003
17.403519	1226.659427	13.971021
17.409364	1221.633401	13.976039
17.440174	1225.539815	13.981056
17.478618	1225.194568	13.986074
17.776479	1223.987666	13.991091
17.419471	1214.325798	13.996109
17.781747	1195.992912	14.001127
17.532538	1194.761672	14.006144
17.349228	1189.426019	14.011162
17.533112	1198.053906	14.016179
17.384441	1215.938041	14.021197
17.986858	1209.410869	14.026215
17.719306	1216.885588	14.031232
17.712063	1203.063147	14.036250
17.636554	1186.752742	14.041267
17.335076	1207.144252	14.046285
17.672621	1209.426174	14.051303
17.345118	1231.397586	14.056320
17.816186	1219.674919	14.061338
17.780702	1234.964743	14.066355
17.741124	1231.328315	14.071373
18.076467	1216.271258	14.076391
17.677363	1236.355953	14.081408
17.870650	1223.102437	14.086426
18.035363	1222.926454	14.091443
17.652365	1223.695396	14.096461
18.051186	1220.607696	14.101479
18.214614	1219.198434	14.106496
18.110626	1208.503554	14.111514
17.923822	1199.872279	14.116531
17.969524	1200.936070	14.121549
17.895408	1192.057665	14.126567
18.156815	1191.056761	14.131584
17.901419	1183.295766	14.136602
18.246205	1190.192967	14.141619
17.771512	1200.434009	14.146637
17.823987	1193.780630	14.151655
17.989548	1210.449803	14.156672
17.950565	1220.543470	14.161690
18.372730	1214.214564	14.166707
17.853435	1222.374501	14.171725
17.818322	1215.154172	14.176743
17.904983	1224.136677	14.181760
18.281755	1220.421998	14.186778
18.098188	1225.335360	14.191795
17.933614	1229.462620	14.196813
18.505528	1226.848607	14.201831
18.188188	1231.828953	14.206848
18.450473	1225.045625	14.211866
18.393843	1222.117629	14.216883
17.849016	1229.519689	14.221901
17.908679	1224.381633	14.226919
17.841348	1223.988915	14.231936
17.671535	1226.511553	14.236954
18.466325	1229.097980	14.241971
18.004112	1233.153776	14.246989
17.980384	1236.673590	14.252007
18.260617	1242.137783	14.257024
18.094860	1255.691915	14.262042
18.638646	1248.939211	14.267059
18.688431	1257.494818	14.272077
18.881311	1256.628840	14.277095
18.474278	1250.871932	14.282112
18.480758	1252.834804	14.287130
18.618644	1236.051936	14.292147
18.491266	1252.526882	14.297165
18.872848	1252.978355	14.302183
18.786088	1245.761429	14.307200
17.955590	1243.227226	14.312218
18.393382	1233.577877	14.317235
18.018058	1250.710246	14.322253
18.478076	1250.324657	14.327271
18.384018	1255.756627	14.332288
18.404909	1256.562550	14.337306
18.844149	1244.720141	14.342323
18.331806	1241.390155	14.347341
18.653282	1242.256230	14.352359
18.681031	1256.526511	14.357376
18.599001	1277.768342	14.362394
19.008822	1273.603565	14.367411
18.786047	1268.579286	14.372429
18.974067	1262.672075	14.377447
19.048261	1258.100428	14.382464
18.598959	1256.904611	14.387482
18.682271	1256.649180	14.392499
18.605029	1276.043815	14.397517
19.165112	1272.275015	14.402535
19.388913	1264.957157	14.407552
19.096394	1271.452697	14.412570
19.146612	1247.861012	14.417587
18.691750	1259.224450	14.422605
18.903169	1242.357780	14.427623
18.896647	1249.071956	14.432640
19.100579	1265.495509	14.437658
18.995006	1276.604609	14.442675
18.939919	1278.017891	14.447693
18.685542	1277.616127	14.452711
19.033053	1275.298604	14.457728
19.013764	1277.499958	14.462746
18.934345	1269.022332	14.467763
18.677474	1273.035740	14.472781
18.980817	1275.612065	14.477799
19.516938	1278.887815	14.482816
18.967356	1285.856493	14.487834
19.463682	1282.310994	14.492851
19.090857	1274.023960	14.497869
19.197362	1280.614367	14.502887
19.224129	1269.653184	14.507904
19.320388	1277.772045	14.512922
19.452860	1278.098961	14.517939
19.129415	1289.146254	14.522957
19.019287	1274.394617	14.527975
19.368350	1272.588975	14.532992
19.286226	1293.337209	14.538010
19.782415	1307.177020	14.543027
19.093626	1301.769175	14.548045
19.362972	1303.374087	14.553063
19.559343	1302.310312	14.558080
19.608917	1305.777876	14.563098
19.654242	1297.234152	14.568115
19.419201	1298.706108	14.573133
19.687233	1300.712365	14.578151
19.948306	1294.815507	14.583168
19.461245	1289.436328	14.588186
19.886927	1274.601655	14.593203
19.827473	1276.905894	14.598221
19.812120	1270.916949	14.603239
19.465360	1279.437524	14.608256
19.550349	1281.093763	14.613274
19.565768	1265.379191	14.618291
19.363939	1279.829146	14.623309
19.521494	1292.090873	14.628327
19.685039	1287.643408	14.633344
19.254814	1303.980489	14.638362
20.111323	1304.036788	14.643379
19.978093	1301.703446	14.648397
19.957348	1301.657901	14.653415
20.105864	1297.397538	14.658432
19.791383	1297.405653	14.663450
20.142348	1289.222394	14.668467
19.867854	1296.396370	14.673485
19.974406	1299.416386	14.678503
19.981298	1295.349092	14.683520
19.840955	1299.658759	14.688538
19.975084	1286.978275	14.693555
20.255050	1289.035701	14.698573
20.113221	1299.094257	14.703591
20.180160	1285.158315	14.708608
19.988470	1286.152499	14.713626
19.835358	1290.087356	14.718643
20.084966	1293.609250	14.723661
20.008180	1281.776116	14.728679
20.391455	1281.893694	14.733696
19.938312	1300.188825	14.738714
20.455301	1296.831811	14.743731
20.355415	1295.187945	14.748749
20.381342	1309.674886	14.753767
20.094272	1284.690847	14.758784
19.871608	1299.534763	14.763802
20.181547	1289.577811	14.768819
19.675210	1296.226003	14.773837
19.912872	1298.762996	14.778855
20.038745	1293.501983	14.783872
19.930763	1301.899065	14.788890
19.908739	1301.246923	14.793907
20.218057	1318.949402	14.798925
20.226646	1314.855250	14.803943
20.072226	1329.677485	14.808960
20.404742	1332.588324	14.813978
20.525696	1322.695058	14.818995
20.952087	1324.921769	14.824013
20.354118	1322.811466	14.829031
20.796584	1325.175069	14.834048
20.633822	1326.871075	14.839066
20.705169	1325.977547	14.844083
20.480807	1322.717455	14.849101
20.564381	1329.382136	14.854119
20.494107	1322.314988	14.859136
20.170577	1322.354713	14.864154
20.127947	1325.886725	14.869171
20.295113	1322.950856	14.874189
20.300881	1325.676156	14.879207
20.729648	1331.617540	14.884224
20.822102	1350.910416	14.889242
20.716401	1337.401724	14.894259
20.832302	1333.574048	14.899277
20.832035	1330.174966	14.904295
20.730207	1321.294178	14.909312
20.973215	1340.543462	14.914330
20.741967	1330.857785	14.919347
20.944161	1332.743448	14.924365
20.974274	1347.885356	14.929383
21.022423	1346.514619	14.934400
20.921928	1358.516130	14.939418
21.198493	1351.415468	14.944435
21.000890	1334.648177	14.949453
20.716794	1332.512377	14.954471
21.528969	1330.409947	14.959488
20.920072	1321.634016	14.964506
20.856847	1315.972609	14.969523
21.032769	1329.991138	14.974541
20.936520	1343.192763	14.979559
21.237094	1346.473403	14.984576
21.029743	1351.473991	14.989594
20.896497	1343.438234	14.994611
21.460110	1341.965977	14.999629
21.309161	1349.300640	15.004647
21.808779	1341.096329	15.009664
21.400090	1327.658384	15.014682
21.141482	1325.709489	15.019699
21.338366	1319.099112	15.024717
21.226394	1321.452778	15.029735
21.615024	1309.326793	15.034752
21.235508	1314.986840	15.039770
21.093341	1316.013191	15.044787
21.372683	1321.245897	15.049805
21.260570	1338.762370	15.054823
21.620081	1339.900475	15.059840
21.795033	1339.485232	15.064858
21.525219	1327.476707	15.069875
21.289140	1314.294462	15.074893
21.161749	1333.330773	15.079911
21.677930	1343.926792	15.084928
21.284802	1344.446067	15.089946
21.280276	1337.003332	15.094963
21.688042	1340.096790	15.099981
21.203713	1346.157191	15.104999
21.356188	1338.444839	15.110016
21.430856	1342.698516	15.115034
21.570926	1338.514726	15.120051
21.711399	1332.765916	15.125069
21.734548	1346.053310	15.130087
21.818560	1335.833310	15.135104
21.628471	1344.577602	15.140122
21.470329	1347.542171	15.145139
21.674459	1340.769781	15.150157
21.527548	1368.068918	15.155175
21.913651	1373.450710	15.160192
22.163182	1373.912397	15.165210
21.901575	1369.824896	15.170227
21.960218	1369.096435	15.175245
22.191082	1366.669059	15.180263
22.119497	1357.132941	15.185280
21.799337	1341.565666	15.190298
21.724223	1348.510286	15.195315
21.909119	1357.521117	15.200333
22.034470	1370.230297	15.205351
22.160595	1372.544034	15.210368
22.312812	1369.358493	15.215386
22.045183	1363.262404	15.220403
21.961842	1346.410675	15.225421
22.112047	1368.222638	15.230439
22.068769	1365.100504	15.235456
22.440685	1374.484520	15.240474
22.211959	1376.878944	15.245491
22.205045	1374.008836	15.250509
22.422363	1368.567549	15.255527
22.569837	1367.479570	15.260544
22.447094	1350.526094	15.265562
22.220192	1345.385362	15.270579
22.165284	1329.666994	15.275597
21.995404	1347.553605	15.280615
22.469466	1362.169267	15.285632
22.344829	1365.580016	15.290650
22.378282	1369.299242	15.295667
22.462404	1369.409967	15.300685
22.484042	1377.353639	15.305703
22.572550	1376.860763	15.310720
22.255041	1374.134294	15.315738
22.428721	1381.690880	15.320755
22.746617	1376.542575	15.325773
22.539951	1370.004377	15.330791
22.586921	1383.781701	15.335808
22.340149	1371.530191	15.340826
22.422850	1390.334436	15.345843
22.766417	1380.326402	15.350861
22.608753	1373.658467	15.355879
22.796444	1360.939744	15.360896
22.605132	1370.581972	15.365914
22.130497	1371.811086	15.370931
22.746899	1367.977058	15.375949
22.447479	1366.151029	15.380967
22.421897	1366.754034	15.385984
22.803041	1372.972168	15.391002
22.791356	1407.866559	15.396019
23.121860	1399.522076	15.401037
22.753291	1404.176340	15.406055
22.844547	1398.249246	15.411072
22.989878	1393.092646	15.416090
22.809312	1398.223058	15.421107
23.318069	1387.946609	15.426125
22.894146	1407.763222	15.431143
22.766354	1402.912746	15.436160
23.009415	1395.684546	15.441178
22.819146	1394.203028	15.446195
23.065383	1397.431249	15.451213
22.952181	1398.784863	15.456231
22.859007	1397.466804	15.461248
22.840827	1395.441755	15.466266
22.832274	1401.416072	15.471283
23.171396	1393.691940	15.476301
22.948931	1398.050241	15.481319
23.064345	1417.865521	15.486336
23.465654	1424.387392	15.491354
23.349215	1433.824594	15.496371
23.624587	1420.584899	15.501389
23.573743	1408.885749	15.506407
23.430212	1394.164120	15.511424
23.173492	1396.664932	15.516442
23.108956	1404.122922	15.521459
23.553319	1414.436604	15.526477
23.685099	1416.772638	15.531495
22.710690	1418.173509	15.536512
23.221144	1418.687145	15.541530
23.453955	1434.941363	15.546547
23.793438	1426.353483	15.551565
23.411473	1426.810885	15.556583
23.744021	1424.275762	15.561600
23.638453	1419.468846	15.566618
23.439396	1425.894287	15.571635
23.842950	1418.837757	15.576653
23.949988	1430.032880	15.581671
23.508781	1437.862938	15.586688
23.718392	1418.654932	15.591706
23.506126	1427.279526	15.596723
23.768044	1434.106488	15.601741
23.855291	1422.167408	15.606759
23.607358	1421.214447	15.611776
23.914592	1412.821250	15.616794
23.943535	1421.784082	15.621811
23.846619	1417.545942	15.626829
23.822050	1406.435291	15.631847
23.603992	1417.791990	15.636864
24.086532	1411.299503	15.641882
24.018613	1414.020660	15.646899
23.784419	1410.700371	15.651917
23.965868	1408.714564	15.656935
23.649931	1408.055090	15.661952
23.923370	1404.107083	15.666970
23.977204	1414.163296	15.671987
24.230648	1428.423403	15.677005
24.212987	1424.659111	15.682023
24.141174	1405.606080	15.687040
24.073190	1412.243487	15.692058
23.922730	1420.424256	15.697075
24.382690	1422.379326	15.702093
24.385348	1433.315357	15.707111
24.432857	1424.963107	15.712128
24.681111	1425.139807	15.717146
24.199197	1411.941222	15.722163
24.359447	1408.992898	15.727181
24.312586	1413.209009	15.732199
24.439192	1429.427237	15.737216
24.383981	1429.434428	15.742234
24.317779	1427.646613	15.747251
24.289801	1424.245595	15.752269
24.566591	1429.534855	15.757287
24.314164	1432.208760	15.762304
24.661937	1421.560123	15.767322
24.689017	1430.483509	15.772339
24.684754	1438.228958	15.777357
24.957694	1430.902114	15.782375
24.657635	1438.309684	15.787392
25.029226	1428.154485	15.792410
24.600456	1421.272308	15.797427
24.545934	1417.690859	15.802445
24.947774	1427.231557	15.807463
24.518368	1432.127940	15.812480
24.815748	1434.850732	15.817498
24.635373	1433.325454	15.822515
24.634859	1439.842681	15.827533
24.854989	1434.599898	15.832551
24.723660	1432.560475	15.837568
24.759349	1436.074256	15.842586
24.546970	1435.644486	15.847603
24.275738	1437.229509	15.852621
24.599635	1442.396830	15.857639
24.659340	1440.060515	15.862656
25.107950	1456.035030	15.867674
24.988290	1461.125873	15.872691
25.260186	1458.881442	15.877709
25.397971	1449.893863	15.882727
25.039582	1447.706552	15.887744
25.324030	1428.033664	15.892762
25.390716	1430.389708	15.897779
25.226150	1417.634872	15.902797
25.399019	1424.514926	15.907815
24.991076	1430.291314	15.912832
25.061500	1420.937962	15.917850
25.204238	1434.027935	15.922867
25.124305	1428.231863	15.927885
25.290112	1435.633694	15.932903
24.968548	1456.538632	15.937920
25.432635	1449.062686	15.942938
25.189558	1461.108506	15.947955
25.431387	1455.116158	15.952973
25.702564	1452.371121	15.957991
25.773791	1448.483485	15.963008
25.818972	1454.474530	15.968026
25.711180	1451.763187	15.973043
25.311665	1427.908188	15.978061
25.615658	1444.151834	15.983079
25.352260	1456.129561	15.988096
25.938321	1443.572468	15.993114
25.699505	1446.934198	15.998131
25.368702	1449.388607	16.003149
25.815071	1449.358179	16.008167
25.477161	1461.627520	16.013184
25.903170	1456.817184	16.018202
25.655520	1451.933357	16.023219
25.644665	1447.080469	16.028237
26.072115	1449.631590	16.033255
26.033476	1452.521516	16.038272
26.016331	1449.565891	16.043290
25.921887	1449.214257	16.048307
25.818683	1451.002193	16.053325
25.869119	1441.715904	16.058343
25.568346	1452.429292	16.063360
26.040742	1457.497677	16.068378
26.109931	1447.789439	16.073395
25.896702	1454.053081	16.078413
25.883309	1451.773524	16.083431
25.750939	1456.399398	16.088448
25.553740	1452.371891	16.093466
25.698571	1456.248301	16.098483
25.815095	1474.065881	16.103501
25.833294	1472.270608	16.108519
25.687305	1476.537562	16.113536
26.023345	1469.356552	16.118554
26.047249	1485.318616	16.123571
26.036575	1485.918573	16.128589
26.584356	1494.464839	16.133607
26.609231	1488.597690	16.138624
26.505381	1484.685048	16.143642
26.558042	1484.751372	16.148659
26.288833	1471.176878	16.153677
26.690620	1462.354103	16.158695
26.510698	1473.818700	16.163712
26.843619	1472.637084	16.168730
26.568414	1477.054313	16.173747
26.086861	1479.840885	16.178765
26.784571	1469.258189	16.183783
26.050296	1476.103359	16.188800
26.274616	1485.825577	16.193818
26.668330	1497.505790	16.198835
26.576295	1513.226247	16.203853
27.120437	1507.884426	16.208871
26.703957	1501.777057	16.213888
26.811556	1500.673024	16.218906
27.119476	1509.699044	16.223923
26.935999	1496.010568	16.228941
26.795854	1474.562340	16.233959
26.438137	1480.257816	16.238976
26.875804	1489.599152	16.243994
26.978850	1494.120983	16.249011
26.959214	1494.621449	16.254029
26.923156	1499.326487	16.259047
27.051670	1507.250398	16.264064
27.087052	1493.415928	16.269082
27.104864	1491.889778	16.274099
27.412981	1493.618603	16.279117
27.439296	1484.297696	16.284135
27.538218	1480.437164	16.289152
26.941683	1472.302332	16.294170
27.459334	1460.339333	16.299187
27.207356	1461.373212	16.304205
27.338822	1448.601708	16.309223
27.480333	1458.145885	16.314240
27.315053	1457.603620	16.319258
27.086994	1464.067330	16.324275
27.369831	1463.700389	16.329293
27.402472	1450.521054	16.334311
27.011370	1466.399929	16.339328
27.279579	1455.750442	16.344346
27.449737	1469.922789	16.349363
27.194669	1478.501539	16.354381
27.807259	1489.377952	16.359399
27.524424	1489.447954	16.364416
27.538497	1487.542941	16.369434
27.659421	1486.609718	16.374451
27.606471	1499.730314	16.379469
27.687429	1484.279261	16.384487
27.421395	1491.340132	16.389504
27.454844	1497.295145	16.394522
27.643128	1490.048988	16.399539
27.423594	1491.865995	16.404557
27.771339	1487.948989	16.409575
27.694925	1491.133121	16.414592
27.221741	1491.095621	16.419610
27.539486	1488.098620	16.424627
27.395697	1501.117511	16.429645
27.627883	1510.377279	16.434663
27.732535	1509.922081	16.439680
27.955883	1523.349161	16.444698
27.866191	1521.521718	16.449715
27.980397	1522.813946	16.454733
27.711080	1522.442002	16.459751
27.819925	1524.859590	16.464768
27.931802	1521.728907	16.469786
28.415734	1512.509897	16.474803
28.073185	1525.119187	16.479821
28.254475	1518.292037	16.484839
28.238997	1508.356639	16.489856
28.101770	1508.251022	16.494874
27.950338	1520.762592	16.499891
28.008333	1517.201103	16.504909
28.747912	1524.944916	16.509927
28.467057	1517.241692	16.514944
28.229105	1510.380494	16.519962
28.422657	1499.925182	16.524979
28.233403	1506.758043	16.529997
28.484358	1532.115960	16.535015
28.611024	1531.072350	16.540032
28.705600	1523.935746	16.545050
28.830981	1504.797648	16.550067
28.082963	1507.003531	16.555085
28.087856	1511.691177	16.560103
28.353170	1519.109080	16.565120
28.480101	1544.384967	16.570138
28.778074	1529.995317	16.575155
28.519482	1535.002661	16.580173
28.851508	1524.367381	16.585191
28.676513	1533.453143	16.590208
28.131640	1541.510989	16.595226
28.354563	1534.587395	16.600243
28.214365	1535.801995	16.605261
28.311913	1551.520095	16.610279
28.641109	1554.079008	16.615296
28.465597	1558.539424	16.620314
29.050557	1561.663284	16.625331
28.944609	1562.198880	16.630349
28.948966	1554.973049	16.635367
29.144408	1562.333040	16.640384
29.175901	1556.936961	16.645402
29.401878	1551.431588	16.650419
29.259535	1547.942367	16.655437
29.323560	1550.196913	16.660455
29.243783	1549.250402	16.665472
29.291222	1553.094906	16.670490
29.314602	1543.132201	16.675507
29.271101	1543.845052	16.680525
29.471784	1549.308133	16.685543
29.632353	1548.111494	16.690560
29.439754	1551.421717	16.695578
29.949408	1545.861790	16.700595
29.361161	1538.196560	16.705613
29.367631	1533.496472	16.710631
29.278578	1531.336284	16.715648
29.347648	1549.486952	16.720666
29.915627	1535.398897	16.725683
29.701098	1537.898269	16.730701
29.657430	1544.590173	16.735719
29.870089	1534.453296	16.740736
29.670549	1521.558501	16.745754
29.922403	1506.112054	16.750771
29.611294	1513.389611	16.755789
29.669244	1518.166904	16.760807
29.517684	1521.327836	16.765824
29.435065	1546.954263	16.770842
29.982806	1535.220263	16.775859
29.733803	1540.647628	16.780877
29.873915	1547.860672	16.785895
29.888638	1543.063165	16.790912
29.843605	1546.096274	16.795930
29.883838	1550.680268	16.800947
29.366077	1549.463461	16.805965
29.501053	1546.008914	16.810983
29.790927	1548.029309	16.816000
29.717000	1552.533559	16.821018
30.043466	1550.008672	16.826035
29.750149	1566.591090	16.831053
29.829499	1575.528164	16.836071
29.710630	1581.641634	16.841088
30.085621	1578.122616	16.846106
30.304564	1577.232631	16.851123
29.975384	1573.716413	16.856141
30.011012	1586.232159	16.861159
30.281003	1574.479469	16.866176
30.132559	1591.686521	16.871194
30.430987	1584.564621	16.876211
30.339653	1602.718240	16.881229
30.173344	1608.184516	16.886247
30.657411	1599.724204	16.891264
30.815109	1602.880300	16.896282
30.888828	1594.263617	16.901299
30.664891	1588.749324	16.906317
30.498544	1579.319663	16.911335
30.651980	1562.848204	16.916352
30.679369	1566.215766	16.921370
30.371920	1550.768013	16.926387
30.632901	1568.574427	16.931405
30.661630	1586.770384	16.936423
30.914559	1592.284091	16.941440
30.850857	1603.562078	16.946458
30.968493	1598.389714	16.951475
30.687109	1593.072686	16.956493
31.030278	1595.143722	16.961511
31.051950	1595.722001	16.966528
30.870852	1605.462283	16.971546
30.799611	1596.035593	16.976563
31.036654	1594.761557	16.981581
30.870127	1596.102547	16.986599
31.069992	1593.582435	16.991616
31.028644	1592.941346	16.996634
31.468153	1589.011709	17.001651
31.282197	1595.613972	17.006669
31.220213	1585.202800	17.011687
31.429347	1588.043932	17.016704
31.154057	1591.305631	17.021722
30.864613	1589.293891	17.026739
31.252499	1592.006282	17.031757
31.044194	1601.933518	17.036775
31.155791	1595.093641	17.041792
31.095653	1612.106418	17.046810
31.390496	1599.603623	17.051827
31.106559	1589.883187	17.056845
31.189684	1611.868177	17.061863
31.534008	1612.828127	17.066880
31.690373	1612.597424	17.071898
32.216933	1598.929102	17.076915
31.940073	1597.888400	17.081933
31.837585	1593.813317	17.086951
31.640776	1591.411312	17.091968
31.734901	1591.004499	17.096986
31.734591	1587.988198	17.102003
31.786411	1580.106357	17.107021
31.633104	1572.867798	17.112039
32.221431	1578.540420	17.117056
31.761437	1582.674670	17.122074
31.899588	1583.637983	17.127091
31.850147	1586.350802	17.132109
31.808534	1589.610691	17.137127
32.112938	1578.528218	17.142144
31.325767	1588.501309	17.147162
31.875652	1600.883859	17.152179
32.213106	1612.574048	17.157197
32.185057	1617.548240	17.162215
32.162206	1620.692252	17.167232
31.934420	1623.868951	17.172250
32.308250	1628.159479	17.177267
32.627076	1623.221152	17.182285
31.996582	1620.702053	17.187303
32.264249	1609.295942	17.192320
32.016789	1628.921096	17.197338
32.290340	1633.093764	17.202355
32.492056	1629.680329	17.207373
32.216425	1638.229499	17.212391
32.435691	1639.399268	17.217408
32.263381	1631.049182	17.222426
32.671419	1624.547071	17.227443
32.448713	1624.480379	17.232461
32.211415	1622.346251	17.237479
32.411726	1632.831304	17.242496
32.752200	1644.082090	17.247514
32.833353	1642.653123	17.252531
32.765146	1656.622147	17.257549
32.665089	1646.318396	17.262567
33.154350	1635.407674	17.267584
32.695633	1624.242641	17.272602
32.373318	1609.998923	17.277619
32.811784	1630.559820	17.282637
32.679965	1634.024958	17.287655
32.888541	1638.987610	17.292672
32.618423	1642.998185	17.297690
32.719720	1642.859644	17.302707
33.007427	1626.222047	17.307725
33.006412	1640.179165	17.312743
33.280166	1634.185211	17.317760
33.083243	1630.044435	17.322778
32.628280	1634.504603	17.327795
33.025971	1638.910076	17.332813
32.887118	1651.440930	17.337831
33.090306	1654.070285	17.342848
32.984635	1658.952605	17.347866
33.356849	1663.786462	17.352883
33.273591	1664.294297	17.357901
33.254935	1663.945290	17.362919
33.184169	1655.386501	17.367936
33.154385	1665.535429	17.372954
33.250807	1663.240645	17.377971
33.491438	1664.170889	17.382989
33.003260	1662.332124	17.388007
33.432195	1678.885060	17.393024
33.319392	1681.530619	17.398042
33.372411	1687.739333	17.403059
34.240323	1673.492937	17.408077
33.979844	1690.572370	17.413095
34.448821	1674.771601	17.418112
34.563528	1653.043631	17.423130
34.248373	1635.581146	17.428147
34.347877	1634.025933	17.433165
34.458844	1637.688719	17.438183
34.534595	1632.357536	17.443200
34.227122	1627.751028	17.448218
34.216285	1621.278774	17.453235
34.441895	1598.844836	17.458253
34.230821	1597.373231	17.463271
34.091862	1590.023840	17.468288
34.266769	1601.784185	17.473306
34.122012	1602.264785	17.478323
34.350613	1598.837269	17.483341
33.891825	1597.000741	17.488359
34.066531	1590.932041	17.493376
34.450155	1597.886978	17.498394
34.185392	1601.097536	17.503411
34.395662	1595.542976	17.508429
33.953253	1604.834765	17.513447
34.198631	1608.435179	17.518464
34.224627	1630.456996	17.523482
34.254523	1632.889813	17.528499
34.526127	1629.202850	17.533517
34.464075	1642.432541	17.538535
34.470561	1636.754377	17.543552
34.530195	1638.347334	17.548570
34.440532	1639.016249	17.553587
34.684898	1632.062889	17.558605
34.768099	1634.214487	17.563623
34.556692	1638.654876	17.568640
34.702036	1638.582867	17.573658
34.550917	1637.251728	17.578675
34.777007	1632.221648	17.583693
34.500633	1640.935490	17.588711
34.766381	1662.981506	17.593728
34.778554	1658.229656	17.598746
34.838468	1665.761093	17.603763
35.016774	1662.510755	17.608781
34.841985	1682.726461	17.613799
35.094260	1670.789639	17.618816
35.064540	1665.571139	17.623834
34.788684	1673.180900	17.628851
35.376936	1669.760463	17.633869
34.825369	1671.385143	17.638887
34.937189	1666.758147	17.643904
35.485483	1661.847233	17.648922
34.728959	1672.122956	17.653939
35.687346	1683.361215	17.658957
35.294415	1694.028392	17.663975
35.508131	1699.160274	17.668992
35.770327	1688.417734	17.674010
35.358750	1690.435379	17.679027
35.512588	1687.675837	17.684045
35.288818	1700.666977	17.689063
35.376556	1696.262038	17.694080
35.785909	1702.094387	17.699098
35.766309	1700.310254	17.704115
35.902120	1690.826654	17.709133
35.770100	1696.819128	17.714151
35.678904	1689.947965	17.719168
35.836380	1704.581040	17.724186
35.827534	1701.773585	17.729203
35.882971	1692.866789	17.734221
35.692583	1693.770635	17.739239
35.960054	1689.986714	17.744256
36.335840	1695.144956	17.749274
35.978787	1690.259055	17.754291
36.013155	1690.371115	17.759309
36.068093	1694.945636	17.764327
35.867364	1692.110647	17.769344
36.383734	1693.266162	17.774362
35.832125	1705.766266	17.779379
36.050094	1697.455377	17.784397
35.893770	1693.192532	17.789415
36.003761	1706.923712	17.794432
36.248073	1713.098856	17.799450
36.083901	1721.042903	17.804467
36.370627	1723.078604	17.809485
36.432881	1726.429416	17.814503
36.143147	1728.023036	17.819520
36.683187	1713.357018	17.824538
36.653032	1720.885652	17.829555
36.782213	1712.541598	17.834573
36.508304	1715.288581	17.839591
36.989232	1711.612081	17.844608
36.975169	1720.526098	17.849626
36.713335	1731.381653	17.854643
36.528027	1724.586454	17.859661
36.672435	1718.938219	17.864679
36.663308	1723.872314	17.869696
36.827939	1706.670385	17.874714
36.539875	1729.910066	17.879731
36.945437	1706.179437	17.884749
36.877084	1725.456252	17.889767
37.038082	1736.664136	17.894784
37.517026	1727.407441	17.899802
37.020985	1730.147636	17.904819
37.097580	1729.265224	17.909837
37.138730	1739.779998	17.914855
37.082733	1740.971448	17.919872
37.507548	1742.788487	17.924890
37.484811	1738.440765	17.929907
37.587865	1720.692952	17.934925
36.930936	1710.799457	17.939943
37.156394	1732.500890	17.944960
37.818832	1732.484555	17.949978
37.150263	1743.724821	17.954995
37.747351	1739.016822	17.960013
37.600026	1743.384060	17.965031
37.495489	1746.226668	17.970048
37.546547	1736.957223	17.975066
37.524677	1752.609051	17.980083
37.533118	1747.786144	17.985101
37.505109	1751.109560	17.990119
37.254264	1748.811725	17.995136
37.719035	1748.941626	18.000154
37.553061	1751.343648	18.005171
37.510670	1739.873534	18.010189
37.700615	1748.259417	18.015207
37.600728	1752.646374	18.020224
37.574840	1765.478895	18.025242
37.462078	1766.786410	18.030259
37.578830	1762.005830	18.035277
37.635686	1770.035804	18.040295
37.827657	1782.988227	18.045312
38.194699	1785.495064	18.050330
38.189463	1794.714326	18.055347
38.466680	1774.579247	18.060365
38.269640	1788.420680	18.065383
38.400455	1791.280894	18.070400
38.624465	1788.457184	18.075418
38.252124	1796.230180	18.080435
38.376853	1784.771191	18.085453
38.515396	1796.918955	18.090471
38.359381	1786.457051	18.095488
38.726463	1779.998254	18.100506
38.300922	1788.528386	18.105523
38.483134	1794.000118	18.110541
38.637226	1784.180010	18.115559
38.438028	1786.656024	18.120576
38.611341	1775.388796	18.125594
38.834739	1780.491943	18.130611
38.545416	1778.275848	18.135629
38.643250	1785.298767	18.140647
38.767047	1791.157672	18.145664
38.837605	1782.882316	18.150682
38.590420	1798.577134	18.155699
38.802767	1811.834254	18.160717
39.043711	1816.120618	18.165735
38.859033	1815.365621	18.170752
39.300511	1817.391508	18.175770
39.211665	1815.227309	18.180787
39.165669	1811.126890	18.185805
39.669757	1805.774267	18.190823
39.615162	1807.386314	18.195840
39.599766	1808.458276	18.200858
39.372905	1807.990932	18.205875
39.418287	1810.185611	18.210893
39.570796	1806.899549	18.215911
39.341168	1810.625353	18.220928
39.694218	1795.527016	18.225946
39.508165	1809.580017	18.230963
39.775477	1810.500349	18.235981
40.048998	1808.374683	18.240999
39.518752	1796.441895	18.246016
39.712352	1794.839623	18.251034
39.607198	1790.981049	18.256051
39.583226	1798.683878	18.261069
39.634176	1810.573911	18.266087
39.509669	1814.404774	18.271104
39.682797	1810.419507	18.276122
39.712447	1804.318794	18.281139
39.625183	1801.348905	18.286157
39.871923	1797.490438	18.291175
39.780236	1807.901436	18.296192
39.497845	1793.270870	18.301210
39.828900	1809.588967	18.306227
39.768676	1834.681122	18.311245
40.121650	1839.105066	18.316263
39.787681	1840.269632	18.321280
39.944607	1834.747029	18.326298
40.096920	1836.849639	18.331315
39.935753	1833.236508	18.336333
40.272627	1838.513423	18.341351
40.298045	1857.276530	18.346368
40.709971	1856.365858	18.351386
40.940611	1858.452574	18.356403
40.894610	1857.540616	18.361421
40.867485	1842.661933	18.366439
40.465044	1847.042621	18.371456
40.882455	1829.231909	18.376474
40.754569	1826.411036	18.381491
40.639667	1828.412345	18.386509
40.832787	1828.175960	18.391527
40.672702	1848.055037	18.396544
41.193224	1854.711708	18.401562
41.119049	1849.087540	18.406579
40.625225	1838.590293	18.411597
40.820269	1839.574927	18.416615
41.257591	1856.176664	18.421632
40.934507	1853.571096	18.426650
41.234569	1852.592305	18.431667
40.770952	1861.540934	18.436685
41.142504	1850.862682	18.441703
40.900061	1850.777992	18.446720
41.169207	1842.242643	18.451738
41.017154	1844.224309	18.456755
41.084676	1864.728329	18.461773
41.423152	1855.810685	18.466791
41.013215	1856.912421	18.471808
41.773715	1866.768300	18.476826
41.814282	1875.622596	18.481843
41.460135	1875.225295	18.486861
41.735988	1880.387123	18.491879
41.372794	1891.787443	18.496896
41.798290	1884.636141	18.501914
41.991264	1872.852649	18.506931
41.834675	1877.570831	18.511949
41.804030	1881.386593	18.516967
42.245339	1886.225636	18.521984
42.019046	1864.851921	18.527002
41.363774	1860.373284	18.532019
41.682058	1867.098417	18.537037
41.866363	1866.222998	18.542055
41.556367	1873.052157	18.547072
41.473674	1876.514742	18.552090
41.837258	1875.048529	18.557107
41.402204	1902.752692	18.562125
42.170695	1906.549183	18.567143
41.976305	1915.731279	18.572160
41.941247	1910.009688	18.577178
42.033458	1907.104007	18.582195
42.008800	1897.076971	18.587213
42.383610	1909.779228	18.592231
42.504960	1933.985516	18.597248
42.691906	1932.290441	18.602266
42.330148	1922.425188	18.607283
42.649842	1932.743093	18.612301
42.868171	1921.356519	18.617319
42.555171	1931.143997	18.622336
42.671911	1931.475891	18.627354
42.529656	1930.380443	18.632371
42.811332	1935.949361	18.637389
43.315512	1934.928567	18.642407
43.101719	1928.650929	18.647424
43.078068	1925.687824	18.652442
43.023343	1909.679096	18.657459
42.922532	1922.458782	18.662477
42.992733	1912.499910	18.667495
43.245621	1926.694240	18.672512
43.091750	1926.338046	18.677530
43.158119	1922.503451	18.682547
43.023985	1933.917716	18.687565
43.569241	1923.789396	18.692583
43.332357	1923.866173	18.697600
43.337621	1927.674240	18.702618
43.323278	1930.968470	18.707635
42.946086	1926.352135	18.712653
42.902049	1925.962438	18.717671
43.240664	1929.565038	18.722688
43.144326	1928.250802	18.727706
43.286471	1929.220957	18.732723
43.165372	1935.837251	18.737741
43.541490	1946.880420	18.742759
43.297539	1952.893851	18.747776
43.363348	1957.860909	18.752794
43.698690	1955.607695	18.757811
43.769165	1953.823017	18.762829
43.875613	1946.845462	18.767847
43.662276	1961.827632	18.772864
43.615603	1970.203727	18.777882
44.102476	1976.639260	18.782899
44.592100	1983.362505	18.787917
44.812157	1967.770865	18.792935
44.551385	1952.183314	18.797952
44.321401	1937.350463	18.802970
44.666105	1932.050708	18.807987
44.480382	1934.142271	18.813005
44.603703	1937.229517	18.818023
44.550668	1943.792445	18.823040
44.418256	1941.779115	18.828058
44.512731	1928.764334	18.833075
44.598297	1931.157489	18.838093
44.372078	1928.116845	18.843111
44.801921	1940.476993	18.848128
44.458221	1934.421394	18.853146
44.515439	1931.727575	18.858163
44.885941	1943.966835	18.863181
44.579087	1937.437471	18.868199
44.503484	1942.881593	18.873216
44.698058	1950.311592	18.878234
45.031168	1963.214271	18.883251
44.500127	1978.230064	18.888269
44.978575	1965.302967	18.893287
44.983738	1979.126508	18.898304
44.720327	1975.172398	18.903322
45.091057	1964.480622	18.908339
44.900128	1975.731288	18.913357
45.071610	1956.432663	18.918375
44.942491	1962.154902	18.923392
44.944294	1983.614343	18.928410
46.098833	1980.883850	18.933427
45.300630	1970.885000	18.938445
45.661643	1958.055262	18.943463
45.443403	1955.331376	18.948480
45.609150	1952.038568	18.953498
45.876193	1951.790555	18.958515
45.502992	1963.705331	18.963533
45.570224	1953.157213	18.968551
45.834121	1951.949374	18.973568
45.611382	1959.857360	18.978586
45.790156	1955.916394	18.983603
45.568092	1975.846426	18.988621
45.896278	1973.306819	18.993639
46.064569	1990.975707	18.998656
46.053880	1977.915868	19.003674
46.326207	1978.252756	19.008691
46.280795	1987.898028	19.013709
46.126021	1973.635536	19.018727
46.026190	1960.750270	19.023744
46.245334	1977.722416	19.028762
46.279089	1972.720271	19.033779
46.376627	1977.336454	19.038797
46.149938	1974.049837	19.043815
46.471191	1966.428956	19.048832
46.295618	1985.269327	19.053850
46.355933	1974.703048	19.058867
46.548873	1979.839442	19.063885
46.407797	1971.864289	19.068903
46.715098	1970.430202	19.073920
46.259530	1963.979531	19.078938
46.562344	1968.707642	19.083955
46.532923	1965.897043	19.088973
46.417981	1976.541702	19.093991
46.760052	1991.144347	19.099008
46.578288	2005.367865	19.104026
46.876613	2005.763839	19.109043
46.749581	2003.549629	19.114061
47.027661	1995.171171	19.119079
46.896710	2001.758022	19.124096
46.840457	2004.924559	19.129114
47.317321	1984.226142	19.134131
47.184198	1999.831652	19.139149
47.222594	1985.570688	19.144167
47.382154	1990.065218	19.149184
47.231840	1998.630881	19.154202
47.140578	1999.802787	19.159219
47.358808	2006.708281	19.164237
47.647726	2021.676992	19.169255
47.850533	2016.638432	19.174272
47.694148	2006.404964	19.179290
47.853396	1999.919797	19.184307
47.601774	1997.185673	19.189325
47.593257	2000.876558	19.194343
47.689564	2015.948347	19.199360
47.565732	2019.701990	19.204378
47.888542	2031.359095	19.209395
48.120213	2024.263182	19.214413
47.820208	2021.981892	19.219431
47.875571	2017.011395	19.224448
47.329956	2022.598762	19.229466
48.187108	2024.764629	19.234483
48.113159	2021.338008	19.239501
48.042779	2025.546362	19.244519
48.267319	2020.984286	19.249536
47.830554	2025.805698	19.254554
47.834356	2038.510126	19.259571
47.944379	2047.434729	19.264589
48.213126	2055.108799	19.269607
48.477847	2045.978058	19.274624
47.984615	2053.319031	19.279642
48.176244	2046.765901	19.284659
48.515692	2049.440517	19.289677
48.442115	2055.948428	19.294695
48.763367	2078.558063	19.299712
48.957665	2080.051456	19.304730
49.244109	2080.639930	19.309747
49.254154	2077.523208	19.314765
49.139809	2063.082116	19.319783
49.189497	2040.940562	19.324800
49.049415	2037.499671	19.329818
49.102431	2030.994058	19.334835
49.055946	2035.902343	19.339853
49.280315	2034.146943	19.344871
49.246164	2040.090505	19.349888
49.067086	2039.741820	19.354906
49.164616	2036.100849	19.359923
49.520227	2050.556641	19.364941
49.392013	2045.677490	19.369959
49.650045	2040.002684	19.374976
49.376976	2036.036769	19.379994
49.368219	2057.908064	19.385011
49.587066	2072.154409	19.390029
49.353240	2077.447968	19.395047
49.795103	2063.980423	19.400064
49.282765	2075.132713	19.405082
49.477123	2073.354318	19.410099
49.485546	2063.468742	19.415117
49.554737	2071.586985	19.420135
49.684528	2069.332293	19.425152
49.437566	2088.482987	19.430170
49.863498	2101.700535	19.435187
50.161347	2095.190455	19.440205
49.939025	2096.096058	19.445223
50.140979	2092.672051	19.450240
50.358345	2090.076926	19.455258
50.210550	2096.730178	19.460275
49.947889	2097.989860	19.465293
50.031140	2101.349094	19.470311
50.231513	2097.456881	19.475328
50.327080	2114.924955	19.480346
50.520926	2109.788444	19.485363
50.397510	2113.227303	19.490381
50.247185	2120.532506	19.495399
50.036886	2112.128991	19.500416
50.236041	2118.673544	19.505434
50.830997	2129.675169	19.510451
51.133345	2142.757675	19.515469
50.884060	2130.747883	19.520487
51.342601	2130.511920	19.525504
50.873203	2121.135944	19.530522
50.914782	2114.462317	19.535539
51.000112	2114.354362	19.540557
50.978571	2122.826969	19.545575
51.746132	2133.189688	19.550592
51.170125	2141.537808	19.555610
51.379888	2139.965702	19.560627
51.270659	2139.087205	19.565645
51.204289	2153.124282	19.570663
51.364760	2140.019093	19.575680
51.464413	2142.071988	19.580698
51.513870	2146.686129	19.585715
51.549141	2134.618090	19.590733
51.470388	2149.282752	19.595751
51.778328	2136.714963	19.600768
51.447406	2137.999117	19.605786
51.659152	2145.512587	19.610803
51.645431	2131.000280	19.615821
51.570748	2133.137294	19.620839
51.999132	2138.192907	19.625856
52.042474	2158.752884	19.630874
51.865258	2159.078639	19.635891
52.178802	2156.154445	19.640909
51.979219	2162.372026	19.645927
52.423270	2150.053563	19.650944
52.461213	2160.025299	19.655962
52.681525	2157.742644	19.660979
52.530782	2137.362484	19.665997
52.090381	2135.903528	19.671015
52.285165	2145.892639	19.676032
52.446659	2141.418697	19.681050
52.348987	2153.570938	19.686067
52.897781	2158.171458	19.691085
52.500553	2162.881268	19.696103
52.784746	2147.482574	19.701120
52.748463	2154.111714	19.706138
52.642594	2157.684877	19.711155
52.786610	2152.333179	19.716173
52.406709	2152.743015	19.721191
52.841287	2146.189455	19.726208
53.069924	2143.701703	19.731226
52.637345	2156.795245	19.736243
52.899672	2155.756142	19.741261
52.770765	2171.966003	19.746279
52.719406	2169.621556	19.751296
53.236505	2177.387511	19.756314
53.055454	2186.384112	19.761331
53.238972	2182.583633	19.766349
53.161302	2187.972084	19.771367
53.201717	2180.199491	19.776384
53.304029	2203.041145	19.781402
53.361771	2218.009669	19.786419
53.536368	2215.956198	19.791437
53.657320	2213.417927	19.796455
53.617995	2202.702615	19.801472
53.994293	2216.055423	19.806490
53.737800	2207.006388	19.811507
53.978923	2210.417898	19.816525
53.838018	2211.398629	19.821543
54.224701	2212.834458	19.826560
54.439228	2207.548445	19.831578
54.076358	2206.964400	19.836595
54.315516	2197.446090	19.841613
54.169366	2203.510577	19.846631
54.201110	2207.602899	19.851648
54.095650	2211.509840	19.856666
54.213720	2228.610374	19.861683
54.433172	2224.134507	19.866701
54.199807	2236.991274	19.871719
54.135395	2221.972728	19.876736
54.716169	2240.167002	19.881754
54.430281	2237.476487	19.886771
54.836293	2228.716945	19.891789
54.504568	2240.434935	19.896807
54.535727	2228.552332	19.901824
54.992223	2224.750233	19.906842
54.964073	2242.598319	19.911859
54.934299	2249.546284	19.916877
54.871820	2258.323346	19.921895
55.585396	2252.517872	19.926912
55.397069	2262.671740	19.931930
55.309932	2259.814528	19.936947
55.415693	2242.752234	19.941965
55.128952	2234.670712	19.946983
55.268286	2238.324229	19.952000
55.655700	2245.021768	19.957018
55.268510	2257.101076	19.962035
55.785358	2248.079525	19.967053
55.612025	2253.649150	19.972071
55.689452	2256.292896	19.977088
55.728771	2250.181355	19.982106
55.706946	2252.720251	19.987123
55.656496	2250.907297	19.992141
56.022881	2248.107218	19.997159
55.945676	2248.017067	20.002176
56.123051	2250.984428	20.007194
55.941867	2248.406324	20.012211
56.069812	2244.183351	20.017229
55.870974	2238.447171	20.022247
55.862776	2235.291308	20.027264
56.101804	2226.610343	20.032282
55.732322	2236.992739	20.037299
55.939533	2256.793733	20.042317
56.277897	2268.452581	20.047335
56.143650	2272.069236	20.052352
56.313886	2265.491992	20.057370
56.381768	2265.099734	20.062387
56.386214	2271.738335	20.067405
56.435023	2280.519853	20.072423
56.180146	2290.650684	20.077440
56.469998	2285.139811	20.082458
56.477318	2308.739787	20.087475
56.933834	2297.279720	20.092493
56.977715	2306.527586	20.097511
57.080757	2299.949818	20.102528
56.895831	2310.039576	20.107546
56.994661	2306.662090	20.112563
57.108196	2300.730378	20.117581
56.977004	2303.852671	20.122599
57.498546	2314.134918	20.127616
57.195615	2326.759178	20.132634
57.417459	2331.072660	20.137651
57.688442	2325.520011	20.142669
57.958498	2324.873098	20.147687
57.927202	2318.853903	20.152704
58.084741	2311.472492	20.157722
57.832219	2298.941878	20.162739
57.975009	2281.137449	20.167757
57.717358	2282.741569	20.172775
57.774353	2289.619509	20.177792
58.491339	2284.074662	20.182810
57.676542	2284.492003	20.187827
58.045264	2287.384448	20.192845
58.186501	2308.203034	20.197863
57.799990	2312.564685	20.202880
58.175981	2308.897318	20.207898
57.959365	2326.594177	20.212915
58.252504	2322.788933	20.217933
58.448238	2313.215528	20.222951
58.037120	2318.587085	20.227968
58.269769	2300.804986	20.232986
58.504445	2320.357839	20.238003
58.834660	2327.510112	20.243021
58.281686	2324.466893	20.248039
58.518853	2340.564668	20.253056
58.774829	2342.480346	20.258074
58.900598	2353.966925	20.263091
59.145876	2340.594812	20.268109
59.236032	2343.998821	20.273127
58.548294	2344.382569	20.278144
58.857432	2342.428297	20.283162
58.917039	2345.666500	20.288179
58.895960	2337.529014	20.293197
59.187621	2349.009827	20.298215
59.133826	2367.535283	20.303232
59.331920	2371.249984	20.308250
59.158683	2378.259704	20.313267
59.959818	2373.126878	20.318285
59.451902	2372.440424	20.323303
59.104736	2372.224226	20.328320
59.849755	2366.212936	20.333338
59.441823	2370.889541	20.338355
59.404638	2371.882667	20.343373
59.262819	2384.422282	20.348391
59.419570	2374.737966	20.353408
59.959814	2384.692190	20.358426
60.078097	2394.795673	20.363443
59.871322	2391.532839	20.368461
59.886793	2403.739410	20.373479
59.983618	2404.993053	20.378496
60.193207	2399.246599	20.383514
60.071617	2398.315999	20.388531
60.073055	2399.332664	20.393549
60.083747	2404.780206	20.398567
60.537457	2413.813373	20.403584
60.551597	2408.946801	20.408602
60.790696	2423.075368	20.413619
61.000192	2420.017344	20.418637
60.781310	2417.914703	20.423655
60.828066	2412.627410	20.428672
61.022323	2403.705728	20.433690
60.729543	2415.257778	20.438707
60.936629	2423.168785	20.443725
61.367976	2423.452636	20.448743
60.994041	2421.474431	20.453760
61.252587	2404.549300	20.458778
61.045371	2416.269483	20.463795
61.320379	2409.717775	20.468813
61.097416	2413.481989	20.473831
61.204119	2422.996102	20.478848
61.287741	2416.575618	20.483866
61.207035	2431.012537	20.488883
61.364316	2435.480410	20.493901
61.289476	2440.075221	20.498919
61.163775	2444.418216	20.503936
61.537790	2449.166401	20.508954
61.454736	2455.706162	20.513971
61.385399	2465.645038	20.518989
62.287571	2456.663031	20.524007
61.846415	2466.808226	20.529024
62.561084	2452.392165	20.534042
62.503248	2464.312096	20.539059
62.135483	2476.206485	20.544077
62.217542	2470.882632	20.549095
62.278399	2470.956859	20.554112
62.629693	2468.771798	20.559130
62.224291	2473.105515	20.564147
62.489595	2470.123687	20.569165
62.633106	2467.139940	20.574183
62.127446	2463.978053	20.579200
62.559755	2467.263938	20.584218
62.441071	2468.291403	20.589235
62.380525	2479.545296	20.594253
62.934828	2483.167304	20.599271
62.746859	2482.903537	20.604288
63.067146	2479.339425	20.609306
62.947952	2486.229639	20.614323
62.988054	2474.798494	20.619341
63.277191	2476.433331	20.624359
62.992036	2483.427737	20.629376
63.080585	2477.814636	20.634394
63.355000	2487.120769	20.639411
63.230117	2506.130158	20.644429
63.475946	2519.614430	20.649447
63.161645	2514.452118	20.654464
63.595105	2505.499511	20.659482
63.723476	2510.184376	20.664499
63.485395	2515.850223	20.669517
64.036192	2504.744876	20.674535
63.993240	2508.748249	20.679552
64.073047	2503.655453	20.684570
64.162642	2500.277482	20.689587
64.045488	2493.258289	20.694605
64.393868	2494.221565	20.699623
64.121257	2498.751442	20.704640
64.383526	2491.463657	20.709658
64.289244	2493.061075	20.714675
64.158970	2497.647348	20.719693
64.275550	2490.291123	20.724711
64.257574	2489.542203	20.729728
64.268521	2490.786424	20.734746
64.405975	2503.663822	20.739763
64.309312	2524.777511	20.744781
64.778412	2523.553632	20.749799
64.508693	2530.064038	20.754816
64.847938	2519.098359	20.759834
64.636528	2524.757833	20.764851
64.795280	2518.412682	20.769869
65.138723	2529.403799	20.774887
64.945875	2556.574052	20.779904
65.050256	2562.292373	20.784922
65.252297	2564.174278	20.789939
64.926237	2558.686746	20.794957
65.409102	2545.519868	20.799975
65.119117	2562.052803	20.804992
65.527617	2542.882382	20.810010
65.429325	2546.098888	20.815027
65.671338	2565.051657	20.820045
65.674061	2569.212450	20.825063
65.829445	2578.470595	20.830080
66.099021	2575.706140	20.835098
66.131945	2572.606009	20.840115
66.062010	2579.946763	20.845133
66.395743	2577.338233	20.850151
66.259566	2578.457175	20.855168
66.242813	2571.718191	20.860186
66.347530	2573.111088	20.865203
66.315982	2578.288519	20.870221
66.361553	2571.299879	20.875239
66.270643	2579.238950	20.880256
66.575188	2567.720338	20.885274
66.418853	2564.382206	20.890291
66.393277	2576.738996	20.895309
66.274066	2562.333475	20.900327
66.437534	2580.661086	20.905344
66.747025	2596.330071	20.910362
66.764424	2593.206912	20.915379
67.035140	2603.991607	20.920397
67.056304	2611.709823	20.925415
67.145217	2610.640492	20.930432
66.669734	2601.504978	20.935450
66.993756	2601.520364	20.940467
66.947603	2606.555737	20.945485
66.906975	2624.535256	20.950503
66.886122	2637.690095	20.955520
67.163486	2631.719374	20.960538
67.364328	2630.966963	20.965555
67.578960	2637.638701	20.970573
67.936442	2651.231796	20.975591
67.860973	2659.639202	20.980608
68.018845	2663.221257	20.985626
68.704286	2625.994754	20.990643
68.680134	2619.966782	20.995661
68.746733	2596.706926	21.000679
68.673524	2601.690473	21.005696
69.205362	2595.155297	21.010714
69.131448	2569.068842	21.015731
68.887763	2567.303727	21.020749
69.259118	2557.336208	21.025767
68.872698	2541.475333	21.030784
68.488022	2527.108988	21.035802
68.716996	2521.915556	21.040819
68.712226	2521.201064	21.045837
68.955430	2507.174657	21.050855
68.667605	2517.245337	21.055872
68.863213	2525.697634	21.060890
68.766425	2535.542278	21.065907
68.980845	2547.947570	21.070925
69.347781	2549.765613	21.075943
68.784972	2555.524897	21.080960
68.715623	2563.569054	21.085978
69.293838	2553.582707	21.090995
68.894657	2556.420219	21.096013
69.127798	2549.686798	21.101031
69.321560	2564.754829	21.106048
69.499438	2576.209538	21.111066
69.813641	2575.519888	21.116083
69.440884	2578.409728	21.121101
69.712238	2579.641631	21.126119
69.586460	2578.365273	21.131136
69.434058	2593.882249	21.136154
69.653181	2595.025544	21.141171
69.730423	2598.913808	21.146189
69.714363	2609.260487	21.151207
69.917564	2623.075501	21.156224
69.684965	2624.556820	21.161242
69.973990	2625.107491	21.166259
69.777441	2620.650061	21.171277
70.133786	2634.381512	21.176295
70.297606	2649.000657	21.181312
69.797777	2648.421903	21.186330
69.970066	2656.255318	21.191347
69.898490	2673.397526	21.196365
70.389023	2676.952957	21.201383
70.485928	2678.413294	21.206400
70.490215	2699.929812	21.211418
70.976770	2706.969620	21.216435
71.076323	2707.918126	21.221453
71.260417	2699.774693	21.226471
71.533098	2699.956824	21.231488
71.405741	2706.161506	21.236506
71.644215	2684.988382	21.241523
71.736566	2701.940941	21.246541
71.647501	2694.354441	21.251559
71.679372	2699.534031	21.256576
71.589213	2703.786584	21.261594
71.694630	2693.624351	21.266611
71.789710	2702.941747	21.271629
71.883998	2708.050398	21.276647
71.662626	2701.426663	21.281664
71.769503	2693.506615	21.286682
71.701777	2702.269443	21.291699
71.431501	2711.197238	21.296717
71.724308	2729.568610	21.301735
72.162041	2731.038375	21.306752
72.254014	2733.610117	21.311770
72.388450	2730.707344	21.316787
72.346771	2725.141657	21.321805
72.680724	2733.036582	21.326823
72.464770	2737.611495	21.331840
72.580031	2755.171719	21.336858
72.911361	2749.859726	21.341875
72.850022	2751.172210	21.346893
73.007555	2751.139915	21.351911
72.787107	2737.068665	21.356928
73.254954	2750.507395	21.361946
73.339469	2742.743767	21.366963
73.223756	2744.666394	21.371981
73.224268	2740.403914	21.376999
73.581742	2746.391491	21.382016
73.591751	2751.603450	21.387034
73.502435	2750.123422	21.392051
73.237255	2749.098817	21.397069
73.542684	2746.439427	21.402087
73.637128	2740.813446	21.407104
73.456741	2742.407009	21.412122
73.530703	2747.450137	21.417139
73.674954	2758.951482	21.422157
74.116474	2765.510195	21.427175
74.567457	2752.642887	21.432192
74.409069	2771.176662	21.437210
74.535355	2764.397815	21.442227
74.803224	2766.786959	21.447245
74.680218	2757.803727	21.452263
74.569384	2739.924348	21.457280
74.451077	2745.459466	21.462298
74.875434	2739.205762	21.467315
74.491324	2747.188253	21.472333
74.781741	2743.414853	21.477351
74.954003	2745.250129	21.482368
74.583253	2757.808192	21.487386
75.229516	2758.345110	21.492403
75.187243	2759.725701	21.497421
74.800623	2747.963310	21.502439
75.082131	2751.324569	21.507456
75.063614	2753.620490	21.512474
75.118601	2746.368807	21.517491
75.258867	2762.636770	21.522509
74.975085	2777.700855	21.527527
75.529062	2773.927200	21.532544
75.434097	2770.821391	21.537562
75.536398	2780.655732	21.542579
75.533519	2785.031674	21.547597
75.716579	2795.963662	21.552615
76.033403	2802.139074	21.557632
75.426629	2820.385598	21.562650
75.966777	2808.291672	21.567667
75.897563	2815.489510	21.572685
75.769812	2825.148910	21.577703
76.147578	2814.718371	21.582720
75.726386	2830.833919	21.587738
75.808733	2835.265475	21.592755
76.252978	2837.067628	21.597773
76.214029	2847.093850	21.602791
76.861696	2850.285572	21.607808
76.971340	2869.042878	21.612826
77.130747	2855.994148	21.617843
77.689843	2843.519911	21.622861
77.261760	2841.750984	21.627879
77.542780	2824.539800	21.632896
77.444650	2826.864242	21.637914
77.185688	2815.454707	21.642931
77.315736	2823.023937	21.647949
77.271471	2821.375439	21.652967
77.542682	2827.300140	21.657984
77.366118	2853.641479	21.663002
77.406453	2848.861382	21.668019
77.688544	2846.574324	21.673037
77.498520	2849.399372	21.678055
77.891716	2845.505817	21.683072
77.768357	2846.599431	21.688090
77.616900	2843.808839	21.693107
77.744677	2848.775000	21.698125
77.646173	2861.212570	21.703143
77.870876	2858.055494	21.708160
77.972308	2866.664087	21.713178
77.974450	2878.705524	21.718195
78.070955	2870.596554	21.723213
78.385618	2886.098056	21.728231
78.256890	2902.009053	21.733248
78.461020	2908.386196	21.738266
78.888915	2897.742600	21.743283
78.627269	2906.305311	21.748301
78.573765	2907.836193	21.753319
78.777695	2893.197836	21.758336
78.634985	2916.290869	21.763354
78.863523	2921.326621	21.768371
79.717078	2929.828284	21.773389
79.779038	2931.422368	21.778407
79.890852	2922.075048	21.783424
79.848522	2929.903913	21.788442
79.854198	2915.589233	21.793459
79.981243	2907.347642	21.798477
79.875146	2903.286981	21.803495
80.056177	2890.889353	21.808512
79.914399	2889.023111	21.813530
79.799270	2893.873131	21.818547
79.501607	2902.591788	21.823565
79.830893	2918.853482	21.828583
80.177236	2916.272734	21.833600
80.312639	2921.459698	21.838618
80.110267	2927.716233	21.843635
80.299117	2928.928336	21.848653
80.014379	2940.336930	21.853671
80.482795	2942.445330	21.858688
80.431243	2942.926708	21.863706
80.621625	2946.590856	21.868723
81.166853	2941.145422	21.873741
80.891559	2960.517617	21.878759
81.139755	2945.954964	21.883776
81.126327	2949.448861	21.888794
81.366692	2937.523663	21.893811
81.005322	2937.757032	21.898829
80.736647	2950.282635	21.903847
81.506989	2949.324292	21.908864
81.003035	2955.263361	21.913882
81.454503	2950.279076	21.918899
81.789293	2941.023635	21.923917
81.778383	2954.385757	21.928935
82.070344	2938.745040	21.933952
81.936880	2960.555150	21.938970
82.242107	2947.090130	21.943987
82.217094	2945.543947	21.949005
82.216873	2954.802442	21.954023
82.687868	2945.057180	21.959040
82.530393	2951.696059	21.964058
82.588203	2959.898932	21.969075
82.581760	2958.218579	21.974093
82.556907	2964.704055	21.979111
82.593435	2958.693088	21.984128
82.299315	2956.309899	21.989146
82.311843	2976.161309	21.994163
82.755521	2985.214188	21.999181
82.875072	2992.785630	22.004199
82.856605	2998.185445	22.009216
82.630572	3000.511363	22.014234
82.665683	2996.647024	22.019251
83.041778	2999.910032	22.024269
83.136544	3025.623768	22.029287
83.327593	3024.146201	22.034304
83.335533	3028.357042	22.039322
83.329559	3035.830746	22.044339
83.801951	3025.247426	22.049357
83.469028	3019.920307	22.054375
83.641186	3019.063172	22.059392
83.617146	3040.863186	22.064410
83.378367	3049.133620	22.069427
83.926131	3043.996388	22.074445
84.160348	3048.393066	22.079463
84.340956	3045.871967	22.084480
84.602111	3055.276697	22.089498
84.377661	3050.745407	22.094515
84.843594	3047.724411	22.099533
84.361149	3043.650315	22.104551
84.743286	3045.400554	22.109568
84.558404	3045.512636	22.114586
84.607188	3064.209765	22.119603
85.025901	3069.729484	22.124621
85.124053	3069.950304	22.129639
85.412177	3058.542308	22.134656
85.465615	3060.641348	22.139674
85.170119	3070.517199	22.144691
85.670788	3062.919677	22.149709
85.545375	3069.345045	22.154727
85.572493	3066.137902	22.159744
85.363129	3065.475304	22.164762
85.252620	3074.775717	22.169779
85.557864	3062.884976	22.174797
85.981459	3074.695507	22.179815
86.042174	3092.817088	22.184832
86.154242	3100.274073	22.189850
86.002158	3096.195370	22.194867
86.297704	3094.227308	22.199885
86.476900	3097.667361	22.204903
86.293698	3099.368903	22.209920
86.418032	3094.288634	22.214938
86.029277	3101.948850	22.219955
86.633113	3096.830681	22.224973
86.565518	3099.023348	22.229991
86.478984	3109.862708	22.235008
86.863866	3120.191111	22.240026
86.847737	3121.093799	22.245043
87.010704	3109.347792	22.250061
87.039268	3116.678035	22.255079
87.162173	3117.581763	22.260096
87.421600	3111.155169	22.265114
87.294011	3113.556173	22.270131
87.908319	3117.397944	22.275149
87.920789	3130.657143	22.280167
87.722525	3130.356482	22.285184
88.103377	3120.700021	22.290202
87.978924	3125.668188	22.295219
88.236697	3124.293758	22.300237
87.800562	3128.955562	22.305255
88.243835	3142.781368	22.310272
88.327348	3132.727190	22.315290
88.264534	3133.084452	22.320307
88.173859	3128.240879	22.325325
88.303271	3139.334336	22.330343
88.467322	3135.493929	22.335360
88.440404	3141.287704	22.340378
88.215802	3150.661740	22.345395
88.989898	3152.979497	22.350413
88.829253	3169.186196	22.355431
88.780637	3170.305670	22.360448
88.782791	3160.055473	22.365466
88.378495	3162.614807	22.370483
88.781021	3160.217647	22.375501
88.920515	3184.039633	22.380519
89.052525	3201.379882	22.385536
89.282908	3193.776962	22.390554
89.369457	3196.305978	22.395571
89.486850	3189.334717	22.400589
89.466994	3200.658787	22.405607
89.778531	3216.794202	22.410624
90.131781	3220.645280	22.415642
90.089695	3220.462509	22.420659
90.386871	3213.490269	22.425677
90.157120	3213.796378	22.430695
90.153149	3204.551486	22.435712
90.041863	3203.885666	22.440730
90.128479	3216.498440	22.445747
90.307412	3212.388629	22.450765
90.743145	3237.648346	22.455783
90.449792	3239.808260	22.460800
90.599665	3231.995792	22.465818
90.616789	3232.793780	22.470835
90.906710	3232.041976	22.475853
91.147226	3247.911996	22.480871
90.984399	3267.421892	22.485888
91.253376	3258.626349	22.490906
91.208185	3272.377085	22.495923
91.500249	3265.516296	22.500941
91.335389	3255.646388	22.505959
91.247850	3272.462370	22.510976
91.973394	3266.581519	22.515994
91.981038	3284.607370	22.521011
92.171238	3279.657887	22.526029
92.308811	3282.528484	22.531047
92.174519	3287.442029	22.536064
92.649898	3282.554476	22.541082
92.534213	3282.822840	22.546099
92.803452	3274.589841	22.551117
92.815672	3271.362677	22.556135
92.502731	3273.917956	22.561152
92.771176	3267.524847	22.566170
92.527724	3284.128024	22.571187
92.886360	3275.371986	22.576205
92.601145	3272.832946	22.581223
93.006781	3270.830922	22.586240
93.188775	3274.180395	22.591258
93.008835	3275.063705	22.596275
93.112499	3277.441481	22.601293
93.147122	3298.188074	22.606311
93.233290	3309.890371	22.611328
93.390757	3309.033680	22.616346
93.053042	3313.800928	22.621363
93.382192	3325.855604	22.626381
93.746318	3327.558458	22.631399
93.780113	3331.103299	22.636416
94.146428	3332.356187	22.641434
93.958169	3339.159766	22.646451
94.074807	3331.746048	22.651469
94.282745	3352.432971	22.656487
94.310216	3370.013912	22.661504
94.307898	3365.265113	22.666522
94.088262	3371.239245	22.671539
94.175155	3367.205233	22.676557
94.424876	3377.729766	22.681575
94.614099	3394.630462	22.686592
94.838504	3396.096176	22.691610
94.978008	3399.863722	22.696627
95.146419	3404.702087	22.701645
95.215229	3390.516694	22.706663
94.950319	3407.804653	22.711680
95.424144	3416.739419	22.716698
95.156574	3415.782091	22.721715
95.263978	3424.269929	22.726733
95.955725	3423.797780	22.731751
95.758794	3418.598839	22.736768
96.063512	3418.035527	22.741786
95.928841	3418.427504	22.746803
95.742813	3429.485891	22.751821
96.125902	3439.380944	22.756839
96.365703	3437.570478	22.761856
96.447359	3444.020444	22.766874
96.366816	3449.595241	22.771891
96.781360	3444.929897	22.776909
96.579515	3450.991671	22.781927
96.432517	3450.330560	22.786944
96.971457	3448.125777	22.791962
96.823153	3465.035868	22.796979
97.214333	3470.631148	22.801997
97.545208	3467.356799	22.807015
97.532591	3471.847143	22.812032
97.369129	3454.759106	22.817050
97.457951	3468.491020	22.822067
97.460193	3468.925334	22.827085
97.400549	3466.701745	22.832103
97.155043	3473.042004	22.837120
97.299745	3476.255950	22.842138
97.621292	3496.343184	22.847155
97.373149	3488.221159	22.852173
97.620829	3497.070899	22.857191
97.562963	3514.429882	22.862208
97.648174	3505.946460	22.867226
98.006938	3529.155177	22.872243
98.220373	3530.699883	22.877261
98.431218	3539.670697	22.882279
98.154737	3549.978753	22.887296
99.131955	3567.938022	22.892314
98.935068	3567.121368	22.897331
99.344346	3574.580257	22.902349
99.782047	3576.211927	22.907367
99.303744	3572.159839	22.912384
99.448848	3578.267482	22.917402
99.772322	3579.528651	22.922419
99.712015	3571.626334	22.927437
99.958740	3560.605920	22.932455
99.250371	3569.077457	22.937472
99.960082	3558.280543	22.942490
99.929832	3567.211290	22.947507
99.798011	3573.145790	22.952525
100.213371	3572.984275	22.957543
99.784119	3578.626190	22.962560
99.842968	3585.900862	22.967578
100.339515	3601.800591	22.972595
100.607936	3602.464158	22.977613
100.511644	3599.117847	22.982631
100.629367	3604.707182	22.987648
100.971849	3605.813635	22.992666
100.785069	3612.275351	22.997683
100.719103	3624.401850	23.002701
100.882388	3619.514190	23.007719
100.982709	3622.508330	23.012736
101.062461	3605.114186	23.017754
101.315887	3633.907488	23.022771
101.636857	3644.379483	23.027789
102.139432	3643.835832	23.032807
101.988017	3659.723400	23.037824
101.791001	3657.823277	23.042842
101.997614	3651.891418	23.047859
102.053391	3647.910114	23.052877
102.275957	3646.130426	23.057895
102.068119	3651.398371	23.062912
102.120348	3641.017139	23.067930
102.474345	3641.231518	23.072947
102.298742	3645.076785	23.077965
102.658065	3645.494619	23.082983
102.457227	3653.840207	23.088000
102.747261	3653.903342	23.093018
102.641130	3673.421308	23.098035
102.724195	3670.739059	23.103053
103.076263	3673.240026	23.108071
102.932676	3673.766949	23.113088
103.104266	3688.758635	23.118106
103.508223	3692.839253	23.123123
103.394761	3698.004609	23.128141
103.739705	3699.209091	23.133159
103.574763	3717.769092	23.138176
103.579189	3698.345904	23.143194
103.517455	3695.784430	23.148211
103.658473	3716.363209	23.153229
104.193946	3720.085874	23.158247
104.142316	3727.356821	23.163264
103.911964	3728.861099	23.168282
104.363253	3738.247031	23.173299
104.288678	3750.367176	23.178317
104.419694	3747.275405	23.183335
104.717063	3749.279898	23.188352
104.593239	3750.411448	23.193370
104.866969	3758.634576	23.198387
105.082918	3777.389589	23.203405
105.856526	3760.198734	23.208423
105.933295	3768.649301	23.213440
106.089088	3751.569995	23.218458
106.149153	3744.274880	23.223475
106.052084	3733.828885	23.228493
106.180908	3717.828901	23.233511
106.057901	3729.178275	23.238528
106.118635	3725.326057	23.243546
106.288975	3719.621431	23.248563
105.977327	3737.364734	23.253581
106.407801	3745.834796	23.258599
106.517597	3753.255856	23.263616
106.580858	3758.623925	23.268634
106.468127	3760.767055	23.273651
106.169751	3764.766894	23.278669
106.457044	3759.446483	23.283687
106.339585	3782.438990	23.288704
106.354941	3788.144915	23.293722
107.221065	3790.551507	23.298739
106.662060	3802.127316	23.303757
107.183252	3814.453797	23.308775
107.141451	3828.472976	23.313792
106.990781	3833.678384	23.318810
107.392356	3827.380374	23.323827
107.215107	3851.215171	23.328845
107.590776	3852.979566	23.333863
107.447014	3866.495532	23.338880
107.986104	3861.891770	23.343898
108.196914	3862.341633	23.348915
108.296556	3872.418846	23.353933
108.823373	3860.954680	23.358951
108.713089	3862.888750	23.363968
108.721191	3856.672678	23.368986
109.326821	3862.965759	23.374003
109.059079	3865.098690	23.379021
109.243632	3859.823569	23.384039
108.990087	3860.814352	23.389056
109.297489	3866.724025	23.394074
109.609070	3858.346316	23.399091
109.711343	3857.118388	23.404109
109.458590	3860.090995	23.409127
109.184947	3858.114923	23.414144
109.778936	3856.269111	23.419162
109.945257	3841.064406	23.424179
109.613660	3850.196297	23.429197
109.819823	3851.325689	23.434215
109.806137	3881.623480	23.439232
110.044183	3891.413652	23.444250
110.295045	3884.970045	23.449267
109.675069	3894.387812	23.454285
110.257174	3903.229769	23.459303
110.706521	3912.083825	23.464320
110.954234	3909.775130	23.469338
110.806171	3902.433228	23.474355
110.861759	3914.336317	23.479373
110.496070	3910.512782	23.484391
110.832561	3934.095879	23.489408
110.996463	3936.244503	23.494426
111.245855	3937.120686	23.499443
110.938485	3945.504507	23.504461
111.640012	3966.915835	23.509479
111.808706	3979.625906	23.514496
111.481858	3980.921341	23.519514
111.970279	3975.451869	23.524531
111.993991	3986.959083	23.529549
112.207529	3986.784851	23.534567
112.309302	4003.185285	23.539584
112.422182	4004.348607	23.544602
112.304470	4001.940040	23.549619
112.383404	4004.887393	23.554637
112.830732	4013.308359	23.559655
112.581462	4018.952187	23.564672
112.755619	4023.070080	23.569690
112.993761	4025.718676	23.574707
112.957113	4015.379047	23.579725
113.636382	4026.287785	23.584743
114.014477	4038.403436	23.589760
113.937713	4037.604310	23.594778
113.978211	4020.813064	23.599795
113.768175	4021.113961	23.604813
114.149349	4030.475041	23.609831
114.039671	4031.804675	23.614848
114.103060	4042.075399	23.619866
114.179380	4036.890941	23.624883
114.364216	4038.196714	23.629901
114.199272	4032.874164	23.634919
114.078717	4034.770975	23.639936
114.244557	4054.356686	23.644954
114.432177	4064.176562	23.649971
114.688746	4074.237817	23.654989
115.045884	4086.920381	23.660007
114.983819	4088.674063	23.665024
115.033057	4095.878511	23.670042
115.317588	4091.263989	23.675059
115.132627	4099.402063	23.680077
115.685865	4121.140092	23.685095
115.773780	4122.576854	23.690112
115.328902	4121.277500	23.695130
115.764021	4111.609495	23.700147
115.744304	4131.948442	23.705165
115.958851	4149.667076	23.710183
115.980453	4145.912957	23.715200
116.176819	4144.074547	23.720218
116.889295	4146.384928	23.725235
116.607765	4151.247874	23.730253
116.470638	4152.152504	23.735271
116.672497	4157.906097	23.740288
116.845307	4169.800642	23.745306
117.371420	4168.036094	23.750323
117.315998	4181.046763	23.755341
117.138195	4183.427487	23.760359
117.404149	4181.185427	23.765376
117.462487	4175.558989	23.770394
118.029785	4193.828865	23.775411
118.008369	4200.192629	23.780429
118.097065	4203.630559	23.785447
118.121214	4210.657306	23.790464
118.239618	4205.049281	23.795482
118.204674	4198.171644	23.800499
118.502616	4192.980042	23.805517
117.926944	4206.836191	23.810535
117.986465	4208.328443	23.815552
118.099879	4221.101786	23.820570
118.532581	4222.106760	23.825587
118.415423	4248.450485	23.830605
118.437903	4255.779514	23.835623
119.153845	4261.763570	23.840640
119.137090	4281.435255	23.845658
119.625390	4283.185421	23.850675
119.532005	4294.196432	23.855693
119.668604	4288.711362	23.860711
120.025297	4285.852289	23.865728
119.923131	4298.391617	23.870746
120.215439	4274.687206	23.875763
120.112278	4290.007172	23.880781
120.383027	4314.882496	23.885799
120.631125	4307.874964	23.890816
120.542052	4312.670329	23.895834
120.681031	4305.490266	23.900851
120.689014	4304.865717	23.905869
120.986901	4306.129996	23.910887
121.081174	4309.394970	23.915904
121.119701	4321.692946	23.920922
121.425069	4324.671845	23.925939
121.526560	4331.960293	23.930957
121.369477	4343.043680	23.935975
121.415067	4339.229248	23.940992
120.972340	4354.381358	23.946010
121.500546	4357.424235	23.951027
121.744541	4361.729116	23.956045
121.942627	4371.299409	23.961063
122.289812	4376.169564	23.966080
122.302701	4398.986312	23.971098
122.386205	4413.158944	23.976115
122.856797	4416.291674	23.981133
122.371585	4412.420043	23.986151
122.654224	4404.007453	23.991168
122.885492	4430.464001	23.996186
122.911000	4443.071724	24.001203
123.055478	4445.703979	24.006221
123.185837	4438.537485	24.011239
123.270874	4436.383950	24.016256
123.193693	4446.395472	24.021274
123.634137	4452.560175	24.026291
123.726595	4455.076609	24.031309
123.679004	4459.402926	24.036327
124.155276	4466.348385	24.041344
124.110635	4478.935444	24.046362
124.371971	4481.480279	24.051379
125.384439	4459.955966	24.056397
125.564069	4454.846038	24.061415
126.022963	4425.427642	24.066432
125.569310	4423.059559	24.071450
125.755868	4409.682579	24.076467
126.008800	4413.505257	24.081485
125.692998	4398.657254	24.086503
125.974833	4378.421578	24.091520
125.622843	4382.437520	24.096538
125.899103	4383.697505	24.101555
125.911458	4375.813876	24.106573
125.942246	4390.289706	24.111591
125.676175	4377.436396	24.116608
125.959819	4404.430739	24.121626
126.173937	4405.315141	24.126643
126.060401	4407.385258	24.131661
125.976116	4407.469305	24.136679
126.194631	4422.380712	24.141696
126.331387	4434.489698	24.146714
126.195161	4440.382339	24.151731
126.304487	4454.265683	24.156749
126.475891	4476.581514	24.161767
126.626638	4479.905702	24.166784
126.657452	4496.570368	24.171802
126.913850	4506.603190	24.176819
127.026737	4502.678771	24.181837
127.064914	4529.513089	24.186855
127.397909	4535.847562	24.191872
127.597611	4551.257120	24.196890
127.998108	4555.898427	24.201907
128.251098	4551.363005	24.206925
128.374870	4552.272975	24.211943
128.559837	4545.766753	24.216960
128.670685	4552.254090	24.221978
128.976338	4549.729807	24.226995
129.391382	4546.659062	24.232013
128.948431	4535.701528	24.237031
129.445495	4549.362212	24.242048
129.294030	4575.158178	24.247066
129.374037	4577.765672	24.252083
129.796644	4567.376170	24.257101
129.616762	4571.294423	24.262119
130.022339	4567.927970	24.267136
129.833059	4570.806750	24.272154
129.660933	4577.297547	24.277171
129.848796	4592.505937	24.282189
130.066367	4606.627455	24.287207
130.593975	4592.476189	24.292224
130.321305	4597.885490	24.297242
130.354034	4626.928926	24.302259
130.441061	4626.540536	24.307277
130.745696	4636.386323	24.312295
130.833332	4630.936785	24.317312
131.025880	4642.550059	24.322330
130.925739	4658.696335	24.327347
131.476363	4656.466230	24.332365
131.152936	4665.887032	24.337383
131.546621	4673.860491	24.342400
131.548382	4687.120423	24.347418
131.681732	4694.212028	24.352435
131.813260	4695.151043	24.357453
132.022907	4718.736996	24.362471
132.087194	4717.471969	24.367488
132.289728	4726.689746	24.372506
132.211220	4733.929772	24.377523
133.005440	4736.947276	24.382541
132.958242	4751.496568	24.387559
133.497810	4738.654730	24.392576
133.692198	4730.615242	24.397594
133.679192	4732.827465	24.402611
133.443917	4733.453438	24.407629
133.310300	4732.837702	24.412647
134.083573	4730.359360	24.417664
134.086886	4729.491055	24.422682
133.917098	4733.068674	24.427699
134.182415	4732.787446	24.432717
134.155688	4736.691458	24.437735
133.881389	4744.241032	24.442752
134.170143	4752.057051	24.447770
134.312326	4761.683676	24.452787
134.691043	4751.923408	24.457805
134.723786	4765.986234	24.462823
135.218345	4780.924818	24.467840
135.136072	4788.774603	24.472858
135.474236	4788.256907	24.477875
135.575485	4781.284848	24.482893
135.101613	4785.001317	24.487911
135.676415	4794.861622	24.492928
135.973876	4803.814130	24.497946
135.954530	4813.086734	24.502963
135.974686	4801.021682	24.507981
136.271462	4809.422287	24.512999
136.216363	4811.749755	24.518016
136.600431	4815.850104	24.523034
136.475315	4832.271577	24.528051
136.720588	4823.533410	24.533069
136.795434	4838.104747	24.538087
136.459725	4833.332236	24.543104
136.867759	4853.643572	24.548122
136.935399	4871.492825	24.553139
136.974528	4863.786040	24.558157
137.195846	4877.339019	24.563175
137.437778	4886.396035	24.568192
137.729043	4889.780958	24.573210
137.526303	4902.537016	24.578227
137.999653	4912.061369	24.583245
138.163906	4921.995107	24.588263
138.110644	4917.400331	24.593280
138.439074	4921.454385	24.598298
138.336202	4933.456096	24.603315
138.978217	4930.624573	24.608333
139.497576	4932.834299	24.613351
139.683242	4928.152003	24.618368
139.769222	4918.852249	24.623386
139.890613	4922.429046	24.628403
139.700171	4925.460066	24.633421
139.784721	4936.152728	24.638439
140.060869	4950.034146	24.643456
140.050480	4952.100678	24.648474
139.952224	4953.924616	24.653491
140.424839	4946.428080	24.658509
140.108707	4960.685751	24.663527
140.709235	4949.738590	24.668544
140.548593	4969.052199	24.673562
140.370438	4985.296357	24.678579
140.997833	4975.024337	24.683597
140.901436	4987.081325	24.688615
140.971286	4994.263489	24.693632
140.930315	5011.152792	24.698650
141.124069	5013.954973	24.703667
141.608898	5011.513621	24.708685
141.696588	5030.183452	24.713703
141.878587	5045.067233	24.718720
142.127611	5048.483977	24.723738
141.956196	5047.829586	24.728755
141.941244	5048.851101	24.733773
142.114006	5061.815349	24.738791
142.229014	5067.743098	24.743808
142.506065	5064.346592	24.748826
142.441260	5082.332156	24.753843
142.868244	5098.148055	24.758861
143.157198	5096.772243	24.763879
143.138092	5102.496157	24.768896
143.530569	5096.746451	24.773914
143.114258	5117.307349	24.778931
143.198121	5123.313896	24.783949
143.234963	5125.759304	24.788967
143.584970	5151.569825	24.793984
144.002669	5156.945958	24.799002
143.645216	5167.907900	24.804019
143.942520	5184.760788	24.809037
144.435587	5181.629386	24.814055
144.654191	5186.576563	24.819072
144.960938	5182.121852	24.824090
144.780426	5204.159039	24.829107
145.213880	5216.865352	24.834125
145.602129	5219.757100	24.839143
145.504267	5213.975370	24.844160
145.948653	5213.304267	24.849178
145.858304	5211.417824	24.854195
146.011508	5216.458898	24.859213
146.049619	5232.262410	24.864231
146.202938	5242.858868	24.869248
146.452416	5244.642312	24.874266
146.140629	5245.613664	24.879283
146.546184	5250.618170	24.884301
147.091732	5251.065921	24.889319
147.147373	5260.363805	24.894336
147.432446	5261.697614	24.899354
147.466265	5266.178439	24.904371
147.604627	5263.466306	24.909389
147.817259	5262.826015	24.914407
147.657137	5262.561135	24.919424
147.064531	5260.856115	24.924442
147.256976	5286.981119	24.929459
147.862899	5290.181050	24.934477
148.023514	5311.053614	24.939495
147.955967	5335.419465	24.944512
148.504836	5323.838767	24.949530
148.375408	5333.730339	24.954547
148.518041	5343.649411	24.959565
148.230481	5353.748250	24.964583
148.776197	5367.318927	24.969600
149.285483	5372.743003	24.974618
149.497121	5382.524698	24.979635
149.514913	5379.773799	24.984653
149.565706	5398.964800	24.989671
149.841803	5406.900185	24.994688
149.972376	5411.218981	24.999706
150.198299	5418.777967	25.004723
150.237037	5433.314086	25.009741
150.435973	5437.831465	25.014759
150.403324	5438.606290	25.019776
151.227330	5431.645242	25.024794
151.285781	5432.867674	25.029811
151.390543	5433.001994	25.034829
151.356887	5438.167336	25.039847
151.629842	5453.415267	25.044864
151.613775	5460.582311	25.049882
151.683877	5468.982138	25.054899
151.709830	5459.279329	25.059917
151.902785	5462.354595	25.064935
151.901022	5476.817515	25.069952
152.170410	5478.371681	25.074970
152.209154	5490.353174	25.079987
152.495375	5494.098956	25.085005
152.580231	5510.705765	25.090023
152.733392	5516.777401	25.095040
153.040128	5511.405937	25.100058
153.102231	5515.692370	25.105075
153.168551	5511.359589	25.110093
153.360825	5523.747688	25.115111
153.298061	5541.182577	25.120128
154.049908	5538.202074	25.125146
154.108521	5543.637283	25.130163
153.989979	5551.035504	25.135181
154.271194	5557.276968	25.140199
154.224322	5572.279789	25.145216
154.340896	5568.845117	25.150234
154.486758	5574.834899	25.155251
154.760841	5597.933117	25.160269
155.048154	5589.843578	25.165287
154.960311	5597.205641	25.170304
155.209326	5587.613947	25.175322
155.462210	5614.818250	25.180339
155.333799	5632.710610	25.185357
155.991142	5628.721541	25.190375
155.753284	5645.945679	25.195392
155.786063	5642.453961	25.200410
155.940850	5653.386725	25.205427
156.123141	5652.573847	25.210445
156.766717	5662.761975	25.215463
157.106041	5678.700444	25.220480
157.426931	5680.867474	25.225498
157.891577	5675.652960	25.230515
158.033619	5669.608158	25.235533
158.305548	5667.008551	25.240551
158.035001	5653.533182	25.245568
158.478436	5640.028050	25.250586
158.031692	5642.336878	25.255603
158.257531	5654.813250	25.260621
158.892070	5654.193400	25.265639
158.578826	5654.790158	25.270656
158.906475	5649.585689	25.275674
159.092390	5646.786882	25.280691
158.947710	5662.902963	25.285709
159.038993	5651.950079	25.290727
158.981891	5659.529172	25.295744
159.087616	5663.940740	25.300762
159.321159	5672.071116	25.305779
159.100167	5684.744984	25.310797
159.264246	5685.106156	25.315815
159.408022	5717.503850	25.320832
159.290280	5716.361748	25.325850
159.570317	5740.956271	25.330867
159.302057	5752.345681	25.335885
159.976088	5762.890315	25.340903
160.397524	5781.132215	25.345920
160.806967	5792.717595	25.350938
160.814568	5807.318664	25.355955
160.964770	5804.195757	25.360973
161.571528	5800.476857	25.365991
161.826686	5813.427326	25.371008
161.893650	5809.717289	25.376026
161.804463	5811.468556	25.381043
161.850627	5823.992077	25.386061
162.399657	5827.518502	25.391079
162.543403	5837.362496	25.396096
162.556583	5836.189301	25.401114
162.793311	5842.683546	25.406131
162.491791	5850.974091	25.411149
163.064405	5848.695696	25.416167
162.951013	5870.566797	25.421184
163.266632	5871.504605	25.426202
163.573076	5877.747936	25.431219
163.406645	5877.467549	25.436237
163.776542	5871.937077	25.441255
163.389548	5895.120554	25.446272
163.642223	5898.784955	25.451290
164.105928	5904.574683	25.456307
164.157681	5926.457950	25.461325
164.600682	5926.369824	25.466343
164.269860	5942.758720	25.471360
164.352323	5946.129945	25.476378
165.256991	5971.147690	25.481395
165.175543	5962.762140	25.486413
165.619297	5965.995705	25.491431
165.033285	5976.486439	25.496448
165.462457	5990.988095	25.501466
165.823547	6007.723439	25.506483
165.366126	6018.219730	25.511501
166.114533	6022.764617	25.516519
166.015981	6029.151319	25.521536
166.110929	6038.757003	25.526554
166.190958	6060.141998	25.531571
166.325796	6066.934323	25.536589
166.662395	6079.073778	25.541607
167.076568	6090.200249	25.546624
167.347989	6091.258780	25.551642
167.373173	6105.963540	25.556659
167.189495	6122.576385	25.561677
167.757464	6124.178149	25.566695
168.133513	6141.179715	25.571712
168.020825	6140.965258	25.576730
168.283695	6139.700381	25.581747
168.016764	6156.377421	25.586765
168.636805	6169.504943	25.591783
169.045103	6176.487606	25.596800
168.798863	6178.686988	25.601818
169.468303	6194.654128	25.606835
169.736494	6208.254070	25.611853
169.828221	6203.640472	25.616871
169.799561	6202.505666	25.621888
170.162371	6196.591930	25.626906
170.294691	6207.522494	25.631923
170.296242	6221.103501	25.636941
170.667681	6220.583023	25.641959
170.769864	6228.781858	25.646976
170.429408	6235.235391	25.651994
170.894972	6239.827866	25.657011
170.580887	6261.404264	25.662029
170.979385	6259.364071	25.667047
171.083678	6283.152108	25.672064
171.171320	6295.235998	25.677082
171.973452	6314.570164	25.682100
171.822583	6328.266229	25.687117
171.810796	6318.439573	25.692135
172.179053	6331.341856	25.697152
172.081510	6345.426838	25.702170
172.670893	6350.905360	25.707188
173.131130	6351.481443	25.712205
173.231946	6368.120780	25.717223
173.266843	6373.205009	25.722240
173.060270	6380.880027	25.727258
173.643211	6364.604238	25.732276
173.405056	6378.738473	25.737293
173.733106	6384.432662	25.742311
173.979618	6396.503768	25.747328
173.885870	6405.475372	25.752346
174.483719	6423.924350	25.757364
174.192894	6430.305969	25.762381
174.650239	6422.852608	25.767399
174.761672	6417.997062	25.772416
174.772177	6443.164097	25.777434
175.374231	6449.517111	25.782452
175.240047	6455.439702	25.787469
175.392054	6443.870602	25.792487
175.632860	6462.043909	25.797504
175.912692	6471.394067	25.802522
176.190021	6472.437473	25.807540
176.567520	6484.724059	25.812557
176.538261	6493.092025	25.817575
176.779443	6493.187670	25.822592
176.832060	6501.989445	25.827610
176.917404	6499.094485	25.832628
176.921951	6509.728984	25.837645
177.313174	6520.009776	25.842663
177.772693	6529.015254	25.847680
177.416697	6530.974499	25.852698
177.728520	6535.158518	25.857716
177.731894	6556.166223	25.862733
177.907547	6557.487906	25.867751
178.266045	6578.510993	25.872768
178.213375	6578.729224	25.877786
178.571543	6572.553858	25.882804
178.518306	6599.739175	25.887821
179.362404	6610.307477	25.892839
179.223442	6617.732805	25.897856
179.134013	6617.927183	25.902874
179.856709	6629.047164	25.907892
179.691517	6638.327617	25.912909
180.082676	6636.933608	25.917927
180.655961	6656.339876	25.922944
180.683653	6672.342662	25.927962
181.126540	6667.083379	25.932980
181.101970	6674.711927	25.937997
181.073365	6668.077486	25.943015
181.306182	6668.440713	25.948032
181.246006	6671.114249	25.953050
181.402764	6693.108819	25.958068
181.403722	6705.679890	25.963085
181.769589	6690.397320	25.968103
182.133159	6700.246486	25.973120
182.219972	6714.869963	25.978138
182.464717	6711.808438	25.983156
182.722027	6718.365801	25.988173
183.022753	6736.513774	25.993191
182.849772	6742.306632	25.998208
182.840654	6737.030655	26.003226
183.151011	6762.874009	26.008244
183.216733	6780.799388	26.013261
183.282614	6776.194620	26.018279
183.661053	6785.808261	26.023296
183.662294	6811.961096	26.028314
183.573754	6818.126729	26.033332
184.039285	6833.335127	26.038349
184.188766	6846.619729	26.043367
184.344967	6865.005163	26.048384
184.455265	6890.533673	26.053402
185.184583	6895.796310	26.058420
185.346449	6906.874480	26.063437
185.237323	6906.340454	26.068455
185.578519	6913.485750	26.073472
185.893273	6917.710343	26.078490
185.985981	6928.181704	26.083508
186.141387	6928.670353	26.088525
186.428157	6950.779264	26.093543
187.017464	6958.043464	26.098560
187.013400	6966.442171	26.103578
187.155079	6953.978923	26.108596
187.324463	6961.948876	26.113613
187.097334	6960.939743	26.118631
187.534337	6972.581301	26.123648
187.832671	6979.402924	26.128666
188.082342	6985.128398	26.133684
188.075763	6976.960699	26.138701
188.548260	6992.141322	26.143719
188.410708	7007.290444	26.148736
188.142678	7026.221077	26.153754
188.964147	7008.425341	26.158772
188.734396	7025.397224	26.163789
188.752109	7043.148902	26.168807
189.526944	7029.466541	26.173824
189.023626	7051.135140	26.178842
189.731988	7057.930003	26.183860
189.632798	7064.625963	26.188877
189.516034	7095.403008	26.193895
189.753044	7103.440618	26.198912
189.579831	7129.633831	26.203930
190.007602	7133.622433	26.208948
190.387639	7152.939169	26.213965
190.935755	7165.956549	26.218983
191.286338	7183.415531	26.224000
191.245385	7194.213954	26.229018
191.397300	7185.670266	26.234036
191.842102	7201.115573	26.239053
191.747074	7214.877214	26.244071
191.857045	7214.481033	26.249088
192.087910	7235.337852	26.254106
192.388325	7245.705797	26.259124
192.472342	7264.255630	26.264141
192.210247	7286.284005	26.269159
192.865091	7297.449541	26.274176
192.872961	7309.419799	26.279194
193.348249	7321.030874	26.284212
193.730528	7322.633522	26.289229
194.097019	7336.697060	26.294247
194.164128	7350.616327	26.299264
194.433332	7374.207852	26.304282
194.934220	7367.735299	26.309300
195.247168	7374.405823	26.314317
195.182412	7387.832606	26.319335
195.685297	7370.377370	26.324352
195.796616	7373.037652	26.329370
195.989452	7376.693387	26.334388
196.272749	7374.796532	26.339405
196.198174	7374.122888	26.344423
196.482347	7377.905300	26.349440
196.201747	7404.080480	26.354458
196.759073	7412.090526	26.359476
196.857440	7407.310083	26.364493
196.887066	7435.992201	26.369511
197.214969	7427.651648	26.374528
197.171361	7435.464071	26.379546
197.431887	7441.642367	26.384564
198.185537	7462.348523	26.389581
198.098579	7462.285742	26.394599
198.006061	7463.005186	26.399616
198.164980	7479.523469	26.404634
198.502860	7483.773536	26.409652
198.875776	7482.068215	26.414669
198.592850	7501.890301	26.419687
199.058142	7510.202294	26.424704
199.377416	7519.718259	26.429722
199.503445	7527.481432	26.434740
199.858374	7532.970759	26.439757
199.554922	7551.091118	26.444775
199.989703	7533.351601	26.449792
200.370179	7559.046056	26.454810
200.426591	7576.439876	26.459828
200.683906	7568.386578	26.464845
200.969864	7576.481715	26.469863
201.083717	7583.905891	26.474880
201.137683	7595.771873	26.479898
201.140236	7596.693785	26.484916
201.343544	7628.117594	26.489933
201.212355	7638.068002	26.494951
201.508738	7643.744255	26.499968
201.954162	7661.155803	26.504986
202.311772	7668.004163	26.510004
202.588373	7676.587645	26.515021
202.648747	7692.757767	26.520039
202.975160	7706.434448	26.525056
202.956852	7723.996724	26.530074
203.044718	7727.489520	26.535092
203.458139	7743.720290	26.540109
203.642485	7757.069209	26.545127
204.270579	7758.201246	26.550144
204.666583	7776.306320	26.555162
205.098380	7789.539556	26.560180
205.471727	7777.967566	26.565197
205.504913	7782.789465	26.570215
205.530447	7783.920249	26.575232
205.677457	7777.733625	26.580250
205.464162	7783.431132	26.585268
205.765685	7787.062703	26.590285
205.808090	7800.207488	26.595303
205.957307	7806.281451	26.600320
206.125722	7817.659265	26.605338
206.320173	7837.037434	26.610356
206.800518	7854.419797	26.615373
206.797373	7862.701472	26.620391
207.418449	7863.658248	26.625408
206.933712	7886.072375	26.630426
207.237206	7891.178874	26.635444
207.930769	7904.595005	26.640461
207.573624	7925.072588	26.645479
207.949156	7929.942722	26.650496
208.420238	7945.127650	26.655514
208.500594	7948.858025	26.660532
208.928574	7963.750792	26.665549
208.855777	7978.525470	26.670567
209.110020	7992.341920	26.675584
209.078654	8012.810683	26.680602
209.422987	8032.475442	26.685620
210.001801	8048.759538	26.690637
210.010386	8062.832452	26.695655
210.233759	8066.102085	26.700672
210.339956	8082.908534	26.705690
210.618154	8093.869862	26.710708
211.038797	8097.595244	26.715725
211.002644	8120.540488	26.720743
211.832354	8125.777507	26.725760
211.721205	8129.556895	26.730778
211.669835	8134.475575	26.735796
212.022248	8148.594937	26.740813
211.761662	8158.738756	26.745831
212.128622	8182.344478	26.750848
212.679611	8193.350594	26.755866
212.763429	8194.704920	26.760884
212.950947	8211.224755	26.765901
213.181345	8223.284173	26.770919
213.267603	8238.456565	26.775936
213.676389	8249.648471	26.780954
213.650798	8250.538839	26.785972
213.933363	8254.257142	26.790989
214.040126	8281.354325	26.796007
214.420690	8278.305505	26.801024
214.843352	8295.546657	26.806042
214.486892	8317.829924	26.811060
215.085041	8311.214898	26.816077
215.120881	8333.037179	26.821095
215.687376	8329.163677	26.826112
215.507867	8338.746009	26.831130
215.244724	8358.487916	26.836148
216.425704	8364.961090	26.841165
216.496646	8389.013009	26.846183
216.695928	8391.218631	26.851200
217.076479	8398.388821	26.856218
217.144044	8417.366482	26.861236
217.529695	8415.537662	26.866253
217.590598	8427.412573	26.871271
218.098070	8432.726569	26.876288
218.224552	8438.869906	26.881306
217.945435	8448.732628	26.886324
218.238956	8455.606098	26.891341
218.185312	8474.477042	26.896359
218.348769	8477.783442	26.901376
218.705142	8506.942816	26.906394
218.533195	8519.075238	26.911412
218.921361	8538.918485	26.916429
219.197128	8552.949263	26.921447
219.299527	8569.150354	26.926464
219.706836	8593.431351	26.931482
219.757963	8609.609449	26.936500
220.509075	8623.810652	26.941517
221.152644	8631.851971	26.946535
221.504068	8622.978385	26.951552
221.766590	8641.796501	26.956570
221.648380	8666.454301	26.961588
222.053514	8666.969485	26.966605
222.031819	8676.923717	26.971623
222.399440	8685.870004	26.976640
222.346045	8698.311432	26.981658
222.730683	8708.226904	26.986676
222.448408	8718.722812	26.991693
222.716087	8733.234778	26.996711
222.781694	8751.679121	27.001728
223.172390	8760.379821	27.006746
223.339436	8786.918111	27.011764
223.956101	8791.152403	27.016781
224.200407	8806.047956	27.021799
224.089926	8818.356341	27.026816
224.676591	8822.824025	27.031834
224.860285	8846.751670	27.036852
225.231252	8842.676412	27.041869
225.276569	8853.330168	27.046887
225.243825	8874.290203	27.051904
225.517156	8890.119164	27.056922
226.087823	8901.317868	27.061940
226.366247	8911.659822	27.066957
226.100874	8933.163274	27.071975
226.082387	8943.351084	27.076992
226.602781	8943.140684	27.082010
226.401807	8972.488311	27.087028
226.912851	8992.496929	27.092045
226.754512	9005.654613	27.097063
227.488966	9039.412439	27.102080
227.930364	9046.791060	27.107098
228.473631	9060.025061	27.112116
228.420391	9064.585152	27.117133
228.711986	9071.539553	27.122151
228.959185	9093.847831	27.127168
229.379018	9100.784208	27.132186
229.340277	9106.944864	27.137204
229.814520	9107.562073	27.142221
229.984786	9127.320755	27.147239
230.109935	9136.136430	27.152256
230.288639	9133.237381	27.157274
229.927434	9149.921324	27.162292
230.435597	9169.216204	27.167309
230.642163	9189.395107	27.172327
230.912399	9198.779979	27.177344
231.285989	9206.355773	27.182362
231.212080	9228.536125	27.187380
231.482055	9239.909996	27.192397
231.727950	9252.735640	27.197415
232.208145	9277.469595	27.202432
232.530635	9282.849890	27.207450
232.739939	9301.114375	27.212468
233.002220	9305.039506	27.217485
233.414853	9313.346188	27.222503
233.319325	9324.010138	27.227520
234.133080	9331.936262	27.232538
234.255704	9345.855197	27.237556
234.161626	9342.538013	27.242573
234.639320	9352.280973	27.247591
234.793377	9369.852823	27.252608
235.261119	9368.878384	27.257626
235.220167	9386.986603	27.262644
235.298738	9408.094366	27.267661
235.639339	9402.606117	27.272679
235.599883	9418.128091	27.277696
235.976902	9426.896798	27.282714
236.093011	9461.836058	27.287732
236.202951	9472.361394	27.292749
236.307390	9477.209058	27.297767
236.485590	9501.519846	27.302784
236.988957	9515.373659	27.307802
237.402449	9535.133621	27.312820
237.329852	9557.552890	27.317837
237.818977	9570.692286	27.322855
237.931559	9593.780498	27.327872
238.298454	9598.785702	27.332890
238.368633	9624.010156	27.337908
238.515090	9631.764683	27.342925
239.151851	9664.242612	27.347943
239.156640	9674.836657	27.352960
239.777916	9672.812013	27.357978
240.050539	9692.299263	27.362996
240.377512	9699.192955	27.368013
240.804687	9719.256520	27.373031
241.111627	9740.579849	27.378048
240.794699	9731.230014	27.383066
241.103015	9744.417546	27.388084
241.427343	9764.559603	27.393101
241.839427	9765.448636	27.398119
241.541114	9790.001653	27.403136
241.911242	9806.365365	27.408154
242.093468	9816.624550	27.413172
242.158778	9823.429978	27.418189
242.417894	9846.189496	27.423207
242.786313	9864.508686	27.428224
243.294617	9876.006694	27.433242
243.233202	9893.584001	27.438260
243.792402	9905.689625	27.443277
244.345871	9906.413515	27.448295
244.203337	9920.444506	27.453312
244.370519	9932.797675	27.458330
244.897967	9939.188073	27.463348
244.663530	9964.420068	27.468365
245.214055	9968.972826	27.473383
245.078525	9982.265397	27.478400
245.508113	9999.647475	27.483418
245.607791	9994.517075	27.488436
246.110118	10020.500238	27.493453
246.409444	10029.168681	27.498471
246.242825	10061.851842	27.503488
246.544201	10061.681561	27.508506
246.914509	10080.974330	27.513524
247.457708	10090.268940	27.518541
247.645336	10092.670512	27.523559
247.543686	10121.836050	27.528576
247.694783	10130.216307	27.533594
247.647419	10154.214813	27.538612
248.301779	10175.055153	27.543629
248.861587	10175.754378	27.548647
248.808264	10188.393103	27.553664
249.414992	10208.467005	27.558682
249.301924	10228.811894	27.563700
249.392509	10243.195374	27.568717
249.705955	10254.049177	27.573735
250.182153	10280.462463	27.578752
250.727560	10295.664936	27.583770
250.922212	10317.055641	27.588788
250.887165	10325.573889	27.593805
251.882883	10342.705255	27.598823
251.485985	10356.699091	27.603840
251.896498	10360.963147	27.608858
252.181462	10372.615003	27.613876
252.037894	10395.211024	27.618893
253.150059	10415.252882	27.623911
253.013176	10419.756281	27.628928
253.158717	10431.465876	27.633946
253.392083	10444.213411	27.638964
253.721297	10465.273282	27.643981
253.930532	10463.298503	27.648999
254.096695	10482.626276	27.654016
254.254530	10487.178681	27.659034
254.522099	10507.354687	27.664052
255.227532	10514.243711	27.669069
255.975699	10501.941384	27.674087
256.654164	10516.253187	27.679104
256.882410	10510.007971	27.684122
257.248817	10514.862298	27.689140
257.322606	10511.696743	27.694157
258.016558	10506.055996	27.699175
257.984970	10497.866200	27.704192
258.146628	10489.941464	27.709210
258.604758	10483.563746	27.714228
258.451638	10479.849596	27.719245
258.835062	10481.223940	27.724263
258.989316	10491.528357	27.729280
258.831666	10487.670006	27.734298
258.823293	10496.227265	27.739316
258.843833	10505.892854	27.744333
259.320676	10521.814281	27.749351
259.292856	10533.398194	27.754368
259.093025	10551.401637	27.759386
259.767244	10559.743743	27.764404
259.735029	10584.994509	27.769421
260.055408	10606.397915	27.774439
259.956070	10639.378365	27.779456
260.156844	10655.332145	27.784474
260.358028	10680.858817	27.789492
260.124163	10705.511299	27.794509
260.774418	10739.975156	27.799527
261.162240	10776.424304	27.804544
261.150247	10790.786623	27.809562
261.634315	10808.512716	27.814580
261.703426	10842.383508	27.819597
261.957991	10852.974877	27.824615
262.401606	10877.524355	27.829632
262.682102	10912.857935	27.834650
262.982501	10933.645097	27.839668
263.236414	10956.376332	27.844685
263.825533	10967.216586	27.849703
263.936601	10992.627872	27.854720
264.331497	11012.637738	27.859738
264.930356	11030.706705	27.864756
264.970097	11049.191061	27.869773
265.195220	11071.904371	27.874791
265.208100	11099.231401	27.879808
265.934480	11106.946764	27.884826
266.297789	11123.853377	27.889844
266.489311	11128.352345	27.894861
266.999038	11138.128137	27.899879
267.353902	11167.513996	27.904896
267.610093	11174.700478	27.909914
268.202378	11189.368239	27.914932
268.218279	11208.294730	27.919949
268.057437	11205.755499	27.924967
268.378626	11227.233653	27.929984
268.452843	11243.498048	27.935002
268.672083	11260.479026	27.940020
268.926972	11289.073348	27.945037
269.374608	11288.128911	27.950055
269.613776	11319.518625	27.955072
269.771875	11341.532795	27.960090
270.208386	11355.854605	27.965108
270.343467	11380.889908	27.970125
270.903194	11404.763196	27.975143
271.009183	11415.897860	27.980160
271.319808	11427.904697	27.985178
271.988440	11444.471291	27.990196
271.929918	11466.890116	27.995213
271.974146	11488.773619	28.000231
272.278890	11506.508055	28.005248
272.621221	11516.355853	28.010266
273.043807	11532.672489	28.015284
273.307735	11554.591473	28.020301
273.445015	11560.051200	28.025319
273.680302	11587.454970	28.030336
273.624147	11620.623312	28.035354
274.482014	11637.524387	28.040372
274.642567	11656.148619	28.045389
274.864963	11670.910235	28.050407
275.378105	11690.843902	28.055424
275.274110	11701.558887	28.060442
275.849833	11721.930520	28.065460
276.230428	11753.777497	28.070477
276.574259	11760.728385	28.075495
276.949738	11772.293827	28.080512
277.213958	11784.540217	28.085530
277.393332	11798.864728	28.090548
277.454197	11821.666899	28.095565
277.667442	11834.370020	28.100583
277.926264	11854.161557	28.105600
277.836663	11872.692651	28.110618
278.392241	11891.424425	28.115636
278.652762	11920.748467	28.120653
279.174292	11930.541703	28.125671
279.389229	11937.817277	28.130688
279.529867	11964.002799	28.135706
280.059725	11985.394707	28.140724
280.250247	12000.991479	28.145741
280.559612	12011.112104	28.150759
280.831720	12034.038028	28.155776
280.736370	12050.127204	28.160794
281.184985	12062.404004	28.165812
281.710824	12078.422092	28.170829
282.199819	12072.850912	28.175847
282.994483	12084.270115	28.180864
283.207116	12104.920455	28.185882
283.597364	12103.372519	28.190900
283.707093	12093.879902	28.195917
283.756728	12098.018909	28.200935
284.385604	12113.728509	28.205952
284.214650	12129.990188	28.210970
284.080527	12136.326120	28.215988
284.256679	12157.136182	28.221005
284.879748	12158.389937	28.226023
285.189000	12165.191510	28.231040
284.893893	12194.013029	28.236058
285.492684	12213.895379	28.241076
285.450392	12230.514854	28.246093
285.937146	12263.719299	28.251111
286.355800	12281.906115	28.256128
286.132030	12304.592123	28.261146
286.384529	12326.337569	28.266164
286.873003	12360.444804	28.271181
287.268707	12384.096900	28.276199
287.776205	12406.589751	28.281216
287.791777	12436.851777	28.286234
288.323021	12435.475116	28.291252
288.642301	12456.086226	28.296269
288.848171	12486.996036	28.301287
288.982441	12499.905755	28.306304
289.461768	12512.200674	28.311322
289.926471	12539.963666	28.316340
289.971922	12560.958930	28.321357
290.491696	12581.751374	28.326375
290.700413	12596.881667	28.331392
290.730352	12614.299523	28.336410
291.243327	12638.068129	28.341428
291.520050	12668.686102	28.346445
291.553176	12692.107043	28.351463
292.081777	12706.541691	28.356480
292.235136	12727.172682	28.361498
292.886280	12744.242231	28.366516
293.142050	12769.333023	28.371533
293.066908	12795.576816	28.376551
293.817837	12817.267364	28.381568
293.827221	12845.437014	28.386586
294.340925	12858.558512	28.391604
294.431176	12874.446087	28.396621
294.684126	12904.450741	28.401639
295.113430	12914.820784	28.406656
295.153348	12944.521921	28.411674
295.239537	12961.466009	28.416692
295.831309	12982.165135	28.421709
295.938548	13001.627003	28.426727
296.902294	13013.139483	28.431744
297.039300	13039.755169	28.436762
297.317975	13048.312843	28.441780
297.744606	13063.062478	28.446797
298.120242	13084.980846	28.451815
298.845351	13106.318350	28.456832
298.831287	13119.355497	28.461850
298.941239	13126.745076	28.466868
299.239275	13145.163948	28.471885
299.456513	13170.025362	28.476903
299.777630	13178.965310	28.481920
299.670927	13203.001009	28.486938
299.858825	13215.283158	28.491956
300.277435	13241.557980	28.496973
300.408617	13257.568384	28.501991
300.704151	13275.959454	28.507008
300.795336	13305.413262	28.512026
300.967105	13324.291269	28.517044
301.466118	13350.784625	28.522061
301.559235	13384.959342	28.527079
302.413587	13403.270839	28.532096
302.544098	13449.614151	28.537114
303.092997	13471.904673	28.542132
303.500157	13478.898633	28.547149
303.537771	13511.776442	28.552167
303.757433	13525.326834	28.557184
304.129804	13543.610965	28.562202
304.444357	13570.795423	28.567220
304.595616	13594.946665	28.572237
304.860615	13613.412499	28.577255
305.718470	13635.365403	28.582272
305.699088	13654.229676	28.587290
306.001615	13683.070925	28.592308
306.586437	13691.419203	28.597325
306.832958	13731.833224	28.602343
307.419081	13731.522112	28.607360
307.282694	13760.059389	28.612378
307.548066	13788.483065	28.617396
307.847400	13793.808830	28.622413
308.218246	13826.526641	28.627431
308.766037	13841.603655	28.632448
308.955026	13866.588992	28.637466
309.477450	13884.415360	28.642484
310.043579	13899.119074	28.647501
310.109052	13910.183360	28.652519
310.551175	13929.553194	28.657536
310.639635	13953.267802	28.662554
310.630930	13977.622537	28.667572
311.240328	14002.292792	28.672589
311.540506	14022.601763	28.677607
312.015712	14044.111014	28.682624
312.413876	14057.441681	28.687642
312.890888	14063.790859	28.692660
312.923301	14083.841578	28.697677
313.129255	14096.830552	28.702695
313.473491	14116.988958	28.707712
313.653722	14147.923507	28.712730
313.716431	14163.815320	28.717748
314.207451	14183.680084	28.722765
314.474843	14210.016128	28.727783
315.168514	14240.861300	28.732800
315.450173	14262.472157	28.737818
315.358182	14276.630952	28.742836
315.820139	14302.299920	28.747853
316.028495	14328.226723	28.752871
316.503398	14344.480832	28.757888
316.975887	14376.183842	28.762906
317.411559	14398.666119	28.767924
317.675539	14414.884229	28.772941
317.529950	14443.012913	28.777959
317.861103	14454.328369	28.782976
317.972598	14487.761693	28.787994
318.378547	14513.537954	28.793012
319.265899	14538.071702	28.798029
319.506858	14564.001374	28.803047
320.070903	14569.486956	28.808064
320.791443	14585.470641	28.813082
321.026956	14589.381010	28.818100
321.169631	14608.080934	28.823117
321.331509	14633.057745	28.828135
321.562779	14629.376047	28.833152
321.553939	14646.607076	28.838170
321.785603	14656.668918	28.843188
322.565258	14670.731328	28.848205
322.520309	14694.552580	28.853223
323.423220	14706.382059	28.858240
323.324441	14719.347808	28.863258
323.442900	14739.049445	28.868276
324.071879	14753.885388	28.873293
324.044416	14774.156447	28.878311
324.724538	14782.889835	28.883328
324.665288	14817.863366	28.888346
324.580156	14843.930882	28.893364
325.276463	14860.331739	28.898381
325.267679	14883.532675	28.903399
325.663029	14904.362845	28.908416
326.055318	14933.974729	28.913434
326.291739	14967.752443	28.918452
326.585723	14989.841319	28.923469
326.724837	15024.779369	28.928487
327.175250	15057.472328	28.933504
327.658605	15088.059150	28.938522
328.019582	15124.010350	28.943540
328.307434	15146.154034	28.948557
328.075148	15181.022971	28.953575
328.599482	15210.711253	28.958592
329.109443	15245.290648	28.963610
329.533605	15279.844891	28.968628
330.025264	15309.970571	28.973645
330.156435	15347.706421	28.978663
330.357072	15372.293417	28.983680
330.728592	15401.841814	28.988698
331.158666	15432.863604	28.993716
331.886444	15462.813445	28.998733
332.092894	15504.091097	29.003751
332.969037	15516.723051	29.008768
333.633652	15538.492973	29.013786
333.755633	15557.014586	29.018804
334.490850	15575.074002	29.023821
334.450820	15597.494683	29.028839
334.573675	15605.768978	29.033856
334.976726	15620.704503	29.038874
335.118030	15652.655409	29.043892
335.386613	15664.814182	29.048909
335.849679	15687.935154	29.053927
335.942686	15706.059836	29.058944
336.222612	15731.310388	29.063962
336.406653	15754.283699	29.068980
336.582879	15777.307190	29.073997
336.988659	15812.653612	29.079015
337.174145	15844.912801	29.084032
337.813111	15869.239005	29.089050
338.223643	15898.028507	29.094068
338.859358	15910.714674	29.099085
338.992382	15951.392504	29.104103
339.254494	15963.804736	29.109120
340.195763	15994.467330	29.114138
340.530875	16008.780862	29.119156
340.834269	16028.127257	29.124173
341.090040	16047.282960	29.129191
341.971697	16061.514125	29.134208
342.982347	16064.526102	29.139226
343.266585	16053.623302	29.144244
343.792429	16054.009282	29.149261
343.921564	16066.166175	29.154279
344.173091	16082.198875	29.159296
344.390341	16088.653232	29.164314
344.405972	16087.930426	29.169332
344.660594	16074.413094	29.174349
345.001483	16113.454136	29.179367
344.883623	16107.821886	29.184384
345.213174	16119.102516	29.189402
345.515668	16147.156949	29.194420
345.529808	16165.265224	29.199437
345.877695	16186.694321	29.204455
345.825235	16209.778267	29.209472
346.377493	16250.154320	29.214490
346.562619	16289.032384	29.219508
346.837202	16300.735152	29.224525
347.057812	16333.976127	29.229543
347.132813	16364.413727	29.234560
347.906824	16390.720027	29.239578
348.109910	16437.767497	29.244596
348.597469	16467.818760	29.249613
348.777570	16496.147761	29.254631
348.998369	16514.446085	29.259648
349.527620	16549.220488	29.264666
349.685786	16601.223236	29.269684
350.570901	16634.511074	29.274701
350.860754	16662.611031	29.279719
351.097090	16696.895106	29.284736
351.958369	16719.136895	29.289754
351.844473	16746.376939	29.294772
351.975337	16767.718135	29.299789
352.056699	16802.546578	29.304807
352.895659	16837.576194	29.309824
353.460213	16864.780004	29.314842
353.471508	16898.039362	29.319860
354.043685	16913.378413	29.324877
354.887414	16954.585956	29.329895
354.956621	16972.452753	29.334912
355.503875	17002.613344	29.339930
355.679941	17036.748894	29.344948
356.097155	17051.661320	29.349965
356.625386	17079.732066	29.354983
356.748561	17115.916062	29.360000
356.934984	17152.847821	29.365018
357.259272	17176.922181	29.370036
357.870617	17193.815426	29.375053
358.223284	17223.025041	29.380071
358.495631	17246.115097	29.385088
359.135214	17284.299423	29.390106
359.081178	17305.941389	29.395124
359.836300	17320.793507	29.400141
360.021722	17361.480355	29.405159
360.751520	17377.416393	29.410176
361.058051	17393.025174	29.415194
361.360316	17428.166782	29.420212
361.981480	17449.333291	29.425229
362.189489	17463.769968	29.430247
362.014011	17482.943422	29.435264
363.092515	17497.769074	29.440282
363.627753	17531.196919	29.445300
363.728659	17551.724457	29.450317
364.113073	17573.015352	29.455335
364.744043	17586.988213	29.460352
365.022082	17615.496833	29.465370
365.306853	17633.169537	29.470388
365.553166	17652.691203	29.475405
366.030793	17662.492016	29.480423
366.129003	17695.075037	29.485440
366.426477	17715.179405	29.490458
366.177415	17745.108806	29.495476
366.715047	17770.463354	29.500493
367.247844	17790.393382	29.505511
367.532167	17828.833112	29.510528
368.475791	17839.605238	29.515546
368.727604	17859.089985	29.520564
369.177427	17863.216360	29.525581
369.559958	17884.511122	29.530599
369.646558	17914.607625	29.535616
370.217756	17936.618421	29.540634
370.398043	17954.185784	29.545652
370.505372	17970.406501	29.550669
371.018089	18004.843092	29.555687
371.037720	18026.752826	29.560704
371.617259	18043.144651	29.565722
371.455957	18087.686169	29.570740
371.762485	18117.994181	29.575757
372.168200	18149.756511	29.580775
371.911800	18194.936649	29.585792
372.681088	18223.800211	29.590810
373.107922	18272.658604	29.595828
373.816345	18315.971006	29.600845
374.268506	18342.079825	29.605863
374.893503	18377.915716	29.610880
375.197384	18402.682493	29.615898
375.276331	18434.179366	29.620916
375.901896	18458.640880	29.625933
376.439035	18487.661477	29.630951
376.490019	18522.317291	29.635968
377.590923	18542.879471	29.640986
377.766206	18593.225828	29.646004
377.825959	18621.291473	29.651021
378.346846	18640.516737	29.656039
379.740303	18655.529431	29.661056
380.786479	18654.803356	29.666074
381.012105	18677.970914	29.671092
381.393654	18694.102902	29.676109
381.471907	18697.009334	29.681127
381.294948	18720.629655	29.686144
381.903110	18723.358700	29.691162
382.273809	18757.845543	29.696180
382.533766	18778.414533	29.701197
382.906154	18793.129447	29.706215
382.733298	18818.818934	29.711232
383.464497	18836.933058	29.716250
383.477250	18881.381747	29.721268
383.475538	18906.942213	29.726285
383.927076	18923.835263	29.731303
384.106841	18959.750696	29.736320
384.362624	19001.312699	29.741338
384.346851	19046.901506	29.746356
384.757329	19086.480350	29.751373
385.583629	19127.248521	29.756391
385.363467	19172.964443	29.761408
386.029780	19202.696382	29.766426
386.508923	19256.519286	29.771444
386.732958	19303.470564	29.776461
387.343968	19337.940981	29.781479
388.188085	19386.483078	29.786496
388.710975	19408.462829	29.791514
389.446108	19440.743862	29.796532
389.953110	19475.007900	29.801549
390.499231	19490.172376	29.806567
390.574407	19515.601269	29.811584
391.341877	19529.822793	29.816602
391.774271	19553.439790	29.821620
391.750921	19586.281490	29.826637
392.494434	19599.827606	29.831655
393.014354	19636.531679	29.836672
393.172470	19664.458300	29.841690
393.693120	19676.468048	29.846708
393.768543	19698.656100	29.851725
394.238923	19729.447591	29.856743
394.546659	19746.838159	29.861760
394.657798	19772.616195	29.866778
394.948540	19800.771785	29.871796
394.876521	19833.707139	29.876813
395.436861	19857.322348	29.881831
395.469232	19917.005074	29.886848
395.931637	19957.975702	29.891866
396.243752	19979.256414	29.896884
396.436962	20028.938901	29.901901
397.081350	20054.977674	29.906919
397.206715	20103.202350	29.911936
397.990304	20141.192918	29.916954
398.191852	20186.216100	29.921972
398.640486	20231.167057	29.926989
399.160224	20263.715433	29.932007
399.334422	20300.443399	29.937024
399.970424	20342.395228	29.942042
400.398758	20386.547536	29.947060
400.697120	20434.738284	29.952077
401.311591	20464.047516	29.957095
401.466848	20509.391358	29.962112
402.060024	20544.825721	29.967130
402.263971	20594.512845	29.972148
402.709740	20640.635131	29.977165
403.943050	20660.766614	29.982183
404.820078	20681.581271	29.987200
405.376857	20703.312779	29.992218
406.065884	20730.959570	29.997236
405.743394	20751.538933	30.002253
406.251733	20783.856885	30.007271
406.938675	20821.365217	30.012288
407.012130	20830.604078	30.017306
407.833668	20850.387617	30.022324
407.749762	20893.675249	30.027341
408.393305	20919.789610	30.032359
408.574980	20949.670948	30.037376
409.262128	20965.199722	30.042394
410.178772	20986.933636	30.047412
410.395560	21008.255056	30.052429
410.805666	21023.952621	30.057447
410.776267	21063.407029	30.062464
411.206064	21080.837156	30.067482
411.741663	21095.156662	30.072500
411.800607	21136.587812	30.077517
412.523843	21157.084785	30.082535
412.966124	21180.797048	30.087552
413.086600	21209.032011	30.092570
413.280383	21249.591408	30.097588
413.635755	21281.908791	30.102605
414.312461	21312.974972	30.107623
414.188769	21347.985551	30.112640
414.780156	21367.391513	30.117658
415.120264	21409.450081	30.122676
415.746380	21449.897552	30.127693
416.115689	21478.963706	30.132711
416.554433	21516.021131	30.137728
416.995586	21557.084324	30.142746
417.227459	21587.450399	30.147764
417.398861	21631.955870	30.152781
417.950924	21659.305199	30.157799
418.472249	21701.025551	30.162816
419.352529	21725.962189	30.167834
419.867157	21761.892969	30.172852
419.901593	21807.302849	30.177869
420.723059	21826.340249	30.182887
420.578581	21858.720820	30.187904
421.415934	21883.027835	30.192922
422.233967	21894.523385	30.197940
422.452553	21913.144926	30.202957
422.946129	21938.579331	30.207975
423.345137	21970.502985	30.212992
423.583731	21989.425592	30.218010
424.154014	21997.812056	30.223028
424.002998	22030.848336	30.228045
424.465126	22060.888707	30.233063
424.956141	22091.807272	30.238080
424.951974	22130.020785	30.243098
425.524670	22177.168485	30.248116
425.502744	22198.284896	30.253133
426.117309	22242.586338	30.258151
426.626047	22281.417071	30.263168
427.026811	22333.654647	30.268186
427.453126	22372.691559	30.273204
427.512684	22432.337748	30.278221
428.045713	22468.810947	30.283239
428.166396	22508.231337	30.288256
428.571229	22558.137045	30.293274
429.422336	22599.297459	30.298292
429.555862	22657.845896	30.303309
429.984012	22696.027115	30.308327
431.447351	22730.843044	30.313344
431.608778	22767.211146	30.318362
432.699070	22783.381374	30.323380
433.411446	22817.288803	30.328397
434.036382	22844.009959	30.333415
434.330704	22870.043147	30.338432
434.844576	22891.570153	30.343450
435.348045	22906.538235	30.348468
435.516890	22941.557406	30.353485
435.579139	22959.187376	30.358503
436.438417	22991.211947	30.363520
436.414329	23038.564705	30.368538
436.902883	23051.583405	30.373556
437.500233	23086.637731	30.378573
437.483044	23117.478152	30.383591
437.682594	23152.219914	30.388608
438.193822	23192.438278	30.393626
439.021882	23238.619646	30.398644
439.283063	23272.148424	30.403661
439.793233	23311.427511	30.408679
440.082226	23343.319907	30.413696
439.953093	23404.090226	30.418714
440.826277	23428.158624	30.423732
440.844568	23484.649222	30.428749
441.067001	23522.358576	30.433767
441.829463	23566.222798	30.438784
442.190457	23609.576355	30.443802
442.772378	23660.386360	30.448820
442.941184	23710.468486	30.453837
443.181641	23752.126783	30.458855
444.026770	23799.913606	30.463872
444.112548	23861.626093	30.468890
444.574544	23900.889276	30.473908
445.021110	23963.532763	30.478925
445.691238	24006.046289	30.483943
446.379351	24054.481030	30.488960
446.744523	24100.452659	30.493978
447.591015	24140.463365	30.498996
447.905307	24181.566517	30.504013
448.303927	24216.089931	30.509031
449.358960	24259.385690	30.514048
449.527598	24291.875295	30.519066
450.212734	24320.927288	30.524084
450.736193	24360.856269	30.529101
451.163521	24390.166995	30.534119
451.623049	24411.514117	30.539136
451.890612	24433.493755	30.544154
452.314674	24464.247963	30.549172
452.841376	24501.188609	30.554189
452.950475	24532.360799	30.559207
453.240361	24566.128651	30.564224
453.724214	24598.787533	30.569242
454.305888	24641.744594	30.574260
454.314924	24670.484693	30.579277
454.913676	24711.810205	30.584295
455.215806	24763.549626	30.589312
455.896557	24812.039781	30.594330
456.135340	24859.936061	30.599348
456.658321	24905.245158	30.604365
457.062858	24935.623414	30.609383
457.387935	24983.218790	30.614400
457.696401	25035.254445	30.619418
458.355555	25085.707460	30.624436
458.835668	25132.191154	30.629453
458.944521	25174.428169	30.634471
459.645371	25223.428673	30.639488
459.942633	25278.253337	30.644506
460.595015	25326.702336	30.649524
461.078703	25372.405514	30.654541
461.640230	25420.574901	30.659559
462.332781	25464.627463	30.664576
462.474426	25522.569423	30.669594
463.377511	25546.812515	30.674612
463.515270	25608.571625	30.679629
463.990475	25660.283597	30.684647
464.674443	25694.870108	30.689664
464.969089	25742.351200	30.694682
465.819465	25775.670890	30.699700
466.285354	25823.486624	30.704717
466.885380	25870.129140	30.709735
467.241666	25912.096865	30.714752
467.665095	25956.633554	30.719770
468.212285	25987.490022	30.724788
469.049844	26022.553309	30.729805
469.690519	26064.717289	30.734823
470.312321	26092.738799	30.739840
470.610975	26124.913940	30.744858
471.194199	26165.939603	30.749876
471.372377	26199.005292	30.754893
472.000429	26234.472641	30.759911
472.806461	26259.918695	30.764928
472.844488	26301.993568	30.769946
473.186791	26342.201551	30.774964
473.735979	26371.017715	30.779981
473.980955	26425.204956	30.784999
474.489040	26464.149449	30.790016
475.121850	26497.689423	30.795034
475.508060	26538.685441	30.800052
475.814777	26577.799081	30.805069
476.366845	26615.342545	30.810087
476.985035	26658.606173	30.815104
477.080720	26705.028325	30.820122
477.824282	26744.783014	30.825140
478.179284	26788.415318	30.830157
478.348764	26826.539719	30.835175
478.980126	26866.603405	30.840192
479.386135	26920.358723	30.845210
479.982619	26958.728297	30.850228
480.218741	27012.631825	30.855245
480.448831	27063.234093	30.860263
481.203567	27104.265211	30.865280
481.641385	27161.510865	30.870298
482.536341	27196.481913	30.875316
482.749499	27236.060402	30.880333
483.244768	27272.775666	30.885351
483.653064	27321.967712	30.890368
484.171257	27360.319573	30.895386
484.731095	27387.252610	30.900404
486.067951	27416.697438	30.905421
486.357274	27444.716150	30.910439
486.996070	27465.431864	30.915456
487.156007	27498.411593	30.920474
487.572355	27530.156719	30.925492
488.155125	27566.542731	30.930509
488.565802	27604.332511	30.935527
489.562071	27628.134187	30.940544
489.863573	27661.794249	30.945562
490.482182	27695.890911	30.950580
490.411527	27723.363914	30.955597
491.072950	27763.254392	30.960615
491.800109	27794.147471	30.965632
493.195830	27820.624529	30.970650
493.886451	27820.280221	30.975668
494.442257	27832.159080	30.980685
495.170997	27856.213450	30.985703
495.482479	27880.989723	30.990720
495.807737	27909.618349	30.995738
495.875071	27931.706527	31.000756
496.297966	27939.689730	31.005773
496.237597	27983.636561	31.010791
496.568309	28002.567985	31.015808
496.732138	28046.414855	31.020826
496.982411	28102.048040	31.025844
497.291388	28147.054076	31.030861
497.425407	28206.400573	31.035879
498.228051	28249.139341	31.040896
498.327968	28314.696536	31.045914
498.517027	28362.590296	31.050932
498.883667	28430.775661	31.055949
499.282589	28487.855494	31.060967
499.999954	28561.081010	31.065984
500.335076	28629.013697	31.071002
500.764985	28694.978372	31.076020
500.989526	28758.185501	31.081037
501.549792	28827.949233	31.086055
502.281226	28895.826964	31.091072
503.199291	28970.137753	31.096090
503.524167	29034.783552	31.101108
504.454560	29083.727181	31.106125
505.104661	29149.316522	31.111143
505.835971	29199.542568	31.116160
506.232262	29261.593825	31.121178
506.443529	29318.606441	31.126196
507.389938	29378.564083	31.131213
507.615260	29423.536776	31.136231
508.442986	29467.914806	31.141248
509.005203	29535.403426	31.146266
509.366531	29596.045223	31.151284
510.201238	29644.375313	31.156301
510.398706	29706.990981	31.161319
510.997541	29738.631149	31.166336
511.563583	29796.350157	31.171354
511.714159	29855.201112	31.176372
512.555339	29896.934389	31.181389
513.138753	29960.566122	31.186407
513.669943	30015.269407	31.191424
513.933589	30061.852631	31.196442
514.665467	30117.822834	31.201460
515.245285	30160.593656	31.206477
515.270625	30218.087900	31.211495
516.234214	30266.294322	31.216512
516.958467	30316.127260	31.221530
516.996925	30360.126865	31.226548
517.525186	30406.048964	31.231565
518.235200	30461.989180	31.236583
518.347570	30502.005046	31.241600
519.224215	30549.564106	31.246618
519.939658	30606.065444	31.251636
520.465026	30648.089299	31.256653
520.730015	30689.146716	31.261671
521.025019	30734.183840	31.266688
521.601396	30781.565981	31.271706
522.061715	30854.196861	31.276724
522.846239	30904.961675	31.281741
523.044629	30956.157870	31.286759
523.729341	31007.081437	31.291776
524.408512	31042.950881	31.296794
525.154638	31102.616275	31.301812
525.524667	31135.776426	31.306829
525.874918	31196.832596	31.311847
526.675210	31240.487730	31.316864
527.107311	31297.823683	31.321882
527.463740	31359.415739	31.326900
528.114103	31404.339099	31.331917
528.694941	31457.606343	31.336935
529.623580	31507.841151	31.341952
530.066095	31553.240923	31.346970
530.452380	31614.279973	31.351988
531.197467	31655.780930	31.357005
531.869793	31699.518291	31.362023
532.521280	31748.670073	31.367040
533.243909	31785.123850	31.372058
533.591743	31832.956739	31.377076
533.898912	31880.660809	31.382093
534.231491	31940.283780	31.387111
534.679157	31988.110067	31.392128
535.137437	32042.513069	31.397146
535.488186	32102.849793	31.402164
536.392041	32135.333657	31.407181
537.122533	32194.203953	31.412199
537.673717	32246.184893	31.417216
538.583832	32279.573509	31.422234
538.838025	32338.794302	31.427252
539.437292	32373.455476	31.432269
539.972536	32422.634654	31.437287
540.212720	32472.291806	31.442304
540.904606	32524.745689	31.447322
541.242782	32596.653020	31.452340
542.000713	32630.578579	31.457357
542.071912	32681.949102	31.462375
542.838722	32746.463042	31.467392
543.161343	32789.932737	31.472410
543.525105	32859.779715	31.477428
544.277457	32913.183954	31.482445
544.841785	32971.137722	31.487463
545.164569	33028.405868	31.492480
545.827906	33083.942503	31.497498
546.067872	33150.378149	31.502516
546.653253	33205.164465	31.507533
546.845327	33279.225368	31.512551
547.467408	33341.755462	31.517568
548.502934	33408.439309	31.522586
548.826074	33474.436464	31.527604
549.531486	33520.337442	31.532621
550.289164	33572.259782	31.537639
551.453226	33615.592523	31.542656
552.655384	33657.701107	31.547674
552.824929	33708.149618	31.552692
552.979557	33747.689418	31.557709
553.435388	33800.782448	31.562727
553.764862	33850.816835	31.567744
554.382598	33893.006734	31.572762
554.665433	33950.839813	31.577780
555.186253	33985.734835	31.582797
555.685170	34051.105572	31.587815
555.858920	34105.719695	31.592832
556.619304	34157.577040	31.597850
557.061594	34227.533192	31.602868
557.908925	34267.180616	31.607885
558.831221	34318.674053	31.612903
559.018861	34367.726724	31.617920
559.756259	34426.032169	31.622938
560.327858	34488.214918	31.627956
560.644116	34527.180696	31.632973
561.483653	34594.623994	31.637991
562.092302	34654.617576	31.643008
563.082139	34694.930327	31.648026
563.164163	34748.270952	31.653044
563.584399	34799.810844	31.658061
564.156822	34858.214378	31.663079
565.202296	34917.335177	31.668096
565.977198	34957.160197	31.673114
566.349185	35015.591042	31.678132
566.859508	35045.226327	31.683149
567.616682	35107.775040	31.688167
568.078825	35162.063918	31.693184
568.822288	35212.361942	31.698202
568.980690	35261.851070	31.703220
569.883207	35311.176407	31.708237
570.324207	35354.263616	31.713255
570.870611	35417.977960	31.718272
571.729610	35459.847716	31.723290
571.957023	35521.434538	31.728308
572.629953	35569.154390	31.733325
573.186076	35617.038827	31.738343
573.471466	35679.834723	31.743360
574.240365	35735.838728	31.748378
574.882329	35808.469412	31.753396
575.095012	35859.986687	31.758413
575.937229	35921.255590	31.763431
576.127926	35970.659295	31.768448
576.563757	36022.881788	31.773466
576.980479	36095.762277	31.778484
577.541035	36167.117140	31.783501
577.969228	36239.059041	31.788519
578.248506	36314.162728	31.793536
579.133363	36388.093717	31.798554
579.314047	36460.336165	31.803572
580.352198	36537.729679	31.808589
580.814220	36604.390832	31.813607
581.409141	36681.154410	31.818624
582.255455	36739.301091	31.823642
583.023638	36802.043263	31.828660
583.448587	36870.784969	31.833677
584.096818	36942.598665	31.838695
584.357266	37017.844107	31.843712
585.363010	37071.136911	31.848730
586.195958	37148.131424	31.853748
586.672449	37214.603090	31.858765
587.386728	37281.168279	31.863783
587.625916	37349.693170	31.868800
588.565841	37405.068183	31.873818
588.870997	37466.850818	31.878836
589.566119	37533.729395	31.883853
590.112882	37603.391123	31.888871
590.515678	37672.054330	31.893888
590.747235	37743.210985	31.898906
591.364453	37809.235527	31.903924
592.384659	37858.242292	31.908941
593.273286	37894.984170	31.913959
593.869830	37966.649521	31.918976
594.637937	38024.967922	31.923994
595.001491	38075.857485	31.929012
595.434186	38147.282342	31.934029
595.962756	38199.852479	31.939047
596.169588	38264.753436	31.944064
597.078591	38328.115209	31.949082
597.484709	38394.328252	31.954100
597.971728	38464.855340	31.959117
598.893940	38525.457094	31.964135
599.214239	38593.698709	31.969152
600.119398	38645.513569	31.974170
600.825716	38712.426220	31.979188
601.484457	38787.423866	31.984205
602.376013	38841.514047	31.989223
602.497352	38912.901814	31.994240
603.727825	38969.208929	31.999258
603.983682	39025.131150	32.004276
604.609397	39077.883480	32.009293
605.255896	39144.479348	32.014311
605.839600	39210.773353	32.019328
606.712779	39273.749808	32.024346
607.285487	39330.375003	32.029364
607.596860	39390.780683	32.034381
608.278815	39454.275428	32.039399
609.366651	39513.672641	32.044416
609.665404	39578.361099	32.049434
610.327397	39646.575483	32.054452
610.727270	39713.687631	32.059469
611.428384	39770.681229	32.064487
611.876937	39827.410544	32.069504
612.793903	39888.743699	32.074522
613.598033	39950.250364	32.079540
614.102412	40024.246439	32.084557
614.526274	40083.758334	32.089575
614.778874	40157.894386	32.094592
615.630461	40216.471187	32.099610
615.646650	40296.350671	32.104628
616.167009	40380.146575	32.109645
616.843647	40447.127324	32.114663
617.767214	40522.928021	32.119680
618.361369	40577.132458	32.124698
619.897808	40643.350073	32.129716
620.238621	40719.692915	32.134733
620.861331	40780.771477	32.139751
621.748910	40845.685988	32.144768
622.374085	40908.465990	32.149786
623.036398	40963.509449	32.154804
623.560329	41026.448626	32.159821
624.087090	41077.278583	32.164839
624.814935	41148.780100	32.169856
625.285033	41206.450824	32.174874
626.219168	41274.298040	32.179892
626.870212	41316.269381	32.184909
628.110372	41365.053565	32.189927
628.655442	41426.800543	32.194944
629.125199	41481.972064	32.199962
629.934309	41529.517834	32.204980
629.905442	41578.376439	32.209997
630.977186	41634.926354	32.215015
631.138353	41700.292169	32.220032
631.615795	41761.552672	32.225050
632.131005	41819.391492	32.230068
632.443671	41887.817136	32.235085
632.963049	41937.590009	32.240103
633.424115	42010.101767	32.245120
633.825056	42081.278928	32.250138
634.476071	42149.684388	32.255156
634.716254	42221.936716	32.260173
636.412673	42273.981606	32.265191
637.380846	42323.406751	32.270208
637.946384	42378.937653	32.275226
638.568972	42449.890216	32.280244
639.036986	42505.036678	32.285261
639.930668	42565.972243	32.290279
640.297900	42624.071640	32.295296
640.917501	42687.591044	32.300314
641.191638	42751.041445	32.305332
641.547771	42838.095766	32.310349
642.128831	42902.383102	32.315367
642.840429	42968.297049	32.320384
643.307641	43048.148709	32.325402
643.609739	43119.213599	32.330420
644.273040	43200.520482	32.335437
645.152000	43279.339084	32.340455
645.602502	43372.864893	32.345472
645.895681	43463.837829	32.350490
647.098056	43534.657753	32.355508
647.799849	43612.430466	32.360525
649.021111	43685.470445	32.365543
649.562827	43761.994751	32.370560
650.154893	43840.149610	32.375578
650.860344	43910.803628	32.380596
651.626815	43988.320976	32.385613
652.053827	44062.863825	32.390631
652.865986	44132.954873	32.395648
653.009466	44223.088021	32.400666
654.063230	44288.760717	32.405684
654.149412	44382.364402	32.410701
655.246459	44465.338504	32.415719
655.672519	44558.264962	32.420736
655.963380	44630.111009	32.425754
656.944011	44725.990319	32.430772
657.015648	44824.871293	32.435789
657.821291	44911.264347	32.440807
658.418796	45013.800890	32.445824
659.225565	45097.861352	32.450842
660.046583	45180.615848	32.455860
660.989224	45261.285699	32.460877
662.013170	45344.121070	32.465895
662.691550	45425.858269	32.470912
663.407008	45502.518891	32.475930
664.590394	45578.366864	32.480948
665.236644	45659.943048	32.485965
665.988345	45722.585857	32.490983
667.061039	45796.438540	32.496000
667.438798	45857.375377	32.501018
668.730978	45912.620002	32.506036
669.590983	45970.073791	32.511053
670.764601	46016.080529	32.516071
671.835618	46065.378664	32.521088
672.695179	46109.157776	32.526106
673.106989	46137.845347	32.531124
673.493284	46198.646109	32.536141
674.298584	46238.263382	32.541159
674.584690	46291.663931	32.546176
674.873595	46347.211309	32.551194
675.503249	46403.220416	32.556212
675.731263	46468.790860	32.561229
676.205064	46519.338181	32.566247
676.890747	46588.032091	32.571264
677.525423	46657.363040	32.576282
677.461140	46719.322959	32.581300
677.810166	46807.865250	32.586317
678.723183	46870.987312	32.591335
679.337237	46944.269782	32.596352
680.105414	47011.915901	32.601370
681.423323	47072.729826	32.606388
681.724015	47147.646835	32.611405
682.120793	47215.595008	32.616423
682.911731	47280.554284	32.621440
683.403225	47352.557601	32.626458
684.280115	47423.357600	32.631476
684.831892	47502.241718	32.636493
685.478069	47578.950664	32.641511
686.218448	47658.420050	32.646528
687.310720	47742.107304	32.651546
688.296694	47804.806771	32.656564
688.732913	47867.161461	32.661581
689.095026	47934.322171	32.666599
689.500092	48024.717704	32.671616
690.048924	48109.371053	32.676634
690.811399	48195.960004	32.681652
691.217164	48288.497712	32.686669
691.776460	48370.883139	32.691687
693.407520	48452.460338	32.696704
693.164602	48532.102093	32.701722
694.254301	48616.570482	32.706740
695.087964	48706.806898	32.711757
695.492624	48808.224322	32.716775
696.164410	48890.602896	32.721792
697.038602	48965.122886	32.726810
697.935253	49060.883386	32.731828
698.413988	49146.383483	32.736845
699.056600	49244.236416	32.741863
699.956694	49329.686696	32.746880
700.460078	49425.286594	32.751898
701.032836	49512.083401	32.756916
701.474415	49598.636985	32.761933
701.468408	49715.077498	32.766951
702.726844	49813.412737	32.771968
703.140365	49911.502725	32.776986
704.297916	50022.804126	32.782004
704.644307	50120.394647	32.787021
705.456756	50228.807651	32.792039
706.686515	50323.047740	32.797056
706.941542	50438.170456	32.802074
707.926923	50525.759595	32.807092
709.165284	50619.775487	32.812109
710.330710	50699.250522	32.817127
711.999941	50761.783719	32.822144
712.952112	50840.801867	32.827162
713.753591	50903.450409	32.832180
714.211087	50987.989474	32.837197
715.111179	51050.420078	32.842215
715.782299	51117.010344	32.847232
716.486171	51192.442000	32.852250
717.149302	51246.868030	32.857268
717.496497	51323.802480	32.862285
717.986050	51398.123843	32.867303
718.632058	51474.030443	32.872320
719.115190	51560.800781	32.877338
720.042231	51630.202612	32.882356
720.587324	51717.342434	32.887373
721.100026	51803.407805	32.892391
722.155913	51875.995081	32.897408
722.278495	51965.656774	32.902426
722.843455	52038.202552	32.907444
723.714464	52123.850108	32.912461
724.363480	52206.578322	32.917479
725.524974	52284.838202	32.922496
726.215896	52376.764211	32.927514
726.572757	52446.755873	32.932532
727.356001	52525.641419	32.937549
728.040256	52617.620209	32.942567
728.903165	52679.165183	32.947584
729.383288	52767.192235	32.952602
730.099752	52849.520387	32.957620
730.450702	52935.990220	32.962637
731.132332	53032.766236	32.967655
731.971634	53127.709931	32.972672
731.800108	53241.444683	32.977690
732.684875	53338.435050	32.982708
733.554892	53439.250397	32.987725
734.249499	53541.946257	32.992743
734.888933	53644.215861	32.997760
735.238435	53762.612065	33.002778
736.379895	53862.405552	33.007796
737.619071	53964.483028	33.012813
738.680486	54053.310682	33.017831
739.916635	54141.629741	33.022848
741.221248	54233.583212	33.027866
742.259812	54298.762259	33.032884
743.457110	54371.382896	33.037901
745.461470	54405.471096	33.042919
746.599146	54459.508727	33.047936
746.869878	54524.600526	33.052954
747.582027	54575.410857	33.057972
748.162426	54634.614215	33.062989
748.979012	54685.837200	33.068007
749.136996	54739.159211	33.073024
749.755091	54807.397748	33.078042
750.410043	54865.648126	33.083060
751.002768	54933.032054	33.088077
751.558502	55009.336964	33.093095
752.096382	55084.419430	33.098112
752.726892	55158.469687	33.103130
753.500138	55233.216907	33.108148
754.050754	55312.657586	33.113165
754.478784	55385.320572	33.118183
755.700702	55469.029456	33.123200
755.899959	55558.726584	33.128218
756.924661	55657.676605	33.133236
757.192470	55746.718815	33.138253
757.771518	55837.902454	33.143271
758.753642	55931.086020	33.148288
759.153539	56032.655771	33.153306
759.447242	56118.580466	33.158324
760.568766	56222.970044	33.163341
760.701892	56330.594134	33.168359
761.665449	56437.241322	33.173376
762.448787	56556.524165	33.178394
763.286050	56647.953233	33.183412
764.021134	56762.070444	33.188429
764.901109	56864.531921	33.193447
765.964083	56962.629157	33.198464
766.456251	57081.009136	33.203482
767.109272	57184.956714	33.208500
768.062915	57273.292262	33.213517
768.749603	57398.301906	33.218535
769.700287	57489.058976	33.223552
770.203159	57593.317830	33.228570
771.070364	57705.756808	33.233588
772.122580	57811.752229	33.238605
772.605785	57917.380901	33.243623
773.497552	58018.190833	33.248640
774.355740	58123.069909	33.253658
774.969810	58225.689738	33.258676
776.174386	58325.059390	33.263693
776.793095	58433.764739	33.268711
777.681312	58526.249316	33.273728
778.373396	58610.235911	33.278746
779.044109	58692.893051	33.283764
780.717152	58766.102165	33.288781
781.741417	58847.595708	33.293799
782.556178	58919.272535	33.298816
783.153926	59002.410625	33.303834
783.988482	59090.287315	33.308852
784.690105	59158.906204	33.313869
785.504800	59250.041306	33.318887
786.433565	59325.751441	33.323904
787.064993	59422.920962	33.328922
787.546755	59510.838797	33.333940
787.807935	59604.588352	33.338957
788.275716	59699.631312	33.343975
789.271394	59793.355247	33.348992
789.651805	59901.412766	33.354010
790.422892	60023.347281	33.359028
791.201394	60132.294553	33.364045
791.469056	60251.229621	33.369063
792.304154	60363.764664	33.374080
793.357246	60464.983684	33.379098
793.741920	60583.699158	33.384116
795.115622	60691.205058	33.389133
795.750431	60816.389950	33.394151
796.613416	60922.186594	33.399168
797.503150	61030.930752	33.404186
798.445799	61158.430556	33.409204
799.312756	61255.835452	33.414221
799.876214	61377.610190	33.419239
801.323374	61482.251538	33.424256
802.408603	61592.407390	33.429274
803.473972	61695.747758	33.434292
804.186059	61793.718019	33.439309
805.188859	61891.034012	33.444327
806.719291	61975.540852	33.449344
807.589638	62073.796018	33.454362
808.114181	62154.854558	33.459380
809.059429	62241.759698	33.464397
809.864142	62338.952541	33.469415
810.618901	62435.604231	33.474432
811.419392	62530.896275	33.479450
812.202729	62619.580497	33.484468
813.014905	62699.418119	33.489485
813.266969	62803.220755	33.494503
814.103730	62908.469556	33.499520
814.919305	63007.945477	33.504538
816.006146	63087.676056	33.509556
817.427915	63175.239666	33.514573
818.508056	63258.435673	33.519591
819.275016	63340.343770	33.524608
820.363360	63421.838850	33.529626
821.478281	63488.969388	33.534644
822.697045	63567.719322	33.539661
822.952808	63653.638214	33.544679
823.729785	63728.075164	33.549696
824.252968	63809.203699	33.554714
824.686803	63898.001744	33.559732
825.861304	63967.292032	33.564749
826.267750	64066.587823	33.569767
826.849861	64152.429627	33.574784
827.649563	64242.015735	33.579802
828.086860	64348.121680	33.584820
829.013025	64445.746935	33.589837
829.551413	64549.580654	33.594855
829.851064	64660.932049	33.599872
830.446278	64754.915638	33.604890
830.910427	64868.782041	33.609908
831.711672	64976.044759	33.614925
832.124749	65093.612349	33.619943
832.574142	65216.579201	33.624960
833.154836	65335.776632	33.629978
833.919677	65456.176982	33.634996
835.035514	65590.325731	33.640013
835.422020	65726.909383	33.645031
836.078121	65863.266096	33.650048
837.631454	65984.512801	33.655066
838.862025	66111.268908	33.660084
840.191940	66219.557017	33.665101
840.610532	66345.753273	33.670119
841.415001	66477.304138	33.675136
842.472667	66596.411080	33.680154
843.177308	66717.460838	33.685172
844.449112	66824.333007	33.690189
845.204364	66957.753596	33.695207
846.272734	67081.305689	33.700224
847.244934	67196.637137	33.705242
847.954261	67310.141377	33.710260
849.031229	67430.767126	33.715277
849.724941	67549.560296	33.720295
850.609208	67659.238099	33.725312
851.453340	67792.965435	33.730330
852.263670	67908.055688	33.735348
853.755794	68013.905010	33.740365
855.271124	68116.109541	33.745383
856.980363	68211.657024	33.750400
858.478205	68292.762254	33.755418
858.505750	68390.604988	33.760436
859.420107	68472.995820	33.765453
859.815057	68575.950264	33.770471
860.713268	68680.099196	33.775488
861.722826	68783.572745	33.780506
861.701617	68892.458168	33.785524
862.556714	69001.996064	33.790541
863.040399	69114.244917	33.795559
863.894572	69225.194006	33.800576
864.678717	69346.808494	33.805594
865.348927	69477.502560	33.810612
866.355280	69600.750943	33.815629
867.006931	69714.492642	33.820647
867.679211	69842.387742	33.825664
868.335798	69959.050959	33.830682
868.841296	70095.839400	33.835700
869.803189	70238.363896	33.840717
870.904594	70375.763881	33.845735
871.964079	70513.057867	33.850752
873.274076	70630.381931	33.855770
873.925983	70761.529519	33.860788
875.095707	70887.717480	33.865805
876.130771	71006.258745	33.870823
876.990928	71133.839735	33.875840
878.364659	71242.759788	33.880858
879.338825	71365.505235	33.885876
880.273765	71466.626742	33.890893
880.991638	71595.890622	33.895911
881.723992	71716.009671	33.900928
882.863998	71832.793016	33.905946
883.433620	71952.611458	33.910964
884.368859	72054.279486	33.915981
885.712089	72163.784681	33.920999
886.807007	72275.215773	33.926016
888.287025	72363.301447	33.931034
889.241620	72478.860590	33.936052
890.010893	72569.328223	33.941069
890.513469	72668.610815	33.946087
891.615687	72768.553662	33.951104
892.286710	72860.151662	33.956122
893.052739	72959.075920	33.961140
893.485325	73050.568660	33.966157
893.933371	73170.768080	33.971175
894.803084	73270.916060	33.976192
895.588443	73389.024810	33.981210
896.096519	73498.073954	33.986228
896.974334	73618.426228	33.991245
897.774158	73735.744024	33.996263
898.595197	73861.222899	34.001280
899.382156	73986.853576	34.006298
900.208436	74121.515218	34.011316
901.095448	74245.081953	34.016333
902.110539	74386.322488	34.021351
902.548599	74515.618453	34.026368
903.635182	74641.785247	34.031386
904.344116	74805.718871	34.036404
905.290883	74942.572785	34.041421
905.863142	75080.444335	34.046439
906.497132	75226.654420	34.051456
907.913108	75362.649303	34.056474
908.931239	75505.914007	34.061492
909.951633	75644.480352	34.066509
910.412416	75778.409402	34.071527
911.819179	75936.253504	34.076544
913.245250	76075.419649	34.081562
913.842862	76213.629345	34.086580
915.151073	76351.962910	34.091597
916.316697	76472.858949	34.096615
917.089077	76610.650167	34.101632
918.198185	76742.353006	34.106650
919.625601	76876.053250	34.111668
921.220190	76986.945326	34.116685
922.015540	77100.208863	34.121703
923.019950	77209.713210	34.126720
924.007347	77331.250565	34.131738
924.532550	77457.848829	34.136756
925.461990	77583.887737	34.141773
926.070808	77718.632700	34.146791
926.873934	77855.661309	34.151808
927.545747	77968.861146	34.156826
928.144608	78114.387832	34.161844
929.173336	78253.645989	34.166861
929.603972	78394.325706	34.171879
930.283384	78541.935483	34.176896
931.434807	78681.808573	34.181914
932.311702	78835.548364	34.186932
932.669037	78988.141586	34.191949
933.893478	79136.089098	34.196967
934.805295	79293.880772	34.201984
936.020021	79430.825823	34.207002
936.974143	79600.194374	34.212020
937.819348	79742.819293	34.217037
938.952918	79896.878234	34.222055
939.767635	80069.878873	34.227072
941.272663	80196.027295	34.232090
942.609826	80331.009367	34.237108
943.937130	80460.471604	34.242125
945.170655	80590.797711	34.247143
946.437425	80718.436987	34.252160
947.510311	80843.610333	34.257178
948.331769	80965.043078	34.262196
949.099397	81085.024103	34.267213
950.214125	81208.415017	34.272231
951.030701	81318.552525	34.277248
952.482576	81431.343770	34.282266
953.813959	81542.599294	34.287284
954.696756	81641.372397	34.292301
955.528800	81743.146503	34.297319
956.531239	81847.341103	34.302336
956.697160	81931.570130	34.307354
957.880075	82052.993325	34.312372
958.355951	82167.821907	34.317389
958.996832	82282.199975	34.322407
959.814262	82417.191773	34.327424
960.659201	82525.388331	34.332442
961.727485	82653.849430	34.337460
962.850263	82779.423801	34.342477
963.729758	82897.358891	34.347495
964.234863	83042.161134	34.352512
965.075462	83179.848653	34.357530
965.945095	83307.466867	34.362548
966.736960	83463.656286	34.367565
967.535946	83600.904033	34.372583
967.766646	83761.224444	34.377600
968.520936	83914.209252	34.382618
969.493023	84071.246127	34.387636
970.397343	84233.540080	34.392653
971.656417	84399.401820	34.397671
972.201200	84569.722856	34.402688
973.116057	84729.038657	34.407706
974.574028	84909.549450	34.412724
974.831386	85074.777932	34.417741
975.868771	85246.376591	34.422759
976.796219	85434.166502	34.427776
978.029483	85603.381823	34.432794
979.285341	85766.697795	34.437812
980.009274	85958.094039	34.442829
981.378540	86131.998166	34.447847
983.283571	86292.211566	34.452864
985.037061	86444.472387	34.457882
985.877285	86592.993686	34.462900
986.441669	86747.945785	34.467917
987.782847	86902.258142	34.472935
988.617275	87069.506238	34.477952
989.784647	87220.786910	34.482970
990.792553	87362.331507	34.487988
991.306826	87518.360015	34.493005
992.490914	87674.266317	34.498023
993.247579	87842.095931	34.503040
994.325925	88000.476994	34.508058
995.366362	88169.584588	34.513076
996.374193	88327.783339	34.518093
997.446515	88475.803678	34.523111
998.157300	88643.906032	34.528128
1000.175942	88791.196279	34.533146
1001.161180	88932.152927	34.538164
1002.073638	89093.625134	34.543181
1003.414744	89244.099151	34.548199
1004.212735	89400.289456	34.553216
1005.225176	89555.597417	34.558234
1006.138391	89700.759753	34.563252
1007.119172	89856.853278	34.568269
1008.029346	90012.402601	34.573287
1008.419278	90162.982536	34.578304
1009.372522	90319.855699	34.583322
1010.676559	90484.671034	34.588340
1011.371306	90652.853563	34.593357
1012.509668	90825.640766	34.598375
1013.208511	90984.110772	34.603392
1014.456084	91134.194516	34.608410
1016.002147	91300.437418	34.613428
1016.871065	91460.970935	34.618445
1018.497161	91596.407607	34.623463
1019.144459	91751.885089	34.628480
1020.253909	91899.597854	34.633498
1021.147609	92036.385704	34.638516
1021.997155	92174.947359	34.643533
1022.698417	92313.660871	34.648551
1023.320618	92477.108876	34.653568
1024.159301	92639.351393	34.658586
1025.407305	92799.324939	34.663604
1026.291939	92960.460785	34.668621
1027.152164	93110.576511	34.673639
1028.244096	93283.002968	34.678656
1028.912030	93462.658920	34.683674
1030.168848	93628.864376	34.688692
1030.761550	93805.851709	34.693709
1032.047978	93973.630615	34.698727
1032.901917	94147.729127	34.703744
1034.525978	94318.682628	34.708762
1035.991537	94469.257464	34.713780
1037.077064	94633.725825	34.718797
1038.302843	94797.450576	34.723815
1039.347135	94954.319849	34.728832
1040.502681	95114.849243	34.733850
1042.302700	95256.524964	34.738868
1043.658823	95412.010137	34.743885
1044.766161	95549.599019	34.748903
1045.519158	95715.256225	34.753920
1046.463042	95853.873893	34.758938
1047.355067	96005.128866	34.763956
1048.129024	96172.342818	34.768973
1048.953214	96327.636753	34.773991
1049.727046	96501.936105	34.779008
1050.739010	96672.057565	34.784026
1052.034662	96844.532438	34.789044
1052.880096	97012.651794	34.794061
1053.817851	97173.274861	34.799079
1054.286849	97345.611168	34.804096
1055.500753	97529.948015	34.809114
1056.386165	97703.636019	34.814132
1057.582346	97890.523218	34.819149
1058.560556	98083.379329	34.824167
1059.855660	98265.435618	34.829184
1060.728340	98444.049585	34.834202
1062.089580	98619.254341	34.839220
1062.649276	98811.089982	34.844237
1063.667977	99003.959162	34.849255
1064.813036	99196.201222	34.854272
1066.136660	99368.587633	34.859290
1067.847280	99531.244352	34.864308
1068.798939	99726.978959	34.869325
1070.133107	99905.375188	34.874343
1071.595976	100071.444278	34.879360
1072.820672	100236.610480	34.884378
1074.401960	100398.591415	34.889396
1075.416211	100565.833064	34.894413
1076.337660	100734.256040	34.899431
1077.313667	100897.188442	34.904448
1078.587511	101065.283202	34.909466
1079.543450	101222.624323	34.914484
1080.779480	101385.605563	34.919501
1081.601243	101537.981825	34.924519
1082.841860	101702.844702	34.929536
1083.756147	101864.261316	34.934554
1085.345202	102012.569350	34.939572
1086.286623	102177.085806	34.944589
1087.272088	102336.676549	34.949607
1088.362172	102497.865531	34.954624
1089.272426	102665.606637	34.959642
1090.455679	102823.021379	34.964660
1091.230826	102987.355204	34.969677
1091.954288	103140.187763	34.974695
1092.913504	103298.300881	34.979712
1093.940039	103466.021671	34.984730
1094.537760	103623.987515	34.989748
1095.582256	103790.289139	34.994765
1096.654931	103946.570278	34.999783
1098.148726	104111.489110	35.004800
1099.032282	104289.996631	35.009818
1099.812480	104465.483119	35.014836
1100.893372	104649.070390	35.019853
1102.112053	104816.996146	35.024871
1103.127354	104999.596258	35.029888
1103.875846	105180.886625	35.034906
1104.922631	105370.563416	35.039924
1105.940878	105567.464987	35.044941
1107.024602	105747.310854	35.049959
1108.397482	105936.114716	35.054976
1109.524047	106118.970223	35.059994
1110.637751	106313.480680	35.065012
1112.045052	106513.592620	35.070029
1113.251868	106698.515937	35.075047
1114.628963	106880.702128	35.080064
1115.748330	107056.764222	35.085082
1117.496044	107234.053602	35.090100
1119.585232	107398.407231	35.095117
1120.785008	107557.259968	35.100135
1122.325439	107702.809408	35.105152
1123.594484	107857.789563	35.110170
1125.050565	108016.045454	35.115188
1125.754945	108169.068820	35.120205
1126.402671	108333.792856	35.125223
1127.245548	108487.086494	35.130240
1127.810202	108665.429333	35.135258
1129.032700	108848.249835	35.140276
1129.902786	109038.172077	35.145293
1130.893747	109211.027111	35.150311
1131.764062	109388.450341	35.155328
1132.233152	109587.663660	35.160346
1133.275694	109784.085847	35.165364
1134.326809	109995.074503	35.170381
1134.970326	110209.640739	35.175399
1135.713377	110409.207561	35.180416
1136.643595	110636.687870	35.185434
1137.965690	110850.653161	35.190452
1138.713416	111076.634591	35.195469
1139.856850	111316.613054	35.200487
1141.047439	111539.611788	35.205504
1142.190085	111771.525379	35.210522
1143.359651	111988.450941	35.215540
1144.635768	112229.732941	35.220557
1146.003962	112445.717277	35.225575
1147.185449	112676.340024	35.230592
1148.071662	112914.398799	35.235610
1149.433651	113148.162665	35.240628
1150.886282	113361.530659	35.245645
1153.010161	113553.633704	35.250663
1155.100762	113759.843314	35.255680
1156.487963	113956.948040	35.260698
1158.181411	114147.834101	35.265716
1159.270442	114337.858446	35.270733
1160.510990	114525.452048	35.275751
1161.889941	114700.697463	35.280768
1162.950531	114884.522595	35.285786
1164.201296	115052.519527	35.290804
1165.131170	115240.929359	35.295821
1165.876348	115436.085511	35.300839
1167.169439	115611.110103	35.305856
1168.706842	115793.532248	35.310874
1169.951830	115953.376609	35.315892
1171.215617	116114.067619	35.320909
1172.112874	116286.931969	35.325927
1173.524624	116449.006767	35.330944
1174.526133	116610.668776	35.335962
1175.688600	116763.461768	35.340980
1176.629886	116931.812429	35.345997
1177.291149	117112.918065	35.351015
1178.161828	117290.708804	35.356032
1178.932279	117487.408032	35.361050
1180.026642	117680.646922	35.366068
1181.212622	117858.756598	35.371085
1182.063046	118072.880698	35.376103
1183.512044	118255.079909	35.381120
1184.130027	118467.851613	35.386138
1185.030197	118665.424475	35.391156
1186.367411	118880.868017	35.396173
1187.291095	119109.799631	35.401191
1188.484808	119310.407439	35.406208
1190.031240	119537.161658	35.411226
1191.532562	119744.817373	35.416244
1193.377230	119937.567500	35.421261
1195.122473	120126.394621	35.426279
1196.586212	120315.130060	35.431296
1197.672570	120524.228356	35.436314
1198.363909	120730.415598	35.441332
1199.510361	120929.711948	35.446349
1200.543250	121134.464486	35.451367
1201.563315	121344.960815	35.456384
1202.477708	121569.060164	35.461402
1203.111202	121787.467273	35.466420
1204.279267	122020.246396	35.471437
1205.411543	122243.339197	35.476455
1206.517019	122477.412145	35.481472
1207.802835	122705.665992	35.486490
1208.969033	122944.218578	35.491508
1209.809224	123176.516050	35.496525
1210.897901	123432.890089	35.501543
1212.633794	123674.497300	35.506560
1213.499770	123902.690276	35.511578
1215.294265	124118.363082	35.516596
1217.084388	124349.663844	35.521613
1218.472683	124579.980870	35.526631
1220.885827	124789.042491	35.531648
1222.356503	125003.393776	35.536666
1223.494930	125205.850554	35.541684
1224.915461	125410.011051	35.546701
1226.172542	125612.349594	35.551719
1227.857432	125810.842172	35.556736
1228.904832	126008.186598	35.561754
1230.391069	126200.846659	35.566772
1231.606833	126393.425855	35.571789
1232.957336	126585.705208	35.576807
1234.371067	126772.905779	35.581824
1235.397659	126979.575288	35.586842
1236.702773	127163.437581	35.591860
1237.561833	127361.316177	35.596877
1238.587895	127553.439735	35.601895
1239.633942	127758.083425	35.606912
1240.395823	127962.686665	35.611930
1241.471700	128174.717389	35.616948
1242.527761	128377.842618	35.621965
1243.727523	128590.337391	35.626983
1245.633540	128772.208946	35.632000
1246.661790	128981.299869	35.637018
1247.840173	129184.410217	35.642036
1249.614364	129399.261994	35.647053
1250.462404	129601.618403	35.652071
1251.805947	129800.383323	35.657088
1252.781770	130004.356355	35.662106
1253.626611	130188.350689	35.667124
1255.091262	130378.036454	35.672141
1255.933885	130589.133512	35.677159
1256.912487	130783.490485	35.682176
1258.388702	130987.919711	35.687194
1258.945119	131215.660638	35.692212
1260.089924	131445.118734	35.697229
1260.925589	131670.814078	35.702247
1262.029451	131898.862528	35.707264
1263.091311	132142.321013	35.712282
1264.346605	132375.443692	35.717300
1264.996755	132606.741171	35.722317
1266.150534	132873.007405	35.727335
1267.468933	133139.907867	35.732352
1268.926321	133389.458705	35.737370
1270.064615	133654.555083	35.742388
1270.754399	133916.406356	35.747405
1271.880521	134195.162123	35.752423
1272.975901	134464.088005	35.757440
1274.590881	134756.421082	35.762458
1275.700858	135033.158402	35.767476
1276.945612	135306.630434	35.772493
1278.587467	135588.368310	35.777511
1280.715190	135840.477030	35.782528
1282.689353	136105.366767	35.787546
1283.935999	136363.722907	35.792564
1285.230879	136633.571940	35.797581
1286.390892	136900.833788	35.802599
1287.778911	137167.299486	35.807616
1289.270102	137432.558557	35.812634
1289.942212	137697.384427	35.817652
1291.260886	137962.688897	35.822669
1292.201946	138234.828117	35.827687
1293.919546	138507.475318	35.832704
1295.351763	138775.861098	35.837722
1297.031124	139043.980021	35.842740
1299.040313	139310.487147	35.847757
1300.198507	139557.357641	35.852775
1302.116283	139812.536154	35.857792
1303.805566	140047.543725	35.862810
1305.666998	140287.000292	35.867828
1307.806809	140508.560102	35.872845
1309.990366	140717.751712	35.877863
1311.406363	140931.673954	35.882880
1312.614054	141139.773961	35.887898
1314.188030	141324.725156	35.892916
1316.042634	141516.680952	35.897933
1316.735666	141741.441950	35.902951
1318.102371	141937.474767	35.907968
1319.379037	142138.075662	35.912986
1319.967898	142344.408494	35.918004
1321.004578	142550.136084	35.923021
1322.014884	142788.140284	35.928039
1322.917449	143013.027153	35.933056
1323.727298	143235.458117	35.938074
1325.064110	143471.434983	35.943092
1325.976790	143702.271763	35.948109
1326.737020	143969.769481	35.953127
1327.955580	144224.614344	35.958144
1328.722392	144470.291325	35.963162
1329.581736	144741.012170	35.968180
1330.952944	145006.337283	35.973197
1332.017806	145288.390570	35.978215
1333.113261	145560.181982	35.983232
1334.191085	145843.949513	35.988250
1335.400172	146131.692279	35.993268
1336.511042	146387.787927	35.998285
1337.605236	146675.338455	36.003303
1338.602501	146951.734734	36.008320
1340.332902	147234.213525	36.013338
1341.345214	147523.762719	36.018356
1343.184947	147801.079071	36.023373
1344.270692	148093.334651	36.028391
1345.710016	148374.183685	36.033408
1347.549549	148657.340421	36.038426
1349.047108	148931.310354	36.043444
1350.615717	149209.189497	36.048461
1352.467474	149481.456374	36.053479
1354.275812	149746.655520	36.058496
1356.309381	150006.771676	36.063514
1357.636573	150275.757402	36.068532
1359.129071	150534.140248	36.073549
1360.556802	150793.410712	36.078567
1362.014697	151049.900410	36.083584
1363.313529	151302.917570	36.088602
1364.287871	151571.273336	36.093620
1366.191187	151826.147495	36.098637
1367.825151	152084.758725	36.103655
1369.497858	152325.113744	36.108672
1371.215871	152573.757898	36.113690
1372.274798	152834.891751	36.118708
1373.584418	153077.962379	36.123725
1374.961346	153333.187277	36.128743
1376.078683	153585.983361	36.133760
1377.730828	153843.842571	36.138778
1378.660073	154112.756540	36.143796
1379.627032	154370.973383	36.148813
1380.739929	154640.900846	36.153831
1381.910396	154916.084717	36.158848
1383.550867	155193.019544	36.163866
1384.998982	155473.108502	36.168884
1386.314302	155756.405246	36.173901
1387.264056	156040.855273	36.178919
1388.824355	156310.631724	36.183936
1391.047461	156582.901056	36.188954
1392.695792	156854.341134	36.193972
1394.374968	157112.040031	36.198989
1395.417223	157394.137857	36.204007
1397.078881	157660.621376	36.209024
1399.138769	157914.888392	36.214042
1400.679881	158173.263937	36.219060
1402.618947	158409.020634	36.224077
1403.875940	158669.450594	36.229095
1404.863331	158915.350902	36.234112
1406.123742	159173.119577	36.239130
1407.139624	159450.314219	36.244148
1408.542601	159719.188340	36.249165
1409.600510	159973.963613	36.254183
1410.565712	160253.709320	36.259200
1411.878235	160521.398505	36.264218
1412.704965	160814.288417	36.269236
1413.750130	161121.873237	36.274253
1414.785073	161416.242762	36.279271
1416.264945	161704.857392	36.284288
1418.125910	161998.625350	36.289306
1419.104606	162302.462013	36.294324
1420.784560	162600.285797	36.299341
1422.692060	162906.181089	36.304359
1423.571722	163207.541372	36.309376
1425.253589	163502.948054	36.314394
1426.384179	163810.652856	36.319412
1427.633427	164108.418872	36.324429
1429.324326	164415.566177	36.329447
1430.379758	164720.473399	36.334464
1431.835745	165009.508022	36.339482
1432.992925	165307.335686	36.344500
1434.527177	165591.590776	36.349517
1436.267680	165880.267124	36.354535
1437.731822	166181.107939	36.359552
1439.144969	166482.619036	36.364570
1440.506474	166767.887349	36.369588
1441.983858	167068.148475	36.374605
1443.944064	167340.671657	36.379623
1445.548591	167632.960165	36.384640
1447.432200	167917.147435	36.389658
1448.843619	168211.235338	36.394676
1450.347493	168483.447564	36.399693
1452.070496	168759.774479	36.404711
1453.440112	169055.169116	36.409728
1455.554573	169328.173956	36.414746
1456.897807	169600.927071	36.419764
1458.502792	169877.737175	36.424781
1460.222694	170146.713579	36.429799
1461.642165	170416.197972	36.434816
1463.311147	170695.781440	36.439834
1464.868292	170979.788255	36.444852
1466.130179	171239.596258	36.449869
1468.507877	171508.751336	36.454887
1468.970136	171782.766926	36.459904
1470.655026	172063.333219	36.464922
1471.763906	172343.602897	36.469940
1472.891967	172625.799939	36.474957
1474.307424	172915.362101	36.479975
1475.112451	173208.605339	36.484992
1476.862597	173509.498761	36.490010
1477.942642	173813.956383	36.495028
1479.379304	174123.953460	36.500045
1480.260863	174429.526466	36.505063
1481.631261	174756.581548	36.510080
1482.949861	175073.380918	36.515098
1484.611367	175394.047148	36.520116
1485.744135	175728.584696	36.525133
1488.051474	176033.006249	36.530151
1489.990068	176346.120246	36.535168
1491.504795	176658.087898	36.540186
1493.159489	176973.257928	36.545204
1494.445393	177301.562522	36.550221
1496.031658	177618.778548	36.555239
1497.089557	177949.003361	36.560256
1498.576399	178263.371742	36.565274
1500.171748	178585.757783	36.570292
1501.624932	178905.986456	36.575309
1503.842158	179229.098964	36.580327
1505.253302	179537.154823	36.585344
1507.191121	179855.088552	36.590362
1508.331422	180170.719083	36.595380
1509.878902	180495.892037	36.600397
1510.967867	180813.730693	36.605415
1511.974799	181149.924674	36.610432
1513.280399	181484.459677	36.615450
1514.662822	181821.091052	36.620468
1515.801608	182178.529198	36.625485
1517.728398	182499.831838	36.630503
1519.237590	182852.035027	36.635520
1521.065055	183180.377082	36.640538
1522.238812	183529.784356	36.645556
1523.824784	183870.164946	36.650573
1525.159599	184218.890151	36.655591
1526.453415	184569.629844	36.660608
1527.830486	184922.845876	36.665626
1529.340720	185284.559181	36.670644
1530.770631	185642.531022	36.675661
1532.446782	185968.528807	36.680679
1534.012939	186314.868407	36.685696
1535.691100	186648.638100	36.690714
1537.046265	186981.803054	36.695732
1538.676917	187325.955089	36.700749
1540.001518	187653.213985	36.705767
1541.712986	188001.012547	36.710784
1542.960354	188340.486669	36.715802
1545.528395	188664.512476	36.720820
1547.182796	188988.005430	36.725837
1548.982076	189317.213917	36.730855
1550.298588	189647.405221	36.735872
1551.862309	189981.606997	36.740890
1553.787501	190319.965475	36.745908
1554.656278	190662.384640	36.750925
1556.650145	191003.934666	36.755943
1558.104855	191330.951849	36.760960
1560.432265	191652.000137	36.765978
1562.418257	191974.769466	36.770996
1563.963031	192302.234134	36.776013
1565.974704	192628.722235	36.781031
1567.784964	192942.538040	36.786048
1569.169331	193256.108383	36.791066
1570.833079	193563.210705	36.796084
1572.836767	193867.656044	36.801101
1574.615560	194183.349567	36.806119
1575.785211	194511.916317	36.811136
1577.075624	194823.986779	36.816154
1578.710701	195141.828961	36.821172
1579.935489	195467.852643	36.826189
1581.552800	195781.105361	36.831207
1583.219769	196105.472477	36.836224
1585.200411	196414.821715	36.841242
1587.258850	196732.335437	36.846260
1588.635438	197047.627281	36.851277
1590.239345	197351.063648	36.856295
1591.574212	197679.022869	36.861312
1593.083515	198008.681562	36.866330
1594.433966	198330.255582	36.871348
1595.474200	198669.821456	36.876365
1596.904057	198999.053866	36.881383
1597.930730	199352.692436	36.886400
1599.036532	199697.521523	36.891418
1600.254844	200068.094027	36.896436
1601.271345	200452.286672	36.901453
1602.856498	200824.199336	36.906471
1604.302490	201204.199084	36.911488
1605.098028	201595.315942	36.916506
1607.156335	201993.628622	36.921524
1608.409160	202381.259107	36.926541
1610.027496	202787.838095	36.931559
1611.905210	203194.198863	36.936576
1613.471811	203598.188214	36.941594
1615.521865	203987.828938	36.946612
1617.037182	204392.237488	36.951629
1618.736389	204789.774325	36.956647
1620.106084	205207.568510	36.961664
1622.404353	205607.626475	36.966682
1624.411346	205983.191206	36.971700
1625.854495	206385.286288	36.976717
1627.265823	206784.773132	36.981735
1628.902477	207182.980557	36.986752
1630.540704	207572.327045	36.991770
1632.556393	207967.428619	36.996788
1634.184611	208359.155116	37.001805
1635.785605	208757.859000	37.006823
1637.584204	209163.249313	37.011840
1639.579001	209545.093256	37.016858
1642.136701	209895.012975	37.021876
1644.363954	210237.725611	37.026893
1646.493243	210569.535733	37.031911
1648.514164	210898.888996	37.036928
1650.347684	211220.122433	37.041946
1652.315735	211544.103069	37.046964
1653.660225	211875.044773	37.051981
1655.140813	212187.629322	37.056999
1656.556639	212516.657058	37.062016
1658.584726	212846.854856	37.067034
1660.257779	213161.392125	37.072052
1661.559053	213483.814001	37.077069
1662.993890	213816.957792	37.082087
1664.364573	214166.621284	37.087104
1666.058147	214505.286863	37.092122
1667.534595	214837.360966	37.097140
1668.791640	215188.418648	37.102157
1670.423819	215536.266558	37.107175
1672.020572	215883.867668	37.112192
1673.235416	216253.654137	37.117210
1675.171309	216612.376840	37.122228
1676.655241	216988.902932	37.127245
1678.459019	217362.863396	37.132263
1679.658827	217731.616866	37.137280
1681.186741	218172.955290	37.142298
1682.919062	218565.320233	37.147316
1684.188235	218947.400784	37.152333
1686.071544	219333.115004	37.157351
1688.132687	219714.153508	37.162368
1689.821068	220098.455143	37.167386
1692.347004	220464.612589	37.172404
1694.901573	220812.403529	37.177421
1697.062429	221176.795057	37.182439
1699.075903	221527.674700	37.187456
1700.891363	221895.783120	37.192474
1702.008529	222242.876214	37.197492
1703.447221	222614.376519	37.202509
1704.970998	222989.826301	37.207527
1706.197119	223373.606579	37.212544
1707.751412	223748.596732	37.217562
1709.053943	224138.640636	37.222580
1710.455259	224531.285721	37.227597
1711.896991	224929.945151	37.232615
1713.481618	225325.661437	37.237632
1714.937014	225737.224336	37.242650
1716.910497	226125.259281	37.247668
1718.283759	226540.445267	37.252685
1719.991237	226945.442994	37.257703
1721.651678	227360.939997	37.262720
1723.454649	227773.062073	37.267738
1725.503190	228186.846794	37.272756
1727.307015	228603.416457	37.277773
1728.996543	229018.863312	37.282791
1730.776638	229432.797926	37.287808
1732.929981	229830.949390	37.292826
1735.109689	230227.141850	37.297844
1736.409409	230648.424017	37.302861
1738.235064	231046.404503	37.307879
1740.185456	231455.135452	37.312896
1741.935640	231873.654519	37.317914
1743.571354	232271.999998	37.322932
1745.376797	232684.873302	37.327949
1746.841315	233095.162301	37.332967
1748.663739	233514.969580	37.337984
1749.800633	233942.003437	37.343002
1751.778095	234350.204494	37.348020
1753.391973	234777.034935	37.353037
1754.883145	235187.350477	37.358055
1756.524162	235590.885557	37.363072
1757.675121	236010.022774	37.368090
1759.791544	236407.385043	37.373108
1761.493567	236815.612282	37.378125
1763.035893	237240.250896	37.383143
1764.702130	237639.773188	37.388160
1766.345777	238068.689944	37.393178
1768.149433	238498.800591	37.398196
1768.971080	238946.169711	37.403213
1770.817043	239387.528435	37.408231
1772.336030	239824.141122	37.413248
1773.437680	240287.699000	37.418266
1775.193035	240755.163618	37.423284
1777.035534	241221.802035	37.428301
1778.844153	241684.255690	37.433319
1780.878595	242135.851690	37.438336
1782.560269	242616.287644	37.443354
1785.125062	243083.217246	37.448372
1787.865735	243530.076227	37.453389
1789.730982	243992.702982	37.458407
1792.195888	244425.383690	37.463424
1794.984563	244861.009216	37.468442
1796.917367	245284.583405	37.473460
1798.708924	245722.788079	37.478477
1800.687874	246151.588930	37.483495
1802.748613	246574.559702	37.488512
1804.295535	247014.915122	37.493530
1806.450512	247434.543789	37.498548
1807.930721	247872.828394	37.503565
1809.679306	248299.079158	37.508583
1811.709306	248731.152098	37.513600
1812.961952	249156.088572	37.518618
1814.719100	249587.318451	37.523636
1816.534508	250025.931474	37.528653
1818.331000	250469.196852	37.533671
1820.150043	250900.646571	37.538688
1821.640074	251344.471480	37.543706
1823.713883	251791.223482	37.548724
1825.141782	252267.321433	37.553741
1826.750658	252710.035662	37.558759
1828.646747	253163.981873	37.563776
1830.633983	253620.860174	37.568794
1832.865845	254059.941632	37.573812
1835.003650	254510.444941	37.578829
1837.539271	254940.052269	37.583847
1839.617996	255380.760217	37.588864
1841.508954	255824.369941	37.593882
1843.078306	256267.702693	37.598900
1844.815826	256697.772794	37.603917
1846.857870	257135.667837	37.608935
1849.067989	257567.743352	37.613952
1850.390911	258019.195644	37.618970
1852.339864	258435.691448	37.623988
1854.465708	258875.630803	37.629005
1856.050358	259320.892585	37.634023
1857.741663	259750.488381	37.639040
1859.277615	260201.601030	37.644058
1860.960104	260651.495555	37.649076
1862.482328	261100.197141	37.654093
1863.723035	261568.150025	37.659111
1865.681010	262023.054238	37.664128
1867.662258	262489.741653	37.669146
1869.918309	262938.728334	37.674164
1871.663016	263397.935146	37.679181
1873.798931	263852.936530	37.684199
1876.283965	264308.794660	37.689216
1877.668763	264761.938113	37.694234
1879.886951	265201.759585	37.699252
1881.917309	265638.919069	37.704269
1883.393588	266064.331811	37.709287
1885.151029	266506.641844	37.714304
1886.388086	266945.303156	37.719322
1888.011055	267381.080744	37.724340
1889.809053	267823.967411	37.729357
1891.334525	268282.115135	37.734375
1893.617306	268730.992412	37.739392
1894.806854	269201.591410	37.744410
1896.656497	269674.367308	37.749428
1898.194939	270151.487138	37.754445
1899.301383	270643.004958	37.759463
1901.763018	271125.153556	37.764480
1903.500871	271614.609956	37.769498
1905.406390	272109.448846	37.774516
1908.053185	272597.864845	37.779533
1909.575258	273100.132363	37.784551
1911.707118	273578.750144	37.789568
1913.479798	274081.381193	37.794586
1915.790917	274588.368038	37.799604
1918.105160	275071.043153	37.804621
1920.075209	275576.077670	37.809639
1921.935195	276059.283209	37.814656
1923.739712	276570.719159	37.819674
1925.785354	277076.347940	37.824692
1927.979346	277567.319428	37.829709
1929.167936	278070.674261	37.834727
1931.252279	278573.880234	37.839744
1933.011928	279102.007398	37.844762
1935.010950	279614.141243	37.849780
1936.226117	280135.039856	37.854797
1937.956023	280676.021447	37.859815
1939.970411	281215.151113	37.864832
1941.765668	281756.754016	37.869850
1944.152544	282286.598362	37.874868
1946.121226	282827.813948	37.879885
1947.831235	283376.284656	37.884903
1950.196134	283913.570553	37.889920
1952.212555	284463.384396	37.894938
1954.195135	285006.445258	37.899956
1956.289536	285548.317429	37.904973
1957.995936	286098.939010	37.909991
1960.029997	286652.374957	37.915008
1961.886168	287200.250038	37.920026
1963.795522	287759.494002	37.925044
1967.164152	288270.258902	37.930061
1969.225698	288808.060844	37.935079
1971.305660	289337.932714	37.940096
1973.501857	289880.305905	37.945114
1975.196272	290402.718748	37.950132
1977.253797	290938.328688	37.955149
1979.080010	291486.598572	37.960167
1981.107792	292022.894829	37.965184
1982.624433	292551.475339	37.970202
1984.854679	293099.824109	37.975220
1986.789910	293648.193726	37.980237
1988.252687	294200.372577	37.985255
1990.670264	294725.442410	37.990272
1993.095145	295265.646821	37.995290
1995.341954	295790.028885	38.000308
1997.401210	296336.359067	38.005325
1999.033607	296872.648161	38.010343
2001.475401	297393.485561	38.015360
2003.797096	297931.357573	38.020378
2005.586834	298457.986805	38.025396
2007.390539	298984.712736	38.030413
2009.201098	299533.557023	38.035431
2011.033328	300062.634894	38.040448
2012.874782	300576.799738	38.045466
2014.505469	301102.908462	38.050484
2016.459301	301623.297368	38.055501
2017.967647	302149.547723	38.060519
2019.558685	302671.489386	38.065536
2021.222176	303216.274098	38.070554
2023.144808	303765.940049	38.075572
2025.541039	304298.025939	38.080589
2027.658289	304839.983485	38.085607
2029.564826	305391.140894	38.090624
2031.418653	305951.497295	38.095642
2033.672537	306519.885736	38.100660
2035.785126	307055.303763	38.105677
2038.036259	307614.872981	38.110695
2039.911752	308169.040347	38.115712
2041.872821	308738.859340	38.120730
2043.640500	309308.757168	38.125748
2046.026741	309861.635559	38.130765
2047.786781	310456.795435	38.135783
2050.010088	311031.863052	38.140800
2052.145342	311599.246358	38.145818
2054.083456	312185.145651	38.150836
2056.396757	312761.658827	38.155853
2058.385268	313347.693470	38.160871
2060.688550	313923.056888	38.165888
2063.056201	314508.766163	38.170906
2065.078590	315093.080370	38.175924
2067.133959	315675.048326	38.180941
2069.117106	316270.786915	38.185959
2071.240303	316847.681056	38.190976
2073.150642	317436.845196	38.195994
2074.560599	318046.756862	38.201012
2076.892210	318643.916466	38.206029
2078.679307	319247.458120	38.211047
2080.981362	319857.689320	38.216064
2083.240535	320468.023727	38.221082
2085.797822	321074.926360	38.226100
2088.244875	321696.035587	38.231117
2089.611369	322312.975303	38.236135
2091.456606	322914.900304	38.241152
2093.246151	323541.508864	38.246170
2095.129808	324169.314567	38.251188
2097.681538	324779.002141	38.256205
2099.818140	325403.453192	38.261223
2101.936308	326037.498435	38.266240
2104.386985	326674.097490	38.271258
2106.704894	327283.951473	38.276276
2108.637387	327909.147152	38.281293
2110.590633	328539.867697	38.286311
2112.812718	329166.094252	38.291328
2115.270507	329796.413605	38.296346
2117.190788	330429.632907	38.301364
2119.644215	331037.775850	38.306381
2121.867097	331669.230715	38.311399
2123.785752	332296.946087	38.316416
2126.316288	332912.012459	38.321434
2128.483322	333544.572660	38.326452
2131.056083	334162.639321	38.331469
2132.927477	334784.343397	38.336487
2135.050399	335398.484745	38.341504
2137.569353	336019.915624	38.346522
2139.255811	336639.166577	38.351540
2141.056460	337256.969967	38.356557
2143.248274	337896.963930	38.361575
2145.170958	338511.889433	38.366592
2147.420369	339150.995500	38.371610
2149.134444	339789.293530	38.376628
2151.694278	340390.841345	38.381645
2153.800492	340997.838070	38.386663
2156.128375	341595.323179	38.391680
2158.415870	342193.594687	38.396698
2160.480745	342783.697285	38.401716
2162.729771	343375.463054	38.406733
2165.015361	343967.520234	38.411751
2166.873099	344557.534139	38.416768
2169.053033	345162.462456	38.421786
2171.260474	345773.444579	38.426804
2173.473394	346375.737922	38.431821
2175.465392	346984.100465	38.436839
2177.609377	347595.627904	38.441856
2179.986017	348189.673402	38.446874
2182.818511	348778.205015	38.451892
2185.604978	349377.954053	38.456909
2187.880746	349981.027872	38.461927
2189.724971	350596.320895	38.466944
2191.901640	351193.177319	38.471962
2193.526690	351809.834905	38.476980
2195.492771	352417.901072	38.481997
2198.007339	353037.719285	38.487015
2200.335574	353655.504011	38.492032
2202.266509	354264.210209	38.497050
2204.381795	354899.724722	38.502068
2206.650424	355520.715388	38.507085
2208.840814	356158.279645	38.512103
2210.457428	356793.696019	38.517120
2212.727479	357437.647596	38.522138
2214.459553	358100.860419	38.527156
2216.027319	358761.704705	38.532173
2218.325052	359424.980710	38.537191
2219.670363	360114.384336	38.542208
2222.442956	360781.822609	38.547226
2224.345588	361476.134891	38.552244
2226.612280	362162.357919	38.557261
2228.996099	362845.911315	38.562279
2231.014678	363558.790333	38.567296
2233.416196	364269.233941	38.572314
2235.380562	364964.007832	38.577332
2237.731532	365669.918566	38.582349
2239.937080	366377.210277	38.587367
2242.245448	367098.119896	38.592384
2244.411263	367798.517206	38.597402
2246.652067	368529.380190	38.602420
2249.289983	369245.476358	38.607437
2251.619245	369967.443858	38.612455
2254.043646	370691.258671	38.617472
2256.456520	371397.686220	38.622490
2258.571652	372128.904915	38.627508
2261.134732	372834.265333	38.632525
2263.843527	373546.765814	38.637543
2265.776799	374267.191829	38.642560
2268.584167	374983.528006	38.647578
2270.967077	375713.057165	38.652596
2273.412041	376409.286905	38.657613
2275.806381	377103.000439	38.662631
2278.320862	377819.504662	38.667648
2280.516401	378521.160440	38.672666
2282.998278	379229.931381	38.677684
2285.089501	379927.264532	38.682701
2287.861755	380623.608906	38.687719
2290.142196	381307.746889	38.692736
2292.793355	381999.163418	38.697754
2295.212292	382694.179231	38.702772
2297.302899	383367.656549	38.707789
2300.167211	384055.749557	38.712807
2302.417147	384735.486210	38.717824
2304.873868	385399.860450	38.722842
2306.869437	386062.674492	38.727860
2308.817259	386714.986445	38.732877
2311.065935	387355.674564	38.737895
2313.068298	388008.382235	38.742912
2315.411932	388665.938550	38.747930
2317.534531	389328.030230	38.752948
2320.026421	389979.805315	38.757965
2322.637612	390633.397760	38.762983
2324.663294	391285.780209	38.768000
2327.158442	391945.929844	38.773018
2329.159685	392616.083546	38.778036
2332.018411	393284.332210	38.783053
2334.464594	393937.704479	38.788071
2336.723452	394603.767187	38.793088
2338.948494	395265.004957	38.798106
2340.686524	395960.272210	38.803124
2342.481563	396654.576151	38.808141
2345.052220	397344.503440	38.813159
2346.747036	398051.919907	38.818176
2348.614008	398753.411303	38.823194
2350.377051	399484.630440	38.828212
2352.592394	400223.308713	38.833229
2354.756212	400964.738941	38.838247
2356.376461	401732.366395	38.843264
2358.872727	402488.501752	38.848282
2360.933688	403255.002131	38.853300
2363.116897	404027.036262	38.858317
2366.353741	404795.125505	38.863335
2368.907754	405565.586728	38.868352
2372.067085	406314.846585	38.873370
2374.219872	407085.078609	38.878388
2376.961009	407844.652600	38.883405
2380.157298	408608.741517	38.888423
2382.282678	409377.925832	38.893440
2384.939276	410130.964789	38.898458
2386.961591	410906.380175	38.903476
2389.575428	411666.881857	38.908493
2392.133046	412434.666641	38.913511
2394.381632	413205.241310	38.918528
2397.999919	413956.570433	38.923546
2400.588628	414711.720646	38.928564
2402.817835	415457.308992	38.933581
2405.286837	416214.765856	38.938599
2407.113444	416988.515789	38.943616
2409.727355	417734.659286	38.948634
2412.370261	418501.695165	38.953652
2414.333013	419257.348189	38.958669
2417.164736	420011.316134	38.963687
2419.417160	420773.435282	38.968704
2421.840862	421543.657008	38.973722
2424.046487	422323.766513	38.978740
2426.564071	423092.279321	38.983757
2429.032336	423853.965471	38.988775
2431.224058	424625.295117	38.993792
2433.726599	425395.739217	38.998810
2436.432387	426166.986434	39.003828
2439.089344	426936.242651	39.008845
2441.319530	427707.772714	39.013863
2443.008814	428501.948534	39.018880
2445.881474	429269.677397	39.023898
2448.521197	430050.076868	39.028916
2450.667703	430834.227803	39.033933
2453.165862	431604.373344	39.038951
2455.270390	432393.137030	39.043968
2457.998815	433184.707414	39.048986
2460.724584	433967.950027	39.054004
2463.244583	434743.253393	39.059021
2465.798583	435504.909738	39.064039
2467.968800	436262.707007	39.069056
2470.348805	437016.294554	39.074074
2472.389050	437758.171727	39.079092
2474.733933	438518.902223	39.084109
2477.287510	439260.544596	39.089127
2480.535868	440005.084431	39.094144
2483.426138	440746.875485	39.099162
2485.815662	441498.338947	39.104180
2488.458306	442245.484973	39.109197
2490.910854	442996.179146	39.114215
2493.000572	443739.925327	39.119232
2495.466488	444496.182615	39.124250
2498.103260	445258.254537	39.129268
2500.365948	446013.126976	39.134285
2502.992104	446778.587806	39.139303
2505.039455	447559.849944	39.144320
2507.528482	448340.808669	39.149338
2509.862158	449122.877510	39.154356
2511.635425	449909.866113	39.159373
2514.510937	450705.495579	39.164391
2516.803368	451509.132224	39.169408
2519.236682	452332.844659	39.174426
2521.683931	453141.248990	39.179444
2523.908795	453967.157010	39.184461
2526.694582	454788.540220	39.189479
2529.241738	455612.863297	39.194496
2531.456485	456442.669552	39.199514
2534.362984	457270.052937	39.204532
2536.760575	458100.571172	39.209549
2539.355214	458945.281251	39.214567
2542.028435	459796.161987	39.219584
2544.519826	460634.094517	39.224602
2547.788407	461468.729737	39.229620
2550.303459	462320.187240	39.234637
2552.977891	463164.404109	39.239655
2555.676432	464015.809540	39.244672
2558.029389	464862.281896	39.249690
2560.994866	465709.880563	39.254708
2563.439766	466544.387747	39.259725
2566.364313	467378.224349	39.264743
2569.248298	468219.309292	39.269760
2571.701244	469062.955585	39.274778
2573.994129	469919.275125	39.279796
2576.327457	470775.802561	39.284813
2579.107519	471644.647979	39.289831
2580.899275	472511.039963	39.294848
2582.888898	473394.083093	39.299866
2585.312142	474265.444240	39.304884
2587.591559	475151.287679	39.309901
2590.085595	476054.785138	39.314919
2592.484502	476973.661298	39.319936
2594.655579	477874.093036	39.324954
2597.324012	478783.692655	39.329972
2599.434444	479705.258901	39.334989
2602.642533	480620.840548	39.340007
2605.216192	481546.177174	39.345024
2607.697166	482475.016972	39.350042
2610.879774	483395.159705	39.355060
2613.078616	484333.645850	39.360077
2615.759815	485234.842250	39.365095
2618.500627	486175.061396	39.370112
2621.073068	487126.264565	39.375130
2623.786268	488042.610867	39.380148
2626.271019	488982.218733	39.385165
2629.209963	489897.775212	39.390183
2632.893238	490814.574472	39.395200
2635.607291	491717.554985	39.400218
2638.334070	492631.337495	39.405236
2640.899149	493516.937827	39.410253
2643.398829	494388.676196	39.415271
2645.917550	495262.688457	39.420288
2648.736011	496151.492200	39.425306
2651.532755	497019.767753	39.430324
2654.206857	497882.973718	39.435341
2656.879653	498750.827869	39.440359
2659.567493	499625.243687	39.445376
2662.039453	500502.020547	39.450394
2664.215749	501391.814679	39.455412
2666.243107	502292.481122	39.460429
2668.749122	503204.065785	39.465447
2671.948161	504093.647437	39.470464
2674.506455	505004.064947	39.475482
2677.319248	505911.868520	39.480500
2679.168933	506840.354682	39.485517
2681.889472	507757.651921	39.490535
2684.519843	508699.971536	39.495552
2687.921951	509613.068044	39.500570
2691.530944	510525.171175	39.505588
2694.429602	511448.934417	39.510605
2696.885784	512363.593031	39.515623
2699.834467	513289.308224	39.520640
2702.097319	514211.705368	39.525658
2705.432922	515129.587763	39.530676
2707.996617	516056.061110	39.535693
2710.704230	516983.917452	39.540711
2714.164582	517913.307935	39.545728
2716.998190	518822.993734	39.550746
2719.822236	519750.010915	39.555764
2722.238994	520678.803006	39.560781
2725.134634	521603.328967	39.565799
2727.703842	522537.827612	39.570816
2730.060060	523477.039341	39.575834
2732.781614	524415.629202	39.580852
2735.327351	525365.220434	39.585869
2737.900549	526310.013217	39.590887
2740.581886	527269.182526	39.595904
2742.698108	528230.347594	39.600922
2745.360957	529197.302588	39.605940
2747.662102	530179.863295	39.610957
2750.189502	531169.521368	39.615975
2752.447105	532159.459683	39.620992
2754.987808	533159.050934	39.626010
2757.655179	534163.737936	39.631028
2760.226059	535185.737014	39.636045
2763.200188	536205.785932	39.641063
2766.555716	537225.146583	39.646080
2769.392051	538234.103849	39.651098
2772.476160	539261.165314	39.656116
2775.137088	540273.429884	39.661133
2778.013974	541288.404578	39.666151
2781.059236	542310.875746	39.671168
2783.878053	543336.026918	39.676186
2787.181371	544346.285301	39.681204
2789.790613	545371.624646	39.686221
2792.546551	546376.294264	39.691239
2795.674144	547388.172767	39.696256
2798.023882	548416.398891	39.701274
2800.841555	549440.951718	39.706292
2804.137661	550461.176390	39.711309
2807.457785	551467.797111	39.716327
2810.541300	552475.136927	39.721344
2813.233784	553474.976795	39.726362
2816.199336	554464.896465	39.731380
2819.120659	555468.673496	39.736397
2821.701754	556478.915204	39.741415
2824.385427	557475.797148	39.746432
2826.840173	558450.834143	39.751450
2829.654554	559409.310098	39.756468
2831.973299	560383.826230	39.761485
2834.835009	561363.858342	39.766503
2837.520703	562330.584671	39.771520
2839.863753	563318.695291	39.776538
2842.793542	564310.803799	39.781556
2845.303769	565306.773510	39.786573
2847.413403	566314.585178	39.791591
2850.211333	567332.851139	39.796608
2852.145127	568365.640613	39.801626
2854.704134	569401.507966	39.806644
2857.286584	570448.734584	39.811661
2860.340652	571518.889900	39.816679
2863.130017	572576.651004	39.821696
2865.462437	573664.865744	39.826714
2867.745697	574755.253614	39.831732
2870.841970	575843.958081	39.836749
2874.477909	576935.339591	39.841767
2877.854926	578030.180949	39.846784
2880.681800	579139.566210	39.851802
2883.108901	580251.175918	39.856820
2885.938519	581355.296213	39.861837
2888.960928	582478.044466	39.866855
2892.278863	583601.444043	39.871872
2894.936612	584725.451283	39.876890
2897.790168	585854.938811	39.881908
2900.273765	587007.495942	39.886925
2903.444596	588157.925273	39.891943
2906.251366	589304.344971	39.896960
2908.559498	590463.218361	39.901978
2911.934337	591613.283901	39.906996
2915.152622	592777.797459	39.912013
2918.731919	593920.290281	39.917031
2922.047759	595058.908581	39.922048
2925.563611	596213.415881	39.927066
2929.019168	597359.955163	39.932084
2932.335381	598494.684503	39.937101
2935.744012	599623.979535	39.942119
2938.698690	600750.084891	39.947136
2941.795487	601889.727949	39.952154
2944.657928	603014.526804	39.957172
2947.345273	604140.796768	39.962189
2949.775147	605266.147723	39.967207
2953.519499	606391.872203	39.972224
2956.267537	607521.753849	39.977242
2959.304044	608649.223627	39.982260
2962.777281	609785.916729	39.987277
2965.472766	610915.368457	39.992295
2968.789238	612038.350714	39.997312
2971.659223	613169.848308	40.002330
2974.107727	614298.349595	40.007348
2976.761553	615445.608243	40.012365
2979.308893	616599.217046	40.017383
2982.058516	617742.171271	40.022400
2984.452164	618906.965191	40.027418
2987.598077	620073.111401	40.032436
2990.685046	621238.093281	40.037453
2993.499207	622406.344509	40.042471
2996.649593	623580.162157	40.047488
2999.460437	624761.104497	40.052506
3002.360469	625933.758336	40.057524
3004.739727	627125.205483	40.062541
3007.900755	628308.947966	40.067559
3011.117347	629499.393223	40.072576
3014.143230	630715.358189	40.077594
3017.050694	631899.492180	40.082612
3020.472988	633089.850014	40.087629
3023.459168	634246.044638	40.092647
3025.934549	635407.437881	40.097664
3028.864526	636568.427611	40.102682
3031.902658	637707.658754	40.107700
3035.269143	638858.039444	40.112717
3038.278724	640015.636545	40.117735
3041.535845	641169.370852	40.122752
3044.308413	642330.938037	40.127770
3047.335372	643494.476705	40.132788
3050.494730	644659.207782	40.137805
3053.053255	645833.779271	40.142823
3055.904150	647015.048200	40.147840
3058.821400	648217.807512	40.152858
3061.655771	649415.401801	40.157876
3064.643586	650622.199542	40.162893
3067.853901	651831.357180	40.167911
3071.519258	653029.130148	40.172928
3074.390443	654238.848950	40.177946
3077.564642	655454.947004	40.182964
3081.063645	656668.600116	40.187981
3083.883765	657893.273691	40.192999
3086.880949	659115.075853	40.198016
3089.727391	660342.078785	40.203034
3093.058685	661589.959526	40.208052
3095.612691	662834.074148	40.213069
3098.364875	664086.956695	40.218087
3102.114672	665345.285961	40.223104
3104.961328	666615.493662	40.228122
3108.106291	667863.788522	40.233140
3111.209939	669138.147250	40.238157
3114.240946	670416.128161	40.243175
3117.202184	671705.537910	40.248192
3120.004662	673001.710944	40.253210
3123.118731	674289.946788	40.258228
3126.485894	675575.527969	40.263245
3129.740141	676885.857242	40.268263
3133.166314	678177.036231	40.273280
3136.175562	679487.039798	40.278298
3139.804031	680793.178286	40.283316
3142.890747	682094.749597	40.288333
3145.797259	683405.207800	40.293351
3148.878977	684716.045894	40.298368
3152.090088	686046.241971	40.303386
3154.841695	687363.806117	40.308404
3157.998664	688691.588097	40.313421
3160.683888	690039.208719	40.318439
3164.126986	691370.471195	40.323456
3167.745204	692711.234296	40.328474
3171.487473	694039.272044	40.333492
3175.132137	695360.728185	40.338509
3178.489212	696674.296940	40.343527
3181.927851	697984.334480	40.348544
3185.464860	699312.608840	40.353562
3188.288168	700630.140103	40.358580
3191.957535	701939.897840	40.363597
3194.970561	703261.017529	40.368615
3198.558798	704565.140441	40.373632
3201.818544	705871.995654	40.378650
3204.798903	707163.786523	40.383668
3208.471991	708482.267826	40.388685
3211.700984	709772.982389	40.393703
3215.095951	711075.113040	40.398720
3218.293857	712373.265037	40.403738
3221.692686	713667.869045	40.408756
3225.478555	714936.323353	40.413773
3228.792473	716219.958448	40.418791
3232.193399	717496.554932	40.423808
3234.971954	718761.828732	40.428826
3237.650494	720009.761904	40.433844
3240.690927	721238.653233	40.438861
3243.456720	722488.179883	40.443879
3247.124912	723728.617599	40.448896
3250.345214	724968.448867	40.453914
3254.076085	726195.058304	40.458932
3257.678851	727419.973829	40.463949
3260.680593	728651.081684	40.468967
3263.622435	729890.908180	40.473984
3266.705922	731131.510998	40.479002
3269.831852	732380.660685	40.484020
3273.323491	733628.174834	40.489037
3276.364156	734889.051690	40.494055
3279.945808	736142.038771	40.499072
3282.898706	737412.902979	40.504090
3285.537734	738687.417838	40.509108
3289.110753	739955.505527	40.514125
3291.734011	741263.218236	40.519143
3294.922597	742567.465123	40.524160
3297.441621	743881.965648	40.529178
3300.707513	745208.157452	40.534196
3304.046847	746537.367905	40.539213
3306.830170	747883.206592	40.544231
3310.040455	749236.383395	40.549248
3313.649446	750596.060525	40.554266
3316.705216	751956.576234	40.559284
3320.273088	753321.842847	40.564301
3323.340242	754706.456013	40.569319
3326.786192	756105.531851	40.574336
3329.632511	757491.550695	40.579354
3333.080056	758911.384500	40.584372
3336.093826	760316.800481	40.589389
3339.356187	761742.338057	40.594407
3342.283130	763160.331335	40.599424
3345.539148	764591.679441	40.604442
3348.553186	766051.271951	40.609460
3352.232098	767503.930635	40.614477
3355.220582	768980.412455	40.619495
3358.155796	770447.565928	40.624512
3361.284358	771941.918204	40.629530
3364.229778	773430.888741	40.634548
3368.173322	774930.250506	40.639565
3371.328372	776438.816849	40.644583
3374.893519	777941.259600	40.649600
3378.467162	779444.962524	40.654618
3381.940255	780949.745355	40.659636
3385.278685	782470.726533	40.664653
3388.422147	783994.952029	40.669671
3391.762551	785514.849042	40.674688
3395.292302	787052.832638	40.679706
3398.690579	788584.623205	40.684724
3402.066129	790122.558922	40.689741
3405.026892	791666.405123	40.694759
3408.701876	793212.932820	40.699776
3412.296160	794754.333713	40.704794
3416.023735	796302.280455	40.709812
3419.652421	797824.389416	40.714829
3423.379366	799353.640631	40.719847
3427.157736	800884.945545	40.724864
3431.151428	802418.323526	40.729882
3434.398814	803948.353023	40.734900
3438.364129	805479.245043	40.739917
3441.416888	807008.478873	40.744935
3445.251542	808516.952196	40.749952
3448.663009	810025.063764	40.754970
3451.655461	811558.957314	40.759988
3455.772346	813060.657980	40.765005
3459.167188	814559.360384	40.770010
3462.813215	815996.057362	40.775015
3466.172065	817383.003481	40.780020
3469.331118	818701.860898	40.785024
3472.372962	819941.890186	40.790029
3475.461014	821126.689551	40.795034
3478.058336	822246.690928	40.800039
3481.128485	823288.660443	40.805044
3483.775597	824268.528413	40.810048
3486.179888	825168.788176	40.815053
3488.383945	826006.722816	40.820058
3490.860957	826787.801780	40.825063
3493.451801	827491.347343	40.830068
3495.174494	828130.301905	40.835072
3497.270823	828718.944844	40.840077
3499.230620	829251.070195	40.845082
3501.046581	829716.871902	40.850087
3502.533077	830137.745593	40.855092
3503.940099	830511.802295	40.860096
3505.500804	830834.956902	40.865101
3507.049177	831138.020049	40.870106
3508.241478	831379.383593	40.875111
3509.188236	831567.633286	40.880116
3510.243221	831740.912923	40.885120
3511.212149	831860.375362	40.890125
3512.260315	831952.714128	40.895130
3512.632689	832017.468621	40.900135
3514.063936	832052.058308	40.905140
3514.521276	832071.227263	40.910144
3514.907824	832045.716270	40.915149
3515.508401	832009.912762	40.920154
3516.133205	831953.053299	40.925159
3517.119631	831874.544462	40.930164
3517.184354	831777.136815	40.935168
3517.647349	831656.997455	40.940173
3517.911107	831527.998493	40.945178
3518.245646	831376.857014	40.950183
3518.610841	831218.721482	40.955188
3518.540077	831040.967015	40.960192
3518.972716	830853.354305	40.965197
3519.343271	830655.145140	40.970202
3519.133623	830464.793502	40.975207
3519.887955	830240.712875	40.980212
3519.923196	830032.768604	40.985216
3520.095327	829780.772079	40.990221
3520.218519	829557.602562	40.995226
3520.596697	829306.433290	41.000231
3520.283952	829045.350659	41.005236
3519.999564	828792.169502	41.010240
3520.415270	828532.070322	41.015245
3520.393690	828270.664419	41.020250
3520.650676	827999.329698	41.025255
3520.773990	827717.937336	41.030260
3520.511702	827450.184448	41.035264
3520.985703	827162.405217	41.040269
3520.876387	826886.881077	41.045274
3520.605955	826588.103039	41.050279
3520.807300	826287.278228	41.055284
3521.045083	825994.500275	41.060288
3521.091615	825695.433862	41.065293
3521.241915	825397.607977	41.070298
3520.861365	825080.151212	41.075303
3520.723188	824765.866469	41.080308
3520.364099	824464.806142	41.085312
3520.540498	824156.455222	41.090317
3520.783175	823861.478824	41.095322
3520.552912	823543.580968	41.100327
3520.454354	823230.243581	41.105332
3520.028026	822921.836477	41.110336
3520.128479	822617.045661	41.115341
3519.859390	822313.964824	41.120346
3520.035339	822007.274700	41.125351
3520.128107	821691.631634	41.130356
3519.676283	821388.929954	41.135360
3519.557413	821080.288613	41.140365
3519.692806	820789.400567	41.145370
3519.462396	820487.061640	41.150375
3519.401836	820177.781621	41.155380
3519.097345	819881.397024	41.160384
3519.083782	819581.770465	41.165389
3519.013120	819285.516575	41.170394
3519.260668	818975.983178	41.175399
3518.991912	818669.799631	41.180404
3518.871506	818380.120993	41.185408
3518.872239	818076.117295	41.190413
3518.566231	817780.080083	41.195418
3518.371504	817494.438083	41.200423
3518.531908	817193.696662	41.205428
3518.148203	816900.619501	41.210432
3518.195397	816605.451267	41.215437
3517.996765	816321.816127	41.220442
3518.010572	816030.936581	41.225447
3517.885302	815746.677501	41.230452
3517.298327	815461.307252	41.235456
3517.435329	815177.764358	41.240461
3517.661463	814901.001705	41.245466
3517.414820	814623.277128	41.250471
3517.499640	814335.985468	41.255476
3517.337018	814060.721546	41.260480
3517.444005	813777.663382	41.265485
3517.019966	813488.656204	41.270490
3517.167195	813223.201130	41.275495
3516.908682	812942.274381	41.280500
3516.508759	812675.418370	41.285504
3516.625401	812386.862821	41.290509
3516.675714	812124.466841	41.295514
3516.213780	811849.847977	41.300519
3516.416141	811578.783133	41.305524
3516.129867	811328.513362	41.310528
3516.028831	811049.931930	41.315533
3515.981056	810796.614353	41.320538
3516.096894	810537.968171	41.325543
3516.189338	810276.620787	41.330548
3515.735935	810020.057809	41.335552
3515.947541	809750.633648	41.340557
3515.793408	809493.168369	41.345562
3515.321550	809237.510092	41.350567
3515.234521	808979.769289	41.355572
3515.057870	808741.100302	41.360576
3515.009417	808477.403351	41.365581
3515.034440	808235.399327	41.370586
3515.071256	807996.718155	41.375591
3514.874737	807742.183963	41.380596
3514.134226	807501.701674	41.385600
3514.562974	807263.861798	41.390605
3514.124271	807031.990771	41.395610
3514.076377	806788.967000	41.400615
3513.811182	806563.180112	41.405620
3513.661282	806328.001657	41.410624
3513.829534	806095.900890	41.415629
3513.933179	805874.639743	41.420634
3513.651848	805646.569695	41.425639
3513.965306	805410.940217	41.430644
3513.634951	805195.858515	41.435648
3513.581441	804959.391274	41.440653
3513.650025	804736.480854	41.445658
3513.427727	804532.101105	41.450663
3513.503218	804297.747846	41.455668
3513.157196	804084.890121	41.460672
3512.920975	803849.444843	41.465677
3512.746783	803644.883682	41.470682
3512.661510	803431.766622	41.475687
3513.315467	803218.815538	41.480692
3512.919083	803009.562920	41.485696
3512.412151	802794.042829	41.490701
3512.331208	802582.517725	41.495706
3512.372659	802382.789518	41.500711
3512.264891	802175.720866	41.505716
3511.849220	801981.355025	41.510720
3511.959779	801772.766455	41.515725
3512.058542	801577.813896	41.520730
3511.949529	801381.761527	41.525735
3512.147037	801169.558555	41.530740
3512.021430	800978.109971	41.535744
3511.909937	800780.274470	41.540749
3511.863639	800578.202308	41.545754
3511.591684	800380.283688	41.550759
3511.839954	800191.254605	41.555764
3511.530678	799999.024053	41.560768
3511.526737	799801.241095	41.565773
3511.586914	799617.478792	41.570778
3511.090965	799427.717178	41.575783
3511.491930	799229.998525	41.580788
3511.180114	799055.313835	41.585792
3511.038503	798869.208992	41.590797
3511.160859	798679.914165	41.595802
3510.826623	798494.861867	41.600807
3510.774611	798315.796116	41.605812
3510.826254	798135.186897	41.610816
3510.717750	797955.973946	41.615821
3510.636468	797765.509653	41.620826
3510.577815	797604.983837	41.625831
3510.575626	797429.323719	41.630836
3510.335663	797267.052576	41.635840
3510.492280	797083.551285	41.640845
3510.359956	796911.090929	41.645850
3510.086269	796753.625113	41.650855
3510.264943	796568.977396	41.655860
3510.139971	796406.569149	41.660864
3510.029353	796228.932656	41.665869
3510.263791	796064.444027	41.670874
3509.784326	795897.319200	41.675879
3510.171308	795731.864630	41.680884
3509.591589	795574.177175	41.685888
3509.313784	795404.699301	41.690893
3509.469761	795257.049177	41.695898
3509.548848	795096.148502	41.700903
3509.632181	794948.700310	41.705908
3509.440445	794792.257420	41.710912
3509.375663	794624.395493	41.715917
3509.293753	794468.467570	41.720922
3508.824346	794312.845603	41.725927
3508.986257	794164.680391	41.730932
3508.853851	794022.995142	41.735936
3508.954446	793875.472493	41.740941
3509.068860	793734.723191	41.745946
3509.008007	793593.508727	41.750951
3508.640535	793439.275197	41.755956
3508.425446	793303.876864	41.760960
3508.942627	793156.958296	41.765965
3508.829508	793010.828260	41.770970
3508.615604	792873.309044	41.775975
3508.729901	792729.149926	41.780980
3508.604949	792594.754828	41.785984
3508.586982	792448.548351	41.790989
3507.821775	792306.883728	41.795994
3507.949708	792181.184422	41.800999
3508.011679	792048.172961	41.806004
3507.951907	791923.580918	41.811008
3507.956699	791786.250186	41.816013
3507.782269	791661.623282	41.821018
3507.643819	791533.990936	41.826023
3507.880352	791408.702248	41.831028
3507.720326	791286.375816	41.836032
3507.976990	791158.622485	41.841037
3507.763471	791026.718270	41.846042
3507.760208	790898.659090	41.851047
3508.173605	790760.651481	41.856052
3507.634327	790645.059724	41.861056
3507.729129	790519.680388	41.866061
3507.625451	790396.739601	41.871066
3507.329412	790277.071947	41.876071
3507.407889	790151.000757	41.881076
3507.563116	790033.171353	41.886080
3507.164950	789915.676888	41.891085
3507.555382	789792.251065	41.896090
3506.820944	789687.439356	41.901095
3507.210507	789550.984945	41.906100
3507.349990	789436.146395	41.911104
3507.015936	789324.529702	41.916109
3507.264113	789199.200108	41.921114
3507.085899	789095.959240	41.926119
3507.288896	788978.448567	41.931124
3507.122808	788869.549697	41.936128
3506.780024	788742.146589	41.941133
3507.189013	788635.263106	41.946138
3506.374778	788521.943288	41.951143
3506.930702	788412.476085	41.956148
3506.920213	788311.015056	41.961152
3506.562304	788200.662798	41.966157
3506.855711	788097.428092	41.971162
3506.529764	787997.980978	41.976167
3506.522502	787888.696832	41.981172
3506.444445	787783.011526	41.986176
3506.166781	787685.715246	41.991181
3506.504302	787586.054778	41.996186
3506.257425	787487.423306	42.001191
3506.271214	787368.737338	42.006196
3506.189278	787278.384719	42.011200
3506.707464	787179.475477	42.016205
3506.542088	787075.367411	42.021210
3506.172526	786978.764980	42.026215
3506.340212	786873.025735	42.031220
3506.413092	786776.298521	42.036224
3506.079744	786680.571142	42.041229
3506.113577	786576.177146	42.046234
3505.797875	786486.639760	42.051239
3506.421786	786384.014272	42.056244
3505.950117	786293.467550	42.061248
3505.846397	786196.023997	42.066253
3505.784815	786103.194523	42.071258
3505.849934	786023.767602	42.076263
3505.957894	785915.614513	42.081268
3505.521082	785835.825611	42.086272
3505.715069	785754.456627	42.091277
3505.751533	785668.244162	42.096282
3505.712227	785583.715174	42.101287
3505.926798	785487.783243	42.106292
3505.645480	785404.177209	42.111296
3505.703894	785303.940821	42.116301
3505.727987	785206.807027	42.121306
3505.229839	785123.135075	42.126311
3505.304853	785037.843118	42.131316
3505.095156	784961.449757	42.136320
3505.196374	784877.528668	42.141325
3505.585781	784798.674142	42.146330
3504.791420	784722.423727	42.151335
3505.325034	784650.331116	42.156340
3505.410946	784557.654090	42.161344
3505.251416	784479.575070	42.166349
3505.372183	784394.071200	42.171354
3505.456737	784316.491245	42.176359
3505.349105	784228.563725	42.181364
3504.916248	784148.657039	42.186368
3505.196511	784066.959615	42.191373
3505.303096	783987.946043	42.196378
3505.364052	783920.695256	42.201383
3505.386436	783826.150100	42.206388
3505.094092	783746.215800	42.211392
3505.213496	783663.753261	42.216397
3505.324435	783578.142940	42.221402
3505.157319	783507.974399	42.226407
3505.165187	783425.970236	42.231412
3504.984569	783356.048400	42.236416
3505.023787	783266.314006	42.241421
3505.241506	783187.125770	42.246426
3504.697773	783122.328440	42.251431
3505.100879	783039.664450	42.256436
3504.973659	782964.466174	42.261440
3504.916764	782885.073882	42.266445
3504.652771	782812.061164	42.271450
3504.915522	782745.159743	42.276455
3504.813517	782674.136017	42.281460
3504.442540	782604.139853	42.286464
3504.708159	782536.153674	42.291469
3504.517329	782468.340440	42.296474
3504.525945	782400.198520	42.301479
3504.587624	782329.242838	42.306484
3504.650932	782265.272608	42.311488
3504.838217	782197.640550	42.316493
3504.564762	782122.014782	42.321498
3504.484932	782056.836259	42.326503
3504.583120	781980.114557	42.331508
3504.454524	781914.499965	42.336512
3504.338209	781844.946519	42.341517
3504.169316	781786.275014	42.346522
3504.406097	781725.469652	42.351527
3504.186452	781657.309128	42.356532
3504.099728	781600.295523	42.361536
3503.756381	781524.625814	42.366541
3503.928233	781477.114434	42.371546
3503.780117	781426.407867	42.376551
3504.196654	781368.374628	42.381556
3504.488765	781305.883620	42.386560
3504.213458	781237.629898	42.391565
3504.799841	781182.716449	42.396570
3504.125073	781115.659149	42.401575
3503.974844	781045.660738	42.406580
3503.903526	780992.035184	42.411584
3503.841575	780931.715247	42.416589
3504.097160	780882.513067	42.421594
3504.065032	780845.463553	42.426599
3503.991638	780768.904914	42.431604
3504.065250	780712.792908	42.436608
3503.974370	780660.447600	42.441613
3504.318052	780592.184260	42.446618
3503.955464	780534.912443	42.451623
3503.964643	780476.348628	42.456628
3503.962700	780417.687749	42.461632
3503.713590	780351.143804	42.466637
3504.037728	780302.713813	42.471642
3503.868742	780250.378412	42.476647
3503.947821	780194.458353	42.481652
3503.931007	780139.095020	42.486656
3503.711534	780091.540598	42.491661
3503.963732	780042.579360	42.496666
3503.524633	779980.295815	42.501671
3503.570516	779923.493257	42.506676
3503.714248	779876.861921	42.511680
3503.633487	779816.683464	42.516685
3503.767208	779766.312597	42.521690
3503.581604	779718.947023	42.526695
3503.249722	779662.746045	42.531700
3503.300176	779621.837696	42.536704
3503.509159	779570.222622	42.541709
3503.951740	779526.837447	42.546714
3503.262386	779483.195496	42.551719
3503.916463	779438.495264	42.556724
3503.818687	779384.862195	42.561728
3503.664111	779330.253687	42.566733
3503.321639	779280.646976	42.571738
3503.303923	779230.887991	42.576743
3503.414575	779179.286342	42.581748
3503.501730	779145.358653	42.586752
3503.588506	779097.008956	42.591757
3503.415582	779041.515314	42.596762
3503.290657	778987.293123	42.601767
3503.382615	778937.612512	42.606772
3503.428832	778896.602340	42.611776
3503.102405	778853.979729	42.616781
3503.161684	778810.456535	42.621786
3503.420484	778775.612826	42.626791
3503.497663	778718.008122	42.631796
3503.344944	778672.648508	42.636800
3503.327310	778631.893485	42.641805
3503.630443	778585.621420	42.646810
3503.020479	778550.132137	42.651815
3503.431107	778489.960215	42.656820
3503.290302	778453.605569	42.661824
3503.130658	778410.263724	42.666829
3503.258819	778360.819349	42.671834
3503.137709	778322.984011	42.676839
3503.108378	778278.438473	42.681844
3503.248244	778241.248902	42.686848
3502.937764	778196.306127	42.691853
3503.194773	778153.091032	42.696858
3503.003078	778113.001743	42.701863
3503.329800	778065.541018	42.706868
3503.232633	778024.352643	42.711872
3502.975913	777982.058048	42.716877
3502.876436	777940.131141	42.721882
3502.855968	777910.842997	42.726887
3503.004705	777874.880837	42.731892
3502.848385	777853.885450	42.736896
3503.029295	777812.207003	42.741901
3502.643458	777771.261670	42.746906
3502.848134	777738.883456	42.751911
3502.908066	777687.525759	42.756916
3502.797178	777669.082373	42.761920
3502.684368	777626.171234	42.766925
3502.780205	777583.323938	42.771930
3502.505510	777555.553199	42.776935
3502.835408	777529.356658	42.781940
3502.460335	777490.032634	42.786945
3502.644477	777459.428932	42.791949
3502.920766	777421.228061	42.796954
3502.887930	777388.838187	42.801959
3502.925854	777339.204826	42.806964
3502.998830	777313.394467	42.811969
3502.845254	777275.854448	42.816973
3502.916437	777237.440233	42.821978
3502.760618	777205.906786	42.826983
3502.853566	777164.829950	42.831988
3502.712550	777131.078183	42.836993
3502.702583	777099.569487	42.841997
3502.772752	777059.431277	42.847002
3502.350629	777037.935736	42.852007
3502.475104	777000.594679	42.857012
3502.469243	776977.208671	42.862017
3502.313848	776945.033962	42.867021
3502.558650	776908.903519	42.872026
3502.493438	776896.555963	42.877031
3502.471982	776848.553855	42.882036
3502.341465	776836.709322	42.887041
3502.328263	776814.013316	42.892045
3502.470238	776772.975441	42.897050
3502.760591	776746.388716	42.902055
3502.807761	776708.172628	42.907060
3502.517604	776683.946233	42.912065
3502.582337	776644.545210	42.917069
3502.833697	776607.279723	42.922074
3502.850109	776590.240557	42.927079
3502.890424	776534.052617	42.932084
3502.993358	776500.011560	42.937089
3502.665011	776475.298373	42.942093
3502.790097	776426.924686	42.947098
3502.615103	776403.909383	42.952103
3502.693856	776364.455304	42.957108
3502.758552	776338.150471	42.962113
3502.775308	776300.380426	42.967117
3502.886509	776265.549070	42.972122
3502.363661	776245.741970	42.977127
3502.673990	776208.120055	42.982132
3502.650140	776187.541227	42.987137
3502.593380	776162.388316	42.992141
3502.831231	776115.274274	42.997146
3502.595800	776101.032988	43.002151
3502.469065	776046.296835	43.007156
3502.621843	776026.377850	43.012161
3502.501913	776003.056762	43.017165
3502.454398	775960.962218	43.022170
3502.282112	775948.187514	43.027175
3502.654516	775901.591606	43.032180
3502.837284	775880.239234	43.037185
3502.777545	775855.036516	43.042189
3503.070602	775807.074262	43.047194
3502.504799	775773.139985	43.052199
3502.781921	775751.279256	43.057204
3502.839414	775712.416100	43.062209
3502.627363	775677.093508	43.067213
3502.654961	775647.345183	43.072218
3502.391799	775609.272971	43.077223
3502.607795	775584.516355	43.082228
3502.094278	775553.182442	43.087233
3502.167299	775532.191854	43.092237
3502.243917	775503.469027	43.097242
3502.393394	775471.927066	43.102247
3502.427544	775442.029091	43.107252
3502.450277	775435.623373	43.112257
3502.253591	775391.038570	43.117261
3502.393863	775374.419395	43.122266
3502.235208	775352.727756	43.127271
3502.361341	775327.541855	43.132276
3502.116813	775308.178836	43.137281
3502.110559	775275.282764	43.142285
3502.265915	775249.500813	43.147290
3502.008615	775230.582921	43.152295
3501.996186	775197.589022	43.157300
3502.061109	775196.691902	43.162305
3501.904688	775159.880219	43.167309
3502.036238	775140.504058	43.172314
3501.989550	775140.511784	43.177319
3502.118412	775106.952474	43.182324
3502.188964	775082.858355	43.187329
3502.055089	775062.737732	43.192333
3502.059201	775042.495827	43.197338
3501.852787	775035.142527	43.202343
3502.606975	774994.880341	43.207348
3502.411908	774974.572559	43.212353
3502.604881	774942.971913	43.217357
3502.896358	774902.292944	43.222362
3502.510554	774884.774322	43.227367
3502.522657	774849.164570	43.232372
3502.561551	774819.903534	43.237377
3502.172214	774798.937761	43.242381
3502.445356	774765.500878	43.247386
3502.565977	774748.341767	43.252391
3502.780805	774709.053379	43.257396
3502.582667	774681.012862	43.262401
3502.375028	774653.023053	43.267405
3502.464088	774630.549703	43.272410
3501.922563	774612.317305	43.277415
3502.017023	774594.374116	43.282420
3502.286785	774559.213036	43.287425
3502.029596	774542.411192	43.292429
3502.456919	774508.110455	43.297434
3502.107242	774488.664088	43.302439
3502.229581	774451.950697	43.307444
3502.288656	774441.006863	43.312449
3501.898801	774420.828140	43.317453
3502.195292	774404.821332	43.322458
3502.192164	774382.510170	43.327463
3502.379549	774349.922832	43.332468
3502.301637	774325.850689	43.337473
3502.296131	774290.191877	43.342477
3502.262088	774273.648184	43.347482
3502.083663	774249.641602	43.352487
3502.138130	774221.557721	43.357492
3502.276072	774199.666056	43.362497
3501.970380	774179.423552	43.367501
3502.159656	774149.839551	43.372506
3502.512186	774136.285673	43.377511
3502.584772	774100.957866	43.382516
3502.218875	774074.469577	43.387521
3502.043698	774054.993317	43.392525
3502.201256	774030.438121	43.397530
3502.153015	774015.521623	43.402535
3502.191772	773992.660566	43.407540
3502.044495	773954.708453	43.412545
3501.613037	773948.671792	43.417549
3501.821265	773933.072549	43.422554
3501.738485	773923.875285	43.427559
3501.883065	773897.794837	43.432564
3501.871083	773886.615601	43.437569
3501.569190	773864.204310	43.442573
3502.022281	773840.732707	43.447578
3501.606474	773832.821608	43.452583
3501.612353	773825.875438	43.457588
3502.008031	773808.225516	43.462593
3501.845051	773800.913079	43.467597
3501.986885	773781.925707	43.472602
3502.102759	773760.873748	43.477607
3502.016958	773735.717310	43.482612
3501.983249	773719.320088	43.487617
3502.102648	773707.921909	43.492621
3502.299382	773673.556759	43.497626
3501.874994	773647.027307	43.502631
3502.033958	773632.075901	43.507636
3502.062291	773602.516215	43.512641
3501.496771	773599.456858	43.517645
3502.340365	773593.554684	43.522650
3501.963631	773565.884141	43.527655
3501.978168	773543.863080	43.532660
3501.926763	773511.902478	43.537665
3501.772227	773497.987623	43.542669
3501.999275	773479.625806	43.547674
3501.826298	773452.906462	43.552679
3501.880825	773439.400395	43.557684
3501.985984	773431.649345	43.562689
3502.096970	773411.483869	43.567693
3502.262484	773394.757550	43.572698
3501.843915	773373.102880	43.577703
3502.024576	773349.723854	43.582708
3501.972443	773326.038277	43.587713
3501.753551	773299.128897	43.592717
3502.231065	773282.006106	43.597722
3501.823770	773271.629964	43.602727
3501.801880	773249.712546	43.607732
3502.024135	773234.700649	43.612737
3501.929972	773214.716211	43.617741
3502.037540	773200.708358	43.622746
3502.025586	773186.227554	43.627751
3501.482140	773161.784937	43.632756
3501.478565	773143.411011	43.637761
3501.685995	773137.169916	43.642765
3501.918100	773125.161133	43.647770
3501.694671	773086.872261	43.652775
3501.783441	773080.158044	43.657780
3501.909106	773076.541252	43.662785
3501.805527	773055.178595	43.667789
3502.032654	773033.761401	43.672794
3502.008292	773022.435107	43.677799
3501.723934	773000.510921	43.682804
3501.978538	772994.508248	43.687809
3501.768491	772995.922235	43.692813
3501.888927	772957.526787	43.697818
3501.822029	772954.582072	43.702823
3501.919063	772938.604944	43.707828
3501.950242	772906.036957	43.712833
3502.054090	772909.074203	43.717837
3501.985832	772885.045024	43.722842
3501.780996	772868.132201	43.727847
3502.167534	772834.667887	43.732852
3502.002063	772819.719014	43.737857
3501.685727	772814.302879	43.742861
3501.636877	772807.808139	43.747866
3501.921105	772776.478758	43.752871
3501.549520	772756.982153	43.757876
3501.887287	772754.709663	43.762881
3501.521712	772738.167868	43.767885
3501.776902	772709.109142	43.772890
3501.393658	772715.428894	43.777895
3501.748712	772691.526414	43.782900
3502.011669	772682.319913	43.787905
3501.716705	772664.731764	43.792909
3501.830427	772646.288015	43.797914
3501.819240	772633.579536	43.802919
3501.553566	772616.922483	43.807924
3501.721149	772597.385908	43.812929
3501.734018	772606.251561	43.817933
3501.986081	772570.197146	43.822938
3502.021075	772549.450649	43.827943
3501.550019	772541.153129	43.832948
3501.698377	772515.214972	43.837953
3501.792543	772507.169169	43.842957
3501.693455	772500.189775	43.847962
3501.841431	772488.193817	43.852967
3501.828824	772460.360609	43.857972
3501.977030	772445.408575	43.862977
3501.615689	772445.271066	43.867981
3501.931999	772415.856257	43.872986
3501.541462	772404.540065	43.877991
3501.647592	772396.295106	43.882996
3501.980817	772364.069109	43.888001
3501.761436	772347.354555	43.893005
3502.100490	772330.745044	43.898010
3501.453896	772319.815769	43.903015
3501.555789	772296.150783	43.908020
3501.717735	772298.193366	43.913025
3501.618287	772290.129954	43.918029
3501.820474	772271.621431	43.923034
3501.980172	772258.490020	43.928039
3501.862565	772250.232485	43.933044
3502.468890	772232.544110	43.938049
3502.114254	772218.659800	43.943053
3502.052980	772181.768286	43.948058
3502.067330	772167.527492	43.953063
3502.024258	772145.758091	43.958068
3501.957276	772123.056465	43.963073
3501.549886	772108.589416	43.968077
3501.891244	772085.229189	43.973082
3501.732488	772072.494785	43.978087
3501.678634	772064.128003	43.983092
3501.904862	772046.353989	43.988097
3501.727354	772016.723324	43.993101
3501.900250	772008.368397	43.998106
3501.945919	772004.370107	44.003111
3501.645234	771963.181249	44.008116
3501.733054	771961.491657	44.013121
3501.999341	771955.387682	44.018125
3501.748012	771933.947579	44.023130
3501.811152	771923.689119	44.028135
3501.967062	771906.517590	44.033140
3501.904003	771882.435023	44.038145
3501.785225	771871.713757	44.043149
3502.014593	771852.115768	44.048154
3501.845582	771835.687378	44.053159
3501.875267	771812.229820	44.058164
3502.021257	771805.849916	44.063169
3501.455393	771780.174641	44.068173
3501.399226	771772.054263	44.073178
3501.404861	771779.493247	44.078183
3501.424483	771767.369453	44.083188
3502.125340	771740.746324	44.088193
3501.912034	771733.735748	44.093197
3501.969254	771707.021435	44.098202
3501.646104	771692.046980	44.103207
3501.568403	771685.260377	44.108212
3501.804204	771667.976593	44.113217
3501.621795	771652.289074	44.118221
3502.001312	771626.851714	44.123226
3501.925741	771630.855204	44.128231
3502.006011	771600.835509	44.133236
3502.261402	771573.102632	44.138241
3502.001647	771567.035718	44.143245
3501.760412	771541.059778	44.148250
3501.696964	771521.804782	44.153255
3501.527394	771522.522563	44.158260
3501.923996	771490.430145	44.163265
3501.814210	771480.101010	44.168269
3501.671605	771467.017993	44.173274
3501.674776	771466.130597	44.178279
3501.787626	771452.266383	44.183284
3501.990530	771436.909121	44.188289
3501.449907	771436.554752	44.193293
3501.562787	771387.115245	44.198298
3501.779681	771383.482602	44.203303
3501.732441	771384.328066	44.208308
3501.988612	771368.124241	44.213313
3501.607862	771338.721431	44.218317
3502.212685	771332.758276	44.223322
3502.035753	771299.971130	44.228327
3501.564868	771290.440319	44.233332
3501.744792	771281.541403	44.238337
3501.696796	771270.167043	44.243341
3501.830830	771247.675990	44.248346
3501.992213	771235.577249	44.253351
3501.691981	771228.580511	44.258356
3501.693393	771190.589694	44.263361
3501.627306	771184.786210	44.268365
3501.851205	771178.688582	44.273370
3501.768236	771158.696738	44.278375
3501.601531	771139.753406	44.283380
3502.098086	771128.978979	44.288385
3501.672768	771122.446220	44.293389
3501.819507	771102.219285	44.298394
3501.643275	771095.103444	44.303399
3501.816836	771078.567668	44.308404
3501.943883	771057.210521	44.313409
3501.749269	771053.497676	44.318413
3501.927302	771031.491475	44.323418
3501.886119	770998.384978	44.328423
3501.746492	770987.961520	44.333428
3501.996587	770979.986928	44.338433
3501.801190	770950.404214	44.343437
3501.627065	770935.206572	44.348442
3501.519874	770941.482352	44.353447
3501.802916	770913.249692	44.358452
3501.836998	770894.863977	44.363457
3501.812292	770900.682715	44.368461
3501.590209	770870.463483	44.373466
3501.634022	770863.409726	44.378471
3501.857492	770848.836289	44.383476
3501.773802	770839.388945	44.388481
3501.802315	770811.838426	44.393485
3501.804053	770794.541887	44.398490
3501.649779	770795.552879	44.403495
3501.611534	770777.228064	44.408500
3501.564272	770759.200354	44.413505
3501.207082	770759.949111	44.418509
3501.535237	770753.981795	44.423514
3501.760447	770748.179264	44.428519
3501.577863	770722.979231	44.433524
3502.013703	770703.147087	44.438529
3501.637370	770704.539615	44.443533
3501.517396	770686.178759	44.448538
3501.295889	770665.518513	44.453543
3501.430558	770666.186259	44.458548
3501.826069	770653.998727	44.463553
3501.657160	770655.997712	44.468557
3501.753199	770622.620543	44.473562
3501.853818	770621.421324	44.478567
3501.664899	770614.947729	44.483572
3501.769079	770592.706001	44.488577
3501.679376	770581.288175	44.493581
3501.796931	770564.859039	44.498586
3501.874095	770557.799498	44.503591
3501.783060	770533.076528	44.508596
3501.811784	770510.748425	44.513601
3501.345277	770501.757942	44.518605
3501.571688	770492.505471	44.523610
3501.770920	770471.627542	44.528615
3501.085143	770462.377452	44.533620
3501.694562	770457.595555	44.538625
3501.560501	770467.424282	44.543629
3501.745267	770439.452407	44.548634
3501.649712	770425.817724	44.553639
3501.395845	770413.441087	44.558644
3501.925203	770412.614730	44.563649
3501.558513	770386.359724	44.568653
3501.777402	770360.796649	44.573658
3501.813722	770361.184943	44.578663
3501.714877	770345.037367	44.583668
3501.910437	770314.402112	44.588673
3501.950115	770323.068961	44.593677
3501.771683	770300.380106	44.598682
3501.675748	770276.889102	44.603687
3501.943431	770262.800040	44.608692
3501.845861	770253.847044	44.613697
3501.738931	770228.435745	44.618701
3501.830089	770217.776064	44.623706
3501.921216	770213.030105	44.628711
3501.682510	770179.311835	44.633716
3501.732925	770164.864127	44.638721
3501.595977	770162.767620	44.643725
3501.679256	770132.100827	44.648730
3501.473586	770119.715760	44.653735
3501.485943	770114.687023	44.658740
3501.506615	770110.100450	44.663745
3501.368857	770115.100636	44.668749
3501.639538	770087.014720	44.673754
3501.632339	770075.434679	44.678759
3501.359135	770076.711767	44.683764
3501.422751	770066.056405	44.688769
3501.384085	770066.949887	44.693773
3501.563731	770036.956776	44.698778
3501.673769	770020.182699	44.703783
3501.629512	770014.226855	44.708788
3501.984502	770007.367440	44.713793
3501.347617	769982.387572	44.718797
3501.348009	769975.931517	44.723802
3501.772685	769959.647584	44.728807
3501.131691	769969.905450	44.733812
3501.596654	769953.861282	44.738817
3501.424621	769931.909488	44.743821
3501.544726	769915.527780	44.748826
3501.695291	769916.882940	44.753831
3501.700555	769906.631226	44.758836
3501.402914	769890.170424	44.763841
3501.305447	769888.560168	44.768845
3501.670984	769880.713235	44.773850
3501.613739	769883.679698	44.778855
3501.496554	769881.629139	44.783860
3501.798469	769859.352645	44.788865
3501.499569	769847.081046	44.793869
3501.907141	769824.442059	44.798874
3501.618235	769824.736102	44.803879
3501.559144	769799.857577	44.808884
3501.738757	769782.627949	44.813889
3501.457887	769776.612322	44.818893
3501.412239	769773.416417	44.823898
3501.478107	769768.477200	44.828903
3501.383830	769745.082809	44.833908
3501.510792	769732.001607	44.838913
3501.639357	769727.249173	44.843917
3501.579621	769720.950654	44.848922
3501.144627	769697.464383	44.853927
3501.336354	769690.237294	44.858932
3501.462679	769677.796802	44.863937
3501.308799	769675.604376	44.868941
3501.412520	769673.615940	44.873946
3501.486473	769677.940844	44.878951
3501.217469	769680.350854	44.883956
3501.115964	769663.019401	44.888961
3501.130950	769653.357153	44.893965
3501.662826	769631.436376	44.898970
3501.262640	769629.530933	44.903975
3501.224537	769627.615131	44.908980
3501.751019	769608.652274	44.913985
3501.393716	769631.086568	44.918989
3501.231578	769601.640851	44.923994
3501.382083	769587.766956	44.928999
3501.046347	769575.895258	44.934004
3501.214200	769575.177650	44.939009
3501.198404	769574.342437	44.944013
3501.135283	769567.305065	44.949018
3501.178558	769570.846519	44.954023
3500.897087	769567.048661	44.959028
3501.310756	769565.156997	44.964033
3500.979926	769573.885752	44.969037
3500.895838	769562.761145	44.974042
3501.339540	769571.756603	44.979047
3501.274278	769562.748165	44.984052
3501.231570	769544.667470	44.989057
3500.780598	769532.026114	44.994061
3501.230066	769518.595701	44.999066
3501.153794	769520.727585	45.004071
3501.123122	769521.570530	45.009076
3501.198166	769504.357483	45.014081
3501.044201	769510.445030	45.019085
3500.663162	769511.148546	45.024090
3501.223505	769513.569854	45.029095
3501.076927	769510.094747	45.034100
3501.082980	769519.507359	45.039105
3501.080748	769510.833476	45.044109
3501.040240	769514.191614	45.049114
3501.275126	769509.372242	45.054119
3501.289625	769510.552748	45.059124
3501.601204	769508.185029	45.064129
3501.617237	769487.482373	45.069133
3501.168875	769471.538328	45.074138
3501.316096	769468.507666	45.079143
3501.208032	769460.787592	45.084148
3501.535126	769466.204501	45.089153
3501.204952	769468.723226	45.094157
3501.298459	769455.154189	45.099162
3501.292545	769442.932231	45.104167
3501.077473	769424.583919	45.109172
3501.370888	769418.769121	45.114177
3501.658684	769417.883883	45.119181
3501.282827	769413.017193	45.124186
3501.328216	769413.354757	45.129191
3501.375118	769404.229078	45.134196
3501.508085	769390.850570	45.139201
3501.256700	769379.605387	45.144205
3501.429862	769365.628773	45.149210
3501.438270	769361.043758	45.154215
3501.362228	769378.799526	45.159220
3501.409362	769358.239247	45.164225
3501.345413	769355.391184	45.169229
3501.222250	769334.366023	45.174234
3501.429664	769326.840278	45.179239
3501.368747	769324.287426	45.184244
3501.334466	769313.647112	45.189249
3501.055848	769317.586719	45.194253
3501.293308	769316.364751	45.199258
3501.408319	769321.718127	45.204263
3501.463426	769305.050060	45.209268
3501.577914	769280.880513	45.214273
3501.688131	769281.108830	45.219277
3501.711753	769274.007605	45.224282
3501.548844	769262.353372	45.229287
3501.122799	769249.756715	45.234292
3501.495383	769231.557564	45.239297
3501.305148	769238.489196	45.244301
3501.411572	769215.454379	45.249306
3501.491398	769223.918746	45.254311
3501.352130	769221.428052	45.259316
3501.485227	769197.748047	45.264321
3501.225452	769192.369211	45.269325
3501.316570	769191.220616	45.274330
3501.176162	769184.589916	45.279335
3501.498900	769175.418520	45.284340
3501.474104	769167.684425	45.289345
3501.246947	769156.237761	45.294349
3501.277841	769141.051958	45.299354
3501.285511	769131.390237	45.304359
3501.241017	769127.750270	45.309364
3501.195250	769132.883825	45.314369
3501.040784	769135.817311	45.319373
3501.266018	769123.458178	45.324378
3501.115690	769129.249707	45.329383
3501.174977	769132.000120	45.334388
3501.251154	769132.628355	45.339393
3501.443331	769129.935169	45.344397
3501.521712	769106.362462	45.349402
3501.443893	769097.799125	45.354407
3501.359891	769086.870946	45.359412
3501.150421	769079.265756	45.364417
3501.349350	769093.723861	45.369421
3501.112404	769090.263442	45.374426
3501.478315	769078.916121	45.379431
3501.349346	769069.621848	45.384436
3501.699954	769038.758648	45.389441
3501.329785	769054.937103	45.394445
3501.201710	769041.354523	45.399450
3501.439452	769035.795044	45.404455
3501.513489	769040.317461	45.409460
3501.640474	769004.709934	45.414465
3501.354469	769003.869878	45.419469
3501.273651	768994.961892	45.424474
3501.530191	769000.686501	45.429479
3501.013049	769002.250395	45.434484
3501.581098	768985.497120	45.439489
3501.804748	768963.477288	45.444493
3501.667245	768944.622120	45.449498
3501.569605	768945.229713	45.454503
3501.357705	768943.588810	45.459508
3501.854971	768924.234714	45.464513
3501.656960	768914.261565	45.469517
3502.004859	768909.669640	45.474522
3501.721505	768887.535940	45.479527
3501.437467	768870.676316	45.484532
3501.587068	768852.956583	45.489537
3501.513755	768859.080665	45.494541
3501.433879	768842.877410	45.499546
3501.665283	768817.257685	45.504551
3501.677369	768812.967470	45.509556
3501.742775	768813.942539	45.514561
3501.558998	768793.813061	45.519565
3501.591174	768762.015359	45.524570
3501.421198	768764.655801	45.529575
3501.526300	768761.878245	45.534580
3501.285832	768757.235273	45.539585
3501.556914	768759.507320	45.544589
3501.398172	768733.064339	45.549594
3501.565622	768723.178606	45.554599
3501.798485	768726.639942	45.559604
3501.705070	768711.720195	45.564609
3501.394116	768688.703210	45.569613
3501.295347	768673.094191	45.574618
3501.521856	768663.691564	45.579623
3501.459405	768670.306926	45.584628
3501.808695	768652.849572	45.589633
3501.331186	768627.937469	45.594637
3501.349051	768610.978234	45.599642
3501.592103	768608.128606	45.604647
3501.413411	768617.129165	45.609652
3501.469981	768606.719334	45.614657
3501.220021	768592.663095	45.619661
3501.460822	768568.125387	45.624666
3501.718942	768570.153169	45.629671
3501.484018	768576.994191	45.634676
3501.521760	768572.946071	45.639681
3501.526781	768555.890243	45.644685
3501.632703	768526.445408	45.649690
3501.716992	768512.826882	45.654695
3501.454502	768520.362590	45.659700
3501.534061	768514.237272	45.664705
3501.358511	768492.725439	45.669709
3501.180706	768466.481821	45.674714
3501.358228	768470.346735	45.679719
3501.561873	768467.552838	45.684724
3501.626780	768465.373305	45.689729
3501.417341	768450.225683	45.694733
3501.639704	768431.457815	45.699738
3501.839007	768423.833912	45.704743
3501.663260	768431.306128	45.709748
3501.480268	768407.379923	45.714753
3501.470281	768396.438538	45.719757
3501.714975	768382.300421	45.724762
3502.027739	768379.439224	45.729767
3501.469489	768361.144816	45.734772
3501.957511	768358.402623	45.739777
3501.656134	768339.129274	45.744781
3501.630487	768333.661954	45.749786
3501.876772	768303.749477	45.754791
3501.490253	768297.109230	45.759796
3501.612159	768280.279987	45.764801
3501.414491	768287.065844	45.769805
3501.524400	768260.379756	45.774810
3501.768419	768233.572895	45.779815
3501.650205	768158.763433	45.784820
3501.565323	768033.124218	45.789825
3501.851335	767855.660443	45.794829
3501.488251	767619.240295	45.799834
3501.007686	767319.284281	45.804839
3500.935221	766972.411756	45.809844
3500.866427	766564.236418	45.814849
3500.249016	766100.361765	45.819853
3500.115701	765581.988081	45.824858
3499.957614	765002.382419	45.829863
3499.429987	764371.845942	45.834868
3499.467453	763672.948504	45.839873
3499.097502	762924.773797	45.844877
3498.749236	762121.908490	45.849882
3498.446705	761252.687132	45.854887
3497.933135	760321.866605	45.859892
3497.256284	759320.977341	45.864897
3496.765483	758286.904588	45.869901
3496.262165	757171.091507	45.874906
3496.003274	756004.368560	45.879911
3495.131929	754779.644424	45.884916
3494.609132	753496.190309	45.889921
3494.052372	752157.300885	45.894925
3493.332763	750745.429661	45.899930
3492.758556	749272.001028	45.904935
3491.757218	747747.949207	45.909940
3491.183649	746142.899031	45.914945
3489.993511	744499.844808	45.919949
3489.289959	742792.270869	45.924954
3488.636712	741018.279565	45.929959
3487.836996	739189.537818	45.934964
3486.950666	737295.210731	45.939969
3486.041245	735350.193536	45.944973
3485.115874	733344.646353	45.949978
3484.107166	731272.148475	45.954983
3482.687795	729153.017380	45.959988
3481.752852	726951.739550	45.964993
3480.423585	724707.605671	45.969997
3479.369703	722413.383604	45.975002
3478.574950	720050.836388	45.980007
3476.994135	717649.501226	45.985012
3475.954501	715187.047228	45.990017
3474.770811	712663.488740	45.995021
3473.449605	710078.377819	46.000026
3472.464429	707449.516650	46.005031
3470.435463	704752.454047	46.010036
3469.375148	702009.812110	46.015041
3468.017119	699216.691675	46.020045
3466.638038	696351.769531	46.025050
3465.192606	693428.621686	46.030055
3464.025238	690483.868632	46.035060
3462.208321	687452.733686	46.040065
3460.672283	684386.776040	46.045069
3459.010571	681267.305349	46.050074
3457.617308	678096.154634	46.055079
3456.007865	674875.703080	46.060084
3454.620916	671590.926839	46.065089
3452.513611	668249.008096	46.070093
3451.021345	664872.033842	46.075098
3449.238246	661430.724555	46.080103
3447.281310	657944.929556	46.085108
3446.053725	654403.923987	46.090113
3443.910222	650819.126653	46.095117
3442.178271	647166.788420	46.100122
3440.379049	643495.988987	46.105127
3438.056407	639766.624937	46.110132
3436.620718	635974.110912	46.115137
3434.492505	632145.738860	46.120141
3432.149758	628281.056093	46.125146
3430.765630	624345.526560	46.130151
3428.670960	620359.663370	46.135156
3426.586227	616331.883834	46.140161
3424.344906	612257.874250	46.145165
3422.171355	608132.498175	46.150170
3420.271133	603961.808574	46.155175
3417.692304	599755.272228	46.160180
3416.164483	595487.822393	46.165185
3413.964045	591184.922720	46.170189
3411.391122	586831.980237	46.175194
3409.577542	582428.173475	46.180199
3406.860280	577995.123447	46.185204
3404.788042	573503.834565	46.190209
3402.169598	568980.943339	46.195213
3399.832104	564417.442417	46.200218
3397.754398	559798.155924	46.205223
3394.915957	555151.388486	46.210228
3392.559495	550440.690306	46.215233
3390.365224	545711.055382	46.220237
3387.399440	540924.159022	46.225242
3385.216826	536100.505225	46.230247
3382.646042	531241.693278	46.235252
3380.257234	526346.008834	46.240257
3377.608740	521403.316582	46.245261
3374.932616	516423.012479	46.250266
3372.265527	511401.953169	46.255271
3369.861761	506357.128921	46.260276
3367.014588	501251.142586	46.265281
3364.309285	496123.486181	46.270285
3361.607744	490953.804682	46.275290
3358.920934	485749.889563	46.280295
3355.918256	480502.890112	46.285300
3353.047510	475215.112716	46.290305
3350.362824	469909.957263	46.295309
3347.369837	464554.539377	46.300314
3344.690914	459180.739214	46.305319
3341.269773	453772.885921	46.310324
3338.687582	448334.333189	46.315329
3335.754001	442859.308646	46.320333
3332.704506	437349.918781	46.325338
3329.957867	431812.557286	46.330343
3326.696444	426246.620378	46.335348
3323.586549	420648.594479	46.340353
3320.588875	415015.562924	46.345357
3317.496528	409362.389244	46.350362
3314.269364	403678.519102	46.355367
3311.073685	397979.197591	46.360372
3308.129615	392246.864607	46.365377
3304.946552	386479.570256	46.370381
3301.452936	380700.413476	46.375386
3298.325072	374895.949844	46.380391
3295.026270	369063.557057	46.385396
3292.272832	363195.267932	46.390401
3288.421557	357318.224817	46.395405
3284.849400	351431.356646	46.400410
3281.944098	345489.632732	46.405415
3278.004631	339546.933307	46.410420
3274.947325	333579.782158	46.415425
3271.295709	327598.317430	46.420429
3267.777284	321595.110453	46.425434
3264.304562	315572.666627	46.430439
3260.681162	309549.296765	46.435444
3257.178610	303507.262189	46.440449
3253.792319	297450.407981	46.445453
3250.004214	291376.299275	46.450458
3246.802562	285282.049588	46.455463
3242.903991	279196.013502	46.460468
3239.543017	273082.235852	46.465473
3235.609692	266950.198357	46.470477
3232.144643	260810.583623	46.475482
3228.321424	254663.788022	46.480487
3224.315268	248519.109820	46.485492
3220.595979	242354.244330	46.490497
3217.279160	236185.198609	46.495501
3212.831311	230015.288086	46.500506
3209.281699	223824.475707	46.505511
3205.198798	217638.241151	46.510516
3201.408266	211428.447567	46.515521
3197.715493	205178.222191	46.520525
3193.215182	198997.896417	46.525530
3189.452662	192795.887239	46.530535
3185.091787	186613.113001	46.535540
3181.188920	180416.241230	46.540545
3177.039850	174230.133369	46.545549
3172.498403	168059.370986	46.550554
3168.388060	161885.821676	46.555559
3164.088077	155738.883797	46.560564
3159.877311	149581.199559	46.565569
3155.536772	143436.247168	46.570573
3150.966726	137310.678173	46.575578
3146.771577	131193.154635	46.580583
3141.634708	125094.796591	46.585588
3137.136392	119020.736840	46.590593
3132.584156	112972.946511	46.595597
3127.583586	106934.044456	46.600602
3122.710616	100936.483331	46.605607
3117.747790	94948.608144	46.610612
3112.379158	89003.025953	46.615617
3106.911152	83104.997817	46.620621
3100.744366	77258.404853	46.625626
3094.239243	71473.182762	46.630631
3084.281856	65830.377280	46.635636
3068.696015	60440.784680	46.640641
3052.447708	55224.692369	46.645645
3036.686888	50218.515698	46.650650
3021.798263	45443.786851	46.655655
3006.833584	40925.530291	46.660660
2992.880385	36659.603837	46.665665
2979.705037	32641.675347	46.670669
2967.360827	28882.012955	46.675674
2955.747242	25360.468899	46.680679
2944.168623	22089.414807	46.685684
2933.374755	19032.550611	46.690689
2923.366047	16179.088159	46.695693
2913.603306	13548.563763	46.700698
2904.697671	11087.295123	46.705703
2895.660216	8810.838579	46.710708
2887.120410	6689.611526	46.715713
2878.790557	4752.900086	46.720717
2870.465806	2975.115330	46.725722
2860.416427	1382.416599	46.730727
2837.776010	318.607406	46.735732
2788.491355	239.870300	46.740737
2756.385363	237.559490	46.745741
2746.169826	233.976420	46.750746
2751.429229	232.298247	46.755751
2762.835992	234.679850	46.760756
2774.475476	230.611192	46.765761
2781.911688	225.073205	46.770765
2785.025731	224.247282	46.775770
2784.146656	217.380195	46.780775
2780.806868	223.174626	46.785780
2777.394283	229.637545	46.790785
2773.697497	222.337795	46.795789
2770.401984	222.626320	46.800794
2767.648104	222.979456	46.805799
2764.407133	224.023704	46.810804
2762.061793	222.487535	46.815809
2759.566160	201.598968	46.820813
2756.262385	215.670053	46.825818
2753.664208	207.124753	46.830823
2750.560942	223.430186	46.835828
2747.415555	213.196465	46.840833
2744.477425	211.970353	46.845837
2740.827824	208.317800	46.850842
2737.818390	197.571933	46.855847
2734.649736	206.401148	46.860852
2731.499669	213.297223	46.865857
2728.834110	200.748778	46.870861
2725.064286	217.243136	46.875866
2721.872752	202.616521	46.880871
2718.017990	200.689230	46.885876
2714.567288	191.103067	46.890881
2711.919132	204.681976	46.895885
2708.634917	212.155926	46.900890
2705.327380	201.467904	46.905895
2701.975114	193.806153	46.910900
2698.803872	194.763356	46.915905
2695.157816	200.602979	46.920909
2691.559129	208.594062	46.925914
2688.603410	205.474337	46.930919
2685.058794	200.687085	46.935924
2681.721513	204.294144	46.940929
2678.856509	191.028309	46.945933
2674.458795	196.100287	46.950938
2671.469345	191.812874	46.955943
2667.871132	196.374179	46.960948
2664.463775	192.921076	46.965953
2661.486583	189.401192	46.970957
2657.700186	194.126424	46.975962
2654.365139	186.428514	46.980967
2650.883062	195.003287	46.985972
2647.716764	197.142919	46.990977
2644.617678	190.905732	46.995981
2640.942770	187.760276	47.000986
2637.422849	196.522729	47.005991
2633.674765	189.811453	47.010996
2630.539633	192.503280	47.016001
2626.797015	185.082931	47.021005
2623.243348	192.787402	47.026010
2619.897069	186.453653	47.031015
2616.252085	182.152414	47.036020
2612.995610	191.271597	47.041025
2609.777654	178.439702	47.046029
2606.242672	182.069223	47.051034
2603.534712	185.908476	47.056039
2600.180206	183.838677	47.061044
2595.952509	178.090204	47.066049
2592.673130	183.618215	47.071053
2589.011560	185.433847	47.076058
2585.616870	177.462660	47.081063
2581.910057	187.126812	47.086068
2579.030499	183.835343	47.091073
2575.328325	175.302683	47.096077
2571.589984	189.610213	47.101082
2568.593607	179.061189	47.106087
2564.866934	183.293377	47.111092
2560.859171	175.884431	47.116097
2557.620331	171.472054	47.121101
2554.631232	166.453281	47.126106
2551.069762	180.294683	47.131111
2547.290252	188.969641	47.136116
2543.759194	188.443600	47.141121
2540.737495	182.447456	47.146125
2536.960192	174.670112	47.151130
2533.420109	173.196068	47.156135
2530.080588	179.160620	47.161140
2526.340666	179.564757	47.166145
2523.184298	173.089544	47.171149
2519.919257	171.848371	47.176154
2516.197002	172.801205	47.181159
2512.993918	173.247350	47.186164
2509.010760	181.311557	47.191169
2506.252379	173.487757	47.196173
2502.458780	170.885237	47.201178
2498.648306	167.084622	47.206183
2495.521025	164.711419	47.211188
2491.850174	173.858218	47.216193
2488.320296	175.481992	47.221197
2484.842595	182.233465	47.226202
2481.519224	168.646236	47.231207
2477.607956	168.164575	47.236212
2474.276015	167.475502	47.241217
2470.854928	166.738187	47.246221
2467.144046	163.224347	47.251226
2463.783765	163.236190	47.256231
2460.136562	174.766357	47.261236
2456.987925	171.580681	47.266241
2453.542546	171.755538	47.271245
2450.270162	174.522059	47.276250
2446.631234	163.164401	47.281255
2443.110237	166.820095	47.286260
2439.594546	173.206889	47.291265
2436.258564	163.385718	47.296269
2432.367576	166.236600	47.301274
2428.996213	168.273292	47.306279
2425.658865	180.816120	47.311284
2421.889562	170.244779	47.316289
2418.612264	160.206659	47.321293
2415.291049	167.621184	47.326298
2411.832413	168.610408	47.331303
2408.376111	166.039035	47.336308
2404.431109	169.548015	47.341313
2401.421125	171.584515	47.346317
2397.987553	176.201749	47.351322
2394.358375	161.790692	47.356327
2390.710521	161.827302	47.361332
2386.851273	158.355830	47.366337
2383.806571	168.258428	47.371341
2380.312574	171.839748	47.376346
2376.786009	158.527913	47.381351
2373.253080	160.354689	47.386356
2370.091988	164.017061	47.391361
2366.462503	164.900897	47.396365
2362.510457	172.033131	47.401370
2359.118896	169.071069	47.406375
2355.639225	164.315712	47.411380
2352.313705	159.805458	47.416385
2349.034216	162.127645	47.421389
2345.389769	166.878631	47.426394
2341.660156	160.088520	47.431399
2338.165364	159.153475	47.436404
2334.653569	156.250129	47.441409
2331.688675	159.079046	47.446413
2328.294203	170.636045	47.451418
2324.283150	160.164824	47.456423
2320.713501	162.947470	47.461428
2317.191695	171.678274	47.466433
2314.015950	156.244278	47.471437
2310.205313	164.984536	47.476442
2306.944791	167.931479	47.481447
2303.431765	167.935929	47.486452
2300.012997	166.449291	47.491457
2296.339309	158.150859	47.496461
2292.865629	160.510524	47.501466
2289.323614	168.156658	47.506471
2285.897850	163.714963	47.511476
2282.391988	159.013096	47.516481
2279.013115	156.664714	47.521485
2275.304810	152.040245	47.526490
2271.816975	150.624406	47.531495
2268.518739	161.372822	47.536500
2264.924392	166.418462	47.541505
2261.600351	162.227959	47.546509
2257.930643	158.792484	47.551514
2254.595885	146.705421	47.556519
2250.886320	157.674308	47.561524
2247.298077	156.931123	47.566529
2244.158340	155.647110	47.571533
2240.365500	164.647980	47.576538
2236.840656	166.034452	47.581543
2233.310861	159.098185	47.586548
2229.739234	154.811104	47.591553
2226.323667	148.463547	47.596557
2222.622204	153.887961	47.601562
2219.457190	157.183334	47.606567
2216.227748	145.806928	47.611572
2212.219572	150.232895	47.616577
2209.571335	164.110426	47.621581
2205.645667	166.785212	47.626586
2202.114846	160.833549	47.631591
2198.418861	165.774434	47.636596
2194.805011	161.595953	47.641601
2191.396965	154.853620	47.646605
2187.771642	155.553743	47.651610
2184.519688	154.183787	47.656615
2180.893469	157.986783	47.661620
2177.451878	155.052500	47.666625
2174.389324	161.658753	47.671629
2170.552591	156.413946	47.676634
2166.935604	150.442087	47.681639
2163.190545	152.504225	47.686644
2159.926736	164.973824	47.691649
2156.629187	151.608175	47.696653
2153.081800	155.568366	47.701658
2149.553339	142.174815	47.706663
2146.158602	148.439061	47.711668
2142.300612	157.891028	47.716673
2138.536865	154.593071	47.721677
2135.251691	152.981970	47.726682
2131.960636	144.857701	47.731687
2128.689614	155.329075	47.736692
2125.178370	151.966586	47.741697
2121.583843	153.011209	47.746701
2117.520785	147.716061	47.751706
2114.249798	140.536111	47.756711
2111.038227	143.808521	47.761716
2107.332925	159.817529	47.766721
2104.422824	147.969009	47.771725
2100.650286	153.122346	47.776730
2097.256762	139.216435	47.781735
2093.544513	144.875912	47.786740
2090.147460	142.929991	47.791745
2086.306187	152.861168	47.796749
2082.647619	149.440032	47.801754
2079.400342	138.337468	47.806759
2075.838550	137.452080	47.811764
2072.018473	140.426304	47.816769
2068.962007	146.064038	47.821773
2065.126684	149.811108	47.826778
2061.801021	142.922367	47.831783
2058.393723	144.894406	47.836788
2054.608703	146.140868	47.841793
2051.469213	138.980202	47.846797
2048.176255	141.473440	47.851802
2044.532058	137.318798	47.856807
2041.476887	141.430178	47.861812
2037.597678	146.451375	47.866817
2034.329448	137.846777	47.871821
2030.233825	143.363525	47.876826
2026.686657	142.804479	47.881831
2023.107253	140.124267	47.886836
2020.057093	136.782852	47.891841
2016.944111	138.645878	47.896845
2012.731574	145.696035	47.901850
2009.069997	133.369532	47.906855
2005.919031	133.840640	47.911860
2002.376415	133.633757	47.916865
1999.106191	128.304087	47.921869
1995.430824	132.287922	47.926874
1992.177751	136.840807	47.931879
1988.531172	149.102283	47.936884
1984.995211	143.235749	47.941889
1981.560811	138.719378	47.946893
1977.907752	139.956441	47.951898
1974.331108	140.897749	47.956903
1971.150471	129.672183	47.961908
1967.368651	134.641924	47.966913
1963.868758	137.030820	47.971917
1960.478638	138.585702	47.976922
1956.847708	129.628299	47.981927
1953.545388	125.844598	47.986932
1949.701985	139.590408	47.991937
1946.733908	138.454807	47.996941
1943.024461	136.671685	48.001946
1939.505172	132.641522	48.006951
1935.985241	136.178075	48.011956
1932.444050	122.939599	48.016961
1929.013613	133.795456	48.021965
1925.351767	128.507544	48.026970
1922.453934	124.695209	48.031975
1918.492449	134.260326	48.036980
1914.451417	139.233593	48.041985
1911.195710	135.908973	48.046989
1907.750679	132.491774	48.051994
1904.550471	127.344760	48.056999
1901.092918	127.175097	48.062004
1897.112922	138.294979	48.067009
1894.241565	130.791619	48.072013
1890.565378	135.082959	48.077018
1886.851292	135.744597	48.082023
1883.210396	128.290562	48.087028
1880.008702	133.991389	48.092033
1876.914401	127.584216	48.097037
1872.571058	130.252306	48.102042
1869.107777	134.650991	48.107047
1865.866562	133.368499	48.112052
1862.294661	123.983796	48.117057
1859.083985	128.746095	48.122061
1855.386286	131.744531	48.127066
1851.852224	129.153120	48.132071
1848.830541	133.296141	48.137076
1844.838202	133.715923	48.142081
1840.984914	133.417718	48.147085
1837.631467	132.798193	48.152090
1834.607865	134.971527	48.157095
1831.187503	129.740016	48.162100
1827.675608	140.642009	48.167105
1824.219265	127.573893	48.172109
1820.551039	139.195347	48.177114
1816.995652	127.577773	48.182119
1813.642311	131.419470	48.187124
1809.907855	128.769887	48.192129
1806.173619	119.217155	48.197133
1802.587685	130.551848	48.202138
1799.027306	131.021437	48.207143
1795.790765	115.582334	48.212148
1792.364394	131.324403	48.217153
1788.919021	139.872301	48.222157
1785.338193	141.449948	48.227162
1781.673545	133.867291	48.232167
1778.477926	130.347542	48.237172
1775.163893	126.011502	48.242177
1771.659671	125.728844	48.247181
1767.859263	130.344504	48.252186
1764.335771	141.113865	48.257191
1760.785435	130.249338	48.262196
1757.180215	127.678696	48.267201
1753.399772	121.912327	48.272205
1750.232442	144.657549	48.277210
1747.229784	133.059112	48.282215
1743.522376	139.987577	48.287220
1739.912446	136.541832	48.292225
1736.298722	136.619307	48.297229
1732.797328	126.435852	48.302234
1729.278443	125.868638	48.307239
1725.804566	120.495563	48.312244
1722.231020	133.392173	48.317249
1719.384636	124.841568	48.322253
1715.300805	134.022762	48.327258
1711.540284	126.134937	48.332263
1708.209889	120.846424	48.337268
1704.640297	124.901139	48.342273
1701.370204	124.639077	48.347277
1697.748820	121.237079	48.352282
1694.603539	128.475824	48.357287
1690.834904	122.511706	48.362292
1687.129314	124.180034	48.367297
1684.025171	120.885077	48.372301
1679.974161	115.281001	48.377306
1676.668332	123.161572	48.382311
1673.717127	120.147124	48.387316
1669.760604	134.882993	48.392321
1666.633844	121.561107	48.397325
1662.978605	130.597507	48.402330
1659.228193	120.243275	48.407335
1655.689617	123.849228	48.412340
1652.013801	124.723396	48.417345
1648.591486	120.029206	48.422349
1645.169126	113.007389	48.427354
1641.936593	123.388499	48.432359
1638.472753	114.787997	48.437364
1634.440938	123.990632	48.442369
1631.226438	120.298362	48.447373
1627.693730	126.634313	48.452378
1624.275573	131.391383	48.457383
1620.919395	116.368835	48.462388
1617.436884	115.673635	48.467393
1613.749519	118.096981	48.472397
1610.202814	121.782433	48.477402
1606.724116	119.408140	48.482407
1603.473706	106.916395	48.487412
1599.700076	118.508157	48.492417
1596.317719	118.831263	48.497421
1592.633334	120.536588	48.502426
1589.090830	127.743053	48.507431
1585.438747	120.796568	48.512436
1581.839049	127.750833	48.517441
1578.881325	109.230745	48.522445
1575.203300	125.093232	48.527450
1571.719554	113.540557	48.532455
1568.178856	114.697223	48.537460
1564.405219	124.612511	48.542465
1561.314524	124.037760	48.547469
1557.658672	128.891799	48.552474
1554.140315	112.707726	48.557479
1550.655304	123.966463	48.562484
1546.926721	116.127046	48.567489
1544.037506	115.733732	48.572493
1540.335327	123.032964	48.577498
1536.448064	115.785347	48.582503
1532.811161	119.081420	48.587508
1529.398152	117.662582	48.592513
1526.812530	110.414444	48.597517
1523.277906	109.992295	48.602522
1519.542272	112.981070	48.607527
1515.624530	107.006846	48.612532
1511.789848	125.532332	48.617537
1508.625575	112.615415	48.622541
1504.879046	122.927297	48.627546
1501.334473	109.612220	48.632551
1498.496394	115.764423	48.637556
1494.518679	121.755663	48.642561
1490.952299	119.761922	48.647565
1487.812974	125.730919	48.652570
1484.258661	121.980065	48.657575
1480.873028	117.718742	48.662580
1477.222176	116.854376	48.667585
1473.901377	112.329300	48.672589
1470.252182	118.334602	48.677594
1466.703528	132.430625	48.682599
1463.052680	122.593626	48.687604
1459.191865	140.782205	48.692609
1455.899140	109.666281	48.697613
1452.421502	121.424229	48.702618
1448.681999	116.611425	48.707623
1445.867468	107.328304	48.712628
1441.806254	111.391467	48.717633
1438.669000	116.019971	48.722637
1434.820770	111.842029	48.727642
1431.914722	108.845989	48.732647
1428.438870	110.168027	48.737652
1424.810816	126.468254	48.742657
1421.034151	116.713811	48.747661
1417.797732	111.880838	48.752666
1414.315952	122.282151	48.757671
1410.548985	118.747376	48.762676
1406.691884	120.578580	48.767681
1403.836610	119.308376	48.772685
1400.337205	118.252125	48.777690
1396.231197	116.621672	48.782695
1392.796570	114.965450	48.787700
1389.306370	120.705599	48.792705
1385.976096	123.468302	48.797709
1382.431675	121.804359	48.802714
1378.491922	119.454687	48.807719
1375.634196	115.275879	48.812724
1372.181707	112.843714	48.817729
1368.777949	118.476766	48.822733
1365.301573	121.423814	48.827738
1361.501054	119.605527	48.832743
1358.006671	111.887596	48.837748
1354.422651	116.999108	48.842753
1351.262704	126.133245	48.847757
1347.714411	117.249200	48.852762
1343.910238	133.190511	48.857767
1340.463006	120.678815	48.862772
1336.729438	113.751061	48.867777
1333.804283	121.820605	48.872781
1330.243661	124.919795	48.877786
1326.494646	120.837613	48.882791
1323.179405	111.128719	48.887796
1319.290138	126.987098	48.892801
1316.365906	108.067706	48.897805
1312.705020	118.223464	48.902810
1308.881786	117.114557	48.907815
1305.643652	118.633602	48.912820
1301.611916	120.412690	48.917825
1298.424956	112.869875	48.922829
1294.845695	117.499871	48.927834
1291.620845	117.916401	48.932839
1288.015983	117.530729	48.937844
1284.267124	123.407049	48.942849
1280.590508	117.925719	48.947853
1277.026637	113.679425	48.952858
1274.067227	114.113709	48.957863
1271.294459	116.120273	48.962868
1266.892363	116.655670	48.967873
1263.434657	111.858615	48.972877
1259.658548	114.845619	48.977882
1256.045448	119.421926	48.982887
1252.829672	121.296912	48.987892
1249.364944	112.141837	48.992897
1246.075654	119.916844	48.997901
1242.425757	103.746419	49.002906
1238.945714	111.522133	49.007911
1235.684844	109.612568	49.012916
1231.708697	118.393025	49.017921
1228.445861	106.496687	49.022925
1225.213160	106.198783	49.027930
1221.459452	112.293569	49.032935
1217.890588	106.590470	49.037940
1214.357801	116.500183	49.042945
1211.129195	106.697143	49.047949
1207.490576	120.620946	49.052954
1203.870653	123.028630	49.057959
1200.587219	109.572378	49.062964
1196.799120	110.291384	49.067969
1193.141841	100.760879	49.072973
1189.719286	106.873327	49.077978
1186.191357	117.182601	49.082983
1182.558819	112.559183	49.087988
1178.886729	115.485451	49.092993
1176.047957	105.956373	49.097997
1172.437643	116.458020	49.103002
1168.888109	109.944738	49.108007
1165.634139	111.108137	49.113012
1161.816405	116.299856	49.118017
1158.168201	114.348907	49.123021
1154.491747	108.929881	49.128026
1151.135586	101.135786	49.133031
1148.095833	107.900520	49.138036
1144.379129	110.500806	49.143041
1141.026198	103.885237	49.148045
1137.127308	112.803140	49.153050
1133.637253	118.844381	49.158055
1130.606378	106.839167	49.163060
1126.714424	121.166405	49.168065
1123.222105	102.707835	49.173069
1120.085696	105.645338	49.178074
1116.508711	109.916914	49.183079
1113.019915	107.452602	49.188084
1109.167223	112.467602	49.193089
1105.685584	112.217463	49.198093
1102.238068	114.767806	49.203098
1098.431261	113.037528	49.208103
1095.628559	110.685879	49.213108
1091.684980	106.853502	49.218113
1088.555223	95.273779	49.223117
1084.557458	99.979771	49.228122
1080.982752	109.439770	49.233127
1077.882687	108.995238	49.238132
1073.988591	106.522487	49.243137
1070.749968	107.640973	49.248141
1066.978242	103.529551	49.253146
1063.904085	107.040754	49.258151
1060.673175	99.964581	49.263156
1056.601835	111.236838	49.268161
1053.123621	96.958673	49.273165
1049.633571	103.766019	49.278170
1046.045769	97.738707	49.283175
1042.850962	93.407151	49.288180
1039.160362	106.200296	49.293185
1035.937667	101.488681	49.298189
1032.465196	103.995326	49.303194
1028.596830	107.379880	49.308199
1025.284157	98.311032	49.313204
1021.879356	111.361358	49.318209
1018.277192	110.157121	49.323213
1014.601329	107.983513	49.328218
1010.988503	118.992446	49.333223
1007.936452	104.136251	49.338228
1004.066093	109.920689	49.343233
1000.856510	98.034152	49.348237
997.326633	93.804213	49.353242
993.592915	102.987031	49.358247
990.486179	106.184290	49.363252
986.504501	110.123285	49.368257
983.064324	105.120161	49.373261
979.544771	114.337875	49.378266
975.598078	109.742476	49.383271
972.511469	103.935230	49.388276
969.372447	103.710181	49.393281
965.845379	101.964969	49.398285
962.384187	107.458015	49.403290
958.456385	116.035577	49.408295
955.308274	114.093327	49.413300
951.665574	112.426605	49.418305
948.338170	105.134877	49.423309
944.806734	103.119484	49.428314
941.129718	104.085676	49.433319
937.623527	102.356468	49.438324
934.007954	108.885169	49.443329
930.604329	110.029486	49.448333
927.136156	99.910613	49.453338
923.747794	96.247318	49.458343
920.335540	100.193348	49.463348
916.697988	107.066447	49.468353
912.924266	102.384815	49.473357
909.605001	103.121965	49.478362
905.848772	101.180512	49.483367
902.832465	95.717356	49.488372
899.481738	98.418839	49.493377
895.866001	105.117471	49.498381
891.732753	98.546939	49.503386
888.454607	97.535716	49.508391
885.172250	102.199058	49.513396
881.439210	105.828409	49.518401
878.156620	104.955551	49.523405
874.418783	98.936246	49.528410
871.295788	94.423724	49.533415
867.999217	99.000431	49.538420
864.309082	103.401998	49.543425
860.681542	102.655171	49.548429
857.003764	91.294239	49.553434
853.357104	117.025397	49.558439
850.186629	100.907696	49.563444
846.526906	106.431211	49.568449
842.514827	105.997397	49.573453
839.639277	111.004589	49.578458
835.846916	107.309494	49.583463
832.598610	102.102518	49.588468
828.940646	103.442987	49.593473
825.690740	93.167777	49.598477
822.585823	100.405008	49.603482
818.403828	104.987762	49.608487
815.035342	99.106788	49.613492
811.740384	101.742967	49.618497
808.055007	95.626644	49.623501
804.346735	104.137045	49.628506
800.644992	99.671889	49.633511
797.841312	104.640687	49.638516
793.901103	96.496435	49.643521
790.427181	93.320502	49.648525
786.758412	96.207943	49.653530
783.357913	95.401172	49.658535
780.039540	105.282062	49.663540
776.653212	111.873019	49.668545
773.027837	96.220587	49.673549
769.487586	98.570246	49.678554
765.825016	97.063777	49.683559
762.344104	99.091292	49.688564
758.847621	107.841895	49.693569
755.249473	105.152944	49.698573
751.707135	99.848559	49.703578
748.354550	101.314939	49.708583
745.282951	96.366514	49.713588
741.579060	97.079067	49.718593
737.614521	95.245121	49.723597
734.485915	98.502335	49.728602
730.724923	107.145688	49.733607
727.706014	94.252704	49.738612
724.266614	106.761601	49.743617
720.476900	98.099949	49.748621
716.790994	101.670399	49.753626
713.612909	103.780817	49.758631
710.152006	92.939802	49.763636
706.410917	106.653111	49.768641
702.758062	101.585630	49.773645
699.361881	106.356546	49.778650
695.590501	116.853130	49.783655
692.580840	97.608977	49.788660
688.931017	102.482362	49.793665
685.217198	98.945758	49.798669
681.749893	82.027380	49.803674
678.294367	99.870561	49.808679
675.096872	96.293577	49.813684
671.664974	109.751421	49.818689
667.923393	88.022255	49.823693
664.435250	98.726499	49.828698
661.185434	101.191621	49.833703
657.409881	89.350829	49.838708
653.504869	98.696167	49.843713
650.212009	98.834282	49.848717
646.945623	99.928055	49.853722
642.842073	91.337828	49.858727
639.981862	94.792462	49.863732
636.490038	94.329872	49.868737
633.121251	100.387019	49.873741
629.631567	95.294214	49.878746
625.813601	93.404066	49.883751
622.750227	87.798380	49.888756
618.766580	90.592791	49.893761
615.147345	90.379745	49.898765
611.703232	86.877666	49.903770
608.336191	90.868563	49.908775
604.788027	85.866135	49.913780
601.215501	95.969019	49.918785
597.411792	88.477962	49.923789
594.361897	92.180496	49.928794
590.830503	90.365963	49.933799
587.364425	86.490953	49.938804
583.627572	91.275765	49.943809
580.550249	87.473976	49.948813
577.033382	89.039003	49.953818
573.378341	92.425760	49.958823
570.397217	87.600505	49.963828
566.404464	84.922191	49.968833
562.796838	97.433475	49.973837
559.745117	88.520799	49.978842
555.506605	92.768234	49.983847
552.404801	77.722463	49.988852
548.555391	92.658908	49.993857
544.834984	97.802504	49.998861
541.163327	92.062828	50.003866
537.696603	86.855298	50.008871
534.925840	87.472929	50.013876
531.272557	87.482006	50.018881
527.811239	92.939852	50.023885
524.806485	103.054848	50.028890
521.136584	96.105656	50.033895
517.628225	96.069295	50.038900
514.043261	97.230752	50.043905
509.855785	97.830638	50.048909
506.350897	91.607346	50.053914
503.180926	99.652495	50.058919
499.654598	92.223711	50.063924
496.447735	95.113240	50.068929
492.635627	104.049181	50.073933
489.343890	93.751685	50.078938
485.391641	90.140344	50.083943
482.147017	84.617357	50.088948
478.664146	87.628945	50.093953
474.967474	84.382452	50.098957
471.573927	90.410018	50.103962
467.934118	97.001839	50.108967
464.561487	88.656031	50.113972
461.025077	88.125626	50.118977
457.905830	80.701746	50.123981
454.462919	84.827187	50.128986
450.938511	89.767973	50.133991
447.247203	84.582306	50.138996
443.098824	93.971895	50.144001
439.992102	87.890246	50.149005
436.774883	78.283411	50.154010
433.223138	87.797898	50.159015
429.787923	82.938123	50.164020
426.336794	93.343733	50.169025
422.962099	90.977273	50.174029
419.417509	84.014457	50.179034
415.362559	92.239475	50.184039
411.888882	84.512791	50.189044
408.078086	92.252045	50.194049
405.076190	87.488810	50.199053
401.753446	88.233594	50.204058
398.019340	90.386487	50.209063
394.695325	91.028488	50.214068
391.210964	90.543981	50.219073
387.794063	93.101256	50.224077
384.365618	94.719160	50.229082
380.307416	83.252507	50.234087
377.358905	91.984564	50.239092
373.698992	80.324655	50.244097
369.965794	89.069045	50.249101
366.670813	90.332238	50.254106
362.781596	95.725202	50.259111
359.408617	91.716948	50.264116
355.710253	98.006053	50.269121
352.652484	94.313222	50.274125
349.530875	94.130187	50.279130
345.692582	94.213146	50.284135
342.292004	79.500802	50.289140
338.386500	91.568008	50.294145
334.811743	94.657005	50.299149
331.148210	89.241291	50.304154
328.100556	97.411819	50.309159
324.846533	86.733107	50.314164
321.093053	91.100035	50.319169
317.427031	93.100449	50.324173
314.124236	96.891256	50.329178
310.667265	98.310678	50.334183
307.178335	86.606580	50.339188
303.421982	90.170238	50.344193
300.131732	90.063234	50.349197
296.528999	83.103294	50.354202
292.623295	84.296947	50.359207
289.307583	87.633217	50.364212
285.967775	94.678512	50.369217
282.665370	88.910253	50.374221
279.368939	80.896383	50.379226
275.635925	82.612116	50.384231
271.942378	77.351657	50.389236
268.252219	76.981625	50.394241
264.643483	88.773318	50.399245
261.767027	83.994662	50.404250
257.552154	93.389221	50.409255
254.673716	80.940070	50.414260
251.064998	91.546609	50.419265
247.404734	85.851212	50.424269
244.496466	78.627990	50.429274
240.426487	87.550321	50.434279
236.902466	86.518891	50.439284
233.094609	98.646577	50.444289
229.750830	86.253999	50.449293
226.652429	90.751490	50.454298
223.134560	84.666073	50.459303
219.815092	79.800025	50.464308
216.314890	88.349917	50.469313
212.144557	95.514023	50.474317
208.993674	86.478728	50.479322
205.468820	92.814316	50.484327
202.113947	83.380125	50.489332
197.936342	78.472281	50.494337
194.808665	84.161949	50.499341
191.525184	85.311750	50.504346
187.899186	93.185536	50.509351
184.322350	86.380519	50.514356
180.981990	84.646235	50.519361
177.562336	84.095414	50.524365
174.253250	76.991831	50.529370
170.052921	85.861351	50.534375
166.640649	86.590762	50.539380
163.447327	94.958860	50.544385
159.640177	84.274178	50.549389
156.460178	79.359174	50.554394
152.545857	77.149711	50.559399
149.443061	79.928678	50.564404
146.130746	87.177556	50.569409
142.623630	88.420470	50.574413
139.055230	91.360436	50.579418
135.272006	86.431565	50.584423
132.221130	83.785935	50.589428
128.484497	90.507869	50.594433
124.834661	85.185918	50.599437
121.610875	84.755383	50.604442
117.586828	90.490011	50.609447
114.206624	84.452749	50.614452
110.695896	87.394150	50.619457
107.082234	90.706541	50.624461
103.891205	99.868668	50.629466
100.153709	101.198017	50.634471
97.021185	86.679203	50.639476
93.297878	93.860271	50.644481
89.715887	84.529780	50.649485
86.163724	86.907316	50.654490
82.798802	91.216972	50.659495
79.849895	90.241341	50.664500
76.090461	89.257092	50.669505
72.030191	82.628227	50.674509
68.713458	85.171578	50.679514
65.233836	90.595082	50.684519
61.632617	85.791863	50.689524
58.059383	92.609560	50.694529
54.832818	86.857908	50.699533
51.279202	84.585448	50.704538
47.841901	79.061006	50.709543
44.453609	83.270262	50.714548
40.861906	72.383539	50.719553
37.094163	93.930578	50.724557
33.897029	84.702661	50.729562
30.419245	83.974278	50.734567
26.720869	76.675158	50.739572
23.232557	87.660768	50.744577
19.532329	83.088909	50.749581
16.559280	79.886784	50.754586
12.645930	78.615667	50.759591
9.326020	88.077334	50.764596
5.525919	94.358077	50.769601
2.285569	94.451737	50.774605