Thu Jun 16 18:13:27 2022

Number of Points = 9932

Depth (nm)	Load (N)	Time (s)
-0.843518	100.768969	0.000000
-1.485790	102.953435	0.005005
-1.217198	82.503864	0.010010
-1.524293	78.757779	0.015014
-1.675623	80.395258	0.020019
-1.492438	51.914057	0.025024
-2.639792	55.032299	0.030029
-2.438754	46.373543	0.035034
-2.504906	43.635570	0.040038
-2.761449	47.801220	0.045043
-3.196480	21.706712	0.050048
-3.732484	25.516814	0.055053
-4.229143	12.764729	0.060058
-3.911211	7.153976	0.065062
-4.640281	9.175096	0.070067
-4.380697	-6.880823	0.075072
-4.378936	0.045124	0.080077
-5.433287	-11.446697	0.085082
-5.918265	-16.380276	0.090086
-6.019554	-15.304237	0.095091
-5.916962	-12.239555	0.100096
-5.876502	-2.088153	0.105101
-6.212671	-7.048398	0.110106
-6.555215	-8.406569	0.115110
-6.598023	-13.030636	0.120115
-7.608263	-30.115004	0.125120
-8.653433	-7.336961	0.130125
-8.787919	-9.528130	0.135130
-8.011875	-9.354651	0.140134
-8.393377	-5.886181	0.145139
-8.279714	-13.860199	0.150144
-8.477556	-15.079402	0.155149
-9.011377	-17.101187	0.160154
-10.020390	-16.888231	0.165158
-9.906522	-14.014141	0.170163
-9.991228	-16.377205	0.175168
-10.297168	-15.150735	0.180173
-10.368317	-16.371440	0.185178
-10.305514	-16.798896	0.190182
-11.383419	-24.749526	0.195187
-11.281895	-30.914066	0.200192
-11.721505	-19.426177	0.205197
-11.856397	-12.389158	0.210202
-11.635428	-12.681648	0.215206
-12.017590	-6.924561	0.220211
-11.988025	-20.764339	0.225216
-12.811547	-16.514972	0.230221
-13.133557	-18.991537	0.235226
-13.591886	-17.077513	0.240230
-13.725863	-3.773069	0.245235
-13.828873	-16.341964	0.250240
-14.004035	-18.435548	0.255245
-13.695014	-19.819609	0.260250
-14.354972	-12.444642	0.265254
-14.906527	-9.888453	0.270259
-14.851748	-22.711313	0.275264
-15.333191	-22.117620	0.280269
-15.281861	-16.323160	0.285274
-15.701950	-12.396276	0.290278
-16.759345	-12.151252	0.295283
-16.711345	-19.167521	0.300288
-16.678456	-16.361637	0.305293
-16.968709	-16.885044	0.310298
-16.850855	-15.913096	0.315302
-17.054444	-10.321961	0.320307
-16.906962	-8.645576	0.325312
-17.408598	-26.231211	0.330317
-17.430827	-16.754522	0.335322
-17.826476	-12.225045	0.340326
-18.467709	-7.690103	0.345331
-18.618933	-22.451138	0.350336
-19.317933	-20.298747	0.355341
-19.369391	-18.507504	0.360346
-19.509053	-15.394601	0.365350
-19.793515	-8.742184	0.370355
-19.694421	-18.246599	0.375360
-20.156168	-20.692277	0.380365
-20.624754	-19.468920	0.385370
-20.986186	-17.352189	0.390374
-21.739999	-8.337450	0.395379
-21.603191	-15.364352	0.400384
-21.701361	-18.997744	0.405389
-21.850025	-17.546287	0.410394
-21.364017	-14.507184	0.415398
-21.834934	-5.920991	0.420403
-22.518311	-14.665492	0.425408
-22.819762	-17.018386	0.430413
-23.252800	-24.370002	0.435418
-23.103020	-20.125410	0.440422
-23.225526	-17.175657	0.445427
-23.261958	-18.699643	0.450432
-24.056569	-17.360254	0.455437
-24.441004	-16.089045	0.460442
-24.452403	-18.238697	0.465446
-25.017609	-15.989734	0.470451
-24.723722	-15.836217	0.475456
-25.365098	-21.566435	0.480461
-25.923602	-18.945564	0.485466
-26.247115	-14.005764	0.490470
-26.442889	-14.818651	0.495475
-26.829315	-22.318949	0.500480
-26.581655	-11.431300	0.505485
-26.292504	-13.671267	0.510490
-26.256416	-17.308596	0.515494
-26.679955	-12.257162	0.520499
-27.347358	-14.887078	0.525504
-27.814252	-3.762654	0.530509
-27.854562	-13.118939	0.535514
-27.959680	-24.074758	0.540518
-28.706330	-14.707034	0.545523
-29.141278	-22.647306	0.550528
-29.905092	-8.308067	0.555533
-29.712930	-7.074333	0.560538
-29.544797	-12.154024	0.565542
-29.683536	-10.106947	0.570547
-29.774671	-15.785443	0.575552
-30.184059	-6.654482	0.580557
-29.753840	-16.046202	0.585562
-30.568541	-11.639948	0.590566
-31.101689	-9.790114	0.595571
-31.089731	-18.953479	0.600576
-31.283070	-11.970435	0.605581
-31.718690	-17.925949	0.610586
-32.327625	-12.191173	0.615590
-32.672706	-9.304869	0.620595
-32.224135	-11.123485	0.625600
-32.687812	-9.316207	0.630605
-32.643481	-12.374412	0.635610
-33.377849	-19.033491	0.640614
-34.295350	-11.234363	0.645619
-34.331777	-11.487670	0.650624
-33.790645	-15.510053	0.655629
-33.993711	-7.811135	0.660634
-34.210105	-13.074804	0.665638
-34.631371	-8.566249	0.670643
-34.867718	-8.783853	0.675648
-35.625386	-6.585952	0.680653
-35.666189	-10.091202	0.685658
-35.920212	-17.637257	0.690662
-36.334419	-18.080590	0.695667
-36.131748	-22.259441	0.700672
-36.306750	-9.256523	0.705677
-36.525501	-10.625580	0.710682
-37.124020	-17.457954	0.715686
-37.730085	-17.954917	0.720691
-37.403244	-18.669292	0.725696
-37.529910	-5.573828	0.730701
-38.093821	-9.685387	0.735706
-38.051513	-18.286894	0.740710
-38.686285	-13.221960	0.745715
-39.317640	-25.125211	0.750720
-39.513730	-15.234048	0.755725
-39.612092	-8.997636	0.760730
-39.481749	-3.062132	0.765734
-39.882618	-9.991595	0.770739
-39.613272	-12.863630	0.775744
-39.866432	-14.693442	0.780749
-40.074111	-13.384160	0.785754
-40.797297	-8.243841	0.790758
-41.226316	-9.498830	0.795763
-40.934679	-26.063657	0.800768
-41.433201	-14.461455	0.805773
-42.404308	-8.900439	0.810778
-42.804020	-10.878482	0.815782
-42.701532	-3.547729	0.820787
-42.071391	-21.966990	0.825792
-42.309490	-19.513312	0.830797
-42.631703	-26.377335	0.835802
-43.260753	-18.797244	0.840806
-43.876452	-13.590241	0.845811
-43.777233	-14.697531	0.850816
-44.062343	-11.146533	0.855821
-44.308867	-18.876535	0.860826
-43.947607	-23.941276	0.865830
-44.526102	-19.947766	0.870835
-45.300123	-17.134217	0.875840
-45.614257	-12.959757	0.880845
-45.645578	-15.526486	0.885850
-45.537432	-21.871181	0.890854
-45.659584	-18.795307	0.895859
-46.493808	-25.176245	0.900864
-47.205399	-17.477642	0.905869
-47.251017	-15.915751	0.910874
-47.528596	-17.071658	0.915878
-47.517182	-16.484930	0.920883
-47.135062	-23.199873	0.925888
-47.631258	-7.761940	0.930893
-47.580015	-8.865840	0.935898
-47.678644	-22.300458	0.940902
-48.757171	-14.913933	0.945907
-48.971397	-14.507350	0.950912
-49.236464	-18.039661	0.955917
-49.205050	-19.066390	0.960922
-49.073951	-13.011840	0.965926
-50.098468	-17.312360	0.970931
-50.132423	-19.712123	0.975936
-50.265128	-13.074726	0.980941
-50.577285	-15.705635	0.985946
-50.354163	-15.830176	0.990950
-51.311191	-15.264234	0.995955
-51.324282	-25.367684	1.000960
-51.860292	-14.618179	1.005965
-52.317863	-8.910389	1.010970
-52.009343	-10.279867	1.015974
-52.353643	-8.515698	1.020979
-52.367294	-16.494026	1.025984
-52.437247	-17.586971	1.030989
-53.336151	-22.187147	1.035994
-53.532700	-22.095828	1.040998
-54.154942	-17.437944	1.046003
-53.665851	-27.182016	1.051008
-53.843962	-9.761200	1.056013
-53.921418	-14.467044	1.061018
-53.831243	-11.124275	1.066022
-55.014482	-15.886117	1.071027
-55.183571	-18.825784	1.076032
-55.349995	-27.398412	1.081037
-55.753342	-11.388140	1.086042
-55.615955	-18.695512	1.091046
-56.271542	-19.924796	1.096051
-56.527236	-13.414267	1.101056
-57.088487	-20.499334	1.106061
-57.260904	-12.656418	1.111066
-57.077156	-23.586376	1.116070
-57.190885	-11.263852	1.121075
-57.030022	-11.108182	1.126080
-57.454673	-3.296580	1.131085
-58.110187	-13.551259	1.136090
-58.404764	-14.107985	1.141094
-58.410923	-15.267510	1.146099
-58.315022	-18.692156	1.151104
-59.190641	-12.303714	1.156109
-59.699967	-13.258639	1.161114
-59.935288	-22.626587	1.166118
-60.228081	-14.404771	1.171123
-59.955916	-15.222282	1.176128
-60.293896	-12.170720	1.181133
-60.292287	-13.624338	1.186138
-60.177834	-25.396310	1.191142
-61.043908	-20.384998	1.196147
-61.425061	-26.826405	1.201152
-61.912581	-9.808566	1.206157
-61.774062	-3.855868	1.211162
-61.502893	-17.194347	1.216166
-62.867462	-17.120130	1.221171
-62.868458	-21.319878	1.226176
-63.175225	-13.275601	1.231181
-63.371908	-9.775226	1.236186
-63.162546	-21.273234	1.241190
-63.593885	-8.724584	1.246195
-63.593698	-13.123518	1.251200
-63.951155	-13.382667	1.256205
-64.726083	-17.983797	1.261210
-64.890926	-15.547157	1.266214
-65.472794	-9.521774	1.271219
-65.098268	-12.442268	1.276224
-65.205562	-1.893142	1.281229
-65.437389	-14.311503	1.286234
-65.202171	-15.901003	1.291238
-66.233798	-14.059054	1.296243
-66.394961	-22.933846	1.301248
-66.906575	-17.519703	1.306253
-66.845659	-11.293931	1.311258
-66.593570	-17.729797	1.316262
-67.099570	-10.301940	1.321267
-67.453195	-24.323438	1.326272
-68.015542	-11.204222	1.331277
-68.508003	-13.765377	1.336282
-67.890353	-10.854780	1.341286
-68.357412	-9.828193	1.346291
-68.811126	-18.820576	1.351296
-69.235868	-9.552219	1.356301
-69.687455	-12.837649	1.361306
-69.349118	-16.721450	1.366310
-69.823074	-7.471200	1.371315
-69.475676	-13.608800	1.376320
-70.625460	-17.254161	1.381325
-70.887151	-17.879855	1.386330
-71.226928	-11.754293	1.391334
-70.970437	-3.831808	1.396339
-71.016633	-6.802243	1.401344
-71.459961	-10.482575	1.406349
-72.210823	-18.980814	1.411354
-72.367153	-13.496444	1.416358
-72.807484	-4.819018	1.421363
-72.760639	-9.787900	1.426368
-72.811332	-10.088374	1.431373
-72.862559	-13.402481	1.436378
-72.954205	-10.937785	1.441382
-73.715793	-10.825299	1.446387
-73.893685	-18.247490	1.451392
-74.336768	-9.857093	1.456397
-74.516553	-4.529553	1.461402
-74.417996	-16.772547	1.466406
-74.556941	-10.851934	1.471411
-75.153463	-20.500646	1.476416
-75.756043	-11.086980	1.481421
-76.280530	-18.635684	1.486426
-76.107392	-15.432512	1.491430
-76.407150	-11.916287	1.496435
-76.062037	-17.480714	1.501440
-75.943513	-13.444350	1.506445
-76.616180	-8.115363	1.511450
-76.967567	-12.428273	1.516454
-77.452159	-12.210425	1.521459
-77.473192	-23.342620	1.526464
-77.664334	-18.013997	1.531469
-78.084308	-14.660614	1.536474
-78.507468	-17.952219	1.541478
-79.245744	-17.424991	1.546483
-79.572126	-17.544843	1.551488
-79.393544	-15.583061	1.556493
-79.548692	-11.878035	1.561498
-79.586512	-22.117783	1.566502
-79.503576	-18.027494	1.571507
-79.348731	-21.535379	1.576512
-80.070608	-29.912813	1.581517
-80.885394	-15.124071	1.586522
-81.115019	-16.501490	1.591526
-81.604365	-10.336311	1.596531
-81.153818	-16.303907	1.601536
-81.516806	-21.512166	1.606541
-82.025080	-16.307624	1.611546
-82.489261	-23.406953	1.616550
-83.258189	-15.293597	1.621555
-83.020772	-21.527753	1.626560
-83.221931	-9.616477	1.631565
-83.118517	-20.303194	1.636570
-82.777157	-24.983344	1.641574
-83.282211	-16.683732	1.646579
-83.273841	-8.939357	1.651584
-83.748799	-8.628885	1.656589
-84.472539	-9.054108	1.661594
-84.340980	-15.214636	1.666598
-84.726704	-13.372589	1.671603
-85.593558	-16.230281	1.676608
-85.866561	-14.342244	1.681613
-86.126302	-8.005171	1.686618
-86.237961	-8.989905	1.691622
-86.018442	-7.234666	1.696627
-86.110252	-13.753887	1.701632
-86.198949	-9.371129	1.706637
-86.833164	-8.060214	1.711642
-87.151276	-15.269517	1.716646
-87.573758	0.525208	1.721651
-87.536211	-3.428850	1.726656
-87.967277	-8.091445	1.731661
-87.788358	-7.610930	1.736666
-88.174673	-12.191834	1.741670
-88.997877	-16.778569	1.746675
-88.888483	-15.813512	1.751680
-89.212600	-11.049809	1.756685
-89.518884	-7.169650	1.761690
-89.457650	-17.374964	1.766694
-90.216982	-6.861033	1.771699
-90.666806	-2.213979	1.776704
-90.839135	-11.025763	1.781709
-91.217272	-7.589911	1.786714
-90.907145	-15.646607	1.791718
-91.047431	-7.991414	1.796723
-91.038488	-17.688889	1.801728
-91.168246	-13.874507	1.806733
-91.665308	-12.227253	1.811738
-91.714859	-19.666410	1.816742
-92.704975	-9.081486	1.821747
-92.680743	-12.941986	1.826752
-92.739701	-12.820231	1.831757
-93.385583	-19.608362	1.836762
-94.087634	-9.489839	1.841766
-94.097910	-1.859780	1.846771
-93.642676	-6.374073	1.851776
-94.479938	-10.653640	1.856781
-94.545990	-10.617923	1.861786
-94.248855	-21.628279	1.866790
-94.291610	-12.273593	1.871795
-94.932816	-3.190643	1.876800
-95.692396	-7.879743	1.881805
-95.933005	-11.067051	1.886810
-95.520024	-20.728600	1.891814
-96.216944	-16.139269	1.896819
-96.211479	-19.291774	1.901824
-96.386584	-14.647015	1.906829
-97.005518	-15.394304	1.911834
-97.291604	-21.062672	1.916838
-97.501216	-14.804525	1.921843
-97.521927	-20.682098	1.926848
-98.033779	-14.445426	1.931853
-98.564622	-14.168631	1.936858
-98.924615	-26.085048	1.941862
-99.251547	-15.752488	1.946867
-99.273967	-18.404247	1.951872
-99.164849	-8.107049	1.956877
-99.389624	-8.190419	1.961882
-99.315652	-20.810745	1.966886
-99.608453	-18.529156	1.971891
-99.817345	-20.685924	1.976896
-100.451211	-18.867682	1.981901
-101.053593	-8.023151	1.986906
-100.819332	-15.886671	1.991910
-101.006995	-16.107583	1.996915
-101.118568	-19.927109	2.006912
-101.147182	-13.214248	2.016909
-101.174234	-15.887867	2.026906
-100.493507	-13.370830	2.036902
-99.884957	-17.641394	2.046899
-98.602197	-24.558018	2.056896
-98.671684	-11.758894	2.066893
-98.107453	-9.499883	2.076890
-98.052057	-16.155183	2.086886
-97.276786	-13.591540	2.096883
-96.717323	-6.013735	2.106880
-96.205539	-10.755400	2.116877
-95.523257	-5.139148	2.126874
-95.446080	-4.907837	2.136870
-94.392596	-8.702317	2.146867
-93.703034	-12.827726	2.156864
-93.811771	-10.446033	2.166861
-93.636506	-10.446673	2.176858
-92.832634	-10.659467	2.186854
-92.226416	-18.693419	2.196851
-91.040252	-25.637542	2.206848
-90.993112	-16.590153	2.216845
-90.920968	-18.621984	2.226842
-90.436067	-8.134199	2.236838
-89.352019	-15.747586	2.246835
-89.038822	-16.344645	2.256832
-89.049176	-19.429782	2.266829
-87.885682	-12.095435	2.276826
-87.809878	-16.160105	2.286822
-87.482949	-16.497762	2.296819
-86.191960	-6.379186	2.306816
-85.791397	-13.924263	2.316813
-85.982262	-15.082566	2.326810
-85.240804	-15.771839	2.336806
-84.784564	-18.955920	2.346803
-84.370264	-15.716517	2.356800
-83.705535	-14.386263	2.366797
-83.226358	-20.404621	2.376794
-82.422681	-18.969212	2.386790
-81.471287	-16.990518	2.396787
-81.223498	-12.925835	2.406784
-81.332077	-18.135828	2.416781
-81.094272	-21.921147	2.426778
-80.164748	-10.093181	2.436774
-79.692622	-16.581168	2.446771
-79.142773	-20.517729	2.456768
-78.501170	-12.199203	2.466765
-78.383630	-14.391254	2.476762
-77.435735	-17.608879	2.486758
-77.051920	-14.427064	2.496755
-77.030092	-13.935305	2.506752
-75.578986	-13.959213	2.516749
-75.043133	-19.006630	2.526746
-75.171719	-20.718920	2.536742
-75.262939	-16.491921	2.546739
-74.099057	-19.810238	2.556736
-73.634776	-17.260292	2.566733
-73.054995	-11.942015	2.576730
-72.231228	-19.807048	2.586726
-72.131601	-10.489961	2.596723
-71.937905	-18.275560	2.606720
-70.798856	-24.784466	2.616717
-70.372782	-9.969117	2.626714
-70.074900	-16.032193	2.636710
-69.897462	-16.415179	2.646707
-68.704005	-18.209640	2.656704
-68.183449	-24.303884	2.666701
-68.223283	-26.448884	2.676698
-67.699410	-22.566148	2.686694
-66.986381	-17.717967	2.696691
-66.994429	-23.023600	2.706688
-65.974793	-20.900304	2.716685
-65.777890	-21.406329	2.726682
-65.375926	-20.468372	2.736678
-64.207075	-20.360481	2.746675
-63.960745	-19.472174	2.756672
-63.855125	-15.715604	2.766669
-63.218303	-12.831050	2.776666
-62.414684	-13.075310	2.786662
-61.901669	-14.096764	2.796659
-61.898574	-19.051294	2.806656
-61.071824	-20.181298	2.816653
-60.718419	-12.040362	2.826650
-59.659023	-16.161297	2.836646
-59.556312	-23.952799	2.846643
-59.374739	-16.858704	2.856640
-58.489129	-23.208965	2.866637
-58.013343	-15.362769	2.876634
-57.648540	-18.416756	2.886630
-57.030300	-19.577595	2.896627
-56.119559	-16.428432	2.906624
-56.278733	-19.694243	2.916621
-55.991385	-16.460428	2.926618
-55.144660	-18.448391	2.936614
-54.543750	-14.403244	2.946611
-53.799125	-7.869533	2.956608
-53.331909	-9.998168	2.966605
-53.270184	-8.987583	2.976602
-52.750789	-14.208409	2.986598
-51.948810	-21.785446	2.996595
-51.716296	-11.746297	3.006592
-50.516891	-17.249309	3.016589
-50.317612	-9.516747	3.026586
-50.400950	-10.231216	3.036582
-49.838717	-13.632451	3.046579
-48.586311	-7.491053	3.056576
-48.223494	-13.570196	3.066573
-48.475404	-19.974778	3.076570
-47.483381	-17.976714	3.086566
-46.724294	-24.368000	3.096563
-46.621755	-21.672033	3.106560
-46.514595	-19.913278	3.116557
-45.706176	-19.008709	3.126554
-44.980196	-12.892529	3.136550
-43.924803	-14.626830	3.146547
-43.821963	-19.407394	3.156544
-43.646739	-15.755180	3.166541
-43.382420	-13.347422	3.176538
-42.422402	-11.329053	3.186534
-42.091668	-16.977144	3.196531
-41.630978	-20.980561	3.206528
-40.511825	-15.226394	3.216525
-40.263294	-24.642060	3.226522
-40.083580	-18.529348	3.236518
-40.033108	-16.740480	3.246515
-38.882648	-17.226580	3.256512
-38.642510	-15.518151	3.266509
-37.518457	-14.923168	3.276506
-37.647755	-22.942743	3.286502
-37.096877	-20.885899	3.296499
-36.716951	-22.842747	3.306496
-35.511369	-10.407544	3.316493
-35.541162	-19.160523	3.326490
-35.453514	-18.791462	3.336486
-34.539567	-17.767617	3.346483
-34.337965	-26.612372	3.356480
-33.369179	-17.051206	3.366477
-33.184662	-15.650575	3.376474
-32.652814	-17.937963	3.386470
-31.646127	-15.668300	3.396467
-31.704480	-18.498651	3.406464
-31.254355	-18.261702	3.416461
-30.271996	-17.746528	3.426458
-29.865742	-19.667227	3.436454
-29.749800	-13.001069	3.446451
-28.748121	-20.676206	3.456448
-28.328054	-17.024053	3.466445
-28.264503	-19.722722	3.476442
-27.708591	-21.734140	3.486438
-26.850737	-10.357996	3.496435
-26.443547	-15.599493	3.506432
-25.452393	-21.343191	3.516429
-25.646481	-16.446837	3.526426
-25.178455	-12.661647	3.536422
-24.621624	-17.326887	3.546419
-23.467996	-15.746799	3.556416
-23.358578	-24.410566	3.566413
-23.333352	-17.564156	3.576410
-22.640091	-15.356886	3.586406
-21.770291	-16.932886	3.596403
-21.529086	-16.163947	3.606400
-20.859793	-19.771841	3.616397
-20.055071	-11.162678	3.626394
-20.047008	-13.108847	3.636390
-19.730013	-18.625955	3.646387
-18.734913	-14.963628	3.656384
-18.544111	-14.761169	3.666381
-18.418217	-17.414626	3.676378
-17.178430	-14.781342	3.686374
-16.678984	-12.593012	3.696371
-16.533814	-12.206390	3.706368
-15.849028	-12.121819	3.716365
-15.384679	-8.469177	3.726362
-15.477399	-5.850289	3.736358
-14.410997	-15.362004	3.746355
-13.673995	-17.755504	3.756352
-13.690198	-14.223876	3.766349
-12.218256	-12.414368	3.776346
-12.391828	-17.554950	3.786342
-11.871801	-15.878450	3.796339
-11.887526	-14.984864	3.806336
-10.637346	-14.615593	3.816333
-10.065264	-10.388459	3.826330
-10.337194	-11.452665	3.836326
-9.707912	-13.435805	3.846323
-8.854436	-23.378774	3.856320
-8.662871	-13.140525	3.866317
-7.881147	-12.378032	3.876314
-7.665934	-26.794446	3.886310
-6.677491	-21.236880	3.896307
-5.857348	-16.732764	3.906304
-6.144784	-23.366480	3.916301
-5.788429	-15.684372	3.926298
-4.701113	-8.261351	3.936294
-4.556411	-1.084100	3.946291
-4.117862	-1.076978	3.956288
-3.392805	6.715004	3.966285
-2.962614	22.263668	3.976282
-2.850938	21.692505	3.986278
-2.290885	27.903697	3.996275
-1.927028	53.285344	4.006272
-1.552294	68.894587	4.016269
-0.972299	88.000800	4.026266
-0.415197	114.974694	4.036262
0.000000	118.757110	4.041267
-0.178873	141.397341	4.046272
0.257472	142.930014	4.051277
0.191528	154.543335	4.056282
0.260618	162.452982	4.061286
0.902316	167.263818	4.066291
0.672745	178.068971	4.071296
0.799774	170.898475	4.076301
0.829601	177.392879	4.081306
1.075853	177.083679	4.086310
0.888396	174.781863	4.091315
0.588073	182.136162	4.096320
0.911203	175.359552	4.101325
0.908605	169.437865	4.106330
0.950178	185.877970	4.111334
0.960252	189.137142	4.116339
0.906862	186.830927	4.121344
1.081098	183.710865	4.126349
0.902220	184.991725	4.131354
0.958453	177.306790	4.136358
1.311457	182.667303	4.141363
0.690038	191.827699	4.146368
1.058807	193.390685	4.151373
1.057512	193.467001	4.156378
0.710879	185.526030	4.161382
0.853162	182.667756	4.166387
0.766052	191.273702	4.171392
0.812365	182.674080	4.176397
0.761966	191.143535	4.181402
0.990735	193.726187	4.186406
1.299246	195.071332	4.191411
1.041432	213.271847	4.196416
1.589101	218.650913	4.201421
1.332784	209.711001	4.206426
0.983931	188.870140	4.211430
1.294275	178.826162	4.216435
1.232083	189.217717	4.221440
1.263589	183.284075	4.226445
0.992820	190.819067	4.231450
1.287119	206.043416	4.236454
1.252696	204.018392	4.241459
0.860950	215.958977	4.246464
1.423071	213.791664	4.251469
1.606986	213.225504	4.256474
1.372683	209.514515	4.261478
1.526325	210.812051	4.266483
0.976944	203.618358	4.271488
1.667405	206.298549	4.276493
1.276406	212.960774	4.281498
1.170216	198.179158	4.286502
1.285746	209.707776	4.291507
1.160159	217.298504	4.296512
1.372385	215.611659	4.301517
1.041839	221.560969	4.306522
1.255532	216.694961	4.311526
1.120312	220.386885	4.316531
1.169013	221.562560	4.321536
1.399674	212.670918	4.326541
1.329970	223.283150	4.331546
1.290673	220.032822	4.336550
1.579918	218.680225	4.341555
1.635359	216.659094	4.346560
1.711326	221.167133	4.351565
1.646704	229.182868	4.356570
1.741021	214.815313	4.361574
1.808061	216.904873	4.366579
1.587035	216.355316	4.371584
1.841684	218.314526	4.376589
1.172178	222.842662	4.381594
0.993645	213.078836	4.386598
1.562835	216.781915	4.391603
1.540414	230.053921	4.396608
1.961716	233.656544	4.401613
1.808567	233.263486	4.406618
1.584666	222.720462	4.411622
1.636602	222.502764	4.416627
1.367346	229.976753	4.421632
1.537451	238.218696	4.426637
1.870665	241.995505	4.431642
1.764193	243.584447	4.436646
1.737445	245.554153	4.441651
1.618413	246.402284	4.446656
1.737335	244.820929	4.451661
1.510299	251.145701	4.456666
1.582372	257.725698	4.461670
1.802123	254.204162	4.466675
1.810445	243.536915	4.471680
1.574550	249.890577	4.476685
1.841489	252.680129	4.481690
1.904463	265.075987	4.486694
1.788485	243.756952	4.491699
1.567192	251.585392	4.496704
2.204603	242.170227	4.501709
2.007092	246.170889	4.506714
1.698285	247.561918	4.511718
2.018956	247.065796	4.516723
1.829410	249.521851	4.521728
2.000333	241.855913	4.526733
1.853981	246.468279	4.531738
1.763425	247.539306	4.536742
2.077343	244.519667	4.541747
2.034332	253.273942	4.546752
2.461975	244.083257	4.551757
2.310966	252.881917	4.556762
1.696737	253.695468	4.561766
2.196052	237.314361	4.566771
1.782099	243.357868	4.571776
1.890839	233.605552	4.576781
1.632749	253.180549	4.581786
2.268713	279.122651	4.586790
2.170618	281.730329	4.591795
1.996769	276.027704	4.596800
2.057311	280.629172	4.601805
1.977698	279.787206	4.606810
2.092538	282.477295	4.611814
2.260138	275.063860	4.616819
2.107969	274.140259	4.621824
2.410744	271.741925	4.626829
1.955790	282.508430	4.631834
2.005237	281.916640	4.636838
2.507439	275.831875	4.641843
2.569226	282.692487	4.646848
2.808121	284.605966	4.651853
2.418437	281.938483	4.656858
2.665152	280.293682	4.661862
2.507375	274.474157	4.666867
2.089026	263.261292	4.671872
2.268562	276.348031	4.676877
2.232164	282.097512	4.681882
1.995543	287.636400	4.686886
2.106516	285.662712	4.691891
1.630129	285.536170	4.696896
2.066448	280.099419	4.701901
2.075803	286.362449	4.706906
2.331677	303.047945	4.711910
2.663796	306.572388	4.716915
2.340716	306.946847	4.721920
2.491846	297.062981	4.726925
2.271121	305.623984	4.731930
2.364995	308.829574	4.736934
2.181088	307.523294	4.741939
2.246344	315.824733	4.746944
2.542602	310.544304	4.751949
2.569473	315.141383	4.756954
2.708118	315.565624	4.761958
2.717870	311.340131	4.766963
2.578375	317.043128	4.771968
2.522556	314.909155	4.776973
2.469185	320.863506	4.781978
2.005845	306.707792	4.786982
2.636189	310.236523	4.791987
2.435481	318.760485	4.796992
2.707924	312.894414	4.801997
2.548141	316.491171	4.807002
2.636772	319.350652	4.812006
2.731912	314.260323	4.817011
2.535540	312.708177	4.822016
2.470964	315.869907	4.827021
2.734300	334.643670	4.832026
2.852563	335.335979	4.837030
2.771051	326.210049	4.842035
2.490070	328.806521	4.847040
2.853584	346.947136	4.852045
3.032060	358.133875	4.857050
2.763077	348.289607	4.862054
2.877386	348.276772	4.867059
2.706068	356.915274	4.872064
2.540574	353.220897	4.877069
2.752899	361.909360	4.882074
2.948153	353.732640	4.887078
3.225823	354.296891	4.892083
2.994785	356.796619	4.897088
3.256982	353.063233	4.902093
2.843762	341.089997	4.907098
2.556885	339.865055	4.912102
2.942003	334.838776	4.917107
2.788997	353.996577	4.922112
2.779778	346.947173	4.927117
2.875480	359.501767	4.932122
3.049132	365.241627	4.937126
3.277426	344.632129	4.942131
2.899182	350.141366	4.947136
3.235251	348.957814	4.952141
3.150102	359.692661	4.957146
2.995378	356.261992	4.962150
3.405104	356.046432	4.967155
3.365460	353.958321	4.972160
3.200565	352.863772	4.977165
3.289445	356.620609	4.982170
2.936673	344.263567	4.987174
3.197083	354.715872	4.992179
2.862486	373.812744	4.997184
3.090093	361.898251	5.002189
3.294987	351.872079	5.007194
3.123741	356.254476	5.012198
3.414305	352.589015	5.017203
3.076950	368.212994	5.022208
3.209319	362.839170	5.027213
3.014633	356.498683	5.032218
3.071633	351.797437	5.037222
3.578340	356.431846	5.042227
2.742400	354.187346	5.047232
3.188316	350.795638	5.052237
2.938991	353.578674	5.057242
2.970012	360.815456	5.062246
3.207885	355.669365	5.067251
2.770196	361.320137	5.072256
3.107378	367.380446	5.077261
3.407453	385.339206	5.082266
2.984005	387.269120	5.087270
3.393613	379.258423	5.092275
3.333141	385.768923	5.097280
3.545752	372.977956	5.102285
3.474767	382.341798	5.107290
3.188286	389.443021	5.112294
3.578067	383.093742	5.117299
3.255242	387.862779	5.122304
3.526774	381.783535	5.127309
3.400994	380.417623	5.132314
3.440324	392.603010	5.137318
3.389295	380.659667	5.142323
3.522892	376.297569	5.147328
3.203023	372.441151	5.152333
3.225067	377.654769	5.157338
3.353345	386.132590	5.162342
3.740798	382.355511	5.167347
3.600331	376.456133	5.172352
3.682276	378.284867	5.177357
3.378087	388.299127	5.182362
3.424243	387.911901	5.187366
4.003899	386.612916	5.192371
3.567880	390.048947	5.197376
3.699643	375.071366	5.202381
3.730906	381.942197	5.207386
3.359780	382.402933	5.212390
3.720544	391.957270	5.217395
3.692212	410.039489	5.222400
3.878501	407.475499	5.227405
3.946247	394.784026	5.232410
3.749041	385.564315	5.237414
3.773036	381.443591	5.242419
3.519367	386.343168	5.247424
3.904161	398.074075	5.252429
4.045809	408.938505	5.257434
3.675181	406.411596	5.262438
3.808071	383.667560	5.267443
3.783638	394.886082	5.272448
3.667574	400.482436	5.277453
3.769153	407.959948	5.282458
3.666067	399.313959	5.287462
3.962844	406.326795	5.292467
3.808744	407.051488	5.297472
3.982697	399.262932	5.302477
3.898402	403.600291	5.307482
3.613546	406.007007	5.312486
3.768713	402.763671	5.317491
3.488372	401.198359	5.322496
3.586860	395.182532	5.327501
3.661694	393.754758	5.332506
3.621942	408.412374	5.337510
4.029681	413.760076	5.342515
3.913343	429.339305	5.347520
4.213736	435.975077	5.352525
4.214111	422.997950	5.357530
4.026988	431.345498	5.362534
4.317019	429.765741	5.367539
4.145630	427.986783	5.372544
4.018470	416.910866	5.377549
3.781200	422.154823	5.382554
3.832088	429.904337	5.387558
4.116692	424.748132	5.392563
3.926849	439.449721	5.397568
4.117805	435.554252	5.402573
4.351476	432.950166	5.407578
4.368216	436.952567	5.412582
4.238975	428.074401	5.417587
4.234422	438.507803	5.422592
4.375819	440.185638	5.427597
4.017623	446.883980	5.432602
4.023565	441.735738	5.437606
4.042904	431.914310	5.442611
4.033384	438.075647	5.447616
3.993711	436.030347	5.452621
4.168666	437.884463	5.457626
3.970674	435.913866	5.462630
4.422305	434.710324	5.467635
3.908326	431.261659	5.472640
4.349367	448.018232	5.477645
4.719595	456.309995	5.482650
4.249299	457.786924	5.487654
4.432040	449.118733	5.492659
4.254657	455.783251	5.497664
4.464018	453.021972	5.502669
4.768745	457.238724	5.507674
4.324206	458.274735	5.512678
4.536286	452.987648	5.517683
4.046179	449.402437	5.522688
4.522328	451.870160	5.527693
4.489992	466.133353	5.532698
4.371852	472.004938	5.537702
4.849661	460.476805	5.542707
4.626257	470.221157	5.547712
4.553635	470.265359	5.552717
4.640940	464.612245	5.557722
4.504125	473.906517	5.562726
4.762214	457.904228	5.567731
4.482616	462.863461	5.572736
4.435506	462.201887	5.577741
4.691414	458.750889	5.582746
4.312532	464.901353	5.587750
4.417228	465.424836	5.592755
4.497587	469.020816	5.597760
4.615451	479.248439	5.602765
4.830567	468.405386	5.607770
4.502299	468.980095	5.612774
4.842532	459.898834	5.617779
4.740131	472.537659	5.622784
4.740429	476.578205	5.627789
4.874250	469.645004	5.632794
4.288280	473.545851	5.637798
4.603808	457.890424	5.642803
4.560330	467.988823	5.647808
4.490895	479.467704	5.652813
4.410790	469.803768	5.657818
4.435440	469.793319	5.662822
4.801030	483.199627	5.667827
4.967226	501.515001	5.672832
5.144459	504.064984	5.677837
5.201243	501.924512	5.682842
4.397411	489.922872	5.687846
4.870836	482.807459	5.692851
4.929532	500.092251	5.697856
5.098545	504.890739	5.702861
4.960895	506.839737	5.707866
4.843505	505.515344	5.712870
5.198450	500.931647	5.717875
5.170293	487.815633	5.722880
5.045017	488.234460	5.727885
5.067130	478.675963	5.732890
4.812133	478.568377	5.737894
4.856499	486.951003	5.742899
4.502815	493.827981	5.747904
5.017044	507.161206	5.752909
4.822507	504.098568	5.757914
4.962113	504.345268	5.762918
5.110255	507.921176	5.767923
4.624740	521.293935	5.772928
4.965765	505.274044	5.777933
5.157207	504.789207	5.782938
5.238464	514.996661	5.787942
5.578623	507.625534	5.792947
5.166710	513.435086	5.797952
5.305438	502.895380	5.802957
5.230390	505.020299	5.807962
5.452134	509.647979	5.812966
5.640324	509.946733	5.817971
5.418524	508.967043	5.822976
5.334671	502.430890	5.827981
5.486743	497.819946	5.832986
5.093355	499.798577	5.837990
5.209230	489.443201	5.842995
5.059967	512.175079	5.848000
5.163642	510.100950	5.853005
5.499256	506.106479	5.858010
5.096339	504.027670	5.863014
5.463694	510.935461	5.868019
5.174614	511.446868	5.873024
5.132970	508.242348	5.878029
5.112703	513.785323	5.883034
4.951286	509.331253	5.888038
5.271260	502.886022	5.893043
4.909586	513.256056	5.898048
5.373822	511.773490	5.903053
5.406793	508.721399	5.908058
4.898464	517.435317	5.913062
5.443049	524.319843	5.918067
5.571239	540.269491	5.923072
5.458595	541.001547	5.928077
5.389074	546.551390	5.933082
5.285961	548.468047	5.938086
5.376507	546.832944	5.943091
5.321854	539.423259	5.948096
5.547941	536.513876	5.953101
5.634821	541.070817	5.958106
5.134081	548.170622	5.963110
5.674192	545.252852	5.968115
5.628928	544.663089	5.973120
5.403490	540.586206	5.978125
5.436394	545.289796	5.983130
5.428086	554.397034	5.988134
5.670856	544.706923	5.993139
5.966630	551.331078	5.998144
5.722336	535.006144	6.003149
5.588535	536.222558	6.008154
5.300205	548.032852	6.013158
5.398061	541.063633	6.018163
5.598306	556.899081	6.023168
6.032505	563.301469	6.028173
5.948933	554.104709	6.033178
5.667752	547.748642	6.038182
5.853358	540.163300	6.043187
5.759820	551.807822	6.048192
5.705564	554.000050	6.053197
5.782898	551.338117	6.058202
5.560089	549.654955	6.063206
5.680096	541.968771	6.068211
5.739805	555.487747	6.073216
5.939699	568.348598	6.078221
5.951860	559.198368	6.083226
5.616045	555.897719	6.088230
5.985045	541.819413	6.093235
5.813083	548.877712	6.098240
5.481328	540.382299	6.103245
5.724410	542.974780	6.108250
5.557375	553.408966	6.113254
5.859425	565.512301	6.118259
5.950620	578.839826	6.123264
5.796022	560.864372	6.128269
6.121501	551.182492	6.133274
5.849327	549.354073	6.138278
6.047774	539.214992	6.143283
5.663942	551.266605	6.148288
5.821048	543.813339	6.153293
6.074407	540.721271	6.158298
5.852041	542.193740	6.163302
5.757712	546.425654	6.168307
5.625883	543.699136	6.173312
5.516518	556.364338	6.178317
5.711379	551.976676	6.183322
5.865888	550.053673	6.188326
6.098260	545.912972	6.193331
5.909661	553.622803	6.198336
5.278361	555.407625	6.203341
6.137188	555.896563	6.208346
5.480644	554.151690	6.213350
5.793868	549.961716	6.218355
5.986111	554.644798	6.223360
6.032075	543.067703	6.228365
5.971921	546.543273	6.233370
5.689750	553.485709	6.238374
5.703902	552.160983	6.243379
5.941467	561.518045	6.248384
5.684786	554.712678	6.253389
6.002861	539.984734	6.258394
5.560237	544.810909	6.263398
6.168230	541.087718	6.268403
6.062477	552.743928	6.273408
6.312456	548.713479	6.278413
5.980889	527.494792	6.283418
5.918852	510.225001	6.288422
5.810460	508.979429	6.293427
5.681202	519.257684	6.298432
5.404625	520.913835	6.303437
5.603474	513.673498	6.308442
5.618930	535.884206	6.313446
5.515828	535.552424	6.318451
5.799780	544.143024	6.323456
5.956397	548.273977	6.328461
6.162860	546.398427	6.333466
6.080854	531.003768	6.338470
5.622862	519.570844	6.343475
5.642767	523.880560	6.348480
5.736542	517.034362	6.353485
5.876480	516.141105	6.358490
5.426984	521.493470	6.363494
5.817593	514.217299	6.368499
5.671849	538.314071	6.373504
5.934003	539.752643	6.378509
5.566897	536.028398	6.383514
5.452294	548.658350	6.388518
5.874588	547.585142	6.393523
5.731277	559.066031	6.398528
5.455163	556.513513	6.403533
5.666089	548.194103	6.408538
5.222452	555.830059	6.413542
5.543494	544.578462	6.418547
6.127919	543.718893	6.423552
5.600590	554.430558	6.428557
5.788522	549.061596	6.433562
5.612770	547.511937	6.438566
6.059197	544.314659	6.443571
5.992005	555.902245	6.448576
6.073839	557.902192	6.453581
6.042520	559.780940	6.458586
5.707151	551.977915	6.463590
5.930639	541.208606	6.468595
5.791464	549.291781	6.473600
6.003990	546.840836	6.478605
5.801479	547.248948	6.483610
5.986426	550.867521	6.488614
5.968396	538.669981	6.493619
5.665880	520.951557	6.498624
5.750620	507.385730	6.503629
5.853961	526.545582	6.508634
5.310205	535.999682	6.513638
5.863732	527.422797	6.518643
5.891963	550.049629	6.523648
5.476683	541.508428	6.528653
5.637355	552.248662	6.533658
5.612720	554.843655	6.538662
5.744447	544.388444	6.543667
5.818418	549.372247	6.548672
5.729667	540.688589	6.553677
5.979321	542.571712	6.558682
5.537925	556.697280	6.563686
6.055828	545.973533	6.568691
5.789534	547.993321	6.573696
5.984063	546.341133	6.578701
6.224622	549.568410	6.583706
5.641621	538.121600	6.588710
5.826311	517.575017	6.593715
5.513317	521.153040	6.598720
5.454417	528.468791	6.603725
5.737540	541.822775	6.608730
5.292854	541.482820	6.613734
5.980162	548.011587	6.618739
5.836039	552.112918	6.623744
5.563322	547.281312	6.628749
5.643433	547.746212	6.633754
5.684881	550.983504	6.638758
6.009118	547.646787	6.643763
5.783454	554.116188	6.648768
5.833333	556.379705	6.653773
5.739566	549.876445	6.658778
5.470923	548.759169	6.663782
5.503543	546.876731	6.668787
5.332570	548.928912	6.673792
5.383017	558.303378	6.678797
5.808929	556.532940	6.683802
5.286334	552.737898	6.688806
5.681551	556.974649	6.693811
5.424264	568.945674	6.698816
5.753011	583.329950	6.703821
5.576043	582.986005	6.708826
5.675839	585.831752	6.713830
6.089571	585.614838	6.718835
5.764863	582.385652	6.723840
5.932099	588.604264	6.728845
5.839800	583.701789	6.733850
5.850591	594.804137	6.738854
5.720334	584.912621	6.743859
5.946027	584.194416	6.748864
6.052465	577.296671	6.753869
5.768363	557.827021	6.758874
5.460574	565.954446	6.763878
5.562026	559.595028	6.768883
5.700442	575.039763	6.773888
5.494696	580.667873	6.778893
5.671970	579.967437	6.783898
5.624344	586.146377	6.788902
5.750502	578.706496	6.793907
5.382334	590.305665	6.798912
5.627108	597.030514	6.803917
5.934922	579.034365	6.808922
5.854188	580.526250	6.813926
5.805402	582.083990	6.818931
5.762372	574.282860	6.823936
5.635870	590.591444	6.828941
5.847614	583.263800	6.833946
5.828892	589.975165	6.838950
6.087504	581.793379	6.843955
5.734040	582.590588	6.848960
5.632729	581.139418	6.853965
5.672242	575.510244	6.858970
5.773224	589.635102	6.863974
5.803819	580.936237	6.868979
5.975217	585.950618	6.873984
5.878412	583.092317	6.878989
6.169822	585.167738	6.883994
6.018513	589.632937	6.888998
5.845523	576.244804	6.894003
6.015743	576.028076	6.899008
5.795884	561.902923	6.904013
5.976192	552.141144	6.909018
5.624268	552.839044	6.914022
5.701182	552.087712	6.919027
5.365574	550.069991	6.924032
5.540809	566.488316	6.929037
5.909296	569.770325	6.934042
5.734508	584.299969	6.939046
6.220296	585.562183	6.944051
5.910203	575.495279	6.949056
5.835559	562.978048	6.954061
5.799857	553.959153	6.959066
5.264200	555.925685	6.964070
5.626290	561.244873	6.969075
5.889925	582.124175	6.974080
5.836702	574.141026	6.979085
5.970819	565.485442	6.984090
5.688753	564.297177	6.989094
5.997268	552.573588	6.994099
5.657057	553.063355	6.999104
5.411915	558.431983	7.004109
5.600728	573.092631	7.009114
5.540739	588.437076	7.014118
5.934374	587.098077	7.019123
5.865130	593.185090	7.024128
5.510988	590.228725	7.029133
5.855111	582.591317	7.034138
5.735256	592.655161	7.039142
5.588254	591.551916	7.044147
5.697947	592.158043	7.049152
5.543866	585.835514	7.054157
5.817317	577.173670	7.059162
5.384699	592.032139	7.064166
5.791433	581.688522	7.069171
5.520384	595.695799	7.074176
5.527683	587.216252	7.079181
5.824214	587.910980	7.084186
5.709026	593.771764	7.089190
5.615530	589.409348	7.094195
5.708342	593.588742	7.099200
5.761104	581.916669	7.104205
5.822667	574.449186	7.109210
5.738103	596.413583	7.114214
5.774260	592.043159	7.119219
5.554690	595.658148	7.124224
5.828261	594.148676	7.129229
5.895001	586.809871	7.134234
6.023530	591.085277	7.139238
6.038116	587.508185	7.144243
6.124245	590.972615	7.149248
6.145413	592.730123	7.154253
6.015532	583.861838	7.159258
5.571754	589.798232	7.164262
5.980505	585.010274	7.169267
5.868153	589.763928	7.174272
5.730544	593.562198	7.179277
6.151148	575.598026	7.184282
6.094380	584.467036	7.189286
5.438511	569.901592	7.194291
5.736792	581.336949	7.199296
5.916482	590.369533	7.204301
6.036379	581.893284	7.209306
5.868608	573.034227	7.214310
5.613023	561.060913	7.219315
5.527313	555.424716	7.224320
5.792970	578.979114	7.229325
5.992682	581.592483	7.234330
5.740216	569.676066	7.239334
5.524387	552.953549	7.244339
5.694879	574.646877	7.249344
5.609364	587.847435	7.254349
5.949748	591.935304	7.259354
5.757261	596.926554	7.264358
6.124326	581.635023	7.269363
6.095992	576.760752	7.274368
5.755614	565.066051	7.279373
5.932341	553.395417	7.284378
5.381422	562.859398	7.289382
5.367519	570.559015	7.294387
5.509061	572.655451	7.299392
5.948502	582.275931	7.304397
5.812163	588.294808	7.309402
5.843688	590.305441	7.314406
5.960966	598.233593	7.319411
5.969735	589.440361	7.324416
5.513656	577.979946	7.329421
5.951351	566.965964	7.334426
5.864866	579.084976	7.339430
5.731111	574.811993	7.344435
5.967316	575.068283	7.349440
5.262712	572.161550	7.354445
5.796352	570.118076	7.359450
5.709289	596.507550	7.364454
5.890813	582.352749	7.369459
6.035218	582.662983	7.374464
5.617822	577.008288	7.379469
5.719518	570.598015	7.384474
5.616432	577.575291	7.389478
6.039932	582.010416	7.394483
5.999167	566.312238	7.399488
5.784311	575.858815	7.404493
6.102602	566.224680	7.409498
5.835732	569.117008	7.414502
5.441927	565.348233	7.419507
5.710789	570.334959	7.424512
5.506240	564.901706	7.429517
5.680931	563.332018	7.434522
5.529830	568.120878	7.439526
6.066836	578.836627	7.444531
5.696235	567.653139	7.449536
5.797116	567.578987	7.454541
5.628221	562.337556	7.459546
5.465795	588.430963	7.464550
5.817600	599.130272	7.469555
6.051082	595.220632	7.474560
5.822158	592.917120	7.479565
5.856013	584.062918	7.484570
5.720676	590.476858	7.489574
5.645105	576.175419	7.494579
5.601033	585.259678	7.499584
5.553681	590.385191	7.504589
5.846774	595.649987	7.509594
5.338269	601.759377	7.514598
5.647348	600.340723	7.519603
5.935691	593.669523	7.524608
5.599250	600.884368	7.529613
6.064667	586.772527	7.534618
5.987475	600.117735	7.539622
6.086138	589.375433	7.544627
5.751121	597.620340	7.549632
5.715682	597.770178	7.554637
6.001501	596.517761	7.559642
5.798666	593.909125	7.564646
5.475033	581.081109	7.569651
5.690868	594.342568	7.574656
5.686215	603.971138	7.579661
6.005857	595.478842	7.584666
5.710846	589.668359	7.589670
5.819533	588.290024	7.594675
5.799048	608.514847	7.599680
5.798610	603.465771	7.604685
5.852061	597.766013	7.609690
5.408319	600.459771	7.614694
5.711715	595.853587	7.619699
5.886041	598.981518	7.624704
5.647088	591.146754	7.629709
5.763598	583.975338	7.634714
5.560382	597.568977	7.639718
5.735518	590.860744	7.644723
5.708725	599.275515	7.649728
5.552154	592.899527	7.654733
5.857983	593.856533	7.659738
5.347838	599.580139	7.664742
5.614206	593.995948	7.669747
5.817424	598.311007	7.674752
5.704638	597.026394	7.679757
6.001370	593.589338	7.684762
6.042138	598.177299	7.689766
5.592370	595.012088	7.694771
5.685412	594.379045	7.699776
5.408464	601.061559	7.704781
5.706160	598.077091	7.709786
5.576020	592.790767	7.714790
5.477539	595.981342	7.719795
5.795288	596.415162	7.724800
5.723067	605.098594	7.729805
6.009637	596.650043	7.734810
5.709961	595.036505	7.739814
5.967190	599.793018	7.744819
5.890475	596.152381	7.749824
5.813251	595.515410	7.754829
5.800761	601.712821	7.759834
5.819310	601.060911	7.764838
5.882339	601.575203	7.769843
6.000651	593.588560	7.774848
5.802329	594.664298	7.779853
5.776016	587.045583	7.784858
5.736427	590.614549	7.789862
5.827097	595.170288	7.794867
6.081501	593.044009	7.799872
5.856399	600.256833	7.804877
6.043631	600.093824	7.809882
5.900732	603.296970	7.814886
5.899700	602.657669	7.819891
6.342934	601.747434	7.824896
5.939215	583.660102	7.829901
5.604367	570.602394	7.834906
5.471338	578.622907	7.839910
5.864431	580.976219	7.844915
5.815001	575.537257	7.849920
5.662380	576.251453	7.854925
6.139596	579.978109	7.859930
5.941251	573.755837	7.864934
6.033592	557.603151	7.869939
5.810644	566.654310	7.874944
5.530586	576.135299	7.879949
5.836936	551.746512	7.884954
5.674571	557.338932	7.889958
5.145955	566.176494	7.894963
5.664989	566.810871	7.899968
5.890273	591.905123	7.904973
6.094856	584.587146	7.909978
5.793686	578.221051	7.914982
5.380952	566.459872	7.919987
6.119798	580.682944	7.924992
5.838212	579.721910	7.929997
5.881882	563.330218	7.935002
5.508136	569.029398	7.940006
5.591370	561.892103	7.945011
5.870257	572.418062	7.950016
5.839017	570.351027	7.955021
5.724775	564.575697	7.960026
5.383247	564.191859	7.965030
5.197859	575.648241	7.970035
5.544731	574.367485	7.975040
5.313563	589.496728	7.980045
5.689548	578.866459	7.985050
5.556373	582.962437	7.990054
5.546394	589.179850	7.995059
5.713326	588.843301	8.000064
5.603887	595.561273	8.005069
5.506058	587.239590	8.010074
5.581754	612.569923	8.015078
5.804577	621.940705	8.020083
5.939217	622.059182	8.025088
5.754817	611.608613	8.030093
5.617284	592.650812	8.035098
5.623632	612.397937	8.040102
5.841876	625.917469	8.045120
6.137174	630.832199	8.050138
5.856319	609.818512	8.055155
5.994122	592.219983	8.060173
5.957016	598.215237	8.065190
5.924791	596.496008	8.070208
5.789802	593.031675	8.075226
5.827106	595.702431	8.080243
5.962789	594.675403	8.085261
5.400101	597.995606	8.090278
5.232957	603.491972	8.095296
5.883995	606.003837	8.100314
5.837816	617.793069	8.105331
5.753508	611.015827	8.110349
5.862874	622.190191	8.115366
5.686116	625.394860	8.120384
5.906164	625.363946	8.125402
5.758527	631.202805	8.130419
6.047953	622.430871	8.135437
5.717042	625.413027	8.140454
6.016389	628.963844	8.145472
6.004011	623.573871	8.150490
5.774293	628.137546	8.155507
6.263610	635.533647	8.160525
6.089159	616.793202	8.165542
5.880398	600.417772	8.170560
5.855744	605.994510	8.175578
5.698794	603.043163	8.180595
5.800535	590.462988	8.185613
5.970805	614.325401	8.190630
5.662266	635.257173	8.195648
6.064029	629.948634	8.200666
5.869149	634.209559	8.205683
6.497663	632.363618	8.210701
5.993337	610.234505	8.215718
5.925799	603.811418	8.220736
5.911220	607.481616	8.225754
5.596190	606.122844	8.230771
5.941215	611.714070	8.235789
6.322420	623.560413	8.240806
5.836555	617.035813	8.245824
6.057504	610.550486	8.250842
5.606884	610.107465	8.255859
5.788290	626.001958	8.260877
6.072595	629.760934	8.265894
5.689488	636.442896	8.270912
6.141796	630.254701	8.275930
6.132695	638.029869	8.280947
6.580093	630.375324	8.285965
6.338110	627.438122	8.290982
6.031264	611.770006	8.296000
6.082727	599.985689	8.301018
5.805480	603.722320	8.306035
5.843971	592.190600	8.311053
6.071076	624.724858	8.316070
5.824149	636.278724	8.321088
6.108874	634.948176	8.326106
5.804284	637.490826	8.331123
5.934128	626.545157	8.336141
5.937242	636.170143	8.341158
6.009254	631.420142	8.346176
6.090933	630.789468	8.351194
5.772852	631.508291	8.356211
5.894822	625.176594	8.361229
6.271883	635.985035	8.366246
6.059880	641.061246	8.371264
6.432714	635.691060	8.376282
6.467767	641.772519	8.381299
6.389819	636.173535	8.386317
6.386110	633.552109	8.391334
6.231203	642.772089	8.396352
6.202838	624.708157	8.401370
6.159547	626.395759	8.406387
6.086821	624.016901	8.411405
5.996937	616.145595	8.416422
5.857263	636.638021	8.421440
6.474900	634.095182	8.426458
5.806483	639.206568	8.431475
5.938725	636.395481	8.436493
6.460345	633.972231	8.441510
6.265588	627.550084	8.446528
6.324948	631.790642	8.451546
6.317420	634.638370	8.456563
5.951751	639.709271	8.461581
6.030756	632.634311	8.466598
5.900019	642.129774	8.471616
6.006181	627.305632	8.476634
5.757660	635.230680	8.481651
6.084829	639.567412	8.486669
6.039591	638.161986	8.491686
5.664256	649.291294	8.496704
6.180125	655.580751	8.501722
6.411173	657.332155	8.506739
6.377234	656.620014	8.511757
6.396670	637.061716	8.516774
6.232323	640.862559	8.521792
6.206593	628.349473	8.526810
6.066362	641.096717	8.531827
6.289430	644.124214	8.536845
6.579488	658.888580	8.541862
6.234852	647.993654	8.546880
6.361746	638.337116	8.551898
6.031987	634.166410	8.556915
6.037395	653.674718	8.561933
6.161371	647.166431	8.566951
6.231909	663.735272	8.571968
6.819983	670.044194	8.576986
6.532895	665.151986	8.582003
6.304925	654.978295	8.587021
6.288288	641.728097	8.592039
6.446325	662.814651	8.597056
6.290915	668.978670	8.602074
6.245557	665.210287	8.607091
6.234056	653.085215	8.612109
6.869045	650.973780	8.617127
6.419803	654.480920	8.622144
6.658167	643.877478	8.627162
6.232659	637.508811	8.632179
5.848764	645.701566	8.637197
6.474217	647.539537	8.642215
6.497055	660.041383	8.647232
6.454993	655.097369	8.652250
6.473135	660.082413	8.657267
6.400001	658.957236	8.662285
6.499854	660.373396	8.667303
6.365331	663.517461	8.672320
6.906191	648.803024	8.677338
6.996269	631.949019	8.682355
6.407871	629.051547	8.687373
6.556076	635.135560	8.692391
6.484918	637.059913	8.697408
6.904978	631.067762	8.702426
6.505007	627.993311	8.707443
6.349671	636.908491	8.712461
6.399812	626.808917	8.717479
6.346856	635.825463	8.722496
6.299729	637.917862	8.727514
6.457511	637.442692	8.732531
6.452512	641.547951	8.737549
6.360494	631.502176	8.742567
6.450108	625.210957	8.747584
6.456676	635.964995	8.752602
6.129166	635.064994	8.757619
6.328135	653.294586	8.762637
6.468431	653.549540	8.767655
6.571231	656.225621	8.772672
6.599746	663.624769	8.777690
6.802988	667.748467	8.782707
6.827815	674.691912	8.787725
6.895755	651.302033	8.792743
6.839856	642.512167	8.797760
6.691977	635.038851	8.802778
6.710942	631.462174	8.807795
6.654594	629.714059	8.812813
6.869323	624.384077	8.817831
6.602154	630.025503	8.822848
6.577788	617.352781	8.827866
6.354274	628.101635	8.832883
6.188659	625.871764	8.837901
6.373305	620.319630	8.842919
6.046398	627.094251	8.847936
6.599192	644.871140	8.852954
6.632631	655.623703	8.857971
6.674062	661.903393	8.862989
6.657531	660.896988	8.868007
6.625061	664.638944	8.873024
6.829114	655.446234	8.878042
6.757948	651.338282	8.883059
6.663557	666.198958	8.888077
6.682346	660.661720	8.893095
6.689603	666.872662	8.898112
6.905542	660.664373	8.903130
6.596973	663.827655	8.908147
6.516011	673.608857	8.913165
6.621396	673.957655	8.918183
6.819483	677.621461	8.923200
6.844906	666.486560	8.928218
6.909708	662.165225	8.933235
6.780229	659.893163	8.938253
7.042003	660.259122	8.943271
6.727259	662.915737	8.948288
6.614364	667.643648	8.953306
7.083703	648.058420	8.958323
6.723519	655.948496	8.963341
6.926319	661.378335	8.968359
6.738158	668.498682	8.973376
6.992410	665.312075	8.978394
7.054724	653.945535	8.983411
6.647716	648.489098	8.988429
6.625485	640.216413	8.993447
7.008948	652.459873	8.998464
6.953282	650.314961	9.003482
7.030792	639.461086	9.008499
6.480460	643.140610	9.013517
6.871675	645.546331	9.018535
6.484665	655.594594	9.023552
7.062889	662.198397	9.028570
6.830211	659.475263	9.033587
6.898733	675.599547	9.038605
7.099649	660.982707	9.043623
6.637840	664.763826	9.048640
6.806340	662.045839	9.053658
6.807622	668.084473	9.058675
6.661350	674.717275	9.063693
6.979009	670.564844	9.068711
6.959124	672.732751	9.073728
6.639790	665.804692	9.078746
6.732279	663.109894	9.083763
6.243332	671.431322	9.088781
7.062902	666.380933	9.093799
6.910561	673.938888	9.098816
6.807084	666.941304	9.103834
6.760247	663.823053	9.108851
6.970450	669.486670	9.113869
7.275341	674.820031	9.118887
6.848286	671.746406	9.123904
6.627943	658.922898	9.128922
6.681763	658.834922	9.133939
6.594713	668.299367	9.138957
7.022614	689.232916	9.143975
6.696061	697.377744	9.148992
6.903117	705.900456	9.154010
7.234057	700.711551	9.159027
7.072382	704.280905	9.164045
7.323220	702.450527	9.169063
6.919209	714.081976	9.174080
6.718301	712.524740	9.179098
7.046287	703.858770	9.184115
6.803906	695.480333	9.189133
6.822206	694.501827	9.194151
6.911095	707.757526	9.199168
6.756989	703.040146	9.204186
7.154239	701.392034	9.209203
7.029099	705.905876	9.214221
7.324854	702.498168	9.219239
7.069353	702.864782	9.224256
7.042924	702.542669	9.229274
7.111431	693.878843	9.234291
7.302274	695.159715	9.239309
7.246275	696.700337	9.244327
7.136315	704.931895	9.249344
7.017195	703.821596	9.254362
7.359380	701.952504	9.259379
6.967544	705.316137	9.264397
7.273243	697.655550	9.269415
7.248262	706.272111	9.274432
7.128579	707.924028	9.279450
7.208594	701.546387	9.284467
6.851891	710.841874	9.289485
6.695206	708.122804	9.294503
7.070814	698.234117	9.299520
6.814434	703.749694	9.304538
7.467722	706.041163	9.309555
7.119815	706.779974	9.314573
7.039704	699.685125	9.319591
7.400063	703.359023	9.324608
7.100516	710.662434	9.329626
7.485622	708.650445	9.334643
7.318142	713.062545	9.339661
7.187131	696.888595	9.344679
7.423936	703.279395	9.349696
7.102035	698.967830	9.354714
7.355593	702.876466	9.359731
6.927010	704.662192	9.364749
7.423815	714.395865	9.369767
7.356308	719.377074	9.374784
7.066683	714.828320	9.379802
7.671397	725.511030	9.384819
7.424432	729.802139	9.389837
7.109452	707.688044	9.394855
6.891514	705.215178	9.399872
7.215436	727.517698	9.404890
7.313332	724.900821	9.409907
7.404184	736.455133	9.414925
7.081251	729.890373	9.419943
7.260553	731.799033	9.424960
7.035179	731.686340	9.429978
7.292988	734.880034	9.434995
7.198802	733.206554	9.440013
7.177920	743.883426	9.445031
7.504225	734.583867	9.450048
7.173868	727.816432	9.455066
7.665330	730.377913	9.460083
7.203351	744.593428	9.465101
7.402737	731.976040	9.470119
7.347092	729.162133	9.475136
7.113661	731.397419	9.480154
7.342624	728.358163	9.485171
7.241854	741.749940	9.490189
7.198475	730.847585	9.495207
7.498351	751.732702	9.500224
7.641291	762.614563	9.505242
7.582438	756.073265	9.510259
7.516480	748.209943	9.515277
7.445875	740.389512	9.520295
7.175567	732.973284	9.525312
7.716768	755.280089	9.530330
7.446232	758.386916	9.535347
7.657705	764.035104	9.540365
7.782285	758.203919	9.545383
7.940070	736.733285	9.550400
7.458309	738.297527	9.555418
7.728718	731.626250	9.560435
7.514476	735.957024	9.565453
7.305102	742.455328	9.570471
7.392565	734.334613	9.575488
7.209132	742.878872	9.580506
7.578929	743.705050	9.585523
7.880817	757.406614	9.590541
7.356551	751.486823	9.595559
7.849082	751.474944	9.600576
7.718096	762.936431	9.605594
7.706461	743.379885	9.610611
7.670494	740.014392	9.615629
7.286808	730.074026	9.620647
7.457231	744.164563	9.625664
7.707401	762.112936	9.630682
8.143153	753.344399	9.635699
7.716667	754.494852	9.640717
7.509307	748.716360	9.645735
7.515357	731.628536	9.650752
7.568933	743.362016	9.655770
7.625862	741.426398	9.660787
7.561638	752.248013	9.665805
7.828675	771.042088	9.670823
7.945978	757.152240	9.675840
7.545585	747.396089	9.680858
7.602245	738.234183	9.685875
8.135132	757.871756	9.690893
8.093009	741.249482	9.695911
7.625015	735.312723	9.700928
7.539946	729.369762	9.705946
7.806504	720.898056	9.710963
7.671575	730.063515	9.715981
7.553746	735.586418	9.720999
7.676098	737.901470	9.726016
7.781957	752.801762	9.731034
7.857083	750.650376	9.736051
7.826359	751.427802	9.741069
7.689906	749.543625	9.746087
8.045487	745.190944	9.751104
7.887601	746.198403	9.756122
7.573767	736.023693	9.761139
7.961203	751.476168	9.766157
7.564806	752.204986	9.771175
8.120806	760.998258	9.776192
7.783108	765.668089	9.781210
8.033110	740.932166	9.786227
7.950981	740.394295	9.791245
8.038178	735.221548	9.796263
7.838702	729.265807	9.801280
7.479461	736.360627	9.806298
7.998689	734.707017	9.811315
7.829882	741.446802	9.816333
7.818477	738.398849	9.821351
7.807279	748.715721	9.826368
7.610031	762.604480	9.831386
7.758157	770.718435	9.836403
7.887553	769.677970	9.841421
7.703607	771.682681	9.846439
7.740052	761.023959	9.851456
7.730826	769.943313	9.856474
8.079429	775.845767	9.861491
7.938241	777.000444	9.866509
7.912914	777.552016	9.871527
8.172427	769.259567	9.876544
8.054342	770.715886	9.881562
7.931671	770.851137	9.886579
8.024722	763.488804	9.891597
8.106359	770.876667	9.896615
8.006038	768.000659	9.901632
7.687494	766.553590	9.906650
8.049073	770.289497	9.911667
8.154636	780.548715	9.916685
7.559467	771.681680	9.921703
7.873577	776.726593	9.926720
7.892398	770.505469	9.931738
7.813611	776.672810	9.936755
8.190126	776.546465	9.941773
7.916346	783.612816	9.946791
8.121117	786.058128	9.951808
8.081055	798.120064	9.956826
8.273877	799.268553	9.961843
7.914645	778.992368	9.966861
7.975198	792.560055	9.971879
8.397424	791.563307	9.976896
7.963382	795.572803	9.981914
8.027544	790.631759	9.986931
8.504167	798.503482	9.991949
8.355600	796.841737	9.996967
8.638807	778.734206	10.001984
8.274504	770.275008	10.007002
8.338637	759.653043	10.012019
8.340188	759.877590	10.017037
8.240669	757.695035	10.022055
8.337997	770.890349	10.027072
8.266568	763.045835	10.032090
8.085186	765.299291	10.037107
8.257755	759.916792	10.042125
8.030023	762.103511	10.047143
8.394150	762.615523	10.052160
8.411859	762.850389	10.057178
8.286143	769.188841	10.062195
8.256996	759.307564	10.067213
8.089873	768.584057	10.072231
8.162813	772.609159	10.077248
8.147906	766.597119	10.082266
7.924988	757.353865	10.087283
8.012478	759.690230	10.092301
8.135867	770.295846	10.097319
8.307525	783.151383	10.102336
8.189118	787.958181	10.107354
8.557638	792.313710	10.112371
8.573189	792.636321	10.117389
8.311332	779.092725	10.122407
8.709243	770.088347	10.127424
8.409362	773.440931	10.132442
8.117940	763.659873	10.137459
8.100471	772.664042	10.142477
7.931031	777.818190	10.147495
8.344529	780.501404	10.152512
8.167100	791.081168	10.157530
8.282495	795.986317	10.162547
8.460333	790.253781	10.167565
8.538449	803.612901	10.172583
8.437069	788.028742	10.177600
8.445610	794.202522	10.182618
8.218318	789.676510	10.187635
8.512228	787.796000	10.192653
8.441711	796.381855	10.197671
8.522208	802.633495	10.202688
8.605695	795.449864	10.207706
8.383285	793.705259	10.212723
8.582644	786.857149	10.217741
8.330894	802.530836	10.222759
8.235313	794.382670	10.227776
8.243651	789.412275	10.232794
8.345137	798.215926	10.237811
8.295715	794.879608	10.242829
8.282069	805.088475	10.247847
8.414521	793.373487	10.252864
8.850269	797.018220	10.257882
8.335502	793.241369	10.262899
8.479853	795.624829	10.267917
8.233521	808.498290	10.272935
8.517573	819.007716	10.277952
8.441071	829.027806	10.282970
8.681222	838.304152	10.287987
8.837575	829.183778	10.293005
8.608941	827.645480	10.298023
8.794599	822.153529	10.303040
8.799959	826.149072	10.308058
8.620884	813.774052	10.313075
8.586220	808.751712	10.318093
8.617236	819.360621	10.323111
8.900871	810.782123	10.328128
8.509875	811.277019	10.333146
8.659603	826.825143	10.338163
9.247743	819.689381	10.343181
8.667173	810.962210	10.348199
9.104025	794.486869	10.353216
8.402111	798.804960	10.358234
8.251354	794.417455	10.363251
8.909485	795.424296	10.368269
8.590892	800.090390	10.373287
8.615693	808.665617	10.378304
9.227735	810.162673	10.383322
8.916477	806.896586	10.388339
9.015949	793.622149	10.393357
8.559202	807.857720	10.398375
8.616678	794.598292	10.403392
8.533664	799.853303	10.408410
8.617177	805.988718	10.413427
9.054898	813.642703	10.418445
8.735475	813.840778	10.423463
9.042111	819.715938	10.428480
8.643114	813.567385	10.433498
8.922463	819.116597	10.438515
9.018591	800.413090	10.443533
8.590934	796.655302	10.448551
8.869859	813.980583	10.453568
8.693549	816.500487	10.458586
9.050805	834.106499	10.463603
9.003313	833.889619	10.468621
8.734738	834.021033	10.473639
8.656132	825.281166	10.478656
8.651384	832.187549	10.483674
8.700199	837.139338	10.488691
8.729863	839.299868	10.493709
8.619744	839.819596	10.498727
8.515577	837.045375	10.503744
8.530605	828.300661	10.508762
8.468457	841.382845	10.513779
9.182279	848.028582	10.518797
9.271560	854.331343	10.523815
8.572199	843.328881	10.528832
8.998626	849.964247	10.533850
8.798125	853.830654	10.538867
9.230511	860.026135	10.543885
9.107990	864.704918	10.548903
9.067688	864.407728	10.553920
9.341085	846.214744	10.558938
8.450112	844.347388	10.563955
9.173963	854.880993	10.568973
9.255985	859.141193	10.573991
9.114724	854.997141	10.579008
9.102557	853.422674	10.584026
9.182769	851.837074	10.589043
9.087134	839.315983	10.594061
9.132348	831.912318	10.599079
8.888740	831.431833	10.604096
8.941116	848.482240	10.609114
9.152502	867.626125	10.614131
9.225066	869.994890	10.619149
9.079388	871.269981	10.624167
9.020849	868.069187	10.629184
9.215854	865.592119	10.634202
9.207651	872.006847	10.639219
9.112433	866.806927	10.644237
9.030892	862.195991	10.649255
9.216739	859.599000	10.654272
9.320977	859.143497	10.659290
9.010029	872.901367	10.664307
9.269674	864.730085	10.669325
9.246556	866.387613	10.674343
9.312141	865.652127	10.679360
9.201620	858.827639	10.684378
9.035276	863.425095	10.689395
9.346407	858.990766	10.694413
9.333631	869.472125	10.699431
9.215286	866.868128	10.704448
9.284466	859.094998	10.709466
9.488619	872.975979	10.714483
9.409748	860.502092	10.719501
9.411293	870.915152	10.724519
9.133883	874.253218	10.729536
9.491567	871.172784	10.734554
9.074553	869.417227	10.739571
9.220610	860.947643	10.744589
9.465684	862.447287	10.749607
9.083072	875.366351	10.754624
9.239502	861.993875	10.759642
9.102774	867.521720	10.764659
9.281217	856.421817	10.769677
9.382794	864.451994	10.774695
9.053024	870.466982	10.779712
9.363151	869.463168	10.784730
9.073607	872.738290	10.789747
9.401163	886.042483	10.794765
9.554387	890.887877	10.799783
9.548856	895.162358	10.804800
9.800107	871.718923	10.809818
9.460380	865.143889	10.814835
9.640970	867.651273	10.819853
9.308681	868.256921	10.824871
9.126393	869.972638	10.829888
9.448101	870.507803	10.834906
9.619157	890.958369	10.839923
9.617232	896.449383	10.844941
9.369988	875.711918	10.849959
9.262928	890.044672	10.854976
9.804895	894.342438	10.859994
9.593811	898.019690	10.865011
9.600057	895.901121	10.870029
9.957873	897.075492	10.875047
9.527328	881.467695	10.880064
9.495249	876.982023	10.885082
9.287177	871.006588	10.890099
9.610457	889.835207	10.895117
9.830132	895.467131	10.900135
9.420107	899.980084	10.905152
9.807918	885.924571	10.910170
9.389059	902.866918	10.915187
9.662705	895.112531	10.920205
9.784772	901.679929	10.925223
9.582602	896.940319	10.930240
9.784052	891.060560	10.935258
9.722471	895.013648	10.940275
9.417278	893.052827	10.945293
9.884569	885.170988	10.950311
9.685144	899.491854	10.955328
10.060374	893.048816	10.960346
9.900295	896.421623	10.965363
9.553112	884.604754	10.970381
9.685553	886.903793	10.975399
9.566919	899.051418	10.980416
9.778471	890.270649	10.985434
9.824444	892.850078	10.990451
9.753157	888.288022	10.995469
9.737127	884.613345	11.000487
9.601753	893.497328	11.005504
9.868083	889.830704	11.010522
9.765791	886.441696	11.015539
9.874268	888.787996	11.020557
9.996239	885.958485	11.025575
9.734811	893.073231	11.030592
9.947365	887.863578	11.035610
9.810203	897.546745	11.040627
9.805386	889.606920	11.045645
9.356703	890.666577	11.050663
9.694039	896.787834	11.055680
10.031002	892.022310	11.060698
9.863249	900.342840	11.065715
9.829612	897.581555	11.070733
10.071178	898.355519	11.075751
9.883851	893.391642	11.080768
10.436113	879.550062	11.085786
9.796138	901.660211	11.090803
9.924396	891.212766	11.095821
9.996581	886.202856	11.100839
9.871514	896.010579	11.105856
10.225509	872.120115	11.110874
9.899748	887.644334	11.115891
10.017386	894.561027	11.120909
10.406422	880.559047	11.125927
10.563395	885.133391	11.130944
10.413131	880.950274	11.135962
10.426770	892.123826	11.140979
10.143713	893.519834	11.145997
10.284308	872.332910	11.151015
9.868343	860.714994	11.156032
9.925265	874.377432	11.161050
9.986110	889.094774	11.166067
10.240115	892.334201	11.171085
10.255475	888.494323	11.176103
10.046189	888.810397	11.181120
10.161894	886.884927	11.186138
10.026780	894.738717	11.191155
9.779285	900.145334	11.196173
10.109050	905.332168	11.201191
9.902222	902.879182	11.206208
10.208388	905.016859	11.211226
10.146043	901.219145	11.216243
10.127634	896.060844	11.221261
10.280247	891.017960	11.226279
9.875183	897.236906	11.231296
9.976406	885.128253	11.236314
10.161720	876.660637	11.241331
9.903818	880.022839	11.246349
10.157212	883.867780	11.251367
9.790527	892.373518	11.256384
10.302034	903.382926	11.261402
10.393250	905.164849	11.266419
10.324964	912.914115	11.271437
10.365884	900.247002	11.276455
10.331455	906.637343	11.281472
10.357457	911.801948	11.286490
10.628918	918.493854	11.291507
10.424188	911.588273	11.296525
10.485810	898.090903	11.301543
10.164786	902.301794	11.306560
10.111616	886.829824	11.311578
10.151235	898.400401	11.316595
10.142595	908.656926	11.321613
10.458313	915.408042	11.326631
10.179187	908.622023	11.331648
10.483721	909.097242	11.336666
10.730220	907.487306	11.341683
10.078890	914.356702	11.346701
10.425392	907.226585	11.351719
10.083800	908.566137	11.356736
10.380069	906.614958	11.361754
10.349858	912.657809	11.366771
10.418925	918.734249	11.371789
10.429823	907.023713	11.376807
10.320100	905.668873	11.381824
10.456035	910.945605	11.386842
10.404535	906.302924	11.391859
10.219823	918.052493	11.396877
10.518148	928.254566	11.401895
10.469620	942.329507	11.406912
10.574451	948.611432	11.411930
10.968491	945.162237	11.416947
10.556352	930.924754	11.421965
10.606188	920.335155	11.426983
10.414265	922.017042	11.432000
10.580386	938.813356	11.437018
10.892171	946.116624	11.442035
10.402993	929.959695	11.447053
10.476165	937.450595	11.452071
10.379856	947.262651	11.457088
10.973090	942.277034	11.462106
11.018180	941.105236	11.467123
10.773302	937.137118	11.472141
10.618710	927.105624	11.477159
10.746971	928.425003	11.482176
10.929534	932.078347	11.487194
10.632950	922.795796	11.492211
10.579769	932.151378	11.497229
10.889106	937.757084	11.502247
10.764731	945.241860	11.507264
11.100146	933.602460	11.512282
10.791453	922.625721	11.517299
10.486032	917.191272	11.522317
10.851167	924.773266	11.527335
10.633379	940.514500	11.532352
10.947632	934.535978	11.537370
10.945351	938.340126	11.542387
10.800672	929.830572	11.547405
10.799922	935.449141	11.552423
10.830670	931.514992	11.557440
10.895061	947.858320	11.562458
11.083734	934.302330	11.567475
10.364492	938.779006	11.572493
11.144494	943.452542	11.577511
10.953635	942.885395	11.582528
10.794843	947.488123	11.587546
10.836966	932.044448	11.592563
10.617564	943.233126	11.597581
10.915141	934.530228	11.602599
10.778513	930.360787	11.607616
10.608568	949.953755	11.612634
11.004009	949.153126	11.617651
10.711695	949.305194	11.622669
11.090000	944.249008	11.627687
10.981079	952.812561	11.632704
11.127073	943.166551	11.637722
10.719123	941.985578	11.642739
10.342492	950.609115	11.647757
10.455810	957.709789	11.652775
10.897459	971.508115	11.657792
11.285531	968.513767	11.662810
10.991653	966.898651	11.667827
10.963810	980.487410	11.672845
11.081694	987.031326	11.677863
10.785786	982.450268	11.682880
10.882656	975.347990	11.687898
11.316941	970.721650	11.692915
11.123555	986.705318	11.697933
11.641785	978.310760	11.702951
11.451380	977.053880	11.707968
11.167215	971.856019	11.712986
11.469645	970.433654	11.718003
11.193200	971.669348	11.723021
11.196858	974.107971	11.728039
10.964478	979.194450	11.733056
10.891568	987.270649	11.738074
11.361466	986.259516	11.743091
11.112609	982.275511	11.748109
11.476873	973.367310	11.753127
11.498615	974.490155	11.758144
11.336120	973.568768	11.763162
11.650846	983.417236	11.768179
11.490909	984.663595	11.773197
11.272311	974.911307	11.778215
11.172558	981.988944	11.783232
11.154518	968.954018	11.788250
11.563494	973.095268	11.793267
11.273315	982.098176	11.798285
11.010817	982.242364	11.803303
11.442509	975.501423	11.808320
11.295217	979.220113	11.813338
11.255088	970.707824	11.818355
11.202829	976.757493	11.823373
11.438296	971.507810	11.828391
11.013884	973.320234	11.833408
11.016709	979.565297	11.838426
11.257396	981.673458	11.843443
11.256816	996.260720	11.848461
11.569124	997.047602	11.853479
11.402788	1001.310897	11.858496
11.315801	1007.812312	11.863514
11.767461	1009.626399	11.868531
11.492549	1013.627762	11.873549
11.702393	1010.618968	11.878567
11.667683	1016.799000	11.883584
11.403206	1016.441230	11.888602
11.780820	1013.708406	11.893619
11.577418	1020.056058	11.898637
12.040756	1003.222629	11.903655
11.749850	987.243472	11.908672
11.235919	991.091247	11.913690
11.326057	980.192828	11.918707
11.555373	994.123885	11.923725
11.867404	1002.965880	11.928743
11.728622	1008.740140	11.933760
11.753363	1007.863781	11.938778
11.653548	977.816816	11.943795
11.301291	993.403188	11.948813
11.485491	999.349430	11.953831
11.861583	993.832247	11.958848
11.755224	1005.828344	11.963866
11.689814	1008.900535	11.968883
11.977709	1009.462550	11.973901
12.005385	1003.821669	11.978919
11.901192	1002.992204	11.983936
11.634279	986.286360	11.988954
12.054115	991.150905	11.993971
11.672485	986.985131	11.998989
11.730990	984.254660	12.004007
11.933717	1000.619271	12.009024
11.713070	996.197793	12.014042
12.202965	1002.744796	12.019059
11.557801	988.810688	12.024077
11.862023	990.082690	12.029095
11.927536	996.137507	12.034112
11.445300	1011.127754	12.039130
11.781343	1004.900169	12.044147
11.987475	1007.516132	12.049165
12.024181	1014.594065	12.054183
12.155934	1017.621671	12.059200
11.998894	1017.341604	12.064218
12.034759	1011.380321	12.069235
11.885030	1009.565619	12.074253
11.887150	1007.336906	12.079271
12.079347	1008.802198	12.084288
11.892078	1020.287741	12.089306
11.831563	1017.215767	12.094323
11.935188	1013.557305	12.099341
12.213788	1018.023806	12.104359
12.201334	1018.792125	12.109376
11.842086	1011.887824	12.114394
12.119118	1013.959082	12.119411
11.628948	1008.206365	12.124429
11.617601	1018.748604	12.129447
11.952355	1018.608296	12.134464
12.186853	1016.417941	12.139482
11.717142	1011.157829	12.144499
11.702083	1014.918249	12.149517
11.686187	1012.949363	12.154535
11.962931	1028.497760	12.159552
12.321229	1051.853178	12.164570
12.321090	1043.186624	12.169587
12.310032	1041.203158	12.174605
12.452725	1037.197143	12.179623
12.404911	1020.289922	12.184640
12.005539	1018.511552	12.189658
11.913408	1021.991250	12.194675
12.102771	1032.521391	12.199693
11.901846	1037.660753	12.204711
12.200605	1032.577139	12.209728
12.046215	1034.962965	12.214746
12.341211	1035.899538	12.219763
12.098536	1038.768387	12.224781
12.119580	1040.630611	12.229799
12.233543	1034.350357	12.234816
12.494591	1039.328350	12.239834
12.720602	1032.186007	12.244851
12.561013	1032.584999	12.249869
12.562642	1041.917222	12.254887
12.738402	1043.476165	12.259904
12.472522	1044.287348	12.264922
12.614804	1042.176982	12.269939
12.696767	1040.485971	12.274957
12.436871	1037.955920	12.279975
12.737170	1036.903137	12.284992
12.438991	1030.031840	12.290010
12.340540	1015.412175	12.295027
12.535966	1007.214035	12.300045
12.317188	1014.274158	12.305063
12.838354	1014.159335	12.310080
12.751272	1013.169782	12.315098
12.711297	1009.193765	12.320115
12.590298	1010.608665	12.325133
12.454242	1011.296046	12.330151
12.795155	1000.555746	12.335168
12.401747	1010.099075	12.340186
12.354334	1002.443747	12.345203
12.152757	1014.613632	12.350221
12.384298	1032.490608	12.355239
12.784957	1024.425447	12.360256
12.890782	1026.977293	12.365274
12.629646	1026.643770	12.370291
12.897230	1026.491141	12.375309
12.708913	1027.477470	12.380327
12.919917	1014.125562	12.385344
12.595578	1009.356114	12.390362
12.895402	1002.978239	12.395379
12.939221	1001.824360	12.400397
12.934935	1003.258155	12.405415
12.608695	997.870025	12.410432
12.467116	1011.697651	12.415450
12.387420	1008.423762	12.420467
12.544120	1012.460081	12.425485
12.544216	1033.657483	12.430503
13.023853	1031.257940	12.435520
13.083007	1027.862296	12.440538
12.925497	1028.611483	12.445555
13.075901	1019.921442	12.450573
12.764475	1012.763016	12.455591
13.048606	1009.169199	12.460608
12.373282	1006.255117	12.465626
12.428297	1018.674881	12.470643
12.604279	1026.258857	12.475661
12.402962	1032.627427	12.480679
12.670669	1032.606254	12.485696
12.501194	1032.080444	12.490714
12.612773	1037.365378	12.495731
12.932922	1040.590167	12.500749
12.662016	1059.831706	12.505767
13.189474	1067.361556	12.510784
12.730432	1070.105954	12.515802
13.395555	1065.953568	12.520819
13.165679	1062.470070	12.525837
13.053616	1062.749021	12.530855
13.078797	1055.799280	12.535872
12.998699	1049.634147	12.540890
13.068029	1050.860929	12.545907
13.219810	1062.033622	12.550925
13.063088	1059.362127	12.555943
13.023451	1057.418808	12.560960
13.014436	1062.837442	12.565978
12.947183	1063.930913	12.570995
13.101382	1056.171386	12.576013
12.984035	1067.636946	12.581031
13.213613	1066.222675	12.586048
13.045705	1063.004486	12.591066
13.077921	1075.296194	12.596083
13.590065	1066.588467	12.601101
13.304050	1073.093277	12.606119
13.247254	1071.384845	12.611136
13.461236	1072.288949	12.616154
13.083431	1070.912658	12.621171
13.394157	1071.875567	12.626189
13.444638	1071.443506	12.631207
13.277089	1062.908528	12.636224
13.167468	1063.941097	12.641242
13.224263	1071.437721	12.646259
13.653813	1065.088770	12.651277
13.361560	1074.366443	12.656295
13.359782	1072.317668	12.661312
13.343808	1080.964343	12.666330
13.097856	1068.439366	12.671347
13.377397	1066.075246	12.676365
13.353519	1063.158405	12.681383
13.373838	1066.755534	12.686400
13.265480	1069.691155	12.691418
13.342826	1070.224000	12.696435
13.770876	1073.146951	12.701453
13.168127	1069.054304	12.706471
13.778869	1061.095528	12.711488
13.881593	1072.800471	12.716506
13.798205	1070.029269	12.721523
13.893498	1066.272973	12.726541
13.624257	1054.360231	12.731559
13.649730	1039.652358	12.736576
13.796107	1034.201267	12.741594
13.536348	1039.414910	12.746611
13.621551	1030.905100	12.751629
13.254528	1038.002525	12.756647
13.681796	1029.068528	12.761664
13.551943	1031.808905	12.766682
13.504599	1047.905490	12.771699
13.720485	1058.013611	12.776717
13.820759	1074.383815	12.781735
13.860053	1052.729794	12.786752
13.938831	1039.006074	12.791770
13.665417	1035.642950	12.796787
13.885031	1034.695219	12.801805
13.443514	1038.240924	12.806823
13.321395	1031.171463	12.811840
13.604224	1047.366021	12.816858
13.979881	1070.825079	12.821875
13.770597	1065.087331	12.826893
13.634659	1071.321509	12.831911
13.377701	1076.743332	12.836928
13.544982	1060.613983	12.841946
13.341582	1059.321847	12.846963
13.734858	1056.085714	12.851981
13.495413	1068.690576	12.856999
13.428124	1060.931236	12.862016
13.293741	1075.305877	12.867034
13.595068	1098.781985	12.872051
13.665252	1105.394062	12.877069
13.718882	1098.282930	12.882087
13.936777	1098.349504	12.887104
13.987542	1093.033271	12.892122
14.259251	1093.631226	12.897139
14.169451	1103.438370	12.902157
14.323323	1096.175654	12.907175
14.289399	1092.575331	12.912192
14.484480	1087.129951	12.917210
14.172703	1090.678044	12.922227
14.162887	1070.271499	12.927245
14.087632	1072.672988	12.932263
13.679090	1071.424199	12.937280
13.449219	1073.975828	12.942298
13.552187	1079.902853	12.947315
13.981732	1084.378873	12.952333
14.132713	1093.900981	12.957351
13.973106	1096.553781	12.962368
14.290528	1104.232318	12.967386
14.292121	1105.348269	12.972403
14.596137	1085.308677	12.977421
14.117148	1099.183087	12.982439
14.297627	1095.821899	12.987456
14.507986	1088.858271	12.992474
14.299643	1100.460528	12.997491
14.626156	1081.325359	13.002509
14.179362	1092.226377	13.007527
14.127014	1093.637418	13.012544
13.931345	1093.672941	13.017562
13.989057	1104.868493	13.022579
14.490491	1096.169212	13.027597
14.059786	1094.145261	13.032615
14.257296	1090.425996	13.037632
14.325946	1083.142139	13.042650
14.077333	1103.909941	13.047667
14.257693	1099.138939	13.052685
14.247553	1097.355087	13.057703
14.401510	1092.507556	13.062720
14.233775	1088.071600	13.067738
14.363409	1088.904026	13.072755
13.984967	1107.256442	13.077773
14.287181	1123.027858	13.082791
14.178607	1123.745540	13.087808
14.821819	1130.533957	13.092826
14.376392	1127.275014	13.097843
14.715646	1121.280479	13.102861
14.386345	1136.111145	13.107879
14.029783	1134.353046	13.112896
14.219511	1137.336453	13.117914
14.093425	1130.232371	13.122931
14.272501	1127.724237	13.127949
14.153837	1134.822784	13.132967
14.496864	1156.828717	13.137984
14.917979	1154.041246	13.143002
14.737506	1158.088841	13.148019
14.868727	1153.336571	13.153037
14.948803	1146.870756	13.158055
14.936411	1144.045886	13.163072
14.657753	1132.084843	13.168090
14.443051	1140.598471	13.173107
14.401986	1126.506148	13.178125
14.698631	1136.401200	13.183143
14.947597	1146.649365	13.188160
15.066332	1141.093962	13.193178
14.815020	1145.592764	13.198195
14.720297	1130.095335	13.203213
14.807912	1123.976265	13.208231
14.692758	1125.120761	13.213248
15.175025	1130.514917	13.218266
14.787419	1125.214823	13.223283
14.939838	1129.696108	13.228301
14.697535	1129.769844	13.233319
14.610996	1128.273771	13.238336
14.748648	1131.909982	13.243354
14.698447	1152.016805	13.248371
14.680108	1155.339280	13.253389
14.910888	1164.832106	13.258407
14.607674	1169.400507	13.263424
15.261229	1165.927075	13.268442
14.604918	1160.275564	13.273459
14.799114	1161.260492	13.278477
15.038753	1152.240911	13.283495
14.914115	1160.119676	13.288512
15.113751	1152.863148	13.293530
14.905594	1168.000157	13.298547
14.884245	1152.662602	13.303565
14.902374	1150.672724	13.308583
15.146858	1146.400093	13.313600
14.977802	1151.915274	13.318618
15.455558	1173.688367	13.323635
15.244774	1165.449413	13.328653
15.243225	1157.647275	13.333671
15.104634	1153.265726	13.338688
14.955817	1153.564137	13.343706
14.817872	1158.702579	13.348723
15.303710	1172.683716	13.353741
15.351189	1185.707728	13.358759
14.920841	1181.229918	13.363776
15.404376	1183.431421	13.368794
15.230763	1186.627813	13.373811
15.503903	1180.607375	13.378829
15.436828	1181.747668	13.383847
15.159696	1192.603005	13.388864
15.380549	1188.190980	13.393882
15.497342	1181.760810	13.398899
15.385240	1177.325278	13.403917
15.690722	1181.468927	13.408935
15.471213	1189.311029	13.413952
15.694284	1182.492482	13.418970
15.540022	1174.182183	13.423987
15.288542	1156.985285	13.429005
15.085587	1160.105036	13.434023
15.305314	1173.620381	13.439040
15.704567	1183.284561	13.444058
15.049433	1183.798514	13.449075
15.403744	1180.440269	13.454093
15.565167	1193.548199	13.459111
15.329549	1181.583155	13.464128
15.662477	1186.767004	13.469146
15.942838	1180.940818	13.474163
15.476610	1185.336190	13.479181
15.652338	1184.723215	13.484199
15.257871	1182.181328	13.489216
15.884678	1181.386543	13.494234
15.961259	1189.123424	13.499251
15.828923	1182.581492	13.504269
16.236809	1184.573677	13.509287
15.667677	1191.878168	13.514304
15.663274	1185.219832	13.519322
15.445898	1196.192640	13.524339
15.631142	1180.841584	13.529357
15.570353	1181.999734	13.534375
15.751859	1184.400537	13.539392
15.797908	1179.551325	13.544410
15.446633	1182.503492	13.549427
15.538606	1177.417001	13.554445
15.788744	1178.255893	13.559463
15.521664	1189.784864	13.564480
15.838802	1180.404478	13.569498
15.624334	1185.698074	13.574515
15.433159	1192.599407	13.579533
16.221181	1186.749160	13.584551
15.785888	1198.031171	13.589568
15.859817	1181.793912	13.594586
15.656831	1195.455694	13.599603
15.952785	1212.764833	13.604621
16.244959	1211.944255	13.609639
16.029280	1222.889246	13.614656
16.129985	1223.659148	13.619674
16.259811	1219.431621	13.624691
15.683876	1205.870073	13.629709
16.092593	1200.878258	13.634727
15.894993	1209.878792	13.639744
16.241263	1209.481104	13.644762
15.732619	1201.799746	13.649779
16.093081	1209.799721	13.654797
15.926966	1214.040009	13.659815
15.961637	1210.842833	13.664832
16.222759	1204.902313	13.669850
16.373172	1209.881325	13.674867
16.115174	1211.464925	13.679885
16.579859	1203.107044	13.684903
16.452988	1212.458242	13.689920
16.503814	1215.321529	13.694938
16.399612	1213.866157	13.699955
16.511323	1206.231472	13.704973
16.484602	1203.485523	13.709991
16.135433	1210.879050	13.715008
16.207260	1202.598096	13.720026
16.444450	1214.150825	13.725043
16.507326	1207.981685	13.730061
16.703473	1201.878700	13.735079
16.131601	1199.973915	13.740096
16.098544	1198.558552	13.745114
16.628933	1199.119275	13.750131
16.443132	1204.874217	13.755149
16.540116	1207.146688	13.760167
16.390323	1210.195074	13.765184
16.528394	1208.426279	13.770202
16.735977	1208.217825	13.775219
16.246268	1211.924268	13.780237
16.439856	1205.245013	13.785255
16.034945	1202.301754	13.790272
16.365152	1207.158350	13.795290
16.099703	1213.987333	13.800307
16.232640	1212.998804	13.805325
16.389112	1202.117806	13.810343
16.156116	1201.446998	13.815360
16.541589	1225.310912	13.820378
16.640102	1239.263020	13.825395
16.537386	1245.099115	13.830413
16.935706	1246.320161	13.835431
16.766229	1239.428289	13.840448
17.041855	1230.919180	13.845466
16.806028	1237.398247	13.850483
16.767890	1231.910856	13.855501
16.755940	1222.372061	13.860519
16.352936	1223.537954	13.865536
16.650387	1227.445770	13.870554
17.119177	1244.680720	13.875571
16.712257	1256.549540	13.880589
16.835415	1252.565002	13.885607
16.602256	1260.091723	13.890624
16.766486	1248.908269	13.895642
16.854711	1249.183846	13.900659
16.768459	1256.476080	13.905677
16.642244	1254.972380	13.910695
16.846888	1254.445951	13.915712
16.875469	1241.708756	13.920730
16.929123	1245.376392	13.925747
16.803736	1252.797123	13.930765
17.046989	1241.169572	13.935783
17.077408	1249.185728	13.940800
16.830370	1251.340671	13.945818
17.074512	1246.635844	13.950835
16.605139	1241.795815	13.955853
16.868068	1247.432727	13.960871
16.934608	1260.842969	13.965888
17.277396	1281.948063	13.970906
17.379422	1278.172101	13.975923
17.287283	1271.479610	13.980941
17.340174	1255.628375	13.985959
17.373151	1247.681135	13.990976
17.598117	1236.404988	13.995994
17.409308	1240.355177	14.001011
16.909104	1247.553631	14.006029
17.100795	1227.844973	14.011047
17.317313	1244.637230	14.016064
17.148468	1239.650307	14.021082
17.535138	1235.303374	14.026099
16.935975	1241.025669	14.031117
17.539936	1247.815507	14.036135
17.123110	1249.243296	14.041152
17.681867	1261.860485	14.046170
17.393532	1249.285089	14.051187
17.146145	1250.057798	14.056205
17.475890	1259.752999	14.061223
17.440429	1267.386798	14.066240
17.569159	1274.046351	14.071258
17.841108	1272.063325	14.076275
17.621973	1257.068939	14.081293
17.539489	1240.200665	14.086311
17.190312	1242.830888	14.091328
17.162206	1248.863484	14.096346
17.207338	1266.717214	14.101363
17.038140	1276.262035	14.106381
17.507152	1280.756194	14.111399
17.518648	1271.638437	14.116416
17.334571	1275.097762	14.121434
17.430713	1268.785520	14.126451
17.591413	1275.039451	14.131469
17.491767	1273.041661	14.136487
17.504186	1273.976725	14.141504
17.503569	1300.706345	14.146522
17.683247	1295.702159	14.151539
17.198117	1308.371632	14.156557
17.872712	1299.755812	14.161575
17.886556	1296.941339	14.166592
17.676055	1304.490318	14.171610
17.820454	1295.362000	14.176627
17.668005	1292.889927	14.181645
17.768349	1289.117784	14.186663
17.968174	1299.711134	14.191680
17.631875	1306.686297	14.196698
18.155786	1298.937983	14.201715
17.862561	1301.724694	14.206733
17.977875	1292.766517	14.211751
18.032070	1298.796555	14.216768
18.090426	1295.659611	14.221786
18.123069	1299.352973	14.226803
17.790627	1311.615181	14.231821
17.918472	1304.984341	14.236839
17.915471	1297.473279	14.241856
18.070987	1299.811868	14.246874
18.149094	1287.107785	14.251891
18.012378	1291.652840	14.256909
18.331626	1292.441347	14.261927
18.246538	1294.151479	14.266944
18.349955	1292.403950	14.271962
18.348495	1294.963926	14.276979
18.067046	1300.265677	14.281997
17.901212	1291.987341	14.287015
18.391677	1285.611700	14.292032
18.072947	1287.278366	14.297050
18.181368	1286.855226	14.302067
17.924693	1294.700768	14.307085
18.017033	1289.061300	14.312103
18.129644	1285.470768	14.317120
17.915776	1298.439848	14.322138
18.344527	1284.731097	14.327155
18.006717	1313.717152	14.332173
18.558235	1318.219535	14.337191
18.658688	1317.146420	14.342208
18.097277	1327.055850	14.347226
18.541933	1320.423233	14.352243
18.599553	1326.671782	14.357261
18.446780	1321.507396	14.362279
18.202640	1322.767106	14.367296
18.323628	1320.481111	14.372314
18.561416	1327.634606	14.377331
18.894631	1328.257246	14.382349
18.638489	1332.431352	14.387367
18.788342	1322.038897	14.392384
18.276830	1315.191113	14.397402
18.525439	1321.853709	14.402419
18.354616	1325.905657	14.407437
18.404114	1325.693015	14.412455
18.430946	1321.967850	14.417472
18.373490	1314.257932	14.422490
18.707472	1323.896968	14.427507
18.854777	1312.276363	14.432525
18.777975	1317.654524	14.437543
18.955304	1314.938015	14.442560
18.725966	1332.577173	14.447578
19.022540	1320.643349	14.452595
18.824528	1325.492206	14.457613
18.905718	1333.883430	14.462631
19.133111	1322.431842	14.467648
18.595468	1326.227128	14.472666
19.081820	1316.862195	14.477683
18.911187	1325.714658	14.482701
18.548863	1324.403295	14.487719
18.842073	1321.064566	14.492736
18.419719	1318.776246	14.497754
18.868481	1324.692278	14.502771
18.686836	1322.873759	14.507789
18.528058	1320.447013	14.512807
19.331361	1333.136432	14.517824
18.805528	1354.665249	14.522842
19.209736	1353.016216	14.527859
19.237626	1350.551926	14.532877
19.272579	1339.929660	14.537895
18.956766	1320.632857	14.542912
18.826228	1339.991884	14.547930
19.125494	1345.610231	14.552947
19.257869	1350.566288	14.557965
18.959492	1355.112096	14.562983
19.255231	1354.941427	14.568000
18.974103	1353.072817	14.573018
19.062705	1345.145268	14.578035
19.317962	1343.008712	14.583053
19.165390	1344.855576	14.588071
19.491527	1344.752709	14.593088
19.175376	1366.047508	14.598106
19.467870	1349.164584	14.603123
19.453753	1347.044003	14.608141
19.416403	1345.133535	14.613159
19.799795	1337.489317	14.618176
19.510733	1345.732312	14.623194
19.818694	1347.723121	14.628211
19.647974	1331.258058	14.633229
19.038261	1311.599652	14.638247
19.167949	1318.400189	14.643264
19.301291	1337.478433	14.648282
19.434480	1352.971955	14.653299
19.362314	1356.097490	14.658317
19.346926	1357.810873	14.663335
19.457784	1347.017221	14.668352
19.585145	1348.755432	14.673370
19.682800	1343.015669	14.678387
19.623567	1341.815221	14.683405
19.522570	1345.997349	14.688423
19.402594	1345.534600	14.693440
19.323993	1358.092254	14.698458
19.609256	1344.848050	14.703475
19.506546	1343.674469	14.708493
19.610482	1355.775241	14.713511
19.861487	1356.265620	14.718528
19.508771	1376.338289	14.723546
19.706125	1362.367157	14.728563
19.933385	1372.433059	14.733581
19.581710	1369.297136	14.738599
19.846772	1356.758926	14.743616
19.398972	1371.390530	14.748634
19.814912	1363.101437	14.753651
19.613465	1366.154453	14.758669
20.011276	1374.837821	14.763687
20.072070	1368.642979	14.768704
19.851350	1368.132515	14.773722
19.671727	1366.430964	14.778739
19.803218	1371.455078	14.783757
19.767368	1371.724983	14.788775
19.837189	1388.752832	14.793792
20.251481	1401.731565	14.798810
20.447093	1387.222184	14.803827
20.359729	1384.425208	14.808845
19.945302	1379.345769	14.813863
20.498348	1351.959516	14.818880
20.275401	1362.457047	14.823898
20.454882	1363.162566	14.828915
20.261745	1359.030493	14.833933
20.242997	1360.109277	14.838951
20.526189	1359.866676	14.843968
20.253826	1358.076331	14.848986
20.205012	1358.265317	14.854003
20.334827	1350.879506	14.859021
20.225408	1365.276469	14.864039
20.151657	1354.261777	14.869056
20.301607	1359.947318	14.874074
20.052690	1356.352151	14.879091
19.959803	1363.833894	14.884109
20.423065	1387.549396	14.889127
20.512734	1396.136865	14.894144
20.822324	1392.798563	14.899162
20.627013	1382.099374	14.904179
20.504583	1364.359725	14.909197
20.515299	1370.101542	14.914215
20.878576	1361.129117	14.919232
20.367712	1346.610356	14.924250
20.145223	1351.323717	14.929267
20.461327	1372.151885	14.934285
20.451574	1381.550753	14.939303
20.729474	1382.647437	14.944320
20.739329	1390.011833	14.949338
20.733572	1386.358368	14.954355
21.032261	1380.132476	14.959373
20.396439	1381.257730	14.964391
20.379336	1384.933352	14.969408
20.435948	1394.936143	14.974426
20.630514	1397.917424	14.979443
20.534200	1388.004526	14.984461
20.696475	1393.785864	14.989479
20.455982	1389.830681	14.994496
20.645078	1395.373170	14.999514
20.795093	1393.962570	15.004531
21.139342	1395.053802	15.009549
20.669012	1403.734211	15.014567
21.059849	1411.535399	15.019584
21.137896	1417.692234	15.024602
21.176000	1396.570930	15.029619
20.901352	1391.878179	15.034637
20.811497	1390.947910	15.039655
21.152854	1402.782349	15.044672
21.306333	1410.756602	15.049690
21.269038	1399.855129	15.054707
21.617014	1393.391588	15.059725
21.160435	1395.231813	15.064743
21.240438	1391.743876	15.069760
20.951972	1391.764619	15.074778
20.801995	1388.085583	15.079795
21.134667	1384.450001	15.084813
21.079232	1390.535589	15.089831
21.471807	1405.248992	15.094848
21.493632	1398.930476	15.099866
21.075966	1394.300723	15.104883
21.501590	1398.066551	15.109901
21.024441	1408.488026	15.114919
21.030590	1404.926475	15.119936
21.364615	1413.556240	15.124954
20.969394	1414.044961	15.129971
21.536501	1413.076787	15.134989
20.950965	1424.214324	15.140007
21.359729	1422.350581	15.145024
21.391230	1410.597483	15.150042
21.450959	1405.062956	15.155059
21.568103	1411.150343	15.160077
21.053200	1423.105826	15.165095
21.082735	1421.647623	15.170112
21.476437	1425.747039	15.175130
21.775486	1446.335243	15.180147
21.742162	1442.140718	15.185165
21.662892	1447.439814	15.190183
21.922502	1439.668973	15.195200
21.885871	1433.805324	15.200218
21.605960	1420.543639	15.205235
21.757679	1413.370685	15.210253
21.556751	1414.997821	15.215271
21.831316	1431.011691	15.220288
22.044118	1428.313904	15.225306
21.635504	1434.776927	15.230323
21.753442	1423.437632	15.235341
21.635643	1430.491098	15.240359
22.234347	1426.821779	15.245376
22.332892	1428.325617	15.250394
21.635678	1423.209638	15.255411
21.695818	1405.602546	15.260429
21.798522	1428.796076	15.265447
22.314487	1442.652222	15.270464
22.142558	1441.693786	15.275482
21.906833	1419.696753	15.280499
22.213540	1409.596389	15.285517
21.728111	1417.291040	15.290535
21.950675	1428.432423	15.295552
22.241934	1431.877594	15.300570
22.200835	1449.324183	15.305587
22.225855	1443.256075	15.310605
22.011229	1443.368539	15.315623
22.016643	1436.467360	15.320640
21.944826	1436.518237	15.325658
22.250647	1444.938141	15.330675
22.347208	1442.130049	15.335693
22.071068	1455.282364	15.340711
22.212575	1446.725428	15.345728
22.431041	1437.035445	15.350746
22.023227	1444.832032	15.355763
22.285290	1435.889871	15.360781
22.331383	1444.336555	15.365799
21.838104	1446.746953	15.370816
22.046955	1436.356482	15.375834
21.910312	1460.508002	15.380851
22.545743	1462.907056	15.385869
21.971608	1465.989793	15.390887
22.226202	1464.229269	15.395904
22.670504	1461.331822	15.400922
22.331942	1464.721848	15.405939
22.315998	1458.369987	15.410957
22.374621	1458.329435	15.415975
22.442310	1462.366805	15.420992
22.838243	1468.181007	15.426010
22.325957	1463.123223	15.431027
22.618639	1482.225899	15.436045
23.012022	1491.585573	15.441063
22.721410	1472.902843	15.446080
23.049824	1475.087706	15.451098
23.198847	1480.909452	15.456115
22.801746	1459.746215	15.461133
22.949060	1465.931579	15.466151
22.878088	1457.702036	15.471168
23.089357	1461.463150	15.476186
23.097092	1452.318746	15.481203
23.350463	1451.776188	15.486221
22.928967	1461.212638	15.491239
23.021082	1463.869566	15.496256
23.121386	1461.117144	15.501274
23.037413	1461.770744	15.506291
22.910578	1454.201732	15.511309
22.743953	1464.610901	15.516327
22.750856	1453.545019	15.521344
23.046739	1457.302385	15.526362
22.943038	1471.941780	15.531379
22.621871	1458.836664	15.536397
22.967785	1474.905710	15.541415
23.150203	1493.751262	15.546432
23.341023	1491.278133	15.551450
23.286512	1508.051300	15.556467
23.573647	1497.707489	15.561485
23.191580	1494.482282	15.566503
23.313726	1495.219327	15.571520
23.629435	1497.886353	15.576538
23.000105	1485.659992	15.581555
23.449727	1484.247309	15.586573
23.466634	1492.698252	15.591591
23.595537	1492.106192	15.596608
23.723119	1478.879860	15.601626
23.586341	1465.379943	15.606643
23.181392	1462.786596	15.611661
23.430850	1465.311040	15.616679
23.439536	1474.765178	15.621696
23.447171	1477.542552	15.626714
23.099698	1488.387085	15.631731
23.112657	1489.458867	15.636749
23.359357	1497.116221	15.641767
23.170665	1500.561006	15.646784
23.271277	1497.660513	15.651802
23.636495	1491.481843	15.656819
23.251358	1484.954593	15.661837
23.672945	1510.432864	15.666855
23.955424	1517.642834	15.671872
24.011226	1519.650536	15.676890
23.765814	1528.231451	15.681907
24.167075	1521.524041	15.686925
23.854571	1500.696135	15.691943
23.434154	1498.316337	15.696960
24.287205	1506.924156	15.701978
24.255797	1517.322825	15.706995
24.005362	1502.020615	15.712013
24.011756	1496.180143	15.717031
23.708167	1491.430930	15.722048
23.962916	1500.254335	15.727066
23.838062	1514.813811	15.732083
24.255201	1525.085022	15.737101
24.585580	1517.297527	15.742119
23.962122	1498.077124	15.747136
23.923892	1495.590277	15.752154
23.826287	1508.944406	15.757171
24.181762	1522.937368	15.762189
24.373567	1518.018891	15.767207
24.274265	1513.584689	15.772224
24.502867	1511.446611	15.777242
24.532646	1509.938365	15.782259
23.991763	1509.073175	15.787277
24.255934	1510.303224	15.792295
23.961964	1518.972661	15.797312
24.432005	1509.531380	15.802330
24.478016	1513.012766	15.807347
24.157973	1512.514774	15.812365
24.337310	1512.809153	15.817383
24.264693	1527.111810	15.822400
24.513161	1522.550262	15.827418
24.378137	1514.661549	15.832435
24.269878	1511.710935	15.837453
24.630795	1507.280792	15.842471
24.220763	1517.156469	15.847488
24.274785	1516.771444	15.852506
24.240040	1522.682228	15.857523
24.124391	1535.381959	15.862541
24.512446	1542.638857	15.867559
24.370741	1550.282283	15.872576
24.706875	1545.228148	15.877594
24.287969	1545.007878	15.882611
24.536175	1553.885538	15.887629
24.901916	1544.691956	15.892647
24.452616	1550.760026	15.897664
24.765035	1536.784288	15.902682
24.672637	1544.792944	15.907699
24.518264	1564.630742	15.912717
25.030625	1568.054364	15.917735
25.473120	1580.311742	15.922752
25.627928	1551.923746	15.927770
25.368136	1536.479561	15.932787
25.133755	1537.888641	15.937805
25.473903	1533.435154	15.942823
24.907455	1533.762432	15.947840
25.239944	1534.234038	15.952858
24.944873	1542.341138	15.957875
25.703631	1529.365143	15.962893
25.483954	1528.851942	15.967911
25.413546	1534.717843	15.972928
25.367681	1526.302443	15.977946
25.196525	1541.982063	15.982963
25.345612	1536.576602	15.987981
25.278542	1538.657755	15.992999
25.386472	1538.668104	15.998016
25.568709	1527.253350	16.003034
25.367194	1510.039928	16.008051
25.120137	1511.248369	16.013069
25.597316	1525.035023	16.018087
25.226536	1529.196634	16.023104
25.641857	1524.731514	16.028122
25.495167	1526.564239	16.033139
25.242456	1524.888132	16.038157
25.412943	1518.551496	16.043175
25.264296	1524.939514	16.048192
25.627331	1528.119135	16.053210
25.481576	1532.670872	16.058227
25.504594	1532.181337	16.063245
25.766573	1527.191819	16.068263
25.851672	1526.802838	16.073280
25.693941	1531.685256	16.078298
25.685714	1527.001972	16.083315
25.254825	1525.530289	16.088333
25.580808	1512.954525	16.093351
25.465943	1518.739195	16.098368
25.771230	1529.568789	16.103386
25.465869	1538.951846	16.108403
25.385100	1550.335941	16.113421
25.941890	1552.933023	16.118439
25.573984	1560.691187	16.123456
25.849195	1556.331683	16.128474
25.764552	1566.269552	16.133491
25.683409	1564.858361	16.138509
25.969509	1558.952748	16.143527
25.809668	1568.304492	16.148544
25.955944	1558.887357	16.153562
25.954851	1564.390477	16.158579
25.761267	1582.558792	16.163597
26.311137	1588.324966	16.168615
26.547346	1598.206488	16.173632
26.222907	1584.322368	16.178650
26.255907	1590.658350	16.183667
26.339986	1590.224857	16.188685
26.715787	1581.063839	16.193703
26.114660	1563.624497	16.198720
26.163154	1554.438065	16.203738
26.459670	1562.335616	16.208755
26.501643	1574.482032	16.213773
26.547940	1562.262451	16.218791
26.335740	1553.919793	16.223808
26.415382	1554.482587	16.228826
26.594004	1571.768808	16.233843
26.515558	1575.497521	16.238861
26.739380	1562.473496	16.243879
26.687654	1554.029722	16.248896
26.599359	1553.912673	16.253914
26.301499	1554.789789	16.258931
26.434862	1565.256526	16.263949
26.487980	1578.012843	16.268967
26.629265	1593.337572	16.273984
26.375076	1583.082569	16.279002
26.621734	1577.768045	16.284019
26.583246	1589.667169	16.289037
26.518183	1573.437113	16.294055
26.310624	1575.877078	16.299072
26.360911	1583.697037	16.304090
26.665987	1585.623598	16.309107
26.808402	1605.916874	16.314125
26.799103	1613.037523	16.319143
26.840222	1614.706561	16.324160
27.011137	1610.269799	16.329178
27.018035	1613.526595	16.334195
26.798897	1614.740075	16.339213
26.828734	1606.782344	16.344231
26.974995	1609.159514	16.349248
27.550228	1605.453486	16.354266
28.114689	1600.574767	16.359283
27.657689	1602.070439	16.364301
27.907123	1580.783267	16.369319
27.693387	1576.037680	16.374336
27.473096	1583.131575	16.379354
27.681855	1574.164288	16.384371
27.686743	1576.331181	16.389389
27.814612	1568.401752	16.394407
27.887680	1552.521880	16.399424
27.370169	1540.405721	16.404442
27.520311	1531.176918	16.409459
27.333134	1540.907331	16.414477
27.392264	1541.056241	16.419495
27.150653	1534.963465	16.424512
27.590710	1550.606452	16.429530
27.641363	1549.601189	16.434547
27.312714	1554.180794	16.439565
27.726904	1562.889315	16.444583
27.710734	1575.011682	16.449600
27.579890	1570.328966	16.454618
27.808305	1570.072582	16.459635
27.512871	1569.497694	16.464653
27.504785	1562.055052	16.469671
27.322457	1574.619001	16.474688
27.088439	1567.520546	16.479706
27.474986	1568.165286	16.484723
27.054588	1576.877102	16.489741
27.615158	1582.662173	16.494759
27.497207	1591.211628	16.499776
27.498727	1598.164360	16.504794
27.815359	1598.810026	16.509811
27.488838	1603.981746	16.514829
27.844762	1599.810246	16.519847
27.594683	1611.318417	16.524864
27.881709	1631.053638	16.529882
28.158085	1624.297930	16.534899
28.277960	1629.436044	16.539917
28.277540	1632.328544	16.544935
28.274789	1638.116579	16.549952
28.356450	1638.167682	16.554970
28.520003	1628.662619	16.559987
28.400355	1615.922644	16.565005
28.330818	1614.740411	16.570023
28.450879	1599.555204	16.575040
28.163792	1600.012086	16.580058
28.224433	1599.779294	16.585075
27.942843	1607.178375	16.590093
28.346244	1622.691878	16.595111
28.343323	1616.013625	16.600128
28.324459	1617.585107	16.605146
28.829906	1627.047395	16.610163
28.138616	1630.094411	16.615181
28.363704	1626.924927	16.620199
28.518551	1627.748887	16.625216
28.586740	1622.125296	16.630234
28.819750	1620.315374	16.635251
28.457142	1635.307123	16.640269
28.644157	1615.067110	16.645287
28.658116	1624.167358	16.650304
28.627445	1625.496135	16.655322
28.916021	1621.888846	16.660339
28.754012	1630.067103	16.665357
28.724113	1620.363133	16.670375
28.858800	1620.874515	16.675392
28.787731	1623.921979	16.680410
28.755450	1625.144931	16.685427
28.442264	1633.332623	16.690445
28.609227	1637.430199	16.695463
28.777731	1646.828115	16.700480
28.626862	1651.489381	16.705498
29.052771	1655.807331	16.710515
28.808691	1658.223623	16.715533
28.746745	1663.354397	16.720551
28.834156	1661.373277	16.725568
28.927406	1661.044160	16.730586
29.193267	1666.722864	16.735603
29.279946	1690.028281	16.740621
29.545990	1687.796994	16.745639
29.388275	1678.015892	16.750656
29.525804	1665.632153	16.755674
29.346281	1642.765962	16.760691
29.230071	1654.401830	16.765709
29.220638	1652.182019	16.770727
29.551333	1670.654110	16.775744
29.531863	1682.050217	16.780762
29.837448	1674.625364	16.785779
29.546546	1665.907110	16.790797
29.283679	1649.386863	16.795815
29.539153	1645.991709	16.800832
29.661230	1672.290130	16.805850
29.876302	1669.666918	16.810867
29.853582	1678.353227	16.815885
29.474675	1659.818704	16.820903
29.890416	1659.187110	16.825920
29.640624	1669.937880	16.830938
30.000615	1670.746838	16.835955
30.111344	1672.246719	16.840973
29.618660	1658.768048	16.845991
29.596714	1668.508831	16.851008
29.765494	1679.717349	16.856026
30.195545	1667.584450	16.861043
30.158916	1673.166111	16.866061
29.885416	1687.390118	16.871079
30.054308	1670.115896	16.876096
29.918368	1675.696846	16.881114
30.055532	1657.504950	16.886131
29.839907	1669.295628	16.891149
29.978516	1670.864319	16.896167
30.290344	1666.070433	16.901184
30.175023	1671.904048	16.906202
30.014464	1669.930641	16.911219
29.890987	1676.670428	16.916237
30.036639	1675.839595	16.921255
30.342963	1674.295672	16.926272
30.290682	1682.278480	16.931290
30.289036	1673.348858	16.936307
30.248761	1673.640559	16.941325
29.917398	1673.098374	16.946343
30.470869	1681.701868	16.951360
30.258495	1699.063473	16.956378
30.590524	1699.293455	16.961395
30.622483	1706.572863	16.966413
30.532468	1706.830663	16.971431
30.863893	1702.250828	16.976448
30.696343	1692.416426	16.981466
30.903227	1685.340913	16.986483
30.521039	1686.727390	16.991501
30.694341	1685.359367	16.996519
31.015643	1681.483497	17.001536
30.826256	1689.466331	17.006554
30.671106	1683.750504	17.011571
31.013997	1685.974340	17.016589
30.660380	1687.654685	17.021607
31.246275	1683.082995	17.026624
30.775080	1700.028957	17.031642
30.991543	1689.892739	17.036659
30.758504	1695.936544	17.041677
30.766682	1695.664000	17.046695
31.168693	1678.937205	17.051712
30.698249	1696.017473	17.056730
31.066909	1692.919909	17.061747
31.106619	1696.090405	17.066765
31.227495	1697.806698	17.071783
31.319757	1687.840595	17.076800
31.117930	1681.586873	17.081818
31.316547	1683.219656	17.086835
30.884439	1689.616792	17.091853
30.905041	1691.516763	17.096871
31.125088	1691.220033	17.101888
31.083257	1712.955556	17.106906
31.468698	1707.337768	17.111923
31.799145	1712.512365	17.116941
31.618444	1724.194765	17.121959
31.732070	1722.262056	17.126976
31.760436	1713.989388	17.131994
31.724664	1689.004912	17.137011
31.677823	1683.973079	17.142029
31.409751	1681.060847	17.147047
31.670526	1686.499480	17.152064
31.474432	1714.823370	17.157082
31.825808	1718.827706	17.162099
31.874427	1713.908225	17.167117
31.507611	1712.996739	17.172135
31.839732	1711.817013	17.177152
31.683443	1717.370242	17.182170
32.216167	1724.968439	17.187187
32.048755	1713.968967	17.192205
31.973651	1715.811536	17.197223
32.444490	1710.284742	17.202240
32.337849	1712.190783	17.207258
31.977221	1699.675582	17.212275
32.058637	1709.006833	17.217293
32.087840	1709.327010	17.222311
32.600916	1702.795905	17.227328
32.067737	1689.899230	17.232346
31.669647	1689.607414	17.237363
32.232762	1700.150258	17.242381
32.200699	1709.948639	17.247399
32.262118	1713.311592	17.252416
32.119882	1716.340523	17.257434
32.321203	1711.651883	17.262451
32.205868	1712.414996	17.267469
31.890031	1719.837701	17.272487
32.361994	1712.607752	17.277504
32.244256	1710.649702	17.282522
32.384382	1708.968690	17.287539
32.417675	1709.136633	17.292557
32.249648	1714.339279	17.297575
32.434856	1720.703306	17.302592
32.426656	1728.702277	17.307610
32.568765	1725.926563	17.312627
32.513026	1737.556831	17.317645
32.646377	1739.460417	17.322663
32.769709	1733.957383	17.327680
32.773812	1729.997318	17.332698
32.686893	1729.699154	17.337715
32.724514	1743.987732	17.342733
32.824167	1738.094950	17.347751
32.718173	1730.432013	17.352768
32.626274	1741.813562	17.357786
32.757444	1737.796674	17.362803
32.876219	1743.651271	17.367821
33.302878	1734.442786	17.372839
34.373457	1725.948087	17.377856
33.725993	1726.183058	17.382874
33.443964	1726.278319	17.387891
33.850945	1715.709855	17.392909
33.554099	1703.261858	17.397927
33.747661	1696.651483	17.402944
33.472806	1693.512638	17.407962
33.866495	1687.814566	17.412979
33.937375	1673.344424	17.417997
33.686349	1687.865866	17.423015
33.629949	1689.045176	17.428032
33.680120	1685.909309	17.433050
34.004645	1687.339417	17.438067
33.782464	1669.608223	17.443085
33.249669	1658.987442	17.448103
33.887819	1660.833188	17.453120
33.799335	1660.677001	17.458138
33.547045	1651.662839	17.463155
33.723332	1648.958058	17.468173
33.303065	1651.084798	17.473191
33.391807	1663.633353	17.478208
33.493678	1678.239366	17.483226
33.521937	1674.265088	17.488243
33.701558	1680.505824	17.493261
33.376608	1687.098023	17.498279
33.928330	1678.327517	17.503296
33.434074	1687.255514	17.508314
33.754355	1695.113975	17.513331
33.959074	1698.324322	17.518349
33.648929	1709.205355	17.523367
34.113635	1710.433776	17.528384
34.035697	1704.161932	17.533402
34.070293	1710.627214	17.538419
34.440425	1706.583837	17.543437
34.038948	1706.959634	17.548455
34.101850	1699.805950	17.553472
34.212873	1702.773934	17.558490
34.326127	1707.134315	17.563507
34.475542	1706.969520	17.568525
34.146513	1716.240663	17.573543
34.298249	1712.241246	17.578560
34.317770	1708.462478	17.583578
34.107297	1712.439789	17.588595
34.454331	1720.485553	17.593613
34.489160	1739.324697	17.598631
34.590270	1733.452737	17.603648
34.860833	1734.567391	17.608666
34.285341	1751.412547	17.613683
34.536950	1738.614663	17.618701
34.684563	1734.818263	17.623719
34.498576	1732.871488	17.628736
34.569442	1726.057974	17.633754
34.350340	1738.655100	17.638771
34.889583	1726.526352	17.643789
34.570589	1733.316975	17.648807
34.599065	1732.830271	17.653824
34.642340	1748.098328	17.658842
34.831690	1766.323645	17.663859
34.999136	1763.655340	17.668877
34.843566	1768.750248	17.673895
34.882957	1767.632080	17.678912
34.849333	1766.115784	17.683930
34.874851	1768.838686	17.688947
35.240575	1770.838902	17.693965
34.733776	1762.181072	17.698983
34.809087	1772.811464	17.704000
35.219644	1776.237590	17.709018
35.480746	1789.460449	17.714035
35.425491	1782.222915	17.719053
35.233861	1792.960813	17.724071
35.579664	1793.015310	17.729088
35.569204	1785.033440	17.734106
35.619201	1800.296107	17.739123
35.650077	1780.903249	17.744141
35.560634	1779.973282	17.749159
35.568428	1793.007515	17.754176
35.607737	1787.880121	17.759194
35.732085	1784.021813	17.764211
35.647600	1772.715121	17.769229
35.541687	1788.468650	17.774247
35.572363	1784.966928	17.779264
35.525869	1787.043532	17.784282
35.420948	1788.566661	17.789299
35.853193	1784.266567	17.794317
36.021510	1789.823655	17.799335
36.062356	1793.502002	17.804352
36.250222	1785.981992	17.809370
35.869010	1786.507577	17.814387
36.327219	1794.407660	17.819405
36.093251	1806.618754	17.824423
36.148169	1794.702454	17.829440
36.661228	1796.167946	17.834458
35.910899	1792.858859	17.839475
36.042358	1787.134997	17.844493
36.126250	1807.988746	17.849511
36.123943	1814.377501	17.854528
36.406658	1818.397342	17.859546
36.225940	1818.644545	17.864563
36.227107	1801.953939	17.869581
36.261180	1810.486464	17.874599
35.995004	1814.551147	17.879616
36.510118	1805.585655	17.884634
36.278627	1813.090520	17.889651
36.241593	1815.467700	17.894669
36.521672	1833.980633	17.899687
36.577837	1847.852701	17.904704
36.886868	1843.816039	17.909722
36.822847	1847.632779	17.914739
37.076502	1825.696210	17.919757
37.060640	1836.396629	17.924775
36.926927	1839.868029	17.929792
37.023897	1837.089717	17.934810
37.087184	1846.533682	17.939827
36.842247	1832.095897	17.944845
37.142501	1834.996026	17.949863
37.123491	1824.379392	17.954880
37.508495	1835.034037	17.959898
36.953185	1828.604241	17.964915
37.205875	1808.129720	17.969933
36.868293	1806.490832	17.974951
36.733421	1820.943208	17.979968
37.236040	1822.323822	17.984986
36.990096	1832.636121	17.990003
37.243763	1834.224197	17.995021
37.026427	1838.731756	18.000039
37.439560	1840.487950	18.005056
37.224323	1824.318663	18.010074
36.794125	1827.797524	18.015091
37.072222	1843.271924	18.020109
37.596150	1857.860326	18.025127
37.514205	1872.610274	18.030144
37.941168	1853.095972	18.035162
38.154587	1862.856247	18.040179
37.812868	1858.574789	18.045197
37.654901	1855.208151	18.050215
37.618521	1859.455717	18.055232
37.961724	1859.003607	18.060250
37.858784	1852.433108	18.065267
37.718006	1852.291859	18.070285
37.913377	1859.490600	18.075303
38.091365	1870.441068	18.080320
38.092918	1852.210729	18.085338
38.046998	1850.235085	18.090355
38.103219	1854.160093	18.095373
38.070548	1857.879736	18.100391
37.904367	1859.639940	18.105408
38.106712	1853.728373	18.110426
37.786629	1852.296607	18.115443
38.245248	1853.539627	18.120461
38.047008	1850.745535	18.125479
37.928975	1854.635172	18.130496
38.150320	1865.747944	18.135514
38.180005	1882.202516	18.140531
38.244154	1883.659136	18.145549
38.630077	1880.200056	18.150567
38.622607	1869.277969	18.155584
38.486607	1870.485800	18.160602
38.450170	1876.410580	18.165619
38.300921	1878.285891	18.170637
38.610626	1874.188486	18.175655
38.298628	1881.819472	18.180672
38.406335	1875.500348	18.185690
38.462682	1887.188576	18.190707
38.914588	1895.423579	18.195725
38.861384	1894.621463	18.200743
38.859395	1899.255642	18.205760
39.000214	1900.668494	18.210778
38.778991	1896.108871	18.215795
38.696407	1888.600633	18.220813
38.983618	1896.633937	18.225831
38.918683	1898.970470	18.230848
39.090682	1900.225822	18.235866
39.303957	1893.981362	18.240883
39.217558	1901.797301	18.245901
39.382827	1899.888710	18.250919
39.355172	1905.552035	18.255936
39.483960	1908.333677	18.260954
39.606807	1897.527621	18.265971
39.013574	1903.369636	18.270989
39.448537	1903.237369	18.276007
39.382441	1904.469277	18.281024
39.485376	1902.517842	18.286042
39.840431	1921.653470	18.291059
39.893284	1907.777175	18.296077
40.115678	1906.806298	18.301095
39.639469	1904.905688	18.306112
39.683725	1898.647035	18.311130
39.543154	1904.552030	18.316147
39.494466	1894.678568	18.321165
39.871656	1897.139067	18.326183
39.405111	1902.549162	18.331200
39.557245	1921.814771	18.336218
39.638047	1933.673190	18.341235
39.807665	1944.265087	18.346253
39.886986	1931.644123	18.351271
39.829996	1929.896655	18.356288
40.161890	1929.404486	18.361306
40.228801	1926.360874	18.366323
40.235248	1932.210289	18.371341
40.005272	1929.139366	18.376359
40.002560	1935.824077	18.381376
40.033834	1940.007537	18.386394
40.492462	1957.472310	18.391411
40.496424	1967.405046	18.396429
40.520149	1962.030192	18.401447
40.399205	1961.420746	18.406464
40.667594	1954.071781	18.411482
40.560839	1960.597137	18.416499
40.501909	1959.560354	18.421517
40.548310	1954.505742	18.426535
40.738371	1958.302371	18.431552
40.859435	1952.426833	18.436570
40.804886	1956.525474	18.441587
40.779189	1957.948133	18.446605
40.779935	1946.667186	18.451623
40.699158	1961.235153	18.456640
41.056468	1959.460159	18.461658
40.851054	1954.169035	18.466675
40.438773	1965.801311	18.471693
40.798497	1955.277302	18.476711
40.740875	1967.531029	18.481728
40.904211	1951.692124	18.486746
40.996021	1974.551299	18.491763
41.420169	1973.950585	18.496781
41.732770	1981.063089	18.501799
41.503272	1982.991237	18.506816
41.495757	1961.955430	18.511834
41.001967	1958.690520	18.516851
40.853928	1963.820070	18.521869
40.982945	1974.526956	18.526887
41.018942	1980.146526	18.531904
40.824755	1976.296126	18.536922
40.972644	1994.359682	18.541939
41.363394	2004.912324	18.546957
41.477719	2007.340105	18.551975
41.634158	2000.677867	18.556992
42.055041	1995.483806	18.562010
41.964243	2002.644872	18.567027
42.000060	2005.991256	18.572045
42.242005	1998.626563	18.577063
41.819335	2001.178905	18.582080
41.987834	2008.061122	18.587098
41.818613	2006.468006	18.592115
41.651958	1998.124272	18.597133
42.090391	2001.017346	18.602151
42.120901	2002.859621	18.607168
41.862193	1996.231541	18.612186
42.110866	1998.716248	18.617203
42.253918	2001.523106	18.622221
42.121587	1999.392838	18.627239
42.248159	2002.035899	18.632256
42.418976	1997.134517	18.637274
42.159188	1999.140697	18.642291
42.504983	1997.639232	18.647309
42.530535	1996.812089	18.652327
42.245898	2000.200600	18.657344
42.439711	2018.678606	18.662362
42.702758	2016.882178	18.667379
42.790868	2027.534449	18.672397
42.739734	2036.319741	18.677415
42.393646	2027.189571	18.682432
42.897992	2027.570399	18.687450
43.041016	2024.692915	18.692467
42.716834	2036.456145	18.697485
43.130765	2031.936786	18.702503
42.549664	2020.649188	18.707520
42.956352	2024.239578	18.712538
42.907326	2029.512224	18.717555
43.173375	2030.487107	18.722573
43.222226	2024.584896	18.727591
43.227096	2031.234146	18.732608
43.011836	2021.448950	18.737626
43.384254	2023.834085	18.742643
43.059043	2013.611984	18.747661
43.369492	2018.262674	18.752679
43.140789	2015.164360	18.757696
43.266395	2026.270826	18.762714
43.430138	2021.272583	18.767731
43.332658	2026.785891	18.772749
43.342139	2020.722092	18.777767
43.425215	2020.230490	18.782784
43.311541	2042.326744	18.787802
43.971506	2037.583867	18.792819
43.827521	2050.883733	18.797837
43.854700	2037.730793	18.802855
43.981794	2056.763327	18.807872
43.824212	2041.351346	18.812890
44.143177	2040.099959	18.817907
43.877573	2043.279447	18.822925
43.840715	2041.251497	18.827943
44.180042	2040.009342	18.832960
44.408683	2046.761176	18.837978
44.129094	2042.815039	18.842995
44.172147	2047.288093	18.848013
44.111229	2045.126729	18.853031
44.080594	2041.623467	18.858048
44.240048	2039.942178	18.863066
44.549513	2047.995899	18.868083
44.193845	2048.283825	18.873101
44.287648	2048.719505	18.878119
44.176834	2036.575112	18.883136
44.186948	2038.143227	18.888154
44.327364	2045.581826	18.893171
44.178197	2051.462118	18.898189
44.243267	2044.527385	18.903207
44.254412	2070.940283	18.908224
44.316342	2076.081627	18.913242
44.825760	2075.785887	18.918259
44.728814	2083.987684	18.923277
44.961534	2078.198560	18.928295
44.878907	2070.431798	18.933312
45.045649	2089.207447	18.938330
45.086105	2076.299111	18.943347
44.713323	2081.200901	18.948365
44.769046	2064.568510	18.953383
45.045312	2059.293610	18.958400
44.922146	2071.590531	18.963418
44.919942	2077.186136	18.968435
44.889483	2093.141466	18.973453
45.595363	2087.881186	18.978471
45.207480	2088.617313	18.983488
45.148952	2092.060008	18.988506
45.597676	2074.602293	18.993523
45.547954	2086.019838	18.998541
45.813017	2084.995447	19.003559
45.616377	2095.988299	19.008576
45.372791	2095.392027	19.013594
45.677174	2089.514292	19.018611
45.418359	2080.812938	19.023629
45.471073	2079.875602	19.028647
45.582044	2078.162561	19.033664
45.627651	2090.537110	19.038682
46.001089	2091.704668	19.043699
45.968785	2093.592173	19.048717
45.757987	2083.404855	19.053735
45.757193	2087.817652	19.058752
45.594263	2089.414957	19.063770
45.906086	2105.034626	19.068787
45.934852	2129.564550	19.073805
46.132683	2125.097605	19.078823
46.241979	2121.787720	19.083840
45.889928	2118.817634	19.088858
45.899360	2115.372886	19.093875
46.000163	2122.066948	19.098893
46.181200	2125.548009	19.103911
46.321475	2146.565324	19.108928
46.280544	2155.161611	19.113946
46.545065	2154.323905	19.118963
46.442737	2156.999503	19.123981
46.732065	2138.619311	19.128999
47.034342	2135.618647	19.134016
46.950046	2149.150053	19.139034
47.130334	2144.222652	19.144051
47.411526	2140.081271	19.149069
47.557389	2130.999459	19.154087
47.203270	2113.661180	19.159104
47.247935	2106.783330	19.164122
47.147007	2103.201717	19.169139
47.176021	2104.131136	19.174157
47.074139	2104.538136	19.179175
47.157221	2100.540517	19.184192
46.621323	2103.146229	19.189210
47.508934	2105.706851	19.194227
47.068054	2105.286082	19.199245
47.172567	2122.904829	19.204263
47.423644	2127.485054	19.209280
47.195031	2130.287217	19.214298
47.621442	2126.919613	19.219315
47.348355	2123.611700	19.224333
47.742033	2130.386491	19.229351
47.627832	2131.642900	19.234368
47.458426	2135.094676	19.239386
47.836057	2129.595342	19.244403
47.348134	2132.685218	19.249421
47.299197	2131.775699	19.254439
47.829491	2128.815894	19.259456
47.724459	2135.587476	19.264474
47.777867	2154.596483	19.269491
47.532558	2155.016360	19.274509
47.742632	2167.954495	19.279527
48.380203	2161.217799	19.284544
48.264987	2164.329156	19.289562
47.952822	2160.732636	19.294579
47.998887	2161.280925	19.299597
48.185242	2163.070499	19.304615
48.300214	2160.069683	19.309632
47.934102	2158.036092	19.314650
48.528563	2156.803732	19.319667
48.651628	2167.630230	19.324685
47.978300	2162.106538	19.329703
48.299678	2173.438810	19.334720
47.932604	2186.223534	19.339738
48.390475	2184.189200	19.344755
48.416671	2191.933140	19.349773
48.418166	2185.242887	19.354791
48.624739	2183.762836	19.359808
48.544844	2198.579090	19.364826
48.729363	2202.516252	19.369843
49.107153	2220.324972	19.374861
48.899756	2217.704360	19.379879
49.319474	2206.347297	19.384896
49.122137	2210.754421	19.389914
49.454213	2210.016564	19.394931
49.630978	2214.566973	19.399949
49.325414	2215.282416	19.404967
49.602056	2190.360454	19.409984
49.022909	2186.260647	19.415002
49.595584	2197.998621	19.420019
49.551710	2202.462858	19.425037
49.680227	2201.212420	19.430055
49.659989	2198.180204	19.435072
49.496866	2194.335639	19.440090
49.891840	2182.612041	19.445107
49.519413	2186.640839	19.450125
49.745023	2201.814061	19.455143
50.032867	2207.962724	19.460160
49.479680	2194.433740	19.465178
49.731888	2201.761232	19.470195
49.743787	2208.259605	19.475213
49.815160	2202.597877	19.480231
50.010531	2195.183902	19.485248
49.865992	2209.314444	19.490266
49.693213	2199.738043	19.495283
49.645163	2197.485168	19.500301
49.541408	2224.590100	19.505319
49.722437	2229.680320	19.510336
49.683357	2232.607074	19.515354
50.386161	2234.900445	19.520371
50.058013	2246.289517	19.525389
50.485026	2265.882547	19.530407
51.161749	2255.201235	19.535424
51.119733	2259.393546	19.540442
50.723434	2236.909908	19.545459
50.735230	2224.157158	19.550477
50.620194	2219.674962	19.555495
50.949955	2221.812275	19.560512
51.029717	2225.075269	19.565530
50.734205	2221.055936	19.570547
51.250481	2215.489963	19.575565
50.943989	2215.061549	19.580583
50.897197	2224.265098	19.585600
50.845526	2232.269348	19.590618
51.249456	2242.932763	19.595635
50.961323	2244.595258	19.600653
51.000502	2250.805697	19.605671
51.365001	2247.399483	19.610688
51.446960	2250.833170	19.615706
51.553115	2252.285639	19.620723
51.807087	2250.899711	19.625741
51.752892	2250.956142	19.630759
51.796172	2243.953075	19.635776
51.506927	2246.980814	19.640794
51.755137	2240.325746	19.645811
51.814873	2246.887289	19.650829
51.636270	2250.267583	19.655847
51.599454	2241.808567	19.660864
52.110084	2237.164713	19.665882
52.152608	2239.580383	19.670899
51.857724	2239.378380	19.675917
51.686689	2249.109918	19.680935
52.018331	2242.036564	19.685952
51.734979	2238.998807	19.690970
52.131593	2236.570485	19.695987
51.808598	2234.100458	19.701005
51.975429	2244.161960	19.706023
52.303499	2244.091644	19.711040
52.076606	2244.915339	19.716058
52.191931	2254.109634	19.721075
52.363635	2263.152502	19.726093
52.234352	2271.664444	19.731111
52.360152	2269.124187	19.736128
52.374903	2277.665871	19.741146
52.301924	2268.957322	19.746163
52.550096	2263.633654	19.751181
52.539393	2264.608620	19.756199
52.478981	2265.811863	19.761216
52.655512	2286.629888	19.766234
52.529939	2285.702515	19.771251
52.616671	2284.769584	19.776269
52.493444	2294.286373	19.781287
52.984028	2292.339331	19.786304
52.526470	2302.531606	19.791322
52.778765	2307.506932	19.796339
52.971606	2315.385393	19.801357
53.304444	2323.366897	19.806375
53.467630	2322.089856	19.811392
53.515608	2327.377280	19.816410
53.637793	2320.135958	19.821427
53.594923	2314.803874	19.826445
53.317181	2319.489455	19.831463
53.681919	2326.227386	19.836480
53.397949	2325.076989	19.841498
53.725392	2327.552866	19.846515
53.774577	2313.830542	19.851533
53.496873	2318.456869	19.856551
53.986713	2334.504804	19.861568
54.106847	2350.415633	19.866586
54.137819	2350.925283	19.871603
54.402772	2352.314515	19.876621
54.116504	2350.189953	19.881639
54.255883	2349.350083	19.886656
54.360603	2352.979822	19.891674
54.471039	2361.312840	19.896691
54.857597	2332.768192	19.901709
54.115649	2315.679981	19.906727
54.431667	2316.697017	19.911744
54.443082	2314.384695	19.916762
54.429322	2337.171110	19.921779
54.485715	2342.436875	19.926797
54.401291	2343.112631	19.931815
54.793529	2347.959341	19.936832
54.675236	2345.862530	19.941850
54.634130	2344.857616	19.946867
54.828929	2342.455541	19.951885
54.686688	2338.463601	19.956903
54.809605	2342.203512	19.961920
54.924874	2341.623712	19.966938
54.742237	2345.066304	19.971955
54.900673	2344.942923	19.976973
54.589712	2368.774888	19.981991
55.185111	2369.022973	19.987008
55.292283	2373.074725	19.992026
54.878142	2381.744226	19.997043
55.249512	2372.394905	20.002061
55.179427	2376.161796	20.007079
55.440281	2370.402559	20.012096
55.181941	2370.502763	20.017114
55.223011	2383.394012	20.022131
55.485921	2392.654743	20.027149
55.388305	2408.863607	20.032167
55.564066	2415.901096	20.037184
55.699240	2406.797859	20.042202
55.904350	2399.592400	20.047219
55.965643	2383.752594	20.052237
55.962920	2394.908286	20.057255
55.636246	2402.137450	20.062272
55.830619	2401.337305	20.067290
56.144313	2425.288759	20.072307
56.173912	2424.696933	20.077325
56.037460	2426.250135	20.082343
56.281082	2420.511049	20.087360
56.605246	2421.599576	20.092378
56.608292	2426.877924	20.097395
56.822930	2418.600868	20.102413
56.649913	2413.192034	20.107431
56.898192	2403.262284	20.112448
57.146595	2412.235679	20.117466
56.807270	2401.401910	20.122483
56.891154	2392.059928	20.127501
56.827028	2389.024297	20.132519
57.063079	2397.940280	20.137536
56.983073	2397.011471	20.142554
56.825984	2409.468587	20.147571
56.906375	2418.782329	20.152589
56.774057	2418.524327	20.157607
57.108057	2409.165806	20.162624
57.131853	2417.686192	20.167642
57.295253	2412.909126	20.172659
57.028726	2410.136844	20.177677
57.257781	2415.016840	20.182695
57.225051	2407.683367	20.187712
57.348559	2412.441442	20.192730
57.180303	2430.044593	20.197747
57.023482	2443.685085	20.202765
57.469490	2449.479972	20.207783
57.191416	2455.294913	20.212800
57.348701	2451.191247	20.217818
57.457381	2466.324803	20.222835
58.073357	2463.410224	20.227853
57.646805	2466.374282	20.232871
57.602040	2469.638615	20.237888
57.983299	2470.133887	20.242906
57.870860	2463.936329	20.247923
57.727209	2468.120887	20.252941
57.805784	2494.187165	20.257959
58.289444	2490.981471	20.262976
58.330344	2494.587146	20.267994
58.137036	2500.827835	20.273011
58.296327	2496.231727	20.278029
58.481070	2487.118677	20.283047
58.875436	2475.075095	20.288064
59.046011	2480.429710	20.293082
59.147288	2479.098520	20.298099
59.346528	2468.384751	20.303117
59.159302	2472.727684	20.308135
59.046956	2464.479047	20.313152
59.296654	2454.632096	20.318170
58.817569	2465.914192	20.323187
59.481950	2456.165634	20.328205
59.571609	2467.348630	20.333223
59.275502	2477.253331	20.338240
59.554637	2467.986907	20.343258
59.178361	2465.405181	20.348275
59.487130	2459.284077	20.353293
59.405489	2468.784457	20.358311
59.208344	2469.383969	20.363328
59.438965	2470.622989	20.368346
59.527616	2470.923320	20.373363
59.692256	2464.588249	20.378381
59.230346	2466.710560	20.383399
59.482179	2474.946459	20.388416
59.348304	2472.590016	20.393434
59.048640	2481.203256	20.398451
59.651719	2500.383260	20.403469
59.796376	2497.600099	20.408487
59.894965	2496.525243	20.413504
59.902676	2505.234546	20.418522
59.915890	2503.061655	20.423539
59.842800	2512.651982	20.428557
60.234308	2517.988604	20.433575
60.270106	2519.779085	20.438592
60.759236	2514.977294	20.443610
60.789414	2518.602461	20.448627
60.606306	2520.520843	20.453645
60.723637	2521.595528	20.458663
60.780854	2534.524390	20.463680
61.405382	2515.487605	20.468698
61.070627	2503.762900	20.473715
61.086718	2505.185004	20.478733
61.065000	2490.394181	20.483751
60.580340	2492.934011	20.488768
60.866203	2500.521818	20.493786
60.878129	2516.844969	20.498803
61.002766	2516.077995	20.503821
61.136500	2510.117677	20.508839
61.069012	2516.629298	20.513856
61.364556	2515.595119	20.518874
61.073671	2518.538736	20.523891
61.042804	2520.790603	20.528909
61.151119	2529.480539	20.533927
60.968776	2534.694289	20.538944
61.437232	2537.357321	20.543962
61.321668	2550.208847	20.548979
61.218703	2546.199734	20.553997
61.694369	2560.849140	20.559015
61.697628	2570.577667	20.564032
61.980133	2566.073770	20.569050
61.907455	2578.219844	20.574067
62.061928	2570.748278	20.579085
62.142787	2563.447533	20.584103
61.991141	2575.604292	20.589120
62.320376	2566.482672	20.594138
62.372718	2564.843830	20.599155
62.361785	2559.482959	20.604173
62.863143	2555.893246	20.609191
62.736321	2559.391619	20.614208
62.936964	2569.149335	20.619226
62.912787	2563.174542	20.624243
62.779248	2553.621947	20.629261
63.033630	2548.140470	20.634279
62.918978	2556.745619	20.639296
62.988488	2551.050609	20.644314
62.946127	2558.943850	20.649331
63.204872	2557.988580	20.654349
63.362128	2554.574620	20.659367
63.293056	2550.757532	20.664384
63.248878	2558.221961	20.669402
63.115926	2558.916375	20.674419
63.331713	2563.549017	20.679437
63.173185	2563.220939	20.684455
63.241596	2558.236308	20.689472
63.420626	2554.604980	20.694490
63.349464	2561.589644	20.699507
63.394614	2563.529758	20.704525
63.697434	2560.070877	20.709543
63.158753	2576.037856	20.714560
63.243741	2584.437992	20.719578
63.635626	2587.623503	20.724595
63.843876	2581.722494	20.729613
64.193955	2584.933810	20.734631
63.474983	2596.923717	20.739648
63.742958	2599.167943	20.744666
63.942090	2614.399684	20.749683
64.082189	2616.936291	20.754701
64.153059	2621.907843	20.759719
63.957917	2626.145045	20.764736
63.914370	2623.107542	20.769754
63.944275	2638.919607	20.774771
64.454507	2649.254927	20.779789
64.585193	2648.235778	20.784807
64.311272	2648.375564	20.789824
64.817657	2649.268650	20.794842
64.597643	2652.370652	20.799859
64.559485	2656.122099	20.804877
65.216427	2654.497902	20.809895
64.450020	2660.714859	20.814912
65.005005	2668.792899	20.819930
64.944864	2677.533982	20.824947
65.502006	2668.345509	20.829965
65.541910	2672.825760	20.834983
65.584776	2675.681186	20.840000
65.935725	2670.580149	20.845018
65.654724	2676.035435	20.850035
65.826889	2667.537323	20.855053
66.128844	2664.758059	20.860071
65.951822	2648.537302	20.865088
66.181891	2635.353871	20.870106
66.025651	2637.602064	20.875123
65.738379	2629.329885	20.880141
66.133140	2624.667664	20.885159
65.497759	2627.724131	20.890176
65.898627	2639.581775	20.895194
66.021191	2654.689602	20.900211
65.956751	2668.034330	20.905229
66.148006	2664.339543	20.910247
65.941998	2667.217589	20.915264
66.151889	2658.514437	20.920282
66.356588	2661.815538	20.925299
65.951274	2661.843184	20.930317
66.439415	2679.248785	20.935335
66.459608	2685.593633	20.940352
66.440699	2689.135617	20.945370
66.282364	2690.739310	20.950387
66.428808	2700.530474	20.955405
67.061335	2707.907955	20.960423
67.034507	2726.312447	20.965440
66.967410	2719.180954	20.970458
66.979338	2722.774541	20.975475
66.924503	2715.838259	20.980493
66.942479	2717.588403	20.985511
67.035922	2722.725542	20.990528
67.361997	2712.041432	20.995546
67.439951	2719.328284	21.000563
67.325252	2719.409477	21.005581
67.864295	2725.882374	21.010599
67.667853	2720.946575	21.015616
67.626817	2721.102206	21.020634
67.394639	2729.583176	21.025651
67.318342	2740.527663	21.030669
67.829245	2736.498553	21.035687
67.527992	2743.995710	21.040704
68.192294	2740.782950	21.045722
68.143361	2737.950637	21.050739
68.201465	2745.402586	21.055757
68.432296	2731.705581	21.060775
68.418068	2746.610126	21.065792
68.124978	2741.738320	21.070810
68.383112	2739.811920	21.075827
68.576808	2749.288233	21.080845
69.165722	2750.528304	21.085863
69.141113	2742.659887	21.090880
69.019310	2721.363203	21.095898
69.238813	2722.922179	21.100915
68.724207	2726.569705	21.105933
69.494973	2708.427773	21.110951
69.276499	2712.369260	21.115968
69.368394	2714.444183	21.120986
69.460818	2715.400955	21.126003
69.015811	2713.189978	21.131021
69.348981	2717.536352	21.136039
69.118602	2722.013251	21.141056
68.924182	2709.238864	21.146074
68.818416	2720.283477	21.151091
69.341258	2739.856552	21.156109
69.184378	2747.205449	21.161127
69.327930	2760.746587	21.166144
69.304531	2750.407196	21.171162
69.588590	2748.979641	21.176179
69.434797	2773.288401	21.181197
69.885443	2769.561749	21.186215
69.809058	2780.955868	21.191232
70.043803	2778.833335	21.196250
69.970024	2779.915997	21.201267
69.781678	2773.844633	21.206285
70.049206	2792.054898	21.211303
70.049535	2802.722997	21.216320
69.940674	2804.775202	21.221338
70.620391	2800.176862	21.226355
70.589242	2807.308561	21.231373
70.586934	2790.789503	21.236391
70.390389	2792.367238	21.241408
70.649755	2807.034906	21.246426
70.922297	2823.697585	21.251443
71.048765	2834.486195	21.256461
71.236071	2815.145716	21.261479
71.413533	2815.175482	21.266496
71.444078	2810.291512	21.271514
71.708958	2810.243843	21.276531
71.836240	2817.572981	21.281549
72.106220	2796.433887	21.286567
71.788585	2786.102150	21.291584
71.472902	2783.631612	21.296602
71.510291	2784.606931	21.301619
71.440397	2778.846294	21.306637
71.578752	2779.579347	21.311655
71.629962	2785.388027	21.316672
72.047009	2791.847255	21.321690
71.968788	2793.613304	21.326707
71.725996	2810.528442	21.331725
72.243775	2797.375281	21.336743
72.010820	2807.021733	21.341760
71.827039	2797.532799	21.346778
71.932393	2797.355592	21.351795
72.085068	2801.531429	21.356813
72.036659	2809.038803	21.361831
72.770206	2830.765680	21.366848
72.607062	2833.282355	21.371866
72.525367	2826.946111	21.376883
72.523638	2842.323863	21.381901
72.870975	2836.034826	21.386919
72.706155	2838.225806	21.391936
72.469613	2841.216406	21.396954
72.320450	2822.550001	21.401971
72.603200	2840.614112	21.406989
72.887910	2849.027057	21.412007
72.925602	2858.452053	21.417024
72.878346	2858.485489	21.422042
73.366204	2855.032187	21.427059
73.162631	2863.434883	21.432077
73.536673	2860.599974	21.437095
73.929847	2882.554423	21.442112
73.480548	2886.190800	21.447130
73.943802	2875.152031	21.452147
73.706614	2882.936690	21.457165
73.833434	2875.375456	21.462183
73.364731	2882.001952	21.467200
73.872823	2895.306991	21.472218
74.082863	2881.938871	21.477235
74.139953	2875.975724	21.482253
74.034934	2875.065192	21.487271
73.914531	2883.462817	21.492288
73.947937	2902.883912	21.497306
74.135294	2906.063919	21.502323
74.106301	2909.927296	21.507341
74.347741	2904.987975	21.512359
74.834795	2918.352414	21.517376
74.682988	2937.419522	21.522394
74.899820	2924.580937	21.527411
74.891781	2932.335236	21.532429
75.068422	2932.342304	21.537447
75.504570	2929.921912	21.542464
75.357372	2935.003219	21.547482
75.742282	2925.254097	21.552499
75.644177	2920.868502	21.557517
75.886621	2936.686695	21.562535
75.732457	2924.319640	21.567552
75.434840	2906.557167	21.572570
75.852738	2918.423630	21.577587
75.849964	2925.838482	21.582605
75.940028	2913.510604	21.587623
76.085029	2918.181821	21.592640
76.316190	2921.821903	21.597658
75.852308	2902.994419	21.602675
76.148967	2916.223000	21.607693
75.868826	2917.167336	21.612711
75.774293	2917.868014	21.617728
75.735182	2933.244554	21.622746
75.586136	2921.713640	21.627763
75.777896	2938.910250	21.632781
75.920779	2960.155795	21.637799
76.248202	2954.455813	21.642816
76.175555	2957.000073	21.647834
76.384348	2969.709768	21.652851
76.491695	2991.020282	21.657869
76.659609	2988.024140	21.662887
76.828005	2976.341914	21.667904
76.680859	2981.979907	21.672922
77.144310	2978.611318	21.677939
77.366040	3003.861512	21.682957
77.179583	3003.188440	21.687975
77.813606	3001.998695	21.692992
78.041355	3001.901652	21.698010
77.953223	2986.220170	21.703027
77.866438	2981.228371	21.708045
77.592588	2970.089689	21.713063
77.961646	2972.273961	21.718080
77.563547	2965.780894	21.723098
77.883078	2968.543413	21.728115
78.012961	2970.029825	21.733133
77.848171	2964.849352	21.738151
78.158922	2959.277317	21.743168
77.936542	2981.530469	21.748186
78.077328	2988.772814	21.753203
78.251473	3000.202858	21.758221
78.114099	2998.670515	21.763239
78.458462	2990.859108	21.768256
78.175367	2987.363492	21.773274
78.699744	2979.516440	21.778291
78.672378	2994.279697	21.783309
78.864142	2996.518072	21.788327
79.174774	3002.266250	21.793344
79.127152	3001.260008	21.798362
79.246710	3000.889904	21.803379
79.163220	3000.767915	21.808397
79.168565	3009.883001	21.813415
79.577491	3009.265085	21.818432
79.430767	3013.940838	21.823450
79.264298	3013.848701	21.828467
79.383502	3019.106089	21.833485
79.741082	3017.367943	21.838503
79.933131	3013.767428	21.843520
79.549260	3020.395319	21.848538
79.649215	3016.949388	21.853555
79.815565	3013.145645	21.858573
79.620796	3004.060752	21.863591
79.886582	3008.070715	21.868608
79.822519	3034.837836	21.873626
80.057940	3033.939936	21.878643
80.163999	3049.568187	21.883661
79.851568	3045.964808	21.888679
79.942583	3038.564133	21.893696
79.938106	3066.698206	21.898714
80.088355	3075.834267	21.903731
80.216306	3074.521847	21.908749
80.266349	3087.830697	21.913767
80.946163	3098.743011	21.918784
80.592625	3106.505671	21.923802
80.885118	3097.101628	21.928819
81.362769	3089.100434	21.933837
81.228300	3094.617478	21.938855
81.590077	3093.527044	21.943872
81.192697	3098.341877	21.948890
81.899243	3091.669765	21.953907
82.052176	3096.423583	21.958925
81.729787	3093.582849	21.963943
81.440561	3088.865014	21.968960
81.766308	3098.133110	21.973978
81.622859	3095.616345	21.978995
81.919148	3111.330939	21.984013
81.530218	3118.298284	21.989031
81.736485	3118.615413	21.994048
81.755559	3120.613449	21.999066
81.904518	3126.614764	22.004083
81.909225	3144.651948	22.009101
81.959137	3150.841684	22.014119
82.202491	3150.974735	22.019136
82.102632	3152.741250	22.024154
82.017987	3154.685170	22.029171
82.479008	3178.251248	22.034189
82.792263	3184.491968	22.039207
82.735924	3178.870673	22.044224
82.666285	3179.080641	22.049242
82.933855	3174.029439	22.054259
83.520439	3167.739317	22.059277
83.282664	3171.619543	22.064295
83.734875	3170.670458	22.069312
83.180210	3175.753427	22.074330
83.471593	3177.267109	22.079347
83.429680	3173.654431	22.084365
83.634629	3178.519756	22.089383
83.846486	3192.011009	22.094400
83.751879	3200.773830	22.099418
83.726183	3196.138794	22.104435
83.851156	3192.660738	22.109453
84.049570	3191.516584	22.114471
84.287900	3198.949206	22.119488
84.140998	3197.842035	22.124506
84.044429	3187.619953	22.129523
84.030655	3185.288436	22.134541
84.050932	3204.238854	22.139559
83.859557	3221.827039	22.144576
84.252360	3226.562519	22.149594
84.065861	3227.851632	22.154611
84.484540	3242.706378	22.159629
84.634436	3255.884306	22.164647
84.831513	3248.810884	22.169664
84.941876	3246.149792	22.174682
84.759408	3252.785838	22.179699
85.288021	3277.377898	22.184717
85.062408	3282.556528	22.189735
85.573728	3282.114595	22.194752
85.509974	3291.864096	22.199770
86.147965	3281.846555	22.204787
85.937658	3273.699106	22.209805
85.887751	3287.925426	22.214823
86.100839	3272.506870	22.219840
86.243441	3275.418367	22.224858
85.997925	3283.701843	22.229875
86.497004	3274.760799	22.234893
86.185676	3275.196137	22.239911
86.279866	3271.263311	22.244928
86.289816	3276.266400	22.249946
86.220874	3267.462922	22.254963
86.250698	3272.267058	22.259981
86.188509	3269.460853	22.264999
86.606834	3284.542469	22.270016
86.633351	3299.767977	22.275034
86.694122	3304.780788	22.280051
86.858286	3300.480487	22.285069
86.991920	3305.523778	22.290087
87.031850	3295.652691	22.295104
86.818395	3297.681299	22.300122
87.241446	3324.062523	22.305139
87.451967	3322.402187	22.310157
86.819886	3329.562954	22.315175
87.299071	3326.583029	22.320192
87.241212	3334.082376	22.325210
87.802548	3344.429405	22.330227
87.894980	3355.891325	22.335245
87.711165	3352.152841	22.340263
88.308779	3356.227354	22.345280
88.224996	3357.178244	22.350298
87.982197	3356.885726	22.355315
88.301698	3348.268014	22.360333
87.933428	3366.872206	22.365351
88.381175	3353.928968	22.370368
88.337952	3358.665280	22.375386
88.386970	3375.759191	22.380403
88.771143	3382.765833	22.385421
88.590772	3391.628760	22.390439
88.904504	3380.934815	22.395456
89.104676	3376.817520	22.400474
89.124534	3379.855618	22.405491
89.424471	3369.379315	22.410509
89.165126	3371.557641	22.415527
89.070264	3372.746583	22.420544
89.072800	3363.842262	22.425562
89.200487	3364.213327	22.430579
89.598193	3365.358671	22.435597
89.721179	3390.993135	22.440615
89.929547	3390.689451	22.445632
90.145095	3394.145216	22.450650
89.883171	3402.776349	22.455667
90.086646	3393.974241	22.460685
89.780630	3394.943351	22.465703
90.075473	3387.095442	22.470720
90.291583	3394.474350	22.475738
89.818820	3405.908834	22.480755
90.068813	3408.093947	22.485773
90.268296	3434.618995	22.490791
90.259674	3423.844034	22.495808
90.209958	3427.279073	22.500826
90.491062	3430.699998	22.505843
90.920471	3440.143297	22.510861
90.812616	3456.243135	22.515879
91.279024	3453.547190	22.520896
91.060710	3455.291580	22.525914
90.934954	3445.686360	22.530931
91.282223	3447.515245	22.535949
91.351326	3456.137772	22.540967
91.196641	3471.587485	22.545984
91.591923	3485.322308	22.551002
91.431641	3489.839419	22.556019
91.627855	3489.813727	22.561037
91.720608	3488.381104	22.566055
91.808495	3485.092184	22.571072
92.377907	3494.047811	22.576090
92.096856	3504.602256	22.581107
92.639793	3507.846861	22.586125
92.412959	3511.995837	22.591143
92.814978	3500.889186	22.596160
92.506337	3501.053217	22.601178
92.439254	3504.386417	22.606195
92.727149	3510.254292	22.611213
92.644356	3507.474284	22.616231
92.591628	3500.513286	22.621248
92.721098	3518.238554	22.626266
92.782791	3532.996268	22.631283
93.293221	3525.347314	22.636301
93.644409	3531.748052	22.641319
93.411628	3533.449959	22.646336
93.418202	3534.976093	22.651354
93.649667	3538.509182	22.656371
93.574759	3525.056098	22.661389
93.639037	3544.808331	22.666407
93.809363	3557.915422	22.671424
93.954602	3550.476409	22.676442
93.771106	3568.521169	22.681459
94.150611	3564.797819	22.686477
94.119849	3549.697240	22.691495
94.486350	3558.357690	22.696512
94.467283	3561.180993	22.701530
94.013477	3568.698635	22.706547
94.367893	3579.121353	22.711565
94.553656	3588.888865	22.716583
94.629630	3587.103095	22.721600
94.453602	3587.468052	22.726618
94.568199	3591.448425	22.731635
95.003361	3597.918779	22.736653
95.087927	3607.303019	22.741671
95.101382	3607.631548	22.746688
95.083992	3604.413149	22.751706
95.217792	3605.076915	22.756723
95.304131	3596.497989	22.761741
95.421411	3599.596805	22.766759
95.530430	3628.579690	22.771776
95.803610	3628.744827	22.776794
95.813199	3641.614765	22.781811
95.939785	3623.613653	22.786829
96.047552	3628.396752	22.791847
96.174672	3632.180968	22.796864
96.128203	3629.738642	22.801882
96.174418	3639.945789	22.806899
96.413675	3644.091406	22.811917
96.448456	3649.980293	22.816935
96.269182	3655.260052	22.821952
96.467689	3657.816313	22.826970
96.757008	3665.038368	22.831987
96.948222	3680.872480	22.837005
97.003506	3689.432064	22.842023
97.309841	3678.830084	22.847040
97.762857	3675.765442	22.852058
97.583731	3679.544760	22.857075
97.532181	3674.615421	22.862093
97.652482	3673.457763	22.867111
97.653912	3670.365771	22.872128
98.024088	3659.150487	22.877146
97.743893	3663.620532	22.882163
97.858575	3674.477030	22.887181
98.208485	3673.918845	22.892199
97.945982	3671.950408	22.897216
98.365097	3684.290498	22.902234
98.317694	3687.398827	22.907251
98.265085	3691.711585	22.912269
98.381439	3693.989296	22.917287
98.292264	3709.150068	22.922304
98.772188	3690.461345	22.927322
98.609226	3701.892886	22.932339
98.563454	3715.579137	22.937357
98.765105	3721.968048	22.942375
98.401930	3729.953873	22.947392
99.202691	3729.906634	22.952410
98.668620	3751.764348	22.957427
99.250867	3756.585622	22.962445
99.295950	3753.550968	22.967463
99.668085	3750.192582	22.972480
100.005527	3737.023154	22.977498
100.139845	3744.228338	22.982515
100.170885	3746.239438	22.987533
100.275478	3727.829625	22.992551
100.328474	3748.450144	22.997568
100.681852	3743.599152	23.002586
100.438205	3739.152333	23.007603
100.969583	3746.901765	23.012621
100.931067	3730.816834	23.017639
100.941408	3730.135226	23.022656
101.089608	3717.582531	23.027674
101.030269	3720.315271	23.032691
101.160501	3706.342294	23.037709
101.193146	3716.424566	23.042727
101.320197	3717.138272	23.047744
101.500380	3714.368317	23.052762
101.269053	3729.125423	23.057779
101.222288	3739.223587	23.062797
101.737223	3737.200695	23.067815
101.594426	3751.492001	23.072832
101.704395	3746.896982	23.077850
101.791376	3751.671743	23.082867
101.919379	3755.399543	23.087885
101.966598	3751.674756	23.092903
101.645861	3761.548513	23.097920
101.826488	3748.239630	23.102938
101.872803	3764.343839	23.107955
102.050359	3779.558640	23.112973
102.213987	3772.274754	23.117991
102.073301	3788.141377	23.123008
102.173055	3798.069301	23.128026
102.413258	3803.022702	23.133043
102.486970	3804.351543	23.138061
102.844072	3808.187566	23.143079
103.067699	3825.845263	23.148096
103.286914	3830.137947	23.153114
103.453940	3840.621335	23.158131
103.301932	3833.858095	23.163149
103.118831	3833.785235	23.168167
103.544064	3834.330381	23.173184
103.477817	3845.618877	23.178202
103.675984	3862.707576	23.183219
103.710941	3864.195587	23.188237
103.689947	3866.434599	23.193255
103.693210	3872.023649	23.198272
104.074050	3886.362416	23.203290
104.044132	3885.255550	23.208307
104.244016	3888.922683	23.213325
104.633949	3892.351321	23.218343
104.928746	3915.484161	23.223360
105.187362	3919.916822	23.228378
105.510633	3918.686235	23.233395
105.216288	3904.792687	23.238413
105.371175	3885.931841	23.243431
105.032532	3900.328088	23.248448
105.445666	3896.932580	23.253466
105.599664	3900.425009	23.258483
105.652048	3912.746744	23.263501
105.343102	3899.015067	23.268519
105.423955	3904.165703	23.273536
105.574670	3912.633261	23.278554
105.461736	3926.867429	23.283571
105.800724	3930.467491	23.288589
105.801559	3921.912751	23.293607
105.930005	3931.974213	23.298624
106.141919	3954.974346	23.303642
106.583342	3966.646383	23.308659
106.523161	3967.151660	23.313677
106.415842	3968.420661	23.318695
106.556139	3971.985845	23.323712
106.570781	3978.476239	23.328730
106.999025	3988.793724	23.333747
107.318919	3991.730393	23.338765
107.293770	3983.396851	23.343783
107.371207	3987.360236	23.348800
107.621551	3969.957197	23.353818
107.704782	3970.234044	23.358835
107.386272	3982.763189	23.363853
107.770188	3989.592585	23.368871
108.211195	4010.812355	23.373888
108.169676	4012.640983	23.378906
108.523671	4003.697119	23.383923
108.291718	4006.339923	23.388941
108.629105	4007.283466	23.393959
108.666161	4004.637901	23.398976
107.997434	4008.001329	23.403994
108.274470	4002.674270	23.409011
108.150535	4004.928737	23.414029
108.551516	4007.546093	23.419047
108.122824	4026.923291	23.424064
108.688736	4035.856977	23.429082
108.516443	4039.769117	23.434099
108.807729	4064.731186	23.439117
108.967749	4061.332978	23.444135
109.546683	4061.681468	23.449152
109.200015	4057.033066	23.454170
109.648400	4068.990263	23.459187
109.841008	4073.825232	23.464205
110.345602	4075.415984	23.469223
110.262359	4080.625291	23.474240
110.156067	4080.972435	23.479258
110.381899	4076.208562	23.484275
110.058998	4077.876990	23.489293
110.758644	4076.753893	23.494311
110.638722	4082.474403	23.499328
110.731467	4088.072368	23.504346
110.682535	4082.353454	23.509363
110.719226	4100.312049	23.514381
110.946954	4102.543463	23.519399
110.933798	4118.051538	23.524416
111.150509	4112.785199	23.529434
111.148049	4115.268834	23.534451
110.926465	4133.706386	23.539469
111.348033	4132.514268	23.544487
111.339405	4143.387533	23.549504
111.402696	4147.462751	23.554522
111.917013	4150.242516	23.559539
112.020766	4167.807805	23.564557
111.969872	4170.790422	23.569575
112.094641	4173.064057	23.574592
112.300219	4173.847097	23.579610
112.507427	4167.069240	23.584627
112.407599	4181.491642	23.589645
112.691745	4188.955361	23.594663
112.716994	4203.564608	23.599680
113.050019	4210.811981	23.604698
113.289576	4197.671334	23.609715
112.794514	4200.461982	23.614733
113.205767	4198.355373	23.619751
113.183064	4219.096509	23.624768
113.382488	4230.797709	23.629786
113.608195	4235.141404	23.634803
113.393530	4240.544144	23.639821
113.601299	4235.463898	23.644839
113.788472	4254.588423	23.649856
113.796789	4253.475606	23.654874
114.089111	4256.830292	23.659891
113.904341	4265.951543	23.664909
114.212300	4272.033335	23.669927
113.996607	4291.086670	23.674944
114.288268	4285.896083	23.679962
114.701074	4275.075702	23.684979
114.702462	4294.963696	23.689997
114.821001	4290.446634	23.695015
115.666017	4282.988893	23.700032
115.559305	4297.652711	23.705050
116.315124	4294.528861	23.710067
115.606810	4300.532119	23.715085
115.788889	4293.640242	23.720103
116.108317	4296.354593	23.725120
116.120511	4297.642457	23.730138
116.604124	4298.904790	23.735155
116.310880	4291.587488	23.740173
116.176200	4265.235001	23.745191
116.381732	4266.414140	23.750208
116.373251	4263.378395	23.755226
116.444797	4271.498973	23.760243
116.228437	4285.829697	23.765261
116.309487	4292.919521	23.770279
116.509945	4290.647326	23.775296
116.210505	4295.582567	23.780314
116.349162	4319.788329	23.785331
116.235849	4336.813657	23.790349
116.399208	4350.010369	23.795367
116.846419	4361.868767	23.800384
116.971052	4366.899323	23.805402
117.366920	4379.843848	23.810419
117.261200	4398.414939	23.815437
117.170666	4402.888895	23.820455
117.510730	4419.855935	23.825472
117.192431	4425.671952	23.830490
117.860277	4410.072399	23.835507
117.544820	4432.588293	23.840525
118.238576	4451.259643	23.845543
118.123925	4448.667026	23.850560
118.381222	4463.406688	23.855578
118.752966	4464.206778	23.860595
118.631939	4467.455389	23.865613
118.681401	4465.114018	23.870631
119.125692	4476.949364	23.875648
119.190966	4499.350077	23.880666
119.596648	4492.976717	23.885683
119.461161	4492.668016	23.890701
119.565474	4495.706945	23.895719
119.892265	4494.596215	23.900736
119.712364	4504.290070	23.905754
120.768598	4496.413836	23.910771
120.769934	4501.104152	23.915789
121.223802	4484.431534	23.920807
121.107432	4482.530977	23.925824
121.131047	4483.385049	23.930842
121.301918	4474.066030	23.935859
121.096654	4487.491103	23.940877
121.079072	4485.830540	23.945895
121.259441	4474.854320	23.950912
121.075697	4482.410062	23.955930
121.417467	4477.069783	23.960947
121.484776	4478.563925	23.965965
121.225165	4496.348299	23.970983
121.300830	4488.046650	23.976000
121.291871	4491.146424	23.981018
121.625733	4499.381268	23.986035
121.516194	4515.776200	23.991053
121.737441	4527.213761	23.996071
121.951743	4539.625781	24.001088
121.749203	4541.600377	24.006106
121.856394	4536.459482	24.011123
122.104807	4555.437240	24.016141
122.010108	4571.310840	24.021159
122.387657	4574.787744	24.026176
122.343595	4592.242098	24.031194
122.658772	4596.640803	24.036211
122.746890	4612.761818	24.041229
123.315705	4622.467081	24.046247
123.562104	4623.810769	24.051264
123.489595	4622.932165	24.056282
123.970523	4627.021971	24.061299
123.763714	4625.913175	24.066317
123.541396	4629.203756	24.071335
123.958003	4630.165747	24.076352
123.726334	4644.440269	24.081370
123.852968	4648.995350	24.086387
124.038964	4663.556022	24.091405
123.878742	4665.706728	24.096423
124.479723	4683.658587	24.101440
124.237378	4689.599958	24.106458
124.287313	4690.363858	24.111475
124.503518	4702.761124	24.116493
124.731160	4718.520976	24.121511
124.942856	4722.154857	24.126528
124.916472	4723.644424	24.131546
125.234168	4727.737211	24.136563
125.315895	4737.945509	24.141581
125.339429	4748.791438	24.146599
126.319001	4741.897129	24.151616
126.379907	4740.681878	24.156634
126.670547	4721.473549	24.161651
126.693475	4734.190991	24.166669
126.334622	4728.214755	24.171687
126.557283	4729.561193	24.176704
126.294145	4739.309108	24.181722
126.868396	4749.710465	24.186739
126.987379	4757.903386	24.191757
126.946231	4750.568230	24.196775
127.263604	4756.110026	24.201792
126.754216	4773.857239	24.206810
126.901590	4763.226457	24.211827
127.295187	4771.690180	24.216845
127.337464	4776.419094	24.221863
127.442343	4784.018636	24.226880
127.454707	4801.283175	24.231898
127.827130	4801.723690	24.236915
128.095769	4814.898675	24.241933
128.222557	4816.042045	24.246951
128.407506	4820.100487	24.251968
128.412692	4847.287272	24.256986
128.964579	4840.973086	24.262003
128.832897	4835.525467	24.267021
128.802444	4845.726385	24.272039
129.121226	4847.229803	24.277056
128.795321	4843.844388	24.282074
129.253363	4856.851486	24.287091
129.238567	4865.292574	24.292109
129.352608	4866.970783	24.297127
129.713274	4869.633930	24.302144
129.814976	4877.592345	24.307162
130.169199	4888.109687	24.312179
129.976852	4893.086873	24.317197
130.187175	4899.448063	24.322215
130.047244	4893.765149	24.327232
130.131052	4897.322163	24.332250
130.544633	4912.762876	24.337267
130.748250	4924.192618	24.342285
130.975567	4929.953314	24.347303
131.276403	4922.366667	24.352320
131.196972	4920.191816	24.357338
131.126139	4928.229165	24.362355
131.706044	4924.995272	24.367373
131.532083	4942.858528	24.372391
131.991718	4930.544769	24.377408
132.098475	4942.305915	24.382426
132.290025	4939.552766	24.387443
132.397740	4942.542397	24.392461
132.462300	4934.202580	24.397479
132.180905	4924.804070	24.402496
132.293735	4939.779494	24.407514
132.608638	4942.395091	24.412531
132.707910	4942.897676	24.417549
132.830288	4963.142551	24.422567
132.856003	4962.090989	24.427584
132.739156	4967.903843	24.432602
133.009730	4969.246323	24.437619
133.004925	4964.459654	24.442637
132.879152	4993.664601	24.447655
132.989777	4988.743486	24.452672
133.316390	4998.130307	24.457690
133.259389	5018.313938	24.462707
133.653166	5031.303057	24.467725
133.666770	5026.317638	24.472743
134.127490	5044.518705	24.477760
134.290534	5067.452956	24.482778
134.345823	5057.244322	24.487795
134.529827	5049.376099	24.492813
134.457017	5058.496242	24.497831
135.044078	5067.039982	24.502848
134.871639	5084.819675	24.507866
134.993664	5075.679648	24.512883
135.392741	5077.461586	24.517901
135.044742	5084.933328	24.522919
135.673532	5101.878603	24.527936
135.568602	5107.777344	24.532954
135.622787	5120.888012	24.537971
135.881043	5108.114027	24.542989
136.207528	5129.163280	24.548007
136.407896	5137.250029	24.553024
136.375100	5131.899366	24.558042
136.470430	5128.827794	24.563059
136.896062	5133.992742	24.568077
136.792220	5137.604835	24.573095
137.000421	5155.470549	24.578112
137.111103	5158.744016	24.583130
137.237512	5157.607684	24.588147
137.321131	5149.042530	24.593165
137.495632	5160.034685	24.598183
137.753073	5174.602930	24.603200
137.895082	5184.528693	24.608218
137.661046	5180.714590	24.613235
138.312830	5183.528531	24.618253
137.988267	5186.995195	24.623271
138.669805	5201.392590	24.628288
138.741573	5218.425701	24.633306
138.560957	5224.713415	24.638323
139.060492	5214.048945	24.643341
138.683551	5217.610107	24.648359
139.056462	5213.847694	24.653376
139.130556	5223.855185	24.658394
139.166389	5239.625995	24.663411
139.416409	5248.251120	24.668429
139.289923	5241.285388	24.673447
139.023006	5242.083951	24.678464
139.522710	5257.587558	24.683482
139.404227	5277.013478	24.688499
140.246582	5279.507724	24.693517
139.893313	5308.318904	24.698535
140.089974	5298.471053	24.703552
140.156129	5306.501317	24.708570
140.578066	5317.597204	24.713587
141.147985	5319.995511	24.718605
140.806435	5332.001912	24.723623
140.915921	5339.001282	24.728640
141.489071	5333.641384	24.733658
141.760451	5341.742887	24.738675
142.077165	5335.912696	24.743693
141.953178	5337.572011	24.748711
142.282617	5333.791159	24.753728
142.225269	5336.986508	24.758746
142.363528	5349.098705	24.763763
142.391232	5334.847871	24.768781
142.282919	5336.953078	24.773799
142.246575	5340.158738	24.778816
142.244830	5344.741536	24.783834
142.465698	5363.801610	24.788851
142.866032	5361.796668	24.793869
142.944722	5371.846019	24.798887
142.816762	5381.115637	24.803904
143.202850	5392.737648	24.808922
143.197427	5400.029295	24.813939
143.272777	5398.266654	24.818957
143.498657	5414.190908	24.823975
143.737599	5431.017075	24.828992
143.851174	5433.416384	24.834010
143.790990	5446.639148	24.839027
144.435683	5458.005062	24.844045
144.822339	5454.447436	24.849063
145.071353	5451.240945	24.854080
145.244912	5454.122931	24.859098
144.998869	5462.118234	24.864115
145.305874	5456.682963	24.869133
145.459815	5454.907331	24.874151
145.438115	5472.216432	24.879168
145.369137	5476.478049	24.884186
145.592314	5486.952086	24.889203
145.642531	5479.975950	24.894221
145.867983	5487.958723	24.899239
145.951414	5506.106907	24.904256
146.217860	5504.823773	24.909274
145.997872	5520.455614	24.914291
146.509732	5531.263136	24.919309
146.645528	5542.656105	24.924327
146.683573	5541.390232	24.929344
147.000095	5538.729732	24.934362
147.358394	5557.772847	24.939379
147.456675	5581.437945	24.944397
147.458863	5566.373284	24.949415
147.709902	5566.790175	24.954432
147.771362	5561.245025	24.959450
147.596017	5563.988985	24.964467
147.388568	5581.631304	24.969485
147.798025	5595.746810	24.974503
147.858178	5613.193745	24.979520
148.313847	5630.196946	24.984538
148.697553	5642.583426	24.989555
148.846579	5623.747051	24.994573
148.621522	5643.552110	24.999591
148.685253	5659.397484	25.004608
148.825710	5670.098729	25.009626
148.980822	5684.382344	25.014643
149.534674	5684.427108	25.019661
149.776722	5688.283795	25.024679
150.190502	5686.307305	25.029696
150.238414	5678.369902	25.034714
150.365442	5702.733687	25.039731
150.837295	5696.499721	25.044749
150.835931	5714.194763	25.049767
151.016376	5714.930456	25.054784
151.129345	5688.329107	25.059802
151.190385	5693.928557	25.064819
151.008197	5699.394944	25.069837
150.910871	5702.034290	25.074855
151.021938	5708.559477	25.079872
151.424466	5723.001489	25.084890
151.120656	5725.866325	25.089907
151.597275	5726.422352	25.094925
151.744129	5747.171360	25.099943
151.729423	5760.250632	25.104960
152.267496	5766.388704	25.109978
151.902172	5774.586580	25.114995
152.309402	5779.679183	25.120013
152.385160	5788.128644	25.125031
152.575669	5792.719182	25.130048
152.721154	5805.994893	25.135066
152.661111	5826.004842	25.140083
153.102893	5826.183892	25.145101
153.700582	5810.767805	25.150119
153.571806	5821.260844	25.155136
154.071188	5822.994402	25.160154
154.201109	5840.752948	25.165171
154.267768	5829.244089	25.170189
154.142636	5839.945232	25.175207
154.265033	5840.768487	25.180224
154.489982	5834.568963	25.185242
154.249012	5860.008131	25.190259
154.657366	5869.772979	25.195277
154.589610	5875.997809	25.200295
154.621905	5886.630445	25.205312
154.936747	5896.090237	25.210330
154.983778	5911.136920	25.215347
155.145728	5925.575556	25.220365
155.607371	5928.463581	25.225383
155.372415	5940.650110	25.230400
156.032629	5939.394414	25.235418
155.814834	5954.549473	25.240435
156.392456	5948.540492	25.245453
156.788251	5959.832921	25.250471
156.983080	5979.216604	25.255488
156.931073	5970.174116	25.260506
157.325757	5975.509842	25.265523
157.555043	5974.842755	25.270541
157.709712	5970.070775	25.275559
157.270207	5977.943949	25.280576
157.740892	5981.786557	25.285594
158.011061	6001.316112	25.290611
157.959299	6004.318909	25.295629
158.275369	6001.421360	25.300647
157.983404	6000.964830	25.305664
158.581929	6018.694189	25.310682
158.354725	6039.185650	25.315699
158.882804	6042.989651	25.320717
159.221464	6028.471417	25.325735
158.802877	6033.616288	25.330752
159.307808	6038.110056	25.335770
159.128508	6052.877682	25.340787
159.296661	6064.926822	25.345805
159.513133	6080.813537	25.350823
159.643147	6093.024933	25.355840
160.042363	6080.998656	25.360858
159.898697	6089.212047	25.365875
160.233685	6108.914523	25.370893
160.658133	6114.693489	25.375911
160.714141	6115.188299	25.380928
161.110916	6111.638700	25.385946
161.163309	6119.839401	25.390963
161.319808	6129.810622	25.395981
161.201121	6131.694380	25.400999
161.144300	6136.311710	25.406016
161.637290	6128.344642	25.411034
161.452060	6157.823829	25.416051
162.048052	6156.804754	25.421069
162.184609	6152.738199	25.426087
161.788548	6170.543074	25.431104
162.201303	6172.713110	25.436122
162.498613	6188.700771	25.441139
162.121056	6199.480882	25.446157
162.807016	6210.198680	25.451175
163.127674	6215.008827	25.456192
163.686746	6208.171954	25.461210
164.150650	6207.352686	25.466227
164.473369	6215.411902	25.471245
164.446116	6210.887271	25.476263
164.357511	6206.987064	25.481280
164.626972	6196.724188	25.486298
164.445719	6204.572916	25.491315
164.441396	6201.918855	25.496333
164.431499	6203.571222	25.501351
164.644419	6218.801064	25.506368
164.720649	6226.227663	25.511386
164.752629	6237.339417	25.516403
165.146818	6240.270149	25.521421
165.078019	6248.070392	25.526439
164.931452	6264.493744	25.531456
165.233921	6269.807006	25.536474
165.263654	6283.687395	25.541491
165.520912	6300.511865	25.546509
165.733218	6303.301764	25.551527
165.748041	6337.227027	25.556544
165.795005	6337.417768	25.561562
165.889627	6357.094905	25.566579
166.378562	6370.257642	25.571597
166.807095	6383.561891	25.576615
166.970362	6399.207278	25.581632
167.321670	6408.851155	25.586650
167.677746	6409.681509	25.591667
167.464829	6422.518438	25.596685
167.889313	6413.306396	25.601703
168.238412	6429.803170	25.606720
168.126832	6437.149854	25.611738
168.391735	6448.447725	25.616755
168.322959	6453.982264	25.621773
168.749751	6448.917884	25.626791
168.950667	6467.062337	25.631808
169.399370	6469.558037	25.636826
169.412983	6473.795251	25.641843
169.693233	6472.032106	25.646861
169.762525	6476.601921	25.651879
169.635714	6482.508336	25.656896
170.074978	6498.033401	25.661914
170.019469	6504.798296	25.666931
170.196778	6503.948400	25.671949
170.542271	6501.399514	25.676967
170.827928	6532.839015	25.681984
170.590235	6542.771673	25.687002
170.745501	6536.477067	25.692020
171.155256	6534.312914	25.697037
171.562272	6542.667095	25.702055
171.431526	6565.358713	25.707072
171.672607	6568.501459	25.712090
171.500148	6566.198018	25.717108
171.896130	6563.889650	25.722125
172.395545	6575.847433	25.727143
172.231290	6588.812705	25.732160
172.669475	6587.835432	25.737178
172.929244	6575.719986	25.742196
172.746964	6593.389206	25.747213
173.131317	6602.655226	25.752231
172.691079	6609.665662	25.757248
173.055771	6607.966520	25.762266
173.715609	6620.442038	25.767284
174.095864	6635.602107	25.772301
174.567867	6622.237920	25.777319
174.331020	6623.876637	25.782336
174.625055	6624.483347	25.787354
174.645911	6624.435048	25.792372
174.342237	6622.571477	25.797389
174.639908	6618.624669	25.802407
174.928037	6643.145222	25.807424
174.892787	6655.509585	25.812442
174.969191	6651.852926	25.817460
175.037667	6659.573197	25.822477
175.076434	6682.694553	25.827495
175.253295	6697.815833	25.832512
175.536878	6712.350868	25.837530
175.866328	6715.658609	25.842548
175.685650	6724.528191	25.847565
175.916418	6733.754296	25.852583
175.864311	6750.961932	25.857600
176.024245	6771.353362	25.862618
176.579836	6789.599462	25.867636
176.312906	6799.559951	25.872653
177.008015	6805.420465	25.877671
177.169859	6824.193970	25.882688
177.688512	6846.191949	25.887706
177.713280	6851.679668	25.892724
177.708291	6858.312718	25.897741
178.216642	6864.718401	25.902759
178.205769	6875.172183	25.907776
178.276828	6880.253749	25.912794
178.764749	6895.328548	25.917812
178.632895	6911.412271	25.922829
178.807930	6908.609532	25.927847
179.123701	6927.878317	25.932864
179.250269	6930.050855	25.937882
179.842947	6930.967371	25.942900
179.618881	6944.433480	25.947917
180.033945	6960.368605	25.952935
180.375542	6966.302555	25.957952
180.467288	6962.012436	25.962970
180.710956	6974.948428	25.967988
180.393746	6992.620699	25.973005
180.930525	6984.942100	25.978023
180.612067	7000.047851	25.983040
180.792801	7012.813128	25.988058
181.648537	7015.735482	25.993076
181.925997	7024.917027	25.998093
181.993707	7036.987446	26.003111
182.487271	7043.210564	26.008128
182.460888	7045.639152	26.013146
182.736226	7031.928286	26.018164
182.608463	7040.218302	26.023181
182.704837	7047.386781	26.028199
183.172019	7059.514078	26.033216
183.135850	7065.308073	26.038234
183.613230	7056.254676	26.043252
183.437927	7060.788678	26.048269
183.871722	7076.696412	26.053287
184.072920	7076.293040	26.058304
184.189983	7077.590584	26.063322
184.217795	7081.969743	26.068340
184.064871	7106.726923	26.073357
184.545138	7108.587442	26.078375
184.641153	7111.525865	26.083392
184.519495	7129.666886	26.088410
185.133713	7135.869317	26.093428
185.003797	7151.238619	26.098445
185.502885	7163.434758	26.103463
185.898461	7183.445184	26.108480
185.418112	7178.577714	26.113498
185.923190	7175.330537	26.118516
186.310747	7195.711685	26.123533
186.499222	7202.490123	26.128551
186.544252	7196.066977	26.133568
186.488935	7212.084016	26.138586
186.544453	7228.300134	26.143604
186.461127	7237.718624	26.148621
186.936115	7248.224692	26.153639
187.647943	7256.845506	26.158656
187.597728	7257.807621	26.163674
187.949604	7253.604396	26.168692
187.975369	7273.824896	26.173709
188.412202	7286.423641	26.178727
188.646398	7286.342453	26.183744
188.651784	7280.758314	26.188762
189.034694	7286.536704	26.193780
188.707076	7312.314657	26.198797
189.109282	7321.337147	26.203815
189.187711	7325.767869	26.208832
189.081325	7344.329553	26.213850
189.285004	7340.813164	26.218868
189.552350	7362.793532	26.223885
189.777525	7369.695932	26.228903
189.996004	7392.795723	26.233920
190.046577	7420.646559	26.238938
190.450180	7416.730097	26.243956
190.471437	7442.826305	26.248973
190.818387	7447.369429	26.253991
190.845156	7454.922920	26.259008
191.204084	7477.303384	26.264026
191.869268	7474.466817	26.269044
191.705996	7494.195072	26.274061
192.085573	7505.034483	26.279079
192.414739	7493.539321	26.284096
192.168423	7509.804811	26.289114
192.595898	7527.364876	26.294132
192.812517	7533.863143	26.299149
192.985904	7539.311581	26.304167
192.965529	7552.698082	26.309184
192.851085	7565.633871	26.314202
193.197466	7577.097880	26.319220
193.745592	7587.955968	26.324237
194.039986	7596.351374	26.329255
194.202612	7609.507633	26.334272
194.009339	7618.960268	26.339290
194.521042	7628.645343	26.344308
194.924635	7645.459674	26.349325
194.864093	7648.373658	26.354343
195.047888	7655.252304	26.359360
195.331216	7671.819533	26.364378
195.524167	7665.461544	26.369396
195.698684	7686.718128	26.374413
195.691320	7714.463273	26.379431
196.128477	7720.870833	26.384448
196.163247	7728.086031	26.389466
196.229162	7739.382265	26.394484
196.267168	7743.606338	26.399501
196.731589	7766.028065	26.404519
197.431583	7769.715089	26.409536
197.411061	7778.865184	26.414554
197.562944	7789.834563	26.419572
197.767567	7804.011107	26.424589
198.180452	7803.893306	26.429607
198.465806	7799.567033	26.434624
198.397215	7819.450964	26.439642
198.572122	7835.662157	26.444660
198.702550	7838.697422	26.449677
199.057138	7834.561333	26.454695
199.841586	7840.231840	26.459712
199.720336	7844.365684	26.464730
200.026955	7848.902986	26.469748
199.706883	7844.108853	26.474765
200.242227	7845.386971	26.479783
200.245615	7846.970367	26.484800
200.126920	7849.460801	26.489818
200.294076	7862.452696	26.494836
200.700341	7884.157220	26.499853
200.750218	7880.268373	26.504871
200.848574	7892.411570	26.509888
201.006321	7905.647645	26.514906
200.992828	7900.961942	26.519924
201.246808	7922.205712	26.524941
201.499456	7944.194043	26.529959
201.829801	7950.366516	26.534976
201.853280	7972.780265	26.539994
202.092331	7984.481266	26.545012
202.234195	7993.441614	26.550029
202.261255	8003.106178	26.555047
202.753131	8015.163972	26.560064
202.651520	8030.620027	26.565082
203.085220	8053.439481	26.570100
202.881869	8063.497375	26.575117
203.634761	8073.698947	26.580135
204.317593	8069.358913	26.585152
204.588796	8081.392570	26.590170
205.083622	8100.456774	26.595188
205.493378	8109.567473	26.600205
205.373633	8112.370027	26.605223
205.634928	8102.795666	26.610240
205.753790	8113.172120	26.615258
205.762270	8104.811537	26.620276
205.706337	8118.888851	26.625293
205.745534	8138.189847	26.630311
206.248235	8129.086764	26.635328
206.169007	8152.025765	26.640346
206.779330	8168.074778	26.645364
206.630435	8167.908020	26.650381
206.418169	8178.410115	26.655399
206.836736	8192.646964	26.660416
206.622260	8214.458441	26.665434
207.277631	8231.999752	26.670452
207.789436	8248.280940	26.675469
207.953820	8270.897885	26.680487
209.279176	8237.014918	26.685504
209.353655	8227.063348	26.690522
209.274068	8225.386248	26.695540
209.551334	8225.061649	26.700557
209.744756	8225.021853	26.705575
210.362234	8254.135240	26.710592
210.219480	8251.348540	26.715610
210.350481	8253.530770	26.720628
210.511660	8259.351668	26.725645
210.259727	8259.565826	26.730663
211.028559	8258.086446	26.735680
210.596515	8264.312542	26.740698
210.675508	8266.949962	26.745716
210.915227	8291.033691	26.750733
211.007997	8292.543290	26.755751
211.490480	8294.350029	26.760768
211.668197	8319.065500	26.765786
211.711173	8334.873672	26.770804
211.981685	8341.922600	26.775821
212.056037	8364.649860	26.780839
212.102551	8355.351069	26.785856
212.178601	8379.965285	26.790874
212.367479	8398.917354	26.795892
212.572313	8404.204941	26.800909
212.860210	8422.495590	26.805927
213.322436	8437.806897	26.810944
213.017067	8454.326496	26.815962
213.283341	8465.889454	26.820980
213.820869	8481.442776	26.825997
213.743812	8492.170062	26.831015
214.378918	8513.070461	26.836032
214.307244	8519.145747	26.841050
214.442017	8532.814629	26.846068
214.969764	8544.085543	26.851085
215.255766	8568.439303	26.856103
215.796879	8564.239915	26.861120
215.809947	8573.132866	26.866138
215.888980	8586.541624	26.871156
216.430688	8596.729594	26.876173
216.241541	8611.995885	26.881191
216.910842	8621.866629	26.886208
217.403092	8619.412889	26.891226
217.471070	8625.050042	26.896244
217.837032	8615.524245	26.901261
217.524964	8625.301143	26.906279
217.825305	8638.447320	26.911296
218.001955	8653.005751	26.916314
218.009809	8654.512085	26.921332
218.597322	8671.747669	26.926349
218.503366	8687.056591	26.931367
218.700156	8696.899904	26.936384
218.870510	8717.496129	26.941402
219.005124	8725.680660	26.946420
219.213064	8751.116467	26.951437
219.150445	8753.342571	26.956455
219.530151	8763.765361	26.961472
219.627678	8792.789995	26.966490
220.300807	8811.532583	26.971508
220.304262	8827.665995	26.976525
220.288120	8847.694568	26.981543
220.824253	8849.154598	26.986560
221.195627	8878.896614	26.991578
221.263197	8894.390933	26.996596
221.735393	8899.091014	27.001613
222.098588	8901.416924	27.006631
222.297422	8898.614631	27.011648
222.596696	8925.493620	27.016666
222.860140	8934.998393	27.021684
223.136292	8932.258150	27.026701
223.125431	8943.328472	27.031719
223.506281	8950.122351	27.036736
223.739447	8952.316154	27.041754
223.697103	8965.542851	27.046772
224.080123	8973.191016	27.051789
224.313488	8988.461114	27.056807
224.495959	8986.568133	27.061824
224.899842	9008.792102	27.066842
224.929692	9015.510095	27.071860
225.216274	9020.220399	27.076877
225.128207	9048.579063	27.081895
225.411685	9050.350244	27.086912
225.458150	9069.477092	27.091930
225.505368	9085.553123	27.096948
226.000577	9100.312967	27.101965
226.322797	9117.279368	27.106983
226.712459	9129.524256	27.112000
226.802263	9145.415293	27.117018
227.156892	9151.181715	27.122036
227.438661	9175.612725	27.127053
227.429751	9177.675626	27.132071
227.721713	9189.212025	27.137088
228.333161	9200.813802	27.142106
227.861879	9205.587935	27.147124
228.633929	9224.840062	27.152141
228.919007	9233.114211	27.157159
228.869467	9227.302154	27.162176
229.069609	9233.678600	27.167194
229.044635	9255.302654	27.172212
229.605906	9254.390754	27.177229
229.692298	9280.868346	27.182247
229.555025	9295.231894	27.187264
230.154927	9306.819902	27.192282
230.248132	9328.389871	27.197300
230.473762	9328.001316	27.202317
230.519366	9352.258149	27.207335
230.707553	9363.373071	27.212352
231.279998	9378.029828	27.217370
231.478517	9382.409776	27.222388
231.431373	9391.758185	27.227405
231.486038	9420.124647	27.232423
231.972070	9431.935576	27.237440
232.276965	9439.815857	27.242458
232.148559	9470.362304	27.247476
232.568771	9479.023862	27.252493
232.771419	9508.365633	27.257511
233.081072	9532.290024	27.262528
233.604250	9536.243001	27.267546
233.624670	9549.925350	27.272564
234.386172	9568.000433	27.277581
234.439621	9581.647419	27.282599
234.756795	9607.241420	27.287616
234.993473	9601.590682	27.292634
235.112751	9618.379253	27.297652
235.376394	9627.932459	27.302669
235.623713	9639.286721	27.307687
235.557223	9648.323390	27.312704
236.359736	9653.329109	27.317722
236.737359	9679.711983	27.322740
237.667950	9679.554332	27.327757
237.932852	9666.820481	27.332775
237.677357	9680.649356	27.337792
238.031770	9674.356056	27.342810
238.059163	9677.156629	27.347828
238.047381	9681.339817	27.352845
238.053701	9695.046676	27.357863
238.346174	9705.519159	27.362880
238.721676	9703.270451	27.367898
238.848806	9726.959831	27.372916
238.999097	9736.262430	27.377933
239.329205	9752.465693	27.382951
239.336693	9767.905407	27.387968
239.975962	9767.999908	27.392986
239.965487	9791.545909	27.398004
240.112061	9790.872647	27.403021
239.979088	9808.901221	27.408039
240.406178	9832.655419	27.413056
240.653628	9831.080874	27.418074
240.690341	9859.577119	27.423092
241.318484	9873.352332	27.428109
241.369690	9899.639044	27.433127
241.456227	9905.203477	27.438144
242.003391	9924.455798	27.443162
241.916473	9936.091574	27.448180
242.236831	9953.061537	27.453197
242.593142	9975.761843	27.458215
242.902616	9993.298451	27.463232
243.146841	10005.853204	27.468250
243.419148	10016.634077	27.473268
243.725010	10046.017289	27.478285
243.841849	10050.904040	27.483303
244.186132	10073.039301	27.488320
244.496194	10090.007961	27.493338
244.871976	10090.223197	27.498356
245.245715	10103.090629	27.503373
245.413795	10105.517490	27.508391
245.549700	10120.380185	27.513408
245.843197	10129.322201	27.518426
245.983160	10146.957094	27.523444
246.168242	10148.152278	27.528461
246.409879	10164.636833	27.533479
246.206961	10180.648161	27.538496
247.066753	10195.147127	27.543514
246.926500	10215.916345	27.548532
247.054819	10232.081750	27.553549
247.460148	10254.751509	27.558567
247.497552	10257.039283	27.563584
248.002791	10269.128888	27.568602
248.370672	10287.697571	27.573620
248.421625	10298.126059	27.578637
249.399974	10302.479829	27.583655
249.649502	10315.935134	27.588672
250.133798	10316.762645	27.593690
250.440993	10327.581290	27.598708
249.975560	10324.033003	27.603725
250.512708	10331.748528	27.608743
250.380602	10345.584373	27.613760
250.751750	10354.433336	27.618778
250.841977	10376.712613	27.623796
250.764935	10387.394693	27.628813
251.003540	10407.528081	27.633831
251.177360	10424.202141	27.638848
251.635787	10444.482017	27.643866
251.638859	10474.579333	27.648884
251.932284	10482.692052	27.653901
252.364695	10513.404643	27.658919
252.352652	10534.547757	27.663936
252.733897	10551.997498	27.668954
252.537455	10571.246628	27.673972
253.169362	10594.042501	27.678989
253.876818	10615.462306	27.684007
253.787223	10647.072794	27.689024
254.143770	10663.403383	27.694042
254.483934	10686.398840	27.699060
254.959288	10686.462140	27.704077
255.391799	10712.576115	27.709095
255.308728	10731.114257	27.714112
256.027355	10733.711007	27.719130
256.058605	10752.654107	27.724148
256.440002	10776.257341	27.729165
257.145895	10776.493677	27.734183
256.781854	10792.591317	27.739200
256.943808	10805.273730	27.744218
257.282102	10809.132320	27.749236
257.718216	10822.788043	27.754253
258.300855	10837.116749	27.759271
258.345346	10849.059190	27.764288
258.816580	10845.504135	27.769306
259.047339	10859.068560	27.774324
258.984213	10858.215626	27.779341
259.593432	10886.436349	27.784359
259.213635	10896.771747	27.789376
259.764895	10907.043922	27.794394
259.769097	10929.697406	27.799412
259.828371	10942.178678	27.804429
260.485020	10954.926794	27.809447
260.268649	10974.413670	27.814464
260.913494	10988.484872	27.819482
260.503369	11012.272795	27.824500
260.958178	11030.747627	27.829517
261.399242	11048.387336	27.834535
261.413199	11070.277619	27.839552
261.724593	11085.597493	27.844570
261.836383	11106.756353	27.849588
262.306719	11133.249992	27.854605
262.472045	11148.159199	27.859623
262.768484	11173.080847	27.864640
263.403253	11188.734987	27.869658
263.736872	11197.147880	27.874676
264.117484	11223.881014	27.879693
264.485833	11221.727029	27.884711
264.604751	11230.496043	27.889728
264.840278	11250.547494	27.894746
265.016473	11263.646236	27.899764
265.029754	11286.561847	27.904781
265.739732	11289.266474	27.909799
265.532932	11320.365099	27.914816
265.992158	11327.391268	27.919834
266.253636	11357.186784	27.924852
266.465167	11358.484831	27.929869
267.071114	11369.405295	27.934887
267.602896	11373.867811	27.939904
268.433504	11384.969389	27.944922
268.333317	11401.397462	27.949940
268.727264	11409.217527	27.954957
268.875762	11398.023573	27.959975
268.984553	11412.582341	27.964992
269.324465	11431.867573	27.970010
269.410411	11433.891459	27.975028
269.235485	11441.857520	27.980045
269.813763	11457.759962	27.985063
269.989665	11478.321805	27.990080
270.254533	11483.557170	27.995098
270.480554	11502.413829	28.000116
270.431786	11540.333602	28.005133
270.857725	11547.795511	28.010151
271.162572	11568.922296	28.015168
271.442961	11585.371188	28.020186
271.759575	11609.699323	28.025204
271.667216	11619.042319	28.030221
271.787799	11639.951479	28.035239
272.083588	11673.531298	28.040256
272.519141	11691.921051	28.045274
272.891846	11707.727715	28.050292
273.147091	11733.287292	28.055309
273.744867	11738.466953	28.060327
273.891316	11767.658282	28.065344
274.280299	11784.294270	28.070362
274.452961	11810.092142	28.075380
274.859024	11819.330061	28.080397
275.064800	11828.090567	28.085415
275.342698	11856.288954	28.090432
275.438372	11869.065881	28.095450
276.056816	11883.724438	28.100468
276.497438	11896.043393	28.105485
277.143520	11897.825110	28.110503
277.371674	11910.278444	28.115520
277.594317	11916.426929	28.120538
277.827089	11918.378562	28.125556
277.687388	11955.798309	28.130573
278.194250	11945.819476	28.135591
278.414427	11966.539285	28.140608
278.382537	11978.246229	28.145626
278.746726	11993.915137	28.150644
278.501341	12017.182564	28.155661
279.181543	12030.999890	28.160679
278.930695	12052.349110	28.165696
279.245742	12069.196931	28.170714
279.913953	12096.726987	28.175732
280.057293	12109.610465	28.180749
280.391329	12130.507845	28.185767
280.467442	12146.481329	28.190784
281.133734	12160.997515	28.195802
281.265270	12177.749713	28.200820
281.403803	12199.193153	28.205837
281.868492	12210.117835	28.210855
282.366499	12229.823824	28.215872
283.072517	12223.988272	28.220890
283.423712	12215.709945	28.225908
283.754989	12247.488032	28.230925
284.153457	12247.241035	28.235943
284.212965	12262.887272	28.240960
284.245771	12255.268166	28.245978
284.621123	12271.248274	28.250996
284.555252	12282.506467	28.256013
285.082469	12302.574068	28.261031
284.914515	12331.496921	28.266048
284.684109	12352.765951	28.271066
285.381390	12362.730527	28.276084
285.296550	12387.115920	28.281101
286.001902	12408.435268	28.286119
286.142995	12440.026920	28.291136
286.490803	12461.424316	28.296154
286.613490	12482.349979	28.301172
286.382370	12514.256958	28.306189
286.852010	12545.102798	28.311207
287.329218	12570.538004	28.316224
287.263014	12605.558324	28.321242
287.644081	12625.636292	28.326260
288.384043	12651.565539	28.331277
288.984965	12682.651523	28.336295
289.730959	12691.484762	28.341312
289.841788	12716.044744	28.346330
290.196939	12730.151948	28.351348
290.533529	12749.123374	28.356365
291.011074	12761.957675	28.361383
291.334315	12779.809418	28.366400
291.635096	12782.941180	28.371418
292.075973	12801.949014	28.376436
291.962118	12825.366053	28.381453
292.506607	12826.631275	28.386471
292.597058	12842.238295	28.391488
292.644323	12847.126363	28.396506
293.019454	12872.076248	28.401524
293.038619	12889.269262	28.406541
293.516081	12897.141651	28.411559
293.771245	12923.193974	28.416576
294.204052	12944.242333	28.421594
294.616181	12960.615715	28.426612
294.196914	12988.254474	28.431629
295.129824	13017.582861	28.436647
294.965218	13033.451234	28.441664
295.467457	13053.500261	28.446682
295.645908	13081.714857	28.451700
295.921245	13107.160625	28.456717
296.403848	13118.409149	28.461735
296.498572	13134.239504	28.466752
296.588800	13160.385641	28.471770
297.089253	13178.369277	28.476788
297.287684	13205.630594	28.481805
297.492691	13240.771362	28.486823
298.413563	13257.779554	28.491840
298.068361	13278.972640	28.496858
298.572565	13294.785928	28.501876
298.711110	13320.059231	28.506893
299.460380	13343.753583	28.511911
299.860222	13359.965518	28.516928
300.065560	13390.150681	28.521946
300.420165	13396.834975	28.526964
300.757875	13409.363553	28.531981
300.544909	13424.250694	28.536999
301.279477	13440.599658	28.542016
301.198055	13466.487850	28.547034
301.634002	13482.490664	28.552052
301.751600	13503.180541	28.557069
301.790294	13523.290975	28.562087
302.184529	13546.730693	28.567104
302.459217	13579.232226	28.572122
302.842545	13593.390683	28.577140
302.951178	13613.644105	28.582157
303.631743	13643.640920	28.587175
303.929181	13668.124242	28.592192
303.764465	13700.079311	28.597210
304.117567	13711.603354	28.602228
304.665933	13746.570305	28.607245
304.773539	13787.820518	28.612263
305.093114	13806.490284	28.617280
305.687869	13845.742368	28.622298
305.906122	13869.436972	28.627316
306.436846	13890.355350	28.632333
306.729168	13905.391103	28.637351
307.310608	13935.828739	28.642368
307.436065	13972.979262	28.647386
307.912072	13988.221124	28.652404
308.443900	14005.883750	28.657421
308.792639	14003.957207	28.662439
309.243603	14014.128971	28.667456
309.636283	14032.624606	28.672474
310.016996	14055.870312	28.677492
310.044683	14066.847965	28.682509
309.908203	14082.782052	28.687527
310.452946	14100.644359	28.692544
310.550033	14119.280328	28.697562
311.087476	14146.293387	28.702580
311.220165	14173.447425	28.707597
311.286132	14199.402258	28.712615
312.198555	14206.068800	28.717632
312.042141	14233.401498	28.722650
312.624695	14245.291439	28.727668
312.989124	14278.242855	28.732685
313.313411	14299.358181	28.737703
313.868384	14303.968979	28.742720
314.257132	14319.835437	28.747738
314.654243	14327.813205	28.752756
315.012706	14350.371193	28.757773
315.705287	14359.690099	28.762791
316.215013	14363.077617	28.767808
316.371877	14375.917329	28.772826
316.447707	14375.778768	28.777844
316.720223	14389.938895	28.782861
317.113384	14412.196545	28.787879
317.357119	14412.283964	28.792896
317.520144	14425.669534	28.797914
317.421216	14443.974225	28.802932
317.541136	14466.582815	28.807949
318.134709	14488.257471	28.812967
318.454521	14505.653096	28.817984
318.372165	14522.429660	28.823002
318.984832	14533.344080	28.828020
319.257275	14554.633774	28.833037
319.479981	14590.731117	28.838055
319.835332	14609.098048	28.843072
319.822521	14641.285166	28.848090
320.231855	14661.996086	28.853108
320.411573	14682.599981	28.858125
320.228175	14708.103558	28.863143
320.781792	14750.815904	28.868160
320.635091	14778.398483	28.873178
321.209690	14803.345177	28.878196
321.609312	14833.677428	28.883213
322.251733	14862.311735	28.888231
322.750253	14886.533586	28.893248
322.665261	14912.081109	28.898266
323.423613	14940.352845	28.903284
323.849331	14960.473610	28.908301
324.353627	14983.599366	28.913319
324.705736	15000.203784	28.918336
324.763998	15026.687576	28.923354
325.273231	15049.030935	28.928372
325.407493	15066.810828	28.933389
325.553775	15083.906364	28.938407
326.068383	15099.065671	28.943424
326.391452	15133.223383	28.948442
326.819582	15160.538285	28.953460
326.889801	15178.149219	28.958477
327.481649	15212.371435	28.963495
327.846620	15234.994190	28.968512
328.042409	15246.879420	28.973530
328.396385	15268.954022	28.978548
328.725910	15299.073355	28.983565
329.252544	15321.842881	28.988583
329.845496	15339.425943	28.993600
329.784188	15361.911267	28.998618
330.173326	15378.520985	29.003636
330.852731	15396.110314	29.008653
331.044567	15425.146280	29.013671
331.756888	15438.763439	29.018688
332.084034	15454.968990	29.023706
332.589632	15465.006561	29.028724
332.545381	15488.419080	29.033741
332.601453	15499.742880	29.038759
333.737763	15512.855081	29.043776
333.713079	15519.688019	29.048794
334.459878	15540.364795	29.053812
335.036115	15550.794207	29.058829
335.189484	15552.065961	29.063847
335.527803	15569.201200	29.068864
335.551446	15584.722600	29.073882
335.541750	15585.417684	29.078900
335.701083	15612.076425	29.083917
335.772367	15638.918388	29.088935
336.259235	15662.692579	29.093952
336.166871	15695.257398	29.098970
336.122936	15726.157880	29.103988
336.668902	15758.239125	29.109005
336.830253	15789.491939	29.114023
337.275063	15816.118034	29.119040
337.163646	15848.865973	29.124058
337.803856	15883.816040	29.129076
338.471850	15919.699336	29.134093
338.924985	15963.042960	29.139111
339.213530	15982.937056	29.144128
339.606391	16023.264784	29.149146
340.224920	16044.544953	29.154164
340.725204	16067.135475	29.159181
340.774597	16093.682348	29.164199
341.503544	16129.984725	29.169216
341.697121	16146.840301	29.174234
341.500716	16174.805391	29.179252
342.147818	16199.020406	29.184269
342.131596	16227.772224	29.189287
342.766395	16257.563925	29.194304
342.969242	16283.964398	29.199322
343.161653	16318.527579	29.204340
343.486308	16350.017689	29.209357
343.848572	16380.623765	29.214375
344.172774	16399.415521	29.219392
344.714683	16422.705744	29.224410
344.737985	16452.132296	29.229428
345.449781	16484.168655	29.234445
345.681591	16509.401546	29.239463
346.350320	16528.923008	29.244480
346.597477	16558.635870	29.249498
347.067209	16577.826184	29.254516
347.497650	16589.612158	29.259533
347.710248	16620.372648	29.264551
348.175710	16645.398505	29.269568
348.478303	16677.184467	29.274586
348.708286	16695.629621	29.279604
349.051214	16708.057432	29.284621
349.457267	16747.880403	29.289639
350.007569	16766.449246	29.294656
350.541415	16790.830426	29.299674
350.807007	16805.372062	29.304692
351.308206	16818.977972	29.309709
351.482070	16847.232937	29.314727
351.679672	16877.454196	29.319744
352.259767	16900.300625	29.324762
352.332263	16925.639281	29.329780
352.671906	16943.374672	29.334797
352.838671	16970.913878	29.339815
353.363954	17004.777294	29.344832
353.775171	17022.767316	29.349850
354.032860	17055.984691	29.354868
354.320760	17074.029816	29.359885
354.798298	17107.245651	29.364903
355.091690	17139.284636	29.369920
355.219902	17174.560037	29.374938
355.418136	17198.730894	29.379956
355.823809	17234.053580	29.384973
356.223356	17268.460022	29.389991
356.129823	17284.932325	29.395008
357.206936	17324.239181	29.400026
357.441780	17353.827843	29.405044
357.898316	17385.090093	29.410061
358.533614	17414.541781	29.415079
358.798179	17432.253851	29.420096
359.547112	17472.827366	29.425114
359.700770	17493.461167	29.430132
360.088457	17508.875380	29.435149
360.521984	17537.715958	29.440167
360.450353	17569.773524	29.445184
361.002634	17588.908827	29.450202
361.223803	17623.287158	29.455220
361.603771	17658.053870	29.460237
361.711241	17684.598442	29.465255
362.297016	17711.965636	29.470272
362.626692	17736.229055	29.475290
363.205449	17759.890228	29.480308
363.921030	17776.435842	29.485325
364.429224	17793.531156	29.490343
364.995587	17808.884610	29.495360
365.448667	17822.464626	29.500378
365.682413	17841.304498	29.505396
366.249970	17844.654831	29.510413
366.596295	17878.770280	29.515431
366.695084	17882.133435	29.520448
366.887502	17899.519037	29.525466
366.785993	17916.592255	29.530484
367.214065	17947.989526	29.535501
367.936608	17969.633310	29.540519
368.067761	17981.023651	29.545536
368.705308	17992.784302	29.550554
368.787097	18010.431037	29.555572
369.120696	18033.234645	29.560589
369.633713	18046.235920	29.565607
369.933955	18070.488931	29.570624
370.300000	18084.622618	29.575642
370.256464	18120.330356	29.580660
370.784007	18138.425330	29.585677
371.020244	18171.673715	29.590695
371.229653	18200.940237	29.595712
371.514354	18221.967857	29.600730
371.647186	18255.684304	29.605748
371.983626	18291.088470	29.610765
372.111653	18334.318657	29.615783
372.255056	18360.946650	29.620800
373.089629	18394.594743	29.625818
373.298440	18437.524971	29.630836
373.894126	18475.125026	29.635853
374.559740	18507.834997	29.640871
374.849554	18534.833156	29.645888
375.488296	18566.821013	29.650906
375.666772	18593.552351	29.655924
376.323995	18621.771487	29.660941
376.585124	18651.749054	29.665959
377.377881	18689.812001	29.670976
377.745371	18706.564227	29.675994
377.676191	18744.143893	29.681012
378.268816	18771.103448	29.686029
378.824323	18813.819746	29.691047
379.108938	18844.881442	29.696064
379.711358	18862.428891	29.701082
379.959419	18890.216383	29.706100
380.604215	18920.395878	29.711117
380.855091	18940.414843	29.716135
380.805722	18977.307636	29.721152
381.392345	18996.483038	29.726170
381.592022	19027.765608	29.731188
381.526731	19058.812996	29.736205
382.241390	19087.720182	29.741223
382.397612	19132.878813	29.746240
383.180672	19145.188466	29.751258
383.586062	19194.442446	29.756276
384.239147	19220.055996	29.761293
384.984699	19236.286009	29.766311
385.374977	19250.738267	29.771328
385.919381	19263.448421	29.776346
385.833307	19294.420863	29.781364
386.351815	19322.457606	29.786381
386.653897	19349.075159	29.791399
386.808815	19378.362218	29.796416
387.579333	19398.231262	29.801434
387.409147	19427.203241	29.806452
388.101447	19452.087115	29.811469
388.323842	19488.177908	29.816487
388.436338	19522.760993	29.821504
389.152234	19538.044065	29.826522
389.109865	19568.473825	29.831540
389.701998	19597.838802	29.836557
390.088528	19636.160197	29.841575
390.226005	19684.865586	29.846592
390.758727	19714.344625	29.851610
390.659369	19753.645106	29.856628
391.314559	19783.127682	29.861645
391.834915	19815.725508	29.866663
392.346737	19852.010469	29.871680
392.723476	19883.497132	29.876698
393.017961	19928.657151	29.881716
393.263072	19954.572541	29.886733
393.377501	19988.147358	29.891751
393.589653	20015.855959	29.896768
394.450127	20047.737529	29.901786
395.044634	20098.723822	29.906804
395.504883	20131.863456	29.911821
395.669957	20155.981047	29.916839
396.010050	20192.946191	29.921856
396.594835	20216.904680	29.926874
396.868859	20248.122085	29.931892
397.283139	20280.774602	29.936909
397.876748	20316.878385	29.941927
398.269432	20354.514654	29.946944
398.573221	20377.944383	29.951962
398.873432	20414.446819	29.956980
399.438027	20444.781063	29.961997
399.967761	20471.501533	29.967015
400.402967	20509.764872	29.972032
400.727233	20536.609247	29.977050
401.072486	20580.439975	29.982068
401.500050	20615.301185	29.987085
402.095384	20638.293726	29.992103
402.094041	20671.923725	29.997120
402.378639	20701.803365	30.002138
402.876744	20742.025889	30.007156
403.223939	20780.689052	30.012173
403.664537	20817.173906	30.017191
403.669424	20852.524785	30.022208
404.352187	20898.026871	30.027226
404.642384	20936.327752	30.032244
405.172722	20969.493730	30.037261
405.628801	21012.823291	30.042279
405.935635	21068.647976	30.047296
406.353027	21098.853225	30.052314
407.395703	21143.025836	30.057332
408.116292	21155.473432	30.062349
409.154860	21180.059904	30.067367
409.390971	21206.577808	30.072384
409.866144	21210.792283	30.077402
410.199658	21234.814237	30.082420
410.452953	21260.807552	30.087437
410.773923	21276.734482	30.092455
411.228290	21306.740083	30.097472
411.177541	21334.874248	30.102490
411.647959	21364.795320	30.107508
411.950533	21380.857819	30.112525
412.460143	21421.233002	30.117543
412.807216	21461.390764	30.122560
413.007905	21483.551017	30.127578
413.402770	21527.191569	30.132596
413.360520	21578.479903	30.137613
414.054516	21602.242610	30.142631
414.105702	21640.149445	30.147648
415.109040	21677.676780	30.152666
415.468597	21719.018690	30.157684
415.795705	21741.286104	30.162701
416.523302	21776.973605	30.167719
416.958138	21832.133281	30.172736
417.170079	21859.256895	30.177754
417.659509	21891.010935	30.182772
417.728075	21924.270850	30.187789
418.298515	21974.552630	30.192807
418.281506	22000.670571	30.197824
418.812541	22045.287975	30.202842
419.249884	22091.237457	30.207860
419.521460	22128.140935	30.212877
419.992109	22163.171678	30.217895
420.388807	22228.296976	30.222912
420.655204	22255.511561	30.227930
421.245234	22289.838583	30.232948
421.529093	22342.894824	30.237965
422.078075	22367.034164	30.242983
422.476896	22396.424957	30.248000
423.128703	22436.337626	30.253018
423.735827	22474.755212	30.258036
424.282800	22508.965238	30.263053
424.888726	22538.683125	30.268071
424.540742	22578.368694	30.273088
425.381991	22597.857779	30.278106
425.938583	22648.117055	30.283124
425.937409	22681.177132	30.288141
426.657741	22721.884844	30.293159
426.706779	22759.228519	30.298176
427.058578	22793.551775	30.303194
427.997057	22832.848844	30.308212
428.274124	22875.487497	30.313229
428.506984	22917.819797	30.318247
428.918709	22961.168013	30.323264
429.769858	22994.713864	30.328282
429.850506	23025.624654	30.333300
430.342506	23071.086880	30.338317
430.850501	23111.450619	30.343335
431.373500	23170.541918	30.348352
431.439426	23194.101590	30.353370
431.752262	23246.656060	30.358388
432.192296	23292.092777	30.363405
432.737066	23339.891621	30.368423
432.859943	23387.824938	30.373440
433.507591	23426.132354	30.378458
433.793097	23485.659749	30.383476
434.222105	23540.477509	30.388493
434.839681	23575.244092	30.393511
435.256986	23623.241389	30.398528
435.853096	23669.810688	30.403546
436.460473	23706.007782	30.408564
436.916265	23752.146374	30.413581
437.630425	23792.715777	30.418599
437.819793	23851.853527	30.423616
438.199266	23877.134668	30.428634
438.951112	23913.235808	30.433652
439.075264	23964.030853	30.438669
439.581809	24013.652812	30.443687
440.217281	24050.997072	30.448704
440.840249	24090.068514	30.453722
441.545020	24132.133523	30.458740
441.829395	24168.842239	30.463757
442.263221	24198.853229	30.468775
442.434050	24225.493886	30.473792
442.704429	24273.843698	30.478810
443.549187	24314.954130	30.483828
443.645834	24356.081015	30.488845
444.343703	24398.256626	30.493863
445.174041	24418.333055	30.498880
445.387008	24456.880174	30.503898
446.032997	24486.298422	30.508916
446.589283	24531.714528	30.513933
447.057103	24554.413389	30.518951
447.308936	24601.054729	30.523968
447.673053	24638.634330	30.528986
448.324849	24672.186480	30.534004
448.405105	24706.258860	30.539021
448.783922	24742.779760	30.544039
449.071005	24784.814463	30.549056
449.397946	24822.435301	30.554074
449.869737	24857.469859	30.559092
450.079779	24912.260411	30.564109
450.865959	24931.669834	30.569127
451.673185	24967.199544	30.574144
452.566705	24992.072593	30.579162
453.104672	25016.001503	30.584180
453.462978	25048.850696	30.589197
453.846573	25062.203660	30.594215
454.019852	25092.967297	30.599232
454.205683	25129.749556	30.604250
454.917141	25157.150746	30.609268
454.770791	25205.250350	30.614285
455.711272	25230.123876	30.619303
455.463407	25270.641261	30.624320
456.117571	25321.385921	30.629338
456.722045	25357.796749	30.634356
457.002734	25399.494983	30.639373
457.158779	25437.556989	30.644391
457.609608	25482.699740	30.649408
457.785809	25528.976067	30.654426
458.634627	25584.312964	30.659444
458.213811	25629.947014	30.664461
459.365703	25688.902186	30.669479
459.988789	25748.165687	30.674496
459.860145	25792.717418	30.679514
460.627384	25843.930660	30.684532
460.924386	25909.247398	30.689549
461.972070	25955.794095	30.694567
462.289945	25992.838680	30.699584
462.774218	26051.444902	30.704602
463.545983	26088.326407	30.709620
463.890377	26134.317961	30.714637
464.542823	26180.066358	30.719655
464.885640	26237.860770	30.724672
465.179556	26284.583337	30.729690
466.008486	26328.009997	30.734708
466.028849	26370.709272	30.739725
466.768433	26423.360754	30.744743
467.523176	26462.936291	30.749760
468.283638	26498.476917	30.754778
468.842566	26537.939885	30.759796
469.409609	26585.523376	30.764813
469.435426	26618.047283	30.769831
469.895272	26653.092228	30.774848
470.198171	26704.719080	30.779866
470.754517	26745.233270	30.784884
471.013749	26796.836070	30.789901
471.375794	26837.322644	30.794919
471.697055	26879.635989	30.799936
471.973334	26940.342412	30.804954
472.858890	26998.349378	30.809972
472.793339	27053.517180	30.814989
473.329311	27105.138277	30.820007
474.211177	27163.007624	30.825024
474.746008	27209.345949	30.830042
475.538218	27254.418052	30.835060
476.040316	27301.392875	30.840077
476.978365	27332.057862	30.845095
478.342374	27353.107847	30.850112
478.316027	27381.730571	30.855130
478.980546	27422.357814	30.860148
479.164023	27460.683153	30.865165
479.568243	27500.303211	30.870183
480.331485	27515.292373	30.875200
480.711684	27557.017265	30.880218
480.902536	27581.459740	30.885236
481.368699	27632.346388	30.890253
481.368133	27663.539212	30.895271
481.921313	27699.659102	30.900288
482.836046	27740.501263	30.905306
482.948485	27765.562576	30.910324
483.167874	27818.070840	30.915341
483.512245	27847.897981	30.920359
483.854959	27894.273038	30.925376
484.357306	27923.525363	30.930394
485.460117	27952.820499	30.935412
485.745752	27980.089940	30.940429
486.199024	28023.892067	30.945447
486.646570	28064.250691	30.950464
486.922374	28112.321813	30.955482
487.119872	28145.050510	30.960500
487.838320	28199.729722	30.965517
488.053715	28240.117640	30.970535
488.247052	28294.786104	30.975552
488.596755	28342.870895	30.980570
489.193546	28396.697054	30.985588
489.535196	28461.930932	30.990605
489.784702	28517.953535	30.995623
490.558032	28572.126458	31.000640
490.777229	28643.447255	31.005658
491.671386	28692.894139	31.010676
492.017272	28753.633293	31.015693
492.484258	28810.504175	31.020711
493.400382	28861.137155	31.025728
493.967818	28912.572345	31.030746
494.696793	28959.328086	31.035764
495.204139	29007.221492	31.040781
495.641465	29069.643786	31.045799
496.164952	29116.695720	31.050816
496.378931	29158.130166	31.055834
497.316766	29216.580748	31.060852
498.026758	29259.580191	31.065869
498.501716	29308.388296	31.070887
499.485009	29344.084109	31.075904
500.013978	29382.050640	31.080922
501.699196	29382.848038	31.085940
502.535237	29410.530400	31.090957
502.636978	29429.491732	31.095975
503.228710	29453.577256	31.100992
503.749883	29480.721827	31.106010
504.163275	29488.675771	31.111028
504.653821	29515.330180	31.116045
504.812179	29533.376897	31.121063
505.430321	29567.871638	31.126080
505.115669	29609.293529	31.131098
505.912618	29640.399190	31.136116
506.243132	29667.528225	31.141133
506.515871	29701.635478	31.146151
506.924159	29741.102262	31.151168
506.866371	29798.697148	31.156186
507.407262	29850.066943	31.161204
507.956418	29897.848641	31.166221
508.222833	29958.292819	31.171239
508.175917	30002.125776	31.176256
508.611905	30067.432123	31.181274
509.371443	30131.637901	31.186292
509.535973	30187.881826	31.191309
510.163242	30249.415734	31.196327
510.756885	30300.323858	31.201344
510.928769	30375.101415	31.206362
511.348961	30430.691865	31.211380
512.254022	30487.407537	31.216397
512.504286	30548.723995	31.221415
513.601836	30593.785909	31.226432
514.172491	30670.928074	31.231450
514.923631	30728.117938	31.236468
515.735053	30782.518608	31.241485
516.048897	30818.984238	31.246503
516.565150	30873.273048	31.251520
516.951807	30920.191558	31.256538
517.413026	30964.059726	31.261556
518.061553	31000.773323	31.266573
518.350620	31062.343873	31.271591
519.389243	31097.355846	31.276608
519.392174	31157.557439	31.281626
519.462169	31199.269753	31.286644
520.379876	31253.010728	31.291661
520.843915	31305.864543	31.296679
521.617419	31359.850511	31.301696
522.131124	31422.495765	31.306714
522.256881	31466.515249	31.311732
522.965616	31521.323240	31.316749
522.995955	31567.920585	31.321767
523.812542	31624.613544	31.326784
524.370934	31690.082409	31.331802
524.473431	31745.732663	31.336820
525.031872	31814.003642	31.341837
525.301483	31886.727040	31.346855
525.864510	31935.928631	31.351872
526.258939	32014.664413	31.356890
527.112639	32066.206747	31.361908
527.932916	32140.796391	31.366925
528.396926	32193.889515	31.371943
529.123378	32259.553599	31.376960
529.874120	32328.305940	31.381978
530.223393	32380.702364	31.386996
530.988424	32440.258715	31.392013
531.256123	32502.175438	31.397031
532.120300	32557.989569	31.402048
532.470256	32616.857835	31.407066
533.191420	32674.926670	31.412084
533.857997	32735.610908	31.417101
533.851086	32796.371889	31.422119
534.634762	32851.001264	31.427136
535.187129	32907.950246	31.432154
535.866385	32963.319765	31.437172
536.271439	33026.316817	31.442189
536.477803	33094.060875	31.447207
537.337099	33159.390841	31.452224
538.179955	33219.479677	31.457242
538.230366	33273.010376	31.462260
539.153119	33332.998052	31.467277
539.184143	33395.799463	31.472295
540.157024	33457.072962	31.477312
540.624636	33510.989838	31.482330
541.133885	33571.870167	31.487348
542.413882	33612.381776	31.492365
543.099916	33657.689921	31.497383
543.765515	33710.028573	31.502400
544.434600	33748.792351	31.507418
544.880343	33810.173073	31.512436
545.470227	33849.111076	31.517453
546.067081	33899.031985	31.522471
546.421899	33927.447840	31.527488
547.356781	33978.546908	31.532506
548.083839	34012.312967	31.537524
548.832230	34050.142921	31.542541
549.086831	34099.243713	31.547559
549.758842	34123.874604	31.552576
550.103967	34160.607040	31.557594
550.620072	34203.328777	31.562612
551.232026	34234.072405	31.567629
551.490561	34285.356645	31.572647
552.165173	34327.285719	31.577664
552.687840	34384.332710	31.582682
552.745334	34428.579108	31.587700
553.291698	34465.840617	31.592717
553.233933	34519.402407	31.597735
553.960468	34571.077189	31.602752
554.250452	34629.933649	31.607770
554.492442	34684.591886	31.612788
554.987904	34728.933936	31.617805
555.348721	34797.760274	31.622823
555.830292	34857.567223	31.627840
556.201869	34923.179890	31.632858
556.521965	34994.345692	31.637876
557.667975	35057.252816	31.642893
558.031032	35131.791733	31.647911
558.836376	35190.482876	31.652928
559.705047	35263.181142	31.657946
560.150789	35335.485675	31.662964
561.127252	35393.126789	31.667981
561.389863	35447.679820	31.672999
562.040752	35499.287740	31.678016
562.569002	35563.406331	31.683034
563.118331	35634.849239	31.688052
563.780510	35687.554028	31.693069
564.203968	35758.532237	31.698087
564.910366	35816.061535	31.703104
565.395961	35872.851171	31.708122
565.920348	35936.937025	31.713140
566.420699	36007.919302	31.718157
566.937199	36073.108313	31.723175
567.740113	36132.680264	31.728192
568.432142	36190.459291	31.733210
568.804221	36253.924494	31.738228
569.600113	36320.797652	31.743245
570.333793	36382.193318	31.748263
571.143108	36435.762801	31.753280
572.061738	36480.910323	31.758298
572.553118	36535.671884	31.763316
573.154171	36581.787316	31.768333
573.810435	36637.456095	31.773351
574.190292	36689.475140	31.778368
574.924111	36749.256218	31.783386
574.848248	36813.318107	31.788404
576.002038	36869.590268	31.793421
576.147245	36924.435436	31.798439
576.833351	36990.290917	31.803456
577.150321	37044.240194	31.808474
577.565720	37103.229243	31.813492
578.526188	37171.706871	31.818509
578.925146	37237.575967	31.823527
579.390922	37294.938298	31.828544
580.499451	37355.997652	31.833562
580.632115	37417.726511	31.838580
581.365049	37484.163085	31.843597
581.982540	37545.802838	31.848615
582.439793	37613.219612	31.853632
582.839370	37672.743356	31.858650
583.020360	37740.897414	31.863668
584.074095	37809.683983	31.868685
584.238963	37880.561785	31.873703
585.019386	37953.597980	31.878720
585.487246	38019.641605	31.883738
585.615463	38088.436915	31.888756
586.946078	38149.206628	31.893773
587.450257	38223.277415	31.898791
587.889234	38297.343492	31.903808
588.935429	38359.568546	31.908826
589.197644	38435.229853	31.913844
589.554050	38496.505663	31.918861
590.413484	38563.515526	31.923879
590.910336	38638.649713	31.928896
591.350688	38687.823908	31.933914
591.922295	38749.137623	31.938932
592.610080	38815.270919	31.943949
593.713827	38864.885219	31.948967
594.685693	38910.980081	31.953984
595.281654	38959.195051	31.959002
595.659694	39018.840403	31.964020
596.431574	39074.743796	31.969037
596.723782	39129.722873	31.974055
597.241731	39191.760275	31.979072
597.724982	39245.717059	31.984090
598.184436	39312.107665	31.989108
598.340408	39383.564108	31.994125
598.905795	39459.290080	31.999143
599.607617	39522.081023	32.004160
599.782692	39597.477485	32.009178
599.830726	39669.025470	32.014196
600.467714	39753.278954	32.019213
601.073042	39840.331513	32.024231
601.647343	39924.757121	32.029248
602.561346	40007.678192	32.034266
603.098095	40096.810794	32.039284
603.540201	40178.339652	32.044301
604.115021	40267.580433	32.049319
604.790542	40361.161041	32.054336
605.727370	40439.538045	32.059354
606.289934	40528.046645	32.064372
607.502985	40593.057977	32.069389
607.720321	40669.569310	32.074407
608.505467	40749.683567	32.079424
609.330783	40824.810396	32.084442
609.981602	40908.602899	32.089460
610.574680	40981.552771	32.094477
611.385906	41055.537012	32.099495
612.101902	41130.304350	32.104512
613.545530	41196.905433	32.109530
613.654201	41258.326136	32.114548
614.686650	41325.841592	32.119565
615.232762	41366.693939	32.124583
615.802698	41431.476699	32.129600
616.509521	41484.415114	32.134618
617.280838	41561.444763	32.139636
617.940225	41622.251708	32.144653
618.570778	41691.788918	32.149671
619.059319	41751.244998	32.154688
619.599965	41799.126199	32.159706
619.970432	41864.435886	32.164724
620.712890	41931.897291	32.169741
621.623931	41996.811958	32.174759
621.696417	42069.485939	32.179776
622.367375	42135.779244	32.184794
622.423276	42197.982066	32.189812
623.022959	42271.216925	32.194829
623.644221	42345.285085	32.199847
624.319717	42432.493043	32.204864
624.963916	42510.450528	32.209882
625.378587	42594.217101	32.214900
626.402592	42663.472012	32.219917
626.734716	42732.942474	32.224935
627.262888	42808.066498	32.229952
628.210791	42880.570674	32.234970
628.644408	42962.627866	32.239988
629.526639	43039.973701	32.245005
630.307585	43112.095949	32.250023
630.543070	43193.735435	32.255040
631.946737	43244.988466	32.260058
632.251055	43312.704071	32.265076
633.136599	43371.651501	32.270093
633.794837	43433.026557	32.275111
634.168847	43504.519830	32.280128
634.889926	43560.094851	32.285146
635.473712	43633.385085	32.290164
636.240522	43684.981299	32.295181
636.538400	43745.703398	32.300199
637.129937	43808.536673	32.305216
637.904081	43869.309962	32.310234
638.726476	43947.509265	32.315252
639.097821	44021.622248	32.320269
639.423278	44085.592782	32.325287
639.914479	44151.342073	32.330304
641.189997	44213.912212	32.335322
641.627424	44287.860638	32.340340
642.327385	44361.756527	32.345357
643.123454	44432.299640	32.350375
643.278437	44501.029292	32.355392
643.885516	44569.731892	32.360410
644.850958	44649.189208	32.365428
645.529814	44717.561614	32.370445
646.328524	44784.768378	32.375463
646.884430	44869.712187	32.380480
647.623525	44937.999676	32.385498
647.987333	45012.550394	32.390516
648.396201	45079.983628	32.395533
649.291043	45154.684012	32.400551
649.362924	45250.659203	32.405568
650.498193	45324.979564	32.410586
651.125240	45405.465303	32.415604
651.402774	45488.279289	32.420621
652.291574	45565.773465	32.425639
653.289776	45641.023900	32.430656
654.323984	45714.740486	32.435674
655.327472	45783.277882	32.440692
655.735067	45859.697115	32.445709
656.601627	45938.513173	32.450727
656.914038	46000.114825	32.455744
657.775856	46072.393052	32.460762
658.549769	46139.902428	32.465780
658.827394	46207.430859	32.470797
659.315738	46284.473148	32.475815
659.985445	46373.355068	32.480832
660.400163	46446.507435	32.485850
661.062251	46526.341734	32.490868
661.681705	46616.006708	32.495885
662.163821	46691.801282	32.500903
662.637041	46785.548748	32.505920
663.300494	46857.900644	32.510938
663.992266	46942.281966	32.515956
664.092974	47034.361792	32.520973
665.176688	47134.423399	32.525991
665.912441	47231.865269	32.531008
666.790229	47299.026930	32.536026
667.436972	47392.732964	32.541044
667.984259	47481.277184	32.546061
669.080483	47564.981889	32.551079
669.681605	47662.672416	32.556096
670.310139	47754.763311	32.561114
671.121607	47826.952374	32.566132
671.799837	47915.619101	32.571149
672.482382	47995.835171	32.576167
672.973021	48084.003150	32.581184
673.712071	48166.288473	32.586202
674.775963	48248.738398	32.591220
674.914907	48330.173017	32.596237
675.969680	48405.213569	32.601255
676.590603	48490.352440	32.606272
677.166886	48567.913724	32.611290
678.046421	48648.816871	32.616308
678.767048	48723.440173	32.621325
679.692854	48779.764223	32.626343
680.252675	48842.360611	32.631360
681.361524	48905.633926	32.636378
681.893872	48975.369174	32.641396
682.355885	49044.194155	32.646413
683.135318	49110.238437	32.651431
683.482574	49184.934684	32.656448
684.453645	49254.487969	32.661466
685.285493	49307.731063	32.666484
685.508015	49391.594431	32.671501
686.459314	49465.730944	32.676519
686.658452	49541.586796	32.681536
687.345451	49624.900768	32.686554
688.009657	49703.784874	32.691572
688.530045	49794.232859	32.696589
689.232281	49889.290554	32.701607
689.778799	49972.256577	32.706624
689.978099	50061.290306	32.711642
690.842742	50154.010711	32.716660
691.133306	50249.308720	32.721677
691.679572	50348.481168	32.726695
692.466446	50457.468095	32.731712
693.138923	50552.126579	32.736730
694.110670	50651.735648	32.741748
694.878865	50748.157397	32.746765
695.680204	50847.394521	32.751783
696.577104	50942.081030	32.756800
697.490691	51037.207417	32.761818
698.822015	51116.249304	32.766836
700.226930	51185.390541	32.771853
701.169451	51257.154036	32.776871
701.758487	51322.406741	32.781888
702.589441	51399.507905	32.786906
703.332255	51471.519950	32.791924
704.149562	51538.324367	32.796941
705.039686	51592.240089	32.801959
705.281488	51664.992548	32.806976
705.977203	51732.515733	32.811994
707.016329	51797.405140	32.817012
706.896855	51867.283815	32.822029
707.926541	51952.714843	32.827047
708.456908	52029.751302	32.832064
709.072745	52111.783349	32.837082
709.665606	52185.822159	32.842100
710.033131	52263.928755	32.847117
710.681378	52359.481348	32.852135
711.343167	52443.623441	32.857152
712.139301	52524.364036	32.862170
712.901180	52613.405083	32.867188
713.536855	52703.105419	32.872205
714.526921	52781.067070	32.877223
715.066990	52877.783502	32.882240
715.402219	52963.472654	32.887258
716.693541	53049.206447	32.892276
717.022015	53129.641434	32.897293
718.116815	53216.678208	32.902311
718.484773	53300.392418	32.907328
719.279497	53373.423226	32.912346
720.264616	53472.994093	32.917364
720.780029	53564.449248	32.922381
721.354289	53650.929544	32.927399
721.953493	53737.317658	32.932416
722.409551	53833.250382	32.937434
723.007428	53930.442632	32.942452
723.684111	54039.227862	32.947469
724.097326	54132.509402	32.952487
724.748628	54243.656453	32.957504
725.271438	54335.429883	32.962522
726.449599	54411.591717	32.967540
726.950122	54509.346249	32.972557
727.857552	54601.461749	32.977575
728.231617	54713.503840	32.982592
728.855849	54816.331672	32.987610
729.955667	54903.084516	32.992628
730.420966	55005.503649	32.997645
731.663473	55086.313818	33.002663
732.367986	55185.105771	33.007680
733.055515	55285.031955	33.012698
734.040155	55379.558172	33.017716
734.964788	55475.547918	33.022733
735.688494	55558.543317	33.027751
736.543302	55652.346746	33.032768
737.409177	55751.437124	33.037786
738.325147	55841.573120	33.042804
738.946159	55916.594435	33.047821
739.919422	56000.776228	33.052839
740.405567	56095.944214	33.057856
741.092769	56197.062923	33.062874
741.995134	56275.255175	33.067892
742.511481	56374.520134	33.072909
743.468405	56445.469491	33.077927
745.114167	56528.632630	33.082944
745.487632	56606.509155	33.087962
746.183139	56682.778456	33.092980
747.163987	56781.261080	33.097997
747.742475	56866.604861	33.103015
748.555380	56950.507575	33.108032
749.105250	57025.538531	33.113050
750.214211	57099.618111	33.118068
751.061526	57176.300230	33.123085
751.965985	57256.202051	33.128103
752.783845	57333.591016	33.133120
752.802614	57425.651631	33.138138
753.940028	57511.942163	33.143156
754.156401	57593.639759	33.148173
754.713093	57677.537307	33.153191
755.094645	57776.433459	33.158208
755.645721	57884.824650	33.163226
756.592056	57983.925554	33.168244
756.950522	58090.643566	33.173261
757.560152	58192.935306	33.178279
758.012719	58300.883740	33.183296
758.604055	58428.822255	33.188314
759.705129	58535.729649	33.193332
760.084192	58651.679437	33.198349
760.633796	58769.042501	33.203367
761.752166	58887.475061	33.208384
762.780950	59018.302491	33.213402
763.578326	59136.884324	33.218420
764.339545	59245.064930	33.223437
765.364382	59347.704765	33.228455
766.960647	59440.386230	33.233472
767.804926	59541.148423	33.238490
769.002301	59633.435335	33.243508
769.337796	59739.856277	33.248525
770.276430	59823.592326	33.253543
771.187613	59905.146706	33.258560
771.903429	60006.595996	33.263578
772.948287	60097.993894	33.268596
773.242320	60199.817147	33.273613
774.168130	60296.948531	33.278631
774.932398	60391.004103	33.283648
775.528351	60478.976766	33.288666
776.687709	60561.522933	33.293684
777.760524	60644.330200	33.298701
778.269315	60727.755486	33.303719
779.394940	60803.912610	33.308736
779.909909	60890.611202	33.313754
780.466612	60955.626208	33.318772
780.838505	61046.412751	33.323789
781.412005	61121.461471	33.328807
782.375735	61221.460273	33.333824
782.538889	61323.778473	33.338842
783.234761	61421.970749	33.343860
783.926517	61532.475576	33.348877
784.394278	61633.354632	33.353895
785.193557	61738.047337	33.358912
785.394852	61860.409259	33.363930
786.419060	61983.716776	33.368948
787.609390	62102.883161	33.373965
788.062597	62212.887542	33.378983
788.650838	62325.733299	33.384000
789.449917	62439.233779	33.389018
790.309825	62566.212449	33.394036
791.033109	62696.121846	33.399053
792.032867	62821.536839	33.404071
792.746446	62941.393612	33.409088
793.193592	63064.284678	33.414106
794.157316	63193.177854	33.419124
794.978327	63321.760417	33.424141
795.475743	63443.608883	33.429159
796.882102	63572.469279	33.434176
797.752910	63689.871019	33.439194
798.479293	63817.701195	33.444212
799.082563	63956.588557	33.449229
800.100242	64089.934603	33.454247
800.887980	64210.007774	33.459264
801.781350	64334.817509	33.464282
802.678241	64449.185255	33.469300
803.353563	64576.263744	33.474317
804.263640	64698.158960	33.479335
805.750225	64819.706857	33.484352
805.906251	64949.338597	33.489370
807.449933	65048.173127	33.494388
808.910285	65167.799471	33.499405
809.411134	65272.376201	33.504423
810.449700	65384.734568	33.509440
810.975200	65509.030598	33.514458
812.143856	65614.661893	33.519476
812.913041	65711.636285	33.524493
813.487117	65825.002972	33.529511
814.358448	65931.854428	33.534528
815.517340	66040.492159	33.539546
816.515665	66140.199494	33.544564
817.183108	66235.998384	33.549581
818.050865	66337.428700	33.554599
819.023810	66451.478880	33.559616
819.439555	66554.306092	33.564634
820.304345	66654.177015	33.569652
821.992661	66745.561571	33.574669
822.784035	66849.434498	33.579687
823.562490	66928.611271	33.584704
824.149756	67044.915685	33.589722
825.175667	67132.005084	33.594740
825.755712	67229.049390	33.599757
826.193502	67324.720518	33.604775
827.324426	67423.760957	33.609792
827.996855	67525.027004	33.614810
828.899425	67637.426317	33.619828
829.555066	67741.281836	33.624845
829.873222	67851.028759	33.629863
830.859977	67949.229382	33.634880
831.366766	68047.642481	33.639898
832.240777	68138.762988	33.644916
833.318422	68243.784109	33.649933
833.487692	68355.012326	33.654951
834.292978	68466.034955	33.659968
835.026827	68566.688961	33.664986
835.885785	68674.416300	33.670004
836.547598	68787.032219	33.675021
837.489761	68897.231597	33.680039
837.995484	69010.405553	33.685056
838.578432	69145.493238	33.690074
839.429590	69278.179250	33.695092
840.186845	69408.472758	33.700109
840.776646	69542.784192	33.705127
841.716335	69659.651831	33.710144
842.531936	69803.076285	33.715162
842.763073	69942.564409	33.720180
843.230851	70088.001899	33.725197
844.287145	70236.207377	33.730215
845.084351	70377.950600	33.735232
845.706506	70529.618781	33.740250
846.512174	70684.292685	33.745268
847.678806	70848.088886	33.750285
848.407053	71007.374630	33.755303
849.274964	71149.939614	33.760320
850.090227	71313.607718	33.765338
851.121463	71473.637284	33.770356
852.269530	71626.769244	33.775373
852.769189	71781.830425	33.780391
853.795402	71932.234130	33.785408
854.841517	72085.588546	33.790426
855.952802	72231.503468	33.795444
857.303427	72376.444013	33.800461
857.792002	72522.425793	33.805479
858.775651	72668.465930	33.810496
859.854403	72821.668449	33.815514
860.879142	72965.907965	33.820532
862.535018	73095.936475	33.825549
863.360470	73216.623890	33.830567
865.143932	73336.932470	33.835584
865.750114	73460.977337	33.840602
866.705182	73581.967896	33.845620
867.910765	73709.058072	33.850637
868.768501	73836.200105	33.855655
869.564691	73944.514560	33.860672
870.192169	74069.419428	33.865690
871.139973	74186.911185	33.870708
871.614181	74314.125671	33.875725
872.312819	74452.427595	33.880743
873.858713	74570.037683	33.885760
875.240659	74684.557760	33.890778
875.998079	74783.871142	33.895796
877.566666	74874.191073	33.900813
878.127231	74983.643672	33.905831
879.197325	75083.981886	33.910848
879.537407	75209.143123	33.915866
880.143688	75317.141622	33.920884
880.925193	75428.292790	33.925901
881.250632	75547.665426	33.930919
882.393513	75665.038085	33.935936
883.111455	75794.320616	33.940954
883.719198	75937.225751	33.945972
884.481971	76042.406633	33.950989
884.997156	76174.766907	33.956007
886.234667	76308.716313	33.961024
886.785683	76441.805916	33.966042
887.444588	76588.931599	33.971060
888.342239	76721.655759	33.976077
889.245380	76862.380434	33.981095
890.019549	76982.003005	33.986112
890.563377	77116.571513	33.991130
891.042597	77256.445296	33.996148
892.561275	77391.436393	34.001165
893.050869	77527.116864	34.006183
893.802736	77666.809081	34.011200
894.919013	77798.093179	34.016218
896.105210	77934.755334	34.021236
897.038391	78071.618232	34.026253
897.449623	78220.345285	34.031271
898.608747	78356.318760	34.036288
899.560571	78494.705522	34.041306
900.264561	78651.337734	34.046324
901.656714	78789.463873	34.051341
902.474537	78937.881910	34.056359
903.668157	79070.425800	34.061376
904.186874	79207.781589	34.066394
904.893270	79358.883764	34.071412
905.994997	79504.665317	34.076429
906.388928	79664.297125	34.081447
907.299375	79812.357782	34.086464
908.084110	79970.655833	34.091482
908.683447	80136.063883	34.096500
909.630000	80293.413965	34.101517
911.224382	80453.934859	34.106535
911.649998	80615.484864	34.111552
912.591737	80785.117307	34.116570
913.191784	80948.519637	34.121588
914.109825	81111.851669	34.126605
914.809743	81272.848703	34.131623
916.332361	81443.984308	34.136640
917.808774	81598.782595	34.141658
918.340351	81764.719859	34.146676
920.268887	81910.279272	34.151693
921.507767	82061.956932	34.156711
923.003552	82182.203029	34.161728
924.535933	82325.875756	34.166746
925.353269	82448.841657	34.171764
926.138056	82571.067104	34.176781
927.463063	82708.127639	34.181799
928.196911	82842.768740	34.186816
929.099065	82974.333559	34.191834
929.561011	83097.083280	34.196852
930.904636	83213.020072	34.201869
931.881219	83347.326734	34.206887
932.688403	83475.500177	34.211904
933.595136	83614.564791	34.216922
934.204194	83757.576549	34.221940
935.618044	83881.546176	34.226957
936.150635	84021.421570	34.231975
936.496978	84153.964342	34.236992
937.474416	84298.070098	34.242010
937.877973	84453.185123	34.247028
939.074526	84601.875122	34.252045
939.356429	84750.805671	34.257063
940.124357	84900.131451	34.262080
941.093147	85058.497807	34.267098
942.293158	85208.228760	34.272116
943.528136	85360.662859	34.277133
944.677843	85517.534633	34.282151
945.669823	85666.088110	34.287168
947.079118	85811.201292	34.292186
947.483441	85964.402896	34.297204
948.487450	86099.398090	34.302221
949.407094	86257.926292	34.307239
950.235076	86413.288092	34.312256
951.425988	86551.962839	34.317274
952.505948	86699.103737	34.322292
953.633577	86828.103410	34.327309
954.436740	86958.074843	34.332327
954.969188	87090.920067	34.337344
955.862412	87229.230381	34.342362
956.418772	87378.328620	34.347380
957.195296	87526.929547	34.352397
958.208817	87677.371588	34.357415
959.553935	87814.794491	34.362432
960.925936	87958.699641	34.367450
961.853824	88110.778489	34.372468
962.755153	88245.992879	34.377485
963.765166	88406.767091	34.382503
964.517303	88559.422049	34.387520
965.482770	88699.716047	34.392538
966.217077	88857.640683	34.397556
967.437638	88992.066282	34.402573
968.309685	89153.140463	34.407591
968.952616	89309.380970	34.412608
970.167596	89474.216533	34.417626
970.683704	89634.473150	34.422644
972.018338	89791.634123	34.427661
972.180672	89961.532220	34.432679
972.936810	90132.194137	34.437696
974.020231	90309.694780	34.442714
974.689223	90490.011678	34.447732
975.345848	90666.832370	34.452749
976.313394	90863.449090	34.457767
977.417452	91051.482411	34.462784
979.011493	91222.266930	34.467802
979.865844	91425.463346	34.472820
980.847262	91601.750022	34.477837
981.889180	91776.623032	34.482855
983.346015	91959.839723	34.487872
984.438615	92122.593655	34.492890
985.122477	92310.541669	34.497908
986.279285	92490.280439	34.502925
987.569756	92662.568307	34.507943
988.699248	92832.839722	34.512960
990.002722	92997.938115	34.517978
991.729330	93163.929796	34.522996
993.455723	93299.232811	34.528013
994.830447	93444.290884	34.533031
995.922048	93592.206724	34.538048
996.664829	93732.896126	34.543066
996.873872	93890.497619	34.548084
997.668591	94045.794514	34.553101
998.672078	94209.311390	34.558119
999.281907	94368.558728	34.563136
1000.335392	94517.309303	34.568154
1000.961713	94691.265597	34.573172
1001.648725	94864.326978	34.578189
1002.773556	95055.590729	34.583207
1003.284971	95228.595058	34.588224
1004.540422	95395.762099	34.593242
1005.213736	95581.604031	34.598260
1006.193545	95764.276204	34.603277
1006.880856	95956.929462	34.608295
1007.796200	96147.356454	34.613312
1009.189949	96328.128814	34.618330
1009.919014	96523.317884	34.623348
1011.228138	96709.753311	34.628365
1012.254529	96886.406284	34.633383
1012.778975	97080.854936	34.638400
1014.329297	97261.487993	34.643418
1015.123237	97458.129641	34.648436
1016.664897	97637.361563	34.653453
1017.980276	97807.370958	34.658471
1018.653722	97983.513943	34.663488
1019.959633	98143.088516	34.668506
1020.848546	98311.595497	34.673524
1021.751591	98488.786637	34.678541
1022.891700	98641.941054	34.683559
1024.011765	98820.035620	34.688576
1024.871893	98984.019226	34.693594
1025.480597	99168.999711	34.698612
1026.868804	99343.863098	34.703629
1027.789734	99504.579777	34.708647
1028.284500	99684.714560	34.713664
1030.149119	99852.431395	34.718682
1031.251622	100043.616911	34.723700
1031.931580	100217.837255	34.728717
1033.183999	100387.735240	34.733735
1033.599668	100568.661748	34.738752
1035.133032	100741.231702	34.743770
1036.498947	100922.478681	34.748788
1037.170040	101102.328531	34.753805
1038.121963	101290.617011	34.758823
1038.691806	101485.111208	34.763840
1039.851049	101662.940750	34.768858
1040.906362	101858.193365	34.773876
1041.973680	102045.354055	34.778893
1042.926990	102245.197678	34.783911
1043.609118	102447.113683	34.788928
1044.663679	102641.789901	34.793946
1045.621883	102849.773362	34.798964
1046.997064	103050.750262	34.803981
1048.960004	103222.404955	34.808999
1050.421202	103402.431761	34.814016
1051.846222	103577.906972	34.819034
1052.585421	103780.343201	34.824052
1053.335210	103944.490900	34.829069
1054.224240	104146.917920	34.834087
1054.906965	104345.777732	34.839104
1055.968140	104531.361840	34.844122
1057.196054	104733.262585	34.849140
1057.659349	104928.598168	34.854157
1059.047661	105128.905155	34.859175
1060.254493	105328.369805	34.864192
1061.440294	105533.462420	34.869210
1062.586339	105710.916723	34.874228
1063.973239	105913.433562	34.879245
1065.274104	106101.604478	34.884263
1066.046249	106299.223252	34.889280
1067.278984	106477.782921	34.894298
1068.562409	106676.092671	34.899316
1069.373997	106857.523380	34.904333
1070.203308	107055.176375	34.909351
1071.676693	107253.243792	34.914368
1072.298385	107439.370624	34.919386
1073.491417	107636.220659	34.924404
1074.141961	107843.965343	34.929421
1075.462251	108044.951668	34.934439
1076.220534	108247.172197	34.939456
1077.249302	108442.396112	34.944474
1078.184128	108653.165281	34.949492
1078.980571	108866.758130	34.954509
1080.190326	109061.893360	34.959527
1081.717850	109271.594268	34.964544
1083.230791	109461.463908	34.969562
1084.585018	109666.877330	34.974580
1085.380239	109859.160865	34.979597
1086.886027	110053.203112	34.984615
1087.444861	110250.937059	34.989632
1088.872318	110446.489722	34.994650
1089.941073	110638.429648	34.999668
1090.789308	110829.216652	35.004685
1092.553362	110996.622628	35.009703
1093.883728	111155.538327	35.014720
1095.188841	111325.834174	35.019738
1096.126254	111505.324824	35.024756
1096.872468	111677.171857	35.029773
1098.215802	111850.124797	35.034791
1098.787229	112033.656883	35.039808
1099.829884	112214.654912	35.044826
1101.008494	112399.761330	35.049844
1102.434703	112570.184290	35.054861
1103.863867	112736.148774	35.059879
1104.639730	112923.985440	35.064896
1105.456612	113107.167489	35.069914
1106.927043	113294.081273	35.074932
1108.068856	113474.817873	35.079949
1109.159579	113653.068460	35.084967
1110.272930	113825.071012	35.089984
1111.320792	114017.202756	35.095002
1111.897999	114199.430808	35.100020
1112.604320	114391.976242	35.105037
1113.656886	114585.656699	35.110055
1114.227258	114811.406547	35.115072
1115.230752	115021.326739	35.120090
1116.057368	115239.981235	35.125108
1116.852391	115462.633387	35.130125
1117.782235	115692.410421	35.135143
1118.580514	115932.245062	35.140160
1119.530706	116176.212207	35.145178
1120.798640	116410.398896	35.150196
1121.685713	116652.974281	35.155213
1123.149294	116889.919949	35.160231
1124.438987	117126.744271	35.165248
1125.672258	117364.352745	35.170266
1126.759369	117608.664401	35.175284
1128.134764	117852.461775	35.180301
1130.797943	118041.364245	35.185319
1132.629904	118264.842894	35.190336
1133.861383	118466.033924	35.195354
1135.081939	118662.489435	35.200372
1135.748603	118877.029854	35.205389
1136.886759	119089.606125	35.210407
1137.847304	119310.715330	35.215424
1138.897654	119535.270539	35.220442
1140.104390	119747.447551	35.225460
1140.936568	119971.522661	35.230477
1142.634215	120163.411457	35.235495
1143.335653	120394.518533	35.240512
1144.206275	120615.956675	35.245530
1145.453127	120832.291191	35.250548
1146.894778	121061.988904	35.255565
1148.362050	121274.032702	35.260583
1149.205693	121482.899026	35.265600
1150.597628	121689.471450	35.270618
1152.185673	121906.315163	35.275636
1153.294778	122110.250811	35.280653
1154.164980	122325.695486	35.285671
1155.722808	122529.433251	35.290688
1156.935716	122735.358291	35.295706
1158.678434	122940.132841	35.300724
1160.584786	123118.548625	35.305741
1161.979631	123293.324224	35.310759
1163.333399	123480.856183	35.315776
1164.326236	123669.817547	35.320794
1165.587222	123853.147201	35.325812
1166.241569	124043.332698	35.330829
1167.170111	124213.438403	35.335847
1168.206312	124416.996450	35.340864
1168.583200	124599.868331	35.345882
1169.619751	124787.372167	35.350900
1170.574742	124971.266120	35.355917
1171.492208	125159.641042	35.360935
1172.050595	125374.474925	35.365952
1173.313746	125579.460831	35.370970
1174.476811	125787.759760	35.375988
1175.161181	125997.888097	35.381005
1176.059104	126205.828120	35.386023
1177.138488	126432.813620	35.391040
1178.244227	126649.517974	35.396058
1179.870288	126880.193388	35.401076
1180.779594	127121.559018	35.406093
1181.682064	127351.343518	35.411111
1183.022110	127577.255245	35.416128
1184.100823	127811.589510	35.421146
1185.378506	128035.575739	35.426164
1186.188793	128281.871866	35.431181
1187.198564	128524.651512	35.436199
1189.205271	128762.261994	35.441216
1190.138399	128997.592602	35.446234
1191.830077	129227.108752	35.451252
1193.135730	129465.220604	35.456269
1194.932027	129696.180585	35.461287
1196.215708	129920.040060	35.466304
1197.470709	130154.844653	35.471322
1198.404025	130374.113388	35.476340
1199.621364	130610.892310	35.481357
1200.885953	130847.880706	35.486375
1202.147715	131078.115229	35.491392
1202.965035	131309.426184	35.496410
1204.531356	131538.587068	35.501428
1206.377760	131762.100621	35.506445
1207.465533	131969.363551	35.511463
1208.978478	132198.069018	35.516480
1209.855457	132427.502243	35.521498
1211.174356	132647.559778	35.526516
1212.338225	132884.922338	35.531533
1213.145100	133111.963553	35.536551
1214.373414	133350.256994	35.541568
1215.859835	133583.527677	35.546586
1217.133629	133808.874152	35.551604
1217.929487	134060.504140	35.556621
1219.070868	134278.662634	35.561639
1220.463016	134502.447843	35.566656
1221.600203	134737.888926	35.571674
1222.833142	134975.217498	35.576692
1224.434547	135219.015800	35.581709
1225.514743	135452.075465	35.586727
1226.864887	135688.477130	35.591744
1227.518117	135930.015863	35.596762
1228.767354	136176.706563	35.601780
1230.125538	136424.851760	35.606797
1231.436402	136655.929558	35.611815
1232.591477	136904.149936	35.616832
1233.298871	137148.287676	35.621850
1234.504678	137399.799705	35.626868
1235.675039	137663.845605	35.631885
1236.616423	137921.452766	35.636903
1237.557596	138172.177564	35.641920
1238.634939	138437.766382	35.646938
1240.297075	138698.163974	35.651956
1240.927627	138974.011754	35.656973
1242.292743	139233.473595	35.661991
1244.093837	139497.201679	35.667008
1245.491866	139752.680907	35.672026
1247.104914	140015.772102	35.677044
1248.430890	140267.311227	35.682061
1249.740686	140504.755480	35.687079
1251.447924	140736.924558	35.692096
1252.386104	140974.230560	35.697114
1253.640701	141205.285672	35.702132
1254.760007	141455.333469	35.707149
1255.795741	141680.468470	35.712167
1257.470357	141909.519010	35.717184
1258.375860	142145.507147	35.722202
1260.169316	142374.148091	35.727220
1261.177852	142616.589258	35.732237
1262.114634	142863.329874	35.737255
1263.323844	143115.758772	35.742272
1264.331022	143356.607627	35.747290
1266.078422	143604.487756	35.752308
1267.339501	143850.433709	35.757325
1268.493104	144113.606772	35.762343
1270.699283	144358.144924	35.767360
1270.931253	144609.997766	35.772378
1272.642778	144833.646790	35.777396
1274.180096	145080.177141	35.782413
1275.115560	145330.815775	35.787431
1276.843693	145578.028246	35.792448
1277.393771	145848.085629	35.797466
1278.864615	146104.195762	35.802484
1280.031167	146373.787625	35.807501
1280.823160	146633.944860	35.812519
1282.282762	146897.925106	35.817536
1282.942153	147178.741224	35.822554
1284.310080	147447.394841	35.827572
1285.721774	147718.528895	35.832589
1287.052550	147998.302121	35.837607
1288.275000	148274.049788	35.842624
1289.280766	148569.505448	35.847642
1290.715121	148845.501483	35.852660
1291.930456	149126.228250	35.857677
1293.141618	149415.620024	35.862695
1294.494740	149691.547069	35.867712
1296.275484	149979.733208	35.872730
1297.816429	150243.445298	35.877748
1299.971398	150528.010085	35.882765
1301.394339	150796.133878	35.887783
1302.976004	151058.678216	35.892800
1303.530174	151333.062516	35.897818
1305.168276	151611.468095	35.902836
1306.078251	151887.509980	35.907853
1306.991277	152168.880444	35.912871
1308.534623	152448.614270	35.917888
1309.315949	152728.006643	35.922906
1310.719434	153005.953916	35.927924
1311.861083	153302.553637	35.932941
1313.040900	153592.566405	35.937959
1314.647734	153884.844763	35.942976
1315.960012	154166.214881	35.947994
1317.720490	154452.244306	35.953012
1318.940289	154738.200200	35.958029
1320.425945	155035.872790	35.963047
1321.417153	155320.006111	35.968064
1323.063527	155608.967694	35.973082
1324.270207	155886.651191	35.978100
1325.900132	156165.306964	35.983117
1327.089032	156453.931718	35.988135
1328.629590	156735.663358	35.993152
1329.817591	157012.698309	35.998170
1331.256393	157293.017323	36.003188
1332.586319	157573.787593	36.008205
1333.547094	157874.663602	36.013223
1334.881291	158153.407614	36.018240
1336.344211	158432.145018	36.023258
1337.684130	158700.895729	36.028276
1339.508449	158966.625219	36.033293
1340.586747	159238.340416	36.038311
1342.031710	159483.914827	36.043328
1343.620222	159748.407126	36.048346
1344.956118	159998.582285	36.053364
1346.003928	160271.971327	36.058381
1347.177698	160544.897400	36.063399
1348.722088	160806.562165	36.068416
1349.764407	161090.563308	36.073434
1350.901688	161360.684476	36.078452
1352.171364	161626.294541	36.083469
1353.363501	161913.334084	36.088487
1354.378776	162191.853983	36.093504
1355.768522	162496.524817	36.098522
1357.341264	162782.581422	36.103540
1358.574235	163085.290596	36.108557
1360.276882	163363.273521	36.113575
1361.854888	163647.685854	36.118592
1363.387702	163923.607136	36.123610
1364.768517	164210.669374	36.128628
1366.396805	164502.222109	36.133645
1367.335308	164801.934539	36.138663
1368.937645	165089.943091	36.143680
1370.107412	165379.661679	36.148698
1371.565550	165682.326864	36.153716
1372.827090	165970.740143	36.158733
1374.107382	166269.416765	36.163751
1374.939243	166580.971636	36.168768
1376.140236	166888.826340	36.173786
1377.673508	167192.606230	36.178804
1379.266606	167500.730429	36.183821
1380.355065	167809.993208	36.188839
1382.029436	168125.201159	36.193856
1383.140710	168453.027871	36.198874
1384.516654	168767.426826	36.203892
1385.908803	169097.800421	36.208909
1386.625708	169422.108446	36.213927
1388.334685	169743.476223	36.218944
1389.784313	170060.295682	36.223962
1391.202237	170392.768234	36.228980
1392.800668	170723.132411	36.233997
1393.850767	171054.350837	36.239015
1395.534039	171385.441793	36.244032
1396.819110	171721.486297	36.249050
1398.029385	172055.527961	36.254068
1399.863564	172382.096401	36.259085
1401.064408	172720.763453	36.264103
1402.986323	173047.943896	36.269120
1404.668674	173384.531317	36.274138
1406.198656	173698.672323	36.279156
1408.185155	174003.032182	36.284173
1409.407555	174335.704944	36.289191
1410.836935	174650.731819	36.294208
1412.059632	174974.728881	36.299226
1413.637691	175297.819238	36.304244
1415.142646	175586.494516	36.309261
1416.272398	175905.525846	36.314279
1417.807340	176220.050684	36.319296
1419.602789	176543.278496	36.324314
1420.679881	176867.223473	36.329332
1422.294271	177182.591710	36.334349
1423.513057	177504.651959	36.339367
1424.891664	177816.522390	36.344384
1426.255985	178128.879411	36.349402
1427.600481	178447.866496	36.354420
1428.855555	178767.009985	36.359437
1429.961366	179102.437827	36.364455
1431.450192	179419.833562	36.369472
1432.493736	179731.453970	36.374490
1433.228119	180039.332517	36.379508
1435.091213	180366.686131	36.384525
1436.249429	180689.551047	36.389543
1437.872505	181020.844845	36.394560
1438.916232	181350.802194	36.399578
1440.501680	181677.613471	36.404596
1442.190670	182004.600104	36.409613
1443.417048	182344.243106	36.414631
1445.370621	182671.685255	36.419648
1446.904978	183003.158645	36.424666
1447.839304	183340.749356	36.429684
1449.180930	183683.593171	36.434701
1450.192651	184031.050284	36.439719
1452.105517	184374.654680	36.444736
1453.273269	184723.664430	36.449754
1454.591276	185076.218334	36.454772
1456.330582	185424.249786	36.459789
1457.896933	185779.420096	36.464807
1459.481818	186125.476008	36.469824
1461.918685	186469.641845	36.474842
1463.332385	186810.792667	36.479860
1464.979306	187166.631369	36.484877
1466.346380	187513.150783	36.489895
1467.790327	187864.800520	36.494912
1469.364634	188209.881057	36.499930
1470.426024	188543.801770	36.504948
1472.297404	188881.424283	36.509965
1473.519123	189248.135950	36.514983
1474.683779	189597.392592	36.520000
1476.106624	189955.951496	36.525018
1477.435646	190320.494299	36.530036
1479.187290	190681.009078	36.535053
1480.294731	191046.164209	36.540071
1481.682669	191404.572740	36.545088
1482.960678	191768.561707	36.550106
1484.360960	192152.374119	36.555124
1485.762599	192522.275583	36.560141
1487.700696	192891.164090	36.565159
1489.797771	193260.409455	36.570176
1491.136294	193619.194821	36.575194
1492.519987	193989.425563	36.580212
1494.319030	194346.323831	36.585229
1496.012398	194711.023611	36.590247
1497.936307	195077.464795	36.595264
1499.932658	195422.720726	36.600282
1501.277257	195772.694454	36.605300
1503.264532	196106.809266	36.610317
1504.920576	196463.044952	36.615335
1506.184344	196809.940075	36.620352
1507.986578	197154.564598	36.625370
1509.297651	197501.112859	36.630388
1510.531192	197856.461113	36.635405
1511.683087	198201.553983	36.640423
1513.486762	198540.091686	36.645440
1514.600151	198897.407843	36.650458
1516.041727	199264.599930	36.655476
1517.841911	199598.319177	36.660493
1519.494263	199966.038948	36.665511
1520.926064	200309.585725	36.670528
1522.741571	200665.221113	36.675546
1524.062656	201015.125081	36.680564
1525.295549	201363.318690	36.685581
1526.717393	201722.528669	36.690599
1527.994235	202078.272922	36.695616
1529.160533	202441.439251	36.700634
1530.721946	202806.256282	36.705652
1532.232129	203142.021177	36.710669
1534.359953	203497.086196	36.715687
1535.484273	203843.253115	36.720704
1537.184473	204180.794446	36.725722
1538.502681	204526.526340	36.730740
1540.334241	204860.278187	36.735757
1541.953905	205205.277906	36.740775
1543.102334	205550.103050	36.745792
1544.588297	205905.831652	36.750810
1545.753706	206257.805700	36.755828
1547.379434	206628.243307	36.760845
1548.808724	206995.718585	36.765863
1550.572213	207357.820315	36.770880
1552.617223	207707.014874	36.775898
1554.027480	208062.461292	36.780916
1555.717976	208425.087946	36.785933
1557.315185	208790.093407	36.790951
1558.739919	209143.675786	36.795968
1560.148988	209514.670786	36.800986
1561.429127	209893.535954	36.806004
1563.202427	210257.719095	36.811021
1564.651025	210623.341503	36.816039
1565.705732	211015.797654	36.821056
1567.357165	211388.284932	36.826074
1569.104474	211781.125634	36.831092
1570.869421	212151.692879	36.836109
1572.461550	212541.692968	36.841127
1573.993479	212922.790658	36.846144
1576.022313	213299.744614	36.851162
1577.309850	213697.190558	36.856180
1579.082022	214074.317197	36.861197
1580.864683	214456.065929	36.866215
1582.206102	214851.374850	36.871232
1584.096353	215229.350395	36.876250
1585.205536	215620.231136	36.881268
1586.944079	216015.860571	36.886285
1588.704434	216404.656228	36.891303
1589.902971	216812.975242	36.896320
1591.584455	217199.653839	36.901338
1592.920998	217605.007399	36.906356
1595.408791	217977.892190	36.911373
1597.392336	218360.969966	36.916391
1598.879266	218815.499425	36.921408
1600.801705	219204.330525	36.926426
1602.384073	219588.292017	36.931444
1603.826687	219964.429980	36.936461
1605.410521	220360.763124	36.941479
1607.062648	220743.295182	36.946496
1608.715888	221128.749307	36.951514
1610.229043	221523.981046	36.956532
1612.197512	221912.713266	36.961549
1613.414813	222289.963590	36.966567
1614.560159	222686.047701	36.971584
1615.973487	223081.936647	36.976602
1617.445594	223488.078558	36.981620
1618.971207	223898.327797	36.986637
1620.542023	224297.471594	36.991655
1622.028028	224701.913858	36.996672
1623.592109	225112.923127	37.001690
1624.992340	225538.768824	37.006708
1626.393575	225947.852136	37.011725
1628.094507	226377.816785	37.016743
1629.623380	226793.358862	37.021760
1631.686456	227214.630794	37.026778
1633.147729	227632.879262	37.031796
1634.187031	228051.325752	37.036813
1636.201437	228482.897022	37.041831
1637.836587	228914.989524	37.046848
1639.641109	229306.846803	37.051866
1641.232655	229714.082227	37.056884
1642.750524	230102.941108	37.061901
1644.727281	230506.584714	37.066919
1646.374640	230903.705097	37.071936
1648.019744	231306.643748	37.076954
1649.792805	231713.753567	37.081972
1651.463314	232107.749234	37.086989
1653.341555	232509.712986	37.092007
1654.687257	232924.415389	37.097024
1656.567865	233326.838188	37.102042
1658.063612	233739.435200	37.107060
1659.513245	234136.114388	37.112077
1660.837943	234565.303391	37.117095
1662.110774	234993.994087	37.122112
1663.982470	235413.290209	37.127130
1665.136533	235860.266378	37.132148
1666.515524	236293.667623	37.137165
1668.024227	236733.297361	37.142183
1669.657717	237187.589778	37.147200
1671.539191	237624.899508	37.152218
1672.918076	238092.318118	37.157236
1675.003828	238546.005907	37.162253
1677.235771	238986.334679	37.167271
1678.997425	239437.512485	37.172288
1681.316287	239867.109298	37.177306
1682.734443	240317.939355	37.182324
1685.028662	240762.224534	37.187341
1686.860563	241196.730891	37.192359
1688.643736	241641.534073	37.197376
1690.480335	242069.640051	37.202394
1692.480037	242508.922363	37.207412
1694.155202	242945.617214	37.212429
1696.129711	243366.209161	37.217447
1697.431930	243807.209327	37.222464
1699.362350	244229.613611	37.227482
1701.163897	244662.785138	37.232500
1703.198564	245098.357573	37.237517
1705.025605	245513.795281	37.242535
1706.336599	245947.583272	37.247552
1707.945390	246379.976451	37.252570
1709.354855	246825.409357	37.257588
1710.380134	247273.598997	37.262605
1712.346261	247720.795762	37.267623
1713.983205	248159.435888	37.272640
1715.738019	248601.740558	37.277658
1717.692425	249051.582929	37.282676
1718.979577	249502.323434	37.287693
1721.182302	249957.257335	37.292711
1722.745291	250416.920651	37.297728
1725.044324	250855.124501	37.302746
1726.760559	251290.910043	37.307764
1728.674719	251734.766935	37.312781
1730.692581	252177.895845	37.317799
1732.471994	252619.235461	37.322816
1733.928767	253055.217803	37.327834
1735.388128	253502.860109	37.332852
1736.835291	253955.102737	37.337869
1738.788254	254401.444906	37.342887
1740.503547	254857.174958	37.347904
1742.118093	255294.225130	37.352922
1744.213485	255740.824039	37.357940
1745.547793	256195.093499	37.362957
1747.177833	256662.346255	37.367975
1748.746319	257123.563381	37.372992
1750.411961	257580.471491	37.378010
1752.182883	258037.692615	37.383028
1754.012789	258482.964574	37.388045
1755.857470	258911.798248	37.393063
1757.645191	259350.751899	37.398080
1759.259205	259777.870908	37.403098
1761.488362	260211.671142	37.408116
1763.026614	260640.199862	37.413133
1765.207109	261077.564578	37.418151
1766.530417	261517.356969	37.423168
1768.529524	261948.629323	37.428186
1770.586377	262372.499717	37.433204
1771.776027	262809.519570	37.438221
1773.456454	263245.391404	37.443239
1775.116264	263691.707249	37.448256
1776.635439	264141.018313	37.453274
1777.948134	264592.166881	37.458292
1779.328621	265058.749223	37.463309
1781.319539	265534.883834	37.468327
1783.071176	266006.027795	37.473344
1785.062920	266460.568956	37.478362
1786.808940	266935.472883	37.483380
1789.096968	267405.079383	37.488397
1791.239009	267879.764808	37.493415
1793.123060	268341.638403	37.498432
1794.752431	268811.326938	37.503450
1796.602098	269281.181897	37.508468
1798.254445	269760.518851	37.513485
1800.196909	270233.202633	37.518503
1801.796616	270724.969244	37.523520
1803.061861	271199.668832	37.528538
1805.178141	271688.148222	37.533556
1806.650425	272182.982291	37.538573
1808.590717	272673.140532	37.543591
1810.272339	273177.845713	37.548608
1811.768470	273674.401006	37.553626
1813.893704	274171.842418	37.558644
1815.484655	274677.017333	37.563661
1817.630699	275176.638217	37.568679
1819.363871	275688.316317	37.573696
1821.288721	276185.101335	37.578714
1823.031274	276696.877526	37.583732
1825.331956	277213.107629	37.588749
1827.348580	277710.052288	37.593767
1829.351267	278223.331882	37.598784
1831.340822	278706.460009	37.603802
1833.835638	279208.275964	37.608820
1835.348442	279697.323059	37.613837
1837.488078	280190.761785	37.618855
1839.161275	280692.709741	37.623872
1841.053916	281191.749821	37.628890
1842.658389	281673.283458	37.633908
1844.326530	282186.938689	37.638925
1845.911628	282690.851933	37.643943
1847.584165	283213.317991	37.648960
1849.307961	283727.137519	37.653978
1850.909897	284233.914010	37.658996
1852.409594	284758.537684	37.664013
1854.332210	285276.536393	37.669031
1855.943372	285801.189175	37.674048
1857.626119	286339.824497	37.679066
1859.506714	286871.846444	37.684084
1861.442734	287410.487077	37.689101
1863.342221	287937.802995	37.694119
1864.842927	288487.738764	37.699136
1867.030339	289015.638327	37.704154
1868.924946	289559.866050	37.709172
1870.745471	290103.494260	37.714189
1872.635856	290633.062342	37.719207
1874.460300	291177.168220	37.724224
1876.476913	291704.272799	37.729242
1878.855720	292232.509304	37.734260
1880.192067	292741.916357	37.739277
1882.236141	293248.588415	37.744295
1884.155943	293766.988225	37.749312
1885.575078	294286.255813	37.754330
1887.920721	294800.567801	37.759348
1889.541856	295328.281005	37.764365
1891.665606	295846.968330	37.769383
1893.633565	296360.573760	37.774400
1895.313862	296886.212713	37.779418
1897.194019	297415.600681	37.784436
1898.690924	297958.053562	37.789453
1900.921253	298481.765446	37.794471
1902.918143	299016.028317	37.799488
1904.207000	299558.913780	37.804506
1906.639979	300089.670444	37.809524
1908.588994	300637.851204	37.814541
1910.841614	301161.520528	37.819559
1912.917403	301710.893641	37.824576
1914.550070	302257.593822	37.829594
1916.743771	302793.378971	37.834612
1918.449827	303344.657887	37.839629
1920.749179	303875.924170	37.844647
1922.787488	304424.068886	37.849664
1924.454047	304971.103410	37.854682
1926.507834	305516.369193	37.859700
1927.957149	306080.245660	37.864717
1929.797945	306634.428665	37.869735
1931.748604	307198.393106	37.874752
1933.749093	307757.596565	37.879770
1935.618059	308326.595602	37.884788
1937.409956	308900.962095	37.889805
1939.477609	309457.324347	37.894823
1941.726748	310027.569745	37.899840
1943.888895	310590.460850	37.904858
1945.770556	311153.470505	37.909876
1947.386816	311740.899279	37.914893
1949.456649	312317.735404	37.919911
1951.580426	312891.358659	37.924928
1953.709617	313465.002178	37.929946
1955.900562	314035.660089	37.934964
1957.545109	314611.050969	37.939981
1959.574443	315194.677800	37.944999
1961.752427	315764.512121	37.950016
1963.846121	316343.218285	37.955034
1966.136005	316900.176175	37.960052
1968.050932	317470.015156	37.965069
1970.321145	318033.544323	37.970087
1972.035676	318604.854657	37.975104
1973.685380	319184.906057	37.980122
1975.913273	319748.682326	37.985140
1977.926326	320325.007718	37.990157
1980.043994	320887.040721	37.995175
1982.483260	321453.992765	38.000192
1984.224677	322032.379692	38.005210
1986.499637	322592.696554	38.010228
1988.580809	323163.400129	38.015245
1990.409256	323745.490063	38.020263
1992.064044	324304.472559	38.025280
1993.988790	324877.370325	38.030298
1995.905597	325439.752699	38.035316
1997.823204	326017.338439	38.040333
1999.587380	326591.821188	38.045351
2001.556306	327170.276335	38.050368
2003.489251	327758.075151	38.055386
2005.588075	328325.986756	38.060404
2007.612465	328913.479939	38.065421
2009.431249	329490.871247	38.070439
2011.214131	330061.331850	38.075456
2012.699737	330625.488937	38.080474
2014.480649	331192.562195	38.085492
2016.539704	331759.609380	38.090509
2018.222906	332344.357019	38.095527
2020.668757	332921.305987	38.100544
2022.277895	333499.275564	38.105562
2024.599342	334080.193421	38.110580
2026.521497	334664.572773	38.115597
2028.726545	335238.998759	38.120615
2031.052596	335826.319991	38.125632
2033.129146	336413.929840	38.130650
2035.393639	337007.543887	38.135668
2037.104359	337591.291823	38.140685
2038.921489	338170.015015	38.145703
2041.192071	338776.706543	38.150720
2043.030730	339386.000615	38.155738
2045.293917	339981.510343	38.160756
2047.029545	340590.857890	38.165773
2048.862991	341198.633637	38.170791
2051.166125	341824.295516	38.175808
2052.289494	342448.392766	38.180826
2054.724744	343072.468866	38.185844
2056.488548	343704.972997	38.190861
2058.281207	344344.266393	38.195879
2060.524351	344975.583574	38.200896
2062.414570	345629.742542	38.205914
2064.501723	346274.520116	38.210932
2066.970523	346910.444506	38.215949
2069.185882	347554.802768	38.220967
2071.575362	348205.315978	38.225984
2073.615310	348866.308451	38.231002
2075.651281	349527.799664	38.236020
2077.961908	350165.811924	38.241037
2079.862742	350807.004273	38.246055
2082.245798	351452.117609	38.251072
2084.101509	352118.447745	38.256090
2086.524368	352759.069227	38.261108
2088.768343	353414.200806	38.266125
2090.868811	354073.355654	38.271143
2093.091669	354718.676000	38.276160
2094.933139	355391.074197	38.281178
2097.245815	356033.974731	38.286196
2099.615077	356686.447761	38.291213
2101.627898	357350.666937	38.296231
2104.146886	357996.497742	38.301248
2105.783211	358663.473157	38.306266
2108.125014	359312.941104	38.311284
2110.038978	359965.996129	38.316301
2111.884059	360621.157963	38.321319
2114.434940	361279.567256	38.326336
2116.407804	361938.340214	38.331354
2118.903955	362600.847036	38.336372
2121.162521	363248.464250	38.341389
2123.531516	363900.771464	38.346407
2125.648232	364541.997611	38.351424
2127.332447	365202.920249	38.356442
2129.773120	365859.470323	38.361460
2131.778425	366523.412445	38.366477
2133.606508	367183.617866	38.371495
2136.296939	367836.998025	38.376512
2137.911840	368501.325218	38.381530
2139.780703	369161.641642	38.386548
2141.813354	369817.683277	38.391565
2143.777451	370496.274629	38.396583
2146.266900	371159.471735	38.401600
2148.208200	371837.484115	38.406618
2150.111878	372494.919775	38.411636
2152.262697	373155.397143	38.416653
2154.245194	373803.335373	38.421671
2156.222061	374457.070909	38.426688
2158.001470	375124.142241	38.431706
2160.187460	375783.931215	38.436724
2162.114086	376436.624070	38.441741
2164.197010	377102.010164	38.446759
2166.572574	377765.027501	38.451776
2168.517489	378442.558317	38.456794
2171.319061	379099.013027	38.461812
2173.349677	379777.771351	38.466829
2175.885695	380446.644460	38.471847
2178.310926	381102.209722	38.476864
2180.402965	381776.556308	38.481882
2182.680239	382456.513362	38.486900
2184.971636	383130.977230	38.491917
2186.870000	383804.122962	38.496935
2188.730035	384487.251270	38.501952
2190.749549	385176.804515	38.506970
2192.589725	385866.448804	38.511988
2194.875118	386583.944794	38.517005
2196.892915	387291.733325	38.522023
2199.493601	387990.638102	38.527040
2201.680891	388708.229456	38.532058
2203.749386	389413.554042	38.537076
2206.157459	390122.634824	38.542093
2207.793465	390840.952982	38.547111
2210.320445	391562.555220	38.552128
2212.389044	392289.108618	38.557146
2214.346765	393030.289259	38.562164
2216.756170	393758.019147	38.567181
2219.005412	394501.473383	38.572199
2221.453561	395229.947390	38.577216
2223.474069	395979.967751	38.582234
2225.630722	396723.686575	38.587252
2228.255131	397464.014885	38.592269
2230.220491	398213.202448	38.597287
2232.785919	398947.141952	38.602304
2234.593468	399710.889878	38.607322
2236.826866	400459.519664	38.612340
2239.172631	401218.704352	38.617357
2241.227149	401976.396628	38.622375
2243.554783	402749.709426	38.627392
2245.630543	403512.552244	38.632410
2247.365884	404274.290441	38.637428
2250.136192	405053.118015	38.642445
2252.060225	405832.266219	38.647463
2254.220123	406605.501009	38.652480
2256.582028	407391.424958	38.657498
2258.877858	408173.917175	38.662516
2261.413255	408959.919766	38.667533
2263.723193	409735.246051	38.672551
2266.181332	410515.997726	38.677568
2268.438228	411318.419187	38.682586
2270.976252	412100.125105	38.687604
2273.342622	412880.367290	38.692621
2275.594542	413652.246531	38.697639
2277.800077	414425.529360	38.702656
2280.460918	415216.267146	38.707674
2282.632777	416003.110550	38.712692
2285.498716	416764.412679	38.717709
2287.793682	417538.728376	38.722727
2290.748328	418299.362873	38.727744
2293.126264	419054.853011	38.732762
2295.102934	419811.399945	38.737780
2298.358337	420561.332047	38.742797
2300.564730	421321.088127	38.747815
2302.680557	422052.956878	38.752832
2305.215240	422775.189142	38.757850
2307.234762	423480.495462	38.762868
2309.859761	424198.113901	38.767885
2311.455158	424924.970792	38.772903
2314.031953	425628.604861	38.777920
2316.605123	426334.700452	38.782938
2318.789581	427038.763743	38.787956
2321.700680	427742.028621	38.792973
2324.113203	428453.405531	38.797991
2326.247234	429150.378084	38.803008
2328.486894	429882.499148	38.808026
2330.586160	430601.913812	38.813044
2332.366185	431308.348875	38.818061
2334.412540	432036.689338	38.823079
2336.955058	432767.355340	38.828096
2339.157587	433507.115617	38.833114
2341.334792	434252.374057	38.838132
2343.303611	435002.856514	38.843149
2345.346602	435760.135467	38.848167
2347.557517	436516.147180	38.853184
2349.489861	437290.248274	38.858202
2351.387874	438075.007512	38.863220
2353.672238	438863.167975	38.868237
2355.243887	439672.268327	38.873255
2357.531076	440475.149187	38.878272
2359.901481	441288.664788	38.883290
2361.966765	442122.694396	38.888308
2364.308165	442931.853830	38.893325
2366.688657	443776.698721	38.898343
2369.469536	444613.046482	38.903360
2371.754301	445444.941403	38.908378
2374.436889	446284.024196	38.913396
2377.372396	447119.643456	38.918413
2379.599497	447960.254230	38.923431
2382.451497	448802.449101	38.928448
2384.767867	449646.317894	38.933466
2386.671822	450498.567255	38.938484
2389.445626	451339.511634	38.943501
2391.620843	452198.678501	38.948519
2394.063651	453060.750157	38.953536
2396.449507	453908.989348	38.958554
2398.394249	454775.624070	38.963572
2401.030768	455637.405717	38.968589
2403.672209	456504.005071	38.973607
2406.341533	457362.675300	38.978624
2408.956882	458219.397105	38.983642
2411.185176	459090.000309	38.988660
2414.115245	459945.788663	38.993677
2416.410613	460804.779944	38.998695
2418.755024	461670.601850	39.003712
2421.275012	462531.049519	39.008730
2423.083177	463418.217049	39.013748
2425.994163	464283.630081	39.018765
2428.131051	465158.584822	39.023783
2430.682242	466031.562345	39.028800
2432.990032	466903.783061	39.033818
2434.956137	467792.749333	39.038836
2437.420373	468680.430546	39.043853
2439.835999	469570.605775	39.048871
2442.533380	470457.712127	39.053888
2444.902039	471342.153660	39.058906
2447.617733	472231.398147	39.063924
2450.610444	473114.290428	39.068941
2453.140747	474002.168959	39.073959
2455.407346	474879.692715	39.078976
2458.238048	475754.304066	39.083994
2460.520514	476639.269942	39.089012
2463.453308	477502.820889	39.094029
2465.816466	478353.798061	39.099047
2468.210172	479184.325895	39.104064
2470.533908	480014.474274	39.109082
2472.922394	480853.210466	39.114100
2475.286965	481688.427545	39.119117
2477.878339	482533.163639	39.124135
2480.187172	483379.623827	39.129152
2483.097583	484212.412825	39.134170
2485.413530	485057.530706	39.139188
2487.660738	485907.012622	39.144205
2490.332917	486747.649866	39.149223
2493.060011	487592.579969	39.154240
2495.662144	488445.315065	39.159258
2498.194023	489294.537460	39.164276
2500.759609	490136.394113	39.169293
2503.014178	490996.230516	39.174311
2505.350214	491855.910175	39.179328
2507.524422	492717.088081	39.184346
2510.080414	493603.746980	39.189364
2512.508200	494470.296611	39.194381
2514.861067	495363.408266	39.199399
2516.918351	496245.976081	39.204416
2519.631848	497135.807145	39.209434
2521.825772	498042.327009	39.214452
2524.163000	498948.825123	39.219469
2526.769069	499854.675217	39.224487
2529.109683	500768.389705	39.229504
2531.742062	501695.222191	39.234522
2534.116116	502622.903153	39.239540
2536.638112	503556.408994	39.244557
2539.364960	504485.087485	39.249575
2541.759780	505422.341649	39.254592
2544.634978	506361.429742	39.259610
2547.063727	507311.278072	39.264628
2549.396335	508250.649265	39.269645
2552.141277	509207.292828	39.274663
2554.218703	510154.965095	39.279680
2557.178577	511106.015389	39.284698
2559.622656	512070.604278	39.289716
2562.623177	513030.657606	39.294733
2565.365945	513995.483813	39.299751
2567.817527	514960.349563	39.304768
2570.895349	515913.259741	39.309786
2573.594970	516864.763321	39.314804
2576.650514	517815.747172	39.319821
2579.550139	518765.993191	39.324839
2582.277198	519717.267556	39.329856
2584.546529	520662.512843	39.334874
2586.974627	521608.328869	39.339892
2589.827380	522567.870216	39.344909
2592.600797	523508.826847	39.349927
2595.505873	524460.180696	39.354944
2598.490383	525391.365145	39.359962
2600.828392	526343.852531	39.364980
2603.465359	527275.733380	39.369997
2605.831300	528224.370234	39.375015
2608.040323	529175.641545	39.380032
2610.945520	530110.373054	39.385050
2613.495562	531064.488349	39.390068
2616.116444	532012.740685	39.395085
2619.296341	532952.634080	39.400103
2621.787478	533898.017375	39.405120
2624.804879	534837.061535	39.410138
2627.552045	535782.733554	39.415156
2630.063175	536705.030242	39.420173
2632.299444	537640.599433	39.425191
2634.974736	538573.318128	39.430208
2637.757368	539490.258969	39.435226
2640.478513	540407.050573	39.440244
2642.996045	541306.861402	39.445261
2645.411477	542212.971129	39.450279
2647.457434	543107.211504	39.455296
2649.993948	544013.739307	39.460314
2652.754041	544930.231865	39.465332
2655.042270	545849.257156	39.470349
2657.332939	546764.248468	39.475367
2659.630325	547716.845784	39.480384
2662.347419	548649.395131	39.485402
2664.612114	549607.349161	39.490420
2666.776478	550564.197327	39.495437
2669.540636	551525.404864	39.500455
2671.926957	552498.823428	39.505472
2675.006713	553485.128167	39.510490
2677.438591	554472.674523	39.515508
2680.254190	555446.163236	39.520525
2683.035361	556443.761479	39.525543
2685.643087	557437.796571	39.530560
2688.669925	558433.598413	39.535578
2691.170672	559442.677855	39.540596
2693.472224	560451.261481	39.545613
2696.387218	561451.377914	39.550631
2698.826877	562472.846965	39.555648
2701.865748	563486.251767	39.560666
2704.245282	564518.572471	39.565684
2706.981396	565553.866791	39.570701
2709.936110	566601.396790	39.575719
2712.375297	567638.884233	39.580736
2715.241810	568678.176316	39.585754
2718.108273	569727.677103	39.590772
2720.424823	570778.086462	39.595789
2723.420044	571828.649190	39.600807
2726.087823	572888.515587	39.605824
2728.793639	573954.761926	39.610842
2731.316946	575024.461631	39.615860
2733.752397	576085.754960	39.620877
2736.778608	577167.534580	39.625895
2739.142623	578259.715826	39.630912
2741.993451	579326.636842	39.635930
2744.856352	580439.615788	39.640948
2747.320599	581538.465547	39.645965
2750.316025	582635.675491	39.650983
2752.964652	583739.063497	39.656000
2755.636413	584831.767478	39.661018
2758.599274	585939.619090	39.666036
2761.905760	587037.285747	39.671053
2764.815763	588140.633565	39.676071
2767.225367	589248.123790	39.681088
2770.674278	590341.256115	39.686106
2774.050727	591444.926064	39.691124
2776.829838	592529.949966	39.696141
2780.545895	593603.495999	39.701159
2783.452316	594681.688110	39.706176
2786.702326	595753.061936	39.711194
2789.201495	596825.564301	39.716212
2792.388597	597875.915184	39.721229
2795.494487	598929.791568	39.726247
2798.450443	599985.751102	39.731264
2801.575057	601031.070563	39.736282
2804.095655	602085.008068	39.741300
2806.804889	603136.715507	39.746317
2809.463787	604190.788431	39.751335
2811.702251	605240.628867	39.756352
2814.788322	606279.921912	39.761370
2816.957788	607338.440880	39.766388
2819.521893	608409.858387	39.771405
2822.330791	609463.619775	39.776423
2824.859356	610507.772053	39.781440
2827.613299	611539.082200	39.786458
2829.933077	612577.823307	39.791476
2832.058744	613617.800621	39.796493
2834.845223	614671.477215	39.801511
2837.600871	615726.459448	39.806528
2840.589305	616782.353115	39.811546
2843.299288	617848.092571	39.816564
2845.885993	618923.049077	39.821581
2848.840797	619999.589488	39.826599
2851.342418	621091.245429	39.831616
2853.736848	622195.255864	39.836634
2856.646235	623301.218457	39.841652
2858.602678	624411.922789	39.846669
2861.549952	625540.188489	39.851687
2864.596086	626673.615784	39.856704
2867.285400	627794.492625	39.861722
2870.163489	628949.988081	39.866740
2873.106773	630097.355958	39.871757
2876.382101	631248.740322	39.876775
2879.463885	632412.615360	39.881792
2882.069741	633573.943907	39.886810
2885.122969	634730.277652	39.891828
2888.100713	635890.290180	39.896845
2891.394260	637056.460976	39.901863
2894.274370	638233.898554	39.906880
2897.533044	639392.725904	39.911898
2900.427800	640562.610508	39.916916
2903.573530	641742.299327	39.921933
2906.819569	642899.736608	39.926951
2909.449711	644076.697663	39.931968
2912.529938	645250.506212	39.936986
2915.566350	646428.275757	39.942004
2918.313669	647626.798840	39.947021
2921.536184	648791.946465	39.952039
2924.611539	649975.378675	39.957056
2927.967313	651159.073740	39.962074
2930.583095	652323.662114	39.967092
2933.737610	653507.411032	39.972109
2937.010126	654685.069998	39.977127
2939.548000	655865.101460	39.982144
2942.403492	657058.240403	39.987162
2945.329017	658245.196172	39.992180
2948.535386	659435.547907	39.997197
2951.414546	660606.437315	40.002215
2955.182205	661787.545698	40.007232
2958.303626	662960.800586	40.012250
2961.365662	664138.901066	40.017268
2964.268396	665319.422454	40.022285
2967.699534	666478.063066	40.027303
2970.695448	667648.428888	40.032320
2973.109227	668822.429270	40.037338
2976.374867	670008.183990	40.042356
2979.160795	671182.578103	40.047373
2982.228235	672364.787831	40.052391
2984.686022	673559.034490	40.057408
2987.357502	674735.790381	40.062426
2990.444256	675919.042174	40.067444
2993.057911	677121.361186	40.072461
2995.935372	678321.394059	40.077479
2998.979276	679529.047239	40.082496
3001.901227	680717.978159	40.087514
3005.657895	681916.058774	40.092532
3008.690724	683128.857461	40.097549
3011.471758	684329.963586	40.102567
3014.044916	685531.442918	40.107584
3016.966872	686739.559520	40.112602
3019.866866	687936.148616	40.117620
3022.948261	689120.982157	40.122637
3025.533584	690277.496769	40.127655
3028.377060	691452.532309	40.132672
3031.722403	692627.083258	40.137690
3034.574421	693788.908073	40.142708
3037.500074	694973.689792	40.147725
3040.469477	696159.100282	40.152743
3043.372049	697352.150744	40.157760
3046.083056	698560.694018	40.162778
3048.898888	699743.318515	40.167796
3051.721677	700972.586948	40.172813
3054.523645	702185.178372	40.177831
3057.352529	703422.281307	40.182848
3060.478082	704646.571503	40.187866
3063.854303	705881.549348	40.192884
3066.607682	707133.645894	40.197901
3069.752544	708386.288874	40.202919
3072.683598	709649.978666	40.207936
3075.174643	710927.470866	40.212954
3078.120194	712202.815661	40.217972
3080.800786	713497.420634	40.222989
3084.064920	714802.028362	40.228007
3087.088515	716109.988701	40.233024
3089.927031	717420.300576	40.238042
3092.834404	718742.370656	40.243060
3095.898248	720076.475057	40.248077
3099.089599	721405.844417	40.253095
3102.172171	722758.213526	40.258112
3105.345950	724110.891221	40.263130
3108.337839	725453.440731	40.268148
3111.055795	726839.809357	40.273165
3114.588877	728189.831090	40.278183
3118.137151	729550.894091	40.283200
3121.408029	730915.283685	40.288218
3125.183717	732278.472248	40.293236
3128.434625	733646.308860	40.298253
3131.653163	734978.464466	40.303271
3135.109978	736352.771154	40.308288
3138.051513	737718.881395	40.313306
3141.497086	739070.905489	40.318324
3144.365713	740449.393444	40.323341
3147.998160	741806.252022	40.328359
3151.381509	743164.054040	40.333376
3154.676926	744526.865347	40.338394
3158.342049	745871.183652	40.343412
3161.105202	747240.516281	40.348429
3164.419452	748603.110225	40.353447
3167.543277	749961.751823	40.358464
3170.173868	751333.788928	40.363482
3173.333621	752704.609270	40.368500
3176.290498	754079.604137	40.373517
3179.650906	755446.751611	40.378535
3183.143098	756826.338743	40.383552
3186.364019	758196.219743	40.388570
3189.826549	759567.636385	40.393588
3192.747010	760937.566250	40.398605
3196.151095	762309.186496	40.403623
3199.403282	763670.693946	40.408640
3202.003085	765046.180377	40.413658
3205.436747	766430.523596	40.418676
3208.321661	767814.160414	40.423693
3210.792423	769211.128698	40.428711
3214.539741	770600.988783	40.433728
3217.576511	772000.190266	40.438746
3221.547320	773372.538649	40.443764
3224.867410	774748.128362	40.448781
3228.676314	776130.551022	40.453799
3232.059687	777485.233754	40.458816
3235.258752	778830.956081	40.463834
3238.281294	780138.856410	40.468852
3241.345935	781460.698427	40.473869
3244.803991	782780.860237	40.478887
3247.461214	784111.019324	40.483904
3250.511807	785437.777378	40.488922
3254.240809	786756.036957	40.493940
3257.253223	788077.407934	40.498957
3260.571633	789397.748305	40.503975
3263.722324	790742.232575	40.508992
3266.608991	792092.582329	40.514010
3269.721082	793440.579093	40.519028
3272.427999	794819.737550	40.524045
3275.378862	796197.066812	40.529063
3278.895536	797571.975375	40.534080
3281.519962	798961.301260	40.539098
3284.823731	800349.014320	40.544116
3288.004698	801762.457300	40.549133
3290.822697	803182.032283	40.554151
3294.183570	804597.312203	40.559168
3297.242665	806042.136529	40.564186
3300.977989	807477.694273	40.569204
3304.204913	808931.807555	40.574221
3306.821182	810381.165439	40.579239
3311.129734	811832.818542	40.584256
3314.095943	813296.400409	40.589274
3317.461913	814756.277525	40.594292
3320.634044	816233.499660	40.599309
3323.890089	817724.883733	40.604327
3327.483857	819188.836384	40.609344
3331.128257	820678.422647	40.614362
3334.682213	822144.366952	40.619380
3338.038073	823635.385960	40.624397
3341.337552	825118.225455	40.629415
3345.266321	826593.849599	40.634432
3348.090292	828089.847039	40.639450
3351.631145	829582.898629	40.644468
3355.069835	831076.209835	40.649485
3358.274170	832565.319313	40.654503
3361.971385	834070.856900	40.659520
3365.357219	835561.827887	40.664538
3369.073504	837052.447835	40.669556
3372.073338	838541.428143	40.674573
3375.344716	840050.405167	40.679591
3379.302395	841541.885678	40.684608
3382.696031	843054.606115	40.689626
3385.925835	844553.718166	40.694644
3388.843672	846071.873655	40.699661
3392.365547	847584.120492	40.704679
3395.976372	849101.041685	40.709696
3398.767407	850632.109059	40.714714
3402.427236	852155.372913	40.719732
3405.934900	853679.842456	40.724749
3408.835917	855210.444530	40.729767
3412.212258	856742.045185	40.734784
3415.524563	858290.838803	40.739802
3419.320561	859832.565563	40.744820
3423.022617	861375.374313	40.749837
3426.176345	862915.847192	40.754855
3429.661841	864460.334443	40.759872
3432.828628	866009.907883	40.764890
3436.587132	867562.765272	40.769908
3440.533455	869116.063336	40.774925
3443.789038	870671.688103	40.779943
3447.257749	872209.544561	40.784960
3450.732194	873768.780755	40.789978
3454.284601	875322.564063	40.794996
3457.910765	876842.013538	40.800000
3461.368978	878322.479236	40.805005
3464.660678	879747.929477	40.810010
3467.463755	881125.143162	40.815015
3470.547000	882432.710724	40.820020
3473.719590	883679.040203	40.825024
3476.338787	884853.912908	40.830029
3479.171414	885946.787293	40.835034
3481.672150	886991.877868	40.840039
3484.368647	887953.694849	40.845044
3486.640065	888868.675589	40.850048
3489.058260	889693.395197	40.855053
3491.191563	890461.344460	40.860058
3493.180329	891169.523718	40.865063
3495.614091	891820.179433	40.870068
3497.908005	892394.179250	40.875072
3499.816426	892926.500907	40.880077
3501.563282	893390.911433	40.885082
3502.767635	893819.304529	40.890087
3504.227660	894191.347816	40.895092
3505.820083	894516.741424	40.900096
3506.888403	894804.302969	40.905101
3508.556986	895033.260251	40.910106
3509.584425	895240.271808	40.915111
3510.569946	895391.115665	40.920116
3511.604592	895530.153555	40.925120
3512.641553	895629.166614	40.930125
3513.325735	895688.698759	40.935130
3514.078007	895728.885528	40.940135
3514.582181	895729.479199	40.945140
3515.161427	895717.107002	40.950144
3515.668085	895675.456178	40.955149
3516.403970	895622.746967	40.960154
3516.882246	895550.068865	40.965159
3517.449021	895439.189652	40.970164
3518.046195	895322.696149	40.975168
3518.173396	895187.715720	40.980173
3518.458476	895035.303795	40.985178
3518.942297	894876.280675	40.990183
3519.487479	894684.950147	40.995188
3519.606546	894494.456908	41.000192
3520.098282	894286.588047	41.005197
3520.117102	894071.537335	41.010202
3520.177618	893860.823143	41.015207
3520.685097	893626.818796	41.020212
3520.833066	893371.008191	41.025216
3520.611972	893127.432652	41.030221
3520.758509	892862.702079	41.035226
3521.213758	892599.552685	41.040231
3520.914469	892327.036420	41.045236
3521.136769	892051.229206	41.050240
3520.911391	891785.446139	41.055245
3521.409237	891494.282721	41.060250
3521.194522	891215.605179	41.065255
3521.209427	890912.882559	41.070260
3521.173245	890625.923347	41.075264
3521.403449	890325.746739	41.080269
3521.241122	890014.007440	41.085274
3521.181077	889715.588606	41.090279
3521.261480	889403.969876	41.095284
3521.212379	889097.775311	41.100288
3520.945679	888802.633801	41.105293
3521.172812	888479.713995	41.110298
3521.301804	888164.923128	41.115303
3520.695443	887850.526651	41.120308
3520.858133	887539.471424	41.125312
3520.691618	887223.322735	41.130317
3520.932445	886917.158589	41.135322
3520.711310	886603.211845	41.140327
3520.821389	886286.095105	41.145332
3520.616984	885975.500581	41.150336
3520.649672	885654.973014	41.155341
3520.593849	885331.246549	41.160346
3520.723490	885015.800438	41.165351
3520.423892	884679.197074	41.170356
3520.170649	884357.482886	41.175360
3520.315444	884046.146690	41.180365
3520.430395	883722.302664	41.185370
3520.220530	883414.769093	41.190375
3520.062964	883083.765818	41.195380
3520.142891	882761.133696	41.200384
3519.800574	882448.823715	41.205389
3519.963206	882138.836277	41.210394
3519.777607	881826.176564	41.215399
3519.557300	881507.400802	41.220404
3519.453740	881183.936729	41.225408
3519.628456	880881.730616	41.230413
3519.295075	880561.759080	41.235418
3519.119940	880260.644758	41.240423
3518.821100	879959.438446	41.245428
3518.844300	879638.291637	41.250432
3518.492626	879346.368556	41.255437
3518.518438	879033.331399	41.260442
3518.436017	878733.286984	41.265447
3518.240486	878437.318104	41.270452
3517.967812	878137.565575	41.275456
3517.922017	877851.820570	41.280461
3517.740963	877552.508069	41.285466
3517.941517	877263.009099	41.290471
3517.641597	876971.929717	41.295476
3517.812081	876672.223802	41.300480
3517.404368	876383.363884	41.305485
3517.162984	876098.827251	41.310490
3516.991740	875829.009324	41.315495
3516.764725	875535.422323	41.320500
3516.833989	875253.413057	41.325504
3516.882823	874973.334028	41.330509
3516.971927	874690.615674	41.335514
3516.479095	874419.525400	41.340519
3516.403500	874148.936198	41.345524
3516.431168	873869.293767	41.350528
3516.181042	873608.120756	41.355533
3515.960684	873333.151703	41.360538
3516.139039	873061.306759	41.365543
3515.928052	872800.188929	41.370548
3516.000486	872535.227914	41.375552
3515.507246	872270.639482	41.380557
3515.536867	872011.194531	41.385562
3515.728259	871762.971298	41.390567
3515.588689	871488.874608	41.395572
3515.859389	871222.560815	41.400576
3515.393363	870967.617645	41.405581
3515.698247	870706.905838	41.410586
3515.498684	870443.158991	41.415591
3515.129638	870180.205182	41.420596
3515.139387	869929.023097	41.425600
3514.783215	869671.676399	41.430605
3514.957696	869421.028518	41.435610
3515.071981	869171.254063	41.440615
3514.673507	868925.826597	41.445620
3514.780625	868682.345258	41.450624
3514.807510	868444.985804	41.455629
3514.615689	868187.451353	41.460634
3514.447285	867941.071701	41.465639
3514.211361	867694.595959	41.470644
3514.038048	867458.590442	41.475648
3514.086565	867223.024845	41.480653
3513.999170	866972.609561	41.485658
3513.545720	866749.833902	41.490663
3513.585306	866519.973988	41.495668
3513.629533	866286.995635	41.500672
3513.329051	866062.032019	41.505677
3513.306805	865821.176882	41.510682
3513.024064	865603.577567	41.515687
3513.042975	865388.738631	41.520692
3513.039587	865158.445378	41.525696
3512.774669	864941.888241	41.530701
3512.876609	864715.059114	41.535706
3512.546610	864508.409495	41.540711
3512.543006	864292.466397	41.545716
3512.721287	864074.541866	41.550720
3512.463533	863865.720287	41.555725
3512.246633	863645.221231	41.560730
3512.194275	863439.558654	41.565735
3511.986694	863246.356666	41.570740
3511.854967	863042.248968	41.575744
3511.764770	862848.917814	41.580749
3512.041621	862645.021126	41.585754
3511.707994	862443.551342	41.590759
3511.271026	862240.828068	41.595764
3511.732744	862041.838909	41.600768
3511.103084	861852.259414	41.605773
3511.381689	861645.703930	41.610778
3511.128699	861465.870441	41.615783
3511.270623	861274.006797	41.620788
3511.151215	861086.458613	41.625792
3510.920595	860894.255452	41.630797
3510.859565	860710.867457	41.635802
3510.814971	860540.404984	41.640807
3510.644772	860345.354477	41.645812
3510.800379	860162.108842	41.650816
3510.474706	859991.969141	41.655821
3510.910098	859803.512190	41.660826
3510.337375	859622.899082	41.665831
3510.273781	859448.616170	41.670836
3510.710464	859262.768490	41.675840
3510.022383	859099.764131	41.680845
3510.218115	858905.288373	41.685850
3510.426373	858743.683264	41.690855
3510.346970	858567.918815	41.695860
3510.225786	858390.891574	41.700864
3510.160338	858221.048981	41.705869
3510.172700	858044.184319	41.710874
3509.788496	857878.276177	41.715879
3509.896792	857717.146977	41.720884
3510.027724	857547.156130	41.725888
3509.661246	857387.653196	41.730893
3509.948755	857224.341063	41.735898
3509.780938	857042.320451	41.740903
3509.406157	856875.508001	41.745908
3509.813780	856712.162509	41.750912
3509.158622	856561.248694	41.755917
3509.290572	856399.497269	41.760922
3509.292706	856242.044807	41.765927
3508.982851	856091.646503	41.770932
3509.169936	855924.618460	41.775936
3508.849659	855771.099848	41.780941
3508.898817	855614.791499	41.785946
3508.676043	855459.302596	41.790951
3508.420859	855310.530805	41.795956
3508.614134	855168.689400	41.800960
3508.438436	855024.374853	41.805965
3508.694742	854883.879201	41.810970
3508.820695	854741.649754	41.815975
3508.448785	854582.561871	41.820980
3508.458336	854445.503820	41.825984
3508.164505	854321.050135	41.830989
3508.216357	854171.421623	41.835994
3507.902666	854014.451178	41.840999
3508.051327	853888.358329	41.846004
3507.801331	853758.142397	41.851008
3507.608966	853637.455038	41.856013
3507.823792	853496.545341	41.861018
3507.512121	853374.996311	41.866023
3507.528532	853243.849467	41.871028
3507.741221	853119.872403	41.876032
3507.606919	852993.710620	41.881037
3507.798316	852853.082277	41.886042
3507.724980	852735.960374	41.891047
3507.403673	852613.034843	41.896052
3507.648672	852487.384530	41.901056
3507.371341	852356.851585	41.906061
3507.318187	852235.237666	41.911066
3507.240206	852109.827679	41.916071
3507.118143	851983.059092	41.921076
3507.176622	851870.670846	41.926080
3507.071195	851756.846800	41.931085
3507.197879	851634.704603	41.936090
3507.067641	851514.452707	41.941095
3507.118827	851401.375476	41.946100
3506.965948	851280.538454	41.951104
3506.812501	851178.496165	41.956109
3506.834288	851057.139075	41.961114
3506.929765	850940.539953	41.966119
3506.967622	850822.876753	41.971124
3506.787167	850720.344419	41.976128
3506.696406	850603.867083	41.981133
3506.393711	850490.247205	41.986138
3506.399613	850373.067809	41.991143
3506.528024	850269.503133	41.996148
3506.448418	850160.905716	42.001152
3506.516732	850063.289494	42.006157
3506.424964	849953.229306	42.011162
3506.176228	849851.765493	42.016167
3505.971334	849740.940885	42.021172
3506.332711	849633.625495	42.026176
3505.792025	849544.089716	42.031181
3506.098856	849442.138070	42.036186
3506.232002	849350.637541	42.041191
3505.721634	849248.427655	42.046196
3506.397065	849149.820364	42.051200
3506.151143	849050.291588	42.056205
3505.799049	848943.374164	42.061210
3505.804529	848854.225690	42.066215
3505.695507	848757.592604	42.071220
3506.029146	848657.085235	42.076224
3505.732849	848567.690093	42.081229
3505.539301	848476.522908	42.086234
3505.687039	848381.498137	42.091239
3505.692697	848292.731396	42.096244
3505.863860	848191.561261	42.101248
3505.427127	848110.172805	42.106253
3505.657233	848004.799971	42.111258
3505.607855	847913.990634	42.116263
3505.542634	847830.880805	42.121268
3505.746760	847731.939084	42.126272
3505.664374	847652.337818	42.131277
3505.700634	847550.789784	42.136282
3505.840531	847466.666850	42.141287
3505.602684	847377.732375	42.146292
3505.731272	847280.745046	42.151296
3505.495277	847191.612723	42.156301
3505.414010	847101.186709	42.161306
3505.292017	847008.232183	42.166311
3505.176791	846927.847480	42.171316
3505.127332	846843.357556	42.176320
3505.049717	846757.506662	42.181325
3505.338024	846673.835989	42.186330
3504.912542	846600.515581	42.191335
3504.836147	846510.859995	42.196340
3505.381238	846432.017118	42.201344
3504.792173	846354.822094	42.206349
3504.865170	846272.935993	42.211354
3504.944312	846195.434012	42.216359
3504.639337	846119.846318	42.221364
3505.026468	846039.367522	42.226368
3504.956830	845964.908888	42.231373
3504.908817	845869.098589	42.236378
3504.859912	845805.941875	42.241383
3505.012582	845729.201867	42.246388
3504.651137	845654.397715	42.251392
3504.345061	845593.523257	42.256397
3504.807852	845505.031791	42.261402
3504.646129	845433.798946	42.266407
3504.634371	845368.487110	42.271412
3504.755112	845285.995423	42.276416
3504.562760	845212.912912	42.281421
3504.341630	845138.761933	42.286426
3504.597810	845072.135562	42.291431
3504.393172	844990.278536	42.296436
3504.645574	844927.745829	42.301440
3504.393424	844859.836079	42.306445
3504.002428	844790.681062	42.311450
3504.386101	844728.807213	42.316455
3504.430122	844657.239234	42.321460
3504.162380	844593.716454	42.326464
3504.140108	844530.640085	42.331469
3504.043932	844459.872937	42.336474
3504.237356	844393.444746	42.341479
3503.768788	844330.634889	42.346484
3504.122498	844266.226457	42.351488
3503.925409	844208.148205	42.356493
3503.856663	844150.925804	42.361498
3504.035873	844099.512249	42.366503
3503.903782	844030.013749	42.371508
3503.889330	843968.783073	42.376512
3503.707499	843918.890099	42.381517
3503.996744	843861.508608	42.386522
3503.917968	843787.854616	42.391527
3503.740958	843737.179350	42.396532
3504.006525	843663.174663	42.401536
3503.657034	843608.090061	42.406541
3503.755385	843556.587906	42.411546
3503.474660	843501.978613	42.416551
3503.261544	843444.383552	42.421556
3503.662178	843385.175402	42.426560
3503.435191	843348.596069	42.431565
3504.179031	843291.085780	42.436570
3504.152610	843241.795725	42.441575
3503.840935	843175.389195	42.446580
3503.958271	843113.055846	42.451584
3503.443072	843054.385531	42.456589
3503.971402	842984.620499	42.461594
3503.868000	842937.193645	42.466599
3503.681081	842879.686657	42.471604
3504.155458	842816.999023	42.476608
3503.645051	842769.004050	42.481613
3503.695874	842707.018999	42.486618
3504.085473	842648.878572	42.491623
3503.631554	842596.484329	42.496628
3504.082666	842538.722868	42.501632
3503.950123	842484.909384	42.506637
3504.071084	842419.691544	42.511642
3504.006505	842368.547933	42.516647
3503.709855	842316.222999	42.521652
3503.772099	842248.672333	42.526656
3503.780271	842194.248016	42.531661
3503.900394	842128.344594	42.536666
3503.707090	842066.491036	42.541671
3503.617210	842014.227089	42.546676
3503.864852	841952.055948	42.551680
3503.659359	841908.344603	42.556685
3503.667680	841845.870464	42.561690
3503.676520	841795.978143	42.566695
3503.267139	841749.470662	42.571700
3503.643169	841689.714297	42.576704
3503.325475	841643.190935	42.581709
3503.464475	841582.594736	42.586714
3503.775749	841536.503476	42.591719
3503.339702	841489.315682	42.596724
3503.254308	841434.168692	42.601728
3503.233828	841391.203670	42.606733
3503.266475	841347.302923	42.611738
3503.380129	841295.438498	42.616743
3503.187592	841243.185121	42.621748
3503.626524	841183.657515	42.626752
3503.276245	841141.184094	42.631757
3503.304056	841094.502258	42.636762
3503.455467	841045.751165	42.641767
3503.062171	841000.308603	42.646772
3503.093910	840947.674429	42.651776
3502.874810	840921.322736	42.656781
3502.799494	840878.948602	42.661786
3503.333322	840832.474156	42.666791
3503.253677	840776.442538	42.671796
3503.214075	840732.451898	42.676800
3502.865752	840698.755154	42.681805
3503.321995	840647.560692	42.686810
3503.218736	840600.896827	42.691815
3503.182302	840552.758246	42.696820
3503.087533	840504.970365	42.701824
3503.203309	840458.366937	42.706829
3502.976862	840426.843762	42.711834
3503.020346	840374.349258	42.716839
3502.894324	840331.199347	42.721844
3503.077616	840283.705472	42.726848
3502.402216	840241.816189	42.731853
3502.511516	840195.894848	42.736858
3502.612208	840168.560513	42.741863
3502.305067	840138.659003	42.746868
3503.025310	840097.319403	42.751872
3502.405409	840068.834989	42.756877
3502.483133	840039.455014	42.761882
3502.510729	839989.838150	42.766887
3502.369357	839955.274066	42.771892
3502.612393	839931.378898	42.776896
3502.377806	839901.757028	42.781901
3502.479500	839868.664741	42.786906
3502.873069	839829.279798	42.791911
3502.412032	839797.792150	42.796916
3502.754921	839754.658673	42.801921
3502.472959	839735.191111	42.806925
3502.489948	839686.646911	42.811930
3502.691098	839653.829842	42.816935
3502.399245	839633.046381	42.821940
3502.938059	839587.488992	42.826945
3502.439801	839556.640505	42.831949
3502.794389	839514.040129	42.836954
3502.566391	839478.999866	42.841959
3502.463301	839445.451245	42.846964
3502.425204	839402.768446	42.851969
3502.671761	839367.015162	42.856973
3502.582698	839336.342149	42.861978
3502.658561	839306.520015	42.866983
3502.240362	839278.925822	42.871988
3502.637531	839241.585793	42.876993
3502.504895	839223.458162	42.881997
3502.642877	839176.792934	42.887002
3502.576533	839133.869044	42.892007
3502.466402	839104.466922	42.897012
3502.500799	839065.087646	42.902017
3502.389867	839026.463923	42.907021
3502.169281	839001.714626	42.912026
3502.553818	838965.253299	42.917031
3502.369091	838942.254343	42.922036
3502.636583	838907.714826	42.927041
3502.487141	838877.879012	42.932045
3502.565451	838842.394469	42.937050
3502.441526	838813.676368	42.942055
3502.307704	838779.738977	42.947060
3502.481098	838743.652714	42.952065
3502.216190	838713.347224	42.957069
3502.021397	838693.862125	42.962074
3502.106894	838664.767309	42.967079
3501.988510	838648.197085	42.972084
3501.924122	838608.831271	42.977089
3502.199512	838594.928501	42.982093
3502.010568	838564.951351	42.987098
3502.300311	838549.191941	42.992103
3501.925964	838519.391499	42.997108
3502.169043	838501.297523	43.002113
3502.042423	838461.013953	43.007117
3501.849742	838457.239724	43.012122
3502.242823	838419.895579	43.017127
3501.885574	838402.339363	43.022132
3501.902305	838370.814770	43.027137
3502.422270	838354.138640	43.032141
3502.084848	838319.256426	43.037146
3502.238603	838296.296984	43.042151
3501.960782	838265.015572	43.047156
3502.269792	838245.494919	43.052161
3502.189214	838215.986251	43.057165
3501.900107	838193.001791	43.062170
3502.105280	838163.543408	43.067175
3502.094938	838146.954089	43.072180
3502.218395	838113.165973	43.077185
3502.297717	838083.971942	43.082189
3502.110262	838062.824586	43.087194
3502.619134	838025.459073	43.092199
3502.180401	838007.134419	43.097204
3502.151106	837959.267911	43.102209
3502.058381	837952.402597	43.107213
3502.475821	837926.080080	43.112218
3502.384320	837894.863767	43.117223
3502.276778	837867.407501	43.122228
3502.100972	837826.981645	43.127233
3502.074345	837815.176522	43.132237
3501.897228	837790.756975	43.137242
3502.091597	837753.539282	43.142247
3501.998216	837739.841804	43.147252
3502.144311	837702.729369	43.152257
3502.045034	837688.837550	43.157261
3501.899260	837669.097250	43.162266
3502.008272	837646.435658	43.167271
3501.856165	837622.596964	43.172276
3501.804836	837598.985589	43.177281
3501.844316	837580.922555	43.182285
3501.713196	837551.370348	43.187290
3501.941316	837531.812049	43.192295
3501.783115	837513.293365	43.197300
3502.005636	837498.957713	43.202305
3501.666541	837471.830705	43.207309
3501.896653	837438.167873	43.212314
3501.855357	837439.785201	43.217319
3501.899159	837418.109598	43.222324
3502.128609	837395.232070	43.227329
3502.125888	837371.660654	43.232333
3502.185324	837348.469341	43.237338
3502.391620	837313.394481	43.242343
3501.876730	837292.103297	43.247348
3502.422699	837256.240119	43.252353
3502.188090	837226.654658	43.257357
3502.266103	837198.140071	43.262362
3502.323672	837171.580914	43.267367
3501.890607	837156.083559	43.272372
3502.125040	837133.155473	43.277377
3501.897991	837106.789343	43.282381
3501.718564	837091.738106	43.287386
3501.732209	837065.869021	43.292391
3501.672934	837053.970263	43.297396
3502.022649	837030.485961	43.302401
3502.019471	837002.715966	43.307405
3501.541541	836977.269135	43.312410
3502.083499	836959.219199	43.317415
3501.965873	836951.283174	43.322420
3502.124215	836921.045902	43.327425
3501.846429	836903.082025	43.332429
3501.830396	836870.335284	43.337434
3501.988051	836856.789798	43.342439
3501.718130	836845.169385	43.347444
3501.884274	836807.023519	43.352449
3501.837394	836801.125570	43.357453
3501.573117	836769.541777	43.362458
3501.890842	836755.725673	43.367463
3501.884572	836747.966286	43.372468
3501.870655	836712.338722	43.377473
3502.005747	836708.851124	43.382477
3501.683909	836676.446614	43.387482
3501.794178	836650.901602	43.392487
3501.952636	836634.182951	43.397492
3501.990043	836601.328418	43.402497
3501.869610	836594.710258	43.407501
3501.834241	836578.218624	43.412506
3501.916461	836556.045691	43.417511
3501.868569	836533.747684	43.422516
3502.029060	836515.905771	43.427521
3502.227524	836488.783677	43.432525
3502.311797	836456.652835	43.437530
3502.194746	836427.630047	43.442535
3502.087528	836404.902072	43.447540
3502.052613	836365.224766	43.452545
3502.082684	836350.332525	43.457549
3501.825005	836326.359970	43.462554
3502.284960	836297.241553	43.467559
3502.269031	836276.401729	43.472564
3502.425745	836250.261739	43.477569
3502.281214	836215.922042	43.482573
3502.302043	836193.513911	43.487578
3502.211159	836169.513297	43.492583
3502.270827	836148.904670	43.497588
3502.192198	836115.139330	43.502593
3502.262657	836092.527422	43.507597
3502.116646	836085.864137	43.512602
3502.733130	836046.516888	43.517607
3502.186060	836018.881043	43.522612
3502.251429	835987.678428	43.527617
3501.672548	835957.704500	43.532621
3501.849694	835937.124658	43.537626
3502.216840	835919.832824	43.542631
3502.209835	835883.516130	43.547636
3502.246071	835858.956459	43.552641
3502.087640	835842.092689	43.557645
3501.920988	835817.468648	43.562650
3502.409146	835786.048973	43.567655
3501.967468	835755.563349	43.572660
3502.455973	835725.900680	43.577665
3502.239468	835702.797698	43.582669
3502.131014	835679.335123	43.587674
3502.095441	835645.218512	43.592679
3501.879097	835630.023479	43.597684
3502.144409	835609.867419	43.602689
3501.905868	835580.372652	43.607693
3502.056451	835554.719017	43.612698
3502.052567	835527.040400	43.617703
3501.885305	835504.319131	43.622708
3501.900174	835481.811870	43.627713
3502.024897	835473.492376	43.632717
3501.930978	835438.115021	43.637722
3501.970613	835420.143526	43.642727
3501.763643	835387.811231	43.647732
3501.988026	835371.957175	43.652737
3502.299421	835346.862045	43.657741
3502.000990	835329.531805	43.662746
3502.118748	835300.465255	43.667751
3501.849334	835287.426185	43.672756
3502.028022	835259.618709	43.677761
3501.932934	835245.574456	43.682765
3501.616962	835217.652999	43.687770
3502.007047	835188.101710	43.692775
3501.812387	835181.787238	43.697780
3501.927866	835163.997816	43.702785
3501.733035	835149.139842	43.707789
3501.607867	835131.438789	43.712794
3501.713072	835097.589010	43.717799
3501.706278	835091.926992	43.722804
3501.895417	835075.345705	43.727809
3502.046077	835041.097579	43.732813
3501.689674	835030.415717	43.737818
3502.124805	835000.758511	43.742823
3501.736740	834995.989168	43.747828
3501.858549	834961.110693	43.752833
3501.704568	834938.482883	43.757837
3501.870691	834931.669343	43.762842
3501.936324	834903.000162	43.767847
3501.862483	834891.978597	43.772852
3501.790531	834867.335322	43.777857
3501.896785	834837.438603	43.782861
3502.045979	834819.105632	43.787866
3502.102070	834792.829838	43.792871
3501.828551	834793.509623	43.797876
3501.859039	834745.706982	43.802881
3501.900851	834739.109008	43.807885
3501.900813	834712.451547	43.812890
3501.802957	834694.451853	43.817895
3501.665623	834680.510974	43.822900
3502.027889	834657.894793	43.827905
3501.870441	834632.044107	43.832909
3501.276596	834618.227109	43.837914
3501.884482	834596.790860	43.842919
3501.592795	834593.372420	43.847924
3501.866268	834557.587947	43.852929
3501.659285	834548.101284	43.857933
3501.588958	834541.863352	43.862938
3501.611145	834518.375030	43.867943
3501.393292	834517.532104	43.872948
3501.635714	834495.862768	43.877953
3501.588239	834476.194117	43.882957
3501.820081	834451.645691	43.887962
3501.792412	834436.856190	43.892967
3501.600523	834415.258121	43.897972
3501.584198	834392.410417	43.902977
3501.807387	834396.621535	43.907981
3501.183693	834372.604333	43.912986
3501.712295	834344.784108	43.917991
3501.590811	834338.456753	43.922996
3501.381179	834317.984283	43.928001
3501.575973	834295.443246	43.933005
3501.459230	834294.974248	43.938010
3501.409460	834291.174013	43.943015
3501.222560	834284.515593	43.948020
3501.258021	834246.131962	43.953025
3501.406769	834243.470846	43.958029
3501.147619	834244.880722	43.963034
3501.579562	834233.091145	43.968039
3501.534626	834221.966019	43.973044
3501.140361	834202.793099	43.978049
3501.377098	834197.236664	43.983053
3501.022912	834193.632994	43.988058
3501.389252	834176.580770	43.993063
3500.958998	834173.136101	43.998068
3501.338283	834146.902098	44.003073
3501.078830	834147.140182	44.008077
3501.221331	834138.620732	44.013082
3501.386875	834134.638456	44.018087
3501.048966	834126.588742	44.023092
3501.171120	834119.879247	44.028097
3501.591236	834096.665642	44.033101
3501.749940	834096.200087	44.038106
3501.707742	834089.078179	44.043111
3501.556697	834072.110899	44.048116
3501.012349	834042.317662	44.053121
3501.405985	834031.510597	44.058125
3501.096610	834039.569466	44.063130
3501.298826	834033.823264	44.068135
3501.105976	834007.487620	44.073140
3500.942310	833980.951747	44.078145
3501.117006	833982.339048	44.083149
3500.879158	833978.862582	44.088154
3501.443438	833976.865347	44.093159
3501.170454	833982.281529	44.098164
3501.084878	833975.020153	44.103169
3501.619125	833971.904798	44.108173
3501.012899	833959.895093	44.113178
3501.355291	833938.695715	44.118183
3500.978324	833933.093652	44.123188
3501.087162	833922.430975	44.128193
3501.048412	833930.298915	44.133197
3501.091039	833920.184261	44.138202
3501.055549	833906.810885	44.143207
3501.323134	833897.879880	44.148212
3501.276281	833885.094285	44.153217
3501.443590	833880.720927	44.158221
3501.187585	833884.864822	44.163226
3501.122265	833870.715011	44.168231
3501.005504	833842.559461	44.173236
3501.045063	833831.224425	44.178241
3501.137008	833822.029265	44.183245
3500.852073	833821.099634	44.188250
3501.344303	833833.714411	44.193255
3501.110520	833828.967612	44.198260
3501.170818	833830.227300	44.203265
3501.206091	833826.363953	44.208269
3501.079888	833793.277905	44.213274
3501.207424	833778.412501	44.218279
3501.125505	833779.304980	44.223284
3500.960117	833772.007691	44.228289
3501.130328	833775.300165	44.233293
3500.925261	833775.626962	44.238298
3501.375839	833770.816228	44.243303
3501.163779	833752.393243	44.248308
3500.994832	833737.771903	44.253313
3501.177552	833735.153815	44.258317
3501.083104	833732.532548	44.263322
3501.193673	833730.658804	44.268327
3501.267354	833729.572427	44.273332
3501.253308	833723.812741	44.278337
3501.266013	833706.866361	44.283341
3501.152568	833700.097576	44.288346
3501.309153	833690.452103	44.293351
3501.015570	833693.821011	44.298356
3501.225115	833688.708101	44.303361
3501.268233	833674.588830	44.308365
3500.995929	833661.693434	44.313370
3501.134614	833647.216543	44.318375
3501.014615	833639.618640	44.323380
3501.059407	833632.091247	44.328385
3501.063408	833627.353965	44.333389
3501.059823	833632.481907	44.338394
3501.168355	833627.825070	44.343399
3501.258822	833645.975525	44.348404
3501.059038	833614.170297	44.353409
3501.165474	833601.603051	44.358413
3500.878831	833603.261751	44.363418
3500.899686	833590.269094	44.368423
3500.979744	833584.737943	44.373428
3500.628355	833578.203550	44.378433
3501.007309	833585.075301	44.383437
3500.618842	833571.466380	44.388442
3501.175503	833581.336448	44.393447
3501.070652	833581.109596	44.398452
3501.134279	833576.020632	44.403457
3500.937351	833589.774873	44.408461
3500.847346	833575.530817	44.413466
3501.511407	833558.965082	44.418471
3501.011249	833553.187649	44.423476
3501.003445	833537.318509	44.428481
3501.022265	833543.712469	44.433485
3500.752080	833539.996929	44.438490
3501.136572	833532.608796	44.443495
3501.190814	833536.848307	44.448500
3501.454471	833527.673279	44.453505
3501.113134	833512.103176	44.458509
3501.028696	833501.813468	44.463514
3501.535574	833495.821278	44.468519
3500.963790	833498.796617	44.473524
3501.141936	833485.826675	44.478529
3501.504188	833479.858292	44.483533
3501.190647	833465.211319	44.488538
3501.543506	833440.541459	44.493543
3501.623391	833433.642884	44.498548
3501.346695	833429.684187	44.503553
3501.008651	833402.930497	44.508557
3501.084522	833396.569709	44.513562
3501.559188	833386.236559	44.518567
3501.471335	833382.100227	44.523572
3501.378203	833382.701606	44.528577
3501.599650	833357.271740	44.533581
3501.379577	833351.643326	44.538586
3501.283127	833338.034646	44.543591
3501.307309	833348.041613	44.548596
3501.316492	833327.627627	44.553601
3501.618157	833298.033438	44.558605
3501.499929	833296.880932	44.563610
3501.636701	833283.673230	44.568615
3501.206712	833274.612097	44.573620
3501.405341	833266.472929	44.578625
3501.431770	833242.100253	44.583629
3501.418882	833252.845991	44.588634
3501.211108	833224.995749	44.593639
3501.339474	833211.154434	44.598644
3501.226626	833209.024331	44.603649
3501.630708	833206.516074	44.608653
3501.148064	833195.070599	44.613658
3501.683212	833158.307424	44.618663
3501.283088	833163.989403	44.623668
3501.457604	833146.087035	44.628673
3501.453578	833141.448390	44.633677
3501.202360	833132.797128	44.638682
3501.220511	833116.727340	44.643687
3501.248632	833116.527404	44.648692
3501.391512	833110.692489	44.653697
3501.343567	833101.519349	44.658701
3500.875642	833088.313179	44.663706
3501.547606	833064.663713	44.668711
3501.270252	833058.116596	44.673716
3501.399533	833055.604709	44.678721
3501.648363	833047.701179	44.683725
3501.693544	833029.477940	44.688730
3501.558651	833009.233190	44.693735
3501.747552	833011.595088	44.698740
3501.676337	832975.077261	44.703745
3501.754143	832965.785542	44.708749
3501.577559	832964.691424	44.713754
3501.661892	832951.052153	44.718759
3501.862024	832938.028657	44.723764
3501.843709	832923.087642	44.728769
3501.636124	832901.145235	44.733773
3501.274318	832893.439771	44.738778
3501.350730	832867.348153	44.743783
3501.068425	832858.848155	44.748788
3501.510536	832845.345080	44.753793
3501.733514	832833.245523	44.758797
3501.412460	832826.070479	44.763802
3501.419933	832794.227080	44.768807
3501.524538	832790.302858	44.773812
3501.760436	832796.124585	44.778817
3501.746270	832777.177844	44.783821
3501.532334	832762.903574	44.788826
3501.766888	832747.285607	44.793831
3501.635461	832728.309200	44.798836
3501.544997	832716.065699	44.803841
3501.837021	832697.165968	44.808845
3500.972222	832667.419164	44.813850
3501.181440	832647.800346	44.818855
3501.471929	832643.943096	44.823860
3501.566974	832646.027555	44.828865
3501.982895	832645.470695	44.833869
3501.676542	832617.975950	44.838874
3501.784867	832609.069407	44.843879
3501.828742	832586.303086	44.848884
3501.753147	832560.332949	44.853889
3501.292790	832560.115776	44.858893
3501.478868	832535.128068	44.863898
3501.841570	832516.411529	44.868903
3501.614828	832512.737077	44.873908
3501.434535	832492.156307	44.878913
3501.780651	832468.900229	44.883917
3501.412534	832467.495691	44.888922
3501.582141	832457.357838	44.893927
3501.098245	832439.659651	44.898932
3501.456483	832423.141402	44.903937
3501.730068	832410.007068	44.908941
3501.543744	832406.716623	44.913946
3501.722068	832373.915043	44.918951
3501.464445	832373.664469	44.923956
3501.518981	832370.285492	44.928961
3501.525094	832331.699976	44.933965
3501.487706	832323.158931	44.938970
3501.670612	832312.432564	44.943975
3501.527297	832294.189466	44.948980
3501.650302	832288.796662	44.953985
3501.531409	832277.240797	44.958989
3501.337984	832263.841198	44.963994
3501.583246	832236.888920	44.968999
3501.765628	832229.239551	44.974004
3501.359321	832227.010934	44.979009
3501.373831	832204.394634	44.984013
3501.340253	832208.991378	44.989018
3501.426643	832195.496706	44.994023
3501.461169	832185.917945	44.999028
3501.344409	832163.958079	45.004033
3501.735566	832136.688298	45.009037
3501.547925	832141.261623	45.014042
3501.450302	832136.930732	45.019047
3501.673285	832117.649945	45.024052
3501.262428	832104.383516	45.029057
3501.251947	832088.657797	45.034061
3501.121088	832089.363194	45.039066
3501.342860	832076.480936	45.044071
3500.930930	832053.104015	45.049076
3501.174352	832040.022745	45.054081
3501.410399	832032.901586	45.059085
3501.323976	832039.314366	45.064090
3501.453798	832027.179810	45.069095
3501.672746	832020.207984	45.074100
3501.238428	832004.014590	45.079105
3501.576278	831991.650328	45.084109
3501.511094	831982.185378	45.089114
3501.215365	831953.269584	45.094119
3501.307441	831944.853249	45.099124
3501.160948	831934.033982	45.104129
3501.383723	831936.586075	45.109133
3501.032622	831936.790476	45.114138
3501.128885	831904.097728	45.119143
3501.222627	831905.547662	45.124148
3501.130912	831902.045997	45.129153
3501.281034	831895.671509	45.134157
3501.085482	831897.559853	45.139162
3501.265541	831891.473498	45.144167
3501.256368	831870.178740	45.149172
3501.484867	831857.539166	45.154177
3501.659696	831839.486609	45.159181
3501.303395	831836.810011	45.164186
3501.676785	831819.506214	45.169191
3501.476966	831803.078311	45.174196
3501.564849	831798.081648	45.179201
3501.547428	831783.089012	45.184205
3501.397291	831763.770943	45.189210
3501.592715	831743.858595	45.194215
3501.539218	831747.335493	45.199220
3501.345840	831723.432925	45.204225
3501.780242	831704.653395	45.209229
3501.405282	831701.882122	45.214234
3501.484283	831692.734923	45.219239
3501.664316	831668.428723	45.224244
3501.732112	831654.740605	45.229249
3501.625099	831642.790881	45.234253
3501.650395	831635.459769	45.239258
3501.717534	831609.071539	45.244263
3501.644599	831607.764727	45.249268
3501.476217	831581.854801	45.254273
3501.487103	831560.164947	45.259277
3501.426081	831559.393481	45.264282
3501.625061	831531.810890	45.269287
3501.186347	831520.648286	45.274292
3501.518416	831517.369695	45.279297
3501.422667	831515.089672	45.284301
3501.250260	831502.124663	45.289306
3501.466362	831475.662507	45.294311
3501.408839	831464.046236	45.299316
3501.321177	831467.773150	45.304321
3501.492305	831462.176344	45.309325
3501.418394	831438.546136	45.314330
3501.327578	831427.814549	45.319335
3501.406347	831424.235697	45.324340
3501.042758	831429.668919	45.329345
3501.606391	831417.559467	45.334349
3501.487733	831388.367747	45.339354
3501.408150	831376.266468	45.344359
3501.396199	831377.440839	45.349364
3501.251768	831361.540028	45.354369
3501.544237	831331.205662	45.359373
3501.323474	831335.101122	45.364378
3501.313982	831330.266686	45.369383
3501.399529	831325.221197	45.374388
3501.287343	831301.547945	45.379393
3501.475925	831282.221500	45.384397
3501.502503	831291.205414	45.389402
3501.357442	831280.824463	45.394407
3501.276919	831263.300859	45.399412
3501.247403	831246.745797	45.404417
3501.456195	831229.076748	45.409421
3501.594392	831233.597037	45.414426
3501.498410	831208.846088	45.419431
3501.978686	831204.028586	45.424436
3501.476347	831182.324306	45.429441
3501.589140	831163.058841	45.434445
3501.296369	831142.052659	45.439450
3501.647461	831137.989142	45.444455
3501.537616	831135.222804	45.449460
3501.716498	831110.377355	45.454465
3501.610724	831098.182171	45.459469
3501.506870	831092.532640	45.464474
3501.449577	831057.418391	45.469479
3501.485965	831047.300285	45.474484
3501.409486	831040.278371	45.479489
3501.390479	831031.928003	45.484493
3501.314689	830998.428569	45.489498
3501.300471	830989.344588	45.494503
3501.220519	830986.280153	45.499508
3501.102243	830991.722182	45.504513
3501.709160	830983.806020	45.509517
3501.492710	830971.384570	45.514522
3501.538094	830959.701596	45.519527
3501.286577	830949.875018	45.524532
3500.962232	830953.885470	45.529537
3501.375184	830916.738937	45.534541
3500.799629	830907.503040	45.539546
3501.174843	830898.843307	45.544551
3501.425505	830894.356513	45.549556
3501.107887	830901.541278	45.554561
3501.121475	830894.015849	45.559565
3500.937720	830899.224480	45.564570
3500.989525	830884.658038	45.569575
3501.187992	830859.808406	45.574580
3501.162689	830864.258180	45.579585
3501.370480	830846.148586	45.584589
3501.408630	830845.751520	45.589594
3501.206224	830832.594703	45.594599
3501.492100	830820.725308	45.599604
3501.326216	830808.637187	45.604609
3501.643081	830793.831471	45.609613
3501.164968	830804.218216	45.614618
3501.261398	830788.227475	45.619623
3501.112310	830773.840433	45.624628
3500.995567	830755.442070	45.629633
3501.188864	830752.772196	45.634637
3501.139149	830748.237072	45.639642
3501.205606	830743.096569	45.644647
3501.139201	830753.415581	45.649652
3501.129898	830741.448103	45.654657
3501.533828	830710.799369	45.659661
3501.060614	830708.874356	45.664666
3501.173467	830697.668333	45.669671
3501.389984	830706.768330	45.674676
3500.952726	830696.336866	45.679681
3501.101758	830686.395059	45.684685
3500.818497	830674.130606	45.689690
3501.206169	830662.244156	45.694695
3501.090883	830664.461608	45.699700
3501.177610	830668.062547	45.704705
3501.157490	830667.919337	45.709709
3501.049333	830663.247218	45.714714
3501.072899	830659.188500	45.719719
3501.375091	830651.615254	45.724724
3500.978077	830624.224693	45.729729
3501.362588	830615.172220	45.734733
3501.177923	830625.999455	45.739738
3501.304391	830617.966573	45.744743
3501.076407	830604.764653	45.749748
3500.984800	830598.819549	45.754753
3501.385108	830574.961527	45.759757
3501.211553	830578.409970	45.764762
3501.125192	830566.796844	45.769767
3501.376826	830568.660764	45.774772
3501.201831	830574.943012	45.779777
3501.390368	830551.119784	45.784781
3501.189519	830533.320903	45.789786
3501.366258	830520.198713	45.794791
3501.735586	830511.002033	45.799796
3501.355613	830508.328775	45.804801
3501.288126	830464.858787	45.809805
3501.110932	830402.743673	45.814810
3501.125956	830276.643079	45.819815
3501.302556	830103.316686	45.824820
3500.893920	829873.453800	45.829825
3500.815537	829571.310655	45.834829
3500.879949	829234.094166	45.839834
3500.413382	828808.351012	45.844839
3500.294218	828352.809262	45.849844
3500.093405	827824.376791	45.854849
3499.860395	827243.655011	45.859853
3499.499518	826614.752110	45.864858
3499.411102	825916.028193	45.869863
3498.878667	825171.146507	45.874868
3498.526589	824357.103044	45.879873
3498.281294	823480.389176	45.884877
3497.608362	822558.139292	45.889882
3497.568158	821553.273083	45.894887
3496.628892	820514.886244	45.899892
3495.637930	819397.703535	45.904897
3495.379343	818226.225495	45.909901
3494.848457	817005.680953	45.914906
3494.087378	815722.816330	45.919911
3493.673711	814384.357810	45.924916
3492.975191	812979.355726	45.929921
3492.147027	811508.037819	45.934925
3491.238630	809983.242351	45.939930
3490.356133	808385.653142	45.944935
3489.677180	806742.451435	45.949940
3488.752187	805033.916211	45.954945
3487.868700	803269.371330	45.959949
3486.602456	801443.889703	45.964954
3485.537294	799562.187831	45.969959
3485.116197	797623.952904	45.974964
3483.800632	795632.094643	45.979969
3483.011639	793571.992006	45.984973
3481.704569	791458.157228	45.989978
3480.561830	789278.587073	45.994983
3479.539515	787046.015222	45.999988
3478.229828	784772.020803	46.004993
3477.002129	782425.364410	46.009997
3475.628240	780025.161708	46.015002
3474.437621	777568.011157	46.020007
3473.446793	775071.242119	46.025012
3471.938224	772516.758289	46.030017
3470.638559	769895.169273	46.035021
3469.135677	767233.790348	46.040026
3467.515612	764500.710851	46.045031
3466.546944	761726.568029	46.050036
3464.765829	758905.888846	46.055041
3463.423411	756010.180521	46.060045
3461.518565	753082.551788	46.065050
3460.438377	750094.086818	46.070055
3458.783642	747052.813896	46.075060
3457.318408	743964.043238	46.080065
3455.704848	740811.211346	46.085069
3453.918384	737625.384817	46.090074
3452.174287	734368.475204	46.095079
3450.931073	731067.374906	46.100084
3448.867100	727718.096700	46.105089
3446.944750	724310.619259	46.110093
3445.170610	720869.330167	46.115098
3443.358248	717366.497525	46.120103
3441.599454	713813.259281	46.125108
3439.731000	710217.288857	46.130113
3437.943076	706559.390115	46.135117
3435.904970	702868.874254	46.140122
3433.905770	699126.078586	46.145127
3431.957390	695328.264110	46.150132
3429.686800	691502.109365	46.155137
3427.807576	687602.922718	46.160141
3425.499712	683677.378112	46.165146
3423.374433	679711.059124	46.170151
3421.465070	675683.090523	46.175156
3419.215361	671618.985619	46.180161
3417.204523	667500.961131	46.185165
3414.907802	663347.870354	46.190170
3412.562832	659138.278624	46.195175
3410.852932	654896.399221	46.200180
3408.095215	650609.046583	46.205185
3406.091679	646268.838153	46.210189
3403.628041	641902.589132	46.215194
3400.871061	637477.036192	46.220199
3399.145055	633008.229583	46.225204
3396.453602	628494.264823	46.230209
3394.512705	623946.802194	46.235213
3391.672170	619356.824751	46.240218
3389.171785	614718.685853	46.245223
3386.811616	610052.151477	46.250228
3383.931491	605349.042474	46.255233
3381.631705	600594.751399	46.260237
3378.884354	595816.186065	46.265242
3376.145580	590985.333390	46.270247
3374.018747	586125.989440	46.275252
3370.911818	581228.054208	46.280257
3368.737291	576282.092447	46.285261
3365.771340	571308.344792	46.290266
3363.191234	566286.277160	46.295271
3359.958979	561243.942328	46.300276
3357.309429	556169.458261	46.305281
3354.402460	551055.451559	46.310285
3351.416554	545927.247685	46.315290
3348.696595	540741.580470	46.320295
3346.314266	535533.179948	46.325300
3343.210973	530293.096727	46.330305
3340.469265	525007.825301	46.335309
3337.634619	519696.880000	46.340314
3334.335838	514346.034147	46.345319
3331.498791	508985.514362	46.350324
3328.632435	503572.906506	46.355329
3325.313151	498137.506536	46.360333
3322.303750	492680.523855	46.365338
3319.060030	487187.644701	46.370343
3315.990021	481658.709745	46.375348
3312.622990	476120.598164	46.380353
3309.519119	470539.412349	46.385357
3306.665234	464957.524952	46.390362
3303.231672	459340.445688	46.395367
3300.565933	453703.685919	46.400372
3296.964288	448034.623396	46.405377
3293.906913	442342.825329	46.410381
3290.616825	436618.046753	46.415386
3287.274102	430871.598690	46.420391
3283.932522	425110.966935	46.425396
3280.660724	419328.586874	46.430401
3277.358002	413523.365926	46.435405
3273.930656	407708.332923	46.440410
3270.498314	401859.655216	46.445415
3267.392283	395990.292136	46.450420
3263.808641	390106.158161	46.455425
3260.343596	384199.494930	46.460429
3256.740939	378283.578942	46.465434
3253.380347	372341.433026	46.470439
3249.924200	366394.108517	46.475444
3246.146897	360430.856087	46.480449
3242.621038	354426.822053	46.485453
3238.849575	348437.592163	46.490458
3235.365435	342426.010139	46.495463
3232.273255	336400.247913	46.500468
3228.400741	330377.422825	46.505473
3224.981214	324316.861239	46.510477
3221.207901	318275.001137	46.515482
3217.209033	312193.959502	46.520487
3213.715308	306117.811998	46.525492
3209.745176	300035.801751	46.530497
3206.368813	293931.254311	46.535501
3202.333828	287839.927480	46.540506
3198.577412	281726.070380	46.545511
3194.586342	275604.948704	46.550516
3190.671742	269497.297609	46.555521
3187.262070	263373.687112	46.560525
3183.099980	257258.116501	46.565530
3179.150864	251138.767303	46.570535
3175.173990	245012.271706	46.575540
3171.205799	238889.529192	46.580545
3167.239665	232753.941928	46.585549
3163.291951	226630.902580	46.590554
3159.230824	220510.811226	46.595559
3155.452792	214371.226317	46.600564
3150.810585	208188.745075	46.605569
3146.561920	202070.519514	46.610573
3142.764631	195955.309025	46.615578
3138.694777	189861.588840	46.620583
3134.604229	183758.011989	46.625588
3130.011171	177686.692059	46.630593
3125.956820	171603.534051	46.635597
3121.957390	165541.737482	46.640602
3117.208367	159482.263688	46.645607
3112.758057	153445.937846	46.650612
3108.063072	147430.274067	46.655617
3103.883644	141418.042188	46.660621
3099.455811	135431.954916	46.665626
3094.567699	129458.413122	46.670631
3090.394500	123508.322558	46.675636
3085.391269	117581.366825	46.680641
3081.349730	111672.729346	46.685645
3076.714656	105780.471650	46.690650
3071.313502	99920.955656	46.695655
3066.805910	94081.752635	46.700660
3061.889561	88296.336735	46.705665
3057.000602	82514.641967	46.710669
3052.179857	76782.856378	46.715674
3046.589344	71067.935540	46.720679
3041.555162	65393.099413	46.725684
3036.447321	59769.002286	46.730689
3031.195538	54186.000043	46.735693
3025.366751	48661.375346	46.740698
3018.901271	43177.023497	46.745703
3012.569935	37753.854249	46.750708
3003.389665	32477.157206	46.755713
2986.911122	27496.131043	46.760717
2969.674677	22702.004297	46.765722
2952.531429	18142.857090	46.770727
2936.075531	13847.994522	46.775732
2919.241628	9837.730761	46.780737
2902.928632	6130.672264	46.785741
2880.000011	2927.522013	46.790746
2837.854878	621.459899	46.795751
2746.423210	291.357229	46.800756
2682.443505	280.632989	46.805761
2664.122358	263.864925	46.810765
2677.842873	266.363208	46.815770
2706.355183	272.037880	46.820775
2735.075763	270.534247	46.825780
2755.051196	263.743681	46.830785
2765.142028	244.441358	46.835789
2765.741380	254.600063	46.840794
2761.834200	257.871673	46.845799
2756.344859	262.725090	46.850804
2750.707362	271.986011	46.855809
2746.346573	260.715829	46.860813
2743.733726	250.032594	46.865818
2740.833502	241.913659	46.870823
2738.979343	242.011710	46.875828
2736.135730	250.483270	46.880833
2733.832360	253.311013	46.885837
2731.084675	246.250118	46.890842
2728.009095	244.889692	46.895847
2725.063693	241.228861	46.900852
2721.875022	251.318805	46.905857
2718.839620	241.850696	46.910861
2715.789698	244.984836	46.915866
2712.653638	246.997901	46.920871
2709.649441	235.644789	46.925876
2706.197364	243.321335	46.930881
2702.832136	239.709802	46.935885
2699.677713	237.252070	46.940890
2696.744574	232.358745	46.945895
2693.946263	227.873942	46.950900
2690.181028	242.221900	46.955905
2686.598151	235.180834	46.960909
2683.315127	229.850128	46.965914
2679.676877	235.924951	46.970919
2676.713642	225.145921	46.975924
2673.229325	231.840206	46.980929
2669.940473	232.942985	46.985933
2667.012443	230.157783	46.990938
2663.156273	229.010934	46.995943
2659.801647	219.490922	47.000948
2656.639276	234.056182	47.005953
2653.063074	231.471384	47.010957
2649.658340	231.302217	47.015962
2646.413741	220.764351	47.020967
2643.342799	225.404665	47.025972
2639.511430	221.405041	47.030977
2636.216545	234.808832	47.035981
2633.151832	238.031471	47.040986
2629.379303	223.604275	47.045991
2626.432837	219.289947	47.050996
2622.925010	210.105209	47.056001
2619.340239	219.618399	47.061005
2615.486242	217.070251	47.066010
2611.658405	221.609543	47.071015
2608.845159	219.109412	47.076020
2606.092050	216.937867	47.081025
2601.996217	223.184654	47.086029
2598.286082	218.323398	47.091034
2595.323827	214.487326	47.096039
2591.792214	221.677801	47.101044
2587.995555	228.978775	47.106049
2584.511202	222.371610	47.111053
2581.020336	214.041546	47.116058
2577.814908	213.305603	47.121063
2574.639067	211.464236	47.126068
2571.124969	208.806495	47.131073
2567.739347	206.246161	47.136077
2565.045245	201.896271	47.141082
2560.710954	206.131261	47.146087
2557.711095	204.323336	47.151092
2553.522796	211.459709	47.156097
2549.689813	214.151392	47.161101
2546.335487	209.166184	47.166106
2543.204951	213.497193	47.171111
2540.685849	198.567616	47.176116
2536.592694	204.868150	47.181121
2533.215086	199.932174	47.186125
2529.870563	202.904019	47.191130
2526.123692	210.267342	47.196135
2522.786609	200.218964	47.201140
2519.521743	197.774892	47.206145
2516.093816	205.705008	47.211149
2512.252413	198.547349	47.216154
2508.146307	205.362370	47.221159
2505.131144	200.855302	47.226164
2501.527096	208.510201	47.231169
2497.971209	203.821282	47.236173
2495.241016	193.584646	47.241178
2491.270410	203.343227	47.246183
2488.136822	200.924088	47.251188
2484.210796	209.827446	47.256193
2480.658051	200.879287	47.261197
2477.358154	197.939723	47.266202
2473.869584	203.850037	47.271207
2470.666545	192.989523	47.276212
2466.655166	199.551665	47.281217
2463.088425	202.254140	47.286221
2460.523286	193.082757	47.291226
2456.716853	201.737709	47.296231
2452.911751	191.800689	47.301236
2449.606094	194.980444	47.306241
2445.886115	189.709987	47.311245
2442.773059	196.950961	47.316250
2438.977638	202.769722	47.321255
2435.745045	196.014282	47.326260
2432.104807	191.953071	47.331265
2428.740972	197.679056	47.336269
2425.157170	192.620468	47.341274
2421.631398	198.792858	47.346279
2418.384515	194.103243	47.351284
2414.967117	202.156265	47.356289
2411.249371	195.283131	47.361293
2407.905082	194.919810	47.366298
2404.271750	203.851983	47.371303
2400.606287	198.783194	47.376308
2397.063122	197.385872	47.381313
2393.772349	190.875451	47.386317
2390.255354	190.835413	47.391322
2386.854247	196.768135	47.396327
2383.690621	193.179656	47.401332
2380.051196	187.135388	47.406337
2376.149101	186.771233	47.411341
2372.707506	186.870112	47.416346
2369.525723	194.049041	47.421351
2366.129719	194.441808	47.426356
2362.404480	194.187603	47.431361
2358.617533	193.818378	47.436365
2355.510452	189.173420	47.441370
2352.332952	189.261016	47.446375
2348.673188	187.779947	47.451380
2345.290193	194.068027	47.456385
2341.100796	191.653482	47.461389
2338.382217	182.718595	47.466394
2334.411146	192.887635	47.471399
2330.994644	186.094113	47.476404
2327.573299	185.947268	47.481409
2323.949201	184.729176	47.486413
2320.607975	185.529172	47.491418
2316.709581	188.142660	47.496423
2313.547779	183.469750	47.501428
2309.791763	177.494575	47.506433
2306.328708	184.254240	47.511437
2303.174919	175.220569	47.516442
2299.229296	176.308594	47.521447
2296.253432	179.220419	47.526452
2292.557798	195.207655	47.531457
2289.177544	179.957732	47.536461
2285.899760	171.217709	47.541466
2281.745626	177.608324	47.546471
2278.652052	175.419069	47.551476
2275.141610	179.571406	47.556481
2271.527805	174.465861	47.561485
2268.189270	176.269587	47.566490
2264.717813	182.921043	47.571495
2261.161774	166.793565	47.576500
2257.605038	177.161855	47.581505
2254.008630	173.401132	47.586509
2250.313155	171.158636	47.591514
2246.793144	177.950505	47.596519
2243.413328	173.911067	47.601524
2240.045068	177.469226	47.606529
2236.395025	181.553444	47.611533
2233.018379	183.588512	47.616538
2229.432449	181.061578	47.621543
2226.376915	177.107180	47.626548
2222.755618	173.198249	47.631553
2219.501458	183.262308	47.636557
2216.055845	183.354719	47.641562
2212.206086	173.925524	47.646567
2208.876493	169.109860	47.651572
2205.292811	179.920265	47.656577
2201.441315	174.236850	47.661581
2198.095894	167.280637	47.666586
2194.147082	180.180387	47.671591
2190.616285	180.088160	47.676596
2187.486598	177.348071	47.681601
2184.408164	177.340668	47.686605
2180.968153	167.808296	47.691610
2177.384861	170.699595	47.696615
2173.849559	171.608027	47.701620
2169.962938	171.595417	47.706625
2166.198355	170.029620	47.711629
2162.837975	156.618580	47.716634
2159.358835	171.898556	47.721639
2156.668143	172.191162	47.726644
2153.153862	170.273113	47.731649
2149.612474	165.703841	47.736653
2145.785167	163.749820	47.741658
2142.202162	170.379466	47.746663
2138.790778	168.488158	47.751668
2135.037823	173.536321	47.756673
2131.530077	171.625492	47.761677
2128.300931	162.112931	47.766682
2124.587886	170.362995	47.771687
2121.305025	167.620086	47.776692
2117.490429	167.133998	47.781697
2113.883718	169.589467	47.786701
2110.932910	165.830262	47.791706
2107.360354	168.190517	47.796711
2103.788257	156.572041	47.801716
2100.283422	166.448787	47.806721
2096.802618	162.163454	47.811725
2093.187746	158.178654	47.816730
2089.532468	162.032738	47.821735
2086.170682	161.209543	47.826740
2082.551032	170.570803	47.831745
2078.786371	170.316437	47.836749
2075.658774	159.415897	47.841754
2072.014336	166.476187	47.846759
2068.872970	160.459258	47.851764
2065.308571	159.813438	47.856769
2061.808578	169.740408	47.861773
2058.210053	157.001807	47.866778
2054.494502	157.066110	47.871783
2050.863077	158.076486	47.876788
2047.963963	160.880830	47.881793
2044.084418	171.389066	47.886797
2040.773465	164.119140	47.891802
2037.349500	166.998722	47.896807
2033.926818	162.225340	47.901812
2030.360153	157.638795	47.906817
2026.614527	165.843069	47.911821
2023.084459	164.716367	47.916826
2019.216641	172.087999	47.921831
2016.081347	157.163094	47.926836
2012.867565	155.109911	47.931841
2009.404556	156.331180	47.936845
2005.960068	160.192064	47.941850
2002.084413	163.921531	47.946855
1998.396380	161.381274	47.951860
1994.987155	159.585380	47.956865
1991.681935	151.615051	47.961869
1988.122632	156.017180	47.966874
1984.779953	155.524446	47.971879
1981.324325	158.263851	47.976884
1977.952285	162.897823	47.981889
1974.413351	162.606174	47.986893
1970.506742	158.337778	47.991898
1967.071281	161.931996	47.996903
1963.857560	155.536764	48.001908
1960.187883	159.577082	48.006913
1956.422969	172.826220	48.011917
1953.048571	156.539353	48.016922
1949.478222	155.000134	48.021927
1946.449232	161.939409	48.026932
1943.037567	165.597984	48.031937
1939.212661	168.910960	48.036941
1935.655063	155.860731	48.041946
1932.027889	155.773973	48.046951
1928.539315	160.578433	48.051956
1925.250418	154.256594	48.056961
1921.848633	160.273655	48.061965
1918.292633	163.677736	48.066970
1914.291451	166.863826	48.071975
1911.170845	157.218344	48.076980
1907.793658	152.681803	48.081985
1904.388673	162.755249	48.086989
1900.963861	163.391930	48.091994
1897.123801	158.247757	48.096999
1893.739065	157.728558	48.102004
1889.918618	160.252836	48.107009
1886.328404	158.903391	48.112013
1883.416530	152.575608	48.117018
1879.692837	154.492274	48.122023
1876.009316	158.353285	48.127028
1873.036627	159.567026	48.132033
1869.403481	161.806862	48.137037
1865.814677	142.901525	48.142042
1862.083886	152.575299	48.147047
1858.719499	139.018414	48.152052
1855.121865	148.599481	48.157057
1851.768402	157.765072	48.162061
1848.142381	158.194347	48.167066
1844.310508	153.303099	48.172071
1841.135329	146.841787	48.177076
1837.577618	160.151091	48.182081
1834.091779	154.139812	48.187085
1830.668310	146.579769	48.192090
1827.013795	149.092487	48.197095
1823.963776	141.284470	48.202100
1820.425426	151.832488	48.207105
1816.694532	155.547632	48.212109
1813.154015	150.381024	48.217114
1809.578944	158.806260	48.222119
1806.190301	151.667081	48.227124
1802.333157	154.354324	48.232129
1798.909107	159.181145	48.237133
1795.326532	158.018429	48.242138
1792.429360	159.025682	48.247143
1788.940521	150.785541	48.252148
1785.293654	143.513371	48.257153
1781.751406	143.071418	48.262157
1778.294534	149.493143	48.267162
1774.803741	156.912182	48.272167
1771.029298	143.192736	48.277172
1767.403274	143.989948	48.282177
1763.889875	139.591686	48.287181
1760.618127	147.665291	48.292186
1757.239421	148.447648	48.297191
1753.571121	154.611354	48.302196
1749.930260	148.947525	48.307201
1746.463193	152.010943	48.312205
1743.092198	139.821536	48.317210
1739.333522	155.804518	48.322215
1736.141869	146.427667	48.327220
1732.604262	150.323073	48.332225
1729.169467	141.228652	48.337229
1726.000387	143.658853	48.342234
1721.932711	142.931192	48.347239
1718.515343	150.334485	48.352244
1715.242042	144.215396	48.357249
1711.605199	149.662702	48.362253
1708.350103	146.664920	48.367258
1704.497675	142.200393	48.372263
1701.187272	139.791951	48.377268
1697.268395	150.101008	48.382273
1693.708586	148.221488	48.387277
1690.800431	144.276966	48.392282
1686.828671	148.113505	48.397287
1683.469076	156.170857	48.402292
1680.363162	144.855167	48.407297
1676.396492	148.090636	48.412301
1673.040826	140.187511	48.417306
1669.445619	140.913191	48.422311
1666.099922	136.374544	48.427316
1662.486507	147.673758	48.432321
1658.966998	147.995476	48.437325
1655.801549	152.836215	48.442330
1651.853702	146.967574	48.447335
1648.384878	136.886416	48.452340
1644.770920	144.075333	48.457345
1641.392685	146.640221	48.462349
1638.170390	142.231579	48.467354
1634.382757	141.104956	48.472359
1631.070421	140.206730	48.477364
1627.537685	136.961100	48.482369
1623.791348	146.432522	48.487373
1620.538280	142.778275	48.492378
1617.021041	151.291418	48.497383
1613.901012	142.268543	48.502388
1610.443592	143.463819	48.507393
1606.435377	144.641069	48.512397
1603.154537	142.267555	48.517402
1598.969573	139.456522	48.522407
1595.925145	140.190796	48.527412
1592.456875	144.513752	48.532417
1588.957840	141.728147	48.537421
1585.720059	132.526521	48.542426
1582.005117	131.637931	48.547431
1578.055494	147.581833	48.552436
1575.031076	141.949568	48.557441
1571.379225	145.078285	48.562445
1567.830380	132.790677	48.567450
1564.570368	145.948235	48.572455
1561.282496	140.672792	48.577460
1557.595366	149.817683	48.582465
1553.799330	138.106683	48.587469
1550.569988	139.850870	48.592474
1546.783990	145.978643	48.597479
1543.194593	141.662694	48.602484
1539.806114	138.283004	48.607489
1536.022613	141.855916	48.612493
1532.911509	133.845427	48.617498
1529.611518	138.405239	48.622503
1526.128693	138.099621	48.627508
1522.321951	138.481339	48.632513
1518.904614	138.168074	48.637517
1515.356043	140.964956	48.642522
1512.184853	141.304243	48.647527
1508.385330	136.344916	48.652532
1505.239322	131.045403	48.657537
1500.828863	138.518749	48.662541
1498.134792	137.746551	48.667546
1494.208884	143.322854	48.672551
1490.719789	139.493537	48.677556
1487.411052	133.481249	48.682561
1483.987074	135.964668	48.687565
1480.335042	133.749358	48.692570
1476.795144	135.905917	48.697575
1473.181440	140.083531	48.702580
1469.814682	133.068895	48.707585
1466.229972	137.432235	48.712589
1463.101842	135.279542	48.717594
1459.940281	136.911655	48.722599
1455.874194	135.385744	48.727604
1452.513778	135.741884	48.732609
1448.469332	146.302435	48.737613
1445.063492	135.222946	48.742618
1441.655573	141.539551	48.747623
1438.304491	132.420835	48.752628
1434.938400	133.839675	48.757633
1431.026943	142.942516	48.762637
1428.061675	130.092031	48.767642
1424.322503	135.851635	48.772647
1420.467459	134.829092	48.777652
1417.399421	128.856538	48.782657
1413.793329	134.985063	48.787661
1410.538900	135.427026	48.792666
1407.181332	135.177353	48.797671
1403.627291	134.930610	48.802676
1399.938477	133.484927	48.807681
1396.000558	135.467677	48.812685
1393.053428	141.996035	48.817690
1389.699568	131.085095	48.822695
1385.879585	131.283101	48.827700
1382.156038	132.715581	48.832705
1378.532463	129.292894	48.837709
1375.103275	129.832086	48.842714
1371.684438	134.717418	48.847719
1367.936019	131.697148	48.852724
1364.994221	123.620924	48.857729
1361.498882	134.468932	48.862733
1357.850449	133.995786	48.867738
1354.166997	136.234997	48.872743
1350.976193	136.504489	48.877748
1347.703062	127.821854	48.882753
1343.196878	142.437331	48.887757
1339.896188	130.173827	48.892762
1336.499790	133.182948	48.897767
1333.281698	138.323638	48.902772
1330.005020	123.862528	48.907777
1325.971369	136.357307	48.912781
1322.711985	133.335072	48.917786
1319.148123	134.311080	48.922791
1315.406443	139.559116	48.927796
1312.367086	120.123596	48.932801
1308.811310	126.675685	48.937805
1305.501200	130.143541	48.942810
1301.622912	140.869606	48.947815
1297.826798	135.175040	48.952820
1294.927317	134.795844	48.957825
1291.407333	133.914397	48.962829
1288.151216	124.019053	48.967834
1284.258697	130.540117	48.972839
1280.715639	131.692168	48.977844
1277.071213	133.939677	48.982849
1273.698297	138.537581	48.987853
1270.045403	123.799621	48.992858
1266.632115	123.515213	48.997863
1263.142391	137.872868	49.002868
1260.066583	135.365445	49.007873
1256.128131	130.669534	49.012877
1252.788608	119.971687	49.017882
1249.103796	126.949993	49.022887
1245.641402	137.201158	49.027892
1242.251347	136.237615	49.032897
1238.573079	135.079938	49.037901
1234.996282	120.650575	49.042906
1231.579826	117.604692	49.047911
1227.866672	125.802752	49.052916
1224.847483	124.355153	49.057921
1221.277155	131.541488	49.062925
1217.958341	129.006817	49.067930
1214.462427	121.285261	49.072935
1210.379724	119.930552	49.077940
1206.729728	129.291038	49.082945
1203.734599	129.992283	49.087949
1200.639552	119.833723	49.092954
1197.005504	124.121570	49.097959
1192.886992	131.720329	49.102964
1189.690941	115.783309	49.107969
1185.866317	120.181645	49.112973
1182.521619	126.572763	49.117978
1179.033938	127.514266	49.122983
1175.322872	126.683761	49.127988
1172.433598	125.614401	49.132993
1168.558614	140.264082	49.137997
1164.994794	131.614835	49.143002
1161.243081	127.967372	49.148007
1157.877276	131.574913	49.153012
1155.041326	120.295971	49.158017
1150.969887	127.081638	49.163021
1147.977286	116.245095	49.168026
1144.346776	129.824927	49.173031
1140.690635	132.435525	49.178036
1137.228685	124.379975	49.183041
1133.196029	124.711592	49.188045
1129.933461	122.618052	49.193050
1126.415891	129.824231	49.198055
1122.618121	139.757985	49.203060
1119.879188	123.897963	49.208065
1116.250740	122.555533	49.213069
1112.828490	109.003070	49.218074
1109.027088	114.294011	49.223079
1105.237799	122.539125	49.228084
1102.322907	115.501012	49.233089
1098.529912	121.878763	49.238093
1095.510169	120.310460	49.243098
1091.570845	122.052094	49.248103
1087.680510	118.858991	49.253108
1084.610202	114.763153	49.258113
1081.215059	125.902535	49.263117
1077.667090	130.110623	49.268122
1073.820820	124.477064	49.273127
1070.046011	122.366703	49.278132
1067.323619	119.757815	49.283137
1063.476067	134.864130	49.288141
1060.114807	128.815760	49.293146
1056.554322	121.833049	49.298151
1052.953481	126.694504	49.303156
1049.600532	126.811250	49.308161
1045.642397	121.563973	49.313165
1042.498836	120.176257	49.318170
1039.188397	126.126898	49.323175
1035.597409	116.923628	49.328180
1032.003523	109.977036	49.333185
1028.231713	121.054511	49.338189
1025.197716	123.196629	49.343194
1021.541373	126.036303	49.348199
1018.006866	123.231805	49.353204
1014.451374	117.364703	49.358209
1010.489488	121.097559	49.363213
1007.469005	123.278790	49.368218
1004.157845	122.188295	49.373223
1000.674581	120.539700	49.378228
997.855708	125.750366	49.383233
993.533380	125.304524	49.388237
989.798604	122.741668	49.393242
986.434372	129.125046	49.398247
982.405902	122.615164	49.403252
979.664920	122.987155	49.408257
976.330741	125.182802	49.413261
972.570021	125.928075	49.418266
968.738143	119.644424	49.423271
965.173621	122.733269	49.428276
961.827611	114.893293	49.433281
958.272313	123.942572	49.438285
954.823689	117.538627	49.443290
951.762452	117.357753	49.448295
947.740378	122.414990	49.453300
944.514199	119.341395	49.458305
940.782360	119.857077	49.463309
937.098611	120.254620	49.468314
934.322919	112.417178	49.473319
930.264898	119.489907	49.478324
926.931787	117.974608	49.483329
923.305717	121.997166	49.488333
919.924606	118.711994	49.493338
916.600999	116.723944	49.498343
913.023021	117.455255	49.503348
909.436840	118.223834	49.508353
905.674380	118.191026	49.513357
902.569553	115.161543	49.518362
899.258478	106.871093	49.523367
895.162201	119.293721	49.528372
891.896614	122.114717	49.533377
888.050054	116.253033	49.538381
884.765988	112.177201	49.543386
881.610453	110.579330	49.548391
878.083041	116.401994	49.553396
874.301231	117.550956	49.558401
870.573501	113.167574	49.563405
867.291799	114.023427	49.568410
863.889153	114.896292	49.573415
860.122103	118.827717	49.578420
857.093812	106.194180	49.583425
853.316892	110.081953	49.588429
849.796369	111.466489	49.593434
846.380632	110.101813	49.598439
842.507193	109.808166	49.603444
839.358345	104.693471	49.608449
835.344857	113.988838	49.613453
832.142015	115.097764	49.618458
829.208821	116.614604	49.623463
825.380059	122.750175	49.628468
821.785133	117.569052	49.633473
817.821849	123.668534	49.638477
814.361087	113.782110	49.643482
811.174034	113.183546	49.648487
807.791043	117.506583	49.653492
804.411770	112.292328	49.658497
800.990642	111.323982	49.663501
797.407193	121.081698	49.668506
794.072794	117.225253	49.673511
790.234063	113.373760	49.678516
787.039722	110.236782	49.683521
783.335012	123.000581	49.688525
779.584323	120.179135	49.693530
776.261883	112.179301	49.698535
772.184436	110.727116	49.703540
769.406457	107.326445	49.708545
765.098978	116.076681	49.713549
762.135628	111.998563	49.718554
759.031444	101.171402	49.723559
755.387656	111.904749	49.728564
751.887800	111.744309	49.733569
748.297003	120.085460	49.738573
744.959514	102.492464	49.743578
741.173396	117.465624	49.748583
737.589692	120.842376	49.753588
734.418152	109.298061	49.758593
730.631688	109.131788	49.763597
727.280801	101.472022	49.768602
723.532557	107.683429	49.773607
719.952364	116.545426	49.778612
716.540704	111.296612	49.783617
712.778273	120.464358	49.788621
709.578112	106.068865	49.793626
706.138827	100.560619	49.798631
702.723576	124.864490	49.803636
699.541635	110.522521	49.808641
695.638860	119.330465	49.813645
692.382363	109.608982	49.818650
688.996005	111.518990	49.823655
685.200883	103.415454	49.828660
681.752055	102.862455	49.833665
677.989986	104.790219	49.838669
674.354201	105.191627	49.843674
671.192997	96.726706	49.848679
667.564430	109.619540	49.853684
664.206826	102.638593	49.858689
660.612682	111.617952	49.863693
656.889288	102.226660	49.868698
653.468110	112.658985	49.873703
650.221209	115.062152	49.878708
646.856507	108.625787	49.883713
643.155006	109.408621	49.888717
639.733325	112.215160	49.893722
636.168947	101.036201	49.898727
632.432278	105.361891	49.903732
629.168402	99.521251	49.908737
625.963892	111.365293	49.913741
622.297538	107.266319	49.918746
618.270603	106.504379	49.923751
614.974558	112.848435	49.928756
611.487742	96.464773	49.933761
607.780533	107.854661	49.938765
604.530166	112.978783	49.943770
601.547422	110.165078	49.948775
597.952899	107.946492	49.953780
594.054335	105.070066	49.958785
590.548655	116.315989	49.963789
587.125994	106.359194	49.968794
583.471227	105.483419	49.973799
579.830006	111.720238	49.978804
576.634311	106.646469	49.983809
572.821365	107.726355	49.988813
569.688320	99.432843	49.993818
566.179545	103.485037	49.998823
562.126741	116.565590	50.003828
558.854266	104.031363	50.008833
555.321188	108.451523	50.013837
552.042526	117.807390	50.018842
548.826288	111.694916	50.023847
545.151090	114.066667	50.028852
541.968929	109.142907	50.033857
538.194390	106.305126	50.038861
534.439551	108.772119	50.043866
531.119527	105.912049	50.048871
527.110465	110.273415	50.053876
523.931929	108.044270	50.058881
520.349722	104.834069	50.063885
517.127265	111.289925	50.068890
513.676895	106.049400	50.073895
509.686197	113.750428	50.078900
506.303346	108.144479	50.083905
503.110398	104.672974	50.088909
499.597335	113.777527	50.093914
496.422921	105.440868	50.098919
492.493021	115.341082	50.103924
488.679535	97.220749	50.108929
485.305634	107.147903	50.113933
481.995684	114.458979	50.118938
478.658760	108.854140	50.123943
475.139582	108.319876	50.128948
471.438081	104.984088	50.133953
468.020564	107.168092	50.138957
464.328531	108.907516	50.143962
460.850059	111.895088	50.148967
457.532069	109.087108	50.153972
454.245753	103.788345	50.158977
450.365713	106.918714	50.163981
446.739812	105.593801	50.168986
443.341385	102.785601	50.173991
439.731802	105.737917	50.178996
436.313832	95.986543	50.184001
433.177641	103.460226	50.189005
429.403217	112.574539	50.194010
425.767293	104.097509	50.199015
422.484691	103.214313	50.204020
419.096120	88.126405	50.209025
415.400040	101.762521	50.214029
411.667926	100.111258	50.219034
408.442633	94.959997	50.224039
404.867579	97.222739	50.229044
401.487504	97.605240	50.234049
397.641934	105.309480	50.239053
393.886592	103.008663	50.244058
391.115460	95.507861	50.249063
387.466058	105.181440	50.254068
383.774335	94.080320	50.259073
380.432635	103.112513	50.264077
377.041779	90.845400	50.269082
373.672929	93.276832	50.274087
369.651661	98.102013	50.279092
366.467592	99.131797	50.284097
362.794192	106.341955	50.289101
359.089951	95.531194	50.294106
355.752532	92.102678	50.299111
352.431764	102.529681	50.304116
348.744168	92.406281	50.309121
344.990978	102.546503	50.314125
341.721373	93.287838	50.319130
338.390025	98.752795	50.324135
334.560374	100.800043	50.329140
331.605954	94.831004	50.334145
328.100384	101.942714	50.339149
324.425337	101.407350	50.344154
320.718352	99.223586	50.349159
317.080540	103.854927	50.354164
313.752395	89.548332	50.359169
310.172719	91.937575	50.364173
306.810798	105.374102	50.369178
303.606512	92.505288	50.374183
300.058051	103.828635	50.379188
296.570435	88.560058	50.384193
292.677931	92.402800	50.389197
288.878660	99.181448	50.394202
285.631466	99.137170	50.399207
281.964212	104.165158	50.404212
278.769916	98.915616	50.409217
275.412274	99.786279	50.414221
271.816446	101.689764	50.419226
268.511244	99.967562	50.424231
264.561696	106.905620	50.429236
261.102540	98.812964	50.434241
258.056887	97.613384	50.439245
254.133407	100.873178	50.444250
250.948684	104.273443	50.449255
247.103467	106.722575	50.454260
243.396487	91.458608	50.459265
239.933727	99.067616	50.464269
236.696107	99.996407	50.469274
233.350065	107.870959	50.474279
229.599802	111.069296	50.479284
226.373785	100.466504	50.484289
223.005014	100.621209	50.489293
219.337905	97.592833	50.494298
215.663467	95.254587	50.499303
212.059406	101.027778	50.504308
208.613968	91.984905	50.509313
205.122663	95.716521	50.514317
201.633005	100.254975	50.519322
198.518498	89.120574	50.524327
194.736605	95.767356	50.529332
191.344246	83.777548	50.534337
187.841627	90.190642	50.539341
184.246694	99.315958	50.544346
180.555022	101.587039	50.549351
177.002318	97.720051	50.554356
173.793165	92.146177	50.559361
170.272658	87.591767	50.564365
166.445755	86.472386	50.569370
163.098934	86.150144	50.574375
159.345804	95.107157	50.579380
156.139404	94.491793	50.584385
152.722516	95.318541	50.589389
149.120321	89.456338	50.594394
145.834413	86.090462	50.599399
141.991418	104.771092	50.604404
138.557572	96.303089	50.609409
135.353630	100.863228	50.614413
131.594948	83.427889	50.619418
128.179084	86.653106	50.624423
124.695168	93.209251	50.629428
121.382610	89.782086	50.634433
117.518976	84.738542	50.639437
113.694702	79.862626	50.644442
110.663952	77.361457	50.649447
106.902214	97.307247	50.654452
103.639310	92.568541	50.659457
99.968168	102.155672	50.664461
96.929418	95.879270	50.669466
93.296886	85.475352	50.674471
89.700364	81.887064	50.679476
86.006766	87.995742	50.684481
82.490326	96.983729	50.689485
78.880624	97.766708	50.694490
75.544216	85.273463	50.699495
71.842687	89.196945	50.704500
68.853246	85.865586	50.709505
64.997472	87.020521	50.714509
61.290620	87.559605	50.719514
58.108530	87.085891	50.724519
54.456002	92.948361	50.729524
51.107153	82.821287	50.734529
47.314887	88.845167	50.739533
43.931738	91.355981	50.744538
40.561358	98.225088	50.749543
37.164583	100.217549	50.754548
33.832147	85.204591	50.759553
30.041155	90.530674	50.764557
26.221953	93.760246	50.769562
23.028828	92.840376	50.774567
19.496440	94.510059	50.779572
15.970578	85.131558	50.784577
12.563659	88.582857	50.789581
8.999598	103.180736	50.794586
5.367530	87.960016	50.799591
2.010790	90.328664	50.804596