Thu Jun 16 18:19:00 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.314654	116.889474	0.000000
-0.302752	119.629355	0.005005
0.267960	113.772141	0.010010
0.257748	104.266842	0.015014
-0.253687	109.692873	0.020019
0.109646	104.623073	0.025024
-0.191436	109.856592	0.030029
-0.280547	88.532937	0.035034
-0.338961	75.221195	0.040038
-0.967796	62.440775	0.045043
-1.003605	50.908617	0.050048
-1.574031	47.835832	0.055053
-1.786313	23.426948	0.060058
-2.015385	16.485717	0.065062
-2.458027	14.297675	0.070067
-2.942593	7.083763	0.075072
-2.917459	11.618923	0.080077
-3.471450	9.161605	0.085082
-3.746371	5.057488	0.090086
-3.965428	5.583302	0.095091
-4.089226	-9.092124	0.100096
-4.419224	0.110100	0.105101
-4.643283	-6.129327	0.110106
-4.809227	-3.497123	0.115110
-5.445832	-0.015853	0.120115
-5.578984	-8.806035	0.125120
-6.039933	-8.429566	0.130125
-5.876223	-2.153948	0.135130
-6.138291	-16.161707	0.140134
-7.055430	-1.143320	0.145139
-7.046355	-7.986172	0.150144
-7.343502	-13.158894	0.155149
-7.122690	2.245911	0.160154
-7.543932	-12.897112	0.165158
-7.339376	-10.804023	0.170163
-7.777631	-14.197561	0.175168
-8.471278	-1.745822	0.180173
-8.786758	1.733583	0.185178
-8.741106	-5.690869	0.190182
-9.125618	-7.293425	0.195187
-9.048571	-17.649960	0.200192
-9.608698	-10.779900	0.205197
-9.601185	1.322650	0.210202
-10.058751	-14.567601	0.215206
-10.425276	-6.116917	0.220211
-10.220647	-11.471315	0.225216
-10.580238	-20.858421	0.230221
-11.405337	-6.252829	0.235226
-11.252804	-9.831606	0.240230
-11.627225	-8.541485	0.245235
-11.646137	-10.919907	0.250240
-11.799691	-13.339610	0.255245
-12.433489	-7.694608	0.260250
-12.794216	-6.744545	0.265254
-13.012684	-0.078136	0.270259
-12.929098	-5.678606	0.275264
-13.083420	-13.629381	0.280269
-13.623814	-15.275136	0.285274
-14.525980	-12.361150	0.290278
-14.798633	-1.703080	0.295283
-13.893197	-13.931168	0.300288
-14.539065	-6.883071	0.305293
-15.007703	-4.383751	0.310298
-14.828788	-11.595424	0.315302
-14.890275	-10.676660	0.320307
-15.643961	-14.654001	0.325312
-16.083181	-4.437018	0.330317
-16.778261	1.948755	0.335322
-16.553889	-15.160015	0.340326
-16.669546	-3.898374	0.345331
-16.173408	-11.939971	0.350336
-16.799253	-8.755656	0.355341
-17.409787	-1.348075	0.360346
-17.639615	-6.153976	0.365350
-18.030913	-5.413041	0.370355
-17.827755	-6.003337	0.375360
-17.902513	-15.581554	0.380365
-18.792129	-14.750376	0.385370
-19.098620	-15.617328	0.390374
-19.639443	1.907555	0.395379
-19.386619	-2.206428	0.400384
-19.588860	-1.940092	0.405389
-19.922659	-4.787080	0.410394
-19.805988	-11.744688	0.415398
-20.113912	-1.191086	0.420403
-20.649708	-17.101847	0.425408
-21.022118	-7.349918	0.430413
-21.195734	-10.603395	0.435418
-21.115876	-15.662121	0.440422
-21.347183	-9.292815	0.445427
-21.523449	-12.674204	0.450432
-21.975989	-8.712912	0.455437
-22.895680	-9.143889	0.460442
-22.763314	-11.511399	0.465446
-22.616329	-0.004100	0.470451
-22.640156	-10.235349	0.475456
-23.625695	-11.314066	0.480461
-24.212148	-9.431700	0.485466
-24.078229	-16.067286	0.490470
-24.605164	-8.721964	0.495475
-24.499774	-12.619300	0.500480
-24.653411	-9.157173	0.505485
-24.644833	-6.002921	0.510490
-24.849530	-16.033503	0.515494
-25.073860	-15.444763	0.520499
-25.288973	-2.998116	0.525504
-25.929011	-8.224172	0.530509
-26.296030	-21.287714	0.535514
-26.105881	-17.802886	0.540518
-26.499369	-15.309180	0.545523
-26.956446	-17.522354	0.550528
-27.671918	-19.065774	0.555533
-28.164376	-11.341593	0.560538
-27.911240	-23.916280	0.565542
-27.936894	-10.974626	0.570547
-27.790783	-15.366145	0.575552
-27.935232	-9.242639	0.580557
-28.015779	-3.029160	0.585562
-28.483086	-12.690882	0.590566
-28.800989	-5.483592	0.595571
-28.800507	-13.014719	0.600576
-30.233017	-15.504820	0.605581
-30.627741	-9.209629	0.610586
-30.387673	-11.553996	0.615590
-30.555328	-11.709109	0.620595
-30.758615	-16.532512	0.625600
-30.711403	-9.433214	0.630605
-30.562778	-4.566565	0.635610
-30.642017	-14.041932	0.640614
-31.809695	-12.275128	0.645619
-31.971477	-11.445253	0.650624
-32.184250	-7.312856	0.655629
-32.411153	-7.274087	0.660634
-32.503814	-11.712373	0.665638
-33.079156	-8.446923	0.670643
-33.150465	-9.851147	0.675648
-33.400004	-4.841352	0.680653
-33.934821	-14.200093	0.685658
-33.474209	-19.816003	0.690662
-34.236496	-11.908324	0.695667
-34.064203	-17.086111	0.700672
-34.859502	-4.421843	0.705677
-35.009770	1.281470	0.710682
-34.661979	-9.362010	0.715686
-35.209431	6.167193	0.720691
-35.398499	-9.672720	0.725696
-36.459534	-19.612981	0.730701
-37.188957	-4.099689	0.735706
-36.433553	-10.100636	0.740710
-36.582765	-2.807671	0.745715
-36.944613	-12.831225	0.750720
-37.373391	0.774120	0.755725
-37.319659	-2.326723	0.760730
-37.159087	-12.702093	0.765734
-37.504828	-5.687415	0.770739
-38.353528	-7.400307	0.775744
-38.613896	-5.096903	0.780749
-38.991123	-0.419980	0.785754
-38.641669	-10.408071	0.790758
-39.004407	0.049423	0.795763
-39.041057	-11.787684	0.800768
-39.959626	-8.675745	0.805773
-40.448647	-19.173427	0.810778
-40.253701	-16.606786	0.815782
-40.342866	-3.065561	0.820787
-40.728133	-4.688215	0.825792
-40.455888	-3.847591	0.830797
-40.724942	-8.779599	0.835802
-41.586698	-12.999723	0.840806
-41.933133	-1.733288	0.845811
-41.729851	4.457259	0.850816
-42.052641	-0.336829	0.855821
-42.162959	-1.921657	0.860826
-42.815573	-9.031819	0.865830
-43.547434	7.667130	0.870835
-43.486058	-15.306091	0.875840
-43.874521	-13.032426	0.880845
-43.749389	-1.913377	0.885850
-43.663658	-13.974529	0.890854
-44.139216	-13.298197	0.895859
-43.842544	-11.545007	0.900864
-44.238932	-4.274137	0.905869
-45.001139	-4.382293	0.910874
-44.858738	-8.274401	0.915878
-45.087814	-6.511077	0.920883
-45.436883	-6.861241	0.925888
-46.145257	-8.518299	0.930893
-46.952007	2.138558	0.935898
-46.726941	-1.736433	0.940902
-46.879539	1.776135	0.945907
-46.846675	-12.105051	0.950912
-46.855064	-6.513682	0.955917
-46.873264	-4.545673	0.960922
-47.432901	-7.788135	0.965926
-48.188550	-8.566453	0.970931
-48.276425	-1.754407	0.975936
-48.266875	-7.405877	0.980941
-48.549185	-2.434370	0.985946
-48.657582	-14.890614	0.990950
-49.424663	-6.626489	0.995955
-49.721556	-5.056272	1.000960
-49.866464	-9.685897	1.005965
-50.032468	-8.168585	1.010970
-49.990909	-12.912289	1.015974
-50.029857	-4.688586	1.020979
-50.615971	-14.654652	1.025984
-51.113135	-9.578778	1.030989
-51.750215	-7.659927	1.035994
-51.387724	-31.066950	1.040998
-51.924815	-5.654442	1.046003
-51.755863	-1.016876	1.051008
-51.702422	-13.246521	1.056013
-52.468764	-2.574246	1.061018
-52.930997	-10.892430	1.066022
-53.519009	-17.648732	1.071027
-53.335401	-19.599999	1.076032
-53.329759	-12.955639	1.081037
-53.804299	-3.580661	1.086042
-53.428191	-9.694531	1.091046
-53.934516	-10.807650	1.096051
-54.390127	-6.521964	1.101056
-54.602106	-9.606022	1.106061
-54.886337	-1.707002	1.111066
-54.900845	-15.213161	1.116070
-55.906167	-9.930975	1.121075
-56.231671	-3.241650	1.126080
-56.669984	-6.987473	1.131085
-56.199345	-7.492145	1.136090
-55.964229	-16.094470	1.141094
-56.593870	-7.887983	1.146099
-56.680933	-14.092821	1.151104
-57.031131	-15.246836	1.156109
-58.045868	-3.966739	1.161114
-58.171948	-19.582445	1.166118
-58.096530	-8.378039	1.171123
-58.376875	-11.457605	1.176128
-58.391572	-7.464196	1.181133
-58.465222	-3.074413	1.186138
-58.358694	-11.914656	1.191142
-58.982353	-10.527701	1.196147
-59.563151	-5.551261	1.201152
-59.685430	-17.998893	1.206157
-60.097021	0.251445	1.211162
-60.102438	-13.639492	1.216166
-60.233163	-12.970722	1.221171
-60.904004	-8.611089	1.226176
-61.306986	-11.368306	1.231181
-61.462681	-8.562882	1.236186
-61.422927	-8.664271	1.241190
-61.657516	-8.074426	1.246195
-61.757575	-11.477088	1.251200
-61.485967	-10.043049	1.256205
-62.335654	-7.843804	1.261210
-62.662219	-8.452216	1.266214
-63.222274	-4.924697	1.271219
-63.070567	-10.508995	1.276224
-63.202444	-10.323050	1.281229
-63.953431	-5.945041	1.286234
-64.494390	-0.109483	1.291238
-65.016016	-9.541433	1.296243
-65.097021	-4.838587	1.301248
-64.594238	-10.098913	1.306253
-65.045326	-10.392062	1.311258
-65.131055	-12.237653	1.316262
-64.974006	-8.707597	1.321267
-65.164125	-9.832919	1.326272
-65.673231	-14.009212	1.331277
-66.354046	-2.790514	1.336282
-66.194866	-6.635476	1.341286
-66.500032	-11.288533	1.346291
-67.474114	-4.790848	1.351296
-67.821470	-1.609440	1.356301
-67.426040	1.197935	1.361306
-67.768107	0.507932	1.366310
-68.095343	10.175750	1.371315
-67.932127	3.400455	1.376320
-68.021318	-5.945017	1.381325
-68.370582	0.446252	1.386330
-68.772480	-4.563835	1.391334
-69.460565	-6.533725	1.396339
-69.961497	-9.368673	1.401344
-69.772555	2.560541	1.406349
-69.957123	3.550651	1.411354
-69.824175	-8.678817	1.416358
-70.900309	-8.792604	1.421363
-71.129056	-10.979384	1.426368
-70.872044	-9.763428	1.431373
-71.432193	1.915584	1.436378
-71.227966	-8.678814	1.441382
-71.320557	-16.057521	1.446387
-71.898268	-11.869155	1.451392
-72.803679	-15.671357	1.456397
-72.961198	-14.227564	1.461402
-72.960036	-12.271143	1.466406
-73.114298	2.084584	1.471411
-73.089162	-15.071853	1.476416
-72.921618	-21.401044	1.481421
-73.170826	-8.834628	1.486426
-74.192935	-2.173523	1.491430
-74.288969	3.953232	1.496435
-74.490281	-8.242993	1.501440
-74.698130	-4.796471	1.506445
-74.969891	-11.279970	1.511450
-75.233669	-1.492719	1.516454
-75.740987	-2.273895	1.521459
-75.994719	-3.882276	1.526464
-76.282802	-13.357554	1.531469
-76.481299	-4.636900	1.536474
-76.122319	-11.648264	1.541478
-76.221993	-7.971898	1.546483
-76.774375	-5.484484	1.551488
-77.212717	-4.323886	1.556493
-78.043974	-5.388334	1.561498
-77.885488	-11.386129	1.566502
-77.941874	-15.292736	1.571507
-78.143042	-14.315669	1.576512
-77.892382	-14.326918	1.581517
-78.753439	-7.202412	1.586522
-79.461045	-3.434058	1.591526
-79.439309	-0.461829	1.596531
-79.614488	-5.715080	1.601536
-79.560878	-5.145537	1.606541
-79.964792	-4.828013	1.611546
-80.274931	-5.732638	1.616550
-81.280905	-0.825622	1.621555
-81.053053	-1.659536	1.626560
-81.153549	-13.306631	1.631565
-81.456107	-10.395544	1.636570
-80.958347	-12.581244	1.641574
-81.153422	-0.114334	1.646579
-81.583301	-9.528986	1.651584
-82.338036	-6.357598	1.656589
-82.841235	-2.193875	1.661594
-82.963698	-7.005773	1.666598
-82.897618	-5.892236	1.671603
-82.955520	3.335260	1.676608
-83.690322	-3.608201	1.681613
-84.472652	-8.007975	1.686618
-84.370444	-10.645354	1.691622
-84.622109	-3.574304	1.696627
-84.479000	2.246855	1.701632
-84.530204	-9.828561	1.706637
-84.842743	-12.182031	1.711642
-84.487404	-18.802116	1.716646
-85.403949	-13.597740	1.721651
-85.850979	-14.853346	1.726656
-85.973942	-8.068852	1.731661
-86.317427	8.424535	1.736666
-85.757251	-6.769589	1.741670
-86.543132	-8.323958	1.746675
-87.190721	-4.616921	1.751680
-87.165431	-10.855125	1.756685
-87.612184	3.090589	1.761690
-87.546070	-9.234280	1.766694
-87.872357	-7.320521	1.771699
-88.891584	-8.076780	1.776704
-88.620419	-12.093656	1.781709
-88.643361	-2.933404	1.786714
-88.585276	-16.158845	1.791718
-89.147775	-3.698398	1.796723
-90.172835	2.801995	1.801728
-90.459731	-12.575913	1.806733
-90.275516	-6.268080	1.811738
-89.977431	-20.165264	1.816742
-90.576714	-9.323985	1.821747
-90.370157	0.735464	1.826752
-90.629519	0.999896	1.831757
-91.589722	-0.252092	1.836762
-91.557004	-7.547825	1.841766
-91.999629	-13.541574	1.846771
-92.272165	-7.333958	1.851776
-92.219043	-7.943953	1.856781
-92.364960	-2.701391	1.861786
-92.333682	-5.904081	1.866790
-93.207546	-8.260969	1.871795
-93.336653	-9.685926	1.876800
-93.285190	-15.748704	1.881805
-93.755593	-1.953877	1.886810
-94.013464	-8.402280	1.891814
-94.042649	-1.891660	1.896819
-95.151062	-5.440112	1.901824
-95.029913	-12.247612	1.906829
-95.676625	-2.810440	1.911834
-95.466286	-9.006322	1.916838
-95.670150	1.504824	1.921843
-95.811583	-10.238995	1.926848
-95.535104	-6.072032	1.931853
-96.009580	-0.117829	1.936858
-96.534306	-6.294334	1.941862
-96.666310	-3.325407	1.946867
-97.177195	-5.615118	1.951872
-97.177911	-8.141074	1.956877
-97.542154	-2.224131	1.961882
-97.693378	-4.548127	1.966886
-97.942158	0.732549	1.971891
-98.817007	-8.690739	1.976896
-98.495995	-14.649492	1.981901
-98.819814	-4.333100	1.986906
-98.803080	-6.214664	1.991910
-98.778944	-3.377695	1.996915
-99.516916	-11.998109	2.006912
-99.927772	-6.765151	2.016909
-99.074759	0.430934	2.026906
-98.067048	-5.645429	2.036902
-98.049257	0.048923	2.046899
-97.317966	-3.261712	2.056896
-96.751351	-7.524942	2.066893
-96.797030	-4.255951	2.076890
-95.332232	-5.702899	2.086886
-94.700492	-12.271978	2.096883
-94.716242	-0.108324	2.106880
-94.695414	-8.586739	2.116877
-93.837924	-1.113324	2.126874
-93.031188	-0.010921	2.136870
-93.151566	-3.214781	2.146867
-92.062499	-11.574386	2.156864
-91.907844	1.169599	2.166861
-91.290043	-8.508001	2.176858
-90.344436	-12.949835	2.186854
-90.122297	-9.918324	2.196851
-90.118060	-4.426012	2.206848
-89.240482	-5.336530	2.216845
-88.493295	-4.275750	2.226842
-88.239610	-7.236986	2.236838
-88.070931	-5.843522	2.246835
-87.007622	-11.502532	2.256832
-87.122107	-16.302979	2.266829
-86.491804	-9.479142	2.276826
-85.611719	-4.904249	2.286822
-85.371515	-7.856046	2.296819
-84.273201	-10.046800	2.306816
-83.965733	-9.929018	2.316813
-83.854948	-12.390115	2.326810
-83.846095	-8.786081	2.336806
-82.806522	-10.029889	2.346803
-82.327317	-13.245714	2.356800
-81.318905	-12.254580	2.366797
-81.116970	-4.757971	2.376794
-81.087668	-11.396105	2.386790
-80.150153	-16.252667	2.396787
-79.311350	-9.707870	2.406784
-79.321080	-9.220183	2.416781
-79.193703	-2.672393	2.426778
-78.318645	-16.269873	2.436774
-77.703022	-12.042448	2.446771
-77.090944	-13.289788	2.456768
-76.154068	-7.251351	2.466765
-76.407597	-8.489681	2.476762
-75.899542	-2.099240	2.486758
-75.384279	-17.797210	2.496755
-74.889269	-17.483720	2.506752
-74.173210	-2.985800	2.516749
-73.237330	-6.264554	2.526746
-73.103782	-3.315402	2.536742
-72.983385	-4.372923	2.546739
-72.407769	-5.555858	2.556736
-71.747125	-11.749404	2.566733
-71.500743	-5.841235	2.576730
-70.518412	-5.760010	2.586726
-70.004729	-10.104184	2.596723
-69.875544	-2.454490	2.606720
-69.555855	-2.304648	2.616717
-68.604410	-1.044399	2.626714
-68.336674	-9.294442	2.636710
-66.969022	-5.499595	2.646707
-66.970579	-3.991660	2.656704
-66.747594	-8.576629	2.666701
-66.610554	-5.804775	2.676698
-65.690615	-11.671830	2.686694
-65.271443	-10.974979	2.696691
-64.793235	-8.455491	2.706688
-63.947483	-2.109696	2.716685
-63.611612	-4.439965	2.726682
-63.452023	-10.618074	2.736678
-62.747564	-10.062905	2.746675
-62.173765	-8.757136	2.756672
-61.788777	-11.144716	2.766669
-60.795355	-7.995690	2.776666
-60.663074	-19.067753	2.786662
-60.418886	-16.193885	2.796659
-59.482522	-10.513443	2.806656
-59.190500	-11.498175	2.816653
-59.143589	-7.470533	2.826650
-58.225602	-12.870918	2.836646
-57.670351	-5.778630	2.846643
-57.178233	-5.152609	2.856640
-56.414402	-3.240018	2.866637
-56.281370	-3.956065	2.876634
-55.811025	-7.356135	2.886630
-54.711045	-7.306995	2.896627
-54.454262	-18.077310	2.906624
-54.546679	-11.667251	2.916621
-54.074074	-4.122813	2.926618
-53.109667	-15.983862	2.936614
-52.829886	-12.445742	2.946611
-51.449482	-2.885251	2.956608
-51.501660	-14.361669	2.966605
-51.032319	-6.963383	2.976602
-51.000206	-13.385059	2.986598
-50.533997	-10.495230	2.996595
-49.906815	-7.347514	3.006592
-48.858402	-10.173082	3.016589
-48.201876	-9.986743	3.026586
-47.998141	-6.751265	3.036582
-47.876673	-14.830640	3.046579
-47.710902	-3.542254	3.056576
-46.922268	-3.078340	3.066573
-45.674198	-10.607685	3.076570
-45.250023	-8.158982	3.086566
-44.825789	-9.309191	3.096563
-44.541443	-15.221055	3.106560
-44.640244	-13.828330	3.116557
-43.642269	-8.484835	3.126554
-43.200570	-16.302217	3.136550
-42.781498	-19.517683	3.146547
-42.010787	-10.692915	3.156544
-41.729131	-12.521205	3.166541
-41.172199	-10.445313	3.176538
-40.144666	-13.788501	3.186534
-40.017194	-14.359210	3.196531
-39.934916	-8.374132	3.206528
-39.154130	-5.538364	3.216525
-38.481522	-6.360474	3.226522
-38.262769	-7.668262	3.236518
-37.865921	-16.770589	3.246515
-37.346729	-19.414061	3.256512
-36.711083	-8.905369	3.266509
-35.943160	-11.453432	3.276506
-35.755433	-8.837434	3.286502
-35.261308	-11.154442	3.296499
-34.266968	-11.708878	3.306496
-33.912298	-9.555799	3.316493
-34.255752	-9.339629	3.326490
-33.073636	-10.315383	3.336486
-32.448596	-10.844350	3.346483
-32.302785	-8.869826	3.356480
-31.428673	-4.065553	3.366477
-30.923465	-2.727404	3.376474
-30.900477	-5.851041	3.386470
-29.852493	-6.570417	3.396467
-29.381593	-11.335835	3.406464
-29.474341	-7.318599	3.416461
-28.521296	-7.813955	3.426458
-27.758961	-5.030947	3.436454
-27.428964	-8.246512	3.446451
-27.564303	-10.880007	3.456448
-26.748099	-1.928899	3.466445
-26.320096	-11.911286	3.476442
-25.276581	-12.198346	3.486438
-24.808757	-6.219096	3.496435
-24.615924	-3.020438	3.506432
-24.403953	-3.919533	3.516429
-23.331429	-8.559845	3.526426
-23.061893	-2.191223	3.536422
-22.769473	-3.042369	3.546419
-21.736573	-2.854709	3.556416
-21.567341	-5.706960	3.566413
-21.335510	-8.282003	3.576410
-20.492564	-13.946768	3.586406
-19.730741	2.755819	3.596403
-19.752066	-5.047777	3.606400
-19.340821	-9.722632	3.616397
-18.354293	-5.319515	3.626394
-18.037130	-13.002719	3.636390
-17.672742	-7.007165	3.646387
-16.641666	-11.668977	3.656384
-16.277263	-8.564165	3.666381
-16.387127	-8.630490	3.676378
-16.021256	-9.983630	3.686374
-15.045494	2.780156	3.696371
-14.695108	-6.070608	3.706368
-13.749898	-6.698516	3.716365
-13.317938	-7.621321	3.726362
-13.073609	-9.323226	3.736358
-12.930205	-13.253062	3.746355
-12.127712	-11.191866	3.756352
-11.994506	-2.859560	3.766349
-10.762216	-6.833124	3.776346
-10.125142	-12.061728	3.786342
-10.107563	-9.221035	3.796339
-9.839452	-8.960724	3.806336
-8.722447	-7.430494	3.816333
-8.322245	-11.292923	3.826330
-8.312157	-6.998707	3.836326
-7.547192	-17.955542	3.846323
-6.964804	-16.285103	3.856320
-6.901715	-10.570082	3.866317
-6.551635	-9.036194	3.876314
-5.459052	-12.609620	3.886310
-4.616303	-5.723280	3.896307
-4.330214	4.343460	3.906304
-4.317847	-5.349271	3.916301
-4.254047	10.144220	3.926298
-3.418318	21.291887	3.936294
-2.595640	28.914915	3.946291
-2.357012	37.790311	3.956288
-1.987225	56.727391	3.966285
-1.948656	68.312163	3.976282
-0.954148	90.790805	3.986278
-0.590703	104.018597	3.996275
0.000000	135.584366	4.001280
0.152993	139.295868	4.006285
-0.058819	146.373821	4.011290
0.349370	132.327673	4.016294
0.341621	150.976032	4.021299
0.881270	154.882908	4.026304
0.681199	172.547607	4.031309
0.491881	178.064271	4.036314
0.651583	173.524341	4.041318
0.828413	171.091840	4.046323
0.705708	177.392369	4.051328
0.846107	174.998247	4.056333
0.592235	177.569343	4.061338
0.969034	167.722627	4.066342
0.958079	179.111929	4.071347
0.845068	169.767418	4.076352
1.070302	171.794765	4.081357
0.936866	171.715879	4.086362
0.978024	171.422766	4.091366
0.897143	170.150826	4.096371
1.049805	162.567431	4.101376
1.045729	170.231711	4.106381
0.549375	179.266391	4.111386
0.899666	167.814675	4.116390
0.751642	171.345271	4.121395
0.783969	165.303238	4.126400
1.079066	170.520534	4.131405
0.679376	174.981910	4.136410
0.986579	174.292825	4.141414
0.830749	180.404477	4.146419
0.786506	174.316295	4.151424
0.843196	172.490652	4.156429
0.620978	172.696460	4.161434
0.887765	165.647567	4.166438
0.971610	176.882490	4.171443
1.047101	171.758916	4.176448
0.929878	175.174322	4.181453
1.113327	186.306862	4.186458
1.181377	192.459263	4.191462
1.111015	194.697555	4.196467
1.317158	212.578314	4.201472
1.519907	190.644536	4.206477
1.051144	183.699036	4.211482
1.239919	175.284209	4.216486
1.119160	176.722634	4.221491
1.024873	182.051440	4.226496
1.414408	182.243365	4.231501
1.108333	191.212571	4.236506
1.421016	180.946201	4.241510
1.238705	184.454941	4.246515
1.246871	183.772259	4.251520
1.302694	175.927241	4.256525
1.067571	187.713789	4.261530
1.357975	191.753615	4.266534
1.366291	200.409136	4.271539
1.654835	208.862672	4.276544
1.483308	185.509819	4.281549
1.223787	191.218039	4.286554
1.326315	173.507953	4.291558
1.301672	182.679851	4.296563
1.059593	193.208894	4.301568
1.637089	199.718104	4.306573
1.300658	202.707535	4.311578
1.315618	204.167536	4.316582
1.366685	194.600259	4.321587
1.603139	208.005190	4.326592
1.619724	208.915800	4.331597
1.339461	210.021182	4.336602
1.469097	200.978200	4.341606
1.393534	203.444954	4.346611
1.316428	205.061543	4.351616
1.273105	206.827638	4.356621
1.283419	207.354030	4.361626
1.451079	192.989848	4.366630
1.456071	209.871011	4.371635
1.274804	216.898566	4.376640
1.585744	211.505805	4.381645
1.466439	208.508098	4.386650
1.568496	202.352418	4.391654
1.543476	206.037712	4.396659
1.335138	211.676018	4.401664
1.488985	219.196922	4.406669
1.486133	224.048624	4.411674
1.714644	232.591020	4.416678
1.913674	240.205295	4.421683
1.886730	233.095206	4.426688
1.925833	223.800700	4.431693
1.509096	231.129207	4.436698
1.714827	233.692236	4.441702
1.742528	235.615892	4.446707
1.742151	237.355063	4.451712
2.014571	240.268846	4.456717
1.530701	239.311717	4.461722
1.772576	238.763356	4.466726
1.734228	239.049176	4.471731
1.596977	238.690340	4.476736
2.049583	245.673437	4.481741
1.892373	245.584273	4.486746
1.923254	239.181268	4.491750
1.814443	240.371477	4.496755
1.783373	243.657529	4.501760
2.073507	240.137347	4.506765
1.509736	239.399811	4.511770
1.812787	240.859266	4.516774
1.906020	241.058031	4.521779
1.745664	235.851864	4.526784
1.803679	229.468451	4.531789
1.776035	241.275310	4.536794
1.638306	238.134631	4.541798
1.969581	245.613599	4.546803
1.390586	256.145877	4.551808
1.543377	251.556653	4.556813
2.116426	264.168944	4.561818
2.079517	269.288025	4.566822
1.831646	272.011556	4.571827
1.809502	279.628956	4.576832
2.198519	264.346923	4.581837
2.136004	271.276644	4.586842
2.230536	269.827920	4.591846
2.280188	280.898880	4.596851
2.414570	278.375509	4.601856
2.393087	279.572303	4.606861
2.290326	278.928568	4.611866
2.001353	281.112530	4.616870
2.123206	281.631740	4.621875
2.060922	279.283033	4.626880
2.356899	286.359810	4.631885
2.089248	283.021672	4.636890
2.662536	274.232281	4.641894
2.623697	273.984942	4.646899
2.119950	270.300370	4.651904
2.319551	276.094447	4.656909
1.981515	277.368119	4.661914
2.176753	285.945936	4.666918
2.039907	286.887727	4.671923
1.971626	276.727067	4.676928
2.091497	279.292059	4.681933
2.066099	282.593559	4.686938
2.091214	278.231619	4.691942
2.289335	279.252523	4.696947
2.144226	285.380006	4.701952
2.265162	277.084956	4.706957
2.331175	297.483316	4.711962
2.651831	297.141249	4.716966
2.455456	301.868683	4.721971
2.453997	302.697040	4.726976
2.222245	302.995979	4.731981
2.482897	298.233432	4.736986
2.571211	292.175981	4.741990
2.822850	295.966719	4.746995
2.660291	309.720232	4.752000
2.561219	285.950857	4.757005
2.631243	289.749507	4.762010
2.146730	280.836483	4.767014
2.735497	285.261316	4.772019
2.741197	298.836562	4.777024
2.984261	298.723475	4.782029
2.463713	291.796644	4.787034
2.439939	278.927694	4.792038
2.339951	281.734028	4.797043
2.189379	303.471250	4.802048
2.821121	296.669007	4.807053
2.117226	300.665108	4.812058
2.702534	298.214708	4.817062
2.706547	302.550113	4.822067
2.647536	306.401759	4.827072
2.839722	298.241923	4.832077
2.439718	311.143605	4.837082
2.636745	303.938953	4.842086
2.838775	300.951859	4.847091
2.413965	298.189407	4.852096
2.683085	299.088774	4.857101
2.500747	312.839738	4.862106
2.324198	292.629982	4.867110
2.606318	309.543495	4.872115
2.709977	325.512180	4.877120
3.331579	329.612443	4.882125
2.919077	337.852782	4.887130
3.142566	320.526243	4.892134
2.932660	300.797023	4.897139
2.454781	313.397748	4.902144
2.786648	321.895687	4.907149
2.801834	337.998380	4.912154
2.962680	332.366274	4.917158
2.942366	331.153767	4.922163
2.796814	323.283054	4.927168
3.101532	334.974978	4.932173
2.719387	336.119994	4.937178
2.692224	330.936082	4.942182
3.059386	335.061130	4.947187
2.939349	333.171343	4.952192
3.174700	332.308847	4.957197
2.764232	339.061986	4.962202
3.007715	342.775749	4.967206
2.960768	342.378803	4.972211
2.995651	342.985492	4.977216
2.759472	330.223422	4.982221
2.964929	336.391946	4.987226
2.530305	339.252506	4.992230
2.698003	349.065068	4.997235
3.094915	357.535802	5.002240
3.601336	350.583174	5.007245
3.246195	362.146004	5.012250
3.419333	373.920869	5.017254
3.270628	359.986277	5.022259
3.201977	374.299107	5.027264
3.530038	357.319983	5.032269
3.141021	350.063677	5.037274
3.194445	350.636422	5.042278
3.522486	351.862182	5.047283
3.219716	341.786599	5.052288
3.417843	332.598541	5.057293
3.336659	342.942654	5.062298
3.467685	339.768492	5.067302
3.345396	331.085828	5.072307
2.892771	332.204410	5.077312
3.257644	340.116898	5.082317
3.718076	362.031543	5.087322
3.239728	353.018800	5.092326
3.546505	340.866673	5.097331
3.469257	340.465264	5.102336
3.759763	332.878342	5.107341
2.985210	337.430816	5.112346
3.168838	341.600796	5.117350
3.621744	344.628616	5.122355
3.201041	357.321447	5.127360
3.409422	353.959085	5.132365
3.653588	371.307507	5.137370
3.643758	365.369935	5.142374
3.659279	363.109778	5.147379
3.374313	367.827800	5.152384
3.839436	365.737225	5.157389
3.590696	358.612922	5.162394
3.461147	347.539991	5.167398
3.789404	348.118818	5.172403
3.328710	354.126126	5.177408
3.500122	348.747100	5.182413
3.450995	362.494642	5.187418
3.627571	372.248136	5.192422
3.734288	360.308810	5.197427
3.635096	369.242746	5.202432
3.884339	365.507018	5.207437
3.657139	369.109839	5.212442
3.931956	369.671255	5.217446
3.726430	347.767825	5.222451
3.207174	361.518373	5.227456
3.490952	355.834966	5.232461
3.641094	366.104068	5.237466
3.620693	370.442440	5.242470
3.820044	372.153356	5.247475
3.708094	369.169794	5.252480
3.661931	358.018948	5.257485
3.628626	372.344977	5.262490
3.478318	365.621430	5.267494
3.941995	366.040646	5.272499
3.496088	372.600564	5.277504
4.171345	368.427033	5.282509
3.568826	364.210817	5.287514
3.341219	370.024423	5.292518
3.755091	371.932622	5.297523
3.870850	393.801865	5.302528
4.135890	391.639971	5.307533
3.878406	386.923460	5.312538
3.921238	381.225205	5.317542
4.210833	392.557598	5.322547
3.638938	394.233085	5.327552
4.098152	388.659781	5.332557
3.924395	390.364086	5.337562
3.778495	390.672812	5.342566
3.626113	399.526271	5.347571
3.516561	402.794052	5.352576
4.102843	403.338429	5.357581
3.923567	392.359418	5.362586
3.899116	406.342758	5.367590
3.905961	399.052581	5.372595
4.147206	409.669421	5.377600
4.379983	398.679927	5.382605
4.214615	399.787348	5.387610
4.024220	396.727064	5.392614
4.292769	395.307779	5.397619
4.134648	398.509690	5.402624
3.909672	399.380022	5.407629
4.350746	402.799507	5.412634
4.343279	395.833025	5.417638
4.388842	398.752166	5.422643
3.767104	402.290262	5.427648
3.745918	390.281875	5.432653
3.923430	397.981671	5.437658
3.958089	403.391553	5.442662
4.228917	413.186818	5.447667
4.107397	420.238431	5.452672
4.363649	418.956831	5.457677
4.582418	421.222158	5.462682
4.225187	435.310340	5.467686
4.418514	432.121226	5.472691
4.392005	434.554851	5.477696
4.424712	426.661336	5.482701
4.358570	418.997360	5.487706
4.181509	422.198953	5.492710
4.552353	422.982268	5.497715
4.154564	435.389609	5.502720
4.207558	433.107859	5.507725
4.578257	430.285249	5.512730
4.473204	421.951500	5.517734
4.676345	423.023972	5.522739
4.273187	438.145296	5.527744
4.242518	428.389330	5.532749
4.437770	431.529990	5.537754
4.162815	430.324828	5.542758
4.432790	426.108352	5.547763
4.244910	436.454966	5.552768
4.322187	430.221996	5.557773
4.330082	436.327608	5.562778
4.133627	431.288746	5.567782
4.225900	435.177974	5.572787
4.199440	437.855670	5.577792
4.827923	448.755919	5.582797
5.022363	457.912002	5.587802
4.794420	454.027900	5.592806
4.927017	439.864428	5.597811
4.514756	442.313064	5.602816
4.259218	428.907309	5.607821
4.767008	443.161152	5.612826
4.687578	464.877965	5.617830
4.835627	458.549527	5.622835
4.596675	460.506523	5.627840
4.740514	455.136457	5.632845
4.774886	457.157006	5.637850
4.420056	464.418269	5.642854
4.538290	464.363695	5.647859
4.769319	472.604408	5.652864
4.839311	471.670671	5.657869
4.783650	474.591558	5.662874
4.742508	467.948979	5.667878
4.887347	469.035035	5.672883
4.982533	475.844470	5.677888
4.889938	470.955360	5.682893
5.233766	466.439080	5.687898
4.954123	468.190489	5.692902
5.112757	463.362371	5.697907
5.051972	471.176169	5.702912
4.659431	454.586838	5.707917
4.876816	471.064503	5.712922
5.094008	469.661690	5.717926
5.162559	466.446721	5.722931
4.981899	454.055010	5.727936
4.967089	458.851836	5.732941
4.972946	446.044344	5.737946
4.846831	458.781019	5.742950
5.016694	455.752052	5.747955
5.209333	464.766073	5.752960
5.095176	460.341757	5.757965
5.128460	453.806755	5.762970
4.923351	452.632175	5.767974
4.836510	457.836523	5.772979
4.838328	460.714365	5.777984
4.636380	461.447410	5.782989
4.987618	459.414120	5.787994
4.565809	465.169385	5.792998
4.975344	459.304838	5.798003
5.127978	465.799132	5.803008
5.218708	474.895805	5.808013
4.833615	470.297337	5.813018
5.128050	471.428818	5.818022
4.913652	462.008540	5.823027
5.187469	475.567259	5.828032
5.081172	496.220876	5.833037
5.148467	506.068876	5.838042
5.154007	501.395585	5.843046
5.226849	502.519982	5.848051
5.094300	508.107000	5.853056
5.551074	498.267576	5.858061
5.340679	502.550268	5.863066
5.084563	507.871892	5.868070
5.335561	495.742773	5.873075
4.980149	499.738754	5.878080
5.221439	501.361361	5.883085
5.291957	499.949733	5.888090
4.997976	489.627236	5.893094
5.299524	488.590513	5.898099
5.092942	497.619323	5.903104
5.165368	487.257686	5.908109
5.226255	492.786785	5.913114
5.524176	519.884596	5.918118
5.398748	521.058137	5.923123
5.165684	526.209225	5.928128
5.767489	522.375536	5.933133
5.568570	527.763583	5.938138
5.543315	531.166040	5.943142
5.983249	527.074371	5.948147
5.238806	523.932672	5.953152
5.419103	508.920485	5.958157
5.444470	522.033324	5.963162
5.496440	523.535976	5.968166
5.826385	532.405108	5.973171
5.738775	547.064367	5.978176
5.223594	537.731633	5.983181
5.407473	531.959993	5.988186
5.430751	532.613398	5.993190
5.799684	527.049933	5.998195
5.582619	529.641444	6.003200
5.663623	523.821299	6.008205
6.076161	534.773870	6.013210
5.555170	533.285955	6.018214
5.856726	533.513735	6.023219
5.842920	538.383032	6.028224
5.950544	523.476567	6.033229
5.843009	512.525768	6.038234
5.294813	505.706408	6.043238
5.512239	501.717025	6.048243
5.546572	527.390766	6.053248
5.426108	535.392142	6.058253
5.999923	529.010187	6.063258
5.842333	524.707276	6.068262
5.880509	510.761099	6.073267
5.416663	511.331526	6.078272
5.586800	509.800534	6.083277
5.779826	509.620735	6.088282
5.362749	504.694964	6.093286
5.637466	511.470701	6.098291
5.608587	531.525147	6.103296
5.904205	530.547314	6.108301
5.554804	511.724363	6.113306
5.672082	520.135241	6.118310
6.027733	520.347669	6.123315
5.529897	510.242549	6.128320
5.438356	500.885606	6.133325
5.752166	508.693459	6.138330
5.588699	511.063007	6.143334
5.895052	505.300341	6.148339
5.434610	500.713526	6.153344
5.622691	492.720801	6.158349
5.843509	499.534642	6.163354
5.505216	504.375567	6.168358
5.557593	496.332949	6.173363
5.439800	517.186502	6.178368
5.745147	522.512032	6.183373
5.978581	527.430741	6.188378
5.702847	523.255978	6.193382
5.606420	504.403367	6.198387
5.521571	501.805395	6.203392
5.832877	502.566489	6.208397
5.656687	496.155765	6.213402
5.670886	507.696935	6.218406
6.082900	491.702904	6.223411
5.872773	502.274727	6.228416
5.797804	491.083754	6.233421
6.142288	492.592917	6.238426
5.629240	494.055848	6.243430
5.712676	487.420791	6.248435
5.628417	494.771431	6.253440
5.677871	490.838618	6.258445
5.595400	492.291660	6.263450
5.679592	498.540470	6.268454
5.614020	499.258774	6.273459
5.777115	501.701723	6.278464
5.537332	505.871080	6.283469
5.787742	494.314771	6.288474
5.456075	501.870271	6.293478
5.958879	496.263482	6.298483
5.635965	500.441840	6.303488
5.881762	502.570017	6.308493
5.827615	503.516110	6.313498
5.687130	504.225680	6.318502
5.624956	495.013257	6.323507
5.699021	501.939059	6.328512
5.707663	501.173411	6.333517
5.551457	503.384004	6.338522
5.325374	502.740315	6.343526
5.326866	491.125893	6.348531
5.543776	497.482900	6.353536
4.896352	508.048362	6.358541
5.052047	510.543147	6.363546
5.235620	513.206077	6.368550
5.594823	523.340400	6.373555
5.720337	533.621379	6.378560
5.622264	544.363940	6.383565
5.672194	540.986780	6.388570
5.807984	546.219679	6.393574
5.963320	538.098658	6.398579
5.589162	524.262638	6.403584
5.761733	522.870154	6.408589
5.639671	523.726050	6.413594
5.483935	526.181241	6.418598
5.841639	525.515071	6.423603
5.609440	522.020962	6.428608
5.883332	510.596318	6.433613
5.749972	513.585301	6.438618
5.429561	509.506520	6.443622
5.539306	503.504343	6.448627
5.494929	513.878893	6.453632
5.730480	530.255949	6.458637
6.186393	528.419243	6.463642
5.669166	521.547107	6.468646
5.731406	497.923399	6.473651
5.585737	499.792470	6.478656
5.544948	504.093307	6.483661
5.663528	506.386155	6.488666
5.465069	513.627815	6.493670
5.299956	504.463178	6.498675
5.273260	517.384143	6.503680
5.578333	514.195686	6.508685
6.122414	529.589925	6.513690
5.621227	542.415584	6.518694
5.721024	536.818947	6.523699
5.797062	547.131691	6.528704
5.849391	530.234841	6.533709
5.820804	508.713940	6.538714
5.446171	510.264693	6.543718
5.715145	504.698318	6.548723
5.651969	513.902334	6.553728
5.459218	508.669562	6.558733
5.842700	506.571052	6.563738
5.633742	507.401054	6.568742
5.399226	495.938792	6.573747
5.844008	520.530681	6.578752
5.731053	522.574401	6.583757
5.856653	514.869318	6.588762
5.366204	508.557089	6.593766
5.570015	497.775646	6.598771
5.074974	512.132924	6.603776
5.585437	521.385104	6.608781
5.803897	530.816563	6.613786
5.905340	536.116698	6.618790
6.058646	526.608977	6.623795
6.050859	511.835151	6.628800
5.717730	503.430426	6.633805
5.637191	503.231904	6.638810
5.605171	502.536906	6.643814
5.793256	506.016770	6.648819
5.604204	500.917959	6.653824
5.647267	499.335355	6.658829
5.750722	503.819833	6.663834
5.401340	508.563243	6.668838
5.635430	495.905346	6.673843
5.456914	499.397054	6.678848
5.561556	504.950793	6.683853
5.655585	501.396759	6.688858
5.528872	500.691463	6.693862
5.720861	497.299222	6.698867
5.640357	505.975512	6.703872
5.606795	503.789350	6.708877
5.472634	507.354333	6.713882
5.512650	523.141850	6.718886
5.710114	524.527620	6.723891
5.588125	537.708530	6.728896
5.752314	534.987708	6.733901
5.674574	532.778455	6.738906
5.487838	536.926327	6.743910
5.843897	530.462952	6.748915
5.888229	536.841491	6.753920
5.722923	525.737245	6.758925
5.863916	514.477911	6.763930
5.424067	508.342600	6.768934
5.428943	495.747740	6.773939
5.463917	512.160191	6.778944
5.877770	533.554857	6.783949
5.788712	532.232147	6.788954
5.689267	531.662537	6.793958
5.770485	513.083045	6.798963
5.766762	508.732316	6.803968
5.653365	508.258048	6.808973
5.966747	509.381567	6.813978
5.989272	501.610750	6.818982
5.712847	499.440057	6.823987
5.744223	502.174013	6.828992
6.040769	505.210045	6.833997
5.867734	490.193223	6.839002
5.538994	505.430472	6.844006
5.961160	498.286394	6.849011
5.761383	507.525312	6.854016
5.688127	505.538093	6.859021
5.740261	503.283901	6.864026
5.672824	509.379399	6.869030
5.876874	508.438996	6.874035
6.228240	498.564702	6.879040
5.432863	484.271687	6.884045
5.815867	470.459959	6.889050
5.535887	480.054361	6.894054
5.671713	470.884311	6.899059
5.442452	485.257724	6.904064
5.555620	487.460698	6.909069
5.762245	492.184043	6.914074
5.732512	509.068510	6.919078
5.736090	496.525364	6.924083
5.668823	476.535961	6.929088
5.616721	475.976288	6.934093
5.515321	472.948834	6.939098
5.471776	487.802314	6.944102
5.917637	485.251212	6.949107
5.704149	483.060453	6.954112
5.369148	479.087782	6.959117
5.929044	498.895814	6.964122
5.422012	489.013420	6.969126
5.878475	488.255458	6.974131
5.511181	475.817322	6.979136
5.728560	487.203057	6.984141
5.786262	489.905726	6.989146
5.505163	491.310298	6.994150
5.638228	483.453346	6.999155
5.411001	486.456159	7.004160
5.789928	494.128440	7.009165
5.588032	502.750894	7.014170
5.277605	507.141772	7.019174
5.666912	500.042192	7.024179
5.516027	507.581927	7.029184
5.430034	499.065822	7.034189
5.779692	494.328760	7.039194
5.774731	500.782221	7.044198
5.816190	491.427378	7.049203
5.323289	497.439373	7.054208
5.465560	508.795113	7.059213
5.888363	501.962590	7.064218
5.728410	506.024042	7.069222
6.004420	503.826678	7.074227
6.036189	503.412674	7.079232
5.783350	493.883792	7.084237
6.030659	472.358785	7.089242
5.504902	479.367520	7.094246
5.780723	463.107547	7.099251
5.886047	473.051057	7.104256
5.448596	470.934998	7.109261
5.879892	459.524336	7.114266
5.270430	469.006151	7.119270
5.207673	466.735039	7.124275
5.061445	488.265509	7.129280
5.149529	487.341509	7.134285
5.781840	484.794916	7.139290
5.563503	497.922356	7.144294
5.741296	496.589982	7.149299
5.879500	490.831726	7.154304
5.574566	501.246761	7.159309
5.742003	499.661263	7.164314
5.682257	502.394886	7.169318
5.614263	512.521167	7.174323
5.918879	503.331295	7.179328
5.589531	499.721635	7.184333
5.627277	501.411126	7.189338
5.479442	504.968996	7.194342
5.675848	495.203481	7.199347
5.766457	503.207451	7.204352
5.792889	509.606103	7.209357
5.879804	501.524723	7.214362
5.415658	500.956287	7.219366
5.635448	496.255286	7.224371
5.627207	494.923663	7.229376
5.558255	500.126154	7.234381
5.625999	502.918425	7.239386
5.412395	502.177962	7.244390
5.799752	504.411593	7.249395
5.866213	499.900986	7.254400
5.514480	506.293168	7.259405
5.650240	500.729472	7.264410
5.619101	499.656566	7.269414
5.840557	497.851506	7.274419
5.648915	506.562145	7.279424
5.573043	502.161384	7.284429
5.663274	491.607279	7.289434
5.452068	500.626989	7.294438
5.861487	496.535635	7.299443
5.815920	505.843090	7.304448
5.607841	501.514591	7.309453
5.905221	498.504698	7.314458
5.520141	505.681298	7.319462
5.583554	507.701593	7.324467
5.712567	505.028421	7.329472
5.461254	505.622821	7.334477
5.620196	499.054504	7.339482
5.489734	509.767272	7.344486
5.897832	503.851446	7.349491
5.524622	503.246671	7.354496
5.285759	507.936694	7.359501
5.562235	501.843330	7.364506
5.572400	507.060275	7.369510
5.435264	505.566644	7.374515
5.416588	493.900403	7.379520
5.450262	503.036514	7.384525
5.485762	501.114590	7.389530
5.276332	505.848782	7.394534
5.576105	498.893537	7.399539
5.655257	508.952484	7.404544
5.899314	519.775625	7.409549
5.788440	496.028496	7.414554
5.591126	503.129373	7.419558
5.705373	503.059475	7.424563
5.669455	509.226915	7.429568
5.660002	504.949155	7.434573
5.826198	506.200687	7.439578
5.548949	502.728530	7.444582
6.012761	491.474369	7.449587
5.737079	500.932221	7.454592
5.703868	515.433387	7.459597
5.647128	508.510119	7.464602
5.815314	510.891357	7.469606
5.702327	502.462091	7.474611
5.710631	502.846363	7.479616
5.736378	511.239016	7.484621
6.010233	508.480246	7.489626
5.924789	509.017047	7.494630
5.780381	496.540384	7.499635
5.775536	502.180191	7.504640
5.623823	499.814856	7.509645
5.837998	486.403351	7.514650
5.713479	499.910317	7.519654
5.310901	503.945861	7.524659
5.420656	507.492537	7.529664
5.495831	499.663396	7.534669
5.709419	497.344047	7.539674
5.437764	497.832397	7.544678
5.701785	503.595690	7.549683
5.720550	501.522033	7.554688
5.735373	507.972228	7.559693
5.789796	497.467644	7.564698
5.510260	499.692994	7.569702
5.599893	494.508273	7.574707
5.899682	505.385927	7.579712
5.563757	508.870599	7.584717
5.787430	498.287236	7.589722
5.601858	502.264326	7.594726
5.585485	494.442521	7.599731
5.637257	497.201124	7.604736
5.696347	500.988512	7.609741
5.870359	497.732924	7.614746
5.563690	505.674784	7.619750
5.653245	503.159969	7.624755
5.847010	504.730445	7.629760
5.698007	496.026353	7.634765
6.085990	490.935286	7.639770
5.577360	509.937867	7.644774
5.806271	495.242739	7.649779
5.981118	482.749635	7.654784
5.437541	479.772956	7.659789
5.702139	470.313769	7.664794
5.235389	477.835739	7.669798
5.776588	487.710582	7.674803
5.980487	489.230349	7.679808
5.508331	482.942534	7.684813
5.301869	473.295602	7.689818
5.377218	497.086429	7.694822
5.770671	499.648769	7.699827
6.010213	495.312500	7.704832
5.549131	493.927258	7.709837
5.734425	486.649085	7.714842
5.699592	500.420730	7.719846
5.751958	496.857797	7.724851
5.808138	487.199715	7.729856
5.272429	485.693519	7.734861
5.480497	488.230159	7.739866
5.063365	500.288341	7.744870
5.584567	491.993623	7.749875
5.520511	496.154163	7.754880
5.373299	499.087421	7.759885
5.553427	508.563481	7.764890
5.512252	510.261082	7.769894
5.530453	505.216123	7.774899
5.750358	496.833664	7.779904
5.225749	504.654573	7.784909
5.609873	500.625804	7.789914
5.408827	502.541518	7.794918
5.429639	500.872910	7.799923
5.832089	505.428144	7.804928
5.357231	513.755735	7.809933
5.936860	524.391420	7.814938
5.555813	529.601988	7.819942
5.381356	523.434752	7.824947
5.664104	531.434904	7.829952
5.646273	545.272051	7.834957
5.773809	545.474130	7.839962
5.910196	544.381922	7.844966
5.742310	522.838835	7.849971
5.751309	512.923043	7.854976
5.401760	515.050059	7.859981
5.443524	502.999118	7.864986
5.515697	531.604364	7.869990
5.853297	527.599851	7.874995
5.605888	545.555358	7.880000
5.277176	553.099245	7.885005
5.787866	543.515584	7.890010
5.460630	546.589691	7.895014
5.860888	543.624252	7.900019
6.014259	536.249220	7.905024
5.630790	546.404768	7.910029
5.924313	540.629508	7.915034
5.624863	527.111942	7.920038
5.463152	513.111384	7.925043
5.471610	510.711883	7.930048
5.444803	530.815709	7.935053
5.886142	541.493792	7.940058
5.703056	541.067642	7.945062
5.766153	543.246833	7.950067
5.900471	532.855108	7.955072
5.378775	519.681597	7.960077
5.648787	523.063672	7.965082
5.549181	536.449544	7.970086
5.563163	538.115145	7.975091
5.904695	536.124787	7.980096
5.812974	535.330833	7.985101
5.429242	525.477960	7.990106
5.621382	525.364606	7.995110
5.586240	529.718483	8.000115
5.723089	522.494823	8.005133
5.697009	524.374264	8.010150
5.883643	524.545932	8.015168
5.320552	523.664844	8.020186
5.792857	534.987517	8.025203
5.788843	529.513496	8.030221
5.358601	539.161548	8.035238
5.641600	531.354988	8.040256
5.765096	533.049997	8.045274
5.791738	546.007652	8.050291
6.009806	537.989714	8.055309
5.472139	538.659844	8.060326
5.729370	533.957065	8.065344
5.767623	540.136791	8.070362
5.655281	543.272976	8.075379
6.197664	533.970964	8.080397
5.448624	523.184755	8.085414
5.433732	522.107484	8.090432
5.593665	533.473905	8.095450
5.629226	537.052686	8.100467
6.046789	536.860170	8.105485
5.698985	542.775507	8.110502
5.929593	542.472671	8.115520
6.192978	544.350235	8.120538
6.063316	537.789109	8.125555
6.213080	517.811857	8.130573
5.463149	523.642782	8.135590
5.571954	522.789512	8.140608
5.519879	514.121968	8.145626
5.783978	508.873086	8.150643
5.693137	518.551340	8.155661
5.532699	543.355425	8.160678
5.767304	536.042498	8.165696
5.907716	543.911030	8.170714
5.834749	539.228768	8.175731
5.862767	534.199369	8.180749
5.802910	549.090157	8.185766
5.921157	546.335086	8.190784
5.836938	547.887290	8.195802
6.035569	552.463053	8.200819
6.219971	546.794435	8.205837
6.051385	534.329024	8.210854
5.806196	522.161466	8.215872
5.924959	517.351382	8.220890
5.325281	511.796211	8.225907
5.503914	523.452688	8.230925
6.042983	547.478709	8.235942
6.245658	548.152652	8.240960
5.956459	547.009116	8.245978
6.110408	546.453250	8.250995
5.933713	522.421743	8.256013
5.917473	530.064234	8.261030
5.664507	517.912135	8.266048
5.961916	534.708070	8.271066
5.842578	545.899334	8.276083
6.424407	542.985386	8.281101
5.649207	540.667082	8.286118
5.847159	543.725715	8.291136
5.549895	542.082424	8.296154
5.481031	542.314421	8.301171
5.907425	540.191471	8.306189
5.943827	550.445261	8.311206
5.731939	553.339088	8.316224
5.924348	550.166914	8.321242
5.825524	553.176087	8.326259
5.956891	542.310109	8.331277
5.921690	555.463488	8.336294
5.372804	548.326479	8.341312
5.599331	549.753329	8.346330
5.733326	562.256625	8.351347
6.110650	569.919613	8.356365
5.775176	574.327196	8.361382
6.089612	584.088096	8.366400
5.866898	575.714908	8.371418
5.842855	580.868126	8.376435
5.742892	574.471928	8.381453
5.727085	581.459079	8.386470
5.837696	581.684838	8.391488
6.098569	578.462080	8.396506
5.845588	586.370944	8.401523
6.411162	575.008659	8.406541
6.166915	578.269878	8.411558
6.096846	587.324482	8.416576
6.402471	579.585996	8.421594
5.828211	583.222363	8.426611
5.964328	576.289406	8.431629
6.059907	584.344666	8.436646
6.073379	583.543755	8.441664
6.108506	585.871568	8.446682
5.893540	577.208963	8.451699
6.197414	574.031058	8.456717
6.337366	579.734923	8.461734
6.241140	594.710295	8.466752
6.443827	588.370553	8.471770
6.089915	589.226617	8.476787
6.090432	577.522847	8.481805
5.841576	579.816304	8.486822
5.680496	583.648123	8.491840
6.320890	583.594932	8.496858
6.134616	589.978483	8.501875
6.446231	579.843675	8.506893
6.047603	583.571567	8.511910
6.146336	585.575147	8.516928
6.219201	587.654741	8.521946
6.066460	600.795305	8.526963
6.088784	585.628709	8.531981
6.103791	588.227318	8.536998
5.921579	590.047250	8.542016
6.107170	599.750727	8.547034
6.278569	616.645415	8.552051
6.742356	614.798312	8.557069
6.406873	593.137690	8.562087
6.584969	593.207835	8.567104
6.538252	580.239265	8.572122
6.316007	599.777453	8.577139
6.322868	583.231480	8.582157
6.026568	582.987278	8.587175
6.451343	586.182224	8.592192
6.402540	579.553889	8.597210
6.199911	586.546231	8.602227
6.670332	587.686959	8.607245
6.284568	589.096810	8.612263
6.292823	581.252966	8.617280
6.501398	581.576590	8.622298
6.354709	592.863139	8.627315
6.087943	583.808769	8.632333
6.107450	586.904280	8.637351
6.229125	586.906204	8.642368
6.180071	579.385750	8.647386
6.246671	585.869021	8.652403
6.446894	585.489430	8.657421
6.399276	588.514651	8.662439
6.307296	587.197208	8.667456
6.259225	588.046719	8.672474
5.974763	592.765505	8.677491
6.493767	588.991911	8.682509
6.465571	585.807966	8.687527
6.095093	587.275418	8.692544
6.503909	588.571281	8.697562
6.296576	601.736514	8.702579
6.524649	596.688795	8.707597
6.529668	591.838343	8.712615
6.249936	591.616989	8.717632
6.348078	598.650758	8.722650
6.448506	598.405058	8.727667
6.290444	614.200953	8.732685
6.498832	616.715553	8.737703
6.494088	625.705949	8.742720
6.845089	613.462428	8.747738
6.191548	602.685967	8.752755
6.507179	593.145556	8.757773
6.615269	587.970647	8.762791
6.373932	600.814590	8.767808
6.514449	592.623056	8.772826
6.309796	595.366411	8.777843
6.646810	614.811313	8.782861
6.751035	596.090177	8.787879
6.544591	593.595409	8.792896
6.992810	590.848782	8.797914
6.627305	585.416470	8.802931
6.293465	585.756024	8.807949
6.594956	582.692467	8.812967
6.681446	596.567762	8.817984
6.570989	579.990796	8.823002
6.640715	591.277893	8.828019
6.359978	575.085797	8.833037
6.483960	574.136727	8.838055
6.528171	583.692328	8.843072
6.543452	583.330900	8.848090
6.579500	588.715879	8.853107
6.367308	585.389340	8.858125
6.646091	588.427146	8.863143
6.512027	598.076969	8.868160
6.495700	587.722187	8.873178
6.468620	589.526224	8.878195
6.821582	592.440080	8.883213
6.635226	585.271780	8.888231
6.795615	589.271007	8.893248
6.589969	584.294966	8.898266
6.465357	587.892160	8.903283
6.557444	579.930643	8.908301
6.721604	585.530528	8.913319
6.555138	597.203841	8.918336
6.847386	592.880031	8.923354
6.734550	590.720716	8.928371
6.352992	589.255591	8.933389
6.848330	598.760466	8.938407
6.560681	600.992141	8.943424
6.762978	602.240947	8.948442
6.841630	620.358720	8.953459
6.681987	609.291126	8.958477
6.685818	590.338600	8.963495
6.665785	601.820525	8.968512
6.763243	601.940801	8.973530
6.716713	604.271876	8.978547
6.523620	606.037811	8.983565
6.974280	612.631905	8.988583
6.645680	626.022674	8.993600
6.803800	622.646740	8.998618
6.882007	618.222295	9.003635
6.496097	614.128538	9.008653
6.631075	601.290033	9.013671
6.722872	618.573794	9.018688
6.731978	620.253471	9.023706
6.301105	629.264298	9.028723
6.844675	624.847381	9.033741
6.738656	619.355742	9.038759
6.592199	624.884455	9.043776
6.696918	614.637384	9.048794
6.849914	626.977483	9.053811
6.608582	624.866164	9.058829
6.619079	622.212139	9.063847
6.754162	625.434693	9.068864
6.771456	608.347204	9.073882
6.697176	619.648672	9.078899
6.602727	618.572044	9.083917
6.826774	615.489296	9.088935
6.246155	624.305516	9.093952
6.850641	630.955482	9.098970
7.242558	638.775415	9.103987
6.991756	649.102909	9.109005
7.029189	640.621647	9.114023
6.809849	635.084568	9.119040
6.947019	634.828072	9.124058
6.850841	623.966967	9.129075
6.831033	636.061467	9.134093
7.035626	647.507781	9.139111
6.835313	644.628497	9.144128
6.835597	656.495323	9.149146
6.855849	647.967103	9.154163
6.749940	651.531796	9.159181
7.105459	646.756255	9.164199
6.800147	659.210989	9.169216
6.949239	668.560073	9.174234
7.033966	653.301813	9.179251
7.065133	646.363928	9.184269
7.430614	653.211640	9.189287
6.840295	656.047179	9.194304
6.937545	650.121910	9.199322
6.947985	650.417463	9.204339
7.118689	649.601587	9.209357
7.118786	644.895508	9.214375
7.030167	650.887324	9.219392
6.877484	649.945098	9.224410
7.042128	648.770838	9.229427
6.674863	649.502265	9.234445
7.308142	642.425419	9.239463
7.136183	655.423169	9.244480
7.002536	656.171984	9.249498
7.377418	645.276122	9.254515
6.990692	646.869077	9.259533
7.386275	644.999487	9.264551
7.174385	658.389104	9.269568
7.023510	649.937186	9.274586
7.099466	639.699378	9.279603
7.318949	654.348078	9.284621
7.193608	626.608580	9.289639
6.915290	636.646472	9.294656
6.845457	644.707154	9.299674
7.069531	648.581817	9.304691
7.188291	657.135754	9.309709
7.156542	649.476308	9.314727
6.892529	645.153578	9.319744
7.006282	660.339840	9.324762
7.135270	652.124692	9.329779
6.920768	654.524668	9.334797
7.248345	658.372783	9.339815
7.231723	651.327951	9.344832
7.351245	653.320625	9.349850
7.204861	656.510679	9.354867
7.131635	649.357802	9.359885
7.098697	643.498825	9.364903
7.137567	645.562395	9.369920
7.094915	645.198041	9.374938
7.173295	651.325322	9.379955
7.436393	650.777985	9.384973
7.402728	645.384203	9.389991
7.329455	651.977805	9.395008
7.237299	637.885597	9.400026
7.498874	653.321982	9.405043
7.127043	659.698044	9.410061
7.493455	649.232932	9.415079
7.005761	643.193935	9.420096
6.981084	647.717766	9.425114
7.258742	638.467214	9.430131
7.087014	650.797816	9.435149
7.457221	647.621138	9.440167
7.550311	659.130859	9.445184
7.034166	659.942982	9.450202
7.255861	658.200141	9.455219
7.404412	664.552206	9.460237
7.370122	656.289150	9.465255
7.432375	654.728142	9.470272
7.357915	652.625260	9.475290
7.369887	648.373534	9.480307
7.227448	647.812224	9.485325
6.915078	660.146886	9.490343
7.143750	650.694124	9.495360
7.267560	654.777450	9.500378
7.477028	668.697338	9.505395
7.503817	679.524355	9.510413
7.634435	686.333545	9.515431
7.588517	665.792087	9.520448
7.168529	660.533093	9.525466
7.393930	652.538978	9.530483
7.719992	647.551807	9.535501
7.341305	647.140542	9.540519
7.357209	649.016997	9.545536
7.128415	648.898228	9.550554
7.459798	660.975354	9.555571
7.276504	666.021968	9.560589
7.797716	665.587657	9.565607
7.620793	678.473865	9.570624
7.525839	673.390444	9.575642
7.551689	665.921928	9.580659
6.920948	659.078758	9.585677
7.335691	669.207123	9.590695
7.341391	678.910855	9.595712
7.382322	690.255333	9.600730
7.685972	674.382629	9.605747
7.496978	678.205701	9.610765
7.565279	679.884656	9.615783
7.620315	686.714996	9.620800
7.565614	691.885815	9.625818
8.028272	677.761422	9.630835
7.519773	686.069094	9.635853
7.898379	681.936759	9.640871
7.720072	685.787097	9.645888
7.682699	688.874610	9.650906
7.517521	683.328366	9.655923
7.483571	685.998850	9.660941
7.632549	674.531352	9.665959
7.914105	674.641379	9.670976
7.573892	680.180973	9.675994
7.742658	684.210921	9.681011
7.396864	681.669396	9.686029
7.603163	679.082199	9.691047
7.537056	683.723498	9.696064
7.439085	688.301473	9.701082
7.617169	686.800342	9.706099
7.546779	682.664660	9.711117
7.395837	680.675773	9.716135
7.690855	685.196481	9.721152
7.215022	689.173237	9.726170
7.525345	685.452115	9.731187
7.880885	680.965288	9.736205
7.807057	677.586342	9.741223
7.844019	677.134435	9.746240
7.261622	691.819343	9.751258
7.533961	684.584446	9.756275
7.769598	693.204507	9.761293
7.575394	689.336780	9.766311
7.691400	689.342396	9.771328
7.971834	695.289283	9.776346
7.683243	699.580610	9.781363
7.395922	701.310757	9.786381
7.737546	702.324675	9.791399
7.990117	705.324422	9.796416
7.894580	709.076653	9.801434
7.725694	701.514929	9.806451
7.932633	705.910656	9.811469
7.666969	704.723855	9.816487
8.138533	710.182648	9.821504
7.850463	702.552445	9.826522
7.905626	704.420057	9.831539
8.056592	715.701692	9.836557
8.165792	705.983355	9.841575
7.677605	691.464995	9.846592
7.960851	681.700000	9.851610
7.705050	674.157574	9.856627
7.894440	683.515064	9.861645
7.594208	709.578324	9.866663
8.229197	709.139184	9.871680
8.244748	711.231415	9.876698
8.235425	695.037050	9.881715
8.239794	684.811043	9.886733
7.787195	677.118885	9.891751
8.149807	679.410799	9.896768
7.744506	672.568550	9.901786
7.777040	673.101847	9.906803
7.876741	674.593951	9.911821
7.862633	677.098487	9.916839
7.825826	679.327690	9.921856
8.065485	702.209842	9.926874
8.043340	700.034343	9.931891
8.126663	695.810767	9.936909
7.973234	693.135500	9.941927
8.042591	677.949035	9.946944
7.816175	681.859380	9.951962
7.986700	694.356549	9.956979
8.091952	707.794570	9.961997
8.257335	706.773405	9.967015
8.274534	704.778674	9.972032
7.919553	701.842374	9.977050
8.166530	685.011675	9.982067
8.124538	682.375858	9.987085
8.137954	690.565400	9.992103
8.163466	681.064415	9.997120
7.805366	693.667442	10.002138
8.151800	706.476928	10.007155
8.228769	706.474333	10.012173
8.167785	702.398892	10.017191
8.472147	686.085584	10.022208
7.876413	679.627299	10.027226
7.850659	691.189060	10.032243
8.056026	709.099318	10.037261
8.190143	711.560766	10.042279
8.543188	706.085245	10.047296
8.452660	704.155454	10.052314
8.110192	691.482471	10.057331
8.282963	676.087515	10.062349
8.110602	679.834426	10.067367
8.083259	674.085026	10.072384
8.311678	687.916972	10.077402
8.287939	692.292558	10.082419
8.106067	694.864577	10.087437
7.932701	697.907156	10.092455
8.226094	698.848054	10.097472
8.093676	706.319904	10.102490
8.408283	712.649862	10.107507
8.060539	709.561309	10.112525
7.909252	712.863582	10.117543
8.343684	708.748387	10.122560
8.324105	709.365186	10.127578
8.100935	701.040618	10.132595
8.587060	709.247311	10.137613
8.135955	717.100809	10.142631
8.386522	707.553268	10.147648
8.374314	718.945518	10.152666
8.319475	701.426124	10.157683
8.309794	699.449022	10.162701
8.008209	712.612802	10.167719
8.221311	707.034839	10.172736
8.479735	713.889445	10.177754
7.905036	708.319445	10.182771
8.261143	709.972295	10.187789
8.309736	706.209691	10.192807
8.512029	712.238481	10.197824
8.417348	714.375007	10.202842
8.526973	703.693677	10.207859
8.426426	710.583198	10.212877
8.146596	707.006143	10.217895
8.506399	705.603107	10.222912
8.292983	703.809057	10.227930
8.472516	709.020786	10.232947
8.526351	707.811594	10.237965
8.291501	707.642653	10.242983
8.258695	723.211107	10.248000
8.522291	739.086144	10.253018
8.757528	741.634117	10.258035
8.668992	728.734821	10.263053
8.517534	733.249417	10.268071
8.736601	711.638202	10.273088
8.431613	714.054715	10.278106
8.640068	706.613474	10.283123
8.518723	703.986240	10.288141
8.491653	700.050346	10.293159
8.499518	697.568170	10.298176
8.369802	715.892998	10.303194
8.472583	731.166956	10.308211
8.665948	736.094075	10.313229
8.342115	745.437613	10.318247
8.568314	734.009170	10.323264
8.518658	737.895830	10.328282
8.601535	741.663558	10.333299
8.759737	742.300773	10.338317
8.608515	742.959501	10.343335
9.146693	742.589499	10.348352
8.269860	745.392986	10.353370
8.604777	742.260007	10.358387
8.569189	744.868382	10.363405
9.084883	744.215137	10.368423
9.108098	741.374966	10.373440
8.905084	724.455031	10.378458
8.606295	709.210102	10.383475
8.573983	711.942908	10.388493
8.391404	720.675199	10.393511
8.883856	723.432095	10.398528
8.753301	736.030914	10.403546
8.861801	738.823315	10.408563
8.635696	732.719699	10.413581
8.646021	735.414367	10.418599
8.506193	733.123196	10.423616
8.628399	742.181838	10.428634
8.795919	745.238948	10.433651
9.163080	741.914059	10.438669
8.542000	740.143383	10.443687
9.143637	741.580200	10.448704
8.730286	729.757830	10.453722
8.673131	742.462811	10.458739
9.262265	727.542015	10.463757
8.764804	738.201912	10.468775
8.721522	729.887064	10.473792
8.905909	737.284729	10.478810
8.658413	733.695140	10.483827
8.752167	738.792140	10.488845
8.584707	724.616349	10.493863
8.557396	723.907686	10.498880
8.719900	724.387229	10.503898
8.451946	735.891821	10.508915
8.946724	736.714810	10.513933
8.813457	728.614995	10.518951
8.833738	730.538464	10.523968
8.835753	731.194896	10.528986
8.336262	729.349315	10.534003
9.156659	733.600275	10.539021
8.939723	740.638056	10.544039
9.069258	742.727791	10.549056
9.040620	739.894516	10.554074
8.929799	734.680452	10.559091
9.091079	720.476220	10.564109
8.934074	722.899573	10.569127
9.007107	726.634678	10.574144
9.496211	729.376679	10.579162
9.143322	726.129945	10.584179
8.980925	722.727836	10.589197
9.013137	728.838175	10.594215
9.041221	732.932519	10.599232
9.198791	729.757406	10.604250
9.082978	727.016577	10.609267
9.375080	726.737626	10.614285
9.251260	736.128111	10.619303
8.762899	729.185016	10.624320
8.993347	724.360348	10.629338
8.871826	713.093794	10.634355
8.890066	717.473963	10.639373
8.813772	726.099535	10.644391
8.895277	750.392202	10.649408
9.386328	754.637073	10.654426
9.101449	758.071551	10.659443
9.288668	753.546685	10.664461
9.375972	763.964715	10.669479
8.948791	755.920935	10.674496
9.539450	758.091627	10.679514
8.960973	743.291832	10.684531
9.388226	746.241759	10.689549
9.365048	751.356413	10.694567
9.381722	743.796478	10.699584
8.997184	729.028023	10.704602
8.826660	737.622134	10.709619
9.387583	752.724848	10.714637
9.598674	750.196286	10.719655
9.284902	749.063487	10.724672
9.510952	737.546105	10.729690
9.027197	735.071358	10.734707
9.295858	732.460758	10.739725
9.517677	736.893890	10.744743
9.293021	738.452690	10.749760
9.285024	725.336481	10.754778
9.245014	731.147098	10.759795
9.306798	730.934549	10.764813
9.287771	735.483845	10.769831
9.220741	753.608432	10.774848
9.270354	750.210055	10.779866
9.290313	752.620701	10.784883
9.634768	765.253330	10.789901
9.428783	767.464153	10.794919
9.348781	766.123459	10.799936
9.803375	754.366067	10.804954
9.097858	744.399729	10.809971
9.641619	736.844903	10.814989
9.461713	738.026588	10.820007
9.256592	731.932790	10.825024
9.318844	738.644068	10.830042
9.507334	751.275890	10.835059
9.516355	751.813468	10.840077
9.124698	752.918552	10.845095
9.160076	752.959143	10.850112
9.661843	754.963060	10.855130
9.391599	762.937061	10.860147
9.487865	763.594254	10.865165
9.227003	759.580170	10.870183
9.729402	769.533218	10.875200
9.600567	748.674207	10.880218
9.531550	763.766485	10.885235
9.491070	762.337778	10.890253
9.325145	771.278234	10.895271
9.290752	767.940971	10.900288
9.539737	762.702275	10.905306
9.449981	767.553279	10.910323
9.621300	763.582912	10.915341
9.383427	764.494699	10.920359
9.027621	759.940887	10.925376
9.532730	775.327603	10.930394
9.827428	788.608523	10.935411
9.751777	778.449507	10.940429
9.909238	765.581367	10.945447
9.373463	755.731040	10.950464
9.627320	754.241687	10.955482
9.935496	774.454812	10.960499
9.624757	761.728013	10.965517
9.494724	769.083082	10.970535
9.894190	784.239473	10.975552
9.837829	769.979346	10.980570
9.729896	772.790790	10.985587
9.854209	764.665907	10.990605
9.940854	759.226322	10.995623
9.733293	766.369436	11.000640
9.838285	756.348467	11.005658
9.830069	757.240016	11.010675
9.749883	760.312968	11.015693
10.143221	752.633117	11.020711
10.056995	761.357479	11.025728
9.971068	762.951319	11.030746
9.678953	763.670922	11.035763
9.704769	761.978547	11.040781
9.623336	758.353047	11.045799
9.817229	756.119795	11.050816
9.691776	749.539284	11.055834
9.518920	764.528467	11.060851
9.985671	758.840273	11.065869
10.012092	761.638566	11.070887
9.939426	766.039775	11.075904
10.064675	762.220698	11.080922
9.784341	765.444817	11.085939
10.225875	763.617414	11.090957
9.900228	753.441076	11.095975
9.788267	763.628694	11.100992
9.980485	762.662629	11.106010
9.699405	767.972146	11.111027
9.528192	763.933404	11.116045
9.926763	765.815817	11.121063
10.123252	786.049185	11.126080
10.276536	770.921483	11.131098
10.181806	780.127297	11.136115
9.813928	762.058683	11.141133
10.039756	769.324241	11.146151
9.810964	772.060595	11.151168
10.272810	783.029828	11.156186
9.631610	779.612358	11.161203
10.124446	773.841318	11.166221
10.013486	768.835891	11.171239
9.878802	778.150062	11.176256
10.281738	786.778644	11.181274
10.364242	796.836133	11.186291
10.201799	793.502705	11.191309
10.420524	786.406717	11.196327
10.120031	790.277765	11.201344
9.999405	763.660279	11.206362
10.021915	782.561995	11.211379
10.214764	787.637321	11.216397
10.539356	782.978346	11.221415
10.233113	772.025495	11.226432
10.169928	764.286260	11.231450
10.140286	762.973852	11.236467
10.333067	760.200521	11.241485
10.454670	753.637832	11.246503
10.099334	754.412757	11.251520
10.333442	751.678260	11.256538
10.146824	757.939911	11.261555
9.694745	764.718187	11.266573
10.141468	765.840999	11.271591
10.270888	783.690974	11.276608
10.506574	784.291670	11.281626
10.536331	794.121103	11.286643
10.438298	782.570349	11.291661
10.090821	765.075623	11.296679
10.190033	784.487019	11.301696
10.201065	785.474977	11.306714
10.406696	782.952035	11.311731
10.350353	786.791986	11.316749
10.424661	783.507413	11.321767
10.197905	790.153796	11.326784
10.351182	792.211764	11.331802
10.401874	795.129457	11.336819
10.395406	786.375693	11.341837
10.483816	786.213852	11.346855
10.472797	792.943068	11.351872
10.820271	787.329093	11.356890
10.600261	799.019379	11.361907
10.373259	795.861552	11.366925
10.793948	783.635609	11.371943
10.132737	774.596416	11.376960
10.354488	783.589330	11.381978
10.367526	786.309144	11.386995
10.305651	795.349526	11.392013
10.669890	785.007201	11.397031
10.474694	799.811757	11.402048
10.595134	796.284165	11.407066
10.665732	797.984206	11.412083
10.592728	803.531745	11.417101
10.246603	786.532948	11.422119
10.179541	790.393171	11.427136
10.632142	797.561042	11.432154
10.560781	793.304054	11.437171
10.434918	810.560724	11.442189
10.368767	798.093031	11.447207
10.016645	799.404541	11.452224
10.251328	801.524833	11.457242
10.365519	796.649485	11.462259
10.418260	798.371568	11.467277
10.657619	804.538635	11.472295
11.166234	820.028344	11.477312
10.970683	812.789619	11.482330
10.765405	799.931599	11.487347
10.378141	793.103832	11.492365
10.900169	782.544717	11.497383
10.522707	796.168965	11.502400
10.601169	787.543464	11.507418
10.674202	798.276815	11.512435
10.641153	815.166439	11.517453
10.864344	797.488017	11.522471
10.613516	810.391075	11.527488
11.096158	808.620840	11.532506
10.963281	805.334877	11.537523
10.803480	803.086458	11.542541
10.775167	781.949613	11.547559
10.482683	789.904866	11.552576
10.718379	794.943788	11.557594
10.867463	810.034513	11.562611
10.647401	813.854289	11.567629
11.049036	796.467585	11.572647
10.760869	811.558730	11.577664
10.749147	809.810949	11.582682
10.965959	805.931265	11.587699
10.743103	815.255108	11.592717
11.157982	799.749361	11.597735
11.027427	804.394950	11.602752
10.841602	801.819982	11.607770
10.901434	802.339719	11.612787
10.888452	811.405883	11.617805
10.912189	797.915433	11.622823
10.852372	795.886870	11.627840
10.934982	806.421434	11.632858
11.007847	803.096551	11.637875
11.018068	804.679230	11.642893
11.011694	796.736332	11.647911
11.018227	807.404510	11.652928
11.192759	806.520879	11.657946
11.306089	807.086490	11.662963
10.927058	804.638315	11.667981
10.922022	802.938634	11.672999
10.688522	807.397924	11.678016
10.587854	797.612652	11.683034
11.125456	798.125273	11.688051
11.062598	808.018437	11.693069
11.006500	806.080385	11.698087
10.911619	810.107388	11.703104
10.908499	806.140643	11.708122
11.272332	802.776731	11.713139
11.070583	798.883948	11.718157
11.253970	798.260424	11.723175
10.990996	803.803929	11.728192
10.969233	823.948435	11.733210
11.468446	829.513018	11.738227
11.235726	828.019042	11.743245
11.445594	823.849014	11.748263
11.152339	816.749640	11.753280
11.243277	807.668993	11.758298
10.962596	795.196210	11.763315
10.721610	827.537305	11.768333
11.577569	820.544032	11.773351
11.621093	830.825469	11.778368
11.525349	836.795212	11.783386
11.450384	818.279176	11.788403
11.336907	811.678551	11.793421
11.481255	804.368703	11.798439
11.195038	805.689398	11.803456
11.477870	807.693681	11.808474
11.358050	792.574087	11.813491
11.160170	799.358985	11.818509
11.241685	803.602464	11.823527
11.453398	819.853518	11.828544
11.242637	828.024972	11.833562
11.509561	819.147086	11.838579
11.165088	831.446645	11.843597
11.333723	818.507335	11.848615
11.504877	827.512572	11.853632
11.334572	822.413212	11.858650
11.648219	829.570995	11.863667
11.351323	817.174877	11.868685
11.591126	819.809397	11.873703
11.730580	816.416037	11.878720
11.477798	823.689465	11.883738
11.782483	831.068969	11.888755
11.660573	822.933571	11.893773
11.443715	816.805858	11.898791
11.199130	825.337958	11.903808
11.020554	829.272122	11.908826
11.425167	825.187411	11.913843
11.308511	825.312172	11.918861
11.595789	821.533025	11.923879
11.363008	822.357964	11.928896
11.406152	833.214566	11.933914
11.405360	823.176001	11.938931
11.313592	828.846315	11.943949
11.684808	845.784896	11.948967
12.067536	851.324059	11.953984
11.899735	844.974090	11.959002
12.118155	825.939167	11.964019
11.633378	833.908112	11.969037
11.315309	828.783767	11.974055
11.770482	834.922071	11.979072
11.882827	822.985791	11.984090
11.670481	823.698317	11.989107
11.242594	821.168267	11.994125
11.524641	828.813672	11.999143
11.947604	850.041811	12.004160
11.833788	856.995882	12.009178
12.232128	845.242404	12.014195
11.806033	842.538658	12.019213
11.558608	834.381878	12.024231
11.595300	842.291616	12.029248
11.792342	854.373972	12.034266
11.907478	854.113044	12.039283
11.959987	853.960482	12.044301
11.754046	853.874247	12.049319
12.287029	856.619156	12.054336
11.886705	864.167337	12.059354
12.218858	856.327101	12.064371
11.848505	831.822275	12.069389
11.982855	825.348576	12.074407
11.928369	820.650085	12.079424
12.083553	841.766978	12.084442
12.024961	819.116637	12.089459
12.140821	820.620846	12.094477
11.879201	828.245679	12.099495
11.865474	830.489492	12.104512
11.773726	834.539799	12.109530
12.389426	830.591238	12.114547
12.206047	841.165845	12.119565
12.056902	834.218998	12.124583
11.899576	825.674953	12.129600
11.792801	822.596449	12.134618
12.100315	833.640820	12.139635
12.338714	847.627239	12.144653
12.174424	843.908736	12.149671
11.972121	839.265174	12.154688
11.993856	839.303887	12.159706
12.056913	841.615708	12.164723
12.156853	853.246470	12.169741
11.820581	849.303278	12.174759
12.170197	853.170041	12.179776
12.120503	855.522147	12.184794
12.732682	851.822744	12.189811
12.385714	842.773110	12.194829
12.144084	849.051367	12.199847
12.603978	848.994645	12.204864
12.036403	848.829611	12.209882
12.310213	829.518055	12.214899
12.265370	829.927946	12.219917
12.130361	834.322944	12.224935
12.363181	833.545604	12.229952
12.159893	858.700036	12.234970
12.452346	858.851663	12.239987
12.057104	848.838508	12.245005
12.265796	855.992392	12.250023
12.567449	839.659983	12.255040
12.403872	854.262352	12.260058
12.543599	851.410975	12.265075
12.409588	850.477165	12.270093
12.151558	855.206226	12.275111
12.222168	842.258492	12.280128
12.037597	852.729777	12.285146
12.302936	849.753527	12.290163
11.986898	857.452513	12.295181
11.784687	858.076175	12.300199
12.328062	853.346384	12.305216
12.081416	864.044238	12.310234
12.311782	872.073733	12.315251
12.606889	878.063535	12.320269
12.584114	879.704618	12.325287
12.927977	888.155846	12.330304
12.617158	879.993968	12.335322
12.737304	859.420970	12.340339
12.264897	861.047393	12.345357
12.282786	865.641112	12.350375
12.881928	868.019046	12.355392
12.861305	879.756352	12.360410
12.851307	861.402925	12.365427
13.014005	846.010841	12.370445
12.885457	844.750198	12.375463
12.769811	846.842576	12.380480
12.743457	847.544049	12.385498
12.448065	841.771373	12.390515
12.582628	841.972513	12.395533
12.427175	840.768472	12.400551
12.751394	848.766701	12.405568
12.560595	847.683049	12.410586
12.519153	842.620448	12.415603
12.637289	853.717386	12.420621
12.573930	869.459120	12.425639
12.824533	882.766500	12.430656
12.551578	890.389103	12.435674
12.695518	876.382148	12.440691
12.686554	881.269829	12.445709
12.503101	882.413928	12.450727
12.804568	882.584535	12.455744
12.790205	881.022388	12.460762
12.935297	871.950270	12.465779
12.678230	881.261502	12.470797
12.684464	884.431007	12.475815
12.981541	877.577499	12.480832
12.949413	879.076451	12.485850
13.161932	872.801984	12.490867
13.067128	889.750116	12.495885
12.859440	885.948041	12.500903
13.082810	879.770385	12.505920
12.810604	870.990222	12.510938
12.779706	872.535026	12.515955
12.998355	873.510133	12.520973
12.849548	871.458084	12.525991
13.077326	875.458747	12.531008
12.793613	872.980442	12.536026
13.069278	873.443257	12.541043
13.393937	870.283016	12.546061
12.843239	876.347639	12.551079
13.025609	869.952192	12.556096
12.981918	877.838034	12.561114
13.002877	874.918106	12.566131
13.039826	884.347458	12.571149
13.126965	888.340859	12.576167
13.211470	875.014681	12.581184
13.106165	877.340159	12.586202
13.480014	877.890079	12.591219
13.075412	878.876071	12.596237
12.994975	876.601142	12.601255
13.274954	867.664584	12.606272
13.251085	880.505396	12.611290
13.289997	876.781844	12.616307
13.023084	876.839324	12.621325
12.904075	875.119893	12.626343
13.259427	878.569050	12.631360
13.162537	899.315738	12.636378
13.281381	914.746941	12.641395
13.643429	907.733889	12.646413
13.361517	901.253958	12.651431
13.247393	885.453521	12.656448
13.061159	891.128840	12.661466
13.021086	896.396409	12.666483
13.443716	897.462396	12.671501
13.154003	906.300178	12.676519
13.552841	899.841392	12.681536
13.624764	898.580878	12.686554
13.548615	904.439356	12.691571
13.455665	902.994507	12.696589
13.400274	903.481918	12.701607
13.573847	898.648488	12.706624
13.865238	894.686784	12.711642
13.562422	887.437211	12.716659
13.902668	882.607339	12.721677
13.304735	879.450566	12.726695
13.654443	868.871845	12.731712
13.451105	861.656428	12.736730
13.169229	868.800062	12.741747
13.695909	878.558649	12.746765
13.960551	885.864495	12.751783
13.520931	874.068201	12.756800
13.225171	876.483607	12.761818
13.626605	887.083039	12.766835
14.082076	888.326049	12.771853
13.547060	881.122921	12.776871
13.679908	860.387809	12.781888
13.931864	863.696988	12.786906
13.534551	871.447989	12.791923
13.713836	869.091566	12.796941
13.546573	866.376337	12.801959
13.535329	866.449825	12.806976
13.721175	869.419201	12.811994
13.874463	896.910835	12.817011
14.244643	873.761673	12.822029
13.577309	886.064244	12.827047
13.827675	878.742942	12.832064
13.819356	866.749022	12.837082
13.558554	860.726371	12.842099
13.818515	852.543007	12.847117
13.587473	870.128688	12.852135
13.840388	888.524229	12.857152
13.968933	903.252358	12.862170
13.967130	893.791380	12.867187
14.037557	891.936525	12.872205
13.929275	888.276264	12.877223
13.810840	887.276502	12.882240
13.965139	886.201950	12.887258
13.725572	897.940023	12.892275
14.137199	896.913679	12.897293
13.826111	899.651058	12.902311
13.850664	892.240906	12.907328
13.913589	892.528282	12.912346
13.756172	893.978265	12.917363
14.310291	887.292675	12.922381
14.054500	893.077309	12.927399
14.177492	890.456607	12.932416
14.104762	899.085328	12.937434
13.868614	906.596362	12.942451
14.024709	905.662630	12.947469
14.369124	906.285121	12.952487
14.018691	898.345493	12.957504
14.181364	894.761695	12.962522
14.170135	904.353129	12.967539
14.401592	886.243584	12.972557
14.214745	910.020016	12.977575
14.098596	913.190069	12.982592
14.096871	897.248820	12.987610
13.848897	905.185755	12.992627
14.114337	901.105916	12.997645
14.095536	898.315566	13.002663
13.900469	886.837648	13.007680
14.158203	895.387352	13.012698
13.825863	902.019936	13.017715
14.013433	897.924625	13.022733
14.165879	910.790253	13.027751
14.200456	908.864168	13.032768
14.710694	920.957211	13.037786
14.130469	910.686639	13.042803
14.373787	913.407981	13.047821
14.313240	924.252654	13.052839
14.488049	926.453515	13.057856
14.610944	924.297710	13.062874
14.346457	905.726288	13.067891
14.529973	904.593765	13.072909
14.431090	911.501503	13.077927
14.169893	902.895262	13.082944
14.446776	919.326763	13.087962
14.584698	923.029150	13.092979
14.801641	924.683765	13.097997
14.705375	919.356620	13.103015
14.481395	905.567500	13.108032
14.786532	896.365984	13.113050
14.185530	909.941066	13.118067
14.557778	906.877857	13.123085
14.501902	919.868456	13.128103
14.767693	920.029607	13.133120
14.933752	917.359074	13.138138
14.503211	907.385960	13.143155
14.732146	895.960980	13.148173
14.652724	900.734543	13.153191
14.136304	905.109927	13.158208
14.532368	914.943264	13.163226
14.770531	927.702630	13.168243
14.773491	927.563962	13.173261
14.724087	919.933378	13.178279
14.601839	929.799433	13.183296
15.034490	918.869427	13.188314
15.066908	935.482266	13.193331
15.185385	921.574738	13.198349
14.756500	906.865497	13.203367
14.704380	894.444809	13.208384
14.711448	890.944197	13.213402
14.567920	899.973925	13.218419
14.827475	918.490039	13.223437
15.013662	922.216727	13.228455
14.743707	928.468797	13.233472
14.745185	926.441110	13.238490
14.693048	928.040995	13.243507
15.081960	927.401412	13.248525
14.647157	921.978267	13.253543
14.618690	929.380988	13.258560
14.851453	923.287378	13.263578
14.683129	918.042996	13.268595
14.934687	917.823293	13.273613
14.945440	920.507884	13.278631
14.756595	925.365275	13.283648
14.993899	918.752496	13.288666
14.739892	928.830057	13.293683
14.625632	917.051998	13.298701
15.234363	940.853674	13.303719
15.203730	942.631671	13.308736
15.569491	942.721783	13.313754
14.955765	940.903418	13.318771
14.932127	931.447402	13.323789
15.091484	936.387194	13.328807
15.521243	951.148846	13.333824
15.538954	933.112357	13.338842
15.376991	920.138040	13.343859
15.185627	924.041079	13.348877
15.216188	919.931163	13.353895
15.417272	917.309754	13.358912
15.289969	913.524108	13.363930
15.180653	916.836907	13.368947
15.456236	914.249047	13.373965
15.428563	924.900128	13.378983
15.097065	922.937111	13.384000
15.353940	906.392775	13.389018
15.001296	917.384909	13.394035
14.998780	912.820102	13.399053
15.193663	925.636217	13.404071
15.389921	941.140468	13.409088
15.493137	937.951463	13.414106
15.560468	941.423826	13.419123
15.833253	939.896491	13.424141
15.718661	931.482311	13.429159
15.382067	916.564533	13.434176
15.490594	911.372026	13.439194
15.312982	911.293705	13.444211
15.160420	907.295734	13.449229
15.419079	916.673312	13.454247
15.701808	942.380732	13.459264
15.846046	936.514704	13.464282
15.402481	942.772441	13.469299
15.585155	934.013120	13.474317
15.938714	935.735107	13.479335
15.207300	922.664371	13.484352
15.540028	932.410760	13.489370
15.671754	928.962756	13.494387
15.563435	933.307906	13.499405
15.586767	930.928040	13.504423
15.142776	934.016863	13.509440
15.945076	932.662023	13.514458
15.750225	939.938135	13.519475
15.705662	931.652124	13.524493
16.254352	927.157026	13.529511
15.830681	935.078332	13.534528
15.835919	935.305175	13.539546
15.815582	932.614859	13.544563
15.938188	938.531829	13.549581
16.146389	934.987931	13.554599
15.686821	928.596983	13.559616
15.786620	925.495933	13.564634
15.910912	934.903404	13.569651
15.868885	933.588304	13.574669
15.861362	930.885243	13.579687
15.934713	933.507138	13.584704
16.056442	932.801096	13.589722
15.952842	936.040328	13.594739
16.152021	932.171793	13.599757
16.363365	925.774290	13.604775
15.752058	920.285053	13.609792
15.810259	921.369933	13.614810
15.786246	932.201685	13.619827
15.752122	932.589338	13.624845
16.048169	935.574172	13.629863
15.813986	934.061335	13.634880
16.092043	932.498096	13.639898
15.979517	931.131468	13.644915
16.000790	933.142973	13.649933
15.888007	940.117381	13.654951
15.968905	942.118444	13.659968
16.050125	923.911063	13.664986
16.049369	926.539496	13.670003
15.787032	929.515635	13.675021
15.942947	929.175932	13.680039
16.049739	967.323677	13.685056
16.400935	959.268858	13.690074
16.741672	956.248046	13.695091
16.333174	951.672771	13.700109
16.548800	941.650522	13.705127
16.277432	933.501384	13.710144
16.550759	928.608750	13.715162
16.528069	921.849987	13.720179
16.353197	924.617215	13.725197
16.474603	921.221894	13.730215
16.617678	927.614534	13.735232
16.322276	925.663264	13.740250
16.506504	928.544548	13.745267
16.185170	924.536870	13.750285
16.450657	922.617498	13.755303
16.145306	931.606675	13.760320
16.318357	929.793902	13.765338
16.406500	923.680497	13.770355
16.160794	937.398629	13.775373
16.600471	951.132822	13.780391
16.597291	956.161477	13.785408
16.627304	952.565538	13.790426
16.495556	950.424452	13.795443
16.615704	958.794006	13.800461
16.937376	959.850898	13.805479
16.803492	954.585855	13.810496
16.477216	930.710887	13.815514
16.631727	944.903156	13.820531
16.884397	954.136298	13.825549
16.734771	938.687877	13.830567
16.369799	933.686780	13.835584
16.671834	939.368817	13.840602
16.688950	950.224096	13.845619
16.563722	965.556336	13.850637
16.467754	957.230979	13.855655
16.581241	968.061685	13.860672
16.857742	961.223152	13.865690
16.766089	958.764268	13.870707
16.664177	965.487323	13.875725
17.141722	962.561601	13.880743
16.923768	961.264746	13.885760
17.006375	961.631141	13.890778
17.015902	972.533351	13.895795
16.989490	962.191300	13.900813
16.860380	946.829231	13.905831
16.707865	956.432434	13.910848
17.097128	947.953482	13.915866
17.253108	951.652695	13.920883
16.818367	958.848596	13.925901
16.947278	945.354611	13.930919
16.795270	957.689384	13.935936
17.160859	950.410611	13.940954
17.246548	953.105262	13.945971
16.945815	955.094602	13.950989
17.219385	959.696679	13.956007
16.951789	963.004744	13.961024
16.732467	951.059207	13.966042
17.131513	958.290917	13.971059
17.095175	950.264716	13.976077
17.307810	960.680079	13.981095
17.070621	954.175809	13.986112
16.954910	966.538837	13.991130
17.128494	958.513763	13.996147
16.850227	956.361658	14.001165
17.145207	953.015587	14.006183
16.923434	960.685270	14.011200
17.203845	981.640345	14.016218
17.441664	978.705226	14.021235
17.436601	991.677254	14.026253
17.657089	982.242273	14.031271
17.663581	978.660056	14.036288
17.149925	959.112777	14.041306
17.593243	959.383153	14.046323
17.294481	950.751995	14.051341
17.653904	950.590832	14.056359
17.676126	952.438627	14.061376
17.418519	950.151436	14.066394
17.524736	955.458029	14.071411
17.401756	955.934961	14.076429
17.694384	954.562392	14.081447
17.389603	959.502721	14.086464
17.206296	945.151223	14.091482
17.528004	955.061234	14.096499
17.257895	978.715332	14.101517
17.410457	976.778401	14.106535
17.729948	980.188042	14.111552
17.869903	983.040634	14.116570
18.104190	978.143414	14.121587
17.676132	979.027989	14.126605
17.864536	974.629811	14.131623
17.556805	961.775792	14.136640
17.413022	972.143780	14.141658
17.618687	978.487915	14.146675
17.484932	980.658686	14.151693
17.651123	969.204657	14.156711
17.902194	970.364934	14.161728
17.576811	983.938819	14.166746
17.774725	976.263203	14.171763
17.879959	970.972810	14.176781
17.996806	970.669281	14.181799
17.742563	969.330005	14.186816
17.818456	977.960190	14.191834
18.271472	971.809695	14.196851
17.807291	973.353483	14.201869
17.957445	974.111606	14.206887
18.022696	974.057117	14.211904
17.641642	980.377166	14.216922
18.073848	979.356273	14.221939
17.886578	979.594460	14.226957
17.866063	979.400428	14.231975
18.067120	982.548780	14.236992
17.894566	980.529179	14.242010
18.008831	967.916591	14.247027
18.095569	975.701217	14.252045
18.213686	975.382915	14.257063
18.296523	976.674324	14.262080
17.802406	983.498022	14.267098
17.719471	968.783119	14.272115
17.977543	968.879218	14.277133
17.926573	976.342758	14.282151
18.397330	987.205368	14.287168
18.166987	997.997652	14.292186
18.390633	995.866519	14.297203
18.311009	995.854079	14.302221
18.440026	1001.284656	14.307239
18.602657	979.958332	14.312256
18.189343	987.762618	14.317274
18.335484	965.658845	14.322291
17.889269	988.008215	14.327309
18.586353	981.968540	14.332327
18.512514	993.230747	14.337344
18.444998	1000.636216	14.342362
18.860799	985.988462	14.347379
18.391822	978.892662	14.352397
18.408322	969.688611	14.357415
18.474221	963.883148	14.362432
18.259620	975.950961	14.367450
18.525906	983.640184	14.372467
18.480884	992.907192	14.377485
18.375115	986.388276	14.382503
18.710777	994.879298	14.387520
18.604394	1000.424157	14.392538
18.789670	987.408541	14.397555
18.857815	998.874616	14.402573
18.674890	992.846326	14.407591
18.798583	995.529587	14.412608
18.371273	990.188039	14.417626
19.011332	995.807743	14.422643
18.723693	998.945729	14.427661
18.637359	996.695769	14.432679
18.953284	987.064333	14.437696
18.879390	994.272853	14.442714
18.841643	987.426406	14.447731
18.955676	983.435926	14.452749
18.707250	966.918934	14.457767
18.628511	964.929887	14.462784
18.591891	979.913103	14.467802
18.744171	986.994100	14.472819
18.868450	988.790000	14.477837
18.670337	997.504250	14.482855
18.650588	985.970519	14.487872
18.554534	1004.490786	14.492890
18.906730	997.156340	14.497907
18.853213	991.301714	14.502925
18.956958	996.220798	14.507943
19.038615	988.803524	14.512960
18.892497	985.214246	14.517978
18.880262	987.422605	14.522995
18.916354	983.203310	14.528013
19.225912	991.172152	14.533031
19.406455	988.508857	14.538048
19.221166	997.513068	14.543066
19.296447	988.624242	14.548083
19.141927	990.448304	14.553101
19.118573	985.649160	14.558119
19.074234	981.794481	14.563136
19.157318	990.663211	14.568154
19.085862	984.000065	14.573171
19.300234	996.875411	14.578189
19.333304	1004.551617	14.583207
19.435439	1001.413557	14.588224
18.749600	1004.189265	14.593242
19.260908	1017.863853	14.598259
19.555995	1012.135048	14.603277
19.301594	1018.346598	14.608295
19.440831	1015.290974	14.613312
19.541679	1014.421672	14.618330
19.265523	1016.379403	14.623347
19.448388	1018.151060	14.628365
19.679596	1009.334667	14.633383
19.864645	1009.070057	14.638400
19.494803	1011.753986	14.643418
19.639940	1013.754677	14.648435
19.870741	1010.008633	14.653453
19.178774	1001.393417	14.658471
19.896799	999.258133	14.663488
19.682237	1006.175189	14.668506
19.751053	999.130250	14.673523
19.734654	993.971939	14.678541
19.599265	994.799688	14.683559
19.765923	986.458273	14.688576
19.402693	992.483498	14.693594
19.556828	1006.614086	14.698611
19.718500	1001.373992	14.703629
19.854400	1010.054309	14.708647
20.072822	1019.020751	14.713664
19.703711	1011.372688	14.718682
19.921448	1008.973084	14.723699
20.070234	1011.807689	14.728717
19.753649	1017.768531	14.733735
20.208783	1003.327614	14.738752
19.647818	996.922492	14.743770
19.847878	1006.039182	14.748787
19.912557	1009.397646	14.753805
19.611828	1010.737682	14.758823
20.016354	1006.179193	14.763840
20.021644	1020.322975	14.768858
19.846405	1013.460858	14.773875
20.372317	1007.239650	14.778893
19.838270	1013.485994	14.783911
19.991074	1014.366891	14.788928
19.788506	1014.880792	14.793946
19.923248	1012.275251	14.798963
20.170751	1012.804329	14.803981
19.902629	1021.990918	14.808999
20.215059	1012.251202	14.814016
19.906167	1017.370745	14.819034
20.041069	1011.979190	14.824051
20.243955	1012.995882	14.829069
20.133049	1015.213662	14.834087
20.268738	1005.131365	14.839104
20.189572	1017.146912	14.844122
20.066981	1014.486273	14.849139
20.444596	1016.988228	14.854157
20.307389	1038.063566	14.859175
20.683658	1031.473633	14.864192
20.759685	1023.364269	14.869210
20.441579	1010.635329	14.874227
20.475449	1009.148060	14.879245
20.305669	1006.100793	14.884263
20.268172	1002.691956	14.889280
20.358961	1010.065955	14.894298
20.234683	1014.097082	14.899315
20.542226	1032.437713	14.904333
20.536934	1035.577662	14.909351
20.628446	1030.723308	14.914368
20.684367	1040.672572	14.919386
20.558282	1041.396833	14.924403
21.076134	1034.987801	14.929421
20.522789	1022.441011	14.934439
20.595993	1001.432931	14.939456
20.579702	1001.834762	14.944474
20.688677	1017.597571	14.949491
21.028583	1030.161892	14.954509
20.718042	1037.141665	14.959527
20.940960	1019.260111	14.964544
20.242625	1004.700798	14.969562
20.753090	1021.885420	14.974579
20.939821	1021.936231	14.979597
20.765617	1033.544923	14.984615
21.051721	1034.114861	14.989632
20.865195	1026.541523	14.994650
20.841098	1036.226688	14.999667
21.277077	1027.275478	15.004685
21.065447	1044.696364	15.009703
20.988414	1029.306514	15.014720
21.029414	1037.053461	15.019738
20.732549	1039.215571	15.024755
20.809379	1032.434409	15.029773
21.048580	1037.275028	15.034791
20.822168	1027.155915	15.039808
20.837145	1029.802432	15.044826
20.983443	1036.725213	15.049843
20.908777	1042.877154	15.054861
20.971868	1033.692527	15.059879
20.915460	1033.173177	15.064896
21.146843	1033.001091	15.069914
20.955216	1037.927274	15.074931
21.375005	1038.238345	15.079949
21.137683	1051.965231	15.084967
21.128010	1057.927332	15.089984
21.663296	1047.687647	15.095002
21.577095	1047.459791	15.100019
21.238070	1027.301175	15.105037
21.375191	1037.951083	15.110055
21.479575	1025.364487	15.115072
21.594166	1013.215319	15.120090
21.479495	1018.908973	15.125107
21.578100	1010.625437	15.130125
21.279617	1023.189752	15.135143
21.409481	1017.161330	15.140160
21.330627	1021.388661	15.145178
21.342741	1036.005863	15.150195
21.578189	1038.582488	15.155213
21.818977	1051.516301	15.160231
21.586569	1038.393904	15.165248
21.603310	1034.868633	15.170266
21.316026	1046.049436	15.175283
21.663092	1044.905819	15.180301
21.593122	1045.849709	15.185319
21.663394	1037.554702	15.190336
21.567792	1051.252854	15.195354
21.799057	1052.533716	15.200371
22.052846	1052.765936	15.205389
21.710782	1055.659029	15.210407
21.952096	1043.303885	15.215424
22.176407	1040.173380	15.220442
21.985661	1044.716012	15.225459
21.800456	1030.686942	15.230477
21.622206	1033.156761	15.235495
21.931135	1039.540345	15.240512
21.911327	1042.727176	15.245530
21.730402	1044.160983	15.250547
21.980322	1043.894312	15.255565
22.016184	1046.068554	15.260583
22.085258	1047.539776	15.265600
21.923661	1042.906942	15.270618
22.075413	1046.020745	15.275635
22.112092	1047.592582	15.280653
22.128248	1045.272536	15.285671
22.008882	1048.856472	15.290688
22.316283	1041.970678	15.295706
21.782651	1048.850139	15.300723
22.143878	1042.792331	15.305741
21.999663	1052.536327	15.310759
21.771192	1058.575523	15.315776
21.992766	1044.641596	15.320794
21.922907	1044.463591	15.325811
22.072319	1050.168135	15.330829
22.152148	1066.515644	15.335847
22.145281	1077.132099	15.340864
22.379229	1078.801241	15.345882
22.293066	1081.060210	15.350899
22.416187	1072.845414	15.355917
22.401646	1080.458276	15.360935
22.561229	1079.340324	15.365952
22.738031	1068.992765	15.370970
22.534236	1069.769626	15.375987
22.638206	1074.350560	15.381005
22.734650	1081.110169	15.386023
22.617228	1072.523767	15.391040
22.587733	1068.440269	15.396058
22.462278	1069.162064	15.401075
22.555409	1070.444892	15.406093
22.536332	1071.251849	15.411111
22.488061	1077.168965	15.416128
22.468813	1066.466265	15.421146
22.374501	1067.394693	15.426163
22.620088	1075.285778	15.431181
22.552813	1081.370185	15.436199
22.793949	1079.146794	15.441216
22.594677	1074.979949	15.446234
22.644464	1077.047776	15.451251
22.494388	1074.678830	15.456269
22.717413	1088.446390	15.461287
22.813061	1102.137389	15.466304
23.242453	1104.127334	15.471322
23.238086	1115.408067	15.476339
23.285406	1094.497234	15.481357
22.908499	1079.882961	15.486375
22.750031	1073.052686	15.491392
23.286811	1080.915335	15.496410
22.944724	1078.430503	15.501427
23.105813	1070.261394	15.506445
22.990216	1074.812481	15.511463
23.073503	1095.464708	15.516480
23.472378	1094.073782	15.521498
23.035038	1084.826370	15.526515
22.903475	1076.035642	15.531533
22.694845	1079.367249	15.536551
22.817491	1092.866208	15.541568
23.194378	1091.074252	15.546586
23.283431	1093.765026	15.551603
22.939282	1086.453891	15.556621
23.322118	1088.371815	15.561639
23.559124	1094.951925	15.566656
23.830177	1096.068366	15.571674
23.489329	1093.932881	15.576691
23.673156	1090.753945	15.581709
23.611104	1085.107356	15.586727
23.648724	1105.293592	15.591744
23.944759	1090.823577	15.596762
23.674869	1083.596221	15.601779
23.525928	1059.467371	15.606797
23.607072	1056.965154	15.611815
23.467128	1058.327238	15.616832
23.649930	1054.158079	15.621850
23.357344	1069.231902	15.626867
23.523548	1081.304575	15.631885
23.866742	1078.717521	15.636903
23.347676	1091.511423	15.641920
23.828923	1089.683524	15.646938
23.804603	1098.116393	15.651955
23.753028	1091.544782	15.656973
23.749308	1087.214733	15.661991
23.711958	1083.581280	15.667008
23.629462	1087.917680	15.672026
23.328784	1088.215941	15.677043
23.629124	1092.986247	15.682061
23.469415	1078.174296	15.687079
23.655501	1090.658392	15.692096
23.830450	1084.392017	15.697114
23.604459	1097.803339	15.702131
23.939574	1110.639933	15.707149
24.222965	1119.146158	15.712167
24.081157	1116.651251	15.717184
24.146623	1108.641604	15.722202
23.985234	1127.228319	15.727219
24.001170	1128.104679	15.732237
24.287588	1118.665411	15.737255
24.392685	1114.859812	15.742272
24.367343	1108.301769	15.747290
24.049755	1115.769678	15.752307
23.893846	1126.371235	15.757325
24.432156	1123.650567	15.762343
24.324126	1121.506915	15.767360
24.436069	1111.782554	15.772378
24.363089	1113.150701	15.777395
24.348422	1123.496863	15.782413
24.320125	1123.323798	15.787431
24.392333	1118.141159	15.792448
24.807788	1115.171739	15.797466
24.699654	1116.365408	15.802483
24.350406	1093.238360	15.807501
24.770027	1097.315632	15.812519
24.320768	1087.037468	15.817536
24.775490	1086.916454	15.822554
24.409795	1079.482720	15.827571
24.582921	1089.657690	15.832589
24.618355	1091.526937	15.837607
24.494446	1109.305589	15.842624
24.822058	1109.974363	15.847642
24.712978	1113.237960	15.852659
24.826487	1100.823784	15.857677
24.705878	1088.156420	15.862695
24.207069	1096.972771	15.867712
24.802737	1102.771282	15.872730
24.726982	1111.205966	15.877747
24.525908	1125.031833	15.882765
24.847551	1111.525142	15.887783
24.533351	1104.634577	15.892800
24.548544	1103.774505	15.897818
24.906203	1111.717550	15.902835
24.682314	1110.491731	15.907853
24.877801	1101.418039	15.912871
24.835170	1103.560188	15.917888
24.753170	1108.097072	15.922906
24.984915	1110.883740	15.927923
25.331541	1115.508236	15.932941
25.410435	1108.463943	15.937959
24.625258	1116.671623	15.942976
25.213458	1115.021687	15.947994
25.414127	1116.227898	15.953011
25.129157	1093.355740	15.958029
25.529901	1100.274292	15.963047
25.019283	1109.801945	15.968064
25.335139	1108.563496	15.973082
25.038305	1109.394507	15.978099
25.237765	1113.386136	15.983117
25.394479	1112.804207	15.988135
25.628152	1121.895533	15.993152
25.448320	1122.301758	15.998170
25.161244	1105.484158	16.003187
25.299978	1121.966066	16.008205
25.508037	1110.384951	16.013223
25.386986	1119.061145	16.018240
25.441124	1120.582670	16.023258
25.523235	1119.480273	16.028275
25.315811	1129.248540	16.033293
25.604721	1114.128596	16.038311
25.265315	1116.163316	16.043328
25.303275	1114.842265	16.048346
25.564491	1115.281496	16.053363
25.415192	1126.362402	16.058381
25.573553	1115.967866	16.063399
25.296914	1120.870924	16.068416
25.397650	1126.219027	16.073434
26.026687	1142.537268	16.078451
26.000178	1143.471619	16.083469
26.170478	1138.208797	16.088487
26.042531	1136.023165	16.093504
25.927413	1123.622148	16.098522
26.074135	1120.050381	16.103539
25.776270	1113.851892	16.108557
26.131799	1112.304372	16.113575
26.019964	1111.789259	16.118592
26.051815	1100.002266	16.123610
26.051899	1107.083867	16.128627
25.952589	1099.359880	16.133645
26.403278	1100.902670	16.138663
26.003655	1103.519893	16.143680
25.991727	1100.810247	16.148698
26.336468	1122.288664	16.153715
26.242942	1131.565149	16.158733
26.123553	1115.140436	16.163751
26.028865	1127.768978	16.168768
26.106129	1136.237632	16.173786
26.185601	1131.499195	16.178803
26.050744	1131.831857	16.183821
26.045722	1137.106312	16.188839
25.760718	1147.683751	16.193856
25.903366	1146.148379	16.198874
26.189512	1139.034789	16.203891
26.289695	1156.355462	16.208909
26.773175	1162.925970	16.213927
26.433887	1160.644175	16.218944
26.691532	1150.592212	16.223962
26.718706	1142.393825	16.228979
26.407173	1135.591375	16.233997
26.704504	1130.617360	16.239015
26.699493	1132.377564	16.244032
26.502149	1134.504738	16.249050
27.014659	1134.626500	16.254067
26.628420	1132.865975	16.259085
26.883043	1131.211525	16.264103
26.784583	1128.879310	16.269120
26.651839	1129.507247	16.274138
26.702552	1129.219369	16.279155
26.590389	1141.288097	16.284173
26.969125	1154.836904	16.289191
26.589696	1165.024899	16.294208
26.770189	1145.275087	16.299226
27.244001	1142.640654	16.304243
27.004879	1153.038886	16.309261
27.190803	1153.686595	16.314279
27.260647	1156.222113	16.319296
27.173028	1153.367508	16.324314
27.425785	1146.271439	16.329331
27.277329	1139.531395	16.334349
27.360726	1126.304184	16.339367
27.115566	1121.676671	16.344384
27.080045	1112.726764	16.349402
27.318044	1112.722457	16.354419
27.000083	1124.882455	16.359437
26.825675	1126.611015	16.364455
26.889462	1134.824847	16.369472
26.948834	1145.910254	16.374490
27.489921	1144.405286	16.379507
27.516913	1146.978391	16.384525
27.234900	1149.203602	16.389543
27.234134	1155.664589	16.394560
27.448712	1152.658093	16.399578
27.316098	1139.092802	16.404595
27.165559	1147.915990	16.409613
27.216057	1155.589392	16.414631
27.219031	1156.382277	16.419648
27.450442	1174.312887	16.424666
27.544365	1176.308286	16.429683
27.304544	1175.996380	16.434701
27.769078	1188.058415	16.439719
27.920127	1189.065579	16.444736
27.524250	1188.226588	16.449754
27.620115	1183.781250	16.454771
27.200093	1185.175654	16.459789
27.565615	1179.942162	16.464807
27.702305	1185.846863	16.469824
27.482128	1185.987748	16.474842
27.776238	1175.717372	16.479859
27.600284	1192.511753	16.484877
27.983771	1198.865959	16.489895
28.163717	1199.032050	16.494912
28.082490	1203.349771	16.499930
28.485266	1197.339753	16.504947
28.339905	1181.138521	16.509965
28.446437	1178.343744	16.514983
28.341299	1175.948855	16.520000
28.333120	1179.010189	16.525018
28.402390	1169.057247	16.530035
28.565468	1171.241778	16.535053
28.085756	1169.553578	16.540071
28.490193	1171.523644	16.545088
28.411639	1178.789508	16.550106
28.290456	1167.624517	16.555123
28.544967	1178.229930	16.560141
28.235289	1181.971706	16.565159
28.456576	1176.755161	16.570176
28.398433	1175.680071	16.575194
28.362830	1162.081407	16.580211
28.530170	1174.986327	16.585229
28.578066	1178.967985	16.590247
28.339071	1174.221934	16.595264
28.206696	1183.830611	16.600282
28.574808	1183.583378	16.605299
28.761460	1171.999062	16.610317
28.340091	1176.700890	16.615335
28.529087	1166.017834	16.620352
28.266976	1179.117328	16.625370
28.538289	1183.987722	16.630387
28.514075	1171.582667	16.635405
28.709117	1185.455712	16.640423
29.005783	1199.626892	16.645440
28.900717	1203.802116	16.650458
28.689005	1199.703425	16.655475
28.762925	1207.515875	16.660493
28.887613	1209.339683	16.665511
28.785700	1198.877487	16.670528
28.859983	1209.319032	16.675546
29.053750	1206.357887	16.680563
28.779364	1203.702027	16.685581
28.841725	1206.125813	16.690599
29.061983	1196.425619	16.695616
29.057237	1210.825530	16.700634
28.930325	1198.478953	16.705651
28.751131	1207.138037	16.710669
28.573627	1203.058295	16.715687
29.043864	1219.208203	16.720704
28.744643	1232.234161	16.725722
29.334772	1234.680565	16.730739
29.397254	1231.831649	16.735757
29.584768	1230.392580	16.740775
29.662257	1231.206813	16.745792
29.459344	1232.860972	16.750810
29.881760	1222.545546	16.755827
29.628556	1231.372364	16.760845
29.735709	1220.004271	16.765863
29.609892	1210.769271	16.770880
29.447444	1207.732758	16.775898
29.316815	1202.608409	16.780915
29.511424	1220.001136	16.785933
29.757906	1217.647136	16.790951
29.644722	1221.715258	16.795968
29.647720	1236.152490	16.800986
29.700099	1225.071752	16.806003
29.929921	1232.055021	16.811021
29.776295	1227.102748	16.816039
30.034518	1213.955611	16.821056
30.074778	1209.151593	16.826074
30.394509	1212.871243	16.831091
29.774615	1196.456327	16.836109
29.632970	1193.391186	16.841127
30.076422	1192.872091	16.846144
29.897021	1208.204866	16.851162
29.789396	1215.939068	16.856179
29.949722	1218.159883	16.861197
29.950681	1220.418057	16.866215
29.920944	1211.927110	16.871232
30.157234	1230.742091	16.876250
30.362569	1212.163710	16.881267
30.259580	1223.050641	16.886285
29.997870	1224.725144	16.891303
30.047732	1215.232205	16.896320
30.074687	1220.726374	16.901338
29.735639	1216.796928	16.906355
29.961318	1213.198511	16.911373
30.216767	1206.482624	16.916391
30.325012	1227.178536	16.921408
30.093032	1234.701834	16.926426
30.450190	1240.242806	16.931443
30.593437	1246.711526	16.936461
30.636012	1256.529689	16.941479
30.837635	1240.397219	16.946496
30.833392	1250.852950	16.951514
30.718365	1236.720768	16.956531
30.947640	1213.042883	16.961549
30.730994	1217.688849	16.966567
30.749433	1213.183669	16.971584
30.664453	1219.050418	16.976602
30.853850	1213.170721	16.981619
30.569063	1209.728894	16.986637
30.601983	1212.546271	16.991655
30.989870	1206.520800	16.996672
30.578254	1230.153794	17.001690
31.170351	1237.582050	17.006707
31.066257	1240.282724	17.011725
30.842101	1247.400657	17.016743
30.788260	1238.850696	17.021760
30.954054	1237.241815	17.026778
30.985207	1240.509623	17.031795
31.115609	1235.587763	17.036813
30.931408	1244.514390	17.041831
31.023502	1237.514110	17.046848
30.873865	1242.420822	17.051866
30.775830	1233.078869	17.056883
31.037026	1239.286789	17.061901
30.846019	1234.350335	17.066919
31.418822	1244.928588	17.071936
31.305161	1268.804882	17.076954
31.770804	1243.896125	17.081971
31.844388	1234.404765	17.086989
31.659742	1222.055507	17.092007
31.920910	1208.587460	17.097024
31.922674	1215.986505	17.102042
31.680530	1222.047904	17.107059
31.806649	1220.434755	17.112077
31.950915	1218.682013	17.117095
32.108150	1212.548022	17.122112
32.027061	1212.518503	17.127130
31.745942	1201.608231	17.132147
31.921277	1185.226655	17.137165
31.635532	1185.141991	17.142183
31.648386	1178.284145	17.147200
31.859583	1191.861065	17.152218
32.282726	1195.083966	17.157235
31.936161	1178.045047	17.162253
31.611765	1185.945943	17.167271
31.499230	1189.030034	17.172288
31.984345	1212.869688	17.177306
31.911115	1219.700304	17.182323
32.153251	1205.486691	17.187341
31.993572	1212.246365	17.192359
31.963833	1204.394703	17.197376
32.041662	1203.741764	17.202394
32.342489	1205.572285	17.207411
32.346252	1213.442585	17.212429
32.217196	1218.972178	17.217447
32.084397	1209.180340	17.222464
31.878179	1214.883487	17.227482
31.998673	1209.387762	17.232499
31.988707	1202.750181	17.237517
31.980639	1219.002354	17.242535
32.368137	1215.161282	17.247552
32.472828	1206.889625	17.252570
31.923838	1217.904578	17.257587
32.246409	1231.958334	17.262605
32.653136	1237.472614	17.267623
32.601970	1249.044210	17.272640
32.678873	1248.204046	17.277658
32.598700	1245.514706	17.282675
32.830554	1240.200147	17.287693
32.799654	1247.467419	17.292711
32.734232	1248.830590	17.297728
32.842888	1241.550051	17.302746
32.901701	1233.764044	17.307763
32.512923	1244.100860	17.312781
32.634819	1243.478820	17.317799
32.807399	1239.226076	17.322816
32.689806	1240.111911	17.327834
32.532320	1246.728344	17.332851
32.695359	1239.436261	17.337869
32.535581	1241.256497	17.342887
32.977407	1247.348166	17.347904
32.751577	1256.045492	17.352922
32.871476	1265.130314	17.357939
33.176780	1262.406598	17.362957
32.993449	1264.602724	17.367975
33.386370	1263.363338	17.372992
33.305740	1274.726073	17.378010
33.015324	1266.764327	17.383027
33.233178	1265.168687	17.388045
33.285485	1277.102091	17.393063
33.084193	1268.976621	17.398080
33.301829	1275.027407	17.403098
32.889996	1269.080529	17.408115
33.500834	1257.032210	17.413133
33.251918	1266.351774	17.418151
33.495075	1293.217739	17.423168
33.777049	1294.035580	17.428186
33.795584	1287.794182	17.433203
34.280116	1279.763810	17.438221
33.835475	1271.671860	17.443239
34.226622	1251.493651	17.448256
33.976585	1249.786382	17.453274
33.632306	1259.496059	17.458291
33.965433	1245.475415	17.463309
33.778417	1250.708538	17.468327
34.085612	1245.758836	17.473344
33.940969	1250.728496	17.478362
33.877868	1252.708127	17.483379
34.016257	1239.505190	17.488397
34.105710	1240.645747	17.493415
34.336853	1238.639113	17.498432
34.210513	1238.142532	17.503450
33.970820	1249.391198	17.508467
34.280995	1248.516619	17.513485
34.032502	1253.057440	17.518503
34.075784	1252.264362	17.523520
34.360498	1251.794131	17.528538
34.058226	1252.886445	17.533555
33.826657	1247.055633	17.538573
33.902948	1257.321904	17.543591
33.760224	1274.653328	17.548608
34.409313	1283.223802	17.553626
34.273033	1278.383787	17.558643
34.047719	1271.663865	17.563661
34.275378	1285.114149	17.568679
34.161248	1275.344377	17.573696
34.611258	1281.131599	17.578714
34.168847	1282.065405	17.583731
34.702200	1291.359637	17.588749
34.675231	1307.939984	17.593767
34.959230	1306.009634	17.598784
34.752914	1288.316202	17.603802
34.685875	1289.901267	17.608819
34.802534	1294.035939	17.613837
35.069070	1301.705796	17.618855
35.142378	1303.452094	17.623872
35.016614	1277.588595	17.628890
34.608965	1290.427037	17.633907
34.878318	1274.106198	17.638925
34.772452	1298.574280	17.643943
34.942613	1304.669925	17.648960
35.200791	1304.962834	17.653978
34.999277	1304.487333	17.658995
35.092529	1300.190012	17.664013
35.164895	1293.501783	17.669031
35.218309	1295.488146	17.674048
35.335193	1301.509928	17.679066
34.907104	1310.006487	17.684083
35.077353	1307.698335	17.689101
35.294604	1299.703264	17.694119
35.171021	1300.755030	17.699136
35.228369	1298.372635	17.704154
34.992731	1310.472923	17.709171
35.280834	1324.592491	17.714189
35.911637	1329.704077	17.719207
35.622976	1329.255376	17.724224
35.902953	1328.015754	17.729242
35.794889	1329.092316	17.734259
36.112488	1326.516931	17.739277
35.682242	1300.742877	17.744295
35.494499	1301.348812	17.749312
35.875776	1310.763253	17.754330
35.613030	1323.218967	17.759347
35.727071	1324.004136	17.764365
35.891678	1328.973301	17.769383
35.922801	1331.969911	17.774400
36.089358	1328.259206	17.779418
36.109624	1329.893225	17.784435
36.025120	1331.536094	17.789453
36.330502	1328.066981	17.794471
36.144818	1330.961444	17.799488
36.789570	1315.260325	17.804506
36.254066	1311.545774	17.809523
36.049403	1303.114782	17.814541
36.074639	1312.486498	17.819559
36.146755	1317.948045	17.824576
36.695242	1322.134578	17.829594
36.263560	1316.984162	17.834611
35.880109	1329.417313	17.839629
36.284435	1327.768218	17.844647
36.038704	1334.799612	17.849664
36.404486	1316.478806	17.854682
36.077379	1320.204205	17.859699
36.452941	1318.873995	17.864717
36.704541	1325.321497	17.869735
36.362346	1328.684283	17.874752
36.868778	1332.336108	17.879770
36.896959	1349.334297	17.884787
36.591148	1337.649764	17.889805
36.710224	1338.124892	17.894823
36.883859	1338.641390	17.899840
37.069545	1336.804438	17.904858
36.922280	1341.926706	17.909875
37.237774	1329.501208	17.914893
37.033224	1321.532527	17.919911
36.859660	1321.648783	17.924928
37.076097	1312.027484	17.929946
37.141783	1318.325217	17.934963
36.872858	1329.005424	17.939981
37.237462	1326.467737	17.944999
37.166145	1327.852752	17.950016
37.096790	1329.764538	17.955034
37.218642	1341.620956	17.960051
37.378424	1337.996594	17.965069
37.237145	1333.729556	17.970087
37.098390	1340.590342	17.975104
37.246844	1334.407170	17.980122
37.153635	1348.921421	17.985139
37.162432	1341.847666	17.990157
37.231316	1336.937513	17.995175
37.149797	1345.827155	18.000192
37.478239	1345.594939	18.005210
37.488324	1369.651112	18.010227
37.593091	1366.360202	18.015245
37.929826	1367.559498	18.020263
38.028288	1370.640841	18.025280
38.018787	1363.298481	18.030298
37.676720	1361.055496	18.035315
37.536845	1355.614948	18.040333
37.916515	1359.518602	18.045351
38.092423	1369.635630	18.050368
38.071561	1358.829266	18.055386
38.026043	1371.384340	18.060403
37.976242	1368.161288	18.065421
37.948458	1366.889855	18.070439
37.572280	1367.024437	18.075456
38.025053	1358.459777	18.080474
38.118812	1365.802359	18.085491
38.213325	1364.369592	18.090509
38.282311	1357.715158	18.095527
38.012602	1360.673701	18.100544
38.210153	1352.948752	18.105562
37.858180	1368.578476	18.110579
37.984230	1376.937640	18.115597
38.313692	1384.069059	18.120615
38.094251	1388.481512	18.125632
38.383865	1391.096682	18.130650
38.780496	1392.844082	18.135667
38.414258	1397.637246	18.140685
38.660168	1390.125715	18.145703
38.790944	1391.643066	18.150720
38.350206	1379.528691	18.155738
38.316282	1385.969865	18.160755
38.661118	1410.525830	18.165773
39.316058	1413.440430	18.170791
39.274192	1417.599561	18.175808
39.459632	1397.370519	18.180826
39.253734	1389.533308	18.185843
38.900362	1380.238183	18.190861
38.988657	1372.639335	18.195879
38.991350	1370.042959	18.200896
38.990506	1378.213475	18.205914
39.103896	1378.717689	18.210931
38.931439	1368.563452	18.215949
39.306399	1379.289635	18.220967
38.970372	1393.658842	18.225984
39.706664	1397.059340	18.231002
39.802794	1409.400315	18.236019
39.577219	1391.610943	18.241037
39.297656	1374.824282	18.246055
39.238204	1380.497331	18.251072
39.087484	1389.260262	18.256090
39.213302	1405.289156	18.261107
39.717137	1407.481577	18.266125
39.713958	1403.601882	18.271143
39.461091	1403.943421	18.276160
39.700061	1402.494062	18.281178
40.148385	1397.499144	18.286195
39.433022	1403.842132	18.291213
39.750858	1406.962025	18.296231
39.840895	1410.085511	18.301248
39.671699	1399.761248	18.306266
39.915860	1391.401493	18.311283
39.674887	1408.395412	18.316301
39.789143	1402.498143	18.321319
39.556184	1404.804249	18.326336
39.685174	1405.848532	18.331354
40.413210	1416.037520	18.336371
40.051951	1422.825283	18.341389
40.534233	1422.684165	18.346407
40.200642	1426.678540	18.351424
40.152299	1413.291969	18.356442
40.188725	1417.480676	18.361459
40.047809	1418.068052	18.366477
40.089139	1416.098470	18.371495
40.426249	1424.691449	18.376512
40.440174	1431.797680	18.381530
40.421775	1419.486530	18.386547
40.118207	1425.388889	18.391565
40.486048	1422.092874	18.396583
40.604408	1419.203592	18.401600
40.428313	1430.146839	18.406618
40.373569	1430.595582	18.411635
40.483271	1438.279418	18.416653
40.928548	1441.084988	18.421671
41.135086	1451.241490	18.426688
41.097179	1452.900487	18.431706
41.020117	1453.443064	18.436723
41.178458	1456.462371	18.441741
41.255509	1444.906197	18.446759
41.373133	1436.134312	18.451776
41.044144	1423.926839	18.456794
41.360301	1425.141744	18.461811
40.999948	1421.965079	18.466829
41.035098	1429.360087	18.471847
41.034900	1442.595438	18.476864
41.201790	1456.519241	18.481882
41.269965	1444.415391	18.486899
41.239414	1441.925664	18.491917
41.696756	1439.178368	18.496935
41.291084	1446.769049	18.501952
41.403462	1444.355887	18.506970
41.463495	1440.770816	18.511987
41.357011	1448.673626	18.517005
41.371453	1440.045545	18.522023
41.657621	1439.299908	18.527040
41.319020	1442.928626	18.532058
41.886838	1445.527947	18.537075
41.426822	1453.066595	18.542093
41.537157	1457.883768	18.547111
41.960656	1465.060308	18.552128
41.796772	1477.541536	18.557146
42.049052	1466.428772	18.562163
42.161221	1468.467055	18.567181
42.087558	1464.813925	18.572199
42.286564	1459.664345	18.577216
41.969150	1463.318107	18.582234
42.027926	1465.454768	18.587251
41.894017	1464.966515	18.592269
42.308178	1464.979550	18.597287
42.287968	1460.820012	18.602304
41.955740	1463.697383	18.607322
41.997333	1458.466151	18.612339
42.109668	1459.617312	18.617357
42.442724	1458.453544	18.622375
42.355310	1463.864546	18.627392
42.493588	1484.560566	18.632410
42.910503	1472.131578	18.637427
42.327779	1472.491410	18.642445
42.493928	1469.727079	18.647463
42.729901	1491.594021	18.652480
42.517164	1495.384804	18.657498
42.848612	1487.114498	18.662515
42.608602	1484.509592	18.667533
43.143748	1486.994256	18.672551
43.283194	1485.561139	18.677568
43.075797	1496.210627	18.682586
43.346613	1493.598462	18.687603
42.936866	1486.362730	18.692621
43.030622	1487.669700	18.697639
43.300742	1485.159017	18.702656
42.971686	1491.180559	18.707674
43.411914	1492.103347	18.712691
43.030902	1488.727350	18.717709
43.011771	1492.157440	18.722727
43.215578	1491.822802	18.727744
43.280928	1498.633200	18.732762
43.317059	1494.044513	18.737779
43.116192	1497.344222	18.742797
43.142792	1483.337801	18.747815
43.249915	1487.616210	18.752832
43.351598	1498.227221	18.757850
43.873506	1507.411090	18.762867
43.483374	1514.670929	18.767885
43.556874	1523.448453	18.772903
43.529211	1509.902691	18.777920
43.456965	1512.690854	18.782938
43.496284	1506.770697	18.787955
43.485128	1506.069858	18.792973
43.655854	1515.776471	18.797991
43.918784	1520.661940	18.803008
44.019031	1523.271029	18.808026
44.300651	1531.649840	18.813043
44.039482	1540.105556	18.818061
44.163135	1527.927914	18.823079
44.529769	1539.836544	18.828096
44.239420	1534.287154	18.833114
44.556210	1524.372795	18.838131
44.473613	1525.028874	18.843149
44.445819	1515.181501	18.848167
44.585363	1519.646270	18.853184
44.198370	1528.826822	18.858202
44.798989	1523.416980	18.863219
44.775671	1530.009592	18.868237
44.735991	1522.265697	18.873255
44.898225	1507.938844	18.878272
44.447114	1506.744241	18.883290
44.819252	1517.311754	18.888307
44.666870	1522.222748	18.893325
44.834275	1519.785523	18.898343
44.728409	1511.478624	18.903360
44.566251	1520.386809	18.908378
45.036935	1526.704109	18.913395
44.801849	1515.044167	18.918413
44.768237	1523.873048	18.923431
44.888174	1513.826088	18.928448
44.982474	1521.947694	18.933466
44.893041	1513.872499	18.938483
45.062457	1526.203622	18.943501
44.824571	1518.785556	18.948519
44.972056	1527.124333	18.953536
45.213872	1542.053623	18.958554
45.442444	1545.238289	18.963571
45.357610	1553.100572	18.968589
45.574172	1547.123750	18.973607
45.561572	1540.021553	18.978624
45.013887	1539.767599	18.983642
45.776168	1536.599664	18.988659
45.763294	1548.045881	18.993677
45.522172	1549.982535	18.998695
45.901485	1542.366218	19.003712
45.603750	1548.641040	19.008730
45.894042	1538.478325	19.013747
45.624645	1546.353781	19.018765
45.351869	1549.806116	19.023783
45.812751	1552.846501	19.028800
46.051840	1565.547200	19.033818
46.315789	1569.212778	19.038835
46.272132	1568.446253	19.043853
46.311894	1571.082666	19.048871
46.417943	1560.766939	19.053888
46.214877	1568.029549	19.058906
46.323136	1569.634487	19.063923
46.314883	1571.851129	19.068941
46.701628	1570.473978	19.073959
46.607047	1564.472984	19.078976
46.617787	1570.043570	19.083994
46.230047	1572.079053	19.089011
46.291702	1562.220805	19.094029
46.467839	1580.911919	19.099047
46.505044	1564.517534	19.104064
46.968061	1557.965597	19.109082
46.670890	1562.746020	19.114099
46.709009	1565.644287	19.119117
46.592756	1567.665611	19.124135
46.628431	1557.089107	19.129152
46.632186	1562.427211	19.134170
47.122550	1565.976053	19.139187
47.219541	1579.246636	19.144205
46.989257	1579.075451	19.149223
47.547267	1580.658820	19.154240
47.273265	1573.239020	19.159258
47.113788	1558.675158	19.164275
47.030916	1566.744382	19.169293
46.776892	1593.635755	19.174311
47.464883	1584.379618	19.179328
47.477099	1589.941307	19.184346
47.537670	1577.272139	19.189363
47.566648	1584.158460	19.194381
47.405556	1593.355453	19.199399
47.750048	1577.743446	19.204416
47.659881	1594.321554	19.209434
47.668380	1582.608514	19.214451
47.795878	1582.106388	19.219469
47.508154	1572.889263	19.224487
47.618217	1587.987793	19.229504
47.158800	1587.595053	19.234522
47.654685	1597.734150	19.239539
47.618620	1617.277209	19.244557
47.567483	1613.846673	19.249575
47.970318	1607.500897	19.254592
47.818609	1618.069228	19.259610
48.007079	1623.485479	19.264627
48.274540	1611.335181	19.269645
47.995778	1617.171119	19.274663
48.488472	1618.787527	19.279680
48.441235	1625.990559	19.284698
48.168789	1619.072587	19.289715
48.427916	1622.414406	19.294733
48.572069	1621.173784	19.299751
48.719860	1618.874808	19.304768
48.955108	1626.903895	19.309786
48.833688	1616.390707	19.314803
48.952232	1611.004796	19.319821
48.899932	1608.063570	19.324839
49.120070	1589.041592	19.329856
48.804959	1589.186751	19.334874
48.904698	1588.432155	19.339891
48.934335	1597.501975	19.344909
48.493009	1602.460939	19.349927
48.971522	1588.981642	19.354944
49.086597	1614.302195	19.359962
49.187279	1629.299769	19.364979
49.154115	1621.859632	19.369997
49.091131	1631.288636	19.375015
49.436994	1627.283891	19.380032
49.254137	1634.143238	19.385050
49.267232	1618.649134	19.390067
49.578407	1620.119180	19.395085
49.313063	1631.389487	19.400103
49.589187	1626.795744	19.405120
49.552800	1633.782838	19.410138
49.234714	1628.572998	19.415155
49.166687	1617.646898	19.420173
48.995861	1631.410550	19.425191
49.414167	1639.486550	19.430208
49.565049	1652.864027	19.435226
49.433117	1649.370859	19.440243
49.840867	1650.855851	19.445261
49.832682	1658.059137	19.450279
49.964645	1647.930780	19.455296
49.760268	1654.628751	19.460314
50.166917	1666.689315	19.465331
50.617104	1676.411653	19.470349
49.908370	1664.052000	19.475367
50.212495	1654.892519	19.480384
50.670280	1671.553174	19.485402
50.542451	1668.841126	19.490419
50.692549	1668.774977	19.495437
50.493706	1654.997954	19.500455
50.321110	1650.126229	19.505472
50.690648	1657.972923	19.510490
51.056373	1663.964553	19.515507
50.752586	1653.308857	19.520525
50.393060	1651.392298	19.525543
50.813944	1656.838454	19.530560
50.805843	1661.052300	19.535578
50.934704	1668.669116	19.540595
51.097519	1671.286393	19.545613
50.849077	1668.395873	19.550631
51.264773	1668.026021	19.555648
51.316237	1663.748888	19.560666
50.993249	1659.916267	19.565683
51.311169	1663.896930	19.570701
50.865830	1661.883932	19.575719
51.335580	1661.372485	19.580736
51.162385	1661.224736	19.585754
50.911470	1670.034891	19.590771
51.251211	1667.358559	19.595789
51.024756	1664.556522	19.600807
51.028640	1673.835147	19.605824
51.581961	1682.544299	19.610842
51.529538	1691.877510	19.615859
51.437348	1687.021617	19.620877
51.661748	1696.858436	19.625895
51.736254	1689.165265	19.630912
51.832834	1690.337745	19.635930
51.656914	1686.682368	19.640947
51.796827	1685.506804	19.645965
51.643784	1700.635538	19.650983
51.508032	1689.885128	19.656000
51.911012	1691.604548	19.661018
51.965996	1701.719536	19.666035
52.243954	1710.579313	19.671053
52.021322	1722.979709	19.676071
52.121975	1709.073628	19.681088
52.478233	1711.597929	19.686106
52.348118	1713.619791	19.691123
52.541912	1711.612970	19.696141
52.466181	1715.221539	19.701159
52.342920	1710.040099	19.706176
52.597690	1712.994905	19.711194
52.237710	1714.304834	19.716211
52.899379	1707.424764	19.721229
52.316109	1714.922692	19.726247
52.745826	1721.628496	19.731264
52.515014	1729.879518	19.736282
52.673563	1742.461403	19.741299
52.996473	1734.115219	19.746317
53.015013	1744.729904	19.751335
53.219376	1742.935877	19.756352
53.225028	1743.808854	19.761370
53.104310	1746.862719	19.766387
53.524047	1735.924037	19.771405
53.435601	1742.254303	19.776423
53.174507	1739.440852	19.781440
53.166571	1735.768726	19.786458
52.957301	1738.739399	19.791475
53.485453	1732.783647	19.796493
53.320864	1736.136263	19.801511
53.338913	1732.860195	19.806528
53.597327	1746.520345	19.811546
53.548669	1756.828067	19.816563
53.603317	1755.364061	19.821581
53.693965	1760.754010	19.826599
54.110660	1752.837547	19.831616
54.243408	1750.114311	19.836634
53.943466	1749.211997	19.841651
54.222068	1741.512039	19.846669
54.398461	1760.783189	19.851687
54.133004	1750.580099	19.856704
54.347981	1750.202867	19.861722
53.964929	1746.698816	19.866739
54.316105	1736.886502	19.871757
54.381691	1750.981430	19.876775
54.637690	1752.396047	19.881792
54.342359	1748.642880	19.886810
54.264312	1751.623560	19.891827
54.346033	1743.497522	19.896845
54.375147	1746.363456	19.901863
54.191081	1745.502421	19.906880
54.715825	1772.711628	19.911898
54.677258	1778.864590	19.916915
55.004338	1770.250796	19.921933
55.119838	1775.527994	19.926951
54.979412	1764.855657	19.931968
55.241033	1770.797020	19.936986
55.352251	1781.925495	19.942003
55.409814	1778.272651	19.947021
55.714716	1771.132447	19.952039
55.203620	1765.654878	19.957056
55.259792	1751.064844	19.962074
55.515750	1745.227484	19.967091
55.247330	1738.874086	19.972109
55.348985	1749.857480	19.977127
55.042906	1754.115080	19.982144
55.468210	1767.836442	19.987162
55.319282	1774.499123	19.992179
55.475403	1762.132878	19.997197
55.282613	1758.899322	20.002215
55.705445	1768.413467	20.007232
55.514980	1763.246854	20.012250
55.653148	1769.492642	20.017267
55.810660	1773.153223	20.022285
56.004235	1787.709858	20.027303
56.146156	1792.087513	20.032320
56.472301	1787.439005	20.037338
56.037397	1789.000665	20.042355
55.970758	1789.647820	20.047373
56.044718	1785.328948	20.052391
56.022815	1785.003456	20.057408
56.371679	1790.790070	20.062426
56.357819	1792.277038	20.067443
56.542640	1785.102148	20.072461
56.306024	1779.552449	20.077479
56.220039	1790.422603	20.082496
56.699987	1796.435761	20.087514
56.853908	1809.038935	20.092531
56.951877	1801.111737	20.097549
56.835896	1800.801594	20.102567
57.119297	1803.017510	20.107584
57.340658	1792.973685	20.112602
57.185429	1789.137914	20.117619
56.847815	1773.087891	20.122637
56.637650	1772.635652	20.127655
56.854710	1796.150863	20.132672
57.176134	1801.838877	20.137690
57.075141	1803.952189	20.142707
57.208233	1801.984321	20.147725
57.219714	1799.752327	20.152743
57.233689	1797.878152	20.157760
57.548279	1797.059306	20.162778
57.551981	1808.205960	20.167795
57.681932	1817.041639	20.172813
57.730998	1825.945015	20.177831
57.749551	1829.224282	20.182848
57.803432	1821.924768	20.187866
57.637517	1826.325351	20.192883
57.593651	1826.507176	20.197901
57.936525	1821.014641	20.202919
57.646373	1834.537589	20.207936
58.048338	1827.956261	20.212954
57.814552	1833.385478	20.217971
57.771264	1832.055747	20.222989
58.469585	1836.805007	20.228007
58.266162	1846.178224	20.233024
58.583982	1843.014194	20.238042
58.564296	1849.191227	20.243059
58.592763	1851.765584	20.248077
59.156826	1849.646581	20.253095
59.020037	1833.139731	20.258112
58.697184	1819.534612	20.263130
58.673200	1816.953788	20.268147
58.669770	1821.089355	20.273165
58.611994	1835.348628	20.278183
58.675881	1845.339417	20.283200
58.985795	1841.112628	20.288218
58.990120	1846.859356	20.293235
58.945625	1847.041089	20.298253
58.976339	1840.801982	20.303271
58.969524	1852.293678	20.308288
59.064065	1844.471738	20.313306
59.160867	1846.905091	20.318323
58.963390	1856.494239	20.323341
59.372466	1842.641785	20.328359
59.009324	1846.494512	20.333376
59.686489	1860.717984	20.338394
59.918927	1869.847160	20.343411
59.913951	1869.962133	20.348429
59.933956	1870.404244	20.353447
59.995715	1854.351719	20.358464
59.895136	1842.154784	20.363482
59.688645	1838.038327	20.368499
60.051644	1850.099164	20.373517
60.107046	1858.630092	20.378535
60.018000	1876.363518	20.383552
59.940234	1859.825628	20.388570
59.993371	1872.424841	20.393587
59.562691	1864.708774	20.398605
59.611113	1857.091279	20.403623
59.750595	1871.213669	20.408640
60.072075	1882.870015	20.413658
60.401860	1891.807939	20.418675
60.435549	1902.377124	20.423693
60.371601	1897.035638	20.428711
60.348049	1899.526876	20.433728
60.673784	1886.286326	20.438746
60.378990	1900.471844	20.443763
60.368082	1921.346830	20.448781
61.247605	1919.764216	20.453799
60.741697	1926.762303	20.458816
61.196708	1919.993055	20.463834
61.045045	1921.247909	20.468851
60.838861	1918.571990	20.473869
61.303632	1902.105805	20.478887
61.061677	1914.815424	20.483904
61.259746	1912.710834	20.488922
61.292078	1922.791327	20.493939
61.588073	1929.161282	20.498957
62.013838	1938.074712	20.503975
61.345412	1928.515990	20.508992
61.640680	1920.716742	20.514010
62.043262	1938.031433	20.519027
61.757452	1933.511561	20.524045
61.828716	1935.509032	20.529063
61.882806	1943.485158	20.534080
62.259982	1938.845100	20.539098
62.078313	1934.020054	20.544115
62.240718	1943.320084	20.549133
62.381446	1932.652151	20.554151
62.187642	1939.850812	20.559168
62.448378	1934.743821	20.564186
62.475713	1925.672238	20.569203
62.516166	1929.174657	20.574221
62.879563	1930.461122	20.579239
62.379118	1936.492261	20.584256
62.551614	1937.503017	20.589274
62.676320	1925.339846	20.594291
62.505901	1935.284379	20.599309
62.627814	1922.263485	20.604327
62.540937	1930.981138	20.609344
62.624970	1931.131398	20.614362
62.611293	1932.658305	20.619379
62.936788	1931.559330	20.624397
62.826243	1921.414573	20.629415
62.789110	1946.073094	20.634432
62.997581	1950.481132	20.639450
63.045090	1960.156621	20.644467
62.964381	1952.846414	20.649485
63.414848	1948.836308	20.654503
63.230393	1962.865475	20.659520
62.950954	1959.189347	20.664538
63.044464	1965.978568	20.669555
63.444292	1978.244424	20.674573
64.241296	1973.180486	20.679591
64.117239	1965.055268	20.684608
64.452622	1954.387434	20.689626
64.523626	1938.008717	20.694643
64.199678	1940.999559	20.699661
64.523340	1931.228672	20.704679
64.461249	1925.298539	20.709696
64.306265	1921.398920	20.714714
64.404310	1927.362651	20.719731
64.206980	1928.446722	20.724749
64.639868	1916.396593	20.729767
64.228557	1939.127164	20.734784
64.210565	1930.329381	20.739802
64.650900	1917.494236	20.744819
64.296688	1934.205113	20.749837
64.391459	1918.723782	20.754855
64.470057	1934.426418	20.759872
64.487890	1945.159654	20.764890
64.864366	1953.362211	20.769907
64.542230	1955.514842	20.774925
64.464455	1950.439967	20.779943
64.627206	1967.174498	20.784960
64.392445	1966.748362	20.789978
64.985194	1976.874264	20.794995
65.123723	1989.584649	20.800013
65.269358	1984.848205	20.805031
65.549265	1987.925278	20.810048
65.377134	1992.823150	20.815066
65.481850	1991.543941	20.820083
65.425978	1984.462468	20.825101
65.465654	1984.053575	20.830119
65.738673	1983.887986	20.835136
65.604180	1987.754731	20.840154
65.752878	1982.194431	20.845171
65.494339	1999.022430	20.850189
65.693286	2008.004284	20.855207
65.908767	2013.567771	20.860224
65.722657	2019.283440	20.865242
65.840466	2018.211692	20.870259
65.813021	2025.643706	20.875277
65.951671	2018.765289	20.880295
66.486523	2031.036432	20.885312
66.095504	2042.104792	20.890330
66.545733	2042.922431	20.895347
66.353773	2045.728897	20.900365
66.535411	2036.394764	20.905383
66.646889	2042.051227	20.910400
66.715639	2049.451611	20.915418
66.774337	2037.403187	20.920435
66.564286	2048.212337	20.925453
66.481057	2054.581236	20.930471
66.895396	2067.145133	20.935488
66.879681	2079.395884	20.940506
67.403126	2073.002827	20.945523
67.279603	2072.973231	20.950541
67.476366	2063.630480	20.955559
67.550664	2072.488493	20.960576
67.460000	2071.032329	20.965594
67.574243	2062.956454	20.970611
67.543270	2068.098914	20.975629
67.622691	2066.332386	20.980647
67.393049	2068.325271	20.985664
67.658243	2074.929098	20.990682
67.481334	2065.429017	20.995699
67.566841	2060.484985	21.000717
67.748188	2057.002155	21.005735
68.005035	2071.800354	21.010752
68.220019	2076.212863	21.015770
68.239109	2075.179864	21.020787
68.084135	2090.031763	21.025805
68.141190	2083.971850	21.030823
68.210066	2078.457381	21.035840
68.365876	2084.077600	21.040858
68.226234	2094.471442	21.045875
68.469104	2095.766225	21.050893
68.365902	2080.535735	21.055911
68.590203	2090.876915	21.060928
68.437796	2090.702695	21.065946
68.574213	2102.801369	21.070963
68.866918	2105.904301	21.075981
68.576100	2108.636374	21.080999
68.755352	2115.329020	21.086016
68.744292	2113.843951	21.091034
68.827603	2102.683658	21.096051
68.755728	2105.530129	21.101069
68.612771	2117.444093	21.106087
69.075400	2123.027995	21.111104
69.418876	2144.020692	21.116122
69.869731	2130.858069	21.121139
69.990461	2132.044308	21.126157
69.878015	2124.456020	21.131175
70.008664	2117.613720	21.136192
70.090677	2125.283383	21.141210
70.313355	2112.953493	21.146227
70.085432	2115.199623	21.151245
70.019857	2110.408089	21.156263
70.328200	2108.593886	21.161280
70.208402	2109.597841	21.166298
70.230895	2112.635592	21.171315
70.210594	2103.835730	21.176333
70.501315	2110.902834	21.181351
70.620106	2101.665850	21.186368
70.724912	2106.618578	21.191386
70.733495	2108.778976	21.196403
70.630232	2108.274615	21.201421
70.681156	2103.233930	21.206439
71.072295	2096.240140	21.211456
70.951277	2106.409869	21.216474
71.104771	2097.408865	21.221491
70.556899	2096.673471	21.226509
70.798593	2089.575059	21.231527
71.031146	2090.917999	21.236544
70.952948	2123.705545	21.241562
71.111377	2126.317917	21.246579
71.183663	2136.636614	21.251597
71.306562	2129.766458	21.256615
71.340973	2122.383019	21.261632
71.356479	2124.236592	21.266650
71.518982	2123.857788	21.271667
71.216697	2134.729677	21.276685
71.323095	2141.407209	21.281703
72.142516	2141.570785	21.286720
71.997461	2152.206486	21.291738
72.226256	2156.065008	21.296755
71.840733	2149.239885	21.301773
71.941032	2152.432096	21.306791
71.968983	2148.154975	21.311808
72.282079	2160.144584	21.316826
72.088338	2149.731163	21.321843
72.295802	2148.046609	21.326861
71.899876	2159.529020	21.331879
72.319698	2162.851294	21.336896
72.325981	2188.542709	21.341914
72.666849	2187.406731	21.346931
73.239541	2179.923293	21.351949
72.732020	2182.945302	21.356967
73.404693	2179.562541	21.361984
73.237695	2178.263260	21.367002
73.527099	2177.789869	21.372019
73.433370	2174.291252	21.377037
73.027082	2173.152370	21.382055
73.247261	2172.568381	21.387072
73.174722	2173.235816	21.392090
73.205462	2177.778791	21.397107
73.439495	2172.430289	21.402125
73.208262	2173.321176	21.407143
73.335334	2175.403347	21.412160
73.485679	2183.267440	21.417178
73.366642	2175.797135	21.422195
73.562533	2184.650867	21.427213
73.482671	2202.776624	21.432231
73.846832	2199.123407	21.437248
73.710607	2200.832389	21.442266
73.885636	2193.887455	21.447283
74.129483	2207.715764	21.452301
74.053662	2222.263395	21.457319
74.428300	2231.056714	21.462336
74.656571	2236.986645	21.467354
74.785055	2220.067068	21.472371
74.934454	2216.639872	21.477389
75.196944	2219.405130	21.482407
75.206549	2212.062949	21.487424
75.014310	2207.959390	21.492442
74.786121	2192.463441	21.497459
75.095531	2205.589827	21.502477
74.885869	2201.795424	21.507495
75.283062	2205.688333	21.512512
74.868872	2220.969579	21.517530
74.824860	2219.777325	21.522547
75.212217	2219.164528	21.527565
74.659284	2217.802845	21.532583
75.200227	2217.389849	21.537600
75.287870	2239.442984	21.542618
75.147097	2250.267597	21.547635
75.257306	2245.129478	21.552653
75.018768	2252.313040	21.557671
75.703426	2255.603382	21.562688
75.539101	2274.113034	21.567706
75.681478	2279.735151	21.572723
76.033185	2279.367595	21.577741
75.909862	2278.706908	21.582759
75.976986	2291.441742	21.587776
76.101973	2296.684876	21.592794
76.451320	2295.760270	21.597811
76.738543	2296.691467	21.602829
76.614723	2294.554785	21.607847
76.928887	2301.756874	21.612864
76.858428	2299.271241	21.617882
77.016316	2293.801824	21.622899
77.022489	2290.386666	21.627917
76.792923	2300.199878	21.632935
76.987804	2294.045263	21.637952
76.999966	2295.238039	21.642970
77.084958	2291.717343	21.647987
77.298607	2285.126196	21.653005
77.238360	2284.985560	21.658023
77.513912	2292.783156	21.663040
77.698800	2288.087571	21.668058
77.279200	2286.421586	21.673075
77.465500	2279.268073	21.678093
77.351095	2296.912085	21.683111
77.651732	2305.839320	21.688128
77.594941	2319.869367	21.693146
77.570436	2322.209463	21.698163
77.930816	2316.662880	21.703181
77.746267	2320.630098	21.708199
77.766195	2306.238428	21.713216
78.153259	2324.534988	21.718234
78.509012	2338.092579	21.723251
78.787105	2334.725188	21.728269
78.527369	2326.291513	21.733287
78.618797	2330.522164	21.738304
78.742088	2332.929565	21.743322
78.689407	2337.233634	21.748339
78.808726	2341.203988	21.753357
78.635342	2337.798412	21.758375
79.011762	2337.861782	21.763392
78.928508	2331.851530	21.768410
79.097458	2329.352117	21.773427
78.987309	2326.863983	21.778445
78.854667	2334.273177	21.783463
79.042592	2329.433978	21.788480
79.086116	2348.017633	21.793498
79.152454	2353.672616	21.798515
79.172143	2357.143724	21.803533
79.478718	2365.350769	21.808551
79.350167	2359.244062	21.813568
79.265979	2363.557478	21.818586
79.668185	2385.325787	21.823603
80.169583	2388.217926	21.828621
80.041765	2396.589676	21.833639
80.241505	2390.395246	21.838656
80.376011	2383.767729	21.843674
80.410880	2385.556721	21.848691
80.614449	2375.471367	21.853709
80.404331	2389.220730	21.858727
80.407119	2386.479491	21.863744
80.567584	2382.521134	21.868762
80.493030	2382.736578	21.873779
80.850821	2389.394920	21.878797
80.738201	2409.420894	21.883815
81.103408	2408.662547	21.888832
81.089958	2417.480341	21.893850
80.848351	2422.619539	21.898867
81.265715	2403.291151	21.903885
80.765183	2402.051493	21.908903
80.984258	2407.927501	21.913920
80.907455	2411.550581	21.918938
80.958098	2428.895440	21.923955
81.431233	2430.705317	21.928973
81.324508	2430.662315	21.933991
81.482813	2430.613311	21.939008
81.899401	2435.374083	21.944026
81.758349	2458.067645	21.949043
82.153848	2452.780550	21.954061
82.418314	2460.843039	21.959079
82.581565	2445.982701	21.964096
82.817229	2446.774799	21.969114
82.464257	2438.639129	21.974131
82.646650	2413.232218	21.979149
82.364051	2420.976056	21.984167
82.147348	2426.242628	21.989184
82.417286	2438.423235	21.994202
82.385773	2444.061549	21.999219
82.669628	2445.974748	22.004237
82.446523	2448.851193	22.009255
82.576323	2463.992594	22.014272
82.659751	2458.074035	22.019290
82.885919	2466.253479	22.024307
82.964203	2475.765554	22.029325
83.152870	2475.854438	22.034343
83.182740	2487.764930	22.039360
83.494621	2481.262974	22.044378
83.254302	2466.943684	22.049395
83.619242	2465.008284	22.054413
83.356854	2473.625921	22.059431
83.405043	2497.873216	22.064448
83.858804	2501.682646	22.069466
83.770068	2503.338541	22.074483
84.351571	2496.880997	22.079501
84.062087	2503.914637	22.084519
84.118769	2510.521022	22.089536
84.157073	2508.698249	22.094554
84.337792	2503.330493	22.099571
84.334531	2503.072767	22.104589
84.639791	2512.652077	22.109607
84.575914	2525.960688	22.114624
84.718906	2526.527173	22.119642
84.664851	2526.862846	22.124659
84.751697	2519.586688	22.129677
84.822769	2518.071080	22.134695
84.913651	2530.452992	22.139712
84.953184	2517.221995	22.144730
85.136084	2525.097614	22.149747
84.652588	2534.301002	22.154765
85.429060	2548.729363	22.159783
85.323073	2555.202026	22.164800
85.679016	2550.038750	22.169818
85.589974	2556.610970	22.174835
85.939182	2543.198865	22.179853
86.042494	2549.794412	22.184871
85.845655	2548.186071	22.189888
86.104378	2547.457124	22.194906
85.904301	2546.617781	22.199923
86.164579	2542.580491	22.204941
85.732535	2556.870387	22.209959
85.750406	2572.007556	22.214976
86.420558	2569.342612	22.219994
85.918918	2580.576477	22.225011
86.002028	2577.368412	22.230029
86.606846	2591.600781	22.235047
87.125264	2587.828289	22.240064
87.689782	2581.349896	22.245082
87.682428	2593.341026	22.250099
87.801265	2578.323341	22.255117
87.437079	2552.797476	22.260135
87.571408	2550.582079	22.265152
87.834135	2537.109076	22.270170
87.441288	2542.280391	22.275187
87.696601	2538.768697	22.280205
87.777566	2540.085154	22.285223
87.496217	2550.057861	22.290240
87.536558	2541.649281	22.295258
87.627168	2547.445002	22.300275
87.668567	2550.797808	22.305293
87.767667	2573.640036	22.310311
87.927573	2576.266217	22.315328
88.121997	2567.960108	22.320346
87.691812	2586.745548	22.325363
88.045031	2576.490855	22.330381
88.163119	2596.656498	22.335399
88.082018	2604.876553	22.340416
88.504295	2608.998677	22.345434
88.499408	2609.931709	22.350451
88.602588	2607.500597	22.355469
88.309886	2602.216940	22.360487
88.331542	2611.936478	22.365504
88.940823	2626.420097	22.370522
88.735090	2645.601963	22.375539
89.226950	2647.712302	22.380557
89.189502	2629.567002	22.385575
88.888996	2630.058356	22.390592
89.127709	2627.516661	22.395610
88.947323	2647.750194	22.400627
89.435102	2648.090033	22.405645
89.529567	2658.228651	22.410663
89.732344	2652.543039	22.415680
89.685537	2650.486294	22.420698
89.472265	2666.769965	22.425715
90.248278	2681.928415	22.430733
90.597729	2681.526581	22.435751
90.536324	2692.042141	22.440768
90.649841	2676.178823	22.445786
90.684143	2679.785181	22.450803
90.905580	2687.195875	22.455821
90.727529	2688.932293	22.460839
90.720975	2682.845848	22.465856
91.214645	2682.222554	22.470874
90.685809	2684.045675	22.475891
90.973418	2680.928201	22.480909
91.018835	2681.058473	22.485927
90.910774	2688.122845	22.490944
91.396022	2674.168486	22.495962
91.436546	2684.895535	22.500979
91.224404	2678.461190	22.505997
91.669414	2679.015962	22.511015
91.487994	2692.857502	22.516032
91.443477	2695.284816	22.521050
91.876155	2699.889082	22.526067
91.743830	2702.667112	22.531085
92.028721	2698.579260	22.536103
91.812594	2701.683328	22.541120
91.881102	2707.239858	22.546138
92.137741	2718.274511	22.551155
92.075933	2724.626957	22.556173
92.341071	2722.149775	22.561191
92.659871	2725.555596	22.566208
92.754580	2718.143799	22.571226
92.909820	2723.711199	22.576243
92.647884	2726.849218	22.581261
92.634647	2723.569646	22.586279
92.965457	2746.964761	22.591296
93.194130	2750.097697	22.596314
93.009983	2760.113529	22.601331
92.947517	2756.006685	22.606349
92.977817	2750.403473	22.611367
93.224695	2753.637728	22.616384
93.499998	2758.989641	22.621402
93.945315	2765.136263	22.626419
93.946185	2774.847921	22.631437
94.105405	2765.157422	22.636455
94.212086	2772.065881	22.641472
94.324077	2762.656012	22.646490
94.835438	2761.657367	22.651507
94.351183	2764.967951	22.656525
94.590643	2755.577966	22.661543
94.607727	2766.180603	22.666560
94.723864	2768.945540	22.671578
94.623069	2762.132933	22.676595
94.661824	2753.265858	22.681613
94.869749	2748.699000	22.686631
94.138783	2755.093923	22.691648
94.664742	2754.570012	22.696666
94.536187	2752.585813	22.701683
94.789672	2766.815379	22.706701
95.002442	2772.091806	22.711719
94.975341	2781.543140	22.716736
95.418265	2781.137669	22.721754
95.404657	2776.827872	22.726771
95.467531	2779.786251	22.731789
95.724593	2773.960134	22.736807
95.405368	2798.977640	22.741824
95.701002	2796.125343	22.746842
96.147246	2798.012148	22.751859
96.197951	2804.770428	22.756877
96.056232	2801.409711	22.761895
95.935293	2798.387281	22.766912
96.203187	2792.060961	22.771930
96.240967	2813.947572	22.776947
96.244867	2828.297960	22.781965
96.389986	2825.338250	22.786983
96.550834	2832.276760	22.792000
96.545545	2828.410046	22.797018
96.846836	2854.539237	22.802035
97.137836	2849.164555	22.807053
97.386228	2851.705692	22.812071
97.432600	2859.620971	22.817088
97.514662	2854.828431	22.822106
97.816224	2855.410457	22.827123
97.228502	2856.047305	22.832141
97.562990	2852.882682	22.837159
97.729693	2848.724561	22.842176
97.604681	2844.870146	22.847194
97.839582	2851.623994	22.852211
97.764531	2878.355943	22.857229
98.372273	2873.269061	22.862247
98.080317	2882.738632	22.867264
98.086746	2878.300303	22.872282
98.353040	2882.677402	22.877299
98.315184	2880.738435	22.882317
98.900984	2890.124779	22.887335
98.539227	2889.199930	22.892352
98.996793	2890.491983	22.897370
98.948322	2888.724447	22.902387
99.211958	2895.858987	22.907405
99.182380	2897.924032	22.912423
99.271157	2898.870738	22.917440
99.515681	2891.683701	22.922458
99.187353	2887.841612	22.927475
99.049973	2898.269083	22.932493
99.368248	2899.945164	22.937511
99.386586	2913.740901	22.942528
99.604877	2920.843576	22.947546
99.701674	2912.184529	22.952563
99.653035	2922.128075	22.957581
100.307430	2929.102394	22.962599
100.216190	2947.903915	22.967616
99.952566	2958.355435	22.972634
100.636656	2950.890231	22.977651
100.568658	2958.660684	22.982669
100.566061	2947.531891	22.987687
100.773262	2943.435948	22.992704
100.584426	2952.269642	22.997722
100.865467	2962.950055	23.002739
100.938455	2975.408113	23.007757
101.564525	2965.799791	23.012775
101.640718	2964.810445	23.017792
101.679144	2965.035967	23.022810
101.732403	2964.109464	23.027827
101.530099	2969.161246	23.032845
102.081162	2960.549941	23.037863
102.074938	2964.781155	23.042880
101.816609	2957.023654	23.047898
101.919174	2956.810243	23.052915
101.586796	2967.689261	23.057933
101.836335	2961.183628	23.062951
101.816593	2965.848166	23.067968
101.652736	2964.200474	23.072986
102.042738	2975.905381	23.078003
101.884995	2993.316802	23.083021
102.325441	2986.192227	23.088039
102.271005	2991.234543	23.093056
102.821930	3007.020258	23.098074
103.080081	3013.564828	23.103091
102.939308	3015.444331	23.108109
103.238079	3014.222932	23.113127
103.136815	3010.340143	23.118144
103.074609	3008.061885	23.123162
103.548070	3010.746168	23.128179
103.387101	3030.815579	23.133197
103.700904	3025.277624	23.138215
103.758405	3037.972932	23.143232
103.906549	3040.942073	23.148250
103.991522	3046.063338	23.153267
103.766479	3046.422158	23.158285
103.538380	3037.089972	23.163303
104.018854	3045.382030	23.168320
104.138741	3071.116374	23.173338
104.611767	3069.372881	23.178355
104.342363	3073.933826	23.183373
104.722011	3065.695269	23.188391
104.773715	3058.214827	23.193408
104.889876	3078.138508	23.198426
105.166164	3097.623166	23.203443
105.242966	3096.986459	23.208461
105.801783	3091.921765	23.213479
105.310477	3090.271868	23.218496
105.432568	3084.027396	23.223514
105.706657	3082.977783	23.228531
105.469453	3091.573884	23.233549
105.508966	3082.834445	23.238567
105.931420	3079.755240	23.243584
105.701441	3090.769783	23.248602
106.160748	3106.956558	23.253619
106.108864	3109.084765	23.258637
106.293517	3114.977362	23.263655
106.375429	3117.420071	23.268672
106.247887	3120.570212	23.273690
106.533245	3112.632245	23.278707
106.074914	3127.211254	23.283725
106.548962	3132.838719	23.288743
106.875601	3128.548192	23.293760
106.810502	3141.469351	23.298778
107.295047	3133.423658	23.303795
107.283534	3141.214396	23.308813
107.378945	3151.845299	23.313831
107.624326	3149.742962	23.318848
107.525745	3162.157868	23.323866
107.855724	3160.765162	23.328883
108.189151	3153.830240	23.333901
108.293039	3159.256679	23.338919
108.236820	3152.677082	23.343936
107.839292	3158.502511	23.348954
108.339692	3151.260476	23.353971
108.076375	3156.136576	23.358989
108.129406	3155.557732	23.364007
108.188789	3160.949007	23.369024
108.182068	3176.117207	23.374042
108.406683	3171.110860	23.379059
108.706009	3184.340337	23.384077
108.581980	3183.757284	23.389095
108.443403	3195.668990	23.394112
108.410999	3215.380392	23.399130
108.784350	3214.469485	23.404147
108.826987	3222.637532	23.409165
108.783728	3233.973681	23.414183
109.155624	3243.223935	23.419200
108.926151	3264.923062	23.424218
109.599083	3269.965357	23.429235
109.642267	3274.441639	23.434253
110.184742	3264.880019	23.439271
110.343643	3262.378575	23.444288
110.163721	3257.690618	23.449306
110.680757	3244.666315	23.454323
110.795822	3258.620390	23.459341
110.502991	3256.652248	23.464359
110.906900	3272.142845	23.469376
110.913501	3286.858168	23.474394
110.684198	3281.244118	23.479411
110.920676	3289.456548	23.484429
111.189459	3283.411771	23.489447
111.311222	3288.809319	23.494464
111.077145	3290.746791	23.499482
111.302930	3298.612176	23.504499
111.515677	3314.458023	23.509517
111.928101	3313.231995	23.514535
112.140669	3311.846079	23.519552
111.937555	3318.107550	23.524570
112.237692	3312.295769	23.529587
111.994880	3311.235098	23.534605
112.233860	3314.068417	23.539623
112.476082	3309.126045	23.544640
112.422645	3313.921846	23.549658
112.452518	3329.975878	23.554675
112.711224	3336.018920	23.559693
112.771265	3338.188507	23.564711
112.709875	3337.530925	23.569728
112.577430	3346.513005	23.574746
112.802823	3357.840285	23.579763
112.886019	3367.570207	23.584781
112.380544	3374.627724	23.589799
112.822475	3371.025560	23.594816
113.034410	3388.422795	23.599834
113.517167	3397.434744	23.604851
113.786462	3409.079611	23.609869
114.018220	3417.766118	23.614887
114.458723	3415.378749	23.619904
114.500988	3411.065843	23.624922
114.696399	3400.354794	23.629939
114.698998	3402.356323	23.634957
114.932532	3410.900406	23.639975
114.944221	3401.995307	23.644992
115.026620	3398.613962	23.650010
115.404166	3396.461802	23.655027
115.186310	3398.636371	23.660045
115.303864	3406.914577	23.665063
115.644190	3403.870927	23.670080
115.684314	3398.346960	23.675098
115.777865	3389.208263	23.680115
115.921095	3382.134982	23.685133
115.748976	3386.618526	23.690151
116.162941	3389.439087	23.695168
116.247469	3385.060543	23.700186
116.417506	3381.927319	23.705203
116.235601	3384.369568	23.710221
115.848671	3384.291759	23.715239
116.252951	3376.008024	23.720256
115.968287	3385.520789	23.725274
115.806369	3398.098317	23.730291
116.352991	3408.381611	23.735309
115.908664	3412.841638	23.740327
116.494927	3430.214469	23.745344
116.370013	3445.921756	23.750362
116.858741	3449.720923	23.755379
116.755376	3463.648676	23.760397
117.099689	3464.433507	23.765415
117.467918	3476.087274	23.770432
117.375988	3486.372589	23.775450
117.522649	3480.468389	23.780467
118.009314	3485.171454	23.785485
117.868419	3497.401886	23.790503
117.998225	3498.258384	23.795520
118.070295	3502.572477	23.800538
118.128972	3498.855658	23.805555
118.572813	3500.973661	23.810573
118.345642	3513.437654	23.815591
118.758974	3515.635110	23.820608
118.817417	3531.686599	23.825626
118.800731	3543.495358	23.830643
118.893714	3530.763330	23.835661
118.818707	3537.686798	23.840679
119.335211	3543.332204	23.845696
119.272737	3553.862304	23.850714
119.434395	3554.198183	23.855731
119.563671	3551.722060	23.860749
119.403572	3555.810749	23.865767
119.674874	3559.654926	23.870784
120.146070	3572.211447	23.875802
120.099396	3575.986907	23.880819
120.346120	3572.832706	23.885837
120.546133	3582.848582	23.890855
120.687389	3570.815247	23.895872
120.372619	3579.783492	23.900890
120.513584	3583.150386	23.905907
120.727899	3594.411165	23.910925
120.966842	3611.960097	23.915943
120.858509	3605.721206	23.920960
120.871764	3610.674191	23.925978
120.930102	3623.067079	23.930995
121.066459	3633.096655	23.936013
121.241803	3632.751130	23.941031
121.414542	3637.943916	23.946048
121.609809	3656.424932	23.951066
122.069300	3666.355467	23.956083
122.146349	3658.354791	23.961101
122.286158	3659.019879	23.966119
122.449718	3650.113952	23.971136
122.349408	3660.999596	23.976154
122.312805	3678.794923	23.981171
122.713178	3685.685183	23.986189
122.949654	3680.242060	23.991207
123.131593	3682.636440	23.996224
123.454935	3672.250923	24.001242
123.291844	3677.684650	24.006259
123.703083	3668.114155	24.011277
123.510836	3661.070589	24.016295
123.870049	3662.535265	24.021312
124.068330	3665.315924	24.026330
123.897813	3681.682177	24.031347
124.051481	3662.940297	24.036365
123.926774	3660.502976	24.041383
124.307862	3665.108973	24.046400
124.249543	3688.118621	24.051418
124.032356	3692.445129	24.056435
124.500458	3689.974418	24.061453
124.148106	3694.448066	24.066471
124.431658	3695.020505	24.071488
124.450838	3703.090710	24.076506
124.725855	3730.600551	24.081523
124.771958	3715.383546	24.086541
125.268532	3727.065509	24.091559
125.350074	3721.172765	24.096576
125.360170	3740.459691	24.101594
125.292298	3749.935675	24.106611
125.334115	3747.896424	24.111629
125.194027	3757.939082	24.116647
125.590968	3760.491259	24.121664
125.929000	3780.370126	24.126682
125.991233	3782.408308	24.131699
126.213120	3781.253494	24.136717
126.280209	3795.666384	24.141735
126.897309	3799.793649	24.146752
127.107897	3801.437625	24.151770
127.056266	3792.352209	24.156787
127.311262	3789.093839	24.161805
127.479794	3802.579714	24.166823
127.692264	3790.234435	24.171840
127.735097	3793.976260	24.176858
127.867096	3785.156576	24.181875
127.744383	3791.787245	24.186893
127.752130	3797.129791	24.191911
127.809994	3797.194630	24.196928
128.394017	3799.885985	24.201946
128.217216	3813.989970	24.206963
128.475979	3804.390647	24.211981
128.382248	3819.624642	24.216999
128.573142	3818.964331	24.222016
128.851518	3812.114200	24.227034
128.368881	3816.959420	24.232051
128.639912	3819.645802	24.237069
129.264902	3835.384693	24.242087
129.154082	3844.045366	24.247104
129.556160	3849.013316	24.252122
129.152543	3843.616845	24.257139
129.637042	3838.286232	24.262157
129.855119	3855.960545	24.267175
129.833484	3857.442105	24.272192
129.933613	3862.220967	24.277210
129.957616	3865.530082	24.282227
130.344679	3856.011893	24.287245
130.041147	3867.341508	24.292263
130.424218	3877.557650	24.297280
130.818262	3888.337357	24.302298
130.870053	3891.876539	24.307315
130.976345	3891.136894	24.312333
130.734111	3892.341905	24.317351
131.030845	3900.649432	24.322368
131.000643	3906.518382	24.327386
131.130068	3920.380913	24.332403
131.492221	3919.644266	24.337421
131.429136	3925.363927	24.342439
131.715176	3935.873709	24.347456
132.452744	3928.424013	24.352474
132.238906	3929.571184	24.357491
132.714254	3929.525307	24.362509
132.579637	3936.682038	24.367527
132.578214	3923.133763	24.372544
132.768950	3918.264276	24.377562
132.267601	3931.391250	24.382579
132.809426	3923.882952	24.387597
132.770726	3941.034810	24.392615
132.633270	3961.403121	24.397632
132.831727	3956.294543	24.402650
132.837671	3966.597074	24.407667
133.048848	3966.405470	24.412685
133.220981	3990.677929	24.417703
133.409319	3995.171774	24.422720
133.636989	3984.315619	24.427738
133.949660	4011.453187	24.432755
133.918976	4017.732512	24.437773
133.957443	4028.092704	24.442791
134.248889	4014.821562	24.447808
134.463070	4015.810611	24.452826
134.525457	4035.125877	24.457843
134.530394	4035.177414	24.462861
134.745328	4043.620193	24.467879
134.612280	4049.032154	24.472896
135.029089	4066.077387	24.477914
134.860367	4070.476309	24.482931
135.369237	4067.395235	24.487949
135.652649	4084.443631	24.492967
135.760289	4092.487216	24.497984
136.093502	4085.643261	24.503002
135.662340	4094.584179	24.508019
136.058621	4089.898009	24.513037
136.560762	4110.705738	24.518055
136.311149	4115.757439	24.523072
136.565744	4111.856126	24.528090
136.602735	4116.814011	24.533107
136.843109	4118.226711	24.538125
137.102781	4125.731784	24.543143
137.172824	4132.493353	24.548160
137.660910	4131.631947	24.553178
137.846204	4131.834007	24.558195
137.906743	4126.259556	24.563213
137.884974	4129.534162	24.568231
137.915242	4136.722010	24.573248
138.232620	4121.410569	24.578266
138.040464	4116.113320	24.583283
137.640547	4120.992997	24.588301
138.298756	4152.022720	24.593319
138.078492	4156.210487	24.598336
138.627827	4151.354908	24.603354
138.342647	4168.913903	24.608371
138.899150	4176.754225	24.613389
139.378956	4181.760623	24.618407
139.134188	4189.650273	24.623424
139.432990	4189.756015	24.628442
139.309929	4215.681226	24.633459
139.599635	4215.244742	24.638477
139.726719	4218.978654	24.643495
139.893186	4222.882448	24.648512
140.153158	4222.936729	24.653530
140.427255	4245.517058	24.658547
140.450931	4237.230400	24.663565
140.719658	4233.569255	24.668583
140.491525	4246.172975	24.673600
140.514746	4242.075990	24.678618
140.427622	4255.567492	24.683635
140.960151	4262.182223	24.688653
141.384860	4274.922597	24.693671
141.500105	4273.677884	24.698688
141.592342	4270.371501	24.703706
141.588318	4283.682358	24.708723
141.795127	4280.258611	24.713741
142.211071	4291.320430	24.718759
141.603739	4299.466117	24.723776
142.202052	4288.538272	24.728794
142.345431	4303.235895	24.733811
142.391760	4305.826411	24.738829
142.220489	4300.069716	24.743847
142.366582	4320.523935	24.748864
142.635957	4312.385234	24.753882
142.897790	4328.726004	24.758899
142.781542	4332.865921	24.763917
143.147159	4343.791203	24.768935
143.157018	4340.523221	24.773952
143.241765	4349.521962	24.778970
143.216061	4356.210861	24.783987
143.561432	4368.846304	24.789005
144.055161	4381.108403	24.794023
144.016931	4371.443232	24.799040
144.490337	4362.614845	24.804058
144.706536	4379.665615	24.809075
144.717784	4382.887965	24.814093
145.018123	4386.409421	24.819111
145.213839	4395.979260	24.824128
145.288828	4387.614354	24.829146
145.567704	4390.871624	24.834163
145.156935	4387.974728	24.839181
145.363631	4383.773369	24.844199
145.376238	4389.393680	24.849216
145.794311	4407.112350	24.854234
145.905107	4424.709360	24.859251
145.697699	4418.314061	24.864269
145.995085	4411.671566	24.869287
146.095172	4430.534215	24.874304
146.313202	4439.401528	24.879322
146.293718	4447.806483	24.884339
146.174459	4458.096954	24.889357
146.654398	4468.026989	24.894375
146.659421	4473.679688	24.899392
146.990503	4478.373726	24.904410
147.388726	4491.476947	24.909427
147.175942	4497.364082	24.914445
147.864151	4495.413612	24.919463
147.557597	4503.314023	24.924480
147.914233	4512.584491	24.929498
148.140009	4521.816346	24.934515
148.202510	4520.277156	24.939533
148.565462	4523.482370	24.944551
148.850666	4536.576349	24.949568
149.021353	4542.376910	24.954586
149.166366	4546.332759	24.959603
149.157640	4548.304807	24.964621
149.713905	4553.380196	24.969639
149.667193	4544.786477	24.974656
149.955087	4539.803099	24.979674
149.682700	4542.404582	24.984691
149.718852	4532.723871	24.989709
150.280891	4537.328581	24.994727
149.967331	4541.514542	24.999744
150.157136	4548.271071	25.004762
150.248339	4564.683594	25.009779
149.807452	4568.566560	25.014797
150.213813	4567.759979	25.019815
150.358299	4595.752796	25.024832
150.587019	4604.985001	25.029850
151.045210	4608.415460	25.034867
151.133866	4618.181880	25.039885
151.311056	4618.588452	25.044903
150.942847	4631.084908	25.049920
151.311173	4640.161773	25.054938
151.661406	4652.143836	25.059955
151.947061	4657.241136	25.064973
152.042105	4651.600555	25.069991
152.392935	4661.087837	25.075008
153.073378	4665.843114	25.080026
153.139438	4662.735084	25.085043
153.258808	4675.945960	25.090061
153.415037	4649.861319	25.095079
153.235352	4643.466465	25.100096
153.452584	4638.597102	25.105114
153.660077	4657.397393	25.110131
153.386598	4662.599680	25.115149
154.109906	4659.713789	25.120167
153.927713	4657.754743	25.125184
154.059335	4646.035976	25.130202
154.102531	4661.653713	25.135219
153.946116	4666.477968	25.140237
154.559392	4669.235913	25.145255
154.134136	4683.798305	25.150272
154.379627	4685.454721	25.155290
154.364417	4692.158173	25.160307
154.556554	4728.496416	25.165325
154.453799	4726.823474	25.170343
154.827223	4742.513116	25.175360
154.999593	4748.320956	25.180378
155.156662	4757.256009	25.185395
155.225238	4777.076729	25.190413
156.023527	4779.652930	25.195431
155.973543	4785.883385	25.200448
156.203667	4796.501817	25.205466
156.476526	4802.219051	25.210483
156.411459	4803.606293	25.215501
156.783885	4802.670650	25.220519
157.140459	4829.254309	25.225536
157.031018	4831.980504	25.230554
157.374864	4824.688761	25.235571
157.489118	4820.825031	25.240589
157.735844	4814.568724	25.245607
157.592256	4838.470222	25.250624
157.438659	4853.026077	25.255642
158.266485	4859.252478	25.260659
157.976548	4853.725834	25.265677
158.260321	4866.787254	25.270695
158.570476	4876.165629	25.275712
158.505806	4883.634888	25.280730
158.986883	4891.579385	25.285747
159.048284	4889.166635	25.290765
159.184559	4893.642176	25.295783
159.506672	4909.416456	25.300800
159.753581	4913.394543	25.305818
159.568685	4907.880842	25.310835
159.473551	4917.258091	25.315853
159.906321	4933.774816	25.320871
159.620442	4938.013006	25.325888
159.802616	4953.166294	25.330906
160.459082	4956.734560	25.335923
160.088997	4970.132079	25.340941
160.565922	4975.459718	25.345959
160.636103	4993.490896	25.350976
160.432363	5006.977115	25.355994
160.825020	5002.142440	25.361011
161.184915	5023.073331	25.366029
161.700834	5023.760202	25.371047
161.664554	5032.145803	25.376064
161.690293	5030.286225	25.381082
162.009585	5042.385524	25.386099
161.880977	5051.225019	25.391117
162.532509	5053.367988	25.396135
162.670723	5049.179343	25.401152
162.986954	5069.101260	25.406170
163.255003	5080.214460	25.411187
163.117671	5065.661161	25.416205
163.498407	5057.887574	25.421223
163.557090	5066.599271	25.426240
163.395047	5068.157694	25.431258
163.720177	5059.636913	25.436275
163.991887	5065.522563	25.441293
163.638501	5063.793348	25.446311
164.117015	5069.276679	25.451328
163.799754	5090.171498	25.456346
164.182802	5082.399486	25.461363
164.425399	5100.243620	25.466381
164.814124	5118.253808	25.471399
164.848610	5127.335719	25.476416
164.912197	5129.255337	25.481434
165.401240	5125.476472	25.486451
165.105694	5148.485339	25.491469
165.447156	5156.929473	25.496487
165.654372	5168.214223	25.501504
165.297638	5163.276917	25.506522
165.925173	5171.236733	25.511539
165.903467	5182.687286	25.516557
166.161161	5187.848049	25.521575
166.362909	5200.415763	25.526592
166.682991	5196.687636	25.531610
166.978495	5193.271481	25.536627
166.680242	5218.149223	25.541645
167.193148	5229.157891	25.546663
167.252399	5223.641537	25.551680
167.439775	5245.571424	25.556698
167.866592	5240.578259	25.561715
167.849193	5255.372644	25.566733
168.281404	5261.627959	25.571751
168.440602	5262.263927	25.576768
168.567638	5279.157558	25.581786
168.650098	5276.997599	25.586803
168.715102	5279.956891	25.591821
168.780613	5279.599556	25.596839
168.992801	5293.228347	25.601856
168.890166	5313.963183	25.606874
169.544986	5307.982208	25.611891
169.686467	5315.724735	25.616909
170.012937	5325.886215	25.621927
170.584538	5329.799342	25.626944
170.149262	5335.287278	25.631962
170.275626	5328.369074	25.636979
170.887494	5322.847608	25.641997
170.683607	5319.983683	25.647015
170.939008	5337.543260	25.652032
170.915353	5358.314718	25.657050
171.272610	5353.987030	25.662067
171.182932	5358.272452	25.667085
171.483542	5368.461858	25.672103
171.407050	5378.235959	25.677120
171.724474	5387.146453	25.682138
172.393163	5397.098661	25.687156
172.525040	5398.066750	25.692173
172.825741	5401.436785	25.697191
172.790089	5394.540203	25.702208
172.721492	5404.450042	25.707226
173.245814	5396.917558	25.712244
173.300954	5406.228926	25.717261
173.230257	5410.087549	25.722279
173.368222	5421.570956	25.727296
173.309494	5438.176120	25.732314
173.556548	5425.729338	25.737332
173.664110	5446.666658	25.742349
174.158704	5451.071737	25.747367
174.377233	5464.971319	25.752384
174.237889	5475.100793	25.757402
174.393711	5471.946272	25.762420
174.267853	5493.161623	25.767437
174.396441	5491.473212	25.772455
174.786566	5501.032478	25.777472
174.532406	5516.388346	25.782490
174.928660	5516.661885	25.787508
175.464370	5536.776119	25.792525
175.804758	5550.063435	25.797543
176.036114	5543.260485	25.802560
175.860913	5552.637167	25.807578
176.245562	5571.772330	25.812596
176.423655	5580.085397	25.817613
176.194966	5580.404707	25.822631
176.945293	5589.266627	25.827648
176.997223	5592.936899	25.832666
177.220283	5599.022549	25.837684
177.223524	5598.143925	25.842701
177.615174	5612.088666	25.847719
178.208548	5612.343025	25.852736
177.931857	5622.350779	25.857754
178.705081	5612.450752	25.862772
178.568704	5615.213033	25.867789
178.656014	5606.667069	25.872807
178.781290	5624.967076	25.877824
178.708688	5632.027706	25.882842
178.997579	5640.254772	25.887860
179.092066	5642.165410	25.892877
178.919962	5656.716011	25.897895
179.305579	5655.610796	25.902912
179.498123	5677.692031	25.907930
179.779027	5684.333200	25.912948
179.604424	5696.618958	25.917965
179.939154	5710.533423	25.922983
180.549398	5719.626075	25.928000
180.397836	5732.977505	25.933018
180.652062	5735.785521	25.938036
180.857523	5757.720225	25.943053
180.852255	5758.909453	25.948071
181.172400	5758.311580	25.953088
181.573633	5782.584410	25.958106
181.343055	5780.343408	25.963124
181.907921	5798.660763	25.968141
181.901006	5803.300404	25.973159
182.742454	5804.677344	25.978176
182.596862	5807.069471	25.983194
182.939876	5798.890271	25.988212
183.093763	5819.056932	25.993229
183.256529	5837.232076	25.998247
184.032836	5837.662153	26.003264
183.845735	5828.125420	26.008282
184.230368	5829.802285	26.013300
184.566807	5820.127865	26.018317
184.544816	5814.497542	26.023335
184.862803	5819.090593	26.028352
184.405502	5825.734090	26.033370
184.442898	5820.546779	26.038388
184.670832	5813.851381	26.043405
184.752673	5835.246690	26.048423
185.175083	5846.550320	26.053440
184.755890	5856.903078	26.058458
185.207571	5870.342384	26.063476
185.191530	5881.485375	26.068493
185.097582	5891.592260	26.073511
185.838990	5906.705262	26.078528
185.888073	5914.693705	26.083546
186.187799	5932.632122	26.088564
186.233580	5942.440317	26.093581
186.234411	5953.490793	26.098599
186.341595	5945.722198	26.103616
186.694630	5978.409395	26.108634
186.814077	5983.900009	26.113652
186.925298	5995.805648	26.118669
187.568522	6003.682581	26.123687
187.988733	5999.862907	26.128704
187.963750	6000.674245	26.133722
188.215920	6023.810467	26.138740
188.265671	6031.743731	26.143757
188.066982	6032.750728	26.148775
188.599130	6039.544270	26.153792
188.790773	6053.774858	26.158810
189.008698	6059.706785	26.163828
189.108895	6061.571642	26.168845
189.344169	6073.058350	26.173863
189.852580	6080.798514	26.178880
189.796032	6075.308476	26.183898
189.937115	6083.681872	26.188916
190.388017	6107.557169	26.193933
190.192139	6113.854390	26.198951
190.267102	6114.790189	26.203968
190.568103	6136.858482	26.208986
190.815664	6141.193927	26.214004
191.199061	6154.321081	26.219021
191.394083	6164.710375	26.224039
191.772092	6165.942625	26.229056
191.905496	6168.124112	26.234074
191.663425	6172.766489	26.239092
192.466193	6188.248434	26.244109
192.462020	6196.693930	26.249127
192.480973	6180.606022	26.254144
192.788570	6195.871311	26.259162
193.208268	6202.400777	26.264180
193.353175	6204.985166	26.269197
193.674321	6210.869382	26.274215
193.783706	6199.772927	26.279232
193.779579	6205.599841	26.284250
194.338471	6224.756629	26.289268
194.647017	6227.126549	26.294285
194.475528	6223.209276	26.299303
195.177768	6216.857464	26.304320
194.951953	6226.156280	26.309338
194.714379	6246.266887	26.314356
195.126748	6243.849494	26.319373
195.345922	6267.004916	26.324391
195.609477	6258.262912	26.329408
195.757261	6274.003584	26.334426
195.371682	6287.514643	26.339444
195.716620	6299.705580	26.344461
196.357170	6318.372525	26.349479
196.240864	6319.677797	26.354496
196.514103	6338.613368	26.359514
196.602382	6349.628410	26.364532
196.878402	6351.296503	26.369549
196.473046	6377.255785	26.374567
197.102691	6381.883353	26.379584
197.175296	6405.501861	26.384602
197.240693	6415.843435	26.389620
198.177640	6411.791802	26.394637
198.995544	6426.042900	26.399655
199.126621	6436.216124	26.404672
199.320354	6426.602715	26.409690
199.477629	6431.790328	26.414708
199.687702	6420.346309	26.419725
199.639097	6422.557116	26.424743
199.830229	6425.802538	26.429760
199.530598	6420.203694	26.434778
199.795819	6422.319335	26.439796
200.004390	6426.525842	26.444813
200.052302	6445.529486	26.449831
200.333003	6448.074152	26.454848
200.270900	6449.083809	26.459866
200.180382	6470.220216	26.464884
200.627961	6485.801309	26.469901
200.634207	6498.837493	26.474919
200.679791	6517.229675	26.479936
200.866385	6539.452111	26.484954
200.931000	6550.025445	26.489972
201.559718	6573.914601	26.494989
201.300330	6583.120728	26.500007
201.813968	6598.920199	26.505024
201.903754	6623.896318	26.510042
202.329522	6639.096835	26.515060
202.640243	6636.920635	26.520077
202.774415	6671.703344	26.525095
202.941881	6676.103363	26.530112
203.210414	6693.270476	26.535130
203.525045	6709.691252	26.540148
203.818761	6712.586643	26.545165
204.162442	6733.395702	26.550183
204.142292	6739.937424	26.555200
204.616713	6749.891883	26.560218
204.820533	6765.445010	26.565236
205.210790	6750.078018	26.570253
205.784162	6748.629439	26.575271
205.796652	6762.077496	26.580288
206.526478	6770.046832	26.585306
206.667689	6785.255128	26.590324
206.735234	6777.700592	26.595341
206.915033	6777.748055	26.600359
206.867652	6775.872788	26.605376
207.306160	6771.152865	26.610394
207.095050	6779.482438	26.615412
207.405239	6769.209284	26.620429
207.136069	6780.167913	26.625447
207.465178	6787.083539	26.630464
207.784992	6794.390551	26.635482
207.490063	6821.449096	26.640500
207.895418	6826.841575	26.645517
208.000084	6843.925667	26.650535
208.062592	6862.790364	26.655552
208.488516	6877.461048	26.660570
208.697824	6893.623767	26.665588
208.921696	6904.277349	26.670605
208.957143	6929.118015	26.675623
209.331837	6929.702698	26.680640
209.515683	6933.496010	26.685658
209.634557	6953.892009	26.690676
209.786160	6966.733658	26.695693
210.160726	6976.431470	26.700711
210.163341	6995.926836	26.705728
210.593930	7008.951613	26.710746
210.911301	7032.707827	26.715764
211.239228	7034.420187	26.720781
211.753592	7052.670959	26.725799
211.809070	7045.249815	26.730816
212.233839	7063.915497	26.735834
212.423468	7075.828690	26.740852
212.584112	7078.478357	26.745869
212.547838	7082.063133	26.750887
212.728499	7099.921746	26.755904
212.981774	7093.739066	26.760922
213.102656	7113.327663	26.765940
213.301522	7127.168960	26.770957
213.313607	7142.506047	26.775975
213.296328	7145.015002	26.780992
214.166491	7155.354837	26.786010
213.946472	7166.022867	26.791028
214.225553	7174.244092	26.796045
214.350719	7192.437254	26.801063
214.689826	7200.466641	26.806080
214.999259	7206.646941	26.811098
214.910306	7222.537150	26.816116
215.237580	7231.300971	26.821133
215.460515	7256.445903	26.826151
215.520366	7258.006468	26.831168
216.238048	7260.557830	26.836186
216.210612	7279.410320	26.841204
216.320729	7285.378640	26.846221
216.343583	7308.601896	26.851239
216.610229	7309.557291	26.856256
217.134001	7336.188462	26.861274
217.036236	7356.830277	26.866292
217.397105	7359.919470	26.871309
217.543655	7375.970974	26.876327
218.066056	7382.710796	26.881344
218.814318	7376.206006	26.886362
219.053652	7387.977330	26.891380
218.988560	7391.274738	26.896397
219.455255	7384.659732	26.901415
219.806991	7401.277514	26.906432
219.542896	7411.522173	26.911450
220.002612	7406.248025	26.916468
220.049316	7413.718591	26.921485
220.008101	7420.646062	26.926503
220.076181	7438.719773	26.931520
220.518981	7437.105259	26.936538
220.340941	7464.408650	26.941556
220.392261	7475.712549	26.946573
220.862410	7501.447112	26.951591
221.301063	7510.259633	26.956608
221.434583	7522.809370	26.961626
221.577581	7541.382766	26.966644
221.981351	7549.867126	26.971661
222.134527	7564.482701	26.976679
222.199293	7584.714393	26.981696
222.702941	7598.235597	26.986714
222.512079	7606.746561	26.991732
223.210428	7617.619950	26.996749
223.608908	7627.437081	27.001767
223.958947	7642.180876	27.006784
224.332411	7646.911798	27.011802
224.444787	7656.154001	27.016820
224.610408	7656.694496	27.021837
224.707689	7666.514947	27.026855
225.085100	7682.146626	27.031872
225.300248	7669.750213	27.036890
225.421143	7673.090986	27.041908
225.934187	7685.767964	27.046925
226.232964	7698.252731	27.051943
226.114080	7705.662580	27.056960
226.908543	7693.860388	27.061978
226.995768	7696.626255	27.066996
226.774278	7697.077912	27.072013
226.794665	7722.133395	27.077031
226.741658	7738.326142	27.082048
227.236509	7733.033481	27.087066
227.181248	7753.597904	27.092084
227.364273	7763.442054	27.097101
227.400184	7787.267961	27.102119
227.719460	7801.501883	27.107136
227.872562	7811.780261	27.112154
228.392266	7823.296081	27.117172
228.547161	7846.144668	27.122189
229.580128	7853.889624	27.127207
229.923894	7853.636697	27.132224
230.009366	7834.537623	27.137242
230.187392	7839.859320	27.142260
230.167924	7855.873369	27.147277
230.457594	7863.378829	27.152295
230.523135	7873.524428	27.157312
230.839174	7863.371683	27.162330
230.923748	7886.081510	27.167348
230.996078	7896.451263	27.172365
231.275451	7903.955294	27.177383
231.254230	7924.535581	27.182400
231.500134	7925.105354	27.187418
231.386820	7943.815298	27.192436
231.787580	7959.764748	27.197453
231.952639	7985.053512	27.202471
232.127349	8002.410045	27.207488
232.745620	8017.472973	27.212506
233.098464	8025.131900	27.217524
233.120291	8053.739111	27.222541
233.468477	8063.679820	27.227559
233.666025	8081.469016	27.232576
234.032531	8082.125200	27.237594
234.093000	8102.187346	27.242612
233.989897	8116.251107	27.247629
234.572651	8137.048514	27.252647
234.611688	8146.587458	27.257664
235.329387	8167.075908	27.262682
235.608285	8175.948279	27.267700
236.056642	8189.546076	27.272717
236.362998	8200.768187	27.277735
236.287344	8209.550291	27.282752
236.872428	8218.548530	27.287770
237.046252	8232.159429	27.292788
237.274329	8247.332728	27.297805
237.298794	8246.465415	27.302823
237.731062	8257.373759	27.307840
238.107943	8265.893668	27.312858
237.864551	8274.664138	27.317876
238.074102	8292.429535	27.322893
238.571981	8305.213487	27.327911
238.631416	8300.728241	27.332928
239.048492	8306.632842	27.337946
239.218669	8313.671493	27.342964
239.377620	8332.303043	27.347981
239.697327	8344.009817	27.352999
239.564769	8355.878751	27.358016
239.762953	8372.716688	27.363034
239.975078	8390.407730	27.368052
240.056641	8413.548080	27.373069
240.224026	8420.357245	27.378087
240.813492	8438.026955	27.383104
241.231899	8457.849253	27.388122
241.613440	8471.422100	27.393140
241.830806	8480.540318	27.398157
242.294234	8504.133625	27.403175
242.144534	8511.078708	27.408192
242.442003	8524.318922	27.413210
242.707518	8535.013985	27.418228
242.729743	8544.548858	27.423245
243.097175	8559.758507	27.428263
243.013104	8573.962882	27.433280
243.289504	8599.698951	27.438298
243.931972	8616.067549	27.443316
244.001676	8632.336241	27.448333
244.632059	8623.703256	27.453351
245.170211	8634.421869	27.458368
245.167002	8654.464515	27.463386
245.534151	8660.557086	27.468404
245.360517	8663.628513	27.473421
245.593111	8660.191297	27.478439
245.957268	8680.055130	27.483456
245.944893	8691.053778	27.488474
246.513377	8700.412638	27.493492
246.430787	8716.193019	27.498509
246.592978	8716.549805	27.503527
246.932906	8745.099405	27.508544
247.266475	8759.713849	27.513562
247.363570	8773.341040	27.518580
247.434834	8788.840080	27.523597
247.777130	8794.692631	27.528615
247.986849	8810.631181	27.533632
248.044457	8825.800903	27.538650
248.535127	8836.813424	27.543668
248.420316	8859.050323	27.548685
249.078477	8872.057159	27.553703
249.137537	8890.761793	27.558720
249.506694	8914.527246	27.563738
250.243415	8918.399833	27.568756
250.696977	8934.046951	27.573773
250.934616	8944.317611	27.578791
251.202262	8949.258605	27.583808
251.468492	8957.300143	27.588826
251.720816	8962.522511	27.593844
251.626748	8994.415499	27.598861
251.731144	8983.926799	27.603879
252.453601	9009.108563	27.608896
252.445095	9020.614854	27.613914
252.633952	9021.985717	27.618932
252.616638	9050.342829	27.623949
253.293428	9051.395200	27.628967
253.468033	9070.857613	27.633984
253.847857	9085.804209	27.639002
254.175946	9096.639761	27.644020
254.162116	9108.567621	27.649037
254.306554	9115.768419	27.654055
254.519756	9139.503262	27.659072
254.643869	9148.831042	27.664090
254.987703	9166.711503	27.669108
254.791972	9191.144924	27.674125
255.545883	9205.001889	27.679143
255.750944	9226.420815	27.684160
255.864321	9242.780591	27.689178
256.508645	9267.243118	27.694196
256.177197	9290.581374	27.699213
256.387582	9299.156918	27.704231
256.734337	9325.357520	27.709248
256.802130	9342.618967	27.714266
257.547760	9356.933511	27.719284
257.526503	9370.878518	27.724301
258.114574	9383.750057	27.729319
258.969657	9394.687795	27.734336
259.109518	9414.245379	27.739354
259.562520	9426.319269	27.744372
259.341566	9437.677426	27.749389
259.732010	9441.969699	27.754407
259.707506	9454.780234	27.759424
260.181947	9465.590284	27.764442
260.230213	9489.826310	27.769460
260.137708	9507.877706	27.774477
260.643127	9522.082422	27.779495
260.882555	9536.673750	27.784512
260.984481	9558.285821	27.789530
261.561390	9573.116817	27.794548
261.651794	9600.081767	27.799565
262.106306	9599.686065	27.804583
262.001765	9616.543039	27.809600
262.446838	9628.538834	27.814618
262.708431	9646.501164	27.819636
262.883967	9662.658111	27.824653
263.480528	9670.341378	27.829671
264.108478	9678.567713	27.834688
264.238422	9687.993311	27.839706
264.599189	9687.893522	27.844724
264.742051	9708.963388	27.849741
264.932157	9713.879621	27.854759
265.648352	9721.563629	27.859776
265.616624	9733.533511	27.864794
266.131583	9732.034466	27.869812
266.074804	9735.134843	27.874829
266.308178	9747.762007	27.879847
266.693837	9759.965435	27.884864
266.604841	9769.509964	27.889882
266.909703	9770.663222	27.894900
266.940017	9790.246455	27.899917
267.219139	9809.694868	27.904935
267.718547	9829.217191	27.909952
267.835881	9838.321207	27.914970
268.037989	9853.409743	27.919988
268.251534	9877.608811	27.925005
268.526580	9886.990073	27.930023
268.935831	9894.037192	27.935040
269.247002	9908.253866	27.940058
269.458896	9930.498936	27.945076
269.745717	9953.260224	27.950093
269.868039	9972.966334	27.955111
270.265600	9970.017547	27.960128
270.447870	9991.275056	27.965146
270.827560	10019.546244	27.970164
271.254719	10035.148396	27.975181
271.727203	10040.374922	27.980199
271.882432	10048.132862	27.985216
272.149508	10073.103239	27.990234
271.922234	10084.455021	27.995252
272.303637	10098.349106	28.000269
272.920004	10128.001673	28.005287
273.375335	10135.969242	28.010304
273.618530	10152.527494	28.015322
273.422017	10159.319540	28.020340
273.840216	10182.454895	28.025357
273.937932	10198.354259	28.030375
274.447752	10201.178361	28.035392
274.627872	10222.197059	28.040410
275.120683	10255.255994	28.045428
275.397592	10266.609684	28.050445
275.755463	10272.208919	28.055463
275.850067	10271.799406	28.060480
276.022794	10301.793424	28.065498
276.326615	10319.840916	28.070516
276.632235	10342.809195	28.075533
276.901294	10360.008555	28.080551
277.084894	10359.513439	28.085568
277.258043	10390.780557	28.090586
277.875972	10410.768480	28.095604
278.333435	10410.109953	28.100621
278.661835	10427.241290	28.105639
278.845983	10439.616388	28.110656
278.708349	10459.132870	28.115674
279.276800	10476.361668	28.120692
279.585638	10483.632031	28.125709
280.001262	10504.640552	28.130727
280.462577	10503.571753	28.135744
280.383431	10521.121072	28.140762
280.663818	10529.448600	28.145780
281.142427	10536.267912	28.150797
280.739191	10545.012464	28.155815
281.582217	10557.516704	28.160832
281.557443	10578.379084	28.165850
282.029461	10590.409755	28.170868
281.866526	10606.522743	28.175885
282.187589	10626.497748	28.180903
282.585638	10638.465839	28.185920
282.527015	10667.924485	28.190938
282.898564	10696.150950	28.195956
283.323397	10702.902805	28.200973
283.577356	10734.396725	28.205991
284.218157	10738.881170	28.211008
284.282718	10767.432621	28.216026
284.657518	10782.455691	28.221044
285.024981	10804.137441	28.226061
285.293888	10809.482147	28.231079
285.861904	10815.937826	28.236096
285.666991	10838.125325	28.241114
286.160043	10855.897950	28.246132
286.319246	10867.214794	28.251149
286.490306	10894.655446	28.256167
287.234533	10904.293812	28.261184
287.044390	10942.507979	28.266202
287.328927	10957.310580	28.271220
287.908287	10967.298423	28.276237
287.655114	10999.060986	28.281255
288.213647	11016.074580	28.286272
288.381745	11038.130693	28.291290
288.741863	11062.033189	28.296308
288.818349	11082.715636	28.301325
289.573357	11098.976035	28.306343
290.185466	11109.692773	28.311360
290.052532	11131.631737	28.316378
290.349755	11161.310588	28.321396
290.594592	11176.058504	28.326413
290.965741	11196.318216	28.331431
291.474202	11207.017480	28.336448
291.709489	11237.194347	28.341466
292.021448	11255.702409	28.346484
292.449017	11271.406540	28.351501
292.378651	11287.431652	28.356519
293.162797	11296.208904	28.361536
293.204744	11314.106984	28.366554
293.448165	11330.051150	28.371572
294.044916	11348.131763	28.376589
293.637789	11368.139763	28.381607
294.526136	11375.480231	28.386624
294.908979	11394.602255	28.391642
295.118225	11414.859055	28.396660
295.531948	11428.297549	28.401677
295.715236	11440.731861	28.406695
296.142227	11451.592069	28.411712
296.004107	11467.682125	28.416730
296.494871	11501.076424	28.421748
296.542197	11503.499762	28.426765
296.919351	11519.779686	28.431783
297.764024	11530.552823	28.436800
297.793989	11547.492018	28.441818
298.207039	11554.951271	28.446836
298.655851	11565.893823	28.451853
298.612138	11588.688410	28.456871
299.351086	11586.656668	28.461888
299.483779	11607.254875	28.466906
299.539519	11617.321754	28.471924
299.884896	11631.100227	28.476941
300.102227	11658.870937	28.481959
300.456217	11657.371533	28.486976
300.725266	11676.559963	28.491994
300.744357	11687.991133	28.497012
301.104500	11708.394330	28.502029
301.269046	11725.657329	28.507047
301.924091	11735.748961	28.512064
301.890922	11755.630272	28.517082
301.885617	11778.535380	28.522100
302.468250	11793.201271	28.527117
302.592267	11816.753139	28.532135
302.455569	11830.044194	28.537152
302.900073	11854.542917	28.542170
302.731124	11879.738618	28.547188
303.814078	11905.500392	28.552205
303.769319	11924.461282	28.557223
304.562597	11948.479465	28.562240
305.107958	11983.946402	28.567258
304.995627	12005.559354	28.572276
305.463312	12014.063912	28.577293
306.096332	12040.346147	28.582311
306.684541	12060.925616	28.587328
306.752377	12077.521919	28.592346
306.917003	12082.565996	28.597364
307.362844	12094.862111	28.602381
307.667965	12121.546873	28.607399
308.091757	12133.160456	28.612416
308.151150	12152.991512	28.617434
308.222608	12173.660435	28.622452
308.885096	12185.581270	28.627469
308.527069	12210.800847	28.632487
308.826466	12242.019198	28.637504
309.372825	12255.924148	28.642522
310.281995	12270.398657	28.647540
311.710312	12266.530724	28.652557
311.798329	12274.221275	28.657575
312.084762	12275.384070	28.662592
312.252187	12288.622109	28.667610
312.678560	12291.564373	28.672628
312.868585	12298.599930	28.677645
312.674649	12296.000558	28.682663
312.947270	12319.368679	28.687680
313.156364	12333.520073	28.692698
313.314386	12347.941482	28.697716
313.516913	12362.166469	28.702733
313.592983	12386.685902	28.707751
313.904334	12401.718610	28.712768
314.184423	12429.069023	28.717786
313.990962	12464.622047	28.722804
314.826276	12490.985839	28.727821
314.805083	12515.023611	28.732839
315.192392	12545.298358	28.737856
315.708200	12568.880354	28.742874
315.630481	12594.760141	28.747892
316.334008	12620.066549	28.752909
316.575961	12653.266413	28.757927
317.313484	12671.043208	28.762944
317.132788	12699.358912	28.767962
317.543728	12726.021678	28.772980
317.882002	12739.468220	28.777997
318.098573	12776.077685	28.783015
318.503162	12808.545071	28.788032
318.766814	12820.663055	28.793050
319.028202	12850.232761	28.798068
319.392279	12866.013548	28.803085
319.803335	12896.015577	28.808103
320.233090	12912.026648	28.813120
320.857042	12933.656293	28.818138
320.758710	12959.217038	28.823156
321.377073	12972.429989	28.828173
321.541632	12997.991485	28.833191
321.496286	13028.989403	28.838208
322.096585	13042.170728	28.843226
321.871151	13067.840884	28.848244
322.258766	13092.899254	28.853261
322.991708	13123.393744	28.858279
323.066792	13145.271925	28.863296
323.513393	13160.628091	28.868314
323.863854	13176.343673	28.873332
324.343186	13215.402022	28.878349
324.598265	13232.876227	28.883367
324.841964	13258.034266	28.888384
325.041534	13283.771645	28.893402
325.680857	13311.139841	28.898420
326.181220	13325.034406	28.903437
326.535208	13353.897963	28.908455
326.882726	13372.806776	28.913472
327.258219	13391.714141	28.918490
327.320170	13415.648118	28.923508
327.983979	13427.919488	28.928525
327.639727	13453.236418	28.933543
328.022252	13476.469870	28.938560
328.549127	13497.369378	28.943578
328.552020	13534.305806	28.948596
328.885462	13558.615884	28.953613
329.187504	13597.360916	28.958631
329.570427	13619.359069	28.963648
330.204581	13644.070280	28.968666
330.350369	13681.517639	28.973684
331.058468	13702.226739	28.978701
331.325996	13726.987613	28.983719
331.249344	13757.295577	28.988736
332.209220	13789.780353	28.993754
332.860996	13816.806968	28.998772
333.054805	13824.840071	29.003789
333.561854	13847.760378	29.008807
333.380803	13876.270445	29.013824
333.888035	13893.817167	29.018842
334.165709	13912.772818	29.023860
334.591140	13924.240869	29.028877
335.054145	13937.417244	29.033895
335.436192	13952.797434	29.038912
335.823440	13972.089619	29.043930
336.117858	13987.990168	29.048948
336.500424	14008.323232	29.053965
336.847003	14029.325702	29.058983
337.176684	14048.206733	29.064000
337.875865	14065.903156	29.069018
337.607189	14087.585684	29.074036
338.021902	14096.185983	29.079053
338.243502	14108.967440	29.084071
338.815225	14150.564105	29.089088
339.393826	14161.026831	29.094106
339.095074	14189.076249	29.099124
339.735714	14205.611623	29.104141
339.949387	14227.220955	29.109159
339.701953	14257.187733	29.114176
340.537239	14280.293961	29.119194
340.302222	14307.381221	29.124212
340.858357	14332.449915	29.129229
341.462669	14367.070031	29.134247
341.385356	14393.913909	29.139264
342.186519	14416.786434	29.144282
342.242753	14441.745621	29.149300
342.545451	14460.097361	29.154317
342.937066	14489.691091	29.159335
343.216144	14527.896875	29.164352
343.751560	14545.174895	29.169370
343.881530	14569.639870	29.174388
344.590211	14594.658553	29.179405
345.055340	14611.354137	29.184423
344.850971	14628.009051	29.189440
345.612134	14653.192506	29.194458
345.876022	14679.044392	29.199476
346.505689	14695.356722	29.204493
346.947954	14712.601456	29.209511
347.272806	14730.226492	29.214528
348.117174	14738.037533	29.219546
348.162261	14750.888053	29.224564
348.318243	14756.983173	29.229581
348.939451	14775.927206	29.234599
349.127955	14803.500050	29.239616
349.415409	14831.901295	29.244634
349.339475	14857.287968	29.249652
350.057458	14863.786707	29.254669
349.997940	14887.566410	29.259687
350.086933	14922.814965	29.264704
350.774778	14941.836435	29.269722
350.408477	14978.819795	29.274740
350.762908	15003.908663	29.279757
351.421144	15024.451187	29.284775
351.784951	15062.109977	29.289792
352.641358	15083.269132	29.294810
352.974881	15122.833672	29.299828
353.239601	15141.707794	29.304845
353.485344	15174.674216	29.309863
353.847673	15201.193062	29.314880
354.614746	15216.212986	29.319898
355.217441	15250.494840	29.324916
355.415171	15272.707063	29.329933
355.738467	15290.485833	29.334951
356.042357	15315.994861	29.339968
356.507777	15335.806856	29.344986
356.547938	15360.267365	29.350004
356.870042	15382.405608	29.355021
357.024274	15415.069283	29.360039
356.845173	15450.788782	29.365056
357.324940	15475.320256	29.370074
357.906815	15523.634074	29.375092
358.142893	15548.945060	29.380109
358.555174	15577.566534	29.385127
358.867399	15617.865482	29.390144
359.218095	15641.312168	29.395162
359.390314	15680.832210	29.400180
359.838856	15712.525889	29.405197
360.827271	15728.168498	29.410215
360.858972	15778.837124	29.415232
361.842847	15786.067716	29.420250
362.103220	15823.345038	29.425268
362.483547	15866.292110	29.430285
362.747896	15875.234977	29.435303
363.095910	15901.164735	29.440320
363.781342	15926.159363	29.445338
364.017328	15947.162088	29.450356
364.429778	15960.250743	29.455373
365.822653	15956.936316	29.460391
366.090435	15970.885757	29.465408
366.719934	15978.647793	29.470426
367.050199	15976.021117	29.475444
367.203640	16003.844490	29.480461
367.728818	16015.081624	29.485479
367.673237	16020.775602	29.490496
368.281111	16007.124308	29.495514
368.552691	16023.932119	29.500532
368.856988	16040.255422	29.505549
369.007690	16033.344750	29.510567
368.888483	16041.410169	29.515584
369.147544	16045.312218	29.520602
369.611334	16071.158502	29.525620
369.619081	16101.707466	29.530637
370.088504	16108.183152	29.535655
370.963805	16119.033124	29.540672
371.305943	16131.260396	29.545690
371.724064	16151.722653	29.550708
371.992720	16166.275749	29.555725
372.463958	16182.762321	29.560743
372.271678	16204.638342	29.565760
372.562990	16217.698358	29.570778
373.170136	16240.558221	29.575796
373.149211	16257.493396	29.580813
373.937199	16288.775926	29.585831
373.798514	16328.578998	29.590848
374.379567	16355.919397	29.595866
374.667016	16380.255469	29.600884
374.745947	16405.592164	29.605901
375.261705	16433.052228	29.610919
375.538499	16470.985540	29.615936
375.849181	16493.593698	29.620954
376.041309	16527.205291	29.625972
376.542039	16561.183640	29.630989
377.105666	16593.903395	29.636007
377.331050	16638.012882	29.641024
377.806581	16667.464303	29.646042
378.872396	16684.262948	29.651060
379.235536	16704.542693	29.656077
379.621485	16719.272343	29.661095
379.793871	16756.982417	29.666112
380.268966	16778.178398	29.671130
380.826718	16790.811859	29.676148
381.277407	16826.359386	29.681165
381.637760	16843.219569	29.686183
381.500440	16873.295875	29.691200
382.130691	16895.947940	29.696218
382.849806	16916.892588	29.701236
382.786142	16945.982807	29.706253
383.338956	16978.862730	29.711271
383.547886	17003.288351	29.716288
383.679109	17031.648296	29.721306
384.524749	17059.179429	29.726324
384.802639	17092.927746	29.731341
385.332315	17105.086938	29.736359
385.731651	17142.591757	29.741376
385.838827	17167.541954	29.746394
386.319655	17194.107499	29.751412
386.805385	17229.823488	29.756429
386.997338	17254.796064	29.761447
387.681222	17274.640520	29.766464
387.606033	17301.427334	29.771482
388.672210	17329.571873	29.776500
388.829941	17356.667059	29.781517
388.809372	17369.554121	29.786535
389.375834	17408.883948	29.791552
389.908707	17434.394699	29.796570
390.295680	17464.190025	29.801588
390.405989	17495.236893	29.806605
390.726723	17521.786857	29.811623
390.968203	17560.351110	29.816640
391.332690	17585.963993	29.821658
391.889589	17623.538451	29.826676
391.791241	17676.486798	29.831693
392.365620	17699.374599	29.836711
392.926493	17730.933831	29.841728
393.386406	17748.733681	29.846746
393.938272	17780.874543	29.851764
394.066790	17818.129308	29.856781
394.668611	17845.995215	29.861799
394.932762	17878.592037	29.866816
394.825244	17908.769335	29.871834
395.405448	17933.688260	29.876852
395.347464	17986.047724	29.881869
395.673332	18016.951203	29.886887
396.049483	18056.470060	29.891904
397.176831	18089.892519	29.896922
397.924670	18127.034639	29.901940
398.304549	18165.377258	29.906957
398.668812	18193.588789	29.911975
399.098706	18213.220982	29.916992
399.289498	18242.845207	29.922010
400.241967	18260.075604	29.927028
400.580730	18283.890575	29.932045
401.288478	18307.518527	29.937063
401.277525	18332.296116	29.942080
401.648996	18355.334991	29.947098
402.537030	18382.541355	29.952116
402.524942	18420.835825	29.957133
402.821421	18452.611926	29.962151
403.154153	18473.776863	29.967168
403.202332	18512.257047	29.972186
403.950084	18543.517416	29.977204
404.109554	18586.813871	29.982221
404.456938	18618.621289	29.987239
405.022934	18661.932753	29.992256
405.029753	18680.825171	29.997274
405.700240	18715.985794	30.002292
406.154349	18754.432586	30.007309
406.838069	18786.129596	30.012327
407.353046	18814.295220	30.017344
407.923235	18840.747771	30.022362
408.730262	18863.852545	30.027380
408.814911	18899.685690	30.032397
408.977401	18926.300306	30.037415
409.498098	18951.867434	30.042432
409.881039	18981.152278	30.047450
410.142099	19010.819864	30.052468
410.212392	19060.754467	30.057485
410.678904	19087.763648	30.062503
411.183047	19126.943919	30.067520
411.347518	19171.921458	30.072538
411.611885	19202.960265	30.077556
412.160504	19239.162030	30.082573
412.388972	19288.885179	30.087591
412.988520	19332.418271	30.092608
413.538335	19370.642601	30.097626
414.388750	19386.718219	30.102644
414.349477	19435.593809	30.107661
414.600581	19464.735765	30.112679
414.933962	19495.158388	30.117696
415.090223	19548.437944	30.122714
415.763386	19596.507439	30.127732
416.191873	19637.473273	30.132749
417.030876	19660.338995	30.137767
418.059174	19700.581651	30.142784
417.845680	19743.364188	30.147802
418.522351	19772.426926	30.152820
418.489061	19807.455470	30.157837
419.092500	19843.215983	30.162855
419.881302	19870.106988	30.167872
420.163935	19915.899364	30.172890
420.432534	19938.955856	30.177908
420.796058	19972.511453	30.182925
420.965303	19998.157166	30.187943
421.372053	20031.585933	30.192960
421.595964	20071.336519	30.197978
422.434871	20100.130259	30.202996
422.200077	20145.206330	30.208013
422.703398	20172.297897	30.213031
423.158009	20212.294470	30.218048
423.624862	20260.846099	30.223066
424.445547	20290.163407	30.228084
425.136776	20318.575195	30.233101
426.160160	20340.514393	30.238119
426.709442	20348.687452	30.243136
426.920321	20384.919125	30.248154
427.615705	20406.732876	30.253172
427.612535	20430.880139	30.258189
428.027168	20452.071903	30.263207
428.584072	20481.868229	30.268224
428.674533	20506.684325	30.273242
429.212493	20531.067098	30.278260
429.484334	20563.584366	30.283277
429.586257	20598.456656	30.288295
430.086351	20625.371351	30.293312
430.131697	20665.613182	30.298330
430.515874	20703.623578	30.303348
430.597599	20752.200841	30.308365
430.917622	20803.554516	30.313383
431.650501	20856.593227	30.318400
431.893589	20908.767106	30.323418
432.764846	20953.041501	30.328436
432.902488	20999.168217	30.333453
433.417312	21035.032633	30.338471
434.080551	21082.635094	30.343488
434.345629	21131.153213	30.348506
434.951792	21163.835560	30.353524
435.515366	21209.712772	30.358541
435.909999	21254.542812	30.363559
436.322013	21297.594906	30.368576
436.387039	21345.650078	30.373594
437.484646	21381.201404	30.378612
438.052819	21430.964678	30.383629
438.528012	21464.399194	30.388647
438.824011	21497.648964	30.393664
439.274082	21539.814091	30.398682
439.794386	21572.508265	30.403700
440.219895	21616.495435	30.408717
440.844053	21645.227993	30.413735
440.912779	21685.447912	30.418752
441.494339	21719.412442	30.423770
442.566775	21750.104933	30.428788
442.927400	21795.467041	30.433805
443.249805	21817.103028	30.438823
443.530416	21851.040284	30.443840
444.309462	21877.909339	30.448858
444.935783	21906.258873	30.453876
445.261573	21937.760867	30.458893
445.862295	21963.764001	30.463911
446.472526	21988.119620	30.468928
446.466838	22029.478357	30.473946
446.393930	22052.138531	30.478964
447.173457	22084.678944	30.483981
447.561276	22120.109440	30.488999
448.358063	22145.640590	30.494016
448.761518	22183.214429	30.499034
449.351453	22215.058009	30.504052
449.256051	22243.735446	30.509069
450.333941	22261.460127	30.514087
450.870526	22291.865309	30.519104
451.216273	22312.921028	30.524122
451.167913	22339.843935	30.529140
451.549924	22374.520712	30.534157
451.731551	22406.335924	30.539175
452.328136	22430.672366	30.544192
452.462993	22469.568304	30.549210
452.552427	22510.314954	30.554228
452.987724	22546.222541	30.559245
453.296652	22587.352513	30.564263
453.996634	22628.846847	30.569280
454.440845	22673.897948	30.574298
455.261232	22704.547105	30.579316
455.844116	22742.327479	30.584333
455.916384	22787.399328	30.589351
456.448509	22830.971583	30.594368
456.590423	22881.187967	30.599386
457.202850	22914.717799	30.604404
458.178058	22957.022050	30.609421
457.951151	22999.966455	30.614439
458.503647	23045.533589	30.619456
459.209841	23096.466257	30.624474
459.839035	23132.672598	30.629492
460.056808	23164.273563	30.634509
460.741199	23217.316702	30.639527
461.242290	23253.716326	30.644544
461.488035	23296.359512	30.649562
462.106210	23327.270255	30.654580
462.888559	23376.543496	30.659597
463.221553	23426.211186	30.664615
463.321656	23456.545507	30.669632
464.029550	23495.528900	30.674650
464.986953	23523.252532	30.679668
465.299496	23560.379312	30.684685
465.643526	23604.497079	30.689703
466.178680	23651.185061	30.694720
466.380028	23685.359848	30.699738
467.019762	23725.734708	30.704756
467.712738	23767.251919	30.709773
468.079998	23810.628452	30.714791
468.708706	23847.306287	30.719808
469.096339	23888.363353	30.724826
469.605061	23927.754342	30.729844
469.911945	23961.190079	30.734861
470.090781	24015.128125	30.739879
471.455296	24034.155506	30.744896
472.244710	24060.833966	30.749914
472.516634	24098.288726	30.754932
473.139684	24116.295488	30.759949
472.976354	24149.000361	30.764967
473.378344	24181.717564	30.769984
473.961168	24225.751777	30.775002
474.418838	24254.327069	30.780020
474.509001	24293.674515	30.785037
475.171394	24349.045926	30.790055
475.713853	24374.669774	30.795072
476.109197	24416.031173	30.800090
476.549474	24453.425793	30.805108
476.732850	24489.018019	30.810125
477.226054	24541.592294	30.815143
477.971127	24583.985939	30.820160
478.469694	24625.890582	30.825178
478.591409	24668.789503	30.830196
479.330318	24710.165826	30.835213
479.725785	24761.722501	30.840231
479.938043	24789.443567	30.845248
480.607624	24840.180956	30.850266
480.798934	24885.448439	30.855284
481.602015	24931.680967	30.860301
481.774468	24979.526874	30.865319
482.476747	25022.997816	30.870336
482.424559	25058.582835	30.875354
483.085702	25103.940443	30.880372
483.803598	25148.637534	30.885389
483.975311	25201.755793	30.890407
484.677606	25238.039711	30.895424
485.283981	25280.587309	30.900442
485.814486	25315.445847	30.905460
486.751168	25340.474611	30.910477
487.326406	25388.584711	30.915495
487.690492	25425.358549	30.920512
487.942756	25461.062850	30.925530
488.624384	25504.763935	30.930548
488.734872	25538.372406	30.935565
489.520717	25586.380468	30.940583
490.832649	25605.102923	30.945600
491.475342	25621.368664	30.950618
492.229381	25653.152184	30.955636
492.655040	25670.497765	30.960653
492.980272	25701.563726	30.965671
493.239627	25718.085267	30.970688
493.560518	25756.847618	30.975706
494.045905	25799.976320	30.980724
494.514228	25833.393800	30.985741
494.587061	25878.126814	30.990759
494.978416	25903.278023	30.995776
495.218330	25951.333132	31.000794
495.214253	25985.475502	31.005812
496.179222	26038.706613	31.010829
496.344509	26100.787613	31.015847
496.879807	26153.799886	31.020864
497.616423	26202.290912	31.025882
497.955290	26249.718635	31.030900
498.649203	26288.909449	31.035917
499.429169	26322.613891	31.040935
500.388751	26368.255161	31.045952
500.549680	26412.063498	31.050970
500.578995	26457.022840	31.055988
501.667965	26496.126797	31.061005
502.106867	26529.336020	31.066023
502.914263	26566.644670	31.071040
503.514782	26609.081420	31.076058
503.794958	26644.805659	31.081076
504.997841	26684.096247	31.086093
505.175676	26733.561069	31.091111
505.980598	26736.519131	31.096128
506.427711	26788.570161	31.101146
506.386670	26814.119004	31.106164
506.974959	26848.625749	31.111181
507.038050	26894.731914	31.116199
507.253365	26944.519182	31.121216
508.141843	26989.817436	31.126234
508.573583	27048.580683	31.131252
508.558406	27075.138129	31.136269
509.138126	27128.224931	31.141287
509.664321	27177.712344	31.146304
510.017168	27236.063447	31.151322
510.165820	27291.950340	31.156340
510.973214	27334.748990	31.161357
511.294348	27388.674171	31.166375
512.099308	27454.950465	31.171392
512.541981	27509.130366	31.176410
512.521030	27569.001601	31.181428
513.343781	27615.829562	31.186445
513.895020	27682.905665	31.191463
514.240986	27736.862530	31.196480
515.387839	27799.752745	31.201498
515.896946	27853.149950	31.206516
517.019418	27886.958609	31.211533
517.739759	27915.906699	31.216551
518.103181	27948.055505	31.221568
518.657262	27974.958761	31.226586
518.790761	28025.106486	31.231604
519.220029	28056.077510	31.236621
519.963967	28099.058878	31.241639
520.158867	28143.276073	31.246656
520.625370	28187.868053	31.251674
520.601959	28240.780318	31.256692
521.364108	28278.831977	31.261709
521.385453	28333.645540	31.266727
522.371445	28391.482745	31.271744
522.728558	28444.373787	31.276762
522.479050	28512.985937	31.281780
523.321651	28554.863863	31.286797
524.387308	28602.887769	31.291815
525.760020	28665.554570	31.296832
526.523930	28694.275959	31.301850
527.021179	28745.595932	31.306868
527.403288	28780.254163	31.311885
527.580161	28827.551704	31.316903
528.108986	28874.267595	31.321920
528.699792	28912.904144	31.326938
529.182237	28975.816906	31.331956
529.608665	29021.345080	31.336973
530.351384	29073.429884	31.341991
530.683549	29129.371265	31.347008
531.286730	29174.958975	31.352026
531.402412	29220.053195	31.357044
532.515769	29280.443304	31.362061
533.274113	29327.538910	31.367079
533.600731	29375.942552	31.372096
534.013521	29409.287817	31.377114
534.177946	29473.863755	31.382132
534.896607	29513.294413	31.387149
535.225655	29569.348136	31.392167
535.658970	29617.709591	31.397184
536.275573	29674.899147	31.402202
536.774157	29737.805692	31.407220
537.328439	29790.191916	31.412237
538.486672	29845.989697	31.417255
538.946196	29895.338163	31.422272
539.744692	29945.463619	31.427290
540.213076	29996.391410	31.432308
541.158096	30035.599739	31.437325
541.362966	30088.208617	31.442343
541.530370	30133.448086	31.447360
542.351365	30169.446762	31.452378
542.486703	30221.632173	31.457396
543.046254	30273.564697	31.462413
543.693831	30319.447778	31.467431
544.298359	30375.676273	31.472448
544.873217	30428.199827	31.477466
545.366570	30476.739882	31.482484
546.098772	30531.789984	31.487501
546.988368	30565.998842	31.492519
547.479537	30613.549030	31.497536
548.553207	30652.393626	31.502554
549.402064	30697.449442	31.507572
549.890684	30725.579235	31.512589
550.215475	30766.115729	31.517607
550.160329	30799.304330	31.522624
551.018503	30831.534501	31.527642
551.089679	30879.788908	31.532660
551.629190	30928.467719	31.537677
552.299646	30967.023114	31.542695
552.620316	31026.417609	31.547712
553.479821	31058.884597	31.552730
553.957359	31107.813915	31.557748
554.391422	31134.858627	31.562765
555.074010	31176.113082	31.567783
554.945113	31222.117318	31.572800
555.387184	31265.594917	31.577818
555.736183	31326.752512	31.582836
555.991634	31384.770818	31.587853
556.861867	31440.902065	31.592871
557.056096	31495.308950	31.597888
557.644115	31554.291944	31.602906
558.060883	31622.238367	31.607924
558.500738	31681.852020	31.612941
559.425239	31744.338924	31.617959
559.629120	31824.815167	31.622976
560.416618	31881.554635	31.627994
561.366067	31944.713312	31.633012
562.226460	31985.482822	31.638029
563.385306	32020.047596	31.643047
563.888829	32069.385463	31.648064
564.373504	32119.837171	31.653082
565.110915	32180.536045	31.658100
565.517528	32228.315971	31.663117
566.039482	32273.994602	31.668135
566.195987	32337.228865	31.673152
566.734622	32377.900984	31.678170
567.137401	32446.177879	31.683188
567.789899	32508.374827	31.688205
568.489674	32571.709511	31.693223
568.841304	32634.515060	31.698240
569.476232	32683.769842	31.703258
570.455121	32742.938369	31.708276
571.142939	32794.409138	31.713293
571.890544	32836.041691	31.718311
571.911770	32904.626330	31.723328
572.418490	32960.333410	31.728346
572.960721	33022.878529	31.733364
573.713131	33081.820559	31.738381
574.340169	33144.017643	31.743399
574.422129	33207.393544	31.748416
574.879700	33265.611840	31.753434
575.582934	33339.553640	31.758452
576.323726	33406.702462	31.763469
576.879007	33468.167883	31.768487
576.986654	33547.042878	31.773504
577.396166	33611.864912	31.778522
578.283804	33684.417739	31.783540
579.006248	33747.150218	31.788557
580.217055	33796.212015	31.793575
581.167841	33857.850119	31.798592
582.169820	33911.190734	31.803610
582.699898	33960.125606	31.808628
583.100765	34001.843418	31.813645
583.405106	34049.058250	31.818663
583.807255	34112.614849	31.823680
584.472815	34164.705438	31.828698
585.052430	34225.734015	31.833716
585.354921	34286.609777	31.838733
585.986980	34343.348123	31.843751
586.543555	34415.513698	31.848768
587.317774	34459.865714	31.853786
588.007391	34511.757708	31.858804
588.259815	34584.665260	31.863821
589.155090	34627.069676	31.868839
589.368013	34685.620192	31.873856
590.348842	34744.754072	31.878874
590.986267	34799.138944	31.883892
591.384215	34852.654730	31.888909
592.104217	34901.147446	31.893927
592.617369	34956.629378	31.898944
593.435194	34998.955961	31.903962
593.771386	35058.273086	31.908980
594.165403	35110.253514	31.913997
595.086258	35155.766405	31.919015
595.056747	35205.639680	31.924032
595.597036	35264.229541	31.929050
596.249007	35342.094832	31.934068
596.511756	35391.402827	31.939085
596.991841	35455.831777	31.944103
597.909988	35530.529807	31.949120
598.527150	35592.203782	31.954138
598.901495	35660.923757	31.959156
599.564235	35739.091947	31.964173
600.237335	35793.748508	31.969191
600.192250	35863.229639	31.974208
601.436214	35930.453206	31.979226
601.979252	36006.458547	31.984244
602.405143	36083.121028	31.989261
602.870771	36149.053862	31.994279
603.582610	36227.714692	31.999296
603.759395	36289.659462	32.004314
604.393712	36374.856832	32.009332
605.108496	36460.716670	32.014349
606.552051	36517.835994	32.019367
607.316038	36584.547989	32.024384
608.450890	36626.920748	32.029402
609.697065	36663.919675	32.034420
610.313351	36727.791049	32.039437
611.157813	36771.559682	32.044455
611.028245	36829.381642	32.049472
611.710739	36882.171668	32.054490
612.128216	36934.115644	32.059508
612.739303	37005.080255	32.064525
613.746402	37049.696904	32.069543
614.021960	37097.681972	32.074560
614.773989	37150.963102	32.079578
615.463780	37208.045007	32.084596
615.385981	37261.488764	32.089613
616.148063	37332.110972	32.094631
616.851657	37399.574472	32.099648
617.557633	37456.730237	32.104666
618.175508	37504.356874	32.109684
618.815443	37569.641235	32.114701
620.081741	37624.000257	32.119719
620.294350	37689.485026	32.124736
620.668797	37749.038277	32.129754
621.245469	37809.947005	32.134772
622.028784	37874.142029	32.139789
622.770037	37924.334246	32.144807
622.784500	37994.577544	32.149824
623.418558	38060.495876	32.154842
624.141440	38122.252603	32.159860
624.183016	38202.497213	32.164877
624.955957	38274.292250	32.169895
625.477342	38350.674023	32.174912
625.839080	38413.220467	32.179930
626.713283	38496.819620	32.184948
627.497043	38557.349480	32.189965
628.216793	38631.862757	32.194983
628.864006	38698.156830	32.200000
629.561555	38775.189892	32.205018
630.681845	38825.344104	32.210036
631.068613	38886.862261	32.215053
632.219250	38953.629630	32.220071
632.717922	39006.674013	32.225088
633.342279	39067.080400	32.230106
634.405857	39112.687064	32.235124
634.640879	39167.075861	32.240141
635.655306	39215.648381	32.245159
636.140154	39267.307020	32.250176
636.322374	39325.874544	32.255194
636.808677	39376.289649	32.260212
636.986630	39441.322482	32.265229
637.731202	39496.972727	32.270247
638.017643	39563.818783	32.275264
639.011111	39633.325955	32.280282
639.416952	39694.714281	32.285300
639.785445	39769.908897	32.290317
640.372417	39842.782473	32.295335
640.902338	39906.313185	32.300352
641.424015	39986.808335	32.305370
642.039497	40070.135496	32.310388
642.699463	40158.865929	32.315405
642.931304	40245.394808	32.320423
643.824089	40328.607907	32.325440
644.465209	40410.461444	32.330458
645.654027	40486.104333	32.335476
645.997462	40577.098660	32.340493
646.679842	40657.759619	32.345511
647.167229	40743.942462	32.350528
647.880615	40826.164716	32.355546
648.669242	40914.451422	32.360564
649.064707	40987.610563	32.365581
650.267182	41078.058299	32.370599
651.692670	41118.161829	32.375616
652.954753	41183.943560	32.380634
654.134967	41242.226136	32.385652
654.150641	41321.191343	32.390669
655.148435	41372.168293	32.395687
655.529636	41432.480613	32.400704
655.977774	41496.750084	32.405722
656.632390	41551.370252	32.410740
657.196856	41621.722925	32.415757
657.783305	41682.399919	32.420775
658.234798	41753.731409	32.425792
658.623614	41821.357991	32.430810
659.628764	41873.528384	32.435828
660.121125	41961.660707	32.440845
661.061340	42026.810433	32.445863
662.103574	42092.110854	32.450880
662.428817	42155.007601	32.455898
663.311263	42215.100805	32.460916
663.696038	42282.963356	32.465933
664.485598	42342.497766	32.470951
665.620467	42396.169833	32.475968
666.613963	42459.200337	32.480986
667.353262	42505.812944	32.486004
667.422825	42566.524547	32.491021
668.090050	42644.109269	32.496039
668.764892	42706.482934	32.501056
669.040974	42772.196420	32.506074
669.575930	42844.380191	32.511092
670.092096	42921.084975	32.516109
670.576415	42988.883168	32.521127
671.176538	43062.613422	32.526144
672.217406	43134.238068	32.531162
674.138946	43164.426919	32.536180
674.725156	43226.684383	32.541197
675.361916	43289.000007	32.546215
675.968902	43349.006642	32.551232
676.314591	43405.403912	32.556250
676.876675	43452.970036	32.561268
677.113258	43529.054214	32.566285
677.403555	43606.787303	32.571303
677.998116	43675.412745	32.576320
677.943254	43741.184320	32.581338
679.023686	43805.628915	32.586356
679.366775	43882.104217	32.591373
679.848685	43964.776491	32.596391
680.577536	44055.102362	32.601408
680.709412	44139.579132	32.606426
681.527520	44220.185896	32.611444
682.124455	44301.688295	32.616461
682.780421	44401.221670	32.621479
683.678775	44491.363803	32.626496
684.070067	44598.459328	32.631514
685.138125	44679.961352	32.636532
685.609032	44775.981674	32.641549
686.103881	44868.623379	32.646567
686.876717	44960.859700	32.651584
687.269654	45050.147118	32.656602
688.266899	45146.833869	32.661620
688.849208	45250.220114	32.666637
689.493836	45353.883960	32.671655
690.187584	45438.223292	32.676672
690.695639	45548.888625	32.681690
691.945512	45642.915562	32.686708
692.814010	45735.739817	32.691725
693.552511	45827.032528	32.696743
694.533141	45909.672094	32.701760
695.372035	46019.584607	32.706778
696.337445	46104.062049	32.711796
697.288241	46180.348510	32.716813
698.415886	46256.669226	32.721831
699.111502	46324.027853	32.726848
699.856409	46410.453406	32.731866
700.408967	46478.496142	32.736884
701.035514	46562.201164	32.741901
701.742584	46642.407269	32.746919
702.391576	46718.944686	32.751936
703.003408	46799.565047	32.756954
703.494642	46883.243319	32.761972
704.376869	46971.657030	32.766989
705.222062	47053.585101	32.772007
705.863052	47120.548260	32.777024
706.021510	47204.563946	32.782042
707.169299	47287.993492	32.787060
707.768138	47385.935387	32.792077
708.394081	47479.866140	32.797095
709.542420	47553.545668	32.802112
709.847775	47636.519059	32.807130
710.725959	47724.567504	32.812148
711.574359	47802.967895	32.817165
712.125756	47888.330103	32.822183
713.222552	47966.197532	32.827200
713.388926	48056.761858	32.832218
714.432005	48132.819929	32.837236
715.303582	48204.725619	32.842253
715.871404	48298.922661	32.847271
717.394439	48369.098243	32.852288
718.623531	48433.767882	32.857306
719.373256	48489.722126	32.862324
719.877938	48555.184443	32.867341
720.072150	48620.035091	32.872359
720.767795	48690.534818	32.877376
721.498776	48775.542933	32.882394
721.795798	48840.835259	32.887412
722.630353	48921.778409	32.892429
723.047909	49006.021395	32.897447
723.775262	49091.432585	32.902464
724.178562	49182.266311	32.907482
724.897148	49265.317526	32.912500
725.000858	49343.512503	32.917517
725.520411	49434.552454	32.922535
725.999947	49518.342178	32.927552
726.990614	49607.814541	32.932570
728.185530	49706.333159	32.937588
729.032708	49784.018715	32.942605
729.639570	49870.899711	32.947623
730.382915	49953.056075	32.952640
731.433344	50025.501258	32.957658
732.861369	50097.217985	32.962676
734.041329	50165.432462	32.967693
734.680761	50237.339948	32.972711
735.785829	50290.458427	32.977728
736.270194	50365.224912	32.982746
736.618518	50431.745907	32.987764
737.837301	50496.610589	32.992781
738.258158	50560.426073	32.997799
738.864995	50646.442072	33.002816
739.357909	50724.404709	33.007834
739.828873	50802.721858	33.012852
740.544358	50875.727738	33.017869
740.991303	50966.799594	33.022887
741.569718	51050.690231	33.027904
742.026402	51139.790497	33.032922
743.199556	51220.501116	33.037940
744.094472	51308.253818	33.042957
744.877177	51406.441816	33.047975
745.751974	51488.428283	33.052992
745.833524	51584.575785	33.058010
746.918438	51669.629893	33.063028
747.464354	51775.000087	33.068045
748.086846	51876.334324	33.073063
749.095074	51965.457871	33.078080
749.651186	52055.073411	33.083098
749.692957	52165.487824	33.088116
750.869778	52268.210759	33.093133
751.513120	52381.590837	33.098151
752.246994	52476.504287	33.103168
752.698969	52577.744011	33.108186
753.610707	52682.111158	33.113204
754.471282	52788.281408	33.118221
755.215878	52897.964840	33.123239
756.669092	52993.197922	33.128256
757.780493	53081.532541	33.133274
758.651355	53179.661280	33.138292
759.428729	53275.500106	33.143309
759.991251	53362.972718	33.148327
760.995956	53446.051572	33.153344
761.744495	53544.379239	33.158362
762.514067	53631.932583	33.163380
763.589531	53717.426832	33.168397
764.279173	53809.151108	33.173415
765.172596	53889.129354	33.178432
766.302514	53966.598689	33.183450
766.848059	54046.761380	33.188468
767.851169	54117.625054	33.193485
768.517848	54216.051756	33.198503
768.931891	54296.717333	33.203520
769.803401	54386.133590	33.208538
770.254415	54477.571888	33.213556
771.051051	54559.495784	33.218573
771.097031	54664.035469	33.223591
771.881401	54762.635019	33.228608
772.782763	54859.573093	33.233626
773.668324	54956.495302	33.238644
774.133452	55052.931436	33.243661
774.692987	55159.556015	33.248679
775.624309	55265.292117	33.253696
776.282455	55362.481332	33.258714
776.823638	55450.908195	33.263732
777.730717	55540.349115	33.268749
778.247085	55648.487186	33.273767
779.260144	55737.627185	33.278784
780.228870	55838.343556	33.283802
780.851584	55932.527650	33.288820
782.187879	56015.133012	33.293837
783.186794	56102.413110	33.298855
783.952262	56180.374703	33.303872
785.355454	56262.647824	33.308890
785.795034	56349.275812	33.313908
786.736474	56432.434643	33.318925
787.153714	56519.041790	33.323943
787.918311	56615.770998	33.328960
788.775842	56704.644085	33.333978
789.199426	56788.837702	33.338996
790.360652	56869.314619	33.344013
791.472398	56971.561198	33.349031
791.853548	57064.293072	33.354048
792.868699	57154.235268	33.359066
793.182935	57255.357596	33.364084
793.892751	57350.601914	33.369101
794.723288	57455.178473	33.374119
795.218148	57555.729091	33.379136
796.005414	57662.279020	33.384154
796.202017	57783.283440	33.389172
797.104007	57883.648429	33.394189
798.133136	57992.896258	33.399207
799.150147	58106.291910	33.404224
800.208926	58223.371590	33.409242
800.498971	58330.651734	33.414260
801.197530	58442.048203	33.419277
802.189968	58546.843883	33.424295
802.685410	58671.324066	33.429312
803.485638	58792.974266	33.434330
804.493574	58900.840352	33.439348
805.700519	59018.974492	33.444365
806.286511	59127.252711	33.449383
807.141545	59238.766801	33.454400
808.390634	59348.055233	33.459418
809.225957	59461.166287	33.464436
810.155111	59555.013603	33.469453
811.006931	59674.467806	33.474471
811.519209	59774.925599	33.479488
812.808893	59871.343758	33.484506
813.235251	59985.966141	33.489524
814.370481	60089.008437	33.494541
815.127893	60204.190394	33.499559
815.766069	60304.099192	33.504576
816.744427	60407.042627	33.509594
817.528848	60525.590340	33.514612
818.230747	60619.745576	33.519629
818.571125	60738.247785	33.524647
819.544445	60854.604878	33.529664
820.284005	60959.638177	33.534682
821.079304	61084.589365	33.539700
822.416446	61188.179044	33.544717
823.120339	61303.641543	33.549735
823.595462	61415.230411	33.554752
824.596530	61524.919204	33.559770
825.684381	61645.376257	33.564788
827.246455	61724.365531	33.569805
828.407801	61815.808675	33.574823
829.973051	61899.298019	33.579840
831.423009	61970.008442	33.584858
832.665534	62036.796938	33.589876
833.856910	62087.755712	33.594893
834.571017	62150.422594	33.599911
835.061074	62206.035375	33.604928
835.928679	62263.109145	33.609946
836.281844	62323.624077	33.614964
836.959365	62380.843329	33.619981
837.532924	62452.686110	33.624999
837.565910	62528.555965	33.630016
838.176154	62606.517623	33.635034
838.487673	62697.213890	33.640052
839.246910	62788.241137	33.645069
839.720281	62893.454799	33.650087
840.260019	62988.267199	33.655104
841.166314	63104.092045	33.660122
841.529103	63209.186539	33.665140
841.852043	63310.723355	33.670157
842.636547	63444.855635	33.675175
843.574501	63571.878013	33.680192
844.570579	63687.729259	33.685210
845.452911	63816.083356	33.690228
845.949331	63934.363484	33.695245
846.763179	64065.789695	33.700263
847.659604	64202.544217	33.705280
848.585762	64320.313148	33.710298
850.037784	64438.994627	33.715316
851.539221	64543.250559	33.720333
852.667176	64662.865450	33.725351
853.607542	64764.269571	33.730368
854.919554	64878.551997	33.735386
855.379782	64985.535794	33.740404
856.642249	65092.741662	33.745421
857.132717	65193.880840	33.750439
857.200619	65322.530509	33.755456
858.470090	65433.694048	33.760474
859.092254	65558.473578	33.765492
859.691230	65687.056782	33.770509
860.697461	65793.284542	33.775527
861.240909	65916.966672	33.780544
862.248798	66036.685193	33.785562
863.088305	66167.260825	33.790580
864.060836	66296.607910	33.795597
864.842069	66412.219131	33.800615
865.678795	66540.477571	33.805632
866.855327	66658.117321	33.810650
867.326071	66789.996779	33.815668
868.498003	66917.342450	33.820685
869.363242	67037.444294	33.825703
870.186055	67163.161216	33.830720
871.285493	67284.951649	33.835738
872.341268	67428.623483	33.840756
873.015413	67536.128756	33.845773
874.379683	67655.905205	33.850791
875.080795	67773.566520	33.855808
876.130566	67883.850100	33.860826
877.070365	68013.358630	33.865844
877.638094	68136.961396	33.870861
878.508908	68248.698900	33.875879
879.311167	68375.899534	33.880896
880.249779	68502.920370	33.885914
880.634153	68630.792147	33.890932
881.214090	68752.069947	33.895949
883.031600	68858.191981	33.900967
884.313479	68975.669298	33.905984
885.506061	69078.165479	33.911002
886.410930	69194.334322	33.916020
887.538593	69315.272031	33.921037
888.016795	69417.894139	33.926055
888.996016	69527.281230	33.931072
889.440946	69630.434626	33.936090
890.670340	69752.685760	33.941108
891.082434	69857.951083	33.946125
891.633196	69960.020098	33.951143
892.075778	70059.230679	33.956160
893.249047	70177.010801	33.961178
894.058237	70292.234102	33.966196
895.310833	70419.043898	33.971213
896.076776	70528.016133	33.976231
896.714198	70644.319280	33.981248
897.496709	70756.501922	33.986266
898.096947	70886.141026	33.991284
899.380288	71011.672062	33.996301
900.440633	71134.015965	34.001319
901.125840	71263.497905	34.006336
902.215214	71375.298019	34.011354
903.483268	71489.023033	34.016372
903.875383	71614.224215	34.021389
905.408931	71737.473520	34.026407
906.005366	71865.089475	34.031424
907.096881	71980.256310	34.036442
908.077303	72099.368822	34.041460
908.664630	72220.494459	34.046477
909.607110	72359.210427	34.051495
910.260981	72484.424056	34.056512
911.499806	72612.475871	34.061530
912.016789	72753.850895	34.066548
912.703339	72889.697453	34.071565
913.828080	73019.522120	34.076583
914.511597	73162.377315	34.081600
915.479836	73297.465373	34.086618
916.697058	73425.051318	34.091636
917.706852	73553.810520	34.096653
918.867966	73688.552997	34.101671
919.470590	73829.269582	34.106688
920.428511	73962.769924	34.111706
921.264100	74101.394590	34.116724
922.095024	74242.297494	34.121741
922.654397	74379.319019	34.126759
923.663326	74537.439670	34.131776
924.999048	74664.222857	34.136794
925.914629	74804.034028	34.141812
926.749756	74953.003947	34.146829
927.723924	75087.868188	34.151847
928.358814	75237.012237	34.156864
929.506904	75370.825003	34.161882
930.476838	75515.811255	34.166900
932.018684	75632.656014	34.171917
933.123160	75769.577303	34.176935
934.206263	75908.507787	34.181952
935.078206	76038.234127	34.186970
936.189692	76174.486408	34.191988
937.267963	76304.616641	34.197005
937.951234	76433.623863	34.202023
938.198837	76561.217512	34.207040
939.614388	76690.718816	34.212058
940.268165	76829.403461	34.217076
941.075184	76969.265357	34.222093
942.260503	77102.962379	34.227111
943.763236	77227.266222	34.232128
945.241727	77339.058122	34.237146
946.358584	77452.093027	34.242164
947.353959	77583.813051	34.247181
948.039894	77701.018849	34.252199
948.225786	77838.490492	34.257216
949.117095	77967.314213	34.262234
950.176945	78098.786309	34.267252
950.066311	78229.358214	34.272269
951.041274	78378.929127	34.277287
951.827085	78518.386865	34.282304
952.804119	78660.679181	34.287322
953.558527	78802.465200	34.292340
953.875058	78936.841719	34.297357
955.177547	79082.555525	34.302375
956.161856	79220.738819	34.307392
957.581905	79366.877843	34.312410
958.821190	79510.985604	34.317428
959.300971	79650.937403	34.322445
960.118885	79783.414523	34.327463
961.123337	79933.838604	34.332480
961.907782	80082.649061	34.337498
963.162657	80240.624470	34.342516
963.974975	80384.972813	34.347533
965.078625	80529.590267	34.352551
965.686350	80703.198892	34.357568
966.958358	80850.301908	34.362586
967.885742	81000.309380	34.367604
968.440654	81168.850719	34.372621
969.557861	81316.494727	34.377639
970.605043	81492.503957	34.382656
971.527054	81644.129699	34.387674
972.677414	81801.570299	34.392692
973.191820	81968.163224	34.397709
974.555047	82132.814298	34.402727
975.376944	82292.185056	34.407744
976.801975	82442.575409	34.412762
978.382948	82601.481402	34.417780
979.566653	82740.798415	34.422797
980.750838	82890.598871	34.427815
981.644507	83045.268945	34.432832
982.311774	83207.170544	34.437850
983.469640	83355.605575	34.442868
984.128327	83516.441615	34.447885
985.170103	83662.405176	34.452903
986.411037	83810.608019	34.457920
987.086310	83971.292679	34.462938
988.714949	84114.941600	34.467956
989.594478	84268.072250	34.472973
990.596025	84408.650551	34.477991
992.325452	84566.843438	34.483008
993.092331	84697.573528	34.488026
993.930787	84838.738141	34.493044
995.064511	84987.731828	34.498061
995.996042	85128.370371	34.503079
996.917834	85267.454950	34.508096
997.862094	85413.306535	34.513114
998.968632	85555.696672	34.518132
1000.021776	85705.556115	34.523149
1001.846609	85821.122752	34.528167
1003.243308	85948.737916	34.533184
1004.392040	86074.939473	34.538202
1005.480755	86204.403808	34.543220
1005.904511	86341.489084	34.548237
1006.849323	86467.391096	34.553255
1007.595729	86605.095347	34.558272
1008.205852	86745.758804	34.563290
1009.552318	86880.448708	34.568308
1010.490349	87015.700360	34.573325
1011.350473	87146.909755	34.578343
1012.520781	87286.439957	34.583360
1013.401363	87427.315970	34.588378
1014.410948	87563.001905	34.593396
1014.826715	87708.075596	34.598413
1016.338715	87849.678825	34.603431
1016.889689	88005.931982	34.608448
1017.769361	88156.228136	34.613466
1018.546109	88302.454501	34.618484
1019.128052	88449.884581	34.623501
1020.184824	88597.509291	34.628519
1020.836988	88760.812638	34.633536
1021.182816	88909.790614	34.638554
1022.048680	89075.288290	34.643572
1023.022890	89246.742894	34.648589
1023.876088	89419.446364	34.653607
1024.553415	89585.940605	34.658624
1025.472016	89774.785226	34.663642
1026.895820	89946.006133	34.668660
1027.807100	90136.044541	34.673677
1028.988910	90315.642387	34.678695
1030.284459	90496.399886	34.683712
1031.887958	90659.806060	34.688730
1033.925382	90803.207122	34.693748
1035.418065	90968.772722	34.698765
1036.434183	91128.880685	34.703783
1037.708654	91263.892278	34.708800
1038.922316	91407.673454	34.713818
1040.066141	91546.530685	34.718836
1040.895361	91693.142655	34.723853
1041.836005	91846.508851	34.728871
1042.558975	92010.879699	34.733888
1043.350360	92162.184059	34.738906
1044.385837	92320.575347	34.743924
1044.954652	92488.702592	34.748941
1045.936598	92665.958740	34.753959
1046.440735	92825.181543	34.758976
1047.448666	93013.498997	34.763994
1048.314160	93184.442821	34.769012
1049.328630	93378.078447	34.774029
1050.670744	93559.142439	34.779047
1051.570212	93734.021269	34.784064
1052.651225	93925.624929	34.789082
1053.490280	94107.548226	34.794100
1055.011085	94295.309926	34.799117
1056.208805	94469.866313	34.804135
1057.673201	94654.943770	34.809152
1058.774671	94840.272430	34.814170
1060.192138	95016.461102	34.819188
1061.359243	95194.249453	34.824205
1062.981260	95345.790973	34.829223
1064.155061	95499.382280	34.834240
1065.385805	95660.510158	34.839258
1066.983983	95814.622041	34.844276
1067.431255	95985.211435	34.849293
1068.525625	96140.111135	34.854311
1069.569602	96290.538578	34.859328
1070.225093	96465.648096	34.864346
1071.643924	96607.761383	34.869364
1072.458380	96786.467663	34.874381
1073.117563	96945.919564	34.879399
1074.534276	97104.570116	34.884416
1075.310166	97286.508376	34.889434
1076.286337	97450.101729	34.894452
1077.184518	97622.856184	34.899469
1078.693953	97803.563014	34.904487
1079.681772	97970.354643	34.909504
1080.336261	98152.819368	34.914522
1081.603092	98328.796975	34.919540
1082.720817	98501.141445	34.924557
1083.544993	98667.781162	34.929575
1084.540725	98850.650435	34.934592
1085.275512	99039.400902	34.939610
1086.425829	99219.240322	34.944628
1087.110719	99403.082871	34.949645
1087.671590	99601.457215	34.954663
1088.980848	99791.694834	34.959680
1090.056100	99988.778135	34.964698
1091.444291	100167.198604	34.969716
1093.005796	100335.196394	34.974733
1094.628859	100493.840680	34.979751
1096.076531	100658.731930	34.984768
1097.163947	100829.299334	34.989786
1098.513986	101000.463967	34.994804
1099.513806	101159.525525	34.999821
1100.167669	101322.272929	35.004839
1101.040956	101496.153352	35.009856
1101.732301	101671.286921	35.014874
1102.642257	101848.702847	35.019892
1103.557454	102031.475429	35.024909
1104.055365	102220.320330	35.029927
1105.110341	102418.198221	35.034944
1106.185346	102615.681781	35.039962
1107.417460	102823.309325	35.044980
1109.014925	103007.369161	35.049997
1109.997247	103213.230262	35.055015
1111.720553	103393.200860	35.060032
1112.868666	103595.434933	35.065050
1114.210100	103770.412173	35.070068
1115.737469	103967.597138	35.075085
1116.647504	104151.594989	35.080103
1117.902085	104315.870457	35.085120
1118.763314	104514.112991	35.090138
1119.884015	104706.406474	35.095156
1121.064690	104899.115721	35.100173
1122.063150	105092.825278	35.105191
1123.470574	105270.106594	35.110208
1124.420084	105479.720691	35.115226
1125.236205	105657.178227	35.120244
1126.763548	105850.894743	35.125261
1128.021198	106034.031624	35.130279
1129.602322	106220.447193	35.135296
1130.592801	106408.405368	35.140314
1131.600271	106598.173153	35.145332
1132.629426	106790.965646	35.150349
1133.356188	106990.990540	35.155367
1134.528090	107163.852754	35.160384
1135.416094	107382.218423	35.165402
1136.805263	107577.426938	35.170420
1137.363883	107783.704244	35.175437
1137.957700	107994.790237	35.180455
1139.388601	108215.846887	35.185472
1140.164658	108438.128054	35.190490
1141.385763	108652.953423	35.195508
1142.930073	108863.180097	35.200525
1144.241351	109073.218902	35.205543
1145.909285	109276.994077	35.210560
1146.897223	109492.839965	35.215578
1148.016803	109694.378239	35.220596
1149.612009	109900.627416	35.225613
1150.301176	110118.516265	35.230631
1151.509561	110311.266595	35.235648
1152.892491	110533.300251	35.240666
1153.614695	110734.633218	35.245684
1155.126654	110943.944134	35.250701
1155.440895	111162.333945	35.255719
1156.965405	111379.246350	35.260736
1157.821547	111603.187109	35.265754
1159.164946	111823.388420	35.270772
1160.540636	112025.433772	35.275789
1161.441508	112251.310575	35.280807
1162.993811	112454.077322	35.285824
1164.047029	112658.334069	35.290842
1165.699288	112867.142532	35.295860
1167.311485	113064.760779	35.300877
1168.325703	113273.056918	35.305895
1169.514833	113456.610344	35.310912
1170.690537	113636.493442	35.315930
1172.037472	113823.646350	35.320948
1172.887628	114005.865870	35.325965
1174.232186	114193.287703	35.330983
1175.861577	114371.884522	35.336000
1177.040183	114547.288411	35.341018
1177.884160	114741.637599	35.346036
1179.093698	114933.153347	35.351053
1180.081440	115118.740002	35.356071
1181.529813	115301.946114	35.361088
1182.608457	115496.882600	35.366106
1183.828792	115694.685607	35.371124
1184.412992	115884.626102	35.376141
1185.268600	116087.052979	35.381159
1186.750406	116280.395378	35.386176
1188.099556	116484.922778	35.391194
1188.995500	116710.532565	35.396212
1190.332045	116905.676965	35.401229
1191.049776	117109.768320	35.406247
1192.214758	117322.504152	35.411264
1193.047416	117552.248780	35.416282
1193.908282	117781.876578	35.421300
1195.295675	117999.053278	35.426317
1196.626019	118228.353778	35.431335
1198.039905	118441.956476	35.436352
1199.478427	118662.310032	35.441370
1200.786991	118887.020049	35.446388
1202.576636	119096.409678	35.451405
1203.640363	119321.721019	35.456423
1205.180277	119525.035044	35.461440
1206.295765	119742.764002	35.466458
1207.719781	119949.812723	35.471476
1208.836986	120155.279003	35.476493
1210.033552	120376.458552	35.481511
1211.212103	120582.171157	35.486528
1212.756662	120798.113937	35.491546
1213.728753	121013.861371	35.496564
1215.281197	121226.549468	35.501581
1216.273194	121433.794125	35.506599
1217.384876	121651.335273	35.511616
1218.286022	121867.594920	35.516634
1219.693664	122081.846429	35.521652
1221.018242	122292.349631	35.526669
1221.931279	122513.059939	35.531687
1223.521037	122732.316948	35.536704
1224.806798	122946.886335	35.541722
1226.379750	123150.473624	35.546740
1227.765206	123355.677320	35.551757
1228.680437	123573.771991	35.556775
1230.247784	123783.992301	35.561792
1231.752921	123993.793494	35.566810
1232.586999	124195.799097	35.571828
1234.191415	124413.532711	35.576845
1234.642917	124634.056175	35.581863
1236.160038	124833.139940	35.586880
1237.401020	125061.887804	35.591898
1238.590179	125279.113289	35.596916
1239.558980	125496.275329	35.601933
1240.761638	125730.572863	35.606951
1241.883922	125940.679003	35.611968
1242.599162	126161.626379	35.616986
1243.856486	126400.634678	35.622004
1244.972935	126625.549462	35.627021
1246.027081	126863.948580	35.632039
1247.206876	127094.192100	35.637056
1248.507444	127326.876205	35.642074
1249.624494	127552.380744	35.647092
1250.761221	127772.763277	35.652109
1251.896837	128008.306163	35.657127
1253.489235	128226.145235	35.662144
1254.467789	128442.794362	35.667162
1255.970251	128670.816446	35.672180
1257.180001	128885.288503	35.677197
1258.531089	129124.746215	35.682215
1259.215048	129359.892331	35.687232
1260.345145	129598.933883	35.692250
1261.359153	129841.431402	35.697268
1262.694482	130084.473511	35.702285
1263.684643	130328.994125	35.707303
1264.862506	130580.343091	35.712320
1267.075995	130822.688279	35.717338
1268.508902	131064.619127	35.722356
1270.203078	131300.665196	35.727373
1271.433404	131532.872760	35.732391
1273.262032	131759.836856	35.737408
1274.991684	131977.717538	35.742426
1276.455927	132195.770289	35.747444
1278.055179	132423.106582	35.752461
1278.970888	132642.672675	35.757479
1280.305332	132861.499321	35.762496
1281.864298	133083.979262	35.767514
1282.709052	133316.200135	35.772532
1284.287405	133535.954566	35.777549
1285.478719	133746.025987	35.782567
1286.879609	133979.681083	35.787584
1288.079962	134205.904281	35.792602
1289.097776	134432.526829	35.797620
1290.339966	134658.949132	35.802637
1291.479403	134887.266200	35.807655
1292.458047	135138.329069	35.812672
1293.976517	135381.571590	35.817690
1295.138754	135618.269773	35.822708
1296.781977	135840.133631	35.827725
1297.622876	136087.714877	35.832743
1299.072673	136330.329250	35.837760
1300.447555	136560.470132	35.842778
1301.696208	136807.710605	35.847796
1303.261344	137040.029401	35.852813
1304.609852	137278.369649	35.857831
1305.864176	137517.716060	35.862848
1307.511054	137755.706229	35.867866
1308.296446	138007.735785	35.872884
1309.839965	138238.367662	35.877901
1310.827405	138480.554325	35.882919
1311.985025	138725.744855	35.887936
1313.437470	138973.145339	35.892954
1314.340079	139234.001891	35.897972
1315.441399	139493.116015	35.902989
1317.410865	139749.375539	35.908007
1318.200092	140000.734796	35.913024
1319.645784	140249.565845	35.918042
1320.693312	140512.969574	35.923060
1321.992986	140771.122493	35.928077
1323.478195	141021.867275	35.933095
1324.637173	141287.046416	35.938112
1326.575785	141543.185111	35.943130
1327.536962	141805.788902	35.948148
1328.836433	142052.882082	35.953165
1330.549266	142309.431481	35.958183
1331.833740	142568.145703	35.963200
1333.541043	142818.537286	35.968218
1334.574464	143079.186113	35.973236
1335.893841	143326.361204	35.978253
1337.215702	143587.511497	35.983271
1337.988091	143825.599765	35.988288
1339.975443	144053.940629	35.993306
1341.114726	144303.472925	35.998324
1342.315732	144535.586075	36.003341
1343.723929	144781.869151	36.008359
1344.886768	145018.848570	36.013376
1346.340011	145260.980885	36.018394
1347.680959	145498.733038	36.023412
1349.218599	145747.093873	36.028429
1350.186339	146008.498131	36.033447
1351.650275	146263.938241	36.038464
1352.997180	146508.937257	36.043482
1353.839164	146773.538252	36.048500
1355.299978	147026.549462	36.053517
1356.908294	147279.246432	36.058535
1358.344826	147538.225687	36.063552
1359.682918	147793.786239	36.068570
1361.207568	148058.017692	36.073588
1362.435353	148327.677292	36.078605
1364.097289	148593.069424	36.083623
1364.883411	148858.062694	36.088640
1366.262627	149119.408928	36.093658
1367.338434	149402.659066	36.098676
1368.173350	149678.912298	36.103693
1369.849976	149967.698714	36.108711
1370.695110	150257.284126	36.113728
1372.305373	150543.942609	36.118746
1373.528336	150846.241959	36.123764
1374.639194	151128.599057	36.128781
1376.321899	151425.614484	36.133799
1377.629257	151732.016449	36.138816
1380.040234	151991.272137	36.143834
1381.562052	152279.696183	36.148852
1383.255979	152549.005235	36.153869
1384.884421	152845.546191	36.158887
1386.263795	153132.858732	36.163904
1387.754017	153396.195321	36.168922
1389.656632	153663.803587	36.173940
1391.247948	153943.083693	36.178957
1392.464589	154215.920710	36.183975
1393.833717	154475.961484	36.188992
1395.441529	154742.509732	36.194010
1396.834129	155011.302427	36.199028
1398.326177	155283.670291	36.204045
1399.622695	155550.909715	36.209063
1400.864395	155809.471031	36.214080
1402.234663	156068.710506	36.219098
1403.595063	156364.257333	36.224116
1404.948907	156628.209306	36.229133
1406.050429	156909.862237	36.234151
1406.970848	157189.048104	36.239168
1408.530938	157466.608157	36.244186
1409.860051	157754.470672	36.249204
1410.870939	158059.931679	36.254221
1412.380090	158335.730263	36.259239
1413.842773	158619.073646	36.264256
1415.512730	158904.186192	36.269274
1416.831874	159201.080289	36.274292
1418.106143	159495.155038	36.279309
1420.001749	159785.463156	36.284327
1421.003833	160086.894224	36.289344
1422.438314	160366.258446	36.294362
1423.480253	160671.746827	36.299380
1424.750280	160980.447543	36.304397
1426.255578	161271.135136	36.309415
1427.520486	161575.197951	36.314432
1429.321097	161870.928326	36.319450
1430.922343	162167.772085	36.324468
1432.342858	162454.092413	36.329485
1433.837149	162722.273042	36.334503
1435.130681	163002.807526	36.339520
1436.562060	163278.347836	36.344538
1437.777995	163558.962285	36.349556
1439.402515	163848.366827	36.354573
1440.565347	164130.617804	36.359591
1442.197351	164412.260370	36.364608
1443.738568	164705.211601	36.369626
1444.922983	164998.540917	36.374644
1446.343039	165275.745477	36.379661
1447.783081	165571.789748	36.384679
1449.014655	165872.425374	36.389696
1450.750526	166162.601201	36.394714
1452.350358	166467.011930	36.399732
1453.429544	166771.142762	36.404749
1454.933572	167068.557028	36.409767
1456.183283	167380.885879	36.414784
1457.548906	167696.610983	36.419802
1458.619428	167999.571769	36.424820
1460.119155	168325.493411	36.429837
1461.859808	168637.115729	36.434855
1463.038807	168973.715404	36.439872
1464.599347	169296.474654	36.444890
1465.995921	169623.044571	36.449908
1467.408540	169935.757881	36.454925
1469.329704	170254.695891	36.459943
1470.692878	170593.751679	36.464960
1472.506864	170910.250300	36.469978
1474.008616	171236.383076	36.474996
1476.090784	171551.522203	36.480013
1477.659946	171846.914491	36.485031
1479.305109	172174.108874	36.490048
1480.893923	172482.711836	36.495066
1482.119499	172810.868235	36.500084
1482.939572	173131.924107	36.505101
1485.018035	173442.762182	36.510119
1486.221300	173776.131907	36.515136
1487.835696	174110.134103	36.520154
1489.174965	174439.869399	36.525172
1490.271786	174778.809371	36.530189
1491.590288	175106.902984	36.535207
1492.969184	175450.166660	36.540224
1494.285426	175781.564783	36.545242
1495.585847	176126.039142	36.550260
1496.962816	176476.861372	36.555277
1498.967957	176819.092322	36.560295
1500.789659	177179.351643	36.565312
1502.186805	177514.771251	36.570330
1503.893321	177841.829439	36.575348
1505.204272	178189.514748	36.580365
1507.210810	178531.973137	36.585383
1508.641239	178883.920538	36.590400
1510.517617	179222.128159	36.595418
1512.286517	179535.163149	36.600436
1513.665864	179866.667164	36.605453
1515.429762	180193.680500	36.610471
1516.805800	180531.611389	36.615488
1518.538816	180856.996841	36.620506
1519.989109	181184.004809	36.625524
1521.075432	181522.548478	36.630541
1522.800268	181851.419171	36.635559
1524.457747	182187.017215	36.640576
1525.596343	182516.813840	36.645594
1527.404469	182863.255926	36.650612
1528.535638	183211.246241	36.655629
1530.100081	183532.348125	36.660647
1531.301842	183877.208815	36.665664
1533.198280	184192.307086	36.670682
1534.481046	184518.030738	36.675700
1535.530646	184853.720605	36.680717
1537.340408	185168.420038	36.685735
1538.805792	185497.191137	36.690752
1540.245919	185831.502547	36.695770
1542.303206	186148.641940	36.700788
1543.758933	186474.945354	36.705805
1545.337969	186798.120505	36.710823
1546.968021	187124.868638	36.715840
1548.442118	187456.569461	36.720858
1549.769869	187779.702918	36.725876
1551.259747	188126.878445	36.730893
1552.953487	188449.079497	36.735911
1554.128500	188789.824606	36.740928
1555.777086	189145.649976	36.745946
1557.225250	189494.148193	36.750964
1558.051905	189852.068418	36.755981
1559.475759	190205.804843	36.760999
1561.014119	190567.762988	36.766016
1562.298788	190940.225229	36.771034
1563.734723	191309.770582	36.776052
1565.210692	191696.322042	36.781069
1566.705683	192066.522475	36.786087
1568.082102	192456.141949	36.791104
1569.865357	192835.972775	36.796122
1571.599669	193214.760409	36.801140
1573.448608	193614.135043	36.806157
1575.283144	194005.097999	36.811175
1576.597451	194374.060166	36.816192
1578.172955	194758.888232	36.821210
1580.291804	195146.193424	36.826228
1581.658624	195536.519592	36.831245
1583.986846	195902.416315	36.836263
1586.494147	196263.715308	36.841280
1588.302971	196633.751744	36.846298
1590.056609	196988.425273	36.851316
1591.666778	197360.555335	36.856333
1593.488360	197709.597513	36.861351
1594.706069	198077.187949	36.866368
1595.866912	198442.301473	36.871386
1597.828815	198806.408835	36.876404
1599.164898	199181.019352	36.881421
1600.852452	199533.318048	36.886439
1602.542353	199894.378430	36.891456
1604.014718	200276.920260	36.896474
1605.879772	200627.963866	36.901492
1607.697943	201003.177845	36.906509
1609.460460	201352.401134	36.911527
1610.823466	201705.272467	36.916544
1612.798940	202066.805032	36.921562
1614.428069	202433.424403	36.926580
1615.855865	202797.996674	36.931597
1617.848673	203150.479332	36.936615
1619.052917	203518.977335	36.941632
1620.667432	203880.705677	36.946650
1622.727646	204228.027644	36.951668
1624.099935	204587.437882	36.956685
1625.201032	204957.369562	36.961703
1626.850653	205320.876816	36.966720
1628.457932	205694.271114	36.971738
1630.276563	206060.242709	36.976756
1631.994587	206427.515097	36.981773
1634.093153	206778.347094	36.986791
1635.820021	207121.204674	36.991808
1637.211752	207502.528457	36.996826
1639.151052	207857.099285	37.001844
1640.188702	208213.788599	37.006861
1641.760403	208551.840392	37.011879
1642.873294	208900.597179	37.016896
1644.115117	209261.269969	37.021914
1645.974798	209612.992178	37.026932
1647.322775	209978.755139	37.031949
1648.736298	210352.229181	37.036967
1650.164837	210712.776064	37.041984
1651.235890	211085.751249	37.047002
1652.737157	211458.898391	37.052020
1654.341987	211844.423362	37.057037
1656.249690	212230.763595	37.062055
1657.914701	212614.504422	37.067072
1659.193257	213004.736008	37.072090
1660.688317	213405.016034	37.077108
1662.023533	213814.365458	37.082125
1663.797152	214208.076284	37.087143
1665.883198	214616.924607	37.092160
1667.477710	215038.808336	37.097178
1669.153667	215444.096330	37.102196
1670.728535	215870.253879	37.107213
1672.429543	216283.363790	37.112231
1674.680262	216696.638821	37.117248
1676.113133	217117.288903	37.122266
1678.093127	217532.796464	37.127284
1679.563816	217977.597254	37.132301
1681.318388	218441.452444	37.137319
1683.331981	218840.756272	37.142336
1685.104699	219245.816028	37.147354
1687.612850	219651.949812	37.152372
1689.548459	220072.682115	37.157389
1691.017036	220473.428504	37.162407
1693.276991	220875.290420	37.167424
1695.267114	221266.861199	37.172442
1697.227893	221649.980535	37.177460
1699.023005	222046.691529	37.182477
1700.090981	222444.438323	37.187495
1702.092762	222839.670421	37.192512
1703.145550	223256.852894	37.197530
1704.962140	223654.252006	37.202548
1706.099212	224068.451934	37.207565
1707.658020	224479.104099	37.212583
1708.899734	224897.531480	37.217600
1710.303098	225338.183674	37.222618
1711.906569	225760.643806	37.227636
1713.558965	226199.657973	37.232653
1715.155554	226644.982104	37.237671
1717.045655	227079.083504	37.242688
1718.209381	227528.495455	37.247706
1719.899868	227977.949123	37.252724
1721.907290	228438.375767	37.257741
1723.583530	228886.742794	37.262759
1725.530247	229340.934220	37.267776
1726.937301	229796.689470	37.272794
1728.931868	230248.259866	37.277812
1731.184771	230696.588672	37.282829
1732.719349	231153.165658	37.287847
1734.806107	231588.519618	37.292864
1736.257289	232043.919413	37.297882
1738.260395	232485.894117	37.302900
1740.268234	232937.140729	37.307917
1742.078174	233378.006926	37.312935
1744.041808	233808.536194	37.317952
1745.621294	234257.749118	37.322970
1747.950791	234682.759196	37.327988
1749.849742	235128.543526	37.333005
1751.484860	235568.530287	37.338023
1753.492111	235982.775945	37.343040
1755.157410	236409.297176	37.348058
1756.845529	236811.963614	37.353076
1758.441085	237237.863366	37.358093
1759.702432	237651.372441	37.363111
1761.241208	238063.871429	37.368128
1762.578411	238495.659184	37.373146
1764.455575	238919.941507	37.378164
1765.631733	239353.281904	37.383181
1767.090616	239793.358957	37.388199
1768.850817	240225.080804	37.393216
1770.498515	240671.047308	37.398234
1772.491779	241127.575866	37.403252
1774.123444	241580.938976	37.408269
1775.716947	242042.590466	37.413287
1777.599721	242493.424605	37.418304
1779.183646	242961.531741	37.423322
1781.231968	243411.375065	37.428340
1783.102984	243884.644150	37.433357
1784.987012	244341.171734	37.438375
1786.669698	244815.921583	37.443392
1788.241319	245282.536375	37.448410
1790.235224	245759.116351	37.453428
1792.160878	246234.641485	37.458445
1793.574006	246704.536337	37.463463
1795.525253	247186.206247	37.468480
1796.949109	247671.063050	37.473498
1800.156018	248125.066809	37.478516
1802.994196	248576.617130	37.483533
1804.698834	249045.070154	37.488551
1806.926035	249499.440557	37.493568
1808.807447	249962.403951	37.498586
1811.053478	250408.567161	37.503604
1812.887439	250838.286864	37.508621
1815.117857	251281.024167	37.513639
1817.090913	251718.012461	37.518656
1818.754686	252156.652574	37.523674
1820.736149	252598.593877	37.528692
1822.264407	253046.478440	37.533709
1823.878762	253480.072581	37.538727
1825.933573	253924.593955	37.543744
1827.133458	254380.357870	37.548762
1829.158055	254815.561855	37.553780
1830.932646	255259.241211	37.558797
1832.500803	255733.997629	37.563815
1834.282748	256181.562954	37.568832
1835.740899	256642.975870	37.573850
1837.532658	257109.236779	37.578868
1839.021326	257576.386167	37.583885
1841.016628	258045.789230	37.588903
1842.810467	258524.650275	37.593920
1844.282561	258992.031398	37.598938
1846.164256	259473.901119	37.603956
1848.168051	259950.263633	37.608973
1849.986819	260433.007519	37.613991
1852.605748	260885.135435	37.619008
1854.543389	261363.134662	37.624026
1856.350550	261830.714599	37.629044
1858.305844	262303.706326	37.634061
1860.110846	262778.577178	37.639079
1861.989842	263247.999387	37.644096
1863.526633	263721.034348	37.649114
1865.379360	264192.924666	37.654132
1867.363222	264679.044367	37.659149
1869.039723	265150.379029	37.664167
1870.973564	265621.061301	37.669184
1872.102605	266118.193766	37.674202
1873.907692	266604.062364	37.679220
1875.902469	267096.605746	37.684237
1877.739824	267582.214233	37.689255
1879.211210	268057.950049	37.694272
1880.701399	268528.474700	37.699290
1882.384022	268997.011128	37.704308
1884.408747	269474.864385	37.709325
1885.881889	269964.671329	37.714343
1888.241389	270454.433110	37.719360
1889.875938	270948.505371	37.724378
1891.678575	271439.704143	37.729396
1893.875859	271926.899713	37.734413
1895.652241	272428.211818	37.739431
1897.774770	272923.928268	37.744448
1899.204708	273425.118191	37.749466
1901.221055	273928.319008	37.754484
1903.193697	274424.261022	37.759501
1904.806864	274946.629432	37.764519
1906.973747	275455.950205	37.769536
1908.685959	275976.242711	37.774554
1910.536690	276488.204715	37.779572
1912.789975	277004.697124	37.784589
1914.295165	277532.768322	37.789607
1916.415210	278055.148413	37.794624
1918.509310	278575.143786	37.799642
1920.591651	279107.231347	37.804660
1922.799179	279620.778788	37.809677
1924.388540	280160.438690	37.814695
1926.753927	280679.368136	37.819712
1928.818129	281210.081624	37.824730
1930.391032	281731.272800	37.829748
1932.438193	282268.235058	37.834765
1934.253170	282806.707367	37.839783
1936.103367	283346.518561	37.844800
1938.382273	283885.139730	37.849818
1939.749561	284429.497927	37.854836
1942.360526	284966.028809	37.859853
1944.512877	285499.712448	37.864871
1946.814957	286027.120926	37.869888
1948.828165	286574.921641	37.874906
1950.587652	287103.965480	37.879924
1952.671565	287634.935249	37.884941
1954.251526	288168.094534	37.889959
1956.018193	288713.819887	37.894976
1958.049094	289262.598474	37.899994
1959.710982	289818.166957	37.905012
1961.783304	290358.907819	37.910029
1963.848274	290913.313163	37.915047
1966.384642	291448.054823	37.920064
1969.183439	291985.824442	37.925082
1971.309546	292522.915372	37.930100
1973.489273	293056.286788	37.935117
1975.226502	293590.236908	37.940135
1977.577886	294105.719380	37.945152
1979.763684	294633.444200	37.950170
1981.664594	295160.934276	37.955188
1983.930108	295685.517107	37.960205
1985.265430	296207.228463	37.965223
1987.235459	296714.736189	37.970240
1989.505823	297247.057780	37.975258
1991.571324	297782.407677	37.980276
1993.892090	298289.443946	37.985293
1995.805410	298812.063642	37.990311
1998.072868	299319.027622	37.995328
2000.211978	299834.112428	38.000346
2002.124219	300344.279412	38.005364
2004.077714	300843.033246	38.010381
2005.842615	301371.150501	38.015399
2007.615906	301894.590349	38.020416
2009.424074	302409.107026	38.025434
2011.111008	302917.850303	38.030452
2012.909051	303427.232891	38.035469
2014.491748	303935.175210	38.040487
2016.161088	304442.973499	38.045504
2018.116415	304965.934709	38.050522
2019.699445	305487.227340	38.055540
2021.602456	306006.076889	38.060557
2023.331506	306542.475827	38.065575
2025.173796	307077.913160	38.070592
2027.113708	307620.569074	38.075610
2028.810952	308182.156373	38.080628
2031.011809	308725.320982	38.085645
2033.348313	309282.757593	38.090663
2035.487317	309833.061468	38.095680
2037.507034	310387.876353	38.100698
2039.358543	310950.790928	38.105716
2041.811013	311499.812881	38.110733
2043.759190	312070.499974	38.115751
2045.972190	312630.422654	38.120768
2048.263969	313187.255575	38.125786
2050.099138	313763.510354	38.130804
2052.342688	314336.189028	38.135821
2054.457314	314901.317198	38.140839
2056.324440	315466.354951	38.145856
2058.784428	316031.823880	38.150874
2060.484257	316623.086611	38.155892
2062.630870	317191.950162	38.160909
2064.747300	317781.839634	38.165927
2066.398392	318363.116604	38.170944
2068.267775	318964.920800	38.175962
2070.036621	319565.263615	38.180980
2072.079371	320161.874162	38.185997
2073.844538	320779.524421	38.191015
2076.055573	321388.386136	38.196032
2078.155549	322003.710061	38.201050
2080.024254	322624.246222	38.206068
2082.220075	323227.659799	38.211085
2084.543686	323858.037081	38.216103
2086.821988	324467.341517	38.221120
2089.333649	325091.251824	38.226138
2092.153379	325700.251980	38.231156
2094.452030	326296.078666	38.236173
2096.491603	326899.914656	38.241191
2098.868377	327510.036407	38.246208
2100.737997	328113.507579	38.251226
2102.541056	328730.617450	38.256244
2104.857602	329332.174653	38.261261
2107.040528	329950.453240	38.266279
2108.686428	330562.796921	38.271296
2110.640079	331176.302006	38.276314
2112.298751	331799.039456	38.281332
2114.562199	332427.204776	38.286349
2116.885809	333069.849102	38.291367
2118.487559	333701.485794	38.296384
2120.706829	334329.408620	38.301402
2122.751934	334969.208278	38.306420
2124.939340	335589.760005	38.311437
2127.386594	336236.078733	38.316455
2129.523846	336874.216041	38.321472
2132.106336	337511.434584	38.326490
2133.789322	338152.423767	38.331508
2136.174118	338787.273325	38.336525
2138.012672	339425.632036	38.341543
2139.671887	340069.520652	38.346560
2142.982758	340682.288155	38.351578
2145.558435	341331.390932	38.356596
2147.492067	341943.761078	38.361613
2149.698554	342575.699231	38.366631
2151.574687	343193.723732	38.371648
2153.568081	343799.461800	38.376666
2155.523266	344403.015864	38.381684
2157.823667	345004.652674	38.386701
2159.931172	345597.506673	38.391719
2161.848559	346205.562147	38.396736
2163.860183	346804.432093	38.401754
2165.665170	347430.586343	38.406772
2167.927013	348040.820140	38.411789
2170.050697	348669.113216	38.416807
2172.170229	349287.043912	38.421824
2175.641205	349880.329417	38.426842
2177.772766	350489.638589	38.431860
2179.961332	351095.453405	38.436877
2182.544986	351722.384980	38.441895
2184.791466	352332.665287	38.446912
2186.866618	352927.105036	38.451930
2189.720722	353518.946801	38.456948
2192.256487	354114.360310	38.461965
2194.439583	354715.558707	38.466983
2196.696876	355319.553151	38.472000
2199.120891	355912.321267	38.477018
2201.093534	356519.517568	38.482036
2203.246880	357114.495762	38.487053
2204.995658	357721.686325	38.492071
2206.674109	358339.409655	38.497088
2208.770997	358954.162278	38.502106
2210.586373	359583.313115	38.507124
2212.854690	360222.503161	38.512141
2214.991218	360851.886004	38.517159
2217.058533	361502.176594	38.522176
2219.152383	362145.652860	38.527194
2221.591849	362790.939215	38.532212
2223.461026	363431.133608	38.537229
2225.751669	364089.083124	38.542247
2227.741894	364752.424098	38.547264
2230.067929	365414.556814	38.552282
2232.651494	366078.842815	38.557300
2234.916807	366730.460421	38.562317
2237.175773	367390.058796	38.567335
2239.329508	368059.936812	38.572352
2241.774045	368712.657801	38.577370
2244.255232	369389.992112	38.582388
2246.470966	370058.606687	38.587405
2248.744895	370721.441672	38.592423
2251.038394	371391.820274	38.597440
2252.838160	372068.203323	38.602458
2254.838242	372745.758261	38.607476
2256.892161	373434.857415	38.612493
2259.031853	374132.603393	38.617511
2260.720461	374830.765221	38.622528
2263.248043	375524.083023	38.627546
2265.284492	376221.957199	38.632564
2267.529276	376944.256544	38.637581
2270.009183	377643.348041	38.642599
2272.220435	378350.077747	38.647616
2275.346508	379042.745133	38.652634
2277.534114	379750.996870	38.657652
2279.955580	380439.669338	38.662669
2282.268558	381143.763307	38.667687
2284.630465	381845.171965	38.672704
2286.978087	382539.290872	38.677722
2289.508011	383241.276418	38.682740
2291.293366	383943.445918	38.687757
2293.837066	384643.320202	38.692775
2296.116760	385350.829456	38.697792
2298.539456	386046.307240	38.702810
2300.304390	386750.574817	38.707828
2302.550499	387453.885638	38.712845
2304.997468	388140.922291	38.717863
2306.559605	388829.585776	38.722880
2308.542338	389515.072059	38.727898
2310.645124	390212.894828	38.732916
2312.305539	390907.302003	38.737933
2314.416853	391621.062561	38.742951
2316.621400	392346.096992	38.747968
2319.111711	393065.414526	38.752986
2322.147423	393776.868779	38.758004
2324.545208	394494.570995	38.763021
2327.297742	395205.582229	38.768039
2329.370214	395921.200427	38.773056
2331.554706	396645.299160	38.778074
2334.235534	397363.266392	38.783092
2336.360120	398084.982877	38.788109
2338.904267	398808.665364	38.793127
2340.541310	399548.952526	38.798144
2343.255229	400284.963240	38.803162
2345.845995	401013.423768	38.808180
2348.361305	401760.301323	38.813197
2351.011220	402483.215916	38.818215
2353.236714	403229.596150	38.823232
2355.521919	403975.060077	38.828250
2358.266057	404715.259646	38.833268
2360.272148	405446.034428	38.838285
2363.421914	406175.410719	38.843303
2365.981525	406914.873100	38.848320
2368.311487	407651.617347	38.853338
2370.649180	408394.953086	38.858356
2372.647368	409143.974223	38.863373
2375.450734	409896.946103	38.868391
2377.564216	410651.378823	38.873408
2380.131250	411387.603115	38.878426
2382.804538	412151.375805	38.883444
2385.182393	412893.745490	38.888461
2387.591347	413638.217068	38.893479
2390.133329	414384.444169	38.898496
2393.027200	415124.183949	38.903514
2395.513089	415859.664359	38.908532
2397.888650	416602.309851	38.913549
2400.573329	417335.968188	38.918567
2402.673426	418077.654393	38.923584
2405.234314	418823.042007	38.928602
2407.588774	419571.936712	38.933620
2409.778519	420324.407191	38.938637
2412.093991	421080.835622	38.943655
2414.415055	421835.797098	38.948672
2416.687896	422584.286889	38.953690
2419.091406	423343.063520	38.958708
2421.171459	424113.087006	38.963725
2423.307544	424879.000951	38.968743
2425.498357	425660.224904	38.973760
2427.629000	426437.889459	38.978778
2430.318604	427211.437063	38.983796
2432.115598	427996.195508	38.988813
2434.731712	428796.134293	38.993831
2437.205279	429602.044107	38.998848
2439.213120	430398.941444	39.003866
2441.368770	431202.622114	39.008884
2443.785757	432026.633544	39.013901
2446.234997	432829.704313	39.018919
2448.782692	433646.297427	39.023936
2451.283945	434467.121563	39.028954
2454.000855	435273.607485	39.033972
2456.596780	436086.158966	39.038989
2459.056766	436895.768690	39.044007
2461.476846	437714.314499	39.049024
2464.047249	438521.267374	39.054042
2466.678043	439317.554165	39.059060
2468.927155	440092.520427	39.064077
2471.440163	440865.038153	39.069095
2474.016521	441645.260898	39.074112
2476.578982	442412.859259	39.079130
2479.749788	443177.800905	39.084148
2481.492979	443963.544260	39.089165
2484.336222	444726.968357	39.094183
2486.901038	445514.241082	39.099200
2489.677340	446284.199000	39.104218
2492.786973	447042.540340	39.109236
2494.955342	447822.611209	39.114253
2497.431402	448590.159062	39.119271
2499.802466	449368.319433	39.124288
2502.525395	450145.483020	39.129306
2504.805032	450933.313185	39.134324
2506.897207	451731.564139	39.139341
2509.220398	452514.270472	39.144359
2511.625699	453330.717919	39.149376
2513.917084	454142.600804	39.154394
2516.442334	454956.942065	39.159412
2518.404479	455776.805631	39.164429
2521.536816	456588.605977	39.169447
2524.249489	457409.949630	39.174464
2526.503189	458229.111299	39.179482
2529.333730	459055.577399	39.184500
2531.680392	459893.667539	39.189517
2534.096209	460737.323330	39.194535
2536.943144	461569.902497	39.199552
2538.680064	462425.226870	39.204570
2541.400176	463273.578890	39.209588
2543.244811	464134.423248	39.214605
2545.725361	464995.074839	39.219623
2548.520882	465870.799931	39.224640
2551.018570	466748.304013	39.229658
2553.398726	467622.402010	39.234676
2555.690002	468514.314771	39.239693
2558.615667	469391.881858	39.244711
2560.881782	470294.834176	39.249728
2563.383621	471201.899152	39.254746
2566.381818	472102.927659	39.259764
2568.881585	473008.694495	39.264781
2571.509003	473911.113102	39.269799
2574.212364	474811.606841	39.274816
2576.718002	475710.978672	39.279834
2580.066148	476603.348914	39.284852
2583.251462	477485.398735	39.289869
2586.013516	478375.406498	39.294887
2588.875470	479258.889972	39.299904
2591.622485	480157.400543	39.304922
2594.830780	481034.226381	39.309940
2597.328354	481905.370228	39.314957
2600.036780	482771.286803	39.319975
2602.462082	483648.065182	39.324992
2605.109659	484520.825855	39.330010
2607.937563	485380.235384	39.335028
2610.160408	486241.319002	39.340045
2613.765057	487110.715826	39.345063
2616.378375	487982.707160	39.350080
2618.747326	488845.104443	39.355098
2621.660759	489698.081753	39.360116
2624.547960	490545.873388	39.365133
2627.897569	491370.582262	39.370151
2630.959078	492203.223529	39.375168
2633.966064	493034.016956	39.380186
2636.865676	493856.612627	39.385204
2639.049440	494676.461040	39.390221
2641.421688	495474.994957	39.395239
2644.406569	496256.284956	39.400256
2646.586564	497041.859735	39.405274
2649.041840	497823.467816	39.410292
2651.057539	498618.128935	39.415309
2653.100545	499415.775119	39.420327
2655.553658	500220.176712	39.425344
2657.652049	501030.399326	39.430362
2659.888217	501853.876726	39.435380
2661.906870	502700.047182	39.440397
2664.248567	503542.691475	39.445415
2666.655353	504396.024652	39.450432
2668.379910	505272.826507	39.455450
2671.199014	506148.947217	39.460468
2673.232146	507037.757140	39.465485
2675.848464	507946.188528	39.470503
2678.711580	508840.864278	39.475520
2680.976253	509774.411046	39.480538
2683.774885	510698.388031	39.485556
2686.603383	511624.272916	39.490573
2688.917630	512555.229814	39.495591
2692.007260	513487.819064	39.500608
2694.552936	514432.136661	39.505626
2697.377752	515377.712576	39.510644
2699.982423	516338.437487	39.515661
2702.335931	517304.436263	39.520679
2705.347452	518250.715085	39.525696
2707.725146	519219.614558	39.530714
2711.310417	520178.479733	39.535732
2714.203148	521160.272674	39.540749
2717.579832	522134.215228	39.545767
2720.570056	523094.205579	39.550784
2723.177712	524067.798976	39.555802
2726.306189	525018.880399	39.560820
2729.604671	525975.716429	39.565837
2732.461823	526925.564086	39.570855
2735.683128	527873.529077	39.575872
2738.296754	528824.958378	39.580890
2741.423870	529774.278570	39.585908
2744.542357	530712.512940	39.590925
2747.150264	531637.933632	39.595943
2750.536998	532564.426472	39.600960
2753.047179	533518.037992	39.605978
2755.738431	534444.627372	39.610996
2758.495225	535385.592857	39.616013
2761.143093	536333.913951	39.621031
2763.682180	537273.182357	39.626048
2766.137612	538234.092967	39.631066
2768.551892	539190.920541	39.636084
2771.152247	540161.390100	39.641101
2774.023962	541104.982170	39.646119
2777.088365	542054.818997	39.651136
2780.043899	543027.298509	39.656154
2782.890551	543981.971942	39.661172
2785.514154	544933.850899	39.666189
2788.111451	545900.909456	39.671207
2791.264472	546870.575640	39.676224
2793.570592	547835.838133	39.681242
2796.449543	548814.868319	39.686260
2799.217082	549792.691072	39.691277
2802.060806	550761.029748	39.696295
2804.831170	551727.150401	39.701312
2807.332534	552706.468661	39.706330
2810.647597	553675.428334	39.711348
2813.319893	554657.845481	39.716365
2815.795112	555637.861588	39.721383
2818.402013	556612.206283	39.726400
2821.391961	557597.774572	39.731418
2824.521305	558557.921460	39.736436
2827.329423	559513.881817	39.741453
2830.019609	560455.323047	39.746471
2833.139412	561383.614708	39.751488
2835.684721	562326.353532	39.756506
2838.592806	563263.489848	39.761524
2841.502555	564214.070507	39.766541
2843.871527	565155.480141	39.771559
2846.292914	566111.126287	39.776576
2848.603378	567078.019451	39.781594
2851.161161	568047.511305	39.786612
2853.818591	569024.294865	39.791629
2856.408665	570019.993332	39.796647
2859.142057	571023.372274	39.801664
2861.718417	572034.027323	39.806682
2864.238724	573049.379940	39.811700
2867.396880	574070.920440	39.816717
2869.933321	575092.932651	39.821735
2872.754550	576135.490091	39.826752
2875.421447	577171.664141	39.831770
2878.069089	578227.223006	39.836788
2880.979284	579291.378818	39.841805
2884.041444	580360.535393	39.846823
2887.083708	581433.064125	39.851840
2890.066499	582520.506231	39.856858
2892.830029	583583.966049	39.861876
2895.837418	584674.673946	39.866893
2898.291309	585759.007600	39.871911
2901.637634	586850.618420	39.876928
2904.752986	587954.451897	39.881946
2907.644516	589047.343469	39.886964
2910.573633	590146.395323	39.891981
2913.457635	591249.764591	39.896999
2916.722713	592345.051083	39.902016
2919.700708	593454.114853	39.907034
2922.752910	594564.566055	39.912052
2926.023973	595668.313756	39.917069
2929.305905	596774.511331	39.922087
2932.623927	597872.483963	39.927104
2935.606250	598976.369399	39.932122
2938.356650	600085.397268	39.937140
2941.873353	601184.027360	39.942157
2945.406565	602293.266243	39.947175
2948.116839	603372.042667	39.952192
2950.974119	604469.417593	39.957210
2954.400385	605562.689242	39.962228
2957.372708	606647.672270	39.967245
2960.655532	607737.205486	39.972263
2964.095837	608812.345583	39.977280
2967.333062	609890.369387	39.982298
2970.145673	610958.052981	39.987316
2973.286572	612035.286998	39.992333
2976.008562	613128.344567	39.997351
2978.690932	614195.641265	40.002368
2981.880633	615287.409814	40.007386
2984.739750	616351.569552	40.012404
2987.832542	617420.889081	40.017421
2990.655891	618497.799508	40.022439
2994.157285	619556.294106	40.027456
2997.081736	620640.677049	40.032474
3000.308155	621704.408181	40.037492
3003.495156	622773.689802	40.042509
3006.570933	623840.785396	40.047527
3010.135266	624898.400515	40.052544
3013.503100	625940.904282	40.057562
3016.191167	626991.063168	40.062580
3019.075909	628038.638882	40.067597
3022.065647	629091.589350	40.072615
3024.344864	630133.714285	40.077632
3027.183158	631165.556507	40.082650
3030.027491	632196.448257	40.087668
3032.962746	633217.737161	40.092685
3035.777363	634252.677010	40.097703
3038.431762	635289.088816	40.102720
3041.089509	636315.813182	40.107738
3044.025383	637359.411016	40.112756
3046.961112	638407.545606	40.117773
3049.555992	639470.301860	40.122791
3051.930168	640537.625732	40.127808
3054.785686	641627.161484	40.132826
3057.188441	642729.327629	40.137844
3060.530935	643831.220358	40.142861
3063.474545	644961.389568	40.147879
3066.373231	646069.098664	40.152896
3069.834756	647188.162825	40.157914
3073.011521	648313.681698	40.162932
3075.945428	649438.566555	40.167949
3079.045242	650574.863025	40.172967
3082.089202	651715.475837	40.177984
3085.393446	652865.434368	40.183002
3088.402609	654006.787547	40.188020
3091.654767	655155.642553	40.193037
3094.815960	656309.311272	40.198055
3098.051276	657475.336071	40.203072
3100.999121	658649.239167	40.208090
3104.401490	659811.820919	40.213108
3107.353625	660980.264175	40.218125
3110.032499	662160.312858	40.223143
3113.695312	663337.516967	40.228160
3116.543596	664521.083554	40.233178
3119.625966	665724.574014	40.238196
3123.312475	666915.920324	40.243213
3126.370017	668110.406677	40.248231
3129.607738	669298.992344	40.253248
3132.926045	670497.962606	40.258266
3135.853811	671700.625965	40.263284
3139.342359	672893.495067	40.268301
3142.628362	674100.269805	40.273319
3145.768159	675295.428031	40.278336
3148.723099	676490.961376	40.283354
3151.963978	677699.318195	40.288372
3155.395981	678891.084946	40.293389
3158.525552	680103.521252	40.298407
3161.780758	681308.722060	40.303424
3165.039177	682517.292259	40.308442
3167.955396	683727.250189	40.313460
3171.305299	684945.420693	40.318477
3174.103422	686164.016236	40.323495
3177.167239	687380.418647	40.328512
3180.403877	688594.693203	40.333530
3183.040836	689847.674584	40.338548
3186.694781	691077.481832	40.343565
3189.295088	692321.140897	40.348583
3192.435759	693551.487698	40.353600
3195.839071	694792.934033	40.358618
3199.267810	696038.022902	40.363636
3203.086629	697275.283790	40.368653
3206.407480	698516.817964	40.373671
3209.832718	699732.424209	40.378688
3213.220719	700963.040185	40.383706
3216.454527	702193.558327	40.388724
3220.020234	703406.747941	40.393741
3223.008162	704633.542261	40.398759
3226.641189	705853.912428	40.403776
3229.896702	707069.267681	40.408794
3233.102551	708282.577476	40.413812
3236.210120	709480.823241	40.418829
3239.249299	710669.998378	40.423847
3242.241506	711852.380464	40.428864
3245.148274	713018.075866	40.433882
3247.875928	714190.670632	40.438900
3251.244652	715374.283106	40.443917
3254.293310	716571.244055	40.448935
3257.145853	717764.009666	40.453952
3260.342658	718963.673914	40.458970
3263.302477	720183.240574	40.463988
3266.375039	721388.266579	40.469005
3269.648955	722610.097617	40.474023
3272.579929	723843.672826	40.479040
3275.973948	725079.410541	40.484058
3279.149246	726331.707574	40.489076
3282.332236	727576.695542	40.494093
3285.333050	728838.376048	40.499111
3288.634604	730098.478341	40.504128
3291.817601	731372.238107	40.509146
3295.140894	732642.366970	40.514164
3298.924103	733916.764609	40.519181
3302.339154	735210.526564	40.524199
3305.449546	736485.863639	40.529216
3308.998350	737777.462625	40.534234
3312.355064	739074.610066	40.539252
3316.248121	740362.131729	40.544269
3319.830771	741658.278524	40.549287
3322.731239	742952.549983	40.554304
3326.665501	744235.440312	40.559322
3329.795942	745535.563819	40.564340
3332.976288	746832.308436	40.569357
3336.604253	748143.504989	40.574375
3339.868138	749456.217297	40.579392
3343.449320	750764.368554	40.584410
3346.372582	752079.207530	40.589428
3349.845745	753395.210550	40.594445
3353.220026	754712.877181	40.599463
3356.043509	756043.459640	40.604480
3359.561262	757376.454336	40.609498
3362.464784	758725.859418	40.614516
3365.807597	760069.637264	40.619533
3368.833969	761411.507122	40.624551
3372.306233	762763.940095	40.629568
3375.972982	764119.788503	40.634586
3379.620049	765482.872363	40.639604
3384.302339	766811.260936	40.644621
3388.358885	768147.285432	40.649639
3391.657055	769493.617556	40.654656
3395.745114	770808.561052	40.659674
3398.800582	772135.727153	40.664692
3402.594205	773457.767361	40.669709
3405.944478	774766.183028	40.674727
3409.295143	776085.515132	40.679744
3412.858831	777415.820226	40.684762
3416.007318	778730.092475	40.689780
3419.555907	780043.423465	40.694797
3423.222895	781363.417825	40.699815
3426.517173	782676.902570	40.704832
3430.397751	783992.750203	40.709850
3433.356110	785312.825907	40.714868
3436.846196	786617.857630	40.719885
3440.327087	787944.277819	40.724903
3443.092274	789266.647104	40.729920
3446.872769	790573.015610	40.734938
3449.906937	791914.552824	40.739956
3453.234626	793215.215513	40.744973
3456.541891	794563.211478	40.749991
3459.907883	795894.530658	40.755008
3463.633692	797198.854428	40.760013
3467.233826	798468.536773	40.765018
3470.207121	799676.741602	40.770023
3473.412850	800833.075021	40.775028
3476.103747	801928.952123	40.780032
3479.521580	802958.407977	40.785037
3482.057380	803933.852127	40.790042
3484.711322	804825.226169	40.795047
3486.948613	805657.561604	40.800052
3489.041894	806440.199870	40.805056
3491.594502	807151.192612	40.810061
3493.824225	807825.986618	40.815066
3495.808160	808411.641045	40.820071
3497.824748	808946.559783	40.825076
3499.287683	809441.829578	40.830080
3500.854172	809862.702853	40.835085
3502.560504	810249.714118	40.840090
3503.808516	810602.232633	40.845095
3505.622356	810897.800264	40.850100
3506.490492	811164.455177	40.855104
3507.827205	811373.501094	40.860109
3508.525882	811561.136934	40.865114
3509.738858	811712.525555	40.870119
3510.372284	811828.535455	40.875124
3511.161139	811916.396244	40.880128
3512.520180	811979.519123	40.885133
3512.934384	812007.131219	40.890138
3513.434508	812015.083454	40.895143
3514.174323	812004.477380	40.900148
3514.422505	811977.833968	40.905152
3515.131430	811922.748111	40.910157
3515.141301	811842.153751	40.915162
3515.466785	811752.834606	40.920167
3516.198996	811646.495307	40.925172
3516.238338	811533.311172	40.930176
3516.847909	811402.833648	40.935181
3517.218516	811261.123672	40.940186
3517.304539	811105.248164	40.945191
3517.465351	810929.953016	40.950196
3517.474355	810752.865321	40.955200
3517.862169	810575.955624	40.960205
3517.908196	810388.414903	40.965210
3518.158574	810174.568792	40.970215
3518.287181	809963.627391	40.975220
3518.100506	809756.995068	40.980224
3518.436214	809535.469582	40.985229
3518.654921	809299.840964	40.990234
3518.436448	809074.225810	40.995239
3518.688623	808842.987032	41.000244
3518.698384	808600.849742	41.005248
3519.153631	808356.326638	41.010253
3518.738460	808112.820503	41.015258
3518.452633	807847.763930	41.020263
3518.751450	807594.758590	41.025268
3518.566215	807346.824192	41.030272
3518.687309	807081.082565	41.035277
3518.661609	806823.885841	41.040282
3518.644384	806566.236784	41.045287
3518.457717	806296.347782	41.050292
3518.498914	806036.904027	41.055296
3518.480753	805759.807105	41.060301
3518.216340	805499.804941	41.065306
3518.128885	805237.066570	41.070311
3518.381550	804955.528004	41.075316
3518.106689	804695.055728	41.080320
3518.022638	804424.880091	41.085325
3517.839016	804163.097452	41.090330
3517.849689	803897.741272	41.095335
3517.768677	803630.133598	41.100340
3517.465523	803369.174364	41.105344
3517.574480	803096.069730	41.110349
3517.310567	802826.842192	41.115354
3517.020553	802555.106430	41.120359
3517.182526	802310.563557	41.125364
3517.094329	802046.673400	41.130368
3517.311794	801781.299952	41.135373
3517.079858	801509.268213	41.140378
3516.552630	801247.137230	41.145383
3516.860279	800991.826818	41.150388
3516.534639	800728.759760	41.155392
3516.577222	800465.916520	41.160397
3516.572215	800215.192935	41.165402
3515.972845	799963.920191	41.170407
3516.099108	799712.518836	41.175412
3515.964852	799467.237379	41.180416
3516.390657	799200.798413	41.185421
3515.941959	798953.685495	41.190426
3515.650370	798697.064213	41.195431
3515.793243	798441.687307	41.200436
3515.502526	798198.743198	41.205440
3515.568890	797951.706278	41.210445
3515.370304	797714.572070	41.215450
3515.002730	797463.220018	41.220455
3515.055937	797222.099994	41.225460
3514.566685	796983.957830	41.230464
3514.771261	796744.956768	41.235469
3514.499377	796512.605696	41.240474
3514.272574	796282.694670	41.245479
3514.076963	796058.663582	41.250484
3514.414005	795828.251934	41.255488
3514.444282	795589.927686	41.260493
3514.279210	795362.333519	41.265498
3513.805883	795132.670947	41.270503
3514.050976	794909.218135	41.275508
3513.583531	794688.576899	41.280512
3513.595011	794459.500075	41.285517
3513.445362	794242.770928	41.290522
3513.587794	794027.509697	41.295527
3513.477085	793805.897869	41.300532
3513.045535	793600.640552	41.305536
3513.109801	793375.695175	41.310541
3513.162192	793165.482207	41.315546
3512.912324	792953.249435	41.320551
3512.799826	792740.545499	41.325556
3512.463042	792546.885309	41.330560
3512.693503	792329.297789	41.335565
3512.529128	792129.996817	41.340570
3511.991661	791924.511666	41.345575
3512.441121	791732.075398	41.350580
3511.956615	791527.847519	41.355584
3512.153885	791326.646289	41.360589
3511.798221	791131.279749	41.365594
3511.808745	790939.189081	41.370599
3511.879966	790746.739216	41.375604
3511.195413	790560.698984	41.380608
3511.289716	790375.655909	41.385613
3510.953033	790189.352060	41.390618
3510.701364	790011.482651	41.395623
3511.244673	789825.171743	41.400628
3510.728403	789660.607229	41.405632
3510.915067	789487.862381	41.410637
3510.755236	789310.697571	41.415642
3510.799630	789124.991181	41.420647
3510.893765	788949.004371	41.425652
3510.490368	788769.900036	41.430656
3510.528151	788591.603353	41.435661
3510.297357	788415.361940	41.440666
3510.114483	788261.377492	41.445671
3510.345303	788087.903192	41.450676
3509.735269	787929.803298	41.455680
3509.861211	787764.302586	41.460685
3509.879530	787603.437172	41.465690
3509.675140	787443.588119	41.470695
3509.880208	787275.555638	41.475700
3509.702496	787123.856612	41.480704
3509.673280	786948.627461	41.485709
3509.254554	786806.450889	41.490714
3509.184447	786664.164896	41.495719
3509.721986	786500.927321	41.500724
3509.237892	786354.130410	41.505728
3509.371056	786197.246595	41.510733
3509.183608	786061.606383	41.515738
3508.833956	785899.533908	41.520743
3509.110225	785743.255868	41.525748
3508.905386	785604.954340	41.530752
3508.840090	785449.513005	41.535757
3508.892521	785309.983127	41.540762
3508.791398	785181.443091	41.545767
3508.918123	785013.124558	41.550772
3508.690749	784884.845917	41.555776
3508.643400	784728.943387	41.560781
3508.603818	784596.152952	41.565786
3508.347321	784469.298041	41.570791
3508.453362	784324.821666	41.575796
3508.381864	784195.078637	41.580800
3508.278062	784047.778404	41.585805
3507.920917	783920.536889	41.590810
3507.773563	783777.616132	41.595815
3507.452481	783645.936712	41.600820
3507.327441	783536.358914	41.605824
3507.665297	783405.747169	41.610829
3507.630606	783286.410541	41.615834
3507.206543	783167.332851	41.620839
3507.356139	783050.421676	41.625844
3507.300995	782932.410826	41.630848
3507.224286	782813.171682	41.635853
3507.295328	782698.579992	41.640858
3507.128665	782578.072649	41.645863
3507.414704	782456.209550	41.650868
3507.214178	782353.760093	41.655872
3507.039310	782235.905182	41.660877
3507.216778	782124.681703	41.665882
3506.815652	782011.928147	41.670887
3507.188638	781894.912278	41.675892
3506.994836	781778.037081	41.680896
3506.779848	781662.295189	41.685901
3506.555460	781554.278222	41.690906
3506.605546	781445.033488	41.695911
3506.421948	781330.954130	41.700916
3506.406146	781238.742658	41.705920
3506.308484	781128.434923	41.710925
3506.300707	781018.848837	41.715930
3506.360926	780926.522452	41.720935
3506.166705	780830.496832	41.725940
3506.066395	780734.306838	41.730944
3505.738863	780632.296828	41.735949
3505.828678	780535.876039	41.740954
3505.513037	780443.556205	41.745959
3505.633512	780355.444925	41.750964
3505.792875	780270.672721	41.755968
3505.527282	780179.128702	41.760973
3505.336486	780088.998448	41.765978
3505.565191	780006.081912	41.770983
3505.591192	779912.468654	41.775988
3505.160354	779851.264950	41.780992
3505.598538	779750.199186	41.785997
3505.323489	779667.115672	41.791002
3505.340228	779573.844106	41.796007
3505.369339	779493.120218	41.801012
3504.935409	779404.005900	41.806016
3504.918313	779326.142520	41.811021
3504.869767	779251.925831	41.816026
3504.562633	779180.950366	41.821031
3504.764982	779103.737558	41.826036
3504.735459	779036.554262	41.831040
3504.817066	778957.784682	41.836045
3504.608562	778897.422332	41.841050
3504.525721	778825.618885	41.846055
3505.006158	778751.802203	41.851060
3504.429721	778672.596463	41.856064
3504.569754	778594.945505	41.861069
3504.702385	778534.376280	41.866074
3504.498132	778466.921157	41.871079
3504.909198	778381.839360	41.876084
3504.513072	778314.660566	41.881088
3504.646211	778244.194175	41.886093
3504.755105	778177.866261	41.891098
3504.497812	778106.675204	41.896103
3505.274615	778033.983933	41.901108
3504.748826	777961.161892	41.906112
3504.503598	777884.403734	41.911117
3504.552533	777814.390135	41.916122
3504.317391	777748.754988	41.921127
3504.544094	777674.083046	41.926132
3504.300623	777616.177421	41.931136
3504.220528	777546.084040	41.936141
3504.212352	777480.458327	41.941146
3504.442208	777413.069653	41.946151
3504.663989	777340.315210	41.951156
3504.095221	777292.848918	41.956160
3504.412957	777219.437425	41.961165
3504.453380	777148.631096	41.966170
3504.115102	777083.450072	41.971175
3504.169152	777015.791283	41.976180
3503.917435	776953.105871	41.981184
3503.873993	776895.604713	41.986189
3503.873020	776836.668230	41.991194
3503.809986	776779.514047	41.996199
3504.142310	776725.396283	42.001204
3503.943670	776663.782882	42.006208
3504.052468	776603.792439	42.011213
3503.823877	776539.967186	42.016218
3503.720892	776480.109092	42.021223
3503.903751	776419.711025	42.026228
3503.840802	776377.424139	42.031232
3503.779976	776301.603787	42.036237
3503.684420	776259.173867	42.041242
3503.546928	776210.201510	42.046247
3503.785549	776153.977584	42.051252
3503.895282	776097.134309	42.056256
3503.766480	776044.121556	42.061261
3503.777539	775987.490654	42.066266
3503.557547	775930.848129	42.071271
3503.677727	775880.993994	42.076276
3503.449655	775829.424103	42.081280
3503.454777	775777.224506	42.086285
3503.825671	775716.494209	42.091290
3503.215791	775663.853415	42.096295
3503.643348	775605.279646	42.101300
3503.956692	775559.380388	42.106304
3503.613244	775511.816170	42.111309
3503.822483	775459.038982	42.116314
3503.731780	775405.670613	42.121319
3503.796955	775340.062883	42.126324
3503.389959	775292.950938	42.131328
3503.228300	775236.588927	42.136333
3503.424194	775201.098076	42.141338
3503.288947	775147.094938	42.146343
3503.392896	775101.621299	42.151348
3503.253366	775054.759260	42.156352
3502.921408	774998.915966	42.161357
3503.349419	774944.867813	42.166362
3503.200339	774902.044859	42.171367
3503.044807	774842.920809	42.176372
3503.127273	774811.091298	42.181376
3502.912525	774761.826492	42.186381
3503.162304	774731.397358	42.191386
3503.103605	774699.295108	42.196391
3503.189515	774653.772419	42.201396
3502.991304	774615.634809	42.206400
3503.222732	774569.004081	42.211405
3503.120651	774527.008491	42.216410
3502.983670	774474.330515	42.221415
3503.261390	774416.560008	42.226420
3503.118108	774387.770307	42.231424
3503.106258	774331.622945	42.236429
3502.788813	774294.537642	42.241434
3502.609833	774264.423473	42.246439
3503.119701	774219.665591	42.251444
3502.863686	774182.077055	42.256448
3502.664455	774137.336963	42.261453
3502.924349	774093.210552	42.266458
3502.791238	774063.679072	42.271463
3502.755994	774020.487443	42.276468
3502.801195	774000.137212	42.281472
3502.553034	773960.428233	42.286477
3502.951022	773913.076327	42.291482
3502.413659	773875.089253	42.296487
3502.975438	773840.664487	42.301492
3502.625717	773804.567174	42.306496
3502.414031	773757.511722	42.311501
3502.852315	773726.357779	42.316506
3502.523530	773694.394148	42.321511
3502.742208	773655.345500	42.326516
3502.379065	773627.524950	42.331520
3502.258541	773591.635132	42.336525
3502.463531	773562.242986	42.341530
3502.630693	773533.448065	42.346535
3502.623404	773487.342407	42.351540
3502.491370	773468.891767	42.356544
3502.764787	773431.655529	42.361549
3502.489654	773401.849229	42.366554
3502.302692	773365.575172	42.371559
3502.237966	773332.827570	42.376564
3502.341016	773303.057097	42.381568
3502.625988	773274.389544	42.386573
3502.529465	773234.405367	42.391578
3502.351034	773218.129239	42.396583
3502.577455	773173.214655	42.401588
3502.316277	773151.927315	42.406592
3502.272602	773113.362370	42.411597
3502.533924	773083.367893	42.416602
3502.238341	773062.381535	42.421607
3502.431431	773020.377996	42.426612
3502.532051	772999.178408	42.431616
3502.469280	772960.862126	42.436621
3502.483666	772930.809179	42.441626
3502.096417	772896.487074	42.446631
3502.369876	772868.312477	42.451636
3502.672055	772832.152282	42.456640
3502.160951	772800.017744	42.461645
3502.069085	772771.558104	42.466650
3502.471128	772737.942746	42.471655
3502.536917	772703.348061	42.476660
3502.372766	772679.777191	42.481664
3502.394279	772637.947535	42.486669
3502.559701	772615.701602	42.491674
3502.510696	772586.840067	42.496679
3502.386141	772546.955314	42.501684
3502.116586	772521.085803	42.506688
3502.013455	772493.070339	42.511693
3502.387021	772476.849449	42.516698
3502.076406	772452.562984	42.521703
3502.277040	772421.294889	42.526708
3502.023658	772401.235764	42.531712
3502.328128	772378.227211	42.536717
3502.343311	772344.033316	42.541722
3502.034442	772306.345381	42.546727
3502.376357	772283.970845	42.551732
3502.215670	772264.930701	42.556736
3502.404685	772220.952580	42.561741
3502.368869	772194.600011	42.566746
3502.078598	772170.457070	42.571751
3502.134701	772132.609595	42.576756
3502.202885	772122.744617	42.581760
3501.952325	772089.283077	42.586765
3502.066479	772066.157097	42.591770
3502.024412	772048.624198	42.596775
3502.049781	772014.969064	42.601780
3502.165651	771980.116399	42.606784
3502.133019	771971.105409	42.611789
3502.164678	771936.069328	42.616794
3501.890124	771909.952149	42.621799
3502.063739	771882.135135	42.626804
3501.766336	771853.804356	42.631808
3501.932193	771839.045130	42.636813
3501.961208	771809.970628	42.641818
3502.245257	771785.633288	42.646823
3502.105614	771764.371194	42.651828
3501.933896	771757.156613	42.656832
3501.803192	771736.040779	42.661837
3502.165848	771709.620847	42.666842
3501.801344	771690.711338	42.671847
3502.236125	771661.273786	42.676852
3501.902869	771632.504618	42.681856
3502.029736	771608.044769	42.686861
3502.164983	771564.367238	42.691866
3501.869738	771564.711493	42.696871
3501.950436	771530.995772	42.701876
3501.938295	771516.363769	42.706880
3501.675411	771484.626069	42.711885
3502.127892	771462.920665	42.716890
3501.736632	771448.695887	42.721895
3501.601106	771419.893322	42.726900
3502.022967	771409.377857	42.731904
3501.765102	771393.504975	42.736909
3501.686695	771367.797033	42.741914
3501.606229	771351.402103	42.746919
3501.616089	771330.163410	42.751924
3501.881874	771322.087955	42.756928
3501.349866	771283.495352	42.761933
3501.820869	771279.032344	42.766938
3501.384846	771265.159505	42.771943
3501.798493	771238.729498	42.776948
3501.989579	771230.074952	42.781952
3501.786978	771205.766595	42.786957
3502.018000	771185.821478	42.791962
3501.690008	771165.377087	42.796967
3501.910418	771142.279996	42.801972
3501.570930	771112.524326	42.806977
3501.795665	771095.585804	42.811981
3501.799241	771087.454734	42.816986
3501.519135	771078.877625	42.821991
3501.820772	771052.662509	42.826996
3501.662050	771024.453536	42.832001
3501.594169	771012.786280	42.837005
3501.859774	770997.811847	42.842010
3501.851045	770984.853622	42.847015
3501.973217	770963.595379	42.852020
3501.577761	770949.863095	42.857025
3501.645480	770934.181980	42.862029
3502.052759	770907.948952	42.867034
3501.724339	770889.130002	42.872039
3501.418789	770872.820364	42.877044
3501.973373	770848.632498	42.882049
3501.360908	770833.506704	42.887053
3501.441970	770819.449300	42.892058
3501.343320	770797.684903	42.897063
3501.756407	770775.688317	42.902068
3501.529337	770781.934692	42.907073
3501.646173	770750.180574	42.912077
3501.943896	770736.087324	42.917082
3501.395393	770726.075677	42.922087
3501.644785	770694.595155	42.927092
3501.353660	770684.787448	42.932097
3501.146399	770665.258075	42.937101
3501.644365	770636.890181	42.942106
3501.546492	770633.506067	42.947111
3501.627520	770640.687383	42.952116
3501.571001	770609.848233	42.957121
3501.445866	770604.743839	42.962125
3501.570757	770579.689580	42.967130
3501.549283	770558.010325	42.972135
3501.830647	770551.754797	42.977140
3501.801297	770526.035855	42.982145
3501.711762	770503.825580	42.987149
3501.668381	770491.217157	42.992154
3501.524615	770483.701050	42.997159
3501.475139	770457.837347	43.002164
3501.281189	770462.797259	43.007169
3501.612630	770433.470425	43.012173
3502.027261	770414.675714	43.017178
3501.260797	770393.956454	43.022183
3501.396692	770371.462250	43.027188
3501.321671	770363.441893	43.032193
3501.781473	770350.848910	43.037197
3501.766090	770324.831287	43.042202
3501.622969	770321.553045	43.047207
3502.086684	770295.209999	43.052212
3502.002842	770278.714691	43.057217
3501.861628	770272.873502	43.062221
3501.884088	770253.403766	43.067226
3501.717370	770234.704360	43.072231
3502.058566	770205.917116	43.077236
3501.936964	770195.785148	43.082241
3501.716436	770166.696025	43.087245
3502.162294	770150.458153	43.092250
3501.644904	770121.664161	43.097255
3501.850824	770109.112589	43.102260
3501.828726	770083.489484	43.107265
3502.059577	770065.759093	43.112269
3502.195769	770031.731726	43.117274
3501.474858	770018.593427	43.122279
3501.523782	769993.254008	43.127284
3501.730278	769973.309679	43.132289
3501.625328	769963.371782	43.137293
3501.696448	769935.367224	43.142298
3501.514815	769927.856789	43.147303
3501.756638	769914.362593	43.152308
3501.910935	769892.997429	43.157313
3501.535832	769875.809948	43.162317
3501.567945	769843.671642	43.167322
3501.519780	769826.578046	43.172327
3501.706067	769818.021218	43.177332
3501.668515	769799.841564	43.182337
3501.617977	769792.210831	43.187341
3501.852798	769759.989490	43.192346
3501.348242	769745.977232	43.197351
3501.577477	769728.739150	43.202356
3501.319552	769723.064605	43.207361
3501.343074	769702.311850	43.212365
3501.424624	769695.989950	43.217370
3501.333991	769694.674176	43.222375
3501.417785	769666.370808	43.227380
3501.391674	769647.153910	43.232385
3501.473637	769637.924068	43.237389
3501.605298	769627.059613	43.242394
3501.461007	769606.974942	43.247399
3501.600940	769594.334802	43.252404
3501.366355	769583.284183	43.257409
3501.259990	769562.453861	43.262413
3501.002837	769538.986881	43.267418
3501.200229	769550.437956	43.272423
3501.527640	769538.949700	43.277428
3501.611874	769531.493643	43.282433
3500.917786	769520.420046	43.287437
3501.277391	769517.847215	43.292442
3500.735767	769524.146453	43.297447
3501.039511	769522.765688	43.302452
3501.043020	769488.659120	43.307457
3501.440001	769475.089286	43.312461
3501.432795	769463.409599	43.317466
3501.253881	769469.057702	43.322471
3500.877076	769454.777419	43.327476
3501.046207	769435.379955	43.332481
3501.156182	769428.363133	43.337485
3501.444117	769422.253438	43.342490
3501.302089	769436.224930	43.347495
3501.124575	769421.172456	43.352500
3501.073988	769396.340261	43.357505
3501.235057	769388.181389	43.362509
3501.313366	769382.204764	43.367514
3501.054559	769388.950400	43.372519
3501.045474	769380.770260	43.377524
3501.317881	769357.116904	43.382529
3501.753636	769343.146147	43.387533
3501.717379	769332.456783	43.392538
3501.350014	769323.103414	43.397543
3501.169596	769305.931831	43.402548
3501.225795	769294.340009	43.407553
3501.029645	769292.203657	43.412557
3501.564449	769283.638097	43.417562
3501.460579	769260.982880	43.422567
3501.501804	769255.455852	43.427572
3501.551947	769248.152990	43.432577
3501.703868	769210.176250	43.437581
3501.644447	769200.032681	43.442586
3501.312989	769191.363264	43.447591
3501.430365	769165.960463	43.452596
3501.438409	769159.206620	43.457601
3501.149703	769166.598130	43.462605
3501.637292	769143.845133	43.467610
3501.291862	769120.489949	43.472615
3501.470421	769110.602790	43.477620
3501.626500	769110.330626	43.482625
3501.253728	769078.206417	43.487629
3501.396159	769066.994350	43.492634
3501.448723	769071.668133	43.497639
3501.561667	769042.223945	43.502644
3501.706217	769035.299637	43.507649
3501.244782	769033.206906	43.512653
3501.525091	768994.320713	43.517658
3501.328521	768990.212762	43.522663
3501.201405	768975.397532	43.527668
3501.585046	768970.306787	43.532673
3501.180060	768953.417828	43.537677
3501.527793	768931.673016	43.542682
3501.514910	768935.766187	43.547687
3501.466991	768911.129093	43.552692
3501.574704	768894.500580	43.557697
3501.166187	768894.370698	43.562701
3501.514513	768872.379165	43.567706
3501.427099	768854.451865	43.572711
3501.364898	768841.350839	43.577716
3501.705789	768852.138578	43.582721
3501.424321	768835.524748	43.587725
3501.401089	768823.353791	43.592730
3501.091076	768820.003791	43.597735
3501.495301	768801.650349	43.602740
3501.171858	768768.777316	43.607745
3501.360525	768769.978502	43.612749
3501.397026	768756.614615	43.617754
3501.195378	768752.704533	43.622759
3501.015315	768737.601803	43.627764
3501.084078	768730.443241	43.632769
3501.111824	768722.847806	43.637773
3501.180298	768713.520458	43.642778
3501.044316	768729.414640	43.647783
3501.337224	768702.404027	43.652788
3501.554254	768694.530928	43.657793
3501.176710	768687.889463	43.662797
3501.426140	768672.321524	43.667802
3501.138596	768655.461834	43.672807
3501.523064	768640.315212	43.677812
3501.421113	768639.198281	43.682817
3501.051577	768627.922009	43.687821
3501.371967	768601.645884	43.692826
3500.922024	768601.374941	43.697831
3501.100905	768593.606604	43.702836
3501.139728	768590.741253	43.707841
3501.220739	768586.538064	43.712845
3501.388405	768571.969228	43.717850
3501.110258	768556.192195	43.722855
3501.454236	768544.699683	43.727860
3501.369207	768545.650234	43.732865
3501.109222	768533.320631	43.737869
3501.707108	768500.886167	43.742874
3501.349256	768495.375018	43.747879
3501.622083	768493.900576	43.752884
3501.930716	768465.555612	43.757889
3501.687239	768458.201755	43.762893
3501.149829	768434.974626	43.767898
3501.310867	768428.490679	43.772903
3501.509185	768415.395286	43.777908
3501.577790	768401.631128	43.782913
3501.549628	768388.129351	43.787917
3501.658518	768368.739036	43.792922
3501.372576	768360.209030	43.797927
3501.014430	768327.438352	43.802932
3501.323970	768320.535500	43.807937
3501.389004	768318.700900	43.812941
3501.361429	768310.177572	43.817946
3501.125362	768295.181758	43.822951
3501.202120	768283.732862	43.827956
3501.548795	768280.865979	43.832961
3500.935789	768278.305053	43.837965
3501.380738	768250.725527	43.842970
3501.333245	768247.282729	43.847975
3501.046100	768240.576677	43.852980
3501.264736	768235.808382	43.857985
3501.058108	768237.814185	43.862989
3501.330253	768217.164224	43.867994
3500.865104	768199.839810	43.872999
3501.239874	768187.651552	43.878004
3501.269487	768187.005830	43.883009
3501.189944	768190.075199	43.888013
3501.030091	768161.954135	43.893018
3501.342882	768168.705306	43.898023
3500.879647	768159.563438	43.903028
3501.041115	768147.213069	43.908033
3501.187144	768155.322688	43.913037
3501.317391	768139.428207	43.918042
3500.863409	768120.179257	43.923047
3501.222669	768109.324399	43.928052
3501.433693	768105.986840	43.933057
3501.153039	768108.349938	43.938061
3501.068372	768090.173871	43.943066
3500.914669	768068.706326	43.948071
3500.645704	768064.116829	43.953076
3500.784549	768073.657294	43.958081
3500.619767	768066.043608	43.963085
3500.858722	768063.736637	43.968090
3500.799542	768073.112538	43.973095
3501.147509	768061.766516	43.978100
3501.424200	768063.889937	43.983105
3501.033098	768058.236051	43.988109
3501.128245	768038.157002	43.993114
3501.085209	768027.959842	43.998119
3500.978179	768031.280282	44.003124
3501.104231	768023.372168	44.008129
3501.128969	768035.001905	44.013133
3501.140088	768024.894411	44.018138
3500.759611	768006.076721	44.023143
3501.118136	767985.904853	44.028148
3501.393488	767975.063622	44.033153
3501.112425	767983.588851	44.038157
3501.138512	767978.507036	44.043162
3500.996753	767978.382486	44.048167
3501.345280	767965.212266	44.053172
3501.325893	767950.475845	44.058177
3501.007099	767963.690466	44.063181
3501.350246	767938.788559	44.068186
3500.987360	767931.453849	44.073191
3501.371278	767908.664875	44.078196
3501.365147	767889.489449	44.083201
3501.145350	767897.758200	44.088205
3501.322428	767903.151659	44.093210
3501.128326	767878.683123	44.098215
3501.080494	767870.211926	44.103220
3501.360851	767852.763905	44.108225
3500.949556	767867.275655	44.113229
3501.166250	767851.760698	44.118234
3501.185284	767842.046030	44.123239
3501.351180	767802.778100	44.128244
3501.284696	767811.810450	44.133249
3501.184739	767808.326794	44.138253
3501.357323	767801.298132	44.143258
3501.403270	767774.275547	44.148263
3500.909352	767757.842197	44.153268
3501.381549	767764.271694	44.158273
3500.986766	767765.174769	44.163277
3501.225182	767759.121176	44.168282
3501.013471	767736.232597	44.173287
3501.549815	767729.242546	44.178292
3501.586276	767719.524848	44.183297
3501.132549	767710.972435	44.188301
3501.325326	767688.017082	44.193306
3501.156182	767675.276709	44.198311
3501.355417	767671.546514	44.203316
3501.556281	767666.977979	44.208321
3501.275997	767656.720793	44.213325
3501.545509	767635.823170	44.218330
3501.302603	767642.271966	44.223335
3501.343412	767620.426003	44.228340
3501.161662	767593.538867	44.233345
3500.915816	767588.797371	44.238349
3501.555053	767580.409869	44.243354
3501.501605	767580.122868	44.248359
3501.572161	767567.638622	44.253364
3501.438286	767551.983593	44.258369
3501.321542	767549.488561	44.263373
3501.512341	767524.314575	44.268378
3501.149599	767506.330787	44.273383
3501.125237	767512.497200	44.278388
3501.412917	767501.554655	44.283393
3501.165431	767482.023544	44.288397
3501.531189	767457.412109	44.293402
3500.881115	767456.582482	44.298407
3501.399039	767459.898834	44.303412
3501.394790	767438.848556	44.308417
3501.073687	767439.591632	44.313421
3501.671418	767419.773237	44.318426
3501.218368	767421.277547	44.323431
3501.002021	767402.480596	44.328436
3501.297230	767384.043037	44.333441
3501.062063	767383.983162	44.338445
3501.031010	767378.121548	44.343450
3500.913410	767374.640596	44.348455
3500.783854	767377.866435	44.353460
3501.102244	767379.391584	44.358465
3500.772376	767355.929699	44.363469
3500.795912	767331.571421	44.368474
3501.205549	767336.631182	44.373479
3500.993270	767327.644152	44.378484
3501.187597	767326.133116	44.383489
3501.378514	767328.813184	44.388493
3501.375487	767314.713720	44.393498
3501.200842	767302.811727	44.398503
3501.124656	767293.950142	44.403508
3501.505890	767278.160390	44.408513
3501.321365	767280.902318	44.413517
3501.155613	767257.807498	44.418522
3500.817119	767250.024387	44.423527
3501.166828	767233.105811	44.428532
3501.322944	767249.398735	44.433537
3501.076676	767245.298002	44.438541
3501.098382	767217.192773	44.443546
3501.387181	767204.228261	44.448551
3501.052604	767201.916897	44.453556
3501.523633	767195.775234	44.458561
3501.316987	767193.245590	44.463565
3501.136855	767159.996746	44.468570
3501.127127	767153.441222	44.473575
3501.350729	767157.447112	44.478580
3501.059584	767146.697997	44.483585
3500.903528	767146.723690	44.488589
3501.327179	767119.143506	44.493594
3501.273745	767114.271410	44.498599
3501.003382	767117.668460	44.503604
3501.188083	767107.925549	44.508609
3500.950180	767114.620483	44.513613
3501.366176	767103.853431	44.518618
3501.351265	767085.269012	44.523623
3501.187371	767084.457861	44.528628
3501.212352	767069.317976	44.533633
3501.103118	767072.392693	44.538637
3501.108135	767045.127704	44.543642
3500.929017	767026.964606	44.548647
3500.945841	767033.962771	44.553652
3501.270012	767016.949309	44.558657
3500.993914	767028.383653	44.563661
3501.251959	767026.812760	44.568666
3501.098266	767000.116076	44.573671
3501.224268	766993.587358	44.578676
3501.241769	766988.802101	44.583681
3500.976468	766994.959324	44.588685
3501.032714	766993.076546	44.593690
3500.936904	766984.612247	44.598695
3500.950845	766950.344448	44.603700
3501.123824	766940.110221	44.608705
3501.068099	766939.034721	44.613709
3501.151501	766938.380032	44.618714
3501.241189	766944.823945	44.623719
3501.068714	766943.323949	44.628724
3500.965765	766910.800829	44.633729
3501.028911	766911.825784	44.638733
3501.111067	766899.042693	44.643738
3501.254181	766902.766159	44.648743
3500.901914	766903.465114	44.653748
3501.057134	766906.447035	44.658753
3500.972457	766882.746063	44.663757
3501.284273	766854.788900	44.668762
3501.037814	766854.237842	44.673767
3501.145945	766853.924197	44.678772
3501.622271	766850.838205	44.683777
3501.198153	766843.709720	44.688781
3501.212498	766826.105911	44.693786
3501.196098	766816.297139	44.698791
3500.988866	766814.654931	44.703796
3501.379726	766801.229177	44.708801
3501.010348	766793.302763	44.713805
3501.122373	766771.442590	44.718810
3500.905590	766775.471922	44.723815
3501.604441	766777.476874	44.728820
3501.488939	766760.387341	44.733825
3501.170774	766747.226192	44.738829
3500.991883	766732.957381	44.743834
3501.279867	766731.332193	44.748839
3501.000553	766734.928106	44.753844
3501.582254	766728.965053	44.758849
3501.277946	766705.891351	44.763853
3501.333871	766697.648257	44.768858
3501.492605	766687.810469	44.773863
3501.359149	766678.365930	44.778868
3501.449190	766650.050097	44.783873
3501.170452	766644.623147	44.788877
3501.140986	766639.944013	44.793882
3501.125410	766621.062720	44.798887
3501.191252	766601.379085	44.803892
3501.278959	766596.483402	44.808897
3501.137671	766596.950411	44.813901
3500.996499	766595.938242	44.818906
3501.211022	766591.859858	44.823911
3501.061087	766572.507520	44.828916
3501.321887	766562.849978	44.833921
3501.298031	766566.946254	44.838925
3501.084345	766559.437695	44.843930
3500.705033	766564.282799	44.848935
3500.955155	766555.810340	44.853940
3501.368982	766522.904579	44.858945
3501.127520	766513.477622	44.863949
3501.393916	766511.313578	44.868954
3501.234910	766513.854357	44.873959
3500.920606	766501.037278	44.878964
3501.041927	766477.153172	44.883969
3500.742657	766475.131599	44.888973
3500.783136	766472.363778	44.893978
3501.302874	766468.037828	44.898983
3500.914823	766477.321980	44.903988
3501.346126	766464.875086	44.908993
3500.968494	766457.393429	44.913997
3500.820281	766443.907913	44.919002
3501.137533	766431.183912	44.924007
3501.132767	766436.016711	44.929012
3501.183657	766420.082344	44.934017
3500.853858	766421.615850	44.939021
3501.278964	766418.883267	44.944026
3501.175307	766405.686182	44.949031
3500.888374	766405.832047	44.954036
3501.306492	766386.632193	44.959041
3501.163980	766400.362903	44.964045
3501.110494	766389.376322	44.969050
3500.870591	766386.062972	44.974055
3501.008189	766352.511670	44.979060
3501.063807	766337.562487	44.984065
3500.458597	766346.340193	44.989069
3500.923166	766344.439302	44.994074
3501.076720	766337.560326	44.999079
3500.760205	766341.458395	45.004084
3501.055096	766343.382089	45.009089
3500.819523	766358.607413	45.014093
3500.974002	766351.629684	45.019098
3501.274331	766346.945351	45.024103
3500.954045	766324.612707	45.029108
3501.167910	766303.276773	45.034113
3500.967671	766309.621068	45.039117
3500.914899	766301.789900	45.044122
3500.987006	766304.884367	45.049127
3501.036444	766308.426332	45.054132
3501.067326	766305.857258	45.059137
3500.965780	766278.705646	45.064141
3500.953634	766266.035623	45.069146
3501.226383	766266.631682	45.074151
3501.174011	766260.476859	45.079156
3501.316309	766250.443976	45.084161
3501.175070	766242.035627	45.089165
3501.191391	766217.526991	45.094170
3501.238181	766201.937991	45.099175
3501.077152	766221.884870	45.104180
3501.395612	766216.457853	45.109185
3500.962487	766204.399454	45.114189
3501.151006	766179.418558	45.119194
3501.180481	766170.834085	45.124199
3500.750709	766178.794158	45.129204
3501.171979	766175.026650	45.134209
3501.005996	766176.730454	45.139213
3501.066935	766174.255001	45.144218
3501.457931	766147.909329	45.149223
3500.943258	766136.850419	45.154228
3501.199571	766131.384270	45.159233
3500.887518	766125.913119	45.164237
3501.385851	766126.965117	45.169242
3500.999203	766106.417855	45.174247
3501.184905	766098.744429	45.179252
3501.430549	766090.863887	45.184257
3501.259876	766090.546827	45.189261
3501.440530	766081.394956	45.194266
3501.416257	766061.675438	45.199271
3501.181432	766050.668921	45.204276
3501.527519	766042.821093	45.209281
3501.292084	766040.887504	45.214285
3501.267189	766024.718236	45.219290
3501.393704	766022.626404	45.224295
3501.095186	766010.989301	45.229300
3501.296068	765999.220612	45.234305
3501.116485	765982.090547	45.239309
3501.104918	765967.891335	45.244314
3501.254397	765966.535346	45.249319
3500.923356	765970.929093	45.254324
3501.400513	765972.773553	45.259329
3501.079325	765946.593795	45.264333
3501.192912	765926.604666	45.269338
3501.190509	765928.182961	45.274343
3501.032555	765933.041316	45.279348
3500.990095	765928.166640	45.284353
3500.933252	765917.377158	45.289357
3501.148785	765894.166014	45.294362
3501.227812	765881.233774	45.299367
3501.058094	765883.382048	45.304372
3501.186467	765881.733661	45.309377
3501.156252	765878.188305	45.314381
3501.093311	765857.734970	45.319386
3501.428062	765845.549508	45.324391
3501.111879	765836.232624	45.329396
3501.203774	765834.442305	45.334401
3500.784659	765839.294428	45.339405
3501.114559	765826.961804	45.344410
3501.126524	765800.578729	45.349415
3501.169913	765793.076364	45.354420
3500.809490	765799.940579	45.359425
3501.154817	765801.067139	45.364429
3501.288843	765792.810186	45.369434
3501.046490	765777.563795	45.374439
3501.046924	765760.502193	45.379444
3501.209812	765752.191131	45.384449
3501.278947	765744.142057	45.389453
3501.346463	765746.695091	45.394458
3501.206416	765748.542651	45.399463
3500.933532	765721.861041	45.404468
3501.219378	765702.286741	45.409473
3500.789117	765709.359786	45.414477
3500.901075	765709.439955	45.419482
3501.400142	765715.570940	45.424487
3500.965663	765703.610576	45.429492
3501.556903	765661.352000	45.434497
3501.149417	765658.361798	45.439501
3501.201192	765671.075608	45.444506
3501.503373	765667.820581	45.449511
3500.977645	765644.829389	45.454516
3501.260116	765626.784106	45.459521
3500.656604	765626.143828	45.464525
3500.913034	765620.825226	45.469530
3501.235618	765620.229650	45.474535
3501.306078	765632.989759	45.479540
3501.449437	765602.442164	45.484545
3501.146146	765588.586157	45.489549
3501.280996	765582.991683	45.494554
3501.416634	765576.854642	45.499559
3501.003826	765564.002869	45.504564
3501.009269	765549.454878	45.509569
3501.161118	765545.484878	45.514573
3501.161043	765540.602968	45.519578
3501.231985	765534.377925	45.524583
3501.111039	765527.494111	45.529588
3501.290339	765500.835857	45.534593
3501.021919	765497.378870	45.539597
3501.254735	765492.310629	45.544602
3501.461017	765488.331633	45.549607
3501.134514	765485.525271	45.554612
3501.178759	765453.908521	45.559617
3500.872975	765443.504552	45.564621
3500.933125	765441.571430	45.569626
3501.347548	765442.637352	45.574631
3501.252692	765440.877701	45.579636
3501.053255	765415.366412	45.584641
3500.928640	765410.455617	45.589645
3500.749514	765398.502017	45.594650
3500.622306	765395.564167	45.599655
3500.864097	765408.838881	45.604660
3501.033773	765400.674253	45.609665
3500.859493	765404.845253	45.614669
3500.825203	765400.955150	45.619674
3501.213791	765404.984123	45.624679
3500.936672	765399.062866	45.629684
3500.909927	765377.221489	45.634689
3500.955990	765376.424877	45.639693
3500.840941	765367.123591	45.644698
3500.776391	765367.035585	45.649703
3501.193618	765362.873837	45.654708
3501.138406	765358.740591	45.659713
3500.984708	765362.365777	45.664717
3500.694799	765364.090175	45.669722
3501.191015	765356.611412	45.674727
3500.674957	765332.335517	45.679732
3501.028198	765320.491356	45.684737
3500.789189	765322.996398	45.689741
3500.880307	765327.271666	45.694746
3501.300354	765319.164336	45.699751
3501.037003	765319.109076	45.704756
3501.025372	765324.239604	45.709761
3500.863369	765322.195102	45.714765
3501.095090	765297.598667	45.719770
3501.211775	765277.804557	45.724775
3501.283670	765278.285843	45.729780
3501.429091	765275.253725	45.734785
3501.726364	765265.095372	45.739789
3501.250612	765244.609735	45.744794
3501.204331	765238.354441	45.749799
3501.076769	765233.345388	45.754804
3500.921886	765218.231393	45.759809
3501.104245	765192.804402	45.764813
3501.124686	765172.483408	45.769818
3501.159753	765114.680608	45.774823
3501.009077	764991.170210	45.779828
3500.779430	764818.797813	45.784833
3500.807631	764593.756376	45.789837
3500.511495	764303.412431	45.794842
3500.334862	763968.252850	45.799847
3500.163235	763571.076062	45.804852
3499.762719	763107.076651	45.809857
3499.241429	762599.213023	45.814861
3498.930330	762031.683935	45.819866
3498.727617	761414.015269	45.824871
3498.233216	760748.086448	45.829876
3497.954884	760006.412900	45.834881
3497.454332	759229.218570	45.839885
3496.815785	758386.024469	45.844890
3496.575916	757492.220999	45.849895
3495.817473	756534.759736	45.854900
3495.291169	755527.072160	45.859905
3494.189549	754465.123559	45.864909
3493.507581	753339.689297	45.869914
3493.114953	752159.161340	45.874919
3492.217583	750920.780202	45.879924
3491.336451	749628.484939	45.884929
3490.316436	748294.383658	45.889933
3489.656092	746889.554542	45.894938
3488.775505	745452.125867	45.899943
3487.441959	743951.113403	45.904948
3486.705865	742376.614527	45.909953
3485.673079	740769.992527	45.914957
3484.143713	739099.594313	45.919962
3483.709092	737376.700113	45.924967
3482.097362	735607.295246	45.929972
3481.008388	733773.592217	45.934977
3479.420565	731905.828838	45.939981
3478.367392	729980.332816	45.944986
3477.324611	727996.606783	45.949991
3475.752904	725961.043470	45.954996
3474.454450	723882.844202	45.960001
3473.319699	721743.055641	45.965005
3471.694516	719567.929479	45.970010
3470.511909	717316.654806	45.975015
3468.675248	715043.050103	45.980020
3467.220230	712708.062429	45.985025
3466.041723	710327.104647	45.990029
3464.163942	707902.289887	45.995034
3462.523418	705414.750606	46.000039
3460.667722	702900.939276	46.005044
3459.119845	700326.302193	46.010049
3457.566061	697708.892967	46.015053
3455.843737	695051.590614	46.020058
3454.387944	692345.337223	46.025063
3452.295064	689590.591517	46.030068
3450.815380	686774.762136	46.035073
3448.554752	683928.258279	46.040077
3446.983297	681036.169478	46.045082
3444.828549	678089.749450	46.050087
3442.683904	675116.422729	46.055092
3441.213036	672102.698192	46.060097
3439.049711	669036.898521	46.065101
3436.810302	665933.250527	46.070106
3434.994047	662776.220533	46.075111
3432.687624	659586.437155	46.080116
3430.436766	656344.857913	46.085121
3428.496416	653086.673375	46.090125
3425.825211	649778.262645	46.095130
3423.867250	646431.747355	46.100135
3421.276911	643041.370661	46.105140
3419.219590	639620.315768	46.110145
3416.937344	636152.323418	46.115149
3414.602390	632653.300151	46.120154
3412.575629	629107.092143	46.125159
3410.064537	625528.774110	46.130164
3407.824405	621911.487204	46.135169
3405.110866	618269.364720	46.140173
3402.670601	614582.815608	46.145178
3400.722140	610858.043959	46.150183
3397.642141	607084.856197	46.155188
3395.009343	603271.692825	46.160193
3392.474275	599441.383755	46.165197
3389.829686	595574.372213	46.170202
3387.700731	591682.292492	46.175207
3384.502597	587739.864044	46.180212
3382.199581	583772.171608	46.185217
3379.373574	579780.598203	46.190221
3376.699972	575754.964451	46.195226
3374.053022	571690.142610	46.200231
3370.838187	567601.364628	46.205236
3368.635129	563476.732849	46.210241
3365.657826	559320.204034	46.215245
3362.947320	555127.010294	46.220250
3360.164400	550912.919902	46.225255
3356.886099	546667.364194	46.230260
3353.879799	542396.462428	46.235265
3351.096696	538098.454547	46.240269
3347.855542	533780.514951	46.245274
3345.198200	529414.508249	46.250279
3342.033992	525040.082464	46.255284
3339.021010	520627.341933	46.260289
3336.118480	516200.788048	46.265293
3332.539905	511739.637682	46.270298
3329.947654	507257.412266	46.275303
3326.797487	502758.013261	46.280308
3323.703111	498230.170519	46.285313
3320.266613	493681.540033	46.290317
3317.605515	489101.975542	46.295322
3314.432794	484493.613331	46.300327
3310.867137	479880.842681	46.305332
3307.765993	475227.432635	46.310337
3304.640881	470556.306755	46.315341
3301.316621	465868.267091	46.320346
3298.154007	461156.172555	46.325351
3294.601498	456437.765887	46.330356
3291.173605	451688.645138	46.335361
3288.151200	446933.216802	46.340365
3285.005217	442150.335475	46.345370
3281.568182	437336.841918	46.350375
3277.724227	432510.932766	46.355380
3274.321071	427682.742776	46.360385
3271.033636	422835.648786	46.365389
3267.272425	417983.349399	46.370394
3264.140529	413090.846202	46.375399
3260.819161	408199.428890	46.380404
3257.208858	403282.621589	46.385409
3253.810824	398351.004279	46.390413
3250.044733	393422.560263	46.395418
3246.423288	388466.507389	46.400423
3242.947354	383513.215154	46.405428
3239.435603	378531.320163	46.410433
3235.691615	373555.607740	46.415437
3232.213642	368558.537353	46.420442
3228.427125	363560.090605	46.425447
3224.688979	358552.454980	46.430452
3221.420061	353525.285111	46.435457
3217.513919	348482.528059	46.440461
3213.895624	343442.328447	46.445466
3210.346418	338381.188740	46.450471
3206.445879	333327.556936	46.455476
3202.608600	328253.068457	46.460481
3198.752149	323177.160917	46.465485
3195.103839	318109.298940	46.470490
3191.563544	313028.121295	46.475495
3187.456719	307945.277012	46.480500
3183.873963	302849.440153	46.485505
3180.103454	297749.288652	46.490509
3176.211544	292659.332984	46.495514
3172.697202	287557.165442	46.500519
3168.208384	282452.386257	46.505524
3164.548722	277342.820435	46.510529
3160.819181	272237.842288	46.515533
3157.085811	267134.188323	46.520538
3153.140816	262013.435363	46.525543
3149.153829	256912.389608	46.530548
3145.213573	251796.992561	46.535553
3141.302517	246676.423049	46.540557
3137.092092	241583.595489	46.545562
3133.143027	236486.716799	46.550567
3129.172062	231391.290551	46.555572
3125.135429	226286.024376	46.560577
3121.194174	221191.245368	46.565581
3117.045793	216101.101615	46.570586
3113.150087	211011.704348	46.575591
3108.910419	205910.581779	46.580596
3104.960209	200800.070052	46.585601
3100.697833	195739.117669	46.590605
3096.406531	190680.406201	46.595610
3092.209817	185624.111963	46.600615
3088.131709	180590.799129	46.605620
3083.688106	175565.381027	46.610625
3079.598988	170558.886598	46.615629
3075.302703	165560.468425	46.620634
3070.976143	160565.533989	46.625639
3066.770316	155592.438742	46.630644
3062.371861	150626.697365	46.635649
3058.417069	145682.891373	46.640653
3053.773539	140759.830065	46.645658
3049.527862	135835.277812	46.650663
3045.036515	130951.765311	46.655668
3040.389877	126057.408768	46.660673
3036.024956	121191.438739	46.665677
3031.497382	116353.524125	46.670682
3027.190656	111533.481493	46.675687
3022.252016	106741.843934	46.680692
3017.433898	101965.036695	46.685697
3012.722731	97216.135710	46.690701
3007.652871	92487.881243	46.695706
3003.222406	87817.127547	46.700711
2997.996064	83171.539932	46.705716
2992.740629	78553.792528	46.710721
2986.824784	73989.034076	46.715725
2980.843494	69480.853260	46.720730
2972.739405	65078.520438	46.725735
2959.841051	60879.240132	46.730740
2946.954541	56809.150608	46.735745
2934.721562	52896.091740	46.740749
2922.025676	49153.106177	46.745754
2910.533152	45587.817498	46.750759
2899.593137	42220.462383	46.755764
2888.936587	39032.893621	46.760769
2878.995079	36024.312628	46.765773
2869.452182	33185.610414	46.770778
2860.638978	30506.048906	46.775783
2852.017507	28008.125007	46.780788
2843.524278	25650.086742	46.785793
2835.742899	23429.513930	46.790797
2827.986354	21355.707803	46.795802
2820.690670	19395.794961	46.800807
2813.547022	17567.585306	46.805812
2807.326627	15835.480834	46.810817
2800.806460	14217.708274	46.815821
2794.606099	12703.052071	46.820826
2789.251204	11263.328742	46.825831
2783.493809	9907.340302	46.830836
2778.183402	8626.627267	46.835841
2772.878824	7414.714520	46.840845
2767.733110	6276.643347	46.845850
2762.077567	5205.124795	46.850855
2755.188429	4235.732318	46.855860
2748.187782	3345.156306	46.860865
2741.354283	2552.252624	46.865869
2734.052178	1836.004445	46.870874
2726.936337	1201.170162	46.875879
2719.518571	667.034605	46.880884
2711.100531	256.719713	46.885889
2693.130444	224.722139	46.890893
2679.652223	226.857322	46.895898
2674.246390	221.332279	46.900903
2673.390502	228.930856	46.905908
2674.867958	231.141700	46.910913
2676.265719	208.773036	46.915917
2676.328638	223.316002	46.920922
2675.863554	221.457861	46.925927
2674.012027	215.336050	46.930932
2670.538279	210.549202	46.935937
2667.868895	214.028019	46.940941
2664.376728	223.402134	46.945946
2660.975889	209.408804	46.950951
2658.092644	210.528914	46.955956
2654.985190	212.293635	46.960961
2652.237668	208.266607	46.965965
2648.972578	216.384743	46.970970
2646.219530	215.441535	46.975975
2643.213905	217.765347	46.980980
2639.574291	214.650119	46.985985
2637.066532	208.068639	46.990989
2632.945630	218.791806	46.995994
2630.090007	213.505069	47.000999
2626.829971	205.083520	47.006004
2623.587114	213.398768	47.011009
2620.439522	206.701302	47.016013
2617.088388	214.682192	47.021018
2613.736654	200.688200	47.026023
2610.351490	202.728998	47.031028
2606.658527	205.938754	47.036033
2603.403928	204.825200	47.041037
2600.067184	204.165213	47.046042
2596.805485	210.788412	47.051047
2593.822657	201.249340	47.056052
2590.139088	205.320723	47.061057
2587.125177	194.627044	47.066061
2583.418080	196.002499	47.071066
2579.824084	193.885221	47.076071
2576.821770	197.660475	47.081076
2572.874320	203.059229	47.086081
2569.860843	195.164252	47.091085
2566.311541	194.148343	47.096090
2563.002485	194.762331	47.101095
2559.746541	204.967992	47.106100
2555.859924	206.693902	47.111105
2552.881866	195.169241	47.116109
2549.107884	193.214154	47.121114
2545.578476	190.111294	47.126119
2542.700167	186.974279	47.131124
2539.193512	186.942677	47.136129
2535.425839	184.381779	47.141133
2531.843072	195.076914	47.146138
2528.553591	199.949567	47.151143
2525.232824	195.063874	47.156148
2521.751146	201.027624	47.161153
2518.789544	191.311850	47.166157
2515.452606	189.844211	47.171162
2512.025580	190.942160	47.176167
2508.104805	195.720614	47.181172
2504.424916	191.201079	47.186177
2500.835926	187.000913	47.191181
2497.262255	196.561560	47.196186
2493.887210	193.104044	47.201191
2491.066891	191.843553	47.206196
2487.629282	196.480976	47.211201
2484.012580	191.142620	47.216205
2480.054445	186.361560	47.221210
2476.650608	183.750364	47.226215
2473.497733	188.498002	47.231220
2469.826732	184.646522	47.236225
2466.666693	194.764369	47.241229
2463.317907	191.689874	47.246234
2459.814935	181.876548	47.251239
2456.134617	172.141607	47.256244
2452.393963	173.750065	47.261249
2449.562672	183.765850	47.266253
2445.652734	184.707668	47.271258
2441.972850	174.700067	47.276263
2438.533911	171.410777	47.281268
2435.336660	175.917222	47.286273
2431.440630	169.859667	47.291277
2428.325319	184.037159	47.296282
2424.848904	168.327077	47.301287
2420.969318	178.986242	47.306292
2417.591489	181.162947	47.311297
2414.621957	170.951501	47.316301
2411.001681	176.702347	47.321306
2407.162549	171.235466	47.326311
2404.087700	174.865674	47.331316
2400.452920	174.297942	47.336321
2397.163633	166.944998	47.341325
2393.386182	177.847987	47.346330
2390.007967	172.097526	47.351335
2386.483921	173.209163	47.356340
2382.894297	178.417177	47.361345
2379.591466	174.726816	47.366349
2375.952072	188.402550	47.371354
2372.378790	175.663106	47.376359
2368.680543	170.196197	47.381364
2365.738119	175.792654	47.386369
2362.433990	175.077869	47.391373
2358.815465	175.338677	47.396378
2354.995760	175.060936	47.401383
2351.678639	165.683590	47.406388
2347.826941	170.357387	47.411393
2344.922034	169.920302	47.416397
2340.809157	171.628182	47.421402
2337.653795	171.827118	47.426407
2334.486823	172.171026	47.431412
2331.061263	175.488833	47.436417
2328.044240	167.956255	47.441421
2323.969781	179.067095	47.446426
2320.054532	164.733823	47.451431
2316.494696	167.187627	47.456436
2313.094497	170.628232	47.461441
2309.573767	166.432108	47.466445
2306.084372	174.489758	47.471450
2302.446805	170.422318	47.476455
2299.106863	170.001058	47.481460
2295.304433	170.982048	47.486465
2292.627126	159.545774	47.491469
2289.229013	168.204496	47.496474
2285.332103	175.517897	47.501479
2282.221595	175.969720	47.506484
2278.418962	172.789623	47.511489
2275.150738	169.535399	47.516493
2271.291821	168.590823	47.521498
2267.652551	171.617540	47.526503
2264.667199	170.262809	47.531508
2260.926715	173.129722	47.536513
2257.502868	162.829517	47.541517
2253.768008	168.811934	47.546522
2250.591745	164.281205	47.551527
2246.903622	163.125659	47.556532
2243.376865	171.392927	47.561537
2240.074133	166.627338	47.566541
2236.435547	174.862049	47.571546
2232.641226	152.206480	47.576551
2229.688590	157.586328	47.581556
2225.799869	157.185961	47.586561
2222.743401	158.323748	47.591565
2219.154154	162.545870	47.596570
2215.395602	155.785816	47.601575
2212.168811	153.106878	47.606580
2208.190602	155.696229	47.611585
2204.746009	160.470861	47.616589
2201.565286	163.352421	47.621594
2197.888782	161.293145	47.626599
2194.787101	156.470742	47.631604
2191.267275	161.218522	47.636609
2187.760073	153.925413	47.641613
2183.912456	156.628597	47.646618
2180.293888	152.137413	47.651623
2177.144049	163.754343	47.656628
2173.274871	162.194797	47.661633
2170.219043	153.373119	47.666637
2166.430328	163.094733	47.671642
2162.914407	157.798147	47.676647
2159.501223	157.952667	47.681652
2155.843481	160.827882	47.686657
2152.626757	156.559203	47.691661
2149.102225	158.386104	47.696666
2145.551323	160.043224	47.701671
2142.179475	159.125127	47.706676
2138.237583	169.291222	47.711681
2135.160575	150.165806	47.716685
2131.555450	150.368574	47.721690
2128.408283	147.585085	47.726695
2124.677229	153.047390	47.731700
2120.893606	158.260477	47.736705
2117.471858	145.488820	47.741709
2113.960100	154.885367	47.746714
2110.673294	154.988183	47.751719
2107.319991	154.600687	47.756724
2103.427066	159.943591	47.761729
2100.196465	157.606197	47.766733
2096.292981	155.922517	47.771738
2092.964857	152.797049	47.776743
2089.699591	139.974543	47.781748
2085.853516	147.545716	47.786753
2082.777272	141.974896	47.791757
2079.185854	143.283657	47.796762
2075.420531	153.326819	47.801767
2072.169463	152.823915	47.806772
2068.278843	152.542334	47.811777
2065.048023	154.020508	47.816781
2061.673415	169.455340	47.821786
2058.235247	157.417970	47.826791
2054.703137	148.599150	47.831796
2050.927577	159.875764	47.836801
2047.629796	152.053317	47.841805
2044.096536	156.842541	47.846810
2040.510445	154.902806	47.851815
2037.143845	146.773053	47.856820
2033.471093	153.921817	47.861825
2030.511637	142.964644	47.866829
2026.530821	150.530447	47.871834
2022.993808	150.880674	47.876839
2019.765454	148.849578	47.881844
2015.860784	146.008582	47.886849
2012.593446	148.119183	47.891853
2009.082686	158.130050	47.896858
2005.219508	150.786255	47.901863
2002.395624	142.282070	47.906868
1998.424853	143.479711	47.911873
1995.383036	138.662233	47.916877
1991.342561	148.869799	47.921882
1988.106644	152.093321	47.926887
1984.670529	139.053895	47.931892
1980.601312	149.229506	47.936897
1977.994205	139.337955	47.941901
1974.184427	143.108991	47.946906
1970.902746	146.923139	47.951911
1967.226077	151.509238	47.956916
1963.471617	155.728240	47.961921
1960.257852	148.792533	47.966925
1956.705196	143.196677	47.971930
1952.790635	150.160128	47.976935
1949.345502	143.455179	47.981940
1945.941178	144.462125	47.986945
1942.801287	152.419527	47.991949
1939.491085	143.881649	47.996954
1935.632517	139.738107	48.001959
1931.974553	140.156476	48.006964
1928.625606	152.499394	48.011969
1925.223183	139.407879	48.016973
1921.460811	139.440658	48.021978
1917.956794	133.636131	48.026983
1914.612623	138.892534	48.031988
1910.966622	146.087544	48.036993
1907.534776	143.545381	48.041997
1904.174693	147.976969	48.047002
1900.506271	138.447307	48.052007
1897.146101	136.558873	48.057012
1893.399391	146.544081	48.062017
1890.003596	139.079450	48.067021
1886.647285	138.247999	48.072026
1883.128575	151.255973	48.077031
1879.687115	133.943330	48.082036
1875.966546	139.071930	48.087041
1872.525457	133.249943	48.092045
1869.126549	139.637729	48.097050
1865.521423	150.342487	48.102055
1862.484786	132.756281	48.107060
1858.444383	140.121846	48.112065
1855.176140	133.958901	48.117069
1851.311842	139.326300	48.122074
1847.645283	143.706166	48.127079
1844.339892	140.832497	48.132084
1841.019742	144.297974	48.137089
1838.022806	130.062571	48.142093
1834.438972	130.632630	48.147098
1830.737695	134.604063	48.152103
1827.072031	143.336780	48.157108
1823.318578	147.165290	48.162113
1820.017639	135.199461	48.167117
1816.495611	135.217403	48.172122
1813.005172	144.386882	48.177127
1809.696860	141.140291	48.182132
1806.111130	145.192023	48.187137
1802.445412	129.834152	48.192141
1798.735103	142.805982	48.197146
1795.610670	140.951610	48.202151
1792.465262	138.099717	48.207156
1788.504171	146.541515	48.212161
1784.904821	133.330748	48.217165
1781.510453	135.497724	48.222170
1777.823070	136.773726	48.227175
1774.502839	135.935092	48.232180
1770.764904	147.503252	48.237185
1767.752251	140.897331	48.242189
1764.093674	133.179268	48.247194
1760.385327	134.226891	48.252199
1757.425677	130.195790	48.257204
1753.472166	135.887739	48.262209
1750.239407	129.533421	48.267213
1746.584030	131.275248	48.272218
1743.099598	139.269238	48.277223
1739.423633	137.238827	48.282228
1735.808250	138.861887	48.287233
1732.374697	134.975091	48.292237
1729.128899	140.498683	48.297242
1725.543845	153.966456	48.302247
1722.158205	138.807582	48.307252
1718.152348	138.118607	48.312257
1714.948033	132.781412	48.317261
1711.631860	130.774030	48.322266
1707.694012	131.727247	48.327271
1704.568674	135.330130	48.332276
1701.258003	137.673052	48.337281
1697.570669	126.797298	48.342285
1693.951425	134.095913	48.347290
1690.316383	131.876062	48.352295
1686.962605	125.393464	48.357300
1683.074249	139.914440	48.362305
1679.680362	124.060937	48.367309
1676.774773	132.535993	48.372314
1673.139836	131.972007	48.377319
1669.699223	125.790743	48.382324
1666.156716	125.842524	48.387329
1662.452763	134.078271	48.392333
1658.893910	136.258336	48.397338
1655.020871	130.825127	48.402343
1652.282244	125.790067	48.407348
1648.613157	125.250277	48.412353
1645.018126	127.697761	48.417357
1640.987127	131.098300	48.422362
1637.645316	136.852450	48.427367
1634.440946	122.917972	48.432372
1630.989211	133.991439	48.437377
1627.684626	123.618375	48.442381
1623.843834	129.412050	48.447386
1620.466817	134.762882	48.452391
1617.151385	127.843352	48.457396
1613.456614	128.448006	48.462401
1609.916340	121.330780	48.467405
1606.364214	123.268146	48.472410
1603.082456	137.006932	48.477415
1599.893095	133.776729	48.482420
1595.726352	131.672096	48.487425
1592.164465	116.322799	48.492429
1588.936902	124.609004	48.497434
1585.219277	120.098886	48.502439
1581.783400	117.350771	48.507444
1578.399498	134.415691	48.512449
1575.107003	124.495080	48.517453
1571.412003	114.859130	48.522458
1567.619764	118.900944	48.527463
1564.504321	122.796740	48.532468
1560.502702	130.117766	48.537473
1557.262080	128.570167	48.542477
1554.026562	121.551259	48.547482
1550.536475	134.527088	48.552487
1547.304649	111.160301	48.557492
1543.395579	120.877545	48.562497
1540.028259	117.295136	48.567501
1536.106529	122.308013	48.572506
1532.598707	125.048182	48.577511
1529.511062	118.633729	48.582516
1525.649038	122.960362	48.587521
1522.120122	117.601761	48.592525
1518.968302	115.815673	48.597530
1515.258936	119.820751	48.602535
1511.980706	116.271206	48.607540
1508.518539	108.614916	48.612545
1505.228224	120.027800	48.617549
1501.333869	123.639877	48.622554
1497.338198	132.940899	48.627559
1494.343628	121.111965	48.632564
1490.397666	129.225827	48.637569
1487.100925	122.176411	48.642573
1484.124979	124.843228	48.647578
1480.258152	129.978685	48.652583
1476.945882	125.035809	48.657588
1473.436129	129.331463	48.662593
1469.843956	131.585685	48.667597
1466.209142	116.796254	48.672602
1462.725910	128.580872	48.677607
1459.430267	124.505323	48.682612
1455.506831	127.556324	48.687617
1451.789033	134.524330	48.692621
1449.000408	120.505567	48.697626
1445.573723	125.014041	48.702631
1442.078648	126.416621	48.707636
1438.123596	129.722453	48.712641
1434.622116	127.707906	48.717645
1431.201767	124.886073	48.722650
1427.931122	114.124147	48.727655
1424.524939	116.237789	48.732660
1420.340578	124.703377	48.737665
1417.237405	118.412301	48.742669
1413.562605	116.498392	48.747674
1410.046715	114.066549	48.752679
1406.539581	108.360797	48.757684
1403.599132	114.660370	48.762689
1400.165533	120.044898	48.767693
1396.649298	122.156097	48.772698
1392.718271	120.006964	48.777703
1389.503724	113.239224	48.782708
1385.432625	115.275671	48.787713
1382.011378	119.110529	48.792717
1379.201984	115.889647	48.797722
1375.070180	119.784761	48.802727
1371.516102	112.654566	48.807732
1367.962820	118.889063	48.812737
1364.784677	120.317704	48.817741
1361.414186	119.201952	48.822746
1357.319976	129.754788	48.827751
1354.129473	106.976033	48.832756
1350.511383	122.031732	48.837761
1347.520383	119.967209	48.842765
1344.061735	123.737226	48.847770
1340.032388	127.079938	48.852775
1336.739833	124.759255	48.857780
1333.087623	127.942940	48.862785
1329.690757	116.614694	48.867789
1326.176390	119.060363	48.872794
1322.467763	125.639581	48.877799
1319.440459	124.999164	48.882804
1315.575068	127.534645	48.887809
1312.102666	113.410597	48.892813
1308.900216	122.346758	48.897818
1304.887743	117.562072	48.902823
1301.685269	126.410437	48.907828
1297.971866	129.598616	48.912833
1294.296978	118.724526	48.917837
1291.478343	112.344030	48.922842
1287.679094	117.909027	48.927847
1284.435052	124.277404	48.932852
1280.503768	129.994825	48.937857
1277.118279	116.776924	48.942861
1274.087726	115.494903	48.947866
1270.021234	125.821718	48.952871
1266.408583	108.419682	48.957876
1263.384397	122.983541	48.962881
1259.554106	124.787435	48.967885
1255.811516	121.670921	48.972890
1252.307350	119.723508	48.977895
1249.469514	118.563789	48.982900
1245.902057	121.811367	48.987905
1242.090904	120.886308	48.992909
1238.717686	124.723762	48.997914
1235.061301	135.060743	49.002919
1231.695323	116.572236	49.007924
1227.796419	122.218827	49.012929
1224.442541	119.006203	49.017933
1221.589882	120.435046	49.022938
1217.781438	119.736860	49.027943
1214.296545	112.696066	49.032948
1210.421760	119.150535	49.037953
1207.158175	119.152165	49.042957
1203.709416	114.357855	49.047962
1199.950858	124.874199	49.052967
1196.520544	113.538931	49.057972
1193.066989	119.055986	49.062977
1189.311156	116.155784	49.067981
1186.264091	120.673134	49.072986
1182.722043	120.433750	49.077991
1179.038933	117.003007	49.082996
1175.324815	119.415622	49.088001
1171.953649	110.366657	49.093005
1168.597399	113.810163	49.098010
1164.947204	118.902219	49.103015
1161.908114	115.507237	49.108020
1157.841282	122.409178	49.113025
1154.581673	112.893507	49.118029
1151.251186	118.250072	49.123034
1147.328159	108.584261	49.128039
1143.958710	113.639844	49.133044
1140.560831	114.525446	49.138049
1136.900924	115.156361	49.143053
1133.310755	116.157668	49.148058
1129.659028	122.597552	49.153063
1126.825530	101.339926	49.158068
1123.153831	106.791996	49.163073
1119.494531	111.868605	49.168077
1115.976154	112.149710	49.173082
1112.400827	125.492560	49.178087
1109.202210	111.979025	49.183092
1105.524953	111.969972	49.188097
1101.783134	121.009064	49.193101
1098.472522	111.411576	49.198106
1094.528153	120.793104	49.203111
1091.516838	104.605345	49.208116
1087.828851	120.615839	49.213121
1084.548352	126.601410	49.218125
1080.990396	120.211261	49.223130
1077.279290	124.419089	49.228135
1073.997099	118.347660	49.233140
1070.356942	113.622513	49.238145
1067.075198	117.338687	49.243149
1063.697313	117.303416	49.248154
1059.971429	117.508411	49.253159
1056.576075	112.710003	49.258164
1052.846481	118.606845	49.263169
1049.458635	101.037630	49.268173
1045.993894	113.136819	49.273178
1042.533431	121.746402	49.278183
1039.002033	114.751074	49.283188
1035.353823	110.985830	49.288193
1031.796914	108.862459	49.293197
1028.457015	111.170056	49.298202
1025.054309	114.752314	49.303207
1021.601309	109.794938	49.308212
1017.691275	113.726938	49.313217
1014.060368	112.004798	49.318221
1010.750601	107.342147	49.323226
1007.314739	119.025681	49.328231
1004.233287	107.318125	49.333236
1000.531593	113.208213	49.338241
996.905007	119.432684	49.343245
993.236402	120.645314	49.348250
989.717783	115.366807	49.353255
986.322830	111.875873	49.358260
983.099409	112.036526	49.363265
979.373753	114.025936	49.368269
976.109988	107.845566	49.373274
972.421097	116.407750	49.378279
968.873184	105.167914	49.383284
964.882225	107.488227	49.388289
961.494382	113.358972	49.393293
958.441422	99.794658	49.398298
955.059697	115.182222	49.403303
951.628120	101.035503	49.408308
948.509360	110.000100	49.413313
944.625474	107.900970	49.418317
940.923618	105.217435	49.423322
936.863103	110.341534	49.428327
933.542483	112.649544	49.433332
930.276015	107.701969	49.438337
927.069171	98.908775	49.443341
923.353514	109.529532	49.448346
919.907376	111.664215	49.453351
916.473080	103.013551	49.458356
912.628546	111.938866	49.463361
909.226446	108.898241	49.468365
905.769975	102.752888	49.473370
901.883602	109.559455	49.478375
898.696630	110.398512	49.483380
895.501396	109.419899	49.488385
891.588759	106.046562	49.493389
888.225957	99.058911	49.498394
884.939822	105.174137	49.503399
881.350795	110.386157	49.508404
877.569469	109.012230	49.513409
874.628786	116.344773	49.518413
871.122323	105.107824	49.523418
867.018848	114.824231	49.528423
863.862656	107.494369	49.533428
859.817934	112.092824	49.538433
857.004008	117.377539	49.543437
853.555639	109.989673	49.548442
849.716465	111.945609	49.553447
846.537568	98.961049	49.558452
842.430005	115.112339	49.563457
839.398509	113.067662	49.568461
835.799044	103.965145	49.573466
831.894949	110.361006	49.578471
828.635678	108.472040	49.583476
825.270619	113.809494	49.588481
821.605696	105.650594	49.593485
818.480341	96.909022	49.598490
814.455221	106.094564	49.603495
811.280961	106.451992	49.608500
807.885015	108.159939	49.613505
804.100596	110.062068	49.618509
800.886674	112.177406	49.623514
796.691878	113.820357	49.628519
794.021624	99.505306	49.633524
790.404399	115.544375	49.638529
786.596692	113.912132	49.643533
783.432182	104.597236	49.648538
780.274247	109.913232	49.653543
776.380885	112.677572	49.658548
772.085069	107.012846	49.663553
768.619559	110.394765	49.668557
765.176784	114.025592	49.673562
762.051134	126.981183	49.678567
758.754632	104.713448	49.683572
755.344833	112.644606	49.688577
751.894171	112.134540	49.693581
748.692754	109.106737	49.698586
744.433157	105.013670	49.703591
741.361922	102.702226	49.708596
737.812419	110.029104	49.713601
733.953228	114.832387	49.718605
730.947227	104.426838	49.723610
727.295724	98.190281	49.728615
723.813148	93.892551	49.733620
719.784398	98.473744	49.738625
716.451769	101.598051	49.743629
712.797083	99.051195	49.748634
709.343179	106.986990	49.753639
706.252355	107.448879	49.758644
702.761235	105.055162	49.763649
699.179194	108.941059	49.768653
695.849714	94.932251	49.773658
691.843423	108.097512	49.778663
688.297466	108.078644	49.783668
685.207173	101.426525	49.788673
681.468495	106.137517	49.793677
678.248190	105.704579	49.798682
674.449476	113.095040	49.803687
671.164019	113.621646	49.808692
667.754768	118.069781	49.813697
663.971172	108.666787	49.818701
660.651974	98.682871	49.823706
656.933793	103.554949	49.828711
653.751091	109.582457	49.833716
650.148693	109.851044	49.838721
646.173529	114.595390	49.843725
643.037356	110.917867	49.848730
639.517077	118.808229	49.853735
636.051461	97.593075	49.858740
632.367482	103.298887	49.863745
629.042612	91.796917	49.868749
625.528001	104.336022	49.873754
621.984246	114.737426	49.878759
618.805856	96.813585	49.883764
615.331235	97.720311	49.888769
611.363152	110.719674	49.893773
607.923095	103.964948	49.898778
604.476211	108.779619	49.903783
601.308866	105.492225	49.908788
597.536974	100.422415	49.913793
593.921337	103.024867	49.918797
590.393831	98.116056	49.923802
586.787776	107.547214	49.928807
583.361893	101.822406	49.933812
579.853755	110.931758	49.938817
576.137939	103.039213	49.943821
572.966187	101.467705	49.948826
569.595945	102.077523	49.953831
566.180119	102.273609	49.958836
562.711330	98.523702	49.963841
558.746609	99.798990	49.968845
555.685890	105.787250	49.973850
552.243180	105.393280	49.978855
548.727969	99.634115	49.983860
545.089327	99.792332	49.988865
541.428533	106.922413	49.993869
537.770274	108.891162	49.998874
534.223385	105.203596	50.003879
531.107397	100.442610	50.008884
527.765829	100.440483	50.013889
523.816431	105.954599	50.018893
520.422912	105.403648	50.023898
516.578461	113.995781	50.028903
513.306168	106.686870	50.033908
509.837184	105.182445	50.038913
506.448454	108.190530	50.043917
503.061284	103.660614	50.048922
499.453812	99.641923	50.053927
495.934823	97.420938	50.058932
492.237091	100.239348	50.063937
488.401783	109.210204	50.068941
485.582668	92.554437	50.073946
481.965352	104.970177	50.078951
478.526149	94.962888	50.083956
474.671999	100.018230	50.088961
471.342940	107.359822	50.093965
468.126267	92.874865	50.098970
464.640510	102.832562	50.103975
460.849754	91.600924	50.108980
457.321629	102.356747	50.113985
453.534765	112.651975	50.118989
450.684603	104.751972	50.123994
446.833578	109.543206	50.128999
443.633046	98.159520	50.134004
439.972048	101.706288	50.139009
436.439789	102.756801	50.144013
432.830065	94.702198	50.149018
429.170161	94.707622	50.154023
425.767845	95.162890	50.159028
422.224854	93.422520	50.164033
418.863227	104.358628	50.169037
415.399645	87.680326	50.174042
411.700112	106.746283	50.179047
408.045268	98.816056	50.184052
404.945648	94.176150	50.189057
401.095143	96.554681	50.194061
397.869927	89.364842	50.199066
394.462228	103.401047	50.204071
390.856583	91.800192	50.209076
387.330926	92.705996	50.214081
383.807712	106.000256	50.219085
380.216856	99.499068	50.224090
376.859721	103.928270	50.229095
373.332988	95.721975	50.234100
369.562843	107.806173	50.239105
366.134564	109.148340	50.244109
362.600248	103.183489	50.249114
359.057935	112.003505	50.254119
355.720834	103.329434	50.259124
352.739567	93.036142	50.264129
349.190189	106.482821	50.269133
345.485156	100.282674	50.274138
341.593504	102.833484	50.279143
338.199709	96.237418	50.284148
334.999348	101.448142	50.289153
331.308679	102.706210	50.294157
327.793526	87.659978	50.299162
324.280109	100.442390	50.304167
320.814801	99.541731	50.309172
317.182060	106.460799	50.314177
313.420300	103.260707	50.319181
310.263550	95.490754	50.324186
306.929830	100.085808	50.329191
303.488115	100.072915	50.334196
299.827479	100.949963	50.339201
295.846152	99.786806	50.344205
292.831947	88.302788	50.349210
289.239405	99.423203	50.354215
285.415882	105.470115	50.359220
282.017922	106.257703	50.364225
278.406665	92.427926	50.369229
275.345110	88.647312	50.374234
271.518293	105.910198	50.379239
268.068525	105.780860	50.384244
264.821835	102.722611	50.389249
261.021515	104.789564	50.394253
257.952651	94.678316	50.399258
254.416205	90.585197	50.404263
250.574498	91.530565	50.409268
247.334554	87.704855	50.414273
243.468858	100.975149	50.419277
240.441224	92.421787	50.424282
236.695397	84.917613	50.429287
233.002488	80.376023	50.434292
229.237369	80.641539	50.439297
225.771740	85.422191	50.444301
222.603802	85.922502	50.449306
218.951552	91.121315	50.454311
215.574363	86.731492	50.459316
212.001305	87.742004	50.464321
208.891557	94.326097	50.469325
205.384994	89.295377	50.474330
201.786058	88.023029	50.479335
198.176817	83.967131	50.484340
194.898872	88.172799	50.489345
191.186392	88.182902	50.494349
187.923614	85.254919	50.499354
183.729289	95.141276	50.504359
180.259123	82.361743	50.509364
177.067462	85.313255	50.514369
173.313110	89.356435	50.519373
170.265256	81.440226	50.524378
166.506883	83.508785	50.529383
163.112462	93.103458	50.534388
160.069371	83.358964	50.539393
156.220379	94.459655	50.544397
152.741316	83.897718	50.549402
149.144831	89.876502	50.554407
145.393394	88.215325	50.559412
142.354735	88.198963	50.564417
138.693223	90.926933	50.569421
135.271636	84.457822	50.574426
131.555176	82.603429	50.579431
127.752815	82.114818	50.584436
124.531757	86.448349	50.589441
120.595306	91.862284	50.594445
117.251721	82.631939	50.599450
113.929431	85.588689	50.604455
110.618011	88.448540	50.609460
107.686414	86.697596	50.614465
103.638672	84.901710	50.619469
100.254847	86.429936	50.624474
96.372398	82.347325	50.629479
92.874066	92.978215	50.634484
89.558204	91.393969	50.639489
85.845518	89.506226	50.644493
82.554268	89.761302	50.649498
78.929008	84.840347	50.654503
75.403666	83.994239	50.659508
72.033745	77.441851	50.664513
68.021550	87.208494	50.669517
65.018566	87.896991	50.674522
61.930354	84.155227	50.679527
57.790520	94.713078	50.684532
54.663535	85.810821	50.689537
50.747560	92.668693	50.694541
47.585010	83.315838	50.699546
43.990204	90.491092	50.704551
40.245606	96.073739	50.709556
37.179427	83.879955	50.714561
33.227656	80.218856	50.719565
29.984365	77.943308	50.724570
26.850828	91.241676	50.729575
22.694596	97.984378	50.734580
19.810141	91.559461	50.739585
15.848712	92.631598	50.744589
12.613891	83.456942	50.749594
9.036033	89.050427	50.754599
5.475878	89.939449	50.759604
1.950732	88.596915	50.764609