Thu Jun 16 18:21:46 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.383504	82.418606	0.000000
0.991205	96.067223	0.005005
0.737621	112.088792	0.010010
1.020197	110.509380	0.015014
1.198749	97.260404	0.020019
0.639665	83.936815	0.025024
0.906243	75.353138	0.030029
0.800736	84.436331	0.035034
0.655022	71.870781	0.040038
0.292515	57.825226	0.045043
-0.491619	45.975778	0.050048
-0.532304	31.761440	0.055053
-0.635940	27.807695	0.060058
-1.254782	15.776757	0.065062
-1.381302	6.648095	0.070067
-1.601001	9.271238	0.075072
-1.734587	-9.871709	0.080077
-2.184444	-2.181792	0.085082
-2.665260	1.729725	0.090086
-2.579161	2.314433	0.095091
-3.471151	-0.708143	0.100096
-3.688493	-10.259715	0.105101
-4.021496	-6.829399	0.110106
-3.982244	-13.687571	0.115110
-3.791464	-8.173899	0.120115
-4.122103	-3.544131	0.125120
-4.924458	-0.824307	0.130125
-5.221166	4.360611	0.135130
-5.953987	2.152272	0.140134
-5.906700	-5.404722	0.145139
-5.868576	1.240400	0.150144
-5.966357	-10.622391	0.155149
-6.058315	-8.992507	0.160154
-6.094301	-5.458754	0.165158
-6.552668	-4.621289	0.170163
-7.275181	-1.399681	0.175168
-7.089488	-9.542767	0.180173
-7.199045	-7.068546	0.185178
-7.638181	-7.947995	0.190182
-8.395129	-19.808690	0.195187
-8.897401	-14.600265	0.200192
-8.638613	-1.201880	0.205197
-8.823837	-3.302908	0.210202
-9.083351	-11.426877	0.215206
-8.642005	-14.190033	0.220211
-9.090432	-6.407618	0.225216
-9.443134	-5.310296	0.230221
-9.839770	-12.239977	0.235226
-10.325286	-7.230050	0.240230
-10.258029	-5.837106	0.245235
-10.535127	0.889705	0.250240
-11.189785	-5.591670	0.255245
-11.699577	-2.046209	0.260250
-11.708491	4.461763	0.265254
-11.866188	-2.363176	0.270259
-11.963870	3.482199	0.275264
-11.717615	-6.217020	0.280269
-12.452824	0.973310	0.285274
-13.262256	0.452599	0.290278
-13.239875	-2.523771	0.295283
-13.514272	4.580443	0.300288
-13.393461	-6.953252	0.305293
-13.424096	-2.599377	0.310298
-13.596810	0.261454	0.315302
-14.230426	-9.712627	0.320307
-14.829890	-1.938201	0.325312
-14.926449	-14.049701	0.330317
-15.198962	1.361343	0.335322
-15.250524	0.446652	0.340326
-15.098085	-11.833462	0.345331
-16.124522	4.070259	0.350336
-16.341817	-9.671199	0.355341
-16.557838	-4.622642	0.360346
-16.877494	-4.800470	0.365350
-16.775506	-2.481270	0.370355
-16.934652	5.328026	0.375360
-16.562268	2.147114	0.380365
-17.322576	0.860318	0.385370
-17.961048	-1.735441	0.390374
-18.146466	-2.569114	0.395379
-18.427120	-1.272871	0.400384
-18.240367	-8.807826	0.405389
-18.428029	-7.834755	0.410394
-19.353145	-2.614457	0.415398
-19.810417	-15.492186	0.420403
-19.859856	-4.003634	0.425408
-19.808578	-7.093398	0.430413
-19.942975	0.516271	0.435418
-19.783323	-3.572231	0.440422
-20.031593	-5.757252	0.445427
-21.166858	-8.837190	0.450432
-21.178932	-12.841965	0.455437
-21.400247	-7.731466	0.460442
-21.602451	-3.844683	0.465446
-21.440761	-14.213304	0.470451
-21.904897	-12.538982	0.475456
-22.072287	-1.794033	0.480461
-22.811400	5.005185	0.485466
-22.808611	-2.393218	0.490470
-22.951836	-12.002712	0.495475
-23.135697	-0.844438	0.500480
-23.441635	-9.037982	0.505485
-24.041170	-10.030420	0.510490
-24.796220	-5.845198	0.515494
-24.604108	-8.762603	0.520499
-24.927025	0.485705	0.525504
-24.926721	-20.359939	0.530509
-24.750566	-8.661543	0.535514
-24.771677	-8.535523	0.540518
-24.956056	-0.731432	0.545523
-25.901413	-12.917926	0.550528
-26.052669	-8.442504	0.555533
-26.336594	-5.038944	0.560538
-26.567501	-13.754043	0.565542
-26.516522	-11.612775	0.570547
-27.358680	-2.607970	0.575552
-27.878888	-9.023164	0.580557
-27.587811	-7.620841	0.585562
-27.768353	-12.001274	0.590566
-27.860997	-10.906776	0.595571
-28.155399	9.013563	0.600576
-28.259242	6.037630	0.605581
-29.036690	-3.303685	0.610586
-29.409788	-15.544989	0.615590
-29.124394	-9.042253	0.620595
-29.559013	-4.247418	0.625600
-29.621905	-11.257606	0.630605
-29.850439	-3.797728	0.635610
-30.558000	-5.547939	0.640614
-30.804210	-11.466502	0.645619
-31.186901	-3.428383	0.650624
-31.243380	-8.043204	0.655629
-31.226722	-7.450376	0.660634
-31.439102	-1.832686	0.665638
-31.264276	-3.112818	0.670643
-32.436536	-4.846609	0.675648
-32.587345	-20.164796	0.680653
-32.775514	-14.574001	0.685658
-32.857937	-11.112486	0.690662
-32.682557	-3.990562	0.695667
-32.929967	1.794219	0.700672
-33.490748	-1.766596	0.705677
-34.146730	-8.016894	0.710682
-34.332818	-2.708098	0.715686
-34.336740	-10.775452	0.720691
-34.456557	1.853247	0.725696
-34.710394	-11.305036	0.730701
-34.974487	-3.185988	0.735706
-35.559635	-5.196358	0.740710
-35.526918	-3.437516	0.745715
-35.763367	-4.372262	0.750720
-35.966080	-2.557346	0.755725
-36.310481	-13.952099	0.760730
-36.285364	-14.065558	0.765734
-37.302504	-7.589564	0.770739
-37.397756	-5.086335	0.775744
-37.144709	-1.864645	0.780749
-37.618129	-7.731059	0.785754
-37.849313	-5.482783	0.790758
-37.492531	-7.405336	0.795763
-38.213200	0.873716	0.800768
-38.525618	-7.657734	0.805773
-38.868088	-5.396986	0.810778
-39.187393	-0.305116	0.815782
-38.890030	-14.511935	0.820787
-39.753442	-3.807147	0.825792
-40.657836	-4.624798	0.830797
-40.850436	-1.230115	0.835802
-40.229195	-16.616603	0.840806
-40.627058	-12.330491	0.845811
-40.614754	-4.823401	0.850816
-40.901029	-6.108129	0.855821
-40.830714	-2.993569	0.860826
-41.599791	-0.707305	0.865830
-41.754798	-10.606869	0.870835
-42.379682	-2.094348	0.875840
-42.140394	-11.183708	0.880845
-42.193713	-4.324986	0.885850
-42.654360	-9.761794	0.890854
-43.309335	-8.239134	0.895859
-43.603759	1.235811	0.900864
-43.794385	-5.048182	0.905869
-43.641385	-8.016935	0.910874
-44.161332	-7.739714	0.915878
-44.111048	-7.423053	0.920883
-45.156454	0.839029	0.925888
-45.312950	-14.448132	0.930893
-45.174770	-7.713992	0.935898
-45.573609	-10.217939	0.940902
-45.350833	-7.681242	0.945907
-45.354670	1.015140	0.950912
-45.603262	1.607509	0.955917
-46.024775	-4.148505	0.960922
-46.536532	-0.970011	0.965926
-46.491856	-6.180850	0.970931
-47.266188	-9.914630	0.975936
-47.812136	-8.787441	0.980941
-47.990364	-8.035042	0.985946
-48.454330	-3.320397	0.990950
-48.008000	-10.605834	0.995955
-48.161341	0.244820	1.000960
-48.236532	-5.328992	1.005965
-48.344990	-4.796975	1.010970
-48.964381	-15.724726	1.015974
-49.569945	-13.179682	1.020979
-49.856623	0.193515	1.025984
-50.182660	0.537444	1.030989
-50.132464	-9.532275	1.035994
-50.101504	-6.072826	1.040998
-50.183074	-1.979862	1.046003
-51.233761	-5.735549	1.051008
-51.281364	-4.666055	1.056013
-51.146139	6.220573	1.061018
-51.753668	1.556827	1.066022
-51.669997	-11.746217	1.071027
-51.914197	-11.738414	1.076032
-52.072514	-12.146527	1.081037
-52.815348	-11.617994	1.086042
-52.942153	1.100646	1.091046
-53.182295	-7.586783	1.096051
-53.401749	-1.727207	1.101056
-53.622265	-14.972183	1.106061
-54.616798	-8.488777	1.111066
-54.323204	-5.872724	1.116070
-54.071275	-10.874925	1.121075
-54.891832	-5.069517	1.126080
-54.891757	-9.630148	1.131085
-54.805597	-14.278799	1.136090
-55.059841	-26.771373	1.141094
-55.606850	-10.612263	1.146099
-56.190483	-6.523242	1.151104
-56.572201	-7.839550	1.156109
-56.703328	-9.283101	1.161114
-57.435764	-10.137553	1.166118
-56.871265	-10.072502	1.171123
-57.216394	-6.274665	1.176128
-57.050733	-8.685940	1.181133
-57.106617	-3.034133	1.186138
-57.993504	-0.595706	1.191142
-58.042342	-4.024082	1.196147
-58.380390	4.344949	1.201152
-58.435797	-4.428554	1.206157
-58.567898	-0.568746	1.211162
-59.153286	-10.693837	1.216166
-59.410528	-8.436520	1.221171
-59.814077	-5.027001	1.226176
-59.747156	0.668144	1.231181
-60.000039	-11.325177	1.236186
-60.467628	-2.663637	1.241190
-60.854625	-12.218830	1.246195
-61.428148	3.350083	1.251200
-61.251640	5.209960	1.256205
-61.212801	-9.006818	1.261210
-61.753677	3.943727	1.266214
-61.518054	-10.468648	1.271219
-61.769352	-10.519457	1.276224
-62.430413	-8.265151	1.281229
-63.051438	-7.394980	1.286234
-63.480315	-9.892976	1.291238
-63.282442	-10.132752	1.296243
-63.387218	-0.187195	1.301248
-63.555104	-11.574910	1.306253
-63.184536	-5.468639	1.311258
-63.776053	-4.370618	1.316262
-64.262839	-7.078255	1.321267
-64.855676	-3.017703	1.326272
-65.040978	-1.397943	1.331277
-64.711666	-7.038702	1.336282
-65.624172	-0.139600	1.341286
-65.968550	-4.781719	1.346291
-66.258769	-4.803996	1.351296
-66.475528	-12.880467	1.356301
-66.281586	-12.268499	1.361306
-66.883339	-10.940301	1.366310
-66.646953	-13.134877	1.371315
-67.070925	-3.293431	1.376320
-67.136434	-14.918655	1.381325
-67.775247	-7.783621	1.386330
-68.098970	-2.288017	1.391334
-68.249556	-5.781559	1.396339
-68.206878	-5.423587	1.401344
-68.418477	-6.973605	1.406349
-68.792093	-6.821983	1.411354
-69.600997	-10.913983	1.416358
-69.746837	-17.134832	1.421363
-69.635606	-0.192558	1.426368
-69.812078	-3.976406	1.431373
-69.624962	-9.916956	1.436378
-70.677234	-6.624961	1.441382
-70.857961	-16.387478	1.446387
-71.161423	-7.167253	1.451392
-71.343289	-8.511656	1.456397
-71.281925	-5.557807	1.461402
-71.452399	-6.318378	1.466406
-71.526467	-6.566190	1.471411
-72.148248	8.884820	1.476416
-72.580963	-4.651246	1.481421
-72.952140	-9.772441	1.486426
-73.319193	-8.076573	1.491430
-73.101718	-10.311629	1.496435
-73.013090	2.955542	1.501440
-73.475938	-4.752925	1.506445
-73.518387	-9.569542	1.511450
-74.546419	-3.772166	1.516454
-74.585639	-11.250237	1.521459
-74.569036	-2.934297	1.526464
-74.824241	-8.824634	1.531469
-74.879151	-15.472593	1.536474
-75.802955	-12.402297	1.541478
-75.932283	-14.317122	1.546483
-76.262733	13.184190	1.551488
-76.077479	-7.471630	1.556493
-76.347574	-0.037933	1.561498
-76.316584	-5.872475	1.566502
-76.752261	-11.717792	1.571507
-77.646937	-14.207665	1.576512
-77.751591	-10.169687	1.581517
-77.531966	0.580356	1.586522
-77.894405	2.947895	1.591526
-77.792073	3.094752	1.596531
-78.559717	-4.497242	1.601536
-79.145410	-9.909927	1.606541
-79.198533	-9.384983	1.611546
-79.736959	-13.761019	1.616550
-79.402653	-5.981589	1.621555
-79.576361	-2.467794	1.626560
-79.579766	1.750566	1.631565
-79.459920	2.762692	1.636570
-80.462191	-8.749449	1.641574
-81.063167	-2.785682	1.646579
-81.338007	6.750153	1.651584
-81.323475	6.733744	1.656589
-81.186770	13.106859	1.661594
-81.394403	6.209871	1.666598
-81.743231	1.669214	1.671603
-82.356670	-2.153502	1.676608
-82.699820	-1.593549	1.681613
-82.867941	3.975292	1.686618
-83.100690	-1.507170	1.691622
-82.809518	-2.625104	1.696627
-83.273535	-11.069931	1.701632
-83.667312	4.704765	1.706637
-84.233312	-5.027528	1.711642
-84.215845	5.164689	1.716646
-84.382474	-5.543797	1.721651
-84.888635	-1.744108	1.726656
-84.450862	-5.134715	1.731661
-85.302417	-12.038333	1.736666
-86.125473	-5.717334	1.741670
-85.894882	-2.359937	1.746675
-86.218379	-5.437581	1.751680
-86.163339	-9.478900	1.756685
-86.354349	-2.998554	1.761690
-86.210582	-3.187954	1.766694
-86.551274	-5.065579	1.771699
-87.235013	6.526717	1.776704
-87.106986	7.878936	1.781709
-87.352920	15.691725	1.786714
-88.189994	3.757260	1.791718
-88.659884	-5.641776	1.796723
-89.028796	0.197317	1.801728
-89.023599	-1.608827	1.806733
-89.105386	-8.948553	1.811738
-89.464412	5.810469	1.816742
-89.412570	-2.626881	1.821747
-89.293648	-5.323436	1.826752
-89.374291	-3.243582	1.831757
-89.745202	2.122298	1.836762
-90.585652	2.331541	1.841766
-90.753665	2.968801	1.846771
-91.203528	6.569771	1.851776
-90.990414	-2.793769	1.856781
-91.780228	0.040108	1.861786
-92.573483	-3.059640	1.866790
-91.761385	2.424150	1.871795
-92.348457	3.633414	1.876800
-92.503399	-3.422726	1.881805
-92.653793	-5.580411	1.886810
-92.349046	8.074075	1.891814
-92.786233	-3.702722	1.896819
-93.825138	4.092837	1.901824
-94.056903	-3.175836	1.906829
-94.201099	-0.702795	1.911834
-94.213677	-1.385380	1.916838
-93.998609	-2.881312	1.921843
-94.536606	-0.824131	1.926848
-95.215323	-1.890884	1.931853
-95.441496	-13.804951	1.936858
-95.944404	9.648533	1.941862
-95.815914	-3.409659	1.946867
-95.916015	1.711984	1.951872
-95.672448	0.043530	1.956877
-96.345816	4.899827	1.961882
-96.967878	3.072058	1.966886
-97.157836	0.011904	1.971891
-97.828364	4.078788	1.976896
-97.586032	-0.820018	1.981901
-97.799441	-7.216849	1.986906
-97.581215	1.787725	1.991910
-97.660897	-12.238487	1.996915
-98.786714	2.434790	2.006912
-98.274271	0.919649	2.016909
-97.707946	-5.348069	2.026906
-97.404343	3.629377	2.036902
-96.530410	-2.942555	2.046899
-96.426187	-7.698609	2.056896
-95.718372	0.082072	2.066893
-94.997727	-5.831435	2.076890
-95.012586	-4.025330	2.086886
-94.023476	-6.435478	2.096883
-93.445332	-3.153694	2.106880
-93.183317	-4.846246	2.116877
-93.183226	-8.146341	2.126874
-92.280697	-6.966398	2.136870
-91.859335	-4.441149	2.146867
-90.753939	0.428432	2.156864
-90.347612	3.407992	2.166861
-90.255616	-4.191931	2.176858
-90.182957	-3.867388	2.186854
-88.971620	-4.448186	2.196851
-88.905244	-5.132150	2.206848
-88.268646	-0.741822	2.216845
-87.674822	-1.087209	2.226842
-87.359455	-10.224237	2.236838
-86.876961	-6.507023	2.246835
-86.182120	2.169578	2.256832
-86.004745	3.035521	2.266829
-84.800433	-5.997816	2.276826
-84.285506	-4.191747	2.286822
-84.641198	-6.329558	2.296819
-83.923414	-0.177745	2.306816
-83.314474	-2.346564	2.316813
-82.536906	-2.539968	2.326810
-81.706314	-1.710957	2.336806
-81.779187	-1.658805	2.346803
-81.621307	-3.470662	2.356800
-80.725383	4.939585	2.366797
-80.131475	0.678000	2.376794
-79.573670	4.540821	2.386790
-78.640499	6.624195	2.396787
-78.872536	4.396009	2.406784
-78.215960	1.865582	2.416781
-77.756411	9.121581	2.426778
-76.775951	0.829448	2.436774
-76.392219	5.553666	2.446771
-76.635129	4.159609	2.456768
-75.956350	0.227658	2.466765
-75.304072	1.036551	2.476762
-74.654361	8.292930	2.486758
-73.935415	2.220861	2.496755
-73.671090	2.178958	2.506752
-73.438927	3.967256	2.516749
-72.564265	-7.984817	2.526746
-72.086679	-4.743113	2.536742
-71.606824	2.721118	2.546739
-70.747169	7.459044	2.556736
-70.307755	6.966112	2.566733
-70.032807	7.111817	2.576730
-70.259700	6.323605	2.586726
-69.221226	8.153096	2.596723
-68.848258	2.729412	2.606720
-68.095501	0.985391	2.616717
-67.362323	-1.401423	2.626714
-67.176500	-2.136342	2.636710
-67.018368	-0.800476	2.646707
-65.979957	-1.396945	2.656704
-65.688576	-1.252672	2.666701
-65.222246	0.888002	2.676698
-64.007434	-10.105998	2.686694
-63.788914	-3.262093	2.696691
-63.999281	5.358155	2.706688
-63.518325	2.893597	2.716685
-62.569664	-1.761977	2.726682
-62.169858	0.992751	2.736678
-61.208955	0.455124	2.746675
-60.830355	3.755864	2.756672
-60.821365	4.840976	2.766669
-60.504356	-7.984030	2.776666
-59.579717	-3.340316	2.786662
-59.391180	0.759464	2.796659
-58.768682	0.839829	2.806656
-57.766933	3.856815	2.816653
-57.844281	-4.641494	2.826650
-57.356883	-13.010479	2.836646
-56.629924	-6.220967	2.846643
-55.979845	-8.665860	2.856640
-55.191250	-3.993932	2.866637
-54.801087	3.506362	2.876634
-54.788218	4.460047	2.886630
-54.570788	-3.300187	2.896627
-53.716810	3.153423	2.906624
-53.185118	1.403265	2.916621
-52.164653	-7.610847	2.926618
-51.538109	-2.769991	2.936614
-51.711644	-3.708081	2.946611
-51.564096	-1.949756	2.956608
-50.743098	1.205564	2.966605
-49.641196	-1.616566	2.976602
-49.759840	2.666446	2.986598
-49.154161	2.435763	2.996595
-48.536367	-2.105762	3.006592
-48.332964	1.188964	3.016589
-47.460263	3.257246	3.026586
-46.793573	5.695135	3.036582
-46.757892	7.506522	3.046579
-46.272000	0.511531	3.056576
-45.390042	10.269203	3.066573
-45.090890	-6.091303	3.076570
-44.758340	-7.954745	3.086566
-43.716895	-1.449337	3.096563
-43.725945	6.546831	3.106560
-43.406578	-6.292298	3.116557
-42.225596	-7.274062	3.126554
-41.956303	-2.320822	3.136550
-41.838134	-5.179915	3.146547
-41.256302	-5.934147	3.156544
-40.816282	4.261752	3.166541
-39.505953	1.356280	3.176538
-39.560809	-0.068363	3.186534
-39.184031	1.280958	3.196531
-38.774879	5.918596	3.206528
-37.789257	-2.508629	3.216525
-37.281715	1.135406	3.226522
-37.339451	1.839383	3.236518
-37.139424	-1.857569	3.246515
-36.258438	-2.999862	3.256512
-35.228558	-1.228906	3.266509
-34.476346	3.826582	3.276506
-34.377989	0.676888	3.286502
-34.212666	-4.687387	3.296499
-33.936119	4.933259	3.306496
-33.086019	9.765528	3.316493
-32.660438	-1.531203	3.326490
-31.978887	-2.052690	3.336486
-31.443565	-3.452772	3.346483
-31.150780	2.316473	3.356480
-30.778123	2.278697	3.366477
-29.667463	-5.954439	3.376474
-29.121160	-4.193458	3.386470
-29.301458	0.611332	3.396467
-28.633455	5.957623	3.406464
-27.951972	8.118260	3.416461
-27.604612	-0.175334	3.426458
-27.051548	9.542754	3.436454
-26.132712	1.878883	3.446451
-25.963973	2.204144	3.456448
-25.932862	4.883686	3.466445
-24.892244	-1.860602	3.476442
-24.358299	-1.777946	3.486438
-24.319653	1.932417	3.496435
-23.458533	-4.751879	3.506432
-23.195550	-1.999232	3.516429
-22.455028	3.617688	3.526426
-21.477385	6.787825	3.536422
-21.331865	-1.425294	3.546419
-21.391824	0.085600	3.556416
-20.847715	5.529812	3.566413
-19.919270	-3.236167	3.576410
-19.663191	4.879671	3.586406
-18.407419	7.331441	3.596403
-18.651153	0.993113	3.606400
-18.223316	6.121079	3.616397
-17.643648	-0.165144	3.626394
-16.929547	-5.546616	3.636390
-16.536345	2.913632	3.646387
-16.055942	1.176595	3.656384
-15.259972	1.346934	3.666381
-15.023726	4.412692	3.676378
-14.892298	8.302917	3.686374
-13.651675	5.994249	3.696371
-13.232487	5.734626	3.706368
-13.240652	4.090182	3.716365
-12.843021	-0.530434	3.726362
-12.074015	5.408353	3.736358
-11.278547	1.260251	3.746355
-10.808238	1.114669	3.756352
-10.745483	4.687497	3.766349
-10.004017	0.659745	3.776346
-9.116455	-3.204465	3.786342
-8.491712	-0.814464	3.796339
-8.548284	2.897411	3.806336
-8.465464	0.010375	3.816333
-7.732039	11.373204	3.826330
-7.089638	-3.727376	3.836326
-6.311335	-2.578947	3.846323
-5.478533	4.737670	3.856320
-5.205886	6.296431	3.866317
-5.207630	3.541216	3.876314
-4.929067	11.140174	3.886310
-4.167410	14.543572	3.896307
-3.796574	11.611703	3.906304
-3.308897	25.082057	3.916301
-2.829754	34.568490	3.926298
-2.239206	36.776464	3.936294
-1.787989	60.169563	3.946291
-1.229014	71.277960	3.956288
-1.201684	83.205407	3.966285
-0.583450	108.590773	3.976282
0.000000	113.226214	3.981286
0.028725	129.651709	3.986291
0.345773	142.467206	3.991296
0.545985	148.043601	3.996301
0.445908	154.637834	4.001306
0.681286	153.795187	4.006310
0.533049	159.079829	4.011315
0.311101	159.049324	4.016320
0.836007	160.742436	4.021325
0.783315	168.863440	4.026330
1.027413	179.676860	4.031334
0.973324	171.423937	4.036339
0.666021	155.666069	4.041344
0.753826	161.318957	4.046349
1.019871	165.976351	4.051354
0.904292	164.816413	4.056358
1.049712	160.641231	4.061363
0.808457	155.114532	4.066368
0.940573	149.100728	4.071373
0.552539	158.428163	4.076378
1.391743	171.675339	4.081382
0.735597	174.390071	4.086387
1.114846	173.938497	4.091392
1.194615	164.669299	4.096397
1.079671	163.184777	4.101402
1.237014	157.841806	4.106406
0.819442	152.945455	4.111411
0.712518	151.104940	4.116416
1.046700	159.639599	4.121421
1.137364	179.133474	4.126426
1.333152	173.880433	4.131430
1.220608	181.828228	4.136435
0.855438	170.540945	4.141440
1.158823	178.556248	4.146445
1.383763	178.866742	4.151450
1.092707	169.413168	4.156454
0.982203	164.388722	4.161459
1.174921	183.233450	4.166464
1.386507	182.098864	4.171469
1.219944	176.574711	4.176474
1.498655	178.300025	4.181478
1.009087	161.345877	4.186483
1.000556	164.402470	4.191488
1.195579	173.699068	4.196493
0.844820	176.281547	4.201498
1.172944	167.535817	4.206502
1.283579	178.447848	4.211507
1.460264	175.360113	4.216512
1.560837	175.376445	4.221517
1.365054	188.939304	4.226522
1.609337	175.244126	4.231526
1.430031	168.942205	4.236531
1.046773	173.901945	4.241536
1.357924	178.121255	4.246541
0.825436	185.710282	4.251546
1.157892	169.764298	4.256550
1.058359	185.733848	4.261555
1.191010	180.185897	4.266560
1.213015	170.130777	4.271565
1.108912	176.447967	4.276570
1.177660	175.589546	4.281574
1.396781	190.772934	4.286579
1.481594	205.742841	4.291584
1.993613	207.203188	4.296589
1.484463	188.354097	4.301594
1.520914	184.466543	4.306598
1.285545	178.626616	4.311603
1.439093	194.654981	4.316608
1.629862	199.238698	4.321613
1.496484	217.394870	4.326618
1.908782	206.720976	4.331622
1.680310	206.370422	4.336627
1.667398	193.749973	4.341632
1.727102	177.584853	4.346637
1.031240	179.263649	4.351642
1.648701	192.792451	4.356646
2.029464	200.252172	4.361651
1.953606	202.666696	4.366656
1.587867	181.718677	4.371661
1.579428	178.260003	4.376666
1.544888	178.962225	4.381670
1.626620	194.136356	4.386675
1.806219	212.138000	4.391680
1.926833	196.774638	4.396685
1.837749	216.677105	4.401690
1.943487	201.536496	4.406694
1.695162	195.241431	4.411699
1.642750	192.099999	4.416704
2.048621	187.976380	4.421709
1.519197	195.702531	4.426714
1.822401	201.124399	4.431718
1.393945	212.398623	4.436723
1.299402	212.201151	4.441728
1.916125	208.998465	4.446733
1.744591	204.946386	4.451738
1.628510	213.152571	4.456742
1.390272	216.442474	4.461747
1.460405	204.877531	4.466752
2.198157	225.517072	4.471757
1.683193	222.171888	4.476762
2.151400	228.804539	4.481766
2.049537	218.656007	4.486771
1.650827	223.434125	4.491776
2.046900	223.318260	4.496781
2.342616	236.899679	4.501786
2.269499	238.987005	4.506790
2.279902	215.588798	4.511795
2.071658	201.165514	4.516800
2.039658	203.758462	4.521805
2.008029	209.294958	4.526810
2.268274	216.049084	4.531814
2.114129	221.037274	4.536819
1.996749	220.371997	4.541824
2.355844	209.654704	4.546829
2.003394	222.128369	4.551834
1.922419	223.688192	4.556838
2.170461	216.732471	4.561843
1.822410	219.033832	4.566848
2.412393	223.512911	4.571853
2.146930	225.011471	4.576858
2.092677	220.514402	4.581862
1.999620	235.279621	4.586867
2.315162	248.469956	4.591872
2.588414	240.299245	4.596877
2.390605	232.063923	4.601882
2.487003	206.527345	4.606886
2.268593	213.564591	4.611891
2.041993	206.551659	4.616896
2.125893	200.269467	4.621901
2.395238	224.159200	4.626906
2.378952	230.040637	4.631910
2.413432	228.501424	4.636915
2.244053	227.878875	4.641920
2.418642	231.156498	4.646925
2.293287	236.198439	4.651930
2.550641	234.900803	4.656934
2.614716	235.065232	4.661939
2.343216	238.698536	4.666944
2.414079	232.403391	4.671949
2.428553	239.180482	4.676954
2.450635	236.979555	4.681958
2.565984	240.113263	4.686963
2.429964	227.840078	4.691968
2.506790	226.219382	4.696973
2.431889	237.066320	4.701978
2.661839	240.627807	4.706982
2.882450	231.878990	4.711987
2.548771	227.385673	4.716992
2.474261	210.862180	4.721997
2.294515	222.121158	4.727002
2.422527	237.630318	4.732006
2.795112	249.832159	4.737011
2.496784	252.986581	4.742016
2.672965	241.418982	4.747021
2.737037	242.545709	4.752026
2.634936	233.076754	4.757030
2.778667	245.491527	4.762035
2.200346	241.859260	4.767040
2.598295	242.410102	4.772045
2.545163	241.951942	4.777050
2.653874	237.610058	4.782054
2.826109	234.891331	4.787059
2.352176	236.003080	4.792064
2.828365	238.515604	4.797069
2.862597	248.509782	4.802074
3.105086	234.668048	4.807078
2.792569	245.293115	4.812083
2.754281	241.472653	4.817088
2.858279	236.619027	4.822093
2.780662	243.292654	4.827098
2.599388	237.420383	4.832102
2.410876	248.571913	4.837107
2.562387	252.386495	4.842112
2.932553	243.706385	4.847117
2.447126	238.959831	4.852122
2.465482	236.984655	4.857126
2.573543	258.813029	4.862131
3.040252	263.893579	4.867136
3.021824	261.224114	4.872141
3.147472	266.289008	4.877146
3.281323	262.430721	4.882150
3.031066	256.191790	4.887155
2.268910	244.176264	4.892160
3.087642	250.517972	4.897165
3.108013	271.950543	4.902170
2.749422	272.366349	4.907174
3.061172	278.871564	4.912179
2.925393	278.665910	4.917184
2.846494	280.586578	4.922189
3.052478	279.972734	4.927194
3.431799	266.031801	4.932198
3.022240	279.272041	4.937203
2.926254	270.420039	4.942208
3.123030	287.901972	4.947213
2.842520	285.738218	4.952218
3.028253	267.668323	4.957222
3.050586	271.464302	4.962227
2.785559	274.214157	4.967232
3.158597	271.702963	4.972237
2.738454	281.534488	4.977242
3.093302	275.343143	4.982246
3.231319	280.475353	4.987251
3.115816	290.673563	4.992256
3.776837	290.179664	4.997261
2.882366	280.661377	5.002266
3.198282	288.188486	5.007270
3.188900	289.985002	5.012275
3.468537	287.762124	5.017280
3.651471	288.918442	5.022285
3.251641	285.186128	5.027290
3.195954	290.192600	5.032294
3.495738	281.355396	5.037299
3.138374	283.736343	5.042304
3.611811	283.089054	5.047309
3.344724	284.177476	5.052314
3.421553	299.449008	5.057318
3.409133	283.851430	5.062323
3.108113	290.446370	5.067328
3.444322	286.035998	5.072333
3.189674	301.751511	5.077338
3.430251	298.138400	5.082342
3.565857	300.867239	5.087347
3.613077	299.153560	5.092352
3.738022	291.575594	5.097357
3.349840	294.742505	5.102362
3.509197	298.145685	5.107366
3.744959	291.309657	5.112371
3.479680	295.396952	5.117376
3.637142	287.325658	5.122381
3.657209	292.961375	5.127386
3.633442	291.367555	5.132390
3.673996	298.160489	5.137395
3.544523	303.064026	5.142400
3.886290	295.971136	5.147405
3.554310	299.741025	5.152410
3.487739	293.822055	5.157414
3.646669	298.510114	5.162419
3.839828	300.115901	5.167424
3.899850	286.656874	5.172429
3.770670	302.911532	5.177434
3.645502	291.090917	5.182438
3.667439	289.429364	5.187443
3.608633	300.118500	5.192448
3.991131	286.783666	5.197453
4.001436	288.719191	5.202458
3.896667	294.767601	5.207462
3.730710	286.407612	5.212467
3.463105	279.673320	5.217472
3.722780	289.206144	5.222477
3.623485	293.656986	5.227482
3.638457	293.939336	5.232486
3.940114	296.611531	5.237491
3.526855	305.254992	5.242496
3.809029	301.740372	5.247501
3.901450	297.852222	5.252506
3.537113	297.725971	5.257510
3.955272	298.902611	5.262515
3.522055	301.123051	5.267520
3.722043	296.524455	5.272525
4.047224	295.435315	5.277530
3.739946	296.844799	5.282534
3.820863	292.851805	5.287539
3.698395	296.706347	5.292544
4.052523	313.606276	5.297549
4.140181	326.816382	5.302554
4.322630	317.869504	5.307558
4.239416	297.953748	5.312563
3.873583	300.731021	5.317568
4.283119	292.339461	5.322573
4.213249	299.068363	5.327578
3.755092	294.762130	5.332582
3.988363	285.643693	5.337587
3.948173	299.686948	5.342592
4.236025	312.438352	5.347597
4.156720	313.697202	5.352602
4.112222	311.952112	5.357606
3.929741	314.602009	5.362611
4.150936	322.822464	5.367616
4.536892	310.628599	5.372621
4.468806	315.610688	5.377626
3.845805	301.242729	5.382630
3.727827	310.088872	5.387635
3.922424	319.398258	5.392640
4.334014	311.082511	5.397645
4.311657	319.148068	5.402650
4.021048	325.586708	5.407654
4.291666	316.628713	5.412659
4.327435	327.483571	5.417664
4.290088	331.163737	5.422669
4.292354	323.919068	5.427674
3.905931	323.143455	5.432678
4.049063	329.134436	5.437683
4.221835	333.574365	5.442688
4.064600	326.343623	5.447693
4.167519	332.053961	5.452698
4.144979	332.108101	5.457702
4.458964	339.057029	5.462707
4.353851	356.147437	5.467712
4.537504	340.912917	5.472717
4.558803	342.449241	5.477722
4.781107	349.629285	5.482726
4.637171	345.840363	5.487731
4.146429	332.880654	5.492736
4.594941	339.717277	5.497741
4.447435	354.090369	5.502746
4.735345	349.538099	5.507750
5.060705	340.529904	5.512755
4.499724	330.379625	5.517760
4.393598	327.325375	5.522765
4.403218	340.500639	5.527770
4.218115	349.033808	5.532774
4.469066	351.384976	5.537779
4.554122	351.004311	5.542784
4.794001	351.959334	5.547789
4.513912	352.658930	5.552794
4.694466	357.104092	5.557798
4.900673	355.519815	5.562803
4.277909	357.366696	5.567808
4.290154	351.580790	5.572813
4.832183	352.535309	5.577818
4.551149	357.217266	5.582822
4.635953	349.568164	5.587827
4.796102	358.789048	5.592832
4.990138	339.619739	5.597837
4.562494	357.620485	5.602842
4.416855	355.136191	5.607846
5.007921	354.162834	5.612851
4.725721	357.424022	5.617856
4.786408	352.840044	5.622861
4.929185	360.008669	5.627866
4.877852	355.866738	5.632870
4.999331	349.078773	5.637875
4.766665	351.887027	5.642880
4.777109	352.337647	5.647885
4.712895	355.917287	5.652890
4.520271	360.860678	5.657894
5.010827	354.366689	5.662899
4.646283	350.087392	5.667904
4.740723	364.500029	5.672909
4.928279	360.888168	5.677914
4.668022	382.548206	5.682918
5.273183	384.767245	5.687923
4.762251	386.455950	5.692928
5.178519	372.968264	5.697933
5.136995	386.163561	5.702938
5.074584	399.125543	5.707942
5.103592	386.751065	5.712947
4.892621	389.207381	5.717952
5.016584	379.292437	5.722957
4.754370	383.832875	5.727962
4.839408	384.754492	5.732966
4.899326	393.132850	5.737971
4.887362	395.971728	5.742976
5.070229	397.551010	5.747981
4.963971	393.421499	5.752986
5.144891	390.618142	5.757990
5.172879	378.194313	5.762995
5.163702	385.417560	5.768000
5.112724	390.940844	5.773005
4.945954	389.867288	5.778010
4.851020	389.940002	5.783014
5.167862	375.665770	5.788019
5.012291	383.766398	5.793024
4.920292	397.883319	5.798029
5.174748	407.995114	5.803034
5.533063	418.875069	5.808038
5.591464	412.973482	5.813043
5.176837	423.365054	5.818048
5.690161	415.213180	5.823053
5.222187	408.878161	5.828058
5.281081	403.823769	5.833062
5.459795	397.031257	5.838067
5.396853	395.175848	5.843072
5.599475	400.617862	5.848077
5.353562	395.122922	5.853082
5.406962	388.511047	5.858086
5.588933	386.665679	5.863091
5.149723	383.613975	5.868096
5.472837	396.181052	5.873101
5.581190	403.860711	5.878106
5.401844	389.322866	5.883110
5.882016	390.277448	5.888115
5.398519	386.419434	5.893120
5.285999	384.126386	5.898125
5.343016	394.667896	5.903130
5.485346	409.527275	5.908134
5.614866	406.497209	5.913139
5.530460	411.977978	5.918144
5.990126	399.368352	5.923149
5.464959	393.929624	5.928154
5.251860	394.826615	5.933158
5.890781	403.282737	5.938163
5.454129	414.525511	5.943168
5.682719	417.604531	5.948173
6.081603	425.358821	5.953178
5.301937	403.826379	5.958182
5.473043	393.896038	5.963187
5.709127	406.342048	5.968192
5.776269	405.368352	5.973197
5.700692	415.325142	5.978202
5.349200	409.758853	5.983206
5.640766	412.740154	5.988211
5.407574	423.040970	5.993216
5.616612	421.949210	5.998221
5.656559	421.693006	6.003226
5.517183	419.918989	6.008230
5.798695	419.326695	6.013235
5.526102	425.882762	6.018240
5.913213	430.432918	6.023245
5.788279	420.805821	6.028250
5.595846	418.126804	6.033254
5.788278	415.415166	6.038259
5.978099	416.981067	6.043264
5.705280	416.546085	6.048269
5.606573	421.377981	6.053274
5.609955	424.557854	6.058278
5.850565	419.624767	6.063283
5.268003	425.272019	6.068288
5.429001	415.672654	6.073293
5.765271	418.827703	6.078298
5.518822	423.391396	6.083302
5.804729	412.631499	6.088307
5.737112	423.598320	6.093312
5.998222	419.805882	6.098317
6.169015	423.739557	6.103322
6.080592	420.641025	6.108326
5.690506	414.889223	6.113331
5.735600	416.397155	6.118336
5.808463	419.508323	6.123341
5.656613	418.463377	6.128346
5.610929	413.733384	6.133350
5.617562	415.174369	6.138355
5.538555	417.256575	6.143360
5.590869	423.129117	6.148365
5.547791	418.594035	6.153370
5.655942	422.117977	6.158374
5.924430	410.971163	6.163379
5.998732	420.191078	6.168384
5.934803	404.846757	6.173389
5.955435	416.321480	6.178394
5.476941	412.534160	6.183398
5.607583	410.353547	6.188403
5.903873	422.757360	6.193408
5.695810	410.285597	6.198413
5.979047	414.729592	6.203418
5.731411	418.222155	6.208422
5.676974	405.711788	6.213427
5.850852	409.434315	6.218432
5.858816	416.192040	6.223437
5.891766	411.233585	6.228442
5.527764	415.374912	6.233446
5.980496	413.273767	6.238451
5.695012	414.811960	6.243456
5.782022	403.501674	6.248461
5.409799	400.652096	6.253466
5.664210	396.488141	6.258470
5.922129	415.064390	6.263475
5.734726	416.240283	6.268480
5.771818	413.295536	6.273485
6.109116	406.924227	6.278490
5.759515	402.953908	6.283494
5.734166	391.324000	6.288499
5.456965	394.659843	6.293504
5.703955	381.653849	6.298509
5.489345	390.261077	6.303514
5.395444	394.186987	6.308518
5.386803	402.511961	6.313523
5.570327	419.674710	6.318528
5.666628	409.271423	6.323533
5.594877	415.662192	6.328538
5.882226	419.296516	6.333542
6.063545	418.120940	6.338547
5.824730	417.174816	6.343552
5.794316	413.217060	6.348557
5.848775	415.521684	6.353562
6.001299	414.298183	6.358566
5.600719	401.172471	6.363571
5.419309	399.007813	6.368576
5.733928	415.521628	6.373581
6.097703	414.303470	6.378586
5.850928	412.982874	6.383590
5.735941	402.631280	6.388595
5.694476	396.927239	6.393600
5.555209	378.093051	6.398605
5.457468	393.575943	6.403610
5.517595	397.175001	6.408614
6.032893	409.944938	6.413619
5.563369	416.477901	6.418624
5.741855	418.638510	6.423629
5.634982	410.975867	6.428634
5.761114	414.672743	6.433638
6.223813	412.771903	6.438643
5.405038	405.544783	6.443648
5.431644	402.865385	6.448653
5.752062	405.810148	6.453658
5.766519	413.568667	6.458662
6.112095	406.769393	6.463667
5.451106	398.621278	6.468672
5.510255	397.644266	6.473677
6.145844	413.063706	6.478682
5.696583	411.847803	6.483686
5.523405	396.254479	6.488691
5.999035	398.352267	6.493696
5.894128	395.680692	6.498701
5.848313	384.453735	6.503706
5.743332	389.228351	6.508710
5.759473	381.682627	6.513715
5.248219	397.566037	6.518720
5.571397	384.531270	6.523725
5.895388	397.683834	6.528730
5.608762	401.590491	6.533734
5.768296	396.760292	6.538739
5.935730	398.132872	6.543744
5.887462	391.578345	6.548749
5.593704	385.250260	6.553754
5.354597	391.440974	6.558758
5.616286	387.726683	6.563763
5.720032	409.401289	6.568768
5.849206	412.633082	6.573773
5.685845	412.769788	6.578778
5.763418	413.845362	6.583782
5.903685	409.195828	6.588787
5.525752	401.608174	6.593792
5.903718	402.798568	6.598797
5.529763	394.921883	6.603802
5.824694	401.413750	6.608806
5.719196	409.522396	6.613811
5.324898	404.732909	6.618816
5.531325	406.002756	6.623821
5.756858	411.161490	6.628826
5.568295	429.081078	6.633830
5.831745	415.685104	6.638835
5.988778	423.888690	6.643840
5.585021	411.432493	6.648845
5.825166	417.406885	6.653850
5.622156	424.695923	6.658854
6.080962	417.216531	6.663859
5.779971	418.977886	6.668864
5.653477	399.599042	6.673869
5.500103	405.327590	6.678874
5.626228	420.511873	6.683878
5.764282	411.564089	6.688883
5.971579	415.660631	6.693888
5.521087	410.572321	6.698893
5.998633	417.419374	6.703898
5.433688	412.632040	6.708902
5.707860	409.452280	6.713907
5.811733	423.601181	6.718912
5.509681	423.464043	6.723917
5.731978	426.511844	6.728922
5.526789	410.960101	6.733926
5.854644	413.795114	6.738931
5.704919	424.195199	6.743936
5.737986	415.553040	6.748941
6.086386	419.141067	6.753946
5.657329	435.771979	6.758950
5.789403	409.105160	6.763955
5.418022	414.543576	6.768960
5.742768	421.132734	6.773965
5.877517	419.105939	6.778970
5.787635	424.912202	6.783974
5.827597	407.735506	6.788979
5.698381	402.365813	6.793984
5.725858	389.121228	6.798989
5.578675	399.815665	6.803994
5.563706	424.742231	6.808998
5.892932	422.311161	6.814003
5.810964	430.792703	6.819008
5.549707	414.753184	6.824013
5.469117	404.568456	6.829018
5.427228	417.361515	6.834022
5.589025	420.578547	6.839027
5.590850	432.812009	6.844032
5.842837	418.930458	6.849037
5.639917	412.374250	6.854042
5.620661	415.103938	6.859046
5.946008	424.607643	6.864051
6.062472	437.213935	6.869056
6.061561	427.451501	6.874061
6.183623	432.532334	6.879066
5.775838	399.397949	6.884070
5.735407	401.373147	6.889075
5.291480	406.104828	6.894080
5.308659	399.219437	6.899085
5.595483	409.067401	6.904090
5.859752	423.124287	6.909094
5.948308	419.035878	6.914099
5.705475	427.683603	6.919104
5.846830	427.761961	6.924109
5.785406	417.868650	6.929114
5.261912	418.183554	6.934118
5.677473	417.565260	6.939123
5.264291	430.548929	6.944128
5.787648	425.368741	6.949133
5.841641	429.652914	6.954138
5.605001	426.367254	6.959142
5.708093	427.672332	6.964147
5.644443	431.353712	6.969152
5.860828	434.751642	6.974157
5.518066	427.433417	6.979162
5.532731	425.313405	6.984166
5.760249	416.944062	6.989171
6.015920	415.654187	6.994176
5.732925	422.985053	6.999181
5.677290	423.768022	7.004186
5.702991	422.141941	7.009190
5.655444	419.596044	7.014195
5.365012	423.213774	7.019200
5.399073	420.716151	7.024205
5.551724	430.458441	7.029210
5.185124	435.667977	7.034214
5.385648	420.377709	7.039219
5.313650	430.969768	7.044224
6.129295	437.867508	7.049229
5.766879	427.808856	7.054234
5.788185	438.579561	7.059238
5.779017	419.649139	7.064243
5.777287	425.152556	7.069248
5.593120	429.396666	7.074253
5.539841	418.321272	7.079258
5.501842	420.118882	7.084262
6.152206	427.498151	7.089267
5.687757	430.166054	7.094272
5.965169	426.539821	7.099277
5.870302	420.452728	7.104282
5.901732	422.261655	7.109286
5.818239	416.475464	7.114291
5.579086	428.792649	7.119296
5.867121	429.155468	7.124301
5.847062	422.262704	7.129306
5.613629	426.550373	7.134310
5.723457	431.677723	7.139315
5.644381	432.907243	7.144320
5.945473	426.557891	7.149325
5.800825	418.745805	7.154330
5.804135	424.903575	7.159334
5.497339	429.403150	7.164339
5.505263	431.757396	7.169344
5.444256	433.666741	7.174349
5.676895	424.232524	7.179354
5.315230	419.095199	7.184358
6.077917	422.386865	7.189363
5.570133	426.952902	7.194368
5.523073	424.943720	7.199373
5.853894	417.547238	7.204378
5.705158	429.637368	7.209382
5.942082	414.986805	7.214387
5.843452	433.092403	7.219392
5.718864	428.042278	7.224397
5.797098	424.290615	7.229402
5.594381	427.628560	7.234406
5.945536	421.939640	7.239411
5.659890	428.187585	7.244416
5.636062	441.033223	7.249421
5.769210	425.172201	7.254426
5.626782	438.224984	7.259430
6.123372	423.231089	7.264435
5.801273	426.686829	7.269440
5.678648	418.025804	7.274445
6.112710	423.808130	7.279450
5.997126	417.547765	7.284454
5.894781	417.690172	7.289459
5.806619	432.368643	7.294464
5.470504	425.181522	7.299469
5.660220	426.585051	7.304474
5.316307	429.620661	7.309478
5.402924	416.992559	7.314483
5.450841	416.454948	7.319488
5.502907	426.848425	7.324493
5.589886	429.612651	7.329498
5.516643	424.873594	7.334502
5.342581	424.647823	7.339507
5.582887	438.347300	7.344512
5.620531	451.144311	7.349517
5.885238	458.478211	7.354522
6.042602	466.819493	7.359526
5.988828	443.740442	7.364531
5.787034	442.811976	7.369536
5.642849	425.370507	7.374541
5.510462	430.543507	7.379546
5.794866	431.624760	7.384550
5.853437	427.699157	7.389555
5.694077	438.352027	7.394560
5.533216	421.948140	7.399565
5.484035	433.675137	7.404570
5.446043	449.489370	7.409574
5.745108	451.630353	7.414579
5.876772	464.479024	7.419584
5.828860	455.792608	7.424589
5.988238	443.865856	7.429594
5.714557	455.257733	7.434598
5.871365	436.385695	7.439603
5.310908	439.783550	7.444608
5.723652	441.520092	7.449613
5.897192	440.335244	7.454618
5.613118	448.026697	7.459622
5.937711	438.270252	7.464627
5.809272	437.778556	7.469632
5.441421	429.262529	7.474637
5.758897	431.562167	7.479642
5.528111	446.187267	7.484646
5.993349	444.902714	7.489651
5.652452	445.597860	7.494656
5.669845	440.300117	7.499661
5.789020	441.147529	7.504666
5.345616	447.955884	7.509670
5.693685	452.042985	7.514675
5.718840	464.953753	7.519680
6.232836	459.293452	7.524685
6.041244	444.499687	7.529690
5.588424	441.664013	7.534694
5.621152	429.390799	7.539699
5.416960	434.006805	7.544704
5.703043	429.995854	7.549709
6.153524	423.970965	7.554714
5.749167	431.870231	7.559718
6.014262	432.560636	7.564723
5.297183	438.622385	7.569728
5.670585	427.917375	7.574733
5.852919	423.929983	7.579738
5.657169	433.289836	7.584742
5.792045	427.245279	7.589747
5.752976	426.837867	7.594752
5.783596	430.829337	7.599757
5.603737	431.734058	7.604762
5.483446	435.794568	7.609766
5.686862	433.977221	7.614771
5.787995	428.048341	7.619776
5.491677	437.394725	7.624781
5.817590	430.100074	7.629786
5.398915	442.478507	7.634790
5.936943	437.707098	7.639795
5.579541	443.005585	7.644800
5.851906	445.751708	7.649805
5.869052	437.958652	7.654810
5.614961	448.681051	7.659814
5.696937	432.564666	7.664819
5.715840	437.093786	7.669824
5.689083	437.478732	7.674829
6.025429	426.812009	7.679834
5.983733	435.485892	7.684838
6.154843	424.594110	7.689843
5.431914	438.242821	7.694848
5.452193	440.687469	7.699853
5.828443	437.782763	7.704858
5.465465	436.547371	7.709862
5.686202	431.439586	7.714867
5.596353	430.819967	7.719872
5.775246	442.566404	7.724877
5.800169	429.685070	7.729882
5.926723	438.162445	7.734886
5.995830	432.299235	7.739891
5.725354	439.791122	7.744896
5.721451	442.530708	7.749901
5.764370	431.394716	7.754906
5.802789	439.830125	7.759910
5.864182	431.307980	7.764915
5.574628	438.375929	7.769920
5.931463	431.095800	7.774925
5.911050	428.564360	7.779930
5.732754	432.201939	7.784934
5.905747	423.556186	7.789939
5.825232	435.255510	7.794944
5.662744	432.794904	7.799949
5.828715	431.282579	7.804954
5.942736	432.607556	7.809958
5.954264	435.239028	7.814963
5.687763	430.970638	7.819968
5.896195	447.057482	7.824973
5.852542	435.422772	7.829978
5.829406	438.612160	7.834982
5.831972	427.087221	7.839987
5.774193	416.134118	7.844992
5.585352	407.373841	7.849997
5.727313	403.027402	7.855002
5.491079	404.865366	7.860006
5.865985	426.632518	7.865011
5.981708	422.827107	7.870016
5.798608	411.427080	7.875021
5.871749	395.944984	7.880026
5.378286	406.549947	7.885030
5.468881	402.560652	7.890035
5.436585	412.931853	7.895040
5.625045	430.904666	7.900045
5.725440	425.137511	7.905050
5.737377	431.614299	7.910054
5.598926	429.077898	7.915059
5.868817	429.194999	7.920064
5.713667	436.657072	7.925069
5.849779	436.390698	7.930074
5.718920	444.030291	7.935078
5.880478	435.495735	7.940083
5.542272	449.966234	7.945088
5.589191	435.958829	7.950093
5.890558	432.699689	7.955098
5.693431	432.031698	7.960102
5.937475	424.447205	7.965107
5.760980	423.122789	7.970112
5.579021	436.136523	7.975117
5.737880	430.735394	7.980122
5.614762	437.194598	7.985139
5.925585	429.899853	7.990157
5.749536	429.541129	7.995174
5.616485	422.543909	8.000192
5.824216	425.808745	8.005210
5.582540	432.983620	8.010227
5.846752	429.850991	8.015245
5.630143	432.435606	8.020262
5.878803	436.330072	8.025280
6.143120	434.311580	8.030298
5.604980	429.265876	8.035315
5.513497	409.211079	8.040333
5.708348	424.040457	8.045350
5.762072	428.513781	8.050368
5.829408	422.538262	8.055386
5.721745	440.990379	8.060403
6.251406	443.649664	8.065421
5.597788	431.359288	8.070438
5.498996	438.915397	8.075456
6.139680	428.220037	8.080474
5.753756	433.582886	8.085491
5.913055	437.725835	8.090509
5.766575	428.498192	8.095526
5.821666	427.401702	8.100544
5.719205	420.802401	8.105562
5.393251	432.289778	8.110579
5.786814	439.230867	8.115597
5.984647	437.775714	8.120614
5.680270	438.830546	8.125632
5.629466	436.322697	8.130650
5.492099	429.824417	8.135667
5.643898	434.836153	8.140685
6.012341	439.771547	8.145702
5.562882	437.733633	8.150720
5.945978	433.185170	8.155738
5.545514	437.684154	8.160755
5.764823	440.577072	8.165773
5.739426	435.825103	8.170790
5.688260	442.133229	8.175808
6.082557	449.233816	8.180826
5.723821	468.416596	8.185843
6.218493	462.079553	8.190861
6.204258	445.184958	8.195878
5.810234	449.464715	8.200896
6.182405	441.437623	8.205914
6.058140	435.118932	8.210931
6.122152	429.410738	8.215949
5.899556	432.797269	8.220966
5.681155	447.954458	8.225984
6.006600	440.128949	8.231002
5.828857	438.838500	8.236019
5.914605	433.585876	8.241037
5.991359	434.962983	8.246054
5.934438	440.770090	8.251072
6.249018	424.285657	8.256090
5.615084	436.548398	8.261107
5.873866	444.186534	8.266125
6.376394	454.248289	8.271142
6.040775	449.851657	8.276160
5.972423	448.173811	8.281178
6.043330	443.783017	8.286195
5.899849	439.551547	8.291213
6.221846	444.582789	8.296230
5.823710	441.100844	8.301248
6.025731	449.837423	8.306266
5.951199	464.199841	8.311283
6.226234	464.386237	8.316301
6.386231	471.605656	8.321318
5.930680	456.855039	8.326336
5.815337	442.743652	8.331354
5.723010	451.316416	8.336371
5.588031	459.960689	8.341389
5.838456	454.821172	8.346406
5.932755	456.646280	8.351424
6.082260	456.867099	8.356442
6.184244	474.077067	8.361459
5.917712	479.799755	8.366477
6.114513	466.553911	8.371494
5.808577	470.924215	8.376512
6.137768	464.736541	8.381530
5.751595	473.021130	8.386547
6.026865	478.891737	8.391565
6.099723	466.139612	8.396582
6.131281	468.264011	8.401600
6.292237	466.716937	8.406618
5.921739	463.016681	8.411635
6.044141	472.822331	8.416653
6.540696	479.852009	8.421670
5.832941	479.943679	8.426688
6.298766	482.336999	8.431706
6.232263	479.446476	8.436723
6.132873	472.645305	8.441741
6.422784	479.546170	8.446758
6.161617	471.415497	8.451776
6.264701	459.293891	8.456794
6.224002	470.094122	8.461811
5.925353	464.376667	8.466829
6.228849	481.858993	8.471846
6.375826	495.450919	8.476864
6.387784	494.201445	8.481882
5.918543	476.660687	8.486899
6.242748	482.798452	8.491917
6.364760	496.692775	8.496934
6.387695	496.300674	8.501952
6.315153	482.210519	8.506970
6.261268	482.779850	8.511987
6.175560	480.051132	8.517005
6.550905	474.211960	8.522022
6.014104	490.348600	8.527040
6.405076	487.224435	8.532058
6.401007	486.726581	8.537075
5.895689	476.786702	8.542093
6.252332	480.202400	8.547110
6.308017	502.056176	8.552128
6.344100	494.780036	8.557146
6.638785	504.307480	8.562163
6.655173	500.478626	8.567181
6.559713	469.597327	8.572199
6.255090	478.335970	8.577216
6.113916	466.475253	8.582234
6.155454	484.005496	8.587251
6.477959	489.857281	8.592269
6.842697	483.555281	8.597287
6.058836	470.488713	8.602304
6.227662	474.826025	8.607322
6.084760	481.163399	8.612339
6.236817	494.372963	8.617357
6.682522	493.861007	8.622375
6.418630	500.352707	8.627392
6.624005	504.644232	8.632410
6.611447	496.337644	8.637427
6.302400	481.889601	8.642445
6.366164	485.777733	8.647463
6.289500	500.509068	8.652480
6.430378	503.944486	8.657498
6.708835	504.669782	8.662515
6.269571	495.767989	8.667533
6.320713	496.839256	8.672551
6.523213	498.810040	8.677568
6.635377	507.591024	8.682586
6.261945	501.975168	8.687603
6.420855	500.348522	8.692621
6.480304	501.872366	8.697639
6.417757	504.117616	8.702656
6.274599	516.885132	8.707674
6.649099	499.606810	8.712691
6.368132	507.483751	8.717709
6.501357	506.614160	8.722727
6.260983	497.824353	8.727744
6.382447	496.649973	8.732762
6.603505	508.978429	8.737779
6.437722	508.008968	8.742797
6.523554	492.452943	8.747815
6.966470	502.529009	8.752832
6.370035	502.489116	8.757850
6.817166	496.956910	8.762867
6.520027	501.987848	8.767885
6.705813	496.211680	8.772903
6.652156	506.928465	8.777920
6.337120	503.462589	8.782938
6.244871	500.149725	8.787955
6.275363	503.572090	8.792973
6.498013	491.229164	8.797991
6.388669	501.098814	8.803008
6.517340	503.631400	8.808026
6.910888	494.063046	8.813043
6.589273	498.019591	8.818061
6.540894	487.384330	8.823079
6.478445	501.248128	8.828096
6.376276	499.928455	8.833114
6.706915	491.230770	8.838131
6.462301	500.948397	8.843149
6.849381	495.137390	8.848167
6.710131	497.531509	8.853184
6.561863	499.598343	8.858202
6.926978	501.628360	8.863219
6.504836	506.850299	8.868237
6.579839	501.341700	8.873255
6.713916	496.320392	8.878272
6.600533	500.862094	8.883290
6.762155	495.762922	8.888307
6.458151	506.108852	8.893325
6.549265	507.671747	8.898343
6.756031	525.437281	8.903360
6.892885	534.015911	8.908378
6.772719	523.712409	8.913395
6.805647	520.582359	8.918413
6.918269	506.410411	8.923431
6.527726	509.864666	8.928448
6.420301	513.329605	8.933466
6.828586	520.544821	8.938483
6.499780	534.443316	8.943501
7.085918	531.034280	8.948519
6.709304	538.822929	8.953536
6.798251	533.175131	8.958554
7.069101	533.980313	8.963571
6.637665	535.794100	8.968589
6.974662	526.368118	8.973607
7.051806	523.658338	8.978624
7.165639	521.326282	8.983642
7.138808	505.072657	8.988659
6.774209	508.966734	8.993677
7.077078	494.965288	8.998695
7.005116	497.166137	9.003712
6.808549	500.226592	9.008730
7.014670	496.075004	9.013747
6.713962	513.191947	9.018765
6.699945	503.915405	9.023783
6.551020	499.663759	9.028800
6.595931	502.861539	9.033818
6.526549	501.154631	9.038835
6.577342	515.475031	9.043853
6.636452	526.097322	9.048871
6.988066	538.089227	9.053888
6.767494	534.592186	9.058906
6.998047	536.351783	9.063923
6.848738	537.768521	9.068941
7.033014	525.375325	9.073959
7.145582	532.591983	9.078976
6.869738	538.429105	9.083994
7.049632	522.182434	9.089011
6.977706	537.365693	9.094029
6.856896	518.181384	9.099047
7.147280	530.728181	9.104064
6.908596	531.459525	9.109082
6.980839	528.543210	9.114099
6.964797	528.696524	9.119117
7.160241	520.688066	9.124135
7.192332	535.677986	9.129152
7.202302	527.264332	9.134170
7.189478	525.722156	9.139187
6.900008	522.312670	9.144205
7.003164	522.802222	9.149223
6.941901	524.056701	9.154240
6.864654	521.227678	9.159258
7.340297	521.785572	9.164275
7.081320	525.597841	9.169293
7.197427	525.545197	9.174311
7.003489	518.580333	9.179328
6.745611	523.589931	9.184346
7.282312	515.905522	9.189363
7.100604	519.983511	9.194381
7.056539	532.704158	9.199399
7.069780	522.832266	9.204416
6.861150	523.819519	9.209434
7.197964	529.934948	9.214451
7.223690	531.355431	9.219469
7.145824	528.828520	9.224487
7.239475	521.141945	9.229504
7.128635	528.507901	9.234522
7.275498	528.282489	9.239539
6.945212	525.977180	9.244557
6.764514	533.932921	9.249575
6.929566	521.729385	9.254592
6.430990	535.596105	9.259610
6.885846	520.585451	9.264627
7.078576	540.539035	9.269645
6.951392	528.784894	9.274663
7.042503	532.895936	9.279680
6.857679	537.244571	9.284698
7.309176	546.403770	9.289715
7.192503	559.109672	9.294733
7.327044	554.976490	9.299751
7.320955	549.906196	9.304768
7.591682	550.262762	9.309786
7.206955	530.593409	9.314803
6.904746	533.764422	9.319821
6.879203	551.175930	9.324839
7.177351	553.230208	9.329856
7.133676	557.728129	9.334874
7.533667	552.073894	9.339891
7.240608	561.097136	9.344909
7.273791	562.031834	9.349927
7.397442	564.222607	9.354944
7.079501	569.925188	9.359962
7.304449	570.954945	9.364979
7.131575	561.966579	9.369997
7.381629	557.074976	9.375015
7.591841	563.579579	9.380032
7.395270	564.737841	9.385050
7.465129	562.254708	9.390067
7.655496	567.663780	9.395085
7.677779	558.718840	9.400103
7.410194	534.551132	9.405120
7.450679	530.146940	9.410138
7.170063	526.041632	9.415155
7.120765	535.560007	9.420173
7.575297	551.252921	9.425191
7.329443	537.724524	9.430208
7.187764	546.342399	9.435226
7.462322	550.433956	9.440243
7.375232	550.752131	9.445261
7.231567	563.333584	9.450279
7.260353	560.117317	9.455296
7.325789	568.470017	9.460314
7.277993	561.720407	9.465331
7.478642	559.818502	9.470349
7.576826	553.214721	9.475367
7.878797	544.391945	9.480384
7.646232	553.976241	9.485402
7.660557	554.545423	9.490419
7.563395	553.269791	9.495437
7.311377	548.445908	9.500455
7.445610	542.553166	9.505472
7.448109	543.869340	9.510490
7.463047	554.321228	9.515507
7.803815	556.674607	9.520525
7.272107	555.867071	9.525543
7.394988	552.545312	9.530560
6.939796	561.096325	9.535578
7.254533	552.964023	9.540595
7.284163	558.645081	9.545613
7.171702	567.831360	9.550631
7.389965	567.543174	9.555648
7.051142	564.816611	9.560666
7.532876	576.817352	9.565683
7.784591	585.628262	9.570701
7.447407	574.376814	9.575719
7.909529	576.344658	9.580736
7.380410	565.888375	9.585754
7.438000	562.278640	9.590771
7.623791	578.437371	9.595789
7.611422	590.196607	9.600807
8.020736	586.318249	9.605824
7.638980	583.449986	9.610842
7.703530	574.701067	9.615859
7.742187	561.935522	9.620877
7.650275	554.613884	9.625895
7.585201	552.739065	9.630912
7.644398	566.091964	9.635930
7.598581	561.115224	9.640947
7.989827	556.627965	9.645965
7.867564	564.128183	9.650983
7.851715	551.585886	9.656000
7.529203	567.392661	9.661018
7.711199	557.502110	9.666035
7.740776	560.720642	9.671053
7.600104	562.406082	9.676071
7.476965	564.238303	9.681088
7.383043	571.091538	9.686106
7.813856	588.061698	9.691123
8.021187	588.755748	9.696141
7.608636	594.388850	9.701159
7.780517	590.283636	9.706176
7.957069	592.456518	9.711194
7.976642	586.982734	9.716211
8.310097	574.660005	9.721229
7.584176	567.922081	9.726247
8.073576	567.674604	9.731264
7.358513	561.022273	9.736282
7.366212	567.497265	9.741299
7.506393	574.851282	9.746317
7.867187	584.703715	9.751335
8.209762	589.090187	9.756352
7.702909	587.826360	9.761370
8.202303	588.973432	9.766387
8.155919	571.180536	9.771405
7.515463	573.597170	9.776423
7.778231	565.979851	9.781440
7.964075	578.560889	9.786458
7.810512	580.379343	9.791475
8.212983	585.280130	9.796493
7.910868	586.081297	9.801511
8.154763	564.129285	9.806528
7.682695	562.630720	9.811546
7.963898	562.697911	9.816563
8.014986	561.625002	9.821581
7.618544	569.561995	9.826599
7.984131	575.014639	9.831616
8.276412	582.782126	9.836634
8.113183	572.852274	9.841651
7.982877	565.191074	9.846669
7.832011	565.469110	9.851687
7.897557	549.167502	9.856704
7.655897	565.218150	9.861722
7.891148	570.673831	9.866739
7.882551	584.985610	9.871757
8.000600	596.300935	9.876775
8.204013	588.304509	9.881792
8.345379	588.459267	9.886810
8.236922	583.308554	9.891827
7.839010	571.212576	9.896845
7.820334	588.075159	9.901863
8.090706	574.342250	9.906880
8.294789	587.591516	9.911898
8.127483	586.700535	9.916915
8.226509	581.046822	9.921933
7.789611	571.415299	9.926951
7.982238	578.171489	9.931968
8.222162	585.768528	9.936986
8.099879	583.122888	9.942003
8.279803	584.640215	9.947021
8.028962	586.935192	9.952039
7.938680	589.862473	9.957056
8.302264	587.857767	9.962074
8.058263	584.875614	9.967091
8.188887	585.407078	9.972109
7.994496	593.118602	9.977127
8.091237	592.198747	9.982144
8.537053	594.388834	9.987162
8.161741	596.067491	9.992179
8.533813	583.745754	9.997197
8.075864	585.338674	10.002215
8.285699	593.688584	10.007232
8.269172	591.076934	10.012250
8.066078	590.670027	10.017267
8.256178	585.354741	10.022285
7.995753	585.633562	10.027303
8.199940	586.641165	10.032320
8.311320	592.160229	10.037338
8.094541	597.223481	10.042355
8.281158	585.737853	10.047373
8.329644	589.243764	10.052391
8.544809	587.610667	10.057408
8.726347	585.091952	10.062426
8.455041	578.325639	10.067443
8.061483	563.447275	10.072461
7.976778	580.502519	10.077479
8.159005	583.935747	10.082496
8.295286	582.573218	10.087514
8.200158	594.752063	10.092531
8.300552	590.841305	10.097549
8.053038	594.137223	10.102567
7.925935	587.983475	10.107584
8.312953	583.543651	10.112602
8.227595	585.688961	10.117619
8.490406	582.459011	10.122637
8.068560	597.403064	10.127655
8.380462	586.253655	10.132672
8.487969	579.516948	10.137690
7.604959	589.146660	10.142707
8.535367	605.673912	10.147725
8.565583	618.418372	10.152743
8.646619	615.536803	10.157760
8.541515	597.992906	10.162778
8.212032	588.424807	10.167795
8.608646	575.489094	10.172813
8.295423	582.624986	10.177831
8.203396	590.423018	10.182848
8.676021	607.327442	10.187866
8.370722	612.633238	10.192883
8.989409	604.118850	10.197901
8.585748	602.637416	10.202919
8.236022	581.766270	10.207936
8.516180	580.872886	10.212954
8.465226	590.993231	10.217971
8.504343	588.979754	10.222989
8.588438	615.169736	10.228007
8.793748	613.522323	10.233024
8.454474	595.894412	10.238042
8.101657	596.241346	10.243059
8.648111	604.950618	10.248077
8.411527	611.400162	10.253095
8.670273	606.062995	10.258112
8.858607	621.232358	10.263130
8.478665	615.613009	10.268147
8.680392	616.532355	10.273165
8.642545	613.153105	10.278183
8.617490	608.517048	10.283200
8.546170	614.513770	10.288218
8.453153	601.869933	10.293235
8.709857	598.353739	10.298253
8.339569	614.996162	10.303271
8.183549	617.040280	10.308288
8.491281	618.888000	10.313306
8.455736	618.380682	10.318323
9.073295	619.208283	10.323341
8.504824	613.039585	10.328359
8.268444	607.414031	10.333376
8.486013	611.996332	10.338394
8.617087	624.247445	10.343411
8.889745	625.814499	10.348429
8.736901	623.045284	10.353447
8.708500	624.432799	10.358464
8.964731	623.542974	10.363482
8.919626	621.620464	10.368499
8.899986	614.186577	10.373517
8.976373	616.122321	10.378535
8.766956	620.205703	10.383552
8.551651	618.900583	10.388570
8.722816	621.287313	10.393587
9.039308	611.454802	10.398605
8.749176	612.859392	10.403623
8.875206	612.400752	10.408640
8.940286	620.975251	10.413658
8.860242	621.747004	10.418675
8.953315	619.707484	10.423693
8.579893	617.565560	10.428711
8.720148	615.270159	10.433728
8.894041	608.118015	10.438746
8.648659	626.307338	10.443763
8.953077	643.035895	10.448781
8.920898	639.971787	10.453799
9.109446	641.780161	10.458816
9.031850	625.803844	10.463834
8.780517	622.800656	10.468851
9.063178	613.982310	10.473869
8.872976	617.254100	10.478887
8.761851	619.325439	10.483904
9.529192	622.808609	10.488922
8.967628	621.754572	10.493939
9.210791	608.228258	10.498957
9.112525	610.851505	10.503975
9.102988	617.683829	10.508992
8.809259	605.776475	10.514010
8.653820	610.117814	10.519027
9.153971	607.577737	10.524045
9.107315	609.913470	10.529063
9.148060	616.562319	10.534080
9.364915	618.412166	10.539098
8.989691	612.956870	10.544115
8.809633	612.942540	10.549133
8.947887	615.268972	10.554151
9.000773	615.924188	10.559168
9.039579	609.293785	10.564186
8.946855	616.239247	10.569203
9.248617	614.415688	10.574221
9.198521	611.468600	10.579239
8.932207	610.492422	10.584256
9.243183	620.466575	10.589274
9.089518	625.618305	10.594291
9.150363	631.068583	10.599309
9.029015	620.964683	10.604327
8.991083	633.295101	10.609344
9.586491	626.984544	10.614362
8.909661	632.352925	10.619379
9.161467	647.707459	10.624397
9.066248	644.122268	10.629415
9.223595	657.270183	10.634432
9.247427	645.979491	10.639450
9.260599	643.845121	10.644467
9.327348	633.991377	10.649485
9.286683	642.830070	10.654503
9.264100	642.081380	10.659520
9.330435	638.897172	10.664538
9.299037	648.959313	10.669555
9.348949	641.083583	10.674573
9.417173	638.852533	10.679591
9.228712	643.301879	10.684608
9.529740	634.640891	10.689626
9.283945	642.006372	10.694643
9.368172	633.019269	10.699661
9.389583	618.083003	10.704679
9.173006	614.887000	10.709696
9.122456	625.984879	10.714714
9.237351	641.443415	10.719731
9.268719	638.769619	10.724749
9.311327	625.105597	10.729767
9.254047	641.312436	10.734784
9.307519	642.988534	10.739802
9.247744	637.216974	10.744819
9.487865	654.376369	10.749837
9.683295	637.807972	10.754855
9.886345	643.083994	10.759872
9.511875	639.665796	10.764890
9.490646	637.183238	10.769907
9.510540	647.759249	10.774925
9.568697	653.148376	10.779943
9.302358	640.125743	10.784960
9.540572	636.642708	10.789978
9.436437	639.254333	10.794995
9.497758	640.804156	10.800013
9.591068	646.991657	10.805031
9.339153	645.186574	10.810048
9.445663	640.914326	10.815066
9.833101	639.660260	10.820083
9.638612	635.433819	10.825101
9.807276	623.804306	10.830119
9.004972	618.307203	10.835136
9.654759	617.690174	10.840154
9.723395	632.642659	10.845171
9.407314	624.707952	10.850189
9.573835	634.132467	10.855207
9.531797	647.278683	10.860224
9.683538	653.339427	10.865242
9.469075	644.714613	10.870259
9.183677	649.439874	10.875277
9.601847	639.144756	10.880295
9.698290	646.628258	10.885312
9.689378	643.609016	10.890330
9.161955	637.888954	10.895347
8.837162	646.337083	10.900365
9.543855	630.410748	10.905383
9.243000	648.061528	10.910400
9.376910	655.381194	10.915418
9.842576	664.707187	10.920435
9.826062	663.985343	10.925453
9.732140	657.480968	10.930471
9.666514	663.436027	10.935488
9.982929	660.718271	10.940506
9.917959	662.816727	10.945523
9.957032	661.824030	10.950541
10.166015	647.300754	10.955559
9.536158	644.776180	10.960576
9.784208	640.701664	10.965594
9.788938	643.407189	10.970611
9.711914	635.785467	10.975629
10.015454	636.675197	10.980647
9.774917	635.438407	10.985664
9.550161	637.001554	10.990682
9.906115	648.153610	10.995699
10.099961	661.969884	11.000717
10.009604	652.607461	11.005735
9.656054	655.015368	11.010752
9.934559	651.541417	11.015770
9.804364	657.701893	11.020787
9.565695	673.669694	11.025805
10.088243	655.006246	11.030823
9.929573	662.970910	11.035840
9.996567	665.466086	11.040858
10.145682	663.740077	11.045875
10.152501	663.915888	11.050893
10.119372	645.119516	11.055911
9.855181	641.879220	11.060928
9.921578	643.369849	11.065946
9.993459	643.549473	11.070963
9.618855	647.329117	11.075981
10.108529	650.808287	11.080999
10.200372	662.399399	11.086016
10.228822	647.292385	11.091034
10.180471	637.566892	11.096051
9.944622	640.356554	11.101069
10.249570	637.841941	11.106087
10.203320	641.469799	11.111104
9.948327	644.008636	11.116122
9.932663	634.366015	11.121139
9.825030	639.731560	11.126157
10.237052	640.662899	11.131175
9.891050	642.126814	11.136192
10.105899	655.920620	11.141210
10.268418	660.280381	11.146227
10.243090	654.150036	11.151245
10.420492	645.181184	11.156263
10.021473	643.657155	11.161280
9.945007	639.960815	11.166298
10.245632	634.773480	11.171315
10.243945	642.749981	11.176333
10.416397	633.967550	11.181351
9.851138	639.143511	11.186368
10.165531	644.896222	11.191386
10.508102	652.793991	11.196403
10.158441	644.538111	11.201421
10.409233	633.129326	11.206439
10.287274	639.847881	11.211456
10.073148	635.482191	11.216474
10.160882	645.985288	11.221491
10.319875	662.364344	11.226509
10.517061	651.086725	11.231527
10.203200	642.330826	11.236544
10.254156	650.998997	11.241562
10.438366	646.979313	11.246579
10.061803	661.039724	11.251597
10.669970	657.026439	11.256615
9.959314	645.906229	11.261632
10.127643	666.902209	11.266650
10.469534	658.976153	11.271667
10.462678	663.018986	11.276685
10.468525	664.668219	11.281703
10.215563	662.221491	11.286720
10.069124	661.510784	11.291738
10.578327	653.211573	11.296755
9.973258	664.962630	11.301773
10.441660	664.423301	11.306791
10.639494	667.109219	11.311808
10.214118	669.903932	11.316826
10.255428	669.019015	11.321843
10.198605	674.356002	11.326861
10.570512	663.563878	11.331879
10.402311	663.072280	11.336896
10.529126	660.790804	11.341914
10.450725	663.205498	11.346931
10.524960	682.396507	11.351949
10.562220	658.392657	11.356967
10.492946	666.057759	11.361984
10.171799	667.387178	11.367002
10.208886	655.092696	11.372019
10.200917	677.358055	11.377037
10.533474	681.030686	11.382055
10.796286	695.930971	11.387072
10.543862	697.438373	11.392090
10.587584	696.398556	11.397107
10.522292	694.214459	11.402125
10.958482	682.061741	11.407143
10.839305	703.009333	11.412160
10.841087	696.190164	11.417178
10.896871	672.740219	11.422195
10.355948	669.978444	11.427213
10.514158	659.243386	11.432231
10.355200	673.367043	11.437248
10.518490	688.961009	11.442266
11.022942	697.084662	11.447283
10.700710	699.419598	11.452301
10.899126	698.363271	11.457319
11.002362	687.922365	11.462336
10.822979	680.204958	11.467354
10.825791	661.647957	11.472371
10.507934	666.576879	11.477389
11.059699	672.656942	11.482407
11.078920	663.584124	11.487424
10.576948	662.861022	11.492442
10.905581	656.579286	11.497459
10.641466	664.669920	11.502477
10.655602	655.032793	11.507495
10.744967	670.061107	11.512512
10.906622	686.860934	11.517530
11.007205	680.122867	11.522547
10.895117	695.734990	11.527565
10.972626	689.295267	11.532583
10.885674	676.045848	11.537600
10.795564	678.074556	11.542618
11.116166	677.284700	11.547635
10.864342	671.839005	11.552653
10.695312	668.151952	11.557671
11.129888	689.927145	11.562688
10.730214	689.710665	11.567706
10.994428	685.633762	11.572723
11.059851	687.329736	11.577741
11.092723	690.009362	11.582759
11.211228	679.011804	11.587776
10.993073	679.476422	11.592794
11.024045	658.958524	11.597811
10.957292	661.532091	11.602829
11.077712	662.261763	11.607847
10.905927	670.380639	11.612864
10.877589	687.572823	11.617882
11.219462	687.307999	11.622899
10.889130	685.379378	11.627917
10.919154	686.331138	11.632935
10.996730	692.191985	11.637952
10.897588	687.235825	11.642970
11.204601	691.770993	11.647987
11.219365	692.948071	11.653005
10.956297	690.865445	11.658023
11.150851	694.388966	11.663040
11.140867	690.449090	11.668058
11.306476	678.044882	11.673075
11.188499	687.952095	11.678093
10.942499	698.168904	11.683111
11.087543	694.344032	11.688128
10.996849	696.622697	11.693146
11.046550	687.477714	11.698163
10.951486	687.154312	11.703181
10.909276	683.388827	11.708199
11.043424	681.445249	11.713216
11.272670	715.721987	11.718234
11.510456	708.757235	11.723251
11.284621	696.370366	11.728269
11.224379	694.803435	11.733287
11.397328	692.584200	11.738304
10.917778	688.734026	11.743322
11.523391	700.679557	11.748339
11.562900	715.881776	11.753357
11.822914	709.583705	11.758375
11.427944	685.382587	11.763392
11.312215	682.343889	11.768410
11.664769	679.254180	11.773427
11.592345	679.289866	11.778445
11.387455	687.320242	11.783463
11.676732	685.022346	11.788480
11.678445	690.391586	11.793498
11.735791	679.838999	11.798515
11.658912	683.126025	11.803533
11.545175	681.838755	11.808551
11.521510	677.641641	11.813568
11.425421	685.231375	11.818586
11.509060	678.088701	11.823603
11.546954	683.653106	11.828621
11.393773	687.432481	11.833639
11.581496	682.544349	11.838656
11.492987	685.646028	11.843674
11.767835	682.948226	11.848691
11.809062	679.010714	11.853709
11.333067	678.358009	11.858727
11.639975	673.831809	11.863744
11.445858	677.942200	11.868762
11.575823	679.156725	11.873779
11.516796	681.155695	11.878797
11.577187	669.486668	11.883815
11.240512	669.853865	11.888832
11.057762	678.684962	11.893850
11.185573	676.802558	11.898867
11.335139	681.709645	11.903885
11.462775	695.991929	11.908903
11.804754	694.932937	11.913920
11.253943	702.697216	11.918938
11.839935	701.443104	11.923955
11.674526	712.618579	11.928973
11.548353	710.139377	11.933991
11.199899	698.142390	11.939008
11.618667	705.394242	11.944026
11.737666	700.645785	11.949043
11.277084	708.759167	11.954061
11.476729	719.515821	11.959079
11.616265	705.593429	11.964096
12.025223	712.126068	11.969114
12.066449	715.504884	11.974131
12.071877	707.295488	11.979149
11.703898	699.438598	11.984167
12.097057	709.876309	11.989184
11.690845	714.157266	11.994202
11.955252	697.070114	11.999219
12.032298	716.136215	12.004237
11.794205	710.873342	12.009255
12.100609	703.613149	12.014272
12.213983	706.433975	12.019290
12.303749	703.366038	12.024307
12.215105	705.716891	12.029325
11.808252	714.467150	12.034343
12.006468	717.849349	12.039360
12.099089	717.768898	12.044378
12.136350	708.710491	12.049395
12.126181	706.323813	12.054413
11.762347	710.949771	12.059431
12.022848	698.827549	12.064448
11.847955	711.016814	12.069466
11.645659	707.166971	12.074483
11.784706	708.931968	12.079501
11.949411	705.847907	12.084519
11.776079	701.997215	12.089536
11.732912	713.673953	12.094554
12.021394	723.392289	12.099571
12.306965	733.069388	12.104589
12.333749	728.755380	12.109607
12.523569	715.920935	12.114624
12.566355	714.390904	12.119642
11.833714	715.898250	12.124659
12.205843	703.821248	12.129677
11.893957	700.017464	12.134695
12.320180	695.975586	12.139712
11.884157	705.990969	12.144730
12.118997	706.990071	12.149747
12.300630	714.828164	12.154765
11.776577	714.482363	12.159783
12.461348	725.113682	12.164800
12.614037	730.696037	12.169818
12.173471	717.383189	12.174835
12.229071	703.433929	12.179853
12.335372	720.788120	12.184871
12.505470	729.250263	12.189888
12.415550	722.403428	12.194906
12.506991	705.350360	12.199923
12.507970	704.517669	12.204941
12.339410	701.386338	12.209959
12.532256	699.868315	12.214976
12.191026	702.998575	12.219994
12.410040	700.946301	12.225011
12.706201	701.257337	12.230029
12.525414	707.430425	12.235047
12.395066	698.554911	12.240064
11.953400	709.169056	12.245082
12.242895	709.085201	12.250099
12.491826	711.632292	12.255117
12.306267	725.352689	12.260135
12.878774	726.090810	12.265152
12.655471	716.543759	12.270170
12.485259	707.329711	12.275187
12.305247	699.924941	12.280205
12.628553	711.260556	12.285223
12.554132	707.961626	12.290240
12.655416	704.296811	12.295258
12.403191	706.134733	12.300275
12.350832	717.745289	12.305293
12.288576	728.768714	12.310311
12.626242	733.929329	12.315328
12.649210	750.978581	12.320346
12.797566	743.410294	12.325363
12.526808	739.619484	12.330381
12.675618	739.631109	12.335399
12.661409	733.826102	12.340416
12.598438	730.986809	12.345434
12.336534	725.228937	12.350451
12.655259	730.148137	12.355469
12.554449	741.074121	12.360487
12.396480	742.885351	12.365504
12.670293	735.398286	12.370522
12.758030	741.446319	12.375539
12.933960	736.621230	12.380557
12.851281	739.155618	12.385575
13.057134	737.329196	12.390592
12.835605	727.636299	12.395610
12.820905	744.835445	12.400627
12.853891	739.074597	12.405645
12.859277	743.967151	12.410663
13.212274	741.164707	12.415680
12.819287	734.307429	12.420698
12.871320	737.529963	12.425715
12.832667	733.143022	12.430733
12.802294	740.380644	12.435751
12.847108	732.280158	12.440768
13.020107	745.887983	12.445786
13.000233	741.033351	12.450803
13.298428	737.310795	12.455821
13.060389	745.319420	12.460839
12.554983	739.614083	12.465856
12.790151	736.301185	12.470874
12.983726	744.810038	12.475891
13.241031	733.715600	12.480909
12.988743	731.512802	12.485927
13.233851	729.995095	12.490944
12.997229	732.994904	12.495962
12.691323	737.618875	12.500979
12.886393	726.052133	12.505997
13.057214	732.783358	12.511015
13.091990	727.172192	12.516032
13.067124	720.024107	12.521050
12.816653	730.015436	12.526067
13.067519	738.216543	12.531085
12.256831	732.042556	12.536103
12.749069	738.328708	12.541120
13.300772	743.559352	12.546138
12.980689	755.670300	12.551155
13.262946	754.789550	12.556173
13.176044	752.910440	12.561191
13.250523	764.100435	12.566208
13.438514	746.725612	12.571226
13.244184	756.243784	12.576243
13.923704	744.628462	12.581261
13.275147	745.929527	12.586279
13.466622	729.318189	12.591296
13.364845	728.987235	12.596314
12.992602	725.361993	12.601331
13.428153	725.636021	12.606349
13.376299	723.760570	12.611367
13.271052	730.277913	12.616384
13.638934	723.369496	12.621402
13.376678	734.360731	12.626419
13.331613	725.696660	12.631437
13.236733	730.817356	12.636455
13.515010	734.376846	12.641472
13.239841	732.497458	12.646490
13.284973	745.858448	12.651507
13.392835	744.629122	12.656525
13.104143	748.293134	12.661543
13.604447	752.855423	12.666560
13.625378	750.095651	12.671578
13.599339	745.994564	12.676595
13.629480	753.131164	12.681613
13.545483	753.528740	12.686631
13.375040	755.474786	12.691648
13.778399	745.375712	12.696666
13.593155	758.617330	12.701683
13.476692	748.419248	12.706701
13.520826	762.020631	12.711719
13.505893	752.223511	12.716736
13.645937	744.211594	12.721754
13.561944	740.786407	12.726771
13.711314	740.587247	12.731789
13.704789	745.717654	12.736807
13.620020	746.013505	12.741824
13.715602	731.272120	12.746842
13.518373	746.135603	12.751859
13.624941	746.232836	12.756877
13.685675	749.309767	12.761895
13.538256	744.674011	12.766912
13.763524	751.912102	12.771930
13.533826	756.503312	12.776947
13.637094	748.562420	12.781965
13.603755	758.702401	12.786983
13.609453	745.631475	12.792000
13.780387	749.012384	12.797018
13.606462	749.873857	12.802035
13.656554	743.954203	12.807053
13.597556	750.040953	12.812071
13.525986	744.328871	12.817088
14.014204	765.297709	12.822106
14.195695	775.262460	12.827123
13.890692	767.384697	12.832141
13.898678	763.248951	12.837159
13.901643	764.813351	12.842176
14.287672	753.942564	12.847194
14.188095	744.237180	12.852211
14.150116	745.507215	12.857229
14.087046	747.270190	12.862247
13.917997	752.509824	12.867264
14.012885	748.359919	12.872282
13.858953	760.270610	12.877299
14.187960	749.615808	12.882317
14.038657	748.152157	12.887335
13.929816	752.163844	12.892352
13.555457	750.470993	12.897370
13.697444	758.277675	12.902387
13.961745	765.842238	12.907405
14.349532	768.208742	12.912423
14.563378	768.903201	12.917440
14.407621	759.408532	12.922458
14.511094	759.424992	12.927475
14.249028	749.138096	12.932493
13.825214	754.321621	12.937511
13.909071	745.897802	12.942528
14.202972	735.645002	12.947546
13.863111	756.413032	12.952563
14.273666	771.030654	12.957581
14.690310	770.699644	12.962599
14.307637	767.925969	12.967616
14.308531	744.324777	12.972634
14.096578	743.972371	12.977651
13.996591	757.782673	12.982669
14.510177	767.348209	12.987687
14.223954	771.402597	12.992704
14.259772	762.940554	12.997722
14.521437	775.772368	13.002739
14.400998	768.734920	13.007757
14.802061	772.613538	13.012775
14.531619	774.698039	13.017792
14.433811	751.817652	13.022810
14.411891	748.789910	13.027827
14.420956	755.105530	13.032845
14.349745	744.078756	13.037863
14.341490	763.279562	13.042880
14.882112	760.821735	13.047898
14.659497	746.411511	13.052915
14.650679	737.524649	13.057933
14.703322	735.053978	13.062951
14.543211	738.198105	13.067968
14.637943	726.653848	13.072986
14.331181	741.792765	13.078003
14.253691	737.418538	13.083021
14.423062	747.302611	13.088039
14.252076	760.882466	13.093056
14.579757	757.645598	13.098074
14.478661	766.775895	13.103091
14.677086	764.759097	13.108109
14.626653	758.821999	13.113127
14.588632	774.466640	13.118144
14.528617	769.691848	13.123162
14.505911	767.219649	13.128179
14.803674	769.562160	13.133197
14.836052	766.631427	13.138215
15.250692	764.885441	13.143232
14.882552	759.489344	13.148250
15.028354	767.241571	13.153267
14.752717	762.568839	13.158285
14.851164	762.568219	13.163303
14.794156	759.915304	13.168320
14.738043	768.627118	13.173338
14.861292	761.258901	13.178355
14.894901	763.776635	13.183373
14.693341	758.806476	13.188391
14.605020	766.072088	13.193408
15.023420	766.896790	13.198426
14.822297	764.762881	13.203443
14.411389	767.880262	13.208461
14.763304	759.408202	13.213479
14.650805	769.915640	13.218496
15.008263	763.222180	13.223514
14.839048	769.666168	13.228531
14.502600	760.774291	13.233549
14.890309	773.118819	13.238567
14.723274	787.390642	13.243584
15.131443	787.817202	13.248602
15.175215	795.925321	13.253619
14.909692	795.008341	13.258637
15.311914	791.726280	13.263655
15.397399	795.783903	13.268672
15.468181	785.228137	13.273690
15.142228	766.157719	13.278707
15.120975	760.211076	13.283725
15.094065	747.572333	13.288743
15.034597	752.463306	13.293760
15.222557	758.352584	13.298778
15.223581	771.762217	13.303795
15.094258	778.820770	13.308813
15.220796	765.834170	13.313831
15.311120	778.777653	13.318848
15.310739	789.228493	13.323866
15.251925	795.035652	13.328883
15.261035	779.974905	13.333901
15.483127	776.445692	13.338919
15.490649	776.192919	13.343936
15.558660	773.970643	13.348954
15.320913	759.589281	13.353971
14.984507	759.536527	13.358989
15.212656	763.683145	13.364007
15.292502	775.966464	13.369024
15.701885	773.919625	13.374042
15.649264	782.428640	13.379059
15.466570	782.262802	13.384077
15.720765	769.526613	13.389095
15.527197	760.395906	13.394112
15.296332	753.077651	13.399130
15.235170	758.307823	13.404147
15.265833	777.692242	13.409165
15.918842	778.908318	13.414183
15.402283	781.820168	13.419200
15.408894	781.041257	13.424218
15.673580	780.393685	13.429235
15.597759	782.393869	13.434253
15.884718	783.935942	13.439271
15.395699	793.458847	13.444288
15.750685	777.156107	13.449306
15.991893	775.193743	13.454323
15.276120	773.380273	13.459341
15.603629	770.723646	13.464359
15.332263	785.973371	13.469376
15.493539	782.365639	13.474394
15.720793	779.601387	13.479411
15.583855	774.029700	13.484429
16.042480	778.151422	13.489447
15.608812	789.670544	13.494464
15.666485	791.663627	13.499482
16.070111	782.759458	13.504499
15.787204	775.741277	13.509517
15.981110	778.665422	13.514535
15.636499	783.093082	13.519552
15.546877	785.650963	13.524570
15.615565	780.175980	13.529587
15.617916	787.758748	13.534605
15.822075	779.282555	13.539623
15.928650	784.776405	13.544640
15.844661	777.526960	13.549658
15.827808	773.500712	13.554675
15.345858	781.853155	13.559693
15.960280	797.968150	13.564711
16.236825	810.837390	13.569728
16.059291	807.305324	13.574746
16.412851	796.664244	13.579763
16.220726	788.844378	13.584781
15.968246	780.246829	13.589799
15.849010	779.971507	13.594816
16.056716	785.520089	13.599834
16.248266	770.071389	13.604851
15.782876	771.457325	13.609869
16.071174	797.684728	13.614887
16.467314	805.212073	13.619904
16.332381	804.232574	13.624922
16.415430	779.862170	13.629939
15.875833	781.741980	13.634957
16.074421	783.296689	13.639975
16.207274	791.272388	13.644992
16.530617	800.018642	13.650010
16.348672	782.816408	13.655027
16.082054	776.559381	13.660045
16.256447	786.788063	13.665063
16.522588	802.066085	13.670080
16.455001	792.544032	13.675098
16.345889	772.795559	13.680115
16.116198	780.869150	13.685133
16.544095	777.169927	13.690151
16.613253	783.704625	13.695168
16.364108	779.911611	13.700186
16.274393	773.069344	13.705203
16.144248	784.871909	13.710221
16.806152	776.432260	13.715239
16.568644	782.673993	13.720256
16.004341	779.691001	13.725274
16.427898	788.609238	13.730291
16.649767	795.915420	13.735309
16.704944	791.513941	13.740327
16.761974	805.293318	13.745344
16.500063	794.130236	13.750362
16.376388	790.085422	13.755379
16.566206	798.250299	13.760397
16.726839	792.120856	13.765415
16.537667	808.447386	13.770432
16.300845	811.742862	13.775450
16.251241	801.369354	13.780467
16.620403	810.657161	13.785485
16.674797	798.536446	13.790503
16.761276	809.994229	13.795520
16.469554	792.479079	13.800538
16.847847	793.021975	13.805555
16.476016	800.526056	13.810573
16.792199	802.314243	13.815591
16.703725	802.813823	13.820608
16.704117	797.146020	13.825626
16.839461	795.305461	13.830643
16.856580	798.321215	13.835661
17.061215	805.026809	13.840679
16.978126	804.045434	13.845696
16.896603	808.959259	13.850714
16.833241	798.760241	13.855731
16.613999	795.453340	13.860749
17.036408	795.618143	13.865767
16.939441	797.855051	13.870784
16.647859	801.436102	13.875802
16.787843	797.971823	13.880819
16.571089	809.976089	13.885837
16.848333	806.205511	13.890855
16.997956	823.754594	13.895872
17.062650	830.375075	13.900890
17.246959	825.262007	13.905907
17.167833	832.904710	13.910925
17.342021	821.503820	13.915943
17.536554	815.211115	13.920960
17.062825	807.602511	13.925978
17.223862	791.638645	13.930995
17.165401	796.274489	13.936013
17.073698	794.669251	13.941031
17.292060	798.703539	13.946048
16.860631	801.738112	13.951066
17.124538	786.692723	13.956083
17.173069	806.670876	13.961101
17.139173	815.112062	13.966119
17.330787	822.464785	13.971136
17.031980	826.177919	13.976154
17.575800	815.071797	13.981171
17.318793	821.281735	13.986189
17.458862	825.003039	13.991207
17.812450	822.910502	13.996224
17.446363	822.662588	14.001242
17.448581	806.596036	14.006259
16.874729	797.087968	14.011277
16.969565	814.645307	14.016295
17.177128	818.503856	14.021312
17.265697	828.384605	14.026330
17.583584	827.591451	14.031347
17.241189	822.614235	14.036365
17.541312	823.295423	14.041383
17.544366	814.867599	14.046400
17.459344	823.174151	14.051418
17.416493	824.192875	14.056435
17.395182	833.599151	14.061453
17.551406	819.204687	14.066471
17.666219	829.709143	14.071488
17.463174	823.804129	14.076506
17.477633	824.172151	14.081523
17.271134	837.810099	14.086541
17.804642	838.513734	14.091559
18.192957	833.098295	14.096576
17.824469	825.992873	14.101594
17.713630	818.717733	14.106611
17.782173	814.736014	14.111629
17.753361	813.883244	14.116647
17.749329	814.918580	14.121664
17.567615	811.356303	14.126682
17.867430	805.827568	14.131699
17.470745	814.096461	14.136717
17.763772	838.569117	14.141735
18.122432	846.601806	14.146752
17.872943	847.779067	14.151770
17.781549	838.709468	14.156787
18.048528	850.494283	14.161805
18.138401	841.227038	14.166823
17.839160	829.694373	14.171840
17.704366	828.821721	14.176858
17.822409	836.022856	14.181875
18.195308	846.013887	14.186893
17.895919	840.430642	14.191911
18.228095	841.842829	14.196928
18.703464	844.774992	14.201946
18.440983	823.975403	14.206963
18.129469	823.724374	14.211981
17.896883	812.011051	14.216999
17.959780	813.722612	14.222016
17.989188	814.337532	14.227034
18.315366	813.389491	14.232051
17.875260	818.435792	14.237069
18.053970	836.437880	14.242087
18.494900	835.260477	14.247104
18.126293	834.376471	14.252122
17.990423	836.087029	14.257139
18.170833	841.653723	14.262157
18.421689	838.753496	14.267175
18.695332	839.807896	14.272192
18.195757	847.502767	14.277210
18.481111	839.398689	14.282227
18.484717	837.447634	14.287245
18.134010	840.289377	14.292263
18.652746	846.524649	14.297280
18.377909	841.266031	14.302298
18.354012	824.696774	14.307315
18.586833	827.179335	14.312333
18.254424	828.692881	14.317351
18.583847	826.643898	14.322368
18.391036	839.893233	14.327386
18.577122	841.631676	14.332403
18.732865	850.229110	14.337421
18.490618	840.114340	14.342439
18.817558	841.509678	14.347456
18.503018	833.439591	14.352474
18.614227	822.056587	14.357491
18.249453	823.633346	14.362509
18.354531	839.031313	14.367527
18.499741	844.186965	14.372544
18.337181	842.768992	14.377562
18.517315	843.666828	14.382579
18.705966	846.924476	14.387597
18.363772	845.772172	14.392615
18.399581	839.233488	14.397632
18.352952	853.291610	14.402650
18.506933	859.150031	14.407667
19.057048	854.733465	14.412685
18.864795	874.451153	14.417703
19.081916	872.736811	14.422720
18.947429	860.584278	14.427738
19.010455	853.514406	14.432755
19.041486	847.535667	14.437773
18.750716	842.883912	14.442791
19.211210	839.734707	14.447808
18.932448	840.740654	14.452826
18.771029	839.818276	14.457843
18.822952	834.941417	14.462861
18.679535	851.266336	14.467879
19.137666	857.104215	14.472896
18.892877	864.196649	14.477914
18.957762	873.072452	14.482931
19.174886	869.445631	14.487949
19.061025	874.697837	14.492967
19.336132	869.400683	14.497984
19.407864	872.037213	14.503002
18.966809	862.935042	14.508019
19.081073	865.051634	14.513037
18.988735	869.494903	14.518055
19.359121	871.850031	14.523072
19.347455	871.095589	14.528090
19.288761	873.220689	14.533107
19.655115	871.508847	14.538125
18.861612	853.875989	14.543143
19.397108	859.207465	14.548160
19.154599	866.343021	14.553178
19.022949	873.425423	14.558195
19.421909	866.196112	14.563213
19.020923	871.117087	14.568231
19.651221	865.742344	14.573248
19.336789	873.724887	14.578266
19.447192	866.745195	14.583283
19.332001	867.969544	14.588301
19.567039	865.504138	14.593319
19.320968	873.266757	14.598336
19.523787	863.328579	14.603354
19.333308	870.181962	14.608371
19.708801	868.933887	14.613389
19.590498	873.283826	14.618407
19.676360	873.274166	14.623424
19.677019	871.654838	14.628442
19.387357	863.414312	14.633459
19.415610	866.734095	14.638477
19.308173	871.793144	14.643495
19.662046	869.274837	14.648512
19.702023	868.187702	14.653530
19.793521	862.501868	14.658547
19.609011	861.582715	14.663565
19.697011	877.733418	14.668583
19.946916	869.597984	14.673600
19.871471	869.117228	14.678618
19.653042	873.159357	14.683635
19.950867	855.386894	14.688653
19.726369	862.263805	14.693671
19.810457	857.945506	14.698688
19.875579	866.782494	14.703706
19.434027	871.151407	14.708723
19.875299	885.998473	14.713741
20.261781	896.406515	14.718759
20.503727	883.477110	14.723776
20.022187	872.741735	14.728794
19.616660	867.369098	14.733811
20.293772	861.667185	14.738829
19.845819	865.556722	14.743847
19.912483	863.152206	14.748864
19.898100	872.237926	14.753882
20.047492	888.551498	14.758899
20.312832	892.331238	14.763917
20.170132	895.483837	14.768935
20.152957	890.989775	14.773952
20.150636	882.118387	14.778970
20.260969	887.011948	14.783987
20.075312	888.466215	14.789005
19.890343	891.421698	14.794023
20.140225	895.724577	14.799040
20.003219	900.425983	14.804058
20.060845	896.449983	14.809075
20.469595	887.748811	14.814093
20.352098	898.190540	14.819111
20.234985	894.059392	14.824128
20.131768	893.359245	14.829146
20.140331	899.162591	14.834163
20.524260	892.132373	14.839181
20.193493	888.608881	14.844199
20.214985	898.673762	14.849216
20.447302	893.337814	14.854234
20.104784	892.670520	14.859251
20.537311	906.458792	14.864269
20.474635	911.437634	14.869287
20.797767	906.841866	14.874304
20.899144	921.170818	14.879322
20.210149	902.604640	14.884339
20.591925	905.197222	14.889357
20.847153	910.941704	14.894375
20.664818	897.820633	14.899392
20.486758	901.755918	14.904410
20.644982	902.780389	14.909427
20.967373	903.443533	14.914445
20.630808	910.928456	14.919463
20.802913	915.726989	14.924480
20.958573	907.915721	14.929498
20.391413	905.739737	14.934515
20.827433	913.601436	14.939533
20.932581	914.583112	14.944551
21.005239	910.093684	14.949568
20.730867	912.393187	14.954586
21.153098	912.208669	14.959603
20.955821	911.231790	14.964621
20.778451	914.438932	14.969639
20.852511	913.868322	14.974656
20.997889	906.687588	14.979674
20.713717	914.613781	14.984691
20.794802	901.807976	14.989709
20.665839	906.089224	14.994727
20.768137	905.984343	14.999744
20.766715	908.788651	15.004762
20.956994	911.492591	15.009779
20.890112	899.945290	15.014797
20.893653	909.223511	15.019815
20.918452	926.045231	15.024832
21.296341	933.894700	15.029850
21.173795	943.716921	15.034867
21.578790	925.762323	15.039885
21.641494	923.950876	15.044903
21.399830	908.493522	15.049920
21.556661	907.178446	15.054938
21.275784	911.699333	15.059955
21.387392	899.079006	15.064973
21.410696	900.038188	15.069991
21.298889	894.543983	15.075008
21.159081	895.857626	15.080026
21.338449	903.964061	15.085043
21.189614	893.830276	15.090061
21.430057	916.889342	15.095079
21.534527	928.123804	15.100096
21.874560	924.955519	15.105114
21.743649	905.791485	15.110131
21.578218	906.809608	15.115149
21.496080	908.200715	15.120167
21.541179	910.484033	15.125184
21.726418	892.521701	15.130202
21.467697	911.813682	15.135219
21.727124	904.201965	15.140237
21.774246	900.558354	15.145255
21.357312	890.835942	15.150272
21.815649	896.690729	15.155290
21.646114	897.247597	15.160307
21.866993	898.113313	15.165325
21.421430	908.233732	15.170343
21.651729	921.222501	15.175360
21.785971	926.463248	15.180378
21.980331	929.346802	15.185395
22.065211	922.241403	15.190413
22.102651	901.783026	15.195431
21.677356	909.498127	15.200448
21.760520	908.490059	15.205466
21.728943	929.315530	15.210483
21.917636	929.018841	15.215501
22.016932	934.098266	15.220519
21.972167	931.019745	15.225536
22.153271	923.774841	15.230554
21.965629	932.686112	15.235571
22.150128	918.388834	15.240589
22.106421	926.427436	15.245607
22.013368	930.363246	15.250624
22.597707	929.126907	15.255642
21.992523	924.447767	15.260659
21.744635	925.734004	15.265677
22.217832	924.022805	15.270695
21.959007	936.474404	15.275712
22.170844	935.138821	15.280730
21.845060	930.420396	15.285747
21.846884	937.529976	15.290765
22.203826	928.142966	15.295783
22.025551	925.723611	15.300800
22.239829	932.455812	15.305818
21.890271	938.635035	15.310835
21.801224	949.220105	15.315853
22.059327	951.249564	15.320871
22.606914	957.993615	15.325888
22.872606	955.522341	15.330906
22.659809	961.837807	15.335923
22.791700	956.331454	15.340941
22.974981	954.695715	15.345959
22.546335	951.901064	15.350976
22.898751	929.338960	15.355994
22.513512	922.473427	15.361011
22.435591	917.155278	15.366029
22.662430	920.441665	15.371047
22.283445	928.589209	15.376064
22.947481	937.945867	15.381082
22.666852	952.901862	15.386099
22.800174	947.771397	15.391117
22.655952	953.226253	15.396135
22.123294	950.604671	15.401152
22.494606	954.747365	15.406170
22.677519	953.349052	15.411187
22.489377	962.062815	15.416205
22.764099	951.632854	15.421223
22.730324	955.117212	15.426240
22.961551	952.391046	15.431258
22.786654	952.803353	15.436275
22.490133	947.631340	15.441293
22.936024	954.539218	15.446311
23.061695	971.814717	15.451328
22.976015	959.488712	15.456346
22.888544	956.873273	15.461363
22.785489	970.556045	15.466381
23.372045	965.966129	15.471399
23.238548	982.202357	15.476416
23.527835	965.288917	15.481434
23.291136	960.114492	15.486451
23.185384	947.989026	15.491469
23.247642	940.494112	15.496487
23.179956	940.340168	15.501504
23.160680	935.532514	15.506522
23.213540	938.143044	15.511539
23.159043	950.762826	15.516557
23.077872	931.922770	15.521575
23.044492	941.806228	15.526592
23.652202	948.734402	15.531610
23.578261	954.877139	15.536627
23.477898	942.854510	15.541645
23.421328	940.805726	15.546663
22.914705	946.753862	15.551680
23.268079	949.456247	15.556698
23.376696	965.221019	15.561715
22.881522	969.724391	15.566733
23.356749	963.351782	15.571751
23.095733	965.445378	15.576768
23.647185	967.929630	15.581786
23.451449	974.789832	15.586803
23.556170	965.928064	15.591821
23.784959	961.171914	15.596839
23.356601	969.387077	15.601856
22.935764	962.074331	15.606874
23.490343	982.082062	15.611891
23.627514	989.884344	15.616909
24.014269	982.400933	15.621927
24.052932	981.397656	15.626944
24.215622	986.474102	15.631962
24.515509	981.171438	15.636979
24.136068	958.518651	15.641997
24.617991	949.320390	15.647015
24.323573	954.951027	15.652032
24.398668	949.634152	15.657050
24.285191	946.984632	15.662067
23.834185	929.087050	15.667085
23.884738	919.928010	15.672103
23.876474	931.828638	15.677120
24.471467	934.177363	15.682138
24.280129	923.877775	15.687155
23.945492	924.616036	15.692173
24.230256	919.327898	15.697191
24.132048	924.393313	15.702208
24.210776	914.526191	15.707226
24.277655	914.977270	15.712243
23.823913	913.946921	15.717261
24.100466	923.644723	15.722279
24.108640	944.030447	15.727296
24.341818	946.302372	15.732314
24.473896	956.416920	15.737331
24.168357	945.505385	15.742349
24.358754	942.629300	15.747367
24.095119	955.367491	15.752384
24.322015	946.803014	15.757402
24.313637	952.514511	15.762419
24.384845	970.259171	15.767437
24.712356	949.182808	15.772455
24.631391	955.789428	15.777472
24.470792	949.800394	15.782490
24.770767	947.547043	15.787507
24.102692	953.231357	15.792525
24.265964	955.199335	15.797543
24.344478	950.106661	15.802560
24.228269	954.778273	15.807578
24.383990	955.147163	15.812595
24.388345	950.789070	15.817613
24.605689	953.518068	15.822631
24.586099	960.634149	15.827648
24.843415	978.173289	15.832666
24.859040	970.414259	15.837683
24.710262	967.505060	15.842701
25.063306	969.121258	15.847719
24.991147	973.517529	15.852736
24.423062	957.775931	15.857754
24.797131	956.158066	15.862771
24.846690	969.177530	15.867789
25.059746	958.368052	15.872807
24.992292	982.032143	15.877824
24.967625	973.624755	15.882842
25.041491	975.894276	15.887859
24.918469	975.938619	15.892877
24.960688	973.365514	15.897895
25.274663	978.841300	15.902912
25.272264	971.677674	15.907930
25.393855	968.741903	15.912947
25.043465	977.759412	15.917965
25.314540	962.367642	15.922983
24.783323	975.676953	15.928000
24.987684	969.137128	15.933018
25.258965	969.970113	15.938035
25.371053	983.976736	15.943053
25.210385	971.411775	15.948071
25.166553	976.776440	15.953088
25.577207	970.933707	15.958106
25.560547	967.248464	15.963123
25.110236	970.237181	15.968141
25.359193	963.551035	15.973159
25.296972	979.921521	15.978176
25.081797	982.839500	15.983194
25.475581	974.887485	15.988211
25.091389	963.245942	15.993229
25.289209	969.479187	15.998247
25.308768	984.382852	16.003264
25.411378	1003.846106	16.008282
25.863770	996.144394	16.013299
25.901402	1006.564301	16.018317
25.920897	995.486437	16.023335
25.562192	982.117906	16.028352
25.755457	995.254371	16.033370
25.998422	988.743586	16.038387
25.351160	971.790250	16.043405
25.613962	987.378409	16.048423
25.488338	998.998726	16.053440
25.538213	1005.497735	16.058458
25.821945	991.919112	16.063475
25.740151	998.191294	16.068493
25.881866	996.887172	16.073511
26.036069	999.240649	16.078528
26.114798	1001.138759	16.083546
25.981546	986.788431	16.088563
25.984427	1000.565320	16.093581
25.929206	992.654429	16.098599
26.104787	989.968353	16.103616
26.161028	995.091129	16.108634
26.275162	999.318848	16.113651
26.073775	997.880903	16.118669
26.349760	994.133713	16.123687
26.155335	1008.861968	16.128704
26.087409	999.212107	16.133722
25.991113	1001.695351	16.138739
25.707032	1007.244981	16.143757
26.302274	1014.634033	16.148775
26.649063	1004.106707	16.153792
26.550234	1017.107630	16.158810
26.657925	1000.249944	16.163827
26.518356	999.922080	16.168845
26.389132	1003.956194	16.173863
26.542624	985.761045	16.178880
26.802623	998.285988	16.183898
26.587591	984.763222	16.188915
26.310459	989.640149	16.193933
26.514425	997.694742	16.198951
26.519100	996.987389	16.203968
26.321484	992.379240	16.208986
26.600146	990.619091	16.214003
26.403796	998.405638	16.219021
26.325820	1012.249631	16.224039
26.563305	1022.630225	16.229056
26.601025	1022.421662	16.234074
26.856422	1019.973730	16.239091
26.871175	1030.074452	16.244109
26.647239	1012.870041	16.249127
26.687973	1012.864689	16.254144
26.823097	1016.139486	16.259162
27.347733	1011.251176	16.264179
26.812968	1018.477217	16.269197
26.643778	1023.274122	16.274215
26.751827	1016.368755	16.279232
26.756674	1017.944286	16.284250
26.704242	1012.168222	16.289267
26.722850	1018.336629	16.294285
26.834938	1043.157378	16.299303
27.506840	1053.664993	16.304320
27.352728	1049.927849	16.309338
27.346926	1033.289441	16.314355
27.285229	1020.560273	16.319373
26.925182	1011.130501	16.324391
27.448194	1015.380210	16.329408
27.053531	1018.006055	16.334426
27.817638	1017.615655	16.339443
27.462912	1022.382993	16.344461
27.213835	1013.374184	16.349479
27.638075	998.084016	16.354496
27.338052	1003.931311	16.359514
27.764167	993.434184	16.364531
27.385001	996.113559	16.369549
27.736088	1007.702146	16.374567
27.322538	1002.369559	16.379584
27.607274	1004.448947	16.384602
27.724065	1000.200783	16.389619
27.553877	996.967608	16.394637
27.916209	989.610061	16.399655
27.741640	990.789517	16.404672
27.187251	1003.894446	16.409690
27.688878	996.339691	16.414707
27.456022	994.238548	16.419725
27.648842	1012.186157	16.424743
27.975271	1018.519411	16.429760
27.977930	1029.134256	16.434778
28.003578	1015.412660	16.439795
28.098197	1008.184764	16.444813
28.008982	999.302474	16.449831
28.014907	991.612939	16.454848
27.565519	996.053840	16.459866
27.907326	1005.165804	16.464883
27.824040	1018.149791	16.469901
27.874085	1027.572540	16.474919
28.371865	1027.439897	16.479936
28.322218	1024.440104	16.484954
28.402245	1028.508533	16.489971
28.340552	1015.136751	16.494989
28.001177	996.325309	16.500007
28.132943	991.968784	16.505024
27.823274	1003.524651	16.510042
28.464332	1008.294924	16.515059
28.538523	1016.753000	16.520077
28.213907	1015.015191	16.525095
28.038994	1017.032370	16.530112
27.932773	1031.690765	16.535130
28.372329	1020.868220	16.540147
28.224563	1023.098400	16.545165
28.406147	1018.317361	16.550183
28.611443	1020.225852	16.555200
28.229454	1034.812517	16.560218
28.595843	1018.448198	16.565235
28.858437	1019.413507	16.570253
28.411863	1026.903478	16.575271
28.185461	1015.974878	16.580288
28.378104	1018.290318	16.585306
28.554115	1017.500525	16.590323
28.356104	1018.894651	16.595341
28.246711	1025.319216	16.600359
28.807084	1029.896955	16.605376
28.944794	1039.117262	16.610394
28.636863	1033.088969	16.615411
28.665545	1037.668956	16.620429
28.844787	1037.072890	16.625447
29.119688	1036.565330	16.630464
28.628139	1047.001070	16.635482
28.913677	1040.870963	16.640499
28.910287	1043.478014	16.645517
28.942233	1033.889764	16.650535
29.281516	1034.426127	16.655552
29.017419	1035.766815	16.660570
29.152683	1045.193402	16.665587
29.078075	1040.257675	16.670605
28.884209	1040.459766	16.675623
29.066644	1031.209192	16.680640
28.830213	1032.294953	16.685658
29.341427	1033.121162	16.690675
29.338274	1033.778866	16.695693
29.151694	1039.478118	16.700711
29.334089	1032.834628	16.705728
29.210521	1042.606106	16.710746
29.204793	1026.174551	16.715763
29.237542	1038.587104	16.720781
29.222496	1056.628162	16.725799
29.463710	1062.955440	16.730816
29.297189	1074.518409	16.735834
29.526716	1062.613586	16.740851
29.696652	1059.263375	16.745869
29.464787	1063.925593	16.750887
29.781013	1059.324229	16.755904
29.403510	1066.475099	16.760922
29.909692	1068.249242	16.765939
29.927289	1062.274017	16.770957
29.670210	1065.382766	16.775975
29.917023	1062.910266	16.780992
29.818751	1063.932456	16.786010
29.703679	1056.060945	16.791027
30.221770	1068.417135	16.796045
29.872309	1071.241787	16.801063
30.184076	1061.313230	16.806080
29.880324	1069.622602	16.811098
29.885141	1067.427259	16.816115
30.117779	1054.627970	16.821133
30.007119	1065.513890	16.826151
30.033398	1056.562686	16.831168
30.189972	1053.739210	16.836186
29.969527	1055.409446	16.841203
30.228719	1062.167742	16.846221
29.940023	1069.927071	16.851239
30.433311	1058.799602	16.856256
30.396471	1056.113190	16.861274
30.319846	1059.957749	16.866291
30.424872	1055.727259	16.871309
30.239011	1053.656524	16.876327
30.526787	1041.596051	16.881344
30.160324	1056.504923	16.886362
30.259618	1053.646038	16.891379
30.291592	1057.373846	16.896397
29.883232	1062.932420	16.901415
30.080966	1063.262880	16.906432
30.165248	1064.065561	16.911450
29.938198	1054.114845	16.916467
30.241954	1065.230465	16.921485
30.629945	1086.746937	16.926503
30.578789	1088.894439	16.931520
30.648935	1088.852538	16.936538
30.808662	1081.572516	16.941555
30.841415	1086.981248	16.946573
30.595245	1087.554329	16.951591
31.021483	1081.017352	16.956608
30.818386	1086.933098	16.961626
30.537886	1087.679740	16.966643
30.928577	1084.751832	16.971661
30.752317	1087.532908	16.976679
30.961471	1081.056997	16.981696
31.018002	1083.834243	16.986714
30.532448	1081.996859	16.991731
31.093852	1083.116898	16.996749
30.576678	1077.029281	17.001767
30.979666	1078.687427	17.006784
30.914980	1087.340512	17.011802
31.020119	1105.203326	17.016819
31.072784	1117.973031	17.021837
31.072353	1119.276059	17.026855
31.713027	1114.788362	17.031872
31.663331	1110.271070	17.036890
31.391476	1104.913064	17.041907
31.533772	1084.288910	17.046925
31.271459	1079.422372	17.051943
31.394193	1081.438594	17.056960
31.503118	1092.930079	17.061978
31.541475	1092.393704	17.066995
31.410685	1088.298420	17.072013
31.657601	1091.397499	17.077031
31.791451	1087.387598	17.082048
31.690576	1080.902298	17.087066
31.270639	1067.739648	17.092083
31.737712	1084.888593	17.097101
31.424375	1093.723302	17.102119
31.389167	1096.513151	17.107136
31.536816	1094.493582	17.112154
31.579987	1100.657569	17.117171
31.507465	1092.559947	17.122189
31.446225	1103.624707	17.127207
31.612026	1101.454128	17.132224
31.813048	1096.168746	17.137242
31.581201	1115.746458	17.142259
32.164945	1119.916683	17.147277
32.148497	1116.863559	17.152295
32.006775	1119.473012	17.157312
32.438053	1130.113737	17.162330
31.990930	1119.338056	17.167347
32.235704	1111.690081	17.172365
32.034438	1117.372302	17.177383
32.130375	1124.371942	17.182400
32.278043	1115.962963	17.187418
32.124238	1120.976417	17.192435
32.471825	1108.305704	17.197453
32.483600	1118.785070	17.202471
32.348386	1114.395277	17.207488
32.619065	1119.657042	17.212506
32.218457	1110.600195	17.217523
32.361891	1097.475504	17.222541
32.340639	1102.972878	17.227559
32.338345	1109.961780	17.232576
32.455717	1118.515517	17.237594
32.440446	1125.446342	17.242611
32.444224	1116.238428	17.247629
32.354548	1125.225929	17.252647
32.353002	1111.044637	17.257664
32.622722	1118.713877	17.262682
32.352713	1123.914227	17.267699
32.580022	1112.832838	17.272717
32.460724	1118.359016	17.277735
32.408825	1134.671474	17.282752
32.642347	1140.892986	17.287770
32.744484	1139.451319	17.292787
33.118740	1134.081401	17.297805
33.277213	1148.105112	17.302823
33.252042	1145.229381	17.307840
33.357022	1140.117707	17.312858
33.100649	1137.059744	17.317875
33.096624	1116.775625	17.322893
33.075465	1123.405893	17.327911
32.907366	1128.448873	17.332928
33.257393	1138.798942	17.337946
33.105788	1136.342670	17.342963
33.301489	1131.807651	17.347981
33.414204	1136.922717	17.352999
33.092414	1130.888408	17.358016
33.508759	1142.531462	17.363034
33.109954	1146.005132	17.368051
33.281904	1145.970814	17.373069
33.122702	1140.714241	17.378087
33.346427	1131.883885	17.383104
33.638138	1136.132684	17.388122
33.212271	1150.394081	17.393139
33.362147	1137.687127	17.398157
33.210706	1142.935006	17.403175
33.334434	1143.129491	17.408192
33.732402	1141.908780	17.413210
33.432542	1164.029506	17.418227
33.621680	1159.897277	17.423245
33.915044	1161.642829	17.428263
33.825691	1160.279255	17.433280
34.033069	1164.132411	17.438298
33.783081	1165.711294	17.443315
33.889016	1155.654903	17.448333
34.411361	1148.545798	17.453351
34.209082	1158.304572	17.458368
34.426449	1147.977446	17.463386
34.228446	1141.079298	17.468403
34.274265	1127.330256	17.473421
34.139432	1122.997280	17.478439
33.955783	1128.382150	17.483456
34.014038	1120.914971	17.488474
34.085350	1139.464809	17.493491
34.336293	1144.419850	17.498509
34.064687	1145.992659	17.503527
34.188942	1155.886027	17.508544
34.332197	1153.212350	17.513562
34.361214	1155.697546	17.518579
34.206638	1152.971132	17.523597
34.500004	1148.035577	17.528615
34.183318	1146.351946	17.533632
34.506499	1145.856284	17.538650
34.285506	1153.117925	17.543667
34.488283	1150.268295	17.548685
34.617866	1151.452808	17.553703
34.338769	1150.381772	17.558720
34.389111	1152.997282	17.563738
33.979776	1153.657359	17.568755
34.551834	1162.824072	17.573773
34.588712	1171.845207	17.578791
34.566524	1178.125523	17.583808
34.838556	1173.073424	17.588826
35.171865	1179.180641	17.593843
35.035774	1176.753487	17.598861
35.250051	1175.562341	17.603879
35.381022	1170.510722	17.608896
35.505126	1165.368915	17.613914
35.055854	1151.158043	17.618931
34.925045	1139.136551	17.623949
35.040166	1148.240005	17.628967
35.064081	1169.586475	17.633984
35.327444	1168.129973	17.639002
35.297365	1170.780426	17.644019
35.316345	1168.118820	17.649037
35.442455	1163.435473	17.654055
35.367349	1171.334925	17.659072
35.139894	1169.303720	17.664090
35.155446	1176.605405	17.669107
35.493210	1174.372939	17.674125
35.465335	1161.599487	17.679143
35.391514	1175.185891	17.684160
35.555538	1169.034482	17.689178
35.280055	1172.344886	17.694195
35.595249	1172.823433	17.699213
35.431738	1175.046987	17.704231
35.296681	1172.323249	17.709248
35.712854	1168.969326	17.714266
35.573913	1166.406640	17.719283
35.516673	1168.228632	17.724301
35.496919	1174.637265	17.729319
35.567292	1196.519324	17.734336
35.633310	1189.694634	17.739354
36.003281	1199.414570	17.744371
36.096553	1194.234153	17.749389
36.227641	1193.776926	17.754407
36.044231	1188.618810	17.759424
36.314203	1189.236899	17.764442
36.136719	1192.274064	17.769459
36.112091	1205.430970	17.774477
36.483366	1195.047281	17.779495
36.295815	1197.117352	17.784512
36.522245	1184.513835	17.789530
35.943064	1199.516256	17.794547
35.853199	1196.064677	17.799565
36.112686	1196.029474	17.804583
36.238441	1192.520614	17.809600
36.413597	1193.676344	17.814618
36.180947	1197.286718	17.819635
36.321222	1198.493480	17.824653
36.603931	1187.446773	17.829671
36.472178	1189.258053	17.834688
36.755212	1192.986920	17.839706
36.544015	1195.578934	17.844723
36.646036	1193.999703	17.849741
36.823273	1198.362895	17.854759
36.536332	1199.629823	17.859776
37.012474	1205.287131	17.864794
36.667220	1216.347535	17.869811
36.684798	1218.989530	17.874829
37.292857	1221.968337	17.879847
36.899414	1225.573403	17.884864
37.114700	1211.406770	17.889882
36.572260	1218.765058	17.894899
36.844511	1220.701087	17.899917
36.859607	1216.926887	17.904935
36.894401	1218.291810	17.909952
36.988962	1213.703609	17.914970
37.021666	1211.238518	17.919987
36.968633	1214.319089	17.925005
37.225041	1213.227262	17.930023
37.307135	1221.167486	17.935040
37.196702	1211.983111	17.940058
37.342479	1204.856496	17.945075
37.088633	1206.867455	17.950093
37.367154	1202.484650	17.955111
36.967455	1213.978595	17.960128
37.275850	1227.626670	17.965146
37.447385	1234.904575	17.970163
37.496711	1233.336016	17.975181
37.699072	1227.305396	17.980199
37.365469	1237.566561	17.985216
37.380139	1235.073742	17.990234
37.525862	1230.890803	17.995251
37.602789	1225.986659	18.000269
37.743115	1228.072622	18.005287
37.540990	1229.959108	18.010304
37.843926	1253.469707	18.015322
38.658889	1255.613655	18.020339
38.020258	1231.232085	18.025357
38.397991	1219.021194	18.030375
38.110811	1221.917656	18.035392
38.485270	1223.255776	18.040410
38.213226	1219.757536	18.045427
38.533240	1225.028112	18.050445
38.473582	1214.609337	18.055463
38.368239	1212.343608	18.060480
38.419357	1208.376869	18.065498
38.434364	1216.188040	18.070515
38.452637	1227.317691	18.075533
38.326536	1217.700924	18.080551
38.445268	1213.385264	18.085568
38.729536	1211.749934	18.090586
38.494743	1214.467880	18.095603
38.250977	1214.879568	18.100621
38.502787	1214.395698	18.105639
38.500923	1219.461231	18.110656
38.223855	1219.122230	18.115674
38.101342	1210.747808	18.120691
38.120246	1221.240040	18.125709
39.008835	1229.831727	18.130727
38.564772	1245.243890	18.135744
38.482599	1247.311119	18.140762
38.606335	1244.956159	18.145779
38.487682	1257.767871	18.150797
38.794707	1244.233595	18.155815
38.595588	1240.926223	18.160832
38.645307	1244.169126	18.165850
38.982346	1255.451014	18.170867
38.991433	1263.325186	18.175885
39.481813	1276.046703	18.180903
39.544123	1277.706255	18.185920
39.342521	1257.486485	18.190938
39.393704	1241.336199	18.195955
39.183424	1244.124105	18.200973
39.378128	1240.474922	18.205991
39.271284	1250.977325	18.211008
39.258347	1263.914664	18.216026
39.621626	1265.974811	18.221043
39.353510	1273.379709	18.226061
39.670264	1265.781763	18.231079
39.534014	1269.313831	18.236096
39.570371	1261.314253	18.241114
39.842060	1266.972107	18.246131
39.392969	1277.276592	18.251149
39.826450	1271.569523	18.256167
39.805589	1266.296737	18.261184
39.672740	1260.858823	18.266202
39.988267	1272.613702	18.271219
39.796355	1276.196302	18.276237
40.026583	1267.385461	18.281255
39.776600	1261.945843	18.286272
39.889970	1263.211774	18.291290
40.164916	1259.483193	18.296307
39.920839	1260.680060	18.301325
40.220979	1260.763319	18.306343
40.002025	1262.062122	18.311360
40.121302	1267.736895	18.316378
40.129782	1261.263366	18.321395
39.609107	1266.162911	18.326413
40.067962	1263.357546	18.331431
40.239798	1264.459703	18.336448
40.045084	1267.198984	18.341466
40.443655	1280.673566	18.346483
40.314755	1295.967763	18.351501
40.471215	1297.467094	18.356519
40.666608	1293.094262	18.361536
40.850747	1285.097609	18.366554
40.901590	1291.728452	18.371571
40.695683	1299.020340	18.376589
40.662002	1288.999136	18.381607
40.471083	1282.168642	18.386624
40.682689	1286.626953	18.391642
40.814278	1291.142183	18.396659
40.282031	1288.761580	18.401677
40.216904	1283.128634	18.406695
40.699125	1285.636781	18.411712
40.799242	1305.074653	18.416730
41.007867	1305.462562	18.421747
41.188121	1315.758534	18.426765
41.201104	1317.412071	18.431783
41.334445	1315.773132	18.436800
41.244619	1313.849068	18.441818
41.543009	1310.862563	18.446835
41.256361	1309.127498	18.451853
41.451676	1314.733235	18.456871
41.571169	1320.082643	18.461888
41.220481	1295.150504	18.466906
41.446139	1290.088514	18.471923
41.711348	1310.658597	18.476941
41.547722	1308.911077	18.481959
41.283094	1310.071978	18.486976
41.473614	1307.359170	18.491994
41.564285	1310.258160	18.497011
41.135993	1316.078153	18.502029
41.331235	1317.023318	18.507047
41.395654	1306.582206	18.512064
41.224499	1307.973100	18.517082
41.967165	1321.402075	18.522099
41.492812	1328.625952	18.527117
42.145981	1340.571708	18.532135
42.463247	1338.567970	18.537152
42.211791	1337.580135	18.542170
42.435991	1315.643886	18.547187
41.957965	1306.484377	18.552205
42.019912	1297.244894	18.557223
42.212990	1310.695200	18.562240
42.255565	1325.080895	18.567258
42.713400	1317.472601	18.572275
42.130747	1303.987666	18.577293
42.305302	1295.884732	18.582311
42.571131	1291.980903	18.587328
42.397629	1304.242544	18.592346
42.750811	1297.757110	18.597363
42.332750	1303.973188	18.602381
42.229551	1293.048240	18.607399
42.534564	1305.156014	18.612416
42.205951	1318.974191	18.617434
42.326754	1324.565280	18.622451
42.116688	1335.929566	18.627469
42.486215	1319.944673	18.632487
42.490660	1323.085050	18.637504
42.477854	1316.738817	18.642522
42.774305	1338.320959	18.647539
43.087532	1337.032163	18.652557
43.212718	1347.115829	18.657575
43.499410	1344.682554	18.662592
42.882845	1342.499513	18.667610
43.408629	1331.495202	18.672627
43.001560	1331.550858	18.677645
43.172406	1309.347881	18.682663
43.350554	1313.296052	18.687680
43.389828	1336.819448	18.692698
43.374995	1332.909436	18.697715
43.324738	1330.190355	18.702733
43.114316	1327.142474	18.707751
43.532683	1339.578347	18.712768
43.644315	1337.757388	18.717786
43.827566	1329.521522	18.722803
43.664930	1336.768291	18.727821
43.773982	1331.221293	18.732839
43.846356	1334.492553	18.737856
43.525031	1325.814746	18.742874
43.780845	1331.999192	18.747891
43.501661	1336.761425	18.752909
43.499759	1331.705139	18.757927
43.607923	1333.548236	18.762944
43.347813	1340.263354	18.767962
43.549066	1339.420561	18.772979
43.683454	1339.697331	18.777997
43.858984	1361.608699	18.783015
43.974615	1361.998594	18.788032
43.779021	1362.564310	18.793050
44.055999	1360.220029	18.798067
44.159799	1359.451206	18.803085
43.935408	1367.707471	18.808103
44.407890	1361.766985	18.813120
44.197204	1363.571449	18.818138
44.625368	1355.123860	18.823155
44.042008	1361.148998	18.828173
43.977159	1352.229411	18.833191
44.347130	1363.250066	18.838208
44.372128	1375.644293	18.843226
45.003358	1375.046547	18.848243
44.866549	1380.691248	18.853261
44.978902	1376.824963	18.858279
44.968550	1375.985054	18.863296
45.046502	1377.483392	18.868314
44.795341	1364.593736	18.873331
44.808904	1379.363950	18.878349
45.040562	1380.802838	18.883367
45.158903	1382.812544	18.888384
45.034369	1389.260233	18.893402
45.311855	1368.654888	18.898419
45.113089	1368.618453	18.903437
45.099970	1367.198567	18.908455
45.351872	1358.321700	18.913472
45.101181	1366.983438	18.918490
45.055750	1368.401193	18.923507
45.426563	1371.789067	18.928525
45.081321	1386.620549	18.933543
45.028959	1373.095948	18.938560
45.261018	1376.153256	18.943578
45.329298	1377.358940	18.948595
45.337382	1381.982586	18.953613
44.980560	1374.283718	18.958631
45.194200	1382.984468	18.963648
45.528004	1398.234191	18.968666
45.693840	1401.756719	18.973683
45.755337	1404.968776	18.978701
45.672832	1409.442855	18.983719
46.065887	1402.986807	18.988736
45.823331	1411.090409	18.993754
46.029961	1404.649815	18.998771
46.191622	1410.045035	19.003789
45.912598	1409.151306	19.008807
46.242759	1404.478649	19.013824
45.957500	1418.757210	19.018842
46.107388	1408.275728	19.023859
46.013714	1404.225202	19.028877
45.800853	1409.957669	19.033895
46.146149	1397.619141	19.038912
45.948701	1407.669165	19.043930
46.257535	1415.907608	19.048947
46.852953	1422.188314	19.053965
46.962329	1422.516850	19.058983
47.087809	1407.032569	19.064000
46.939515	1396.677130	19.069018
46.655920	1403.663247	19.074035
46.715322	1391.920124	19.079053
46.711381	1387.727429	19.084071
46.883788	1380.977581	19.089088
46.747232	1380.511039	19.094106
46.757681	1390.776271	19.099123
46.686805	1389.079745	19.104141
46.523427	1409.214551	19.109159
46.946953	1416.708742	19.114176
46.943040	1427.106079	19.119194
46.945900	1425.012768	19.124211
47.056289	1409.174528	19.129229
46.868386	1419.393630	19.134247
47.079313	1422.347957	19.139264
46.563964	1428.685463	19.144282
46.878591	1445.005587	19.149299
47.441399	1445.673119	19.154317
47.377886	1449.041849	19.159335
47.485553	1447.824212	19.164352
47.712609	1447.971118	19.169370
47.202483	1447.664718	19.174387
47.739145	1447.871276	19.179405
47.738433	1445.465403	19.184423
47.916768	1443.730444	19.189440
47.858250	1440.166753	19.194458
47.883206	1445.945553	19.199475
48.088756	1442.735813	19.204493
48.042478	1445.436622	19.209511
48.174785	1439.967031	19.214528
48.181415	1440.113752	19.219546
48.207144	1442.813487	19.224563
48.514138	1441.122614	19.229581
48.239191	1435.953363	19.234599
48.693508	1434.972107	19.239616
48.071424	1449.074102	19.244634
48.317427	1440.235362	19.249651
48.675768	1435.176002	19.254669
48.083159	1432.291440	19.259687
47.941018	1424.381895	19.264704
48.128607	1432.482135	19.269722
47.961538	1448.664962	19.274739
48.411583	1439.204785	19.279757
47.924215	1445.127884	19.284775
48.698258	1444.141424	19.289792
48.230838	1451.327012	19.294810
48.582202	1455.566831	19.299827
48.948344	1451.730430	19.304845
48.842819	1463.406430	19.309863
48.958658	1456.488754	19.314880
48.984512	1455.818229	19.319898
49.284156	1453.178493	19.324915
49.473104	1445.226036	19.329933
49.186006	1450.514151	19.334951
48.863347	1453.384436	19.339968
49.039118	1452.673785	19.344986
49.240727	1452.573157	19.350003
49.019033	1455.779666	19.355021
49.085315	1453.334378	19.360039
49.354944	1444.006951	19.365056
49.186540	1448.216728	19.370074
49.442317	1442.383470	19.375091
49.539236	1446.001244	19.380109
49.328187	1459.796183	19.385127
49.639479	1475.451227	19.390144
49.880081	1468.756205	19.395162
49.858580	1480.991294	19.400179
49.955653	1478.015389	19.405197
49.858073	1479.243174	19.410215
49.987229	1483.002265	19.415232
50.089831	1485.009272	19.420250
49.790054	1482.787835	19.425267
50.427012	1481.495525	19.430285
50.159740	1490.456885	19.435303
50.197013	1481.709890	19.440320
50.145600	1470.242664	19.445338
50.034819	1481.610924	19.450355
50.276261	1473.008717	19.455373
50.121653	1487.166354	19.460391
50.240553	1492.469863	19.465408
50.418892	1489.778521	19.470426
50.198425	1474.582216	19.475443
50.685199	1465.145478	19.480461
50.114740	1479.263769	19.485479
50.223304	1483.369526	19.490496
50.318163	1480.567588	19.495514
50.566662	1493.080075	19.500531
50.812612	1496.097125	19.505549
50.618748	1502.299066	19.510567
51.010555	1502.205389	19.515584
50.966377	1498.224012	19.520602
51.036616	1497.738056	19.525619
50.830002	1505.127194	19.530637
50.888999	1498.453509	19.535655
51.014635	1501.186148	19.540672
50.692844	1502.097880	19.545690
51.052425	1517.434002	19.550707
51.320631	1512.494617	19.555725
51.130255	1527.089447	19.560743
51.493579	1535.482316	19.565760
51.497216	1519.171309	19.570778
51.424587	1536.349915	19.575795
51.736150	1530.289321	19.580813
51.268221	1530.600477	19.585831
51.371440	1525.312216	19.590848
51.529909	1519.647549	19.595866
51.669110	1532.681218	19.600883
51.645235	1516.387554	19.605901
51.472515	1528.404195	19.610919
51.538372	1522.469038	19.615936
51.967018	1526.044021	19.620954
52.095119	1542.218322	19.625971
52.154104	1540.970341	19.630989
51.995367	1532.436985	19.636007
52.033904	1548.492644	19.641024
52.398634	1546.489697	19.646042
51.976421	1556.732650	19.651059
52.486102	1542.496988	19.656077
52.162188	1546.622266	19.661095
52.330081	1546.402225	19.666112
52.500134	1542.273835	19.671130
52.307967	1550.354617	19.676147
52.908071	1544.480758	19.681165
52.757064	1550.633909	19.686183
52.659406	1537.345755	19.691200
52.748100	1541.661283	19.696218
52.559127	1552.536278	19.701235
52.553090	1541.977138	19.706253
53.006791	1534.312341	19.711271
52.790342	1548.647950	19.716288
52.959871	1534.817478	19.721306
52.522403	1539.544716	19.726323
52.915866	1543.947464	19.731341
53.236319	1563.546867	19.736359
52.984259	1572.991726	19.741376
53.662295	1563.236153	19.746394
53.496199	1570.301735	19.751411
53.395506	1556.523180	19.756429
53.292847	1563.854031	19.761447
53.322918	1563.792574	19.766464
53.647646	1567.372535	19.771482
53.318662	1571.541566	19.776499
53.617905	1562.205238	19.781517
53.564804	1562.836381	19.786535
53.691288	1563.968493	19.791552
53.942603	1558.545131	19.796570
53.603972	1563.653043	19.801587
53.588121	1562.554418	19.806605
53.771371	1556.882099	19.811623
53.754393	1564.171433	19.816640
53.708144	1564.918162	19.821658
53.790445	1589.733695	19.826675
54.020740	1587.531920	19.831693
54.195228	1589.408571	19.836711
54.586333	1584.348866	19.841728
55.063757	1572.239910	19.846746
54.972834	1576.736686	19.851763
54.846487	1555.066659	19.856781
54.847596	1535.269662	19.861799
54.660438	1530.032138	19.866816
55.017290	1527.250472	19.871834
54.856102	1534.513235	19.876851
54.946456	1531.860044	19.881869
54.796638	1536.845813	19.886887
54.735945	1534.028432	19.891904
55.128929	1530.576899	19.896922
55.078240	1537.094720	19.901939
54.851085	1541.247113	19.906957
54.902613	1540.165699	19.911975
54.930814	1546.437248	19.916992
55.113622	1541.436383	19.922010
54.873738	1534.019254	19.927027
54.998843	1536.605549	19.932045
55.183148	1545.559634	19.937063
55.287457	1556.435179	19.942080
55.521232	1565.822387	19.947098
55.358195	1561.571496	19.952115
55.651597	1558.864278	19.957133
55.484278	1563.328010	19.962151
55.063115	1565.606004	19.967168
55.487796	1566.931922	19.972186
55.521260	1571.910050	19.977203
55.294123	1564.264449	19.982221
55.172717	1565.643208	19.987239
55.693798	1586.951996	19.992256
56.027916	1583.310990	19.997274
55.886500	1597.194140	20.002291
56.055132	1587.908313	20.007309
56.267136	1590.202927	20.012327
56.099657	1591.727672	20.017344
55.974053	1584.834089	20.022362
56.080320	1589.881285	20.027379
55.878197	1596.501115	20.032397
56.258556	1601.684300	20.037415
56.022228	1597.148695	20.042432
56.425062	1612.175242	20.047450
56.600519	1613.861404	20.052467
56.541688	1622.535671	20.057485
56.845429	1621.026988	20.062503
56.619290	1629.042764	20.067520
57.051954	1614.144251	20.072538
56.652824	1615.160884	20.077555
56.418884	1613.366096	20.082573
56.569562	1601.066258	20.087591
56.717285	1612.963484	20.092608
56.883965	1618.088098	20.097626
56.832387	1643.765705	20.102643
56.704198	1640.469553	20.107661
56.807271	1643.995423	20.112679
57.151061	1641.607189	20.117696
57.276407	1646.376873	20.122714
57.235656	1654.696242	20.127731
57.268960	1628.106982	20.132749
57.558687	1646.876823	20.137767
57.674837	1662.717241	20.142784
57.588838	1655.298834	20.147802
57.768961	1661.685861	20.152819
57.983222	1666.927614	20.157837
57.950248	1658.053954	20.162855
57.916836	1657.480212	20.167872
58.281644	1648.061156	20.172890
58.146807	1657.700452	20.177907
58.042060	1654.511435	20.182925
58.226237	1655.712161	20.187943
58.236108	1653.176371	20.192960
58.281032	1646.515379	20.197978
58.206734	1648.087716	20.202995
58.379502	1645.897998	20.208013
58.686433	1648.466075	20.213031
58.266068	1660.022223	20.218048
58.542349	1654.952732	20.223066
58.597477	1651.282034	20.228083
58.707837	1651.721424	20.233101
58.721047	1646.670607	20.238119
58.373781	1653.713809	20.243136
58.476117	1646.269599	20.248154
58.287173	1645.958736	20.253171
58.218711	1645.367955	20.258189
58.514221	1655.698647	20.263207
58.424547	1677.068136	20.268224
58.874776	1675.961178	20.273242
58.866183	1684.859632	20.278259
58.776193	1684.758769	20.283277
59.289723	1693.350698	20.288295
59.418173	1702.326898	20.293312
59.818197	1696.176434	20.298330
59.537224	1686.432226	20.303347
59.371148	1679.463408	20.308365
59.335214	1671.894216	20.313383
59.422000	1678.150824	20.318400
59.696448	1697.811145	20.323418
59.568118	1703.315012	20.328435
59.515126	1698.369005	20.333453
59.808667	1691.963530	20.338471
59.558342	1688.586972	20.343488
59.492998	1700.448813	20.348506
59.700705	1702.262712	20.353523
59.785081	1712.489765	20.358541
60.194861	1724.641182	20.363559
60.310033	1730.197134	20.368576
60.436902	1725.983321	20.373594
60.786570	1721.061508	20.378611
60.451387	1727.603982	20.383629
60.728396	1728.435475	20.388647
60.323369	1724.695145	20.393664
60.813092	1725.469246	20.398682
60.726937	1715.420415	20.403699
60.979872	1719.010899	20.408717
60.885888	1704.601643	20.413735
60.576305	1706.710055	20.418752
60.817196	1712.323956	20.423770
61.040932	1714.985508	20.428787
61.202996	1721.701690	20.433805
61.324041	1706.908512	20.438823
60.904179	1724.053181	20.443840
60.754661	1709.808396	20.448858
61.062759	1715.704664	20.453875
60.987074	1727.964452	20.458893
61.177183	1718.909618	20.463911
61.048741	1724.898890	20.468928
61.321400	1719.281809	20.473946
61.288819	1723.809140	20.478963
61.353670	1736.899949	20.483981
61.668976	1737.285005	20.488999
61.431310	1745.578504	20.494016
61.309510	1747.548225	20.499034
61.536269	1741.494870	20.504051
61.484516	1741.351472	20.509069
61.777733	1748.165074	20.514087
61.854269	1769.954225	20.519104
62.223535	1776.380706	20.524122
62.456789	1778.937558	20.529139
61.967509	1778.469060	20.534157
62.070127	1766.783856	20.539175
62.163635	1775.263762	20.544192
62.025085	1772.709373	20.549210
62.306136	1769.011155	20.554227
62.231076	1771.735870	20.559245
62.471016	1788.020479	20.564263
62.596194	1784.779269	20.569280
62.580061	1792.696457	20.574298
62.851961	1789.822298	20.579315
62.495964	1797.039037	20.584333
62.774633	1790.270467	20.589351
62.698851	1782.954039	20.594368
62.962978	1778.179990	20.599386
63.067111	1784.241669	20.604403
62.773676	1791.460664	20.609421
63.132260	1798.486298	20.614439
63.415877	1809.036162	20.619456
63.761487	1815.044369	20.624474
63.791964	1790.831034	20.629491
63.313747	1786.637674	20.634509
63.676700	1774.002258	20.639527
63.759247	1768.235294	20.644544
63.747797	1774.146992	20.649562
63.611530	1767.813888	20.654579
63.543660	1771.093851	20.659597
63.758797	1772.473900	20.664615
63.774187	1797.522259	20.669632
63.657325	1806.004073	20.674650
63.934552	1806.196428	20.679667
63.666257	1809.678596	20.684685
64.148592	1806.391354	20.689703
63.996678	1800.543252	20.694720
63.601666	1810.881670	20.699738
63.896739	1816.798829	20.704755
64.140428	1833.133255	20.709773
64.486882	1827.368324	20.714791
64.356088	1832.145947	20.719808
64.444992	1833.289603	20.724826
64.642730	1831.130376	20.729843
64.289355	1837.868403	20.734861
64.621790	1839.346779	20.739879
64.544154	1842.155388	20.744896
64.717705	1858.194374	20.749914
65.565468	1856.969357	20.754931
65.658157	1846.017354	20.759949
65.868184	1830.331491	20.764967
65.537689	1810.350181	20.769984
65.583354	1813.068141	20.775002
65.779016	1795.288448	20.780019
65.768664	1800.490798	20.785037
65.805625	1802.716545	20.790055
65.810533	1805.155835	20.795072
65.710746	1809.397084	20.800090
66.027427	1809.936820	20.805107
65.624062	1808.113121	20.810125
65.539629	1799.586823	20.815143
65.573417	1811.393200	20.820160
65.346564	1818.564988	20.825178
65.552775	1809.614516	20.830195
65.653276	1816.727486	20.835213
65.881802	1813.095412	20.840231
65.875601	1834.275162	20.845248
65.725133	1844.047459	20.850266
66.065647	1841.243834	20.855283
65.998631	1844.182958	20.860301
66.169930	1837.233902	20.865319
66.326095	1846.215645	20.870336
66.139692	1864.309586	20.875354
66.548495	1870.331583	20.880371
66.486206	1873.743112	20.885389
66.591657	1875.266480	20.890407
66.355442	1876.261325	20.895424
66.940761	1871.233995	20.900442
66.911953	1870.678577	20.905459
66.755768	1885.613140	20.910477
66.898518	1900.607759	20.915495
67.111862	1897.394472	20.920512
67.047613	1898.685673	20.925530
67.483215	1897.827157	20.930547
67.435792	1900.663851	20.935565
67.452942	1899.505817	20.940583
67.269646	1901.756165	20.945600
67.272105	1899.316630	20.950618
67.537917	1893.272509	20.955635
67.598738	1891.797054	20.960653
67.720756	1886.351444	20.965671
67.560287	1893.779397	20.970688
67.568096	1896.912052	20.975706
68.263538	1901.911201	20.980723
68.100946	1910.326227	20.985741
68.201766	1901.052993	20.990759
68.203557	1894.536803	20.995776
68.054510	1909.151343	21.000794
68.133395	1911.481782	21.005811
68.137224	1926.690702	21.010829
68.334335	1911.810357	21.015847
68.189603	1903.981891	21.020864
68.249252	1914.142501	21.025882
68.338407	1912.682045	21.030899
68.371674	1924.641926	21.035917
68.500805	1931.643339	21.040935
68.894335	1940.774085	21.045952
68.790556	1948.196633	21.050970
68.816640	1944.636166	21.055987
68.730270	1952.086742	21.061005
69.084791	1950.018312	21.066023
68.873659	1951.494994	21.071040
68.850106	1957.611696	21.076058
68.751800	1942.108941	21.081075
69.073533	1949.637735	21.086093
69.391195	1960.472011	21.091111
69.549844	1960.287938	21.096128
69.450695	1979.145867	21.101146
69.603466	1963.372490	21.106163
70.023883	1967.716385	21.111181
69.867252	1969.006718	21.116199
69.938596	1962.404210	21.121216
69.575706	1973.042517	21.126234
70.193523	1957.922348	21.131251
70.389500	1954.625707	21.136269
70.087957	1949.933072	21.141287
70.369686	1956.362679	21.146304
70.116221	1958.991131	21.151322
70.381722	1955.015938	21.156339
70.367506	1963.208659	21.161357
70.631446	1981.322603	21.166375
70.515023	1977.996877	21.171392
70.514143	1994.932860	21.176410
71.137282	1993.704208	21.181427
70.776058	1986.545471	21.186445
70.591354	1981.697312	21.191463
70.871610	1978.271395	21.196480
70.857652	1991.798829	21.201498
70.929651	1976.887329	21.206515
71.101777	1985.870453	21.211533
70.969168	1993.391676	21.216551
71.010352	1979.996346	21.221568
71.201839	1985.094151	21.226586
71.483001	1986.023192	21.231603
71.572139	1996.997610	21.236621
71.691019	2007.127826	21.241639
71.614510	2001.542753	21.246656
71.694057	2007.324947	21.251674
71.827432	1996.765093	21.256691
72.167162	1987.851898	21.261709
71.583938	2003.703126	21.266727
72.031562	1998.008612	21.271744
71.710165	2003.670264	21.276762
71.919256	2003.410539	21.281779
72.264713	1998.225775	21.286797
72.066432	1996.769111	21.291815
72.167128	1995.639583	21.296832
72.094133	2007.634409	21.301850
72.180657	2025.751150	21.306867
72.472497	2030.863684	21.311885
72.095410	2032.464639	21.316903
72.482715	2023.999820	21.321920
72.161719	2037.642591	21.326938
72.288094	2027.827704	21.331955
72.415550	2046.278226	21.336973
72.893695	2043.970871	21.341991
72.750830	2045.076865	21.347008
72.726516	2059.344980	21.352026
72.870345	2049.806698	21.357043
73.222160	2047.716854	21.362061
73.045027	2074.659516	21.367079
73.548451	2076.044313	21.372096
73.362488	2083.279933	21.377114
73.517856	2076.301122	21.382131
73.637691	2087.849418	21.387149
73.766610	2095.814834	21.392167
74.041678	2067.809196	21.397184
73.677747	2082.237774	21.402202
73.992132	2082.463164	21.407219
73.959440	2088.746571	21.412237
73.425842	2091.112701	21.417255
73.820385	2086.319763	21.422272
74.110660	2087.446894	21.427290
74.200161	2099.781837	21.432307
74.375178	2103.436267	21.437325
74.374646	2106.800638	21.442343
74.216743	2105.559714	21.447360
74.043451	2122.861306	21.452378
73.888053	2111.462355	21.457395
74.648631	2116.428964	21.462413
74.710231	2129.683819	21.467431
74.938734	2127.694846	21.472448
74.879360	2133.685068	21.477466
75.269794	2137.031490	21.482483
75.285926	2141.235172	21.487501
75.259814	2139.456761	21.492519
75.408544	2121.224251	21.497536
74.935737	2124.369644	21.502554
75.662806	2130.487762	21.507571
75.530781	2124.392176	21.512589
75.466228	2131.229245	21.517607
75.172200	2138.359726	21.522624
75.472385	2137.516882	21.527642
75.874653	2148.068829	21.532659
76.063554	2147.867945	21.537677
75.826532	2147.519743	21.542695
76.108275	2149.172262	21.547712
75.863569	2158.875690	21.552730
75.891096	2162.993840	21.557747
76.211269	2152.228618	21.562765
76.029734	2157.839658	21.567783
76.198457	2155.444649	21.572800
76.287699	2179.626966	21.577818
76.454118	2186.132215	21.582835
76.761535	2176.563280	21.587853
76.704074	2181.880227	21.592871
76.984115	2175.295894	21.597888
77.040766	2179.188781	21.602906
76.774222	2171.396251	21.607923
76.895864	2174.483186	21.612941
76.901580	2180.789612	21.617959
77.067082	2183.593732	21.622976
77.309917	2180.892796	21.627994
77.197625	2179.891158	21.633011
77.621763	2178.946144	21.638029
77.422581	2168.344677	21.643047
77.633303	2166.897964	21.648064
77.428664	2177.608088	21.653082
77.642138	2190.761528	21.658099
78.150064	2190.119375	21.663117
78.101398	2187.518570	21.668135
77.860079	2171.726249	21.673152
77.952176	2186.493511	21.678170
77.785873	2196.065316	21.683187
78.210306	2188.947709	21.688205
77.963485	2198.989281	21.693223
77.900109	2187.180217	21.698240
78.015722	2196.223389	21.703258
77.793360	2191.792574	21.708275
78.700193	2207.426723	21.713293
78.344730	2216.963858	21.718311
79.061650	2206.350345	21.723328
79.193258	2209.929105	21.728346
79.280370	2208.074108	21.733363
78.955723	2202.413439	21.738381
78.951806	2202.635527	21.743399
79.003253	2212.824656	21.748416
79.167600	2220.880732	21.753434
79.091113	2214.620630	21.758451
79.351564	2210.047238	21.763469
79.381223	2208.391286	21.768487
79.555787	2210.513062	21.773504
79.516187	2204.037043	21.778522
79.245311	2209.799271	21.783539
79.724825	2201.312427	21.788557
79.685942	2203.293305	21.793575
79.605812	2209.550744	21.798592
79.693234	2229.496370	21.803610
79.661928	2231.449821	21.808627
79.882229	2223.128426	21.813645
79.744592	2243.665744	21.818663
79.663828	2233.704063	21.823680
80.089802	2256.710079	21.828698
80.432811	2257.488574	21.833715
80.428290	2263.080047	21.838733
80.786077	2268.826991	21.843751
80.661544	2262.190586	21.848768
80.853963	2263.667734	21.853786
80.670456	2260.488653	21.858803
80.920686	2252.634308	21.863821
80.941547	2261.126683	21.868839
81.143387	2269.327365	21.873856
81.534594	2279.796591	21.878874
81.076118	2278.699998	21.883891
81.073379	2277.137968	21.888909
81.441701	2276.788349	21.893927
81.183791	2281.352093	21.898944
81.644341	2286.017771	21.903962
81.539609	2280.555952	21.908979
81.558547	2273.193130	21.913997
81.638857	2275.917848	21.919015
81.718385	2280.464215	21.924032
82.135323	2295.217469	21.929050
82.027357	2312.153779	21.934067
82.446657	2302.013563	21.939085
82.347282	2294.797831	21.944103
82.170288	2307.199810	21.949120
82.407600	2301.105521	21.954138
82.416945	2306.050079	21.959155
82.455066	2308.116468	21.964173
82.497939	2304.573024	21.969191
82.230794	2308.492482	21.974208
82.606890	2304.640451	21.979226
82.692092	2315.544097	21.984243
83.014657	2315.172710	21.989261
83.197754	2319.961208	21.994279
83.055928	2330.932102	21.999296
83.265526	2320.701337	22.004314
82.832400	2338.135470	22.009331
82.839043	2330.311889	22.014349
83.441685	2331.258889	22.019367
83.282745	2317.894170	22.024384
83.301436	2319.812009	22.029402
83.012530	2333.159208	22.034419
83.462685	2344.037605	22.039437
83.368665	2351.614038	22.044455
83.623948	2351.380924	22.049472
83.877380	2344.409999	22.054490
83.540750	2354.027959	22.059507
83.985257	2362.013407	22.064525
84.186855	2369.631151	22.069543
83.921056	2365.463549	22.074560
84.466833	2359.995385	22.079578
84.252245	2374.950306	22.084595
84.434339	2371.716497	22.089613
84.478299	2388.159708	22.094631
84.319840	2397.289622	22.099648
84.918886	2396.695393	22.104666
84.775931	2404.284662	22.109683
85.004361	2402.746622	22.114701
85.208983	2390.195132	22.119719
85.159863	2394.960613	22.124736
85.312897	2399.487980	22.129754
85.419240	2412.085924	22.134771
85.365753	2416.786192	22.139789
85.911789	2419.204859	22.144807
85.567069	2423.258023	22.149824
85.870395	2410.048910	22.154842
85.509277	2421.449976	22.159859
85.829794	2414.964359	22.164877
85.653789	2421.726080	22.169895
85.614737	2422.051806	22.174912
85.928016	2424.624675	22.179930
85.817731	2432.344771	22.184947
86.369992	2439.650292	22.189965
86.456246	2454.690216	22.194983
86.327874	2458.317112	22.200000
86.633123	2441.244114	22.205018
86.703165	2440.759737	22.210035
86.625569	2438.718753	22.215053
86.820257	2439.950284	22.220071
86.646355	2453.068359	22.225088
86.868852	2457.341170	22.230106
87.027971	2466.333613	22.235123
87.389371	2467.582478	22.240141
87.379803	2469.686294	22.245159
87.263658	2471.966766	22.250176
87.350043	2462.310959	22.255194
87.383699	2473.371257	22.260211
87.202293	2473.679170	22.265229
87.583748	2473.813371	22.270247
87.613562	2487.512736	22.275264
87.937415	2487.113969	22.280282
88.011304	2500.528126	22.285299
87.781314	2498.088719	22.290317
88.445907	2498.417459	22.295335
88.054646	2498.850201	22.300352
88.289022	2503.263180	22.305370
88.164068	2492.165197	22.310387
88.036318	2494.848355	22.315405
88.451083	2512.281543	22.320423
88.472997	2522.361590	22.325440
89.055618	2508.496829	22.330458
88.738723	2520.649670	22.335475
88.639730	2524.303221	22.340493
88.636835	2520.431484	22.345511
88.581964	2523.408885	22.350528
88.926714	2516.167296	22.355546
89.022594	2535.394835	22.360563
89.233910	2542.933112	22.365581
89.056016	2548.733838	22.370599
88.990801	2557.521685	22.375616
89.440842	2548.871421	22.380634
89.625660	2569.198811	22.385651
89.836168	2570.326563	22.390669
89.820405	2568.771774	22.395687
90.062000	2568.931843	22.400704
90.241644	2560.192009	22.405722
90.406944	2570.959773	22.410739
90.070565	2571.905860	22.415757
90.673757	2556.470420	22.420775
90.096751	2565.666051	22.425792
90.441971	2558.671202	22.430810
90.455770	2566.092923	22.435827
90.551352	2569.548594	22.440845
90.863624	2575.569499	22.445863
90.545511	2597.198468	22.450880
91.051019	2591.690424	22.455898
90.824297	2590.338593	22.460915
91.052050	2599.702037	22.465933
90.961549	2586.350381	22.470951
91.108237	2601.138348	22.475968
91.326233	2600.786597	22.480986
91.579570	2607.658154	22.486003
91.530895	2617.789688	22.491021
91.612316	2615.340535	22.496039
91.535946	2618.120336	22.501056
91.829596	2614.181071	22.506074
91.729743	2614.042856	22.511091
91.741069	2628.394185	22.516109
92.191815	2633.005688	22.521127
92.304867	2654.534752	22.526144
92.403926	2644.451561	22.531162
92.322725	2642.141868	22.536179
92.368547	2651.314550	22.541197
92.602138	2638.473835	22.546215
92.400295	2642.375105	22.551232
92.442435	2650.444513	22.556250
92.916035	2666.565464	22.561267
92.860816	2663.387737	22.566285
93.192017	2663.642838	22.571303
93.116655	2663.939137	22.576320
93.233647	2661.683695	22.581338
93.204798	2665.001688	22.586355
93.206717	2668.470890	22.591373
93.691343	2681.252794	22.596391
93.475436	2695.325606	22.601408
93.840018	2684.775699	22.606426
94.021571	2688.104204	22.611443
94.350162	2680.228232	22.616461
94.322044	2669.392848	22.621479
94.493884	2689.030447	22.626496
94.561808	2694.305198	22.631514
94.469164	2686.742517	22.636531
94.115965	2687.707531	22.641549
94.303331	2675.866109	22.646567
94.216669	2685.646108	22.651584
94.253649	2670.037988	22.656602
94.254610	2682.277403	22.661619
94.363194	2699.124813	22.666637
94.724367	2704.560943	22.671655
94.997143	2710.304583	22.676672
94.967790	2693.068892	22.681690
95.086092	2704.418897	22.686707
95.121190	2715.842892	22.691725
95.313308	2721.936857	22.696743
95.226051	2740.255190	22.701760
95.596700	2745.655126	22.706778
95.680608	2740.713130	22.711795
95.769801	2743.671492	22.716813
95.684974	2746.216897	22.721831
95.909167	2748.575812	22.726848
95.918198	2741.905713	22.731866
96.009026	2742.069832	22.736883
95.917409	2758.084284	22.741901
96.285127	2748.836515	22.746919
96.342092	2771.672986	22.751936
96.194489	2766.246818	22.756954
96.179612	2764.620606	22.761971
96.362805	2788.058264	22.766989
96.549602	2788.854531	22.772007
96.545737	2798.542183	22.777024
96.536589	2803.190362	22.782042
97.020451	2805.371738	22.787059
97.209795	2817.264001	22.792077
97.808849	2811.000688	22.797095
97.873335	2806.852008	22.802112
97.759029	2811.425837	22.807130
98.096197	2804.883766	22.812147
98.041417	2805.172729	22.817165
98.114171	2801.223857	22.822183
98.315320	2803.503127	22.827200
97.964798	2795.945998	22.832218
98.403150	2794.226782	22.837235
98.179342	2794.170462	22.842253
98.225556	2799.253175	22.847271
98.347441	2806.770139	22.852288
98.098786	2808.726114	22.857306
98.514169	2803.310838	22.862323
98.225931	2800.334179	22.867341
98.538567	2817.916080	22.872359
98.841677	2827.980175	22.877376
98.516832	2823.832833	22.882394
99.024014	2831.415666	22.887411
99.026055	2832.792050	22.892429
99.125065	2841.878106	22.897447
99.218069	2856.566138	22.902464
99.392535	2860.459611	22.907482
99.397840	2858.798953	22.912499
99.336919	2858.846815	22.917517
99.496151	2863.868749	22.922535
99.830699	2880.709726	22.927552
99.741638	2887.121074	22.932570
99.767306	2890.244681	22.937587
99.998397	2893.933142	22.942605
100.043565	2885.010236	22.947623
100.285736	2899.274461	22.952640
100.619735	2904.223043	22.957658
100.880804	2899.718243	22.962675
100.434043	2915.470292	22.967693
100.516878	2914.065706	22.972711
100.803198	2909.801998	22.977728
100.802640	2910.662300	22.982746
100.706779	2914.650060	22.987763
100.941007	2932.359217	22.992781
101.091256	2933.811905	22.997799
101.578013	2941.490683	23.002816
101.336033	2941.281071	23.007834
101.722663	2930.124617	23.012851
101.596260	2939.978664	23.017869
101.706922	2932.685409	23.022887
101.492633	2940.791436	23.027904
101.897687	2957.402349	23.032922
102.153547	2956.656944	23.037939
101.928864	2957.919626	23.042957
102.392810	2963.573899	23.047975
102.423811	2954.798565	23.052992
102.558095	2952.126063	23.058010
102.396450	2954.601914	23.063027
102.378491	2963.373521	23.068045
102.710619	2962.571420	23.073063
103.253631	2980.477634	23.078080
103.021035	2976.545710	23.083098
103.625768	2984.300682	23.088115
103.059975	2979.619900	23.093133
102.943350	2988.338535	23.098151
103.088972	2975.804983	23.103168
103.332261	2982.974029	23.108186
103.342005	2977.452104	23.113203
103.525044	2999.226769	23.118221
103.627799	3002.642770	23.123239
103.871466	3001.604503	23.128256
103.828916	3009.133383	23.133274
103.876981	3005.049172	23.138291
104.125424	3021.910043	23.143309
104.105585	3028.438748	23.148327
105.108750	3024.658906	23.153344
105.284018	3025.119698	23.158362
105.373796	3011.926857	23.163379
105.210371	3005.961107	23.168397
104.790060	2993.391925	23.173415
105.356416	2995.666388	23.178432
104.760007	3003.001359	23.183450
105.373048	3002.631959	23.188467
105.295588	3010.553999	23.193485
105.535071	3019.675609	23.198503
105.618790	3005.800721	23.203520
105.539627	3015.665120	23.208538
105.558533	3001.989523	23.213555
105.369740	3007.094601	23.218573
105.830589	3025.092001	23.223591
106.045026	3032.389850	23.228608
105.614128	3037.132197	23.233626
106.147360	3034.233921	23.238643
105.986054	3050.829467	23.243661
105.900247	3063.442961	23.248679
106.440254	3067.463482	23.253696
106.400599	3077.606031	23.258714
106.386837	3082.244032	23.263731
106.375831	3091.616519	23.268749
106.763112	3100.809422	23.273767
106.887672	3100.783329	23.278784
106.890715	3094.596342	23.283802
107.385508	3097.125160	23.288819
107.282656	3125.381757	23.293837
107.627902	3128.265994	23.298855
107.902574	3121.941594	23.303872
107.815761	3128.122753	23.308890
107.941604	3126.472857	23.313907
108.056616	3119.277219	23.318925
107.968765	3121.940899	23.323943
108.058957	3117.350101	23.328960
108.032555	3125.229905	23.333978
108.349597	3132.665569	23.338995
108.233060	3136.474128	23.344013
108.218869	3142.398021	23.349031
108.264259	3140.141350	23.354048
108.451134	3151.021699	23.359066
108.666388	3156.769499	23.364083
108.521189	3172.503079	23.369101
108.665238	3165.541594	23.374119
108.793909	3158.333445	23.379136
108.949321	3195.567818	23.384154
109.726073	3192.822579	23.389171
109.618161	3207.106747	23.394189
109.261184	3206.109450	23.399207
109.682869	3206.779527	23.404224
109.672751	3210.986262	23.409242
109.710459	3205.415935	23.414259
109.499786	3224.255226	23.419277
109.556498	3242.710597	23.424295
109.724035	3247.255699	23.429312
110.249479	3253.632981	23.434330
110.514600	3254.149011	23.439347
110.619603	3252.257666	23.444365
110.980108	3263.534596	23.449383
111.148839	3262.453578	23.454400
111.211424	3261.511358	23.459418
111.160006	3252.244755	23.464435
111.264631	3252.517229	23.469453
111.280603	3252.514985	23.474471
111.720663	3250.171431	23.479488
111.104909	3262.279352	23.484506
111.173888	3275.194997	23.489523
111.306533	3285.198188	23.494541
111.333833	3282.668898	23.499559
111.780616	3297.822508	23.504576
112.024195	3317.934480	23.509594
112.086247	3318.755325	23.514611
112.466740	3330.617974	23.519629
112.358910	3321.227187	23.524647
112.264146	3312.724793	23.529664
112.394153	3333.089408	23.534682
112.488776	3343.108762	23.539699
112.665735	3338.155532	23.544717
112.778849	3345.931687	23.549735
113.092019	3354.158645	23.554752
113.471288	3367.877816	23.559770
113.458564	3373.489352	23.564787
113.329649	3368.042955	23.569805
113.589642	3368.381884	23.574823
113.739449	3370.521692	23.579840
113.550595	3369.660383	23.584858
113.703105	3369.931640	23.589875
114.281979	3389.881216	23.594893
114.329536	3391.345011	23.599911
114.295034	3392.721577	23.604928
114.175528	3399.748402	23.609946
114.503704	3391.288283	23.614963
115.099119	3388.088725	23.619981
114.675883	3394.868886	23.624999
115.130990	3377.694115	23.630016
114.945450	3376.581471	23.635034
115.138301	3378.101964	23.640051
115.125110	3393.328523	23.645069
115.312564	3408.118400	23.650087
115.416364	3396.597719	23.655104
115.153749	3410.439526	23.660122
115.690833	3405.251966	23.665139
115.813074	3415.751055	23.670157
115.511434	3414.259167	23.675175
116.135792	3407.624508	23.680192
116.260793	3429.533777	23.685210
115.875724	3436.392689	23.690227
116.246908	3447.100271	23.695245
116.155524	3440.471661	23.700263
116.483847	3435.612681	23.705280
116.279166	3437.407135	23.710298
116.649442	3425.624683	23.715315
116.636934	3440.771648	23.720333
116.827387	3462.157549	23.725351
117.160674	3448.505990	23.730368
116.916561	3463.266443	23.735386
117.221927	3466.782927	23.740403
117.181104	3470.418426	23.745421
117.410371	3489.636133	23.750439
117.851060	3479.682171	23.755456
117.806891	3481.385541	23.760474
118.226474	3485.909932	23.765491
118.371459	3483.269824	23.770509
118.345748	3491.692616	23.775527
118.231838	3478.461776	23.780544
118.281461	3479.978387	23.785562
118.335721	3473.833179	23.790579
118.790885	3490.000558	23.795597
118.661282	3495.456253	23.800615
118.949083	3509.680430	23.805632
119.074804	3506.635625	23.810650
118.895008	3499.676714	23.815667
118.954704	3492.932960	23.820685
119.245145	3521.295763	23.825703
119.139654	3532.538471	23.830720
119.306085	3541.320882	23.835738
119.385288	3536.523507	23.840755
119.749281	3534.590121	23.845773
119.518301	3565.086815	23.850791
120.025200	3563.332964	23.855808
120.149875	3567.921070	23.860826
120.377584	3561.821578	23.865843
120.627570	3556.018803	23.870861
120.784668	3585.308095	23.875879
120.873042	3572.026821	23.880896
120.636102	3590.231913	23.885914
120.284058	3595.407071	23.890931
120.873980	3584.014984	23.895949
120.608446	3583.490351	23.900967
121.047631	3596.829349	23.905984
120.985661	3609.274384	23.911002
120.803038	3613.596741	23.916019
121.095140	3633.720791	23.921037
121.610566	3642.602682	23.926055
121.800960	3635.128991	23.931072
121.893629	3636.024717	23.936090
121.954395	3653.754701	23.941107
122.402305	3672.019169	23.946125
122.381721	3664.080318	23.951143
122.632820	3659.141902	23.956160
122.545402	3661.455203	23.961178
122.347418	3665.819877	23.966195
122.539016	3682.298334	23.971213
122.987990	3699.270511	23.976231
123.034652	3685.864928	23.981248
123.494957	3688.533800	23.986266
123.279272	3689.167483	23.991283
123.355602	3686.499314	23.996301
123.559013	3706.719217	24.001319
124.245080	3709.418507	24.006336
124.309790	3709.082219	24.011354
124.407088	3710.286639	24.016371
124.693827	3703.221808	24.021389
124.130682	3702.373899	24.026407
124.819340	3709.105906	24.031424
124.627566	3705.648160	24.036442
124.635321	3701.868858	24.041459
124.786146	3708.527920	24.046477
124.589228	3711.271928	24.051495
124.885945	3700.228603	24.056512
125.204423	3710.312782	24.061530
125.067982	3714.983842	24.066547
125.283132	3706.601679	24.071565
125.146858	3719.929569	24.076583
125.192618	3733.030537	24.081600
125.467642	3734.172521	24.086618
125.413632	3739.328009	24.091635
125.474776	3756.169052	24.096653
125.977800	3760.633280	24.101671
126.853519	3755.718793	24.106688
126.691560	3749.089507	24.111706
126.361050	3742.939659	24.116723
126.829059	3748.270710	24.121741
126.519031	3750.229854	24.126759
126.447913	3748.527791	24.131776
126.849792	3758.589166	24.136794
126.746475	3771.304160	24.141811
127.139036	3773.527538	24.146829
126.915750	3781.213430	24.151847
126.957270	3793.738759	24.156864
127.319934	3797.026161	24.161882
126.916163	3804.816692	24.166899
127.604682	3815.278783	24.171917
127.625193	3840.542203	24.176935
127.608345	3841.261544	24.181952
127.924109	3844.964985	24.186970
128.077104	3856.933741	24.191987
128.674864	3853.755357	24.197005
128.603705	3859.434206	24.202023
128.768986	3862.971959	24.207040
129.065824	3857.167238	24.212058
128.900029	3861.437668	24.217075
129.346898	3874.624845	24.222093
129.484450	3882.625978	24.227111
129.220951	3880.588748	24.232128
129.501211	3889.400581	24.237146
129.465437	3888.882462	24.242163
129.639031	3882.690209	24.247181
129.341378	3896.759503	24.252199
130.248544	3907.235924	24.257216
130.393574	3914.090920	24.262234
129.846805	3915.450205	24.267251
130.499994	3915.178099	24.272269
130.535793	3935.736242	24.277287
130.607774	3940.299700	24.282304
130.715780	3938.649516	24.287322
130.815675	3937.197925	24.292339
130.906691	3939.333747	24.297357
131.289494	3944.580124	24.302375
131.203370	3960.521281	24.307392
131.134529	3957.594367	24.312410
131.059049	3964.726380	24.317427
131.381878	3974.601344	24.322445
131.682370	3989.043164	24.327463
131.635172	3988.966709	24.332480
132.037260	3993.002785	24.337498
132.082064	4009.147564	24.342515
132.119513	4012.568280	24.347533
132.172524	4010.231087	24.352551
132.397771	4023.480208	24.357568
132.778792	4031.433314	24.362586
132.986743	4045.748740	24.367603
133.045152	4045.417817	24.372621
133.214326	4053.247271	24.377639
133.165551	4043.149017	24.382656
133.306430	4043.886401	24.387674
133.200280	4051.659768	24.392691
133.717589	4058.702931	24.397709
134.121248	4073.095892	24.402727
133.876776	4066.404510	24.407744
133.875900	4062.972230	24.412762
133.837791	4065.672735	24.417779
134.086003	4069.270852	24.422797
134.384905	4092.494897	24.427815
134.459452	4099.219883	24.432832
134.610048	4097.011441	24.437850
134.579877	4102.639508	24.442867
134.710249	4116.116206	24.447885
134.890809	4124.837555	24.452903
135.068423	4130.386022	24.457920
135.347711	4124.455356	24.462938
135.531912	4149.620573	24.467955
135.757301	4150.568419	24.472973
136.001934	4157.366117	24.477991
136.080359	4163.307775	24.483008
136.642605	4151.925362	24.488026
136.354485	4155.987333	24.493043
136.123593	4148.446388	24.498061
136.552992	4161.719378	24.503079
136.804623	4164.917720	24.508096
136.934133	4183.523212	24.513114
136.860347	4180.128545	24.518131
136.837189	4178.314174	24.523149
137.224991	4179.191089	24.528167
137.209050	4199.221489	24.533184
137.573656	4205.011146	24.538202
137.500250	4208.041934	24.543219
137.751781	4205.029751	24.548237
137.567124	4200.630907	24.553255
137.476747	4213.781153	24.558272
138.259786	4226.220922	24.563290
138.042239	4233.463545	24.568307
137.824694	4242.614539	24.573325
138.268074	4253.169012	24.578343
138.316228	4254.694210	24.583360
138.896933	4265.001184	24.588378
139.069354	4287.653474	24.593395
139.294958	4270.779046	24.598413
139.385192	4283.336880	24.603431
139.412878	4288.503855	24.608448
139.718137	4275.697197	24.613466
139.632242	4287.782928	24.618483
140.203108	4306.640461	24.623501
140.210363	4322.078342	24.628519
139.946610	4318.171695	24.633536
140.289148	4315.397224	24.638554
140.326798	4313.106228	24.643571
140.737647	4314.402595	24.648589
140.789618	4327.012458	24.653607
140.790532	4344.100717	24.658624
140.879858	4342.121669	24.663642
140.992607	4340.617520	24.668659
140.638594	4331.842424	24.673677
140.928393	4355.829829	24.678695
141.022778	4373.874782	24.683712
141.374333	4384.494125	24.688730
141.465926	4396.903391	24.693747
141.719332	4407.607870	24.698765
141.487347	4400.119742	24.703783
142.121835	4413.613407	24.708800
142.854761	4411.311851	24.713818
142.858887	4424.489182	24.718835
142.732028	4421.302064	24.723853
143.240767	4428.963388	24.728871
142.981535	4421.700633	24.733888
143.241667	4409.170632	24.738906
143.086531	4412.227956	24.743923
142.779676	4418.243215	24.748941
143.594037	4426.865128	24.753959
143.332723	4445.034689	24.758976
143.384460	4448.134615	24.763994
143.768539	4445.764309	24.769011
143.578286	4456.516536	24.774029
144.152421	4474.261848	24.779047
144.176829	4479.623142	24.784064
144.365858	4478.075665	24.789082
144.361948	4498.972631	24.794099
144.431885	4502.821975	24.799117
144.851026	4498.572509	24.804135
144.720584	4502.404565	24.809152
145.165773	4514.384606	24.814170
145.300855	4530.287433	24.819187
145.024108	4540.008659	24.824205
145.116084	4529.881715	24.829223
145.725616	4555.427341	24.834240
145.765604	4568.692183	24.839258
145.677534	4569.748152	24.844275
146.004175	4585.350071	24.849293
146.504969	4587.560017	24.854311
146.441441	4598.852075	24.859328
146.843700	4589.952660	24.864346
147.026491	4596.907238	24.869363
147.582082	4607.439080	24.874381
147.956327	4589.749531	24.879399
147.688488	4589.149251	24.884416
147.935462	4579.380158	24.889434
147.869929	4581.932122	24.894451
148.044493	4589.894430	24.899469
148.315670	4580.055584	24.904487
147.963226	4590.204340	24.909504
148.539007	4594.657579	24.914522
148.342170	4599.464481	24.919539
148.666564	4600.655465	24.924557
148.710720	4595.829696	24.929575
148.640340	4599.996759	24.934592
148.609317	4609.779403	24.939610
149.049112	4623.583001	24.944627
148.838525	4630.443919	24.949645
149.091737	4642.734149	24.954663
149.036800	4659.149250	24.959680
148.925930	4667.376889	24.964698
149.356667	4678.037292	24.969715
149.339290	4695.788066	24.974733
149.825387	4704.686441	24.979751
150.011860	4724.845106	24.984768
150.426712	4727.750827	24.989786
150.673983	4722.311093	24.994803
150.499549	4731.999390	24.999821
150.977536	4737.596877	25.004839
150.921960	4745.431529	25.009856
151.026364	4741.303300	25.014874
151.063597	4743.465838	25.019891
151.177864	4775.001249	25.024909
151.398118	4779.624319	25.029927
151.471456	4776.416649	25.034944
151.584143	4789.975205	25.039962
152.053250	4788.661759	25.044979
152.173410	4810.949396	25.049997
152.092089	4812.914190	25.055015
152.213183	4814.690013	25.060032
152.502458	4830.911007	25.065050
153.132860	4826.471808	25.070067
153.099352	4825.376066	25.075085
153.140463	4821.982749	25.080103
152.935754	4828.841994	25.085120
152.964347	4826.591792	25.090138
153.733862	4848.177253	25.095155
153.583173	4847.345775	25.100173
153.709673	4867.033388	25.105191
153.771054	4860.618716	25.110208
153.962402	4868.622099	25.115226
154.211484	4869.995249	25.120243
154.331947	4886.097329	25.125261
154.494753	4884.514378	25.130279
154.671877	4900.384649	25.135296
155.007960	4898.844332	25.140314
155.213632	4902.654417	25.145331
154.923703	4907.179522	25.150349
155.514819	4904.031562	25.155367
155.642774	4930.109388	25.160384
155.851774	4932.378229	25.165402
155.753667	4923.170713	25.170419
155.582255	4928.909826	25.175437
156.070533	4943.126604	25.180455
156.030784	4951.803315	25.185472
156.362568	4960.282803	25.190490
156.656367	4967.431036	25.195507
156.347400	4977.564196	25.200525
157.009872	4974.526098	25.205543
156.983843	4985.651593	25.210560
157.079662	4995.173338	25.215578
157.379726	5014.156799	25.220595
157.283812	5012.127951	25.225613
157.547560	5014.841743	25.230631
157.872680	5028.329181	25.235648
157.863763	5038.352953	25.240666
158.280597	5044.334318	25.245683
158.102626	5056.824085	25.250701
158.416373	5062.081860	25.255719
158.394807	5072.173893	25.260736
158.523484	5071.697861	25.265754
158.986871	5091.176532	25.270771
159.046620	5106.971514	25.275789
159.095010	5106.873746	25.280807
159.426590	5117.899299	25.285824
159.399116	5135.351814	25.290842
159.789880	5138.823466	25.295859
159.887067	5141.819159	25.300877
160.175783	5160.499521	25.305895
160.333939	5155.466533	25.310912
160.330921	5158.780788	25.315930
160.881005	5145.260454	25.320947
160.834391	5159.882775	25.325965
161.068587	5187.964568	25.330983
161.265697	5186.296383	25.336000
161.287907	5183.853068	25.341018
161.526347	5185.452441	25.346035
161.664677	5193.908108	25.351053
161.596011	5201.836894	25.356071
161.819902	5217.204427	25.361088
161.951443	5223.852756	25.366106
162.131218	5225.216128	25.371123
161.902855	5245.298322	25.376141
162.176837	5245.885018	25.381159
162.268987	5248.557510	25.386176
162.633040	5270.232208	25.391194
162.937306	5276.818158	25.396211
162.938451	5285.600514	25.401229
163.161381	5286.831550	25.406247
163.498035	5298.458038	25.411264
163.380159	5301.370385	25.416282
163.364322	5300.552432	25.421299
163.752211	5310.942363	25.426317
163.618789	5328.816586	25.431335
163.806931	5339.150159	25.436352
163.707114	5363.399576	25.441370
164.498230	5367.933617	25.446387
164.309807	5387.973563	25.451405
164.923258	5395.916529	25.456423
165.020641	5398.937833	25.461440
165.050094	5401.753799	25.466458
165.601261	5418.447551	25.471475
165.740972	5427.046441	25.476493
165.781664	5421.745732	25.481511
166.000138	5422.731026	25.486528
166.107575	5424.207563	25.491546
166.445217	5429.889916	25.496563
166.761386	5440.096089	25.501581
166.665084	5453.925609	25.506599
166.855615	5454.915916	25.511616
167.019755	5463.107195	25.516634
167.026618	5463.546277	25.521651
167.136885	5473.785706	25.526669
167.256126	5481.888731	25.531687
167.727189	5480.225651	25.536704
167.821361	5501.166418	25.541722
167.870390	5493.738432	25.546739
168.204774	5503.726649	25.551757
168.227247	5523.485826	25.556775
168.525067	5525.847968	25.561792
168.374263	5532.491892	25.566810
168.539841	5539.143000	25.571827
168.705612	5559.190005	25.576845
168.539079	5565.154952	25.581863
169.272894	5562.960193	25.586880
169.178403	5592.187327	25.591898
169.705670	5586.544319	25.596915
169.954268	5593.781029	25.601933
170.100085	5608.411742	25.606951
170.274404	5605.323457	25.611968
170.483892	5614.203482	25.616986
170.815051	5616.669988	25.622003
170.751953	5621.568505	25.627021
170.662603	5639.504313	25.632039
171.029019	5642.666278	25.637056
171.279386	5648.498191	25.642074
171.339239	5648.228029	25.647091
171.394511	5662.856822	25.652109
171.516848	5668.500418	25.657127
171.678105	5672.473171	25.662144
171.911297	5684.275332	25.667162
172.176580	5699.022237	25.672180
172.287790	5698.925900	25.677197
172.322593	5716.238437	25.682215
172.851787	5721.061961	25.687232
172.856897	5734.025240	25.692250
173.391430	5723.758250	25.697268
173.410262	5725.797962	25.702285
173.330617	5742.714417	25.707303
173.593773	5745.407565	25.712320
173.143556	5755.278693	25.717338
173.549478	5766.713350	25.722356
173.861877	5772.785491	25.727373
173.822439	5774.302473	25.732391
174.704000	5798.803860	25.737408
174.635086	5806.781819	25.742426
174.931913	5813.532242	25.747444
174.804895	5804.182506	25.752461
175.011851	5813.724581	25.757479
175.538251	5825.022034	25.762496
175.226299	5825.935128	25.767514
175.494424	5834.474831	25.772532
175.847740	5839.040793	25.777549
175.820314	5861.509453	25.782567
176.150666	5860.123954	25.787584
176.384178	5870.177505	25.792602
176.609249	5872.329639	25.797620
176.461076	5895.349090	25.802637
176.268957	5889.136539	25.807655
176.615870	5901.177989	25.812672
176.679081	5923.516783	25.817690
177.102355	5923.315331	25.822708
177.407109	5944.803092	25.827725
177.289892	5961.026664	25.832743
178.023403	5971.765508	25.837760
178.146326	5987.353269	25.842778
178.467609	5975.523452	25.847796
178.745975	5991.155623	25.852813
178.654119	5988.371129	25.857831
178.839647	5994.733655	25.862848
179.126307	6020.402364	25.867866
179.370497	6017.467836	25.872884
179.949675	6018.853491	25.877901
180.102050	6017.513924	25.882919
179.851596	6016.915831	25.887936
179.821253	6040.302704	25.892954
179.926713	6056.566760	25.897972
180.077872	6046.884254	25.902989
180.084287	6074.741448	25.908007
180.625647	6066.581342	25.913024
180.413897	6077.054323	25.918042
180.636143	6090.817594	25.923060
181.416649	6103.592422	25.928077
180.900473	6121.051569	25.933095
181.429967	6129.601801	25.938112
181.259625	6141.000427	25.943130
181.682642	6157.442868	25.948148
182.199113	6162.489144	25.953165
182.250728	6170.886819	25.958183
182.583049	6184.045268	25.963200
182.551577	6194.499565	25.968218
182.991910	6188.529703	25.973236
183.585437	6194.616988	25.978253
183.473783	6204.634066	25.983271
183.837130	6208.033706	25.988288
183.959946	6208.509566	25.993306
183.981999	6203.443604	25.998324
184.008256	6205.058454	26.003341
184.179678	6208.928465	26.008359
184.735487	6214.868419	26.013376
184.745872	6225.252818	26.018394
184.916401	6227.610899	26.023412
185.014697	6227.358396	26.028429
184.940224	6232.929183	26.033447
185.225431	6249.992236	26.038464
185.378708	6263.530004	26.043482
185.296308	6273.789583	26.048500
185.773804	6281.877537	26.053517
185.546782	6290.649721	26.058535
186.001075	6296.330051	26.063552
185.875565	6318.743903	26.068570
186.056723	6335.880158	26.073588
186.420419	6334.620631	26.078605
186.382447	6356.832638	26.083623
186.737547	6360.640049	26.088640
186.709722	6384.986253	26.093658
186.834078	6397.777592	26.098676
187.388231	6395.735268	26.103693
187.307013	6414.070297	26.108711
187.768949	6414.545261	26.113728
187.827562	6438.448051	26.118746
187.686191	6454.648557	26.123764
188.199348	6464.745279	26.128781
188.518251	6483.291498	26.133799
188.425313	6480.863069	26.138816
189.294909	6500.377582	26.143834
189.360081	6513.387496	26.148852
189.567486	6512.408948	26.153869
189.289924	6522.617452	26.158887
189.823492	6536.814813	26.163904
190.148875	6540.454703	26.168922
189.929292	6539.537252	26.173940
190.229285	6563.499581	26.178957
190.232425	6580.723007	26.183975
190.746068	6596.781570	26.188992
190.751324	6607.932578	26.194010
190.976816	6610.433635	26.199028
191.354980	6627.064332	26.204045
191.576663	6637.566091	26.209063
191.715754	6634.721271	26.214080
191.816980	6650.091969	26.219098
192.120786	6662.552236	26.224116
192.577871	6658.301048	26.229133
192.702786	6668.024163	26.234151
193.063191	6669.862648	26.239168
193.017099	6687.503860	26.244186
192.881713	6694.947467	26.249204
193.400374	6696.730668	26.254221
193.331742	6723.053053	26.259239
193.542118	6715.671077	26.264256
193.746159	6726.165572	26.269274
193.645291	6737.976074	26.274292
194.504870	6749.787772	26.279309
194.462046	6770.117297	26.284327
194.877746	6766.818003	26.289344
194.914364	6775.341340	26.294362
195.303457	6789.753392	26.299380
195.455343	6786.630782	26.304397
195.362040	6800.985511	26.309415
195.601292	6817.030568	26.314432
195.779961	6815.351085	26.319450
196.283807	6820.811562	26.324468
196.740856	6837.961848	26.329485
196.960340	6850.851248	26.334503
197.330688	6835.092925	26.339520
197.674413	6831.340054	26.344538
197.620889	6832.541285	26.349556
198.109116	6820.923462	26.354573
198.298025	6825.382204	26.359591
198.640401	6823.037738	26.364608
198.664452	6818.449305	26.369626
198.513662	6813.568432	26.374644
198.815419	6815.144913	26.379661
198.615998	6828.233457	26.384679
198.599183	6831.439297	26.389696
199.093956	6834.103819	26.394714
199.067525	6857.292003	26.399732
199.213638	6848.911699	26.404749
199.038889	6861.867821	26.409767
199.360250	6879.268968	26.414784
199.327493	6881.478806	26.419802
199.376803	6899.744791	26.424820
199.866488	6926.040637	26.429837
199.695183	6940.461937	26.434855
199.887978	6955.909951	26.439872
200.029627	6971.487718	26.444890
200.121593	6992.299310	26.449908
200.443080	6999.326552	26.454925
200.619259	7021.167026	26.459943
201.059161	7032.797041	26.464960
201.653336	7044.370073	26.469978
201.625306	7079.532489	26.474996
202.090953	7070.306963	26.480013
202.392624	7082.211881	26.485031
202.593789	7082.753583	26.490048
203.131363	7086.809042	26.495066
202.936670	7103.234035	26.500084
203.820500	7111.805808	26.505101
203.575455	7134.157084	26.510119
203.748955	7132.364222	26.515136
204.179784	7131.010059	26.520154
203.972061	7138.202772	26.525172
204.032819	7158.865373	26.530189
203.997596	7160.351863	26.535207
204.365063	7177.955221	26.540224
204.589525	7185.229341	26.545242
204.519157	7199.212838	26.550260
204.984797	7208.794932	26.555277
204.845096	7239.319123	26.560295
204.820868	7255.983891	26.565312
205.254871	7274.979070	26.570330
205.455351	7302.353502	26.575348
205.901024	7298.893203	26.580365
206.203076	7320.101332	26.585383
206.379443	7333.707877	26.590400
206.572631	7342.204864	26.595418
206.996815	7355.707475	26.600436
208.131460	7353.620319	26.605453
208.399835	7366.958871	26.610471
208.543482	7361.373109	26.615488
208.698263	7366.298390	26.620506
208.638794	7367.587280	26.625524
208.891821	7359.288279	26.630541
208.900371	7368.953868	26.635559
208.804839	7390.816120	26.640576
208.999681	7386.623820	26.645594
208.987203	7406.180452	26.650612
209.245816	7412.979624	26.655629
209.570103	7420.886344	26.660647
209.413878	7446.830606	26.665664
209.738728	7445.606556	26.670682
210.009117	7470.543123	26.675700
210.357925	7484.281191	26.680717
210.556029	7498.072524	26.685735
210.608107	7515.654335	26.690752
211.087534	7514.244068	26.695770
210.390548	7546.666123	26.700788
211.116525	7563.318318	26.705805
211.578567	7573.924334	26.710823
211.581406	7583.964326	26.715840
212.113927	7584.897087	26.720858
212.028477	7601.986618	26.725876
212.593488	7606.229858	26.730893
213.224248	7623.567319	26.735911
213.419195	7635.142952	26.740928
213.850217	7622.710153	26.745946
214.004029	7625.291740	26.750964
213.967567	7622.602555	26.755981
214.293821	7625.632156	26.760999
214.124792	7637.538866	26.766016
214.708003	7643.827692	26.771034
214.752590	7653.020446	26.776052
214.623292	7660.130340	26.781069
214.766164	7668.462541	26.786087
214.812769	7683.830669	26.791104
215.358746	7679.992989	26.796122
215.148430	7690.454197	26.801140
215.220264	7709.945291	26.806157
215.395721	7723.354631	26.811175
215.675811	7761.945776	26.816192
215.717221	7772.451299	26.821210
215.717978	7798.063815	26.826228
216.099970	7813.761016	26.831245
216.552501	7831.157294	26.836263
216.614521	7860.423812	26.841280
217.276364	7863.167240	26.846298
217.281895	7887.915876	26.851316
217.239119	7910.712916	26.856333
217.572104	7912.151242	26.861351
217.899857	7935.210025	26.866368
218.597757	7950.514125	26.871386
218.807093	7966.726758	26.876404
219.198971	7969.047745	26.881421
219.224379	7984.693762	26.886439
219.207620	7988.449593	26.891456
219.789240	7995.583952	26.896474
220.243736	8001.421610	26.901492
220.478750	8000.702269	26.906509
220.870984	8021.912194	26.911527
221.117210	8026.494130	26.916544
221.405313	8019.846958	26.921562
221.701893	8014.367234	26.926580
221.722150	8020.623990	26.931597
222.244583	8012.373867	26.936615
222.008168	8041.033929	26.941632
222.205300	8031.164609	26.946650
222.563281	8040.915437	26.951668
222.455275	8039.955830	26.956685
222.722625	8050.744774	26.961703
222.438065	8069.880899	26.966720
222.957044	8083.105403	26.971738
222.753664	8093.870545	26.976756
222.923315	8105.262457	26.981773
223.509259	8124.016169	26.986791
223.454001	8142.479660	26.991808
224.054873	8154.539166	26.996826
223.924399	8173.926420	27.001844
224.411241	8191.272532	27.006861
224.458344	8208.757478	27.011879
224.773094	8226.066688	27.016896
224.937372	8229.045192	27.021914
225.358888	8254.623584	27.026932
225.296416	8269.050951	27.031949
225.866901	8285.448413	27.036967
225.834882	8309.139014	27.041984
226.341135	8323.513424	27.047002
226.384497	8327.243649	27.052020
226.807201	8345.934015	27.057037
227.142251	8343.000592	27.062055
227.136477	8355.584237	27.067072
227.556451	8371.090620	27.072090
227.784239	8383.244235	27.077108
227.943286	8388.103756	27.082125
228.372328	8397.835188	27.087143
228.544427	8426.224448	27.092160
228.575713	8412.589746	27.097178
228.780926	8443.985548	27.102196
228.992865	8454.681528	27.107213
229.311452	8458.548260	27.112231
229.342642	8465.438235	27.117248
229.616491	8470.537952	27.122266
230.109159	8493.092982	27.127284
230.084635	8518.802207	27.132301
230.210470	8518.260777	27.137319
230.573210	8526.559467	27.142336
230.526812	8525.863757	27.147354
230.934339	8527.762420	27.152372
231.537190	8543.871247	27.157389
231.403008	8564.093719	27.162407
231.534416	8578.991862	27.167424
231.706179	8593.567499	27.172442
232.283369	8616.399388	27.177460
232.233998	8624.664609	27.182477
232.879755	8623.219682	27.187495
233.103092	8647.861840	27.192512
233.358518	8660.185964	27.197530
233.330732	8662.814266	27.202548
233.317669	8680.074161	27.207565
233.779254	8686.692268	27.212583
233.933572	8708.278754	27.217600
234.123250	8717.367811	27.222618
234.367952	8749.764332	27.227636
234.224341	8759.112485	27.232653
235.011139	8778.033857	27.237671
234.834054	8799.886317	27.242688
235.308768	8797.445662	27.247706
235.528189	8822.931547	27.252724
236.023633	8833.031147	27.257741
236.861693	8838.621432	27.262759
236.763039	8857.549773	27.267776
236.801547	8861.314796	27.272794
237.042853	8879.757714	27.277812
237.049361	8896.978378	27.282829
237.741387	8905.706497	27.287847
237.897057	8917.288769	27.292864
237.908605	8933.561852	27.297882
238.199620	8935.602694	27.302900
238.473140	8964.789044	27.307917
238.648210	8965.767563	27.312935
238.823309	8990.585999	27.317952
239.053213	9004.972817	27.322970
239.529216	9010.470959	27.327988
239.513598	9030.008055	27.333005
239.805875	9037.147372	27.338023
239.458258	9058.157971	27.343040
240.240415	9074.595323	27.348058
241.065265	9089.406945	27.353076
240.691569	9089.738863	27.358093
241.327569	9096.758403	27.363111
241.803712	9111.288953	27.368128
241.843349	9110.161528	27.373146
242.307534	9116.061017	27.378164
242.254403	9134.797061	27.383181
242.619021	9139.655932	27.388199
242.547885	9150.004518	27.393216
242.703341	9162.874876	27.398234
243.081954	9170.414313	27.403252
243.441218	9207.590658	27.408269
243.451941	9208.235582	27.413287
243.523028	9220.283398	27.418304
243.738388	9240.793199	27.423322
244.196562	9252.944077	27.428340
244.033866	9288.329773	27.433357
244.271162	9293.120717	27.438375
244.482178	9310.342698	27.443392
244.505086	9317.685760	27.448410
245.064032	9337.339408	27.453428
245.179884	9358.310063	27.458445
245.672210	9376.999596	27.463463
245.537366	9395.342205	27.468480
246.056312	9413.827307	27.473498
246.301415	9425.900879	27.478516
246.241979	9454.825694	27.483533
246.740181	9467.165473	27.488551
247.037683	9484.878272	27.493568
247.298152	9504.564111	27.498586
247.736372	9512.569638	27.503604
247.838535	9531.673556	27.508621
247.970786	9552.959991	27.513639
247.928106	9566.368332	27.518656
248.528787	9575.353742	27.523674
248.899281	9598.080982	27.528692
249.065875	9608.734818	27.533709
249.729406	9636.191955	27.538727
249.854829	9648.400475	27.543744
249.930883	9661.205583	27.548762
250.376114	9665.923688	27.553780
250.856987	9687.340969	27.558797
251.435137	9697.040690	27.563815
251.700916	9695.317371	27.568832
251.465472	9711.935326	27.573850
251.818638	9728.445810	27.578868
251.498814	9734.694834	27.583885
252.021992	9756.033536	27.588903
252.365049	9769.070319	27.593920
252.302009	9793.899417	27.598938
252.701988	9800.311548	27.603956
253.047899	9828.454032	27.608973
253.731541	9829.606167	27.613991
253.880906	9843.441466	27.619008
254.148619	9850.576543	27.624026
254.357295	9862.765171	27.629044
254.561980	9881.639884	27.634061
254.821764	9882.955003	27.639079
255.376588	9899.037697	27.644096
255.247104	9912.113282	27.649114
255.802233	9921.366365	27.654132
255.859103	9947.637124	27.659149
256.061343	9951.109889	27.664167
256.607197	9958.496036	27.669184
256.500114	9979.988006	27.674202
256.761294	9990.977798	27.679220
256.336893	10010.753781	27.684237
257.180940	10021.126606	27.689255
257.084628	10043.496778	27.694272
257.437993	10059.086712	27.699290
258.113087	10056.657668	27.704308
258.656645	10076.767720	27.709325
258.879696	10081.199687	27.714343
259.238007	10089.620453	27.719360
259.015219	10111.888729	27.724378
259.512598	10122.670226	27.729396
259.559284	10130.613928	27.734413
259.958871	10148.794270	27.739431
260.068789	10156.161943	27.744448
260.000884	10185.491225	27.749466
260.802563	10190.020621	27.754484
260.778271	10212.827355	27.759501
260.887902	10230.502701	27.764519
261.140333	10241.064005	27.769536
261.329835	10254.291981	27.774554
261.859470	10263.028778	27.779572
262.027688	10295.448168	27.784589
262.200383	10308.026713	27.789607
262.468389	10330.982259	27.794624
262.505239	10335.676657	27.799642
262.823703	10350.977239	27.804660
262.718995	10377.146208	27.809677
263.293727	10390.179097	27.814695
263.611227	10411.082371	27.819712
263.923959	10428.699961	27.824730
264.321136	10448.956769	27.829748
264.393727	10459.694451	27.834765
264.456455	10482.510824	27.839783
265.145435	10504.950414	27.844800
265.113178	10529.313942	27.849818
265.615510	10545.358697	27.854836
265.746577	10554.449822	27.859853
265.883844	10580.581509	27.864871
266.202923	10605.470049	27.869888
266.438596	10622.644471	27.874906
266.682219	10648.475890	27.879924
266.739852	10677.419810	27.884941
267.182146	10691.754944	27.889959
267.608243	10713.751420	27.894976
267.777504	10739.505466	27.899994
267.994069	10750.917519	27.905012
268.515563	10767.244503	27.910029
268.891807	10778.784597	27.915047
269.814589	10796.092258	27.920064
269.949801	10808.781375	27.925082
270.172114	10818.495669	27.930100
270.188830	10836.500568	27.935117
270.498568	10848.482611	27.940135
271.055024	10858.990156	27.945152
270.957361	10874.796415	27.950170
271.558408	10897.690662	27.955188
271.923134	10903.441820	27.960205
271.823447	10909.574576	27.965223
272.256654	10920.817036	27.970240
272.623596	10932.449373	27.975258
273.149588	10948.036865	27.980276
273.401417	10963.044172	27.985293
273.232624	10961.444512	27.990311
274.189411	10970.267109	27.995328
274.489288	10989.875793	28.000346
274.565187	10980.958203	28.005364
274.974958	10985.357999	28.010381
274.970652	10990.622651	28.015399
275.429692	11012.744868	28.020416
275.360866	11015.434694	28.025434
275.759180	11028.914777	28.030452
276.180291	11039.389658	28.035469
276.092810	11042.949917	28.040487
276.234980	11054.342178	28.045504
276.181237	11074.311897	28.050522
276.679451	11091.552162	28.055540
276.653733	11111.421974	28.060557
276.739432	11150.086532	28.065575
277.056115	11161.122318	28.070592
277.095858	11188.195182	28.075610
277.251333	11216.059607	28.080628
277.871531	11241.825830	28.085645
277.807337	11281.449788	28.090663
278.385223	11299.660280	28.095680
278.604939	11323.520162	28.100698
278.654158	11348.659268	28.105716
279.029901	11380.106725	28.110733
279.226429	11414.256856	28.115751
279.853222	11420.166581	28.120768
280.139523	11447.302349	28.125786
280.609596	11465.154272	28.130804
281.004187	11476.651662	28.135821
281.239852	11496.737954	28.140839
281.891934	11513.717700	28.145856
282.007811	11520.360235	28.150874
282.442695	11538.661589	28.155892
282.956922	11535.809861	28.160909
283.405113	11538.411205	28.165927
284.174609	11529.763172	28.170944
283.904329	11548.130617	28.175962
284.057782	11562.187312	28.180980
284.245605	11562.392625	28.185997
284.044476	11582.058020	28.191015
284.658299	11585.669552	28.196032
284.676230	11599.606864	28.201050
284.693076	11626.018549	28.206068
285.070620	11644.248352	28.211085
284.988234	11674.484002	28.216103
285.548427	11695.014037	28.221120
285.729146	11722.230737	28.226138
286.082280	11738.268252	28.231156
286.430345	11759.756735	28.236173
286.579330	11792.055488	28.241191
287.213615	11813.096545	28.246208
287.425451	11840.315395	28.251226
287.766779	11857.999949	28.256244
287.955760	11880.348391	28.261261
288.129534	11899.618199	28.266279
288.626669	11924.284778	28.271296
288.916598	11952.956270	28.276314
289.191335	11970.243855	28.281332
289.775324	11978.633064	28.286349
289.847873	11996.781300	28.291367
290.708507	12008.728347	28.296384
291.181931	12023.143042	28.301402
291.353021	12035.972162	28.306420
291.250549	12055.544627	28.311437
291.118703	12063.558960	28.316455
291.816725	12077.569469	28.321472
292.107148	12098.811883	28.326490
292.581065	12121.405872	28.331508
293.100833	12121.675317	28.336525
293.075032	12152.181408	28.341543
293.711609	12155.136196	28.346560
293.859033	12169.742752	28.351578
293.684210	12195.086427	28.356596
294.061756	12205.699263	28.361613
294.197464	12232.323929	28.366631
294.347117	12256.295250	28.371648
294.964123	12273.937082	28.376666
294.909718	12290.442700	28.381684
295.528155	12310.380109	28.386701
295.586440	12340.589040	28.391719
295.999207	12349.131999	28.396736
295.888788	12382.652620	28.401754
295.943653	12406.893511	28.406772
296.560348	12437.440534	28.411789
296.750406	12458.492011	28.416807
297.264905	12481.101861	28.421824
297.840911	12514.692135	28.426842
297.838959	12538.052334	28.431860
298.207345	12557.144235	28.436877
299.132640	12570.262017	28.441895
299.748371	12572.025939	28.446912
300.153215	12588.130606	28.451930
300.193772	12590.408693	28.456948
300.559420	12610.790045	28.461965
300.762788	12614.549199	28.466983
300.890310	12602.934012	28.472000
301.220742	12631.119427	28.477018
301.323066	12641.434513	28.482036
301.554323	12650.407852	28.487053
301.296056	12682.070534	28.492071
301.688091	12691.146543	28.497088
301.895379	12709.039325	28.502106
302.127549	12736.380811	28.507124
302.554220	12764.342563	28.512141
302.505478	12800.297820	28.517159
302.988870	12827.697227	28.522176
303.530897	12852.910898	28.527194
303.642309	12865.388117	28.532212
304.051437	12883.618047	28.537229
304.356438	12932.187287	28.542247
305.018218	12952.137240	28.547264
304.985487	12969.567299	28.552282
305.026571	12995.261041	28.557300
305.599307	13012.184574	28.562317
305.872682	13044.642556	28.567335
306.190963	13063.540061	28.572352
306.635597	13097.115434	28.577370
306.807333	13124.601499	28.582388
307.051659	13141.820517	28.587405
307.499102	13171.462462	28.592423
308.278052	13182.751818	28.597440
308.969311	13220.503469	28.602458
308.859414	13222.319587	28.607476
309.591536	13244.038908	28.612493
309.721748	13243.966973	28.617511
310.139062	13263.198174	28.622528
310.523963	13278.337721	28.627546
310.585789	13298.094124	28.632564
310.932694	13311.547587	28.637581
310.863870	13335.874911	28.642599
311.221364	13348.578157	28.647616
311.603652	13375.008753	28.652634
311.791647	13401.444702	28.657652
312.290107	13410.836029	28.662669
312.461674	13449.422573	28.667687
312.935589	13457.138181	28.672704
313.208469	13472.843219	28.677722
313.278845	13501.311059	28.682740
313.571155	13515.295302	28.687757
313.947884	13543.785093	28.692775
314.002738	13566.779684	28.697792
314.868738	13587.043363	28.702810
314.964422	13615.398492	28.707828
315.126314	13632.327518	28.712845
315.550261	13652.999959	28.717863
315.810591	13682.311314	28.722880
316.255990	13701.388694	28.727898
316.378171	13722.415211	28.732916
316.841784	13750.536451	28.737933
316.967677	13776.770534	28.742951
317.117801	13805.481018	28.747968
317.536618	13821.508967	28.752986
317.716301	13861.825417	28.758004
318.234907	13895.521019	28.763021
318.561179	13920.827154	28.768039
319.003803	13938.704479	28.773056
319.589879	13951.742336	28.778074
320.041091	13972.541476	28.783092
320.492100	13989.191461	28.788109
320.742595	14018.123692	28.793127
320.821952	14028.530129	28.798144
321.372776	14042.100218	28.803162
321.625023	14056.910993	28.808180
321.814439	14061.459144	28.813197
322.470954	14087.267259	28.818215
322.884699	14089.654098	28.823232
323.305771	14108.661912	28.828250
323.291649	14124.019454	28.833268
323.584153	14114.161385	28.838285
324.037631	14138.553331	28.843303
324.376148	14149.148683	28.848320
324.557487	14170.400810	28.853338
324.444337	14190.831736	28.858356
324.705891	14210.345086	28.863373
325.053566	14227.458360	28.868391
325.450434	14245.868350	28.873408
326.007745	14257.281751	28.878426
325.745540	14291.988085	28.883444
326.384680	14310.372306	28.888461
326.619192	14329.444293	28.893479
326.681509	14366.309713	28.898496
327.432507	14385.362627	28.903514
327.551985	14421.968164	28.908532
327.871068	14437.485276	28.913549
328.097863	14478.449468	28.918567
328.678439	14491.586376	28.923584
328.978882	14520.375722	28.928602
329.346167	14554.310438	28.933620
329.691668	14569.315870	28.938637
330.032495	14591.404220	28.943655
330.002021	14618.792269	28.948672
330.570792	14642.499315	28.953690
330.969936	14673.412717	28.958708
330.903921	14705.901723	28.963725
331.470827	14730.844727	28.968743
332.247118	14749.206789	28.973760
332.619827	14765.057330	28.978778
332.634531	14794.411270	28.983796
333.011586	14816.104686	28.988813
333.445655	14846.049753	28.993831
333.124386	14882.287874	28.998848
333.595485	14912.206457	29.003866
334.092889	14946.561757	29.008884
334.407480	14963.170665	29.013901
335.130143	14988.567421	29.018919
335.506312	15020.534858	29.023936
335.679009	15046.298350	29.028954
335.978402	15066.821390	29.033972
336.672121	15087.968005	29.038989
337.453282	15115.240139	29.044007
337.108843	15138.139012	29.049024
337.847816	15152.224234	29.054042
338.007089	15178.894755	29.059060
338.232986	15203.399966	29.064077
338.450689	15227.574038	29.069095
338.464573	15262.314044	29.074112
339.247203	15292.791763	29.079130
338.965549	15317.105196	29.084148
339.434365	15339.039458	29.089165
340.362787	15365.625772	29.094183
340.182511	15402.030869	29.099200
340.563475	15420.378624	29.104218
341.224213	15466.354597	29.109236
341.068279	15493.917709	29.114253
341.633315	15511.872679	29.119271
341.911270	15540.995350	29.124288
342.357954	15553.138717	29.129306
342.439680	15605.221604	29.134324
342.406773	15642.668270	29.139341
343.102987	15661.351915	29.144359
343.363319	15693.281493	29.149376
343.762203	15723.684723	29.154394
344.048644	15748.242214	29.159412
344.699498	15775.757623	29.164429
345.562712	15797.945704	29.169447
345.695990	15824.820153	29.174464
346.271995	15842.113320	29.179482
346.757556	15851.454612	29.184500
346.822471	15861.457988	29.189517
347.658647	15879.697962	29.194535
347.964323	15895.834908	29.199552
347.979203	15907.400548	29.204570
348.365316	15927.536824	29.209588
348.584641	15940.989903	29.214605
349.073668	15962.617489	29.219623
349.225901	15981.809019	29.224640
349.812712	16006.011524	29.229658
349.813594	16034.325052	29.234676
349.734620	16055.848014	29.239693
350.443388	16081.690064	29.244711
350.550442	16107.514929	29.249728
351.020388	16137.667630	29.254746
351.205781	16178.639771	29.259764
351.558961	16206.621163	29.264781
352.005333	16228.839292	29.269799
352.271589	16265.200906	29.274816
352.753922	16292.207585	29.279834
353.044138	16313.619460	29.284852
353.746247	16352.123649	29.289869
354.240680	16371.957307	29.294887
354.334416	16398.845533	29.299904
354.850449	16413.681068	29.304922
355.206048	16452.669855	29.309940
355.825915	16480.358636	29.314957
355.751380	16493.558105	29.319975
356.071967	16525.049077	29.324992
356.518701	16547.694701	29.330010
356.638424	16581.737567	29.335028
356.995958	16625.130069	29.340045
357.494277	16650.564898	29.345063
357.708703	16675.922153	29.350080
358.108360	16696.925574	29.355098
358.578283	16729.697289	29.360116
358.772302	16767.175228	29.365133
359.668156	16796.112942	29.370151
359.659668	16830.021467	29.375168
360.080183	16846.517071	29.380186
360.502673	16874.680440	29.385204
360.810278	16905.141921	29.390221
361.568009	16924.436271	29.395239
361.771215	16949.592480	29.400256
362.388887	16970.448330	29.405274
363.074395	16977.760273	29.410292
363.258802	17003.677793	29.415309
363.438585	17017.160354	29.420327
363.665562	17043.274227	29.425344
364.129825	17089.745872	29.430362
364.489960	17093.848990	29.435380
364.637188	17128.935008	29.440397
364.872250	17142.162659	29.445415
364.974605	17175.123652	29.450432
365.019964	17212.220514	29.455450
365.495414	17236.012941	29.460468
366.036285	17279.558141	29.465485
366.398296	17307.915079	29.470503
366.666320	17346.099267	29.475520
366.924258	17368.014343	29.480538
367.637960	17390.960635	29.485556
368.073257	17412.499712	29.490573
368.753084	17432.917162	29.495591
369.075772	17469.872642	29.500608
369.110672	17484.891082	29.505626
369.805373	17506.683754	29.510644
369.786938	17529.848909	29.515661
370.400843	17554.228911	29.520679
370.599733	17578.612883	29.525696
371.014593	17601.490622	29.530714
371.582994	17632.356431	29.535732
371.487996	17660.616089	29.540749
371.867949	17685.711125	29.545767
372.271712	17714.251009	29.550784
372.706693	17739.157348	29.555802
372.738381	17781.355214	29.560820
373.111892	17816.852958	29.565837
373.650054	17850.201985	29.570855
373.479754	17885.784984	29.575872
373.663074	17925.798742	29.580890
374.738890	17955.334535	29.585908
375.255206	18009.681333	29.590925
375.563684	18038.228061	29.595943
375.966599	18069.344274	29.600960
376.412255	18091.795173	29.605978
376.965599	18112.995688	29.610996
377.703739	18137.866735	29.616013
378.169723	18162.674017	29.621031
378.556562	18196.483788	29.626048
378.919255	18220.028301	29.631066
379.483750	18233.270187	29.636084
379.623438	18262.273928	29.641101
380.098914	18281.950670	29.646119
380.360568	18312.611494	29.651136
380.630885	18339.391747	29.656154
380.717393	18368.016696	29.661172
380.969990	18399.334906	29.666189
381.483755	18425.706235	29.671207
382.246789	18462.931670	29.676224
382.420373	18490.621899	29.681242
382.883186	18524.716131	29.686260
383.059615	18551.603662	29.691277
383.827830	18573.341467	29.696295
383.969888	18604.497051	29.701312
384.475976	18632.633851	29.706330
385.055915	18658.523308	29.711348
385.013194	18691.074654	29.716365
385.312759	18714.349717	29.721383
385.961602	18740.708693	29.726400
385.970585	18774.604132	29.731418
386.725710	18795.797413	29.736436
387.031819	18824.780952	29.741453
387.322005	18869.286018	29.746471
387.899140	18895.296109	29.751488
388.449082	18926.173691	29.756506
388.735313	18946.713210	29.761524
389.056010	18984.837310	29.766541
389.684567	19006.256692	29.771559
389.797975	19035.887202	29.776576
389.976093	19063.733695	29.781594
390.680033	19092.384006	29.786612
390.613715	19138.056851	29.791629
391.313850	19166.101025	29.796647
391.722158	19197.395019	29.801664
391.945098	19231.282844	29.806682
392.519760	19256.285045	29.811700
392.466612	19301.763848	29.816717
392.824342	19330.328313	29.821735
393.099935	19351.060829	29.826752
393.371960	19396.643812	29.831770
393.875681	19433.513869	29.836788
394.143846	19471.241059	29.841805
394.639976	19499.853889	29.846823
395.303839	19541.764212	29.851840
395.559719	19574.521758	29.856858
396.373160	19598.909650	29.861876
396.502191	19642.172839	29.866893
396.718110	19660.889937	29.871911
397.132553	19701.399465	29.876928
397.552009	19735.588473	29.881946
398.156514	19772.144693	29.886964
398.401465	19811.268453	29.891981
399.098535	19840.504462	29.896999
399.107812	19862.164399	29.902016
399.257655	19909.599184	29.907034
399.934677	19934.470419	29.912052
400.011019	19979.154081	29.917069
400.521904	20030.385501	29.922087
400.990423	20065.799849	29.927104
401.416961	20102.026766	29.932122
402.069913	20138.199019	29.937140
402.303488	20169.068116	29.942157
402.915266	20213.440101	29.947175
403.374650	20258.562546	29.952192
403.515062	20293.517656	29.957210
404.307427	20320.255853	29.962228
404.939215	20356.316995	29.967245
405.121367	20380.949048	29.972263
405.604909	20420.717432	29.977280
407.023031	20430.826364	29.982298
407.464564	20451.690486	29.987316
407.812922	20468.685605	29.992333
408.272683	20480.743749	29.997351
408.613184	20507.733457	30.002368
408.605485	20531.845329	30.007386
408.789103	20562.549994	30.012404
409.246462	20592.597821	30.017421
409.466170	20622.815807	30.022439
410.063212	20645.246733	30.027456
409.595332	20688.546601	30.032474
410.008318	20712.508840	30.037492
410.409115	20761.315549	30.042509
410.927634	20800.714890	30.047527
411.428986	20842.855548	30.052544
411.653475	20898.670970	30.057562
412.272280	20933.089627	30.062580
412.409083	20984.046817	30.067597
413.010475	21012.974351	30.072615
413.356227	21047.644873	30.077632
414.064734	21093.764197	30.082650
414.205387	21131.557193	30.087668
414.637711	21173.101544	30.092685
415.507728	21199.905576	30.097703
416.433465	21223.585203	30.102720
417.091427	21259.276638	30.107738
417.770236	21264.341880	30.112756
418.030945	21297.172951	30.117773
418.227239	21321.761488	30.122791
418.582981	21350.558340	30.127808
418.689868	21383.091796	30.132826
419.378617	21405.625261	30.137844
419.691118	21422.154306	30.142861
420.222202	21456.590108	30.147879
420.639319	21479.436558	30.152896
420.931927	21513.358496	30.157914
421.614974	21531.473953	30.162932
421.629653	21547.505249	30.167949
421.928428	21561.246169	30.172967
422.305099	21595.966323	30.177984
422.095449	21632.441963	30.183002
422.426123	21662.570972	30.188020
423.014983	21707.357467	30.193037
422.979667	21746.215156	30.198055
423.772123	21766.269342	30.203072
423.853910	21827.911710	30.208090
424.395056	21862.747140	30.213108
425.169783	21901.701562	30.218125
425.005562	21946.813324	30.223143
425.602874	21991.561343	30.228160
426.250893	22031.536569	30.233178
426.693534	22067.063487	30.238196
427.172439	22102.485161	30.243213
427.557173	22153.064393	30.248231
428.395484	22185.931073	30.253248
428.909029	22226.581702	30.258266
429.109953	22263.624693	30.263284
429.659093	22301.040668	30.268301
430.063908	22341.608631	30.273319
430.592518	22375.382959	30.278336
430.630743	22422.375027	30.283354
431.034377	22457.084622	30.288372
431.445650	22499.668442	30.293389
431.858680	22545.969854	30.298407
432.729706	22588.605663	30.303424
432.895687	22627.269734	30.308442
433.513765	22646.976957	30.313460
434.249746	22683.811083	30.318477
434.945013	22722.714315	30.323495
435.722416	22755.144393	30.328512
436.177416	22783.785405	30.333530
436.417465	22808.113463	30.338548
436.699266	22835.819816	30.343565
436.675594	22881.584107	30.348583
437.475741	22907.943599	30.353600
437.803370	22951.664987	30.358618
438.196075	22984.469664	30.363636
438.662878	23012.136287	30.368653
438.580570	23062.251430	30.373671
439.195113	23100.738426	30.378688
439.649185	23143.873383	30.383706
440.791438	23159.516557	30.388724
442.158416	23177.758905	30.393741
442.328836	23204.930833	30.398759
442.910470	23223.474822	30.403776
442.970350	23244.359740	30.408794
443.682873	23272.162794	30.413812
443.840101	23290.947249	30.418829
444.036239	23316.142614	30.423847
444.191680	23336.360668	30.428864
444.438130	23387.359051	30.433882
444.806256	23429.052024	30.438900
445.139614	23458.059581	30.443917
445.033370	23497.565292	30.448935
445.815812	23542.843445	30.453952
446.215546	23582.565358	30.458970
446.794626	23625.089610	30.463988
447.202929	23672.877051	30.469005
447.633748	23714.929336	30.474023
447.877988	23744.095591	30.479040
448.385211	23793.148951	30.484058
448.726533	23845.176869	30.489076
449.406079	23881.532553	30.494093
449.854583	23934.744554	30.499111
449.815113	23968.097143	30.504128
450.353464	24009.854880	30.509146
450.796399	24043.448022	30.514164
451.463837	24093.062356	30.519181
451.796644	24135.362088	30.524199
452.506970	24176.760699	30.529216
452.933622	24220.047995	30.534234
453.232989	24247.969783	30.539252
453.573419	24305.193314	30.544269
453.806524	24335.302214	30.549287
454.316236	24382.846263	30.554304
454.920798	24431.450183	30.559322
455.077210	24469.345811	30.564340
455.791497	24515.926103	30.569357
455.851512	24575.199458	30.574375
456.619047	24611.896967	30.579392
457.012499	24667.876703	30.584410
457.528618	24707.324996	30.589428
457.898559	24765.450320	30.594445
458.470067	24817.919408	30.599463
458.993739	24859.005179	30.604480
459.658862	24909.311376	30.609498
460.049650	24943.831081	30.614516
460.942405	24999.702626	30.619533
461.006890	25042.003204	30.624551
461.595593	25100.645450	30.629568
461.935046	25131.953984	30.634586
462.445398	25180.165609	30.639604
462.434969	25228.189012	30.644621
462.875882	25270.959398	30.649639
464.066834	25315.750612	30.654656
464.378490	25367.819625	30.659674
464.660138	25423.260501	30.664692
465.132528	25467.776575	30.669709
465.550723	25522.018823	30.674727
466.146401	25559.596735	30.679744
466.932809	25605.724976	30.684762
467.292447	25655.579212	30.689780
468.270780	25691.233403	30.694797
469.035373	25722.277253	30.699815
470.106882	25750.712631	30.704832
470.520431	25771.513846	30.709850
471.013186	25792.853940	30.714868
472.523123	25800.580824	30.719885
473.139345	25820.146973	30.724903
473.369711	25831.810031	30.729920
473.744462	25841.566344	30.734938
473.853025	25852.492589	30.739956
474.130699	25872.524732	30.744973
474.491104	25894.454526	30.749991
474.307639	25927.841039	30.755008
474.554474	25960.156733	30.760026
474.358973	25991.687675	30.765044
475.262205	26036.911521	30.770061
475.023083	26077.448121	30.775079
475.590638	26131.858450	30.780096
476.364753	26188.073616	30.785114
476.508285	26229.257019	30.790132
476.824630	26280.000196	30.795149
477.528920	26327.528567	30.800167
477.983562	26374.757670	30.805184
478.576261	26422.024026	30.810202
478.949614	26474.101985	30.815220
479.335925	26516.116494	30.820237
479.942762	26573.224769	30.825255
480.110378	26619.382260	30.830272
480.868085	26665.092300	30.835290
481.111271	26722.727945	30.840308
481.546340	26774.115334	30.845325
481.853318	26815.787266	30.850343
482.357411	26875.815308	30.855360
482.809405	26917.192277	30.860378
483.333622	26952.794793	30.865396
484.493076	26986.384196	30.870413
484.991168	27036.222733	30.875431
485.608638	27076.774752	30.880448
486.184702	27107.669318	30.885466
486.852496	27149.960609	30.890484
487.321681	27179.024608	30.895501
487.781822	27217.010205	30.900519
488.533737	27252.575734	30.905536
489.023896	27290.373591	30.910554
488.984858	27326.413728	30.915572
489.832775	27354.472357	30.920589
490.250165	27405.094923	30.925607
490.325007	27444.008922	30.930624
490.794585	27492.109199	30.935642
491.245661	27536.828155	30.940660
491.752986	27580.045972	30.945677
491.965743	27623.694219	30.950695
492.053518	27678.895253	30.955712
492.683795	27731.183768	30.960730
492.871210	27795.528767	30.965748
493.275252	27849.804367	30.970765
494.413236	27907.901806	30.975783
494.833032	27960.001825	30.980800
495.890719	28002.946843	30.985818
495.956087	28067.543282	30.990836
496.499971	28110.573437	30.995853
497.497283	28162.241158	31.000871
497.468434	28215.535852	31.005888
498.380744	28252.950654	31.010906
498.744465	28307.739054	31.015924
499.509334	28346.244596	31.020941
499.775275	28399.115790	31.025959
500.169692	28449.344604	31.030976
500.923057	28488.385460	31.035994
501.130333	28539.241631	31.041012
501.661960	28583.167693	31.046029
502.129081	28634.407073	31.051047
502.460562	28693.242871	31.056064
503.039288	28739.495851	31.061082
503.722954	28797.403197	31.066100
504.008868	28836.291773	31.071117
504.690792	28895.887386	31.076135
504.673981	28948.485201	31.081152
505.969274	29002.809631	31.086170
506.129265	29065.514066	31.091188
506.757575	29117.680919	31.096205
507.577426	29151.728120	31.101223
508.579596	29192.795698	31.106240
509.351702	29220.727936	31.111258
509.917652	29264.527028	31.116276
510.648968	29297.652234	31.121293
511.294061	29327.608777	31.126311
511.697014	29352.349834	31.131328
512.099991	29382.160342	31.136346
512.420017	29414.366320	31.141364
512.864142	29445.949332	31.146381
513.295318	29486.310652	31.151399
513.145441	29534.616719	31.156416
513.830685	29574.888959	31.161434
514.347937	29626.627730	31.166452
514.721017	29674.472406	31.171469
515.157156	29713.063679	31.176487
515.864966	29764.455920	31.181504
516.968743	29785.949264	31.186522
517.971175	29805.336286	31.191540
518.472905	29821.440003	31.196557
519.038396	29862.795814	31.201575
519.060621	29891.181080	31.206592
519.603121	29904.054057	31.211610
519.742991	29945.272157	31.216628
520.097479	29976.167443	31.221645
520.382960	30004.755477	31.226663
520.413609	30051.162421	31.231680
521.158741	30106.972412	31.236698
521.630024	30152.155372	31.241716
521.631347	30201.365801	31.246733
521.976728	30250.532158	31.251751
522.508341	30315.485833	31.256768
523.150415	30375.610485	31.261786
523.469410	30438.763662	31.266804
523.512445	30507.079718	31.271821
524.263205	30560.606163	31.276839
524.603204	30631.974825	31.281856
525.499684	30688.509369	31.286874
525.794089	30750.326934	31.291892
526.423159	30815.821622	31.296909
527.066430	30884.049472	31.301927
527.729259	30954.230378	31.306944
528.505957	31008.684599	31.311962
528.888014	31068.504390	31.316980
529.530446	31128.448588	31.321997
530.243937	31196.218061	31.327015
530.489953	31252.568460	31.332032
531.383690	31314.427840	31.337050
531.906378	31364.243199	31.342068
532.648608	31427.566658	31.347085
533.268981	31487.938495	31.352103
533.849037	31545.752201	31.357120
534.398844	31588.307271	31.362138
535.166835	31645.159544	31.367156
535.399894	31701.374705	31.372173
535.740893	31754.199505	31.377191
536.226164	31813.831264	31.382208
536.785383	31866.386887	31.387226
537.295082	31925.860395	31.392244
537.719537	31991.185038	31.397261
538.332778	32048.676259	31.402279
539.086373	32109.662397	31.407296
539.889760	32159.181243	31.412314
540.494487	32220.492088	31.417332
540.769619	32270.082721	31.422349
541.767425	32313.458448	31.427367
542.375109	32370.459441	31.432384
543.241930	32416.097196	31.437402
543.563763	32462.096426	31.442420
544.290802	32505.451091	31.447437
545.175706	32537.266626	31.452455
545.262567	32603.646331	31.457472
545.612959	32638.604535	31.462490
546.865551	32672.953137	31.467508
547.426464	32718.374013	31.472525
548.303856	32741.814138	31.477543
548.636809	32784.701355	31.482560
548.867889	32819.701712	31.487578
549.258201	32861.989620	31.492596
549.419029	32906.278079	31.497613
550.229255	32947.269454	31.502631
550.839304	33006.641692	31.507648
551.172189	33050.756955	31.512666
551.247856	33102.358058	31.517684
551.588462	33156.313555	31.522701
552.383352	33202.372258	31.527719
552.946910	33262.002299	31.532736
553.270473	33313.869137	31.537754
553.709536	33362.555438	31.542772
554.063454	33415.493519	31.547789
554.671699	33460.233249	31.552807
556.790483	33478.840469	31.557824
557.959404	33507.199944	31.562842
558.688917	33534.941023	31.567860
558.959178	33565.481056	31.572877
559.786452	33585.661656	31.577895
560.317996	33619.812514	31.582912
560.376308	33644.910007	31.587930
561.037812	33675.360366	31.592948
561.240090	33711.269678	31.597965
561.703331	33735.801871	31.602983
561.775026	33777.317888	31.608000
562.408433	33827.374357	31.613018
562.554536	33872.936133	31.618036
563.196813	33918.173109	31.623053
564.336075	33957.717800	31.628071
564.710836	34007.672349	31.633088
565.214901	34050.777342	31.638106
565.434214	34091.837420	31.643124
565.584649	34149.667514	31.648141
566.341041	34210.449037	31.653159
566.843537	34275.084502	31.658176
567.290039	34321.493966	31.663194
567.520990	34381.302618	31.668212
568.167220	34438.770927	31.673229
568.723604	34501.861592	31.678247
569.153990	34569.028129	31.683264
569.776837	34639.119862	31.688282
570.606045	34708.310014	31.693300
571.151079	34770.103422	31.698317
571.933931	34828.809492	31.703335
572.456844	34882.004880	31.708352
572.987967	34933.772748	31.713370
573.415727	35003.819249	31.718388
573.813074	35072.242756	31.723405
574.719168	35130.440346	31.728423
575.125410	35199.910538	31.733440
575.645154	35263.189821	31.738458
576.429438	35320.398346	31.743476
576.530441	35404.959581	31.748493
577.679105	35461.360483	31.753511
578.396029	35528.101471	31.758528
579.052604	35580.336471	31.763546
580.024051	35638.010546	31.768564
580.702398	35685.032189	31.773581
581.774578	35716.948744	31.778599
582.160149	35770.857414	31.783616
582.865452	35821.728110	31.788634
583.238614	35863.647308	31.793652
583.925538	35912.214448	31.798669
584.702044	35964.039450	31.803687
584.574230	36004.687899	31.808704
585.553787	36060.178206	31.813722
586.451668	36108.423861	31.818740
586.707112	36156.223487	31.823757
587.315827	36201.563327	31.828775
587.810884	36245.344147	31.833792
588.173182	36291.614853	31.838810
589.171620	36342.946704	31.843828
589.638436	36400.804418	31.848845
590.039110	36444.945301	31.853863
590.830382	36504.920986	31.858880
590.991839	36559.500215	31.863898
591.632209	36613.871121	31.868916
591.685152	36669.465864	31.873933
592.494812	36716.115069	31.878951
592.816854	36772.811276	31.883968
592.953524	36833.675683	31.888986
593.572506	36899.560614	31.894004
594.328405	36966.404670	31.899021
594.740963	37015.537688	31.904039
595.361817	37083.225029	31.909056
595.572787	37151.359038	31.914074
595.961405	37222.408496	31.919092
596.356507	37309.167719	31.924109
597.154529	37381.308438	31.929127
597.864718	37459.031180	31.934144
598.153994	37533.954936	31.939162
599.656010	37596.354331	31.944180
600.344261	37658.822067	31.949197
601.252348	37727.480641	31.954215
602.094601	37781.316760	31.959232
602.063775	37854.527309	31.964250
603.231089	37901.148923	31.969268
603.632252	37972.691616	31.974285
604.299343	38038.522268	31.979303
604.881011	38108.830047	31.984320
605.304369	38178.987502	31.989338
605.905830	38242.771926	31.994356
606.287149	38304.336271	31.999373
606.982914	38371.902451	32.004391
607.729925	38443.857002	32.009408
608.111647	38519.659621	32.014426
609.068573	38582.057769	32.019444
609.577215	38660.263992	32.024461
609.897675	38731.864044	32.029479
610.832505	38799.827899	32.034496
612.116430	38844.141247	32.039514
613.477163	38889.076430	32.044532
614.106071	38949.465816	32.049549
614.914560	38996.632435	32.054567
615.492271	39045.548007	32.059584
615.646507	39092.920776	32.064602
616.540530	39140.733312	32.069620
616.998235	39181.244859	32.074637
617.614707	39237.676071	32.079655
618.126862	39289.377545	32.084672
618.686647	39352.863438	32.089690
619.180288	39402.137897	32.094708
619.461771	39462.444333	32.099725
620.116240	39522.446325	32.104743
620.780124	39591.969805	32.109760
620.847265	39658.315755	32.114778
621.935974	39720.825469	32.119796
623.065514	39766.646934	32.124813
623.879228	39815.863340	32.129831
624.448966	39871.483564	32.134848
625.150764	39921.097511	32.139866
625.715360	39980.525600	32.144884
625.544547	40038.882192	32.149901
626.374210	40093.639483	32.154919
626.683030	40161.386703	32.159936
627.540787	40223.065093	32.164954
628.130891	40281.846023	32.169972
629.123105	40329.269844	32.174989
629.939729	40393.916425	32.180007
630.286310	40438.139110	32.185024
630.615450	40500.969498	32.190042
631.410222	40562.185953	32.195060
632.080283	40633.278038	32.200077
632.744209	40689.090376	32.205095
633.545088	40738.996372	32.210112
633.774000	40801.904322	32.215130
634.212924	40847.965674	32.220148
634.475730	40913.311626	32.225165
634.733566	40986.667018	32.230183
635.507742	41052.784461	32.235200
635.708220	41133.719557	32.240218
636.321253	41207.929447	32.245236
636.921892	41280.329744	32.250253
637.279392	41358.632475	32.255271
637.747244	41438.454634	32.260288
638.303139	41527.739099	32.265306
639.662425	41588.938359	32.270324
641.380622	41649.384064	32.275341
641.676939	41714.894642	32.280359
642.928307	41781.781915	32.285376
642.968079	41854.501235	32.290394
643.602270	41922.396946	32.295412
644.090223	41994.780788	32.300429
644.796851	42075.841630	32.305447
645.601758	42136.180912	32.310464
646.209952	42209.322319	32.315482
647.723802	42252.254860	32.320500
648.897281	42295.316321	32.325517
649.476705	42343.429121	32.330535
650.059763	42400.882650	32.335552
650.450307	42460.458012	32.340570
650.939973	42523.575023	32.345588
651.476748	42577.573626	32.350605
651.678365	42645.486617	32.355623
652.700904	42698.114168	32.360640
652.951167	42760.807458	32.365658
653.349708	42836.214776	32.370676
654.457680	42903.246615	32.375693
654.791514	42977.885426	32.380711
655.236033	43056.269391	32.385728
655.764494	43132.625656	32.390746
656.263156	43203.051966	32.395764
656.948540	43282.066395	32.400781
657.387848	43385.118499	32.405799
658.319747	43441.838886	32.410816
658.721010	43529.267493	32.415834
659.245433	43612.401478	32.420852
659.728444	43701.449608	32.425869
660.287555	43802.912009	32.430887
661.205537	43890.165422	32.435904
661.981744	43990.607969	32.440922
662.446588	44066.009335	32.445940
663.175003	44157.456450	32.450957
663.631084	44244.544706	32.455975
664.756600	44331.724874	32.460992
665.476581	44409.945928	32.466010
665.857375	44494.733544	32.471028
666.845516	44575.357864	32.476045
667.730456	44664.202145	32.481063
668.674538	44745.184932	32.486080
669.039271	44829.256862	32.491098
669.687274	44901.777170	32.496116
670.621998	44984.505373	32.501133
670.934507	45067.248296	32.506151
671.743059	45140.314492	32.511168
672.231711	45228.226026	32.516186
672.750866	45311.273738	32.521204
674.138056	45391.160003	32.526221
674.659821	45472.496696	32.531239
675.043806	45557.279133	32.536256
675.706518	45632.619417	32.541274
676.300237	45704.570836	32.546292
677.148759	45791.841457	32.551309
677.733018	45865.361153	32.556327
678.951166	45932.414133	32.561344
679.302647	46016.806173	32.566362
680.113382	46078.650791	32.571380
681.016333	46133.300203	32.576397
681.924984	46196.243641	32.581415
682.387299	46260.246151	32.586432
682.814481	46329.903527	32.591450
683.472573	46410.700778	32.596468
683.942477	46490.035924	32.601485
684.409778	46574.594479	32.606503
684.782491	46651.268722	32.611520
685.480418	46729.042098	32.616538
686.132078	46818.484545	32.621556
686.741237	46899.039363	32.626573
687.202030	46996.506162	32.631591
688.163176	47085.510374	32.636608
688.625224	47179.327643	32.641626
689.583404	47272.520320	32.646644
690.470712	47349.039789	32.651661
691.069912	47437.366528	32.656679
692.324275	47514.694427	32.661696
692.951340	47595.460828	32.666714
693.229179	47696.801284	32.671732
694.194045	47770.167667	32.676749
694.860615	47863.105108	32.681767
695.742031	47941.892093	32.686784
696.549784	48035.852303	32.691802
697.151728	48118.301889	32.696820
697.761368	48192.609611	32.701837
698.503039	48279.246243	32.706855
699.306443	48365.446762	32.711872
699.683765	48453.401197	32.716890
700.304540	48553.486436	32.721908
700.948442	48639.613486	32.726925
701.547422	48737.442214	32.731943
702.195888	48827.200998	32.736960
703.121226	48925.096798	32.741978
703.603613	49031.286509	32.746996
703.919422	49127.187098	32.752013
705.090171	49231.719980	32.757031
705.540940	49322.271671	32.762048
706.227911	49409.926742	32.767066
706.716773	49515.265401	32.772084
707.629152	49622.938008	32.777101
708.473882	49712.551698	32.782119
708.979060	49814.898587	32.787136
710.161417	49915.476169	32.792154
710.720906	50012.834761	32.797172
711.786189	50102.221207	32.802189
712.440099	50198.813507	32.807207
714.351042	50271.698532	32.812224
715.114863	50354.923767	32.817242
715.946729	50432.311198	32.822260
716.790441	50507.249352	32.827277
717.363110	50580.204963	32.832295
717.991683	50644.156891	32.837312
718.746379	50716.801876	32.842330
718.935088	50797.723719	32.847348
719.925650	50864.026373	32.852365
720.338443	50955.015265	32.857383
721.017858	51037.136196	32.862400
721.879416	51111.268388	32.867418
722.344688	51202.764594	32.872436
722.683052	51274.460292	32.877453
723.356739	51380.928318	32.882471
724.158447	51469.742460	32.887488
725.480197	51534.975732	32.892506
726.363410	51610.991841	32.897524
727.547360	51668.955538	32.902541
728.022249	51732.172123	32.907559
728.500646	51799.500637	32.912576
729.562200	51871.246524	32.917594
729.680456	51941.553425	32.922612
730.048472	52016.582331	32.927629
730.889125	52094.995190	32.932647
731.550085	52172.250442	32.937664
732.662743	52256.677064	32.942682
732.706727	52327.882019	32.947700
733.556208	52418.657246	32.952717
733.730277	52522.753560	32.957735
734.259017	52612.376088	32.962752
734.954292	52715.123930	32.967770
735.873238	52815.504322	32.972788
736.311916	52901.365354	32.977805
737.054192	53003.190957	32.982823
737.864552	53108.398253	32.987840
738.889742	53208.188253	32.992858
739.177422	53323.837181	32.997876
739.963162	53421.962124	33.002893
740.894737	53525.616525	33.007911
741.989271	53634.734471	33.012928
742.786189	53725.688742	33.017946
743.101722	53833.969864	33.022964
744.491965	53933.355832	33.027981
744.970378	54040.511941	33.032999
745.602697	54130.591860	33.038016
746.829575	54223.088450	33.043034
747.852567	54325.664319	33.048052
749.120604	54414.604462	33.053069
749.776404	54493.253373	33.058087
750.012191	54586.136469	33.063104
751.171455	54666.762541	33.068122
752.396457	54757.057047	33.073140
753.440986	54828.175404	33.078157
754.588194	54901.229297	33.083175
754.998440	54988.885857	33.088192
755.676848	55061.910359	33.093210
755.848686	55152.026795	33.098228
756.566800	55232.146790	33.103245
757.485159	55317.964505	33.108263
757.990524	55418.218083	33.113280
758.712936	55511.170513	33.118298
759.166235	55594.633764	33.123316
759.864474	55687.799518	33.128333
760.622673	55784.689861	33.133351
761.348686	55880.992082	33.138368
762.126360	55973.305746	33.143386
762.748828	56082.736423	33.148404
763.449036	56177.098320	33.153421
765.138125	56255.280376	33.158439
765.740058	56356.546351	33.163456
766.538758	56440.360522	33.168474
767.263369	56518.702890	33.173492
767.754663	56620.519235	33.178509
768.212919	56718.082899	33.183527
768.547939	56819.774431	33.188544
769.554488	56911.865131	33.193562
770.678015	57014.274139	33.198580
771.780950	57094.856279	33.203597
772.628387	57187.309421	33.208615
773.610905	57280.385193	33.213632
774.645770	57363.968397	33.218650
775.137320	57465.277225	33.223668
776.144499	57532.354891	33.228685
776.623146	57621.749496	33.233703
777.323342	57707.443013	33.238720
778.021564	57789.901985	33.243738
778.724189	57866.174416	33.248756
779.438931	57941.345653	33.253773
780.536333	58025.136155	33.258791
780.760569	58108.287650	33.263808
781.604976	58190.389238	33.268826
782.004295	58286.093605	33.273844
782.684942	58381.315962	33.278861
783.547402	58482.733012	33.283879
783.841686	58585.015327	33.288896
784.396453	58669.833368	33.293914
785.492121	58788.098116	33.298932
786.103623	58896.244359	33.303949
786.583296	59005.063834	33.308967
786.915314	59126.553098	33.313984
787.760085	59245.544458	33.319002
788.893971	59357.227880	33.324020
790.137545	59465.538233	33.329037
790.926333	59573.835799	33.334055
791.735497	59687.375707	33.339072
792.597638	59789.835815	33.344090
793.820041	59903.586764	33.349108
794.432902	60007.492072	33.354125
795.538089	60111.127032	33.359143
796.410087	60204.917193	33.364160
797.834390	60285.547624	33.369178
799.357735	60374.156370	33.374196
800.010959	60469.348932	33.379213
800.889051	60560.175816	33.384231
801.366473	60665.452978	33.389248
802.378645	60741.685240	33.394266
803.003433	60827.252879	33.399284
803.737888	60910.761472	33.404301
804.776603	60992.659169	33.409319
805.372233	61095.416397	33.414336
806.170143	61187.460117	33.419354
806.911241	61287.451465	33.424372
807.497304	61384.106688	33.429389
807.735867	61483.651108	33.434407
808.402227	61583.763698	33.439424
809.047693	61693.967035	33.444442
809.528081	61804.381511	33.449460
810.230139	61927.918482	33.454477
811.352404	62035.415767	33.459495
811.964309	62159.417762	33.464512
812.843871	62269.857334	33.469530
813.852555	62379.454549	33.474548
814.721643	62485.965817	33.479565
815.238172	62609.404833	33.484583
816.396935	62722.701791	33.489600
817.804154	62818.311783	33.494618
819.001285	62906.422960	33.499636
820.420289	62997.316807	33.504653
821.654593	63081.870508	33.509671
822.422696	63167.911014	33.514688
823.199172	63248.622289	33.519706
824.902106	63317.519472	33.524724
826.350433	63359.109807	33.529741
828.411442	63386.358793	33.534759
829.500811	63444.656986	33.539776
830.016583	63488.139736	33.544794
830.379171	63552.291037	33.549812
830.606777	63599.784642	33.554829
831.739548	63644.922985	33.559847
832.126677	63696.189188	33.564864
832.506376	63763.669321	33.569882
832.967770	63822.116527	33.574900
833.420069	63893.067810	33.579917
833.830240	63957.692898	33.584935
833.972772	64050.831167	33.589952
834.640294	64122.992899	33.594970
835.391894	64202.972509	33.599988
835.646624	64297.920089	33.605005
836.882610	64391.454545	33.610023
837.014093	64484.078285	33.615040
837.427375	64595.467047	33.620058
837.973465	64699.653845	33.625076
838.368447	64821.034000	33.630093
839.317134	64940.926486	33.635111
839.754095	65070.467979	33.640128
840.211710	65191.732510	33.645146
840.875059	65325.719903	33.650164
841.505316	65489.233715	33.655181
842.681123	65617.126894	33.660199
843.029749	65771.845996	33.665216
843.964172	65914.996265	33.670234
844.909206	66061.255897	33.675252
845.733945	66215.899690	33.680269
846.632357	66354.501174	33.685287
847.165073	66513.051501	33.690304
848.554238	66651.308424	33.695322
849.894799	66790.984012	33.700340
850.643035	66928.286572	33.705357
852.272488	67059.906720	33.710375
853.274185	67202.390956	33.715392
854.043889	67337.081780	33.720410
855.141257	67459.461355	33.725428
856.007549	67587.999360	33.730445
857.282087	67720.719060	33.735463
858.158151	67849.174870	33.740480
858.775077	67972.110917	33.745498
860.138728	68091.965684	33.750516
861.011477	68210.606174	33.755533
862.500294	68324.985682	33.760551
863.891463	68430.050496	33.765568
864.923546	68526.614947	33.770586
865.839024	68628.509718	33.775604
866.819969	68723.932884	33.780621
868.054650	68813.757348	33.785639
868.885015	68911.166117	33.790656
869.478169	68993.301932	33.795674
870.457045	69108.838370	33.800692
871.034909	69214.629369	33.805709
871.304994	69308.320107	33.810727
872.065891	69415.257850	33.815744
873.105724	69527.340801	33.820762
874.430123	69633.168691	33.825780
874.823191	69759.692714	33.830797
875.970593	69872.834561	33.835815
876.321864	69969.018545	33.840832
877.137154	70083.423964	33.845850
878.022214	70184.041451	33.850868
878.704988	70310.767508	33.855885
879.440710	70431.769847	33.860903
879.935246	70560.602323	33.865920
880.296699	70693.169028	33.870938
881.479820	70824.993897	33.875956
882.135231	70951.481697	33.880973
882.897150	71074.222148	33.885991
883.890501	71230.152154	33.891008
884.610067	71370.238828	33.896026
885.419304	71497.083840	33.901044
886.073758	71646.471601	33.906061
886.689710	71778.263220	33.911079
887.855073	71921.884071	33.916096
888.768068	72062.929752	33.921114
889.639740	72190.015163	33.926132
890.625821	72315.944249	33.931149
891.589208	72436.939321	33.936167
892.299839	72582.150943	33.941184
893.017126	72718.402207	33.946202
893.754985	72856.263410	33.951220
895.044780	72987.141786	33.956237
896.443241	73111.350693	33.961255
897.706830	73236.404645	33.966272
899.440491	73344.402919	33.971290
901.611872	73443.457453	33.976308
902.694872	73547.687814	33.981325
903.595002	73628.741057	33.986343
904.421758	73735.278499	33.991360
904.994664	73821.451763	33.996378
905.879108	73914.460479	34.001396
906.462201	74021.981800	34.006413
907.219340	74126.578618	34.011431
907.662981	74230.987397	34.016448
908.296766	74342.138136	34.021466
909.196938	74454.358465	34.026484
910.164298	74591.421321	34.031501
911.010410	74703.702455	34.036519
912.036716	74830.139149	34.041536
912.630795	74955.749928	34.046554
913.449824	75075.670568	34.051572
913.955029	75208.032612	34.056589
914.872755	75335.761313	34.061607
915.842166	75464.177887	34.066624
916.523022	75594.565423	34.071642
916.962951	75739.343268	34.076660
917.748595	75888.618489	34.081677
919.001384	76038.462681	34.086695
920.006213	76182.334341	34.091712
920.614112	76323.356917	34.096730
921.358136	76466.166722	34.101748
922.297128	76631.144324	34.106765
923.578675	76782.728092	34.111783
924.608513	76921.376372	34.116800
925.217817	77071.814527	34.121818
925.869498	77221.051344	34.126836
926.789585	77392.811514	34.131853
927.903043	77544.080410	34.136871
928.781956	77698.450282	34.141888
929.966115	77857.116020	34.146906
931.125876	78014.224669	34.151924
931.718804	78168.411013	34.156941
932.818137	78316.031689	34.161959
933.912355	78458.942032	34.166976
934.855596	78619.367088	34.171994
935.681757	78764.815741	34.177012
936.721637	78921.805126	34.182029
937.391836	79090.564639	34.187047
938.841987	79228.848025	34.192064
939.246617	79394.440449	34.197082
940.095370	79535.443706	34.202100
940.670639	79700.934322	34.207117
941.886783	79855.744212	34.212135
943.306468	80017.226580	34.217152
944.193398	80173.509930	34.222170
944.980788	80337.483723	34.227188
946.423365	80497.593122	34.232205
947.341639	80642.077279	34.237223
948.109815	80790.730481	34.242240
949.139958	80938.620278	34.247258
950.131330	81086.568053	34.252276
950.687202	81244.729004	34.257293
951.872265	81393.981566	34.262311
953.145268	81532.194531	34.267328
953.880284	81675.001242	34.272346
954.820862	81810.076186	34.277364
955.750481	81963.043753	34.282381
956.466731	82095.759872	34.287399
957.650695	82240.349561	34.292416
958.289684	82385.700720	34.297434
959.508960	82538.548430	34.302452
960.400925	82685.915753	34.307469
961.394105	82831.242913	34.312487
962.901513	82958.304287	34.317504
964.146570	83094.538599	34.322522
965.410177	83214.360033	34.327540
966.337408	83344.657234	34.332557
967.282394	83491.249188	34.337575
968.453733	83626.467635	34.342592
969.192672	83757.532150	34.347610
970.206702	83892.151812	34.352628
971.235538	84029.142298	34.357645
971.991139	84169.854492	34.362663
972.840056	84317.941705	34.367680
973.657828	84474.196489	34.372698
974.484068	84623.548434	34.377716
975.674270	84755.227432	34.382733
976.408111	84899.832342	34.387751
977.572531	85052.522422	34.392768
978.449333	85208.797751	34.397786
979.361718	85351.958785	34.402804
980.625727	85495.840875	34.407821
981.540989	85655.618037	34.412839
982.762206	85795.738137	34.417856
983.983968	85934.568261	34.422874
985.392370	86072.647107	34.427892
986.302974	86209.454940	34.432909
987.037040	86344.843787	34.437927
988.029614	86484.006090	34.442944
988.730588	86635.954252	34.447962
989.456454	86786.026397	34.452980
990.255722	86940.390021	34.457997
991.346567	87103.621892	34.463015
992.359771	87250.606087	34.468032
993.305581	87407.726371	34.473050
994.532463	87565.807390	34.478068
995.244216	87723.550572	34.483085
996.106333	87890.723506	34.488103
997.374168	88022.306966	34.493120
998.076951	88188.223804	34.498138
999.246700	88353.261090	34.503156
1000.149626	88527.272146	34.508173
1001.195016	88674.538376	34.513191
1002.400857	88832.283361	34.518208
1003.341209	88990.895866	34.523226
1004.270859	89143.974211	34.528244
1005.278224	89308.102120	34.533261
1006.448085	89468.097417	34.538279
1007.375161	89621.907008	34.543296
1008.457706	89783.671741	34.548314
1009.729272	89933.920682	34.553332
1011.021556	90085.432802	34.558349
1011.410399	90242.341188	34.563367
1012.798786	90393.061024	34.568384
1013.678142	90551.238399	34.573402
1014.744831	90704.139646	34.578420
1015.759352	90862.176529	34.583437
1016.724421	91006.192362	34.588455
1017.989622	91155.152721	34.593472
1019.081832	91319.033687	34.598490
1020.031274	91464.200330	34.603508
1021.005190	91601.573249	34.608525
1021.636609	91733.719052	34.613543
1022.899573	91874.292426	34.618560
1024.544837	92001.101763	34.623578
1025.539431	92141.113446	34.628596
1026.451716	92287.436712	34.633613
1027.431930	92416.933870	34.638631
1028.890082	92555.941094	34.643648
1029.760487	92693.906945	34.648666
1030.714708	92810.334938	34.653684
1032.105086	92945.988593	34.658701
1032.677475	93082.999555	34.663719
1033.562877	93232.200040	34.668736
1034.324937	93385.231931	34.673754
1034.977832	93529.732127	34.678772
1035.807693	93677.178686	34.683789
1037.098610	93841.189566	34.688807
1037.664491	93986.491668	34.693824
1038.452053	94158.366457	34.698842
1039.872598	94327.954332	34.703860
1040.784778	94476.176982	34.708877
1041.835378	94653.917166	34.713895
1043.039141	94813.398112	34.718912
1044.108289	94976.662058	34.723930
1044.770876	95141.114545	34.728948
1045.874404	95321.439633	34.733965
1046.675627	95493.169639	34.738983
1048.188597	95656.947175	34.744000
1049.402471	95820.072578	34.749018
1050.810754	95985.034255	34.754036
1051.931163	96160.817930	34.759053
1052.908941	96326.910049	34.764071
1053.824357	96485.398694	34.769088
1054.805944	96656.303133	34.774106
1055.847663	96829.091495	34.779124
1056.984653	96998.535732	34.784141
1057.598383	97178.853982	34.789159
1058.633216	97353.305618	34.794176
1060.187408	97524.108850	34.799194
1061.106610	97693.416538	34.804212
1062.898753	97855.826877	34.809229
1063.443386	98034.288976	34.814247
1064.956245	98193.050720	34.819264
1065.940828	98366.574528	34.824282
1067.104889	98538.177111	34.829300
1068.152880	98710.559690	34.834317
1068.926730	98880.424849	34.839335
1069.804754	99029.623670	34.844352
1070.813710	99210.283838	34.849370
1071.856589	99385.172483	34.854388
1072.803520	99562.198964	34.859405
1074.302136	99732.444027	34.864423
1076.399133	99895.285741	34.869440
1078.588679	100035.107052	34.874458
1079.220238	100183.600032	34.879476
1080.269066	100319.793732	34.884493
1081.170625	100476.974149	34.889511
1081.805173	100613.592351	34.894528
1083.043825	100775.612802	34.899546
1084.282928	100932.961908	34.904564
1084.741190	101085.876188	34.909581
1085.570398	101258.761793	34.914599
1086.393129	101414.897400	34.919616
1087.430172	101589.675612	34.924634
1088.360969	101758.970712	34.929652
1089.233298	101921.299513	34.934669
1090.388962	102085.418655	34.939687
1092.023352	102240.861833	34.944704
1092.976868	102398.830617	34.949722
1093.695598	102560.536693	34.954740
1094.631580	102711.311451	34.959757
1095.687689	102882.745991	34.964775
1096.891495	103042.032357	34.969792
1097.785883	103219.042278	34.974810
1098.624728	103394.093441	34.979828
1099.448579	103569.458519	34.984845
1100.289324	103750.450905	34.989863
1101.340202	103927.952719	34.994880
1102.494479	104118.653185	34.999898
1103.029192	104309.514317	35.004916
1103.726258	104497.241080	35.009933
1104.554556	104715.701871	35.014951
1105.565751	104920.241857	35.019968
1106.670802	105134.031766	35.024986
1107.608818	105344.773589	35.030004
1108.831483	105558.408246	35.035021
1110.138011	105765.863220	35.040039
1111.599795	105983.527157	35.045056
1112.930672	106197.035174	35.050074
1113.931185	106405.204278	35.055092
1115.427711	106614.154357	35.060109
1116.458426	106823.018343	35.065127
1117.794847	107022.271406	35.070144
1119.189600	107234.346131	35.075162
1120.815840	107423.916206	35.080180
1122.441211	107617.072069	35.085197
1123.579020	107821.936681	35.090215
1125.413303	107988.881344	35.095232
1126.949109	108162.348442	35.100250
1127.895107	108346.312550	35.105268
1128.902151	108518.969993	35.110285
1129.834883	108707.042483	35.115303
1130.811203	108905.938475	35.120320
1131.552629	109083.671789	35.125338
1132.396322	109281.629845	35.130356
1133.276763	109474.833466	35.135373
1134.216048	109667.914766	35.140391
1135.408229	109871.722136	35.145408
1136.361394	110085.906361	35.150426
1137.275964	110305.418626	35.155444
1138.440248	110526.234122	35.160461
1139.252118	110739.648848	35.165479
1140.127447	110953.156112	35.170496
1141.668384	111167.125197	35.175514
1142.390312	111393.708257	35.180532
1143.501443	111597.288648	35.185549
1144.558944	111841.946808	35.190567
1145.891048	112064.951210	35.195584
1147.279415	112288.239496	35.200602
1148.551594	112519.770070	35.205620
1149.907274	112730.171712	35.210637
1151.324293	112951.421164	35.215655
1152.538705	113173.009871	35.220672
1153.760648	113375.356387	35.225690
1155.268693	113596.786017	35.230708
1156.667794	113794.659853	35.235725
1157.693702	114000.223027	35.240743
1159.702115	114181.023522	35.245760
1161.263694	114377.164467	35.250778
1162.058769	114571.393686	35.255796
1163.451236	114765.322950	35.260813
1164.349626	114955.496493	35.265831
1166.238083	115143.138831	35.270848
1168.279060	115290.786873	35.275866
1169.868243	115449.722304	35.280884
1171.221526	115590.542856	35.285901
1172.235113	115732.611084	35.290919
1173.071090	115880.017727	35.295936
1173.976512	116025.031866	35.300954
1174.973528	116185.830242	35.305972
1176.203618	116329.512761	35.310989
1177.579451	116489.426833	35.316007
1178.111028	116634.581839	35.321024
1179.456042	116785.481997	35.326042
1180.004079	116970.735215	35.331060
1180.972419	117134.204357	35.336077
1181.927415	117316.617993	35.341095
1182.402099	117499.631551	35.346112
1183.713120	117681.114539	35.351130
1184.347932	117884.515463	35.356148
1185.165122	118073.469111	35.361165
1186.142261	118293.655067	35.366183
1187.491718	118494.636393	35.371200
1189.608347	118688.587123	35.376218
1191.102391	118870.123487	35.381236
1191.986805	119067.004332	35.386253
1193.105757	119269.891720	35.391271
1194.437380	119465.155652	35.396288
1195.732030	119654.306996	35.401306
1197.175832	119866.090577	35.406324
1198.064513	120068.096615	35.411341
1199.015244	120262.275749	35.416359
1199.899662	120474.764332	35.421376
1201.211084	120682.470269	35.426394
1202.004884	120907.496209	35.431412
1203.058839	121133.215891	35.436429
1204.239971	121346.789629	35.441447
1205.413276	121569.033642	35.446464
1206.442305	121785.144680	35.451482
1207.576020	122023.669230	35.456500
1208.982560	122245.955912	35.461517
1209.854337	122486.187481	35.466535
1210.617129	122709.255540	35.471552
1212.102651	122968.752807	35.476570
1213.037051	123210.411902	35.481588
1214.147262	123458.519587	35.486605
1215.639898	123703.930326	35.491623
1216.562738	123949.525852	35.496640
1218.348037	124186.338198	35.501658
1219.745468	124432.683102	35.506676
1220.744730	124677.879152	35.511693
1222.187488	124920.786213	35.516711
1223.040589	125170.864221	35.521728
1224.830451	125416.265316	35.526746
1226.745644	125646.274875	35.531764
1228.339684	125869.457488	35.536781
1229.524294	126089.300134	35.541799
1230.714579	126314.897296	35.546816
1232.510168	126542.791573	35.551834
1233.468923	126776.921826	35.556852
1234.714157	126998.383314	35.561869
1235.813386	127217.411743	35.566887
1236.769199	127465.970868	35.571904
1238.213476	127671.574357	35.576922
1239.321846	127898.426174	35.581940
1240.237228	128124.804546	35.586957
1242.190084	128348.845997	35.591975
1243.123395	128573.564350	35.596992
1244.886639	128793.014095	35.602010
1246.386921	129014.029781	35.607028
1247.679975	129230.505614	35.612045
1249.121345	129435.550997	35.617063
1250.090337	129641.689709	35.622080
1251.594964	129847.069597	35.627098
1252.871317	130048.381744	35.632116
1253.816124	130251.144198	35.637133
1254.974290	130445.038006	35.642151
1255.736177	130658.493300	35.647168
1256.623902	130854.031389	35.652186
1257.643691	131080.553514	35.657204
1258.835541	131299.734973	35.662221
1259.661698	131522.248680	35.667239
1260.627501	131768.267411	35.672256
1261.890587	131992.208071	35.677274
1263.174861	132227.491932	35.682292
1264.541721	132468.265380	35.687309
1265.968726	132702.223554	35.692327
1267.030727	132947.905974	35.697344
1268.510930	133180.464477	35.702362
1269.486197	133408.392327	35.707380
1270.963725	133661.389417	35.712397
1272.262754	133912.262912	35.717415
1273.375260	134156.818039	35.722432
1274.483120	134404.899987	35.727450
1275.759754	134660.587580	35.732468
1277.251876	134902.791155	35.737485
1278.965584	135151.767657	35.742503
1279.734536	135400.724520	35.747520
1281.282878	135652.685980	35.752538
1282.471403	135907.662647	35.757556
1283.923213	136156.398477	35.762573
1285.572786	136421.571956	35.767591
1286.075531	136677.098848	35.772608
1287.593472	136923.940586	35.777626
1288.762823	137186.575163	35.782644
1289.729727	137452.719057	35.787661
1291.469920	137724.303215	35.792679
1292.830517	137984.440303	35.797696
1294.464252	138244.597741	35.802714
1296.069076	138494.974143	35.807732
1297.004422	138746.984360	35.812749
1298.423091	139010.898114	35.817767
1299.639429	139269.560264	35.822784
1301.060852	139526.618371	35.827802
1302.685304	139789.363177	35.832820
1303.669841	140047.296143	35.837837
1305.573183	140295.709482	35.842855
1307.117875	140556.115081	35.847872
1308.622053	140789.687041	35.852890
1310.297442	141029.965164	35.857908
1311.754772	141272.132191	35.862925
1313.266628	141500.395011	35.867943
1314.720940	141744.696073	35.872960
1316.061156	141982.512942	35.877978
1317.835932	142188.154140	35.882996
1319.848041	142405.258165	35.888013
1321.245169	142613.906000	35.893031
1322.636923	142836.567565	35.898048
1323.385912	143056.445551	35.903066
1324.773749	143280.505445	35.908084
1325.440173	143508.071519	35.913101
1326.916045	143729.190600	35.918119
1327.805253	143958.447393	35.923136
1329.231220	144192.854214	35.928154
1330.258470	144429.889922	35.933172
1331.378408	144680.645277	35.938189
1332.894173	144911.072977	35.943207
1334.146653	145134.266742	35.948224
1335.434144	145376.896243	35.953242
1336.460817	145629.144741	35.958260
1337.406120	145867.776104	35.963277
1338.552617	146085.515052	35.968295
1339.724298	146319.381944	35.973312
1340.814423	146556.345435	35.978330
1341.762707	146798.444588	35.983348
1343.355372	147059.867365	35.988365
1344.678783	147303.036684	35.993383
1345.948390	147547.497394	35.998400
1347.380091	147793.454842	36.003418
1349.099228	148045.250990	36.008436
1349.790615	148300.363674	36.013453
1351.367473	148542.180563	36.018471
1352.559620	148808.856436	36.023488
1353.449957	149063.117282	36.028506
1354.952268	149320.056359	36.033524
1356.586729	149592.295968	36.038541
1357.647734	149857.149468	36.043559
1359.062067	150142.429210	36.048576
1360.787224	150405.921449	36.053594
1361.805165	150660.146909	36.058612
1363.892886	150929.645483	36.063629
1365.773908	151191.100978	36.068647
1367.410984	151452.027825	36.073664
1368.483403	151710.297410	36.078682
1370.996650	151942.076399	36.083700
1372.695066	152177.022643	36.088717
1374.152614	152420.305138	36.093735
1375.767890	152657.475038	36.098752
1376.963179	152894.690374	36.103770
1378.434914	153132.178666	36.108788
1379.354322	153380.096939	36.113805
1380.963005	153611.147595	36.118823
1382.152985	153869.945269	36.123840
1383.330038	154121.161736	36.128858
1384.351201	154364.744331	36.133876
1385.291605	154629.105940	36.138893
1386.439773	154892.775489	36.143911
1387.728483	155159.785022	36.148928
1388.980815	155419.622959	36.153946
1390.228808	155696.638321	36.158964
1391.259435	155976.723173	36.163981
1392.657766	156246.347819	36.168999
1393.952256	156545.103280	36.174016
1394.870922	156835.449468	36.179034
1396.523659	157124.877494	36.184052
1397.726506	157418.758276	36.189069
1399.132573	157717.339309	36.194087
1400.476804	158009.552057	36.199104
1401.946083	158304.143866	36.204122
1403.896687	158593.888651	36.209140
1405.084951	158898.895318	36.214157
1406.597377	159185.367685	36.219175
1408.437523	159467.335284	36.224192
1409.890715	159753.225232	36.229210
1411.582699	160042.883593	36.234228
1412.899275	160336.437176	36.239245
1414.126500	160621.431761	36.244263
1415.422196	160908.243858	36.249280
1417.077217	161194.897175	36.254298
1418.903165	161466.338608	36.259316
1420.805867	161752.333303	36.264333
1422.524252	162021.436449	36.269351
1424.355643	162298.045909	36.274368
1425.802341	162555.284548	36.279386
1427.391107	162810.243072	36.284404
1428.861608	163072.048242	36.289421
1430.391234	163330.838470	36.294439
1432.175514	163584.652992	36.299456
1433.167847	163837.660887	36.304474
1434.578034	164078.002913	36.309492
1435.279848	164326.443525	36.314509
1436.879826	164568.342927	36.319527
1438.006363	164816.513318	36.324544
1439.128385	165076.028554	36.329562
1440.452301	165336.400181	36.334580
1441.366106	165598.909162	36.339597
1442.908080	165867.431587	36.344615
1444.151616	166145.203628	36.349632
1445.374911	166424.782480	36.354650
1446.737147	166694.164418	36.359668
1447.562500	166981.501460	36.364685
1449.128244	167272.511978	36.369703
1450.439146	167557.399990	36.374720
1452.002505	167861.458348	36.379738
1453.153824	168158.024494	36.384756
1454.826676	168468.869974	36.389773
1456.311149	168774.038845	36.394791
1457.617066	169075.648374	36.399808
1458.806141	169373.485277	36.404826
1460.238517	169694.758420	36.409844
1461.527784	170016.679236	36.414861
1462.789126	170332.554279	36.419879
1463.785676	170672.901825	36.424896
1465.155162	171013.329960	36.429914
1466.783972	171343.870917	36.434932
1468.264623	171683.511651	36.439949
1469.872683	172016.344978	36.444967
1471.621595	172349.208222	36.449984
1473.557575	172675.304758	36.455002
1475.274147	172999.790119	36.460020
1476.733961	173335.918657	36.465037
1478.420443	173680.057646	36.470055
1480.144120	174001.249383	36.475072
1481.523432	174320.139768	36.480090
1482.937368	174649.978256	36.485108
1484.706795	174968.453295	36.490125
1486.065739	175302.226683	36.495143
1487.587899	175637.142988	36.500160
1489.038044	175971.350145	36.505178
1490.725360	176291.586125	36.510196
1492.451976	176628.937560	36.515213
1493.927194	176955.406005	36.520231
1495.435638	177294.866657	36.525248
1496.932092	177620.181157	36.530266
1498.547164	177944.259886	36.535284
1500.001669	178274.446310	36.540301
1501.533069	178581.955650	36.545319
1503.999340	178897.561989	36.550336
1505.583619	179209.838415	36.555354
1507.818705	179523.773508	36.560372
1508.994435	179817.946908	36.565389
1510.804837	180121.459870	36.570407
1512.510047	180414.254811	36.575424
1513.918286	180729.133392	36.580442
1515.306037	181028.609358	36.585460
1516.719007	181334.758872	36.590477
1517.739578	181647.130584	36.595495
1519.493006	181959.611707	36.600512
1520.433197	182267.723181	36.605530
1521.603311	182582.449272	36.610548
1523.052739	182908.579641	36.615565
1524.350918	183237.491242	36.620583
1525.797009	183548.979085	36.625600
1527.159823	183901.352548	36.630618
1528.380413	184238.571399	36.635636
1529.730174	184576.329539	36.640653
1531.296974	184919.791134	36.645671
1533.054115	185236.136888	36.650688
1534.888553	185550.174307	36.655706
1536.405420	185857.652872	36.660724
1537.939523	186168.176665	36.665741
1539.347949	186476.108157	36.670759
1541.150335	186781.602726	36.675776
1542.502364	187102.874918	36.680794
1543.741278	187413.746361	36.685812
1545.458328	187730.709655	36.690829
1546.601799	188064.626390	36.695847
1548.615691	188392.308544	36.700864
1549.742973	188730.408078	36.705882
1551.333467	189046.422221	36.710900
1552.763335	189389.502456	36.715917
1554.196769	189725.437486	36.720935
1555.973455	190066.547749	36.725952
1557.256443	190402.181489	36.730970
1558.990294	190745.397320	36.735988
1560.846388	191082.603332	36.741005
1562.186270	191432.933469	36.746023
1563.948897	191771.174381	36.751040
1565.398455	192117.859885	36.756058
1567.445068	192454.813765	36.761076
1569.061664	192790.913790	36.766093
1570.696078	193131.595508	36.771111
1572.859427	193473.791395	36.776128
1574.193721	193811.492410	36.781146
1575.853531	194148.709950	36.786164
1577.422410	194478.416259	36.791181
1578.911581	194828.081287	36.796199
1580.555826	195172.187650	36.801216
1582.162104	195514.918402	36.806234
1583.790187	195863.982324	36.811252
1585.441029	196202.596219	36.816269
1586.720636	196554.057366	36.821287
1588.464925	196893.814790	36.826304
1589.685908	197243.575512	36.831322
1590.806068	197597.417333	36.836340
1593.046207	197949.146551	36.841357
1594.061292	198306.386587	36.846375
1595.718454	198663.395664	36.851392
1597.521565	199028.863386	36.856410
1599.102988	199383.057670	36.861428
1601.005181	199733.125504	36.866445
1602.593288	200100.780174	36.871463
1604.347799	200449.923894	36.876480
1605.888857	200820.027869	36.881498
1607.634076	201187.891015	36.886516
1609.291864	201536.408725	36.891533
1610.621843	201908.902185	36.896551
1611.802203	202261.984115	36.901568
1613.021474	202640.124240	36.906586
1615.009209	203025.655947	36.911604
1616.652645	203389.230626	36.916621
1617.932660	203779.961824	36.921639
1619.553057	204149.346533	36.926656
1621.279504	204528.492167	36.931674
1622.443007	204920.112107	36.936692
1624.532166	205301.550815	36.941709
1625.644040	205682.860704	36.946727
1626.980717	206065.455944	36.951744
1628.761166	206456.004502	36.956762
1630.398758	206857.841068	36.961780
1632.284372	207236.732952	36.966797
1633.757499	207629.293607	36.971815
1635.594451	208024.157940	36.976832
1637.064065	208424.989202	36.981850
1638.722098	208809.983000	36.986868
1640.684076	209177.355064	36.991885
1641.936218	209552.045503	36.996903
1643.664091	209916.208989	37.001920
1645.257796	210302.249095	37.006938
1646.463120	210681.358611	37.011956
1648.402092	211058.291772	37.016973
1649.676760	211437.279040	37.021991
1650.997696	211828.996484	37.027008
1652.467978	212223.052948	37.032026
1653.981973	212623.275314	37.037044
1655.790522	213027.692145	37.042061
1657.377654	213434.915619	37.047079
1659.577181	213823.195697	37.052096
1661.115700	214226.545208	37.057114
1662.930843	214632.441391	37.062132
1664.715031	215021.252399	37.067149
1666.397487	215440.126562	37.072167
1667.871010	215834.351098	37.077184
1669.570344	216245.226071	37.082202
1671.132910	216662.525572	37.087220
1673.262326	217080.723916	37.092237
1674.764157	217484.068474	37.097255
1676.738226	217889.648018	37.102272
1679.101487	218295.901599	37.107290
1680.992193	218690.983572	37.112308
1683.106100	219090.246384	37.117325
1684.859474	219532.086751	37.122343
1686.915241	219922.879526	37.127360
1688.853060	220310.289899	37.132378
1690.530068	220698.506727	37.137396
1692.527313	221068.664640	37.142413
1694.069201	221453.503196	37.147431
1695.830000	221838.992812	37.152448
1696.826918	222222.958938	37.157466
1698.706917	222617.397478	37.162484
1700.404401	223005.949609	37.167501
1702.045917	223394.283763	37.172519
1703.419866	223804.786091	37.177536
1705.299160	224209.186931	37.182554
1706.390314	224617.376755	37.187572
1708.294166	225023.402001	37.192589
1710.208199	225427.420433	37.197607
1712.185335	225824.419561	37.202624
1713.847961	226217.306363	37.207642
1715.039883	226633.639904	37.212660
1717.226835	227040.895363	37.217677
1718.306472	227454.557850	37.222695
1720.175676	227856.077239	37.227712
1721.954896	228274.681630	37.232730
1723.918643	228691.859944	37.237748
1725.740843	229102.230288	37.242765
1727.407965	229522.432042	37.247783
1729.544644	229921.449904	37.252800
1730.905471	230328.928319	37.257818
1732.355213	230732.862606	37.262836
1734.840664	231136.779609	37.267853
1736.640983	231547.211798	37.272871
1738.955115	231931.295981	37.277888
1740.931097	232328.010408	37.282906
1742.777332	232727.058806	37.287924
1745.287055	233107.049674	37.292941
1746.271095	233503.930909	37.297959
1748.148964	233894.137627	37.302976
1750.067964	234279.410715	37.307994
1751.334560	234668.831182	37.313012
1753.455927	235049.805355	37.318029
1754.880511	235445.247161	37.323047
1755.993308	235827.481806	37.328064
1758.082815	236194.061283	37.333082
1759.367414	236571.595406	37.338100
1761.876545	236932.468102	37.343117
1763.768049	237295.221556	37.348135
1765.928150	237639.693016	37.353152
1768.038795	237999.541358	37.358170
1769.932595	238348.046176	37.363188
1772.112395	238698.257194	37.368205
1773.527607	239049.915899	37.373223
1775.204957	239408.238117	37.378240
1776.410733	239774.538810	37.383258
1777.708359	240153.500646	37.388276
1779.049915	240524.606699	37.393293
1780.445488	240906.576623	37.398311
1781.817813	241297.264025	37.403328
1783.643154	241693.948537	37.408346
1784.596666	242105.307696	37.413364
1785.906469	242521.054239	37.418381
1787.290095	242959.143441	37.423399
1788.659580	243390.504154	37.428416
1790.748340	243824.871484	37.433434
1792.216537	244266.911898	37.438452
1794.116497	244715.562725	37.443469
1795.840811	245171.508441	37.448487
1797.414467	245622.805700	37.453504
1799.658035	246076.838279	37.458522
1801.666407	246552.096244	37.463540
1802.987392	247001.455949	37.468557
1805.082632	247463.161357	37.473575
1806.815336	247934.148473	37.478592
1809.077435	248396.437360	37.483610
1811.244772	248861.130378	37.488628
1813.918995	249303.589031	37.493645
1815.587379	249755.511628	37.498663
1817.781689	250207.551219	37.503680
1820.007808	250652.778063	37.508698
1821.642490	251111.109303	37.513716
1823.709629	251554.305660	37.518733
1825.799146	251987.566139	37.523751
1827.681785	252433.740511	37.528768
1829.197594	252869.763722	37.533786
1830.984279	253330.358255	37.538804
1832.690381	253767.493914	37.543821
1834.517883	254215.812662	37.548839
1836.320709	254670.918440	37.553856
1837.840515	255122.870388	37.558874
1839.412276	255587.287018	37.563892
1841.611877	256048.170891	37.568909
1843.115428	256495.934711	37.573927
1845.033565	256956.408176	37.578944
1847.067735	257420.698573	37.583962
1848.831974	257895.601422	37.588980
1850.626039	258358.001066	37.593997
1852.808189	258812.944435	37.599015
1854.246892	259286.935985	37.604032
1856.405638	259748.996277	37.609050
1857.754200	260223.460048	37.614068
1859.508444	260691.404465	37.619085
1860.873112	261168.380497	37.624103
1862.321074	261669.221849	37.629120
1865.103929	262139.867025	37.634138
1866.694690	262636.239062	37.639156
1868.586641	263115.744303	37.644173
1871.284475	263578.655129	37.649191
1872.949196	264063.786242	37.654208
1875.266562	264531.255834	37.659226
1877.369475	265002.037598	37.664244
1879.224718	265453.528108	37.669261
1881.329616	265897.483235	37.674279
1883.104905	266333.668280	37.679296
1885.062066	266764.691604	37.684314
1887.000069	267207.047609	37.689332
1888.744225	267631.830882	37.694349
1890.665488	268073.223667	37.699367
1892.219701	268508.935530	37.704384
1894.215349	268958.368070	37.709402
1895.474929	269415.669533	37.714420
1897.408388	269865.035243	37.719437
1899.349951	270313.205204	37.724455
1901.029246	270775.262559	37.729472
1903.014006	271230.003741	37.734490
1905.097873	271695.854499	37.739508
1906.464403	272162.381845	37.744525
1908.733603	272631.147533	37.749543
1910.268486	273108.035571	37.754560
1912.660134	273570.225790	37.759578
1914.673479	274043.502504	37.764596
1916.285937	274524.973453	37.769613
1917.897976	275006.265850	37.774631
1919.659325	275486.288061	37.779648
1921.763098	275973.899104	37.784666
1923.940828	276465.993282	37.789684
1925.940375	276963.831449	37.794701
1928.347333	277444.530993	37.799719
1929.398777	277945.089177	37.804736
1931.689861	278422.732155	37.809754
1933.864202	278919.114832	37.814772
1936.287917	279418.909953	37.819789
1937.996515	279915.494187	37.824807
1939.777925	280415.596117	37.829824
1941.477975	280904.660371	37.834842
1943.707197	281402.603019	37.839860
1945.411890	281903.882349	37.844877
1947.713167	282400.464224	37.849895
1949.148414	282920.531805	37.854912
1951.317674	283428.436436	37.859930
1953.414883	283930.940958	37.864948
1955.391189	284448.400052	37.869965
1956.954214	284960.261217	37.874983
1958.655973	285483.934949	37.880000
1960.526498	286005.750266	37.885018
1962.462080	286519.704179	37.890036
1964.365563	287045.955825	37.895053
1966.512920	287573.918107	37.900071
1968.188421	288109.297225	37.905088
1970.402716	288637.143085	37.910106
1972.859044	289164.185074	37.915124
1974.402613	289691.401055	37.920141
1976.647627	290212.479417	37.925159
1978.728215	290752.176036	37.930176
1980.906039	291273.261403	37.935194
1983.236436	291794.929156	37.940212
1985.321197	292325.398375	37.945229
1987.487063	292835.963792	37.950247
1989.471431	293358.698237	37.955264
1991.801976	293868.546468	37.960282
1994.133044	294376.817698	37.965300
1995.999442	294894.510472	37.970317
1998.496321	295396.069910	37.975335
2000.438845	295902.671504	37.980352
2002.660291	296392.410541	37.985370
2004.418434	296893.653501	37.990388
2006.461819	297394.466181	37.995405
2008.620609	297903.258214	38.000423
2009.902522	298417.069067	38.005440
2011.778706	298921.940702	38.010458
2013.469069	299420.592531	38.015476
2015.193732	299909.534118	38.020493
2017.164184	300382.533497	38.025511
2018.873105	300876.197165	38.030528
2020.901898	301379.990287	38.035546
2022.896851	301882.541942	38.040564
2024.429014	302381.256094	38.045581
2026.699569	302892.290769	38.050599
2027.943345	303407.809656	38.055616
2030.389070	303920.867132	38.060634
2032.988417	304440.017204	38.065652
2034.580982	304961.539967	38.070669
2036.881506	305476.695337	38.075687
2039.140896	306002.800594	38.080704
2040.866579	306525.892386	38.085722
2042.784903	307054.765119	38.090740
2044.871920	307596.025658	38.095757
2046.641314	308139.087531	38.100775
2048.736233	308680.898651	38.105792
2050.144836	309219.568817	38.110810
2052.329535	309783.884165	38.115828
2053.797455	310341.533267	38.120845
2055.687033	310913.584378	38.125863
2058.215790	311495.785672	38.130880
2059.825597	312067.925493	38.135898
2061.887719	312637.777220	38.140916
2063.973064	313230.145990	38.145933
2066.246372	313815.368776	38.150951
2068.196173	314417.324441	38.155968
2070.198245	314997.199278	38.160986
2072.696604	315579.247815	38.166004
2074.676429	316175.394571	38.171021
2077.123393	316761.200484	38.176039
2079.172718	317357.224519	38.181056
2081.247757	317948.820972	38.186074
2083.883081	318534.048064	38.191092
2085.964248	319131.219999	38.196109
2088.779512	319712.674824	38.201127
2090.962893	320293.314826	38.206144
2093.347695	320862.337938	38.211162
2096.211629	321427.112989	38.216180
2098.161014	321997.823358	38.221197
2100.469885	322570.373866	38.226215
2102.781499	323143.883784	38.231232
2104.278783	323708.686933	38.236250
2106.452821	324271.723130	38.241268
2107.994755	324846.639748	38.246285
2110.235714	325428.265809	38.251303
2112.138773	326010.907020	38.256320
2114.082624	326595.871892	38.261338
2116.410629	327184.957110	38.266356
2118.023317	327768.162768	38.271373
2120.395206	328356.721612	38.276391
2122.312032	328940.424325	38.281408
2124.582328	329534.726162	38.286426
2127.061392	330115.379516	38.291444
2129.165222	330708.554459	38.296461
2131.879783	331283.140394	38.301479
2133.433151	331877.968144	38.306496
2135.839734	332464.144290	38.311514
2138.042814	333045.092839	38.316532
2139.982022	333645.855064	38.321549
2142.003410	334227.862134	38.326567
2143.896866	334816.332232	38.331584
2145.796016	335419.747304	38.336602
2148.209330	336018.704576	38.341620
2150.302115	336616.134169	38.346637
2152.188657	337193.892380	38.351655
2154.180943	337772.515329	38.356672
2156.131608	338352.560313	38.361690
2158.258597	338936.555092	38.366708
2159.773273	339517.115926	38.371725
2162.249624	340103.425993	38.376743
2163.908264	340690.549535	38.381760
2165.555303	341297.035389	38.386778
2167.884877	341888.451013	38.391796
2169.753586	342501.739071	38.396813
2171.948955	343121.361952	38.401831
2173.914959	343740.126506	38.406848
2176.137349	344370.211803	38.411866
2177.990737	344987.151634	38.416884
2180.081845	345635.541820	38.421901
2182.323801	346273.822338	38.426919
2184.698957	346915.701646	38.431936
2186.808347	347564.646201	38.436954
2189.260395	348195.911998	38.441972
2191.623009	348835.482880	38.446989
2194.227540	349486.298472	38.452007
2196.573932	350130.955078	38.457024
2199.313326	350764.498341	38.462042
2201.970070	351383.378110	38.467060
2204.220691	352018.760715	38.472077
2206.655884	352643.014133	38.477095
2209.237386	353285.023499	38.482112
2210.908669	353929.635046	38.487130
2213.326399	354566.425123	38.492148
2215.162264	355206.093065	38.497165
2217.079322	355853.578957	38.502183
2219.748081	356496.744265	38.507200
2221.855164	357146.716592	38.512218
2224.101578	357792.215496	38.517236
2226.182834	358446.358625	38.522253
2228.573332	359096.050933	38.527271
2230.737383	359740.264500	38.532288
2232.926881	360400.397483	38.537306
2235.448331	361051.204329	38.542324
2237.529784	361709.557814	38.547341
2239.803693	362365.889848	38.552359
2242.356492	363032.364057	38.557376
2244.799098	363681.111539	38.562394
2247.683664	364316.050462	38.567412
2249.979417	364969.824085	38.572429
2252.097564	365623.489173	38.577447
2253.770694	366268.515233	38.582464
2256.231790	366921.010941	38.587482
2258.498901	367583.496944	38.592500
2261.180921	368240.347577	38.597517
2263.226135	368890.772551	38.602535
2265.464885	369552.543774	38.607552
2267.763494	370209.397789	38.612570
2269.888015	370866.547888	38.617588
2272.252002	371525.346227	38.622605
2274.677655	372168.878531	38.627623
2276.921718	372822.372081	38.632640
2279.151034	373492.139633	38.637658
2281.626011	374156.654792	38.642676
2283.757119	374813.199739	38.647693
2286.204886	375456.771045	38.652711
2288.880496	376106.506669	38.657728
2291.136912	376748.868586	38.662746
2293.541931	377396.114175	38.667764
2295.751608	378061.182800	38.672781
2297.868960	378715.044858	38.677799
2300.108973	379365.957942	38.682816
2302.202770	380029.486051	38.687834
2304.230579	380669.961426	38.692852
2306.461499	381305.015329	38.697869
2308.470894	381947.599537	38.702887
2310.682068	382572.794061	38.707904
2312.674630	383217.309077	38.712922
2314.729912	383868.317662	38.717940
2316.944695	384517.968603	38.722957
2318.868266	385169.961971	38.727975
2321.289706	385834.638786	38.732992
2322.980524	386503.200159	38.738010
2325.338687	387166.338803	38.743028
2327.840641	387850.178570	38.748045
2330.347285	388530.250779	38.753063
2332.626698	389206.010745	38.758080
2334.781715	389904.364584	38.763098
2337.520033	390566.684994	38.768116
2339.919386	391267.883445	38.773133
2342.220140	391954.886649	38.778151
2344.658737	392648.189063	38.783168
2346.844389	393353.355187	38.788186
2349.269771	394051.038645	38.793204
2351.712188	394754.887978	38.798221
2354.145941	395460.598002	38.803239
2356.410701	396172.300972	38.808256
2358.427089	396894.267471	38.813274
2360.938136	397606.427888	38.818292
2363.228982	398332.648098	38.823309
2365.608520	399063.093478	38.828327
2368.028877	399769.362216	38.833344
2370.233890	400506.921612	38.838362
2372.741236	401238.913285	38.843380
2375.435904	401967.611858	38.848397
2378.222088	402686.444811	38.853415
2381.129056	403404.251499	38.858432
2383.448782	404130.346690	38.863450
2385.551891	404854.001121	38.868468
2388.252634	405591.803491	38.873485
2390.478244	406321.075493	38.878503
2392.795473	407044.511256	38.883520
2394.907571	407782.301924	38.888538
2397.251754	408523.936153	38.893556
2399.694878	409279.239845	38.898573
2401.922468	410023.411377	38.903591
2404.231902	410764.863716	38.908608
2406.398602	411529.903481	38.913626
2408.883517	412277.440949	38.918644
2411.281537	413039.511676	38.923661
2413.706028	413800.770964	38.928679
2416.001035	414565.778426	38.933696
2418.445257	415328.434153	38.938714
2420.998660	416099.281203	38.943732
2423.576160	416881.802565	38.948749
2425.439081	417633.621363	38.953767
2428.687289	418404.411952	38.958784
2431.214413	419174.614507	38.963802
2433.255517	419942.240271	38.968820
2436.046241	420707.617439	38.973837
2438.583025	421480.837959	38.978855
2440.885944	422253.262992	38.983872
2443.231508	423022.010967	38.988890
2445.646451	423787.103021	38.993908
2448.306218	424558.182445	38.998925
2450.744968	425332.236501	39.003943
2453.447536	426099.336253	39.008960
2456.038360	426875.240672	39.013978
2458.534538	427644.452501	39.018996
2461.258122	428400.539696	39.024013
2463.654121	429164.808486	39.029031
2466.485780	429904.983671	39.034048
2468.731935	430640.878626	39.039066
2470.974429	431379.637024	39.044084
2473.514946	432099.947155	39.049101
2475.436445	432828.993594	39.054119
2478.414685	433559.260544	39.059136
2480.529432	434280.586397	39.064154
2482.797704	435023.477883	39.069172
2485.289055	435760.083158	39.074189
2487.197018	436503.695139	39.079207
2490.050367	437250.366364	39.084224
2492.495255	437997.738503	39.089242
2495.030352	438763.796349	39.094260
2497.848074	439521.735294	39.099277
2500.456823	440277.709674	39.104295
2502.860019	441027.569551	39.109312
2504.921594	441791.629079	39.114330
2507.268094	442566.140223	39.119348
2509.957361	443337.380182	39.124365
2512.130493	444132.407951	39.129383
2514.569278	444919.622292	39.134400
2516.728071	445708.068749	39.139418
2518.894077	446502.202293	39.144436
2521.093399	447312.793288	39.149453
2523.360570	448138.974084	39.154471
2525.505307	448967.369120	39.159488
2528.382373	449792.121209	39.164506
2531.050408	450621.883415	39.169524
2533.880509	451458.364099	39.174541
2536.472039	452293.384311	39.179559
2539.133093	453123.555339	39.184576
2541.925782	453965.607033	39.189594
2544.388191	454813.697155	39.194612
2547.262817	455636.147441	39.199629
2550.063439	456490.838898	39.204647
2552.865126	457324.055277	39.209664
2554.968910	458172.774488	39.214682
2557.484911	459032.311570	39.219700
2560.397786	459869.147281	39.224717
2562.815855	460729.538672	39.229735
2565.152850	461569.836707	39.234752
2567.512584	462428.345115	39.239770
2570.030265	463292.907146	39.244788
2573.033866	464149.213343	39.249805
2575.426213	465022.768748	39.254823
2578.155715	465891.529380	39.259840
2580.782380	466751.676576	39.264858
2583.329887	467624.939066	39.269876
2586.692479	468475.943593	39.274893
2589.138696	469354.653530	39.279911
2591.723482	470215.159675	39.284928
2594.628390	471080.576980	39.289946
2596.768312	471952.801414	39.294964
2599.829259	472811.394456	39.299981
2602.187199	473667.386846	39.304999
2604.918850	474542.476675	39.310016
2607.649423	475391.003980	39.315034
2610.438903	476259.386435	39.320052
2613.207978	477116.669416	39.325069
2615.886354	477991.202656	39.330087
2618.413470	478836.777999	39.335104
2621.231856	479697.519538	39.340122
2623.648752	480570.912963	39.345140
2626.684108	481423.558070	39.350157
2629.057435	482270.414492	39.355175
2632.018500	483117.235529	39.360192
2634.655119	483964.373359	39.365210
2636.881514	484825.373849	39.370228
2639.812356	485675.816010	39.375245
2641.812570	486510.972436	39.380263
2644.075052	487342.714452	39.385280
2646.753278	488162.031151	39.390298
2648.447631	488993.385422	39.395316
2651.461896	489832.458403	39.400333
2653.728842	490679.286710	39.405351
2656.660270	491536.614272	39.410368
2659.333500	492379.255224	39.415386
2661.598362	493235.599412	39.420404
2663.928115	494095.877247	39.425421
2666.237337	494966.309009	39.430439
2668.813343	495848.712662	39.435456
2671.347907	496745.155289	39.440474
2673.518479	497644.688443	39.445492
2676.074484	498543.555347	39.450509
2678.445328	499463.997389	39.455527
2681.329004	500387.331330	39.460544
2684.048635	501309.632515	39.465562
2686.527894	502249.425460	39.470580
2689.299772	503177.314417	39.475597
2691.713143	504121.602007	39.480615
2694.180057	505078.636572	39.485632
2697.207772	506027.101145	39.490650
2699.771309	506994.698945	39.495668
2703.458593	507946.674777	39.500685
2706.187490	508896.735850	39.505703
2709.050044	509854.231275	39.510720
2712.105947	510802.159857	39.515738
2714.700057	511769.264983	39.520756
2717.376432	512730.450544	39.525773
2719.917569	513701.883054	39.530791
2722.941718	514674.134015	39.535808
2725.742352	515648.377865	39.540826
2728.202469	516624.986057	39.545844
2731.326577	517581.720121	39.550861
2734.322573	518554.491023	39.555879
2737.164179	519518.559872	39.560896
2740.490295	520490.902868	39.565914
2743.082565	521451.415618	39.570932
2746.427549	522416.832324	39.575949
2749.191407	523377.447913	39.580967
2752.154930	524342.453039	39.585984
2754.887303	525300.484118	39.591002
2757.096647	526273.196816	39.596020
2760.103754	527237.405571	39.601037
2762.439952	528200.403979	39.606055
2765.385102	529178.749300	39.611072
2768.295078	530149.332337	39.616090
2770.973611	531122.810216	39.621108
2773.751026	532085.383499	39.626125
2776.660977	533062.118711	39.631143
2779.515077	534034.418655	39.636160
2782.734357	535006.593722	39.641178
2785.487529	535977.321077	39.646196
2788.305879	536943.241877	39.651213
2791.284686	537926.836359	39.656231
2793.426304	538906.727534	39.661248
2796.669083	539855.475045	39.666266
2799.439339	540832.011170	39.671284
2802.672144	541785.411887	39.676301
2805.634825	542768.374077	39.681319
2808.247876	543734.322714	39.686336
2811.224395	544694.410936	39.691354
2813.874564	545659.969721	39.696372
2816.555888	546626.965563	39.701389
2819.341611	547602.577384	39.706407
2822.069848	548567.620206	39.711424
2825.157587	549528.011000	39.716442
2828.231632	550457.465274	39.721460
2831.040878	551377.750000	39.726477
2833.838246	552299.935539	39.731495
2836.257275	553223.729805	39.736512
2839.491638	554153.157923	39.741530
2841.359837	555075.459384	39.746548
2844.106584	556003.785359	39.751565
2847.027146	556946.794041	39.756583
2849.442567	557905.096534	39.761600
2852.380521	558843.144764	39.766618
2855.089630	559796.640341	39.771636
2858.175647	560747.392872	39.776653
2861.052892	561712.479711	39.781671
2863.453757	562685.963700	39.786688
2866.202509	563655.199470	39.791706
2869.243971	564648.926598	39.796724
2871.963364	565624.299859	39.801741
2874.689673	566605.474646	39.806759
2876.862556	567623.474458	39.811776
2879.891521	568627.294348	39.816794
2882.528969	569650.430541	39.821812
2885.087612	570689.262179	39.826829
2887.823977	571718.141203	39.831847
2889.986540	572780.160747	39.836864
2892.740762	573833.160497	39.841882
2895.528533	574898.413197	39.846900
2898.148267	575972.385681	39.851917
2901.074558	577063.728186	39.856935
2903.668730	578168.677695	39.861952
2906.688313	579261.218037	39.866970
2909.612547	580365.216114	39.871988
2912.591047	581469.207276	39.877005
2915.568734	582574.052882	39.882023
2918.655182	583699.493929	39.887040
2921.611419	584824.100952	39.892058
2924.614906	585955.616581	39.897076
2927.861463	587072.848218	39.902093
2930.899279	588205.702921	39.907111
2934.148431	589334.957764	39.912128
2937.376036	590452.281114	39.917146
2940.569720	591570.909319	39.922164
2943.584940	592712.063685	39.927181
2946.788847	593839.898904	39.932199
2950.083071	594959.795754	39.937216
2953.414004	596078.628596	39.942234
2956.115559	597186.187535	39.947252
2959.201848	598309.006419	39.952269
2962.438155	599421.074715	39.957287
2965.132697	600537.132671	39.962304
2968.009159	601657.109597	39.967322
2970.768687	602782.304984	39.972340
2973.815188	603920.110196	39.977357
2977.032163	605037.900452	39.982375
2979.611029	606163.645739	39.987392
2982.667158	607307.770399	39.992410
2985.452766	608432.356604	39.997428
2988.594660	609566.330431	40.002445
2991.766899	610700.785871	40.007463
2994.585523	611851.495410	40.012480
2997.252773	612994.758061	40.017498
3000.301751	614137.090599	40.022516
3003.193885	615268.278379	40.027533
3006.432771	616429.850255	40.032551
3009.112000	617576.590833	40.037568
3011.908430	618728.642860	40.042586
3014.610552	619898.737768	40.047604
3017.608545	621064.359805	40.052621
3020.480146	622217.232169	40.057639
3022.914223	623362.657536	40.062656
3025.896066	624494.878453	40.067674
3028.863340	625636.477077	40.072692
3031.593336	626769.949675	40.077709
3034.772830	627907.075212	40.082727
3037.391410	629068.549024	40.087744
3040.254118	630225.560595	40.092762
3043.186544	631381.585631	40.097780
3045.929809	632545.854895	40.102797
3050.333761	633709.072927	40.107815
3053.016928	634882.131191	40.112832
3056.198085	636044.143583	40.117850
3059.139110	637224.184923	40.122868
3061.667464	638405.807429	40.127885
3065.406928	639584.500852	40.132903
3068.065470	640786.789151	40.137920
3071.618781	641976.267135	40.142938
3074.976648	643168.582707	40.147956
3077.893645	644359.285720	40.152973
3081.407851	645557.681156	40.157991
3084.711020	646763.549877	40.163008
3087.710387	647952.372186	40.168026
3090.904605	649150.893792	40.173044
3093.806420	650349.121397	40.178061
3097.209904	651542.288323	40.183079
3100.391874	652756.330941	40.188096
3103.702684	653962.081800	40.193114
3106.679314	655176.161765	40.198132
3109.522224	656390.264237	40.203149
3113.212918	657603.280525	40.208167
3116.099825	658824.248627	40.213184
3119.499526	660027.300738	40.218202
3122.435565	661256.273796	40.223220
3125.468932	662483.681513	40.228237
3128.981239	663706.573701	40.233255
3132.266015	664934.425748	40.238272
3135.220312	666166.854042	40.243290
3138.728524	667386.791176	40.248308
3141.920507	668619.710851	40.253325
3145.043872	669848.701428	40.258343
3148.078510	671081.029782	40.263360
3151.050594	672318.231611	40.268378
3154.327284	673554.027624	40.273396
3157.183943	674799.924012	40.278413
3160.762115	676034.498771	40.283431
3163.563663	677282.858088	40.288448
3166.894440	678521.071849	40.293466
3170.311752	679776.898016	40.298484
3173.489147	681023.748381	40.303501
3176.657164	682273.412856	40.308519
3180.007060	683519.201441	40.313536
3182.848476	684767.537037	40.318554
3186.167394	686022.874338	40.323572
3189.393106	687272.740668	40.328589
3192.911409	688522.337053	40.333607
3196.132239	689782.135649	40.338624
3199.288103	691041.520793	40.343642
3202.287214	692302.293843	40.348660
3205.187211	693569.108619	40.353677
3208.332511	694822.952200	40.358695
3211.622765	696094.355050	40.363712
3214.432296	697364.712518	40.368730
3217.804112	698630.430647	40.373748
3220.690525	699911.418932	40.378765
3224.231594	701168.909419	40.383783
3227.273761	702459.019359	40.388800
3230.658815	703733.120521	40.393818
3234.201548	704993.380774	40.398836
3236.837413	706239.931353	40.403853
3240.305789	707460.402418	40.408871
3243.601524	708700.444746	40.413888
3246.537658	709929.916690	40.418906
3249.835228	711169.700960	40.423924
3252.351746	712408.196092	40.428941
3255.809019	713635.909972	40.433959
3259.314868	714883.981133	40.438976
3262.568203	716132.701741	40.443994
3265.674775	717387.546462	40.449012
3268.397899	718656.665448	40.454029
3271.558683	719924.234038	40.459047
3274.836436	721203.165630	40.464064
3278.135080	722487.584933	40.469082
3281.598896	723775.932088	40.474100
3284.725186	725064.134409	40.479117
3288.180807	726363.549862	40.484135
3291.359983	727677.237728	40.489152
3294.413428	728985.596582	40.494170
3297.497263	730305.500439	40.499188
3300.296393	731630.226978	40.504205
3303.608373	732960.580216	40.509223
3307.037438	734297.461348	40.514240
3310.103924	735658.918391	40.519258
3313.519143	737026.308022	40.524276
3316.283502	738405.269953	40.529293
3319.698952	739765.429569	40.534311
3322.996575	741144.965402	40.539328
3326.526212	742517.514014	40.544346
3330.108016	743899.187877	40.549364
3333.507948	745287.011617	40.554381
3336.854019	746687.567314	40.559399
3340.282167	748085.542233	40.564416
3343.426901	749493.270335	40.569434
3347.005400	750890.274217	40.574452
3350.014926	752302.394826	40.579469
3353.600547	753715.049571	40.584487
3357.102644	755129.675735	40.589504
3360.242682	756538.044039	40.594522
3364.713961	757950.365413	40.599540
3367.818388	759381.799947	40.604557
3371.581084	760790.561271	40.609575
3375.211717	762191.996697	40.614592
3378.543642	763606.948235	40.619610
3382.318001	765014.281138	40.624628
3385.375232	766418.173414	40.629645
3388.821526	767841.554640	40.634663
3392.465484	769247.769234	40.639680
3395.591699	770660.930538	40.644698
3399.043544	772071.950660	40.649716
3402.146593	773497.892274	40.654733
3405.465926	774915.662432	40.659751
3409.117291	776339.833048	40.664768
3412.487921	777759.942665	40.669786
3416.314242	779174.103970	40.674804
3419.652563	780598.133503	40.679821
3422.912375	782024.104826	40.684839
3426.457619	783444.105160	40.689856
3429.555690	784871.356075	40.694874
3433.622818	786289.825715	40.699892
3436.908221	787716.430519	40.704909
3440.517033	789130.586997	40.709927
3443.892616	790544.991028	40.714944
3447.436908	791972.219560	40.719962
3451.044284	793377.639188	40.724980
3454.287046	794797.731316	40.729997
3457.833677	796208.866119	40.735015
3461.837866	797595.379587	40.740020
3465.188040	798933.558557	40.745024
3468.886343	800208.802085	40.750029
3471.916243	801449.329047	40.755034
3475.429340	802603.799204	40.760039
3478.267939	803688.240370	40.765044
3481.140605	804712.034001	40.770048
3484.001715	805641.966887	40.775053
3486.570480	806520.829512	40.780058
3488.817816	807331.389135	40.785063
3491.710731	808065.079096	40.790068
3494.040185	808743.199775	40.795072
3496.390823	809350.821047	40.800077
3498.193354	809905.305953	40.805082
3499.797239	810391.173800	40.810087
3501.718505	810827.758437	40.815092
3503.102357	811226.577549	40.820096
3504.896960	811567.638671	40.825101
3505.640501	811857.070432	40.830106
3506.727544	812126.738906	40.835111
3508.111941	812350.738740	40.840116
3508.726064	812529.544241	40.845120
3510.310927	812673.453434	40.850125
3511.106999	812790.106281	40.855130
3511.880504	812881.631324	40.860135
3513.014957	812938.708247	40.865140
3513.562062	812962.865695	40.870144
3514.100662	812956.555899	40.875149
3514.731848	812944.597573	40.880154
3515.170213	812902.398124	40.885159
3516.147950	812826.309404	40.890164
3516.395925	812735.840036	40.895168
3516.874462	812643.861866	40.900173
3517.135549	812514.295484	40.905178
3517.203616	812374.666659	40.910183
3517.567832	812224.453283	40.915188
3517.846360	812072.046080	40.920192
3518.186462	811903.604763	40.925197
3518.440967	811729.245111	40.930202
3518.297946	811542.060737	40.935207
3518.703173	811337.534094	40.940212
3518.133238	811137.718732	40.945216
3518.885039	810920.529917	40.950221
3518.892852	810707.572807	40.955226
3518.788151	810474.389396	40.960231
3518.781347	810250.002671	40.965236
3519.064430	810026.148865	40.970240
3519.239195	809776.037350	40.975245
3519.279513	809540.886734	40.980250
3518.943763	809293.978208	40.985255
3519.166563	809042.802611	40.990260
3519.034776	808790.352760	40.995264
3519.067695	808514.583410	41.000269
3519.009221	808261.562727	41.005274
3519.219034	808000.400071	41.010279
3519.013975	807740.962534	41.015284
3518.676225	807470.359433	41.020288
3518.768208	807190.506894	41.025293
3518.610226	806939.610826	41.030298
3518.472683	806669.482382	41.035303
3518.490304	806412.654456	41.040308
3518.170990	806153.567813	41.045312
3518.469530	805885.101848	41.050317
3518.153877	805614.274664	41.055322
3518.035374	805330.948230	41.060327
3517.991508	805070.794546	41.065332
3517.582223	804807.209119	41.070336
3517.623986	804547.708149	41.075341
3517.520578	804279.000427	41.080346
3517.380099	804012.348390	41.085351
3517.357557	803758.027465	41.090356
3516.859495	803506.718650	41.095360
3516.966322	803233.717002	41.100365
3516.759608	802983.322224	41.105370
3516.370107	802732.801297	41.110375
3516.590971	802484.231269	41.115380
3516.642929	802228.517103	41.120384
3516.576656	801974.284868	41.125389
3516.363162	801720.803525	41.130394
3515.939111	801473.088448	41.135399
3516.070833	801218.108896	41.140404
3515.694805	800972.281694	41.145408
3515.838038	800722.679810	41.150413
3515.532349	800486.000342	41.155418
3515.147524	800238.185610	41.160423
3515.349214	799996.498290	41.165428
3515.093544	799765.528113	41.170432
3514.797223	799522.483047	41.175437
3515.046527	799292.101106	41.180442
3514.597396	799058.930617	41.185447
3515.021052	798825.804901	41.190452
3514.873887	798601.895689	41.195456
3514.843815	798362.251485	41.200461
3514.854028	798143.063266	41.205466
3514.491157	797903.065381	41.210471
3514.692457	797674.356134	41.215476
3514.216928	797434.900748	41.220480
3514.138558	797211.721140	41.225485
3513.575807	796987.730414	41.230490
3513.386422	796777.271809	41.235495
3513.761963	796551.197647	41.240500
3513.422330	796341.192599	41.245504
3513.407562	796118.458688	41.250509
3513.101737	795913.296630	41.255514
3512.697334	795711.140380	41.260519
3513.135105	795497.691791	41.265524
3512.750569	795291.836992	41.270528
3512.741176	795093.232070	41.275533
3512.828609	794886.452744	41.280538
3512.463030	794684.800794	41.285543
3512.344373	794485.509089	41.290548
3512.506696	794292.059580	41.295552
3512.382673	794087.207178	41.300557
3511.994676	793894.426818	41.305562
3511.916823	793696.874400	41.310567
3511.991599	793511.228234	41.315572
3511.792685	793324.345026	41.320576
3511.589877	793117.610684	41.325581
3511.413576	792932.973171	41.330586
3511.476050	792747.063288	41.335591
3511.554824	792568.073116	41.340596
3511.113907	792396.484518	41.345600
3511.164959	792202.455585	41.350605
3511.118181	792036.050461	41.355610
3510.767158	791853.427984	41.360615
3511.040386	791676.102918	41.365620
3510.393892	791506.344604	41.370624
3510.590159	791330.890778	41.375629
3510.588426	791167.946644	41.380634
3510.468169	790985.755168	41.385639
3510.326034	790813.243569	41.390644
3510.008629	790659.873269	41.395648
3509.792868	790495.916943	41.400653
3510.087915	790339.637628	41.405658
3509.550007	790181.378788	41.410663
3509.879005	790016.682763	41.415668
3509.605382	789861.518695	41.420672
3509.313689	789718.739885	41.425677
3509.615819	789564.113431	41.430682
3509.404972	789406.078350	41.435687
3509.462919	789249.519217	41.440692
3509.141442	789111.451776	41.445696
3508.889217	788966.242830	41.450701
3509.256011	788811.097824	41.455706
3508.960489	788666.627236	41.460711
3509.163842	788516.615037	41.465716
3508.915244	788388.402275	41.470720
3508.831781	788240.102896	41.475725
3508.800564	788099.018443	41.480730
3508.625290	787957.168343	41.485735
3508.676526	787820.882646	41.490740
3508.244950	787687.967826	41.495744
3508.362236	787552.649399	41.500749
3508.386443	787419.507015	41.505754
3507.986571	787279.302897	41.510759
3508.184602	787153.649364	41.515764
3508.157638	787021.442170	41.520768
3507.939012	786895.410218	41.525773
3507.794113	786779.247018	41.530778
3507.484619	786657.257751	41.535783
3507.713166	786528.392126	41.540788
3507.600907	786418.511635	41.545792
3507.601663	786289.285852	41.550797
3507.771363	786176.896557	41.555802
3507.646705	786049.949112	41.560807
3507.628665	785914.326949	41.565812
3507.390012	785802.343275	41.570816
3507.312666	785687.479004	41.575821
3507.107567	785561.814773	41.580826
3506.850232	785458.582496	41.585831
3506.948824	785338.224809	41.590836
3506.814488	785232.460859	41.595840
3507.083503	785124.415767	41.600845
3507.162571	785013.105156	41.605850
3506.516239	784910.617618	41.610855
3506.912658	784804.120565	41.615860
3506.720853	784698.407402	41.620864
3506.335253	784588.740644	41.625869
3506.303290	784488.555937	41.630874
3506.175886	784386.959158	41.635879
3506.437481	784285.591991	41.640884
3506.350403	784206.661100	41.645888
3506.212097	784098.766067	41.650893
3506.155252	784002.710491	41.655898
3506.023429	783904.550840	41.660903
3506.399869	783806.158561	41.665908
3506.010572	783714.482626	41.670912
3506.024800	783613.737038	41.675917
3506.083876	783523.263790	41.680922
3505.533198	783428.068965	41.685927
3506.004734	783334.869011	41.690932
3505.835694	783242.904828	41.695936
3506.018821	783158.408225	41.700941
3505.898645	783073.567031	41.705946
3505.659484	782983.874068	41.710951
3505.596633	782878.014546	41.715956
3505.632862	782796.735671	41.720960
3505.406381	782703.150569	41.725965
3505.677114	782614.008590	41.730970
3505.443255	782541.381008	41.735975
3505.582519	782459.786178	41.740980
3505.033063	782379.041867	41.745984
3505.112706	782293.912598	41.750989
3505.124539	782218.633681	41.755994
3505.177781	782137.000175	41.760999
3505.581113	782049.354639	41.766004
3505.268217	781981.753056	41.771008
3505.212848	781897.477802	41.776013
3505.165606	781814.577930	41.781018
3505.027451	781736.120460	41.786023
3505.315741	781660.790201	41.791028
3505.023198	781586.145294	41.796032
3504.594566	781512.358530	41.801037
3504.681630	781436.517821	41.806042
3504.623910	781364.931943	41.811047
3504.766066	781295.575965	41.816052
3504.566219	781215.745215	41.821056
3504.805208	781146.667108	41.826061
3504.671310	781077.403721	41.831066
3504.420217	781003.188853	41.836071
3504.700885	780945.272432	41.841076
3504.561245	780881.125905	41.846080
3504.243532	780812.677625	41.851085
3504.706035	780744.887558	41.856090
3504.732397	780680.515070	41.861095
3504.379767	780600.112168	41.866100
3504.299236	780548.748044	41.871104
3504.299601	780476.504066	41.876109
3504.321771	780414.246053	41.881114
3504.320083	780361.735716	41.886119
3504.376330	780282.393854	41.891124
3504.210852	780221.543091	41.896128
3504.175314	780159.046323	41.901133
3504.277162	780104.154755	41.906138
3503.608034	780044.714279	41.911143
3503.841968	779989.160282	41.916148
3504.113204	779941.621985	41.921152
3504.089663	779876.266260	41.926157
3504.043808	779817.016556	41.931162
3504.272261	779753.143949	41.936167
3504.036275	779692.546455	41.941172
3503.926203	779635.422224	41.946176
3503.574446	779576.516257	41.951181
3503.968326	779520.784681	41.956186
3503.752977	779476.178205	41.961191
3503.868289	779417.833872	41.966196
3503.808799	779367.836089	41.971200
3503.341043	779313.573798	41.976205
3503.909423	779257.122373	41.981210
3503.377171	779205.084840	41.986215
3503.625795	779148.783687	41.991220
3503.891424	779112.020444	41.996224
3503.383401	779042.503938	42.001229
3503.714059	778990.322732	42.006234
3503.504684	778957.525550	42.011239
3503.355458	778903.995303	42.016244
3503.570673	778854.637873	42.021248
3503.963862	778797.670288	42.026253
3503.581349	778740.387009	42.031258
3503.555126	778691.806612	42.036263
3503.820024	778629.099539	42.041268
3503.279730	778591.531141	42.046272
3503.427917	778543.019475	42.051277
3503.360544	778484.107045	42.056282
3503.247072	778452.670124	42.061287
3503.175731	778410.199355	42.066292
3503.198589	778362.543986	42.071296
3503.227160	778319.268598	42.076301
3503.247642	778273.582132	42.081306
3503.004668	778233.353846	42.086311
3503.406537	778176.921492	42.091316
3503.250948	778137.269022	42.096320
3503.128841	778093.820201	42.101325
3503.015876	778048.252763	42.106330
3502.763191	778005.464902	42.111335
3503.088756	777966.864528	42.116340
3502.819634	777935.943315	42.121344
3502.840079	777896.506689	42.126349
3503.228465	777864.738418	42.131354
3502.957979	777826.432404	42.136359
3503.124019	777774.663467	42.141364
3502.810694	777735.428642	42.146368
3503.050427	777702.699528	42.151373
3503.028717	777658.690033	42.156378
3503.230520	777612.378781	42.161383
3502.990627	777576.281857	42.166388
3503.229418	777538.136604	42.171392
3502.610935	777494.864444	42.176397
3503.211120	777458.333165	42.181402
3502.867395	777424.418850	42.186407
3502.894760	777382.319707	42.191412
3502.958850	777344.546856	42.196416
3503.084418	777285.002159	42.201421
3503.296720	777245.924294	42.206426
3503.031087	777207.761937	42.211431
3502.629873	777168.390835	42.216436
3502.397241	777139.872755	42.221440
3502.885561	777111.826636	42.226445
3502.734765	777060.351007	42.231450
3502.741940	777034.500984	42.236455
3502.716067	777000.384635	42.241460
3502.812875	776968.118904	42.246464
3502.710579	776938.003002	42.251469
3503.117526	776896.035483	42.256474
3502.913550	776856.039366	42.261479
3503.067844	776816.525630	42.266484
3503.091836	776778.559512	42.271488
3502.553451	776737.780789	42.276493
3502.954371	776701.032370	42.281498
3502.763964	776664.922791	42.286503
3502.864483	776626.056985	42.291508
3502.536419	776597.749463	42.296512
3502.337898	776555.682770	42.301517
3502.511785	776517.444411	42.306522
3502.158217	776498.446957	42.311527
3502.281667	776464.598952	42.316532
3502.521887	776429.500555	42.321536
3502.625157	776414.169876	42.326541
3502.867030	776377.544514	42.331546
3502.704648	776354.378999	42.336551
3502.794867	776301.134910	42.341556
3502.678558	776275.302546	42.346560
3502.474246	776245.594527	42.351565
3502.315239	776214.056989	42.356570
3502.480067	776183.352325	42.361575
3502.460818	776147.999870	42.366580
3502.390614	776119.451055	42.371584
3502.599453	776092.136466	42.376589
3502.616023	776054.660241	42.381594
3502.438346	776033.810631	42.386599
3502.617259	775997.735413	42.391604
3502.403702	775960.198125	42.396608
3502.126879	775926.610541	42.401613
3502.569911	775899.059685	42.406618
3502.257703	775880.300029	42.411623
3502.502795	775845.641230	42.416628
3502.436543	775820.882386	42.421632
3502.290720	775792.837196	42.426637
3502.235456	775762.511734	42.431642
3502.025222	775736.889921	42.436647
3502.192282	775707.364770	42.441652
3501.994476	775676.274511	42.446656
3501.973802	775662.637011	42.451661
3502.090240	775635.828396	42.456666
3502.009696	775623.924273	42.461671
3502.332336	775597.574009	42.466676
3501.990643	775568.082853	42.471680
3501.860755	775541.314467	42.476685
3502.156083	775517.233729	42.481690
3502.088717	775509.808651	42.486695
3502.143255	775475.425724	42.491700
3501.798436	775454.257271	42.496704
3501.519980	775431.945149	42.501709
3502.006966	775412.757173	42.506714
3501.829995	775402.247486	42.511719
3501.646213	775367.509334	42.516724
3501.714209	775348.587194	42.521728
3501.701260	775345.732984	42.526733
3502.209257	775319.154201	42.531738
3502.012592	775312.735171	42.536743
3502.065010	775280.912555	42.541748
3502.081008	775275.591161	42.546752
3501.910593	775234.940442	42.551757
3502.173081	775208.795685	42.556762
3501.908097	775181.063272	42.561767
3502.338525	775155.333899	42.566772
3502.124404	775135.275713	42.571776
3501.998561	775119.980070	42.576781
3502.292758	775082.945641	42.581786
3501.778095	775075.002811	42.586791
3501.823798	775046.184481	42.591796
3502.090077	775025.702120	42.596800
3502.225196	775004.157815	42.601805
3502.483873	774978.899363	42.606810
3502.302668	774963.070764	42.611815
3502.043151	774926.077502	42.616820
3502.261426	774903.041700	42.621824
3501.791236	774880.513231	42.626829
3502.319911	774860.085689	42.631834
3501.929614	774834.490382	42.636839
3501.982127	774807.738527	42.641844
3502.222776	774795.780155	42.646848
3502.006611	774784.685025	42.651853
3502.223904	774740.323125	42.656858
3501.796750	774733.744546	42.661863
3502.182387	774701.569026	42.666868
3502.135230	774686.013260	42.671872
3502.077188	774656.964235	42.676877
3501.947993	774629.798395	42.681882
3501.942268	774612.413320	42.686887
3501.819079	774593.422224	42.691892
3502.171853	774564.108154	42.696896
3501.797097	774537.130177	42.701901
3502.068050	774519.994827	42.706906
3501.956387	774497.553883	42.711911
3501.995956	774471.837252	42.716916
3502.177537	774449.643380	42.721920
3501.984904	774432.879707	42.726925
3502.074881	774408.681408	42.731930
3501.631600	774383.191761	42.736935
3501.564422	774359.511725	42.741940
3501.700480	774352.840031	42.746944
3501.728333	774329.883056	42.751949
3501.931258	774319.998799	42.756954
3501.800992	774305.539510	42.761959
3501.800403	774271.898849	42.766964
3501.937741	774258.725260	42.771968
3501.696992	774231.428560	42.776973
3501.767783	774217.724057	42.781978
3501.794506	774216.685304	42.786983
3501.923605	774196.765039	42.791988
3501.740833	774178.423000	42.796993
3501.802836	774149.352196	42.801997
3501.977715	774127.207712	42.807002
3501.699967	774112.624569	42.812007
3501.748677	774083.161649	42.817012
3502.005501	774080.262512	42.822017
3501.762513	774062.225636	42.827021
3501.858607	774049.945075	42.832026
3501.612488	774019.052781	42.837031
3501.758588	773998.144055	42.842036
3502.150318	773987.046101	42.847041
3501.896275	773961.967129	42.852045
3501.736124	773950.418202	42.857050
3501.639829	773920.338178	42.862055
3501.628309	773902.607583	42.867060
3501.873073	773900.055161	42.872065
3501.434767	773869.637209	42.877069
3501.726370	773850.871415	42.882074
3501.593122	773834.736941	42.887079
3501.659408	773829.159931	42.892084
3501.508358	773817.510781	42.897089
3501.315090	773809.858434	42.902093
3501.536674	773776.917780	42.907098
3501.474298	773778.553564	42.912103
3501.623502	773769.564061	42.917108
3501.761837	773744.124168	42.922113
3501.129524	773733.884124	42.927117
3501.643037	773723.061264	42.932122
3500.935149	773708.695945	42.937127
3501.614514	773682.871173	42.942132
3501.657982	773684.489544	42.947137
3501.515331	773681.951603	42.952141
3501.251460	773649.927738	42.957146
3501.533940	773653.132283	42.962151
3501.453272	773634.575035	42.967156
3501.796839	773624.420388	42.972161
3501.558724	773606.824922	42.977165
3501.328963	773591.888028	42.982170
3501.687986	773584.390770	42.987175
3501.821534	773565.551768	42.992180
3501.892949	773547.314064	42.997185
3501.456613	773540.637402	43.002189
3501.674071	773515.577762	43.007194
3501.361895	773515.678444	43.012199
3501.605026	773486.920009	43.017204
3501.471417	773461.228375	43.022209
3501.035839	773475.240673	43.027213
3501.834362	773458.557818	43.032218
3501.537481	773439.395313	43.037223
3501.495824	773421.372963	43.042228
3501.566086	773418.898380	43.047233
3501.653349	773400.115840	43.052237
3501.839866	773378.262753	43.057242
3501.681985	773371.096725	43.062247
3501.296220	773341.899449	43.067252
3501.493003	773338.714349	43.072257
3501.339610	773337.458837	43.077261
3501.636610	773302.040603	43.082266
3501.636681	773291.843559	43.087271
3501.442578	773275.028227	43.092276
3501.721814	773255.770347	43.097281
3501.321114	773238.447088	43.102285
3501.609539	773233.621221	43.107290
3501.550368	773237.571885	43.112295
3501.736918	773219.905544	43.117300
3502.058601	773209.015010	43.122305
3501.804076	773190.534543	43.127309
3501.973651	773173.166457	43.132314
3502.117173	773145.408338	43.137319
3501.763598	773119.259124	43.142324
3501.853663	773103.726674	43.147329
3501.462351	773082.608300	43.152333
3501.891073	773069.236806	43.157338
3501.534250	773058.112974	43.162343
3501.714421	773025.668416	43.167348
3501.969423	773012.818063	43.172353
3501.777166	773001.026619	43.177357
3501.688567	772987.641663	43.182362
3501.702336	772965.815811	43.187367
3501.788709	772944.470569	43.192372
3501.854102	772926.232323	43.197377
3501.159377	772915.065405	43.202381
3501.391199	772891.380662	43.207386
3501.165877	772890.580295	43.212391
3501.544795	772887.808375	43.217396
3501.633995	772864.787469	43.222401
3501.357094	772864.241914	43.227405
3501.792436	772849.637335	43.232410
3501.706156	772839.256833	43.237415
3501.290218	772827.748276	43.242420
3501.383711	772815.170504	43.247425
3501.377909	772788.125338	43.252429
3501.404583	772764.671038	43.257434
3501.529208	772766.522566	43.262439
3501.509895	772762.880169	43.267444
3501.491808	772729.678735	43.272449
3501.529573	772723.317351	43.277453
3501.626132	772712.610964	43.282458
3501.482135	772699.727260	43.287463
3501.149928	772683.573772	43.292468
3501.644066	772673.097431	43.297473
3501.360496	772681.026569	43.302477
3501.495253	772646.666487	43.307482
3501.476071	772651.300592	43.312487
3501.764808	772633.616019	43.317492
3501.474698	772607.454534	43.322497
3501.562988	772598.522907	43.327501
3501.507709	772598.532014	43.332506
3501.575359	772576.548339	43.337511
3501.223273	772567.048756	43.342516
3501.659829	772552.886786	43.347521
3501.455848	772538.978096	43.352525
3501.600349	772507.128330	43.357530
3501.491836	772511.530906	43.362535
3501.493009	772500.642859	43.367540
3501.481479	772479.016801	43.372545
3501.096454	772482.923008	43.377549
3501.553329	772468.609732	43.382554
3501.531750	772466.445559	43.387559
3501.549465	772436.685570	43.392564
3501.286851	772425.249661	43.397569
3501.347326	772422.283689	43.402573
3501.430198	772400.050648	43.407578
3501.614240	772387.161631	43.412583
3501.483751	772383.143223	43.417588
3501.726281	772373.545446	43.422593
3501.193420	772349.837125	43.427597
3501.207273	772339.291623	43.432602
3501.513240	772334.610087	43.437607
3501.374349	772330.937906	43.442612
3501.371252	772307.289990	43.447617
3501.220980	772303.915276	43.452621
3501.481390	772293.624703	43.457626
3501.553835	772295.337142	43.462631
3501.553414	772282.626131	43.467636
3501.456074	772264.560860	43.472641
3501.397646	772247.178889	43.477645
3501.411382	772228.011336	43.482650
3501.489816	772215.435025	43.487655
3501.491106	772213.168474	43.492660
3501.785962	772193.708186	43.497665
3501.255163	772175.024337	43.502669
3501.185251	772167.547036	43.507674
3501.540087	772155.959736	43.512679
3501.399823	772157.953587	43.517684
3501.717640	772134.991288	43.522689
3501.353765	772131.947292	43.527693
3501.761444	772123.405903	43.532698
3501.486707	772101.329406	43.537703
3501.478297	772094.531666	43.542708
3501.413155	772086.018846	43.547713
3501.612745	772059.676219	43.552717
3501.323880	772040.755102	43.557722
3501.474992	772039.301399	43.562727
3501.253815	772037.761211	43.567732
3501.222109	772015.742965	43.572737
3501.159887	772006.391990	43.577741
3501.333368	771993.208410	43.582746
3501.269169	772000.215285	43.587751
3501.275783	771991.838346	43.592756
3501.537777	771959.917602	43.597761
3501.353332	771956.499088	43.602765
3501.280671	771950.253768	43.607770
3501.245222	771949.224938	43.612775
3501.244880	771931.832658	43.617780
3501.041765	771911.074088	43.622785
3501.316873	771908.171098	43.627789
3501.319359	771907.677987	43.632794
3501.681182	771903.430414	43.637799
3501.351796	771884.959004	43.642804
3501.726982	771871.544902	43.647809
3501.309321	771865.257797	43.652813
3501.299931	771835.499854	43.657818
3501.201653	771822.114379	43.662823
3500.745285	771817.114651	43.667828
3501.436735	771808.821784	43.672833
3501.406546	771816.118857	43.677837
3501.638060	771798.441718	43.682842
3501.411610	771793.157746	43.687847
3501.353618	771783.263810	43.692852
3501.833124	771771.162664	43.697857
3501.485480	771749.392751	43.702861
3501.550547	771734.255714	43.707866
3501.215490	771724.702965	43.712871
3500.931910	771707.553898	43.717876
3501.455437	771690.025487	43.722881
3501.126123	771693.282395	43.727885
3501.139133	771694.117873	43.732890
3501.088073	771681.217083	43.737895
3501.086018	771687.277853	43.742900
3501.383891	771662.592865	43.747905
3501.533643	771649.511127	43.752909
3501.441596	771639.721152	43.757914
3501.269441	771645.711430	43.762919
3501.324750	771618.307014	43.767924
3501.253365	771610.780120	43.772929
3501.208996	771612.511959	43.777933
3501.293726	771607.669321	43.782938
3501.378912	771602.136792	43.787943
3501.414335	771572.271864	43.792948
3501.510965	771564.717248	43.797953
3501.137614	771572.120358	43.802957
3501.420108	771551.182244	43.807962
3501.385558	771540.643577	43.812967
3501.262024	771516.963700	43.817972
3501.470125	771506.729927	43.822977
3501.542669	771518.395663	43.827981
3501.441380	771477.959195	43.832986
3501.147035	771472.883270	43.837991
3501.231308	771467.104425	43.842996
3501.428314	771466.185058	43.848001
3500.966631	771455.223893	43.853005
3500.925331	771433.402588	43.858010
3501.352499	771424.660095	43.863015
3501.104900	771440.665481	43.868020
3501.196974	771442.621253	43.873025
3501.320004	771446.887773	43.878029
3501.125280	771417.651412	43.883034
3501.233405	771410.932396	43.888039
3501.205422	771393.050667	43.893044
3501.519083	771393.984477	43.898049
3501.211138	771402.017541	43.903053
3501.232541	771373.188867	43.908058
3501.418479	771368.181580	43.913063
3501.047860	771352.869159	43.918068
3501.210626	771354.616214	43.923073
3501.098533	771362.814156	43.928077
3501.248764	771342.488526	43.933082
3501.267907	771320.016369	43.938087
3501.010938	771307.198118	43.943092
3501.162502	771311.903485	43.948097
3501.286583	771304.146985	43.953101
3501.520924	771303.369272	43.958106
3501.547699	771292.475230	43.963111
3500.881234	771281.843184	43.968116
3501.256838	771264.535235	43.973121
3501.178890	771271.840710	43.978125
3500.904803	771249.761561	43.983130
3501.196612	771228.722455	43.988135
3501.249603	771229.600674	43.993140
3501.210079	771228.227491	43.998145
3501.143519	771230.012350	44.003149
3501.056290	771224.655763	44.008154
3501.060563	771219.826125	44.013159
3501.134580	771204.489432	44.018164
3501.483919	771186.889979	44.023169
3501.479680	771193.000788	44.028173
3501.244753	771175.793197	44.033178
3501.201320	771162.742421	44.038183
3501.042875	771150.893175	44.043188
3501.121958	771139.941018	44.048193
3501.334571	771134.929181	44.053197
3501.488596	771119.283481	44.058202
3501.143402	771117.270769	44.063207
3501.015667	771109.407717	44.068212
3501.202413	771081.339083	44.073217
3501.056843	771102.453073	44.078221
3501.323256	771100.339614	44.083226
3501.433977	771109.240269	44.088231
3501.099470	771081.257494	44.093236
3501.066161	771053.520656	44.098241
3501.227744	771044.673636	44.103245
3501.525331	771042.259370	44.108250
3501.545047	771042.059020	44.113255
3500.858116	771033.105370	44.118260
3501.441871	771014.924860	44.123265
3501.393889	771020.500978	44.128269
3501.133427	771017.538033	44.133274
3501.567219	771013.425931	44.138279
3501.381819	770988.966135	44.143284
3501.276182	770980.212331	44.148289
3501.291741	770976.858969	44.153293
3501.233426	770963.218975	44.158298
3501.406722	770934.018638	44.163303
3501.300627	770942.905930	44.168308
3501.392131	770928.452767	44.173313
3501.115176	770930.272353	44.178317
3501.409015	770910.069716	44.183322
3500.968974	770893.043083	44.188327
3501.219412	770893.297496	44.193332
3501.467671	770888.378176	44.198337
3501.111367	770890.161564	44.203341
3500.753749	770884.159390	44.208346
3501.292740	770863.078533	44.213351
3501.081683	770853.701339	44.218356
3501.234614	770847.861425	44.223361
3501.165283	770848.956949	44.228365
3500.681137	770847.262713	44.233370
3501.401337	770841.033691	44.238375
3500.772595	770845.276557	44.243380
3501.205615	770826.036312	44.248385
3501.294780	770808.281708	44.253389
3501.036721	770798.419410	44.258394
3501.318482	770798.471556	44.263399
3501.051076	770803.098427	44.268404
3501.331394	770797.188213	44.273409
3501.202777	770787.403134	44.278413
3501.199207	770768.382488	44.283418
3501.337533	770770.330820	44.288423
3501.036914	770776.392235	44.293428
3501.483969	770765.871693	44.298433
3501.369115	770752.831960	44.303437
3501.342200	770732.681675	44.308442
3501.252411	770733.484916	44.313447
3500.949954	770735.160914	44.318452
3501.346557	770723.515227	44.323457
3501.235125	770710.179186	44.328461
3501.203842	770690.128060	44.333466
3501.189318	770692.594374	44.338471
3501.268048	770681.198093	44.343476
3501.297843	770676.807403	44.348481
3501.328540	770654.429883	44.353485
3501.429582	770636.278682	44.358490
3501.451394	770638.443355	44.363495
3501.565785	770632.658900	44.368500
3501.551000	770606.839213	44.373505
3501.328383	770605.200399	44.378509
3501.088002	770598.538054	44.383514
3501.286167	770591.951304	44.388519
3501.230872	770574.712727	44.393524
3501.688397	770559.410090	44.398529
3501.156984	770564.474828	44.403533
3501.274744	770558.147688	44.408538
3501.491154	770530.761997	44.413543
3501.148322	770525.496286	44.418548
3501.192568	770509.965944	44.423553
3501.072322	770520.088062	44.428557
3501.211954	770519.079473	44.433562
3501.454954	770495.730194	44.438567
3501.168440	770476.509007	44.443572
3501.564224	770471.318713	44.448577
3501.445041	770467.445237	44.453581
3501.411886	770455.771361	44.458586
3501.679411	770442.520258	44.463591
3501.423957	770444.681378	44.468596
3501.279079	770413.905164	44.473601
3501.427557	770397.864617	44.478605
3501.280380	770393.059387	44.483610
3501.581403	770387.391841	44.488615
3501.233940	770389.469572	44.493620
3501.501774	770344.136639	44.498625
3501.377809	770347.508145	44.503629
3501.252770	770346.641691	44.508634
3501.507176	770330.780674	44.513639
3500.677608	770323.820884	44.518644
3500.754118	770294.929661	44.523649
3501.230706	770305.495853	44.528653
3501.112855	770308.077876	44.533658
3501.335675	770301.289684	44.538663
3501.152731	770307.332097	44.543668
3501.461876	770276.973339	44.548673
3501.318959	770274.187856	44.553677
3501.383813	770269.150495	44.558682
3501.175349	770262.039059	44.563687
3500.906123	770271.052586	44.568692
3501.136129	770241.643062	44.573697
3501.108141	770233.220554	44.578701
3501.191587	770233.256092	44.583706
3501.666023	770223.617342	44.588711
3501.086838	770227.408857	44.593716
3501.339363	770204.944162	44.598721
3500.700211	770188.786492	44.603725
3500.564349	770182.155836	44.608730
3500.870409	770179.937026	44.613735
3501.001119	770185.927873	44.618740
3501.288046	770179.129011	44.623745
3501.597837	770183.316217	44.628749
3501.406688	770176.694664	44.633754
3501.412123	770143.379196	44.638759
3501.252609	770140.645679	44.643764
3501.445611	770134.059375	44.648769
3501.514677	770129.809740	44.653773
3501.170691	770119.122893	44.658778
3501.495650	770116.950234	44.663783
3501.241018	770114.281656	44.668788
3501.564248	770101.365746	44.673793
3501.163573	770081.078127	44.678797
3501.334728	770062.618282	44.683802
3501.104761	770053.538884	44.688807
3501.282491	770052.819654	44.693812
3501.649098	770044.578349	44.698817
3501.707622	770020.124461	44.703821
3501.369198	770015.350487	44.708826
3501.540124	770001.473834	44.713831
3501.251158	769980.428294	44.718836
3501.413404	769968.622900	44.723841
3501.505289	769971.515473	44.728845
3501.486841	769955.156485	44.733850
3501.360319	769941.870832	44.738855
3501.184399	769935.640821	44.743860
3501.302788	769916.302203	44.748865
3500.947541	769927.893057	44.753869
3501.095389	769908.894552	44.758874
3501.188699	769884.533055	44.763879
3500.871801	769883.648864	44.768884
3501.275636	769879.294660	44.773889
3501.221450	769882.211329	44.778893
3501.192785	769883.940984	44.783898
3501.163837	769874.039714	44.788903
3501.152822	769857.827139	44.793908
3501.454928	769852.799701	44.798913
3501.509053	769848.700218	44.803917
3501.316423	769841.388633	44.808922
3501.293203	769814.335479	44.813927
3500.967055	769819.317622	44.818932
3501.142046	769803.517847	44.823937
3501.192942	769793.554035	44.828941
3501.070279	769799.192654	44.833946
3501.540869	769790.490383	44.838951
3500.869369	769783.257618	44.843956
3501.439279	769767.146294	44.848961
3501.174393	769759.156546	44.853965
3501.162137	769761.770649	44.858970
3501.706269	769753.105505	44.863975
3501.378719	769738.374061	44.868980
3501.345366	769719.503489	44.873985
3501.222417	769716.123088	44.878989
3501.158310	769709.628045	44.883994
3501.366356	769681.550617	44.888999
3501.199948	769680.789467	44.894004
3501.182278	769670.097507	44.899009
3501.289748	769671.213365	44.904013
3501.127553	769667.001559	44.909018
3501.169439	769640.380615	44.914023
3501.125565	769631.910756	44.919028
3501.446324	769618.501564	44.924033
3501.437853	769619.291529	44.929037
3501.399137	769611.806508	44.934042
3501.489606	769603.807345	44.939047
3501.487816	769588.282661	44.944052
3501.423392	769582.921130	44.949057
3501.428580	769563.994530	44.954061
3501.435611	769554.333337	44.959066
3501.480546	769536.780126	44.964071
3501.258992	769533.859458	44.969076
3501.311859	769509.503396	44.974081
3501.311580	769503.096231	44.979085
3501.275453	769502.116458	44.984090
3501.276180	769496.793420	44.989095
3500.965678	769502.512490	44.994100
3500.939265	769465.305614	44.999105
3501.277307	769458.300532	45.004109
3500.855625	769464.629383	45.009114
3501.694666	769459.217520	45.014119
3501.241455	769463.777248	45.019124
3501.155141	769448.561914	45.024129
3501.326692	769434.388382	45.029133
3501.235139	769431.347687	45.034138
3501.265162	769420.746086	45.039143
3501.183806	769429.631109	45.044148
3501.400051	769415.203745	45.049153
3501.715905	769393.909057	45.054157
3501.173476	769383.401696	45.059162
3501.417620	769387.649456	45.064167
3501.172340	769372.115140	45.069172
3501.395138	769337.330931	45.074177
3501.358791	769337.336920	45.079181
3501.462219	769343.924389	45.084186
3501.423830	769315.738313	45.089191
3501.049934	769308.653209	45.094196
3501.488264	769290.492455	45.099201
3501.509557	769295.072702	45.104205
3501.395457	769278.284391	45.109210
3501.528524	769245.831060	45.114215
3501.229061	769253.076429	45.119220
3501.257662	769242.671960	45.124225
3501.363620	769238.908620	45.129229
3501.218847	769215.471335	45.134234
3501.321441	769201.160853	45.139239
3501.320417	769209.244295	45.144244
3501.333942	769200.173032	45.149249
3501.373442	769183.359207	45.154253
3501.295199	769173.514413	45.159258
3501.185966	769169.885061	45.164263
3501.530243	769165.490967	45.169268
3501.334160	769158.524296	45.174273
3500.872468	769130.308665	45.179277
3500.998797	769120.775126	45.184282
3501.178947	769111.824175	45.189287
3500.664443	769129.406449	45.194292
3501.143791	769118.188229	45.199297
3501.466754	769120.993784	45.204301
3501.269853	769112.006363	45.209306
3501.244096	769093.034373	45.214311
3501.255283	769080.660987	45.219316
3501.101942	769082.263496	45.224321
3501.131595	769078.414066	45.229325
3500.801987	769078.862672	45.234330
3501.256511	769067.451309	45.239335
3501.178975	769044.150277	45.244340
3500.803971	769035.487836	45.249345
3501.011056	769036.242357	45.254349
3500.806626	769037.360397	45.259354
3501.107044	769033.909949	45.264359
3501.074927	769049.342799	45.269364
3501.198166	769034.387836	45.274369
3501.041688	769029.336805	45.279373
3500.896372	769009.004191	45.284378
3501.290907	768991.687847	45.289383
3501.090346	768995.417607	45.294388
3501.143789	768988.113937	45.299393
3501.247876	768990.117670	45.304397
3500.693530	768997.996745	45.309402
3501.076821	768987.287048	45.314407
3500.894599	768971.051451	45.319412
3501.299229	768950.825252	45.324417
3501.397183	768953.322904	45.329421
3500.754902	768945.493021	45.334426
3501.146874	768942.816090	45.339431
3500.938006	768945.117834	45.344436
3500.764223	768947.709539	45.349441
3500.957708	768931.264100	45.354445
3500.805471	768939.668482	45.359450
3501.215865	768909.731086	45.364455
3501.124105	768913.196515	45.369460
3501.115770	768896.833534	45.374465
3501.210754	768897.310792	45.379469
3500.885831	768922.600894	45.384474
3501.161142	768911.563844	45.389479
3500.879684	768907.174089	45.394484
3501.204434	768889.671843	45.399489
3501.282243	768869.893580	45.404493
3500.998114	768862.053905	45.409498
3500.963039	768857.524955	45.414503
3500.912341	768876.017238	45.419508
3500.936387	768860.782523	45.424513
3501.407567	768860.310589	45.429517
3500.908224	768860.787165	45.434522
3501.521397	768824.753291	45.439527
3501.305762	768827.204058	45.444532
3500.847199	768825.209381	45.449537
3500.941552	768831.207311	45.454541
3500.936959	768836.876499	45.459546
3501.227503	768823.618730	45.464551
3501.455244	768805.787231	45.469556
3501.306932	768782.497038	45.474561
3501.297618	768792.061029	45.479565
3501.197110	768785.965502	45.484570
3501.379099	768777.161721	45.489575
3501.185239	768759.005227	45.494580
3501.351555	768738.423377	45.499585
3501.235676	768742.582937	45.504589
3500.793268	768746.746987	45.509594
3500.811455	768742.997856	45.514599
3501.098218	768746.548886	45.519604
3501.011165	768728.867638	45.524609
3501.100795	768705.192970	45.529613
3500.979448	768705.903041	45.534618
3501.109346	768704.649357	45.539623
3501.120846	768696.366479	45.544628
3501.240858	768703.247535	45.549633
3501.227661	768692.947767	45.554637
3501.060989	768683.461931	45.559642
3501.717712	768661.616091	45.564647
3501.164935	768663.530942	45.569652
3501.433453	768667.676518	45.574657
3501.205177	768636.808100	45.579661
3501.098389	768616.763820	45.584666
3501.350574	768619.581225	45.589671
3500.933799	768611.960303	45.594676
3501.371605	768614.796428	45.599681
3501.571339	768628.318858	45.604685
3501.383108	768601.633522	45.609690
3501.132250	768581.514293	45.614695
3501.002836	768590.211063	45.619700
3501.016663	768571.231223	45.624705
3501.340604	768564.079752	45.629709
3501.224261	768550.691351	45.634714
3501.300029	768524.553764	45.639719
3501.419623	768531.089998	45.644724
3501.063539	768534.500556	45.649729
3501.192333	768520.578795	45.654733
3500.841939	768500.377156	45.659738
3500.981037	768484.531207	45.664743
3500.800447	768490.919750	45.669748
3500.686919	768482.065713	45.674753
3501.030657	768485.656778	45.679757
3500.761404	768487.870022	45.684762
3501.151352	768483.369422	45.689767
3500.792194	768478.400694	45.694772
3501.007229	768476.886484	45.699777
3501.184633	768488.391831	45.704781
3501.011709	768495.222744	45.709786
3501.286750	768458.848459	45.714791
3501.208036	768458.516373	45.719796
3501.136451	768444.775356	45.724801
3501.255596	768435.044952	45.729805
3501.091743	768455.183597	45.734810
3501.212135	768441.608125	45.739815
3501.103246	768414.317529	45.744820
3500.928661	768388.467170	45.749825
3501.481240	768329.519310	45.754829
3501.227969	768211.698069	45.759834
3501.052370	768021.495897	45.764839
3500.662810	767802.189347	45.769844
3500.529783	767518.153580	45.774849
3500.511944	767183.110366	45.779853
3500.179819	766794.658396	45.784858
3499.705696	766327.712954	45.789863
3499.457599	765821.400763	45.794868
3498.848440	765258.254748	45.799873
3498.705969	764650.899252	45.804877
3498.200671	763973.417955	45.809882
3498.058870	763241.210541	45.814887
3497.460196	762466.334822	45.819892
3496.531386	761610.273289	45.824897
3496.210516	760712.862101	45.829901
3495.364872	759771.065671	45.834906
3494.679115	758781.102575	45.839911
3493.769213	757730.084438	45.844916
3492.949455	756624.303414	45.849921
3492.240047	755454.647337	45.854925
3491.345918	754243.409106	45.859930
3490.553355	752966.615875	45.864935
3489.608730	751649.275147	45.869940
3488.730798	750281.745171	45.874945
3487.774353	748847.616711	45.879949
3486.557255	747370.807786	45.884954
3485.502584	745826.505968	45.889959
3484.538959	744239.112232	45.894964
3483.256968	742595.809784	45.899969
3482.172956	740904.791012	45.904973
3480.991709	739157.317475	45.909978
3479.842636	737361.300569	45.914983
3478.339845	735506.278280	45.919988
3477.039742	733612.371678	45.924993
3475.671207	731673.458871	45.929997
3474.442952	729677.635659	45.935002
3472.938950	727637.319053	45.940007
3471.377676	725550.905917	45.945012
3470.017555	723400.721700	45.950017
3468.713718	721208.811097	45.955021
3466.638767	718966.649718	45.960026
3465.384582	716676.022159	45.965031
3463.815817	714345.218985	45.970036
3461.947249	711973.215479	45.975041
3460.573174	709547.286835	45.980045
3458.779068	707080.059699	45.985050
3456.895673	704562.355879	45.990055
3455.196185	702003.584159	45.995060
3453.335830	699407.996130	46.000065
3452.098933	696756.040056	46.005069
3449.557528	694068.533628	46.010074
3448.027558	691339.445717	46.015079
3446.065466	688555.393318	46.020084
3443.844147	685733.282548	46.025089
3441.870239	682866.227283	46.030093
3439.925803	679969.125421	46.035098
3438.024271	677020.323457	46.040103
3435.868452	674027.805529	46.045108
3433.178259	671003.153827	46.050113
3431.432918	667945.253759	46.055117
3429.058620	664839.769332	46.060122
3427.369569	661700.074532	46.065127
3425.201789	658514.651996	46.070132
3422.611073	655310.231386	46.075137
3420.440655	652043.941849	46.080141
3418.190959	648748.604904	46.085146
3415.954350	645406.236558	46.090151
3413.471730	642036.400625	46.095156
3410.709345	638631.331114	46.100161
3408.552048	635182.950589	46.105165
3405.985182	631716.929376	46.110170
3403.403927	628196.535354	46.115175
3401.207283	624659.787635	46.120180
3398.335955	621086.158893	46.125185
3395.919841	617458.544362	46.130189
3393.316262	613835.484757	46.135194
3391.082848	610144.817182	46.140199
3388.538576	606420.223756	46.145204
3385.911792	602679.719530	46.150209
3382.997845	598874.326868	46.155213
3380.176166	595065.268017	46.160218
3377.719483	591219.346070	46.165223
3374.411926	587353.630144	46.170228
3371.298413	583460.754718	46.175233
3368.794312	579524.244990	46.180237
3365.588998	575585.900174	46.185242
3363.227423	571600.185508	46.190247
3360.324114	567607.174131	46.195252
3357.392778	563572.245482	46.200257
3354.771697	559505.196122	46.205261
3351.260059	555410.294047	46.210266
3348.328409	551296.362781	46.215271
3345.519223	547143.563188	46.220276
3342.555265	542982.589826	46.225281
3339.742069	538775.011717	46.230285
3336.168368	534560.118424	46.235290
3333.286140	530321.480228	46.240295
3330.338669	526050.334633	46.245300
3326.835478	521771.453679	46.250305
3323.993215	517467.675536	46.255309
3320.385223	513125.641326	46.260314
3317.358616	508772.314670	46.265319
3314.197924	504397.460432	46.270324
3311.198756	500001.641373	46.275329
3308.141808	495582.875554	46.280333
3304.906704	491155.710334	46.285338
3301.662530	486689.561990	46.290343
3298.136666	482223.604608	46.295348
3294.615197	477713.908665	46.300353
3291.615208	473202.321076	46.305357
3288.129080	468685.078315	46.310362
3284.854909	464119.060482	46.315367
3281.405165	459550.093297	46.320372
3277.999670	454976.033509	46.325377
3274.994016	450363.932336	46.330381
3271.600615	445759.163177	46.335386
3268.158294	441120.555936	46.340391
3264.481783	436475.698371	46.345396
3260.935022	431807.905147	46.350401
3257.823778	427118.660701	46.355405
3253.921144	422438.669423	46.360410
3250.446734	417727.948557	46.365415
3247.079785	413017.948927	46.370420
3243.232526	408294.646295	46.375425
3240.004175	403547.945901	46.380429
3236.158106	398803.246068	46.385434
3233.081069	394029.317381	46.390439
3229.273750	389251.328099	46.395444
3225.320037	384486.365834	46.400449
3221.997032	379682.419960	46.405453
3218.058051	374887.764247	46.410458
3214.306500	370079.104736	46.415463
3210.737899	365271.164945	46.420468
3207.206837	360450.413314	46.425473
3203.632251	355606.430444	46.430477
3199.833891	350772.188889	46.435482
3196.046500	345921.548671	46.440487
3191.907989	341069.428565	46.445492
3188.077529	336209.283265	46.450497
3184.356978	331350.487058	46.455501
3180.490066	326487.536188	46.460506
3177.075643	321614.173271	46.465511
3173.180991	316753.566920	46.470516
3169.259422	311887.520342	46.475521
3165.481804	307015.243281	46.480525
3161.661598	302141.122405	46.485530
3157.898689	297269.090782	46.490535
3154.072975	292390.284053	46.495540
3150.090270	287510.678889	46.500545
3146.219077	282620.047232	46.505549
3141.991833	277748.825340	46.510554
3138.054614	272871.519557	46.515559
3134.671962	267991.577985	46.520564
3130.088723	263113.469509	46.525569
3126.172147	258247.178532	46.530573
3122.177319	253383.763878	46.535578
3118.655838	248507.525452	46.540583
3114.625797	243643.382710	46.545588
3110.331631	238788.114080	46.550593
3106.393762	233932.069436	46.555597
3102.295124	229103.144680	46.560602
3098.683498	224248.037519	46.565607
3094.451147	219404.366940	46.570612
3090.086613	214579.946409	46.575617
3086.150235	209756.631274	46.580621
3082.091076	204922.230303	46.585626
3078.521896	200036.564720	46.590631
3074.153810	195239.036649	46.595636
3069.694992	190430.295211	46.600641
3065.642326	185644.201941	46.605645
3061.487133	180860.197516	46.610650
3057.145363	176110.562601	46.615655
3053.338690	171348.581925	46.620660
3048.948752	166607.072795	46.625665
3045.002321	161862.304589	46.630669
3040.514717	157153.967945	46.635674
3036.323474	152428.911920	46.640679
3032.075016	147729.972963	46.645684
3027.781347	143058.436140	46.650689
3023.481619	138389.535637	46.655693
3019.204031	133746.726835	46.660698
3014.658865	129106.867603	46.665703
3010.565802	124488.806740	46.670708
3005.551121	119896.672555	46.675713
3001.373101	115305.698988	46.680717
2996.917477	110753.022930	46.685722
2992.495358	106214.892144	46.690727
2988.472197	101699.869635	46.695732
2983.604021	97203.925765	46.700737
2979.443997	92725.789348	46.705741
2974.811724	88277.727769	46.710746
2969.955996	83841.666492	46.715751
2965.457412	79441.648457	46.720756
2960.538211	75066.789270	46.725761
2955.751354	70712.776000	46.730765
2950.813588	66405.914752	46.735770
2945.805963	62126.033731	46.740775
2940.953984	57878.920979	46.745780
2935.501859	53675.549745	46.750785
2930.392649	49508.441819	46.755789
2923.982615	45408.565709	46.760794
2914.203141	41468.365513	46.765799
2901.115438	37684.467860	46.770804
2888.484382	34042.923651	46.775809
2876.680131	30540.782817	46.780813
2864.639526	27228.641801	46.785818
2853.410923	24087.664635	46.790823
2842.245868	21119.671707	46.795828
2831.455085	18367.365964	46.800833
2821.483436	15789.615413	46.805837
2810.964811	13384.724414	46.810842
2801.648753	11159.086618	46.815847
2792.638230	9098.728178	46.820852
2784.022002	7194.636956	46.825857
2774.757663	5453.906176	46.830861
2762.352014	3972.522445	46.835866
2748.446517	2718.511022	46.840871
2735.122337	1655.049886	46.845876
2721.285493	840.691312	46.850881
2704.151346	336.602681	46.855885
2681.797011	241.291037	46.860890
2668.243530	249.484315	46.865895
2665.336331	231.300143	46.870900
2668.721320	238.926033	46.875905
2674.202841	238.109576	46.880909
2678.532828	242.695260	46.885914
2680.809376	239.486613	46.890919
2680.856419	238.381470	46.895924
2678.604752	235.881430	46.900929
2676.342095	224.827562	46.905933
2672.873935	229.349798	46.910938
2669.474135	234.207553	46.915943
2666.553023	226.232886	46.920948
2663.287721	228.705576	46.925953
2660.524782	231.638855	46.930957
2657.865863	230.917906	46.935962
2655.004680	221.658392	46.940967
2652.112064	224.168198	46.945972
2648.940603	226.667450	46.950977
2646.207363	228.773905	46.955981
2643.000141	228.004651	46.960986
2639.191137	229.534526	46.965991
2636.614843	219.407104	46.970996
2633.249585	225.105475	46.976001
2630.277249	227.526618	46.981005
2626.828332	217.897563	46.986010
2623.202095	221.405520	46.991015
2620.196052	215.075425	46.996020
2616.648386	225.274424	47.001025
2613.691857	219.919800	47.006029
2610.204050	214.795636	47.011034
2606.839587	208.848054	47.016039
2603.524216	222.355864	47.021044
2599.585167	214.917175	47.026049
2596.797868	222.296225	47.031053
2593.642209	213.234472	47.036058
2590.298343	206.174475	47.041063
2587.207774	212.576488	47.046068
2583.282374	211.913050	47.051073
2580.365166	208.600027	47.056077
2576.949415	212.756608	47.061082
2572.872044	217.570929	47.066087
2569.914105	205.577688	47.071092
2566.323705	210.887686	47.076097
2563.029666	205.252807	47.081101
2559.373078	211.823239	47.086106
2555.665402	219.087780	47.091111
2552.787628	206.413998	47.096116
2549.629841	205.346478	47.101121
2546.324508	201.787383	47.106125
2542.895302	213.569485	47.111130
2538.482180	209.441671	47.116135
2535.606423	204.585512	47.121140
2532.029173	215.511794	47.126145
2528.805473	207.756198	47.131149
2525.124889	211.600014	47.136154
2521.307369	201.705247	47.141159
2518.104666	200.578355	47.146164
2514.391309	206.537402	47.151169
2511.177214	207.370575	47.156173
2507.961790	205.328255	47.161178
2505.099881	209.633279	47.166183
2501.875824	209.836878	47.171188
2497.924509	219.718199	47.176193
2494.720195	210.324739	47.181197
2490.799527	205.770147	47.186202
2487.101207	204.079765	47.191207
2483.739914	199.531104	47.196212
2479.832022	200.745866	47.201217
2476.507441	186.602694	47.206221
2473.265153	195.216531	47.211226
2469.979119	189.692953	47.216231
2466.574423	192.373984	47.221236
2463.374192	204.571092	47.226241
2460.106396	187.561894	47.231245
2456.288597	188.200935	47.236250
2452.018134	187.680500	47.241255
2448.927300	188.786981	47.246260
2444.962006	197.874833	47.251265
2441.998721	198.730507	47.256269
2439.203999	190.137053	47.261274
2435.846014	188.923531	47.266279
2432.344378	196.880659	47.271284
2428.705814	203.227073	47.276289
2424.819177	201.085730	47.281293
2421.256354	194.067162	47.286298
2417.684079	194.483707	47.291303
2414.051836	188.903102	47.296308
2410.730404	187.476972	47.301313
2407.583578	195.421276	47.306317
2403.939706	197.115428	47.311322
2400.422456	197.827566	47.316327
2397.319253	192.560377	47.321332
2393.569094	192.052337	47.326337
2389.946758	193.345940	47.331341
2386.675990	195.493373	47.336346
2382.758070	199.653225	47.341351
2379.485755	197.733507	47.346356
2376.386618	196.208872	47.351361
2372.675541	188.892464	47.356365
2369.179940	195.714932	47.361370
2365.604987	188.040935	47.366375
2362.165541	189.671992	47.371380
2358.502370	190.298111	47.376385
2355.385857	188.412695	47.381389
2351.850891	186.834849	47.386394
2348.194746	187.584814	47.391399
2344.665967	181.829628	47.396404
2341.191216	183.488320	47.401409
2337.629026	183.691518	47.406413
2334.279843	184.758172	47.411418
2330.541869	183.235521	47.416423
2327.517462	178.217610	47.421428
2324.178331	178.830261	47.426433
2320.567372	185.341657	47.431437
2317.142646	176.460591	47.436442
2313.146191	191.105750	47.441447
2309.953454	185.090344	47.446452
2305.902001	185.890430	47.451457
2302.691667	170.467084	47.456461
2299.179788	172.617909	47.461466
2295.493338	175.091432	47.466471
2292.603264	167.691867	47.471476
2289.344425	184.751396	47.476481
2285.623264	177.395467	47.481485
2282.040230	177.055165	47.486490
2278.236157	175.420416	47.491495
2275.147248	180.931854	47.496500
2271.438980	181.867643	47.501505
2267.787018	185.337172	47.506509
2264.575145	174.509915	47.511514
2260.774311	172.500923	47.516519
2257.656323	172.792204	47.521524
2253.899062	180.910435	47.526529
2250.562723	167.852132	47.531533
2246.806914	171.284632	47.536538
2243.246337	180.731325	47.541543
2239.970003	167.848017	47.546548
2235.928003	178.341164	47.551553
2232.988468	170.974546	47.556557
2229.750458	173.310600	47.561562
2226.518004	178.587145	47.566567
2222.927801	170.529702	47.571572
2219.067190	193.382390	47.576577
2215.686848	183.252535	47.581581
2212.280352	168.854597	47.586586
2208.360369	174.865700	47.591591
2204.763808	165.725751	47.596596
2201.519438	177.379385	47.601601
2198.066640	171.249278	47.606605
2195.302408	166.461507	47.611610
2191.298773	170.628379	47.616615
2187.369960	174.393409	47.621620
2183.739150	179.579203	47.626625
2180.208645	190.627619	47.631629
2177.157260	176.591803	47.636634
2173.562084	175.502568	47.641639
2170.380704	165.956057	47.646644
2166.630139	170.324787	47.651649
2163.144134	168.854685	47.656653
2159.513735	166.175961	47.661658
2156.031989	177.925590	47.666663
2152.515774	173.736219	47.671668
2149.130137	172.352963	47.676673
2145.592706	161.263279	47.681677
2141.977252	172.959687	47.686682
2138.463103	180.471961	47.691687
2135.191878	160.353549	47.696692
2131.902247	177.127048	47.701697
2127.950870	170.168994	47.706701
2124.533331	162.144891	47.711706
2121.070961	163.372177	47.716711
2117.746109	161.450793	47.721716
2113.990859	179.331982	47.726721
2110.544154	180.520483	47.731725
2107.764294	160.477906	47.736730
2103.762919	175.434221	47.741735
2100.349615	154.662577	47.746740
2096.564261	162.332756	47.751745
2092.558100	172.147199	47.756749
2089.492931	163.778091	47.761754
2085.677985	168.853315	47.766759
2082.708446	160.828936	47.771764
2079.338401	165.872013	47.776769
2075.904630	162.730749	47.781773
2072.457148	163.041730	47.786778
2068.809932	176.297472	47.791783
2065.093827	163.708891	47.796788
2061.394380	158.457650	47.801793
2057.941306	166.610132	47.806797
2054.893869	165.301165	47.811802
2051.033023	165.435276	47.816807
2047.837827	161.937484	47.821812
2043.934765	164.612009	47.826817
2040.580241	156.315819	47.831821
2037.393201	159.929257	47.836826
2033.381696	164.688960	47.841831
2029.975560	164.332032	47.846836
2026.615590	164.919739	47.851841
2023.298142	159.712450	47.856845
2019.672236	161.961926	47.861850
2015.929425	165.560009	47.866855
2013.051478	166.318799	47.871860
2009.307277	164.005316	47.876865
2005.863106	162.499977	47.881869
2002.059955	160.318954	47.886874
1998.565179	156.245706	47.891879
1995.078884	146.235098	47.896884
1991.492990	162.478960	47.901889
1987.809512	167.710323	47.906893
1984.678269	157.551857	47.911898
1980.904651	165.267211	47.916903
1977.710093	159.666349	47.921908
1974.251342	155.608185	47.926913
1970.837471	152.084648	47.931917
1967.670182	158.697811	47.936922
1963.909080	165.596882	47.941927
1960.428394	155.875812	47.946932
1956.604452	161.934621	47.951937
1953.184583	153.939218	47.956941
1949.784476	159.984443	47.961946
1945.651189	171.129510	47.966951
1942.682498	162.891463	47.971956
1939.120355	156.720640	47.976961
1935.481616	160.530873	47.981965
1932.654290	161.151509	47.986970
1928.482097	161.159759	47.991975
1925.079565	154.978892	47.996980
1921.409481	159.967939	48.001985
1917.797434	150.064051	48.006989
1914.938143	149.573453	48.011994
1911.691249	154.505612	48.016999
1907.679230	150.630413	48.022004
1904.263780	162.118588	48.027009
1900.254384	156.413739	48.032013
1897.248303	157.168950	48.037018
1893.487381	155.934944	48.042023
1890.136059	149.544091	48.047028
1886.891908	161.225794	48.052033
1883.255263	151.851141	48.057037
1879.947218	154.580501	48.062042
1875.752703	151.740162	48.067047
1872.779272	147.067061	48.072052
1869.079684	148.176438	48.077057
1865.426496	160.301912	48.082061
1862.133330	149.037539	48.087066
1858.738329	159.441260	48.092071
1855.627352	159.425023	48.097076
1851.921907	153.828404	48.102081
1848.034104	151.126311	48.107085
1844.363897	143.888236	48.112090
1840.812711	165.295408	48.117095
1837.554047	144.082899	48.122100
1834.256585	148.518498	48.127105
1830.743647	147.633115	48.132109
1827.259221	146.663807	48.137114
1823.204689	160.632640	48.142119
1819.994867	157.838533	48.147124
1816.511942	149.311387	48.152129
1812.922542	146.372139	48.157133
1810.049113	138.328202	48.162138
1806.170270	147.942094	48.167143
1802.537298	146.261714	48.172148
1798.877575	148.663083	48.177153
1795.467864	144.420227	48.182157
1792.271599	146.637497	48.187162
1788.526896	139.927137	48.192167
1785.330925	143.173263	48.197172
1781.945653	146.901294	48.202177
1777.958328	143.924524	48.207181
1774.820209	139.515323	48.212186
1770.947414	158.104033	48.217191
1767.431479	153.768910	48.222196
1763.995689	145.175811	48.227201
1760.631311	142.571601	48.232205
1757.654333	148.809811	48.237210
1753.927465	157.714168	48.242215
1750.089247	148.583984	48.247220
1746.335514	145.456812	48.252225
1742.839763	140.734201	48.257229
1739.451217	143.952137	48.262234
1735.654230	149.781163	48.267239
1732.575386	138.311621	48.272244
1729.174556	148.600914	48.277249
1725.618071	140.854507	48.282253
1722.143419	130.614941	48.287258
1718.044030	142.235750	48.292263
1715.050296	146.193106	48.297268
1711.691214	142.588840	48.302273
1708.116845	147.977932	48.307277
1704.620604	140.860603	48.312282
1700.591847	144.826554	48.317287
1697.251265	140.001116	48.322292
1694.216135	144.428509	48.327297
1690.984207	145.137112	48.332301
1687.595628	140.953178	48.337306
1683.814649	149.862445	48.342311
1680.296930	135.608123	48.347316
1676.215397	135.864384	48.352321
1672.701540	139.644262	48.357325
1669.425268	136.588408	48.362330
1665.831520	137.124978	48.367335
1662.518891	136.879769	48.372340
1659.124091	138.030116	48.377345
1655.402475	135.878158	48.382349
1652.546351	128.934834	48.387354
1648.576281	137.725845	48.392359
1645.220033	144.913905	48.397364
1641.464533	134.273611	48.402369
1637.687696	138.784050	48.407373
1634.920849	143.757661	48.412378
1630.599860	144.650637	48.417383
1627.392493	143.276102	48.422388
1623.564217	140.651037	48.427393
1620.344600	137.029922	48.432397
1617.033238	132.359335	48.437402
1613.627819	137.794677	48.442407
1610.061320	135.911837	48.447412
1606.760494	143.722866	48.452417
1603.069191	131.965459	48.457421
1599.947812	133.621619	48.462426
1595.695118	140.111243	48.467431
1592.285417	123.048831	48.472436
1588.938529	130.523935	48.477441
1585.035531	139.488102	48.482445
1581.973679	136.047462	48.487450
1578.342592	143.864462	48.492455
1575.091533	134.908122	48.497460
1571.786637	128.549842	48.502465
1567.509857	135.954360	48.507469
1564.119371	137.887282	48.512474
1560.997700	140.055343	48.517479
1557.455841	133.234400	48.522484
1554.290892	137.779459	48.527489
1550.881255	129.542374	48.532493
1547.519932	127.174351	48.537498
1543.248815	135.806134	48.542503
1539.559892	123.002119	48.547508
1536.369381	129.928159	48.552513
1532.683440	140.323567	48.557517
1529.460393	129.992772	48.562522
1525.940003	136.703627	48.567527
1522.318836	128.323983	48.572532
1519.082569	124.799492	48.577537
1515.524991	135.101997	48.582541
1512.026712	128.830319	48.587546
1508.344514	130.055001	48.592551
1504.845656	135.969992	48.597556
1501.133344	130.227226	48.602561
1497.676808	127.866752	48.607565
1494.535780	134.838312	48.612570
1490.817197	133.456656	48.617575
1487.417760	142.802639	48.622580
1484.191310	132.282613	48.627585
1480.578683	131.948188	48.632589
1476.853409	127.801683	48.637594
1472.981987	141.032855	48.642599
1469.802885	133.364413	48.647604
1466.199955	126.900288	48.652609
1462.675161	129.320296	48.657613
1459.397267	127.900260	48.662618
1456.006193	141.079293	48.667623
1452.392023	145.399601	48.672628
1448.907683	132.673949	48.677633
1445.287996	127.970184	48.682637
1441.930900	128.894700	48.687642
1438.139236	135.270235	48.692647
1434.902205	127.273968	48.697652
1431.356213	141.537665	48.702657
1427.704337	144.921733	48.707661
1424.501426	131.002362	48.712666
1420.633081	140.174281	48.717671
1417.516170	121.909075	48.722676
1414.089666	128.749111	48.727681
1410.185725	133.456938	48.732685
1406.998468	123.943014	48.737690
1403.414835	134.131178	48.742695
1399.768761	133.533868	48.747700
1396.294885	135.693336	48.752705
1392.717275	134.752550	48.757709
1389.451931	131.223550	48.762714
1385.832957	133.549037	48.767719
1382.409099	128.628990	48.772724
1378.909046	134.411637	48.777729
1374.917339	138.382003	48.782733
1371.728477	128.890657	48.787738
1367.840251	135.867991	48.792743
1364.696808	134.233723	48.797748
1361.205503	126.489112	48.802753
1357.775724	130.542051	48.807757
1354.612539	139.169636	48.812762
1350.999975	131.015094	48.817767
1347.440718	136.671183	48.822772
1343.752803	121.936902	48.827777
1340.107390	125.817766	48.832781
1337.014831	130.246286	48.837786
1333.204314	137.587584	48.842791
1329.453367	138.970508	48.847796
1326.041990	135.351593	48.852801
1322.563925	138.584095	48.857805
1319.190098	126.623629	48.862810
1315.631554	120.444787	48.867815
1312.483376	128.036371	48.872820
1308.838348	128.698495	48.877825
1304.957530	136.025067	48.882829
1301.862676	126.713488	48.887834
1298.528578	122.616470	48.892839
1294.893160	115.820602	48.897844
1291.391942	127.118908	48.902849
1287.687707	132.307838	48.907853
1284.223064	130.162800	48.912858
1280.421958	127.860794	48.917863
1276.852744	126.029783	48.922868
1274.095529	126.043411	48.927873
1270.175504	126.485262	48.932877
1266.677279	125.642725	48.937882
1263.058946	132.015284	48.942887
1259.474139	127.205336	48.947892
1256.166506	119.874429	48.952897
1252.715240	136.294881	48.957901
1249.510872	133.742458	48.962906
1245.929625	134.393888	48.967911
1242.476903	123.460593	48.972916
1238.762982	122.728162	48.977921
1235.219250	117.926347	48.982925
1231.385766	121.496856	48.987930
1227.914539	130.364160	48.992935
1224.631255	132.476168	48.997940
1221.305673	132.145205	49.002945
1217.474374	124.032972	49.007949
1214.202528	124.200240	49.012954
1210.819009	130.080534	49.017959
1206.911950	137.577131	49.022964
1203.499271	119.789062	49.027969
1199.834701	137.992357	49.032973
1196.841994	124.238607	49.037978
1193.412744	127.201372	49.042983
1189.603777	127.911239	49.047988
1186.536369	128.091635	49.052993
1182.631354	123.198345	49.057997
1179.097403	124.235151	49.063002
1175.357561	125.486982	49.068007
1171.825580	128.095568	49.073012
1168.681721	136.250026	49.078017
1165.144313	131.877051	49.083021
1161.801914	127.440811	49.088026
1158.487760	123.955109	49.093031
1154.781330	128.368329	49.098036
1151.016975	116.356818	49.103041
1147.325280	131.099667	49.108045
1144.135335	121.648392	49.113050
1140.568239	126.102448	49.118055
1136.952854	120.551476	49.123060
1133.738164	122.724417	49.128065
1130.014300	121.613759	49.133069
1126.899341	121.774111	49.138074
1123.160276	124.501258	49.143079
1119.552816	127.864921	49.148084
1116.238705	119.110258	49.153089
1112.211192	118.173948	49.158093
1108.918801	118.435817	49.163098
1105.494214	128.332258	49.168103
1101.888768	125.026381	49.173108
1098.573791	119.216390	49.178113
1095.096410	127.593945	49.183117
1091.279796	128.533618	49.188122
1088.023073	131.818972	49.193127
1084.348506	125.828417	49.198132
1081.465725	126.419967	49.203137
1077.753434	126.947896	49.208141
1073.972720	126.361051	49.213146
1070.470167	126.460518	49.218151
1066.921582	128.723539	49.223156
1063.842225	120.594407	49.228161
1059.898355	129.327797	49.233165
1056.627298	117.365037	49.238170
1052.909087	127.824864	49.243175
1049.517534	143.220845	49.248180
1046.214458	127.463888	49.253185
1042.127561	131.064299	49.258189
1039.000367	118.621015	49.263194
1035.533623	115.083324	49.268199
1031.909443	127.121142	49.273204
1028.469954	116.980186	49.278209
1024.814120	131.977418	49.283213
1021.349879	124.915884	49.288218
1017.523046	129.353194	49.293223
1014.124854	129.392248	49.298228
1010.914649	120.019769	49.303233
1007.590526	130.050213	49.308237
1004.217044	120.200953	49.313242
1000.882966	120.495703	49.318247
997.038926	116.412303	49.323252
993.510387	120.552154	49.328257
989.911470	119.042398	49.333261
986.507772	122.149322	49.338266
982.899767	120.360095	49.343271
979.355152	126.526948	49.348276
976.019741	128.281757	49.353281
972.489747	129.819882	49.358285
969.009723	126.292409	49.363290
965.725721	127.882758	49.368295
961.760169	130.351316	49.373300
958.608971	124.413136	49.378305
954.690669	126.707165	49.383309
951.552655	119.582142	49.388314
948.127447	119.871741	49.393319
944.590877	117.809005	49.398324
941.051322	116.689726	49.403329
937.147802	125.879113	49.408333
933.793032	118.926431	49.413338
930.369618	118.632384	49.418343
926.608585	118.723007	49.423348
923.429903	116.610957	49.428353
920.022181	127.148027	49.433357
916.797674	119.169322	49.438362
913.025705	118.487105	49.443367
909.127191	122.809038	49.448372
905.597991	111.746623	49.453377
902.427076	117.200768	49.458381
898.764013	113.670410	49.463386
895.661509	118.375014	49.468391
891.746217	111.695553	49.473396
888.732011	119.005113	49.478401
884.673891	119.707453	49.483405
881.287348	108.762284	49.488410
877.617973	113.231673	49.493415
874.191920	113.650985	49.498420
871.033329	110.596038	49.503425
866.972048	111.910780	49.508429
863.760591	112.415320	49.513434
860.481706	117.605843	49.518439
856.750203	121.234194	49.523444
853.682620	110.214865	49.528449
850.035701	120.635282	49.533453
846.346216	111.722860	49.538458
842.767882	118.100842	49.543463
839.219593	111.586935	49.548468
836.056852	107.619032	49.553473
831.960537	114.726780	49.558477
828.530386	107.510668	49.563482
825.142619	118.190289	49.568487
821.787349	124.581566	49.573492
818.315046	121.634879	49.578497
814.434441	123.678290	49.583501
811.188934	112.388251	49.588506
808.313595	109.377524	49.593511
804.477294	116.865784	49.598516
800.977335	109.907068	49.603521
797.189701	114.208973	49.608525
793.810630	112.804891	49.613530
790.122360	110.603029	49.618535
786.557547	110.270253	49.623540
783.266177	111.135594	49.628545
779.725824	115.752232	49.633549
776.214929	107.070919	49.638554
772.802322	111.466684	49.643559
769.202940	116.977730	49.648564
765.912543	112.388590	49.653569
762.166603	114.889953	49.658573
758.988158	105.478742	49.663578
755.388769	115.280861	49.668583
751.832312	118.426835	49.673588
748.324370	109.497620	49.678593
744.563628	120.276455	49.683597
741.044997	108.556140	49.688602
737.794842	108.169947	49.693607
734.062994	108.337941	49.698612
731.088123	107.283965	49.703617
727.303432	101.132073	49.708621
723.752892	92.671334	49.713626
719.936432	108.967560	49.718631
716.322636	106.619369	49.723636
713.437557	107.644359	49.728641
709.714403	101.043294	49.733645
706.193098	111.425067	49.738650
702.915277	118.582399	49.743655
699.037406	115.624325	49.748660
695.683837	106.351285	49.753665
691.923838	120.309917	49.758669
688.587613	115.539953	49.763674
685.169596	121.162758	49.768679
681.552983	106.107402	49.773684
677.992598	109.519150	49.778689
674.462626	112.571603	49.783693
671.161068	96.118952	49.788698
667.627915	105.166690	49.793703
664.075233	109.666735	49.798708
661.043817	106.352341	49.803713
657.107131	106.093384	49.808717
653.708637	105.328622	49.813722
650.386931	97.449597	49.818727
646.844717	117.992911	49.823732
643.345911	109.198891	49.828737
639.724555	116.431631	49.833741
636.084845	109.828962	49.838746
632.641911	98.792048	49.843751
628.894054	110.043831	49.848756
625.121430	104.228105	49.853761
621.713397	106.240732	49.858765
618.565386	112.420873	49.863770
615.140571	104.703426	49.868775
611.349600	106.670289	49.873780
608.282352	105.632219	49.878785
604.721783	108.751815	49.883789
601.173511	106.946822	49.888794
597.722678	104.627129	49.893799
594.116796	113.710495	49.898804
590.696167	104.551988	49.903809
587.179343	119.843204	49.908813
583.724002	118.543086	49.913818
579.776385	116.907849	49.918823
576.254592	111.278619	49.923828
573.038779	103.420918	49.928833
569.122623	111.430168	49.933837
566.052606	109.339616	49.938842
562.523102	113.583028	49.943847
559.123025	118.226229	49.948852
556.128040	104.597267	49.953857
552.381040	102.215627	49.958861
548.438030	104.455560	49.963866
544.902841	112.907611	49.968871
541.108858	115.403711	49.973876
538.052686	121.724597	49.978881
534.732481	120.421028	49.983885
530.926154	116.059101	49.988890
527.531519	104.457851	49.993895
523.799257	113.318146	49.998900
520.675888	103.922544	50.003905
516.522736	111.330885	50.008909
513.528996	109.743436	50.013914
510.445544	107.623364	50.018919
506.821471	105.333718	50.023924
503.123986	104.235833	50.028929
499.328076	109.303058	50.033933
496.292796	114.360173	50.038938
492.328707	114.055921	50.043943
488.857548	111.342060	50.048948
485.644680	103.923930	50.053953
481.380746	111.672308	50.058957
478.210067	123.668986	50.063962
474.723975	113.965726	50.068967
471.123929	119.423259	50.073972
468.234284	106.782650	50.078977
464.571286	108.730035	50.083981
461.118024	109.488399	50.088986
457.988486	109.270856	50.093991
453.945854	111.050298	50.098996
450.806149	101.823475	50.104001
446.792970	104.947376	50.109005
442.962252	103.129344	50.114010
439.803439	90.240811	50.119015
436.395511	108.096013	50.124020
433.180444	100.721786	50.129025
429.208785	107.727076	50.134029
425.531548	103.438902	50.139034
422.156411	99.848740	50.144039
418.719364	97.161448	50.149044
415.618709	104.861736	50.154049
412.062868	112.669580	50.159053
408.641204	105.840137	50.164058
405.305230	104.459528	50.169063
401.421775	99.922885	50.174068
397.893365	102.091358	50.179073
393.961076	105.018526	50.184077
390.858738	112.439020	50.189082
387.244075	111.741580	50.194087
383.951503	113.298205	50.199092
380.328493	104.383893	50.204097
376.996628	102.415223	50.209101
373.562641	108.303725	50.214106
369.961999	107.370854	50.219111
365.797025	114.949245	50.224116
362.757029	106.007591	50.229121
359.639276	98.672677	50.234125
356.276512	107.718945	50.239130
352.585319	93.434626	50.244135
348.566695	110.568351	50.249140
345.722662	111.219915	50.254145
341.858202	108.088782	50.259149
338.297156	100.574454	50.264154
334.877171	103.687339	50.269159
330.934069	103.176094	50.274164
327.650799	98.049631	50.279169
324.130972	109.028585	50.284173
320.655704	104.029539	50.289178
317.190256	109.491942	50.294183
313.747457	105.339628	50.299188
310.679992	101.432130	50.304193
307.131449	105.354825	50.309197
303.181824	102.296685	50.314202
299.776878	114.359649	50.319207
296.216448	109.494651	50.324212
292.759984	108.491439	50.329217
288.893130	99.968888	50.334221
285.556226	94.956379	50.339226
282.565753	98.755613	50.344231
278.670534	119.834666	50.349236
275.345021	99.146988	50.354241
271.560443	105.472298	50.359245
268.168148	100.609632	50.364250
264.998515	96.304289	50.369255
261.503366	105.395356	50.374260
257.969963	95.289359	50.379265
254.390901	95.090838	50.384269
250.678555	100.281914	50.389274
246.997142	101.508521	50.394279
243.198699	112.884761	50.399284
240.417977	103.627952	50.404289
236.812064	103.176385	50.409293
233.166767	106.967416	50.414298
229.787666	100.526366	50.419303
225.837232	100.168032	50.424308
222.783454	96.785142	50.429313
219.157402	93.903170	50.434317
215.977583	104.517298	50.439322
212.531711	100.177317	50.444327
208.863285	107.251999	50.449332
205.179742	99.688048	50.454337
201.646198	95.742583	50.459341
198.159388	96.426718	50.464346
194.828371	95.756417	50.469351
191.186395	104.832214	50.474356
187.728296	104.789252	50.479361
183.615956	107.734453	50.484365
180.174135	98.902906	50.489370
177.182777	88.051938	50.494375
173.376906	107.324366	50.499380
170.526675	95.044232	50.504385
166.841158	100.683354	50.509389
163.569454	107.138852	50.514394
160.122345	110.136737	50.519399
156.156072	104.669109	50.524404
152.564014	101.284925	50.529409
149.247306	102.005402	50.534413
145.282108	104.554085	50.539418
142.043539	96.539393	50.544423
138.693185	93.357088	50.549428
135.182981	102.435011	50.554433
131.672186	104.544086	50.559437
128.072901	103.972111	50.564442
124.822622	90.278765	50.569447
120.602447	89.544499	50.574452
117.570265	89.205672	50.579457
114.260352	102.374320	50.584461
110.645121	99.095903	50.589466
107.268874	85.696368	50.594471
103.650630	94.868908	50.599476
100.099016	84.865281	50.604481
96.356402	97.703903	50.609485
92.950533	101.873054	50.614490
89.879426	85.995092	50.619495
86.159444	99.335886	50.624500
82.459488	82.140709	50.629505
78.916735	98.945223	50.634509
75.330876	94.741220	50.639514
72.032250	93.987201	50.644519
68.676952	95.000790	50.649524
65.051329	93.655107	50.654529
61.747952	88.287752	50.659533
57.800574	95.362035	50.664538
54.294230	91.274737	50.669543
50.988051	93.983411	50.674548
47.785318	90.889527	50.679553
44.173796	92.463807	50.684557
40.664254	93.976052	50.689562
36.906591	96.874078	50.694567
33.169279	97.442835	50.699572
29.658140	88.652343	50.704577
26.665171	87.201743	50.709581
23.169695	98.888203	50.714586
20.011150	93.737656	50.719591
16.188730	95.983428	50.724596
12.776043	96.063284	50.729601
9.101268	97.387092	50.734605
5.382320	94.987636	50.739610
1.811121	98.069246	50.744615