Thu Jun 16 18:24:23 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.986741	113.965982	0.000000
0.912963	110.719842	0.005005
0.915325	107.815589	0.010010
0.622288	104.964494	0.015014
0.738237	93.157633	0.020019
0.606994	85.818994	0.025024
0.550390	88.425918	0.030029
0.296585	65.977537	0.035034
-0.277246	60.497714	0.040038
-0.129576	37.283661	0.045043
-0.380485	37.223479	0.050048
-1.512778	33.233309	0.055053
-1.303179	27.107867	0.060058
-1.646674	35.691270	0.065062
-1.875313	19.740771	0.070067
-2.365316	19.857923	0.075072
-2.286237	19.606276	0.080077
-2.332199	12.147920	0.085082
-2.985727	4.401271	0.090086
-3.205725	-13.163237	0.095091
-3.462402	-0.652247	0.100096
-3.725978	-4.779950	0.105101
-4.203485	-16.895409	0.110106
-4.915120	3.170192	0.115110
-4.922158	-16.408031	0.120115
-4.962980	-7.110687	0.125120
-5.051607	-7.616969	0.130125
-5.387874	-6.467445	0.135130
-6.300839	-4.544561	0.140134
-6.169941	-14.147590	0.145139
-6.572657	-23.870590	0.150144
-6.378715	-16.482544	0.155149
-6.110063	-19.977721	0.160154
-6.721348	-16.164843	0.165158
-7.637982	-7.395887	0.170163
-7.715102	-9.716460	0.175168
-8.377226	-3.767487	0.180173
-8.094319	-9.741360	0.185178
-8.099947	-12.333408	0.190182
-8.204223	-13.347347	0.195187
-8.225139	-14.449053	0.200192
-9.130906	-9.066249	0.205197
-9.206624	-13.190071	0.210202
-9.745077	-8.157521	0.215206
-9.638064	-15.042111	0.220211
-9.918638	-8.381160	0.225216
-9.966563	-10.311248	0.230221
-10.651319	-8.624177	0.235226
-11.191611	-3.986237	0.240230
-11.237847	-14.212496	0.245235
-11.238038	-13.566897	0.250240
-11.266966	-14.639459	0.255245
-11.245782	-15.783539	0.260250
-12.275729	-16.325355	0.265254
-12.523867	-20.238366	0.270259
-12.838493	-12.970983	0.275264
-13.000862	-4.049256	0.280269
-12.872052	-13.046691	0.285274
-13.176113	1.161891	0.290278
-13.082532	-6.090735	0.295283
-13.852014	-6.685460	0.300288
-14.395103	-10.223380	0.305293
-14.325706	-14.618906	0.310298
-14.227472	-7.567632	0.315302
-14.464604	-10.303539	0.320307
-15.109660	-13.600660	0.325312
-15.809777	-11.555202	0.330317
-16.232600	-17.230031	0.335322
-16.140239	-11.482105	0.340326
-16.279888	-14.350138	0.345331
-16.034097	-14.465273	0.350336
-16.415181	-8.165166	0.355341
-16.148844	-20.606677	0.360346
-17.120842	-5.640838	0.365350
-17.587765	-14.609966	0.370355
-17.619271	-7.950813	0.375360
-17.961551	-2.751298	0.380365
-17.904989	-12.879711	0.385370
-18.131514	-11.280797	0.390374
-17.902735	-16.858107	0.395379
-18.733896	-8.743744	0.400384
-19.468761	-12.985837	0.405389
-19.534134	-16.841743	0.410394
-19.873508	-3.928390	0.415398
-19.617674	-8.751419	0.420403
-19.388289	-3.457947	0.425408
-20.629238	-15.995758	0.430413
-20.674245	-23.299661	0.435418
-21.138490	-15.914225	0.440422
-21.127867	-14.444278	0.445427
-21.083165	-8.197864	0.450432
-21.542893	-6.378688	0.455437
-21.401891	-13.780717	0.460442
-22.524156	-6.293931	0.465446
-22.696955	-8.962630	0.470451
-22.758313	-11.888885	0.475456
-22.925255	-15.464203	0.480461
-22.655421	-16.966156	0.485466
-22.964462	-7.614919	0.490470
-23.370624	-2.493735	0.495475
-23.809166	-6.312835	0.500480
-24.307039	-5.647832	0.505485
-24.335619	-6.925555	0.510490
-24.305480	-1.243208	0.515494
-24.488434	-15.930836	0.520499
-25.169886	-15.015297	0.525504
-25.737428	-5.668496	0.530509
-25.827198	-13.028737	0.535514
-26.312756	-12.528353	0.540518
-26.150375	-8.985786	0.545523
-26.176813	-17.331695	0.550528
-26.253559	-5.865013	0.555533
-25.993763	-8.099103	0.560538
-26.697631	-5.718287	0.565542
-27.156807	-7.263039	0.570547
-27.447393	-13.114313	0.575552
-28.247210	-9.076616	0.580557
-28.610268	-22.077564	0.585562
-28.965445	-7.502821	0.590566
-28.533476	-12.154194	0.595571
-28.267792	-12.799927	0.600576
-28.753046	-1.276288	0.605581
-28.724586	-6.754890	0.610586
-29.630200	-1.753606	0.615590
-30.498443	-9.388794	0.620595
-30.142133	-6.171380	0.625600
-30.401126	-7.937151	0.630605
-30.442498	-13.414964	0.635610
-30.486228	-15.637664	0.640614
-30.568265	-21.326880	0.645619
-31.377163	-16.255260	0.650624
-31.856046	-8.316316	0.655629
-31.896462	-9.186414	0.660634
-31.898798	-13.257940	0.665638
-32.438891	-6.267114	0.670643
-32.708488	-7.257875	0.675648
-33.291018	-12.766614	0.680653
-33.255233	-16.916458	0.685658
-33.447958	-9.135298	0.690662
-33.779562	-5.084905	0.695667
-33.321638	-7.971982	0.700672
-33.636803	1.763843	0.705677
-34.186316	-14.569148	0.710682
-35.033937	-11.029353	0.715686
-35.403458	-15.808324	0.720691
-35.390150	-15.539549	0.725696
-35.695562	-9.422523	0.730701
-35.795523	-18.861214	0.735706
-35.608248	-1.106395	0.740710
-35.695902	-8.477741	0.745715
-35.843040	-7.940154	0.750720
-37.062728	-0.243012	0.755725
-37.079776	-18.034016	0.760730
-37.195549	-6.382617	0.765734
-36.929049	-5.416759	0.770739
-36.657434	1.183620	0.775744
-37.713067	2.194837	0.780749
-38.318866	-4.996467	0.785754
-38.357031	-3.220222	0.790758
-38.518472	-17.656378	0.795763
-38.514487	-9.317476	0.800768
-39.546421	-17.109006	0.805773
-39.906990	-22.689149	0.810778
-39.949121	-4.069301	0.815782
-40.307365	-6.480249	0.820787
-40.122767	-15.906479	0.825792
-39.971353	-3.734140	0.830797
-40.059056	-3.061056	0.835802
-40.385647	-6.905660	0.840806
-41.065999	-12.656214	0.845811
-41.154603	-13.166544	0.850816
-41.744736	-10.617178	0.855821
-41.649854	-9.029550	0.860826
-42.398654	-12.717560	0.865830
-43.127370	-7.954166	0.870835
-42.589366	-11.758452	0.875840
-43.172106	-5.742687	0.880845
-43.369196	-13.000149	0.885850
-43.502162	-11.939173	0.890854
-43.265218	-12.093985	0.895859
-43.376135	-13.210118	0.900864
-43.743786	-4.225463	0.905869
-44.419685	-6.824335	0.910874
-44.911115	-7.223205	0.915878
-44.867888	-13.092748	0.920883
-44.767097	-13.767957	0.925888
-45.241319	-7.417436	0.930893
-45.733669	-20.438252	0.935898
-46.284003	-19.851000	0.940902
-46.574932	-10.472866	0.945907
-46.542329	-11.718081	0.950912
-46.792892	-7.736131	0.955917
-46.521682	-6.281922	0.960922
-46.781829	-14.863861	0.965926
-46.902609	-8.361814	0.970931
-47.571347	-18.287386	0.975936
-48.108761	-6.992988	0.980941
-48.007529	-12.164959	0.985946
-48.150021	-10.683618	0.990950
-48.410557	-14.529763	0.995955
-49.440734	-16.605321	1.000960
-49.653901	-13.195141	1.005965
-49.720750	-18.618525	1.010970
-50.013462	-15.772330	1.015974
-49.919605	-12.957366	1.020979
-50.188931	-16.546048	1.025984
-50.004556	-9.079965	1.030989
-50.276260	-14.800384	1.035994
-50.771181	-19.125335	1.040998
-51.240356	-15.614147	1.046003
-51.003347	-18.753180	1.051008
-51.477689	-7.413071	1.056013
-51.487148	-11.844694	1.061018
-52.704589	-5.465164	1.066022
-53.140960	-2.261081	1.071027
-52.637453	-16.299055	1.076032
-52.784947	-9.782827	1.081037
-52.693400	-15.260901	1.086042
-53.006356	-4.675140	1.091046
-53.516703	-2.502205	1.096051
-53.994156	-16.389702	1.101056
-54.691391	-8.903408	1.106061
-54.556997	-20.034480	1.111066
-54.399763	-13.833305	1.116070
-54.672974	-12.161661	1.121075
-54.449625	-14.685397	1.126080
-55.687378	-15.097659	1.131085
-56.043345	-16.446271	1.136090
-56.445987	-12.075251	1.141094
-56.390540	-11.928768	1.146099
-56.447077	-17.359677	1.151104
-56.514667	1.285198	1.156109
-56.332334	-4.099462	1.161114
-56.845367	-13.134756	1.166118
-57.699244	-5.996081	1.171123
-57.644544	-17.144172	1.176128
-58.026826	-7.929505	1.181133
-57.886568	-12.974446	1.186138
-57.928060	-12.522192	1.191142
-59.070126	-5.570687	1.196147
-59.391575	-16.510211	1.201152
-59.423599	-9.056706	1.206157
-59.290940	-4.181037	1.211162
-59.396407	-10.672492	1.216166
-59.692269	-11.947476	1.221171
-59.560641	-26.222611	1.226176
-60.647511	-18.764663	1.231181
-60.732596	-15.351579	1.236186
-61.186831	-13.405551	1.241190
-61.580176	-16.093539	1.246195
-61.546807	-9.261514	1.251200
-61.659780	-13.617033	1.256205
-61.437213	-21.343200	1.261210
-62.434899	-11.665654	1.266214
-62.870157	-17.437472	1.271219
-62.793223	-19.261223	1.276224
-63.217955	-3.063064	1.281229
-63.163347	-11.208088	1.286234
-63.078647	-4.089567	1.291238
-62.874115	-12.210830	1.296243
-63.868858	-14.309013	1.301248
-64.375882	-18.713254	1.306253
-64.100318	-17.209749	1.311258
-64.477130	-13.712443	1.316262
-65.043195	-14.366627	1.321267
-65.451207	-20.624677	1.326272
-66.066576	-2.329673	1.331277
-65.971752	-14.056990	1.336282
-66.008295	-10.268949	1.341286
-66.161738	-13.838110	1.346291
-66.092784	-9.946258	1.351296
-66.385556	-10.150755	1.356301
-66.245151	-15.109988	1.361306
-67.154603	-13.543624	1.366310
-67.721916	-13.249627	1.371315
-67.432907	-15.556420	1.376320
-67.777459	-9.948003	1.381325
-68.223709	-11.150285	1.386330
-68.819332	-7.781864	1.391334
-69.241238	-6.993664	1.396339
-69.064658	-24.392538	1.401344
-69.280427	-13.177446	1.406349
-69.260051	-22.347849	1.411354
-69.270639	-9.454609	1.416358
-69.470701	-4.832349	1.421363
-69.598665	-9.724737	1.426368
-70.698069	2.166277	1.431373
-70.835491	-9.103278	1.436378
-70.921441	-17.434316	1.441382
-71.103067	-13.980021	1.446387
-71.418235	-11.779953	1.451392
-72.254194	-15.427903	1.456397
-72.700712	-9.833808	1.461402
-72.502919	-7.763305	1.466406
-72.192457	-9.453007	1.471411
-72.363044	-12.208095	1.476416
-72.767662	-5.740627	1.481421
-72.470229	-15.089513	1.486426
-73.685398	-11.283670	1.491430
-74.288998	-6.952342	1.496435
-73.980514	-14.888442	1.501440
-74.493463	-14.091510	1.506445
-74.142686	-12.193878	1.511450
-74.445575	-14.572239	1.516454
-74.825183	-10.306443	1.521459
-75.206643	-25.217945	1.526464
-75.505763	-15.779368	1.531469
-75.830058	-27.138286	1.536474
-75.953975	-19.675519	1.541478
-76.153932	-20.616325	1.546483
-76.010119	-22.467604	1.551488
-76.824289	-0.472153	1.556493
-77.301320	-14.894722	1.561498
-77.480783	-13.114562	1.566502
-77.790099	-6.700925	1.571507
-77.482533	-11.983257	1.576512
-77.563414	-15.881287	1.581517
-77.924616	-11.456838	1.586522
-78.465526	-19.889571	1.591526
-78.653834	-5.979720	1.596531
-78.765884	-14.582777	1.601536
-78.985373	-3.129602	1.606541
-79.183328	-15.383490	1.611546
-80.021461	-5.163070	1.616550
-80.559373	-12.711270	1.621555
-80.141165	-19.654092	1.626560
-80.693484	-6.328100	1.631565
-80.701165	-13.768297	1.636570
-80.609188	-10.999292	1.641574
-80.931645	-5.056040	1.646579
-81.154424	-16.967536	1.651584
-81.806518	-4.111223	1.656589
-82.489978	-13.497576	1.661594
-82.277611	-8.994385	1.666598
-82.221496	-5.413147	1.671603
-82.244878	-12.003304	1.676608
-83.111068	-2.895611	1.681613
-83.470739	-5.869145	1.686618
-83.572486	-10.963569	1.691622
-83.969040	-6.795500	1.696627
-83.742139	-14.122833	1.701632
-83.526469	-6.982356	1.706637
-84.546709	-9.765426	1.711642
-84.686641	-9.248168	1.716646
-85.304042	-3.698045	1.721651
-85.269218	-5.769368	1.726656
-85.373698	-13.411002	1.731661
-85.497497	-8.347732	1.736666
-86.107293	-2.526183	1.741670
-86.882420	-9.028504	1.746675
-86.838625	-6.536057	1.751680
-87.115606	-5.761449	1.756685
-87.273264	-6.419594	1.761690
-87.016840	-16.750716	1.766694
-87.270722	-6.692561	1.771699
-86.880620	-20.136925	1.776704
-87.842357	-10.540395	1.781709
-88.336297	-8.533938	1.786714
-88.161306	-3.481868	1.791718
-88.652792	-5.829257	1.796723
-88.635213	-16.180986	1.801728
-89.414391	-13.341503	1.806733
-89.562052	-11.621352	1.811738
-89.976280	-20.156903	1.816742
-90.092454	-8.482162	1.821747
-90.101931	-20.208808	1.826752
-90.439427	-12.477225	1.831757
-90.290404	-20.967551	1.836762
-91.247184	-14.073009	1.841766
-91.623646	-4.002880	1.846771
-91.635832	-17.359352	1.851776
-91.968154	-8.542926	1.856781
-91.874926	-9.908752	1.861786
-91.589137	-9.948912	1.866790
-92.447432	-5.404126	1.871795
-92.847618	-5.896108	1.876800
-93.109191	-13.161258	1.881805
-93.138026	-3.839659	1.886810
-93.199317	-12.241463	1.891814
-93.813046	-15.073760	1.896819
-94.123458	-29.253337	1.901824
-94.554465	-13.622504	1.906829
-94.488303	-12.846698	1.911834
-94.798857	-23.941912	1.916838
-94.996621	-2.049228	1.921843
-95.056407	-14.961089	1.926848
-95.195252	-11.618340	1.931853
-95.853714	-13.559789	1.936858
-96.204346	-14.258651	1.941862
-96.692666	-14.996515	1.946867
-96.552863	-20.355296	1.951872
-96.605764	-5.788687	1.956877
-96.770586	-11.825888	1.961882
-96.926593	-10.829668	1.966886
-98.016914	-14.657646	1.971891
-98.331439	-13.673407	1.976896
-98.427301	-18.748970	1.981901
-98.023743	-17.260504	1.986906
-98.404065	-14.062725	1.991910
-98.309858	-7.041179	1.996915
-98.845852	-5.592892	2.006912
-98.944748	-16.114185	2.016909
-98.577123	-19.006071	2.026906
-97.509098	-12.661218	2.036902
-97.406256	-10.200154	2.046899
-96.945280	-3.975744	2.056896
-96.438528	-6.821973	2.066893
-95.734247	-9.758634	2.076890
-94.721410	-12.907106	2.086886
-94.558724	-13.398622	2.096883
-94.469583	-11.547342	2.106880
-94.112217	-11.957731	2.116877
-93.170912	-14.842686	2.126874
-92.845224	-6.486052	2.136870
-91.840626	-7.331759	2.146867
-91.347102	-15.630890	2.156864
-91.297402	-12.070697	2.166861
-91.192831	-11.265392	2.176858
-90.227802	-4.137167	2.186854
-89.859620	-10.076841	2.196851
-89.020532	-8.929054	2.206848
-88.232633	-14.746162	2.216845
-88.290984	-6.963788	2.226842
-88.248564	-10.872913	2.236838
-87.232436	-10.325538	2.246835
-86.687125	-9.666369	2.256832
-86.256677	-8.180187	2.266829
-85.410052	-11.086833	2.276826
-85.366990	-16.925061	2.286822
-84.987732	-13.473170	2.296819
-84.102218	-18.194826	2.306816
-83.744409	-17.647407	2.316813
-82.956307	-11.613579	2.326810
-82.270861	-1.237943	2.336806
-82.277295	-0.026081	2.346803
-82.133196	-11.574560	2.356800
-81.408726	-15.341749	2.366797
-80.518297	-15.677149	2.376794
-80.275467	-11.572882	2.386790
-79.505777	-14.301452	2.396787
-79.106118	-20.685111	2.406784
-78.972603	-10.450004	2.416781
-78.149367	-15.506706	2.426778
-77.638355	-14.192876	2.436774
-77.454681	-11.368518	2.446771
-76.718102	-12.716286	2.456768
-76.334688	-15.211902	2.466765
-75.111689	-1.648733	2.476762
-75.127009	-15.685932	2.486758
-74.745569	-11.995350	2.496755
-74.584015	-8.189995	2.506752
-73.330543	-12.385703	2.516749
-73.123209	-18.605507	2.526746
-73.196926	-10.835411	2.536742
-71.955469	-8.295517	2.546739
-71.317392	-11.256005	2.556736
-71.305727	-14.818956	2.566733
-70.619804	-10.833257	2.576730
-70.085037	-3.048640	2.586726
-69.612019	-0.916548	2.596723
-69.327862	-1.661559	2.606720
-68.471174	-4.052946	2.616717
-68.162297	-3.648080	2.626714
-67.785860	-2.879407	2.636710
-67.002572	-4.111022	2.646707
-66.659134	-5.980182	2.656704
-66.412683	-6.054756	2.666701
-65.509649	0.792812	2.676698
-65.277913	1.322740	2.686694
-64.686295	-2.349495	2.696691
-63.850537	-3.620008	2.706688
-63.440178	-7.337064	2.716685
-63.645630	-3.836445	2.726682
-62.858651	-6.800699	2.736678
-62.170506	-2.620073	2.746675
-61.117302	-0.579420	2.756672
-61.110843	1.195340	2.766669
-60.597784	-4.022976	2.776666
-60.626501	-1.593508	2.786662
-59.391709	-4.764138	2.796659
-58.682164	0.833229	2.806656
-58.717413	-7.258400	2.816653
-58.403704	-11.275977	2.826650
-57.487732	-7.054176	2.836646
-57.318264	-9.790430	2.846643
-56.703312	-6.342716	2.856640
-55.570327	-7.082109	2.866637
-55.531091	-0.412921	2.876634
-55.516296	0.217365	2.886630
-54.624137	-5.717732	2.896627
-54.070292	-7.616329	2.906624
-54.139944	-13.355920	2.916621
-53.219943	-9.142688	2.926618
-52.563351	-5.908307	2.936614
-52.179199	-11.670641	2.946611
-51.118938	-11.930483	2.956608
-50.994331	-12.092988	2.966605
-50.990969	-11.686923	2.976602
-50.185383	-10.848211	2.986598
-49.426228	-12.078996	2.996595
-49.054398	-11.286347	3.006592
-48.578588	-7.548730	3.016589
-48.084979	-10.677471	3.026586
-47.801586	-11.486464	3.036582
-46.621800	-9.021127	3.046579
-46.265154	-11.375508	3.056576
-46.028905	-10.624956	3.066573
-46.001393	-10.755609	3.076570
-45.666599	-11.267270	3.086566
-44.653094	-14.326942	3.096563
-43.419026	-14.304939	3.106560
-43.660273	-12.444693	3.116557
-43.287101	-14.303354	3.126554
-42.930996	-15.507931	3.136550
-42.000967	-11.715285	3.146547
-41.853074	-9.816222	3.156544
-40.871615	-15.656424	3.166541
-40.312266	-17.848025	3.176538
-40.273908	-9.522925	3.186534
-39.489580	-15.322746	3.196531
-38.470075	-18.482683	3.206528
-38.551171	-7.850859	3.216525
-38.462542	-17.620308	3.226522
-37.644150	-6.098353	3.236518
-36.904723	-8.621293	3.246515
-36.769431	-5.810569	3.256512
-36.274916	-14.087540	3.266509
-35.376738	-9.204123	3.276506
-35.407230	-5.368113	3.286502
-34.391896	-9.508458	3.296499
-33.667227	-15.175732	3.306496
-33.824570	-9.318243	3.316493
-33.186591	-0.101456	3.326490
-32.239539	-3.830058	3.336486
-32.125379	-14.944289	3.346483
-31.759532	-14.281733	3.356480
-30.657514	-14.431022	3.366477
-30.294126	-5.888775	3.376474
-30.414630	-4.157735	3.386470
-29.873241	-10.035946	3.396467
-29.222454	-5.523855	3.406464
-28.676358	-12.145975	3.416461
-27.771067	-9.680709	3.426458
-27.486901	-2.034452	3.436454
-27.401015	-3.172936	3.446451
-26.402491	-13.360951	3.456448
-26.164174	-13.145541	3.466445
-25.398783	-16.001119	3.476442
-24.583807	-10.373661	3.486438
-24.191586	-8.799662	3.496435
-23.952640	-11.129158	3.506432
-24.027373	-5.041329	3.516429
-23.445839	-7.892701	3.526426
-22.820158	-8.062840	3.536422
-21.904945	-5.584791	3.546419
-21.027341	-2.916002	3.556416
-20.814801	-9.586621	3.566413
-21.003514	-9.189017	3.576410
-20.169195	-3.159156	3.586406
-19.570201	-7.552524	3.596403
-18.808478	-0.336748	3.606400
-17.879912	-8.481767	3.616397
-18.095084	-12.995835	3.626394
-17.988135	-2.320700	3.636390
-17.253818	-0.480021	3.646387
-16.298516	-5.081927	3.656384
-16.000673	-7.916940	3.666381
-15.458266	-1.225207	3.676378
-14.758247	-7.075600	3.686374
-14.537676	-5.478962	3.696371
-14.182585	-11.116672	3.706368
-13.341093	-4.094158	3.716365
-12.873806	-2.925317	3.726362
-12.795966	-2.073807	3.736358
-12.092670	-4.894626	3.746355
-11.637941	-6.714016	3.756352
-10.966985	-3.292541	3.766349
-10.056392	-8.075235	3.776346
-9.598322	-6.330063	3.786342
-9.684614	-5.396803	3.796339
-9.498671	-6.215077	3.806336
-8.485166	-7.982391	3.816333
-8.263534	-3.511492	3.826330
-7.352537	-1.224872	3.836326
-6.769490	-7.555966	3.846323
-6.467926	-6.428193	3.856320
-6.236670	-9.834319	3.866317
-5.234988	-5.145904	3.876314
-5.047155	-2.117750	3.886310
-4.908284	-4.371045	3.896307
-4.193536	5.505963	3.906304
-3.713899	14.810572	3.916301
-3.261016	19.014681	3.926298
-2.897923	29.692655	3.936294
-2.614483	46.165189	3.946291
-1.959871	65.789573	3.956288
-1.329221	72.254970	3.966285
-0.730647	86.154361	3.976282
-0.641336	106.017526	3.986278
0.000000	116.392765	3.991283
0.388216	124.279148	3.996288
0.723381	125.848590	4.001293
0.595346	138.510786	4.006298
0.486070	137.412621	4.011302
0.786314	139.299095	4.016307
0.744538	144.620956	4.021312
0.886921	133.881295	4.026317
0.699092	143.109991	4.031322
0.692243	137.267211	4.036326
0.684874	138.907171	4.041331
0.595127	148.064316	4.046336
0.408097	143.332973	4.051341
0.374247	143.976051	4.056346
0.687748	151.276151	4.061350
0.959713	161.585813	4.066355
0.906724	173.377624	4.071360
1.191471	167.189690	4.076365
0.822920	167.829182	4.081370
0.770680	149.798830	4.086374
1.196395	159.203071	4.091379
0.653180	156.417382	4.096384
0.965818	157.695372	4.101389
1.024814	174.487605	4.106394
1.024576	172.653005	4.111398
1.211151	164.443751	4.116403
1.142282	160.453020	4.121408
0.838493	152.854591	4.126413
0.833137	168.974951	4.131418
1.468671	177.307852	4.136422
1.326870	171.621335	4.141427
0.782528	159.386259	4.146432
0.715890	162.215054	4.151437
0.980516	169.938088	4.156442
1.279541	168.255094	4.161446
1.272569	176.305468	4.166451
1.276048	185.095717	4.171456
1.223037	179.709533	4.176461
1.079076	192.913956	4.181466
1.383530	185.236896	4.186470
1.154821	175.441406	4.191475
1.214272	181.344900	4.196480
1.403842	185.808810	4.201485
1.224696	155.424687	4.206490
1.004803	154.266666	4.211494
1.320080	168.438562	4.216499
1.082446	165.472935	4.221504
1.684011	171.406607	4.226509
1.149018	178.154472	4.231514
1.128752	172.242370	4.236518
1.460268	177.110790	4.241523
1.218263	182.362164	4.246528
1.337210	167.605917	4.251533
1.402334	180.214325	4.256538
1.138749	183.736963	4.261542
1.293340	178.406446	4.266547
1.284760	189.849680	4.271552
1.398857	178.936094	4.276557
1.279171	185.322420	4.281562
1.385082	179.162851	4.286566
1.341777	181.383426	4.291571
1.195260	172.960769	4.296576
1.149954	185.543233	4.301581
1.361434	178.485514	4.306586
1.390759	179.672107	4.311590
1.361379	178.642325	4.316595
1.408892	176.815421	4.321600
1.810885	179.133082	4.326605
1.568460	184.699634	4.331610
1.670669	172.993243	4.336614
1.225367	180.270474	4.341619
1.545562	189.224147	4.346624
1.569487	187.116516	4.351629
1.171054	189.361842	4.356634
1.507127	199.757816	4.361638
2.030628	201.571788	4.366643
1.680656	209.120467	4.371648
1.901861	200.716938	4.376653
1.794063	192.277908	4.381658
1.579226	188.557341	4.386662
1.630354	174.559320	4.391667
1.436229	180.256599	4.396672
1.921466	190.641137	4.401677
1.562413	205.892914	4.406682
2.080635	208.693928	4.411686
1.588659	193.612124	4.416691
1.389649	196.193666	4.421696
1.704303	208.443089	4.426701
1.638558	211.831225	4.431706
1.368008	201.043244	4.436710
1.853065	204.687626	4.441715
1.724197	199.804589	4.446720
1.658013	197.164700	4.451725
1.653470	209.184322	4.456730
1.779875	207.673494	4.461734
1.981702	210.780736	4.466739
1.531599	202.380806	4.471744
1.472318	201.393551	4.476749
1.610551	215.430584	4.481754
2.065976	234.966908	4.486758
2.353080	227.123104	4.491763
1.981362	226.499530	4.496768
1.768304	208.608548	4.501773
1.965962	226.319697	4.506778
2.058677	238.878606	4.511782
2.351329	224.860653	4.516787
1.924652	214.753443	4.521792
1.934450	207.276306	4.526797
2.009694	226.544751	4.531802
2.364048	209.244379	4.536806
2.323847	208.035052	4.541811
2.091959	206.880489	4.546816
2.217561	204.035369	4.551821
1.817958	210.920500	4.556826
2.012763	205.222740	4.561830
2.506249	193.547960	4.566835
1.759000	208.242950	4.571840
2.053363	209.480752	4.576845
2.097782	222.859867	4.581850
2.198522	236.330020	4.586854
2.309475	241.657160	4.591859
2.280210	231.846333	4.596864
1.969347	219.662698	4.601869
2.153418	224.173107	4.606874
2.214566	226.550260	4.611878
1.900495	237.394952	4.616883
1.664020	238.410010	4.621888
2.059620	236.707892	4.626893
2.513490	244.257921	4.631898
2.425661	239.351515	4.636902
2.207215	242.691295	4.641907
2.169242	242.250132	4.646912
2.326674	231.978705	4.651917
2.629385	240.971603	4.656922
2.275601	234.211393	4.661926
3.223508	233.364218	4.666931
2.530798	232.036304	4.671936
2.646267	230.521756	4.676941
2.663488	247.816920	4.681946
2.312222	244.255031	4.686950
2.755827	234.845529	4.691955
2.451890	244.679099	4.696960
2.320112	232.411302	4.701965
2.539431	231.966787	4.706970
2.304598	234.315408	4.711974
2.586815	232.921881	4.716979
2.130594	244.307819	4.721984
2.295255	241.252116	4.726989
2.359571	235.640628	4.731994
2.250228	241.973473	4.736998
2.319816	233.474128	4.742003
2.391293	252.712743	4.747008
2.353963	244.604575	4.752013
2.596262	240.259920	4.757018
2.603841	243.795573	4.762022
2.586248	241.163432	4.767027
2.409036	237.489614	4.772032
2.537088	236.990431	4.777037
2.755944	256.372904	4.782042
3.138396	259.615556	4.787046
3.086286	254.776150	4.792051
2.452095	245.109580	4.797056
2.579989	250.268081	4.802061
2.409094	242.761397	4.807066
2.340959	253.595746	4.812070
2.690936	265.560771	4.817075
2.732546	274.589537	4.822080
2.828373	268.091331	4.827085
2.903714	279.562495	4.832090
2.886889	275.768143	4.837094
2.999918	272.212589	4.842099
2.690898	276.678022	4.847104
2.847096	269.232699	4.852109
2.673802	265.042055	4.857114
2.757950	271.138914	4.862118
3.134591	270.116810	4.867123
2.738429	276.884395	4.872128
3.091514	270.752409	4.877133
3.291778	264.754795	4.882138
2.990143	271.736923	4.887142
2.895644	260.040874	4.892147
2.783445	276.438470	4.897152
2.762529	268.322743	4.902157
3.000303	263.185432	4.907162
3.085988	272.691614	4.912166
2.960199	261.228040	4.917171
2.831931	271.372172	4.922176
2.716803	268.302028	4.927181
2.754186	266.203804	4.932186
3.002868	273.227485	4.937190
3.357656	262.922436	4.942195
3.025488	266.442023	4.947200
3.080615	264.871837	4.952205
3.131841	263.157172	4.957210
2.867815	270.849430	4.962214
3.481308	272.108591	4.967219
3.130216	279.117541	4.972224
2.941907	275.362774	4.977229
2.812240	268.819947	4.982234
2.885309	266.521966	4.987238
2.920995	264.446911	4.992243
3.058035	271.049130	4.997248
3.215995	290.259885	5.002253
3.488733	300.360854	5.007258
3.500925	297.225860	5.012262
3.291783	276.903738	5.017267
2.992322	274.853779	5.022272
3.109268	287.677465	5.027277
3.438548	297.214637	5.032282
3.316539	302.975022	5.037286
3.581492	300.965763	5.042291
2.991373	301.658352	5.047296
3.519377	301.758908	5.052301
3.433466	301.274857	5.057306
3.304378	302.779959	5.062310
3.429923	304.486862	5.067315
3.252456	302.473467	5.072320
3.144569	302.136889	5.077325
3.450691	298.631601	5.082330
3.235479	313.644050	5.087334
3.549927	300.073881	5.092339
3.444841	301.230112	5.097344
3.248363	303.159822	5.102349
3.579517	304.120147	5.107354
3.749757	292.614930	5.112358
3.524937	299.234538	5.117363
3.571292	309.362762	5.122368
3.526798	299.995899	5.127373
3.675350	308.281588	5.132378
3.282221	313.956851	5.137382
3.729394	303.609278	5.142387
3.696099	304.047755	5.147392
3.510654	301.372211	5.152397
3.891587	310.426019	5.157402
3.690291	307.858655	5.162406
3.464050	307.070056	5.167411
3.425907	309.436500	5.172416
3.659716	309.351363	5.177421
3.287112	303.373622	5.182426
3.387033	292.902604	5.187430
3.282106	297.007071	5.192435
3.245551	307.805458	5.197440
3.534316	311.154467	5.202445
3.840448	323.890487	5.207450
3.747276	328.990146	5.212454
3.941056	332.180727	5.217459
3.950152	313.335596	5.222464
3.658636	301.158860	5.227469
3.507653	304.918439	5.232474
3.561463	324.470043	5.237478
4.118745	319.418132	5.242483
3.587745	333.492171	5.247488
3.772020	332.595281	5.252493
3.993703	331.759789	5.257498
4.016327	333.856725	5.262502
3.755130	325.147494	5.267507
3.743417	329.862051	5.272512
4.007549	335.792454	5.277517
3.797355	335.232947	5.282522
3.874731	334.059034	5.287526
3.877438	327.763344	5.292531
3.742109	338.085580	5.297536
3.915150	325.204693	5.302541
3.748507	328.465490	5.307546
3.759067	334.178625	5.312550
4.133353	320.791424	5.317555
3.903582	325.987156	5.322560
4.263273	328.019214	5.327565
4.136648	336.628704	5.332570
3.858337	344.925168	5.337574
4.276456	323.457013	5.342579
4.307418	328.537835	5.347584
4.350588	322.135423	5.352589
4.279985	325.233546	5.357594
4.207210	329.071069	5.362598
4.089564	325.350982	5.367603
3.792710	341.980818	5.372608
4.187433	330.141715	5.377613
4.140795	331.991419	5.382618
4.263277	335.152149	5.387622
4.245216	331.316157	5.392627
4.207971	341.884614	5.397632
4.223695	331.166536	5.402637
4.230916	322.493255	5.407642
3.981068	322.407542	5.412646
4.210560	326.953095	5.417651
4.097098	324.224807	5.422656
4.033182	326.116532	5.427661
4.314420	331.947028	5.432666
3.854064	333.014775	5.437670
4.348581	346.562511	5.442675
4.234478	357.555672	5.447680
4.344580	359.073738	5.452685
4.616030	356.148944	5.457690
4.666077	355.263283	5.462694
4.632664	350.144517	5.467699
4.172325	336.841559	5.472704
4.027986	332.127076	5.477709
4.452298	347.495391	5.482714
4.358506	364.371783	5.487718
4.567382	361.584596	5.492723
4.541709	364.500679	5.497728
4.435343	357.713535	5.502733
4.722542	361.208728	5.507738
4.541907	361.442177	5.512742
4.441329	357.998856	5.517747
4.543139	366.343898	5.522752
4.858836	355.348135	5.527757
4.494859	342.030137	5.532762
4.379622	345.179247	5.537766
4.336173	345.065738	5.542771
4.650991	357.394574	5.547776
4.707818	367.912381	5.552781
4.523047	363.576508	5.557786
4.544408	367.268257	5.562790
4.907327	362.180279	5.567795
4.965961	361.355058	5.572800
4.593543	352.538896	5.577805
4.980737	343.185315	5.582810
4.486669	333.809361	5.587814
4.601222	336.871659	5.592819
4.825606	345.650751	5.597824
4.319902	346.576034	5.602829
4.865625	358.723462	5.607834
4.843622	361.497364	5.612838
4.835777	363.220003	5.617843
4.733262	363.350271	5.622848
4.766402	363.856203	5.627853
4.789939	350.544599	5.632858
4.692757	362.355599	5.637862
5.052465	351.296627	5.642867
4.931926	359.289997	5.647872
4.909852	361.216445	5.652877
5.202137	355.092007	5.657882
4.552514	359.551498	5.662886
4.990635	349.856035	5.667891
4.804822	353.790578	5.672896
4.515379	350.264028	5.677901
4.821629	356.131244	5.682906
4.630678	356.695518	5.687910
4.874957	345.212852	5.692915
4.841146	361.097492	5.697920
4.887010	363.363637	5.702925
5.082788	366.397522	5.707930
4.665709	378.710981	5.712934
4.969434	361.948003	5.717939
5.165504	377.290926	5.722944
5.268945	366.589404	5.727949
5.014417	351.279572	5.732954
5.086568	372.368246	5.737958
5.193633	360.000892	5.742963
4.870034	368.699285	5.747968
4.716950	365.439362	5.752973
4.787172	366.181271	5.757978
4.524820	376.434746	5.762982
5.264033	372.096235	5.767987
5.320365	394.203231	5.772992
5.218703	395.271097	5.777997
5.369913	394.749436	5.783002
4.739466	379.715983	5.788006
5.203680	388.180901	5.793011
4.889914	399.193375	5.798016
5.183499	401.937922	5.803021
5.028994	396.368653	5.808026
5.068975	391.929629	5.813030
5.332595	398.318997	5.818035
5.406774	397.847753	5.823040
5.070062	397.725782	5.828045
5.163498	397.401710	5.833050
5.294198	401.819078	5.838054
5.523341	394.145974	5.843059
5.165592	395.933938	5.848064
5.357215	398.569546	5.853069
5.350733	398.546415	5.858074
5.145782	401.197047	5.863078
5.253772	392.209918	5.868083
5.106463	396.775634	5.873088
4.964776	394.097676	5.878093
5.088322	411.266534	5.883098
5.289717	435.754397	5.888102
5.630106	428.466797	5.893107
5.781406	434.823934	5.898112
5.618230	433.784773	5.903117
5.271415	428.250726	5.908122
5.213346	431.482256	5.913126
5.667713	427.773179	5.918131
5.872053	433.137538	5.923136
5.536299	436.342444	5.928141
5.562850	430.576708	5.933146
5.666039	434.282771	5.938150
5.591226	438.021113	5.943155
5.674851	436.305909	5.948160
5.612227	425.081773	5.953165
5.787292	414.555536	5.958170
5.420603	416.820608	5.963174
5.426223	426.192228	5.968179
5.594869	435.910727	5.973184
5.560255	435.160402	5.978189
5.826161	438.087902	5.983194
5.690133	435.122894	5.988198
5.849190	428.452571	5.993203
5.716605	439.713938	5.998208
5.623549	431.886387	6.003213
5.896532	421.222022	6.008218
5.390365	440.374012	6.013222
5.763948	429.969357	6.018227
5.451316	435.436809	6.023232
5.345893	432.641171	6.028237
5.710480	437.778280	6.033242
5.684589	444.531611	6.038246
5.654348	433.968748	6.043251
5.641980	432.981618	6.048256
5.754377	432.298751	6.053261
6.068084	429.421024	6.058266
5.694253	439.318458	6.063270
5.937988	421.649094	6.068275
5.962731	426.910830	6.073280
6.221013	431.827641	6.078285
5.736019	419.216627	6.083290
5.368622	411.078366	6.088294
5.569710	422.325030	6.093299
5.541323	422.022075	6.098304
5.348460	437.912755	6.103309
5.795404	430.471595	6.108314
5.721818	439.043865	6.113318
5.916647	425.986248	6.118323
5.733998	435.963470	6.123328
5.695847	436.110529	6.128333
5.896907	435.605688	6.133338
5.921239	433.520450	6.138342
5.850459	422.221698	6.143347
5.493172	405.458793	6.148352
5.479970	421.036618	6.153357
5.535546	421.337780	6.158362
5.327744	440.101277	6.163366
5.303896	432.601868	6.168371
5.382058	433.745387	6.173376
5.536232	432.558972	6.178381
5.715030	421.796518	6.183386
5.400893	432.094301	6.188390
5.702843	430.136035	6.193395
5.610583	438.632564	6.198400
5.560175	445.555593	6.203405
5.644655	424.695903	6.208410
5.487090	427.905201	6.213414
5.542496	437.708219	6.218419
6.030770	445.423637	6.223424
5.886687	439.680472	6.228429
5.594311	425.614680	6.233434
5.579385	437.428817	6.238438
5.772754	426.582756	6.243443
5.825242	430.606588	6.248448
5.607312	432.520324	6.253453
5.956514	428.776042	6.258458
5.321556	443.205460	6.263462
5.452038	438.389491	6.268467
5.840810	432.705272	6.273472
5.645131	438.517839	6.278477
5.799374	440.097383	6.283482
5.624150	435.955452	6.288486
5.883029	443.155307	6.293491
5.806793	442.036368	6.298496
5.574058	438.650286	6.303501
5.612098	426.314215	6.308506
5.603323	434.228184	6.313510
5.780160	444.285605	6.318515
5.958884	436.504692	6.323520
5.633311	446.916648	6.328525
5.771993	447.527378	6.333530
5.718183	440.479837	6.338534
5.653165	433.202206	6.343539
5.604979	434.846970	6.348544
5.423797	440.690390	6.353549
5.993676	443.337391	6.358554
5.681104	430.863520	6.363558
5.555158	430.473195	6.368563
5.670928	430.735701	6.373568
5.732278	453.846191	6.378573
5.979196	449.206122	6.383578
5.515202	443.666375	6.388582
6.039289	433.137597	6.393587
5.946458	434.211702	6.398592
5.359477	428.224647	6.403597
5.630603	425.793280	6.408602
5.275818	438.070643	6.413606
5.906846	448.478028	6.418611
6.006015	451.580678	6.423616
5.547386	450.662756	6.428621
5.694225	439.871336	6.433626
5.602025	430.426445	6.438630
5.564002	436.435431	6.443635
5.701437	438.937046	6.448640
5.574006	451.952101	6.453645
5.934679	451.228105	6.458650
5.759538	459.712296	6.463654
5.836261	457.935484	6.468659
5.656403	452.529125	6.473664
5.326363	437.514834	6.478669
6.138500	444.139738	6.483674
5.782428	447.209687	6.488678
5.580475	429.697727	6.493683
5.497752	434.900962	6.498688
5.809722	444.216639	6.503693
5.858018	442.799596	6.508698
5.387302	443.619359	6.513702
5.579228	450.897567	6.518707
5.617941	451.567143	6.523712
5.912122	448.630189	6.528717
5.747728	439.874213	6.533722
5.688150	453.359802	6.538726
5.396878	447.820022	6.543731
6.099630	447.731679	6.548736
5.767362	447.249958	6.553741
5.674856	440.500148	6.558746
5.715000	451.433257	6.563750
5.749863	442.955123	6.568755
5.759899	450.736355	6.573760
5.692390	448.506664	6.578765
5.636727	438.529686	6.583770
5.668577	447.048823	6.588774
5.860578	448.475719	6.593779
5.957750	438.348386	6.598784
5.875348	444.339256	6.603789
5.623378	435.990412	6.608794
5.462148	438.059143	6.613798
5.420243	444.851032	6.618803
5.598791	434.147016	6.623808
5.867702	443.996444	6.628813
5.629686	446.699410	6.633818
5.822549	456.383731	6.638822
6.092822	451.738815	6.643827
6.042759	441.882456	6.648832
6.162901	439.665462	6.653837
6.032572	424.241208	6.658842
5.695742	430.670920	6.663846
5.801295	424.738421	6.668851
5.763612	428.957303	6.673856
5.707928	433.674324	6.678861
5.787595	432.219145	6.683866
5.903771	437.924435	6.688870
5.633674	429.945203	6.693875
5.639645	434.322518	6.698880
5.678905	438.626753	6.703885
5.685434	438.016135	6.708890
5.868713	435.763056	6.713894
5.732895	438.218372	6.718899
5.789102	427.682565	6.723904
5.781066	423.000777	6.728909
5.685644	428.319368	6.733914
5.856637	438.944738	6.738918
5.774357	447.302389	6.743923
5.710779	442.942323	6.748928
5.538295	446.126071	6.753933
5.931159	438.702526	6.758938
5.588873	443.199352	6.763942
5.767465	433.067052	6.768947
5.878372	432.411759	6.773952
5.648569	442.751453	6.778957
5.660920	441.606430	6.783962
5.766554	430.133689	6.788966
5.865930	436.748222	6.793971
5.961680	422.080903	6.798976
5.770955	408.913279	6.803981
5.772929	399.584848	6.808986
5.288519	403.940589	6.813990
5.614299	418.470292	6.818995
6.050525	438.106239	6.824000
5.510237	415.241985	6.829005
5.687977	414.050296	6.834010
5.444139	427.806248	6.839014
5.567102	436.296905	6.844019
5.927777	437.800306	6.849024
5.826474	442.467154	6.854029
5.530246	428.817246	6.859034
5.630746	431.496726	6.864038
5.961292	430.519522	6.869043
5.951380	426.129873	6.874048
5.341541	416.207494	6.879053
5.534835	417.586127	6.884058
5.786137	434.991298	6.889062
5.928902	431.966308	6.894067
5.773464	438.966675	6.899072
5.677414	432.167434	6.904077
5.863282	417.067216	6.909082
5.729356	411.556201	6.914086
5.421345	407.471147	6.919091
5.749525	421.872004	6.924096
5.401985	426.360815	6.929101
5.634566	432.921466	6.934106
5.543944	427.780261	6.939110
5.826833	440.995454	6.944115
5.687972	434.036162	6.949120
5.655369	429.601821	6.954125
6.103416	435.470398	6.959130
5.954433	432.689753	6.964134
5.747308	419.188605	6.969139
5.518990	411.660052	6.974144
5.572932	420.175326	6.979149
5.851417	422.532279	6.984154
5.754309	432.954516	6.989158
5.624986	423.656549	6.994163
5.898375	432.458965	6.999168
5.319980	420.475457	7.004173
5.516338	429.963447	7.009178
5.634397	434.090097	7.014182
5.931527	437.522104	7.019187
5.639552	439.422920	7.024192
5.467232	445.863434	7.029197
5.825935	437.604773	7.034202
5.830161	436.338955	7.039206
5.845915	438.963085	7.044211
6.110863	437.286483	7.049216
5.818759	422.169253	7.054221
5.669320	405.098127	7.059226
5.287171	410.384971	7.064230
5.439623	425.833413	7.069235
5.523465	431.440453	7.074240
5.740902	439.910764	7.079245
5.997282	427.627698	7.084250
5.627137	433.214656	7.089254
6.055793	437.225556	7.094259
5.800299	425.926841	7.099264
5.513165	413.161982	7.104269
5.694535	429.739324	7.109274
5.899731	436.356101	7.114278
5.699321	421.287846	7.119283
5.698621	403.259531	7.124288
5.355999	410.178250	7.129293
5.815786	413.878358	7.134298
5.811288	434.755634	7.139302
5.759740	423.962875	7.144307
6.061402	421.166264	7.149312
5.702238	407.245996	7.154317
5.273031	405.100650	7.159322
5.455421	420.132835	7.164326
5.413863	423.529156	7.169331
5.719450	434.228669	7.174336
5.228947	448.454268	7.179341
5.683453	452.186631	7.184346
5.425305	444.272800	7.189350
5.529777	442.210130	7.194355
5.631847	433.904990	7.199360
5.446939	437.743017	7.204365
5.476226	426.556374	7.209370
5.250198	443.291821	7.214374
5.159379	451.517303	7.219379
5.708573	449.486407	7.224384
5.691429	454.141620	7.229389
5.766084	456.136546	7.234394
5.871724	457.723728	7.239398
5.953255	461.412955	7.244403
6.043685	447.475081	7.249408
5.573641	445.683655	7.254413
5.750740	441.000569	7.259418
5.736024	437.834476	7.264422
5.610530	440.583664	7.269427
5.748781	429.416995	7.274432
5.483671	428.864587	7.279437
5.692223	432.308172	7.284442
5.759818	425.874451	7.289446
5.766684	446.109773	7.294451
5.714606	449.187890	7.299456
5.504103	442.399470	7.304461
5.798595	437.077611	7.309466
5.867919	445.236965	7.314470
5.764011	446.519886	7.319475
5.611527	433.743216	7.324480
5.043364	447.697120	7.329485
5.692153	442.028234	7.334490
5.396325	467.617650	7.339494
5.570514	467.662629	7.344499
5.626998	470.413616	7.349504
5.746480	460.909652	7.354509
5.763564	457.056672	7.359514
5.926700	469.705553	7.364518
5.783064	470.617675	7.369523
5.856425	458.634560	7.374528
5.710152	468.961059	7.379533
6.114096	457.501451	7.384538
5.787851	471.800163	7.389542
5.910116	462.222731	7.394547
6.118758	438.754903	7.399552
5.414342	448.450858	7.404557
5.808843	438.547968	7.409562
5.520613	450.393172	7.414566
5.531944	449.519133	7.419571
5.784948	434.381067	7.424576
5.527191	441.812706	7.429581
5.718599	445.095257	7.434586
5.760327	441.834299	7.439590
5.457326	452.471316	7.444595
5.828626	449.671281	7.449600
5.678725	463.582717	7.454605
5.631165	465.552951	7.459610
5.446892	460.779815	7.464614
5.646801	470.306114	7.469619
5.898208	472.569484	7.474624
5.667212	478.024052	7.479629
5.818914	474.209003	7.484634
5.647493	467.811112	7.489638
5.612624	477.329055	7.494643
5.753323	476.159367	7.499648
5.640224	470.011308	7.504653
5.762832	464.058218	7.509658
5.906175	465.895583	7.514662
5.374463	468.287874	7.519667
5.746341	467.799100	7.524672
5.767128	465.027883	7.529677
5.949794	465.617928	7.534682
5.743041	474.823017	7.539686
5.782565	462.151136	7.544691
5.905687	461.794434	7.549696
5.621634	453.284940	7.554701
5.812622	437.758245	7.559706
5.425210	443.689811	7.564710
5.435546	458.666115	7.569715
5.801857	461.831466	7.574720
5.849402	462.188120	7.579725
5.711066	461.126896	7.584730
5.447363	464.497387	7.589734
5.712389	469.395437	7.594739
5.899744	460.968454	7.599744
5.746473	475.203857	7.604749
5.803804	469.658651	7.609754
5.772170	462.481941	7.614758
5.711549	452.685528	7.619763
5.539335	450.358204	7.624768
5.519697	451.143776	7.629773
5.788761	458.529799	7.634778
5.927586	453.824818	7.639782
5.860843	450.116612	7.644787
5.436384	439.182035	7.649792
5.595134	452.738786	7.654797
5.546302	456.637991	7.659802
5.351955	455.332967	7.664806
5.426431	463.017230	7.669811
5.469715	455.486491	7.674816
5.047814	462.354404	7.679821
5.757639	464.298233	7.684826
5.718856	468.908190	7.689830
5.601078	469.530423	7.694835
5.891585	472.159075	7.699840
5.714974	466.932225	7.704845
5.898902	465.290122	7.709850
5.703775	468.355182	7.714854
5.830019	462.630576	7.719859
6.047884	464.076581	7.724864
5.698761	472.875639	7.729869
6.021592	476.893284	7.734874
5.820002	471.581275	7.739878
5.711200	470.714854	7.744883
6.115854	465.511817	7.749888
6.093152	471.576395	7.754893
5.530669	448.232236	7.759898
5.774856	456.654923	7.764902
5.561770	452.822618	7.769907
5.754822	453.613096	7.774912
5.722947	469.751769	7.779917
5.838500	457.911840	7.784922
5.742648	450.175605	7.789926
5.399807	446.587611	7.794931
5.919346	448.050948	7.799936
5.651077	463.122034	7.804941
6.102520	463.527272	7.809946
5.632406	450.046768	7.814950
5.661098	439.762243	7.819955
5.587949	435.239791	7.824960
5.524493	440.258412	7.829965
5.783888	448.907665	7.834970
5.913040	443.238623	7.839974
5.607030	439.309503	7.844979
5.756169	442.884061	7.849984
5.774048	446.752014	7.854989
5.512534	437.243544	7.859994
6.041949	444.143366	7.864998
5.742599	450.523482	7.870003
5.979005	440.135275	7.875008
5.550575	439.998962	7.880013
5.704527	445.525557	7.885018
6.012551	436.276460	7.890022
5.527309	435.516448	7.895027
5.673781	447.913824	7.900032
5.340897	449.002640	7.905037
5.400325	449.206087	7.910042
5.665330	441.066893	7.915046
5.809244	451.919319	7.920051
5.910487	449.012078	7.925056
5.483322	440.584450	7.930061
5.731281	428.947503	7.935066
5.574953	444.627634	7.940070
5.620236	450.961650	7.945075
5.781944	462.586199	7.950080
5.682621	473.815260	7.955085
5.865246	461.717501	7.960090
5.756116	452.422591	7.965094
5.199935	451.090543	7.970099
5.670258	456.038028	7.975104
5.661500	476.995485	7.980109
6.123687	476.742082	7.985114
6.081404	470.079066	7.990118
5.876533	446.229719	7.995136
6.337297	438.079320	8.000154
5.711568	442.209670	8.005171
5.989736	442.055030	8.010189
6.009481	435.384033	8.015206
5.924101	440.785256	8.020224
5.851475	431.948747	8.025242
5.558957	434.522058	8.030259
5.938849	433.807603	8.035277
5.763771	427.587325	8.040294
5.525375	445.131268	8.045312
5.871000	439.105886	8.050330
5.645202	440.105188	8.055347
5.652797	432.448793	8.060365
5.776014	434.014509	8.065382
5.714170	427.600356	8.070400
5.364072	433.480770	8.075418
5.878855	450.946109	8.080435
5.783016	443.578796	8.085453
5.811746	438.554714	8.090470
5.230401	444.751836	8.095488
5.896717	441.193541	8.100506
5.748312	428.898280	8.105523
5.740082	434.090136	8.110541
5.824836	442.109385	8.115558
5.516097	442.553015	8.120576
5.722757	435.011233	8.125594
5.376497	447.793125	8.130611
5.858425	450.496478	8.135629
6.111640	458.898644	8.140646
5.803476	471.506182	8.145664
6.224877	461.951227	8.150682
5.897194	450.081169	8.155699
5.569767	453.087040	8.160717
5.869351	446.554205	8.165734
5.985519	448.628175	8.170752
6.224998	455.586136	8.175770
5.835210	452.288767	8.180787
6.025618	442.663750	8.185805
6.358696	450.881880	8.190822
5.827229	451.133917	8.195840
5.793626	442.626419	8.200858
5.958521	440.818086	8.205875
5.885156	444.230309	8.210893
6.081866	435.867494	8.215910
5.898100	440.585998	8.220928
6.188143	436.746546	8.225946
5.693302	437.145946	8.230963
5.555675	439.996654	8.235981
5.779799	436.200373	8.240998
5.838111	447.718592	8.246016
6.318882	451.858375	8.251034
5.953114	450.320378	8.256051
5.618512	446.072930	8.261069
6.088297	444.283686	8.266086
5.965486	455.526193	8.271104
6.450033	456.489391	8.276122
5.940994	450.102092	8.281139
5.861022	443.175575	8.286157
6.060984	437.516522	8.291174
5.882303	447.567308	8.296192
6.166145	445.810367	8.301210
6.220727	441.042886	8.306227
5.813744	447.582383	8.311245
5.961593	441.078956	8.316262
5.872133	452.978814	8.321280
6.397538	449.583540	8.326298
6.301849	453.116754	8.331315
5.875852	448.722235	8.336333
6.231915	445.641998	8.341350
5.871806	446.339543	8.346368
6.098448	439.998947	8.351386
6.161961	446.181218	8.356403
6.092997	442.606172	8.361421
5.941917	437.861756	8.366438
5.922070	446.984106	8.371456
6.163576	446.420054	8.376474
6.218231	453.623870	8.381491
6.010234	449.906475	8.386509
5.866547	453.355021	8.391526
6.001607	471.633384	8.396544
5.812151	466.532477	8.401562
6.048092	468.677879	8.406579
5.892672	466.693288	8.411597
6.360063	479.023582	8.416614
6.198636	467.382188	8.421632
6.024535	455.866790	8.426650
6.008625	469.197633	8.431667
5.999051	465.298850	8.436685
6.439144	463.668419	8.441702
6.077345	467.878955	8.446720
6.130123	462.983149	8.451738
6.052382	469.527486	8.456755
5.906500	468.671319	8.461773
6.075490	466.063542	8.466790
5.930930	471.787193	8.471808
6.037891	461.421473	8.476826
5.856849	464.555291	8.481843
6.043192	457.275467	8.486861
6.427156	472.966831	8.491878
6.366076	484.153694	8.496896
5.977330	475.778279	8.501914
5.963153	484.576449	8.506931
6.249318	493.290647	8.511949
6.252778	496.986291	8.516966
6.444263	498.767165	8.521984
6.490275	496.174983	8.527002
6.223847	495.144283	8.532019
6.089349	492.299111	8.537037
6.214166	492.395164	8.542054
6.099672	500.258134	8.547072
6.162292	502.705949	8.552090
6.510742	503.212992	8.557107
6.286277	507.595492	8.562125
6.563018	501.974111	8.567143
6.535058	502.722753	8.572160
6.453917	492.160975	8.577178
6.281245	473.711413	8.582195
5.854137	479.265856	8.587213
6.263158	478.611828	8.592231
6.264640	491.981836	8.597248
6.345251	488.473480	8.602266
6.443813	493.694255	8.607283
5.992167	497.320844	8.612301
6.445822	503.757009	8.617319
6.538144	491.407648	8.622336
6.319216	500.754920	8.627354
6.467065	489.800546	8.632371
6.291237	496.162028	8.637389
6.409635	495.173915	8.642407
6.531000	495.095965	8.647424
6.635524	495.099130	8.652442
6.834424	495.819433	8.657459
6.428487	495.685244	8.662477
6.687031	484.569793	8.667495
6.348261	460.881771	8.672512
6.151072	465.907462	8.677530
6.653346	476.257959	8.682547
6.081464	488.778605	8.687565
6.507014	498.055192	8.692583
6.409079	491.320464	8.697600
6.737789	494.075912	8.702618
6.703334	485.905278	8.707635
6.393294	488.317844	8.712653
6.422438	463.589874	8.717671
6.451143	473.866198	8.722688
6.123476	490.905557	8.727706
6.553229	497.311326	8.732723
6.663374	496.428002	8.737741
6.602579	495.736871	8.742759
6.786271	500.424388	8.747776
6.585074	480.043974	8.752794
6.416458	468.802312	8.757811
6.428229	473.577176	8.762829
6.540644	488.013582	8.767847
6.607383	495.349352	8.772864
6.364365	504.313575	8.777882
6.616524	486.657506	8.782899
6.676972	497.483317	8.787917
6.664662	493.913460	8.792935
6.768638	496.654974	8.797952
6.104366	482.238548	8.802970
6.907755	480.208576	8.807987
6.800802	483.638265	8.813005
6.636704	466.821824	8.818023
6.398756	467.787808	8.823040
6.273322	476.963051	8.828058
6.767934	487.160422	8.833075
6.618197	501.046476	8.838093
6.734446	490.914589	8.843111
6.927730	495.375168	8.848128
6.356309	478.899892	8.853146
6.746363	486.000668	8.858163
6.398190	491.186037	8.863181
6.805776	501.292504	8.868199
6.517576	497.320587	8.873216
6.576846	499.439589	8.878234
6.878403	496.598818	8.883251
6.564991	490.129478	8.888269
6.613462	503.205959	8.893287
6.794710	498.242069	8.898304
6.607514	504.657589	8.903322
6.556951	491.960945	8.908339
6.551484	504.096029	8.913357
6.739484	490.808394	8.918375
6.729036	493.002389	8.923392
6.581475	504.226978	8.928410
6.782738	490.875548	8.933427
6.935922	504.269307	8.938445
7.040962	496.178254	8.943463
6.638566	493.539527	8.948480
6.367868	499.296235	8.953498
6.619746	504.956747	8.958515
6.623352	497.302356	8.963533
6.512735	490.386885	8.968551
6.632563	491.366271	8.973568
6.691932	503.509730	8.978586
6.515602	489.011580	8.983603
6.517864	495.793546	8.988621
6.455086	494.928367	8.993639
6.605494	508.711688	8.998656
6.583630	518.027881	9.003674
6.788030	512.959589	9.008691
6.974783	527.316240	9.013709
7.117275	509.535381	9.018727
7.335211	519.251529	9.023744
6.686885	514.691211	9.028762
6.829242	504.427466	9.033779
6.852524	509.248659	9.038797
6.923223	516.307459	9.043815
7.039241	500.485242	9.048832
7.159271	498.297677	9.053850
6.866654	481.623302	9.058867
6.815917	487.948463	9.063885
6.406893	493.126469	9.068903
6.790078	505.866590	9.073920
6.795088	514.208346	9.078938
6.803553	513.818604	9.083955
6.910836	523.631568	9.088973
6.607668	517.856948	9.093991
6.664122	520.743892	9.099008
6.940860	519.898083	9.104026
7.017322	516.317389	9.109043
7.021155	520.720028	9.114061
7.145255	524.446224	9.119079
7.051762	518.611269	9.124096
6.838751	527.259188	9.129114
7.163360	514.926824	9.134131
6.733497	518.293074	9.139149
6.695701	529.811984	9.144167
6.716191	523.284007	9.149184
6.589018	512.519134	9.154202
6.416566	518.853891	9.159219
6.897895	531.372341	9.164237
7.104828	552.669949	9.169255
7.343522	546.196044	9.174272
6.977616	548.996422	9.179290
7.319860	526.795459	9.184307
7.238264	530.595307	9.189325
7.027536	519.886157	9.194343
7.127660	515.745850	9.199360
6.995127	527.092753	9.204378
7.371919	529.171785	9.209395
7.126113	526.145924	9.214413
7.338956	529.905282	9.219431
7.211797	520.708904	9.224448
7.270247	513.897053	9.229466
7.338540	505.524326	9.234483
7.578449	519.783423	9.239501
7.249683	519.088651	9.244519
7.501836	521.792004	9.249536
7.433552	521.955493	9.254554
7.317018	508.742179	9.259571
7.326242	496.391195	9.264589
6.653392	494.015723	9.269607
7.087378	499.097324	9.274624
6.934543	521.809007	9.279642
7.161291	523.577760	9.284659
7.645917	520.612162	9.289677
7.136935	518.265304	9.294695
7.283719	514.967225	9.299712
7.187161	516.953448	9.304730
7.322563	516.275161	9.309747
7.158522	509.545248	9.314765
7.065510	515.063485	9.319783
7.273795	519.688981	9.324800
7.063887	527.131201	9.329818
6.884123	520.379575	9.334835
7.000950	525.587698	9.339853
7.194986	520.643436	9.344871
7.395752	528.713329	9.349888
7.357525	515.765756	9.354906
7.203566	515.062368	9.359923
7.167378	518.421425	9.364941
7.298386	516.450998	9.369959
7.555345	521.093152	9.374976
7.143503	520.045052	9.379994
7.180133	518.631851	9.385011
7.438815	512.714393	9.390029
7.489898	518.971076	9.395047
7.315125	512.604285	9.400064
7.245952	519.520583	9.405082
6.906505	521.656964	9.410099
7.056075	527.171134	9.415117
6.913766	524.398198	9.420135
7.213600	516.218753	9.425152
7.070770	521.864296	9.430170
7.113647	519.571095	9.435187
7.609594	537.922059	9.440205
7.375417	544.300781	9.445223
7.497791	529.977499	9.450240
7.364133	521.407669	9.455258
7.199944	535.568433	9.460275
7.399695	537.863303	9.465293
7.598823	553.184287	9.470311
7.546654	534.653430	9.475328
7.465257	530.202039	9.480346
7.106065	524.101403	9.485363
7.711767	534.813714	9.490381
7.657020	532.588504	9.495399
7.485550	520.264704	9.500416
7.601972	530.855937	9.505434
7.304534	530.069291	9.510451
7.155395	527.468514	9.515469
7.112570	535.160239	9.520487
7.606810	535.749470	9.525504
7.402159	550.488284	9.530522
7.563053	552.837304	9.535539
7.790733	548.425956	9.540557
7.800577	561.525303	9.545575
7.730086	538.007257	9.550592
7.810829	535.571699	9.555610
7.639415	532.381701	9.560627
7.351525	527.937373	9.565645
7.247520	522.449956	9.570663
7.510858	522.194439	9.575680
7.534349	529.561383	9.580698
7.476157	529.694765	9.585715
7.880712	540.582124	9.590733
7.489173	553.603334	9.595751
7.553775	541.602248	9.600768
7.802256	549.551492	9.605786
7.404308	543.349202	9.610803
7.606161	549.454923	9.615821
7.607516	555.385748	9.620839
7.694796	550.993271	9.625856
7.626262	558.848873	9.630874
7.654932	559.320984	9.635891
7.805782	551.135044	9.640909
7.663509	551.801613	9.645927
7.767496	547.850880	9.650944
7.775086	544.334799	9.655962
7.450556	535.950706	9.660979
7.775499	524.703804	9.665997
7.952497	541.123798	9.671015
7.585591	536.216729	9.676032
7.732458	520.393134	9.681050
7.203226	526.154001	9.686067
7.454729	538.743698	9.691085
7.461920	553.000543	9.696103
7.949648	554.556714	9.701120
7.985604	554.164790	9.706138
7.844239	549.322590	9.711155
8.182065	561.799241	9.716173
7.549869	556.322537	9.721191
7.808937	567.306483	9.726208
8.007246	557.797981	9.731226
7.522929	554.642564	9.736243
7.912648	544.450296	9.741261
7.651554	548.370050	9.746279
7.990010	543.357337	9.751296
8.052750	558.024810	9.756314
7.914265	551.681331	9.761331
7.925762	529.526657	9.766349
7.537770	529.223884	9.771367
7.901758	537.034469	9.776384
7.688404	535.071645	9.781402
7.515843	553.333042	9.786419
7.845076	546.715162	9.791437
7.579790	557.622596	9.796455
7.870261	548.053306	9.801472
7.848558	554.263972	9.806490
7.741436	558.903225	9.811507
7.795226	555.335616	9.816525
7.581872	559.415465	9.821543
7.942129	563.657659	9.826560
7.542302	550.128300	9.831578
7.577960	564.494701	9.836595
7.908306	559.688403	9.841613
7.585919	549.963745	9.846631
7.976577	564.738914	9.851648
8.088230	566.659147	9.856666
8.071785	565.539798	9.861683
8.093321	547.252505	9.866701
7.740011	562.760444	9.871719
7.971752	565.549250	9.876736
7.977098	560.664498	9.881754
7.767660	575.661954	9.886771
8.367838	582.348594	9.891789
8.059419	575.622928	9.896807
7.703116	567.367471	9.901824
8.232370	570.231104	9.906842
7.755286	583.459452	9.911859
8.351299	578.650773	9.916877
8.080809	580.909305	9.921895
8.059191	576.498308	9.926912
8.071387	570.774092	9.931930
8.251742	577.657348	9.936947
7.706425	563.273245	9.941965
7.888137	573.187896	9.946983
7.995186	584.946150	9.952000
8.094020	575.448859	9.957018
7.980476	589.818193	9.962035
8.554585	580.998419	9.967053
8.157124	586.774731	9.972071
8.439757	582.404479	9.977088
8.356009	569.751437	9.982106
8.386961	573.762280	9.987123
7.990285	550.368676	9.992141
8.083472	563.099791	9.997159
8.159200	573.349221	10.002176
8.280971	578.063920	10.007194
8.013860	576.154749	10.012211
8.044002	578.213628	10.017229
8.304653	582.350066	10.022247
8.171417	586.175388	10.027264
8.462614	587.589860	10.032282
8.317294	584.923198	10.037299
8.166412	563.659814	10.042317
8.314125	568.493921	10.047335
8.309766	566.548416	10.052352
8.200625	559.621353	10.057370
8.043185	556.560611	10.062387
8.480570	567.627274	10.067405
8.352808	555.526987	10.072423
7.987858	560.690647	10.077440
7.931983	575.119125	10.082458
7.985373	584.876382	10.087475
8.115751	580.046145	10.092493
8.220741	585.068288	10.097511
8.125143	585.280967	10.102528
8.152045	587.798172	10.107546
8.255375	598.832480	10.112563
8.595638	582.817539	10.117581
8.268421	587.721575	10.122599
8.033159	589.700813	10.127616
8.244117	579.467800	10.132634
8.299610	587.628746	10.137651
8.287615	579.765317	10.142669
8.192217	585.400487	10.147687
7.957342	591.244797	10.152704
8.179357	601.141096	10.157722
8.468183	613.459971	10.162739
8.615909	602.377313	10.167757
8.658107	614.784280	10.172775
8.549425	615.427194	10.177792
8.621933	593.991444	10.182810
8.463464	595.032572	10.187827
8.352424	586.848955	10.192845
8.597685	584.416315	10.197863
8.329169	585.273303	10.202880
8.469045	588.945638	10.207898
8.518023	595.213230	10.212915
8.545176	601.482266	10.217933
8.616067	602.845760	10.222951
8.326892	598.120278	10.227968
8.633753	600.601946	10.232986
8.815252	593.670924	10.238003
8.572639	577.218848	10.243021
8.581521	585.735463	10.248039
8.068952	580.869475	10.253056
8.547982	589.883390	10.258074
8.521570	606.726466	10.263091
8.532374	611.377441	10.268109
9.110403	608.068991	10.273127
8.582119	600.302974	10.278144
8.787833	588.478496	10.283162
8.433697	584.885495	10.288179
8.454988	585.729624	10.293197
8.882299	604.430531	10.298215
8.869687	596.548793	10.303232
8.723895	575.839273	10.308250
8.507772	583.157766	10.313267
8.459401	590.031000	10.318285
8.407657	590.569147	10.323303
8.614406	607.380877	10.328320
8.932705	605.250082	10.333338
8.922691	606.468905	10.338355
8.617549	591.913711	10.343373
8.751036	589.687892	10.348391
8.631524	588.298422	10.353408
8.877654	593.134772	10.358426
8.682652	588.164540	10.363443
8.648433	584.087845	10.368461
8.473646	584.418120	10.373479
8.500046	615.038328	10.378496
8.896839	607.486100	10.383514
8.609533	611.373890	10.388531
8.782743	611.916096	10.393549
8.340120	619.348302	10.398567
8.423641	617.155535	10.403584
8.582882	608.338077	10.408602
8.696289	607.601719	10.413619
8.749822	608.558315	10.418637
8.758638	607.317979	10.423655
8.887998	613.251487	10.428672
9.001404	605.522707	10.433690
8.869991	615.806495	10.438707
8.921054	610.012959	10.443725
8.703198	605.013237	10.448743
8.778416	611.267347	10.453760
8.884817	599.525893	10.458778
8.830345	611.827694	10.463795
8.539910	608.374921	10.468813
9.006136	606.904595	10.473831
8.418484	623.594222	10.478848
9.112891	621.688227	10.483866
8.944134	633.230136	10.488883
9.102415	636.041525	10.493901
9.080612	623.009076	10.498919
9.019857	613.353129	10.503936
8.728429	608.543976	10.508954
8.663187	624.445827	10.513971
9.134771	638.385205	10.518989
9.040748	630.489546	10.524007
8.963541	646.396054	10.529024
9.182362	643.329405	10.534042
9.200012	643.648151	10.539059
9.046035	629.615775	10.544077
9.224338	616.400192	10.549095
8.851146	613.064027	10.554112
8.773143	616.822956	10.559130
8.898867	639.076255	10.564147
9.236051	642.355235	10.569165
9.640563	644.094330	10.574183
9.101246	637.781431	10.579200
9.213739	620.307709	10.584218
8.886365	611.139936	10.589235
8.919756	616.860410	10.594253
9.054519	629.552431	10.599271
9.339850	639.856228	10.604288
9.251748	630.937235	10.609306
9.267095	616.303962	10.614323
8.784266	611.523879	10.619341
9.212300	611.325676	10.624359
9.168552	631.543175	10.629376
9.062623	641.050172	10.634394
9.364070	635.839940	10.639411
9.199741	643.850760	10.644429
9.320490	649.796038	10.649447
9.195436	643.449120	10.654464
9.444344	631.996634	10.659482
9.195245	629.502598	10.664499
9.108253	633.844899	10.669517
9.321714	631.585291	10.674535
9.237843	634.697673	10.679552
9.272662	634.121224	10.684570
9.068410	636.170724	10.689587
8.969295	647.434942	10.694605
9.390659	654.482206	10.699623
9.188774	648.176128	10.704640
9.190820	638.434801	10.709658
9.091726	633.770300	10.714675
8.822494	648.108734	10.719693
9.223252	628.509295	10.724711
9.458268	643.828179	10.729728
9.395280	643.595294	10.734746
9.111497	641.509770	10.739763
9.083929	644.206722	10.744781
9.085989	636.352455	10.749799
9.201515	642.580727	10.754816
9.307694	651.841890	10.759834
9.563381	654.281935	10.764851
9.202700	654.562827	10.769869
9.726238	662.916693	10.774887
9.186701	662.659527	10.779904
9.392645	668.292952	10.784922
9.695034	673.100940	10.789939
9.130597	674.642943	10.794957
9.496882	668.486226	10.799975
9.468720	668.268449	10.804992
9.723633	668.384236	10.810010
9.535328	674.249222	10.815027
9.791604	674.208415	10.820045
9.604503	649.315820	10.825063
9.604648	641.183669	10.830080
9.370431	642.211732	10.835098
9.379204	639.765417	10.840115
9.356670	639.604967	10.845133
9.714446	655.879187	10.850151
9.497091	652.344261	10.855168
9.536687	660.111093	10.860186
9.938029	662.202619	10.865203
9.570289	656.644289	10.870221
9.614701	654.250733	10.875239
9.298957	642.722389	10.880256
9.286321	659.360428	10.885274
9.758321	665.360047	10.890291
9.708491	671.581214	10.895309
9.712156	669.879307	10.900327
9.310734	669.887848	10.905344
9.445383	676.393829	10.910362
9.469671	670.469582	10.915379
9.589724	674.608812	10.920397
9.664645	675.908862	10.925415
10.076710	678.606483	10.930432
9.776286	676.932095	10.935450
9.871657	669.185893	10.940467
9.616578	679.884873	10.945485
9.604415	671.323321	10.950503
9.681929	675.688537	10.955520
9.588900	675.506376	10.960538
9.808851	671.045098	10.965555
9.595728	684.944253	10.970573
9.823256	667.095822	10.975591
9.720029	671.872924	10.980608
9.571253	673.169989	10.985626
10.066625	672.692496	10.990643
9.756796	672.231455	10.995661
9.664212	663.107906	11.000679
9.821190	678.388450	11.005696
9.753490	676.393863	11.010714
10.040033	669.918690	11.015731
9.765106	667.767339	11.020749
10.044281	669.594657	11.025767
10.178023	669.526864	11.030784
10.010006	668.181616	11.035802
9.963992	670.530208	11.040819
9.852593	676.876885	11.045837
9.840580	676.355311	11.050855
9.764335	668.866366	11.055872
9.859043	681.201728	11.060890
9.944415	665.076194	11.065907
9.829442	679.064813	11.070925
9.578243	672.121320	11.075943
9.732899	665.165377	11.080960
9.939739	668.170286	11.085978
9.814958	673.490618	11.090995
9.788435	683.507851	11.096013
9.697937	696.023509	11.101031
10.000593	700.429171	11.106048
10.022327	712.047809	11.111066
10.407609	703.818127	11.116083
10.013625	704.318855	11.121101
10.017773	699.341263	11.126119
10.439124	702.278157	11.131136
10.087867	691.774656	11.136154
10.550902	675.432792	11.141171
10.108524	678.669573	11.146189
9.640928	680.056818	11.151207
9.571735	680.006619	11.156224
9.980205	694.192459	11.161242
9.992369	701.868882	11.166259
10.010398	704.794292	11.171277
9.748410	697.344786	11.176295
10.088050	706.760379	11.181312
10.088428	706.222684	11.186330
10.048221	700.090028	11.191347
10.053829	691.310900	11.196365
10.320474	706.083967	11.201383
10.053215	706.302383	11.206400
9.885131	702.833305	11.211418
10.080348	707.232121	11.216435
10.205041	709.429105	11.221453
10.206498	698.036062	11.226471
10.517401	699.167810	11.231488
10.035202	708.689990	11.236506
10.138682	699.149541	11.241523
9.991971	719.892053	11.246541
10.178045	737.827027	11.251559
10.294897	735.688764	11.256576
10.232921	740.917947	11.261594
10.810773	732.800200	11.266611
10.290141	734.735096	11.271629
10.144036	722.763573	11.276647
10.426880	738.746281	11.281664
10.000039	749.604183	11.286682
10.774671	730.127248	11.291699
10.577888	732.940058	11.296717
10.378429	741.396520	11.301735
10.984373	737.771771	11.306752
10.336414	724.048362	11.311770
10.249881	711.478818	11.316787
10.483983	706.246135	11.321805
10.488724	703.549536	11.326823
10.470585	699.272255	11.331840
10.277774	702.108809	11.336858
10.173873	709.495907	11.341875
10.421819	728.436116	11.346893
10.435914	734.141125	11.351911
10.645173	728.077055	11.356928
10.111533	744.316724	11.361946
10.352801	732.677368	11.366963
11.079597	727.495714	11.371981
10.558470	725.092966	11.376999
10.927493	729.417799	11.382016
10.682574	725.674456	11.387034
10.761829	708.008327	11.392051
10.584173	705.685904	11.397069
10.535863	707.378304	11.402087
10.455233	697.629936	11.407104
10.032928	705.747287	11.412122
10.309641	707.173906	11.417139
10.688547	731.816568	11.422157
10.434674	727.332216	11.427175
10.774432	732.755592	11.432192
10.654627	742.936678	11.437210
10.333907	733.539721	11.442227
10.707724	733.143622	11.447245
10.836636	733.718641	11.452263
10.978919	730.885155	11.457280
10.450801	742.253600	11.462298
11.122683	729.660168	11.467315
10.837162	735.924640	11.472333
10.906069	728.532425	11.477351
10.960962	733.788249	11.482368
10.865647	726.257848	11.487386
10.461471	720.895049	11.492403
10.736966	725.121282	11.497421
10.653518	728.862735	11.502439
10.635630	727.385998	11.507456
10.787789	737.569275	11.512474
10.588012	735.060576	11.517491
10.824273	737.366959	11.522509
10.802912	734.157141	11.527527
10.743622	729.911451	11.532544
10.753950	727.970486	11.537562
10.708196	722.293874	11.542579
11.096900	725.733226	11.547597
10.996882	734.549760	11.552615
10.891629	729.994004	11.557632
10.553333	732.600909	11.562650
10.658573	730.886047	11.567667
10.814775	732.718737	11.572685
10.735885	726.374981	11.577703
10.774283	724.191722	11.582720
10.491591	731.576788	11.587738
10.966649	741.532033	11.592755
11.393561	748.448230	11.597773
11.298285	755.802337	11.602791
11.172723	735.278301	11.607808
10.924763	729.147392	11.612826
11.272735	725.942770	11.617843
11.204334	723.736420	11.622861
10.700867	736.226967	11.627879
11.143248	718.432326	11.632896
11.020918	721.946386	11.637914
10.833285	732.831958	11.642931
11.269007	721.629981	11.647949
10.858353	730.533175	11.652967
11.317140	715.542718	11.657984
11.078620	733.580426	11.663002
11.024038	723.155119	11.668019
11.039022	723.380033	11.673037
10.980521	745.282304	11.678055
11.423015	743.534244	11.683072
11.131332	749.595838	11.688090
11.218296	748.547068	11.693107
11.362539	741.154895	11.698125
10.971850	743.018131	11.703143
11.572356	744.140403	11.708160
10.986937	730.722838	11.713178
11.246451	737.544077	11.718195
11.224280	736.196470	11.723213
11.333790	759.809473	11.728231
11.433980	751.440297	11.733248
11.146777	737.042209	11.738266
11.101605	725.713731	11.743283
11.566751	742.105610	11.748301
11.104774	736.244277	11.753319
11.372516	743.316378	11.758336
11.438850	753.494462	11.763354
11.544137	751.074890	11.768371
11.648241	736.457735	11.773389
10.985105	734.913937	11.778407
11.282945	722.137386	11.783424
11.044737	732.708046	11.788442
11.365284	746.574173	11.793459
11.540003	749.921553	11.798477
11.404458	766.143382	11.803495
11.529571	749.265062	11.808512
11.581385	757.913039	11.813530
11.403197	762.437445	11.818547
11.350500	755.833684	11.823565
11.279628	755.145486	11.828583
11.353841	747.344779	11.833600
11.202397	758.086913	11.838618
11.174529	761.556833	11.843635
11.550227	753.862868	11.848653
11.284411	761.748714	11.853671
11.470103	758.962371	11.858688
11.459685	759.520757	11.863706
11.290707	765.351191	11.868723
11.793063	756.526741	11.873741
11.460047	760.986001	11.878759
11.546372	756.454474	11.883776
11.920099	759.062103	11.888794
11.519435	760.138542	11.893811
11.668761	750.451532	11.898829
11.197900	760.275853	11.903847
11.640525	756.421146	11.908864
11.471004	760.849549	11.913882
11.461128	765.673546	11.918899
11.848778	756.722702	11.923917
11.130106	764.286704	11.928935
11.516671	776.692395	11.933952
11.556168	777.932474	11.938970
11.666628	783.254513	11.943987
11.726436	789.330367	11.949005
11.881978	797.887616	11.954023
12.025969	794.057352	11.959040
12.152555	784.486264	11.964058
11.711110	781.215663	11.969075
11.789429	775.778916	11.974093
11.862370	784.213118	11.979111
11.831621	785.689374	11.984128
11.984031	778.005332	11.989146
11.929617	767.008117	11.994163
12.133765	758.833334	11.999181
12.158497	756.689036	12.004199
11.930087	760.043303	12.009216
11.938162	758.018370	12.014234
11.583718	756.472073	12.019251
11.877111	758.383848	12.024269
11.368823	761.641084	12.029287
11.928173	759.304321	12.034304
12.274568	780.749937	12.039322
11.890655	780.928094	12.044339
11.780003	761.978060	12.049357
12.235648	775.281528	12.054375
11.827392	756.381862	12.059392
12.043629	754.055943	12.064410
11.615602	765.114312	12.069427
12.094089	786.731873	12.074445
12.049751	787.811427	12.079463
11.961166	790.432479	12.084480
12.364699	791.439201	12.089498
12.101640	781.156064	12.094515
11.898485	769.773753	12.099533
11.869079	778.116124	12.104551
11.860071	783.851932	12.109568
12.027255	793.211054	12.114586
11.805846	788.182533	12.119603
12.176232	792.035979	12.124621
12.074676	787.284452	12.129639
11.762690	780.863858	12.134656
11.915555	783.620766	12.139674
11.779696	787.918439	12.144691
12.207012	791.999248	12.149709
12.045672	798.021116	12.154727
11.932865	788.377794	12.159744
12.223482	784.638834	12.164762
11.977342	781.788833	12.169779
12.337425	798.392196	12.174797
12.016246	807.173481	12.179815
12.212111	817.908351	12.184832
12.400492	818.044484	12.189850
12.313599	813.014195	12.194867
12.443576	802.120515	12.199885
12.491370	819.722395	12.204903
12.321613	807.973475	12.209920
12.340260	800.423221	12.214938
12.309932	814.932629	12.219955
12.360352	810.750367	12.224973
12.192667	798.404757	12.229991
12.214841	802.681042	12.235008
12.728893	808.252580	12.240026
12.449287	813.182573	12.245043
12.735212	814.647043	12.250061
12.282754	801.670062	12.255079
12.016926	796.854750	12.260096
12.588206	807.606498	12.265114
12.683805	815.732005	12.270131
12.609363	816.319572	12.275149
12.652119	799.903254	12.280167
12.199448	792.336419	12.285184
12.879879	798.914929	12.290202
12.378874	803.850408	12.295219
12.667406	792.144841	12.300237
12.297521	789.508955	12.305255
12.651110	799.418673	12.310272
12.552922	802.599880	12.315290
12.816564	813.344410	12.320307
12.715944	803.674660	12.325325
12.564513	788.959057	12.330343
12.343278	786.209843	12.335360
12.644639	793.220811	12.340378
12.500015	794.900894	12.345395
12.863501	805.078028	12.350413
12.749828	812.642352	12.355431
12.495034	813.683077	12.360448
12.814141	807.478206	12.365466
12.736302	810.667664	12.370483
12.754079	806.661635	12.375501
12.909820	801.881755	12.380519
12.549890	795.926284	12.385536
12.925204	787.229289	12.390554
12.656351	797.169044	12.395571
12.708916	804.681881	12.400589
13.006778	802.051373	12.405607
12.695804	810.628646	12.410624
12.753139	795.652789	12.415642
13.008553	804.237033	12.420659
12.751546	796.228876	12.425677
12.893149	803.967902	12.430695
12.627699	810.659625	12.435712
12.874796	811.178508	12.440730
12.501814	807.828882	12.445747
12.761181	808.517361	12.450765
13.153891	815.433336	12.455783
12.734565	818.072639	12.460800
12.758552	813.242296	12.465818
12.717273	819.543297	12.470835
13.103824	810.355932	12.475853
12.850427	814.364426	12.480871
12.697490	814.966540	12.485888
12.806983	815.395583	12.490906
12.729527	817.052562	12.495923
12.699107	814.849074	12.500941
12.807924	808.989925	12.505959
12.916995	812.601963	12.510976
12.992658	828.042329	12.515994
12.996400	851.660356	12.521011
13.320850	851.034559	12.526029
13.110767	830.751196	12.531047
12.928492	829.700563	12.536064
13.053843	823.590490	12.541082
13.121576	831.649953	12.546099
13.236837	831.924526	12.551117
13.503358	840.852763	12.556135
13.077553	832.322575	12.561152
13.213964	821.219783	12.566170
13.208674	825.137288	12.571187
12.953789	824.087436	12.576205
13.393035	825.041416	12.581223
13.120021	840.648649	12.586240
13.348472	831.583641	12.591258
13.505727	835.322542	12.596275
12.912309	826.382530	12.601293
13.053472	825.567376	12.606311
13.322386	843.905250	12.611328
13.332007	835.405054	12.616346
13.162174	834.262617	12.621363
13.175892	846.262243	12.626381
13.918986	840.253588	12.631399
13.257230	848.052769	12.636416
13.695888	836.227296	12.641434
13.657942	832.072425	12.646451
13.412749	818.562443	12.651469
13.202276	804.910144	12.656487
13.162937	819.082323	12.661504
13.347592	837.902145	12.666522
13.501210	832.842141	12.671539
13.092680	840.108412	12.676557
13.453901	829.873430	12.681575
13.325871	839.158354	12.686592
13.568304	836.253780	12.691610
13.672748	834.477336	12.696627
13.514560	851.618296	12.701645
13.385348	839.166902	12.706663
13.294661	843.382138	12.711680
13.344483	842.330938	12.716698
13.332145	842.302046	12.721715
13.444323	835.484422	12.726733
13.746978	834.177697	12.731751
13.302429	840.057045	12.736768
13.649113	831.815468	12.741786
13.692505	845.278447	12.746803
13.659625	840.760985	12.751821
13.705253	832.711654	12.756839
13.542446	832.369299	12.761856
13.536143	832.098505	12.766874
13.760952	842.542438	12.771891
13.530603	837.064863	12.776909
13.507912	840.002342	12.781927
13.573816	866.732037	12.786944
13.672833	859.188745	12.791962
14.319364	850.685240	12.796979
13.684388	855.105761	12.801997
14.411015	832.398292	12.807015
13.831665	835.842455	12.812032
13.888865	831.245160	12.817050
13.992858	833.013864	12.822067
13.556881	833.852287	12.827085
13.837710	828.415219	12.832103
13.841689	838.955869	12.837120
13.949599	818.573916	12.842138
13.944528	823.749243	12.847155
13.668538	829.874701	12.852173
13.924637	821.843932	12.857191
13.967463	833.621453	12.862208
13.874809	831.912023	12.867226
14.157629	842.220013	12.872243
13.714062	834.843156	12.877261
13.923969	832.890452	12.882279
13.902187	845.580279	12.887296
14.001640	856.771587	12.892314
14.447138	867.334356	12.897331
14.136506	855.994639	12.902349
13.958740	843.023008	12.907367
14.030086	833.844615	12.912384
14.345939	833.529440	12.917402
13.904318	836.876839	12.922419
13.735946	837.016228	12.927437
14.260659	849.654520	12.932455
14.375003	871.668738	12.937472
14.355428	858.121241	12.942490
14.032768	850.697234	12.947507
13.745731	857.661988	12.952525
14.079842	860.206508	12.957543
14.355906	858.174769	12.962560
14.095823	855.460107	12.967578
14.336664	860.691446	12.972595
14.328268	865.181820	12.977613
14.263856	863.606280	12.982631
14.362952	860.713776	12.987648
14.380558	858.874134	12.992666
14.556389	857.044165	12.997683
14.354293	854.544686	13.002701
14.387259	855.822655	13.007719
13.999610	857.202410	13.012736
14.217477	853.364057	13.017754
14.523219	850.245706	13.022771
14.128481	854.733791	13.027789
14.101131	852.967119	13.032807
14.120308	864.008537	13.037824
14.375608	858.781156	13.042842
14.772376	870.683648	13.047859
14.274981	871.413147	13.052877
14.688743	853.434529	13.057895
14.539298	850.968272	13.062912
14.501304	849.747953	13.067930
14.401987	853.047251	13.072947
14.427917	860.535782	13.077965
14.658694	851.445973	13.082983
14.626342	858.847693	13.088000
14.416337	855.293988	13.093018
14.614443	847.058258	13.098035
14.479351	855.595469	13.103053
14.769356	854.700214	13.108071
14.171284	851.534601	13.113088
14.232860	857.158297	13.118106
14.375777	858.456279	13.123123
14.451556	857.505496	13.128141
14.677337	870.294960	13.133159
14.948008	883.112836	13.138176
14.965336	880.105320	13.143194
14.959173	859.590417	13.148211
14.534705	860.793414	13.153229
14.569326	855.113016	13.158247
14.432830	849.561472	13.163264
14.841042	862.885452	13.168282
15.153428	865.918522	13.173299
14.737538	873.836508	13.178317
15.039376	862.643760	13.183335
14.668593	859.451804	13.188352
14.656088	859.355628	13.193370
15.240844	858.925161	13.198387
14.528988	867.584655	13.203405
14.590983	861.764320	13.208423
14.970116	878.448467	13.213440
14.872017	875.450185	13.218458
15.150044	881.257376	13.223475
15.107344	889.710647	13.228493
15.092869	877.655351	13.233511
15.107856	861.979261	13.238528
14.827703	860.100453	13.243546
15.061546	857.177023	13.248563
14.858912	853.902565	13.253581
14.990498	867.599766	13.258599
15.153614	878.994314	13.263616
15.188338	875.383236	13.268634
15.037645	859.863836	13.273651
14.930763	873.035781	13.278669
15.136170	874.088633	13.283687
15.203204	883.526358	13.288704
15.311443	883.633026	13.293722
15.204523	878.101186	13.298739
14.691110	872.257059	13.303757
14.945586	877.497959	13.308775
15.180229	880.359461	13.313792
15.076667	894.222493	13.318810
15.138262	883.920866	13.323827
14.845257	888.160888	13.328845
14.510272	881.285664	13.333863
14.820781	880.165599	13.338880
15.149047	882.985059	13.343898
15.386778	892.296172	13.348915
15.509537	900.608346	13.353933
15.726791	886.255473	13.358951
15.447041	881.857523	13.363968
15.334750	874.288326	13.368986
15.832448	863.319468	13.374003
15.471567	873.102855	13.379021
15.461413	871.034569	13.384039
15.577530	865.881556	13.389056
15.449731	883.399946	13.394074
15.556731	867.895424	13.399091
15.848450	874.581109	13.404109
15.497268	871.257980	13.409127
15.808477	869.079707	13.414144
15.555013	877.318040	13.419162
15.560339	877.233482	13.424179
15.735018	878.422100	13.429197
15.453935	863.643023	13.434215
15.545278	865.501602	13.439232
15.705101	872.665109	13.444250
15.291974	866.538313	13.449267
15.611043	878.205661	13.454285
15.496900	879.802382	13.459303
15.639117	878.984099	13.464320
15.353712	874.567797	13.469338
15.372157	872.093670	13.474355
16.040934	866.141964	13.479373
15.780960	874.704349	13.484391
15.954583	867.000914	13.489408
15.258696	877.533251	13.494426
15.837154	872.975373	13.499443
15.727270	876.703517	13.504461
15.539360	880.689004	13.509479
15.870053	872.837583	13.514496
15.497737	870.693735	13.519514
15.517508	856.670523	13.524531
15.283647	869.866401	13.529549
15.865351	875.016616	13.534567
15.681885	873.857730	13.539584
15.637591	896.172761	13.544602
16.153783	886.753922	13.549619
15.997476	896.591101	13.554637
15.657361	895.576585	13.559655
15.863696	893.317822	13.564672
15.489844	897.952640	13.569690
15.930443	905.769452	13.574707
15.715595	903.510616	13.579725
15.721672	902.924047	13.584743
16.010995	899.566903	13.589760
15.592846	893.099250	13.594778
15.902013	891.471419	13.599795
15.777858	891.067763	13.604813
15.847351	900.913685	13.609831
16.469995	908.266037	13.614848
16.287522	908.145989	13.619866
16.037602	890.980431	13.624883
15.907209	908.294982	13.629901
16.178035	919.292885	13.634919
16.720067	907.290852	13.639936
16.243847	904.227316	13.644954
16.306836	888.951860	13.649971
16.217710	892.072346	13.654989
16.045563	896.019805	13.660007
16.385993	882.320092	13.665024
16.096479	886.036788	13.670042
16.223741	882.122274	13.675059
16.621991	884.473551	13.680077
16.409743	888.449285	13.685095
16.498841	883.535337	13.690112
16.651804	890.601972	13.695130
16.869181	882.105994	13.700147
16.705404	889.270238	13.705165
16.492637	901.980651	13.710183
16.295380	889.919138	13.715200
16.355659	886.381380	13.720218
16.601892	879.633694	13.725235
16.490295	879.280513	13.730253
16.618557	892.292966	13.735271
16.502336	878.277445	13.740288
16.239486	886.744856	13.745306
16.211029	887.925515	13.750323
16.451874	887.114945	13.755341
16.055776	891.749698	13.760359
16.206218	891.505944	13.765376
16.435308	885.611735	13.770394
15.944494	890.989186	13.775411
16.087561	907.960563	13.780429
16.157882	917.507787	13.785447
16.497078	906.312770	13.790464
16.406058	912.301412	13.795482
16.538330	915.741361	13.800499
16.690991	913.408013	13.805517
16.410081	933.658606	13.810535
16.858291	929.630225	13.815552
16.602728	919.424286	13.820570
16.429868	928.903059	13.825587
16.505332	924.616447	13.830605
16.866906	942.792104	13.835623
17.477877	932.542548	13.840640
17.429343	908.180875	13.845658
17.363545	901.390861	13.850675
17.383506	902.979397	13.855693
17.332434	904.719806	13.860711
17.525047	900.996817	13.865728
17.470268	883.870071	13.870746
17.301035	865.595720	13.875763
17.231264	871.821740	13.880781
17.139370	866.732426	13.885799
17.524623	864.614347	13.890816
16.916995	869.552903	13.895834
16.998029	867.000335	13.900851
16.848354	864.880709	13.905869
17.003164	872.963791	13.910887
17.091052	867.340520	13.915904
17.394705	873.118280	13.920922
17.158015	859.117174	13.925939
17.202820	864.080960	13.930957
17.037717	860.217128	13.935975
17.249603	852.409952	13.940992
17.414119	866.456179	13.946010
17.226844	865.024544	13.951027
17.172507	850.090902	13.956045
16.849922	844.770669	13.961063
17.166996	844.203956	13.966080
16.990183	865.395955	13.971098
17.043223	861.061303	13.976115
17.105966	853.790499	13.981133
17.234607	858.599310	13.986151
17.269984	864.493240	13.991168
17.130271	860.315420	13.996186
17.116884	862.509560	14.001203
17.191224	863.741329	14.006221
17.209495	866.300058	14.011239
17.200872	862.230672	14.016256
17.524933	868.884833	14.021274
17.284046	872.052241	14.026291
17.593702	876.048991	14.031309
17.441999	863.963438	14.036327
17.470551	856.668170	14.041344
17.335558	868.868935	14.046362
17.310180	871.424840	14.051379
17.493504	867.467410	14.056397
17.277073	892.088456	14.061415
17.655477	893.033207	14.066432
17.641601	899.784559	14.071450
17.601176	895.887518	14.076467
17.552466	904.542349	14.081485
17.200672	905.321596	14.086503
17.719855	897.737192	14.091520
17.738655	900.766235	14.096538
17.600082	900.584807	14.101555
17.860371	890.029707	14.106573
17.454991	899.820465	14.111591
17.497147	901.484454	14.116608
17.332894	901.419259	14.121626
17.523205	894.187778	14.126643
17.655906	896.661865	14.131661
17.090689	905.702002	14.136679
17.421866	906.978521	14.141696
17.460545	912.958130	14.146714
17.544696	926.033798	14.151731
17.738750	924.578701	14.156749
17.516242	925.337764	14.161767
17.911972	928.649940	14.166784
17.850005	935.133118	14.171802
17.538300	931.769205	14.176819
17.820555	924.499685	14.181837
17.623343	947.344112	14.186855
17.942852	929.098546	14.191872
17.903705	921.993343	14.196890
17.832013	924.132963	14.201907
18.030052	917.594963	14.206925
17.946091	942.775994	14.211943
17.679157	956.472804	14.216960
18.305540	966.756381	14.221978
18.014364	985.385571	14.226995
18.412442	965.111157	14.232013
18.372410	966.659425	14.237031
18.215287	955.152951	14.242048
18.116107	935.666738	14.247066
17.944074	934.669121	14.252083
18.292607	940.813446	14.257101
18.314458	963.702982	14.262119
18.313805	957.732557	14.267136
17.982361	947.708207	14.272154
18.544809	962.016071	14.277171
18.333058	950.607984	14.282189
18.277146	943.147527	14.287207
18.189681	953.287686	14.292224
18.398682	953.670176	14.297242
18.358990	952.159034	14.302259
18.742638	950.252002	14.307277
18.307919	943.123787	14.312295
18.078648	945.860225	14.317312
18.733149	945.021445	14.322330
18.572746	953.430236	14.327347
18.615359	936.277694	14.332365
18.211540	930.344775	14.337383
18.445817	946.486293	14.342400
18.339840	954.785714	14.347418
18.336304	954.454234	14.352435
18.833168	958.117557	14.357453
18.349832	942.295622	14.362471
18.464403	948.391619	14.367488
18.603827	952.127590	14.372506
18.515030	949.976636	14.377523
18.488370	954.156719	14.382541
18.288303	965.746563	14.387559
18.431988	959.844593	14.392576
18.728963	966.841802	14.397594
18.730932	964.847866	14.402611
18.776393	953.238241	14.407629
18.724266	954.350585	14.412647
18.783006	958.551196	14.417664
18.926484	946.604958	14.422682
18.786302	955.854959	14.427699
18.942094	945.600509	14.432717
18.776397	959.487055	14.437735
18.389926	956.839513	14.442752
18.724409	944.843408	14.447770
18.654912	954.787322	14.452787
19.094943	963.160271	14.457805
18.979501	977.214484	14.462823
19.172970	982.372406	14.467840
19.261520	956.032802	14.472858
19.154865	959.317393	14.477875
19.096532	951.708734	14.482893
18.877600	950.226622	14.487911
18.879868	949.368874	14.492928
19.209996	942.701966	14.497946
18.899216	952.559197	14.502963
19.050575	944.570669	14.507981
19.075920	947.858243	14.512999
18.985951	942.713280	14.518016
19.273152	944.487739	14.523034
19.072233	961.818728	14.528051
19.361655	957.683924	14.533069
19.499980	949.412554	14.538087
19.197121	952.035978	14.543104
19.266856	949.753331	14.548122
19.072136	952.921195	14.553139
18.968323	952.536810	14.558157
19.234259	971.585845	14.563175
19.086710	968.149921	14.568192
19.644012	978.496292	14.573210
19.570587	988.984689	14.578227
19.596331	983.400381	14.583245
19.535862	956.134175	14.588263
19.365045	957.426737	14.593280
19.323761	949.423985	14.598298
19.380810	968.269779	14.603315
19.438570	967.915179	14.608333
19.445621	970.939682	14.613351
19.329818	982.678581	14.618368
19.324604	972.171631	14.623386
19.332382	976.322017	14.628403
19.477113	971.062878	14.633421
19.714014	968.604398	14.638439
19.298296	968.930506	14.643456
19.258935	962.784024	14.648474
19.132455	972.894231	14.653491
19.719640	965.945305	14.658509
19.411026	974.743896	14.663527
19.406048	979.142021	14.668544
20.034484	980.282627	14.673562
19.692416	989.847462	14.678579
19.914197	978.818230	14.683597
19.941381	969.463618	14.688615
19.605837	969.142916	14.693632
19.941444	970.393910	14.698650
20.108098	963.398749	14.703667
19.896877	958.815267	14.708685
19.678292	962.210270	14.713703
19.548098	967.137074	14.718720
20.207796	969.878949	14.723738
19.817796	982.431935	14.728755
19.842504	979.053946	14.733773
20.253700	984.379400	14.738791
20.036821	990.593957	14.743808
20.267751	977.151981	14.748826
20.089812	970.791820	14.753843
19.997955	968.824017	14.758861
19.858523	962.944623	14.763879
19.999434	969.515333	14.768896
20.447360	956.711621	14.773914
20.152375	966.163362	14.778931
19.984622	954.862746	14.783949
19.854793	973.225730	14.788967
20.174577	986.685081	14.793984
20.424207	976.706987	14.799002
20.729861	985.822710	14.804019
20.048288	975.908554	14.809037
20.230427	969.617019	14.814055
19.976510	970.899499	14.819072
20.142263	985.619146	14.824090
20.237184	989.693137	14.829107
20.193874	994.299538	14.834125
20.140935	987.738032	14.839143
19.977811	994.226537	14.844160
20.424589	987.612368	14.849178
20.147701	990.312006	14.854195
19.995765	999.562991	14.859213
20.274945	990.599923	14.864231
20.255071	989.268348	14.869248
20.293985	989.485867	14.874266
20.544540	1007.359524	14.879283
20.591133	1012.159702	14.884301
21.029328	1003.291196	14.889319
21.105429	994.861804	14.894336
21.179500	986.328240	14.899354
21.023296	979.148865	14.904371
20.566826	984.616720	14.909389
20.778448	980.080069	14.914407
20.796213	988.493880	14.919424
20.780568	989.021155	14.924442
20.956231	983.640579	14.929459
20.840593	990.675871	14.934477
21.014628	978.222669	14.939495
20.799994	987.712516	14.944512
20.894590	978.924620	14.949530
20.755473	979.561654	14.954547
20.603090	983.764490	14.959565
20.781828	975.632467	14.964583
20.954276	980.527566	14.969600
21.118772	975.531062	14.974618
20.997055	984.463905	14.979635
20.808027	981.231062	14.984653
20.984935	983.503204	14.989671
20.547036	985.316994	14.994688
20.618913	973.747272	14.999706
20.802002	987.322506	15.004723
20.797133	982.651578	15.009741
20.756091	980.323266	15.014759
20.680886	975.065634	15.019776
20.940949	981.714478	15.024794
20.939317	991.536786	15.029811
21.034934	1011.408576	15.034829
21.425281	1013.033145	15.039847
21.216310	1008.854724	15.044864
21.266845	1017.856547	15.049882
21.419989	1015.116672	15.054899
21.338346	1006.257113	15.059917
21.251938	1008.116938	15.064935
20.995141	1015.032284	15.069952
21.157337	1017.972506	15.074970
21.370811	1013.491239	15.079987
21.028161	1011.532793	15.085005
21.515504	1008.646958	15.090023
21.435421	1013.323407	15.095040
21.431223	1004.456169	15.100058
21.700661	1005.806079	15.105075
21.212937	1005.522726	15.110093
21.511538	997.663555	15.115111
21.361277	1005.963236	15.120128
21.266361	1007.040338	15.125146
21.518631	1015.323103	15.130163
21.594722	1010.724207	15.135181
21.643689	1012.246160	15.140199
21.366042	1013.548311	15.145216
21.410672	1005.742323	15.150234
21.837939	1003.258678	15.155251
21.460921	1003.130233	15.160269
21.652458	1004.860675	15.165287
21.594630	998.393068	15.170304
21.583349	1001.848886	15.175322
21.835007	1003.426896	15.180339
21.494283	1016.673624	15.185357
21.625515	1008.021761	15.190375
21.777202	1013.212579	15.195392
21.941173	1027.774909	15.200410
21.916602	1024.336954	15.205427
21.753748	1020.556949	15.210445
21.883283	1031.647169	15.215463
22.009042	1040.828080	15.220480
22.021120	1032.738920	15.225498
22.063567	1005.027930	15.230515
21.817736	1014.087386	15.235533
22.187278	1009.398272	15.240551
21.923284	1016.088071	15.245568
21.990771	1018.485173	15.250586
22.186986	1019.168353	15.255603
21.979576	1028.204346	15.260621
22.440309	1026.847077	15.265639
22.319001	1020.531859	15.270656
22.000067	1010.618964	15.275674
22.251256	1012.274009	15.280691
21.976527	1004.701477	15.285709
22.207535	1009.587106	15.290727
22.509654	1029.468488	15.295744
21.943528	1014.741880	15.300762
22.336397	1023.995158	15.305779
21.958441	1029.739379	15.310797
22.039352	1027.377326	15.315815
22.460161	1036.589583	15.320832
22.519556	1028.352470	15.325850
22.820449	1029.742059	15.330867
22.405668	1036.268625	15.335885
22.587788	1031.281590	15.340903
22.416317	1027.200888	15.345920
22.445859	1021.269339	15.350938
22.457925	1031.004579	15.355955
22.325163	1032.822863	15.360973
22.630172	1027.656884	15.365991
22.764263	1045.519719	15.371008
22.708120	1025.687946	15.376026
22.747887	1022.705232	15.381043
22.475917	1024.625050	15.386061
22.730051	1019.275386	15.391079
22.543772	1022.684351	15.396096
22.479916	1032.346325	15.401114
22.724234	1032.011871	15.406131
22.374925	1036.639526	15.411149
22.670785	1024.031923	15.416167
22.688295	1032.196233	15.421184
22.446693	1033.893351	15.426202
22.703711	1026.717113	15.431219
22.539607	1030.233816	15.436237
22.768623	1031.143037	15.441255
22.649332	1034.491140	15.446272
22.891446	1055.621256	15.451290
23.164108	1051.771634	15.456307
22.909313	1065.505702	15.461325
23.087405	1054.858578	15.466343
23.081071	1052.407019	15.471360
22.997995	1053.985436	15.476378
22.883905	1046.909486	15.481395
22.995502	1050.520769	15.486413
22.962639	1051.379581	15.491431
23.428552	1055.216718	15.496448
22.940490	1048.442294	15.501466
23.282601	1052.567171	15.506483
23.354890	1057.865401	15.511501
23.409085	1048.286824	15.516519
23.593746	1052.169848	15.521536
23.161547	1047.245552	15.526554
23.288674	1030.507612	15.531571
23.388032	1021.183358	15.536589
23.121177	1019.802254	15.541607
23.361528	1032.793352	15.546624
23.357394	1038.138254	15.551642
23.403307	1037.611032	15.556659
23.433060	1053.300513	15.561677
23.746931	1051.245182	15.566695
23.440459	1033.574322	15.571712
23.089637	1032.544246	15.576730
23.565520	1036.537974	15.581747
23.491968	1045.943527	15.586765
23.305889	1046.188190	15.591783
23.079334	1043.845454	15.596800
23.238339	1057.347182	15.601818
23.641333	1048.403378	15.606835
23.472899	1052.438044	15.611853
23.152029	1055.629532	15.616871
23.612839	1040.805624	15.621888
23.806896	1050.803670	15.626906
23.411627	1037.939459	15.631923
23.400525	1045.574532	15.636941
23.448842	1056.666973	15.641959
23.970360	1060.837783	15.646976
23.790759	1065.893041	15.651994
24.211867	1065.119394	15.657011
24.180356	1075.377533	15.662029
23.798529	1065.674178	15.667047
23.926857	1075.735063	15.672064
23.545337	1070.019236	15.677082
24.198360	1058.416004	15.682099
24.125804	1067.902890	15.687117
24.014675	1068.739602	15.692135
24.072853	1062.983789	15.697152
23.905768	1072.604982	15.702170
24.162238	1068.170326	15.707187
24.031404	1073.106520	15.712205
24.180453	1071.168961	15.717223
24.295304	1064.764707	15.722240
23.803803	1073.054880	15.727258
24.080161	1066.786705	15.732275
23.814525	1069.599833	15.737293
23.637888	1076.841869	15.742311
23.760815	1068.692055	15.747328
23.998554	1083.098765	15.752346
24.327693	1085.576636	15.757363
24.374907	1094.843186	15.762381
24.552151	1091.206537	15.767399
24.789743	1084.531831	15.772416
24.631157	1099.718312	15.777434
24.859944	1072.996331	15.782451
24.534341	1061.095636	15.787469
24.565994	1061.506649	15.792487
24.299041	1062.497242	15.797504
24.459737	1060.084210	15.802522
24.300048	1059.452599	15.807539
24.402170	1072.016247	15.812557
24.777683	1079.593549	15.817575
24.933383	1083.478218	15.822592
24.968660	1088.891418	15.827610
24.751892	1078.712421	15.832627
25.123277	1062.336186	15.837645
24.659164	1064.104127	15.842663
24.773516	1058.774793	15.847680
24.600127	1060.775160	15.852698
24.660348	1052.241880	15.857715
24.489676	1058.711977	15.862733
24.740848	1079.159435	15.867751
25.170975	1085.393272	15.872768
24.609808	1075.856337	15.877786
24.772576	1078.254827	15.882803
24.816540	1094.352765	15.887821
24.658821	1101.230520	15.892839
24.546054	1092.782095	15.897856
24.670298	1099.492209	15.902874
24.581838	1097.780876	15.907891
24.915413	1093.857211	15.912909
24.793536	1097.623408	15.917927
25.349174	1097.165274	15.922944
24.731958	1106.409759	15.927962
25.014406	1115.719917	15.932979
25.348924	1115.457157	15.937997
25.571281	1120.421208	15.943015
26.014745	1108.357761	15.948032
25.535146	1088.750978	15.953050
25.705310	1080.260923	15.958067
25.528883	1072.554611	15.963085
25.369795	1076.097853	15.968103
25.343115	1077.764774	15.973120
25.023834	1080.133098	15.978138
25.227857	1088.389235	15.983155
25.472754	1078.915717	15.988173
25.585152	1080.363425	15.993191
25.597881	1082.416293	15.998208
25.488225	1075.932026	16.003226
25.438863	1075.078473	16.008243
25.656685	1074.512606	16.013261
25.755429	1082.020506	16.018279
25.680739	1070.891011	16.023296
25.726790	1078.739062	16.028314
25.373194	1083.493404	16.033331
25.723593	1078.567508	16.038349
25.361260	1085.748516	16.043367
25.980682	1078.003781	16.048384
25.808005	1078.606608	16.053402
25.667315	1075.261245	16.058419
25.587968	1068.326174	16.063437
25.578642	1078.039589	16.068455
25.770115	1086.234620	16.073472
25.844556	1108.941497	16.078490
26.015751	1110.020293	16.083507
26.223110	1107.499951	16.088525
26.217054	1104.309866	16.093543
25.984443	1095.555899	16.098560
25.627278	1082.821750	16.103578
25.525434	1096.936808	16.108595
26.191386	1105.820647	16.113613
25.595140	1109.681574	16.118631
26.018803	1104.408181	16.123648
25.848019	1109.773956	16.128666
26.001383	1112.111612	16.133683
26.203367	1110.422546	16.138701
25.774680	1103.028141	16.143719
25.939201	1101.498589	16.148736
25.790348	1124.831080	16.153754
26.071130	1131.898354	16.158771
26.429886	1126.394966	16.163789
26.298285	1138.533386	16.168807
26.449252	1134.646185	16.173824
26.661139	1131.309268	16.178842
26.323439	1126.283713	16.183859
26.612770	1124.534155	16.188877
26.565681	1133.273283	16.193895
26.781575	1124.818356	16.198912
26.626707	1132.778563	16.203930
26.359538	1131.548265	16.208947
26.663454	1129.322154	16.213965
26.521443	1145.147971	16.218983
27.049536	1133.967434	16.224000
26.914223	1126.925461	16.229018
26.570793	1131.217182	16.234035
26.575853	1109.913789	16.239053
26.601857	1129.694102	16.244071
26.684151	1127.148566	16.249088
26.567579	1140.681539	16.254106
26.501285	1134.955913	16.259123
26.913737	1130.454524	16.264141
26.696873	1128.684300	16.269159
26.331467	1121.756523	16.274176
26.427762	1126.297576	16.279194
26.839105	1127.928333	16.284211
27.171898	1135.054522	16.289229
27.017873	1136.012286	16.294247
27.079363	1125.876632	16.299264
26.910533	1128.598194	16.304282
26.848559	1134.132780	16.309299
26.889273	1142.756434	16.314317
27.179532	1160.906346	16.319335
26.950457	1161.418707	16.324352
27.554530	1147.049496	16.329370
27.098804	1155.496572	16.334387
27.284237	1149.631324	16.339405
27.250017	1152.227905	16.344423
27.448357	1147.794763	16.349440
27.682768	1156.122479	16.354458
27.609622	1148.692719	16.359475
27.393717	1135.292363	16.364493
27.147438	1117.354214	16.369511
27.480098	1134.858011	16.374528
27.675414	1140.413064	16.379546
27.404246	1140.469063	16.384563
27.370757	1136.551723	16.389581
27.445733	1145.730461	16.394599
27.542765	1145.021781	16.399616
27.643166	1147.477037	16.404634
27.498364	1143.363949	16.409651
27.654642	1140.971907	16.414669
27.282000	1144.368002	16.419687
27.647256	1145.237986	16.424704
27.583105	1137.536510	16.429722
27.654518	1140.666141	16.434739
28.075988	1142.539678	16.439757
27.642224	1145.055651	16.444775
27.879314	1139.466278	16.449792
27.929833	1139.910194	16.454810
27.622611	1152.301825	16.459827
27.786755	1145.621911	16.464845
27.716601	1150.513461	16.469863
27.434085	1152.181925	16.474880
27.519343	1145.781740	16.479898
27.447014	1161.282719	16.484915
28.066652	1169.441876	16.489933
27.976364	1165.090673	16.494951
28.126760	1173.200425	16.499968
28.105812	1169.679371	16.504986
28.007869	1181.060404	16.510003
28.260978	1174.095145	16.515021
28.247125	1170.953375	16.520039
28.447239	1167.966966	16.525056
28.294743	1166.290023	16.530074
28.067458	1173.946319	16.535091
28.471597	1166.464643	16.540109
28.324434	1166.564707	16.545127
28.379914	1168.714248	16.550144
28.499134	1167.777327	16.555162
28.239738	1167.484975	16.560179
28.388341	1162.095425	16.565197
28.662255	1169.399643	16.570215
28.618781	1158.986474	16.575232
28.628617	1170.194789	16.580250
28.536177	1165.923653	16.585267
28.480796	1165.283854	16.590285
28.732807	1163.800853	16.595303
28.483224	1170.580647	16.600320
28.693374	1165.426362	16.605338
28.537684	1161.592389	16.610355
28.734313	1167.384799	16.615373
28.695651	1165.900037	16.620391
28.597976	1168.606107	16.625408
28.770122	1160.616788	16.630426
28.794106	1161.516598	16.635443
28.751543	1174.528194	16.640461
28.801397	1187.110612	16.645479
29.279736	1183.909547	16.650496
29.245585	1172.727616	16.655514
28.981992	1169.251777	16.660531
29.097713	1156.127656	16.665549
29.400828	1158.620861	16.670567
29.088767	1159.577975	16.675584
29.650690	1150.891271	16.680602
29.497730	1160.091349	16.685619
29.435994	1159.540578	16.690637
29.058486	1147.408271	16.695655
29.224359	1152.739291	16.700672
29.088611	1152.078722	16.705690
29.026267	1153.085698	16.710707
29.723836	1151.929207	16.715725
29.464628	1157.389127	16.720743
29.114005	1150.948978	16.725760
29.265275	1145.017932	16.730778
29.349369	1158.825983	16.735795
29.178558	1150.553039	16.740813
29.412523	1151.610246	16.745831
29.294784	1162.775671	16.750848
29.530433	1173.365065	16.755866
29.180930	1187.486688	16.760883
29.638698	1183.975486	16.765901
29.743832	1189.118750	16.770919
29.629068	1184.009491	16.775936
30.060483	1185.132089	16.780954
29.427076	1196.305206	16.785971
29.860381	1176.118970	16.790989
29.827784	1187.703745	16.796007
29.773767	1190.085328	16.801024
30.155152	1186.876272	16.806042
29.885708	1191.627959	16.811059
30.355197	1191.348798	16.816077
29.834934	1181.817240	16.821095
30.064819	1178.564137	16.826112
30.189500	1162.678105	16.831130
29.885974	1172.641348	16.836147
30.112188	1174.950246	16.841165
30.327399	1177.395195	16.846183
30.208304	1159.132284	16.851200
30.098696	1148.118329	16.856218
29.497009	1155.750279	16.861235
29.850449	1163.400552	16.866253
30.066494	1176.664253	16.871271
29.908554	1184.505524	16.876288
30.492320	1183.112166	16.881306
30.346330	1186.837888	16.886323
29.791536	1190.832122	16.891341
29.983693	1190.682834	16.896359
29.750223	1201.348392	16.901376
30.209321	1188.509970	16.906394
30.202946	1195.342090	16.911411
30.090687	1191.525535	16.916429
30.345330	1204.500639	16.921447
30.280047	1201.056186	16.926464
30.442663	1201.148753	16.931482
30.155772	1202.761064	16.936499
30.572479	1202.321162	16.941517
30.578442	1206.359525	16.946535
30.391242	1211.151950	16.951552
30.669988	1211.775444	16.956570
30.606810	1223.267479	16.961587
30.965072	1233.790989	16.966605
31.226479	1227.616546	16.971623
30.969209	1213.920638	16.976640
31.056464	1207.359884	16.981658
31.060797	1214.185520	16.986675
31.061866	1193.204082	16.991693
30.803765	1189.988513	16.996711
30.452793	1191.386641	17.001728
30.776088	1199.876635	17.006746
31.056947	1216.381357	17.011763
31.285416	1227.358730	17.016781
31.569152	1230.282451	17.021799
31.039910	1224.812009	17.026816
31.256501	1225.166485	17.031834
30.799776	1227.480389	17.036851
30.808398	1215.088184	17.041869
31.140076	1221.371806	17.046887
31.240169	1226.205724	17.051904
31.468147	1215.986797	17.056922
31.449230	1226.240593	17.061939
31.062112	1224.845490	17.066957
31.730443	1228.253216	17.071975
31.415230	1234.932875	17.076992
31.738129	1225.264908	17.082010
31.701069	1225.483963	17.087027
31.166376	1223.182869	17.092045
31.140503	1220.127511	17.097063
31.476903	1223.073036	17.102080
31.720203	1212.535285	17.107098
31.322546	1232.832332	17.112115
31.832660	1228.562575	17.117133
31.575662	1218.268497	17.122151
31.333461	1232.618261	17.127168
32.023935	1241.591225	17.132186
32.037687	1244.958327	17.137203
31.923792	1242.981731	17.142221
32.269453	1237.305886	17.147239
32.000165	1236.091873	17.152256
32.135949	1225.007985	17.157274
31.856463	1222.392118	17.162291
31.536462	1224.241562	17.167309
32.142687	1226.988386	17.172327
31.951858	1243.636233	17.177344
32.351962	1241.965980	17.182362
32.441249	1250.770815	17.187379
32.535559	1247.194088	17.192397
32.428798	1226.141460	17.197415
31.977031	1217.439385	17.202432
32.264211	1210.376367	17.207450
31.942338	1217.288189	17.212467
32.117177	1218.578959	17.217485
32.619531	1213.668258	17.222503
32.502721	1235.188794	17.227520
32.650356	1240.493532	17.232538
32.606072	1222.720473	17.237555
32.666161	1215.981357	17.242573
32.425978	1193.245554	17.247591
32.573021	1193.404072	17.252608
32.544053	1191.221349	17.257626
32.821141	1184.824285	17.262643
32.610692	1189.539651	17.267661
32.956656	1187.221360	17.272679
32.643540	1196.126121	17.277696
33.085560	1187.870766	17.282714
33.177684	1188.243841	17.287731
32.790991	1185.881686	17.292749
32.993806	1181.991613	17.297767
33.191290	1184.906944	17.302784
33.062809	1178.953226	17.307802
32.839469	1182.531320	17.312819
32.582257	1182.734597	17.317837
32.985079	1195.074469	17.322855
33.040981	1193.088911	17.327872
32.705699	1185.653640	17.332890
33.068710	1183.264235	17.337907
32.718547	1185.972865	17.342925
33.291654	1189.933445	17.347943
33.170412	1219.758413	17.352960
33.331177	1225.202884	17.357978
33.338028	1227.896613	17.362995
33.202717	1219.890167	17.368013
33.520148	1217.239036	17.373031
33.012848	1218.581122	17.378048
32.949620	1222.832075	17.383066
33.026096	1224.019236	17.388083
32.892683	1228.400866	17.393101
33.065856	1232.217144	17.398119
33.170912	1230.486020	17.403136
33.141271	1244.268264	17.408154
33.601805	1244.214567	17.413171
33.316733	1253.875250	17.418189
34.021958	1243.689824	17.423207
33.747637	1241.829292	17.428224
33.382308	1249.708017	17.433242
33.716757	1254.345167	17.438259
33.495106	1244.868342	17.443277
33.622767	1235.281050	17.448295
33.489716	1247.700071	17.453312
33.552108	1248.601805	17.458330
34.003601	1264.792005	17.463347
33.734239	1270.363863	17.468365
34.072394	1271.931741	17.473383
34.505369	1265.938744	17.478400
33.901576	1267.513481	17.483418
34.007680	1276.597599	17.488435
34.150853	1275.309715	17.493453
34.637183	1272.745609	17.498471
34.081166	1258.218443	17.503488
34.146736	1265.436091	17.508506
34.611831	1272.149986	17.513523
34.519017	1270.030158	17.518541
34.309650	1252.434127	17.523559
34.371201	1249.204497	17.528576
34.180195	1250.852731	17.533594
34.383184	1254.015753	17.538611
34.275444	1273.875629	17.543629
34.568073	1271.918846	17.548647
34.144490	1281.242642	17.553664
34.540131	1271.078441	17.558682
34.370800	1265.961245	17.563699
34.589027	1267.978802	17.568717
34.895409	1263.628743	17.573735
34.448343	1275.461184	17.578752
34.301694	1272.864295	17.583770
34.623576	1285.416407	17.588787
34.713528	1285.266097	17.593805
34.862788	1265.850795	17.598823
34.609410	1265.964279	17.603840
34.317061	1276.153466	17.608858
34.975385	1281.387604	17.613875
35.138749	1295.935331	17.618893
35.261091	1289.321112	17.623911
35.128246	1285.207780	17.628928
34.751505	1272.848112	17.633946
35.471529	1283.179020	17.638963
34.820445	1287.714708	17.643981
35.131265	1292.541182	17.648999
35.484388	1302.599906	17.654016
35.462045	1295.147902	17.659034
35.504919	1285.555498	17.664051
34.912495	1277.530873	17.669069
35.199590	1282.689368	17.674087
35.320923	1297.956739	17.679104
35.367178	1298.506074	17.684122
35.563553	1299.290212	17.689139
35.043082	1301.180469	17.694157
35.355877	1282.662600	17.699175
35.088361	1283.209463	17.704192
35.361721	1288.507613	17.709210
35.493877	1285.468445	17.714227
35.460816	1293.302715	17.719245
35.812734	1310.910799	17.724263
35.793972	1309.480995	17.729280
35.838515	1308.808537	17.734298
35.877901	1296.550730	17.739315
35.958245	1303.008775	17.744333
35.791607	1302.076964	17.749351
35.701019	1309.940038	17.754368
35.534439	1318.778337	17.759386
36.046732	1313.135354	17.764403
35.962140	1321.771353	17.769421
36.061182	1313.572215	17.774439
36.336669	1313.425098	17.779456
36.097142	1316.400469	17.784474
36.199128	1312.009970	17.789491
35.844950	1322.381429	17.794509
36.073550	1322.360155	17.799527
36.249470	1316.295656	17.804544
35.959860	1322.329675	17.809562
36.492720	1315.738342	17.814579
36.196698	1320.675342	17.819597
35.944888	1306.325191	17.824615
35.956354	1321.424349	17.829632
36.224247	1336.917899	17.834650
36.675669	1346.231372	17.839667
36.658152	1349.911694	17.844685
36.999968	1342.443578	17.849703
36.983818	1338.327481	17.854720
36.788523	1346.151978	17.859738
37.078001	1336.573705	17.864755
36.448270	1322.102946	17.869773
36.558418	1343.824285	17.874791
36.606619	1351.601067	17.879808
36.663083	1342.724790	17.884826
36.915014	1342.653604	17.889843
36.839151	1343.150099	17.894861
36.826932	1336.577582	17.899879
37.010169	1338.825703	17.904896
36.892830	1349.695765	17.909914
37.107512	1350.092877	17.914931
37.081933	1352.314688	17.919949
37.084570	1344.537709	17.924967
37.341169	1329.444359	17.929984
36.994491	1339.897650	17.935002
37.255120	1339.051312	17.940019
37.125477	1343.121764	17.945037
37.217309	1334.400845	17.950055
37.580193	1333.173683	17.955072
37.622586	1341.801306	17.960090
37.350651	1344.265964	17.965107
37.212714	1341.505245	17.970125
37.188412	1336.702597	17.975143
37.541300	1330.904084	17.980160
36.974222	1330.259871	17.985178
37.476621	1341.203672	17.990195
37.815487	1363.330884	17.995213
37.755260	1360.488431	18.000231
37.712425	1367.549458	18.005248
37.501803	1372.200153	18.010266
37.986200	1358.905304	18.015283
37.872197	1356.132754	18.020301
37.317788	1357.914861	18.025319
37.810044	1355.927047	18.030336
37.401886	1363.491296	18.035354
37.900927	1356.311913	18.040371
37.639434	1362.989639	18.045389
37.512307	1361.339186	18.050407
38.532715	1380.537049	18.055424
38.073815	1385.161659	18.060442
38.455684	1384.428731	18.065459
38.505964	1380.788982	18.070477
38.724542	1380.374535	18.075495
38.867093	1350.141791	18.080512
38.363073	1349.985908	18.085530
38.764071	1333.628505	18.090547
38.899261	1346.030833	18.095565
38.375329	1345.197230	18.100583
38.640693	1342.267910	18.105600
38.602718	1351.185553	18.110618
38.616484	1340.539997	18.115635
38.655109	1342.475250	18.120653
38.518077	1348.516147	18.125671
38.701378	1349.716959	18.130688
38.413516	1347.373678	18.135706
38.898482	1348.485472	18.140723
38.792676	1344.740440	18.145741
38.535763	1347.974954	18.150759
38.667635	1354.591609	18.155776
38.748577	1351.241840	18.160794
38.867801	1342.995656	18.165811
38.741392	1327.536917	18.170829
38.848741	1343.642555	18.175847
38.930795	1353.554007	18.180864
38.803014	1375.790433	18.185882
38.984788	1385.664957	18.190899
39.100669	1378.351271	18.195917
39.018149	1379.392496	18.200935
39.429292	1373.742587	18.205952
38.984263	1371.020406	18.210970
39.125830	1377.259732	18.215987
39.083839	1382.403952	18.221005
39.058351	1378.762946	18.226023
39.132847	1372.141247	18.231040
38.999440	1388.590809	18.236058
39.574517	1399.459068	18.241075
39.588702	1388.178650	18.246093
39.638716	1399.569444	18.251111
39.790932	1398.578835	18.256128
39.544703	1411.699671	18.261146
39.632008	1411.748788	18.266163
39.695791	1405.139473	18.271181
39.468632	1400.816528	18.276199
39.956713	1394.986203	18.281216
39.767542	1399.251522	18.286234
39.498664	1394.217654	18.291251
39.762284	1406.652344	18.296269
39.659952	1403.366506	18.301287
40.089919	1389.232705	18.306304
39.609360	1399.954584	18.311322
39.668295	1411.185470	18.316339
40.080813	1421.262603	18.321357
40.353819	1432.517963	18.326375
40.837418	1424.578995	18.331392
40.784346	1407.078399	18.336410
40.352954	1396.727401	18.341427
40.291880	1383.719297	18.346445
40.281549	1386.370229	18.351463
40.642827	1379.317722	18.356480
40.641588	1379.958362	18.361498
40.498727	1385.926231	18.366515
40.564765	1371.767951	18.371533
40.446053	1378.353004	18.376551
40.313395	1374.903505	18.381568
40.620483	1396.849231	18.386586
40.746596	1402.336298	18.391603
40.944284	1410.045500	18.396621
41.193688	1416.358349	18.401639
40.931153	1387.398614	18.406656
40.853332	1387.362630	18.411674
40.775873	1377.237175	18.416691
40.842901	1380.341009	18.421709
40.327590	1395.056682	18.426727
40.689861	1406.854680	18.431744
40.984142	1410.362050	18.436762
41.129931	1404.801250	18.441779
41.219360	1402.585548	18.446797
41.016115	1411.953710	18.451815
41.536762	1398.766994	18.456832
41.561177	1399.335885	18.461850
41.276843	1403.405148	18.466867
41.155470	1408.615046	18.471885
40.996325	1404.907944	18.476903
41.526881	1400.558789	18.481920
41.107118	1411.384001	18.486938
41.103721	1402.254820	18.491955
41.393487	1421.509702	18.496973
41.562835	1433.362433	18.501991
41.537168	1441.121550	18.507008
41.677335	1437.083322	18.512026
41.706197	1433.139266	18.517043
41.894698	1439.506080	18.522061
41.618227	1437.384889	18.527079
41.872234	1431.318267	18.532096
41.742977	1430.346220	18.537114
41.792582	1434.090460	18.542131
42.149311	1436.162504	18.547149
42.025977	1435.119015	18.552167
42.137840	1428.807611	18.557184
42.199326	1432.360345	18.562202
41.974352	1424.083409	18.567219
42.067048	1429.003248	18.572237
41.997335	1428.765754	18.577255
41.974273	1433.214235	18.582272
42.147856	1429.110259	18.587290
41.810719	1431.769934	18.592307
42.465826	1446.058023	18.597325
42.086946	1467.125010	18.602343
42.313746	1465.391653	18.607360
42.516132	1463.758971	18.612378
42.295537	1458.069548	18.617395
43.023922	1454.194118	18.622413
42.500657	1458.373736	18.627431
42.868505	1457.275649	18.632448
42.928297	1465.302510	18.637466
42.675763	1464.117791	18.642483
42.724569	1460.487715	18.647501
42.787395	1454.058436	18.652519
42.702904	1455.858360	18.657536
42.932322	1454.929193	18.662554
42.907539	1460.077286	18.667571
42.978454	1460.155880	18.672589
42.699808	1451.468364	18.677607
42.895193	1465.533068	18.682624
42.993774	1458.676082	18.687642
42.949191	1463.612516	18.692659
43.387708	1462.613760	18.697677
42.995673	1468.625592	18.702695
43.115227	1480.556067	18.707712
43.101260	1476.312816	18.712730
42.993826	1484.252376	18.717747
43.620683	1470.431787	18.722765
43.188825	1471.906092	18.727783
43.408876	1475.947726	18.732800
43.770045	1472.252054	18.737818
43.501545	1478.084048	18.742835
43.975306	1487.609638	18.747853
43.875972	1482.321571	18.752871
43.674178	1465.316686	18.757888
43.707613	1465.894127	18.762906
43.802101	1464.284196	18.767923
43.989311	1465.296994	18.772941
43.965186	1469.128614	18.777959
43.870894	1461.607523	18.782976
44.082169	1463.365068	18.787994
43.768793	1474.859664	18.793011
44.067466	1471.402637	18.798029
44.045269	1475.812804	18.803047
44.095937	1470.632417	18.808064
44.115242	1477.672400	18.813082
43.850617	1488.762937	18.818099
44.429581	1501.082216	18.823117
44.594566	1504.921763	18.828135
44.232788	1502.612125	18.833152
44.510480	1507.095761	18.838170
43.983646	1513.812675	18.843187
44.387195	1495.517911	18.848205
44.747585	1497.774769	18.853223
44.464001	1494.975499	18.858240
44.829153	1500.194389	18.863258
44.552678	1503.161138	18.868275
44.968184	1491.239005	18.873293
44.588495	1499.210768	18.878311
44.555454	1502.559875	18.883328
44.879857	1503.689750	18.888346
44.692277	1506.171397	18.893363
44.961159	1494.110518	18.898381
44.684852	1492.050308	18.903399
44.635823	1513.262432	18.908416
44.962509	1517.613186	18.913434
44.800161	1519.072680	18.918451
44.760553	1534.914255	18.923469
44.827305	1520.948610	18.928487
44.974412	1524.526778	18.933504
45.093470	1521.945775	18.938522
45.176334	1548.761837	18.943539
45.495882	1543.574783	18.948557
45.661506	1549.309281	18.953575
45.759823	1552.076917	18.958592
45.758214	1544.055096	18.963610
45.553582	1538.661393	18.968627
45.674995	1517.247471	18.973645
45.601424	1512.676307	18.978663
45.375900	1529.077273	18.983680
45.699878	1526.402177	18.988698
45.489576	1548.679455	18.993715
45.940925	1545.104280	18.998733
45.641749	1547.798839	19.003751
46.024931	1545.103327	19.008768
45.994540	1537.757838	19.013786
46.066365	1540.594212	19.018803
46.183223	1550.887788	19.023821
46.136321	1549.477373	19.028839
45.660528	1549.453420	19.033856
45.952152	1528.696311	19.038874
45.937802	1535.845413	19.043891
46.203142	1545.373202	19.048909
46.529418	1551.939709	19.053927
46.312684	1563.289676	19.058944
46.559682	1569.125877	19.063962
46.391443	1579.188862	19.068979
46.900553	1569.834159	19.073997
46.776048	1560.065921	19.079015
46.510072	1562.383387	19.084032
46.418984	1560.818678	19.089050
46.457132	1569.839011	19.094067
46.775486	1556.924932	19.099085
47.143579	1569.463342	19.104103
46.808355	1574.297660	19.109120
47.139052	1557.947897	19.114138
47.127019	1553.635417	19.119155
47.183259	1554.962544	19.124173
47.104207	1558.058078	19.129191
46.951260	1550.358076	19.134208
47.199318	1539.323708	19.139226
46.931920	1549.203281	19.144243
47.133863	1543.161949	19.149261
47.268961	1543.312997	19.154279
46.829774	1536.794023	19.159296
47.232813	1548.222446	19.164314
47.111275	1550.814037	19.169331
47.470428	1562.589051	19.174349
47.643891	1578.710778	19.179367
47.803767	1584.888508	19.184384
47.784599	1569.761566	19.189402
47.667243	1573.966843	19.194419
47.821862	1576.341958	19.199437
48.179304	1558.590304	19.204455
47.652399	1553.630120	19.209472
47.725942	1539.870593	19.214490
47.781102	1562.870269	19.219507
47.778709	1573.846086	19.224525
48.029445	1583.561722	19.229543
47.906465	1588.019083	19.234560
47.994794	1580.798032	19.239578
47.426744	1588.249261	19.244595
47.605411	1593.624379	19.249613
47.800495	1588.436030	19.254631
47.811776	1594.277142	19.259648
48.293768	1601.527697	19.264666
48.077279	1604.871712	19.269683
48.261155	1619.210868	19.274701
48.562076	1603.773548	19.279719
48.291150	1603.410855	19.284736
48.348265	1594.189287	19.289754
48.306699	1605.366064	19.294771
48.712210	1607.648156	19.299789
48.801811	1597.227460	19.304807
48.543317	1602.197515	19.309824
48.863576	1591.809566	19.314842
48.595072	1584.913982	19.319859
48.929232	1604.984102	19.324877
49.319015	1606.929463	19.329895
48.850767	1613.904227	19.334912
49.063005	1596.402285	19.339930
48.896789	1599.899784	19.344947
48.844422	1612.175071	19.349965
48.942187	1621.823698	19.354983
48.564680	1628.067219	19.360000
49.029852	1624.232095	19.365018
48.983541	1620.971004	19.370035
49.154965	1616.970079	19.375053
49.187752	1627.753135	19.380071
49.663938	1645.397558	19.385088
50.179826	1640.416583	19.390106
49.919112	1635.707232	19.395123
49.636092	1621.226133	19.400141
49.746086	1615.846939	19.405159
49.874224	1618.277021	19.410176
49.730872	1607.483642	19.415194
49.984212	1613.894729	19.420211
49.629537	1614.798287	19.425229
50.010533	1614.794345	19.430247
49.960935	1622.874204	19.435264
50.348564	1625.859172	19.440282
50.079139	1621.309121	19.445299
49.853292	1622.290198	19.450317
50.125791	1623.524122	19.455335
50.028637	1634.327473	19.460352
50.336658	1643.440837	19.465370
50.314967	1635.633876	19.470387
50.690419	1632.263131	19.475405
50.584883	1632.549800	19.480423
50.416497	1646.647621	19.485440
50.461195	1633.660603	19.490458
50.485577	1627.920989	19.495475
50.480782	1636.174729	19.500493
50.771880	1629.267745	19.505511
50.704145	1625.072507	19.510528
50.680856	1629.228597	19.515546
50.730612	1625.750276	19.520563
50.262552	1634.024670	19.525581
50.696181	1629.012611	19.530599
50.579167	1643.509767	19.535616
50.988489	1658.790727	19.540634
51.042996	1669.741857	19.545651
51.186158	1660.858942	19.550669
51.451573	1660.110014	19.555687
51.426916	1664.746206	19.560704
51.109029	1663.971635	19.565722
51.198631	1658.004131	19.570739
51.226183	1659.229131	19.575757
51.456131	1650.836547	19.580775
51.452664	1658.351582	19.585792
51.164699	1659.628524	19.590810
51.493148	1659.101240	19.595827
51.371723	1658.653021	19.600845
51.701173	1650.567974	19.605863
51.652548	1660.352811	19.610880
51.824834	1651.868980	19.615898
51.876186	1651.061736	19.620915
51.676651	1653.199161	19.625933
51.963273	1661.344726	19.630951
51.895528	1675.292690	19.635968
51.943400	1678.170052	19.640986
52.304352	1675.785244	19.646003
52.361838	1679.678421	19.651021
52.278641	1666.152927	19.656039
52.252379	1669.086627	19.661056
52.330152	1672.774505	19.666074
52.541138	1665.444966	19.671091
52.432380	1675.700917	19.676109
52.214593	1671.460589	19.681127
52.373370	1677.085451	19.686144
52.382281	1673.477467	19.691162
52.323458	1669.455331	19.696179
52.121069	1671.143674	19.701197
52.484699	1664.067030	19.706215
52.473946	1668.945780	19.711232
52.441191	1684.262420	19.716250
52.602605	1687.481414	19.721267
52.639066	1701.604877	19.726285
52.734926	1700.150189	19.731303
52.819559	1701.077407	19.736320
52.908524	1692.578191	19.741338
52.991283	1703.340838	19.746355
53.143047	1695.738426	19.751373
53.208838	1706.769007	19.756391
53.103836	1715.784148	19.761408
53.275433	1719.795078	19.766426
53.792883	1718.825582	19.771443
53.345820	1731.530518	19.776461
53.931176	1722.129860	19.781479
53.941461	1714.851571	19.786496
53.675850	1699.107425	19.791514
53.601229	1690.714958	19.796531
53.656648	1688.517826	19.801549
53.666020	1702.658954	19.806567
53.843395	1707.139150	19.811584
54.068217	1711.608357	19.816602
54.213989	1720.084084	19.821619
54.105740	1726.067032	19.826637
54.153299	1717.969089	19.831655
54.135412	1715.210902	19.836672
54.107689	1718.450528	19.841690
54.118707	1711.969866	19.846707
53.789965	1706.324793	19.851725
54.114382	1712.233089	19.856743
54.344403	1716.456977	19.861760
53.811743	1723.685320	19.866778
54.345682	1721.587830	19.871795
54.050969	1717.177937	19.876813
54.356265	1727.568628	19.881831
54.390899	1733.329761	19.886848
54.361754	1743.494461	19.891866
54.500743	1740.302319	19.896883
54.621553	1754.159557	19.901901
55.064268	1750.029131	19.906919
54.830200	1748.506138	19.911936
54.890489	1745.610631	19.916954
54.891071	1744.446458	19.921971
54.665106	1754.501578	19.926989
55.299293	1759.855608	19.932007
55.501821	1768.527670	19.937024
55.122127	1751.981543	19.942042
55.195391	1741.194396	19.947059
55.469224	1766.183610	19.952077
55.443498	1763.533982	19.957095
55.542668	1751.025409	19.962112
55.455333	1765.073925	19.967130
55.528766	1757.848363	19.972147
54.833972	1769.970319	19.977165
55.262015	1769.941873	19.982183
55.767262	1766.798837	19.987200
55.478431	1768.102699	19.992218
55.848312	1755.063023	19.997235
55.657143	1771.550883	20.002253
55.753321	1774.706076	20.007271
55.646362	1782.231778	20.012288
55.909024	1791.071062	20.017306
56.094457	1793.523984	20.022323
56.058456	1805.806957	20.027341
56.176780	1799.897638	20.032359
56.378323	1790.663502	20.037376
55.832221	1802.981951	20.042394
56.172583	1805.090803	20.047411
56.035019	1806.828089	20.052429
56.255411	1803.384319	20.057447
56.191500	1803.887711	20.062464
56.231351	1822.735033	20.067482
56.771366	1812.716484	20.072499
56.926924	1810.820667	20.077517
56.833995	1814.580287	20.082535
57.042489	1817.715158	20.087552
56.855411	1818.461125	20.092570
57.322481	1813.057892	20.097587
57.431261	1817.793721	20.102605
57.178551	1807.301116	20.107623
57.460404	1805.831431	20.112640
57.691403	1806.037494	20.117658
57.385010	1784.966503	20.122675
57.607757	1783.045021	20.127693
57.284711	1776.074909	20.132711
57.211742	1775.990293	20.137728
57.348577	1763.661686	20.142746
57.414473	1780.259618	20.147763
57.260160	1797.195500	20.152781
57.370994	1805.497933	20.157799
57.695766	1802.927570	20.162816
57.287767	1809.541518	20.167834
57.620607	1800.154000	20.172851
57.535239	1806.133198	20.177869
57.527645	1812.903399	20.182887
57.725811	1829.461222	20.187904
57.930363	1836.026118	20.192922
58.116889	1832.692062	20.197939
58.150531	1828.826634	20.202957
58.179433	1843.909251	20.207975
58.303242	1841.141799	20.212992
58.024028	1833.909915	20.218010
58.084088	1836.452059	20.223027
57.979754	1833.002304	20.228045
58.369475	1838.571938	20.233063
58.348570	1837.203653	20.238080
58.040388	1859.234391	20.243098
58.467736	1852.320343	20.248115
58.803801	1859.041255	20.253133
58.699658	1851.165141	20.258151
58.968484	1845.584245	20.263168
58.762617	1850.941312	20.268186
58.699529	1850.195090	20.273203
58.867948	1842.810894	20.278221
58.632992	1854.393392	20.283239
59.229688	1869.823306	20.288256
59.183685	1883.584026	20.293274
59.435833	1865.108352	20.298291
59.438504	1872.228029	20.303309
59.414947	1874.242712	20.308327
59.667905	1874.895693	20.313344
59.550345	1877.806728	20.318362
59.717564	1869.060059	20.323379
59.509534	1861.790221	20.328397
59.677209	1863.803614	20.333415
59.760075	1852.464464	20.338432
59.709976	1858.754948	20.343450
59.930060	1852.921697	20.348467
59.870944	1861.741958	20.353485
59.892747	1864.682908	20.358503
59.978210	1864.675447	20.363520
59.884772	1865.387243	20.368538
59.865442	1862.906209	20.373555
60.174785	1865.908491	20.378573
59.851674	1862.846224	20.383591
59.883536	1855.316691	20.388608
60.071280	1881.944367	20.393626
60.378097	1881.779867	20.398643
60.427444	1892.285202	20.403661
60.539975	1893.247974	20.408679
60.720403	1883.891891	20.413696
60.751598	1902.498442	20.418714
60.950601	1893.941763	20.423731
60.847597	1893.879627	20.428749
60.644625	1894.209564	20.433767
60.872006	1882.729397	20.438784
60.737409	1886.009354	20.443802
60.840612	1875.344318	20.448819
60.958017	1878.465713	20.453837
60.915588	1877.905231	20.458855
61.301640	1872.187249	20.463872
61.335997	1890.138604	20.468890
61.328839	1899.748647	20.473907
61.600556	1899.334264	20.478925
61.343011	1913.014427	20.483943
61.958191	1913.811865	20.488960
61.562092	1905.559600	20.493978
61.796518	1897.400766	20.498995
62.078585	1893.393099	20.504013
61.652610	1887.470354	20.509031
61.730361	1887.062829	20.514048
61.842824	1899.263081	20.519066
61.645369	1910.951619	20.524083
62.154835	1899.855295	20.529101
61.560610	1911.269668	20.534119
61.789895	1900.087175	20.539136
61.974203	1910.297807	20.544154
61.700362	1905.730685	20.549171
62.240528	1918.728104	20.554189
61.988648	1930.183547	20.559207
62.323058	1938.151104	20.564224
62.164048	1940.569639	20.569242
62.331890	1941.696289	20.574259
62.388644	1926.985740	20.579277
62.457676	1936.291511	20.584295
63.019074	1943.522023	20.589312
62.888067	1954.081413	20.594330
62.967957	1955.205277	20.599347
63.067185	1955.336079	20.604365
62.889603	1952.496572	20.609383
63.006435	1950.445342	20.614400
63.134430	1962.331690	20.619418
63.164829	1966.242801	20.624435
63.536439	1961.424727	20.629453
63.225511	1958.339759	20.634471
63.404901	1949.605205	20.639488
63.356478	1955.580914	20.644506
63.339723	1959.375024	20.649523
63.610782	1959.963606	20.654541
63.348786	1971.794732	20.659559
63.851239	1960.519029	20.664576
63.571743	1961.334599	20.669594
63.561834	1956.664011	20.674611
63.736831	1945.362910	20.679629
63.627744	1954.832759	20.684647
63.775033	1964.204742	20.689664
63.711347	1980.901461	20.694682
63.960004	1981.719316	20.699699
63.982616	1985.024098	20.704717
64.002885	1986.156242	20.709735
64.228501	1984.671623	20.714752
64.260654	1992.286633	20.719770
63.205132	2004.487865	20.724787
63.699325	2003.500546	20.729805
63.917015	2014.979038	20.734823
64.394035	2025.065005	20.739840
64.815405	2028.187181	20.744858
64.754947	2034.269034	20.749875
64.966404	2040.244741	20.754893
65.404388	2046.185774	20.759911
65.048515	2034.542449	20.764928
65.497644	2037.274248	20.769946
65.532468	2037.025965	20.774963
65.612820	2008.827025	20.779981
65.246839	2003.272239	20.784999
65.290721	2003.932022	20.790016
65.221879	2012.218789	20.795034
65.052532	2007.712118	20.800051
65.171882	2016.479947	20.805069
65.045791	2037.080583	20.810087
65.375973	2041.286632	20.815104
65.693159	2037.511687	20.820122
65.468728	2036.313026	20.825139
65.447883	2033.582434	20.830157
65.416397	2065.420992	20.835175
65.488342	2071.904762	20.840192
65.735309	2064.154756	20.845210
65.860736	2064.350318	20.850227
65.985940	2061.386550	20.855245
66.009564	2060.297082	20.860263
66.446795	2063.567025	20.865280
66.629143	2072.938989	20.870298
66.333637	2073.513137	20.875315
66.913452	2066.854681	20.880333
66.663570	2064.140673	20.885351
66.519466	2064.960447	20.890368
66.354853	2058.049254	20.895386
66.828671	2086.993583	20.900403
67.214832	2081.131031	20.905421
66.957709	2078.256420	20.910439
67.106564	2073.808949	20.915456
67.434855	2065.936064	20.920474
67.109098	2066.859866	20.925491
67.208961	2067.304119	20.930509
67.307404	2076.899184	20.935527
67.372399	2067.515809	20.940544
67.581671	2065.675450	20.945562
67.416460	2059.988066	20.950579
67.747647	2060.449994	20.955597
67.200123	2058.326265	20.960615
67.311118	2060.034315	20.965632
67.317542	2050.337035	20.970650
67.047868	2068.386865	20.975667
67.434030	2059.979663	20.980685
67.286865	2075.931686	20.985703
67.360674	2084.682278	20.990720
67.597257	2096.486421	20.995738
67.550670	2089.819467	21.000755
67.675100	2085.802764	21.005773
67.900623	2096.871595	21.010791
68.106789	2122.321153	21.015808
68.563133	2107.137546	21.020826
68.667019	2120.253879	21.025843
68.702965	2113.853961	21.030861
68.581862	2125.304866	21.035879
68.633656	2124.472921	21.040896
68.535873	2121.900880	21.045914
68.530594	2120.393582	21.050931
69.116261	2116.011111	21.055949
68.876559	2116.634105	21.060967
69.085372	2112.311546	21.065984
68.905400	2113.401795	21.071002
68.755851	2120.559140	21.076019
69.056397	2111.471038	21.081037
68.733124	2107.354506	21.086055
68.821517	2121.363286	21.091072
69.146735	2130.237897	21.096090
69.134896	2140.895823	21.101107
69.658141	2135.993391	21.106125
69.795032	2142.362333	21.111143
69.409454	2138.496029	21.116160
70.010070	2144.547813	21.121178
69.468256	2143.622045	21.126195
69.744155	2137.846387	21.131213
69.697376	2139.101817	21.136231
69.785735	2139.167691	21.141248
70.111636	2156.552916	21.146266
70.075834	2158.989310	21.151283
70.432347	2163.708914	21.156301
70.491832	2166.809823	21.161319
70.361737	2171.207903	21.166336
70.556162	2159.107240	21.171354
70.157298	2163.282626	21.176371
70.626219	2157.678001	21.181389
70.493358	2155.452078	21.186407
70.272679	2156.829348	21.191424
70.462699	2161.899468	21.196442
70.583549	2169.035577	21.201459
70.700910	2173.189043	21.206477
70.633264	2193.020054	21.211495
70.728094	2185.507905	21.216512
71.096008	2183.134272	21.221530
70.683720	2197.785850	21.226547
70.851485	2194.590435	21.231565
71.123708	2202.658359	21.236583
71.202694	2202.296879	21.241600
71.444386	2192.691922	21.246618
71.615021	2192.782386	21.251635
72.276692	2187.767307	21.256653
72.232709	2187.012203	21.261671
72.195926	2191.569265	21.266688
72.217479	2187.575834	21.271706
72.000259	2172.894379	21.276723
71.894825	2172.050030	21.281741
71.935257	2175.394227	21.286759
71.921901	2191.531524	21.291776
72.301759	2180.606996	21.296794
72.372534	2187.278395	21.301811
72.714576	2187.212789	21.306829
72.539890	2184.740644	21.311847
72.292214	2180.262612	21.316864
72.400478	2180.387593	21.321882
72.554233	2191.106569	21.326899
72.674828	2185.273493	21.331917
72.860389	2188.196303	21.336935
72.634082	2196.189136	21.341952
72.771922	2178.539196	21.346970
72.778291	2187.372836	21.351987
72.726682	2184.176275	21.357005
72.797080	2178.378266	21.362023
73.030453	2178.201888	21.367040
73.055375	2184.688358	21.372058
72.909620	2206.131377	21.377075
73.152963	2201.027362	21.382093
73.214569	2213.640173	21.387111
73.206853	2218.687085	21.392128
73.373336	2215.211388	21.397146
73.305136	2228.564502	21.402163
73.682788	2232.436998	21.407181
74.072031	2230.200767	21.412199
73.821218	2236.514927	21.417216
74.351786	2231.990359	21.422234
74.151304	2240.609411	21.427251
74.059580	2233.940208	21.432269
74.384622	2231.965945	21.437287
73.970550	2247.717780	21.442304
74.510225	2234.485090	21.447322
74.172506	2229.656793	21.452339
74.184365	2232.399079	21.457357
74.527948	2230.005249	21.462375
74.524192	2230.641419	21.467392
74.514446	2248.307392	21.472410
74.837605	2256.819256	21.477427
75.211991	2254.514025	21.482445
75.315079	2250.715948	21.487463
75.176970	2262.797669	21.492480
75.257546	2261.938325	21.497498
74.911157	2271.516079	21.502515
75.163621	2263.410367	21.507533
75.060886	2259.110709	21.512551
75.336961	2264.852418	21.517568
75.632492	2252.248200	21.522586
75.403123	2270.279992	21.527603
75.298911	2262.810735	21.532621
75.176131	2270.752053	21.537639
75.291630	2285.683402	21.542656
75.412153	2286.004769	21.547674
75.707394	2286.881473	21.552691
75.366759	2282.332165	21.557709
75.976991	2288.797348	21.562727
75.657699	2315.526093	21.567744
76.387834	2324.811038	21.572762
76.412948	2317.966204	21.577779
76.472467	2319.112161	21.582797
76.499471	2307.177227	21.587815
76.181405	2317.733329	21.592832
76.717952	2312.431232	21.597850
76.726839	2316.178282	21.602867
76.676909	2320.296837	21.607885
76.859201	2313.867143	21.612903
76.593453	2318.628797	21.617920
76.938406	2323.708799	21.622938
76.656833	2337.179936	21.627955
76.810907	2347.421049	21.632973
77.037797	2336.718132	21.637991
77.166371	2342.973382	21.643008
77.291774	2341.947779	21.648026
77.391135	2338.072939	21.653043
77.224760	2337.950804	21.658061
77.579827	2334.706892	21.663079
77.737902	2359.245562	21.668096
78.138780	2353.707816	21.673114
77.944883	2362.522094	21.678131
77.592123	2358.524925	21.683149
77.987992	2346.261704	21.688167
77.955654	2349.809290	21.693184
78.143177	2348.496471	21.698202
78.202737	2352.125716	21.703219
78.132999	2350.948315	21.708237
78.528781	2354.405473	21.713255
78.478742	2358.371115	21.718272
78.432483	2348.655780	21.723290
78.324134	2345.542573	21.728307
78.540008	2354.714103	21.733325
78.409562	2351.683478	21.738343
78.451978	2378.743479	21.743360
78.500950	2389.825554	21.748378
78.900314	2384.040820	21.753395
78.665375	2382.196865	21.758413
78.977953	2383.851760	21.763431
78.857337	2395.189800	21.768448
78.834169	2409.334000	21.773466
78.960998	2406.784437	21.778483
79.330237	2403.385030	21.783501
79.479757	2405.899888	21.788519
79.769576	2396.871459	21.793536
79.827521	2400.403744	21.798554
80.044982	2390.950689	21.803571
80.012156	2404.142214	21.808589
80.190608	2406.399946	21.813607
80.208026	2400.401764	21.818624
80.289628	2387.812316	21.823642
80.124656	2398.283730	21.828659
79.856751	2399.307629	21.833677
80.396418	2411.562292	21.838695
80.266786	2427.017520	21.843712
80.429508	2418.435840	21.848730
80.113686	2417.627423	21.853747
80.181936	2431.948061	21.858765
80.392024	2436.211857	21.863783
80.695038	2453.635057	21.868800
80.593749	2457.000372	21.873818
80.773330	2452.140261	21.878835
80.679209	2462.775197	21.883853
81.153379	2463.576679	21.888871
80.828341	2466.868740	21.893888
81.120027	2484.280855	21.898906
81.314526	2484.810461	21.903923
81.259761	2493.070948	21.908941
81.740028	2480.183673	21.913959
81.821392	2481.633887	21.918976
81.395217	2474.661797	21.923994
81.726279	2475.038924	21.929011
81.717109	2480.062935	21.934029
81.655245	2482.856028	21.939047
81.798360	2508.757167	21.944064
82.388931	2502.106001	21.949082
82.375154	2511.245499	21.954099
82.418831	2520.810522	21.959117
82.289772	2506.766505	21.964135
82.352311	2502.067050	21.969152
82.067690	2506.145700	21.974170
82.591368	2511.464720	21.979187
82.490778	2507.407537	21.984205
82.504820	2507.161893	21.989223
83.048024	2531.883639	21.994240
83.147505	2521.471318	21.999258
83.160233	2522.580536	22.004275
83.201313	2527.173449	22.009293
83.536158	2511.962676	22.014311
83.284483	2517.017323	22.019328
83.077370	2516.262587	22.024346
83.712259	2517.224117	22.029363
83.362893	2525.877377	22.034381
83.802208	2516.836380	22.039399
83.707613	2522.461100	22.044416
83.715753	2526.068963	22.049434
83.744309	2532.777997	22.054451
83.483690	2535.159480	22.059469
83.937692	2518.498385	22.064487
83.727281	2526.557851	22.069504
83.581873	2524.876829	22.074522
84.068261	2539.307005	22.079539
84.083672	2540.804341	22.084557
84.439771	2554.151005	22.089575
84.491101	2560.709053	22.094592
83.891398	2557.716560	22.099610
84.269660	2551.796874	22.104627
84.326259	2569.140456	22.109645
84.693618	2566.698751	22.114663
84.592858	2568.621958	22.119680
84.729109	2569.617466	22.124698
84.901024	2584.650012	22.129715
85.317019	2591.544250	22.134733
85.459851	2588.294807	22.139751
85.751880	2589.295283	22.144768
85.937908	2586.762679	22.149786
86.057806	2569.910294	22.154803
85.779834	2560.407121	22.159821
86.159336	2553.886869	22.164839
86.167310	2553.292246	22.169856
85.965793	2546.281819	22.174874
86.183571	2543.040867	22.179891
86.065840	2549.999659	22.184909
85.582262	2541.235945	22.189927
86.085133	2568.235939	22.194944
86.275427	2573.554955	22.199962
86.538497	2569.447505	22.204979
86.375146	2580.634089	22.209997
86.261599	2575.527512	22.215015
86.569657	2580.236552	22.220032
86.108467	2579.856061	22.225050
86.624735	2590.378412	22.230067
86.987166	2605.272810	22.235085
86.649572	2602.442103	22.240103
87.081050	2610.378224	22.245120
86.886583	2612.723591	22.250138
87.108717	2608.927997	22.255155
86.854557	2619.646963	22.260173
86.988119	2633.945382	22.265191
87.274270	2640.038305	22.270208
87.217375	2643.571513	22.275226
87.938913	2637.012029	22.280243
87.752142	2645.828242	22.285261
87.832604	2641.967866	22.290279
87.876662	2647.459096	22.295296
87.900850	2656.017238	22.300314
87.997699	2650.232988	22.305331
88.258798	2660.248760	22.310349
88.231458	2661.944896	22.315367
88.625039	2657.959550	22.320384
87.974769	2664.758373	22.325402
88.639958	2661.829273	22.330419
88.736672	2647.979305	22.335437
88.396430	2652.653375	22.340455
88.684610	2657.267303	22.345472
88.659553	2672.363584	22.350490
89.191648	2679.276863	22.355507
88.720218	2692.174592	22.360525
89.046994	2682.843841	22.365543
89.353814	2679.893250	22.370560
89.149394	2685.862934	22.375578
89.222559	2680.972307	22.380595
88.908469	2689.920995	22.385613
89.336891	2694.224767	22.390631
89.870168	2711.120467	22.395648
89.591500	2713.794709	22.400666
89.840761	2710.258376	22.405683
89.846857	2714.418563	22.410701
89.645717	2708.736679	22.415719
89.729735	2713.805601	22.420736
89.511703	2739.764048	22.425754
90.289954	2740.178700	22.430771
91.064556	2732.451011	22.435789
90.845801	2723.554067	22.440807
91.106168	2727.687595	22.445824
90.813938	2730.866420	22.450842
91.044389	2719.886285	22.455859
91.127528	2733.286477	22.460877
91.022369	2728.190667	22.465895
91.368094	2721.650337	22.470912
90.958000	2726.540293	22.475930
91.159859	2714.345650	22.480947
91.105529	2714.308536	22.485965
91.385384	2725.815671	22.490983
91.285087	2716.216904	22.496000
91.223717	2736.071392	22.501018
91.424674	2749.419847	22.506035
91.567807	2753.675505	22.511053
91.631242	2746.350351	22.516071
91.730194	2744.382481	22.521088
91.740872	2756.232924	22.526106
92.031571	2749.402869	22.531123
92.626856	2763.977066	22.536141
92.619945	2770.667656	22.541159
92.755622	2781.449476	22.546176
92.918372	2772.208372	22.551194
93.220629	2762.501720	22.556211
92.909954	2757.993379	22.561229
92.502057	2761.776338	22.566247
93.282642	2760.904047	22.571264
92.927367	2761.620175	22.576282
93.275976	2751.033467	22.581299
93.038984	2763.720476	22.586317
92.991409	2763.628311	22.591335
93.065295	2764.963651	22.596352
92.897750	2768.180934	22.601370
93.204090	2771.693911	22.606387
93.436549	2788.216194	22.611405
93.532513	2795.864952	22.616423
93.508158	2793.673760	22.621440
93.234771	2799.471820	22.626458
93.711607	2812.194057	22.631475
93.725573	2820.973263	22.636493
93.729122	2819.766393	22.641511
93.596711	2823.511325	22.646528
94.070773	2843.301489	22.651546
94.771774	2836.092980	22.656563
94.836641	2838.371907	22.661581
94.679708	2846.820325	22.666599
95.345123	2840.725919	22.671616
95.293083	2836.263398	22.676634
95.002694	2833.141787	22.681651
95.363630	2826.790625	22.686669
95.032841	2837.480673	22.691687
95.383357	2830.373779	22.696704
95.283366	2840.029667	22.701722
95.336102	2834.921903	22.706739
95.273426	2833.530708	22.711757
95.368521	2839.317105	22.716775
95.716356	2831.820117	22.721792
95.504316	2826.736818	22.726810
95.499718	2843.282190	22.731827
95.666051	2856.928575	22.736845
95.677546	2875.495657	22.741863
96.231253	2856.697328	22.746880
95.993540	2862.834386	22.751898
96.103648	2866.234540	22.756915
96.235394	2882.023593	22.761933
96.341456	2884.238241	22.766951
96.680564	2876.922983	22.771968
96.867903	2881.012323	22.776986
96.630652	2882.314050	22.782003
96.587080	2879.334710	22.787021
96.759731	2895.181581	22.792039
97.171952	2899.567613	22.797056
96.921361	2917.899717	22.802074
97.027373	2903.329898	22.807091
97.346601	2901.643708	22.812109
97.458888	2911.287003	22.817127
97.783429	2908.867676	22.822144
97.863217	2915.899502	22.827162
97.573958	2923.147033	22.832179
97.545742	2930.941177	22.837197
97.503083	2939.940430	22.842215
97.803066	2923.513006	22.847232
98.452559	2939.017358	22.852250
98.141518	2939.500994	22.857267
98.364464	2941.815624	22.862285
97.988324	2971.267012	22.867303
98.618212	2961.758847	22.872320
98.362439	2960.579463	22.877338
98.743150	2960.861001	22.882355
98.928559	2958.970547	22.887373
98.937382	2963.135468	22.892391
99.049033	2972.471042	22.897408
99.343208	2982.027634	22.902426
99.202069	2982.129270	22.907443
99.241290	2977.775246	22.912461
99.206552	2976.997907	22.917479
99.732543	2975.078337	22.922496
99.531064	2978.800074	22.927514
99.685699	2977.410751	22.932531
99.700749	2986.137510	22.937549
99.927844	3001.575112	22.942567
100.444560	3003.850658	22.947584
100.070367	3007.757236	22.952602
100.200856	3008.275786	22.957619
100.656474	3009.594132	22.962637
100.462000	3005.883031	22.967655
100.331918	3005.771821	22.972672
100.506709	3003.429585	22.977690
100.327167	3023.540575	22.982707
100.870422	3036.825237	22.987725
100.897865	3041.728029	22.992743
101.120672	3031.533957	22.997760
101.259150	3037.764429	23.002778
101.237640	3035.079832	23.007795
101.467342	3022.710272	23.012813
101.260423	3035.943306	23.017831
101.392554	3034.612814	23.022848
101.863309	3039.088818	23.027866
101.922685	3059.552492	23.032883
101.894691	3058.737028	23.037901
101.584692	3054.133215	23.042919
101.752040	3054.481113	23.047936
102.108768	3058.344483	23.052954
101.934358	3054.134397	23.057971
102.178083	3055.196035	23.062989
102.139471	3075.240105	23.068007
102.012373	3082.059742	23.073024
102.589709	3079.028551	23.078042
102.307314	3081.590875	23.083059
102.637498	3093.543108	23.088077
102.787573	3110.200212	23.093095
103.151215	3102.318602	23.098112
103.620566	3101.295760	23.103130
103.503479	3101.216259	23.108147
103.643385	3101.469483	23.113165
103.639736	3103.852682	23.118183
103.836156	3103.102099	23.123200
103.813353	3099.194108	23.128218
103.726628	3102.104803	23.133235
103.989708	3091.659554	23.138253
104.091481	3095.607582	23.143271
104.074793	3096.432338	23.148288
104.270917	3104.720984	23.153306
103.760109	3125.998240	23.158323
104.387828	3118.537543	23.163341
104.473582	3123.850796	23.168359
104.509398	3112.250590	23.173376
104.686055	3125.539608	23.178394
104.429518	3127.093749	23.183411
104.753265	3142.124977	23.188429
104.893791	3152.893263	23.193447
105.149058	3154.289609	23.198464
105.058494	3158.243057	23.203482
104.725075	3160.483516	23.208499
105.391984	3173.501804	23.213517
105.433735	3180.588067	23.218535
105.413666	3185.261751	23.223552
105.754212	3182.159828	23.228570
105.384858	3200.030793	23.233587
105.832684	3202.997665	23.238605
105.918970	3210.050992	23.243623
106.096301	3205.142200	23.248640
106.323272	3207.737698	23.253658
106.331429	3226.910863	23.258675
106.805691	3224.504149	23.263693
106.929791	3230.894947	23.268711
107.099672	3226.457846	23.273728
107.247261	3226.209809	23.278746
107.198036	3219.702250	23.283763
107.444604	3217.105211	23.288781
107.486157	3216.218799	23.293799
107.204315	3216.658641	23.298816
107.660266	3219.093078	23.303834
107.499536	3218.325522	23.308851
107.693366	3215.781293	23.313869
107.189518	3222.359706	23.318887
107.170896	3225.159959	23.323904
107.769780	3234.047469	23.328922
108.016489	3236.646009	23.333939
108.414637	3238.538826	23.338957
108.189792	3242.651096	23.343975
108.256539	3230.635460	23.348992
108.526617	3234.095482	23.354010
108.284209	3234.596130	23.359027
108.913432	3241.425901	23.364045
109.092834	3265.198715	23.369063
108.565180	3255.027716	23.374080
109.174443	3257.107302	23.379098
109.078796	3254.124684	23.384115
109.201735	3256.868087	23.389133
108.971093	3261.171869	23.394151
109.189898	3271.693054	23.399168
109.257534	3259.284733	23.404186
109.071220	3287.096708	23.409203
109.390756	3284.979723	23.414221
109.574408	3292.450853	23.419239
109.332915	3295.060783	23.424256
109.944132	3307.863588	23.429274
109.988862	3320.936779	23.434291
109.879733	3317.064650	23.439309
110.139933	3325.632589	23.444327
110.493636	3334.426419	23.449344
110.835913	3335.398565	23.454362
110.747869	3339.982741	23.459379
111.012834	3334.971240	23.464397
111.262932	3338.805451	23.469415
110.891599	3338.340798	23.474432
111.416381	3344.355200	23.479450
111.019195	3347.747160	23.484467
111.506965	3337.302808	23.489485
111.464345	3337.965721	23.494503
111.355351	3351.385991	23.499520
111.910202	3351.611205	23.504538
111.500954	3357.687431	23.509555
111.645587	3362.243796	23.514573
111.773258	3366.727375	23.519591
112.029200	3389.070021	23.524608
112.235775	3389.811444	23.529626
112.185547	3390.230342	23.534643
112.230376	3397.427219	23.539661
112.497042	3407.340195	23.544679
112.298206	3422.305290	23.549696
112.664810	3425.556886	23.554714
112.850998	3421.556406	23.559731
112.721577	3423.611225	23.564749
113.296487	3436.402813	23.569767
113.352412	3445.241186	23.574784
113.512006	3442.401395	23.579802
113.304642	3448.652172	23.584819
113.854155	3441.068812	23.589837
113.877784	3455.888913	23.594855
113.801259	3454.790501	23.599872
114.254228	3447.773486	23.604890
114.038118	3458.682805	23.609907
114.243893	3464.138941	23.614925
114.823009	3469.612918	23.619943
114.421143	3481.990746	23.624960
114.883383	3468.883587	23.629978
114.810629	3478.614504	23.634995
114.445583	3469.566104	23.640013
115.004315	3467.109570	23.645031
114.889530	3466.075354	23.650048
115.305162	3481.590549	23.655066
114.969222	3497.163019	23.660083
115.054208	3493.786726	23.665101
115.265234	3505.606605	23.670119
115.254887	3506.683880	23.675136
115.383584	3509.619292	23.680154
115.837175	3514.710087	23.685171
115.966393	3520.355272	23.690189
115.948690	3516.352632	23.695207
116.059943	3509.130635	23.700224
116.480018	3506.782046	23.705242
116.184791	3508.388286	23.710259
116.686633	3514.189222	23.715277
116.681367	3532.702774	23.720295
116.820046	3545.013775	23.725312
117.087258	3542.656975	23.730330
117.027284	3545.113722	23.735347
117.252365	3531.505931	23.740365
117.257909	3530.459701	23.745383
117.158327	3540.749819	23.750400
117.370894	3539.103628	23.755418
117.158036	3550.169955	23.760435
117.133909	3565.763412	23.765453
117.332585	3566.075044	23.770471
117.272651	3571.969615	23.775488
117.753077	3572.044926	23.780506
117.733557	3601.974018	23.785523
118.082595	3605.769506	23.790541
118.428969	3599.922412	23.795559
118.065359	3606.821911	23.800576
118.777460	3609.675508	23.805594
118.960825	3612.190484	23.810611
118.737288	3619.707796	23.815629
118.937225	3619.383386	23.820647
119.108005	3628.558402	23.825664
119.448134	3616.267763	23.830682
119.480743	3616.530064	23.835699
119.792746	3610.266200	23.840717
119.789962	3609.747725	23.845735
119.660739	3614.994306	23.850752
119.841323	3632.858363	23.855770
120.082635	3640.163045	23.860787
120.211806	3643.339746	23.865805
120.705992	3630.532689	23.870823
120.083220	3646.064119	23.875840
120.354654	3635.410824	23.880858
120.338948	3642.379625	23.885875
120.204938	3645.015947	23.890893
121.181027	3660.886752	23.895911
120.747013	3665.316770	23.900928
120.948058	3667.454813	23.905946
120.746804	3673.023556	23.910963
120.998173	3680.363210	23.915981
121.487765	3684.383923	23.920999
121.215826	3700.007438	23.926016
121.642340	3697.786894	23.931034
121.803975	3690.276956	23.936051
121.446256	3700.011397	23.941069
122.047405	3704.593612	23.946087
122.036506	3728.143458	23.951104
121.787958	3723.915123	23.956122
121.809286	3729.180567	23.961139
122.122342	3750.917828	23.966157
122.401287	3754.977697	23.971175
122.366753	3750.704149	23.976192
122.890431	3760.037864	23.981210
122.898400	3755.317913	23.986227
123.434759	3760.076603	23.991245
123.923552	3753.228339	23.996263
123.975157	3766.072024	24.001280
124.058860	3751.918885	24.006298
124.220332	3734.160711	24.011315
124.074132	3726.624454	24.016333
124.171324	3710.805705	24.021351
124.021527	3716.357299	24.026368
124.225956	3715.282525	24.031386
124.106205	3723.670549	24.036403
124.090522	3734.424106	24.041421
124.398959	3738.349173	24.046439
124.187392	3751.583583	24.051456
124.050798	3747.946598	24.056474
124.447295	3756.536350	24.061491
124.448186	3773.677096	24.066509
124.762224	3777.389432	24.071527
124.665771	3798.523151	24.076544
125.105713	3794.106622	24.081562
125.196900	3807.749726	24.086579
124.920069	3819.323676	24.091597
125.164540	3812.307485	24.096615
125.183130	3834.448253	24.101632
125.598926	3837.982369	24.106650
125.780348	3842.497363	24.111667
125.838825	3856.386078	24.116685
126.548412	3858.964541	24.121703
126.564667	3863.326513	24.126720
126.566967	3868.149860	24.131738
126.772199	3858.225877	24.136755
126.788877	3861.629091	24.141773
127.251581	3855.823311	24.146791
127.015701	3883.300045	24.151808
127.068379	3887.837506	24.156826
127.341646	3894.468899	24.161843
127.246436	3893.989310	24.166861
127.341107	3887.720300	24.171879
127.224446	3894.925587	24.176896
127.282392	3912.800387	24.181914
127.478029	3923.780188	24.186931
127.508048	3928.923000	24.191949
127.629671	3948.319259	24.196967
128.092138	3956.877355	24.201984
127.942429	3954.333470	24.207002
128.114867	3970.874414	24.212019
128.528861	3978.105839	24.217037
128.420716	3986.086954	24.222055
128.544766	4013.259945	24.227072
128.818868	4016.403325	24.232090
129.023229	4019.894857	24.237107
129.272580	4025.221940	24.242125
129.618232	4052.004038	24.247143
129.724345	4044.947216	24.252160
129.809587	4043.739352	24.257178
130.164410	4031.173903	24.262195
129.811075	4032.647271	24.267213
130.100788	4039.822093	24.272231
130.305452	4050.175664	24.277248
130.804939	4060.247053	24.282266
130.712083	4064.152288	24.287283
130.418404	4057.328456	24.292301
130.408835	4065.180326	24.297319
130.624809	4074.627284	24.302336
130.607685	4089.789775	24.307354
130.993494	4095.506951	24.312371
130.941002	4098.709825	24.317389
131.335829	4107.310679	24.322407
131.456735	4119.842798	24.327424
131.618500	4123.286271	24.332442
131.978756	4124.131478	24.337459
131.793033	4139.875445	24.342477
132.076914	4152.073954	24.347495
132.164747	4159.989309	24.352512
132.037572	4166.253894	24.357530
132.331776	4152.629809	24.362547
132.398427	4160.183292	24.367565
132.412652	4168.575403	24.372583
132.428592	4182.643099	24.377600
132.781409	4180.125202	24.382618
132.864924	4185.990791	24.387635
132.971474	4213.911942	24.392653
133.427636	4219.955351	24.397671
133.140109	4211.757530	24.402688
133.366746	4217.780200	24.407706
134.125889	4227.737924	24.412723
133.679292	4233.362761	24.417741
133.715205	4244.532575	24.422759
133.952676	4248.460049	24.427776
134.242957	4247.149389	24.432794
134.351089	4244.037628	24.437811
134.282443	4259.942301	24.442829
134.535209	4254.697077	24.447847
134.962624	4253.074372	24.452864
134.858174	4260.860911	24.457882
135.347121	4267.512340	24.462899
135.341550	4286.807984	24.467917
135.421705	4285.039100	24.472935
135.784454	4282.755780	24.477952
135.620108	4283.288444	24.482970
135.747171	4278.223441	24.487987
135.895495	4282.309363	24.493005
136.138111	4287.038010	24.498023
136.319054	4307.253306	24.503040
136.084367	4314.128662	24.508058
136.322866	4304.094956	24.513075
136.500929	4319.126988	24.518093
136.654584	4337.093947	24.523111
136.490063	4337.251817	24.528128
137.145761	4331.183253	24.533146
137.439765	4325.831186	24.538163
137.456779	4329.361619	24.543181
137.434288	4347.565188	24.548199
137.936465	4351.684397	24.553216
137.749981	4360.299550	24.558234
138.042459	4363.306493	24.563251
137.878902	4359.776582	24.568269
137.966152	4366.352294	24.573287
138.148188	4378.866646	24.578304
138.315524	4393.608379	24.583322
138.408034	4392.532366	24.588339
138.835805	4378.611195	24.593357
138.632496	4394.579597	24.598375
139.131708	4402.879885	24.603392
139.238100	4414.183067	24.608410
139.556934	4403.989557	24.613427
139.311116	4406.721651	24.618445
139.420456	4410.375832	24.623463
139.696759	4423.894788	24.628480
140.066923	4443.166338	24.633498
139.850650	4441.862586	24.638515
139.824378	4445.747070	24.643533
140.208820	4442.432123	24.648551
140.448385	4450.520993	24.653568
140.532938	4461.819942	24.658586
140.714488	4469.985735	24.663603
140.683333	4467.903705	24.668621
140.905768	4461.217659	24.673639
141.588321	4461.897813	24.678656
141.352761	4469.766361	24.683674
141.767437	4467.106299	24.688691
141.800158	4474.523800	24.693709
142.064080	4483.578806	24.698727
142.044688	4481.175517	24.703744
142.003289	4475.839447	24.708762
142.354682	4470.101052	24.713779
142.364452	4476.971521	24.718797
142.384930	4463.481377	24.723815
142.776374	4464.840384	24.728832
142.296397	4456.090335	24.733850
142.781013	4465.520310	24.738867
142.685577	4494.962840	24.743885
142.743064	4496.997545	24.748903
143.099873	4495.465228	24.753920
142.578779	4516.553541	24.758938
143.022990	4524.835029	24.763955
143.446312	4537.719512	24.768973
143.320060	4532.709276	24.773991
143.836189	4544.038163	24.779008
143.974894	4564.620641	24.784026
143.814146	4563.188009	24.789043
144.000399	4565.505800	24.794061
144.175656	4581.621699	24.799079
144.443715	4581.549421	24.804096
144.366699	4591.037230	24.809114
144.666992	4596.541540	24.814131
144.939599	4615.992428	24.819149
144.961598	4615.155234	24.824167
145.007726	4607.988770	24.829184
145.044222	4636.736095	24.834202
145.534415	4638.365830	24.839219
145.914313	4640.045683	24.844237
145.770600	4657.668809	24.849255
145.839790	4667.111244	24.854272
145.890824	4671.605502	24.859290
146.216145	4681.197372	24.864307
146.382598	4687.426248	24.869325
146.384812	4695.563519	24.874343
146.646508	4700.046601	24.879360
146.620809	4707.197070	24.884378
146.665458	4718.184270	24.889395
146.857584	4731.338236	24.894413
147.055898	4732.889034	24.899431
147.560943	4745.755856	24.904448
147.845350	4754.335548	24.909466
147.844170	4756.795764	24.914483
148.392326	4755.262123	24.919501
148.192905	4767.232679	24.924519
148.227124	4764.746073	24.929536
148.490276	4780.393284	24.934554
148.840067	4772.647784	24.939571
149.158218	4781.973949	24.944589
148.906187	4790.598593	24.949607
149.221419	4778.253673	24.954624
149.401382	4790.111949	24.959642
149.353267	4781.583298	24.964659
149.690917	4809.419294	24.969677
149.100026	4804.804670	24.974695
149.793334	4809.290489	24.979712
149.451018	4812.460682	24.984730
149.799777	4838.104936	24.989747
150.160595	4841.023115	24.994765
149.825323	4854.523801	24.999783
150.360643	4861.629285	25.004800
150.284041	4874.940384	25.009818
150.315449	4871.940398	25.014835
150.622926	4889.808161	25.019853
150.535294	4910.284384	25.024871
151.015113	4917.474663	25.029888
150.912846	4937.848606	25.034906
151.462201	4929.741675	25.039923
151.638964	4931.495286	25.044941
151.843243	4931.654040	25.049959
152.660062	4935.503682	25.054976
152.596160	4937.845931	25.059994
152.766433	4936.386919	25.065011
153.054647	4941.440154	25.070029
153.042713	4953.193240	25.075047
152.990971	4937.748286	25.080064
152.923814	4944.385191	25.085082
153.177826	4936.342414	25.090099
153.414795	4936.300078	25.095117
153.002287	4947.159018	25.100135
153.212725	4947.219108	25.105152
153.406025	4971.971856	25.110170
153.440586	4985.834817	25.115187
153.674028	4980.636250	25.120205
153.662246	4994.067462	25.125223
153.953785	5002.679581	25.130240
154.170564	5002.361026	25.135258
154.559187	5025.222342	25.140275
154.435720	5023.615380	25.145293
154.716201	5035.935629	25.150311
155.323891	5037.158948	25.155328
155.645751	5049.477489	25.160346
155.839341	5049.293093	25.165363
155.852312	5049.405892	25.170381
155.859915	5054.789024	25.175399
156.053872	5041.317360	25.180416
156.421825	5043.630399	25.185434
156.020815	5050.741454	25.190451
156.211520	5055.881712	25.195469
156.167735	5080.250927	25.200487
156.361241	5078.602610	25.205504
156.365893	5084.319740	25.210522
156.334469	5096.961681	25.215539
156.359163	5109.226605	25.220557
156.339515	5136.487113	25.225575
156.966432	5135.638926	25.230592
156.901811	5160.070769	25.235610
157.087405	5172.002429	25.240627
157.656370	5180.040795	25.245645
157.796760	5203.818684	25.250663
158.227959	5201.008511	25.255680
158.536621	5202.464344	25.260698
158.492917	5219.708938	25.265715
158.793722	5230.524235	25.270733
158.875123	5232.613754	25.275751
159.020121	5218.221968	25.280768
159.408651	5229.784669	25.285786
159.754636	5241.526869	25.290803
160.085273	5237.696178	25.295821
160.279627	5247.182070	25.300839
160.292087	5241.705327	25.305856
160.187814	5246.016726	25.310874
160.222329	5243.085849	25.315891
160.621320	5239.757702	25.320909
160.362532	5239.180674	25.325927
160.616023	5237.989806	25.330944
160.730469	5260.663279	25.335962
160.524405	5264.534755	25.340979
160.880819	5259.523283	25.345997
160.921426	5288.097089	25.351015
161.211857	5289.178733	25.356032
161.410976	5293.991656	25.361050
161.985583	5312.281175	25.366067
162.326453	5318.732303	25.371085
162.037025	5329.249083	25.376103
162.516293	5329.049375	25.381120
162.512381	5328.965728	25.386138
162.506373	5330.785022	25.391155
162.643411	5334.187176	25.396173
162.488653	5335.108888	25.401191
162.582661	5353.107348	25.406208
162.999439	5353.389283	25.411226
163.069986	5369.699697	25.416243
163.396881	5372.186127	25.421261
163.339361	5388.403140	25.426279
163.548328	5386.892805	25.431296
163.773468	5394.613243	25.436314
163.829467	5415.143570	25.441331
164.088214	5403.451275	25.446349
163.907605	5422.852842	25.451367
164.472695	5425.021935	25.456384
164.620313	5438.494522	25.461402
164.317875	5456.305816	25.466419
165.087826	5461.246155	25.471437
164.901287	5478.172463	25.476455
165.290834	5476.123161	25.481472
165.561297	5491.557646	25.486490
165.693265	5501.054000	25.491507
165.498673	5491.354517	25.496525
165.655452	5529.457290	25.501543
165.349680	5530.037775	25.506560
166.162645	5545.878018	25.511578
166.050696	5566.269340	25.516595
166.380981	5572.859348	25.521613
166.723751	5586.630178	25.526631
166.926943	5588.783884	25.531648
167.480774	5594.980617	25.536666
167.332826	5618.674869	25.541683
167.857787	5623.741973	25.546701
168.020100	5619.726768	25.551719
168.066842	5618.323542	25.556736
168.398544	5617.679252	25.561754
168.568127	5644.979860	25.566771
168.947212	5643.517388	25.571789
168.854087	5652.573400	25.576807
169.042979	5651.572729	25.581824
169.056687	5656.617609	25.586842
168.958359	5663.690740	25.591859
169.048588	5671.506451	25.596877
169.380172	5680.274162	25.601895
169.463947	5676.228212	25.606912
169.635624	5692.402156	25.611930
170.004303	5704.164188	25.616947
170.318447	5694.801448	25.621965
170.275197	5703.716158	25.626983
170.699089	5705.662917	25.632000
170.832789	5710.632469	25.637018
170.623227	5730.925944	25.642035
170.818491	5729.822625	25.647053
170.828157	5736.536949	25.652071
171.251171	5762.412613	25.657088
171.231741	5752.740334	25.662106
171.420673	5772.053709	25.667123
171.783386	5782.677244	25.672141
172.265310	5799.502505	25.677159
172.142469	5801.701055	25.682176
172.631826	5813.950393	25.687194
172.443198	5814.298900	25.692212
173.070724	5812.302769	25.697229
173.075961	5814.588836	25.702247
172.805496	5826.899152	25.707264
173.560489	5840.878122	25.712282
173.568808	5847.087126	25.717300
173.603539	5841.923078	25.722317
173.647919	5865.424089	25.727335
173.442532	5870.793473	25.732352
174.066328	5862.678099	25.737370
174.014807	5877.440068	25.742388
174.332800	5891.539327	25.747405
174.341838	5896.022763	25.752423
174.568153	5887.980138	25.757440
174.704519	5906.102963	25.762458
174.750648	5919.635259	25.767476
174.883988	5916.880478	25.772493
175.202016	5931.247526	25.777511
175.578266	5943.970058	25.782528
176.006810	5945.572718	25.787546
175.872472	5960.731975	25.792564
176.124943	5969.716104	25.797581
176.388635	5981.434264	25.802599
176.513419	5993.236024	25.807616
176.453779	5989.425535	25.812634
176.469498	6015.295673	25.817652
176.919265	6007.661811	25.822669
177.106489	6010.158034	25.827687
176.824296	6037.046883	25.832704
177.536745	6035.308392	25.837722
177.454105	6059.661528	25.842740
177.621971	6073.983428	25.847757
178.101085	6073.768778	25.852775
178.410471	6070.048503	25.857792
178.867662	6087.457787	25.862810
178.802503	6097.100085	25.867828
179.238891	6097.334302	25.872845
179.291830	6103.733707	25.877863
179.350604	6105.428193	25.882880
179.555948	6103.390741	25.887898
179.549680	6119.289751	25.892916
179.456522	6127.749876	25.897933
179.431806	6136.270362	25.902951
179.438034	6170.474478	25.907968
180.139736	6162.757175	25.912986
179.986481	6180.473760	25.918004
180.437895	6185.955240	25.923021
180.458295	6192.320680	25.928039
180.813405	6215.769298	25.933056
181.278813	6211.827113	25.938074
181.023791	6224.590387	25.943092
181.568752	6230.932174	25.948109
182.618091	6228.050404	25.953127
182.454544	6240.348889	25.958144
182.868528	6225.845584	25.963162
182.669268	6231.781109	25.968180
182.948735	6218.021425	25.973197
183.236758	6219.308689	25.978215
183.202197	6222.055803	25.983232
183.548865	6240.798715	25.988250
183.601616	6237.616957	25.993268
183.666975	6243.341017	25.998285
184.010295	6244.240338	26.003303
183.591260	6257.871047	26.008320
184.329428	6248.083525	26.013338
184.193145	6262.677938	26.018356
183.919002	6269.394493	26.023373
184.505283	6270.754550	26.028391
184.374233	6280.603946	26.033408
184.808084	6308.257786	26.038426
184.750078	6309.606169	26.043444
184.755791	6325.176575	26.048461
185.388512	6345.619129	26.053479
185.261743	6340.385521	26.058496
185.851578	6351.329464	26.063514
185.422215	6373.280858	26.068532
185.868181	6379.399648	26.073549
186.101821	6393.069118	26.078567
186.266311	6393.104125	26.083584
186.772794	6390.293122	26.088602
186.870866	6414.889441	26.093620
186.826188	6423.414957	26.098637
187.556623	6421.864831	26.103655
187.520597	6427.467888	26.108672
187.722857	6416.749716	26.113690
187.952076	6431.391790	26.118708
187.735199	6448.730925	26.123725
188.169928	6446.740584	26.128743
187.899242	6460.304428	26.133760
188.328983	6477.650164	26.138778
187.860963	6486.225972	26.143796
188.375374	6502.603229	26.148813
188.613780	6511.285208	26.153831
188.861965	6541.435976	26.158848
189.117608	6547.557139	26.163866
189.419808	6566.214067	26.168884
189.960052	6568.285837	26.173901
189.905865	6572.756285	26.178919
190.074906	6591.684902	26.183936
190.396111	6604.467471	26.188954
190.522612	6607.319563	26.193972
190.748807	6626.868040	26.198989
190.935081	6628.599009	26.204007
190.806873	6636.044516	26.209024
191.017890	6649.943191	26.214042
191.014195	6666.080959	26.219060
191.474085	6691.870157	26.224077
191.761027	6699.593630	26.229095
191.826482	6715.683008	26.234112
192.368713	6726.216094	26.239130
192.716748	6736.550515	26.244148
193.016155	6723.480945	26.249165
193.354930	6729.386826	26.254183
193.546199	6749.656338	26.259200
193.839550	6754.040275	26.264218
194.170299	6745.689348	26.269236
193.839737	6756.376113	26.274253
194.121081	6747.122130	26.279271
194.525410	6747.289989	26.284288
194.640588	6762.210323	26.289306
194.563258	6768.958364	26.294324
194.893246	6769.083376	26.299341
195.320610	6768.414181	26.304359
195.030438	6775.513994	26.309376
195.027015	6779.781584	26.314394
195.345703	6789.389237	26.319412
195.350956	6812.661069	26.324429
195.748175	6819.151157	26.329447
195.684506	6845.943847	26.334464
196.053223	6848.191273	26.339482
196.579875	6851.790859	26.344500
196.388422	6865.607371	26.349517
196.890804	6876.378689	26.354535
196.820605	6890.783197	26.359552
196.952339	6907.042175	26.364570
197.402997	6922.017491	26.369588
196.950760	6927.013753	26.374605
197.696191	6937.826864	26.379623
198.101670	6951.864580	26.384640
198.397287	6973.519029	26.389658
198.052854	6980.697994	26.394676
198.008403	6997.471324	26.399693
198.312684	7012.365376	26.404711
198.766621	7033.200654	26.409728
198.872484	7049.506582	26.414746
199.352559	7050.477868	26.419764
199.370870	7044.098535	26.424781
200.204874	7050.284215	26.429799
200.519227	7057.245679	26.434816
200.583507	7068.755024	26.439834
200.942349	7061.469616	26.444852
200.861935	7070.339260	26.449869
201.089957	7059.128881	26.454887
201.148242	7073.991966	26.459904
201.148241	7077.213158	26.464922
201.452114	7086.049245	26.469940
201.435897	7090.601775	26.474957
201.806368	7099.441042	26.479975
201.684251	7118.972860	26.484992
201.816918	7136.688956	26.490010
202.364548	7137.501019	26.495028
202.438569	7157.172959	26.500045
202.525630	7157.723245	26.505063
202.524017	7179.939021	26.510080
203.040414	7185.420357	26.515098
203.072436	7186.597996	26.520116
203.025086	7211.262904	26.525133
203.439662	7227.136027	26.530151
203.693316	7244.263612	26.535168
203.839427	7267.079665	26.540186
204.399265	7272.325452	26.545204
204.397721	7281.703570	26.550221
204.842102	7293.488942	26.555239
204.673192	7314.518076	26.560256
205.072537	7311.136281	26.565274
205.577739	7333.593025	26.570292
205.682552	7340.674298	26.575309
205.795298	7333.825589	26.580327
206.112604	7354.155389	26.585344
205.817625	7365.963738	26.590362
206.234110	7383.731668	26.595380
206.242382	7401.156725	26.600397
206.827607	7414.427174	26.605415
207.215253	7427.188409	26.610432
207.254504	7437.786963	26.615450
207.457810	7448.122926	26.620468
207.708476	7458.009225	26.625485
207.776928	7474.980211	26.630503
207.962022	7493.173210	26.635520
208.142502	7510.080043	26.640538
208.769213	7510.165491	26.645556
208.739127	7535.729861	26.650573
209.238319	7530.383770	26.655591
209.249338	7535.371413	26.660608
209.000546	7542.769535	26.665626
209.846880	7553.907437	26.670644
209.245629	7571.341238	26.675661
209.692424	7587.129065	26.680679
209.918315	7598.266332	26.685696
210.319234	7615.759070	26.690714
210.641384	7616.984106	26.695732
210.997997	7640.805566	26.700749
211.168346	7644.735934	26.705767
211.316464	7660.065172	26.710784
211.474345	7693.073987	26.715802
211.561370	7679.042387	26.720820
212.228913	7674.901837	26.725837
212.821270	7690.450699	26.730855
212.992038	7695.658523	26.735872
212.898859	7701.258872	26.740890
213.326946	7688.741419	26.745908
213.830062	7687.020022	26.750925
213.603152	7688.631925	26.755943
213.777686	7688.134426	26.760960
213.692693	7709.027351	26.765978
214.140317	7715.618175	26.770996
213.954715	7728.499571	26.776013
214.041822	7735.992720	26.781031
214.119552	7744.642070	26.786048
214.304326	7758.237313	26.791066
214.374735	7762.379551	26.796084
214.276998	7781.569482	26.801101
214.407445	7794.708248	26.806119
214.711202	7815.537082	26.811136
214.742265	7848.413588	26.816154
215.140521	7875.372715	26.821172
215.412938	7889.886137	26.826189
215.666432	7914.289775	26.831207
216.155657	7929.807080	26.836224
216.239522	7935.528697	26.841242
217.033634	7949.124244	26.846260
216.765057	7955.282949	26.851277
217.168616	7973.578241	26.856295
217.485379	7996.357699	26.861312
217.396626	8014.029448	26.866330
218.006025	8024.163221	26.871348
218.117981	8038.897837	26.876365
218.696222	8053.901986	26.881383
218.721408	8070.217571	26.886400
219.200637	8079.563986	26.891418
219.445830	8097.134182	26.896436
219.874126	8103.427486	26.901453
219.547653	8115.481036	26.906471
220.118152	8111.659650	26.911488
219.982466	8127.217388	26.916506
220.407318	8126.951829	26.921524
220.329642	8151.079740	26.926541
220.449062	8164.697157	26.931559
220.836964	8173.617638	26.936576
220.611017	8198.905896	26.941594
220.992382	8220.598298	26.946612
221.399663	8240.592228	26.951629
221.253854	8237.739816	26.956647
221.668252	8258.412329	26.961664
221.676159	8286.900880	26.966682
221.926565	8300.397528	26.971700
222.394330	8319.170165	26.976717
222.466302	8337.822332	26.981735
223.200136	8354.607136	26.986752
223.098219	8367.706792	26.991770
223.503234	8382.546113	26.996788
223.841823	8399.019770	27.001805
223.785015	8414.768758	27.006823
224.178488	8423.857806	27.011840
224.280624	8445.519461	27.016858
224.906836	8454.095906	27.021876
224.860726	8468.280475	27.026893
225.094203	8493.109706	27.031911
225.710818	8485.348638	27.036928
225.352105	8514.714970	27.041946
225.537823	8523.717102	27.046964
225.627784	8546.953857	27.051981
226.153514	8561.331525	27.056999
226.342164	8573.216032	27.062016
226.517429	8593.281035	27.067034
226.936720	8610.700950	27.072052
226.966304	8628.314447	27.077069
227.087203	8639.698218	27.082087
227.789552	8660.284296	27.087104
227.711259	8674.199471	27.092122
227.992294	8688.742922	27.097140
228.024407	8689.471689	27.102157
228.300764	8708.238604	27.107175
229.143715	8724.656838	27.112192
228.927092	8730.389006	27.117210
229.141358	8749.631739	27.122228
229.276935	8746.102611	27.127245
229.842217	8754.695588	27.132263
229.881208	8766.335585	27.137280
230.372402	8779.572311	27.142298
230.588165	8778.083381	27.147316
230.672058	8795.873982	27.152333
230.608211	8806.366034	27.157351
231.321331	8798.556577	27.162368
231.431586	8821.614730	27.167386
231.210702	8833.481240	27.172404
231.691755	8861.453127	27.177421
231.857029	8872.149970	27.182439
231.888827	8874.312365	27.187456
232.143488	8896.670945	27.192474
232.165421	8902.318074	27.197492
232.674094	8934.613018	27.202509
232.727388	8957.058514	27.207527
233.069125	8968.473774	27.212544
233.618809	8996.899291	27.217562
233.617847	9011.764530	27.222580
233.966280	9020.998420	27.227597
233.649749	9051.376455	27.232615
234.121413	9068.432187	27.237632
234.129086	9079.130002	27.242650
234.681948	9096.379510	27.247668
234.457020	9116.913014	27.252685
234.930702	9142.695271	27.257703
235.560884	9160.602396	27.262720
235.671802	9196.353012	27.267738
236.387256	9205.419245	27.272756
236.629986	9205.111296	27.277773
237.099119	9220.285817	27.282791
237.604811	9219.550028	27.287808
237.901725	9222.797430	27.292826
238.067003	9218.215660	27.297844
238.068318	9227.722061	27.302861
238.243595	9246.516553	27.307879
238.763693	9246.883516	27.312896
238.681051	9253.371187	27.317914
238.962224	9261.368624	27.322932
239.179043	9272.943377	27.327949
239.068992	9275.109570	27.332967
239.180398	9294.522771	27.337984
239.603106	9312.229613	27.343002
239.849137	9315.206597	27.348020
240.128655	9328.259776	27.353037
240.169684	9346.368427	27.358055
240.892621	9371.827880	27.363072
240.644111	9380.635998	27.368090
240.711090	9394.133163	27.373108
241.114219	9408.396373	27.378125
241.674973	9440.470273	27.383143
241.594033	9434.188300	27.388160
241.280759	9456.426457	27.393178
241.740804	9472.017840	27.398196
242.078912	9494.691945	27.403213
241.859031	9521.255017	27.408231
243.055341	9535.087965	27.413248
242.663625	9570.780677	27.418266
243.144219	9580.715388	27.423284
243.562443	9605.550492	27.428301
243.881043	9622.127187	27.433319
244.302677	9633.837720	27.438336
244.234920	9653.110813	27.443354
244.544537	9654.324695	27.448372
244.828842	9663.003977	27.453389
245.221920	9679.458146	27.458407
245.920708	9686.454935	27.463424
245.895837	9696.154206	27.468442
246.305036	9695.509173	27.473460
246.545448	9695.870369	27.478477
246.571926	9708.326830	27.483495
247.054588	9708.139926	27.488512
247.273323	9715.554759	27.493530
247.265952	9718.162498	27.498548
247.847674	9730.281474	27.503565
247.754967	9753.287073	27.508583
247.823370	9750.938582	27.513600
247.729559	9767.337797	27.518618
248.143794	9772.441488	27.523636
248.143459	9781.582990	27.528653
248.572892	9799.007261	27.533671
249.103229	9814.478662	27.538688
249.155875	9820.085596	27.543706
249.078553	9842.705161	27.548724
249.459664	9866.160413	27.553741
249.435847	9887.635306	27.558759
250.560216	9900.061770	27.563776
251.286197	9908.880900	27.568794
251.185003	9915.446739	27.573812
251.740507	9909.676216	27.578829
251.628435	9933.679383	27.583847
251.944093	9935.950207	27.588864
252.115271	9946.969766	27.593882
252.359229	9963.625318	27.598900
252.596481	9976.748243	27.603917
252.500518	9990.353181	27.608935
252.638993	10005.706757	27.613952
252.723260	10026.135203	27.618970
252.865071	10045.031481	27.623988
253.431610	10059.489631	27.629005
253.773269	10069.816262	27.634023
253.799424	10082.128125	27.639040
254.249694	10108.443599	27.644058
254.321438	10130.015674	27.649076
254.775391	10134.832486	27.654093
254.904515	10168.178888	27.659111
255.268122	10175.189523	27.664128
255.484742	10200.473215	27.669146
255.383597	10226.386860	27.674164
255.791031	10236.730303	27.679181
256.026071	10273.274987	27.684199
255.964753	10282.150352	27.689216
256.494411	10315.248130	27.694234
256.391587	10335.424292	27.699252
257.027664	10354.719013	27.704269
257.220912	10378.161943	27.709287
257.407506	10409.140833	27.714304
257.948910	10423.493969	27.719322
258.163802	10444.396862	27.724340
258.220638	10476.777462	27.729357
258.253020	10494.302753	27.734375
258.886821	10511.643623	27.739392
259.111416	10538.227901	27.744410
259.380913	10555.053944	27.749428
259.948707	10567.644576	27.754445
259.904096	10604.066849	27.759463
260.199910	10617.959721	27.764480
260.570580	10640.398474	27.769498
260.904785	10659.814337	27.774516
261.391649	10676.573085	27.779533
261.390200	10689.632049	27.784551
261.639288	10707.771676	27.789568
261.865181	10725.071458	27.794586
262.074005	10745.941086	27.799604
262.451448	10751.438753	27.804621
262.619451	10775.247232	27.809639
262.812215	10782.557353	27.814656
263.056353	10806.608537	27.819674
263.347100	10823.729917	27.824692
263.266750	10839.463914	27.829709
263.772725	10866.765600	27.834727
264.047563	10883.154680	27.839744
264.100288	10901.705887	27.844762
264.462160	10939.400192	27.849780
265.117118	10953.702747	27.854797
265.133009	10964.372893	27.859815
265.560570	10985.659667	27.864832
265.807275	11005.508716	27.869850
265.984415	11023.440797	27.874868
266.077166	11050.451839	27.879885
266.001241	11079.225492	27.884903
266.670174	11102.615312	27.889920
267.189970	11121.732439	27.894938
267.369543	11147.126157	27.899956
267.721271	11160.077523	27.904973
267.793645	11188.985216	27.909991
268.072846	11208.328114	27.915008
268.524761	11231.260034	27.920026
268.639943	11250.082566	27.925044
269.144581	11272.111690	27.930061
269.307957	11299.759048	27.935079
269.497774	11321.101302	27.940096
270.085490	11334.134353	27.945114
270.318772	11342.804861	27.950132
270.821446	11366.225687	27.955149
271.042247	11365.465192	27.960167
271.888808	11374.209286	27.965184
272.028877	11375.711290	27.970202
272.229136	11393.657297	27.975220
272.325808	11415.370362	27.980237
272.712437	11418.769621	27.985255
272.878348	11429.842279	27.990272
273.082940	11445.364355	27.995290
273.018371	11462.023595	28.000308
273.616720	11465.653375	28.005325
273.201125	11489.650717	28.010343
273.723157	11510.825681	28.015360
274.180220	11525.345002	28.020378
274.299991	11555.693509	28.025396
274.636371	11566.445034	28.030413
274.756172	11594.836698	28.035431
274.840545	11622.130545	28.040448
275.121863	11639.240173	28.045466
274.963145	11670.203705	28.050484
275.471253	11695.604673	28.055501
275.976156	11715.036944	28.060519
275.962838	11742.576388	28.065536
276.988047	11761.578478	28.070554
277.101879	11787.233019	28.075572
277.275898	11803.226091	28.080589
277.795434	11831.706545	28.085607
278.102903	11837.228754	28.090624
278.327403	11867.503036	28.095642
278.250595	11878.816998	28.100660
278.489183	11891.886913	28.105677
278.882591	11916.886484	28.110695
278.881127	11939.840748	28.115712
279.506521	11960.491870	28.120730
279.633754	11985.590671	28.125748
279.993078	11991.852015	28.130765
280.516149	12003.206402	28.135783
280.940877	12024.708525	28.140800
281.401885	12022.772266	28.145818
281.564262	12051.954198	28.150836
281.904715	12046.684847	28.155853
282.001700	12058.698177	28.160871
282.173000	12076.908139	28.165888
282.675907	12096.849353	28.170906
282.506552	12118.122800	28.175924
283.026323	12127.163953	28.180941
283.578530	12148.849231	28.185959
283.267854	12157.160981	28.190976
283.693396	12169.477790	28.195994
283.784987	12206.546909	28.201012
284.005777	12228.761327	28.206029
284.361454	12254.893479	28.211047
284.633636	12273.132690	28.216064
284.736687	12301.436978	28.221082
284.941304	12333.189473	28.226100
285.562115	12347.124692	28.231117
285.649155	12371.980987	28.236135
285.990897	12403.627455	28.241152
286.064087	12421.122892	28.246170
286.659296	12446.784041	28.251188
286.805118	12466.977732	28.256205
287.422636	12487.824645	28.261223
287.892257	12507.583571	28.266240
288.471662	12517.706270	28.271258
288.720591	12534.559846	28.276276
288.833409	12554.440806	28.281293
289.149331	12566.934389	28.286311
289.026858	12594.559500	28.291328
289.751368	12595.361566	28.296346
290.077903	12621.398281	28.301364
290.301767	12648.523490	28.306381
290.519576	12665.076655	28.311399
291.000629	12695.238410	28.316416
290.943221	12705.496374	28.321434
291.223741	12729.274974	28.326452
291.407733	12750.247425	28.331469
291.731305	12763.898058	28.336487
292.069770	12798.938391	28.341504
292.639143	12796.891960	28.346522
292.542091	12830.587728	28.351540
293.269535	12852.130761	28.356557
293.834100	12871.708996	28.361575
293.986073	12902.979678	28.366592
294.198327	12905.662740	28.371610
294.090171	12927.197379	28.376628
294.336810	12946.260960	28.381645
294.541079	12965.181867	28.386663
294.604602	12983.954293	28.391680
295.037318	13019.847772	28.396698
295.475651	13060.292771	28.401716
295.512871	13081.014141	28.406733
295.984428	13102.973240	28.411751
295.979555	13133.963007	28.416768
296.579897	13156.362602	28.421786
296.621897	13180.354605	28.426804
297.020737	13207.702391	28.431821
297.479951	13239.770731	28.436839
297.737800	13266.702268	28.441856
298.135091	13296.401523	28.446874
298.617310	13322.284433	28.451892
298.819859	13346.051609	28.456909
299.430739	13356.324064	28.461927
299.479741	13377.032836	28.466944
299.881176	13397.276854	28.471962
299.973011	13413.607350	28.476980
300.040171	13430.375282	28.481997
300.478591	13461.155343	28.487015
300.817990	13488.757674	28.492032
300.871495	13509.016766	28.497050
301.396893	13528.416325	28.502068
301.749114	13554.113076	28.507085
302.609160	13554.139570	28.512103
302.901602	13584.094622	28.517120
303.061796	13597.826530	28.522138
303.357076	13606.920577	28.527156
303.552448	13627.555061	28.532173
303.915366	13643.423412	28.537191
303.876964	13658.324344	28.542208
304.728797	13671.767134	28.547226
305.431035	13681.575597	28.552244
305.688155	13693.706299	28.557261
305.691531	13707.738400	28.562279
306.054371	13723.732909	28.567296
306.373490	13740.672273	28.572314
306.651014	13752.148831	28.577332
306.670394	13768.371892	28.582349
306.964694	13772.907325	28.587367
307.093315	13810.913981	28.592384
307.445554	13830.868838	28.597402
307.936346	13849.858479	28.602420
307.662538	13872.316813	28.607437
308.059015	13893.734696	28.612455
307.978133	13930.950504	28.617472
308.555557	13952.149469	28.622490
309.138974	14000.902770	28.627508
308.854853	14024.968809	28.632525
309.465334	14049.600952	28.637543
309.678734	14086.891415	28.642560
309.982529	14113.681245	28.647578
310.212064	14136.083575	28.652596
310.677548	14165.399678	28.657613
311.325834	14186.595122	28.662631
311.586387	14226.667403	28.667648
311.960366	14251.288496	28.672666
312.392376	14270.806805	28.677684
312.321981	14302.006608	28.682701
313.016149	14325.049464	28.687719
313.231127	14348.808175	28.692736
313.622578	14367.349949	28.697754
314.308293	14399.386315	28.702772
314.362071	14420.514814	28.707789
314.917246	14445.197668	28.712807
315.029925	14464.682291	28.717824
315.589050	14479.242571	28.722842
316.136889	14495.933768	28.727860
316.304722	14513.084888	28.732877
316.644532	14528.013959	28.737895
316.907797	14555.071236	28.742912
317.226441	14567.030109	28.747930
317.350859	14584.978006	28.752948
317.524459	14610.595626	28.757965
317.574680	14620.230291	28.762983
318.034960	14637.077931	28.768000
318.856861	14647.883678	28.773018
319.796298	14659.324020	28.778036
319.772049	14658.830006	28.783053
320.308733	14673.329556	28.788071
320.550329	14693.409339	28.793088
321.071614	14703.848746	28.798106
321.053585	14725.148671	28.803124
320.990203	14730.109078	28.808141
321.367971	14744.564030	28.813159
321.166942	14773.312118	28.818176
321.508430	14796.864625	28.823194
321.659082	14804.059031	28.828212
321.732820	14821.708255	28.833229
321.977284	14849.549213	28.838247
322.029561	14882.832155	28.843264
322.149946	14925.373589	28.848282
322.935494	14958.162048	28.853300
323.285643	14990.258168	28.858317
323.388775	15010.202045	28.863335
323.616087	15040.462091	28.868352
324.311959	15073.741534	28.873370
324.524698	15101.236725	28.878388
324.511707	15148.990403	28.883405
325.207016	15167.837483	28.888423
325.409061	15204.845555	28.893440
325.994517	15232.131251	28.898458
326.944492	15257.933670	28.903476
326.995278	15288.699282	28.908493
327.334796	15306.653413	28.913511
327.440814	15334.016908	28.918528
327.992497	15363.741716	28.923546
328.173285	15384.858360	28.928564
328.454976	15422.258796	28.933581
328.460000	15442.399071	28.938599
328.938015	15484.351769	28.943616
329.300879	15515.682465	28.948634
329.632497	15544.339184	28.953652
329.885680	15588.619220	28.958669
330.512554	15608.289759	28.963687
330.658053	15640.827576	28.968704
331.191920	15670.484965	28.973722
331.701874	15704.836579	28.978740
331.902023	15719.882801	28.983757
332.523095	15740.709678	28.988775
332.524704	15761.883202	28.993792
332.822475	15788.312719	28.998810
333.372891	15813.296302	29.003828
333.568894	15844.822254	29.008845
334.077618	15872.129577	29.013863
334.503425	15899.228423	29.018880
334.576903	15926.839418	29.023898
335.224018	15950.915200	29.028916
335.427179	15975.740482	29.033933
335.736652	15994.324445	29.038951
336.143617	16012.384837	29.043968
336.189208	16044.974635	29.048986
336.857518	16073.266176	29.054004
337.020206	16110.036934	29.059021
337.050534	16130.708157	29.064039
337.466048	16163.536528	29.069056
337.536626	16201.916104	29.074074
338.079899	16221.500326	29.079092
338.120799	16268.208158	29.084109
338.445413	16302.092030	29.089127
339.036986	16332.926294	29.094144
339.171150	16366.721980	29.099162
339.742616	16391.069385	29.104180
339.783094	16426.948491	29.109197
340.227194	16463.629420	29.114215
340.773663	16492.085237	29.119232
340.783184	16528.990986	29.124250
341.550650	16563.829852	29.129268
341.925012	16594.672122	29.134285
342.386199	16626.820881	29.139303
342.411733	16648.067248	29.144320
342.637256	16678.533934	29.149338
343.689731	16692.240825	29.154356
344.238948	16734.393008	29.159373
344.363615	16744.989088	29.164391
344.655094	16761.233210	29.169408
344.818393	16793.585967	29.174426
345.315908	16803.841516	29.179444
345.552928	16836.011957	29.184461
345.890001	16856.458468	29.189479
346.135621	16872.094011	29.194496
346.187342	16889.987095	29.199514
346.788534	16916.169712	29.204532
346.964357	16952.490987	29.209549
347.186458	16986.878656	29.214567
347.981679	17018.583694	29.219584
348.131325	17043.272850	29.224602
348.578538	17072.088094	29.229620
348.610584	17106.092883	29.234637
349.136647	17131.418221	29.239655
349.508429	17159.825248	29.244672
349.777631	17205.694187	29.249690
350.273853	17222.711935	29.254708
350.605151	17247.144420	29.259725
350.887400	17272.611128	29.264743
351.816325	17298.674015	29.269760
352.238726	17317.623830	29.274778
352.993127	17329.966678	29.279796
353.306958	17363.348568	29.284813
353.604330	17372.282029	29.289831
354.045521	17395.590106	29.294848
353.923450	17415.213166	29.299866
353.870131	17432.947660	29.304884
354.493399	17458.227496	29.309901
354.538547	17485.127047	29.314919
355.115595	17512.572400	29.319936
355.136699	17537.029764	29.324954
355.773700	17566.363036	29.329972
355.884073	17598.949938	29.334989
356.277137	17636.239292	29.340007
356.982582	17650.138298	29.345024
356.854754	17687.085092	29.350042
357.635032	17724.936433	29.355060
357.561822	17757.511417	29.360077
357.763915	17788.144800	29.365095
358.302765	17810.712272	29.370112
358.576089	17853.229719	29.375130
358.931198	17883.035702	29.380148
359.392550	17913.736824	29.385165
359.967290	17942.157382	29.390183
360.550511	17977.486790	29.395200
361.153606	17999.594682	29.400218
361.178015	18029.244346	29.405236
361.529796	18061.234290	29.410253
362.035635	18090.820295	29.415271
362.309143	18115.862588	29.420288
362.098871	18149.624255	29.425306
362.753928	18176.496683	29.430324
363.308066	18207.791456	29.435341
363.285125	18246.410339	29.440359
363.788019	18271.227398	29.445376
364.458325	18312.288606	29.450394
364.624434	18335.957132	29.455412
365.284324	18366.358332	29.460429
365.919154	18390.439724	29.465447
366.500104	18417.772449	29.470464
366.528649	18446.892549	29.475482
366.457329	18473.414149	29.480500
366.909788	18500.735135	29.485517
367.066666	18527.242768	29.490535
367.531290	18548.244075	29.495552
367.567210	18578.299502	29.500570
367.701541	18615.389483	29.505588
368.333027	18648.376286	29.510605
368.730305	18672.957612	29.515623
369.368287	18695.470511	29.520640
369.696964	18733.496500	29.525658
370.145615	18755.768058	29.530676
370.356346	18781.305654	29.535693
370.460338	18817.843086	29.540711
371.044138	18852.037747	29.545728
371.014697	18888.077192	29.550746
371.714490	18919.242061	29.555764
372.249208	18949.737522	29.560781
372.488707	18995.107178	29.565799
372.954975	19024.157557	29.570816
372.722003	19057.877529	29.575834
373.802486	19087.447628	29.580852
374.211803	19106.556141	29.585869
374.721048	19138.055557	29.590887
375.479939	19160.965272	29.595904
375.824970	19187.936274	29.600922
376.406273	19212.560513	29.605940
376.263473	19254.007442	29.610957
376.615862	19275.250479	29.615975
377.508633	19294.816882	29.620992
377.550478	19330.558613	29.626010
377.754342	19347.715130	29.631028
378.305455	19379.214393	29.636045
378.477568	19409.106951	29.641063
378.468448	19443.993495	29.646080
378.885026	19483.986604	29.651098
378.824932	19520.899491	29.656116
379.806829	19557.454313	29.661133
380.236196	19591.461622	29.666151
380.944551	19618.321283	29.671168
380.912632	19662.895807	29.676186
381.576329	19687.631675	29.681204
382.329411	19702.821920	29.686221
382.551928	19729.650096	29.691239
382.863798	19760.360418	29.696256
382.658458	19794.261754	29.701274
383.028465	19837.909632	29.706292
383.851469	19867.630857	29.711309
383.995911	19915.876761	29.716327
384.485915	19947.259506	29.721344
384.354018	19975.048336	29.726362
384.579298	20022.551311	29.731380
385.096965	20057.278024	29.736397
385.471619	20108.235748	29.741415
386.248117	20134.823299	29.746432
386.707977	20178.427274	29.751450
387.669244	20209.027993	29.756468
388.368580	20237.174947	29.761485
388.573736	20269.924841	29.766503
389.358668	20285.029961	29.771520
389.519401	20315.931801	29.776538
389.367844	20331.434439	29.781556
389.939359	20357.578543	29.786573
389.959851	20398.911483	29.791591
390.689961	20425.702644	29.796608
390.894888	20447.012525	29.801626
391.068949	20489.274082	29.806644
391.618229	20517.247662	29.811661
391.909027	20545.812603	29.816679
392.340300	20566.784139	29.821696
392.983781	20608.519156	29.826714
393.021516	20645.399448	29.831732
393.507073	20662.848154	29.836749
394.128557	20704.774646	29.841767
394.544469	20722.256989	29.846784
395.411173	20742.907732	29.851802
395.471623	20760.989573	29.856820
395.841533	20787.941716	29.861837
396.088012	20809.409151	29.866855
396.151272	20835.664766	29.871872
396.767585	20865.362011	29.876890
396.762020	20888.491832	29.881908
397.448545	20931.010375	29.886925
397.371922	20960.133320	29.891943
397.779358	20992.703023	29.896960
398.233041	21030.420373	29.901978
398.380116	21071.831807	29.906996
398.719644	21116.462355	29.912013
399.051627	21165.194832	29.917031
399.419040	21197.855102	29.922048
399.643864	21246.405297	29.927066
399.940345	21284.869668	29.932084
401.060445	21335.334349	29.937101
401.039116	21385.853730	29.942119
401.910702	21426.254026	29.947136
402.101420	21468.477463	29.952154
402.374236	21506.151664	29.957172
402.916371	21541.824937	29.962189
403.529113	21592.593348	29.967207
404.000177	21621.850841	29.972224
404.792989	21651.906587	29.977242
405.002332	21704.802566	29.982260
405.759440	21732.228306	29.987277
405.856219	21769.538030	29.992295
406.647947	21795.513998	29.997312
406.997169	21829.947441	30.002330
407.027892	21866.941938	30.007348
407.439455	21903.496797	30.012365
408.041583	21940.094356	30.017383
409.262312	21953.880332	30.022400
409.626530	21974.527317	30.027418
409.817126	22013.445994	30.032436
410.438705	22030.146839	30.037453
410.858404	22059.489258	30.042471
411.084953	22071.347389	30.047488
411.333453	22098.397374	30.052506
411.782067	22133.975416	30.057524
412.285527	22153.708827	30.062541
412.397145	22199.142989	30.067559
413.080493	22216.618979	30.072576
413.202366	22240.778070	30.077594
413.378278	22274.859509	30.082612
413.771192	22309.097520	30.087629
413.796330	22345.632036	30.092647
414.237876	22391.611340	30.097664
414.947681	22420.971110	30.102682
414.858652	22482.268770	30.107700
415.401496	22514.063838	30.112717
415.906768	22554.339741	30.117735
416.135081	22587.443507	30.122752
416.559615	22637.853576	30.127770
417.191886	22672.183649	30.132788
417.943957	22708.606753	30.137805
418.052568	22752.228144	30.142823
418.576159	22794.724718	30.147840
419.351881	22832.935299	30.152858
419.412459	22883.354192	30.157876
420.079531	22899.080298	30.162893
420.240171	22941.969881	30.167911
420.708549	22989.081608	30.172928
421.090287	23011.592213	30.177946
421.379979	23049.888303	30.182964
421.933545	23078.224940	30.187981
422.582413	23113.261115	30.192999
422.668551	23144.081146	30.198016
423.311937	23184.878131	30.203034
423.719143	23223.320759	30.208052
424.002859	23241.991192	30.213069
424.058139	23280.676560	30.218087
424.537434	23313.814397	30.223104
425.258874	23346.336790	30.228122
426.634951	23366.257017	30.233140
427.885814	23371.259908	30.238157
427.715707	23385.171180	30.243175
428.049359	23410.753872	30.248192
428.665840	23436.244156	30.253210
428.764514	23446.801490	30.258228
429.491395	23475.570576	30.263245
429.617289	23494.295740	30.268263
429.929932	23515.057200	30.273280
430.426698	23558.730081	30.278298
430.622830	23583.883221	30.283316
431.459314	23594.834371	30.288333
431.111727	23630.911326	30.293351
431.317438	23662.592384	30.298368
431.944662	23700.835770	30.303386
431.994487	23749.067307	30.308404
432.552719	23782.823735	30.313421
432.691563	23823.054396	30.318439
433.288065	23869.281758	30.323456
433.599665	23918.731964	30.328474
433.920855	23960.347212	30.333492
434.395416	23995.603226	30.338509
434.875656	24056.367890	30.343527
434.900288	24108.981819	30.348544
435.648975	24149.386881	30.353562
436.186836	24208.608333	30.358580
436.963479	24239.180687	30.363597
437.332371	24273.246889	30.368615
437.726365	24319.969363	30.373632
438.536781	24358.679097	30.378650
439.357297	24391.973976	30.383668
439.793763	24423.448038	30.388685
440.247072	24457.139569	30.393703
440.526726	24493.486875	30.398720
440.999647	24516.913184	30.403738
441.343676	24558.059377	30.408756
441.901909	24594.416071	30.413773
442.340709	24622.682797	30.418791
442.653773	24670.263221	30.423808
443.148147	24689.887568	30.428826
443.305037	24734.354436	30.433844
444.048899	24767.465606	30.438861
444.339144	24814.875172	30.443879
444.496804	24854.671525	30.448896
445.150141	24886.905369	30.453914
445.661991	24932.028446	30.458932
445.807328	24961.167344	30.463949
446.232389	25000.385303	30.468967
446.183330	25051.798534	30.473984
446.928331	25100.420522	30.479002
447.272150	25138.400159	30.484020
447.468649	25199.695157	30.489037
448.372940	25251.191200	30.494055
448.679771	25297.077644	30.499072
449.214781	25344.749443	30.504090
449.168517	25378.536358	30.509108
449.903130	25427.298187	30.514125
450.174791	25473.233491	30.519143
450.611390	25524.957425	30.524160
451.286555	25571.343576	30.529178
451.576814	25620.348091	30.534196
451.919701	25660.074724	30.539213
452.354663	25701.533508	30.544231
453.117143	25740.935553	30.549248
453.714029	25775.861236	30.554266
454.186816	25822.827130	30.559284
454.752278	25860.416944	30.564301
455.057587	25893.643748	30.569319
455.506430	25934.807488	30.574336
456.157207	25983.744030	30.579354
456.425439	26032.661899	30.584372
457.272831	26061.406003	30.589389
458.642529	26088.543659	30.594407
458.982995	26107.411299	30.599424
459.272349	26143.782597	30.604442
459.995806	26174.446067	30.609460
460.182383	26199.152050	30.614477
460.882036	26229.542000	30.619495
461.059273	26255.328278	30.624512
461.480330	26278.995822	30.629530
461.880214	26314.339938	30.634548
461.827832	26349.424506	30.639565
462.602838	26385.220912	30.644583
462.678541	26428.702614	30.649600
463.226319	26481.653772	30.654618
463.344785	26516.461290	30.659636
463.795295	26566.615353	30.664653
464.162034	26612.970117	30.669671
464.471411	26664.295864	30.674688
465.349052	26709.768514	30.679706
465.862254	26754.222779	30.684724
466.523904	26801.418796	30.689741
467.335680	26834.469143	30.694759
467.830940	26872.000231	30.699776
468.099157	26905.030105	30.704794
468.555883	26941.962117	30.709812
469.064315	26978.992909	30.714829
469.398314	27018.534912	30.719847
468.980904	27066.225313	30.724864
469.913423	27116.594701	30.729882
470.248611	27171.239042	30.734900
470.779281	27215.079703	30.739917
471.388620	27271.735610	30.744935
471.867772	27318.389129	30.749952
472.319211	27364.943263	30.754970
472.857182	27417.820070	30.759988
473.423879	27465.759069	30.765005
474.115595	27506.671975	30.770023
474.526014	27545.874526	30.775040
475.116522	27587.081915	30.780058
475.731954	27631.344924	30.785076
475.864454	27673.921423	30.790093
476.444106	27715.641906	30.795111
477.087373	27755.046196	30.800128
477.515374	27794.407277	30.805146
478.238006	27846.220288	30.810164
478.531428	27890.833658	30.815181
479.182980	27917.379974	30.820199
479.596939	27957.298906	30.825216
480.305167	27994.279954	30.830234
480.604363	28031.745019	30.835252
481.025161	28071.511677	30.840269
481.601872	28108.789124	30.845287
481.718531	28144.764186	30.850304
482.551797	28181.406392	30.855322
482.891721	28210.742626	30.860340
483.324853	28249.368928	30.865357
483.495417	28284.669804	30.870375
483.579353	28337.381541	30.875392
484.199670	28380.352363	30.880410
484.606625	28423.251286	30.885428
484.927102	28468.666053	30.890445
485.917978	28511.440353	30.895463
486.198503	28565.095028	30.900480
486.438209	28604.381806	30.905498
486.800963	28646.973140	30.910516
487.008770	28711.952147	30.915533
487.690570	28760.008216	30.920551
488.123362	28820.855964	30.925568
488.984293	28863.469640	30.930586
490.290215	28891.981870	30.935604
490.916008	28924.145840	30.940621
491.374446	28950.615238	30.945639
491.773013	29005.614526	30.950656
492.228468	29041.390381	30.955674
492.433861	29086.440926	30.960692
493.131355	29130.527032	30.965709
493.860880	29163.078093	30.970727
493.915290	29209.513504	30.975744
494.581842	29250.422082	30.980762
494.820680	29299.975524	30.985780
495.371803	29344.209379	30.990797
495.910766	29387.735573	30.995815
496.082933	29435.619020	31.000832
496.871563	29485.473347	31.005850
497.191149	29524.944601	31.010868
497.313609	29579.896675	31.015885
497.880545	29624.422011	31.020903
498.920449	29673.083933	31.025920
499.305637	29720.958217	31.030938
499.723825	29771.455008	31.035956
500.089212	29824.459162	31.040973
500.688664	29871.080766	31.045991
501.085386	29922.534253	31.051008
501.488220	29973.021547	31.056026
502.317818	30030.053904	31.061044
502.567106	30085.797383	31.066061
503.138542	30128.638651	31.071079
503.656065	30182.366433	31.076096
504.059981	30238.879852	31.081114
504.843446	30291.201195	31.086132
505.096736	30351.733772	31.091149
505.614551	30398.013783	31.096167
506.006870	30464.451598	31.101184
507.012770	30506.193573	31.106202
507.273816	30542.859576	31.111220
507.923857	30594.042902	31.116237
508.871360	30619.992389	31.121255
509.337972	30664.934462	31.126272
510.288978	30702.650965	31.131290
510.508008	30748.129454	31.136308
510.496272	30793.217120	31.141325
511.347602	30833.341738	31.146343
511.339530	30891.695189	31.151360
511.964020	30934.255199	31.156378
512.514539	31000.230394	31.161396
512.364274	31040.561939	31.166413
513.039316	31091.853015	31.171431
513.623843	31153.829076	31.176448
514.012766	31211.411319	31.181466
514.678682	31262.347896	31.186484
514.991798	31324.277898	31.191501
515.637201	31358.616881	31.196519
516.509916	31420.606229	31.201536
516.907677	31464.012646	31.206554
517.829727	31513.935920	31.211572
518.411706	31553.008752	31.216589
518.710960	31588.112075	31.221607
519.305413	31634.603549	31.226624
519.829933	31675.582294	31.231642
520.583186	31714.475755	31.236660
520.310718	31752.245170	31.241677
521.135995	31803.220098	31.246695
521.218005	31866.070434	31.251712
522.055469	31914.535422	31.256730
522.510321	31959.814039	31.261748
522.753350	32017.441955	31.266765
523.046777	32069.360524	31.271783
523.625443	32142.828657	31.276800
524.050046	32206.197845	31.281818
524.795185	32257.575405	31.286836
524.931796	32316.007496	31.291853
525.591010	32379.243902	31.296871
525.961199	32450.428737	31.301888
526.130624	32514.166160	31.306906
526.738639	32575.401898	31.311924
527.076753	32649.735373	31.316941
527.843056	32725.528702	31.321959
528.410265	32791.186035	31.326976
529.345321	32860.105291	31.331994
529.843452	32920.227655	31.337012
529.970573	32999.904537	31.342029
530.655109	33057.503944	31.347047
531.438610	33136.773279	31.352064
532.081775	33203.476611	31.357082
532.709542	33255.873534	31.362100
532.903305	33331.076178	31.367117
533.526420	33381.596841	31.372135
534.626286	33443.123519	31.377152
535.398361	33502.893397	31.382170
536.413635	33550.178668	31.387188
536.897041	33611.754114	31.392205
537.622944	33653.934782	31.397223
538.335097	33700.683628	31.402240
538.417563	33759.353461	31.407258
539.202042	33792.702371	31.412276
539.282359	33852.237440	31.417293
539.891187	33916.468998	31.422311
540.385424	33972.815415	31.427328
540.860216	34020.825453	31.432346
541.562298	34080.943317	31.437364
541.959863	34119.165622	31.442381
543.361505	34164.252490	31.447399
544.089519	34205.194035	31.452416
544.364691	34252.139575	31.457434
545.313942	34282.950450	31.462452
545.579120	34329.250974	31.467469
546.050948	34371.727755	31.472487
546.431101	34421.994902	31.477504
546.859179	34477.965725	31.482522
546.992020	34515.509998	31.487540
547.309714	34570.931355	31.492557
547.948099	34625.839210	31.497575
548.408704	34685.490966	31.502592
548.711365	34756.197645	31.507610
549.249934	34796.461845	31.512628
549.745225	34876.619629	31.517645
550.513603	34929.506319	31.522663
551.079404	34984.667093	31.527680
551.574315	35053.127973	31.532698
552.305789	35098.138574	31.537716
552.234777	35158.394083	31.542733
552.853202	35213.269178	31.547751
553.373368	35261.180402	31.552768
553.798553	35333.528997	31.557786
554.454876	35396.552596	31.562804
554.726380	35469.185887	31.567821
555.145555	35522.573809	31.572839
555.692870	35592.530207	31.577856
555.932296	35665.276885	31.582874
556.561407	35721.530822	31.587892
557.407175	35790.567722	31.592909
557.806837	35866.513909	31.597927
558.613064	35919.381504	31.602944
559.026090	36014.165964	31.607962
560.173276	36068.079047	31.612980
560.370070	36140.667442	31.617997
561.290276	36203.192710	31.623015
561.896761	36262.336488	31.628032
562.230094	36327.613161	31.633050
563.080679	36383.337133	31.638068
563.369939	36468.336105	31.643085
563.882919	36543.142960	31.648103
564.580019	36595.339441	31.653120
564.919252	36658.864835	31.658138
565.752507	36726.193764	31.663156
566.421530	36793.344936	31.668173
567.058281	36862.019687	31.673191
567.827712	36916.313309	31.678208
568.580530	36968.984532	31.683226
569.224325	37029.232408	31.688244
569.428874	37098.386564	31.693261
570.263903	37168.329991	31.698279
570.754586	37221.919454	31.703296
571.234375	37295.368381	31.708314
571.560762	37364.979991	31.713332
572.372843	37430.465634	31.718349
572.866742	37494.669069	31.723367
573.851837	37544.501059	31.728384
574.125990	37615.413082	31.733402
574.938613	37673.078828	31.738420
575.336048	37735.563219	31.743437
575.752827	37801.762496	31.748455
576.446334	37860.442681	31.753472
576.903724	37943.129517	31.758490
577.424455	38006.105769	31.763508
578.117691	38072.386622	31.768525
578.697104	38146.169730	31.773543
579.291824	38190.860348	31.778560
579.754155	38270.382246	31.783578
580.047051	38333.015370	31.788596
580.967643	38398.805379	31.793613
581.389889	38472.382217	31.798631
582.273965	38537.194026	31.803648
582.193206	38608.380025	31.808666
583.220862	38685.714642	31.813684
583.956662	38761.573325	31.818701
584.012589	38825.566602	31.823719
584.743867	38894.722692	31.828736
585.550618	38974.613733	31.833754
586.207249	39039.616406	31.838772
586.961039	39105.471250	31.843789
587.064782	39165.465095	31.848807
588.226484	39224.984551	31.853824
588.673599	39307.341578	31.858842
589.581021	39354.237050	31.863860
590.560394	39413.380069	31.868877
590.636790	39481.945844	31.873895
591.449519	39533.841336	31.878912
591.873458	39604.101963	31.883930
592.289489	39656.350556	31.888948
592.769706	39710.113245	31.893965
593.221612	39775.979344	31.898983
593.868259	39849.139609	31.904000
593.939713	39907.007476	31.909018
594.486139	39964.490903	31.914036
594.892836	40038.073487	31.919053
595.613073	40113.507944	31.924071
596.334385	40175.192839	31.929088
597.766853	40237.660092	31.934106
598.655271	40289.974523	31.939124
599.565024	40352.092902	31.944141
600.150864	40396.001283	31.949159
600.959668	40451.208084	31.954176
600.924274	40505.828474	31.959194
601.406365	40563.176054	31.964212
602.499527	40625.703834	31.969229
602.473640	40692.567558	31.974247
603.263142	40753.741249	31.979264
603.767256	40806.931878	31.984282
604.026649	40873.013655	31.989300
604.675229	40931.827972	31.994317
604.955820	41005.047010	31.999335
605.651497	41078.832271	32.004352
605.997704	41163.373482	32.009370
606.521118	41226.909692	32.014388
607.536199	41298.973206	32.019405
607.839215	41383.699338	32.024423
608.771174	41451.351482	32.029440
609.180186	41530.583888	32.034458
609.956833	41596.926924	32.039476
610.763793	41671.602173	32.044493
611.185152	41739.156616	32.049511
612.066144	41814.647292	32.054528
612.380166	41902.821198	32.059546
612.809103	41975.656570	32.064564
613.634823	42055.759984	32.069581
614.045873	42132.882734	32.074599
614.692546	42204.865432	32.079616
615.338146	42288.371115	32.084634
615.955578	42362.218646	32.089652
616.624925	42429.699938	32.094669
617.163082	42524.093579	32.099687
617.943125	42592.854671	32.104704
618.392709	42676.081947	32.109722
619.220418	42758.644173	32.114740
619.891177	42831.190428	32.119757
620.751864	42906.884661	32.124775
621.954926	42956.626003	32.129792
622.575676	43028.041624	32.134810
622.884231	43094.533656	32.139828
623.737003	43161.820008	32.144845
624.262675	43232.402885	32.149863
624.551447	43300.149102	32.154880
625.193368	43371.581493	32.159898
625.977359	43448.307176	32.164916
626.701088	43511.976029	32.169933
627.237063	43581.327277	32.174951
627.719292	43647.372717	32.179968
628.368843	43719.553419	32.184986
628.845591	43800.931201	32.190004
629.506631	43865.606112	32.195021
629.775438	43948.458531	32.200039
630.393635	44010.706868	32.205056
631.029488	44096.637536	32.210074
631.745856	44176.285146	32.215092
632.865809	44248.980607	32.220109
632.796377	44320.862481	32.225127
633.431395	44393.711213	32.230144
634.208163	44473.148056	32.235162
634.627102	44555.005952	32.240180
635.196991	44630.152208	32.245197
635.702915	44701.034391	32.250215
636.655830	44772.783890	32.255232
637.255844	44846.985175	32.260250
637.638473	44918.119028	32.265268
638.359219	44987.669168	32.270285
639.272630	45075.888610	32.275303
640.409684	45130.897331	32.280320
641.050319	45199.754248	32.285338
641.315932	45291.311665	32.290356
642.164514	45358.401429	32.295373
642.697857	45440.604252	32.300391
643.906792	45517.934492	32.305408
643.985337	45589.051653	32.310426
643.904191	45656.176050	32.315444
644.837544	45729.394343	32.320461
645.106894	45819.131877	32.325479
645.908371	45892.028423	32.330496
647.042920	45982.987877	32.335514
647.631976	46072.898005	32.340532
648.312420	46157.299397	32.345549
648.629038	46238.316393	32.350567
649.778527	46307.787999	32.355584
650.399288	46380.321595	32.360602
650.821077	46466.235353	32.365620
652.122319	46543.785083	32.370637
652.798710	46616.960866	32.375655
653.673372	46698.901270	32.380672
653.676670	46775.823234	32.385690
654.374614	46852.905504	32.390708
655.468580	46927.557611	32.395725
655.558446	47009.310054	32.400743
656.407148	47084.319053	32.405760
657.110575	47159.497597	32.410778
657.854408	47253.748560	32.415796
659.008470	47315.758341	32.420813
660.519251	47373.939101	32.425831
661.734207	47422.727297	32.430848
663.012580	47475.843873	32.435866
663.440224	47517.505870	32.440884
663.998140	47555.252942	32.445901
664.235100	47616.388905	32.450919
664.636051	47665.618466	32.455936
665.347555	47720.635592	32.460954
665.555623	47776.067587	32.465972
665.903374	47839.822724	32.470989
666.501085	47918.650055	32.476007
667.109470	47984.342580	32.481024
667.523496	48052.881057	32.486042
667.924483	48129.206015	32.491060
668.898915	48212.718591	32.496077
669.043554	48285.565504	32.501095
669.759728	48361.953028	32.506112
670.961779	48425.932205	32.511130
671.308886	48513.032860	32.516148
671.875154	48592.123972	32.521165
672.671220	48662.897365	32.526183
673.587795	48740.892284	32.531200
674.434258	48812.902143	32.536218
674.989115	48889.027897	32.541236
675.774963	48948.327986	32.546253
675.989045	49032.506594	32.551271
676.482120	49100.562096	32.556288
677.719819	49182.285923	32.561306
677.757527	49260.083889	32.566324
678.291521	49325.853339	32.571341
678.746917	49410.622213	32.576359
679.354597	49490.708163	32.581376
679.850649	49568.636965	32.586394
680.278422	49670.841012	32.591412
680.679464	49741.869978	32.596429
681.207905	49842.251876	32.601447
681.580013	49944.352884	32.606464
682.596912	50037.410360	32.611482
682.984272	50143.069152	32.616500
683.948208	50251.412516	32.621517
684.642288	50348.134631	32.626535
685.044747	50442.738851	32.631552
686.305660	50535.376303	32.636570
686.882394	50639.089501	32.641588
687.622591	50733.329867	32.646605
688.513730	50823.822148	32.651623
689.558356	50917.406751	32.656640
690.397977	51007.744175	32.661658
690.733430	51115.450845	32.666676
691.826992	51190.792479	32.671693
693.161853	51277.802603	32.676711
693.876083	51365.294621	32.681728
695.294871	51433.732981	32.686746
695.743295	51501.687523	32.691764
697.172571	51574.855936	32.696781
697.790447	51641.525940	32.701799
698.407042	51703.433470	32.706816
698.832894	51763.771370	32.711834
699.372548	51842.476018	32.716852
699.890257	51915.158256	32.721869
700.531749	52001.783962	32.726887
700.735079	52084.275302	32.731904
701.553695	52163.424755	32.736922
701.857234	52256.462328	32.741940
702.300096	52347.563267	32.746957
702.603780	52441.820902	32.751975
703.084543	52537.129981	32.756992
704.291760	52632.957593	32.762010
704.759790	52735.433418	32.767028
705.557970	52826.579004	32.772045
706.264739	52939.837898	32.777063
707.062353	53034.888626	32.782080
707.717829	53125.762270	32.787098
708.355212	53222.179648	32.792116
709.514769	53324.020036	32.797133
710.331525	53426.498771	32.802151
710.284542	53529.815605	32.807168
711.250258	53624.077040	32.812186
711.914092	53722.116121	32.817204
713.085083	53807.632687	32.822221
713.420860	53905.196190	32.827239
714.234803	54016.440975	32.832256
715.267764	54100.509616	32.837274
715.573740	54215.130911	32.842292
716.875294	54305.018885	32.847309
717.559637	54396.613905	32.852327
718.115830	54509.925740	32.857344
718.932541	54584.921950	32.862362
719.542593	54688.654464	32.867380
720.039753	54775.335306	32.872397
720.789333	54868.867663	32.877415
721.393861	54977.309444	32.882432
722.316263	55070.719455	32.887450
723.145267	55181.576661	32.892468
724.029600	55271.683289	32.897485
724.733051	55371.265685	32.902503
725.411208	55467.017687	32.907520
726.043869	55541.965816	32.912538
726.554599	55631.276527	32.917556
727.360987	55719.907001	32.922573
728.469276	55801.601192	32.927591
728.870524	55889.610653	32.932608
729.845714	55970.019651	32.937626
730.653812	56051.454859	32.942644
731.146534	56141.086768	32.947661
731.913925	56237.421699	32.952679
732.544608	56332.655008	32.957696
733.385063	56423.854594	32.962714
733.920904	56520.191232	32.967732
734.367846	56604.626427	32.972749
735.178133	56702.106498	32.977767
736.059377	56791.892026	32.982784
737.285468	56890.504876	32.987802
738.070810	56988.912985	32.992820
738.812576	57068.233980	32.997837
739.825551	57157.765626	33.002855
741.028239	57237.263927	33.007872
742.213164	57322.610255	33.012890
742.467434	57402.922982	33.017908
743.084815	57479.732365	33.022925
743.912760	57557.556186	33.027943
744.159540	57650.818273	33.032960
745.168927	57730.988672	33.037978
746.068682	57819.486761	33.042996
746.821578	57892.863194	33.048013
747.770309	57982.712476	33.053031
748.258464	58084.144965	33.058048
749.070311	58166.599276	33.063066
749.496554	58252.921624	33.068084
750.137245	58338.697093	33.073101
751.449956	58422.030238	33.078119
751.959157	58501.496461	33.083136
753.038254	58589.519704	33.088154
753.822250	58687.538339	33.093172
754.648467	58766.473014	33.098189
755.382769	58845.088265	33.103207
755.815108	58932.903866	33.108224
757.253415	58998.986271	33.113242
758.342636	59078.434838	33.118260
758.787369	59151.639297	33.123277
759.455322	59224.598626	33.128295
759.991938	59318.471524	33.133312
760.826027	59394.633203	33.138330
761.647461	59482.949383	33.143348
762.345283	59569.769712	33.148365
762.693169	59643.743966	33.153383
763.256365	59734.897077	33.158400
763.745135	59832.603539	33.163418
764.278781	59938.347788	33.168436
764.674528	60033.252089	33.173453
765.696347	60131.048923	33.178471
765.828551	60251.187556	33.183488
766.515137	60352.668274	33.188506
767.002130	60479.600160	33.193524
767.527627	60587.807514	33.198541
768.851045	60697.153951	33.203559
769.878338	60818.487935	33.208576
770.361544	60928.972900	33.213594
770.899313	61041.288532	33.218612
771.740632	61164.892531	33.223629
772.441529	61268.372568	33.228647
773.489351	61396.178223	33.233664
774.150090	61499.659753	33.238682
775.125869	61620.191772	33.243700
775.681259	61736.824926	33.248717
776.812532	61841.576674	33.253735
777.667059	61937.551765	33.258752
778.412738	62034.885157	33.263770
779.001476	62135.354462	33.268788
780.039842	62236.824452	33.273805
780.789595	62344.296283	33.278823
781.626722	62436.958473	33.283840
782.942921	62532.670529	33.288858
783.729737	62637.363171	33.293876
784.195040	62747.412236	33.298893
784.795975	62839.502182	33.303911
785.060784	62955.090547	33.308928
785.556423	63063.271774	33.313946
786.753359	63163.057905	33.318964
787.266416	63298.693789	33.323981
787.746530	63415.873583	33.328999
788.544160	63541.123610	33.334016
789.319159	63667.281994	33.339034
790.155861	63794.530767	33.344052
790.315602	63912.455255	33.349069
791.283122	64046.466136	33.354087
792.152654	64173.831931	33.359104
792.852118	64319.734069	33.364122
793.790790	64451.470522	33.369140
794.361095	64583.161191	33.374157
795.843537	64713.286180	33.379175
796.693698	64838.092965	33.384192
797.886217	64972.186496	33.389210
798.551515	65093.852182	33.394228
799.378898	65221.882486	33.399245
800.879012	65327.223271	33.404263
801.478364	65452.492381	33.409280
802.394716	65567.646483	33.414298
803.472728	65693.173035	33.419316
804.266718	65787.804417	33.424333
805.829527	65890.090847	33.429351
806.568250	65989.075036	33.434368
808.050420	66076.495203	33.439386
809.139905	66151.148096	33.444404
810.026910	66252.201446	33.449421
810.470092	66331.355118	33.454439
811.215967	66431.680388	33.459456
812.297573	66523.897071	33.464474
813.268782	66628.731266	33.469492
813.403751	66720.011501	33.474509
814.195464	66813.061211	33.479527
815.155698	66920.003784	33.484544
815.697571	67019.012735	33.489562
816.561106	67101.842360	33.494580
816.890227	67200.779835	33.499597
817.706654	67306.901024	33.504615
818.366822	67420.343914	33.509632
818.927112	67521.665986	33.514650
819.973965	67631.309965	33.519668
820.425153	67754.145537	33.524685
821.671097	67864.782012	33.529703
822.343387	67986.248506	33.534720
822.894160	68100.256831	33.539738
823.929326	68207.199933	33.544756
824.009187	68327.192035	33.549773
824.936079	68446.242046	33.554791
825.859159	68573.474223	33.559808
826.502204	68694.222590	33.564826
827.586419	68822.921703	33.569844
828.137270	68951.703352	33.574861
829.089192	69075.374363	33.579879
829.826701	69187.562207	33.584896
830.252059	69298.291144	33.589914
831.164114	69423.582982	33.594932
831.870489	69544.610264	33.599949
832.543550	69662.906106	33.604967
833.434269	69781.558665	33.609984
834.360760	69901.148041	33.615002
835.853696	70013.575914	33.620020
837.270616	70118.474057	33.625037
838.865223	70212.405210	33.630055
839.912819	70313.148101	33.635072
840.605562	70410.150121	33.640090
841.431115	70498.171351	33.645108
842.062793	70608.443119	33.650125
842.785254	70708.533422	33.655143
843.327013	70812.510953	33.660160
844.214007	70922.362820	33.665178
844.873668	71027.011120	33.670196
845.528271	71139.007995	33.675213
846.650299	71245.623324	33.680231
847.565974	71366.544226	33.685248
847.793106	71474.541444	33.690266
849.129978	71587.907603	33.695284
849.307356	71717.437929	33.700301
850.350648	71825.611986	33.705319
850.687218	71954.782335	33.710336
851.658900	72087.250471	33.715354
851.997792	72217.383142	33.720372
852.844865	72368.463904	33.725389
853.893746	72489.944570	33.730407
855.411552	72602.698154	33.735424
856.818583	72722.217670	33.740442
858.199162	72827.337480	33.745460
858.722844	72958.474840	33.750477
859.436807	73071.565964	33.755495
860.446099	73186.613472	33.760512
861.641008	73307.315819	33.765530
862.424871	73425.279040	33.770548
862.887377	73539.811651	33.775565
864.007967	73656.474780	33.780583
865.177121	73770.373392	33.785600
865.730139	73900.095118	33.790618
866.332443	73997.020789	33.795636
867.118597	74128.653104	33.800653
867.826176	74258.832062	33.805671
868.378077	74376.358153	33.810688
869.344061	74510.606467	33.815706
870.679389	74634.436009	33.820724
871.438936	74758.626935	33.825741
872.040731	74886.088835	33.830759
873.117274	75011.575877	33.835776
873.683388	75144.521808	33.840794
874.650984	75260.238585	33.845812
875.898737	75380.646510	33.850829
877.439389	75496.200353	33.855847
878.683505	75616.559588	33.860864
879.123686	75735.110680	33.865882
880.058629	75843.291099	33.870900
880.766405	75958.244965	33.875917
881.702470	76070.815403	33.880935
882.699854	76187.512446	33.885952
883.169113	76307.421577	33.890970
884.317196	76424.702144	33.895988
884.897896	76529.541882	33.901005
885.739225	76663.887254	33.906023
886.474396	76789.807683	33.911040
886.773027	76921.777657	33.916058
887.739268	77047.990287	33.921076
888.481777	77181.830191	33.926093
889.351230	77311.001282	33.931111
889.933396	77423.403064	33.936128
890.517613	77560.515993	33.941146
891.458265	77697.083908	33.946164
892.158581	77832.699346	33.951181
892.642682	77963.101648	33.956199
893.933784	78108.696793	33.961216
894.758495	78240.809148	33.966234
896.259278	78367.187724	33.971252
897.268619	78503.806195	33.976269
898.513831	78631.069704	33.981287
900.011517	78745.572434	33.986304
900.824822	78870.878266	33.991322
902.052065	78990.721069	33.996340
902.664564	79123.746586	34.001357
903.433833	79230.427597	34.006375
904.002450	79352.575958	34.011392
904.979892	79485.170181	34.016410
906.040130	79591.444331	34.021428
906.627460	79738.172073	34.026445
907.189209	79877.940688	34.031463
908.419091	80020.243910	34.036480
908.971483	80150.540200	34.041498
910.250464	80280.344072	34.046516
911.229326	80425.398650	34.051533
912.031795	80550.911778	34.056551
913.591814	80675.092325	34.061568
914.751506	80805.197257	34.066586
915.945041	80933.279444	34.071604
917.042036	81053.844303	34.076621
917.656406	81184.775256	34.081639
918.428694	81295.956918	34.086656
918.957025	81441.984375	34.091674
919.997809	81571.809723	34.096692
920.734640	81702.356552	34.101709
921.323899	81838.583936	34.106727
922.171714	81981.494019	34.111744
922.605555	82121.379905	34.116762
924.166283	82248.010857	34.121780
925.338115	82397.259430	34.126797
925.756767	82529.476722	34.131815
927.046226	82673.842856	34.136832
927.765517	82822.068173	34.141850
928.961273	82964.053965	34.146868
929.615173	83103.605895	34.151885
930.631101	83251.380140	34.156903
931.690721	83393.884544	34.161920
932.535783	83543.137639	34.166938
933.128371	83675.997137	34.171956
934.209349	83834.298038	34.176973
934.885260	83980.190883	34.181991
935.858967	84138.587516	34.187008
936.169483	84297.025146	34.192026
937.178485	84444.491901	34.197044
938.405155	84607.873415	34.202061
939.089405	84771.225437	34.207079
940.132295	84920.625650	34.212096
941.232956	85080.045407	34.217114
941.874089	85237.270769	34.222132
943.346152	85399.567110	34.227149
944.511317	85550.678478	34.232167
945.819562	85688.100770	34.237184
947.081342	85836.293935	34.242202
948.185636	85971.739568	34.247220
949.468556	86093.369607	34.252237
950.566027	86241.579837	34.257255
951.976356	86347.701182	34.262272
953.017997	86477.383349	34.267290
954.369009	86586.577979	34.272308
954.827655	86699.596632	34.277325
955.813394	86808.783011	34.282343
956.501470	86915.614641	34.287360
956.830638	87035.319038	34.292378
957.532851	87170.312863	34.297396
958.266290	87298.620481	34.302413
959.049103	87438.322856	34.307431
959.765542	87565.691943	34.312448
960.296281	87729.589997	34.317466
960.975422	87874.620954	34.322484
961.562183	88020.332466	34.327501
962.291578	88181.347088	34.332519
963.096046	88339.129583	34.337536
964.130480	88510.720429	34.342554
965.415374	88664.274737	34.347572
966.548312	88818.101922	34.352589
967.637226	88986.510633	34.357607
968.428271	89148.205104	34.362624
969.651190	89320.549066	34.367642
970.624500	89480.386913	34.372660
971.912363	89643.122811	34.377677
972.708077	89809.934153	34.382695
973.933740	89969.379257	34.387712
974.929247	90131.135274	34.392730
975.604011	90295.862689	34.397748
976.399880	90453.996107	34.402765
977.477440	90634.442240	34.407783
978.712033	90793.853426	34.412800
979.269617	90958.940176	34.417818
980.407986	91128.855763	34.422836
981.638439	91294.738719	34.427853
983.076150	91472.258554	34.432871
984.559319	91598.997472	34.437888
985.915498	91758.698792	34.442906
987.169562	91898.792670	34.447924
988.300654	92032.642201	34.452941
988.992237	92197.417906	34.457959
989.978605	92355.905835	34.462976
990.589454	92503.539487	34.467994
991.552748	92656.856182	34.473012
992.708130	92796.022238	34.478029
993.557685	92957.416380	34.483047
994.429311	93114.010544	34.488064
995.199204	93272.154154	34.493082
995.795124	93441.643987	34.498100
996.783095	93607.532273	34.503117
997.560419	93782.589520	34.508135
998.628520	93947.859297	34.513152
999.524083	94129.659165	34.518170
1000.513881	94310.894179	34.523188
1001.483867	94471.930389	34.528205
1002.065779	94654.210019	34.533223
1003.124873	94834.298180	34.538240
1003.894497	95019.638331	34.543258
1005.141120	95208.515325	34.548276
1005.860818	95398.012455	34.553293
1006.823863	95592.977693	34.558311
1007.875959	95778.125025	34.563328
1008.971287	95969.127986	34.568346
1009.880938	96155.922099	34.573364
1011.548481	96341.421478	34.578381
1012.172568	96520.498744	34.583399
1013.574264	96698.815932	34.588416
1014.664720	96875.831169	34.593434
1015.731307	97049.990427	34.598452
1016.864255	97228.881195	34.603469
1017.389722	97404.638841	34.608487
1018.886714	97565.829833	34.613504
1020.178168	97727.935705	34.618522
1021.228693	97876.257110	34.623540
1023.547478	98014.823927	34.628557
1024.422974	98160.396920	34.633575
1025.705407	98289.685171	34.638592
1026.480452	98437.086846	34.643610
1027.438840	98585.085834	34.648628
1028.644041	98729.037758	34.653645
1028.875298	98890.661510	34.658663
1029.914033	99039.662801	34.663680
1030.682389	99201.073269	34.668698
1031.869964	99350.172113	34.673716
1032.748458	99508.401053	34.678733
1033.301815	99693.837116	34.683751
1034.082150	99857.288305	34.688768
1034.799955	100034.368438	34.693786
1035.615216	100215.472805	34.698804
1036.462481	100398.814323	34.703821
1037.785416	100592.018223	34.708839
1038.711558	100758.591312	34.713856
1039.952354	100958.997240	34.718874
1040.440633	101147.082066	34.723892
1042.049750	101334.109546	34.728909
1042.967368	101521.322202	34.733927
1043.869196	101715.344905	34.738944
1045.321629	101900.135826	34.743962
1046.084002	102087.865772	34.748980
1048.028633	102248.107422	34.753997
1049.319784	102436.987247	34.759015
1050.469945	102608.442268	34.764032
1051.982200	102782.700490	34.769050
1053.104817	102966.958393	34.774068
1054.581762	103125.307294	34.779085
1055.075652	103303.536107	34.784103
1056.044914	103464.155310	34.789120
1057.238589	103632.811377	34.794138
1057.922090	103825.087851	34.799156
1059.508727	103973.653969	34.804173
1060.223010	104164.756503	34.809191
1060.893207	104351.929297	34.814208
1062.451778	104519.384827	34.819226
1063.447147	104688.213469	34.824244
1064.821758	104847.343302	34.829261
1066.045714	105031.839784	34.834279
1067.028699	105192.423093	34.839296
1067.810307	105372.796843	34.844314
1068.884546	105548.766999	34.849332
1070.193751	105724.496918	34.854349
1071.141360	105904.796271	34.859367
1072.194716	106085.560659	34.864384
1073.459589	106254.247273	34.869402
1074.294091	106424.791746	34.874420
1075.264275	106596.214127	34.879437
1076.186960	106779.601145	34.884455
1077.135304	106969.571005	34.889472
1078.557778	107142.480065	34.894490
1079.376458	107334.323055	34.899508
1080.392603	107511.063162	34.904525
1081.292165	107690.964700	34.909543
1082.073345	107873.711392	34.914560
1083.258673	108069.425454	34.919578
1084.244017	108265.667929	34.924596
1085.316785	108446.457907	34.929613
1086.244908	108649.235493	34.934631
1087.052552	108842.345089	34.939648
1088.359381	109048.495644	34.944666
1089.679536	109225.348922	34.949684
1090.776585	109400.302274	34.954701
1091.686373	109589.942530	34.959719
1092.559050	109777.398973	34.964736
1093.978193	109958.306631	34.969754
1094.667259	110144.199966	34.974772
1095.811952	110314.249452	34.979789
1096.882124	110519.753685	34.984807
1098.086542	110700.017758	34.989824
1099.031885	110896.843387	34.994842
1100.015215	111098.388949	34.999860
1101.107368	111289.366387	35.004877
1102.302642	111484.178953	35.009895
1103.583446	111682.753628	35.014912
1104.930889	111858.010883	35.019930
1105.945567	112054.060728	35.024948
1107.339785	112244.918990	35.029965
1108.556074	112436.301991	35.034983
1109.590279	112630.338594	35.040000
1110.916207	112811.065270	35.045018
1111.711858	113021.447418	35.050036
1113.036847	113190.661672	35.055053
1114.352596	113381.895492	35.060071
1115.435479	113579.401787	35.065088
1116.551006	113762.196332	35.070106
1117.411171	113971.890992	35.075124
1119.538242	114138.064940	35.080141
1120.939418	114315.216568	35.085159
1122.153004	114498.063123	35.090176
1123.067798	114675.145314	35.095194
1123.962150	114867.523114	35.100212
1124.824925	115055.562062	35.105229
1126.037420	115249.397561	35.110247
1126.651470	115452.505518	35.115264
1127.799526	115646.823160	35.120282
1128.250693	115851.151783	35.125300
1129.530129	116051.671088	35.130317
1130.602151	116256.685664	35.135335
1131.570166	116476.491440	35.140352
1132.778420	116682.284797	35.145370
1133.944620	116897.056677	35.150388
1134.972945	117101.248407	35.155405
1136.025596	117321.426874	35.160423
1137.096005	117543.529942	35.165440
1138.936081	117742.308942	35.170458
1140.149314	117951.861012	35.175476
1141.089223	118143.746848	35.180493
1142.878590	118358.591624	35.185511
1143.828146	118565.188874	35.190528
1145.359997	118771.742175	35.195546
1146.219281	118978.724752	35.200564
1147.307145	119190.511268	35.205581
1148.741762	119389.774119	35.210599
1149.819070	119596.129628	35.215616
1151.017031	119786.691437	35.220634
1152.129729	120005.740267	35.225652
1153.266092	120191.347888	35.230669
1154.509434	120395.337551	35.235687
1155.619231	120608.575361	35.240704
1157.032439	120809.017286	35.245722
1157.538348	121013.994674	35.250740
1158.561278	121222.461525	35.255757
1159.720607	121440.284340	35.260775
1160.440348	121641.543399	35.265792
1161.837663	121864.056628	35.270810
1162.494112	122096.058369	35.275828
1163.859839	122308.176560	35.280845
1165.096520	122522.560541	35.285863
1166.173838	122751.672107	35.290880
1167.600306	122947.235022	35.295898
1168.597723	123158.279626	35.300916
1169.914179	123359.147796	35.305933
1171.179295	123560.634083	35.310951
1172.155591	123758.240906	35.315968
1173.401494	123951.876006	35.320986
1174.742718	124160.121012	35.326004
1176.905220	124336.625801	35.331021
1179.087139	124512.583495	35.336039
1180.213558	124698.690110	35.341056
1181.663760	124876.114068	35.346074
1182.844320	125059.654027	35.351092
1183.930808	125227.673258	35.356109
1185.050368	125399.565998	35.361127
1185.754432	125593.554635	35.366144
1186.916880	125759.904087	35.371162
1187.940294	125949.546000	35.376180
1189.106686	126125.161167	35.381197
1190.672657	126318.378509	35.386215
1191.365025	126514.276040	35.391232
1192.337339	126719.089038	35.396250
1193.311597	126922.889180	35.401268
1194.024143	127122.830288	35.406285
1195.228695	127329.434117	35.411303
1196.085240	127541.204489	35.416320
1197.449984	127747.607266	35.421338
1198.447250	127968.495522	35.426356
1199.216449	128190.753833	35.431373
1200.596270	128420.327574	35.436391
1201.373822	128654.134376	35.441408
1202.585530	128879.303158	35.446426
1203.680470	129135.812394	35.451444
1204.447892	129361.932590	35.456461
1205.578282	129615.207832	35.461479
1206.438751	129852.850538	35.466496
1208.010995	130096.436334	35.471514
1209.243076	130356.177869	35.476532
1210.059473	130618.664697	35.481549
1211.502284	130867.170592	35.486567
1212.839885	131131.426313	35.491584
1214.390410	131373.428499	35.496602
1215.440376	131633.033205	35.501620
1216.594616	131869.375121	35.506637
1219.099756	132110.731032	35.511655
1220.907266	132330.616462	35.516672
1223.083547	132542.203000	35.521690
1225.055214	132763.015048	35.526708
1226.474151	132969.265948	35.531725
1227.690720	133165.448434	35.536743
1228.435613	133377.695115	35.541760
1229.656269	133583.412264	35.546778
1230.644517	133800.857033	35.551796
1231.646568	134012.456986	35.556813
1232.622247	134210.840691	35.561831
1233.557172	134439.264085	35.566848
1234.273524	134663.085368	35.571866
1235.537852	134898.670890	35.576884
1236.504285	135134.015718	35.581901
1237.309245	135374.840162	35.586919
1238.429916	135613.776050	35.591936
1239.601287	135851.044566	35.596954
1240.913462	136081.978112	35.601972
1242.512286	136313.423795	35.606989
1244.254402	136552.885187	35.612007
1245.869492	136782.810165	35.617024
1247.081139	137014.743073	35.622042
1248.240451	137240.512034	35.627060
1249.665405	137466.834568	35.632077
1250.922889	137672.787016	35.637095
1252.554916	137872.035493	35.642112
1253.923209	138069.071946	35.647130
1255.177084	138260.359758	35.652148
1256.537062	138444.556540	35.657165
1258.037349	138657.803207	35.662183
1258.867003	138875.510718	35.667200
1259.960395	139082.817561	35.672218
1261.525730	139281.679755	35.677236
1262.684503	139482.727611	35.682253
1264.044131	139685.987700	35.687271
1265.070935	139886.248295	35.692288
1266.672880	140085.806550	35.697306
1267.849581	140297.088375	35.702324
1269.369063	140489.600300	35.707341
1270.795724	140699.550091	35.712359
1271.794628	140923.088080	35.717376
1272.494376	141137.611044	35.722394
1273.879705	141350.462608	35.727412
1274.830033	141565.910555	35.732429
1275.856401	141783.616988	35.737447
1277.161459	142023.595355	35.742464
1278.152109	142236.796527	35.747482
1279.404413	142473.249036	35.752500
1280.629231	142708.579174	35.757517
1281.957862	142941.433820	35.762535
1282.968477	143190.459168	35.767552
1284.091487	143433.140241	35.772570
1285.545856	143678.735547	35.777588
1286.763744	143932.017992	35.782605
1288.343257	144162.721757	35.787623
1289.347101	144407.496222	35.792640
1290.723137	144664.004130	35.797658
1291.528656	144910.894493	35.802676
1292.636551	145177.544411	35.807693
1293.993367	145437.903473	35.812711
1295.123807	145706.164157	35.817728
1296.098374	145972.296775	35.822746
1297.699422	146243.451267	35.827764
1298.935526	146514.655374	35.832781
1299.922567	146794.145678	35.837799
1301.191631	147068.810619	35.842816
1302.427879	147349.621060	35.847834
1303.817597	147631.917506	35.852852
1305.056706	147903.943251	35.857869
1306.264464	148187.745181	35.862887
1307.893998	148478.264683	35.867904
1309.010551	148747.869326	35.872922
1310.238588	149027.286397	35.877940
1311.648786	149326.916759	35.882957
1312.925357	149601.434771	35.887975
1314.452964	149902.572365	35.892992
1315.823550	150199.134491	35.898010
1317.375724	150473.676932	35.903028
1318.672777	150773.502615	35.908045
1320.091378	151052.840187	35.913063
1321.270091	151330.202826	35.918080
1322.468826	151622.847544	35.923098
1324.100278	151896.562986	35.928116
1325.221984	152181.487938	35.933133
1326.947023	152474.470990	35.938151
1328.510664	152740.644377	35.943168
1330.098211	153023.279170	35.948186
1331.593589	153301.961246	35.953204
1332.539783	153586.164721	35.958221
1334.080610	153851.411055	35.963239
1335.103076	154119.547968	35.968256
1336.416523	154413.387631	35.973274
1337.867228	154656.621983	35.978292
1338.907521	154944.523812	35.983309
1340.443855	155200.812365	35.988327
1341.645482	155455.990879	35.993344
1343.383355	155731.276484	35.998362
1344.663136	155983.502734	36.003380
1345.941216	156239.929561	36.008397
1347.809340	156488.040894	36.013415
1349.646651	156737.503489	36.018432
1351.407748	156980.472830	36.023450
1353.167286	157219.181734	36.028468
1354.009532	157472.415785	36.033485
1355.263577	157704.462530	36.038503
1357.441900	157940.328602	36.043520
1359.023064	158164.585999	36.048538
1360.511133	158398.209221	36.053556
1361.592502	158642.417260	36.058573
1362.848372	158887.511356	36.063591
1363.946084	159125.021624	36.068608
1365.176265	159375.641222	36.073626
1366.580709	159620.626467	36.078644
1367.894943	159873.480684	36.083661
1368.995933	160105.604656	36.088679
1370.262043	160353.966276	36.093696
1371.088886	160628.218277	36.098714
1372.547267	160882.082559	36.103732
1374.251385	161148.708378	36.108749
1375.451648	161406.716198	36.113767
1376.390099	161677.632959	36.118784
1377.527693	161957.424619	36.123802
1378.960382	162235.164975	36.128820
1379.939159	162518.221734	36.133837
1380.970698	162802.324719	36.138855
1382.127626	163101.227287	36.143872
1382.998589	163404.480085	36.148890
1384.433445	163705.244145	36.153908
1385.578548	164012.249531	36.158925
1386.883479	164329.748547	36.163943
1388.413768	164634.233537	36.168960
1389.819803	164957.264953	36.173978
1391.232556	165256.026349	36.178996
1392.620980	165576.921152	36.184013
1393.900130	165888.764628	36.189031
1395.558137	166213.705152	36.194048
1397.383945	166529.954548	36.199066
1398.938195	166831.266479	36.204084
1400.104916	167145.319899	36.209101
1401.711182	167457.996149	36.214119
1403.581173	167760.987986	36.219136
1405.534497	168073.433709	36.224154
1407.144071	168366.436161	36.229172
1407.871982	168670.663181	36.234189
1409.666530	168983.116152	36.239207
1411.587179	169265.566985	36.244224
1412.868337	169570.470169	36.249242
1414.696502	169854.056595	36.254260
1416.771415	170148.186711	36.259277
1418.149527	170430.886678	36.264295
1419.350794	170716.586856	36.269312
1420.285703	171005.378204	36.274330
1421.942923	171281.781611	36.279348
1422.682021	171577.131195	36.284365
1424.570958	171858.892840	36.289383
1426.214456	172147.663278	36.294400
1427.221836	172444.217726	36.299418
1428.795407	172732.318115	36.304436
1429.721436	173030.577466	36.309453
1430.973282	173333.074132	36.314471
1432.604302	173614.800174	36.319488
1433.692321	173895.678456	36.324506
1434.822050	174179.140309	36.329524
1436.063785	174482.673934	36.334541
1437.011913	174767.260631	36.339559
1438.366018	175073.089110	36.344576
1439.310275	175391.398417	36.349594
1440.810411	175696.090020	36.354612
1441.821927	176022.565095	36.359629
1442.797013	176353.236309	36.364647
1444.470846	176679.149647	36.369664
1445.746249	177018.837036	36.374682
1447.090364	177348.921096	36.379700
1448.617861	177692.099631	36.384717
1449.708198	178043.462320	36.389735
1451.585332	178375.825843	36.394752
1452.829524	178738.120569	36.399770
1454.213098	179081.281700	36.404788
1455.804035	179434.424528	36.409805
1457.538546	179785.198202	36.414823
1459.199061	180128.676133	36.419840
1461.428276	180475.019712	36.424858
1463.655785	180795.601549	36.429876
1465.254315	181133.474008	36.434893
1466.770662	181450.775869	36.439911
1468.603953	181784.692038	36.444928
1470.261443	182102.469594	36.449946
1472.028791	182417.959056	36.454964
1473.829638	182733.026049	36.459981
1475.300440	183058.747518	36.464999
1476.971057	183373.281374	36.470016
1478.034720	183694.821984	36.475034
1479.411000	184017.975681	36.480052
1480.342062	184332.269166	36.485069
1481.882037	184655.018917	36.490087
1483.722847	184977.924045	36.495104
1484.894946	185299.722934	36.500122
1486.424528	185628.750502	36.505140
1488.010926	185972.088437	36.510157
1489.379621	186317.799984	36.515175
1491.219928	186640.093073	36.520192
1492.209053	186960.256404	36.525210
1494.367247	187276.585674	36.530228
1496.235854	187605.683333	36.535245
1497.360511	187934.220243	36.540263
1499.192791	188260.167053	36.545280
1500.219800	188588.736581	36.550298
1501.462480	188921.042453	36.555316
1503.017825	189246.380549	36.560333
1504.431342	189575.526667	36.565351
1505.874695	189906.269178	36.570368
1507.025406	190253.551388	36.575386
1508.441834	190605.552107	36.580404
1510.029771	190948.551871	36.585421
1511.766211	191295.108908	36.590439
1513.457800	191623.230550	36.595456
1514.461345	191965.456749	36.600474
1516.401068	192299.075926	36.605492
1517.946195	192639.832924	36.610509
1519.393230	192984.314859	36.615527
1521.080746	193319.390409	36.620544
1522.051489	193664.703786	36.625562
1523.812768	194013.900224	36.630580
1525.232027	194364.208760	36.635597
1526.641060	194705.317129	36.640615
1528.010916	195063.115095	36.645632
1529.643225	195430.558162	36.650650
1531.113912	195766.279431	36.655668
1532.512281	196109.034883	36.660685
1533.698667	196440.502956	36.665703
1535.626927	196769.425520	36.670720
1537.479116	197091.735309	36.675738
1539.844205	197405.265666	36.680756
1542.324429	197701.791897	36.685773
1544.239489	198012.923819	36.690791
1546.454309	198312.949832	36.695808
1547.732143	198600.271058	36.700826
1548.665696	198890.354544	36.705844
1550.510153	199198.786825	36.710861
1551.661806	199509.759767	36.715879
1553.071477	199816.362257	36.720896
1554.211982	200132.380214	36.725914
1555.685392	200444.307363	36.730932
1557.337191	200754.302087	36.735949
1558.379228	201079.342245	36.740967
1559.802544	201406.555564	36.745984
1561.140276	201740.170796	36.751002
1562.490014	202069.100687	36.756020
1563.757802	202427.018905	36.761037
1564.808141	202779.134434	36.766055
1566.137071	203122.952978	36.771072
1567.416141	203490.803419	36.776090
1568.654822	203864.160078	36.781108
1570.187062	204230.398136	36.786125
1571.549365	204625.602135	36.791143
1573.069746	205003.196991	36.796160
1574.433239	205391.827929	36.801178
1576.340851	205782.745464	36.806196
1578.180204	206161.766438	36.811213
1580.159929	206545.692655	36.816231
1582.706708	206904.272494	36.821248
1584.491477	207279.498906	36.826266
1586.295337	207654.495447	36.831284
1588.152446	208020.698423	36.836301
1588.914926	208401.431860	36.841319
1590.492144	208777.423510	36.846336
1591.757147	209156.833321	36.851354
1593.110062	209546.693288	36.856372
1594.829126	209933.447284	36.861389
1596.879586	210312.123464	36.866407
1598.825857	210683.796703	36.871424
1600.256404	211080.508046	36.876442
1601.990718	211462.035226	36.881460
1603.396711	211839.237517	36.886477
1605.264937	212213.038343	36.891495
1607.054962	212597.367753	36.896512
1608.503033	212980.993425	36.901530
1609.662405	213369.442972	36.906548
1611.615695	213748.899864	36.911565
1612.590284	214141.954720	36.916583
1614.381145	214528.298877	36.921600
1615.784482	214934.619813	36.926618
1617.264976	215340.167945	36.931636
1618.811339	215739.891084	36.936653
1620.628024	216148.181028	36.941671
1621.946132	216540.402335	36.946688
1623.359469	216952.013230	36.951706
1624.647168	217363.291091	36.956724
1626.731884	217779.874330	36.961741
1628.256995	218183.217881	36.966759
1630.466833	218656.599110	36.971776
1632.979762	219041.496749	36.976794
1634.527478	219435.190499	36.981812
1636.151632	219826.409567	36.986829
1637.654565	220220.875739	36.991847
1639.461261	220598.987555	36.996864
1641.371916	220965.705091	37.001882
1642.962365	221335.676978	37.006900
1644.959600	221697.938061	37.011917
1645.967316	222071.640695	37.016935
1647.420372	222438.159487	37.021952
1649.348737	222804.956691	37.026970
1650.599773	223174.914768	37.031988
1652.257002	223541.454393	37.037005
1653.276790	223931.010463	37.042023
1654.992664	224310.826716	37.047040
1656.798071	224697.182505	37.052058
1658.394719	225090.889080	37.057076
1660.212772	225472.851285	37.062093
1661.746096	225876.781577	37.067111
1663.042678	226269.881238	37.072128
1664.492850	226672.862763	37.077146
1666.054497	227075.243038	37.082164
1668.183826	227487.030554	37.087181
1669.879462	227900.287992	37.092199
1671.443467	228303.687863	37.097216
1673.390760	228702.479140	37.102234
1674.626771	229121.582220	37.107252
1676.510396	229531.842074	37.112269
1678.077725	229967.276413	37.117287
1679.624214	230377.442091	37.122304
1681.606059	230787.841984	37.127322
1683.416766	231197.712519	37.132340
1685.421723	231619.769961	37.137357
1686.781877	232053.314608	37.142375
1688.518761	232450.221123	37.147392
1690.553176	232872.988603	37.152410
1692.022262	233305.452148	37.157428
1694.134412	233720.258675	37.162445
1695.476330	234152.008978	37.167463
1697.266619	234578.072830	37.172480
1698.876829	235002.338644	37.177498
1700.244306	235426.290005	37.182516
1702.165377	235857.441344	37.187533
1703.461505	236289.484351	37.192551
1705.487593	236734.286624	37.197568
1707.571569	237171.205986	37.202586
1708.823766	237615.782565	37.207604
1710.394155	238034.753579	37.212621
1712.147965	238479.554343	37.217639
1713.951977	238919.394519	37.222656
1716.293565	239347.284317	37.227674
1718.257688	239783.213560	37.232692
1720.426417	240204.224406	37.237709
1722.035987	240636.835530	37.242727
1723.404406	241074.034329	37.247744
1725.601394	241498.675656	37.252762
1727.096970	241939.335347	37.257780
1728.497133	242366.929470	37.262797
1730.174818	242811.396578	37.267815
1731.679920	243257.391751	37.272832
1733.316872	243676.972866	37.277850
1735.474206	244124.691012	37.282868
1737.260541	244551.488672	37.287885
1739.528983	244979.020383	37.292903
1741.472613	245419.104457	37.297920
1743.184566	245824.756063	37.302938
1744.845624	246250.738803	37.307956
1746.626732	246662.578449	37.312973
1748.434611	247104.211688	37.317991
1750.287327	247533.238376	37.323008
1752.151469	247961.908118	37.328026
1753.416762	248391.693330	37.333044
1755.511742	248801.756575	37.338061
1757.339320	249208.257197	37.343079
1759.479917	249599.845906	37.348096
1761.305902	249983.764420	37.353114
1762.650289	250374.418346	37.358132
1764.498768	250768.926952	37.363149
1765.708183	251182.288801	37.368167
1767.206686	251588.947739	37.373184
1768.808480	251987.867454	37.378202
1770.353627	252419.516048	37.383220
1771.782816	252846.078106	37.388237
1773.169293	253279.023737	37.393255
1774.638169	253713.302469	37.398272
1776.287227	254151.590890	37.403290
1777.714168	254600.992045	37.408308
1779.320148	255063.776850	37.413325
1780.995971	255520.885490	37.418343
1782.485701	255992.149286	37.423360
1784.451625	256466.154524	37.428378
1786.084310	256939.046402	37.433396
1787.904464	257414.701903	37.438413
1789.534588	257897.247806	37.443431
1791.133841	258370.247303	37.448448
1793.299505	258859.386180	37.453466
1794.965984	259360.267615	37.458484
1796.760282	259847.511852	37.463501
1798.574370	260348.140401	37.468519
1799.788342	260849.477630	37.473536
1802.094423	261356.807672	37.478554
1803.806289	261871.780459	37.483572
1805.543472	262368.890455	37.488589
1807.439796	262872.934580	37.493607
1809.302622	263391.717979	37.498624
1811.339492	263910.624889	37.503642
1813.462525	264425.376621	37.508660
1816.009441	264906.322655	37.513677
1818.602625	265401.334191	37.518695
1821.412273	265862.879086	37.523712
1824.361025	266324.883410	37.528730
1826.056287	266789.228073	37.533748
1828.038078	267246.107407	37.538765
1829.767164	267703.358318	37.543783
1831.712102	268169.159502	37.548800
1833.852790	268614.859534	37.553818
1835.424902	269065.555753	37.558836
1836.782400	269515.626465	37.563853
1838.812166	269976.407512	37.568871
1840.281609	270448.102169	37.573888
1842.215351	270903.436385	37.578906
1843.526538	271375.054434	37.583924
1845.560802	271840.151074	37.588941
1847.189674	272307.955880	37.593959
1848.436340	272789.235790	37.598976
1849.937160	273254.774146	37.603994
1851.834017	273751.009224	37.609012
1853.149867	274251.505384	37.614029
1854.545515	274751.708100	37.619047
1856.027370	275262.539414	37.624064
1857.829179	275776.822554	37.629082
1859.592232	276291.517530	37.634100
1861.402581	276806.610112	37.639117
1863.019037	277327.957204	37.644135
1864.944687	277863.858522	37.649152
1866.960184	278380.412638	37.654170
1869.003664	278907.172665	37.659188
1871.669982	279409.595010	37.664205
1874.217088	279911.426194	37.669223
1876.395813	280422.690300	37.674240
1878.175920	280914.459341	37.679258
1879.786876	281403.638670	37.684276
1881.687210	281882.227257	37.689293
1883.821085	282343.350473	37.694311
1885.493740	282820.272307	37.699328
1887.109717	283293.696810	37.704346
1888.772989	283792.259845	37.709364
1890.548979	284268.119292	37.714381
1892.102186	284770.101466	37.719399
1894.010739	285267.476673	37.724416
1895.804243	285765.555185	37.729434
1897.836876	286272.559343	37.734452
1899.669005	286762.753988	37.739469
1901.399938	287267.848795	37.744487
1903.302930	287783.124735	37.749504
1905.512357	288294.563614	37.754522
1907.411887	288809.201522	37.759540
1909.141033	289318.125133	37.764557
1911.274061	289839.553592	37.769575
1912.945755	290362.453215	37.774592
1914.686515	290881.910383	37.779610
1916.282525	291414.902381	37.784628
1917.510684	291967.485659	37.789645
1919.652283	292500.916630	37.794663
1921.220150	293057.096793	37.799680
1923.056378	293608.378839	37.804698
1925.128183	294167.620480	37.809716
1926.918097	294723.324682	37.814733
1929.373214	295297.102620	37.819751
1931.072667	295856.092944	37.824768
1933.602309	296408.593798	37.829786
1936.039556	296960.065834	37.834804
1937.884948	297531.012224	37.839821
1940.285814	298081.519515	37.844839
1942.327716	298619.307641	37.849856
1944.473953	299183.211042	37.854874
1945.988605	299720.648772	37.859892
1948.133870	300275.834754	37.864909
1950.500328	300824.555489	37.869927
1952.645381	301379.710079	37.874944
1954.818686	301911.262223	37.879962
1956.956895	302457.014658	37.884980
1958.654740	302997.630138	37.889997
1961.364602	303532.411995	37.895015
1963.638922	304064.494355	37.900032
1965.494929	304597.379204	37.905050
1967.591888	305132.532368	37.910068
1969.151837	305663.707460	37.915085
1971.233716	306202.717132	37.920103
1973.234603	306740.695641	37.925120
1974.511556	307278.383926	37.930138
1976.176290	307831.953815	37.935156
1977.762307	308386.091842	37.940173
1979.712381	308932.801377	37.945191
1981.658979	309511.303487	37.950208
1983.598792	310070.349635	37.955226
1986.463915	310616.897165	37.960244
1988.525169	311145.060437	37.965261
1990.915779	311695.970741	37.970279
1992.676721	312260.211853	37.975296
1994.732263	312815.486766	37.980314
1996.683354	313351.297302	37.985332
1999.591802	313876.255162	37.990349
2002.076048	314404.783780	37.995367
2004.210897	314943.473164	38.000384
2006.394505	315463.308371	38.005402
2008.507010	315981.043982	38.010420
2010.251448	316495.332343	38.015437
2012.066284	317003.790382	38.020455
2013.673229	317505.321397	38.025472
2015.735696	318013.299757	38.030490
2017.644175	318504.692978	38.035508
2019.216136	319006.523847	38.040525
2021.089705	319502.562663	38.045543
2022.871685	320015.524263	38.050560
2024.598354	320540.069921	38.055578
2026.768404	321071.902035	38.060596
2028.211322	321607.887144	38.065613
2029.544916	322136.370105	38.070631
2031.382594	322698.205968	38.075648
2033.109442	323255.053261	38.080666
2035.064516	323796.471308	38.085684
2037.056040	324358.470555	38.090701
2039.560993	324922.284448	38.095719
2041.838585	325473.410353	38.100736
2043.800062	326046.114192	38.105754
2046.013618	326615.115065	38.110772
2047.502017	327197.458177	38.115789
2049.394528	327770.309698	38.120807
2050.717338	328368.130926	38.125824
2052.786027	328969.656875	38.130842
2054.722772	329576.047693	38.135860
2056.613270	330190.513337	38.140877
2058.365246	330793.316938	38.145895
2060.671581	331410.899988	38.150912
2062.871964	332030.524860	38.155930
2065.170215	332651.497751	38.160948
2067.258981	333286.156451	38.165965
2069.144319	333910.839224	38.170983
2071.001057	334540.393834	38.176000
2073.735651	335155.123395	38.181018
2076.993897	335772.399771	38.186036
2079.446930	336371.549834	38.191053
2082.774031	336963.212766	38.196071
2085.260495	337552.951596	38.201088
2087.217862	338144.954172	38.206106
2089.709436	338734.755073	38.211124
2091.655942	339314.358690	38.216141
2093.802206	339897.958862	38.221159
2095.682777	340479.997060	38.226176
2097.571933	341066.951504	38.231194
2099.269842	341657.611175	38.236212
2101.384284	342246.088453	38.241229
2103.566453	342845.436560	38.246247
2105.280706	343449.778650	38.251264
2107.256225	344060.212546	38.256282
2109.226077	344657.136920	38.261300
2111.111799	345272.798914	38.266317
2113.081450	345881.687941	38.271335
2115.165094	346501.996888	38.276352
2116.570414	347119.414745	38.281370
2118.512467	347763.765224	38.286388
2120.199035	348408.174318	38.291405
2122.214852	349046.683010	38.296423
2124.660140	349684.553681	38.301440
2127.000418	350329.234101	38.306458
2129.634427	350963.045969	38.311476
2131.790260	351608.144593	38.316493
2134.328725	352235.559116	38.321511
2136.218023	352872.816482	38.326528
2138.296362	353505.820984	38.331546
2140.730670	354136.423038	38.336564
2142.906872	354763.708928	38.341581
2145.239815	355408.976272	38.346599
2147.144656	356041.642457	38.351616
2148.842143	356673.242340	38.356634
2151.051564	357315.024882	38.361652
2153.374266	357936.911332	38.366669
2155.568989	358545.260266	38.371687
2157.859382	359141.583090	38.376704
2160.160735	359746.217701	38.381722
2162.630673	360332.750563	38.386740
2164.662438	360941.877460	38.391757
2166.992145	361543.918166	38.396775
2169.145587	362139.788389	38.401792
2171.282987	362752.625400	38.406810
2173.387057	363357.466817	38.411828
2174.819931	363974.866310	38.416845
2177.287713	364597.692112	38.421863
2178.980168	365231.975843	38.426880
2181.000675	365853.916667	38.431898
2183.390104	366485.908587	38.436916
2185.187280	367121.285590	38.441933
2187.730836	367742.830506	38.446951
2190.144878	368381.940582	38.451968
2192.365643	369028.326542	38.456986
2194.356623	369679.102226	38.462004
2196.520684	370327.631185	38.467021
2198.652046	370972.704504	38.472039
2200.686762	371627.446453	38.477056
2202.525713	372302.043895	38.482074
2205.376229	372944.934710	38.487092
2207.621799	373608.077783	38.492109
2210.186961	374265.322442	38.497127
2212.604524	374930.086652	38.502144
2214.674088	375597.634910	38.507162
2216.782630	376254.258666	38.512180
2218.985018	376934.237569	38.517197
2220.772099	377606.739631	38.522215
2222.765995	378288.374908	38.527232
2224.789348	378978.791634	38.532250
2227.133831	379646.191577	38.537268
2229.034364	380346.338840	38.542285
2231.251920	381052.353152	38.547303
2233.490852	381751.350493	38.552320
2235.499129	382466.244742	38.557338
2238.014274	383165.674098	38.562356
2240.302205	383863.655517	38.567373
2242.587531	384563.143897	38.572391
2245.165626	385266.245508	38.577408
2247.452114	385989.663408	38.582426
2249.714527	386694.713070	38.587444
2251.624569	387421.051299	38.592461
2254.165958	388136.418065	38.597479
2256.383389	388867.515032	38.602496
2257.932128	389587.626833	38.607514
2260.586605	390307.818691	38.612532
2263.039714	391019.610912	38.617549
2265.347734	391756.532246	38.622567
2267.222610	392483.342508	38.627584
2269.077807	393222.153996	38.632602
2271.415490	393967.078301	38.637620
2273.888823	394710.111661	38.642637
2276.559871	395435.123477	38.647655
2279.795927	396158.301137	38.652672
2282.306382	396889.438016	38.657690
2285.215570	397580.978788	38.662708
2287.943632	398299.017887	38.667725
2290.163555	399001.663739	38.672743
2292.639226	399688.056463	38.677760
2295.065020	400385.287767	38.682778
2297.386235	401069.696662	38.687796
2299.958447	401774.067417	38.692813
2301.868276	402464.516843	38.697831
2304.515483	403135.240291	38.702848
2306.128674	403806.194444	38.707866
2308.103974	404471.270440	38.712884
2309.961879	405141.215015	38.717901
2311.841352	405812.964339	38.722919
2314.843990	406486.488585	38.727936
2316.593270	407165.169074	38.732954
2319.214490	407831.148010	38.737972
2321.335228	408513.889133	38.742989
2323.644232	409201.218399	38.748007
2325.941763	409888.126901	38.753024
2327.777550	410597.589933	38.758042
2330.364566	411286.163236	38.763060
2332.544485	411990.719714	38.768077
2334.754917	412687.982599	38.773095
2336.947393	413388.067211	38.778112
2339.084005	414106.658603	38.783130
2341.370509	414817.227073	38.788148
2343.908927	415549.061270	38.793165
2346.162167	416277.806709	38.798183
2348.534557	417005.752292	38.803200
2350.702106	417739.688182	38.808218
2352.931328	418466.805781	38.813236
2355.719203	419205.181491	38.818253
2357.658908	419955.577994	38.823271
2360.054328	420686.428930	38.828288
2362.679277	421452.064729	38.833306
2365.065476	422188.596580	38.838324
2368.098422	422933.254808	38.843341
2370.914472	423676.989716	38.848359
2373.903792	424411.811946	38.853376
2377.190020	425124.662630	38.858394
2379.921558	425841.432458	38.863412
2382.173390	426563.779582	38.868429
2384.524165	427283.101650	38.873447
2386.531450	427991.775775	38.878464
2388.937630	428719.147145	38.883482
2391.121050	429438.584581	38.888500
2393.411983	430171.753260	38.893517
2395.657035	430904.856359	38.898535
2397.713242	431648.143384	38.903552
2399.875893	432394.679960	38.908570
2402.112227	433143.104316	38.913588
2404.282114	433893.641744	38.918605
2406.433970	434655.496323	38.923623
2408.838206	435416.525086	38.928640
2410.852536	436195.105574	38.933658
2413.104508	436965.573210	38.938676
2415.586813	437753.791929	38.943693
2417.700825	438527.114540	38.948711
2420.132163	439314.882778	38.953728
2422.476908	440112.202281	38.958746
2425.108492	440909.648687	38.963764
2427.572740	441697.732998	38.968781
2430.124452	442493.820465	38.973799
2432.781214	443281.766393	38.978816
2435.320033	444091.409535	38.983834
2437.789949	444885.248808	38.988852
2439.738040	445684.103459	38.993869
2441.738753	446499.665759	38.998887
2443.929253	447314.710879	39.003904
2446.473950	448121.117719	39.008922
2449.258205	448924.773876	39.013940
2451.831660	449733.138912	39.018957
2454.335134	450555.900541	39.023975
2457.152714	451352.429068	39.028992
2459.431744	452171.321040	39.034010
2461.843464	452983.078778	39.039028
2464.943770	453763.487769	39.044045
2467.122416	454550.846738	39.049063
2469.863532	455323.316847	39.054080
2471.925140	456090.156033	39.059098
2474.375575	456858.874719	39.064116
2476.759821	457642.441420	39.069133
2478.697319	458423.169764	39.074151
2481.162222	459207.067700	39.079168
2483.519904	460010.165183	39.084186
2485.837666	460804.288938	39.089204
2488.698062	461601.577969	39.094221
2491.076353	462406.042662	39.099239
2493.781940	463188.937220	39.104256
2497.334321	463968.375761	39.109274
2500.375523	464758.988091	39.114292
2503.394360	465524.148746	39.119309
2505.919187	466311.397486	39.124327
2508.396523	467087.250906	39.129344
2510.987531	467866.845122	39.134362
2513.038207	468661.203177	39.139380
2515.650165	469444.571327	39.144397
2517.715106	470244.168090	39.149415
2519.623479	471036.481120	39.154432
2522.270565	471870.375485	39.159450
2524.090315	472685.372212	39.164468
2526.275371	473515.380236	39.169485
2528.334769	474353.051776	39.174503
2530.528397	475206.779456	39.179520
2533.330270	476051.729729	39.184538
2535.659206	476883.939686	39.189556
2538.603709	477761.421172	39.194573
2541.114180	478615.748841	39.199591
2543.826984	479465.053939	39.204608
2546.449987	480338.627445	39.209626
2549.309932	481191.515265	39.214644
2552.049673	482053.826546	39.219661
2554.904173	482923.551646	39.224679
2557.977555	483781.887954	39.229696
2560.399451	484636.402849	39.234714
2562.636930	485494.189371	39.239732
2565.444424	486358.252777	39.244749
2567.816054	487234.614110	39.249767
2570.222007	488099.921229	39.254784
2572.735470	488974.254773	39.259802
2575.174498	489857.946085	39.264820
2577.974951	490729.217294	39.269837
2580.242881	491629.100499	39.274855
2582.830897	492504.305388	39.279872
2585.487233	493402.367176	39.284890
2587.508270	494298.872099	39.289908
2590.314437	495208.522952	39.294925
2592.896419	496115.084408	39.299943
2595.528307	497005.342296	39.304960
2598.633533	497906.424131	39.309978
2600.785492	498812.660307	39.314996
2603.420185	499719.928537	39.320013
2605.455529	500639.908566	39.325031
2608.065466	501550.007711	39.330048
2610.700829	502468.375677	39.335066
2613.965188	503382.503680	39.340084
2617.015651	504283.503261	39.345101
2619.768867	505207.449267	39.350119
2622.238312	506103.351209	39.355136
2625.125210	507000.950599	39.360154
2628.213046	507903.913175	39.365172
2631.251149	508806.279047	39.370189
2633.568619	509692.730691	39.375207
2635.987222	510594.947366	39.380224
2639.054131	511462.675325	39.385242
2641.340836	512328.065091	39.390260
2644.447885	513166.607096	39.395277
2646.994980	514015.026022	39.400295
2649.545916	514862.793981	39.405312
2652.084620	515718.179056	39.410330
2655.011205	516559.644948	39.415348
2657.821467	517397.506807	39.420365
2660.009437	518257.799916	39.425383
2662.536693	519121.063188	39.430400
2665.423019	519970.363151	39.435418
2667.178597	520843.129989	39.440436
2670.014691	521711.135044	39.445453
2671.923955	522604.281083	39.450471
2674.288560	523492.262473	39.455488
2676.884711	524378.995380	39.460506
2679.329336	525281.869593	39.465524
2682.058891	526197.788197	39.470541
2684.710536	527122.527651	39.475559
2687.154081	528050.719195	39.480576
2689.690397	528984.528035	39.485594
2691.723309	529939.207250	39.490612
2694.238916	530882.467315	39.495629
2696.403912	531857.241584	39.500647
2699.300517	532830.723267	39.505664
2702.068255	533808.239122	39.510682
2704.490452	534801.652725	39.515700
2707.280188	535780.542982	39.520717
2710.497146	536771.124131	39.525735
2713.361119	537768.741182	39.530752
2715.810154	538761.375686	39.535770
2718.341485	539776.420359	39.540788
2720.712912	540795.897379	39.545805
2723.078830	541827.678932	39.550823
2725.770471	542859.834881	39.555840
2728.507985	543895.932234	39.560858
2731.438890	544953.802041	39.565876
2733.737344	545991.477222	39.570893
2736.681317	547056.428707	39.575911
2739.101108	548111.327402	39.580928
2742.174219	549168.703287	39.585946
2745.099702	550226.223702	39.590964
2747.962427	551300.314917	39.595981
2751.177468	552359.835529	39.600999
2754.014819	553426.072269	39.606016
2757.247064	554484.268715	39.611034
2759.491813	555554.406978	39.616052
2762.730923	556612.285045	39.621069
2765.652484	557680.283438	39.626087
2768.171836	558746.856027	39.631104
2771.335266	559802.434504	39.636122
2773.574896	560874.108467	39.641140
2776.649858	561945.658575	39.646157
2779.640510	563010.605283	39.651175
2782.616793	564074.614236	39.656192
2785.265200	565145.220543	39.661210
2788.103775	566217.917443	39.666228
2790.918195	567280.386073	39.671245
2794.171743	568347.063732	39.676263
2797.506538	569395.464380	39.681280
2800.566384	570445.331039	39.686298
2803.077778	571517.139654	39.691316
2805.939081	572552.458676	39.696333
2808.447022	573615.106404	39.701351
2810.600321	574684.498912	39.706368
2813.518542	575748.756896	39.711386
2816.159864	576826.268077	39.716404
2819.291523	577882.131034	39.721421
2821.409684	578948.908736	39.726439
2824.034687	579995.896495	39.731456
2826.858662	581039.151493	39.736474
2829.037642	582079.064237	39.741492
2832.168706	583123.697611	39.746509
2834.756114	584163.417113	39.751527
2837.541491	585229.592699	39.756544
2840.368977	586277.065949	39.761562
2842.724712	587350.798257	39.766580
2845.971372	588400.325503	39.771597
2849.094505	589484.971517	39.776615
2852.411584	590528.737695	39.781632
2855.957939	591587.060071	39.786650
2858.890482	592648.396758	39.791668
2862.269297	593700.345126	39.796685
2865.303615	594754.862543	39.801703
2868.157258	595807.361826	39.806720
2871.551213	596854.868874	39.811738
2874.377459	597913.797112	39.816756
2877.140295	598965.277228	39.821773
2879.758152	600017.287555	39.826791
2882.522224	601092.014464	39.831808
2885.396246	602149.047786	39.836826
2887.579360	603225.625307	39.841844
2890.455886	604307.545139	39.846861
2893.219526	605396.089642	39.851879
2896.032689	606494.383269	39.856896
2898.913685	607576.794191	39.861914
2901.833038	608682.967333	39.866932
2904.980754	609800.153829	39.871949
2907.568601	610892.554521	39.876967
2910.304262	612013.392244	39.881984
2913.246068	613123.528603	39.887002
2916.379690	614258.783422	39.892020
2919.343993	615370.843331	39.897037
2922.587503	616484.946279	39.902055
2925.754983	617615.251283	39.907072
2929.279702	618725.281462	39.912090
2932.590950	619838.684339	39.917108
2935.676911	620937.064103	39.922125
2939.372619	622044.829997	39.927143
2942.314388	623155.406202	39.932160
2945.578988	624249.773543	39.937178
2948.578622	625337.527691	39.942196
2951.778704	626438.529547	39.947213
2954.832155	627524.504749	39.952231
2957.880652	628622.309744	39.957248
2960.603554	629710.065561	39.962266
2963.281478	630820.542100	39.967284
2966.509272	631891.459718	39.972301
2969.229131	632981.527204	39.977319
2972.393149	634090.331744	39.982336
2975.271393	635189.630757	39.987354
2978.246521	636280.112585	39.992372
2980.899293	637392.994456	39.997389
2984.025832	638481.424060	40.002407
2986.583499	639590.991807	40.007424
2989.215748	640711.106144	40.012442
2992.314420	641827.978482	40.017460
2995.097646	642943.135108	40.022477
2997.501213	644077.686312	40.027495
2999.738374	645215.879466	40.032512
3002.927916	646360.919700	40.037530
3005.477717	647522.889731	40.042548
3008.452494	648675.133285	40.047565
3011.713142	649828.643668	40.052583
3014.391076	651000.461089	40.057600
3017.429962	652150.700193	40.062618
3020.230552	653312.706680	40.067636
3023.500856	654449.784729	40.072653
3026.557200	655591.251717	40.077671
3029.017119	656720.330329	40.082688
3032.294926	657840.228418	40.087706
3035.421499	658973.023186	40.092724
3038.533525	660099.613603	40.097741
3041.321094	661241.563844	40.102759
3044.001195	662406.400247	40.107776
3046.847522	663563.900648	40.112794
3049.433246	664727.826199	40.117812
3052.012171	665901.815351	40.122829
3054.932849	667096.406389	40.127847
3057.662481	668299.488100	40.132864
3060.269775	669509.552898	40.137882
3063.460479	670721.009298	40.142900
3066.026991	671960.317524	40.147917
3069.111044	673198.880683	40.152935
3072.205715	674442.550233	40.157952
3075.217699	675693.278016	40.162970
3078.171921	676949.117730	40.167988
3081.607634	678214.501130	40.173005
3085.291783	679480.068942	40.178023
3088.476818	680745.198263	40.183040
3091.364898	682017.109497	40.188058
3095.054935	683284.241750	40.193076
3098.081014	684567.004654	40.198093
3101.623216	685832.070179	40.203111
3104.716066	687118.337366	40.208128
3107.729571	688393.115062	40.213146
3110.878355	689662.329409	40.218164
3114.101213	690958.405111	40.223181
3117.198296	692236.150262	40.228199
3120.080257	693536.872837	40.233216
3123.367342	694831.038133	40.238234
3126.372695	696124.069564	40.243252
3129.824656	697432.215270	40.248269
3132.801766	698717.035951	40.253287
3136.161296	700032.349855	40.258304
3139.615171	701331.685244	40.263322
3143.455207	702632.548779	40.268340
3146.637658	703913.947181	40.273357
3149.919125	705198.559959	40.278375
3153.437686	706494.537946	40.283392
3157.035416	707770.789002	40.288410
3160.746351	709054.262551	40.293428
3163.757565	710345.980140	40.298445
3167.169831	711612.181640	40.303463
3170.296327	712880.173329	40.308480
3173.348334	714153.433860	40.313498
3176.531675	715429.302952	40.318516
3179.535453	716723.963785	40.323533
3182.813331	717992.303254	40.328551
3185.918182	719266.119882	40.333568
3188.661230	720556.918117	40.338586
3192.064187	721835.834444	40.343604
3195.282013	723127.689546	40.348621
3198.938216	724400.235085	40.353639
3201.869688	725697.076571	40.358656
3205.210612	726957.761025	40.363674
3208.355180	728243.983659	40.368692
3211.548265	729524.807921	40.373709
3214.322565	730811.182005	40.378727
3217.506770	732111.215614	40.383744
3220.374305	733402.746225	40.388762
3223.900660	734685.715306	40.393780
3226.751568	735990.661974	40.398797
3229.717969	737287.874178	40.403815
3232.608140	738579.311538	40.408832
3235.816400	739847.687873	40.413850
3238.776252	741113.781478	40.418868
3241.848727	742385.920274	40.423885
3245.160280	743651.205539	40.428903
3248.160867	744935.129808	40.433920
3251.276970	746211.478333	40.438938
3254.009450	747503.558016	40.443956
3257.317142	748804.892760	40.448973
3259.921081	750102.528452	40.453991
3263.108198	751422.371670	40.459008
3266.257860	752753.968892	40.464026
3269.988028	754059.625307	40.469044
3273.263374	755388.382699	40.474061
3277.066114	756707.762445	40.479079
3280.679805	758042.652191	40.484096
3283.597537	759385.594862	40.489114
3286.965885	760717.496785	40.494132
3290.081586	762064.953621	40.499149
3293.357943	763411.012362	40.504167
3296.595069	764764.855600	40.509184
3299.964944	766131.515859	40.514202
3303.102446	767491.425026	40.519220
3306.089368	768867.729268	40.524237
3309.279497	770254.658325	40.529255
3312.382360	771651.024561	40.534272
3315.541109	773051.982735	40.539290
3318.517364	774451.427619	40.544308
3321.559175	775884.487157	40.549325
3325.224568	777297.765859	40.554343
3328.133756	778746.590914	40.559360
3331.721307	780171.747663	40.564378
3335.208454	781598.653452	40.569396
3339.028688	783045.243609	40.574413
3342.300229	784487.169554	40.579431
3345.874772	785937.045936	40.584448
3348.853207	787384.373267	40.589466
3352.224134	788843.894531	40.594484
3355.368761	790307.320657	40.599501
3358.761329	791773.638903	40.604519
3361.694686	793248.842882	40.609536
3364.898400	794729.033627	40.614554
3368.519546	796207.913320	40.619572
3371.596174	797694.307619	40.624589
3375.110339	799184.034334	40.629607
3378.687404	800694.430468	40.634624
3381.823201	802194.734104	40.639642
3385.116386	803701.829597	40.644660
3388.446187	805218.079181	40.649677
3392.056992	806718.249345	40.654695
3395.429670	808237.736629	40.659712
3399.101297	809750.041610	40.664730
3402.938764	811251.524353	40.669748
3406.576790	812759.841230	40.674765
3410.630805	814247.137945	40.679783
3414.403775	815743.383322	40.684800
3418.135307	817219.721642	40.689818
3422.147938	818704.475347	40.694836
3425.373119	820176.875280	40.699853
3428.484216	821633.450713	40.704871
3432.452751	823118.251172	40.709888
3435.642712	824589.677072	40.714906
3439.363349	826038.645582	40.719924
3442.983650	827510.127622	40.724941
3446.203599	828963.358992	40.729959
3450.140400	830423.799692	40.734976
3453.211083	831889.122270	40.739994
3457.404128	833326.505506	40.745012
3461.013667	834766.869085	40.750016
3464.716336	836123.507954	40.755021
3467.750080	837444.295736	40.760026
3470.599616	838702.435109	40.765031
3473.875105	839896.544605	40.770036
3476.597589	841033.064033	40.775040
3479.448469	842087.576438	40.780045
3482.241812	843075.853586	40.785050
3485.063398	843997.960702	40.790055
3487.565393	844842.479534	40.795060
3489.799811	845646.280186	40.800064
3492.090112	846373.943498	40.805069
3494.011082	847045.544858	40.810074
3495.758097	847652.202046	40.815079
3498.389769	848192.979906	40.820084
3499.863953	848686.354394	40.825088
3501.874718	849127.868327	40.830093
3503.722201	849500.307026	40.835098
3504.925291	849838.636911	40.840103
3506.598765	850132.841409	40.845108
3507.758003	850387.374821	40.850112
3508.994881	850589.482033	40.855117
3510.143883	850753.610797	40.860122
3511.183093	850900.903327	40.865127
3512.492128	850981.333481	40.870132
3513.234318	851051.239739	40.875136
3513.921931	851084.533390	40.880141
3514.664306	851076.911581	40.885146
3515.271102	851061.520386	40.890151
3516.108338	851016.774736	40.895156
3516.526164	850942.488843	40.900160
3516.920201	850862.849015	40.905165
3517.396578	850755.922338	40.910170
3517.832437	850632.149791	40.915175
3518.197624	850479.846690	40.920180
3518.610517	850343.604297	40.925184
3518.842773	850166.476466	40.930189
3518.787744	849995.625372	40.935194
3519.320243	849793.889400	40.940199
3519.594095	849588.292754	40.945204
3519.710483	849390.801360	40.950208
3519.808822	849167.196613	40.955213
3519.920561	848931.110698	40.960218
3520.210784	848699.078686	40.965223
3520.669767	848454.538366	40.970228
3520.566327	848201.214033	40.975232
3520.465121	847943.201747	40.980237
3520.839587	847665.025991	40.985242
3520.780941	847409.031182	40.990247
3520.961586	847119.071332	40.995252
3521.037955	846843.344758	41.000256
3520.974607	846553.399023	41.005261
3521.072826	846264.777916	41.010266
3521.081425	845972.746706	41.015271
3521.092198	845666.664475	41.020276
3520.739889	845378.369427	41.025280
3520.961211	845073.393550	41.030285
3520.845228	844764.753729	41.035290
3520.854108	844460.563213	41.040295
3521.166049	844145.095232	41.045300
3520.971387	843843.199889	41.050304
3520.981401	843525.556825	41.055309
3520.921348	843215.954615	41.060314
3520.589202	842903.310134	41.065319
3520.541549	842585.678233	41.070324
3520.555261	842284.600844	41.075328
3520.670156	841970.715167	41.080333
3520.330775	841648.500203	41.085338
3520.406880	841338.296292	41.090343
3520.397299	841012.531880	41.095348
3520.089090	840704.701641	41.100352
3520.094628	840394.170696	41.105357
3520.133578	840074.740610	41.110362
3520.148341	839760.664925	41.115367
3520.247955	839446.462239	41.120372
3519.870823	839129.297631	41.125376
3519.851548	838809.423533	41.130381
3519.901561	838484.642510	41.135386
3519.534211	838175.480202	41.140391
3519.742257	837852.153799	41.145396
3519.285223	837549.466458	41.150400
3519.362659	837250.288337	41.155405
3519.432912	836928.743861	41.160410
3519.021747	836613.607817	41.165415
3519.073983	836304.042160	41.170420
3518.751729	836011.315334	41.175424
3518.564030	835700.198091	41.180429
3518.559172	835393.038834	41.185434
3518.474413	835108.823944	41.190439
3518.515835	834801.628883	41.195444
3518.531579	834498.134163	41.200448
3518.353953	834193.924611	41.205453
3518.302085	833895.734944	41.210458
3517.876485	833608.678001	41.215463
3517.427521	833299.978495	41.220468
3517.617552	832995.798510	41.225472
3517.377531	832713.115417	41.230477
3517.503644	832422.007850	41.235482
3517.339112	832128.932512	41.240487
3517.501898	831842.237632	41.245492
3517.315038	831580.060325	41.250496
3516.849894	831279.913276	41.255501
3516.866906	831001.558606	41.260506
3516.846221	830726.862275	41.265511
3517.007072	830447.336562	41.270516
3516.429459	830167.334187	41.275520
3516.451956	829886.536883	41.280525
3516.705201	829609.793910	41.285530
3516.360637	829343.399173	41.290535
3516.262013	829062.928413	41.295540
3515.953698	828794.746120	41.300544
3515.882581	828522.799597	41.305549
3516.182025	828248.092739	41.310554
3515.982639	827991.540061	41.315559
3515.824439	827728.323361	41.320564
3515.372677	827465.291067	41.325568
3515.240185	827215.930964	41.330573
3515.682659	826945.838421	41.335578
3515.097265	826687.098538	41.340583
3515.164683	826430.489678	41.345588
3515.016469	826174.639628	41.350592
3514.869725	825914.281506	41.355597
3514.638121	825670.696915	41.360602
3514.290125	825429.078211	41.365607
3514.686331	825183.123057	41.370612
3514.510546	824941.018013	41.375616
3514.260690	824699.992046	41.380621
3514.517602	824456.477657	41.385626
3514.090279	824211.844418	41.390631
3514.290877	823960.105357	41.395636
3514.102362	823735.661506	41.400640
3514.059890	823495.290952	41.405645
3513.889947	823250.530784	41.410650
3513.657959	823018.293089	41.415655
3513.691818	822781.894750	41.420660
3513.639050	822553.866668	41.425664
3513.325845	822333.211094	41.430669
3513.276855	822098.807584	41.435674
3513.000119	821877.984085	41.440679
3513.287582	821641.307590	41.445684
3513.186144	821432.915369	41.450688
3513.152202	821204.397454	41.455693
3513.037032	820981.609441	41.460698
3513.162977	820755.300352	41.465703
3513.038169	820530.492752	41.470708
3513.017853	820307.079348	41.475712
3512.579042	820092.584236	41.480717
3512.547102	819878.308798	41.485722
3512.164389	819666.824660	41.490727
3512.548910	819468.224819	41.495732
3512.243919	819254.365786	41.500736
3512.110742	819036.703160	41.505741
3512.148280	818830.262023	41.510746
3511.743647	818618.748243	41.515751
3511.842004	818413.703574	41.520756
3511.616470	818214.726407	41.525760
3511.666768	818015.355243	41.530765
3511.611322	817820.401015	41.535770
3511.406366	817625.123074	41.540775
3511.613991	817424.337752	41.545780
3511.614574	817237.385510	41.550784
3511.348060	817035.638599	41.555789
3511.430083	816849.151659	41.560794
3511.407224	816652.738318	41.565799
3511.178895	816456.695783	41.570804
3511.068728	816260.236367	41.575808
3510.640862	816086.542048	41.580813
3510.749535	815890.966057	41.585818
3510.748036	815707.496888	41.590823
3510.936114	815522.963190	41.595828
3510.402127	815334.381105	41.600832
3510.573757	815156.842448	41.605837
3510.867114	814972.178358	41.610842
3510.222798	814797.898730	41.615847
3510.435943	814616.127410	41.620852
3510.363612	814440.568963	41.625856
3510.400079	814267.044992	41.630861
3510.167305	814089.152992	41.635866
3510.072804	813920.784239	41.640871
3510.132018	813740.826856	41.645876
3509.781599	813576.263062	41.650880
3509.846488	813404.328569	41.655885
3510.259161	813236.398001	41.660890
3509.654743	813081.856509	41.665895
3509.850662	812901.413380	41.670900
3509.320278	812732.156054	41.675904
3509.530941	812567.181333	41.680909
3509.529324	812405.078917	41.685914
3509.245182	812248.310091	41.690919
3509.258036	812087.422436	41.695924
3509.472413	811935.071440	41.700928
3508.900939	811787.010906	41.705933
3509.434936	811622.988786	41.710938
3509.009196	811470.536804	41.715943
3509.100655	811308.539801	41.720948
3508.909587	811153.837180	41.725952
3508.977318	810993.894490	41.730957
3509.166798	810848.628067	41.735962
3508.741843	810698.902622	41.740967
3508.896997	810542.413991	41.745972
3508.696087	810388.283573	41.750976
3508.693634	810240.487575	41.755981
3508.809187	810098.696625	41.760986
3508.380563	809944.103584	41.765991
3508.414434	809801.241738	41.770996
3508.708887	809660.539369	41.776000
3508.578377	809517.404589	41.781005
3508.340717	809370.069512	41.786010
3508.059148	809230.923472	41.791015
3508.362948	809081.924594	41.796020
3508.129801	808941.441315	41.801024
3507.884345	808810.809174	41.806029
3507.832654	808666.565206	41.811034
3507.790397	808541.923405	41.816039
3507.714071	808401.109060	41.821044
3507.666731	808276.022079	41.826048
3507.425109	808142.190280	41.831053
3507.635194	808015.242389	41.836058
3507.516506	807891.679758	41.841063
3507.838615	807758.286820	41.846068
3507.548864	807624.697922	41.851072
3507.491918	807510.579749	41.856077
3507.495152	807381.546119	41.861082
3507.254231	807259.364897	41.866087
3507.379326	807127.560944	41.871092
3507.372199	807008.033209	41.876096
3507.116729	806886.387029	41.881101
3507.347384	806765.099881	41.886106
3507.260175	806647.295075	41.891111
3507.145865	806516.450374	41.896116
3506.966752	806405.569970	41.901120
3506.955225	806285.540031	41.906125
3507.124875	806164.448436	41.911130
3506.775445	806048.932096	41.916135
3506.715550	805934.395864	41.921140
3506.709864	805811.708751	41.926144
3506.906480	805704.187667	41.931149
3506.710843	805583.145984	41.936154
3506.596543	805475.427341	41.941159
3506.647902	805364.737345	41.946164
3506.574310	805261.177002	41.951168
3506.403093	805147.136378	41.956173
3506.644350	805026.405250	41.961178
3506.117464	804920.658506	41.966183
3506.281644	804814.698218	41.971188
3506.348202	804707.379137	41.976192
3506.043721	804617.628564	41.981197
3506.197266	804506.270334	41.986202
3505.625247	804418.719244	41.991207
3506.019899	804318.157492	41.996212
3505.951695	804220.122903	42.001216
3505.687327	804122.070180	42.006221
3506.232155	804015.593460	42.011226
3505.753500	803926.402103	42.016231
3505.887290	803826.072340	42.021236
3506.070726	803729.068427	42.026240
3505.655929	803642.855006	42.031245
3505.956129	803535.479184	42.036250
3505.896788	803436.401881	42.041255
3505.993464	803330.380832	42.046260
3505.909256	803240.625086	42.051264
3505.683326	803149.517966	42.056269
3505.781456	803053.352548	42.061274
3505.364625	802956.534761	42.066279
3505.646119	802866.419573	42.071284
3505.726901	802775.355109	42.076288
3505.310175	802690.111257	42.081293
3505.443095	802575.781738	42.086298
3505.471485	802493.700068	42.091303
3505.308363	802386.628005	42.096308
3505.238257	802310.055186	42.101312
3504.896256	802222.732681	42.106317
3505.321675	802141.709862	42.111322
3505.063845	802067.324029	42.116327
3505.172274	801986.842241	42.121332
3505.075736	801894.912246	42.126336
3505.137042	801810.216637	42.131341
3505.165978	801727.635140	42.136346
3505.315530	801656.219844	42.141351
3504.701925	801569.767954	42.146356
3505.113076	801483.636863	42.151360
3504.913367	801405.603369	42.156365
3504.944276	801321.986289	42.161370
3504.714289	801244.201306	42.166375
3504.879866	801166.104947	42.171380
3504.744383	801089.185907	42.176384
3504.614417	801017.270299	42.181389
3504.793128	800917.970493	42.186394
3504.566092	800848.424540	42.191399
3504.476044	800772.083360	42.196404
3504.209460	800702.493385	42.201408
3504.432153	800638.563685	42.206413
3504.473515	800571.375330	42.211418
3504.367638	800498.812421	42.216423
3504.489072	800426.652985	42.221428
3504.247648	800357.398927	42.226432
3504.547313	800285.699421	42.231437
3504.637458	800218.254237	42.236442
3504.590433	800132.132773	42.241447
3504.451244	800060.503230	42.246452
3504.339016	799991.371474	42.251456
3504.184460	799910.761684	42.256461
3504.571694	799843.263926	42.261466
3504.429110	799787.533642	42.266471
3504.164378	799711.553132	42.271476
3504.201441	799645.338128	42.276480
3504.163703	799580.018265	42.281485
3504.040380	799518.245726	42.286490
3504.246145	799456.173025	42.291495
3504.111637	799381.688989	42.296500
3504.354545	799310.921346	42.301504
3504.097405	799249.512041	42.306509
3504.089531	799175.446685	42.311514
3503.537456	799118.649570	42.316519
3503.797327	799056.073552	42.321524
3503.876850	798989.403555	42.326528
3503.708700	798947.316318	42.331533
3503.960487	798887.537970	42.336538
3503.808594	798820.168189	42.341543
3503.828440	798770.587840	42.346548
3503.791632	798709.726517	42.351552
3503.923869	798648.247772	42.356557
3504.126705	798581.160862	42.361562
3503.810901	798521.620132	42.366567
3503.478881	798464.486902	42.371572
3503.833410	798401.889424	42.376576
3503.698983	798344.231772	42.381581
3503.574960	798289.713674	42.386586
3503.341236	798234.869588	42.391591
3503.658970	798179.786966	42.396596
3503.778998	798139.414640	42.401600
3503.847469	798068.957672	42.406605
3503.670061	798000.160523	42.411610
3503.503369	797957.821611	42.416615
3503.368887	797901.878535	42.421620
3503.593813	797844.992139	42.426624
3503.531964	797794.043706	42.431629
3503.722870	797732.645420	42.436634
3503.599434	797692.556083	42.441639
3503.410946	797636.963438	42.446644
3503.648646	797589.400775	42.451648
3503.402282	797536.762545	42.456653
3503.443632	797473.177337	42.461658
3502.996230	797434.760033	42.466663
3503.269169	797383.017021	42.471668
3503.428822	797332.470603	42.476672
3503.297098	797294.835172	42.481677
3503.625200	797218.828030	42.486682
3503.321783	797182.889583	42.491687
3503.221870	797128.996720	42.496692
3503.275872	797080.135209	42.501696
3503.122171	797032.780527	42.506701
3503.065902	796980.548682	42.511706
3503.321452	796943.093062	42.516711
3503.013287	796886.974072	42.521716
3503.223122	796842.847897	42.526720
3503.273156	796790.548024	42.531725
3502.988539	796745.029668	42.536730
3503.010361	796699.951549	42.541735
3503.239711	796654.937160	42.546740
3503.383581	796606.794062	42.551744
3502.851947	796563.033764	42.556749
3503.352256	796527.892499	42.561754
3503.002078	796480.026315	42.566759
3502.780125	796435.379467	42.571764
3502.860797	796382.285854	42.576768
3502.442798	796358.637818	42.581773
3502.687917	796317.104995	42.586778
3503.058281	796278.743049	42.591783
3502.850008	796224.124508	42.596788
3502.728603	796172.486615	42.601792
3502.860388	796152.430167	42.606797
3503.101868	796094.250095	42.611802
3502.733352	796054.289947	42.616807
3502.652824	796023.170263	42.621812
3502.949035	795982.118099	42.626816
3502.742305	795940.804793	42.631821
3502.809264	795887.955228	42.636826
3502.756897	795852.950727	42.641831
3502.773669	795814.546274	42.646836
3502.856911	795773.527970	42.651840
3502.773555	795735.286897	42.656845
3502.676865	795699.650533	42.661850
3502.336100	795671.420412	42.666855
3502.611347	795623.347139	42.671860
3502.585853	795587.060065	42.676864
3502.441711	795557.814926	42.681869
3502.619344	795521.739601	42.686874
3502.614387	795495.074059	42.691879
3502.483892	795434.396101	42.696884
3502.647693	795412.760754	42.701888
3502.500233	795370.943229	42.706893
3502.535528	795332.827750	42.711898
3502.295620	795312.781018	42.716903
3502.262094	795268.783249	42.721908
3502.541924	795242.118949	42.726912
3502.305296	795211.561599	42.731917
3502.420900	795165.181273	42.736922
3502.524591	795134.567533	42.741927
3502.269065	795111.134077	42.746932
3502.672679	795065.737008	42.751936
3502.733223	795036.947106	42.756941
3502.835085	794996.068532	42.761946
3502.426262	794973.838576	42.766951
3502.537309	794940.226884	42.771956
3502.686021	794904.300494	42.776960
3502.630611	794863.152372	42.781965
3502.547226	794832.126105	42.786970
3502.434025	794804.886405	42.791975
3502.657770	794758.583813	42.796980
3502.601487	794728.534915	42.801985
3502.353231	794688.547173	42.806989
3502.139877	794652.384445	42.811994
3502.533904	794622.162688	42.816999
3502.602989	794593.467795	42.822004
3502.344762	794550.337507	42.827009
3502.363047	794514.528842	42.832013
3502.346345	794481.869211	42.837018
3502.233436	794457.771568	42.842023
3502.332571	794422.980569	42.847028
3502.555030	794396.224282	42.852033
3502.251504	794362.088711	42.857037
3502.237110	794323.975948	42.862042
3502.507580	794291.611954	42.867047
3502.378960	794259.706493	42.872052
3502.689322	794224.585013	42.877057
3502.406975	794193.883412	42.882061
3502.587718	794158.635599	42.887066
3502.549656	794135.850730	42.892071
3502.286356	794099.103956	42.897076
3502.549622	794062.663212	42.902081
3502.431851	794045.932859	42.907085
3502.487011	793999.554807	42.912090
3502.327767	793975.266664	42.917095
3502.336088	793941.519765	42.922100
3502.397415	793900.788867	42.927105
3502.193866	793880.732057	42.932109
3502.375930	793839.244107	42.937114
3502.078082	793809.869647	42.942119
3502.002466	793792.493173	42.947124
3502.136948	793750.423083	42.952129
3501.956035	793742.347793	42.957133
3502.273339	793716.261006	42.962138
3502.242009	793677.410707	42.967143
3502.438220	793645.448957	42.972148
3502.200666	793620.533900	42.977153
3501.834002	793591.464597	42.982157
3502.332915	793562.989443	42.987162
3502.084977	793539.795110	42.992167
3502.032256	793507.284261	42.997172
3502.119526	793477.108128	43.002177
3502.212618	793449.190595	43.007181
3502.086257	793428.530298	43.012186
3502.143523	793396.885051	43.017191
3501.972527	793368.568582	43.022196
3501.913173	793338.612505	43.027201
3502.241102	793316.305069	43.032205
3502.331407	793292.612087	43.037210
3502.101342	793280.467010	43.042215
3501.716612	793237.054761	43.047220
3502.093163	793219.946272	43.052225
3501.925669	793193.495281	43.057229
3502.176861	793169.480632	43.062234
3502.068975	793139.728207	43.067239
3502.121793	793116.777696	43.072244
3502.233541	793084.385184	43.077249
3501.705740	793070.028981	43.082253
3501.793004	793035.626101	43.087258
3502.060153	793022.956542	43.092263
3501.950456	792994.972362	43.097268
3502.284001	792965.785140	43.102273
3501.793478	792948.720563	43.107277
3501.869317	792924.783094	43.112282
3501.881855	792905.179184	43.117287
3502.032840	792882.752144	43.122292
3502.070491	792850.518148	43.127297
3501.927790	792820.720984	43.132301
3502.130479	792795.239213	43.137306
3502.163558	792779.709210	43.142311
3501.730573	792738.365226	43.147316
3501.679675	792718.083446	43.152321
3501.764667	792707.654119	43.157325
3502.087889	792671.294575	43.162330
3501.890649	792663.515510	43.167335
3502.008154	792627.287884	43.172340
3502.169842	792608.199005	43.177345
3501.932647	792576.549455	43.182349
3502.117488	792558.881391	43.187354
3502.385051	792531.570180	43.192359
3502.108988	792508.622735	43.197364
3502.004780	792480.144309	43.202369
3501.743049	792471.982611	43.207373
3502.215803	792431.322856	43.212378
3501.647007	792422.376457	43.217383
3501.778182	792399.656364	43.222388
3502.172913	792378.464980	43.227393
3501.926132	792351.237795	43.232397
3501.929445	792317.582216	43.237402
3502.421741	792303.695130	43.242407
3501.892028	792282.459203	43.247412
3502.067224	792238.015073	43.252417
3501.510690	792229.066408	43.257421
3501.693900	792197.247645	43.262426
3501.646821	792190.082043	43.267431
3501.790890	792171.289683	43.272436
3501.996780	792137.698146	43.277441
3501.951388	792134.168032	43.282445
3502.021601	792097.896351	43.287450
3501.701292	792081.047297	43.292455
3501.798075	792050.470439	43.297460
3502.173770	792022.598987	43.302465
3501.905682	792011.686324	43.307469
3501.840499	791982.413324	43.312474
3501.970340	791960.085111	43.317479
3501.630069	791936.655042	43.322484
3502.101489	791902.576445	43.327489
3501.994876	791895.666023	43.332493
3502.113195	791874.174721	43.337498
3502.147350	791842.673725	43.342503
3501.585133	791835.494346	43.347508
3501.713810	791794.396261	43.352513
3501.682228	791781.675420	43.357517
3501.715831	791754.596291	43.362522
3501.959633	791734.607095	43.367527
3501.504804	791723.429931	43.372532
3502.124976	791705.786305	43.377537
3501.671251	791683.160254	43.382541
3501.747430	791670.765415	43.387546
3501.903032	791641.995136	43.392551
3501.703893	791617.214084	43.397556
3501.629409	791587.695301	43.402561
3501.471035	791575.781160	43.407565
3501.590029	791567.604839	43.412570
3501.581827	791539.991271	43.417575
3501.232432	791524.521512	43.422580
3501.613444	791514.336491	43.427585
3501.352269	791507.942519	43.432589
3501.750294	791489.253931	43.437594
3501.868142	791473.363136	43.442599
3501.820632	791447.622903	43.447604
3501.882999	791429.431684	43.452609
3501.688297	791415.852575	43.457613
3501.686591	791379.048542	43.462618
3502.023195	791377.813755	43.467623
3501.737775	791352.751159	43.472628
3502.035188	791318.993251	43.477633
3501.969465	791307.161672	43.482637
3501.870614	791291.748411	43.487642
3501.812559	791264.387675	43.492647
3501.726278	791231.233076	43.497652
3501.783125	791217.169900	43.502657
3501.481028	791203.362378	43.507661
3501.582106	791181.920956	43.512666
3501.736472	791171.969335	43.517671
3501.429516	791144.993111	43.522676
3501.605911	791121.868354	43.527681
3502.058401	791113.538299	43.532685
3501.936417	791082.010499	43.537690
3501.897339	791069.240472	43.542695
3501.790650	791040.609237	43.547700
3501.652002	791022.597506	43.552705
3501.756702	790995.995172	43.557709
3501.756787	790982.874554	43.562714
3501.687123	790972.124162	43.567719
3501.582851	790938.528889	43.572724
3501.772837	790916.973740	43.577729
3501.555256	790913.618804	43.582733
3501.494366	790882.080050	43.587738
3501.627155	790878.421677	43.592743
3501.461914	790865.180649	43.597748
3501.452988	790851.373290	43.602753
3501.265655	790831.845700	43.607757
3501.365661	790821.804259	43.612762
3501.706780	790805.580342	43.617767
3501.747744	790778.103134	43.622772
3501.952203	790767.208993	43.627777
3501.662498	790747.010040	43.632781
3501.535454	790720.543131	43.637786
3501.524061	790726.442085	43.642791
3501.353427	790702.144558	43.647796
3501.923548	790682.442649	43.652801
3501.372613	790676.095650	43.657805
3501.492014	790637.646104	43.662810
3501.632256	790634.428667	43.667815
3501.176497	790622.709334	43.672820
3501.299415	790605.980327	43.677825
3501.307479	790587.451889	43.682829
3501.518953	790575.868291	43.687834
3501.412464	790576.917816	43.692839
3501.461572	790564.476360	43.697844
3501.527123	790534.291255	43.702849
3501.478753	790543.095941	43.707853
3501.689866	790523.747590	43.712858
3501.807284	790499.057913	43.717863
3501.277551	790483.074993	43.722868
3501.554384	790475.608580	43.727873
3501.507485	790448.292001	43.732877
3501.324053	790429.696405	43.737882
3501.476488	790421.365823	43.742887
3501.122775	790414.396365	43.747892
3501.647941	790390.130594	43.752897
3501.356904	790391.505413	43.757901
3501.582578	790373.235442	43.762906
3501.509989	790350.296620	43.767911
3501.605927	790337.945343	43.772916
3501.851607	790319.671939	43.777921
3501.272002	790296.963894	43.782925
3501.247160	790285.762768	43.787930
3501.583153	790280.399667	43.792935
3501.431844	790272.610399	43.797940
3501.474334	790245.917211	43.802945
3501.551707	790242.955683	43.807949
3501.150299	790228.081403	43.812954
3501.484638	790206.647761	43.817959
3501.478572	790196.328031	43.822964
3501.898657	790177.779805	43.827969
3501.463549	790160.355324	43.832973
3501.457485	790143.351594	43.837978
3501.444656	790129.592620	43.842983
3501.364392	790117.958039	43.847988
3501.494977	790086.679091	43.852993
3501.646603	790094.075275	43.857997
3501.311260	790066.116679	43.863002
3501.745044	790045.550820	43.868007
3501.648980	790039.767233	43.873012
3502.027164	790026.533421	43.878017
3501.600500	789996.476255	43.883021
3501.494124	789968.676151	43.888026
3501.414060	789955.271949	43.893031
3501.451618	789951.530492	43.898036
3502.070689	789922.676905	43.903041
3501.795839	789918.102223	43.908045
3501.601391	789888.497831	43.913050
3501.676320	789880.277680	43.918055
3501.503425	789848.163000	43.923060
3501.497037	789831.650065	43.928065
3501.606360	789833.401381	43.933069
3501.426757	789809.495464	43.938074
3501.753243	789788.553347	43.943079
3501.391495	789790.824608	43.948084
3501.562537	789752.509214	43.953089
3501.749059	789746.629693	43.958093
3501.581939	789730.044698	43.963098
3501.572173	789710.828819	43.968103
3501.360025	789704.621734	43.973108
3501.396845	789687.659000	43.978113
3501.560509	789679.424001	43.983117
3501.651054	789644.610920	43.988122
3501.530241	789644.876539	43.993127
3501.219792	789631.018173	43.998132
3501.356847	789595.312486	44.003137
3501.545453	789593.118772	44.008141
3501.444350	789589.105062	44.013146
3501.428386	789564.778164	44.018151
3501.514284	789545.152875	44.023156
3501.818700	789533.208219	44.028161
3501.508976	789517.924138	44.033165
3501.213543	789497.771719	44.038170
3501.287358	789497.268019	44.043175
3501.385577	789487.814803	44.048180
3501.555974	789467.585568	44.053185
3501.369792	789460.980782	44.058189
3501.272765	789444.924240	44.063194
3501.254898	789441.732310	44.068199
3501.032970	789430.463996	44.073204
3501.046051	789405.148738	44.078209
3501.258807	789404.818752	44.083213
3501.190958	789398.489327	44.088218
3501.234984	789397.007493	44.093223
3501.372980	789396.050849	44.098228
3501.458044	789362.859299	44.103233
3501.537172	789353.654809	44.108237
3501.366131	789347.735552	44.113242
3501.584488	789336.640327	44.118247
3501.089672	789314.849057	44.123252
3501.383467	789306.936259	44.128257
3501.069414	789314.508266	44.133261
3501.512813	789302.835245	44.138266
3501.120392	789277.930394	44.143271
3501.078874	789274.398216	44.148276
3501.243874	789259.576063	44.153281
3501.168768	789258.212128	44.158285
3501.251964	789248.220388	44.163290
3501.273451	789221.575967	44.168295
3501.244765	789223.694238	44.173300
3501.597980	789205.596876	44.178305
3501.338851	789211.587047	44.183309
3501.145242	789182.667717	44.188314
3501.260135	789169.623146	44.193319
3501.133873	789163.155673	44.198324
3501.116856	789144.824219	44.203329
3500.830974	789154.849428	44.208333
3501.096915	789149.054641	44.213338
3501.170107	789145.257737	44.218343
3501.134040	789121.571630	44.223348
3501.293496	789107.978916	44.228353
3501.475189	789096.053743	44.233357
3501.434056	789111.003233	44.238362
3501.728322	789065.389091	44.243367
3501.202644	789068.523197	44.248372
3501.283203	789044.276929	44.253377
3501.470232	789041.051069	44.258381
3501.269475	789022.798721	44.263386
3501.586715	789007.066189	44.268391
3501.349633	788998.552333	44.273396
3501.540968	788982.447249	44.278401
3501.392353	788961.777579	44.283405
3501.282875	788953.832508	44.288410
3501.475903	788954.390540	44.293415
3501.191958	788940.133219	44.298420
3501.435439	788914.434181	44.303425
3501.216536	788920.417969	44.308429
3501.193550	788916.833406	44.313434
3501.312557	788899.511172	44.318439
3501.047423	788891.788291	44.323444
3501.181588	788864.534112	44.328449
3501.105799	788858.992000	44.333453
3500.955081	788860.737236	44.338458
3501.405763	788863.612297	44.343463
3501.246452	788865.014859	44.348468
3501.047947	788825.428151	44.353473
3501.043413	788823.216861	44.358477
3501.279311	788812.265399	44.363482
3501.472796	788814.248885	44.368487
3500.929455	788821.171000	44.373492
3501.319549	788785.812822	44.378497
3501.255455	788773.632660	44.383501
3501.287644	788770.530496	44.388506
3501.146731	788758.559585	44.393511
3501.300783	788761.139455	44.398516
3500.955117	788745.564695	44.403521
3501.239483	788725.216269	44.408525
3501.168459	788719.624107	44.413530
3501.536766	788709.781277	44.418535
3501.347207	788709.271748	44.423540
3501.416209	788680.700374	44.428545
3501.188788	788668.792719	44.433549
3501.221465	788661.856198	44.438554
3501.456747	788657.540768	44.443559
3501.064086	788651.903219	44.448564
3501.351515	788626.097590	44.453569
3501.542647	788609.647599	44.458573
3501.439012	788618.758710	44.463578
3501.489224	788602.036971	44.468583
3501.229916	788577.500996	44.473588
3501.460182	788568.565542	44.478593
3501.408284	788565.280510	44.483597
3501.249881	788545.102817	44.488602
3501.549088	788525.242953	44.493607
3501.461029	788533.565083	44.498612
3501.714356	788512.827904	44.503617
3501.529643	788490.147339	44.508621
3501.362367	788478.524406	44.513626
3501.484797	788475.407249	44.518631
3501.440916	788456.390236	44.523636
3501.265928	788421.418281	44.528641
3501.561751	788426.727795	44.533645
3500.988388	788428.788544	44.538650
3501.208709	788404.123810	44.543655
3501.633840	788396.827436	44.548660
3501.211926	788378.806498	44.553665
3501.249152	788383.716211	44.558669
3500.976701	788373.880145	44.563674
3501.282555	788356.820770	44.568679
3501.162992	788336.291975	44.573684
3501.148861	788317.662964	44.578689
3501.248342	788324.872944	44.583693
3501.252875	788320.005411	44.588698
3501.096163	788296.287273	44.593703
3501.166079	788288.656025	44.598708
3501.471413	788275.480132	44.603713
3501.631961	788283.859922	44.608717
3501.254577	788277.236368	44.613722
3501.473441	788239.298237	44.618727
3501.135832	788249.972310	44.623732
3501.420556	788234.784190	44.628737
3501.132831	788236.847103	44.633741
3501.153218	788205.676367	44.638746
3501.191460	788185.907705	44.643751
3501.036442	788198.567343	44.648756
3501.204474	788187.134503	44.653761
3501.181313	788181.534035	44.658765
3501.095143	788167.930830	44.663770
3501.275648	788137.274183	44.668775
3501.366787	788146.206334	44.673780
3501.224849	788129.760940	44.678785
3501.187078	788142.548845	44.683789
3501.074582	788133.964270	44.688794
3501.521458	788101.051372	44.693799
3501.209814	788088.517528	44.698804
3501.218742	788084.484843	44.703809
3501.445402	788090.789218	44.708813
3501.343657	788068.683573	44.713818
3501.401106	788040.996437	44.718823
3501.249794	788043.479384	44.723828
3501.369844	788043.803707	44.728833
3501.400098	788026.199006	44.733837
3501.195444	788003.913467	44.738842
3501.590035	787988.952536	44.743847
3501.505225	787988.769829	44.748852
3501.165929	787958.493004	44.753857
3501.340652	787946.862032	44.758861
3501.102777	787940.854286	44.763866
3501.230455	787937.932679	44.768871
3500.963848	787944.662565	44.773876
3501.003790	787916.289564	44.778881
3500.788787	787900.396457	44.783885
3500.966844	787900.170449	44.788890
3500.935812	787899.978882	44.793895
3501.326211	787901.635218	44.798900
3501.335856	787892.931910	44.803905
3501.145111	787896.011348	44.808909
3501.225097	787887.788069	44.813914
3501.411039	787858.505871	44.818919
3501.133510	787866.466688	44.823924
3501.488808	787846.841513	44.828929
3501.196609	787851.609204	44.833933
3501.214364	787822.797025	44.838938
3501.256435	787800.322722	44.843943
3501.344978	787801.782989	44.848948
3501.321229	787792.347617	44.853953
3501.529631	787782.972320	44.858957
3501.411281	787783.581738	44.863962
3501.437617	787758.061795	44.868967
3501.062700	787762.204051	44.873972
3501.276824	787749.533845	44.878977
3501.399803	787711.854522	44.883981
3501.083001	787712.349144	44.888986
3501.441917	787699.949980	44.893991
3501.270195	787701.256485	44.898996
3501.514000	787678.650243	44.904001
3501.299562	787669.885246	44.909005
3501.220910	787656.623973	44.914010
3501.627282	787646.625923	44.919015
3501.461570	787634.263897	44.924020
3501.553306	787610.355063	44.929025
3501.341366	787612.307341	44.934029
3501.138084	787597.394908	44.939034
3501.331191	787576.320782	44.944039
3501.379567	787573.461254	44.949044
3501.403315	787567.016784	44.954049
3501.268089	787565.170781	44.959053
3501.395757	787538.797570	44.964058
3501.564023	787516.744070	44.969063
3501.333646	787522.190101	44.974068
3501.218139	787510.507896	44.979073
3501.751528	787479.642810	44.984077
3501.352270	787469.826380	44.989082
3501.500105	787463.410542	44.994087
3501.451113	787445.620803	44.999092
3501.379624	787429.653842	45.004097
3501.521469	787428.892968	45.009101
3501.036768	787430.398569	45.014106
3501.530826	787398.998796	45.019111
3501.207149	787388.727314	45.024116
3501.365034	787381.424767	45.029121
3501.175131	787369.705420	45.034125
3501.195827	787365.277065	45.039130
3501.357991	787349.861428	45.044135
3501.073316	787336.387666	45.049140
3500.930596	787342.311055	45.054145
3500.971300	787331.684476	45.059149
3501.243793	787334.048694	45.064154
3501.432042	787317.891202	45.069159
3501.435104	787301.075851	45.074164
3501.318838	787296.571680	45.079169
3501.647701	787287.667556	45.084173
3501.208451	787255.830890	45.089178
3501.303083	787236.984478	45.094183
3501.258228	787228.731837	45.099188
3501.363190	787228.616185	45.104193
3501.514525	787224.067890	45.109197
3501.149051	787194.185466	45.114202
3501.485944	787186.312398	45.119207
3501.345487	787193.858046	45.124212
3501.458776	787178.843427	45.129217
3501.641676	787161.014784	45.134221
3501.506435	787134.585054	45.139226
3501.472584	787128.887186	45.144231
3501.117016	787102.247791	45.149236
3501.250017	787096.473246	45.154241
3501.321191	787088.889679	45.159245
3501.275789	787088.798791	45.164250
3501.554442	787049.566140	45.169255
3501.384565	787038.137957	45.174260
3501.614297	787033.920805	45.179265
3501.742999	787030.261140	45.184269
3501.364514	787008.197796	45.189274
3501.227782	786994.944860	45.194279
3501.278086	786999.755035	45.199284
3501.132275	786984.291003	45.204289
3501.604184	786959.235668	45.209293
3501.230718	786957.920434	45.214298
3501.624676	786945.710871	45.219303
3501.326536	786935.041179	45.224308
3501.343366	786909.421436	45.229313
3501.465344	786903.402707	45.234317
3501.225358	786907.277381	45.239322
3501.151422	786884.425957	45.244327
3501.122783	786865.943056	45.249332
3501.344076	786860.497963	45.254337
3501.017403	786843.686679	45.259341
3500.676100	786850.184047	45.264346
3501.105847	786844.852114	45.269351
3500.948068	786848.172416	45.274356
3501.253851	786841.484159	45.279361
3501.276501	786812.912950	45.284365
3501.084177	786807.142590	45.289370
3501.254991	786799.640643	45.294375
3501.006157	786810.892267	45.299380
3501.142997	786799.954047	45.304385
3501.454955	786778.857998	45.309389
3501.399440	786762.641066	45.314394
3501.423736	786753.737279	45.319399
3501.291789	786766.149798	45.324404
3501.386344	786731.125164	45.329409
3501.559253	786718.656605	45.334413
3501.097369	786705.309179	45.339418
3501.113032	786698.078534	45.344423
3501.084303	786694.887163	45.349428
3500.890823	786676.529265	45.354433
3501.029545	786662.738637	45.359437
3500.664352	786666.978258	45.364442
3500.631214	786652.380018	45.369447
3501.016923	786656.250106	45.374452
3500.916908	786658.085862	45.379457
3501.277910	786662.402551	45.384461
3501.057031	786659.488668	45.389466
3501.314283	786653.004912	45.394471
3501.289787	786642.584733	45.399476
3501.197720	786627.651955	45.404481
3501.370054	786605.299952	45.409485
3501.209925	786609.899196	45.414490
3501.029077	786609.879783	45.419495
3501.041053	786579.883445	45.424500
3501.002155	786572.219119	45.429505
3500.921300	786570.118045	45.434509
3500.757276	786563.998627	45.439514
3500.889804	786569.533117	45.444519
3501.342342	786566.655786	45.449524
3501.079146	786562.027839	45.454529
3501.139220	786562.952167	45.459533
3501.009841	786537.256832	45.464538
3501.203093	786506.836957	45.469543
3500.710474	786515.129729	45.474548
3501.075530	786508.578915	45.479553
3500.875138	786494.991337	45.484557
3500.720327	786507.014698	45.489562
3501.024983	786493.884816	45.494567
3501.180963	786503.644261	45.499572
3501.025864	786503.718950	45.504577
3501.427814	786496.670331	45.509581
3501.220117	786472.315299	45.514586
3501.486354	786462.486204	45.519591
3501.735450	786459.888201	45.524596
3501.375118	786441.606356	45.529601
3501.561752	786420.726585	45.534605
3501.328687	786414.765929	45.539610
3501.436674	786397.193587	45.544615
3501.403105	786365.974545	45.549620
3501.262486	786359.752752	45.554625
3501.152010	786357.558149	45.559629
3501.093222	786361.944168	45.564634
3501.301948	786346.371185	45.569639
3501.500148	786329.963964	45.574644
3501.276225	786327.099618	45.579649
3501.369753	786318.724788	45.584653
3501.128500	786305.291098	45.589658
3501.236272	786271.097979	45.594663
3501.161781	786269.782540	45.599668
3501.159039	786265.996618	45.604673
3501.517546	786267.412734	45.609677
3501.127213	786264.280733	45.614682
3501.798374	786238.452463	45.619687
3501.533874	786237.266663	45.624692
3501.640202	786223.185485	45.629697
3501.711464	786192.981067	45.634701
3501.042516	786195.992477	45.639706
3501.169698	786182.252000	45.644711
3501.185684	786185.937376	45.649716
3501.521627	786157.016903	45.654721
3501.720177	786142.035242	45.659725
3501.464631	786139.176029	45.664730
3501.276157	786117.472027	45.669735
3501.188547	786095.948044	45.674740
3501.247859	786091.020796	45.679745
3501.461444	786084.543722	45.684749
3501.430822	786092.367483	45.689754
3501.254239	786060.629748	45.694759
3501.041550	786053.780288	45.699764
3501.135394	786044.274066	45.704769
3501.765674	786031.827327	45.709773
3501.180537	786017.515417	45.714778
3501.445824	786002.768348	45.719783
3501.403510	785991.317479	45.724788
3501.279610	785978.503122	45.729793
3501.541839	785962.035339	45.734797
3501.100975	785956.600281	45.739802
3501.180049	785947.637293	45.744807
3501.470933	785941.688289	45.749812
3501.024692	785919.632742	45.754817
3501.046327	785898.139345	45.759821
3500.766323	785841.092079	45.764826
3501.135669	785714.302988	45.769831
3501.110034	785540.218196	45.774836
3501.097151	785300.373830	45.779841
3500.966163	785015.588819	45.784845
3500.478235	784665.633276	45.789850
3500.518809	784255.664043	45.794855
3500.335353	783798.141601	45.799860
3499.904329	783270.726841	45.804865
3499.749838	782688.667849	45.809869
3499.285269	782056.476292	45.814874
3499.103661	781359.574615	45.819879
3498.716603	780617.611037	45.824884
3498.161174	779805.858676	45.829889
3497.833839	778942.786151	45.834893
3497.303373	778016.483710	45.839898
3496.981173	777025.234941	45.844903
3496.598693	775979.497528	45.849908
3495.703667	774874.496439	45.854913
3495.450715	773712.527297	45.859917
3494.679648	772498.927759	45.864922
3494.309054	771214.452186	45.869927
3493.396963	769861.486614	45.874932
3492.662232	768467.430873	45.879937
3492.304321	767000.528241	45.884941
3490.808136	765470.503820	45.889946
3490.530980	763889.755765	45.894951
3489.243511	762245.103194	45.899956
3488.695081	760550.478246	45.904961
3487.740064	758788.466852	45.909965
3486.935050	756975.816164	45.914970
3486.191117	755096.063082	45.919975
3485.220215	753159.135801	45.924980
3483.749664	751152.835260	45.929985
3483.203765	749097.927747	45.934989
3481.939827	746988.666942	45.939994
3480.998449	744815.593992	45.944999
3479.882856	742570.778060	45.950004
3478.674692	740288.384024	45.955009
3477.504468	737943.023694	45.960013
3476.233852	735540.014754	45.965018
3474.967683	733082.115032	45.970023
3473.964595	730573.446788	45.975028
3472.499095	727994.168703	45.980033
3471.400640	725373.078099	45.985037
3469.860377	722702.638412	45.990042
3468.270766	719969.252615	45.995047
3467.090100	717190.005497	46.000052
3465.475264	714338.643331	46.005057
3464.771587	711438.659593	46.010061
3462.848393	708507.745655	46.015066
3461.112483	705494.324570	46.020071
3459.349892	702432.347768	46.025076
3457.821875	699342.908924	46.030081
3456.372719	696183.590298	46.035085
3454.522873	692986.396171	46.040090
3452.930356	689716.994977	46.045095
3451.274736	686417.591855	46.050100
3449.536971	683054.349154	46.055105
3447.764921	679640.254019	46.060109
3445.882891	676181.554535	46.065114
3444.181688	672667.045968	46.070119
3442.570750	669112.455826	46.075124
3440.830795	665496.032032	46.080129
3438.788028	661831.175122	46.085133
3436.708836	658128.037680	46.090138
3434.876307	654373.055979	46.095143
3432.626362	650569.444093	46.100148
3430.734678	646730.832989	46.105153
3428.659761	642822.728621	46.110157
3426.790881	638885.080593	46.115162
3424.736968	634884.101650	46.120167
3422.606891	630855.920859	46.125172
3420.558093	626779.812285	46.130177
3418.328556	622641.401862	46.135181
3415.890961	618478.038635	46.140186
3413.990674	614245.010074	46.145191
3411.784729	609976.359710	46.150196
3409.274673	605668.153796	46.155201
3407.486332	601317.489508	46.160205
3404.771671	596933.301995	46.165210
3402.536443	592476.909350	46.170215
3400.340165	588005.977285	46.175220
3397.603748	583477.066959	46.180225
3395.552758	578907.189726	46.185229
3392.846653	574305.000559	46.190234
3390.631713	569650.670681	46.195239
3388.134994	564961.820996	46.200244
3385.311550	560236.132227	46.205249
3382.742027	555459.892270	46.210253
3380.220392	550652.517335	46.215258
3377.934877	545801.669535	46.220263
3375.278226	540928.771151	46.225268
3372.560351	535999.214068	46.230273
3370.323582	531038.474401	46.235277
3366.988206	526043.026148	46.240282
3364.699298	521000.088239	46.245287
3361.781668	515927.557465	46.250292
3359.375915	510821.409850	46.255297
3356.532847	505672.602479	46.260301
3353.369457	500495.727299	46.265306
3350.746923	495272.844248	46.270311
3347.938899	490034.279480	46.275316
3344.843309	484756.129016	46.280321
3342.245293	479434.367182	46.285325
3338.973258	474089.650513	46.290330
3336.149445	468711.832589	46.295335
3333.044085	463314.982374	46.300340
3330.320869	457879.549163	46.305345
3327.415421	452403.100547	46.310349
3323.720697	446896.904069	46.315354
3320.971333	441363.534255	46.320359
3317.922311	435828.895319	46.325364
3314.639102	430243.429828	46.330369
3311.524080	424648.048792	46.335373
3308.661833	419015.532601	46.340378
3305.466392	413353.463962	46.345383
3302.397954	407663.215737	46.350388
3298.924728	401951.001286	46.355393
3296.088160	396209.135267	46.360397
3292.353970	390451.599255	46.365402
3289.115599	384664.500934	46.370407
3285.707660	378866.999590	46.375412
3281.937180	373055.203166	46.380417
3278.703717	367208.074027	46.385421
3275.419732	361354.510379	46.390426
3272.139133	355477.200008	46.395431
3268.590690	349571.062676	46.400436
3264.844471	343660.478463	46.405441
3261.571177	337713.217846	46.410445
3257.915271	331769.217229	46.415450
3254.459865	325816.469442	46.420455
3250.789428	319828.591236	46.425460
3247.216049	313849.924326	46.430465
3243.833086	307832.259079	46.435469
3240.117306	301831.566506	46.440474
3236.579944	295797.704843	46.445479
3233.071956	289756.008594	46.450484
3229.107106	283714.301616	46.455489
3225.820535	277649.912208	46.460493
3221.607760	271584.728530	46.465498
3217.539027	265503.398731	46.470503
3214.367921	259433.027653	46.475508
3209.830027	253342.080717	46.480513
3206.277932	247244.080289	46.485517
3202.484497	241152.807377	46.490522
3198.605597	235051.687029	46.495527
3194.809746	228947.827320	46.500532
3190.526666	222847.260373	46.505537
3186.643583	216743.580365	46.510541
3182.678863	210606.102774	46.515546
3178.545108	204450.371826	46.520551
3174.651644	198349.148657	46.525556
3170.163370	192257.075158	46.530561
3166.115320	186157.655767	46.535565
3161.717225	180076.807039	46.540570
3157.550699	174004.711115	46.545575
3153.495531	167932.903948	46.550580
3148.952000	161884.306629	46.555585
3144.661884	155838.278024	46.560589
3140.228826	149813.640927	46.565594
3135.293862	143799.768633	46.570599
3131.208018	137793.677943	46.575604
3126.436866	131815.153437	46.580609
3122.044161	125857.234636	46.585613
3117.276224	119919.959475	46.590618
3112.395128	113987.778778	46.595623
3107.794319	108089.387078	46.600628
3102.636053	102235.070004	46.605633
3098.154014	96384.537349	46.610637
3092.887476	90579.197132	46.615642
3087.533077	84805.929247	46.620647
3082.755824	79057.001240	46.625652
3077.044512	73369.209266	46.630657
3071.795176	67708.293013	46.635661
3065.664066	62106.117561	46.640666
3059.874588	56549.587443	46.645671
3053.444720	51056.409588	46.650676
3046.047112	45665.430771	46.655681
3032.913243	40485.537399	46.660685
3016.297849	35531.296951	46.665690
3000.219900	30759.870915	46.670695
2984.836397	26217.309968	46.675700
2970.027507	21921.677172	46.680705
2956.222538	17905.541195	46.685709
2942.249100	14129.486951	46.690714
2928.568300	10613.667393	46.695719
2915.888155	7368.284129	46.700724
2902.772629	4389.505911	46.705729
2889.208227	1684.431264	46.710733
2839.094854	269.754872	46.715738
2757.681981	266.591362	46.720743
2714.050278	248.150030	46.725748
2705.813555	247.064901	46.730753
2721.642220	244.563303	46.735757
2745.542369	250.583439	46.740762
2766.844214	237.807918	46.745767
2781.164705	237.100881	46.750772
2786.745542	236.348302	46.755777
2786.076260	229.536762	46.760781
2781.962359	241.731776	46.765786
2776.626502	244.133256	46.770791
2772.116589	242.665295	46.775796
2768.360285	241.602795	46.780801
2765.567650	235.299474	46.785805
2763.511799	233.558246	46.790810
2760.611010	230.480474	46.795815
2758.076070	221.052854	46.800820
2755.394595	227.623825	46.805825
2752.954645	223.873882	46.810829
2749.757097	227.458376	46.815834
2746.986194	219.241738	46.820839
2743.577930	225.301806	46.825844
2740.272593	227.741177	46.830849
2737.234193	223.364167	46.835853
2734.009016	220.333378	46.840858
2730.809976	219.221349	46.845863
2727.470269	216.215267	46.850868
2724.146017	217.315996	46.855873
2721.126258	227.577357	46.860877
2717.825958	225.898458	46.865882
2714.697334	218.697116	46.870887
2711.649716	213.460542	46.875892
2708.133496	218.496381	46.880897
2704.786552	207.484616	46.885901
2701.325725	215.613170	46.890906
2697.914554	210.745840	46.895911
2694.464208	213.461407	46.900916
2691.166112	217.490088	46.905921
2687.942234	207.947303	46.910925
2684.734070	204.213846	46.915930
2681.016761	212.662517	46.920935
2677.891165	194.282228	46.925940
2674.586409	207.792264	46.930945
2671.579221	206.242943	46.935949
2668.091613	209.883181	46.940954
2664.356082	202.998099	46.945959
2660.635295	195.809583	46.950964
2657.142138	210.149235	46.955969
2653.764679	203.639714	46.960973
2650.003753	192.143955	46.965978
2647.539480	196.104129	46.970983
2644.331339	197.106917	46.975988
2640.648409	200.953108	46.980993
2637.124423	202.587894	46.985997
2633.026473	199.399852	46.991002
2630.025082	191.335039	46.996007
2626.787106	183.481202	47.001012
2623.125378	203.124639	47.006017
2619.802136	191.671965	47.011021
2616.075676	202.635997	47.016026
2612.500655	200.813118	47.021031
2608.951990	195.313609	47.026036
2606.067029	191.620133	47.031041
2602.979728	184.412147	47.036045
2599.021660	192.054142	47.041050
2595.711739	202.639414	47.046055
2592.477643	191.307121	47.051060
2588.566928	182.367299	47.056065
2585.501895	195.517379	47.061069
2582.302695	196.840148	47.066074
2578.472304	203.708435	47.071079
2574.988458	202.503635	47.076084
2570.839281	196.080366	47.081089
2567.444573	184.235008	47.086093
2564.463270	192.536210	47.091098
2561.160891	186.316062	47.096103
2557.713533	183.035985	47.101108
2554.292003	186.280698	47.106113
2550.658560	189.715941	47.111117
2547.080322	191.355568	47.116122
2543.529517	201.214489	47.121127
2539.942878	195.781262	47.126132
2536.620289	194.728068	47.131137
2533.094121	184.256331	47.136141
2530.024337	195.191922	47.141146
2526.543804	189.736373	47.146151
2523.369653	183.987804	47.151156
2519.453199	193.626536	47.156161
2516.111703	185.116872	47.161165
2512.472459	193.985050	47.166170
2508.840338	195.241508	47.171175
2505.364632	188.570191	47.176180
2501.397966	185.180921	47.181185
2498.499503	184.387131	47.186189
2494.567943	184.729767	47.191194
2491.431876	184.667252	47.196199
2488.242376	180.655161	47.201204
2484.600347	187.417243	47.206209
2481.196114	175.828249	47.211213
2477.742741	175.747721	47.216218
2474.304822	184.879179	47.221223
2470.748695	180.178240	47.226228
2467.190555	183.964264	47.231233
2463.604602	190.797909	47.236237
2460.515889	177.077267	47.241242
2456.591095	187.176850	47.246247
2453.110791	177.727006	47.251252
2449.254793	172.515248	47.256257
2446.122727	180.116396	47.261261
2442.626522	180.228622	47.266266
2438.861347	174.842262	47.271271
2435.874705	182.557851	47.276276
2431.964138	186.919868	47.281281
2428.915701	180.363219	47.286285
2425.700122	171.766349	47.291290
2421.988450	172.226964	47.296295
2418.651830	177.638974	47.301300
2414.688159	174.364890	47.306305
2411.251749	169.125595	47.311309
2408.233211	163.674040	47.316314
2404.647170	172.612104	47.321319
2400.779591	158.648802	47.326324
2396.949500	171.379199	47.331329
2393.805004	168.274299	47.336333
2390.613625	163.823439	47.341338
2387.030275	174.110617	47.346343
2383.780091	170.379699	47.351348
2379.648447	172.311336	47.356353
2376.426431	169.599063	47.361357
2373.256596	167.168934	47.366362
2369.372430	162.454571	47.371367
2365.921588	170.384457	47.376372
2362.583236	176.844726	47.381377
2358.931671	163.715005	47.386381
2355.627673	167.622243	47.391386
2351.844850	162.487170	47.396391
2348.907606	158.622084	47.401396
2344.999064	168.035219	47.406401
2341.437583	172.552412	47.411405
2337.973391	163.645468	47.416410
2334.363699	171.941245	47.421415
2331.192375	158.075377	47.426420
2327.580529	170.937723	47.431425
2323.971165	165.530075	47.436429
2320.747785	165.500777	47.441434
2317.216059	165.079257	47.446439
2313.709325	162.283643	47.451444
2309.689138	171.749244	47.456449
2306.364148	177.037042	47.461453
2303.082722	172.718573	47.466458
2299.835946	165.957922	47.471463
2296.312050	163.860492	47.476468
2292.503690	162.708659	47.481473
2289.201703	167.776704	47.486477
2285.588201	165.085926	47.491482
2281.895843	173.202382	47.496487
2279.009235	162.282587	47.501492
2274.952925	162.613847	47.506497
2271.676769	166.141427	47.511501
2268.191189	164.633489	47.516506
2264.694035	169.254844	47.521511
2261.347611	163.834448	47.526516
2257.843506	169.487440	47.531521
2254.107728	162.866264	47.536525
2250.778357	161.581093	47.541530
2247.022955	162.200249	47.546535
2243.590150	157.834168	47.551540
2239.852144	166.008976	47.556545
2236.675624	165.296470	47.561549
2233.219629	166.326098	47.566554
2229.750098	160.126101	47.571559
2225.916406	157.752355	47.576564
2222.445356	156.031507	47.581569
2219.084225	162.689445	47.586573
2215.815003	160.746873	47.591578
2212.110358	166.359656	47.596583
2208.871160	162.612310	47.601588
2205.038896	171.879735	47.606593
2201.719210	166.461469	47.611597
2198.119323	158.482968	47.616602
2194.740497	161.477590	47.621607
2191.250805	152.332537	47.626612
2187.739987	161.016360	47.631617
2183.934061	155.032589	47.636621
2180.536087	162.844902	47.641626
2177.211448	169.275350	47.646631
2173.861762	157.588462	47.651636
2170.171464	154.866806	47.656641
2166.817679	156.142726	47.661645
2163.444522	152.935654	47.666650
2159.201090	165.097868	47.671655
2156.006014	150.620397	47.676660
2152.932155	155.189043	47.681665
2149.273301	162.579816	47.686669
2145.855152	154.456729	47.691674
2142.490909	159.386813	47.696679
2139.089953	150.898918	47.701684
2135.347648	169.670576	47.706689
2131.614931	157.149496	47.711693
2128.149444	160.209447	47.716698
2124.584294	162.054386	47.721703
2121.110025	149.400910	47.726708
2117.648853	148.280892	47.731713
2113.724387	158.236898	47.736717
2110.601652	145.986575	47.741722
2107.229823	152.261351	47.746727
2104.077833	146.636120	47.751732
2100.215837	155.258129	47.756737
2096.665235	158.127910	47.761741
2093.350195	159.725017	47.766746
2089.540245	157.317042	47.771751
2086.177308	154.096088	47.776756
2083.107262	159.949549	47.781761
2079.247161	166.594446	47.786765
2075.805056	152.807433	47.791770
2071.947904	153.403898	47.796775
2068.594067	150.678295	47.801780
2065.024054	159.317567	47.806785
2061.389604	145.785167	47.811789
2058.290631	154.491075	47.816794
2054.633033	164.505397	47.821799
2051.505146	155.912913	47.826804
2048.045796	159.497932	47.831809
2044.408823	151.110782	47.836813
2040.929778	148.901998	47.841818
2037.211549	148.629572	47.846823
2033.655997	149.109316	47.851828
2030.370427	157.979205	47.856833
2026.492945	157.257719	47.861837
2023.058258	149.753254	47.866842
2019.289002	156.443369	47.871847
2016.311010	148.881033	47.876852
2012.562576	156.805284	47.881857
2009.155459	151.619578	47.886861
2005.798886	150.883305	47.891866
2002.057162	157.654917	47.896871
1998.788547	144.964436	47.901876
1995.380339	150.126967	47.906881
1991.763520	142.022341	47.911885
1988.264359	152.999592	47.916890
1984.200368	148.274571	47.921895
1981.671505	145.279827	47.926900
1977.935948	152.869193	47.931905
1974.012315	158.848906	47.936909
1970.453462	152.340680	47.941914
1966.849402	155.117327	47.946919
1963.786948	160.334615	47.951924
1960.382161	146.399455	47.956929
1956.749987	144.446934	47.961933
1953.055509	138.201134	47.966938
1949.294837	147.423890	47.971943
1946.256797	146.843067	47.976948
1942.934533	145.488991	47.981953
1938.925536	140.731841	47.986957
1935.746219	145.441877	47.991962
1932.172318	148.814784	47.996967
1928.641269	152.716436	48.001972
1925.414262	151.151310	48.006977
1921.661494	148.220381	48.011981
1918.125962	149.676651	48.016986
1914.337496	156.383201	48.021991
1911.327392	142.282824	48.026996
1907.485358	148.190007	48.032001
1904.321347	141.985763	48.037005
1900.945913	132.688061	48.042010
1897.067887	134.731425	48.047015
1893.568680	127.275671	48.052020
1889.913489	139.873593	48.057025
1886.472870	151.365489	48.062029
1883.566600	141.844670	48.067034
1879.777901	142.508967	48.072039
1876.332656	136.450783	48.077044
1872.798603	145.306960	48.082049
1869.071808	147.532473	48.087053
1865.953563	137.809267	48.092058
1861.916044	145.952640	48.097063
1858.748233	129.881487	48.102068
1855.117976	142.979945	48.107073
1851.615831	152.324455	48.112077
1847.861449	141.717558	48.117082
1844.518417	146.019657	48.122087
1841.028112	136.366038	48.127092
1837.799161	137.221746	48.132097
1834.051615	140.775279	48.137101
1830.733677	139.496213	48.142106
1827.389065	144.660356	48.147111
1823.526345	140.642951	48.152116
1820.022287	150.350849	48.157121
1816.702451	150.488238	48.162125
1813.121261	142.299898	48.167130
1809.329398	148.955159	48.172135
1806.041306	133.985564	48.177140
1803.071154	133.804019	48.182145
1799.094548	136.453968	48.187149
1795.763621	135.138488	48.192154
1792.007187	139.795317	48.197159
1788.533857	136.403009	48.202164
1784.991174	139.562072	48.207169
1781.666646	141.507168	48.212173
1778.166431	135.434527	48.217178
1774.475902	129.996978	48.222183
1771.358123	130.306652	48.227188
1767.583497	131.902086	48.232193
1763.988255	140.532312	48.237197
1760.973113	137.920768	48.242202
1757.194833	149.568954	48.247207
1753.482701	130.342920	48.252212
1749.792764	133.712856	48.257217
1746.473573	133.065841	48.262221
1743.166065	136.462755	48.267226
1739.493683	145.833421	48.272231
1736.088906	142.257177	48.277236
1732.585531	142.078796	48.282241
1729.154064	141.310024	48.287245
1725.732148	134.380969	48.292250
1722.134497	141.086897	48.297255
1718.410059	133.158441	48.302260
1715.115983	131.314723	48.307265
1711.452315	132.455810	48.312269
1708.354261	130.211463	48.317274
1704.705790	133.483418	48.322279
1700.958623	127.788192	48.327284
1697.221513	137.796224	48.332289
1693.783263	140.768110	48.337293
1690.494818	126.410725	48.342298
1686.762401	138.168075	48.347303
1683.570623	134.858310	48.352308
1680.186644	135.096321	48.357313
1676.508252	137.340578	48.362317
1673.070469	132.078132	48.367322
1669.615705	140.254971	48.372327
1666.105814	138.079782	48.377332
1662.838174	129.178891	48.382337
1658.862949	138.707490	48.387341
1655.354311	124.895339	48.392346
1651.871177	132.164082	48.397351
1648.706907	133.496075	48.402356
1645.240247	127.100198	48.407361
1641.586686	127.967258	48.412365
1637.984968	131.971561	48.417370
1634.194302	139.356965	48.422375
1630.728209	135.105816	48.427380
1627.490573	130.474629	48.432385
1623.957887	143.337064	48.437389
1620.341868	130.854994	48.442394
1616.975897	134.581259	48.447399
1613.813756	133.543062	48.452404
1610.574292	124.265022	48.457409
1606.354110	131.795010	48.462413
1603.203417	120.694034	48.467418
1599.254356	134.894804	48.472423
1596.008235	127.821288	48.477428
1592.358653	129.009438	48.482433
1588.798497	127.924859	48.487437
1585.230803	129.762972	48.492442
1581.698543	132.868414	48.497447
1578.340588	126.758501	48.502452
1575.025936	114.082307	48.507457
1571.535476	126.218369	48.512461
1568.282641	121.880961	48.517466
1564.294851	133.527777	48.522471
1560.607631	127.835073	48.527476
1557.330580	120.525664	48.532481
1553.998157	130.142582	48.537485
1550.566468	122.041319	48.542490
1546.904579	133.317374	48.547495
1543.409301	132.680079	48.552500
1539.994529	126.352849	48.557505
1536.331589	135.127426	48.562509
1532.736897	122.138352	48.567514
1529.351571	131.886149	48.572519
1526.187109	133.505023	48.577524
1522.514250	132.013469	48.582529
1518.791023	128.968679	48.587533
1515.297028	123.687481	48.592538
1511.650416	131.404626	48.597543
1508.043366	120.614020	48.602548
1505.072598	126.126515	48.607553
1501.234578	138.719335	48.612557
1498.225723	130.167596	48.617562
1494.337903	127.363873	48.622567
1490.842555	124.944075	48.627572
1487.416886	121.547023	48.632577
1483.757260	129.434143	48.637581
1480.178456	117.215861	48.642586
1476.839118	125.512629	48.647591
1473.283737	125.598680	48.652596
1469.727231	127.578056	48.657601
1466.380058	126.262456	48.662605
1463.009928	125.427951	48.667610
1459.271354	125.265931	48.672615
1455.716948	126.981749	48.677620
1452.602185	133.160980	48.682625
1449.136778	135.964117	48.687629
1445.832169	121.617251	48.692634
1441.449102	130.171138	48.697639
1437.977944	132.617102	48.702644
1434.925596	123.129414	48.707649
1431.276128	124.012973	48.712653
1428.145813	124.194539	48.717658
1424.473442	130.341994	48.722663
1420.797817	123.617082	48.727668
1417.472826	138.785362	48.732673
1413.802665	136.616729	48.737677
1410.431327	123.542330	48.742682
1406.695036	134.457501	48.747687
1403.080270	124.620176	48.752692
1399.795429	126.617691	48.757697
1396.070426	129.769041	48.762701
1393.108015	115.177399	48.767706
1389.380772	125.309417	48.772711
1385.544851	130.719981	48.777716
1382.279115	130.934474	48.782721
1378.654567	133.784430	48.787725
1375.236655	129.074802	48.792730
1371.420451	119.533175	48.797735
1368.154023	118.944030	48.802740
1365.040989	121.704631	48.807745
1361.293178	119.398099	48.812749
1358.062172	125.020687	48.817754
1354.013839	130.892722	48.822759
1350.284238	123.838564	48.827764
1347.401382	130.752536	48.832769
1343.557563	120.113287	48.837773
1340.398593	122.454690	48.842778
1336.384735	129.390290	48.847783
1333.178573	122.556768	48.852788
1329.887911	122.976464	48.857793
1326.525223	130.629067	48.862797
1322.584615	115.071372	48.867802
1319.305159	122.421960	48.872807
1315.734450	122.747597	48.877812
1312.486196	112.888316	48.882817
1308.885738	114.974371	48.887821
1305.749246	114.713548	48.892826
1301.637641	114.366050	48.897831
1297.899733	125.274819	48.902836
1294.715563	120.307538	48.907841
1291.284412	126.081085	48.912845
1287.645771	118.751992	48.917850
1283.933408	123.038235	48.922855
1280.164445	120.390926	48.927860
1277.283309	114.551625	48.932865
1274.104970	125.561900	48.937869
1270.460358	117.061264	48.942874
1267.118149	130.726622	48.947879
1263.204393	114.719200	48.952884
1259.457339	115.994543	48.957889
1255.464720	111.684701	48.962893
1252.815951	113.373954	48.967898
1249.168437	115.560149	48.972903
1245.382302	117.584839	48.977908
1241.901946	115.247544	48.982913
1238.515632	123.516247	48.987917
1235.465941	111.631066	48.992922
1231.947819	126.360382	48.997927
1228.121047	116.514661	49.002932
1224.889215	107.025055	49.007937
1220.920714	121.460331	49.012941
1217.780144	116.593627	49.017946
1214.227186	126.374441	49.022951
1210.397241	121.442869	49.027956
1207.127375	122.404369	49.032961
1203.524032	127.798827	49.037965
1200.064879	110.323966	49.042970
1196.677577	125.966475	49.047975
1193.414463	121.899895	49.052980
1189.733455	112.028067	49.057985
1185.973848	116.244217	49.062989
1182.738554	119.278626	49.067994
1179.081608	122.235939	49.072999
1175.346294	117.270813	49.078004
1172.365471	110.869001	49.083009
1168.608158	110.730556	49.088013
1165.317705	112.455428	49.093018
1161.272032	112.671906	49.098023
1157.608766	117.860907	49.103028
1154.274783	119.103632	49.108033
1150.537576	120.056772	49.113037
1147.651897	118.556723	49.118042
1144.307704	112.130955	49.123047
1140.812792	122.055921	49.128052
1137.165538	111.014601	49.133057
1133.296020	112.766615	49.138061
1130.158455	105.410843	49.143066
1126.661305	106.641054	49.148071
1122.925770	113.335370	49.153076
1119.826567	112.629847	49.158081
1116.374378	127.223914	49.163085
1112.817253	115.630836	49.168090
1108.903164	112.261246	49.173095
1105.383409	115.501586	49.178100
1101.729130	106.122144	49.183105
1097.856733	117.274779	49.188109
1095.108505	113.189054	49.193114
1091.777576	120.594105	49.198119
1088.108237	113.611755	49.203124
1084.497510	113.376347	49.208129
1080.958556	122.072142	49.213133
1077.602973	109.822602	49.218138
1073.873251	117.958839	49.223143
1070.305687	103.773339	49.228148
1067.390650	99.689519	49.233153
1063.634161	114.393124	49.238157
1060.059644	104.965616	49.243162
1056.669771	102.142596	49.248167
1052.826870	120.474867	49.253172
1049.310041	108.006312	49.258177
1045.819637	127.449974	49.263181
1042.836407	112.174832	49.268186
1038.937212	115.239198	49.273191
1035.483842	119.131980	49.278196
1031.520708	113.815649	49.283201
1028.178569	115.674314	49.288205
1024.994040	109.071505	49.293210
1021.597823	109.359113	49.298215
1018.078687	118.662642	49.303220
1014.724677	110.197852	49.308225
1011.147176	111.466644	49.313229
1007.659561	106.837496	49.318234
1003.969345	101.794099	49.323239
1000.025686	108.781215	49.328244
996.898048	99.484287	49.333249
993.369696	126.072141	49.338253
990.309273	104.727885	49.343258
986.451388	113.191256	49.348263
982.876017	113.075556	49.353268
979.514658	112.290160	49.358273
975.874344	114.935145	49.363277
972.112552	113.092266	49.368282
968.610089	104.579011	49.373287
965.333006	109.236607	49.378292
962.016972	111.615649	49.383297
958.616075	117.815672	49.388301
955.268611	120.089511	49.393306
951.466155	109.696266	49.398311
947.674752	114.095072	49.403316
944.141222	109.651419	49.408321
940.252762	116.313655	49.413325
937.400994	102.369563	49.418330
933.861187	112.081326	49.423335
930.386271	122.455911	49.428340
927.272342	106.953711	49.433345
923.460197	120.347330	49.438349
919.972976	108.659771	49.443354
916.416800	123.201029	49.448359
912.741334	123.268919	49.453364
909.267679	106.096873	49.458369
906.075267	112.988310	49.463373
902.231269	106.611960	49.468378
898.993772	116.638359	49.473383
895.249884	121.602445	49.478388
891.956443	102.196668	49.483393
888.012879	118.022180	49.488397
884.912006	105.846333	49.493402
881.073948	116.496757	49.498407
877.760320	114.150478	49.503412
874.412892	92.145652	49.508417
870.806935	105.352415	49.513421
867.511422	100.047106	49.518426
863.659201	103.427007	49.523431
860.589797	103.024297	49.528436
857.121326	106.181506	49.533441
852.968354	116.611750	49.538445
849.518926	109.408058	49.543450
845.965070	109.010371	49.548455
842.800199	103.170487	49.553460
839.338075	103.820779	49.558465
835.775321	112.897769	49.563469
832.293502	103.080895	49.568474
829.110498	104.275956	49.573479
825.418176	115.080316	49.578484
821.860945	117.345053	49.583489
818.186027	107.620943	49.588493
814.930892	113.764894	49.593498
811.190655	110.832044	49.598503
807.898818	106.648870	49.603508
804.437877	96.318417	49.608513
800.680706	112.183227	49.613517
797.509390	108.722842	49.618522
793.724118	103.022036	49.623527
790.046778	103.483450	49.628532
786.369003	106.962445	49.633537
783.055797	115.382239	49.638541
780.034620	114.051333	49.643546
776.210572	108.924904	49.648551
772.522508	107.468243	49.653556
769.486598	108.247473	49.658561
765.764977	103.101080	49.663565
762.055170	109.472067	49.668570
758.513250	109.412624	49.673575
755.413397	107.075305	49.678580
751.939773	98.033953	49.683585
747.843464	96.404004	49.688589
744.555021	100.602254	49.693594
741.374983	103.443146	49.698599
737.688538	116.354074	49.703604
734.348213	105.815997	49.708609
730.370758	99.530071	49.713613
726.958797	106.991565	49.718618
723.852438	104.490482	49.723623
719.907874	113.721835	49.728628
716.713893	103.808466	49.733633
712.902358	105.228333	49.738637
709.766086	102.182681	49.743642
706.649690	102.876477	49.748647
702.654487	115.334374	49.753652
699.027157	104.108727	49.758657
695.171537	114.508294	49.763661
691.852801	104.521325	49.768666
688.815178	101.895651	49.773671
685.239103	97.787407	49.778676
681.721020	94.097955	49.783681
678.150164	99.269456	49.788685
674.726846	96.548849	49.793690
671.259334	94.329021	49.798695
667.688526	105.837809	49.803700
664.158325	92.094130	49.808705
660.830061	104.977200	49.813709
656.825670	93.772033	49.818714
653.437396	98.599665	49.823719
649.739345	93.556694	49.828724
646.863005	88.795726	49.833729
643.338918	104.038346	49.838733
639.881562	99.071548	49.843738
635.911275	100.131043	49.848743
632.425618	97.319040	49.853748
628.984239	95.836420	49.858753
625.345482	99.816147	49.863757
621.887701	91.726960	49.868762
619.056355	100.445181	49.873767
615.462008	102.399762	49.878772
612.143770	91.926886	49.883777
607.996623	102.650478	49.888781
604.244499	102.653657	49.893786
600.680946	104.805898	49.898791
597.143755	102.795819	49.903796
594.346725	102.205195	49.908801
590.614121	103.633404	49.913805
587.234092	94.276192	49.918810
583.582748	104.441596	49.923815
579.983713	92.880768	49.928820
576.743852	91.839725	49.933825
573.001770	98.617958	49.938829
569.617484	101.678334	49.943834
565.882424	99.653303	49.948839
562.262119	110.972805	49.953844
559.054773	104.830802	49.958849
555.387034	108.289219	49.963853
552.106173	102.599667	49.968858
548.546561	93.716685	49.973863
544.935572	96.275163	49.978868
541.759133	95.924121	49.983873
537.976206	94.122184	49.988877
534.575173	90.036420	49.993882
530.937566	98.360033	49.998887
527.059747	99.050539	50.003892
524.089928	103.169919	50.008897
520.542744	96.968055	50.013901
517.177904	86.532240	50.018906
513.247940	87.413782	50.023911
509.560289	98.557962	50.028916
506.624554	98.174380	50.033921
502.641342	99.540049	50.038925
499.532249	95.373229	50.043930
496.012071	96.825201	50.048935
492.356218	102.554725	50.053940
489.269225	99.074359	50.058945
485.352847	94.733679	50.063949
481.865028	104.182807	50.068954
478.594134	95.453338	50.073959
474.818585	103.782797	50.078964
471.919691	92.601447	50.083969
467.929170	100.200846	50.088973
464.218103	95.251199	50.093978
461.221723	89.819361	50.098983
456.943980	99.899857	50.103988
453.980633	93.192861	50.108993
450.441399	111.843572	50.113997
446.883065	103.296856	50.119002
443.225526	97.841646	50.124007
439.490274	101.273786	50.129012
436.287897	96.072017	50.134017
433.147672	97.137666	50.139021
429.441463	94.611909	50.144026
425.957757	90.620071	50.149031
422.652836	102.169192	50.154036
419.140503	95.429185	50.159041
415.370706	102.477759	50.164045
412.056080	103.802195	50.169050
408.297793	102.278519	50.174055
404.553925	106.511118	50.179060
401.377691	89.539428	50.184065
397.544305	101.837149	50.189069
394.537963	96.032687	50.194074
390.992867	93.812711	50.199079
387.172168	101.938151	50.204084
384.003627	98.727323	50.209089
380.136061	102.387248	50.214093
376.392350	91.673448	50.219098
373.211174	92.258235	50.224103
370.130497	92.084034	50.229108
366.639361	90.980132	50.234113
362.851209	104.929495	50.239117
359.158971	107.208388	50.244122
355.618491	94.644670	50.249127
352.009896	116.405860	50.254132
348.802648	98.096708	50.259137
345.556570	105.177087	50.264141
342.075024	100.213275	50.269146
338.262472	101.182369	50.274151
334.738526	94.576632	50.279156
331.256448	96.825358	50.284161
327.855674	88.734139	50.289165
324.412043	83.724814	50.294170
320.869717	95.187207	50.299175
317.393668	92.248206	50.304180
313.855715	86.767701	50.309185
310.234689	102.206013	50.314189
306.853416	105.448238	50.319194
303.124638	98.844591	50.324199
299.268427	112.694541	50.329204
296.038195	95.930529	50.334209
292.121857	96.395597	50.339213
289.415769	89.043894	50.344218
285.907274	87.396351	50.349223
282.264697	96.804538	50.354228
278.942257	93.491729	50.359233
275.167375	104.999869	50.364237
271.660470	99.478936	50.369242
268.412120	104.587296	50.374247
264.607164	107.746722	50.379252
261.038441	97.254969	50.384257
257.865540	100.091055	50.389261
254.172017	99.500120	50.394266
250.819538	96.253455	50.399271
247.331292	89.407470	50.404276
243.759031	80.045639	50.409281
240.047943	91.215611	50.414285
236.492044	89.857294	50.419290
233.239993	95.217752	50.424295
229.327627	106.880237	50.429300
226.491774	96.591607	50.434305
222.777300	98.466404	50.439309
219.239132	96.648884	50.444314
215.904121	86.504892	50.449319
212.162158	100.384533	50.454324
208.784389	91.408983	50.459329
205.000357	104.166072	50.464333
201.573503	89.357520	50.469338
198.269450	101.453335	50.474343
194.762687	104.533243	50.479348
191.364411	91.739756	50.484353
187.823034	105.999738	50.489357
183.931282	97.285323	50.494362
180.931615	90.341683	50.499367
176.561154	100.090486	50.504372
173.631711	89.691765	50.509377
170.043777	88.271398	50.514381
166.466988	89.862532	50.519386
163.494967	83.941738	50.524391
159.532485	95.831348	50.529396
156.070408	95.285790	50.534401
152.699636	84.762300	50.539405
149.092716	88.222916	50.544410
145.501253	83.056894	50.549415
142.024110	85.681274	50.554420
138.616576	83.116308	50.559425
135.121827	84.240679	50.564429
131.512831	89.824916	50.569434
128.253959	90.421181	50.574439
124.385553	90.860970	50.579444
121.156184	83.328167	50.584449
117.464442	90.661733	50.589453
114.012222	82.562182	50.594458
111.025882	68.811420	50.599463
107.192131	82.094495	50.604468
103.579160	79.944011	50.609473
100.011335	88.287567	50.614477
96.035436	94.075699	50.619482
93.064862	84.991505	50.624487
89.496537	98.258268	50.629492
86.203712	100.513338	50.634497
81.987275	101.319553	50.639501
78.993655	95.003898	50.644506
75.762697	92.488219	50.649511
72.134315	97.178715	50.654516
68.944710	91.839291	50.659521
65.031544	91.387463	50.664525
61.525623	93.915222	50.669530
58.028356	89.181584	50.674535
54.464970	88.128272	50.679540
50.704505	86.077663	50.684545
47.425530	89.232175	50.689549
43.902122	101.918743	50.694554
40.742800	93.918420	50.699559
36.893085	99.079891	50.704564
33.797297	88.429840	50.709569
30.198891	91.169125	50.714573
26.589523	102.984077	50.719578
23.159995	89.177152	50.724583
19.418442	79.946246	50.729588
16.342805	88.351655	50.734593
12.495742	87.161253	50.739597
8.742367	88.875379	50.744602
5.284673	80.372710	50.749607
1.980419	92.901134	50.754612