Thu Jun 16 18:27:09 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
1.363997	86.804901	0.000000
1.151947	90.758518	0.005005
1.192233	85.992907	0.010010
1.049229	76.184436	0.015014
0.430367	63.750272	0.020019
0.185414	36.271879	0.025024
-0.109193	43.542689	0.030029
-0.174339	31.165820	0.035034
-0.141251	21.047512	0.040038
-1.239666	18.615151	0.045043
-1.272400	11.958676	0.050048
-1.740532	7.368265	0.055053
-2.476559	12.451331	0.060058
-2.923628	2.410805	0.065062
-3.539424	12.131102	0.070067
-3.325206	5.220528	0.075072
-3.379830	3.679079	0.080077
-3.692658	1.909690	0.085082
-3.310650	0.248140	0.090086
-3.647392	5.384593	0.095091
-3.788639	0.888739	0.100096
-4.301594	8.758046	0.105101
-4.836732	6.570892	0.110106
-4.773844	8.996665	0.115110
-5.173058	4.555082	0.120115
-5.617197	-2.580737	0.125120
-5.798345	-4.952174	0.130125
-6.212673	-0.514103	0.135130
-6.351571	-9.840578	0.140134
-6.538532	2.016837	0.145139
-6.125944	-4.228631	0.150144
-6.964450	0.917439	0.155149
-7.593284	2.681701	0.160154
-7.895421	-2.842578	0.165158
-8.264413	0.807444	0.170163
-8.413779	-3.493210	0.175168
-8.546078	2.366829	0.180173
-8.716793	-2.099589	0.185178
-8.452920	0.535068	0.190182
-8.631715	9.266544	0.195187
-8.908874	12.119652	0.200192
-9.473023	14.702025	0.205197
-10.103934	4.646696	0.210202
-9.872489	8.597343	0.215206
-9.819421	2.630299	0.220211
-10.665290	5.573344	0.225216
-11.161680	-0.786602	0.230221
-11.713744	1.986346	0.235226
-11.573555	-1.788481	0.240230
-11.437425	-0.689092	0.245235
-11.559639	-11.379955	0.250240
-11.633945	-2.859412	0.255245
-12.029747	2.536594	0.260250
-12.402674	-0.268308	0.265254
-13.124986	8.648387	0.270259
-13.248498	7.576673	0.275264
-13.564785	0.875115	0.280269
-13.188007	5.509986	0.285274
-13.297349	-4.281896	0.290278
-14.363796	4.585909	0.295283
-14.789041	8.703678	0.300288
-14.744957	-0.866825	0.305293
-15.208569	11.978270	0.310298
-14.806832	8.116416	0.315302
-14.964997	10.781357	0.320307
-15.064797	11.394990	0.325312
-15.732173	11.678796	0.330317
-16.248086	13.248201	0.335322
-15.772070	9.673784	0.340326
-16.300168	10.262798	0.345331
-16.679003	3.036177	0.350336
-17.233374	0.405889	0.355341
-18.204968	7.753338	0.360346
-17.675648	0.861232	0.365350
-17.692125	4.958112	0.370355
-18.086865	3.028924	0.375360
-17.958450	1.148734	0.380365
-18.076911	17.290170	0.385370
-18.794865	5.616883	0.390374
-19.209058	13.086203	0.395379
-19.485826	6.128517	0.400384
-19.086981	0.895643	0.405389
-19.564413	2.505351	0.410394
-19.854335	-6.832273	0.415398
-20.851505	-3.101230	0.420403
-20.934169	-2.628151	0.425408
-20.635544	12.025007	0.430413
-21.190894	16.953912	0.435418
-20.767039	10.156577	0.440422
-21.672308	15.531712	0.445427
-22.209000	8.451240	0.450432
-22.546061	11.897692	0.455437
-22.976478	14.957849	0.460442
-22.476029	4.933190	0.465446
-22.813702	10.263754	0.470451
-22.739525	12.467168	0.475456
-22.656404	11.318884	0.480461
-22.943725	12.710127	0.485466
-23.665950	2.441310	0.490470
-24.016231	9.984515	0.495475
-23.945457	12.882232	0.500480
-25.002819	-0.517750	0.505485
-25.686971	1.978300	0.510490
-25.543975	-0.330093	0.515494
-25.309126	11.498266	0.520499
-25.810006	-2.652396	0.525504
-26.211226	5.265233	0.530509
-26.176809	12.569457	0.535514
-25.847346	19.369336	0.540518
-25.829832	20.092920	0.545523
-26.597530	7.346893	0.550528
-27.000811	10.741248	0.555533
-27.597424	15.434380	0.560538
-27.631192	7.165961	0.565542
-27.686606	8.108080	0.570547
-28.207596	19.339693	0.575552
-28.375256	12.505938	0.580557
-29.040160	16.456732	0.585562
-28.682959	11.815562	0.590566
-29.133915	14.466737	0.595571
-29.280367	11.835530	0.600576
-28.978265	3.985841	0.605581
-29.579140	14.509978	0.610586
-30.124439	7.124607	0.615590
-30.390480	8.165364	0.620595
-30.518022	10.030579	0.625600
-30.558659	14.720621	0.630605
-31.285578	19.262544	0.635610
-31.701474	15.653898	0.640614
-31.952333	14.092690	0.645619
-32.129070	14.005764	0.650624
-31.791102	22.242627	0.655629
-32.662096	12.746884	0.660634
-32.596030	19.903719	0.665638
-32.739597	17.685891	0.670643
-32.616992	13.436180	0.675648
-32.957657	18.868954	0.680653
-33.470317	25.470407	0.685658
-33.599840	11.536769	0.690662
-33.935673	18.894881	0.695667
-35.138152	17.031403	0.700672
-35.146457	12.573560	0.705677
-35.198902	20.813972	0.710682
-35.017252	16.337660	0.715686
-35.300590	12.045134	0.720691
-35.218486	4.461471	0.725696
-35.300334	12.950711	0.730701
-35.961097	0.789702	0.735706
-36.341356	7.581473	0.740710
-36.840519	16.376254	0.745715
-36.638550	16.487489	0.750720
-36.991557	14.817476	0.755725
-37.457607	18.062089	0.760730
-38.026894	13.916066	0.765734
-38.017653	18.568762	0.770739
-38.743085	9.432735	0.775744
-38.828520	7.426486	0.780749
-39.140010	12.972132	0.785754
-38.598985	12.146445	0.790758
-38.755306	17.470224	0.795763
-38.888833	23.951801	0.800768
-38.585733	11.695622	0.805773
-39.723657	8.638804	0.810778
-39.966611	8.185467	0.815782
-40.224687	15.666772	0.820787
-41.036353	10.045172	0.825792
-41.392961	11.931965	0.830797
-41.391425	22.839962	0.835802
-41.507363	18.609251	0.840806
-41.971116	21.581296	0.845811
-42.470761	14.559419	0.850816
-42.118034	22.071786	0.855821
-42.443388	15.808470	0.860826
-42.021043	9.304685	0.865830
-42.408877	13.573135	0.870835
-42.903080	9.462750	0.875840
-43.323458	14.600794	0.880845
-43.535863	14.398319	0.885850
-43.418366	10.865294	0.890854
-43.866525	13.480886	0.895859
-44.373613	7.866271	0.900864
-44.366226	1.941999	0.905869
-44.637435	7.022832	0.910874
-44.844311	-0.279457	0.915878
-45.767847	9.706269	0.920883
-46.136966	12.080907	0.925888
-46.317085	21.604015	0.930893
-46.971505	10.415677	0.935898
-46.334940	7.247131	0.940902
-46.503786	12.754996	0.945907
-46.344365	4.973677	0.950912
-46.526570	0.130622	0.955917
-47.525151	18.350841	0.960922
-47.966895	7.440093	0.965926
-48.133475	8.880540	0.970931
-48.585172	24.205336	0.975936
-48.619407	12.827983	0.980941
-48.620108	11.828512	0.985946
-48.531458	11.524490	0.990950
-48.456641	13.060398	0.995955
-49.497164	5.616289	1.000960
-49.618172	5.252207	1.005965
-50.048833	18.666525	1.010970
-49.936320	14.711685	1.015974
-50.090807	1.974821	1.020979
-50.673970	13.182667	1.025984
-51.337736	21.280034	1.030989
-51.661834	21.744871	1.035994
-51.429981	16.383714	1.040998
-51.773475	22.019002	1.046003
-51.851038	19.566320	1.051008
-51.660266	19.725377	1.056013
-52.188343	19.178873	1.061018
-52.507722	8.672810	1.066022
-52.985079	15.093608	1.071027
-53.064809	11.145087	1.076032
-53.282171	7.000890	1.081037
-53.669006	9.474347	1.086042
-53.834197	11.368476	1.091046
-54.388647	16.695898	1.096051
-54.693669	14.078170	1.101056
-54.882367	12.394915	1.106061
-55.144137	11.166894	1.111066
-54.618648	5.758989	1.116070
-55.037002	16.160031	1.121075
-55.675248	20.032332	1.126080
-56.046046	13.832959	1.131085
-56.123525	20.177907	1.136090
-56.126367	7.126131	1.141094
-56.493939	28.542773	1.146099
-56.783589	25.267731	1.151104
-57.376667	12.975172	1.156109
-57.914251	15.388898	1.161114
-57.659012	5.811418	1.166118
-57.753785	13.824416	1.171123
-57.561912	15.172477	1.176128
-58.403278	18.033492	1.181133
-59.442839	16.237705	1.186138
-59.273876	10.868791	1.191142
-59.501462	7.887353	1.196147
-59.773539	15.912981	1.201152
-59.370916	7.678499	1.206157
-59.827343	23.523887	1.211162
-59.816574	9.288271	1.216166
-59.419720	15.529572	1.221171
-60.716418	11.075605	1.226176
-60.543540	0.091802	1.231181
-60.878523	13.572087	1.236186
-61.518523	4.839554	1.241190
-62.397869	6.006235	1.246195
-62.647449	9.907333	1.251200
-61.808414	13.432595	1.256205
-62.380691	8.526146	1.261210
-62.462176	4.058401	1.266214
-62.538644	10.470165	1.271219
-62.863566	16.039932	1.276224
-63.334574	1.415532	1.281229
-63.695035	14.630108	1.286234
-63.992911	6.311618	1.291238
-64.113765	9.553639	1.296243
-64.432970	8.059765	1.301248
-64.766643	9.049943	1.306253
-65.307897	7.821447	1.311258
-65.493823	8.328759	1.316262
-65.752086	14.239016	1.321267
-65.894255	19.825444	1.326272
-65.958222	10.167235	1.331277
-65.975302	14.865517	1.336282
-65.727576	10.280027	1.341286
-66.441537	1.155828	1.346291
-67.129270	0.414133	1.351296
-67.464519	7.943013	1.356301
-67.993626	9.034646	1.361306
-67.858808	2.493144	1.366310
-68.051735	12.974229	1.371315
-67.951475	12.909203	1.376320
-67.712111	12.703691	1.381325
-68.691550	19.638096	1.386330
-69.136057	15.230540	1.391334
-69.163731	21.960200	1.396339
-69.326147	35.285409	1.401344
-69.331733	20.976226	1.406349
-70.075651	21.896285	1.411354
-70.332485	20.555376	1.416358
-70.604711	21.504619	1.421363
-70.850579	22.667435	1.426368
-70.738358	14.990495	1.431373
-70.783787	17.078123	1.436378
-71.437804	12.754817	1.441382
-71.880936	12.647299	1.446387
-72.203198	12.940371	1.451392
-72.372203	11.719118	1.456397
-72.490098	9.213221	1.461402
-72.286126	5.905736	1.466406
-72.690737	12.757273	1.471411
-73.455170	21.842238	1.476416
-73.544774	16.937508	1.481421
-74.286238	12.576367	1.486426
-73.777120	8.939849	1.491430
-74.219344	14.158652	1.496435
-74.432154	13.992057	1.501440
-74.053353	8.340743	1.506445
-75.042758	6.534303	1.511450
-75.705691	2.681675	1.516454
-75.718189	2.032308	1.521459
-75.992456	14.052530	1.526464
-76.043536	4.948806	1.531469
-76.107814	17.115753	1.536474
-75.932794	7.323441	1.541478
-76.418705	14.698461	1.546483
-77.246434	14.567195	1.551488
-77.124356	19.669753	1.556493
-77.435294	12.698184	1.561498
-77.025870	-0.488604	1.566502
-77.682151	4.710128	1.571507
-78.566629	15.056005	1.576512
-78.776255	5.294609	1.581517
-79.235322	17.254514	1.586522
-79.012021	13.323392	1.591526
-79.225954	19.009877	1.596531
-78.947818	22.485279	1.601536
-79.088965	12.839431	1.606541
-80.297530	18.462698	1.611546
-80.586778	6.993229	1.616550
-80.820632	15.466154	1.621555
-81.036117	10.761881	1.626560
-80.648206	5.942103	1.631565
-81.128421	7.574868	1.636570
-81.132387	13.116057	1.641574
-81.724758	19.003201	1.646579
-82.352357	17.412214	1.651584
-82.434302	15.248922	1.656589
-82.512913	22.691000	1.661594
-82.688236	10.667400	1.666598
-82.462960	9.790995	1.671603
-83.176997	8.859003	1.676608
-83.580522	15.378389	1.681613
-83.924528	5.320054	1.686618
-83.907658	5.099025	1.691622
-83.735253	5.630381	1.696627
-84.254226	12.472900	1.701632
-84.836700	9.117118	1.706637
-85.481092	17.057775	1.711642
-85.238752	8.164428	1.716646
-85.412219	7.032604	1.721651
-85.903948	13.706064	1.726656
-85.472763	10.210283	1.731661
-86.612976	14.295373	1.736666
-86.942506	12.263663	1.741670
-87.238904	10.370908	1.746675
-87.363719	13.268490	1.751680
-87.086620	3.318531	1.756685
-87.639564	5.893038	1.761690
-87.270535	7.675101	1.766694
-87.246851	4.775555	1.771699
-87.913830	13.818365	1.776704
-88.505916	17.079961	1.781709
-89.135800	19.628514	1.786714
-89.014464	13.098708	1.791718
-89.186427	16.384593	1.796723
-89.584536	9.304708	1.801728
-89.774897	10.519121	1.806733
-90.181853	16.528240	1.811738
-90.381605	10.307806	1.816742
-90.402867	8.600532	1.821747
-90.511859	16.838838	1.826752
-90.597678	8.444067	1.831757
-91.635024	19.209633	1.836762
-91.981493	15.138174	1.841766
-92.159833	12.799325	1.846771
-92.110613	8.483808	1.851776
-91.915392	1.513339	1.856781
-92.324160	13.778847	1.861786
-92.403166	4.621929	1.866790
-92.430545	12.501848	1.871795
-93.244353	13.381369	1.876800
-93.850718	15.049487	1.881805
-93.971238	5.074577	1.886810
-93.644599	7.342416	1.891814
-93.832931	6.446072	1.896819
-94.487871	15.129368	1.901824
-94.905959	2.658642	1.906829
-95.107383	9.174220	1.911834
-95.174701	10.664559	1.916838
-95.400268	17.442804	1.921843
-95.856504	13.393630	1.926848
-95.907499	7.038317	1.931853
-96.431300	14.564226	1.936858
-96.491688	8.740142	1.941862
-96.370470	11.939690	1.946867
-96.561791	24.814274	1.951872
-96.863842	18.770663	1.956877
-98.099786	10.321505	1.961882
-98.112304	11.615047	1.966886
-97.956097	9.905474	1.971891
-98.498545	17.339955	1.976896
-98.271097	16.962582	1.981901
-98.484936	18.402455	1.986906
-99.192868	5.457252	1.991910
-99.503449	6.610341	1.996915
-99.676794	18.486408	2.006912
-98.890080	15.399442	2.016909
-98.838230	20.115540	2.026906
-98.609342	18.484735	2.036902
-97.527652	15.065418	2.046899
-96.955454	12.277651	2.056896
-97.292731	21.222672	2.066893
-96.499714	13.386849	2.076890
-96.085080	18.384575	2.086886
-94.789187	16.777064	2.096883
-94.418819	12.289341	2.106880
-94.434263	13.697220	2.116877
-93.964429	18.006209	2.126874
-93.278959	15.556815	2.136870
-92.998515	16.850993	2.146867
-91.797093	18.054799	2.156864
-91.356959	16.971100	2.166861
-91.434249	11.279726	2.176858
-91.008149	16.467687	2.186854
-89.963845	10.751370	2.196851
-89.664905	12.101660	2.206848
-89.704123	23.053354	2.216845
-88.332787	16.953947	2.226842
-88.460970	15.316465	2.236838
-87.738494	9.787778	2.246835
-86.862937	11.266215	2.256832
-86.926117	10.988380	2.266829
-86.566218	21.752611	2.276826
-85.395463	18.449560	2.286822
-85.240978	12.499401	2.296819
-84.592447	13.115364	2.306816
-84.000534	10.512023	2.316813
-83.769012	13.535349	2.326810
-83.677730	17.851091	2.336806
-82.503919	11.863159	2.346803
-82.487132	13.883389	2.356800
-81.815646	19.294938	2.366797
-81.353434	12.556323	2.376794
-80.679340	14.022815	2.386790
-79.794031	11.947571	2.396787
-79.571169	11.511533	2.406784
-79.311302	16.582056	2.416781
-78.801409	19.600866	2.426778
-77.750255	17.021101	2.436774
-77.636634	8.551863	2.446771
-77.728996	13.881715	2.456768
-76.649914	16.532241	2.466765
-76.239960	12.425593	2.476762
-75.707308	4.584105	2.486758
-75.010088	11.883848	2.496755
-74.688750	5.180372	2.506752
-74.355544	20.696335	2.516749
-73.465053	19.435575	2.526746
-73.269619	17.500324	2.536742
-72.741121	9.905683	2.546739
-71.862583	13.686909	2.556736
-71.753085	10.832577	2.566733
-71.594708	6.341860	2.576730
-70.300989	7.042733	2.586726
-70.086682	14.801507	2.596723
-69.891619	7.053940	2.606720
-69.144799	5.600298	2.616717
-68.433012	9.375002	2.626714
-68.356118	6.151382	2.636710
-67.637862	9.382314	2.646707
-66.991899	10.164853	2.656704
-66.799728	13.184804	2.666701
-66.157027	9.662607	2.676698
-65.257785	0.632210	2.686694
-65.029119	10.575967	2.696691
-65.171994	12.984617	2.706688
-64.069522	11.588958	2.716685
-63.825237	10.951620	2.726682
-63.222191	16.798253	2.736678
-62.131408	12.712542	2.746675
-61.755966	19.791351	2.756672
-61.903494	8.826892	2.766669
-61.642400	8.569157	2.776666
-60.716217	8.850993	2.786662
-60.428018	5.496635	2.796659
-59.174073	11.713501	2.806656
-59.084944	12.293796	2.816653
-58.882889	17.261364	2.826650
-58.190061	20.155312	2.836646
-57.516091	11.104796	2.846643
-57.078478	22.274824	2.856640
-56.491616	20.135899	2.866637
-55.799031	17.670120	2.876634
-55.773871	11.794279	2.886630
-55.476551	15.055958	2.896627
-54.132712	15.310063	2.906624
-54.245218	10.618541	2.916621
-53.748706	8.182697	2.926618
-53.211453	12.623782	2.936614
-52.308135	16.351032	2.946611
-52.498538	14.813129	2.956608
-51.350545	15.091501	2.966605
-50.994238	12.271849	2.976602
-50.999058	9.383858	2.986598
-49.741143	11.606647	2.996595
-49.504502	13.967789	3.006592
-49.040707	21.559294	3.016589
-49.122271	20.395466	3.026586
-47.974780	11.897215	3.036582
-47.835188	12.929096	3.046579
-47.160647	2.119101	3.056576
-46.809387	17.808408	3.066573
-46.313669	11.824180	3.076570
-45.307280	10.052242	3.086566
-45.195607	12.863340	3.096563
-44.766159	10.607890	3.106560
-43.819514	17.043672	3.116557
-43.857809	17.966954	3.126554
-42.755327	10.070016	3.136550
-42.310678	6.811797	3.146547
-42.042990	16.394637	3.156544
-41.827462	15.660504	3.166541
-41.284474	9.237187	3.176538
-40.469731	6.859783	3.186534
-40.355640	7.926994	3.196531
-39.131990	10.175401	3.206528
-38.645456	18.459259	3.216525
-38.537953	11.319437	3.226522
-38.400533	12.144237	3.236518
-37.859387	19.696288	3.246515
-37.413932	14.597641	3.256512
-36.228240	14.397710	3.266509
-35.608504	6.598629	3.276506
-35.465622	0.426454	3.286502
-35.326308	9.553886	3.296499
-34.756358	4.753337	3.306496
-33.979248	2.004118	3.316493
-33.804249	0.464210	3.326490
-33.274933	9.690378	3.336486
-32.320286	14.633047	3.346483
-32.359344	9.687867	3.356480
-31.200019	6.091952	3.366477
-31.037808	13.720255	3.376474
-30.548802	9.041543	3.386470
-30.116568	8.047069	3.396467
-29.486780	4.199747	3.406464
-29.276608	16.392111	3.416461
-28.538046	10.176017	3.426458
-27.581761	10.124832	3.436454
-27.316973	4.671391	3.446451
-27.348374	7.909950	3.456448
-26.754735	21.191625	3.466445
-26.278594	14.641355	3.476442
-25.634852	19.671165	3.486438
-24.578876	21.465433	3.496435
-24.211772	10.670281	3.506432
-24.106159	12.153577	3.516429
-24.018640	12.329037	3.526426
-22.806946	12.132023	3.536422
-22.553598	10.939026	3.546419
-22.302763	7.489888	3.556416
-21.715191	14.034108	3.566413
-21.249136	16.405446	3.576410
-20.147420	10.533256	3.586406
-19.749475	4.725115	3.596403
-19.633952	7.793791	3.606400
-19.220187	14.401406	3.616397
-18.416731	17.481257	3.626394
-18.096727	22.538393	3.636390
-17.660412	22.750351	3.646387
-16.515560	17.939842	3.656384
-16.429549	17.535114	3.666381
-16.410284	18.684773	3.676378
-15.738902	12.213269	3.686374
-14.850601	22.726413	3.696371
-14.671066	20.407950	3.706368
-13.591136	21.120558	3.716365
-13.121146	19.159395	3.726362
-13.114949	14.896226	3.736358
-12.959343	20.752306	3.746355
-12.084383	12.563039	3.756352
-11.756843	11.965780	3.766349
-10.717612	21.072230	3.776346
-10.027291	14.984720	3.786342
-9.879127	13.608579	3.796339
-9.720519	14.282398	3.806336
-9.671712	14.079799	3.816333
-8.429885	5.406731	3.826330
-8.098758	17.259258	3.836326
-7.265206	15.993395	3.846323
-6.961911	13.525769	3.856320
-6.535298	22.738201	3.866317
-6.011147	18.857067	3.876314
-5.252978	16.602613	3.886310
-5.085734	14.729709	3.896307
-4.771185	16.281705	3.906304
-3.771894	21.497840	3.916301
-3.524450	21.632845	3.926298
-3.232214	15.504140	3.936294
-2.608174	19.243374	3.946291
-2.273338	39.218286	3.956288
-1.663778	55.007201	3.966285
-1.345763	60.254340	3.976282
-0.922105	67.582735	3.986278
-0.681027	85.030169	3.996275
-0.251237	101.901854	4.006272
0.000000	117.364492	4.011277
0.514023	126.404284	4.016282
0.607419	145.090493	4.021286
0.596576	152.123957	4.026291
0.820252	151.930608	4.031296
0.846069	159.204853	4.036301
1.352641	171.570308	4.041306
1.103519	168.576213	4.046310
1.337360	175.297159	4.051315
1.567695	183.184900	4.056320
1.275886	186.531767	4.061325
1.413354	181.476395	4.066330
1.168974	179.904725	4.071334
1.226832	182.305510	4.076339
1.559744	177.905868	4.081344
0.932833	182.444628	4.086349
1.249160	182.133563	4.091354
1.577179	186.423162	4.096358
1.236192	183.631199	4.101363
1.824398	175.275688	4.106368
1.220070	187.037560	4.111373
1.331595	183.674084	4.116378
1.061871	190.856599	4.121382
1.177861	189.973089	4.126387
1.208038	191.916838	4.131392
1.128412	189.044687	4.136397
1.248290	187.689847	4.141402
1.163446	197.506511	4.146406
1.023045	219.774285	4.151411
1.401637	208.323528	4.156416
1.896070	213.263403	4.161421
1.857541	209.965069	4.166426
1.782801	212.760789	4.171430
1.778941	222.284889	4.176435
2.037707	212.918510	4.181440
1.897175	223.908042	4.186445
1.817233	205.894486	4.191450
1.419374	201.926466	4.196454
1.452861	191.204106	4.201459
1.922582	193.100377	4.206464
1.819917	213.661175	4.211469
1.829932	194.829211	4.216474
1.479958	181.744768	4.221478
1.643427	185.431050	4.226483
1.763089	198.110262	4.231488
1.625183	211.179120	4.236493
1.724761	222.092470	4.241498
1.366256	217.789515	4.246502
1.889297	217.954539	4.251507
1.696050	209.038739	4.256512
1.824114	220.146468	4.261517
2.012545	201.631690	4.266522
1.779301	209.006779	4.271526
2.102503	214.856641	4.276531
2.431280	195.685601	4.281536
2.061033	209.489956	4.286541
1.851644	183.590432	4.291546
1.534751	203.264974	4.296550
2.102222	201.144391	4.301555
2.179314	214.887751	4.306560
1.844844	214.970236	4.311565
2.116237	191.572981	4.316570
1.679930	189.752252	4.321574
2.112899	206.212383	4.326579
2.286066	209.231237	4.331584
1.985929	193.315405	4.336589
1.700168	181.441417	4.341594
2.039987	196.223994	4.346598
1.672917	211.273458	4.351603
2.050303	211.214629	4.356608
1.651071	214.425942	4.361613
2.029957	222.616003	4.366618
2.132134	221.621911	4.371622
2.275538	219.369751	4.376627
1.987192	218.423423	4.381632
1.829490	223.869738	4.386637
1.945429	217.644791	4.391642
1.810631	227.278435	4.396646
2.160985	212.392199	4.401651
2.017733	209.333641	4.406656
1.697523	216.819393	4.411661
2.418865	228.616068	4.416666
2.254794	222.672588	4.421670
2.171578	225.558305	4.426675
2.195858	224.642101	4.431680
2.180404	220.492790	4.436685
2.466369	222.833096	4.441690
2.090832	219.150642	4.446694
2.269998	236.350937	4.451699
2.582782	235.036727	4.456704
2.247000	230.412341	4.461709
2.251426	221.643224	4.466714
2.341119	228.089185	4.471718
2.010297	242.408552	4.476723
2.535726	240.552798	4.481728
2.216021	249.821795	4.486733
2.272666	247.684597	4.491738
2.479916	238.911846	4.496742
2.703498	244.601389	4.501747
2.761284	240.098915	4.506752
2.226764	243.314241	4.511757
1.974116	238.966756	4.516762
2.209031	245.973165	4.521766
2.064740	244.807395	4.526771
2.261449	248.178517	4.531776
2.188636	256.342413	4.536781
2.018831	262.593016	4.541786
2.516604	257.692754	4.546790
2.235924	261.388127	4.551795
2.596561	263.439171	4.556800
2.664609	272.715532	4.561805
2.823871	262.056196	4.566810
2.727027	261.362153	4.571814
2.262233	244.684621	4.576819
2.715998	245.576154	4.581824
2.643516	252.919568	4.586829
2.742712	262.819217	4.591834
2.650340	260.768401	4.596838
2.712306	258.221589	4.601843
2.968736	246.658792	4.606848
2.342056	254.983867	4.611853
2.317169	254.924528	4.616858
2.824431	278.365622	4.621862
2.828625	272.817159	4.626867
3.030045	280.208750	4.631872
2.734336	272.246984	4.636877
2.956193	274.494993	4.641882
2.499030	261.235914	4.646886
2.393010	284.965023	4.651891
2.795688	263.803424	4.656896
2.143147	281.028151	4.661901
2.994314	278.785105	4.666906
2.868218	269.814763	4.671910
2.516928	283.266118	4.676915
3.063157	274.125574	4.681920
2.734523	281.619952	4.686925
3.108055	277.522957	4.691930
2.707239	282.812550	4.696934
2.801899	280.776502	4.701939
3.086470	275.029773	4.706944
2.836063	280.035635	4.711949
3.005737	281.017033	4.716954
2.698745	286.643524	4.721958
2.991810	276.315060	4.726963
3.208836	281.421851	4.731968
2.799694	274.459772	4.736973
3.162514	280.535842	4.741978
2.838445	273.783359	4.746982
2.728996	277.842599	4.751987
3.245177	273.745018	4.756992
2.932352	279.601946	4.761997
3.325383	274.651013	4.767002
3.127750	282.898395	4.772006
2.613945	274.170591	4.777011
3.285973	278.125945	4.782016
3.038352	282.098314	4.787021
3.255484	289.274609	4.792026
2.921029	279.768163	4.797030
3.425214	290.658206	4.802035
3.503165	289.076076	4.807040
2.992734	285.753303	4.812045
2.866347	286.468616	4.817050
3.395134	299.612654	4.822054
3.125571	301.125590	4.827059
3.257203	300.771151	4.832064
3.286231	311.789158	4.837069
3.520518	310.187899	4.842074
3.180425	290.094831	4.847078
3.122321	299.561350	4.852083
3.274609	298.513689	4.857088
2.845756	307.070994	4.862093
3.184633	304.158963	4.867098
3.161878	308.839629	4.872102
3.180087	311.384020	4.877107
3.322153	312.116435	4.882112
3.366702	315.875281	4.887117
3.353241	310.300223	4.892122
3.550723	311.864135	4.897126
3.437628	309.333516	4.902131
3.474048	309.151280	4.907136
3.192433	310.117875	4.912141
3.334045	303.567523	4.917146
3.259004	311.281547	4.922150
3.411999	310.437496	4.927155
3.808177	310.283810	4.932160
3.346996	313.948942	4.937165
3.307752	313.646517	4.942170
3.585143	313.680375	4.947174
3.280815	309.211775	4.952179
3.516607	303.417849	4.957184
3.226307	319.774463	4.962189
3.468142	333.513198	4.967194
3.470920	337.761187	4.972198
3.803152	348.745492	4.977203
4.077838	341.083170	4.982208
3.498947	339.156942	4.987213
3.842197	328.346202	4.992218
3.255675	322.680957	4.997222
3.459675	341.147769	5.002227
3.896628	337.552109	5.007232
3.527007	342.115780	5.012237
3.792026	345.912389	5.017242
4.052014	350.000770	5.022246
3.787128	350.802805	5.027251
4.073987	338.723867	5.032256
3.645545	340.598891	5.037261
3.792628	319.704391	5.042266
3.776044	331.930505	5.047270
3.584553	325.130735	5.052275
4.044785	322.286944	5.057280
3.635840	325.543393	5.062285
3.879316	335.524020	5.067290
4.274408	337.018479	5.072294
3.869081	330.647685	5.077299
3.853606	318.240573	5.082304
3.366522	324.809907	5.087309
3.879916	340.877261	5.092314
3.751960	337.274029	5.097318
3.874705	344.329209	5.102323
4.069696	333.729724	5.107328
3.883084	340.577643	5.112333
4.367375	344.636651	5.117338
4.361321	356.847726	5.122342
3.663583	341.171772	5.127347
3.900946	334.909743	5.132352
3.905968	343.408293	5.137357
3.750467	348.067301	5.142362
3.807616	348.674052	5.147366
3.565576	343.870074	5.152371
4.009622	346.743365	5.157376
3.906214	337.503452	5.162381
4.237124	342.203722	5.167386
4.134833	342.747536	5.172390
4.167898	353.069078	5.177395
4.101423	350.033616	5.182400
3.670205	354.520749	5.187405
3.820149	338.536308	5.192410
4.167704	345.430129	5.197414
4.428615	346.846627	5.202419
4.576805	346.908546	5.207424
4.171296	343.363807	5.212429
4.000536	341.174989	5.217434
4.079428	347.730025	5.222438
4.074631	350.704324	5.227443
4.091901	352.440580	5.232448
4.301293	351.262921	5.237453
4.002324	355.887235	5.242458
4.152200	356.581563	5.247462
4.112083	363.978283	5.252467
4.326566	370.707348	5.257472
4.166306	375.563183	5.262477
4.128998	381.891089	5.267482
4.369545	393.121928	5.272486
3.944561	379.237368	5.277491
4.656860	379.567546	5.282496
4.347376	379.720092	5.287501
4.040435	372.193827	5.292506
4.503203	379.536457	5.297510
4.019169	376.699826	5.302515
4.488373	376.202880	5.307520
4.055323	383.146297	5.312525
4.143760	388.627763	5.317530
4.532828	378.530405	5.322534
4.254798	390.638268	5.327539
4.742714	388.250226	5.332544
4.433447	393.811425	5.337549
4.125534	395.409733	5.342554
4.622439	409.685405	5.347558
4.703873	415.895933	5.352563
4.688887	406.255321	5.357568
4.781057	407.993413	5.362573
4.326153	389.709425	5.367578
4.360720	398.073783	5.372582
4.521648	410.076072	5.377587
4.980618	414.887798	5.382592
4.722674	421.426607	5.387597
4.791760	409.685888	5.392602
4.619984	403.297680	5.397606
4.161618	408.749448	5.402611
4.434248	425.882222	5.407616
4.352503	417.612037	5.412621
4.558150	424.021554	5.417626
4.770589	417.271902	5.422630
4.573014	428.296461	5.427635
4.665557	409.706021	5.432640
4.653205	410.738029	5.437645
4.688824	407.625207	5.442650
5.000617	412.919813	5.447654
4.642434	413.537685	5.452659
4.743099	421.531624	5.457664
4.869832	420.951376	5.462669
4.537155	418.310027	5.467674
4.697626	418.891123	5.472678
4.528303	430.146609	5.477683
5.050388	422.212308	5.482688
5.247107	423.023403	5.487693
4.762804	416.128335	5.492698
4.831779	419.219698	5.497702
4.555619	412.872709	5.502707
5.219085	415.788581	5.507712
4.951175	429.456353	5.512717
5.115638	422.397739	5.517722
5.054454	420.589082	5.522726
4.861587	427.031308	5.527731
4.920075	411.264153	5.532736
5.019495	424.652791	5.537741
5.113223	431.043316	5.542746
5.380827	423.914776	5.547750
4.995509	421.333921	5.552755
5.013736	414.287933	5.557760
4.727740	415.192610	5.562765
5.166350	433.638817	5.567770
5.344455	436.194394	5.572774
4.879582	442.575914	5.577779
5.399370	431.111328	5.582784
5.173877	422.590627	5.587789
4.842124	424.604278	5.592794
5.411629	425.157441	5.597798
5.073713	434.594613	5.602803
5.223560	426.408980	5.607808
5.329880	426.793028	5.612813
4.934286	425.754309	5.617818
4.961432	425.598466	5.622822
5.131610	451.639908	5.627827
5.333839	444.421333	5.632832
5.391642	452.326675	5.637837
5.176977	458.323228	5.642842
5.053768	452.306017	5.647846
5.186249	455.451217	5.652851
5.624158	443.400709	5.657856
5.139186	451.861902	5.662861
5.313324	447.040023	5.667866
5.025488	447.862825	5.672870
4.953299	451.571539	5.677875
5.095780	450.401970	5.682880
5.250553	445.273408	5.687885
5.245902	441.012841	5.692890
5.500991	443.920830	5.697894
4.688529	453.187914	5.702899
5.525135	469.520556	5.707904
5.540129	476.937130	5.712909
5.513611	491.144977	5.717914
5.526893	489.359425	5.722918
5.324642	492.804028	5.727923
5.729342	482.296364	5.732928
5.521773	489.016498	5.737933
5.468637	479.796507	5.742938
5.638766	479.773408	5.747942
5.470748	478.848122	5.752947
5.718296	476.287279	5.757952
5.755117	487.930207	5.762957
5.591381	471.591191	5.767962
5.212642	466.053847	5.772966
5.418572	485.744068	5.777971
5.899265	479.960809	5.782976
5.880735	491.627981	5.787981
5.485042	486.594416	5.792986
5.658395	489.974680	5.797990
5.460197	493.971887	5.802995
5.648084	484.576212	5.808000
5.411112	482.608556	5.813005
5.745605	488.578301	5.818010
5.950707	483.702163	5.823014
5.554412	488.505385	5.828019
5.654502	495.141334	5.833024
5.555408	491.160073	5.838029
5.865342	488.116840	5.843034
5.802561	497.334648	5.848038
5.585309	503.743248	5.853043
5.654115	486.050875	5.858048
5.711305	482.771688	5.863053
5.612644	489.291998	5.868058
5.895665	478.569737	5.873062
5.540739	486.682408	5.878067
5.842043	485.557723	5.883072
5.806048	489.258295	5.888077
5.567497	487.450231	5.893082
5.816675	493.258664	5.898086
5.790580	514.156360	5.903091
6.087341	508.439003	5.908096
6.341122	513.330346	5.913101
6.148291	504.731688	5.918106
5.473164	492.401480	5.923110
5.870665	493.758521	5.928115
6.023200	510.830336	5.933120
6.130119	502.974270	5.938125
5.891907	507.028705	5.943130
6.289869	501.632135	5.948134
6.123075	505.227254	5.953139
5.942544	505.408117	5.958144
6.144801	516.638863	5.963149
5.712670	505.606785	5.968154
5.730827	510.461592	5.973158
5.818976	518.293780	5.978163
6.176074	504.998391	5.983168
6.001114	513.951697	5.988173
5.620378	523.235186	5.993178
5.930642	520.010065	5.998182
5.812555	527.271762	6.003187
6.137599	516.000404	6.008192
6.078098	528.218277	6.013197
6.081964	537.194531	6.018202
6.388429	540.365556	6.023206
6.203943	535.061970	6.028211
6.191771	538.052422	6.033216
5.993603	548.059899	6.038221
6.296115	560.407891	6.043226
6.314568	550.787707	6.048230
6.234988	545.292157	6.053235
6.256824	540.430599	6.058240
6.229344	541.430882	6.063245
5.886606	536.812977	6.068250
6.612782	540.357816	6.073254
5.898677	525.556023	6.078259
6.084810	525.830693	6.083264
6.262175	539.073460	6.088269
6.263899	540.136498	6.093274
6.428332	548.425806	6.098278
6.142648	541.522425	6.103283
6.325026	538.243356	6.108288
6.211913	533.186658	6.113293
6.162786	530.644150	6.118298
6.548725	515.410778	6.123302
6.239850	518.142543	6.128307
6.483316	521.129716	6.133312
5.926247	512.585325	6.138317
6.162284	524.277936	6.143322
6.115855	516.372126	6.148326
5.983448	524.929003	6.153331
5.844265	517.930784	6.158336
6.194527	536.669240	6.163341
6.336340	552.772767	6.168346
6.543636	546.167752	6.173350
6.201763	530.038361	6.178355
6.137518	524.578760	6.183360
6.020480	516.225266	6.188365
6.054884	513.997192	6.193370
6.530886	530.307111	6.198374
6.059932	530.594866	6.203379
5.911090	526.755499	6.208384
6.264270	537.566489	6.213389
6.520989	543.427661	6.218394
6.368195	529.635020	6.223398
5.847233	529.503651	6.228403
6.238294	528.506790	6.233408
6.173796	537.458135	6.238413
6.312882	531.551947	6.243418
6.265968	520.236588	6.248422
6.111652	515.127115	6.253427
6.260066	515.489214	6.258432
6.275199	522.058314	6.263437
6.250765	519.398961	6.268442
6.203302	515.610227	6.273446
6.187453	527.997286	6.278451
6.565976	515.075222	6.283456
6.251912	518.336059	6.288461
6.053572	529.880449	6.293466
6.331366	514.009071	6.298470
6.066986	509.893813	6.303475
6.052877	510.400173	6.308480
5.938213	512.793410	6.313485
6.194834	519.438821	6.318490
6.369979	503.209714	6.323494
6.031080	507.121454	6.328499
6.214611	513.251910	6.333504
6.332927	520.963881	6.338509
6.217796	525.022448	6.343514
6.362937	512.172892	6.348518
6.261750	514.550683	6.353523
6.146279	520.080494	6.358528
6.307352	520.708456	6.363533
6.213465	521.589384	6.368538
6.627273	522.788841	6.373542
6.228147	525.821629	6.378547
6.345249	516.883171	6.383552
6.336099	527.408728	6.388557
6.359550	526.793747	6.393562
6.320052	526.875534	6.398566
6.316334	527.577789	6.403571
6.421428	513.242843	6.408576
6.297472	513.775050	6.413581
6.268921	526.918153	6.418586
6.564796	515.850017	6.423590
6.055941	515.544983	6.428595
6.699568	520.156140	6.433600
6.293640	507.674685	6.438605
5.991323	507.801285	6.443610
6.282938	507.330427	6.448614
6.153039	503.799695	6.453619
6.084485	509.969933	6.458624
6.122009	517.679665	6.463629
6.020565	517.577135	6.468634
6.552865	516.806441	6.473638
5.958287	519.188615	6.478643
6.415640	514.660481	6.483648
6.561402	514.579748	6.488653
6.180241	505.694630	6.493658
6.029744	500.536584	6.498662
6.228062	497.652974	6.503667
6.152158	509.221807	6.508672
5.959822	499.554604	6.513677
6.204167	503.441290	6.518682
6.251355	510.215624	6.523686
6.220324	518.509791	6.528691
6.352325	513.774472	6.533696
6.248440	506.531376	6.538701
5.896063	501.535538	6.543706
6.467919	513.834642	6.548710
6.018026	512.497273	6.553715
5.744315	520.607097	6.558720
5.704697	520.234090	6.563725
6.085759	512.708505	6.568730
6.377331	519.635827	6.573734
6.315453	535.775069	6.578739
6.464450	520.909183	6.583744
6.264073	517.048835	6.588749
6.185467	532.074718	6.593754
6.286320	518.745992	6.598758
6.243815	524.658083	6.603763
5.941392	524.628229	6.608768
6.071915	527.552083	6.613773
6.032903	525.303286	6.618778
6.394916	513.169271	6.623782
6.119629	511.552259	6.628787
6.108514	519.316005	6.633792
6.297528	525.428689	6.638797
6.137529	534.986382	6.643802
6.236460	531.264908	6.648806
6.297786	531.600456	6.653811
6.252845	530.047883	6.658816
5.828078	527.939096	6.663821
6.177297	524.988318	6.668826
6.313454	517.462160	6.673830
6.074401	529.166099	6.678835
6.081135	521.044318	6.683840
6.596399	526.003544	6.688845
6.479575	528.482776	6.693850
6.682813	519.419487	6.698854
6.325596	526.856848	6.703859
6.163262	531.982806	6.708864
6.107133	522.196789	6.713869
5.997113	525.205183	6.718874
6.094097	528.259086	6.723878
6.049309	527.111776	6.728883
6.420029	518.998612	6.733888
6.468273	525.129823	6.738893
6.375795	521.961587	6.743898
6.481680	513.442112	6.748902
6.063093	498.462959	6.753907
5.840656	487.222407	6.758912
6.366754	512.745587	6.763917
6.313433	521.656697	6.768922
6.209253	514.223434	6.773926
5.988104	519.202931	6.778931
6.143279	523.667104	6.783936
6.413116	517.301668	6.788941
6.184477	526.296508	6.793946
6.136757	527.679179	6.798950
6.129837	531.956547	6.803955
6.054524	532.428723	6.808960
6.442441	529.502528	6.813965
6.223692	541.045761	6.818970
6.478967	519.126896	6.823974
5.875072	513.629801	6.828979
6.443200	513.725324	6.833984
6.282621	493.876396	6.838989
5.939653	498.851255	6.843994
6.028600	507.387723	6.848998
6.001174	525.202295	6.854003
6.495397	519.005381	6.859008
6.515327	528.506994	6.864013
6.291876	514.657179	6.869018
6.273773	504.001237	6.874022
6.081662	500.686291	6.879027
6.125592	491.677067	6.884032
5.822893	495.890734	6.889037
6.124344	518.133278	6.894042
6.201255	518.765381	6.899046
6.217267	523.044876	6.904051
6.419924	530.164679	6.909056
6.485369	533.186601	6.914061
6.044873	513.147619	6.919066
6.150600	501.998248	6.924070
5.914350	514.237130	6.929075
6.291942	526.952521	6.934080
6.389331	517.916591	6.939085
5.983591	520.452050	6.944090
6.334747	521.898047	6.949094
6.355290	531.426199	6.954099
6.278953	510.177971	6.959104
5.973527	505.134219	6.964109
5.723453	509.946137	6.969114
6.389356	520.334681	6.974118
6.493995	521.034617	6.979123
6.294903	523.834862	6.984128
6.482793	527.187081	6.989133
6.349512	504.550876	6.994138
6.639335	495.002497	6.999142
6.141503	486.602435	7.004147
6.286225	493.833709	7.009152
6.012426	491.237964	7.014157
5.933901	501.678480	7.019162
6.265798	488.629870	7.024166
5.848522	501.313216	7.029171
6.019610	504.619469	7.034176
6.181575	499.751243	7.039181
6.028928	516.978075	7.044186
6.381139	521.289916	7.049190
6.212340	519.952859	7.054195
6.202540	514.885606	7.059200
6.053553	519.235579	7.064205
6.057378	527.634783	7.069210
6.549940	533.200071	7.074214
6.183397	529.900625	7.079219
5.930953	516.626633	7.084224
6.099747	517.989901	7.089229
6.167479	520.414561	7.094234
6.161101	513.670443	7.099238
6.029373	521.198893	7.104243
6.419717	525.113747	7.109248
6.130304	523.222530	7.114253
5.668149	529.306872	7.119258
5.828212	521.583095	7.124262
5.762452	534.041351	7.129267
6.227617	527.558194	7.134272
6.596151	529.771940	7.139277
6.390950	545.334936	7.144282
6.226022	523.468042	7.149286
6.005926	538.327494	7.154291
6.115792	526.006842	7.159296
6.261133	530.388783	7.164301
6.183770	534.604193	7.169306
6.182507	529.035919	7.174310
6.027345	529.670955	7.179315
6.307737	529.310871	7.184320
6.401123	526.338340	7.189325
6.169149	528.910792	7.194330
6.391283	525.965625	7.199334
6.281240	525.183676	7.204339
6.338107	517.930585	7.209344
6.680772	512.477245	7.214349
6.268809	521.889709	7.219354
6.432924	511.216081	7.224358
6.372410	516.362402	7.229363
6.319805	521.957891	7.234368
6.271098	512.401710	7.239373
6.288831	506.424131	7.244378
6.397189	498.620710	7.249382
5.824368	499.598441	7.254387
6.008411	498.577485	7.259392
6.000755	505.563326	7.264397
5.864105	521.506247	7.269402
6.455844	522.168211	7.274406
6.095042	529.298648	7.279411
6.222952	532.037556	7.284416
6.467403	522.694368	7.289421
6.105190	528.775119	7.294426
6.611014	521.896927	7.299430
6.351499	522.523161	7.304435
6.087620	513.823177	7.309440
6.296326	506.037601	7.314445
5.768798	496.089860	7.319450
6.327249	507.340466	7.324454
6.466118	508.139224	7.329459
6.042939	513.825644	7.334464
6.191696	501.236648	7.339469
5.900637	506.939906	7.344474
6.345622	524.020432	7.349478
6.406165	525.543756	7.354483
6.120191	513.021460	7.359488
6.295360	514.607924	7.364493
5.970476	519.918296	7.369498
6.499756	524.999120	7.374502
6.184271	513.835882	7.379507
6.055274	516.906606	7.384512
6.242402	504.837113	7.389517
6.066939	506.902395	7.394522
6.656458	511.887032	7.399526
6.514455	506.291018	7.404531
6.132781	511.254519	7.409536
6.388378	500.642338	7.414541
6.130745	500.650366	7.419546
6.422054	500.006119	7.424550
6.142740	498.753033	7.429555
5.776130	509.583109	7.434560
5.930845	494.342192	7.439565
6.050509	501.605826	7.444570
6.157191	498.572699	7.449574
6.161266	521.257936	7.454579
6.306589	525.985479	7.459584
6.464335	512.528275	7.464589
6.269660	518.517899	7.469594
6.248550	511.460608	7.474598
6.468980	507.908387	7.479603
6.283998	509.414074	7.484608
6.099120	499.604261	7.489613
5.731872	500.244747	7.494618
5.880730	489.095755	7.499622
6.096230	505.445046	7.504627
6.388502	529.483615	7.509632
6.449763	527.048654	7.514637
5.933812	506.254590	7.519642
6.103966	517.351731	7.524646
6.079582	528.326135	7.529651
6.185523	526.414868	7.534656
5.944830	512.231481	7.539661
6.094891	530.820694	7.544666
6.307287	523.182980	7.549670
6.375105	526.116801	7.554675
6.198330	534.632278	7.559680
6.214683	523.731284	7.564685
6.131869	528.875078	7.569690
6.158017	535.331275	7.574694
5.627166	527.549216	7.579699
6.027431	529.820365	7.584704
6.320352	525.778162	7.589709
6.504235	536.795503	7.594714
6.519374	522.951636	7.599718
6.383451	532.690924	7.604723
6.259427	528.228178	7.609728
6.565439	527.303678	7.614733
5.984043	515.131601	7.619738
6.366740	516.288053	7.624742
5.880403	515.655501	7.629747
6.303172	509.014993	7.634752
6.950045	525.924531	7.639757
6.158057	509.897760	7.644762
6.299381	494.544119	7.649766
6.064992	488.979755	7.654771
6.187733	502.101190	7.659776
6.367088	501.170984	7.664781
6.199727	497.973396	7.669786
6.072430	498.787133	7.674790
6.294132	486.295407	7.679795
6.333712	488.976489	7.684800
6.341507	490.405429	7.689805
6.247413	499.567739	7.694810
6.609576	499.320621	7.699814
6.194439	506.529186	7.704819
6.037604	492.803150	7.709824
6.428305	491.714499	7.714829
5.992387	498.851417	7.719834
5.965429	490.134196	7.724838
6.206376	493.431467	7.729843
6.194487	491.848475	7.734848
6.455468	481.687568	7.739853
6.246728	494.004464	7.744858
6.039356	491.498965	7.749862
6.224142	496.046930	7.754867
6.135143	495.259137	7.759872
6.280893	484.038544	7.764877
6.290446	489.816330	7.769882
6.299585	491.759450	7.774886
6.402751	496.284794	7.779891
5.948138	501.461706	7.784896
6.490341	496.526206	7.789901
6.243217	496.868724	7.794906
6.067446	493.343700	7.799910
6.161993	487.656017	7.804915
6.181036	498.182617	7.809920
5.907362	492.529638	7.814925
6.051463	500.383647	7.819930
6.076466	495.184663	7.824934
6.047439	489.284667	7.829939
6.122500	498.457993	7.834944
6.182491	487.108318	7.839949
5.856700	501.124904	7.844954
5.899370	494.980323	7.849958
5.690776	500.064882	7.854963
6.213733	512.174749	7.859968
6.535839	521.613104	7.864973
6.292534	523.500175	7.869978
6.745712	520.517913	7.874982
6.159101	504.770842	7.879987
6.105954	498.116839	7.884992
6.288603	484.545443	7.889997
6.013969	499.791336	7.895002
6.377205	500.149406	7.900006
6.309094	493.852454	7.905011
6.190116	489.712681	7.910016
6.420432	490.309172	7.915021
6.183786	503.786366	7.920026
6.390486	498.403350	7.925030
6.265033	497.697547	7.930035
5.842705	506.239776	7.935040
6.114627	492.570845	7.940045
6.133753	502.653375	7.945050
6.351210	485.753128	7.950054
6.258415	489.442368	7.955059
6.404761	497.719643	7.960064
6.218627	482.163025	7.965069
5.872596	490.185337	7.970074
6.068213	488.524152	7.975078
6.174858	493.834534	7.980083
6.068225	493.943694	7.985088
5.931303	490.532415	7.990093
5.799290	513.156271	7.995098
6.768693	513.507501	8.000102
6.419821	522.645629	8.005107
6.122685	506.633869	8.010112
6.111062	489.924966	8.015130
6.129978	507.538324	8.020147
6.034610	515.155862	8.025165
6.312180	514.807672	8.030182
6.282893	528.187114	8.035200
6.294178	525.566341	8.040218
6.433302	522.259116	8.045235
6.521177	505.025426	8.050253
6.447800	499.036618	8.055270
6.157674	505.072670	8.060288
6.502804	494.572643	8.065306
6.263757	499.211640	8.070323
6.386341	495.845159	8.075341
6.258584	489.260438	8.080358
6.285027	493.242490	8.085376
6.628666	492.951578	8.090394
6.508652	498.482343	8.095411
6.372248	496.095389	8.100429
6.298970	491.864892	8.105446
6.402474	509.140616	8.110464
6.801846	496.269576	8.115482
6.480727	507.608060	8.120499
6.576959	496.472226	8.125517
6.612031	496.602805	8.130534
6.128023	474.289944	8.135552
6.506173	471.312549	8.140570
6.452726	468.198250	8.145587
5.942933	460.152167	8.150605
5.910744	469.026319	8.155622
6.102596	487.261343	8.160640
6.297142	487.424809	8.165658
6.179547	494.378718	8.170675
5.973799	482.587617	8.175693
6.180131	485.560798	8.180710
5.989983	490.516747	8.185728
6.054819	486.249553	8.190746
5.777198	497.187610	8.195763
6.140964	504.873731	8.200781
6.052579	515.903340	8.205798
6.243540	520.543514	8.210816
6.379675	513.179685	8.215834
6.416482	521.809734	8.220851
6.072030	513.812073	8.225869
6.234877	519.713346	8.230886
6.126125	526.622312	8.235904
6.210356	521.587383	8.240922
6.211547	528.853700	8.245939
6.396772	518.656112	8.250957
6.371756	514.753397	8.255974
6.477010	529.377588	8.260992
6.625202	520.281580	8.266010
6.503471	520.782593	8.271027
6.512556	514.180660	8.276045
6.827642	519.631364	8.281062
6.279139	523.809990	8.286080
6.842328	514.568059	8.291098
6.679068	524.889221	8.296115
6.476227	518.550316	8.301133
6.754567	522.122708	8.306150
6.486957	522.023045	8.311168
6.521332	515.260762	8.316186
6.525920	520.559961	8.321203
6.367268	508.318426	8.326221
6.391585	512.343837	8.331238
6.255384	522.050210	8.336256
6.466020	525.815744	8.341274
6.319963	518.021865	8.346291
6.209017	527.303183	8.351309
6.671066	539.022999	8.356326
6.632695	549.315470	8.361344
6.467372	530.965248	8.366362
6.731016	534.228319	8.371379
6.743902	532.996584	8.376397
6.643024	527.976006	8.381414
6.673567	523.203049	8.386432
6.516124	517.397583	8.391450
6.345542	521.007062	8.396467
6.396041	525.108646	8.401485
6.818421	537.472690	8.406502
6.774755	546.565081	8.411520
6.874608	528.354372	8.416538
6.671864	524.730583	8.421555
6.548465	528.076507	8.426573
6.856245	518.204467	8.431590
6.616344	526.997645	8.436608
6.407604	531.187141	8.441626
6.699618	519.765048	8.446643
6.304419	529.829520	8.451661
6.295227	529.615906	8.456678
6.701169	550.987761	8.461696
6.849497	557.265983	8.466714
6.400971	557.186572	8.471731
6.663995	551.851173	8.476749
6.840954	547.500091	8.481766
6.253584	564.779929	8.486784
6.827866	563.213535	8.491802
6.940116	566.920943	8.496819
7.093631	561.842668	8.501837
6.933528	567.697838	8.506854
6.686043	548.552564	8.511872
7.034916	544.467801	8.516890
6.663788	533.957986	8.521907
6.475203	527.641028	8.526925
6.763753	536.731555	8.531942
6.920919	543.927625	8.536960
6.527971	540.404246	8.541978
6.610406	545.405013	8.546995
6.822281	548.565936	8.552013
6.844163	556.280239	8.557030
6.943027	553.558587	8.562048
6.601930	549.060186	8.567066
6.701647	544.409330	8.572083
6.821824	559.635498	8.577101
7.038646	552.441648	8.582119
6.405761	565.229954	8.587136
6.867491	558.993277	8.592154
6.939335	549.196224	8.597171
6.607127	560.164897	8.602189
6.799236	552.256565	8.607207
6.662813	562.616617	8.612224
6.991906	556.067867	8.617242
6.783810	553.238310	8.622259
6.469238	557.836173	8.627277
7.032679	554.253940	8.632295
6.591462	555.183367	8.637312
6.866553	561.136468	8.642330
6.801371	553.860405	8.647347
6.543727	554.877879	8.652365
6.509191	557.768264	8.657383
6.499059	561.204512	8.662400
6.859492	557.090676	8.667418
6.834835	558.686757	8.672435
6.851304	566.016008	8.677453
7.134573	557.988298	8.682471
6.644017	568.488749	8.687488
6.627705	585.104072	8.692506
6.919347	587.601548	8.697523
7.031761	595.512190	8.702541
7.177184	591.883989	8.707559
6.861777	588.523835	8.712576
7.185542	583.052427	8.717594
7.205325	568.508651	8.722611
6.279758	565.598579	8.727629
7.170661	572.078443	8.732647
7.199510	587.043207	8.737664
7.106626	574.680240	8.742682
6.729885	572.356510	8.747699
6.937106	584.795313	8.752717
7.369962	584.151629	8.757735
6.812934	581.849129	8.762752
6.889998	571.139263	8.767770
7.150069	572.821832	8.772787
6.979809	587.706430	8.777805
7.258035	586.048040	8.782823
7.106946	574.749514	8.787840
7.109250	563.157785	8.792858
6.815647	560.150070	8.797875
6.933995	569.880242	8.802893
7.020509	590.641086	8.807911
7.170006	596.738751	8.812928
7.365960	577.599970	8.817946
7.173739	578.062051	8.822963
6.876003	574.638657	8.827981
7.073839	556.146124	8.832999
6.862082	560.454313	8.838016
6.931134	585.730969	8.843034
7.466062	583.697542	8.848051
7.041089	588.313266	8.853069
7.294382	596.131545	8.858087
7.290904	584.398557	8.863104
7.220892	566.951859	8.868122
7.330237	568.701256	8.873139
7.140624	558.852932	8.878157
6.780057	561.276918	8.883175
6.845580	560.740090	8.888192
7.006296	569.554081	8.893210
7.085609	576.421757	8.898227
6.921424	586.872814	8.903245
7.003658	580.731020	8.908263
7.258903	582.411927	8.913280
7.260396	598.442344	8.918298
7.338913	587.438973	8.923315
7.339179	588.475236	8.928333
7.215204	588.242014	8.933351
7.523112	599.165749	8.938368
7.367716	587.076734	8.943386
7.563593	584.590278	8.948403
7.099518	567.366543	8.953421
6.906331	563.251690	8.958439
7.354825	594.242132	8.963456
7.074488	589.577015	8.968474
7.236309	590.674949	8.973491
7.081418	598.172665	8.978509
7.109846	591.833497	8.983527
7.495917	590.850167	8.988544
7.075369	591.623650	8.993562
7.352177	594.657338	8.998579
7.240861	595.911905	9.003597
7.491520	585.146575	9.008615
7.417487	586.511592	9.013632
7.445208	593.964072	9.018650
7.455586	595.577001	9.023667
7.223890	598.932965	9.028685
7.150638	597.842404	9.033703
7.390024	600.659976	9.038720
6.893728	586.149901	9.043738
7.411886	589.174013	9.048755
7.304849	589.987010	9.053773
7.372427	592.377938	9.058791
7.250832	586.312435	9.063808
7.366979	599.378491	9.068826
7.260774	595.114536	9.073843
7.289569	591.400116	9.078861
7.131422	595.245602	9.083879
7.630743	584.840386	9.088896
7.060592	599.239016	9.093914
7.273452	586.918016	9.098931
7.257289	603.625148	9.103949
7.139781	588.188758	9.108967
7.143425	585.696969	9.113984
7.093406	602.188082	9.119002
7.532056	606.757238	9.124019
7.501032	618.954292	9.129037
7.747697	611.378485	9.134055
7.639392	595.669357	9.139072
7.430800	596.451506	9.144090
7.866349	589.186363	9.149107
7.398663	599.373074	9.154125
7.400827	583.225210	9.159143
7.205984	589.886374	9.164160
7.236015	593.520581	9.169178
7.735869	597.570069	9.174195
7.014184	601.811285	9.179213
7.405991	612.169693	9.184231
7.521589	620.344043	9.189248
7.618882	624.136205	9.194266
7.809660	617.929126	9.199283
7.508078	621.602492	9.204301
7.633806	622.377812	9.209319
7.516444	621.027855	9.214336
7.784081	619.833429	9.219354
7.974029	616.790472	9.224371
7.693122	592.318972	9.229389
7.675019	596.703024	9.234407
7.702315	584.766267	9.239424
7.227648	594.402262	9.244442
7.849871	576.167466	9.249459
7.352166	593.679716	9.254477
7.209876	589.716750	9.259495
7.521116	593.683254	9.264512
7.708448	621.314489	9.269530
7.737878	616.320764	9.274547
7.788811	626.760015	9.279565
7.733576	616.178063	9.284583
7.834909	599.859295	9.289600
7.589517	594.393765	9.294618
7.355221	593.421041	9.299635
7.644551	610.234065	9.304653
7.739625	620.888319	9.309671
7.813613	618.337272	9.314688
7.613834	613.397268	9.319706
7.830722	616.597035	9.324723
7.802081	616.597421	9.329741
7.363795	607.359347	9.334759
7.809683	607.004005	9.339776
7.993672	627.299859	9.344794
7.775778	618.645716	9.349811
7.597848	591.730875	9.354829
7.844995	609.182149	9.359847
7.766033	615.470795	9.364864
7.503504	614.665893	9.369882
7.589634	617.246933	9.374899
7.605357	630.478303	9.379917
7.305809	625.346751	9.384935
7.685716	628.616905	9.389952
7.446466	621.793709	9.394970
7.317308	621.781381	9.399987
7.504160	628.199204	9.405005
7.706311	633.378015	9.410023
7.745483	624.752044	9.415040
7.516053	630.079816	9.420058
7.938834	633.256288	9.425075
7.948948	650.532744	9.430093
7.726244	652.982476	9.435111
7.842409	641.855249	9.440128
8.090008	657.984895	9.445146
7.753132	651.539171	9.450163
7.713343	639.493302	9.455181
8.053306	640.326412	9.460199
8.177691	642.499928	9.465216
7.848142	640.850646	9.470234
7.606164	624.806753	9.475251
8.098635	634.957140	9.480269
7.933033	634.198806	9.485287
7.763279	627.329091	9.490304
7.984971	630.246819	9.495322
8.133258	632.455747	9.500339
7.866351	637.647714	9.505357
7.895233	633.482662	9.510375
8.208189	637.078391	9.515392
7.787153	638.586665	9.520410
7.885199	632.972652	9.525427
8.069277	629.602179	9.530445
7.941412	632.399752	9.535463
8.204150	625.910552	9.540480
7.838099	630.280767	9.545498
7.894864	633.792279	9.550515
8.236913	631.783242	9.555533
8.126250	640.314423	9.560551
8.050156	628.902204	9.565568
7.988301	651.562600	9.570586
8.075312	636.593060	9.575603
8.182436	623.901485	9.580621
7.809548	635.768896	9.585639
8.084259	636.577854	9.590656
8.162776	636.702731	9.595674
7.556689	621.919579	9.600691
8.069562	632.955504	9.605709
7.764828	647.128855	9.610727
8.013397	647.162551	9.615744
8.003626	656.728944	9.620762
8.523326	656.469751	9.625779
8.375202	645.126597	9.630797
8.027387	651.438331	9.635815
8.152433	646.568731	9.640832
8.179612	650.710023	9.645850
8.092730	647.376253	9.650867
8.190136	646.546214	9.655885
7.832715	649.923161	9.660903
8.175868	644.650755	9.665920
8.004299	647.209043	9.670938
8.168276	657.125297	9.675955
8.174027	647.625369	9.680973
7.921245	647.313647	9.685991
8.128482	652.417523	9.691008
8.261583	646.475133	9.696026
8.291994	646.352987	9.701043
8.498261	647.203860	9.706061
8.076065	649.833186	9.711079
8.061474	639.357276	9.716096
7.952668	651.752116	9.721114
7.609806	654.376402	9.726131
8.113581	650.261979	9.731149
8.032420	652.568265	9.736167
8.382319	650.747952	9.741184
8.213122	646.532083	9.746202
8.299770	645.150772	9.751219
8.258892	636.027585	9.756237
8.273748	641.350223	9.761255
8.335613	645.720581	9.766272
8.211793	645.250269	9.771290
7.952932	654.467737	9.776307
8.457239	651.456962	9.781325
8.226002	660.792091	9.786343
8.433997	662.839904	9.791360
8.235909	670.283190	9.796378
8.102833	651.085915	9.801395
8.932243	664.579826	9.806413
8.340571	674.057089	9.811431
8.668888	640.706208	9.816448
8.396465	643.761881	9.821466
8.256668	649.692649	9.826483
8.742194	640.796684	9.831501
8.247387	657.411939	9.836519
8.235354	648.465736	9.841536
7.968478	656.152919	9.846554
8.334991	670.497205	9.851571
8.918717	674.666196	9.856589
8.338919	661.065849	9.861607
8.413145	653.066139	9.866624
8.650276	641.495574	9.871642
8.656618	643.819872	9.876659
8.625948	639.579341	9.881677
8.597486	639.626540	9.886695
8.431770	639.993709	9.891712
8.708692	635.226747	9.896730
8.581714	645.901968	9.901747
8.322149	643.465475	9.906765
8.078220	651.363194	9.911783
8.390253	647.453950	9.916800
8.144540	656.463280	9.921818
8.344877	666.617778	9.926835
8.434412	666.266216	9.931853
8.475128	681.058275	9.936871
8.502937	670.570515	9.941888
8.620600	676.254159	9.946906
8.560468	689.307696	9.951923
8.809499	682.282448	9.956941
8.675884	688.704739	9.961959
8.822785	680.294258	9.966976
8.825332	665.473959	9.971994
8.513807	666.721269	9.977011
8.920921	653.256702	9.982029
8.314352	650.328832	9.987047
8.397850	645.451928	9.992064
8.479404	652.424169	9.997082
8.664921	675.493247	10.002099
9.093747	671.423187	10.007117
8.458926	651.838241	10.012135
8.503040	665.297289	10.017152
8.644896	673.434658	10.022170
8.612679	683.939844	10.027187
8.868176	674.751322	10.032205
8.765872	691.921227	10.037223
8.688148	684.886010	10.042240
8.411042	678.183887	10.047258
8.589059	680.183122	10.052275
8.701758	667.948085	10.057293
8.807150	678.866867	10.062311
8.851315	681.437926	10.067328
8.638017	677.901065	10.072346
8.748442	684.692893	10.077363
8.900684	689.813644	10.082381
8.337939	694.257220	10.087399
8.658178	682.048987	10.092416
8.834830	683.253513	10.097434
8.704681	685.377972	10.102451
8.806510	685.160278	10.107469
8.783536	684.524508	10.112487
8.819686	686.519634	10.117504
8.981993	671.620772	10.122522
8.799629	679.086164	10.127539
8.594393	677.324718	10.132557
8.486562	682.201881	10.137575
9.196118	689.051171	10.142592
8.831567	686.375177	10.147610
8.439784	696.026471	10.152627
8.845115	682.082043	10.157645
8.731111	684.864444	10.162663
8.652309	680.099077	10.167680
8.950911	691.453375	10.172698
8.730211	694.361460	10.177715
8.557706	685.936941	10.182733
8.682994	690.558595	10.187751
8.689891	708.577049	10.192768
9.134908	705.413887	10.197786
8.679011	715.539780	10.202803
9.007814	708.481065	10.207821
9.318150	716.048880	10.212839
9.010259	718.467728	10.217856
9.085396	715.765518	10.222874
8.984314	720.909641	10.227891
8.991963	723.797119	10.232909
8.624341	709.557148	10.237927
8.774218	703.952060	10.242944
9.073332	704.038811	10.247962
9.040079	713.887810	10.252979
9.238731	718.010723	10.257997
9.242819	711.983741	10.263015
9.415070	712.544919	10.268032
9.292940	714.283971	10.273050
8.942865	705.891638	10.278067
9.261919	692.935694	10.283085
8.812801	686.431352	10.288103
9.270791	697.636109	10.293120
9.454978	683.928287	10.298138
9.067755	690.483023	10.303155
9.054582	685.171276	10.308173
9.037536	685.091020	10.313191
8.741827	681.772169	10.318208
9.149225	686.320830	10.323226
8.913392	704.526117	10.328243
9.137471	696.832468	10.333261
9.223211	708.910610	10.338279
9.094002	711.517607	10.343296
9.241882	717.524068	10.348314
8.964226	707.837121	10.353331
9.366188	715.853689	10.358349
9.351396	705.999014	10.363367
9.076149	715.238908	10.368384
9.332875	710.866037	10.373402
9.455376	719.712704	10.378419
9.122261	701.520790	10.383437
9.250704	704.544378	10.388455
9.380077	711.245897	10.393472
9.159050	707.334586	10.398490
9.417289	708.937862	10.403507
9.122201	706.902139	10.408525
9.193984	714.687591	10.413543
8.969070	719.528711	10.418560
9.288195	703.287307	10.423578
9.424275	708.730264	10.428595
9.434910	703.595548	10.433613
9.393572	711.066976	10.438631
8.964083	707.890186	10.443648
9.522592	704.797918	10.448666
9.226852	712.971604	10.453683
9.423815	711.704417	10.458701
9.469659	706.326128	10.463719
9.289910	721.274814	10.468736
9.347368	712.926824	10.473754
9.139941	716.393251	10.478771
9.334772	711.360353	10.483789
9.275280	707.227304	10.488807
9.253234	708.680672	10.493824
9.592620	703.714719	10.498842
9.429491	710.335169	10.503859
9.534908	700.231246	10.508877
9.478282	706.065727	10.513895
9.393012	710.463469	10.518912
9.115937	698.941423	10.523930
9.225006	705.561862	10.528947
9.415946	716.918618	10.533965
9.459458	715.391111	10.538983
9.228080	724.937976	10.544000
9.524104	702.361456	10.549018
9.341203	706.824141	10.554035
9.223951	715.798008	10.559053
9.394360	716.288538	10.564071
9.593270	735.919884	10.569088
10.035487	738.911702	10.574106
9.919973	723.628559	10.579123
9.798283	714.206629	10.584141
9.698928	711.643667	10.589159
9.342589	703.838585	10.594176
9.490957	707.515949	10.599194
9.458408	711.528865	10.604211
9.382907	705.895777	10.609229
9.402264	704.715508	10.614247
9.457297	699.087618	10.619264
9.705793	717.360298	10.624282
9.459976	723.027956	10.629299
9.535081	736.592949	10.634317
9.934367	724.499353	10.639335
9.612045	735.425086	10.644352
9.696950	739.228378	10.649370
9.870465	745.188593	10.654387
9.298618	732.254960	10.659405
9.779198	731.812796	10.664423
10.171435	746.299529	10.669440
9.923104	723.022326	10.674458
9.722321	712.604000	10.679475
9.473909	709.484377	10.684493
9.868025	696.002240	10.689511
9.302389	707.046592	10.694528
9.946220	722.859495	10.699546
9.673630	742.381102	10.704563
9.524556	743.924154	10.709581
9.923690	733.968192	10.714599
9.442166	743.489981	10.719616
9.688544	734.128059	10.724634
9.637551	740.012204	10.729651
9.812959	746.282879	10.734669
9.869402	742.334858	10.739687
9.987050	739.773033	10.744704
10.077604	741.059989	10.749722
9.848416	744.107749	10.754739
9.940399	731.145997	10.759757
9.964640	736.240287	10.764775
9.866674	731.255965	10.769792
9.765197	736.679932	10.774810
9.840629	744.979372	10.779827
9.660421	742.499341	10.784845
9.748483	745.016609	10.789863
9.550329	750.331776	10.794880
9.572325	746.107607	10.799898
9.861045	744.773688	10.804915
9.851864	743.270434	10.809933
10.015075	737.179653	10.814951
9.831984	742.247489	10.819968
10.125143	737.368087	10.824986
10.125258	741.495179	10.830003
9.698991	749.331757	10.835021
10.037136	744.657481	10.840039
9.846085	749.383683	10.845056
9.962362	744.766047	10.850074
9.676155	734.996554	10.855091
9.774957	746.362752	10.860109
10.110790	751.551100	10.865127
9.934687	765.745520	10.870144
10.332174	761.466775	10.875162
10.486591	762.658154	10.880179
9.960937	751.595578	10.885197
10.218111	742.094785	10.890215
9.982700	745.350329	10.895232
10.132004	746.338552	10.900250
10.099435	737.661491	10.905267
9.744366	748.598353	10.910285
10.835362	752.749570	10.915303
10.323590	748.634961	10.920320
10.155388	733.367994	10.925338
10.382490	733.181656	10.930355
9.920492	736.010748	10.935373
10.077975	724.606405	10.940391
9.897103	737.759843	10.945408
10.181620	741.522177	10.950426
9.998946	735.782106	10.955443
10.024213	755.221147	10.960461
10.427215	754.352115	10.965479
10.241932	758.288529	10.970496
10.383469	758.326432	10.975514
10.148155	758.572647	10.980531
10.134288	758.763275	10.985549
10.262682	759.317826	10.990567
10.170185	773.711491	10.995584
10.514466	764.193928	11.000602
10.496019	763.374072	11.005619
10.257790	761.994184	11.010637
10.195442	753.284541	11.015655
10.559942	760.828273	11.020672
10.521055	763.951756	11.025690
10.217815	750.096609	11.030707
10.106608	752.137154	11.035725
10.501846	752.855938	11.040743
10.443217	760.770230	11.045760
10.670475	754.941743	11.050778
10.344528	743.692753	11.055795
9.934476	746.039920	11.060813
10.649812	748.912506	11.065831
10.532804	751.791363	11.070848
10.335883	748.239872	11.075866
10.692578	745.352471	11.080883
10.441378	744.228718	11.085901
10.595334	741.348349	11.090919
10.189798	743.212473	11.095936
10.417794	739.126674	11.100954
10.529315	732.812096	11.105971
10.311943	741.487225	11.110989
10.537267	753.215129	11.116007
10.584068	755.290577	11.121024
10.364805	755.063454	11.126042
10.555661	761.462072	11.131059
10.747300	763.812451	11.136077
10.509233	743.743195	11.141095
10.520114	749.365097	11.146112
10.766447	753.112094	11.151130
10.645968	738.991167	11.156147
10.298284	740.009362	11.161165
10.385220	754.090532	11.166183
10.397419	764.711247	11.171200
10.605604	777.924717	11.176218
10.651589	774.557351	11.181235
10.361517	770.960727	11.186253
10.409428	764.993892	11.191271
10.389256	764.562344	11.196288
10.001185	766.674229	11.201306
10.286186	755.394730	11.206323
9.914632	767.777679	11.211341
10.631280	774.068453	11.216359
10.790132	786.029376	11.221376
10.959033	800.571962	11.226394
11.073856	782.895394	11.231411
10.586134	776.046765	11.236429
10.575902	783.450008	11.241447
10.754159	790.176845	11.246464
10.722976	785.759814	11.251482
11.044449	776.459165	11.256499
10.720194	801.438732	11.261517
10.734059	773.603942	11.266535
10.780466	778.183648	11.271552
10.764665	790.526425	11.276570
11.044597	787.565497	11.281587
10.888016	787.760913	11.286605
11.006869	772.245423	11.291623
10.834166	764.116905	11.296640
10.777435	753.573189	11.301658
10.682642	748.549663	11.306675
11.007556	765.833173	11.311693
10.874001	777.884726	11.316711
11.158573	767.257440	11.321728
10.568203	770.616324	11.326746
11.083178	769.260660	11.331763
10.750773	775.427601	11.336781
11.004629	774.453218	11.341799
11.089422	790.194329	11.346816
10.818765	767.989755	11.351834
10.989002	770.332355	11.356851
11.137426	778.380815	11.361869
10.703073	767.301762	11.366887
11.003302	772.382439	11.371904
11.156371	789.289621	11.376922
11.171613	783.535130	11.381939
11.112888	773.469009	11.386957
10.918990	759.295345	11.391975
10.807933	759.834948	11.396992
10.771431	773.017404	11.402010
11.187521	780.621015	11.407027
11.157518	794.131196	11.412045
11.351084	797.060984	11.417063
11.277683	788.878746	11.422080
11.059356	775.468815	11.427098
10.870112	766.961599	11.432115
11.135407	776.321418	11.437133
11.153010	780.661833	11.442151
10.892965	780.219342	11.447168
10.705005	796.159541	11.452186
10.930835	791.858770	11.457203
10.832181	794.911736	11.462221
11.115057	790.034116	11.467239
11.512825	785.016961	11.472256
11.021342	785.772062	11.477274
11.306824	790.936369	11.482291
10.935753	795.588415	11.487309
10.982387	781.381772	11.492327
11.308706	787.634021	11.497344
11.088187	787.719551	11.502362
11.116966	783.077394	11.507379
11.625917	798.800972	11.512397
11.204721	791.953151	11.517415
11.599409	782.379519	11.522432
11.413799	782.995014	11.527450
11.484250	784.850748	11.532467
11.576391	785.323807	11.537485
11.535738	782.854560	11.542503
11.550953	783.817511	11.547520
11.227947	792.277684	11.552538
11.362663	788.341516	11.557555
11.769552	784.769060	11.562573
11.463440	782.257771	11.567591
11.499966	781.140789	11.572608
11.449888	786.272963	11.577626
11.365550	787.667353	11.582643
11.325084	787.458608	11.587661
11.548107	781.369932	11.592679
11.608984	785.966635	11.597696
11.390290	788.057520	11.602714
11.394208	785.150470	11.607731
11.636630	788.463651	11.612749
11.461442	780.600055	11.617767
11.582496	770.337820	11.622784
11.476668	772.493797	11.627802
11.582309	756.010499	11.632819
11.444408	761.290520	11.637837
11.533874	779.807824	11.642855
11.264514	778.215105	11.647872
11.347726	785.220099	11.652890
11.616940	787.053222	11.657907
11.670959	784.234235	11.662925
11.530525	788.900322	11.667943
12.092201	780.705840	11.672960
11.510814	783.804134	11.677978
11.774207	783.962427	11.682995
11.438538	783.306783	11.688013
11.654405	787.108126	11.693031
11.913432	781.163671	11.698048
11.824074	779.987388	11.703066
11.382340	762.600714	11.708083
11.451869	766.807959	11.713101
11.269224	780.736887	11.718119
11.794298	773.940637	11.723136
11.658496	788.124974	11.728154
11.551215	787.711658	11.733171
11.648947	794.660626	11.738189
11.271248	782.642340	11.743207
11.883203	778.080259	11.748224
11.500162	789.737692	11.753242
11.387529	787.259083	11.758259
11.289081	782.049764	11.763277
11.321904	793.220243	11.768295
11.662136	801.606050	11.773312
12.098320	818.198316	11.778330
12.062054	814.169551	11.783347
12.203064	800.062728	11.788365
11.577896	799.220811	11.793383
11.962617	782.491794	11.798400
11.968495	785.200868	11.803418
11.458512	793.315922	11.808435
11.751699	797.302094	11.813453
11.861358	797.625728	11.818471
12.092089	806.571075	11.823488
12.003280	813.784892	11.828506
12.045718	816.429967	11.833523
11.760940	805.760740	11.838541
11.987806	812.930264	11.843559
12.494690	813.347579	11.848576
11.899573	807.355909	11.853594
11.964149	792.357057	11.858611
12.028452	780.634565	11.863629
11.810413	785.864659	11.868647
11.982610	792.553332	11.873664
11.886037	801.991861	11.878682
11.975120	803.918423	11.883699
12.408211	803.576805	11.888717
12.016720	800.686677	11.893735
12.069004	794.137417	11.898752
12.219677	812.134005	11.903770
12.142076	802.366801	11.908787
12.196515	790.007558	11.913805
12.177677	781.195942	11.918823
12.181088	783.189602	11.923840
11.619218	778.021834	11.928858
12.237238	798.614826	11.933875
12.624985	798.290936	11.938893
12.459863	797.116248	11.943911
12.482657	772.604410	11.948928
12.229602	777.466928	11.953946
11.957895	779.108778	11.958963
11.996058	773.604494	11.963981
11.648136	780.065288	11.968999
12.475652	789.461910	11.974016
12.394705	804.478292	11.979034
12.249096	791.227757	11.984051
12.420541	795.241034	11.989069
12.385585	793.360013	11.994087
12.138078	781.867659	11.999104
11.828966	787.717325	12.004122
12.004108	796.303117	12.009139
12.402683	808.509039	12.014157
12.358515	814.543929	12.019175
12.344704	809.562995	12.024192
12.219077	808.646892	12.029210
12.235616	810.465876	12.034227
12.087147	795.506557	12.039245
11.929823	806.683866	12.044263
11.826957	797.675237	12.049280
12.149391	802.820451	12.054298
12.586006	821.623490	12.059315
12.800241	819.949178	12.064333
12.241267	805.620778	12.069351
12.195508	808.025156	12.074368
12.423845	818.690492	12.079386
12.524167	841.747131	12.084403
12.548645	833.128392	12.089421
12.598478	833.789318	12.094439
13.100232	830.535666	12.099456
12.376822	820.817700	12.104474
12.424884	807.309201	12.109491
12.481373	797.569537	12.114509
12.531311	801.887590	12.119527
12.649790	794.254249	12.124544
12.746320	798.890529	12.129562
12.490025	798.167545	12.134579
12.477042	795.747060	12.139597
12.240592	810.745944	12.144615
12.628158	823.733781	12.149632
13.018025	831.964183	12.154650
12.633715	836.636733	12.159667
12.664939	822.884293	12.164685
12.722526	825.788633	12.169703
12.756841	820.389576	12.174720
13.182664	804.987668	12.179738
12.808361	802.763580	12.184755
12.752338	804.503233	12.189773
12.709162	803.628712	12.194791
12.458702	801.378550	12.199808
12.624496	801.235112	12.204826
12.403542	811.516894	12.209843
12.379841	817.703790	12.214861
12.632939	831.237386	12.219879
12.633387	818.006878	12.224896
13.196122	819.342955	12.229914
12.766219	828.860989	12.234931
12.970077	828.282496	12.239949
12.975683	826.633803	12.244967
12.682090	839.811761	12.249984
12.904562	833.608313	12.255002
12.643002	838.636499	12.260019
13.342066	828.022944	12.265037
13.065604	830.825034	12.270055
13.093873	822.821907	12.275072
12.988864	829.459767	12.280090
12.939549	832.799616	12.285107
13.386336	826.971236	12.290125
12.884483	813.857984	12.295143
12.871944	818.714523	12.300160
13.366387	816.679590	12.305178
12.902699	816.969351	12.310195
13.032787	805.420387	12.315213
13.236716	804.099589	12.320231
12.734500	803.937725	12.325248
12.555276	806.003393	12.330266
12.843706	827.692738	12.335283
12.999913	824.586332	12.340301
12.894045	829.028843	12.345319
12.913632	817.644463	12.350336
13.022875	823.050663	12.355354
13.068588	809.286197	12.360371
13.219854	814.302248	12.365389
13.426569	821.797885	12.370407
13.163248	816.772958	12.375424
13.117369	826.991180	12.380442
12.861070	825.319046	12.385459
13.455384	818.239925	12.390477
13.094252	831.038159	12.395495
13.570065	819.073748	12.400512
13.273129	832.228241	12.405530
13.022098	827.661044	12.410547
13.289111	817.887267	12.415565
13.446842	830.280127	12.420583
13.139226	822.092587	12.425600
13.084473	812.048812	12.430618
13.145885	821.242189	12.435635
13.398186	810.546104	12.440653
12.972120	827.605420	12.445671
13.257964	835.089365	12.450688
13.378657	824.103162	12.455706
13.308367	832.194289	12.460723
13.304775	816.499318	12.465741
13.383680	819.221621	12.470759
13.731656	823.830430	12.475776
13.474636	825.157706	12.480794
13.301010	820.965646	12.485811
13.433852	810.333291	12.490829
13.515383	833.561104	12.495847
13.380552	833.233428	12.500864
13.495446	826.263642	12.505882
13.254486	827.424710	12.510899
13.518073	817.754040	12.515917
12.952219	827.519698	12.520935
12.967670	844.024164	12.525952
13.603002	834.898052	12.530970
13.644189	850.886155	12.535987
13.935707	843.733655	12.541005
13.870278	851.137098	12.546023
13.913871	841.856054	12.551040
13.895957	829.100341	12.556058
13.704253	824.632968	12.561075
13.676813	816.453059	12.566093
13.567964	826.365008	12.571111
13.801555	816.988223	12.576128
13.741421	816.369708	12.581146
13.720381	817.251955	12.586163
13.655889	809.244778	12.591181
13.286743	817.967762	12.596199
13.311089	813.681976	12.601216
13.729974	815.790318	12.606234
13.837026	833.739622	12.611251
14.017895	835.241936	12.616269
14.046281	838.190270	12.621287
13.666151	837.797440	12.626304
13.907946	826.486157	12.631322
13.547199	812.942767	12.636339
13.748833	828.454606	12.641357
13.815190	834.608323	12.646375
14.040906	841.298997	12.651392
13.862233	845.706505	12.656410
13.915543	840.465495	12.661427
13.773846	835.277181	12.666445
13.732371	844.863692	12.671463
13.840800	845.145313	12.676480
13.658989	847.630437	12.681498
13.552772	850.374480	12.686515
13.730981	841.914946	12.691533
13.672119	846.047187	12.696551
13.534878	853.503435	12.701568
13.952025	833.760063	12.706586
13.536836	849.282138	12.711603
13.617575	846.364941	12.716621
13.953852	859.796643	12.721639
14.153824	872.421099	12.726656
14.550478	871.010682	12.731674
13.858733	868.001092	12.736691
13.760635	865.438980	12.741709
13.905649	878.657070	12.746727
13.868618	874.195614	12.751744
14.405491	870.840103	12.756762
14.508889	871.749617	12.761779
14.637326	865.247968	12.766797
14.694691	841.779244	12.771815
14.594020	833.893663	12.776832
14.734361	824.936741	12.781850
14.409895	829.875534	12.786867
14.359004	830.515513	12.791885
14.463332	826.836085	12.796903
14.488432	824.905281	12.801920
14.750858	821.131236	12.806938
14.528119	815.351110	12.811955
14.488350	799.775107	12.816973
14.173920	803.499745	12.821991
14.094762	813.579289	12.827008
14.241885	791.484843	12.832026
13.941883	799.743123	12.837043
14.138907	804.751511	12.842061
14.532896	796.884778	12.847079
14.261830	806.772841	12.852096
14.230982	791.353908	12.857114
14.158873	807.288260	12.862131
14.374036	812.796322	12.867149
14.403346	819.115970	12.872167
14.147911	823.446014	12.877184
14.391271	828.206144	12.882202
14.380387	828.966458	12.887219
14.341435	822.327359	12.892237
14.364745	822.474056	12.897255
14.567727	818.774391	12.902272
14.378943	822.283717	12.907290
14.701812	829.639514	12.912307
14.703696	816.141690	12.917325
14.843450	822.066970	12.922343
14.386329	823.846533	12.927360
14.581227	835.575691	12.932378
14.608292	831.941505	12.937395
14.681763	827.315173	12.942413
14.769625	830.777210	12.947431
14.661763	831.561029	12.952448
14.546606	836.083804	12.957466
14.613035	837.039772	12.962483
14.296407	827.240409	12.967501
14.760422	831.249829	12.972519
14.441550	831.527861	12.977536
14.557610	819.295003	12.982554
14.556679	833.592898	12.987571
14.357637	829.431212	12.992589
14.905014	815.887331	12.997607
14.586929	824.512034	13.002624
14.552595	823.279124	13.007642
14.600991	827.390879	13.012659
14.576286	837.324357	13.017677
14.904226	843.040625	13.022695
14.701267	855.624781	13.027712
14.983416	855.675367	13.032730
14.973611	856.389646	13.037747
15.026100	861.613342	13.042765
14.821191	845.990382	13.047783
14.717769	844.179616	13.052800
14.767199	865.168084	13.057818
14.735719	852.933600	13.062835
14.965277	862.708168	13.067853
14.903083	869.025243	13.072871
14.639318	871.347369	13.077888
14.870851	857.141592	13.082906
14.956622	862.182062	13.087923
14.917994	865.546919	13.092941
14.780864	859.160997	13.097959
14.819834	870.876979	13.102976
15.542161	860.644927	13.107994
14.805904	861.154308	13.113011
14.995245	858.408302	13.118029
15.187980	864.511427	13.123047
14.830039	861.340002	13.128064
14.795874	864.937940	13.133082
14.932770	866.926381	13.138099
15.012211	871.063131	13.143117
15.166315	869.238344	13.148135
15.180894	876.571697	13.153152
15.419275	881.247641	13.158170
15.056394	862.028147	13.163187
14.775736	861.961930	13.168205
15.412765	865.856168	13.173223
15.424862	882.673973	13.178240
15.143202	883.171213	13.183258
15.256734	882.399805	13.188275
15.173039	885.362340	13.193293
15.432711	877.176285	13.198311
15.423346	887.399140	13.203328
15.592097	876.419917	13.208346
15.186775	870.626249	13.213363
14.990006	876.693958	13.218381
15.547171	881.392800	13.223399
15.666758	899.431630	13.228416
15.271949	885.977254	13.233434
15.461362	885.348005	13.238451
15.471664	890.894181	13.243469
15.717514	880.120485	13.248487
15.822250	870.417775	13.253504
15.513425	857.059630	13.258522
15.542629	848.275956	13.263539
15.218620	846.159771	13.268557
15.569807	848.454078	13.273575
14.977177	852.669015	13.278592
15.316626	863.207772	13.283610
15.954019	871.958222	13.288627
15.616066	890.014785	13.293645
15.753536	875.234280	13.298663
15.563708	876.190478	13.303680
15.694475	874.427017	13.308698
15.754219	871.840395	13.313715
15.208138	873.575619	13.318733
15.879333	873.721927	13.323751
15.865614	888.316031	13.328768
15.800210	872.785325	13.333786
15.847486	866.510831	13.338803
15.701315	868.416150	13.343821
15.643161	861.298792	13.348839
15.571662	862.315934	13.353856
15.824469	870.574321	13.358874
15.796541	871.081788	13.363891
16.151703	875.941351	13.368909
16.054496	858.352088	13.373927
15.684348	859.682119	13.378944
15.775216	855.410324	13.383962
15.792025	848.871430	13.388979
15.620586	848.039653	13.393997
16.273089	862.519506	13.399015
16.071582	854.775753	13.404032
15.783794	864.238637	13.409050
15.722767	850.661035	13.414067
15.737045	866.083225	13.419085
15.737427	868.851972	13.424103
15.994959	868.361442	13.429120
16.018641	879.710138	13.434138
16.275574	878.855987	13.439155
15.932500	881.774981	13.444173
15.951370	881.970239	13.449191
16.039394	879.781433	13.454208
15.982877	879.722460	13.459226
15.973836	872.601902	13.464243
15.874773	881.992868	13.469261
15.850010	874.207499	13.474279
16.149060	879.179665	13.479296
15.795333	882.975864	13.484314
16.084003	878.872326	13.489331
15.921074	886.134246	13.494349
16.136201	871.668612	13.499367
15.995033	872.987966	13.504384
16.007312	880.309105	13.509402
15.990849	884.432971	13.514419
15.907308	888.750767	13.519437
16.101248	902.888001	13.524455
16.594351	905.442874	13.529472
16.648618	890.802656	13.534490
16.863780	873.104089	13.539507
16.543890	872.692643	13.544525
16.431249	881.032485	13.549543
16.552944	869.485746	13.554560
16.330561	872.066737	13.559578
16.792123	870.259831	13.564595
16.356393	877.781162	13.569613
16.826723	869.686263	13.574631
16.665454	863.938275	13.579648
16.294618	863.764343	13.584666
16.350703	863.541119	13.589683
16.429971	872.075190	13.594701
16.488656	862.824902	13.599719
16.773567	862.511116	13.604736
16.644954	868.656914	13.609754
16.843286	855.153162	13.614771
16.434294	870.814959	13.619789
16.015894	864.482403	13.624807
16.135811	856.899670	13.629824
16.407263	861.394582	13.634842
16.893533	860.312016	13.639859
16.537262	873.685370	13.644877
16.513120	870.999439	13.649895
16.892084	870.324893	13.654912
16.729859	865.071272	13.659930
16.588112	861.225842	13.664947
16.661895	865.669380	13.669965
16.922698	856.728157	13.674983
16.866476	859.082705	13.680000
16.411079	857.607024	13.685018
16.524249	862.155647	13.690035
16.660436	865.220599	13.695053
16.480100	857.834505	13.700071
16.592987	868.218218	13.705088
16.421308	872.519477	13.710106
16.713828	868.943760	13.715123
16.768513	890.876315	13.720141
16.993842	897.842033	13.725159
16.851344	900.857588	13.730176
16.794280	888.271851	13.735194
16.943063	886.242857	13.740211
16.786075	897.222276	13.745229
16.601219	896.366537	13.750247
16.775407	893.369331	13.755264
16.895124	893.405822	13.760282
16.812474	892.874475	13.765299
16.999341	901.192980	13.770317
17.175828	901.390730	13.775335
16.959799	899.750115	13.780352
17.004849	897.167098	13.785370
16.754731	898.840229	13.790387
16.946131	900.610253	13.795405
16.887378	894.080874	13.800423
17.333364	897.750434	13.805440
17.176639	897.519076	13.810458
17.447405	897.969312	13.815475
17.252072	898.041331	13.820493
17.008452	909.584590	13.825511
17.476511	893.485078	13.830528
16.705241	900.922325	13.835546
16.904826	898.876078	13.840563
17.031419	901.531077	13.845581
17.038288	906.555077	13.850599
17.402068	916.486013	13.855616
17.647673	924.531679	13.860634
17.811288	914.976665	13.865651
17.424684	898.940442	13.870669
17.139342	902.466529	13.875687
17.375309	879.641547	13.880704
17.141496	896.040828	13.885722
17.285149	890.655366	13.890739
17.442980	900.358164	13.895757
17.479479	913.275766	13.900775
17.471122	900.666224	13.905792
17.303246	914.148811	13.910810
17.528428	901.304645	13.915827
17.495154	917.225017	13.920845
17.509442	909.101342	13.925863
17.690096	911.570863	13.930880
17.673845	917.917958	13.935898
17.513801	904.907368	13.940915
17.449484	899.811149	13.945933
17.621685	916.044358	13.950951
17.920945	915.296382	13.955968
17.343894	912.749246	13.960986
17.639474	907.401654	13.966003
17.667109	921.028878	13.971021
17.564553	920.765934	13.976039
17.890609	917.896751	13.981056
17.778853	917.899064	13.986074
17.728994	920.153767	13.991091
17.637262	923.205418	13.996109
17.554715	917.429641	14.001127
18.077839	916.480328	14.006144
17.705494	925.266194	14.011162
17.809795	912.090872	14.016179
18.082711	913.417183	14.021197
17.730800	930.355813	14.026215
17.730370	904.463872	14.031232
17.956559	925.391131	14.036250
17.985492	916.382303	14.041267
18.027787	915.748432	14.046285
18.098814	917.691081	14.051303
18.085189	906.384552	14.056320
17.678177	892.329925	14.061338
17.584432	892.708135	14.066355
17.856505	917.572422	14.071373
17.783739	917.964485	14.076391
17.870744	906.191008	14.081408
17.802135	914.912506	14.086426
18.038006	926.894369	14.091443
17.811791	921.922518	14.096461
18.154090	916.386720	14.101479
18.081443	922.321750	14.106496
17.944918	922.010884	14.111514
18.061937	922.956136	14.116531
17.914506	917.226705	14.121549
17.949322	916.794037	14.126567
18.112286	911.407147	14.131584
18.399477	940.397229	14.136602
18.507062	932.740132	14.141619
18.596468	925.597966	14.146637
18.288045	919.572159	14.151655
18.710786	908.860732	14.156672
18.508132	909.211081	14.161690
18.464612	908.538448	14.166707
18.243220	915.337286	14.171725
18.325351	908.724393	14.176743
18.703407	914.836671	14.181760
18.435574	904.870166	14.186778
18.282940	917.200034	14.191795
18.409364	905.803248	14.196813
18.212460	908.571735	14.201831
18.602142	902.157783	14.206848
18.324408	909.099766	14.211866
18.258191	915.468107	14.216883
18.743690	900.298427	14.221901
18.350981	909.726520	14.226919
18.838851	891.281998	14.231936
18.854930	911.288804	14.236954
18.655219	891.916344	14.241971
18.768748	902.919360	14.246989
18.530884	910.190132	14.252007
18.634020	907.684310	14.257024
18.902575	907.989463	14.262042
18.816894	903.144764	14.267059
18.683113	905.353501	14.272077
18.711542	908.556720	14.277095
18.502090	912.210994	14.282112
18.473513	900.345419	14.287130
18.464258	899.589774	14.292147
18.601880	897.302628	14.297165
18.571632	904.822900	14.302183
18.230005	897.591175	14.307200
18.732200	912.456288	14.312218
18.598765	915.412483	14.317235
18.834164	925.885814	14.322253
18.861230	935.606307	14.327271
19.131910	933.009616	14.332288
18.952207	932.610625	14.337306
18.672679	933.684586	14.342323
19.001454	926.064156	14.347341
19.117818	934.998168	14.352359
19.037770	929.249724	14.357376
19.136560	932.376766	14.362394
18.857361	938.038701	14.367411
18.962119	929.578463	14.372429
18.918513	930.625443	14.377447
18.936573	935.229365	14.382464
19.247793	935.127141	14.387482
19.053085	932.340863	14.392499
19.076582	927.752479	14.397517
19.154540	933.822048	14.402535
18.925987	935.570347	14.407552
18.927519	945.501331	14.412570
19.009000	943.052420	14.417587
19.280834	932.347413	14.422605
18.976200	940.614308	14.427623
19.412817	925.735509	14.432640
19.337898	921.438148	14.437658
19.155794	935.489154	14.442675
19.362392	930.771118	14.447693
18.952057	938.601026	14.452711
19.240170	928.035435	14.457728
18.996815	925.180832	14.462746
19.081336	942.294361	14.467763
19.569336	950.367493	14.472781
19.340439	955.816825	14.477799
19.588582	957.476117	14.482816
19.719400	961.048389	14.487834
19.478695	948.452405	14.492851
19.280655	944.037020	14.497869
19.081971	958.404318	14.502887
19.842268	968.581917	14.507904
19.853035	957.522854	14.512922
19.662998	959.424018	14.517939
20.027704	932.981808	14.522957
19.702398	930.591067	14.527975
19.611530	922.156666	14.532992
19.498032	930.839338	14.538010
19.377645	939.465091	14.543027
19.881655	937.911161	14.548045
19.518979	933.947522	14.553063
19.443172	928.452667	14.558080
19.817350	938.537189	14.563098
19.582684	951.771637	14.568115
19.848884	942.609429	14.573133
19.764640	955.302178	14.578151
20.080386	951.843451	14.583168
20.112250	935.215287	14.588186
19.939877	932.929370	14.593203
20.099065	912.915191	14.598221
19.684694	924.312297	14.603239
20.023835	920.067949	14.608256
19.863528	920.808676	14.613274
20.130020	934.417304	14.618291
20.198195	929.234230	14.623309
19.892819	932.262930	14.628327
20.027436	921.809308	14.633344
20.061183	918.864435	14.638362
19.823282	917.284707	14.643379
20.070866	919.791586	14.648397
19.676461	924.789202	14.653415
19.906210	925.698899	14.658432
20.129256	932.630960	14.663450
19.925909	949.292543	14.668467
20.370815	949.207393	14.673485
20.382976	962.430781	14.678503
20.173880	946.780855	14.683520
20.085019	934.350900	14.688538
19.872361	933.955388	14.693555
20.228516	953.224469	14.698573
20.119256	963.433376	14.703591
20.153701	956.567952	14.708608
20.311196	952.474656	14.713626
20.350157	957.528207	14.718643
20.353470	942.500755	14.723661
19.967491	947.131494	14.728679
19.858863	947.480281	14.733696
20.246236	950.929656	14.738714
20.154070	949.867486	14.743731
20.189270	945.675129	14.748749
19.908120	953.336870	14.753767
20.179632	970.789155	14.758784
20.765037	978.202609	14.763802
20.458465	978.270967	14.768819
20.941174	982.920542	14.773837
20.923845	981.359467	14.778855
20.433338	956.742719	14.783872
20.605487	939.986661	14.788890
20.570430	957.971404	14.793907
20.494474	969.237238	14.798925
20.445430	971.210364	14.803943
20.984222	978.335702	14.808960
21.038743	971.580320	14.813978
20.680283	972.354976	14.818995
21.071375	945.051043	14.824013
20.936971	934.526336	14.829031
20.692332	946.334118	14.834048
20.956515	945.637008	14.839066
20.954293	952.986361	14.844083
20.983667	942.992958	14.849101
20.838571	949.940988	14.854119
20.677597	946.601979	14.859136
20.985706	943.903840	14.864154
20.547251	941.227514	14.869171
20.595078	939.844622	14.874189
20.759683	946.920381	14.879207
20.645196	948.514027	14.884224
21.043579	962.950944	14.889242
20.701416	977.830080	14.894259
20.966103	982.728640	14.899277
21.172733	982.100479	14.904295
21.235721	985.730809	14.909312
21.201441	964.378280	14.914330
20.962265	978.720601	14.919347
20.953366	979.969492	14.924365
20.831523	983.802384	14.929383
20.630560	984.449849	14.934400
21.002842	987.552766	14.939418
21.005270	980.861886	14.944435
21.073348	975.508171	14.949453
21.130641	979.817481	14.954471
21.111681	977.546947	14.959488
21.199703	981.407353	14.964506
20.658827	988.267876	14.969523
20.958065	993.286694	14.974541
21.129528	996.968775	14.979559
21.258681	1010.060684	14.984576
21.626433	1002.540255	14.989594
21.378407	1003.259660	14.994611
21.327733	986.393940	14.999629
21.325301	995.335612	15.004647
21.425659	1004.990502	15.009664
21.535890	995.236813	15.014682
21.289516	994.724646	15.019699
21.677483	990.283855	15.024717
21.878924	986.706039	15.029735
21.630335	997.181655	15.034752
22.009345	984.053183	15.039770
21.762825	991.711976	15.044787
21.825320	988.457466	15.049805
22.082666	988.263963	15.054823
21.649437	992.292582	15.059840
21.811603	977.625397	15.064858
21.567688	978.792869	15.069875
21.545580	978.430620	15.074893
21.838082	983.483417	15.079911
22.034121	991.906148	15.084928
22.212805	979.242998	15.089946
21.825836	976.145626	15.094963
21.752544	977.014866	15.099981
21.377481	975.595375	15.104999
21.894767	983.190926	15.110016
21.709757	995.598242	15.115034
21.676601	999.256075	15.120051
21.557373	985.771817	15.125069
21.899192	983.516848	15.130087
21.462055	987.744112	15.135104
21.868133	983.846699	15.140122
21.715815	991.242327	15.145139
21.576890	994.880635	15.150157
21.674354	999.699371	15.155175
21.679083	1009.238395	15.160192
22.122744	1018.359276	15.165210
22.117001	1021.505382	15.170227
22.153325	1024.512863	15.175245
22.264201	1010.282993	15.180263
22.274237	1024.501707	15.185280
22.599753	1007.200432	15.190298
22.464888	1005.641457	15.195315
22.434447	1014.088635	15.200333
22.938781	1003.470926	15.205351
22.241316	999.852115	15.210368
22.332089	987.779969	15.215386
22.121066	989.354538	15.220403
22.110686	987.441779	15.225421
22.469438	973.525255	15.230439
22.030039	980.222769	15.235456
22.283352	992.500572	15.240474
22.057243	1006.120205	15.245491
22.457928	1012.941071	15.250509
22.801856	1011.629105	15.255527
22.351782	1013.193385	15.260544
22.498408	1000.448128	15.265562
22.240214	1008.939631	15.270579
22.277794	1014.496893	15.275597
22.634895	1018.028833	15.280615
22.246698	1011.383005	15.285632
22.613661	1019.371270	15.290650
22.694884	1014.136217	15.295667
22.215298	1014.623262	15.300685
22.350236	1002.733539	15.305703
22.055674	1018.944596	15.310720
22.542015	1026.365587	15.315738
22.751174	1037.491654	15.320755
22.575247	1040.587552	15.325773
22.968287	1028.782500	15.330791
23.033437	1035.179765	15.335808
23.158167	1022.221213	15.340826
23.136825	1034.372417	15.345843
23.064340	1022.887961	15.350861
22.931135	1023.899761	15.355879
23.023556	1041.767882	15.360896
23.422435	1027.794882	15.365914
23.146396	1024.207786	15.370931
22.983033	1006.040205	15.375949
22.740395	1001.773489	15.380967
22.931384	1004.493246	15.385984
22.719814	1010.395370	15.391002
22.981348	1016.895587	15.396019
22.977695	1039.135388	15.401037
23.156203	1029.284385	15.406055
23.432990	1040.978715	15.411072
23.306053	1039.171221	15.416090
23.017291	1035.462228	15.421107
23.133154	1040.390518	15.426125
23.049451	1034.771359	15.431143
23.036206	1043.558965	15.436160
23.009996	1039.554065	15.441178
23.270776	1042.428215	15.446195
23.358274	1039.770452	15.451213
23.262049	1047.398925	15.456231
23.162626	1042.066175	15.461248
23.298215	1043.500021	15.466266
23.129784	1039.371599	15.471283
23.022549	1048.419189	15.476301
23.076503	1053.336457	15.481319
23.262277	1057.599758	15.486336
23.449563	1068.793232	15.491354
23.585484	1059.868198	15.496371
23.543387	1070.075525	15.501389
23.821240	1065.208884	15.506407
23.538747	1065.038850	15.511424
23.632046	1049.775592	15.516442
23.889680	1051.057401	15.521459
23.700080	1063.419671	15.526477
23.692249	1054.463680	15.531495
23.780802	1054.978869	15.536512
23.696784	1054.288910	15.541530
24.052829	1054.654990	15.546547
23.946325	1062.911450	15.551565
23.679006	1059.784054	15.556583
23.638338	1053.516537	15.561600
23.803560	1063.160548	15.566618
23.915691	1057.843219	15.571635
23.755919	1057.131138	15.576653
24.351789	1050.616331	15.581671
23.908523	1056.168631	15.586688
23.747207	1052.389960	15.591706
23.883007	1045.554983	15.596723
23.502579	1058.298729	15.601741
23.507897	1065.674248	15.606759
23.682539	1061.044708	15.611776
23.849379	1052.973491	15.616794
23.945171	1050.788298	15.621811
23.867865	1059.962228	15.626829
24.169349	1069.220200	15.631847
24.219035	1080.286050	15.636864
24.454486	1082.744379	15.641882
24.322689	1073.035556	15.646899
24.120039	1074.003922	15.651917
24.405542	1063.908479	15.656935
24.010123	1062.157946	15.661952
24.074688	1078.346525	15.666970
24.679591	1072.458269	15.671987
24.562379	1083.900073	15.677005
24.708856	1058.662624	15.682023
24.017655	1057.943888	15.687040
24.322265	1064.373827	15.692058
24.543292	1076.918214	15.697075
24.395375	1084.955776	15.702093
25.027388	1079.334453	15.707111
24.472632	1068.089672	15.712128
24.411019	1046.172737	15.717146
24.648839	1047.584966	15.722163
24.289539	1055.027227	15.727181
24.547802	1064.898150	15.732199
24.909409	1071.150786	15.737216
24.678383	1069.956263	15.742234
24.737028	1073.809148	15.747251
24.735380	1086.331096	15.752269
24.949410	1078.949992	15.757287
24.745443	1064.741395	15.762304
24.702445	1063.276074	15.767322
24.921566	1061.854237	15.772339
24.759269	1064.012795	15.777357
25.069435	1061.707543	15.782375
24.981315	1060.553963	15.787392
24.647165	1053.739564	15.792410
24.675046	1058.092530	15.797427
24.829928	1068.778053	15.802445
25.185334	1071.388774	15.807463
24.963588	1072.032985	15.812480
24.841757	1074.253548	15.817498
24.943603	1080.387721	15.822515
24.956700	1083.290408	15.827533
25.004331	1083.795237	15.832551
24.891269	1080.362861	15.837568
25.045278	1079.332038	15.842586
25.147270	1074.431865	15.847603
24.924714	1083.935080	15.852621
24.726170	1069.778134	15.857639
24.884192	1076.340750	15.862656
24.620924	1085.837113	15.867674
25.117565	1095.154372	15.872691
25.099514	1100.411259	15.877709
25.314931	1097.289306	15.882727
25.501920	1093.673112	15.887744
25.708852	1082.418970	15.892762
26.228027	1085.902296	15.897779
26.152043	1070.812047	15.902797
25.837013	1060.146852	15.907815
25.902344	1053.233571	15.912832
25.934088	1063.182666	15.917850
26.019645	1045.340973	15.922867
25.660052	1037.322511	15.927885
25.177106	1027.304675	15.932903
25.785152	1036.693633	15.937920
25.667369	1051.544225	15.942938
25.940164	1050.213109	15.947955
25.384910	1041.308223	15.952973
25.584864	1042.534810	15.957991
25.568888	1052.598263	15.963008
25.574502	1059.842255	15.968026
25.524456	1056.016065	15.973043
25.335362	1054.252497	15.978061
25.811528	1051.663950	15.983079
25.928472	1065.770168	15.988096
25.703391	1059.382163	15.993114
25.903173	1047.512591	15.998131
25.744627	1054.797484	16.003149
25.774107	1036.058124	16.008167
25.792463	1051.027338	16.013184
25.638239	1057.170751	16.018202
25.870696	1050.174744	16.023219
25.745910	1064.822207	16.028237
25.972655	1069.661722	16.033255
26.355063	1086.061525	16.038272
26.296824	1092.423307	16.043290
26.156967	1085.066039	16.048307
26.024384	1083.860168	16.053325
26.217731	1089.374986	16.058343
26.171151	1077.752567	16.063360
26.119824	1091.766752	16.068378
26.275275	1086.644586	16.073395
26.481368	1080.798218	16.078413
26.098807	1076.094045	16.083431
26.333118	1071.696533	16.088448
25.914219	1091.838239	16.093466
26.454753	1087.129924	16.098483
26.639905	1080.575512	16.103501
26.273425	1089.985209	16.108519
26.463604	1090.123818	16.113536
26.023020	1099.553246	16.118554
26.325334	1091.341136	16.123571
26.083941	1084.861539	16.128589
26.182320	1085.755361	16.133607
26.460144	1089.207323	16.138624
26.441467	1102.090901	16.143642
26.814403	1113.764282	16.148659
26.878780	1114.021893	16.153677
26.699186	1111.535795	16.158695
26.632729	1112.221855	16.163712
26.569332	1119.401699	16.168730
26.569866	1122.258249	16.173747
27.057722	1116.909908	16.178765
26.672042	1111.205801	16.183783
27.104479	1099.509718	16.188800
26.895843	1110.498611	16.193818
27.051602	1113.496018	16.198835
27.181407	1112.568784	16.203853
27.162847	1122.731908	16.208871
27.122714	1105.156548	16.213888
26.691120	1096.828938	16.218906
26.701797	1105.306571	16.223923
27.052019	1109.735596	16.228941
27.039314	1098.624807	16.233959
27.234652	1100.169435	16.238976
27.041300	1099.129683	16.243994
27.495704	1092.314861	16.249011
27.168645	1093.829100	16.254029
27.031532	1098.214459	16.259047
27.221296	1098.028778	16.264064
27.383275	1109.094790	16.269082
27.379081	1107.030624	16.274099
27.428686	1099.775878	16.279117
27.077390	1096.035478	16.284135
27.144248	1098.895037	16.289152
27.158533	1102.223451	16.294170
27.497330	1101.067616	16.299187
27.925224	1095.940774	16.304205
27.345362	1105.865590	16.309223
27.406125	1096.652213	16.314240
27.239917	1102.505938	16.319258
27.489199	1103.412615	16.324275
27.131615	1102.521440	16.329293
27.397318	1122.115674	16.334311
27.458892	1101.814275	16.339328
27.470115	1098.970122	16.344346
27.546303	1102.958085	16.349363
27.932576	1109.691627	16.354381
27.389020	1118.034707	16.359399
27.658472	1116.366788	16.364416
27.563372	1128.966606	16.369434
27.792508	1133.367230	16.374451
28.337077	1131.139553	16.379469
28.128661	1134.478598	16.384487
28.170179	1129.937562	16.389504
27.531109	1106.816750	16.394522
28.051598	1121.991792	16.399539
27.755442	1116.116810	16.404557
27.627386	1129.675080	16.409575
28.174887	1126.503165	16.414592
27.743490	1132.502873	16.419610
27.749651	1133.194450	16.424627
27.830972	1134.492019	16.429645
28.178907	1137.620247	16.434663
27.785979	1131.763416	16.439680
27.900146	1137.675333	16.444698
27.828546	1128.661540	16.449715
28.223602	1141.170136	16.454733
28.298295	1158.554781	16.459751
28.685315	1153.029223	16.464768
28.665112	1146.281980	16.469786
28.369838	1136.523961	16.474803
28.472108	1121.664599	16.479821
28.309981	1119.424788	16.484839
28.601250	1115.233371	16.489856
28.381451	1122.142256	16.494874
28.536196	1120.318909	16.499891
28.396858	1117.578951	16.504909
28.693541	1135.713579	16.509927
28.656203	1134.575220	16.514944
28.589351	1133.948551	16.519962
28.838405	1128.208238	16.524979
28.609690	1123.820110	16.529997
28.411411	1130.879948	16.535015
28.666590	1135.575042	16.540032
28.822368	1150.632061	16.545050
28.891317	1152.231434	16.550067
29.262953	1137.897537	16.555085
28.960466	1133.024625	16.560103
29.014546	1125.034002	16.565120
28.723210	1135.068812	16.570138
28.568193	1119.829197	16.575155
29.005545	1106.736249	16.580173
28.702602	1114.003306	16.585191
28.964867	1129.270822	16.590208
29.052301	1142.933040	16.595226
29.217810	1156.285759	16.600243
29.336794	1145.360624	16.605261
29.159076	1140.983746	16.610279
28.934223	1130.108158	16.615296
29.266472	1121.388603	16.620314
28.944522	1133.919629	16.625331
28.978719	1121.708127	16.630349
29.288553	1149.494454	16.635367
29.135587	1141.959824	16.640384
29.332507	1151.925770	16.645402
29.285512	1153.969239	16.650419
29.419693	1152.773996	16.655437
29.365678	1159.730492	16.660455
29.384279	1148.570209	16.665472
29.399395	1150.957888	16.670490
29.391640	1145.702853	16.675507
29.761015	1151.332482	16.680525
29.096948	1153.673365	16.685543
29.385257	1143.791744	16.690560
29.338496	1142.617939	16.695578
29.399808	1142.115739	16.700595
29.419464	1144.303090	16.705613
29.127053	1148.649767	16.710631
29.319036	1155.282384	16.715648
29.703042	1170.865404	16.720666
29.755085	1172.319956	16.725683
29.879210	1168.553920	16.730701
29.487386	1175.329076	16.735719
29.709509	1170.323601	16.740736
29.755517	1172.972282	16.745754
29.669239	1180.153770	16.750771
30.040953	1181.923358	16.755789
29.759989	1170.515952	16.760807
29.933427	1170.264867	16.765824
29.791267	1176.886972	16.770842
29.615230	1177.594488	16.775859
30.035365	1170.875635	16.780877
29.963983	1187.607584	16.785895
29.835633	1179.665384	16.790912
30.468123	1184.801415	16.795930
30.465132	1194.271171	16.800947
30.798026	1173.447550	16.805965
30.613935	1162.504582	16.810983
30.934512	1159.070795	16.816000
30.883135	1157.577327	16.821018
30.821622	1149.497344	16.826035
30.615040	1152.278693	16.831053
30.758586	1146.118472	16.836071
30.556727	1128.068114	16.841088
30.333628	1116.758846	16.846106
30.392800	1128.402210	16.851123
30.337241	1117.343560	16.856141
30.608075	1128.853931	16.861159
30.880061	1126.216054	16.866176
30.954883	1121.463642	16.871194
30.207742	1122.457627	16.876211
30.711979	1120.929032	16.881229
30.647293	1135.782741	16.886247
30.621247	1137.888484	16.891264
30.759797	1131.029594	16.896282
30.465776	1142.583717	16.901299
30.852731	1136.846003	16.906317
30.848163	1140.119281	16.911335
30.477416	1152.163381	16.916352
30.920197	1146.753986	16.921370
30.704719	1156.334608	16.926387
30.975628	1151.512387	16.931405
31.131888	1154.394973	16.936423
30.968141	1159.056955	16.941440
30.788212	1146.578500	16.946458
30.697759	1148.637416	16.951475
31.044153	1148.384518	16.956493
31.097186	1149.612364	16.961511
31.158521	1140.488617	16.966528
31.269635	1137.674400	16.971546
30.984952	1143.982692	16.976563
31.217381	1145.626692	16.981581
31.058117	1154.309967	16.986599
31.386663	1148.980266	16.991616
31.169745	1151.201398	16.996634
30.745196	1159.533691	17.001651
30.969530	1168.672406	17.006669
31.308854	1169.910022	17.011687
31.076502	1182.159786	17.016704
31.025719	1174.677732	17.021722
31.484186	1175.396325	17.026739
31.490705	1171.093703	17.031757
31.455575	1167.561827	17.036775
31.305158	1166.021151	17.041792
31.616822	1187.861673	17.046810
31.556979	1201.420150	17.051827
32.150859	1203.370319	17.056845
32.242263	1203.387083	17.061863
31.974592	1179.464739	17.066880
31.966500	1170.903743	17.071898
31.801660	1167.045912	17.076915
32.012571	1164.403753	17.081933
31.760956	1153.046029	17.086951
31.843605	1161.239006	17.091968
31.613153	1149.300708	17.096986
31.480233	1169.271261	17.102003
31.500670	1188.085562	17.107021
32.164596	1190.124532	17.112039
32.324616	1199.395135	17.117056
32.544713	1188.879182	17.122074
32.278879	1204.151966	17.127091
32.538886	1196.134953	17.132109
32.349322	1185.848486	17.137127
32.082944	1167.599718	17.142144
32.201206	1165.086829	17.147162
31.938135	1185.714446	17.152179
32.451054	1187.575644	17.157197
32.472535	1192.087950	17.162215
32.262976	1201.283819	17.167232
32.676327	1182.909129	17.172250
32.443558	1190.699586	17.177267
32.907760	1189.095526	17.182285
32.693462	1188.934101	17.187303
32.483977	1179.573235	17.192320
32.904967	1174.431565	17.197338
32.184117	1175.648734	17.202355
32.609141	1177.751391	17.207373
32.739094	1189.326420	17.212391
32.406077	1201.762297	17.217408
32.477297	1189.110041	17.222426
32.537381	1193.649231	17.227443
32.771585	1194.514711	17.232461
32.755706	1191.073926	17.237479
32.577997	1192.719180	17.242496
32.887050	1185.763203	17.247514
32.582326	1186.494543	17.252531
33.121532	1183.196054	17.257549
33.183278	1179.492875	17.262567
32.875732	1187.680867	17.267584
33.122819	1175.705756	17.272602
33.034922	1187.245927	17.277619
32.856755	1177.500612	17.282637
32.529689	1194.275607	17.287655
32.770576	1191.695016	17.292672
33.543979	1204.372211	17.297690
33.242201	1210.179885	17.302707
33.481458	1204.027443	17.307725
33.545076	1201.941627	17.312743
33.111399	1205.647783	17.317760
33.306629	1205.461001	17.322778
33.155219	1210.509879	17.327795
33.361694	1215.863739	17.332813
33.497667	1211.005736	17.337831
33.442163	1212.583167	17.342848
33.286917	1211.358593	17.347866
33.145012	1214.728587	17.352883
32.957133	1214.290197	17.357901
33.442203	1213.828386	17.362919
33.610791	1196.125924	17.367936
33.888894	1212.850142	17.372954
33.803171	1208.693835	17.377971
34.033237	1216.786311	17.382989
33.847875	1201.721487	17.388007
33.858713	1199.779018	17.393024
33.922150	1194.149853	17.398042
33.773427	1193.536318	17.403059
33.826835	1202.148655	17.408077
33.772082	1207.677550	17.413095
34.071828	1224.684973	17.418112
34.175249	1233.529186	17.423130
34.124211	1235.017902	17.428147
34.401849	1227.641174	17.433165
34.405515	1202.218851	17.438183
34.206552	1203.626512	17.443200
34.457725	1198.185189	17.448218
34.290287	1202.393135	17.453235
34.129350	1194.525987	17.458253
34.255332	1197.172871	17.463271
33.947241	1190.918195	17.468288
33.991936	1200.328704	17.473306
34.099148	1214.559682	17.478323
34.255090	1224.606058	17.483341
34.525376	1228.052015	17.488359
34.274190	1235.756181	17.493376
34.642026	1225.607859	17.498394
34.685773	1229.775995	17.503411
34.520046	1229.166449	17.508429
34.499024	1227.155827	17.513447
34.315605	1226.954854	17.518464
34.200593	1223.922316	17.523482
34.430584	1221.953668	17.528499
34.323818	1241.092356	17.533517
34.868525	1238.053145	17.538535
34.431995	1259.118521	17.543552
34.998279	1256.461906	17.548570
34.877121	1258.925067	17.553587
35.021649	1257.326589	17.558605
35.470855	1249.196208	17.563623
34.964393	1254.410450	17.568640
35.183792	1241.139852	17.573658
34.830881	1242.366490	17.578675
34.890772	1253.559698	17.583693
35.204732	1252.531365	17.588711
35.073202	1258.306396	17.593728
35.168897	1257.549137	17.598746
35.189492	1248.138202	17.603763
34.878069	1255.833831	17.608781
35.438160	1247.935880	17.613799
35.039681	1246.009674	17.618816
35.439976	1240.430324	17.623834
35.453724	1244.574095	17.628851
35.213914	1249.350626	17.633869
35.693853	1242.680119	17.638887
35.315210	1246.635816	17.643904
35.389629	1245.995442	17.648922
35.620677	1250.694363	17.653939
35.271334	1259.234526	17.658957
35.485946	1246.539042	17.663975
35.223810	1266.697389	17.668992
35.770803	1269.105054	17.674010
35.974387	1276.299507	17.679027
35.931022	1271.885825	17.684045
36.441531	1268.831199	17.689063
35.861706	1256.393150	17.694080
35.469075	1243.697044	17.699098
35.861915	1251.323727	17.704115
36.160908	1269.477815	17.709133
36.384087	1258.752279	17.714151
35.988393	1264.051945	17.719168
35.964084	1236.173122	17.724186
36.034131	1252.014966	17.729203
36.001089	1265.036469	17.734221
35.888021	1270.824594	17.739239
35.668282	1266.496941	17.744256
36.206907	1270.454785	17.749274
36.124267	1266.713642	17.754291
36.259267	1278.279835	17.759309
36.506224	1267.146681	17.764327
35.922019	1268.976619	17.769344
36.143618	1285.450447	17.774362
36.301272	1269.371725	17.779379
36.181608	1271.478392	17.784397
36.665993	1279.063980	17.789415
36.679728	1294.996068	17.794432
36.601691	1292.547875	17.799450
36.646801	1296.561494	17.804467
36.613049	1284.578580	17.809485
36.235544	1289.034423	17.814503
36.275483	1297.701591	17.819520
36.815561	1288.647049	17.824538
36.865692	1290.458178	17.829555
36.802083	1284.596270	17.834573
36.751137	1273.541666	17.839591
36.764790	1286.098252	17.844608
37.065813	1286.550193	17.849626
37.060447	1278.310689	17.854643
36.996113	1293.265068	17.859661
37.256892	1277.409222	17.864679
37.040036	1284.295453	17.869696
36.865112	1288.075390	17.874714
36.985538	1279.425783	17.879731
36.778054	1290.558491	17.884749
37.395675	1296.319175	17.889767
37.378081	1312.014169	17.894784
37.742123	1291.404306	17.899802
37.544230	1276.554243	17.904819
37.246067	1286.096844	17.909837
37.361675	1282.204057	17.914855
37.355663	1273.989068	17.919872
36.916994	1277.611432	17.924890
37.607684	1290.336025	17.929907
37.365658	1301.009356	17.934925
38.006383	1307.069924	17.939943
37.496473	1307.637566	17.944960
37.584568	1299.952015	17.949978
37.808167	1299.087410	17.954995
37.644902	1302.373759	17.960013
37.739900	1303.948374	17.965031
37.731675	1302.266881	17.970048
37.750296	1299.980838	17.975066
38.078563	1312.269148	17.980083
37.772386	1311.372024	17.985101
37.651773	1294.242167	17.990119
38.009097	1297.805824	17.995136
37.914764	1295.876786	18.000154
38.034515	1297.475259	18.005171
37.781933	1299.971166	18.010189
37.843593	1293.538434	18.015207
37.590824	1300.769929	18.020224
38.151547	1322.140609	18.025242
38.584384	1323.242134	18.030259
38.302799	1320.066457	18.035277
38.612915	1324.237839	18.040295
38.931557	1318.353691	18.045312
38.301763	1300.830868	18.050330
38.448269	1289.560382	18.055347
38.043009	1288.039171	18.060365
38.510591	1307.099762	18.065383
38.448888	1320.929480	18.070400
38.623711	1316.367541	18.075418
38.749385	1307.084462	18.080435
38.621074	1327.058985	18.085453
38.757356	1316.650877	18.090471
39.433990	1315.381335	18.095488
38.667928	1315.725988	18.100506
38.731424	1305.558820	18.105523
39.165785	1318.345476	18.110541
38.995121	1318.212857	18.115559
39.066072	1318.057632	18.120576
38.772685	1305.411405	18.125594
38.841414	1298.763556	18.130611
38.944405	1313.989673	18.135629
38.844642	1312.019016	18.140647
38.911282	1312.670888	18.145664
38.751115	1330.981227	18.150682
38.756382	1326.665581	18.155699
38.766404	1319.282645	18.160717
38.718337	1336.303579	18.165735
39.055108	1351.611951	18.170752
39.092024	1339.417147	18.175770
39.586055	1341.306877	18.180787
39.393084	1358.114214	18.185805
39.276507	1357.130449	18.190823
39.469315	1347.901400	18.195840
39.348319	1354.884798	18.200858
39.416166	1345.121161	18.205875
39.310542	1354.891992	18.210893
39.556704	1351.648782	18.215911
39.490782	1359.467454	18.220928
39.676009	1374.765069	18.225946
40.048650	1378.026649	18.230963
40.159416	1383.698902	18.235981
40.026958	1360.659321	18.240999
39.923425	1347.225884	18.246016
39.787961	1349.732165	18.251034
40.126138	1361.322712	18.256051
39.939995	1352.836897	18.261069
40.175028	1350.554647	18.266087
39.942879	1355.481500	18.271104
39.962843	1343.209781	18.276122
40.299540	1361.179031	18.281139
40.491099	1366.564932	18.286157
40.559376	1362.193988	18.291175
40.479384	1345.531706	18.296192
40.143921	1346.701341	18.301210
40.199817	1346.775935	18.306227
40.351199	1344.658079	18.311245
40.162340	1351.736340	18.316263
40.435162	1358.352145	18.321280
40.148211	1364.891578	18.326298
40.367770	1365.065095	18.331315
40.342785	1368.423084	18.336333
40.284407	1363.855184	18.341351
40.594888	1365.889603	18.346368
40.426037	1364.914081	18.351386
40.551808	1372.341683	18.356403
40.417126	1374.934442	18.361421
40.753353	1393.297652	18.366439
40.814001	1400.485472	18.371456
40.768069	1400.277523	18.376474
41.349751	1389.592249	18.381491
41.329531	1385.411489	18.386509
41.254382	1382.718348	18.391527
41.486143	1365.359930	18.396544
41.222568	1360.969621	18.401562
41.052590	1357.566466	18.406579
40.936994	1354.776091	18.411597
41.279097	1377.278693	18.416615
41.435429	1384.835879	18.421632
41.236387	1384.123381	18.426650
41.406264	1379.427219	18.431667
41.387141	1384.717054	18.436685
41.323137	1372.771546	18.441703
41.066744	1378.171444	18.446720
41.078828	1383.565555	18.451738
41.384924	1385.566257	18.456755
41.499423	1385.583732	18.461773
41.412731	1392.110948	18.466791
41.606767	1383.888824	18.471808
41.562189	1398.485560	18.476826
41.712764	1385.824163	18.481843
41.801915	1381.630054	18.486861
41.546373	1393.373453	18.491879
42.031861	1398.359070	18.496896
42.115106	1406.930770	18.501914
42.151454	1405.774900	18.506931
42.172209	1402.801573	18.511949
42.189847	1403.596567	18.516967
42.267589	1379.796532	18.521984
41.668062	1385.093706	18.527002
41.958715	1403.496935	18.532019
42.024146	1412.026508	18.537037
42.063232	1399.406945	18.542055
42.804654	1402.086793	18.547072
42.548477	1415.108490	18.552090
42.802052	1402.866024	18.557107
42.891212	1394.844271	18.562125
42.720754	1400.753134	18.567143
42.704739	1376.206887	18.572160
42.191227	1377.119765	18.577178
42.376256	1375.548239	18.582195
42.611017	1380.044645	18.587213
42.724849	1385.526654	18.592231
42.690070	1388.456993	18.597248
42.461606	1392.246589	18.602266
42.343523	1400.538407	18.607283
42.774812	1398.912604	18.612301
42.469158	1408.023505	18.617319
42.641110	1398.277076	18.622336
42.643856	1394.601702	18.627354
43.193209	1396.015431	18.632371
42.992516	1398.119955	18.637389
42.708284	1397.035168	18.642407
42.948152	1399.518603	18.647424
43.205316	1421.596388	18.652442
43.487772	1428.570623	18.657459
43.306990	1407.502873	18.662477
43.054652	1411.842606	18.667495
43.690751	1421.130724	18.672512
43.512355	1414.575623	18.677530
43.346001	1402.497222	18.682547
43.335586	1400.317327	18.687565
43.634698	1421.492236	18.692583
43.528658	1417.260303	18.697600
43.818800	1424.676319	18.702618
43.856082	1412.563669	18.707635
43.704013	1403.013871	18.712653
43.841585	1393.835648	18.717671
43.476228	1392.581812	18.722688
43.355361	1399.046774	18.727706
43.690218	1411.544874	18.732723
43.742310	1418.657749	18.737741
43.599490	1430.079635	18.742759
43.961208	1419.053967	18.747776
43.881246	1431.603507	18.752794
44.018349	1427.272936	18.757811
44.186304	1420.722795	18.762829
43.984874	1416.625311	18.767847
44.222818	1411.214441	18.772864
44.162694	1420.422554	18.777882
44.040471	1416.537344	18.782899
44.060982	1421.885595	18.787917
44.048700	1446.387548	18.792935
44.203227	1444.916516	18.797952
44.444546	1454.110658	18.802970
44.279509	1455.937877	18.807987
44.473585	1455.292287	18.813005
44.427219	1456.694830	18.818023
44.768279	1436.897127	18.823040
44.354574	1453.872917	18.828058
44.411012	1439.134586	18.833075
44.582264	1445.718204	18.838093
44.433776	1463.500068	18.843111
44.642625	1471.322008	18.848128
44.948570	1468.473370	18.853146
45.062900	1475.747421	18.858163
45.050475	1464.844562	18.863181
45.100546	1465.796383	18.868199
45.146894	1466.983830	18.873216
45.093949	1465.313645	18.878234
44.705342	1463.660940	18.883251
45.234386	1460.234365	18.888269
45.253522	1461.305457	18.893287
45.324552	1451.174936	18.898304
45.290037	1463.245990	18.903322
45.015931	1468.758083	18.908339
45.428615	1460.028588	18.913357
44.831561	1457.108529	18.918375
45.392044	1466.795537	18.923392
45.821878	1482.017017	18.928410
45.736836	1482.542996	18.933427
45.735433	1458.438438	18.938445
45.797538	1458.332699	18.943463
45.377422	1457.346336	18.948480
45.460088	1463.618067	18.953498
45.669237	1479.574544	18.958515
46.074485	1476.071388	18.963533
45.845974	1477.381804	18.968551
46.190334	1473.897764	18.973568
46.298909	1474.945023	18.978586
46.122775	1494.538740	18.983603
46.337775	1483.501645	18.988621
46.351967	1475.842389	18.993639
45.889920	1455.375901	18.998656
46.186350	1466.310324	19.003674
46.413917	1475.034961	19.008691
46.552024	1472.048134	19.013709
46.422673	1475.144885	19.018727
46.471446	1446.258652	19.023744
46.645413	1451.594545	19.028762
46.430441	1454.654659	19.033779
46.233912	1451.397191	19.038797
46.267074	1473.517577	19.043815
46.348546	1476.827294	19.048832
46.390741	1476.991149	19.053850
46.287475	1482.547251	19.058867
46.558469	1475.410252	19.063885
46.559335	1475.855311	19.068903
46.601007	1472.042205	19.073920
46.905257	1484.488343	19.078938
46.587887	1507.521907	19.083955
47.128836	1498.471430	19.088973
46.797127	1510.153301	19.093991
46.783938	1516.626696	19.099008
47.116297	1518.608314	19.104026
47.221424	1522.017859	19.109043
47.184922	1508.474593	19.114061
47.108032	1512.551141	19.119079
47.195225	1505.921015	19.124096
46.917063	1508.350914	19.129114
47.074654	1508.920254	19.134131
46.937352	1513.567934	19.139149
47.255350	1523.631620	19.144167
47.321082	1529.800087	19.149184
47.489777	1520.224767	19.154202
47.603094	1526.810907	19.159219
47.884786	1527.002895	19.164237
47.970077	1532.797902	19.169255
48.136351	1525.301657	19.174272
48.100048	1517.498382	19.179290
47.926476	1529.708397	19.184307
48.233733	1522.017224	19.189325
48.221633	1515.710353	19.194343
48.205052	1512.057434	19.199360
48.124775	1513.950368	19.204378
48.027983	1523.054379	19.209395
48.238670	1516.648299	19.214413
48.055124	1522.023021	19.219431
48.048319	1521.050826	19.224448
48.222903	1519.094840	19.229466
48.205726	1528.113069	19.234483
48.098038	1513.649985	19.239501
48.210415	1512.437455	19.244519
48.160200	1518.398138	19.249536
48.353268	1525.328928	19.254554
48.332784	1542.857280	19.259571
49.007733	1534.977404	19.264589
48.838039	1543.853740	19.269607
48.764976	1547.538177	19.274624
49.076126	1533.951219	19.279642
49.021052	1535.187316	19.284659
49.209749	1511.848799	19.289677
48.923443	1509.118491	19.294695
48.771959	1505.353631	19.299712
48.855740	1507.711321	19.304730
48.705557	1524.557433	19.309747
48.822097	1525.625818	19.314765
49.195620	1526.946780	19.319783
49.240648	1529.497862	19.324800
49.378956	1529.391536	19.329818
49.034331	1537.735231	19.334835
49.231496	1522.557870	19.339853
49.194751	1533.871371	19.344871
49.171612	1531.885072	19.349888
49.475188	1538.681677	19.354906
49.162970	1527.503353	19.359923
49.503669	1531.485904	19.364941
49.121877	1533.486924	19.369959
49.259339	1557.561408	19.374976
49.482278	1548.497318	19.379994
49.887087	1570.163959	19.385011
49.724293	1570.493562	19.390029
49.714929	1569.582213	19.395047
49.685469	1566.994468	19.400064
49.678252	1557.104928	19.405082
49.501242	1563.389890	19.410099
50.073257	1570.894224	19.415117
50.645538	1582.135465	19.420135
50.476800	1585.425929	19.425152
50.305877	1556.405341	19.430170
50.418904	1561.207512	19.435187
50.122642	1547.478424	19.440205
50.628151	1557.790640	19.445223
49.946306	1563.403998	19.450240
50.402979	1568.194852	19.455258
50.044946	1583.174623	19.460275
50.102481	1575.683725	19.465293
49.933686	1581.605766	19.470311
50.031185	1594.032031	19.475328
50.519292	1589.999472	19.480346
50.884772	1603.193567	19.485363
50.972553	1610.625004	19.490381
50.968494	1599.130777	19.495399
50.859468	1616.909643	19.500416
50.944049	1598.973779	19.505434
50.870866	1612.378739	19.510451
51.180081	1609.045341	19.515469
51.171620	1596.905660	19.520487
51.139952	1607.524366	19.525504
51.333337	1587.899870	19.530522
51.239530	1601.066525	19.535539
51.236678	1601.738553	19.540557
51.445207	1592.565415	19.545575
51.584888	1597.695436	19.550592
51.318359	1600.935928	19.555610
51.370682	1601.341586	19.560627
51.497418	1602.867291	19.565645
51.568416	1596.924563	19.570663
51.391436	1603.160329	19.575680
51.558518	1615.118868	19.580698
51.617897	1620.737700	19.585715
51.335177	1629.426684	19.590733
51.783414	1626.330909	19.595751
51.740132	1624.965373	19.600768
52.523634	1624.387317	19.605786
51.994410	1622.343510	19.610803
51.899950	1623.457397	19.615821
52.141826	1620.375254	19.620839
52.034957	1617.708767	19.625856
52.557550	1611.050541	19.630874
52.546111	1612.965572	19.635891
52.506164	1613.225867	19.640909
52.559465	1603.563473	19.645927
52.453600	1615.278764	19.650944
52.372894	1614.000309	19.655962
52.679633	1618.875396	19.660979
52.585207	1615.803753	19.665997
52.569674	1614.378914	19.671015
52.292427	1616.999405	19.676032
52.227609	1616.139927	19.681050
52.144708	1618.823371	19.686067
52.611198	1639.283406	19.691085
53.068920	1638.679272	19.696103
52.682855	1646.823401	19.701120
52.847818	1660.723830	19.706138
52.774884	1656.893794	19.711155
52.708970	1652.287294	19.716173
53.039121	1648.407973	19.721191
53.010979	1644.141650	19.726208
53.256381	1653.213599	19.731226
53.160417	1672.190623	19.736243
53.178962	1674.476255	19.741261
53.425174	1680.730497	19.746279
53.099196	1688.479921	19.751296
53.661748	1682.671459	19.756314
53.474077	1684.427453	19.761331
53.146911	1681.573762	19.766349
53.424917	1668.598589	19.771367
53.285598	1683.926917	19.776384
53.755433	1687.554743	19.781402
54.908301	1679.195671	19.786419
54.806415	1659.752144	19.791437
54.581005	1650.302489	19.796455
54.611326	1651.285142	19.801472
54.561468	1622.986856	19.806490
54.545799	1624.311910	19.811507
54.452801	1610.805052	19.816525
54.450680	1604.962778	19.821543
54.215823	1604.418963	19.826560
54.477104	1599.931226	19.831578
54.538966	1607.513778	19.836595
54.262401	1600.825624	19.841613
54.462422	1593.735137	19.846631
54.680383	1607.808432	19.851648
54.604716	1608.436594	19.856666
54.566999	1607.862958	19.861683
54.222815	1609.479275	19.866701
54.798639	1623.008271	19.871719
54.739440	1645.121532	19.876736
54.963372	1642.515128	19.881754
54.902055	1647.801594	19.886771
54.890545	1646.641214	19.891789
54.903451	1629.799905	19.896807
55.099851	1639.964854	19.901824
55.078367	1637.377748	19.906842
55.041470	1645.103197	19.911859
54.910035	1641.168868	19.916877
54.989676	1635.808880	19.921895
54.810365	1636.347292	19.926912
55.206634	1651.890199	19.931930
54.876420	1658.737461	19.936947
55.091375	1669.096977	19.941965
55.375233	1678.113773	19.946983
55.371737	1673.718384	19.952000
55.296697	1671.487523	19.957018
55.719051	1695.219904	19.962035
55.577103	1706.258627	19.967053
56.122488	1701.981168	19.972071
55.691666	1711.450884	19.977088
56.012970	1703.173705	19.982106
56.521913	1704.175883	19.987123
56.217671	1696.795883	19.992141
56.128122	1679.651014	19.997159
56.099937	1675.448856	20.002176
55.996962	1692.006871	20.007194
56.034567	1695.629557	20.012211
56.015962	1709.673344	20.017229
56.149544	1704.012916	20.022247
56.200545	1697.200521	20.027264
56.310527	1697.398054	20.032282
56.680581	1695.731559	20.037299
56.152913	1698.306249	20.042317
56.452136	1695.814153	20.047335
55.970795	1709.624794	20.052352
56.662616	1712.488074	20.057370
56.731425	1723.541977	20.062387
56.598815	1738.562002	20.067405
56.648329	1721.280340	20.072423
56.816172	1727.640849	20.077440
56.734217	1717.438593	20.082458
56.854453	1724.365959	20.087475
56.953384	1749.895570	20.092493
57.543232	1744.734472	20.097511
57.362927	1748.047154	20.102528
57.297820	1748.894615	20.107546
57.658594	1741.570826	20.112563
57.527122	1740.552099	20.117581
58.045411	1745.212762	20.122599
57.972840	1743.692624	20.127616
57.221380	1724.326830	20.132634
57.420372	1722.299076	20.137651
57.510885	1728.140730	20.142669
57.565044	1735.628171	20.147687
57.899045	1740.562172	20.152704
57.680104	1741.978102	20.157722
57.879551	1744.669236	20.162739
57.713970	1735.532638	20.167757
58.270604	1737.440615	20.172775
57.950992	1726.626122	20.177792
57.748672	1735.939407	20.182810
58.217909	1749.716614	20.187827
58.144887	1761.284085	20.192845
58.277586	1761.735120	20.197863
58.264166	1755.198867	20.202880
58.430696	1759.099640	20.207898
58.728121	1755.521337	20.212915
58.246130	1768.716458	20.217933
58.209036	1766.560209	20.222951
58.187519	1767.203835	20.227968
58.285341	1778.194919	20.232986
58.549743	1794.114643	20.238003
58.663450	1785.171997	20.243021
59.378818	1788.319756	20.248039
59.205829	1784.678840	20.253056
59.117970	1785.645601	20.258074
59.109205	1771.421215	20.263091
58.970158	1779.332491	20.268109
59.278394	1783.230128	20.273127
59.240303	1776.224765	20.278144
59.284150	1788.840742	20.283162
59.670771	1786.891806	20.288179
59.349069	1784.964848	20.293197
59.360411	1790.530663	20.298215
59.405781	1779.528473	20.303232
59.443443	1781.794034	20.308250
59.509377	1775.895966	20.313267
59.273121	1790.183840	20.318285
59.850843	1806.271661	20.323303
59.853192	1811.467946	20.328320
59.387148	1807.811677	20.333338
59.413961	1799.797457	20.338355
59.582362	1804.364594	20.343373
60.140055	1796.408304	20.348391
60.049590	1810.546332	20.353408
60.198289	1830.016333	20.358426
60.543441	1824.106750	20.363443
60.677177	1818.216751	20.368461
60.586209	1800.673599	20.373479
60.831348	1788.531030	20.378496
60.731853	1790.905862	20.383514
60.955598	1785.733207	20.388531
60.622395	1786.276780	20.393549
60.877370	1781.816211	20.398567
61.077492	1790.170408	20.403584
60.358402	1796.803870	20.408602
60.761653	1794.472895	20.413619
60.981445	1798.786880	20.418637
60.829863	1792.608247	20.423655
60.817740	1793.014521	20.428672
60.642088	1810.581810	20.433690
61.295579	1819.704717	20.438707
60.794002	1826.302642	20.443725
61.168337	1840.747907	20.448743
61.211965	1838.747583	20.453760
61.269369	1835.912786	20.458778
61.346275	1831.202327	20.463795
61.304654	1831.452273	20.468813
61.133494	1837.125222	20.473831
61.573252	1852.005506	20.478848
61.364883	1864.434112	20.483866
61.495316	1858.142126	20.488883
61.799962	1860.807827	20.493901
61.574286	1855.244894	20.498919
61.926731	1853.874176	20.503936
61.746353	1854.109457	20.508954
62.243045	1873.064182	20.513971
62.376243	1867.992870	20.518989
62.315073	1863.509724	20.524007
62.378450	1853.852201	20.529024
62.520848	1859.015125	20.534042
62.314370	1859.033875	20.539059
62.619199	1862.695702	20.544077
62.450019	1873.318616	20.549095
62.569505	1866.756220	20.554112
62.718610	1870.664625	20.559130
62.740987	1868.735912	20.564147
62.709795	1870.360372	20.569165
62.661418	1869.712708	20.574183
63.000005	1877.255570	20.579200
62.763898	1871.908112	20.584218
62.689972	1876.254907	20.589235
63.000086	1873.183483	20.594253
62.728234	1859.649471	20.599271
63.131067	1875.456650	20.604288
62.973381	1872.797729	20.609306
63.048262	1886.424498	20.614323
63.028915	1890.777631	20.619341
62.851780	1893.412921	20.624359
63.670107	1897.086351	20.629376
63.450627	1898.036684	20.634394
63.536040	1895.706252	20.639411
63.322938	1902.260477	20.644429
63.486592	1910.844365	20.649447
63.835435	1915.574612	20.654464
63.759710	1924.872209	20.659482
64.149982	1929.814294	20.664499
64.405535	1918.760543	20.669517
64.306098	1927.086960	20.674535
64.363583	1910.770602	20.679552
64.147854	1894.902321	20.684570
64.569819	1896.038951	20.689587
64.487921	1891.152177	20.694605
64.611828	1885.845214	20.699623
64.489986	1884.859331	20.704640
64.232363	1882.526930	20.709658
64.322363	1872.293597	20.714675
64.394291	1894.530415	20.719693
64.298884	1914.246941	20.724711
64.536426	1917.121161	20.729728
64.479582	1907.672428	20.734746
64.615283	1918.849854	20.739763
64.814535	1920.896036	20.744781
64.525256	1918.811750	20.749799
65.220560	1923.769760	20.754816
64.977386	1924.672243	20.759834
65.453932	1919.455408	20.764851
65.770052	1923.196873	20.769869
65.417317	1935.824570	20.774887
65.799661	1930.199521	20.779904
65.353776	1931.601006	20.784922
65.889482	1928.041944	20.789939
65.640277	1920.584244	20.794957
65.374504	1928.370685	20.799975
65.758389	1926.136976	20.804992
65.616395	1933.734479	20.810010
65.844650	1928.416951	20.815027
66.075336	1924.189072	20.820045
65.860447	1930.265306	20.825063
65.783713	1927.094032	20.830080
66.029892	1924.838595	20.835098
65.880623	1927.872001	20.840115
65.842778	1926.216198	20.845133
65.711963	1949.001703	20.850151
66.233995	1960.118666	20.855168
66.169199	1958.900342	20.860186
66.044478	1944.779201	20.865203
66.422694	1946.364164	20.870221
66.266756	1945.187867	20.875239
66.854418	1947.206679	20.880256
67.143039	1960.806659	20.885274
66.958531	1957.110917	20.890291
66.988824	1954.959647	20.895309
67.152347	1965.974848	20.900327
67.586168	1956.794184	20.905344
67.309867	1948.081622	20.910362
66.692087	1939.543787	20.915379
67.070070	1950.710725	20.920397
66.865717	1964.041218	20.925415
67.463142	1956.996697	20.930432
67.549257	1962.195135	20.935450
67.285419	1953.048465	20.940467
67.421455	1958.314630	20.945485
67.543930	1968.860874	20.950503
67.661706	1963.622214	20.955520
67.561615	1966.893148	20.960538
67.449516	1965.773576	20.965555
67.896402	1982.922079	20.970573
67.984706	1973.353266	20.975591
68.641240	1964.867419	20.980608
68.485987	1972.193142	20.985626
68.547498	1953.914844	20.990643
68.259005	1935.997326	20.995661
68.319067	1941.544714	21.000679
68.329294	1941.486320	21.005696
68.183633	1944.456935	21.010714
68.629527	1961.202861	21.015731
68.743093	1961.391539	21.020749
68.310427	1951.339985	21.025767
68.513339	1964.386469	21.030784
68.265285	1972.356797	21.035802
68.440020	1975.610663	21.040819
68.825646	1967.887424	21.045837
68.579845	1973.715657	21.050855
69.053719	1975.426535	21.055872
68.935489	1977.232105	21.060890
68.814281	1994.366237	21.065907
69.151548	1994.704941	21.070925
69.256248	1998.146352	21.075943
69.568966	1996.237750	21.080960
69.411608	1995.300047	21.085978
69.247431	2007.556324	21.090995
69.471984	2002.129944	21.096013
69.619365	2000.070726	21.101031
69.433635	1995.041641	21.106048
69.759139	1990.937237	21.111066
69.481031	2000.226200	21.116083
69.858498	2016.637070	21.121101
69.677406	2024.939241	21.126119
69.631769	2021.091415	21.131136
69.980867	2032.453916	21.136154
69.939161	2032.828080	21.141171
70.385956	2028.177491	21.146189
70.075504	2045.117381	21.151207
70.252209	2050.479406	21.156224
70.188981	2068.512028	21.161242
70.410602	2062.441484	21.166259
70.688921	2063.986082	21.171277
70.523410	2061.084349	21.176295
70.616422	2053.927090	21.181312
71.133522	2057.589909	21.186330
70.654035	2063.118829	21.191347
71.032087	2051.928215	21.196365
70.924061	2069.126388	21.201383
71.148232	2055.694080	21.206400
71.101502	2055.410473	21.211418
71.049199	2078.840223	21.216435
71.719553	2075.199829	21.221453
71.665770	2070.015267	21.226471
71.831659	2078.088886	21.231488
71.386479	2069.171504	21.236506
71.647660	2079.190029	21.241523
71.833239	2077.788996	21.246541
71.782992	2079.970121	21.251559
72.010135	2079.214721	21.256576
71.775983	2079.154980	21.261594
71.973401	2085.264316	21.266611
72.170640	2077.332016	21.271629
71.880144	2084.070351	21.276647
71.889270	2069.457139	21.281664
71.867223	2075.354726	21.286682
71.943797	2081.015960	21.291699
72.220254	2077.433175	21.296717
72.487187	2089.236423	21.301735
72.491067	2091.478087	21.306752
72.441055	2097.438763	21.311770
72.343469	2103.588782	21.316787
72.116278	2103.479864	21.321805
72.333496	2108.538194	21.326823
72.439144	2121.999669	21.331840
72.921980	2127.962260	21.336858
73.208282	2124.734106	21.341875
73.361965	2116.312373	21.346893
73.521570	2121.186150	21.351911
73.641475	2111.456138	21.356928
73.734606	2102.531077	21.361946
73.505488	2089.751151	21.366963
73.666755	2073.020657	21.371981
73.606653	2069.456089	21.376999
73.250793	2075.979061	21.382016
73.559221	2087.262898	21.387034
73.657147	2106.698336	21.392051
73.807457	2091.618898	21.397069
73.817782	2109.861836	21.402087
73.712296	2109.213560	21.407104
73.999564	2113.749338	21.412122
73.941047	2117.007528	21.417139
74.449847	2098.270930	21.422157
74.220508	2101.412671	21.427175
74.459391	2101.004710	21.432192
74.111523	2106.551066	21.437210
74.140288	2106.715179	21.442227
74.391526	2117.809097	21.447245
74.437702	2135.173775	21.452263
74.446398	2135.527409	21.457280
74.547571	2133.184692	21.462298
74.212439	2128.976049	21.467315
74.468695	2133.738986	21.472333
74.720761	2157.258115	21.477351
75.020603	2167.875573	21.482368
75.192185	2164.465006	21.487386
75.172136	2176.560800	21.492403
75.139768	2169.147654	21.497421
75.031516	2168.233910	21.502439
75.019664	2156.457310	21.507456
75.576190	2163.391515	21.512474
75.303526	2191.773777	21.517491
75.951250	2182.684396	21.522509
75.667083	2183.323807	21.527527
75.904917	2183.873418	21.532544
75.918414	2181.405233	21.537562
76.038135	2179.591487	21.542579
76.445666	2174.969389	21.547597
76.070408	2177.790207	21.552615
76.323028	2182.659853	21.557632
76.632308	2173.255567	21.562650
76.265239	2178.301423	21.567667
76.186896	2173.107893	21.572685
76.171294	2177.509697	21.577703
76.450003	2172.752993	21.582720
76.759869	2182.184848	21.587738
76.718459	2175.428453	21.592755
76.904935	2175.220669	21.597773
76.798735	2184.240411	21.602791
76.577787	2201.702449	21.607808
77.025597	2187.905737	21.612826
76.703127	2198.223915	21.617843
76.874332	2194.116414	21.622861
77.296425	2195.108374	21.627879
77.257144	2202.941378	21.632896
77.422544	2204.129286	21.637914
77.006557	2213.625594	21.642931
77.515510	2222.028593	21.647949
77.751072	2216.799122	21.652967
77.782649	2216.203778	21.657984
78.180073	2207.178575	21.663002
78.112653	2219.788687	21.668019
77.962257	2210.198546	21.673037
77.817961	2219.041350	21.678055
78.098458	2227.484858	21.683072
78.199763	2217.629517	21.688090
77.955946	2228.384289	21.693107
77.957830	2214.881102	21.698125
78.218411	2220.098433	21.703143
78.062527	2214.050842	21.708160
78.408512	2216.478101	21.713178
78.570716	2247.961189	21.718195
78.849373	2246.787459	21.723213
78.912356	2251.415650	21.728231
78.826815	2253.308559	21.733248
78.883465	2244.944519	21.738266
78.807105	2249.468579	21.743283
78.706398	2243.165226	21.748301
78.673856	2237.286797	21.753319
78.687242	2253.756114	21.758336
79.168062	2252.621216	21.763354
79.127766	2259.763525	21.768371
79.447354	2250.336625	21.773389
79.597533	2255.187004	21.778407
79.576175	2256.539428	21.783424
79.900766	2249.076313	21.788442
79.318487	2259.526432	21.793459
79.791497	2256.867353	21.798477
80.107392	2260.036935	21.803495
80.034306	2286.956780	21.808512
80.208698	2280.888641	21.813530
80.184446	2284.399846	21.818547
80.017239	2276.099943	21.823565
80.138368	2279.156055	21.828583
80.089538	2289.047806	21.833600
80.682433	2291.484668	21.838618
80.543966	2294.036475	21.843635
80.504877	2284.080875	21.848653
80.650817	2289.945865	21.853671
80.496122	2305.951709	21.858688
80.847717	2301.796066	21.863706
80.539400	2312.292086	21.868723
81.002956	2301.375332	21.873741
80.970286	2299.189342	21.878759
80.562999	2316.485071	21.883776
81.487833	2319.889847	21.888794
81.320798	2344.412107	21.893811
81.233389	2326.864618	21.898829
81.618658	2328.633680	21.903847
81.744714	2330.589068	21.908864
81.993564	2329.729880	21.913882
82.356519	2323.000298	21.918899
82.204183	2323.660053	21.923917
81.985068	2329.745014	21.928935
81.960472	2322.324407	21.933952
82.350625	2322.103240	21.938970
82.372204	2315.980029	21.943987
82.271721	2316.651293	21.949005
82.670159	2317.239327	21.954023
82.362914	2321.015397	21.959040
82.805212	2318.456454	21.964058
82.736195	2316.306387	21.969075
82.701407	2315.420059	21.974093
82.763986	2313.026807	21.979111
82.702133	2309.883307	21.984128
82.561598	2312.385857	21.989146
82.799507	2341.785718	21.994163
82.940733	2353.525301	21.999181
83.085056	2348.163629	22.004199
83.223915	2357.444925	22.009216
83.479343	2341.851452	22.014234
83.187655	2336.369719	22.019251
82.743332	2344.557498	22.024269
83.097796	2353.559482	22.029287
83.377529	2376.535240	22.034304
83.626021	2376.542190	22.039322
84.032350	2385.220881	22.044339
83.551132	2375.820332	22.049357
84.116189	2371.780765	22.054375
83.838262	2363.580009	22.059392
83.819119	2374.620175	22.064410
83.810078	2389.121236	22.069427
84.160694	2407.774405	22.074445
84.598041	2401.908027	22.079463
84.609981	2405.935882	22.084480
84.382224	2401.886574	22.089498
84.311983	2393.317846	22.094515
84.184812	2400.064957	22.099533
84.676595	2406.841085	22.104551
84.438454	2433.158973	22.109568
84.528207	2431.267872	22.114586
84.965451	2436.058473	22.119603
84.784187	2436.959808	22.124621
85.395573	2435.583260	22.129639
85.687852	2450.373936	22.134656
85.472045	2451.438646	22.139674
85.692732	2448.405311	22.144691
85.961016	2453.422642	22.149709
86.283390	2439.159458	22.154727
85.862453	2430.033148	22.159744
85.997866	2418.452472	22.164762
86.308864	2415.381191	22.169779
85.851938	2417.519136	22.174797
85.860583	2421.131032	22.179815
86.304269	2433.980463	22.184832
86.316015	2441.802007	22.189850
86.555591	2438.462226	22.194867
86.544312	2440.768056	22.199885
86.455316	2438.027414	22.204903
86.375648	2440.559294	22.209920
86.260303	2432.249753	22.214938
86.614565	2441.569320	22.219955
86.599408	2458.656327	22.224973
86.743991	2456.088883	22.229991
87.154878	2462.327652	22.235008
87.155181	2471.262840	22.240026
87.129415	2466.566594	22.245043
87.070111	2471.647707	22.250061
87.287560	2467.479346	22.255079
87.134429	2476.970960	22.260096
87.336350	2484.876447	22.265114
87.847380	2502.587731	22.270131
87.566028	2502.748371	22.275149
87.829430	2489.399751	22.280167
87.706815	2492.738292	22.285184
87.811398	2495.741279	22.290202
88.008211	2491.026750	22.295219
88.168640	2510.580117	22.300237
88.361887	2518.267777	22.305255
88.371888	2521.416311	22.310272
88.596691	2521.695271	22.315290
88.756176	2512.458043	22.320307
88.672350	2511.744363	22.325325
88.640204	2507.170805	22.330343
88.631926	2521.472467	22.335360
89.065076	2528.345341	22.340378
88.789373	2514.534632	22.345395
88.523680	2517.372837	22.350413
88.532057	2518.209968	22.355431
88.934738	2527.346007	22.360448
88.683636	2536.707004	22.365466
89.240222	2525.805428	22.370483
89.290676	2539.877730	22.375501
89.310814	2533.711367	22.380519
89.619760	2558.254916	22.385536
89.717001	2569.201978	22.390554
89.731683	2564.621453	22.395571
89.502218	2558.376252	22.400589
89.958435	2555.118358	22.405607
89.747303	2562.136288	22.410624
89.729129	2562.799473	22.415642
89.927428	2568.880118	22.420659
90.035802	2588.091023	22.425677
90.434764	2587.915246	22.430695
90.242983	2595.198483	22.435712
90.500920	2592.999272	22.440730
90.780952	2579.911985	22.445747
90.442388	2593.896263	22.450765
91.078013	2605.136651	22.455783
91.701976	2595.237223	22.460800
91.580319	2602.529741	22.465818
91.108275	2600.828295	22.470835
91.251088	2605.401671	22.475853
91.537382	2616.869467	22.480871
91.391434	2606.564209	22.485888
91.792900	2606.415576	22.490906
91.890735	2597.058177	22.495923
92.148595	2596.569908	22.500941
92.047684	2599.153353	22.505959
92.391447	2607.854712	22.510976
92.185606	2615.441445	22.515994
92.309693	2605.439187	22.521011
91.935490	2609.153559	22.526029
91.779485	2602.950136	22.531047
91.894058	2603.864207	22.536064
91.697854	2608.302668	22.541082
92.197288	2621.335948	22.546099
92.261517	2626.628576	22.551117
92.291890	2628.815943	22.556135
92.486858	2642.812100	22.561152
92.832711	2652.484348	22.566170
92.945439	2648.877702	22.571187
93.013119	2653.395400	22.576205
93.168200	2645.428441	22.581223
93.271040	2645.669292	22.586240
92.782185	2655.751107	22.591258
93.410146	2661.437186	22.596275
93.383723	2662.827291	22.601293
93.735172	2671.023505	22.606311
94.006155	2667.836745	22.611328
93.837612	2671.719895	22.616346
94.019362	2668.204196	22.621363
93.712447	2672.403109	22.626381
94.077102	2672.999103	22.631399
94.237608	2670.175856	22.636416
93.765374	2678.294016	22.641434
94.562703	2679.340931	22.646451
94.394557	2701.074710	22.651469
94.808739	2698.850848	22.656487
94.653802	2684.981057	22.661504
94.802818	2692.250938	22.666522
95.003355	2686.677114	22.671539
94.895757	2703.844034	22.676557
94.963091	2689.797753	22.681575
95.410318	2688.094785	22.686592
95.217681	2688.395484	22.691610
95.711594	2681.494509	22.696627
95.373190	2699.993985	22.701645
95.482982	2696.382696	22.706663
95.359080	2690.529033	22.711680
95.222248	2705.856782	22.716698
95.850360	2718.010262	22.721715
95.960151	2712.812037	22.726733
95.910863	2711.621010	22.731751
95.737898	2713.929385	22.736768
95.862976	2714.837003	22.741786
96.101681	2710.931194	22.746803
96.076611	2725.858230	22.751821
96.289639	2730.631842	22.756839
96.715509	2721.523693	22.761856
96.464648	2733.366935	22.766874
96.469004	2725.342954	22.771891
96.878868	2726.807030	22.776909
96.899730	2738.633721	22.781927
97.195075	2745.947555	22.786944
97.113678	2758.727730	22.791962
97.491332	2749.820830	22.796979
97.569951	2760.037674	22.801997
97.440021	2755.997893	22.807015
97.770568	2752.925678	22.812032
97.434328	2759.868705	22.817050
97.904901	2743.481832	22.822067
97.595583	2743.993536	22.827085
97.683011	2752.635764	22.832103
98.238727	2738.324102	22.837120
98.028582	2745.104562	22.842138
97.872440	2752.779996	22.847155
98.467593	2775.436525	22.852173
98.529546	2774.954639	22.857191
99.173032	2765.743580	22.862208
99.030440	2769.113826	22.867226
99.103664	2756.327086	22.872243
99.205030	2759.761346	22.877261
99.245389	2750.637357	22.882279
99.078139	2731.874113	22.887296
98.809107	2751.835347	22.892314
99.127803	2753.680616	22.897331
99.194423	2763.625835	22.902349
98.980256	2776.179549	22.907367
99.252200	2763.913092	22.912384
99.493995	2775.693464	22.917402
99.759136	2775.009901	22.922419
99.522240	2780.957037	22.927437
99.370809	2787.538845	22.932455
99.933073	2782.087492	22.937472
99.751517	2786.588935	22.942490
99.860419	2805.648063	22.947507
100.065594	2809.600590	22.952525
100.217708	2813.455986	22.957543
100.506673	2810.720145	22.962560
100.541949	2808.344320	22.967578
100.339658	2819.127283	22.972595
100.607806	2823.433173	22.977613
100.663254	2834.718419	22.982631
100.705329	2834.131158	22.987648
100.604257	2833.449446	22.992666
101.212226	2837.657852	22.997683
101.430276	2836.105725	23.002701
101.109253	2846.068596	23.007719
101.260605	2852.988573	23.012736
101.043498	2857.265998	23.017754
101.936376	2850.086042	23.022771
102.185485	2851.745191	23.027789
102.050529	2850.860029	23.032807
102.319199	2849.926283	23.037824
102.688616	2848.425518	23.042842
102.789383	2840.044615	23.047859
102.799239	2848.504446	23.052877
102.493962	2850.195754	23.057895
103.011655	2824.478937	23.062912
102.475409	2821.692055	23.067930
102.798277	2831.543010	23.072947
102.869877	2840.945353	23.077965
102.942203	2841.930590	23.082983
102.975119	2841.540898	23.088000
102.993392	2844.566482	23.093018
102.927729	2842.411653	23.098035
102.978503	2845.508243	23.103053
103.002723	2837.613199	23.108071
103.147007	2843.792244	23.113088
103.275340	2865.548129	23.118106
103.558090	2866.191129	23.123123
103.591952	2868.822031	23.128141
103.407246	2880.953261	23.133159
103.420327	2885.164707	23.138176
103.251964	2895.441742	23.143194
103.519171	2903.089815	23.148211
103.912434	2909.689147	23.153229
104.136021	2927.114571	23.158247
104.318328	2920.863385	23.163264
104.246635	2929.754438	23.168282
104.995286	2947.998212	23.173299
105.212169	2938.359134	23.178317
105.190362	2948.022637	23.183335
105.870939	2941.195032	23.188352
105.874927	2941.046723	23.193370
105.554392	2920.350376	23.198387
105.701302	2913.326329	23.203405
105.195774	2920.616679	23.208423
105.821403	2915.909903	23.213440
105.591868	2912.601081	23.218458
105.457505	2934.993362	23.223475
105.805749	2937.904208	23.228493
105.623910	2941.871114	23.233511
105.859353	2938.473251	23.238528
105.965370	2943.774043	23.243546
105.799043	2947.463200	23.248563
106.328402	2945.129332	23.253581
106.321986	2960.426728	23.258599
106.600760	2959.784998	23.263616
106.562664	2969.948434	23.268634
106.727479	2987.659219	23.273651
106.950372	2994.687514	23.278669
106.641349	3005.226046	23.283687
107.287433	2987.353266	23.288704
107.263734	2986.838677	23.293722
107.010380	2992.888610	23.298739
107.356979	3004.660501	23.303757
107.120944	3026.151237	23.308775
107.423215	3021.726199	23.313792
107.673091	3014.600056	23.318810
107.635855	3020.914281	23.323827
108.088900	3028.265969	23.328845
108.180730	3039.791803	23.333863
108.491468	3042.586428	23.338880
108.700471	3036.620146	23.343898
108.996137	3046.343848	23.348915
109.114761	3032.228547	23.353933
108.739732	3036.499046	23.358951
108.928045	3029.747231	23.363968
108.941129	3035.544107	23.368986
108.813258	3034.096361	23.374003
108.820399	3027.581171	23.379021
108.681818	3038.861619	23.384039
108.872941	3016.396392	23.389056
109.233298	3035.329217	23.394074
108.973395	3050.342612	23.399091
109.362103	3051.454320	23.404109
109.523750	3063.470984	23.409127
109.704957	3056.348687	23.414144
109.697861	3068.540872	23.419162
109.456465	3076.513223	23.424179
110.332626	3076.912908	23.429197
109.890960	3076.192583	23.434215
110.292602	3091.118753	23.439232
110.291248	3091.110693	23.444250
110.474510	3107.604029	23.449267
110.829946	3105.998860	23.454285
110.901595	3117.559187	23.459303
111.111540	3113.034422	23.464320
111.310662	3111.225952	23.469338
110.821914	3107.702839	23.474355
111.314284	3108.619080	23.479373
111.296136	3097.784515	23.484391
111.337801	3102.914110	23.489408
111.527448	3112.598680	23.494426
111.545459	3142.113563	23.499443
111.794491	3131.502144	23.504461
111.594693	3134.669721	23.509479
111.704438	3140.373106	23.514496
111.894059	3140.870881	23.519514
111.830133	3162.805798	23.524531
112.326814	3148.923981	23.529549
112.217608	3154.828114	23.534567
112.117936	3167.604953	23.539584
112.374321	3178.309619	23.544602
112.486780	3184.675159	23.549619
113.198867	3181.378403	23.554637
113.247378	3193.317013	23.559655
113.014603	3178.992325	23.564672
113.317130	3168.149998	23.569690
113.381147	3179.504156	23.574707
113.710815	3192.449439	23.579725
113.907677	3205.207232	23.584743
113.935785	3214.650846	23.589760
114.383345	3209.338377	23.594778
114.098298	3208.028395	23.599795
114.087057	3197.864655	23.604813
114.174559	3199.727708	23.609831
114.380407	3202.052301	23.614848
114.556970	3192.748068	23.619866
114.495892	3204.002445	23.624883
114.997524	3195.994476	23.629901
114.499507	3202.360897	23.634919
114.846077	3198.610369	23.639936
114.690866	3210.898397	23.644954
114.880259	3214.610728	23.649971
115.012942	3219.609576	23.654989
114.906932	3223.850634	23.660007
115.033948	3231.072830	23.665024
115.744336	3238.638787	23.670042
115.458006	3258.678333	23.675059
115.775198	3239.942691	23.680077
115.497916	3258.363441	23.685095
115.918080	3253.520833	23.690112
116.104008	3256.439269	23.695130
116.231388	3281.248218	23.700147
116.701593	3284.590153	23.705165
116.513349	3270.243062	23.710183
116.750450	3271.356216	23.715200
117.120920	3277.856325	23.720218
116.809261	3273.268884	23.725235
117.476376	3273.227534	23.730253
117.126897	3276.303338	23.735271
116.762593	3270.660829	23.740288
116.970915	3256.196256	23.745306
117.019239	3265.875928	23.750323
117.254880	3270.475107	23.755341
117.082631	3298.711900	23.760359
117.000353	3294.039700	23.765376
117.365322	3307.920182	23.770394
117.432124	3326.194789	23.775411
117.438251	3328.533504	23.780429
117.474744	3338.638795	23.785447
117.905231	3344.890434	23.790464
118.239059	3343.273852	23.795482
118.485986	3350.504242	23.800499
118.895706	3338.588581	23.805517
118.863438	3341.826549	23.810535
118.952925	3351.823486	23.815552
119.010593	3356.573358	23.820570
119.079344	3373.168575	23.825587
119.578566	3366.922325	23.830605
119.697490	3380.047075	23.835623
119.354116	3380.547494	23.840640
119.676492	3366.695072	23.845658
119.628397	3380.232457	23.850675
119.679717	3369.781103	23.855693
119.726346	3374.074539	23.860711
119.948085	3395.289753	23.865728
120.168615	3397.335572	23.870746
119.926428	3411.575525	23.875763
120.228018	3402.808381	23.880781
120.530610	3409.068975	23.885799
120.626783	3421.346734	23.890816
120.811070	3430.259162	23.895834
121.002898	3427.111707	23.900851
120.984586	3430.523765	23.905869
121.009005	3415.966597	23.910887
121.351130	3431.061985	23.915904
121.762126	3446.497976	23.920922
121.436575	3451.807654	23.925939
121.746287	3443.467098	23.930957
121.718312	3449.427999	23.935975
121.553892	3452.430740	23.940992
121.880532	3449.943288	23.946010
122.180500	3451.275595	23.951027
122.104416	3463.943662	23.956045
122.688109	3470.053109	23.961063
122.834211	3469.685251	23.966080
123.290635	3464.343672	23.971098
123.175442	3458.308358	23.976115
123.641031	3451.810151	23.981133
123.187228	3451.287481	23.986151
123.250507	3461.220315	23.991168
123.350986	3457.111570	23.996186
123.463353	3453.127239	24.001203
123.533572	3452.545935	24.006221
123.874565	3441.045488	24.011239
123.866498	3439.753106	24.016256
124.106790	3440.185825	24.021274
123.853118	3446.041892	24.026291
123.675021	3439.536664	24.031309
124.074456	3457.540716	24.036327
124.000030	3467.376622	24.041344
124.501627	3464.238605	24.046362
124.640146	3482.044853	24.051379
124.447301	3478.472759	24.056397
124.654955	3483.489619	24.061415
124.788831	3496.876172	24.066432
124.878156	3501.077155	24.071450
125.053828	3509.686328	24.076467
124.852937	3501.121053	24.081485
125.334324	3504.423395	24.086503
125.218072	3522.582023	24.091520
125.476947	3523.180967	24.096538
125.533438	3526.853916	24.101555
125.321880	3530.630605	24.106573
125.243618	3538.960491	24.111591
125.522431	3559.307832	24.116608
125.538259	3561.906005	24.121626
125.923721	3590.270073	24.126643
126.486164	3593.275574	24.131661
126.365459	3597.815621	24.136679
126.420762	3616.652711	24.141696
126.814865	3625.564836	24.146714
126.897251	3626.279561	24.151731
127.014861	3622.947477	24.156749
127.616919	3617.803833	24.161767
127.574117	3626.181844	24.166784
128.112308	3628.074024	24.171802
128.124638	3643.926877	24.176819
128.140658	3641.460799	24.181837
128.725646	3635.775869	24.186855
128.200292	3618.584517	24.191872
128.632915	3628.324932	24.196890
128.325015	3628.190356	24.201907
128.418929	3624.805100	24.206925
128.908078	3619.864366	24.211943
128.604410	3627.636656	24.216960
128.903909	3623.333563	24.221978
129.084576	3630.427394	24.226995
128.997320	3627.243335	24.232013
128.934698	3639.557348	24.237031
128.927465	3651.320480	24.242048
129.288234	3648.058845	24.247066
129.044795	3663.538226	24.252083
129.328991	3673.831549	24.257101
129.344561	3689.231150	24.262119
129.523487	3700.553317	24.267136
129.775124	3713.720596	24.272154
129.927054	3718.216811	24.277171
130.201588	3714.194201	24.282189
130.459998	3718.373604	24.287207
130.603064	3747.119355	24.292224
130.970201	3730.395776	24.297242
131.072196	3737.679824	24.302259
131.142176	3741.921865	24.307277
131.155060	3734.023120	24.312295
130.956976	3749.195874	24.317312
131.364138	3757.431102	24.322330
131.621103	3763.165904	24.327347
131.279258	3764.175934	24.332365
131.619840	3751.095375	24.337383
132.122357	3774.919489	24.342400
132.083910	3787.835149	24.347418
132.101943	3777.863047	24.352435
132.629718	3786.331909	24.357453
132.688423	3776.471594	24.362471
133.021071	3788.462928	24.367488
133.211675	3774.142931	24.372506
133.088616	3771.103737	24.377523
133.048868	3774.534767	24.382541
133.137132	3768.894069	24.387559
133.059014	3787.500651	24.392576
133.304441	3802.130085	24.397594
133.242631	3816.712265	24.402611
133.400981	3808.939057	24.407629
133.607718	3810.909257	24.412647
133.623345	3811.584626	24.417664
134.053541	3823.752394	24.422682
134.004899	3826.020311	24.427699
134.393282	3829.306594	24.432717
134.463299	3826.809516	24.437735
134.407736	3827.153728	24.442752
134.593509	3832.885359	24.447770
134.832679	3848.087932	24.452787
134.950333	3860.290441	24.457805
135.210861	3865.090416	24.462823
134.834684	3872.283453	24.467840
134.894423	3869.449869	24.472858
135.180047	3886.824390	24.477875
134.827373	3889.592170	24.482893
135.271122	3886.322681	24.487911
135.574215	3917.643559	24.492928
135.654065	3930.163795	24.497946
136.102033	3924.005325	24.502963
135.991218	3939.642992	24.507981
136.027586	3945.489118	24.512999
136.182345	3946.980901	24.518016
136.263036	3959.817961	24.523034
136.545453	3974.098915	24.528051
136.820407	3972.638460	24.533069
137.051633	3981.107608	24.538087
137.384934	4001.352035	24.543104
137.564165	3998.544748	24.548122
138.110992	3991.856512	24.553139
137.833561	3990.719225	24.558157
138.137276	3985.782638	24.563175
138.484596	3992.745552	24.568192
138.311673	3990.785063	24.573210
138.478054	3983.899054	24.578227
138.615301	3992.832178	24.583245
138.418996	3991.295252	24.588263
138.483542	4007.274497	24.593280
138.843672	4016.469243	24.598298
139.208516	4012.793853	24.603315
138.924374	4017.366144	24.608333
139.540916	4010.391963	24.613351
139.607671	4015.070454	24.618368
139.575904	4011.816121	24.623386
139.845337	4024.457476	24.628403
139.968289	4027.683326	24.633421
140.112084	4041.336829	24.638439
139.848779	4050.614527	24.643456
140.318672	4022.072818	24.648474
141.455010	4016.127354	24.653491
141.038774	4013.663739	24.658509
141.530252	4009.705999	24.663527
141.276191	4004.656443	24.668544
141.392393	4021.611061	24.673562
141.588906	4011.719165	24.678579
141.180053	4020.027945	24.683597
141.620456	4002.121454	24.688615
141.438136	4004.847720	24.693632
141.491533	3997.942577	24.698650
141.216115	4016.658807	24.703667
141.282953	4034.259808	24.708685
141.507117	4031.798647	24.713703
141.545537	4053.630899	24.718720
141.632889	4071.973857	24.723738
141.921525	4079.393375	24.728755
142.216897	4095.382605	24.733773
142.636841	4097.660148	24.738791
142.614413	4098.394182	24.743808
142.592848	4100.367102	24.748826
143.115493	4106.158137	24.753843
143.186796	4116.676310	24.758861
143.205006	4122.031780	24.763879
143.615792	4123.867908	24.768896
143.649861	4128.108114	24.773914
143.812070	4138.052595	24.778931
143.724186	4149.491226	24.783949
143.780242	4150.015829	24.788967
144.093745	4144.267697	24.793984
143.947050	4152.523387	24.799002
144.498171	4161.320897	24.804019
144.499443	4160.834428	24.809037
144.656565	4161.939604	24.814055
144.965762	4169.082921	24.819072
144.790924	4196.109902	24.824090
145.198426	4187.652000	24.829107
145.336470	4188.703634	24.834125
145.549533	4187.795538	24.839143
145.774087	4198.436482	24.844160
145.986486	4210.626367	24.849178
146.242730	4199.986258	24.854195
146.183417	4219.371782	24.859213
146.320727	4210.399036	24.864231
146.604554	4212.704599	24.869248
146.457561	4224.272348	24.874266
146.943097	4231.569243	24.879283
146.995520	4239.827908	24.884301
146.904237	4243.047466	24.889319
147.286975	4232.654952	24.894336
147.315798	4238.479598	24.899354
147.753204	4254.736484	24.904371
147.587130	4266.254265	24.909389
147.817801	4264.130200	24.914407
148.121459	4270.764610	24.919424
148.032614	4272.199820	24.924442
148.215455	4275.396534	24.929459
148.489567	4278.741956	24.934477
148.553977	4295.889692	24.939495
148.603635	4300.380927	24.944512
148.779003	4298.669166	24.949530
148.851258	4294.383358	24.954547
148.911575	4310.413223	24.959565
149.524268	4317.919871	24.964583
149.557753	4322.092506	24.969600
149.582784	4337.801439	24.974618
149.816344	4328.440260	24.979635
149.384796	4324.957413	24.984653
149.626867	4334.844727	24.989671
149.908590	4348.621782	24.994688
150.008163	4358.003885	24.999706
150.503049	4367.380523	25.004723
150.307385	4362.940922	25.009741
151.178215	4373.657497	25.014759
151.056343	4369.436029	25.019776
151.274331	4378.898192	25.024794
151.218976	4375.416565	25.029811
151.253162	4383.620441	25.034829
151.490135	4394.552793	25.039847
151.640474	4390.350520	25.044864
151.391792	4393.993778	25.049882
151.882962	4404.870355	25.054899
151.874646	4418.910763	25.059917
152.218177	4428.477417	25.064935
152.458873	4427.086759	25.069952
152.374861	4425.014667	25.074970
152.467467	4441.772055	25.079987
152.578951	4452.521625	25.085005
152.860881	4447.216029	25.090023
152.863154	4453.170348	25.095040
153.151441	4465.603816	25.100058
153.481475	4480.983346	25.105075
153.183369	4490.128068	25.110093
153.279583	4488.051388	25.115111
153.932353	4507.425132	25.120128
153.510485	4515.674114	25.125146
153.735870	4510.751881	25.130163
153.873913	4520.409241	25.135181
154.462353	4539.231804	25.140199
154.756962	4529.041463	25.145216
154.548223	4534.856257	25.150234
154.937777	4529.122192	25.155251
155.037521	4537.931502	25.160269
155.019376	4547.450895	25.165287
155.376621	4543.886095	25.170304
155.364202	4546.956848	25.175322
155.800554	4563.570950	25.180339
156.188459	4568.932817	25.185357
155.888144	4574.096567	25.190375
156.279588	4573.777524	25.195392
156.175549	4574.356943	25.200410
156.682691	4596.383395	25.205427
156.513236	4607.917735	25.210445
156.448114	4599.499905	25.215463
157.062714	4607.661940	25.220480
157.166202	4618.757066	25.225498
157.574440	4627.689090	25.230515
157.245306	4625.908672	25.235533
157.546742	4637.209312	25.240551
157.868498	4640.639074	25.245568
157.826171	4650.196386	25.250586
158.105710	4650.436030	25.255603
158.185133	4658.211678	25.260621
158.337656	4651.663912	25.265639
158.509913	4675.051420	25.270656
158.418902	4678.804529	25.275674
159.028518	4677.661973	25.280691
159.019291	4683.534808	25.285709
158.818830	4693.347821	25.290727
159.274233	4707.847344	25.295744
159.415746	4701.751018	25.300762
159.506151	4718.667347	25.305779
159.945184	4736.010777	25.310797
159.912671	4740.882675	25.315815
160.164041	4729.383886	25.320832
160.535170	4727.079058	25.325850
161.492637	4723.418982	25.330867
161.696970	4708.079243	25.335885
161.514996	4726.160360	25.340903
161.662598	4712.752194	25.345920
161.470772	4717.752384	25.350938
161.737504	4700.806150	25.355955
161.655281	4700.152343	25.360973
161.888334	4708.135328	25.365991
162.204936	4705.700919	25.371008
161.872494	4727.379627	25.376026
162.102785	4736.683663	25.381043
162.850912	4746.580547	25.386061
162.278391	4746.577481	25.391079
162.317890	4738.141503	25.396096
162.623207	4750.579079	25.401114
162.798798	4761.283228	25.406131
162.898844	4768.051503	25.411149
162.768912	4778.892373	25.416167
162.943410	4786.798058	25.421184
162.936049	4800.983546	25.426202
162.887238	4798.402395	25.431219
163.126795	4815.311903	25.436237
163.472089	4832.428388	25.441255
163.927598	4845.194011	25.446272
163.602584	4866.433062	25.451290
163.999161	4857.729733	25.456307
164.179784	4884.046751	25.461325
164.376859	4884.482719	25.466343
164.804515	4892.348992	25.471360
164.634153	4917.340072	25.476378
164.730882	4925.952050	25.481395
165.644473	4932.790326	25.486413
165.569813	4941.364482	25.491431
166.123413	4930.284551	25.496448
165.855696	4940.137180	25.501466
165.853209	4933.251881	25.506483
165.971775	4960.659305	25.511501
166.339878	4984.285022	25.516519
166.404479	4979.829803	25.521536
166.401305	4996.584319	25.526554
166.951200	5010.220003	25.531571
166.990454	5007.249032	25.536589
166.592019	5016.864226	25.541607
167.356789	5023.220782	25.546624
167.613830	5030.519979	25.551642
167.722293	5038.543013	25.556659
168.081491	5045.111092	25.561677
168.474867	5064.508704	25.566695
168.628678	5054.432635	25.571712
168.501553	5058.468601	25.576730
168.925096	5051.893213	25.581747
169.156709	5047.434004	25.586765
168.592976	5081.825549	25.591783
169.359638	5073.871275	25.596800
169.294061	5082.366440	25.601818
169.275058	5090.636962	25.606835
169.506405	5101.221885	25.611853
169.873072	5107.620629	25.616871
169.848807	5113.996951	25.621888
170.139076	5124.430013	25.626906
170.130864	5137.040581	25.631923
170.647447	5135.916910	25.636941
170.793664	5142.443048	25.641959
170.974809	5146.656080	25.646976
171.231305	5165.930749	25.651994
171.139785	5164.715011	25.657011
171.909058	5151.230134	25.662029
171.920941	5155.993240	25.667047
172.256510	5143.311211	25.672064
172.390973	5146.004232	25.677082
172.269312	5130.615963	25.682100
172.498052	5145.157677	25.687117
172.451119	5167.099301	25.692135
172.870162	5174.361562	25.697152
172.836916	5171.427739	25.702170
173.442952	5169.423050	25.707188
173.241047	5177.580122	25.712205
173.626185	5177.647982	25.717223
173.606563	5183.355381	25.722240
173.506101	5194.731099	25.727258
173.847967	5212.938848	25.732276
173.831024	5211.403662	25.737293
173.755116	5212.631285	25.742311
173.871398	5229.185978	25.747328
173.973793	5227.949613	25.752346
173.870728	5251.863451	25.757364
174.211910	5251.055402	25.762381
174.817363	5272.859852	25.767399
174.979381	5288.871949	25.772416
174.775670	5295.623704	25.777434
175.191413	5303.755964	25.782452
175.897558	5314.012160	25.787469
175.774962	5327.091833	25.792487
176.293842	5325.380693	25.797504
176.041045	5322.151975	25.802522
176.156345	5321.736798	25.807540
176.796661	5341.021503	25.812557
176.746829	5339.025541	25.817575
177.049513	5341.171054	25.822592
176.904629	5345.048986	25.827610
176.960655	5352.318941	25.832628
177.585229	5351.534938	25.837645
177.644320	5368.485495	25.842663
177.993247	5350.861118	25.847680
178.213151	5353.656608	25.852698
177.998932	5369.956963	25.857716
178.537422	5383.425548	25.862733
178.199561	5383.662874	25.867751
178.410996	5389.424309	25.872768
178.842032	5404.638046	25.877786
178.849776	5424.904253	25.882804
179.012327	5411.467033	25.887821
178.942459	5424.548707	25.892839
179.194316	5443.231890	25.897856
179.528674	5446.413656	25.902874
179.562564	5470.990721	25.907892
180.305382	5473.775434	25.912909
180.420969	5475.474652	25.917927
180.257383	5474.897649	25.922944
180.463247	5485.920958	25.927962
181.194948	5501.098499	25.932980
181.269349	5491.990513	25.937997
181.433502	5499.366704	25.943015
181.547321	5505.655795	25.948032
181.830852	5518.053878	25.953050
182.011626	5512.981202	25.958068
182.223696	5510.147353	25.963085
182.488422	5504.564681	25.968103
182.452254	5523.244755	25.973120
182.617791	5519.930732	25.978138
182.531399	5541.175763	25.983156
182.849831	5539.531583	25.988173
182.770398	5545.775051	25.993191
182.961221	5561.129825	25.998208
183.048555	5571.262025	26.003226
183.050443	5585.121061	26.008244
183.120295	5602.960766	26.013261
184.009568	5611.466586	26.018279
183.599050	5620.229694	26.023296
184.221120	5637.602556	26.028314
184.069693	5646.926892	26.033332
184.511201	5668.899555	26.038349
184.651680	5675.225654	26.043367
184.775248	5680.753649	26.048384
184.880611	5682.352202	26.053402
184.849844	5712.902203	26.058420
185.395651	5711.499218	26.063437
185.710861	5723.021238	26.068455
185.884025	5723.436769	26.073472
186.493911	5719.810277	26.078490
186.576939	5739.652188	26.083508
187.172874	5744.753682	26.088525
186.990507	5743.337129	26.093543
186.887023	5755.778082	26.098560
187.370025	5740.040847	26.103578
187.187042	5748.151774	26.108596
187.378376	5743.639961	26.113613
187.513695	5766.064197	26.118631
187.321386	5778.756099	26.123648
187.480479	5781.075815	26.128666
187.888876	5788.928400	26.133684
187.863236	5798.976642	26.138701
187.790314	5804.584003	26.143719
187.975434	5819.675365	26.148736
188.502446	5835.305620	26.153754
188.351710	5860.450101	26.158772
188.908453	5867.961632	26.163789
189.349827	5870.740312	26.168807
189.265759	5899.283029	26.173824
189.729703	5894.286692	26.178842
190.064832	5912.249086	26.183860
190.010911	5915.487621	26.188877
190.502143	5908.940858	26.193895
190.661043	5911.238575	26.198912
191.216253	5915.991681	26.203930
191.596703	5927.684203	26.208948
191.784087	5923.435238	26.213965
191.782127	5931.347820	26.218983
191.645650	5918.966818	26.224000
191.870204	5925.567756	26.229018
191.900882	5929.870439	26.234036
192.186323	5944.176720	26.239053
192.370167	5952.931982	26.244071
192.237596	5955.323539	26.249088
192.392224	5972.692892	26.254106
192.567816	5990.450202	26.259124
192.335782	5993.286615	26.264141
193.185481	6001.027805	26.269159
193.413140	6017.253460	26.274176
194.097611	6031.182031	26.279194
194.002159	6037.815412	26.284212
194.135388	6030.626847	26.289229
194.469783	6035.070748	26.294247
194.496905	6058.768604	26.299264
195.130957	6058.687454	26.304282
194.895916	6077.854665	26.309300
195.038688	6064.802895	26.314317
195.347361	6079.253519	26.319335
195.474717	6097.519791	26.324352
195.468615	6089.105190	26.329370
195.909643	6106.441547	26.334388
195.926629	6121.938997	26.339405
196.009560	6133.978520	26.344423
196.553977	6126.462086	26.349440
196.529249	6140.539432	26.354458
196.641299	6158.119997	26.359476
196.662052	6166.001381	26.364493
197.428544	6179.830691	26.369511
197.179389	6191.726666	26.374528
197.561442	6200.057910	26.379546
197.507331	6211.219976	26.384564
197.772093	6217.718314	26.389581
198.275479	6219.850479	26.394599
198.229223	6217.519897	26.399616
198.530043	6240.377390	26.404634
198.694223	6240.099809	26.409652
198.847917	6249.024026	26.414669
198.952590	6269.826983	26.419687
198.935758	6276.079692	26.424704
199.428587	6286.572601	26.429722
199.548189	6302.584867	26.434740
199.768444	6295.023470	26.439757
200.087395	6316.837732	26.444775
200.083924	6325.129571	26.449792
200.396758	6333.609356	26.454810
200.414810	6343.354610	26.459828
200.886386	6344.670638	26.464845
201.335354	6346.496793	26.469863
201.086374	6359.393050	26.474880
201.516868	6365.015878	26.479898
201.824666	6378.584081	26.484916
201.899534	6369.417231	26.489933
202.346407	6376.651831	26.494951
202.125839	6403.162514	26.499968
202.669631	6401.718065	26.504986
202.789271	6411.626138	26.510004
202.744730	6418.155975	26.515021
203.261369	6420.926258	26.520039
203.391448	6435.393329	26.525056
203.390450	6435.482471	26.530074
203.426343	6450.031271	26.535092
203.666369	6468.554215	26.540109
203.953358	6478.637870	26.545127
203.960155	6496.522873	26.550144
204.395760	6491.866531	26.555162
204.350305	6519.519570	26.560180
204.817468	6516.077143	26.565197
205.308248	6532.886753	26.570215
205.541080	6554.990432	26.575232
205.913394	6560.596954	26.580250
205.585320	6565.657648	26.585268
205.602579	6583.610327	26.590285
206.004703	6580.344020	26.595303
206.033213	6592.073136	26.600320
206.307054	6611.895648	26.605338
206.707330	6626.395433	26.610356
206.762924	6640.385924	26.615373
207.297526	6636.332995	26.620391
207.296776	6652.282020	26.625408
207.544331	6665.454830	26.630426
207.908118	6668.070848	26.635444
208.265535	6675.880324	26.640461
208.675639	6682.818717	26.645479
208.993512	6688.783171	26.650496
209.494987	6687.815079	26.655514
209.605035	6677.564062	26.660532
209.900036	6680.935695	26.665549
210.308237	6675.800263	26.670567
210.184923	6671.784358	26.675584
210.024938	6673.984449	26.680602
210.239573	6678.143535	26.685620
210.056994	6698.338478	26.690637
210.154936	6695.605181	26.695655
210.300764	6707.551270	26.700672
210.556301	6723.599786	26.705690
210.474683	6737.275955	26.710708
210.586440	6751.496685	26.715725
211.260417	6754.374132	26.720743
211.421871	6773.209694	26.725760
212.288182	6780.446851	26.730778
212.626797	6785.558916	26.735796
212.865669	6784.202618	26.740813
213.053268	6781.891594	26.745831
213.073798	6807.306992	26.750848
213.086136	6796.103331	26.755866
213.203749	6798.271751	26.760884
213.263533	6797.320711	26.765901
213.528862	6810.322167	26.770919
213.428336	6840.226293	26.775936
213.711496	6837.035507	26.780954
214.133164	6863.404624	26.785972
213.752853	6876.589989	26.790989
214.081561	6872.519826	26.796007
214.285936	6894.462507	26.801024
214.420988	6901.728393	26.806042
214.913463	6912.829002	26.811060
214.744589	6932.310800	26.816077
215.502700	6960.561144	26.821095
215.526464	6967.385502	26.826112
215.668649	6986.133142	26.831130
216.604191	6989.437604	26.836148
216.722345	6995.884093	26.841165
217.032951	6986.138445	26.846183
217.282651	7007.545329	26.851200
217.378131	7006.638784	26.856218
217.313973	7017.415592	26.861236
217.739227	7010.348450	26.866253
217.833324	7023.954882	26.871271
217.856511	7036.747655	26.876288
218.190842	7054.417723	26.881306
218.385798	7059.118867	26.886324
218.256258	7076.625387	26.891341
218.470678	7076.988462	26.896359
218.518700	7108.827274	26.901376
218.622177	7120.319936	26.906394
219.144657	7129.916966	26.911412
219.200287	7150.865442	26.916429
219.290712	7166.215534	26.921447
219.786156	7178.253070	26.926464
220.083786	7190.405996	26.931482
220.110772	7221.643643	26.936500
220.454538	7219.930526	26.941517
220.900914	7240.731079	26.946535
221.384124	7253.482677	26.951552
221.578227	7274.446244	26.956570
222.127038	7268.997557	26.961588
222.371348	7282.028078	26.966605
222.329865	7274.364540	26.971623
222.556614	7287.257775	26.976640
223.216328	7309.592059	26.981658
223.685978	7312.652228	26.986676
223.397410	7317.979929	26.991693
223.555041	7307.603290	26.996711
223.345355	7324.592487	27.001728
223.369031	7342.377999	27.006746
223.813155	7345.906286	27.011764
223.814831	7368.370638	27.016781
224.202636	7374.768793	27.021799
224.238022	7399.009955	27.026816
224.487987	7421.626323	27.031834
224.843917	7430.153139	27.036852
225.149755	7451.217408	27.041869
225.331082	7472.122702	27.046887
225.588778	7474.749298	27.051904
225.806696	7490.841041	27.056922
226.218735	7506.378546	27.061940
226.602166	7534.376784	27.066957
226.862921	7533.644530	27.071975
227.084137	7538.373772	27.076992
226.662455	7542.875288	27.082010
227.352393	7552.874944	27.087028
227.356561	7573.155141	27.092045
227.281085	7580.378150	27.097063
228.136339	7594.945430	27.102080
228.012886	7610.223387	27.107098
228.282035	7629.573027	27.112116
228.506907	7641.184631	27.117133
228.995273	7645.841413	27.122151
229.190017	7657.569060	27.127168
229.553454	7677.663227	27.132186
229.412593	7680.788893	27.137204
230.211745	7669.570397	27.142221
230.543882	7665.768043	27.147239
230.886548	7667.029089	27.152256
230.679253	7692.481976	27.157274
231.013893	7698.898500	27.162292
231.263386	7701.868314	27.167309
230.894867	7712.411551	27.172327
231.491805	7714.646614	27.177344
231.798880	7727.806542	27.182362
232.001368	7724.623395	27.187380
231.952919	7752.028625	27.192397
232.085219	7756.482780	27.197415
232.374233	7772.172406	27.202432
232.581394	7801.711680	27.207450
232.990068	7803.904613	27.212468
233.140394	7827.536727	27.217485
233.257117	7831.393309	27.222503
233.304716	7841.911201	27.227520
233.358379	7862.664828	27.232538
233.997147	7886.871634	27.237556
234.064176	7897.245368	27.242573
234.438109	7902.728449	27.247591
234.685565	7910.065231	27.252608
234.868230	7938.195808	27.257626
235.413472	7948.410229	27.262644
235.809431	7954.914392	27.267661
235.769911	7980.252595	27.272679
235.929725	7989.513894	27.277696
235.947016	8007.743068	27.282714
236.437605	8008.110948	27.287732
236.741328	8037.508688	27.292749
236.623672	8034.123967	27.297767
237.545725	8064.736519	27.302784
237.227274	8078.365548	27.307802
237.608000	8089.488604	27.312820
237.885343	8097.721589	27.317837
238.022390	8111.547912	27.322855
238.208475	8132.273713	27.327872
238.104234	8146.454198	27.332890
238.890209	8151.124973	27.337908
238.829816	8173.698389	27.342925
239.099159	8202.972944	27.347943
239.492894	8210.630685	27.352960
239.640289	8223.746520	27.357978
240.333533	8236.146009	27.362996
240.689104	8247.180390	27.368013
240.858943	8256.225163	27.373031
241.259050	8254.553828	27.378048
241.209634	8284.696407	27.383066
241.811051	8287.208854	27.388084
241.836700	8287.682700	27.393101
242.231464	8302.388942	27.398119
242.323745	8303.485046	27.403136
242.052654	8304.573447	27.408154
242.389371	8330.169832	27.413172
242.477402	8335.794030	27.418189
242.674780	8368.713406	27.423207
242.935974	8380.730705	27.428224
243.204199	8404.703368	27.433242
243.324687	8419.744889	27.438260
243.786858	8439.320404	27.443277
243.705650	8444.072316	27.448295
244.261020	8463.189015	27.453312
244.185149	8483.417437	27.458330
244.469368	8500.994221	27.463348
244.701522	8522.624237	27.468365
245.015452	8541.039736	27.473383
245.177200	8549.612631	27.478400
245.681919	8580.200614	27.483418
246.343265	8585.560046	27.488436
246.212121	8601.962641	27.493453
246.694421	8599.650715	27.498471
247.258670	8611.700037	27.503488
247.036156	8621.013057	27.508506
247.468149	8623.277870	27.513524
247.622980	8640.424068	27.518541
247.467887	8663.498238	27.523559
247.906906	8677.409067	27.528576
247.927845	8699.987910	27.533594
248.451198	8705.221314	27.538612
249.037292	8707.745027	27.543629
249.010381	8718.753135	27.548647
249.661982	8736.032397	27.553664
249.651532	8749.168444	27.558682
249.970089	8768.867340	27.563700
250.124325	8778.003207	27.568717
250.361209	8786.110120	27.573735
250.839575	8801.878183	27.578752
250.537495	8809.454256	27.583770
250.830884	8821.115270	27.588788
251.155854	8832.056657	27.593805
251.254295	8860.767545	27.598823
251.693924	8876.956398	27.603840
251.860658	8893.589704	27.608858
251.949719	8905.305804	27.613876
252.776079	8920.541524	27.618893
252.622197	8932.219014	27.623911
253.466188	8953.865111	27.628928
253.438537	8951.663380	27.633946
254.104114	8954.799417	27.638964
254.645027	8966.577967	27.643981
255.044723	8977.045530	27.648999
255.113823	8972.830261	27.654016
255.163004	8983.510123	27.659034
255.737332	8994.026826	27.664052
255.707722	9000.523752	27.669069
255.844471	9009.413735	27.674087
255.906102	9008.235407	27.679104
256.096089	9030.725352	27.684122
256.347827	9040.224924	27.689140
256.522464	9051.898638	27.694157
256.245017	9080.414453	27.699175
256.699704	9080.813502	27.704192
256.753422	9102.135872	27.709210
257.330633	9124.533618	27.714228
257.327668	9131.104176	27.719245
257.990803	9158.983459	27.724263
258.394903	9165.656919	27.729280
258.316672	9191.683223	27.734298
258.621320	9206.369748	27.739316
259.101042	9223.625164	27.744333
259.096831	9234.314015	27.749351
259.532183	9257.970486	27.754368
259.688957	9269.006918	27.759386
259.559923	9293.345091	27.764404
260.250550	9305.061349	27.769421
260.106903	9328.291341	27.774439
260.211003	9338.566157	27.779456
260.622823	9359.984098	27.784474
260.797688	9388.835338	27.789492
261.121635	9397.855301	27.794509
261.545118	9436.318804	27.799527
261.889968	9447.746495	27.804544
262.221985	9449.319016	27.809562
262.728491	9466.137035	27.814580
262.984604	9481.762110	27.819597
263.179803	9486.814468	27.824615
263.613146	9489.327312	27.829632
263.741331	9510.248012	27.834650
264.034214	9506.150808	27.839668
264.448189	9527.185007	27.844685
264.316212	9550.245612	27.849703
264.403981	9558.834426	27.854720
265.043584	9569.545533	27.859738
264.980839	9587.391161	27.864756
265.381390	9595.965342	27.869773
265.422282	9617.617419	27.874791
265.724521	9630.878980	27.879808
265.970618	9656.591727	27.884826
265.999100	9679.849720	27.889844
266.994301	9686.198883	27.894861
267.141066	9723.877761	27.899879
267.328423	9736.679459	27.904896
267.936335	9752.747666	27.909914
267.737534	9760.486724	27.914932
268.158490	9774.462944	27.919949
268.341407	9792.401339	27.924967
269.211334	9802.902829	27.929984
269.324874	9802.387004	27.935002
269.481726	9821.282878	27.940020
270.200838	9815.383770	27.945037
270.473105	9826.616555	27.950055
270.588473	9850.722997	27.955072
270.496341	9861.814352	27.960090
270.615578	9869.229944	27.965108
271.090511	9877.233494	27.970125
270.989134	9892.460366	27.975143
271.699240	9906.904890	27.980160
271.671971	9922.273154	27.985178
271.447839	9949.912851	27.990196
271.675166	9955.988033	27.995213
272.016477	9993.194278	28.000231
272.459185	10017.543864	28.005248
272.894150	10026.873540	28.010266
274.032749	10027.180898	28.015284
274.672732	10015.397846	28.020301
274.837121	10020.972215	28.025319
275.005156	10026.117459	28.030336
275.008664	10035.620826	28.035354
275.347429	10054.719303	28.040372
275.624835	10052.764783	28.045389
275.557753	10066.347675	28.050407
275.949159	10076.715718	28.055424
275.892441	10086.380309	28.060442
276.040150	10108.310017	28.065460
276.260929	10115.715250	28.070477
276.365356	10151.945612	28.075495
276.638283	10169.521381	28.080512
277.025044	10188.522287	28.085530
276.805080	10218.754992	28.090548
277.390297	10221.808462	28.095565
277.766414	10239.740650	28.100583
278.082214	10257.652888	28.105600
278.734707	10286.818351	28.110618
278.940144	10309.193325	28.115636
279.213634	10316.685260	28.120653
279.253419	10340.977443	28.125671
279.592900	10352.954156	28.130688
279.823204	10363.772021	28.135706
279.972192	10386.954416	28.140724
280.697969	10407.338002	28.145741
280.553405	10427.154851	28.150759
280.775360	10449.987339	28.155776
281.324947	10457.678716	28.160794
281.500302	10473.084143	28.165812
281.796679	10476.799829	28.170829
281.821435	10485.006464	28.175847
282.668747	10503.128938	28.180864
283.041489	10516.320508	28.185882
283.077481	10539.034960	28.190900
283.640572	10535.514394	28.195917
283.854638	10559.158153	28.200935
283.897215	10568.074806	28.205952
284.126795	10586.049710	28.210970
284.482637	10594.911473	28.215988
284.783640	10606.280281	28.221005
284.632599	10621.572770	28.226023
284.997048	10642.240074	28.231040
285.778786	10649.215718	28.236058
285.829426	10678.723172	28.241076
285.902899	10692.429109	28.246093
286.398879	10712.885712	28.251111
286.371694	10727.487452	28.256128
287.020769	10750.736644	28.261146
287.090499	10772.661239	28.266164
287.744872	10794.894189	28.271181
287.495520	10806.566761	28.276199
287.799715	10822.026077	28.281216
288.488801	10851.232217	28.286234
288.630312	10873.015896	28.291252
288.652912	10892.771829	28.296269
288.934691	10915.760530	28.301287
289.431297	10930.824212	28.306304
289.641011	10952.793675	28.311322
289.932585	10979.737059	28.316340
290.078533	10993.845650	28.321357
290.571007	11014.856239	28.326375
290.604982	11031.712227	28.331392
291.280261	11045.864187	28.336410
291.724288	11074.030385	28.341428
291.950565	11088.110821	28.346445
292.212915	11112.832984	28.351463
292.514333	11129.327415	28.356480
292.862367	11145.907120	28.361498
292.818976	11163.083264	28.366516
293.258636	11183.222843	28.371533
293.649062	11206.288546	28.376551
293.764184	11227.928962	28.381568
294.308257	11250.730646	28.386586
294.315521	11262.508469	28.391604
294.541532	11291.330271	28.396621
294.680109	11318.205751	28.401639
295.110031	11340.366250	28.406656
295.740916	11360.012812	28.411674
296.088293	11391.932050	28.416692
296.747904	11383.032039	28.421709
297.016965	11403.014158	28.426727
297.443761	11417.177562	28.431744
298.230436	11427.596203	28.436762
298.468778	11427.868779	28.441780
298.694206	11419.677806	28.446797
299.249253	11428.425192	28.451815
299.478498	11432.609116	28.456832
299.678895	11417.110720	28.461850
299.570888	11434.393941	28.466868
300.297298	11446.944881	28.471885
300.004963	11456.183633	28.476903
299.676597	11457.579488	28.481920
300.006648	11486.458506	28.486938
300.198133	11511.222139	28.491956
300.391322	11520.026993	28.496973
300.848962	11550.225100	28.501991
300.721064	11573.116986	28.507008
301.079810	11591.014169	28.512026
301.267833	11621.343611	28.517044
301.738003	11637.657852	28.522061
301.908135	11663.561268	28.527079
302.308197	11704.871003	28.532096
302.617217	11722.300709	28.537114
302.791432	11744.567037	28.542132
303.013143	11763.359162	28.547149
303.641203	11793.067124	28.552167
303.980060	11821.676643	28.557184
304.267396	11826.412789	28.562202
304.604665	11865.076786	28.567220
305.306715	11886.539193	28.572237
305.631249	11902.133272	28.577255
305.838165	11932.197834	28.582272
306.333280	11933.036200	28.587290
306.729388	11949.455169	28.592308
307.134721	11969.100350	28.597325
307.411463	11977.790810	28.602343
307.507363	11996.077723	28.607360
307.905403	12009.572811	28.612378
308.047676	12029.594776	28.617396
308.601795	12049.992275	28.622413
308.678390	12080.009313	28.627431
308.576756	12098.141473	28.632448
309.411988	12102.607560	28.637466
309.522308	12126.444090	28.642484
309.390272	12147.315108	28.647501
310.075803	12172.174614	28.652519
310.040281	12188.892032	28.657536
310.255731	12219.734890	28.662554
310.745199	12248.581062	28.667572
310.788765	12286.594204	28.672589
311.401737	12303.530772	28.677607
311.739245	12341.857103	28.682624
312.219443	12358.952749	28.687642
312.433895	12391.311913	28.692660
312.127496	12418.004328	28.697677
312.790282	12439.434568	28.702695
312.951104	12466.401256	28.707712
313.546247	12493.797311	28.712730
313.795558	12519.536179	28.717748
314.844099	12551.600299	28.722765
315.224173	12562.080553	28.727783
315.490400	12599.785838	28.732800
316.067129	12590.426937	28.737818
316.011940	12622.285913	28.742836
316.262344	12643.188933	28.747853
317.091238	12636.928749	28.752871
317.084740	12661.279355	28.757888
317.473134	12668.082154	28.762906
317.938175	12688.417181	28.767924
317.935810	12707.460148	28.772941
318.429461	12721.085792	28.777959
318.299892	12736.615460	28.782976
318.783337	12760.291227	28.787994
319.432214	12773.208982	28.793012
319.545637	12803.188978	28.798029
319.809352	12815.083143	28.803047
320.202497	12838.909455	28.808064
320.073559	12855.392452	28.813082
320.624166	12869.705290	28.818100
320.729125	12888.298987	28.823117
321.550621	12916.857506	28.828135
321.360072	12932.386405	28.833152
321.490526	12956.317743	28.838170
321.848665	12973.932143	28.843188
322.088932	13004.474584	28.848205
322.557215	13025.652528	28.853223
322.818252	13049.578188	28.858240
323.432158	13073.451892	28.863258
323.385613	13099.221651	28.868276
323.626391	13112.107825	28.873293
324.001891	13141.975820	28.878311
324.476010	13160.691633	28.883328
325.172806	13170.494381	28.888346
325.385206	13192.929733	28.893364
325.556844	13214.043475	28.898381
326.095652	13231.926132	28.903399
326.279260	13260.073786	28.908416
326.742188	13271.543008	28.913434
327.278505	13295.754469	28.918452
327.670444	13306.781619	28.923469
328.577572	13316.204614	28.928487
328.398166	13325.353286	28.933504
328.750836	13347.453675	28.938522
328.892478	13355.399004	28.943540
329.419590	13387.514689	28.948557
329.554263	13405.700670	28.953575
329.963382	13429.893951	28.958592
330.151951	13439.063838	28.963610
330.439127	13457.494144	28.968628
330.668403	13479.541036	28.973645
330.996758	13490.061955	28.978663
331.269228	13521.537652	28.983680
331.610145	13540.747076	28.988698
331.899996	13558.315091	28.993716
332.315997	13590.887609	28.998733
333.302705	13589.378848	29.003751
333.615560	13608.099760	29.008768
333.809336	13615.121058	29.013786
334.497544	13627.799784	29.018804
334.816493	13635.698626	29.023821
335.357375	13648.893361	29.028839
335.550248	13670.667608	29.033856
335.554188	13675.380207	29.038874
335.949945	13691.167533	29.043892
335.717433	13711.626965	29.048909
336.256128	13722.403238	29.053927
336.507242	13743.236651	29.058944
336.421404	13771.187030	29.063962
337.047346	13787.100308	29.068980
337.127755	13817.736877	29.073997
337.640714	13840.432337	29.079015
337.652954	13880.363517	29.084032
337.639547	13907.536307	29.089050
338.451946	13940.133865	29.094068
338.473311	13962.415893	29.099085
338.885290	13994.099534	29.104103
339.076029	14031.221801	29.109120
339.407441	14055.619533	29.114138
339.408959	14085.031017	29.119156
339.809496	14132.144456	29.124173
340.504039	14167.127307	29.129191
340.496132	14196.800568	29.134208
341.006809	14235.079137	29.139226
341.754220	14260.703819	29.144244
342.002282	14286.494555	29.149261
342.501625	14317.419005	29.154279
343.148463	14338.670028	29.159296
343.262941	14365.806698	29.164314
344.154197	14387.304218	29.169332
344.169384	14412.894090	29.174349
344.571955	14428.266550	29.179367
345.041210	14456.996295	29.184384
344.991708	14473.220394	29.189402
345.605686	14499.346568	29.194420
345.789622	14513.013861	29.199437
346.439105	14523.906320	29.204455
346.865568	14537.820382	29.209472
347.048210	14551.856682	29.214490
347.280521	14571.892131	29.219508
347.351961	14596.691352	29.224525
348.212524	14617.568614	29.229543
348.188958	14647.070356	29.234560
348.373967	14667.082218	29.239578
348.508426	14695.815688	29.244596
348.510248	14726.043027	29.249613
348.674551	14752.893173	29.254631
349.412731	14791.285182	29.259648
349.715099	14830.724775	29.264666
350.170401	14865.641491	29.269684
350.163647	14905.359265	29.274701
350.870203	14928.903638	29.279719
351.214542	14964.341620	29.284736
351.384714	14989.634157	29.289754
352.184414	15017.681502	29.294772
352.361207	15051.424842	29.299789
352.924527	15081.378847	29.304807
353.610433	15109.780827	29.309824
353.731973	15128.779370	29.314842
354.588469	15151.092113	29.319860
354.409410	15185.164004	29.324877
355.239851	15209.039758	29.329895
355.436704	15229.920286	29.334912
355.811607	15257.942087	29.339930
356.258302	15272.149719	29.344948
356.789794	15286.935921	29.349965
357.143605	15297.209533	29.354983
357.726011	15321.534604	29.360000
357.614683	15342.522922	29.365018
358.020818	15369.118223	29.370036
358.384616	15391.350363	29.375053
358.403148	15415.700957	29.380071
358.834672	15443.026593	29.385088
358.907056	15470.547139	29.390106
359.427287	15494.443038	29.395124
359.615173	15538.798287	29.400141
360.079489	15563.288218	29.405159
360.123317	15593.606358	29.410176
360.728387	15633.957672	29.415194
361.103077	15660.728851	29.420212
361.443232	15692.025779	29.425229
361.965551	15730.616413	29.430247
362.802341	15748.755217	29.435264
362.443044	15772.924476	29.440282
363.563227	15785.517776	29.445300
363.801739	15823.920688	29.450317
364.276198	15847.083933	29.455335
364.636394	15867.465485	29.460352
364.573916	15896.012955	29.465370
365.119111	15915.574414	29.470388
365.203790	15933.074870	29.475405
365.723202	15966.528670	29.480423
366.265932	15986.962171	29.485440
366.611240	16019.711983	29.490458
367.046300	16046.495886	29.495476
366.897922	16070.711118	29.500493
367.468647	16094.304832	29.505511
367.875130	16121.687750	29.510528
367.965244	16149.759702	29.515546
368.289949	16170.390207	29.520564
368.906124	16202.887600	29.525581
369.346081	16227.997215	29.530599
369.902974	16246.748619	29.535616
370.100005	16269.621015	29.540634
370.838813	16292.235305	29.545652
371.247660	16314.456530	29.550669
371.408225	16339.360299	29.555687
372.143051	16339.973344	29.560704
371.993590	16365.823577	29.565722
372.621208	16390.565161	29.570740
372.537857	16410.580936	29.575757
372.805640	16433.974589	29.580775
373.723318	16447.558541	29.585792
373.878639	16484.875062	29.590810
374.508242	16499.926701	29.595828
374.567438	16528.639573	29.600845
375.134645	16544.858413	29.605863
375.827572	16548.427259	29.610880
376.134444	16588.455079	29.615898
376.690655	16578.637086	29.620916
377.217159	16614.469369	29.625933
377.392674	16629.797882	29.630951
378.201238	16646.527012	29.635968
378.049049	16667.260565	29.640986
378.554924	16684.638656	29.646004
378.704103	16706.409988	29.651021
378.937172	16731.423735	29.656039
379.274831	16749.991277	29.661056
379.603212	16775.605607	29.666074
379.792004	16801.417985	29.671092
380.578460	16830.945885	29.676109
380.601712	16860.900953	29.681127
381.208380	16888.114960	29.686144
380.890868	16929.227103	29.691162
381.539102	16954.019722	29.696180
381.702907	16974.669939	29.701197
382.197133	17011.945856	29.706215
382.332964	17054.903160	29.711232
382.698573	17094.556843	29.716250
383.743529	17123.500373	29.721268
384.307675	17149.505052	29.726285
385.148647	17171.684426	29.731303
385.546040	17188.368551	29.736320
386.251182	17198.995125	29.741338
386.705020	17207.609487	29.746356
387.009547	17222.220580	29.751373
387.585997	17237.568541	29.756391
387.890163	17255.915222	29.761408
387.927771	17278.143914	29.766426
388.771145	17283.644092	29.771444
388.830775	17298.005694	29.776461
388.717657	17324.226555	29.781479
389.268969	17337.195597	29.786496
389.542749	17368.438914	29.791514
390.015332	17377.351318	29.796532
390.461559	17405.800036	29.801549
390.687920	17430.806498	29.806567
390.767762	17452.472058	29.811584
390.838743	17483.419672	29.816602
391.619428	17502.652535	29.821620
391.930967	17527.050851	29.826637
391.642107	17562.969456	29.831655
392.501013	17596.919016	29.836672
392.606848	17623.507688	29.841690
393.070139	17663.085133	29.846708
393.351520	17700.353638	29.851725
393.551585	17739.073159	29.856743
394.104762	17770.914177	29.861760
394.138312	17805.032031	29.866778
394.396010	17834.201438	29.871796
395.156068	17865.270794	29.876813
396.053137	17889.873980	29.881831
396.778398	17907.379478	29.886848
397.214077	17934.309796	29.891866
397.897549	17956.811005	29.896884
398.217698	17974.238482	29.901901
398.277582	18005.114823	29.906919
398.933695	18019.351723	29.911936
398.838748	18046.719803	29.916954
399.349276	18075.635079	29.921972
399.636428	18100.351943	29.926989
399.633692	18129.527063	29.932007
400.299309	18161.566207	29.937024
400.473300	18189.763338	29.942042
400.870642	18234.315084	29.947060
401.036505	18277.059389	29.952077
401.671306	18310.216751	29.957095
402.030443	18336.797830	29.962112
402.436021	18376.845213	29.967130
402.923438	18425.813485	29.972148
403.794981	18440.391892	29.977165
403.673250	18490.168726	29.982183
404.532563	18519.139080	29.987200
404.684097	18542.162436	29.992218
404.741906	18587.343411	29.997236
405.331636	18620.918676	30.002253
405.804800	18663.127717	30.007271
406.334947	18703.153735	30.012288
406.644685	18736.064575	30.017306
407.063963	18775.454918	30.022324
407.679283	18794.815918	30.027341
407.507493	18836.283885	30.032359
408.552752	18872.347496	30.037376
408.370077	18915.644408	30.042394
408.555662	18955.297618	30.047412
409.366815	18997.030798	30.052429
409.625803	19035.442540	30.057447
410.000087	19072.252685	30.062464
410.585985	19129.515627	30.067482
411.096167	19167.939775	30.072500
411.883124	19185.151123	30.077517
412.441634	19235.470429	30.082535
412.880512	19250.924965	30.087552
413.495029	19282.375709	30.092570
413.911451	19311.776868	30.097588
414.389029	19340.644626	30.102605
415.003860	19370.672033	30.107623
415.604244	19394.219869	30.112640
415.798726	19415.944725	30.117658
415.804646	19447.627153	30.122676
416.412177	19477.566107	30.127693
416.384324	19505.272307	30.132711
417.001026	19538.214427	30.137728
417.399018	19574.514175	30.142746
417.352667	19610.165418	30.147764
417.947148	19640.439439	30.152781
418.112794	19680.994638	30.157799
418.678770	19711.109551	30.162816
418.996786	19755.743118	30.167834
419.286436	19792.989739	30.172852
420.125177	19816.281257	30.177869
420.388776	19860.804288	30.182887
420.755927	19897.305310	30.187904
421.328141	19926.270378	30.192922
421.748852	19957.175870	30.197940
422.266545	19987.464784	30.202957
422.546062	20017.758414	30.207975
422.895595	20052.588525	30.212992
423.344347	20084.050829	30.218010
423.576739	20114.976687	30.223028
423.894931	20146.608860	30.228045
424.367249	20194.651591	30.233063
424.409121	20221.913943	30.238080
425.159302	20270.399691	30.243098
425.336674	20305.315520	30.248116
425.759659	20337.892381	30.253133
426.472828	20383.170181	30.258151
427.008038	20417.227871	30.263168
427.567763	20455.588482	30.268186
428.048217	20492.913923	30.273204
428.291765	20522.251189	30.278221
428.901777	20564.445604	30.283239
429.173876	20594.839250	30.288256
429.646750	20631.225096	30.293274
430.202075	20682.961829	30.298292
431.218831	20697.084714	30.303309
431.350431	20736.963907	30.308327
431.897125	20768.310428	30.313344
432.285800	20792.327176	30.318362
432.828076	20831.966920	30.323380
433.247835	20860.854747	30.328397
433.265500	20896.107186	30.333415
433.547891	20931.005398	30.338432
434.093942	20959.194635	30.343450
434.590992	20995.635613	30.348468
435.112945	21039.300897	30.353485
436.057240	21061.239837	30.358503
436.571864	21099.757571	30.363520
436.886905	21126.958933	30.368538
437.426834	21141.485726	30.373556
438.581493	21143.128483	30.378573
438.545188	21173.435389	30.383591
439.938027	21183.088583	30.388608
440.555307	21198.078762	30.393626
440.121819	21231.746340	30.398644
440.284261	21237.022965	30.403661
440.613892	21270.506234	30.408679
441.035326	21295.612414	30.413696
441.348068	21328.862107	30.418714
441.390414	21356.692210	30.423732
442.206893	21394.760319	30.428749
442.232227	21431.467775	30.433767
442.612257	21465.431841	30.438784
442.888349	21499.698502	30.443802
442.721715	21538.407029	30.448820
443.172032	21579.381744	30.453837
443.535686	21629.554423	30.458855
443.834643	21679.553478	30.463872
444.860968	21723.946020	30.468890
445.073051	21768.796379	30.473908
445.326776	21824.524777	30.478925
445.988535	21868.443457	30.483943
446.437681	21909.931566	30.488960
447.279035	21958.813914	30.493978
447.833243	21991.933591	30.498996
448.179015	22023.623091	30.504013
448.612023	22066.298289	30.509031
449.440375	22092.811007	30.514048
450.114578	22123.959270	30.519066
450.552305	22154.389874	30.524084
450.589357	22193.435192	30.529101
451.076453	22229.733870	30.534119
451.314843	22253.870559	30.539136
451.766913	22284.894997	30.544154
452.244787	22337.723322	30.549172
452.445438	22366.115455	30.554189
452.646504	22410.458512	30.559207
453.310628	22449.564813	30.564224
453.807099	22486.021738	30.569242
454.283435	22540.233678	30.574260
454.894969	22572.944560	30.579277
455.174389	22606.665825	30.584295
455.517700	22645.615877	30.589312
455.878625	22679.563479	30.594330
456.470547	22738.171649	30.599348
457.091357	22763.535624	30.604365
457.356566	22808.909742	30.609383
458.097842	22850.724015	30.614400
458.463617	22882.752393	30.619418
458.910388	22934.271186	30.624436
459.365802	22968.553788	30.629453
459.730318	23025.451959	30.634471
459.962209	23060.093316	30.639488
460.721619	23111.758098	30.644506
461.057073	23155.617359	30.649524
461.299914	23196.311785	30.654541
461.948627	23246.071662	30.659559
462.269471	23290.389360	30.664576
462.907615	23330.659318	30.669594
463.428135	23376.642403	30.674612
464.331009	23421.417741	30.679629
464.784197	23465.792875	30.684647
464.812942	23509.140817	30.689664
466.056655	23545.154945	30.694682
466.101832	23584.014499	30.699700
466.438166	23631.343716	30.704717
466.601834	23673.069377	30.709735
466.917880	23728.817419	30.714752
467.511639	23775.461195	30.719770
468.127069	23821.798777	30.724788
468.462544	23867.884718	30.729805
469.238438	23908.986340	30.734823
469.700000	23952.175621	30.739840
470.402725	23996.365863	30.744858
471.063668	24042.959858	30.749876
471.722021	24073.392169	30.754893
471.888339	24108.243603	30.759911
472.269183	24151.292197	30.764928
473.328795	24184.755285	30.769946
473.244720	24223.659729	30.774964
474.104351	24266.117064	30.779981
474.601103	24295.553111	30.784999
474.891735	24338.492513	30.790016
475.610094	24357.436121	30.795034
476.130773	24392.719999	30.800052
476.663311	24424.707982	30.805069
477.167022	24449.352720	30.810087
477.172657	24495.195247	30.815104
477.757693	24527.053335	30.820122
477.766135	24570.237039	30.825140
477.866771	24619.471779	30.830157
478.927415	24649.515421	30.835175
479.291096	24699.460682	30.840192
480.041435	24735.992481	30.845210
480.272080	24786.923437	30.850228
481.122123	24811.437382	30.855245
481.551199	24855.749177	30.860263
482.239880	24890.364551	30.865280
482.408238	24932.986621	30.870298
482.727474	24978.851186	30.875316
483.203520	25018.335103	30.880333
483.565997	25063.743340	30.885351
483.759187	25110.199914	30.890368
484.254784	25139.839458	30.895386
484.508744	25196.911398	30.900404
484.844062	25236.275566	30.905421
485.450485	25274.680434	30.910439
485.851698	25334.437651	30.915456
486.496153	25377.729652	30.920474
486.822767	25427.099705	30.925492
487.339656	25479.027797	30.930509
487.767226	25522.458490	30.935527
487.806419	25597.826610	30.940544
488.299469	25646.334025	30.945562
489.002425	25693.810272	30.950580
489.354309	25752.739738	30.955597
490.176276	25800.095698	30.960615
490.471715	25860.993447	30.965632
491.581946	25897.042512	30.970650
492.020962	25959.825034	30.975668
492.446784	26015.491465	30.980685
493.309934	26053.735831	30.985703
493.872433	26114.729147	30.990720
494.305761	26153.290742	30.995738
495.247608	26200.842484	31.000756
495.315012	26235.386585	31.005773
495.886143	26275.180988	31.010791
496.262268	26323.876801	31.015808
497.017398	26373.686604	31.020826
497.220848	26411.324771	31.025844
497.226150	26471.234934	31.030861
498.355820	26520.320949	31.035879
498.537059	26552.068160	31.040896
499.086002	26595.677082	31.045914
500.220108	26660.706608	31.050932
500.168876	26701.024291	31.055949
501.036687	26739.925474	31.060967
501.367401	26793.178330	31.065984
501.946077	26829.228848	31.071002
502.524255	26865.399380	31.076020
502.839549	26922.884863	31.081037
504.100364	26942.531865	31.086055
504.975443	26980.341063	31.091072
505.418855	27011.326675	31.096090
506.040079	27036.517181	31.101108
506.405542	27067.279208	31.106125
507.142315	27099.206930	31.111143
507.537003	27153.629995	31.116160
507.793228	27176.237797	31.121178
507.934243	27215.679612	31.126196
508.025062	27243.304745	31.131213
508.702956	27288.382907	31.136231
509.053447	27334.981971	31.141248
509.644510	27390.423700	31.146266
509.692791	27446.778513	31.151284
510.385136	27503.462414	31.156301
510.602662	27538.302914	31.161319
510.496290	27595.658419	31.166336
511.180977	27650.237025	31.171354
511.913205	27713.646232	31.176372
512.326763	27776.020079	31.181389
513.188557	27834.667436	31.186407
512.907487	27893.087394	31.191424
513.584831	27950.355634	31.196442
514.225713	28007.850890	31.201460
514.810470	28074.313938	31.206477
515.472137	28128.554037	31.211495
516.231043	28187.459319	31.216512
517.146670	28222.627506	31.221530
518.294952	28255.214909	31.226548
518.450799	28291.660078	31.231565
519.342218	28322.378480	31.236583
520.075056	28365.942589	31.241600
520.301167	28382.055739	31.246618
520.929939	28426.681296	31.251636
521.678270	28459.701059	31.256653
521.872603	28480.106396	31.261671
522.375024	28519.207598	31.266688
522.345016	28553.677803	31.271706
522.994885	28598.410724	31.276724
523.579082	28640.413395	31.281741
524.202567	28684.775518	31.286759
524.321262	28727.918339	31.291776
524.544981	28773.343528	31.296794
525.396754	28822.873175	31.301812
525.305035	28871.735479	31.306829
526.096942	28929.038513	31.311847
526.355965	28985.414001	31.316864
526.828315	29046.495679	31.321882
527.370091	29107.657587	31.326900
527.656143	29168.221575	31.331917
528.406597	29218.491478	31.336935
528.851575	29292.345013	31.341952
529.759496	29354.292736	31.346970
530.453500	29395.364273	31.351988
530.754510	29446.832103	31.357005
531.903691	29504.525981	31.362023
532.489005	29547.918691	31.367040
533.454857	29598.050016	31.372058
533.930387	29651.634768	31.377076
534.317560	29685.972067	31.382093
534.961099	29732.078071	31.387111
535.191960	29780.583647	31.392128
535.952466	29821.739849	31.397146
536.715938	29874.037947	31.402164
537.025661	29912.962757	31.407181
537.631832	29942.967723	31.412199
537.917894	29998.922459	31.417216
538.322001	30048.450678	31.422234
539.280654	30086.095144	31.427252
539.793699	30138.697242	31.432269
540.553756	30179.450561	31.437287
540.494448	30232.153784	31.442304
540.873895	30275.191124	31.447322
541.345417	30334.886223	31.452340
541.577324	30392.191935	31.457357
542.348350	30447.443366	31.462375
542.709087	30513.413289	31.467392
543.189195	30571.751221	31.472410
543.929889	30628.150271	31.477428
544.557711	30679.946341	31.482445
544.954474	30733.771422	31.487463
545.187439	30804.158216	31.492480
545.594379	30852.934244	31.497498
546.263134	30925.350676	31.502516
547.018815	30995.115577	31.507533
547.381157	31050.537373	31.512551
548.310176	31119.447561	31.517568
548.584082	31180.613664	31.522586
549.465228	31223.646194	31.527604
549.925755	31290.470165	31.532621
550.613574	31349.505172	31.537639
551.252895	31399.553640	31.542656
551.424235	31459.160182	31.547674
552.251525	31510.436747	31.552692
552.680244	31561.659405	31.557709
553.122886	31605.825372	31.562727
553.876741	31654.161425	31.567744
554.386036	31712.520423	31.572762
555.005348	31759.408758	31.577780
555.768032	31797.572003	31.582797
556.331583	31845.681304	31.587815
556.974506	31898.125264	31.592832
557.493752	31947.005679	31.597850
558.446394	31987.715634	31.602868
558.274511	32033.905602	31.607885
558.964465	32086.093106	31.612903
559.642556	32126.586858	31.617920
559.715415	32195.835145	31.622938
560.445818	32249.442553	31.627956
561.016674	32299.432328	31.632973
561.437806	32361.707754	31.637991
561.845848	32411.115800	31.643008
562.604928	32476.326874	31.648026
563.304023	32526.501198	31.653044
563.693050	32582.232624	31.658061
564.210830	32630.976355	31.663079
564.767745	32689.188746	31.668096
565.133269	32764.423623	31.673114
565.974494	32828.360358	31.678132
566.401706	32896.921830	31.683149
567.169385	32953.128274	31.688167
567.480603	33017.004934	31.693184
567.835676	33091.334222	31.698202
568.538716	33144.819509	31.703220
568.973164	33209.288630	31.708237
570.114552	33263.585353	31.713255
570.578427	33329.902203	31.718272
570.940957	33404.111673	31.723290
571.550442	33455.142749	31.728308
571.874545	33524.241154	31.733325
572.673844	33594.962071	31.738343
573.953487	33643.560678	31.743360
574.111630	33705.499326	31.748378
575.243890	33766.822929	31.753396
575.266319	33830.011863	31.758413
575.918531	33898.338110	31.763431
576.567484	33945.599701	31.768448
577.127892	34011.354118	31.773466
578.056629	34072.510449	31.778484
578.454289	34125.910300	31.783501
578.783700	34189.702987	31.788519
579.900356	34247.597712	31.793536
580.334624	34302.658127	31.798554
581.194663	34357.522174	31.803572
581.453160	34415.167902	31.808589
581.931240	34463.206943	31.813607
582.439185	34519.928274	31.818624
582.878290	34582.350543	31.823642
583.384710	34642.663490	31.828660
584.026234	34720.057327	31.833677
584.194907	34777.229955	31.838695
584.667203	34840.906711	31.843712
585.335727	34920.960253	31.848730
586.098064	34987.000486	31.853748
586.682397	35057.563931	31.858765
587.166846	35120.072107	31.863783
588.015614	35177.872106	31.868800
588.303753	35252.852618	31.873818
589.568509	35311.916024	31.878836
589.721442	35369.970419	31.883853
590.382973	35432.570358	31.888871
591.398217	35494.736572	31.893888
591.760233	35561.349957	31.898906
592.316456	35611.831156	31.903924
592.958709	35679.881875	31.908941
592.672174	35728.369336	31.913959
593.419999	35795.071345	31.918976
593.748816	35849.286129	31.923994
594.399070	35919.744265	31.929012
594.803986	36004.024410	31.934029
595.541697	36069.791853	31.939047
596.144457	36139.141552	31.944064
596.592958	36214.516172	31.949082
597.553735	36293.688153	31.954100
597.980681	36361.518246	31.959117
598.365484	36432.725990	31.964135
599.580928	36496.418452	31.969152
600.498039	36555.133127	31.974170
601.382185	36614.333131	31.979188
601.795074	36680.500451	31.984205
602.447786	36737.713010	31.989223
603.342883	36798.849532	31.994240
603.414052	36867.516648	31.999258
604.474434	36912.325967	32.004276
604.738697	36979.333162	32.009293
605.208790	37057.620683	32.014311
606.236980	37107.021398	32.019328
606.746200	37169.277001	32.024346
607.701584	37227.993869	32.029364
608.956946	37267.858017	32.034381
609.651160	37328.780198	32.039399
610.384727	37381.944936	32.044416
610.491311	37427.919834	32.049434
611.107415	37484.162451	32.054452
611.428540	37536.209097	32.059469
611.559458	37597.177877	32.064487
612.438182	37647.775656	32.069504
612.774534	37736.916632	32.074522
613.570949	37787.440027	32.079540
614.015385	37839.053735	32.084557
614.850849	37904.309931	32.089575
615.815982	37970.352910	32.094592
615.881560	38037.450504	32.099610
616.739611	38083.659604	32.104628
617.807047	38151.431689	32.109645
618.615250	38203.444001	32.114663
619.354442	38257.885477	32.119680
619.823505	38313.227052	32.124698
620.378561	38372.335695	32.129716
620.918334	38407.043425	32.134733
620.961512	38478.880630	32.139751
621.482048	38546.091186	32.144768
621.820166	38622.696624	32.149786
622.479098	38679.232573	32.154804
623.044766	38749.248630	32.159821
623.695567	38809.494915	32.164839
625.132969	38881.595829	32.169856
625.559647	38957.774585	32.174874
626.128038	39008.518961	32.179892
626.406507	39061.407142	32.184909
627.117887	39157.727407	32.189927
627.808278	39208.449037	32.194944
627.946497	39283.439520	32.199962
628.732463	39364.437182	32.204980
629.324586	39428.081975	32.209997
629.745078	39503.755866	32.215015
630.393834	39576.722069	32.220032
630.918716	39646.334832	32.225050
631.374956	39725.949241	32.230068
632.130937	39801.493208	32.235085
632.470241	39881.288585	32.240103
633.389261	39948.738379	32.245120
633.921120	40013.225315	32.250138
634.713756	40078.417496	32.255156
635.730930	40144.327227	32.260173
636.333455	40220.504319	32.265191
637.585895	40270.091284	32.270208
637.954692	40344.006400	32.275226
638.838207	40397.306733	32.280244
639.473763	40443.407078	32.285261
640.343168	40491.126104	32.290279
641.168071	40548.341206	32.295296
641.329784	40615.691265	32.300314
641.924062	40672.793329	32.305332
642.389880	40745.289366	32.310349
642.750500	40811.660320	32.315367
643.580980	40867.148838	32.320384
643.933541	40931.848555	32.325402
644.765129	41001.150674	32.330420
645.520695	41069.124037	32.335437
645.733854	41144.248671	32.340455
646.396547	41200.510881	32.345472
646.977473	41289.366855	32.350490
647.828745	41350.099810	32.355508
648.431568	41418.715249	32.360525
649.084761	41501.202712	32.365543
649.954407	41564.600770	32.370560
650.408923	41646.121012	32.375578
651.077451	41718.634769	32.380596
652.317975	41794.915075	32.385613
652.731497	41861.779858	32.390631
653.686557	41915.991422	32.395648
654.553583	41989.464698	32.400666
655.234236	42044.432239	32.405684
656.022899	42110.225791	32.410701
656.659134	42172.326001	32.415719
657.575390	42222.314721	32.420736
657.683261	42278.371960	32.425754
658.225946	42342.069775	32.430772
658.991423	42406.621254	32.435789
659.479847	42486.292844	32.440807
660.511252	42538.391148	32.445824
660.996827	42613.129528	32.450842
661.132251	42677.249332	32.455860
661.646366	42743.068385	32.460877
662.166104	42833.416201	32.465895
663.094289	42905.926475	32.470912
663.445621	42992.994390	32.475930
664.048785	43074.439570	32.480948
664.781916	43161.066383	32.485965
665.371327	43241.488544	32.490983
666.223822	43324.787858	32.496000
666.950870	43411.868305	32.501018
667.328112	43492.579157	32.506036
667.931795	43567.674419	32.511053
668.580414	43650.677375	32.516071
669.525333	43733.972736	32.521088
670.088941	43821.271521	32.526106
670.531207	43912.189884	32.531124
671.502732	43993.505652	32.536141
671.637309	44082.713976	32.541159
672.396394	44162.960563	32.546176
673.335215	44259.522574	32.551194
674.068934	44334.634189	32.556212
675.377819	44407.557888	32.561229
675.808242	44489.625044	32.566247
676.274915	44564.503852	32.571264
676.992133	44645.640305	32.576282
677.271045	44734.246975	32.581300
678.004902	44816.363334	32.586317
678.972055	44888.410796	32.591335
679.624346	44949.639930	32.596352
680.397920	45026.196954	32.601370
680.609741	45099.124568	32.606388
681.516238	45164.435900	32.611405
682.013700	45263.418745	32.616423
682.133476	45346.813385	32.621440
682.788547	45427.480419	32.626458
683.436249	45529.215200	32.631476
684.279106	45606.041008	32.636493
684.834416	45701.369798	32.641511
685.566525	45778.846090	32.646528
686.464836	45879.916214	32.651546
686.723000	45982.908150	32.656564
687.839911	46064.111048	32.661581
688.433685	46169.994527	32.666599
688.957032	46248.795499	32.671616
690.142989	46339.564960	32.676634
690.852615	46436.937032	32.681652
691.820396	46521.251468	32.686669
692.560029	46609.573042	32.691687
693.529458	46688.532694	32.696704
694.469138	46773.617041	32.701722
694.773260	46864.001026	32.706740
695.608742	46925.910512	32.711757
695.993090	47014.813670	32.716775
696.567439	47103.398521	32.721792
697.241138	47192.662071	32.726810
697.929799	47275.068214	32.731828
698.898370	47367.675262	32.736845
699.820379	47448.767912	32.741863
700.365109	47548.882285	32.746880
701.088610	47627.542288	32.751898
701.576569	47709.572962	32.756916
702.775950	47785.742501	32.761933
703.688733	47870.630980	32.766951
704.571870	47945.198702	32.771968
705.593716	48014.154471	32.776986
706.628688	48093.731269	32.782004
707.602123	48155.738846	32.787021
708.585979	48215.698616	32.792039
709.035957	48291.602376	32.797056
710.053031	48342.762411	32.802074
710.135901	48400.844202	32.807092
710.925606	48468.207335	32.812109
711.330220	48532.536396	32.817127
711.987713	48601.106048	32.822144
712.927147	48671.407303	32.827162
713.328650	48750.516725	32.832180
713.884965	48825.969264	32.837197
714.552626	48906.456461	32.842215
715.215322	48990.159642	32.847232
715.922378	49059.351201	32.852250
716.109220	49140.193533	32.857268
717.335042	49222.301530	32.862285
717.642312	49300.487708	32.867303
718.138230	49385.075993	32.872320
719.044706	49465.289259	32.877338
719.522049	49568.447666	32.882356
720.439034	49648.082037	32.887373
721.029725	49744.309618	32.892391
721.822779	49830.799359	32.897408
722.589906	49909.628982	32.902426
723.302147	50012.858373	32.907444
724.190435	50095.922785	32.912461
724.986971	50173.649599	32.917479
725.339469	50251.844830	32.922496
726.241886	50329.011582	32.927514
726.590783	50418.896599	32.932532
727.538215	50491.909835	32.937549
728.272887	50569.812701	32.942567
728.962144	50661.594442	32.947584
729.786616	50736.637566	32.952602
730.093141	50823.660609	32.957620
730.634081	50910.847465	32.962637
731.578178	50995.659414	32.967655
732.013075	51083.982610	32.972672
732.904743	51173.503592	32.977690
733.608426	51272.846938	32.982708
733.880856	51355.806894	32.987725
734.819033	51466.387901	32.992743
735.412372	51563.006325	32.997760
736.085808	51671.942483	33.002778
736.858429	51772.584607	33.007796
737.347924	51865.090454	33.012813
738.434986	51979.146222	33.017831
739.105474	52073.246632	33.022848
739.903593	52177.124103	33.027866
740.441709	52287.172601	33.032884
741.391576	52382.820277	33.037901
742.209437	52498.490198	33.042919
742.887806	52591.536868	33.047936
744.091839	52694.528856	33.052954
744.683274	52806.706705	33.057972
745.372589	52900.915419	33.062989
746.240402	53009.612220	33.068007
746.946668	53107.855882	33.073024
747.477992	53199.167217	33.078042
748.107755	53310.634104	33.083060
749.086312	53423.421227	33.088077
750.129440	53519.362341	33.093095
750.806776	53622.016637	33.098112
751.831142	53718.290338	33.103130
752.351074	53820.820054	33.108148
753.335262	53922.881954	33.113165
753.854924	54021.356884	33.118183
754.572254	54128.290580	33.123200
755.711083	54229.589384	33.128218
756.263300	54334.018083	33.133236
756.560325	54432.493942	33.138253
757.731018	54539.367657	33.143271
758.077802	54650.945786	33.148288
759.646843	54735.219170	33.153306
759.886387	54851.794610	33.158324
760.486114	54957.899345	33.163341
761.425459	55062.975608	33.168359
762.277214	55174.264836	33.173376
763.199608	55284.595327	33.178394
763.748049	55385.365800	33.183412
764.397534	55495.654090	33.188429
765.371444	55591.844252	33.193447
765.779147	55716.579011	33.198464
766.812050	55820.841472	33.203482
767.526600	55925.055963	33.208500
768.220515	56029.710373	33.213517
769.335835	56127.490956	33.218535
769.983424	56237.815305	33.223552
770.857171	56346.049458	33.228570
771.319024	56451.862776	33.233588
772.276483	56564.740957	33.238605
772.979449	56667.059433	33.243623
773.871493	56768.045607	33.248640
774.599864	56868.465382	33.253658
775.342534	56964.157027	33.258676
776.094722	57068.598803	33.263693
777.110603	57171.443204	33.268711
777.616329	57267.364999	33.273728
778.228935	57363.655047	33.278746
779.009507	57470.640680	33.283764
779.855657	57564.378288	33.288781
780.971966	57647.374049	33.293799
781.789145	57737.256489	33.298816
782.687690	57832.307339	33.303834
783.495961	57928.352974	33.308852
784.033916	58022.604912	33.313869
784.827322	58128.884252	33.318887
785.481704	58232.217206	33.323904
785.848895	58330.719861	33.328922
786.867067	58433.709433	33.333940
787.578153	58538.848170	33.338957
788.496028	58638.853813	33.343975
789.616410	58744.690657	33.348992
790.420119	58839.717736	33.354010
791.241890	58935.822865	33.359028
791.921675	59041.929932	33.364045
792.592320	59138.244244	33.369063
793.114620	59258.186008	33.374080
794.063668	59366.449440	33.379098
794.657286	59477.874948	33.384116
795.745099	59590.470707	33.389133
796.600508	59691.414553	33.394151
797.421723	59812.220264	33.399168
797.994445	59914.267257	33.404186
799.071163	60023.739132	33.409204
799.487919	60131.879723	33.414221
800.575759	60242.570626	33.419239
801.424375	60354.647720	33.424256
802.178499	60455.081274	33.429274
802.875417	60568.859316	33.434292
803.601739	60674.840924	33.439309
804.958914	60794.988934	33.444327
806.187981	60887.648749	33.449344
807.596440	60977.903116	33.454362
809.069689	61069.392198	33.459380
809.640930	61144.674809	33.464397
810.894619	61231.239782	33.469415
811.518024	61312.979661	33.474432
811.743295	61398.609181	33.479450
812.615583	61495.369144	33.484468
812.839819	61595.352343	33.489485
813.637996	61693.199890	33.494503
813.946640	61797.278172	33.499520
814.593394	61909.972344	33.504538
815.515000	62006.334753	33.509556
816.075701	62123.190327	33.514573
816.867776	62233.346866	33.519591
817.653414	62341.918683	33.524608
818.282313	62461.078144	33.529626
818.943475	62576.099488	33.534644
819.260758	62696.190301	33.539661
820.320618	62823.288603	33.544679
820.864457	62964.125039	33.549696
821.273352	63094.025021	33.554714
822.279228	63220.325686	33.559732
822.991201	63357.622863	33.564749
824.159947	63481.976801	33.569767
824.632184	63625.699161	33.574784
825.737617	63751.721198	33.579802
826.407391	63877.879154	33.584820
827.230700	64016.862632	33.589837
828.017265	64142.813308	33.594855
828.848464	64270.975998	33.599872
829.830984	64412.609577	33.604890
830.807100	64525.605100	33.609908
831.681564	64663.345599	33.614925
832.727264	64757.703052	33.619943
833.501670	64877.351885	33.624960
834.329852	64989.198667	33.629978
835.567975	65097.425912	33.634996
836.284230	65215.392254	33.640013
837.539098	65328.156513	33.645031
838.453198	65436.748776	33.650048
838.967108	65541.539098	33.655066
840.203587	65650.875728	33.660084
840.760869	65775.300233	33.665101
841.727210	65887.552587	33.670119
842.241554	65994.260489	33.675136
843.241922	66118.898353	33.680154
843.914840	66233.065839	33.685172
844.698558	66349.244849	33.690189
845.653435	66469.157543	33.695207
846.708784	66583.402879	33.700224
847.385258	66702.275581	33.705242
848.508110	66813.830687	33.710260
848.989396	66949.249085	33.715277
850.161275	67052.225211	33.720295
851.068267	67189.926545	33.725312
851.917949	67311.701079	33.730330
852.881611	67423.329982	33.735348
853.538812	67544.277888	33.740365
854.213069	67662.404123	33.745383
855.152093	67773.665972	33.750400
855.816237	67903.130408	33.755418
857.530961	68010.333187	33.760436
858.297715	68128.351946	33.765453
859.635725	68233.696179	33.770471
860.371918	68342.415145	33.775488
861.196628	68460.552643	33.780506
862.188008	68567.675400	33.785524
863.023767	68690.345340	33.790541
863.827890	68795.104069	33.795559
864.743158	68912.242886	33.800576
865.250646	69021.154854	33.805594
866.073012	69133.296673	33.810612
867.107838	69255.519761	33.815629
867.864506	69361.085752	33.820647
868.854801	69493.736855	33.825664
869.316728	69607.287378	33.830682
870.364533	69732.419410	33.835700
870.879520	69861.490576	33.840717
871.468463	69982.248788	33.845735
872.953687	70100.330659	33.850752
874.245905	70211.635580	33.855770
875.185638	70322.335406	33.860788
875.729999	70443.053021	33.865805
876.686607	70567.522186	33.870823
877.607913	70691.618542	33.875840
878.217450	70813.825996	33.880858
879.046024	70926.583268	33.885876
879.161657	71072.211385	33.890893
880.285756	71198.066585	33.895911
881.148431	71323.592637	33.900928
881.780960	71457.984335	33.905946
882.882915	71593.601917	33.910964
883.331617	71716.713674	33.915981
883.897942	71868.943650	33.920999
884.774567	72016.210371	33.926016
885.113978	72168.245980	33.931034
886.032110	72307.306642	33.936052
887.164486	72462.583701	33.941069
888.117050	72600.489736	33.946087
889.190745	72738.553710	33.951104
889.914289	72882.493930	33.956122
891.245521	73008.129533	33.961140
892.184091	73140.900370	33.966157
892.692244	73282.690896	33.971175
894.237236	73418.765381	33.976192
895.132235	73543.084940	33.981210
896.577592	73659.099924	33.986228
897.192443	73794.963584	33.991245
898.155067	73916.447436	33.996263
899.198326	74030.873990	34.001280
899.614108	74168.296884	34.006298
900.942036	74288.995274	34.011316
902.039613	74419.154933	34.016333
902.580763	74539.143543	34.021351
903.484369	74661.691082	34.026368
904.694386	74802.496640	34.031386
905.523714	74914.661245	34.036404
906.418906	75054.780505	34.041421
907.278817	75176.579271	34.046439
908.235899	75313.755600	34.051456
908.711013	75459.651184	34.056474
909.523135	75597.599481	34.061492
910.128574	75732.142381	34.066509
910.737688	75877.430472	34.071527
911.801756	76018.982620	34.076544
912.913013	76177.464571	34.081562
913.623369	76326.862419	34.086580
914.178948	76482.617629	34.091597
915.593682	76628.201416	34.096615
916.544182	76775.115077	34.101632
917.367136	76932.695070	34.106650
918.055445	77077.478377	34.111668
919.262132	77225.592374	34.116685
920.352293	77369.596562	34.121703
921.493581	77522.011509	34.126720
922.468590	77675.340434	34.131738
923.402519	77825.046739	34.136756
924.354421	77963.518081	34.141773
925.639902	78112.409300	34.146791
926.498869	78247.804870	34.151808
927.443325	78401.428490	34.156826
928.599335	78522.665589	34.161844
929.461982	78673.939031	34.166861
930.031376	78812.700204	34.171879
931.196622	78960.111577	34.176896
932.018523	79110.623043	34.181914
933.037543	79259.262329	34.186932
933.756795	79410.368363	34.191949
934.601474	79555.173645	34.196967
935.784627	79690.220845	34.201984
936.806741	79843.006629	34.207002
938.085647	79967.324428	34.212020
938.633592	80111.454874	34.217037
939.501917	80271.808970	34.222055
940.627830	80410.646316	34.227072
941.254269	80566.671476	34.232090
942.511020	80712.782537	34.237108
943.566639	80850.217255	34.242125
944.731352	80997.800276	34.247143
946.289818	81115.075673	34.252160
946.899019	81255.199115	34.257178
948.136520	81384.491036	34.262196
949.088936	81520.510911	34.267213
949.889618	81650.875969	34.272231
950.840061	81773.910560	34.277248
951.948900	81911.083589	34.282266
953.186639	82034.160727	34.287284
953.872158	82150.813852	34.292301
954.333653	82269.775635	34.297319
955.573614	82381.840549	34.302336
956.249268	82511.219017	34.307354
957.134892	82629.372497	34.312372
958.123909	82758.966338	34.317389
958.679383	82897.248886	34.322407
959.265291	83014.372054	34.327424
960.279008	83159.501522	34.332442
961.421400	83298.720799	34.337460
962.251622	83439.770192	34.342477
962.535469	83585.636533	34.347495
963.960851	83722.502510	34.352512
964.409851	83874.524424	34.357530
965.449259	84024.925160	34.362548
966.399892	84185.413540	34.367565
967.430131	84347.009721	34.372583
968.070207	84495.834537	34.377600
968.867480	84653.118549	34.382618
969.663899	84813.782292	34.387636
970.871673	84996.561193	34.392653
971.711625	85152.702735	34.397671
972.448713	85331.310320	34.402688
973.435027	85503.386640	34.407706
974.305062	85676.831097	34.412724
975.479535	85853.984883	34.417741
976.610323	86026.964997	34.422759
978.067045	86193.331299	34.427776
979.069164	86369.030586	34.432794
979.931653	86537.326029	34.437812
980.846258	86701.203940	34.442829
981.546567	86867.953043	34.447847
983.047312	87035.513975	34.452864
983.771664	87203.761106	34.457882
985.284270	87369.221760	34.462900
986.689476	87538.750948	34.467917
987.194551	87704.146191	34.472935
988.494483	87853.731491	34.477952
989.604400	88025.217570	34.482970
991.027611	88176.967630	34.487988
992.132087	88316.894087	34.493005
993.418697	88480.811634	34.498023
994.905266	88623.802772	34.503040
995.635099	88770.880964	34.508058
996.591535	88915.524381	34.513076
997.367911	89069.842222	34.518093
998.337538	89230.349593	34.523111
999.029137	89363.718683	34.528128
1000.091887	89528.085461	34.533146
1001.057453	89688.856064	34.538164
1002.034796	89843.949446	34.543181
1002.391574	90000.082868	34.548199
1003.488454	90171.966387	34.553216
1004.875486	90326.742155	34.558234
1005.917756	90489.410331	34.563252
1006.818527	90639.787950	34.568269
1007.635375	90804.223138	34.573287
1008.786750	90958.712841	34.578304
1009.950518	91134.914605	34.583322
1011.230881	91298.776722	34.588340
1012.240348	91441.781340	34.593357
1013.134393	91597.450470	34.598375
1014.380096	91761.074657	34.603392
1015.298517	91926.867783	34.608410
1015.734439	92093.374586	34.613428
1016.512240	92251.136649	34.618445
1017.485594	92411.474946	34.623463
1019.088729	92564.609328	34.628480
1019.404437	92727.526564	34.633498
1020.429186	92886.821592	34.638516
1021.663096	93036.089632	34.643533
1022.665459	93188.529699	34.648551
1023.741530	93338.578820	34.653568
1024.657653	93503.307212	34.658586
1025.641894	93653.474708	34.663604
1026.573370	93815.759626	34.668621
1027.248180	93990.778161	34.673639
1028.389280	94141.232910	34.678656
1029.413295	94321.417842	34.683674
1030.566917	94483.486988	34.688692
1032.397488	94638.008376	34.693709
1033.149021	94810.108590	34.698727
1034.468562	94963.241636	34.703744
1035.558205	95119.261892	34.708762
1036.767784	95255.983414	34.713780
1038.003708	95421.127698	34.718797
1038.922647	95575.489028	34.723815
1039.869015	95728.302351	34.728832
1040.509951	95892.339053	34.733850
1041.344339	96056.420869	34.738868
1042.166586	96224.183415	34.743885
1043.006959	96410.895771	34.748903
1044.123249	96576.884114	34.753920
1044.885152	96754.813428	34.758938
1045.798809	96939.808588	34.763956
1047.340105	97122.131507	34.768973
1047.537081	97312.400433	34.773991
1048.884430	97489.206559	34.779008
1050.026041	97680.911229	34.784026
1050.974485	97870.060190	34.789044
1052.570125	98060.382465	34.794061
1053.514479	98237.830163	34.799079
1054.592752	98412.256408	34.804096
1056.085148	98599.358676	34.809114
1056.932810	98788.759128	34.814132
1058.667425	98958.250665	34.819149
1059.977671	99128.376827	34.824167
1061.204486	99282.817993	34.829184
1062.809469	99440.907441	34.834202
1063.504784	99620.020352	34.839220
1064.478859	99773.031199	34.844237
1065.225325	99946.193423	34.849255
1066.232733	100125.378686	34.854272
1067.457275	100296.147305	34.859290
1068.029357	100479.724593	34.864308
1068.916600	100658.237064	34.869325
1069.599062	100837.987488	34.874343
1070.803346	101027.491486	34.879360
1072.073625	101209.686252	34.884378
1072.628978	101403.757270	34.889396
1073.442446	101584.782895	34.894413
1074.701377	101789.168163	34.899431
1075.759370	101975.999927	34.904448
1076.748326	102168.213421	34.909466
1077.425929	102371.711622	34.914484
1078.526490	102566.423236	34.919501
1080.040955	102765.436719	34.924519
1080.737567	102967.689203	34.929536
1082.684327	103167.020654	34.934554
1083.584015	103373.719227	34.939572
1085.338750	103541.851378	34.944589
1086.320971	103729.005981	34.949607
1087.552231	103906.502884	34.954624
1088.768704	104085.611724	34.959642
1089.759849	104269.045657	34.964660
1091.147688	104443.842022	34.969677
1091.951837	104611.302232	34.974695
1093.300397	104779.376497	34.979712
1094.034951	104942.975164	34.984730
1095.001783	105117.522622	34.989748
1095.793128	105294.170810	34.994765
1097.008771	105469.040473	34.999783
1097.885726	105645.334966	35.004800
1098.417743	105833.794799	35.009818
1099.271646	106026.141523	35.014836
1100.323686	106216.189976	35.019853
1101.404475	106411.034990	35.024871
1102.329511	106610.567812	35.029888
1103.665497	106803.283904	35.034906
1104.668977	106992.041485	35.039924
1105.836309	107199.403731	35.044941
1107.060523	107403.199291	35.049959
1108.189147	107605.846989	35.054976
1109.254856	107806.822123	35.059994
1110.656538	108013.278138	35.065012
1112.086991	108203.696369	35.070029
1113.346110	108405.594019	35.075047
1114.618464	108602.184052	35.080064
1116.197694	108775.521016	35.085082
1117.058514	108970.522467	35.090100
1118.468599	109161.318205	35.095117
1119.459396	109354.882400	35.100135
1120.577646	109546.501686	35.105152
1121.800846	109736.015073	35.110170
1122.560264	109925.251694	35.115188
1123.367531	110127.008903	35.120205
1124.645161	110327.587982	35.125223
1125.386482	110536.262425	35.130240
1126.611268	110735.763920	35.135258
1127.450643	110951.670774	35.140276
1129.129913	111157.763131	35.145293
1129.839332	111358.456304	35.150311
1130.980981	111573.507508	35.155328
1132.266520	111782.861722	35.160346
1133.379363	111999.479113	35.165364
1134.536380	112198.014462	35.170381
1135.271284	112419.219848	35.175399
1136.237458	112632.661568	35.180416
1137.816496	112841.709412	35.185434
1138.708606	113066.846404	35.190452
1140.195258	113270.047536	35.195469
1141.275886	113496.664407	35.200487
1142.058796	113713.400447	35.205504
1143.750270	113914.710297	35.210522
1144.929642	114130.902768	35.215540
1146.733281	114332.045117	35.220557
1148.063138	114554.208218	35.225575
1149.253716	114769.808393	35.230592
1150.572925	114957.061727	35.235610
1151.382888	115161.072535	35.240628
1152.862008	115355.067291	35.245645
1153.884940	115555.878600	35.250663
1154.774792	115756.092531	35.255680
1156.440041	115953.481362	35.260698
1157.452869	116176.368487	35.265716
1158.622479	116362.046914	35.270733
1159.932802	116548.159437	35.275751
1160.756954	116755.739603	35.280768
1161.947088	116954.240110	35.285786
1162.631070	117165.875364	35.290804
1164.069009	117372.155113	35.295821
1164.940952	117576.223868	35.300839
1166.287476	117780.760560	35.305856
1167.687685	117975.559241	35.310874
1168.767953	118173.579607	35.315892
1170.427063	118343.998695	35.320909
1171.667022	118533.911590	35.325927
1172.632182	118718.207434	35.330944
1173.735526	118904.382228	35.335962
1174.424638	119105.615894	35.340980
1175.355970	119300.678385	35.345997
1176.657234	119495.782502	35.351015
1177.330142	119711.822520	35.356032
1178.059190	119909.431350	35.361050
1179.046420	120121.215797	35.366068
1180.066054	120333.883424	35.371085
1181.401412	120570.449090	35.376103
1181.974021	120807.966223	35.381120
1182.962574	121030.122229	35.386138
1184.441544	121257.026827	35.391156
1185.896090	121480.439857	35.396173
1187.445542	121719.121017	35.401191
1188.277513	121942.817748	35.406208
1189.957664	122152.006238	35.411226
1190.878792	122407.536307	35.416244
1192.324827	122637.536337	35.421261
1193.400776	122850.238324	35.426279
1194.486501	123094.430903	35.431296
1196.233593	123331.242366	35.436314
1197.334805	123561.293834	35.441332
1198.751944	123789.685516	35.446349
1199.891391	124012.612165	35.451367
1201.233069	124248.217920	35.456384
1202.542299	124467.812349	35.461402
1203.775137	124688.802358	35.466420
1205.413387	124919.460010	35.471437
1206.554212	125140.379829	35.476455
1207.465465	125376.927295	35.481472
1209.144123	125590.474514	35.486490
1210.386895	125816.363105	35.491508
1211.620116	126046.487934	35.496525
1212.858712	126259.833711	35.501543
1213.975610	126493.871953	35.506560
1214.969778	126714.117771	35.511578
1216.189045	126939.334234	35.516596
1216.860451	127157.000357	35.521613
1218.750317	127394.162494	35.526631
1219.860156	127625.992636	35.531648
1221.057842	127847.607215	35.536666
1222.295286	128085.414723	35.541684
1223.902983	128304.049811	35.546701
1225.281755	128536.184657	35.551719
1225.965372	128770.185099	35.556736
1227.708665	128989.778627	35.561754
1228.590043	129220.061475	35.566772
1229.709538	129454.844371	35.571789
1230.963799	129687.312612	35.576807
1232.134817	129919.517479	35.581824
1233.401605	130149.540802	35.586842
1234.539268	130376.240843	35.591860
1236.120551	130610.271763	35.596877
1237.797159	130822.702274	35.601895
1239.461022	131055.353934	35.606912
1240.409394	131266.918955	35.611930
1241.785738	131481.025972	35.616948
1242.911752	131693.274381	35.621965
1244.312787	131923.681508	35.626983
1245.524962	132152.980641	35.632000
1246.490989	132360.290919	35.637018
1247.419340	132588.486519	35.642036
1248.707428	132831.950060	35.647053
1249.500615	133049.776687	35.652071
1250.358547	133277.025434	35.657088
1252.017453	133480.235540	35.662106
1253.006622	133713.119481	35.667124
1253.995113	133946.081286	35.672141
1255.620031	134149.415335	35.677159
1256.865768	134375.441585	35.682176
1257.814009	134597.804152	35.687194
1259.273714	134823.506653	35.692212
1259.836980	135065.471418	35.697229
1261.438134	135292.091951	35.702247
1262.398059	135541.347627	35.707264
1263.648903	135786.969464	35.712282
1264.968004	136021.007250	35.717300
1265.755495	136275.494805	35.722317
1267.355802	136522.408324	35.727335
1267.907838	136772.311208	35.732352
1269.130546	137033.236553	35.737370
1270.623331	137295.691470	35.742388
1271.519371	137561.239014	35.747405
1272.593378	137822.524771	35.752423
1273.401337	138112.737848	35.757440
1274.893777	138388.767355	35.762458
1276.161024	138661.311668	35.767476
1277.373547	138939.065503	35.772493
1279.212246	139227.710819	35.777511
1280.515662	139516.510362	35.782528
1281.915001	139783.552030	35.787546
1283.370376	140060.907369	35.792564
1284.242610	140336.535423	35.797581
1285.886471	140616.501487	35.802599
1287.322078	140898.710455	35.807616
1288.669199	141166.443657	35.812634
1290.039714	141444.268091	35.817652
1290.810866	141734.163383	35.822669
1292.585440	142019.102530	35.827687
1293.732924	142318.691453	35.832704
1295.114011	142604.296351	35.837722
1296.959884	142870.882732	35.842740
1297.975180	143147.866584	35.847757
1299.711893	143419.623394	35.852775
1301.080716	143705.467642	35.857792
1302.790853	143982.685838	35.862810
1304.147336	144242.313117	35.867828
1305.301675	144518.042206	35.872845
1307.099741	144764.374438	35.877863
1308.757938	145033.202115	35.882880
1310.155360	145293.401049	35.887898
1312.279287	145548.130557	35.892916
1312.990721	145809.055197	35.897933
1314.799969	146066.401974	35.902951
1315.693660	146307.834378	35.907968
1317.356219	146549.445877	35.912986
1318.432593	146802.569175	35.918004
1319.385028	147057.223837	35.923021
1321.000787	147306.330354	35.928039
1322.146909	147568.996910	35.933056
1323.436005	147830.018495	35.938074
1324.853815	148079.505438	35.943092
1325.851188	148344.852728	35.948109
1327.048017	148601.608544	35.953127
1327.978521	148865.220523	35.958144
1329.364591	149143.952729	35.963162
1330.216682	149405.121160	35.968180
1331.326928	149694.531006	35.973197
1332.908303	149946.806579	35.978215
1334.491431	150236.370931	35.983232
1335.352918	150510.608917	35.988250
1336.913452	150774.409631	35.993268
1338.151795	151044.644969	35.998285
1339.214531	151304.257414	36.003303
1340.617944	151562.496384	36.008320
1342.489653	151804.615461	36.013338
1344.015891	152064.384989	36.018356
1344.866624	152340.502663	36.023373
1346.136577	152597.743423	36.028391
1347.317141	152869.954732	36.033408
1348.693302	153132.331172	36.038426
1350.132599	153405.848108	36.043444
1350.966191	153677.856115	36.048461
1352.695327	153941.714643	36.053479
1353.819091	154216.697397	36.058496
1355.327444	154503.351546	36.063514
1357.123389	154774.853365	36.068532
1357.896660	155075.953673	36.073549
1359.370741	155345.736814	36.078567
1360.454495	155635.247349	36.083584
1361.866991	155918.211234	36.088602
1363.437658	156204.144675	36.093620
1364.665011	156489.071340	36.098637
1366.137811	156766.196381	36.103655
1367.806248	157054.073375	36.108672
1369.266059	157346.997533	36.113690
1371.008581	157627.712073	36.118708
1372.282391	157923.652227	36.123725
1373.776666	158207.887621	36.128743
1375.761452	158487.553426	36.133760
1376.902400	158765.013619	36.138778
1378.146016	159038.792629	36.143796
1379.090780	159319.511195	36.148813
1380.780797	159611.005874	36.153831
1382.219605	159905.411138	36.158848
1383.485073	160188.252111	36.163866
1385.196463	160466.124618	36.168884
1386.329864	160756.184366	36.173901
1387.743319	161046.352191	36.178919
1389.613471	161321.667058	36.183936
1390.876935	161603.236833	36.188954
1392.344947	161887.071043	36.193972
1393.597427	162178.745060	36.198989
1394.891655	162468.206747	36.204007
1396.897759	162730.288987	36.209024
1398.029899	163020.643969	36.214042
1399.581975	163306.732270	36.219060
1400.693514	163605.721864	36.224077
1401.951447	163885.722103	36.229095
1403.155270	164186.058112	36.234112
1404.588945	164477.527926	36.239130
1406.030777	164783.525507	36.244148
1407.034120	165079.726756	36.249165
1408.182492	165374.408985	36.254183
1409.648883	165682.312092	36.259200
1410.665331	166000.962093	36.264218
1412.527657	166299.339177	36.269236
1413.568089	166617.533001	36.274253
1414.576681	166927.043084	36.279271
1416.262598	167248.497338	36.284288
1417.369746	167565.342126	36.289306
1419.119929	167883.631062	36.294324
1420.172976	168208.457694	36.299341
1421.201496	168536.132992	36.304359
1422.632004	168863.490599	36.309376
1423.848787	169200.618132	36.314394
1425.507754	169529.554395	36.319412
1426.723535	169870.404961	36.324429
1428.461144	170193.090164	36.329447
1430.476796	170520.908939	36.334464
1431.867925	170835.331859	36.339482
1433.717845	171139.377557	36.344500
1434.880049	171448.906366	36.349517
1436.262341	171738.605431	36.354535
1438.432503	172030.447728	36.359552
1439.733022	172338.779583	36.364570
1441.437878	172626.146869	36.369588
1443.035301	172919.345571	36.374605
1443.993571	173223.628302	36.379623
1445.554467	173521.278259	36.384640
1446.812838	173832.050728	36.389658
1448.053228	174135.912120	36.394676
1449.158323	174445.444918	36.399693
1450.323593	174768.662585	36.404711
1451.991156	175078.639680	36.409728
1452.872452	175417.187770	36.414746
1454.147161	175744.302629	36.419764
1455.648421	176073.044794	36.424781
1456.841908	176412.639756	36.429799
1458.139925	176760.253106	36.434816
1459.730470	177108.290225	36.439834
1461.385792	177453.032172	36.444852
1462.736404	177802.129086	36.449869
1464.222724	178136.243229	36.454887
1466.535069	178472.672721	36.459904
1467.981284	178815.466157	36.464922
1469.352507	179155.177621	36.469940
1470.732764	179502.162111	36.474957
1471.958631	179852.195060	36.479975
1473.730593	180203.117572	36.484992
1474.722106	180557.509224	36.490010
1476.147316	180909.318785	36.495028
1477.939756	181263.875074	36.500045
1479.886402	181615.971493	36.505063
1481.759566	181955.644188	36.510080
1483.387465	182298.291469	36.515098
1485.254342	182628.463159	36.520116
1487.118011	182969.311709	36.525133
1488.763911	183302.671801	36.530151
1490.731330	183623.999229	36.535168
1492.144657	183952.984806	36.540186
1493.526712	184273.206955	36.545204
1495.123187	184603.334038	36.550221
1496.379836	184930.422181	36.555239
1497.911976	185263.952903	36.560256
1499.393941	185611.265814	36.565274
1500.990641	185922.780340	36.570292
1503.205273	186253.208944	36.575309
1504.147382	186586.350075	36.580327
1505.951187	186900.882333	36.585344
1507.138500	187232.869887	36.590362
1508.461605	187547.789767	36.595380
1509.963647	187876.974747	36.600397
1511.114839	188207.171565	36.605415
1512.942728	188536.788986	36.610432
1514.273148	188873.535415	36.615450
1515.374771	189196.637699	36.620468
1516.970340	189534.702505	36.625485
1518.667379	189876.027586	36.630503
1520.214543	190194.238262	36.635520
1521.640851	190536.525875	36.640538
1523.281258	190875.784350	36.645556
1524.611361	191215.413347	36.650573
1526.074297	191552.115390	36.655591
1527.986890	191896.869539	36.660608
1529.305011	192241.000196	36.665626
1530.628547	192576.144230	36.670644
1531.975668	192905.510210	36.675661
1533.325899	193237.568736	36.680679
1534.732852	193569.505465	36.685696
1536.405587	193894.773470	36.690714
1537.872651	194232.797374	36.695732
1539.305551	194540.500619	36.700749
1540.737366	194873.227372	36.705767
1542.365010	195203.676567	36.710784
1543.733146	195544.402591	36.715802
1545.421091	195874.642250	36.720820
1546.894408	196217.868205	36.725837
1547.967849	196560.247932	36.730855
1550.143166	196903.437918	36.735872
1551.359539	197251.561461	36.740890
1552.921665	197586.591528	36.745908
1554.436674	197938.935184	36.750925
1555.697073	198305.821197	36.755943
1557.425909	198652.674277	36.760960
1558.964646	199020.597480	36.765978
1560.542352	199380.721027	36.770996
1561.798161	199740.201353	36.776013
1563.530342	200111.323408	36.781031
1565.561872	200450.048517	36.786048
1567.228795	200820.651986	36.791066
1569.040529	201181.965338	36.796084
1571.198339	201537.078489	36.801101
1572.338323	201899.522136	36.806119
1573.956134	202243.669492	36.811136
1575.739355	202619.735542	36.816154
1576.863441	202965.224843	36.821172
1578.662717	203337.495795	36.826189
1580.373588	203696.667626	36.831207
1581.988592	204053.000306	36.836224
1583.220180	204427.732159	36.841242
1584.610641	204804.229980	36.846260
1585.889557	205174.653618	36.851277
1587.560873	205549.978886	36.856295
1589.488024	205899.247601	36.861312
1591.179015	206294.609295	36.866330
1592.629743	206679.321689	36.871348
1593.925457	207051.148524	36.876365
1595.444581	207430.393614	36.881383
1597.551491	207797.646168	36.886400
1599.150137	208186.620719	36.891418
1600.450242	208568.434296	36.896436
1602.285499	208957.640278	36.901453
1603.568029	209338.266906	36.906471
1605.888380	209717.390855	36.911488
1607.033617	210113.776220	36.916506
1608.345352	210489.971968	36.921524
1610.031025	210882.589547	36.926541
1611.183578	211279.030143	36.931559
1613.014103	211672.897362	36.936576
1614.586171	212077.932548	36.941594
1616.321417	212452.492749	36.946612
1618.519259	212851.409492	36.951629
1619.455810	213259.323350	36.956647
1621.586732	213651.296224	36.961664
1622.836207	214060.051086	36.966682
1624.278817	214463.214090	36.971700
1625.718119	214869.325506	36.976717
1626.922240	215276.671223	36.981735
1628.935744	215683.859834	36.986752
1630.885217	216079.530497	36.991770
1632.587031	216494.139323	36.996788
1634.492252	216883.852359	37.001805
1636.051294	217301.942379	37.006823
1637.754651	217690.219000	37.011840
1639.385928	218105.659280	37.016858
1640.289339	218548.371753	37.021876
1642.145593	218939.193356	37.026893
1644.008048	219326.358166	37.031911
1645.637204	219700.152748	37.036928
1647.013301	220091.947043	37.041946
1648.576276	220484.626362	37.046964
1650.601788	220865.268204	37.051981
1652.244186	221256.388064	37.056999
1654.338873	221641.618479	37.062016
1655.842122	222027.887639	37.067034
1657.390321	222407.445496	37.072052
1658.909552	222781.040730	37.077069
1660.542523	223184.106724	37.082087
1662.702870	223555.668510	37.087104
1664.992994	223938.055581	37.092122
1666.774773	224313.212842	37.097140
1669.676050	224697.279611	37.102157
1670.818663	225067.185553	37.107175
1672.710903	225434.708445	37.112192
1674.174151	225811.523323	37.117210
1675.815689	226193.770918	37.122228
1676.995963	226560.119396	37.127245
1678.452357	226938.234351	37.132263
1680.137136	227335.540528	37.137280
1680.966110	227732.201780	37.142298
1682.444418	228135.665979	37.147316
1683.950680	228535.926434	37.152333
1685.431035	228944.295087	37.157351
1686.820972	229365.964307	37.162368
1688.372641	229808.131717	37.167386
1690.121939	230236.500925	37.172404
1691.636797	230655.969172	37.177421
1693.705228	231083.729580	37.182439
1695.370596	231517.450767	37.187456
1697.296996	231933.400467	37.192474
1698.905653	232365.457142	37.197492
1700.521245	232796.599522	37.202509
1702.405336	233241.974231	37.207527
1703.309953	233685.682977	37.212544
1705.613748	234127.028475	37.217562
1707.020575	234574.136883	37.222580
1709.261913	235000.127399	37.227597
1711.156816	235444.693800	37.232615
1712.654606	235882.595543	37.237632
1714.909994	236310.898689	37.242650
1716.780233	236756.514125	37.247668
1718.465615	237201.653177	37.252685
1719.677410	237635.186705	37.257703
1721.734259	238076.278598	37.262720
1723.240219	238512.915514	37.267738
1724.497166	238972.126002	37.272756
1726.599279	239419.564074	37.277773
1728.322607	239861.121599	37.282791
1730.538095	240304.504064	37.287808
1732.146074	240737.039414	37.292826
1733.920056	241190.759082	37.297844
1736.072000	241617.160790	37.302861
1737.695402	242061.990965	37.307879
1739.548217	242507.444642	37.312896
1741.605917	242928.936363	37.317914
1743.081870	243363.607059	37.322932
1744.998223	243800.466706	37.327949
1746.616979	244253.989459	37.332967
1748.149034	244693.276503	37.337984
1749.548340	245126.768998	37.343002
1751.395686	245549.976426	37.348020
1753.858996	245992.414315	37.353037
1755.557814	246426.189681	37.358055
1757.528752	246849.454872	37.363072
1759.146188	247250.475341	37.368090
1760.358843	247666.499956	37.373108
1761.949670	248077.788600	37.378125
1763.964709	248495.663324	37.383143
1765.626682	248910.827888	37.388160
1767.498461	249337.135613	37.393178
1768.962409	249767.169138	37.398196
1770.648124	250184.033216	37.403213
1772.076474	250622.761374	37.408231
1773.930229	251055.373891	37.413248
1775.160491	251483.440935	37.418266
1776.816261	251930.846140	37.423284
1778.481011	252373.398285	37.428301
1780.128190	252838.867339	37.433319
1781.860160	253293.907513	37.438336
1783.801951	253756.890031	37.443354
1785.519261	254226.336938	37.448372
1787.313808	254681.291609	37.453389
1789.395611	255150.882245	37.458407
1790.917761	255609.235646	37.463424
1792.941198	256093.621140	37.468442
1794.603512	256565.618857	37.473460
1796.278894	257042.288831	37.478477
1798.171096	257516.205072	37.483495
1800.106486	258000.301068	37.488512
1802.052777	258464.987285	37.493530
1803.804276	258947.716681	37.498548
1805.463204	259430.359818	37.503565
1807.938780	259906.161819	37.508583
1809.777001	260388.750060	37.513600
1811.890411	260858.896092	37.518618
1813.007608	261340.079055	37.523636
1815.435802	261813.500916	37.528653
1817.356373	262301.029062	37.533671
1818.818049	262782.637621	37.538688
1821.032323	263260.108176	37.543706
1822.264477	263759.943048	37.548724
1824.120848	264241.587618	37.553741
1825.811091	264736.240438	37.558759
1827.285073	265238.956096	37.563776
1829.497830	265733.090314	37.568794
1831.023271	266226.296063	37.573812
1832.664655	266723.546850	37.578829
1834.624952	267233.471632	37.583847
1835.829713	267760.667734	37.588864
1837.952815	268282.173967	37.593882
1839.724977	268803.889986	37.598900
1841.230880	269313.659122	37.603917
1843.357632	269832.622788	37.608935
1845.208502	270359.328452	37.613952
1847.474139	270881.798933	37.618970
1849.416679	271394.999137	37.623988
1851.430121	271908.745800	37.629005
1853.617678	272417.458636	37.634023
1855.422168	272932.178161	37.639040
1857.602104	273425.471203	37.644058
1859.936128	273929.330995	37.649076
1862.304480	274428.129148	37.654093
1864.198004	274922.864140	37.659111
1866.694430	275410.665509	37.664128
1869.438734	275873.530602	37.669146
1871.450238	276339.868897	37.674164
1873.701374	276806.141412	37.679181
1875.050237	277256.634568	37.684199
1876.731593	277730.239010	37.689216
1878.627866	278202.130496	37.694234
1879.980520	278665.702532	37.699252
1881.590592	279127.071957	37.704269
1883.196761	279565.909329	37.709287
1884.446811	280035.515696	37.714304
1886.173500	280486.371870	37.719322
1887.798169	280957.336855	37.724340
1889.702874	281432.039420	37.729357
1891.725728	281887.314305	37.734375
1893.349655	282367.471474	37.739392
1895.301634	282834.161170	37.744410
1896.980712	283330.157419	37.749428
1898.465400	283815.795096	37.754445
1900.618737	284297.079072	37.759463
1902.051654	284793.340382	37.764480
1903.804569	285294.856328	37.769498
1905.307954	285810.916046	37.774516
1907.592248	286317.167434	37.779533
1909.379761	286813.922908	37.784551
1911.119323	287333.647254	37.789568
1913.228494	287850.717954	37.794586
1914.508311	288391.038457	37.799604
1916.311316	288913.185305	37.804621
1918.431406	289447.952892	37.809639
1920.132760	289993.328761	37.814656
1922.069837	290537.063363	37.819674
1924.167616	291079.143652	37.824692
1926.011387	291632.541358	37.829709
1928.862844	292162.021346	37.834727
1931.085114	292701.153363	37.839744
1933.213741	293224.829952	37.844762
1935.363408	293764.477374	37.849780
1937.519079	294291.015162	37.854797
1939.480764	294825.812127	37.859815
1941.003840	295374.242366	37.864832
1942.925136	295906.983722	37.869850
1944.649712	296448.086020	37.874868
1946.905462	296996.159086	37.879885
1948.996994	297525.461268	37.884903
1950.551715	298086.496477	37.889920
1952.741483	298622.025269	37.894938
1954.924051	299167.610427	37.899956
1956.170936	299724.090661	37.904973
1958.599305	300268.613595	37.909991
1960.670038	300823.910678	37.915008
1962.279662	301370.873996	37.920026
1964.358872	301931.166979	37.925044
1966.096239	302497.151466	37.930061
1968.350251	303058.348870	37.935079
1969.888810	303636.270959	37.940096
1972.035583	304193.923701	37.945114
1973.640806	304771.903995	37.950132
1975.295306	305338.901015	37.955149
1977.530611	305912.986017	37.960167
1979.806600	306485.232072	37.965184
1981.685317	307067.419213	37.970202
1983.871892	307642.212152	37.975220
1985.470070	308218.520504	37.980237
1987.892449	308788.720960	37.985255
1989.737995	309367.596505	37.990272
1992.101357	309935.284711	37.995290
1994.652969	310503.369683	38.000308
1996.232152	311068.868386	38.005325
1998.418355	311643.684605	38.010343
2000.200764	312223.667664	38.015360
2002.394296	312791.312969	38.020378
2004.220687	313359.395612	38.025396
2006.335376	313936.187589	38.030413
2008.550815	314494.141476	38.035431
2010.725335	315051.031437	38.040448
2012.938577	315579.545937	38.045466
2015.051185	316111.577586	38.050484
2016.955575	316646.204455	38.055501
2019.317954	317181.666008	38.060519
2021.274900	317703.249628	38.065536
2022.768646	318230.416088	38.070554
2025.047579	318770.602542	38.075572
2026.725476	319311.061700	38.080589
2028.970457	319846.954064	38.085607
2030.359408	320404.135071	38.090624
2032.314012	320954.844852	38.095642
2034.934039	321495.613796	38.100660
2037.154233	322046.220034	38.105677
2039.656888	322579.382073	38.110695
2041.419759	323131.501976	38.115712
2043.270799	323682.637800	38.120730
2045.603513	324234.857443	38.125748
2046.603245	324803.719764	38.130765
2048.763315	325358.319444	38.135783
2050.342017	325934.109173	38.140800
2052.122230	326508.743198	38.145818
2054.127962	327102.046731	38.150836
2055.443564	327700.866239	38.155853
2057.687481	328299.196676	38.160871
2059.238266	328916.397738	38.165888
2060.796990	329528.386463	38.170906
2062.804914	330152.481092	38.175924
2065.077323	330784.395698	38.180941
2067.049551	331404.649222	38.185959
2069.121069	332038.817339	38.190976
2071.367657	332677.011454	38.195994
2074.154719	333319.348811	38.201012
2075.818349	333961.305569	38.206029
2078.332833	334589.659888	38.211047
2080.352773	335230.959244	38.216064
2082.470482	335868.680948	38.221082
2084.916681	336509.641044	38.226100
2086.731906	337155.495300	38.231117
2088.836732	337792.790078	38.236135
2090.970391	338445.303023	38.241152
2092.743690	339088.221311	38.246170
2095.548854	339730.529928	38.251188
2097.513674	340385.356220	38.256205
2099.908331	341017.867620	38.261223
2102.206673	341666.530447	38.266240
2104.398590	342309.389860	38.271258
2106.713180	342943.844640	38.276276
2108.661449	343586.499243	38.281293
2111.128643	344219.770227	38.286311
2113.333120	344866.807488	38.291328
2115.490804	345505.163563	38.296346
2118.030584	346136.722299	38.301364
2119.706030	346775.623144	38.306381
2122.237571	347397.471229	38.311399
2124.522843	348042.421585	38.316416
2126.577557	348688.568459	38.321434
2128.419555	349304.794473	38.326452
2130.241656	349953.423688	38.331469
2132.270508	350587.493341	38.336487
2134.602397	351239.471509	38.341504
2136.448715	351873.603915	38.346522
2138.847917	352515.985132	38.351540
2140.946584	353169.191623	38.356557
2142.830395	353819.277189	38.361575
2145.022078	354458.339955	38.366592
2147.300500	355110.371209	38.371610
2149.213519	355748.902572	38.376628
2150.998446	356391.708465	38.381645
2153.573152	357017.779605	38.386663
2155.265241	357643.682516	38.391680
2157.085108	358276.431236	38.396698
2159.295715	358892.587989	38.401716
2161.143161	359545.306851	38.406733
2163.351830	360166.722416	38.411751
2165.443945	360816.970299	38.416768
2167.853613	361454.697962	38.421786
2170.189072	362069.213163	38.426804
2172.373696	362723.804253	38.431821
2175.059046	363371.731090	38.436839
2177.118341	364021.881629	38.441856
2179.114838	364659.879780	38.446874
2181.437349	365293.145839	38.451892
2183.362368	365951.632844	38.456909
2185.668948	366600.507236	38.461927
2187.942920	367257.823507	38.466944
2189.798594	367925.775610	38.471962
2191.912095	368580.584094	38.476980
2193.629541	369252.746431	38.481997
2195.770919	369931.269751	38.487015
2198.253687	370603.103988	38.492032
2200.501361	371279.200744	38.497050
2202.953156	371944.090964	38.502068
2205.210454	372635.354491	38.507085
2207.204584	373322.082787	38.512103
2209.643184	374009.130521	38.517120
2212.181371	374708.880725	38.522138
2213.892304	375390.315290	38.527156
2215.409106	376093.326190	38.532173
2218.046625	376788.783501	38.537191
2220.305589	377495.219852	38.542208
2222.776429	378208.124467	38.547226
2225.146669	378905.713748	38.552244
2226.847815	379606.366208	38.557261
2228.998966	380333.531238	38.562279
2231.848804	381047.252508	38.567296
2233.749094	381762.763489	38.572314
2236.608614	382467.653964	38.577332
2238.450506	383189.559351	38.582349
2241.031773	383889.191423	38.587367
2243.694560	384608.420218	38.592384
2245.713445	385317.267877	38.597402
2248.219961	386019.224771	38.602420
2250.523132	386735.524799	38.607437
2252.706583	387437.098484	38.612455
2255.283285	388149.594956	38.617472
2257.492595	388867.307865	38.622490
2259.518575	389583.361543	38.627508
2261.476935	390311.806633	38.632525
2263.723112	391018.259373	38.637543
2265.773950	391761.561321	38.642560
2267.684692	392500.939426	38.647578
2270.014308	393231.738987	38.652596
2272.240958	393976.073806	38.657613
2274.739002	394703.058894	38.662631
2277.369382	395435.378176	38.667648
2279.567738	396170.234783	38.672666
2282.196591	396890.859671	38.677684
2284.651983	397621.785681	38.682701
2286.731694	398345.938037	38.687719
2289.229910	399071.752289	38.692736
2291.275815	399817.922758	38.697754
2293.252986	400544.724032	38.702772
2295.533971	401282.404547	38.707789
2297.899782	402013.336870	38.712807
2300.558027	402752.742019	38.717824
2302.231590	403484.131022	38.722842
2304.792686	404196.680040	38.727860
2306.280213	404919.042000	38.732877
2308.740378	405631.216650	38.737895
2311.230928	406331.383741	38.742912
2313.524200	407035.290194	38.747930
2315.580694	407750.821569	38.752948
2318.442689	408476.867620	38.757965
2320.530328	409200.184672	38.762983
2322.631829	409931.232388	38.768000
2324.662618	410659.434784	38.773018
2326.690469	411399.524246	38.778036
2328.901890	412138.803123	38.783053
2331.291529	412899.031531	38.788071
2333.855296	413630.789021	38.793088
2335.615512	414391.255803	38.798106
2338.107884	415138.256998	38.803124
2340.609476	415909.803599	38.808141
2342.458098	416680.852524	38.813159
2344.871656	417446.416188	38.818176
2347.069046	418247.702137	38.823194
2349.513389	419020.330505	38.828212
2352.194301	419798.366559	38.833229
2354.764327	420574.928352	38.838247
2357.916798	421346.609639	38.843264
2360.304976	422131.256823	38.848282
2362.541275	422903.775701	38.853300
2364.841514	423690.388855	38.858317
2367.265153	424476.095888	38.863335
2369.768430	425244.016411	38.868352
2371.945847	426044.677404	38.873370
2374.405599	426842.531419	38.878388
2376.900781	427623.695384	38.883405
2379.096159	428427.515581	38.888423
2381.531533	429224.788905	38.893440
2383.813622	430032.692785	38.898458
2386.003148	430834.509529	38.903476
2388.572176	431636.894780	38.908493
2390.954979	432444.851980	38.913511
2393.313816	433257.796848	38.918528
2395.149480	434079.404966	38.923546
2397.714558	434894.030606	38.928564
2400.197544	435719.472844	38.933581
2402.001494	436538.772106	38.938599
2404.699707	437375.710007	38.943616
2407.208940	438218.417958	38.948634
2409.319105	439055.796099	38.953652
2411.712585	439907.671098	38.958669
2413.952683	440757.768078	38.963687
2416.912009	441589.750557	38.968704
2419.399348	442431.697507	38.973722
2422.240035	443271.682190	38.978740
2424.772621	444112.394138	38.983757
2427.139636	444949.357317	38.988775
2429.832726	445790.585748	38.993792
2432.125806	446637.918566	38.998810
2434.477677	447476.001538	39.003828
2437.063965	448325.091846	39.008845
2439.370568	449172.323147	39.013863
2441.765275	450001.903693	39.018880
2444.028376	450850.997792	39.023898
2446.030607	451708.851043	39.028916
2448.714660	452564.786904	39.033933
2451.000358	453421.663963	39.038951
2453.463449	454266.339362	39.043968
2455.684433	455138.480134	39.048986
2458.334529	455999.590807	39.054004
2461.044380	456848.165931	39.059021
2463.341505	457698.088761	39.064039
2466.376092	458528.540102	39.069056
2468.618444	459345.083145	39.074074
2471.189407	460161.690861	39.079092
2473.999391	460973.625621	39.084109
2476.680194	461807.438723	39.089127
2478.721529	462614.782959	39.094144
2481.074813	463442.616838	39.099162
2483.402909	464258.289016	39.104180
2485.857751	465081.943439	39.109197
2487.746602	465924.155625	39.114215
2490.116937	466764.533940	39.119232
2492.357735	467607.020147	39.124250
2495.334870	468440.504605	39.129268
2498.217714	469294.839564	39.134285
2500.704856	470139.044985	39.139303
2503.540840	470975.071042	39.144320
2506.432413	471844.399842	39.149338
2508.547944	472688.453147	39.154356
2511.592183	473539.389132	39.159373
2513.894369	474381.770084	39.164391
2516.743690	475223.467490	39.169408
2519.375981	476090.219113	39.174426
2521.959671	476946.280086	39.179444
2524.658107	477786.725140	39.184461
2527.110730	478640.961736	39.189479
2529.738656	479503.261586	39.194496
2531.964523	480356.849968	39.199514
2534.216511	481213.575941	39.204532
2536.957299	482067.555119	39.209549
2539.621711	482934.585671	39.214567
2542.104534	483797.716502	39.219584
2544.853156	484676.515967	39.224602
2547.380886	485544.958327	39.229620
2549.715617	486423.134509	39.234637
2552.510292	487309.723621	39.239655
2554.832675	488169.994238	39.244672
2557.210522	489068.377026	39.249690
2559.469362	489955.578009	39.254708
2562.254612	490825.586698	39.259725
2564.654651	491737.911676	39.264743
2567.200509	492632.096513	39.269760
2570.007530	493532.803389	39.274778
2572.726021	494435.143188	39.279796
2575.511263	495332.428867	39.284813
2577.685145	496240.667548	39.289831
2580.448740	497130.999869	39.294848
2582.867278	498055.752113	39.299866
2585.314932	498957.392762	39.304884
2587.964307	499867.175057	39.309901
2590.309008	500806.973559	39.314919
2592.289969	501723.625864	39.319936
2594.995917	502653.626206	39.324954
2597.748049	503580.086616	39.329972
2600.706629	504514.278404	39.334989
2603.050667	505456.184076	39.340007
2605.639850	506374.495407	39.345024
2608.742795	507299.477914	39.350042
2611.029485	508231.198212	39.355060
2613.382006	509161.442322	39.360077
2616.123885	510111.080110	39.365095
2618.840811	511049.070640	39.370112
2621.572374	512004.093237	39.375130
2624.365418	512945.186254	39.380148
2627.207264	513880.973336	39.385165
2629.976526	514811.727226	39.390183
2632.777169	515736.574678	39.395200
2635.673580	516666.845098	39.400218
2638.238523	517587.741684	39.405236
2641.251123	518473.438315	39.410253
2643.929786	519360.197632	39.415271
2646.350826	520233.495878	39.420288
2649.326504	521121.415172	39.425306
2652.240444	521989.796664	39.430324
2654.924585	522859.627712	39.435341
2657.408002	523738.257612	39.440359
2659.796330	524606.778363	39.445376
2662.696513	525499.593221	39.450394
2665.021752	526391.493157	39.455412
2667.088960	527278.648813	39.460429
2669.486101	528187.301423	39.465447
2671.970383	529091.906372	39.470464
2674.120726	530011.113608	39.475482
2676.321418	530947.726783	39.480500
2679.128132	531886.597373	39.485517
2681.255059	532830.403441	39.490535
2683.681200	533792.171387	39.495552
2686.457343	534738.717605	39.500570
2689.373525	535697.007492	39.505588
2692.066444	536661.964772	39.510605
2694.572127	537637.859659	39.515623
2697.582551	538620.147250	39.520640
2700.194431	539595.187401	39.525658
2702.743142	540591.052574	39.530676
2705.304337	541579.651509	39.535693
2707.908915	542593.177909	39.540711
2710.179962	543601.253778	39.545728
2712.876519	544615.575741	39.550746
2715.653307	545643.492237	39.555764
2717.911504	546673.531068	39.560781
2720.484880	547723.910003	39.565799
2723.207197	548764.580265	39.570816
2726.025169	549808.022613	39.575834
2728.907868	550866.810906	39.580852
2731.523758	551931.996729	39.585869
2734.076853	552990.172581	39.590887
2737.232342	554059.627878	39.595904
2739.740774	555121.917957	39.600922
2742.672383	556197.122228	39.605940
2745.780065	557264.271376	39.610957
2748.510101	558338.433069	39.615975
2751.752684	559404.133242	39.620992
2754.724905	560461.351883	39.626010
2757.513797	561551.322579	39.631028
2760.732199	562598.834888	39.636045
2763.447361	563676.133744	39.641063
2766.352983	564742.614495	39.646080
2769.041196	565810.450327	39.651098
2771.596326	566878.722756	39.656116
2774.570555	567936.694892	39.661133
2777.401210	569016.345175	39.666151
2779.988264	570092.832371	39.671168
2782.726006	571153.892917	39.676186
2785.622555	572235.621097	39.681204
2788.369449	573300.969285	39.686221
2790.577839	574391.762737	39.691239
2793.521464	575467.185189	39.696256
2796.262397	576562.069507	39.701274
2798.811964	577634.962972	39.706292
2801.609894	578736.572308	39.711309
2804.188619	579842.986679	39.716327
2806.804233	580941.019584	39.721344
2810.188657	582038.176329	39.726362
2813.292034	583133.827318	39.731380
2816.121512	584224.561265	39.736397
2818.933005	585322.572332	39.741415
2822.203369	586403.812473	39.746432
2825.110772	587458.694821	39.751450
2827.751917	588506.911814	39.756468
2830.675123	589545.818010	39.761485
2833.736977	590586.817089	39.766503
2837.510235	591600.343920	39.771520
2840.636331	592621.308421	39.776538
2842.996789	593674.231847	39.781556
2845.425044	594690.072676	39.786573
2848.486556	595721.604169	39.791591
2850.896853	596781.658027	39.796608
2853.931579	597807.350306	39.801626
2856.512746	598844.247331	39.806644
2859.512442	599897.961737	39.811661
2861.841103	600945.231164	39.816679
2864.717473	602011.294114	39.821696
2867.395774	603073.486140	39.826714
2870.512027	604158.738427	39.831732
2873.212808	605233.694268	39.836749
2876.007494	606313.489263	39.841767
2878.454914	607401.697964	39.846784
2881.321466	608499.742749	39.851802
2883.958670	609611.480344	39.856820
2886.598271	610712.550483	39.861837
2889.860467	611827.118986	39.866855
2892.730225	612953.747853	39.871872
2895.431263	614064.534288	39.876890
2898.250005	615208.901669	39.881908
2901.408692	616338.891960	39.886925
2904.024382	617466.406077	39.891943
2906.847219	618612.971193	39.896960
2909.730621	619759.056788	39.901978
2912.662759	620927.610124	39.906996
2915.230084	622080.353232	39.912013
2918.373116	623250.922031	39.917031
2921.209133	624416.417619	39.922048
2924.399989	625600.117562	39.927066
2927.233656	626777.001189	39.932084
2930.279777	627954.270270	39.937101
2933.627552	629126.864318	39.942119
2936.426492	630300.968123	39.947136
2939.632805	631471.079459	39.952154
2942.767114	632657.102673	39.957172
2946.071330	633836.423673	39.962189
2949.281268	635012.432713	39.967207
2952.028130	636183.044707	39.972224
2955.927081	637350.240974	39.977242
2958.830443	638503.645879	39.982260
2962.061056	639675.881331	39.987277
2965.013817	640836.154236	39.992295
2967.574092	642022.354291	39.997312
2970.480456	643171.794475	40.002330
2973.914943	644357.380708	40.007348
2976.213349	645524.712675	40.012365
2978.807477	646702.932580	40.017383
2981.634417	647877.038013	40.022400
2984.759646	649055.594430	40.027418
2987.709600	650255.477409	40.032436
2990.605125	651436.334789	40.037453
2993.661929	652628.489006	40.042471
2996.424962	653827.027242	40.047488
2999.642732	655029.780485	40.052506
3001.992183	656220.225009	40.057524
3005.270338	657423.922424	40.062541
3008.546963	658614.024489	40.067559
3011.619298	659827.572179	40.072576
3014.363153	661021.602778	40.077594
3017.292024	662231.837378	40.082612
3020.314946	663418.805903	40.087629
3023.258181	664600.365476	40.092647
3025.987038	665779.277240	40.097664
3029.046519	666935.495894	40.102682
3031.640867	668115.635780	40.107700
3034.493764	669279.367657	40.112717
3038.341325	670448.166119	40.117735
3041.202598	671639.316904	40.122752
3043.868793	672810.207261	40.127770
3047.179215	673991.985347	40.132788
3050.055587	675182.785596	40.137805
3053.164617	676376.528328	40.142823
3056.076619	677577.756568	40.147840
3058.819770	678779.106213	40.152858
3061.530353	679994.717822	40.157876
3064.423168	681213.816803	40.162893
3067.561201	682435.347495	40.167911
3070.051586	683677.984963	40.172928
3073.356518	684929.459048	40.177946
3076.235632	686170.402557	40.182964
3079.767339	687427.456052	40.187981
3083.468928	688671.448193	40.192999
3086.461449	689931.122815	40.198016
3089.754538	691163.421163	40.203034
3093.574143	692426.382652	40.208052
3096.688502	693675.338513	40.213069
3099.557257	694924.705936	40.218087
3102.838142	696185.587216	40.223104
3106.169020	697443.503428	40.228122
3109.414230	698719.455776	40.233140
3112.292173	699965.581550	40.238157
3115.812877	701221.538990	40.243175
3119.237493	702477.431321	40.248192
3122.340340	703728.437751	40.253210
3125.613342	704993.905604	40.258228
3128.721993	706244.796628	40.263245
3131.878278	707500.354208	40.268263
3134.726942	708778.516934	40.273280
3137.373519	710052.362451	40.278298
3140.545441	711338.262961	40.283316
3143.937163	712616.159905	40.288333
3147.464170	713894.090264	40.293351
3150.439611	715167.117603	40.298368
3153.998015	716453.071678	40.303386
3157.187047	717727.162700	40.308404
3160.298945	719013.937305	40.313421
3163.713649	720290.273772	40.318439
3166.733265	721567.222236	40.323456
3169.704367	722847.543588	40.328474
3173.064320	724129.680173	40.333492
3176.789152	725426.142415	40.338509
3179.459006	726708.338587	40.343527
3182.608574	727993.418928	40.348544
3185.732489	729273.360511	40.353562
3188.842380	730568.667392	40.358580
3191.954414	731875.129944	40.363597
3194.922762	733164.464616	40.368615
3197.553765	734479.872436	40.373632
3200.543061	735788.637398	40.378650
3203.754591	737107.569474	40.383668
3206.813988	738422.163519	40.388685
3210.187968	739745.767686	40.393703
3213.395425	741093.653693	40.398720
3216.578154	742414.871653	40.403738
3219.689560	743746.584839	40.408756
3222.479656	745076.597478	40.413773
3225.990090	746407.203601	40.418791
3228.674220	747771.245154	40.423808
3232.313398	749084.612759	40.428826
3235.413515	750383.900320	40.433844
3238.138705	751690.768888	40.438861
3241.631683	752980.982803	40.443879
3245.032187	754291.340853	40.448896
3248.190596	755591.911797	40.453914
3251.534863	756897.500881	40.458932
3254.683670	758196.154339	40.463949
3257.988064	759507.556996	40.468967
3261.176097	760816.833325	40.473984
3264.114632	762141.770231	40.479002
3267.692572	763458.251615	40.484020
3270.202307	764780.680567	40.489037
3273.785091	766128.078781	40.494055
3277.192858	767457.511601	40.499072
3280.462898	768804.676061	40.504090
3283.678375	770161.584700	40.509108
3286.661967	771519.758051	40.514125
3289.788170	772873.039736	40.519143
3292.975912	774263.745533	40.524160
3296.277762	775631.230547	40.529178
3299.469664	777011.836940	40.534196
3302.723848	778408.621478	40.539213
3306.381274	779805.759231	40.544231
3309.829961	781192.453501	40.549248
3312.985766	782596.793262	40.554266
3316.178905	784006.888616	40.559284
3319.103844	785435.686794	40.564301
3322.268168	786842.924909	40.569319
3325.994146	788283.725574	40.574336
3329.133280	789712.516840	40.579354
3332.957036	791136.545817	40.584372
3336.197071	792576.605323	40.589389
3339.839919	794022.674189	40.594407
3343.077188	795445.930873	40.599424
3346.122264	796897.238025	40.604442
3349.508120	798349.656934	40.609460
3352.432551	799813.304660	40.614477
3355.806025	801265.753672	40.619495
3359.479226	802747.943031	40.624512
3362.595032	804219.925845	40.629530
3366.421846	805682.966067	40.634548
3369.510162	807147.332001	40.639565
3373.300218	808622.856248	40.644583
3377.109816	810086.326543	40.649600
3380.432323	811560.020291	40.654618
3383.567032	813033.766515	40.659636
3387.038213	814517.882618	40.664653
3390.472918	815983.656249	40.669671
3394.234100	817458.089151	40.674688
3398.257872	818915.995445	40.679706
3401.853853	820379.168629	40.684724
3405.462903	821842.359254	40.689741
3409.100766	823290.976961	40.694759
3412.930168	824746.415350	40.699776
3415.988863	826211.509308	40.704794
3419.190104	827642.418715	40.709812
3423.045317	829080.024022	40.714829
3427.153531	830525.945158	40.719847
3430.880753	831954.701773	40.724864
3434.166142	833375.228121	40.729882
3437.592256	834808.081082	40.734900
3440.798219	836244.400943	40.739917
3444.147461	837661.879011	40.744935
3448.387892	839077.047538	40.749952
3451.861586	840492.856119	40.754970
3455.771647	841896.652124	40.759988
3459.229870	843307.118446	40.765005
3462.710251	844691.517795	40.770010
3465.638967	846037.017808	40.775015
3468.470812	847323.091399	40.780020
3471.706411	848542.481506	40.785024
3474.227613	849712.750913	40.790029
3477.427254	850819.963739	40.795034
3480.272848	851869.192251	40.800039
3482.865934	852839.222174	40.805044
3485.260067	853736.896291	40.810048
3487.119931	854597.928094	40.815053
3489.577455	855382.728010	40.820058
3491.526428	856118.950678	40.825063
3493.325040	856795.850603	40.830068
3495.423162	857415.708245	40.835072
3496.918674	857985.694067	40.840077
3498.223346	858497.679832	40.845082
3500.050974	858982.106019	40.850087
3501.007480	859409.445520	40.855092
3502.390764	859802.060700	40.860096
3503.802719	860148.645085	40.865101
3505.006637	860442.729775	40.870106
3506.350311	860712.855107	40.875111
3506.655622	860955.912100	40.880116
3507.661484	861154.017563	40.885120
3509.042225	861320.745201	40.890125
3509.570052	861465.634169	40.895130
3510.631908	861578.928955	40.900135
3511.076263	861666.751993	40.905140
3511.839374	861723.797057	40.910144
3512.575792	861766.845158	40.915149
3512.918829	861785.845311	40.920154
3514.206697	861775.813161	40.925159
3514.165366	861753.846405	40.930164
3514.799840	861699.682733	40.935168
3515.153895	861624.076904	40.940173
3515.652518	861558.947326	40.945178
3516.598863	861449.891342	40.950183
3516.927427	861342.490926	40.955188
3517.335798	861209.696695	40.960192
3517.495100	861071.203499	40.965197
3517.665564	860919.383250	40.970202
3517.920322	860755.584331	40.975207
3517.879967	860582.493938	40.980212
3518.293942	860397.848347	40.985216
3518.387537	860197.203230	40.990221
3518.931928	860006.008389	40.995226
3519.074973	859790.753388	41.000231
3518.799806	859587.425770	41.005236
3518.992174	859345.691503	41.010240
3519.321735	859133.106153	41.015245
3519.275885	858895.965087	41.020250
3519.700837	858648.717731	41.025255
3519.727030	858400.553290	41.030260
3519.819253	858152.757092	41.035264
3519.726482	857900.311486	41.040269
3519.714121	857643.074894	41.045274
3519.920658	857376.937410	41.050279
3519.950631	857116.850222	41.055284
3519.827601	856836.245673	41.060288
3520.188103	856554.283668	41.065293
3519.774323	856289.077173	41.070298
3519.899878	856003.820003	41.075303
3520.038634	855718.450159	41.080308
3520.144247	855436.673742	41.085312
3519.920768	855161.557309	41.090317
3520.014718	854867.784966	41.095322
3519.920834	854574.321642	41.100327
3519.804471	854287.857055	41.105332
3520.270773	853998.168025	41.110336
3519.879183	853708.801478	41.115341
3519.684145	853406.245441	41.120346
3519.741415	853118.822010	41.125351
3519.379670	852832.817464	41.130356
3519.261795	852532.348262	41.135360
3519.129003	852242.091743	41.140365
3518.951745	851953.679283	41.145370
3519.031311	851681.377457	41.150375
3518.944497	851386.009313	41.155380
3518.911653	851102.111053	41.160384
3518.832932	850824.148866	41.165389
3518.436197	850533.466616	41.170394
3518.923071	850234.442873	41.175399
3518.340200	849963.344083	41.180404
3518.661550	849674.841541	41.185408
3518.843777	849390.440379	41.190413
3518.593752	849095.575327	41.195418
3518.283824	848816.490240	41.200423
3518.300738	848537.728630	41.205428
3518.335737	848250.474316	41.210432
3518.579163	847965.608649	41.215437
3518.142243	847677.139035	41.220442
3518.204170	847390.815445	41.225447
3517.803223	847118.589053	41.230452
3517.776460	846829.720601	41.235456
3517.541169	846560.464107	41.240461
3517.426362	846278.505001	41.245466
3517.958530	846007.343970	41.250471
3517.330012	845720.668217	41.255476
3517.282038	845454.160505	41.260480
3517.004571	845175.785777	41.265485
3516.909523	844905.948067	41.270490
3516.901066	844632.379697	41.275495
3516.928593	844367.861136	41.280500
3516.996179	844095.134504	41.285504
3516.704444	843827.623286	41.290509
3516.499305	843563.548216	41.295514
3516.337536	843300.917751	41.300519
3516.131717	843044.720055	41.305524
3516.425859	842785.698957	41.310528
3516.102871	842532.620679	41.315533
3516.048108	842275.099148	41.320538
3515.946718	842014.551212	41.325543
3516.055542	841763.126812	41.330548
3516.025811	841509.081588	41.335552
3516.000605	841254.049988	41.340557
3515.682560	841003.592595	41.345562
3515.790995	840741.348339	41.350567
3515.146515	840498.778150	41.355572
3515.562622	840245.340781	41.360576
3515.366794	839992.921036	41.365581
3515.020459	839750.126908	41.370586
3515.066537	839509.991020	41.375591
3515.031168	839271.664732	41.380596
3515.100960	839030.482342	41.385600
3514.867256	838781.338765	41.390605
3514.810957	838542.452024	41.395610
3514.933304	838294.987489	41.400615
3514.356310	838059.389083	41.405620
3514.613238	837831.647931	41.410624
3514.578555	837592.282994	41.415629
3514.438440	837360.100686	41.420634
3514.286260	837119.468557	41.425639
3514.123151	836892.788191	41.430644
3514.211472	836666.888171	41.435648
3513.862341	836439.099823	41.440653
3513.843603	836205.245012	41.445658
3513.900603	835981.815536	41.450663
3513.670095	835763.697806	41.455668
3513.400861	835535.473771	41.460672
3513.489956	835328.614401	41.465677
3512.964195	835105.055215	41.470682
3512.827727	834894.411012	41.475687
3512.502427	834683.009844	41.480692
3513.275672	834482.064852	41.485696
3512.839260	834267.543522	41.490701
3512.801641	834068.818816	41.495706
3513.297119	833844.412971	41.500711
3513.005988	833643.177741	41.505716
3513.093265	833427.663294	41.510720
3513.058283	833222.661419	41.515725
3512.647935	833003.210301	41.520730
3512.797938	832800.557607	41.525735
3512.410654	832592.126261	41.530740
3512.548261	832390.000013	41.535744
3512.219554	832178.224477	41.540749
3512.099730	831995.177162	41.545754
3512.242701	831798.941813	41.550759
3511.943834	831607.804607	41.555764
3511.880892	831408.660530	41.560768
3511.917978	831213.450765	41.565773
3511.660067	831014.375570	41.570778
3511.666709	830827.806037	41.575783
3511.201443	830639.745531	41.580788
3510.671128	830457.015626	41.585792
3511.125775	830289.899323	41.590797
3511.112088	830106.097327	41.595802
3511.126366	829921.650358	41.600807
3510.954415	829751.740715	41.605812
3510.844594	829574.731311	41.610816
3510.785021	829405.038439	41.615821
3510.536132	829226.527706	41.620826
3510.685920	829044.085951	41.625831
3510.247227	828892.376272	41.630836
3510.570168	828715.858711	41.635840
3510.262351	828548.725673	41.640845
3510.370198	828380.933435	41.645850
3510.509447	828230.432731	41.650855
3510.365542	828062.038433	41.655860
3510.399238	827886.963497	41.660864
3510.498359	827713.486035	41.665869
3509.950673	827551.547956	41.670874
3509.969749	827388.192783	41.675879
3509.944528	827234.910178	41.680884
3510.215106	827067.644050	41.685888
3509.674094	826914.829970	41.690893
3509.519824	826761.166486	41.695898
3509.695426	826604.805281	41.700903
3509.448887	826449.145405	41.705908
3509.532200	826297.338489	41.710912
3509.281847	826143.871930	41.715917
3509.307855	825990.551823	41.720922
3509.271329	825847.554367	41.725927
3509.401427	825692.987912	41.730932
3509.072120	825549.298817	41.735936
3509.012577	825401.406167	41.740941
3508.956125	825256.981230	41.745946
3509.117108	825111.686078	41.750951
3508.992668	824980.957170	41.755956
3509.375414	824824.323928	41.760960
3509.153100	824681.185038	41.765965
3508.935802	824536.966406	41.770970
3508.866054	824402.256081	41.775975
3508.638464	824270.698751	41.780980
3508.522806	824121.123927	41.785984
3508.666355	823980.403636	41.790989
3508.325994	823851.839699	41.795994
3508.620581	823699.693578	41.800999
3508.302622	823573.370229	41.806004
3508.426403	823447.607512	41.811008
3508.407890	823312.524152	41.816013
3508.136704	823173.028801	41.821018
3508.217468	823049.857857	41.826023
3508.239171	822925.226980	41.831028
3508.473371	822794.493517	41.836032
3508.518426	822657.625435	41.841037
3508.075189	822547.053477	41.846042
3508.273358	822403.111142	41.851047
3507.902102	822274.423781	41.856052
3507.909668	822150.025226	41.861056
3507.848074	822022.847349	41.866061
3507.869231	821899.371310	41.871066
3508.138437	821776.879452	41.876071
3507.531025	821662.112574	41.881076
3507.568628	821530.995195	41.886080
3507.356803	821413.370266	41.891085
3507.568778	821298.706753	41.896090
3508.003792	821176.959302	41.901095
3507.255918	821047.820914	41.906100
3507.676858	820936.639412	41.911104
3507.491675	820824.283766	41.916109
3507.502213	820711.355768	41.921114
3507.293033	820597.874888	41.926119
3507.332594	820473.243920	41.931124
3507.068492	820370.288218	41.936128
3507.471894	820256.015570	41.941133
3506.928341	820143.267053	41.946138
3507.183252	820032.978589	41.951143
3506.867280	819932.667071	41.956148
3506.425591	819815.198518	41.961152
3506.980722	819710.287064	41.966157
3506.630469	819608.459292	41.971162
3506.648321	819503.682020	41.976167
3506.630890	819414.226566	41.981172
3506.790438	819305.654606	41.986176
3506.697052	819209.700038	41.991181
3506.307346	819107.675351	41.996186
3506.652561	819007.240991	42.001191
3506.441590	818903.323975	42.006196
3506.566757	818817.507670	42.011200
3506.489251	818725.850465	42.016205
3506.310891	818619.133890	42.021210
3506.480513	818532.131940	42.026215
3506.165448	818436.643269	42.031220
3506.319627	818329.035213	42.036224
3506.485915	818229.157034	42.041229
3506.277548	818135.310672	42.046234
3506.463156	818037.775931	42.051239
3506.053658	817952.379217	42.056244
3506.475584	817854.362338	42.061248
3506.097619	817754.762516	42.066253
3506.252334	817658.402139	42.071258
3506.475584	817566.092078	42.076263
3506.467718	817483.658227	42.081268
3506.001778	817372.955032	42.086272
3505.960109	817281.761653	42.091277
3506.049917	817197.692719	42.096282
3505.940034	817107.829975	42.101287
3505.808656	817020.221527	42.106292
3505.668062	816930.606242	42.111296
3505.721344	816840.272426	42.116301
3505.778158	816759.581461	42.121306
3505.822251	816674.044760	42.126311
3505.416763	816583.880971	42.131316
3505.493353	816501.910717	42.136320
3505.588126	816429.875349	42.141325
3505.591453	816353.300942	42.146330
3505.730216	816268.722690	42.151335
3505.454908	816192.535071	42.156340
3505.528042	816105.370600	42.161344
3505.704825	816032.289249	42.166349
3505.506647	815938.655236	42.171354
3505.695545	815853.084220	42.176359
3505.192303	815782.609333	42.181364
3505.236154	815699.067798	42.186368
3505.412676	815619.861338	42.191373
3504.992765	815550.251672	42.196378
3505.303325	815463.529430	42.201383
3505.426302	815400.586238	42.206388
3505.049861	815312.702054	42.211392
3505.050575	815243.019922	42.216397
3504.933338	815177.665778	42.221402
3505.231000	815093.536254	42.226407
3504.729498	815022.710317	42.231412
3505.137774	814955.798352	42.236416
3504.946261	814887.270524	42.241421
3504.795336	814821.134925	42.246426
3504.720614	814758.512122	42.251431
3504.590950	814688.845725	42.256436
3504.848501	814613.335992	42.261440
3504.844424	814552.217802	42.266445
3504.668783	814492.890385	42.271450
3504.865795	814414.254050	42.276455
3504.810154	814347.167583	42.281460
3504.669553	814277.449757	42.286464
3504.981942	814217.941582	42.291469
3504.630299	814158.003516	42.296474
3504.706001	814069.881694	42.301479
3504.140610	814016.981309	42.306484
3503.960965	813944.817595	42.311488
3504.414282	813901.250246	42.316493
3504.397335	813846.592921	42.321498
3504.465621	813782.419148	42.326503
3504.421118	813724.532742	42.331508
3504.461184	813654.876679	42.336512
3504.509905	813589.381829	42.341517
3504.564396	813538.285827	42.346522
3504.362367	813467.443180	42.351527
3504.336614	813411.461281	42.356532
3504.312501	813351.364128	42.361536
3504.468260	813295.792214	42.366541
3504.222998	813251.013205	42.371546
3504.472420	813171.521044	42.376551
3504.411038	813134.646327	42.381556
3504.768979	813058.269933	42.386560
3504.376533	813005.725000	42.391565
3504.166821	812938.698890	42.396570
3504.669572	812877.922922	42.401575
3504.264377	812818.618587	42.406580
3504.277724	812751.308947	42.411584
3504.268454	812688.607159	42.416589
3503.952303	812635.850831	42.421594
3504.257486	812572.263381	42.426599
3504.142192	812542.105667	42.431604
3504.355329	812474.564412	42.436608
3504.062256	812421.067776	42.441613
3504.070419	812362.916084	42.446618
3504.403179	812287.857860	42.451623
3504.278803	812244.081056	42.456628
3503.902115	812189.175636	42.461632
3504.198738	812133.668955	42.466637
3504.095310	812079.991410	42.471642
3504.223431	812021.964006	42.476647
3504.062912	811969.715758	42.481652
3504.015660	811924.797361	42.486656
3504.098660	811863.101574	42.491661
3503.876514	811801.553474	42.496666
3503.840971	811761.384442	42.501671
3504.145096	811711.458370	42.506676
3504.055222	811652.238850	42.511680
3504.082514	811595.743239	42.516685
3503.565736	811549.380842	42.521690
3503.842489	811480.300340	42.526695
3503.558308	811450.165577	42.531700
3503.595178	811399.693277	42.536704
3503.721801	811346.217008	42.541709
3503.598018	811305.128866	42.546714
3503.650025	811254.212015	42.551719
3503.914103	811218.351195	42.556724
3503.651422	811161.507746	42.561728
3503.865867	811117.079872	42.566733
3503.494939	811072.356135	42.571738
3503.584203	811011.925543	42.576743
3503.504352	810979.893059	42.581748
3503.370187	810940.519401	42.586752
3503.527033	810892.424557	42.591757
3503.363780	810868.441307	42.596762
3503.380668	810808.804834	42.601767
3503.207226	810778.746846	42.606772
3503.054596	810736.385984	42.611776
3503.446870	810686.535859	42.616781
3503.277468	810659.808790	42.621786
3503.631609	810602.222033	42.626791
3503.748248	810573.977444	42.631796
3503.564411	810517.948659	42.636800
3503.545609	810479.141357	42.641805
3503.364351	810439.086503	42.646810
3503.644677	810395.231100	42.651815
3503.560425	810343.790826	42.656820
3503.364760	810299.817193	42.661824
3503.596000	810248.520250	42.666829
3503.357197	810219.058608	42.671834
3503.369702	810172.256574	42.676839
3503.266217	810149.633089	42.681844
3503.441192	810101.774693	42.686848
3503.721586	810055.858845	42.691853
3503.240524	810029.376654	42.696858
3503.506864	809965.967211	42.701863
3503.226076	809930.042324	42.706868
3502.865667	809898.394001	42.711872
3503.273817	809850.887492	42.716877
3503.409468	809814.697372	42.721882
3503.824632	809775.471520	42.726887
3503.448503	809724.613727	42.731892
3503.551690	809687.742160	42.736896
3503.351533	809635.580487	42.741901
3503.305263	809602.212727	42.746906
3503.477340	809564.937071	42.751911
3503.301176	809524.336881	42.756916
3503.289491	809484.199459	42.761920
3503.270778	809426.027033	42.766925
3503.084004	809394.984904	42.771930
3503.594142	809370.591383	42.776935
3503.558337	809332.123417	42.781940
3503.262805	809282.033223	42.786945
3503.425176	809247.404064	42.791949
3503.131668	809216.084628	42.796954
3503.515531	809162.352766	42.801959
3503.001049	809123.276287	42.806964
3502.878648	809085.311319	42.811969
3503.365442	809054.891892	42.816973
3503.023343	809017.992018	42.821978
3503.027125	808980.495819	42.826983
3503.295198	808945.749691	42.831988
3503.239999	808900.812608	42.836993
3503.326170	808870.164259	42.841997
3503.228341	808825.282715	42.847002
3503.087493	808786.583896	42.852007
3503.136722	808751.284640	42.857012
3502.963077	808711.757533	42.862017
3503.323397	808669.250292	42.867021
3503.036226	808638.760431	42.872026
3503.470441	808607.171279	42.877031
3503.382164	808582.040230	42.882036
3503.281771	808527.353780	42.887041
3503.212652	808489.817874	42.892045
3502.963674	808451.331032	42.897050
3503.446823	808414.046868	42.902055
3503.162997	808378.163307	42.907060
3503.222652	808348.252257	42.912065
3503.290612	808293.046014	42.917069
3503.097509	808260.186059	42.922074
3503.521689	808221.636062	42.927079
3503.252363	808193.445181	42.932084
3503.276021	808147.019556	42.937089
3503.435453	808109.345873	42.942093
3502.845153	808061.942352	42.947098
3503.143317	808020.715850	42.952103
3503.067154	807995.482604	42.957108
3502.875773	807969.140754	42.962113
3503.344562	807925.581578	42.967117
3503.058524	807888.813419	42.972122
3503.288818	807861.764417	42.977127
3503.010630	807820.925775	42.982132
3503.170177	807785.358245	42.987137
3503.504393	807754.369899	42.992141
3503.000175	807707.243870	42.997146
3503.321059	807665.815395	43.002151
3503.150550	807638.488364	43.007156
3503.186329	807594.557192	43.012161
3502.987714	807559.292599	43.017165
3502.990180	807532.917138	43.022170
3503.407262	807482.304152	43.027175
3502.860112	807453.616703	43.032180
3502.966757	807411.829779	43.037185
3502.965365	807377.610318	43.042189
3502.588678	807353.355684	43.047194
3502.741867	807313.080285	43.052199
3502.988184	807282.937725	43.057204
3502.834145	807250.213553	43.062209
3502.748628	807205.907653	43.067213
3502.787006	807189.330279	43.072218
3503.037114	807157.029361	43.077223
3502.814273	807117.403072	43.082228
3502.895521	807093.562361	43.087233
3502.927523	807069.043290	43.092237
3502.790257	807029.157256	43.097242
3503.270675	806998.288494	43.102247
3503.382835	806970.961263	43.107252
3503.034068	806933.413841	43.112257
3502.805507	806893.002737	43.117261
3502.834574	806868.042170	43.122266
3502.632303	806833.755019	43.127271
3502.548306	806806.704590	43.132276
3502.625871	806773.449693	43.137281
3502.862535	806746.199119	43.142285
3502.688110	806720.241901	43.147290
3502.652849	806689.750871	43.152295
3502.653415	806667.883182	43.157300
3502.721737	806630.706672	43.162305
3502.803390	806615.052366	43.167309
3502.758096	806583.140618	43.172314
3502.680294	806550.939887	43.177319
3502.660263	806521.818479	43.182324
3502.529847	806490.459666	43.187329
3502.786346	806458.252468	43.192333
3502.503395	806437.019125	43.197338
3502.438560	806408.640098	43.202343
3502.745287	806386.377856	43.207348
3502.157450	806368.822927	43.212353
3502.470890	806346.167186	43.217357
3502.397824	806318.524634	43.222362
3502.453309	806294.930553	43.227367
3502.014533	806261.758223	43.232372
3501.867903	806266.048266	43.237377
3502.224620	806231.273758	43.242381
3502.306140	806212.235231	43.247386
3502.231994	806198.616022	43.252391
3502.310029	806167.907873	43.257396
3502.007432	806160.798716	43.262401
3502.652558	806154.808338	43.267405
3502.320434	806124.314655	43.272410
3502.467907	806093.349563	43.277415
3502.276462	806081.122410	43.282420
3502.199757	806050.194049	43.287425
3502.464636	806018.326651	43.292429
3502.447623	806003.864046	43.297434
3502.246413	805979.379491	43.302439
3502.495213	805962.421243	43.307444
3502.110498	805926.541427	43.312449
3502.577175	805914.205574	43.317453
3502.251396	805901.804085	43.322458
3502.658009	805860.203473	43.327463
3502.276468	805846.241905	43.332468
3502.189293	805827.916609	43.337473
3502.344410	805811.120528	43.342477
3502.368857	805784.685679	43.347482
3502.549128	805754.547284	43.352487
3502.402521	805741.527546	43.357492
3502.095502	805713.087457	43.362497
3502.247764	805692.466643	43.367501
3502.034641	805676.907788	43.372506
3502.093987	805649.093615	43.377511
3502.451590	805640.354999	43.382516
3502.493711	805619.408842	43.387521
3502.542778	805594.783613	43.392525
3502.324066	805576.283158	43.397530
3502.267709	805559.178026	43.402535
3502.707040	805526.347883	43.407540
3502.418871	805512.370254	43.412545
3502.602698	805479.778128	43.417549
3502.190326	805466.899722	43.422554
3502.167804	805431.448048	43.427559
3502.211666	805411.775994	43.432564
3502.329422	805406.607432	43.437569
3502.497192	805388.238969	43.442573
3502.280202	805369.737673	43.447578
3502.583406	805345.314890	43.452583
3502.412708	805319.253672	43.457588
3502.139279	805293.699680	43.462593
3502.855856	805270.385511	43.467597
3502.239033	805241.994498	43.472602
3502.386575	805221.029762	43.477607
3502.404436	805212.395606	43.482612
3502.173055	805166.482200	43.487617
3502.652289	805152.720724	43.492621
3502.242086	805136.555567	43.497626
3502.308123	805104.471479	43.502631
3502.306398	805078.577683	43.507636
3502.119932	805068.260536	43.512641
3502.132026	805044.571222	43.517645
3501.764872	805024.132043	43.522650
3502.045419	805006.332492	43.527655
3502.221813	805000.320247	43.532660
3502.252082	804973.538021	43.537665
3502.458694	804961.831817	43.542669
3501.969226	804933.761848	43.547674
3502.149257	804911.809960	43.552679
3502.118071	804911.324650	43.557684
3501.931609	804899.045524	43.562689
3502.234030	804863.096007	43.567693
3502.088895	804862.188071	43.572698
3502.141031	804831.282041	43.577703
3502.093753	804804.659062	43.582708
3502.218225	804802.676790	43.587713
3502.070517	804782.200744	43.592717
3501.946603	804767.066527	43.597722
3502.043892	804754.446140	43.602727
3502.469098	804737.799129	43.607732
3502.342648	804705.646798	43.612737
3502.298253	804689.322243	43.617741
3502.349637	804679.112467	43.622746
3502.210673	804659.076017	43.627751
3502.175748	804630.684714	43.632756
3502.281270	804621.888243	43.637761
3502.334560	804595.100752	43.642765
3502.203266	804585.607562	43.647770
3502.419634	804568.896452	43.652775
3502.531524	804539.695863	43.657780
3502.257184	804513.893891	43.662785
3502.457195	804500.128062	43.667789
3502.004258	804483.526989	43.672794
3502.506288	804458.038343	43.677799
3502.374025	804438.932028	43.682804
3502.060880	804425.642946	43.687809
3502.183347	804399.971372	43.692813
3502.145003	804380.996565	43.697818
3502.252351	804373.670883	43.702823
3502.248119	804343.752886	43.707828
3502.172855	804325.961140	43.712833
3502.254692	804295.685427	43.717837
3501.902817	804289.906719	43.722842
3502.042369	804268.008496	43.727847
3502.295413	804249.181522	43.732852
3501.961229	804225.399282	43.737857
3502.378111	804207.673311	43.742861
3502.061451	804188.302383	43.747866
3501.951921	804177.775031	43.752871
3502.275750	804162.516686	43.757876
3502.254884	804134.660554	43.762881
3502.617139	804123.761119	43.767885
3502.313238	804098.747236	43.772890
3502.382687	804076.810904	43.777895
3502.293694	804050.486173	43.782900
3501.950964	804034.111105	43.787905
3502.414628	804017.210779	43.792909
3502.339915	803993.041651	43.797914
3502.151426	803978.946378	43.802919
3502.025671	803960.082909	43.807924
3501.996645	803935.464605	43.812929
3502.041995	803915.493730	43.817933
3502.161704	803917.141701	43.822938
3502.297077	803893.428121	43.827943
3502.136272	803881.388202	43.832948
3502.163048	803854.356946	43.837953
3502.216515	803831.539556	43.842957
3502.127169	803829.543174	43.847962
3502.015915	803810.873111	43.852967
3502.114240	803792.119425	43.857972
3501.869361	803788.824272	43.862977
3502.251489	803765.412966	43.867981
3502.213599	803751.292421	43.872986
3501.841333	803734.038579	43.877991
3501.840731	803717.851661	43.882996
3502.026970	803685.839269	43.888001
3502.033758	803674.752418	43.893005
3502.298042	803676.376635	43.898010
3502.410808	803645.847715	43.903015
3502.272308	803631.302027	43.908020
3502.064074	803610.292889	43.913025
3502.803853	803587.018278	43.918029
3502.086055	803576.688302	43.923034
3501.972888	803547.226264	43.928039
3502.210453	803533.599482	43.933044
3502.013434	803514.501266	43.938049
3502.024425	803499.979731	43.943053
3502.016402	803493.407914	43.948058
3502.161507	803466.355648	43.953063
3502.322389	803436.259356	43.958068
3502.261380	803437.937210	43.963073
3502.090800	803400.292051	43.968077
3501.810711	803403.085183	43.973082
3502.321687	803389.462137	43.978087
3502.121021	803360.896686	43.983092
3501.867586	803345.142972	43.988097
3502.083376	803337.454949	43.993101
3501.973815	803316.870151	43.998106
3501.870985	803298.148257	44.003111
3501.957907	803284.938234	44.008116
3501.976793	803276.056210	44.013121
3502.199833	803253.797634	44.018125
3502.013983	803248.088808	44.023130
3501.724899	803223.118356	44.028135
3502.014098	803203.939193	44.033140
3502.073509	803198.189927	44.038145
3501.892201	803191.793532	44.043149
3501.808471	803165.317387	44.048154
3501.831794	803144.170575	44.053159
3502.134648	803132.985033	44.058164
3501.883929	803129.739579	44.063169
3502.377622	803099.930394	44.068173
3502.319297	803104.060684	44.073178
3502.262032	803061.930922	44.078183
3502.408336	803052.291779	44.083188
3502.414013	803043.215406	44.088193
3502.237692	803019.157713	44.093197
3502.250528	803007.382003	44.098202
3502.180743	802964.665030	44.103207
3502.505608	802962.502056	44.108212
3502.208390	802938.120596	44.113217
3502.420076	802899.821057	44.118221
3502.218813	802898.235297	44.123226
3502.182484	802865.127441	44.128231
3502.072555	802846.405491	44.133236
3502.046247	802834.292529	44.138241
3502.031206	802815.211459	44.143245
3501.656802	802807.718178	44.148250
3502.056677	802799.459599	44.153255
3502.125021	802777.568378	44.158260
3501.832752	802776.978745	44.163265
3502.003137	802754.972529	44.168269
3502.105076	802742.151464	44.173274
3502.058800	802716.942951	44.178279
3501.992167	802708.564870	44.183284
3501.829832	802693.628659	44.188289
3502.167323	802668.749230	44.193293
3502.069027	802662.387728	44.198298
3501.728677	802651.209235	44.203303
3502.196274	802626.062927	44.208308
3502.022080	802613.777700	44.213313
3501.794145	802610.233889	44.218317
3502.000031	802605.490253	44.223322
3501.995444	802573.504139	44.228327
3502.281633	802549.761106	44.233332
3501.943941	802547.265599	44.238337
3501.961337	802526.951893	44.243341
3502.095966	802528.156202	44.248346
3502.117275	802499.305321	44.253351
3502.084638	802484.396354	44.258356
3501.895985	802463.380496	44.263361
3501.948849	802455.816453	44.268365
3501.762239	802444.416059	44.273370
3502.085017	802418.360699	44.278375
3502.461413	802413.736029	44.283380
3502.095929	802395.987107	44.288385
3502.173385	802369.088872	44.293389
3501.867347	802363.938780	44.298394
3501.923953	802333.756742	44.303399
3502.280269	802313.926262	44.308404
3502.105573	802309.245110	44.313409
3502.177368	802278.864085	44.318413
3501.787280	802267.104419	44.323418
3501.798575	802275.590242	44.328423
3501.952422	802250.935808	44.333428
3501.883745	802252.173654	44.338433
3501.845690	802240.257833	44.343437
3501.858483	802228.873301	44.348442
3501.422951	802225.020050	44.353447
3501.802389	802188.406117	44.358452
3501.789684	802173.934760	44.363457
3501.993569	802169.289281	44.368461
3501.813852	802177.757623	44.373466
3501.714966	802152.408530	44.378471
3502.090609	802138.167508	44.383476
3501.514880	802144.002666	44.388481
3502.056490	802121.442663	44.393485
3501.949386	802119.301520	44.398490
3501.620263	802091.438854	44.403495
3501.630643	802076.865365	44.408500
3501.651982	802090.992028	44.413505
3501.760396	802078.463046	44.418509
3501.310293	802072.894896	44.423514
3501.561906	802045.476085	44.428519
3501.866340	802043.954021	44.433524
3501.166148	802029.448409	44.438529
3501.639246	802025.298190	44.443533
3501.642309	802025.395797	44.448538
3501.657323	802025.638625	44.453543
3502.073688	802022.380894	44.458548
3501.989647	802001.591718	44.463553
3501.794837	801978.171272	44.468557
3501.856608	801984.490325	44.473562
3502.116874	801955.695945	44.478567
3502.105245	801927.535003	44.483572
3501.649774	801939.876069	44.488577
3501.799072	801919.833239	44.493581
3501.618084	801901.218560	44.498586
3501.440248	801887.607899	44.503591
3501.734223	801887.265074	44.508596
3501.757452	801893.639623	44.513601
3501.762653	801876.809597	44.518605
3501.884348	801856.869262	44.523610
3501.869242	801838.864934	44.528615
3501.876564	801825.665237	44.533620
3501.556474	801831.703872	44.538625
3501.860726	801821.006636	44.543629
3502.199506	801787.979033	44.548634
3501.851915	801787.447487	44.553639
3501.911361	801771.540510	44.558644
3501.977696	801758.232834	44.563649
3502.397687	801727.644842	44.568653
3501.824872	801742.753264	44.573658
3501.388936	801723.542247	44.578663
3501.784550	801683.929975	44.583668
3501.877402	801692.697475	44.588673
3501.997307	801674.817681	44.593677
3502.002362	801674.178973	44.598682
3501.755561	801652.287036	44.603687
3502.088616	801634.126696	44.608692
3501.685457	801637.284266	44.613697
3501.819836	801625.829649	44.618701
3501.986550	801597.000123	44.623706
3501.627187	801593.771833	44.628711
3502.031221	801582.468995	44.633716
3501.832389	801577.202521	44.638721
3501.877537	801553.299511	44.643725
3501.864386	801545.696282	44.648730
3501.797555	801539.573897	44.653735
3501.880992	801531.316871	44.658740
3501.792268	801512.735016	44.663745
3501.928022	801488.767793	44.668749
3501.929514	801493.527066	44.673754
3501.800307	801486.090089	44.678759
3502.010929	801466.673726	44.683764
3501.536432	801464.494758	44.688769
3501.668373	801460.645738	44.693773
3501.764673	801453.760394	44.698778
3501.433512	801451.803150	44.703783
3501.856840	801419.741221	44.708788
3501.518362	801414.203216	44.713793
3501.653144	801396.271185	44.718797
3501.820882	801393.593865	44.723802
3501.682240	801395.235931	44.728807
3501.599725	801389.410405	44.733812
3501.909408	801360.703552	44.738817
3501.819257	801349.825213	44.743821
3502.063473	801344.043969	44.748826
3501.930684	801340.729172	44.753831
3502.130388	801307.869397	44.758836
3502.001419	801304.308609	44.763841
3501.946425	801296.221311	44.768845
3501.921591	801271.445619	44.773850
3501.868959	801260.757237	44.778855
3501.930351	801250.050057	44.783860
3501.652531	801240.281978	44.788865
3501.631267	801211.727158	44.793869
3501.722724	801214.459961	44.798874
3501.911879	801193.672429	44.803879
3501.981446	801196.654191	44.808884
3501.803842	801185.299305	44.813889
3501.790863	801159.834288	44.818893
3501.946160	801155.147067	44.823898
3501.478252	801155.371330	44.828903
3501.907693	801148.921509	44.833908
3501.712268	801127.412006	44.838913
3501.872022	801120.859370	44.843917
3501.685343	801107.935611	44.848922
3501.740061	801099.192100	44.853927
3501.797158	801080.977630	44.858932
3501.648283	801066.182895	44.863937
3501.784367	801061.596916	44.868941
3501.890910	801062.658900	44.873946
3501.554718	801054.961130	44.878951
3501.744691	801020.874838	44.883956
3501.559827	801022.475533	44.888961
3501.655394	801007.247844	44.893965
3501.838938	801011.584896	44.898970
3501.716870	801001.152904	44.903975
3501.816314	800988.525289	44.908980
3501.522573	800966.050061	44.913985
3501.806687	800955.551097	44.918989
3501.808889	800960.212477	44.923994
3501.460207	800949.277951	44.928999
3502.068773	800942.602150	44.934004
3501.636007	800934.233154	44.939009
3501.515407	800913.103232	44.944013
3501.485473	800915.610791	44.949018
3501.587759	800915.299498	44.954023
3501.864690	800908.187575	44.959028
3501.314219	800892.379044	44.964033
3501.488181	800869.188533	44.969037
3501.643559	800870.242503	44.974042
3501.593578	800871.183083	44.979047
3501.786995	800871.641926	44.984052
3501.504158	800868.498831	44.989057
3501.691407	800853.206632	44.994061
3501.797834	800831.302988	44.999066
3501.606193	800819.704453	45.004071
3501.505208	800813.832412	45.009076
3501.713016	800814.975899	45.014081
3501.514741	800806.911630	45.019085
3501.396153	800811.740222	45.024090
3501.356511	800803.208170	45.029095
3501.595536	800795.513509	45.034100
3501.640285	800777.103986	45.039105
3501.792347	800766.233907	45.044109
3501.382944	800767.773500	45.049114
3501.627583	800760.372311	45.054119
3501.899266	800761.210850	45.059124
3501.529138	800744.636188	45.064129
3501.868249	800726.423408	45.069133
3501.851574	800713.078327	45.074138
3501.877954	800710.767540	45.079143
3501.951419	800702.952828	45.084148
3501.434797	800693.223309	45.089153
3501.420576	800683.656389	45.094157
3501.518656	800661.360999	45.099162
3501.593019	800677.935472	45.104167
3501.783784	800658.618267	45.109172
3501.616350	800676.508476	45.114177
3501.677938	800647.250662	45.119181
3501.591342	800630.334584	45.124186
3501.746561	800630.652515	45.129191
3501.492586	800618.327808	45.134196
3501.525451	800625.094525	45.139201
3501.766566	800607.388310	45.144205
3501.835129	800607.327927	45.149210
3501.824599	800584.019632	45.154215
3502.037917	800571.274356	45.159220
3501.557538	800573.120124	45.164225
3501.919114	800557.700412	45.169229
3502.068021	800535.641617	45.174234
3501.588472	800528.408539	45.179239
3501.681246	800524.908974	45.184244
3501.487466	800517.530666	45.189249
3501.822829	800505.648503	45.194253
3501.928731	800487.473511	45.199258
3501.507485	800488.377146	45.204263
3501.719815	800479.410597	45.209268
3501.621912	800488.750861	45.214273
3501.823446	800469.087835	45.219277
3501.920861	800446.497418	45.224282
3501.770457	800441.516547	45.229287
3501.952193	800432.947576	45.234292
3501.869909	800429.378647	45.239297
3501.700602	800404.476431	45.244301
3501.762408	800396.074394	45.249306
3501.537449	800403.668996	45.254311
3501.739855	800388.226052	45.259316
3501.955886	800378.866163	45.264321
3501.667271	800359.381711	45.269325
3502.018709	800350.195781	45.274330
3501.765251	800346.213325	45.279335
3501.555846	800332.850183	45.284340
3501.801492	800318.381474	45.289345
3501.441144	800309.803488	45.294349
3501.504610	800300.517699	45.299354
3501.690411	800300.781533	45.304359
3501.900694	800296.869892	45.309364
3501.612268	800296.328473	45.314369
3501.490547	800268.424305	45.319373
3501.671930	800250.285336	45.324378
3501.451131	800250.272612	45.329383
3501.756844	800244.529405	45.334388
3501.647129	800241.455659	45.339393
3501.490676	800238.144229	45.344397
3501.574029	800212.414488	45.349402
3501.277490	800204.611084	45.354407
3501.680992	800198.998961	45.359412
3501.467654	800205.610334	45.364417
3501.863491	800194.012139	45.369421
3501.488013	800196.625949	45.374426
3501.706274	800198.553043	45.379431
3502.108988	800181.751582	45.384436
3501.663205	800162.145234	45.389441
3501.665995	800159.396458	45.394445
3501.512265	800142.833787	45.399450
3501.167586	800148.976078	45.404455
3501.299147	800146.353318	45.409460
3501.269661	800141.990314	45.414465
3501.733149	800142.944570	45.419469
3501.577560	800116.812139	45.424474
3501.312478	800107.629286	45.429479
3501.643717	800101.341908	45.434484
3501.683245	800101.924307	45.439489
3501.732047	800101.818098	45.444493
3501.750229	800095.631357	45.449498
3501.570664	800077.796778	45.454503
3501.477065	800057.150575	45.459508
3501.589928	800063.953740	45.464513
3501.741464	800053.229868	45.469517
3501.245377	800039.766149	45.474522
3501.518071	800048.849651	45.479527
3501.868132	800044.031448	45.484532
3501.380699	800020.063649	45.489537
3501.586286	800018.704670	45.494541
3501.644629	800010.008270	45.499546
3501.597587	800005.844384	45.504551
3501.723222	799998.511066	45.509556
3501.494022	800011.554441	45.514561
3501.468184	800006.552740	45.519565
3501.729668	799986.338618	45.524570
3501.676777	799972.458222	45.529575
3501.787627	799958.845296	45.534580
3501.666979	799961.908001	45.539585
3501.519487	799949.908112	45.544589
3501.802970	799958.940876	45.549594
3501.636458	799935.018080	45.554599
3501.899578	799919.171469	45.559604
3501.901289	799926.532940	45.564609
3501.529351	799924.434735	45.569613
3501.621973	799904.542661	45.574618
3501.574136	799891.152056	45.579623
3501.926578	799872.296825	45.584628
3501.676712	799864.828901	45.589633
3501.771245	799872.027905	45.594637
3501.811588	799856.708634	45.599642
3501.454210	799852.104983	45.604647
3501.693230	799820.949465	45.609652
3501.727330	799823.888582	45.614657
3501.404017	799828.947892	45.619661
3501.472353	799829.231095	45.624666
3501.428398	799829.189239	45.629671
3501.546531	799823.771059	45.634676
3501.440344	799795.469799	45.639681
3501.665204	799791.310077	45.644685
3501.745113	799779.272437	45.649690
3501.260612	799778.566953	45.654695
3501.666940	799778.450930	45.659700
3501.715124	799784.823307	45.664705
3501.219560	799773.174921	45.669709
3501.600923	799751.566146	45.674714
3501.274764	799738.122930	45.679719
3501.651045	799734.968909	45.684724
3501.632710	799736.198907	45.689729
3501.280759	799712.943927	45.694733
3501.848614	799724.924033	45.699738
3501.592111	799734.684072	45.704743
3501.493945	799729.105127	45.709748
3501.498089	799714.527703	45.714753
3501.109339	799699.769563	45.719757
3501.382082	799693.785935	45.724762
3501.468068	799681.992527	45.729767
3501.328839	799673.769971	45.734772
3501.305474	799681.970195	45.739777
3501.330112	799666.653093	45.744781
3501.523712	799670.743930	45.749786
3501.368146	799673.910672	45.754791
3501.298029	799683.198360	45.759796
3501.433801	799674.194306	45.764801
3501.425692	799681.115933	45.769805
3501.026649	799674.457658	45.774810
3501.480286	799640.468409	45.779815
3501.592179	799572.473199	45.784820
3501.342105	799466.891398	45.789825
3501.101092	799289.891207	45.794829
3501.686793	799053.849082	45.799834
3501.256347	798763.627645	45.804839
3501.242666	798411.669818	45.809844
3500.893158	798008.595926	45.814849
3500.730315	797556.716722	45.819853
3500.340929	797029.921210	45.824858
3500.038807	796451.415614	45.829863
3499.645125	795814.783579	45.834868
3499.218165	795140.577733	45.839873
3499.110913	794393.610446	45.844877
3498.918423	793589.693848	45.849882
3498.192134	792725.345212	45.854887
3498.116290	791794.893426	45.859892
3497.560784	790811.619823	45.864897
3496.974406	789770.513833	45.869901
3496.868005	788669.647436	45.874906
3495.770485	787496.993604	45.879911
3495.526212	786266.424761	45.884916
3494.464091	784995.204038	45.889921
3493.795621	783649.660784	45.894925
3493.315214	782250.255635	45.899930
3492.354861	780798.839801	45.904935
3491.838330	779271.703115	45.909940
3491.115345	777695.491376	45.914945
3490.191051	776048.407833	45.919949
3489.723222	774346.354630	45.924954
3488.583242	772590.909823	45.929959
3488.106157	770759.543325	45.934964
3486.626018	768870.910033	45.939969
3485.759611	766944.176929	45.944973
3485.110389	764930.854759	45.949978
3483.797044	762876.652129	45.954983
3482.806363	760755.766291	45.959988
3481.624653	758585.800404	45.964993
3480.646937	756347.444783	45.969997
3479.711335	754054.448692	45.975002
3478.477727	751716.604737	45.980007
3477.692438	749304.300556	45.985012
3475.997462	746843.696835	45.990017
3474.506831	744317.608074	45.995021
3473.493842	741742.996692	46.000026
3472.025368	739131.998404	46.005031
3471.032201	736434.783375	46.010036
3469.444058	733698.337549	46.015041
3467.969667	730913.594833	46.020045
3466.818046	728075.968870	46.025050
3465.536542	725183.206216	46.030055
3464.225618	722222.050292	46.035060
3462.379903	719212.508602	46.040065
3460.604265	716146.746367	46.045069
3459.464933	713034.843144	46.050074
3457.464121	709868.562532	46.055079
3456.127308	706644.621767	46.060084
3454.296116	703371.257294	46.065089
3452.808419	700049.081104	46.070093
3451.055444	696679.591244	46.075098
3449.187752	693256.352079	46.080103
3447.838877	689772.540056	46.085108
3446.027536	686255.045868	46.090113
3444.241858	682679.256809	46.095117
3442.217616	679044.414206	46.100122
3440.127651	675359.157477	46.105127
3438.527417	671639.108391	46.110132
3436.742023	667854.020409	46.115137
3434.720855	664024.751422	46.120141
3432.976114	660155.724013	46.125146
3430.651089	656218.878325	46.130151
3428.599083	652258.031256	46.135156
3426.618513	648239.263844	46.140161
3424.530529	644176.956863	46.145165
3422.232407	640063.139817	46.150170
3419.674743	635911.642010	46.155175
3418.267677	631706.134664	46.160180
3415.959386	627464.693458	46.165185
3413.462608	623174.652626	46.170189
3411.560084	618824.618930	46.175194
3409.296036	614442.182165	46.180199
3407.175439	610013.849584	46.185204
3404.625859	605528.895245	46.190209
3402.432634	601012.753187	46.195213
3400.496399	596449.908909	46.200218
3398.018563	591854.634921	46.205223
3395.504863	587191.048211	46.210228
3392.984279	582505.907335	46.215233
3390.597519	577775.952333	46.220237
3388.516454	572998.717130	46.225242
3385.814986	568169.447201	46.230247
3383.142542	563316.158641	46.235252
3380.856345	558418.191772	46.240257
3378.215497	553479.632296	46.245261
3375.489081	548486.458495	46.250266
3372.515101	543472.764083	46.255271
3370.128202	538419.554230	46.260276
3367.248612	533322.002793	46.265281
3364.929275	528200.472842	46.270285
3362.427599	523027.623307	46.275290
3359.471246	517835.412214	46.280295
3356.828529	512574.708436	46.285300
3353.720982	507303.747663	46.290305
3350.975243	501999.968451	46.295309
3348.082106	496651.574027	46.300314
3344.893417	491273.058439	46.305319
3342.454675	485859.351599	46.310324
3339.150735	480416.855054	46.315329
3336.161444	474942.351024	46.320333
3333.375579	469425.891177	46.325338
3330.251955	463902.032004	46.330343
3327.318355	458320.741750	46.335348
3324.319315	452728.352985	46.340353
3321.226568	447103.959245	46.345357
3318.393721	441456.095825	46.350362
3315.051930	435760.610621	46.355367
3311.980824	430048.246071	46.360372
3308.783497	424309.278669	46.365377
3305.786083	418554.448852	46.370381
3302.563701	412763.953507	46.375386
3299.279492	406944.445860	46.380391
3296.363545	401099.315632	46.385396
3293.124855	395228.355009	46.390401
3289.553070	389327.635809	46.395405
3286.377586	383410.646722	46.400410
3282.573686	377489.727132	46.405415
3279.563707	371522.072042	46.410420
3276.314234	365552.593486	46.415425
3272.966177	359564.175157	46.420429
3269.091426	353539.606744	46.425434
3265.774542	347494.905362	46.430439
3262.741212	341429.399209	46.435444
3259.134273	335371.425159	46.440449
3255.312682	329283.412143	46.445453
3251.984032	323166.587591	46.450458
3248.182659	317064.309991	46.455463
3244.566576	310932.968068	46.460468
3241.574756	304773.913935	46.465473
3237.479234	298615.519143	46.470477
3234.181447	292444.540492	46.475482
3230.011485	286261.996263	46.480487
3226.573070	280061.311697	46.485492
3222.990002	273849.894956	46.490497
3219.010302	267639.356918	46.495501
3215.190419	261422.711644	46.500506
3211.757884	255203.265637	46.505511
3207.716751	248960.612845	46.510516
3203.934677	242737.684944	46.515521
3200.150997	236483.573028	46.520525
3196.489959	230234.302113	46.525530
3192.486344	223982.470553	46.530535
3188.396578	217722.036160	46.535540
3184.439797	211450.949384	46.540545
3180.210053	205125.028618	46.545549
3176.444748	198869.473885	46.550554
3172.385783	192608.318186	46.555559
3168.413587	186342.693342	46.560564
3164.218262	180109.803229	46.565569
3159.806848	173853.079398	46.570573
3155.813030	167613.854881	46.575578
3151.364017	161392.008213	46.580583
3147.273794	155166.168919	46.585588
3143.224380	148954.340708	46.590593
3138.860650	142760.117780	46.595597
3134.411334	136566.137173	46.600602
3129.831448	130388.477120	46.605607
3125.160892	124228.539759	46.610612
3120.604734	118083.137776	46.615617
3115.471020	111960.701606	46.620621
3110.739260	105864.337266	46.625626
3105.656014	99806.108579	46.630631
3100.821146	93769.371327	46.635636
3095.901595	87780.927842	46.640641
3090.225990	81811.649900	46.645645
3084.770981	75888.299578	46.650650
3077.894035	70031.631888	46.655655
3069.583060	64290.650837	46.660660
3054.099094	58819.540705	46.665665
3037.747150	53527.547660	46.670669
3021.704268	48434.980019	46.675674
3005.698272	43593.927859	46.680679
2990.801084	38983.199653	46.685684
2976.313662	34641.372356	46.690689
2962.651337	30581.517546	46.695693
2949.977114	26765.345703	46.700698
2937.856144	23212.197887	46.705703
2925.759789	19901.913308	46.710708
2914.092653	16837.148770	46.715713
2903.045429	14002.528462	46.720717
2892.554799	11389.330974	46.725722
2879.733558	9052.933790	46.730727
2864.632773	7016.899825	46.735732
2848.473944	5263.259048	46.740737
2832.637338	3787.788300	46.745741
2818.930129	2554.196985	46.750746
2806.096304	1570.690235	46.755751
2795.357170	804.116474	46.760756
2785.487594	243.098987	46.765761
2762.531264	268.603651	46.770765
2750.515624	280.692442	46.775770
2749.091199	284.977336	46.780775
2753.390514	272.831609	46.785780
2759.432199	271.060270	46.790785
2763.456555	259.301250	46.795789
2765.843957	265.501245	46.800794
2764.805450	269.032978	46.805799
2762.917008	267.973423	46.810804
2760.019978	256.820162	46.815809
2756.439092	261.531309	46.820813
2753.521227	262.591277	46.825818
2750.203851	267.129347	46.830823
2747.069815	273.873901	46.835828
2744.985450	254.340120	46.840833
2742.173655	268.576522	46.845837
2739.812132	253.270811	46.850842
2736.295522	260.569858	46.855847
2733.426057	264.933455	46.860852
2729.863831	259.137077	46.865857
2726.721307	268.651614	46.870861
2723.680457	254.254385	46.875866
2720.367372	252.120215	46.880871
2717.301600	254.031939	46.885876
2714.755377	244.212363	46.890881
2710.803901	252.760117	46.895885
2707.581080	242.070930	46.900890
2704.493172	242.798943	46.905895
2700.972831	242.834630	46.910900
2697.892759	251.034101	46.915905
2694.519875	251.747736	46.920909
2691.369795	244.232566	46.925914
2687.617605	252.270358	46.930919
2684.419716	242.521536	46.935924
2681.234804	249.362889	46.940929
2677.939791	245.501098	46.945933
2674.735238	243.835544	46.950938
2670.907326	240.319514	46.955943
2667.719416	246.711084	46.960948
2664.548239	247.411404	46.965953
2660.868250	236.511312	46.970957
2657.730331	237.562706	46.975962
2654.180719	240.039233	46.980967
2650.586814	239.787346	46.985972
2647.215800	228.604673	46.990977
2643.336340	241.065136	46.995981
2640.822765	234.880047	47.000986
2637.106298	232.998301	47.005991
2633.519756	232.928122	47.010996
2630.680966	238.982539	47.016001
2626.798111	253.386372	47.021005
2623.872204	232.195538	47.026010
2619.767931	234.432532	47.031015
2616.590795	233.625948	47.036020
2613.478156	222.939080	47.041025
2608.967753	237.798392	47.046029
2605.912791	238.229079	47.051034
2602.675921	229.205665	47.056039
2599.839052	232.938424	47.061044
2596.159346	236.322779	47.066049
2592.091671	243.596219	47.071053
2589.082263	234.948389	47.076058
2585.578005	229.719793	47.081063
2581.967311	237.700942	47.086068
2578.558674	240.680209	47.091073
2575.171434	242.228155	47.096077
2572.246134	236.472468	47.101082
2568.156431	234.527000	47.106087
2564.841661	225.294174	47.111092
2561.651211	219.635692	47.116097
2557.472991	230.018353	47.121101
2554.111588	223.727539	47.126106
2550.998773	231.548760	47.131111
2547.700684	223.864902	47.136116
2544.059370	229.259142	47.141121
2540.673868	224.231295	47.146125
2537.189252	224.015703	47.151130
2533.775567	226.629794	47.156135
2530.190650	231.394078	47.161140
2526.859111	220.499368	47.166145
2522.823538	220.959679	47.171149
2519.947719	217.677924	47.176154
2516.038613	222.672958	47.181159
2512.262524	221.809204	47.186164
2509.456360	215.420053	47.191169
2505.780581	219.198038	47.196173
2502.241114	223.981672	47.201178
2498.956410	217.376641	47.206183
2495.323755	220.514624	47.211188
2492.284284	213.797336	47.216193
2488.090205	219.365620	47.221197
2484.917242	208.730410	47.226202
2480.931247	210.783996	47.231207
2477.771136	213.070973	47.236212
2474.785580	209.483141	47.241217
2471.277034	210.785149	47.246221
2468.065763	211.063783	47.251226
2464.056554	217.399644	47.256231
2460.479033	220.229022	47.261236
2457.072291	218.134888	47.266241
2453.740966	221.920520	47.271245
2450.120478	205.377248	47.276250
2446.439134	215.688865	47.281255
2442.710902	209.674272	47.286260
2439.830361	200.359070	47.291265
2436.008780	212.105817	47.296269
2432.904151	209.952602	47.301274
2429.369915	216.733537	47.306279
2425.741350	201.759502	47.311284
2422.255272	203.311576	47.316289
2418.570014	208.654999	47.321293
2415.335930	212.341143	47.326298
2411.708192	206.390010	47.331303
2408.488335	211.163495	47.336308
2404.902184	200.535500	47.341313
2401.138060	212.301593	47.346317
2397.740388	201.674979	47.351322
2394.142773	211.097702	47.356327
2390.552550	214.454858	47.361332
2387.712015	195.522843	47.366337
2383.969028	209.478043	47.371341
2380.503606	201.749463	47.376346
2377.177441	194.612467	47.381351
2373.394848	201.206770	47.386356
2369.976647	206.645182	47.391361
2366.228288	214.947055	47.396365
2362.875483	212.699043	47.401370
2359.445156	215.279051	47.406375
2355.746803	220.973522	47.411380
2352.374759	196.551708	47.416385
2348.881481	214.179350	47.421389
2345.549106	204.998590	47.426394
2342.562103	202.477358	47.431399
2338.596549	201.242906	47.436404
2335.174045	188.191260	47.441409
2331.128120	199.357828	47.446413
2327.943906	197.479034	47.451418
2324.370473	209.146715	47.456423
2320.956440	191.313472	47.461428
2317.669889	203.150197	47.466433
2313.894303	197.248070	47.471437
2310.486985	194.852801	47.476442
2307.230668	198.612698	47.481447
2303.298597	206.604715	47.486452
2299.808270	195.254291	47.491457
2296.644409	207.175271	47.496461
2292.985683	197.986311	47.501466
2289.505001	205.233998	47.506471
2286.197116	194.994676	47.511476
2282.568899	197.858339	47.516481
2279.360188	198.490913	47.521485
2276.015206	202.368545	47.526490
2272.156255	191.987876	47.531495
2268.594287	196.348119	47.536500
2264.787265	189.619122	47.541505
2261.132004	204.828541	47.546509
2257.853461	196.055590	47.551514
2255.002128	198.866314	47.556519
2251.173615	193.072499	47.561524
2247.881966	191.092379	47.566529
2244.205603	196.997944	47.571533
2240.526050	193.800329	47.576538
2237.245391	190.729805	47.581543
2233.369153	207.827894	47.586548
2229.819241	194.091221	47.591553
2226.400393	196.099835	47.596557
2223.462011	193.025450	47.601562
2219.557661	191.896497	47.606567
2216.129692	194.342888	47.611572
2212.678055	185.794354	47.616577
2208.852795	196.837559	47.621581
2205.600996	191.695396	47.626586
2202.474152	196.257185	47.631591
2198.601184	192.895262	47.636596
2195.427735	195.576024	47.641601
2191.531261	199.840428	47.646605
2188.236006	196.385888	47.651610
2184.644866	204.914760	47.656615
2181.034767	195.146713	47.661620
2177.618238	188.453695	47.666625
2173.865839	197.146498	47.671629
2170.662584	189.879729	47.676634
2166.855471	187.865291	47.681639
2163.581928	184.827272	47.686644
2160.041488	190.876592	47.691649
2156.731571	178.908701	47.696653
2153.480746	192.377797	47.701658
2149.928676	192.481818	47.706663
2146.154765	198.865828	47.711668
2142.852677	186.833408	47.716673
2138.962255	195.643504	47.721677
2135.933995	193.300043	47.726682
2132.461935	198.869175	47.731687
2128.479365	195.884978	47.736692
2124.894148	197.636647	47.741697
2121.386790	187.669669	47.746701
2118.164283	184.145550	47.751706
2114.695067	191.525583	47.756711
2110.822625	186.180988	47.761716
2108.003820	188.313546	47.766721
2104.309688	186.628474	47.771725
2100.851354	186.447227	47.776730
2097.252619	180.183087	47.781735
2093.686068	179.243748	47.786740
2090.425999	177.841071	47.791745
2086.560800	188.516696	47.796749
2083.035402	192.948433	47.801754
2079.420330	184.346329	47.806759
2076.093113	195.084071	47.811764
2072.959650	187.723067	47.816769
2069.176731	189.981819	47.821773
2065.669656	180.586457	47.826778
2062.213761	173.001719	47.831783
2058.377399	183.933843	47.836788
2055.238811	178.592047	47.841793
2051.420540	180.800897	47.846797
2048.098527	182.087715	47.851802
2044.905068	188.627891	47.856807
2041.304393	189.498565	47.861812
2038.354861	184.404594	47.866817
2033.897012	187.332215	47.871821
2030.412724	172.885473	47.876826
2027.220966	179.938985	47.881831
2023.484671	187.916186	47.886836
2020.217609	173.072726	47.891841
2016.352298	185.950445	47.896845
2012.918170	177.725401	47.901850
2010.086966	179.232475	47.906855
2006.133282	183.598054	47.911860
2002.549058	181.585414	47.916865
1998.921706	178.196014	47.921869
1995.733973	169.264199	47.926874
1992.167885	177.569979	47.931879
1988.779497	191.002324	47.936884
1985.370673	168.969084	47.941889
1981.568870	177.991928	47.946893
1978.273509	170.010985	47.951898
1974.828641	176.009685	47.956903
1971.052299	175.202588	47.961908
1967.738717	175.854765	47.966913
1963.820296	187.711376	47.971917
1960.545821	187.059356	47.976922
1957.580131	177.849412	47.981927
1953.693036	173.038703	47.986932
1950.214809	183.421261	47.991937
1945.987168	176.010959	47.996941
1943.076642	180.693330	48.001946
1939.834439	174.627862	48.006951
1936.181610	175.797837	48.011956
1932.879785	167.339100	48.016961
1929.297996	177.693069	48.021965
1925.693456	179.914472	48.026970
1922.372484	171.223104	48.031975
1918.404238	175.485465	48.036980
1915.205815	173.619069	48.041985
1911.029557	175.733338	48.046989
1908.117318	174.274052	48.051994
1904.608591	173.935467	48.056999
1900.994131	166.996355	48.062004
1897.966429	164.313330	48.067009
1894.309384	166.022495	48.072013
1890.525937	161.927360	48.077018
1887.017687	182.734646	48.082023
1883.905956	180.027997	48.087028
1880.231858	172.717223	48.092033
1876.713506	184.077420	48.097037
1873.008745	175.554859	48.102042
1869.691304	174.541582	48.107047
1866.188610	171.067462	48.112052
1862.718892	162.601540	48.117057
1859.342424	169.265496	48.122061
1855.399038	162.926849	48.127066
1852.110797	170.279880	48.132071
1848.755663	167.110153	48.137076
1845.075556	167.049082	48.142081
1841.543847	169.276759	48.147085
1838.083399	171.891161	48.152090
1834.544372	170.633876	48.157095
1831.100981	185.260024	48.162100
1827.806179	164.120873	48.167105
1824.229368	165.007545	48.172109
1820.709719	162.264934	48.177114
1817.501117	168.900422	48.182119
1813.072568	179.154106	48.187124
1809.970646	174.630273	48.192129
1806.291410	170.986615	48.197133
1803.165012	167.488723	48.202138
1799.714775	166.658596	48.207143
1796.100051	173.491821	48.212148
1792.874960	154.157497	48.217153
1789.053000	167.031886	48.222157
1785.512296	161.320605	48.227162
1782.047353	159.773501	48.232167
1778.439064	162.708491	48.237172
1774.757191	169.029423	48.242177
1771.406747	171.445753	48.247181
1768.353581	175.297737	48.252186
1765.057455	175.623823	48.257191
1760.668220	170.934160	48.262196
1757.609926	161.415910	48.267201
1753.914631	165.613682	48.272205
1750.443733	161.936175	48.277210
1747.316098	162.991569	48.282215
1743.360654	164.555390	48.287220
1739.791490	158.813412	48.292225
1736.122589	164.227331	48.297229
1733.253101	167.438625	48.302234
1729.931746	163.659403	48.307239
1726.120961	167.502233	48.312244
1722.920067	165.493972	48.317249
1718.869683	162.570340	48.322253
1715.428783	164.774805	48.327258
1711.909205	158.311367	48.332263
1708.462217	159.801275	48.337268
1705.000615	157.940223	48.342273
1701.498965	158.265918	48.347277
1697.996963	160.356459	48.352282
1694.539070	163.401834	48.357287
1691.144235	158.648773	48.362292
1688.093149	157.551676	48.367297
1683.976952	164.278860	48.372301
1680.371555	151.169721	48.377306
1677.152445	160.377416	48.382311
1673.368843	164.805758	48.387316
1670.023023	157.208608	48.392321
1666.555212	151.878618	48.397325
1663.001101	154.697185	48.402330
1659.712605	152.832948	48.407335
1655.565191	162.947869	48.412340
1652.426457	162.164480	48.417345
1648.866302	170.703431	48.422349
1645.597339	157.016797	48.427354
1641.869196	154.297043	48.432359
1638.563743	161.658220	48.437364
1635.016137	173.966887	48.442369
1631.208072	165.803571	48.447373
1627.959679	158.528269	48.452378
1624.777345	154.389542	48.457383
1621.003548	161.407038	48.462388
1617.712708	150.911563	48.467393
1613.902907	148.672641	48.472397
1610.251482	158.459585	48.477402
1606.824242	150.370092	48.482407
1603.117147	156.161127	48.487412
1600.142396	148.664093	48.492417
1596.740851	152.210172	48.497421
1593.043789	155.422030	48.502426
1589.585490	166.420301	48.507431
1585.520447	159.154390	48.512436
1582.282669	153.786682	48.517441
1578.794609	154.535802	48.522445
1575.601747	161.242280	48.527450
1571.858549	151.620704	48.532455
1568.178059	155.437964	48.537460
1565.151265	149.025790	48.542465
1561.435667	155.339749	48.547469
1557.948745	152.569679	48.552474
1554.100610	149.954622	48.557479
1550.588640	161.550549	48.562484
1548.011773	147.275326	48.567489
1543.864719	153.210221	48.572493
1540.099704	160.932790	48.577498
1537.280044	150.579217	48.582503
1533.380970	162.220287	48.587508
1529.925334	147.213227	48.592513
1525.991662	155.797977	48.597517
1522.631256	143.859339	48.602522
1519.853924	150.276268	48.607527
1515.706446	151.576028	48.612532
1512.618738	140.725574	48.617537
1508.223459	161.580760	48.622541
1505.409741	151.755716	48.627546
1502.141773	158.002934	48.632551
1498.267950	165.510451	48.637556
1495.283080	151.724741	48.642561
1491.490676	158.286904	48.647565
1487.699085	153.450456	48.652570
1484.162332	158.918843	48.657575
1480.674466	159.394402	48.662580
1477.111378	159.640074	48.667585
1473.841747	157.780607	48.672589
1470.636089	160.924154	48.677594
1467.200850	165.012352	48.682599
1463.267626	159.025565	48.687604
1459.800856	155.243251	48.692609
1456.332026	152.757440	48.697613
1452.783437	158.862852	48.702618
1449.321786	145.787858	48.707623
1445.419488	154.221060	48.712628
1442.501215	142.788128	48.717633
1438.689598	147.379647	48.722637
1434.923665	152.632723	48.727642
1431.638015	141.266053	48.732647
1428.347436	152.084762	48.737652
1424.835101	147.421284	48.742657
1421.472561	149.499889	48.747661
1418.174548	148.162789	48.752666
1414.655880	148.579633	48.757671
1410.892813	156.370108	48.762676
1407.420289	144.379800	48.767681
1403.573072	143.872885	48.772685
1399.931674	150.303122	48.777690
1396.899412	140.296671	48.782695
1393.416537	151.799549	48.787700
1389.941690	133.807239	48.792705
1386.009608	144.117596	48.797709
1382.654013	146.671882	48.802714
1379.125232	139.219740	48.807719
1375.569226	152.236356	48.812724
1372.249731	150.522895	48.817729
1368.639075	151.758803	48.822733
1365.152094	154.659761	48.827738
1361.618273	142.521551	48.832743
1358.198600	150.969747	48.837748
1354.958195	153.781472	48.842753
1351.427045	146.902537	48.847757
1347.990465	143.031642	48.852762
1344.160837	148.437044	48.857767
1340.288736	149.728352	48.862772
1337.185342	136.926189	48.867777
1334.171392	141.451807	48.872781
1330.055359	152.371969	48.877786
1326.681762	141.888356	48.882791
1323.049136	148.911391	48.887796
1320.121200	151.574083	48.892801
1316.695700	150.149947	48.897805
1312.618914	152.656474	48.902810
1308.977661	138.175661	48.907815
1305.354573	158.443232	48.912820
1302.186538	142.371206	48.917825
1298.720783	150.112458	48.922829
1295.186412	153.676058	48.927834
1291.809021	137.910498	48.932839
1288.119290	148.875446	48.937844
1284.887958	150.008236	48.942849
1281.035026	139.484101	48.947853
1277.591875	151.505321	48.952858
1273.989776	148.170757	48.957863
1270.328918	148.231116	48.962868
1267.258339	136.235822	48.967873
1263.829691	138.571165	48.972877
1260.294849	125.926598	48.977882
1257.213010	131.420224	48.982887
1253.030033	149.513476	48.987892
1249.411283	142.628640	48.992897
1246.366913	144.943772	48.997901
1242.328509	146.991463	49.002906
1239.138948	141.820495	49.007911
1235.617537	144.740218	49.012916
1232.290954	145.721038	49.017921
1228.260951	144.682542	49.022925
1225.130272	140.744348	49.027930
1221.927840	142.705851	49.032935
1217.966853	141.801586	49.037940
1214.964495	140.361818	49.042945
1211.060453	148.925445	49.047949
1207.569691	140.932406	49.052954
1204.508478	145.788189	49.057959
1200.627484	151.725024	49.062964
1197.311219	144.178515	49.067969
1193.518781	152.772959	49.072973
1189.841680	147.562725	49.077978
1186.530059	141.955744	49.082983
1182.812140	146.650706	49.087988
1179.718877	142.461985	49.092993
1176.056284	134.486383	49.097997
1172.430227	136.749188	49.103002
1169.160296	135.717556	49.108007
1165.653531	144.411258	49.113012
1162.259502	139.828240	49.118017
1158.678928	144.699828	49.123021
1154.838882	140.519167	49.128026
1151.234335	141.024017	49.133031
1147.899704	143.146581	49.138036
1144.632930	138.988692	49.143041
1141.091414	137.537135	49.148045
1137.270265	141.253218	49.153050
1134.049722	134.098105	49.158055
1130.374666	138.755234	49.163060
1127.120846	136.806216	49.168065
1123.610325	131.607695	49.173069
1119.840148	149.640353	49.178074
1116.824534	132.971377	49.183079
1112.910970	135.691102	49.188084
1109.523252	142.509240	49.193089
1105.958331	148.079917	49.198093
1102.135476	137.095538	49.203098
1098.875212	137.686730	49.208103
1095.245378	148.896207	49.213108
1092.397700	138.135605	49.218113
1088.815363	145.918980	49.223117
1085.092653	152.999221	49.228122
1081.813946	138.226670	49.233127
1077.984457	136.010249	49.238132
1074.364326	122.911168	49.243137
1071.032563	132.536040	49.248141
1067.296918	136.691765	49.253146
1064.300184	143.320475	49.258151
1060.342640	146.936981	49.263156
1056.911637	141.334191	49.268161
1053.592929	137.455540	49.273165
1049.786353	148.774818	49.278170
1046.558985	142.702154	49.283175
1042.927506	149.231843	49.288180
1039.692030	136.393454	49.293185
1035.917502	144.033663	49.298189
1032.214215	153.863051	49.303194
1028.886649	145.357584	49.308199
1025.604214	133.830512	49.313204
1021.788711	139.395931	49.318209
1018.207277	139.189962	49.323213
1015.040170	145.000245	49.328218
1012.101955	144.814265	49.333223
1008.050860	150.556020	49.338228
1004.738046	150.864303	49.343233
1001.076240	147.267063	49.348237
997.136950	145.122979	49.353242
993.495291	152.766432	49.358247
990.271762	143.423579	49.363252
986.821085	141.190049	49.368257
983.242502	147.694852	49.373261
979.592325	152.814302	49.378266
976.294301	147.885821	49.383271
972.998097	155.203211	49.388276
969.577120	146.160624	49.393281
966.222005	150.277746	49.398285
962.381296	148.079719	49.403290
959.294032	137.042849	49.408295
955.639132	148.477907	49.413300
951.888137	141.816247	49.418305
947.919921	139.832551	49.423309
944.643167	147.026278	49.428314
941.492432	134.067411	49.433319
937.656802	144.878814	49.438324
934.255829	128.380331	49.443329
930.758023	138.662303	49.448333
927.067728	131.396827	49.453338
924.137734	134.793527	49.458343
920.357958	142.485464	49.463348
917.066971	139.822494	49.468353
913.195933	151.095354	49.473357
909.761155	140.075144	49.478362
906.381637	129.399701	49.483367
902.735906	140.486682	49.488372
899.640695	135.092643	49.493377
895.707423	128.125493	49.498381
892.265461	143.258481	49.503386
888.771650	132.587120	49.508391
885.311928	136.225108	49.513396
881.677012	133.681791	49.518401
878.454629	129.444795	49.523405
874.456538	135.543289	49.528410
871.470956	128.708143	49.533415
867.835864	143.372545	49.538420
864.623754	128.286666	49.543425
860.923156	128.678880	49.548429
857.416577	133.189244	49.553434
853.901501	122.968437	49.558439
849.913023	133.304132	49.563444
846.949027	128.365560	49.568449
843.168714	136.220897	49.573453
839.615171	144.518068	49.578458
836.196804	126.070606	49.583463
832.709477	137.249549	49.588468
829.216936	135.772314	49.593473
826.017867	133.893826	49.598477
822.222020	140.672832	49.603482
819.087511	134.707000	49.608487
815.150288	137.948643	49.613492
811.617522	136.939576	49.618497
808.371236	133.266142	49.623501
804.560790	144.016324	49.628506
801.590500	131.058233	49.633511
797.732608	137.535445	49.638516
794.604295	136.148337	49.643521
790.674695	137.175278	49.648525
786.862078	143.480955	49.653530
783.548454	134.935156	49.658535
780.245988	136.962310	49.663540
776.488264	129.778308	49.668545
773.086672	125.126713	49.673549
769.493403	126.149229	49.678554
766.119836	127.118300	49.683559
762.837051	137.778795	49.688564
759.454027	123.173356	49.693569
755.847199	124.519146	49.698573
751.922921	134.193748	49.703578
748.450699	133.229866	49.708583
744.919740	135.238831	49.713588
741.891870	134.405495	49.718593
738.476125	120.216380	49.723597
734.806910	131.591139	49.728602
731.250069	124.096869	49.733607
727.574317	132.002670	49.738612
724.058013	119.979501	49.743617
720.688800	127.867928	49.748621
717.162291	122.877983	49.753626
713.683858	118.945986	49.758631
710.011259	132.728331	49.763636
706.813026	114.534277	49.768641
703.348275	132.764157	49.773645
699.476443	132.968681	49.778650
695.648396	122.661542	49.783655
692.420572	134.506234	49.788660
689.026225	124.921361	49.793665
685.547238	128.454893	49.798669
682.278556	128.237409	49.803674
678.819331	128.280870	49.808679
675.014315	119.784135	49.813684
671.709181	130.135413	49.818689
668.289965	139.489872	49.823693
664.566941	134.333123	49.828698
661.307771	120.148982	49.833703
657.684062	128.436306	49.838708
653.805369	120.757972	49.843713
650.770215	124.118478	49.848717
646.793243	127.826911	49.853722
643.799978	122.625819	49.858727
639.831403	137.374582	49.863732
636.795161	124.519433	49.868737
633.058427	128.533692	49.873741
629.281309	121.067283	49.878746
626.076032	119.679159	49.883751
622.553343	126.412652	49.888756
619.297135	121.755779	49.893761
615.466706	112.818839	49.898765
611.985217	125.927107	49.903770
608.651997	130.442994	49.908775
605.192123	128.125855	49.913780
601.562704	124.948222	49.918785
597.772866	121.814648	49.923789
594.469646	134.561805	49.928794
591.175577	120.583351	49.933799
586.804286	126.129796	49.938804
584.055842	127.765230	49.943809
580.983721	133.032386	49.948813
576.996424	126.534011	49.953818
573.981412	122.231556	49.958823
570.142266	128.205007	49.963828
566.773066	117.467604	49.968833
562.832769	111.107297	49.973837
559.167789	121.596382	49.978842
555.720561	120.349969	49.983847
552.458141	129.437557	49.988852
548.919628	127.266327	49.993857
545.590540	120.350467	49.998861
542.153628	117.002068	50.003866
538.671543	119.841939	50.008871
534.609707	119.374131	50.013876
531.285388	117.969313	50.018881
527.866901	113.363467	50.023885
524.212801	108.505704	50.028890
521.146721	120.482765	50.033895
517.692503	126.515785	50.038900
514.077421	117.228925	50.043905
510.643693	108.422465	50.048909
506.922181	131.605226	50.053914
503.722207	119.592501	50.058919
499.894637	121.774398	50.063924
496.182879	115.826848	50.068929
492.746367	120.098606	50.073933
489.272677	133.489474	50.078938
485.784107	126.372981	50.083943
482.482722	132.108090	50.088948
479.033399	116.248532	50.093953
475.532917	122.704160	50.098957
471.760741	127.270320	50.103962
468.512995	122.472336	50.108967
465.081524	133.380465	50.113972
461.564923	125.695721	50.118977
458.118671	118.935215	50.123981
454.163352	137.554417	50.128986
450.959777	130.267350	50.133991
447.270189	124.953188	50.138996
444.044766	118.686193	50.144001
440.274785	120.666231	50.149005
436.634064	121.566045	50.154010
433.039344	122.876859	50.159015
429.513128	131.408835	50.164020
426.192545	128.898703	50.169025
422.882348	129.604919	50.174029
419.657657	133.798613	50.179034
416.222377	131.198417	50.184039
412.432495	130.714371	50.189044
408.682263	126.845203	50.194049
405.505982	121.689560	50.199053
401.841813	116.748491	50.204058
398.418055	115.772749	50.209063
395.113847	124.524372	50.214068
391.300458	120.433018	50.219073
387.738173	130.291186	50.224077
384.272266	126.194129	50.229082
380.958888	112.834031	50.234087
377.294652	132.762088	50.239092
373.934303	133.269436	50.244097
370.403849	119.094982	50.249101
366.467087	126.747018	50.254106
363.252489	116.636124	50.259111
359.807224	114.609521	50.264116
356.155548	116.838998	50.269121
352.713781	110.050392	50.274125
348.968844	122.525997	50.279130
345.939366	107.150545	50.284135
342.421800	113.627503	50.289140
339.252735	116.993591	50.294145
335.280814	122.160684	50.299149
331.507737	126.432481	50.304154
327.995563	122.319325	50.309159
324.523021	115.760161	50.314164
321.510435	121.130054	50.319169
318.129076	123.533912	50.324173
314.247195	119.820035	50.329178
310.921727	116.643860	50.334183
307.280896	126.718663	50.339188
303.582993	121.510147	50.344193
300.211654	111.191277	50.349197
296.707194	121.288342	50.354202
293.398029	115.011196	50.359207
289.813911	111.897398	50.364212
286.270078	117.475037	50.369217
282.723249	114.610403	50.374221
278.998009	123.220509	50.379226
275.751205	121.650300	50.384231
271.750093	133.718005	50.389236
268.887619	109.754241	50.394241
265.404773	116.824144	50.399245
261.496932	130.659252	50.404250
258.276316	122.806067	50.409255
254.806319	123.189725	50.414260
250.979992	117.649372	50.419265
247.716153	115.892475	50.424269
244.069610	130.941394	50.429274
240.533815	124.838159	50.434279
236.501349	127.259460	50.439284
233.647726	124.636964	50.444289
230.632481	124.684755	50.449293
226.640852	130.071915	50.454298
223.149705	130.931054	50.459303
219.834160	128.855569	50.464308
216.086221	129.598007	50.469313
212.807792	122.247385	50.474317
209.258774	124.091404	50.479322
205.671866	118.028702	50.484327
202.042213	124.185170	50.489332
198.630551	115.497490	50.494337
195.149238	117.340886	50.499341
191.704823	123.705106	50.504346
188.103013	117.492553	50.509351
184.458667	118.722122	50.514356
180.703290	122.677449	50.519361
177.861256	127.867689	50.524365
174.648617	131.105599	50.529370
170.798928	121.927771	50.534375
167.103355	128.909850	50.539380
163.078991	122.683566	50.544385
160.072819	119.521114	50.549389
156.452044	130.311283	50.554394
153.194857	114.241348	50.559399
149.741843	117.390733	50.564404
146.367863	114.483117	50.569409
142.630111	113.764402	50.574413
138.879020	117.749133	50.579418
135.364344	112.043613	50.584423
132.145258	113.202156	50.589428
128.671842	112.829660	50.594433
125.369841	108.376561	50.599437
121.871067	120.160366	50.604442
118.359525	116.947663	50.609447
114.430992	119.142023	50.614452
110.643129	121.105274	50.619457
107.903770	106.500288	50.624461
103.912480	127.280205	50.629466
100.699529	114.638584	50.634471
97.141316	112.961190	50.639476
93.507663	118.212516	50.644481
89.890247	121.308890	50.649485
86.271648	127.272298	50.654490
83.047583	119.867094	50.659495
79.215325	111.078317	50.664500
76.164778	118.116536	50.669505
72.876335	112.554507	50.674509
69.304305	124.737863	50.679514
65.586122	116.751749	50.684519
61.835998	119.338313	50.689524
57.939069	122.538804	50.694529
55.060616	123.246771	50.699533
51.769475	123.679810	50.704538
48.227533	110.409202	50.709543
44.412010	121.481887	50.714548
40.874733	130.714351	50.719553
37.596377	119.852174	50.724557
33.715912	124.153619	50.729562
30.464064	118.935102	50.734567
26.750290	107.497220	50.739572
23.601948	113.359268	50.744577
20.503787	122.982361	50.749581
16.522877	119.077668	50.754586
13.473997	129.469438	50.759591
9.246042	116.939075	50.764596
5.487495	121.775424	50.769601
2.162828	104.357873	50.774605