Thu Jun 16 18:29:56 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
2.537108	103.802302	0.000000
2.448415	111.796582	0.005005
2.435357	110.033674	0.010010
2.007202	92.549575	0.015014
2.289520	72.806672	0.020019
2.127068	73.378074	0.025024
1.394747	54.373399	0.030029
1.299858	50.407143	0.035034
1.257381	50.519111	0.040038
1.023485	33.468331	0.045043
0.765054	33.837369	0.050048
0.065898	36.290225	0.055053
-0.255720	26.603746	0.060058
-0.482181	25.060403	0.065062
-0.970796	14.749224	0.070067
-1.247370	10.426574	0.075072
-1.496875	9.703607	0.080077
-1.447607	1.458363	0.085082
-1.272961	4.317892	0.090086
-2.006898	7.222313	0.095091
-2.650636	6.028802	0.100096
-3.196259	12.319109	0.105101
-2.955130	12.269569	0.110106
-2.757956	17.319954	0.115110
-3.500420	5.751351	0.120115
-3.729826	4.534058	0.125120
-4.674438	4.186218	0.130125
-4.598170	3.783018	0.135130
-4.803661	9.987121	0.140134
-5.053899	2.734613	0.145139
-4.768314	21.679725	0.150144
-4.910145	11.411077	0.155149
-5.174234	0.608991	0.160154
-4.859021	-2.713231	0.165158
-5.484307	-0.622320	0.170163
-5.912581	3.774841	0.175168
-6.887006	11.336049	0.180173
-7.410851	1.856147	0.185178
-7.543583	8.713060	0.190182
-7.293860	14.753639	0.195187
-7.155454	-1.413417	0.200192
-7.937613	10.547981	0.205197
-7.850606	10.121795	0.210202
-8.246661	10.001460	0.215206
-8.085518	11.959643	0.220211
-8.511880	11.239070	0.225216
-9.232643	15.899837	0.230221
-9.099849	10.783040	0.235226
-9.528815	11.462118	0.240230
-9.886985	10.028050	0.245235
-9.675660	-0.639805	0.250240
-10.196041	2.489277	0.255245
-10.869946	1.485041	0.260250
-11.341379	2.787433	0.265254
-11.477994	6.293192	0.270259
-10.956993	4.691533	0.275264
-11.624172	10.707641	0.280269
-11.515056	5.776382	0.285274
-11.428394	0.771490	0.290278
-11.946377	3.463235	0.295283
-12.210600	-9.028876	0.300288
-12.633745	7.058710	0.305293
-12.671116	-10.438748	0.310298
-13.798026	3.264937	0.315302
-14.072480	7.552723	0.320307
-13.659036	-4.114265	0.325312
-14.250822	7.174117	0.330317
-14.214902	16.278238	0.335322
-14.485302	5.504224	0.340326
-14.736913	10.550146	0.345331
-14.503379	6.371976	0.350336
-15.280297	15.860125	0.355341
-15.578421	7.265044	0.360346
-15.640546	4.971110	0.365350
-16.268474	14.632043	0.370355
-15.832174	0.509309	0.375360
-16.235674	7.556288	0.380365
-17.076431	-0.922868	0.385370
-17.390566	-0.228633	0.390374
-17.419866	3.183820	0.395379
-17.307356	-2.435127	0.400384
-17.837524	9.188068	0.405389
-17.373483	-1.729219	0.410394
-18.007180	4.893802	0.415398
-18.573858	4.927845	0.420403
-18.785771	4.638666	0.425408
-19.169445	13.518730	0.430413
-18.813847	7.274780	0.435418
-19.267046	5.517046	0.440422
-20.116275	-1.571058	0.445427
-20.145697	-7.532457	0.450432
-20.694767	10.440516	0.455437
-20.584919	12.993086	0.460442
-20.575027	-2.191830	0.465446
-20.796502	12.330521	0.470451
-20.700846	4.525010	0.475456
-21.742141	10.620903	0.480461
-21.723532	1.346332	0.485466
-21.931377	12.104727	0.490470
-22.200150	14.814382	0.495475
-22.123254	8.031765	0.500480
-23.354343	10.493506	0.505485
-23.462230	12.225245	0.510490
-23.695491	9.880274	0.515494
-23.926811	2.365081	0.520499
-23.901472	6.150791	0.525504
-24.222296	12.219758	0.530509
-24.041623	16.107361	0.535514
-23.965029	7.867563	0.540518
-24.339628	3.653162	0.545523
-24.739556	3.727424	0.550528
-25.412674	-12.398333	0.555533
-25.447538	5.499221	0.560538
-25.314139	8.049674	0.565542
-26.049003	11.884072	0.570547
-26.689062	-0.160486	0.575552
-27.036038	13.361234	0.580557
-27.162868	7.156861	0.585562
-27.276672	6.706051	0.590566
-26.945857	9.310793	0.595571
-26.902893	8.057168	0.600576
-27.723252	8.899093	0.605581
-27.984954	6.643568	0.610586
-28.437875	8.964867	0.615590
-29.074123	18.560980	0.620595
-28.811408	0.086663	0.625600
-28.705570	13.804947	0.630605
-28.889484	8.708430	0.635610
-29.430324	-0.721501	0.640614
-30.327667	7.183802	0.645619
-30.158299	8.116193	0.650624
-30.299152	5.003611	0.655629
-30.082527	-2.582453	0.660634
-30.324129	4.540073	0.665638
-31.285593	10.520369	0.670643
-31.469406	2.725235	0.675648
-31.853761	5.353955	0.680653
-31.723562	-0.317638	0.685658
-31.618146	7.027816	0.690662
-32.041254	7.841281	0.695667
-32.248894	2.059880	0.700672
-33.184640	7.321566	0.705677
-33.198328	3.969941	0.710682
-33.266328	8.675051	0.715686
-33.223523	10.846055	0.720691
-33.701192	-1.882872	0.725696
-34.599128	8.548188	0.730701
-34.652704	-13.059796	0.735706
-34.960262	0.657246	0.740710
-35.015275	2.253769	0.745715
-34.683454	-5.610596	0.750720
-35.322343	4.519273	0.755725
-35.142444	2.869412	0.760730
-35.445810	5.775482	0.765734
-36.324299	14.473817	0.770739
-36.392342	6.821342	0.775744
-37.092634	7.090662	0.780749
-36.896105	14.330693	0.785754
-37.057769	8.031449	0.790758
-37.318591	3.192210	0.795763
-36.990013	-3.269737	0.800768
-38.082626	0.770878	0.805773
-38.397691	4.845671	0.810778
-38.401811	-5.356635	0.815782
-38.523353	2.741275	0.820787
-38.260221	-5.873450	0.825792
-38.810560	0.729578	0.830797
-39.525805	2.325414	0.835802
-40.136993	-2.408170	0.840806
-40.021000	3.557821	0.845811
-39.964920	0.904289	0.850816
-39.929923	8.530610	0.855821
-39.951851	2.690795	0.860826
-40.493989	1.654327	0.865830
-40.929321	4.775077	0.870835
-41.230082	-3.577065	0.875840
-41.530110	-3.798900	0.880845
-41.661348	3.383914	0.885850
-42.801709	-0.784725	0.890854
-43.022773	-2.453063	0.895859
-42.269167	-0.147373	0.900864
-42.939907	5.082453	0.905869
-43.195530	0.661737	0.910874
-43.045438	-3.624281	0.915878
-43.273457	0.148349	0.920883
-43.268719	5.515741	0.925888
-43.943636	5.930034	0.930893
-44.076863	3.703295	0.935898
-44.282284	1.274310	0.940902
-44.918468	10.545834	0.945907
-45.069220	5.884628	0.950912
-45.539346	9.495425	0.955917
-45.958525	9.186735	0.960922
-45.995434	2.153110	0.965926
-46.319331	1.792466	0.970931
-46.195819	5.279798	0.975936
-46.388016	0.975174	0.980941
-46.752227	-5.521341	0.985946
-47.605802	2.153175	0.990950
-47.785994	11.519221	0.995955
-47.794500	5.096901	1.000960
-47.987915	11.878406	1.005965
-48.080903	1.572398	1.010970
-47.777141	4.963546	1.015974
-48.060450	6.823916	1.020979
-48.418976	4.462063	1.025984
-49.273102	1.198236	1.030989
-49.206459	-4.085990	1.035994
-49.422278	2.240470	1.040998
-49.521411	12.713147	1.046003
-50.075437	14.764170	1.051008
-50.576131	15.972649	1.056013
-50.665257	6.824995	1.061018
-50.791377	2.758948	1.066022
-50.960385	12.704420	1.071027
-50.950857	9.220805	1.076032
-52.014802	9.783645	1.081037
-52.327871	4.184028	1.086042
-52.497048	8.017572	1.091046
-52.768561	10.494756	1.096051
-52.728132	0.010135	1.101056
-52.544289	14.655604	1.106061
-52.745819	7.938637	1.111066
-52.639425	15.055249	1.116070
-53.542667	11.381044	1.121075
-53.754380	6.715509	1.126080
-54.208184	10.161619	1.131085
-54.006121	14.082186	1.136090
-54.666720	10.388794	1.141094
-55.435968	10.769943	1.146099
-55.481076	0.872050	1.151104
-55.723341	-1.777159	1.156109
-55.870125	0.944001	1.161114
-55.607936	11.874108	1.166118
-55.664132	10.176450	1.171123
-55.575501	-8.357082	1.176128
-56.451026	9.708413	1.181133
-56.804475	0.318055	1.186138
-56.983381	3.291457	1.191142
-57.113805	6.391313	1.196147
-57.806212	1.218132	1.201152
-58.510773	5.225298	1.206157
-58.846847	9.017170	1.211162
-58.304816	5.588202	1.216166
-58.800928	17.730025	1.221171
-58.797477	6.251448	1.226176
-59.100365	17.101022	1.231181
-59.109809	8.277204	1.236186
-59.457871	0.290108	1.241190
-59.597279	9.042094	1.246195
-60.084533	-6.567140	1.251200
-60.531341	1.596167	1.256205
-60.459979	-4.155475	1.261210
-60.714368	1.065324	1.266214
-60.963230	9.059085	1.271219
-61.353251	9.227605	1.276224
-61.870934	12.017761	1.281229
-61.991863	13.478381	1.286234
-62.410998	9.661917	1.291238
-62.460899	10.535345	1.296243
-62.413660	7.568170	1.301248
-62.457648	10.948522	1.306253
-63.290298	2.648771	1.311258
-63.546429	-0.635357	1.316262
-63.741271	2.922445	1.321267
-63.782982	2.535093	1.326272
-63.719064	10.290309	1.331277
-64.424771	-10.365013	1.336282
-64.983325	11.682479	1.341286
-65.417173	4.369560	1.346291
-65.378746	-0.217841	1.351296
-65.646025	4.794363	1.356301
-65.682126	11.834191	1.361306
-65.270795	-0.963621	1.366310
-65.525595	17.312226	1.371315
-65.991292	3.151520	1.376320
-66.555927	4.478100	1.381325
-67.183742	10.116269	1.386330
-66.986580	0.414615	1.391334
-67.323049	6.742174	1.396339
-67.198995	6.516448	1.401344
-68.302075	7.287014	1.406349
-68.710004	-3.927932	1.411354
-68.547271	-4.786803	1.416358
-68.813791	4.817451	1.421363
-68.645416	-6.183557	1.426368
-68.961653	2.939389	1.431373
-69.001618	8.827568	1.436378
-69.265739	-3.359217	1.441382
-70.001432	16.039478	1.446387
-69.997084	14.351248	1.451392
-70.385588	12.571678	1.456397
-70.617256	16.831974	1.461402
-71.292804	9.771996	1.466406
-71.791202	9.190104	1.471411
-71.530799	2.083666	1.476416
-71.743210	18.258957	1.481421
-71.966146	7.063348	1.486426
-72.034877	16.722230	1.491430
-72.200768	9.555526	1.496435
-72.175190	5.641394	1.501440
-72.889264	3.450773	1.506445
-73.384798	4.270784	1.511450
-73.479492	10.586206	1.516454
-73.563683	19.780811	1.521459
-73.519988	11.669475	1.526464
-74.121241	10.864556	1.531469
-74.764177	13.020051	1.536474
-75.180410	14.093226	1.541478
-75.438611	11.744488	1.546483
-75.326053	-1.647961	1.551488
-75.474778	12.002288	1.556493
-75.395159	8.383476	1.561498
-75.378275	0.123761	1.566502
-75.712541	6.960112	1.571507
-76.084572	6.996322	1.576512
-76.451178	4.228857	1.581517
-76.527003	10.305276	1.586522
-77.064237	1.702865	1.591526
-78.063162	6.246235	1.596531
-78.028697	4.472526	1.601536
-78.676683	11.755053	1.606541
-77.990829	6.900134	1.611546
-78.494095	9.902581	1.616550
-78.605452	20.449102	1.621555
-78.298282	10.627646	1.626560
-78.502455	10.831549	1.631565
-79.370944	8.861390	1.636570
-79.705190	-2.793302	1.641574
-80.211331	8.712664	1.646579
-79.849417	-6.023729	1.651584
-80.136688	6.063047	1.656589
-80.754240	0.051364	1.661594
-81.284302	2.261306	1.666598
-81.691384	-2.862247	1.671603
-81.447845	6.005699	1.676608
-81.600728	-7.159968	1.681613
-81.840271	4.278650	1.686618
-81.720748	0.073944	1.691622
-82.858254	4.739464	1.696627
-82.863940	-3.086383	1.701632
-83.316977	6.324555	1.706637
-83.145550	10.426379	1.711642
-83.303085	6.222279	1.716646
-83.517466	19.990130	1.721651
-83.359902	1.779046	1.726656
-84.042536	15.725701	1.731661
-84.556757	-1.591031	1.736666
-84.737796	4.657959	1.741670
-84.811645	8.064160	1.746675
-84.670785	9.428436	1.751680
-85.404489	19.227016	1.756685
-86.130820	12.763710	1.761690
-86.161497	15.413692	1.766694
-86.587097	8.110461	1.771699
-86.363823	3.081908	1.776704
-86.461936	2.803815	1.781709
-86.882604	3.316477	1.786714
-86.470342	7.502307	1.791718
-87.539961	-2.737777	1.796723
-87.545154	2.385603	1.801728
-87.956626	1.708055	1.806733
-88.268169	3.136842	1.811738
-88.403357	5.210588	1.816742
-89.043063	1.282307	1.821747
-89.335838	5.171398	1.826752
-89.715810	4.546061	1.831757
-89.789629	13.324498	1.836762
-89.420268	-2.533944	1.841766
-89.947920	13.582160	1.846771
-89.723646	0.343695	1.851776
-90.060243	7.569920	1.856781
-90.554382	10.175845	1.861786
-90.889166	-5.725443	1.866790
-91.487408	0.151414	1.871795
-91.437611	1.896453	1.876800
-91.829382	4.823647	1.881805
-91.877607	8.265666	1.886810
-92.095938	2.556082	1.891814
-92.677634	3.115780	1.896819
-93.172637	5.449166	1.901824
-93.243217	-9.148260	1.906829
-93.456161	-3.908663	1.911834
-93.399008	-7.896969	1.916838
-93.771131	0.937768	1.921843
-93.495347	0.731556	1.926848
-93.801286	7.060382	1.931853
-94.426513	5.112173	1.936858
-94.781892	1.638756	1.941862
-95.153201	10.518251	1.946867
-94.959306	4.762634	1.951872
-95.097473	9.765635	1.956877
-95.770425	3.063648	1.961882
-96.074582	7.018154	1.966886
-96.432795	5.933634	1.971891
-96.546476	-1.639270	1.976896
-96.521275	-5.305022	1.981901
-96.631215	-5.806683	1.986906
-96.838152	-4.885598	1.991910
-97.577307	6.566833	1.996915
-97.840494	2.897723	2.006912
-97.722129	2.692557	2.016909
-96.569485	3.969892	2.026906
-96.430414	6.513243	2.036902
-96.273771	-1.623791	2.046899
-95.656660	4.945293	2.056896
-95.092289	-4.557801	2.066893
-94.367902	4.660637	2.076890
-93.957178	0.596923	2.086886
-93.569936	3.093921	2.096883
-92.511156	-7.070829	2.106880
-92.582454	-0.843546	2.116877
-92.128296	-1.510694	2.126874
-91.231396	3.370062	2.136870
-91.169348	11.010500	2.146867
-90.431068	7.178025	2.156864
-89.389776	7.275207	2.166861
-89.342687	-1.961477	2.176858
-89.559494	7.245038	2.186854
-88.174745	5.808136	2.196851
-87.987088	6.499661	2.206848
-87.425271	7.283938	2.216845
-86.589678	12.611888	2.226842
-86.612098	10.791016	2.236838
-86.090868	14.081161	2.246835
-85.133376	7.888187	2.256832
-84.792891	7.595635	2.266829
-84.602580	9.691980	2.276826
-84.068234	-3.372542	2.286822
-83.799816	3.478654	2.296819
-82.875307	8.692830	2.306816
-81.855226	4.326692	2.316813
-81.836460	13.769580	2.326810
-82.018344	10.550147	2.336806
-80.741185	4.795036	2.346803
-80.285119	2.880660	2.356800
-80.015166	6.141064	2.366797
-78.870579	3.548903	2.376794
-78.638821	15.251718	2.386790
-78.399357	10.496192	2.396787
-78.405157	8.365413	2.406784
-77.427496	8.995517	2.416781
-76.885759	1.987664	2.426778
-76.302444	12.354147	2.436774
-75.280456	9.943211	2.446771
-75.006699	9.047271	2.456768
-75.266732	7.178298	2.466765
-74.970774	13.785404	2.476762
-74.337845	10.860210	2.486758
-72.988919	14.460001	2.496755
-72.721609	10.580753	2.506752
-72.483035	13.564622	2.516749
-71.998584	8.862794	2.526746
-71.237600	2.014834	2.536742
-71.048741	6.654734	2.546739
-70.463516	9.693228	2.556736
-69.704064	12.193268	2.566733
-69.786481	13.566469	2.576730
-68.659601	5.377684	2.586726
-68.279319	10.856900	2.596723
-67.801013	4.958616	2.606720
-67.460967	13.676647	2.616717
-66.748681	8.884316	2.626714
-66.396568	3.468641	2.636710
-65.850329	3.727313	2.646707
-64.993286	9.572148	2.656704
-64.836102	7.676992	2.666701
-64.703032	1.174627	2.676698
-63.925148	1.940828	2.686694
-63.324164	4.742805	2.696691
-62.864281	12.427685	2.706688
-61.976136	1.791744	2.716685
-61.614428	3.541836	2.726682
-61.502668	0.943360	2.736678
-61.259351	5.696501	2.746675
-60.140636	10.286443	2.756672
-60.039591	6.064246	2.766669
-59.146332	8.752773	2.776666
-58.642811	14.766377	2.786662
-58.530269	8.115920	2.796659
-58.247705	3.485985	2.806656
-57.265523	9.885935	2.816653
-56.825794	9.219741	2.826650
-55.896246	4.476704	2.836646
-55.673385	8.021183	2.846643
-55.576729	5.669341	2.856640
-54.948025	7.344388	2.866637
-54.265153	1.586892	2.876634
-53.798677	10.165935	2.886630
-53.420417	5.364455	2.896627
-52.469328	-5.514019	2.906624
-52.412579	2.204936	2.916621
-52.100011	10.820677	2.926618
-51.347816	15.512389	2.936614
-50.696404	9.918090	2.946611
-50.456619	2.503772	2.956608
-49.297231	4.589710	2.966605
-49.024209	6.466181	2.976602
-49.201007	7.605607	2.986598
-48.782292	6.915376	2.996595
-47.668567	8.986636	3.006592
-47.279466	8.194517	3.016589
-46.596869	5.772951	3.026586
-46.268156	4.297172	3.036582
-46.196910	4.726955	3.046579
-45.258205	6.614861	3.056576
-44.388283	4.911738	3.066573
-44.563884	8.378099	3.076570
-43.933100	4.092949	3.086566
-43.078070	5.825719	3.096563
-42.980819	3.857887	3.106560
-42.289205	5.345227	3.116557
-41.664748	10.979134	3.126554
-41.437261	13.923695	3.136550
-40.711376	11.025073	3.146547
-39.853996	1.565761	3.156544
-39.575202	5.886060	3.166541
-39.668759	7.847515	3.176538
-38.950942	7.294795	3.186534
-38.370753	9.842246	3.196531
-37.930411	7.048406	3.206528
-36.896964	15.706322	3.216525
-36.497801	15.975376	3.226522
-36.261614	13.724294	3.236518
-36.287345	9.252239	3.246515
-35.181919	7.757198	3.256512
-34.863352	15.945515	3.266509
-34.142498	11.143225	3.276506
-33.395209	15.737761	3.286502
-33.439872	11.558262	3.296499
-33.292360	17.982666	3.306496
-32.334134	9.544032	3.316493
-31.883518	10.666546	3.326490
-30.828708	14.447965	3.336486
-30.211045	10.983136	3.346483
-30.451481	8.025812	3.356480
-30.239790	11.958622	3.366477
-29.050325	6.011854	3.376474
-28.546211	13.499771	3.386470
-28.510921	15.464184	3.396467
-27.605004	15.502106	3.406464
-27.182576	8.949050	3.416461
-26.935916	9.990586	3.426458
-26.199582	12.092118	3.436454
-25.414693	18.788430	3.446451
-25.140675	11.879789	3.456448
-25.056041	14.689516	3.466445
-24.243334	9.552589	3.476442
-23.646618	9.788895	3.486438
-23.636276	9.358335	3.496435
-22.608288	13.980962	3.506432
-22.049970	17.851549	3.516429
-22.187468	6.937582	3.526426
-21.052929	5.818730	3.536422
-20.743893	7.115185	3.546419
-20.388680	6.083049	3.556416
-19.372731	9.516959	3.566413
-19.139482	5.692287	3.576410
-19.132368	10.151627	3.586406
-18.076415	4.031439	3.596403
-17.736776	6.823518	3.606400
-17.412327	14.447121	3.616397
-16.379646	14.571570	3.626394
-16.118340	13.225815	3.636390
-16.072467	10.963314	3.646387
-15.147040	8.662533	3.656384
-14.473381	2.756760	3.666381
-14.058308	10.268480	3.676378
-14.146273	10.434703	3.686374
-13.074047	9.695394	3.696371
-12.858612	7.989656	3.706368
-12.168679	9.662541	3.716365
-11.187339	12.967337	3.726362
-11.097586	7.712124	3.736358
-11.021037	9.063597	3.746355
-10.449714	10.198663	3.756352
-9.327259	6.453147	3.766349
-9.006538	6.988736	3.776346
-9.080884	2.787869	3.786342
-8.317244	6.069768	3.796339
-7.804153	-0.584553	3.806336
-7.141430	3.103369	3.816333
-6.151438	11.530904	3.826330
-5.932314	7.121313	3.836326
-6.145743	3.711256	3.846323
-5.609433	3.362094	3.856320
-4.746929	1.728214	3.866317
-4.448993	12.232802	3.876314
-3.757903	19.862100	3.886310
-3.493196	21.370755	3.896307
-2.825915	29.347949	3.906304
-2.617397	25.699140	3.916301
-2.046147	42.940702	3.926298
-1.833302	58.582185	3.936294
-1.029567	90.504115	3.946291
-0.526527	102.302198	3.956288
0.000000	103.163474	3.961293
0.075551	108.629696	3.966298
0.092737	116.490857	3.971302
0.400769	112.272526	3.976307
0.127440	117.687393	3.981312
0.304908	107.670067	3.986317
0.018654	119.285888	3.991322
0.181823	124.561141	3.996326
0.784849	138.626921	4.001331
0.814094	152.434253	4.006336
1.071067	140.816494	4.011341
0.485096	131.105861	4.016346
0.352273	126.300574	4.021350
0.068983	135.337358	4.026355
0.616946	140.739824	4.031360
0.650280	132.099857	4.036365
0.410425	139.693533	4.041370
0.547652	152.089608	4.046374
1.164662	144.334503	4.051379
1.061864	152.988478	4.056384
0.898728	149.818381	4.061389
0.696622	155.025363	4.066394
0.778266	150.304393	4.071398
0.990406	152.125323	4.076403
0.992928	163.721175	4.081408
0.791348	142.639483	4.086413
0.636354	149.120116	4.091418
0.690019	150.783736	4.096422
0.965925	156.685873	4.101427
0.901329	146.334127	4.106432
0.742940	146.487843	4.111437
0.742363	158.636380	4.116442
0.712440	159.803172	4.121446
0.965541	144.492084	4.126451
0.504029	164.488895	4.131456
0.825678	160.990953	4.136461
0.814568	152.453128	4.141466
0.663514	152.646081	4.146470
0.791626	147.943379	4.151475
0.591919	153.659127	4.156480
0.610089	146.644544	4.161485
0.750812	158.523287	4.166490
0.820996	174.035254	4.171494
1.320787	169.894429	4.176499
1.306649	183.153131	4.181504
1.451188	170.769518	4.186509
0.972641	152.842032	4.191514
0.935501	160.800589	4.196518
1.016460	161.260736	4.201523
1.317310	171.750492	4.206528
1.566026	171.051826	4.211533
1.039885	164.691205	4.216538
0.994021	158.143877	4.221542
1.093774	152.115290	4.226547
0.613411	157.016552	4.231552
1.213934	164.362638	4.236557
1.194954	175.078788	4.241562
1.207117	182.583284	4.246566
1.443179	179.705625	4.251571
0.917104	192.365747	4.256576
1.247564	180.617526	4.261581
1.449363	186.315766	4.266586
1.109192	180.835985	4.271590
1.370536	173.749238	4.276595
1.277726	190.214240	4.281600
1.459852	179.194937	4.286605
1.503982	183.196011	4.291610
1.675442	183.559417	4.296614
1.394851	168.426873	4.301619
1.115536	165.383014	4.306624
1.434520	157.320415	4.311629
1.061983	159.453632	4.316634
1.021631	164.948992	4.321638
1.582048	169.969488	4.326643
1.682826	192.980477	4.331648
1.410625	181.387494	4.336653
1.462690	178.463685	4.341658
1.370513	180.905043	4.346662
1.582944	173.362401	4.351667
1.439657	180.905905	4.356672
1.361910	174.546944	4.361677
1.524300	181.323493	4.366682
1.465251	177.226482	4.371686
1.412511	175.041169	4.376691
1.617785	181.848712	4.381696
1.632092	180.368461	4.386701
1.536404	185.898526	4.391706
1.608204	181.754140	4.396710
1.607541	175.550451	4.401715
1.406678	179.829279	4.406720
1.686384	183.162491	4.411725
1.712660	193.183444	4.416730
1.480622	195.623943	4.421734
1.457886	184.305924	4.426739
1.752867	188.395177	4.431744
1.655163	187.100066	4.436749
1.512358	190.407704	4.441754
1.445085	192.078587	4.446758
1.782188	181.739160	4.451763
1.356781	192.916224	4.456768
1.916043	191.083487	4.461773
1.865767	196.636930	4.466778
1.495480	188.668396	4.471782
1.540398	200.717204	4.476787
1.192418	194.002549	4.481792
1.985826	203.228534	4.486797
2.243230	213.267340	4.491802
1.935207	203.050692	4.496806
1.684338	184.628765	4.501811
1.428201	192.353608	4.506816
1.855194	210.246702	4.511821
2.040604	214.648262	4.516826
1.766149	213.799379	4.521830
2.303405	210.896109	4.526835
1.959346	209.073253	4.531840
1.695017	193.200346	4.536845
2.131926	201.805506	4.541850
1.723663	208.674500	4.546854
2.119034	205.012336	4.551859
2.165050	212.211141	4.556864
2.127337	201.917068	4.561869
1.799592	193.220819	4.566874
1.568904	205.087480	4.571878
1.975270	203.248636	4.576883
1.766109	217.868692	4.581888
2.218920	213.534657	4.586893
2.159264	217.049252	4.591898
1.970403	223.855948	4.596902
2.244535	221.614537	4.601907
2.268347	222.622595	4.606912
2.344518	216.953438	4.611917
2.417208	222.613539	4.616922
2.067986	218.417080	4.621926
2.442955	219.856143	4.626931
2.147554	206.128702	4.631936
2.083284	197.195838	4.636941
2.334702	225.227742	4.641946
2.002226	214.777268	4.646950
2.254673	205.877000	4.651955
2.098181	214.625616	4.656960
2.407009	213.349939	4.661965
2.459823	222.996269	4.666970
1.963459	221.225022	4.671974
2.315534	217.200840	4.676979
2.179783	224.478327	4.681984
2.616342	218.319765	4.686989
2.493174	221.509229	4.691994
2.229675	202.784224	4.696998
2.569549	203.544511	4.702003
2.099929	206.501771	4.707008
2.055412	199.506995	4.712013
2.438844	211.705172	4.717018
2.352075	217.103943	4.722022
2.487192	216.129560	4.727027
2.709755	230.201968	4.732032
2.418540	225.110185	4.737037
2.638454	224.713627	4.742042
2.483636	221.047774	4.747046
2.433392	212.850728	4.752051
2.299559	213.716235	4.757056
2.347579	219.153207	4.762061
2.519238	222.083514	4.767066
2.267934	218.659826	4.772070
2.337381	205.333702	4.777075
2.265801	209.387843	4.782080
2.375680	219.247703	4.787085
2.105696	223.733504	4.792090
2.347764	233.745359	4.797094
2.422020	218.870119	4.802099
2.277511	216.791716	4.807104
2.437225	228.578289	4.812109
2.968993	231.762417	4.817114
2.582440	236.643958	4.822118
2.595921	214.747833	4.827123
2.269537	247.326530	4.832128
2.723566	243.379709	4.837133
3.195241	244.246963	4.842138
2.802436	251.908196	4.847142
2.752568	230.712322	4.852147
2.240888	225.698409	4.857152
2.582489	244.553741	4.862157
2.602180	247.025950	4.867162
2.718790	243.819565	4.872166
3.236661	236.513702	4.877171
3.165184	240.093199	4.882176
3.045550	239.519432	4.887181
2.734507	222.405720	4.892186
2.611233	234.039976	4.897190
2.884764	233.029498	4.902195
2.797452	252.953335	4.907200
3.010676	244.530612	4.912205
3.127838	249.729456	4.917210
2.670133	246.104576	4.922214
2.800836	229.511171	4.927219
2.687138	246.075678	4.932224
2.931461	254.584935	4.937229
3.164788	236.417272	4.942234
2.633656	255.137058	4.947238
3.012776	236.267335	4.952243
2.884019	246.013141	4.957248
3.058715	250.396356	4.962253
2.875436	246.513914	4.967258
2.810715	241.450104	4.972262
3.169359	244.046047	4.977267
2.990695	250.378210	4.982272
3.299233	240.303127	4.987277
3.191167	244.190264	4.992282
3.251379	240.397515	4.997286
3.417536	239.874483	5.002291
3.349098	240.760952	5.007296
3.214199	248.020452	5.012301
3.259962	229.790860	5.017306
2.890842	232.477082	5.022310
3.123421	224.046435	5.027315
3.094960	240.841320	5.032320
3.233409	246.928991	5.037325
3.064340	236.810211	5.042330
2.922929	253.619237	5.047334
3.476076	229.193443	5.052339
3.267033	239.807961	5.057344
3.309936	249.174973	5.062349
3.517239	242.713924	5.067354
2.960697	236.198079	5.072358
3.220829	239.238865	5.077363
3.334233	244.076457	5.082368
3.038282	240.740547	5.087373
3.601647	226.645243	5.092378
3.015775	240.031826	5.097382
3.514064	235.629694	5.102387
2.864406	235.085018	5.107392
3.118199	238.168977	5.112397
3.127061	238.247205	5.117402
2.897129	252.470774	5.122406
3.013971	230.748839	5.127411
3.213891	255.869678	5.132416
3.224233	267.089422	5.137421
3.461270	269.749665	5.142426
3.624323	274.249944	5.147430
3.705033	255.650207	5.152435
3.606053	268.077815	5.157440
3.554695	262.842692	5.162445
3.659088	267.949929	5.167450
3.623723	263.338631	5.172454
3.534029	251.181012	5.177459
3.361193	247.725505	5.182464
3.276888	264.686804	5.187469
3.941128	255.492038	5.192474
3.491909	277.564469	5.197478
3.830691	269.148113	5.202483
3.432827	259.935996	5.207488
3.378392	255.538681	5.212493
3.838310	272.627685	5.217498
3.529662	268.133766	5.222502
3.296388	265.113848	5.227507
3.318399	277.453592	5.232512
3.448160	279.816654	5.237517
3.399541	277.441027	5.242522
3.430980	276.772345	5.247526
3.697544	274.530007	5.252531
3.409759	263.599352	5.257536
3.628707	261.802129	5.262541
3.739183	268.528497	5.267546
3.836698	276.409613	5.272550
3.882765	266.004771	5.277555
3.748936	271.004972	5.282560
3.439333	267.958106	5.287565
3.919294	283.679195	5.292570
3.929719	303.694876	5.297574
4.186616	304.309650	5.302579
3.577841	293.123226	5.307584
3.656849	296.859099	5.312589
3.996534	294.085739	5.317594
3.705686	299.905690	5.322598
4.041873	299.565781	5.327603
4.386702	297.602924	5.332608
4.379917	286.973380	5.337613
3.927129	267.606444	5.342618
3.693740	269.859041	5.347622
4.121149	276.933975	5.352627
3.877635	277.636281	5.357632
3.636008	271.019345	5.362637
3.798027	282.502308	5.367642
4.070778	288.093855	5.372646
4.415302	281.496066	5.377651
3.947010	299.641797	5.382656
3.877148	281.335358	5.387661
3.941916	303.779665	5.392666
3.849917	292.564269	5.397670
4.328707	290.940554	5.402675
4.163217	300.572992	5.407680
4.441169	297.010715	5.412685
4.288589	288.993324	5.417690
3.826526	301.207191	5.422694
4.313345	293.473724	5.427699
4.330225	298.292756	5.432704
4.170236	293.536597	5.437709
4.318719	308.003516	5.442714
3.972997	299.452440	5.447718
4.225862	285.462954	5.452723
3.933897	296.159978	5.457728
4.073011	298.053963	5.462733
3.930913	287.223028	5.467738
4.156668	296.462181	5.472742
4.102166	286.431378	5.477747
4.088804	295.006625	5.482752
4.116510	284.380263	5.487757
4.376429	296.348331	5.492762
4.270007	303.480719	5.497766
4.319645	293.720088	5.502771
4.116652	298.991491	5.507776
4.187328	303.880953	5.512781
4.254683	307.110278	5.517786
4.280511	317.809651	5.522790
4.574312	319.233232	5.527795
4.430963	330.690633	5.532800
4.621783	312.559798	5.537805
4.693317	309.138280	5.542810
4.153723	302.113496	5.547814
4.482411	296.564769	5.552819
4.492679	320.005659	5.557824
4.697841	322.846393	5.562829
4.324305	306.724056	5.567834
4.278613	312.342390	5.572838
4.674448	318.821545	5.577843
4.498494	320.727646	5.582848
4.621330	322.428589	5.587853
4.933990	334.475974	5.592858
4.731958	315.662930	5.597862
4.715470	291.691569	5.602867
4.284253	303.374894	5.607872
4.358326	310.128310	5.612877
4.691167	328.242308	5.617882
4.538241	342.100831	5.622886
5.061452	329.899377	5.627891
4.814255	323.433692	5.632896
4.536085	325.018589	5.637901
4.908998	321.297265	5.642906
4.336797	315.237992	5.647910
5.072231	318.636998	5.652915
4.924547	311.486867	5.657920
4.546397	305.861287	5.662925
4.751659	298.352030	5.667930
4.546067	324.768568	5.672934
4.998412	331.986109	5.677939
4.949905	324.979801	5.682944
4.778591	316.348788	5.687949
4.804602	317.212352	5.692954
4.726719	330.815768	5.697958
4.688378	315.097570	5.702963
4.516050	322.981771	5.707968
4.742705	327.035886	5.712973
4.755481	326.919903	5.717978
4.794210	327.633183	5.722982
5.169319	328.869691	5.727987
5.131828	324.612115	5.732992
4.820792	326.919383	5.737997
4.871038	321.336652	5.743002
4.588238	328.662463	5.748006
4.958656	322.028216	5.753011
5.017529	327.275689	5.758016
5.117595	324.600921	5.763021
5.065709	321.439927	5.768026
4.981729	324.841462	5.773030
4.923317	323.600717	5.778035
5.129294	322.020309	5.783040
4.935228	325.873534	5.788045
5.033572	319.433815	5.793050
5.070453	322.629703	5.798054
5.316363	313.124701	5.803059
5.282445	323.211428	5.808064
5.086546	320.917948	5.813069
4.928908	325.025212	5.818074
4.994867	324.634067	5.823078
5.206189	318.779851	5.828083
5.445869	319.352582	5.833088
4.902354	323.362708	5.838093
5.167034	314.418427	5.843098
4.784250	324.734176	5.848102
5.304848	317.129979	5.853107
5.047645	321.044248	5.858112
4.948158	317.667369	5.863117
5.279802	326.763943	5.868122
5.237780	341.479816	5.873126
5.625219	338.694907	5.878131
5.408524	336.681692	5.883136
5.259018	329.105459	5.888141
5.072380	324.253262	5.893146
5.147632	336.868288	5.898150
5.331899	341.732480	5.903155
5.337290	354.717388	5.908160
5.203626	355.005632	5.913165
5.606328	342.798433	5.918170
5.616273	353.982888	5.923174
5.493883	339.099679	5.928179
5.404130	348.061983	5.933184
5.443397	349.871944	5.938189
5.608812	350.477075	5.943194
5.639941	360.794392	5.948198
5.600658	344.591914	5.953203
5.556715	327.803314	5.958208
5.423980	325.089672	5.963213
5.238942	317.493765	5.968218
5.275720	324.987061	5.973222
5.601981	336.185625	5.978227
5.447656	347.063270	5.983232
5.450631	354.469133	5.988237
5.389878	349.127898	5.993242
5.257883	359.633180	5.998246
5.609050	352.851452	6.003251
5.502469	344.290624	6.008256
5.309954	348.979223	6.013261
5.452590	353.187027	6.018266
5.734957	358.872116	6.023270
5.748619	347.853600	6.028275
5.885552	355.922104	6.033280
6.009161	344.982695	6.038285
5.969076	335.413462	6.043290
5.368617	346.988050	6.048294
5.746721	321.382194	6.053299
5.702847	315.641976	6.058304
5.290730	316.864543	6.063309
5.564923	309.121418	6.068314
5.306313	320.583653	6.073318
5.318670	317.278363	6.078323
5.147129	315.363745	6.083328
5.252608	322.333559	6.088333
5.457908	316.681205	6.093338
5.388614	327.785900	6.098342
5.337693	328.260546	6.103347
5.273996	328.017405	6.108352
5.374608	346.185193	6.113357
5.562287	335.045092	6.118362
5.523622	348.499680	6.123366
5.824038	347.232092	6.128371
5.783409	351.233010	6.133376
5.677986	337.730465	6.138381
5.836453	326.874889	6.143386
5.507342	334.896488	6.148390
5.614041	332.051722	6.153395
5.804100	330.051890	6.158400
5.556080	338.215474	6.163405
5.599285	325.455927	6.168410
5.113446	329.074721	6.173414
5.261979	312.237656	6.178419
5.064402	323.641366	6.183424
5.229273	336.541597	6.188429
5.755381	330.470105	6.193434
5.273522	334.113202	6.198438
5.487690	339.879305	6.203443
5.489112	346.451573	6.208448
5.430050	347.469586	6.213453
5.737677	338.145270	6.218458
5.319955	336.705523	6.223462
5.536150	340.996075	6.228467
5.779515	351.919482	6.233472
4.859827	348.457941	6.238477
5.426001	339.676821	6.243482
5.366384	357.469371	6.248486
5.846054	353.563765	6.253491
5.787513	353.793720	6.258496
5.435733	346.131137	6.263501
5.610542	344.931563	6.268506
5.465192	345.715714	6.273510
5.578877	352.042816	6.278515
5.157326	341.429098	6.283520
5.147666	356.186399	6.288525
5.732663	348.204738	6.293530
5.407269	349.639591	6.298534
5.697726	340.836258	6.303539
5.493337	354.274140	6.308544
5.455766	346.950312	6.313549
5.990143	343.647242	6.318554
5.674016	346.335380	6.323558
5.501921	339.523421	6.328563
5.481989	328.736789	6.333568
5.006520	326.204984	6.338573
5.389545	328.831936	6.343578
5.476580	344.945663	6.348582
5.577565	344.384563	6.353587
5.535366	354.270728	6.358592
5.598787	351.351719	6.363597
6.024484	345.732089	6.368602
5.610884	340.276816	6.373606
5.448553	320.264838	6.378611
5.752764	327.587560	6.383616
5.580349	329.545562	6.388621
5.783175	310.752040	6.393626
5.744751	323.842031	6.398630
5.641909	320.448144	6.403635
5.631582	315.503870	6.408640
5.357128	307.632694	6.413645
5.553324	307.169612	6.418650
5.333435	325.611334	6.423654
5.616743	313.936114	6.428659
5.413220	316.820513	6.433664
5.415002	325.077671	6.438669
5.696038	318.757521	6.443674
5.175584	320.011903	6.448678
5.483082	316.936247	6.453683
5.495523	317.965330	6.458688
5.388280	314.868142	6.463693
5.276781	312.482776	6.468698
5.115584	323.256864	6.473702
5.423841	312.020887	6.478707
5.675522	318.311555	6.483712
5.293484	321.441909	6.488717
5.419688	331.425128	6.493722
5.338956	328.312606	6.498726
5.594578	335.004064	6.503731
5.452315	336.849154	6.508736
5.507425	338.873541	6.513741
5.768052	334.477509	6.518746
5.498134	333.436375	6.523750
5.679402	322.768823	6.528755
5.566117	322.771245	6.533760
5.306950	331.253849	6.538765
5.574871	321.861422	6.543770
5.453516	327.717204	6.548774
5.604261	322.825529	6.553779
5.584048	326.803830	6.558784
5.578457	329.342679	6.563789
5.576757	320.886768	6.568794
5.519308	329.977304	6.573798
5.354562	317.766823	6.578803
5.362800	330.900903	6.583808
5.539070	332.586703	6.588813
5.360822	328.405366	6.593818
5.275922	327.463884	6.598822
5.608380	325.449891	6.603827
5.479313	326.100433	6.608832
5.174628	321.014790	6.613837
5.883471	332.204189	6.618842
5.735826	338.059287	6.623846
5.632797	330.489382	6.628851
5.852634	317.789344	6.633856
5.190476	318.005893	6.638861
5.562872	313.795023	6.643866
5.312780	312.670111	6.648870
5.420171	318.973477	6.653875
5.322422	314.237215	6.658880
5.448115	318.942080	6.663885
5.776695	315.472654	6.668890
5.548027	322.996203	6.673894
5.533695	326.349823	6.678899
5.633684	320.923431	6.683904
5.584281	326.747788	6.688909
5.745281	329.580727	6.693914
5.983876	330.205926	6.698918
5.379023	310.196652	6.703923
5.750298	316.927395	6.708928
5.522810	323.936945	6.713933
5.714602	316.125351	6.718938
5.565861	321.409797	6.723942
5.506213	319.812415	6.728947
5.753596	320.823586	6.733952
5.717584	328.026629	6.738957
5.676641	327.404831	6.743962
5.680074	318.501552	6.748966
5.436499	303.040643	6.753971
5.368292	308.675226	6.758976
5.548116	319.952733	6.763981
5.678634	312.247359	6.768986
5.381138	317.618343	6.773990
5.386874	309.049332	6.778995
5.503427	314.855038	6.784000
5.427008	327.195107	6.789005
5.446445	322.723608	6.794010
5.440303	333.425414	6.799014
5.696605	331.439693	6.804019
5.556892	332.607575	6.809024
5.285750	328.322413	6.814029
5.696246	328.207098	6.819034
5.737868	321.669314	6.824038
5.577881	318.818408	6.829043
5.348663	298.814256	6.834048
4.980956	319.426674	6.839053
5.271941	321.294380	6.844058
5.577754	331.926873	6.849062
5.468354	331.460132	6.854067
5.484903	327.858473	6.859072
5.433047	333.574319	6.864077
5.839609	321.255214	6.869082
5.668090	325.042954	6.874086
5.559992	323.878198	6.879091
5.823114	320.799417	6.884096
5.840738	302.504540	6.889101
5.546224	295.071169	6.894106
5.274035	295.560479	6.899110
5.322191	302.705304	6.904115
5.626379	292.217436	6.909120
5.410801	298.708440	6.914125
5.688273	291.095699	6.919130
5.471779	291.964709	6.924134
5.200401	290.587204	6.929139
5.152141	302.008348	6.934144
5.585441	318.008193	6.939149
5.820777	312.417865	6.944154
5.488575	322.891884	6.949158
5.955469	312.531413	6.954163
5.391147	303.450763	6.959168
5.045611	299.076583	6.964173
5.568638	306.275525	6.969178
5.150253	318.269581	6.974182
5.719521	313.725372	6.979187
5.884441	308.388982	6.984192
5.706407	308.982305	6.989197
5.673068	291.739749	6.994202
5.253874	299.541809	6.999206
5.206118	297.453325	7.004211
5.496710	299.597529	7.009216
5.420951	298.191246	7.014221
5.658632	294.781736	7.019226
5.267921	313.602793	7.024230
5.602750	316.916663	7.029235
5.919758	306.763481	7.034240
5.067007	297.163817	7.039245
5.463747	304.823342	7.044250
5.758830	317.692074	7.049254
5.665881	297.716705	7.054259
5.400571	293.836067	7.059264
5.536786	295.982599	7.064269
5.527785	296.039905	7.069274
5.370864	291.411395	7.074278
5.420685	288.385037	7.079283
5.505676	283.376186	7.084288
5.208737	299.696077	7.089293
5.832027	305.396232	7.094298
5.443318	311.302604	7.099302
5.936234	299.756327	7.104307
5.549509	289.910357	7.109312
5.201866	295.100496	7.114317
5.666701	285.309533	7.119322
5.167884	294.888827	7.124326
5.365742	296.368710	7.129331
5.497153	300.375221	7.134336
5.558027	316.611530	7.139341
5.856960	309.625157	7.144346
5.388679	295.562065	7.149350
5.094979	294.865131	7.154355
5.355512	303.675797	7.159360
5.353050	318.043758	7.164365
5.904933	321.677219	7.169370
5.612285	325.437819	7.174374
5.300244	316.838448	7.179379
5.676532	321.390024	7.184384
5.121801	319.448855	7.189389
5.519983	311.858775	7.194394
5.654851	325.286737	7.199398
5.574503	330.514895	7.204403
5.552216	318.515082	7.209408
5.472909	322.804050	7.214413
5.597838	316.237012	7.219418
5.561930	316.590888	7.224422
5.328601	302.496359	7.229427
5.415400	308.768693	7.234432
5.278027	322.004966	7.239437
5.880707	317.187676	7.244442
5.622803	317.382504	7.249446
5.710406	324.669100	7.254451
5.394776	311.308557	7.259456
5.090555	297.553092	7.264461
5.608642	307.457326	7.269466
5.708586	325.682126	7.274470
5.839415	307.307959	7.279475
5.636079	298.755254	7.284480
5.318096	298.521284	7.289485
5.338688	286.245077	7.294490
5.205335	300.401034	7.299494
5.384759	307.186070	7.304499
5.713435	310.583334	7.309504
5.387756	315.953352	7.314509
5.414511	314.735036	7.319514
5.551034	314.500834	7.324518
5.364670	312.101104	7.329523
5.518735	309.827827	7.334528
5.196928	323.353456	7.339533
5.640452	318.447237	7.344538
5.727971	327.135662	7.349542
5.525390	315.207971	7.354547
5.681841	329.714043	7.359552
5.644903	322.387260	7.364557
5.228112	309.658167	7.369562
5.457056	324.267780	7.374566
5.345673	322.981825	7.379571
5.543089	327.999223	7.384576
5.439962	324.082501	7.389581
5.631224	314.206504	7.394586
5.392258	313.750224	7.399590
5.642919	319.037229	7.404595
5.561381	328.298476	7.409600
5.301143	331.393411	7.414605
5.695337	318.056043	7.419610
5.773180	324.196775	7.424614
5.306208	313.568187	7.429619
5.674086	310.148305	7.434624
5.293436	310.218392	7.439629
5.395729	312.136716	7.444634
5.186873	315.771786	7.449638
5.515192	319.390202	7.454643
5.559358	328.756560	7.459648
5.230732	319.154320	7.464653
5.502442	330.469727	7.469658
5.467948	323.263296	7.474662
5.497600	328.489356	7.479667
5.640102	319.835780	7.484672
5.221529	330.520209	7.489677
5.419077	317.811127	7.494682
5.339530	322.143939	7.499686
5.478354	330.534132	7.504691
5.528729	319.977005	7.509696
5.227430	324.736356	7.514701
5.475727	324.681390	7.519706
4.867125	334.257936	7.524710
5.320654	328.530321	7.529715
5.428364	327.020709	7.534720
5.436612	333.128156	7.539725
5.332792	329.943088	7.544730
5.461915	340.921673	7.549734
5.661208	343.733883	7.554739
5.809206	327.707850	7.559744
5.338264	323.094328	7.564749
5.716331	316.984166	7.569754
5.569079	326.067442	7.574758
5.820101	324.753165	7.579763
5.612834	326.298918	7.584768
5.248420	338.098891	7.589773
5.454341	325.450179	7.594778
5.270758	328.715651	7.599782
5.106295	327.548469	7.604787
5.956203	320.668745	7.609792
5.538085	332.256597	7.614797
5.563583	325.292714	7.619802
5.532753	329.425590	7.624806
5.567982	331.937074	7.629811
5.433912	324.553732	7.634816
5.471340	330.106837	7.639821
5.730556	323.069406	7.644826
5.348489	330.384887	7.649830
5.442709	312.667504	7.654835
5.570335	329.101948	7.659840
5.540620	322.939504	7.664845
5.748997	320.910600	7.669850
5.231671	325.709993	7.674854
5.138514	321.983807	7.679859
5.730803	324.941995	7.684864
5.611394	329.124828	7.689869
5.605277	333.097643	7.694874
5.519466	330.031144	7.699878
5.914248	326.957636	7.704883
5.651601	336.567973	7.709888
5.716723	327.248126	7.714893
5.828012	313.624054	7.719898
5.575849	323.285727	7.724902
5.773287	322.534559	7.729907
5.972926	318.449613	7.734912
5.623402	317.883251	7.739917
5.447216	297.830973	7.744922
5.391032	301.500694	7.749926
5.501461	302.882755	7.754931
5.644064	303.954256	7.759936
5.369930	305.157965	7.764941
5.234426	304.091562	7.769946
5.403727	305.181638	7.774950
5.622873	312.329384	7.779955
5.598998	314.526940	7.784960
5.473835	312.768823	7.789965
5.778489	307.949289	7.794970
5.373182	295.346860	7.799974
5.317159	303.870560	7.804979
5.331273	317.661007	7.809984
5.415849	324.434891	7.814989
5.563853	317.005331	7.819994
5.368987	315.695979	7.824998
5.610199	319.364997	7.830003
5.968089	321.519786	7.835008
5.383239	305.301258	7.840013
5.703205	304.049680	7.845018
5.307202	308.898571	7.850022
5.113323	307.688897	7.855027
5.464506	316.179739	7.860032
5.241439	330.193883	7.865037
5.363372	312.869803	7.870042
5.569569	332.626850	7.875046
5.123462	331.812642	7.880051
5.313327	327.557349	7.885056
5.083158	323.014730	7.890061
5.299024	315.055908	7.895066
5.480137	325.017717	7.900070
5.683317	329.587741	7.905075
5.542418	320.441940	7.910080
5.498626	327.643012	7.915085
5.533086	315.386786	7.920090
5.534697	322.946469	7.925094
5.281343	321.027118	7.930099
5.457957	319.960237	7.935104
5.318733	319.431338	7.940109
5.788814	323.680026	7.945114
5.593369	330.896692	7.950118
5.569122	327.603467	7.955123
5.680040	326.331878	7.960128
5.397458	330.947213	7.965146
5.334027	313.700861	7.970163
5.784689	321.386095	7.975181
5.768528	324.696141	7.980198
5.648723	322.618216	7.985216
5.452753	330.094635	7.990234
5.642260	313.896614	7.995251
5.580382	314.321990	8.000269
5.506865	320.620530	8.005286
5.589556	314.648907	8.010304
5.691360	327.714134	8.015322
5.882633	322.509443	8.020339
5.694781	330.717442	8.025357
5.455756	319.832476	8.030374
5.763939	323.120311	8.035392
5.401436	330.222659	8.040410
5.502531	319.251275	8.045427
5.477605	321.538076	8.050445
5.665096	320.791270	8.055462
5.680084	313.141909	8.060480
5.539097	321.224958	8.065498
5.534619	315.098779	8.070515
5.632799	319.669291	8.075533
5.487793	323.988125	8.080550
5.764494	321.893384	8.085568
5.242606	327.327339	8.090586
5.769232	321.948353	8.095603
5.599681	321.817329	8.100621
5.596388	317.391000	8.105638
5.914182	319.468438	8.110656
5.729507	325.722863	8.115674
5.898607	328.367875	8.120691
5.693701	327.768774	8.125709
5.486911	328.117725	8.130726
5.756469	322.860144	8.135744
5.579147	319.880887	8.140762
5.645139	321.093332	8.145779
5.856802	331.402089	8.150797
5.450470	329.578363	8.155814
6.019272	320.055259	8.160832
5.851038	327.146166	8.165850
5.771249	321.015210	8.170867
5.381311	325.504318	8.175885
5.130563	333.652058	8.180902
5.696633	323.817655	8.185920
5.503669	332.777429	8.190938
5.580695	332.845174	8.195955
5.398196	331.990256	8.200973
5.542355	328.241578	8.205990
5.877090	321.496952	8.211008
5.629211	323.072720	8.216026
5.650795	326.725669	8.221043
5.782449	341.606471	8.226061
5.880044	338.798565	8.231078
5.736336	334.157590	8.236096
5.654738	341.258099	8.241114
5.612289	346.255519	8.246131
6.204076	347.360800	8.251149
5.726879	336.889516	8.256166
5.895130	341.139168	8.261184
5.875752	337.880117	8.266202
5.345347	339.053751	8.271219
5.867934	335.980472	8.276237
5.850903	345.694976	8.281254
6.064756	348.872447	8.286272
5.994191	360.550727	8.291290
6.097634	341.573271	8.296307
5.775687	334.267614	8.301325
5.317639	338.331161	8.306342
5.999491	330.116363	8.311360
5.948747	354.357708	8.316378
5.928267	344.186062	8.321395
5.979689	340.774197	8.326413
5.764491	346.232853	8.331430
6.369041	332.450660	8.336448
6.007566	331.954387	8.341466
5.906105	316.385040	8.346483
6.098658	316.870217	8.351501
5.989484	321.251815	8.356518
6.050979	317.834157	8.361536
5.696795	323.772079	8.366554
5.628143	317.615075	8.371571
5.742191	318.168235	8.376589
5.621193	329.021728	8.381606
6.198279	336.190312	8.386624
5.839018	337.743454	8.391642
6.045821	328.716793	8.396659
6.337062	319.532511	8.401677
5.763575	320.182171	8.406694
5.960720	309.578503	8.411712
5.723117	316.561898	8.416730
5.901216	339.900617	8.421747
6.336627	342.408135	8.426765
6.084675	339.664293	8.431782
6.201943	333.750617	8.436800
5.926922	323.049218	8.441818
5.738059	319.120193	8.446835
5.979641	325.737649	8.451853
5.604710	334.823146	8.456870
5.864920	340.550604	8.461888
6.358581	350.158178	8.466906
5.951559	342.703717	8.471923
6.308160	342.878770	8.476941
5.716827	343.550274	8.481958
6.133879	348.762446	8.486976
6.072382	352.424014	8.491994
6.173538	350.578216	8.497011
5.909162	354.580731	8.502029
5.830178	357.402251	8.507046
6.344995	350.212188	8.512064
6.363767	346.046619	8.517082
6.355682	335.531169	8.522099
6.310473	331.678577	8.527117
6.086351	328.090053	8.532134
5.852572	321.015844	8.537152
6.170667	331.537477	8.542170
6.130227	320.776353	8.547187
6.021583	326.260789	8.552205
5.940792	336.588654	8.557223
6.201513	348.218277	8.562240
6.435459	353.690782	8.567258
6.127734	341.047630	8.572275
6.235319	328.190608	8.577293
6.101042	326.105825	8.582311
6.182724	323.888226	8.587328
6.120979	317.118395	8.592346
6.184571	312.111347	8.597363
5.900832	321.931022	8.602381
6.002502	339.967316	8.607399
6.302265	342.983079	8.612416
6.504575	358.563986	8.617434
6.189585	352.160827	8.622451
6.370017	343.675415	8.627469
6.253002	344.679670	8.632487
5.925690	328.020206	8.637504
6.151978	337.468064	8.642522
6.408102	356.062985	8.647539
6.723470	339.885663	8.652557
6.552030	336.575577	8.657575
6.350678	326.458534	8.662592
6.145341	329.054622	8.667610
5.886855	325.721136	8.672627
5.962971	324.307738	8.677645
6.136517	330.388225	8.682663
6.480096	336.309243	8.687680
6.463486	325.360553	8.692698
6.167979	320.905562	8.697715
6.101045	318.501150	8.702733
5.932855	344.914600	8.707751
6.299059	346.750820	8.712768
6.228306	357.125357	8.717786
6.088821	374.375531	8.722803
6.407615	354.276664	8.727821
6.368158	359.191916	8.732839
6.102426	356.983213	8.737856
6.331924	352.667487	8.742874
6.122333	353.126328	8.747891
6.398369	350.452479	8.752909
6.242263	356.330715	8.757927
6.400389	351.764829	8.762944
6.667905	352.146299	8.767962
6.248021	349.875984	8.772979
6.268800	348.391725	8.777997
6.491318	358.782646	8.783015
6.537357	358.759271	8.788032
6.524754	346.187988	8.793050
6.519677	346.691459	8.798067
6.492339	351.360760	8.803085
6.227562	347.705047	8.808103
6.306956	346.093410	8.813120
6.626956	351.504261	8.818138
6.307555	357.187974	8.823155
6.409698	350.985609	8.828173
6.313752	354.395639	8.833191
6.217206	348.542878	8.838208
6.311461	345.075813	8.843226
6.117586	344.291265	8.848243
6.676715	339.572908	8.853261
6.101029	358.492957	8.858279
6.253871	343.495802	8.863296
6.581074	344.350971	8.868314
6.190426	355.950184	8.873331
6.552573	364.570847	8.878349
6.296857	378.973391	8.883367
6.546427	382.388913	8.888384
6.696786	378.465709	8.893402
6.718535	366.929468	8.898419
6.760504	359.404536	8.903437
6.319013	345.687940	8.908455
6.233112	349.135278	8.913472
6.499846	353.562122	8.918490
6.495456	380.995104	8.923507
6.717167	376.400005	8.928525
6.799793	378.472426	8.933543
6.412637	363.167132	8.938560
6.757260	367.188470	8.943578
6.666516	378.609817	8.948595
6.387302	355.507347	8.953613
6.718759	365.492158	8.958631
6.290456	365.169494	8.963648
6.893326	373.643905	8.968666
6.528633	390.733914	8.973683
6.759229	378.398244	8.978701
6.458115	382.437835	8.983719
6.473658	388.568763	8.988736
6.692964	371.724349	8.993754
6.524872	379.235251	8.998771
6.451630	382.890600	9.003789
6.430350	387.282194	9.008807
6.797815	386.892180	9.013824
7.006060	381.721665	9.018842
6.826896	380.896896	9.023859
7.083244	380.401352	9.028877
6.605354	372.882815	9.033895
6.767638	367.420059	9.038912
6.601898	365.009532	9.043930
6.783923	378.269477	9.048947
6.998486	374.015059	9.053965
6.386224	364.753732	9.058983
6.507700	381.707393	9.064000
6.598280	379.357929	9.069018
6.579360	394.475828	9.074035
7.219109	382.039473	9.079053
7.168055	392.447091	9.084071
6.803911	375.330271	9.089088
7.131639	360.769655	9.094106
6.753483	352.168128	9.099123
6.806567	352.913217	9.104141
6.591343	345.377658	9.109159
6.501428	362.216951	9.114176
6.648133	355.565774	9.119194
6.891433	371.660582	9.124211
6.758781	374.105717	9.129229
6.454589	368.504740	9.134247
6.907337	377.485952	9.139264
6.810727	366.962675	9.144282
7.058707	384.867186	9.149299
7.028808	382.292110	9.154317
6.914834	383.772344	9.159335
6.759869	384.107812	9.164352
6.664677	376.203061	9.169370
6.829348	383.335021	9.174387
6.773536	379.653820	9.179405
6.700341	381.013952	9.184423
6.631399	379.426924	9.189440
6.853242	387.028279	9.194458
6.974366	385.762623	9.199475
6.594265	390.598480	9.204493
6.815744	393.664879	9.209511
6.457659	398.202276	9.214528
6.755399	389.344472	9.219546
6.463455	397.289646	9.224563
6.836010	388.869289	9.229581
6.739278	388.065733	9.234599
7.110392	393.909107	9.239616
7.200745	404.618692	9.244634
6.667843	401.621919	9.249651
7.036016	409.060646	9.254669
7.215086	405.819562	9.259687
7.094289	413.823550	9.264704
6.993492	391.843181	9.269722
6.866196	390.623893	9.274739
6.958101	385.630938	9.279757
6.865649	390.422701	9.284775
7.050535	408.564788	9.289792
7.317420	408.315682	9.294810
6.830833	399.351513	9.299827
6.887286	388.635045	9.304845
7.214063	409.208115	9.309863
7.205184	419.286206	9.314880
7.317477	414.234863	9.319898
6.874161	398.830962	9.324915
6.958847	388.248186	9.329933
7.023381	383.405395	9.334951
7.039372	391.718884	9.339968
7.005358	386.795350	9.344986
6.808639	403.668576	9.350003
6.957438	411.328265	9.355021
7.247894	409.056963	9.360039
7.063713	417.739898	9.365056
7.209611	412.313291	9.370074
7.065308	418.107333	9.375091
7.200465	421.325476	9.380109
6.883981	413.686464	9.385127
6.617063	415.180759	9.390144
7.258603	413.699988	9.395162
6.900815	411.109423	9.400179
6.855605	419.336702	9.405197
7.226151	418.093689	9.410215
7.242047	416.380848	9.415232
7.209373	421.505489	9.420250
7.051302	423.367744	9.425267
6.770047	425.605601	9.430285
6.925032	413.403634	9.435303
6.884019	425.443148	9.440320
7.336269	448.211632	9.445338
7.288813	453.801924	9.450355
7.368814	443.643326	9.455373
7.355892	447.448926	9.460391
7.558138	436.746414	9.465408
7.325320	423.128012	9.470426
7.457055	421.677663	9.475443
7.149424	421.602719	9.480461
7.362511	416.089235	9.485479
7.056543	421.442076	9.490496
7.066618	414.243290	9.495514
7.144871	422.625329	9.500531
7.135326	442.611041	9.505549
7.424778	433.916852	9.510567
7.165921	442.904407	9.515584
7.417514	445.799829	9.520602
7.541858	454.275823	9.525619
7.435341	453.358450	9.530637
7.636321	433.132227	9.535655
7.460131	421.759437	9.540672
7.335439	421.044243	9.545690
7.335252	418.905305	9.550707
7.172619	417.189789	9.555725
7.305177	411.630866	9.560743
7.138095	434.456514	9.565760
7.436571	433.068059	9.570778
7.545682	446.824564	9.575795
7.606807	457.000932	9.580813
7.518886	434.900287	9.585831
6.964201	432.802699	9.590848
7.569442	440.549832	9.595866
7.508988	442.947522	9.600883
7.638685	450.943688	9.605901
7.774284	428.063149	9.610919
7.387160	422.875581	9.615936
7.216904	413.956943	9.620954
7.175371	426.147794	9.625971
7.403315	441.036003	9.630989
7.512932	440.358448	9.636007
7.357686	450.653034	9.641024
7.475101	452.145812	9.646042
7.757431	452.971698	9.651059
7.525734	454.500030	9.656077
7.513077	441.375735	9.661095
7.295622	455.337564	9.666112
7.224449	450.772247	9.671130
7.070063	451.500358	9.676147
7.183669	449.547196	9.681165
7.369589	444.191213	9.686183
7.382369	452.919457	9.691200
7.387088	451.293776	9.696218
7.566259	442.815406	9.701235
7.446448	459.814245	9.706253
7.624194	446.501914	9.711271
7.518921	454.187967	9.716288
7.369752	445.423176	9.721306
7.737890	450.055490	9.726323
7.832931	456.205191	9.731341
7.375061	447.276004	9.736359
7.528433	464.218581	9.741376
7.772884	470.307283	9.746394
8.005008	466.147458	9.751411
7.515503	458.104720	9.756429
7.395962	447.041582	9.761447
7.263104	468.870480	9.766464
7.738490	472.163287	9.771482
7.770350	474.232007	9.776499
7.515642	478.522369	9.781517
7.848465	474.997447	9.786535
7.883550	477.903169	9.791552
7.836188	479.536939	9.796570
7.753321	467.896182	9.801587
7.327883	483.570232	9.806605
7.760767	481.012145	9.811623
7.515157	483.913872	9.816640
7.565758	484.287697	9.821658
7.615795	475.664246	9.826675
7.573741	480.698349	9.831693
7.620225	473.324948	9.836711
7.487700	478.119327	9.841728
7.474346	474.315361	9.846746
7.617552	472.650456	9.851763
7.605799	473.095992	9.856781
7.907097	469.657761	9.861799
7.755667	476.077291	9.866816
7.632373	481.507619	9.871834
7.691567	498.107107	9.876851
7.693542	511.446223	9.881869
8.101659	507.317822	9.886887
8.187933	512.447438	9.891904
7.932549	508.223314	9.896922
8.215047	488.452157	9.901939
7.654170	482.064683	9.906957
7.711075	477.338750	9.911975
7.874782	491.335634	9.916992
7.459767	491.218801	9.922010
7.962864	491.622059	9.927027
7.655542	509.196126	9.932045
8.040617	500.881985	9.937063
7.720206	511.269642	9.942080
8.083608	508.457336	9.947098
8.312862	500.382981	9.952115
7.823592	505.969943	9.957133
7.820417	511.854454	9.962151
7.848827	501.987459	9.967168
7.817659	513.413427	9.972186
8.062365	517.526008	9.977203
8.166276	524.223279	9.982221
8.375087	511.841013	9.987239
8.252501	511.747787	9.992256
8.074904	503.142553	9.997274
7.931259	481.874218	10.002291
7.608480	491.080691	10.007309
7.891650	501.442201	10.012327
7.834986	507.632639	10.017344
8.032579	516.695955	10.022362
8.245851	513.447229	10.027379
7.829440	528.158205	10.032397
8.349318	512.356277	10.037415
7.904636	517.135437	10.042432
7.714602	525.784367	10.047450
8.430045	521.044946	10.052467
7.887220	515.594353	10.057485
8.032792	506.847439	10.062503
7.837961	523.718812	10.067520
7.523029	529.300884	10.072538
8.075930	520.360883	10.077555
8.119542	521.153698	10.082573
7.737079	513.670591	10.087591
7.877111	521.899884	10.092608
7.823690	517.774442	10.097626
8.075378	532.287331	10.102643
8.041444	545.679253	10.107661
8.423622	541.756863	10.112679
8.376081	547.158164	10.117696
8.523552	553.971158	10.122714
8.307991	537.088707	10.127731
8.094134	523.663404	10.132749
7.919805	527.270840	10.137767
8.445952	540.750478	10.142784
8.315672	546.592536	10.147802
8.381012	533.536753	10.152819
7.926258	519.564860	10.157837
8.430459	531.648384	10.162855
8.633944	535.917754	10.167872
8.292438	534.401340	10.172890
8.269234	518.184429	10.177907
8.000770	529.329115	10.182925
8.506810	542.758938	10.187943
8.230446	520.099956	10.192960
8.416102	525.636890	10.197978
8.098906	526.700415	10.202995
8.081094	543.955174	10.208013
8.298828	539.032006	10.213031
8.547090	539.347975	10.218048
8.424556	555.704775	10.223066
8.660279	542.916538	10.228083
8.229202	541.066074	10.233101
8.309718	551.423419	10.238119
8.208993	549.358449	10.243136
8.207922	546.015438	10.248154
8.462944	553.890572	10.253171
8.349658	555.916177	10.258189
8.481501	553.349572	10.263207
8.641193	543.554143	10.268224
8.232751	555.087364	10.273242
8.573536	541.727539	10.278259
8.457910	545.710146	10.283277
8.372039	549.428535	10.288295
8.542632	546.637164	10.293312
8.233698	547.580252	10.298330
8.483763	546.436259	10.303347
8.359283	558.112283	10.308365
8.045948	561.273398	10.313383
8.199679	542.389923	10.318400
8.065815	544.126758	10.323418
8.393211	548.827339	10.328435
8.330723	543.817632	10.333453
8.270171	551.132729	10.338471
8.699009	544.853761	10.343488
8.674931	558.888628	10.348506
8.918396	548.354489	10.353523
8.414489	538.924784	10.358541
8.418497	537.740565	10.363559
8.562186	548.694439	10.368576
8.288569	544.759878	10.373594
8.557561	557.533155	10.378611
8.577478	572.929797	10.383629
8.731433	576.593699	10.388647
8.941943	579.757207	10.393664
8.598907	569.748638	10.398682
8.420627	558.998318	10.403699
8.471118	564.944736	10.408717
8.965508	569.327722	10.413735
8.784617	580.014748	10.418752
8.624356	565.484693	10.423770
8.804822	556.317397	10.428787
8.798293	553.297175	10.433805
8.726938	549.008086	10.438823
8.575318	548.404304	10.443840
8.405643	548.773400	10.448858
9.113942	565.035121	10.453875
8.712800	565.188581	10.458893
8.363321	563.990449	10.463911
8.785158	570.544862	10.468928
8.924613	580.285907	10.473946
8.932551	570.921566	10.478963
8.439567	555.113687	10.483981
8.636262	578.254751	10.488999
8.854893	580.237118	10.494016
8.662515	570.821941	10.499034
8.923207	567.245348	10.504051
8.766576	577.730074	10.509069
8.449312	577.942985	10.514087
8.779332	580.894062	10.519104
8.855405	581.455869	10.524122
8.787493	589.748199	10.529139
8.644958	580.147155	10.534157
8.544429	581.918045	10.539175
8.585474	576.745672	10.544192
8.700847	587.056343	10.549210
8.892073	580.974276	10.554227
8.458125	591.102259	10.559245
8.713247	590.561941	10.564263
8.839888	605.096155	10.569280
8.760503	607.886296	10.574298
9.237496	600.485479	10.579315
8.983070	603.390555	10.584333
8.734931	593.591837	10.589351
9.203017	603.818250	10.594368
8.830263	605.779478	10.599386
8.980286	599.508580	10.604403
9.269517	609.272422	10.609421
8.989427	604.653215	10.614439
9.174196	615.348919	10.619456
9.033396	609.158159	10.624474
9.062971	601.658579	10.629491
9.150264	594.119350	10.634509
8.742633	605.058786	10.639527
9.026571	590.418396	10.644544
9.166521	598.774787	10.649562
9.269736	604.619118	10.654579
9.229686	592.947770	10.659597
8.791700	589.485357	10.664615
8.924831	582.107918	10.669632
8.908589	591.261626	10.674650
9.282715	602.403792	10.679667
9.416864	598.251858	10.684685
8.952825	601.521729	10.689703
9.001211	604.299906	10.694720
8.824260	605.839477	10.699738
8.736257	607.701589	10.704755
9.181038	596.342267	10.709773
9.481176	611.194502	10.714791
9.150964	603.687856	10.719808
9.034561	611.707260	10.724826
9.296515	610.670825	10.729843
9.518140	612.568563	10.734861
9.584393	605.758656	10.739879
9.492445	603.743400	10.744896
9.134870	600.504364	10.749914
9.137533	593.411129	10.754931
9.125754	598.029123	10.759949
9.006600	614.348819	10.764967
9.500758	599.060997	10.769984
9.445674	608.895911	10.775002
9.569038	605.828725	10.780019
9.045818	602.770578	10.785037
8.438967	605.959741	10.790055
8.890220	610.221348	10.795072
8.986569	613.437778	10.800090
9.306538	615.090271	10.805107
9.316884	605.256208	10.810125
9.087328	614.344611	10.815143
9.449472	602.318850	10.820160
9.220235	610.605083	10.825178
8.954163	593.646780	10.830195
9.359414	594.820500	10.835213
9.216341	611.462688	10.840231
9.635017	630.757224	10.845248
9.437831	623.857208	10.850266
9.182047	605.615440	10.855283
9.329037	621.421857	10.860301
9.537067	648.369113	10.865319
9.587519	639.752586	10.870336
9.231831	634.608659	10.875354
9.876249	644.357911	10.880371
9.490583	630.913869	10.885389
9.096692	629.934744	10.890407
9.478985	623.616398	10.895424
9.339570	635.987143	10.900442
9.760199	636.431097	10.905459
9.692280	639.648601	10.910477
9.723776	642.270255	10.915495
9.647753	622.801832	10.920512
9.272251	620.659450	10.925530
9.430789	625.645591	10.930547
9.822994	630.057587	10.935565
9.465433	641.735978	10.940583
9.665186	630.683316	10.945600
9.702440	633.482626	10.950618
9.544822	617.489164	10.955635
9.447739	608.951062	10.960653
9.423388	618.311403	10.965671
9.862564	636.744548	10.970688
9.756800	643.901148	10.975706
9.977141	632.170009	10.980723
9.767850	621.996515	10.985741
9.355555	613.934341	10.990759
9.630725	601.137765	10.995776
9.451650	606.531105	11.000794
9.523774	622.929415	11.005811
9.856939	634.469542	11.010829
9.744403	640.125764	11.015847
10.116284	636.552922	11.020864
9.839632	621.002181	11.025882
9.138791	616.562425	11.030899
9.342105	618.550084	11.035917
9.018315	634.688698	11.040935
9.690843	632.043354	11.045952
9.698642	643.550955	11.050970
9.344350	633.431234	11.055987
9.721014	630.555899	11.061005
9.150495	648.304699	11.066023
9.296221	637.738235	11.071040
9.854833	656.070970	11.076058
10.275651	660.679784	11.081075
10.438468	660.773896	11.086093
10.150051	655.099550	11.091111
10.016358	644.179233	11.096128
9.946718	641.739201	11.101146
10.031776	644.899246	11.106163
10.228949	640.299563	11.111181
9.788779	634.420030	11.116199
9.851690	632.356052	11.121216
10.041948	635.372552	11.126234
9.845386	634.200610	11.131251
9.994590	638.390216	11.136269
9.779278	639.245213	11.141287
9.800377	643.634502	11.146304
9.957885	633.970357	11.151322
9.841570	640.585296	11.156339
9.887711	635.003967	11.161357
10.053845	648.506195	11.166375
10.298385	639.209090	11.171392
10.154322	647.814867	11.176410
9.931068	642.266149	11.181427
10.245334	639.212774	11.186445
9.693581	649.186673	11.191463
9.857526	634.218497	11.196480
9.855333	638.933622	11.201498
9.713808	629.708098	11.206515
10.131296	638.725798	11.211533
9.941499	646.376415	11.216551
10.057023	642.790140	11.221568
9.990250	650.629249	11.226586
9.751882	666.711072	11.231603
10.142399	661.601958	11.236621
10.149100	676.363897	11.241639
10.434531	671.544440	11.246656
10.376860	665.910387	11.251674
10.039008	660.438661	11.256691
10.271581	657.194194	11.261709
10.242584	666.920424	11.266727
10.002933	656.971667	11.271744
10.329844	663.685286	11.276762
10.073111	670.717958	11.281779
10.384214	665.463728	11.286797
10.176902	667.865647	11.291815
10.332047	663.371211	11.296832
10.720658	666.557755	11.301850
9.864282	645.067377	11.306867
10.056890	648.972993	11.311885
10.254662	657.135347	11.316903
10.195507	663.284535	11.321920
10.252344	668.834445	11.326938
10.311974	676.191146	11.331955
10.544637	663.910999	11.336973
10.149970	668.235367	11.341991
10.156327	674.298845	11.347008
10.478583	670.582156	11.352026
10.406192	673.265464	11.357043
10.159568	676.106775	11.362061
10.120517	672.457078	11.367079
10.311755	673.353926	11.372096
10.282913	667.269028	11.377114
10.530504	675.600390	11.382131
10.294162	665.406145	11.387149
10.250215	672.035511	11.392167
10.275098	665.923430	11.397184
10.426292	670.913260	11.402202
10.296857	672.293339	11.407219
10.278324	666.483066	11.412237
10.513047	681.914384	11.417255
10.466327	677.805505	11.422272
10.522364	673.123643	11.427290
10.488888	676.603426	11.432307
10.531668	674.525155	11.437325
10.289893	670.656152	11.442343
10.239096	674.314061	11.447360
10.363053	668.758633	11.452378
10.100917	688.428303	11.457395
10.530712	685.476572	11.462413
10.388381	697.496337	11.467431
10.205267	694.385606	11.472448
10.717223	694.730035	11.477466
10.329996	703.355265	11.482483
10.895203	704.073994	11.487501
10.821593	694.617759	11.492519
10.748655	706.392641	11.497536
10.734013	702.950479	11.502554
10.695246	710.314503	11.507571
10.823611	707.934733	11.512589
10.687061	708.970384	11.517607
10.567967	711.848293	11.522624
10.980577	700.605116	11.527642
10.886751	700.481649	11.532659
10.845583	703.217666	11.537677
10.572853	705.562107	11.542695
10.535712	709.508167	11.547712
10.926210	701.889355	11.552730
10.268353	709.556441	11.557747
10.703803	701.533519	11.562765
10.586194	704.068231	11.567783
10.681276	720.330492	11.572800
10.849581	700.667093	11.577818
10.683916	709.896344	11.582835
10.893471	712.285077	11.587853
10.693637	707.486858	11.592871
10.545871	701.676770	11.597888
10.940259	712.957572	11.602906
10.737709	714.499711	11.607923
10.971454	702.170937	11.612941
10.827351	704.477982	11.617959
10.776719	705.342474	11.622976
10.603948	704.042995	11.627994
10.548325	712.469163	11.633011
10.955782	720.796862	11.638029
11.051482	729.129639	11.643047
10.966566	725.995489	11.648064
11.137381	715.242181	11.653082
10.859215	717.874577	11.658099
10.985406	712.114372	11.663117
10.813710	713.316924	11.668135
10.854458	729.893633	11.673152
11.384186	721.751890	11.678170
11.109266	728.682790	11.683187
10.863348	709.474380	11.688205
10.948563	716.529682	11.693223
11.278539	729.090599	11.698240
11.116835	726.278828	11.703258
10.828949	728.699190	11.708275
11.196052	730.780541	11.713293
11.235723	724.513757	11.718311
10.793361	727.990862	11.723328
11.132606	719.515310	11.728346
11.129686	731.052302	11.733363
11.267078	729.617818	11.738381
11.093306	733.011960	11.743399
10.785205	726.964332	11.748416
11.273862	734.004436	11.753434
10.800773	743.349756	11.758451
11.137368	737.617751	11.763469
11.122258	735.520500	11.768487
10.681577	731.682582	11.773504
11.012443	722.869694	11.778522
10.878374	731.588905	11.783539
10.864012	730.265508	11.788557
10.984957	736.585811	11.793575
11.675193	766.247971	11.798592
11.186322	743.875408	11.803610
11.040182	743.229577	11.808627
11.396982	747.254416	11.813645
11.168515	742.290869	11.818663
11.187670	756.936675	11.823680
11.764348	753.947864	11.828698
11.563341	755.058529	11.833715
11.448258	735.329340	11.838733
11.367421	735.867289	11.843751
11.042441	733.141742	11.848768
11.399694	739.341218	11.853786
10.890592	745.716246	11.858803
11.136750	762.894758	11.863821
11.605926	760.673974	11.868839
11.297979	762.655017	11.873856
11.914449	756.275283	11.878874
11.516830	760.299234	11.883891
11.278592	771.093687	11.888909
11.706034	755.182005	11.893927
11.369572	770.169220	11.898944
11.489063	753.263832	11.903962
11.243211	765.740839	11.908979
11.217249	772.140051	11.913997
11.698215	766.041126	11.919015
11.650505	765.339271	11.924032
11.796263	759.495710	11.929050
11.506893	766.705049	11.934067
11.151229	769.782863	11.939085
11.551369	758.363291	11.944103
11.300340	775.188921	11.949120
11.300821	756.779644	11.954138
11.400503	766.071948	11.959155
11.402544	766.915438	11.964173
11.551721	765.425272	11.969191
11.241158	773.277571	11.974208
11.553286	775.374509	11.979226
11.791529	798.189114	11.984243
11.878294	795.903493	11.989261
12.085734	776.705594	11.994279
11.810294	765.350625	11.999296
11.804695	766.961975	12.004314
11.677980	750.551627	12.009331
11.659462	766.650460	12.014349
11.857957	763.228958	12.019367
11.626263	768.558622	12.024384
11.782344	748.025878	12.029402
11.636108	763.736635	12.034419
11.468826	764.925866	12.039437
11.764556	769.616889	12.044455
11.590312	791.844846	12.049472
11.872547	789.328335	12.054490
12.112585	788.445780	12.059507
11.761516	792.505443	12.064525
12.095547	789.707782	12.069543
12.125493	792.771669	12.074560
12.240705	779.489265	12.079578
11.929778	768.500528	12.084595
11.738300	761.530523	12.089613
11.560188	765.460237	12.094631
11.749426	769.708114	12.099648
11.941612	782.522219	12.104666
11.911339	789.729983	12.109683
11.727959	790.197494	12.114701
12.083237	785.087866	12.119719
11.723036	791.539862	12.124736
12.031117	783.558810	12.129754
12.186532	785.016114	12.134771
12.142477	792.125977	12.139789
11.857585	782.695846	12.144807
11.821414	788.987618	12.149824
11.947096	791.628372	12.154842
11.925491	796.827477	12.159859
11.751773	795.371579	12.164877
11.856469	787.214428	12.169895
12.127926	803.254060	12.174912
12.107581	789.380278	12.179930
11.834111	795.385538	12.184947
11.878690	805.521965	12.189965
11.972640	786.628882	12.194983
11.886587	801.744596	12.200000
11.882269	811.586897	12.205018
12.271613	824.793677	12.210035
12.224100	822.839049	12.215053
12.181909	814.092681	12.220071
12.489007	822.858996	12.225088
12.556646	814.587011	12.230106
12.351637	798.236098	12.235123
11.990454	796.958006	12.240141
12.250454	808.742500	12.245159
11.922996	823.754258	12.250176
12.340639	824.281571	12.255194
12.749736	825.999069	12.260211
12.546207	824.252476	12.265229
12.744129	808.033947	12.270247
12.203862	800.591834	12.275264
12.427250	788.381710	12.280282
12.234218	788.215297	12.285299
11.956036	790.232953	12.290317
12.135760	806.034741	12.295335
12.712855	810.049171	12.300352
12.488049	827.190350	12.305370
12.680997	823.593699	12.310387
12.442012	823.756576	12.315405
12.297719	798.694663	12.320423
12.065372	812.959422	12.325440
12.276275	824.433396	12.330458
12.401628	811.996583	12.335475
12.321787	822.787136	12.340493
12.662352	822.488158	12.345511
12.714291	828.785953	12.350528
12.607620	826.506512	12.355546
12.485683	820.020277	12.360563
12.472774	825.078805	12.365581
12.894322	817.784177	12.370599
12.424798	831.893203	12.375616
12.301975	819.439042	12.380634
12.689654	819.275461	12.385651
12.868345	822.340949	12.390669
12.875304	809.055645	12.395687
12.871645	827.117494	12.400704
12.881906	809.782928	12.405722
12.794173	820.133816	12.410739
12.695432	813.150922	12.415757
12.820330	806.809204	12.420775
12.774150	801.562899	12.425792
12.445874	786.979509	12.430810
12.902255	805.103373	12.435827
12.417718	803.178851	12.440845
12.931853	800.234023	12.445863
12.505199	806.287138	12.450880
12.771002	822.312472	12.455898
12.884051	814.215825	12.460915
12.801947	814.764811	12.465933
13.252140	813.976144	12.470951
13.129089	809.178980	12.475968
12.631648	792.792262	12.480986
12.711541	794.243941	12.486003
12.774191	795.754267	12.491021
12.759578	809.115769	12.496039
12.784185	812.957573	12.501056
12.836497	817.099865	12.506074
12.984170	826.792571	12.511091
12.719456	815.714387	12.516109
12.825915	817.283211	12.521127
12.986629	818.342566	12.526144
12.556191	810.737539	12.531162
12.818071	825.397322	12.536179
12.870691	821.444202	12.541197
12.972902	817.370309	12.546215
12.885900	818.984686	12.551232
12.807291	833.946768	12.556250
12.945706	816.660590	12.561267
12.789148	823.851254	12.566285
12.793527	822.104352	12.571303
12.974571	829.550099	12.576320
13.114961	849.324880	12.581338
13.424793	848.865654	12.586355
13.270338	837.610400	12.591373
13.112251	825.499996	12.596391
12.906637	818.012411	12.601408
13.165042	825.859473	12.606426
13.126626	822.200484	12.611443
13.127390	825.294884	12.616461
13.153364	821.028112	12.621479
13.048705	841.446819	12.626496
13.142033	853.376785	12.631514
13.276713	858.596532	12.636531
13.142444	854.583163	12.641549
13.278610	848.652783	12.646567
13.034244	856.965955	12.651584
13.040157	854.803905	12.656602
13.427686	858.685038	12.661619
13.661509	849.421560	12.666637
13.318355	844.344672	12.671655
13.234213	843.849981	12.676672
13.166242	847.780211	12.681690
13.226431	846.980416	12.686707
13.367306	843.450624	12.691725
13.265610	846.666274	12.696743
13.366313	853.143586	12.701760
13.197143	844.474574	12.706778
13.718376	841.267684	12.711795
13.305990	859.076306	12.716813
13.569306	863.615459	12.721831
13.530768	848.062631	12.726848
13.409188	851.842300	12.731866
13.677854	848.910573	12.736883
13.553899	844.845707	12.741901
13.423721	845.441117	12.746919
13.511304	840.009827	12.751936
13.469404	852.119987	12.756954
13.466790	846.028125	12.761971
13.504946	853.818899	12.766989
13.380055	859.437192	12.772007
13.908603	853.412638	12.777024
13.573909	856.814802	12.782042
13.484507	851.574344	12.787059
13.471611	853.432832	12.792077
13.475535	855.236974	12.797095
13.608830	853.338273	12.802112
13.332923	848.727552	12.807130
13.812002	847.087009	12.812147
13.520837	844.614274	12.817165
13.561944	851.430119	12.822183
13.544283	854.786778	12.827200
13.529582	879.406294	12.832218
14.104160	877.705878	12.837235
13.725936	879.671586	12.842253
13.789670	872.548448	12.847271
13.909811	878.500993	12.852288
13.290857	871.707766	12.857306
13.540247	872.234544	12.862323
13.498175	874.749912	12.867341
13.763808	877.367946	12.872359
13.851618	879.222194	12.877376
13.992788	886.053402	12.882394
13.839308	889.213653	12.887411
13.878505	886.208836	12.892429
13.840627	886.819895	12.897447
13.631157	880.088301	12.902464
13.893220	876.989382	12.907482
13.841562	878.136683	12.912499
13.699174	881.972938	12.917517
13.660299	885.049496	12.922535
13.881147	880.188392	12.927552
13.901572	904.671653	12.932570
14.303300	903.253892	12.937587
14.012411	904.494264	12.942605
13.915551	895.613897	12.947623
14.261787	889.906419	12.952640
13.878255	899.277872	12.957658
13.989080	907.584923	12.962675
14.155362	914.195691	12.967693
14.326274	908.385902	12.972711
14.224057	893.953997	12.977728
13.997175	888.489830	12.982746
14.210538	902.599236	12.987763
14.262383	900.137708	12.992781
14.295548	897.689109	12.997799
14.119635	887.157521	13.002816
14.015824	903.430408	13.007834
14.249722	897.869030	13.012851
14.558290	905.369710	13.017869
14.382806	907.536720	13.022887
14.140864	884.202628	13.027904
13.945008	887.041196	13.032922
14.537375	893.036946	13.037939
14.450466	903.091347	13.042957
14.200178	900.032416	13.047975
14.470602	895.710465	13.052992
14.008694	898.908502	13.058010
14.394668	903.561232	13.063027
14.339858	909.800730	13.068045
14.181282	915.277192	13.073063
14.322216	921.513278	13.078080
14.184909	917.651747	13.083098
14.295191	912.794341	13.088115
14.548540	915.272900	13.093133
14.498224	915.339058	13.098151
14.673106	906.058913	13.103168
14.503499	916.169698	13.108186
14.497715	907.889131	13.113203
14.338860	921.099203	13.118221
14.287486	916.729261	13.123239
14.164693	908.995305	13.128256
14.514685	915.399365	13.133274
14.408826	908.073961	13.138291
14.486990	917.867074	13.143309
14.244570	909.244574	13.148327
14.385929	905.935516	13.153344
14.325830	923.685403	13.158362
14.364846	933.987275	13.163379
14.728356	938.665182	13.168397
14.834432	947.174777	13.173415
15.055145	937.752023	13.178432
14.587858	945.918845	13.183450
14.602513	939.727060	13.188467
14.684523	938.290885	13.193485
14.712255	938.353001	13.198503
15.154758	938.733911	13.203520
14.961212	945.698795	13.208538
14.734254	925.089868	13.213555
14.880228	917.968863	13.218573
14.653398	918.781790	13.223591
15.185796	910.745100	13.228608
15.152450	911.801202	13.233626
14.905756	900.115945	13.238643
14.785060	903.508930	13.243661
15.189674	906.304558	13.248679
15.175635	896.544899	13.253696
14.909451	916.932536	13.258714
15.135746	909.541610	13.263731
14.971053	902.352485	13.268749
14.775758	916.417056	13.273767
14.557788	893.317334	13.278784
14.583576	923.026623	13.283802
15.071192	916.086915	13.288819
15.180324	905.660938	13.293837
14.767999	898.577688	13.298855
15.258452	906.412227	13.303872
14.707933	915.761688	13.308890
15.178776	921.203612	13.313907
15.378773	927.274847	13.318925
14.961289	921.332212	13.323943
15.125117	910.045956	13.328960
15.275312	910.515519	13.333978
14.853947	911.724708	13.338995
15.230029	917.062822	13.344013
15.189181	936.479541	13.349031
15.309166	942.033580	13.354048
15.401998	924.518534	13.359066
14.904239	925.133165	13.364083
15.338234	934.908620	13.369101
15.417852	933.599394	13.374119
15.357604	929.323420	13.379136
15.462587	934.404029	13.384154
14.761438	931.346976	13.389171
15.432575	938.157543	13.394189
15.256948	943.720481	13.399207
15.500979	938.065697	13.404224
15.514048	939.364877	13.409242
15.546311	939.237103	13.414259
15.469401	921.744010	13.419277
14.990350	919.760112	13.424295
15.348314	917.583763	13.429312
15.392910	930.558286	13.434330
15.045016	928.205917	13.439347
15.201385	933.944460	13.444365
15.148996	949.867026	13.449383
15.558906	939.872343	13.454400
15.279246	942.531299	13.459418
15.178733	948.721288	13.464435
15.333970	941.870350	13.469453
15.010749	953.631477	13.474471
15.494129	951.204514	13.479488
15.517620	964.367955	13.484506
15.459018	961.094687	13.489523
15.852247	961.117265	13.494541
15.496501	970.344428	13.499559
15.747213	972.051313	13.504576
15.895549	978.834929	13.509594
15.939735	970.178806	13.514611
15.837901	952.938970	13.519629
15.786594	947.513275	13.524647
15.721016	945.273671	13.529664
15.610491	934.208299	13.534682
15.279017	936.222774	13.539699
15.461828	946.081276	13.544717
15.605430	958.131537	13.549735
15.660366	967.836607	13.554752
16.034217	965.114211	13.559770
15.619220	970.340794	13.564787
16.081993	964.171975	13.569805
15.811762	968.119719	13.574823
15.735122	974.057585	13.579840
15.776180	965.054794	13.584858
15.621246	969.461950	13.589875
15.780667	962.312132	13.594893
15.652391	967.969599	13.599911
15.580121	964.743070	13.604928
15.691721	965.201694	13.609946
15.558987	980.793136	13.614963
15.955562	992.593974	13.619981
15.771432	994.826982	13.624999
16.090077	1001.368520	13.630016
16.400741	998.067285	13.635034
16.592806	992.000664	13.640051
16.209366	983.106198	13.645069
15.832790	971.759622	13.650087
16.229841	977.754421	13.655104
16.328608	969.366400	13.660122
15.914573	967.412098	13.665139
16.370576	971.185307	13.670157
16.086309	970.968723	13.675175
16.132462	967.597643	13.680192
16.224899	977.064079	13.685210
16.261945	991.941759	13.690227
16.418032	979.990302	13.695245
16.190677	966.654623	13.700263
16.258860	962.010818	13.705280
16.277795	962.051164	13.710298
15.848002	971.575361	13.715315
16.291709	977.447705	13.720333
16.209491	985.797328	13.725351
16.397904	987.488334	13.730368
16.574863	982.375241	13.735386
16.476211	990.194204	13.740403
16.589506	970.602435	13.745421
16.489567	993.721899	13.750439
16.627704	990.212404	13.755456
16.557192	966.520775	13.760474
16.468743	960.470016	13.765491
16.402376	951.477508	13.770509
16.123891	960.620059	13.775527
16.694787	973.411790	13.780544
16.797990	982.779813	13.785562
16.360601	967.890909	13.790579
16.600908	967.880894	13.795597
16.462357	973.213343	13.800615
16.367133	988.552571	13.805632
16.669100	987.622867	13.810650
16.560995	994.187691	13.815667
16.926824	987.412346	13.820685
16.890665	998.133903	13.825703
16.005547	975.002208	13.830720
16.682667	980.065631	13.835738
16.625942	993.974520	13.840755
16.517713	990.555731	13.845773
16.554835	992.602592	13.850791
16.793019	1004.711263	13.855808
16.870595	999.822823	13.860826
16.517155	998.876450	13.865843
16.756429	1000.432497	13.870861
16.808576	1000.695271	13.875879
16.652277	993.818445	13.880896
17.047298	995.898271	13.885914
16.575027	993.170841	13.890931
16.988059	986.398128	13.895949
16.791924	995.374949	13.900967
16.565815	995.410326	13.905984
17.010664	983.343047	13.911002
16.831040	994.641962	13.916019
16.777147	991.226199	13.921037
16.623006	990.615729	13.926055
16.577416	999.096883	13.931072
17.167959	1018.043870	13.936090
16.831682	1019.065606	13.941107
16.917022	1025.618157	13.946125
17.347533	1027.648428	13.951143
16.915253	1022.817078	13.956160
17.260832	1018.114424	13.961178
17.353092	1016.408282	13.966195
17.128273	1010.354454	13.971213
17.188558	1024.352284	13.976231
17.169176	1011.243375	13.981248
17.579375	1017.985111	13.986266
16.971290	1006.463810	13.991283
17.260328	1004.781244	13.996301
17.230133	1007.420044	14.001319
16.927369	1006.617240	14.006336
17.149423	1014.556810	14.011354
17.381849	1012.822782	14.016371
17.514719	1011.571470	14.021389
17.262628	1006.151185	14.026407
17.281212	1016.895396	14.031424
17.269424	1023.114446	14.036442
17.330269	1022.913455	14.041459
17.474645	1017.899027	14.046477
17.468402	1016.988371	14.051495
17.327368	1012.728873	14.056512
17.610082	1009.185640	14.061530
17.417022	1007.144823	14.066547
17.803639	1010.199113	14.071565
17.663864	1002.442526	14.076583
17.410586	1003.587728	14.081600
17.520012	1001.938782	14.086618
17.322638	1004.844541	14.091635
17.420049	1003.915969	14.096653
17.683100	1010.774524	14.101671
17.394131	1013.863899	14.106688
17.739107	1011.666066	14.111706
17.042181	1011.732210	14.116723
17.791335	1021.144269	14.121741
17.693244	1016.032926	14.126759
17.482272	1020.150980	14.131776
17.532612	1020.608313	14.136794
17.492563	1010.839496	14.141811
17.375049	1010.361730	14.146829
17.637249	1013.739682	14.151847
17.766412	1020.650679	14.156864
17.963646	1000.395694	14.161882
17.683695	1001.900955	14.166899
17.766644	1006.672288	14.171917
17.322377	1016.824199	14.176935
17.519185	1025.187762	14.181952
17.782257	1027.881037	14.186970
17.571890	1038.393851	14.191987
18.343711	1038.897675	14.197005
18.623522	1037.847436	14.202023
18.296105	1019.717785	14.207040
18.126263	998.391165	14.212058
18.241913	998.437768	14.217075
18.314287	998.571039	14.222093
18.140051	998.841111	14.227111
17.932909	997.473381	14.232128
18.448621	994.390582	14.237146
18.132569	991.466694	14.242163
18.170782	994.722236	14.247181
18.113247	996.188182	14.252199
18.025690	1003.725442	14.257216
18.423507	1001.255731	14.262234
18.518662	994.209220	14.267251
18.130249	982.671119	14.272269
18.275556	985.782602	14.277287
17.864261	990.477367	14.282304
18.209972	996.385791	14.287322
17.810472	1002.282551	14.292339
18.202291	995.549947	14.297357
18.368047	991.837494	14.302375
18.039923	1004.025582	14.307392
18.390147	1005.004328	14.312410
17.980459	1003.131770	14.317427
17.955052	996.289995	14.322445
18.178429	999.683808	14.327463
18.310905	996.488977	14.332480
18.035131	998.658008	14.337498
18.323434	990.780298	14.342515
18.403533	987.472490	14.347533
18.353332	995.628670	14.352551
18.530760	1021.279090	14.357568
18.511625	1020.193033	14.362586
18.553474	1020.481718	14.367603
18.631871	1021.025542	14.372621
18.504489	1002.755587	14.377639
18.281007	1002.621659	14.382656
18.580587	1016.758254	14.387674
18.419733	1030.766064	14.392691
18.332451	1032.482363	14.397709
18.833394	1022.532810	14.402727
18.318846	1022.183442	14.407744
18.561236	1029.513653	14.412762
18.590168	1037.931340	14.417779
18.734666	1044.176925	14.422797
18.939452	1026.787333	14.427815
18.710118	1043.466091	14.432832
18.922957	1025.636459	14.437850
18.427692	1030.719265	14.442867
18.668052	1027.455622	14.447885
18.660111	1030.707973	14.452903
18.584164	1024.149298	14.457920
18.754935	1032.548266	14.462938
18.700011	1028.786854	14.467955
18.560419	1035.692672	14.472973
18.759621	1026.445635	14.477991
18.316180	1033.751612	14.483008
18.921974	1037.229850	14.488026
18.796398	1051.826637	14.493043
18.541186	1041.912481	14.498061
18.965108	1044.713998	14.503079
18.775965	1051.677021	14.508096
18.942975	1040.660967	14.513114
18.977938	1048.840889	14.518131
18.505680	1054.350345	14.523149
18.982185	1059.812640	14.528167
18.851510	1057.023826	14.533184
19.110840	1057.760353	14.538202
19.210231	1060.508632	14.543219
18.989981	1054.205055	14.548237
19.080458	1057.425993	14.553255
19.488507	1079.510800	14.558272
19.096449	1064.590889	14.563290
19.306012	1075.884396	14.568307
19.403014	1070.491816	14.573325
19.414754	1055.049349	14.578343
18.739128	1060.342455	14.583360
19.380736	1069.322584	14.588378
19.505166	1075.139872	14.593395
19.420845	1080.633251	14.598413
19.578154	1078.596718	14.603431
19.241592	1066.690985	14.608448
19.371642	1072.258956	14.613466
19.523513	1080.049357	14.618483
19.332059	1089.559432	14.623501
19.617362	1075.104253	14.628519
19.392825	1084.194661	14.633536
19.658680	1088.398474	14.638554
19.564591	1083.578921	14.643571
19.498819	1074.954492	14.648589
19.531987	1078.225056	14.653607
19.303606	1086.148369	14.658624
19.687650	1073.716716	14.663642
19.491929	1077.292781	14.668659
19.506117	1085.797760	14.673677
19.389817	1085.704377	14.678695
19.428572	1087.185123	14.683712
19.270093	1082.971395	14.688730
19.201226	1086.984302	14.693747
19.344418	1087.580796	14.698765
19.711450	1100.606294	14.703783
19.839990	1111.959667	14.708800
20.091423	1102.095188	14.713818
19.607463	1086.230748	14.718835
19.564357	1097.940575	14.723853
19.950266	1104.300990	14.728871
19.749977	1112.572768	14.733888
20.147172	1110.415694	14.738906
20.310061	1105.329488	14.743923
19.863455	1097.078762	14.748941
19.885473	1083.865917	14.753959
19.592472	1095.283430	14.758976
20.022759	1104.341016	14.763994
20.373235	1109.711378	14.769011
19.916324	1112.306756	14.774029
20.136520	1106.856606	14.779047
19.969977	1110.091491	14.784064
19.855468	1113.322500	14.789082
20.085620	1102.006446	14.794099
20.015466	1100.657006	14.799117
20.378175	1099.890459	14.804135
20.055829	1106.180154	14.809152
19.845950	1106.729108	14.814170
20.125284	1108.632232	14.819187
19.935202	1114.153729	14.824205
20.374346	1113.605814	14.829223
20.438556	1111.804706	14.834240
20.244838	1106.622535	14.839258
20.629557	1113.199849	14.844275
20.258498	1112.551414	14.849293
20.352277	1104.412531	14.854311
20.241679	1112.209715	14.859328
20.312217	1108.449003	14.864346
20.512305	1108.670601	14.869363
20.665537	1106.454056	14.874381
20.748293	1110.248831	14.879399
20.394618	1123.632786	14.884416
20.241461	1118.029600	14.889434
20.511347	1117.718089	14.894451
20.100988	1111.131190	14.899469
20.587076	1110.346418	14.904487
20.428876	1112.065983	14.909504
20.093095	1106.602808	14.914522
19.987910	1108.105572	14.919539
20.064567	1118.915049	14.924557
20.681449	1123.723555	14.929575
20.684011	1146.347444	14.934592
20.987051	1131.723362	14.939610
20.575686	1131.109142	14.944627
20.869233	1142.313830	14.949645
20.740365	1116.755518	14.954663
20.538521	1122.297266	14.959680
20.658447	1123.179061	14.964698
20.788596	1133.684674	14.969715
20.755839	1141.793960	14.974733
21.397291	1132.584387	14.979751
20.948858	1147.760328	14.984768
20.789845	1132.592224	14.989786
21.021108	1138.984902	14.994803
20.955646	1128.618529	14.999821
21.166562	1134.686467	15.004839
20.777080	1124.121517	15.009856
20.819200	1134.810748	15.014874
21.294250	1137.719564	15.019891
20.796408	1139.384844	15.024909
20.971654	1140.688928	15.029927
21.026978	1146.947716	15.034944
20.798117	1146.057703	15.039962
20.891764	1146.703130	15.044979
21.011301	1144.041232	15.049997
21.028193	1138.595933	15.055015
20.859339	1136.747721	15.060032
20.850495	1150.585856	15.065050
20.937534	1133.268941	15.070067
20.876675	1142.631305	15.075085
20.918680	1145.228673	15.080103
21.219700	1167.998124	15.085120
21.078650	1166.302181	15.090138
21.940776	1170.195107	15.095155
21.368282	1165.757891	15.100173
21.614750	1160.876129	15.105191
21.405511	1158.546473	15.110208
20.995819	1150.309300	15.115226
21.466319	1156.616983	15.120243
21.312954	1159.591274	15.125261
21.596986	1161.690647	15.130279
21.295075	1172.298589	15.135296
21.338561	1156.758071	15.140314
21.501192	1172.091281	15.145331
21.282981	1171.593542	15.150349
21.160089	1170.677158	15.155367
21.247667	1160.172891	15.160384
21.116118	1166.650928	15.165402
21.265981	1158.732438	15.170419
21.295461	1188.889003	15.175437
21.702552	1194.315777	15.180455
21.618333	1201.560303	15.185472
21.527442	1203.019578	15.190490
21.806216	1190.515872	15.195507
22.048406	1187.665414	15.200525
22.346062	1195.510117	15.205543
22.009275	1172.173546	15.210560
21.703649	1170.289871	15.215578
21.720645	1170.090811	15.220595
21.765617	1177.411598	15.225613
22.020925	1182.342269	15.230631
21.938538	1182.996909	15.235648
21.525170	1193.360726	15.240666
22.074196	1204.987344	15.245683
21.699215	1205.190216	15.250701
21.891374	1200.261519	15.255719
22.088472	1192.936299	15.260736
22.100022	1202.895107	15.265754
22.365851	1191.886431	15.270771
22.270786	1200.623867	15.275789
22.230686	1188.385820	15.280807
22.213744	1180.797399	15.285824
21.881326	1199.798334	15.290842
22.205313	1193.177037	15.295859
22.344685	1204.652488	15.300877
22.077027	1199.916890	15.305895
22.226409	1194.317018	15.310912
21.814725	1198.315161	15.315930
21.991219	1185.968301	15.320947
22.002443	1190.063851	15.325965
22.003959	1194.245048	15.330983
22.382836	1185.201457	15.336000
21.988598	1194.553207	15.341018
22.046234	1189.362142	15.346035
22.213157	1202.961268	15.351053
22.526100	1218.797166	15.356071
22.682661	1229.022930	15.361088
22.332448	1221.896789	15.366106
22.688270	1221.719675	15.371123
22.460278	1234.131518	15.376141
22.600652	1225.650274	15.381159
23.024089	1220.302894	15.386176
22.652059	1205.223260	15.391194
22.300389	1190.767546	15.396211
22.702284	1198.665092	15.401229
22.701087	1211.407887	15.406247
22.641967	1202.239453	15.411264
22.712406	1221.202181	15.416282
22.761395	1215.442934	15.421299
22.588287	1217.812911	15.426317
22.566476	1220.781022	15.431335
22.957734	1219.365554	15.436352
22.509351	1233.187634	15.441370
22.770696	1222.297179	15.446387
23.129340	1208.945538	15.451405
23.056299	1218.007643	15.456423
22.988281	1206.109383	15.461440
22.884686	1211.239512	15.466458
23.022871	1213.068549	15.471475
22.895692	1210.379902	15.476493
23.098441	1217.065865	15.481511
22.890936	1220.689179	15.486528
22.909226	1219.164309	15.491546
23.119754	1213.108328	15.496563
22.855170	1213.887160	15.501581
22.973793	1212.931451	15.506599
23.249937	1209.184367	15.511616
22.862679	1201.600056	15.516634
22.815465	1206.816324	15.521651
22.716719	1211.275672	15.526669
22.878938	1212.294162	15.531687
23.244171	1210.258087	15.536704
23.077874	1216.611985	15.541722
22.905292	1224.542483	15.546739
23.057152	1228.540009	15.551757
22.854984	1244.739760	15.556775
23.093444	1246.590216	15.561792
23.350191	1248.073332	15.566810
23.516857	1233.772041	15.571827
23.607066	1242.806788	15.576845
23.119410	1242.062475	15.581863
23.299493	1246.213783	15.586880
23.265235	1245.153238	15.591898
23.255818	1241.422240	15.596915
23.425855	1247.125576	15.601933
23.260989	1247.814909	15.606951
23.647987	1250.313556	15.611968
23.385296	1250.130405	15.616986
24.044284	1256.964774	15.622003
23.735407	1255.868718	15.627021
23.406299	1246.642331	15.632039
23.963271	1252.279756	15.637056
23.797763	1247.900239	15.642074
24.000048	1236.216107	15.647091
23.786562	1230.143786	15.652109
23.883530	1233.389275	15.657127
23.874163	1222.270172	15.662144
23.840417	1242.367698	15.667162
23.848541	1228.270933	15.672179
23.955251	1231.696871	15.677197
23.697528	1239.880782	15.682215
23.823984	1230.871597	15.687232
23.752765	1247.028059	15.692250
24.015548	1258.759298	15.697267
24.168516	1265.848137	15.702285
23.922805	1269.182543	15.707303
24.404740	1261.355952	15.712320
23.938743	1254.175516	15.717338
23.995126	1251.838165	15.722355
24.145561	1265.943936	15.727373
24.183358	1271.421138	15.732391
24.399289	1266.719759	15.737408
24.191020	1278.173397	15.742426
24.068703	1261.758923	15.747443
24.165448	1265.024334	15.752461
24.169924	1269.172390	15.757479
24.314359	1260.580432	15.762496
23.985298	1271.944987	15.767514
23.935956	1268.942132	15.772531
24.274588	1266.205428	15.777549
24.252897	1261.996601	15.782567
24.068937	1261.414273	15.787584
24.277679	1261.564374	15.792602
24.266627	1261.900186	15.797619
24.457880	1253.898440	15.802637
24.466961	1257.107481	15.807655
24.305005	1264.195616	15.812672
24.316400	1275.979237	15.817690
24.659835	1290.443238	15.822707
24.628765	1287.412756	15.827725
24.460538	1287.468878	15.832743
24.916726	1283.687102	15.837760
24.792392	1290.992228	15.842778
24.709841	1278.857371	15.847795
25.060706	1272.211719	15.852813
24.591188	1277.039795	15.857831
24.968754	1264.588001	15.862848
24.848321	1266.934518	15.867866
24.616113	1257.755881	15.872883
24.814654	1264.144572	15.877901
24.587692	1266.408315	15.882919
24.766047	1279.539151	15.887936
24.931717	1285.504209	15.892954
24.937847	1283.331041	15.897971
25.110201	1282.984274	15.902989
25.070364	1292.917583	15.908007
25.122061	1291.958758	15.913024
25.251644	1296.969881	15.918042
25.011662	1284.944685	15.923059
25.313907	1267.087403	15.928077
24.932752	1289.032501	15.933095
24.857366	1292.428318	15.938112
25.251272	1292.094931	15.943130
24.913506	1281.995471	15.948147
25.069241	1289.026588	15.953165
24.921083	1288.559388	15.958183
25.156881	1277.281046	15.963200
24.973391	1276.621092	15.968218
25.064755	1283.907889	15.973235
25.263259	1287.174399	15.978253
25.002359	1285.862173	15.983271
25.052365	1286.829734	15.988288
25.370551	1302.358990	15.993306
25.437257	1314.262615	15.998323
25.479178	1323.346722	16.003341
25.371130	1318.691388	16.008359
25.622083	1313.380747	16.013376
25.587571	1317.789752	16.018394
25.464533	1316.453560	16.023411
25.816956	1317.304619	16.028429
25.593036	1302.240762	16.033447
25.846809	1303.467325	16.038464
25.731737	1308.816872	16.043482
25.542966	1308.846079	16.048499
25.747668	1305.583744	16.053517
25.648096	1309.702359	16.058535
25.835635	1305.421940	16.063552
25.825635	1319.422206	16.068570
25.832541	1317.026298	16.073587
26.118988	1309.756522	16.078605
25.874705	1310.922697	16.083623
25.913627	1317.874721	16.088640
25.975952	1316.707474	16.093658
25.980895	1309.975489	16.098675
25.986814	1301.126714	16.103693
25.975427	1306.419958	16.108711
26.291855	1302.680759	16.113728
26.349108	1302.523659	16.118746
25.847522	1302.844291	16.123763
25.665902	1287.588247	16.128781
26.147620	1301.715081	16.133799
26.233307	1303.616772	16.138816
26.142925	1306.208097	16.143834
26.064438	1301.267017	16.148851
26.254183	1317.170417	16.153869
26.192041	1309.717730	16.158887
26.201091	1305.028287	16.163904
26.314888	1314.884653	16.168922
26.147761	1318.359605	16.173939
26.207819	1311.407320	16.178957
26.314323	1314.195211	16.183975
26.192595	1306.423089	16.188992
26.340108	1311.925082	16.194010
25.737041	1309.918520	16.199027
26.379746	1310.283677	16.204045
26.466619	1327.555277	16.209063
25.944342	1331.250909	16.214080
26.403077	1329.974456	16.219098
26.244870	1356.173943	16.224115
26.478146	1345.859419	16.229133
26.482151	1348.812266	16.234151
26.560437	1341.582781	16.239168
26.575318	1331.237044	16.244186
26.398857	1340.587927	16.249203
26.797951	1331.128172	16.254221
26.233562	1341.407021	16.259239
26.384717	1349.339586	16.264256
26.843846	1357.003770	16.269274
26.838030	1374.520434	16.274291
27.087147	1357.372125	16.279309
27.148723	1360.519174	16.284327
26.844532	1356.764037	16.289344
27.333427	1359.068131	16.294362
27.051882	1355.653103	16.299379
27.041428	1330.920814	16.304397
26.873968	1339.666749	16.309415
27.048992	1352.762770	16.314432
27.212755	1355.899229	16.319450
26.913594	1362.326121	16.324467
27.189795	1360.408663	16.329485
27.132206	1355.276539	16.334503
27.101667	1361.930261	16.339520
27.174602	1345.960728	16.344538
27.378906	1358.244348	16.349555
27.093285	1355.281901	16.354573
27.289332	1367.997150	16.359591
27.219965	1367.039432	16.364608
27.450779	1361.729742	16.369626
27.471574	1364.993161	16.374643
27.397477	1357.215503	16.379661
27.357677	1364.548617	16.384679
27.227585	1359.275935	16.389696
27.537161	1356.702855	16.394714
27.403392	1355.410356	16.399731
27.276562	1346.783858	16.404749
27.245294	1364.398404	16.409767
27.192884	1348.874130	16.414784
27.671354	1359.346544	16.419802
27.701559	1371.241681	16.424819
27.968815	1376.523149	16.429837
27.827174	1365.858617	16.434855
27.377920	1357.137779	16.439872
27.748611	1363.377212	16.444890
27.694721	1381.569256	16.449907
28.098087	1377.087032	16.454925
27.988447	1383.741633	16.459943
27.854225	1365.013580	16.464960
28.215703	1362.325243	16.469978
27.751626	1365.572151	16.474995
27.859697	1353.905074	16.480013
28.116996	1368.233011	16.485031
27.813269	1373.627929	16.490048
28.150580	1377.672001	16.495066
27.883913	1380.323373	16.500083
27.852372	1374.507699	16.505101
27.906094	1377.156707	16.510119
27.949657	1384.708306	16.515136
27.795657	1388.319274	16.520154
27.824820	1394.481517	16.525171
27.822402	1394.132138	16.530189
27.689810	1388.195973	16.535207
27.920604	1397.858278	16.540224
28.531302	1396.186284	16.545242
28.232772	1410.871828	16.550259
28.587857	1405.790961	16.555277
28.750035	1405.926912	16.560295
28.582895	1404.966455	16.565312
28.363682	1381.176140	16.570330
28.609731	1396.655019	16.575347
28.372351	1385.130232	16.580365
28.507824	1389.805221	16.585383
28.498888	1399.650038	16.590400
28.721548	1401.610984	16.595418
28.478924	1407.250703	16.600435
29.183083	1397.494856	16.605453
28.706036	1384.783660	16.610471
28.446435	1382.448711	16.615488
28.539493	1397.344294	16.620506
28.871355	1414.734146	16.625523
28.612632	1412.021932	16.630541
28.702569	1404.308273	16.635559
28.844082	1408.732105	16.640576
28.972171	1403.613763	16.645594
28.954068	1419.718327	16.650611
28.931237	1409.606889	16.655629
29.163131	1413.472553	16.660647
28.813144	1405.664096	16.665664
29.012912	1405.750533	16.670682
28.776660	1401.099434	16.675699
28.649184	1401.716265	16.680717
28.935594	1403.409624	16.685735
28.900655	1411.008653	16.690752
29.102680	1411.807812	16.695770
29.070385	1416.035203	16.700787
29.085840	1401.322780	16.705805
29.433026	1406.305260	16.710823
28.925425	1421.448142	16.715840
29.301908	1415.737442	16.720858
28.963938	1431.048337	16.725875
29.443679	1432.291105	16.730893
29.133103	1432.482153	16.735911
29.115387	1435.920434	16.740928
29.521774	1433.859618	16.745946
29.519876	1436.219836	16.750963
29.352683	1441.060394	16.755981
29.519389	1428.615365	16.760999
29.385027	1442.842566	16.766016
29.768641	1429.509440	16.771034
29.672985	1425.147262	16.776051
29.653101	1434.730954	16.781069
29.451477	1437.696347	16.786087
29.331100	1443.450308	16.791104
29.511268	1428.410087	16.796122
29.785897	1453.361988	16.801139
29.857906	1455.009102	16.806157
30.022775	1453.294850	16.811175
29.696354	1445.064422	16.816192
30.193461	1449.563146	16.821210
30.145021	1445.191388	16.826227
29.730206	1437.687487	16.831245
30.218364	1447.798370	16.836263
29.930164	1432.522792	16.841280
30.006775	1421.792630	16.846298
29.813622	1435.446941	16.851315
30.434414	1437.884349	16.856333
30.188970	1439.845896	16.861351
30.183087	1438.390345	16.866368
30.115267	1436.994827	16.871386
30.159035	1435.969793	16.876403
30.312230	1442.725650	16.881421
30.454560	1447.503643	16.886439
30.248301	1445.409246	16.891456
30.361497	1444.737454	16.896474
30.289460	1439.240808	16.901491
30.355026	1444.927432	16.906509
30.286420	1440.907978	16.911527
30.329702	1448.567515	16.916544
30.403337	1444.255297	16.921562
30.379577	1445.406493	16.926579
30.210945	1434.941820	16.931597
30.696379	1442.821947	16.936615
30.625228	1447.428161	16.941632
30.815815	1443.306628	16.946650
30.617252	1441.315277	16.951667
30.537953	1452.860314	16.956685
30.953197	1448.513293	16.961703
30.432107	1443.712231	16.966720
30.421518	1445.570999	16.971738
30.541007	1443.310973	16.976755
30.364009	1439.480866	16.981773
30.675787	1455.516782	16.986791
30.840662	1473.504497	16.991808
30.965527	1470.411994	16.996826
30.788841	1473.738973	17.001843
31.039777	1466.560414	17.006861
31.328696	1460.008177	17.011879
31.118387	1469.771766	17.016896
31.241379	1463.476642	17.021914
31.233509	1479.018430	17.026931
31.153098	1463.637626	17.031949
31.529156	1470.659382	17.036967
31.336208	1476.371418	17.041984
31.493267	1461.695764	17.047002
31.117519	1456.988183	17.052019
31.424092	1473.282424	17.057037
31.714165	1457.034993	17.062055
31.364328	1443.904745	17.067072
31.129411	1440.087162	17.072090
31.348256	1441.156931	17.077107
31.273936	1457.557599	17.082125
31.475643	1457.889157	17.087143
31.209214	1465.575675	17.092160
31.435192	1461.878155	17.097178
31.582958	1464.143771	17.102195
31.337246	1466.826925	17.107213
31.456069	1466.530531	17.112231
31.414044	1462.611784	17.117248
31.442192	1450.284701	17.122266
31.454330	1467.938052	17.127283
31.745254	1483.147235	17.132301
32.079688	1488.384573	17.137319
32.034794	1502.480918	17.142336
31.973922	1477.839981	17.147354
31.866419	1471.398127	17.152371
31.484213	1471.705528	17.157389
32.193186	1480.425588	17.162407
31.914964	1496.759416	17.167424
31.981670	1485.777335	17.172442
32.102718	1479.887002	17.177459
32.054605	1493.455395	17.182477
32.162939	1489.024453	17.187495
32.005684	1494.700483	17.192512
32.493290	1497.074095	17.197530
32.030137	1483.960374	17.202547
31.879598	1493.764488	17.207565
32.170605	1483.416121	17.212583
32.030312	1485.646088	17.217600
31.972906	1488.498889	17.222618
32.301746	1495.536726	17.227635
32.215042	1492.231969	17.232653
32.507018	1488.364304	17.237671
32.308503	1492.970912	17.242688
32.065777	1484.452258	17.247706
32.353743	1491.745832	17.252723
32.318979	1513.065573	17.257741
32.800785	1504.836373	17.262759
32.569164	1510.009803	17.267776
32.621561	1523.889131	17.272794
32.764575	1525.409178	17.277811
32.262779	1518.706717	17.282829
32.711135	1519.193358	17.287847
32.389291	1518.008884	17.292864
32.768570	1508.075387	17.297882
32.916809	1517.574071	17.302899
32.414242	1516.490124	17.307917
32.804333	1512.745394	17.312935
33.106586	1524.145945	17.317952
33.001605	1535.180786	17.322970
32.966414	1522.495459	17.327987
33.001427	1536.326495	17.333005
33.419831	1533.876132	17.338023
33.088625	1523.031230	17.343040
33.269507	1524.081692	17.348058
33.273760	1525.389071	17.353075
33.030939	1530.999343	17.358093
33.328511	1535.821976	17.363111
33.467049	1543.488256	17.368128
33.390615	1536.704668	17.373146
33.407411	1531.086236	17.378163
33.634796	1531.301755	17.383181
33.463041	1511.575916	17.388199
33.302143	1496.699262	17.393216
33.630100	1514.617562	17.398234
33.284937	1514.427368	17.403251
33.249788	1529.336591	17.408269
33.658226	1525.455181	17.413287
33.725860	1537.547976	17.418304
33.518927	1536.468708	17.423322
33.571677	1538.051896	17.428339
33.455322	1531.032024	17.433357
33.753855	1531.219646	17.438375
33.468300	1542.128447	17.443392
33.759679	1531.538089	17.448410
33.680265	1524.816801	17.453427
33.373502	1524.304750	17.458445
33.709165	1529.592483	17.463463
33.837147	1557.069851	17.468480
34.128697	1557.348577	17.473498
34.229661	1558.681506	17.478515
34.077926	1564.891623	17.483533
34.354341	1552.178395	17.488551
34.021642	1550.903598	17.493568
34.293284	1557.503728	17.498586
34.410480	1554.907099	17.503603
33.988983	1547.338705	17.508621
34.590220	1562.897423	17.513639
34.270765	1541.238913	17.518656
33.952519	1545.724396	17.523674
34.291151	1545.562127	17.528691
34.244002	1566.571035	17.533709
34.330808	1558.519275	17.538727
34.498220	1557.409832	17.543744
34.557338	1556.336983	17.548762
34.857015	1553.841481	17.553779
34.495478	1565.422616	17.558797
34.887862	1557.576428	17.563815
34.586980	1562.456044	17.568832
34.782092	1565.156906	17.573850
34.756306	1553.798378	17.578867
34.530385	1568.769476	17.583885
34.267988	1558.576089	17.588903
34.734977	1557.545469	17.593920
34.345821	1560.742638	17.598938
34.798814	1555.484539	17.603955
34.739653	1567.672121	17.608973
34.784744	1561.148523	17.613991
34.715335	1554.209454	17.619008
34.444547	1551.642498	17.624026
34.893082	1573.804781	17.629043
34.573672	1596.582921	17.634061
34.916882	1594.573072	17.639079
35.238140	1587.675714	17.644096
34.954799	1584.734299	17.649114
34.846411	1588.530468	17.654131
35.104795	1586.607858	17.659149
35.360699	1579.541405	17.664167
35.457482	1586.575119	17.669184
34.962081	1591.788034	17.674202
35.313342	1590.296870	17.679219
35.426221	1606.960033	17.684237
35.540392	1613.400209	17.689255
35.617555	1607.877468	17.694272
35.698509	1619.820113	17.699290
35.787419	1597.452186	17.704307
35.514646	1587.400044	17.709325
35.558925	1598.956261	17.714343
35.851227	1607.001247	17.719360
35.678114	1607.132774	17.724378
35.883915	1606.674384	17.729395
35.944772	1611.869781	17.734413
35.771364	1604.181827	17.739431
35.943206	1593.182886	17.744448
35.779367	1606.603988	17.749466
36.031292	1596.665302	17.754483
35.708208	1606.887128	17.759501
35.763035	1597.374470	17.764519
35.964319	1601.218078	17.769536
35.870049	1610.646870	17.774554
35.891238	1606.003551	17.779571
35.837132	1610.530431	17.784589
35.840088	1610.623414	17.789607
36.123316	1617.794224	17.794624
36.028984	1620.322089	17.799642
36.255331	1601.768976	17.804659
36.357166	1611.321837	17.809677
36.394047	1622.642315	17.814695
36.480746	1620.794918	17.819712
36.303649	1631.410498	17.824730
36.644867	1629.563553	17.829747
36.846995	1636.261808	17.834765
36.601147	1621.971839	17.839783
36.472418	1606.674064	17.844800
36.733230	1606.162494	17.849818
36.716859	1605.652838	17.854835
36.463307	1608.121984	17.859853
36.621655	1611.211955	17.864871
36.664703	1629.085553	17.869888
36.578826	1639.466798	17.874906
36.741506	1637.901099	17.879923
36.800868	1630.737590	17.884941
36.566809	1631.965673	17.889959
36.812020	1620.757170	17.894976
36.514476	1623.118051	17.899994
36.798387	1627.348160	17.905011
37.030069	1626.147589	17.910029
36.907844	1618.479315	17.915047
36.971971	1619.356582	17.920064
36.861284	1618.369854	17.925082
37.074960	1629.826062	17.930099
37.148644	1650.241956	17.935117
37.541812	1658.701746	17.940135
37.477304	1646.879525	17.945152
37.059862	1646.189720	17.950170
37.215386	1641.795812	17.955187
37.447785	1660.809473	17.960205
37.076238	1660.524436	17.965223
37.158007	1659.470079	17.970240
37.104111	1672.898067	17.975258
37.610015	1656.791116	17.980275
37.658609	1664.989387	17.985293
37.406231	1650.418023	17.990311
37.295672	1650.508311	17.995328
37.459214	1650.497599	18.000346
37.510131	1658.673241	18.005363
37.789374	1674.111880	18.010381
37.796479	1679.682282	18.015399
37.867018	1672.751721	18.020416
37.942670	1675.880171	18.025434
38.422648	1669.809007	18.030451
38.178284	1672.976957	18.035469
38.205685	1675.136526	18.040487
38.168855	1652.850511	18.045504
38.347581	1649.547521	18.050522
38.127058	1632.489509	18.055539
38.227638	1636.950680	18.060557
38.120521	1635.004223	18.065575
38.175051	1630.394753	18.070592
38.102947	1640.571189	18.075610
38.335625	1644.222633	18.080627
38.304247	1655.642201	18.085645
38.407601	1672.433371	18.090663
38.694147	1669.815626	18.095680
38.469526	1666.277748	18.100698
38.142180	1673.093830	18.105715
38.484014	1666.186148	18.110733
38.435593	1676.722233	18.115751
38.626363	1667.570093	18.120768
38.544809	1671.717319	18.125786
38.530237	1663.396661	18.130803
38.532635	1665.287558	18.135821
38.377790	1666.666314	18.140839
38.609356	1662.148430	18.145856
38.193241	1677.883263	18.150874
38.652528	1690.127964	18.155891
38.843923	1698.468973	18.160909
38.627467	1701.317196	18.165927
38.692814	1703.525806	18.170944
38.811458	1700.329966	18.175962
39.028393	1695.090755	18.180979
39.210808	1701.140993	18.185997
39.051819	1693.536625	18.191015
39.475897	1691.415183	18.196032
39.315283	1699.626197	18.201050
39.046900	1696.900570	18.206067
39.210448	1694.658224	18.211085
39.368646	1693.528840	18.216103
39.366331	1692.387796	18.221120
39.107686	1699.070110	18.226138
39.375222	1713.810803	18.231155
39.942085	1719.168454	18.236173
39.635974	1721.147737	18.241191
39.668443	1707.044346	18.246208
39.518597	1700.848145	18.251226
39.364146	1702.899006	18.256243
39.497275	1700.648499	18.261261
39.450002	1717.393752	18.266279
39.855657	1724.111752	18.271296
39.779065	1729.959950	18.276314
39.760665	1724.576766	18.281331
39.918947	1716.643805	18.286349
39.807069	1726.677478	18.291367
39.802303	1712.718408	18.296384
40.040616	1721.823832	18.301402
40.098688	1710.258636	18.306419
40.194437	1712.186861	18.311437
40.045704	1715.430147	18.316455
40.306147	1724.706700	18.321472
40.284765	1714.939271	18.326490
40.427699	1717.863129	18.331507
40.551852	1714.271146	18.336525
40.026542	1722.811307	18.341543
40.157705	1708.915595	18.346560
40.302141	1706.382542	18.351578
40.244737	1706.048738	18.356595
40.150798	1704.162686	18.361613
40.153215	1716.200068	18.366631
40.254530	1724.001316	18.371648
40.354131	1734.400394	18.376666
40.545203	1736.873436	18.381683
40.907098	1736.775819	18.386701
40.699923	1739.546341	18.391719
41.108453	1744.456007	18.396736
40.765362	1742.056068	18.401754
40.501783	1742.858181	18.406771
40.895392	1741.443461	18.411789
40.661059	1744.985907	18.416807
40.877958	1742.664470	18.421824
40.887908	1737.564950	18.426842
41.029047	1735.261348	18.431859
41.129630	1728.276394	18.436877
40.625491	1740.980118	18.441895
40.926274	1749.225527	18.446912
41.275300	1766.082685	18.451930
41.668102	1758.263489	18.456947
41.644727	1756.284479	18.461965
41.603272	1766.757474	18.466983
41.800383	1744.188009	18.472000
41.632108	1737.296098	18.477018
41.248467	1736.245821	18.482035
41.350811	1725.639920	18.487053
41.283177	1738.580134	18.492071
41.706701	1757.653265	18.497088
41.731256	1759.356280	18.502106
41.573511	1758.765466	18.507123
41.643777	1761.473020	18.512141
41.482915	1750.343929	18.517159
41.971857	1754.551410	18.522176
42.252209	1755.287452	18.527194
41.865164	1756.848077	18.532211
42.332919	1749.602655	18.537229
42.192125	1755.755927	18.542247
42.248834	1757.702223	18.547264
42.059968	1745.447180	18.552282
41.691606	1747.633977	18.557299
42.030554	1742.883978	18.562317
42.127070	1758.594604	18.567335
42.319862	1757.193976	18.572352
42.208203	1749.089293	18.577370
42.185169	1759.946992	18.582387
42.530865	1749.742936	18.587405
42.191359	1753.353153	18.592423
42.320250	1746.398548	18.597440
42.460303	1744.468704	18.602458
42.170297	1754.469044	18.607475
42.365867	1752.356422	18.612493
42.333193	1757.790725	18.617511
42.366419	1755.259115	18.622528
42.538220	1747.193014	18.627546
42.309731	1761.272106	18.632563
42.799977	1769.548021	18.637581
42.872211	1779.129892	18.642599
43.134926	1778.929779	18.647616
43.065580	1779.519697	18.652634
42.783719	1784.808005	18.657651
42.937494	1771.944607	18.662669
42.979133	1775.423542	18.667687
43.200406	1767.114635	18.672704
43.606472	1778.628717	18.677722
42.924534	1770.442103	18.682739
43.475883	1765.624717	18.687757
43.321133	1773.847005	18.692775
43.333158	1763.377841	18.697792
43.737507	1752.060080	18.702810
43.445408	1746.150331	18.707827
43.492772	1743.180608	18.712845
43.502706	1745.418852	18.717863
43.001376	1733.826411	18.722880
43.143639	1742.221030	18.727898
43.370092	1761.037593	18.732915
43.442800	1761.317453	18.737933
43.224233	1770.852110	18.742951
43.381036	1762.302705	18.747968
43.582038	1766.269813	18.752986
43.705726	1763.703569	18.758003
43.693247	1766.834596	18.763021
43.802391	1773.587840	18.768039
43.791186	1787.187593	18.773056
43.797151	1782.085961	18.778074
43.781484	1787.185611	18.783091
43.916492	1779.231860	18.788109
44.102659	1786.282584	18.793127
43.867260	1782.849992	18.798144
43.993288	1783.732391	18.803162
43.931586	1775.602118	18.808179
44.389729	1769.258177	18.813197
44.293296	1775.596822	18.818215
44.349154	1776.290839	18.823232
44.335821	1781.352310	18.828250
44.179434	1787.920923	18.833267
44.064827	1800.495763	18.838285
44.280390	1804.656319	18.843303
44.500650	1794.070448	18.848320
44.551593	1794.580849	18.853338
44.590164	1806.206662	18.858355
44.473980	1797.324832	18.863373
44.177213	1809.296583	18.868391
44.883725	1806.252366	18.873408
44.936193	1795.867826	18.878426
44.778831	1808.362149	18.883443
44.948060	1812.146744	18.888461
44.725084	1813.733798	18.893479
45.064879	1823.607271	18.898496
45.622497	1828.059499	18.903514
45.169819	1825.723911	18.908531
45.135928	1814.242527	18.913549
44.974650	1807.237236	18.918567
45.376368	1811.673494	18.923584
45.479084	1827.213892	18.928602
45.146231	1820.097790	18.933619
45.532499	1820.921045	18.938637
45.675060	1832.999919	18.943655
45.370128	1820.459304	18.948672
45.590738	1822.380885	18.953690
45.307250	1825.675594	18.958707
45.685854	1817.126706	18.963725
45.645863	1834.918803	18.968743
45.553415	1822.820778	18.973760
45.808519	1826.209927	18.978778
45.378298	1837.856547	18.983795
45.785123	1823.429598	18.988813
46.220347	1830.198462	18.993831
45.990433	1826.080774	18.998848
45.971116	1819.224636	19.003866
45.742761	1822.600775	19.008883
46.098924	1819.122575	19.013901
46.591601	1828.183863	19.018919
46.395125	1822.683041	19.023936
46.409699	1820.750698	19.028954
46.179885	1833.013537	19.033971
46.049579	1823.907868	19.038989
46.106323	1824.214578	19.044007
46.090864	1833.449989	19.049024
46.210829	1826.353137	19.054042
46.081940	1827.499493	19.059059
46.310552	1834.149172	19.064077
46.323416	1841.804090	19.069095
46.054689	1861.202356	19.074112
46.415274	1858.338511	19.079130
46.443388	1856.876318	19.084147
46.656250	1854.642531	19.089165
46.904095	1852.818667	19.094183
46.816529	1846.038553	19.099200
47.105221	1843.689097	19.104218
46.661283	1856.082407	19.109235
46.733631	1842.284867	19.114253
46.690872	1869.674093	19.119271
47.212661	1868.013596	19.124288
47.235245	1869.525631	19.129306
47.008148	1890.069493	19.134323
47.134649	1872.433842	19.139341
47.501720	1866.740672	19.144359
47.194517	1883.071627	19.149376
47.389539	1877.664339	19.154394
47.335666	1877.064425	19.159411
47.657011	1867.527831	19.164429
47.748701	1875.930882	19.169447
47.575462	1878.459034	19.174464
48.235965	1866.932537	19.179482
47.845482	1858.101906	19.184499
47.765131	1865.190018	19.189517
47.863443	1856.565197	19.194535
47.777705	1868.952467	19.199552
47.545006	1865.236368	19.204570
47.937831	1871.711895	19.209587
47.560844	1868.505219	19.214605
47.882222	1871.953694	19.219623
47.705821	1865.601989	19.224640
47.816719	1864.613663	19.229658
47.721946	1863.665623	19.234675
47.698457	1869.172063	19.239693
48.353646	1889.543157	19.244711
48.008109	1896.867606	19.249728
48.425191	1899.021662	19.254746
48.213670	1893.420161	19.259763
48.323603	1900.253835	19.264781
48.442921	1890.006594	19.269799
48.424624	1901.315925	19.274816
48.336947	1893.750455	19.279834
48.321149	1887.920766	19.284851
48.003662	1897.574593	19.289869
47.997820	1891.920011	19.294887
48.418344	1906.982817	19.299904
49.048973	1921.648748	19.304922
48.828733	1934.024836	19.309939
49.102087	1915.812166	19.314957
49.287563	1907.386080	19.319975
49.211689	1919.454076	19.324992
49.321462	1910.316556	19.330010
49.076433	1896.026983	19.335027
49.081726	1902.752962	19.340045
49.422800	1894.168703	19.345063
49.564018	1901.293437	19.350080
49.321806	1887.187639	19.355098
49.043111	1887.979266	19.360115
49.335306	1894.952289	19.365133
49.166197	1894.718232	19.370151
49.185998	1908.077362	19.375168
49.378354	1906.077838	19.380186
49.409887	1901.344542	19.385203
49.174914	1914.740466	19.390221
49.424494	1899.165140	19.395239
49.321008	1903.787855	19.400256
49.478031	1913.355404	19.405274
49.827284	1944.204626	19.410291
49.864908	1940.734753	19.415309
50.147976	1939.283368	19.420327
49.857182	1950.774170	19.425344
50.013531	1931.158122	19.430362
50.183894	1938.955155	19.435379
50.158268	1937.841762	19.440397
50.525628	1926.316819	19.445415
50.088487	1925.853460	19.450432
50.387570	1927.481406	19.455450
50.246925	1927.040499	19.460467
50.248575	1932.927021	19.465485
50.198429	1927.951137	19.470503
50.114290	1941.094424	19.475520
50.178125	1934.155406	19.480538
50.499237	1941.195318	19.485555
50.318511	1947.112967	19.490573
50.601240	1944.587530	19.495591
50.760293	1956.803329	19.500608
50.738181	1956.088921	19.505626
51.061796	1959.019184	19.510643
50.896458	1949.253942	19.515661
51.490926	1955.769206	19.520679
51.111114	1966.051425	19.525696
51.176302	1956.109316	19.530714
51.124058	1956.536785	19.535731
51.415073	1948.770729	19.540749
50.942477	1936.844676	19.545767
51.129271	1945.183825	19.550784
51.044410	1950.836642	19.555802
51.655909	1955.076480	19.560819
51.290534	1949.842476	19.565837
51.338856	1953.374279	19.570855
51.088592	1956.867639	19.575872
51.262908	1955.816470	19.580890
51.558070	1951.623196	19.585907
51.226738	1958.079663	19.590925
51.634062	1958.816188	19.595943
51.380610	1960.462619	19.600960
51.440233	1958.317520	19.605978
51.662739	1968.826158	19.610995
51.763201	1992.873949	19.616013
52.083660	1992.640869	19.621031
51.891203	1995.983754	19.626048
52.073423	1980.731062	19.631066
52.181062	1986.911870	19.636083
51.789636	1978.859203	19.641101
52.042189	1977.227442	19.646119
52.050827	1986.834124	19.651136
52.311731	1987.175202	19.656154
51.735555	1979.251482	19.661171
51.983673	1998.010625	19.666189
52.464971	1994.452265	19.671207
52.268521	2015.608297	19.676224
52.390902	2002.950072	19.681242
52.689445	2015.257225	19.686259
52.355925	2017.396572	19.691277
52.787978	2014.053609	19.696295
52.681787	2012.596078	19.701312
52.858580	2014.470992	19.706330
52.789419	2011.595664	19.711347
52.600920	2010.528865	19.716365
52.915707	2010.307942	19.721383
52.847749	2020.871308	19.726400
52.775776	2030.523618	19.731418
53.223115	2033.908406	19.736435
53.446537	2038.899737	19.741453
53.346908	2029.406432	19.746471
53.350159	2037.637983	19.751488
53.201539	2032.425409	19.756506
53.346589	2027.390467	19.761523
52.873756	2032.984801	19.766541
53.382215	2031.838058	19.771559
53.207275	2035.980344	19.776576
53.570580	2033.470119	19.781594
53.474135	2029.646038	19.786611
53.239609	2029.955810	19.791629
53.464836	2038.571112	19.796647
54.004208	2055.451459	19.801664
53.835665	2056.576827	19.806682
54.322854	2041.241005	19.811699
54.294432	2053.265047	19.816717
54.609583	2047.410722	19.821735
54.630433	2048.689027	19.826752
54.400635	2048.509677	19.831770
53.956590	2016.523811	19.836787
53.935605	2014.736481	19.841805
54.361187	2037.419912	19.846823
54.228093	2034.435273	19.851840
54.260849	2042.793828	19.856858
54.263679	2031.948674	19.861875
54.370322	2037.096298	19.866893
54.539905	2039.088144	19.871911
54.265669	2042.012900	19.876928
54.581730	2028.738055	19.881946
54.563411	2029.588817	19.886963
54.478950	2045.123953	19.891981
54.682811	2055.908147	19.896999
54.827616	2064.919396	19.902016
55.120759	2073.651830	19.907034
55.266510	2071.372611	19.912051
55.021472	2072.345282	19.917069
54.881851	2070.982829	19.922087
55.010204	2073.442475	19.927104
54.910090	2069.134585	19.932122
55.065692	2062.422646	19.937139
55.057629	2069.036939	19.942157
55.148796	2063.930975	19.947175
55.344752	2063.164780	19.952192
55.498268	2085.686567	19.957210
55.525090	2082.368631	19.962227
55.712696	2099.341602	19.967245
55.622636	2096.969667	19.972263
55.827327	2101.411407	19.977280
55.567492	2101.272844	19.982298
55.800289	2091.109267	19.987315
55.115400	2094.630588	19.992333
55.674250	2101.401975	19.997351
56.002528	2091.877286	20.002368
55.906701	2085.524968	20.007386
56.273942	2081.510479	20.012403
55.976819	2081.272969	20.017421
56.172876	2102.612660	20.022439
56.590598	2101.602353	20.027456
56.406752	2111.285209	20.032474
56.658061	2107.415254	20.037491
56.228295	2108.153714	20.042509
56.465316	2104.628020	20.047527
56.799194	2116.826668	20.052544
56.870865	2112.327598	20.057562
56.884365	2105.983187	20.062579
56.709677	2106.878098	20.067597
57.085605	2109.736563	20.072615
56.803248	2106.517741	20.077632
56.576857	2110.074900	20.082650
56.915388	2111.090495	20.087667
56.852462	2114.027977	20.092685
56.875436	2112.406978	20.097703
57.223600	2109.321538	20.102720
57.004160	2103.299652	20.107738
57.138145	2101.045403	20.112755
57.022154	2114.750746	20.117773
57.312256	2110.925950	20.122791
57.198847	2106.410816	20.127808
57.184950	2122.182576	20.132826
57.253862	2124.407192	20.137843
57.333053	2132.997275	20.142861
57.390160	2136.256235	20.147879
57.799205	2124.869322	20.152896
57.479639	2128.743628	20.157914
57.568915	2127.458688	20.162931
57.564340	2131.648233	20.167949
57.663484	2145.300926	20.172967
57.569694	2155.574190	20.177984
57.742949	2161.544242	20.183002
58.091128	2154.623879	20.188019
57.816137	2159.637383	20.193037
58.400142	2145.161369	20.198055
58.309455	2144.373253	20.203072
58.310655	2159.209957	20.208090
58.522852	2144.016713	20.213107
58.105896	2146.006296	20.218125
58.351576	2161.479709	20.223143
58.547988	2167.660485	20.228160
58.276677	2178.225676	20.233178
58.630913	2187.884221	20.238195
58.740837	2181.070339	20.243213
58.627749	2178.610079	20.248231
58.820430	2187.899882	20.253248
58.480813	2186.857846	20.258266
58.658017	2179.215985	20.263283
58.841038	2189.151229	20.268301
59.166339	2200.045367	20.273319
59.262401	2202.470412	20.278336
59.132923	2211.489872	20.283354
59.155308	2209.171575	20.288371
59.590797	2219.409972	20.293389
59.512561	2215.335218	20.298407
59.847619	2208.585686	20.303424
59.317524	2222.693387	20.308442
59.382364	2214.873440	20.313459
59.650765	2208.643150	20.318477
59.572857	2207.251590	20.323495
59.894595	2203.195578	20.328512
59.677637	2209.624982	20.333530
59.783323	2198.740077	20.338547
59.846157	2191.097427	20.343565
59.571188	2199.253004	20.348583
59.810081	2197.032975	20.353600
59.958935	2200.232893	20.358618
60.066894	2197.987852	20.363635
60.195118	2205.737264	20.368653
60.079547	2239.471339	20.373671
60.281191	2231.686054	20.378688
60.009454	2227.947974	20.383706
60.222762	2233.968910	20.388723
60.430383	2233.344469	20.393741
60.104848	2232.581379	20.398759
60.405808	2230.120398	20.403776
60.687634	2235.347005	20.408794
60.629738	2232.251287	20.413811
60.850851	2246.478749	20.418829
60.762712	2247.551280	20.423847
61.244209	2244.367407	20.428864
61.177364	2245.607666	20.433882
61.569506	2244.583469	20.438899
61.531471	2243.508519	20.443917
61.278133	2244.323332	20.448935
61.355593	2234.234934	20.453952
61.165066	2243.858548	20.458970
61.303841	2238.802528	20.463987
61.451727	2236.795155	20.469005
61.373159	2236.401063	20.474023
61.671895	2249.078224	20.479040
61.677398	2239.271377	20.484058
61.581157	2238.627863	20.489075
61.732364	2233.815047	20.494093
61.648982	2230.858570	20.499111
61.788984	2226.487730	20.504128
61.465768	2244.146803	20.509146
61.768324	2228.778713	20.514163
62.098118	2250.362038	20.519181
61.840778	2269.640637	20.524199
62.011558	2265.059598	20.529216
62.402855	2267.227220	20.534234
62.384131	2269.961380	20.539251
62.374565	2269.631863	20.544269
62.082681	2266.207904	20.549287
62.399708	2255.306341	20.554304
62.210989	2263.141620	20.559322
62.561092	2251.412217	20.564339
62.367055	2262.217038	20.569357
63.040209	2291.709005	20.574375
63.032658	2279.421802	20.579392
62.895057	2290.251565	20.584410
62.794520	2284.987065	20.589427
62.893356	2278.443259	20.594445
62.756475	2293.587142	20.599463
63.094607	2285.051969	20.604480
63.443129	2288.120098	20.609498
63.261718	2288.696864	20.614515
63.565088	2291.813397	20.619533
63.231315	2297.799972	20.624551
63.458273	2293.956238	20.629568
63.400288	2296.080402	20.634586
63.202376	2292.722792	20.639603
63.437121	2293.614813	20.644621
63.426168	2282.348761	20.649639
63.377906	2292.636245	20.654656
63.506445	2290.373420	20.659674
63.273798	2300.533517	20.664691
63.606658	2305.710969	20.669709
63.450654	2307.220868	20.674727
63.580958	2306.099593	20.679744
63.550311	2320.221690	20.684762
64.015231	2331.991995	20.689779
64.385450	2336.530850	20.694797
64.452569	2343.702284	20.699815
64.878995	2332.716451	20.704832
64.661094	2328.798792	20.709850
65.023196	2342.777667	20.714867
64.857534	2323.304486	20.719885
65.034708	2305.226140	20.724903
65.076222	2291.096312	20.729920
64.836910	2295.771115	20.734938
64.984927	2298.020673	20.739955
64.992058	2294.650634	20.744973
64.871324	2281.511727	20.749991
65.075150	2286.009368	20.755008
64.943044	2278.653397	20.760026
65.141311	2280.763557	20.765043
65.220397	2293.970125	20.770061
65.264183	2312.329397	20.775079
65.452342	2312.266591	20.780096
65.543431	2326.047538	20.785114
65.435390	2325.154808	20.790131
65.546369	2319.611069	20.795149
65.017684	2318.200100	20.800167
65.194337	2310.131723	20.805184
65.447867	2320.405177	20.810202
65.147036	2321.625845	20.815219
65.722318	2344.890655	20.820237
65.774244	2341.694883	20.825255
65.850842	2344.999679	20.830272
66.061619	2344.372349	20.835290
66.180514	2347.186333	20.840307
66.315499	2331.026404	20.845325
66.061883	2340.200498	20.850343
66.372571	2345.274942	20.855360
66.418523	2334.597830	20.860378
66.292970	2334.163275	20.865395
66.128867	2349.211915	20.870413
66.553856	2376.341685	20.875431
66.744483	2371.270165	20.880448
66.670011	2365.302955	20.885466
66.551636	2376.886437	20.890483
66.802845	2375.417445	20.895501
66.920597	2374.557473	20.900519
67.015658	2375.325939	20.905536
66.985695	2373.784128	20.910554
67.173343	2356.056723	20.915571
67.465402	2348.658575	20.920589
67.426783	2355.143601	20.925607
67.697370	2357.385314	20.930624
67.480482	2356.060996	20.935642
67.469784	2363.805887	20.940659
67.628508	2356.514409	20.945677
67.467852	2358.071142	20.950695
67.366081	2347.675500	20.955712
67.644327	2347.534820	20.960730
67.443477	2353.708884	20.965747
67.651621	2360.255095	20.970765
67.845388	2382.224641	20.975783
67.912326	2369.322737	20.980800
68.133176	2374.743510	20.985818
67.706869	2384.186307	20.990835
68.218910	2380.225958	20.995853
67.854636	2388.530044	21.000871
68.288480	2386.669674	21.005888
68.201321	2378.937553	21.010906
68.192291	2379.702355	21.015923
68.583307	2397.897860	21.020941
68.397732	2418.447963	21.025959
68.776801	2399.100008	21.030976
68.610538	2409.467695	21.035994
68.740250	2417.835036	21.041011
68.757123	2419.100644	21.046029
68.518777	2402.907655	21.051047
68.778639	2415.996075	21.056064
69.120855	2407.969574	21.061082
68.899635	2415.750265	21.066099
69.425291	2424.871612	21.071117
69.506862	2427.002848	21.076135
69.186828	2436.639715	21.081152
69.573122	2433.375285	21.086170
69.675028	2431.724674	21.091187
70.121275	2422.526524	21.096205
69.448851	2428.056154	21.101223
69.491921	2424.607711	21.106240
69.827405	2422.012659	21.111258
69.684928	2432.590983	21.116275
70.172622	2423.873155	21.121293
69.820350	2421.298060	21.126311
69.854251	2423.475950	21.131328
70.308129	2416.707481	21.136346
69.923615	2417.194988	21.141363
69.911676	2425.865644	21.146381
70.151876	2431.225959	21.151399
70.402380	2448.003501	21.156416
70.660880	2456.801913	21.161434
70.373104	2453.173310	21.166451
70.928457	2450.376969	21.171469
70.633396	2450.789856	21.176487
70.829171	2441.740756	21.181504
70.892703	2444.176136	21.186522
70.547778	2441.598052	21.191539
71.126755	2444.029943	21.196557
70.985453	2448.055763	21.201575
70.625683	2454.613191	21.206592
70.942538	2445.587187	21.211610
70.733748	2468.555995	21.216627
71.353896	2456.307040	21.221645
71.280490	2469.071468	21.226663
71.290931	2459.732926	21.231680
71.533749	2461.130677	21.236698
71.468635	2460.378670	21.241715
71.775847	2462.467506	21.246733
71.359772	2460.210606	21.251751
71.528934	2479.083968	21.256768
72.038755	2488.997092	21.261786
71.794410	2507.643368	21.266803
72.141640	2500.613960	21.271821
72.086851	2496.937791	21.276839
72.400029	2496.985223	21.281856
72.282799	2496.016840	21.286874
71.902695	2492.996361	21.291891
72.154793	2481.606188	21.296909
71.918993	2495.889505	21.301927
72.247237	2492.506317	21.306944
72.451085	2500.166220	21.311962
72.343758	2511.858011	21.316979
72.582641	2508.726973	21.321997
72.613093	2523.443453	21.327015
72.624707	2522.820684	21.332032
72.847103	2523.364978	21.337050
72.664830	2525.867761	21.342067
72.886021	2537.140738	21.347085
72.919716	2545.355128	21.352103
73.110951	2541.280046	21.357120
73.441275	2543.970549	21.362138
73.194051	2545.034155	21.367155
73.326730	2543.187514	21.372173
73.793082	2541.384153	21.377191
73.504946	2544.333541	21.382208
73.895039	2533.103193	21.387226
73.475943	2536.685207	21.392243
73.774763	2535.913801	21.397261
73.961726	2538.951203	21.402279
73.740414	2561.805690	21.407296
74.111222	2571.209981	21.412314
73.838371	2574.213145	21.417331
73.980061	2576.205340	21.422349
74.111935	2565.721536	21.427367
74.251902	2565.872390	21.432384
74.214525	2570.790857	21.437402
73.930278	2576.752033	21.442419
74.257593	2577.644718	21.447437
74.525486	2579.214507	21.452455
74.278951	2583.047527	21.457472
74.738591	2584.421467	21.462490
74.875488	2595.900926	21.467507
74.582079	2592.209838	21.472525
74.937511	2615.056098	21.477543
75.222798	2621.437320	21.482560
75.353892	2615.317939	21.487578
75.145539	2627.121387	21.492595
75.278778	2608.212199	21.497613
75.560565	2620.852313	21.502631
75.512198	2614.438196	21.507648
75.696838	2612.729803	21.512666
75.538332	2618.330470	21.517683
75.593713	2616.265111	21.522701
75.610579	2612.455032	21.527719
75.531329	2616.264747	21.532736
76.025484	2624.176722	21.537754
76.201179	2638.248084	21.542771
76.563210	2633.293225	21.547789
76.355380	2646.209534	21.552807
76.231812	2643.393469	21.557824
76.355320	2634.776649	21.562842
76.281176	2644.523003	21.567859
76.173186	2650.220053	21.572877
76.640113	2640.243005	21.577895
76.774635	2642.922971	21.582912
77.045586	2631.917347	21.587930
76.800205	2646.715351	21.592947
76.879952	2635.398819	21.597965
77.268682	2632.286693	21.602983
76.996251	2646.093945	21.608000
76.901760	2631.018616	21.613018
77.009951	2631.618792	21.618035
76.902862	2631.180193	21.623053
77.009689	2628.440225	21.628071
76.979559	2649.408230	21.633088
77.180050	2651.669051	21.638106
77.279049	2657.293318	21.643123
77.480371	2652.570511	21.648141
77.567683	2655.549997	21.653159
77.046152	2663.910529	21.658176
77.743969	2666.304512	21.663194
77.736113	2668.152149	21.668211
77.733445	2680.583426	21.673229
78.095695	2688.975476	21.678247
78.111067	2684.885326	21.683264
78.103359	2682.373714	21.688282
78.219476	2681.142361	21.693299
78.205522	2683.643731	21.698317
78.311163	2685.563949	21.703335
77.796668	2688.029930	21.708352
78.684555	2695.958763	21.713370
78.311697	2700.380375	21.718387
78.322767	2698.037696	21.723405
78.897566	2704.933681	21.728423
78.630405	2715.522172	21.733440
78.923290	2727.255465	21.738458
78.843489	2725.221091	21.743475
79.273381	2742.429917	21.748493
79.556139	2733.893020	21.753511
79.464781	2739.509011	21.758528
79.214421	2728.137912	21.763546
79.445581	2733.542345	21.768563
79.185828	2741.491960	21.773581
79.579795	2729.180960	21.778599
79.581711	2732.440702	21.783616
79.915419	2741.472507	21.788634
80.030824	2762.945332	21.793651
79.822760	2748.227224	21.798669
80.150552	2749.051341	21.803687
80.392119	2756.498455	21.808704
80.734519	2737.099055	21.813722
80.934029	2737.036144	21.818739
80.832354	2733.161377	21.823757
81.277862	2718.449856	21.828775
80.906780	2718.581231	21.833792
80.933162	2714.345953	21.838810
80.754940	2716.738259	21.843827
80.877591	2713.877951	21.848845
81.156771	2706.949062	21.853863
80.641605	2703.741026	21.858880
80.836951	2711.260321	21.863898
80.710825	2714.857739	21.868915
81.084912	2725.041072	21.873933
81.250041	2732.233890	21.878951
81.101168	2736.268516	21.883968
81.391525	2736.257519	21.888986
81.394349	2735.278731	21.894003
81.036614	2736.493675	21.899021
81.279818	2751.956281	21.904039
81.494605	2756.732355	21.909056
81.442917	2750.261254	21.914074
81.597403	2768.173069	21.919091
81.499235	2772.975668	21.924109
81.924279	2791.499858	21.929127
82.059302	2805.192283	21.934144
82.119417	2800.092390	21.939162
82.052377	2805.749660	21.944179
82.238807	2809.608035	21.949197
82.084501	2789.119834	21.954215
82.287108	2805.038394	21.959232
82.351778	2815.295752	21.964250
82.573805	2829.139956	21.969267
82.839038	2829.673247	21.974285
82.895208	2827.688828	21.979303
82.745293	2823.760201	21.984320
82.912191	2826.048251	21.989338
82.998429	2833.521858	21.994355
83.063772	2828.769109	21.999373
83.209031	2826.955394	22.004391
82.865715	2829.849389	22.009408
83.115293	2848.379415	22.014426
82.986133	2841.942336	22.019443
83.328226	2859.586651	22.024461
83.703778	2855.794403	22.029479
83.551867	2849.165813	22.034496
83.630101	2849.685912	22.039514
84.110910	2865.135745	22.044531
83.898917	2875.761290	22.049549
84.457249	2868.203151	22.054567
84.218110	2863.988482	22.059584
84.267896	2867.541512	22.064602
84.336447	2871.920937	22.069619
84.283456	2869.012856	22.074637
84.485333	2871.095140	22.079655
84.427231	2871.159442	22.084672
84.620484	2867.863046	22.089690
84.389300	2880.851516	22.094707
84.777410	2898.422132	22.099725
85.160911	2892.768394	22.104743
84.849631	2898.634162	22.109760
84.933893	2887.478112	22.114778
84.931428	2901.192948	22.119795
84.980861	2903.055949	22.124813
85.232710	2906.383085	22.129831
86.242044	2902.092013	22.134848
86.339001	2907.637971	22.139866
86.022771	2892.062829	22.144883
86.109515	2877.464378	22.149901
86.140565	2869.973293	22.154919
86.194172	2865.512224	22.159936
85.896036	2871.497066	22.164954
86.134342	2866.725564	22.169971
85.845447	2874.290708	22.174989
86.001345	2891.023738	22.180007
86.123908	2914.696690	22.185024
86.395242	2908.857945	22.190042
86.509348	2911.635817	22.195059
86.565557	2914.681515	22.200077
86.645641	2904.769012	22.205095
86.498488	2907.144796	22.210112
86.626978	2919.294364	22.215130
86.700310	2922.156532	22.220147
86.630395	2928.986722	22.225165
86.681755	2925.069689	22.230183
87.021197	2940.064234	22.235200
87.175442	2954.534691	22.240218
87.226756	2957.046579	22.245235
87.315849	2970.055818	22.250253
87.463641	2955.505866	22.255271
87.703219	2950.400675	22.260288
87.530659	2952.472014	22.265306
87.686803	2951.027340	22.270323
87.523767	2955.204909	22.275341
88.379858	2967.185856	22.280359
88.011627	2981.736378	22.285376
87.860902	2980.617992	22.290394
88.239592	2975.266978	22.295411
88.177879	2978.892788	22.300429
88.461360	2978.505381	22.305447
88.375067	2969.444319	22.310464
88.563685	2973.177575	22.315482
88.743248	2968.053163	22.320499
88.216081	2975.677020	22.325517
88.877646	2982.505645	22.330535
88.948642	3007.988386	22.335552
89.249021	3012.849605	22.340570
89.448630	3009.472603	22.345587
89.461018	3010.859470	22.350605
89.223315	3003.183211	22.355623
89.098506	3007.319438	22.360640
89.123783	3009.849416	22.365658
89.376042	2996.028991	22.370675
89.382564	3002.486751	22.375693
89.996856	3008.756287	22.380711
90.057465	3022.310419	22.385728
89.804618	3018.179860	22.390746
90.064305	3027.135091	22.395763
89.851607	3032.773995	22.400781
89.713330	3021.061727	22.405799
89.679312	3024.703048	22.410816
89.707511	3040.614059	22.415834
90.183701	3046.554474	22.420851
90.406358	3057.551613	22.425869
90.689169	3046.101228	22.430887
90.837481	3059.707040	22.435904
90.395028	3059.814384	22.440922
90.970309	3066.045510	22.445939
91.055017	3078.706756	22.450957
91.104962	3082.340909	22.455975
91.547223	3072.272782	22.460992
91.422967	3070.480348	22.466010
92.041703	3068.121054	22.471027
91.655956	3077.394776	22.476045
91.723471	3062.359970	22.481063
91.679016	3064.959353	22.486080
91.664520	3074.322902	22.491098
91.615696	3063.187537	22.496115
91.358224	3076.873410	22.501133
91.770508	3066.113015	22.506151
91.683070	3089.949674	22.511168
92.083004	3110.304730	22.516186
92.101172	3103.252659	22.521203
92.139134	3107.552168	22.526221
92.009893	3106.633762	22.531239
92.090127	3117.486372	22.536256
92.576020	3124.954313	22.541274
92.403698	3127.612237	22.546291
92.219497	3135.546812	22.551309
92.660387	3150.141340	22.556327
93.196992	3157.102502	22.561344
92.970248	3155.395890	22.566362
93.390445	3151.096598	22.571379
93.176871	3159.646656	22.576397
93.433072	3155.127223	22.581415
93.395409	3148.389469	22.586432
93.378973	3160.056493	22.591450
93.709796	3172.866906	22.596467
93.772385	3177.061973	22.601485
93.880986	3171.015774	22.606503
94.226929	3175.229764	22.611520
94.246694	3176.888256	22.616538
94.446821	3168.919883	22.621555
94.413975	3175.236979	22.626573
94.474288	3173.023490	22.631591
94.598053	3166.264171	22.636608
94.095283	3176.012005	22.641626
94.885766	3175.503412	22.646643
94.675829	3178.857705	22.651661
94.753501	3171.968995	22.656679
94.717731	3163.316392	22.661696
94.451931	3175.937608	22.666714
94.692430	3185.353967	22.671731
94.861847	3192.112834	22.676749
95.061085	3202.030107	22.681767
95.218974	3209.720005	22.686784
95.179464	3221.044830	22.691802
95.424008	3212.248242	22.696819
95.599742	3228.201994	22.701837
95.663137	3230.542248	22.706855
95.766973	3223.764937	22.711872
95.379309	3228.299378	22.716890
95.972977	3239.772338	22.721907
95.901669	3249.345378	22.726925
95.815710	3254.401222	22.731943
95.900649	3250.813592	22.736960
95.975258	3249.203233	22.741978
96.289228	3255.433918	22.746995
96.350274	3269.284646	22.752013
96.476374	3281.888037	22.757031
96.924125	3271.475179	22.762048
96.840807	3278.570726	22.767066
97.179358	3270.777850	22.772083
97.026510	3273.817614	22.777101
97.211817	3279.404224	22.782119
97.385601	3293.861533	22.787136
97.343895	3299.608891	22.792154
97.678099	3302.856363	22.797171
98.065447	3304.458851	22.802189
98.069112	3292.028440	22.807207
98.573086	3299.480881	22.812224
98.328687	3292.707542	22.817242
98.241398	3278.467391	22.822259
98.470662	3254.982548	22.827277
98.143099	3251.770953	22.832295
98.432981	3255.387939	22.837312
98.473037	3268.920092	22.842330
98.722343	3282.176345	22.847347
98.745011	3285.797730	22.852365
98.761283	3274.620748	22.857383
98.878304	3281.264298	22.862400
98.381682	3288.038388	22.867418
98.770365	3284.120640	22.872435
98.767801	3282.719878	22.877453
98.579962	3293.294473	22.882471
99.032865	3301.480936	22.887488
99.020145	3307.834129	22.892506
99.117229	3308.747189	22.897523
99.278768	3323.315210	22.902541
99.429290	3344.716898	22.907559
99.781703	3345.189740	22.912576
99.825902	3344.494231	22.917594
99.992653	3347.350883	22.922611
99.970393	3340.170740	22.927629
100.034669	3342.769131	22.932647
100.320620	3354.891053	22.937664
99.954611	3372.076985	22.942682
100.237935	3355.420417	22.947699
100.300029	3350.829855	22.952717
100.528872	3368.379293	22.957735
101.073689	3368.025858	22.962752
100.997208	3380.663200	22.967770
101.565669	3383.290487	22.972787
101.424044	3368.364747	22.977805
101.396845	3366.760175	22.982823
101.161008	3369.906191	22.987840
100.940596	3363.994206	22.992858
100.889623	3384.098939	22.997875
101.286695	3383.381732	23.002893
101.055404	3399.360400	23.007911
101.173486	3391.995626	23.012928
101.483473	3423.677716	23.017946
101.623171	3416.638097	23.022963
101.882451	3421.469230	23.027981
101.909853	3421.416649	23.032999
102.285896	3430.621390	23.038016
102.325475	3452.511244	23.043034
102.505595	3444.656666	23.048051
102.588820	3448.760996	23.053069
102.615804	3452.841550	23.058087
102.554701	3442.494554	23.063104
102.491752	3450.211221	23.068122
102.440617	3444.480288	23.073139
103.045135	3462.772084	23.078157
102.832383	3474.510367	23.083175
103.052268	3468.744089	23.088192
103.067439	3471.640379	23.093210
103.065687	3494.453263	23.098227
103.602557	3499.475165	23.103245
103.987400	3497.578082	23.108263
104.133535	3488.739726	23.113280
104.145437	3488.638131	23.118298
104.327855	3488.118989	23.123315
104.708088	3478.578175	23.128333
104.272258	3482.271041	23.133351
104.423648	3480.101120	23.138368
104.468587	3487.193284	23.143386
104.238789	3486.589897	23.148403
104.623416	3486.294427	23.153421
104.515946	3494.039340	23.158439
104.881262	3501.694319	23.163456
104.937995	3522.403088	23.168474
105.002257	3514.529431	23.173491
105.306491	3509.459831	23.178509
105.214874	3515.130082	23.183527
105.323015	3505.338150	23.188544
105.482387	3513.657483	23.193562
105.556527	3538.207896	23.198579
105.561642	3541.711376	23.203597
105.768488	3541.075990	23.208615
106.411659	3533.580679	23.213632
105.913173	3533.921693	23.218650
106.139346	3529.447666	23.223667
106.690707	3528.431334	23.228685
106.351306	3536.769319	23.233703
106.287632	3523.000240	23.238720
106.432070	3527.232665	23.243738
106.339137	3534.895667	23.248755
106.812842	3544.357174	23.253773
106.852943	3556.871457	23.258791
106.797866	3559.019131	23.263808
107.113856	3551.090473	23.268826
106.984870	3549.131441	23.273843
107.594805	3568.784286	23.278861
107.357297	3588.761445	23.283879
107.548991	3583.734041	23.288896
107.733971	3591.742095	23.293914
107.771294	3578.886993	23.298931
108.024410	3576.214024	23.303949
107.769236	3579.064850	23.308967
108.079441	3579.586407	23.313984
108.093490	3583.547084	23.319002
108.104960	3581.873896	23.324019
108.228171	3578.196008	23.329037
108.442180	3602.334824	23.334055
108.432579	3596.964298	23.339072
108.472260	3612.024384	23.344090
108.316176	3596.097262	23.349107
108.477224	3595.519836	23.354125
108.631681	3622.424846	23.359143
109.039324	3617.488125	23.364160
109.028787	3634.209697	23.369178
108.771116	3636.388497	23.374195
108.915850	3636.040540	23.379213
109.218412	3656.733669	23.384231
109.188120	3653.769327	23.389248
109.478522	3655.037869	23.394266
109.710897	3654.215187	23.399283
110.427284	3661.127579	23.404301
110.747849	3668.224676	23.409319
111.108228	3651.893645	23.414336
111.207343	3639.879472	23.419354
111.130812	3628.412448	23.424371
111.422059	3628.722965	23.429389
111.367332	3624.295722	23.434407
111.414636	3603.316430	23.439424
111.184702	3602.904006	23.444442
111.095261	3589.051723	23.449459
111.073810	3600.045098	23.454477
111.239785	3612.363821	23.459495
111.260412	3613.991508	23.464512
111.269175	3619.920016	23.469530
111.071093	3626.589799	23.474547
111.386950	3624.918276	23.479565
111.307352	3649.904905	23.484583
111.334386	3660.591488	23.489600
111.571135	3647.101793	23.494618
111.512520	3667.331385	23.499635
112.018963	3683.827816	23.504653
111.797130	3681.637650	23.509671
111.969062	3684.295081	23.514688
112.189631	3708.045571	23.519706
112.108845	3710.975085	23.524723
112.612203	3712.111197	23.529741
112.408459	3733.720390	23.534759
112.546162	3742.758006	23.539776
112.630106	3745.461483	23.544794
112.930247	3748.841848	23.549811
113.130365	3773.362366	23.554829
112.634683	3799.003433	23.559847
113.105531	3793.101469	23.564864
113.568730	3805.788168	23.569882
113.632486	3811.409230	23.574899
114.001620	3796.453797	23.579917
113.882784	3810.596550	23.584935
114.315981	3800.676701	23.589952
114.857911	3794.908663	23.594970
114.655781	3793.075074	23.599987
114.988336	3785.833732	23.605005
114.882664	3786.391341	23.610023
115.097409	3779.212777	23.615040
115.177350	3785.757551	23.620058
114.854628	3779.294585	23.625075
115.314682	3779.578786	23.630093
115.364848	3787.661582	23.635111
115.619482	3805.925774	23.640128
115.564416	3803.917092	23.645146
115.481279	3806.908825	23.650163
115.551977	3800.422179	23.655181
115.482783	3815.368168	23.660199
115.675979	3823.664361	23.665216
115.828692	3816.961789	23.670234
115.451201	3818.415515	23.675251
115.709898	3828.932828	23.680269
116.432085	3841.411797	23.685287
115.860961	3844.253853	23.690304
116.364208	3835.714567	23.695322
116.321687	3864.954569	23.700339
116.609851	3867.725506	23.705357
116.396839	3881.103943	23.710375
116.876642	3880.098628	23.715392
117.119049	3875.542291	23.720410
116.598298	3888.256607	23.725427
117.186732	3897.919064	23.730445
117.440605	3903.345353	23.735463
117.655070	3898.823548	23.740480
117.597781	3895.092339	23.745498
117.396917	3895.789307	23.750515
117.999111	3925.641018	23.755533
117.743267	3918.350777	23.760551
117.552323	3934.234347	23.765568
117.876688	3935.912273	23.770586
117.848880	3957.173797	23.775603
118.483903	3954.143553	23.780621
118.370548	3958.069078	23.785639
118.649072	3970.360825	23.790656
118.944699	3981.869022	23.795674
119.006099	3988.518917	23.800691
118.894914	3984.701708	23.805709
118.888169	3989.317521	23.810727
118.922846	3993.514666	23.815744
119.639446	3996.349086	23.820762
119.202381	4010.122937	23.825779
119.287630	3995.904799	23.830797
119.841567	4013.956780	23.835815
120.121472	4019.070136	23.840832
120.518581	4020.278162	23.845850
120.677047	4029.675912	23.850867
120.603139	4022.496115	23.855885
120.695870	4031.933470	23.860903
120.706171	4022.490070	23.865920
120.628188	4022.121819	23.870938
120.533376	4032.618942	23.875955
120.896115	4019.105744	23.880973
120.846973	4022.115524	23.885991
121.172588	4035.587379	23.891008
121.506003	4054.737303	23.896026
121.098258	4046.662623	23.901043
121.114926	4054.927478	23.906061
121.377294	4059.580342	23.911079
121.858710	4083.508390	23.916096
121.877497	4075.520699	23.921114
121.596519	4090.398794	23.926131
121.963102	4082.834750	23.931149
122.080864	4089.017877	23.936167
121.978543	4107.392984	23.941184
122.008061	4104.458831	23.946202
122.381215	4101.888385	23.951219
122.897442	4120.472333	23.956237
122.995064	4123.136607	23.961255
123.393137	4129.891173	23.966272
123.168368	4125.762763	23.971290
123.507710	4129.576910	23.976307
123.847820	4109.962785	23.981325
124.156870	4112.915756	23.986343
123.721332	4124.677167	23.991360
124.037195	4115.716706	23.996378
123.830532	4122.006213	24.001395
123.967660	4113.163480	24.006413
124.085152	4113.714933	24.011431
124.183602	4117.351551	24.016448
124.514182	4122.675081	24.021466
124.367572	4141.671746	24.026483
124.625678	4146.109977	24.031501
124.738205	4132.235254	24.036519
124.893635	4137.651513	24.041536
124.971256	4140.403351	24.046554
124.960133	4131.611091	24.051571
125.272851	4135.054426	24.056589
125.208706	4146.797399	24.061607
125.078360	4171.370002	24.066624
125.295354	4171.936907	24.071642
125.207704	4178.896960	24.076659
125.421031	4179.294384	24.081677
125.978544	4188.778268	24.086695
125.730120	4195.038482	24.091712
125.992779	4191.944523	24.096730
125.913099	4205.594920	24.101747
126.072423	4224.833666	24.106765
126.512641	4226.273968	24.111783
125.967004	4228.299636	24.116800
126.712976	4230.893410	24.121818
127.001843	4246.940938	24.126835
127.036544	4254.921409	24.131853
127.242705	4258.546168	24.136871
127.219709	4256.928210	24.141888
126.982387	4267.677398	24.146906
127.280581	4275.318656	24.151923
127.621690	4282.194912	24.156941
127.736274	4283.656742	24.161959
127.617125	4300.167830	24.166976
127.859966	4291.479585	24.171994
128.174014	4302.458570	24.177011
128.449268	4297.464770	24.182029
128.771686	4301.490823	24.187047
128.821301	4325.683126	24.192064
129.140544	4327.522976	24.197082
129.160762	4324.047769	24.202099
129.327274	4315.542211	24.207117
130.120602	4319.570774	24.212135
129.652259	4320.891517	24.217152
130.166471	4310.753224	24.222170
130.054362	4317.232708	24.227187
129.608190	4325.358821	24.232205
130.088257	4326.874836	24.237223
129.926197	4319.967355	24.242240
129.911713	4314.041846	24.247258
129.884946	4327.361148	24.252275
129.893017	4330.204044	24.257293
130.396729	4337.884604	24.262311
130.124994	4357.186869	24.267328
130.300008	4350.752840	24.272346
130.435324	4383.788268	24.277363
130.500895	4383.170683	24.282381
130.728185	4391.370597	24.287399
130.739865	4401.468852	24.292416
130.718364	4415.399206	24.297434
130.832614	4423.732784	24.302451
130.953500	4443.960889	24.307469
131.286417	4442.583333	24.312487
131.320706	4469.641169	24.317504
131.695078	4467.802400	24.322522
131.684219	4470.379535	24.327539
132.105872	4486.611681	24.332557
133.013220	4486.182576	24.337575
133.135033	4492.920348	24.342592
133.132333	4486.953060	24.347610
133.107015	4487.578128	24.352627
133.214207	4494.202955	24.357645
133.611553	4481.738434	24.362663
133.480918	4482.562807	24.367680
133.851978	4474.934840	24.372698
133.613797	4479.335481	24.377715
133.625651	4475.493095	24.382733
133.747257	4480.955617	24.387751
134.094479	4488.451075	24.392768
134.195413	4478.471915	24.397786
133.711583	4480.017686	24.402803
133.803852	4482.213585	24.407821
134.236439	4492.065958	24.412839
134.122191	4518.321597	24.417856
134.771966	4511.487377	24.422874
134.552584	4515.715226	24.427891
134.178044	4520.584110	24.432909
134.321869	4531.827228	24.437927
134.466914	4549.492250	24.442944
134.584748	4567.987437	24.447962
134.816688	4586.646874	24.452979
134.803859	4601.433109	24.457997
135.385083	4599.216813	24.463015
135.704907	4617.056195	24.468032
135.912049	4620.801752	24.473050
136.302144	4621.877906	24.478067
136.391320	4630.034621	24.483085
136.758631	4620.144830	24.488103
136.748386	4624.335788	24.493120
136.612187	4625.952090	24.498138
136.749563	4637.745210	24.503155
137.097411	4647.165588	24.508173
137.335899	4650.500430	24.513191
137.122117	4650.691651	24.518208
137.432075	4645.309300	24.523226
137.716861	4655.163364	24.528243
137.775336	4672.937326	24.533261
138.030384	4670.270942	24.538279
137.725790	4681.125237	24.543296
137.811154	4673.427444	24.548314
138.192612	4677.099325	24.553331
138.348123	4710.088009	24.558349
138.393046	4707.993784	24.563367
138.511087	4714.092068	24.568384
138.876286	4710.588513	24.573402
139.000775	4713.598477	24.578419
138.783982	4727.255056	24.583437
139.197399	4741.360706	24.588455
139.075408	4733.217580	24.593472
139.283420	4737.878056	24.598490
139.640832	4753.811623	24.603507
139.528664	4777.230505	24.608525
139.554243	4770.725320	24.613543
139.973481	4775.694633	24.618560
140.247387	4793.770565	24.623578
140.382404	4793.234803	24.628595
140.509353	4801.425921	24.633613
140.883798	4790.920225	24.638631
140.907701	4793.953519	24.643648
140.694078	4785.625096	24.648666
140.765200	4804.596826	24.653683
140.684244	4816.672636	24.658701
141.063159	4814.663771	24.663719
141.419388	4825.397554	24.668736
141.176699	4831.521628	24.673754
141.553688	4836.250677	24.678771
141.574463	4848.796359	24.683789
141.644955	4842.319946	24.688807
141.850565	4859.850497	24.693824
141.983007	4871.172913	24.698842
142.385494	4863.675798	24.703859
142.166301	4876.508814	24.708877
142.799777	4880.739548	24.713895
142.840133	4890.656200	24.718912
142.743913	4896.588759	24.723930
143.132436	4894.345993	24.728947
142.927726	4890.323916	24.733965
142.930855	4907.337141	24.738983
143.337416	4914.667473	24.744000
143.536349	4921.958095	24.749018
143.725195	4918.763976	24.754035
143.683798	4938.978590	24.759053
144.318523	4939.098905	24.764071
144.287436	4942.419294	24.769088
144.317333	4941.778445	24.774106
144.853739	4941.031459	24.779123
144.832717	4942.463392	24.784141
144.897383	4965.493460	24.789159
145.105211	4974.898588	24.794176
145.258859	4965.229337	24.799194
145.754439	4962.399919	24.804211
145.627942	4961.076183	24.809229
145.806172	4962.517717	24.814247
145.768582	4959.147600	24.819264
145.869587	4966.570184	24.824282
146.446861	4965.944014	24.829299
146.559315	4982.424246	24.834317
146.373567	4978.934498	24.839335
146.727640	4983.408299	24.844352
146.680994	4983.578205	24.849370
146.841762	4979.030314	24.854387
146.432052	4985.606892	24.859405
146.968746	5000.976390	24.864423
147.040057	5009.168542	24.869440
147.461351	5012.961887	24.874458
147.462907	5009.451812	24.879475
147.422620	5018.440440	24.884493
147.680186	5031.705484	24.889511
147.551165	5035.794512	24.894528
147.724291	5051.972637	24.899546
148.115838	5059.163379	24.904563
148.204601	5066.365175	24.909581
148.394501	5066.672786	24.914599
148.604162	5083.170530	24.919616
148.631802	5082.451300	24.924634
148.958452	5092.215644	24.929651
149.019865	5095.999965	24.934669
148.876391	5115.941093	24.939687
149.029522	5121.376976	24.944704
149.406557	5126.700658	24.949722
149.797381	5137.538400	24.954739
149.618599	5154.664638	24.959757
149.851808	5147.575322	24.964775
150.048763	5158.193511	24.969792
150.011749	5178.764049	24.974810
150.569892	5187.423155	24.979827
150.489243	5187.255338	24.984845
150.713991	5183.760319	24.989863
150.663821	5198.813160	24.994880
150.497283	5203.749469	24.999898
151.217169	5207.861674	25.004915
150.930648	5236.155476	25.009933
151.245413	5242.299421	25.014951
151.951842	5232.446922	25.019968
152.023935	5245.821545	25.024986
152.498521	5241.426078	25.030003
152.406100	5238.412637	25.035021
152.461381	5236.218982	25.040039
152.608927	5235.805560	25.045056
152.498256	5240.082576	25.050074
152.526247	5246.787747	25.055091
152.521008	5257.072836	25.060109
152.838099	5266.697908	25.065127
153.025113	5279.339315	25.070144
152.866791	5282.322490	25.075162
153.293115	5280.744762	25.080179
153.555281	5279.737530	25.085197
153.794439	5288.458851	25.090215
154.027421	5303.991052	25.095232
153.941479	5300.068942	25.100250
154.636625	5301.283346	25.105267
154.400532	5313.293037	25.110285
154.577084	5305.838558	25.115303
154.911062	5314.062673	25.120320
154.757224	5332.837936	25.125338
154.968747	5331.572895	25.130355
154.935305	5319.369861	25.135373
154.976339	5339.719421	25.140391
155.464505	5354.529504	25.145408
155.320530	5362.814508	25.150426
155.973652	5364.081143	25.155443
155.706958	5377.591789	25.160461
156.044420	5387.540776	25.165479
156.201829	5394.139575	25.170496
156.217537	5405.775799	25.175514
156.642048	5407.594449	25.180531
156.916770	5400.296954	25.185549
157.137398	5412.285590	25.190567
157.511505	5398.211385	25.195584
157.354255	5410.381765	25.200602
157.987940	5403.886478	25.205619
157.558862	5407.950765	25.210637
157.934618	5423.831981	25.215655
157.943266	5439.801829	25.220672
157.979674	5454.116897	25.225690
158.010353	5435.116490	25.230707
158.040456	5448.167080	25.235725
158.814506	5452.983485	25.240743
159.253888	5459.642033	25.245760
158.903516	5465.669171	25.250778
159.444612	5448.978808	25.255795
159.376453	5455.968888	25.260813
159.262553	5453.359007	25.265831
159.482332	5457.411772	25.270848
159.506323	5482.905936	25.275866
159.821051	5480.223649	25.280883
160.174713	5482.182379	25.285901
160.090576	5494.927433	25.290919
160.352809	5493.835126	25.295936
160.320813	5505.846677	25.300954
160.468230	5511.047783	25.305971
160.860485	5513.712831	25.310989
160.641951	5511.513587	25.316007
160.915391	5530.348029	25.321024
160.738196	5544.416941	25.326042
161.213549	5543.352022	25.331059
161.121884	5568.457901	25.336077
161.176446	5585.492502	25.341095
161.694213	5594.297897	25.346112
161.511020	5617.135202	25.351130
161.755852	5611.868023	25.356147
161.911155	5609.259703	25.361165
161.964632	5634.302722	25.366183
162.595319	5631.421331	25.371200
162.328433	5651.254381	25.376218
162.773846	5656.743350	25.381235
163.117023	5665.053939	25.386253
163.551032	5672.236374	25.391271
163.673721	5662.729312	25.396288
163.927997	5664.156772	25.401306
163.740433	5650.023948	25.406323
164.030247	5660.602723	25.411341
164.635513	5668.888908	25.416359
164.794255	5654.391334	25.421376
165.029872	5658.002891	25.426394
165.199219	5664.664409	25.431411
164.922400	5660.087038	25.436429
165.128440	5649.014419	25.441447
165.192601	5648.962845	25.446464
165.116648	5662.986390	25.451482
165.365270	5662.484199	25.456499
165.444078	5679.057351	25.461517
165.483840	5684.158176	25.466535
165.691546	5679.788574	25.471552
165.632917	5703.517363	25.476570
165.939433	5713.294874	25.481587
166.238193	5733.552353	25.486605
166.325238	5753.872799	25.491623
166.409551	5750.652078	25.496640
166.762768	5760.625869	25.501658
166.966119	5772.084487	25.506675
167.217307	5768.336116	25.511693
167.458694	5780.710639	25.516711
167.403484	5782.711373	25.521728
167.437944	5800.935926	25.526746
167.785623	5795.123267	25.531763
168.050178	5818.213701	25.536781
168.448474	5827.344528	25.541799
168.744431	5819.084130	25.546816
168.644420	5822.147549	25.551834
169.127592	5812.770230	25.556851
169.402259	5815.452005	25.561869
169.255325	5826.929167	25.566887
169.992792	5837.619949	25.571904
169.770148	5846.401351	25.576922
170.263519	5837.802766	25.581939
170.271381	5840.011229	25.586957
170.037675	5845.824717	25.591975
170.006106	5844.458837	25.596992
169.982943	5851.993711	25.602010
170.171131	5871.797127	25.607027
170.857873	5867.077412	25.612045
170.604997	5868.208318	25.617063
171.282460	5885.506125	25.622080
170.929694	5904.983155	25.627098
171.037572	5900.107859	25.632115
171.220230	5907.928486	25.637133
171.275454	5932.557849	25.642151
172.013393	5939.365334	25.647168
171.911224	5951.424260	25.652186
172.332214	5966.912272	25.657203
172.443804	5967.231662	25.662221
172.661821	5968.571426	25.667239
172.484547	5961.741334	25.672256
172.753786	5982.200107	25.677274
173.168834	5987.604040	25.682292
173.231766	5989.420686	25.687309
173.291570	5991.520572	25.692327
173.401223	6004.639203	25.697344
173.155124	6015.859615	25.702362
173.758212	6019.860611	25.707380
173.791560	6038.182490	25.712397
173.998086	6048.345298	25.717415
174.209155	6060.216306	25.722432
174.503646	6060.238502	25.727450
174.818624	6076.629327	25.732468
175.265968	6063.654030	25.737485
175.198205	6077.671473	25.742503
175.565905	6070.503998	25.747520
175.623956	6066.670127	25.752538
175.961643	6073.795030	25.757556
176.270354	6083.777170	25.762573
176.048790	6084.228001	25.767591
176.015791	6081.845631	25.772608
176.391324	6086.358340	25.777626
175.921668	6095.193295	25.782644
176.520613	6108.031919	25.787661
176.541931	6116.581789	25.792679
176.811982	6124.684985	25.797696
177.071356	6140.692871	25.802714
176.943838	6145.969937	25.807732
177.523790	6154.500764	25.812749
177.413906	6176.970015	25.817767
177.484111	6179.541518	25.822784
177.801889	6201.882649	25.827802
177.989825	6210.309748	25.832820
178.118397	6213.222854	25.837837
178.171200	6237.708189	25.842855
178.492001	6239.878388	25.847872
179.075295	6252.899277	25.852890
179.034320	6272.782804	25.857908
179.323186	6257.795374	25.862925
179.682048	6271.032921	25.867943
180.233811	6280.604093	25.872960
180.271585	6298.585326	25.877978
180.338658	6287.768333	25.882996
180.630507	6290.855300	25.888013
180.450603	6298.814783	25.893031
180.592163	6306.554195	25.898048
180.701744	6318.199604	25.903066
180.582952	6320.116407	25.908084
181.117792	6334.012457	25.913101
180.893677	6348.182770	25.918119
181.079817	6351.699102	25.923136
181.651009	6359.840866	25.928154
181.849998	6372.530006	25.933172
182.147315	6383.564020	25.938189
181.815554	6397.593868	25.943207
182.138448	6395.650376	25.948224
182.763102	6408.711026	25.953242
182.578095	6433.627371	25.958260
183.203753	6432.758471	25.963277
183.099909	6443.844638	25.968295
183.089782	6465.672501	25.973312
183.294906	6466.522220	25.978330
183.738229	6480.040533	25.983348
184.478148	6487.752832	25.988365
184.365943	6493.049535	25.993383
184.489029	6495.691895	25.998400
184.457346	6487.493950	26.003418
184.360318	6499.706806	26.008436
184.972148	6506.117189	26.013453
184.788745	6524.145463	26.018471
184.923398	6516.262604	26.023488
185.132750	6532.030288	26.028506
185.141949	6547.170300	26.033524
185.545186	6546.650806	26.038541
185.692785	6571.023338	26.043559
185.431217	6583.380005	26.048576
186.128424	6586.448881	26.053594
186.047765	6602.816634	26.058612
186.731972	6616.676441	26.063629
186.846725	6623.992006	26.068647
186.925786	6630.972458	26.073664
187.212089	6631.978886	26.078682
186.896961	6630.656641	26.083700
187.861436	6638.643786	26.088717
187.752119	6655.471539	26.093735
187.917262	6647.537111	26.098752
188.078112	6664.246203	26.103770
188.179000	6673.795246	26.108788
188.622675	6672.162541	26.113805
188.730519	6679.764371	26.118823
188.911429	6698.220149	26.123840
189.612967	6712.889157	26.128858
189.895990	6723.965152	26.133876
189.863831	6717.441529	26.138893
189.906056	6719.774387	26.143911
189.828337	6709.407890	26.148928
190.073643	6729.898370	26.153946
189.715628	6740.722742	26.158964
190.355030	6740.074438	26.163981
190.406347	6752.180284	26.168999
190.825206	6760.471076	26.174016
191.252311	6757.541615	26.179034
191.181189	6777.911965	26.184052
191.474511	6782.933841	26.189069
191.792589	6789.907948	26.194087
191.905499	6793.338034	26.199104
192.384721	6803.096354	26.204122
192.032064	6814.706673	26.209140
192.460598	6829.346081	26.214157
192.508339	6832.868850	26.219175
192.549256	6847.686519	26.224192
192.708077	6854.112042	26.229210
192.839719	6860.983887	26.234228
193.270099	6871.240190	26.239245
193.416376	6880.760595	26.244263
193.455062	6892.592985	26.249280
193.737155	6907.315730	26.254298
193.749283	6911.972996	26.259316
193.923147	6936.977328	26.264333
194.250840	6933.844527	26.269351
194.129880	6960.989413	26.274368
195.145736	6965.339871	26.279386
195.095084	6973.786325	26.284404
195.332171	6980.965281	26.289421
195.540814	6989.555556	26.294439
195.444638	6999.194851	26.299456
196.131642	7006.968134	26.304474
195.910501	7030.922670	26.309492
196.685896	7024.747486	26.314509
196.712819	7036.900898	26.319527
196.867524	7028.566338	26.324544
197.165604	7046.761378	26.329562
197.218627	7058.195370	26.334580
197.555920	7060.258213	26.339597
197.443170	7060.002743	26.344615
197.361797	7068.533869	26.349632
198.100096	7078.158194	26.354650
198.282418	7086.853682	26.359668
198.383868	7082.833612	26.364685
198.455355	7102.888624	26.369703
198.415291	7112.476975	26.374720
198.691121	7117.608173	26.379738
198.700721	7146.782677	26.384756
198.914739	7152.962927	26.389773
199.132356	7160.055397	26.394791
199.101835	7178.733332	26.399808
199.571815	7179.295177	26.404826
199.294337	7201.085536	26.409844
199.970065	7212.603409	26.414861
200.158604	7215.701329	26.419879
199.601361	7236.210874	26.424896
200.299497	7243.694177	26.429914
200.441567	7267.873379	26.434932
200.768330	7288.447213	26.439949
201.046553	7289.003730	26.444967
201.015407	7318.176619	26.449984
201.690600	7325.423537	26.455002
201.604071	7331.580269	26.460020
201.838123	7353.238274	26.465037
202.239933	7363.537425	26.470055
202.369195	7366.073374	26.475072
203.077110	7371.167916	26.480090
203.450864	7382.609794	26.485108
203.850627	7375.330110	26.490125
204.333212	7374.956577	26.495143
204.374134	7386.906320	26.500160
204.240021	7374.140228	26.505178
204.329212	7378.513965	26.510196
204.350060	7376.007513	26.515213
204.724651	7390.958795	26.520231
204.476865	7400.847063	26.525248
205.067777	7410.743254	26.530266
205.010292	7422.219397	26.535284
205.159878	7426.424072	26.540301
205.214910	7438.320330	26.545319
205.287654	7463.795863	26.550336
205.662223	7468.281568	26.555354
205.611372	7486.255170	26.560372
205.697133	7499.966548	26.565389
206.106671	7523.076486	26.570407
205.974785	7542.257551	26.575424
206.146940	7548.231431	26.580442
206.524761	7576.435414	26.585460
206.572013	7590.891222	26.590477
207.007857	7605.972782	26.595495
207.019266	7631.771401	26.600512
207.598781	7643.036913	26.605530
207.882521	7654.984544	26.610548
208.385378	7673.243348	26.615565
208.934222	7689.931950	26.620583
208.518168	7700.476723	26.625600
209.309439	7713.939396	26.630618
209.238489	7721.626404	26.635636
209.235243	7715.845825	26.640653
209.678078	7733.393949	26.645671
209.852294	7747.708417	26.650688
210.319708	7743.930944	26.655706
210.516585	7764.013334	26.660724
210.615696	7772.140113	26.665741
211.046773	7771.546674	26.670759
211.028029	7771.742716	26.675776
211.404001	7778.259544	26.680794
211.309182	7792.831949	26.685812
211.695251	7794.554457	26.690829
212.234886	7795.616771	26.695847
212.139096	7812.614433	26.700864
212.540117	7816.190893	26.705882
212.563026	7834.114897	26.710900
212.559301	7827.785385	26.715917
212.909599	7836.607906	26.720935
212.876494	7852.198014	26.725952
213.179620	7856.746830	26.730970
213.229530	7873.544057	26.735988
213.464629	7894.278750	26.741005
213.572125	7897.661926	26.746023
213.803783	7913.744720	26.751040
213.748511	7918.999412	26.756058
214.379538	7944.552028	26.761076
214.159367	7953.951687	26.766093
214.471961	7964.528253	26.771111
214.776440	7978.171614	26.776128
215.080374	7981.502660	26.781146
215.199973	8004.740761	26.786164
215.216783	8023.313418	26.791181
215.793086	8033.443979	26.796199
215.634114	8049.733228	26.801216
216.145965	8070.315307	26.806234
216.201990	8081.667629	26.811252
216.090572	8090.194818	26.816269
217.119916	8099.461358	26.821287
217.322319	8112.456938	26.826304
217.683680	8128.085321	26.831322
217.889536	8139.669698	26.836340
217.756164	8138.492144	26.841357
218.601744	8163.627661	26.846375
218.509911	8165.713510	26.851392
218.629505	8168.275603	26.856410
218.830992	8173.113828	26.861428
218.840792	8190.214169	26.866445
219.283980	8187.535413	26.871463
219.828726	8199.668746	26.876480
220.204670	8201.804909	26.881498
220.668649	8200.731862	26.886516
220.711463	8199.956819	26.891533
221.155573	8198.115957	26.896551
221.264418	8197.552905	26.901568
221.433835	8201.652906	26.906586
221.808571	8191.301257	26.911604
221.778726	8207.997809	26.916621
221.909548	8219.968771	26.921639
221.713027	8232.668049	26.926656
222.017331	8215.088032	26.931674
222.301735	8235.935536	26.936692
222.100789	8256.931785	26.941709
222.459301	8256.522815	26.946727
222.520331	8280.029343	26.951744
222.962540	8284.259938	26.956762
223.026947	8301.694789	26.961780
223.468149	8319.547866	26.966797
223.937473	8322.483829	26.971815
223.722315	8343.685753	26.976832
224.073029	8358.916788	26.981850
224.375952	8362.215002	26.986868
224.723140	8376.106848	26.991885
224.744771	8372.736059	26.996903
224.804383	8394.254970	27.001920
225.159828	8397.865086	27.006938
225.497268	8414.754005	27.011956
225.329537	8427.431353	27.016973
225.554500	8429.177402	27.021991
225.956222	8461.663046	27.027008
226.117335	8480.898441	27.032026
226.261492	8484.447394	27.037044
226.308075	8506.291547	27.042061
227.161778	8517.597451	27.047079
227.200958	8541.746765	27.052096
227.468431	8559.935217	27.057114
227.734955	8556.643650	27.062132
227.780077	8581.975104	27.067149
228.213862	8584.986303	27.072167
228.540597	8601.553463	27.077184
228.546787	8610.119785	27.082202
228.956241	8623.262736	27.087220
228.598739	8628.090276	27.092237
228.974242	8654.478647	27.097255
229.273337	8654.996323	27.102272
229.492262	8660.806153	27.107290
229.355909	8673.998370	27.112308
229.789482	8698.980694	27.117325
230.313763	8710.347468	27.122343
230.360181	8724.487806	27.127360
230.660948	8755.578450	27.132378
231.247063	8762.703702	27.137396
231.072715	8785.718195	27.142413
231.356737	8787.434046	27.147431
231.463495	8808.187203	27.152448
231.836298	8817.031760	27.157466
232.278063	8832.478994	27.162484
232.414403	8848.198830	27.167501
233.016904	8845.784295	27.172519
233.205708	8868.593186	27.177536
233.225681	8880.786970	27.182554
233.876761	8883.075474	27.187572
233.922866	8899.601093	27.192589
233.900625	8909.228544	27.197607
233.896631	8910.944736	27.202624
234.364774	8932.588281	27.207642
234.670648	8937.173978	27.212660
234.583875	8969.774457	27.217677
234.952078	8978.917607	27.222695
235.233723	8992.522294	27.227712
235.272400	8998.339187	27.232730
235.788572	9015.653707	27.237748
235.839410	9030.101569	27.242765
236.465228	9054.131104	27.247783
236.467633	9064.613150	27.252800
236.263654	9081.584358	27.257818
236.999407	9085.788725	27.262836
236.981678	9107.042539	27.267853
237.383217	9124.252451	27.272871
237.312782	9141.965713	27.277888
237.520356	9171.358565	27.282906
237.824938	9176.000471	27.287924
237.805182	9193.004375	27.292941
238.437019	9214.928457	27.297959
238.470175	9230.066287	27.302976
238.744189	9251.742342	27.307994
239.295276	9263.282315	27.313012
239.860139	9293.106303	27.318029
239.970562	9289.852983	27.323047
240.255997	9313.645341	27.328064
240.466916	9315.692346	27.333082
241.185875	9325.636330	27.338100
241.295815	9332.664861	27.343117
241.677605	9328.565610	27.348135
241.651674	9341.555026	27.353152
241.838903	9363.265264	27.358170
242.313683	9360.562981	27.363188
242.324720	9377.384763	27.368205
242.409306	9379.538508	27.373223
243.003898	9393.940184	27.378240
242.857394	9394.165231	27.383258
243.201885	9401.701702	27.388276
242.985205	9422.943909	27.393293
243.513212	9427.137795	27.398311
243.664098	9445.663180	27.403328
243.600899	9462.596567	27.408346
243.978849	9484.695304	27.413364
243.909175	9491.384150	27.418381
244.553820	9512.402244	27.423399
244.403835	9529.996747	27.428416
244.796774	9555.491264	27.433434
245.053231	9565.267627	27.438452
245.014956	9584.862624	27.443469
245.436328	9597.521551	27.448487
245.577858	9617.490974	27.453504
246.588420	9620.485061	27.458522
247.130526	9616.706630	27.463540
247.606259	9629.137617	27.468557
247.959656	9621.603056	27.473575
247.966349	9628.772447	27.478592
248.269326	9636.831839	27.483610
248.307111	9637.002809	27.488628
248.253719	9663.904838	27.493645
248.373568	9663.248544	27.498663
248.415304	9677.488179	27.503680
248.725812	9689.736193	27.508698
249.020487	9704.010469	27.513716
249.241428	9735.775534	27.518733
249.620267	9744.133594	27.523751
249.934978	9753.200169	27.528768
249.814069	9769.072123	27.533786
250.030266	9782.242453	27.538804
250.462619	9812.662768	27.543821
250.763425	9818.925037	27.548839
251.086646	9835.475161	27.553856
251.114978	9870.343637	27.558874
251.647970	9875.620725	27.563892
251.954599	9883.251118	27.568909
252.570145	9887.603964	27.573927
253.072046	9893.201284	27.578944
252.820386	9911.714948	27.583962
253.480465	9909.082788	27.588980
253.649781	9918.482268	27.593997
254.030868	9932.362789	27.599015
253.810288	9930.842668	27.604032
254.119533	9947.886758	27.609050
254.421530	9961.585803	27.614068
254.529876	9973.591734	27.619085
254.557448	9993.377224	27.624103
254.930472	9998.149067	27.629120
254.837196	10021.810487	27.634138
255.500898	10032.165790	27.639156
255.707084	10054.785241	27.644173
255.771656	10060.851106	27.649191
256.317974	10081.935040	27.654208
256.484868	10103.922203	27.659226
256.700060	10115.763281	27.664244
256.992948	10129.901168	27.669261
257.181096	10152.795508	27.674279
257.112016	10151.571730	27.679296
257.416273	10185.413787	27.684314
257.876503	10196.232132	27.689332
257.940806	10229.447502	27.694349
258.300658	10244.639450	27.699367
258.786433	10257.504891	27.704384
258.473464	10285.170847	27.709402
258.890265	10301.624856	27.714420
259.170601	10321.098793	27.719437
259.375672	10339.685585	27.724455
259.926826	10354.096885	27.729472
259.624680	10382.552905	27.734490
260.196807	10401.163412	27.739508
260.468727	10424.478348	27.744525
260.814115	10462.548345	27.749543
260.824645	10467.090330	27.754560
261.061952	10493.187119	27.759578
261.517636	10504.223057	27.764596
261.690332	10512.014525	27.769613
262.008986	10546.025121	27.774631
262.610261	10554.550097	27.779648
262.557559	10567.984499	27.784666
263.096838	10586.398197	27.789684
263.403138	10611.752742	27.794701
263.327247	10626.893370	27.799719
263.645977	10645.512943	27.804736
263.739627	10658.144934	27.809754
263.872623	10677.383688	27.814772
264.333741	10706.304207	27.819789
264.604929	10730.421652	27.824807
265.345232	10740.026628	27.829824
265.219211	10759.806142	27.834842
265.665520	10772.330328	27.839860
265.573539	10792.746288	27.844877
265.849918	10820.144060	27.849895
266.415766	10830.156042	27.854912
266.518782	10863.303308	27.859930
266.898802	10884.898683	27.864948
267.394944	10906.611186	27.869965
267.576902	10919.483243	27.874983
268.306590	10923.224327	27.880000
268.699401	10943.910154	27.885018
268.560238	10958.766133	27.890036
268.942592	10960.913436	27.895053
269.000818	10964.505502	27.900071
269.665000	10987.277482	27.905088
269.592531	11002.005103	27.910106
270.064437	11020.973212	27.915124
270.481103	11041.181769	27.920141
270.333655	11055.534240	27.925159
270.484498	11066.843875	27.930176
270.863984	11084.486527	27.935194
270.998852	11096.121812	27.940212
271.567036	11113.446567	27.945229
271.783037	11143.515209	27.950247
272.191916	11140.186995	27.955264
272.106513	11187.883350	27.960282
272.652429	11192.151166	27.965300
273.024729	11205.407169	27.970317
272.974385	11231.820534	27.975335
273.308701	11235.769606	27.980352
273.585422	11264.580586	27.985370
273.831830	11279.466905	27.990388
274.538974	11300.216276	27.995405
274.446908	11321.709046	28.000423
275.106512	11335.532955	28.005440
275.011444	11344.063902	28.010458
275.065152	11362.782454	28.015476
275.437283	11380.442403	28.020493
275.617150	11417.828274	28.025511
276.006046	11424.416951	28.030528
276.099500	11441.816557	28.035546
276.171097	11458.264980	28.040564
276.570480	11484.625728	28.045581
276.735523	11515.181680	28.050599
277.123306	11529.509955	28.055616
277.319081	11557.442254	28.060634
277.865067	11595.061898	28.065652
278.360815	11608.828033	28.070669
278.210685	11628.189546	28.075687
279.069615	11655.876160	28.080704
279.643003	11662.813390	28.085722
280.003583	11658.191590	28.090740
280.245737	11678.582619	28.095757
280.608450	11686.650511	28.100775
281.006061	11693.106295	28.105792
281.736907	11682.449345	28.110810
281.580747	11681.332798	28.115828
282.028286	11671.683791	28.120845
281.658338	11686.914966	28.125863
282.288642	11698.371933	28.130880
282.315807	11705.412033	28.135898
282.317182	11719.052748	28.140916
282.427969	11736.304852	28.145933
282.475381	11768.069530	28.150951
282.465351	11772.242644	28.155968
282.839039	11804.127594	28.160986
283.166821	11834.245238	28.166004
283.305750	11850.252789	28.171021
283.410414	11889.837591	28.176039
284.058085	11901.421037	28.181056
284.629085	11922.827906	28.186074
284.828522	11947.456151	28.191092
285.363375	11959.635753	28.196109
285.584196	11987.844339	28.201127
285.932758	11997.632186	28.206144
286.458308	12019.773068	28.211162
286.574381	12037.618643	28.216180
287.133640	12038.302233	28.221197
287.226606	12073.327897	28.226215
287.309093	12083.155029	28.231232
287.905652	12105.337870	28.236250
288.318291	12093.510511	28.241268
288.936192	12112.656690	28.246285
288.975977	12123.821549	28.251303
289.414989	12136.675749	28.256320
289.465095	12160.224450	28.261338
289.429816	12163.807023	28.266356
290.013676	12178.176752	28.271373
290.044396	12207.535856	28.276391
290.184600	12227.351184	28.281408
290.388823	12241.236145	28.286426
290.634446	12265.628773	28.291444
291.219997	12287.315771	28.296461
291.339876	12302.583986	28.301479
291.905079	12307.341320	28.306496
291.910606	12339.526873	28.311514
291.848609	12370.217288	28.316532
292.571243	12392.773619	28.321549
292.754791	12408.693993	28.326567
293.034198	12427.759387	28.331584
293.320143	12462.073311	28.336602
293.954907	12477.351954	28.341620
294.259018	12484.781532	28.346637
294.715063	12503.693352	28.351655
294.988016	12508.658965	28.356672
295.251966	12528.859961	28.361690
295.095687	12549.237559	28.366708
295.571846	12565.062473	28.371725
295.528983	12581.408048	28.376743
295.816464	12615.312361	28.381760
296.046224	12626.816474	28.386778
296.449550	12655.240311	28.391796
297.315164	12669.764047	28.396813
297.417101	12696.940936	28.401831
298.110654	12700.229884	28.406848
298.368496	12727.782876	28.411866
298.398412	12749.765565	28.416884
298.880308	12752.454476	28.421901
299.152861	12779.054963	28.426919
299.606184	12790.648315	28.431936
299.635708	12809.722355	28.436954
300.256701	12816.289807	28.441972
300.815517	12815.486806	28.446989
300.659871	12834.580438	28.452007
300.739957	12834.045617	28.457024
301.334627	12834.010377	28.462042
301.677759	12860.038375	28.467060
302.230767	12861.992294	28.472077
302.098543	12876.802408	28.477095
302.440323	12893.097355	28.482112
302.361420	12909.275885	28.487130
302.692634	12928.843852	28.492148
303.072502	12944.434505	28.497165
303.120491	12967.058983	28.502183
303.128125	12978.540167	28.507200
303.486928	13004.712354	28.512218
303.551756	13038.126464	28.517236
304.082000	13056.429465	28.522253
304.205895	13097.154896	28.527271
303.964272	13122.318714	28.532288
304.465495	13156.253455	28.537306
304.730389	13187.468142	28.542324
305.182810	13222.425880	28.547341
305.435862	13259.800777	28.552359
306.062762	13297.577276	28.557376
306.640159	13312.916617	28.562394
306.740554	13342.757913	28.567412
307.511051	13350.219567	28.572429
307.874261	13393.933287	28.577447
308.069724	13412.526794	28.582464
308.753658	13438.103895	28.587482
308.806706	13460.072695	28.592500
309.460092	13464.107489	28.597517
309.943806	13483.518567	28.602535
309.983315	13497.976260	28.607552
310.544326	13504.090621	28.612570
310.462993	13526.173109	28.617588
310.659972	13551.711080	28.622605
310.968671	13564.020662	28.627623
311.365938	13591.812098	28.632640
311.956873	13606.413581	28.637658
312.148504	13621.268568	28.642676
312.566143	13640.808937	28.647693
312.821278	13673.455435	28.652711
312.776695	13699.407016	28.657728
313.008629	13715.298622	28.662746
313.174694	13745.963419	28.667764
313.471091	13762.906525	28.672781
313.913964	13800.586960	28.677799
313.805979	13822.924811	28.682816
314.538244	13835.500272	28.687834
314.682941	13880.389154	28.692852
315.095321	13902.176272	28.697869
315.286644	13933.426613	28.702887
315.741842	13968.046695	28.707904
316.030671	13986.592343	28.712922
316.243674	14020.346439	28.717940
316.867140	14036.958447	28.722957
316.995994	14064.456231	28.727975
317.635401	14085.900372	28.732992
318.329002	14091.797647	28.738010
318.892040	14103.164230	28.743028
319.072734	14118.998512	28.748045
319.354858	14138.795097	28.753063
319.561435	14157.770556	28.758080
320.057497	14176.672998	28.763098
320.041537	14200.338799	28.768116
320.609330	14201.642765	28.773133
320.763285	14219.457698	28.778151
320.945954	14244.086695	28.783168
321.420752	14247.123728	28.788186
321.527731	14274.012467	28.793204
321.783827	14274.652488	28.798221
322.107515	14296.131735	28.803239
322.334087	14317.620751	28.808256
322.669276	14336.964414	28.813274
322.659212	14364.116899	28.818292
323.417357	14379.900159	28.823309
323.700846	14410.698095	28.828327
323.626775	14422.726448	28.833344
324.085629	14448.022427	28.838362
324.152189	14478.509635	28.843380
324.906613	14501.533281	28.848397
325.504658	14518.813437	28.853415
325.661526	14544.324926	28.858432
326.200502	14557.473419	28.863450
326.322487	14575.645450	28.868468
326.301574	14590.891017	28.873485
326.714754	14611.512787	28.878503
327.121948	14635.471769	28.883520
327.822800	14653.056568	28.888538
327.869685	14679.598174	28.893556
328.342042	14698.467319	28.898573
328.682445	14731.905572	28.903591
328.873154	14748.507860	28.908608
329.299965	14761.544248	28.913626
329.452684	14802.584377	28.918644
329.967436	14818.056844	28.923661
330.565700	14828.346489	28.928679
330.940382	14856.354996	28.933696
331.134429	14871.089381	28.938714
331.254077	14890.578052	28.943732
331.505164	14912.208789	28.948749
332.129438	14937.241810	28.953767
332.339182	14963.867288	28.958784
333.062498	14978.345704	28.963802
333.202510	15009.343407	28.968820
333.483234	15029.388731	28.973837
333.789634	15044.293825	28.978855
333.745273	15079.142217	28.983872
334.288590	15086.709981	28.988890
334.394326	15116.452788	28.993908
334.776038	15138.601222	28.998925
335.179199	15167.748128	29.003943
335.474086	15187.680990	29.008960
336.288627	15208.563434	29.013978
336.861582	15222.200129	29.018996
337.091480	15229.764582	29.024013
337.528160	15254.635241	29.029031
337.764804	15271.728479	29.034048
337.952522	15286.508412	29.039066
338.019974	15315.019193	29.044084
338.279587	15339.673382	29.049101
338.953249	15366.359984	29.054119
338.955387	15385.856052	29.059136
339.275360	15399.005161	29.064154
339.184566	15438.909861	29.069172
339.445873	15480.110263	29.074189
340.126784	15505.059154	29.079207
339.985894	15534.230405	29.084224
340.513937	15569.431282	29.089242
341.206443	15593.700714	29.094260
341.068221	15625.836144	29.099277
341.649599	15656.995406	29.104295
342.340117	15679.506471	29.109312
342.923397	15689.953589	29.114330
343.046962	15711.486676	29.119348
343.730978	15740.671735	29.124365
343.867026	15764.633045	29.129383
343.975910	15780.698295	29.134400
344.283027	15788.179330	29.139418
344.944522	15799.258188	29.144436
345.516393	15819.043621	29.149453
346.077981	15821.603266	29.154471
346.215929	15845.874858	29.159488
347.229029	15860.632426	29.164506
347.274748	15872.706672	29.169524
347.418613	15881.005886	29.174541
347.744823	15883.774639	29.179559
347.794686	15895.304487	29.184576
348.440926	15924.422043	29.189594
348.242557	15931.097771	29.194612
348.770358	15953.968641	29.199629
348.999931	15987.851731	29.204647
348.978777	16004.416224	29.209664
349.964502	16030.417215	29.214682
349.874947	16057.926072	29.219700
350.097362	16090.554450	29.224717
350.612764	16103.552062	29.229735
350.838351	16151.124144	29.234752
350.505047	16154.239884	29.239770
351.180044	16198.095595	29.244788
350.866812	16241.830994	29.249805
351.813171	16265.063416	29.254823
351.433648	16319.092223	29.259840
351.855041	16347.437578	29.264858
353.037477	16389.499931	29.269876
353.149182	16436.021496	29.274893
353.784353	16461.877773	29.279911
353.822288	16516.648370	29.284928
354.186191	16545.146988	29.289946
354.926190	16586.422394	29.294964
355.313253	16623.793897	29.299981
355.416769	16651.509842	29.304999
355.951152	16691.520773	29.310016
356.778930	16719.902082	29.315034
357.214516	16747.471914	29.320052
357.004258	16769.915793	29.325069
357.778510	16790.847901	29.330087
358.084092	16811.206526	29.335104
358.101933	16844.502221	29.340122
358.589834	16877.227000	29.345140
358.734251	16909.553089	29.350157
359.139207	16938.942425	29.355175
359.326001	16978.417278	29.360192
360.418831	17006.293488	29.365210
361.099894	17022.867512	29.370228
361.349231	17052.000631	29.375245
361.839675	17076.430163	29.380263
361.938920	17104.889940	29.385280
362.005421	17132.313342	29.390298
362.866397	17155.677771	29.395316
363.084548	17187.150560	29.400333
363.470057	17203.017040	29.405351
363.622313	17233.348634	29.410368
363.975026	17260.680834	29.415386
364.093008	17285.284116	29.420404
363.899901	17310.717453	29.425421
364.511494	17345.285757	29.430439
364.829633	17384.865978	29.435456
365.342568	17417.921847	29.440474
366.118589	17440.058691	29.445492
366.297394	17473.494563	29.450509
366.838553	17495.331403	29.455527
366.618498	17536.744159	29.460544
367.347881	17557.240175	29.465562
367.690709	17591.278088	29.470580
367.638108	17619.489581	29.475597
368.717047	17638.235117	29.480615
369.562220	17660.113372	29.485632
369.867442	17671.815066	29.490650
370.478890	17685.292996	29.495668
370.772419	17708.660539	29.500685
371.249402	17729.316683	29.505703
371.501583	17742.061181	29.510720
371.524716	17754.919186	29.515738
371.982860	17770.036548	29.520756
372.229077	17797.234340	29.525773
372.681789	17808.159913	29.530791
373.122327	17827.019013	29.535808
373.575974	17833.028237	29.540826
373.899869	17853.402465	29.545844
373.727048	17880.579776	29.550861
374.647774	17898.891494	29.555879
374.981173	17926.852174	29.560896
374.809916	17953.887486	29.565914
375.688840	17972.783091	29.570932
375.530731	18001.879593	29.575949
376.351727	18020.939294	29.580967
376.522058	18055.764831	29.585984
376.564714	18083.964533	29.591002
376.783768	18107.409570	29.596020
377.240013	18149.320563	29.601037
377.953847	18161.908731	29.606055
378.267270	18198.801032	29.611072
378.657897	18242.652432	29.616090
378.888965	18269.881877	29.621108
379.362600	18297.878339	29.626125
379.835185	18333.523047	29.631143
380.108572	18370.868429	29.636160
381.072756	18393.163049	29.641178
381.125825	18416.419997	29.646196
381.205022	18442.781070	29.651213
382.136320	18462.981623	29.656231
382.411782	18499.100610	29.661248
382.527402	18520.933449	29.666266
382.941645	18554.187595	29.671284
383.038642	18597.229368	29.676301
383.695803	18631.687231	29.681319
383.682001	18668.968812	29.686336
383.761802	18702.700954	29.691354
384.051574	18736.896588	29.696372
384.641431	18779.666680	29.701389
385.287814	18814.534967	29.706407
385.969651	18848.576213	29.711424
386.104516	18889.364667	29.716442
386.787640	18911.905037	29.721460
387.062581	18942.454370	29.726477
387.489913	18966.410047	29.731495
387.877519	19010.413729	29.736512
388.231185	19036.703606	29.741530
389.145801	19063.764686	29.746548
389.228741	19088.921850	29.751565
390.434023	19109.539801	29.756583
390.968485	19123.488767	29.761600
391.355522	19141.923139	29.766618
391.566410	19150.690560	29.771636
392.107667	19161.678070	29.776653
392.220753	19182.265312	29.781671
392.626545	19203.193582	29.786688
392.576917	19233.582688	29.791706
393.282956	19251.076999	29.796724
393.097103	19289.367309	29.801741
393.514030	19298.524810	29.806759
393.896757	19323.817239	29.811776
393.788010	19358.710533	29.816794
394.112990	19381.009623	29.821812
394.682856	19421.309786	29.826829
394.908624	19449.598210	29.831847
395.126931	19492.059497	29.836864
395.375975	19528.733667	29.841882
395.845156	19562.918704	29.846900
396.098565	19607.318162	29.851917
396.611794	19642.954243	29.856935
396.815424	19678.980469	29.861952
397.048798	19723.470248	29.866970
397.551678	19768.735351	29.871988
398.030242	19820.578195	29.877005
398.575586	19858.862520	29.882023
399.091266	19898.762926	29.887040
399.338748	19943.548903	29.892058
400.133343	19982.725575	29.897076
400.098710	20006.962427	29.902093
400.950762	20054.041836	29.907111
401.557895	20093.040071	29.912128
401.700169	20120.394417	29.917146
402.227514	20159.524221	29.922164
402.886148	20188.049795	29.927181
403.033842	20218.028176	29.932199
403.593776	20263.550040	29.937216
403.788269	20288.263371	29.942234
404.579746	20314.990561	29.947252
405.113366	20365.976300	29.952269
405.353059	20387.847846	29.957287
406.230575	20408.497920	29.962304
406.396827	20447.008597	29.967322
407.227332	20475.165756	29.972340
407.254414	20511.366403	29.977357
407.456794	20534.652092	29.982375
408.011966	20570.842876	29.987392
408.618112	20609.147258	29.992410
408.661114	20641.940366	29.997428
408.669913	20676.845371	30.002445
409.278430	20710.287716	30.007463
409.705614	20749.856374	30.012480
409.675419	20792.540166	30.017498
410.323080	20825.631023	30.022516
410.893866	20871.319861	30.027533
411.024726	20898.776686	30.032551
411.543533	20944.836908	30.037568
411.717828	21002.398087	30.042586
411.962019	21038.184068	30.047604
412.309807	21093.222846	30.052621
412.867653	21140.048076	30.057639
412.981508	21180.844027	30.062656
414.204139	21225.480231	30.067674
414.758640	21269.736623	30.072692
414.974129	21307.271573	30.077709
415.491104	21339.877390	30.082727
416.477100	21364.185661	30.087744
416.445642	21395.081766	30.092762
417.141819	21426.086325	30.097780
417.775619	21467.159688	30.102797
417.908310	21493.764267	30.107815
418.327788	21523.056850	30.112832
418.634821	21541.079846	30.117850
419.741958	21567.020643	30.122868
420.478785	21583.938457	30.127885
420.818101	21598.306424	30.132903
421.532044	21622.817672	30.137920
421.496650	21640.556804	30.142938
421.762938	21667.423372	30.147956
422.212397	21685.085608	30.152973
422.282855	21716.121548	30.157991
422.772182	21734.567118	30.163008
422.756962	21767.945922	30.168026
423.167512	21786.885422	30.173044
423.222164	21822.748533	30.178061
423.531010	21855.249418	30.183079
424.265070	21894.550940	30.188096
424.297868	21933.254197	30.193114
424.828653	21964.102613	30.198132
425.225099	21998.364562	30.203149
425.440045	22043.757490	30.208167
426.023478	22078.975674	30.213184
426.444616	22119.808281	30.218202
426.877153	22164.405660	30.223220
427.573871	22198.167498	30.228237
427.958217	22254.916264	30.233255
428.602083	22278.255998	30.238272
428.584088	22323.171023	30.243290
429.230192	22364.476317	30.248308
429.960248	22405.424134	30.253325
430.219746	22440.053315	30.258343
430.865899	22466.316041	30.263360
431.225448	22499.140892	30.268378
431.482556	22542.492738	30.273396
432.076653	22579.116588	30.278413
432.363441	22609.371100	30.283431
433.597319	22639.425067	30.288448
434.022270	22663.039577	30.293466
434.767254	22697.658462	30.298484
435.272604	22733.316618	30.303501
435.286637	22759.025173	30.308519
435.930559	22785.194166	30.313536
435.977170	22815.083516	30.318554
436.723074	22832.068892	30.323572
436.991895	22876.810300	30.328589
437.002609	22916.153291	30.333607
437.909127	22943.163677	30.338624
438.124647	22978.474478	30.343642
438.335612	23011.124631	30.348660
438.731242	23043.808986	30.353677
438.811418	23089.455615	30.358695
439.380735	23128.927564	30.363712
439.466265	23177.935102	30.368730
440.187376	23204.782599	30.373748
440.735083	23249.595601	30.378765
440.935462	23297.015670	30.383783
441.979426	23327.756586	30.388800
442.080943	23370.075118	30.393818
443.029513	23415.962323	30.398836
443.943906	23447.349251	30.403853
444.044022	23465.339114	30.408871
444.463973	23499.122478	30.413888
444.674143	23540.322917	30.418906
445.104597	23575.724024	30.423924
445.486227	23612.117167	30.428941
445.741889	23643.037759	30.433959
446.410547	23684.700486	30.438976
446.883355	23723.188520	30.443994
447.512546	23744.657934	30.449012
447.718381	23776.815306	30.454029
448.404343	23816.815157	30.459047
449.443640	23839.721194	30.464064
449.690831	23870.736630	30.469082
449.891162	23889.883517	30.474100
450.538699	23924.052713	30.479117
450.735195	23957.935400	30.484135
451.434793	23979.844446	30.489152
451.689154	24023.906948	30.494170
451.946516	24049.717601	30.499188
452.367202	24064.252412	30.504205
452.448504	24101.514579	30.509223
452.849104	24127.360031	30.514240
452.910282	24178.856380	30.519258
452.941720	24213.578902	30.524276
453.744662	24262.198276	30.529293
453.834075	24308.844789	30.534311
454.349017	24358.114359	30.539328
454.741161	24413.355325	30.544346
455.088322	24457.386276	30.549364
456.075657	24507.133291	30.554381
456.084376	24559.068357	30.559399
456.816451	24598.743914	30.564416
457.282368	24649.315445	30.569434
457.811770	24687.531406	30.574452
458.300232	24742.836375	30.579469
458.633071	24791.686300	30.584487
458.964405	24831.024919	30.589504
459.484763	24875.621247	30.594522
459.969611	24925.253805	30.599540
460.695999	24976.123886	30.604557
461.235843	25024.675368	30.609575
461.786514	25062.242134	30.614592
462.064395	25124.567191	30.619610
462.390090	25175.647555	30.624628
462.862819	25225.806524	30.629645
463.114801	25283.705327	30.634663
464.151367	25327.791800	30.639680
465.251156	25361.841876	30.644698
465.681860	25395.360738	30.649716
466.684972	25427.042606	30.654733
466.832750	25465.283930	30.659751
467.444814	25493.698465	30.664768
467.835845	25523.901534	30.669786
468.058365	25563.974172	30.674804
468.685084	25596.648926	30.679821
469.071302	25641.162183	30.684839
469.609954	25674.349949	30.689856
469.914848	25716.170789	30.694874
470.326541	25749.505830	30.699892
471.233332	25779.261455	30.704909
471.732943	25810.409041	30.709927
472.332176	25832.154133	30.714944
472.497464	25868.100560	30.719962
473.340497	25898.207550	30.724980
473.810737	25936.570130	30.729997
473.983243	25967.002472	30.735015
474.507079	26002.580867	30.740032
474.741202	26031.145462	30.745050
475.218646	26074.219186	30.750068
475.412508	26108.000925	30.755085
475.647355	26148.541262	30.760103
476.352873	26184.600971	30.765120
476.577146	26246.902705	30.770138
476.860842	26286.754034	30.775156
477.203400	26327.636560	30.780173
477.362769	26370.646872	30.785191
478.220297	26429.201761	30.790208
478.467974	26483.782558	30.795226
479.033081	26541.332682	30.800244
479.511148	26580.294682	30.805261
479.736724	26646.688476	30.810279
480.054599	26696.287525	30.815296
480.764510	26756.646823	30.820314
480.910848	26805.700477	30.825332
481.751069	26852.889117	30.830349
481.851602	26916.194649	30.835367
482.732143	26953.308931	30.840384
483.287438	27008.534490	30.845402
483.386248	27043.529193	30.850420
484.248637	27105.927346	30.855437
484.676893	27164.596659	30.860455
485.429932	27208.419404	30.865472
486.066513	27243.155355	30.870490
486.855205	27283.660507	30.875508
487.316845	27320.131931	30.880525
487.818655	27352.808592	30.885543
488.123174	27404.181401	30.890560
489.019296	27448.665589	30.895578
488.766517	27497.355014	30.900596
489.553517	27534.066491	30.905613
489.728640	27581.284986	30.910631
489.866579	27634.152722	30.915648
490.043597	27695.079633	30.920666
490.446442	27753.379790	30.925684
491.149284	27818.147358	30.930701
491.693540	27884.408117	30.935719
492.260052	27922.689837	30.940736
493.486303	27972.344390	30.945754
493.859952	28040.144848	30.950772
494.370961	28079.641040	30.955789
494.838405	28137.641626	30.960807
495.628938	28187.539107	30.965824
496.261315	28238.592122	30.970842
496.606528	28269.145109	30.975860
497.249456	28312.187641	30.980877
497.809097	28358.360577	30.985895
498.369796	28398.789301	30.990912
498.810117	28449.761106	30.995930
499.235171	28480.824910	31.000948
499.446303	28532.169184	31.005965
499.736085	28582.951747	31.010983
500.366469	28645.340172	31.016000
500.717989	28700.784614	31.021018
500.929147	28752.091681	31.026036
501.867604	28800.140064	31.031053
502.393879	28861.502335	31.036071
503.082354	28913.049637	31.041088
503.385198	28957.443293	31.046106
503.960454	29008.369217	31.051124
504.812574	29054.300119	31.056141
504.955762	29102.108470	31.061159
505.510346	29152.161273	31.066176
505.936890	29206.184861	31.071194
506.288817	29268.684617	31.076212
506.901412	29328.734604	31.081229
507.131500	29384.854286	31.086247
507.917919	29440.125152	31.091264
508.408312	29478.407116	31.096282
508.645358	29539.929971	31.101300
509.388564	29594.366187	31.106317
510.117943	29653.177169	31.111335
510.537697	29697.420911	31.116352
511.129915	29737.992665	31.121370
511.638994	29796.443036	31.126388
512.346763	29845.286384	31.131405
512.821812	29910.026845	31.136423
512.943167	29949.796717	31.141440
513.899827	30000.665705	31.146458
514.229986	30060.146552	31.151476
514.439124	30105.299972	31.156493
514.709369	30166.598727	31.161511
515.579666	30206.125594	31.166528
517.007805	30252.453502	31.171546
517.474268	30281.119246	31.176564
518.294632	30300.662999	31.181581
519.097782	30330.989392	31.186599
519.733880	30362.204681	31.191616
520.453389	30376.096084	31.196634
520.500680	30414.894967	31.201652
521.002345	30447.956069	31.206669
521.152042	30475.406238	31.211687
521.485914	30515.574501	31.216704
521.875811	30549.300987	31.221722
521.914203	30601.903961	31.226740
522.658218	30643.093176	31.231757
522.805305	30693.315522	31.236775
523.172803	30745.997070	31.241792
524.027809	30800.790860	31.246810
524.318376	30849.822667	31.251828
524.670643	30909.324839	31.256845
525.121510	30953.683359	31.261863
525.641976	31008.346923	31.266880
526.298684	31057.482885	31.271898
526.426535	31130.478448	31.276916
527.023474	31187.268956	31.281933
527.491734	31245.147264	31.286951
527.940826	31311.342158	31.291968
529.065365	31371.393492	31.296986
529.596424	31421.188528	31.302004
530.382239	31482.334170	31.307021
531.176785	31530.256119	31.312039
531.524835	31583.097990	31.317056
532.254385	31630.011891	31.322074
532.549003	31685.049299	31.327092
533.180631	31735.876075	31.332109
533.706253	31788.190743	31.337127
534.290006	31853.523051	31.342144
535.030714	31900.132950	31.347162
535.073678	31945.498401	31.352180
535.777124	31998.822332	31.357197
536.166789	32051.134999	31.362215
536.755355	32116.524282	31.367232
537.599474	32165.604000	31.372250
537.654789	32219.682448	31.377268
538.134424	32284.613930	31.382285
538.517966	32338.240984	31.387303
539.295848	32400.312426	31.392320
540.405233	32446.455867	31.397338
541.344684	32505.478379	31.402356
541.384896	32549.596405	31.407373
542.103417	32599.259696	31.412391
542.965186	32653.853078	31.417408
543.640212	32685.870649	31.422426
544.317239	32733.360949	31.427444
544.562922	32770.090862	31.432461
545.264014	32819.713482	31.437479
545.554071	32862.566806	31.442496
546.106606	32906.061560	31.447514
546.483077	32961.502770	31.452532
546.837517	33002.487374	31.457549
547.036934	33053.193722	31.462567
547.377109	33121.533736	31.467584
547.989973	33181.429667	31.472602
548.307994	33249.852718	31.477620
548.920684	33319.268606	31.482637
549.067590	33377.143899	31.487655
549.692339	33448.385218	31.492672
550.355267	33497.025278	31.497690
550.921187	33575.603473	31.502708
551.695522	33630.867473	31.507725
552.210884	33686.546752	31.512743
552.673876	33745.033662	31.517760
553.440028	33790.861830	31.522778
553.793460	33860.827523	31.527796
554.311649	33917.497851	31.532813
554.737014	33973.681983	31.537831
555.017880	34050.902060	31.542848
555.695939	34104.239703	31.547866
556.424308	34163.006011	31.552884
557.537486	34214.113797	31.557901
558.432139	34262.869148	31.562919
558.955204	34303.245151	31.567936
559.825069	34349.382647	31.572954
560.306172	34405.183438	31.577972
560.713159	34452.877578	31.582989
561.364938	34507.318884	31.588007
561.638068	34562.949414	31.593024
562.380246	34610.563368	31.598042
562.693291	34674.136397	31.603060
563.063449	34725.652382	31.608077
564.086840	34781.301673	31.613095
564.521190	34829.336256	31.618112
565.074540	34882.068880	31.623130
565.377042	34934.672691	31.628148
565.916080	34997.452209	31.633165
566.562327	35036.386364	31.638183
567.108585	35110.241211	31.643200
567.832562	35168.727566	31.648218
568.142441	35241.261929	31.653236
568.238512	35293.263458	31.658253
569.304211	35364.922443	31.663271
569.556610	35425.832179	31.668288
570.190467	35496.960291	31.673306
570.419712	35573.176210	31.678324
571.204438	35627.201363	31.683341
572.264776	35689.152467	31.688359
572.726240	35747.497892	31.693376
574.116626	35790.094486	31.698394
575.013404	35838.487742	31.703412
575.811480	35906.611351	31.708429
576.310189	35946.818382	31.713447
576.703096	36003.153129	31.718464
577.193980	36033.850188	31.723482
577.610133	36087.663060	31.728500
578.020325	36142.057743	31.733517
578.909207	36184.425692	31.738535
578.606136	36251.706858	31.743552
579.463372	36305.185598	31.748570
579.926989	36362.216698	31.753588
580.484065	36423.903176	31.758605
581.191399	36485.372542	31.763623
581.841575	36548.596748	31.768640
582.378482	36606.402326	31.773658
583.385636	36643.781339	31.778676
583.757210	36713.168225	31.783693
584.682677	36766.665476	31.788711
584.820803	36823.871727	31.793728
585.343577	36876.470112	31.798746
586.344451	36943.491156	31.803764
586.888538	36998.576404	31.808781
587.323155	37043.116955	31.813799
587.592812	37098.822218	31.818816
588.084558	37157.135669	31.823834
588.486616	37214.009218	31.828852
588.799119	37298.907109	31.833869
589.482451	37352.938434	31.838887
589.658085	37431.001573	31.843904
590.062924	37497.065862	31.848922
590.673347	37555.503021	31.853940
590.979878	37634.145064	31.858957
591.445610	37715.620545	31.863975
591.778043	37788.836872	31.868992
592.409752	37872.614830	31.874010
593.135280	37946.161379	31.879028
593.205005	38039.068849	31.884045
593.901919	38106.687278	31.889063
595.289444	38174.961992	31.894080
596.468830	38246.768360	31.899098
597.053793	38321.488494	31.904116
597.732823	38400.438460	31.909133
598.241078	38454.846025	31.914151
598.524334	38531.134982	31.919168
599.125920	38600.140793	31.924186
599.466156	38680.385173	31.929204
600.301115	38754.235712	31.934221
600.880091	38825.288203	31.939239
601.207931	38894.810631	31.944256
601.929198	38978.067597	31.949274
602.485661	39052.773357	31.954292
602.956946	39145.992615	31.959309
603.854327	39223.877988	31.964327
604.330846	39289.075300	31.969344
605.272319	39375.621338	31.974362
606.597541	39441.139846	31.979380
607.058921	39509.348460	31.984397
607.954846	39564.111961	31.989415
608.588989	39650.050383	31.994432
609.378758	39702.634983	31.999450
610.381567	39749.256802	32.004468
611.074141	39801.239083	32.009485
611.947261	39855.653711	32.014503
612.225406	39912.448878	32.019520
612.727625	39962.357712	32.024538
613.221565	40027.204424	32.029556
613.495425	40091.614245	32.034573
614.090461	40142.720329	32.039591
614.752147	40208.982494	32.044608
615.262168	40271.011824	32.049626
616.138635	40335.865896	32.054644
616.454298	40404.906839	32.059661
617.221300	40476.733323	32.064679
617.412303	40558.052281	32.069696
617.896271	40614.900864	32.074714
618.662079	40676.103338	32.079732
619.210429	40761.123658	32.084749
619.584454	40829.812496	32.089767
620.362284	40913.015297	32.094784
621.040005	40978.636810	32.099802
621.768653	41058.994807	32.104820
622.228996	41139.375374	32.109837
622.883506	41201.889060	32.114855
623.304347	41275.758237	32.119872
624.043873	41359.913239	32.124890
624.749142	41428.811617	32.129908
625.199845	41517.750101	32.134925
625.949094	41589.580724	32.139943
626.553829	41660.207522	32.144960
627.161466	41733.302696	32.149978
627.979413	41806.518106	32.154996
628.459306	41879.805426	32.160013
629.333340	41951.493739	32.165031
629.393379	42030.403802	32.170048
630.031787	42104.597093	32.175066
631.052040	42188.652701	32.180084
631.650489	42270.751662	32.185101
632.141135	42332.709083	32.190119
632.923505	42409.294822	32.195136
633.562718	42476.866364	32.200154
634.399956	42541.649478	32.205172
635.020595	42608.495328	32.210189
635.678657	42670.018991	32.215207
636.189500	42729.158439	32.220224
636.574251	42806.553375	32.225242
637.185703	42867.068858	32.230260
637.571442	42947.438067	32.235277
637.980250	43030.512502	32.240295
638.581779	43121.230127	32.245312
638.893776	43199.892049	32.250330
639.668073	43288.602517	32.255348
640.490747	43370.397825	32.260365
641.279343	43439.848750	32.265383
641.955376	43525.245895	32.270400
642.711231	43614.159862	32.275418
643.642948	43678.356768	32.280436
644.575288	43748.637523	32.285453
645.250859	43827.096831	32.290471
645.895970	43896.345852	32.295488
646.270364	43969.049550	32.300506
647.016186	44040.966043	32.305524
647.880601	44114.628081	32.310541
649.641899	44163.191153	32.315559
650.324072	44222.588058	32.320576
651.170580	44285.430922	32.325594
652.083034	44343.148441	32.330612
652.589597	44392.421339	32.335629
653.068404	44442.743990	32.340647
653.702452	44495.295397	32.345664
654.043293	44558.071150	32.350682
654.473356	44622.894061	32.355700
654.739576	44699.801833	32.360717
655.366365	44766.073507	32.365735
655.580512	44851.669847	32.370752
655.771943	44933.547873	32.375770
656.411452	45008.958695	32.380788
656.725757	45103.973702	32.385805
657.173636	45186.495622	32.390823
657.705181	45283.158524	32.395840
658.321995	45377.809224	32.400858
659.610371	45468.731120	32.405876
660.321264	45562.394739	32.410893
661.187804	45649.708806	32.415911
661.784582	45736.281631	32.420928
662.534687	45829.753822	32.425946
663.411832	45903.092443	32.430964
663.968141	45998.334087	32.435981
664.675136	46068.733427	32.440999
665.679131	46145.859983	32.446016
666.349840	46231.194612	32.451034
667.449543	46291.792146	32.456052
668.764811	46352.777385	32.461069
669.713420	46410.451116	32.466087
670.202325	46477.793611	32.471104
670.642018	46547.888406	32.476122
671.599579	46603.985624	32.481140
671.824842	46672.941678	32.486157
672.807989	46729.063463	32.491175
673.145373	46801.774806	32.496192
673.415914	46871.393522	32.501210
674.185418	46946.572789	32.506228
674.490372	47021.188075	32.511245
675.356950	47095.799315	32.516263
676.020946	47164.719443	32.521280
675.985573	47254.504496	32.526298
676.614377	47327.596024	32.531316
677.168984	47408.897517	32.536333
677.551821	47482.339722	32.541351
677.991687	47574.709772	32.546368
678.357348	47663.647413	32.551386
679.398334	47761.312548	32.556404
679.894718	47851.685217	32.561421
680.577661	47936.776078	32.566439
681.209505	48030.029248	32.571456
681.561888	48126.808964	32.576474
682.412306	48220.702750	32.581492
683.063428	48318.435145	32.586509
683.721373	48426.262673	32.591527
684.683038	48524.945893	32.596544
685.016380	48618.829150	32.601562
686.135588	48714.237839	32.606580
686.890870	48814.260873	32.611597
687.674834	48901.793102	32.616615
688.421946	48995.054078	32.621632
688.980690	49094.735245	32.626650
690.116939	49180.808426	32.631668
690.574422	49273.041714	32.636685
691.390411	49358.846473	32.641703
692.175048	49447.631683	32.646720
692.666230	49546.912666	32.651738
693.777965	49636.652159	32.656756
694.625712	49731.507582	32.661773
695.282874	49815.543666	32.666791
696.350757	49892.905482	32.671808
696.644944	49995.082591	32.676826
697.991493	50065.236413	32.681844
699.015839	50143.468612	32.686861
699.784499	50217.574557	32.691879
700.454499	50299.112523	32.696896
701.203844	50380.947237	32.701914
702.480209	50439.062304	32.706932
703.045470	50517.460280	32.711949
703.704997	50578.813766	32.716967
704.387786	50652.493422	32.721984
704.777390	50728.884198	32.727002
705.505646	50803.119095	32.732020
705.984345	50881.318089	32.737037
706.746727	50952.860224	32.742055
707.067758	51033.394594	32.747072
707.730572	51117.410185	32.752090
708.205844	51199.217850	32.757108
708.660528	51299.451962	32.762125
709.066595	51398.965039	32.767143
709.946463	51466.674365	32.772160
710.747840	51576.375198	32.777178
711.417962	51665.467529	32.782196
712.043914	51760.189578	32.787213
712.487745	51862.361369	32.792231
713.480737	51961.909916	32.797248
714.346443	52058.937418	32.802266
714.983580	52152.696207	32.807284
715.735622	52239.336136	32.812301
716.086538	52344.861210	32.817319
717.322010	52433.197264	32.822336
718.077306	52542.061541	32.827354
718.677037	52630.263435	32.832372
719.285689	52713.252583	32.837389
719.997047	52820.382137	32.842407
720.688143	52916.390956	32.847424
721.223890	53022.533551	32.852442
721.754511	53109.466627	32.857460
722.361958	53221.599912	32.862477
722.913909	53329.541949	32.867495
723.694362	53420.130823	32.872512
724.642954	53526.403827	32.877530
725.443635	53613.496714	32.882548
726.146687	53703.404767	32.887565
726.532625	53782.568949	32.892583
727.417044	53878.342110	32.897600
727.943604	53985.830794	32.902618
728.676332	54088.105569	32.907636
729.895046	54174.051610	32.912653
731.031628	54269.507072	32.917671
732.104990	54346.134024	32.922688
732.619660	54440.214681	32.927706
733.212702	54538.004015	32.932724
733.910426	54622.629207	32.937741
734.583323	54711.030607	32.942759
735.439597	54793.002137	32.947776
736.429319	54883.689601	32.952794
737.915078	54951.159390	32.957812
738.820248	55032.037168	32.962829
739.578004	55111.960340	32.967847
740.586401	55186.206808	32.972864
740.616242	55275.386656	32.977882
740.750759	55363.229152	32.982900
741.846369	55444.569986	32.987917
742.090406	55541.941788	32.992935
742.646869	55636.937406	32.997952
743.206594	55742.800173	33.002970
743.869270	55843.718317	33.007988
744.580090	55942.746197	33.013005
744.529767	56058.871109	33.018023
745.651549	56160.953438	33.023040
746.271878	56282.143590	33.028058
747.248224	56375.165289	33.033076
748.352139	56488.701136	33.038093
749.020867	56589.748464	33.043111
749.870731	56698.961441	33.048128
750.564226	56820.452415	33.053146
751.295282	56926.072082	33.058164
752.215596	57038.415609	33.063181
752.701232	57144.664598	33.068199
753.857632	57251.391017	33.073216
754.098305	57362.995604	33.078234
755.199344	57480.809040	33.083252
755.657719	57596.922144	33.088269
756.027783	57712.077415	33.093287
757.031139	57827.343610	33.098304
757.725465	57929.107559	33.103322
758.837630	58032.338516	33.108340
760.014215	58153.264992	33.113357
760.745749	58263.024264	33.118375
761.840647	58357.002481	33.123392
762.686697	58466.838749	33.128410
763.663766	58564.995323	33.133428
764.188982	58660.996362	33.138445
765.020864	58762.779764	33.143463
766.348777	58860.165791	33.148480
767.105317	58948.692374	33.153498
767.834884	59047.593621	33.158516
768.482756	59122.571583	33.163533
768.959570	59221.673409	33.168551
769.616913	59317.598905	33.173568
770.358072	59416.203050	33.178586
770.952674	59516.816160	33.183604
771.731035	59621.980985	33.188621
772.410741	59727.478623	33.193639
773.763781	59819.948660	33.198656
774.635950	59918.261901	33.203674
775.015023	60030.547345	33.208692
776.109687	60118.012129	33.213709
776.555428	60219.519116	33.218727
777.390090	60307.135090	33.223744
778.059082	60386.746555	33.228762
778.197960	60496.957187	33.233780
778.845464	60589.648388	33.238797
779.323707	60693.825624	33.243815
780.227858	60800.903351	33.248832
780.654835	60906.587932	33.253850
781.469945	61027.218560	33.258868
782.211694	61133.642326	33.263885
782.914113	61257.983738	33.268903
783.772790	61372.030209	33.273920
784.641209	61488.414105	33.278938
785.108013	61600.371463	33.283956
785.925800	61718.420881	33.288973
786.851704	61855.046818	33.293991
788.028357	61984.351479	33.299008
788.621533	62092.030913	33.304026
789.359670	62219.955850	33.309044
790.464144	62331.685531	33.314061
791.215029	62448.454588	33.319079
792.613798	62562.930499	33.324096
793.582440	62663.295242	33.329114
794.049972	62779.145973	33.334132
795.078402	62877.738513	33.339149
795.638703	63000.135759	33.344167
796.466472	63100.595440	33.349184
797.535867	63230.576731	33.354202
797.679483	63343.551432	33.359220
798.931131	63472.277975	33.364237
799.426309	63587.477698	33.369255
800.130136	63691.127377	33.374272
800.770518	63823.351259	33.379290
801.451586	63935.779058	33.384308
802.324558	64055.646929	33.389325
802.963488	64187.690093	33.394343
804.202039	64305.343655	33.399360
805.521063	64417.523363	33.404378
805.971737	64538.854379	33.409396
806.970900	64662.908359	33.414413
807.851689	64787.753794	33.419431
808.198713	64895.716170	33.424448
809.368133	65023.941368	33.429466
809.997145	65152.212353	33.434484
810.932232	65273.562511	33.439501
811.083995	65408.721765	33.444519
811.798455	65537.878638	33.449536
812.479630	65669.393322	33.454554
813.084136	65818.684363	33.459572
814.306845	65939.864503	33.464589
814.842678	66079.168396	33.469607
815.997062	66208.054513	33.474624
817.308643	66319.531455	33.479642
818.305627	66447.484187	33.484660
819.268054	66571.580956	33.489677
820.189357	66699.370732	33.494695
820.956852	66815.491712	33.499712
821.897134	66934.669768	33.504730
822.524807	67056.909247	33.509748
823.732131	67166.694767	33.514765
824.359215	67295.270097	33.519783
824.759396	67421.639451	33.524800
825.703635	67540.769738	33.529818
825.963430	67671.064346	33.534836
827.159216	67779.204982	33.539853
827.640274	67913.719200	33.544871
828.812799	68050.414978	33.549888
829.627388	68162.666608	33.554906
829.966638	68289.683455	33.559924
830.874092	68423.865004	33.564941
831.749074	68547.507455	33.569959
832.623274	68665.315402	33.574976
834.092216	68767.833555	33.579994
835.079762	68886.458553	33.585012
836.118659	68987.038317	33.590029
836.902377	69104.907920	33.595047
837.650727	69216.942187	33.600064
838.533201	69315.715872	33.605082
838.951001	69445.489585	33.610100
840.252547	69555.063397	33.615117
840.533213	69668.960213	33.620135
841.435411	69784.525310	33.625152
842.455655	69897.618401	33.630170
843.167982	70032.164846	33.635188
844.396992	70147.052021	33.640205
844.562527	70271.327518	33.645223
845.552445	70402.922059	33.650240
846.312494	70520.626416	33.655258
847.130734	70654.014899	33.660276
847.698223	70784.537135	33.665293
848.436026	70919.028082	33.670311
849.178950	71049.921314	33.675328
850.324027	71188.684204	33.680346
851.178643	71329.784870	33.685364
851.897051	71469.884634	33.690381
852.732623	71595.916173	33.695399
853.433503	71742.773625	33.700416
854.850869	71869.102736	33.705434
855.590582	72012.901562	33.710452
856.347401	72153.954256	33.715469
857.520853	72286.080219	33.720487
858.075679	72426.428239	33.725504
859.578982	72544.526875	33.730522
860.281749	72680.590211	33.735540
860.922173	72807.419895	33.740557
862.062168	72945.556340	33.745575
863.033698	73083.462225	33.750592
863.947976	73200.112473	33.755610
864.577538	73339.910283	33.760628
866.220678	73449.959891	33.765645
867.556725	73571.854315	33.770663
868.315727	73687.805622	33.775680
869.068007	73802.923933	33.780698
869.909779	73946.396305	33.785716
870.413352	74061.411612	33.790733
871.892865	74169.563158	33.795751
872.737878	74284.662393	33.800768
873.449311	74405.456800	33.805786
874.247897	74551.602652	33.810804
875.281214	74639.321806	33.815821
876.514768	74761.309412	33.820839
877.331504	74888.451024	33.825856
878.186346	74986.787433	33.830874
878.709895	75117.602464	33.835892
879.280742	75233.966216	33.840909
879.852161	75357.615899	33.845927
880.359951	75491.066611	33.850944
881.432536	75620.984506	33.855962
881.863675	75760.799033	33.860980
882.671979	75891.015140	33.865997
883.586485	76041.863431	33.871015
883.933429	76201.869313	33.876032
885.166189	76334.440207	33.881050
885.902137	76477.314262	33.886068
886.373561	76627.385936	33.891085
887.517036	76778.290023	33.896103
888.446748	76918.611456	33.901120
889.673667	77053.698515	33.906138
890.166597	77178.237890	33.911156
890.929854	77317.969534	33.916173
891.540560	77464.791990	33.921191
892.337857	77618.162389	33.926208
892.978781	77756.765896	33.931226
893.685063	77912.050808	33.936244
894.438597	78057.594964	33.941261
895.656394	78221.601866	33.946279
896.648473	78380.821272	33.951296
897.743197	78537.311424	33.956314
898.635989	78694.999839	33.961332
899.064081	78847.668040	33.966349
900.466321	78991.985330	33.971367
901.239646	79165.294698	33.976384
902.121252	79323.343620	33.981402
903.107742	79474.317290	33.986420
903.821205	79643.414942	33.991437
904.410479	79808.732807	33.996455
905.496542	79974.602408	34.001472
906.449950	80130.026436	34.006490
907.093009	80307.370202	34.011508
907.854486	80475.833650	34.016525
908.831207	80654.617905	34.021543
910.107348	80833.822243	34.026560
911.426799	80992.335668	34.031578
912.485209	81170.617125	34.036596
913.242168	81336.861082	34.041613
914.420927	81497.286388	34.046631
915.388327	81660.372992	34.051648
916.884929	81806.286940	34.056666
917.974206	81956.722598	34.061684
919.164942	82105.611597	34.066701
920.256638	82247.293528	34.071719
921.226779	82405.166015	34.076736
922.215884	82537.674822	34.081754
923.037602	82694.112478	34.086772
923.817967	82832.173929	34.091789
925.381949	82969.157887	34.096807
926.526542	83112.443355	34.101824
927.359242	83240.452423	34.106842
928.348664	83368.866528	34.111860
929.435813	83502.674326	34.116877
930.382528	83652.176790	34.121895
930.994552	83792.796115	34.126912
931.553142	83930.457968	34.131930
932.348194	84081.025828	34.136948
933.420428	84227.727618	34.141965
933.954516	84380.308116	34.146983
934.707118	84529.993866	34.152000
935.498613	84679.585595	34.157018
936.447158	84836.289004	34.162036
937.634357	84983.413183	34.167053
938.447698	85131.580698	34.172071
938.844563	85284.930090	34.177088
939.996510	85451.765151	34.182106
940.937426	85618.636260	34.187124
941.762806	85793.354234	34.192141
942.864128	85939.094069	34.197159
943.594514	86104.769653	34.202176
944.580967	86274.940744	34.207194
945.103502	86429.270328	34.212212
946.059616	86603.700743	34.217229
947.636186	86762.895032	34.222247
948.409314	86929.075618	34.227264
949.460233	87092.269269	34.232282
950.445612	87258.853750	34.237300
951.139144	87417.280822	34.242317
952.211771	87560.884194	34.247335
952.796437	87720.084269	34.252352
953.873157	87875.249409	34.257370
954.844915	88026.547713	34.262388
955.656724	88183.745524	34.267405
956.697797	88351.866217	34.272423
957.304598	88524.242496	34.277440
958.059310	88682.117484	34.282458
959.188447	88847.778300	34.287476
960.210433	89007.446427	34.292493
961.597944	89169.213126	34.297511
962.394814	89334.236138	34.302528
963.701860	89494.518607	34.307546
965.054258	89651.497728	34.312564
965.765324	89811.292228	34.317581
967.285094	89957.576476	34.322599
968.103224	90113.779907	34.327616
968.854202	90266.369349	34.332634
969.911482	90440.140707	34.337652
970.897086	90606.122292	34.342669
971.786228	90763.330799	34.347687
972.346870	90934.118479	34.352704
973.298475	91101.912734	34.357722
974.398582	91259.773155	34.362740
974.817464	91437.498599	34.367757
975.826009	91613.545846	34.372775
976.840686	91801.579892	34.377792
978.112557	91974.421970	34.382810
978.624879	92161.858275	34.387828
979.390330	92352.728771	34.392845
980.571315	92536.190677	34.397863
981.340348	92722.291537	34.402880
982.403067	92900.598681	34.407898
983.279293	93079.089828	34.412916
984.769640	93273.430142	34.417933
985.937628	93449.787260	34.422951
987.039294	93638.536449	34.427968
987.968478	93803.675989	34.432986
988.858448	94003.773260	34.438004
989.667211	94192.594099	34.443021
991.370164	94373.857093	34.448039
992.343576	94554.064617	34.453056
993.014249	94721.386067	34.458074
993.992709	94910.273053	34.463092
995.048671	95085.850339	34.468109
996.146925	95259.409094	34.473127
997.171290	95435.228295	34.478144
998.170570	95616.122966	34.483162
999.338033	95797.921670	34.488180
1000.048397	95977.284268	34.493197
1001.353402	96165.006627	34.498215
1002.376261	96341.566813	34.503232
1003.572970	96525.803056	34.508250
1004.326510	96704.391562	34.513268
1005.121715	96874.232749	34.518285
1006.487511	97068.275604	34.523303
1007.151868	97253.111555	34.528320
1008.116524	97437.316930	34.533338
1009.006853	97618.839281	34.538356
1009.829375	97804.748343	34.543373
1011.053206	97990.370975	34.548391
1011.872813	98186.633377	34.553408
1012.626883	98365.290699	34.558426
1013.995696	98563.668360	34.563444
1015.097170	98756.084110	34.568461
1016.508620	98925.881855	34.573479
1017.499898	99115.273577	34.578496
1018.950035	99283.269475	34.583514
1019.870107	99455.019456	34.588532
1020.551691	99616.896117	34.593549
1021.521682	99785.962231	34.598567
1022.639668	99961.285175	34.603584
1023.555500	100132.299769	34.608602
1024.557904	100292.114594	34.613620
1025.852993	100457.453300	34.618637
1027.173647	100617.825407	34.623655
1028.895700	100755.138144	34.628672
1030.755969	100909.554195	34.633690
1031.988755	101057.085302	34.638708
1032.801072	101191.163482	34.643725
1033.930943	101346.532150	34.648743
1035.151308	101486.369152	34.653760
1036.127562	101631.058932	34.658778
1037.391166	101775.632448	34.663796
1038.120556	101918.471575	34.668813
1039.204389	102053.598443	34.673831
1040.067816	102203.077558	34.678848
1040.554105	102353.075667	34.683866
1041.475543	102500.894454	34.688884
1042.382405	102661.847920	34.693901
1043.381203	102828.282948	34.698919
1043.480653	103000.375963	34.703936
1044.031084	103173.345409	34.708954
1045.305563	103351.616342	34.713972
1046.158353	103537.587780	34.718989
1047.397130	103721.831592	34.724007
1048.427994	103911.404389	34.729024
1049.092692	104107.719077	34.734042
1050.405922	104291.175837	34.739060
1051.137731	104498.284533	34.744077
1052.074173	104678.507316	34.749095
1052.866123	104878.656639	34.754112
1054.073227	105079.783746	34.759130
1055.233931	105280.837747	34.764148
1056.230758	105485.276382	34.769165
1057.530898	105668.669017	34.774183
1059.513230	105865.222662	34.779200
1060.819274	106047.071908	34.784218
1062.268390	106213.106001	34.789236
1063.395512	106408.348472	34.794253
1064.402003	106583.031991	34.799271
1065.600080	106757.026465	34.804288
1066.593019	106940.909303	34.809306
1067.382216	107125.358990	34.814324
1068.492941	107309.668225	34.819341
1069.146156	107500.817512	34.824359
1070.052423	107685.505077	34.829376
1070.823321	107872.432722	34.834394
1072.002172	108065.880399	34.839412
1072.597793	108263.681410	34.844429
1073.738229	108462.077893	34.849447
1074.866415	108659.527939	34.854464
1075.930862	108858.687196	34.859482
1077.059970	109056.368006	34.864500
1078.381249	109276.019531	34.869517
1079.436509	109464.177980	34.874535
1080.697682	109665.008018	34.879552
1081.803164	109870.703809	34.884570
1082.946695	110055.723231	34.889588
1083.708804	110250.319464	34.894605
1085.425014	110435.398947	34.899623
1086.851176	110633.384302	34.904640
1087.993756	110819.105780	34.909658
1089.132615	110994.796965	34.914676
1090.140087	111180.277216	34.919693
1091.280633	111347.838209	34.924711
1092.854261	111520.737605	34.929728
1093.424105	111691.333704	34.934746
1094.759294	111855.255530	34.939764
1096.018349	112011.653829	34.944781
1096.986557	112166.606280	34.949799
1097.966679	112336.163282	34.954816
1098.671247	112516.774963	34.959834
1100.314120	112689.214293	34.964852
1101.324680	112851.092844	34.969869
1102.390960	113016.573480	34.974887
1103.650524	113189.902641	34.979904
1104.332480	113373.614654	34.984922
1105.535258	113544.193796	34.989940
1106.466690	113728.880434	34.994957
1107.756098	113908.416578	34.999975
1109.047488	114093.768318	35.004992
1109.539693	114271.360815	35.010010
1110.839137	114452.697742	35.015028
1112.002892	114646.954857	35.020045
1112.812756	114836.178947	35.025063
1113.975727	115018.846965	35.030080
1114.707918	115224.150480	35.035098
1115.573309	115432.334698	35.040116
1116.496532	115629.881608	35.045133
1117.297753	115836.723839	35.050151
1118.533731	116051.591447	35.055168
1119.401682	116266.977547	35.060186
1120.764561	116487.414699	35.065204
1121.565866	116698.811571	35.070221
1122.409553	116921.060872	35.075239
1123.855820	117135.876689	35.080256
1124.639747	117369.149340	35.085274
1126.090284	117590.974303	35.090292
1126.888603	117823.108015	35.095309
1128.132047	118045.680232	35.100327
1129.355169	118276.011705	35.105344
1130.626742	118509.935404	35.110362
1131.920374	118733.024177	35.115380
1132.885229	118968.978844	35.120397
1133.977997	119193.764197	35.125415
1135.441208	119430.463976	35.130432
1136.485024	119661.583752	35.135450
1137.704485	119875.646679	35.140468
1138.922606	120107.121376	35.145485
1140.180408	120345.877264	35.150503
1141.385955	120559.301321	35.155520
1142.443756	120800.514168	35.160538
1143.511578	121022.555514	35.165556
1145.006007	121251.003269	35.170573
1145.987668	121477.484661	35.175591
1147.523411	121692.357765	35.180608
1148.664892	121919.867951	35.185626
1150.062750	122142.965778	35.190644
1151.271816	122365.272786	35.195661
1152.243082	122593.006367	35.200679
1154.048128	122797.743457	35.205696
1154.693995	123023.405153	35.210714
1155.906382	123231.297103	35.215732
1157.065828	123458.106554	35.220749
1158.252246	123692.250698	35.225767
1159.814243	123886.593261	35.230784
1160.734944	124104.905706	35.235802
1161.884567	124331.292571	35.240820
1162.913473	124547.689470	35.245837
1163.687121	124764.396207	35.250855
1166.154201	124956.277176	35.255872
1167.073671	125156.348255	35.260890
1168.186152	125356.160688	35.265908
1169.668371	125549.868230	35.270925
1170.493023	125751.631804	35.275943
1172.209586	125946.367780	35.280960
1172.696960	126131.333804	35.285978
1173.820259	126322.507470	35.290996
1175.160696	126512.265061	35.296013
1176.069423	126715.415299	35.301031
1177.305160	126907.258478	35.306048
1178.443966	127104.771470	35.311066
1179.725659	127314.594034	35.316084
1181.251191	127507.216972	35.321101
1182.208902	127704.256773	35.326119
1183.881271	127884.665232	35.331136
1185.165938	128099.980677	35.336154
1186.348615	128290.358397	35.341172
1187.675993	128481.664004	35.346189
1188.934718	128673.413070	35.351207
1189.995178	128864.080682	35.356224
1190.481706	129077.012442	35.361242
1191.830579	129271.995096	35.366260
1193.145471	129479.253959	35.371277
1193.716196	129705.700338	35.376295
1195.102700	129912.405244	35.381312
1195.914437	130133.009731	35.386330
1196.995959	130342.125426	35.391348
1198.869805	130557.626893	35.396365
1199.956086	130769.013558	35.401383
1201.145269	130980.625499	35.406400
1202.039863	131200.006977	35.411418
1202.748022	131430.613456	35.416436
1204.261433	131648.374820	35.421453
1205.235952	131871.271665	35.426471
1206.672163	132095.551615	35.431488
1207.776245	132328.900700	35.436506
1209.234273	132554.752139	35.441524
1210.553487	132787.574712	35.446541
1211.378746	133015.219819	35.451559
1212.996347	133248.047209	35.456576
1214.181165	133483.736583	35.461594
1215.545206	133699.635177	35.466612
1217.069696	133917.790557	35.471629
1217.704315	134161.777593	35.476647
1219.198457	134384.631585	35.481664
1219.889633	134637.271235	35.486682
1220.811532	134877.768112	35.491700
1221.930800	135124.154460	35.496717
1222.799030	135380.168175	35.501735
1224.190320	135623.775110	35.506752
1225.102853	135879.950249	35.511770
1226.352506	136132.395242	35.516788
1227.429272	136392.160409	35.521805
1228.778119	136653.378706	35.526823
1230.523317	136906.191588	35.531840
1231.101603	137167.249568	35.536858
1232.022079	137416.589262	35.541876
1233.454830	137689.770069	35.546893
1234.936976	137953.639087	35.551911
1236.141600	138221.752570	35.556928
1237.140450	138501.350887	35.561946
1238.875694	138760.113116	35.566964
1240.039761	139020.695936	35.571981
1240.836189	139294.869774	35.576999
1242.288378	139549.310628	35.582016
1243.309940	139816.351362	35.587034
1244.700571	140087.859739	35.592052
1246.564152	140346.765157	35.597069
1247.404351	140605.296266	35.602087
1248.872611	140859.997927	35.607104
1250.218143	141107.177447	35.612122
1252.109538	141336.542586	35.617140
1253.897666	141561.906855	35.622157
1255.399258	141791.035076	35.627175
1256.805084	142004.939467	35.632192
1258.185829	142235.561467	35.637210
1259.549894	142452.391919	35.642228
1260.811569	142658.741529	35.647245
1262.149116	142882.147343	35.652263
1263.817389	143092.096996	35.657280
1265.078678	143317.990856	35.662298
1265.971479	143541.854742	35.667316
1267.769923	143747.678426	35.672333
1269.234942	143953.139903	35.677351
1270.707176	144163.229828	35.682368
1271.728134	144386.494673	35.687386
1272.953332	144607.102305	35.692404
1274.458742	144818.889913	35.697421
1274.943371	145031.367202	35.702439
1276.277610	145251.174657	35.707456
1277.146205	145482.029491	35.712474
1278.216609	145710.392370	35.717492
1279.066505	145950.853003	35.722509
1279.718168	146197.853518	35.727527
1280.857792	146447.133954	35.732544
1282.223741	146699.409661	35.737562
1283.207134	146960.817654	35.742580
1284.748833	147226.574005	35.747597
1285.282453	147504.914210	35.752615
1286.616476	147771.583909	35.757632
1287.880848	148042.147768	35.762650
1288.934340	148313.407926	35.767668
1290.408879	148596.103371	35.772685
1291.532113	148872.758811	35.777703
1293.484504	149144.307995	35.782720
1295.083637	149414.864858	35.787738
1296.646906	149678.581045	35.792756
1298.225202	149933.494876	35.797773
1299.330708	150207.626787	35.802791
1300.826903	150472.577278	35.807808
1301.460587	150749.073992	35.812826
1303.275800	151014.762048	35.817844
1305.451140	151261.050802	35.822861
1306.692026	151535.893122	35.827879
1308.145554	151786.451892	35.832896
1309.545155	152043.426349	35.837914
1311.201715	152287.017144	35.842932
1312.977432	152526.201343	35.847949
1314.102729	152784.469124	35.852967
1315.268219	153037.138515	35.857984
1316.335054	153283.699597	35.863002
1317.693113	153529.706857	35.868020
1319.165663	153778.056029	35.873037
1319.777209	154049.139222	35.878055
1321.643535	154294.623583	35.883072
1322.719448	154531.513233	35.888090
1324.593774	154780.157750	35.893108
1326.031973	155013.515077	35.898125
1328.226968	155242.550354	35.903143
1329.749055	155478.509641	35.908160
1330.969229	155709.903000	35.913178
1331.733705	155959.144184	35.918196
1333.206186	156193.073764	35.923213
1334.095008	156432.466763	35.928231
1335.611238	156682.362262	35.933248
1336.113741	156926.946748	35.938266
1336.988019	157165.648944	35.943284
1337.991181	157413.743696	35.948301
1339.024648	157671.386983	35.953319
1340.158552	157919.666291	35.958336
1341.002501	158175.834581	35.963354
1342.097433	158438.952793	35.968372
1343.202220	158716.963967	35.973389
1344.238482	158994.316041	35.978407
1345.774275	159274.365763	35.983424
1347.209381	159555.372804	35.988442
1348.359427	159841.807680	35.993460
1349.780749	160122.744826	35.998477
1351.164772	160404.438551	36.003495
1352.384412	160704.010823	36.008512
1354.203671	160978.735397	36.013530
1355.373243	161266.052424	36.018548
1356.631876	161552.443338	36.023565
1357.851810	161857.174685	36.028583
1359.003421	162144.183637	36.033600
1360.561179	162445.780712	36.038618
1361.802709	162757.277140	36.043636
1363.580881	163042.425417	36.048653
1364.581809	163356.084735	36.053671
1366.212760	163652.514837	36.058688
1367.387651	163959.742968	36.063706
1368.925128	164275.781899	36.068724
1370.400431	164587.304058	36.073741
1371.560165	164886.776742	36.078759
1373.327462	165199.409749	36.083776
1375.285234	165495.278602	36.088794
1376.492496	165809.048876	36.093812
1377.941479	166099.093375	36.098829
1379.010111	166415.263561	36.103847
1380.691807	166718.507302	36.108864
1382.416588	167009.083337	36.113882
1383.468717	167326.747382	36.118900
1384.868039	167625.615861	36.123917
1385.973287	167940.420727	36.128935
1387.827507	168243.633879	36.133952
1389.010084	168558.506523	36.138970
1389.890898	168861.668854	36.143988
1391.813849	169180.826670	36.149005
1393.360861	169487.804123	36.154023
1394.806550	169809.405309	36.159040
1396.145333	170110.153074	36.164058
1397.017031	170433.135030	36.169076
1398.786827	170754.258034	36.174093
1399.996276	171071.935487	36.179111
1401.767776	171378.990252	36.184128
1403.337950	171702.754195	36.189146
1404.305857	172019.374110	36.194164
1405.847164	172331.041454	36.199181
1407.056439	172639.060311	36.204199
1408.444262	172974.322041	36.209216
1410.008747	173295.357081	36.214234
1410.968155	173635.034189	36.219252
1412.505551	173950.418474	36.224269
1414.303782	174269.809969	36.229287
1415.502874	174594.175538	36.234304
1417.194117	174904.794663	36.239322
1418.668071	175223.002442	36.244340
1420.357527	175539.032087	36.249357
1421.676528	175868.856112	36.254375
1422.956364	176199.589892	36.259392
1424.667512	176498.147259	36.264410
1426.371899	176828.307636	36.269428
1427.657792	177141.914270	36.274445
1429.155085	177454.358531	36.279463
1430.717961	177761.273357	36.284480
1432.499148	178044.942031	36.289498
1433.788761	178335.521312	36.294516
1435.827685	178620.039127	36.299533
1437.337068	178894.251767	36.304551
1438.567790	179182.155145	36.309568
1440.098678	179453.499044	36.314586
1441.118001	179746.923258	36.319604
1442.672091	180035.679251	36.324621
1444.195757	180316.509611	36.329639
1445.672696	180605.776554	36.334656
1447.015493	180889.736709	36.339674
1448.536273	181177.578167	36.344692
1449.849221	181458.931867	36.349709
1451.240083	181753.448571	36.354727
1452.047312	182060.577683	36.359744
1453.972659	182340.667433	36.364762
1455.025564	182659.398257	36.369780
1456.661072	182966.573699	36.374797
1457.997338	183267.809505	36.379815
1459.137285	183577.811847	36.384832
1461.053923	183887.281664	36.389850
1462.504918	184212.442052	36.394868
1463.941073	184503.488891	36.399885
1465.371332	184820.253825	36.404903
1466.450722	185137.814708	36.409920
1468.079318	185451.415479	36.414938
1470.174239	185764.674551	36.419956
1471.601341	186077.258659	36.424973
1473.390148	186379.516114	36.429991
1474.631739	186698.125526	36.435008
1476.150176	187009.785945	36.440026
1477.671540	187336.044981	36.445044
1479.802784	187650.146529	36.450061
1481.414065	187945.701600	36.455079
1483.063932	188250.276975	36.460096
1484.279519	188555.001822	36.465114
1485.928318	188868.466239	36.470132
1487.149720	189167.709734	36.475149
1488.200786	189489.552534	36.480167
1489.680194	189807.873706	36.485184
1490.966499	190132.359690	36.490202
1492.170737	190460.326506	36.495220
1493.664970	190783.766288	36.500237
1495.462900	191115.700929	36.505255
1496.639882	191436.416634	36.510272
1497.794110	191770.606514	36.515290
1499.123271	192111.218162	36.520308
1500.835014	192446.462330	36.525325
1502.388433	192785.136635	36.530343
1504.060020	193109.968909	36.535360
1505.561394	193447.094076	36.540378
1506.544517	193789.321058	36.545396
1508.182189	194127.671577	36.550413
1509.690592	194490.076726	36.555431
1511.126013	194833.364722	36.560448
1512.944729	195178.114766	36.565466
1514.245255	195539.798634	36.570484
1516.065726	195867.350307	36.575501
1517.894285	196205.147406	36.580519
1519.449662	196551.179860	36.585536
1521.533093	196880.508797	36.590554
1522.916171	197221.139682	36.595572
1523.939874	197546.292362	36.600589
1525.907268	197869.653218	36.605607
1527.369116	198201.643265	36.610624
1528.670461	198534.461308	36.615642
1530.108047	198876.780374	36.620660
1531.221669	199216.056884	36.625677
1532.661690	199538.522679	36.630695
1534.246148	199865.943005	36.635712
1535.949019	200194.830818	36.640730
1536.939939	200531.379181	36.645748
1538.309290	200858.789019	36.650765
1539.843861	201191.365904	36.655783
1541.246081	201536.180042	36.660800
1542.996896	201873.117435	36.665818
1544.162203	202214.012776	36.670836
1545.767189	202557.313030	36.675853
1547.885784	202895.502386	36.680871
1548.991859	203246.607793	36.685888
1550.465950	203598.784201	36.690906
1552.120096	203953.814775	36.695924
1553.761330	204303.643553	36.700941
1555.718527	204648.787537	36.705959
1557.225244	205002.196973	36.710976
1558.937274	205340.426777	36.715994
1560.351973	205700.419056	36.721012
1562.328751	206059.850534	36.726029
1563.821063	206408.152117	36.731047
1565.115192	206762.074767	36.736064
1566.639958	207116.303832	36.741082
1568.254600	207476.512831	36.746100
1569.336294	207832.481657	36.751117
1570.694939	208198.602439	36.756135
1572.079454	208580.363960	36.761152
1574.089265	208949.148848	36.766170
1576.230211	209312.225292	36.771188
1577.717229	209679.296774	36.776205
1579.328532	210043.962253	36.781223
1581.013158	210420.197640	36.786240
1583.228324	210776.602099	36.791258
1584.656765	211134.623572	36.796276
1586.157113	211503.872401	36.801293
1587.892734	211859.154346	36.806311
1589.457562	212219.291232	36.811328
1591.600549	212591.829180	36.816346
1593.138191	212958.627490	36.821364
1594.696100	213313.767067	36.826381
1596.368604	213664.749559	36.831399
1598.039154	214006.844970	36.836416
1599.603123	214366.533825	36.841434
1601.391725	214730.174375	36.846452
1603.485687	215083.429473	36.851469
1605.473338	215414.227141	36.856487
1607.206347	215763.557129	36.861504
1609.216407	216096.842498	36.866522
1610.860972	216434.710101	36.871540
1612.020797	216779.363829	36.876557
1613.618879	217115.463754	36.881575
1615.225370	217458.598618	36.886592
1616.292469	217809.341432	36.891610
1618.016486	218227.332016	36.896628
1619.177366	218573.134969	36.901645
1621.300823	218900.163621	36.906663
1622.475306	219258.716523	36.911680
1624.749932	219609.825331	36.916698
1626.312258	219958.817858	36.921716
1627.847795	220296.564563	36.926733
1629.904045	220637.706052	36.931751
1631.302597	220991.504043	36.936768
1632.810867	221332.433468	36.941786
1633.992369	221682.917015	36.946804
1635.388209	222047.234069	36.951821
1636.713392	222398.356644	36.956839
1637.863005	222772.723932	36.961856
1639.483839	223137.032958	36.966874
1641.311476	223484.545688	36.971892
1642.135472	223828.516834	36.976909
1644.021797	224181.584475	36.981927
1645.257447	224536.335341	36.986944
1647.378106	224905.774531	36.991962
1649.022353	225260.155432	36.996980
1650.240273	225624.335784	37.001997
1651.858721	225984.133244	37.007015
1653.409844	226372.415973	37.012032
1655.011175	226745.197805	37.017050
1656.381977	227120.406407	37.022068
1657.442472	227519.898902	37.027085
1659.584526	227890.207404	37.032103
1661.340016	228286.488879	37.037120
1662.438866	228676.834691	37.042138
1663.975117	229084.305492	37.047156
1665.211979	229496.449825	37.052173
1667.367765	229908.291425	37.057191
1668.772567	230330.392999	37.062208
1670.175416	230752.267603	37.067226
1672.020971	231168.736319	37.072244
1673.353422	231598.550116	37.077261
1675.259794	232022.199732	37.082279
1677.008673	232447.121225	37.087296
1678.443123	232888.631854	37.092314
1679.942055	233324.341723	37.097332
1681.538675	233782.567512	37.102349
1683.245212	234221.497041	37.107367
1684.971930	234677.748128	37.112384
1686.649399	235108.099307	37.117402
1688.870151	235551.088092	37.122420
1690.358912	236003.114756	37.127437
1693.080554	236434.541805	37.132455
1695.338583	236867.468929	37.137472
1697.073526	237298.883135	37.142490
1699.825518	237722.027448	37.147508
1701.698497	238145.749616	37.152525
1703.895529	238553.390747	37.157543
1705.956457	238945.687089	37.162560
1707.328674	239353.212017	37.167578
1709.418996	239746.673636	37.172596
1710.888277	240148.240143	37.177613
1712.560960	240550.104120	37.182631
1714.281899	240940.174332	37.187648
1716.107608	241339.423572	37.192666
1717.799451	241738.060589	37.197684
1719.325326	242153.389605	37.202701
1721.010870	242562.596494	37.207719
1722.674072	242969.216760	37.212736
1724.046826	243379.569001	37.217754
1726.039265	243787.965328	37.222772
1727.185440	244204.427532	37.227789
1728.560003	244617.575818	37.232807
1730.179521	245038.228915	37.237824
1731.797211	245465.538465	37.242842
1733.612199	245883.239332	37.247860
1734.853028	246331.772804	37.252877
1737.211124	246750.934903	37.257895
1739.141455	247177.001509	37.262912
1740.885477	247606.325596	37.267930
1742.817835	248013.772756	37.272948
1744.696812	248462.331059	37.277965
1746.186451	248877.879615	37.282983
1747.946116	249294.730465	37.288000
1749.904977	249708.652988	37.293018
1751.941913	250137.779466	37.298036
1753.756911	250557.239074	37.303053
1756.153203	250952.394117	37.308071
1757.886138	251340.876349	37.313088
1759.568687	251730.484964	37.318106
1761.309682	252116.222990	37.323124
1762.809961	252517.700156	37.328141
1764.310751	252916.179981	37.333159
1765.925276	253298.891379	37.338176
1767.254840	253695.621789	37.343194
1769.051906	254092.580168	37.348212
1770.662459	254508.596559	37.353229
1771.941384	254920.654204	37.358247
1773.575911	255331.459460	37.363264
1774.821721	255766.893990	37.368282
1776.472002	256192.176916	37.373300
1777.964654	256652.085282	37.378317
1779.304228	257097.767859	37.383335
1780.932795	257535.223064	37.388352
1782.383351	257995.545331	37.393370
1784.537209	258444.828278	37.398388
1786.561692	258918.240400	37.403405
1788.215876	259379.342285	37.408423
1790.033534	259843.897510	37.413440
1791.776584	260329.067157	37.418458
1793.509048	260797.040516	37.423476
1795.345158	261278.714542	37.428493
1796.932121	261757.889292	37.433511
1798.843087	262243.844003	37.438528
1800.376479	262740.555685	37.443546
1802.603145	263221.656851	37.448564
1804.562290	263714.589113	37.453581
1806.012655	264196.707114	37.458599
1808.109185	264693.833236	37.463616
1809.780610	265192.807457	37.468634
1811.633031	265677.805159	37.473652
1813.307018	266191.817054	37.478669
1815.450130	266681.516543	37.483687
1817.103039	267188.596091	37.488704
1819.145465	267704.298830	37.493722
1821.141897	268197.298293	37.498740
1823.144406	268694.919655	37.503757
1824.804226	269196.178882	37.508775
1827.039371	269688.273773	37.513792
1829.050997	270183.631171	37.518810
1831.132132	270685.860725	37.523828
1832.780245	271186.763918	37.528845
1834.935224	271691.190047	37.533863
1836.588898	272179.440331	37.538880
1838.222222	272688.828451	37.543898
1840.041606	273186.423602	37.548916
1842.052748	273685.586719	37.553933
1844.035182	274174.668883	37.558951
1846.341712	274655.161477	37.563968
1847.776971	275169.938138	37.568986
1849.812632	275662.920989	37.574004
1851.458065	276157.313642	37.579021
1853.631315	276651.237244	37.584039
1855.768296	277146.054947	37.589056
1857.546044	277643.623561	37.594074
1859.620214	278120.134502	37.599092
1862.270314	278603.941516	37.604109
1863.737720	279079.331235	37.609127
1866.034987	279566.420437	37.614144
1867.670785	280058.393242	37.619162
1869.369931	280533.055637	37.624180
1870.978188	281020.305902	37.629197
1872.630447	281498.047390	37.634215
1875.201874	281983.993287	37.639232
1876.484237	282473.046388	37.644250
1878.389887	282934.256690	37.649268
1880.250013	283412.416241	37.654285
1881.882111	283881.238931	37.659303
1883.723906	284345.631303	37.664320
1884.965030	284815.760623	37.669338
1886.534061	285288.273065	37.674356
1888.213225	285770.062861	37.679373
1889.981386	286252.750981	37.684391
1891.824467	286755.136565	37.689408
1893.498293	287252.798442	37.694426
1895.849344	287741.659841	37.699444
1897.831205	288233.628650	37.704461
1899.398035	288738.745695	37.709479
1901.751641	289228.312946	37.714496
1903.483541	289734.085066	37.719514
1905.454018	290236.437724	37.724532
1907.051489	290744.895376	37.729549
1908.852373	291265.331923	37.734567
1910.351284	291774.513124	37.739584
1912.042817	292317.214161	37.744602
1914.238988	292828.003402	37.749620
1916.019098	293361.769950	37.754637
1917.846478	293894.332611	37.759655
1920.129434	294435.529901	37.764672
1922.095122	294970.249389	37.769690
1924.151081	295493.039210	37.774708
1926.109545	296033.647724	37.779725
1927.831851	296572.311504	37.784743
1930.198763	297107.945486	37.789760
1932.448686	297658.403807	37.794778
1934.542889	298188.286565	37.799796
1936.826040	298715.900469	37.804813
1938.815906	299247.547724	37.809831
1941.144238	299763.871965	37.814848
1942.933544	300290.035525	37.819866
1945.413489	300815.498302	37.824884
1947.868800	301343.578415	37.829901
1950.294042	301848.497743	37.834919
1952.726141	302346.047978	37.839936
1954.188328	302868.670812	37.844954
1956.405553	303373.032399	37.849972
1958.909746	303862.765844	37.854989
1960.452855	304368.325404	37.860007
1962.608939	304870.860431	37.865024
1964.482656	305377.121853	37.870042
1966.221521	305873.523309	37.875060
1967.926243	306367.743533	37.880077
1969.662853	306888.571388	37.885095
1971.982317	307392.233602	37.890112
1973.672918	307906.332921	37.895130
1975.387072	308412.882626	37.900148
1976.761460	308949.224066	37.905165
1978.212842	309479.251223	37.910183
1980.369253	310009.488858	37.915200
1981.843077	310556.291950	37.920218
1983.727443	311099.265147	37.925236
1985.508581	311647.483113	37.930253
1987.191036	312202.747994	37.935271
1989.332197	312760.218836	37.940288
1991.086543	313324.707620	37.945306
1993.022750	313891.701720	37.950324
1995.214202	314446.511065	37.955341
1997.181756	315023.420692	37.960359
1999.332397	315580.234529	37.965376
2001.347707	316136.990317	37.970394
2003.964498	316691.966696	37.975412
2006.139469	317244.193050	37.980429
2007.640453	317799.979784	37.985447
2010.056813	318352.005407	37.990464
2011.810244	318901.952277	37.995482
2013.772827	319435.888447	38.000500
2015.484530	319962.777426	38.005517
2017.218260	320513.654247	38.010535
2019.287853	321043.472118	38.015552
2020.949764	321600.903034	38.020570
2023.009910	322164.281384	38.025588
2024.917904	322717.777444	38.030605
2026.841410	323288.582949	38.035623
2028.667675	323859.526428	38.040640
2030.196039	324427.898746	38.045658
2032.266627	324990.590690	38.050676
2034.308617	325584.969205	38.055693
2035.847573	326165.612958	38.060711
2037.689153	326759.454755	38.065728
2039.585746	327364.529241	38.070746
2041.589937	327978.745449	38.075764
2043.359637	328594.847474	38.080781
2044.814358	329218.789408	38.085799
2046.905478	329843.559185	38.090816
2048.944582	330493.617398	38.095834
2051.055539	331130.074051	38.100852
2053.203122	331774.286212	38.105869
2055.096913	332418.279103	38.110887
2057.320212	333054.365776	38.115904
2059.987912	333697.657908	38.120922
2062.431548	334335.648434	38.125940
2065.059866	334983.120885	38.130957
2066.940912	335634.059836	38.135975
2069.302191	336268.208165	38.140992
2071.205660	336913.467050	38.146010
2073.328557	337562.540429	38.151028
2075.729921	338202.700724	38.156045
2077.944575	338836.309493	38.161063
2080.678161	339468.327307	38.166080
2082.955252	340108.763860	38.171098
2085.184080	340731.736683	38.176116
2087.485776	341359.893348	38.181133
2089.649625	341986.694255	38.186151
2091.856917	342601.169720	38.191168
2093.791171	343232.257047	38.196186
2095.951095	343865.380365	38.201204
2097.938676	344483.066672	38.206221
2099.603185	345118.996581	38.211239
2101.686199	345748.529282	38.216256
2104.143537	346401.037295	38.221274
2105.756727	347045.579337	38.226292
2108.065438	347679.160744	38.231309
2110.383010	348317.960231	38.236327
2113.062782	348954.127912	38.241344
2115.235950	349578.899231	38.246362
2117.617169	350194.593044	38.251380
2120.111693	350803.763078	38.256397
2123.239196	351411.805388	38.261415
2126.172445	352002.183552	38.266432
2128.091699	352598.151767	38.271450
2130.390201	353204.885187	38.276468
2132.712600	353777.906695	38.281485
2134.553116	354355.466306	38.286503
2136.971453	354931.958665	38.291520
2139.512842	355514.284691	38.296538
2141.157053	356088.123317	38.301556
2143.430695	356663.347504	38.306573
2145.553044	357235.569302	38.311591
2147.508630	357804.816712	38.316608
2149.761730	358386.085083	38.321626
2151.800288	358968.750860	38.326644
2153.788255	359527.058922	38.331661
2155.605673	360089.117274	38.336679
2157.535025	360636.915706	38.341696
2159.401799	361202.375800	38.346714
2161.143593	361759.805872	38.351732
2163.111222	362329.267574	38.356749
2164.708702	362914.156818	38.361767
2166.639590	363488.555293	38.366784
2168.471352	364080.517735	38.371802
2170.485560	364670.132548	38.376820
2172.381610	365274.243716	38.381837
2174.047317	365891.676686	38.386855
2175.767336	366497.091618	38.391872
2177.939935	367128.322999	38.396890
2179.578228	367784.086292	38.401908
2181.441260	368428.081624	38.406925
2183.302379	369083.760272	38.411943
2185.177713	369751.905244	38.416960
2187.081483	370426.704714	38.421978
2188.797286	371109.791939	38.426996
2190.887757	371792.982249	38.432013
2193.031502	372514.197367	38.437031
2195.383425	373211.521930	38.442048
2198.009388	373918.476587	38.447066
2200.169123	374634.523329	38.452084
2202.903617	375338.591383	38.457101
2205.141004	376055.103937	38.462119
2207.902179	376766.164317	38.467136
2210.511901	377473.304313	38.472154
2212.548610	378172.409164	38.477172
2215.193974	378884.535808	38.482189
2217.285528	379605.868301	38.487207
2219.337885	380313.346232	38.492224
2221.830299	381018.911069	38.497242
2224.272042	381731.848548	38.502260
2226.689782	382443.405554	38.507277
2228.481449	383158.473739	38.512295
2230.946329	383866.873664	38.517312
2233.619851	384581.816346	38.522330
2235.617510	385305.374089	38.527348
2237.718688	386025.196975	38.532365
2239.458460	386760.301007	38.537383
2241.996361	387482.453343	38.542400
2244.191090	388209.310837	38.547418
2246.496318	388938.922222	38.552436
2248.665393	389666.561834	38.557453
2250.666174	390421.692570	38.562471
2252.930926	391147.761010	38.567488
2255.207494	391904.153942	38.572506
2257.678581	392629.038301	38.577524
2260.500441	393361.781755	38.582541
2263.062575	394120.455824	38.587559
2265.367509	394842.729640	38.592576
2267.541013	395574.107262	38.597594
2269.601915	396316.891300	38.602612
2272.163176	397055.316389	38.607629
2274.472890	397779.749069	38.612647
2276.607358	398516.738175	38.617664
2279.645538	399245.678030	38.622682
2281.862380	399959.656255	38.627700
2284.964544	400672.051831	38.632717
2287.398253	401392.142549	38.637735
2290.090536	402089.036454	38.642752
2292.359609	402790.747170	38.647770
2294.773773	403497.079191	38.652788
2297.050289	404182.841091	38.657805
2299.404501	404888.742869	38.662823
2301.859208	405577.710094	38.667840
2304.281170	406250.399328	38.672858
2306.125445	406930.464481	38.677876
2308.734657	407574.055152	38.682893
2311.000303	408239.805184	38.687911
2312.881953	408905.323718	38.692928
2315.456423	409552.724625	38.697946
2317.114087	410219.742746	38.702964
2319.909204	410873.029161	38.707981
2322.570024	411529.235107	38.712999
2325.089907	412181.597855	38.718016
2327.362476	412845.511069	38.723034
2329.429158	413529.123355	38.728052
2331.325036	414197.168421	38.733069
2333.208513	414867.756859	38.738087
2335.194086	415549.075919	38.743104
2337.325210	416235.900009	38.748122
2339.335612	416939.543052	38.753140
2342.180284	417625.073048	38.758157
2344.449304	418339.424396	38.763175
2346.622575	419049.491750	38.768192
2348.822523	419757.306458	38.773210
2350.623869	420480.184077	38.778228
2352.698481	421208.339138	38.783245
2354.914058	421946.882635	38.788263
2356.797507	422703.842449	38.793280
2359.129630	423456.603432	38.798298
2361.256973	424219.908424	38.803316
2363.430064	424972.599005	38.808333
2365.381733	425754.419038	38.813351
2367.358738	426556.868944	38.818368
2369.407391	427343.381874	38.823386
2371.752357	428156.908283	38.828404
2373.950308	428981.165036	38.833421
2376.142184	429784.232066	38.838439
2378.544261	430597.261487	38.843456
2381.636454	431429.133545	38.848474
2383.812371	432270.543288	38.853492
2386.270324	433087.679731	38.858509
2388.634980	433939.426564	38.863527
2391.076081	434768.200118	38.868544
2393.757149	435608.394250	38.873562
2395.972788	436444.129983	38.878580
2399.067853	437291.280453	38.883597
2401.681660	438115.755094	38.888615
2404.278345	438948.097587	38.893632
2406.564642	439787.444365	38.898650
2409.173914	440627.617563	38.903668
2412.107686	441457.939576	38.908685
2414.677762	442286.418499	38.913703
2416.982106	443121.589418	38.918720
2419.338078	443961.274048	38.923738
2421.694184	444797.435645	38.928756
2424.056148	445624.508301	38.933773
2426.589459	446448.941262	38.938791
2428.787433	447298.136290	38.943808
2431.557011	448137.339304	38.948826
2434.078253	448970.682715	38.953844
2436.935240	449798.677759	38.958861
2439.351937	450639.662060	38.963879
2441.326877	451472.745011	38.968896
2443.779663	452299.697719	38.973914
2446.094797	453149.652356	38.978932
2448.570000	453990.645312	38.983949
2451.356718	454833.424174	38.988967
2454.122109	455658.726089	38.993984
2456.861021	456483.797199	38.999002
2459.222814	457322.752258	39.004020
2461.442476	458149.662494	39.009037
2464.248259	458965.268693	39.014055
2466.682557	459752.135446	39.019072
2469.358529	460550.762130	39.024090
2471.739745	461343.693105	39.029108
2473.952021	462123.123023	39.034125
2476.628417	462912.455182	39.039143
2478.819651	463713.159053	39.044160
2481.338065	464494.012865	39.049178
2484.047024	465286.631962	39.054196
2486.233326	466079.103176	39.059213
2488.449572	466882.049957	39.064231
2490.728189	467703.501194	39.069248
2493.624548	468512.333405	39.074266
2495.317911	469344.121248	39.079284
2497.366651	470161.968859	39.084301
2499.960299	470996.518397	39.089319
2501.925511	471841.089183	39.094336
2504.136705	472706.701736	39.099354
2506.285066	473571.982086	39.104372
2508.909898	474433.203694	39.109389
2511.454973	475311.676458	39.114407
2513.830576	476203.472319	39.119424
2516.114428	477081.905114	39.124442
2518.284303	477982.338204	39.129460
2520.618829	478891.842512	39.134477
2523.362207	479786.284697	39.139495
2525.470780	480712.453948	39.144512
2528.112925	481615.005234	39.149530
2531.101273	482538.512747	39.154548
2533.630051	483454.727050	39.159565
2536.503706	484384.067371	39.164583
2539.004203	485301.707264	39.169600
2542.249129	486224.983597	39.174618
2545.165603	487138.118618	39.179636
2547.972673	488053.647923	39.184653
2550.788066	488976.448159	39.189671
2553.621813	489890.514810	39.194688
2556.708758	490805.501596	39.199706
2559.433829	491704.146943	39.204724
2561.620390	492618.278515	39.209741
2564.415455	493523.227886	39.214759
2566.725888	494444.156581	39.219776
2569.276073	495342.036165	39.224794
2571.666449	496264.115550	39.229812
2573.795394	497185.834985	39.234829
2576.520472	498095.700819	39.239847
2578.581306	499030.600576	39.244864
2581.066504	499959.627399	39.249882
2584.268824	500888.232350	39.254900
2587.183935	501809.014416	39.259917
2590.442954	502734.581543	39.264935
2592.969309	503661.630024	39.269952
2595.440248	504575.371374	39.274970
2597.868620	505503.996747	39.279988
2600.273234	506428.539131	39.285005
2602.903911	507356.269576	39.290023
2605.214558	508292.370062	39.295040
2607.468838	509236.946730	39.300058
2610.232380	510190.560054	39.305076
2612.674798	511127.281036	39.310093
2615.383034	512078.573017	39.315111
2617.447310	513028.603795	39.320128
2620.498292	513972.467319	39.325146
2623.136669	514914.880891	39.330164
2625.696860	515871.362726	39.335181
2628.716781	516824.283593	39.340199
2631.117972	517775.383857	39.345216
2633.712762	518730.929232	39.350234
2636.293429	519668.682005	39.355252
2638.717852	520592.245858	39.360269
2641.007554	521506.254609	39.365287
2643.221805	522448.583985	39.370304
2646.269914	523374.547631	39.375322
2648.782772	524295.103108	39.380340
2651.217348	525227.502613	39.385357
2654.451655	526160.166104	39.390375
2656.609986	527101.359704	39.395392
2659.320598	528025.533015	39.400410
2662.214705	528972.681976	39.405428
2664.743067	529925.118062	39.410445
2667.920267	530858.656137	39.415463
2670.441105	531800.600976	39.420480
2673.413506	532746.791046	39.425498
2675.979507	533714.079496	39.430516
2678.588947	534663.729469	39.435533
2681.027933	535612.490038	39.440551
2683.918350	536572.287472	39.445568
2686.573066	537543.886838	39.450586
2689.176578	538500.432938	39.455604
2691.651072	539475.504612	39.460621
2694.714709	540438.538159	39.465639
2697.195756	541431.337604	39.470656
2699.903476	542413.364800	39.475674
2702.397676	543403.860786	39.480692
2704.844025	544400.884739	39.485709
2707.553410	545401.667643	39.490727
2710.049384	546414.132967	39.495744
2713.194128	547414.800620	39.500762
2715.615604	548431.004091	39.505780
2718.217828	549466.764272	39.510797
2721.097176	550475.601723	39.515815
2723.687867	551498.289067	39.520832
2726.204561	552520.459829	39.525850
2729.008492	553568.244407	39.530868
2731.258647	554613.576560	39.535885
2734.248758	555656.243326	39.540903
2736.921619	556711.898469	39.545920
2739.607954	557767.770056	39.550938
2742.902390	558811.800377	39.555956
2746.033837	559871.301718	39.560973
2749.220967	560905.990723	39.565991
2751.687007	561960.913240	39.571008
2754.755754	563015.300505	39.576026
2757.418128	564051.537425	39.581044
2760.199363	565121.122941	39.586061
2762.526445	566159.910081	39.591079
2765.301645	567230.327960	39.596096
2768.435691	568286.337808	39.601114
2770.876818	569356.885914	39.606132
2773.219301	570434.942156	39.611149
2776.501455	571501.256986	39.616167
2778.971137	572578.459128	39.621184
2781.543554	573649.078423	39.626202
2784.166691	574728.030550	39.631220
2787.242802	575823.527005	39.636237
2789.946244	576908.803217	39.641255
2792.751875	577999.186883	39.646272
2795.751161	579073.238491	39.651290
2798.699890	580167.372561	39.656308
2801.029381	581257.549467	39.661325
2803.902228	582329.484135	39.666343
2807.137166	583434.416872	39.671360
2809.837136	584521.585854	39.676378
2813.377387	585601.850609	39.681396
2816.184835	586689.811722	39.686413
2818.850387	587763.410337	39.691431
2821.287596	588839.858944	39.696448
2823.996645	589880.577201	39.701466
2827.122599	590942.187791	39.706484
2830.027930	591983.142462	39.711501
2832.899888	593014.239855	39.716519
2835.841099	594047.641719	39.721536
2838.481698	595095.132498	39.726554
2841.193556	596133.300370	39.731572
2843.743667	597194.747872	39.736589
2846.486475	598245.598718	39.741607
2849.187273	599301.120349	39.746624
2851.783814	600369.034018	39.751642
2855.041541	601404.090336	39.756660
2858.665742	602467.985890	39.761677
2861.806108	603521.849570	39.766695
2864.586753	604585.738812	39.771712
2867.014745	605647.785427	39.776730
2869.900076	606722.071481	39.781748
2872.294892	607803.794486	39.786765
2875.372180	608895.961525	39.791783
2878.244446	609989.207919	39.796800
2880.913040	611076.778077	39.801818
2883.374444	612165.928220	39.806836
2886.375148	613288.750638	39.811853
2889.012687	614396.614114	39.816871
2891.779500	615517.700070	39.821888
2894.813684	616641.429266	39.826906
2897.953621	617756.576038	39.831924
2901.172670	618895.096815	39.836941
2904.041150	620016.209262	39.841959
2906.927659	621149.451338	39.846976
2910.026877	622271.544137	39.851994
2913.473276	623391.514749	39.857012
2916.086809	624538.592692	39.862029
2919.211441	625675.470908	39.867047
2922.077057	626822.614128	39.872064
2924.543950	627964.654670	39.877082
2927.534088	629112.781041	39.882100
2930.125858	630284.074744	39.887117
2933.089040	631434.552235	39.892135
2936.152335	632607.858781	39.897152
2939.159672	633765.016358	39.902170
2942.902572	634919.878430	39.907188
2945.504744	636088.229531	39.912205
2948.819069	637245.401432	39.917223
2952.031578	638412.992114	39.922240
2954.761606	639563.813465	39.927258
2958.437755	640717.494343	39.932276
2961.770463	641867.410662	39.937293
2964.926857	643003.907709	39.942311
2967.941675	644147.384963	39.947328
2970.740273	645302.889326	39.952346
2973.747902	646453.590153	39.957364
2976.282446	647610.421424	39.962381
2979.290772	648756.223066	39.967399
2982.608744	649910.517629	39.972416
2985.166648	651063.508733	39.977434
2988.396300	652214.810954	39.982452
2991.173274	653368.646318	39.987469
2994.171235	654534.918159	39.992487
2997.175427	655688.297014	39.997504
2999.970542	656865.986198	40.002522
3003.077779	658025.301982	40.007540
3005.720443	659193.273384	40.012557
3008.759131	660356.707582	40.017575
3011.282411	661523.324538	40.022592
3013.685509	662718.200257	40.027610
3016.711036	663904.960675	40.032628
3019.330215	665080.791262	40.037645
3022.298902	666256.022550	40.042663
3024.746863	667414.873451	40.047680
3027.333587	668606.450611	40.052698
3030.635534	669767.214053	40.057716
3033.662743	670940.565995	40.062733
3036.702038	672110.139784	40.067751
3040.116873	673288.210113	40.072768
3042.933648	674456.485301	40.077786
3045.843696	675636.681753	40.082804
3049.244583	676835.937448	40.087821
3052.607101	678030.422553	40.092839
3056.195773	679217.212159	40.097856
3059.050899	680409.138955	40.102874
3062.422448	681592.280617	40.107892
3065.333797	682799.243085	40.112909
3068.155919	683985.098764	40.117927
3071.542213	685188.737672	40.122944
3074.659272	686389.232840	40.127962
3077.581960	687601.667963	40.132980
3080.430647	688821.946708	40.137997
3083.522178	690021.915703	40.143015
3086.579024	691256.723724	40.148032
3089.852997	692469.688204	40.153050
3092.953372	693699.735854	40.158068
3095.837108	694945.923489	40.163085
3098.808213	696178.180850	40.168103
3101.943934	697436.726961	40.173120
3105.290378	698693.869021	40.178138
3107.813056	699943.975801	40.183156
3110.845063	701210.380535	40.188173
3113.517732	702475.471675	40.193191
3116.654627	703774.651843	40.198208
3119.740352	705056.152603	40.203226
3123.276212	706321.484161	40.208244
3126.291384	707610.744894	40.213261
3129.671262	708919.418444	40.218279
3132.270799	710218.462298	40.223296
3135.303265	711529.865593	40.228314
3138.400532	712857.198002	40.233332
3141.078444	714180.333025	40.238349
3143.824403	715508.299178	40.243367
3146.876487	716850.110846	40.248384
3149.954592	718192.347796	40.253402
3153.111077	719535.792035	40.258420
3156.076397	720912.936165	40.263437
3159.487690	722272.914460	40.268455
3162.743771	723636.454009	40.273472
3166.091773	725014.438085	40.278490
3169.249784	726373.735589	40.283508
3172.545828	727743.461646	40.288525
3175.888878	729116.064507	40.293543
3179.481920	730478.217655	40.298560
3182.857923	731849.515472	40.303578
3186.503615	733199.842232	40.308596
3190.079321	734560.177672	40.313613
3193.082619	735902.603043	40.318631
3197.064403	737235.016621	40.323648
3200.708834	738573.927775	40.328666
3203.967036	739901.376989	40.333684
3207.555304	741242.465190	40.338701
3210.568377	742563.441439	40.343719
3213.906800	743882.170672	40.348736
3216.710110	745212.801204	40.353754
3220.078296	746541.042680	40.358772
3223.558752	747874.217307	40.363789
3226.624460	749196.043575	40.368807
3230.213327	750505.583478	40.373824
3233.471490	751803.623723	40.378842
3237.003941	753077.407932	40.383860
3239.964390	754329.796118	40.388877
3243.311628	755589.649457	40.393895
3246.293880	756845.909172	40.398912
3249.378613	758108.789635	40.403930
3252.571170	759363.714740	40.408948
3255.293057	760638.493504	40.413965
3258.397376	761914.077823	40.418983
3261.268756	763194.947001	40.424000
3264.303214	764482.163915	40.429018
3267.357600	765790.749805	40.434036
3270.375412	767088.491208	40.439053
3273.186758	768411.264837	40.444071
3276.388056	769748.192486	40.449088
3278.897416	771077.866839	40.454106
3282.181385	772416.855998	40.459124
3285.083332	773783.278069	40.464141
3288.056033	775155.575472	40.469159
3291.384487	776535.809035	40.474176
3294.310421	777940.253824	40.479194
3297.847023	779333.428546	40.484212
3300.909826	780729.752344	40.489229
3304.432096	782152.723666	40.494247
3308.064728	783571.127875	40.499264
3311.518741	784986.142636	40.504282
3315.248412	786401.667034	40.509300
3318.544243	787832.135686	40.514317
3321.792909	789253.843623	40.519335
3325.182585	790681.371512	40.524352
3328.410547	792131.476469	40.529370
3331.735201	793573.379423	40.534388
3335.473468	795005.709506	40.539405
3338.439574	796452.274257	40.544423
3341.940140	797909.127148	40.549440
3345.277090	799363.010290	40.554458
3348.884736	800809.741411	40.559476
3352.476088	802280.348321	40.564493
3356.019823	803741.745665	40.569511
3359.200502	805187.141938	40.574528
3362.464269	806670.953863	40.579546
3366.019395	808123.983536	40.584564
3369.503905	809601.989003	40.589581
3372.620440	811066.684707	40.594599
3376.351166	812529.057333	40.599616
3379.643587	814009.798876	40.604634
3383.569614	815466.813055	40.609652
3386.733269	816935.063480	40.614669
3390.553680	818412.111067	40.619687
3394.050197	819858.378934	40.624704
3397.485932	821326.399991	40.629722
3400.562676	822783.958599	40.634740
3404.240505	824249.633222	40.639757
3407.807858	825709.538380	40.644775
3411.736314	827167.792205	40.649792
3414.682391	828646.502648	40.654810
3417.790744	830089.178198	40.659828
3421.145852	831558.389016	40.664845
3424.279663	833042.843134	40.669863
3427.516301	834508.092566	40.674880
3430.940946	836006.720596	40.679898
3433.851099	837494.472335	40.684916
3436.916906	838982.242688	40.689933
3439.883851	840492.064885	40.694951
3443.326308	841987.976624	40.699968
3446.747508	843505.521719	40.704986
3450.148606	845023.289966	40.710004
3454.038678	846523.891134	40.715021
3457.402042	848017.339722	40.720026
3460.768551	849465.424223	40.725031
3464.023553	850863.810124	40.730036
3467.303496	852184.462075	40.735040
3470.704019	853429.262759	40.740045
3474.010868	854642.777366	40.745050
3477.101345	855745.822865	40.750055
3479.745573	856816.536320	40.755060
3482.730610	857788.062941	40.760064
3485.801358	858693.857478	40.765069
3487.812995	859548.046003	40.770074
3490.194537	860324.448513	40.775079
3492.250014	861044.699067	40.780084
3494.342185	861692.617572	40.785088
3496.214163	862295.199223	40.790093
3497.944369	862837.571183	40.795098
3499.750956	863313.784138	40.800103
3501.111159	863752.321151	40.805108
3502.720012	864147.536037	40.810112
3504.657908	864472.795348	40.815117
3505.618920	864777.401589	40.820122
3507.582432	865012.735394	40.825127
3508.282016	865227.861950	40.830132
3509.421326	865395.003701	40.835136
3510.506876	865528.238120	40.840141
3511.244128	865638.401432	40.845146
3512.015564	865700.363299	40.850151
3512.908431	865748.798673	40.855156
3513.811087	865759.921047	40.860160
3514.598989	865754.252877	40.865165
3515.197657	865726.656646	40.870170
3515.862878	865654.936110	40.875175
3516.177979	865591.240100	40.880180
3516.620532	865481.756091	40.885184
3517.193424	865369.042007	40.890189
3517.061585	865237.784774	40.895194
3517.854414	865103.748670	40.900199
3518.100777	864938.217005	40.905204
3518.171263	864771.252090	40.910208
3518.311771	864586.195004	40.915213
3518.926751	864402.220356	40.920218
3518.968021	864200.646202	40.925223
3518.758765	863987.540696	40.930228
3519.129762	863769.083541	40.935232
3519.459288	863551.208568	40.940237
3519.566223	863318.587549	40.945242
3519.520458	863063.430686	40.950247
3519.612392	862825.835716	40.955252
3519.758389	862564.015963	40.960256
3520.216040	862301.939187	40.965261
3519.754931	862044.766448	40.970266
3520.012732	861770.643999	40.975271
3519.848476	861505.329678	40.980276
3519.552870	861223.592453	40.985280
3519.672443	860947.705564	40.990285
3519.602224	860687.882993	40.995290
3519.686583	860402.447249	41.000295
3519.563923	860134.732573	41.005300
3519.664320	859841.293174	41.010304
3519.883775	859558.130030	41.015309
3519.856930	859268.769235	41.020314
3519.588424	858976.613690	41.025319
3519.778938	858684.174071	41.030324
3519.588587	858391.588699	41.035328
3519.583325	858098.861617	41.040333
3519.057408	857806.595522	41.045338
3519.191411	857504.282667	41.050343
3519.222483	857222.015816	41.055348
3518.709071	856928.732961	41.060352
3518.757541	856631.840446	41.065357
3518.202543	856344.861774	41.070362
3518.414100	856054.434649	41.075367
3518.318177	855777.183143	41.080372
3518.589731	855487.108752	41.085376
3518.856863	855197.216146	41.090381
3518.628097	854911.674455	41.095386
3518.861298	854613.875829	41.100391
3518.154202	854325.952365	41.105396
3518.269027	854017.825904	41.110400
3518.566504	853746.162289	41.115405
3518.406350	853461.613361	41.120410
3518.232715	853153.491483	41.125415
3517.995985	852881.001719	41.130420
3517.707342	852588.741830	41.135424
3518.056647	852295.584099	41.140429
3517.781060	852011.572041	41.145434
3517.706407	851725.566192	41.150439
3517.686738	851443.920755	41.155444
3517.544177	851153.906815	41.160448
3517.515867	850859.282759	41.165453
3517.192539	850588.947138	41.170458
3517.066170	850293.630701	41.175463
3517.038595	850032.768365	41.180468
3516.954527	849741.802470	41.185472
3517.173203	849464.704526	41.190477
3516.658841	849192.781223	41.195482
3516.743032	848913.147936	41.200487
3516.840004	848640.223069	41.205492
3516.572541	848367.054032	41.210496
3516.612064	848082.421657	41.215501
3516.573851	847817.473615	41.220506
3516.326083	847547.383972	41.225511
3515.988400	847265.895170	41.230516
3515.747133	846999.971536	41.235520
3515.851592	846741.776854	41.240525
3515.581704	846484.023115	41.245530
3515.594933	846220.656269	41.250535
3515.369963	845955.465599	41.255540
3515.348938	845702.610188	41.260544
3514.975516	845441.711490	41.265549
3515.003388	845181.905763	41.270554
3514.731112	844945.049448	41.275559
3515.009088	844703.901300	41.280564
3514.653977	844441.008320	41.285568
3514.970823	844192.131765	41.290573
3514.570696	843949.213966	41.295578
3514.637359	843704.942308	41.300583
3514.228291	843458.301718	41.305588
3514.153966	843219.397879	41.310592
3514.247740	842986.845053	41.315597
3514.133859	842749.539143	41.320602
3514.017275	842506.226738	41.325607
3513.837785	842275.448386	41.330612
3513.949486	842060.707210	41.335616
3513.831208	841816.051904	41.340621
3513.655611	841580.029255	41.345626
3513.346503	841354.993910	41.350631
3513.182237	841106.855972	41.355636
3513.215508	840881.893831	41.360640
3513.563789	840657.408429	41.365645
3512.894837	840445.082713	41.370650
3513.152785	840202.010730	41.375655
3512.891982	839990.480728	41.380660
3512.928259	839773.674711	41.385664
3512.910289	839539.989818	41.390669
3512.546827	839328.064477	41.395674
3512.341193	839102.200736	41.400679
3512.181660	838900.180939	41.405684
3512.137829	838689.060027	41.410688
3512.256519	838476.441513	41.415693
3511.837879	838286.204742	41.420698
3512.243908	838069.377635	41.425703
3512.202163	837869.599455	41.430708
3512.209527	837655.215220	41.435712
3511.855338	837452.059363	41.440717
3511.565643	837246.348589	41.445722
3511.648994	837038.227060	41.450727
3511.461646	836852.936735	41.455732
3511.388897	836662.985297	41.460736
3511.772810	836464.508742	41.465741
3511.846648	836255.484836	41.470746
3511.653384	836065.145088	41.475751
3511.384383	835861.485569	41.480756
3511.318299	835669.258174	41.485760
3511.508821	835475.225312	41.490765
3511.390136	835291.489707	41.495770
3511.136875	835084.678563	41.500775
3510.844085	834895.394707	41.505780
3510.755503	834707.438736	41.510784
3510.775414	834505.983526	41.515789
3510.818901	834341.480289	41.520794
3510.966942	834145.168379	41.525799
3510.529958	833961.886797	41.530804
3510.239121	833791.320885	41.535808
3510.301797	833611.755898	41.540813
3510.034749	833428.284695	41.545818
3510.294129	833237.786963	41.550823
3510.094450	833075.098466	41.555828
3509.854230	832897.907721	41.560832
3510.044507	832727.381027	41.565837
3509.579411	832567.800373	41.570842
3510.056188	832388.621665	41.575847
3509.693873	832225.010619	41.580852
3509.857381	832054.959083	41.585856
3509.576523	831893.231175	41.590861
3509.431889	831721.609762	41.595866
3509.183764	831556.888429	41.600871
3509.170906	831401.503211	41.605876
3508.715987	831237.100925	41.610880
3508.904323	831090.859007	41.615885
3508.753816	830933.189246	41.620890
3508.850782	830789.984481	41.625895
3508.796142	830635.662626	41.630900
3508.848041	830500.617683	41.635904
3508.643382	830344.994538	41.640909
3508.779742	830202.552077	41.645914
3508.689273	830040.600145	41.650919
3508.328481	829891.148152	41.655924
3508.041228	829749.547334	41.660928
3508.145406	829605.680145	41.665933
3508.257149	829468.600591	41.670938
3508.065124	829314.856450	41.675943
3507.792983	829187.020791	41.680948
3507.819971	829051.754476	41.685952
3508.218504	828912.417000	41.690957
3507.854164	828777.795885	41.695962
3507.638525	828642.072364	41.700967
3507.719404	828506.785891	41.705972
3507.319775	828383.598236	41.710976
3507.472114	828255.234577	41.715981
3507.178188	828129.776581	41.720986
3507.258033	828016.913124	41.725991
3507.309677	827883.231430	41.730996
3507.151947	827756.228698	41.736000
3507.455197	827634.817347	41.741005
3507.128865	827522.452168	41.746010
3507.385462	827394.494367	41.751015
3507.330975	827269.762518	41.756020
3507.138826	827136.252380	41.761024
3507.468336	827008.128388	41.766029
3507.392247	826894.293640	41.771034
3507.314321	826763.201238	41.776039
3506.786981	826641.419472	41.781044
3507.002452	826519.073119	41.786048
3507.164847	826403.821782	41.791053
3506.744567	826289.935472	41.796058
3506.513735	826172.838245	41.801063
3506.616693	826055.097279	41.806068
3506.532151	825948.532002	41.811072
3506.744962	825826.466532	41.816077
3506.350306	825722.148753	41.821082
3506.542457	825613.136775	41.826087
3506.559235	825482.100994	41.831092
3506.396921	825371.823284	41.836096
3506.604369	825265.052155	41.841101
3506.112594	825162.061654	41.846106
3505.863705	825063.528013	41.851111
3506.023193	824945.513398	41.856116
3506.091517	824854.992449	41.861120
3506.222439	824746.367393	41.866125
3506.051968	824650.895289	41.871130
3505.984435	824539.903441	41.876135
3506.057700	824446.784352	41.881140
3505.763565	824346.584803	41.886144
3506.291525	824239.401955	41.891149
3505.827981	824144.313108	41.896154
3505.903739	824037.152559	41.901159
3505.710422	823939.473233	41.906164
3505.663599	823835.068265	41.911168
3506.141217	823738.498091	41.916173
3505.797884	823643.920201	41.921178
3506.111411	823541.309701	41.926183
3505.785808	823436.161824	41.931188
3505.987040	823349.559927	41.936192
3505.889814	823249.996026	41.941197
3505.567964	823155.945619	41.946202
3505.703596	823040.835521	41.951207
3505.745491	822950.928669	41.956212
3505.563281	822861.350986	41.961216
3505.854823	822755.552587	41.966221
3505.404221	822668.070867	41.971226
3505.492423	822567.145459	41.976231
3505.562191	822471.015290	41.981236
3505.163264	822392.081651	41.986240
3505.271653	822298.046010	41.991245
3504.975688	822207.304205	41.996250
3505.285529	822122.331565	42.001255
3505.116867	822033.572060	42.006260
3504.905159	821959.200799	42.011264
3505.163770	821867.286760	42.016269
3504.858058	821791.314734	42.021274
3504.695466	821701.669212	42.026279
3505.153695	821630.559488	42.031284
3504.740790	821541.686863	42.036288
3504.831748	821456.301444	42.041293
3504.686184	821384.848237	42.046298
3504.783903	821307.630048	42.051303
3504.505328	821234.044457	42.056308
3504.385974	821146.830556	42.061312
3504.704808	821070.062439	42.066317
3504.631259	820998.984624	42.071322
3504.333636	820917.276845	42.076327
3504.748666	820846.606194	42.081332
3504.392800	820761.579011	42.086336
3504.661506	820689.560801	42.091341
3504.606244	820617.497317	42.096346
3504.654204	820529.318093	42.101351
3504.743332	820472.935775	42.106356
3504.234607	820399.721363	42.111360
3504.408230	820320.081580	42.116365
3504.466507	820245.597717	42.121370
3504.397388	820169.274565	42.126375
3504.327925	820094.124990	42.131380
3504.310398	820030.710107	42.136384
3504.416352	819956.655561	42.141389
3504.271861	819889.443374	42.146394
3503.785543	819816.659262	42.151399
3504.168861	819751.022536	42.156404
3504.197942	819692.588199	42.161408
3504.424270	819608.526970	42.166413
3504.349677	819538.706080	42.171418
3504.379941	819468.867187	42.176423
3504.299363	819394.592431	42.181428
3504.307704	819318.540400	42.186432
3504.441262	819253.820823	42.191437
3504.362657	819187.471610	42.196442
3504.413066	819105.194850	42.201447
3504.240916	819044.047308	42.206452
3503.897172	818965.259609	42.211456
3504.136848	818899.099809	42.216461
3503.795707	818833.964931	42.221466
3503.519691	818775.083383	42.226471
3503.676785	818720.485930	42.231476
3503.447330	818656.554505	42.236480
3503.867923	818596.186209	42.241485
3503.417662	818541.932059	42.246490
3503.806752	818486.119806	42.251495
3503.629256	818418.408774	42.256500
3503.239302	818369.723076	42.261504
3503.424196	818305.426362	42.266509
3503.452425	818258.384091	42.271514
3503.437020	818193.385092	42.276519
3503.649160	818146.948057	42.281524
3503.286127	818085.823177	42.286528
3503.587058	818025.909976	42.291533
3503.355277	817970.880970	42.296538
3503.632034	817908.816956	42.301543
3503.465488	817856.125823	42.306548
3503.592570	817801.378958	42.311552
3503.780953	817725.279126	42.316557
3503.349997	817687.070622	42.321562
3503.357368	817638.069388	42.326567
3503.577346	817563.626855	42.331572
3503.631908	817524.260507	42.336576
3503.619300	817462.680590	42.341581
3503.358147	817412.889746	42.346586
3503.354428	817346.803632	42.351591
3503.201799	817306.588972	42.356596
3503.241905	817260.125169	42.361600
3503.391739	817213.104472	42.366605
3503.212528	817160.214126	42.371610
3503.298166	817095.922143	42.376615
3503.281617	817042.269745	42.381620
3503.025511	817001.776564	42.386624
3503.516115	816937.808006	42.391629
3503.000926	816888.740495	42.396634
3503.048835	816839.090301	42.401639
3502.995119	816786.029457	42.406644
3502.846110	816742.775452	42.411648
3502.963842	816697.959528	42.416653
3502.925920	816649.154353	42.421658
3503.017337	816594.354541	42.426663
3503.054479	816556.943733	42.431668
3502.850063	816514.872402	42.436672
3503.246517	816468.589213	42.441677
3502.923031	816425.753579	42.446682
3502.742064	816370.311362	42.451687
3502.810481	816333.089996	42.456692
3502.806492	816292.502039	42.461696
3502.949250	816229.808058	42.466701
3502.919982	816195.588672	42.471706
3502.963003	816143.730857	42.476711
3502.842646	816101.055538	42.481716
3502.665908	816064.460614	42.486720
3502.883687	816012.573000	42.491725
3502.916283	815965.758725	42.496730
3502.600537	815918.854611	42.501735
3502.936268	815877.082017	42.506740
3502.825296	815847.232116	42.511744
3502.911310	815799.477561	42.516749
3502.650895	815753.297645	42.521754
3502.922275	815709.967734	42.526759
3502.849551	815666.645258	42.531764
3502.507028	815648.094696	42.536768
3502.846684	815589.132665	42.541773
3502.451306	815550.955072	42.546778
3502.571468	815509.950203	42.551783
3502.801979	815470.053151	42.556788
3502.378301	815436.629371	42.561792
3502.775637	815383.630046	42.566797
3502.789328	815355.520262	42.571802
3502.619687	815313.386702	42.576807
3502.595152	815263.198138	42.581812
3502.491775	815224.774717	42.586816
3502.453046	815191.531152	42.591821
3502.368941	815152.418575	42.596826
3502.246565	815111.989895	42.601831
3501.910175	815083.985610	42.606836
3502.427222	815043.647074	42.611840
3502.853118	815019.875302	42.616845
3502.640936	814977.354881	42.621850
3502.149386	814939.238621	42.626855
3502.522984	814907.052063	42.631860
3502.205236	814884.038930	42.636864
3502.637380	814842.978608	42.641869
3502.375104	814793.756163	42.646874
3502.434511	814758.290553	42.651879
3502.409261	814723.524317	42.656884
3502.420951	814688.506952	42.661888
3502.803341	814644.466280	42.666893
3502.603413	814607.328536	42.671898
3502.340992	814563.050731	42.676903
3502.580497	814530.051910	42.681908
3502.388968	814494.038557	42.686912
3502.355733	814455.893036	42.691917
3502.357928	814420.924819	42.696922
3502.457420	814384.030371	42.701927
3502.663221	814352.407532	42.706932
3502.248241	814308.251130	42.711936
3502.518324	814273.727778	42.716941
3502.371768	814246.472347	42.721946
3502.269433	814212.499785	42.726951
3502.346835	814175.999647	42.731956
3502.173105	814148.699319	42.736960
3502.473091	814117.255770	42.741965
3502.632198	814077.852006	42.746970
3502.335111	814039.012929	42.751975
3502.279523	814014.043514	42.756980
3502.264005	813965.509031	42.761984
3502.219861	813939.655851	42.766989
3502.043198	813909.955108	42.771994
3501.909805	813868.786101	42.776999
3502.146665	813845.335207	42.782004
3501.879785	813816.775427	42.787009
3502.021861	813782.319626	42.792013
3501.977265	813764.645392	42.797018
3502.245355	813741.286952	42.802023
3502.321775	813708.555876	42.807028
3502.042064	813658.054525	42.812033
3502.351961	813630.329573	42.817037
3502.090327	813611.417196	42.822042
3502.340996	813572.093358	42.827047
3502.272896	813544.087450	42.832052
3501.978087	813515.971826	42.837057
3502.049053	813477.656664	42.842061
3501.958823	813456.462467	42.847066
3502.282805	813438.187867	42.852071
3502.149818	813393.146326	42.857076
3501.666545	813379.804787	42.862081
3502.095009	813342.360633	42.867085
3502.047229	813326.253215	42.872090
3502.011277	813288.640349	42.877095
3502.013511	813259.642018	42.882100
3501.805606	813240.621783	42.887105
3501.665040	813193.865746	42.892109
3502.072357	813175.429760	42.897114
3501.870109	813148.815853	42.902119
3501.970764	813120.584455	42.907124
3501.652468	813094.822180	42.912129
3502.229980	813068.765297	42.917133
3502.007613	813040.537788	42.922138
3502.049407	813015.303713	42.927143
3502.170471	812974.724142	42.932148
3501.775215	812966.020874	42.937153
3502.143057	812930.494852	42.942157
3502.048650	812905.037872	42.947162
3501.813078	812870.100784	42.952167
3502.073029	812845.711888	42.957172
3501.829907	812817.976728	42.962177
3502.099133	812768.945866	42.967181
3502.100912	812765.075603	42.972186
3501.865036	812724.896235	42.977191
3501.952205	812712.047251	42.982196
3501.966432	812682.799533	42.987201
3501.945505	812645.719474	42.992205
3502.017692	812634.391425	42.997210
3501.855324	812592.484594	43.002215
3502.003868	812571.689181	43.007220
3501.995189	812556.945155	43.012225
3501.978096	812516.336603	43.017229
3501.903458	812497.096368	43.022234
3501.784942	812479.332968	43.027239
3502.012524	812440.447254	43.032244
3502.095165	812414.420384	43.037249
3501.970400	812375.494356	43.042253
3501.887027	812365.416219	43.047258
3501.680477	812340.759420	43.052263
3502.173367	812313.880751	43.057268
3501.812844	812300.614831	43.062273
3501.817088	812260.099207	43.067277
3501.822936	812239.963156	43.072282
3501.852023	812212.964523	43.077287
3501.676898	812181.100328	43.082292
3501.928592	812155.534526	43.087297
3501.637567	812147.106975	43.092301
3501.576201	812113.460041	43.097306
3501.992027	812086.201233	43.102311
3501.613020	812072.594968	43.107316
3501.662078	812045.151450	43.112321
3502.033501	812018.046659	43.117325
3501.832437	811999.903660	43.122330
3501.752756	811974.293775	43.127335
3501.537836	811939.348473	43.132340
3501.523296	811931.854963	43.137345
3501.994377	811897.776305	43.142349
3501.517186	811877.179818	43.147354
3501.541357	811845.085241	43.152359
3501.830479	811824.558341	43.157364
3501.748103	811796.351570	43.162369
3501.939212	811776.232618	43.167373
3501.636991	811768.149393	43.172378
3501.701871	811753.391500	43.177383
3501.901764	811721.267392	43.182388
3501.901886	811704.756267	43.187393
3501.886063	811672.814446	43.192397
3501.539959	811655.625312	43.197402
3501.623787	811627.635434	43.202407
3501.837113	811601.387935	43.207412
3501.676623	811578.631581	43.212417
3501.828516	811549.503278	43.217421
3501.583175	811547.289876	43.222426
3501.664051	811523.121702	43.227431
3501.415903	811501.212453	43.232436
3501.463133	811475.236805	43.237441
3501.617403	811445.764693	43.242445
3501.606012	811433.174501	43.247450
3501.527375	811408.591227	43.252455
3501.502733	811390.662517	43.257460
3501.427731	811378.817652	43.262465
3501.838677	811350.478769	43.267469
3501.410660	811346.776485	43.272474
3501.095093	811300.428163	43.277479
3501.443133	811295.226095	43.282484
3501.388657	811285.680560	43.287489
3501.758488	811265.873639	43.292493
3501.661130	811252.709302	43.297498
3501.565268	811232.880998	43.302503
3501.972347	811208.608975	43.307508
3501.604915	811187.404330	43.312513
3501.830591	811152.382394	43.317517
3501.608696	811136.151447	43.322522
3501.583368	811104.600502	43.327527
3501.971403	811086.211022	43.332532
3501.873548	811068.587513	43.337537
3501.717628	811066.114227	43.342541
3501.680355	811025.941057	43.347546
3501.746079	811008.927440	43.352551
3501.599454	810984.549825	43.357556
3501.577920	810973.969434	43.362561
3501.979886	810946.365341	43.367565
3501.823496	810922.773111	43.372570
3501.513860	810899.696043	43.377575
3501.830666	810871.762674	43.382580
3501.528509	810858.533305	43.387585
3501.596371	810823.290665	43.392589
3501.349240	810818.578277	43.397594
3501.476144	810807.924176	43.402599
3501.537371	810779.150510	43.407604
3501.371808	810774.669661	43.412609
3501.485791	810735.204872	43.417613
3501.503273	810717.806460	43.422618
3501.454044	810696.400858	43.427623
3501.826082	810668.849571	43.432628
3501.603785	810668.543153	43.437633
3501.371937	810630.898790	43.442637
3501.402375	810615.213056	43.447642
3501.525303	810609.116505	43.452647
3501.677252	810579.739023	43.457652
3501.371991	810571.703867	43.462657
3501.494217	810548.260452	43.467661
3501.460298	810522.392530	43.472666
3501.479525	810516.361981	43.477671
3501.608389	810491.496190	43.482676
3501.470988	810476.278810	43.487681
3501.917896	810461.553189	43.492685
3501.240768	810430.106474	43.497690
3501.638736	810426.806663	43.502695
3501.637231	810394.513441	43.507700
3501.246592	810393.646692	43.512705
3501.652291	810372.116129	43.517709
3501.716623	810339.125744	43.522714
3501.427135	810320.551773	43.527719
3501.539667	810293.874789	43.532724
3501.254066	810284.561934	43.537729
3501.594006	810268.334373	43.542733
3501.750017	810241.110967	43.547738
3501.608055	810233.293535	43.552743
3501.605312	810208.252367	43.557748
3501.390145	810189.812812	43.562753
3501.256701	810175.770234	43.567757
3501.585143	810148.126011	43.572762
3501.456540	810132.612377	43.577767
3501.627944	810115.628122	43.582772
3501.448425	810098.407592	43.587777
3501.851234	810081.091099	43.592781
3501.568176	810057.173682	43.597786
3501.532828	810031.843198	43.602791
3501.762187	810014.212060	43.607796
3501.374470	810015.599080	43.612801
3501.552184	809987.586981	43.617805
3501.537873	809967.692541	43.622810
3501.687857	809931.353599	43.627815
3501.387506	809920.278414	43.632820
3501.361379	809892.054462	43.637825
3501.475396	809895.711218	43.642829
3501.454445	809872.191042	43.647834
3501.287323	809850.361126	43.652839
3501.668881	809840.153642	43.657844
3501.351787	809815.995943	43.662849
3501.476064	809789.119014	43.667853
3501.375671	809791.144864	43.672858
3501.555610	809770.678762	43.677863
3501.680614	809739.929860	43.682868
3501.365271	809729.738987	43.687873
3501.623675	809700.683236	43.692877
3501.168328	809695.220219	43.697882
3501.161863	809683.802186	43.702887
3501.181657	809649.541560	43.707892
3501.213307	809636.254819	43.712897
3501.644712	809648.926142	43.717901
3501.556329	809615.810377	43.722906
3501.697612	809610.739109	43.727911
3501.424494	809579.908034	43.732916
3501.237457	809563.814611	43.737921
3501.169671	809553.092597	43.742925
3501.373239	809543.257058	43.747930
3501.139737	809519.525625	43.752935
3501.438994	809503.351956	43.757940
3501.180109	809493.641531	43.762945
3501.346845	809477.538641	43.767949
3501.392949	809458.318907	43.772954
3501.276178	809448.339955	43.777959
3501.654121	809427.154058	43.782964
3501.165438	809421.206201	43.787969
3501.666647	809409.410019	43.792973
3501.353173	809382.701614	43.797978
3501.346090	809362.608171	43.802983
3501.705015	809367.303118	43.807988
3501.329955	809340.065567	43.812993
3501.388805	809313.099514	43.817997
3501.153060	809305.149426	43.823002
3501.102175	809285.602099	43.828007
3501.371281	809273.892927	43.833012
3501.084911	809274.871303	43.838017
3501.545990	809243.231599	43.843021
3501.206757	809230.299231	43.848026
3501.345713	809215.719677	43.853031
3501.251030	809200.786477	43.858036
3501.422663	809182.476524	43.863041
3501.577809	809159.660069	43.868045
3501.500472	809144.184748	43.873050
3501.226060	809122.321156	43.878055
3501.640185	809120.929569	43.883060
3501.259683	809106.337320	43.888065
3501.763193	809065.475333	43.893069
3501.480540	809068.315634	43.898074
3501.379234	809040.933765	43.903079
3501.648285	809035.497929	43.908084
3501.287889	809005.266790	43.913089
3501.639568	808980.211739	43.918093
3501.515770	808967.194370	43.923098
3501.224245	808935.579181	43.928103
3501.391377	808914.965578	43.933108
3501.562912	808920.917066	43.938113
3501.597620	808883.121089	43.943117
3501.560550	808865.775944	43.948122
3501.574397	808867.734235	43.953127
3501.585001	808837.784344	43.958132
3501.507550	808820.690811	43.963137
3501.606055	808791.804573	43.968141
3501.614296	808778.471001	43.973146
3501.376351	808762.286036	43.978151
3501.361520	808733.565267	43.983156
3501.489411	808736.240047	43.988161
3501.560853	808716.425859	43.993165
3501.291116	808685.198046	43.998170
3501.364604	808681.509709	44.003175
3501.532159	808659.277731	44.008180
3501.031023	808654.605672	44.013185
3501.537454	808639.131079	44.018189
3501.328695	808623.529174	44.023194
3501.286970	808588.636133	44.028199
3501.325134	808583.237972	44.033204
3501.209886	808581.541343	44.038209
3501.220294	808559.383942	44.043213
3501.488758	808546.203120	44.048218
3501.358212	808542.107162	44.053223
3501.384971	808511.466938	44.058228
3501.288286	808503.640057	44.063233
3501.439489	808479.302436	44.068237
3501.407510	808459.945698	44.073242
3501.488389	808459.883336	44.078247
3501.416778	808443.229054	44.083252
3501.295523	808411.044188	44.088257
3501.399199	808400.880334	44.093261
3501.611312	808382.169423	44.098266
3501.447241	808358.324468	44.103271
3501.641351	808345.547655	44.108276
3501.229269	808323.900249	44.113281
3501.319488	808310.013053	44.118285
3501.154648	808305.579469	44.123290
3501.207215	808287.482805	44.128295
3501.410233	808261.861381	44.133300
3501.248248	808249.682256	44.138305
3501.118119	808241.370390	44.143309
3501.253054	808221.152152	44.148314
3501.300270	808206.438497	44.153319
3501.273219	808202.913521	44.158324
3501.235984	808193.801982	44.163329
3501.354893	808158.439105	44.168333
3501.179061	808149.644456	44.173338
3501.114878	808150.733446	44.178343
3501.322992	808142.806924	44.183348
3500.969523	808108.109837	44.188353
3501.115327	808101.075895	44.193357
3501.041171	808099.029235	44.198362
3500.987506	808088.743773	44.203367
3500.932053	808058.360159	44.208372
3500.671176	808045.804794	44.213377
3501.109528	808038.820642	44.218381
3501.366249	808041.964683	44.223386
3501.299802	808040.946171	44.228391
3501.558308	808011.245945	44.233396
3501.596606	807992.611620	44.238401
3501.375607	807989.363586	44.243405
3501.846723	807946.588425	44.248410
3501.420842	807948.129197	44.253415
3501.352653	807908.040764	44.258420
3501.464915	807906.698664	44.263425
3501.407197	807895.874340	44.268429
3501.462123	807870.618998	44.273434
3501.276428	807868.296508	44.278439
3501.310476	807861.967038	44.283444
3501.068437	807823.965673	44.288449
3501.596678	807807.701256	44.293453
3501.306944	807819.318244	44.298458
3501.255669	807791.727030	44.303463
3501.327099	807768.184379	44.308468
3501.221448	807775.408096	44.313473
3501.183588	807750.951957	44.318477
3501.684342	807713.121760	44.323482
3501.185875	807719.233686	44.328487
3501.519105	807713.492097	44.333492
3501.206500	807685.796431	44.338497
3501.430477	807661.002701	44.343501
3501.465958	807664.232385	44.348506
3500.909291	807632.262638	44.353511
3501.319760	807624.351209	44.358516
3501.116070	807618.992125	44.363521
3501.409250	807609.090023	44.368525
3501.072312	807591.055674	44.373530
3501.147884	807577.365499	44.378535
3501.473469	807571.477978	44.383540
3500.994791	807560.967585	44.388545
3501.265193	807530.184779	44.393549
3500.934567	807528.817510	44.398554
3500.824146	807528.443481	44.403559
3501.430066	807504.615785	44.408564
3500.899418	807487.152340	44.413569
3500.856839	807477.991701	44.418573
3500.886625	807478.771170	44.423578
3500.707216	807484.683673	44.428583
3501.214981	807473.863584	44.433588
3501.157957	807444.556046	44.438593
3501.124831	807430.197130	44.443597
3501.023634	807425.458338	44.448602
3500.993812	807420.756810	44.453607
3501.219272	807401.697844	44.458612
3500.759421	807397.851540	44.463617
3501.384051	807391.130202	44.468621
3501.046645	807371.036281	44.473626
3500.981268	807383.058281	44.478631
3501.245876	807351.442193	44.483636
3500.769384	807339.901557	44.488641
3501.030803	807321.915013	44.493645
3501.297277	807330.156473	44.498650
3501.084747	807319.454788	44.503655
3501.389892	807285.233342	44.508660
3501.318085	807281.421106	44.513665
3501.245179	807272.755450	44.518669
3501.206130	807267.859232	44.523674
3501.162035	807247.961766	44.528679
3501.489044	807234.866833	44.533684
3500.961841	807215.441061	44.538689
3501.076691	807199.586486	44.543693
3501.055332	807178.802591	44.548698
3501.144189	807179.523338	44.553703
3501.268127	807168.471832	44.558708
3501.310855	807161.699041	44.563713
3501.210158	807138.770902	44.568717
3501.424438	807128.832077	44.573722
3501.304343	807120.958438	44.578727
3501.369525	807108.347638	44.583732
3501.029372	807106.589631	44.588737
3501.371001	807079.813319	44.593741
3501.215469	807068.121299	44.598746
3501.177347	807046.506292	44.603751
3501.279200	807033.889314	44.608756
3500.739507	807027.849691	44.613761
3501.076940	807012.644412	44.618765
3501.097348	807013.621591	44.623770
3501.020811	807003.289235	44.628775
3501.489092	806995.759788	44.633780
3501.066201	806966.706582	44.638785
3500.693732	806955.099130	44.643789
3500.997747	806952.891775	44.648794
3501.035973	806954.405342	44.653799
3501.147256	806931.735764	44.658804
3500.796521	806920.271758	44.663809
3500.984384	806907.346208	44.668813
3500.957536	806909.703995	44.673818
3501.011119	806900.820916	44.678823
3501.165766	806902.217260	44.683828
3501.173358	806875.691290	44.688833
3501.057422	806853.696259	44.693837
3500.954887	806862.391302	44.698842
3501.080076	806854.820158	44.703847
3501.114335	806840.350846	44.708852
3501.215180	806826.655007	44.713857
3501.245506	806810.323160	44.718861
3501.313503	806809.576494	44.723866
3501.349657	806794.028122	44.728871
3501.389487	806768.673140	44.733876
3501.097239	806768.623197	44.738881
3501.296547	806749.272547	44.743885
3501.387652	806729.155183	44.748890
3501.320587	806714.898417	44.753895
3501.259567	806715.594870	44.758900
3500.974375	806694.264600	44.763905
3500.917919	806677.456426	44.768909
3500.927666	806670.149246	44.773914
3500.958164	806669.850018	44.778919
3501.064662	806652.475605	44.783924
3500.804019	806637.613165	44.788929
3501.024564	806618.994111	44.793933
3501.098981	806618.295398	44.798938
3500.565683	806620.001242	44.803943
3500.752932	806618.107201	44.808948
3500.810245	806614.812665	44.813953
3500.999361	806609.927424	44.818957
3501.005124	806614.682459	44.823962
3500.865796	806584.306113	44.828967
3500.982938	806562.860129	44.833972
3500.906873	806564.196484	44.838977
3500.599900	806555.666537	44.843981
3501.033594	806558.831149	44.848986
3501.323588	806561.087835	44.853991
3501.197902	806527.472919	44.858996
3500.851928	806527.529886	44.864001
3501.132714	806520.275964	44.869005
3501.041529	806511.122037	44.874010
3500.761271	806486.063893	44.879015
3501.054660	806463.951154	44.884020
3500.919880	806464.316558	44.889025
3501.043416	806460.716846	44.894029
3501.191147	806468.194395	44.899034
3501.191687	806461.476894	44.904039
3501.101365	806425.600177	44.909044
3500.915544	806432.593351	44.914049
3501.381580	806423.739781	44.919053
3501.147179	806417.502226	44.924058
3500.927755	806392.973077	44.929063
3501.261138	806375.756721	44.934068
3501.103400	806370.340052	44.939073
3501.173997	806365.817389	44.944077
3501.038986	806353.826570	44.949082
3501.076325	806347.397093	44.954087
3501.118731	806345.183606	44.959092
3501.058382	806343.722537	44.964097
3501.046416	806332.005610	44.969101
3501.277041	806301.861271	44.974106
3501.030821	806296.262984	44.979111
3501.207002	806285.397584	44.984116
3500.945490	806290.098804	44.989121
3500.897067	806263.726792	44.994125
3501.028178	806242.620741	44.999130
3500.911979	806244.159902	45.004135
3501.059121	806239.820683	45.009140
3500.968277	806237.482009	45.014145
3500.960838	806215.319955	45.019149
3501.368442	806209.466798	45.024154
3500.810828	806191.318000	45.029159
3501.303565	806172.800004	45.034164
3501.147848	806182.730521	45.039169
3500.952502	806153.489275	45.044173
3500.861212	806148.404724	45.049178
3500.370989	806137.795963	45.054183
3501.106379	806126.494958	45.059188
3500.995850	806141.762847	45.064193
3501.281567	806132.252124	45.069197
3501.143445	806106.237522	45.074202
3500.814574	806094.719493	45.079207
3501.280204	806074.097204	45.084212
3501.057262	806090.903802	45.089217
3501.120462	806065.493336	45.094221
3500.885859	806048.811035	45.099226
3500.741431	806050.109714	45.104231
3501.133399	806029.009073	45.109236
3500.923116	806049.442289	45.114241
3500.955315	806043.307583	45.119245
3501.118453	806021.411015	45.124250
3500.756302	806008.672443	45.129255
3500.946039	806004.473165	45.134260
3500.776150	805994.497910	45.139265
3500.909864	805988.346434	45.144269
3501.461020	805992.913993	45.149274
3500.957106	805967.204294	45.154279
3501.178762	805952.604170	45.159284
3500.851631	805946.920853	45.164289
3501.431241	805951.876039	45.169293
3501.332745	805927.080124	45.174298
3501.187919	805918.228455	45.179303
3501.400490	805912.995606	45.184308
3501.018464	805895.993964	45.189313
3501.098839	805865.087879	45.194317
3501.420944	805866.751072	45.199322
3501.367272	805861.365894	45.204327
3501.196618	805831.530771	45.209332
3501.233465	805819.167451	45.214337
3501.222652	805801.466951	45.219341
3501.179493	805802.798032	45.224346
3501.119338	805786.380577	45.229351
3501.371425	805748.482440	45.234356
3501.189108	805765.969661	45.239361
3501.017078	805741.479409	45.244365
3501.186481	805727.034525	45.249370
3501.070941	805722.198839	45.254375
3501.040171	805708.669561	45.259380
3500.984648	805703.480713	45.264385
3501.210018	805682.112226	45.269389
3501.470309	805664.857095	45.274394
3500.983964	805665.966977	45.279399
3501.379257	805648.787643	45.284404
3501.329566	805632.319058	45.289409
3501.243261	805619.681437	45.294413
3501.454688	805611.457223	45.299418
3500.972359	805590.352137	45.304423
3501.255620	805587.657389	45.309428
3500.966743	805590.647249	45.314433
3500.995037	805580.001248	45.319437
3501.181055	805551.135961	45.324442
3500.941510	805557.256179	45.329447
3501.174806	805535.934971	45.334452
3500.918180	805543.823407	45.339457
3501.226892	805522.931084	45.344461
3501.113063	805507.355461	45.349466
3501.017041	805493.149963	45.354471
3501.157153	805487.242180	45.359476
3501.100925	805490.291841	45.364481
3501.459109	805471.990281	45.369485
3501.186661	805451.880019	45.374490
3500.962266	805449.710192	45.379495
3501.074409	805438.118412	45.384500
3501.110549	805424.871790	45.389505
3501.361576	805404.380925	45.394509
3501.229769	805398.125540	45.399514
3501.205806	805394.157251	45.404519
3501.310595	805367.805599	45.409524
3501.064347	805346.611834	45.414529
3500.984373	805344.908584	45.419533
3501.209399	805343.449335	45.424538
3500.977777	805331.374560	45.429543
3501.260006	805304.012633	45.434548
3500.954887	805308.966903	45.439553
3500.929987	805305.930483	45.444557
3501.103219	805295.946732	45.449562
3501.291096	805262.960535	45.454567
3501.622829	805253.293899	45.459572
3501.419272	805251.807145	45.464577
3501.382628	805225.183999	45.469581
3501.071582	805211.258540	45.474586
3501.067436	805208.709069	45.479591
3501.194387	805197.653897	45.484596
3501.031035	805173.699641	45.489601
3500.770917	805156.577999	45.494605
3501.053252	805153.981318	45.499610
3500.738953	805166.979989	45.504615
3500.987094	805148.254325	45.509620
3501.120927	805142.249198	45.514625
3501.123200	805111.401630	45.519629
3501.141895	805108.456026	45.524634
3500.851549	805114.977337	45.529639
3501.050010	805095.278877	45.534644
3501.107292	805096.593550	45.539649
3501.156165	805073.339614	45.544653
3501.031781	805061.050531	45.549658
3501.158223	805056.468767	45.554663
3501.264048	805047.770855	45.559668
3501.248252	805017.906687	45.564673
3501.208423	805016.147701	45.569677
3500.831399	805014.051917	45.574682
3501.045117	805000.235759	45.579687
3500.678378	804986.956571	45.584692
3500.922461	804970.143752	45.589697
3501.091148	804963.299002	45.594701
3500.944425	804967.099442	45.599706
3500.460438	804963.010508	45.604711
3500.978965	804947.770840	45.609716
3500.950542	804952.189358	45.614721
3500.781446	804925.047395	45.619725
3501.101150	804917.638251	45.624730
3501.165309	804911.301099	45.629735
3500.966762	804911.186653	45.634740
3501.000245	804907.502879	45.639745
3501.049371	804882.237485	45.644749
3500.758044	804870.858340	45.649754
3500.764633	804861.980366	45.654759
3501.129173	804862.557863	45.659764
3500.950028	804870.679522	45.664769
3501.151371	804856.227550	45.669773
3501.153124	804836.756927	45.674778
3500.897817	804841.507151	45.679783
3501.206271	804821.005092	45.684788
3501.145267	804823.957746	45.689793
3501.047126	804805.631496	45.694797
3501.126366	804783.450544	45.699802
3501.123510	804776.339601	45.704807
3501.043432	804768.603797	45.709812
3501.043220	804762.375199	45.714817
3500.838398	804745.537687	45.719821
3501.273560	804735.559025	45.724826
3500.826511	804722.586819	45.729831
3501.021658	804637.854295	45.734836
3500.964183	804523.048215	45.739841
3500.724991	804343.724352	45.744845
3500.771405	804115.986813	45.749850
3500.379583	803817.484744	45.754855
3500.425507	803466.999307	45.759860
3500.020814	803062.068950	45.764865
3499.906661	802604.180980	45.769869
3499.473607	802079.147898	45.774874
3498.979259	801519.590879	45.779879
3499.118657	800891.773093	45.784884
3498.579355	800208.259593	45.789889
3498.280955	799456.415751	45.794893
3497.831926	798647.377843	45.799898
3497.351310	797790.090626	45.804903
3497.312200	796879.990505	45.809908
3496.681265	795892.231995	45.814913
3495.749809	794846.822275	45.819917
3495.546493	793753.341759	45.824922
3494.663686	792599.226650	45.829927
3494.313149	791384.444600	45.834932
3493.353287	790110.578307	45.839937
3492.652538	788774.995702	45.844941
3492.145791	787396.848260	45.849946
3491.181788	785935.797036	45.854951
3490.704105	784424.542463	45.859956
3489.623902	782855.509481	45.864961
3488.803630	781213.904701	45.869965
3487.916731	779533.350954	45.874970
3486.749702	777798.202401	45.879975
3486.154082	775985.875741	45.884980
3485.096951	774129.733535	45.889985
3483.922120	772221.804995	45.894989
3483.196892	770233.424638	45.899994
3481.873781	768207.540501	45.904999
3481.025628	766116.532112	45.910004
3479.778248	763976.817798	45.915009
3478.549458	761774.623786	45.920013
3477.613040	759508.669306	45.925018
3476.221082	757205.583733	45.930023
3474.845894	754830.247525	45.935028
3473.229756	752417.120004	45.940033
3472.265089	749932.619658	45.945037
3471.169388	747419.024670	45.950042
3469.567184	744826.532610	45.955047
3468.113816	742190.526247	45.960052
3466.783009	739498.206573	45.965057
3465.246180	736761.307200	45.970061
3464.249838	733957.285886	45.975066
3462.403307	731108.102070	45.980071
3460.884597	728208.516795	45.985076
3459.338274	725265.531342	45.990081
3457.779060	722247.073432	45.995085
3456.179898	719184.372498	46.000090
3454.500800	716088.361365	46.005095
3452.433360	712927.095761	46.010100
3450.886065	709731.746153	46.015105
3448.702802	706479.027653	46.020109
3447.294750	703175.014093	46.025114
3444.990920	699826.495518	46.030119
3443.441864	696430.424806	46.035124
3441.254256	692997.436564	46.040129
3439.637733	689510.577593	46.045133
3437.942852	685974.386167	46.050138
3435.640727	682399.016423	46.055143
3433.906519	678760.373722	46.060148
3431.999125	675073.823697	46.065153
3429.786074	671362.335996	46.070157
3428.034628	667586.307434	46.075162
3425.620458	663765.426670	46.080167
3423.868559	659894.345385	46.085172
3421.544701	655994.602035	46.090177
3419.198451	652043.353347	46.095181
3417.074110	648046.114148	46.100186
3414.862224	643996.797911	46.105191
3412.678746	639942.218839	46.110196
3410.753870	635801.324245	46.115201
3407.922729	631627.095120	46.120205
3405.720317	627421.613541	46.125210
3403.138870	623164.886490	46.130215
3401.101050	618864.693226	46.135220
3398.521738	614533.068491	46.140225
3395.900386	610161.387488	46.145229
3393.408196	605739.711866	46.150234
3390.358607	601298.293956	46.155239
3388.103696	596808.836858	46.160244
3386.055599	592296.830632	46.165249
3383.551222	587731.170946	46.170253
3381.049416	583121.501865	46.175258
3378.274704	578483.036588	46.180263
3375.695991	573812.723915	46.185268
3373.104597	569092.569583	46.190273
3370.562900	564332.507242	46.195277
3367.841546	559539.562115	46.200282
3364.841315	554727.451283	46.205287
3362.644352	549851.694856	46.210292
3359.913229	544965.527112	46.215297
3356.857359	540038.817486	46.220301
3354.374152	535060.759886	46.225306
3351.097205	530069.823460	46.230311
3348.238263	525030.732579	46.235316
3345.351790	519965.671217	46.240321
3342.501721	514858.113740	46.245325
3339.595746	509737.335383	46.250330
3336.568463	504577.228315	46.255335
3333.532140	499397.801720	46.260340
3330.480306	494184.149545	46.265345
3327.148417	488926.856776	46.270349
3324.485357	483661.556700	46.275354
3321.283503	478375.717989	46.280359
3318.231819	473043.819265	46.285364
3314.878889	467708.748738	46.290369
3311.940364	462320.047521	46.295373
3308.921504	456922.202094	46.300378
3305.794946	451493.445350	46.305383
3302.505619	446037.911381	46.310388
3299.236957	440561.678835	46.315393
3295.816934	435061.250146	46.320397
3292.655044	429527.852134	46.325402
3289.112541	423984.100418	46.330407
3286.045018	418408.257396	46.335412
3282.698440	412835.947405	46.340417
3279.030674	407231.103033	46.345421
3276.406666	401585.672855	46.350426
3272.853782	395955.271252	46.355431
3269.434612	390280.634356	46.360436
3265.791501	384587.567182	46.365441
3262.349986	378886.993588	46.370445
3258.705104	373173.733388	46.375450
3255.057063	367449.116149	46.380455
3251.749202	361701.298681	46.385460
3248.185810	355932.451090	46.390465
3244.331558	350162.030887	46.395469
3241.169350	344359.158416	46.400474
3237.445016	338553.266697	46.405479
3233.953408	332738.926965	46.410484
3230.334794	326907.742363	46.415489
3226.068599	321066.410214	46.420493
3222.851932	315222.716531	46.425498
3219.165318	309369.856569	46.430503
3215.534852	303492.462329	46.435508
3211.479766	297624.703158	46.440513
3207.580601	291746.595286	46.445517
3204.119583	285858.547838	46.450522
3200.519257	279970.738718	46.455527
3196.425793	274072.426940	46.460532
3192.774155	268170.562489	46.465537
3188.842336	262251.230482	46.470541
3184.949661	256347.919340	46.475546
3180.753452	250437.585355	46.480551
3176.829718	244518.019536	46.485556
3173.359638	238605.236408	46.490561
3169.085041	232682.864051	46.495565
3165.105558	226770.482844	46.500570
3161.076509	220854.321238	46.505575
3157.173731	214935.776475	46.510580
3153.443749	208999.514170	46.515585
3148.877205	203047.970497	46.520589
3144.863008	197130.776348	46.525594
3140.532761	191250.242053	46.530599
3136.845995	185349.111810	46.535604
3132.653920	179471.847708	46.540609
3128.301358	173594.058629	46.545613
3124.210905	167719.299683	46.550618
3119.842979	161877.038811	46.555623
3115.350913	156033.585954	46.560628
3110.969250	150191.965822	46.565633
3106.842700	144373.968115	46.570637
3102.405161	138572.160398	46.575642
3097.722711	132795.811405	46.580647
3093.272070	127025.334397	46.585652
3088.692154	121267.337930	46.590657
3084.005116	115536.046371	46.595661
3079.290312	109823.553575	46.600666
3074.576352	104167.927550	46.605671
3069.812390	98497.975761	46.610676
3064.908617	92869.841152	46.615681
3059.821281	87271.031011	46.620685
3054.793363	81713.902614	46.625690
3049.410031	76192.685193	46.630695
3044.038582	70696.589608	46.635700
3038.652343	65268.376488	46.640705
3032.157470	59894.053966	46.645709
3025.831402	54568.962294	46.650714
3015.564865	49419.956568	46.655719
3000.338536	44497.942369	46.660724
2984.726087	39739.406271	46.665729
2970.280356	35186.176410	46.670733
2956.253089	30850.723555	46.675738
2942.355011	26755.294947	46.680743
2929.599570	22896.173403	46.685748
2917.015347	19261.678907	46.690753
2904.772617	15888.188628	46.695757
2893.609749	12726.829120	46.700762
2882.317476	9801.900322	46.705767
2871.236857	7086.766303	46.710772
2860.477670	4600.166983	46.715777
2848.200740	2360.237163	46.720781
2825.823309	647.204464	46.725786
2765.237866	289.183598	46.730791
2716.060046	295.296282	46.735796
2697.065580	280.762450	46.740801
2701.105003	279.531591	46.745805
2716.505867	267.951572	46.750810
2734.062858	279.933493	46.755815
2747.756280	272.894269	46.760820
2754.300256	277.924322	46.765825
2755.311045	259.617644	46.770829
2752.902863	272.241221	46.775834
2748.750108	260.626700	46.780839
2744.236500	262.415353	46.785844
2740.698781	258.724191	46.790849
2737.649441	266.853782	46.795853
2735.256075	255.591470	46.800858
2732.222856	260.953576	46.805863
2729.740380	263.769447	46.810868
2727.262571	258.917045	46.815873
2724.034177	267.387827	46.820877
2721.420438	255.658100	46.825882
2718.221644	253.574662	46.830887
2715.059710	252.198751	46.835892
2711.762882	258.127712	46.840897
2708.233738	255.076635	46.845901
2706.127018	246.165389	46.850906
2703.093305	250.685329	46.855911
2699.558669	252.159181	46.860916
2696.081394	243.188888	46.865921
2692.435604	247.283205	46.870925
2689.342143	249.598695	46.875930
2686.033556	233.424034	46.880935
2683.235348	240.198380	46.885940
2679.995796	240.558167	46.890945
2676.238096	254.451026	46.895949
2673.213640	251.786272	46.900954
2669.338995	247.901784	46.905959
2666.422643	242.084810	46.910964
2663.448798	236.498808	46.915969
2659.632716	238.779251	46.920973
2656.643788	221.109223	46.925978
2652.607488	243.581725	46.930983
2649.552271	235.779747	46.935988
2646.385446	232.858489	46.940993
2642.767960	238.037946	46.945997
2639.403452	232.352697	46.951002
2635.698194	252.007192	46.956007
2632.468045	241.312668	46.961012
2629.277317	237.324610	46.966017
2625.298265	237.834965	46.971021
2622.551316	230.183635	46.976026
2619.122337	228.571510	46.981031
2615.416949	234.598843	46.986036
2611.964477	227.260283	46.991041
2608.401907	235.590548	46.996045
2605.152087	223.075979	47.001050
2602.210422	237.568610	47.006055
2598.497130	226.852754	47.011060
2594.932069	230.411892	47.016065
2591.166939	234.909809	47.021069
2587.946548	222.649772	47.026074
2584.127184	228.728862	47.031079
2581.052739	219.385789	47.036084
2577.703995	227.645088	47.041089
2574.059979	229.121935	47.046093
2571.221443	222.742945	47.051098
2567.858873	224.451703	47.056103
2564.227210	227.228421	47.061108
2560.792742	213.697067	47.066113
2557.164178	227.185261	47.071117
2553.393597	218.387342	47.076122
2550.055075	219.915641	47.081127
2546.575234	219.472362	47.086132
2543.139665	223.706108	47.091137
2539.350536	227.802615	47.096141
2536.533834	219.335576	47.101146
2532.430451	217.012083	47.106151
2529.255086	206.413382	47.111156
2525.988154	211.746597	47.116161
2522.140817	210.977781	47.121165
2519.197621	206.783119	47.126170
2515.018178	218.614815	47.131175
2511.673004	201.932315	47.136180
2509.149420	209.659345	47.141185
2504.891605	221.785938	47.146189
2501.684797	214.733986	47.151194
2497.759930	226.138255	47.156199
2494.769903	220.091702	47.161204
2490.904917	217.833301	47.166209
2487.255564	221.555851	47.171213
2483.909920	214.691168	47.176218
2480.706706	215.148045	47.181223
2477.473620	223.742391	47.186228
2474.111249	218.814971	47.191233
2470.358078	231.265729	47.196237
2466.813679	212.398840	47.201242
2463.199791	211.843234	47.206247
2459.485200	220.003469	47.211252
2456.355100	218.644226	47.216257
2452.750271	204.573652	47.221261
2449.734583	204.499419	47.226266
2445.490523	199.386025	47.231271
2442.344170	208.088211	47.236276
2438.822467	199.615549	47.241281
2435.329652	217.433219	47.246285
2432.396721	206.463392	47.251290
2428.604435	219.945965	47.256295
2424.915590	223.791868	47.261300
2421.474267	211.868189	47.266305
2417.508150	218.536667	47.271309
2414.626200	202.378271	47.276314
2411.116848	211.151283	47.281319
2407.403423	202.630539	47.286324
2404.497656	200.689926	47.291329
2400.277360	202.277379	47.296333
2396.688049	198.623327	47.301338
2392.988137	212.794207	47.306343
2390.087451	204.548476	47.311348
2387.072968	209.973397	47.316353
2383.112861	214.681932	47.321357
2379.488767	198.993034	47.326362
2376.074964	201.413460	47.331367
2372.802202	207.733193	47.336372
2369.132963	208.416836	47.341377
2365.309307	199.638448	47.346381
2362.385965	205.737869	47.351386
2359.094664	212.133082	47.356391
2355.548756	204.383085	47.361396
2351.823256	193.510772	47.366401
2348.445366	204.901336	47.371405
2344.704053	199.677367	47.376410
2341.105359	202.980019	47.381415
2337.565952	200.023668	47.386420
2334.224135	197.018257	47.391425
2330.590481	207.571963	47.396429
2327.273000	186.999262	47.401434
2323.803258	197.679345	47.406439
2320.239399	201.987708	47.411444
2316.980937	203.205149	47.416449
2313.250993	200.658097	47.421453
2309.529361	190.822568	47.426458
2306.053896	207.083333	47.431463
2302.906653	203.740594	47.436468
2299.448934	197.984379	47.441473
2295.388309	203.313025	47.446477
2292.230166	202.244096	47.451482
2288.957647	200.808771	47.456487
2285.585876	191.740534	47.461492
2282.077624	205.413970	47.466497
2278.197025	202.394150	47.471501
2274.462991	195.978115	47.476506
2271.203352	193.739272	47.481511
2267.616294	202.949183	47.486516
2264.433237	190.264981	47.491521
2260.954842	196.224428	47.496525
2257.487082	189.458646	47.501530
2254.072983	190.735721	47.506535
2250.249639	196.486578	47.511540
2247.019986	193.286406	47.516545
2242.960970	206.009258	47.521549
2240.241397	204.379655	47.526554
2236.588133	197.357085	47.531559
2232.604757	196.508351	47.536564
2229.466071	196.435156	47.541569
2225.927790	199.679059	47.546573
2222.442132	190.224847	47.551578
2218.959273	190.549585	47.556583
2215.604536	186.586813	47.561588
2211.849027	190.500232	47.566593
2208.316863	202.197166	47.571597
2205.047213	196.094274	47.576602
2201.469038	196.539122	47.581607
2197.757725	203.816121	47.586612
2194.628942	195.090055	47.591617
2190.697757	200.188443	47.596621
2187.206647	188.963346	47.601626
2183.907587	201.573694	47.606631
2180.094544	189.984673	47.611636
2177.086624	183.565839	47.616641
2173.341062	186.695670	47.621645
2170.094677	187.876354	47.626650
2166.688294	192.919264	47.631655
2163.093533	179.342303	47.636660
2159.538861	183.896552	47.641665
2155.687428	197.068914	47.646669
2152.445303	182.953719	47.651674
2148.803366	203.494253	47.656679
2145.573633	182.484454	47.661684
2142.302396	184.846734	47.666689
2138.251702	191.481036	47.671693
2135.017464	184.901151	47.676698
2131.361655	186.358641	47.681703
2127.687665	190.392630	47.686708
2124.574127	184.063066	47.691713
2120.994921	196.362893	47.696717
2117.416204	179.884538	47.701722
2113.861657	172.937518	47.706727
2110.582520	185.552088	47.711732
2107.089747	182.096552	47.716737
2103.308630	182.127607	47.721741
2099.973998	172.190298	47.726746
2096.241901	188.925166	47.731751
2093.019754	176.707366	47.736756
2089.268831	179.207300	47.741761
2086.004563	180.201645	47.746765
2082.869099	173.343265	47.751770
2078.601107	184.101433	47.756775
2075.421706	174.389318	47.761780
2072.145416	173.578236	47.766785
2068.633137	177.175156	47.771789
2064.869203	176.125163	47.776794
2061.195721	177.573565	47.781799
2057.540786	179.731220	47.786804
2054.578430	174.821701	47.791809
2050.935298	181.749305	47.796813
2047.891337	169.108695	47.801818
2043.938985	164.762852	47.806823
2040.524554	177.633674	47.811828
2036.953655	173.158311	47.816833
2033.107025	180.274188	47.821837
2030.351803	175.113462	47.826842
2026.313398	174.984062	47.831847
2022.596965	174.341211	47.836852
2019.327764	178.338758	47.841857
2015.783983	183.499992	47.846861
2012.572559	172.436449	47.851866
2009.213242	171.077038	47.856871
2005.415425	172.742406	47.861876
2001.991983	181.020525	47.866881
1998.413511	190.298374	47.871885
1995.313275	182.887656	47.876890
1991.701442	191.658879	47.881895
1987.890591	187.518506	47.886900
1984.607351	176.706069	47.891905
1980.745903	188.896227	47.896909
1977.202014	175.178301	47.901914
1973.864879	172.912428	47.906919
1970.390725	178.633817	47.911924
1967.139890	178.348969	47.916929
1963.645892	171.225017	47.921933
1960.252710	169.053539	47.926938
1956.406817	174.494609	47.931943
1952.911420	177.178083	47.936948
1949.665598	175.332239	47.941953
1945.799907	187.869399	47.946957
1942.285831	172.678351	47.951962
1939.062230	172.780694	47.956967
1935.473300	176.383215	47.961972
1932.227948	173.655596	47.966977
1928.191573	184.238093	47.971981
1924.894763	172.916094	47.976986
1921.293065	171.641010	47.981991
1917.997850	185.279993	47.986996
1914.799805	177.121054	47.992001
1910.737377	173.919429	47.997005
1907.695589	177.215831	48.002010
1903.847026	173.616161	48.007015
1900.130250	169.533527	48.012020
1897.157192	162.072586	48.017025
1893.116487	173.958484	48.022029
1890.153747	178.665682	48.027034
1886.350569	171.018002	48.032039
1883.070044	169.163017	48.037044
1879.520118	166.617482	48.042049
1875.853768	175.560522	48.047053
1872.689180	161.252770	48.052058
1869.029501	170.848909	48.057063
1865.242977	172.467595	48.062068
1861.812976	160.274961	48.067073
1858.075526	170.389853	48.072077
1854.804698	159.454500	48.077082
1851.200573	172.312676	48.082087
1848.284802	161.895498	48.087092
1844.651873	157.155026	48.092097
1840.686161	160.101525	48.097101
1837.690479	153.302989	48.102106
1834.022655	160.615767	48.107111
1830.141331	171.158116	48.112116
1826.721643	158.205125	48.117121
1823.481776	169.257165	48.122125
1820.064235	155.980130	48.127130
1816.325039	161.116365	48.132135
1812.645713	171.460043	48.137140
1809.137444	163.693117	48.142145
1805.583896	163.533367	48.147149
1802.728010	164.695653	48.152154
1799.254880	165.643783	48.157159
1794.998810	161.021052	48.162164
1792.132338	161.170197	48.167169
1788.233814	166.944315	48.172173
1785.346760	157.632235	48.177178
1781.651362	162.217854	48.182183
1777.655581	166.627015	48.187188
1774.328481	167.353549	48.192193
1770.789446	165.886575	48.197197
1766.965381	169.329568	48.202202
1763.832746	161.754436	48.207207
1760.436046	169.008307	48.212212
1756.801697	159.698787	48.217217
1753.464551	160.779295	48.222221
1749.974162	163.007123	48.227226
1746.403420	160.816709	48.232231
1742.481130	159.199691	48.237236
1739.691394	152.995571	48.242241
1735.671414	167.481489	48.247245
1732.473504	152.934162	48.252250
1728.945331	171.910826	48.257255
1725.201877	157.002356	48.262260
1722.239978	164.545482	48.267265
1718.229342	158.867115	48.272269
1714.856922	157.596532	48.277274
1711.494567	161.046534	48.282279
1707.620487	168.324639	48.287284
1704.108939	156.896739	48.292289
1700.418129	168.654737	48.297293
1697.085699	163.861405	48.302298
1693.695547	162.706523	48.307303
1690.491898	154.537196	48.312308
1687.027648	164.233852	48.317313
1683.457739	167.994061	48.322317
1680.019667	167.275069	48.327322
1676.256939	155.532876	48.332327
1672.589545	147.402104	48.337332
1669.338236	155.387236	48.342337
1665.858844	170.548970	48.347341
1662.563170	151.181724	48.352346
1658.762003	161.480055	48.357351
1654.857823	159.226026	48.362356
1651.813822	151.042907	48.367361
1647.985721	158.660328	48.372365
1644.902674	153.594720	48.377370
1641.277192	169.561344	48.382375
1637.893685	162.679407	48.387380
1634.592336	152.375500	48.392385
1630.574290	160.426600	48.397389
1627.089675	157.942341	48.402394
1623.577848	160.844045	48.407399
1619.938236	162.847646	48.412404
1617.038769	149.043856	48.417409
1613.112851	154.011809	48.422413
1609.857333	144.442756	48.427418
1606.344092	155.629454	48.432423
1602.697030	143.481297	48.437428
1599.465011	133.897231	48.442433
1595.506025	150.635929	48.447437
1592.483111	152.567764	48.452442
1588.559228	151.734239	48.457447
1584.879981	154.571048	48.462452
1581.872191	154.363176	48.467457
1578.179725	160.152717	48.472461
1575.100695	150.029500	48.477466
1571.387160	155.152439	48.482471
1567.287388	159.591890	48.487476
1563.655912	146.991108	48.492481
1560.608336	166.367384	48.497485
1557.392101	152.600312	48.502490
1553.911996	157.915398	48.507495
1550.491491	155.349073	48.512500
1547.044009	151.875412	48.517505
1543.157776	166.254983	48.522509
1539.729220	156.105013	48.527514
1536.425291	157.216937	48.532519
1532.822142	150.964244	48.537524
1529.447752	147.544630	48.542529
1525.456451	149.613519	48.547533
1522.128507	150.301931	48.552538
1518.580072	156.270173	48.557543
1515.223371	158.689641	48.562548
1511.470060	157.176278	48.567553
1507.959389	162.186843	48.572557
1504.910845	156.344404	48.577562
1501.181484	147.967256	48.582567
1497.543259	158.174635	48.587572
1494.174899	158.691259	48.592577
1490.353845	161.891985	48.597581
1486.935901	146.052905	48.602586
1483.607417	153.877304	48.607591
1480.319996	153.980915	48.612596
1477.117837	148.339259	48.617601
1473.446876	150.235833	48.622605
1469.840347	163.019263	48.627610
1465.816431	161.094988	48.632615
1462.136901	163.394419	48.637620
1459.181342	165.782139	48.642625
1455.352827	159.254924	48.647629
1452.387471	159.864879	48.652634
1448.916507	147.219626	48.657639
1444.996926	157.212908	48.662644
1441.678859	146.753137	48.667649
1437.859154	156.053346	48.672653
1434.762813	155.613115	48.677658
1431.217175	155.896896	48.682663
1427.654168	149.185986	48.687668
1423.991504	151.234233	48.692673
1420.494829	150.596964	48.697677
1417.007422	151.125578	48.702682
1413.547443	151.970106	48.707687
1410.167477	149.281636	48.712692
1406.774759	141.432643	48.717697
1402.877695	152.941546	48.722701
1399.246946	151.105041	48.727706
1395.656996	150.695589	48.732711
1392.288734	158.100195	48.737716
1389.072160	151.017706	48.742721
1385.701166	158.736891	48.747725
1382.224384	157.539931	48.752730
1378.583511	150.084510	48.757735
1375.033726	164.142437	48.762740
1371.973293	147.747977	48.767745
1368.163436	155.492249	48.772749
1364.875251	149.489361	48.777754
1361.071464	151.961580	48.782759
1357.396080	160.600484	48.787764
1354.057773	149.741483	48.792769
1350.432486	154.964995	48.797773
1346.986009	148.893927	48.802778
1343.221219	145.699563	48.807783
1339.840182	136.722315	48.812788
1336.213833	138.537601	48.817793
1332.813698	147.782608	48.822797
1329.496696	146.138727	48.827802
1326.793441	142.142287	48.832807
1322.955353	140.187821	48.837812
1319.146361	136.023966	48.842817
1315.336610	154.007562	48.847821
1312.267406	152.640463	48.852826
1308.350880	167.738618	48.857831
1304.325064	148.187783	48.862836
1301.518801	146.400614	48.867841
1297.855788	155.517564	48.872845
1294.399309	148.183098	48.877850
1291.218224	146.553699	48.882855
1287.420254	149.208498	48.887860
1284.132596	137.311405	48.892865
1280.285452	156.912455	48.897869
1277.157755	146.857520	48.902874
1273.641121	144.280571	48.907879
1269.937353	145.558954	48.912884
1266.942172	146.726192	48.917889
1263.015367	152.120075	48.922893
1259.506380	142.560013	48.927898
1255.954768	146.005938	48.932903
1252.023660	143.526425	48.937908
1248.648531	133.717961	48.942913
1245.188029	152.247412	48.947917
1242.201304	158.417052	48.952922
1238.833444	144.783339	48.957927
1235.046222	148.598077	48.962932
1231.575737	147.030193	48.967937
1227.890927	153.348519	48.972941
1224.368509	148.836999	48.977946
1220.853364	148.498754	48.982951
1217.128912	147.822140	48.987956
1214.172671	140.300569	48.992961
1210.712000	152.090510	48.997965
1206.636902	139.853450	49.002970
1203.751253	135.880367	49.007975
1199.669266	149.729540	49.012980
1196.409901	136.457189	49.017985
1192.755544	139.952760	49.022989
1189.184383	147.632254	49.027994
1185.675330	142.986154	49.032999
1182.158172	144.630279	49.038004
1178.917028	150.451259	49.043009
1175.339123	142.306120	49.048013
1172.046164	134.577240	49.053018
1168.413671	141.171873	49.058023
1164.957329	144.886048	49.063028
1161.592597	140.965436	49.068033
1157.871910	144.036011	49.073037
1154.654006	151.902859	49.078042
1151.192109	145.676895	49.083047
1147.357211	142.473106	49.088052
1143.520766	143.023766	49.093057
1140.054839	154.789248	49.098061
1136.629499	147.026101	49.103066
1133.159636	144.270436	49.108071
1129.566705	142.671124	49.113076
1126.527669	134.373226	49.118081
1122.913417	144.114488	49.123085
1119.472877	139.845823	49.128090
1116.108417	141.493382	49.133095
1111.914597	141.848525	49.138100
1108.771353	137.949879	49.143105
1105.189525	144.185255	49.148109
1101.849213	143.662133	49.153114
1098.624720	143.670791	49.158119
1094.735576	143.750805	49.163124
1091.655523	130.850947	49.168129
1087.794900	141.189617	49.173133
1084.106806	130.136277	49.178138
1080.751556	137.304642	49.183143
1077.252754	146.572156	49.188148
1073.879727	135.980211	49.193153
1070.205821	148.450326	49.198157
1066.912734	126.774719	49.203162
1063.447209	142.480208	49.208167
1059.736897	147.756764	49.213172
1056.456433	132.106116	49.218177
1052.681504	132.907025	49.223181
1049.109186	129.848775	49.228186
1045.341647	136.046271	49.233191
1042.109519	141.517261	49.238196
1039.007243	128.277287	49.243201
1035.484552	141.186033	49.248205
1031.881148	125.167858	49.253210
1028.440056	128.152773	49.258215
1024.997447	131.295396	49.263220
1021.179714	126.816972	49.268225
1017.630996	132.582147	49.273229
1014.475322	120.928234	49.278234
1010.539381	131.454386	49.283239
1006.737401	133.241223	49.288244
1003.862348	120.479143	49.293249
1000.203643	132.673289	49.298253
996.906093	118.497868	49.303258
993.167260	128.433579	49.308263
989.284118	132.130499	49.313268
986.096419	126.834684	49.318273
982.813019	135.377746	49.323277
978.884269	132.729604	49.328282
975.723444	140.690484	49.333287
972.174468	138.479828	49.338292
968.964294	135.985337	49.343297
965.108976	139.048445	49.348301
961.944542	133.307212	49.353306
958.218221	137.124663	49.358311
954.435991	133.479786	49.363316
951.372638	120.370084	49.368321
947.402907	131.867594	49.373325
944.125659	133.801441	49.378330
940.879235	115.082868	49.383335
937.026196	134.546964	49.388340
933.398690	129.801690	49.393345
929.657901	139.969207	49.398349
926.324034	128.712063	49.403354
923.501902	132.155589	49.408359
919.841482	141.826227	49.413364
916.353562	121.413747	49.418369
912.819806	140.920935	49.423373
909.371920	135.354393	49.428378
905.572818	135.988402	49.433383
901.926295	138.633491	49.438388
898.699146	133.242520	49.443393
895.145692	131.883658	49.448397
891.470765	132.729705	49.453402
887.895614	123.788535	49.458407
884.552682	138.702838	49.463412
881.508553	133.424904	49.468417
877.405033	131.923462	49.473421
874.175497	127.962137	49.478426
870.856791	131.395733	49.483431
867.370377	127.984220	49.488436
863.509920	134.100071	49.493441
859.806519	146.761209	49.498445
856.375331	136.398710	49.503450
852.920998	136.547647	49.508455
849.363697	133.321780	49.513460
846.442340	136.245425	49.518465
842.613009	134.820370	49.523469
839.215800	130.820257	49.528474
835.545902	134.180355	49.533479
831.815967	140.558308	49.538484
828.749106	131.748602	49.543489
824.905158	137.057204	49.548493
821.614180	143.464686	49.553498
818.295062	128.403445	49.558503
814.422119	135.730221	49.563508
811.277428	122.840028	49.568513
807.162108	142.073722	49.573517
803.822208	131.708615	49.578522
800.763165	133.423093	49.583527
797.028133	133.618020	49.588532
793.733481	131.512759	49.593537
789.881027	133.605104	49.598541
786.408068	125.901736	49.603546
783.155637	120.802294	49.608551
779.470710	129.536444	49.613556
776.291102	124.264564	49.618561
772.463071	134.122075	49.623565
768.860008	135.051129	49.628570
765.189722	127.347902	49.633575
761.738246	146.910518	49.638580
758.525339	126.488150	49.643585
755.069879	131.804155	49.648589
751.476471	125.220225	49.653594
747.824671	124.480675	49.658599
744.328966	125.486623	49.663604
741.346688	122.757794	49.668609
737.213787	131.475282	49.673613
733.929557	126.362865	49.678618
730.729503	123.265023	49.683623
726.792215	131.861914	49.688628
723.972817	121.553263	49.693633
720.054452	125.555961	49.698637
716.440628	130.056797	49.703642
712.842603	127.536419	49.708647
709.182523	126.510279	49.713652
706.106730	126.079817	49.718657
702.648623	125.326850	49.723661
698.922167	132.725187	49.728666
695.618449	125.776760	49.733671
691.594821	131.064297	49.738676
688.485836	124.450025	49.743681
684.500880	123.712456	49.748685
681.008937	120.496020	49.753690
677.868646	108.654403	49.758695
674.240079	118.766789	49.763700
671.373011	116.734125	49.768705
667.744816	124.091679	49.773709
664.066289	122.726670	49.778714
660.448745	124.257115	49.783719
656.873495	129.162414	49.788724
653.389847	119.513619	49.793729
649.917273	128.700512	49.798733
646.613076	126.633014	49.803738
642.979723	114.931155	49.808743
638.646896	137.318273	49.813748
635.737240	119.472541	49.818753
632.406116	125.034733	49.823757
628.800242	123.973642	49.828762
625.852232	123.715281	49.833767
621.987934	131.084725	49.838772
618.544629	115.602853	49.843777
614.634930	114.612571	49.848781
611.036821	123.465347	49.853786
607.695368	128.138096	49.858791
604.370150	125.099862	49.863796
600.738136	119.612950	49.868801
597.341829	124.396576	49.873805
593.906048	115.858478	49.878810
590.464759	108.098509	49.883815
586.701985	122.745828	49.888820
583.304819	116.784176	49.893825
579.645770	119.044274	49.898829
576.283542	114.718592	49.903834
573.128162	120.674918	49.908839
569.034358	123.313653	49.913844
566.031082	115.475920	49.918849
562.452193	126.335564	49.923853
559.078086	120.539705	49.928858
555.362516	112.033246	49.933863
551.580823	113.679061	49.938868
548.664566	114.011473	49.943873
544.625704	118.060215	49.948877
541.116548	117.613906	49.953882
537.618474	125.423183	49.958887
533.677651	141.801277	49.963892
530.678059	120.856678	49.968897
527.237902	126.269608	49.973901
524.217729	126.773000	49.978906
520.642347	119.905758	49.983911
516.579784	121.235723	49.988916
513.607981	117.461889	49.993921
509.927210	122.624522	49.998925
506.081262	124.713386	50.003930
502.780836	113.812866	50.008935
498.748712	131.037715	50.013940
495.792167	125.393313	50.018945
492.295064	120.999390	50.023949
488.847136	122.105016	50.028954
485.240157	123.017111	50.033959
481.734365	121.572274	50.038964
478.200455	115.543298	50.043969
474.550995	123.641910	50.048973
471.340845	122.291589	50.053978
468.050823	119.663945	50.058983
464.165227	116.479610	50.063988
460.845608	110.657054	50.068993
457.148035	113.614567	50.073997
453.522927	129.276772	50.079002
449.803504	114.459598	50.084007
446.300563	120.670604	50.089012
443.161615	112.257498	50.094017
439.685472	120.885985	50.099021
436.428807	120.088637	50.104026
432.575990	125.528345	50.109031
428.873264	121.893153	50.114036
426.033112	111.387631	50.119041
422.330202	112.721774	50.124045
418.516960	118.423984	50.129050
415.294161	116.448429	50.134055
411.645292	116.119882	50.139060
408.290910	113.740072	50.144065
404.771984	118.960077	50.149069
401.200279	121.527757	50.154074
397.324693	117.003740	50.159079
394.004830	128.872537	50.164084
390.636887	114.992682	50.169089
387.290560	124.356833	50.174093
383.376145	123.256681	50.179098
380.449161	117.401071	50.184103
376.766598	121.679125	50.189108
373.431626	123.197967	50.194113
369.480639	134.881487	50.199117
366.278899	128.923780	50.204122
362.850879	115.255126	50.209127
358.843241	119.580579	50.214132
355.564353	118.091520	50.219137
351.972316	108.655577	50.224141
348.688940	125.028312	50.229146
345.098941	122.944361	50.234151
341.093254	123.994819	50.239156
338.259276	119.149985	50.244161
334.417177	127.069170	50.249165
330.901045	127.833057	50.254170
327.660773	115.914937	50.259175
324.150484	118.577579	50.264180
320.733506	128.752052	50.269185
316.822117	126.686981	50.274189
313.479226	130.507719	50.279194
310.310838	125.753858	50.284199
306.802006	125.161021	50.289204
303.270789	120.923295	50.294209
299.179340	121.901427	50.299213
295.558363	119.833081	50.304218
292.370424	115.206967	50.309223
288.903908	126.400760	50.314228
286.087898	117.052798	50.319233
282.199929	120.942888	50.324237
278.417561	118.499589	50.329242
275.213973	112.862876	50.334247
271.473013	131.863865	50.339252
267.759524	124.689397	50.344257
264.359979	128.694041	50.349261
261.092101	127.039442	50.354266
257.726461	122.965483	50.359271
253.820248	129.003677	50.364276
250.435038	124.482788	50.369281
246.846354	118.479577	50.374285
243.390134	119.004534	50.379290
240.165324	114.304927	50.384295
236.368581	125.825100	50.389300
233.027577	117.086390	50.394305
229.437863	121.505550	50.399309
225.913250	128.558030	50.404314
222.472488	117.802908	50.409319
219.010167	129.927251	50.414324
215.581361	115.312225	50.419329
211.934027	120.177170	50.424333
208.167829	115.736820	50.429338
205.071786	110.630016	50.434343
201.673781	119.650482	50.439348
198.370263	110.359347	50.444353
194.657586	113.343276	50.449357
190.764637	115.546734	50.454362
187.374230	115.091456	50.459367
183.763964	119.912308	50.464372
180.527763	122.090127	50.469377
176.820279	123.228249	50.474381
173.314846	116.931936	50.479386
170.147402	111.254387	50.484391
166.360654	118.963153	50.489396
163.099273	125.673141	50.494401
159.280429	126.114715	50.499405
155.542576	125.179586	50.504410
152.473248	123.812968	50.509415
148.583125	122.902510	50.514420
145.141997	112.565409	50.519425
141.958424	126.076891	50.524429
138.506338	120.111257	50.529434
134.670644	119.826565	50.534439
131.566778	118.750583	50.539444
128.298205	116.339088	50.544449
124.677470	121.414062	50.549453
120.956740	126.003998	50.554458
117.175101	122.876402	50.559463
113.265168	124.529847	50.564468
110.300450	113.160735	50.569473
106.979506	123.449554	50.574477
103.664848	116.978215	50.579482
99.548103	112.654464	50.584487
96.202444	119.264163	50.589492
92.575721	119.800506	50.594497
89.448594	112.114322	50.599501
86.102627	120.452325	50.604506
82.631106	109.980888	50.609511
79.096454	108.872137	50.614516
75.700378	120.123040	50.619521
71.883320	117.703657	50.624525
68.481644	116.939935	50.629530
64.752526	111.910891	50.634535
61.156230	114.563614	50.639540
57.764238	112.211325	50.644545
54.063932	118.083302	50.649549
50.488724	108.260221	50.654554
47.540030	100.447702	50.659559
43.963957	107.128546	50.664564
40.330839	102.507086	50.669569
36.564069	111.817541	50.674573
33.120611	111.709700	50.679578
29.916593	115.131153	50.684583
25.861228	108.537212	50.689588
22.589662	107.748759	50.694593
19.240318	110.173248	50.699597
15.902926	113.073848	50.704602
12.396716	103.526875	50.709607
8.771463	102.374733	50.714612
5.626372	107.408649	50.719617
2.012281	104.863922	50.724621