Thu Jun 16 18:32:43 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
-0.006975	78.145161	0.000000
-0.154743	100.997337	0.005005
0.558858	89.724024	0.010010
0.169604	107.721327	0.015014
0.252174	94.937988	0.020019
0.461531	96.622934	0.025024
0.020848	80.012808	0.030029
0.228706	80.780603	0.035034
0.048502	79.777537	0.040038
-0.661371	60.763981	0.045043
-0.376638	41.324850	0.050048
-1.001559	29.081513	0.055053
-0.966565	20.162031	0.060058
-1.699640	16.865150	0.065062
-1.988274	7.695495	0.070067
-1.858902	0.823697	0.075072
-2.627679	-10.217108	0.080077
-3.022291	-16.924372	0.085082
-3.197383	-7.497805	0.090086
-3.553821	-7.011849	0.095091
-3.871472	-10.783830	0.100096
-4.763075	-11.990452	0.105101
-4.655691	-12.645036	0.110106
-4.670024	-14.407032	0.115110
-4.754303	-16.657944	0.120115
-4.673067	-18.498674	0.125120
-4.981254	-15.248592	0.130125
-5.341530	-22.011447	0.135130
-5.735942	-19.450032	0.140134
-5.981950	-21.471186	0.145139
-5.987192	-7.997359	0.150144
-6.757958	-17.907344	0.155149
-6.742700	-17.325753	0.160154
-7.040775	-14.727181	0.165158
-7.387190	-9.653067	0.170163
-7.202084	-19.372660	0.175168
-8.083885	-24.883527	0.180173
-8.612266	-20.786315	0.185178
-8.839145	-23.732952	0.190182
-8.881171	-14.455051	0.195187
-8.621481	-23.702572	0.200192
-8.939844	-11.718485	0.205197
-8.720421	-13.189208	0.210202
-9.769560	-12.823283	0.215206
-10.006517	-12.611008	0.220211
-10.570338	-13.779356	0.225216
-10.612271	-6.553584	0.230221
-10.399952	-10.970543	0.235226
-10.489783	-12.774224	0.240230
-11.333676	-16.406559	0.245235
-12.074876	-11.466587	0.250240
-12.240843	-15.534145	0.255245
-12.340888	-14.610997	0.260250
-12.385843	-17.148587	0.265254
-12.514909	-10.506167	0.270259
-12.519121	-5.287444	0.275264
-12.439449	-0.938610	0.280269
-12.043452	-13.353383	0.285274
-12.779769	-14.851243	0.290278
-13.294671	-9.480156	0.295283
-13.582018	-20.888383	0.300288
-14.688563	-8.721855	0.305293
-15.007908	-17.863727	0.310298
-15.204797	-6.311495	0.315302
-15.343183	-16.781667	0.320307
-15.209762	-12.909737	0.325312
-15.486193	-9.296032	0.330317
-15.298838	-15.423583	0.335322
-15.376317	-12.031581	0.340326
-15.754356	-0.453453	0.345331
-16.397191	-11.924187	0.350336
-16.635521	-8.979245	0.355341
-16.374595	-22.029815	0.360346
-17.226428	-17.093365	0.365350
-18.144636	-6.248067	0.370355
-17.794874	-22.579185	0.375360
-17.902567	-9.426027	0.380365
-18.262534	-17.252235	0.385370
-18.299379	-11.676319	0.390374
-18.600226	-8.353458	0.395379
-18.401119	-10.299201	0.400384
-19.333801	-13.213454	0.405389
-19.754568	-14.974778	0.410394
-20.308438	-11.089108	0.415398
-20.467380	-16.223395	0.420403
-19.772264	-17.789697	0.425408
-20.368691	-17.314494	0.430413
-20.145720	-23.865434	0.435418
-20.481307	-17.307471	0.440422
-21.463481	-17.888745	0.445427
-22.032546	-7.226140	0.450432
-22.058837	-7.440536	0.455437
-22.011030	-12.829089	0.460442
-21.938560	-11.281159	0.465446
-21.938814	-7.915730	0.470451
-22.173374	-2.384385	0.475456
-23.228152	-3.546083	0.480461
-23.780583	-15.848121	0.485466
-23.611852	-21.501417	0.490470
-23.942048	-20.550299	0.495475
-23.655037	-25.011167	0.500480
-23.984977	-17.755367	0.505485
-23.701050	-16.268229	0.510490
-24.768003	-15.223672	0.515494
-25.167764	-10.224599	0.520499
-24.798159	-24.769692	0.525504
-25.412700	-14.670985	0.530509
-25.678682	-15.070308	0.535514
-26.064551	-13.266787	0.540518
-26.743932	-11.057336	0.545523
-26.709968	-21.608273	0.550528
-26.833427	-11.970538	0.555533
-26.617860	-19.108140	0.560538
-26.815891	-14.092585	0.565542
-27.275485	-20.741751	0.570547
-27.331872	-23.802096	0.575552
-28.246230	-9.781544	0.580557
-28.408176	-11.947899	0.585562
-28.762809	-9.653208	0.590566
-28.761166	-6.293814	0.595571
-28.767619	-12.660935	0.600576
-29.028980	-16.229220	0.605581
-29.334484	-18.251689	0.610586
-29.644923	-17.258059	0.615590
-30.035176	-13.897240	0.620595
-29.828592	-18.587214	0.625600
-30.136478	-17.636034	0.630605
-30.650895	-26.304872	0.635610
-31.199646	-13.227011	0.640614
-31.867012	-18.989859	0.645619
-31.763635	-18.062840	0.650624
-31.686800	-12.298340	0.655629
-31.599042	-13.840928	0.660634
-31.848265	-8.702472	0.665638
-32.393903	-7.029902	0.670643
-32.525756	-16.220613	0.675648
-33.092165	-15.263114	0.680653
-33.186812	-11.025467	0.685658
-32.980625	-8.107616	0.690662
-33.579795	-5.636666	0.695667
-34.291403	-8.413621	0.700672
-34.692283	-5.509591	0.705677
-34.511087	-15.404144	0.710682
-34.934383	-8.493692	0.715686
-34.688095	-1.001827	0.720691
-34.682255	-11.014005	0.725696
-35.385773	-2.775717	0.730701
-35.749399	-13.285518	0.735706
-36.235119	-4.534506	0.740710
-36.214662	-20.438388	0.745715
-36.059634	-20.965788	0.750720
-36.255915	-7.110762	0.755725
-36.860680	-12.398971	0.760730
-37.673694	-10.664457	0.765734
-37.946956	-6.378548	0.770739
-38.007106	-6.280433	0.775744
-38.142036	-6.658794	0.780749
-37.847632	-22.357658	0.785754
-37.899133	-19.111324	0.790758
-38.606281	-6.945685	0.795763
-38.915172	-18.469820	0.800768
-39.298888	-10.003022	0.805773
-39.557527	-12.252052	0.810778
-39.567295	-15.187411	0.815782
-39.954976	-17.601967	0.820787
-40.216871	-18.740395	0.825792
-40.946759	-15.130283	0.830797
-41.165712	-22.050658	0.835802
-40.992102	-4.528499	0.840806
-41.286281	-12.202304	0.845811
-40.982115	-10.831866	0.850816
-41.385706	-21.323119	0.855821
-42.058925	-13.376041	0.860826
-42.732016	-11.992085	0.865830
-42.892326	-11.834701	0.870835
-42.899989	-25.288377	0.875840
-43.018834	-20.392556	0.880845
-43.147759	-15.840753	0.885850
-42.737179	-13.490699	0.890854
-43.454002	-10.856368	0.895859
-43.870777	-14.429848	0.900864
-44.370644	-11.934169	0.905869
-44.390281	-20.631994	0.910874
-44.446270	-18.229895	0.915878
-45.061086	-23.540904	0.920883
-45.238004	-23.074945	0.925888
-45.834362	-13.325125	0.930893
-45.791804	-22.560735	0.935898
-46.077168	-19.358129	0.940902
-46.121849	-15.605441	0.945907
-46.192308	-19.642312	0.950912
-46.466590	-18.569815	0.955917
-47.317431	-19.682735	0.960922
-47.675238	-22.716943	0.965926
-48.111668	-15.933266	0.970931
-47.595286	-26.992970	0.975936
-47.868058	-19.919165	0.980941
-47.710442	-18.966088	0.985946
-47.942504	-18.758468	0.990950
-48.568058	-12.241571	0.995955
-48.562784	-19.483522	1.000960
-49.437395	-16.434120	1.005965
-49.237477	-14.245675	1.010970
-50.162582	-14.037864	1.015974
-50.801613	-13.219698	1.020979
-50.418828	-17.225616	1.025984
-50.968440	-16.131196	1.030989
-50.531990	-22.095792	1.035994
-50.700808	-19.871370	1.040998
-50.750979	-20.544706	1.046003
-51.291288	-16.655457	1.051008
-52.124795	-17.862694	1.056013
-52.308428	-12.309581	1.061018
-52.353915	-18.486650	1.066022
-52.521084	-6.647414	1.071027
-52.650215	-23.760641	1.076032
-52.952269	-8.637987	1.081037
-52.796885	-10.045052	1.086042
-53.460742	-19.081051	1.091046
-53.829387	-19.694949	1.096051
-54.107952	-26.135676	1.101056
-54.312392	-12.316995	1.106061
-54.349990	-20.248955	1.111066
-54.387508	-9.500267	1.116070
-55.348093	-5.840681	1.121075
-55.707348	-17.488787	1.126080
-55.879313	-13.676096	1.131085
-55.813132	-16.643144	1.136090
-55.890768	-18.722210	1.141094
-56.068967	-21.395724	1.146099
-55.908460	-22.923697	1.151104
-56.766136	-21.255102	1.156109
-57.088032	-17.164486	1.161114
-57.589691	-6.796061	1.166118
-57.676512	-10.571360	1.171123
-57.414471	-13.297504	1.176128
-57.468394	-4.777770	1.181133
-58.121324	-16.957729	1.186138
-58.405809	-16.648612	1.191142
-58.577320	-10.968264	1.196147
-58.839425	-17.161329	1.201152
-59.511653	-4.554554	1.206157
-59.994580	-10.128177	1.211162
-60.391542	-14.339969	1.216166
-60.351511	-9.555738	1.221171
-60.186405	-24.111821	1.226176
-60.369515	-13.919660	1.231181
-60.378533	-14.166407	1.236186
-60.230208	-17.955111	1.241190
-61.377910	-4.146970	1.246195
-61.708250	-16.884463	1.251200
-62.125326	-16.746699	1.256205
-61.817439	-12.785909	1.261210
-62.186011	-17.943262	1.266214
-62.682146	-3.811776	1.271219
-62.947616	-24.335457	1.276224
-63.431755	-14.672650	1.281229
-63.558271	-16.933548	1.286234
-63.946353	-17.062404	1.291238
-63.931001	-15.674525	1.296243
-63.931103	-18.276153	1.301248
-63.886047	-4.854546	1.306253
-64.165192	-20.268713	1.311258
-64.225341	-20.159450	1.316262
-65.130602	-23.441274	1.321267
-65.039193	-15.566102	1.326272
-65.440104	-14.732632	1.331277
-65.737349	-22.475276	1.336282
-66.298491	-8.933366	1.341286
-66.784232	-14.993284	1.346291
-66.818295	-20.628850	1.351296
-66.966131	-10.657681	1.356301
-67.186969	-16.581530	1.361306
-67.178218	-13.477250	1.366310
-67.292025	-13.958348	1.371315
-67.028328	-28.457025	1.376320
-67.924030	-11.786243	1.381325
-68.444110	-23.484616	1.386330
-68.396870	-21.340886	1.391334
-68.805046	-5.027985	1.396339
-68.908683	-11.994549	1.401344
-69.430098	-3.502526	1.406349
-69.904811	-8.731820	1.411354
-69.647830	-2.226498	1.416358
-70.141052	-13.824347	1.421363
-70.041192	-11.747026	1.426368
-70.148805	-9.182690	1.431373
-70.853445	-9.853033	1.436378
-71.227109	-11.407267	1.441382
-71.396790	-13.578458	1.446387
-71.367343	-19.846636	1.451392
-71.773682	-12.041626	1.456397
-71.743284	-10.828780	1.461402
-72.288679	-6.775906	1.466406
-73.030631	-10.802630	1.471411
-73.048443	-23.214510	1.476416
-73.302000	-3.450177	1.481421
-73.634926	-15.419906	1.486426
-73.630420	-5.885499	1.491430
-73.581587	-12.848354	1.496435
-73.553397	-15.938066	1.501440
-74.251922	-12.786846	1.506445
-75.095057	-14.844076	1.511450
-75.017295	-16.251828	1.516454
-74.729371	-6.935328	1.521459
-74.687682	-20.918550	1.526464
-75.332705	-8.967987	1.531469
-76.056330	-16.207370	1.536474
-76.309138	-12.864430	1.541478
-76.290304	-17.074200	1.546483
-76.475766	-23.048089	1.551488
-76.647924	-12.855172	1.556493
-76.854723	-17.408263	1.561498
-77.426968	-25.223547	1.566502
-77.995283	-18.916281	1.571507
-78.210751	-19.252721	1.576512
-78.434109	-9.227341	1.581517
-78.359582	-2.868755	1.586522
-78.079455	-19.982236	1.591526
-78.441100	-4.355867	1.596531
-78.613408	-16.554578	1.601536
-79.551742	-12.623224	1.606541
-79.786553	-11.688262	1.611546
-79.890822	-19.917103	1.616550
-80.062796	-20.193843	1.621555
-80.297809	-28.193206	1.626560
-80.437824	-23.362158	1.631565
-80.803303	-28.683092	1.636570
-81.217168	-24.096830	1.641574
-81.742912	-24.600217	1.646579
-81.614270	-24.722324	1.651584
-81.779468	-11.366606	1.656589
-81.682122	-13.457424	1.661594
-81.938119	-19.290320	1.666598
-82.669018	-22.474087	1.671603
-83.032614	-32.870419	1.676608
-83.494897	-18.001082	1.681613
-83.234841	-20.965838	1.686618
-83.373921	-16.912340	1.691622
-83.617356	-12.462071	1.696627
-83.999348	-16.330155	1.701632
-84.275668	-10.481348	1.706637
-84.643979	-12.453577	1.711642
-84.627657	-6.486307	1.716646
-84.964561	-4.427368	1.721651
-85.467113	-6.278758	1.726656
-85.916152	-7.643252	1.731661
-86.215814	-12.305697	1.736666
-86.376435	-23.401400	1.741670
-86.790665	-6.452067	1.746675
-86.281436	-10.995243	1.751680
-86.820652	-11.772438	1.756685
-86.688541	-13.015146	1.761690
-86.692773	-11.589304	1.766694
-87.672508	0.021075	1.771699
-88.006758	-12.446542	1.776704
-88.225763	-10.591277	1.781709
-88.346322	-10.059160	1.786714
-88.260893	-10.666709	1.791718
-89.115968	-9.181938	1.796723
-89.435847	-12.513839	1.801728
-89.716815	-10.442442	1.806733
-89.917678	-11.220013	1.811738
-89.593170	-17.547214	1.816742
-89.945259	-8.396639	1.821747
-89.729023	-22.405745	1.826752
-90.477935	-18.316477	1.831757
-90.898434	-14.794093	1.836762
-91.319213	-19.447074	1.841766
-91.539224	-8.732454	1.846771
-91.462176	-13.848617	1.851776
-91.548030	-14.282737	1.856781
-92.361263	-10.856353	1.861786
-92.683910	-7.117708	1.866790
-93.447529	-17.683230	1.871795
-92.711052	-12.922647	1.876800
-93.325698	-9.935736	1.881805
-93.306129	-20.039256	1.886810
-93.285997	-13.155328	1.891814
-93.498100	-23.975661	1.896819
-93.775818	-26.501021	1.901824
-94.563651	-17.893747	1.906829
-94.846869	-17.178084	1.911834
-94.516850	-25.817276	1.916838
-95.142385	-11.418271	1.921843
-95.030531	-23.714053	1.926848
-95.548971	-23.111346	1.931853
-96.315279	-11.422104	1.936858
-96.383901	-27.129525	1.941862
-96.344110	-15.942279	1.946867
-96.529442	-26.539438	1.951872
-96.094890	-21.525041	1.956877
-96.808002	-28.306421	1.961882
-97.125038	-23.498404	1.966886
-97.942701	-19.051989	1.971891
-97.907441	-28.080887	1.976896
-97.977830	-29.003141	1.981901
-98.344406	-25.912405	1.986906
-99.075150	-27.946276	1.991910
-99.723990	-23.132947	1.996915
-98.592132	-24.508397	2.006912
-98.861277	-21.616651	2.016909
-98.609899	-15.642630	2.026906
-98.171499	-24.116545	2.036902
-96.937175	-21.544543	2.046899
-96.641093	-25.558488	2.056896
-96.759093	-21.998378	2.066893
-95.700513	-15.672202	2.076890
-95.314299	-19.073933	2.086886
-94.845813	-15.061723	2.096883
-94.561074	-18.472516	2.106880
-93.972219	-15.637368	2.116877
-93.206620	-11.348431	2.126874
-92.554518	-11.821885	2.136870
-92.279165	-16.956286	2.146867
-92.182579	-16.328588	2.156864
-91.147176	-18.226391	2.166861
-91.079730	-15.556717	2.176858
-90.473019	-14.237005	2.186854
-89.490687	-18.652410	2.196851
-89.210131	-17.625814	2.206848
-89.103408	-11.937907	2.216845
-88.131867	-14.666326	2.226842
-87.763035	-8.613820	2.236838
-87.836166	-14.346141	2.246835
-86.418814	-18.122118	2.256832
-86.250257	-15.516371	2.266829
-86.074504	-28.281041	2.276826
-85.157776	-18.437096	2.286822
-84.822699	-13.869913	2.296819
-84.586542	-15.426362	2.306816
-83.392218	-10.157394	2.316813
-83.023815	-14.285927	2.326810
-83.160157	-17.403835	2.336806
-82.611709	-23.788940	2.346803
-81.835730	-22.387703	2.356800
-81.262207	-23.688844	2.366797
-80.336770	-27.957735	2.376794
-80.005759	-21.042453	2.386790
-79.857556	-18.216123	2.396787
-79.787132	-19.413277	2.406784
-78.797979	-11.096742	2.416781
-78.408757	-12.936947	2.426778
-77.577487	-8.818441	2.436774
-77.025212	-15.870805	2.446771
-76.620080	-12.776466	2.456768
-76.712841	-16.212095	2.466765
-75.659743	-18.612850	2.476762
-75.210242	-15.102716	2.486758
-75.017937	-19.746675	2.496755
-73.919148	-23.403967	2.506752
-73.602248	-14.869700	2.516749
-73.366120	-15.720995	2.526746
-73.049612	-11.058432	2.536742
-72.292083	-12.262209	2.546739
-72.090035	-21.135407	2.556736
-70.922267	-18.884105	2.566733
-70.537603	-12.193719	2.576730
-70.578906	-17.985729	2.586726
-69.840447	-12.931590	2.596723
-69.225429	-13.869456	2.606720
-69.002917	-13.861378	2.616717
-68.201179	-15.976060	2.626714
-67.578874	-13.587692	2.636710
-67.166973	-7.952489	2.646707
-66.990699	-6.799404	2.656704
-65.896452	-21.041516	2.666701
-65.836815	-19.925808	2.676698
-65.481262	-11.862839	2.686694
-64.461285	-8.961975	2.696691
-64.510860	-11.794127	2.706688
-63.979505	-12.928669	2.716685
-62.993033	-9.020578	2.726682
-62.774379	-7.622606	2.736678
-62.382638	-20.240185	2.746675
-61.485887	-19.811251	2.756672
-60.973260	-15.209547	2.766669
-60.737730	-17.679517	2.776666
-60.540854	-23.482289	2.786662
-59.832440	-20.059197	2.796659
-59.507043	-25.635367	2.806656
-58.617819	-13.779341	2.816653
-58.325388	-12.158314	2.826650
-57.952757	-7.931411	2.836646
-57.231634	-9.070346	2.846643
-56.750442	-8.828776	2.856640
-56.029457	-13.261196	2.866637
-55.425256	-15.600358	2.876634
-55.161391	-12.808451	2.886630
-55.271618	-13.092995	2.896627
-54.257157	-24.392270	2.906624
-53.668902	-19.472889	2.916621
-53.031316	-20.371167	2.926618
-52.507187	-11.777548	2.936614
-52.352119	-17.718078	2.946611
-52.014519	-20.702129	2.956608
-50.934745	-14.142864	2.966605
-50.237555	-20.456042	2.976602
-50.375710	-15.125505	2.986598
-50.044012	-13.945555	2.996595
-49.314869	-19.526168	3.006592
-48.826007	-19.384103	3.016589
-48.038970	-24.923459	3.026586
-47.294262	-14.826100	3.036582
-47.342766	-23.437660	3.046579
-46.896308	-22.219283	3.056576
-46.404308	-23.310523	3.066573
-45.695473	-20.114842	3.076570
-45.240919	-23.816997	3.086566
-44.446304	-17.518260	3.096563
-43.898408	-20.641821	3.106560
-43.992785	-22.613743	3.116557
-43.395718	-17.588096	3.126554
-42.773273	-21.334394	3.136550
-42.243121	-24.688689	3.146547
-41.050698	-29.796093	3.156544
-41.160143	-21.387202	3.166541
-41.240388	-18.607081	3.176538
-40.257924	-15.761506	3.186534
-39.357976	-13.294948	3.196531
-39.131445	-18.677667	3.206528
-38.810218	-22.021736	3.216525
-37.807866	-18.972353	3.226522
-37.564039	-27.899819	3.236518
-37.323250	-24.884855	3.246515
-36.933204	-21.442535	3.256512
-35.933300	-20.410497	3.266509
-35.833595	-16.801015	3.276506
-35.296461	-32.614076	3.286502
-34.513381	-19.615838	3.296499
-34.458486	-25.657460	3.306496
-33.624277	-21.190145	3.316493
-33.070934	-23.576020	3.326490
-32.933628	-7.365624	3.336486
-32.127163	-18.612453	3.346483
-31.580956	-18.476406	3.356480
-31.289206	-19.581177	3.366477
-30.543245	-21.159442	3.376474
-29.985511	-16.461715	3.386470
-29.759441	-16.339292	3.396467
-29.229937	-20.564185	3.406464
-28.380596	-16.325478	3.416461
-28.046230	-25.503403	3.426458
-28.035513	-14.709640	3.436454
-26.791932	-28.243171	3.446451
-26.529900	-22.604884	3.456448
-26.240100	-27.123795	3.466445
-25.765257	-25.742773	3.476442
-25.495535	-20.584152	3.486438
-24.673518	-24.064319	3.496435
-23.636496	-16.287867	3.506432
-23.267283	-13.146346	3.516429
-22.910237	-15.504870	3.526426
-23.170330	-22.044947	3.536422
-22.436313	-31.003090	3.546419
-21.705083	-27.754161	3.556416
-21.065529	-31.447817	3.566413
-20.377753	-13.095845	3.576410
-20.191378	-16.640183	3.586406
-19.972462	-15.233659	3.596403
-19.023752	-13.714860	3.606400
-18.590661	-13.510283	3.616397
-18.392845	-12.365745	3.626394
-17.366473	-9.777238	3.636390
-17.011440	-16.405487	3.646387
-16.808138	-21.654174	3.656384
-16.205794	-18.730764	3.666381
-15.278151	-12.068805	3.676378
-15.290161	-17.584134	3.686374
-14.631298	-13.793331	3.696371
-14.071579	-6.915285	3.706368
-13.733650	-13.469883	3.716365
-13.085488	-11.968884	3.726362
-12.197504	-15.407056	3.736358
-12.208689	-10.363665	3.746355
-11.870740	-16.305822	3.756352
-11.202624	-13.428445	3.766349
-10.498442	-12.529389	3.776346
-10.346611	-5.848079	3.786342
-9.395218	-18.525500	3.796339
-9.299204	-23.979603	3.806336
-8.785288	-19.808002	3.816333
-7.831693	-14.740855	3.826330
-7.210841	-11.403842	3.836326
-7.312031	-15.533006	3.846323
-6.938585	-12.366006	3.856320
-5.975873	-7.691289	3.866317
-5.773462	-13.804265	3.876314
-4.876429	-10.786416	3.886310
-4.452592	-17.890602	3.896307
-4.465242	-14.139421	3.906304
-3.707024	-19.424345	3.916301
-3.140027	-11.706332	3.926298
-2.661685	-6.909095	3.936294
-2.129176	8.383090	3.946291
-2.060195	15.485673	3.956288
-1.735912	25.812077	3.966285
-1.359969	43.090188	3.976282
-0.896816	73.781784	3.986278
-0.487057	105.259876	3.996275
0.000000	112.337388	4.001280
0.251010	133.156816	4.006285
0.595385	153.417843	4.011290
0.889678	156.475170	4.016294
0.496525	161.251625	4.021299
0.944200	169.086177	4.026304
0.743666	182.626775	4.031309
1.484686	188.472495	4.036314
1.284818	178.688142	4.041318
0.999054	189.706681	4.046323
1.236608	185.330779	4.051328
1.147755	187.135948	4.056333
1.199224	186.091137	4.061338
1.229112	193.517443	4.066342
1.440822	194.189504	4.071347
1.191735	190.122209	4.076352
1.445389	201.519544	4.081357
1.230739	193.730181	4.086362
1.332309	195.832803	4.091366
1.469728	182.191885	4.096371
1.797697	189.376848	4.101376
1.365170	189.412785	4.106381
1.663810	197.681896	4.111386
1.340176	199.134495	4.116390
1.290140	196.318611	4.121395
1.194614	193.251963	4.126400
1.325568	201.838244	4.131405
1.262011	190.818379	4.136410
1.518344	194.011917	4.141414
0.997292	212.460671	4.146419
1.179199	195.807223	4.151424
1.202856	206.935255	4.156429
1.235022	204.853007	4.161434
1.529367	202.096726	4.166438
1.296678	202.192376	4.171443
1.457225	194.951396	4.176448
1.069788	199.352222	4.181453
1.385095	203.089082	4.186458
1.516395	217.209432	4.191462
1.793166	229.603539	4.196467
1.868776	225.773417	4.201472
1.464473	227.036611	4.206477
1.771206	211.567901	4.211482
1.316694	210.805692	4.216486
1.483049	216.122682	4.221491
2.043655	217.665246	4.226496
1.951756	226.316385	4.231501
1.939665	208.087575	4.236506
1.572200	202.310101	4.241510
1.520470	198.873555	4.246515
1.532097	201.452159	4.251520
1.428271	218.929073	4.256525
1.687525	221.843232	4.261530
1.759361	217.035954	4.266534
1.917839	214.204453	4.271539
2.054336	219.812580	4.276544
1.796283	228.372494	4.281549
1.830504	224.452135	4.286554
1.636871	224.984002	4.291558
1.740092	228.411210	4.296563
1.888335	221.641757	4.301568
1.489311	230.845713	4.306573
1.751376	218.662235	4.311578
1.912754	223.231841	4.316582
1.624856	226.325012	4.321587
1.752896	216.056010	4.326592
1.526809	220.175645	4.331597
1.609379	221.738899	4.336602
1.785825	226.749181	4.341606
1.506614	229.431691	4.346611
1.884249	237.875019	4.351616
2.075026	242.212666	4.356621
2.100682	238.198317	4.361626
2.180731	240.074336	4.366630
1.832962	226.769373	4.371635
1.976760	233.428665	4.376640
1.604263	250.897035	4.381645
1.915915	250.926706	4.386650
1.901456	260.513846	4.391654
1.998353	263.640318	4.396659
2.051907	257.524114	4.401664
1.872497	258.821573	4.406669
1.930139	253.843290	4.411674
2.226615	259.016952	4.416678
2.162271	258.751916	4.421683
2.173179	261.782299	4.426688
2.046595	257.316099	4.431693
2.401188	257.000183	4.436698
2.144105	269.827051	4.441702
2.062126	269.504354	4.446707
2.194386	255.073294	4.451712
2.112119	255.187102	4.456717
2.362964	259.048182	4.461722
2.284960	260.034098	4.466726
2.127611	257.552525	4.471731
2.451120	254.284124	4.476736
2.141625	282.129366	4.481741
2.522677	259.575435	4.486746
2.356312	270.434604	4.491750
2.154716	260.396541	4.496755
2.613669	253.383349	4.501760
2.655842	258.135448	4.506765
2.442673	262.445044	4.511770
2.623381	254.305200	4.516774
2.179142	261.243995	4.521779
2.517900	254.954677	4.526784
2.549209	259.909042	4.531789
2.597128	261.693591	4.536794
2.620134	262.650977	4.541798
1.989573	265.946300	4.546803
2.586907	264.762838	4.551808
2.489685	271.277784	4.556813
2.604388	261.133487	4.561818
2.504140	259.162102	4.566822
2.160168	256.679207	4.571827
2.255991	266.853977	4.576832
2.257282	262.139536	4.581837
2.499074	247.519708	4.586842
2.220408	248.737872	4.591846
2.353117	253.072490	4.596851
2.441907	256.050440	4.601856
2.507833	263.386079	4.606861
2.600024	280.019911	4.611866
2.849003	283.521012	4.616870
2.654322	285.320792	4.621875
2.636860	272.998383	4.626880
2.539039	279.144159	4.631885
2.678185	279.783425	4.636890
2.717975	275.395190	4.641894
2.817377	290.984548	4.646899
2.725222	274.200991	4.651904
2.739282	281.382525	4.656909
3.271913	272.400097	4.661914
2.596263	262.399724	4.666918
2.482569	257.848227	4.671923
2.902270	262.490881	4.676928
2.704593	273.611635	4.681933
3.050150	271.049025	4.686938
2.401834	268.407368	4.691942
2.709439	280.948747	4.696947
3.359917	277.032198	4.701952
2.948933	283.949822	4.706957
2.958726	256.473211	4.711962
2.338947	266.382856	4.716966
2.686410	277.188097	4.721971
3.130209	280.385796	4.726976
2.912797	286.979705	4.731981
2.688331	288.958734	4.736986
2.870995	296.982763	4.741990
2.638987	290.305911	4.746995
2.703256	289.950857	4.752000
2.569627	285.639224	4.757005
2.930566	290.372792	4.762010
2.908396	281.358324	4.767014
2.789041	295.265928	4.772019
3.132324	281.486130	4.777024
2.887906	291.060877	4.782029
2.667516	293.878407	4.787034
2.716987	300.642897	4.792038
3.236215	308.143483	4.797043
3.522256	314.785817	4.802048
2.954835	304.656148	4.807053
3.132872	305.665068	4.812058
2.943596	303.418929	4.817062
2.966434	313.557351	4.822067
3.402172	323.868762	4.827072
3.215978	324.922285	4.832077
3.087914	322.060177	4.837082
3.181738	318.048552	4.842086
3.018995	332.663034	4.847091
3.608660	316.327724	4.852096
3.425327	316.870322	4.857101
3.121962	310.559431	4.862106
3.251164	312.239494	4.867110
3.191265	325.323874	4.872115
3.326631	326.271773	4.877120
3.281670	328.198255	4.882125
3.513608	317.353717	4.887130
3.291506	315.111423	4.892134
3.048754	324.394187	4.897139
3.263754	316.259693	4.902144
3.286589	318.752804	4.907149
3.261239	321.250129	4.912154
3.583865	324.424156	4.917158
3.264381	330.420417	4.922163
3.360647	329.085838	4.927168
3.453076	319.537223	4.932173
3.363745	325.889782	4.937178
3.566745	317.767333	4.942182
3.494891	324.418498	4.947187
3.160244	322.785559	4.952192
3.161531	334.018208	4.957197
2.728138	324.840417	4.962202
3.267976	321.515535	4.967206
3.526157	320.958944	4.972211
3.322912	317.242263	4.977216
3.331840	321.360579	4.982221
3.409455	328.519300	4.987226
3.695629	324.122301	4.992230
3.167535	348.447698	4.997235
3.746622	336.662699	5.002240
3.725107	338.450247	5.007245
3.475849	346.432517	5.012250
3.547308	344.747758	5.017254
3.726927	359.298784	5.022259
3.680712	351.330661	5.027264
3.686565	349.905852	5.032269
3.668902	347.132538	5.037274
4.268055	338.420744	5.042278
3.749360	349.139595	5.047283
3.861557	339.925010	5.052288
3.357251	347.333413	5.057293
3.767486	345.920311	5.062298
3.887615	350.509203	5.067302
3.872154	354.281917	5.072307
3.887827	344.673063	5.077312
3.705800	341.643075	5.082317
3.761876	349.558809	5.087322
4.209304	338.973136	5.092326
3.610187	338.929362	5.097331
3.777982	335.372551	5.102336
3.848994	340.422293	5.107341
3.860349	346.920217	5.112346
4.133303	350.758823	5.117350
3.673355	345.152850	5.122355
3.843556	332.532218	5.127360
3.887078	353.730054	5.132365
4.084041	342.640983	5.137370
4.006693	352.515110	5.142374
3.648992	361.265201	5.147379
4.165885	348.717097	5.152384
4.020087	344.350928	5.157389
3.757370	344.989123	5.162394
3.836616	347.764942	5.167398
3.725930	348.855810	5.172403
4.022776	348.693968	5.177408
3.957379	351.617307	5.182413
3.957856	347.180596	5.187418
4.123237	354.934330	5.192422
3.752268	359.558108	5.197427
3.925320	353.456452	5.202432
4.014735	354.852154	5.207437
4.043829	355.193314	5.212442
3.998529	341.692945	5.217446
4.216285	362.538998	5.222451
3.769242	348.536648	5.227456
3.807298	354.745438	5.232461
4.122530	373.905231	5.237466
4.295418	379.210642	5.242470
4.008185	373.957329	5.247475
4.154562	375.118682	5.252480
4.147885	379.290597	5.257485
4.108688	384.278752	5.262490
4.169505	374.809814	5.267494
4.164610	392.219965	5.272499
4.254328	385.823466	5.277504
4.105889	384.502287	5.282509
3.975914	382.621729	5.287514
3.882358	381.667562	5.292518
4.056248	385.453981	5.297523
4.057807	372.364938	5.302528
4.118079	387.949910	5.307533
4.514474	399.219721	5.312538
4.523283	398.098580	5.317542
4.340265	407.408223	5.322547
4.926396	401.215693	5.327552
4.502899	397.121226	5.332557
4.304532	399.720457	5.337562
4.535307	378.845078	5.342566
4.431389	376.374881	5.347571
4.503229	372.520682	5.352576
4.118212	373.243314	5.357581
4.045139	384.291959	5.362586
4.404717	393.324480	5.367590
4.620796	415.437445	5.372595
5.018325	412.239651	5.377600
4.614330	413.981593	5.382605
4.542827	402.884259	5.387610
4.247335	398.667416	5.392614
4.329178	410.579285	5.397619
4.467006	404.291737	5.402624
4.384429	411.248379	5.407629
4.604754	409.395170	5.412634
4.675104	419.912252	5.417638
4.268995	420.394687	5.422643
4.428708	431.635263	5.427648
4.782194	418.977860	5.432653
4.622519	427.985614	5.437658
4.817270	415.150125	5.442662
4.600613	415.174855	5.447667
5.003141	407.591206	5.452672
4.803445	422.404558	5.457677
4.846816	422.473138	5.462682
4.703189	410.672055	5.467686
4.283719	419.285978	5.472691
4.672511	413.065380	5.477696
4.586791	412.352417	5.482701
4.559592	424.664219	5.487706
4.792494	412.043421	5.492710
4.408136	424.837484	5.497715
4.633849	434.265866	5.502720
5.014535	437.461696	5.507725
4.718312	440.088055	5.512730
5.153919	442.955554	5.517734
5.267376	449.367292	5.522739
4.935446	441.381321	5.527744
4.730710	440.239625	5.532749
4.758849	448.086329	5.537754
5.046305	450.039188	5.542758
4.679065	453.792316	5.547763
5.003259	449.492984	5.552768
5.154853	444.026937	5.557773
5.129797	452.772919	5.562778
5.077853	448.065542	5.567782
4.495755	458.570499	5.572787
4.737528	455.779254	5.577792
4.976742	451.766753	5.582797
4.816523	454.585320	5.587802
4.829912	457.681333	5.592806
4.816148	452.507505	5.597811
5.144604	448.765379	5.602816
5.128167	445.090014	5.607821
4.730429	449.465482	5.612826
5.006601	447.793548	5.617830
5.111066	453.164751	5.622835
5.346686	448.858450	5.627840
5.347261	460.851367	5.632845
5.074159	468.613392	5.637850
5.335258	455.670122	5.642854
5.102598	456.670361	5.647859
5.125501	449.496108	5.652864
5.473268	459.852240	5.657869
4.941882	447.075156	5.662874
5.235351	455.539222	5.667878
5.120474	455.646975	5.672883
5.397255	459.429038	5.677888
5.481631	478.980405	5.682893
5.371478	462.685013	5.687898
5.337718	456.566584	5.692902
4.857393	457.917733	5.697907
5.320834	462.924272	5.702912
5.113390	489.476097	5.707917
5.403218	483.374429	5.712922
5.559614	483.065413	5.717926
5.431384	485.871399	5.722931
5.773693	479.950187	5.727936
5.590671	480.018688	5.732941
5.562988	478.400120	5.737946
5.252546	460.808314	5.742950
5.458581	455.422454	5.747955
5.503025	453.866061	5.752960
5.238245	470.058795	5.757965
5.480774	481.745665	5.762970
5.658421	467.729261	5.767974
5.455221	478.286160	5.772979
5.667091	470.117079	5.777984
5.696661	479.620325	5.782989
5.545956	477.586709	5.787994
5.805163	466.554450	5.792998
5.490208	465.363582	5.798003
5.527787	452.211791	5.803008
5.290564	469.689723	5.808013
5.217387	477.386157	5.813018
5.356246	474.639145	5.818022
5.355713	481.615607	5.823027
5.400755	468.313892	5.828032
5.590294	478.678129	5.833037
5.550729	477.209610	5.838042
5.549980	475.904960	5.843046
5.441142	475.788749	5.848051
5.458393	475.584613	5.853056
5.501854	479.981005	5.858061
5.655265	500.453900	5.863066
5.743796	502.550925	5.868070
5.719110	511.055758	5.873075
5.981524	509.830349	5.878080
5.642035	516.483006	5.883085
5.589598	510.289110	5.888090
5.888332	500.575175	5.893094
5.958490	508.833968	5.898099
6.277012	497.512584	5.903104
6.107645	508.770206	5.908109
5.844853	500.590754	5.913114
5.937667	507.357249	5.918118
5.897645	510.725122	5.923123
5.957951	506.813896	5.928128
5.863125	497.579955	5.933133
6.024922	505.666637	5.938138
6.161590	501.776535	5.943142
5.521493	490.169608	5.948147
6.202480	497.108732	5.953152
5.807731	497.907760	5.958157
5.683480	507.117283	5.963162
6.141834	508.358208	5.968166
6.277409	515.050651	5.973171
5.908638	513.786589	5.978176
6.130613	516.449271	5.983181
5.917358	517.694531	5.988186
6.257941	508.014422	5.993190
6.058952	508.045704	5.998195
6.117775	506.380675	6.003200
6.042202	513.564698	6.008205
5.908966	526.823267	6.013210
6.048386	519.400445	6.018214
6.005434	518.919853	6.023219
6.104793	521.189815	6.028224
5.995782	525.797781	6.033229
5.503151	528.258111	6.038234
5.889045	517.508749	6.043238
5.647506	524.627267	6.048243
5.919981	519.315054	6.053248
6.156174	521.157017	6.058253
5.736611	519.703736	6.063258
6.189354	517.652083	6.068262
6.241621	526.876252	6.073267
6.032260	511.699709	6.078272
5.910921	515.860617	6.083277
5.997196	522.969754	6.088282
6.576707	540.844668	6.093286
6.356682	521.422735	6.098291
6.412943	524.914795	6.103296
6.179959	516.520366	6.108301
5.903726	518.505611	6.113306
5.868673	510.837947	6.118310
5.964662	521.401275	6.123315
6.104982	512.934011	6.128320
6.170070	513.252751	6.133325
5.867951	518.115988	6.138330
6.303035	520.823465	6.143334
6.279333	524.011652	6.148339
5.965977	527.410490	6.153344
6.076910	519.156741	6.158349
6.072635	529.889860	6.163354
6.002811	506.684148	6.168358
5.886308	511.805284	6.173363
6.008141	515.410125	6.178368
6.077935	514.974832	6.183373
5.958581	525.053031	6.188378
6.313375	527.951954	6.193382
6.355609	533.249807	6.198387
6.244933	527.310792	6.203392
5.916077	509.562542	6.208397
5.712508	519.722333	6.213402
6.208128	510.407585	6.218406
5.965522	519.460963	6.223411
5.776557	526.621208	6.228416
6.420012	539.740094	6.233421
6.264681	539.931979	6.238426
6.292395	518.137224	6.243430
6.314095	522.030910	6.248435
6.338985	524.280621	6.253440
6.255535	519.169687	6.258445
5.767669	523.653794	6.263450
5.896557	514.656355	6.268454
5.963931	516.293678	6.273459
6.036026	522.573667	6.278464
5.996666	522.388061	6.283469
5.786468	522.826779	6.288474
6.414120	539.486850	6.293478
6.456830	524.299519	6.298483
5.992484	519.925364	6.303488
6.627621	528.753491	6.308493
6.209366	522.766747	6.313498
6.221804	527.623191	6.318502
6.071915	530.727752	6.323507
6.183865	509.775837	6.328512
6.270782	513.044794	6.333517
6.058606	526.362382	6.338522
6.379638	513.149787	6.343526
6.206421	532.153616	6.348531
6.075938	521.158189	6.353536
6.193790	512.302867	6.358541
5.902268	523.106337	6.363546
6.169122	510.372409	6.368550
6.245067	524.208188	6.373555
6.083598	518.717388	6.378560
6.039591	530.992392	6.383565
6.018223	524.268396	6.388570
5.997010	522.728667	6.393574
5.823106	529.703414	6.398579
5.606996	519.015647	6.403584
5.764789	522.009970	6.408589
5.925162	526.834371	6.413594
6.010399	523.083583	6.418598
5.699504	515.741788	6.423603
5.565324	535.212729	6.428608
6.511640	545.005919	6.433613
6.354399	557.337442	6.438618
6.305069	554.724810	6.443622
5.963882	544.503038	6.448627
5.900669	548.260999	6.453632
6.324768	546.890280	6.458637
6.392793	545.309658	6.463642
6.217386	522.681453	6.468646
6.232708	520.937483	6.473651
6.024594	516.305615	6.478656
6.256900	516.385002	6.483661
5.746364	518.876506	6.488666
6.283716	518.378057	6.493670
5.980837	523.117507	6.498675
5.719792	520.579131	6.503680
6.084878	518.722805	6.508685
6.160509	544.192429	6.513690
6.172378	532.697049	6.518694
6.459096	530.352784	6.523699
6.047072	515.880405	6.528704
6.223881	514.611229	6.533709
5.945024	511.325405	6.538714
6.190937	516.612186	6.543718
5.886135	524.264244	6.548723
5.970728	508.420146	6.553728
6.142645	516.155912	6.558733
5.915166	523.969028	6.563738
6.091205	518.127961	6.568742
5.770934	527.859233	6.573747
6.282903	535.534572	6.578752
6.625113	543.474255	6.583757
6.149038	532.324702	6.588762
6.354292	509.953461	6.593766
6.120298	512.334349	6.598771
6.189732	512.125832	6.603776
6.383253	509.445057	6.608781
6.215830	513.611607	6.613786
6.868601	517.719968	6.618790
6.269487	509.685474	6.623795
6.458132	507.378235	6.628800
6.389207	523.296256	6.633805
5.798989	514.856382	6.638810
6.154138	506.697740	6.643814
6.026830	510.654720	6.648819
6.014485	517.038440	6.653824
6.213481	527.102312	6.658829
5.608048	522.269032	6.663834
5.951235	523.625675	6.668838
6.066148	524.962523	6.673843
6.580250	525.582458	6.678848
6.009212	517.090675	6.683853
6.361611	524.893997	6.688858
6.594649	507.288393	6.693862
6.195061	496.289604	6.698867
5.883605	485.970417	6.703872
6.106416	478.758675	6.708877
5.901193	484.729604	6.713882
5.832732	493.570883	6.718886
6.046695	508.053233	6.723891
6.154146	520.377983	6.728896
6.276339	518.653941	6.733901
5.748051	526.365228	6.738906
6.019005	524.631402	6.743910
5.947680	534.942297	6.748915
6.199674	524.320522	6.753920
6.415265	525.498961	6.758925
5.951221	531.825326	6.763930
6.330036	522.876064	6.768934
6.127981	521.495955	6.773939
6.048550	514.120942	6.778944
5.956079	517.578778	6.783949
6.062513	517.097573	6.788954
6.100656	526.044379	6.793958
5.908030	527.275774	6.798963
6.003773	526.096650	6.803968
6.056750	526.914333	6.808973
5.642874	526.088663	6.813978
6.158372	516.621257	6.818982
6.115401	524.457652	6.823987
6.178145	522.271946	6.828992
6.355022	512.929561	6.833997
6.288908	509.924386	6.839002
6.136583	521.820381	6.844006
5.893959	525.163923	6.849011
6.348701	523.590235	6.854016
6.636351	516.965038	6.859021
5.818371	522.072954	6.864026
6.354233	514.586990	6.869030
6.150022	515.836182	6.874035
6.207315	501.188196	6.879040
6.136235	498.694399	6.884045
5.728419	496.018483	6.889050
6.058277	488.561542	6.894054
6.085112	515.917336	6.899059
6.080762	514.968645	6.904064
6.058780	526.388783	6.909069
5.880085	515.757088	6.914074
6.222380	516.553105	6.919078
5.833981	520.163336	6.924083
5.902809	526.930351	6.929088
6.126661	527.067863	6.934093
6.047942	525.309835	6.939098
6.235517	515.059505	6.944102
6.050445	523.971768	6.949107
6.317158	520.058395	6.954112
6.362680	517.505765	6.959117
6.104592	523.875736	6.964122
6.104114	511.641982	6.969126
5.938019	529.419001	6.974131
6.134944	522.216450	6.979136
6.400319	520.649292	6.984141
5.556199	526.154188	6.989146
6.119164	519.044564	6.994150
5.877882	520.673896	6.999155
5.946201	522.791430	7.004160
6.245550	527.449515	7.009165
6.123508	522.472424	7.014170
6.244307	520.311261	7.019174
6.045106	524.171107	7.024179
5.927280	515.994428	7.029184
6.127598	525.010824	7.034189
6.277813	527.055433	7.039194
6.212520	512.605871	7.044198
5.707050	523.360837	7.049203
5.913022	512.014138	7.054208
5.853069	520.397536	7.059213
5.658134	515.242871	7.064218
5.701433	522.434485	7.069222
5.840582	523.074254	7.074227
5.995688	522.170246	7.079232
6.087171	524.896817	7.084237
5.931407	534.352783	7.089242
6.347548	537.707928	7.094246
6.165992	538.423781	7.099251
6.093271	527.259175	7.104256
6.239389	524.989841	7.109261
6.125255	527.796761	7.114266
5.836260	520.425200	7.119270
5.926423	520.370519	7.124275
5.914839	536.758557	7.129280
6.344274	553.763751	7.134285
6.074858	561.039419	7.139290
6.210242	552.718765	7.144294
6.002233	543.464530	7.149299
5.913299	530.404415	7.154304
6.464506	553.545960	7.159309
5.843686	542.057946	7.164314
5.931636	534.197095	7.169318
6.225666	539.263916	7.174323
6.163238	553.628211	7.179328
6.266095	540.714176	7.184333
6.119208	536.083334	7.189338
6.201624	522.579755	7.194342
5.826224	529.129138	7.199347
5.903090	551.132607	7.204352
6.464314	552.720488	7.209357
5.830406	547.675350	7.214362
6.170085	538.089097	7.219366
6.188777	554.510825	7.224371
5.944429	550.583239	7.229376
6.301969	544.222232	7.234381
6.310990	545.648897	7.239386
6.217816	529.129239	7.244390
6.192774	530.523253	7.249395
6.028488	527.706357	7.254400
6.005829	528.038808	7.259405
5.767964	536.605225	7.264410
5.934027	533.444275	7.269414
5.947427	540.031721	7.274419
5.990415	559.172508	7.279424
6.239706	549.775908	7.284429
6.058393	555.223377	7.289434
6.292711	549.387466	7.294438
6.140691	559.226511	7.299443
6.394218	546.601208	7.304448
6.101897	526.416058	7.309453
6.004020	534.557900	7.314458
5.737120	518.894508	7.319462
5.845373	536.698812	7.324467
5.972646	549.593711	7.329472
6.150332	556.876393	7.334477
5.903839	562.575658	7.339482
5.794628	558.561216	7.344486
6.008218	557.669641	7.349491
5.815370	559.555476	7.354496
6.169729	558.968777	7.359501
6.201852	559.821380	7.364506
6.176006	559.244727	7.369510
6.212104	560.133078	7.374515
6.381340	566.512660	7.379520
6.403761	555.286337	7.384525
6.246910	565.751679	7.389530
6.124541	553.938193	7.394534
6.351513	556.043425	7.399539
6.232217	543.079279	7.404544
6.067525	538.328647	7.409549
6.051715	535.615767	7.414554
5.879174	548.812874	7.419558
6.244072	559.356455	7.424563
5.970186	563.841816	7.429568
6.379080	550.442412	7.434573
5.686906	560.037944	7.439578
6.052386	555.671677	7.444582
6.022817	558.823054	7.449587
6.079768	565.413180	7.454592
5.978871	558.047219	7.459597
5.846829	563.440080	7.464602
6.333277	563.558271	7.469606
6.167132	563.558573	7.474611
6.207442	554.876360	7.479616
6.274386	559.077989	7.484621
6.260129	569.951302	7.489626
6.201063	555.311641	7.494630
6.088545	552.162685	7.499635
5.968729	559.434053	7.504640
6.282381	555.811455	7.509645
5.964850	549.594755	7.514650
6.039507	544.024083	7.519654
6.260309	551.014810	7.524659
6.225397	553.335083	7.529664
6.292732	526.340194	7.534669
5.821320	537.773737	7.539674
5.901649	539.547438	7.544678
5.899721	548.637620	7.549683
6.213622	560.575582	7.554688
6.573565	554.080886	7.559693
6.450360	545.445135	7.564698
6.325727	525.584880	7.569702
6.212374	534.222176	7.574707
5.864637	531.373046	7.579712
5.960284	520.777011	7.584717
6.191533	527.560003	7.589722
6.148345	531.581522	7.594726
5.973259	527.913313	7.599731
6.092003	532.052902	7.604736
6.405559	527.938318	7.609741
5.968153	539.809711	7.614746
6.154849	532.486214	7.619750
6.272435	533.917135	7.624755
6.162635	541.952033	7.629760
6.113411	521.008288	7.634765
6.139002	535.265183	7.639770
6.223117	525.246130	7.644774
6.141323	518.263278	7.649779
6.051119	527.849290	7.654784
6.234691	520.158616	7.659789
6.016687	527.640945	7.664794
6.054659	529.515172	7.669798
6.108413	531.386200	7.674803
5.765946	529.161496	7.679808
5.866485	521.673275	7.684813
5.855580	526.192811	7.689818
6.386205	524.729905	7.694822
6.421471	530.703533	7.699827
6.069866	533.715442	7.704832
6.398836	528.879880	7.709837
6.147391	532.835873	7.714842
6.025448	536.954463	7.719846
6.067948	540.575084	7.724851
6.125069	530.011553	7.729856
6.285576	532.721392	7.734861
6.334730	540.923787	7.739866
6.350093	536.248275	7.744870
6.081070	531.771595	7.749875
6.063878	527.007740	7.754880
6.191754	532.614743	7.759885
6.077113	533.637907	7.764890
6.213338	527.231494	7.769894
6.240584	529.417083	7.774899
6.004060	531.487816	7.779904
6.046734	536.438912	7.784909
5.973907	533.404751	7.789914
6.163395	530.457768	7.794918
6.392387	530.139517	7.799923
6.100119	535.059340	7.804928
6.416758	524.041819	7.809933
6.037402	524.788877	7.814938
5.925672	531.603391	7.819942
5.918000	529.630386	7.824947
5.755754	530.099163	7.829952
5.876199	525.923358	7.834957
5.877553	535.141541	7.839962
5.893099	531.464126	7.844966
6.200938	528.997093	7.849971
5.889153	529.058458	7.854976
6.069677	522.797943	7.859981
6.107695	530.021707	7.864986
6.063250	522.557444	7.869990
5.823098	527.255353	7.874995
5.822970	532.024590	7.880000
6.194852	523.697428	7.885005
5.682227	534.454966	7.890010
5.952623	526.554104	7.895014
6.392192	522.465757	7.900019
6.073064	520.583093	7.905024
6.091927	525.906016	7.910029
5.860064	530.160271	7.915034
5.821939	525.552994	7.920038
6.308809	544.478737	7.925043
6.405357	553.239112	7.930048
6.140283	536.403339	7.935053
6.228130	533.798526	7.940058
6.112447	524.607380	7.945062
6.161556	535.110391	7.950067
6.033891	536.739299	7.955072
6.045774	519.803021	7.960077
6.017233	532.555048	7.965082
6.115010	535.627266	7.970086
6.404604	536.576429	7.975091
6.221101	526.852289	7.980096
6.319057	530.928719	7.985101
6.002228	542.139700	7.990106
6.202673	535.343527	7.995110
5.986597	530.660189	8.000115
6.061568	527.263208	8.005133
6.085984	520.906123	8.010150
5.996286	537.997119	8.015168
6.159058	527.424949	8.020186
6.190855	518.150761	8.025203
5.833696	526.159530	8.030221
5.956437	525.681142	8.035238
6.060294	529.965602	8.040256
5.945162	528.357157	8.045274
5.952224	519.357379	8.050291
5.899787	533.413753	8.055309
6.207763	547.361279	8.060326
6.551229	556.824856	8.065344
6.435666	547.601572	8.070362
6.241521	526.751256	8.075379
5.887370	537.515901	8.080397
6.276641	531.315310	8.085414
5.935567	538.481920	8.090432
6.298235	547.467506	8.095450
6.613832	540.012493	8.100467
6.436134	530.175688	8.105485
6.168096	529.071455	8.110502
6.447058	524.655788	8.115520
6.175341	520.540039	8.120538
6.447656	519.835496	8.125555
6.236712	531.118298	8.130573
6.086362	522.771872	8.135590
6.193632	523.793591	8.140608
6.308118	530.734847	8.145626
6.358600	535.124961	8.150643
5.993117	534.121559	8.155661
6.290650	533.048449	8.160678
6.172039	534.485574	8.165696
6.044768	525.831355	8.170714
6.275469	528.080669	8.175731
6.008916	529.495793	8.180749
6.205628	523.463022	8.185766
6.174323	531.894136	8.190784
6.215828	533.667528	8.195802
6.157783	550.179892	8.200819
6.422584	561.814333	8.205837
6.598075	559.953075	8.210854
6.472997	540.980342	8.215872
6.118736	538.237323	8.220890
6.293356	535.151738	8.225907
6.117218	549.342621	8.230925
6.606838	548.181184	8.235942
6.532140	540.001642	8.240960
6.346959	538.004356	8.245978
6.735161	532.153186	8.250995
6.821411	535.769326	8.256013
6.558698	529.775374	8.261030
6.236880	533.839781	8.266048
6.202686	534.564958	8.271066
6.136548	528.361194	8.276083
6.109557	522.306545	8.281101
6.558796	513.007858	8.286118
6.436030	519.786089	8.291136
6.229418	527.046790	8.296154
6.421629	518.931106	8.301171
6.356479	533.806551	8.306189
6.514248	529.543267	8.311206
6.468147	535.271336	8.316224
6.472217	531.439869	8.321242
6.436742	529.972562	8.326259
6.453322	535.169603	8.331277
6.391474	535.502181	8.336294
6.038936	526.969226	8.341312
6.341410	529.221244	8.346330
6.634347	521.756109	8.351347
6.390551	529.074719	8.356365
6.231538	535.125522	8.361382
6.443873	547.713621	8.366400
6.469526	556.970809	8.371418
6.556595	559.346993	8.376435
6.336059	557.815106	8.381453
6.342284	566.936855	8.386470
6.334742	548.265792	8.391488
6.178246	559.089308	8.396506
6.532221	550.403178	8.401523
6.651973	554.772010	8.406541
6.528277	556.281519	8.411558
7.090695	562.793323	8.416576
6.788554	559.937474	8.421594
6.952134	549.731523	8.426611
6.362476	545.284718	8.431629
6.151538	544.790912	8.436646
6.516879	540.825052	8.441664
6.779244	558.695431	8.446682
6.987726	548.504793	8.451699
6.636443	540.929022	8.456717
6.380362	535.381230	8.461734
6.328298	531.064841	8.466752
6.587065	547.074048	8.471770
6.922925	544.212950	8.476787
6.572291	548.374231	8.481805
6.497786	535.449983	8.486822
6.564928	531.132199	8.491840
6.571483	535.301958	8.496858
6.714704	519.374884	8.501875
6.610381	533.186828	8.506893
6.202391	523.451851	8.511910
6.458736	538.360575	8.516928
6.264990	555.381399	8.521946
6.657408	558.722484	8.526963
6.630953	561.394936	8.531981
6.773285	564.622064	8.536998
6.704423	563.816645	8.542016
6.234527	566.792844	8.547034
6.962794	557.959638	8.552051
6.621812	564.030584	8.557069
6.693057	556.040263	8.562087
6.985472	554.773349	8.567104
6.587645	554.124241	8.572122
6.778904	546.178057	8.577139
6.859711	558.043060	8.582157
6.766912	557.573325	8.587175
6.732453	555.201884	8.592192
6.591895	558.093645	8.597210
6.938698	560.910873	8.602227
6.695331	561.218536	8.607245
6.685414	550.279685	8.612263
6.868785	547.609699	8.617280
6.501768	556.878242	8.622298
6.792906	555.002105	8.627315
6.825728	553.079302	8.632333
7.021580	553.758101	8.637351
6.842913	546.659710	8.642368
6.675741	567.933722	8.647386
6.763588	557.366532	8.652403
6.456181	562.489193	8.657421
6.435662	568.887625	8.662439
6.784725	556.197639	8.667456
6.439436	560.209839	8.672474
6.703828	553.386295	8.677491
6.621569	561.432513	8.682509
6.710343	550.095535	8.687527
6.770804	555.900571	8.692544
6.740980	563.995004	8.697562
6.538067	560.244970	8.702579
6.768339	589.855994	8.707597
6.959165	590.198581	8.712615
6.916200	589.268234	8.717632
6.848236	591.552938	8.722650
6.955876	577.706988	8.727667
6.763292	583.426806	8.732685
6.664857	592.769469	8.737703
6.901345	600.879155	8.742720
6.648560	609.414516	8.747738
6.923695	596.491188	8.752755
6.995137	602.192083	8.757773
6.974915	611.638347	8.762791
7.278788	596.826659	8.767808
6.894444	605.955896	8.772826
7.058444	597.339217	8.777843
7.016118	576.995831	8.782861
6.942026	585.386908	8.787879
6.912017	563.553395	8.792896
6.456083	579.717249	8.797914
6.904977	576.985471	8.802931
7.004308	591.943515	8.807949
6.648177	593.621925	8.812967
7.254873	601.730660	8.817984
7.186673	606.917035	8.823002
7.176788	594.976462	8.828019
7.006565	597.661459	8.833037
6.764330	596.571064	8.838055
7.159190	590.173696	8.843072
7.085117	592.493459	8.848090
7.110254	584.407022	8.853107
6.973937	585.642588	8.858125
7.022509	599.285750	8.863143
7.149398	587.753996	8.868160
7.148428	601.099105	8.873178
7.228357	594.578022	8.878195
7.042529	594.196481	8.883213
6.841913	595.870251	8.888231
7.018143	591.935432	8.893248
6.953342	588.474222	8.898266
6.801666	588.497295	8.903283
7.175477	588.870558	8.908301
7.034447	583.891324	8.913319
7.169360	585.321493	8.918336
7.218972	592.619397	8.923354
7.152144	585.552597	8.928371
6.977418	589.653723	8.933389
7.123940	594.163490	8.938407
7.063300	592.030480	8.943424
6.890321	599.845692	8.948442
7.094409	593.449144	8.953459
7.078316	593.775835	8.958477
7.234075	594.785708	8.963495
7.059667	582.505668	8.968512
7.022777	584.134176	8.973530
6.948283	589.000484	8.978547
7.355149	587.306658	8.983565
7.048237	588.180723	8.988583
7.401511	580.878392	8.993600
7.461068	593.458612	8.998618
7.435077	584.299132	9.003635
7.147983	586.626443	9.008653
7.154467	598.853005	9.013671
7.326630	590.269128	9.018688
7.295695	602.591427	9.023706
7.154159	605.374028	9.028723
7.274793	597.913712	9.033741
7.405487	603.193771	9.038759
7.520117	594.971991	9.043776
7.268661	594.815329	9.048794
7.217572	590.612817	9.053811
7.422706	586.765725	9.058829
7.098247	589.743186	9.063847
7.278185	577.329411	9.068864
7.341914	593.127634	9.073882
7.238063	583.010924	9.078899
7.415413	595.823406	9.083917
7.340285	612.461471	9.088935
7.331828	599.628795	9.093952
7.175571	607.863709	9.098970
7.246473	610.567907	9.103987
7.130303	590.180910	9.109005
7.142324	602.284831	9.114023
7.251034	588.406908	9.119040
7.573634	590.377315	9.124058
7.593091	590.261007	9.129075
7.574449	586.500984	9.134093
7.367186	594.745796	9.139111
7.306051	588.910305	9.144128
7.293071	590.245153	9.149146
7.435450	586.405676	9.154163
7.470619	591.420072	9.159181
7.188564	596.288306	9.164199
7.121048	594.396643	9.169216
7.391827	595.704773	9.174234
7.214707	592.304536	9.179251
7.466715	592.163872	9.184269
7.372763	596.301840	9.189287
7.648804	602.675685	9.194304
7.367852	594.106064	9.199322
7.381380	595.342454	9.204339
7.471079	590.553887	9.209357
7.374181	593.433913	9.214375
7.100135	591.889805	9.219392
7.403343	593.033453	9.224410
7.461576	592.992809	9.229427
7.672518	601.334332	9.234445
7.367449	608.318974	9.239463
7.388499	603.564085	9.244480
7.246349	602.188598	9.249498
7.394177	599.633512	9.254515
7.747112	592.845113	9.259533
7.609937	599.513084	9.264551
7.397448	581.016670	9.269568
7.308838	593.597363	9.274586
7.281420	604.724029	9.279603
7.938887	615.087054	9.284621
7.550793	625.442780	9.289639
7.955553	618.674441	9.294656
7.632251	600.182244	9.299674
7.302327	601.262536	9.304691
7.424366	596.124493	9.309709
7.355979	610.499262	9.314727
7.844534	615.089694	9.319744
8.150275	617.483679	9.324762
7.808854	593.690340	9.329779
7.533531	583.270728	9.334797
7.589128	593.582930	9.339815
7.614714	592.130719	9.344832
7.652819	601.282843	9.349850
7.769348	588.276795	9.354867
7.959791	585.068332	9.359885
7.512724	607.825787	9.364903
7.932293	588.795073	9.369920
7.739446	594.594649	9.374938
7.646374	600.580261	9.379955
7.577718	590.240448	9.384973
7.391762	593.868126	9.389991
7.496736	597.733404	9.395008
7.371904	586.018684	9.400026
7.317144	601.686426	9.405043
7.901204	614.205082	9.410061
7.823677	617.306378	9.415079
7.884164	610.671496	9.420096
7.860413	610.517651	9.425114
7.867069	602.133822	9.430131
7.716203	586.616922	9.435149
7.446297	602.331238	9.440167
7.874173	607.282221	9.445184
7.878094	616.714559	9.450202
7.795721	616.345935	9.455219
7.882079	604.854916	9.460237
7.695615	600.984064	9.465255
7.872256	604.695106	9.470272
7.544460	609.228151	9.475290
7.795258	617.281160	9.480307
7.780031	618.203661	9.485325
7.759531	616.940527	9.490343
7.834523	620.444199	9.495360
8.084526	614.121831	9.500378
8.047156	628.878724	9.505395
8.164477	615.627586	9.510413
7.491768	603.773412	9.515431
7.540495	595.560161	9.520448
7.859940	610.259646	9.525466
7.722555	629.011863	9.530483
7.779650	616.386410	9.535501
7.775818	622.939165	9.540519
7.676213	623.558937	9.545536
7.724131	617.843479	9.550554
7.963314	623.461457	9.555571
7.615928	613.158439	9.560589
7.573812	621.116475	9.565607
7.827223	617.895631	9.570624
8.167315	612.442565	9.575642
7.845197	628.087007	9.580659
7.892450	621.471528	9.585677
7.933693	615.693407	9.590695
7.626315	623.631905	9.595712
8.232878	618.909857	9.600730
8.199921	619.349453	9.605747
8.056844	614.608397	9.610765
8.006518	611.473470	9.615783
8.127284	613.035581	9.620800
8.142800	616.348527	9.625818
7.734619	625.021071	9.630835
7.704290	620.844150	9.635853
8.071956	610.179708	9.640871
7.947029	619.594666	9.645888
8.122586	618.907683	9.650906
7.876242	614.819796	9.655923
7.941302	615.883923	9.660941
7.870385	626.140689	9.665959
8.029300	647.806612	9.670976
8.092024	645.413783	9.675994
8.143543	651.095946	9.681011
8.329758	654.929509	9.686029
8.185481	650.097811	9.691047
7.996709	650.041302	9.696064
8.483978	636.868455	9.701082
8.002811	636.882013	9.706099
7.824197	630.973909	9.711117
8.222713	636.529643	9.716135
8.181192	650.899125	9.721152
8.489175	642.583765	9.726170
7.961296	633.241492	9.731187
8.114839	628.386664	9.736205
8.209885	629.806303	9.741223
8.167797	641.855428	9.746240
8.474825	632.761633	9.751258
7.859854	631.361737	9.756275
8.272404	638.867355	9.761293
8.253361	643.662618	9.766311
7.848609	645.232849	9.771328
8.337865	650.672825	9.776346
8.265034	651.747145	9.781363
8.286257	642.595375	9.786381
8.372823	647.324181	9.791399
8.147281	657.506932	9.796416
8.283844	650.716081	9.801434
8.055413	661.461611	9.806451
8.155027	657.867035	9.811469
8.264210	652.812972	9.816487
8.368621	651.173647	9.821504
8.620283	645.835362	9.826522
8.128756	654.867597	9.831539
8.210848	655.882169	9.836557
8.241290	659.790482	9.841575
8.409387	659.596078	9.846592
8.746767	649.033644	9.851610
8.371455	653.056242	9.856627
8.532994	641.175183	9.861645
8.078886	628.490325	9.866663
7.965936	651.557820	9.871680
8.549188	650.358663	9.876698
8.351080	656.178419	9.881715
7.843493	650.433902	9.886733
8.317966	656.330669	9.891751
8.300847	649.943591	9.896768
8.156698	654.140254	9.901786
8.316971	664.846942	9.906803
8.368924	658.741405	9.911821
8.427201	651.002149	9.916839
8.324913	667.452769	9.921856
8.388998	650.915225	9.926874
8.357219	656.247145	9.931891
8.349322	658.465448	9.936909
8.475488	649.302827	9.941927
8.330611	658.735670	9.946944
8.572292	661.524135	9.951962
8.588413	657.878505	9.956979
8.834147	653.255437	9.961997
8.524131	658.192374	9.967015
8.452998	653.195663	9.972032
8.561954	649.439042	9.977050
8.723339	657.824802	9.982067
8.722852	647.224912	9.987085
8.680984	649.719053	9.992103
8.504256	661.303425	9.997120
8.685528	644.962133	10.002138
8.626213	651.632513	10.007155
8.572458	656.236308	10.012173
8.571897	650.519305	10.017191
8.363082	656.344668	10.022208
8.662927	657.180172	10.027226
8.692829	658.728667	10.032243
8.212273	650.184422	10.037261
8.502571	646.723465	10.042279
8.366479	650.795393	10.047296
8.596032	660.195589	10.052314
8.719080	660.525760	10.057331
8.857400	651.709295	10.062349
8.845382	652.539750	10.067367
8.561209	654.571268	10.072384
8.375139	643.105951	10.077402
8.681635	647.537142	10.082419
8.776493	654.648793	10.087437
8.665301	639.435759	10.092455
8.182415	645.868708	10.097472
8.263957	650.896814	10.102490
8.515372	658.015956	10.107507
8.573746	670.799843	10.112525
8.668625	674.380738	10.117543
8.779451	687.824453	10.122560
8.944646	674.856344	10.127578
8.539839	680.641874	10.132595
8.492114	689.147722	10.137613
8.835126	684.678028	10.142631
8.480872	691.138647	10.147648
9.011296	692.077855	10.152666
8.878832	683.974898	10.157683
8.633973	678.588753	10.162701
8.933357	677.263207	10.167719
8.658574	686.371533	10.172736
9.136217	689.058915	10.177754
9.017073	678.898811	10.182771
8.664926	692.023143	10.187789
9.050119	689.786038	10.192807
8.668163	697.196442	10.197824
8.782872	685.678733	10.202842
8.865201	686.333391	10.207859
8.840211	684.876834	10.212877
9.026253	677.528090	10.217895
8.831399	672.056730	10.222912
8.820043	677.289040	10.227930
8.806291	680.746969	10.232947
8.863352	680.257387	10.237965
9.036857	675.685020	10.242983
8.578720	678.642962	10.248000
8.778823	678.288769	10.253018
8.921292	687.033808	10.258035
8.619254	681.473482	10.263053
9.142798	677.574735	10.268071
8.880285	683.991259	10.273088
8.750460	683.019856	10.278106
8.907873	678.663299	10.283123
9.082046	684.526646	10.288141
8.908436	665.629681	10.293159
8.848169	680.417961	10.298176
9.107418	675.669054	10.303194
9.316920	680.790276	10.308211
9.104025	688.345051	10.313229
9.109865	680.560616	10.318247
8.894852	682.738062	10.323264
8.942062	686.999749	10.328282
8.963167	694.879671	10.333299
8.795454	690.261245	10.338317
9.082852	690.878670	10.343335
8.794839	687.915559	10.348352
9.079795	692.868439	10.353370
9.583827	707.725081	10.358387
9.537630	695.790430	10.363405
9.755414	684.546777	10.368423
9.090152	687.792938	10.373440
9.172207	682.821977	10.378458
9.044775	683.311038	10.383475
9.191479	687.549198	10.388493
9.140391	680.481426	10.393511
9.466011	686.148222	10.398528
9.358775	680.523035	10.403546
9.415855	667.603402	10.408563
9.132773	682.924971	10.413581
9.267320	671.876743	10.418599
9.112503	680.151116	10.423616
9.391127	686.114308	10.428634
9.381746	678.496336	10.433651
9.073534	688.330334	10.438669
9.211992	683.756868	10.443687
9.328054	674.957845	10.448704
8.920331	681.343945	10.453722
9.527017	674.534637	10.458739
8.826097	677.116041	10.463757
8.930822	675.001354	10.468775
8.962647	676.496885	10.473792
9.125970	681.311228	10.478810
9.261195	676.230122	10.483827
9.176616	688.107302	10.488845
9.448435	677.669639	10.493863
9.076612	679.902028	10.498880
9.352686	685.275688	10.503898
9.206366	682.903424	10.508915
9.199722	713.749588	10.513933
9.692880	707.559215	10.518951
9.265736	715.067729	10.523968
9.383691	723.116373	10.528986
9.799113	718.326884	10.534003
9.580449	711.089088	10.539021
9.203422	694.496165	10.544039
9.127363	689.647868	10.549056
8.997970	700.423213	10.554074
9.610578	729.795275	10.559091
9.463879	720.364373	10.564109
9.729313	724.053095	10.569127
9.672402	725.171828	10.574144
9.188355	707.602559	10.579162
9.613955	709.967305	10.584179
9.661335	707.292702	10.589197
9.272276	699.707054	10.594215
9.286503	705.289906	10.599232
9.596864	715.317220	10.604250
9.613101	717.536266	10.609267
9.299207	722.305292	10.614285
9.587151	717.325980	10.619303
9.273452	724.344576	10.624320
9.054015	718.915541	10.629338
9.566131	708.804323	10.634355
9.023487	712.604337	10.639373
9.414178	715.393282	10.644391
9.555332	716.910901	10.649408
9.367052	728.190003	10.654426
9.280574	717.823330	10.659443
9.226193	719.560138	10.664461
9.453654	721.001400	10.669479
9.751378	727.915810	10.674496
9.566722	738.155823	10.679514
9.798587	741.192633	10.684531
9.795918	759.020247	10.689549
9.854454	744.530505	10.694567
9.490283	737.712834	10.699584
9.731955	744.014773	10.704602
9.907605	737.149228	10.709619
9.829610	731.418420	10.714637
10.139317	713.500987	10.719655
9.799825	711.897714	10.724672
9.405240	715.865551	10.729690
9.730411	713.309973	10.734707
9.448701	716.694199	10.739725
9.606220	711.543071	10.744743
9.837584	724.242816	10.749760
9.788012	731.093970	10.754778
9.402331	725.386357	10.759795
9.364296	737.334806	10.764813
9.765121	742.578442	10.769831
9.690932	750.159628	10.774848
9.824934	748.204729	10.779866
10.214166	749.073490	10.784883
9.969931	745.918619	10.789901
10.010588	745.163485	10.794919
10.218653	746.102728	10.799936
9.734661	735.125769	10.804954
10.282319	732.218320	10.809971
9.569775	722.833982	10.814989
9.637182	713.346841	10.820007
9.915135	732.728260	10.825024
9.778662	741.509584	10.830042
10.194840	729.214888	10.835059
10.163124	741.129920	10.840077
9.856987	716.018783	10.845095
9.478293	714.987636	10.850112
9.834797	734.279515	10.855130
9.970179	734.367140	10.860147
9.539282	740.247735	10.865165
9.679664	738.800650	10.870183
9.990099	735.996170	10.875200
9.585138	741.691901	10.880218
10.051185	734.606942	10.885235
9.839157	740.527832	10.890253
9.865323	741.377568	10.895271
9.820032	743.015550	10.900288
9.893367	748.394787	10.905306
9.750972	744.844315	10.910323
9.817558	746.776452	10.915341
10.051374	751.945541	10.920359
10.675492	758.481185	10.925376
9.936863	740.598793	10.930394
9.939946	737.628704	10.935411
9.755327	740.179711	10.940429
9.835369	755.113351	10.945447
10.249830	766.407228	10.950464
10.336826	778.436606	10.955482
10.521560	779.111839	10.960499
10.292737	756.421494	10.965517
10.238350	750.217962	10.970535
10.555680	751.913325	10.975552
10.287294	743.058228	10.980570
10.126152	743.107959	10.985587
10.069103	736.485360	10.990605
10.160483	737.102901	10.995623
9.887050	738.438683	11.000640
9.924890	738.771028	11.005658
9.862242	747.310571	11.010675
10.079631	756.063835	11.015693
10.088360	762.663384	11.020711
10.395814	767.239604	11.025728
10.008307	776.061053	11.030746
10.159689	776.074099	11.035763
10.609037	770.761754	11.040781
10.225380	784.242885	11.045799
10.351044	766.938183	11.050816
10.392161	777.570070	11.055834
10.183760	762.731577	11.060851
10.502654	778.910684	11.065869
10.387412	776.193172	11.070887
10.246483	773.917426	11.075904
9.972975	774.414196	11.080922
10.647735	766.860458	11.085939
10.334359	768.298889	11.090957
10.425786	776.793502	11.095975
10.195079	765.224268	11.100992
10.389569	778.783448	11.106010
10.237172	770.672224	11.111027
10.120057	785.100477	11.116045
10.365377	781.108925	11.121063
10.321539	769.415911	11.126080
9.979624	779.434146	11.131098
10.356918	782.809075	11.136115
10.144519	771.165761	11.141133
10.068470	769.164679	11.146151
10.298488	787.403402	11.151168
10.452673	797.161058	11.156186
10.741009	799.223458	11.161203
10.559469	804.739501	11.166221
10.510036	820.602417	11.171239
10.541368	806.310682	11.176256
10.622487	799.260962	11.181274
11.118051	795.792622	11.186291
10.671058	780.584259	11.191309
10.412044	779.150325	11.196327
10.533502	774.579248	11.201344
10.616945	772.595306	11.206362
10.576522	780.847286	11.211379
10.631024	771.834896	11.216397
10.435246	780.162540	11.221415
10.517528	772.940918	11.226432
10.327620	774.600440	11.231450
10.628833	785.452889	11.236467
10.688690	799.172303	11.241485
10.948591	800.752970	11.246503
10.920261	797.996883	11.251520
10.734234	781.373976	11.256538
10.879560	772.120731	11.261555
10.639409	766.592856	11.266573
10.528780	767.378107	11.271591
10.937832	760.479100	11.276608
10.619230	763.472946	11.281626
10.633289	776.942571	11.286643
10.781935	773.787720	11.291661
10.475585	763.943781	11.296679
10.789581	775.143263	11.301696
10.659844	800.111654	11.306714
11.229559	799.404697	11.311731
10.872296	792.608297	11.316749
10.629673	782.557589	11.321767
10.845459	774.980694	11.326784
10.907710	782.209485	11.331802
10.883807	776.562422	11.336819
10.941980	775.024016	11.341837
10.443160	776.335148	11.346855
10.585068	789.749017	11.351872
10.900470	800.091346	11.356890
10.783143	802.121193	11.361907
11.158396	804.775820	11.366925
10.816883	805.596274	11.371943
11.206373	801.626259	11.376960
11.083473	801.287158	11.381978
11.124796	799.523227	11.386995
11.005395	791.977111	11.392013
10.760133	782.426852	11.397031
10.992052	775.208645	11.402048
10.741062	786.738662	11.407066
10.864286	797.299623	11.412083
10.978048	801.527611	11.417101
10.935715	805.996417	11.422119
11.120415	814.357351	11.427136
11.098568	802.096306	11.432154
10.668505	807.981118	11.437171
11.016939	801.981032	11.442189
10.845362	806.393453	11.447207
11.040330	796.970993	11.452224
10.893576	805.110068	11.457242
10.913132	809.932365	11.462259
11.158246	808.162409	11.467277
10.849274	804.514865	11.472295
11.026022	799.485116	11.477312
11.202600	806.796386	11.482330
11.130322	810.528340	11.487347
11.111445	802.034468	11.492365
11.094330	801.366621	11.497383
11.027176	803.694128	11.502400
10.800462	806.107541	11.507418
10.720066	808.465677	11.512435
11.030126	797.646481	11.517453
11.124573	834.002299	11.522471
11.294543	843.694001	11.527488
11.470052	844.039518	11.532506
11.258051	830.202272	11.537523
11.547658	818.892332	11.542541
11.106774	812.232850	11.547559
11.131671	800.696535	11.552576
11.440555	808.196242	11.557594
11.334277	817.015820	11.562611
11.791710	811.224845	11.567629
11.100574	811.367177	11.572647
11.208538	801.802721	11.577664
11.515354	813.072499	11.582682
11.259698	810.046941	11.587699
11.347204	807.948759	11.592717
11.188956	812.515449	11.597735
11.014542	808.187907	11.602752
11.498269	824.246335	11.607770
11.470842	824.255372	11.612787
11.289772	807.752660	11.617805
11.354706	820.457648	11.622823
11.600339	819.809264	11.627840
11.567086	819.742505	11.632858
11.375189	818.053817	11.637875
11.673961	821.478043	11.642893
11.362357	814.822586	11.647911
11.483691	801.535493	11.652928
11.622979	804.294063	11.657946
11.082527	805.399514	11.662963
11.790181	805.253029	11.667981
11.624693	819.199234	11.672999
11.410106	812.140804	11.678016
11.223986	811.875131	11.683034
11.340698	824.671550	11.688051
12.040318	831.294337	11.693069
11.805395	833.424119	11.698087
11.661490	813.715015	11.703104
11.508650	808.497248	11.708122
11.325113	803.999984	11.713139
11.464985	803.329124	11.718157
11.520689	822.385535	11.723175
11.622407	831.825167	11.728192
11.923688	836.218306	11.733210
11.629494	842.296193	11.738227
11.729413	836.334799	11.743245
11.612062	841.581040	11.748263
11.730350	842.767762	11.753280
11.927706	834.499119	11.758298
11.542336	835.625000	11.763315
11.860720	822.371851	11.768333
11.492855	821.779776	11.773351
11.600076	829.558741	11.778368
11.563115	835.110145	11.783386
11.659611	840.377731	11.788403
11.929246	843.749503	11.793421
11.545918	845.914832	11.798439
11.749342	838.626317	11.803456
11.677259	846.196772	11.808474
11.754098	844.678400	11.813491
11.904084	842.356933	11.818509
11.499781	850.864226	11.823527
11.266942	843.159498	11.828544
11.623879	843.040266	11.833562
11.422865	843.718824	11.838579
11.352915	835.973405	11.843597
11.349123	853.913303	11.848615
11.457897	857.430341	11.853632
11.599280	864.646291	11.858650
11.606005	873.010490	11.863667
11.830805	864.815432	11.868685
11.750033	863.609277	11.873703
11.637102	860.567405	11.878720
11.657507	864.104559	11.883738
11.793015	883.082908	11.888755
12.136855	885.319779	11.893773
12.135546	900.451913	11.898791
11.939797	897.603612	11.903808
12.158216	892.080412	11.908826
11.984992	902.802915	11.913843
12.082831	895.542450	11.918861
12.550431	895.972750	11.923879
12.284416	866.347609	11.928896
12.293794	857.973032	11.933914
11.932075	853.472329	11.938931
12.383469	849.837684	11.943949
12.245781	865.862647	11.948967
11.921445	855.600432	11.953984
12.213357	853.202173	11.959002
11.805785	854.895802	11.964019
12.269019	858.124580	11.969037
12.133195	848.747010	11.974055
12.204504	855.608259	11.979072
12.381386	857.373783	11.984090
12.302186	847.742606	11.989107
12.158479	852.854253	11.994125
12.374394	854.942406	11.999143
12.116669	860.456297	12.004160
12.068367	848.848690	12.009178
11.953316	863.645904	12.014195
12.056683	852.780229	12.019213
11.817841	862.119884	12.024231
12.097736	884.288205	12.029248
12.588263	881.462895	12.034266
12.283972	882.166788	12.039283
12.432552	896.286715	12.044301
12.245120	891.329712	12.049319
12.248723	897.428675	12.054336
12.386780	878.838645	12.059354
12.356422	893.781905	12.064371
12.076153	874.308215	12.069389
12.302878	886.092379	12.074407
11.969436	883.902949	12.079424
12.027089	878.066220	12.084442
12.257279	890.960260	12.089459
12.339035	892.486826	12.094477
12.383245	886.031159	12.099495
12.118860	892.414718	12.104512
12.553228	879.598184	12.109530
12.177340	886.388291	12.114547
12.290644	890.675523	12.119565
12.750894	909.238883	12.124583
12.710023	903.224757	12.129600
12.609848	893.892637	12.134618
12.584760	889.086141	12.139635
12.519247	890.835632	12.144653
12.572478	880.886929	12.149671
12.508613	890.631669	12.154688
12.559700	889.020518	12.159706
12.652642	883.456058	12.164723
12.380811	889.673552	12.169741
12.684287	886.926584	12.174759
12.453135	889.382271	12.179776
12.849623	889.443283	12.184794
12.469649	900.515251	12.189811
12.533259	910.139152	12.194829
12.884665	915.542760	12.199847
12.701391	913.824688	12.204864
12.719361	900.380998	12.209882
12.506459	913.981441	12.214899
12.797241	922.518376	12.219917
12.824593	924.114949	12.224935
12.945543	922.224773	12.229952
12.641540	904.682997	12.234970
12.744913	888.085171	12.239987
12.541972	904.400439	12.245005
12.754982	905.166856	12.250023
12.716363	921.815164	12.255040
12.821138	928.850414	12.260058
13.062914	927.689755	12.265075
12.733013	916.952906	12.270093
13.365050	913.730251	12.275111
12.574479	900.120024	12.280128
12.519888	904.082110	12.285146
12.634004	917.632847	12.290163
12.833169	919.979837	12.295181
13.050435	920.975632	12.300199
12.823532	917.948056	12.305216
12.929711	919.675477	12.310234
13.004255	928.314672	12.315251
12.991465	916.958190	12.320269
13.067004	914.549228	12.325287
12.663791	916.947540	12.330304
13.240699	912.986480	12.335322
13.067561	924.847970	12.340339
13.175213	917.665584	12.345357
13.114516	919.430815	12.350375
13.168484	916.951610	12.355392
13.152779	913.191809	12.360410
13.018614	912.111973	12.365427
13.119126	916.067129	12.370445
13.257425	918.735740	12.375463
13.052433	924.165558	12.380480
13.020284	926.877492	12.385498
13.021217	918.896339	12.390515
13.329330	919.619486	12.395533
13.197021	919.225648	12.400551
12.614345	920.700229	12.405568
12.822262	914.238163	12.410586
12.863984	919.820092	12.415603
12.825100	916.837222	12.420621
12.772494	917.473152	12.425639
12.418099	925.722476	12.430656
12.968246	936.548854	12.435674
13.214779	950.758337	12.440691
13.183651	947.471669	12.445709
13.450088	945.198058	12.450727
12.799004	948.244126	12.455744
13.320458	942.763337	12.460762
13.564252	961.760694	12.465779
13.489298	962.231448	12.470797
13.611382	957.350421	12.475815
13.303362	961.793503	12.480832
13.610255	951.010839	12.485850
13.189518	954.520141	12.490867
13.188199	944.545181	12.495885
13.348556	948.136970	12.500903
13.614911	953.619596	12.505920
13.392905	949.530550	12.510938
13.379330	953.355380	12.515955
13.477483	952.297771	12.520973
13.628394	941.263376	12.525991
13.347690	952.654946	12.531008
13.198323	956.481944	12.536026
12.929998	961.836625	12.541043
12.992905	974.115569	12.546061
13.552712	955.999170	12.551079
13.458908	957.365414	12.556096
13.444556	947.420751	12.561114
13.612124	958.530409	12.566131
13.543206	947.310718	12.571149
13.748395	953.569863	12.576167
13.499488	952.398373	12.581184
13.491511	948.377683	12.586202
13.565160	951.058754	12.591219
13.435007	947.397568	12.596237
13.826997	949.188571	12.601255
13.426541	954.403299	12.606272
13.676493	949.442296	12.611290
13.803444	942.275801	12.616307
13.309306	945.699608	12.621325
13.923646	950.850955	12.626343
13.768674	965.396440	12.631360
13.757114	954.721704	12.636378
13.937594	950.400820	12.641395
13.505371	953.186349	12.646413
13.612320	942.300337	12.651431
13.842996	964.319650	12.656448
13.972920	963.142241	12.661466
13.740801	952.433296	12.666483
13.676495	948.854718	12.671501
14.234631	956.486607	12.676519
13.915726	957.387375	12.681536
13.679295	948.123990	12.686554
14.126350	946.617844	12.691571
13.854303	951.567888	12.696589
14.111362	942.836244	12.701607
13.385182	955.357756	12.706624
13.697297	951.290664	12.711642
14.099111	965.863611	12.716659
14.303409	974.744340	12.721677
14.222891	955.025565	12.726695
13.681066	950.566011	12.731712
13.897921	934.061964	12.736730
14.019821	951.402165	12.741747
14.075784	952.579711	12.746765
13.956155	943.147840	12.751783
13.938072	953.803606	12.756800
14.112620	969.601124	12.761818
14.199996	960.069495	12.766835
13.725167	959.358694	12.771853
13.924681	971.672336	12.776871
13.903520	974.906394	12.781888
13.912018	976.132330	12.786906
14.094646	968.240792	12.791923
13.772526	979.100730	12.796941
14.328033	964.958213	12.801959
14.197342	973.878160	12.806976
14.176738	988.351865	12.811994
14.278276	981.212776	12.817011
14.477454	980.680903	12.822029
14.299314	964.503865	12.827047
14.411459	985.177660	12.832064
14.538374	987.288805	12.837082
14.335394	988.076929	12.842099
14.411950	989.216434	12.847117
14.379494	974.267277	12.852135
14.240395	972.076422	12.857152
14.079079	966.341581	12.862170
14.485777	970.972022	12.867187
14.597499	974.796228	12.872205
14.544687	967.157145	12.877223
14.081878	961.587266	12.882240
13.960379	957.533373	12.887258
14.599029	971.647177	12.892275
14.439844	977.629788	12.897293
14.379254	985.591064	12.902311
14.264055	982.485774	12.907328
13.943401	986.353484	12.912346
14.247546	984.187792	12.917363
14.560340	978.777489	12.922381
14.278668	983.045974	12.927399
14.360661	977.218372	12.932416
14.513970	981.950128	12.937434
14.485359	982.480537	12.942451
14.024138	980.864678	12.947469
14.239157	970.323722	12.952487
14.101176	983.292260	12.957504
14.413989	988.981361	12.962522
14.985192	1004.167392	12.967539
14.866130	998.964251	12.972557
14.821817	990.849812	12.977575
14.140874	983.478863	12.982592
14.508582	1002.982285	12.987610
14.824506	1002.687181	12.992627
14.736503	1015.614619	12.997645
14.696452	1000.407874	13.002663
14.984387	990.051478	13.007680
14.632251	988.511081	13.012698
14.651016	971.001508	13.017715
14.437346	980.355182	13.022733
14.775854	1003.718129	13.027751
14.889946	1001.089233	13.032768
14.486882	995.942471	13.037786
14.963225	1000.626559	13.042803
14.956214	1005.000230	13.047821
14.972422	1001.540794	13.052839
15.113067	994.932552	13.057856
14.828037	992.522345	13.062874
14.855868	977.175686	13.067891
14.701508	978.072291	13.072909
14.608839	993.618566	13.077927
14.701943	996.077765	13.082944
14.659440	1017.656744	13.087962
14.836394	1006.596939	13.092979
14.673198	1001.484935	13.097997
14.645263	1002.898754	13.103015
14.841381	993.966359	13.108032
14.348064	1002.502222	13.113050
14.798121	999.312771	13.118067
14.783944	1008.820277	13.123085
15.288927	1017.810768	13.128103
15.051849	1029.240651	13.133120
15.033709	1039.981315	13.138138
15.207623	1030.666801	13.143155
15.196587	1022.057553	13.148173
14.847432	1011.230133	13.153191
15.067829	1018.298868	13.158208
14.982186	1022.563510	13.163226
15.357743	1024.772133	13.168243
14.874420	1033.427012	13.173261
15.357224	1028.958721	13.178279
15.198717	1028.825074	13.183296
15.079661	1042.691181	13.188314
15.186522	1038.301151	13.193331
14.945503	1040.755737	13.198349
15.069549	1040.854488	13.203367
15.468430	1036.025319	13.208384
15.276638	1033.853791	13.213402
15.403635	1021.531760	13.218419
15.275256	1036.485255	13.223437
15.398860	1028.349937	13.228455
15.300597	1032.973501	13.233472
15.149088	1036.863658	13.238490
15.288058	1026.116170	13.243507
14.997145	1031.663751	13.248525
14.953782	1034.830242	13.253543
15.565888	1034.154947	13.258560
15.311176	1035.413754	13.263578
15.376090	1034.159498	13.268595
15.205947	1038.935077	13.273613
15.152487	1034.185578	13.278631
15.494593	1026.022813	13.283648
15.075954	1037.157756	13.288666
15.515075	1048.633761	13.293683
15.582371	1056.490490	13.298701
15.892737	1058.259764	13.303719
15.887933	1044.979134	13.308736
15.564899	1048.632916	13.313754
15.607416	1039.972492	13.318771
15.636204	1037.168347	13.323789
15.557663	1035.123554	13.328807
15.558445	1033.729723	13.333824
15.227208	1032.641702	13.338842
15.702888	1041.830719	13.343859
15.711356	1046.601191	13.348877
15.882948	1058.294614	13.353895
15.782622	1034.878205	13.358912
15.471647	1032.980073	13.363930
15.362663	1042.398953	13.368947
15.467029	1055.144658	13.373965
15.786584	1067.794391	13.378983
16.331072	1062.727406	13.384000
15.805110	1065.385947	13.389018
15.959248	1065.046722	13.394035
15.632728	1045.679458	13.399053
15.806558	1061.613979	13.404071
15.868248	1057.613435	13.409088
15.947988	1056.472064	13.414106
15.777699	1066.557287	13.419123
15.934158	1064.291991	13.424141
15.914299	1065.872369	13.429159
15.894363	1068.204415	13.434176
15.496953	1066.251675	13.439194
15.687247	1055.651173	13.444211
15.666486	1056.054322	13.449229
15.847349	1059.425066	13.454247
16.003927	1057.614603	13.459264
15.680958	1071.981683	13.464282
15.828659	1069.311598	13.469299
15.832316	1063.245373	13.474317
15.954115	1069.611244	13.479335
15.846027	1056.684235	13.484352
15.617320	1069.421026	13.489370
16.329653	1066.348826	13.494387
16.244223	1086.188808	13.499405
16.099403	1072.628976	13.504423
16.183158	1060.000133	13.509440
15.656749	1059.202984	13.514458
15.978652	1069.567841	13.519475
15.905394	1081.777654	13.524493
16.162609	1088.395524	13.529511
16.375876	1082.103147	13.534528
16.017375	1091.156067	13.539546
16.342723	1093.758765	13.544563
16.374245	1085.859269	13.549581
16.328402	1084.831547	13.554599
16.449797	1084.179277	13.559616
16.256869	1082.136257	13.564634
16.373830	1086.292645	13.569651
16.511123	1092.398328	13.574669
16.442716	1088.988676	13.579687
16.527701	1085.625712	13.584704
16.349153	1087.871981	13.589722
16.390636	1083.959009	13.594739
16.492627	1077.090035	13.599757
16.298006	1088.106315	13.604775
16.464996	1076.245671	13.609792
16.362124	1079.263958	13.614810
16.364158	1086.150928	13.619827
16.574338	1087.078821	13.624845
16.403508	1087.488269	13.629863
16.269345	1080.995864	13.634880
16.559011	1089.008353	13.639898
16.576446	1081.463889	13.644915
16.642811	1091.050051	13.649933
16.174982	1090.532546	13.654951
16.282623	1082.734825	13.659968
16.375663	1079.251259	13.664986
16.579170	1065.803532	13.670003
16.787810	1080.195747	13.675021
16.348884	1082.950128	13.680039
16.637412	1075.834024	13.685056
16.444828	1091.713986	13.690074
16.537774	1090.916440	13.695091
16.808325	1105.950317	13.700109
16.710446	1111.579397	13.705127
17.069566	1111.669023	13.710144
16.558288	1100.344001	13.715162
16.675345	1107.217682	13.720179
17.031799	1107.530549	13.725197
16.602645	1109.151406	13.730215
16.764509	1108.874870	13.735232
16.916554	1112.025815	13.740250
16.982951	1121.563574	13.745267
17.255017	1113.632973	13.750285
17.039742	1097.430047	13.755303
16.820945	1082.747761	13.760320
16.776851	1081.614255	13.765338
16.975466	1089.889588	13.770355
17.027099	1087.453452	13.775373
16.725735	1101.834703	13.780391
16.843401	1096.020253	13.785408
17.136186	1108.213489	13.790426
17.227668	1111.861770	13.795443
17.220866	1104.787764	13.800461
16.853165	1099.794154	13.805479
16.920011	1101.336983	13.810496
16.944423	1115.021400	13.815514
16.758146	1125.478932	13.820531
16.922439	1122.474453	13.825549
17.059067	1123.546963	13.830567
17.085661	1107.848660	13.835584
17.265930	1111.804267	13.840602
17.304288	1115.171017	13.845619
17.234372	1113.729028	13.850637
17.131832	1115.290795	13.855655
17.072927	1116.564685	13.860672
17.372621	1114.473912	13.865690
16.989613	1118.678680	13.870707
16.903991	1117.821679	13.875725
16.882518	1115.804250	13.880743
17.348118	1110.382428	13.885760
17.098740	1106.099074	13.890778
16.960731	1119.743810	13.895795
17.298090	1123.548086	13.900813
17.333549	1129.399787	13.905831
17.468889	1131.469605	13.910848
17.607004	1136.330672	13.915866
17.430128	1136.993837	13.920883
17.678177	1139.695524	13.925901
17.444132	1121.084618	13.930919
17.239282	1121.839204	13.935936
17.506718	1124.104679	13.940954
17.355780	1138.257594	13.945971
17.741887	1130.214060	13.950989
17.541057	1141.731723	13.956007
17.938119	1137.759978	13.961024
17.636640	1120.832996	13.966042
17.561457	1109.244397	13.971059
17.458431	1113.767606	13.976077
17.731767	1116.316117	13.981095
17.538826	1115.881709	13.986112
17.524831	1114.935324	13.991130
17.523647	1126.698289	13.996147
17.616820	1133.507828	14.001165
17.621732	1145.574872	14.006183
17.321504	1130.885724	14.011200
17.543428	1136.918197	14.016218
17.355272	1135.275502	14.021235
17.893638	1140.127310	14.026253
17.699794	1137.243812	14.031271
17.699333	1149.181648	14.036288
17.909843	1137.210434	14.041306
17.552841	1147.485988	14.046323
18.182428	1138.782818	14.051341
17.864916	1153.461427	14.056359
17.794441	1147.778427	14.061376
17.776736	1145.457857	14.066394
17.806747	1138.893620	14.071411
18.175830	1137.247608	14.076429
17.808169	1137.596093	14.081447
17.780401	1134.621972	14.086464
17.718335	1138.458010	14.091482
17.498593	1151.282350	14.096499
18.198296	1156.230122	14.101517
18.075124	1165.200504	14.106535
18.209979	1171.185576	14.111552
18.166207	1172.107612	14.116570
18.180082	1174.410862	14.121587
18.413832	1164.752374	14.126605
18.132678	1156.460679	14.131623
17.683592	1146.299187	14.136640
18.188115	1152.821501	14.141658
17.832064	1174.375753	14.146675
18.055638	1170.913700	14.151693
17.974215	1173.232107	14.156711
18.282596	1156.391484	14.161728
18.338714	1168.149145	14.166746
18.295573	1172.249741	14.171763
18.391687	1183.507963	14.176781
18.185773	1177.605833	14.181799
17.856446	1174.885640	14.186816
18.283000	1179.338282	14.191834
17.873171	1178.703134	14.196851
18.016690	1176.968033	14.201869
17.782379	1165.753864	14.206887
18.410379	1187.441540	14.211904
18.481487	1200.972079	14.216922
18.643433	1197.711711	14.221939
18.497647	1200.557809	14.226957
18.774180	1199.856280	14.231975
18.534664	1177.765811	14.236992
18.521685	1161.924408	14.242010
18.339382	1167.629851	14.247027
18.256574	1163.141620	14.252045
18.154256	1177.086566	14.257063
18.464279	1187.014751	14.262080
18.376312	1197.658419	14.267098
18.366309	1207.836717	14.272115
18.559363	1200.055723	14.277133
19.006116	1201.890849	14.282151
18.852080	1198.156789	14.287168
19.167403	1186.383737	14.292186
18.620120	1193.984470	14.297203
18.810156	1187.913770	14.302221
18.987472	1188.395395	14.307239
18.948978	1197.857831	14.312256
18.775586	1187.516718	14.317274
18.763248	1181.198599	14.322291
19.179780	1184.302114	14.327309
18.828613	1168.243007	14.332327
18.416595	1168.061304	14.337344
18.659938	1182.029831	14.342362
18.963257	1187.171246	14.347379
18.860716	1179.509965	14.352397
18.992252	1182.893021	14.357415
19.287890	1185.681523	14.362432
19.074628	1179.461164	14.367450
19.008536	1192.895685	14.372467
19.223177	1187.387766	14.377485
18.957558	1174.954140	14.382503
18.988483	1169.230363	14.387520
19.048391	1153.937864	14.392538
19.052312	1188.812753	14.397555
19.017197	1180.752001	14.402573
19.166896	1184.282427	14.407591
19.053245	1192.181329	14.412608
19.118987	1181.089588	14.417626
19.369860	1196.369683	14.422643
19.278267	1172.120444	14.427661
19.048175	1169.458055	14.432679
19.049572	1179.218370	14.437696
19.436289	1188.700680	14.442714
19.262757	1189.065110	14.447731
18.947810	1188.405819	14.452749
19.064084	1192.652690	14.457767
18.842897	1190.490327	14.462784
19.377597	1182.141347	14.467802
19.044948	1192.084018	14.472819
19.262023	1189.884858	14.477837
19.313025	1185.861641	14.482855
19.039451	1195.655596	14.487872
19.339575	1198.007399	14.492890
19.364103	1187.985694	14.497907
19.174587	1184.583634	14.502925
19.267050	1195.968434	14.507943
19.284817	1205.094263	14.512960
19.590609	1211.579374	14.517978
19.029349	1231.450936	14.522995
19.541358	1225.365593	14.528013
19.568566	1218.277452	14.533031
19.610503	1224.809122	14.538048
19.745267	1213.125917	14.543066
19.539689	1218.794089	14.548083
19.852784	1221.211853	14.553101
19.731214	1208.671928	14.558119
19.498394	1227.633429	14.563136
19.580446	1217.585863	14.568154
19.305293	1225.956681	14.573171
19.661584	1220.482422	14.578189
19.688077	1214.479479	14.583207
19.405842	1227.538193	14.588224
19.472053	1219.550821	14.593242
19.668132	1213.228755	14.598259
19.250530	1214.190131	14.603277
19.375763	1222.989595	14.608295
19.616845	1247.382055	14.613312
20.086022	1242.913790	14.618330
19.797238	1263.984678	14.623347
20.072861	1253.852155	14.628365
20.461580	1244.087706	14.633383
20.083107	1238.549255	14.638400
19.823033	1219.618758	14.643418
19.729170	1221.386355	14.648435
19.647129	1235.453182	14.653453
20.125338	1237.333501	14.658471
20.095450	1242.659702	14.663488
20.067995	1237.303173	14.668506
20.006733	1248.506555	14.673523
20.145397	1246.178632	14.678541
20.438263	1251.899274	14.683559
20.091128	1249.759486	14.688576
20.152179	1248.955000	14.693594
20.158344	1254.034141	14.698611
20.191633	1250.136455	14.703629
20.468596	1244.969545	14.708647
20.242961	1249.544152	14.713664
20.679967	1235.626652	14.718682
20.215206	1221.538736	14.723699
20.386885	1220.706523	14.728717
20.349999	1207.060046	14.733735
19.983347	1218.910438	14.738752
20.314325	1222.217441	14.743770
20.398071	1240.132892	14.748787
20.423578	1244.528419	14.753805
20.444408	1247.741030	14.758823
20.100244	1256.363983	14.763840
20.489477	1257.268597	14.768858
20.189059	1253.671493	14.773875
20.275814	1246.994894	14.778893
20.700866	1237.832429	14.783911
20.261923	1244.729358	14.788928
20.136827	1244.209927	14.793946
20.324529	1253.763150	14.798963
20.181506	1252.421011	14.803981
20.652256	1244.298676	14.808999
20.392438	1255.508894	14.814016
20.454148	1247.981437	14.819034
20.690831	1255.826220	14.824051
20.532279	1270.062982	14.829069
20.787286	1276.540767	14.834087
20.859269	1280.161409	14.839104
21.026603	1275.099404	14.844122
20.735448	1263.827637	14.849139
20.518441	1249.604280	14.854157
20.922915	1247.453070	14.859175
20.688499	1259.606793	14.864192
20.657541	1261.783034	14.869210
20.959743	1266.397767	14.874227
20.826612	1272.327965	14.879245
20.569873	1272.510899	14.884263
20.968534	1275.352069	14.889280
20.961086	1284.520295	14.894298
20.989200	1281.149564	14.899315
20.790626	1281.928510	14.904333
21.151815	1276.034780	14.909351
21.014007	1280.147309	14.914368
21.228787	1289.697063	14.919386
20.949639	1271.678779	14.924403
20.755008	1283.021335	14.929421
20.807184	1270.858102	14.934439
21.032546	1275.824267	14.939456
21.026474	1269.551527	14.944474
21.056357	1279.082033	14.949491
20.904828	1278.543153	14.954509
21.000551	1276.721858	14.959527
20.838076	1283.545956	14.964544
21.079383	1270.712781	14.969562
21.045741	1278.546545	14.974579
21.008420	1297.360094	14.979597
21.117464	1301.751083	14.984615
21.064546	1312.078648	14.989632
21.465560	1295.773081	14.994650
21.386678	1291.377261	14.999667
21.158080	1305.209154	15.004685
21.322054	1297.607695	15.009703
21.418690	1299.810292	15.014720
21.376077	1295.795628	15.019738
21.477035	1288.906851	15.024755
21.287894	1303.694883	15.029773
21.385609	1289.953069	15.034791
21.469254	1297.529109	15.039808
21.418945	1290.864119	15.044826
21.645120	1288.238698	15.049843
21.585745	1297.218493	15.054861
21.351547	1296.637966	15.059879
21.679799	1291.359627	15.064896
21.575662	1296.925447	15.069914
22.022915	1299.923136	15.074931
21.597941	1303.459392	15.079949
21.627028	1293.525829	15.084967
21.779984	1300.075007	15.089984
21.575293	1289.767733	15.095002
22.008123	1289.495821	15.100019
21.727182	1280.870408	15.105037
22.002895	1279.192967	15.110055
21.665679	1300.180975	15.115072
21.826799	1282.912644	15.120090
22.070332	1277.202506	15.125107
21.734955	1289.043454	15.130125
22.085000	1280.957186	15.135143
21.634795	1289.331182	15.140160
21.348348	1288.414062	15.145178
22.405476	1307.717935	15.150195
22.254536	1313.916605	15.155213
22.369553	1293.359094	15.160231
22.142049	1295.990791	15.165248
21.858613	1294.962756	15.170266
22.198955	1279.635207	15.175283
21.935573	1292.743806	15.180301
22.081689	1282.943448	15.185319
22.251135	1295.036956	15.190336
21.890303	1298.698813	15.195354
21.909267	1299.651036	15.200371
21.754636	1317.484922	15.205389
22.420476	1313.663376	15.210407
22.199988	1318.068672	15.215424
22.121629	1315.742355	15.220442
22.376773	1318.517497	15.225459
22.364041	1314.703767	15.230477
22.169240	1320.575483	15.235495
22.032425	1315.231290	15.240512
22.029881	1322.694831	15.245530
22.055078	1324.061715	15.250547
22.009684	1328.711862	15.255565
22.537757	1319.290429	15.260583
22.269023	1324.286887	15.265600
22.136571	1325.371401	15.270618
22.654836	1328.266035	15.275635
22.430944	1343.552103	15.280653
22.591877	1337.060622	15.285671
22.990236	1361.672515	15.290688
22.565821	1341.460541	15.295706
22.764493	1321.994922	15.300723
22.759389	1318.390334	15.305741
22.555637	1325.103179	15.310759
22.859282	1315.770205	15.315776
22.774615	1317.911438	15.320794
22.937969	1308.707542	15.325811
23.012743	1317.960417	15.330829
22.769030	1305.398869	15.335847
22.650467	1322.963452	15.340864
22.629554	1327.093089	15.345882
22.914718	1316.502712	15.350899
23.005421	1316.567415	15.355917
22.961535	1317.978781	15.360935
22.775218	1320.535379	15.365952
23.042438	1329.502163	15.370970
23.156816	1321.044244	15.375987
22.759755	1319.490570	15.381005
23.006445	1315.994354	15.386023
23.173974	1316.049116	15.391040
22.874432	1318.113275	15.396058
23.191963	1314.136520	15.401075
22.793644	1321.802450	15.406093
22.839188	1321.279618	15.411111
23.240264	1318.243059	15.416128
23.541045	1330.106063	15.421146
22.941478	1323.724709	15.426163
23.022494	1314.614523	15.431181
22.760172	1334.381510	15.436199
23.106600	1332.097775	15.441216
23.246779	1343.061077	15.446234
22.930723	1345.977852	15.451251
23.146579	1342.135395	15.456269
23.464697	1336.315286	15.461287
23.598709	1346.764916	15.466304
23.624495	1339.924754	15.471322
23.599593	1344.374696	15.476339
23.309436	1335.080985	15.481357
23.165989	1340.418506	15.486375
23.742643	1347.393488	15.491392
23.126337	1342.204101	15.496410
23.376596	1340.616872	15.501427
23.533887	1339.964368	15.506445
23.812070	1337.411239	15.511463
23.773231	1338.807799	15.516480
23.526825	1345.907373	15.521498
23.585332	1340.689534	15.526515
23.610142	1342.006491	15.531533
23.410364	1342.697069	15.536551
23.779348	1342.174718	15.541568
23.516774	1337.518531	15.546586
23.662007	1334.782872	15.551603
23.385347	1340.973198	15.556621
23.460717	1336.283408	15.561639
23.483862	1335.671573	15.566656
23.481523	1334.556342	15.571674
23.990691	1346.788805	15.576691
23.682852	1357.923972	15.581709
23.632938	1363.062015	15.586727
23.985026	1367.468759	15.591744
23.961431	1375.662084	15.596762
23.958039	1367.237575	15.601779
23.963143	1372.334841	15.606797
23.943581	1368.057132	15.611815
24.261918	1357.137667	15.616832
23.871955	1377.580241	15.621850
24.201789	1365.142539	15.626867
24.080523	1366.129550	15.631885
23.968009	1371.029746	15.636903
24.339835	1370.336869	15.641920
24.178199	1369.524693	15.646938
24.342687	1366.872449	15.651955
24.333342	1363.333701	15.656973
24.295573	1366.924671	15.661991
24.343580	1357.264872	15.667008
24.008871	1348.052127	15.672026
24.230301	1346.261028	15.677043
24.204713	1367.968197	15.682061
23.997532	1363.654966	15.687079
24.278919	1367.060537	15.692096
24.179360	1366.324509	15.697114
23.965622	1365.586879	15.702131
24.137964	1358.349313	15.707149
24.280039	1364.532650	15.712167
24.241767	1359.663627	15.717184
24.173535	1364.252804	15.722202
24.308120	1376.697562	15.727219
24.551488	1390.005537	15.732237
24.615898	1401.287462	15.737255
24.844304	1392.743741	15.742272
24.372832	1406.932352	15.747290
24.794202	1388.417907	15.752307
24.668298	1389.754459	15.757325
24.727238	1382.928088	15.762343
25.219344	1390.169783	15.767360
25.007587	1388.018431	15.772378
24.749387	1375.458433	15.777395
24.846467	1360.773480	15.782413
24.772271	1366.765815	15.787431
24.751510	1354.128611	15.792448
24.644952	1377.034248	15.797466
25.073693	1371.841035	15.802483
25.045117	1375.495637	15.807501
25.088342	1387.073730	15.812519
24.956375	1370.881351	15.817536
24.844944	1382.408433	15.822554
24.952167	1384.792929	15.827571
25.251124	1385.112944	15.832589
25.310643	1382.816384	15.837607
25.020133	1362.921184	15.842624
24.626861	1367.068668	15.847642
24.748938	1371.433511	15.852659
25.026040	1379.425595	15.857677
24.727608	1394.113285	15.862695
24.717934	1385.666579	15.867712
24.874342	1389.852746	15.872730
25.016043	1383.565381	15.877747
24.855359	1386.714722	15.882765
25.037732	1401.806761	15.887783
25.211608	1408.465900	15.892800
25.257328	1415.309583	15.897818
25.554170	1418.517559	15.902835
25.657906	1413.463853	15.907853
25.432855	1419.052060	15.912871
25.625777	1397.170882	15.917888
25.861647	1406.260593	15.922906
25.661091	1391.907630	15.927923
25.358985	1380.040619	15.932941
25.145861	1377.415345	15.937959
25.663075	1386.369982	15.942976
25.491986	1402.740150	15.947994
25.743316	1408.756848	15.953011
26.035210	1413.421748	15.958029
25.743526	1408.023991	15.963047
25.893011	1386.446817	15.968064
25.641497	1381.244767	15.973082
25.549646	1379.323174	15.978099
25.200445	1386.022290	15.983117
25.450786	1397.990125	15.988135
25.735292	1397.309905	15.993152
25.577178	1419.462218	15.998170
25.634171	1410.815923	16.003187
26.078941	1410.914822	16.008205
25.536573	1404.356091	16.013223
25.688506	1392.742541	16.018240
25.403181	1400.926971	16.023258
25.676438	1404.570871	16.028275
26.177541	1412.496236	16.033293
26.008864	1423.938332	16.038311
26.263395	1424.472158	16.043328
26.395308	1436.833166	16.048346
26.290301	1431.310865	16.053363
26.505535	1400.113239	16.058381
26.179756	1409.483533	16.063399
26.280343	1398.390995	16.068416
26.072790	1395.909659	16.073434
26.054908	1400.852289	16.078451
26.681426	1398.120739	16.083469
25.757660	1410.037555	16.088487
25.882634	1405.880617	16.093504
26.150546	1417.941614	16.098522
26.298231	1434.709671	16.103539
26.378022	1430.636954	16.108557
26.395738	1426.484547	16.113575
26.678854	1421.870229	16.118592
26.706559	1419.437995	16.123610
26.684541	1424.288218	16.128627
26.552865	1406.699480	16.133645
26.659091	1425.224736	16.138663
26.530355	1418.446290	16.143680
26.193702	1415.987859	16.148698
26.280726	1423.218763	16.153715
26.738305	1417.905823	16.158733
26.721649	1427.987544	16.163751
26.747822	1429.466073	16.168768
26.738284	1426.855764	16.173786
26.571277	1424.317533	16.178803
26.817879	1416.512624	16.183821
26.888769	1425.927207	16.188839
27.145032	1429.881558	16.193856
27.148579	1422.709055	16.198874
26.966687	1418.872865	16.203891
27.199030	1421.542164	16.208909
26.929084	1434.088064	16.213927
27.126966	1428.547007	16.218944
27.231576	1418.037571	16.223962
26.900263	1399.854354	16.228979
26.959033	1389.151949	16.233997
26.872944	1395.036236	16.239015
27.028904	1406.900595	16.244032
27.105953	1420.657678	16.249050
26.754716	1420.895988	16.254067
26.899213	1423.096205	16.259085
26.736239	1416.673961	16.264103
26.913811	1416.463910	16.269120
26.868022	1418.531222	16.274138
26.667297	1427.646444	16.279155
27.045557	1429.935379	16.284173
27.129431	1452.116837	16.289191
27.502773	1463.766995	16.294208
27.467448	1457.293526	16.299226
27.856607	1458.337124	16.304243
27.956385	1441.793424	16.309261
27.575152	1427.688366	16.314279
27.561574	1413.388333	16.319296
27.543616	1414.312023	16.324314
27.143228	1421.600441	16.329331
27.499964	1415.795965	16.334349
27.495662	1420.198830	16.339367
27.301593	1413.503219	16.344384
27.548844	1438.108517	16.349402
27.600295	1447.720001	16.354419
27.704693	1441.665126	16.359437
27.584708	1447.069467	16.364455
27.651821	1454.892379	16.369472
27.787150	1452.539586	16.374490
27.688920	1447.560577	16.379507
27.802502	1448.581611	16.384525
27.590964	1453.088603	16.389543
27.829407	1448.743437	16.394560
27.797319	1451.995146	16.399578
27.003267	1454.362860	16.404595
27.625465	1446.414384	16.409613
27.575877	1465.368140	16.414631
27.848292	1462.661042	16.419648
28.208470	1476.449528	16.424666
28.190212	1473.375160	16.429683
28.248708	1471.676318	16.434701
28.410497	1473.437126	16.439719
28.313224	1481.001229	16.444736
28.197402	1482.640415	16.449754
28.233058	1478.019144	16.454771
28.364185	1477.581758	16.459789
28.146869	1480.029543	16.464807
28.535694	1474.903907	16.469824
28.213274	1474.408611	16.474842
28.492088	1474.409754	16.479859
28.411898	1477.078942	16.484877
28.248503	1477.016758	16.489895
28.355318	1487.654222	16.494912
28.719295	1470.246662	16.499930
28.352478	1475.640627	16.504947
28.470581	1479.352698	16.509965
28.670059	1471.713992	16.514983
28.602667	1473.755751	16.520000
28.894050	1466.480552	16.525018
28.307804	1460.876367	16.530035
28.350614	1461.954169	16.535053
28.556780	1470.578021	16.540071
28.838390	1467.296642	16.545088
28.752451	1463.411912	16.550106
28.402777	1473.997258	16.555123
28.331361	1474.821925	16.560141
28.392921	1479.610723	16.565159
28.858634	1470.886817	16.570176
28.774574	1461.610343	16.575194
28.635595	1472.892274	16.580211
28.900573	1464.282634	16.585229
28.800352	1464.545007	16.590247
28.781784	1462.894132	16.595264
28.955419	1462.927810	16.600282
28.795632	1483.793453	16.605299
28.904135	1495.055958	16.610317
29.249882	1498.910709	16.615335
29.282284	1500.175053	16.620352
29.445427	1503.703332	16.625370
28.938214	1483.932750	16.630387
29.001929	1486.729716	16.635405
29.205790	1488.034024	16.640423
29.207430	1502.833432	16.645440
29.252321	1492.808164	16.650458
29.072360	1504.168336	16.655475
29.313650	1501.555341	16.660493
29.675150	1501.580413	16.665511
29.316707	1490.783319	16.670528
29.661167	1483.551106	16.675546
29.316295	1490.992961	16.680563
29.467815	1489.869614	16.685581
29.122035	1491.690286	16.690599
29.428687	1494.674639	16.695616
29.534002	1499.319222	16.700634
29.281634	1501.128199	16.705651
29.628682	1491.245889	16.710669
29.438895	1483.148537	16.715687
29.346920	1492.223586	16.720704
29.860075	1492.401331	16.725722
29.586082	1499.941502	16.730739
29.626891	1484.015889	16.735757
29.827074	1496.937442	16.740775
29.812934	1518.472087	16.745792
30.241413	1520.373454	16.750810
29.912485	1513.196801	16.755827
29.795622	1497.329704	16.760845
29.904866	1502.062998	16.765863
29.803380	1514.417958	16.770880
30.174811	1506.711651	16.775898
29.867968	1522.680811	16.780915
29.907469	1518.278550	16.785933
30.005226	1519.108724	16.790951
29.945976	1521.851222	16.795968
30.285221	1519.343281	16.800986
30.081660	1530.840625	16.806003
30.412790	1521.864358	16.811021
30.235282	1516.150094	16.816039
29.956081	1519.814063	16.821056
30.423197	1526.144516	16.826074
30.203091	1522.322094	16.831091
30.340903	1517.163917	16.836109
30.922400	1523.834675	16.841127
30.574809	1520.127010	16.846144
30.614923	1519.565310	16.851162
30.270233	1515.914836	16.856179
30.421444	1509.855543	16.861197
30.428495	1513.275383	16.866215
30.166864	1523.710798	16.871232
30.570633	1513.122732	16.876250
30.339530	1507.196884	16.881267
30.133733	1516.041770	16.886285
30.378500	1514.841210	16.891303
30.087853	1517.718586	16.896320
30.674065	1535.691490	16.901338
30.873972	1546.169536	16.906355
30.963500	1556.607174	16.911373
31.072073	1550.909789	16.916391
30.773917	1560.393508	16.921408
31.024852	1547.941142	16.926426
31.170152	1529.848479	16.931443
30.802894	1520.000143	16.936461
30.563929	1518.353599	16.941479
30.728038	1538.230674	16.946496
30.814170	1538.229409	16.951514
31.034494	1546.079012	16.956531
31.021571	1545.733333	16.961549
31.107375	1546.547966	16.966567
30.966009	1556.037463	16.971584
31.073747	1553.513251	16.976602
31.078267	1549.637761	16.981619
31.197316	1550.329396	16.986637
31.283494	1556.301208	16.991655
30.971873	1555.655128	16.996672
31.150037	1538.653346	17.001690
30.978875	1541.132092	17.006707
31.159281	1550.946320	17.011725
31.129199	1551.794275	17.016743
31.443186	1559.571721	17.021760
31.859371	1559.752107	17.026778
32.114527	1576.526179	17.031795
31.867703	1564.522937	17.036813
31.841050	1548.724728	17.041831
31.449977	1541.246362	17.046848
31.497014	1532.104856	17.051866
31.742356	1530.989228	17.056883
31.528055	1530.136342	17.061901
31.635562	1532.732993	17.066919
31.953092	1548.182520	17.071936
31.749253	1562.962010	17.076954
31.844583	1558.247203	17.081971
31.644138	1562.477231	17.086989
31.921101	1550.663002	17.092007
31.736973	1561.337179	17.097024
32.120551	1552.088480	17.102042
32.339224	1553.535999	17.107059
31.790350	1559.346250	17.112077
32.129118	1558.521050	17.117095
31.885401	1559.300580	17.122112
32.027851	1559.838367	17.127130
31.999665	1558.767346	17.132147
32.043716	1553.830727	17.137165
32.181937	1554.734719	17.142183
32.230390	1560.303762	17.147200
32.045806	1556.720904	17.152218
32.130882	1557.685050	17.157235
31.935959	1561.498074	17.162253
32.406046	1549.659806	17.167271
31.858632	1553.895204	17.172288
32.245769	1555.473723	17.177306
32.453863	1581.220031	17.182323
32.324480	1594.497270	17.187341
32.842020	1589.952223	17.192359
32.386520	1588.175725	17.197376
32.742187	1586.872198	17.202394
32.509819	1584.448862	17.207411
32.331139	1578.916244	17.212429
32.593070	1571.115218	17.217447
32.630342	1588.853738	17.222464
32.607835	1582.039360	17.227482
32.649304	1580.379535	17.232499
32.559231	1589.433266	17.237517
32.635272	1588.185787	17.242535
32.553116	1592.558265	17.247552
32.605716	1589.300729	17.252570
32.459249	1583.936386	17.257587
32.198960	1601.874467	17.262605
32.749937	1605.504606	17.267623
32.866613	1611.065740	17.272640
32.817574	1612.329380	17.277658
33.060735	1616.112934	17.282675
32.990664	1616.805118	17.287693
33.281563	1610.592995	17.292711
33.029287	1620.203208	17.297728
33.213049	1613.169320	17.302746
33.238669	1612.943043	17.307763
33.082266	1611.503292	17.312781
33.203526	1604.712386	17.317799
33.045130	1612.971414	17.322816
33.247478	1606.399363	17.327834
33.253814	1617.262945	17.332851
33.293605	1642.316779	17.337869
33.479106	1635.191857	17.342887
33.603966	1638.849313	17.347904
34.031443	1638.786328	17.352922
34.051934	1619.616084	17.357939
33.400778	1608.971397	17.362957
33.667510	1599.939986	17.367975
33.494926	1608.068105	17.372992
33.556535	1606.743098	17.378010
33.696058	1606.630070	17.383027
34.000829	1623.608174	17.388045
33.978031	1611.509811	17.393063
33.753133	1606.353870	17.398080
33.470213	1597.832726	17.403098
34.145122	1608.966290	17.408115
33.806742	1623.094331	17.413133
34.045113	1623.643235	17.418151
33.831163	1629.248381	17.423168
34.091307	1631.473214	17.428186
34.289607	1628.174272	17.433203
34.032823	1629.030563	17.438221
34.396550	1605.022884	17.443239
34.197477	1625.297250	17.448256
34.150094	1629.458701	17.453274
34.082193	1615.730580	17.458291
33.800957	1628.510365	17.463309
34.043790	1624.524619	17.468327
34.102821	1629.649668	17.473344
34.128965	1637.535539	17.478362
34.336100	1626.893679	17.483379
34.477410	1637.748159	17.488397
34.541725	1629.144031	17.493415
34.482219	1627.502461	17.498432
34.229614	1627.750652	17.503450
34.170442	1625.603772	17.508467
34.191720	1633.865401	17.513485
34.423151	1642.066326	17.518503
34.535677	1648.828610	17.523520
34.533509	1649.996919	17.528538
34.729510	1652.091426	17.533555
34.645926	1654.172888	17.538573
34.627365	1645.514147	17.543591
34.701990	1646.095621	17.548608
34.622505	1650.871563	17.553626
35.213465	1642.275273	17.558643
35.012647	1658.831116	17.563661
35.071711	1652.776563	17.568679
35.026124	1647.219761	17.573696
35.013266	1642.641099	17.578714
35.185497	1641.632219	17.583731
35.014607	1647.190104	17.588749
35.192769	1639.421192	17.593767
35.058086	1646.094812	17.598784
35.062620	1648.240443	17.603802
35.181007	1640.717010	17.608819
34.725452	1635.516507	17.613837
35.413028	1636.369484	17.618855
35.419095	1637.782860	17.623872
35.195868	1638.360212	17.628890
35.568559	1631.943839	17.633907
35.364081	1641.959702	17.638925
35.419926	1636.010793	17.643943
35.396053	1649.712522	17.648960
35.551143	1668.631919	17.653978
36.025988	1666.138748	17.658995
35.716269	1650.511606	17.664013
35.540588	1629.615900	17.669031
35.557380	1635.134303	17.674048
35.383076	1653.498539	17.679066
36.002532	1649.753467	17.684083
35.524418	1658.691657	17.689101
36.028883	1662.207266	17.694119
36.095180	1656.323938	17.699136
35.872208	1667.008740	17.704154
36.341529	1661.120419	17.709171
35.877972	1653.408334	17.714189
35.771085	1634.822046	17.719207
36.130488	1646.950380	17.724224
36.392217	1662.362398	17.729242
36.584994	1639.766612	17.734259
36.190166	1634.780654	17.739277
36.122849	1630.024206	17.744295
35.840577	1628.149007	17.749312
35.796054	1638.153591	17.754330
36.158853	1650.224679	17.759347
36.243995	1643.777086	17.764365
36.205784	1646.127198	17.769383
36.290162	1659.918910	17.774400
36.023929	1654.732386	17.779418
36.840071	1665.615908	17.784435
36.465285	1669.062269	17.789453
36.647781	1663.315033	17.794471
36.509915	1657.000928	17.799488
36.175859	1663.934640	17.804506
36.651887	1661.559568	17.809523
36.676987	1663.076875	17.814541
36.314999	1662.716640	17.819559
36.655699	1660.568434	17.824576
36.521958	1660.088995	17.829594
36.868629	1667.974862	17.834611
37.021247	1675.376324	17.839629
36.879615	1681.764330	17.844647
36.894401	1683.325071	17.849664
36.802908	1686.893108	17.854682
36.590301	1686.324153	17.859699
36.760512	1693.148372	17.864717
36.720959	1696.894618	17.869735
37.027691	1687.693966	17.874752
36.565471	1689.084543	17.879770
37.034728	1680.433549	17.884787
36.855498	1688.129983	17.889805
36.844347	1710.543042	17.894823
37.144070	1700.830016	17.899840
37.424731	1717.138071	17.904858
37.588238	1705.497377	17.909875
37.323515	1703.744451	17.914893
37.478617	1697.523043	17.919911
38.108451	1706.690335	17.924928
37.773603	1702.415819	17.929946
37.787914	1682.433028	17.934963
37.331382	1671.067632	17.939981
37.180522	1686.348073	17.944999
37.388810	1692.728058	17.950016
37.535467	1705.346462	17.955034
37.860931	1703.068894	17.960051
37.888313	1704.309087	17.965069
38.108812	1698.868122	17.970087
37.989821	1701.163095	17.975104
37.746906	1705.168512	17.980122
37.690987	1707.948874	17.985139
37.987299	1708.496277	17.990157
37.818663	1707.454949	17.995175
38.282383	1702.744571	18.000192
37.842232	1698.679954	18.005210
38.246672	1700.461512	18.010227
38.439861	1696.327669	18.015245
37.835362	1697.971653	18.020263
38.018304	1695.049799	18.025280
38.105629	1708.511971	18.030298
38.149102	1697.776647	18.035315
38.037607	1697.938339	18.040333
37.953526	1702.997308	18.045351
38.370564	1694.595852	18.050368
38.119953	1707.715683	18.055386
38.014448	1702.300243	18.060403
38.135256	1704.468396	18.065421
38.579071	1721.332697	18.070439
38.697694	1715.999495	18.075456
38.443277	1715.802170	18.080474
38.524397	1725.628587	18.085491
38.671166	1716.769473	18.090509
38.506282	1722.127005	18.095527
38.527890	1709.534864	18.100544
38.634136	1731.860453	18.105562
38.802363	1722.928506	18.110579
38.533385	1723.167791	18.115597
38.478180	1719.777271	18.120615
39.028513	1732.047724	18.125632
38.842558	1748.022925	18.130650
38.793354	1753.032648	18.135667
39.091113	1759.341977	18.140685
38.530609	1764.928069	18.145703
39.162121	1753.430451	18.150720
38.876534	1755.615574	18.155738
39.515707	1754.776351	18.160755
39.339769	1750.166147	18.165773
39.066337	1747.610413	18.170791
39.622246	1746.027552	18.175808
39.204160	1751.462757	18.180826
39.318438	1749.533037	18.185843
39.555445	1743.889547	18.190861
39.205877	1744.739721	18.195879
39.637040	1733.706672	18.200896
39.434685	1739.861259	18.205914
39.755871	1743.117639	18.210931
39.624055	1726.995324	18.215949
39.285482	1748.715384	18.220967
39.840146	1759.515029	18.225984
39.721705	1765.746892	18.231002
39.926963	1765.273826	18.236019
40.073956	1766.889689	18.241037
39.859201	1758.437695	18.246055
39.894490	1743.881669	18.251072
39.837058	1742.912111	18.256090
39.829627	1749.828696	18.261107
40.211952	1761.906684	18.266125
39.965549	1765.467467	18.271143
40.028248	1759.950204	18.276160
40.027012	1766.702798	18.281178
39.993648	1769.340286	18.286195
40.121880	1769.485984	18.291213
39.770202	1772.258347	18.296231
39.869686	1766.664932	18.301248
40.348859	1773.852655	18.306266
40.014176	1767.412580	18.311283
40.191749	1768.812783	18.316301
40.277305	1779.870847	18.321319
40.408118	1778.650913	18.326336
40.215250	1799.690738	18.331354
40.758191	1802.814434	18.336371
40.880653	1782.761482	18.341389
40.604569	1785.173557	18.346407
40.970341	1788.622558	18.351424
40.944568	1785.482644	18.356442
41.240370	1785.857909	18.361459
41.031367	1759.464780	18.366477
40.842192	1759.959549	18.371495
41.120969	1754.959869	18.376512
40.833511	1747.253476	18.381530
40.891087	1743.456365	18.386547
40.992707	1745.440510	18.391565
40.870634	1751.448386	18.396583
41.013404	1751.196253	18.401600
41.010704	1772.889385	18.406618
41.406521	1789.337920	18.411635
41.446133	1785.725440	18.416653
41.124604	1785.749812	18.421671
41.400664	1780.732857	18.426688
41.382550	1781.254473	18.431706
41.206969	1780.234758	18.436723
41.414912	1780.149002	18.441741
41.528393	1786.425808	18.446759
41.487553	1788.622456	18.451776
41.227685	1776.322612	18.456794
41.030983	1777.726992	18.461811
41.416044	1777.076790	18.466829
41.408226	1782.671942	18.471847
41.341843	1774.908140	18.476864
41.114363	1790.821553	18.481882
41.590470	1802.662447	18.486899
41.791125	1796.762571	18.491917
41.460565	1810.468472	18.496935
42.015746	1815.090776	18.501952
42.045902	1813.083620	18.506970
41.772153	1820.542617	18.511987
42.028264	1812.039750	18.517005
42.078575	1817.659952	18.522023
41.949728	1814.530373	18.527040
41.862404	1808.280287	18.532058
41.722394	1804.887819	18.537075
42.376382	1818.193266	18.542093
42.487341	1827.656980	18.547111
42.427018	1831.065979	18.552128
42.694881	1827.022310	18.557146
42.495387	1819.931199	18.562163
42.968345	1806.333392	18.567181
42.492500	1804.489961	18.572199
42.685339	1788.488128	18.577216
42.831802	1799.180865	18.582234
42.531069	1801.088212	18.587251
42.842582	1801.834266	18.592269
42.540098	1811.800496	18.597287
42.506497	1803.663190	18.602304
42.655913	1805.746914	18.607322
42.387697	1792.417445	18.612339
42.499326	1793.867716	18.617357
42.752156	1810.056861	18.622375
43.125364	1830.235749	18.627392
42.698413	1824.279548	18.632410
42.748443	1823.964992	18.637427
43.352629	1821.772241	18.642445
43.035483	1833.278737	18.647463
43.039515	1828.870242	18.652480
43.030903	1826.762415	18.657498
43.215976	1838.749056	18.662515
43.384415	1826.323089	18.667533
43.288675	1829.642280	18.672551
42.904877	1836.544332	18.677568
43.318366	1830.359300	18.682586
42.882273	1824.577426	18.687603
43.114022	1829.454143	18.692621
42.804395	1852.150564	18.697639
43.323795	1848.337147	18.702656
43.139429	1857.125739	18.707674
42.944923	1860.606715	18.712691
43.429839	1868.649351	18.717709
43.480909	1890.931734	18.722727
43.866421	1893.741537	18.727744
44.144293	1883.443484	18.732762
44.106898	1888.369812	18.737779
44.270944	1888.644029	18.742797
44.317994	1885.530640	18.747815
44.111808	1868.538272	18.752832
44.228514	1848.940863	18.757850
44.168140	1855.605837	18.762867
44.101703	1844.105190	18.767885
43.923441	1848.097992	18.772903
44.112702	1865.509582	18.777920
44.344794	1873.685721	18.782938
44.205585	1879.572869	18.787955
44.548323	1875.314473	18.792973
44.190901	1879.779166	18.797991
44.246110	1878.932901	18.803008
44.711130	1874.824951	18.808026
44.379680	1879.693381	18.813043
44.730481	1875.306501	18.818061
44.614517	1879.369717	18.823079
44.691660	1867.872686	18.828096
44.998663	1865.916025	18.833114
44.618711	1873.663041	18.838131
44.892621	1877.957275	18.843149
44.988348	1874.878754	18.848167
44.730121	1877.577430	18.853184
44.688448	1863.860106	18.858202
44.515774	1874.014746	18.863219
44.694709	1873.994997	18.868237
44.162327	1874.793505	18.873255
44.598196	1877.641435	18.878272
45.158672	1892.704152	18.883290
44.960481	1896.039106	18.888307
45.170868	1893.211883	18.893325
45.260118	1894.858165	18.898343
45.413176	1898.742497	18.903360
45.445272	1889.980178	18.908378
45.280277	1904.720902	18.913395
45.432657	1896.592379	18.918413
45.604947	1892.329667	18.923431
45.355238	1893.888470	18.928448
45.645017	1889.725034	18.933466
45.210434	1903.273421	18.938483
45.354720	1894.368361	18.943501
45.285371	1903.182261	18.948519
45.509359	1929.682749	18.953536
45.753966	1924.943163	18.958554
45.827945	1924.601815	18.963571
45.931920	1921.114481	18.968589
46.010980	1918.164677	18.973607
46.041592	1924.053895	18.978624
46.166224	1915.031413	18.983642
46.045769	1922.080913	18.988659
46.176200	1914.450250	18.993677
46.091001	1913.563608	18.998695
46.032149	1922.057508	19.003712
46.394667	1911.052998	19.008730
46.019162	1916.828040	19.013747
46.375848	1909.253093	19.018765
46.370920	1917.467241	19.023783
46.162422	1914.469886	19.028800
46.535943	1911.604483	19.033818
46.392845	1906.524678	19.038835
46.476183	1909.179319	19.043853
46.866326	1904.983350	19.048871
46.771933	1911.347898	19.053888
46.915368	1913.593830	19.058906
46.797325	1913.171822	19.063923
46.735331	1914.020542	19.068941
46.735479	1911.361705	19.073959
46.270570	1916.467927	19.078976
46.693481	1926.871001	19.083994
46.795989	1941.192003	19.089011
46.783742	1935.368196	19.094029
47.041471	1942.554406	19.099047
46.924858	1937.421794	19.104064
47.288592	1939.845282	19.109082
46.967486	1942.072517	19.114099
46.940305	1940.747194	19.119117
47.232457	1937.761387	19.124135
47.105963	1944.099957	19.129152
47.412834	1948.394669	19.134170
47.423326	1974.592358	19.139187
47.213921	1973.285531	19.144205
47.245818	1973.412311	19.149223
47.280753	1963.211037	19.154240
47.640852	1966.372657	19.159258
47.946289	1977.293751	19.164275
47.735053	1966.991827	19.169293
47.607710	1972.389891	19.174311
47.605197	1970.583370	19.179328
47.996888	1966.590653	19.184346
47.623947	1967.203385	19.189363
47.555945	1971.430730	19.194381
48.075548	1967.332239	19.199399
48.277541	1985.180007	19.204416
48.374794	1976.929854	19.209434
48.598137	1971.654056	19.214451
48.470515	1959.980969	19.219469
48.472423	1954.974028	19.224487
48.423162	1953.705104	19.229504
48.134925	1956.064691	19.234522
48.237207	1963.095907	19.239539
48.003967	1956.870856	19.244557
48.476137	1962.620201	19.249575
48.206247	1968.351434	19.254592
48.345539	1968.924794	19.259610
48.144850	1975.085104	19.264627
48.045434	1979.834523	19.269645
47.769213	1971.622270	19.274663
48.441005	1996.793289	19.279680
48.933621	2002.735906	19.284698
49.114097	2014.701595	19.289715
49.375678	2017.649213	19.294733
49.353640	1999.623017	19.299751
49.112092	1986.900529	19.304768
49.301136	1968.391304	19.309786
48.882479	1969.563112	19.314803
49.031135	1972.489817	19.319821
49.405170	1975.852070	19.324839
49.009504	1992.125734	19.329856
49.471631	1998.784147	19.334874
49.504477	1996.201380	19.339891
49.015309	1999.882638	19.344909
49.086572	1995.389371	19.349927
49.007630	2006.968041	19.354944
49.368711	2004.512119	19.359962
49.460567	2007.939510	19.364979
49.669263	2004.501973	19.369997
49.772365	1988.982040	19.375015
49.727153	1996.209280	19.380032
49.653813	1999.935398	19.385050
49.498765	1999.280154	19.390067
49.666691	2002.907552	19.395085
49.727418	2003.246281	19.400103
49.823617	2025.221626	19.405120
49.727896	2024.689046	19.410138
49.816094	2025.391116	19.415155
49.680373	2037.754710	19.420173
50.083023	2027.979594	19.425191
49.865273	2032.632845	19.430208
50.007166	2031.494320	19.435226
50.192761	2043.974888	19.440243
50.568270	2055.603881	19.445261
50.861448	2058.708869	19.450279
50.778313	2045.149993	19.455296
50.774248	2022.792848	19.460314
50.494271	2017.402584	19.465331
50.858131	2019.964634	19.470349
51.073375	2015.196018	19.475367
50.879419	2016.239172	19.480384
50.614908	2011.904721	19.485402
50.714983	2009.878113	19.490419
50.510207	2026.361192	19.495437
51.293158	2027.847391	19.500455
50.667484	2037.011934	19.505472
50.979563	2046.466759	19.510490
51.185388	2056.606214	19.515507
51.210419	2060.457220	19.520525
51.196666	2052.779848	19.525543
51.306772	2054.321136	19.530560
51.329274	2044.827900	19.535578
51.549261	2045.915440	19.540595
51.155709	2047.209865	19.545613
51.213294	2053.900507	19.550631
51.184607	2053.265519	19.555648
51.456142	2049.404634	19.560666
51.202953	2048.271555	19.565683
51.254956	2055.149324	19.570701
51.499656	2040.739501	19.575719
51.255689	2058.394141	19.580736
51.642601	2071.198322	19.585754
51.812306	2075.951327	19.590771
51.716659	2080.712554	19.595789
51.922383	2075.421327	19.600807
51.985488	2079.156607	19.605824
51.725041	2068.025419	19.610842
51.739851	2074.958945	19.615859
51.866423	2074.135716	19.620877
52.251756	2065.160808	19.625895
51.955492	2079.036855	19.630912
52.161294	2077.125039	19.635930
51.937361	2080.965029	19.640947
52.222109	2095.890256	19.645965
52.601492	2094.341847	19.650983
52.695435	2097.791548	19.656000
52.753394	2097.555197	19.661018
53.182715	2096.363857	19.666035
52.557804	2082.413806	19.671053
52.523687	2069.011952	19.676071
52.727265	2081.605119	19.681088
52.850660	2090.049314	19.686106
53.057506	2093.556532	19.691123
52.978764	2091.468721	19.696141
53.048644	2083.666303	19.701159
52.841863	2087.597349	19.706176
52.883882	2092.428934	19.711194
53.055198	2103.966914	19.716211
52.997159	2096.911941	19.721229
53.060702	2090.758453	19.726247
53.174211	2091.281359	19.731264
52.708522	2091.815728	19.736282
53.277718	2080.031737	19.741299
53.092847	2089.570478	19.746317
53.383580	2094.159408	19.751335
53.614039	2111.509158	19.756352
53.490716	2109.855250	19.761370
53.570194	2103.415487	19.766387
53.693135	2118.590880	19.771405
53.453388	2103.448521	19.776423
53.636853	2106.757262	19.781440
53.757256	2114.647288	19.786458
53.617025	2104.259136	19.791475
53.532480	2102.376399	19.796493
53.642692	2105.349242	19.801511
53.518611	2129.335767	19.806528
53.599681	2141.158349	19.811546
53.839934	2145.894994	19.816563
54.069785	2153.672081	19.821581
54.016977	2140.916703	19.826599
54.172576	2148.279912	19.831616
54.650706	2168.563550	19.836634
54.365594	2156.946848	19.841651
54.297114	2167.618670	19.846669
54.609235	2167.477709	19.851687
55.004328	2172.352542	19.856704
54.683638	2178.062722	19.861722
55.071099	2171.916302	19.866739
54.830739	2167.240639	19.871757
54.807422	2156.240662	19.876775
54.739548	2155.180292	19.881792
54.606149	2169.427111	19.886810
55.251253	2160.647786	19.891827
54.964812	2170.129154	19.896845
55.097760	2158.057377	19.901863
55.109720	2161.676533	19.906880
55.050586	2162.322646	19.911898
55.275074	2163.277178	19.916915
55.207267	2171.975041	19.921933
55.336481	2174.149155	19.926951
55.602089	2170.692532	19.931968
55.443809	2159.658560	19.936986
55.737120	2160.665887	19.942003
55.280639	2161.233380	19.947021
55.360863	2158.434113	19.952039
55.342875	2167.986267	19.957056
55.587060	2168.043328	19.962074
55.675255	2158.256907	19.967091
55.371947	2167.845974	19.972109
55.381667	2190.443865	19.977127
55.821535	2196.821027	19.982144
55.589789	2196.268598	19.987162
56.053785	2190.262465	19.992179
55.814502	2202.400213	19.997197
56.120304	2194.979783	20.002215
55.935658	2190.177200	20.007232
55.887663	2204.162716	20.012250
56.113445	2204.431265	20.017267
56.238177	2224.213182	20.022285
56.432952	2218.343053	20.027303
56.382559	2221.647748	20.032320
56.333075	2226.121887	20.037338
56.662291	2225.212610	20.042355
56.586982	2221.102524	20.047373
56.792719	2220.571694	20.052391
56.691482	2210.261076	20.057408
56.608100	2209.793767	20.062426
56.858077	2216.026542	20.067443
56.974752	2210.801357	20.072461
56.754681	2220.230453	20.077479
56.970367	2242.794190	20.082496
56.834366	2250.168037	20.087514
57.151289	2249.756224	20.092531
57.098125	2250.897969	20.097549
57.263255	2235.873012	20.102567
57.623064	2236.008400	20.107584
57.360604	2241.591077	20.112602
57.333069	2239.526475	20.117619
57.318868	2242.068560	20.122637
57.418982	2236.172337	20.127655
57.629371	2247.361475	20.132672
57.465061	2252.139613	20.137690
57.697120	2253.397010	20.142707
57.850951	2258.037743	20.147725
57.693504	2268.957586	20.152743
57.785374	2271.734295	20.157760
57.756631	2274.680924	20.162778
58.222889	2268.755286	20.167795
58.140931	2272.810230	20.172813
58.439089	2273.479389	20.177831
58.631627	2264.003784	20.182848
58.237161	2270.156273	20.187866
58.416165	2270.055024	20.192883
58.449491	2275.017620	20.197901
58.230797	2274.404374	20.202919
58.473258	2270.718305	20.207936
58.395715	2273.809207	20.212954
58.365991	2262.654713	20.217971
58.362003	2267.534897	20.222989
58.795793	2264.048101	20.228007
58.642872	2269.700082	20.233024
58.771332	2268.887161	20.238042
58.753547	2271.769778	20.243059
58.650044	2269.025259	20.248077
58.692824	2283.520609	20.253095
59.085231	2288.979738	20.258112
58.891102	2291.542509	20.263130
59.109920	2289.009469	20.268147
58.815060	2295.649014	20.273165
58.840272	2288.412690	20.278183
59.240615	2288.529571	20.283200
59.299275	2306.319709	20.288218
59.518948	2315.850005	20.293235
59.575276	2328.904289	20.298253
59.319080	2329.762289	20.303271
59.716590	2318.268280	20.308288
59.686779	2322.514409	20.313306
59.892887	2319.201041	20.318323
59.842874	2310.795530	20.323341
59.526525	2328.044555	20.328359
59.834719	2312.239836	20.333376
59.906250	2312.754530	20.338394
59.714921	2312.663297	20.343411
59.878778	2317.700984	20.348429
59.712001	2314.445493	20.353447
59.663293	2319.013618	20.358464
59.995609	2347.454065	20.363482
60.008429	2342.772337	20.368499
60.232539	2350.034761	20.373517
60.266541	2348.885697	20.378535
60.190847	2342.809838	20.383552
60.245905	2347.609822	20.388570
60.489373	2350.035928	20.393587
60.666373	2370.787476	20.398605
61.113107	2361.693795	20.403623
61.115827	2357.364494	20.408640
61.330196	2364.439571	20.413658
61.319255	2359.496429	20.418675
60.991950	2343.721104	20.423693
61.045138	2336.720865	20.428711
61.359737	2333.163205	20.433728
61.584586	2331.358045	20.438746
61.136909	2323.013908	20.443763
61.223278	2321.723722	20.448781
60.683815	2321.716982	20.453799
61.527119	2333.304122	20.458816
61.395240	2347.467986	20.463834
61.330613	2348.480540	20.468851
61.319625	2358.877658	20.473869
61.417122	2350.588686	20.478887
61.825310	2346.144164	20.483904
61.493158	2357.112621	20.488922
61.790408	2357.894721	20.493939
62.056441	2359.851778	20.498957
61.990653	2372.485561	20.503975
62.323164	2376.779700	20.508992
62.090732	2374.390498	20.514010
61.961992	2369.164870	20.519027
62.212729	2382.847659	20.524045
62.239008	2387.673079	20.529063
62.290704	2383.889971	20.534080
62.121909	2387.186316	20.539098
62.363199	2379.875861	20.544115
62.376915	2377.335952	20.549133
62.443315	2372.584736	20.554151
62.577241	2378.444458	20.559168
62.305685	2380.620853	20.564186
62.458611	2386.002471	20.569203
62.719448	2404.741530	20.574221
62.962846	2410.460939	20.579239
62.784055	2400.909808	20.584256
62.741360	2405.908629	20.589274
62.753398	2407.819086	20.594291
62.929044	2404.224532	20.599309
63.018380	2406.711350	20.604327
63.087891	2419.196247	20.609344
63.342882	2429.934674	20.614362
63.346608	2432.351789	20.619379
63.455115	2427.421366	20.624397
63.171537	2435.086991	20.629415
63.625389	2436.531953	20.634432
63.352994	2438.386665	20.639450
63.632930	2435.504941	20.644467
63.749584	2429.364785	20.649485
63.713435	2433.033290	20.654503
64.036459	2426.261633	20.659520
63.804444	2418.781944	20.664538
63.931821	2422.161238	20.669555
64.242314	2419.425245	20.674573
63.916893	2415.416865	20.679591
64.165982	2422.694093	20.684608
64.302702	2440.227408	20.689626
64.199984	2448.694006	20.694643
64.243355	2442.257116	20.699661
64.425182	2443.931859	20.704679
64.629890	2440.838760	20.709696
64.650586	2450.944898	20.714714
64.376422	2441.799042	20.719731
64.598710	2448.015032	20.724749
64.414819	2450.323594	20.729767
64.457429	2444.084258	20.734784
64.839369	2446.974868	20.739802
65.146299	2450.912453	20.744819
65.166920	2438.546244	20.749837
65.047120	2435.041445	20.754855
65.348504	2452.789872	20.759872
65.540864	2454.093411	20.764890
65.424491	2457.164784	20.769907
65.550680	2437.533173	20.774925
65.028672	2433.644078	20.779943
65.622193	2451.869001	20.784960
65.669211	2455.492471	20.789978
65.480142	2458.010538	20.794995
65.659820	2455.945917	20.800013
65.427663	2467.444940	20.805031
65.915342	2463.133107	20.810048
66.099798	2457.010475	20.815066
65.931738	2461.733591	20.820083
66.036104	2448.765975	20.825101
65.569307	2458.239725	20.830119
65.846275	2448.091831	20.835136
66.020486	2452.719807	20.840154
66.138881	2485.933940	20.845171
65.927967	2490.057097	20.850189
66.144790	2491.197551	20.855207
66.377568	2478.024845	20.860224
66.639416	2477.745742	20.865242
66.688852	2480.568475	20.870259
66.906654	2484.680629	20.875277
66.632993	2476.357847	20.880295
66.701827	2486.052928	20.885312
66.721450	2478.380458	20.890330
66.572441	2479.047537	20.895347
67.125356	2494.868151	20.900365
66.942487	2510.257248	20.905383
67.231365	2505.607409	20.910400
67.271841	2499.739246	20.915418
66.959860	2506.850579	20.920435
67.436608	2502.565736	20.925453
66.974313	2506.803660	20.930471
67.136202	2501.155971	20.935488
67.111487	2504.040958	20.940506
67.276356	2509.783025	20.945523
67.502847	2526.815021	20.950541
67.629319	2543.656882	20.955559
67.872829	2535.220659	20.960576
67.783732	2537.042733	20.965594
67.894780	2531.447525	20.970611
68.004044	2528.874088	20.975629
67.941256	2532.504698	20.980647
67.953838	2522.140616	20.985664
67.858663	2520.765065	20.990682
67.967395	2520.907302	20.995699
68.224000	2521.260130	21.000717
68.279196	2547.167168	21.005735
68.394449	2549.834165	21.010752
68.430222	2563.181396	21.015770
68.379087	2562.515452	21.020787
68.510329	2554.317049	21.025805
68.550493	2554.013163	21.030823
68.698702	2544.601008	21.035840
68.926685	2552.694729	21.040858
68.759200	2551.133891	21.045875
68.848410	2551.589573	21.050893
68.733972	2551.088805	21.055911
68.562396	2572.585585	21.060928
69.271062	2578.283094	21.065946
69.135718	2579.238454	21.070963
69.035575	2575.845329	21.075981
69.333855	2577.314043	21.080999
69.204673	2583.246845	21.086016
69.927656	2574.890419	21.091034
69.316396	2584.058607	21.096051
69.648891	2570.586684	21.101069
69.680722	2586.406887	21.106087
70.013919	2591.277123	21.111104
70.192305	2594.358081	21.116122
69.718326	2599.109349	21.121139
70.161249	2604.733070	21.126157
69.898086	2611.987950	21.131175
70.040192	2608.325667	21.136192
70.468240	2597.998783	21.141210
70.292044	2604.544840	21.146227
70.490109	2601.984669	21.151245
70.074898	2610.579562	21.156263
70.303714	2609.460686	21.161280
70.573071	2600.359563	21.166298
70.467246	2615.118744	21.171315
70.144385	2613.892612	21.176333
70.563107	2630.739029	21.181351
70.223809	2633.423674	21.186368
70.501248	2626.708869	21.191386
70.434215	2637.724065	21.196403
70.769648	2648.115314	21.201421
71.086640	2661.637017	21.206439
70.987446	2670.166733	21.211456
71.450400	2665.168807	21.216474
71.370453	2656.622983	21.221491
71.641747	2657.313133	21.226509
71.810597	2651.941390	21.231527
71.622919	2659.021623	21.236544
71.844800	2653.464355	21.241562
71.502792	2651.661886	21.246579
71.638292	2656.419542	21.251597
71.768352	2652.879312	21.256615
71.706081	2660.178181	21.261632
72.261458	2661.479230	21.266650
72.114023	2689.021088	21.271667
72.284447	2694.943007	21.276685
72.279253	2685.109286	21.281703
72.493809	2682.698338	21.286720
72.636434	2678.571015	21.291738
72.506329	2682.399388	21.296755
72.377178	2675.558057	21.301773
72.706063	2671.382242	21.306791
72.488532	2683.611256	21.311808
72.954839	2671.949327	21.316826
72.538738	2683.790701	21.321843
72.523086	2680.258007	21.326861
72.598625	2681.071839	21.331879
72.935146	2681.233916	21.336896
73.143034	2682.882529	21.341914
72.845671	2685.960626	21.346931
73.131736	2664.910843	21.351949
73.233082	2663.523278	21.356967
73.252975	2667.212694	21.361984
73.483388	2666.863590	21.367002
73.174902	2689.338619	21.372019
73.406721	2696.401124	21.377037
73.200076	2700.406314	21.382055
73.332500	2710.464239	21.387072
73.592099	2696.750720	21.392090
73.351322	2704.752302	21.397107
73.774376	2709.639617	21.402125
74.326787	2718.944717	21.407143
73.862953	2725.165931	21.412160
73.879131	2719.215090	21.417178
73.894757	2720.780127	21.422195
74.111439	2713.242294	21.427213
74.286522	2720.380717	21.432231
73.932668	2726.974685	21.437248
74.158433	2740.031632	21.442266
74.055564	2743.627577	21.447283
74.254556	2737.443774	21.452301
74.532957	2737.552860	21.457319
74.921658	2737.233896	21.462336
74.837034	2737.044322	21.467354
74.747433	2756.483812	21.472371
75.115197	2757.032048	21.477389
75.443042	2758.257716	21.482407
75.248814	2771.757695	21.487424
75.555910	2766.883912	21.492442
75.504932	2772.340105	21.497459
75.901587	2764.426460	21.502477
75.862810	2757.121360	21.507495
75.675042	2743.972251	21.512512
76.045074	2738.222369	21.517530
75.979241	2731.511489	21.522547
75.824558	2735.037257	21.527565
75.973690	2732.189101	21.532583
75.830570	2727.103516	21.537600
75.883352	2743.311345	21.542618
76.012731	2754.805170	21.547635
75.814315	2756.198896	21.552653
76.143970	2755.320816	21.557671
75.985652	2767.217685	21.562688
76.248658	2764.253467	21.567706
76.100750	2762.603943	21.572723
75.987370	2777.988515	21.577741
76.297419	2778.822654	21.582759
76.195898	2794.054108	21.587776
76.344701	2786.932556	21.592794
76.528423	2800.391366	21.597811
76.589679	2809.487141	21.602829
76.802565	2811.841212	21.607847
76.913811	2824.088447	21.612864
77.110484	2818.560087	21.617882
77.003778	2814.289290	21.622899
76.789640	2818.505582	21.627917
77.365212	2827.726610	21.632935
77.345261	2839.933334	21.637952
77.640668	2839.414439	21.642970
77.725887	2838.290536	21.647987
77.970150	2831.598448	21.653005
77.859408	2829.941594	21.658023
78.426203	2834.969758	21.663040
78.506184	2822.059400	21.668058
78.105243	2799.139177	21.673075
78.002402	2798.553417	21.678093
78.080427	2798.467671	21.683111
78.014163	2814.039367	21.688128
77.933180	2821.373686	21.693146
78.371640	2825.204598	21.698163
78.440936	2827.527676	21.703181
78.718870	2830.582784	21.708199
78.261119	2838.702961	21.713216
78.527107	2842.360022	21.718234
78.420183	2845.734229	21.723251
78.361816	2844.569881	21.728269
78.063413	2854.934907	21.733287
78.448034	2865.265028	21.738304
78.445854	2867.087738	21.743322
78.708803	2880.758715	21.748339
78.703685	2897.849469	21.753357
79.373514	2888.017068	21.758375
79.458388	2902.048972	21.763392
79.670972	2897.550990	21.768410
79.508496	2887.747067	21.773427
79.371984	2894.911469	21.778445
79.617846	2899.799384	21.783463
79.922280	2902.789107	21.788480
79.834141	2893.604764	21.793498
79.825908	2897.282348	21.798515
79.884648	2921.008796	21.803533
79.957378	2914.948932	21.808551
79.805107	2933.584854	21.813568
79.893582	2916.710549	21.818586
79.777721	2920.899212	21.823603
80.105858	2940.149044	21.828621
80.353896	2944.286245	21.833639
80.798734	2947.370489	21.838656
80.935037	2933.745243	21.843674
80.861379	2938.568648	21.848691
80.957759	2933.896949	21.853709
81.178719	2938.660256	21.858727
81.211705	2935.556854	21.863744
81.372747	2932.487410	21.868762
81.463862	2939.292183	21.873779
81.407033	2938.340559	21.878797
81.661941	2929.843974	21.883815
81.330694	2942.563225	21.888832
81.580138	2934.711220	21.893850
81.650820	2920.620860	21.898867
81.413177	2931.174315	21.903885
81.620471	2926.103595	21.908903
81.362709	2930.237759	21.913920
81.428708	2932.787768	21.918938
81.659010	2927.214050	21.923955
81.710484	2942.863662	21.928973
81.930766	2948.975071	21.933991
81.710164	2952.794842	21.939008
81.870212	2957.276103	21.944026
82.277238	2951.805454	21.949043
82.178955	2979.622375	21.954061
82.631777	2986.525271	21.959079
82.673665	2989.339108	21.964096
82.653425	2981.622583	21.969114
82.827397	2979.960399	21.974131
82.761579	2984.037270	21.979149
83.069498	2974.439809	21.984167
83.198338	2980.395873	21.989184
83.296895	2972.109740	21.994202
83.206302	2981.274800	21.999219
83.159220	2985.596206	22.004237
83.386957	2981.369703	22.009255
83.403658	2981.625968	22.014272
83.263145	2989.121379	22.019290
83.280038	2981.769574	22.024307
82.921989	2989.601315	22.029325
83.459830	2990.171456	22.034343
83.620146	2994.248759	22.039360
83.323924	3002.885227	22.044378
83.536614	3003.642557	22.049395
83.613670	3031.433353	22.054413
83.950677	3032.483126	22.059431
84.229876	3034.270778	22.064448
84.244544	3041.743723	22.069466
83.992328	3036.196548	22.074483
84.035251	3034.579240	22.079501
84.768780	3051.064659	22.084519
84.478783	3060.130435	22.089536
84.654900	3057.447835	22.094554
84.842260	3057.454254	22.099571
84.743548	3055.696965	22.104589
84.914710	3050.660521	22.109607
84.825604	3062.025720	22.114624
85.010161	3064.369945	22.119642
85.062776	3055.068944	22.124659
85.313133	3082.426482	22.129677
85.727583	3081.309970	22.134695
86.129486	3084.251340	22.139712
85.756340	3067.545272	22.144730
85.801945	3048.505126	22.149747
85.872104	3056.206698	22.154765
86.117932	3056.069994	22.159783
85.945316	3057.484680	22.164800
85.608717	3080.845606	22.169818
85.975154	3069.442396	22.174835
85.790912	3079.882800	22.179853
85.801062	3079.565754	22.184871
85.960896	3075.788230	22.189888
86.175512	3091.764176	22.194906
86.272462	3097.368082	22.199923
86.297100	3113.595122	22.204941
86.546633	3094.484610	22.209959
86.642375	3094.920725	22.214976
86.461103	3105.631516	22.219994
86.897757	3102.053121	22.225011
86.753672	3117.502550	22.230029
87.655792	3107.943433	22.235047
87.811088	3119.632849	22.240064
87.382036	3109.682680	22.245082
87.978415	3107.478648	22.250099
87.740207	3113.147783	22.255117
87.718776	3113.278858	22.260135
87.791545	3113.210513	22.265152
88.131929	3112.018838	22.270170
88.151341	3113.895094	22.275187
87.914221	3110.599287	22.280205
88.413281	3104.415361	22.285223
87.892357	3093.363085	22.290240
88.190027	3105.987998	22.295258
87.907822	3104.511018	22.300275
88.304832	3102.467880	22.305293
88.139468	3095.117791	22.310311
88.434606	3098.854347	22.315328
88.095406	3101.333940	22.320346
88.544486	3128.247709	22.325363
88.404209	3140.152118	22.330381
88.478928	3147.627395	22.335399
88.731841	3142.805755	22.340416
88.749653	3143.924420	22.345434
89.055442	3136.615354	22.350451
89.236662	3143.706898	22.355469
89.081173	3160.842080	22.360487
89.167686	3171.128360	22.365504
89.225736	3168.546351	22.370522
89.444268	3156.962796	22.375539
89.650675	3159.296339	22.380557
89.599850	3152.425318	22.385575
89.626498	3165.607258	22.390592
89.478404	3169.311166	22.395610
89.750771	3179.238794	22.400627
89.984225	3199.767958	22.405645
89.614071	3196.967335	22.410663
90.002439	3192.436284	22.415680
89.692071	3201.809833	22.420698
90.165172	3207.287060	22.425715
90.248336	3219.148310	22.430733
90.143845	3221.051745	22.435751
90.690302	3217.828798	22.440768
90.371249	3225.089261	22.445786
90.730520	3235.694682	22.450803
91.044271	3245.279692	22.455821
91.090650	3239.066185	22.460839
91.438116	3240.517782	22.465856
91.223089	3241.599339	22.470874
91.443306	3245.918381	22.475891
91.293504	3248.072217	22.480909
91.681304	3250.450997	22.485927
91.498824	3249.941370	22.490944
91.427291	3244.856384	22.495962
91.582079	3254.776719	22.500979
91.910228	3274.998213	22.505997
91.818269	3278.592479	22.511015
92.001370	3275.838216	22.516032
92.130867	3273.811307	22.521050
92.146137	3272.738301	22.526067
92.241964	3277.186173	22.531085
92.319096	3292.460642	22.536103
92.983405	3293.938630	22.541120
92.744292	3303.195743	22.546138
92.594949	3293.517738	22.551155
92.762854	3293.426979	22.556173
92.972157	3293.925438	22.561191
93.305930	3290.042350	22.566208
93.067441	3298.988337	22.571226
93.216296	3290.222075	22.576243
93.154329	3295.776329	22.581261
93.077473	3297.482296	22.586279
93.131739	3292.682804	22.591296
92.900622	3307.640509	22.596314
93.378172	3321.661846	22.601331
93.252193	3316.668510	22.606349
93.321001	3320.059057	22.611367
93.750642	3330.634411	22.616384
93.962620	3339.807561	22.621402
93.875922	3342.109249	22.626419
94.381750	3343.515005	22.631437
94.113254	3342.566441	22.636455
94.272585	3334.152751	22.641472
94.252297	3361.821643	22.646490
94.463202	3369.757593	22.651507
94.507946	3378.431629	22.656525
94.626799	3378.853698	22.661543
95.065263	3376.065884	22.666560
94.807455	3378.965139	22.671578
95.186078	3365.355380	22.676595
94.970314	3358.955614	22.681613
94.664654	3376.454034	22.686631
95.196844	3385.961699	22.691648
95.314911	3394.575598	22.696666
95.359044	3388.903738	22.701683
95.688320	3388.977653	22.706701
95.435520	3397.014254	22.711719
95.663782	3386.290335	22.716736
95.737325	3386.008870	22.721754
95.806692	3393.007594	22.726771
96.176787	3404.729842	22.731789
96.227000	3411.481739	22.736807
96.427095	3422.756502	22.741824
96.294628	3426.316944	22.746842
96.627943	3430.137037	22.751859
96.571541	3427.893187	22.756877
96.581099	3424.021907	22.761895
96.788910	3428.696988	22.766912
96.645899	3411.645434	22.771930
96.595980	3415.805224	22.776947
96.683336	3417.183677	22.781965
96.616528	3432.297817	22.786983
97.111048	3437.486942	22.792000
96.665516	3451.833365	22.797018
96.957189	3463.069796	22.802035
97.347168	3476.167555	22.807053
97.593463	3479.167785	22.812071
97.678567	3474.096212	22.817088
97.778777	3485.907605	22.822106
97.799932	3472.736741	22.827123
97.925859	3483.761205	22.832141
97.879462	3483.538927	22.837159
98.629702	3484.980295	22.842176
98.498414	3494.707108	22.847194
98.716912	3488.601675	22.852211
98.677371	3486.262511	22.857229
98.608065	3488.616465	22.862247
99.027159	3482.422377	22.867264
98.989712	3487.729341	22.872282
98.930040	3489.802962	22.877299
99.077733	3484.077342	22.882317
99.026984	3491.719974	22.887335
99.243192	3487.177522	22.892352
98.890642	3493.305060	22.897370
99.053328	3499.224629	22.902387
99.308162	3492.471063	22.907405
99.226649	3516.502306	22.912423
99.305997	3507.108821	22.917440
99.514310	3511.346835	22.922458
99.280734	3509.018863	22.927475
99.707708	3525.248751	22.932493
99.570630	3549.155761	22.937511
99.944251	3539.003786	22.942528
100.239900	3555.680210	22.947546
100.644551	3572.330768	22.952563
100.910679	3575.832863	22.957581
100.936795	3572.644248	22.962599
101.127511	3559.959076	22.967616
100.786365	3544.029493	22.972634
100.906513	3545.997031	22.977651
100.663052	3554.507763	22.982669
100.522461	3559.235727	22.987687
100.632300	3565.051454	22.992704
100.963816	3574.473497	22.997722
101.213025	3588.975331	23.002739
101.502004	3586.490136	23.007757
101.547055	3582.610983	23.012775
101.877092	3580.914680	23.017792
101.753727	3586.904384	23.022810
101.980820	3584.646740	23.027827
102.164761	3579.682818	23.032845
101.773614	3584.148250	23.037863
102.164221	3581.040353	23.042880
102.560660	3580.868918	23.047898
102.387309	3574.461267	23.052915
102.483289	3572.323715	23.057933
102.321702	3579.908720	23.062951
102.678001	3585.513258	23.067968
102.246122	3607.148970	23.072986
102.591805	3599.566952	23.078003
102.607262	3597.255692	23.083021
102.446261	3612.543840	23.088039
102.832846	3610.123617	23.093056
102.914147	3624.181569	23.098074
103.051342	3632.775904	23.103091
103.224445	3643.280476	23.108109
103.281787	3662.460202	23.113127
103.531017	3666.753703	23.118144
103.772322	3663.964558	23.123162
103.678383	3672.138832	23.128179
104.029268	3649.042727	23.133197
103.765396	3668.107817	23.138215
104.274069	3681.158578	23.143232
104.697954	3693.817054	23.148250
104.471218	3695.113571	23.153267
104.764043	3686.810312	23.158285
104.746395	3699.024024	23.163303
104.755765	3685.255312	23.168320
105.149030	3693.402245	23.173338
104.931154	3693.046484	23.178355
104.844379	3681.456294	23.183373
104.594439	3690.864640	23.188391
104.952422	3705.379319	23.193408
105.678070	3721.540376	23.198426
105.392969	3725.359575	23.203443
105.860700	3724.406267	23.208461
105.569974	3722.111722	23.213479
105.686585	3720.853827	23.218496
105.624291	3716.078977	23.223514
105.791579	3727.125520	23.228531
106.121501	3738.342840	23.233549
105.933490	3745.233853	23.238567
106.105080	3744.353887	23.243584
106.189181	3751.308211	23.248602
106.167182	3756.432789	23.253619
106.444678	3771.041932	23.258637
106.492033	3779.901198	23.263655
106.506161	3777.696039	23.268672
106.863364	3785.445034	23.273690
106.731725	3782.011570	23.278707
107.188589	3797.847821	23.283725
107.223970	3812.122591	23.288743
107.443086	3806.689782	23.293760
107.605420	3802.972302	23.298778
107.375375	3806.412730	23.303795
107.595488	3797.242273	23.308813
107.645874	3804.373062	23.313831
107.839886	3821.385865	23.318848
107.999931	3829.093835	23.323866
107.965300	3833.947684	23.328883
108.467535	3823.364421	23.333901
108.520719	3829.438041	23.338919
108.551043	3823.057657	23.343936
108.965106	3816.887498	23.348954
108.935309	3814.735655	23.353971
109.020520	3816.829083	23.358989
109.021316	3817.325791	23.364007
109.257857	3812.539722	23.369024
109.317598	3803.587104	23.374042
109.073073	3805.736982	23.379059
109.496688	3803.869285	23.384077
109.279900	3807.265002	23.389095
109.409004	3798.854481	23.394112
109.323111	3800.559633	23.399130
109.463842	3821.305341	23.404147
109.544312	3828.991025	23.409165
109.889375	3837.961767	23.414183
109.934685	3829.557201	23.419200
109.898006	3834.970064	23.424218
109.511146	3843.412913	23.429235
110.257689	3857.218239	23.434253
110.236781	3873.734709	23.439271
110.144457	3873.729074	23.444288
110.366465	3868.056784	23.449306
110.626837	3893.030963	23.454323
110.750041	3884.333962	23.459341
110.966148	3882.830867	23.464359
110.687991	3879.932236	23.469376
110.984753	3885.090015	23.474394
111.341905	3907.566662	23.479411
111.479260	3903.202873	23.484429
111.338982	3917.943785	23.489447
111.530168	3918.563767	23.494464
111.711875	3906.183355	23.499482
111.472712	3922.157181	23.504499
111.864266	3933.239258	23.509517
112.371709	3935.146789	23.514535
112.600592	3923.197165	23.519552
112.729661	3919.935560	23.524570
112.465984	3927.549021	23.529587
112.908630	3923.587551	23.534605
112.618034	3928.394351	23.539623
112.565427	3929.938107	23.544640
113.025619	3943.303409	23.549658
113.169669	3959.661607	23.554675
113.275595	3959.327929	23.559693
113.347949	3962.768033	23.564711
113.060517	3963.417098	23.569728
113.453334	3955.091270	23.574746
113.035419	3966.345706	23.579763
113.315386	3969.273538	23.584781
113.435255	3985.996006	23.589799
113.403502	3981.397924	23.594816
113.857177	3997.321917	23.599834
114.212256	4007.359250	23.604851
114.244081	4013.660494	23.609869
114.207120	4010.907818	23.614887
114.418459	4005.816789	23.619904
114.766941	4008.349829	23.624922
114.737755	4026.589937	23.629939
114.726035	4033.322022	23.634957
114.780752	4034.848449	23.639975
115.033144	4038.832071	23.644992
115.564446	4031.014049	23.650010
115.163559	4033.962263	23.655027
115.149625	4025.910307	23.660045
115.252459	4048.718955	23.665063
115.492142	4053.504711	23.670080
116.201621	4058.917201	23.675098
115.734280	4073.137870	23.680115
116.024758	4066.510850	23.685133
116.335990	4068.212620	23.690151
115.888110	4064.719532	23.695168
116.310507	4074.270176	23.700186
116.461153	4081.276253	23.705203
116.668402	4081.432545	23.710221
116.979376	4078.436139	23.715239
117.115136	4084.450543	23.720256
117.117285	4082.578829	23.725274
117.027002	4079.793611	23.730291
117.426930	4078.526278	23.735309
117.217853	4082.313315	23.740327
117.072543	4083.353879	23.745344
117.340984	4086.255290	23.750362
117.450743	4095.391051	23.755379
117.434260	4102.974382	23.760397
117.512721	4104.802024	23.765415
117.425954	4107.507396	23.770432
117.388633	4100.843969	23.775450
117.956538	4137.173325	23.780467
117.870213	4140.163681	23.785485
117.869144	4138.712196	23.790503
118.218017	4158.801100	23.795520
118.145356	4168.453681	23.800538
118.010298	4175.914902	23.805555
118.280320	4190.104395	23.810573
118.753431	4194.738628	23.815591
118.886109	4206.699149	23.820608
118.685282	4198.938627	23.825626
118.977493	4228.513818	23.830643
119.066390	4239.985904	23.835661
119.613669	4231.526922	23.840679
119.529357	4234.647679	23.845696
119.984903	4252.218558	23.850714
119.901557	4255.148205	23.855731
120.222812	4258.222034	23.860749
120.227922	4260.455535	23.865767
120.097676	4257.440262	23.870784
120.459019	4251.960569	23.875802
120.329756	4269.730858	23.880819
120.622533	4276.815513	23.885837
120.866801	4274.985665	23.890855
120.549373	4290.515689	23.895872
120.790482	4281.378883	23.900890
121.154337	4301.370608	23.905907
121.103987	4310.310498	23.910925
121.260897	4295.739659	23.915943
121.157349	4308.276720	23.920960
121.474889	4309.664861	23.925978
122.013157	4333.963482	23.930995
121.884969	4335.783167	23.936013
122.010454	4334.778890	23.941031
122.051249	4337.675047	23.946048
122.372660	4331.610159	23.951066
122.332432	4336.667857	23.956083
122.405126	4345.645313	23.961101
122.478539	4355.441600	23.966119
122.313470	4366.683680	23.971136
122.593151	4368.160763	23.976154
122.867181	4366.426386	23.981171
123.206753	4388.532596	23.986189
122.968335	4387.760895	23.991207
123.262941	4384.445857	23.996224
123.470114	4391.412811	24.001242
123.501635	4398.176887	24.006259
123.582473	4402.453139	24.011277
123.607986	4407.820489	24.016295
123.659679	4426.663093	24.021312
123.961384	4424.684752	24.026330
124.082951	4428.665287	24.031347
124.147794	4443.493677	24.036365
124.553682	4450.407350	24.041383
124.612942	4462.557375	24.046400
124.737869	4450.946199	24.051418
124.749540	4447.692858	24.056435
124.561367	4442.705498	24.061453
124.745297	4459.433639	24.066471
125.255384	4462.488120	24.071488
125.463107	4470.533829	24.076506
125.721120	4474.619004	24.081523
125.494663	4481.175332	24.086541
125.557318	4471.317459	24.091559
125.252437	4490.098183	24.096576
125.799999	4495.561601	24.101594
125.689367	4505.461231	24.106611
125.676256	4508.573035	24.111629
126.009853	4511.420451	24.116647
126.209798	4514.706908	24.121664
126.394757	4520.651536	24.126682
126.642852	4529.263873	24.131699
126.790024	4527.865422	24.136717
127.071720	4523.117349	24.141735
127.135801	4525.419102	24.146752
127.305204	4535.207123	24.151770
127.076424	4549.098233	24.156787
127.043998	4553.152279	24.161805
127.125191	4547.983753	24.166823
127.366601	4570.226921	24.171840
127.444275	4585.664394	24.176858
127.706888	4590.740250	24.181875
127.440566	4593.096212	24.186893
128.331464	4593.242708	24.191911
128.133554	4610.638085	24.196928
128.371084	4612.033567	24.201946
128.536222	4604.417901	24.206963
128.685951	4609.965992	24.211981
128.927047	4609.459169	24.216999
128.573027	4641.585805	24.222016
128.783367	4637.401105	24.227034
129.054218	4641.135751	24.232051
128.957847	4665.701970	24.237069
129.181402	4671.089448	24.242087
129.532842	4669.825357	24.247104
129.573807	4670.875341	24.252122
129.695618	4689.767705	24.257139
129.846685	4695.835727	24.262157
130.464882	4690.721349	24.267175
130.188911	4699.418009	24.272192
130.726304	4693.582670	24.277210
131.006326	4692.973736	24.282227
130.855465	4694.449150	24.287245
130.791296	4691.226795	24.292263
131.353442	4703.262024	24.297280
131.471355	4709.922190	24.302298
131.579568	4720.461048	24.307315
131.666122	4712.900836	24.312333
132.193441	4714.063786	24.317351
131.921605	4707.260487	24.322368
132.106018	4703.223767	24.327386
132.163297	4707.560299	24.332403
132.059231	4711.006094	24.337421
132.220515	4710.189988	24.342439
132.427024	4712.452486	24.347456
132.288840	4696.311005	24.352474
132.150457	4702.426855	24.357491
131.986353	4724.285635	24.362509
132.291506	4734.926620	24.367527
132.609564	4725.697701	24.372544
132.445638	4741.876486	24.377562
132.738085	4759.359918	24.382579
132.848067	4773.265732	24.387597
132.908061	4772.216338	24.392615
133.245211	4799.618076	24.397632
133.074533	4789.745795	24.402650
133.663453	4791.457676	24.407667
133.568730	4801.113506	24.412685
134.157036	4806.304138	24.417703
134.355423	4802.419033	24.422720
134.359947	4809.677948	24.427738
134.677003	4796.244851	24.432755
134.524040	4799.308948	24.437773
134.743319	4805.777194	24.442791
135.026148	4808.244438	24.447808
135.176760	4818.510980	24.452826
135.200891	4824.066514	24.457843
135.301920	4839.129479	24.462861
135.393368	4829.884394	24.467879
135.441871	4834.154689	24.472896
135.905983	4837.542462	24.477914
135.921136	4829.014770	24.482931
135.513175	4841.331667	24.487949
135.764182	4849.690134	24.492967
135.907790	4855.612981	24.497984
135.796153	4867.026528	24.503002
136.244651	4882.299471	24.508019
136.074474	4893.941234	24.513037
136.293184	4898.090895	24.518055
136.827288	4920.501970	24.523072
136.436298	4922.376957	24.528090
137.014163	4931.628795	24.533107
136.798286	4951.091100	24.538125
137.100932	4953.134974	24.543143
137.144178	4958.050721	24.548160
136.885323	4972.619682	24.553178
137.273780	4973.531948	24.558195
137.546382	4996.274950	24.563213
138.014525	5001.521333	24.568231
138.703205	5009.318544	24.573248
138.358395	5007.729661	24.578266
138.626039	4997.889166	24.583283
138.801636	5033.952725	24.588301
139.123820	5039.177564	24.593319
139.020330	5037.289329	24.598336
138.930291	5033.161243	24.603354
139.215356	5034.478825	24.608371
139.329286	5031.908144	24.613389
139.647787	5042.077794	24.618407
139.741200	5055.000276	24.623424
139.450586	5062.310436	24.628442
139.738520	5058.327787	24.633459
140.111025	5074.190699	24.638477
140.072441	5076.115755	24.643495
140.223030	5089.606831	24.648512
140.042773	5096.783800	24.653530
140.543451	5101.435409	24.658547
140.953718	5118.325700	24.663565
141.346303	5121.272551	24.668583
141.568528	5116.288825	24.673600
141.128877	5119.316091	24.678618
141.284167	5110.091792	24.683635
141.718644	5109.715224	24.688653
141.381014	5113.149694	24.693671
141.756811	5118.621240	24.698688
141.689054	5133.876962	24.703706
142.336537	5144.286842	24.708723
142.100600	5149.260985	24.713741
142.036614	5139.072397	24.718759
142.427495	5141.739975	24.723776
142.550354	5175.927332	24.728794
142.924997	5173.921099	24.733811
142.695632	5176.257259	24.738829
142.801968	5175.012366	24.743847
142.545455	5168.834749	24.748864
142.643608	5190.490594	24.753882
143.003233	5190.235854	24.758899
143.168643	5203.233973	24.763917
143.220545	5212.540990	24.768935
144.090236	5212.488618	24.773952
143.921026	5208.331043	24.778970
144.260299	5198.180916	24.783987
144.424847	5211.851308	24.789005
144.663549	5228.691711	24.794023
144.974442	5237.992569	24.799040
145.176243	5237.866673	24.804058
145.115100	5238.324442	24.809075
145.309925	5245.584404	24.814093
145.185907	5232.467147	24.819111
145.112168	5238.961939	24.824128
145.321905	5235.085090	24.829146
145.682177	5243.724568	24.834163
145.737182	5262.016389	24.839181
145.863704	5265.515949	24.844199
145.648384	5262.478311	24.849216
145.835525	5275.971384	24.854234
146.054837	5300.234441	24.859251
146.155202	5301.992848	24.864269
146.458692	5291.645400	24.869287
146.570193	5303.264551	24.874304
146.438624	5328.637327	24.879322
147.282847	5332.507747	24.884339
146.936735	5330.317397	24.889357
146.903582	5342.150658	24.894375
147.260173	5357.327821	24.899392
147.202977	5370.901116	24.904410
147.775435	5381.719270	24.909427
147.669748	5389.835744	24.914445
147.914214	5397.314375	24.919463
148.105914	5394.037786	24.924480
148.096192	5427.656186	24.929498
148.155684	5416.237414	24.934515
148.399702	5427.578430	24.939533
148.794451	5446.368732	24.944551
149.062559	5445.399095	24.949568
148.914969	5454.623848	24.954586
149.559914	5452.374469	24.959603
149.218188	5453.716507	24.964621
149.760239	5470.834256	24.969639
149.889714	5470.818747	24.974656
149.825989	5481.552297	24.979674
149.637418	5483.806556	24.984691
150.325788	5494.695019	24.989709
150.549430	5506.678519	24.994727
150.827915	5516.407001	24.999744
150.636489	5513.118877	25.004762
150.596284	5503.810097	25.009779
150.823704	5515.162582	25.014797
151.045393	5528.514320	25.019815
151.231975	5532.362332	25.024832
151.258716	5534.284525	25.029850
151.412235	5533.805533	25.034867
151.485580	5537.680131	25.039885
151.510813	5560.984189	25.044903
151.921262	5568.730004	25.049920
151.771391	5580.451610	25.054938
151.864973	5590.583968	25.059955
152.117646	5592.958276	25.064973
152.360115	5599.652974	25.069991
152.768086	5600.336041	25.075008
152.614395	5609.569768	25.080026
152.737953	5614.703980	25.085043
153.112446	5612.643773	25.090061
153.082582	5622.674485	25.095079
153.405889	5629.423565	25.100096
153.386500	5638.860348	25.105114
153.488233	5650.647929	25.110131
153.551195	5653.706046	25.115149
153.691564	5662.013929	25.120167
154.024721	5670.710100	25.125184
153.804959	5675.657717	25.130202
154.460985	5687.201752	25.135219
154.372333	5704.510987	25.140237
154.155698	5701.856213	25.145255
154.767749	5715.103842	25.150272
154.808716	5730.482358	25.155290
155.254813	5725.285835	25.160307
155.357849	5743.057607	25.165325
155.313216	5759.234268	25.170343
155.657974	5758.631532	25.175360
155.961119	5766.656632	25.180378
156.206422	5780.523658	25.185395
156.516388	5789.991165	25.190413
156.864130	5789.009926	25.195431
156.946407	5792.404693	25.200448
157.254164	5785.486652	25.205466
157.307581	5791.870886	25.210483
157.381662	5781.266489	25.215501
157.394327	5786.377736	25.220519
157.406562	5782.271929	25.225536
157.425802	5785.696011	25.230554
157.642068	5806.961090	25.235571
157.665226	5823.862160	25.240589
157.962092	5826.764717	25.245607
157.853201	5820.310837	25.250624
158.128427	5848.044379	25.255642
158.161723	5848.949231	25.260659
158.531117	5837.128895	25.265677
158.576782	5852.392957	25.270695
159.284348	5867.673675	25.275712
159.452870	5860.705367	25.280730
159.494364	5869.242327	25.285747
159.556042	5864.063598	25.290765
159.407847	5869.418019	25.295783
159.848766	5880.360239	25.300800
159.977975	5896.356326	25.305818
159.907367	5901.598710	25.310835
159.826087	5902.959572	25.315853
159.838264	5923.450529	25.320871
160.165384	5919.987258	25.325888
160.430287	5933.132169	25.330906
160.426471	5949.845676	25.335923
160.754816	5947.074433	25.340941
160.939766	5949.910451	25.345959
161.393983	5960.762327	25.350976
161.804997	5977.875115	25.355994
161.669891	5972.942284	25.361011
162.143869	5965.633650	25.366029
162.073686	5979.779787	25.371047
162.325680	6000.076077	25.376064
162.582273	6004.173704	25.381082
162.342286	6009.192887	25.386099
162.720763	6007.812005	25.391117
162.497876	6009.838898	25.396135
162.743920	6018.780010	25.401152
162.956638	6035.884673	25.406170
162.949501	6032.485268	25.411187
163.391245	6031.689304	25.416205
163.265265	6054.623344	25.421223
163.562303	6059.508924	25.426240
163.844910	6058.251769	25.431258
163.705164	6057.800741	25.436275
164.358203	6066.929008	25.441293
164.243859	6083.052943	25.446311
164.396484	6083.629379	25.451328
164.350454	6085.049798	25.456346
164.493595	6099.676631	25.461363
164.962665	6113.184090	25.466381
164.760811	6114.530241	25.471399
165.206244	6135.843743	25.476416
165.162545	6139.461797	25.481434
165.599923	6145.926854	25.486451
165.604132	6141.251316	25.491469
165.846063	6158.660000	25.496487
166.186765	6169.967074	25.501504
166.590519	6166.904545	25.506522
166.562386	6159.988285	25.511539
166.956135	6173.359397	25.516557
167.189807	6185.778845	25.521575
167.171864	6187.612028	25.526592
167.715458	6191.663073	25.531610
167.407106	6193.307190	25.536627
167.785055	6185.106289	25.541645
167.220570	6197.969487	25.546663
167.804331	6215.324906	25.551680
167.678015	6222.847869	25.556698
167.776510	6227.461528	25.561715
168.289301	6238.081045	25.566733
168.263792	6252.013709	25.571751
168.381266	6259.701171	25.576768
169.015505	6269.650921	25.581786
169.034286	6279.819710	25.586803
169.123950	6274.578732	25.591821
169.072668	6288.092775	25.596839
169.501850	6293.622858	25.601856
169.801742	6304.706021	25.606874
169.622061	6308.734054	25.611891
169.870856	6328.483954	25.616909
169.922131	6337.164461	25.621927
169.536907	6334.640208	25.626944
170.240280	6351.890961	25.631962
170.806616	6371.791637	25.636979
170.918069	6380.646512	25.641997
170.840180	6414.101876	25.647015
170.947029	6413.063534	25.652032
171.077586	6418.118492	25.657050
170.950549	6436.279129	25.662067
171.527844	6435.124467	25.667085
171.561560	6456.722220	25.672103
171.330070	6470.174838	25.677120
171.988255	6473.462786	25.682138
171.918149	6494.171271	25.687156
172.341582	6490.599819	25.692173
172.607333	6520.951584	25.697191
172.704303	6524.696907	25.702208
173.091498	6527.333442	25.707226
173.286814	6550.771132	25.712244
173.892827	6539.219900	25.717261
173.870065	6546.762135	25.722279
174.089656	6538.197375	25.727296
174.639953	6536.583295	25.732314
174.398544	6537.364250	25.737332
174.488566	6540.816179	25.742349
174.886205	6566.149192	25.747367
174.730323	6570.715987	25.752384
175.066525	6568.178819	25.757402
175.220666	6573.475649	25.762420
174.956172	6564.668745	25.767437
174.879736	6582.234459	25.772455
175.132321	6593.708397	25.777472
175.220690	6599.346091	25.782490
175.332169	6607.848263	25.787508
175.569144	6625.785950	25.792525
175.812695	6643.309888	25.797543
176.004459	6664.178520	25.802560
176.514627	6671.809177	25.807578
175.962993	6683.935848	25.812596
176.600953	6690.523142	25.817613
176.626107	6694.220517	25.822631
177.130121	6715.634600	25.827648
177.594131	6717.767034	25.832666
177.527425	6720.906245	25.837684
177.749263	6715.628318	25.842701
178.350843	6745.197319	25.847719
178.453964	6745.675638	25.852736
178.752260	6742.649326	25.857754
178.651542	6740.342622	25.862772
178.994667	6727.647037	25.867789
178.898626	6749.766736	25.872807
178.659112	6765.493063	25.877824
179.333833	6767.010253	25.882842
179.315003	6786.101647	25.887860
179.770504	6792.541139	25.892877
179.951904	6810.337794	25.897895
179.435212	6807.385481	25.902912
179.640120	6808.344729	25.907930
179.800156	6840.687442	25.912948
180.333567	6858.003063	25.917965
180.402095	6861.238882	25.922983
180.198659	6870.683184	25.928000
180.886741	6882.842238	25.933018
180.919073	6903.677673	25.938036
181.303406	6911.316637	25.943053
181.673752	6925.187643	25.948071
181.652875	6925.735285	25.953088
182.318883	6929.648162	25.958106
182.123765	6937.627026	25.963124
182.440333	6952.447308	25.968141
182.728700	6964.477148	25.973159
182.829969	6957.896718	25.978176
183.076019	6957.964728	25.983194
182.982093	6979.422834	25.988212
183.341991	6983.983287	25.993229
183.231337	6994.180223	25.998247
183.658307	7002.483205	26.003264
183.927406	7007.101196	26.008282
183.494587	7023.160573	26.013300
183.761499	7029.819555	26.018317
183.879228	7046.369229	26.023335
183.970312	7059.680055	26.028352
184.340218	7061.812334	26.033370
184.316989	7092.661869	26.038388
184.578215	7099.978666	26.043405
185.119738	7110.759423	26.048423
184.749470	7131.040272	26.053440
185.253865	7143.640210	26.058458
185.596625	7163.033032	26.063476
185.719394	7172.903260	26.068493
185.564169	7174.548166	26.073511
185.822707	7207.906310	26.078528
186.031775	7213.399055	26.083546
186.475745	7225.243504	26.088564
186.883278	7234.995051	26.093581
187.170488	7240.195299	26.098599
187.118140	7247.358412	26.103616
187.592142	7256.360228	26.108634
187.683040	7260.724204	26.113652
188.271517	7252.902242	26.118669
188.594635	7240.945952	26.123687
188.761732	7238.409841	26.128704
188.903155	7245.488169	26.133722
188.865715	7246.935626	26.138740
189.095345	7236.877918	26.143757
189.228614	7252.172181	26.148775
189.345265	7270.998411	26.153792
189.246981	7276.771149	26.158810
189.748482	7282.636177	26.163828
189.829946	7278.057800	26.168845
190.100585	7282.586621	26.173863
189.994531	7300.451012	26.178880
190.460337	7302.145329	26.183898
190.658452	7314.056457	26.188916
190.517777	7312.748641	26.193933
190.369496	7323.922324	26.198951
190.424013	7347.756209	26.203968
190.688446	7359.144476	26.208986
190.741508	7379.135172	26.214004
190.942713	7397.186761	26.219021
191.639107	7399.688087	26.224039
191.544567	7430.984032	26.229056
192.557365	7427.467006	26.234074
192.399585	7432.655779	26.239092
192.458934	7432.616022	26.244109
192.836607	7449.750889	26.249127
192.675300	7459.645390	26.254144
193.002027	7469.611273	26.259162
192.879310	7486.933606	26.264180
193.332921	7491.519680	26.269197
194.098463	7481.586714	26.274215
193.571372	7513.422126	26.279232
193.984651	7503.672577	26.284250
194.421454	7535.321211	26.289268
194.324207	7544.295497	26.294285
194.902230	7545.981540	26.299303
194.352977	7564.913415	26.304320
194.736136	7568.330528	26.309338
194.877958	7590.729509	26.314356
195.149359	7607.488301	26.319373
195.455308	7610.741755	26.324391
195.407773	7643.081026	26.329408
196.024951	7647.844113	26.334426
196.314364	7665.966499	26.339444
196.366235	7676.941963	26.344461
196.950021	7678.185218	26.349479
196.489331	7695.991294	26.354496
196.724385	7707.020000	26.359514
197.063514	7712.533175	26.364532
197.046735	7737.111121	26.369549
197.326534	7741.151813	26.374567
197.615230	7752.086626	26.379584
198.033125	7757.960921	26.384602
198.039999	7769.623598	26.389620
198.213897	7790.862127	26.394637
198.409498	7804.368182	26.399655
198.316872	7815.568459	26.404672
198.546301	7820.160952	26.409690
199.213348	7844.892300	26.414708
199.200792	7859.251921	26.419725
199.475678	7867.238660	26.424743
199.656398	7880.372331	26.429760
200.318982	7890.860318	26.434778
200.363744	7897.646949	26.439796
200.075548	7898.582982	26.444813
200.917792	7884.227973	26.449831
200.790026	7899.004414	26.454848
200.882968	7906.650264	26.459866
201.728509	7913.410926	26.464884
201.533744	7922.731552	26.469901
201.680433	7919.938002	26.474919
201.322975	7937.626475	26.479936
201.764061	7931.937800	26.484954
201.720922	7950.292671	26.489972
201.775496	7967.680753	26.494989
201.978820	7961.850983	26.500007
202.174696	7989.910946	26.505024
202.237310	8005.623241	26.510042
202.434423	8032.764698	26.515060
202.726039	8055.526316	26.520077
203.264089	8068.478234	26.525095
203.086762	8102.311972	26.530112
203.799588	8104.191619	26.535130
204.129786	8121.348449	26.540148
204.231539	8130.291762	26.545165
204.669708	8128.397543	26.550183
204.618572	8145.496895	26.555200
204.977570	8158.816366	26.560218
205.457216	8160.937757	26.565236
205.462819	8183.758628	26.570253
205.828565	8193.225460	26.575271
205.878510	8192.796586	26.580288
205.988316	8213.100317	26.585306
205.605074	8219.857770	26.590324
206.208079	8230.555889	26.595341
206.421134	8243.100876	26.600359
206.850575	8262.398813	26.605376
206.965468	8289.004519	26.610394
207.053922	8291.993170	26.615412
207.389988	8307.911056	26.620429
207.614795	8314.432613	26.625447
207.551882	8329.317674	26.630464
207.887638	8336.155658	26.635482
208.189958	8351.629418	26.640500
208.194594	8376.871955	26.645517
209.005020	8376.404072	26.650535
209.170405	8392.731465	26.655552
209.567692	8411.729290	26.660570
209.909282	8402.728277	26.665588
209.918337	8408.541190	26.670605
210.338862	8411.434829	26.675623
210.454652	8401.662994	26.680640
210.439223	8403.183322	26.685658
210.956008	8415.281288	26.690676
210.784652	8426.685615	26.695693
210.916951	8421.510135	26.700711
211.325023	8434.998166	26.705728
210.988107	8467.698051	26.710746
211.250777	8462.068597	26.715764
211.324249	8494.447897	26.720781
211.530489	8484.218406	26.725799
211.908629	8505.809313	26.730816
212.075679	8522.484709	26.735834
212.316987	8540.946072	26.740852
212.169994	8562.237078	26.745869
212.747743	8577.808907	26.750887
212.735362	8603.045950	26.755904
213.149303	8606.056499	26.760922
213.500049	8619.491146	26.765940
212.981443	8633.285255	26.770957
213.523047	8654.594155	26.775975
213.554895	8669.172443	26.780992
214.003008	8677.401929	26.786010
214.684776	8691.069443	26.791028
214.827885	8698.812933	26.796045
215.134184	8707.640860	26.801063
215.177942	8724.232078	26.806080
215.558854	8723.807584	26.811098
216.166310	8723.359839	26.816116
216.375626	8737.451235	26.821133
216.686409	8735.988368	26.826151
216.715748	8740.042343	26.831168
216.631578	8737.460078	26.836186
216.998073	8735.323216	26.841204
216.837493	8760.956774	26.846221
217.189526	8777.548314	26.851239
217.405496	8779.967772	26.856256
217.142488	8800.961621	26.861274
217.715644	8802.504468	26.866292
217.915574	8830.184804	26.871309
218.023161	8834.759916	26.876327
218.145929	8849.128793	26.881344
218.327366	8866.303920	26.886362
218.802412	8890.420373	26.891380
218.622408	8901.223109	26.896397
218.855681	8914.046487	26.901415
219.493123	8924.858329	26.906432
219.260055	8945.059746	26.911450
219.754297	8964.929927	26.916468
220.365285	8969.343928	26.921485
220.427716	8992.033694	26.926503
220.755489	8989.992991	26.931520
221.099216	9013.768996	26.936538
221.192953	9022.777151	26.941556
221.118095	9034.102167	26.946573
221.594233	9037.472734	26.951591
222.054629	9041.453205	26.956608
221.876802	9055.321343	26.961626
222.271437	9068.515178	26.966644
222.254435	9080.695543	26.971661
222.991252	9094.430718	26.976679
223.069614	9109.222276	26.981696
223.377650	9122.447793	26.986714
223.627120	9129.844669	26.991732
223.423648	9150.725955	26.996749
223.907047	9156.159876	27.001767
224.294075	9170.698059	27.006784
224.051890	9185.916800	27.011802
224.273692	9190.021011	27.016820
224.635295	9201.054271	27.021837
224.924327	9213.465381	27.026855
224.943920	9233.243390	27.031872
224.998604	9241.882393	27.036890
225.452522	9257.922760	27.041908
225.218887	9281.198271	27.046925
225.724450	9299.865770	27.051943
225.925917	9309.630592	27.056960
225.953805	9340.402796	27.061978
226.378945	9353.561896	27.066996
226.458680	9368.822936	27.072013
226.735153	9395.175366	27.077031
227.069299	9405.786371	27.082048
227.127600	9425.822102	27.087066
227.617022	9425.650634	27.092084
227.957408	9464.701382	27.097101
227.968402	9471.717972	27.102119
228.216739	9480.841843	27.107136
228.357668	9500.503249	27.112154
228.846977	9509.741714	27.117172
229.001654	9530.544633	27.122189
229.170151	9539.643131	27.127207
229.430692	9555.433749	27.132224
229.408816	9569.585348	27.137242
229.918656	9585.931103	27.142260
230.223823	9614.988085	27.147277
230.435384	9625.070455	27.152295
230.822634	9631.017471	27.157312
230.424890	9646.604217	27.162330
230.883578	9655.122344	27.167348
231.020744	9677.942527	27.172365
231.590135	9688.449475	27.177383
231.928830	9706.194251	27.182400
231.647899	9727.880741	27.187418
232.266381	9730.242510	27.192436
232.643321	9748.634030	27.197453
232.944551	9762.010870	27.202471
233.384510	9768.666052	27.207488
233.482799	9791.484943	27.212506
233.545753	9791.101141	27.217524
233.959008	9803.192856	27.222541
234.296777	9817.255323	27.227559
234.345821	9803.875662	27.232576
234.422033	9838.492789	27.237594
235.022754	9836.575459	27.242612
235.172164	9849.129080	27.247629
234.890061	9867.169592	27.252647
235.285734	9877.884967	27.257664
235.396206	9911.223632	27.262682
235.989957	9906.498421	27.267700
235.963440	9927.999784	27.272717
236.447505	9936.939243	27.277735
236.787148	9945.941166	27.282752
236.353591	9973.098755	27.287770
236.993089	9986.953189	27.292788
237.098921	10010.127987	27.297805
237.148608	10026.983470	27.302823
237.859929	10035.191449	27.307840
238.058025	10054.545543	27.312858
238.637596	10071.320619	27.317876
238.451638	10080.286568	27.322893
238.406618	10097.977803	27.327911
239.233768	10108.383365	27.332928
239.069228	10125.338940	27.337946
239.263201	10141.708306	27.342964
239.622054	10159.825219	27.347981
239.793712	10189.625296	27.352999
240.396020	10188.200789	27.358016
240.054523	10208.966830	27.363034
240.735996	10217.836809	27.368052
240.894077	10246.238635	27.373069
241.205849	10254.493832	27.378087
241.564925	10270.369711	27.383104
241.636429	10289.834807	27.388122
241.860578	10308.573616	27.393140
242.194124	10315.046522	27.398157
242.153892	10337.902471	27.403175
242.843849	10344.440181	27.408192
242.667512	10351.879617	27.413210
243.483203	10361.528640	27.418228
243.902220	10380.852145	27.423245
243.621786	10388.698731	27.428263
243.876600	10389.639719	27.433280
243.999337	10408.545860	27.438298
244.210661	10419.971098	27.443316
244.258696	10442.834670	27.448333
244.722910	10458.643737	27.453351
244.945282	10461.928924	27.458368
244.814210	10482.939418	27.463386
245.405072	10499.204192	27.468404
245.759199	10499.663217	27.473421
245.869704	10514.176629	27.478439
246.055655	10529.338516	27.483456
246.057929	10550.842260	27.488474
246.371235	10565.705851	27.493492
246.641364	10575.611355	27.498509
246.693713	10596.399482	27.503527
247.157704	10600.455382	27.508544
247.068236	10635.812164	27.513562
247.570955	10650.932073	27.518580
247.962271	10667.341061	27.523597
248.070608	10693.102655	27.528615
248.394704	10701.496271	27.533632
248.545172	10726.795632	27.538650
249.057667	10746.538194	27.543668
249.383232	10755.572837	27.548685
249.366724	10780.696626	27.553703
250.096840	10784.711757	27.558720
250.219534	10800.188429	27.563738
250.414886	10818.947562	27.568756
250.585955	10835.649135	27.573773
250.760487	10854.427504	27.578791
250.989334	10874.028021	27.583808
251.086878	10890.670111	27.588826
251.390654	10909.479185	27.593844
251.666330	10921.501523	27.598861
251.966189	10953.252064	27.603879
252.316483	10955.401516	27.608896
252.470491	10972.477880	27.613914
252.935290	10987.756414	27.618932
253.104921	11009.187433	27.623949
253.051217	11033.025806	27.628967
253.624955	11039.932781	27.633984
253.958002	11074.587350	27.639002
254.176521	11084.685250	27.644020
254.716229	11096.025995	27.649037
254.678149	11113.706962	27.654055
255.107561	11129.427122	27.659072
255.232445	11147.323053	27.664090
255.466278	11158.742736	27.669108
256.051396	11178.356455	27.674125
255.866545	11197.080370	27.679143
256.197210	11212.741298	27.684160
256.775928	11233.137627	27.689178
256.678256	11257.351494	27.694196
256.898100	11272.772394	27.699213
257.072901	11285.103154	27.704231
257.588121	11290.248950	27.709248
257.695472	11318.471987	27.714266
258.164298	11330.856618	27.719284
258.518279	11349.732756	27.724301
258.705948	11354.989409	27.729319
258.935236	11374.896130	27.734336
259.570255	11372.106387	27.739354
259.519371	11398.040373	27.744372
260.039141	11412.227010	27.749389
259.892888	11421.189508	27.754407
260.405189	11428.861514	27.759424
260.232371	11448.136768	27.764442
260.372833	11479.379769	27.769460
260.688588	11490.894083	27.774477
261.187923	11511.207770	27.779495
261.629657	11507.011408	27.784512
261.770813	11521.281176	27.789530
261.983988	11545.863234	27.794548
262.356985	11552.501868	27.799565
262.376622	11566.173324	27.804583
262.809948	11573.765487	27.809600
262.992959	11599.464204	27.814618
262.928299	11609.324032	27.819636
263.593222	11624.308561	27.824653
263.880828	11642.493283	27.829671
264.168446	11648.876632	27.834688
264.316737	11668.583603	27.839706
264.286592	11674.876078	27.844724
264.887386	11687.347902	27.849741
264.829229	11711.240799	27.854759
264.985596	11729.859329	27.859776
264.990829	11742.424073	27.864794
265.709862	11765.887707	27.869812
266.344335	11783.711188	27.874829
266.252351	11798.980854	27.879847
266.452043	11813.743838	27.884864
266.933904	11829.667944	27.889882
266.946211	11860.497981	27.894900
267.748354	11871.433524	27.899917
267.870481	11889.383521	27.904935
268.079681	11892.291450	27.909952
267.977747	11914.991241	27.914970
268.243804	11936.219277	27.919988
268.546244	11949.459091	27.925005
268.684160	11979.476053	27.930023
269.211930	12000.697964	27.935040
269.557338	12016.357242	27.940058
269.473058	12030.781304	27.945076
269.825256	12056.856957	27.950093
269.924242	12077.384037	27.955111
270.029629	12095.539502	27.960128
270.336352	12121.086258	27.965146
270.669077	12152.782531	27.970164
271.102493	12183.203269	27.975181
271.720752	12200.466590	27.980199
272.110166	12212.204029	27.985216
272.211215	12243.622833	27.990234
272.222340	12266.053119	27.995252
272.679515	12279.911307	28.000269
273.193127	12298.079918	28.005287
273.800179	12312.268690	28.010304
274.113170	12327.692547	28.015322
274.299754	12339.080697	28.020340
274.868949	12348.845714	28.025357
274.627891	12363.838798	28.030375
275.098838	12383.914047	28.035392
275.139987	12399.711416	28.040410
275.152173	12410.025442	28.045428
275.870213	12431.878281	28.050445
275.783720	12459.205680	28.055463
275.599908	12468.997479	28.060480
276.037720	12493.736107	28.065498
276.317244	12528.661068	28.070516
277.075336	12526.147034	28.075533
277.325665	12557.851413	28.080551
277.386182	12567.237342	28.085568
277.745878	12588.987297	28.090586
278.198037	12605.055743	28.095604
278.322724	12621.688836	28.100621
278.873613	12640.736439	28.105639
279.467224	12653.026632	28.110656
279.898651	12660.381692	28.115674
279.890065	12682.739391	28.120692
280.428561	12684.260791	28.125709
280.725915	12693.138102	28.130727
280.872281	12713.557319	28.135744
281.287290	12710.756430	28.140762
281.177703	12725.929822	28.145780
281.336704	12728.159969	28.150797
281.663274	12749.469683	28.155815
281.782741	12756.496575	28.160832
282.126589	12768.191526	28.165850
282.191660	12790.748353	28.170868
282.518820	12801.292649	28.175885
282.730458	12810.091217	28.180903
282.675057	12832.987880	28.185920
282.873192	12867.342421	28.190938
282.903880	12877.333815	28.195956
283.431651	12911.685992	28.200973
283.613805	12940.313930	28.205991
284.187910	12964.348467	28.211008
284.594935	12989.264699	28.216026
284.508709	13017.456508	28.221044
284.590157	13045.779816	28.226061
284.762920	13066.979844	28.231079
285.294473	13096.565124	28.236096
285.506380	13115.155592	28.241114
285.886120	13142.240089	28.246132
286.346873	13166.982264	28.251149
286.543302	13185.772341	28.256167
286.953359	13219.164491	28.261184
287.491586	13240.242914	28.266202
287.769404	13262.177487	28.271220
288.157992	13286.693824	28.276237
288.446264	13311.582898	28.281255
288.640246	13334.404401	28.286272
289.289423	13352.705446	28.291290
289.047923	13377.255104	28.296308
289.391876	13392.637834	28.301325
289.932271	13414.267652	28.306343
290.116268	13434.700471	28.311360
290.608484	13462.119900	28.316378
290.639753	13482.702499	28.321396
291.028258	13504.488323	28.326413
291.184085	13529.062390	28.331431
291.627150	13546.863508	28.336448
292.083842	13560.264321	28.341466
292.149673	13588.367393	28.346484
292.694615	13611.084032	28.351501
293.161961	13616.947608	28.356519
293.448771	13630.370241	28.361536
293.707717	13651.927113	28.366554
293.937206	13667.467686	28.371572
294.075487	13683.908952	28.376589
294.386083	13696.016630	28.381607
294.681080	13734.625902	28.386624
294.745238	13738.505986	28.391642
294.982595	13765.381827	28.396660
295.597912	13788.517289	28.401677
295.713760	13807.414374	28.406695
295.605890	13836.537768	28.411712
296.041141	13869.700177	28.416730
296.364422	13902.731447	28.421748
296.660094	13916.431776	28.426765
297.231504	13942.712211	28.431783
296.989937	13979.133614	28.436800
297.794847	13995.343725	28.441818
298.078131	14021.129794	28.446836
298.330806	14042.324199	28.451853
298.632355	14078.663980	28.456871
298.938615	14097.990096	28.461888
299.422248	14131.449187	28.466906
299.325003	14144.789139	28.471924
299.794655	14163.116032	28.476941
300.291333	14179.361491	28.481959
300.281860	14188.091754	28.486976
300.939819	14213.546758	28.491994
301.272694	14223.136064	28.497012
301.705269	14244.450720	28.502029
301.822343	14260.224752	28.507047
301.948499	14277.845799	28.512064
302.645128	14290.594564	28.517082
302.539799	14313.630783	28.522100
302.771595	14328.244992	28.527117
303.371894	14348.376957	28.532135
303.334739	14382.801944	28.537152
303.800463	14391.808387	28.542170
303.737639	14419.253367	28.547188
303.864360	14437.615161	28.552205
304.289846	14462.035780	28.557223
304.532846	14498.860515	28.562240
305.104486	14505.085402	28.567258
305.483181	14549.434808	28.572276
305.719460	14570.961975	28.577293
306.102029	14587.144746	28.582311
305.919295	14623.606723	28.587328
306.623482	14645.316713	28.592346
306.833038	14676.753035	28.597364
306.981566	14703.492238	28.602381
307.248427	14729.018964	28.607399
307.744877	14757.432713	28.612416
308.365229	14784.803267	28.617434
308.648622	14813.001738	28.622452
308.893065	14842.235774	28.627469
309.392331	14865.116157	28.632487
309.513418	14889.474237	28.637504
309.953907	14903.610073	28.642522
310.266753	14932.744719	28.647540
310.272432	14945.913880	28.652557
310.803465	14966.545020	28.657575
311.006809	14999.119244	28.662592
311.857747	15022.475997	28.667610
312.061730	15042.932751	28.672628
312.330550	15076.019527	28.677645
313.030372	15080.174724	28.682663
313.184869	15109.986714	28.687680
313.558405	15118.857501	28.692698
313.806687	15145.472207	28.697716
313.921481	15146.236472	28.702733
314.933218	15163.647564	28.707751
314.888568	15173.109108	28.712768
315.684360	15198.174112	28.717786
315.974994	15210.643962	28.722804
315.840090	15221.135366	28.727821
316.455667	15238.901963	28.732839
316.185674	15256.228616	28.737856
316.541354	15274.325013	28.742874
316.754222	15287.064653	28.747892
316.936835	15318.883321	28.752909
316.988438	15325.552183	28.757927
316.906496	15365.710588	28.762944
317.624547	15391.338749	28.767962
317.669289	15422.740696	28.772980
317.807841	15462.382237	28.777997
318.638525	15479.844067	28.783015
318.886220	15516.600981	28.788032
319.054925	15543.372898	28.793050
319.280886	15567.501904	28.798068
319.366070	15598.799796	28.803085
319.985809	15631.627997	28.808103
320.353083	15669.763418	28.813120
320.412365	15689.332377	28.818138
321.086732	15708.851756	28.823156
321.409725	15745.585713	28.828173
322.502364	15751.682462	28.833191
322.649985	15777.269927	28.838208
322.789509	15783.905540	28.843226
322.804079	15802.720803	28.848244
323.336504	15823.218837	28.853261
323.928079	15842.988458	28.858279
323.833614	15864.521538	28.863296
324.127640	15887.486120	28.868314
324.260790	15898.043995	28.873332
324.202659	15924.105393	28.878349
324.984510	15944.876006	28.883367
325.080799	15982.612480	28.888384
325.315520	16001.128404	28.893402
325.899438	16040.157187	28.898420
326.301570	16058.954425	28.903437
327.162252	16075.638101	28.908455
327.363037	16103.839839	28.913472
327.885497	16125.121620	28.918490
328.174756	16147.036127	28.923508
328.202110	16168.149162	28.928525
328.759390	16182.558386	28.933543
328.929709	16202.122223	28.938560
329.089063	16224.918823	28.943578
329.549528	16247.106208	28.948596
329.430978	16286.328852	28.953613
330.119405	16292.888178	28.958631
330.189435	16337.279243	28.963648
330.461503	16366.449974	28.968666
330.943331	16385.587463	28.973684
330.883706	16426.972543	28.978701
331.445932	16440.591561	28.983719
331.920650	16466.684000	28.988736
332.539250	16490.479993	28.993754
332.804416	16521.830295	28.998772
333.154603	16548.305937	29.003789
333.792583	16573.971249	29.008807
333.903265	16594.051332	29.013824
333.867752	16613.239877	29.018842
334.729149	16641.965424	29.023860
334.820677	16672.906542	29.028877
334.957753	16693.144725	29.033895
335.233388	16719.153822	29.038912
335.520593	16748.344797	29.043930
336.085593	16779.772148	29.048948
336.075858	16806.741097	29.053965
336.597497	16826.443079	29.058983
336.982901	16862.023388	29.064000
337.084702	16890.465062	29.069018
337.655523	16931.881235	29.074036
337.661618	16962.904785	29.079053
338.316554	16989.354437	29.084071
338.361686	17015.398929	29.089088
338.608391	17039.049104	29.094106
339.252656	17077.211390	29.099124
339.803491	17103.356889	29.104141
340.155623	17140.929243	29.109159
340.168114	17168.635903	29.114176
340.534502	17203.408373	29.119194
341.029663	17233.618727	29.124212
341.098248	17263.959501	29.129229
341.713964	17291.863036	29.134247
342.561029	17304.132231	29.139264
342.945630	17325.020661	29.144282
343.638149	17345.223055	29.149300
343.845950	17364.422717	29.154317
344.103897	17375.832550	29.159335
344.309249	17385.996445	29.164352
344.541979	17424.145559	29.169370
345.124745	17430.615622	29.174388
345.378279	17451.902572	29.179405
345.416717	17468.974120	29.184423
345.223488	17486.545777	29.189440
345.515213	17527.716386	29.194458
346.469061	17536.591924	29.199476
346.387700	17568.844726	29.204493
346.446058	17586.324490	29.209511
346.679573	17628.069242	29.214528
346.696276	17657.361682	29.219546
347.375746	17694.173508	29.224564
347.745016	17732.891856	29.229581
347.873087	17772.846484	29.234599
348.228236	17817.347328	29.239616
348.792883	17853.204378	29.244634
349.086847	17888.125810	29.249652
349.408328	17919.595568	29.254669
349.964726	17944.376475	29.259687
350.389353	17991.958870	29.264704
350.489689	18020.087487	29.269722
351.356235	18055.170035	29.274740
351.516098	18089.660090	29.279757
351.964164	18116.076374	29.284775
352.594466	18135.965312	29.289792
352.358238	18163.546070	29.294810
353.077234	18188.945169	29.299828
353.375048	18230.155929	29.304845
353.519393	18262.349153	29.309863
354.532326	18300.319388	29.314880
354.872880	18316.290537	29.319898
355.891458	18341.577332	29.324916
355.835112	18368.425701	29.329933
356.233122	18386.255303	29.334951
356.581363	18404.288603	29.339968
356.547172	18424.656507	29.344986
357.098567	18443.353003	29.350004
357.354883	18489.134578	29.355021
357.605150	18493.413794	29.360039
357.932137	18541.105323	29.365056
357.902182	18572.580785	29.370074
358.337319	18602.999024	29.375092
358.475407	18649.142626	29.380109
359.138681	18668.508159	29.385127
359.564676	18704.497149	29.390144
359.894143	18731.230353	29.395162
360.353762	18763.121837	29.400180
360.190531	18798.633016	29.405197
360.745867	18832.411425	29.410215
361.445420	18865.340091	29.415232
361.589345	18901.368223	29.420250
362.411639	18931.571783	29.425268
362.421547	18959.374871	29.430285
363.352708	18986.206131	29.435303
363.737679	19006.294278	29.440320
364.096197	19034.276353	29.445338
364.855203	19053.311257	29.450356
365.656707	19062.775547	29.455373
365.652513	19063.186064	29.460391
365.901878	19092.753144	29.465408
366.014718	19116.931259	29.470426
366.329689	19130.591779	29.475444
366.919445	19165.154929	29.480461
366.964520	19185.247422	29.485479
367.309464	19215.960699	29.490496
367.675439	19235.524186	29.495514
367.859089	19253.442154	29.500532
367.821634	19289.269366	29.505549
368.156038	19310.778650	29.510567
368.713458	19330.606979	29.515584
368.944455	19363.153741	29.520602
369.169118	19384.265089	29.525620
369.644067	19415.917265	29.530637
369.901113	19444.055514	29.535655
370.334925	19479.081732	29.540672
370.386339	19516.341862	29.545690
371.098300	19544.558041	29.550708
371.321395	19583.984283	29.555725
371.633934	19605.169672	29.560743
372.353326	19637.751368	29.565760
372.608804	19675.602395	29.570778
372.650150	19698.161600	29.575796
373.171036	19747.552291	29.580813
373.451759	19787.311573	29.585831
374.292387	19813.096635	29.590848
374.315041	19844.217427	29.595866
374.751382	19875.749168	29.600884
375.151736	19909.542761	29.605901
375.415784	19926.765585	29.610919
375.918766	19970.792204	29.615936
376.380710	20011.983426	29.620954
376.795859	20050.773700	29.625972
377.243616	20084.143640	29.630989
377.749162	20112.818942	29.636007
378.313866	20133.137298	29.641024
378.682884	20171.396333	29.646042
378.997180	20202.053436	29.651060
379.537556	20228.005399	29.656077
379.571967	20256.930609	29.661095
380.022382	20289.791330	29.666112
380.178214	20318.326122	29.671130
380.499282	20361.039108	29.676148
381.057266	20378.166551	29.681165
381.638765	20407.157716	29.686183
382.006100	20432.681409	29.691200
382.439537	20461.954092	29.696218
382.755837	20494.049137	29.701236
383.020984	20528.113825	29.706253
383.278995	20566.297514	29.711271
383.869258	20599.871958	29.716288
384.230443	20626.434287	29.721306
384.732009	20656.712887	29.726324
385.009176	20695.519571	29.731341
385.269492	20734.997561	29.736359
385.601272	20767.234035	29.741376
385.965340	20798.040083	29.746394
386.457434	20835.667052	29.751412
386.835612	20874.739659	29.756429
387.081974	20906.041454	29.761447
387.817127	20933.337055	29.766464
388.072499	20968.201968	29.771482
388.448719	20997.817686	29.776500
388.840510	21025.195381	29.781517
388.943117	21063.631318	29.786535
389.758542	21098.722446	29.791552
389.582739	21139.537805	29.796570
390.428696	21157.378367	29.801588
390.896060	21191.697930	29.806605
391.420021	21229.514434	29.811623
391.806811	21253.964123	29.816640
392.003603	21286.118266	29.821658
392.402314	21318.325826	29.826676
392.859406	21353.875549	29.831693
392.936422	21391.566027	29.836711
393.718565	21417.511434	29.841728
393.894343	21446.766919	29.846746
394.409270	21473.423438	29.851764
394.527982	21502.445655	29.856781
394.730061	21543.169619	29.861799
395.531428	21565.181698	29.866816
395.471027	21600.073286	29.871834
396.028830	21632.855844	29.876852
396.588405	21647.975772	29.881869
396.785563	21692.016452	29.886887
397.495992	21717.635206	29.891904
397.585178	21765.578617	29.896922
397.790103	21782.873032	29.901940
398.450169	21825.836461	29.906957
398.690378	21871.590563	29.911975
399.398666	21907.479925	29.916992
399.630960	21940.365729	29.922010
399.953267	21983.178820	29.927028
400.302854	22003.145566	29.932045
400.580388	22046.221623	29.937063
401.009066	22081.509557	29.942080
401.104904	22129.579034	29.947098
401.348469	22166.430201	29.952116
401.975419	22209.548284	29.957133
402.492370	22268.244454	29.962151
403.017420	22290.126549	29.967168
403.324940	22334.316226	29.972186
403.854349	22382.111417	29.977204
404.272708	22424.441499	29.982221
404.489005	22471.695846	29.987239
405.370901	22503.102178	29.992256
405.617645	22549.172373	29.997274
405.919775	22588.786561	30.002292
406.412155	22623.210555	30.007309
406.557834	22676.416450	30.012327
407.500253	22697.744517	30.017344
407.654670	22747.914095	30.022362
407.975115	22782.417270	30.027380
408.521324	22817.215902	30.032397
408.589251	22866.780483	30.037415
409.236495	22902.466046	30.042432
409.730304	22953.546686	30.047450
410.148772	22996.056352	30.052468
410.556779	23019.669452	30.057485
410.732064	23077.754779	30.062503
411.244880	23114.391678	30.067520
411.646151	23154.591545	30.072538
411.852715	23192.701402	30.077556
412.056534	23231.146064	30.082573
412.741799	23288.304324	30.087591
413.109725	23322.608398	30.092608
413.628358	23372.757508	30.097626
413.950514	23419.989137	30.102644
414.935679	23459.183497	30.107661
414.988674	23502.686664	30.112679
415.617918	23544.008710	30.117696
416.102499	23586.471098	30.122714
416.543194	23630.077687	30.127732
416.930162	23662.323206	30.132749
417.374637	23698.930089	30.137767
417.654914	23738.219458	30.142784
418.085947	23777.343683	30.147802
418.683753	23823.282097	30.152820
419.046482	23859.106556	30.157837
418.999479	23912.901617	30.162855
419.506942	23950.676501	30.167872
420.326490	23980.720925	30.172890
420.615742	24015.345296	30.177908
421.184899	24042.859434	30.182925
421.170081	24086.143510	30.187943
421.612327	24114.352023	30.192960
422.376594	24148.470886	30.197978
422.889358	24191.940872	30.202996
423.118565	24229.241991	30.208013
423.367036	24271.467577	30.213031
423.569968	24310.643325	30.218048
424.041353	24350.503314	30.223066
424.389550	24398.483938	30.228084
424.973828	24442.321191	30.233101
424.917068	24488.580826	30.238119
425.688460	24521.813079	30.243136
425.939498	24576.734181	30.248154
426.509019	24625.724338	30.253172
426.994607	24655.874008	30.258189
427.007165	24700.082314	30.263207
427.629767	24741.340571	30.268224
428.057413	24796.800882	30.273242
427.968629	24853.961399	30.278260
428.479999	24901.802952	30.283277
429.247234	24957.620835	30.288295
430.067267	25003.905765	30.293312
430.443736	25056.893352	30.298330
430.713663	25112.219898	30.303348
431.255270	25154.433944	30.308365
431.610615	25201.493161	30.313383
432.116258	25229.975321	30.318400
432.529400	25285.431733	30.323418
432.584978	25340.338696	30.328436
433.333040	25385.704593	30.333453
433.817740	25447.201948	30.338471
434.178681	25480.052871	30.343488
434.775967	25528.150070	30.348506
435.191493	25591.802430	30.353524
435.660921	25632.769605	30.358541
435.667261	25692.140709	30.363559
436.178324	25744.313412	30.368576
437.198322	25785.782946	30.373594
436.989050	25850.141872	30.378612
437.899212	25889.374738	30.383629
438.637028	25935.319382	30.388647
439.026320	25963.810948	30.393664
439.812256	26011.460447	30.398682
440.283873	26040.843731	30.403700
441.137594	26077.304551	30.408717
441.299862	26119.146816	30.413735
441.444418	26164.231260	30.418752
442.097851	26193.938022	30.423770
442.402060	26243.269970	30.428788
443.155112	26279.552302	30.433805
443.602132	26319.436689	30.438823
443.725197	26363.288830	30.443840
444.302591	26403.959310	30.448858
444.502118	26438.456758	30.453876
445.090908	26475.892633	30.458893
445.500403	26523.539504	30.463911
445.609157	26564.527484	30.468928
445.971952	26600.669945	30.473946
446.113846	26657.766838	30.478964
446.849479	26701.338876	30.483981
447.205078	26747.433996	30.488999
447.715143	26807.873848	30.494016
448.117581	26840.395655	30.499034
448.309378	26900.960950	30.504052
449.190005	26939.450422	30.509069
449.410544	26997.920120	30.514087
449.961956	27044.191865	30.519104
450.670725	27085.129288	30.524122
451.142984	27117.097570	30.529140
451.615596	27151.721668	30.534157
452.408298	27185.072296	30.539175
452.667215	27223.346527	30.544192
453.016076	27254.799237	30.549210
453.144415	27305.024379	30.554228
453.813287	27333.096690	30.559245
453.913702	27387.048648	30.564263
454.288026	27427.436520	30.569280
454.711485	27463.529771	30.574298
455.182456	27520.745499	30.579316
455.693836	27572.857473	30.584333
456.179246	27610.114179	30.589351
456.456388	27658.410599	30.594368
456.975180	27698.980273	30.599386
457.107756	27759.053683	30.604404
458.120898	27796.450731	30.609421
458.394755	27851.006349	30.614439
458.599387	27900.438355	30.619456
459.211482	27957.812019	30.624474
459.195813	28023.437206	30.629492
459.364089	28076.298172	30.634509
460.155658	28143.632614	30.639527
460.474308	28203.348779	30.644544
461.426154	28256.484627	30.649562
461.474917	28318.554773	30.654580
462.251222	28367.578248	30.659597
462.799538	28438.064252	30.664615
463.374410	28483.623090	30.669632
464.172514	28537.580110	30.674650
464.513302	28593.423484	30.679668
465.018671	28638.748165	30.684685
465.589434	28688.951567	30.689703
465.805070	28738.627042	30.694720
466.423996	28783.144729	30.699738
466.823488	28841.572181	30.704756
467.809112	28886.638379	30.709773
468.733883	28923.465735	30.714791
469.111502	28975.818539	30.719808
469.663949	29007.556264	30.724826
470.075685	29052.865950	30.729844
470.808838	29080.599266	30.734861
471.171060	29118.340133	30.739879
471.441128	29156.033213	30.744896
471.741447	29196.364888	30.749914
471.877392	29257.736303	30.754932
472.278696	29288.247148	30.759949
473.038781	29336.099395	30.764967
472.857748	29399.709786	30.769984
473.586997	29448.365546	30.775002
473.767833	29505.503266	30.780020
474.330368	29546.218313	30.785037
475.055795	29597.805755	30.790055
474.835453	29667.076693	30.795072
475.571292	29715.968711	30.800090
475.871278	29779.778645	30.805108
476.223178	29830.627194	30.810125
478.022718	29881.227313	30.815143
478.172263	29931.570132	30.820160
479.036655	29970.996525	30.825178
479.661499	30021.298953	30.830196
480.046544	30063.082422	30.835213
480.730679	30086.702248	30.840231
481.294888	30126.512976	30.845248
481.929708	30159.800786	30.850266
482.168963	30190.951999	30.855284
482.276923	30244.990467	30.860301
482.270736	30274.567145	30.865319
482.060564	30312.790026	30.870336
482.763712	30356.092720	30.875354
482.999791	30415.337985	30.880372
483.377330	30475.522292	30.885389
484.379540	30524.640741	30.890407
484.608802	30591.030166	30.895424
484.987911	30640.870202	30.900442
485.099665	30703.834415	30.905460
485.835921	30755.357246	30.910477
486.633167	30816.533426	30.915495
486.855650	30875.022178	30.920512
487.260581	30929.120973	30.925530
487.906729	30991.209237	30.930548
488.274514	31039.402281	30.935565
488.905089	31100.215778	30.940583
489.476275	31160.121220	30.945600
490.082436	31209.455292	30.950618
490.174170	31271.664519	30.955636
490.795500	31327.839445	30.960653
491.486625	31385.911762	30.965671
491.862525	31459.776402	30.970688
492.717566	31501.208042	30.975706
493.318816	31555.929424	30.980724
494.041792	31604.671110	30.985741
494.761994	31647.093946	30.990759
495.227307	31704.942755	30.995776
495.816801	31747.990030	31.000794
496.591283	31795.575317	31.005812
496.392421	31843.747431	31.010829
497.309342	31884.273730	31.015847
497.395164	31951.941392	31.020864
497.954918	31989.826212	31.025882
498.106123	32039.761505	31.030900
498.643731	32106.739903	31.035917
499.487344	32161.236991	31.040935
499.479208	32220.402487	31.045952
500.176532	32282.537351	31.050970
500.476062	32327.981337	31.055988
500.927192	32394.908858	31.061005
501.518642	32447.624822	31.066023
501.607179	32522.027278	31.071040
502.308847	32588.122210	31.076058
502.656745	32654.222184	31.081076
502.916633	32716.200501	31.086093
503.917840	32779.949707	31.091111
504.515891	32839.746004	31.096128
505.241640	32899.038665	31.101146
506.002455	32957.038402	31.106164
506.132697	33020.888163	31.111181
507.063472	33070.814357	31.116199
507.752848	33133.562495	31.121216
508.177777	33184.402392	31.126234
508.902667	33231.147832	31.131252
508.969467	33292.245033	31.136269
509.987438	33334.480769	31.141287
510.118710	33391.355351	31.146304
510.860095	33445.179129	31.151322
511.316014	33504.420576	31.156340
512.037011	33536.353242	31.161357
512.526128	33586.767191	31.166375
512.772724	33647.381552	31.171392
513.170024	33689.547110	31.176410
513.742532	33744.081246	31.181428
514.183670	33802.764478	31.186445
515.072661	33845.735855	31.191463
515.401611	33906.940179	31.196480
515.874121	33951.750778	31.201498
516.755342	33999.971245	31.206516
516.639072	34054.714765	31.211533
517.673813	34092.352099	31.216551
517.882778	34151.781648	31.221568
517.970384	34201.459026	31.226586
518.474935	34249.571992	31.231604
519.035877	34299.969795	31.236621
519.705093	34346.932483	31.241639
520.147203	34403.374000	31.246656
520.529765	34469.175253	31.251674
521.077867	34514.795216	31.256692
521.417004	34565.050543	31.261709
522.142899	34633.815519	31.266727
522.466227	34686.336308	31.271744
522.751143	34742.189535	31.276762
523.475540	34803.344252	31.281780
523.912458	34861.447900	31.286797
524.433041	34919.913431	31.291815
524.855052	34991.197637	31.296832
525.328978	35064.373222	31.301850
526.526648	35110.285031	31.306868
527.070057	35177.403465	31.311885
527.497928	35228.974523	31.316903
528.021236	35288.273898	31.321920
528.603234	35353.398570	31.326938
529.071857	35417.242073	31.331956
529.570733	35467.151681	31.336973
530.271023	35522.452773	31.341991
530.341043	35592.090293	31.347008
530.546162	35662.321132	31.352026
531.482036	35715.273935	31.357044
531.340997	35793.338138	31.362061
531.974723	35863.211803	31.367079
532.402396	35940.466362	31.372096
533.039431	36013.628360	31.377114
533.999980	36073.243125	31.382132
534.417556	36145.706615	31.387149
535.370752	36202.438636	31.392167
536.077769	36274.545573	31.397184
536.420592	36346.387903	31.402202
537.268236	36400.199913	31.407220
537.649486	36469.653736	31.412237
538.397765	36516.268246	31.417255
538.833253	36589.368052	31.422272
539.031638	36638.077677	31.427290
539.894634	36703.107197	31.432308
540.459992	36773.576386	31.437325
541.187925	36827.109638	31.442343
541.787796	36892.031818	31.447360
542.165850	36944.493390	31.452378
542.944706	37002.399183	31.457396
543.188763	37072.206211	31.462413
543.917549	37132.124721	31.467431
544.470671	37191.485433	31.472448
544.904712	37241.281295	31.477466
545.588331	37303.445425	31.482484
546.003235	37369.002671	31.487501
546.538274	37419.719677	31.492519
546.876868	37486.681755	31.497536
547.658802	37548.574855	31.502554
548.486155	37588.238970	31.507572
548.957062	37656.375964	31.512589
549.409641	37706.340476	31.517607
549.965539	37770.938545	31.522624
550.212538	37837.424705	31.527642
550.916249	37895.983313	31.532660
551.288177	37956.007687	31.537677
552.137855	38020.741182	31.542695
552.758898	38062.905345	31.547712
552.991648	38127.059392	31.552730
553.639188	38174.707958	31.557748
553.812673	38236.290455	31.562765
554.443688	38295.102231	31.567783
555.115049	38355.005883	31.572800
555.391213	38409.543212	31.577818
556.124486	38467.697954	31.582836
556.427077	38541.225300	31.587853
556.819013	38594.566799	31.592871
557.393017	38671.177656	31.597888
557.939299	38724.705513	31.602906
558.932380	38790.784731	31.607924
559.128341	38862.197364	31.612941
559.338475	38927.131262	31.617959
560.541224	38994.145569	31.622976
560.791570	39071.225043	31.627994
561.470440	39133.355219	31.633012
561.979262	39202.022026	31.638029
562.206348	39261.222438	31.643047
563.249848	39328.488382	31.648064
563.836389	39410.074683	31.653082
564.517367	39465.520482	31.658100
564.852130	39548.405221	31.663117
565.309627	39617.795417	31.668135
565.585237	39692.667031	31.673152
566.292890	39764.667852	31.678170
567.275767	39822.678393	31.683188
567.516823	39898.058430	31.688205
568.178181	39978.312370	31.693223
569.126861	40036.941594	31.698240
569.272328	40123.616406	31.703258
570.207726	40183.712903	31.708276
570.690965	40265.181207	31.713293
571.261743	40331.926042	31.718311
572.064877	40393.320307	31.723328
573.052403	40453.118682	31.728346
574.018757	40508.466861	31.733364
574.807406	40571.887467	31.738381
575.623830	40618.438164	31.743399
576.272158	40662.964968	31.748416
576.592742	40717.274599	31.753434
577.237281	40765.953188	31.758452
577.463424	40826.459348	31.763469
578.022669	40879.764124	31.768487
578.711622	40945.083830	31.773504
579.088731	41002.790968	31.778522
579.595560	41049.838981	31.783540
579.942139	41111.045903	31.788557
580.659976	41174.739140	31.793575
581.352467	41239.822563	31.798592
581.523879	41298.540016	31.803610
582.216114	41354.763081	31.808628
582.761276	41415.070130	31.813645
583.172139	41477.179943	31.818663
583.786062	41547.874290	31.823680
584.402831	41610.910194	31.828698
585.058725	41682.804002	31.833716
585.319380	41746.887249	31.838733
586.091897	41811.062961	31.843751
586.689734	41880.618493	31.848768
586.992867	41956.618629	31.853786
587.568220	42019.877436	31.858804
588.342466	42091.822746	31.863821
588.765473	42161.086216	31.868839
589.687666	42231.157733	31.873856
589.953672	42306.773995	31.878874
590.577972	42376.787932	31.883892
591.467575	42435.617690	31.888909
592.373384	42483.465307	31.893927
593.053400	42533.702225	31.898944
593.763543	42592.871501	31.903962
594.414839	42643.549115	31.908980
595.096434	42695.238394	31.913997
595.226118	42761.676607	31.919015
595.859419	42815.852392	31.924032
595.923228	42873.910735	31.929050
596.338728	42934.954488	31.934068
596.887270	43009.049503	31.939085
597.076402	43091.055606	31.944103
598.093355	43152.947841	31.949120
598.252715	43228.364496	31.954138
598.843577	43311.435437	31.959156
599.153826	43389.460787	31.964173
600.128101	43460.664902	31.969191
600.773513	43535.459518	31.974208
601.066259	43621.340358	31.979226
602.161614	43687.998097	31.984244
602.980134	43757.606332	31.989261
603.327149	43838.825645	31.994279
604.061344	43908.224217	31.999296
604.714444	43973.311158	32.004314
605.646347	44059.138977	32.009332
606.245130	44134.562509	32.014349
606.454150	44201.936767	32.019367
607.367602	44275.840816	32.024384
608.164281	44352.252320	32.029402
608.831039	44414.067686	32.034420
609.068889	44490.909874	32.039437
609.367806	44562.362356	32.044455
610.268746	44641.684590	32.049472
610.724403	44725.731357	32.054490
611.648073	44796.639538	32.059508
612.248703	44881.591304	32.064525
612.783498	44963.040245	32.069543
613.073906	45033.034100	32.074560
613.808103	45120.695976	32.079578
614.399645	45203.630013	32.084596
615.171345	45284.112967	32.089613
615.514324	45364.313447	32.094631
616.623026	45438.515067	32.099648
617.438730	45521.606093	32.104666
618.191226	45599.769731	32.109684
619.010780	45659.325378	32.114701
619.536965	45729.759670	32.119719
620.278688	45798.087345	32.124736
620.767134	45866.337114	32.129754
621.354117	45929.250520	32.134772
622.115839	46011.657992	32.139789
622.352128	46074.942395	32.144807
623.650123	46145.544430	32.149824
623.663322	46220.302658	32.154842
624.026009	46280.728269	32.159860
625.269096	46354.743977	32.164877
625.287873	46430.787240	32.169895
626.044516	46507.195215	32.174912
626.568235	46580.127582	32.179930
627.220869	46664.106303	32.184948
627.711039	46738.557311	32.189965
628.354758	46832.380515	32.194983
628.811868	46900.588691	32.200000
629.620951	46984.874556	32.205018
629.905034	47056.844212	32.210036
630.687676	47135.555534	32.215053
631.222224	47228.495643	32.220071
631.845144	47305.974136	32.225088
632.159739	47399.873461	32.230106
633.278981	47469.622671	32.235124
634.020252	47537.622018	32.240141
634.557870	47616.672638	32.245159
635.477538	47678.223319	32.250176
635.919580	47746.310728	32.255194
636.474972	47830.683315	32.260212
637.144123	47904.389384	32.265229
637.461536	47973.287641	32.270247
638.357054	48053.102008	32.275264
638.709266	48133.126436	32.280282
639.436858	48215.666014	32.285300
640.760192	48290.077115	32.290317
640.936072	48372.471651	32.295335
641.459540	48440.118632	32.300352
642.068719	48518.848565	32.305370
642.515782	48595.960324	32.310388
643.157657	48688.526709	32.315405
643.997940	48770.674296	32.320423
644.682685	48835.807591	32.325440
645.411841	48915.384633	32.330458
646.105957	49006.235475	32.335476
646.866734	49086.597507	32.340493
646.951647	49184.402661	32.345511
647.729277	49267.011175	32.350528
648.170101	49349.612509	32.355546
648.776599	49438.512422	32.360564
649.700531	49525.181259	32.365581
650.477834	49619.002500	32.370599
651.176029	49700.359617	32.375616
651.779148	49780.829562	32.380634
652.484854	49870.289878	32.385652
653.399956	49950.576373	32.390669
654.002137	50045.732942	32.395687
654.932079	50125.897712	32.400704
655.656320	50210.603516	32.405722
656.149510	50278.710480	32.410740
656.943373	50362.180077	32.415757
657.373904	50442.381275	32.420775
657.896289	50523.890940	32.425792
658.442591	50611.789294	32.430810
659.141424	50697.502608	32.435828
659.789584	50788.003147	32.440845
660.317819	50878.062807	32.445863
660.953031	50968.872690	32.450880
661.650411	51065.427198	32.455898
662.138810	51149.765512	32.460916
663.241924	51233.907927	32.465933
663.910059	51330.250668	32.470951
664.744045	51413.655040	32.475968
665.344651	51501.210543	32.480986
665.758131	51595.313145	32.486004
666.561978	51670.597020	32.491021
667.049559	51758.434505	32.496039
667.816957	51860.060198	32.501056
669.057212	51930.769066	32.506074
669.764966	52014.218991	32.511092
670.505240	52090.866834	32.516109
671.082530	52171.319466	32.521127
671.842295	52249.897725	32.526144
672.500335	52332.858190	32.531162
673.071780	52423.615964	32.536180
674.093562	52497.799485	32.541197
674.038483	52579.128931	32.546215
674.591987	52661.318424	32.551232
675.722475	52747.070635	32.556250
676.205257	52830.731797	32.561268
676.962891	52909.224642	32.566285
677.117763	53002.934585	32.571303
677.853351	53070.774479	32.576320
678.566419	53149.749453	32.581338
679.427240	53246.104657	32.586356
680.165314	53315.303226	32.591373
680.695635	53399.603359	32.596391
681.019081	53477.873285	32.601408
681.739975	53550.442719	32.606426
682.209234	53653.826443	32.611444
683.224578	53719.657663	32.616461
683.499898	53815.133161	32.621479
684.215193	53902.431024	32.626496
685.428186	53995.326609	32.631514
685.807523	54085.687951	32.636532
687.031060	54162.788528	32.641549
687.349849	54254.045118	32.646567
688.009052	54338.062681	32.651584
689.087472	54429.889594	32.656602
689.563911	54506.306234	32.661620
690.378312	54597.248822	32.666637
691.295822	54669.448788	32.671655
692.051251	54766.568093	32.676672
692.991151	54854.357499	32.681690
693.239687	54938.552860	32.686708
694.161243	55021.733977	32.691725
694.654651	55102.004075	32.696743
695.346415	55185.596593	32.701760
696.400281	55265.048237	32.706778
696.283888	55354.808633	32.711796
697.582799	55437.910243	32.716813
697.828509	55525.602477	32.721831
698.562709	55619.968503	32.726848
699.331735	55712.831830	32.731866
699.972542	55811.870678	32.736884
700.859964	55898.927875	32.741901
701.456084	55988.080671	32.746919
701.803700	56085.532887	32.751936
702.275425	56185.441864	32.756954
702.749028	56289.375816	32.761972
703.879467	56386.700245	32.766989
704.584913	56496.416217	32.772007
705.216594	56581.692641	32.777024
706.264989	56685.186241	32.782042
706.657232	56796.800593	32.787060
707.318310	56895.835211	32.792077
708.022948	57000.094900	32.797095
708.960813	57094.794501	32.802112
709.805146	57186.698212	32.807130
710.758073	57296.598902	32.812148
711.596114	57378.091395	32.817165
712.134570	57467.968075	32.822183
712.733860	57569.474239	32.827200
713.514906	57664.518393	32.832218
713.873161	57773.047648	32.837236
714.856793	57868.084596	32.842253
715.684335	57966.477819	32.847271
716.217993	58068.597660	32.852288
716.846454	58150.526020	32.857306
717.857761	58250.931316	32.862324
718.814014	58348.685914	32.867341
719.023970	58450.848529	32.872359
720.169271	58548.996265	32.877376
720.620537	58648.219594	32.882394
721.157508	58747.264966	32.887412
722.027206	58835.020440	32.892429
722.526202	58936.834489	32.897447
723.309359	59042.014502	32.902464
724.530005	59137.049953	32.907482
724.850820	59235.274018	32.912500
725.867160	59328.296670	32.917517
726.573412	59420.985482	32.922535
727.149515	59503.256637	32.927552
728.023722	59581.358665	32.932570
728.938975	59672.977750	32.937588
729.469415	59756.571920	32.942605
729.932036	59841.991323	32.947623
730.564546	59926.018024	32.952640
731.516814	60027.219278	32.957658
732.028753	60122.730324	32.962676
732.918229	60204.731418	32.967693
733.795097	60296.738859	32.972711
734.366970	60397.600336	32.977728
735.231215	60489.901448	32.982746
735.343392	60589.007090	32.987764
736.124962	60701.008682	32.992781
737.077766	60798.737871	32.997799
737.949518	60886.236537	33.002816
738.802007	60984.880602	33.007834
739.488751	61085.979342	33.012852
740.069407	61182.672188	33.017869
741.232909	61283.516229	33.022887
741.764422	61387.435510	33.027904
742.496563	61484.939016	33.032922
742.821610	61592.950868	33.037940
743.770114	61683.682473	33.042957
745.130952	61783.301930	33.047975
745.764937	61888.034782	33.052992
746.636635	61994.220471	33.058010
747.218584	62102.255810	33.063028
747.978144	62184.931043	33.068045
748.734549	62288.685074	33.073063
749.441100	62389.553188	33.078080
750.112947	62480.555245	33.083098
750.537404	62594.509708	33.088116
751.100403	62688.633946	33.093133
752.148815	62806.809679	33.098151
752.759142	62930.026291	33.103168
754.005408	63021.106557	33.108186
754.231543	63134.148711	33.113204
755.381589	63241.331494	33.118221
756.362395	63337.551347	33.123239
756.560012	63466.496233	33.128256
757.765873	63558.622144	33.133274
758.563707	63660.543324	33.138292
759.124969	63762.617847	33.143309
760.020789	63860.491247	33.148327
760.945682	63967.354729	33.153344
761.247477	64076.002985	33.158362
762.157365	64178.458141	33.163380
762.886241	64282.820987	33.168397
763.523466	64402.894230	33.173415
764.205788	64510.710798	33.178432
764.931379	64621.346248	33.183450
765.622080	64743.315248	33.188468
766.454293	64848.643649	33.193485
767.585507	64954.150774	33.198503
768.002919	65073.271813	33.203520
769.108101	65173.190198	33.208538
769.898148	65286.524006	33.213556
770.585987	65385.229139	33.218573
771.476740	65498.553801	33.223591
772.088895	65616.571205	33.228608
773.042686	65716.668925	33.233626
773.897732	65832.517180	33.238644
774.254019	65939.004347	33.243661
775.696439	66045.793135	33.248679
775.828853	66150.251261	33.253696
777.038580	66240.428886	33.258714
777.260478	66345.739255	33.263732
778.077655	66445.034935	33.268749
778.874844	66551.774832	33.273767
779.234223	66661.425954	33.278784
780.192620	66762.444582	33.283802
781.248782	66868.074988	33.288820
781.790533	66982.274541	33.293837
783.077539	67074.459632	33.298855
783.329234	67187.842135	33.303872
784.089056	67293.567880	33.308890
785.044677	67403.314097	33.313908
785.350795	67512.049176	33.318925
786.780031	67610.534973	33.323943
787.332814	67734.415573	33.328960
788.144696	67847.089600	33.333978
788.695929	67957.189982	33.338996
790.262727	68082.479367	33.344013
791.364197	68160.949552	33.349031
791.781693	68276.542240	33.354048
792.835595	68365.269095	33.359066
793.456607	68482.631103	33.364084
794.197604	68592.355764	33.369101
795.125769	68701.778236	33.374119
795.770793	68806.101750	33.379136
796.662121	68914.153167	33.384154
797.597751	69018.360201	33.389172
798.360023	69125.441415	33.394189
799.314015	69225.012187	33.399207
800.069847	69338.986896	33.404224
800.613558	69452.086820	33.409242
801.681691	69560.409504	33.414260
802.139908	69671.874564	33.419277
803.059959	69772.895046	33.424295
803.654624	69901.004900	33.429312
804.615287	70002.822736	33.434330
805.096053	70112.572973	33.439348
806.143341	70230.639339	33.444365
807.180570	70329.442847	33.449383
808.483987	70440.070567	33.454400
809.294386	70563.002118	33.459418
810.024347	70656.173744	33.464436
810.709745	70769.092902	33.469453
811.645367	70871.051814	33.474471
812.344227	70986.435804	33.479488
812.992163	71082.948668	33.484506
813.846553	71196.310079	33.489524
814.377396	71315.726004	33.494541
815.338962	71433.699386	33.499559
815.400191	71557.082844	33.504576
815.875175	71669.099375	33.509594
816.748641	71802.802159	33.514612
817.364101	71931.293849	33.519629
818.582686	72051.061907	33.524647
819.321572	72181.918556	33.529664
820.334160	72308.449968	33.534682
821.427192	72436.631868	33.539700
822.051606	72569.166482	33.544717
822.794415	72694.106968	33.549735
823.548089	72827.519747	33.554752
824.406779	72941.174230	33.559770
824.801997	73077.733584	33.564788
825.063975	73221.530937	33.569805
826.769718	73344.463404	33.574823
827.496781	73489.943700	33.579840
828.259452	73628.140584	33.584858
829.105879	73752.747586	33.589876
829.525108	73884.432518	33.594893
830.818146	74003.573094	33.599911
831.332145	74142.377134	33.604928
832.350308	74266.661518	33.609946
833.177511	74389.428799	33.614964
833.853697	74515.358362	33.619981
834.505003	74639.515737	33.624999
835.506904	74772.172264	33.630016
836.274344	74905.127598	33.635034
837.077131	75034.877939	33.640052
837.808023	75172.400577	33.645069
838.995677	75307.647867	33.650087
839.657437	75440.295059	33.655104
840.424515	75571.116944	33.660122
841.694188	75687.127473	33.665140
842.522077	75821.083959	33.670157
843.286379	75946.545562	33.675175
844.157696	76071.294537	33.680192
845.146208	76210.912475	33.685210
846.083559	76338.074304	33.690228
846.794448	76466.659321	33.695245
847.996216	76582.388554	33.700263
848.938776	76725.660263	33.705280
849.561653	76865.987839	33.710298
850.460087	76984.229533	33.715316
851.079083	77111.587543	33.720333
852.430578	77243.777570	33.725351
853.125553	77386.133101	33.730368
853.934070	77506.384731	33.735386
854.960774	77642.741869	33.740404
855.695670	77777.377076	33.745421
856.656444	77905.435886	33.750439
857.545013	78041.090927	33.755456
858.000449	78165.205708	33.760474
859.323552	78288.241822	33.765492
860.008265	78436.608211	33.770509
861.023979	78547.963601	33.775527
861.872793	78696.260353	33.780544
862.605869	78832.268483	33.785562
863.891450	78964.264609	33.790580
864.392766	79094.664227	33.795597
865.308648	79227.690713	33.800615
866.184933	79366.373013	33.805632
866.895028	79510.700506	33.810650
867.927450	79623.348881	33.815668
868.859622	79764.655776	33.820685
869.901894	79896.128302	33.825703
871.110448	80024.879493	33.830720
872.067430	80133.741285	33.835738
873.468552	80258.805884	33.840756
874.734843	80374.771965	33.845773
875.631503	80486.346449	33.850791
876.858365	80595.260807	33.855808
877.259053	80710.827539	33.860826
878.309690	80815.166973	33.865844
878.957356	80941.314958	33.870861
879.757409	81044.077440	33.875879
880.378061	81159.211631	33.880896
881.497717	81276.509688	33.885914
882.234398	81388.026495	33.890932
882.662657	81510.601825	33.895949
883.171997	81633.746417	33.900967
883.869424	81761.427969	33.905984
884.798871	81897.428576	33.911002
885.860867	82023.647041	33.916020
887.068849	82144.667381	33.921037
888.484709	82255.608196	33.926055
889.357504	82381.885200	33.931072
889.699061	82503.809646	33.936090
890.633847	82613.711910	33.941108
891.349260	82724.909845	33.946125
892.387986	82845.209044	33.951143
893.091821	82956.694705	33.956160
893.749034	83068.802263	33.961178
894.736111	83184.246836	33.966196
894.773169	83313.507529	33.971213
896.136354	83432.263227	33.976231
897.076132	83549.691303	33.981248
897.521439	83685.681312	33.986266
898.333223	83833.815507	33.991284
899.050362	83968.357822	33.996301
900.117880	84109.549285	34.001319
901.353209	84243.830514	34.006336
901.806697	84385.352814	34.011354
903.085339	84529.017369	34.016372
903.600591	84676.415121	34.021389
904.527310	84819.139963	34.026407
905.204743	84955.852056	34.031424
906.190420	85103.276098	34.036442
907.405913	85251.061734	34.041460
908.999724	85360.646927	34.046477
910.847956	85485.938512	34.051495
911.985734	85607.785962	34.056512
913.098604	85724.854911	34.061530
913.898234	85846.449422	34.066548
914.691980	85965.932284	34.071565
915.235028	86087.912089	34.076583
916.329679	86205.600211	34.081600
916.759990	86344.740335	34.086618
917.740345	86461.170523	34.091636
918.501363	86606.610179	34.096653
919.079163	86741.197979	34.101671
919.791001	86887.767449	34.106688
920.596801	87027.893676	34.111706
921.285231	87173.165356	34.116724
922.372742	87317.252085	34.121741
923.048485	87464.970085	34.126759
924.099164	87618.189047	34.131776
925.056796	87767.684757	34.136794
926.550827	87911.999101	34.141812
927.100527	88054.034086	34.146829
928.099731	88201.817224	34.151847
929.250025	88331.770016	34.156864
930.086133	88493.699159	34.161882
931.552352	88627.138669	34.166900
932.382286	88757.184671	34.171917
933.307486	88902.491245	34.176935
934.018896	89037.987716	34.181952
934.681926	89183.624063	34.186970
935.906165	89324.593486	34.191988
936.499113	89484.955930	34.197005
937.509020	89634.372594	34.202023
938.338849	89774.707395	34.207040
939.397088	89921.757491	34.212058
940.704005	90080.487321	34.217076
941.279605	90221.429948	34.222093
941.982764	90380.362714	34.227111
943.146783	90520.070866	34.232128
944.279187	90667.391777	34.237146
945.280784	90797.496572	34.242164
946.494487	90942.249078	34.247181
947.633590	91084.736519	34.252199
948.683901	91230.947991	34.257216
949.595876	91363.507152	34.262234
950.574218	91497.074996	34.267252
951.445297	91634.199003	34.272269
952.220104	91776.295044	34.277287
953.517130	91899.965096	34.282304
954.416669	92031.099713	34.287322
955.477206	92148.456029	34.292340
956.767013	92253.516168	34.297357
957.743616	92380.355367	34.302375
958.828109	92489.279381	34.307392
959.335243	92626.912159	34.312410
960.509838	92736.727449	34.317428
961.485408	92862.449135	34.322445
962.193706	92985.601725	34.327463
963.708600	93107.185087	34.332480
964.198550	93222.577571	34.337498
964.923388	93360.355797	34.342516
965.791400	93492.180773	34.347533
966.236651	93626.525649	34.352551
966.808263	93768.394812	34.357568
967.998290	93917.776779	34.362586
968.619327	94067.785262	34.367604
969.619697	94210.877392	34.372621
970.298224	94372.321664	34.377639
971.356222	94518.330248	34.382656
972.011669	94688.844120	34.387674
972.929550	94831.231951	34.392692
974.262824	95013.662190	34.397709
974.831837	95180.794806	34.402727
975.961319	95342.512829	34.407744
976.577854	95514.754198	34.412762
977.850815	95667.209382	34.417780
978.779322	95840.901669	34.422797
979.505243	96014.426075	34.427815
980.782488	96183.784274	34.432832
981.293528	96368.734006	34.437850
982.279300	96543.997930	34.442868
983.480540	96713.536890	34.447885
984.600081	96888.021574	34.452903
986.269074	97067.132664	34.457920
987.214029	97235.824975	34.462938
988.756832	97389.575566	34.467956
989.992562	97546.770779	34.472973
991.076415	97707.574960	34.477991
992.421893	97858.170601	34.483008
993.457825	98011.622576	34.488026
994.055881	98163.349971	34.493044
995.118997	98314.507742	34.498061
995.979733	98472.992466	34.503079
997.265483	98617.683623	34.508096
998.328729	98768.679527	34.513114
999.011069	98924.081961	34.518132
1000.393920	99079.914139	34.523149
1001.519255	99245.659206	34.528167
1002.478100	99379.861949	34.533184
1003.222959	99536.080831	34.538202
1003.984879	99701.654663	34.543220
1005.611886	99846.796693	34.548237
1006.687811	100010.351849	34.553255
1007.891249	100132.388423	34.558272
1008.805124	100279.594237	34.563290
1009.692490	100430.654470	34.568308
1011.006738	100576.985562	34.573325
1011.527559	100727.778871	34.578343
1012.448032	100882.141098	34.583360
1012.769770	101040.192814	34.588378
1013.949669	101201.649249	34.593396
1015.008601	101366.406205	34.598413
1015.645992	101528.600051	34.603431
1016.395257	101692.492217	34.608448
1017.332053	101863.451813	34.613466
1017.968474	102026.332754	34.618484
1019.174497	102199.314151	34.623501
1019.465786	102373.448086	34.628519
1020.776819	102533.745314	34.633536
1021.490882	102709.255296	34.638554
1022.452445	102883.864532	34.643572
1023.721933	103056.587969	34.648589
1024.549046	103241.162360	34.653607
1026.058153	103404.154900	34.658624
1026.832256	103581.383117	34.663642
1027.884853	103753.805119	34.668660
1029.009682	103924.804363	34.673677
1029.743437	104112.148370	34.678695
1030.850631	104291.808530	34.683712
1031.838805	104469.558353	34.688730
1032.468487	104665.636222	34.693748
1033.698064	104849.041204	34.698765
1034.385667	105046.024180	34.703783
1035.264365	105240.387273	34.708800
1036.762243	105441.045046	34.713818
1037.733507	105644.159531	34.718836
1038.681328	105828.878009	34.723853
1039.422812	106036.276055	34.728871
1041.043485	106233.854808	34.733888
1041.961930	106437.832684	34.738906
1042.965899	106640.417554	34.743924
1044.307360	106841.352484	34.748941
1045.086500	107048.714291	34.753959
1046.148855	107246.886744	34.758976
1047.301462	107440.511631	34.763994
1048.301081	107649.108264	34.769012
1049.652133	107846.629606	34.774029
1050.699753	108037.895086	34.779047
1051.761417	108246.942126	34.784064
1052.872574	108448.066571	34.789082
1053.910241	108666.772130	34.794100
1054.816773	108859.004059	34.799117
1056.004757	109070.354551	34.804135
1056.957599	109265.900247	34.809152
1057.736538	109464.237303	34.814170
1058.749455	109686.729793	34.819188
1059.977849	109893.558229	34.824205
1061.142370	110099.714808	34.829223
1062.263379	110311.314107	34.834240
1064.166954	110513.893870	34.839258
1065.328220	110715.749019	34.844276
1066.496676	110907.686333	34.849293
1067.080370	111122.484052	34.854311
1068.460173	111314.326018	34.859328
1069.658355	111511.519516	34.864346
1070.315228	111715.175420	34.869364
1071.384644	111904.704010	34.874381
1072.060017	112120.837198	34.879399
1073.158735	112325.210088	34.884416
1074.456603	112528.284866	34.889434
1075.085716	112741.707052	34.894452
1076.425381	112958.788604	34.899469
1077.449159	113179.762392	34.904487
1078.505149	113372.749011	34.909504
1079.474352	113584.880125	34.914522
1080.219700	113804.220018	34.919540
1081.561046	114013.708676	34.924557
1082.600466	114238.412824	34.929575
1083.617706	114457.358286	34.934592
1084.981658	114669.939279	34.939610
1086.002484	114883.959425	34.944628
1087.175483	115091.685046	34.949645
1088.438639	115309.291723	34.954663
1089.631074	115523.617835	34.959680
1090.832979	115704.561032	34.964698
1091.848844	115904.552495	34.969716
1092.854406	116093.752893	34.974733
1093.795349	116293.949534	34.979751
1094.986670	116493.384109	34.984768
1096.150026	116691.823822	34.989786
1097.229180	116875.062652	34.994804
1098.795828	117058.792333	34.999821
1100.134136	117255.699434	35.004839
1101.061149	117452.903856	35.009856
1102.667803	117633.551889	35.014874
1103.322108	117837.189637	35.019892
1104.114855	118032.785813	35.024909
1105.058268	118234.478160	35.029927
1106.090327	118445.951428	35.034944
1107.099895	118649.891098	35.039962
1107.781878	118874.703878	35.044980
1109.062966	119073.267472	35.049997
1110.372300	119291.327912	35.055015
1111.286030	119488.751304	35.060032
1112.619365	119700.576878	35.065050
1113.671722	119920.445748	35.070068
1115.614728	120123.696934	35.075085
1116.476218	120332.601999	35.080103
1117.475215	120529.777680	35.085120
1118.778295	120736.458656	35.090138
1119.553261	120963.135024	35.095156
1120.670670	121173.220343	35.100173
1121.646287	121379.769869	35.105191
1122.777659	121599.144211	35.110208
1124.294570	121818.304497	35.115226
1125.093019	122037.470973	35.120244
1125.994780	122252.858463	35.125261
1126.888130	122483.721484	35.130279
1128.046153	122710.335474	35.135296
1129.246481	122941.075373	35.140314
1130.218209	123166.899924	35.145332
1131.353949	123394.815422	35.150349
1132.481906	123630.375496	35.155367
1133.566865	123872.813108	35.160384
1135.113875	124097.143116	35.165402
1135.976397	124335.578611	35.170420
1137.132670	124553.272620	35.175437
1138.171067	124787.373894	35.180455
1139.203114	125024.544943	35.185472
1141.025917	125250.472918	35.190490
1142.116390	125488.664520	35.195508
1143.210801	125714.336016	35.200525
1144.556652	125942.084173	35.205543
1145.928775	126172.161656	35.210560
1147.457384	126389.984933	35.215578
1148.418361	126622.529035	35.220596
1149.744362	126829.185274	35.225613
1151.529806	127054.587934	35.230631
1152.100396	127258.773618	35.235648
1152.978841	127474.532048	35.240666
1153.654856	127722.530685	35.245684
1154.922491	127937.784542	35.250701
1155.968034	128171.834738	35.255719
1156.805985	128407.670070	35.260736
1158.311973	128635.285173	35.265754
1159.140412	128874.826644	35.270772
1160.584207	129102.544183	35.275789
1161.924662	129333.436512	35.280807
1163.025313	129574.396081	35.285824
1164.082568	129809.534131	35.290842
1165.210735	130036.055787	35.295860
1166.255855	130260.298569	35.300877
1167.631486	130484.260249	35.305895
1168.630874	130714.560000	35.310912
1169.860163	130917.811860	35.315930
1171.104530	131138.592970	35.320948
1172.568985	131345.281910	35.325965
1174.135431	131555.060948	35.330983
1175.012003	131767.629872	35.336000
1176.433093	131981.783576	35.341018
1177.474554	132198.245059	35.346036
1178.493927	132417.272251	35.351053
1179.898580	132630.596428	35.356071
1180.531412	132849.424200	35.361088
1181.443171	133066.724293	35.366106
1182.644427	133292.598108	35.371124
1183.974374	133536.047404	35.376141
1184.878021	133764.711822	35.381159
1185.568316	134010.716907	35.386176
1187.146347	134246.727398	35.391194
1188.224772	134494.282078	35.396212
1189.425219	134735.885641	35.401229
1190.605864	134964.741041	35.406247
1191.722407	135215.451565	35.411264
1193.539062	135447.057776	35.416282
1194.457525	135695.180482	35.421300
1195.594898	135944.333859	35.426317
1196.905330	136173.328472	35.431335
1197.976899	136423.700739	35.436352
1199.296701	136666.084944	35.441370
1199.994437	136918.715956	35.446388
1201.353416	137179.302986	35.451405
1202.738834	137425.802314	35.456423
1203.877160	137683.386994	35.461440
1205.103105	137922.930650	35.466458
1206.254856	138176.865593	35.471476
1207.410858	138426.617867	35.476493
1209.300411	138668.542347	35.481511
1210.308989	138930.240608	35.486528
1211.661559	139178.102289	35.491546
1212.956263	139436.765085	35.496564
1214.004943	139690.931403	35.501581
1215.394220	139928.890280	35.506599
1216.296427	140193.062990	35.511616
1217.578457	140441.997988	35.516634
1219.420141	140690.487419	35.521652
1220.369466	140943.551086	35.526669
1221.751087	141190.801448	35.531687
1222.806223	141458.521709	35.536704
1224.038828	141692.714913	35.541722
1224.975575	141960.078245	35.546740
1226.084582	142225.361079	35.551757
1227.527557	142462.491914	35.556775
1228.491210	142736.551885	35.561792
1229.972017	142999.471526	35.566810
1231.013129	143262.744703	35.571828
1232.332862	143519.811214	35.576845
1233.374846	143779.867342	35.581863
1234.848733	144039.892164	35.586880
1235.975346	144306.341943	35.591898
1236.953014	144571.600977	35.596916
1238.348362	144835.639116	35.601933
1240.011031	145083.061088	35.606951
1240.701768	145360.902225	35.611968
1242.385280	145612.838930	35.616986
1243.981915	145872.578052	35.622004
1244.796943	146130.698055	35.627021
1246.061125	146389.772991	35.632039
1247.029537	146650.420409	35.637056
1248.370732	146912.377812	35.642074
1249.818419	147177.249029	35.647092
1250.541193	147420.733513	35.652109
1252.637018	147653.847517	35.657127
1253.819039	147896.663369	35.662144
1255.151522	148141.472465	35.667162
1256.556517	148381.236439	35.672180
1257.637334	148614.790488	35.677197
1259.036620	148864.843873	35.682215
1259.902928	149107.428237	35.687232
1261.217650	149365.133801	35.692250
1262.391665	149606.250248	35.697268
1263.427001	149880.099712	35.702285
1264.767994	150123.373406	35.707303
1266.033316	150379.876695	35.712320
1267.425388	150628.649634	35.717338
1269.026742	150881.346796	35.722356
1270.046361	151147.357464	35.727373
1271.073880	151403.653417	35.732391
1272.443833	151667.745550	35.737408
1273.647363	151934.162701	35.742426
1274.923356	152192.731418	35.747444
1276.023607	152469.823505	35.752461
1277.488498	152719.321304	35.757479
1278.975593	152978.951363	35.762496
1279.995905	153255.567741	35.767514
1281.869802	153522.824066	35.772532
1282.911090	153784.359691	35.777549
1284.495833	154051.274243	35.782567
1285.351469	154324.386701	35.787584
1286.714904	154578.213356	35.792602
1288.354977	154847.267952	35.797620
1289.460454	155133.118033	35.802637
1291.107273	155389.275244	35.807655
1292.238642	155654.601384	35.812672
1293.668551	155928.746653	35.817690
1295.427017	156182.112722	35.822708
1296.696366	156445.442655	35.827725
1298.274390	156690.152681	35.832743
1299.602137	156949.353762	35.837760
1300.922695	157210.409760	35.842778
1302.127756	157457.494802	35.847796
1303.298111	157727.686963	35.852813
1304.524932	157994.091414	35.857831
1305.947189	158249.885751	35.862848
1307.147874	158509.118014	35.867866
1309.009160	158766.365466	35.872884
1309.907681	159029.088763	35.877901
1311.692871	159286.428226	35.882919
1313.205209	159534.008219	35.887936
1314.451034	159770.229087	35.892954
1316.222676	160026.700183	35.897972
1316.950936	160284.321928	35.902989
1318.309677	160533.303475	35.908007
1319.424289	160789.012472	35.913024
1320.646299	161043.766558	35.918042
1322.329422	161291.633541	35.923060
1323.522211	161549.338829	35.928077
1324.834958	161802.293854	35.933095
1325.806769	162073.892587	35.938112
1326.951078	162332.714500	35.943130
1328.529043	162579.705818	35.948148
1329.216231	162844.835566	35.953165
1330.756530	163105.728324	35.958183
1332.184795	163385.608283	35.963200
1333.452294	163641.753709	35.968218
1335.184510	163912.223939	35.973236
1336.555806	164174.838623	35.978253
1338.237775	164411.990945	35.983271
1339.492401	164665.759488	35.988288
1340.895299	164905.726478	35.993306
1341.904113	165143.082786	35.998324
1343.148862	165389.739558	36.003341
1344.080400	165621.148091	36.008359
1345.600004	165882.936809	36.013376
1346.648121	166136.075699	36.018394
1347.829900	166388.014037	36.023412
1349.194650	166651.114447	36.028429
1350.367614	166910.911141	36.033447
1351.358920	167177.629023	36.038464
1352.472581	167457.638282	36.043482
1353.905353	167717.079687	36.048500
1354.966309	168016.285914	36.053517
1356.253995	168290.587364	36.058535
1357.825612	168572.063436	36.063552
1359.206260	168854.841674	36.068570
1360.907455	169129.816013	36.073588
1361.852664	169415.423118	36.078605
1363.307953	169689.883179	36.083623
1365.291534	169982.707449	36.088640
1366.433178	170276.459290	36.093658
1367.937230	170559.050265	36.098676
1369.285407	170842.188982	36.103693
1370.451680	171133.074553	36.108711
1371.543447	171436.955473	36.113728
1373.145663	171735.513435	36.118746
1374.634643	172012.748272	36.123764
1375.863642	172320.761858	36.128781
1377.302703	172596.777550	36.133799
1378.614864	172906.481722	36.138816
1379.808551	173212.083309	36.143834
1382.206933	173479.862499	36.148852
1384.071363	173775.357429	36.153869
1385.694615	174051.402083	36.158887
1387.555242	174319.287493	36.163904
1388.525850	174600.303380	36.168922
1390.060851	174882.712551	36.173940
1391.561692	175166.144263	36.178957
1392.971242	175435.874365	36.183975
1394.615660	175695.719398	36.188992
1395.304924	175981.751820	36.194010
1396.815225	176256.469984	36.199028
1398.205600	176554.370061	36.204045
1399.665376	176846.181618	36.209063
1400.862008	177119.052802	36.214080
1402.022694	177415.688887	36.219098
1403.378847	177703.689993	36.224116
1404.436115	178000.905077	36.229133
1405.904913	178296.150358	36.234151
1406.892092	178594.129346	36.239168
1408.160758	178902.559389	36.244186
1409.658471	179208.834071	36.249204
1410.464522	179522.560441	36.254221
1411.713520	179836.621796	36.259239
1413.765062	180132.885899	36.264256
1415.074121	180457.449866	36.269274
1416.768842	180771.405372	36.274292
1418.336037	181084.914250	36.279309
1419.910051	181381.061331	36.284327
1421.068101	181698.867885	36.289344
1422.214200	182016.589516	36.294362
1424.154684	182333.687001	36.299380
1425.204468	182642.416896	36.304397
1426.211537	182953.795662	36.309415
1427.835856	183264.338250	36.314432
1429.100963	183592.178329	36.319450
1430.856913	183905.304913	36.324468
1431.635925	184219.622657	36.329485
1432.626244	184519.399616	36.334503
1434.684072	184826.973147	36.339520
1436.374301	185135.345280	36.344538
1437.886371	185434.051181	36.349556
1439.071671	185741.291561	36.354573
1441.030339	186041.539105	36.359591
1442.700073	186351.317741	36.364608
1444.094534	186656.332823	36.369626
1446.146412	186951.670377	36.374644
1447.529962	187253.936113	36.379661
1449.150519	187550.338105	36.384679
1450.728039	187829.346024	36.389696
1452.050489	188126.142978	36.394714
1453.717569	188420.485533	36.399732
1454.833567	188720.785030	36.404749
1455.981421	189011.420925	36.409767
1457.892394	189302.452817	36.414784
1459.660730	189608.348848	36.419802
1461.133897	189897.945434	36.424820
1462.537904	190198.725594	36.429837
1464.017711	190490.342389	36.434855
1465.187445	190788.460423	36.439872
1466.273279	191105.165415	36.444890
1468.069655	191406.204397	36.449908
1469.131841	191714.005194	36.454925
1470.429497	192028.420590	36.459943
1472.007348	192336.494958	36.464960
1473.284999	192671.875583	36.469978
1474.908056	192982.192734	36.474996
1476.168877	193301.394038	36.480013
1477.170641	193625.260644	36.485031
1479.273987	193953.821990	36.490048
1480.571543	194290.122283	36.495066
1481.847767	194605.163928	36.500084
1483.267490	194946.728722	36.505101
1484.505739	195281.393829	36.510119
1486.533352	195611.728382	36.515136
1488.084060	195957.034830	36.520154
1489.800152	196277.991745	36.525172
1491.509759	196610.008981	36.530189
1492.941374	196949.195929	36.535207
1494.619505	197268.297858	36.540224
1495.705514	197605.247411	36.545242
1497.838810	197925.280416	36.550260
1499.636602	198256.161656	36.555277
1500.620817	198579.929561	36.560295
1502.638984	198901.332072	36.565312
1503.584086	199225.896730	36.570330
1505.283588	199550.528923	36.575348
1506.851185	199884.452505	36.580365
1508.334375	200209.301316	36.585383
1509.721304	200538.458846	36.590400
1511.356539	200861.546324	36.595418
1513.193572	201187.166661	36.600436
1514.899082	201514.270311	36.605453
1516.598997	201840.411509	36.610471
1517.881763	202163.233133	36.615488
1519.277069	202492.284324	36.620506
1521.055850	202809.529513	36.625524
1522.540819	203122.926763	36.630541
1523.814103	203446.073229	36.635559
1525.612410	203768.093394	36.640576
1527.139232	204091.188231	36.645594
1528.779500	204404.552752	36.650612
1530.366087	204726.078848	36.655629
1531.434713	205048.402847	36.660647
1532.784293	205358.175404	36.665664
1533.919382	205667.718012	36.670682
1536.051171	205967.701627	36.675700
1538.338580	206268.651141	36.680717
1539.659477	206565.876008	36.685735
1541.235221	206866.615207	36.690752
1542.845239	207160.239478	36.695770
1544.445506	207451.809522	36.700788
1545.952346	207749.465416	36.705805
1547.136531	208046.756679	36.710823
1548.807990	208348.133436	36.715840
1549.934231	208656.115128	36.720858
1551.260256	208965.728436	36.725876
1552.682169	209281.955274	36.730893
1553.955383	209624.263468	36.735911
1555.417651	209939.838665	36.740928
1556.827220	210269.937315	36.745946
1558.053922	210592.867825	36.750964
1559.357786	210928.713286	36.755981
1560.869861	211284.994780	36.760999
1562.618159	211621.607782	36.766016
1564.181715	211978.137704	36.771034
1565.668866	212330.516776	36.776052
1566.834410	212676.550526	36.781069
1568.597379	213046.765998	36.786087
1570.148759	213389.894571	36.791104
1571.517159	213762.133735	36.796122
1573.076245	214116.920915	36.801140
1574.634416	214494.719134	36.806157
1576.040172	214863.096473	36.811175
1577.772314	215227.129386	36.816192
1579.049142	215608.889856	36.821210
1580.424592	215980.222811	36.826228
1582.314076	216361.428185	36.831245
1583.867812	216749.801792	36.836263
1585.887509	217125.122015	36.841280
1587.339916	217514.048850	36.846298
1588.829103	217898.501212	36.851316
1590.777245	218278.206194	36.856333
1592.556394	218721.613085	36.861351
1594.378076	219086.560502	36.866368
1596.117299	219469.123757	36.871386
1598.233975	219848.654612	36.876404
1600.099595	220209.052614	36.881421
1602.049542	220569.717364	36.886439
1603.804995	220926.148533	36.891456
1605.369034	221281.139396	36.896474
1606.713080	221641.603075	36.901492
1608.741788	221997.103865	36.906509
1609.850007	222353.722875	36.911527
1611.905827	222719.609712	36.916544
1613.322459	223079.329699	36.921562
1614.595624	223427.975151	36.926580
1616.310800	223801.185944	36.931597
1617.392674	224165.536547	36.936615
1619.081990	224541.040001	36.941632
1620.808618	224927.663473	36.946650
1622.584520	225299.091225	36.951668
1624.836201	225652.966769	36.956685
1625.710573	226013.064937	36.961703
1627.493713	226386.069710	36.966720
1628.767645	226771.910353	36.971738
1629.999203	227152.018842	36.976756
1631.923289	227519.492072	36.981773
1633.355987	227921.616901	36.986791
1634.889215	228289.512485	36.991808
1636.562127	228667.469959	36.996826
1638.108376	229056.092147	37.001844
1640.102248	229422.898962	37.006861
1641.276197	229804.675909	37.011879
1642.958344	230169.402587	37.016896
1644.539110	230536.763233	37.021914
1645.570340	230905.841171	37.026932
1647.213110	231270.069271	37.031949
1648.901719	231659.818499	37.036967
1650.450147	232038.288563	37.041984
1652.233375	232415.908057	37.047002
1653.545959	232815.527191	37.052020
1655.103344	233197.377110	37.057037
1656.553411	233595.578597	37.062055
1658.459063	233987.609687	37.067072
1660.494762	234379.848926	37.072090
1661.657485	234778.837505	37.077108
1663.303552	235179.093608	37.082125
1664.636372	235585.016091	37.087143
1666.515707	235996.285321	37.092160
1668.130834	236412.984274	37.097178
1669.662975	236834.143216	37.102196
1671.232706	237247.701889	37.107213
1672.707551	237679.007575	37.112231
1674.210774	238097.227707	37.117248
1675.956855	238530.319595	37.122266
1677.611428	238958.448817	37.127284
1679.642216	239386.923365	37.132301
1681.267195	239834.974540	37.137319
1682.736957	240265.397909	37.142336
1684.957914	240706.417946	37.147354
1686.472137	241152.534343	37.152372
1688.579667	241573.278596	37.157389
1689.950731	242003.925038	37.162407
1691.955376	242445.492388	37.167424
1693.951516	242888.179702	37.172442
1695.573187	243324.477427	37.177460
1697.680511	243757.596728	37.182477
1699.372124	244202.089486	37.187495
1701.010886	244626.091901	37.192512
1702.853573	245059.663542	37.197530
1704.294012	245497.239657	37.202548
1706.542060	245923.734688	37.207565
1708.044740	246353.528671	37.212583
1709.794575	246791.487598	37.217600
1711.305846	247225.117245	37.222618
1713.362521	247662.620358	37.227636
1715.053801	248094.341697	37.232653
1716.786684	248537.792862	37.237671
1718.593224	248965.990704	37.242688
1720.810418	249397.677724	37.247706
1722.481581	249819.116322	37.252724
1724.428855	250245.590428	37.257741
1726.242709	250677.447034	37.262759
1727.799085	251105.586912	37.267776
1729.746953	251535.898091	37.272794
1731.501356	251975.843956	37.277812
1732.991057	252387.763454	37.282829
1734.595383	252821.612679	37.287847
1736.539894	253238.030378	37.292864
1738.812996	253660.389320	37.297882
1740.247142	254083.750671	37.302900
1741.714431	254498.672969	37.307917
1743.374724	254939.347941	37.312935
1744.554404	255363.590360	37.317952
1746.764374	255792.388036	37.322970
1748.084557	256231.138366	37.327988
1750.417572	256662.354858	37.333005
1751.822077	257098.068658	37.338023
1754.222006	257525.413136	37.343040
1756.050477	257947.466520	37.348058
1757.471526	258358.003320	37.353076
1759.107918	258753.643749	37.358093
1760.705191	259175.710132	37.363111
1762.009443	259573.183700	37.368128
1764.358833	259991.518825	37.373146
1765.568994	260397.848317	37.378164
1767.646229	260807.769056	37.383181
1769.282462	261224.697633	37.388199
1770.997377	261642.019648	37.393216
1772.660814	262065.624719	37.398234
1774.028277	262493.114440	37.403252
1775.784314	262913.579466	37.408269
1777.376440	263364.529958	37.413287
1779.468331	263794.236932	37.418304
1781.120547	264220.815473	37.423322
1783.313878	264670.523153	37.428340
1785.199560	265112.609595	37.433357
1786.454742	265550.354258	37.438375
1788.034964	265986.292238	37.443392
1790.233538	266429.469476	37.448410
1791.791646	266894.802039	37.453428
1793.362191	267338.666536	37.458445
1795.365432	267801.918125	37.463463
1797.223239	268256.226017	37.468480
1798.977151	268705.978094	37.473498
1800.641238	269177.972265	37.478516
1802.820228	269637.179497	37.483533
1804.521500	270100.707361	37.488551
1806.042203	270565.483847	37.493568
1807.994918	271014.997560	37.498586
1809.824587	271491.077107	37.503604
1811.770909	271959.084079	37.508621
1813.819150	272423.237787	37.513639
1815.314639	272911.386101	37.518656
1817.257517	273371.745446	37.523674
1818.853366	273849.943288	37.528692
1820.819510	274326.072480	37.533709
1822.761016	274821.079143	37.538727
1824.266306	275304.065254	37.543744
1826.121099	275778.787829	37.548762
1827.975004	276268.725816	37.553780
1829.530097	276754.393743	37.558797
1830.892370	277260.668499	37.563815
1833.125628	277749.728127	37.568832
1835.123876	278230.290326	37.573850
1836.638576	278755.055018	37.578868
1838.918675	279239.074090	37.583885
1840.976799	279741.316637	37.588903
1842.464006	280235.421891	37.593920
1844.722652	280721.651088	37.598938
1846.429900	281224.481342	37.603956
1848.818111	281723.209882	37.608973
1850.697351	282211.276106	37.613991
1852.859152	282699.751682	37.619008
1855.064539	283180.953880	37.624026
1856.668356	283667.410550	37.629044
1858.296980	284158.738879	37.634061
1860.772411	284626.734565	37.639079
1862.350379	285109.711419	37.644096
1864.546806	285591.289376	37.649114
1866.596700	286067.784421	37.654132
1869.462522	286523.212873	37.659149
1871.669844	286985.073496	37.664167
1873.790008	287430.309428	37.669184
1875.926027	287879.021366	37.674202
1877.883924	288323.112968	37.679220
1879.219957	288760.853994	37.684237
1881.165621	289200.626792	37.689255
1882.390733	289637.367402	37.694272
1884.692619	290049.519080	37.699290
1886.110211	290476.801683	37.704308
1887.792430	290909.881389	37.709325
1889.418306	291335.323487	37.714343
1891.002199	291776.519295	37.719360
1892.952594	292209.017099	37.724378
1894.590119	292667.549332	37.729396
1896.144921	293109.431160	37.734413
1898.006039	293562.944850	37.739431
1899.243935	294026.643388	37.744448
1901.370225	294488.466439	37.749466
1903.094186	294958.862939	37.754484
1904.733618	295437.043755	37.759501
1906.455629	295925.648138	37.764519
1908.158735	296407.268761	37.769536
1910.005060	296898.236011	37.774554
1911.804348	297402.035388	37.779572
1913.442606	297914.367672	37.784589
1915.310109	298405.705707	37.789607
1917.178402	298913.347332	37.794624
1919.109040	299428.595818	37.799642
1920.496947	299944.820232	37.804660
1922.155603	300477.531715	37.809677
1924.176351	301009.190161	37.814695
1926.340745	301558.295959	37.819712
1928.195423	302083.728158	37.824730
1930.348745	302633.794914	37.829748
1932.390493	303169.552684	37.834765
1934.695465	303703.663990	37.839783
1936.334545	304246.821967	37.844800
1938.593688	304776.718760	37.849818
1940.496923	305325.795176	37.854836
1942.656881	305864.438606	37.859853
1944.995743	306404.827068	37.864871
1947.047730	306952.573771	37.869888
1949.344153	307476.073950	37.874906
1951.798614	308012.522394	37.879924
1954.037409	308522.692686	37.884941
1956.324121	309051.645014	37.889959
1957.704737	309583.765557	37.894976
1959.709736	310114.408343	37.899994
1961.849799	310652.313920	37.905012
1963.552738	311177.895131	37.910029
1965.456945	311704.557096	37.915047
1967.012977	312240.186634	37.920064
1969.103726	312765.617210	37.925082
1971.409857	313306.727986	37.930100
1973.364486	313838.623975	37.935117
1976.095191	314365.868080	37.940135
1977.998801	314889.258056	37.945152
1980.273481	315413.852869	37.950170
1982.406289	315942.479580	37.955188
1984.178887	316470.933359	37.960205
1986.542097	316978.996598	37.965223
1988.312707	317503.634171	37.970240
1990.401444	318020.216632	37.975258
1992.404346	318518.526662	37.980276
1994.432842	319057.507917	37.985293
1996.251536	319562.011296	37.990311
1998.643764	320089.066270	37.995328
2000.692541	320601.979675	38.000346
2002.372260	321116.346621	38.005364
2004.238458	321625.473586	38.010381
2006.451695	322145.305405	38.015399
2007.620860	322679.295918	38.020416
2009.864344	323200.764843	38.025434
2011.594251	323715.534932	38.030452
2013.295725	324231.625913	38.035469
2015.518558	324734.804568	38.040487
2017.255800	325252.963390	38.045504
2018.733023	325757.932625	38.050522
2020.769033	326280.933950	38.055540
2022.318954	326800.634211	38.060557
2024.515136	327328.779716	38.065575
2025.952114	327875.097553	38.070592
2027.898843	328397.740065	38.075610
2029.895752	328945.580740	38.080628
2031.437763	329509.790793	38.085645
2033.451583	330060.893483	38.090663
2035.362535	330641.178743	38.095680
2037.345488	331207.051493	38.100698
2039.258671	331783.897582	38.105716
2040.983965	332355.589845	38.110733
2042.849399	332938.702750	38.115751
2044.666092	333536.110352	38.120768
2047.052737	334129.761915	38.125786
2049.587665	334720.488633	38.130804
2051.730593	335319.650978	38.135821
2053.775082	335909.887240	38.140839
2055.779379	336508.602374	38.145856
2057.687305	337116.922250	38.150874
2059.793064	337716.267117	38.155892
2062.677814	338308.495981	38.160909
2065.742509	338882.614948	38.165927
2068.355713	339473.250782	38.170944
2071.043412	340037.925540	38.175962
2073.575186	340611.097810	38.180980
2075.635373	341176.294974	38.185997
2077.915489	341734.367756	38.191015
2080.128006	342301.151657	38.196032
2082.268755	342853.320811	38.201050
2084.237334	343404.268483	38.206068
2086.373170	343966.629494	38.211085
2088.313132	344514.498219	38.216103
2090.622234	345077.731535	38.221120
2092.516074	345638.082582	38.226138
2094.519867	346200.642410	38.231156
2095.947935	346767.833567	38.236173
2098.130717	347331.238753	38.241191
2099.995881	347924.611982	38.246208
2101.874805	348513.229478	38.251226
2103.870792	349093.495920	38.256244
2105.710941	349682.967764	38.261261
2107.796113	350268.331078	38.266279
2109.671484	350870.140918	38.271296
2111.859508	351474.911084	38.276314
2114.007987	352082.572598	38.281332
2115.877148	352680.755559	38.286349
2118.090719	353282.324824	38.291367
2119.977748	353897.515924	38.296384
2121.957557	354508.115405	38.301402
2124.203141	355105.670234	38.306420
2126.044314	355732.769275	38.311437
2128.552864	356354.014383	38.316455
2130.556046	356981.651946	38.321472
2132.280548	357603.084145	38.326490
2134.688909	358225.028697	38.331508
2136.601265	358868.130859	38.336525
2138.597249	359489.845364	38.341543
2140.404952	360130.407831	38.346560
2142.639987	360761.527522	38.351578
2145.090485	361390.343798	38.356596
2147.317917	362031.492085	38.361613
2149.542046	362661.848079	38.366631
2152.051399	363283.977796	38.371648
2153.581595	363888.094290	38.376666
2156.069079	364484.787940	38.381684
2158.210574	365094.264898	38.386701
2160.424419	365697.809442	38.391719
2162.984218	366301.718780	38.396736
2164.715206	366908.418954	38.401754
2167.409336	367504.296271	38.406772
2169.164111	368114.879942	38.411789
2170.741365	368726.878204	38.416807
2173.176771	369342.149455	38.421824
2175.277299	369965.963402	38.426842
2177.624862	370578.768224	38.431860
2179.331559	371215.283496	38.436877
2181.672276	371837.986264	38.441895
2184.330683	372468.793318	38.446912
2185.936129	373110.872398	38.451930
2187.783026	373740.472210	38.456948
2189.829192	374396.836713	38.461965
2192.027776	375042.892236	38.466983
2194.891242	375683.348179	38.472000
2197.489277	376328.781766	38.477018
2199.832019	376967.803880	38.482036
2201.988521	377625.434308	38.487053
2204.391555	378256.941452	38.492071
2206.711498	378904.452675	38.497088
2208.975052	379548.385348	38.502106
2211.543418	380182.188224	38.507124
2213.847064	380841.964357	38.512141
2216.079480	381467.557171	38.517159
2218.515951	382112.071902	38.522176
2220.413839	382750.120979	38.527194
2223.003396	383398.262328	38.532212
2224.980069	384046.238481	38.537229
2227.283136	384691.004002	38.542247
2229.564537	385344.228878	38.547264
2231.481722	385987.916805	38.552282
2233.838639	386645.438628	38.557300
2235.716318	387318.161917	38.562317
2237.854053	387970.622128	38.567335
2240.069656	388635.047714	38.572352
2242.181675	389308.881910	38.577370
2244.451649	389973.447878	38.582388
2246.534277	390650.477777	38.587405
2249.098582	391318.541077	38.592423
2251.253948	392008.204448	38.597440
2253.367764	392694.513228	38.602458
2255.793266	393368.182536	38.607476
2257.373176	394062.077179	38.612493
2260.120873	394745.523192	38.617511
2261.982426	395438.883659	38.622528
2263.924417	396144.279579	38.627546
2266.389700	396837.812344	38.632564
2268.569179	397546.709683	38.637581
2270.465935	398253.178299	38.642599
2273.071028	398954.267073	38.647616
2275.240251	399659.440488	38.652634
2277.987775	400366.250129	38.657652
2280.377832	401072.341249	38.662669
2282.256656	401779.031567	38.667687
2284.991579	402491.645065	38.672704
2287.287360	403206.847192	38.677722
2289.994718	403896.573584	38.682740
2291.878064	404604.738842	38.687757
2294.407026	405314.781545	38.692775
2296.800004	406008.435439	38.697792
2298.485041	406711.842090	38.702810
2301.192300	407429.250547	38.707828
2303.233765	408132.587676	38.712845
2305.960045	408813.296646	38.717863
2308.377977	409478.053686	38.722880
2310.406374	410150.180112	38.727898
2313.037845	410814.995902	38.732916
2315.338062	411490.793465	38.737933
2317.283640	412160.426260	38.742951
2320.104486	412837.041311	38.747968
2321.970877	413530.641202	38.752986
2324.062229	414214.763223	38.758004
2326.392165	414875.880086	38.763021
2329.242470	415555.384226	38.768039
2331.800627	416233.373888	38.773056
2333.830039	416934.455350	38.778074
2335.959836	417608.300800	38.783092
2338.333943	418310.275868	38.788109
2340.255011	419007.975880	38.793127
2342.361008	419712.236014	38.798144
2344.501346	420427.613385	38.803162
2346.759888	421144.926262	38.808180
2348.803260	421861.291985	38.813197
2350.818313	422593.948935	38.818215
2353.712416	423331.984708	38.823232
2355.995105	424066.858454	38.828250
2358.469515	424796.918794	38.833268
2360.826301	425526.571823	38.838285
2363.288588	426268.844596	38.843303
2365.773284	427015.040562	38.848320
2367.887600	427779.401020	38.853338
2370.159811	428524.927390	38.858356
2372.935743	429280.119052	38.863373
2375.046264	430047.344716	38.868391
2377.805219	430799.605491	38.873408
2379.608887	431561.466685	38.878426
2382.011452	432326.697579	38.883444
2384.516620	433097.708107	38.888461
2386.901370	433871.750300	38.893479
2389.583791	434634.379443	38.898496
2391.817744	435411.381789	38.903514
2394.435223	436183.537092	38.908532
2397.016124	436959.215419	38.913549
2399.076766	437741.937566	38.918567
2401.766230	438519.620146	38.923584
2403.845821	439308.459651	38.928602
2406.709835	440083.023418	38.933620
2408.732607	440863.316263	38.938637
2410.689352	441662.416775	38.943655
2413.077219	442448.463994	38.948672
2415.376714	443255.951677	38.953690
2417.717393	444059.304804	38.958708
2419.867919	444869.996211	38.963725
2422.169804	445688.019243	38.968743
2424.897864	446512.821720	38.973760
2426.811671	447343.393097	38.978778
2429.404012	448155.204756	38.983796
2432.028961	448992.930552	38.988813
2434.059418	449825.916257	38.993831
2437.283985	450641.323309	38.998848
2439.507922	451478.309580	39.003866
2442.081899	452298.716917	39.008884
2444.651994	453126.780371	39.013901
2446.890808	453948.291251	39.018919
2449.848227	454774.607325	39.023936
2451.940668	455602.297394	39.028954
2454.254940	456442.256178	39.033972
2456.574845	457269.791390	39.038989
2459.007565	458103.291640	39.044007
2461.935278	458944.917722	39.049024
2464.993047	459754.635497	39.054042
2467.123244	460546.829489	39.059060
2469.802399	461331.621987	39.064077
2471.995287	462131.427675	39.069095
2474.773800	462909.974595	39.074112
2477.051959	463700.149312	39.079130
2479.516083	464478.585602	39.084148
2481.859658	465265.148874	39.089165
2484.404573	466081.215143	39.094183
2486.720689	466866.556417	39.099200
2488.693644	467680.477106	39.104218
2491.344928	468487.176834	39.109236
2493.681196	469305.416803	39.114253
2496.223161	470112.824820	39.119271
2499.405337	470922.064093	39.124288
2501.645606	471749.968266	39.129306
2503.998470	472567.662279	39.134324
2506.368453	473398.656557	39.139341
2508.658696	474241.500054	39.144359
2511.265566	475067.329772	39.149376
2513.714202	475898.908207	39.154394
2516.011272	476740.981729	39.159412
2518.652423	477584.324321	39.164429
2521.183126	478443.153396	39.169447
2523.770574	479292.336759	39.174464
2526.701503	480145.919318	39.179482
2528.806580	481003.386015	39.184500
2531.720120	481854.164613	39.189517
2534.147440	482729.222743	39.194535
2536.843751	483583.188022	39.199552
2539.203877	484444.843322	39.204570
2541.599358	485317.307065	39.209588
2544.216719	486188.934401	39.214605
2546.710102	487066.951307	39.219623
2549.108987	487942.315256	39.224640
2552.004884	488827.549214	39.229658
2554.690307	489715.145889	39.234676
2557.179869	490594.098591	39.239693
2559.798966	491472.632444	39.244711
2562.440573	492349.301322	39.249728
2564.817990	493262.659854	39.254746
2567.246975	494150.476512	39.259764
2569.788561	495047.059833	39.264781
2572.280748	495945.521899	39.269799
2575.003762	496846.471985	39.274816
2577.793892	497747.312827	39.279834
2580.408588	498637.691064	39.284852
2583.617137	499526.814543	39.289869
2586.484340	500437.387205	39.294887
2589.021833	501326.778143	39.299904
2591.429069	502235.411788	39.304922
2593.749420	503127.062663	39.309940
2596.313567	504026.644658	39.314957
2598.393212	504943.707344	39.319975
2601.298449	505846.462242	39.324992
2603.577365	506761.171497	39.330010
2606.279817	507676.112591	39.335028
2609.045362	508582.672117	39.340045
2611.965104	509495.659488	39.345063
2615.117512	510399.733938	39.350080
2617.743056	511304.348454	39.355098
2620.381485	512203.263705	39.360116
2623.603144	513113.373852	39.365133
2626.407188	514003.389128	39.370151
2628.867522	514889.983644	39.375168
2631.569471	515781.679585	39.380186
2633.798095	516688.723394	39.385204
2636.814325	517564.038537	39.390221
2640.019271	518440.180460	39.395239
2642.908000	519273.646589	39.400256
2645.698125	520123.862364	39.405274
2648.448328	520940.231275	39.410292
2651.278320	521772.665227	39.415309
2653.677103	522604.167889	39.420327
2655.696959	523440.624443	39.425344
2658.031876	524285.344796	39.430362
2660.100620	525125.377734	39.435380
2662.969510	525972.837393	39.440397
2666.354628	526811.501889	39.445415
2668.905378	527655.746363	39.450432
2671.494302	528519.928821	39.455450
2673.713859	529370.727872	39.460468
2675.970971	530247.403111	39.465485
2678.203841	531129.015026	39.470503
2680.679316	532013.202682	39.475520
2683.426875	532898.097898	39.480538
2685.404400	533798.067816	39.485556
2688.104888	534705.514323	39.490573
2690.623011	535623.554677	39.495591
2693.112942	536547.027622	39.500608
2695.357011	537476.923995	39.505626
2697.742184	538445.888676	39.510644
2700.220032	539395.248685	39.515661
2702.146512	540360.536668	39.520679
2704.650060	541340.405986	39.525696
2707.675356	542321.832319	39.530714
2710.400634	543311.339385	39.535732
2713.577480	544289.887628	39.540749
2716.634545	545299.522583	39.545767
2719.265201	546285.164209	39.550784
2722.695673	547272.766982	39.555802
2725.313711	548264.858906	39.560820
2728.272844	549276.736300	39.565837
2731.341659	550267.805760	39.570855
2734.016307	551273.650324	39.575872
2737.028359	552268.506409	39.580890
2739.646719	553269.789486	39.585908
2742.820649	554250.851132	39.590925
2745.500540	555250.419883	39.595943
2747.659505	556251.759643	39.600960
2750.772878	557260.807978	39.605978
2753.296681	558272.239428	39.610996
2755.972183	559277.187963	39.616013
2758.771444	560301.333886	39.621031
2761.022654	561325.893067	39.626048
2764.026144	562350.801534	39.631066
2766.692953	563388.695875	39.636084
2769.562274	564418.388148	39.641101
2771.528828	565462.411811	39.646119
2774.196033	566513.066353	39.651136
2777.079150	567557.725121	39.656154
2779.893044	568625.810107	39.661172
2783.017234	569656.250459	39.666189
2785.525009	570721.149452	39.671207
2788.202302	571768.312013	39.676224
2791.519968	572827.329988	39.681242
2794.168376	573883.659755	39.686260
2797.035148	574929.025125	39.691277
2799.715886	576005.498064	39.696295
2802.388568	577060.604621	39.701312
2805.512970	578122.321460	39.706330
2808.226997	579197.360886	39.711348
2811.553111	580248.578642	39.716365
2814.395039	581306.458564	39.721383
2817.098670	582361.612436	39.726400
2819.987996	583422.814120	39.731418
2822.061911	584477.238284	39.736436
2825.059619	585502.285621	39.741453
2828.180394	586541.215538	39.746471
2830.606769	587568.188653	39.751488
2833.481058	588606.681490	39.756506
2835.904095	589626.411829	39.761524
2838.928086	590656.332134	39.766541
2841.546041	591696.906125	39.771559
2844.477222	592738.139727	39.776576
2847.521528	593774.503242	39.781594
2849.914459	594832.178377	39.786612
2852.692143	595876.218460	39.791629
2855.836090	596931.427528	39.796647
2858.986515	597961.394662	39.801664
2862.823614	599005.433005	39.806682
2865.819877	600065.543079	39.811700
2868.865678	601098.305769	39.816717
2871.540453	602153.170332	39.821735
2874.539397	603208.235720	39.826752
2877.301304	604259.839168	39.831770
2879.917379	605325.387208	39.836788
2882.883240	606376.312405	39.841805
2885.917730	607445.297955	39.846823
2888.530987	608516.204242	39.851840
2891.687714	609572.658012	39.856858
2893.983522	610651.371157	39.861876
2896.998040	611732.564274	39.866893
2900.064663	612822.699540	39.871911
2902.495420	613911.132612	39.876928
2905.356631	615003.689996	39.881946
2908.222081	616107.742112	39.886964
2911.123092	617210.328131	39.891981
2914.085215	618324.244461	39.896999
2917.169535	619433.878124	39.902016
2919.938288	620544.751300	39.907034
2923.187386	621663.130409	39.912052
2926.873617	622762.529488	39.917069
2930.282454	623859.763912	39.922087
2933.774515	624961.920507	39.927104
2936.761588	626049.207601	39.932122
2939.858498	627160.847808	39.937140
2942.864060	628240.915242	39.942157
2945.394444	629336.686464	39.947175
2948.341723	630438.519519	39.952192
2951.351643	631543.074515	39.957210
2954.439616	632650.497484	39.962228
2957.420132	633753.328131	39.967245
2959.805411	634869.820685	39.972263
2962.391534	635984.563770	39.977280
2965.286231	637096.042354	39.982298
2967.674047	638222.059295	39.987316
2970.620930	639362.084513	39.992333
2974.342956	640482.046785	39.997351
2977.335212	641602.656249	40.002368
2980.511426	642724.809397	40.007386
2983.356185	643872.733038	40.012404
2986.185484	644997.836532	40.017421
2989.108727	646136.265294	40.022439
2991.461558	647294.955397	40.027456
2994.393723	648441.451096	40.032474
2997.587021	649605.471415	40.037492
3000.904706	650738.829518	40.042509
3004.262883	651875.142927	40.047527
3006.518590	653030.247214	40.052544
3009.863853	654172.580260	40.057562
3012.687528	655345.061633	40.062580
3015.721057	656492.061373	40.067597
3018.625925	657647.566555	40.072615
3021.521276	658795.067874	40.077632
3024.441330	659921.613633	40.082650
3027.293488	661048.538587	40.087668
3030.926543	662145.479664	40.092685
3033.753846	663268.466863	40.097703
3036.883710	664386.992918	40.102720
3039.568092	665495.259220	40.107738
3042.334455	666625.779587	40.112756
3045.220409	667752.862727	40.117773
3048.058736	668888.179753	40.122791
3050.601368	670041.867309	40.127808
3053.821984	671178.838025	40.132826
3056.648662	672342.645095	40.137844
3059.526567	673512.914542	40.142861
3062.856038	674679.035835	40.147879
3066.037343	675859.504780	40.152896
3068.931007	677034.602637	40.157914
3071.851433	678225.354578	40.162932
3074.566332	679427.021205	40.167949
3077.716366	680617.875671	40.172967
3080.335298	681821.980203	40.177984
3083.470663	683046.310478	40.183002
3086.378431	684280.449660	40.188020
3089.494433	685515.381418	40.193037
3092.369922	686759.571337	40.198055
3095.243838	688018.735460	40.203072
3098.409755	689252.654796	40.208090
3101.767909	690522.511406	40.213108
3104.599597	691794.757256	40.218125
3107.469931	693057.040193	40.223143
3110.784802	694339.663337	40.228160
3113.805008	695630.683589	40.233178
3117.716121	696907.182787	40.238196
3120.608596	698189.914988	40.243213
3124.115697	699461.747393	40.248231
3128.043961	700747.606264	40.253248
3131.054925	702016.621777	40.258266
3134.407141	703296.004385	40.263284
3137.313612	704582.954469	40.268301
3140.867350	705858.309120	40.273319
3143.708994	707165.698895	40.278336
3146.526481	708452.534379	40.283354
3150.114023	709742.121416	40.288372
3153.394011	711023.690922	40.293389
3156.932936	712309.531554	40.298407
3160.135428	713608.699839	40.303424
3163.297057	714880.846595	40.308442
3166.839592	716175.753903	40.313460
3169.655145	717466.672878	40.318477
3172.827182	718749.220586	40.323495
3175.963476	720050.030570	40.328512
3178.798555	721348.362983	40.333530
3182.377861	722624.412343	40.338548
3185.665529	723920.636679	40.343565
3189.039284	725222.527237	40.348583
3191.979732	726517.610491	40.353600
3195.287425	727811.144364	40.358618
3198.122973	729109.790153	40.363636
3201.040309	730427.090270	40.368653
3203.949362	731731.087715	40.373671
3206.437847	733054.158875	40.378688
3209.326150	734380.553119	40.383706
3212.582600	735729.085602	40.388724
3215.450746	737068.076171	40.393741
3219.754949	738395.747522	40.398759
3223.226527	739721.904344	40.403776
3227.073395	741046.643784	40.408794
3230.384253	742361.975628	40.413812
3233.209371	743665.527903	40.418829
3236.496871	744934.216235	40.423847
3239.897545	746214.318882	40.428864
3243.517171	747479.484368	40.433882
3246.708543	748740.029987	40.438900
3249.934365	750002.879926	40.443917
3253.086083	751261.101947	40.448935
3256.058247	752538.759348	40.453952
3259.064499	753805.460745	40.458970
3262.192604	755088.779131	40.463988
3264.995947	756380.850416	40.469005
3268.045747	757676.553127	40.474023
3270.926842	758980.580697	40.479040
3273.988877	760290.606383	40.484058
3277.220844	761613.911645	40.489076
3280.038691	762948.518426	40.494093
3283.172214	764279.492020	40.499111
3286.439118	765640.507160	40.504128
3289.261395	766988.710057	40.509146
3292.365889	768356.241764	40.514164
3295.278951	769757.080936	40.519181
3298.887859	771142.403285	40.524199
3302.102753	772540.652141	40.529216
3305.472713	773932.223670	40.534234
3308.704209	775345.856484	40.539252
3312.035728	776767.697044	40.544269
3315.098091	778192.006289	40.549287
3318.411930	779620.119800	40.554304
3321.914795	781051.357477	40.559322
3325.640363	782477.908178	40.564340
3329.287805	783910.617405	40.569357
3333.010980	785340.478213	40.574375
3336.586254	786770.470851	40.579392
3340.279074	788209.622019	40.584410
3343.764281	789642.241742	40.589428
3347.053250	791075.438326	40.594445
3350.568005	792503.701370	40.599463
3353.708385	793948.395669	40.604480
3357.004505	795384.979286	40.609498
3360.639591	796818.323520	40.614516
3363.898540	798256.283623	40.619533
3368.009209	799699.534717	40.624551
3372.533530	801112.904301	40.629568
3376.580743	802521.611125	40.634586
3380.505351	803930.099849	40.639604
3383.612062	805331.782851	40.644621
3387.395665	806709.251503	40.649639
3390.748858	808106.707687	40.654656
3393.855936	809497.025533	40.659674
3397.656781	810866.221975	40.664692
3401.225753	812267.480370	40.669709
3404.327983	813639.554238	40.674727
3407.829957	815025.790274	40.679744
3411.271842	816406.378599	40.684762
3414.629219	817780.446968	40.689780
3417.696001	819156.868020	40.694797
3421.452686	820536.210003	40.699815
3424.407925	821934.183764	40.704832
3427.682498	823319.857831	40.709850
3430.688365	824717.088955	40.714868
3433.683853	826121.876463	40.719885
3437.614689	827512.412247	40.724903
3441.324320	828918.774401	40.729920
3444.285439	830325.005647	40.734938
3447.572278	831717.773285	40.739956
3450.723750	833131.307775	40.744973
3453.929252	834550.222639	40.749991
3457.037866	835977.264830	40.755008
3460.758369	837367.032728	40.760013
3464.854786	838700.470938	40.765018
3468.866238	839985.202780	40.770023
3472.245795	841202.471202	40.775028
3475.502208	842367.542943	40.780032
3477.921513	843438.632428	40.785037
3481.417988	844443.259018	40.790042
3484.105686	845391.123115	40.795047
3486.608324	846278.833278	40.800052
3489.201388	847076.546980	40.805056
3491.357290	847829.016106	40.810061
3493.865569	848514.106134	40.815066
3495.800016	849146.508148	40.820071
3497.669297	849696.441815	40.825076
3499.531428	850197.915545	40.830080
3501.073759	850646.414503	40.835085
3502.871059	851042.439798	40.840090
3504.304582	851404.510315	40.845095
3505.670661	851716.222238	40.850100
3506.830822	851994.063541	40.855104
3508.082734	852226.791204	40.860109
3509.471863	852399.309557	40.865114
3510.084182	852558.903043	40.870119
3511.309538	852674.769159	40.875124
3511.988472	852761.804231	40.880128
3513.087745	852813.131761	40.885133
3514.137797	852837.982666	40.890138
3514.871217	852847.696103	40.895143
3515.823222	852809.857430	40.900148
3516.967362	852729.338673	40.905152
3517.755542	852638.166586	40.910157
3518.546100	852527.420664	40.915162
3518.845948	852409.353051	40.920167
3519.422757	852254.720901	40.925172
3519.792449	852095.055238	40.930176
3520.019772	851906.583469	40.935181
3520.713004	851710.530496	40.940186
3520.692182	851503.876096	40.945191
3521.376347	851286.677660	40.950196
3521.320907	851033.361835	40.955200
3521.401397	850796.766308	40.960205
3521.584615	850539.495089	40.965210
3521.632550	850284.086324	40.970215
3521.677035	850015.322111	40.975220
3521.794950	849753.645704	40.980224
3521.726823	849471.627925	40.985229
3521.845915	849193.171358	40.990234
3522.015582	848904.269041	40.995239
3522.031117	848608.948087	41.000244
3522.066071	848304.743020	41.005248
3522.236422	848020.671858	41.010253
3522.470733	847698.377383	41.015258
3521.676665	847401.281404	41.020263
3522.133575	847097.727989	41.025268
3522.037446	846787.720988	41.030272
3522.204288	846454.847847	41.035277
3522.043639	846143.162767	41.040282
3521.922807	845829.506150	41.045287
3522.263687	845504.839789	41.050292
3521.901845	845174.910626	41.055296
3521.580660	844862.603770	41.060301
3521.841600	844535.170916	41.065306
3521.627232	844219.792260	41.070311
3521.375617	843889.777837	41.075316
3521.211089	843568.654299	41.080320
3520.964204	843251.038688	41.085325
3521.037688	842928.234449	41.090330
3520.696130	842622.354418	41.095335
3520.971102	842301.045528	41.100340
3520.872238	841983.780991	41.105344
3520.378982	841666.175407	41.110349
3520.546162	841350.396116	41.115354
3520.358427	841034.123082	41.120359
3520.058950	840708.828746	41.125364
3520.221737	840390.905134	41.130368
3520.271163	840094.448947	41.135373
3520.017339	839768.123436	41.140378
3519.889366	839467.910877	41.145383
3519.447629	839148.219788	41.150388
3519.327750	838843.243887	41.155392
3519.263148	838542.538298	41.160397
3519.497076	838227.666996	41.165402
3519.177873	837934.879973	41.170407
3518.875700	837616.943787	41.175412
3518.801035	837333.117366	41.180416
3518.506861	837026.863603	41.185421
3518.418714	836736.082480	41.190426
3518.255018	836449.254324	41.195431
3518.326170	836150.854799	41.200436
3517.939097	835853.005064	41.205440
3517.686070	835582.213205	41.210445
3517.803310	835293.529832	41.215450
3518.026572	835008.184773	41.220455
3517.577365	834726.892593	41.225460
3517.531106	834441.762169	41.230464
3517.317465	834156.939693	41.235469
3517.328624	833884.568199	41.240474
3517.174734	833599.515990	41.245479
3516.851364	833313.062930	41.250484
3516.801710	833033.731105	41.255488
3516.491760	832781.389077	41.260493
3516.534822	832503.386591	41.265498
3516.260939	832248.233940	41.270503
3515.969696	831975.050443	41.275508
3516.124470	831711.649017	41.280512
3515.800732	831458.036599	41.285517
3515.696898	831196.903929	41.290522
3515.687542	830945.515703	41.295527
3515.613938	830692.369587	41.300532
3515.761317	830437.564971	41.305536
3515.415269	830184.834841	41.310541
3515.701339	829940.590150	41.315546
3515.170170	829695.493680	41.320551
3515.134485	829448.791610	41.325556
3515.025187	829209.959678	41.330560
3514.854039	828961.502344	41.335565
3514.880656	828715.593049	41.340570
3514.859506	828486.640577	41.345575
3514.486264	828240.241680	41.350580
3514.273356	827996.055318	41.355584
3514.050608	827776.886104	41.360589
3514.278673	827544.242770	41.365594
3514.061624	827314.157354	41.370599
3513.978171	827080.180229	41.375604
3514.184562	826845.169353	41.380608
3513.812164	826614.449491	41.385613
3513.703834	826387.197851	41.390618
3513.603826	826170.154602	41.395623
3513.342488	825954.695227	41.400628
3513.717990	825735.652610	41.405632
3513.051481	825510.809382	41.410637
3513.498913	825286.117252	41.415642
3513.045145	825080.244278	41.420647
3513.090172	824860.884710	41.425652
3513.296055	824653.373910	41.430656
3512.567864	824447.673061	41.435661
3512.774089	824225.625152	41.440666
3512.783297	824025.657986	41.445671
3512.386161	823818.415858	41.450676
3512.767720	823607.468743	41.455680
3512.300663	823399.246833	41.460685
3512.267790	823201.755996	41.465690
3512.023204	823005.908214	41.470695
3511.788038	822804.917209	41.475700
3511.719179	822609.468963	41.480704
3511.635236	822432.311979	41.485709
3511.876379	822231.029434	41.490714
3511.722461	822048.737397	41.495719
3511.262067	821850.640723	41.500724
3511.239063	821670.469205	41.505728
3511.177538	821490.641599	41.510733
3511.339144	821308.815403	41.515738
3511.109332	821130.033152	41.520743
3510.792179	820947.003843	41.525748
3510.766178	820770.722541	41.530752
3510.800020	820591.784520	41.535757
3510.691917	820418.638886	41.540762
3510.458547	820248.836749	41.545767
3510.374385	820081.794892	41.550772
3510.665471	819899.370556	41.555776
3510.589835	819732.122783	41.560781
3510.189372	819557.975263	41.565786
3510.013738	819403.704008	41.570791
3509.804031	819237.493601	41.575796
3510.130025	819065.415825	41.580800
3509.756858	818908.914388	41.585805
3509.863831	818753.798481	41.590810
3509.696204	818598.479480	41.595815
3509.833922	818437.526818	41.600820
3509.837121	818276.984008	41.605824
3509.330955	818136.198134	41.610829
3509.728935	817982.827449	41.615834
3509.599837	817824.547195	41.620839
3509.393558	817673.031124	41.625844
3509.606415	817525.358738	41.630848
3509.085286	817384.755309	41.635853
3509.087429	817222.229236	41.640858
3508.916348	817086.163563	41.645863
3508.981261	816934.145501	41.650868
3508.951569	816795.406998	41.655872
3508.511369	816649.536371	41.660877
3508.541189	816505.053933	41.665882
3508.511119	816375.364274	41.670887
3508.517887	816232.887143	41.675892
3508.780897	816095.603755	41.680896
3508.377004	815964.156116	41.685901
3508.593974	815814.486838	41.690906
3508.498217	815692.727038	41.695911
3508.016972	815559.178703	41.700916
3508.257516	815433.441511	41.705920
3508.236243	815299.224641	41.710925
3507.867048	815166.384564	41.715930
3508.185192	815031.616757	41.720935
3507.751257	814901.034726	41.725940
3507.960560	814783.517666	41.730944
3507.627224	814665.451287	41.735949
3507.822340	814526.726845	41.740954
3507.567416	814414.373076	41.745959
3507.645516	814300.395367	41.750964
3507.535945	814178.708392	41.755968
3507.448692	814061.668375	41.760973
3507.580896	813939.055662	41.765978
3507.296029	813836.541769	41.770983
3507.098804	813718.583313	41.775988
3507.582955	813596.641104	41.780992
3506.990183	813483.445816	41.785997
3506.776058	813369.255598	41.791002
3506.867678	813267.062897	41.796007
3506.859388	813158.811131	41.801012
3507.119128	813053.207629	41.806016
3506.847915	812947.934857	41.811021
3507.040083	812837.146674	41.816026
3507.278830	812727.818609	41.821031
3506.721289	812625.135284	41.826036
3506.897033	812505.330653	41.831040
3506.747812	812415.362856	41.836045
3506.838673	812299.977587	41.841050
3506.743928	812204.070225	41.846055
3506.736964	812086.639827	41.851060
3506.951578	811986.171208	41.856064
3506.496367	811880.667168	41.861069
3506.806289	811777.583131	41.866074
3506.306207	811682.372061	41.871079
3505.934823	811587.089458	41.876084
3506.246619	811491.594996	41.881088
3506.016061	811399.373290	41.886093
3506.347382	811305.587870	41.891098
3506.164050	811214.825789	41.896103
3506.284590	811103.041085	41.901108
3506.534555	811014.850883	41.906112
3506.041748	810939.913826	41.911117
3506.096356	810835.779537	41.916122
3505.987235	810745.684965	41.921127
3506.155346	810651.133369	41.926132
3506.201710	810551.994274	41.931136
3505.971592	810459.759725	41.936141
3506.017224	810368.899616	41.941146
3505.973360	810280.650274	41.946151
3505.934161	810195.437336	41.951156
3505.858856	810106.259811	41.956160
3505.492288	810017.374122	41.961165
3505.661817	809928.496984	41.966170
3505.823937	809845.304795	41.971175
3505.599597	809757.029376	41.976180
3505.773338	809652.318245	41.981184
3505.192127	809584.536104	41.986189
3505.653363	809509.034038	41.991194
3505.697812	809430.071022	41.996199
3505.673495	809340.237921	42.001204
3505.408803	809262.255092	42.006208
3505.392548	809197.365760	42.011213
3505.691040	809098.556056	42.016218
3505.392893	809021.066106	42.021223
3505.182701	808943.952900	42.026228
3505.376219	808860.449428	42.031232
3505.291134	808779.245528	42.036237
3505.048493	808699.144962	42.041242
3505.116855	808631.540432	42.046247
3505.062236	808557.632311	42.051252
3505.320192	808488.622664	42.056256
3505.212789	808413.202134	42.061261
3505.091482	808341.900611	42.066266
3505.055797	808262.447087	42.071271
3504.982373	808191.283161	42.076276
3504.907650	808111.981374	42.081280
3504.774925	808043.962966	42.086285
3504.775660	807969.304049	42.091290
3504.506359	807895.375097	42.096295
3504.631058	807836.283178	42.101300
3504.742944	807765.966695	42.106304
3504.761336	807708.557951	42.111309
3504.665362	807634.401534	42.116314
3504.470854	807582.419383	42.121319
3504.485128	807512.018318	42.126324
3504.648918	807437.375759	42.131328
3504.565665	807373.607698	42.136333
3504.684357	807306.668124	42.141338
3504.737817	807251.210800	42.146343
3504.337408	807178.080103	42.151348
3504.367300	807122.478537	42.156352
3504.778599	807060.047884	42.161357
3504.654112	806997.802970	42.166362
3504.515137	806928.499762	42.171367
3504.378317	806863.755201	42.176372
3504.537600	806797.245223	42.181376
3504.494650	806737.926287	42.186381
3504.568911	806668.879509	42.191386
3504.574903	806607.443072	42.196391
3504.146560	806552.843944	42.201396
3504.292518	806479.468694	42.206400
3504.206835	806435.354019	42.211405
3503.901680	806374.358998	42.216410
3504.068813	806321.376082	42.221415
3503.882525	806250.749920	42.226420
3504.328972	806211.008194	42.231424
3504.085512	806149.755844	42.236429
3503.907773	806091.924542	42.241434
3504.158759	806046.182803	42.246439
3503.901242	805984.391906	42.251444
3504.009398	805918.421214	42.256448
3503.654930	805881.947797	42.261453
3503.900999	805826.054926	42.266458
3503.657368	805782.011099	42.271463
3503.267640	805728.232663	42.276468
3503.203412	805678.666457	42.281472
3503.406137	805640.530777	42.286477
3504.022559	805591.293171	42.291482
3503.554489	805541.154994	42.296487
3503.392139	805493.908425	42.301492
3503.526808	805447.740510	42.306496
3503.505587	805404.393214	42.311501
3503.568892	805358.138373	42.316506
3503.394376	805310.745428	42.321511
3503.215956	805268.943414	42.326516
3503.419725	805230.854331	42.331520
3503.263127	805201.946013	42.336525
3503.349963	805154.263737	42.341530
3503.765460	805105.349997	42.346535
3503.030032	805065.256862	42.351540
3503.427550	805033.804472	42.356544
3503.369181	804981.878250	42.361549
3503.187054	804933.306936	42.366554
3503.397510	804892.909867	42.371559
3503.174354	804849.788506	42.376564
3503.382197	804798.356528	42.381568
3503.189152	804765.676004	42.386573
3503.399012	804711.839889	42.391578
3503.084097	804679.326161	42.396583
3502.954348	804651.784356	42.401588
3503.189613	804615.844655	42.406592
3503.176755	804577.101004	42.411597
3503.284857	804525.879602	42.416602
3503.134086	804494.662198	42.421607
3502.985319	804466.926602	42.426612
3503.105791	804421.735063	42.431616
3502.815174	804385.978875	42.436621
3503.260971	804344.607938	42.441626
3502.977855	804318.021952	42.446631
3502.848809	804274.096724	42.451636
3503.016425	804236.351428	42.456640
3502.830356	804197.339882	42.461645
3502.876426	804164.813309	42.466650
3502.347211	804125.514538	42.471655
3502.543737	804111.110889	42.476660
3502.852237	804065.248409	42.481664
3502.558856	804040.526904	42.486669
3503.245338	804013.878137	42.491674
3502.975895	803987.435769	42.496679
3502.766422	803957.157538	42.501684
3503.218736	803916.665859	42.506688
3502.767281	803890.253097	42.511693
3503.047167	803849.936578	42.516698
3502.793573	803832.074846	42.521703
3502.780539	803796.858483	42.526708
3503.066448	803762.083213	42.531712
3502.815761	803723.521087	42.536717
3502.879485	803690.646009	42.541722
3502.804756	803656.665385	42.546727
3502.569442	803632.619577	42.551732
3502.718423	803592.470272	42.556736
3502.741552	803578.731755	42.561741
3502.761985	803533.550872	42.566746
3502.548647	803510.433021	42.571751
3502.659045	803478.873677	42.576756
3502.688695	803439.282721	42.581760
3502.262809	803434.104122	42.586765
3502.783710	803374.761390	42.591770
3502.884799	803350.462972	42.596775
3502.637340	803336.670434	42.601780
3502.905798	803299.001508	42.606784
3502.513995	803267.278642	42.611789
3502.707841	803239.334505	42.616794
3502.461289	803209.500590	42.621799
3502.209837	803187.418090	42.626804
3502.491901	803155.534661	42.631808
3502.275347	803137.615970	42.636813
3502.388380	803116.405265	42.641818
3502.163089	803084.997523	42.646823
3502.182026	803065.224784	42.651828
3502.407288	803044.436878	42.656832
3502.151726	803037.709178	42.661837
3502.314323	803014.086234	42.666842
3502.242754	802982.162139	42.671847
3502.358014	802970.614790	42.676852
3502.388554	802943.039751	42.681856
3502.279811	802928.978263	42.686861
3502.273097	802902.439398	42.691866
3502.174234	802876.994873	42.696871
3502.184320	802856.290901	42.701876
3502.428553	802827.944341	42.706880
3502.018945	802813.098190	42.711885
3502.319133	802791.561314	42.716890
3502.344783	802771.394163	42.721895
3501.809591	802744.745505	42.726900
3502.059352	802731.164206	42.731904
3502.187842	802715.542394	42.736909
3502.275935	802696.591205	42.741914
3502.492929	802669.425893	42.746919
3502.284736	802656.116114	42.751924
3502.309357	802634.575079	42.756928
3502.078693	802611.309890	42.761933
3502.056337	802599.343053	42.766938
3502.319251	802568.441261	42.771943
3502.001820	802545.288260	42.776948
3502.529764	802521.554397	42.781952
3502.112708	802513.430043	42.786957
3502.203629	802495.409979	42.791962
3502.106418	802462.898985	42.796967
3501.927089	802448.553782	42.801972
3502.264474	802436.821774	42.806977
3502.098761	802409.669418	42.811981
3502.216693	802396.354481	42.816986
3501.740566	802361.697683	42.821991
3501.984552	802352.630218	42.826996
3502.110932	802333.033931	42.832001
3502.198885	802323.746822	42.837005
3502.103461	802295.699335	42.842010
3501.935341	802281.646308	42.847015
3501.745980	802275.005080	42.852020
3502.242992	802258.045930	42.857025
3502.336844	802246.991519	42.862029
3502.197540	802210.463190	42.867034
3502.478052	802194.618914	42.872039
3502.071077	802171.871907	42.877044
3502.501981	802153.059015	42.882049
3501.999018	802122.232318	42.887053
3501.924880	802109.193780	42.892058
3502.119427	802090.615901	42.897063
3502.081579	802075.069105	42.902068
3502.336414	802054.126166	42.907073
3502.271535	802038.142169	42.912077
3502.318907	802012.768502	42.917082
3502.179211	801987.916193	42.922087
3502.294386	801971.608003	42.927092
3502.094006	801957.216182	42.932097
3502.196200	801934.826104	42.937101
3501.975426	801915.482073	42.942106
3502.121482	801900.297107	42.947111
3501.862426	801884.197545	42.952116
3502.198895	801859.511667	42.957121
3501.973663	801846.595650	42.962125
3501.934749	801822.560248	42.967130
3502.023383	801812.241977	42.972135
3501.886547	801792.834712	42.977140
3502.056849	801773.180542	42.982145
3501.858959	801761.535561	42.987149
3501.788711	801732.500335	42.992154
3502.052779	801719.405355	42.997159
3501.482049	801720.529718	43.002164
3501.774240	801701.002464	43.007169
3501.761107	801688.100282	43.012173
3501.864752	801675.571368	43.017178
3501.559705	801666.249978	43.022183
3501.655455	801658.187344	43.027188
3501.813760	801639.761425	43.032193
3501.882430	801624.490469	43.037197
3502.124914	801613.459632	43.042202
3501.983163	801594.003553	43.047207
3501.782756	801577.697349	43.052212
3501.916781	801569.333908	43.057217
3501.895553	801558.591754	43.062221
3501.899574	801542.840599	43.067226
3501.819733	801526.710684	43.072231
3501.689333	801519.715547	43.077236
3501.730765	801504.645082	43.082241
3501.833708	801489.270049	43.087245
3501.817560	801481.912584	43.092250
3501.868227	801473.709960	43.097255
3501.699436	801448.615169	43.102260
3502.049047	801443.454528	43.107265
3502.085721	801430.052984	43.112269
3501.571160	801401.482096	43.117274
3501.963966	801394.106246	43.122279
3501.615250	801387.392274	43.127284
3502.088041	801368.668496	43.132289
3501.933176	801354.415128	43.137293
3501.825554	801340.939043	43.142298
3502.099819	801323.474551	43.147303
3501.737938	801311.610480	43.152308
3502.050516	801287.269983	43.157313
3501.929119	801289.448980	43.162317
3502.042493	801266.417008	43.167322
3501.988169	801245.522551	43.172327
3501.985587	801242.382534	43.177332
3502.103132	801220.527380	43.182337
3501.902495	801201.963144	43.187341
3501.692914	801194.342818	43.192346
3501.481481	801174.210064	43.197351
3501.644557	801153.770217	43.202356
3501.631910	801144.694378	43.207361
3501.638450	801146.312580	43.212365
3501.690569	801146.990949	43.217370
3501.853978	801135.825170	43.222375
3501.956110	801108.967080	43.227380
3501.994882	801099.882713	43.232385
3501.969955	801102.242159	43.237389
3502.101971	801065.957522	43.242394
3502.055681	801054.728012	43.247399
3501.932507	801040.370636	43.252404
3501.954044	801010.139573	43.257409
3502.114490	800996.618664	43.262413
3501.950020	800972.797278	43.267418
3502.049416	800969.640340	43.272423
3501.680649	800963.321825	43.277428
3501.778459	800939.751551	43.282433
3501.895963	800917.306595	43.287437
3501.930923	800905.523675	43.292442
3502.287660	800894.129379	43.297447
3502.195621	800882.465482	43.302452
3501.722034	800859.283480	43.307457
3501.845750	800852.196740	43.312461
3502.002669	800833.916126	43.317466
3502.143817	800815.736206	43.322471
3501.943745	800804.139043	43.327476
3502.040765	800778.507320	43.332481
3501.655052	800773.418230	43.337485
3501.816124	800772.312085	43.342490
3501.855862	800746.444316	43.347495
3501.880819	800738.735784	43.352500
3501.962201	800729.300405	43.357505
3501.705274	800719.430010	43.362509
3501.676357	800695.241833	43.367514
3501.950506	800690.338432	43.372519
3501.420903	800686.843313	43.377524
3501.706773	800687.973956	43.382529
3501.232391	800656.547138	43.387533
3501.273628	800633.623094	43.392538
3501.818931	800632.797153	43.397543
3501.317922	800650.840487	43.402548
3501.674345	800644.156865	43.407553
3501.696173	800644.447687	43.412557
3501.550534	800623.713617	43.417562
3501.913022	800604.907806	43.422567
3501.998813	800600.526103	43.427572
3502.012474	800588.746154	43.432577
3501.908632	800560.742101	43.437581
3501.956762	800552.146214	43.442586
3502.111090	800542.355049	43.447591
3501.788735	800515.908101	43.452596
3501.933768	800501.947101	43.457601
3501.849770	800497.004407	43.462605
3501.872345	800465.200420	43.467610
3502.010225	800450.995123	43.472615
3501.762316	800452.557249	43.477620
3502.131669	800428.891440	43.482625
3502.046717	800418.550615	43.487629
3501.946539	800401.292708	43.492634
3502.204982	800383.681239	43.497639
3502.293291	800365.705146	43.502644
3502.129221	800351.058627	43.507649
3502.027391	800319.029085	43.512653
3502.062520	800308.619242	43.517658
3502.031787	800288.159696	43.522663
3501.328147	800267.074786	43.527668
3501.764202	800248.599429	43.532673
3501.936525	800251.957272	43.537677
3501.639705	800227.566213	43.542682
3502.097261	800218.558943	43.547687
3501.777323	800211.593702	43.552692
3502.144570	800191.117395	43.557697
3502.058287	800175.623393	43.562701
3501.919659	800172.946990	43.567706
3501.980306	800153.208144	43.572711
3501.886173	800140.807193	43.577716
3502.246537	800111.203483	43.582721
3502.084653	800095.525446	43.587725
3501.882794	800067.731857	43.592730
3502.029354	800066.775225	43.597735
3502.169868	800061.942473	43.602740
3501.814212	800039.670772	43.607745
3502.056927	800030.894958	43.612749
3501.764139	800007.238624	43.617754
3502.044919	799996.198918	43.622759
3502.359376	799995.410932	43.627764
3502.436846	799958.982265	43.632769
3502.105276	799957.908059	43.637773
3502.111254	799926.153417	43.642778
3502.066474	799901.228912	43.647783
3502.107994	799894.498286	43.652788
3501.801435	799859.113921	43.657793
3502.003300	799861.387355	43.662797
3501.812873	799851.799240	43.667802
3502.051125	799825.993506	43.672807
3501.809144	799823.137674	43.677812
3501.482559	799811.903242	43.682817
3501.717498	799811.324651	43.687821
3501.895657	799791.172790	43.692826
3501.941354	799766.380137	43.697831
3502.126249	799766.987694	43.702836
3501.944522	799737.373525	43.707841
3501.785264	799721.301572	43.712845
3501.867950	799711.521040	43.717850
3501.746771	799704.571629	43.722855
3501.597338	799678.829206	43.727860
3501.902310	799646.778640	43.732865
3502.038094	799661.823902	43.737869
3501.927289	799636.222199	43.742874
3501.805530	799616.462795	43.747879
3501.539993	799621.267322	43.752884
3501.902111	799608.888432	43.757889
3502.164983	799588.476627	43.762893
3501.819582	799581.956672	43.767898
3501.935085	799568.734877	43.772903
3501.547171	799550.687875	43.777908
3501.990390	799515.816317	43.782913
3501.939694	799520.389201	43.787917
3501.904609	799511.413086	43.792922
3502.101098	799487.281740	43.797927
3502.078418	799485.911171	43.802932
3502.118229	799457.977174	43.807937
3502.194518	799438.331888	43.812941
3501.716497	799430.999244	43.817946
3502.062358	799406.744852	43.822951
3501.835131	799389.358111	43.827956
3501.709636	799371.022007	43.832961
3502.022352	799368.958103	43.837965
3501.966128	799348.009166	43.842970
3502.224882	799331.229388	43.847975
3501.926476	799321.952822	43.852980
3502.121044	799291.931197	43.857985
3502.068542	799283.595733	43.862989
3502.033900	799274.275659	43.867994
3502.352555	799251.154116	43.872999
3501.714252	799248.412407	43.878004
3501.963348	799210.086390	43.883009
3501.807280	799208.737738	43.888013
3501.773348	799207.467135	43.893018
3502.031350	799190.196307	43.898023
3502.018612	799183.866600	43.903028
3502.301086	799162.763151	43.908033
3502.354178	799128.395670	43.913037
3501.657776	799117.859117	43.918042
3502.428595	799093.779063	43.923047
3501.508146	799091.231015	43.928052
3501.655171	799060.234538	43.933057
3501.964884	799058.809137	43.938061
3501.664800	799045.556632	43.943066
3501.721776	799015.409226	43.948071
3501.790060	799017.017754	43.953076
3501.852953	798999.091403	43.958081
3501.733749	798990.128471	43.963085
3501.817180	798979.217834	43.968090
3501.754880	798966.171437	43.973095
3501.321952	798975.912489	43.978100
3501.577036	798967.624154	43.983105
3501.547364	798945.884272	43.988109
3501.773652	798921.255205	43.993114
3501.821893	798915.749663	43.998119
3501.673011	798922.744301	44.003124
3501.550242	798907.449823	44.008129
3501.767297	798884.098371	44.013133
3501.567997	798878.829916	44.018138
3501.808838	798870.936498	44.023143
3501.627967	798873.273300	44.028148
3501.867315	798844.175002	44.033153
3502.078852	798833.095778	44.038157
3502.013765	798836.984275	44.043162
3502.318673	798801.444724	44.048167
3501.848566	798795.484517	44.053172
3502.148490	798781.838162	44.058177
3501.808353	798754.307531	44.063181
3502.028360	798741.803254	44.068186
3502.040636	798733.750982	44.073191
3501.804361	798717.689395	44.078196
3502.165426	798696.473418	44.083201
3501.609651	798694.503283	44.088205
3501.344270	798669.414354	44.093210
3501.746825	798659.972358	44.098215
3501.730573	798640.389153	44.103220
3501.911322	798649.882315	44.108225
3502.070657	798638.369594	44.113229
3501.516047	798614.751644	44.118234
3502.066936	798607.739526	44.123239
3501.777157	798603.320254	44.128244
3501.961238	798573.542704	44.133249
3502.106817	798548.974706	44.138253
3501.839859	798550.393121	44.143258
3502.270338	798529.606997	44.148263
3502.011411	798520.813738	44.153268
3501.986274	798513.061904	44.158273
3501.947503	798478.706350	44.163277
3501.388070	798461.421096	44.168282
3502.014436	798451.843779	44.173287
3501.684718	798450.572668	44.178292
3501.605385	798427.808485	44.183297
3501.744192	798413.500705	44.188301
3501.615347	798409.692960	44.193306
3502.040507	798398.921485	44.198311
3501.593196	798388.735503	44.203316
3501.785260	798366.417309	44.208321
3501.839693	798358.701286	44.213325
3501.640125	798369.484710	44.218330
3501.570843	798324.971922	44.223335
3501.679538	798335.753712	44.228340
3501.628545	798322.851518	44.233345
3502.016031	798320.922264	44.238349
3501.965043	798297.907539	44.243354
3501.899976	798282.209466	44.248359
3501.380895	798292.112927	44.253364
3501.682149	798271.887311	44.258369
3501.692442	798253.476808	44.263373
3501.636887	798252.700493	44.268378
3501.965473	798224.959441	44.273383
3501.787969	798223.172312	44.278388
3501.665918	798193.099930	44.283393
3501.355969	798185.345552	44.288397
3501.606949	798182.947839	44.293402
3501.772983	798180.515026	44.298407
3501.780476	798179.384684	44.303412
3502.312749	798146.798884	44.308417
3502.063925	798140.948934	44.313421
3501.814646	798136.768148	44.318426
3501.932008	798105.085041	44.323431
3501.825691	798103.973432	44.328436
3501.749940	798093.382177	44.333441
3501.822242	798069.020926	44.338445
3501.693565	798054.854652	44.343450
3501.826681	798048.843532	44.348455
3501.548659	798044.863791	44.353460
3501.801423	798023.467245	44.358465
3502.197762	798006.170706	44.363469
3501.751268	797996.376748	44.368474
3501.880757	797975.000358	44.373479
3501.852692	797960.277308	44.378484
3501.899138	797950.647553	44.383489
3501.681506	797950.339731	44.388493
3501.710587	797926.279655	44.393498
3501.883399	797907.055990	44.398503
3501.468528	797914.537279	44.403508
3501.434002	797894.611343	44.408513
3501.249352	797905.933042	44.413517
3501.453816	797904.917490	44.418522
3501.761089	797890.237243	44.423527
3501.364196	797876.998455	44.428532
3501.581471	797856.245450	44.433537
3501.634250	797855.598526	44.438541
3501.452963	797856.610222	44.443546
3501.887499	797843.038052	44.448551
3501.590008	797826.837213	44.453556
3501.499698	797814.186019	44.458561
3501.730233	797806.587661	44.463565
3501.395359	797795.204047	44.468570
3501.857801	797788.892993	44.473575
3501.413201	797779.491164	44.478580
3501.553939	797778.878838	44.483585
3501.906520	797768.560193	44.488589
3501.709190	797774.974834	44.493594
3501.512235	797750.509541	44.498599
3501.514529	797738.677550	44.503604
3501.545690	797732.977515	44.508609
3501.431910	797727.203160	44.513613
3501.127333	797734.126442	44.518618
3501.773423	797713.891509	44.523623
3501.394729	797728.485657	44.528628
3501.616359	797712.542703	44.533633
3501.648436	797694.372608	44.538637
3501.329863	797681.758772	44.543642
3501.596069	797681.714902	44.548647
3501.419432	797681.547597	44.553652
3501.341920	797677.534617	44.558657
3501.633388	797660.401781	44.563661
3501.007689	797653.238854	44.568666
3501.557502	797633.510492	44.573671
3501.493797	797635.632026	44.578676
3501.610209	797632.765347	44.583681
3501.501729	797628.413779	44.588685
3501.643763	797622.253540	44.593690
3501.921527	797608.608550	44.598695
3501.542053	797601.895960	44.603700
3501.305322	797592.066881	44.608705
3501.594846	797581.463778	44.613709
3501.375771	797582.039884	44.618714
3501.534735	797572.391075	44.623719
3501.470394	797567.001204	44.628724
3501.452730	797537.497943	44.633729
3501.730904	797538.875862	44.638733
3501.515672	797538.518529	44.643738
3501.441194	797538.383488	44.648743
3501.177541	797535.775752	44.653748
3501.111977	797541.039714	44.658753
3501.475456	797533.762829	44.663757
3501.265173	797525.254869	44.668762
3501.476319	797504.010876	44.673767
3501.774284	797498.217607	44.678772
3501.781244	797483.880547	44.683777
3501.919664	797489.061854	44.688781
3501.726409	797476.917960	44.693786
3501.612020	797446.644717	44.698791
3501.468993	797448.681182	44.703796
3501.713182	797443.534972	44.708801
3501.742791	797442.793634	44.713805
3501.734952	797423.500205	44.718810
3501.833991	797409.147825	44.723815
3501.413270	797416.041454	44.728820
3501.527568	797395.844101	44.733825
3501.870180	797392.154528	44.738829
3501.664812	797380.110653	44.743834
3501.381432	797357.523877	44.748839
3501.648065	797358.461866	44.753844
3501.563466	797354.106192	44.758849
3501.795321	797343.855905	44.763853
3501.237649	797329.120564	44.768858
3501.648194	797320.608290	44.773863
3501.701594	797308.914444	44.778868
3501.814431	797303.642476	44.783873
3502.053800	797299.282504	44.788877
3501.636744	797276.177417	44.793882
3501.655946	797261.543303	44.798887
3501.722423	797262.956147	44.803892
3501.967601	797246.860964	44.808897
3501.803893	797231.667748	44.813901
3501.519076	797226.903097	44.818906
3501.631970	797212.744422	44.823911
3501.769730	797219.251670	44.828916
3501.693679	797181.409955	44.833921
3501.971488	797163.787179	44.838925
3501.765440	797156.358223	44.843930
3501.779496	797151.151509	44.848935
3501.764726	797136.817317	44.853940
3501.805056	797121.786646	44.858945
3501.858224	797120.550413	44.863949
3501.580158	797098.060118	44.868954
3501.777404	797081.579665	44.873959
3501.611551	797068.006692	44.878964
3501.426989	797063.225416	44.883969
3501.951445	797067.901564	44.888973
3501.531689	797064.533786	44.893978
3501.797883	797037.780276	44.898983
3501.573912	797046.753102	44.903988
3501.198215	797040.186642	44.908993
3501.513849	797036.304932	44.913997
3501.515821	797043.865782	44.919002
3501.854590	797010.471893	44.924007
3501.759591	796993.842974	44.929012
3501.838163	796993.879108	44.934017
3502.195863	796983.951261	44.939021
3501.731242	796960.558369	44.944026
3501.884628	796941.433450	44.949031
3501.708028	796932.084529	44.954036
3501.901201	796910.694399	44.959041
3501.886407	796889.878555	44.964045
3502.067472	796893.678488	44.969050
3502.117052	796871.477195	44.974055
3501.677289	796863.546323	44.979060
3501.562109	796843.925276	44.984065
3501.571404	796848.539127	44.989069
3501.511440	796831.953152	44.994074
3501.877457	796806.164319	44.999079
3501.811671	796806.224233	45.004084
3501.636962	796793.683292	45.009089
3501.975526	796795.149617	45.014093
3501.756303	796772.157577	45.019098
3501.674421	796750.321257	45.024103
3501.605914	796749.939712	45.029108
3501.751588	796746.085838	45.034113
3501.433164	796730.966117	45.039117
3501.490213	796715.048004	45.044122
3501.905447	796706.927024	45.049127
3501.835397	796712.143246	45.054132
3501.581246	796696.767359	45.059137
3501.961248	796674.560118	45.064141
3501.769749	796673.118601	45.069146
3501.681944	796653.738017	45.074151
3501.176902	796660.302562	45.079156
3501.515178	796644.927184	45.084161
3502.013118	796626.873989	45.089165
3501.573694	796625.276891	45.094170
3501.738518	796605.118037	45.099175
3501.920336	796601.258131	45.104180
3501.666771	796584.016032	45.109185
3501.802509	796571.423559	45.114189
3501.649573	796570.221177	45.119194
3501.321267	796565.512337	45.124199
3501.669823	796563.245313	45.129204
3501.908067	796534.186689	45.134209
3501.895018	796524.417465	45.139213
3501.615734	796522.352045	45.144218
3501.702667	796509.718397	45.149223
3501.638991	796486.699798	45.154228
3501.607882	796480.174256	45.159233
3501.720444	796473.035810	45.164237
3501.623778	796475.555945	45.169242
3501.836811	796445.911878	45.174247
3501.681505	796442.107412	45.179252
3501.602201	796422.233759	45.184257
3501.667753	796427.329651	45.189261
3501.858272	796419.736384	45.194266
3501.745746	796386.315651	45.199271
3501.742190	796385.628768	45.204276
3501.737453	796380.866507	45.209281
3501.852905	796360.224049	45.214285
3501.598936	796334.142774	45.219290
3501.517388	796331.357275	45.224295
3501.514257	796332.634463	45.229300
3501.567212	796323.246916	45.234305
3501.763386	796331.856829	45.239309
3501.676549	796320.135327	45.244314
3502.037219	796298.863054	45.249319
3501.685566	796299.215576	45.254324
3501.736244	796280.891436	45.259329
3501.614913	796260.484101	45.264333
3501.539233	796255.978961	45.269338
3501.659601	796238.969045	45.274343
3501.545727	796240.510012	45.279348
3501.810912	796236.145132	45.284353
3501.812818	796210.561398	45.289357
3501.487597	796202.807323	45.294362
3501.493792	796196.471790	45.299367
3501.810738	796200.053302	45.304372
3501.661609	796184.609885	45.309377
3501.754365	796159.894887	45.314381
3501.407314	796146.104445	45.319386
3501.889223	796136.695099	45.324391
3501.545987	796138.961337	45.329396
3501.504542	796121.044793	45.334401
3501.813166	796111.811272	45.339405
3501.425091	796119.437365	45.344410
3501.794415	796118.296197	45.349415
3501.922474	796112.775303	45.354420
3501.686120	796077.605706	45.359425
3501.732316	796065.419917	45.364429
3501.518347	796064.129289	45.369434
3501.333497	796062.391914	45.374439
3501.358280	796052.664906	45.379444
3501.480370	796039.238931	45.384449
3501.743101	796020.339019	45.389453
3500.995133	796027.975385	45.394458
3501.607850	796016.580102	45.399463
3501.709937	796023.683610	45.404468
3501.582663	796024.342927	45.409473
3501.656336	795992.362818	45.414477
3501.450211	795982.771959	45.419482
3501.693708	795982.584511	45.424487
3501.498031	795979.326610	45.429492
3501.773469	795981.589206	45.434497
3501.940088	795951.214102	45.439501
3501.789820	795946.622836	45.444506
3501.873004	795921.417510	45.449511
3501.596427	795935.458389	45.454516
3501.545796	795910.275064	45.459521
3501.710816	795886.234691	45.464525
3501.800394	795885.237778	45.469530
3501.787113	795877.775709	45.474535
3501.503355	795864.563569	45.479540
3501.637041	795843.671053	45.484545
3501.706957	795838.896127	45.489549
3501.405703	795838.503761	45.494554
3501.726202	795837.026842	45.499559
3501.684266	795832.564978	45.504564
3501.875630	795808.372678	45.509569
3501.604568	795787.006481	45.514573
3501.671522	795794.214224	45.519578
3501.580417	795782.443418	45.524583
3501.109392	795772.994118	45.529588
3501.430048	795757.914349	45.534593
3501.670114	795746.629119	45.539597
3501.548652	795749.890214	45.544602
3501.829539	795750.089464	45.549607
3501.662993	795738.871196	45.554612
3501.543925	795728.725463	45.559617
3501.882869	795710.057704	45.564621
3501.578859	795695.915528	45.569626
3501.766782	795689.647821	45.574631
3501.639996	795681.418508	45.579636
3501.473492	795677.959227	45.584641
3501.777173	795652.421968	45.589645
3501.406430	795659.210860	45.594650
3501.617173	795648.028519	45.599655
3501.649501	795647.728521	45.604660
3501.613246	795624.555248	45.609665
3501.860621	795608.063079	45.614669
3501.732182	795609.508365	45.619674
3501.774521	795595.996461	45.624679
3501.654207	795581.872907	45.629684
3501.341901	795572.151647	45.634689
3501.766132	795569.626299	45.639693
3501.576213	795565.139530	45.644698
3501.422795	795563.691507	45.649703
3501.490457	795568.198369	45.654708
3501.434934	795545.862863	45.659713
3501.682765	795531.285695	45.664717
3501.338142	795533.699680	45.669722
3501.862571	795528.309478	45.674727
3501.762869	795524.348025	45.679732
3501.543226	795502.972492	45.684737
3501.590383	795482.486031	45.689741
3501.431551	795482.070183	45.694746
3501.730323	795476.029576	45.699751
3501.767473	795474.943022	45.704756
3501.753933	795460.703417	45.709761
3501.757593	795431.482431	45.714765
3501.409481	795435.272102	45.719770
3501.594322	795427.482261	45.724775
3501.878574	795428.122959	45.729780
3501.685532	795414.354816	45.734785
3501.711782	795385.129916	45.739789
3501.500209	795384.771860	45.744794
3501.747265	795377.561040	45.749799
3501.621090	795366.777519	45.754804
3501.543497	795354.414444	45.759809
3501.859103	795334.276217	45.764813
3501.162918	795327.662705	45.769818
3501.426526	795252.675967	45.774823
3501.545786	795135.328658	45.779828
3501.220464	794968.350244	45.784833
3501.372955	794729.925636	45.789837
3500.941902	794442.521489	45.794842
3500.770377	794099.558310	45.799847
3500.582360	793692.280613	45.804852
3500.137448	793239.777486	45.809857
3500.167689	792725.068497	45.814861
3499.771393	792162.733664	45.819866
3499.645864	791532.697165	45.824871
3499.247686	790847.414282	45.829876
3498.705728	790100.999362	45.834881
3498.368179	789296.816579	45.839885
3497.479372	788454.093631	45.844890
3497.369336	787527.808949	45.849895
3496.825840	786558.549030	45.854900
3496.087380	785532.389068	45.859905
3495.614640	784436.391555	45.864909
3494.917234	783304.057565	45.869914
3493.776562	782098.013054	45.874919
3493.455098	780843.898424	45.879924
3492.885737	779530.643181	45.884929
3491.640411	778159.615641	45.889933
3490.937904	776742.449617	45.894938
3489.985426	775248.125029	45.899943
3489.261312	773721.490041	45.904948
3488.227793	772116.350724	45.909953
3487.707267	770457.112558	45.914957
3486.185595	768755.130012	45.919962
3485.110747	766988.837809	45.924967
3484.195070	765168.299805	45.929972
3482.922785	763287.052191	45.934977
3482.327358	761351.542235	45.939981
3480.639720	759360.492140	45.944986
3479.631017	757322.454789	45.949991
3478.564003	755210.209837	45.954996
3477.037336	753070.590181	45.960001
3475.756231	750870.801656	45.965005
3474.213505	748620.418354	45.970010
3472.691472	746320.342200	45.975015
3471.566579	743966.811850	45.980020
3470.156112	741549.310232	45.985025
3468.826434	739090.434781	45.990029
3467.033249	736584.054384	45.995034
3465.663966	734013.792483	46.000039
3464.226480	731403.101441	46.005044
3462.767362	728747.233307	46.010049
3461.005752	726030.782538	46.015053
3459.213079	723280.372841	46.020058
3457.686022	720458.930503	46.025063
3456.000581	717614.980042	46.030068
3454.065225	714715.865300	46.035073
3452.326217	711764.988173	46.040077
3450.276843	708776.291719	46.045082
3448.828125	705721.972078	46.050087
3447.211626	702647.518987	46.055092
3445.207049	699499.760367	46.060097
3443.097855	696314.388265	46.065101
3440.982955	693096.430093	46.070106
3439.301293	689817.270134	46.075111
3437.694455	686493.739431	46.080116
3435.443681	683146.239542	46.085121
3433.347758	679740.144904	46.090125
3431.326347	676278.455994	46.095130
3429.089819	672781.663988	46.100135
3427.272576	669257.618592	46.105140
3424.943750	665666.985554	46.110145
3423.036217	662036.106047	46.115149
3420.871742	658378.493427	46.120154
3418.388741	654664.068878	46.125159
3416.157442	650915.427337	46.130164
3413.730730	647105.822843	46.135169
3411.466542	643285.255132	46.140173
3409.025884	639435.772764	46.145178
3406.812795	635517.954260	46.150183
3404.171999	631560.536702	46.155188
3401.433279	627579.466477	46.160193
3399.642208	623562.437126	46.165197
3396.985873	619509.525070	46.170202
3394.411490	615397.286539	46.175207
3392.091151	611242.500708	46.180212
3389.491176	607082.863257	46.185217
3386.895612	602869.398673	46.190221
3384.059685	598624.505467	46.195226
3381.450578	594352.915963	46.200231
3378.864432	590035.208302	46.205236
3375.803288	585688.780261	46.210241
3373.532479	581308.436300	46.215245
3370.440624	576894.479053	46.220250
3367.717650	572452.890044	46.225255
3365.300903	567975.871352	46.230260
3362.357078	563470.547596	46.235265
3359.644897	558918.804525	46.240269
3356.670794	554332.644488	46.245274
3353.767890	549732.117367	46.250279
3351.195314	545094.751717	46.255284
3348.082759	540441.615285	46.260289
3345.394827	535740.870940	46.265293
3341.918738	531007.388439	46.270298
3339.271021	526252.612209	46.275303
3336.419572	521468.891580	46.280308
3333.115808	516669.809710	46.285313
3330.195634	511825.525933	46.290317
3327.036280	506970.610103	46.295322
3324.142179	502081.231269	46.300327
3320.779709	497170.662325	46.305332
3317.469849	492237.159828	46.310337
3314.602819	487261.488125	46.315341
3311.267622	482283.587273	46.320346
3307.803190	477276.591117	46.325351
3305.092418	472241.223890	46.330356
3301.529495	467180.851114	46.335361
3298.829758	462100.423859	46.340365
3295.175830	457009.029940	46.345370
3292.023251	451879.225166	46.350375
3288.683636	446730.706705	46.355380
3284.801863	441570.047843	46.360385
3281.774074	436402.119104	46.365389
3278.373751	431214.311879	46.370394
3275.124200	426007.171123	46.375399
3271.937263	420772.001034	46.380404
3268.256005	415513.634912	46.385409
3265.180150	410245.146206	46.390413
3261.534472	404965.819372	46.395418
3258.206973	399660.421122	46.400423
3254.972575	394340.294407	46.405428
3250.936003	389001.473525	46.410433
3247.579051	383655.359789	46.415437
3243.956353	378307.736871	46.420442
3240.302000	372921.528457	46.425447
3236.825018	367544.228904	46.430452
3233.056409	362153.828688	46.435457
3229.718727	356744.518219	46.440461
3226.197954	351329.762167	46.445466
3222.425091	345888.209466	46.450471
3218.882014	340428.107074	46.455476
3215.125148	334982.648138	46.460481
3211.211030	329532.166753	46.465485
3207.563065	324054.968813	46.470490
3203.706461	318577.998152	46.475495
3200.044551	313102.297984	46.480500
3196.296160	307616.879550	46.485505
3192.784238	302115.209644	46.490509
3188.566426	296625.542918	46.495514
3184.689056	291133.641561	46.500519
3181.291403	285619.429983	46.505524
3177.178224	280120.401915	46.510529
3173.549418	274610.984981	46.515533
3169.309695	269109.558552	46.520538
3165.175890	263586.171328	46.525543
3161.719974	258073.980316	46.530548
3157.892113	252564.056434	46.535553
3154.024451	247041.156079	46.540557
3150.207434	241525.909034	46.545562
3145.734874	236021.400842	46.550567
3142.163692	230495.022626	46.555572
3138.025684	224989.178149	46.560577
3133.818670	219485.439158	46.565581
3129.479124	213988.185091	46.570586
3125.396475	208456.235293	46.575591
3121.739719	202907.660055	46.580596
3117.301866	197430.297979	46.585601
3113.707791	191940.861427	46.590605
3109.266378	186472.785088	46.595610
3105.166836	181009.670795	46.600615
3101.388517	175540.058932	46.605620
3096.698836	170101.354551	46.610625
3092.772950	164664.105508	46.615629
3088.391418	159251.711824	46.620634
3084.191553	153833.438381	46.625639
3079.757666	148416.986103	46.630644
3075.731259	143040.604099	46.635649
3071.305427	137664.203427	46.640653
3066.439658	132298.301324	46.645658
3062.194312	126962.578400	46.650663
3058.014207	121641.230039	46.655668
3053.055442	116325.356089	46.660673
3048.760409	111036.380576	46.665677
3044.372782	105784.531136	46.670682
3039.575365	100535.605967	46.675687
3035.193031	95320.452520	46.680692
3030.271497	90137.865852	46.685697
3025.465675	84971.716843	46.690701
3020.713629	79842.523356	46.695706
3015.947958	74727.201869	46.700711
3011.201664	69653.668076	46.705716
3005.705781	64608.110498	46.710721
3000.923688	59607.742628	46.715725
2995.487104	54647.658017	46.720730
2989.380648	49747.643101	46.725735
2981.103496	44948.166021	46.730740
2966.886783	40390.501088	46.735745
2952.551924	35976.932196	46.740749
2938.178238	31724.242056	46.745754
2924.223354	27690.732911	46.750759
2911.860051	23856.134287	46.755764
2898.784335	20276.520113	46.760769
2886.920158	16884.019890	46.765773
2875.244088	13744.916081	46.770778
2863.864811	10807.652237	46.775783
2852.772468	8100.232082	46.780788
2840.225286	5623.170178	46.785793
2827.585258	3400.962331	46.790797
2811.456880	1506.888103	46.795802
2780.480760	278.937392	46.800807
2721.206416	257.615976	46.805812
2686.455651	262.596934	46.810817
2678.579829	257.152830	46.815821
2688.576555	248.491141	46.820826
2705.004393	238.599088	46.825831
2719.850015	227.526319	46.830836
2729.093399	242.557597	46.835841
2732.521280	237.941386	46.840845
2731.718934	235.038982	46.845850
2728.422698	236.397616	46.850855
2725.211840	225.594757	46.855860
2720.853339	229.428765	46.860865
2717.031319	224.545889	46.865869
2714.224546	232.242798	46.870874
2711.550006	237.280353	46.875879
2709.200019	224.951581	46.880884
2706.414784	225.279736	46.885889
2703.832151	223.224724	46.890893
2700.747209	227.507617	46.895898
2697.530053	225.834748	46.900903
2694.814017	222.488382	46.905908
2691.289168	228.025743	46.910913
2688.467274	219.969284	46.915917
2685.280620	224.108926	46.920922
2682.099063	223.601673	46.925927
2679.283294	216.994992	46.930932
2675.563115	222.054001	46.935937
2672.462732	210.384795	46.940941
2669.411534	217.075630	46.945946
2665.636172	214.371575	46.950951
2662.540603	215.156992	46.955956
2658.935086	225.309026	46.960961
2655.586867	213.355211	46.965965
2652.856216	210.302516	46.970970
2649.647695	206.785394	46.975975
2646.103852	209.339787	46.980980
2642.320787	203.932083	46.985985
2639.120720	207.903270	46.990989
2635.833604	211.178368	46.995994
2632.534865	215.931224	47.000999
2629.364443	205.372950	47.006004
2625.611750	220.468691	47.011009
2622.355750	215.422103	47.016013
2618.948435	209.837519	47.021018
2615.451485	202.769581	47.026023
2612.563594	205.326037	47.031028
2608.685113	211.571499	47.036033
2605.098389	209.096440	47.041037
2602.348492	208.136238	47.046042
2598.913056	192.330113	47.051047
2595.510899	190.297009	47.056052
2591.589359	200.489417	47.061057
2588.092248	201.075086	47.066061
2584.665267	203.106187	47.071066
2580.847020	201.982465	47.076071
2577.346763	194.538319	47.081076
2574.179727	193.979389	47.086081
2570.979994	199.940690	47.091085
2567.789784	190.142534	47.096090
2564.149857	190.342919	47.101095
2560.681013	196.831925	47.106100
2557.408952	207.003489	47.111105
2554.113955	201.757467	47.116109
2550.998332	202.980727	47.121114
2546.893552	203.803353	47.126119
2543.401258	193.348027	47.131124
2540.055936	194.464631	47.136129
2536.520845	202.880724	47.141133
2532.962866	198.009373	47.146138
2529.382091	193.298257	47.151143
2526.309213	199.267662	47.156148
2522.601420	201.897977	47.161153
2519.277594	201.977003	47.166157
2516.409593	201.473366	47.171162
2512.373491	212.656789	47.176167
2508.897754	198.350363	47.181172
2505.108560	188.504895	47.186177
2501.462931	191.563210	47.191181
2498.415967	182.449844	47.196186
2495.111304	188.140387	47.201191
2491.768318	173.171712	47.206196
2488.029520	187.691673	47.211201
2484.820613	193.589006	47.216205
2481.274985	189.449768	47.221210
2477.548688	184.782113	47.226215
2474.253097	184.967297	47.231220
2470.636696	187.092032	47.236225
2467.645399	186.503872	47.241229
2463.944692	188.374654	47.246234
2460.042965	202.039693	47.251239
2456.661903	186.239100	47.256244
2452.950427	196.030404	47.261249
2450.010907	188.663754	47.266253
2446.394047	181.532224	47.271258
2442.499124	185.122302	47.276263
2439.414922	176.686383	47.281268
2436.083291	182.605151	47.286273
2432.351612	183.955007	47.291277
2429.090140	185.803196	47.296282
2425.071075	189.115411	47.301287
2421.957309	191.613282	47.306292
2418.408357	188.293491	47.311297
2414.963710	180.440603	47.316301
2411.862683	188.152752	47.321306
2407.933391	198.196649	47.326311
2404.363708	190.397233	47.331316
2401.147680	188.673009	47.336321
2397.301941	187.051251	47.341325
2394.064198	177.149745	47.346330
2390.327493	184.408913	47.351335
2387.279951	186.155937	47.356340
2383.544316	196.626472	47.361345
2380.347976	193.532489	47.366349
2376.595383	183.639234	47.371354
2372.885480	191.254886	47.376359
2370.136641	181.722746	47.381364
2366.245906	192.384510	47.386369
2362.771677	182.097391	47.391373
2359.116753	179.429778	47.396378
2355.244869	193.545433	47.401383
2352.421524	176.987289	47.406388
2348.881223	187.443080	47.411393
2345.408253	192.323134	47.416397
2341.723916	181.898221	47.421402
2338.061552	192.790686	47.426407
2334.831486	179.498233	47.431412
2331.251007	191.755455	47.436417
2327.881148	184.565891	47.441421
2324.617034	182.065396	47.446426
2320.867469	189.736938	47.451431
2317.632339	180.687943	47.456436
2313.501373	176.647399	47.461441
2309.863305	180.980697	47.466445
2306.869583	181.506264	47.471450
2303.328340	185.414264	47.476455
2300.361387	171.453642	47.481460
2296.385237	188.011828	47.486465
2293.270068	174.875968	47.491469
2289.141262	177.849104	47.496474
2285.505363	176.577665	47.501479
2282.172327	170.669156	47.506484
2278.966486	179.992359	47.511489
2275.425609	172.643977	47.516493
2272.254512	171.265107	47.521498
2268.182173	177.772060	47.526503
2265.037316	170.682266	47.531508
2261.507989	177.202764	47.536513
2257.424515	178.447937	47.541517
2254.336877	176.117364	47.546522
2250.596705	175.861858	47.551527
2247.688953	170.716101	47.556532
2244.205703	166.311178	47.561537
2240.575301	168.017053	47.566541
2236.931331	176.716691	47.571546
2233.346870	186.591210	47.576551
2230.224336	173.155002	47.581556
2226.688822	178.943701	47.586561
2222.971295	181.391068	47.591565
2219.409125	177.926361	47.596570
2215.871138	177.656469	47.601575
2212.661631	175.588121	47.606580
2209.050709	186.759044	47.611585
2205.135830	171.751184	47.616589
2201.872563	176.505348	47.621594
2198.435556	183.304352	47.626599
2194.838380	169.632028	47.631604
2191.689809	173.960115	47.636609
2188.464923	170.686738	47.641613
2184.704840	157.824153	47.646618
2180.933982	173.772440	47.651623
2177.823849	163.739318	47.656628
2173.742301	168.771213	47.661633
2169.873301	164.304164	47.666637
2166.856644	169.225932	47.671642
2163.444022	169.696437	47.676647
2160.541032	166.577558	47.681652
2156.835445	163.314424	47.686657
2152.577473	170.086557	47.691661
2149.505258	166.529238	47.696666
2145.683504	169.113108	47.701671
2142.561884	173.925028	47.706676
2138.601208	169.482291	47.711681
2135.458630	176.985516	47.716685
2132.113760	166.671481	47.721690
2128.524126	173.342466	47.726695
2125.362755	162.629090	47.731700
2121.652270	170.813597	47.736705
2118.487406	168.962378	47.741709
2114.864726	167.703051	47.746714
2110.972492	169.007621	47.751719
2107.956247	171.671945	47.756724
2103.938272	173.913498	47.761729
2100.229126	176.028048	47.766733
2096.851434	169.278540	47.771738
2093.348440	178.390656	47.776743
2090.118802	169.520736	47.781748
2086.424831	169.173439	47.786753
2082.994632	164.493965	47.791757
2079.824274	160.932741	47.796762
2075.916900	164.837692	47.801767
2072.721238	159.376839	47.806772
2068.832889	163.517013	47.811777
2064.950724	169.986080	47.816781
2062.245108	162.512376	47.821786
2058.838803	163.609154	47.826791
2055.733294	161.743240	47.831796
2051.825675	166.376538	47.836801
2048.041474	168.039405	47.841805
2044.519734	155.061334	47.846810
2040.565186	167.220713	47.851815
2037.307810	162.931954	47.856820
2034.025678	160.682201	47.861825
2030.363612	161.208910	47.866829
2027.136522	158.599944	47.871834
2023.331498	164.531541	47.876839
2020.185753	156.255463	47.881844
2016.476553	167.868364	47.886849
2013.032556	160.898587	47.891853
2009.723972	161.095588	47.896858
2006.227161	161.540490	47.901863
2002.834087	152.845870	47.906868
1998.929388	163.603497	47.911873
1995.273349	164.293494	47.916877
1992.152973	160.517476	47.921882
1988.471311	163.233600	47.926887
1984.977741	149.089424	47.931892
1981.732662	154.926891	47.936897
1978.112934	163.636438	47.941901
1974.735043	152.040560	47.946906
1970.808043	162.882184	47.951911
1967.599092	147.410982	47.956916
1964.208888	149.891980	47.961921
1960.639445	152.781099	47.966925
1956.855831	154.132747	47.971930
1953.164344	158.072485	47.976935
1950.183215	157.832997	47.981940
1946.582433	148.862100	47.986945
1942.899816	158.175065	47.991949
1939.674754	156.823201	47.996954
1936.039718	157.316788	48.001959
1932.845273	154.650292	48.006964
1928.857245	150.537866	48.011969
1925.462220	157.753973	48.016973
1922.159895	153.103806	48.021978
1918.449575	154.656285	48.026983
1914.721634	158.164508	48.031988
1911.137163	157.821729	48.036993
1908.038561	152.379874	48.041997
1904.941472	150.527931	48.047002
1900.988848	153.007227	48.052007
1897.589037	160.693057	48.057012
1893.871434	154.585867	48.062017
1890.537231	162.570663	48.067021
1887.197914	154.912814	48.072026
1883.373538	159.200178	48.077031
1880.373684	151.490081	48.082036
1876.566466	150.945019	48.087041
1872.891385	151.557911	48.092045
1869.393670	145.489442	48.097050
1865.861396	140.893227	48.102055
1862.816987	145.225853	48.107060
1859.124077	140.328500	48.112065
1855.449159	141.837186	48.117069
1851.712822	155.037876	48.122074
1847.821451	156.248221	48.127079
1845.354470	149.317924	48.132084
1841.933828	153.500321	48.137089
1838.143127	146.636681	48.142093
1834.839850	146.009883	48.147098
1831.164218	145.724114	48.152103
1827.652741	149.813669	48.157108
1823.918221	156.824087	48.162113
1820.195279	152.528587	48.167117
1817.089687	143.333412	48.172122
1813.363590	152.730948	48.177127
1809.797331	145.721575	48.182132
1806.405295	154.451729	48.187137
1802.916456	150.017675	48.192141
1799.627827	132.401894	48.197146
1796.193908	147.304666	48.202151
1792.884822	140.257217	48.207156
1789.068376	139.864671	48.212161
1785.273933	145.792750	48.217165
1781.968466	143.310192	48.222170
1778.414227	144.234979	48.227175
1775.060429	142.222215	48.232180
1771.423758	131.693433	48.237185
1767.913171	142.881083	48.242189
1764.520972	141.942925	48.247194
1761.021713	144.544214	48.252199
1757.771375	143.179834	48.257204
1753.731736	135.417709	48.262209
1750.300376	141.970383	48.267213
1746.911971	134.336900	48.272218
1743.272227	132.469694	48.277223
1739.888740	132.883003	48.282228
1736.481819	137.986315	48.287233
1733.262590	141.276313	48.292237
1729.540747	139.529999	48.297242
1726.170745	142.039635	48.302247
1722.421729	133.068477	48.307252
1718.840038	140.344068	48.312257
1715.045741	144.674988	48.317261
1711.911064	136.746207	48.322266
1708.158282	137.073069	48.327271
1704.820351	139.809465	48.332276
1701.297819	127.681797	48.337281
1697.627879	141.580531	48.342285
1694.493653	131.902095	48.347290
1691.131765	148.063527	48.352295
1687.916286	142.237656	48.357300
1684.291924	140.686606	48.362305
1680.235545	138.264564	48.367309
1676.977107	133.042472	48.372314
1673.391143	137.383529	48.377319
1669.804961	138.865233	48.382324
1666.272235	135.101081	48.387329
1662.635561	134.764477	48.392333
1659.326635	134.588965	48.397338
1655.839457	149.833541	48.402343
1652.557175	134.823437	48.407348
1648.664358	142.744413	48.412353
1645.456755	142.153908	48.417357
1642.222115	139.167530	48.422362
1638.289787	139.226701	48.427367
1635.068868	130.048886	48.432372
1631.375111	137.996117	48.437377
1627.801217	151.257790	48.442381
1624.567334	132.725735	48.447386
1620.576728	136.961330	48.452391
1617.554340	124.878060	48.457396
1614.104704	131.774268	48.462401
1610.179978	126.964050	48.467405
1606.772935	125.448215	48.472410
1603.269185	131.394210	48.477415
1600.123755	129.537954	48.482420
1596.271933	127.507915	48.487425
1592.613113	137.224342	48.492429
1589.194066	133.973731	48.497434
1585.794777	143.757735	48.502439
1582.460185	129.128448	48.507444
1578.970983	141.663060	48.512449
1575.178050	130.401512	48.517453
1571.651888	132.478720	48.522458
1568.201568	142.958991	48.527463
1565.080557	130.696777	48.532468
1561.642414	132.892949	48.537473
1557.835170	137.602063	48.542477
1554.264806	131.095293	48.547482
1550.543791	134.622274	48.552487
1547.232838	129.246033	48.557492
1543.918480	127.996897	48.562497
1539.748288	132.696951	48.567501
1536.941835	126.812940	48.572506
1533.098864	129.845063	48.577511
1529.483977	135.184338	48.582516
1526.436128	135.398911	48.587521
1522.850068	127.819188	48.592525
1519.457533	131.455452	48.597530
1515.825914	131.287976	48.602535
1512.330540	124.918225	48.607540
1508.624994	114.697648	48.612545
1504.935478	123.237551	48.617549
1501.888446	122.530245	48.622554
1498.032858	137.466286	48.627559
1494.607182	115.498973	48.632564
1490.929457	124.139935	48.637569
1487.881420	131.106953	48.642573
1484.559187	128.996683	48.647578
1480.949157	133.694696	48.652583
1477.548939	126.388985	48.657588
1473.857937	134.861375	48.662593
1469.967594	129.907743	48.667597
1466.714464	124.639504	48.672602
1463.108325	132.754368	48.677607
1459.594730	140.533625	48.682612
1456.291076	134.705065	48.687617
1452.569207	136.926507	48.692621
1449.440447	125.664153	48.697626
1445.577042	125.231991	48.702631
1441.973959	121.570242	48.707636
1438.502290	123.439133	48.712641
1435.190045	118.929082	48.717645
1432.054679	121.758248	48.722650
1428.264635	130.726575	48.727655
1425.062742	131.195992	48.732660
1421.397509	136.509983	48.737665
1417.597947	134.612106	48.742669
1414.019929	124.128528	48.747674
1410.542493	127.450520	48.752679
1406.812821	125.834521	48.757684
1403.730846	134.986411	48.762689
1400.059116	132.654072	48.767693
1396.897662	119.629606	48.772698
1393.147054	125.344237	48.777703
1389.432608	121.300151	48.782708
1386.317047	126.280739	48.787713
1382.620570	122.786073	48.792717
1379.310062	122.692741	48.797722
1375.404150	136.281980	48.802727
1371.960043	129.458309	48.807732
1368.820639	119.778053	48.812737
1365.033617	118.584423	48.817741
1361.714977	128.740646	48.822746
1357.983674	129.148992	48.827751
1354.722095	129.200811	48.832756
1351.223507	131.153311	48.837761
1347.451852	123.957519	48.842765
1344.033545	116.622909	48.847770
1340.250570	123.597725	48.852775
1337.090731	125.334102	48.857780
1334.014422	112.237715	48.862785
1330.227673	120.920121	48.867789
1326.912737	119.385278	48.872794
1322.948977	112.988766	48.877799
1319.764798	118.180583	48.882804
1316.261895	116.237155	48.887809
1312.608404	127.736828	48.892813
1309.180656	122.239110	48.897818
1305.586628	130.595330	48.902823
1301.979602	129.203519	48.907828
1298.556152	123.609993	48.912833
1294.878411	121.013417	48.917837
1291.297726	113.448244	48.922842
1287.774210	121.674342	48.927847
1284.776044	114.502460	48.932852
1281.750720	122.380351	48.937857
1277.860247	130.295780	48.942861
1274.330131	114.562446	48.947866
1270.619766	130.529143	48.952871
1266.964422	125.552632	48.957876
1263.790814	130.230996	48.962881
1259.979475	124.501834	48.967885
1256.342537	117.984232	48.972890
1252.895746	121.005759	48.977895
1249.530566	111.904567	48.982900
1246.006948	119.302473	48.987905
1242.220140	129.010373	48.992909
1239.140443	115.539306	48.997914
1235.206018	121.958476	49.002919
1232.335545	125.921472	49.007924
1229.071327	118.245296	49.012929
1224.877234	122.714267	49.017933
1221.712182	124.730260	49.022938
1217.595263	125.067766	49.027943
1214.771852	113.544223	49.032948
1211.265791	121.721793	49.037953
1207.491549	122.031055	49.042957
1203.997495	113.841835	49.047962
1200.055829	126.485200	49.052967
1196.564721	124.168640	49.057972
1193.591021	115.996726	49.062977
1190.225073	116.685711	49.067981
1186.816928	118.651872	49.072986
1183.273872	119.367532	49.077991
1179.799359	117.131115	49.082996
1175.847224	119.977913	49.088001
1171.896676	120.555737	49.093005
1168.855768	108.123388	49.098010
1165.445189	119.222820	49.103015
1161.875296	108.937851	49.108020
1158.555571	117.866536	49.113025
1154.795176	124.432135	49.118029
1151.547102	121.123737	49.123034
1148.225145	116.078748	49.128039
1144.223126	121.291400	49.133044
1141.224457	116.837670	49.138049
1137.795125	122.343508	49.143053
1134.007463	118.749695	49.148058
1130.278949	119.686997	49.153063
1126.747976	121.155810	49.158068
1123.522949	117.412000	49.163073
1119.707483	117.907275	49.168077
1116.602441	117.871507	49.173082
1112.710861	116.803211	49.178087
1109.542810	117.769052	49.183092
1106.016893	115.261469	49.188097
1102.210123	117.759333	49.193101
1098.804673	116.634569	49.198106
1095.063330	123.228324	49.203111
1091.549616	122.084833	49.208116
1088.431149	112.989571	49.213121
1085.062054	121.192629	49.218125
1081.838580	108.082016	49.223130
1078.246542	110.845148	49.228135
1074.458047	112.876520	49.233140
1070.822217	107.636554	49.238145
1067.281862	124.502231	49.243149
1063.777703	116.625827	49.248154
1060.303135	115.025523	49.253159
1056.727085	112.681134	49.258164
1053.688915	109.892192	49.263169
1049.671296	122.455125	49.268173
1046.490642	124.523593	49.273178
1042.584286	122.552896	49.278183
1038.999309	114.399504	49.283188
1035.989884	105.090441	49.288193
1032.167487	114.818311	49.293197
1028.883258	110.897765	49.298202
1025.268064	109.668955	49.303207
1021.990273	100.041054	49.308212
1018.709298	103.668294	49.313217
1014.749316	118.152236	49.318221
1011.269447	112.276955	49.323226
1007.759498	126.749452	49.328231
1004.189715	121.195444	49.333236
1001.062368	113.338062	49.338241
997.399389	116.606330	49.343245
993.688809	111.469612	49.348250
990.075030	113.212717	49.353255
986.673037	110.653169	49.358260
983.347765	111.385657	49.363265
980.166930	111.718813	49.368269
976.470740	105.055290	49.373274
972.974852	108.421965	49.378279
969.179029	116.211217	49.383284
965.774609	110.575672	49.388289
962.254139	122.019879	49.393293
959.071875	112.439276	49.398298
955.394447	110.890083	49.403303
951.549621	113.203804	49.408308
948.277941	113.416815	49.413313
944.573478	111.662643	49.418317
941.393240	108.802205	49.423322
937.788342	115.728273	49.428327
934.250403	107.860095	49.433332
930.756480	114.187545	49.438337
927.262769	102.668881	49.443341
923.597701	105.370846	49.448346
919.665645	111.270354	49.453351
916.428233	113.680229	49.458356
913.646118	111.733039	49.463361
909.795160	110.958761	49.468365
906.566808	107.772234	49.473370
902.600703	107.999592	49.478375
899.149738	108.851629	49.483380
895.670081	104.248756	49.488385
891.967766	111.520047	49.493389
888.877116	112.182074	49.498394
885.667180	106.518311	49.503399
881.732729	111.263163	49.508404
878.296534	102.864024	49.513409
874.677439	103.968180	49.518413
871.550977	92.710343	49.523418
867.492198	113.610597	49.528423
864.111691	108.418668	49.533428
861.023365	107.273923	49.538433
856.922031	103.474382	49.543437
853.660476	108.196240	49.548442
849.959520	107.241746	49.553447
846.423202	105.410440	49.558452
843.106059	99.026159	49.563457
839.331927	116.862415	49.568461
836.450472	110.974353	49.573466
833.123669	110.708468	49.578471
829.573929	98.340811	49.583476
826.004531	108.663034	49.588481
821.909399	106.979460	49.593485
818.333649	99.296465	49.598490
815.012137	99.711135	49.603495
811.481406	90.179294	49.608500
808.156415	102.470495	49.613505
804.494476	103.294672	49.618509
800.886542	99.121968	49.623514
797.662957	106.051428	49.628519
794.271820	102.704295	49.633524
790.727256	105.488441	49.638529
787.247964	102.364823	49.643533
784.174260	102.768678	49.648538
780.183299	103.283455	49.653543
776.850326	104.563476	49.658548
773.189351	102.211961	49.663553
769.073843	107.685160	49.668557
765.898514	99.720214	49.673562
762.510313	104.722194	49.678567
758.894816	100.212865	49.683572
755.873942	96.748377	49.688577
752.084146	105.019951	49.693581
748.520212	106.768959	49.698586
744.790233	106.142713	49.703591
741.453230	103.041893	49.708596
738.156716	109.289967	49.713601
734.595534	105.866865	49.718605
731.361786	91.813348	49.723610
727.968906	104.454675	49.728615
723.977220	94.596195	49.733620
720.699558	99.200704	49.738625
717.061745	100.386269	49.743629
713.540010	86.196333	49.748634
709.752698	99.801164	49.753639
706.400137	102.416906	49.758644
703.212190	99.002627	49.763649
699.208264	109.684839	49.768653
696.259110	103.657973	49.773658
692.511507	93.523616	49.778663
688.885979	101.166189	49.783668
685.596048	94.486864	49.788673
681.945606	105.851120	49.793677
678.595775	98.591824	49.798682
674.855240	107.140023	49.803687
671.256378	97.509121	49.808692
667.844662	99.040356	49.813697
664.461794	106.571244	49.818701
661.228780	99.174771	49.823706
657.548044	99.938499	49.828711
654.114782	106.207713	49.833716
650.468559	99.552126	49.838721
646.823488	101.350694	49.843725
643.606871	99.056785	49.848730
640.126992	109.020979	49.853735
636.733544	95.972959	49.858740
633.124646	96.682808	49.863745
629.218307	101.332586	49.868749
625.854294	96.649406	49.873754
622.752896	95.077189	49.878759
618.670597	103.048583	49.883764
615.482660	103.695331	49.888769
611.874997	105.452816	49.893773
608.499020	91.420599	49.898778
604.957642	89.269533	49.903783
601.308745	98.653734	49.908788
597.715076	94.538284	49.913793
594.072577	93.664453	49.918797
591.090741	84.399038	49.923802
587.620970	94.421954	49.928807
583.854093	98.388022	49.933812
580.690008	100.984830	49.938817
576.964990	106.375489	49.943821
573.612930	99.695537	49.948826
569.733674	92.238929	49.953831
566.712519	95.217020	49.958836
562.833761	96.838074	49.963841
559.288496	93.697464	49.968845
555.775571	90.602225	49.973850
552.434279	89.349454	49.978855
548.859691	103.138928	49.983860
545.529856	97.365228	49.988865
541.802874	98.097985	49.993869
538.666495	97.476416	49.998874
534.882798	91.307986	50.003879
531.176957	92.181788	50.008884
527.842706	80.671001	50.013889
524.198559	98.784913	50.018893
520.969745	95.610011	50.023898
517.504613	96.604478	50.028903
513.662879	94.987079	50.033908
510.429909	91.057166	50.038913
506.669634	96.236540	50.043917
503.488202	90.357555	50.048922
499.957888	99.528751	50.053927
496.164193	95.427359	50.058932
492.670091	91.523915	50.063937
489.200427	105.373628	50.068941
486.262994	94.600767	50.073946
482.702151	93.022624	50.078951
478.966210	102.701838	50.083956
475.438687	100.422077	50.088961
471.647916	99.751374	50.093965
468.505284	93.461311	50.098970
464.767690	99.404505	50.103975
460.975271	100.313069	50.108980
457.501826	95.617872	50.113985
454.078593	94.222515	50.118989
451.015351	91.519206	50.123994
447.257408	96.274893	50.128999
443.930603	101.872034	50.134004
440.669059	96.901814	50.139009
436.908863	104.138979	50.144013
433.237973	91.568841	50.149018
429.659417	95.822838	50.154023
426.357450	97.865058	50.159028
422.788078	90.981262	50.164033
419.320488	109.280241	50.169037
416.040987	92.609248	50.174042
412.282828	97.906019	50.179047
408.430464	102.901670	50.184052
405.333791	88.827992	50.189057
401.344283	104.058566	50.194061
398.065990	87.044563	50.199066
394.664266	90.028867	50.204071
391.173738	106.885642	50.209076
388.227984	102.031788	50.214081
384.034589	106.317429	50.219085
380.792447	98.622613	50.224090
377.212049	110.858305	50.229095
373.991713	106.105952	50.234100
370.093655	92.196838	50.239105
366.461563	96.521074	50.244109
363.064530	99.110193	50.249114
359.572072	94.000388	50.254119
355.769384	92.631858	50.259124
352.622470	97.048007	50.264129
349.610314	99.904445	50.269133
345.713757	99.590076	50.274138
342.210614	95.879702	50.279143
338.708643	93.060000	50.284148
335.632753	90.962217	50.289153
331.673181	90.470032	50.294157
328.243289	100.785204	50.299162
324.644649	96.988310	50.304167
320.955813	100.615766	50.309172
317.618138	84.280815	50.314177
314.133777	87.171571	50.319181
310.884103	91.326504	50.324186
307.127201	84.844808	50.329191
303.376518	96.211774	50.334196
299.817541	89.971053	50.339201
296.479904	101.358480	50.344205
293.292474	89.320534	50.349210
289.889708	92.287304	50.354215
286.314440	97.430310	50.359220
282.620642	82.702917	50.364225
279.187340	98.733993	50.369229
275.796475	86.017475	50.374234
272.247824	87.045796	50.379239
268.330807	91.703157	50.384244
264.862382	98.492648	50.389249
261.229294	94.026383	50.394253
257.987267	99.314324	50.399258
254.451818	88.889208	50.404263
250.990803	97.654738	50.409268
247.797430	89.543217	50.414273
243.934825	94.666728	50.419277
240.820350	91.721206	50.424282
237.283759	89.322229	50.429287
233.504574	94.831223	50.434292
230.065338	94.871508	50.439297
226.386744	90.905766	50.444301
223.467967	84.655909	50.449306
219.755047	88.867491	50.454311
215.814920	96.873720	50.459316
212.744406	94.821182	50.464321
209.109828	91.128361	50.469325
205.504340	95.505307	50.474330
202.128774	95.058087	50.479335
198.347470	95.080618	50.484340
195.039606	88.019588	50.489345
191.401998	88.222105	50.494349
188.421134	85.372429	50.499354
184.607295	88.565906	50.504359
180.792815	82.009654	50.509364
177.462942	92.864875	50.514369
174.408572	95.817154	50.519373
170.360275	92.542545	50.524378
166.873218	90.097343	50.529383
163.445024	99.090811	50.534388
159.974322	85.803322	50.539393
156.235207	90.669309	50.544397
152.695151	96.859614	50.549402
149.474250	83.520798	50.554407
145.985302	76.941565	50.559412
142.405256	77.049559	50.564417
139.220139	82.217848	50.569421
135.775446	84.203093	50.574426
132.150893	85.716690	50.579431
128.564040	91.163969	50.584436
125.210782	88.614800	50.589441
121.347344	80.449023	50.594445
117.671979	92.114786	50.599450
114.343019	91.999485	50.604455
110.640454	96.940257	50.609460
108.018456	86.840616	50.614465
104.182425	80.495845	50.619469
100.474036	84.395878	50.624474
96.993611	77.936417	50.629479
93.300126	88.839221	50.634484
90.193341	88.371820	50.639489
86.457144	92.772596	50.644493
82.958863	81.278544	50.649498
79.448180	89.963564	50.654503
75.782055	88.701484	50.659508
72.631314	78.149789	50.664513
68.745471	90.787678	50.669517
65.353587	78.741049	50.674522
61.862722	75.179267	50.679527
58.107544	85.064094	50.684532
55.097553	89.447291	50.689537
50.997379	93.259769	50.694541
47.961263	88.950608	50.699546
44.349421	79.193829	50.704551
41.081263	92.480036	50.709556
37.772829	81.116340	50.714561
33.940258	82.182040	50.719565
30.298914	85.063169	50.724570
26.817267	79.487214	50.729575
22.919043	79.022180	50.734580
20.031568	79.509172	50.739585
16.153008	76.908753	50.744589
12.683445	73.557957	50.749594
9.384002	88.958101	50.754599
5.835742	81.366093	50.759604
2.812120	80.416775	50.764609